Thu Aug 25 12:18:43 2022

Number of Points = 9925

Depth (nm)	Load (N)	Time (s)
2.606232	100.557918	0.000000
2.535561	89.366065	0.005005
2.061853	85.624750	0.010010
1.860530	78.525137	0.015014
1.309160	68.848124	0.020019
1.418677	70.567832	0.025024
1.612635	57.819095	0.030029
1.606389	69.405720	0.035034
1.466298	43.497477	0.040038
1.143122	40.884194	0.045043
0.219703	42.658172	0.050048
-0.117206	30.679166	0.055053
-0.350737	17.326722	0.060058
-0.579477	10.240924	0.065062
-0.689215	11.223024	0.070067
-1.318411	3.016730	0.075072
-1.283149	3.330706	0.080077
-1.519570	-0.384493	0.085082
-1.612484	-8.206573	0.090086
-2.409282	1.412636	0.095091
-3.054461	-2.013891	0.100096
-2.500546	1.164270	0.105101
-2.936151	-2.943662	0.110106
-3.455014	-0.508576	0.115110
-4.071563	-5.293673	0.120115
-4.585826	1.009955	0.125120
-4.072455	1.960864	0.130125
-4.792677	1.719332	0.135130
-4.620334	-0.794414	0.140134
-4.624213	11.842167	0.145139
-4.699157	7.915004	0.150144
-5.498729	2.763113	0.155149
-5.924050	4.870333	0.160154
-5.877124	7.767264	0.165158
-6.033569	7.513329	0.170163
-6.300845	3.201852	0.175168
-6.406461	4.512335	0.180173
-7.263192	9.613617	0.185178
-7.439255	11.976012	0.190182
-7.845210	8.768264	0.195187
-7.830117	2.090354	0.200192
-7.660986	8.780453	0.205197
-8.290481	8.072291	0.210202
-8.114223	2.220177	0.215206
-8.242841	9.918708	0.220211
-8.871559	11.513633	0.225216
-8.661955	2.786774	0.230221
-9.094582	12.668469	0.235226
-9.705231	0.403345	0.240230
-10.007591	6.949020	0.245235
-10.383646	7.124962	0.250240
-10.458978	5.051818	0.255245
-10.832381	8.492333	0.260250
-10.825231	0.354016	0.265254
-11.440821	5.904731	0.270259
-11.874835	1.011940	0.275264
-12.133322	1.194772	0.280269
-11.952239	-0.178231	0.285274
-11.761444	3.221340	0.290278
-11.783726	13.902445	0.295283
-12.420120	16.096521	0.300288
-12.809624	2.920388	0.305293
-13.355402	0.133182	0.310298
-13.265240	2.213418	0.315302
-13.155918	8.375052	0.320307
-14.534104	12.697498	0.325312
-14.387955	-2.973335	0.330317
-14.968867	8.197090	0.335322
-14.822366	7.025658	0.340326
-14.753133	7.277364	0.345331
-14.756795	-0.865586	0.350336
-15.062460	-4.183957	0.355341
-15.710370	7.572766	0.360346
-15.978342	4.251652	0.365350
-16.351427	9.220207	0.370355
-16.420169	9.389128	0.375360
-16.264266	-0.094942	0.380365
-17.372425	4.928674	0.385370
-17.567621	-3.889779	0.390374
-17.810827	-7.271720	0.395379
-17.972261	2.684537	0.400384
-17.717674	-8.229186	0.405389
-17.882440	-0.173820	0.410394
-18.064782	-3.005314	0.415398
-18.603996	2.735913	0.420403
-19.177646	5.831317	0.425408
-19.075977	2.237152	0.430413
-19.324521	-1.599533	0.435418
-19.420401	-0.043803	0.440422
-19.647115	6.208445	0.445427
-20.491295	1.743752	0.450432
-20.904453	0.577752	0.455437
-21.010871	0.939237	0.460442
-20.991244	0.395124	0.465446
-20.700740	4.579499	0.470451
-21.220039	3.483913	0.475456
-21.864657	1.417710	0.480461
-22.282745	7.548084	0.485466
-22.324600	11.120149	0.490470
-22.301298	11.363233	0.495475
-22.480544	5.345357	0.500480
-22.332480	-1.318584	0.505485
-23.518003	3.897488	0.510490
-23.666787	-3.298907	0.515494
-23.614937	5.801358	0.520499
-23.919272	11.629173	0.525504
-23.836587	-0.896441	0.530509
-24.672739	5.172886	0.535514
-24.916007	2.148457	0.540518
-25.101997	0.200220	0.545523
-25.475607	1.970308	0.550528
-25.115665	4.311994	0.555533
-25.337458	5.020586	0.560538
-25.863210	9.788436	0.565542
-26.367127	7.080093	0.570547
-26.561300	11.008217	0.575552
-26.523918	8.787698	0.580557
-26.539759	8.514897	0.585562
-27.066902	-1.700543	0.590566
-27.683183	5.337242	0.595571
-28.308271	9.434123	0.600576
-28.228173	-0.917590	0.605581
-28.385379	5.953352	0.610586
-28.362548	3.709805	0.615590
-28.103252	7.763029	0.620595
-29.094737	9.762807	0.625600
-29.069353	-3.794700	0.630605
-29.647916	14.541246	0.635610
-29.642735	4.131665	0.640614
-29.568526	-3.868460	0.645619
-30.299627	2.851958	0.650624
-30.349898	-2.863420	0.655629
-31.029001	10.998920	0.660634
-30.901263	-2.561970	0.665638
-30.961476	5.182787	0.670643
-31.634729	1.782807	0.675648
-31.907853	5.169644	0.680653
-32.371450	12.427117	0.685658
-32.209562	2.296704	0.690662
-31.923692	6.937385	0.695667
-32.219297	4.968357	0.700672
-32.884876	4.642336	0.705677
-33.474265	10.606563	0.710682
-33.683583	6.083525	0.715686
-33.895189	9.777100	0.720691
-34.038512	10.944796	0.725696
-33.732020	8.166421	0.730701
-34.753258	1.641398	0.735706
-35.124991	4.619744	0.740710
-35.297144	7.136550	0.745715
-35.317281	7.535136	0.750720
-35.541674	-6.233168	0.755725
-35.286887	-0.249355	0.760730
-35.365282	1.468151	0.765734
-35.999420	-0.264336	0.770739
-36.396372	1.553702	0.775744
-36.333395	5.735762	0.780749
-37.303009	11.186926	0.785754
-37.758422	4.244217	0.790758
-37.735111	3.395807	0.795763
-38.052069	10.532226	0.800768
-38.153202	-1.584935	0.805773
-38.343479	6.139073	0.810778
-38.057346	7.878556	0.815782
-38.152960	6.564726	0.820787
-38.655520	5.273530	0.825792
-38.788425	1.886962	0.830797
-39.508885	5.808961	0.835802
-39.791506	5.087579	0.840806
-40.386469	2.972469	0.845811
-41.124122	2.752654	0.850816
-40.550226	2.362139	0.855821
-40.711897	-1.943735	0.860826
-41.275901	5.756573	0.865830
-40.853579	5.753639	0.870835
-41.423021	2.277282	0.875840
-41.217078	7.012743	0.880845
-41.974089	10.826576	0.885850
-42.610197	17.361272	0.890854
-42.804133	9.070963	0.895859
-43.232944	8.903997	0.900864
-42.632770	-1.231811	0.905869
-42.724978	7.989102	0.910874
-43.261705	1.615955	0.915878
-43.911307	1.958146	0.920883
-44.253859	7.203490	0.925888
-44.315267	-1.708691	0.930893
-44.625519	4.458569	0.935898
-44.516880	7.665368	0.940902
-44.907602	7.337410	0.945907
-45.878963	6.091195	0.950912
-45.867073	7.313665	0.955917
-46.062763	13.244679	0.960922
-45.991570	2.274266	0.965926
-45.725167	0.413333	0.970931
-45.682780	-1.548541	0.975936
-46.474707	2.118901	0.980941
-47.038887	-1.139980	0.985946
-47.582379	3.472461	0.990950
-47.413902	1.762913	0.995955
-48.153297	7.007162	1.000960
-48.269658	-0.548653	1.005965
-48.635088	2.080694	1.010970
-48.735756	-1.320416	1.015974
-49.105889	3.008598	1.020979
-49.220671	4.927958	1.025984
-48.873414	-7.060139	1.030989
-49.187815	5.277074	1.035994
-49.471892	0.645531	1.040998
-49.858690	3.407939	1.046003
-50.163784	5.056561	1.051008
-50.276351	-0.449739	1.056013
-50.540217	-5.248963	1.061018
-51.102644	3.210396	1.066022
-51.056737	6.623176	1.071027
-51.771916	11.423871	1.076032
-51.543365	0.466769	1.081037
-51.801790	-2.150323	1.086042
-52.436718	-3.907995	1.091046
-52.858853	5.095693	1.096051
-53.315347	9.169323	1.101056
-53.127207	-4.255495	1.106061
-53.261389	4.351898	1.111066
-53.414464	3.214750	1.116070
-53.447422	0.141552	1.121075
-53.907462	1.460113	1.126080
-54.427691	2.405292	1.131085
-54.479074	-1.500248	1.136090
-54.516274	1.340259	1.141094
-54.542587	2.318779	1.146099
-55.458443	12.412229	1.151104
-55.675160	12.673938	1.156109
-55.680847	10.295653	1.161114
-56.046330	6.958182	1.166118
-56.009456	3.491228	1.171123
-57.084063	7.063759	1.176128
-57.267829	12.505687	1.181133
-57.507050	7.038213	1.186138
-57.426847	9.831852	1.191142
-57.213025	5.090656	1.196147
-57.994117	14.052516	1.201152
-58.004312	5.597379	1.206157
-57.807346	6.945873	1.211162
-58.475047	2.478843	1.216166
-58.569070	6.780414	1.221171
-59.466231	12.707445	1.226176
-59.333550	10.206240	1.231181
-59.248783	5.690908	1.236186
-59.477169	9.921785	1.241190
-59.800702	9.513698	1.246195
-60.574051	17.677082	1.251200
-60.609359	3.569100	1.256205
-60.824747	8.035220	1.261210
-61.005834	9.196178	1.266214
-61.334962	4.033857	1.271219
-62.091620	23.679031	1.276224
-62.391663	10.020648	1.281229
-62.378470	17.197088	1.286234
-62.674014	12.630614	1.291238
-62.343723	15.258518	1.296243
-62.727872	14.809309	1.301248
-62.536268	4.073129	1.306253
-62.886898	7.557533	1.311258
-63.667069	8.407401	1.316262
-63.516049	10.541376	1.321267
-64.376861	11.470318	1.326272
-64.227064	7.378230	1.331277
-64.271164	6.252482	1.336282
-65.032995	-0.983895	1.341286
-65.437798	3.062651	1.346291
-65.531052	13.432169	1.351296
-65.358283	2.360421	1.356301
-65.688561	12.570925	1.361306
-65.498584	9.579853	1.366310
-66.144024	11.702583	1.371315
-66.798334	7.059448	1.376320
-66.650097	11.864062	1.381325
-67.016216	14.977571	1.386330
-67.210372	13.603252	1.391334
-67.420167	13.854386	1.396339
-67.829559	15.206141	1.401344
-68.192331	16.768890	1.406349
-68.302706	2.296185	1.411354
-68.227205	5.815058	1.416358
-68.999753	-1.150720	1.421363
-69.766482	3.800420	1.426368
-69.627352	3.481191	1.431373
-69.751983	2.428172	1.436378
-69.703834	0.493869	1.441382
-69.931717	7.916885	1.446387
-69.924954	15.322121	1.451392
-70.395357	9.723191	1.456397
-70.915069	10.045032	1.461402
-71.205601	4.152165	1.466406
-71.172638	-4.556500	1.471411
-71.810761	9.625281	1.476416
-71.536886	1.954538	1.481421
-72.277954	3.238041	1.486426
-72.805113	5.513079	1.491430
-72.841116	-1.204276	1.496435
-73.115934	11.360855	1.501440
-72.535129	9.377891	1.506445
-72.904432	9.033923	1.511450
-73.580013	8.551285	1.516454
-74.027448	8.197414	1.521459
-74.759349	11.181576	1.526464
-74.457881	4.620148	1.531469
-75.013565	6.263744	1.536474
-74.611384	8.927838	1.541478
-74.511812	7.864999	1.546483
-74.891370	9.522126	1.551488
-75.563807	12.933568	1.556493
-75.978088	15.320635	1.561498
-76.380754	11.821312	1.566502
-76.201032	7.588494	1.571507
-76.383263	12.030437	1.576512
-76.954462	0.078683	1.581517
-77.562900	4.808869	1.586522
-77.500210	3.758136	1.591526
-77.515489	-3.946390	1.596531
-77.659080	4.567564	1.601536
-77.543707	4.973391	1.606541
-77.854940	14.494378	1.611546
-78.747149	0.634563	1.616550
-78.738106	-4.226403	1.621555
-78.768061	-3.772495	1.626560
-79.083635	-5.902905	1.631565
-79.650322	7.495728	1.636570
-79.757747	6.832317	1.641574
-80.085088	6.829787	1.646579
-80.360960	6.967889	1.651584
-80.249665	-2.240268	1.656589
-81.034137	-0.674719	1.661594
-81.521515	-1.598132	1.666598
-81.236259	-1.658685	1.671603
-81.773363	14.133436	1.676608
-81.682294	-0.437267	1.681613
-81.895200	9.599820	1.686618
-82.695786	6.482387	1.691622
-82.573018	5.792399	1.696627
-83.010549	10.078192	1.701632
-82.903875	8.501713	1.706637
-83.087884	5.917254	1.711642
-83.617393	10.916647	1.716646
-84.006119	8.253534	1.721651
-84.566163	5.079428	1.726656
-84.371278	5.184895	1.731661
-84.739350	-0.680001	1.736666
-84.604151	8.552734	1.741670
-84.535887	0.844606	1.746675
-85.706572	13.224246	1.751680
-85.678452	6.598081	1.756685
-85.945003	12.192185	1.761690
-85.791539	8.010938	1.766694
-85.739297	6.977661	1.771699
-86.761326	8.371627	1.776704
-87.029558	5.556756	1.781709
-87.441782	13.299724	1.786714
-87.552324	7.426111	1.791718
-87.454313	-0.482829	1.796723
-87.758290	9.220516	1.801728
-87.967418	-0.165224	1.806733
-88.815110	9.635971	1.811738
-89.020043	8.880272	1.816742
-89.101735	2.998977	1.821747
-89.230389	9.697766	1.826752
-89.016562	5.624120	1.831757
-89.398393	3.320594	1.836762
-89.770937	7.384233	1.841766
-90.294845	6.786082	1.846771
-90.910853	17.000230	1.851776
-91.013699	7.297278	1.856781
-90.927270	16.021966	1.861786
-90.830650	4.468606	1.866790
-90.678955	9.490974	1.871795
-91.209834	15.882632	1.876800
-91.240282	2.878040	1.881805
-91.832509	10.060754	1.886810
-92.979433	2.941669	1.891814
-93.343955	0.714525	1.896819
-93.058638	0.176237	1.901824
-93.223311	6.029621	1.906829
-93.376554	12.143807	1.911834
-93.887959	12.138481	1.916838
-93.955622	6.245496	1.921843
-94.099400	14.193172	1.926848
-94.040665	8.732796	1.931853
-94.663560	18.296292	1.936858
-95.090391	14.829230	1.941862
-94.940073	5.795289	1.946867
-95.313952	13.620833	1.951872
-95.192796	-0.771086	1.956877
-96.017872	10.095911	1.961882
-96.154458	6.766869	1.966886
-96.252776	13.059110	1.971891
-96.686002	16.502674	1.976896
-96.670952	7.116605	1.981901
-96.840847	11.971066	1.986906
-97.763982	13.801954	1.991910
-97.753353	3.410509	1.996915
-98.174727	8.004311	2.006912
-97.551430	13.732150	2.016909
-97.141543	12.163145	2.026906
-97.016334	13.271187	2.036902
-96.139594	11.505486	2.046899
-95.215385	12.545351	2.056896
-95.348020	11.093034	2.066893
-94.654705	16.227028	2.076890
-94.160135	13.231916	2.086886
-93.897744	17.860061	2.096883
-92.985501	18.204887	2.106880
-92.526481	14.626135	2.116877
-92.618071	13.598206	2.126874
-91.714185	16.630634	2.136870
-91.201994	15.919911	2.146867
-90.514425	10.711945	2.156864
-90.036083	8.581018	2.166861
-89.856976	10.355356	2.176858
-89.081668	13.794402	2.186854
-88.659277	10.832775	2.196851
-88.240228	15.306493	2.206848
-87.385435	13.791320	2.216845
-87.188137	13.053912	2.226842
-86.999833	14.335800	2.236838
-86.047560	14.636340	2.246835
-85.601945	9.393428	2.256832
-84.819226	23.874260	2.266829
-84.459960	10.966132	2.276826
-84.292500	11.288275	2.286822
-83.756295	17.995942	2.296819
-83.164159	14.013029	2.306816
-82.813527	22.881703	2.316813
-81.834918	14.599717	2.326810
-81.251579	18.686566	2.336806
-81.439912	13.077319	2.346803
-80.877310	13.948933	2.356800
-80.157465	15.321763	2.366797
-79.849332	9.846969	2.376794
-78.915732	11.769180	2.386790
-78.811394	5.984198	2.396787
-78.187575	7.153496	2.406784
-77.442838	8.383042	2.416781
-77.298311	3.459739	2.426778
-76.365351	5.508763	2.436774
-76.162897	7.878156	2.446771
-75.800821	6.101233	2.456768
-74.988264	0.107080	2.466765
-74.858461	8.025166	2.476762
-74.024600	-2.844397	2.486758
-73.364525	5.690683	2.496755
-73.310458	2.707575	2.506752
-72.695665	3.529830	2.516749
-71.958720	7.418379	2.526746
-71.814634	4.136064	2.536742
-70.658433	5.725624	2.546739
-70.381667	8.891162	2.556736
-70.216178	5.570648	2.566733
-69.805762	1.882306	2.576730
-68.818566	-3.074831	2.586726
-68.680437	3.631851	2.596723
-68.538885	8.532354	2.606720
-67.751490	11.659064	2.616717
-66.578507	8.779400	2.626714
-66.157353	12.464008	2.636710
-65.978391	11.035725	2.646707
-66.015988	8.428108	2.656704
-65.118952	11.265208	2.666701
-64.506299	6.452287	2.676698
-64.159818	6.863589	2.686694
-63.278377	3.931406	2.696691
-63.058641	7.885158	2.706688
-62.792661	7.672346	2.716685
-62.077329	6.093497	2.726682
-61.347138	9.102459	2.736678
-61.264262	11.104118	2.746675
-60.502962	13.639372	2.756672
-60.259297	11.760627	2.766669
-59.577487	15.185817	2.776666
-58.546261	3.411013	2.786662
-58.325359	4.618103	2.796659
-58.532307	5.860553	2.806656
-57.564025	13.121408	2.816653
-57.103745	7.191954	2.826650
-56.951032	5.115218	2.836646
-55.850869	4.806547	2.846643
-55.654878	3.533986	2.856640
-55.145020	1.464647	2.866637
-54.414476	11.537743	2.876634
-54.211170	5.284257	2.886630
-53.045029	13.255376	2.896627
-52.880639	8.303617	2.906624
-52.676999	9.317008	2.916621
-52.502362	5.738468	2.926618
-51.122976	-1.795350	2.936614
-51.393912	2.960710	2.946611
-50.476941	-0.274812	2.956608
-49.783533	4.355490	2.966605
-49.562833	-2.375889	2.976602
-49.106526	-1.177174	2.986598
-48.280745	1.123063	2.996595
-48.142046	-0.460468	3.006592
-47.726724	-0.037777	3.016589
-46.961571	-2.742663	3.026586
-46.689022	2.602980	3.036582
-45.871095	-1.665563	3.046579
-45.383827	-2.771520	3.056576
-45.282604	3.712865	3.066573
-44.191420	-0.370413	3.076570
-43.935360	-2.558375	3.086566
-43.659624	-2.078967	3.096563
-43.292048	5.098613	3.106560
-42.356823	-0.908423	3.116557
-42.286964	5.276768	3.126554
-41.018533	1.764432	3.136550
-41.012934	-1.166733	3.146547
-40.642080	2.680979	3.156544
-39.882713	2.815346	3.166541
-39.384979	-2.042922	3.176538
-39.341973	-1.536552	3.186534
-38.891697	2.339897	3.196531
-38.068505	12.050022	3.206528
-37.017596	2.413568	3.216525
-36.912610	0.952528	3.226522
-36.490990	7.693989	3.236518
-36.175829	-0.759634	3.246515
-35.659086	-1.594610	3.256512
-35.356079	-0.745675	3.266509
-34.524090	2.120627	3.276506
-34.091705	5.996712	3.286502
-33.253711	3.511663	3.296499
-32.840081	-1.837108	3.306496
-32.480072	4.223427	3.316493
-32.420108	0.618506	3.326490
-31.261794	3.927855	3.336486
-30.978650	-3.510223	3.346483
-30.391063	-0.425063	3.356480
-29.780331	-2.674932	3.366477
-29.623987	-1.787178	3.376474
-29.030359	2.088985	3.386470
-28.311416	2.334225	3.396467
-27.993247	2.468030	3.406464
-27.749713	6.506754	3.416461
-26.879168	-5.493123	3.426458
-26.692898	0.300028	3.436454
-25.771771	-1.149506	3.446451
-25.432780	-1.912281	3.456448
-25.215658	0.711407	3.466445
-24.307896	3.065325	3.476442
-23.909530	1.270047	3.486438
-23.719092	1.303490	3.496435
-22.766796	10.660770	3.506432
-22.303141	6.511091	3.516429
-22.098884	2.924743	3.526426
-21.254847	2.824099	3.536422
-21.100095	-2.094470	3.546419
-20.818643	2.457831	3.556416
-19.357943	2.998664	3.566413
-19.328732	4.517723	3.576410
-19.177138	7.633185	3.586406
-18.711618	-1.730981	3.596403
-18.053785	4.596503	3.606400
-17.521073	9.017571	3.616397
-16.728825	2.323350	3.626394
-16.246581	7.126126	3.636390
-16.114679	5.888950	3.646387
-15.376588	9.317997	3.656384
-14.873329	6.831542	3.666381
-14.778176	5.334029	3.676378
-13.639500	9.967431	3.686374
-13.565128	7.792096	3.696371
-13.018434	14.076809	3.706368
-12.130770	7.212415	3.716365
-11.874815	15.395845	3.726362
-11.603479	8.045142	3.736358
-11.109641	6.409135	3.746355
-10.367324	7.857645	3.756352
-10.293357	11.641005	3.766349
-9.529135	15.385907	3.776346
-8.784652	4.365618	3.786342
-8.202397	9.032349	3.796339
-7.649599	9.145232	3.806336
-7.636764	9.754532	3.816333
-7.339011	17.554446	3.826330
-6.501569	11.689441	3.836326
-5.897881	15.316945	3.846323
-5.158606	23.747768	3.856320
-5.171325	18.212369	3.866317
-4.601091	25.285349	3.876314
-3.879971	30.579728	3.886310
-3.707116	34.300082	3.896307
-3.041229	38.133256	3.906304
-2.924391	42.381909	3.916301
-2.462453	58.702859	3.926298
-2.101932	64.281829	3.936294
-1.184016	83.645316	3.946291
-0.668402	88.262322	3.956288
-0.032576	102.702896	3.966285
0.000000	102.970896	3.971290
0.016556	120.353165	3.976294
0.526768	121.864562	3.981299
0.816596	133.249815	3.986304
0.851567	139.929347	3.991309
0.913452	135.186611	3.996314
0.794117	140.583683	4.001318
1.159342	140.596025	4.006323
0.647664	143.627958	4.011328
0.743323	143.723664	4.016333
0.491723	144.661559	4.021338
0.571146	134.395293	4.026342
1.004717	133.710388	4.031347
0.614304	140.500863	4.036352
0.876102	134.916879	4.041357
1.135685	137.619160	4.046362
0.998489	141.044837	4.051366
1.079430	142.091981	4.056371
1.003065	139.718425	4.061376
1.039693	146.511596	4.066381
1.273977	134.920754	4.071386
1.220314	132.116533	4.076390
0.801781	133.681699	4.081395
0.990340	147.791016	4.086400
0.866828	136.699161	4.091405
1.102433	131.245833	4.096410
1.139097	139.250720	4.101414
0.881743	136.491067	4.106419
0.756686	141.765649	4.111424
0.958885	142.945656	4.116429
1.066926	144.833281	4.121434
1.061281	150.506774	4.126438
1.175927	157.173830	4.131443
1.183826	166.597443	4.136448
1.609839	163.041012	4.141453
1.095675	150.697390	4.146458
1.139682	156.223899	4.151462
1.503184	144.049654	4.156467
1.084955	146.503793	4.161472
1.251391	150.891143	4.166477
1.488905	147.405378	4.171482
1.127592	147.819458	4.176486
1.500240	146.267733	4.181491
1.349417	152.960562	4.186496
1.079097	148.931101	4.191501
1.208940	154.760538	4.196506
1.219733	154.970783	4.201510
1.374026	160.941925	4.206515
1.245952	162.828582	4.211520
1.501267	162.288665	4.216525
1.402590	163.632874	4.221530
1.419812	167.262154	4.226534
1.474385	157.224396	4.231539
1.227738	163.460840	4.236544
1.371630	160.894582	4.241549
1.566070	166.242499	4.246554
1.568155	161.379411	4.251558
1.423211	157.599225	4.256563
1.207326	169.987559	4.261568
1.441831	161.810382	4.266573
1.507878	156.880325	4.271578
1.374272	160.406685	4.276582
1.697404	147.593352	4.281587
1.165619	159.996373	4.286592
1.279424	157.422174	4.291597
1.512756	158.015169	4.296602
1.513428	161.548964	4.301606
1.463851	153.571326	4.306611
1.587750	156.940279	4.311616
1.301375	158.035484	4.316621
1.429735	164.475766	4.321626
1.948708	177.384886	4.326630
1.986266	173.965247	4.331635
1.705347	170.573361	4.336640
1.805976	163.299853	4.341645
2.131291	157.471791	4.346650
1.826293	159.832260	4.351654
1.492992	152.838718	4.356659
1.620365	161.680458	4.361664
1.673575	153.297571	4.366669
1.767929	163.071471	4.371674
1.477244	162.294396	4.376678
1.775779	168.261923	4.381683
1.866685	182.361258	4.386688
1.872747	178.326452	4.391693
1.905670	181.608423	4.396698
1.865252	181.867821	4.401702
1.917530	170.210560	4.406707
2.093404	178.854883	4.411712
2.039808	163.708748	4.416717
1.722759	161.689276	4.421722
1.460758	169.933962	4.426726
2.105859	178.805325	4.431731
1.966130	184.939602	4.436736
2.036593	186.599001	4.441741
1.980475	176.711454	4.446746
2.066029	185.240216	4.451750
2.085287	182.440380	4.456755
2.118470	178.132404	4.461760
1.902343	168.301569	4.466765
2.187879	168.573172	4.471770
1.857257	178.492760	4.476774
2.320739	159.753818	4.481779
1.722464	175.777136	4.486784
2.321318	173.702745	4.491789
2.090069	173.982551	4.496794
2.046946	176.014088	4.501798
2.235399	173.633836	4.506803
1.914661	174.278843	4.511808
1.842010	179.896404	4.516813
2.270043	180.655049	4.521818
2.240324	184.576427	4.526822
2.326109	185.360221	4.531827
2.346366	193.627133	4.536832
2.332192	193.227516	4.541837
2.225636	177.134206	4.546842
2.150802	180.477353	4.551846
2.419866	177.499171	4.556851
1.978664	178.137742	4.561856
2.165678	174.564971	4.566861
2.312584	180.749250	4.571866
2.162636	184.835000	4.576870
2.224256	182.120276	4.581875
2.423781	185.224283	4.586880
2.415877	182.564745	4.591885
2.127924	177.819862	4.596890
2.298428	189.065658	4.601894
2.671366	185.008170	4.606899
2.144905	186.757931	4.611904
1.867772	193.356669	4.616909
2.291092	182.767571	4.621914
2.385611	182.787526	4.626918
2.384823	171.679585	4.631923
2.028858	180.027584	4.636928
2.102500	180.041319	4.641933
2.351691	177.616748	4.646938
2.487868	187.055076	4.651942
2.367343	178.980974	4.656947
2.333680	191.432522	4.661952
2.791556	199.327147	4.666957
2.400786	188.191712	4.671962
1.995057	188.343831	4.676966
2.489410	198.026604	4.681971
2.491755	208.064883	4.686976
2.769747	214.431118	4.691981
3.163142	212.509137	4.696986
2.709151	204.882744	4.701990
2.705743	196.230295	4.706995
3.026590	194.414597	4.712000
2.821543	192.190910	4.717005
2.678555	189.422821	4.722010
2.342436	193.414354	4.727014
2.652323	186.747134	4.732019
2.591449	180.590428	4.737024
2.530988	187.313404	4.742029
2.747994	196.147445	4.747034
2.458790	197.543655	4.752038
2.879650	195.304159	4.757043
3.047792	202.921476	4.762048
2.695114	200.195731	4.767053
2.494916	197.268924	4.772058
2.784165	208.749229	4.777062
3.086191	211.808707	4.782067
2.634867	213.410655	4.787072
3.068957	215.338953	4.792077
2.672740	209.313873	4.797082
2.674536	209.740665	4.802086
2.878371	204.868101	4.807091
2.907880	209.194660	4.812096
2.793780	209.902205	4.817101
3.326538	213.453884	4.822106
2.953395	209.680967	4.827110
3.163375	205.367430	4.832115
2.481149	205.749533	4.837120
2.848416	207.681972	4.842125
2.971856	214.752636	4.847130
2.846413	215.658113	4.852134
3.127560	209.504757	4.857139
3.171178	211.098760	4.862144
2.746528	207.327587	4.867149
3.122929	212.836835	4.872154
2.774493	218.333102	4.877158
2.950908	215.401069	4.882163
2.882200	218.486996	4.887168
2.879862	214.118137	4.892173
2.758521	212.387538	4.897178
2.659868	212.184657	4.902182
3.094704	214.119165	4.907187
2.776021	211.293178	4.912192
2.599605	212.630589	4.917197
3.171254	223.209271	4.922202
3.541471	237.448387	4.927206
3.509516	233.204387	4.932211
3.030271	220.829934	4.937216
3.029504	231.738756	4.942221
3.264785	230.151599	4.947226
3.631253	235.184679	4.952230
3.222328	214.737880	4.957235
3.385930	214.088943	4.962240
3.277950	214.333617	4.967245
3.367396	216.578508	4.972250
3.086336	208.966147	4.977254
3.337686	211.650747	4.982259
3.163970	220.650423	4.987264
3.411638	225.771717	4.992269
3.628312	223.279469	4.997274
2.914652	228.269808	5.002278
3.116555	222.979922	5.007283
3.441328	239.655948	5.012288
3.503533	238.984932	5.017293
3.568997	238.221656	5.022298
3.580422	239.523310	5.027302
3.686851	247.207263	5.032307
3.425438	230.499081	5.037312
3.130447	222.050494	5.042317
3.298942	222.324617	5.047322
3.687649	237.706126	5.052326
3.778927	235.429678	5.057331
3.527375	239.689549	5.062336
3.432975	227.552190	5.067341
3.618050	230.645813	5.072346
3.438924	244.040851	5.077350
3.462649	232.308929	5.082355
3.812321	242.235860	5.087360
3.602751	240.060333	5.092365
3.366097	231.017300	5.097370
3.506301	242.682333	5.102374
3.868185	233.969467	5.107379
3.886389	234.349396	5.112384
3.460364	236.962959	5.117389
3.557213	243.034879	5.122394
3.627826	246.535585	5.127398
3.615723	248.419900	5.132403
3.488278	252.258527	5.137408
3.721189	244.489691	5.142413
4.176945	237.783778	5.147418
3.767275	244.738663	5.152422
3.918191	231.983891	5.157427
3.572991	231.860767	5.162432
3.683430	241.163949	5.167437
3.876099	238.707098	5.172442
3.752493	242.576759	5.177446
3.813416	242.114754	5.182451
3.471028	247.075402	5.187456
3.732475	247.556426	5.192461
3.783714	248.472188	5.197466
3.683405	248.794755	5.202470
3.833450	249.347018	5.207475
3.789149	247.091811	5.212480
3.943069	249.959363	5.217485
4.278884	244.983851	5.222490
3.857481	243.066142	5.227494
3.809047	241.795522	5.232499
3.957655	252.503780	5.237504
3.945673	247.291692	5.242509
3.792712	239.409308	5.247514
3.832655	245.142128	5.252518
3.969058	236.353857	5.257523
4.020062	243.951579	5.262528
4.004408	241.372341	5.267533
4.104430	237.670817	5.272538
3.568911	246.818944	5.277542
3.673181	241.901858	5.282547
3.502637	237.704882	5.287552
3.634924	247.858868	5.292557
3.879237	249.411938	5.297562
3.814039	270.103833	5.302566
4.220547	256.739514	5.307571
4.108070	265.764420	5.312576
3.770934	265.146481	5.317581
4.101734	259.064423	5.322586
3.910914	263.077499	5.327590
4.264332	250.952218	5.332595
4.203642	258.988232	5.337600
4.226542	255.115287	5.342605
4.260978	251.088675	5.347610
4.429505	262.220930	5.352614
4.385568	257.526379	5.357619
4.161448	254.036992	5.362624
4.220794	265.724201	5.367629
4.224355	265.407226	5.372634
4.277681	262.791867	5.377638
4.336776	260.846329	5.382643
4.125721	261.211558	5.387648
4.317244	260.833495	5.392653
4.336764	246.802144	5.397658
4.123106	262.439407	5.402662
4.612459	261.786887	5.407667
4.350643	258.945656	5.412672
4.537782	255.129237	5.417677
4.670176	258.645577	5.422682
4.295705	264.376894	5.427686
4.523885	264.787200	5.432691
4.330509	265.772927	5.437696
4.856264	262.137573	5.442701
4.808516	251.571621	5.447706
4.291548	260.666228	5.452710
4.302076	247.484182	5.457715
4.145591	256.288185	5.462720
4.293535	251.832495	5.467725
4.774664	252.424634	5.472730
4.363806	262.609944	5.477734
4.629122	253.213001	5.482739
4.874077	258.625799	5.487744
4.397389	268.327874	5.492749
4.389257	249.419119	5.497754
4.469138	255.588615	5.502758
4.766775	262.505453	5.507763
4.129848	268.008970	5.512768
4.462749	278.713679	5.517773
5.070344	276.524010	5.522778
4.539404	276.293945	5.527782
4.279046	272.250240	5.532787
4.548529	277.864847	5.537792
4.815955	285.450825	5.542797
4.684535	281.817192	5.547802
4.455566	286.098846	5.552806
4.428577	285.843606	5.557811
4.873322	283.173244	5.562816
4.514604	284.596171	5.567821
4.991082	279.500533	5.572826
4.691082	284.277376	5.577830
4.916695	278.259250	5.582835
4.882852	279.074446	5.587840
4.853672	280.202129	5.592845
4.892845	284.476572	5.597850
4.820123	283.380599	5.602854
4.942974	283.494193	5.607859
4.833902	289.778729	5.612864
4.976639	285.029613	5.617869
5.205566	285.019018	5.622874
4.669448	287.434699	5.627878
4.801094	278.954040	5.632883
5.055372	278.784447	5.637888
5.143608	284.734343	5.642893
5.060546	280.760935	5.647898
4.905071	284.543848	5.652902
4.850209	280.281280	5.657907
4.855491	286.373889	5.662912
4.917714	286.310318	5.667917
4.935172	278.116474	5.672922
4.886490	288.052061	5.677926
5.297834	284.722534	5.682931
4.874048	278.356896	5.687936
4.892781	283.033180	5.692941
5.097208	279.549410	5.697946
4.953559	290.521784	5.702950
5.351217	282.654351	5.707955
5.133371	279.894813	5.712960
4.936456	287.101121	5.717965
5.302779	284.079210	5.722970
5.098471	289.366252	5.727974
5.272466	295.777284	5.732979
5.329596	286.624917	5.737984
5.459970	285.399045	5.742989
5.173203	282.770530	5.747994
4.973518	280.527009	5.752998
5.053641	272.291711	5.758003
5.508527	289.178354	5.763008
5.369130	285.435238	5.768013
5.457380	272.509919	5.773018
5.047868	280.856863	5.778022
5.317736	282.918468	5.783027
5.115421	287.218092	5.788032
5.280345	302.989066	5.793037
5.690336	304.509855	5.798042
5.331917	295.909817	5.803046
5.235630	291.612607	5.808051
5.712455	303.816569	5.813056
5.516820	293.685057	5.818061
5.895208	277.885839	5.823066
5.390133	279.891689	5.828070
5.377462	284.838652	5.833075
5.511852	277.724325	5.838080
5.048599	287.326228	5.843085
5.434948	279.375147	5.848090
5.008612	290.742994	5.853094
5.407300	294.736480	5.858099
5.350329	306.685553	5.863104
5.282572	308.508990	5.868109
5.674523	300.493745	5.873114
5.672089	298.244627	5.878118
5.513507	305.242453	5.883123
5.438809	307.883239	5.888128
5.756099	310.193685	5.893133
5.862258	306.212770	5.898138
5.567328	308.986140	5.903142
5.580644	310.790547	5.908147
5.708887	309.973138	5.913152
5.534383	318.618642	5.918157
5.488161	304.784210	5.923162
5.466035	311.507555	5.928166
5.831891	313.705987	5.933171
5.643748	308.720800	5.938176
5.880888	307.921132	5.943181
5.979281	307.693703	5.948186
5.469911	316.790312	5.953190
5.625788	311.463318	5.958195
5.746947	297.400183	5.963200
5.469154	305.520854	5.968205
5.675595	302.938447	5.973210
5.316511	306.588750	5.978214
5.796658	306.579922	5.983219
5.799698	310.945456	5.988224
5.531902	315.350261	5.993229
5.657284	304.190831	5.998234
5.621032	308.755512	6.003238
5.664248	301.731391	6.008243
5.878806	308.613807	6.013248
5.625480	314.490676	6.018253
6.137365	314.400945	6.023258
5.774680	312.616400	6.028262
5.670614	312.740237	6.033267
5.616021	310.296807	6.038272
5.607550	313.053768	6.043277
5.867255	322.593038	6.048282
5.787729	328.679966	6.053286
6.115259	328.929173	6.058291
5.918218	318.180925	6.063296
5.416208	315.342516	6.068301
5.974158	312.217808	6.073306
5.761773	319.094354	6.078310
5.724022	303.524832	6.083315
5.755841	304.089293	6.088320
5.746875	314.262284	6.093325
5.846760	313.620164	6.098330
5.717775	318.607507	6.103334
5.702031	326.702949	6.108339
5.912779	331.140348	6.113344
6.024844	330.126154	6.118349
5.968603	313.629361	6.123354
5.614557	309.559197	6.128358
5.784334	300.205673	6.133363
5.613374	308.828469	6.138368
5.616144	304.952341	6.143373
6.019533	314.753836	6.148378
5.642171	306.985676	6.153382
5.836397	319.195961	6.158387
5.884993	311.478121	6.163392
5.919817	311.814318	6.168397
5.776209	305.354151	6.173402
5.796974	308.536808	6.178406
5.754003	303.408653	6.183411
5.629419	311.372442	6.188416
5.520963	321.133912	6.193421
6.216180	325.109420	6.198426
5.674558	323.106133	6.203430
5.571184	312.852585	6.208435
6.118096	318.740118	6.213440
5.519559	310.848421	6.218445
5.816277	310.396927	6.223450
5.736112	318.831493	6.228454
5.899551	318.941892	6.233459
5.664858	313.894394	6.238464
5.654515	317.183169	6.243469
5.893975	321.166808	6.248474
5.849087	326.296003	6.253478
5.747887	315.763698	6.258483
6.161079	322.662454	6.263488
5.801016	298.930201	6.268493
5.473024	294.153595	6.273498
5.447709	311.966560	6.278502
5.863681	319.943736	6.283507
6.073310	324.906501	6.288512
5.804943	323.812706	6.293517
5.926917	302.124672	6.298522
5.495638	304.315118	6.303526
5.698755	306.880737	6.308531
5.897492	313.066433	6.313536
5.819422	317.954049	6.318541
6.156196	320.919515	6.323546
5.862675	306.310731	6.328550
5.432573	295.867936	6.333555
5.433064	303.403995	6.338560
5.711877	312.206263	6.343565
6.255818	308.400369	6.348570
5.819125	317.776661	6.353574
5.955546	301.461667	6.358579
5.663046	304.943347	6.363584
5.692351	304.752054	6.368589
5.791870	307.840113	6.373594
5.538184	309.297207	6.378598
5.817006	318.295632	6.383603
5.697094	319.484990	6.388608
5.683417	335.654141	6.393613
5.545969	326.298118	6.398618
5.639306	322.689374	6.403622
5.874177	328.568853	6.408627
5.912371	325.592018	6.413632
5.612422	328.764816	6.418637
6.136162	325.955519	6.423642
5.905011	330.313457	6.428646
5.700952	323.321744	6.433651
5.809601	321.858824	6.438656
5.745821	334.789762	6.443661
5.866574	320.040127	6.448666
5.554309	330.282795	6.453670
5.842246	328.548171	6.458675
5.953156	322.775795	6.463680
5.761936	323.517574	6.468685
6.053471	324.009706	6.473690
5.707410	328.170508	6.478694
5.745627	320.435308	6.483699
6.168852	314.765863	6.488704
6.018403	318.348677	6.493709
5.998745	306.000234	6.498714
5.702272	307.574765	6.503718
5.622505	301.294424	6.508723
5.631359	303.453876	6.513728
5.768363	300.749469	6.518733
5.752171	300.745641	6.523738
5.634005	299.087304	6.528742
5.589600	289.972990	6.533747
5.734737	302.270049	6.538752
5.956406	318.275758	6.543757
5.731061	314.878301	6.548762
5.980812	327.405763	6.553766
5.677551	311.289367	6.558771
5.549809	312.720400	6.563776
5.706378	321.858206	6.568781
5.821932	321.147191	6.573786
6.015697	321.641986	6.578790
6.135463	321.075845	6.583795
5.877910	320.840910	6.588800
5.616783	303.338501	6.593805
5.522188	302.511713	6.598810
5.639208	307.650338	6.603814
5.805192	323.016196	6.608819
5.793582	324.982701	6.613824
5.704167	324.718258	6.618829
5.933272	327.352576	6.623834
5.707304	332.481671	6.628838
5.957304	321.596939	6.633843
5.805780	317.691198	6.638848
5.655228	315.481103	6.643853
5.688146	320.914487	6.648858
5.595512	325.804387	6.653862
5.925674	323.572758	6.658867
6.029894	315.333665	6.663872
5.935568	315.895744	6.668877
6.052002	306.999834	6.673882
5.495567	304.641360	6.678886
5.762639	304.371684	6.683891
5.890582	307.581842	6.688896
5.510377	309.998408	6.693901
5.910600	303.642862	6.698906
5.547510	309.093995	6.703910
5.939673	320.143790	6.708915
6.017738	322.450590	6.713920
5.711704	314.234647	6.718925
5.852329	298.077188	6.723930
5.661359	302.387694	6.728934
5.496282	302.672953	6.733939
5.893301	318.144980	6.738944
5.891521	322.726410	6.743949
6.182532	303.922590	6.748954
5.930357	304.496745	6.753958
5.731180	292.666828	6.758963
6.239722	305.261296	6.763968
5.596945	301.894443	6.768973
5.645324	299.536122	6.773978
5.602356	311.106511	6.778982
5.391172	304.229819	6.783987
5.842329	314.656590	6.788992
5.811227	314.702555	6.793997
5.764545	308.429683	6.799002
5.644611	306.879191	6.804006
5.700905	312.463936	6.809011
5.840772	327.163164	6.814016
5.635845	319.766622	6.819021
5.747253	323.064796	6.824026
6.054935	328.743038	6.829030
5.796991	326.720614	6.834035
5.964163	310.154018	6.839040
5.759312	301.321105	6.844045
5.604082	297.330526	6.849050
5.729859	317.081380	6.854054
6.118815	320.623973	6.859059
5.949813	308.412825	6.864064
5.670760	298.920813	6.869069
5.745197	294.562051	6.874074
5.543100	302.493688	6.879078
5.537289	302.716027	6.884083
6.221496	313.932035	6.889088
5.879538	317.810614	6.894093
5.720261	311.849617	6.899098
5.254827	307.607077	6.904102
5.774037	319.636727	6.909107
5.756574	327.957069	6.914112
5.628475	330.315154	6.919117
6.244265	329.946548	6.924122
5.787157	330.252252	6.929126
5.613112	321.702408	6.934131
6.200981	326.416083	6.939136
5.830177	320.523026	6.944141
5.677507	316.554189	6.949146
5.461605	306.906743	6.954150
5.565113	325.148797	6.959155
5.884115	329.173760	6.964160
5.562458	334.428581	6.969165
6.213683	327.226929	6.974170
5.970760	327.929352	6.979174
5.778994	322.052536	6.984179
5.995911	309.012117	6.989184
5.551745	315.988253	6.994189
5.563035	309.851833	6.999194
5.820251	318.799860	7.004198
5.837637	327.026154	7.009203
5.998677	325.937846	7.014208
5.994190	310.875642	7.019213
5.577829	306.574793	7.024218
5.503292	304.612222	7.029222
5.855884	314.061002	7.034227
6.301383	326.810899	7.039232
5.856028	322.669615	7.044237
6.061759	313.370563	7.049242
5.932694	299.669339	7.054246
5.829316	304.842495	7.059251
5.702666	310.727990	7.064256
5.634896	306.366196	7.069261
5.483679	299.919878	7.074266
5.644183	311.467879	7.079270
5.701581	308.418434	7.084275
5.716783	311.804447	7.089280
5.735400	307.289911	7.094285
5.765266	310.474307	7.099290
5.955790	306.315657	7.104294
5.849170	300.839966	7.109299
6.088932	305.076658	7.114304
5.760312	313.977263	7.119309
5.801118	306.203698	7.124314
5.802801	306.216052	7.129318
5.946396	299.324904	7.134323
5.765609	299.331046	7.139328
5.685075	310.859863	7.144333
5.564754	301.089876	7.149338
5.552290	301.338568	7.154342
5.518317	301.343853	7.159347
5.694082	319.849831	7.164352
5.812736	334.141094	7.169357
6.391812	328.602253	7.174362
6.140440	319.858879	7.179366
5.708561	311.469662	7.184371
5.678734	301.470357	7.189376
5.482218	308.521585	7.194381
5.852801	312.187280	7.199386
5.459432	311.375667	7.204390
5.696851	310.658213	7.209395
5.729186	315.117235	7.214400
5.849853	333.736266	7.219405
5.857388	330.609207	7.224410
5.940926	331.393360	7.229414
5.799039	314.425923	7.234419
5.573453	315.150940	7.239424
5.838444	320.541634	7.244429
5.821204	317.279252	7.249434
5.804344	315.399394	7.254438
5.596118	308.174218	7.259443
6.348243	317.626841	7.264448
5.731683	316.866016	7.269453
5.865267	302.582628	7.274458
5.929559	302.237154	7.279462
5.557629	303.095833	7.284467
5.824581	303.493737	7.289472
5.840350	306.816384	7.294477
5.956676	301.992307	7.299482
5.679179	308.663912	7.304486
5.673763	304.241728	7.309491
5.598866	300.855504	7.314496
5.540788	310.305350	7.319501
6.034595	306.323811	7.324506
5.979454	302.618110	7.329510
5.496339	306.964899	7.334515
5.669639	304.270624	7.339520
5.525988	317.815186	7.344525
6.039617	317.022817	7.349530
5.752288	325.796735	7.354534
5.750339	331.786087	7.359539
6.154239	321.291700	7.364544
5.822906	320.410254	7.369549
6.101356	314.519880	7.374554
5.933097	310.031459	7.379558
5.509755	311.983377	7.384563
5.681607	310.257452	7.389568
5.720893	309.808327	7.394573
5.914754	309.471027	7.399578
5.842023	303.679973	7.404582
5.610595	312.233150	7.409587
5.725163	311.139469	7.414592
5.484295	303.236029	7.419597
5.964499	315.107270	7.424602
6.267813	313.673963	7.429606
5.898011	311.773473	7.434611
5.703246	303.970378	7.439616
5.589419	306.696389	7.444621
6.011547	298.508735	7.449626
5.271160	300.181291	7.454630
5.321432	300.891560	7.459635
6.186398	319.602770	7.464640
5.772588	316.839128	7.469645
5.899477	308.878065	7.474650
5.767255	306.203185	7.479654
5.589036	297.862817	7.484659
5.704707	305.912349	7.489664
5.796381	328.332479	7.494669
6.020936	319.505045	7.499674
5.947909	317.520089	7.504678
5.739704	316.679463	7.509683
5.522999	305.209794	7.514688
5.333962	313.794296	7.519693
5.960649	314.974245	7.524698
5.890303	326.688142	7.529702
5.810935	338.669219	7.534707
6.130947	325.470263	7.539712
5.831429	320.499360	7.544717
5.682879	304.434661	7.549722
5.564337	310.167023	7.554726
5.865610	322.879401	7.559731
5.993686	325.823782	7.564736
5.509074	313.032483	7.569741
5.741483	324.050362	7.574746
5.855417	331.505382	7.579750
5.904452	324.622713	7.584755
5.701358	315.058678	7.589760
5.613663	324.418258	7.594765
5.862395	326.347136	7.599770
5.892798	335.526864	7.604774
6.039993	325.933251	7.609779
5.970492	312.396695	7.614784
5.494850	312.721121	7.619789
5.622134	309.110225	7.624794
5.630253	321.308541	7.629798
5.634514	330.084231	7.634803
5.708738	323.153322	7.639808
5.577398	329.210403	7.644813
5.702701	328.918646	7.649818
5.663059	337.049475	7.654822
5.466639	342.408064	7.659827
6.123265	336.183179	7.664832
5.783331	334.515292	7.669837
5.960550	332.978352	7.674842
5.987482	340.747569	7.679846
6.098836	337.085378	7.684851
6.113244	337.775957	7.689856
5.356004	335.673572	7.694861
5.663589	333.407514	7.699866
5.584661	338.940686	7.704870
5.505892	339.228241	7.709875
5.611665	329.166545	7.714880
5.832397	331.413028	7.719885
5.767980	327.199403	7.724890
5.792151	327.423372	7.729894
5.393259	328.450794	7.734899
5.670135	332.131175	7.739904
5.517369	332.423996	7.744909
5.657901	328.016906	7.749914
5.547794	343.008417	7.754918
5.951420	337.342036	7.759923
6.093744	334.064142	7.764928
5.785910	330.733391	7.769933
6.027557	327.772136	7.774938
5.912126	342.916345	7.779942
6.020414	340.032931	7.784947
5.972334	337.841581	7.789952
5.648729	335.854754	7.794957
6.008426	333.235676	7.799962
5.736001	331.905230	7.804966
5.816564	336.926186	7.809971
5.929578	326.945616	7.814976
6.010525	325.844547	7.819981
6.039176	332.743445	7.824986
5.793254	340.729422	7.829990
5.848647	330.982508	7.834995
6.003220	337.260555	7.840000
5.841475	329.167532	7.845005
5.402611	318.684967	7.850010
5.645930	328.872223	7.855014
5.662691	329.138483	7.860019
6.059804	328.576345	7.865024
5.773930	332.297441	7.870029
6.196775	335.312699	7.875034
5.768298	332.541862	7.880038
5.387648	319.784890	7.885043
5.931560	321.604242	7.890048
5.837265	340.095606	7.895053
6.053792	329.763452	7.900058
5.768461	318.263397	7.905062
5.371270	318.028194	7.910067
5.529829	321.901120	7.915072
5.891853	337.331190	7.920077
5.617756	334.203964	7.925082
5.708072	343.491369	7.930086
5.965567	344.814589	7.935091
5.901777	332.707164	7.940096
5.481777	340.182568	7.945101
5.752262	341.440476	7.950106
5.943762	343.466909	7.955110
5.459472	346.738197	7.960115
5.775470	338.140040	7.965120
5.987806	343.257413	7.970125
5.878851	332.574676	7.975142
6.112088	335.807438	7.980160
6.137657	337.810442	7.985178
5.533606	316.032653	7.990195
5.839312	334.328999	7.995213
5.925055	336.893763	8.000230
6.160469	337.696267	8.005248
5.742100	323.093924	8.010266
5.410664	313.429314	8.015283
5.967301	336.151708	8.020301
5.919043	340.331115	8.025318
5.592661	324.404727	8.030336
5.580213	340.917447	8.035354
5.944516	336.868324	8.040371
5.696583	339.213976	8.045389
5.634342	345.298484	8.050406
5.701852	330.282344	8.055424
5.539968	344.887171	8.060442
5.736977	332.135493	8.065459
5.857245	345.118246	8.070477
5.957167	338.551243	8.075494
5.672537	341.660022	8.080512
5.884052	332.579348	8.085530
6.058952	335.635061	8.090547
5.659482	340.699455	8.095565
5.932957	344.632798	8.100582
6.017647	334.991339	8.105600
5.979035	344.445626	8.110618
6.350697	341.061210	8.115635
5.935145	341.760584	8.120653
5.955083	344.130537	8.125670
6.042705	340.588657	8.130688
5.896500	337.291692	8.135706
6.223211	339.215957	8.140723
5.988331	347.924686	8.145741
5.899237	340.850822	8.150758
6.168795	331.041547	8.155776
5.848235	348.116934	8.160794
5.986469	334.566594	8.165811
6.070166	335.029959	8.170829
6.131002	336.140676	8.175846
6.142430	333.314464	8.180864
5.787494	344.159501	8.185882
6.077584	336.865285	8.190899
6.256713	333.599397	8.195917
5.889061	329.926884	8.200934
5.810561	345.244466	8.205952
5.834193	339.800236	8.210970
5.981811	332.048672	8.215987
5.927477	341.757880	8.221005
6.010163	342.533822	8.226022
6.013711	337.521919	8.231040
5.889431	335.878280	8.236058
6.163007	350.077221	8.241075
6.038826	339.048403	8.246093
5.989095	344.465091	8.251110
5.931619	345.291395	8.256128
5.594940	344.618288	8.261146
5.679264	338.912090	8.266163
5.785753	345.061678	8.271181
5.930122	356.412302	8.276198
6.326848	369.124544	8.281216
6.177826	374.878683	8.286234
6.263830	370.942582	8.291251
6.046226	371.588853	8.296269
6.250712	368.022346	8.301286
6.330847	365.355774	8.306304
5.810698	352.438741	8.311322
6.201338	358.310288	8.316339
5.959184	365.331845	8.321357
6.077219	365.692002	8.326374
6.126945	368.085693	8.331392
6.022600	371.005287	8.336410
6.289437	365.784869	8.341427
6.183191	368.234555	8.346445
5.828248	364.780946	8.351462
5.929973	371.483544	8.356480
5.904065	376.893353	8.361498
6.156931	376.755868	8.366515
5.942448	374.365825	8.371533
5.938131	372.053305	8.376550
6.066593	362.881490	8.381568
6.157491	363.681391	8.386586
6.146009	361.600364	8.391603
6.141185	372.693514	8.396621
6.346856	368.893296	8.401638
6.302722	368.669804	8.406656
6.210622	363.761240	8.411674
6.225062	354.269630	8.416691
6.208297	365.746491	8.421709
6.370613	373.888081	8.426726
6.441995	362.238485	8.431744
6.270658	369.258415	8.436762
6.118455	366.849148	8.441779
5.792898	372.129183	8.446797
6.051702	378.699877	8.451814
6.500378	377.875319	8.456832
6.098399	387.957751	8.461850
6.256744	387.806674	8.466867
6.448721	384.264214	8.471885
6.403588	385.397849	8.476902
6.716214	388.362565	8.481920
6.223122	373.882339	8.486938
6.149835	376.421534	8.491955
5.891040	372.719334	8.496973
5.414482	390.756458	8.501990
6.425182	396.376235	8.507008
6.231156	393.872533	8.512026
6.432045	403.270393	8.517043
6.412168	390.420113	8.522061
6.694940	403.106053	8.527078
6.952194	400.389635	8.532096
6.134463	397.945786	8.537114
6.292873	392.537225	8.542131
6.643986	399.705679	8.547149
6.603806	394.350323	8.552166
6.322699	389.982597	8.557184
6.108791	399.259256	8.562202
6.446836	381.505676	8.567219
6.099135	385.356477	8.572237
6.335944	384.224293	8.577255
6.182530	391.285604	8.582272
6.095604	399.529373	8.587290
6.015885	397.844034	8.592307
6.418979	398.888507	8.597325
6.262938	397.959882	8.602343
6.512589	395.282525	8.607360
6.468873	395.503928	8.612378
6.453208	393.029084	8.617395
6.437531	385.239968	8.622413
6.200242	393.639834	8.627431
6.690256	406.697241	8.632448
6.376324	412.010180	8.637466
6.827497	410.465717	8.642483
6.815460	405.008121	8.647501
6.609907	407.826815	8.652519
6.500876	399.395924	8.657536
6.513194	398.848012	8.662554
6.838606	390.554179	8.667571
6.526873	395.740539	8.672589
6.356859	395.628286	8.677607
6.592012	396.525506	8.682624
6.521777	391.253754	8.687642
6.187264	387.099519	8.692659
6.331728	393.987930	8.697677
6.205656	396.140930	8.702695
6.942922	398.982312	8.707712
6.643455	399.076532	8.712730
6.420033	396.189278	8.717747
6.556065	402.214339	8.722765
6.644586	415.886915	8.727783
6.995564	408.371694	8.732800
6.659894	403.113125	8.737818
6.421154	394.759362	8.742835
6.468614	385.451907	8.747853
6.444863	405.131669	8.752871
6.664690	408.268716	8.757888
6.538410	414.041395	8.762906
6.788674	416.119655	8.767923
6.866123	416.902731	8.772941
6.210322	408.043117	8.777959
6.735523	416.951521	8.782976
6.587992	431.046094	8.787994
6.716654	423.398445	8.793011
6.657242	415.919120	8.798029
6.482529	409.609712	8.803047
6.958104	419.504175	8.808064
6.790269	423.150080	8.813082
6.529615	421.240628	8.818099
6.744543	415.163653	8.823117
6.666821	417.602565	8.828135
6.762642	420.307771	8.833152
6.491925	421.221137	8.838170
6.446778	422.168587	8.843187
6.787486	419.811469	8.848205
6.904651	420.203322	8.853223
6.535302	422.489114	8.858240
6.782631	433.214596	8.863258
6.613899	429.255279	8.868275
6.694717	431.416893	8.873293
6.306318	432.708453	8.878311
6.624604	420.508902	8.883328
6.408937	421.767087	8.888346
6.497354	424.325133	8.893363
6.726324	424.557459	8.898381
7.103309	439.797446	8.903399
6.828636	437.514654	8.908416
6.888923	433.099738	8.913434
6.775537	429.321096	8.918451
6.774583	423.060196	8.923469
6.586317	426.766107	8.928487
7.103757	428.127176	8.933504
6.929749	422.328884	8.938522
6.995650	419.292156	8.943539
7.096619	422.596149	8.948557
6.594637	421.191559	8.953575
6.802070	418.997331	8.958592
7.056814	421.087512	8.963610
6.647083	423.811970	8.968627
6.903409	416.330511	8.973645
6.760070	426.101047	8.978663
7.028185	430.716891	8.983680
7.286907	418.230033	8.988698
6.803910	417.734480	8.993715
6.970932	418.389916	8.998733
7.058353	420.591519	9.003751
7.017782	427.127087	9.008768
6.919765	421.020249	9.013786
6.561528	423.297989	9.018803
7.392232	421.914964	9.023821
7.014597	423.678200	9.028839
6.825343	421.883790	9.033856
6.955742	418.237364	9.038874
7.062746	415.026942	9.043891
6.649922	425.859008	9.048909
6.836481	430.377179	9.053927
7.107101	418.876207	9.058944
6.980763	418.141740	9.063962
6.479754	419.491968	9.068979
7.377894	433.627832	9.073997
7.078904	451.779205	9.079015
7.142351	437.628288	9.084032
7.216629	428.518577	9.089050
6.814434	427.063638	9.094067
6.926292	423.757781	9.099085
6.800063	437.331479	9.104103
6.937294	442.453820	9.109120
7.257876	437.840333	9.114138
7.532144	446.172696	9.119155
7.103831	431.584444	9.124173
7.018440	435.687642	9.129191
7.107035	425.288141	9.134208
6.989352	427.537659	9.139226
6.849226	441.990837	9.144243
7.308534	448.318707	9.149261
7.275793	449.021221	9.154279
6.834568	445.944026	9.159296
7.398812	444.063114	9.164314
6.918564	445.545789	9.169331
7.123779	444.368059	9.174349
7.117957	440.152845	9.179367
7.061788	447.763822	9.184384
7.209104	443.183793	9.189402
7.246390	439.911707	9.194419
7.357746	443.804202	9.199437
7.322958	450.521908	9.204455
7.430351	436.278901	9.209472
7.078295	422.773755	9.214490
6.985597	426.537274	9.219507
7.658715	428.650266	9.224525
6.975669	428.132410	9.229543
6.751874	429.410803	9.234560
7.194175	432.153241	9.239578
7.323461	440.987992	9.244595
7.426658	443.041961	9.249613
7.185522	442.896671	9.254631
7.327073	445.787217	9.259648
7.271109	451.706679	9.264666
7.127942	454.935321	9.269683
7.538192	448.723592	9.274701
6.895265	449.572203	9.279719
6.947074	451.646847	9.284736
6.975722	455.823698	9.289754
7.043788	446.961100	9.294771
7.431102	445.603363	9.299789
7.174916	451.207062	9.304807
7.075429	447.827019	9.309824
7.254246	442.194343	9.314842
6.969346	453.101054	9.319859
7.420066	452.465518	9.324877
7.164482	450.028256	9.329895
7.339564	441.398198	9.334912
7.257638	446.475984	9.339930
6.811511	438.678549	9.344947
7.097554	445.036720	9.349965
7.387072	469.438973	9.354983
7.469098	475.381003	9.360000
7.735351	474.752277	9.365018
7.712144	465.143432	9.370035
7.772877	448.089634	9.375053
7.751923	447.221891	9.380071
7.503153	437.563197	9.385088
7.296297	448.113700	9.390106
7.226613	453.915394	9.395123
7.047098	445.460810	9.400141
7.683471	440.741041	9.405159
7.351608	452.216834	9.410176
7.280220	446.686474	9.415194
7.364554	446.944619	9.420211
7.205312	444.299762	9.425229
7.795872	448.319145	9.430247
7.635389	457.555906	9.435264
7.287857	445.896152	9.440282
7.111314	452.430944	9.445299
7.901019	458.495615	9.450317
7.672400	456.814665	9.455335
7.705666	448.979984	9.460352
7.566817	442.718592	9.465370
7.638604	443.076530	9.470387
7.538370	439.267423	9.475405
7.534888	445.753007	9.480423
7.545032	435.880180	9.485440
7.761708	439.554205	9.490458
7.306252	443.791124	9.495475
7.333692	448.034434	9.500493
7.328496	447.479798	9.505511
7.779389	458.889757	9.510528
7.879553	443.082622	9.515546
7.382368	449.598224	9.520563
7.330811	443.070695	9.525581
7.462246	449.958013	9.530599
7.377542	467.428898	9.535616
8.000658	462.307263	9.540634
7.734849	468.568873	9.545651
7.640158	470.123682	9.550669
7.900731	462.269159	9.555687
7.451870	459.294143	9.560704
7.905991	455.704284	9.565722
7.478342	451.750817	9.570739
7.670069	455.334081	9.575757
8.139310	461.452119	9.580775
7.679166	454.127081	9.585792
7.580388	444.842507	9.590810
7.500017	448.518895	9.595827
7.586847	448.912345	9.600845
7.803196	458.367770	9.605863
7.788327	460.497043	9.610880
7.640697	450.434337	9.615898
7.697832	460.656312	9.620915
7.623035	465.789790	9.625933
7.779514	471.723309	9.630951
7.735285	479.805792	9.635968
7.753907	467.504840	9.640986
7.791030	471.181757	9.646003
7.922975	471.495557	9.651021
8.244730	477.996466	9.656039
7.725103	459.752348	9.661056
7.634221	442.365710	9.666074
7.607853	457.880345	9.671091
7.511013	459.460736	9.676109
8.090237	467.142579	9.681127
7.433645	486.558673	9.686144
7.474818	471.025839	9.691162
7.494425	470.855475	9.696179
7.521644	473.189590	9.701197
7.792412	474.425212	9.706215
7.708410	476.603188	9.711232
7.805875	469.613649	9.716250
7.981005	480.969001	9.721267
7.664364	473.324830	9.726285
7.626502	475.082171	9.731303
7.723531	475.158448	9.736320
7.989606	471.039480	9.741338
8.087885	478.228645	9.746355
7.687523	475.242872	9.751373
7.936064	471.584236	9.756391
7.547302	477.868269	9.761408
7.811909	484.589570	9.766426
7.934214	495.211603	9.771443
8.050229	496.622950	9.776461
8.408077	493.745591	9.781479
8.086851	491.422749	9.786496
8.121465	476.190737	9.791514
7.913369	479.820871	9.796531
8.128707	476.344159	9.801549
8.089389	481.229089	9.806567
7.894270	484.538459	9.811584
7.880493	474.016117	9.816602
7.984277	481.305405	9.821619
8.048447	478.098527	9.826637
8.157786	468.080754	9.831655
7.977208	476.490709	9.836672
8.093406	474.758887	9.841690
8.191804	486.195691	9.846707
8.156910	471.337486	9.851725
7.698080	475.268832	9.856743
7.648404	485.914650	9.861760
8.234491	493.330345	9.866778
8.143455	501.461197	9.871795
8.319734	497.488834	9.876813
7.955112	495.011847	9.881831
7.819877	492.631462	9.886848
7.904282	497.235082	9.891866
8.235412	502.503783	9.896883
8.053277	498.644380	9.901901
8.425856	501.981570	9.906919
8.184338	502.170850	9.911936
8.101118	498.513697	9.916954
7.772328	508.969733	9.921971
7.981118	515.172778	9.926989
8.419038	496.990031	9.932007
7.999080	517.811267	9.937024
8.245537	507.213417	9.942042
8.452356	505.823996	9.947059
8.573440	503.933618	9.952077
8.247695	502.529810	9.957095
8.049035	497.114049	9.962112
8.483016	498.986811	9.967130
8.623977	493.659848	9.972147
8.174517	499.142367	9.977165
8.318179	481.150905	9.982183
8.283784	492.636921	9.987200
8.314785	492.748790	9.992218
8.190447	484.809399	9.997235
8.274052	491.439143	10.002253
8.391436	491.180876	10.007271
8.001099	499.118784	10.012288
8.240123	486.937917	10.017306
8.166615	490.774182	10.022323
8.163310	500.750033	10.027341
8.437019	501.230967	10.032359
8.091929	502.629354	10.037376
8.254161	496.204008	10.042394
8.031783	499.129492	10.047411
8.243808	501.639781	10.052429
8.403276	497.537510	10.057447
8.384278	502.583362	10.062464
8.371674	501.250410	10.067482
8.700965	495.247008	10.072499
8.603844	502.299542	10.077517
8.563582	498.604101	10.082535
8.343936	502.901916	10.087552
8.297051	496.215847	10.092570
8.481663	494.378632	10.097587
8.443315	504.798627	10.102605
8.812791	495.330209	10.107623
8.618179	497.197318	10.112640
8.764642	494.539270	10.117658
8.585560	493.759415	10.122675
8.300238	504.650445	10.127693
8.637194	495.278640	10.132711
8.521261	500.648943	10.137728
8.436658	500.826261	10.142746
8.489675	487.241821	10.147763
8.441061	499.181343	10.152781
8.200006	500.793801	10.157799
8.314268	504.644829	10.162816
8.496510	501.564613	10.167834
8.550137	497.441056	10.172851
8.544652	500.455633	10.177869
8.610391	496.033536	10.182887
8.244989	499.817708	10.187904
8.532053	490.892373	10.192922
8.715003	500.709655	10.197939
8.473262	499.422072	10.202957
8.788250	487.630086	10.207975
8.437066	492.456586	10.212992
8.879439	492.926873	10.218010
8.664499	498.066538	10.223027
8.355321	494.719341	10.228045
8.738661	488.925219	10.233063
8.666100	503.468845	10.238080
8.734866	494.274758	10.243098
8.617946	490.512435	10.248115
8.317648	500.165594	10.253133
8.847004	490.949835	10.258151
8.604135	502.812500	10.263168
8.310584	495.341424	10.268186
8.579619	495.131979	10.273203
8.297111	501.462488	10.278221
8.429786	489.850541	10.283239
8.754068	511.593408	10.288256
9.024372	520.810042	10.293274
8.831673	502.189614	10.298291
8.519247	510.677046	10.303309
8.985730	516.334793	10.308327
8.551394	506.522101	10.313344
8.635991	508.392802	10.318362
9.018480	515.196629	10.323379
8.934145	514.837425	10.328397
8.662337	504.895128	10.333415
8.947400	505.740353	10.338432
8.627694	504.862612	10.343450
8.792055	510.416217	10.348467
8.827820	530.907293	10.353485
8.896972	517.096242	10.358503
9.041054	518.986025	10.363520
8.629407	520.833494	10.368538
8.875274	521.031617	10.373555
8.640805	531.261451	10.378573
8.766090	523.746831	10.383591
8.742765	527.193392	10.388608
8.617941	521.933310	10.393626
9.165453	521.481420	10.398643
8.871792	531.105153	10.403661
9.049034	529.695118	10.408679
8.769422	524.039570	10.413696
9.190878	531.310664	10.418714
8.787920	525.178986	10.423731
8.896669	520.188418	10.428749
8.992555	526.611126	10.433767
8.959862	524.653322	10.438784
8.838141	517.246832	10.443802
9.270998	517.952138	10.448819
8.824581	525.677940	10.453837
9.184718	517.372297	10.458855
9.433878	519.529636	10.463872
8.961978	523.532467	10.468890
8.911063	530.246418	10.473907
8.623158	520.028927	10.478925
9.265968	522.099343	10.483943
9.117353	527.891337	10.488960
8.949843	526.611056	10.493978
9.141925	520.515535	10.498995
9.270424	532.209581	10.504013
9.309188	529.612583	10.509031
9.415439	519.364894	10.514048
9.280379	512.998744	10.519066
9.166507	508.907739	10.524083
8.867950	510.163138	10.529101
9.074095	506.063019	10.534119
9.218261	524.021957	10.539136
9.043391	509.690575	10.544154
9.249857	512.851824	10.549171
9.169594	528.273980	10.554189
9.067209	525.134215	10.559207
9.012363	520.270263	10.564224
9.074937	522.819750	10.569242
9.359694	515.949170	10.574259
9.072744	524.539913	10.579277
9.487455	525.648845	10.584295
9.257487	531.576661	10.589312
9.099891	523.711891	10.594330
9.416987	525.009685	10.599347
8.773656	531.567149	10.604365
9.065752	516.853331	10.609383
9.500218	523.955128	10.614400
9.107842	520.586247	10.619418
9.224055	521.603093	10.624435
9.227648	520.987118	10.629453
9.113421	523.800989	10.634471
8.986551	520.283212	10.639488
8.949241	522.217195	10.644506
9.257193	514.885395	10.649523
9.199099	514.809254	10.654541
9.252519	518.149116	10.659559
9.428179	519.049352	10.664576
9.166775	528.033721	10.669594
9.292352	514.595680	10.674611
9.182583	514.259395	10.679629
9.013241	521.771372	10.684647
9.402404	538.085652	10.689664
9.279813	539.682708	10.694682
9.767904	541.862573	10.699699
9.407431	545.822705	10.704717
9.604662	545.665535	10.709735
9.590749	539.902081	10.714752
9.270455	535.070249	10.719770
9.351698	527.840235	10.724787
9.481801	530.129837	10.729805
9.431826	536.887823	10.734823
9.743557	541.866088	10.739840
9.154440	532.708787	10.744858
9.356201	532.036516	10.749875
9.247120	546.346060	10.754893
9.787987	539.321736	10.759911
9.846416	545.033959	10.764928
9.516929	550.469295	10.769946
9.812950	538.162700	10.774963
9.282504	525.524862	10.779981
9.172051	526.129103	10.784999
9.623196	536.832181	10.790016
9.416499	542.573320	10.795034
9.773023	532.523094	10.800051
9.803297	545.838826	10.805069
9.765241	540.934369	10.810087
9.796176	535.410040	10.815104
9.466243	534.047911	10.820122
9.690661	536.341671	10.825139
9.371733	540.099634	10.830157
9.517615	548.004041	10.835175
9.682846	543.487450	10.840192
9.423160	547.324495	10.845210
9.943021	535.099595	10.850227
9.710318	534.959294	10.855245
9.678552	534.352014	10.860263
9.742949	535.818788	10.865280
9.466636	537.449396	10.870298
9.774622	540.304413	10.875315
9.623733	535.048411	10.880333
9.867477	540.135157	10.885351
9.690940	538.108372	10.890368
9.584254	551.473969	10.895386
9.847385	535.088958	10.900403
10.120802	537.441312	10.905421
9.874787	543.630420	10.910439
9.708049	542.728710	10.915456
9.799517	548.801827	10.920474
9.905385	548.078309	10.925491
9.561107	551.051304	10.930509
9.679366	547.763356	10.935527
9.765237	553.067343	10.940544
9.767159	548.532157	10.945562
9.556824	542.108364	10.950579
10.020863	541.338195	10.955597
9.814412	547.868240	10.960615
9.954998	532.824701	10.965632
9.795367	548.685339	10.970650
10.023051	540.602407	10.975667
10.087216	546.165411	10.980685
9.893194	540.442799	10.985703
10.108397	538.736485	10.990720
10.071302	543.232923	10.995738
9.885503	547.979877	11.000755
10.294019	542.468969	11.005773
9.746681	534.131934	11.010791
9.877252	538.264434	11.015808
9.605368	545.136086	11.020826
9.669274	544.381274	11.025843
9.867320	534.049767	11.030861
9.690711	539.429589	11.035879
9.763347	532.964618	11.040896
9.714016	541.638059	11.045914
10.107468	540.620176	11.050931
9.935960	543.916391	11.055949
10.160851	561.714398	11.060967
10.047846	554.391733	11.065984
9.882728	561.997738	11.071002
10.160746	557.712778	11.076019
10.161961	570.824801	11.081037
9.980065	576.953382	11.086055
10.410220	568.327478	11.091072
10.067415	565.149636	11.096090
10.059626	545.212635	11.101107
10.350617	548.306999	11.106125
9.882093	549.399685	11.111143
10.086136	545.233615	11.116160
10.157974	558.309317	11.121178
10.355421	569.257289	11.126195
10.504510	556.648657	11.131213
10.109960	554.204753	11.136231
10.246094	552.766443	11.141248
10.126367	548.632166	11.146266
9.921130	534.576917	11.151283
10.150217	543.342434	11.156301
10.222693	561.337889	11.161319
10.485799	560.599201	11.166336
10.109363	563.157518	11.171354
10.302721	560.921298	11.176371
10.563663	565.153297	11.181389
10.211108	560.752542	11.186407
10.389173	554.495105	11.191424
10.279830	559.072294	11.196442
10.268479	555.233457	11.201459
9.986217	552.311217	11.206477
10.191790	571.787976	11.211495
10.839092	565.741036	11.216512
10.560188	565.497521	11.221530
10.148361	548.258895	11.226547
10.682792	555.606971	11.231565
10.175773	559.984538	11.236583
10.539052	559.498397	11.241600
10.380101	565.023781	11.246618
10.598530	559.432199	11.251635
10.564474	547.167847	11.256653
10.098050	544.271306	11.261671
10.464954	552.772240	11.266688
10.266591	571.965154	11.271706
10.379909	567.664972	11.276723
10.328909	563.011843	11.281741
9.947230	571.144084	11.286759
10.712357	580.885974	11.291776
10.794004	576.480300	11.296794
10.397461	558.579711	11.301811
10.836181	564.443793	11.306829
10.425089	560.475084	11.311847
10.531152	574.744630	11.316864
10.292549	571.020290	11.321882
10.602910	570.198460	11.326899
10.815788	556.267031	11.331917
10.332344	564.550911	11.336935
10.462051	564.858752	11.341952
10.480456	573.499504	11.346970
10.421102	566.969996	11.351987
10.971809	560.565810	11.357005
10.591282	568.312864	11.362023
10.699476	566.358228	11.367040
10.497323	571.341278	11.372058
10.563988	568.058255	11.377075
10.682591	571.561482	11.382093
10.515052	565.635899	11.387111
10.652941	567.097472	11.392128
10.696546	565.074061	11.397146
10.310176	555.881826	11.402163
10.377628	561.494812	11.407181
10.391626	564.424297	11.412199
10.627633	576.868382	11.417216
10.991306	589.267226	11.422234
10.701385	580.296550	11.427251
10.600199	572.192548	11.432269
10.827265	587.352010	11.437287
11.059912	584.301752	11.442304
11.279337	575.863495	11.447322
10.791379	575.655891	11.452339
10.945940	564.494899	11.457357
10.716428	573.991841	11.462375
10.856791	563.028732	11.467392
10.790660	565.352240	11.472410
10.472773	576.425140	11.477427
10.755319	563.085544	11.482445
10.686666	584.766990	11.487463
11.046931	587.746367	11.492480
11.331389	592.160879	11.497498
10.816624	576.992766	11.502515
10.761895	563.349411	11.507533
10.909511	574.623927	11.512551
11.216110	572.994807	11.517568
11.255891	564.733024	11.522586
10.737977	565.476846	11.527603
11.001218	557.634486	11.532621
10.685518	563.263324	11.537639
10.560104	567.940862	11.542656
11.084863	589.292655	11.547674
10.957797	596.204753	11.552691
11.130506	587.628644	11.557709
11.415960	590.692326	11.562727
11.403722	583.713620	11.567744
10.721645	571.402461	11.572762
11.147840	574.333637	11.577779
11.024161	569.770788	11.582797
10.960951	577.360833	11.587815
11.467527	580.607616	11.592832
11.231222	568.226616	11.597850
10.717021	567.098481	11.602867
11.127163	577.994198	11.607885
11.065778	589.411922	11.612903
11.339675	591.448630	11.617920
11.250489	584.766000	11.622938
11.257804	574.357058	11.627955
11.112669	568.699360	11.632973
10.821591	576.142072	11.637991
11.343506	579.471657	11.643008
11.463436	593.139448	11.648026
11.210654	582.095916	11.653043
11.360574	582.993876	11.658061
10.866589	579.246432	11.663079
10.843940	589.884921	11.668096
10.950666	592.361229	11.673114
10.674435	588.907866	11.678131
11.274723	583.322718	11.683149
11.321666	588.509740	11.688167
11.361237	587.932306	11.693184
11.126397	585.652720	11.698202
11.325001	603.903009	11.703219
11.282131	590.254619	11.708237
11.229540	589.852570	11.713255
11.426923	594.094534	11.718272
11.678471	591.268530	11.723290
11.184182	590.689535	11.728307
11.572995	591.266046	11.733325
11.435546	592.025997	11.738343
11.203716	598.253926	11.743360
11.388466	598.281746	11.748378
11.189020	599.130305	11.753395
11.199266	589.696031	11.758413
11.444919	596.735923	11.763431
11.284235	599.957868	11.768448
11.245351	602.049896	11.773466
11.376143	611.297903	11.778483
11.881290	619.325931	11.783501
11.774149	610.740010	11.788519
11.582460	602.697512	11.793536
11.321948	593.226763	11.798554
11.076577	596.843827	11.803571
11.429767	600.089400	11.808589
11.709792	607.388996	11.813607
11.492306	612.914099	11.818624
11.623713	616.443731	11.823642
11.589344	619.333467	11.828659
11.826921	612.833157	11.833677
11.726927	616.443226	11.838695
11.860147	615.279921	11.843712
11.790510	609.234844	11.848730
11.456034	591.529623	11.853747
11.789943	595.526136	11.858765
11.827778	600.556799	11.863783
11.623554	599.638869	11.868800
11.609188	592.000934	11.873818
11.728747	589.962464	11.878835
11.850459	586.607697	11.883853
11.729162	589.242806	11.888871
11.259718	595.157672	11.893888
11.988825	599.190096	11.898906
11.646237	612.447534	11.903923
11.932386	616.899657	11.908941
12.073564	618.408056	11.913959
11.723695	597.091866	11.918976
11.549818	587.178361	11.923994
11.750765	606.084687	11.929011
11.974445	600.886742	11.934029
11.797491	614.004621	11.939047
11.981736	609.702784	11.944064
11.958334	595.997691	11.949082
11.483881	606.375622	11.954099
11.690918	608.615310	11.959117
11.877614	611.587172	11.964135
11.930226	610.351291	11.969152
12.032630	598.826067	11.974170
12.040487	612.542990	11.979187
12.237667	607.794161	11.984205
12.141181	616.351950	11.989223
11.913997	609.227032	11.994240
12.058931	597.881336	11.999258
11.681659	610.863342	12.004275
11.985561	604.803921	12.009293
11.999874	615.007447	12.014311
12.093267	620.865695	12.019328
12.006525	609.079767	12.024346
12.101497	610.712168	12.029363
12.079636	611.655980	12.034381
12.040007	613.741814	12.039399
11.626964	620.932256	12.044416
12.322706	610.945601	12.049434
12.227665	616.612466	12.054451
11.941563	609.613543	12.059469
12.188199	603.367436	12.064487
12.034566	610.217430	12.069504
12.424464	606.063251	12.074522
11.857780	605.855358	12.079539
12.133465	604.319441	12.084557
12.121207	602.506748	12.089575
11.640966	604.166158	12.094592
12.270455	610.896609	12.099610
12.451478	618.593571	12.104627
12.113714	605.751918	12.109645
11.984373	616.571240	12.114663
11.867314	613.935528	12.119680
12.036543	610.185150	12.124698
11.670853	614.316526	12.129715
11.854882	602.756420	12.134733
12.439879	617.291786	12.139751
12.512409	637.105042	12.144768
12.663965	625.120821	12.149786
12.149875	619.489358	12.154803
11.976334	609.970260	12.159821
12.297658	621.836124	12.164839
12.268266	636.133254	12.169856
12.869237	634.319152	12.174874
12.236321	625.364324	12.179891
12.355814	627.302152	12.184909
12.593302	629.098418	12.189927
12.143981	625.953032	12.194944
12.432400	627.362623	12.199962
12.747972	640.479092	12.204979
12.527506	633.589796	12.209997
12.584830	613.314314	12.215015
12.508541	622.067756	12.220032
12.490400	612.581114	12.225050
12.108502	616.014446	12.230067
12.373553	629.978262	12.235085
12.938460	626.803355	12.240103
12.348291	626.138396	12.245120
12.715392	621.006336	12.250138
12.459507	631.974882	12.255155
12.504226	629.859771	12.260173
12.679109	634.884750	12.265191
12.688745	644.615658	12.270208
12.798325	633.695199	12.275226
12.510832	621.997520	12.280243
12.422935	619.786425	12.285261
12.808901	627.129390	12.290279
12.619656	633.208649	12.295296
12.593836	624.127144	12.300314
12.827930	636.770385	12.305331
12.684203	632.993297	12.310349
12.871259	629.053930	12.315367
12.822808	635.111130	12.320384
12.792739	621.495425	12.325402
12.505661	618.154208	12.330419
12.655376	620.320829	12.335437
13.011762	625.939057	12.340455
12.698760	618.262695	12.345472
12.137234	615.213787	12.350490
12.562994	625.857780	12.355507
12.711793	642.459123	12.360525
13.082354	639.810123	12.365543
12.924034	644.710587	12.370560
13.036628	644.639260	12.375578
13.266804	638.629248	12.380595
13.015047	640.057203	12.385613
13.058891	636.916597	12.390631
12.565481	624.105629	12.395648
12.791767	626.515872	12.400666
12.762506	627.946835	12.405683
13.171351	638.454631	12.410701
13.062387	622.831580	12.415719
12.814467	630.472679	12.420736
12.447701	633.335602	12.425754
12.856814	631.983903	12.430771
12.833970	637.030395	12.435789
13.226689	631.723906	12.440807
13.034771	646.567214	12.445824
12.711999	641.338111	12.450842
12.772933	639.693827	12.455859
13.046700	635.160208	12.460877
13.372451	627.920246	12.465895
13.079113	635.173989	12.470912
13.241065	632.093774	12.475930
13.078160	625.015582	12.480947
13.005858	634.339603	12.485965
13.153307	630.570542	12.490983
12.794484	644.676299	12.496000
12.949475	633.512040	12.501018
13.134565	636.496782	12.506035
12.811534	642.467618	12.511053
13.237705	630.500327	12.516071
12.910520	633.243440	12.521088
13.103856	626.570178	12.526106
13.190912	631.643630	12.531123
12.883507	633.493712	12.536141
13.179083	640.885559	12.541159
12.987508	654.188794	12.546176
13.334858	657.798209	12.551194
13.647791	659.746759	12.556211
13.461877	663.007382	12.561229
13.482459	653.836542	12.566247
13.536763	654.771578	12.571264
13.201249	643.621049	12.576282
13.258139	646.433375	12.581299
13.145417	656.697854	12.586317
13.571755	649.953363	12.591335
13.591153	651.054813	12.596352
13.201320	641.086751	12.601370
13.354399	639.301799	12.606387
13.188507	651.228239	12.611405
13.510010	651.417669	12.616423
13.439622	658.194679	12.621440
13.707038	651.623409	12.626458
13.378882	653.101204	12.631475
13.514373	651.672455	12.636493
13.436530	656.910606	12.641511
13.317502	668.892832	12.646528
13.176199	661.549310	12.651546
13.375888	658.620967	12.656563
13.201675	653.220262	12.661581
13.324576	660.948440	12.666599
13.126120	660.241040	12.671616
13.619612	662.533684	12.676634
13.448281	656.498212	12.681651
13.288586	662.011119	12.686669
13.769934	670.008186	12.691687
13.902398	672.496252	12.696704
13.596669	669.069585	12.701722
13.712719	653.755234	12.706739
13.450554	659.549282	12.711757
14.033732	663.847582	12.716775
13.454000	670.284679	12.721792
13.781971	669.930299	12.726810
14.089931	675.628714	12.731827
13.618476	671.454843	12.736845
13.662476	667.361157	12.741863
13.987982	664.031249	12.746880
13.784322	655.570882	12.751898
13.480203	649.351091	12.756915
13.839154	670.994047	12.761933
13.914625	671.465022	12.766951
13.938484	682.446573	12.771968
14.020105	669.977820	12.776986
14.042712	658.039028	12.782003
13.751272	658.078341	12.787021
13.545604	655.983523	12.792039
13.649698	660.950174	12.797056
13.741343	672.441804	12.802074
14.095937	679.726590	12.807091
14.083980	682.439256	12.812109
14.031203	677.066854	12.817127
13.979470	681.568776	12.822144
14.137336	683.030385	12.827162
14.582266	663.887007	12.832179
14.102541	663.646554	12.837197
13.869483	654.165160	12.842215
13.701991	654.977157	12.847232
13.504024	652.221572	12.852250
13.985476	664.712469	12.857267
14.160507	676.705431	12.862285
14.009947	673.134532	12.867303
14.030614	671.913119	12.872320
14.116580	679.593443	12.877338
14.323050	674.855764	12.882355
14.007564	684.104304	12.887373
13.993347	677.024886	12.892391
14.096975	674.376678	12.897408
13.959779	674.199321	12.902426
14.027237	670.830948	12.907443
13.861535	687.289106	12.912461
13.964770	668.978742	12.917479
13.849510	672.354529	12.922496
13.704431	683.671818	12.927514
14.193495	684.144263	12.932531
14.298534	704.097665	12.937549
14.304150	706.059656	12.942567
14.453415	704.426773	12.947584
14.186926	705.834951	12.952602
14.580721	701.159433	12.957619
14.606523	701.631879	12.962637
14.629355	697.787655	12.967655
14.196815	684.784069	12.972672
14.390772	688.408057	12.977690
14.466839	682.561031	12.982707
14.298678	690.265398	12.987725
14.504737	693.612935	12.992743
14.651355	694.284202	12.997760
14.248914	688.591041	13.002778
14.434547	680.662958	13.007795
14.320438	694.982876	13.012813
14.279667	695.080745	13.017831
14.616686	703.763158	13.022848
14.337686	707.761053	13.027866
14.759514	701.282336	13.032883
14.807679	708.299566	13.037901
14.645919	705.762362	13.042919
14.563446	701.887299	13.047936
14.832751	705.000868	13.052954
14.766574	700.577299	13.057971
14.297295	686.493873	13.062989
14.363240	697.260556	13.068007
14.695544	706.827334	13.073024
14.651519	710.441276	13.078042
14.743163	696.512954	13.083059
14.734304	699.439731	13.088077
14.641062	704.282677	13.093095
14.771025	710.706424	13.098112
14.513163	713.018966	13.103130
14.641625	693.817843	13.108147
14.620972	694.909793	13.113165
14.544432	701.384825	13.118183
14.658501	699.006377	13.123200
14.407991	704.132740	13.128218
14.993074	699.285241	13.133235
15.083739	714.661842	13.138253
14.787400	702.918159	13.143271
15.063452	702.152191	13.148288
14.869286	711.874042	13.153306
14.900298	695.301191	13.158323
14.759908	700.871046	13.163341
14.950779	702.336952	13.168359
14.919159	700.580932	13.173376
15.073708	703.122346	13.178394
14.986016	699.431138	13.183411
14.867445	705.155366	13.188429
14.825205	700.712268	13.193447
14.814218	702.127750	13.198464
14.667496	705.618926	13.203482
14.800430	697.127892	13.208499
14.885046	702.170189	13.213517
15.115652	696.800718	13.218535
15.104762	705.070584	13.223552
14.815267	695.875721	13.228570
15.087292	713.417187	13.233587
15.353595	723.391946	13.238605
15.526693	714.686327	13.243623
15.185215	700.074782	13.248640
14.871692	701.550289	13.253658
15.222942	698.222653	13.258675
15.297089	700.274891	13.263693
15.189371	693.481515	13.268711
15.344342	699.238622	13.273728
14.996640	707.330887	13.278746
14.954608	702.685784	13.283763
15.389135	722.726439	13.288781
15.163620	724.431156	13.293799
15.410143	718.847745	13.298816
15.281662	722.815749	13.303834
15.600937	713.367705	13.308851
15.432803	719.945458	13.313869
15.284890	707.660965	13.318887
15.152744	698.236320	13.323904
15.319725	722.487706	13.328922
15.216021	724.327972	13.333939
15.356536	734.429742	13.338957
15.277719	730.932797	13.343975
15.536658	717.820847	13.348992
15.134839	730.746826	13.354010
15.328708	720.450580	13.359027
15.319773	728.227845	13.364045
14.994985	729.799793	13.369063
14.969386	724.120161	13.374080
15.145563	729.552063	13.379098
15.555434	732.678327	13.384115
15.550608	754.242682	13.389133
15.625713	752.457312	13.394151
16.046810	736.978330	13.399168
15.586289	735.280039	13.404186
15.794639	724.435568	13.409203
15.752158	715.987787	13.414221
15.363503	713.479820	13.419239
15.630196	725.237548	13.424256
15.446733	726.585382	13.429274
15.785537	724.010773	13.434291
15.836974	730.465765	13.439309
15.564303	728.851651	13.444327
15.881692	723.604275	13.449344
15.609606	728.298524	13.454362
15.813968	719.445994	13.459379
15.680946	723.095973	13.464397
15.706786	732.464628	13.469415
15.844881	728.179461	13.474432
15.892096	747.138425	13.479450
15.706105	739.227516	13.484467
15.761019	745.350609	13.489485
15.699195	750.807184	13.494503
16.555752	745.229172	13.499520
15.897369	732.917344	13.504538
15.354001	732.844650	13.509555
16.103209	740.073946	13.514573
15.932343	746.560618	13.519591
16.168046	740.401383	13.524608
16.146737	743.658322	13.529626
15.886002	732.912588	13.534643
15.950259	728.042542	13.539661
16.053547	745.518959	13.544679
16.089104	738.444341	13.549696
15.797259	740.355111	13.554714
15.938640	741.888736	13.559731
16.099760	739.622831	13.564749
15.861777	741.910171	13.569767
16.171720	739.377951	13.574784
16.103253	744.447401	13.579802
15.858513	747.215483	13.584819
15.978053	745.647215	13.589837
16.221660	742.478447	13.594855
16.250727	746.674236	13.599872
16.100839	757.992326	13.604890
16.099261	746.142471	13.609907
15.975214	743.804480	13.614925
15.870854	751.442071	13.619943
16.376697	740.800288	13.624960
16.316883	742.876676	13.629978
16.586354	745.235988	13.634995
16.626882	747.233539	13.640013
16.358642	747.010442	13.645031
16.141915	738.615198	13.650048
16.429189	748.949603	13.655066
16.062535	745.163238	13.660083
16.184711	738.535796	13.665101
15.705981	742.492409	13.670119
16.335783	751.188933	13.675136
16.484683	763.536343	13.680154
16.453094	766.630795	13.685171
16.695002	765.153805	13.690189
16.267601	764.292924	13.695207
16.801896	756.139765	13.700224
16.474309	763.518846	13.705242
16.326048	765.599628	13.710259
16.765731	759.525192	13.715277
16.663584	773.846455	13.720295
16.970646	764.472881	13.725312
17.172281	758.729234	13.730330
16.531848	751.959340	13.735347
16.480563	738.902291	13.740365
16.381109	740.360040	13.745383
16.770353	734.539668	13.750400
16.684957	735.013759	13.755418
16.413845	728.141828	13.760435
16.705961	740.971712	13.765453
17.030559	758.268300	13.770471
16.685952	753.755797	13.775488
16.440055	744.307925	13.780506
16.739326	757.354451	13.785523
16.867420	757.905545	13.790541
16.599722	764.502070	13.795559
16.744628	767.104964	13.800576
16.577042	761.905160	13.805594
16.584644	763.740614	13.810611
16.331489	762.827185	13.815629
16.354395	753.924173	13.820647
16.796395	757.102212	13.825664
16.887120	760.609845	13.830682
16.751853	762.764329	13.835699
16.718316	763.132464	13.840717
16.807837	767.126282	13.845735
17.111187	781.415576	13.850752
17.222593	784.579145	13.855770
17.055553	770.167430	13.860787
17.116539	762.012687	13.865805
16.874256	766.273086	13.870823
17.122115	767.635395	13.875840
17.089240	773.942666	13.880858
16.860666	788.599331	13.885875
17.308671	783.400900	13.890893
17.254718	794.691358	13.895911
17.241364	775.417693	13.900928
17.224621	768.474335	13.905946
17.498580	770.192317	13.910963
16.890790	759.447294	13.915981
16.947293	756.841171	13.920999
17.269384	771.462037	13.926016
17.497782	779.274723	13.931034
17.240343	777.954865	13.936051
17.365291	768.988520	13.941069
17.153193	766.929410	13.946087
17.106332	777.496066	13.951104
17.517147	776.819434	13.956122
17.283419	782.555418	13.961139
17.433699	777.618232	13.966157
17.691688	788.629437	13.971175
17.156770	775.064311	13.976192
17.584579	776.076533	13.981210
17.354825	784.333390	13.986227
17.243304	782.577257	13.991245
17.230251	785.132319	13.996263
17.261777	774.798362	14.001280
17.448552	781.683449	14.006298
17.088614	793.302715	14.011315
17.251732	781.275554	14.016333
17.038070	783.625360	14.021351
17.605203	778.591304	14.026368
17.480854	776.000891	14.031386
17.159694	783.341104	14.036403
17.348328	782.449974	14.041421
17.738708	794.658584	14.046439
17.928989	805.642539	14.051456
18.095117	796.354146	14.056474
17.577697	785.389820	14.061491
17.880538	785.102492	14.066509
17.837002	781.114014	14.071527
17.748042	781.664403	14.076544
17.564025	780.695960	14.081562
17.373150	788.744755	14.086579
17.978606	791.026185	14.091597
18.043755	798.899171	14.096615
17.860738	787.813022	14.101632
17.764370	786.300668	14.106650
17.746584	789.348780	14.111667
17.849514	776.138153	14.116685
17.694199	786.983739	14.121703
18.085023	791.684594	14.126720
18.015922	783.493418	14.131738
17.632514	786.933331	14.136755
18.231798	790.449651	14.141773
17.880922	787.787431	14.146791
17.968737	795.622151	14.151808
18.196707	800.231758	14.156826
18.198311	798.681963	14.161843
17.998315	780.106569	14.166861
18.066494	777.220902	14.171879
17.672192	777.453058	14.176896
18.177322	784.054737	14.181914
18.012706	798.546753	14.186931
18.322456	798.330926	14.191949
18.446930	806.125193	14.196967
18.289467	784.734451	14.201984
18.181748	785.414012	14.207002
17.812601	783.190158	14.212019
18.123281	784.318562	14.217037
17.874125	804.245521	14.222055
18.096067	802.112090	14.227072
18.394303	798.432979	14.232090
18.303647	808.141820	14.237107
18.550251	800.055807	14.242125
18.199335	809.436196	14.247143
18.135931	809.291457	14.252160
18.442454	797.156609	14.257178
18.259643	802.108290	14.262195
18.587559	798.247803	14.267213
18.360582	799.665576	14.272231
18.545718	802.994322	14.277248
18.598973	795.560301	14.282266
18.465756	805.364172	14.287283
18.777599	801.604033	14.292301
18.732208	806.452133	14.297319
18.405714	799.462619	14.302336
18.582664	806.346100	14.307354
18.500084	805.885628	14.312371
18.576724	798.040841	14.317389
18.620084	811.679771	14.322407
18.491487	810.320789	14.327424
18.529299	795.959008	14.332442
18.296335	804.437284	14.337459
18.452018	806.640863	14.342477
18.329090	802.917285	14.347495
18.378057	805.128116	14.352512
18.243413	805.821363	14.357530
18.645949	809.318021	14.362547
18.360367	800.403359	14.367565
18.157272	814.516407	14.372583
18.465138	821.060644	14.377600
18.938506	826.884672	14.382618
18.852331	828.914707	14.387635
18.807173	824.109115	14.392653
18.768498	822.149060	14.397671
18.677864	833.524186	14.402688
18.834656	826.458940	14.407706
18.966835	830.805852	14.412723
18.754120	834.035992	14.417741
18.559486	825.886556	14.422759
18.625213	825.128290	14.427776
18.842354	821.916319	14.432794
18.609402	833.361079	14.437811
18.881570	847.850974	14.442829
19.213327	842.077445	14.447847
18.893951	858.449383	14.452864
19.219321	849.214909	14.457882
18.993101	858.304384	14.462899
19.304029	854.026822	14.467917
19.343446	856.109766	14.472935
19.615636	849.193691	14.477952
19.717572	835.197375	14.482970
19.388816	827.384535	14.487987
19.376273	823.365945	14.493005
19.149812	815.631756	14.498023
19.611370	825.424501	14.503040
19.623316	819.000494	14.508058
19.292079	822.773068	14.513075
19.339106	822.882428	14.518093
19.081094	821.423800	14.523111
19.188034	824.335610	14.528128
19.598575	815.242444	14.533146
19.376498	813.481540	14.538163
19.214306	812.654843	14.543181
19.254218	820.800037	14.548199
19.189715	820.074800	14.553216
19.170314	813.961821	14.558234
19.165758	825.159352	14.563251
19.186280	816.537550	14.568269
19.523821	815.648334	14.573287
19.115999	819.840008	14.578304
19.610767	832.647675	14.583322
19.882319	847.945557	14.588339
19.766564	836.709982	14.593357
19.615355	829.513111	14.598375
19.357353	829.528250	14.603392
19.881171	834.012618	14.608410
19.588327	839.619026	14.613427
19.729595	839.035118	14.618445
19.939124	820.499660	14.623463
19.471940	829.118787	14.628480
19.643407	826.674524	14.633498
19.598979	838.569436	14.638515
19.813540	842.868729	14.643533
19.903871	844.817462	14.648551
19.713137	851.723855	14.653568
20.191130	854.501794	14.658586
19.884839	841.708688	14.663603
19.842498	837.893580	14.668621
19.664483	826.626741	14.673639
19.507204	840.328686	14.678656
19.597158	845.168215	14.683674
19.433515	843.612748	14.688691
19.673862	848.040547	14.693709
19.964621	847.998110	14.698727
19.848954	853.463152	14.703744
20.112967	839.403569	14.708762
20.017073	849.119565	14.713779
19.811178	848.747841	14.718797
19.858261	840.626798	14.723815
19.889191	853.276778	14.728832
19.921620	857.800273	14.733850
20.082847	873.058657	14.738867
20.271236	876.080791	14.743885
20.208068	867.345844	14.748903
20.143524	873.538191	14.753920
20.248880	873.423816	14.758938
20.427204	878.845960	14.763955
20.276972	869.266267	14.768973
20.448432	866.837778	14.773991
20.163760	869.984524	14.779008
20.298185	872.832075	14.784026
20.336276	876.288016	14.789043
20.603959	874.971083	14.794061
20.834918	854.169501	14.799079
20.365198	846.703788	14.804096
20.054750	839.875847	14.809114
20.081503	839.085818	14.814131
20.577034	855.926526	14.819149
20.584615	860.368707	14.824167
20.236693	853.925332	14.829184
20.669417	853.027513	14.834202
20.544950	860.283290	14.839219
20.390531	867.196622	14.844237
20.617291	869.319644	14.849255
20.455759	866.533071	14.854272
20.596746	862.452547	14.859290
20.663551	856.120918	14.864307
20.238097	863.954035	14.869325
20.485710	858.338852	14.874343
20.879393	858.400210	14.879360
20.716967	862.099006	14.884378
20.557501	862.442692	14.889395
21.024734	861.962347	14.894413
21.053775	855.529337	14.899431
20.899278	867.084905	14.904448
20.656330	866.469675	14.909466
20.819002	857.689881	14.914483
20.532050	860.909566	14.919501
21.119438	866.232901	14.924519
21.008639	861.106221	14.929536
20.635571	854.963433	14.934554
20.883432	856.972693	14.939571
20.736505	856.377134	14.944589
20.876990	852.662767	14.949607
20.443524	864.126340	14.954624
20.704039	858.774226	14.959642
20.736925	866.229416	14.964659
20.472400	866.255044	14.969677
20.728097	875.022867	14.974695
20.986871	888.107393	14.979712
21.220074	888.455829	14.984730
21.340591	893.057050	14.989747
21.501445	897.099681	14.994765
21.719672	892.151818	14.999783
21.109126	878.345995	15.004800
20.785971	875.351211	15.009818
20.905011	882.265886	15.014835
21.019675	890.027012	15.019853
21.512680	890.988000	15.024871
21.345432	889.802327	15.029888
21.228627	893.269917	15.034906
21.482029	894.880678	15.039923
21.045936	889.804957	15.044941
21.201984	890.212819	15.049959
21.456332	893.350856	15.054976
21.238184	890.349085	15.059994
21.441454	881.985800	15.065011
21.283398	881.429853	15.070029
21.434957	882.699961	15.075047
21.223287	893.873180	15.080064
21.247901	883.051089	15.085082
21.028125	894.414928	15.090099
21.108374	901.146338	15.095117
21.610615	906.066454	15.100135
21.404601	905.502242	15.105152
21.576978	917.691444	15.110170
21.656619	907.908455	15.115187
21.806566	907.916482	15.120205
21.863283	895.483032	15.125223
21.990600	902.080834	15.130240
21.600715	908.630283	15.135258
21.952738	906.347070	15.140275
21.744423	912.091736	15.145293
22.169398	904.694105	15.150311
22.098172	901.177002	15.155328
21.924925	893.188287	15.160346
21.836566	884.201656	15.165363
21.836548	881.194113	15.170381
21.713824	874.279941	15.175399
21.766872	894.181742	15.180416
22.013275	904.024020	15.185434
22.396513	889.731121	15.190451
21.980974	892.680621	15.195469
21.968405	872.475757	15.200487
21.856273	878.987989	15.205504
21.987075	892.502826	15.210522
22.207582	897.735329	15.215539
21.846561	890.353553	15.220557
22.044660	890.622282	15.225575
22.319984	903.297123	15.230592
22.221069	894.697152	15.235610
22.489390	899.802242	15.240627
22.189600	888.100003	15.245645
22.413227	874.914574	15.250663
22.156548	873.345279	15.255680
22.106754	869.477683	15.260698
22.408626	871.999194	15.265715
22.166313	873.529830	15.270733
22.266983	875.098247	15.275751
22.343888	876.982815	15.280768
22.116021	894.271419	15.285786
22.341709	887.861236	15.290803
22.378670	899.771839	15.295821
22.356624	895.742098	15.300839
22.490654	897.033889	15.305856
22.189068	896.188002	15.310874
22.378621	899.664399	15.315891
22.234954	899.813104	15.320909
22.047817	899.094454	15.325927
22.391392	896.828345	15.330944
22.433471	902.991374	15.335962
22.375181	898.383481	15.340979
22.341312	910.522941	15.345997
22.699118	914.408485	15.351015
22.922025	918.902151	15.356032
22.591586	919.572431	15.361050
22.668362	914.451061	15.366067
22.745185	941.067970	15.371085
22.934361	925.003462	15.376103
22.869315	927.071224	15.381120
22.828129	924.149020	15.386138
22.783184	915.499557	15.391155
22.743664	923.130219	15.396173
22.859489	914.900541	15.401191
22.632571	916.188924	15.406208
22.576189	922.080205	15.411226
22.865818	914.479710	15.416243
22.627943	919.736700	15.421261
22.670508	916.167051	15.426279
23.163570	920.867702	15.431296
22.774419	918.041043	15.436314
23.068573	925.531063	15.441331
23.336605	919.249936	15.446349
23.147806	911.598168	15.451367
23.527079	922.972311	15.456384
22.953725	920.228161	15.461402
22.956850	920.549530	15.466419
22.780178	917.487607	15.471437
23.201471	916.389603	15.476455
23.323849	916.843767	15.481472
23.029306	930.964924	15.486490
23.270172	916.419752	15.491507
23.035505	922.951199	15.496525
23.315813	931.001974	15.501543
23.642212	940.020687	15.506560
23.337534	927.195708	15.511578
23.274875	921.925767	15.516595
23.373598	920.553251	15.521613
23.387720	929.005496	15.526631
23.519535	929.600195	15.531648
23.181991	945.119826	15.536666
23.615665	941.908622	15.541683
23.445811	945.504456	15.546701
23.653314	947.479024	15.551719
23.595954	948.702973	15.556736
23.668729	947.953066	15.561754
23.992180	938.939756	15.566771
23.556684	936.505368	15.571789
23.523532	926.913611	15.576807
23.659514	913.407367	15.581824
23.592252	931.444024	15.586842
24.065716	933.045557	15.591859
23.873959	933.870836	15.596877
23.548093	936.714774	15.601895
23.633935	932.904810	15.606912
23.760347	931.060890	15.611930
24.116448	935.369588	15.616947
23.831094	946.065229	15.621965
23.768652	945.702585	15.626983
23.712996	943.732554	15.632000
23.581640	948.524733	15.637018
23.936086	948.238785	15.642035
23.781195	940.707926	15.647053
23.782355	951.368147	15.652071
23.901317	939.855888	15.657088
23.883957	943.333154	15.662106
24.068221	938.804014	15.667123
23.979057	942.106335	15.672141
23.670471	946.708528	15.677159
24.060080	942.112500	15.682176
23.840742	958.576155	15.687194
24.581222	969.016409	15.692211
24.628563	961.024661	15.697229
24.290554	952.260149	15.702247
24.296406	946.057960	15.707264
24.224866	938.681303	15.712282
23.994172	930.000975	15.717299
24.112325	944.890625	15.722317
23.926182	956.706832	15.727335
24.286857	952.509815	15.732352
24.188500	951.764629	15.737370
24.769942	960.030172	15.742387
24.851412	961.544799	15.747405
24.718275	967.549108	15.752423
24.814782	962.490906	15.757440
24.796205	960.710726	15.762458
24.854314	947.844670	15.767475
24.829556	937.061839	15.772493
24.315680	933.926512	15.777511
24.209989	929.477519	15.782528
23.987847	944.925420	15.787546
24.826932	951.932436	15.792563
24.729773	954.986700	15.797581
24.438144	954.729393	15.802599
24.885098	952.952015	15.807616
24.535696	954.581488	15.812634
24.776693	951.955899	15.817651
24.684043	947.915117	15.822669
24.857233	952.716387	15.827687
24.614739	956.737020	15.832704
24.482505	964.994460	15.837722
24.796799	964.257205	15.842739
24.786425	953.547851	15.847757
24.722384	956.596926	15.852775
24.840703	952.993310	15.857792
24.517117	967.939567	15.862810
24.850057	968.581651	15.867827
24.940120	963.164692	15.872845
24.691096	966.574116	15.877863
25.056255	964.948410	15.882880
25.006815	970.201138	15.887898
25.218725	969.988015	15.892915
25.364502	970.435359	15.897933
25.235767	978.316711	15.902951
25.652849	967.278440	15.907968
25.134777	970.821539	15.912986
25.373410	971.001866	15.918003
25.130617	966.646929	15.923021
25.191342	969.061068	15.928039
25.228871	968.086305	15.933056
25.277737	973.708645	15.938074
24.739432	964.735664	15.943091
25.354659	963.118116	15.948109
24.968507	972.655591	15.953127
25.497082	978.982267	15.958144
25.554771	990.886527	15.963162
25.681290	993.744804	15.968179
25.916430	990.444774	15.973197
25.923998	984.229680	15.978215
25.879232	979.493414	15.983232
25.622182	967.544581	15.988250
25.389553	967.003471	15.993267
25.635106	965.522739	15.998285
25.630411	959.265393	16.003303
25.554293	957.838215	16.008320
25.762757	971.997361	16.013338
25.578448	975.229387	16.018355
25.403230	981.858840	16.023373
25.578954	988.856194	16.028391
25.861826	981.960485	16.033408
25.671984	988.566984	16.038426
25.806738	990.978995	16.043443
25.784828	983.471465	16.048461
25.707220	996.135396	16.053479
26.076499	985.631631	16.058496
25.842716	995.303038	16.063514
25.808515	988.876732	16.068531
26.127620	979.804121	16.073549
25.906743	988.233253	16.078567
25.991929	984.240341	16.083584
25.964787	989.975581	16.088602
25.913347	1001.789648	16.093619
26.346889	1023.424503	16.098637
26.264810	1015.759126	16.103655
26.340947	1016.832774	16.108672
26.512562	1010.686644	16.113690
26.556293	996.882361	16.118707
26.309317	992.771073	16.123725
26.202856	993.491470	16.128743
26.426383	979.021549	16.133760
26.361608	985.671569	16.138778
26.422260	979.899446	16.143795
26.536651	979.670044	16.148813
26.224202	983.231422	16.153831
26.368265	983.262462	16.158848
26.618741	999.927105	16.163866
26.432644	1003.954691	16.168883
26.998033	1010.370286	16.173901
26.561586	995.082246	16.178919
26.363464	983.209378	16.183936
26.725573	989.612633	16.188954
26.483756	990.780277	16.193971
26.757005	997.150120	16.198989
26.395364	1004.875468	16.204007
26.864306	1001.005465	16.209024
26.663883	1006.127222	16.214042
26.534038	1009.603189	16.219059
26.651608	1001.518367	16.224077
26.611418	1012.838366	16.229095
26.444216	1005.997385	16.234112
26.768449	995.216645	16.239130
26.556976	1003.634843	16.244147
27.123933	1000.932929	16.249165
26.777036	997.758805	16.254183
26.821773	1001.169547	16.259200
26.898290	996.783508	16.264218
26.960676	1016.598775	16.269235
27.258470	1018.745400	16.274253
27.134674	1016.959609	16.279271
27.185292	1021.000605	16.284288
27.074888	1016.785861	16.289306
27.174095	1017.653920	16.294323
27.552890	1021.454146	16.299341
27.379206	1014.756191	16.304359
27.429636	999.092058	16.309376
27.173666	991.387663	16.314394
26.948012	991.849020	16.319411
27.128305	1004.668213	16.324429
27.271007	1022.163972	16.329447
27.683012	1022.784204	16.334464
27.672268	1014.097776	16.339482
27.424652	1021.732681	16.344499
27.229428	1021.154151	16.349517
26.914290	1025.605910	16.354535
27.663447	1026.621449	16.359552
27.687300	1025.866580	16.364570
27.269967	1029.176152	16.369587
27.611970	1017.041907	16.374605
27.662367	1026.867625	16.379623
27.844921	1017.645973	16.384640
28.000198	1016.618045	16.389658
27.716171	1025.502064	16.394675
27.695126	1012.206544	16.399693
27.618371	1025.511000	16.404711
27.941457	1030.487625	16.409728
27.858129	1021.474889	16.414746
27.820211	1025.472952	16.419763
28.016312	1018.215277	16.424781
28.285093	1033.952418	16.429799
28.074953	1021.541755	16.434816
28.007892	1024.004326	16.439834
27.624411	1026.481758	16.444851
27.838988	1012.395071	16.449869
27.821366	1022.376613	16.454887
27.971908	1023.555370	16.459904
28.119877	1017.914724	16.464922
27.915090	1025.991052	16.469939
28.159975	1011.110653	16.474957
27.833744	1027.490131	16.479975
27.967796	1023.189748	16.484992
28.225601	1034.172731	16.490010
28.539175	1045.784468	16.495027
28.407944	1037.716521	16.500045
28.357767	1037.389824	16.505063
28.298461	1032.889355	16.510080
28.260931	1029.275427	16.515098
28.454265	1041.439340	16.520115
28.530069	1037.839213	16.525133
28.532196	1038.447923	16.530151
28.441600	1031.575994	16.535168
28.434276	1020.534757	16.540186
28.603909	1034.166696	16.545203
28.736760	1037.610978	16.550221
28.577828	1042.855635	16.555239
28.526326	1040.692435	16.560256
28.671292	1042.127692	16.565274
28.902677	1041.857868	16.570291
28.698560	1034.492475	16.575309
28.818886	1040.980968	16.580327
28.685045	1036.208149	16.585344
28.746925	1038.877741	16.590362
28.830089	1044.273819	16.595379
28.636318	1045.272991	16.600397
28.639667	1035.959484	16.605415
28.625890	1043.377877	16.610432
28.827684	1038.836498	16.615450
28.724244	1025.607527	16.620467
28.694503	1024.788470	16.625485
28.649007	1036.251328	16.630503
28.696124	1039.175703	16.635520
29.032591	1045.169578	16.640538
29.077219	1050.723177	16.645555
29.294945	1049.997893	16.650573
29.142004	1053.726800	16.655591
29.175438	1063.081816	16.660608
29.282006	1060.126972	16.665626
29.261648	1056.778597	16.670643
29.418680	1057.798547	16.675661
29.570065	1058.787823	16.680679
29.512204	1046.908716	16.685696
29.403565	1030.616214	16.690714
29.090443	1028.036406	16.695731
29.220420	1030.821562	16.700749
29.480463	1042.672062	16.705767
29.472281	1059.626599	16.710784
29.451342	1056.372991	16.715802
29.393186	1059.399071	16.720819
29.706777	1059.015379	16.725837
29.721676	1054.591643	16.730855
29.782548	1062.055153	16.735872
29.682733	1049.478860	16.740890
29.540147	1053.007326	16.745907
29.469986	1044.150309	16.750925
29.566098	1049.929375	16.755943
29.438373	1052.366740	16.760960
29.796802	1046.058782	16.765978
29.362366	1051.517023	16.770995
29.160744	1044.716134	16.776013
29.281852	1056.477956	16.781031
29.842552	1065.879753	16.786048
30.234005	1068.731247	16.791066
30.068265	1077.546265	16.796083
30.314115	1073.133677	16.801101
30.184987	1076.451752	16.806119
30.248370	1069.492566	16.811136
30.282926	1067.416867	16.816154
30.239544	1070.377516	16.821171
30.171486	1065.859475	16.826189
30.631013	1056.054755	16.831207
30.331925	1054.460529	16.836224
30.377728	1040.999876	16.841242
30.425621	1045.577801	16.846259
30.260858	1041.971182	16.851277
30.376656	1039.784925	16.856295
30.181806	1049.775315	16.861312
30.318372	1044.511994	16.866330
29.957848	1051.486092	16.871347
30.122951	1048.755612	16.876365
30.185242	1058.295456	16.881383
29.823176	1067.286399	16.886400
30.237174	1062.437206	16.891418
30.008944	1072.527514	16.896435
30.614317	1062.450626	16.901453
30.826969	1068.031555	16.906471
30.853438	1073.155652	16.911488
30.630479	1059.885420	16.916506
30.380838	1076.477010	16.921523
30.015344	1063.266977	16.926541
30.901530	1079.320843	16.931559
30.879489	1096.643668	16.936576
31.479349	1088.625257	16.941594
30.731606	1084.649212	16.946611
31.088796	1081.465746	16.951629
30.682200	1070.550152	16.956647
30.987263	1079.537564	16.961664
30.984003	1084.082487	16.966682
31.200898	1085.878871	16.971699
31.118490	1078.011543	16.976717
31.083396	1083.198938	16.981735
30.998973	1088.122660	16.986752
31.695922	1084.624023	16.991770
31.525924	1075.031536	16.996787
31.100564	1064.895229	17.001805
31.277177	1071.409629	17.006823
30.864263	1068.428875	17.011840
31.099948	1064.478639	17.016858
30.916835	1075.991487	17.021875
30.835321	1085.137301	17.026893
31.226218	1088.250823	17.031911
31.286305	1096.216254	17.036928
31.367220	1091.797945	17.041946
31.191163	1089.411251	17.046963
31.508000	1098.352646	17.051981
31.463897	1090.791742	17.056999
31.465695	1099.962382	17.062016
31.490690	1095.215155	17.067034
31.651555	1102.246441	17.072051
31.260253	1099.625221	17.077069
31.691568	1109.501758	17.082087
31.515373	1122.774530	17.087104
31.835590	1123.033597	17.092122
31.702207	1122.682064	17.097139
31.903767	1119.469325	17.102157
31.702380	1109.414668	17.107175
31.662402	1116.890847	17.112192
31.843728	1114.192530	17.117210
31.778081	1116.389799	17.122227
31.684027	1114.507817	17.127245
32.037954	1115.291790	17.132263
32.003807	1122.214779	17.137280
32.343854	1107.814862	17.142298
32.166909	1112.970842	17.147315
32.037895	1106.871780	17.152333
31.983430	1110.632609	17.157351
32.221817	1113.031555	17.162368
31.836001	1103.068915	17.167386
32.209718	1117.044492	17.172403
32.161275	1118.588955	17.177421
32.651929	1117.473760	17.182439
32.413906	1118.088541	17.187456
32.355228	1108.910949	17.192474
32.167977	1112.244448	17.197491
32.335445	1123.803387	17.202509
32.728109	1128.516668	17.207527
32.455887	1139.630098	17.212544
32.770907	1132.126522	17.217562
32.460652	1107.562428	17.222579
32.324530	1113.971205	17.227597
32.556589	1114.285111	17.232615
32.731435	1132.239856	17.237632
32.749809	1130.693716	17.242650
32.772316	1132.419573	17.247667
32.271569	1137.380133	17.252685
32.947057	1125.749001	17.257703
33.252649	1134.326094	17.262720
32.968484	1131.078999	17.267738
32.996074	1115.800203	17.272755
33.249116	1125.000921	17.277773
33.173759	1116.277228	17.282791
33.048953	1104.752562	17.287808
32.789970	1095.155071	17.292826
32.546122	1101.224108	17.297843
32.580225	1123.982041	17.302861
33.118295	1126.103658	17.307879
33.003932	1123.177106	17.312896
32.949342	1125.479943	17.317914
33.020303	1125.159512	17.322931
32.890784	1126.265388	17.327949
33.302732	1127.024492	17.332967
33.070609	1129.938982	17.337984
33.070399	1121.762103	17.343002
33.653940	1136.351775	17.348019
32.878814	1150.589427	17.353037
33.229862	1150.297698	17.358055
33.593342	1150.139723	17.363072
33.735284	1147.374987	17.368090
33.628253	1147.088754	17.373107
33.430049	1156.944026	17.378125
33.241886	1150.349276	17.383143
33.491814	1141.208525	17.388160
33.375386	1140.273654	17.393178
33.694348	1141.340824	17.398195
33.497073	1145.278672	17.403213
33.711259	1140.318750	17.408231
33.849710	1153.296088	17.413248
33.819864	1145.635094	17.418266
33.761261	1144.426069	17.423283
33.825404	1153.041001	17.428301
34.093377	1153.746922	17.433319
34.305756	1154.325851	17.438336
34.049380	1155.962857	17.443354
34.296460	1141.195618	17.448371
34.029416	1151.134257	17.453389
34.147259	1135.247998	17.458407
33.805619	1140.120513	17.463424
34.010157	1138.649349	17.468442
33.974865	1146.793852	17.473459
33.915500	1164.412931	17.478477
34.166988	1156.212381	17.483495
34.319584	1162.052063	17.488512
34.202056	1160.539837	17.493530
34.214678	1162.806901	17.498547
34.212876	1163.154293	17.503565
34.436639	1166.177247	17.508583
34.422204	1160.170671	17.513600
34.300108	1161.811887	17.518618
34.432853	1159.922769	17.523635
34.184665	1158.427858	17.528653
34.501309	1163.493895	17.533671
34.374021	1178.936604	17.538688
34.567017	1180.679936	17.543706
34.621197	1178.241378	17.548723
34.769147	1193.587326	17.553741
35.063013	1186.522554	17.558759
34.921094	1194.478652	17.563776
35.199133	1188.729208	17.568794
35.003417	1186.983071	17.573811
35.375731	1177.924115	17.578829
34.831208	1163.807915	17.583847
35.047027	1156.654394	17.588864
35.127705	1159.762883	17.593882
35.085547	1156.001328	17.598899
35.009473	1155.334696	17.603917
34.845650	1149.837535	17.608935
35.015907	1167.575279	17.613952
35.005483	1167.646304	17.618970
35.055154	1169.954902	17.623987
35.080511	1175.808213	17.629005
35.233666	1174.121028	17.634023
35.218731	1184.925926	17.639040
35.247051	1181.008153	17.644058
35.385211	1180.680348	17.649075
35.147453	1192.937154	17.654093
35.092654	1178.135128	17.659111
35.274345	1183.900830	17.664128
35.119846	1191.379203	17.669146
35.659727	1198.224908	17.674163
34.893526	1215.320448	17.679181
35.486378	1206.602476	17.684199
35.937530	1205.667039	17.689216
36.038975	1206.342248	17.694234
36.124897	1199.818149	17.699251
36.182451	1209.649158	17.704269
36.009980	1191.962138	17.709287
36.042400	1182.621908	17.714304
35.901669	1191.404661	17.719322
35.923221	1168.975526	17.724339
35.747604	1180.013884	17.729357
35.679931	1197.157758	17.734375
36.243096	1192.266225	17.739392
35.915397	1198.733450	17.744410
36.152687	1196.499737	17.749427
36.225952	1201.187338	17.754445
36.205598	1201.035851	17.759463
36.180405	1197.101212	17.764480
36.257081	1194.113159	17.769498
36.079644	1202.384102	17.774515
36.130860	1198.611065	17.779533
36.382878	1201.746366	17.784551
36.655479	1197.263283	17.789568
36.323706	1199.912523	17.794586
36.233936	1199.929706	17.799603
36.043907	1207.315820	17.804621
36.468574	1196.967361	17.809639
36.418033	1185.184847	17.814656
36.256313	1197.275104	17.819674
36.841356	1208.027040	17.824691
36.605379	1220.564460	17.829709
37.072261	1209.540329	17.834727
36.480171	1204.444775	17.839744
36.276526	1219.836365	17.844762
36.699996	1224.273439	17.849779
37.032498	1229.892447	17.854797
37.108928	1222.483020	17.859815
36.647700	1221.453840	17.864832
36.863264	1225.497442	17.869850
36.994797	1210.438972	17.874867
36.975872	1220.247254	17.879885
37.055436	1226.868438	17.884903
36.977328	1216.166383	17.889920
36.989452	1222.634025	17.894938
36.778735	1220.331641	17.899955
36.907559	1221.586401	17.904973
37.264915	1215.101822	17.909991
37.196931	1209.577003	17.915008
37.059750	1221.941150	17.920026
37.214278	1226.912681	17.925043
37.328829	1242.399607	17.930061
37.121102	1245.013639	17.935079
37.385042	1243.750916	17.940096
37.600331	1245.355059	17.945114
37.834112	1231.555533	17.950131
37.612124	1248.161884	17.955149
37.674360	1243.500304	17.960167
38.036276	1235.591694	17.965184
37.823835	1238.872358	17.970202
38.214975	1227.853771	17.975219
37.985986	1223.632311	17.980237
37.635633	1211.518046	17.985255
37.665033	1214.628267	17.990272
37.488010	1225.913033	17.995290
37.894529	1236.270066	18.000307
37.739212	1228.925350	18.005325
37.918185	1237.569670	18.010343
37.842333	1233.892275	18.015360
38.190071	1243.655747	18.020378
38.182429	1237.521845	18.025395
38.097686	1238.806910	18.030413
37.907490	1236.696975	18.035431
37.991682	1235.557092	18.040448
38.097384	1242.890575	18.045466
37.859301	1236.988443	18.050483
38.257634	1240.214440	18.055501
38.333458	1254.956342	18.060519
38.232381	1251.945634	18.065536
38.085435	1256.917068	18.070554
38.501866	1246.169072	18.075571
38.480253	1242.552607	18.080589
38.261550	1249.381481	18.085607
38.715356	1244.219881	18.090624
38.498594	1247.166698	18.095642
38.788535	1247.749257	18.100659
39.054560	1248.733206	18.105677
38.914961	1245.419257	18.110695
38.865277	1244.101528	18.115712
38.658222	1243.445945	18.120730
38.784717	1249.788377	18.125747
39.164036	1250.237009	18.130765
38.992186	1251.387396	18.135783
38.878848	1237.001604	18.140800
38.629829	1239.082446	18.145818
38.832799	1242.465288	18.150835
38.824919	1241.936294	18.155853
38.758627	1250.331861	18.160871
39.226999	1260.054350	18.165888
39.144283	1269.462387	18.170906
39.234144	1260.832663	18.175923
39.434279	1272.023651	18.180941
39.465837	1270.390224	18.185959
39.424956	1265.782665	18.190976
39.409323	1265.374810	18.195994
39.731063	1262.616601	18.201011
39.776530	1254.318893	18.206029
39.319601	1251.089376	18.211047
39.343217	1244.186847	18.216064
39.079729	1263.024622	18.221082
39.395209	1270.861752	18.226099
39.485997	1268.070297	18.231117
39.394648	1262.479693	18.236135
39.427772	1258.356017	18.241152
39.816363	1257.357794	18.246170
39.548707	1260.385173	18.251187
39.475474	1267.279627	18.256205
39.765588	1289.312830	18.261223
39.950172	1283.533816	18.266240
39.718889	1290.733917	18.271258
39.887119	1286.895190	18.276275
40.077755	1288.026657	18.281293
40.071845	1288.257926	18.286311
40.161947	1277.437959	18.291328
40.118164	1291.665283	18.296346
40.173669	1288.718402	18.301363
40.047553	1287.068651	18.306381
40.358820	1276.412854	18.311399
40.430332	1280.337023	18.316416
40.270412	1290.315762	18.321434
40.129654	1283.549428	18.326451
40.538465	1269.460510	18.331469
40.325695	1286.639827	18.336487
40.354248	1275.633838	18.341504
40.033589	1283.605356	18.346522
40.382449	1303.953589	18.351539
40.771781	1311.946429	18.356557
40.940857	1310.689097	18.361575
40.830241	1302.182284	18.366592
40.459840	1306.863684	18.371610
40.851424	1306.505639	18.376627
40.842741	1308.864425	18.381645
40.812586	1306.306515	18.386663
41.179448	1304.756255	18.391680
41.046499	1304.805450	18.396698
41.160814	1304.317272	18.401715
41.554396	1302.743890	18.406733
41.082298	1320.014365	18.411751
41.299475	1299.261764	18.416768
41.413480	1311.359393	18.421786
41.122230	1307.942956	18.426803
41.298528	1304.207105	18.431821
40.947546	1314.919560	18.436839
41.186808	1306.190665	18.441856
41.116674	1305.601993	18.446874
41.161329	1310.253079	18.451891
41.332752	1305.157796	18.456909
41.122173	1310.902944	18.461927
41.285047	1309.018558	18.466944
41.375019	1320.892734	18.471962
41.538968	1329.463711	18.476979
41.496766	1323.650785	18.481997
41.348571	1331.115605	18.487015
41.470004	1315.963951	18.492032
41.231503	1333.324075	18.497050
41.319730	1340.142766	18.502067
41.881881	1339.663320	18.507085
41.923803	1348.284984	18.512103
42.182957	1351.053107	18.517120
42.126418	1351.693111	18.522138
42.488082	1350.500280	18.527155
42.225140	1326.146230	18.532173
41.967188	1324.504507	18.537191
42.286207	1319.717466	18.542208
42.100581	1322.987631	18.547226
42.344714	1340.414161	18.552243
42.258478	1328.441479	18.557261
42.240971	1333.064439	18.562279
42.587814	1339.508085	18.567296
42.493089	1339.172582	18.572314
42.638964	1329.621989	18.577331
42.483160	1326.664026	18.582349
42.098599	1334.661359	18.587367
42.117158	1337.233638	18.592384
42.429119	1337.588681	18.597402
42.518770	1336.432157	18.602419
42.394497	1343.486121	18.607437
42.694085	1347.008485	18.612455
42.599253	1337.912181	18.617472
42.322392	1347.590527	18.622490
42.775152	1350.523984	18.627507
43.189169	1352.743963	18.632525
43.010501	1351.926133	18.637543
42.939691	1342.005526	18.642560
43.024698	1354.836744	18.647578
42.974280	1355.412671	18.652595
42.811709	1354.450302	18.657613
42.910363	1364.132941	18.662631
43.385737	1366.283346	18.667648
43.546842	1371.146585	18.672666
43.240012	1370.036398	18.677683
43.252639	1360.329935	18.682701
43.253634	1370.681152	18.687719
43.535540	1368.973778	18.692736
43.320617	1362.462040	18.697754
43.198464	1369.761844	18.702771
43.173127	1357.138949	18.707789
43.301167	1365.526215	18.712807
43.208749	1368.908022	18.717824
43.321935	1380.081142	18.722842
43.800053	1384.651710	18.727859
43.903685	1385.020459	18.732877
43.875230	1389.316933	18.737895
43.877021	1395.940897	18.742912
43.794772	1398.642593	18.747930
44.014623	1390.923437	18.752947
44.461144	1380.915443	18.757965
44.252136	1380.733550	18.762983
44.515878	1381.812542	18.768000
44.211633	1383.434977	18.773018
43.981554	1394.627172	18.778035
44.039540	1381.378957	18.783053
44.345768	1386.156345	18.788071
44.804391	1381.432624	18.793088
44.473934	1379.284685	18.798106
44.358660	1380.088532	18.803123
44.533114	1374.279516	18.808141
44.572443	1379.755150	18.813159
44.535649	1377.867325	18.818176
44.492706	1377.167089	18.823194
44.174655	1383.967397	18.828211
44.703457	1373.924424	18.833229
44.420449	1379.437937	18.838247
44.458374	1382.168141	18.843264
44.426983	1380.370991	18.848282
44.369358	1381.257327	18.853299
44.677011	1379.552230	18.858317
44.528374	1388.538297	18.863335
44.590681	1399.552137	18.868352
44.877358	1399.204215	18.873370
44.475120	1404.297742	18.878387
44.824007	1404.097870	18.883405
44.786106	1409.765501	18.888423
45.006736	1414.164972	18.893440
45.372350	1415.982272	18.898458
45.461456	1418.694995	18.903475
45.211533	1414.659813	18.908493
45.067402	1418.478937	18.913511
45.244901	1428.587932	18.918528
45.647860	1426.653294	18.923546
45.379556	1435.875893	18.928563
45.724084	1434.568972	18.933581
45.611980	1431.168626	18.938599
45.426129	1431.036755	18.943616
45.779697	1421.049614	18.948634
45.645332	1427.985268	18.953651
45.689205	1426.081643	18.958669
45.762288	1431.356337	18.963687
45.742928	1422.803609	18.968704
46.044705	1427.515431	18.973722
45.911249	1431.348665	18.978739
45.897175	1429.318414	18.983757
45.896495	1415.028441	18.988775
45.998017	1423.038021	18.993792
46.040419	1424.934365	18.998810
45.846528	1423.572941	19.003827
45.723244	1419.669401	19.008845
46.041738	1439.662771	19.013863
46.170081	1442.107407	19.018880
46.299066	1447.111405	19.023898
46.307367	1454.816855	19.028915
46.468242	1447.110072	19.033933
46.649116	1444.490675	19.038951
46.566712	1454.122832	19.043968
46.694416	1443.956462	19.048986
46.254657	1438.190007	19.054003
46.522232	1441.862578	19.059021
46.543152	1448.688700	19.064039
46.312592	1451.009681	19.069056
46.362379	1444.970856	19.074074
46.596890	1462.850312	19.079091
46.819405	1471.604693	19.084109
46.933295	1471.119733	19.089127
46.798207	1473.943333	19.094144
47.087401	1471.130229	19.099162
47.031636	1477.696966	19.104179
47.295438	1467.124236	19.109197
47.191592	1470.283781	19.114215
46.777070	1468.953765	19.119232
47.413917	1461.633169	19.124250
47.385461	1464.648352	19.129267
47.086556	1472.461904	19.134285
47.013184	1468.945025	19.139303
47.222750	1475.820500	19.144320
47.592094	1475.099848	19.149338
47.449639	1487.528124	19.154355
47.757392	1486.062853	19.159373
47.702735	1485.070946	19.164391
47.892693	1488.642074	19.169408
48.224196	1479.207491	19.174426
47.368028	1472.720437	19.179443
47.741453	1476.871914	19.184461
47.859210	1489.593952	19.189479
47.870735	1483.371752	19.194496
47.688632	1490.482173	19.199514
47.693559	1486.773135	19.204531
47.771968	1480.543613	19.209549
47.876069	1490.020331	19.214567
48.088368	1492.713763	19.219584
47.949205	1493.429836	19.224602
48.334531	1499.637127	19.229619
48.443756	1494.166510	19.234637
48.359458	1490.919594	19.239655
48.788625	1497.905844	19.244672
48.754484	1483.658930	19.249690
48.272221	1483.191629	19.254707
48.400032	1482.855973	19.259725
48.679039	1486.747678	19.264743
48.464932	1488.422275	19.269760
48.425755	1483.391496	19.274778
48.279475	1501.119203	19.279795
48.817657	1503.960404	19.284813
48.703757	1505.003893	19.289831
48.633197	1509.963429	19.294848
48.743693	1503.447993	19.299866
48.810748	1504.112822	19.304883
48.846574	1501.639224	19.309901
48.856943	1501.362995	19.314919
48.851314	1510.860072	19.319936
49.244145	1517.018854	19.324954
49.335167	1535.776124	19.329971
49.363883	1521.882266	19.334989
49.072898	1517.695696	19.340007
49.247301	1532.510749	19.345024
49.594741	1522.401430	19.350042
49.566030	1530.627131	19.355059
49.538209	1533.440246	19.360077
49.711653	1527.950089	19.365095
49.707210	1524.605445	19.370112
49.735381	1527.614923	19.375130
49.548294	1525.886335	19.380147
49.608243	1525.807474	19.385165
49.717244	1521.854894	19.390183
49.434916	1529.628003	19.395200
49.631711	1525.298733	19.400218
49.699226	1525.685767	19.405235
49.619097	1530.552130	19.410253
50.225929	1537.340139	19.415271
49.985277	1542.742919	19.420288
49.982048	1541.884969	19.425306
50.035819	1553.521963	19.430323
50.039289	1547.812267	19.435341
50.226193	1553.009201	19.440359
50.148936	1551.705236	19.445376
50.179461	1551.286986	19.450394
50.223151	1553.385123	19.455411
49.859639	1549.380330	19.460429
50.626514	1557.664441	19.465447
50.333079	1564.356813	19.470464
50.520293	1564.235921	19.475482
50.491838	1565.111385	19.480499
50.732974	1571.461218	19.485517
50.885362	1563.427495	19.490535
50.567321	1564.417760	19.495552
50.874620	1562.160410	19.500570
51.273839	1567.942650	19.505587
51.061077	1566.921858	19.510605
51.196903	1566.799550	19.515623
50.928053	1566.841634	19.520640
51.044287	1559.962344	19.525658
51.181469	1558.410177	19.530675
50.843705	1571.067936	19.535693
51.412134	1566.421642	19.540711
50.896585	1587.214913	19.545728
51.326659	1580.005564	19.550746
51.421638	1581.663303	19.555763
51.725485	1580.968689	19.560781
51.830914	1573.478831	19.565799
51.621178	1585.207626	19.570816
51.656002	1586.448735	19.575834
51.349911	1587.894744	19.580851
51.531192	1580.837988	19.585869
51.550662	1583.299702	19.590887
51.163213	1583.360368	19.595904
51.555148	1579.780033	19.600922
51.692162	1591.599680	19.605939
51.759261	1596.667066	19.610957
52.064692	1595.157967	19.615975
52.085355	1615.532728	19.620992
52.032928	1606.445424	19.626010
51.868491	1602.147484	19.631027
51.973422	1605.056581	19.636045
52.202930	1603.682458	19.641063
52.332495	1600.913280	19.646080
52.606720	1602.202094	19.651098
52.674950	1601.803183	19.656115
52.276381	1602.944930	19.661133
52.198946	1608.404212	19.666151
52.408915	1623.245327	19.671168
52.609113	1631.776055	19.676186
52.687748	1638.984547	19.681203
52.622083	1639.067385	19.686221
52.896171	1632.295886	19.691239
52.845874	1628.993121	19.696256
53.123039	1639.787244	19.701274
53.109668	1622.033844	19.706291
53.059065	1625.109331	19.711309
53.043473	1631.884436	19.716327
52.915876	1631.254261	19.721344
52.857114	1623.086327	19.726362
53.141864	1618.282484	19.731379
53.242680	1627.071789	19.736397
53.192948	1635.244024	19.741415
53.436889	1647.744423	19.746432
53.390681	1659.981005	19.751450
53.842608	1655.444465	19.756467
53.949525	1649.254602	19.761485
53.943403	1647.557612	19.766503
53.629878	1633.095562	19.771520
53.343313	1642.920761	19.776538
53.707837	1650.368503	19.781555
53.450668	1650.547620	19.786573
53.701771	1645.944712	19.791591
54.050583	1650.630288	19.796608
53.965488	1639.569293	19.801626
54.073042	1644.071749	19.806643
54.296959	1649.184013	19.811661
54.041992	1643.461125	19.816679
53.957215	1647.362522	19.821696
54.044801	1646.929018	19.826714
53.960698	1655.681034	19.831731
54.134193	1667.618098	19.836749
54.283621	1671.921486	19.841767
54.245424	1671.125816	19.846784
54.597974	1662.353751	19.851802
54.969095	1665.587246	19.856819
54.589607	1670.437429	19.861837
55.254628	1662.591602	19.866855
54.745720	1658.328683	19.871872
54.410533	1660.691330	19.876890
55.128923	1654.654985	19.881907
54.450895	1668.969355	19.886925
54.749630	1662.484333	19.891943
54.771865	1665.826141	19.896960
54.639303	1679.613223	19.901978
55.087426	1685.469895	19.906995
55.169311	1683.831702	19.912013
55.355275	1686.005398	19.917031
55.433581	1684.901125	19.922048
55.214904	1685.014248	19.927066
55.484018	1687.986003	19.932083
55.045821	1682.686307	19.937101
55.246727	1678.908652	19.942119
55.313113	1680.062768	19.947136
55.598491	1687.472430	19.952154
55.696768	1678.692855	19.957171
55.746114	1687.004234	19.962189
55.529273	1679.599539	19.967207
55.723249	1683.056461	19.972224
55.594834	1700.087251	19.977242
55.967968	1703.143703	19.982259
56.074720	1713.525889	19.987277
56.027515	1705.532842	19.992295
56.143311	1711.501553	19.997312
55.922302	1712.647047	20.002330
56.093917	1707.621051	20.007347
56.059867	1708.787749	20.012365
56.536016	1702.404311	20.017383
56.299369	1697.429658	20.022400
56.108201	1697.866693	20.027418
56.239645	1701.172461	20.032435
56.275956	1714.185145	20.037453
56.049092	1728.536181	20.042471
56.770342	1725.980412	20.047488
56.661491	1731.659260	20.052506
56.489298	1734.103684	20.057523
56.731285	1727.015269	20.062541
56.549668	1737.837147	20.067559
56.797531	1742.074634	20.072576
56.580433	1750.781257	20.077594
57.044131	1754.984932	20.082611
57.152585	1754.911095	20.087629
57.036695	1757.573931	20.092647
57.161337	1753.331655	20.097664
57.108130	1755.631200	20.102682
57.513616	1746.557293	20.107699
57.099450	1751.094177	20.112717
57.231527	1748.220435	20.117735
57.624742	1744.886034	20.122752
57.540578	1749.907732	20.127770
57.855160	1762.381363	20.132787
57.460255	1768.995030	20.137805
57.691490	1772.086349	20.142823
57.853114	1774.225998	20.147840
57.893571	1771.896814	20.152858
58.160800	1767.748967	20.157875
58.106650	1771.506728	20.162893
58.099290	1769.506946	20.167911
58.313578	1769.741595	20.172928
58.011174	1768.494981	20.177946
58.019682	1767.881348	20.182963
57.915490	1768.513053	20.187981
58.255201	1765.774045	20.192999
58.092128	1771.985295	20.198016
57.794857	1767.310473	20.203034
58.593171	1780.519418	20.208051
58.401896	1795.054290	20.213069
58.443330	1801.028370	20.218087
58.654299	1800.635495	20.223104
58.281230	1793.703381	20.228122
58.723847	1787.296763	20.233139
58.863497	1792.999817	20.238157
59.003475	1789.714552	20.243175
58.704998	1788.729269	20.248192
58.632128	1791.464270	20.253210
59.110212	1798.531343	20.258227
58.896333	1820.451649	20.263245
59.181944	1816.509206	20.268263
59.861641	1813.748484	20.273280
59.606281	1813.924163	20.278298
59.699211	1800.029496	20.283315
59.314770	1792.117650	20.288333
59.305765	1793.621276	20.293351
59.551888	1801.131815	20.298368
59.283931	1804.493867	20.303386
59.559122	1803.443951	20.308403
59.568495	1816.056963	20.313421
59.502270	1811.484793	20.318439
59.546776	1811.313671	20.323456
59.660012	1815.783720	20.328474
59.985768	1812.967992	20.333491
59.504373	1808.782781	20.338509
59.860824	1817.229152	20.343527
60.049964	1832.080017	20.348544
60.001163	1833.899169	20.353562
59.966842	1832.187645	20.358579
60.130230	1827.169217	20.363597
60.087966	1837.284470	20.368615
60.234690	1829.055844	20.373632
60.103311	1851.793290	20.378650
60.489275	1856.987529	20.383667
60.333731	1862.026753	20.388685
60.252649	1859.388375	20.393703
60.509293	1860.818827	20.398720
60.392705	1866.154925	20.403738
60.701123	1862.972653	20.408755
60.773282	1875.661081	20.413773
60.864642	1889.908735	20.418791
61.245530	1886.027095	20.423808
61.459751	1881.915930	20.428826
61.343842	1878.626555	20.433843
61.470267	1888.346155	20.438861
61.204552	1889.782705	20.443879
61.651857	1880.639059	20.448896
61.809543	1885.960596	20.453914
61.719345	1878.687465	20.458931
61.609383	1870.985061	20.463949
61.337544	1865.009108	20.468967
61.475293	1872.167405	20.473984
61.360165	1884.197172	20.479002
61.876669	1872.562066	20.484019
61.436139	1884.933169	20.489037
61.574680	1884.952453	20.494055
61.970866	1873.342509	20.499072
61.699332	1878.721823	20.504090
62.084438	1879.014923	20.509107
62.323530	1886.917945	20.514125
61.952718	1900.243874	20.519143
62.117699	1892.043919	20.524160
61.988741	1896.261581	20.529178
62.192550	1888.828766	20.534195
62.356055	1898.754015	20.539213
62.310358	1899.278723	20.544231
62.410115	1893.528583	20.549248
62.361964	1899.816553	20.554266
62.630892	1908.522849	20.559283
62.831869	1918.508514	20.564301
62.565235	1924.130087	20.569319
62.871763	1913.622990	20.574336
62.807465	1927.844565	20.579354
62.628962	1921.958120	20.584371
63.170973	1919.575584	20.589389
62.989693	1917.530446	20.594407
62.955105	1911.864469	20.599424
62.772474	1925.773201	20.604442
62.994116	1932.463911	20.609459
63.288306	1941.507116	20.614477
63.178697	1947.839447	20.619495
63.306027	1940.794160	20.624512
63.661601	1952.718667	20.629530
63.424357	1949.987969	20.634547
63.501487	1948.464113	20.639565
63.320038	1943.338723	20.644583
63.580497	1949.540486	20.649600
64.084864	1962.189665	20.654618
63.983250	1964.926040	20.659635
64.079928	1969.395566	20.664653
63.978396	1963.206693	20.669671
64.338229	1960.846382	20.674688
64.238840	1965.327689	20.679706
64.223347	1971.048795	20.684723
64.156796	1969.260250	20.689741
63.921522	1967.930515	20.694759
64.363959	1961.697446	20.699776
64.195742	1958.526712	20.704794
64.580195	1964.409232	20.709811
64.275526	1966.817634	20.714829
64.363603	1983.360307	20.719847
64.825525	1977.906873	20.724864
64.780471	1981.846303	20.729882
65.266962	1982.600081	20.734899
65.361817	1983.238480	20.739917
64.805874	1972.983246	20.744935
65.145979	1977.600841	20.749952
65.527030	1989.010105	20.754970
65.305659	1978.674046	20.759987
65.359208	1990.125153	20.765005
65.265226	1979.305199	20.770023
65.541353	1980.672643	20.775040
65.327314	1981.318409	20.780058
65.398507	1972.009566	20.785075
65.236818	1978.006061	20.790093
65.223865	1982.063547	20.795111
65.713716	1986.572470	20.800128
65.642531	2004.522454	20.805146
65.907742	2005.074199	20.810163
66.114188	2000.282523	20.815181
65.660947	1998.522999	20.820199
65.777607	1996.794116	20.825216
65.949551	1990.060579	20.830234
65.951634	2000.159508	20.835251
66.255464	2011.299998	20.840269
66.224949	2019.497801	20.845287
66.629257	2029.912453	20.850304
66.592467	2020.743588	20.855322
66.425034	2023.480816	20.860339
66.662200	2026.271427	20.865357
66.660390	2031.763174	20.870375
66.827904	2025.131311	20.875392
66.567278	2022.356924	20.880410
66.322902	2020.419497	20.885427
66.849698	2024.341931	20.890445
66.662060	2027.741937	20.895463
66.924108	2031.841561	20.900480
66.812942	2048.977284	20.905498
67.155800	2042.327411	20.910515
67.389232	2045.964429	20.915533
67.296016	2048.355493	20.920551
67.478354	2048.402633	20.925568
67.281068	2046.735556	20.930586
67.433285	2043.344178	20.935603
67.301843	2040.985082	20.940621
67.140476	2054.666504	20.945639
67.656857	2057.839440	20.950656
67.684237	2064.358649	20.955674
67.364203	2069.704590	20.960691
67.845970	2060.476553	20.965709
67.242078	2066.823246	20.970727
67.756477	2078.448378	20.975744
67.697825	2086.290832	20.980762
68.245315	2094.988292	20.985779
68.314393	2085.638693	20.990797
68.237728	2092.537158	20.995815
68.176260	2089.984042	21.000832
68.219322	2088.860018	21.005850
68.196224	2089.914562	21.010867
68.404281	2083.402567	21.015885
68.667643	2103.471595	21.020903
68.701445	2109.967721	21.025920
69.052712	2107.447776	21.030938
69.321256	2121.642606	21.035955
69.335083	2117.016788	21.040973
68.974130	2098.203286	21.045991
69.058845	2108.440820	21.051008
69.211388	2107.605779	21.056026
69.449596	2104.260882	21.061043
69.521125	2107.961151	21.066061
69.684799	2118.842778	21.071079
69.216147	2105.790155	21.076096
69.314649	2109.394673	21.081114
69.301312	2105.246521	21.086131
69.543283	2110.614885	21.091149
69.391394	2118.374123	21.096167
69.369257	2101.480067	21.101184
69.358801	2110.586867	21.106202
69.842067	2128.500605	21.111219
70.227845	2129.620490	21.116237
69.974349	2132.664731	21.121255
69.698605	2126.995440	21.126272
69.706604	2134.025834	21.131290
69.622964	2146.540033	21.136307
70.262099	2142.062412	21.141325
70.433550	2144.869650	21.146343
70.547443	2147.398705	21.151360
70.558882	2148.403658	21.156378
70.568636	2154.701580	21.161395
70.986804	2151.732455	21.166413
70.721448	2155.416081	21.171431
70.788317	2153.691828	21.176448
71.058178	2153.078265	21.181466
70.545103	2150.438091	21.186483
70.966561	2152.215160	21.191501
70.860211	2147.961641	21.196519
71.114892	2148.859050	21.201536
70.842282	2159.569196	21.206554
70.975637	2173.393896	21.211571
71.275651	2174.659776	21.216589
71.360576	2172.724392	21.221607
71.520154	2180.475887	21.226624
71.200272	2170.761115	21.231642
71.168157	2181.515652	21.236659
71.737416	2184.948592	21.241677
71.954460	2189.746482	21.246695
71.898673	2190.787217	21.251712
72.242620	2196.934958	21.256730
71.901512	2201.675119	21.261747
72.072333	2192.069664	21.266765
72.079228	2191.049137	21.271783
72.334702	2197.201271	21.276800
72.233786	2198.533124	21.281818
72.138028	2198.096772	21.286835
72.217388	2193.189245	21.291853
72.288243	2186.913321	21.296871
72.142112	2198.537868	21.301888
72.074539	2202.206297	21.306906
72.429144	2218.454944	21.311923
72.724564	2199.636338	21.316941
72.361342	2216.120533	21.321959
72.830119	2219.859581	21.326976
72.925408	2226.690128	21.331994
72.876706	2235.357978	21.337011
72.954701	2235.102704	21.342029
73.646766	2231.210110	21.347047
72.887933	2230.700903	21.352064
73.029306	2228.917629	21.357082
72.859864	2232.456844	21.362099
73.231709	2239.442900	21.367117
73.454922	2248.787739	21.372135
73.501208	2250.620441	21.377152
74.180432	2254.250780	21.382170
73.925855	2248.546573	21.387187
74.202340	2243.242044	21.392205
74.155222	2250.877618	21.397223
73.912562	2253.396273	21.402240
73.898477	2248.604366	21.407258
74.004162	2256.869309	21.412275
73.974471	2252.089314	21.417293
74.029168	2261.034492	21.422311
73.932932	2275.015172	21.427328
74.417987	2273.559934	21.432346
74.556917	2277.950327	21.437363
74.662757	2283.766142	21.442381
74.743560	2284.308915	21.447399
74.736688	2276.631214	21.452416
74.990927	2277.781186	21.457434
74.798458	2276.722456	21.462451
74.798935	2272.512135	21.467469
74.756020	2275.375072	21.472487
74.849801	2291.418474	21.477504
74.928823	2283.556885	21.482522
74.975807	2299.595002	21.487539
75.057517	2298.963571	21.492557
74.923609	2301.525159	21.497575
75.240011	2319.607255	21.502592
75.806735	2320.013933	21.507610
75.985449	2328.393712	21.512627
75.855957	2322.976024	21.517645
76.024896	2314.791037	21.522663
76.012723	2324.980752	21.527680
76.038560	2325.399582	21.532698
75.816147	2325.030411	21.537715
76.132488	2326.782938	21.542733
76.241988	2322.075800	21.547751
76.116143	2316.843752	21.552768
76.638257	2317.146956	21.557786
76.208987	2322.317564	21.562803
76.263575	2330.628420	21.567821
76.531664	2334.641954	21.572839
76.657242	2349.067665	21.577856
76.699768	2344.958047	21.582874
76.594239	2350.169469	21.587891
76.446841	2341.027237	21.592909
76.832459	2342.920404	21.597927
76.849846	2348.058914	21.602944
77.137293	2360.373098	21.607962
77.276252	2366.202687	21.612979
77.206975	2362.164235	21.617997
77.581721	2366.571358	21.623015
77.053052	2364.953014	21.628032
77.276008	2363.280032	21.633050
77.304175	2371.434086	21.638067
77.472854	2367.405693	21.643085
77.663950	2355.085889	21.648103
77.345751	2367.412907	21.653120
77.843000	2373.858613	21.658138
78.044998	2393.161179	21.663155
77.870130	2385.317230	21.668173
78.036392	2382.277071	21.673191
78.074329	2384.994802	21.678208
78.013158	2387.396670	21.683226
77.883995	2381.959977	21.688243
77.902802	2390.882437	21.693261
78.630483	2399.993670	21.698279
78.541476	2406.136725	21.703296
78.664985	2405.899566	21.708314
78.611328	2414.644025	21.713331
78.778106	2412.067728	21.718349
78.977517	2403.634906	21.723367
78.979384	2407.330370	21.728384
78.956351	2404.193621	21.733402
78.494653	2412.661149	21.738419
78.822010	2425.085900	21.743437
79.039282	2429.230505	21.748455
79.033598	2428.366585	21.753472
79.276016	2428.593681	21.758490
79.031404	2431.156851	21.763507
79.512352	2441.149442	21.768525
79.304405	2454.153590	21.773543
79.638139	2456.177986	21.778560
80.148447	2456.820747	21.783578
79.957021	2460.716936	21.788595
79.972136	2459.714043	21.793613
80.466827	2452.696216	21.798631
80.108133	2465.225324	21.803648
80.347480	2451.935280	21.808666
80.409925	2448.381149	21.813683
80.334583	2457.539320	21.818701
80.382350	2448.505326	21.823719
80.478550	2461.427111	21.828736
80.777555	2467.733480	21.833754
80.771233	2471.136722	21.838771
80.666750	2477.455812	21.843789
80.929570	2473.213811	21.848807
80.501095	2482.332638	21.853824
80.895393	2470.728918	21.858842
80.468451	2469.940464	21.863859
80.806435	2488.473829	21.868877
81.166670	2495.417618	21.873895
81.357905	2497.145577	21.878912
81.438977	2503.568162	21.883930
81.631945	2500.549048	21.888947
81.247032	2499.047037	21.893965
81.441660	2488.004817	21.898983
81.343093	2509.204082	21.904000
81.788950	2512.669045	21.909018
81.882317	2512.878464	21.914035
82.047959	2530.533067	21.919053
81.644484	2528.967684	21.924071
82.149824	2517.756833	21.929088
82.346512	2509.864085	21.934106
82.558014	2531.112636	21.939123
82.218146	2535.044722	21.944141
82.695153	2536.907811	21.949159
82.639875	2537.778056	21.954176
82.460633	2528.202017	21.959194
82.768539	2536.586901	21.964211
82.663149	2539.589069	21.969229
82.837517	2549.408824	21.974247
82.632968	2536.377632	21.979264
82.965832	2533.314502	21.984282
82.864298	2533.519739	21.989299
82.969779	2550.751399	21.994317
83.266585	2555.265464	21.999335
83.177148	2566.325888	22.004352
83.471225	2565.184600	22.009370
83.731862	2559.118679	22.014387
83.077713	2566.076239	22.019405
83.486183	2561.189642	22.024423
83.444977	2561.057190	22.029440
83.620460	2567.152550	22.034458
83.657258	2585.827886	22.039475
83.822019	2583.876795	22.044493
83.845782	2582.673704	22.049511
83.704773	2591.517150	22.054528
83.919190	2595.400282	22.059546
84.223975	2603.192333	22.064563
84.375890	2601.502055	22.069581
84.500373	2600.605109	22.074599
84.321960	2609.669041	22.079616
84.248557	2611.526844	22.084634
84.732502	2626.452113	22.089651
84.830450	2627.547691	22.094669
85.210932	2625.641701	22.099687
85.257089	2624.532939	22.104704
85.171605	2627.898115	22.109722
85.558682	2620.499410	22.114739
85.463559	2620.059791	22.119757
85.504554	2614.530089	22.124775
85.790524	2625.550671	22.129792
85.679611	2627.199734	22.134810
86.264885	2620.274960	22.139827
85.502813	2623.790322	22.144845
86.113518	2621.570524	22.149863
85.985496	2626.662460	22.154880
85.647534	2618.222201	22.159898
85.797159	2622.607847	22.164915
86.012460	2642.678695	22.169933
86.262889	2638.656372	22.174951
86.180182	2651.426422	22.179968
85.840674	2647.146190	22.184986
86.258324	2652.761778	22.190003
86.291066	2662.881525	22.195021
86.646660	2664.596374	22.200039
86.434544	2670.963956	22.205056
86.531511	2670.819325	22.210074
86.925603	2669.697079	22.215091
86.891106	2679.013083	22.220109
87.081789	2682.925202	22.225127
87.321779	2689.098869	22.230144
87.389945	2693.554106	22.235162
87.263276	2691.449824	22.240179
87.168994	2700.229191	22.245197
87.327339	2696.795701	22.250215
87.341637	2704.907893	22.255232
87.359222	2705.804604	22.260250
87.654497	2716.173616	22.265267
87.679049	2721.942341	22.270285
87.700728	2717.002679	22.275303
87.776975	2712.562610	22.280320
88.044538	2732.622214	22.285338
88.528597	2729.172406	22.290355
88.315389	2741.779909	22.295373
88.532988	2734.606548	22.300391
88.500930	2739.472018	22.305408
88.447791	2742.046264	22.310426
88.827538	2732.221575	22.315443
88.737990	2748.628660	22.320461
88.843313	2729.208053	22.325479
89.062228	2731.799642	22.330496
88.922387	2739.793971	22.335514
89.260804	2733.984079	22.340531
88.661096	2744.651133	22.345549
88.749702	2756.100392	22.350567
89.236948	2759.530514	22.355584
89.379758	2766.439038	22.360602
89.865435	2767.454942	22.365619
89.630681	2764.805788	22.370637
89.843051	2763.819317	22.375655
89.556001	2763.179364	22.380672
89.332214	2779.418139	22.385690
89.786251	2777.459580	22.390707
89.573749	2791.645090	22.395725
89.724913	2785.479467	22.400743
89.974700	2802.414172	22.405760
89.935079	2816.421121	22.410778
90.312981	2818.198770	22.415795
90.138081	2817.875799	22.420813
89.941068	2825.020643	22.425831
90.296036	2831.633991	22.430848
90.584799	2840.075671	22.435866
90.949778	2841.416639	22.440883
90.882040	2840.060589	22.445901
91.113260	2833.860313	22.450919
91.003712	2851.154355	22.455936
91.368898	2860.417303	22.460954
91.196905	2856.843010	22.465971
91.395406	2856.669845	22.470989
91.737328	2854.757249	22.476007
91.643104	2852.300685	22.481024
91.398281	2858.673457	22.486042
91.860137	2857.543740	22.491059
92.223385	2876.029361	22.496077
92.178374	2887.351297	22.501095
92.221687	2891.504326	22.506112
92.190512	2883.703926	22.511130
92.482890	2878.510345	22.516147
92.673499	2881.084297	22.521165
92.812786	2880.298640	22.526183
92.789206	2874.832631	22.531200
92.602722	2883.351945	22.536218
92.512391	2874.178408	22.541235
92.663644	2884.724734	22.546253
92.427561	2886.222998	22.551271
92.865951	2884.797118	22.556288
92.746980	2909.607570	22.561306
92.908652	2907.009909	22.566323
93.414322	2906.741277	22.571341
93.207365	2905.766839	22.576359
93.310628	2911.845225	22.581376
93.353848	2930.078046	22.586394
93.558968	2922.868691	22.591411
93.845053	2937.957778	22.596429
93.646742	2931.234555	22.601447
94.117326	2930.396993	22.606464
94.073792	2935.772461	22.611482
93.980362	2925.100192	22.616499
94.060030	2928.998195	22.621517
94.033878	2935.942724	22.626535
94.310022	2942.704178	22.631552
94.247804	2954.028852	22.636570
94.673861	2940.731290	22.641587
94.992658	2941.694446	22.646605
94.814286	2938.903872	22.651623
94.689567	2942.720276	22.656640
94.636159	2952.882089	22.661658
94.861792	2949.318074	22.666675
94.972796	2965.561376	22.671693
94.928179	2969.254770	22.676711
95.038770	2961.747746	22.681728
95.344277	2967.065383	22.686746
95.444562	2985.939497	22.691763
95.730233	2991.818897	22.696781
95.911233	3002.291195	22.701799
95.745076	2989.600842	22.706816
95.481787	2993.568371	22.711834
95.864020	2987.136074	22.716851
95.903292	2991.466507	22.721869
96.346076	2990.674328	22.726887
96.439741	2985.600223	22.731904
96.457353	3012.519855	22.736922
96.302600	3009.293169	22.741939
96.639590	3021.536922	22.746957
96.492782	3007.123391	22.751975
97.057642	3009.461980	22.756992
96.650717	3013.237395	22.762010
96.631134	3008.752299	22.767027
97.119979	3015.436270	22.772045
97.029800	3036.944149	22.777063
97.184230	3032.166663	22.782080
96.972719	3036.233401	22.787098
97.170269	3034.980960	22.792115
97.151467	3039.405720	22.797133
97.335094	3049.328454	22.802151
97.623572	3053.660889	22.807168
97.422879	3059.171484	22.812186
97.633713	3059.138415	22.817203
98.100744	3070.130903	22.822221
97.971940	3080.831688	22.827239
98.353632	3087.245258	22.832256
97.985063	3090.175125	22.837274
98.209427	3084.455584	22.842291
97.983481	3087.893350	22.847309
98.180696	3098.855535	22.852327
98.785885	3099.840111	22.857344
98.716011	3106.599026	22.862362
98.737497	3103.969644	22.867379
98.840599	3109.521032	22.872397
98.822224	3115.015705	22.877415
99.036304	3120.887426	22.882432
99.098030	3129.042877	22.887450
99.441787	3131.182562	22.892467
99.326049	3129.856104	22.897485
99.511083	3138.251052	22.902503
99.740581	3146.632725	22.907520
99.551563	3149.092598	22.912538
99.645439	3155.570222	22.917555
100.283660	3148.636953	22.922573
100.243427	3155.526960	22.927591
99.988654	3154.847217	22.932608
100.034091	3173.139905	22.937626
100.007248	3181.463911	22.942643
100.581021	3179.035210	22.947661
100.153940	3188.267796	22.952679
100.723604	3183.586184	22.957696
100.759143	3197.736308	22.962714
100.838858	3199.194589	22.967731
101.229226	3203.444818	22.972749
101.180289	3196.325657	22.977767
101.456412	3201.654280	22.982784
101.382724	3203.856218	22.987802
101.407056	3205.581989	22.992819
101.881492	3202.850067	22.997837
101.394023	3194.568677	23.002855
101.669094	3197.514504	23.007872
101.537257	3207.224779	23.012890
101.723747	3217.415437	23.017907
101.971148	3223.764877	23.022925
101.964685	3225.738505	23.027943
102.148069	3222.266274	23.032960
102.136803	3223.801937	23.037978
101.893309	3223.641204	23.042995
102.322996	3233.254051	23.048013
102.190243	3256.763610	23.053031
102.612533	3249.324414	23.058048
102.644741	3247.908487	23.063066
102.684665	3247.091039	23.068083
102.971458	3264.427538	23.073101
102.934079	3275.442365	23.078119
103.221500	3266.515603	23.083136
103.062685	3271.189606	23.088154
102.913313	3279.204604	23.093171
103.411127	3285.082427	23.098189
103.415239	3304.379098	23.103207
103.769825	3299.623840	23.108224
103.877758	3298.297046	23.113242
103.464624	3303.345465	23.118259
103.875541	3299.850197	23.123277
103.780387	3315.700018	23.128295
104.638634	3320.151567	23.133312
104.425641	3330.370157	23.138330
104.344170	3321.204473	23.143347
104.525024	3317.451713	23.148365
104.370515	3317.785196	23.153383
104.640191	3328.537324	23.158400
104.744432	3345.280717	23.163418
104.693284	3345.787383	23.168435
105.003678	3344.141646	23.173453
105.168423	3341.404567	23.178471
105.370712	3348.004150	23.183488
105.615063	3357.683976	23.188506
105.511232	3365.452001	23.193523
105.635094	3370.312151	23.198541
105.864345	3365.522855	23.203559
105.495300	3362.323366	23.208576
105.725747	3364.117860	23.213594
105.627268	3378.920377	23.218611
105.735986	3388.637250	23.223629
105.813430	3394.000213	23.228647
105.969394	3392.580668	23.233664
106.417797	3406.246489	23.238682
106.588143	3419.880132	23.243699
106.482758	3411.945941	23.248717
106.412472	3418.452535	23.253735
106.920182	3412.252932	23.258752
107.014835	3434.496146	23.263770
107.267858	3439.875804	23.268787
106.938932	3432.948760	23.273805
106.941741	3439.462847	23.278823
107.440429	3431.004755	23.283840
107.870839	3447.747643	23.288858
107.679491	3455.920797	23.293875
108.236649	3451.929146	23.298893
108.088823	3474.585996	23.303911
108.136018	3464.784605	23.308928
108.147493	3465.082618	23.313946
107.924248	3468.652597	23.318963
108.409685	3465.540159	23.323981
108.123365	3471.506173	23.328999
108.424445	3466.055402	23.334016
108.465579	3454.698917	23.339034
108.004813	3474.838736	23.344051
108.568149	3486.280366	23.349069
108.638547	3487.784318	23.354087
108.949265	3493.625240	23.359104
108.651010	3494.176936	23.364122
108.945873	3516.979112	23.369139
109.241232	3518.271070	23.374157
109.399602	3521.023761	23.379175
109.183895	3515.073182	23.384192
109.381702	3528.936171	23.389210
109.468733	3545.051186	23.394227
109.888555	3538.306645	23.399245
109.801374	3536.922026	23.404263
110.046427	3549.486703	23.409280
110.236567	3557.950484	23.414298
110.436213	3567.924651	23.419315
110.262548	3567.872914	23.424333
109.883622	3566.035303	23.429351
110.487596	3560.761148	23.434368
110.596692	3574.429754	23.439386
110.805408	3587.423095	23.444403
111.191145	3589.647792	23.449421
110.677386	3593.073931	23.454439
111.045010	3588.988849	23.459456
111.232487	3597.866543	23.464474
111.351792	3604.794853	23.469491
111.495694	3613.830885	23.474509
111.346357	3615.991067	23.479527
111.514378	3613.338654	23.484544
111.753845	3623.398146	23.489562
111.986075	3636.390994	23.494579
111.958543	3636.900281	23.499597
111.887842	3646.370802	23.504615
112.261528	3641.707153	23.509632
112.667320	3654.486600	23.514650
112.613579	3662.098557	23.519667
112.476315	3664.477796	23.524685
112.689682	3662.831451	23.529703
112.967159	3661.639041	23.534720
112.947769	3661.039184	23.539738
113.014972	3669.149833	23.544755
113.186281	3680.015427	23.549773
113.338092	3681.143664	23.554791
113.466626	3686.290393	23.559808
113.715299	3689.272000	23.564826
113.460918	3687.130795	23.569843
113.797930	3689.776617	23.574861
113.944050	3701.432095	23.579879
114.489791	3701.075114	23.584896
114.169046	3696.785377	23.589914
113.840359	3706.883425	23.594931
114.243111	3702.878035	23.599949
113.914697	3704.308765	23.604967
114.320760	3713.344807	23.609984
114.535844	3720.665322	23.615002
114.266307	3729.169638	23.620019
114.497017	3727.896173	23.625037
114.803054	3751.239783	23.630055
114.714894	3750.953705	23.635072
115.122502	3766.523149	23.640090
115.344932	3775.183980	23.645107
115.415808	3770.394140	23.650125
115.180248	3773.997671	23.655143
115.601027	3776.904984	23.660160
115.835415	3786.873828	23.665178
116.121870	3802.149806	23.670195
116.342557	3793.353182	23.675213
116.356141	3800.547481	23.680231
116.379327	3811.407953	23.685248
116.290593	3799.658117	23.690266
116.194626	3805.578636	23.695283
116.493619	3803.688450	23.700301
116.655156	3812.942763	23.705319
116.652210	3816.860214	23.710336
116.662915	3828.530678	23.715354
116.486517	3842.269464	23.720371
116.838141	3838.571909	23.725389
117.451793	3842.629491	23.730407
117.088749	3848.755997	23.735424
117.066758	3852.717473	23.740442
117.554270	3870.938451	23.745459
117.572777	3885.814588	23.750477
117.906697	3883.328683	23.755495
117.646731	3891.705320	23.760512
117.836425	3892.527781	23.765530
118.049253	3906.079383	23.770547
117.958617	3906.680629	23.775565
118.404740	3909.145258	23.780583
118.280960	3929.008683	23.785600
118.870960	3930.150352	23.790618
118.811313	3937.813851	23.795635
118.603887	3937.508579	23.800653
119.070344	3946.547902	23.805671
119.091167	3960.000214	23.810688
119.544269	3958.344691	23.815706
119.459869	3964.427582	23.820723
119.519006	3960.674821	23.825741
119.719962	3961.634401	23.830759
119.584020	3967.987347	23.835776
119.983691	3983.419340	23.840794
120.020744	3986.642472	23.845811
120.413906	3982.603804	23.850829
120.397697	3985.686930	23.855847
120.154609	3981.675345	23.860864
120.775114	3985.728730	23.865882
120.744166	4012.733211	23.870899
120.695800	4012.797566	23.875917
120.976852	3999.133714	23.880935
120.553453	4007.965277	23.885952
120.910211	4016.459986	23.890970
121.055914	4023.617893	23.895987
121.311720	4035.439473	23.901005
121.152891	4030.704489	23.906023
121.393171	4041.515306	23.911040
121.634070	4047.455726	23.916058
121.559581	4057.441546	23.921075
121.702594	4059.720112	23.926093
122.000542	4070.196803	23.931111
122.025205	4079.387473	23.936128
122.390196	4080.826384	23.941146
122.533610	4075.251783	23.946163
122.109937	4089.111562	23.951181
122.751918	4092.763902	23.956199
122.736151	4098.596198	23.961216
122.954422	4101.058675	23.966234
122.979061	4097.046154	23.971251
123.059182	4116.095052	23.976269
123.309378	4120.332740	23.981287
123.169862	4125.063910	23.986304
123.419498	4120.160749	23.991322
123.483900	4131.529449	23.996339
123.788488	4139.634682	24.001357
123.970211	4146.793308	24.006375
124.307306	4154.224297	24.011392
124.125772	4152.570335	24.016410
124.395915	4154.323971	24.021427
124.402834	4160.742981	24.026445
124.447619	4162.181562	24.031463
124.420027	4175.846785	24.036480
124.532406	4172.704296	24.041498
124.940094	4175.973556	24.046515
124.773553	4178.745687	24.051533
124.860314	4184.303123	24.056551
124.911087	4201.128282	24.061568
125.311893	4195.718487	24.066586
125.641304	4207.834820	24.071603
125.608191	4225.913616	24.076621
126.042080	4214.621380	24.081639
125.402103	4224.790578	24.086656
125.904644	4225.611389	24.091674
126.071293	4231.926490	24.096691
126.034273	4245.208159	24.101709
126.300987	4239.929833	24.106727
126.349725	4252.917151	24.111744
126.415349	4255.646608	24.116762
126.678840	4271.778815	24.121779
126.887786	4278.150434	24.126797
127.410785	4275.256083	24.131815
127.270580	4282.856595	24.136832
127.526465	4280.856327	24.141850
127.641186	4271.110206	24.146867
127.519816	4278.448939	24.151885
127.782827	4291.696263	24.156903
127.624005	4293.349826	24.161920
127.737091	4288.370163	24.166938
127.777727	4296.826150	24.171955
127.827661	4316.615436	24.176973
128.275595	4320.421325	24.181991
128.491687	4325.545049	24.187008
128.671832	4323.042143	24.192026
128.814492	4331.381156	24.197043
128.647646	4349.509434	24.202061
129.069758	4348.742536	24.207079
129.085422	4352.635093	24.212096
128.879345	4350.893421	24.217114
129.172157	4363.968838	24.222131
129.253277	4381.666901	24.227149
129.531703	4375.632310	24.232167
129.562982	4379.932764	24.237184
129.295690	4388.178206	24.242202
129.908914	4398.091194	24.247219
129.692244	4399.147790	24.252237
130.033087	4422.193263	24.257255
129.832894	4431.125788	24.262272
130.482564	4432.065600	24.267290
130.653342	4448.300869	24.272307
130.835068	4457.176730	24.277325
130.944250	4456.162146	24.282343
131.022997	4455.947759	24.287360
131.227657	4444.394587	24.292378
131.600104	4463.237073	24.297395
131.831005	4469.958844	24.302413
131.728607	4467.777952	24.307431
131.682993	4478.150881	24.312448
131.819048	4476.832222	24.317466
131.627254	4474.734776	24.322483
131.760573	4494.066132	24.327501
131.986675	4480.461032	24.332519
132.177626	4486.494646	24.337536
131.854270	4495.061409	24.342554
132.555367	4512.870798	24.347571
132.304145	4527.019539	24.352589
132.526245	4527.830640	24.357607
132.747781	4543.881281	24.362624
133.078680	4545.994744	24.367642
133.251699	4545.355245	24.372659
133.482782	4549.154121	24.377677
133.621028	4554.571033	24.382695
133.726855	4575.447142	24.387712
133.579210	4562.216183	24.392730
133.598268	4572.575877	24.397747
133.262841	4579.414821	24.402765
133.968453	4587.135468	24.407783
134.049479	4593.053766	24.412800
134.056291	4601.824528	24.417818
134.451826	4605.070520	24.422835
134.208733	4626.471668	24.427853
134.612066	4631.010603	24.432871
134.815303	4649.459979	24.437888
134.889938	4654.053572	24.442906
134.904750	4647.252129	24.447923
135.299673	4666.902524	24.452941
135.508938	4672.229432	24.457959
135.584631	4677.485729	24.462976
135.682805	4676.902141	24.467994
136.142396	4681.586944	24.473011
136.192608	4689.921666	24.478029
136.227159	4693.666137	24.483047
136.262296	4699.657946	24.488064
136.339505	4704.661494	24.493082
136.567256	4706.794293	24.498099
136.719076	4722.906517	24.503117
136.818691	4727.991787	24.508135
136.954845	4731.613027	24.513152
136.969358	4735.884626	24.518170
137.319720	4743.979803	24.523187
137.497804	4756.947218	24.528205
137.707961	4749.591152	24.533223
137.800779	4754.162982	24.538240
137.826175	4764.673306	24.543258
138.130975	4774.751611	24.548275
138.234752	4785.196007	24.553293
138.333067	4782.194503	24.558311
138.161014	4789.768650	24.563328
138.142539	4798.022643	24.568346
138.832718	4803.296343	24.573363
138.296039	4807.092451	24.578381
138.623504	4821.864134	24.583399
138.941897	4837.467416	24.588416
139.055494	4835.969172	24.593434
139.258762	4834.485288	24.598451
139.812087	4850.960856	24.603469
139.764189	4863.332444	24.608487
139.616495	4864.513991	24.613504
139.571310	4862.481915	24.618522
139.892380	4876.156172	24.623539
139.991858	4882.800833	24.628557
140.279190	4888.488045	24.633575
140.529295	4902.145030	24.638592
140.266950	4907.094507	24.643610
140.794067	4904.161537	24.648627
140.788999	4911.895809	24.653645
141.094371	4922.977887	24.658663
141.209569	4928.325920	24.663680
141.556161	4933.716618	24.668698
141.902289	4925.284895	24.673715
141.335690	4940.588153	24.678733
141.762334	4946.635500	24.683751
141.965035	4963.608017	24.688768
141.734939	4957.712877	24.693786
142.136356	4955.213098	24.698803
141.780145	4968.744164	24.703821
141.962234	4981.404925	24.708839
142.125349	4986.694964	24.713856
142.337760	5006.907778	24.718874
142.666734	5010.981819	24.723891
142.421167	5018.283488	24.728909
142.740328	5028.729002	24.733927
143.233776	5037.565781	24.738944
143.118002	5039.035898	24.743962
143.523510	5050.380143	24.748979
143.556992	5065.456919	24.753997
143.457057	5071.163824	24.759015
143.845669	5072.261365	24.764032
143.935016	5087.629281	24.769050
144.326860	5089.534398	24.774067
144.486960	5097.009287	24.779085
144.029196	5103.062665	24.784103
144.612043	5118.457460	24.789120
144.583523	5126.918354	24.794138
144.817337	5129.984599	24.799155
144.707080	5147.356696	24.804173
145.016471	5137.585929	24.809191
145.388215	5150.835786	24.814208
145.201992	5164.289859	24.819226
145.616206	5169.988848	24.824243
145.841037	5181.405673	24.829261
146.005909	5193.021293	24.834279
146.159049	5202.018790	24.839296
146.584635	5212.769710	24.844314
146.533627	5205.492255	24.849331
146.908459	5212.785192	24.854349
146.849839	5217.737558	24.859367
147.025054	5222.564908	24.864384
147.381472	5227.565893	24.869402
147.216828	5223.084036	24.874419
147.022981	5234.894771	24.879437
147.336523	5240.347557	24.884455
147.551525	5249.834129	24.889472
147.773211	5257.709793	24.894490
148.263100	5269.416591	24.899507
147.893949	5282.293342	24.904525
148.264068	5285.549753	24.909543
148.293070	5276.880300	24.914560
148.739337	5295.661580	24.919578
148.989163	5303.059365	24.924595
148.340408	5309.038564	24.929613
148.677600	5313.373385	24.934631
149.112665	5326.341981	24.939648
149.377065	5333.882700	24.944666
149.556667	5326.092421	24.949683
149.659531	5337.307488	24.954701
149.140270	5338.058002	24.959719
149.625311	5354.336388	24.964736
149.653232	5368.779806	24.969754
150.122166	5371.951306	24.974771
150.165465	5376.802520	24.979789
150.514023	5396.467282	24.984807
150.732383	5397.105396	24.989824
150.572179	5403.835122	24.994842
151.032032	5401.016781	24.999859
150.934639	5412.534737	25.004877
151.106574	5422.646844	25.009895
151.097987	5422.667092	25.014912
151.295997	5443.911707	25.019930
151.625652	5460.552291	25.024947
151.960305	5466.128103	25.029965
151.594423	5474.376852	25.034983
152.260308	5478.312988	25.040000
151.869155	5486.650931	25.045018
152.339210	5492.508575	25.050035
152.286908	5496.153179	25.055053
152.596797	5511.922518	25.060071
152.908560	5507.053448	25.065088
152.976553	5512.333289	25.070106
153.041438	5511.000454	25.075123
153.121524	5530.789492	25.080141
153.340476	5547.782104	25.085159
153.182508	5544.261899	25.090176
153.360568	5565.219368	25.095194
153.496069	5560.336861	25.100211
153.868968	5576.440460	25.105229
153.917360	5601.253618	25.110247
154.396488	5592.396701	25.115264
154.410879	5603.969869	25.120282
154.704850	5617.803605	25.125299
154.746506	5625.729730	25.130317
154.508061	5632.225578	25.135335
155.142510	5644.964297	25.140352
155.825576	5649.412316	25.145370
155.497689	5645.580948	25.150387
155.224022	5657.098264	25.155405
155.699562	5668.678144	25.160423
155.901227	5674.072827	25.165440
156.061656	5685.613698	25.170458
156.237452	5696.350373	25.175475
156.441966	5697.757739	25.180493
156.388765	5701.273101	25.185511
156.575710	5712.377370	25.190528
156.375049	5729.031833	25.195546
156.996600	5737.861512	25.200563
157.209743	5744.460270	25.205581
157.231485	5750.312472	25.210599
157.579552	5749.819127	25.215616
157.613386	5759.921489	25.220634
157.761493	5775.583821	25.225651
157.904126	5774.617589	25.230669
157.777390	5789.868427	25.235687
158.457710	5798.758376	25.240704
158.826976	5803.549167	25.245722
158.549178	5801.723888	25.250739
158.816416	5814.090944	25.255757
158.958640	5823.990116	25.260775
159.347920	5826.381846	25.265792
159.269907	5834.623538	25.270810
159.135544	5843.533812	25.275827
159.584584	5843.996909	25.280845
159.792804	5853.604812	25.285863
159.712879	5868.021327	25.290880
159.948448	5887.072978	25.295898
159.890573	5882.403769	25.300915
160.120641	5893.428788	25.305933
160.834749	5915.148679	25.310951
160.777339	5913.181534	25.315968
160.565971	5922.378544	25.320986
160.921504	5933.263976	25.326003
161.091471	5939.206659	25.331021
161.150318	5951.451775	25.336039
161.457028	5959.071356	25.341056
161.391658	5971.313849	25.346074
161.379727	5976.098114	25.351091
161.649719	5981.681057	25.356109
161.857931	5995.799994	25.361127
161.804151	6016.507040	25.366144
162.213621	6028.773040	25.371162
162.602745	6034.911862	25.376179
163.046855	6047.816422	25.381197
162.729400	6050.890269	25.386215
162.929349	6050.536920	25.391232
163.458181	6059.696956	25.396250
163.527326	6068.452344	25.401267
163.576212	6066.626367	25.406285
163.992923	6083.875759	25.411303
163.938961	6071.377175	25.416320
163.677292	6089.660929	25.421338
164.231150	6097.519643	25.426355
164.285549	6098.565435	25.431373
163.888876	6112.974943	25.436391
164.596991	6122.978186	25.441408
164.581640	6127.330551	25.446426
165.040744	6150.880548	25.451443
165.183958	6149.828973	25.456461
165.285003	6162.348571	25.461479
165.485610	6162.396025	25.466496
165.759784	6173.524790	25.471514
165.677488	6172.581148	25.476531
165.928547	6186.324179	25.481549
165.839804	6197.632927	25.486567
166.039475	6207.248670	25.491584
166.368617	6223.899501	25.496602
166.384102	6223.451934	25.501619
166.930144	6240.116151	25.506637
166.722428	6256.961604	25.511655
166.926828	6257.336769	25.516672
167.310415	6267.299386	25.521690
167.577463	6276.437407	25.526707
167.782986	6285.471427	25.531725
167.589177	6295.240406	25.536743
167.929093	6304.247068	25.541760
167.654447	6321.747048	25.546778
168.259815	6333.300699	25.551795
168.276386	6343.295601	25.556813
168.693324	6349.635363	25.561831
168.690805	6356.760587	25.566848
168.819988	6369.882022	25.571866
169.049146	6390.873471	25.576883
169.103144	6402.346234	25.581901
169.271083	6409.580517	25.586919
170.003188	6422.317109	25.591936
169.922824	6426.913333	25.596954
169.976305	6443.910603	25.601971
170.176858	6454.337635	25.606989
170.785067	6445.258053	25.612007
170.625419	6449.345831	25.617024
170.694096	6460.112364	25.622042
170.847917	6470.142655	25.627059
171.211346	6481.096628	25.632077
171.682553	6495.651427	25.637095
171.666991	6501.923256	25.642112
171.920163	6498.414220	25.647130
171.727252	6515.573272	25.652147
172.254660	6509.028612	25.657165
172.331372	6524.251344	25.662183
172.071815	6532.730140	25.667200
172.391287	6530.040955	25.672218
172.598875	6555.483927	25.677236
172.599387	6554.836661	25.682253
172.960504	6558.448278	25.687271
173.176667	6585.342086	25.692288
172.867414	6589.724820	25.697306
173.355132	6592.862026	25.702324
173.721243	6608.298351	25.707341
173.516979	6618.438488	25.712359
173.793082	6625.520167	25.717376
174.384868	6635.838660	25.722394
173.918893	6644.270924	25.727412
174.612622	6648.698581	25.732429
174.420022	6659.029480	25.737447
175.180035	6667.519080	25.742464
175.058676	6672.851019	25.747482
175.052539	6684.645906	25.752500
175.622184	6694.996313	25.757517
175.425102	6701.246136	25.762535
175.674198	6700.338943	25.767552
176.179154	6723.326889	25.772570
175.979462	6721.965964	25.777588
176.083898	6716.810215	25.782605
176.125137	6743.542248	25.787623
176.592718	6742.070473	25.792640
176.673143	6760.774829	25.797658
176.848490	6768.816249	25.802676
176.786311	6765.902702	25.807693
177.083373	6792.869377	25.812711
177.525947	6805.493752	25.817728
177.501771	6807.609445	25.822746
177.480351	6820.679030	25.827764
178.025920	6829.587440	25.832781
178.006550	6846.467063	25.837799
178.270963	6863.258048	25.842816
178.398844	6864.456531	25.847834
178.482109	6883.469941	25.852852
178.760874	6886.096951	25.857869
179.083498	6900.220759	25.862887
179.168216	6916.114978	25.867904
179.658324	6914.507072	25.872922
179.737812	6925.467910	25.877940
179.843245	6945.478644	25.882957
179.986317	6954.570132	25.887975
180.045875	6961.344921	25.892992
180.508691	6966.642252	25.898010
180.457252	6975.600063	25.903028
180.508183	6981.669068	25.908045
180.566887	6995.496508	25.913063
180.704515	7015.691688	25.918080
181.173972	7024.387977	25.923098
181.119034	7034.785913	25.928116
181.381592	7048.452024	25.933133
181.903170	7051.482985	25.938151
182.107813	7072.359092	25.943168
182.413518	7073.719145	25.948186
182.078983	7079.242442	25.953204
182.819117	7085.856991	25.958221
182.918155	7098.134460	25.963239
183.087258	7101.141726	25.968256
183.279773	7104.795649	25.973274
183.636824	7117.862979	25.978292
183.544853	7124.064910	25.983309
183.439035	7134.439304	25.988327
183.824829	7147.113850	25.993344
184.204529	7145.674754	25.998362
183.964785	7170.945575	26.003380
184.138367	7181.462483	26.008397
184.503542	7188.549368	26.013415
184.600465	7206.553912	26.018432
185.071631	7212.708692	26.023450
184.875595	7213.639092	26.028468
185.084465	7235.048243	26.033485
185.387163	7249.702651	26.038503
185.661755	7259.626059	26.043520
185.612986	7270.941832	26.048538
185.978483	7278.031859	26.053556
186.379664	7298.643819	26.058573
186.513105	7304.343269	26.063591
185.957218	7307.792468	26.068608
186.641770	7326.172300	26.073626
186.545456	7324.593090	26.078644
186.958934	7339.217586	26.083661
187.191107	7356.364495	26.088679
187.344814	7357.028595	26.093696
187.481047	7367.194724	26.098714
187.579945	7383.178677	26.103732
187.938201	7376.530777	26.108749
188.305572	7391.642397	26.113767
188.505532	7408.002002	26.118784
188.437866	7414.983151	26.123802
188.568273	7438.513685	26.128820
189.148252	7444.743050	26.133837
189.014084	7453.650914	26.138855
188.993512	7463.096615	26.143872
189.566466	7475.893604	26.148890
189.582959	7486.264819	26.153908
189.606695	7496.477056	26.158925
189.761263	7503.975896	26.163943
189.732177	7528.096631	26.168960
190.189482	7537.622199	26.173978
190.424622	7551.409787	26.178996
190.808243	7569.527622	26.184013
191.030024	7579.670995	26.189031
191.059661	7589.841319	26.194048
191.339459	7607.334584	26.199066
191.481465	7615.154294	26.204084
191.368730	7625.883631	26.209101
192.270523	7628.511014	26.214119
192.004513	7649.628828	26.219136
192.462822	7656.515041	26.224154
192.696192	7666.363046	26.229172
192.589825	7681.675399	26.234189
193.242679	7694.216934	26.239207
193.429490	7705.878066	26.244224
193.888276	7707.113162	26.249242
193.826270	7712.609737	26.254260
194.247561	7720.622516	26.259277
194.032443	7731.472136	26.264295
194.053852	7748.049436	26.269312
194.424480	7744.269204	26.274330
194.574889	7760.949430	26.279348
194.494194	7771.961123	26.284365
194.830162	7782.118290	26.289383
194.811669	7792.110000	26.294400
195.448583	7807.463869	26.299418
195.345926	7832.246876	26.304436
196.028374	7831.382238	26.309453
196.021247	7848.365042	26.314471
196.064815	7851.417354	26.319488
196.682448	7862.575422	26.324506
196.754555	7875.697402	26.329524
196.872102	7884.973300	26.334541
197.578789	7893.162438	26.339559
197.100202	7905.107888	26.344576
197.425300	7911.781445	26.349594
197.518223	7913.209624	26.354612
197.478534	7926.674330	26.359629
198.052116	7941.046916	26.364647
198.024965	7937.133222	26.369664
198.459726	7963.773806	26.374682
198.250617	7967.942279	26.379700
198.655796	7984.248147	26.384717
198.917278	7987.073763	26.389735
198.908483	8003.116165	26.394752
199.235789	8021.202224	26.399770
199.505452	8027.126809	26.404788
199.638876	8039.080653	26.409805
199.826691	8044.042530	26.414823
200.140753	8056.331150	26.419840
200.272838	8065.617490	26.424858
200.322552	8084.394299	26.429876
200.333781	8083.697944	26.434893
201.006908	8096.163965	26.439911
200.719629	8108.900418	26.444928
200.675779	8115.502407	26.449946
201.001329	8133.901403	26.454964
200.745542	8150.800313	26.459981
201.304422	8164.872296	26.464999
201.246349	8186.876863	26.470016
201.509218	8215.161173	26.475034
201.717237	8220.350401	26.480052
201.720184	8245.199501	26.485069
202.599349	8264.313806	26.490087
202.643892	8276.111242	26.495104
202.907926	8303.997709	26.500122
203.130933	8317.491002	26.505140
203.634545	8327.918977	26.510157
203.736729	8338.204633	26.515175
203.867959	8360.113449	26.520192
204.251824	8369.458369	26.525210
204.968598	8379.344683	26.530228
204.633374	8388.732806	26.535245
204.977558	8389.979590	26.540263
205.221438	8406.854127	26.545280
205.442995	8411.491946	26.550298
205.631115	8417.994560	26.555316
205.848319	8443.315504	26.560333
206.555179	8442.459646	26.565351
206.201532	8456.182291	26.570368
206.516816	8461.986213	26.575386
206.846488	8470.664045	26.580404
206.961249	8477.825387	26.585421
207.193360	8489.801948	26.590439
207.197788	8492.443753	26.595456
207.415635	8509.638178	26.600474
207.722506	8528.422510	26.605492
207.926449	8527.875906	26.610509
208.106473	8534.749217	26.615527
208.410836	8555.772396	26.620544
208.364686	8565.901456	26.625562
209.043175	8578.610067	26.630580
208.899909	8586.651680	26.635597
209.298815	8610.845693	26.640615
209.248282	8616.268124	26.645632
209.472729	8617.915699	26.650650
209.650082	8637.405538	26.655668
209.786434	8647.581826	26.660685
210.074187	8656.919848	26.665703
210.227436	8677.783722	26.670720
210.076938	8697.081880	26.675738
210.631755	8704.366961	26.680756
210.575023	8727.319115	26.685773
210.819551	8737.566907	26.690791
211.099035	8751.256886	26.695808
210.598809	8775.187848	26.700826
211.719904	8786.359167	26.705844
211.697796	8807.856840	26.710861
212.032787	8819.388118	26.715879
211.834589	8837.633072	26.720896
212.298245	8845.257683	26.725914
212.747460	8868.721151	26.730932
213.025825	8881.874675	26.735949
213.675160	8897.748450	26.740967
213.883838	8905.709808	26.745984
213.577371	8907.595285	26.751002
213.931892	8913.863628	26.756020
214.365033	8929.919688	26.761037
214.701721	8934.217566	26.766055
214.519937	8933.529315	26.771072
214.453433	8948.435502	26.776090
215.061695	8963.914799	26.781108
214.866358	8977.714059	26.786125
215.340370	8982.391404	26.791143
215.167228	8996.711303	26.796160
215.490532	9012.168979	26.801178
215.995758	9024.355680	26.806196
215.802737	9049.347061	26.811213
215.828564	9058.593714	26.816231
216.320297	9066.971758	26.821248
216.623067	9098.692569	26.826266
216.934926	9103.897351	26.831284
216.653488	9122.010390	26.836301
217.270414	9134.078633	26.841319
217.693770	9155.390105	26.846336
218.026746	9170.546458	26.851354
218.183137	9183.858225	26.856372
217.821444	9196.733370	26.861389
218.537615	9200.018366	26.866407
218.522445	9224.104397	26.871424
218.782547	9253.271605	26.876442
219.134688	9255.338096	26.881460
218.976245	9270.622031	26.886477
219.952826	9289.898947	26.891495
220.167587	9300.038051	26.896512
220.556903	9307.532422	26.901530
220.485249	9313.915024	26.906548
220.437928	9331.085447	26.911565
221.162779	9338.842996	26.916583
221.425800	9350.202756	26.921600
221.304095	9361.941679	26.926618
221.692624	9372.726106	26.931636
221.745382	9381.365656	26.936653
221.870355	9396.993644	26.941671
222.158756	9403.790311	26.946688
222.494470	9427.174390	26.951706
222.657913	9442.430142	26.956724
222.675793	9458.374902	26.961741
223.038756	9461.270096	26.966759
223.436555	9484.104620	26.971776
223.139770	9497.178186	26.976794
223.354776	9512.179646	26.981812
223.906702	9525.969598	26.986829
224.120244	9551.172649	26.991847
224.115336	9560.509614	26.996864
224.274986	9585.279126	27.001882
224.666675	9593.392079	27.006900
224.827750	9621.729211	27.011917
225.667130	9625.244413	27.016935
225.519607	9642.203492	27.021952
225.448438	9656.166928	27.026970
225.851724	9672.742956	27.031988
226.200844	9689.646378	27.037005
226.450176	9710.218511	27.042023
226.468176	9728.493616	27.047040
226.719799	9744.269395	27.052058
227.297143	9745.312408	27.057076
227.255269	9760.569011	27.062093
227.390303	9774.478131	27.067111
227.329989	9794.533696	27.072128
227.383065	9816.655388	27.077146
228.119464	9816.770479	27.082164
228.390549	9841.964908	27.087181
228.479609	9855.000382	27.092199
228.868586	9861.282594	27.097216
228.796953	9886.650753	27.102234
229.283706	9891.370538	27.107252
229.485413	9909.885420	27.112269
229.803549	9913.700195	27.117287
230.146438	9928.751420	27.122304
230.067038	9935.861649	27.127322
230.672516	9949.312000	27.132340
230.815079	9969.768536	27.137357
231.056677	9978.230382	27.142375
231.255783	9988.905916	27.147392
231.357778	9996.180353	27.152410
231.455568	10012.504588	27.157428
231.578097	10030.681521	27.162445
232.111074	10044.774782	27.167463
232.461169	10059.967068	27.172480
232.628009	10076.359478	27.177498
233.028397	10083.363028	27.182516
233.288348	10105.389506	27.187533
233.435910	10113.285178	27.192551
233.483519	10123.245684	27.197568
233.849570	10140.538384	27.202586
233.934166	10152.668582	27.207604
234.485217	10166.345480	27.212621
234.393406	10177.527681	27.217639
234.917559	10190.034244	27.222656
234.885049	10204.955053	27.227674
235.128685	10216.409945	27.232692
235.201916	10225.605547	27.237709
235.500997	10242.738331	27.242727
236.041036	10254.279427	27.247744
236.196798	10284.279216	27.252762
236.466733	10291.050684	27.257780
236.643645	10299.071294	27.262797
236.562022	10321.956688	27.267815
237.226487	10333.402562	27.272832
237.385739	10348.511311	27.277850
237.777226	10359.649485	27.282868
237.982134	10372.424047	27.287885
237.660992	10389.464677	27.292903
238.285629	10406.142455	27.297920
238.095275	10432.600337	27.302938
238.648184	10443.227022	27.307956
238.857843	10459.335201	27.312973
239.154919	10481.987805	27.317991
239.687490	10491.803071	27.323008
239.760047	10504.917363	27.328026
239.684775	10520.018785	27.333044
239.756232	10539.609299	27.338061
240.373395	10555.634780	27.343079
240.567211	10569.424772	27.348096
240.201310	10595.765139	27.353114
240.801243	10613.741552	27.358132
241.186966	10636.636214	27.363149
241.418149	10653.549513	27.368167
241.484329	10666.585980	27.373184
241.642939	10692.825371	27.378202
242.155266	10701.860853	27.383220
242.356144	10718.213761	27.388237
242.920893	10745.611568	27.393255
243.272728	10759.932672	27.398272
243.313915	10767.343237	27.403290
243.907858	10787.480512	27.408308
243.864071	10790.300703	27.413325
244.296778	10820.627401	27.418343
244.484899	10823.998572	27.423360
244.411483	10828.967385	27.428378
244.642101	10838.463861	27.433396
244.552099	10859.920854	27.438413
245.038184	10878.250057	27.443431
245.361604	10880.318076	27.448448
245.306497	10910.484519	27.453466
245.929244	10923.291886	27.458484
246.304465	10927.429473	27.463501
246.295868	10956.764581	27.468519
246.444610	10965.102488	27.473536
246.760230	10989.622084	27.478554
246.923589	10992.469850	27.483572
247.361262	11018.438636	27.488589
247.185480	11033.489906	27.493607
247.446424	11053.783834	27.498624
247.815875	11077.808844	27.503642
248.071895	11086.133158	27.508660
248.550198	11104.858501	27.513677
248.764551	11131.067671	27.518695
249.282875	11148.896346	27.523712
249.319155	11162.487264	27.528730
249.471434	11165.254694	27.533748
249.942212	11193.902502	27.538765
250.052884	11209.082708	27.543783
250.512987	11224.432378	27.548800
250.603958	11242.438605	27.553818
251.070885	11252.270871	27.558836
251.262918	11264.729140	27.563853
251.301822	11283.555071	27.568871
251.681678	11307.319820	27.573888
251.672950	11318.735980	27.578906
252.397429	11341.812104	27.583924
252.837961	11356.956545	27.588941
253.093857	11369.395406	27.593959
253.092179	11384.463890	27.598976
253.182307	11393.464802	27.603994
253.415984	11407.132334	27.609012
253.692972	11425.516933	27.614029
253.616262	11446.691483	27.619047
254.373750	11468.152190	27.624064
254.519216	11479.847428	27.629082
254.397289	11505.250916	27.634100
254.848500	11525.357665	27.639117
255.173234	11548.364042	27.644135
255.431360	11560.199565	27.649152
255.389077	11579.044825	27.654170
255.495804	11593.992292	27.659188
256.184800	11614.908145	27.664205
256.242721	11629.500153	27.669223
256.889156	11643.564220	27.674240
256.928622	11666.830152	27.679258
257.085207	11684.741266	27.684276
257.652233	11698.476783	27.689293
257.733332	11721.688896	27.694311
258.147061	11736.345241	27.699328
258.325844	11754.357149	27.704346
258.436662	11769.683039	27.709364
259.109620	11788.043856	27.714381
259.171802	11799.676555	27.719399
259.390468	11823.489312	27.724416
259.640979	11837.517658	27.729434
259.625496	11849.822517	27.734452
260.019328	11867.488231	27.739469
260.058733	11892.589088	27.744487
260.777622	11899.530799	27.749504
260.782598	11927.175909	27.754522
260.901056	11949.473023	27.759540
261.177190	11958.893466	27.764557
261.696979	11981.778244	27.769575
262.079535	11993.553498	27.774592
262.201794	12008.678853	27.779610
262.547233	12023.886095	27.784628
262.697965	12033.831460	27.789645
262.793699	12057.085902	27.794663
263.389111	12064.356477	27.799680
263.689270	12084.345388	27.804698
263.419363	12111.992779	27.809716
263.892248	12116.604785	27.814733
264.190095	12130.739614	27.819751
264.260367	12150.796185	27.824768
264.592572	12165.951933	27.829786
264.811957	12173.151987	27.834804
265.233360	12205.222626	27.839821
265.433114	12223.446426	27.844839
265.684854	12248.081878	27.849856
265.948425	12265.743109	27.854874
265.824110	12285.214536	27.859892
266.209022	12299.569529	27.864909
266.661486	12332.844955	27.869927
267.145746	12346.597070	27.874944
267.746139	12362.118322	27.879962
267.212489	12392.276841	27.884980
268.128237	12404.947749	27.889997
268.224780	12428.300414	27.895015
268.095561	12449.875884	27.900032
268.760780	12468.169108	27.905050
269.194081	12482.450346	27.910068
269.264266	12502.687301	27.915085
269.201783	12527.486022	27.920103
269.804680	12544.857522	27.925120
270.192364	12558.391242	27.930138
270.258178	12578.812117	27.935156
270.818330	12605.310217	27.940173
270.907727	12621.565404	27.945191
271.155042	12630.892805	27.950208
271.536691	12652.650581	27.955226
271.595291	12663.542278	27.960244
271.879551	12682.628009	27.965261
272.258561	12708.384112	27.970279
272.084284	12732.360623	27.975296
272.724178	12757.690666	27.980314
273.021451	12788.831222	27.985332
273.784994	12797.913631	27.990349
273.553755	12817.294986	27.995367
273.764408	12833.635571	28.000384
274.081073	12854.450078	28.005402
274.592407	12873.137274	28.010420
274.841981	12899.349702	28.015437
275.231707	12920.159153	28.020455
275.752009	12923.699720	28.025472
275.953189	12950.434538	28.030490
276.146869	12964.573678	28.035508
276.424796	12975.800672	28.040525
276.545621	12998.733393	28.045543
276.791336	13016.625494	28.050560
276.969122	13032.175604	28.055578
277.074653	13056.601328	28.060596
277.546997	13072.206383	28.065613
277.634716	13097.386535	28.070631
278.021958	13113.121798	28.075648
278.516382	13126.288675	28.080666
278.801818	13158.019068	28.085684
279.140778	13172.126132	28.090701
279.188634	13192.102054	28.095719
279.541540	13214.474463	28.100736
279.841267	13223.828685	28.105754
279.743278	13241.547466	28.110772
280.231153	13262.900877	28.115789
280.406532	13284.555900	28.120807
280.647801	13306.001675	28.125824
280.917011	13319.914507	28.130842
281.101402	13354.140060	28.135860
281.584191	13366.844705	28.140877
281.834231	13389.151327	28.145895
281.837821	13406.522763	28.150912
282.684931	13419.479855	28.155930
282.548046	13448.453656	28.160948
283.219847	13461.387711	28.165965
283.236597	13478.753994	28.170983
283.625537	13491.972387	28.176000
284.019109	13520.746357	28.181018
284.119227	13544.883022	28.186036
284.439490	13554.471041	28.191053
284.757288	13577.976786	28.196071
284.966698	13592.338149	28.201088
285.496882	13617.459155	28.206106
285.812435	13638.612606	28.211124
285.806900	13644.282078	28.216141
286.201603	13675.295141	28.221159
286.659761	13694.288333	28.226176
287.025417	13703.382981	28.231194
286.976200	13734.588843	28.236212
287.345766	13754.265476	28.241229
287.390044	13772.202477	28.246247
287.869136	13792.550446	28.251264
288.293358	13805.611946	28.256282
288.430603	13832.733830	28.261300
288.858557	13849.031776	28.266317
289.042403	13873.023104	28.271335
289.160578	13900.846002	28.276352
289.914805	13916.069685	28.281370
289.956925	13944.315109	28.286388
290.514183	13955.325235	28.291405
290.664949	13972.952043	28.296423
290.750630	14001.582330	28.301440
291.343227	14015.302902	28.306458
291.405518	14047.922420	28.311476
291.455595	14057.474065	28.316493
291.816494	14087.015111	28.321511
292.317882	14108.149449	28.326528
292.881885	14123.014651	28.331546
292.801550	14149.274169	28.336564
293.073967	14175.851122	28.341581
293.620451	14196.233181	28.346599
293.579162	14219.710701	28.351616
294.448001	14234.032414	28.356634
294.576982	14257.151706	28.361652
294.569149	14283.892719	28.366669
294.994459	14308.930008	28.371687
294.908887	14318.275648	28.376704
295.541200	14342.238371	28.381722
295.796216	14365.113823	28.386740
296.427343	14389.316811	28.391757
296.367091	14415.630396	28.396775
296.509657	14427.416339	28.401792
297.133149	14443.570473	28.406810
297.373856	14467.897881	28.411828
297.559124	14493.342519	28.416845
297.735516	14514.502953	28.421863
298.359991	14540.039919	28.426880
298.798847	14548.273960	28.431898
299.046063	14578.414679	28.436916
299.404338	14592.478717	28.441933
299.347181	14609.819710	28.446951
299.930430	14627.101457	28.451968
300.188147	14645.015320	28.456986
300.205789	14662.527817	28.462004
300.438091	14682.062688	28.467021
301.140149	14696.234019	28.472039
300.955056	14715.903787	28.477056
301.195145	14736.981852	28.482074
301.484274	14759.258692	28.487092
302.206273	14785.762912	28.492109
302.555380	14802.557234	28.497127
302.564446	14829.520597	28.502144
302.687318	14854.173303	28.507162
302.937855	14860.993673	28.512180
303.281800	14893.677895	28.517197
303.571818	14916.965412	28.522215
303.945599	14942.400068	28.527232
304.445236	14973.951499	28.532250
304.336487	14997.974285	28.537268
304.844840	15024.505987	28.542285
305.453964	15041.424018	28.547303
305.311761	15058.965076	28.552320
306.300927	15084.581450	28.557338
306.437157	15103.279072	28.562356
306.615348	15127.705545	28.567373
307.192349	15142.765322	28.572391
307.195242	15166.455003	28.577408
307.704504	15181.342242	28.582426
307.850145	15215.668798	28.587444
308.303948	15233.208244	28.592461
308.997341	15260.061858	28.597479
308.990240	15277.850408	28.602496
309.265172	15289.177147	28.607514
309.629690	15320.750317	28.612532
309.778479	15332.093683	28.617549
310.100768	15355.907274	28.622567
309.955954	15388.293065	28.627584
310.334242	15402.600915	28.632602
310.587674	15440.028240	28.637620
311.244890	15468.855445	28.642637
311.771400	15490.135823	28.647655
312.015668	15511.874177	28.652672
312.399460	15525.666449	28.657690
312.766021	15556.162697	28.662708
312.805130	15575.251835	28.667725
313.160673	15597.402389	28.672743
313.467259	15619.254279	28.677760
314.426724	15647.655407	28.682778
314.309136	15662.814923	28.687796
314.608520	15691.584816	28.692813
315.101607	15710.618767	28.697831
315.204541	15733.867100	28.702848
315.636171	15755.348979	28.707866
315.797843	15767.897081	28.712884
316.377490	15796.338976	28.717901
316.363099	15822.502024	28.722919
316.681358	15844.769248	28.727936
317.091590	15871.393298	28.732954
317.664255	15889.413752	28.737972
317.916621	15917.010111	28.742989
317.908625	15936.375449	28.748007
317.951893	15950.360338	28.753024
318.277249	15979.622463	28.758042
318.960519	16008.822251	28.763060
319.391713	16030.124477	28.768077
319.611002	16048.772109	28.773095
320.003686	16080.547415	28.778112
320.543093	16091.492092	28.783130
320.423047	16105.783776	28.788148
321.004148	16129.418816	28.793165
321.358479	16153.812688	28.798183
320.995294	16166.926507	28.803200
321.375687	16189.481291	28.808218
321.827060	16224.788253	28.813236
322.094114	16239.925873	28.818253
322.754195	16256.685394	28.823271
322.717626	16291.898356	28.828288
323.251716	16306.643611	28.833306
323.437589	16330.078656	28.838324
323.712022	16360.420056	28.843341
324.136550	16386.729893	28.848359
324.443189	16409.369133	28.853376
324.684517	16431.671198	28.858394
324.969430	16460.529788	28.863412
325.009520	16487.935965	28.868429
325.730094	16507.415163	28.873447
325.801721	16537.655954	28.878464
326.384816	16561.404919	28.883482
326.717150	16594.289686	28.888500
326.836942	16620.214861	28.893517
327.579536	16640.395093	28.898535
327.861865	16667.368766	28.903552
328.393133	16694.208726	28.908570
328.484846	16721.727173	28.913588
328.680287	16744.867480	28.918605
329.303277	16771.232036	28.923623
329.305462	16807.684330	28.928640
330.061629	16827.486767	28.933658
330.129259	16855.024968	28.938676
330.641807	16879.300220	28.943693
330.829757	16902.662989	28.948711
331.135916	16938.268801	28.953728
331.297849	16953.960405	28.958746
331.810913	16993.475796	28.963764
331.994361	17010.863387	28.968781
332.715038	17033.188977	28.973799
332.478197	17058.071420	28.978816
332.866316	17088.332986	28.983834
333.504416	17117.247786	28.988852
333.929143	17142.348883	28.993869
334.478631	17173.444444	28.998887
334.697015	17195.223499	29.003904
335.105320	17214.654413	29.008922
335.130389	17241.719724	29.013940
335.839534	17272.367181	29.018957
336.105873	17288.762867	29.023975
336.218308	17324.494495	29.028992
336.628230	17347.974646	29.034010
337.189918	17375.872090	29.039028
337.269833	17399.176575	29.044045
337.868846	17418.767339	29.049063
338.146712	17444.428803	29.054080
338.196100	17463.518200	29.059098
338.884212	17494.952649	29.064116
339.116687	17521.088805	29.069133
339.474512	17537.280853	29.074151
339.314508	17567.477413	29.079168
339.535170	17589.206017	29.084186
340.244128	17621.332313	29.089204
340.335108	17644.553235	29.094221
340.923519	17675.953057	29.099239
341.346894	17704.220096	29.104256
341.471829	17723.519023	29.109274
341.937361	17754.148548	29.114292
342.084795	17795.649656	29.119309
342.741801	17818.061938	29.124327
342.995810	17843.727668	29.129344
343.463834	17871.520468	29.134362
343.769756	17893.090757	29.139380
343.903252	17913.247702	29.144397
344.292348	17923.414655	29.149415
344.638250	17958.978215	29.154432
345.058596	17984.548584	29.159450
345.385078	18005.237650	29.164468
346.008666	18034.800479	29.169485
346.311992	18045.947506	29.174503
346.533716	18070.279286	29.179520
346.702746	18092.351369	29.184538
347.388175	18115.517644	29.189556
347.596000	18150.957882	29.194573
347.942544	18165.560208	29.199591
348.260940	18196.011319	29.204608
348.630115	18213.295088	29.209626
348.865483	18237.309063	29.214644
349.035546	18274.012632	29.219661
349.283576	18303.520982	29.224679
349.846772	18331.691224	29.229696
350.044914	18351.832181	29.234714
350.381272	18384.675138	29.239732
350.520352	18416.361342	29.244749
351.048123	18447.544480	29.249767
351.159926	18476.000436	29.254784
351.729751	18505.262840	29.259802
352.090584	18549.303407	29.264820
352.427411	18579.291043	29.269837
352.951805	18596.051744	29.274855
353.526184	18630.557284	29.279872
353.395699	18648.349308	29.284890
354.144700	18683.749970	29.289908
354.280352	18711.810839	29.294925
354.705274	18744.324645	29.299943
355.214043	18775.441791	29.304960
355.217721	18805.488278	29.309978
355.765988	18838.298807	29.314996
356.056285	18867.618177	29.320013
356.793802	18897.758343	29.325031
357.068954	18925.266975	29.330048
356.922140	18959.020530	29.335066
357.442911	18986.263335	29.340084
357.834603	19030.034808	29.345101
358.512673	19046.171635	29.350119
359.079369	19067.613931	29.355136
359.052185	19109.088331	29.360154
359.568789	19136.117192	29.365172
359.948346	19161.360654	29.370189
360.553334	19179.638153	29.375207
361.008962	19216.690474	29.380224
360.921928	19245.810485	29.385242
361.554242	19272.581332	29.390260
361.492303	19305.873621	29.395277
361.876703	19334.281812	29.400295
362.088901	19369.571951	29.405312
362.541383	19391.948592	29.410330
363.137626	19418.314625	29.415348
363.631197	19460.611663	29.420365
363.839942	19484.618711	29.425383
364.447270	19512.366765	29.430400
364.291844	19541.074625	29.435418
365.018108	19568.102834	29.440436
365.460265	19601.512522	29.445453
365.588643	19628.729237	29.450471
366.287313	19657.019173	29.455488
366.200708	19684.636084	29.460506
366.968868	19717.994907	29.465524
367.409493	19746.773972	29.470541
367.804099	19765.710462	29.475559
368.210249	19791.955142	29.480576
367.902296	19815.999304	29.485594
368.597436	19837.453919	29.490612
368.536631	19871.258754	29.495629
368.771314	19898.408648	29.500647
369.568179	19932.812143	29.505664
369.955764	19965.586556	29.510682
370.638112	19987.814149	29.515700
370.653037	20021.910651	29.520717
370.889010	20045.629806	29.525735
371.235343	20075.725660	29.530752
371.737667	20108.052705	29.535770
372.020517	20126.849096	29.540788
372.520146	20165.640133	29.545805
372.842763	20200.364793	29.550823
373.257135	20233.091230	29.555840
373.474278	20256.162816	29.560858
374.164446	20292.100024	29.565876
374.657148	20331.486386	29.570893
374.431845	20356.308040	29.575911
375.122892	20384.713952	29.580928
375.186420	20418.354934	29.585946
375.703826	20453.289623	29.590964
376.327449	20497.116504	29.595981
376.638817	20517.538917	29.600999
377.256130	20547.877372	29.606016
377.455167	20583.626676	29.611034
377.987056	20611.438652	29.616052
378.015245	20638.918875	29.621069
378.529277	20679.332480	29.626087
379.522280	20714.111000	29.631104
379.259447	20740.992479	29.636122
379.636645	20766.541662	29.641140
379.924245	20802.403858	29.646157
380.333487	20837.501496	29.651175
380.744299	20873.742580	29.656192
380.825809	20902.889194	29.661210
381.681661	20930.518192	29.666228
381.921568	20975.082312	29.671245
381.823844	21005.230190	29.676263
382.621670	21041.253002	29.681280
382.801940	21089.289232	29.686298
383.386456	21121.049046	29.691316
383.776277	21164.181092	29.696333
384.275395	21194.640156	29.701351
384.457261	21226.646446	29.706368
385.072306	21272.277173	29.711386
385.633168	21295.062353	29.716404
386.133392	21329.742231	29.721421
386.435939	21362.702894	29.726439
387.032911	21390.335177	29.731456
386.634915	21427.228409	29.736474
386.929563	21460.575906	29.741492
387.603281	21501.686504	29.746509
387.872735	21534.267204	29.751527
388.786550	21564.409138	29.756544
388.998728	21605.371095	29.761562
389.690308	21631.750446	29.766580
389.845185	21676.645401	29.771597
390.264543	21699.263653	29.776615
390.742354	21720.356296	29.781632
391.122457	21759.624142	29.786650
391.487441	21791.027664	29.791668
391.932961	21819.126579	29.796685
392.509128	21855.653183	29.801703
393.000030	21883.757719	29.806720
393.269717	21909.464236	29.811738
393.706765	21940.174284	29.816756
394.270908	21969.935618	29.821773
394.246377	21985.123376	29.826791
394.714480	22009.813218	29.831808
395.034790	22037.672987	29.836826
394.863796	22068.358419	29.841844
395.760454	22103.344050	29.846861
396.016551	22128.838141	29.851879
396.310415	22163.785602	29.856896
396.408142	22198.618515	29.861914
397.175735	22226.945590	29.866932
397.332932	22267.001297	29.871949
397.684986	22308.448306	29.876967
397.930755	22336.838318	29.881984
398.283694	22379.087832	29.887002
398.857258	22405.019105	29.892020
399.360960	22450.158161	29.897037
399.520365	22492.223388	29.902055
400.167681	22525.435293	29.907072
400.525758	22566.407978	29.912090
400.637737	22599.501654	29.917108
401.897026	22631.998625	29.922125
401.835113	22677.852371	29.927143
402.359377	22709.712642	29.932160
402.642102	22746.621759	29.937178
403.071665	22779.072004	29.942196
403.394702	22813.497882	29.947213
403.901265	22849.727590	29.952231
404.286011	22879.979679	29.957248
404.667712	22937.517948	29.962266
405.033393	22960.518873	29.967284
405.336145	23003.194633	29.972301
405.864898	23041.083131	29.977319
406.417351	23068.610989	29.982336
406.731418	23114.994526	29.987354
407.443185	23152.513338	29.992372
407.961886	23182.688034	29.997389
407.901299	23219.677079	30.002407
408.257547	23252.992665	30.007424
408.595629	23296.952628	30.012442
409.260151	23323.862965	30.017460
410.007772	23376.612124	30.022477
409.954519	23408.993680	30.027495
410.496996	23438.729015	30.032512
410.928390	23482.327214	30.037530
411.330435	23513.335863	30.042548
411.730847	23547.611867	30.047565
411.641770	23590.413450	30.052583
412.605605	23636.146648	30.057600
413.107592	23674.729345	30.062618
413.482596	23717.869264	30.067636
413.912661	23745.941731	30.072653
414.127067	23793.429377	30.077671
414.708530	23812.441591	30.082688
415.131023	23855.877697	30.087706
415.548026	23894.455172	30.092724
416.160600	23937.533077	30.097741
416.298972	23973.955207	30.102759
416.975324	24010.444804	30.107776
417.363080	24043.725178	30.112794
417.620926	24088.691597	30.117812
418.003369	24118.471971	30.122829
418.491831	24160.798826	30.127847
419.151233	24184.102727	30.132864
419.571072	24224.734216	30.137882
419.470569	24259.980945	30.142900
420.386524	24300.073558	30.147917
421.016917	24327.243375	30.152935
421.387294	24353.335404	30.157952
421.509421	24383.719382	30.162970
421.517227	24411.517669	30.167988
422.112300	24442.965172	30.173005
422.613797	24486.864238	30.178023
423.247466	24515.417778	30.183040
423.510601	24552.181632	30.188058
423.846919	24580.244676	30.193076
424.396957	24612.710630	30.198093
424.600829	24656.669325	30.203111
424.895563	24684.618956	30.208128
425.565245	24727.019738	30.213146
425.889713	24759.736129	30.218164
426.122579	24790.672144	30.223181
426.465192	24845.978555	30.228199
427.139590	24880.883812	30.233216
427.395168	24915.216442	30.238234
427.597918	24951.149967	30.243252
428.399864	24991.533569	30.248269
428.882487	25035.961328	30.253287
429.199380	25072.919946	30.258304
429.818277	25113.294545	30.263322
429.993799	25160.652483	30.268340
430.365172	25198.064139	30.273357
430.527427	25248.622164	30.278375
431.455302	25294.105674	30.283392
431.909876	25332.983382	30.288410
432.479362	25379.060404	30.293428
432.971545	25411.239680	30.298445
433.002854	25452.844565	30.303463
433.565175	25487.136446	30.308480
433.977701	25527.259807	30.313498
434.344376	25572.370497	30.318516
434.844044	25606.293201	30.323533
435.415636	25652.029242	30.328551
435.790989	25699.489864	30.333568
436.248360	25734.936191	30.338586
436.825711	25780.513623	30.343604
437.450264	25825.470729	30.348621
437.590185	25862.686033	30.353639
437.762531	25901.425763	30.358656
438.584197	25950.207465	30.363674
438.746442	25992.879995	30.368692
439.687081	26025.337611	30.373709
439.971945	26069.223501	30.378727
440.303765	26109.341700	30.383744
440.534960	26150.082465	30.388762
440.811839	26199.449384	30.393780
441.353068	26232.721984	30.398797
441.459902	26281.515328	30.403815
441.959740	26324.129359	30.408832
442.710569	26388.078864	30.413850
443.157794	26427.579205	30.418868
443.698361	26459.834737	30.423885
444.260948	26511.647811	30.428903
444.614609	26565.914375	30.433920
445.241747	26599.547013	30.438938
445.622347	26650.687404	30.443956
446.426399	26686.378149	30.448973
446.608154	26721.306875	30.453991
447.060664	26759.037366	30.459008
447.607486	26809.210404	30.464026
448.225700	26846.365240	30.469044
448.864807	26880.710663	30.474061
449.170085	26914.204628	30.479079
449.396564	26951.553740	30.484096
450.058472	26985.699840	30.489114
450.219952	27033.348774	30.494132
451.112411	27059.716473	30.499149
451.568881	27091.904020	30.504167
451.964088	27119.639033	30.509184
451.999580	27146.678302	30.514202
452.161051	27188.354849	30.519220
452.459680	27216.313694	30.524237
452.682509	27263.112945	30.529255
453.709348	27308.111461	30.534272
453.830145	27335.207143	30.539290
454.042014	27384.656652	30.544308
454.803564	27431.119093	30.549325
455.454193	27473.515985	30.554343
455.666754	27520.943165	30.559360
456.103661	27565.086576	30.564378
456.661676	27608.774998	30.569396
457.145988	27647.620890	30.574413
457.863311	27698.192892	30.579431
457.850953	27739.347904	30.584448
459.017328	27779.648397	30.589466
459.139293	27827.969039	30.594484
459.617234	27863.510675	30.599501
460.209762	27910.575858	30.604519
460.097698	27944.282259	30.609536
460.951026	27993.114482	30.614554
461.087674	28040.769661	30.619572
461.771750	28080.988275	30.624589
461.944939	28129.870467	30.629607
462.716809	28179.101456	30.634624
462.971811	28221.328004	30.639642
463.651872	28267.021347	30.644660
464.159679	28311.167909	30.649677
464.867414	28352.704386	30.654695
465.497417	28402.160397	30.659712
465.731925	28446.621850	30.664730
466.227605	28494.689589	30.669748
466.677199	28521.646856	30.674765
467.275265	28568.605234	30.679783
467.560470	28623.678102	30.684800
468.159381	28659.101042	30.689818
468.263809	28708.033309	30.694836
469.179552	28741.971933	30.699853
469.515865	28786.279119	30.704871
469.927576	28834.196464	30.709888
470.537243	28875.104631	30.714906
470.716983	28914.544234	30.719924
471.215243	28958.978130	30.724941
471.901226	29012.807255	30.729959
472.516565	29063.158413	30.734976
472.931406	29104.186045	30.739994
473.367854	29145.475858	30.745012
474.064237	29189.443073	30.750029
474.221888	29231.307689	30.755047
474.486148	29274.325083	30.760064
475.125314	29317.302810	30.765082
475.348178	29359.593626	30.770100
475.921058	29408.580611	30.775117
476.487770	29454.060475	30.780135
477.272975	29503.728714	30.785152
477.587932	29539.166043	30.790170
477.832475	29588.862279	30.795188
478.769825	29635.795244	30.800205
479.018354	29685.446841	30.805223
479.511227	29721.640441	30.810240
479.923923	29760.779691	30.815258
480.456565	29819.811995	30.820276
481.169894	29850.073614	30.825293
481.540849	29900.313389	30.830311
481.727891	29934.380764	30.835328
482.216814	29982.560504	30.840346
482.707343	30023.887857	30.845364
483.480525	30064.033193	30.850381
483.744103	30102.874063	30.855399
483.734475	30150.993214	30.860416
484.342705	30196.796923	30.865434
485.041791	30244.438653	30.870452
485.453583	30279.628198	30.875469
486.164490	30336.832479	30.880487
486.232830	30375.508478	30.885504
486.952626	30416.440390	30.890522
486.966648	30463.734784	30.895540
487.525572	30504.300140	30.900557
488.231158	30553.528239	30.905575
488.963412	30609.396110	30.910592
489.534046	30651.824746	30.915610
489.841287	30705.306720	30.920628
490.302188	30753.031179	30.925645
490.663404	30796.017594	30.930663
490.902660	30847.329666	30.935680
491.410916	30896.943492	30.940698
492.246738	30951.740371	30.945716
492.753012	30996.973918	30.950733
493.272280	31051.131590	30.955751
493.607612	31105.204423	30.960768
494.483823	31154.849739	30.965786
494.692336	31208.544443	30.970804
495.335153	31260.856362	30.975821
496.141967	31311.164050	30.980839
496.419739	31360.853015	30.985856
496.818424	31401.318792	30.990874
497.112523	31449.627285	30.995892
497.802135	31507.533520	31.000909
498.472506	31559.589008	31.005927
498.701301	31607.857523	31.010944
499.712006	31655.870928	31.015962
500.126621	31702.403684	31.020980
500.198147	31746.929378	31.025997
500.838110	31790.209247	31.031015
501.340550	31850.225623	31.036032
502.266981	31907.887261	31.041050
502.282018	31957.441788	31.046068
503.032220	31990.166287	31.051085
503.552674	32051.223527	31.056103
503.994914	32105.067269	31.061120
504.449566	32147.586668	31.066138
505.020965	32199.507532	31.071156
505.515055	32247.761264	31.076173
506.351043	32301.714537	31.081191
506.546986	32341.809289	31.086208
507.031230	32404.194524	31.091226
507.745578	32444.619209	31.096244
508.203779	32494.624004	31.101261
508.941295	32546.342696	31.106279
508.901757	32589.382937	31.111296
509.638379	32647.392451	31.116314
510.125358	32696.185708	31.121332
510.444758	32742.773628	31.126349
511.290654	32785.953767	31.131367
511.499861	32839.159434	31.136384
512.322339	32891.270287	31.141402
512.353790	32951.698667	31.146420
513.196489	32992.508927	31.151437
513.682895	33038.609830	31.156455
514.314764	33099.886603	31.161472
514.982894	33149.480751	31.166490
515.538112	33196.772445	31.171508
515.695748	33236.818010	31.176525
516.358964	33283.612495	31.181543
516.557354	33334.045643	31.186560
516.963014	33373.932500	31.191578
517.337426	33423.838835	31.196596
518.049237	33475.418435	31.201613
518.605291	33529.412394	31.206631
519.026766	33577.307546	31.211648
519.613810	33621.168504	31.216666
520.013962	33669.301132	31.221684
520.672805	33722.944404	31.226701
521.481361	33776.848873	31.231719
521.749463	33825.824453	31.236736
522.350400	33867.192718	31.241754
522.969672	33915.595067	31.246772
523.180297	33966.849732	31.251789
523.892922	34008.706580	31.256807
523.969641	34078.646420	31.261824
524.215963	34129.415380	31.266842
524.818861	34194.727316	31.271860
525.795473	34246.735200	31.276877
526.618056	34304.552475	31.281895
526.716819	34367.250493	31.286912
527.384159	34401.806319	31.291930
528.061742	34463.010353	31.296948
528.292858	34520.212722	31.301965
528.808321	34574.904883	31.306983
529.444981	34637.418295	31.312000
529.728785	34693.146023	31.317018
530.580533	34765.717114	31.322036
530.905737	34823.480932	31.327053
531.599643	34877.342943	31.332071
532.135706	34944.412735	31.337088
532.913272	34987.348865	31.342106
533.481673	35051.018609	31.347124
534.149631	35103.026361	31.352141
534.907171	35151.327691	31.357159
535.351850	35223.376084	31.362176
535.626902	35265.348214	31.367194
536.032661	35316.480743	31.372212
536.384066	35381.203444	31.377229
537.280184	35428.724956	31.382247
537.778341	35503.516382	31.387264
538.582458	35543.958254	31.392282
539.150491	35600.472154	31.397300
539.493935	35653.923129	31.402317
540.511231	35706.345546	31.407335
540.704023	35758.821350	31.412352
541.057306	35812.309120	31.417370
541.676297	35860.760224	31.422388
542.168606	35923.704708	31.427405
543.228656	35978.915885	31.432423
543.357315	36028.335716	31.437440
543.860284	36084.323630	31.442458
544.457062	36143.370027	31.447476
544.803545	36199.332167	31.452493
545.354766	36246.877911	31.457511
545.597860	36317.665338	31.462528
546.294513	36359.719028	31.467546
547.184479	36421.142048	31.472564
547.483963	36482.632433	31.477581
547.983404	36534.132606	31.482599
548.573962	36602.432118	31.487616
549.186138	36666.921861	31.492634
549.919940	36718.904281	31.497652
550.206499	36766.619099	31.502669
550.781168	36818.291550	31.507687
551.148974	36879.626939	31.512704
551.442090	36939.083523	31.517722
552.020660	36993.032187	31.522740
552.411112	37058.999562	31.527757
553.487196	37115.684517	31.532775
553.608032	37170.483093	31.537792
554.201138	37220.869977	31.542810
554.679099	37289.872245	31.547828
555.090132	37343.184068	31.552845
556.057356	37406.368387	31.557863
556.597463	37478.352532	31.562880
557.279312	37523.534638	31.567898
557.662946	37578.735743	31.572916
558.154166	37649.305324	31.577933
558.997625	37696.517636	31.582951
559.266783	37765.566782	31.587968
559.581417	37827.653066	31.592986
560.744961	37887.336397	31.598004
561.009503	37939.268798	31.603021
561.583535	37999.999638	31.608039
561.825538	38068.086487	31.613056
562.599569	38135.489477	31.618074
563.543761	38195.966862	31.623092
563.773253	38264.872050	31.628109
564.000438	38313.750520	31.633127
564.491186	38386.371482	31.638144
565.535672	38455.187579	31.643162
566.077459	38523.228913	31.648180
566.569220	38589.121873	31.653197
567.227482	38645.983808	31.658215
567.660384	38719.253656	31.663232
567.939576	38784.118093	31.668250
569.100458	38853.948025	31.673268
569.818713	38925.188175	31.678285
570.418621	38990.148451	31.683303
570.546335	39057.573330	31.688320
571.107573	39107.956970	31.693338
571.823338	39178.407847	31.698356
572.345593	39253.840963	31.703373
572.783676	39312.060851	31.708391
573.282543	39383.064933	31.713408
573.950470	39451.500491	31.718426
574.738444	39520.050271	31.723444
575.269133	39595.989183	31.728461
576.272970	39655.373561	31.733479
576.427662	39716.851577	31.738496
577.151139	39788.207579	31.743514
577.496119	39852.021415	31.748532
578.407050	39935.250670	31.753549
579.027038	39996.321420	31.758567
579.260527	40046.562516	31.763584
580.145852	40129.379124	31.768602
580.659424	40193.300365	31.773620
581.493662	40255.305903	31.778637
582.175847	40321.218567	31.783655
582.792262	40381.747064	31.788672
583.110918	40442.733446	31.793690
583.991451	40502.816156	31.798708
584.082400	40571.794630	31.803725
585.034583	40632.157397	31.808743
585.923700	40707.019490	31.813760
586.392238	40762.898445	31.818778
586.950980	40822.444257	31.823796
587.497433	40884.072913	31.828813
587.971163	40936.005016	31.833831
588.630603	41003.953468	31.838848
589.133188	41070.826225	31.843866
589.851889	41133.193876	31.848884
589.976432	41203.566806	31.853901
590.819072	41250.356916	31.858919
591.321453	41319.791926	31.863936
591.811140	41373.904560	31.868954
592.431569	41432.044625	31.873972
592.882608	41490.382138	31.878989
593.191216	41553.074520	31.884007
594.032821	41615.677281	31.889024
594.474889	41676.110169	31.894042
594.971029	41737.262098	31.899060
595.616044	41812.469785	31.904077
596.410042	41884.163119	31.909095
597.002521	41948.089774	31.914112
597.540085	42025.199804	31.919130
598.316802	42075.967660	31.924148
598.314214	42147.312243	31.929165
599.040491	42212.603854	31.934183
599.416474	42279.221821	31.939200
600.108603	42366.099768	31.944218
600.910154	42422.727731	31.949236
601.186019	42503.359130	31.954253
602.025174	42580.366944	31.959271
602.834854	42650.542321	31.964288
603.292601	42730.450314	31.969306
603.848090	42798.110661	31.974324
604.577546	42869.520030	31.979341
605.125903	42940.306508	31.984359
605.973171	43018.699770	31.989376
606.794566	43095.484456	31.994394
607.474635	43151.892959	31.999412
608.176215	43224.218657	32.004429
608.740303	43299.570585	32.009447
609.498331	43355.024944	32.014464
609.578842	43423.267603	32.019482
610.574440	43490.083136	32.024500
611.505146	43568.174314	32.029517
611.834328	43629.863649	32.034535
612.306324	43701.252765	32.039552
613.475760	43770.831374	32.044570
613.913953	43825.394525	32.049588
614.416076	43900.410303	32.054605
614.984101	43975.858788	32.059623
615.453559	44046.983745	32.064640
616.083106	44112.770511	32.069658
616.813112	44193.039630	32.074676
617.157949	44255.158374	32.079693
617.911889	44335.145937	32.084711
618.416721	44402.623015	32.089728
619.128570	44466.715354	32.094746
619.904411	44536.566740	32.099764
620.535235	44603.904510	32.104781
621.068450	44676.356179	32.109799
621.795215	44751.573684	32.114816
622.045661	44824.386396	32.119834
622.934778	44890.400479	32.124852
623.650548	44955.689151	32.129869
624.191818	45037.983444	32.134887
625.449072	45100.543607	32.139904
625.574730	45170.890992	32.144922
626.064996	45230.250636	32.149940
626.646978	45305.081502	32.154957
627.459997	45383.374586	32.159975
628.183818	45455.103089	32.164992
629.004224	45533.427169	32.170010
629.378193	45597.986841	32.175028
630.240346	45663.988448	32.180045
630.539943	45728.762569	32.185063
631.274392	45789.331646	32.190080
631.945534	45860.563623	32.195098
632.634480	45922.557188	32.200116
633.154151	45987.019246	32.205133
633.630290	46054.739850	32.210151
634.323111	46107.282335	32.215168
634.566304	46175.564839	32.220186
635.586534	46239.044610	32.225204
635.782348	46311.206463	32.230221
636.945848	46387.816040	32.235239
637.460079	46456.967900	32.240256
637.832897	46523.010703	32.245274
638.349070	46587.639504	32.250292
639.237304	46651.508023	32.255309
639.594512	46730.130219	32.260327
640.360975	46796.194412	32.265344
640.652634	46881.596399	32.270362
641.725903	46949.030058	32.275380
642.350218	47026.327231	32.280397
642.497465	47100.466664	32.285415
643.264251	47176.843711	32.290432
643.772901	47249.478317	32.295450
644.576571	47324.761963	32.300468
645.338658	47405.410778	32.305485
645.713331	47490.498392	32.310503
646.721058	47567.965115	32.315520
647.335115	47654.236845	32.320538
648.205231	47717.560810	32.325556
648.573870	47807.869856	32.330573
649.355882	47879.141437	32.335591
650.193307	47954.491475	32.340608
650.807407	48038.771812	32.345626
651.480425	48107.043429	32.350644
651.685941	48182.562773	32.355661
652.626294	48276.301706	32.360679
653.471667	48358.079638	32.365696
653.998352	48436.934259	32.370714
654.956035	48508.471322	32.375732
655.835385	48584.696280	32.380749
656.202909	48665.265834	32.385767
656.867276	48739.519416	32.390784
657.363937	48811.129625	32.395802
658.137778	48892.174118	32.400820
658.801497	48967.523069	32.405837
659.688713	49052.922174	32.410855
660.349620	49129.619706	32.415872
660.774479	49201.868735	32.420890
661.432521	49278.301486	32.425908
661.753817	49355.097244	32.430925
662.636606	49428.800050	32.435943
663.568872	49509.031051	32.440960
664.206727	49588.985765	32.445978
664.785484	49669.019608	32.450996
665.749085	49747.272521	32.456013
666.171489	49822.098967	32.461031
666.978923	49904.419828	32.466048
667.416275	49982.585124	32.471066
667.917656	50059.823233	32.476084
668.884484	50138.943781	32.481101
669.366376	50216.792869	32.486119
670.429886	50295.082615	32.491136
670.732672	50374.845770	32.496154
671.653442	50456.714280	32.501172
672.176942	50532.400348	32.506189
672.570270	50606.025393	32.511207
673.468121	50686.373446	32.516224
674.244212	50762.843252	32.521242
674.939093	50840.091631	32.526260
675.815548	50928.093560	32.531277
676.383914	51004.546077	32.536295
677.335645	51081.793002	32.541312
677.565826	51151.788123	32.546330
678.158756	51219.429807	32.551348
678.970942	51286.353991	32.556365
679.726173	51359.140155	32.561383
680.004001	51432.039275	32.566400
680.618032	51502.304367	32.571418
681.176208	51583.088370	32.576436
682.207212	51656.851005	32.581453
682.745455	51744.921651	32.586471
683.534014	51824.196099	32.591488
684.239817	51890.392031	32.596506
684.916517	51965.489299	32.601524
685.686980	52047.956447	32.606541
686.131029	52133.834977	32.611559
686.606506	52207.458558	32.616576
687.143502	52295.050575	32.621594
687.891030	52372.378059	32.626612
688.584451	52462.730396	32.631629
689.176736	52546.745861	32.636647
690.376807	52634.304916	32.641664
690.928429	52720.542094	32.646682
691.675129	52807.919685	32.651700
692.245617	52892.667504	32.656717
692.798975	52979.088868	32.661735
693.766058	53058.181348	32.666752
694.467603	53137.480204	32.671770
695.038007	53226.057624	32.676788
695.657190	53307.350594	32.681805
696.240495	53409.373585	32.686823
696.962147	53493.074766	32.691840
697.897651	53578.337418	32.696858
698.664806	53677.396577	32.701876
699.698085	53758.385792	32.706893
700.159914	53848.444343	32.711911
700.972847	53937.233255	32.716928
701.502648	54022.580032	32.721946
702.366004	54109.380987	32.726964
702.972995	54197.956332	32.731981
704.041448	54295.274948	32.736999
704.705373	54368.198670	32.742016
705.330152	54461.739884	32.747034
705.920933	54541.586056	32.752052
706.744691	54619.497523	32.757069
707.342936	54715.087935	32.762087
707.922763	54792.196501	32.767104
708.527269	54883.850380	32.772122
709.350186	54979.121895	32.777140
709.984664	55064.019375	32.782157
710.512295	55151.186817	32.787175
711.393573	55237.185388	32.792192
712.313484	55327.196812	32.797210
713.195416	55417.049982	32.802228
714.292636	55495.769524	32.807245
714.440777	55595.927226	32.812263
715.071451	55673.245859	32.817280
715.989360	55752.715789	32.822298
716.409659	55845.724898	32.827316
717.565478	55935.948497	32.832333
718.290480	56025.347560	32.837351
718.663408	56114.466669	32.842368
719.617403	56195.356380	32.847386
720.482447	56284.962317	32.852404
721.166292	56375.210856	32.857421
721.848926	56450.732829	32.862439
722.432111	56547.168349	32.867456
723.068530	56628.064953	32.872474
723.779761	56723.392571	32.877492
724.537658	56804.308720	32.882509
724.809865	56895.250237	32.887527
726.101967	56969.710081	32.892544
727.169099	57048.287556	32.897562
727.564424	57125.249013	32.902580
728.438634	57206.895123	32.907597
728.558548	57292.982344	32.912615
729.491786	57361.449066	32.917632
730.100587	57440.802120	32.922650
730.754632	57521.243280	32.927668
731.450909	57612.443882	32.932685
732.226415	57706.461538	32.937703
732.828049	57798.880198	32.942720
733.826715	57884.939517	32.947738
734.001423	57988.406863	32.952756
735.115935	58065.821997	32.957773
736.161805	58158.938304	32.962791
736.863503	58241.482036	32.967808
737.567835	58340.640006	32.972826
738.083920	58429.625013	32.977844
738.752878	58518.902874	32.982861
739.607743	58616.829498	32.987879
740.592574	58705.969972	32.992896
741.229570	58795.924772	32.997914
741.862022	58894.969675	33.002932
742.866427	58978.873648	33.007949
743.294994	59075.425763	33.012967
744.038956	59170.011032	33.017984
744.838898	59259.448329	33.023002
745.731978	59363.359707	33.028020
746.753122	59450.288211	33.033037
747.610248	59540.768295	33.038055
748.230700	59635.336734	33.043072
748.878153	59725.451570	33.048090
749.394358	59819.195203	33.053108
750.109632	59916.946366	33.058125
751.213799	60011.605086	33.063143
751.948970	60105.821905	33.068160
752.752307	60199.908147	33.073178
753.009735	60295.409493	33.078196
753.962982	60383.307747	33.083213
754.791711	60486.252854	33.088231
755.307746	60584.018889	33.093248
756.313110	60686.101632	33.098266
756.839907	60787.234293	33.103284
757.680497	60871.632503	33.108301
758.804196	60980.300066	33.113319
759.103816	61071.866910	33.118336
759.966421	61159.016205	33.123354
761.025472	61273.677051	33.128372
761.885086	61364.252094	33.133389
762.486397	61456.880886	33.138407
763.202440	61558.347892	33.143424
764.222205	61646.518768	33.148442
764.495953	61748.024162	33.153460
765.296127	61839.971242	33.158477
766.246215	61948.904475	33.163495
767.152165	62056.465105	33.168512
767.948407	62148.363305	33.173530
768.721141	62251.463813	33.178548
769.494378	62340.910175	33.183565
769.986196	62443.656661	33.188583
770.853463	62541.964164	33.193600
771.686013	62626.059436	33.198618
772.352536	62730.761162	33.203636
773.423738	62822.555496	33.208653
774.375708	62929.099829	33.213671
774.737029	63024.095335	33.218688
775.804787	63117.657503	33.223706
776.569076	63210.045749	33.228724
777.176920	63288.423987	33.233741
777.888499	63384.138343	33.238759
778.346067	63474.777713	33.243776
779.616116	63555.496707	33.248794
780.155360	63649.466490	33.253812
780.815127	63747.152850	33.258829
781.748171	63831.565644	33.263847
782.454008	63926.789182	33.268864
783.398380	64025.672881	33.273882
783.786812	64115.179530	33.278900
784.706226	64216.157041	33.283917
785.504736	64306.467476	33.288935
786.060592	64411.655717	33.293952
787.046142	64504.590196	33.298970
787.776752	64605.871065	33.303988
788.858496	64701.222270	33.309005
789.521450	64797.747327	33.314023
790.280913	64898.834928	33.319040
790.774035	64998.021027	33.324058
791.438274	65107.221706	33.329076
792.224516	65221.057070	33.334093
793.470520	65318.094266	33.339111
793.996081	65424.715964	33.344128
794.886660	65531.768449	33.349146
795.727154	65640.317049	33.354164
796.555021	65742.163378	33.359181
797.161258	65844.703266	33.364199
798.063629	65961.885640	33.369216
799.040728	66058.125727	33.374234
799.352328	66167.715420	33.379252
800.284251	66270.440283	33.384269
801.323101	66376.213182	33.389287
802.014584	66491.506295	33.394304
803.214354	66600.268653	33.399322
803.957970	66711.071974	33.404340
804.580785	66812.473509	33.409357
805.432377	66921.874252	33.414375
805.918757	67042.786325	33.419392
807.209409	67143.185524	33.424410
807.943448	67258.374129	33.429428
808.671176	67366.023333	33.434445
809.924718	67455.722877	33.439463
810.716359	67568.580161	33.444480
811.231315	67676.137352	33.449498
811.979044	67789.724292	33.454516
812.643844	67890.673969	33.459533
814.087445	67996.795420	33.464551
814.733231	68101.889856	33.469568
815.300079	68204.382056	33.474586
815.942272	68318.386757	33.479604
816.858647	68429.423719	33.484621
817.844170	68537.771953	33.489639
818.558788	68645.548869	33.494656
819.684430	68753.458162	33.499674
820.789078	68866.037836	33.504692
821.583345	68970.308400	33.509709
822.267402	69069.721006	33.514727
822.814851	69177.589634	33.519744
823.958367	69277.266687	33.524762
824.501764	69378.659105	33.529780
825.509101	69496.677008	33.534797
826.063726	69591.071528	33.539815
826.765045	69699.766735	33.544832
827.586215	69805.214219	33.549850
828.554044	69919.459920	33.554868
829.244533	70030.095855	33.559885
830.310705	70138.210185	33.564903
830.854602	70238.643369	33.569920
831.949021	70338.344842	33.574938
832.858282	70438.886226	33.579956
832.918933	70540.688035	33.584973
834.333927	70638.263443	33.589991
834.999067	70745.569215	33.595008
835.888167	70844.836171	33.600026
836.456377	70954.614956	33.605044
836.904619	71060.144896	33.610061
837.889377	71168.960141	33.615079
838.624299	71286.933801	33.620096
839.487909	71387.435311	33.625114
840.448296	71508.971554	33.630132
841.084916	71617.146582	33.635149
842.017606	71736.585786	33.640167
842.886616	71855.934179	33.645184
843.895560	71972.234171	33.650202
844.810207	72091.310509	33.655220
845.643080	72211.717400	33.660237
846.397700	72319.116897	33.665255
847.275761	72439.289768	33.670272
848.225090	72554.271765	33.675290
849.321783	72676.678633	33.680308
850.246916	72787.713725	33.685325
851.172094	72894.379562	33.690343
851.649975	73014.959679	33.695360
852.698182	73128.370776	33.700378
853.924826	73249.303351	33.705396
854.662652	73374.480150	33.710413
855.452738	73474.975765	33.715431
856.238407	73598.043547	33.720448
856.969853	73705.528270	33.725466
858.184285	73830.771909	33.730484
858.710432	73949.714743	33.735501
859.384235	74054.904624	33.740519
860.252738	74182.306693	33.745536
861.066006	74305.588738	33.750554
862.018485	74421.287617	33.755572
862.628684	74556.711841	33.760589
863.833396	74676.146975	33.765607
864.966430	74796.885871	33.770624
865.655899	74920.582790	33.775642
866.461603	75040.158019	33.780660
867.704134	75159.551376	33.785677
868.462311	75277.197062	33.790695
869.351708	75396.380756	33.795712
870.229147	75511.589389	33.800730
871.414478	75620.100065	33.805748
871.800563	75755.274053	33.810765
873.001050	75877.704624	33.815783
874.018832	75993.843377	33.820800
874.771394	76109.466792	33.825818
875.397651	76229.176712	33.830836
876.148389	76351.464496	33.835853
877.515934	76468.209219	33.840871
878.056443	76586.021341	33.845888
878.899117	76714.186778	33.850906
879.962879	76833.298809	33.855924
880.926630	76951.983649	33.860941
881.596537	77068.143453	33.865959
882.617836	77182.069860	33.870976
883.529217	77302.930626	33.875994
884.580289	77430.306717	33.881012
884.739723	77556.530876	33.886029
886.058734	77676.037323	33.891047
886.780126	77799.159605	33.896064
887.497066	77920.889635	33.901082
888.589975	78035.897842	33.906100
889.395978	78153.371097	33.911117
890.162008	78256.358529	33.916135
890.769544	78382.288282	33.921152
892.044794	78491.531058	33.926170
892.760724	78613.606355	33.931188
893.294466	78730.883998	33.936205
894.733066	78841.863513	33.941223
895.308129	78970.955516	33.946240
896.135628	79087.998646	33.951258
896.995206	79214.728860	33.956276
898.305890	79333.040259	33.961293
899.226690	79459.267920	33.966311
900.009017	79585.125098	33.971328
900.752302	79697.205088	33.976346
901.842049	79824.282113	33.981364
902.506511	79948.917823	33.986381
903.420029	80070.436487	33.991399
904.169711	80201.090504	33.996416
904.994491	80328.806769	34.001434
906.047714	80458.147532	34.006452
906.905444	80592.536586	34.011469
907.924479	80719.869476	34.016487
908.744911	80863.615732	34.021504
909.838122	80989.873995	34.026522
910.801719	81116.064432	34.031540
911.460384	81249.360202	34.036557
912.249092	81378.024450	34.041575
913.319479	81515.197307	34.046592
913.999979	81657.651869	34.051610
915.136854	81785.946716	34.056628
915.934963	81924.177789	34.061645
917.349868	82066.595443	34.066663
917.954122	82203.147773	34.071680
919.087986	82338.376158	34.076698
920.493035	82460.626408	34.081716
920.853609	82600.690452	34.086733
921.934656	82729.961261	34.091751
923.040350	82868.769626	34.096768
924.099462	83000.287763	34.101786
924.763280	83131.538967	34.106804
925.768639	83274.837721	34.111821
926.872409	83400.370188	34.116839
927.876244	83521.838884	34.121856
928.493919	83669.406995	34.126874
929.393528	83786.813145	34.131892
930.084112	83926.832024	34.136909
931.304476	84063.537543	34.141927
932.457606	84205.918184	34.146944
933.429845	84339.977614	34.151962
934.344854	84464.847390	34.156980
935.108839	84609.673132	34.161997
936.063921	84740.290549	34.167015
937.022687	84876.001846	34.172032
937.975733	85010.282812	34.177050
939.086047	85139.623266	34.182068
939.883815	85283.053238	34.187085
940.680313	85420.870623	34.192103
941.777829	85554.802035	34.197120
942.800559	85697.907390	34.202138
943.807269	85817.243802	34.207156
944.667580	85970.031779	34.212173
945.714767	86090.021905	34.217191
946.661309	86235.258030	34.222208
947.284170	86367.442749	34.227226
948.429893	86496.935765	34.232244
949.594518	86630.291378	34.237261
951.027837	86764.758693	34.242279
951.556053	86895.604701	34.247296
952.311060	87025.478037	34.252314
953.377418	87138.563096	34.257332
954.389990	87260.895151	34.262349
955.230315	87388.919247	34.267367
956.496065	87513.785212	34.272384
956.913013	87638.746588	34.277402
957.996457	87770.536031	34.282420
958.698172	87893.248873	34.287437
959.406588	88032.625740	34.292455
960.626714	88155.613339	34.297472
960.798687	88298.167595	34.302490
962.034156	88425.272570	34.307508
963.214202	88577.352389	34.312525
964.294157	88709.323983	34.317543
965.572818	88851.441490	34.322560
966.057073	88982.265609	34.327578
967.204150	89123.467212	34.332596
968.041887	89270.104028	34.337613
968.971091	89412.038136	34.342631
969.909742	89550.118749	34.347648
970.702143	89700.275287	34.352666
971.617302	89844.989122	34.357684
972.495093	89997.883921	34.362701
973.681899	90146.891024	34.367719
974.844615	90289.553147	34.372736
975.719022	90439.371031	34.377754
976.859685	90587.082151	34.382772
977.615920	90750.366949	34.387789
978.458804	90895.401330	34.392807
979.947589	91037.078075	34.397824
980.733787	91182.553625	34.402842
981.790596	91328.393075	34.407860
982.802770	91487.066441	34.412877
983.906532	91634.801135	34.417895
984.955491	91775.333476	34.422912
986.029123	91938.689056	34.427930
987.230303	92091.771961	34.432948
988.057197	92234.521186	34.437965
989.271804	92374.092448	34.442983
990.041342	92522.479482	34.448000
990.673749	92673.689801	34.453018
991.979667	92818.800286	34.458036
993.094810	92962.356985	34.463053
993.899712	93107.052964	34.468071
994.909823	93269.994663	34.473088
996.012223	93418.029721	34.478106
997.340472	93562.367056	34.483124
998.186663	93713.865899	34.488141
998.850421	93870.730277	34.493159
1000.019389	94013.675049	34.498176
1001.263997	94173.301937	34.503194
1002.295386	94317.828712	34.508212
1003.358528	94466.724191	34.513229
1004.464247	94609.516838	34.518247
1005.414397	94748.607907	34.523264
1006.029350	94919.377566	34.528282
1007.387719	95054.311886	34.533300
1008.436204	95199.080920	34.538317
1009.164351	95353.534333	34.543335
1010.520965	95505.342279	34.548352
1011.282935	95653.593418	34.553370
1012.780558	95808.638453	34.558388
1013.404418	95953.490138	34.563405
1014.280050	96102.967852	34.568423
1015.433853	96256.687245	34.573440
1016.315173	96403.402109	34.578458
1017.586473	96545.100201	34.583476
1018.287703	96685.164211	34.588493
1019.565588	96830.475291	34.593511
1020.449064	96972.489549	34.598528
1021.499546	97115.568471	34.603546
1022.352288	97242.605206	34.608564
1023.186363	97385.934731	34.613581
1024.042270	97529.426281	34.618599
1025.420822	97669.375924	34.623616
1026.349196	97822.605804	34.628634
1027.101629	97970.742549	34.633652
1028.140628	98115.387015	34.638669
1029.318370	98264.802282	34.643687
1030.457701	98412.436811	34.648704
1030.921258	98570.433528	34.653722
1032.254942	98723.756399	34.658740
1033.412163	98873.456616	34.663757
1034.084418	99019.189434	34.668775
1035.228417	99178.603875	34.673792
1036.238983	99351.427248	34.678810
1037.008715	99501.140343	34.683828
1038.443588	99661.399049	34.688845
1039.064586	99823.763665	34.693863
1040.071581	99987.450517	34.698880
1041.099625	100156.738417	34.703898
1042.267029	100310.678039	34.708916
1043.843514	100471.780669	34.713933
1044.356198	100646.311655	34.718951
1045.778821	100801.975865	34.723968
1047.078649	100970.388708	34.728986
1048.121041	101129.968111	34.734004
1049.129554	101295.879960	34.739021
1049.991139	101452.763457	34.744039
1051.344623	101614.464479	34.749056
1052.398457	101781.715580	34.754074
1053.627157	101930.936926	34.759092
1054.575330	102099.867048	34.764109
1055.797673	102265.699604	34.769127
1057.078328	102420.620340	34.774144
1058.064755	102585.692692	34.779162
1059.262907	102743.239643	34.784180
1060.097994	102899.512922	34.789197
1060.988834	103054.282114	34.794215
1062.531865	103224.189862	34.799232
1063.236087	103393.443711	34.804250
1064.548983	103548.871824	34.809268
1065.591462	103703.328678	34.814285
1066.550828	103882.662911	34.819303
1067.896053	104033.206776	34.824320
1068.786939	104194.409571	34.829338
1069.672649	104354.371384	34.834356
1070.896111	104519.035823	34.839373
1071.885707	104681.366640	34.844391
1073.174428	104844.881314	34.849408
1074.034624	105011.659104	34.854426
1075.268781	105184.211768	34.859444
1076.513698	105340.419594	34.864461
1077.445345	105500.975598	34.869479
1078.213361	105657.069351	34.874496
1079.026640	105822.336910	34.879514
1080.077618	105993.058440	34.884532
1081.231841	106160.556640	34.889549
1082.700050	106330.060664	34.894567
1083.870446	106495.757420	34.899584
1084.947089	106660.328447	34.904602
1085.582227	106828.710037	34.909620
1087.084339	106990.641966	34.914637
1088.035462	107169.513034	34.919655
1089.204186	107319.287580	34.924672
1089.940482	107489.939036	34.929690
1091.260464	107647.920922	34.934708
1092.040545	107797.200448	34.939725
1093.292874	107961.166889	34.944743
1094.350259	108117.099734	34.949760
1095.735402	108275.467386	34.954778
1096.869012	108438.846000	34.959796
1097.746559	108583.193515	34.964813
1098.417979	108741.852562	34.969831
1099.407979	108902.402638	34.974848
1100.670680	109074.095396	34.979866
1101.887017	109245.276333	34.984884
1102.907168	109399.711704	34.989901
1103.597361	109585.762858	34.994919
1105.014137	109752.780829	34.999936
1106.160887	109932.117370	35.004954
1107.072727	110097.364556	35.009972
1108.263279	110272.929609	35.014989
1109.311064	110457.699286	35.020007
1110.344620	110618.935187	35.025024
1111.208644	110800.780622	35.030042
1112.193034	110990.318607	35.035060
1113.514552	111171.777276	35.040077
1114.686306	111349.785499	35.045095
1116.152095	111526.404301	35.050112
1117.218626	111720.625606	35.055130
1118.424023	111903.171457	35.060148
1119.718271	112078.234588	35.065165
1120.350462	112263.953757	35.070183
1121.942569	112443.334692	35.075200
1122.871385	112623.796896	35.080218
1124.189056	112804.516185	35.085236
1125.296204	112974.768319	35.090253
1126.132888	113172.762068	35.095271
1127.488510	113353.706443	35.100288
1128.600720	113537.518043	35.105306
1129.931785	113720.763639	35.110324
1131.553490	113903.875879	35.115341
1132.106144	114083.275471	35.120359
1133.426686	114269.138121	35.125376
1134.949731	114454.919281	35.130394
1136.035873	114637.231234	35.135412
1137.127140	114808.876866	35.140429
1137.970374	114997.329167	35.145447
1139.463464	115180.341089	35.150464
1140.660446	115363.260760	35.155482
1141.719863	115533.329349	35.160500
1143.088643	115716.997554	35.165517
1143.929579	115896.779400	35.170535
1145.589085	116072.032808	35.175552
1146.477739	116255.702740	35.180570
1147.907154	116437.678106	35.185588
1149.391187	116609.308642	35.190605
1150.225687	116787.840113	35.195623
1151.333658	116967.953144	35.200640
1152.549616	117138.448484	35.205658
1153.729570	117320.784290	35.210676
1154.880169	117480.598905	35.215693
1156.011740	117667.307236	35.220711
1156.847443	117835.328460	35.225728
1158.154721	118017.140338	35.230746
1159.382551	118192.788334	35.235764
1160.162763	118373.809225	35.240781
1161.704035	118558.846914	35.245799
1162.750384	118728.652970	35.250816
1163.966616	118909.506675	35.255834
1164.781745	119096.398413	35.260852
1165.782010	119271.998217	35.265869
1166.896718	119457.753949	35.270887
1168.099973	119629.366019	35.275904
1169.505383	119799.513836	35.280922
1170.131018	119978.092995	35.285940
1171.954315	120140.096704	35.290957
1173.045869	120321.078049	35.295975
1173.897616	120496.300767	35.300992
1175.049017	120676.703582	35.306010
1175.853388	120852.975495	35.311028
1177.649649	121032.619387	35.316045
1178.657641	121216.992225	35.321063
1179.862852	121391.732344	35.326080
1181.294791	121568.340542	35.331098
1182.075868	121749.554722	35.336116
1183.567366	121928.755714	35.341133
1184.292036	122114.027045	35.346151
1185.513903	122292.079469	35.351168
1186.868495	122472.560233	35.356186
1188.027934	122667.153422	35.361204
1189.104790	122850.216514	35.366221
1190.002698	123037.329847	35.371239
1191.101572	123240.016150	35.376256
1192.537064	123428.188887	35.381274
1193.462711	123635.965985	35.386292
1194.820159	123822.896891	35.391309
1195.977099	124022.596864	35.396327
1197.178163	124216.188896	35.401344
1198.772593	124424.550434	35.406362
1199.781834	124616.563274	35.411380
1201.165019	124817.043690	35.416397
1202.456335	125014.241023	35.421415
1203.232388	125206.559580	35.426432
1204.792210	125406.418996	35.431450
1205.560789	125608.547287	35.436468
1206.886497	125811.845340	35.441485
1208.467849	126013.429742	35.446503
1209.847348	126211.101156	35.451520
1210.926451	126418.322969	35.456538
1212.003772	126624.391599	35.461556
1213.002627	126815.401463	35.466573
1214.498157	127023.182788	35.471591
1215.512728	127226.650724	35.476608
1217.152264	127426.837357	35.481626
1218.106246	127640.999366	35.486644
1219.496969	127841.315754	35.491661
1220.840986	128044.761494	35.496679
1222.192872	128253.129692	35.501696
1223.832278	128453.701895	35.506714
1224.044144	128656.059089	35.511732
1225.886994	128855.738614	35.516749
1227.193227	129060.019879	35.521767
1228.529322	129265.236345	35.526784
1229.745431	129462.733069	35.531802
1230.813322	129666.826192	35.536820
1232.163671	129861.652008	35.541837
1233.494330	130071.364719	35.546855
1234.999480	130264.125386	35.551872
1235.958013	130462.935865	35.556890
1237.543770	130660.101131	35.561908
1238.730146	130859.131539	35.566925
1239.700742	131053.210180	35.571943
1240.699540	131255.837168	35.576960
1242.253189	131451.932580	35.581978
1243.248727	131657.239193	35.586996
1244.615718	131858.111117	35.592013
1246.193244	132059.851894	35.597031
1246.854053	132256.407912	35.602048
1248.411468	132451.098808	35.607066
1250.003139	132652.573646	35.612084
1251.179646	132834.523005	35.617101
1252.307715	133023.472215	35.622119
1253.043761	133201.215920	35.627136
1254.759082	133394.185971	35.632154
1256.019873	133583.116798	35.637172
1257.542324	133755.422961	35.642189
1258.532840	133948.585020	35.647207
1259.663005	134141.180424	35.652224
1261.138922	134329.623940	35.657242
1262.251822	134512.478381	35.662260
1263.038298	134700.422300	35.667277
1264.715141	134893.975887	35.672295
1265.627182	135096.634098	35.677312
1267.195150	135295.497921	35.682330
1268.040384	135488.131014	35.687348
1269.147832	135698.755707	35.692365
1270.730668	135895.043859	35.697383
1271.844466	136113.219786	35.702400
1273.254633	136304.321284	35.707418
1274.455737	136522.130186	35.712436
1275.836892	136717.527092	35.717453
1277.234915	136927.388647	35.722471
1278.524599	137139.298507	35.727488
1279.567653	137343.342082	35.732506
1280.811443	137550.286535	35.737524
1282.369144	137758.769036	35.742541
1283.904418	137975.568040	35.747559
1284.689184	138180.899362	35.752576
1286.236119	138388.612265	35.757594
1287.222186	138606.921481	35.762612
1288.393964	138823.781318	35.767629
1289.865375	139040.214537	35.772647
1290.800406	139253.090536	35.777664
1292.492145	139465.988637	35.782682
1293.912209	139698.714907	35.787700
1294.964559	139914.468973	35.792717
1296.446804	140126.984037	35.797735
1297.983297	140352.347335	35.802752
1299.565141	140557.158095	35.807770
1300.585446	140776.411050	35.812788
1301.711106	140986.307958	35.817805
1303.226921	141207.515864	35.822823
1304.641711	141426.012013	35.827840
1305.836719	141644.835445	35.832858
1306.840875	141871.939016	35.837876
1308.497333	142089.448475	35.842893
1309.809797	142313.053814	35.847911
1310.903293	142528.026242	35.852928
1312.619730	142749.133590	35.857946
1313.786203	142975.658440	35.862964
1315.192170	143191.320955	35.867981
1316.797678	143408.488856	35.872999
1317.605013	143635.682136	35.878016
1318.977496	143847.811769	35.883034
1320.299676	144068.923254	35.888052
1321.876024	144295.021889	35.893069
1323.638355	144510.608941	35.898087
1324.573029	144732.317061	35.903104
1325.983261	144948.227628	35.908122
1327.143117	145153.745453	35.913140
1328.514311	145374.626533	35.918157
1330.118213	145596.538285	35.923175
1331.370711	145826.806709	35.928192
1332.575818	146031.825993	35.933210
1333.918330	146251.636510	35.938228
1335.143167	146473.598701	35.943245
1336.518062	146697.531068	35.948263
1337.740807	146921.132830	35.953280
1338.979224	147117.710719	35.958298
1340.374771	147325.358060	35.963316
1341.207215	147531.825107	35.968333
1342.852970	147736.959858	35.973351
1344.060604	147958.169513	35.978368
1345.485316	148160.065793	35.983386
1346.680896	148383.043413	35.988404
1347.914717	148596.686721	35.993421
1349.415848	148807.179280	35.998439
1350.689467	149036.366965	36.003456
1351.903220	149254.483984	36.008474
1353.216991	149477.853868	36.013492
1354.785918	149701.311673	36.018509
1355.830624	149911.156509	36.023527
1357.232340	150147.614777	36.028544
1358.452876	150376.359526	36.033562
1359.804842	150606.925201	36.038580
1361.021649	150830.683955	36.043597
1362.283473	151066.419203	36.048615
1363.437117	151303.352893	36.053632
1364.944036	151548.584673	36.058650
1366.454603	151787.406693	36.063668
1367.410693	152038.629402	36.068685
1369.074818	152280.247504	36.073703
1370.580640	152523.465462	36.078720
1371.871094	152765.347254	36.083738
1373.332281	153010.948064	36.088756
1374.724185	153259.137664	36.093773
1376.370742	153504.610057	36.098791
1377.460787	153754.880120	36.103808
1379.079668	153996.791939	36.108826
1380.088991	154248.003473	36.113844
1381.325654	154502.062114	36.118861
1383.202116	154748.811376	36.123879
1384.645745	155004.325068	36.128896
1386.205519	155253.537980	36.133914
1387.845962	155514.037399	36.138932
1388.892896	155766.747588	36.143949
1390.246644	156008.430046	36.148967
1391.851165	156256.916644	36.153984
1393.222538	156503.853948	36.159002
1394.780061	156754.279584	36.164020
1395.673426	157004.302441	36.169037
1397.617450	157263.873438	36.174055
1398.734650	157513.914172	36.179072
1400.411345	157752.938032	36.184090
1401.906426	158013.877425	36.189108
1403.175129	158270.460891	36.194125
1404.326730	158521.934951	36.199143
1406.056139	158772.722936	36.204160
1407.441423	159032.528624	36.209178
1408.823610	159277.888697	36.214196
1410.159507	159534.492334	36.219213
1412.114482	159787.115357	36.224231
1413.219419	160038.628307	36.229248
1414.664023	160293.123319	36.234266
1416.438979	160535.671966	36.239284
1417.637130	160791.946861	36.244301
1418.957680	161041.068706	36.249319
1420.236961	161294.400252	36.254336
1421.910903	161538.479341	36.259354
1423.422378	161793.261924	36.264372
1424.787778	162051.356599	36.269389
1426.669314	162308.685946	36.274407
1427.955189	162557.552507	36.279424
1429.303981	162799.427399	36.284442
1430.468669	163053.926440	36.289460
1431.938568	163302.894005	36.294477
1433.695858	163529.459699	36.299495
1435.003497	163762.888988	36.304512
1436.044218	164001.490138	36.309530
1437.745851	164229.666661	36.314548
1439.077223	164469.937989	36.319565
1440.639670	164708.320348	36.324583
1441.470588	164938.641591	36.329600
1443.002598	165178.096873	36.334618
1444.306540	165418.629807	36.339636
1445.768440	165672.635249	36.344653
1447.368246	165917.364267	36.349671
1448.389525	166169.167836	36.354688
1450.039713	166419.528045	36.359706
1451.080893	166664.283669	36.364724
1452.787848	166920.426491	36.369741
1454.071683	167177.639525	36.374759
1455.660752	167437.535547	36.379776
1456.875721	167692.590088	36.384794
1458.947252	167955.548633	36.389812
1459.994287	168218.414563	36.394829
1461.369195	168478.741529	36.399847
1462.472187	168755.884815	36.404864
1464.426166	169018.548241	36.409882
1466.038441	169283.031008	36.414900
1467.209461	169547.329857	36.419917
1468.851385	169822.754928	36.424935
1470.421740	170085.901255	36.429952
1472.097802	170356.409129	36.434970
1473.594474	170630.044230	36.439988
1474.876931	170903.244059	36.445005
1476.659989	171173.001701	36.450023
1478.034513	171442.544907	36.455040
1479.416081	171719.122424	36.460058
1480.920907	171983.466551	36.465076
1482.237170	172255.053376	36.470093
1484.265273	172530.961245	36.475111
1485.951262	172810.732972	36.480128
1487.190235	173078.500070	36.485146
1488.978955	173349.242223	36.490164
1490.356288	173625.852631	36.495181
1492.016364	173887.372716	36.500199
1493.514470	174160.207506	36.505216
1494.661764	174427.980840	36.510234
1496.287043	174700.607103	36.515252
1497.623551	174974.574691	36.520269
1499.317631	175241.439775	36.525287
1500.900599	175528.144985	36.530304
1502.204779	175803.961661	36.535322
1504.039557	176069.029673	36.540340
1505.349894	176353.685216	36.545357
1507.381038	176622.317884	36.550375
1508.627552	176890.820252	36.555392
1510.420741	177171.580790	36.560410
1511.956021	177437.144458	36.565428
1512.966082	177714.753156	36.570445
1514.534598	177983.233980	36.575463
1516.280426	178253.745062	36.580480
1517.825684	178524.009011	36.585498
1519.171556	178793.797059	36.590516
1520.395221	179084.049989	36.595533
1522.381544	179353.510941	36.600551
1523.959806	179635.405202	36.605568
1525.521684	179909.175665	36.610586
1526.779093	180168.644895	36.615604
1528.453382	180448.088497	36.620621
1529.593036	180726.448332	36.625639
1531.290309	181006.067835	36.630656
1532.894570	181278.769079	36.635674
1534.430632	181538.858937	36.640692
1535.871727	181802.824910	36.645709
1537.463315	182059.605766	36.650727
1539.012911	182318.552751	36.655744
1540.295033	182579.193202	36.660762
1542.036853	182838.416300	36.665780
1543.170904	183107.920032	36.670797
1544.544732	183376.040862	36.675815
1546.358719	183644.804708	36.680832
1547.903216	183908.938101	36.685850
1548.906149	184187.456493	36.690868
1550.531403	184468.468957	36.695885
1552.171662	184748.794092	36.700903
1553.504168	185034.654365	36.705920
1555.150739	185381.678143	36.710938
1556.710863	185654.779582	36.715956
1558.285712	185951.018162	36.720973
1559.877999	186235.672768	36.725991
1561.459599	186525.790694	36.731008
1562.853596	186812.459055	36.736026
1564.557613	187088.284872	36.741044
1566.190341	187396.430852	36.746061
1567.669458	187681.818249	36.751079
1569.153094	187971.117251	36.756096
1570.678582	188265.490431	36.761114
1572.332428	188573.738043	36.766132
1573.843506	188871.137678	36.771149
1575.473473	189175.504502	36.776167
1577.261958	189477.383531	36.781184
1578.989063	189776.682153	36.786202
1580.767576	190073.585891	36.791220
1582.240249	190383.314598	36.796237
1583.940235	190677.920746	36.801255
1585.704588	190966.192857	36.806272
1586.873163	191273.660065	36.811290
1588.517663	191574.627242	36.816308
1589.905429	191878.937427	36.821325
1591.946601	192179.869427	36.826343
1593.768796	192472.403394	36.831360
1595.000049	192780.016998	36.836378
1596.969994	193084.340645	36.841396
1598.378701	193388.702057	36.846413
1600.032051	193692.009871	36.851431
1602.253091	193991.521003	36.856448
1603.615589	194297.034841	36.861466
1605.126580	194581.366998	36.866484
1607.131738	194882.285612	36.871501
1608.787788	195189.406643	36.876519
1610.585659	195490.003440	36.881536
1612.258866	195772.788651	36.886554
1613.936567	196063.854601	36.891572
1615.305144	196364.723702	36.896589
1617.084110	196660.169498	36.901607
1618.898875	196945.246464	36.906624
1620.697613	197240.436351	36.911642
1622.221460	197540.292965	36.916660
1623.578263	197827.780291	36.921677
1624.920949	198121.112793	36.926695
1626.837398	198415.448354	36.931712
1628.424155	198720.606481	36.936730
1629.887546	199001.881309	36.941748
1632.222337	199296.153095	36.946765
1633.630468	199597.505209	36.951783
1635.334547	199878.032688	36.956800
1636.902183	200175.042581	36.961818
1638.601974	200450.846936	36.966836
1640.246050	200755.796802	36.971853
1641.816174	201029.387025	36.976871
1643.586179	201307.518826	36.981888
1644.745495	201579.142049	36.986906
1646.574719	201845.783608	36.991924
1648.396904	202121.368327	36.996941
1649.234464	202407.725793	37.001959
1651.055555	202676.503694	37.006976
1652.415523	202962.424658	37.011994
1654.528737	203244.417805	37.017012
1655.869110	203527.345215	37.022029
1657.174000	203817.467554	37.027047
1659.478755	204096.663125	37.032064
1660.800942	204383.709895	37.037082
1662.500914	204682.459443	37.042100
1664.000291	204976.388902	37.047117
1665.711349	205261.648704	37.052135
1666.803567	205557.420927	37.057152
1668.621363	205867.635890	37.062170
1670.284103	206171.169201	37.067188
1672.004245	206490.113571	37.072205
1673.879300	206789.804086	37.077223
1675.544171	207090.899668	37.082240
1677.093906	207402.022488	37.087258
1678.512687	207711.692848	37.092276
1680.512592	208026.505730	37.097293
1682.052417	208337.707571	37.102311
1684.020244	208651.230739	37.107328
1685.297864	208973.905880	37.112346
1687.101928	209296.016393	37.117364
1688.957859	209606.255849	37.122381
1690.370643	209938.894568	37.127399
1692.135533	210251.943405	37.132416
1693.772092	210588.028176	37.137434
1695.412461	210905.746074	37.142452
1697.714638	211226.866440	37.147469
1698.928199	211557.582220	37.152487
1701.108387	211880.907098	37.157504
1702.639822	212206.239112	37.162522
1704.468654	212527.892216	37.167540
1706.293707	212856.278191	37.172557
1707.554276	213188.817415	37.177575
1709.606212	213518.794376	37.182592
1711.515562	213850.724646	37.187610
1712.734590	214177.174443	37.192628
1715.110325	214505.552027	37.197645
1716.675398	214836.724153	37.202663
1718.179276	215173.037699	37.207680
1720.276715	215500.646758	37.212698
1722.012639	215822.647602	37.217716
1724.090911	216147.287920	37.222733
1725.357977	216482.623420	37.227751
1727.450606	216807.947872	37.232768
1729.067106	217139.977467	37.237786
1730.789419	217463.073959	37.242804
1732.302486	217802.817555	37.247821
1734.150431	218129.552959	37.252839
1736.073956	218452.212096	37.257856
1737.787022	218781.865026	37.262874
1739.879503	219112.957592	37.267892
1741.245719	219435.653646	37.272909
1743.185986	219760.343146	37.277927
1745.173297	220081.545082	37.282944
1746.794541	220413.474122	37.287962
1748.667512	220741.350068	37.292980
1750.519961	221058.991523	37.297997
1752.109918	221381.577142	37.303015
1754.111167	221704.428754	37.308032
1756.198967	222037.936617	37.313050
1757.626096	222348.608092	37.318068
1759.506775	222648.792999	37.323085
1760.710638	222951.929133	37.328103
1762.461229	223244.970562	37.333120
1764.140404	223557.965412	37.338138
1765.744504	223862.004414	37.343156
1767.425272	224173.601869	37.348173
1769.009389	224487.043572	37.353191
1771.007782	224794.856974	37.358208
1772.782319	225115.686908	37.363226
1774.032541	225422.474223	37.368244
1776.252306	225742.243732	37.373261
1777.891078	226079.810796	37.378279
1779.242391	226396.693091	37.383296
1781.243982	226724.651399	37.388314
1783.027215	227059.350518	37.393332
1784.949028	227380.030260	37.398349
1786.264819	227723.643043	37.403367
1788.153565	228066.530999	37.408384
1789.985207	228402.467102	37.413402
1791.626652	228731.065709	37.418420
1793.265539	229076.888569	37.423437
1795.225770	229415.420887	37.428455
1796.916090	229760.244718	37.433472
1798.292858	230111.925764	37.438490
1800.387348	230467.177938	37.443508
1802.168322	230813.689231	37.448525
1803.903656	231173.442981	37.453543
1805.922614	231531.932776	37.458560
1807.746791	231892.663000	37.463578
1809.296432	232256.382834	37.468596
1811.486551	232606.995414	37.473613
1813.259888	232974.617400	37.478631
1815.063370	233336.340716	37.483648
1816.969244	233700.384911	37.488666
1818.878607	234057.061173	37.493684
1821.211399	234424.543747	37.498701
1822.744186	234786.841810	37.503719
1824.393923	235145.209086	37.508736
1826.544824	235504.742418	37.513754
1828.016284	235881.503872	37.518772
1829.920022	236237.594902	37.523789
1831.773786	236609.977183	37.528807
1833.971287	236970.111535	37.533824
1835.956269	237350.652494	37.538842
1837.599444	237712.905105	37.543860
1839.955727	238070.574703	37.548877
1841.222380	238442.996048	37.553895
1843.232443	238804.605737	37.558912
1845.336323	239176.234698	37.563930
1847.120593	239549.869270	37.568948
1849.309821	239911.830624	37.573965
1850.744048	240278.025002	37.578983
1852.627998	240630.608527	37.584000
1854.364384	241002.648225	37.589018
1855.798628	241372.346761	37.594036
1858.515751	241733.283126	37.599053
1860.568583	242093.459205	37.604071
1862.207589	242463.657554	37.609088
1864.415394	242833.283666	37.614106
1866.139227	243190.105553	37.619124
1868.188033	243561.965451	37.624141
1869.804619	243906.812748	37.629159
1871.566974	244271.273198	37.634176
1873.904135	244642.197049	37.639194
1875.437147	245007.149385	37.644212
1877.344913	245358.375712	37.649229
1879.073096	245733.508167	37.654247
1880.830970	246084.248632	37.659264
1882.566131	246428.666754	37.664282
1884.844385	246777.444750	37.669300
1886.444058	247118.453478	37.674317
1888.224680	247464.844020	37.679335
1889.968762	247811.417448	37.684352
1892.254109	248151.377087	37.689370
1893.948811	248507.025591	37.694388
1895.754608	248852.418838	37.699405
1897.342916	249209.022452	37.704423
1899.412256	249566.007297	37.709440
1901.113721	249917.765288	37.714458
1902.951881	250288.781385	37.719476
1904.750557	250651.623345	37.724493
1906.450309	251013.819515	37.729511
1908.402249	251386.568029	37.734528
1910.543156	251746.559726	37.739546
1912.121288	252130.262377	37.744564
1913.970767	252494.413024	37.749581
1915.607877	252878.053751	37.754599
1917.439804	253271.772868	37.759616
1919.733600	253650.355508	37.764634
1921.608409	254037.385220	37.769652
1923.450659	254430.870947	37.774669
1925.344184	254821.985220	37.779687
1926.799277	255215.935735	37.784704
1929.218635	255610.394671	37.789722
1930.580974	256015.965748	37.794740
1933.054398	256411.175905	37.799757
1934.826305	256810.050780	37.804775
1936.504463	257225.957727	37.809792
1939.043360	257623.338429	37.814810
1941.065350	258039.315926	37.819828
1942.930693	258442.285996	37.824845
1944.912976	258840.638945	37.829863
1946.728295	259249.202326	37.834880
1948.968233	259656.834269	37.839898
1950.665899	260069.832936	37.844916
1953.019206	260473.583476	37.849933
1955.224497	260878.143179	37.854951
1957.347671	261284.670112	37.859968
1959.165551	261693.122960	37.864986
1961.197433	262109.643405	37.870004
1963.407034	262505.357447	37.875021
1965.392085	262902.095788	37.880039
1967.843058	263308.208438	37.885056
1969.823131	263712.843864	37.890074
1971.472387	264122.050610	37.895092
1973.675149	264511.408490	37.900109
1975.535992	264908.539780	37.905127
1977.623506	265313.914193	37.910144
1979.720114	265704.173153	37.915162
1981.719021	266119.768628	37.920180
1983.826741	266516.829612	37.925197
1985.838702	266919.364715	37.930215
1987.675297	267309.988256	37.935232
1989.634445	267705.543766	37.940250
1991.703489	268109.334942	37.945268
1993.570909	268505.358678	37.950285
1995.709513	268916.069281	37.955303
1997.837233	269308.442370	37.960320
1999.765216	269699.625951	37.965338
2002.096170	270109.234468	37.970356
2003.952541	270508.146753	37.975373
2005.903091	270916.947623	37.980391
2007.946713	271300.283745	37.985408
2009.991772	271696.773851	37.990426
2011.774409	272103.411357	37.995444
2014.193511	272483.432729	38.000461
2016.190107	272856.508946	38.005479
2018.181201	273235.019355	38.010496
2020.328100	273599.510039	38.015514
2022.108862	273973.402442	38.020532
2023.812615	274351.495673	38.025549
2025.913691	274723.556842	38.030567
2027.639141	275103.243235	38.035584
2029.661785	275478.513212	38.040602
2031.610268	275867.405406	38.045620
2033.504405	276262.246904	38.050637
2035.250806	276636.894426	38.055655
2037.181485	277046.405170	38.060672
2039.394571	277429.280353	38.065690
2041.098914	277831.152935	38.070708
2042.747214	278243.215764	38.075725
2045.531606	278647.607042	38.080743
2046.974078	279053.323523	38.085760
2049.420804	279459.388616	38.090778
2051.130581	279889.031666	38.095796
2053.298399	280298.868903	38.100813
2055.290412	280712.667541	38.105831
2057.023985	281142.350410	38.110848
2059.392257	281573.429716	38.115866
2061.422475	281998.210823	38.120884
2063.403230	282420.457768	38.125901
2065.350393	282852.484095	38.130919
2067.178897	283284.729508	38.135936
2069.861260	283722.882332	38.140954
2071.722494	284154.126923	38.145972
2073.802868	284597.675638	38.150989
2076.222558	285033.068036	38.156007
2077.946892	285466.966703	38.161024
2080.161627	285910.206562	38.166042
2082.212567	286357.100263	38.171060
2084.484310	286800.046011	38.176077
2086.176767	287242.571592	38.181095
2088.606974	287696.151267	38.186112
2090.958175	288143.214457	38.191130
2092.760213	288587.897498	38.196148
2094.698635	289034.612849	38.201165
2097.384983	289482.045984	38.206183
2098.996112	289933.249733	38.211200
2101.664608	290374.179236	38.216218
2103.529996	290835.391557	38.221236
2105.892387	291279.485630	38.226253
2108.006611	291733.923844	38.231271
2109.964042	292191.353882	38.236288
2112.254828	292645.757707	38.241306
2114.646546	293086.304881	38.246324
2116.872422	293526.341595	38.251341
2119.405171	293986.537068	38.256359
2121.571230	294437.443100	38.261376
2123.220892	294870.806469	38.266394
2125.949686	295319.764302	38.271412
2127.816750	295769.945207	38.276429
2130.485715	296216.417382	38.281447
2132.639406	296654.740903	38.286464
2134.552224	297077.510459	38.291482
2136.717324	297523.797379	38.296500
2138.647729	297965.928523	38.301517
2140.618064	298402.134652	38.306535
2142.950271	298842.774312	38.311552
2145.079632	299279.075628	38.316570
2146.945105	299734.581884	38.321588
2149.383028	300172.681080	38.326605
2151.607555	300614.998910	38.331623
2153.538321	301061.928616	38.336640
2155.739624	301494.189918	38.341658
2157.771756	301913.502019	38.346676
2160.244391	302339.088322	38.351693
2162.155784	302748.893093	38.356711
2163.807278	303175.489613	38.361728
2166.043186	303598.005778	38.366746
2168.091591	304016.130887	38.371764
2170.006260	304449.808949	38.376781
2172.325631	304868.925539	38.381799
2174.452674	305314.899913	38.386816
2176.463326	305750.379621	38.391834
2178.546810	306186.758013	38.396852
2180.235512	306630.885607	38.401869
2182.735834	307082.116546	38.406887
2184.650656	307535.262583	38.411904
2187.054599	307985.307402	38.416922
2189.284581	308438.852750	38.421940
2191.331861	308895.646053	38.426957
2193.318221	309355.896583	38.431975
2195.591241	309828.560419	38.436992
2197.849204	310289.901763	38.442010
2199.910696	310762.564137	38.447028
2201.758537	311236.803505	38.452045
2204.152595	311711.409542	38.457063
2206.294972	312183.689779	38.462080
2208.502956	312664.432052	38.467098
2210.812550	313156.853716	38.472116
2212.707413	313641.898741	38.477133
2215.177909	314126.036471	38.482151
2217.679524	314615.874575	38.487168
2220.143924	315096.348377	38.492186
2222.413928	315581.796368	38.497204
2224.541389	316075.281048	38.502221
2227.020740	316562.792132	38.507239
2229.246428	317064.853762	38.512256
2231.580601	317549.306033	38.517274
2233.749230	318038.930501	38.522292
2235.863661	318524.167757	38.527309
2238.582144	319008.442321	38.532327
2240.769074	319515.252875	38.537344
2243.289868	320006.373509	38.542362
2245.480407	320498.732873	38.547380
2247.852764	320982.912550	38.552397
2250.315099	321481.764981	38.557415
2252.749311	321966.888033	38.562432
2255.185760	322451.929029	38.567450
2257.588656	322936.690546	38.572468
2259.283069	323434.523473	38.577485
2262.026475	323909.882696	38.582503
2263.986797	324399.618909	38.587520
2266.741721	324879.329407	38.592538
2269.273874	325364.042236	38.597556
2270.983667	325850.806265	38.602573
2273.693675	326334.946861	38.607591
2275.782989	326822.527856	38.612608
2278.355715	327305.054441	38.617626
2280.474915	327790.487747	38.622644
2282.587833	328283.781164	38.627661
2284.808499	328762.285753	38.632679
2287.013876	329247.636962	38.637696
2289.491838	329739.687994	38.642714
2291.886257	330226.342102	38.647732
2293.867951	330728.504738	38.652749
2296.460716	331207.809055	38.657767
2298.998083	331686.405736	38.662784
2301.339654	332177.812838	38.667802
2303.387260	332650.436329	38.672820
2305.528459	333141.354960	38.677837
2307.706931	333619.628302	38.682855
2309.783326	334094.943554	38.687872
2311.852161	334558.179266	38.692890
2314.269637	335019.223882	38.697908
2316.142560	335489.454481	38.702925
2318.830575	335951.485192	38.707943
2321.221871	336429.181801	38.712960
2323.192308	336892.251457	38.717978
2325.519795	337374.410008	38.722996
2327.486089	337854.082190	38.728013
2329.729762	338338.320941	38.733031
2331.807703	338833.561736	38.738048
2334.182791	339332.782036	38.743066
2336.622170	339818.542734	38.748084
2338.743530	340322.709340	38.753101
2340.994964	340825.022310	38.758119
2343.419908	341343.735714	38.763136
2345.556991	341850.363505	38.768154
2347.891073	342357.130663	38.773172
2350.379563	342872.666595	38.778189
2352.385048	343388.295765	38.783207
2355.085040	343918.745839	38.788224
2357.020780	344448.521102	38.793242
2359.640414	344962.027122	38.798260
2361.825261	345502.879888	38.803277
2364.254497	346033.922658	38.808295
2366.646251	346561.691695	38.813312
2369.089127	347106.256774	38.818330
2371.705081	347648.681226	38.823348
2374.009446	348190.055215	38.828365
2376.302446	348725.235088	38.833383
2378.998192	349270.536514	38.838400
2381.258654	349828.955252	38.843418
2383.682893	350361.881947	38.848436
2386.205377	350920.342427	38.853453
2388.591454	351462.232706	38.858471
2391.135135	352008.298019	38.863488
2393.490404	352565.640577	38.868506
2396.217180	353103.063670	38.873524
2398.540087	353654.738471	38.878541
2400.796515	354205.729553	38.883559
2403.252523	354757.440355	38.888576
2405.757183	355311.009873	38.893594
2408.733127	355870.605487	38.898612
2410.735440	356423.371919	38.903629
2413.554249	356979.347007	38.908647
2415.943695	357522.172038	38.913664
2418.428260	358076.050244	38.918682
2420.583066	358620.489556	38.923700
2423.350893	359176.179328	38.928717
2425.394566	359725.331055	38.933735
2428.171636	360276.968880	38.938752
2430.768584	360829.740042	38.943770
2433.599296	361384.618905	38.948788
2435.962133	361938.800262	38.953805
2438.485321	362478.321823	38.958823
2440.969820	363026.482293	38.963840
2443.055578	363568.054657	38.968858
2445.910789	364116.745119	38.973876
2448.230591	364662.112990	38.978893
2450.790229	365208.725651	38.983911
2453.294937	365760.531878	38.988928
2455.609561	366307.795707	38.993946
2458.476804	366841.050070	38.998964
2460.787331	367399.241419	39.003981
2462.924476	367946.299041	39.008999
2466.019603	368481.108979	39.014016
2468.213798	369027.604723	39.019034
2470.665535	369554.259580	39.024052
2473.149655	370082.014433	39.029069
2475.618274	370586.298403	39.034087
2478.031518	371089.720446	39.039104
2480.334341	371607.998445	39.044122
2483.245345	372109.069138	39.049140
2485.309651	372626.605282	39.054157
2487.692310	373141.244273	39.059175
2490.256446	373651.436837	39.064192
2492.415881	374184.079459	39.069210
2495.372303	374697.738043	39.074228
2497.583992	375229.034646	39.079245
2499.986258	375761.937707	39.084263
2502.182719	376282.246517	39.089280
2504.686088	376818.279511	39.094298
2506.817836	377352.105345	39.099316
2509.571735	377902.415423	39.104333
2512.015723	378445.720538	39.109351
2514.490266	378994.658461	39.114368
2516.854944	379552.113059	39.119386
2519.122725	380098.198044	39.124404
2521.749528	380671.874761	39.129421
2524.105991	381228.636442	39.134439
2527.105690	381799.671846	39.139456
2529.131313	382367.909056	39.144474
2531.636403	382940.237694	39.149492
2534.285720	383516.026062	39.154509
2536.804820	384089.061375	39.159527
2539.740003	384665.716216	39.164544
2542.124162	385253.308378	39.169562
2544.237099	385839.536535	39.174580
2547.046477	386441.140019	39.179597
2549.487275	387029.112523	39.184615
2552.213813	387607.758661	39.189632
2554.708448	388212.053034	39.194650
2557.450014	388804.975683	39.199668
2559.945313	389405.493437	39.204685
2562.676436	389996.945913	39.209703
2565.097626	390602.054306	39.214720
2567.955514	391193.053060	39.219738
2570.474319	391797.964719	39.224756
2572.864894	392404.754877	39.229773
2575.922470	393010.666041	39.234791
2578.732882	393614.676661	39.239808
2580.857656	394216.247842	39.244826
2583.955030	394827.727048	39.249844
2586.471967	395422.979185	39.254861
2589.092459	396022.554151	39.259879
2591.940299	396627.495335	39.264896
2594.474348	397232.065131	39.269914
2597.187027	397833.756600	39.274932
2600.059844	398440.115409	39.279949
2602.561958	399038.619727	39.284967
2605.796249	399633.450843	39.289984
2608.167927	400235.690583	39.295002
2611.174159	400829.413105	39.300020
2613.526974	401411.479855	39.305037
2616.031188	402012.235283	39.310055
2618.857248	402604.421742	39.315072
2621.104378	403207.463554	39.320090
2624.053687	403795.905180	39.325108
2626.726478	404387.310077	39.330125
2629.192433	404993.913985	39.335143
2631.902938	405586.293707	39.340160
2634.249877	406182.408785	39.345178
2637.312144	406785.379332	39.350196
2639.965295	407383.539798	39.355213
2642.642366	407992.863098	39.360231
2645.477307	408575.934696	39.365248
2647.646109	409151.758422	39.370266
2650.178243	409705.450254	39.375284
2652.587886	410276.299003	39.380301
2655.247281	410833.838231	39.385319
2657.943175	411399.047551	39.390336
2660.559559	411976.042341	39.395354
2662.979874	412539.696732	39.400372
2665.374995	413116.543946	39.405389
2668.013270	413703.708033	39.410407
2670.660269	414280.434044	39.415424
2673.196460	414877.800243	39.420442
2675.329225	415462.263591	39.425460
2678.063411	416065.028481	39.430477
2681.014746	416670.372430	39.435495
2683.805733	417267.176332	39.440512
2686.205700	417878.236651	39.445530
2688.547230	418496.166614	39.450548
2691.281172	419109.364139	39.455565
2693.777263	419729.458715	39.460583
2696.573575	420352.420971	39.465600
2699.115691	420995.025249	39.470618
2701.889442	421624.273925	39.475636
2704.810654	422252.519541	39.480653
2707.265120	422902.511253	39.485671
2710.085817	423544.739414	39.490688
2713.028244	424182.832804	39.495706
2715.440136	424834.994264	39.500724
2718.395630	425486.139653	39.505741
2721.068994	426139.937106	39.510759
2724.076664	426790.071607	39.515776
2726.830804	427448.060464	39.520794
2729.495461	428096.992866	39.525812
2732.392065	428760.628501	39.530829
2735.215023	429426.881984	39.535847
2738.218629	430071.754026	39.540864
2740.939225	430739.192366	39.545882
2743.626741	431404.389302	39.550900
2746.538862	432063.463519	39.555917
2748.854477	432727.056290	39.560935
2752.075694	433400.996761	39.565952
2754.670667	434063.489429	39.570970
2757.564871	434736.221686	39.575988
2760.459749	435398.166823	39.581005
2763.334355	436075.605401	39.586023
2766.157386	436733.169996	39.591040
2769.057232	437405.403479	39.596058
2771.939891	438076.554845	39.601076
2775.323755	438740.783308	39.606093
2777.921109	439414.811708	39.611111
2780.865564	440074.514914	39.616128
2783.768397	440737.788282	39.621146
2786.299746	441405.339664	39.626164
2789.666479	442061.017000	39.631181
2791.979978	442726.534498	39.636199
2795.075471	443386.400057	39.641216
2798.116689	444043.927093	39.646234
2800.751475	444704.474192	39.651252
2804.026914	445355.099154	39.656269
2806.731535	446022.709222	39.661287
2809.508361	446667.405944	39.666304
2812.565090	447315.217605	39.671322
2815.181280	447966.559457	39.676340
2817.807795	448621.613032	39.681357
2820.747555	449283.360197	39.686375
2823.734958	449931.442337	39.691392
2826.352737	450586.880132	39.696410
2829.263469	451244.520121	39.701428
2831.958005	451878.440339	39.706445
2834.509597	452506.907794	39.711463
2837.451429	453127.769764	39.716480
2839.940348	453753.375624	39.721498
2842.504353	454375.464357	39.726516
2845.839247	454995.441830	39.731533
2848.496783	455625.800637	39.736551
2851.230673	456254.459074	39.741568
2853.763913	456890.697238	39.746586
2856.102370	457526.235962	39.751604
2859.114025	458166.036975	39.756621
2861.793637	458815.101848	39.761639
2864.408151	459466.928077	39.766656
2867.449325	460129.512629	39.771674
2870.047645	460786.135806	39.776692
2873.025960	461456.651780	39.781709
2875.579556	462140.427799	39.786727
2878.574301	462802.562533	39.791744
2881.565635	463482.028126	39.796762
2884.317103	464164.177834	39.801780
2887.059089	464842.820321	39.806797
2890.165448	465531.972459	39.811815
2893.089104	466224.857772	39.816832
2895.849388	466929.644578	39.821850
2898.765272	467625.247249	39.826868
2901.927104	468328.802158	39.831885
2904.520710	469032.315103	39.836903
2907.590495	469731.890484	39.841920
2910.486888	470446.038339	39.846938
2913.163782	471160.239820	39.851956
2916.380167	471869.736709	39.856973
2919.245750	472605.882665	39.861991
2922.175237	473314.100731	39.867008
2925.406559	474040.039540	39.872026
2928.159869	474765.869181	39.877044
2931.273406	475495.038128	39.882061
2934.592554	476222.679739	39.887079
2937.358136	476957.230931	39.892096
2940.571604	477689.056909	39.897114
2943.077759	478421.967958	39.902132
2946.227569	479140.731672	39.907149
2949.301059	479884.676342	39.912167
2952.331489	480614.177918	39.917184
2955.380269	481352.210523	39.922202
2958.149207	482093.729451	39.927220
2961.607783	482825.580875	39.932237
2964.783696	483570.039973	39.937255
2967.661600	484297.881547	39.942272
2970.718836	485033.420411	39.947290
2973.884800	485769.461438	39.952308
2976.712360	486505.419401	39.957325
2979.702035	487231.442316	39.962343
2982.562650	487973.521257	39.967360
2985.686475	488710.938838	39.972378
2988.774079	489442.785374	39.977396
2991.944070	490178.361436	39.982413
2994.904378	490923.705757	39.987431
2997.908646	491650.673545	39.992448
3000.941412	492390.192323	39.997466
3003.621858	493133.053458	40.002484
3006.711007	493871.986602	40.007501
3009.837571	494612.589319	40.012519
3012.668331	495348.518602	40.017536
3016.052294	496084.123433	40.022554
3018.788082	496832.228791	40.027572
3022.209790	497564.632358	40.032589
3025.001487	498306.159537	40.037607
3027.982779	499036.695807	40.042624
3031.176523	499762.631968	40.047642
3033.983728	500481.243513	40.052660
3036.789304	501174.552924	40.057677
3039.845243	501878.610961	40.062695
3042.326481	502568.733504	40.067712
3045.942303	503275.001265	40.072730
3048.599899	504001.563503	40.077748
3051.393712	504708.442816	40.082765
3054.245510	505418.397808	40.087783
3056.968566	506141.067290	40.092800
3060.473709	506869.564946	40.097818
3063.193776	507611.429727	40.102836
3066.103067	508330.084708	40.107853
3069.295635	509075.370541	40.112871
3072.329715	509824.263409	40.117888
3075.340229	510571.761909	40.122906
3078.517106	511316.629340	40.127924
3081.657089	512066.793920	40.132941
3084.538370	512821.233253	40.137959
3087.235706	513592.808655	40.142976
3090.904883	514361.775382	40.147994
3093.561528	515135.031033	40.153012
3096.719497	515893.181448	40.158029
3099.898215	516674.213085	40.163047
3102.842788	517446.840966	40.168064
3106.168226	518228.213310	40.173082
3108.967929	519024.150561	40.178100
3112.586321	519813.931535	40.183117
3115.493049	520604.481356	40.188135
3118.680038	521404.389839	40.193152
3122.297582	522195.388549	40.198170
3125.268984	522989.808640	40.203188
3128.620710	523789.800419	40.208205
3131.881999	524586.643017	40.213223
3134.864412	525398.454370	40.218240
3138.402544	526196.915656	40.223258
3141.627596	526987.540495	40.228276
3144.873804	527795.043991	40.233293
3148.036268	528594.674772	40.238311
3151.314562	529402.526537	40.243328
3154.814406	530198.289720	40.248346
3157.687918	531010.625692	40.253364
3160.742974	531803.999857	40.258381
3164.454217	532603.901765	40.263399
3167.300055	533404.140591	40.268416
3170.906899	534205.466077	40.273434
3174.176906	535005.539133	40.278452
3177.723013	535809.585697	40.283469
3180.959715	536600.929193	40.288487
3184.407101	537399.369023	40.293504
3187.731779	538189.646358	40.298522
3190.598606	538988.629279	40.303540
3194.010394	539770.010899	40.308557
3197.156818	540570.456192	40.313575
3200.124838	541367.215189	40.318592
3203.632898	542150.190454	40.323610
3206.981532	542954.968306	40.328628
3210.364234	543749.955457	40.333645
3213.669265	544536.174506	40.338663
3216.772597	545327.040835	40.343680
3220.050663	546111.809789	40.348698
3223.318459	546898.988380	40.353716
3226.302341	547688.368013	40.358733
3229.882135	548469.679531	40.363751
3233.005005	549268.966594	40.368768
3236.579700	550053.788703	40.373786
3239.357346	550842.395607	40.378804
3242.534140	551628.031001	40.383821
3245.816532	552396.401873	40.388839
3248.664887	553151.656635	40.393856
3252.292458	553895.663335	40.398874
3255.017481	554640.517130	40.403892
3257.757499	555398.054223	40.408909
3260.926161	556148.459389	40.413927
3263.853801	556918.601969	40.418944
3267.673334	557676.527690	40.423962
3270.623798	558455.137186	40.428980
3273.606001	559217.305032	40.433997
3276.781737	559994.976495	40.439015
3279.516443	560780.331413	40.444032
3282.770560	561570.963517	40.449050
3286.038982	562376.568925	40.454068
3289.304648	563166.941492	40.459085
3292.466604	563976.210458	40.464103
3295.514450	564798.212898	40.469120
3298.395361	565602.103882	40.474138
3301.817897	566448.671427	40.479156
3305.063229	567275.074832	40.484173
3308.601332	568108.984126	40.489191
3311.845520	568947.485197	40.494208
3315.161321	569792.422157	40.499226
3318.193990	570647.303010	40.504244
3321.352578	571498.245923	40.509261
3324.781683	572358.643037	40.514279
3327.787780	573231.353118	40.519296
3331.309803	574100.061942	40.524314
3334.727482	574985.433975	40.529332
3338.245484	575858.111532	40.534349
3342.073192	576728.021213	40.539367
3344.958636	577620.023540	40.544384
3348.614562	578498.127437	40.549402
3352.098653	579391.345492	40.554420
3355.477216	580278.356246	40.559437
3359.425993	581166.007172	40.564455
3362.317525	582059.453221	40.569472
3365.946299	582945.610997	40.574490
3369.646363	583835.436371	40.579508
3373.024017	584727.539888	40.584525
3376.515115	585632.051204	40.589543
3380.063675	586523.531551	40.594560
3383.515136	587415.403971	40.599578
3387.088817	588303.885345	40.604596
3390.583444	589204.500456	40.609613
3394.578146	590087.072258	40.614631
3397.569645	590973.975902	40.619648
3401.452960	591855.220873	40.624666
3404.958507	592744.995606	40.629684
3408.581151	593623.387984	40.634701
3412.074191	594510.619674	40.639719
3415.664675	595390.120162	40.644736
3419.068299	596260.736975	40.649754
3422.584626	597134.860180	40.654772
3425.791320	598015.101430	40.659789
3429.400698	598892.160359	40.664807
3433.092470	599776.821886	40.669824
3436.665241	600647.349139	40.674842
3439.967742	601515.699624	40.679860
3443.197855	602394.970228	40.684877
3446.859602	603268.908357	40.689895
3450.509988	604142.225648	40.694912
3453.922983	605016.304746	40.699930
3457.368221	605886.063487	40.704948
3461.034028	606755.065644	40.709965
3464.645799	607630.488262	40.714983
3467.798608	608499.073600	40.720000
3471.566716	609363.149317	40.725018
3474.807236	610215.707726	40.730023
3477.895298	611033.605261	40.735028
3481.213744	611800.854954	40.740032
3484.646583	612532.234076	40.745037
3487.363947	613187.188895	40.750042
3490.391846	613807.412299	40.755047
3492.965906	614352.193746	40.760052
3495.669561	614845.495117	40.765056
3498.496208	615304.017881	40.770061
3500.848473	615696.724716	40.775066
3503.101106	616047.952577	40.780071
3505.169825	616348.274016	40.785076
3507.203749	616578.630871	40.790080
3508.369436	616783.083125	40.795085
3510.306596	616945.285567	40.800090
3511.578820	617072.810366	40.805095
3513.118457	617155.869013	40.810100
3514.661791	617198.401444	40.815104
3515.544871	617214.303460	40.820109
3516.855741	617199.157721	40.825114
3517.895347	617148.076422	40.830119
3518.614275	617077.856607	40.835124
3519.831226	616980.974288	40.840128
3520.299987	616854.425368	40.845133
3521.225446	616715.810274	40.850138
3521.610867	616554.390340	40.855143
3522.004898	616376.625198	40.860148
3522.756861	616167.067281	40.865152
3523.307937	615960.534909	40.870157
3523.592691	615736.947967	40.875162
3524.018593	615485.846247	40.880167
3523.912122	615243.717726	40.885172
3524.439977	614981.542096	40.890176
3524.360522	614711.557474	40.895181
3524.396104	614432.250784	40.900186
3524.979371	614157.849158	40.905191
3524.969353	613855.440790	40.910196
3524.944980	613552.075828	40.915200
3524.841863	613259.611617	40.920205
3524.873614	612951.320911	40.925210
3524.814067	612636.286164	40.930215
3524.966879	612331.057108	40.935220
3524.803251	612016.519261	40.940224
3525.000169	611707.714873	40.945229
3524.251381	611386.449413	40.950234
3524.032077	611060.241033	40.955239
3523.926710	610746.104662	40.960244
3523.602313	610432.892871	40.965248
3523.659734	610127.362408	40.970253
3523.575190	609820.444808	40.975258
3523.584215	609499.151239	40.980263
3523.128033	609190.372486	40.985268
3523.188518	608874.352134	40.990272
3523.159425	608561.236705	40.995277
3522.616629	608241.590214	41.000282
3522.638382	607935.849690	41.005287
3522.301598	607627.355166	41.010292
3522.327218	607318.244507	41.015296
3521.875066	607016.251974	41.020301
3521.420063	606715.601570	41.025306
3521.386369	606424.780938	41.030311
3520.968420	606126.808730	41.035316
3520.985122	605834.662926	41.040320
3520.567407	605551.931729	41.045325
3520.310085	605256.410566	41.050330
3520.130076	604969.423889	41.055335
3520.040445	604689.269328	41.060340
3519.747252	604407.037649	41.065344
3519.547997	604127.135159	41.070349
3519.736999	603855.970536	41.075354
3519.482485	603581.015373	41.080359
3518.968266	603310.696963	41.085364
3519.029105	603042.833587	41.090368
3518.544328	602764.239952	41.095373
3518.263624	602498.917951	41.100378
3518.050030	602237.231802	41.105383
3517.562268	601989.043722	41.110388
3517.406561	601731.989899	41.115392
3516.958614	601487.937395	41.120397
3516.741740	601241.540879	41.125402
3517.298597	601003.325650	41.130407
3516.721143	600761.778841	41.135412
3516.105964	600531.994285	41.140416
3516.239062	600308.944808	41.145421
3515.913104	600072.197784	41.150426
3515.805923	599847.223970	41.155431
3515.481882	599621.478348	41.160436
3515.228272	599388.358591	41.165440
3515.159374	599172.324380	41.170445
3514.909558	598958.666749	41.175450
3514.772289	598751.995479	41.180455
3514.226487	598544.883409	41.185460
3514.340485	598333.859461	41.190464
3514.028167	598132.660067	41.195469
3513.927246	597923.964366	41.200474
3513.903886	597732.023902	41.205479
3513.535064	597528.669053	41.210484
3513.537123	597331.260229	41.215488
3513.261874	597142.302312	41.220493
3513.121355	596949.114255	41.225498
3513.046349	596763.623010	41.230503
3512.597330	596571.477653	41.235508
3512.486821	596395.048093	41.240512
3512.401267	596219.312689	41.245517
3512.221585	596041.636272	41.250522
3512.379727	595861.851074	41.255527
3512.020452	595681.292461	41.260532
3511.836794	595511.569520	41.265536
3511.427074	595356.000464	41.270541
3511.547256	595175.358291	41.275546
3511.216908	595011.108588	41.280551
3511.127864	594846.718468	41.285556
3511.223372	594687.505122	41.290560
3510.924153	594539.518770	41.295565
3510.796764	594378.532797	41.300570
3510.879639	594218.412973	41.305575
3510.720751	594064.588720	41.310580
3510.456749	593906.371448	41.315584
3510.339589	593760.699678	41.320589
3510.295525	593613.662237	41.325594
3510.118487	593473.455013	41.330599
3509.998632	593325.323597	41.335604
3509.958539	593181.685360	41.340608
3509.996586	593044.043327	41.345613
3509.368839	592909.258381	41.350618
3509.273566	592766.925456	41.355623
3508.978309	592632.836361	41.360628
3509.150902	592505.284164	41.365632
3509.167854	592371.443521	41.370637
3508.767378	592236.664662	41.375642
3509.035128	592113.350574	41.380647
3509.003102	591998.948061	41.385652
3508.794314	591865.537121	41.390656
3508.546240	591732.180755	41.395661
3508.740285	591616.686887	41.400666
3508.876190	591493.586662	41.405671
3508.376117	591374.792346	41.410676
3508.521378	591248.682211	41.415680
3508.375405	591135.340298	41.420685
3508.198061	591016.691952	41.425690
3507.985767	590908.618062	41.430695
3507.751635	590796.238184	41.435700
3507.752143	590678.710531	41.440704
3507.554364	590584.357757	41.445709
3507.183440	590476.855404	41.450714
3507.214456	590367.235096	41.455719
3507.413241	590267.557187	41.460724
3507.481166	590162.638351	41.465728
3506.984602	590061.263650	41.470733
3506.750575	589959.145544	41.475738
3506.954988	589872.639558	41.480743
3506.698869	589783.298991	41.485748
3506.686506	589676.684533	41.490752
3506.702135	589590.857127	41.495757
3506.430388	589501.366363	41.500762
3506.595543	589393.919719	41.505767
3506.303643	589314.200680	41.510772
3506.173291	589224.585312	41.515776
3506.008854	589138.582048	41.520781
3506.047056	589053.849147	41.525786
3506.247441	588969.290649	41.530791
3505.682675	588890.913880	41.535796
3505.831466	588813.577430	41.540800
3505.805951	588739.374265	41.545805
3505.850583	588655.739580	41.550810
3506.059403	588568.270448	41.555815
3505.597970	588493.482353	41.560820
3505.740821	588404.468882	41.565824
3505.539825	588340.111541	41.570829
3505.976983	588254.859050	41.575834
3506.026877	588171.169697	41.580839
3505.436446	588104.867483	41.585844
3505.464367	588035.461628	41.590848
3505.780476	587954.134240	41.595853
3505.370605	587881.789247	41.600858
3505.591025	587811.249441	41.605863
3505.325798	587729.660478	41.610868
3505.308815	587649.735878	41.615872
3505.399708	587584.376309	41.620877
3505.391953	587512.166437	41.625882
3505.472457	587444.903402	41.630887
3505.260697	587375.029673	41.635892
3505.252770	587292.695629	41.640896
3505.060227	587224.521769	41.645901
3504.751122	587155.664113	41.650906
3504.998242	587094.536831	41.655911
3504.845711	587035.325906	41.660916
3505.346700	586959.374503	41.665920
3505.132345	586891.201964	41.670925
3504.572703	586836.614044	41.675930
3504.938930	586765.844207	41.680935
3504.711476	586707.294710	41.685940
3504.676861	586646.058608	41.690944
3504.985937	586581.410648	41.695949
3504.654112	586517.864826	41.700954
3504.622347	586463.142395	41.705959
3504.295346	586399.545012	41.710964
3504.598795	586327.829923	41.715968
3504.671124	586265.572618	41.720973
3504.280157	586221.730539	41.725978
3504.379547	586154.205991	41.730983
3504.267964	586113.427127	41.735988
3504.685624	586045.350969	41.740992
3504.128347	585988.653444	41.745997
3504.103825	585938.638428	41.751002
3504.086673	585886.968091	41.756007
3504.076030	585834.494578	41.761012
3504.253665	585773.621357	41.766016
3503.934548	585727.410421	41.771021
3504.007189	585661.039769	41.776026
3504.215985	585609.382919	41.781031
3504.046454	585570.214946	41.786036
3504.110639	585519.883421	41.791040
3504.247952	585464.628344	41.796045
3504.169202	585418.378524	41.801050
3503.979897	585358.562786	41.806055
3503.496330	585308.867259	41.811060
3504.400062	585253.591548	41.816064
3503.961924	585213.361596	41.821069
3503.661591	585158.373878	41.826074
3503.764471	585105.678630	41.831079
3503.453280	585065.428289	41.836084
3503.791403	585013.347423	41.841088
3503.614568	584970.469311	41.846093
3503.534632	584930.082073	41.851098
3503.659150	584882.094002	41.856103
3503.469594	584837.613390	41.861108
3503.464144	584792.201577	41.866112
3503.407264	584744.090886	41.871117
3503.514945	584704.475481	41.876122
3503.492011	584653.902971	41.881127
3503.405599	584625.595752	41.886132
3503.079943	584579.380987	41.891136
3503.210811	584543.119774	41.896141
3503.201751	584491.842590	41.901146
3502.970605	584460.750527	41.906151
3503.181911	584421.518908	41.911156
3503.419742	584385.942221	41.916160
3503.179514	584348.585474	41.921165
3502.915564	584299.352294	41.926170
3503.150868	584262.722942	41.931175
3503.209107	584240.858478	41.936180
3503.262777	584199.344869	41.941184
3503.262043	584170.672192	41.946189
3503.426542	584133.451952	41.951194
3503.344217	584096.971957	41.956199
3503.233813	584055.583709	41.961204
3503.164534	584011.331581	41.966208
3503.298803	583976.120652	41.971213
3503.297406	583930.453999	41.976218
3503.416020	583886.422636	41.981223
3502.994812	583855.960114	41.986228
3503.154592	583808.112221	41.991232
3503.677426	583780.058482	41.996237
3503.509935	583735.068660	42.001242
3503.334742	583689.779080	42.006247
3502.898498	583661.473934	42.011252
3503.240433	583606.127377	42.016256
3503.324545	583571.775202	42.021261
3503.382488	583535.672456	42.026266
3503.374054	583506.698470	42.031271
3503.379399	583475.466386	42.036276
3503.274942	583433.523430	42.041280
3503.267164	583388.406960	42.046285
3503.192321	583350.920702	42.051290
3503.007222	583309.741846	42.056295
3503.115703	583270.271539	42.061300
3503.273615	583235.756384	42.066304
3502.822508	583187.449845	42.071309
3503.227083	583160.365521	42.076314
3503.423844	583117.070843	42.081319
3502.996716	583091.469933	42.086324
3503.062482	583048.446124	42.091328
3503.248097	583015.229389	42.096333
3503.169023	582971.375669	42.101338
3503.295967	582939.471329	42.106343
3503.346616	582900.510067	42.111348
3503.416218	582854.176118	42.116352
3503.429330	582817.877495	42.121357
3503.091104	582788.953176	42.126362
3503.327112	582746.553312	42.131367
3502.794737	582713.347642	42.136372
3502.885384	582682.501045	42.141376
3502.984640	582639.670942	42.146381
3502.996966	582604.073616	42.151386
3503.055156	582564.859317	42.156391
3502.949679	582536.299027	42.161396
3502.963248	582497.342137	42.166400
3503.013853	582461.086613	42.171405
3503.150109	582446.325563	42.176410
3503.254866	582389.004570	42.181415
3502.680655	582372.298937	42.186420
3502.704383	582324.365600	42.191424
3503.145726	582288.299103	42.196429
3502.708407	582262.146363	42.201434
3503.029441	582233.769293	42.206439
3502.963972	582205.452572	42.211444
3502.939063	582158.829661	42.216448
3502.701153	582128.183288	42.221453
3502.589615	582096.915433	42.226458
3503.032583	582063.705742	42.231463
3502.805297	582039.725660	42.236468
3502.988146	582006.807147	42.241472
3502.975181	581972.064068	42.246477
3502.606717	581944.295417	42.251482
3503.248998	581909.399571	42.256487
3502.613199	581877.160162	42.261492
3502.867800	581840.319196	42.266496
3502.778134	581805.437171	42.271501
3502.525087	581768.424634	42.276506
3502.739174	581734.096557	42.281511
3502.432144	581706.468118	42.286516
3502.712753	581688.274074	42.291520
3502.890693	581663.427610	42.296525
3502.851339	581625.629109	42.301530
3502.890638	581590.174717	42.306535
3502.817083	581561.456498	42.311540
3502.847351	581519.635621	42.316544
3502.824398	581495.271439	42.321549
3502.457230	581464.041756	42.326554
3502.896297	581439.504945	42.331559
3502.571347	581411.076334	42.336564
3502.760153	581378.455860	42.341568
3502.957382	581342.073465	42.346573
3502.883863	581309.794639	42.351578
3502.874088	581275.650557	42.356583
3502.502612	581242.565726	42.361588
3503.086699	581208.027756	42.366592
3503.051934	581187.224734	42.371597
3502.581243	581151.046408	42.376602
3502.899926	581116.900631	42.381607
3502.744255	581085.787240	42.386612
3502.756874	581048.730765	42.391616
3503.135756	581023.299897	42.396621
3502.693822	580990.676602	42.401626
3502.798756	580963.533463	42.406631
3502.883830	580925.512554	42.411636
3502.948025	580892.609279	42.416640
3502.895735	580867.596455	42.421645
3502.515316	580833.208099	42.426650
3502.620647	580798.292416	42.431655
3502.986738	580769.653843	42.436660
3502.677033	580741.271270	42.441664
3503.041750	580713.635624	42.446669
3502.834890	580682.829961	42.451674
3502.977743	580637.427995	42.456679
3502.712087	580612.548237	42.461684
3502.921412	580574.657132	42.466688
3502.999125	580543.505734	42.471693
3502.879597	580509.025444	42.476698
3502.872897	580472.220781	42.481703
3502.893744	580451.858982	42.486708
3503.005916	580413.731796	42.491712
3502.572953	580391.084045	42.496717
3502.405164	580352.799837	42.501722
3502.739231	580313.183423	42.506727
3502.669197	580291.381339	42.511732
3502.777281	580270.153106	42.516736
3503.321656	580236.520936	42.521741
3502.819404	580202.400395	42.526746
3502.757157	580181.599782	42.531751
3502.636748	580137.540707	42.536756
3502.537246	580117.096817	42.541760
3502.675125	580080.769713	42.546765
3502.300938	580067.940689	42.551770
3502.604644	580027.976985	42.556775
3502.988430	580009.312749	42.561780
3502.646862	579979.228238	42.566784
3502.838026	579941.889425	42.571789
3502.507449	579908.142311	42.576794
3502.925288	579871.971346	42.581799
3502.766159	579843.412496	42.586804
3503.060388	579818.042255	42.591808
3502.784130	579775.109341	42.596813
3502.444773	579747.581363	42.601818
3502.496248	579721.797527	42.606823
3502.613236	579702.823454	42.611828
3502.448348	579662.229627	42.616832
3502.796022	579636.399288	42.621837
3502.635109	579608.792923	42.626842
3502.400468	579578.590314	42.631847
3502.223859	579560.564562	42.636852
3502.378596	579526.289087	42.641856
3502.717726	579502.716449	42.646861
3502.472023	579478.934295	42.651866
3502.783622	579446.740292	42.656871
3502.451998	579417.705828	42.661876
3502.477650	579391.223179	42.666880
3502.696697	579366.164557	42.671885
3502.258313	579336.043290	42.676890
3502.166365	579298.746579	42.681895
3502.469287	579283.905121	42.686900
3502.378516	579261.703064	42.691904
3502.568252	579227.220600	42.696909
3502.673422	579213.563405	42.701914
3502.474454	579166.102582	42.706919
3502.348965	579146.162469	42.711924
3502.130805	579127.490560	42.716928
3502.575870	579093.569570	42.721933
3502.594596	579082.683992	42.726938
3502.549963	579044.977833	42.731943
3502.509519	579023.319089	42.736948
3502.282536	578991.759625	42.741952
3502.485553	578967.354573	42.746957
3502.348080	578945.209336	42.751962
3502.648879	578911.059590	42.756967
3502.733362	578892.540580	42.761972
3502.203931	578866.544670	42.766976
3502.475096	578839.320212	42.771981
3502.269207	578814.427084	42.776986
3502.496833	578787.911428	42.781991
3502.604948	578769.238064	42.786996
3502.443996	578733.856016	42.792001
3502.753890	578705.070469	42.797005
3502.372653	578679.301714	42.802010
3502.431575	578647.345515	42.807015
3502.284926	578634.830329	42.812020
3502.067642	578603.067639	42.817025
3502.289567	578578.357866	42.822029
3502.143421	578556.112908	42.827034
3502.386637	578526.334270	42.832039
3502.491668	578509.466455	42.837044
3502.137647	578485.097278	42.842049
3502.733225	578458.974698	42.847053
3502.229633	578432.773123	42.852058
3502.561259	578401.525888	42.857063
3502.582644	578380.959605	42.862068
3502.097059	578351.896277	42.867073
3502.288574	578331.303307	42.872077
3502.391038	578305.608533	42.877082
3502.553864	578271.729172	42.882087
3502.447423	578263.420215	42.887092
3502.787644	578225.450508	42.892097
3502.639163	578196.534692	42.897101
3502.645627	578172.660175	42.902106
3502.557000	578142.681621	42.907111
3502.459882	578121.832459	42.912116
3502.558534	578083.699417	42.917121
3502.435287	578064.509342	42.922125
3501.905349	578034.298557	42.927130
3502.629792	578014.775258	42.932135
3502.608369	577984.735619	42.937140
3502.684384	577963.959409	42.942145
3502.762628	577927.383840	42.947149
3502.544958	577895.518886	42.952154
3502.837294	577866.081903	42.957159
3502.261144	577838.435756	42.962164
3501.950205	577820.378033	42.967169
3502.734113	577792.719782	42.972173
3502.214905	577758.494083	42.977178
3502.724094	577737.649735	42.982183
3502.549258	577715.206962	42.987188
3502.205353	577688.928519	42.992193
3502.256615	577655.716770	42.997197
3501.955560	577633.594504	43.002202
3501.977414	577606.857435	43.007207
3502.140944	577591.634271	43.012212
3502.101919	577574.988197	43.017217
3502.095318	577548.456065	43.022221
3502.406567	577541.385360	43.027226
3502.552139	577513.224325	43.032231
3502.354379	577492.138936	43.037236
3502.638847	577463.604960	43.042241
3502.583781	577431.061216	43.047245
3502.471572	577409.861983	43.052250
3502.727237	577389.207095	43.057255
3502.264083	577358.031040	43.062260
3502.211277	577332.308148	43.067265
3502.669684	577304.850057	43.072269
3502.228830	577284.905762	43.077274
3502.615763	577247.727975	43.082279
3502.586061	577227.267877	43.087284
3502.295483	577194.659946	43.092289
3502.580527	577169.335293	43.097293
3502.419367	577142.224455	43.102298
3502.420328	577112.780886	43.107303
3502.218633	577090.842652	43.112308
3502.011423	577062.484838	43.117313
3502.385571	577044.770197	43.122317
3502.012810	577023.861763	43.127322
3502.534435	576995.590481	43.132327
3502.366374	576975.302031	43.137332
3502.043242	576954.586347	43.142337
3502.716684	576927.143877	43.147341
3502.309927	576904.434775	43.152346
3502.317732	576878.751527	43.157351
3502.436489	576852.749914	43.162356
3502.206641	576826.050332	43.167361
3502.537405	576795.651486	43.172365
3502.262408	576778.990958	43.177370
3502.283757	576750.646786	43.182375
3502.172735	576736.669242	43.187380
3501.748324	576720.483432	43.192385
3502.372868	576689.637086	43.197389
3502.463399	576670.361040	43.202394
3502.490920	576641.012404	43.207399
3502.399987	576620.008997	43.212404
3502.330606	576589.922955	43.217409
3502.399551	576554.498077	43.222413
3502.148354	576543.451580	43.227418
3502.243949	576507.069313	43.232423
3502.239547	576495.332084	43.237428
3502.228509	576468.948579	43.242433
3502.279755	576449.728458	43.247437
3502.192957	576433.539617	43.252442
3501.809736	576402.147756	43.257447
3502.135161	576385.041643	43.262452
3502.198006	576359.198116	43.267457
3502.416052	576336.139374	43.272461
3502.401104	576308.853177	43.277466
3502.120615	576278.749142	43.282471
3502.403671	576267.869669	43.287476
3502.074122	576246.902866	43.292481
3502.615644	576217.221956	43.297485
3502.392854	576197.341960	43.302490
3502.508730	576168.379584	43.307495
3502.622562	576146.992138	43.312500
3501.963927	576117.699238	43.317505
3502.499694	576098.653591	43.322509
3502.462100	576079.145744	43.327514
3502.504560	576047.836838	43.332519
3502.300487	576017.569665	43.337524
3502.294183	575992.187582	43.342529
3502.355398	575969.604084	43.347533
3501.992124	575936.702876	43.352538
3502.493304	575917.913154	43.357543
3502.608059	575896.424759	43.362548
3502.273322	575872.749180	43.367553
3502.274968	575840.191960	43.372557
3501.999557	575820.871337	43.377562
3502.308797	575802.111428	43.382567
3502.143005	575778.158414	43.387572
3501.882899	575755.273563	43.392577
3502.381768	575734.126132	43.397581
3502.518283	575717.098704	43.402586
3502.523449	575682.734524	43.407591
3502.077830	575665.346532	43.412596
3502.339414	575637.212827	43.417601
3502.700770	575609.314285	43.422605
3502.423307	575592.351385	43.427610
3502.328139	575566.731405	43.432615
3502.477264	575550.654909	43.437620
3502.557756	575521.796734	43.442625
3502.485948	575483.480846	43.447629
3501.986572	575466.301615	43.452634
3502.361001	575430.574611	43.457639
3502.402696	575413.009714	43.462644
3502.082270	575388.628545	43.467649
3502.260826	575363.416813	43.472653
3502.238745	575349.523974	43.477658
3502.266731	575315.757112	43.482663
3502.293553	575299.147539	43.487668
3502.269184	575275.873690	43.492673
3502.175131	575244.533725	43.497677
3502.143359	575229.087060	43.502682
3502.113177	575211.332415	43.507687
3502.288863	575190.987006	43.512692
3502.134224	575163.920543	43.517697
3501.983953	575135.097454	43.522701
3502.380059	575130.169201	43.527706
3502.216057	575092.167403	43.532711
3502.221250	575073.453816	43.537716
3501.960687	575053.226525	43.542721
3502.695675	575029.181270	43.547725
3502.286148	575008.525670	43.552730
3502.490612	574984.713762	43.557735
3502.013662	574962.814403	43.562740
3502.047080	574926.035401	43.567745
3502.355554	574905.317537	43.572749
3502.190321	574894.205810	43.577754
3502.289463	574871.664354	43.582759
3502.570485	574853.509312	43.587764
3502.061167	574823.938850	43.592769
3502.391223	574801.060139	43.597773
3502.344664	574771.567705	43.602778
3502.260681	574752.365831	43.607783
3501.970778	574728.881516	43.612788
3501.926397	574708.118113	43.617793
3502.447144	574681.597119	43.622797
3502.179295	574663.728257	43.627802
3501.911450	574637.129759	43.632807
3501.849900	574618.425852	43.637812
3502.202184	574593.837458	43.642817
3502.422149	574574.788448	43.647821
3502.494894	574548.337178	43.652826
3502.485203	574522.751636	43.657831
3502.287504	574495.439448	43.662836
3502.339375	574472.352707	43.667841
3502.490597	574439.868405	43.672845
3502.132289	574425.826307	43.677850
3502.515249	574400.078762	43.682855
3502.360528	574367.943108	43.687860
3502.139428	574342.942093	43.692865
3502.296077	574320.541063	43.697869
3502.077190	574293.733416	43.702874
3502.226979	574288.542276	43.707879
3502.191157	574253.277061	43.712884
3501.754127	574244.013370	43.717889
3502.123386	574211.644844	43.722893
3501.857900	574207.371511	43.727898
3501.879478	574178.569287	43.732903
3502.044437	574164.846440	43.737908
3501.960269	574133.802881	43.742913
3501.731903	574112.866457	43.747917
3502.028383	574109.157478	43.752922
3501.759134	574085.367560	43.757927
3502.025743	574072.481645	43.762932
3501.764439	574054.610795	43.767937
3501.887518	574033.920321	43.772941
3501.823955	574025.350659	43.777946
3501.957328	574005.009733	43.782951
3502.119815	573992.742080	43.787956
3501.712476	573963.354111	43.792961
3502.320819	573947.454414	43.797965
3501.571957	573921.531506	43.802970
3501.943187	573900.049394	43.807975
3501.854366	573897.504396	43.812980
3501.556771	573878.936513	43.817985
3501.833862	573858.171468	43.822989
3501.920325	573848.775441	43.827994
3502.071139	573823.213399	43.832999
3502.248437	573813.602447	43.838004
3501.978004	573789.561223	43.843009
3502.067547	573764.410018	43.848013
3502.051321	573744.041836	43.853018
3502.374038	573716.646412	43.858023
3502.151737	573701.026747	43.863028
3501.621467	573676.724856	43.868033
3502.134435	573654.417331	43.873037
3501.786936	573647.547530	43.878042
3502.128158	573625.015923	43.883047
3501.958641	573609.387880	43.888052
3501.888204	573587.522650	43.893057
3501.956118	573555.901809	43.898061
3501.761888	573551.316037	43.903066
3501.865387	573530.527355	43.908071
3501.999977	573515.604268	43.913076
3501.787075	573496.019014	43.918081
3501.872100	573484.264674	43.923085
3501.724356	573465.221108	43.928090
3501.777138	573445.544057	43.933095
3501.875537	573441.063020	43.938100
3501.842067	573411.564996	43.943105
3502.158068	573391.495474	43.948109
3501.918915	573376.429928	43.953114
3502.134521	573353.014256	43.958119
3502.057060	573329.493822	43.963124
3501.604804	573319.278406	43.968129
3501.797757	573305.399616	43.973133
3501.727494	573287.547865	43.978138
3501.555391	573270.113416	43.983143
3501.953210	573262.625104	43.988148
3501.615802	573238.191768	43.993153
3501.962833	573218.869736	43.998157
3501.723206	573200.392030	44.003162
3501.856885	573182.056642	44.008167
3502.031938	573169.083663	44.013172
3501.357342	573152.530415	44.018177
3501.516889	573132.183832	44.023181
3501.809828	573128.575444	44.028186
3501.971461	573106.673007	44.033191
3502.019815	573092.364969	44.038196
3501.622347	573071.151991	44.043201
3501.707510	573051.268486	44.048205
3501.785531	573050.905012	44.053210
3501.841109	573026.510140	44.058215
3502.354103	573015.491248	44.063220
3502.140017	572984.314318	44.068225
3502.399521	572960.339022	44.073229
3501.918366	572945.110024	44.078234
3501.698516	572923.718471	44.083239
3502.135978	572902.374654	44.088244
3501.836671	572877.633518	44.093249
3501.828208	572858.316269	44.098253
3501.717443	572850.806837	44.103258
3501.626939	572844.649042	44.108263
3501.883599	572821.125500	44.113268
3501.844181	572807.884568	44.118273
3501.672415	572790.650043	44.123277
3502.015978	572768.668336	44.128282
3502.040353	572757.825938	44.133287
3502.181114	572734.922478	44.138292
3501.589555	572720.663830	44.143297
3501.885068	572688.352671	44.148301
3502.022166	572684.116182	44.153306
3501.536785	572669.489619	44.158311
3501.884940	572649.664656	44.163316
3501.917223	572636.964285	44.168321
3501.927820	572612.675915	44.173325
3501.769989	572591.123501	44.178330
3501.830008	572580.526258	44.183335
3502.030702	572559.018095	44.188340
3501.928516	572550.051921	44.193345
3501.935357	572527.168979	44.198349
3501.896849	572499.024219	44.203354
3501.897490	572492.902164	44.208359
3502.020632	572468.595892	44.213364
3501.870465	572455.271503	44.218369
3502.041802	572431.409236	44.223373
3501.809848	572422.011627	44.228378
3501.828608	572397.972422	44.233383
3502.081942	572381.975504	44.238388
3501.702609	572364.622240	44.243393
3502.113698	572339.317254	44.248397
3502.131009	572327.773026	44.253402
3501.685374	572313.039428	44.258407
3501.755334	572285.178265	44.263412
3501.604084	572282.743024	44.268417
3501.926831	572257.903293	44.273421
3501.968293	572246.907194	44.278426
3501.609321	572223.729564	44.283431
3501.588541	572208.979595	44.288436
3501.584796	572202.908250	44.293441
3501.749556	572185.218750	44.298445
3501.677417	572173.738531	44.303450
3501.987737	572164.155574	44.308455
3502.610657	572146.143484	44.313460
3502.267098	572120.052723	44.318465
3502.066286	572089.373076	44.323469
3502.416899	572068.994725	44.328474
3502.229301	572045.037216	44.333479
3502.190696	572031.042528	44.338484
3501.933504	572006.694364	44.343489
3502.151151	571973.088624	44.348493
3501.909584	571957.620115	44.353498
3501.966473	571940.198009	44.358503
3502.019206	571909.277511	44.363508
3502.256205	571903.268737	44.368513
3501.858056	571873.823732	44.373517
3501.788161	571865.705071	44.378522
3502.365771	571830.135704	44.383527
3502.261633	571816.351727	44.388532
3501.948329	571792.563886	44.393537
3502.184486	571773.407287	44.398541
3502.424343	571754.701723	44.403546
3502.359011	571734.839446	44.408551
3502.018549	571714.769230	44.413556
3502.242984	571693.757555	44.418561
3502.009916	571667.397566	44.423565
3502.261659	571653.708308	44.428570
3501.812886	571631.296259	44.433575
3502.036012	571598.943146	44.438580
3502.179845	571582.109104	44.443585
3501.899439	571556.207912	44.448589
3501.536046	571532.276806	44.453594
3501.834624	571530.473656	44.458599
3501.750852	571509.108351	44.463604
3502.006746	571494.966598	44.468609
3501.996126	571479.963177	44.473613
3502.304032	571454.270888	44.478618
3501.761286	571431.371293	44.483623
3502.028571	571410.151660	44.488628
3501.681539	571405.839827	44.493633
3501.875692	571379.964416	44.498637
3501.518707	571366.771452	44.503642
3502.044934	571359.813855	44.508647
3501.713397	571332.364423	44.513652
3501.428455	571325.132135	44.518657
3501.821238	571310.266167	44.523661
3501.564742	571290.633740	44.528666
3501.831311	571267.356371	44.533671
3501.616229	571252.133689	44.538676
3501.562502	571239.595762	44.543681
3501.761719	571223.655867	44.548685
3501.955133	571209.724270	44.553690
3501.683703	571194.660875	44.558695
3501.896040	571183.887967	44.563700
3501.631930	571160.291857	44.568705
3501.937187	571136.405947	44.573709
3502.066072	571132.019610	44.578714
3501.880166	571116.892557	44.583719
3502.004598	571102.218827	44.588724
3501.809295	571079.715881	44.593729
3502.300201	571057.908592	44.598733
3501.728930	571037.973637	44.603738
3501.596658	571025.497940	44.608743
3501.708189	571011.327971	44.613748
3501.290596	570986.751772	44.618753
3501.935420	570958.948063	44.623757
3501.784310	570966.700353	44.628762
3501.704886	570934.894522	44.633767
3501.899036	570924.726452	44.638772
3501.687181	570913.517737	44.643777
3501.715609	570891.079817	44.648781
3501.986013	570880.197173	44.653786
3501.924234	570856.719365	44.658791
3502.343127	570838.486183	44.663796
3502.119664	570828.684434	44.668801
3501.945660	570806.328181	44.673805
3502.152620	570789.734039	44.678810
3502.075486	570769.922116	44.683815
3502.156898	570735.731786	44.688820
3501.756820	570717.124566	44.693825
3502.123865	570695.285764	44.698829
3502.326748	570678.993225	44.703834
3502.188860	570657.684975	44.708839
3502.276184	570633.480772	44.713844
3502.074617	570613.035587	44.718849
3502.371701	570592.412035	44.723853
3502.172486	570562.029158	44.728858
3501.827258	570551.493384	44.733863
3501.899448	570520.917405	44.738868
3501.802590	570510.894837	44.743873
3501.963972	570493.855698	44.748877
3501.886377	570474.093522	44.753882
3501.729069	570464.582249	44.758887
3501.959161	570433.128145	44.763892
3501.949466	570431.975282	44.768897
3502.014117	570397.284675	44.773901
3501.796658	570385.072540	44.778906
3501.882532	570380.341317	44.783911
3501.877401	570349.124511	44.788916
3502.259867	570340.934048	44.793921
3501.898016	570314.791824	44.798925
3501.885507	570298.331659	44.803930
3501.487959	570276.410830	44.808935
3501.798262	570260.753367	44.813940
3501.300001	570271.019681	44.818945
3501.673122	570239.643065	44.823949
3501.655123	570214.099322	44.828954
3501.490353	570207.299244	44.833959
3501.911698	570197.245582	44.838964
3501.652802	570176.306680	44.843969
3501.860768	570171.656665	44.848973
3502.021343	570153.613348	44.853978
3501.844571	570135.923881	44.858983
3501.999371	570115.472285	44.863988
3501.763768	570109.887785	44.868993
3501.965916	570089.830264	44.873997
3501.725250	570062.965857	44.879002
3501.652019	570050.178723	44.884007
3501.593379	570027.401388	44.889012
3501.535391	570014.662022	44.894017
3501.452957	570007.196476	44.899021
3501.692805	570005.954370	44.904026
3501.591705	569986.094645	44.909031
3501.781823	569959.564177	44.914036
3501.948958	569947.592596	44.919041
3501.823586	569937.021884	44.924045
3501.958631	569916.823977	44.929050
3501.608902	569896.099527	44.934055
3501.560077	569878.991953	44.939060
3501.657029	569871.297511	44.944065
3501.454997	569870.977718	44.949069
3501.693064	569843.636428	44.954074
3501.720902	569837.207550	44.959079
3501.864317	569815.100885	44.964084
3501.960361	569799.626863	44.969089
3501.682729	569787.373304	44.974093
3502.046166	569771.004186	44.979098
3501.470077	569746.751246	44.984103
3501.858828	569740.818002	44.989108
3501.478878	569722.958891	44.994113
3501.751904	569703.341341	44.999117
3501.956799	569692.618389	45.004122
3501.605015	569671.642894	45.009127
3501.728026	569653.705048	45.014132
3501.403124	569647.883321	45.019137
3501.520722	569616.344180	45.024141
3501.754428	569614.299915	45.029146
3501.824841	569615.192332	45.034151
3501.510770	569579.855765	45.039156
3501.500977	569567.560099	45.044161
3501.873453	569561.026998	45.049165
3501.989328	569545.147992	45.054170
3501.480485	569533.833774	45.059175
3502.026877	569526.671153	45.064180
3501.943656	569501.587753	45.069185
3501.979174	569479.798467	45.074189
3502.030287	569457.354194	45.079194
3501.783835	569456.890754	45.084199
3501.769741	569434.004891	45.089204
3501.689889	569418.758626	45.094209
3501.958182	569398.137432	45.099213
3501.668548	569374.993367	45.104218
3501.727816	569365.899064	45.109223
3501.999877	569358.678838	45.114228
3501.694612	569339.753392	45.119233
3501.766684	569314.645307	45.124237
3501.789102	569300.738125	45.129242
3501.376228	569289.408661	45.134247
3501.877415	569278.438230	45.139252
3501.605831	569258.453316	45.144257
3501.684818	569241.324811	45.149261
3501.703467	569232.337140	45.154266
3501.446652	569215.963808	45.159271
3501.796364	569199.997576	45.164276
3501.401871	569189.418052	45.169281
3501.568334	569170.067222	45.174285
3501.491125	569161.747007	45.179290
3501.355432	569155.242923	45.184295
3501.861860	569142.514743	45.189300
3501.529705	569125.902088	45.194305
3501.797266	569104.126010	45.199309
3501.911530	569100.192936	45.204314
3501.941690	569085.631754	45.209319
3501.773401	569069.294568	45.214324
3501.338382	569046.423541	45.219329
3501.770686	569020.555772	45.224333
3501.607245	569015.461405	45.229338
3501.237670	569007.387562	45.234343
3501.840191	568969.094906	45.239348
3501.761866	568966.496967	45.244353
3501.676877	568955.417085	45.249357
3501.687615	568945.677499	45.254362
3501.618047	568929.927025	45.259367
3501.804853	568916.997586	45.264372
3501.873250	568902.731367	45.269377
3501.965600	568885.048093	45.274381
3501.865864	568867.695994	45.279386
3501.614933	568854.383156	45.284391
3501.915404	568838.323730	45.289396
3502.094708	568817.715409	45.294401
3501.855781	568796.971649	45.299405
3501.707833	568791.422996	45.304410
3501.559379	568777.290914	45.309415
3501.540520	568766.551884	45.314420
3501.785506	568749.798265	45.319425
3501.683051	568725.669903	45.324429
3501.314990	568726.781524	45.329434
3500.975399	568712.829831	45.334439
3501.300763	568687.981959	45.339444
3501.139114	568680.176558	45.344449
3501.199443	568674.193718	45.349453
3501.789234	568677.063068	45.354458
3501.437832	568664.920233	45.359463
3501.728199	568640.278515	45.364468
3501.456803	568641.726408	45.369473
3501.339276	568644.254571	45.374477
3501.632721	568619.562131	45.379482
3501.130664	568592.935931	45.384487
3501.262840	568591.559918	45.389492
3501.325304	568595.264676	45.394497
3501.465957	568590.022187	45.399501
3501.606921	568559.731416	45.404506
3501.146749	568552.273777	45.409511
3501.509011	568543.482836	45.414516
3501.727138	568541.189835	45.419521
3501.656247	568526.342561	45.424525
3501.810421	568507.143131	45.429530
3501.328104	568495.120976	45.434535
3501.358757	568478.701653	45.439540
3501.354625	568465.550571	45.444545
3501.565390	568465.768572	45.449549
3501.688000	568455.609504	45.454554
3501.787638	568435.565124	45.459559
3501.779690	568423.067157	45.464564
3501.441071	568408.914153	45.469569
3501.668928	568386.289567	45.474573
3501.790652	568365.689439	45.479578
3501.627851	568362.803382	45.484583
3502.010213	568333.879817	45.489588
3502.014657	568334.983439	45.494593
3501.956844	568307.935745	45.499597
3502.013149	568290.809372	45.504602
3501.541929	568270.552758	45.509607
3501.606050	568245.644377	45.514612
3501.604779	568245.092358	45.519617
3501.439571	568235.680866	45.524621
3501.816815	568212.631000	45.529626
3501.240926	568203.685271	45.534631
3501.380470	568198.041190	45.539636
3501.504465	568194.708668	45.544641
3501.633130	568163.716000	45.549645
3501.590217	568156.594463	45.554650
3501.676409	568157.333931	45.559655
3501.711812	568129.668862	45.564660
3501.976731	568126.264092	45.569665
3501.626710	568104.381877	45.574669
3501.814523	568085.076087	45.579674
3501.590392	568081.848154	45.584679
3501.687226	568054.323898	45.589684
3501.599099	568042.540840	45.594689
3501.701321	568035.647535	45.599693
3501.744242	568021.735603	45.604698
3501.144982	568006.317667	45.609703
3501.592266	567991.489097	45.614708
3501.524545	567989.491671	45.619713
3501.355664	567961.255741	45.624717
3501.804797	567948.836403	45.629722
3501.408686	567944.982722	45.634727
3501.431807	567929.668186	45.639732
3501.343187	567905.786942	45.644737
3501.532172	567897.223399	45.649741
3501.634947	567903.181069	45.654746
3501.578632	567886.222301	45.659751
3501.423224	567865.062204	45.664756
3501.876801	567857.712267	45.669761
3501.579002	567850.027987	45.674765
3502.004569	567822.803189	45.679770
3501.691252	567822.601131	45.684775
3501.674839	567789.521733	45.689780
3501.535777	567784.523408	45.694785
3501.630271	567763.424459	45.699789
3501.654758	567760.207769	45.704794
3501.683842	567743.436242	45.709799
3501.388846	567729.275581	45.714804
3501.388679	567726.514540	45.719809
3501.669309	567710.004844	45.724813
3501.686254	567686.106643	45.729818
3501.664298	567680.688360	45.734823
3501.405579	567649.805072	45.739828
3501.148065	567584.232566	45.744833
3501.472949	567490.556203	45.749837
3501.528551	567322.170202	45.754842
3501.161963	567117.952530	45.759847
3500.659028	566861.038175	45.764852
3499.859758	566562.594286	45.769857
3499.817925	566227.925490	45.774861
3499.490367	565833.995330	45.779866
3499.078538	565392.264538	45.784871
3498.456357	564905.408670	45.789876
3497.545926	564389.653719	45.794881
3496.532908	563808.659677	45.799885
3495.906759	563200.658328	45.804890
3494.799231	562548.755723	45.809895
3494.279707	561847.905515	45.814900
3492.759106	561110.603362	45.819905
3491.803531	560331.926063	45.824909
3490.890195	559509.787164	45.829914
3488.880297	558653.800806	45.834919
3488.111056	557749.375585	45.839924
3486.697748	556825.536751	45.844929
3485.256289	555840.274194	45.849933
3483.919275	554831.947553	45.854938
3481.752755	553781.749343	45.859943
3480.268625	552699.636216	45.864948
3478.555986	551577.397721	45.869953
3476.833318	550428.160686	45.874957
3474.779374	549240.253175	45.879962
3472.718462	548024.474935	45.884967
3470.901437	546787.618221	45.889972
3468.704919	545508.248894	45.894977
3466.550130	544202.183026	45.899981
3464.709660	542872.841207	45.904986
3462.216988	541504.821960	45.909991
3459.935446	540119.312143	45.914996
3457.452061	538705.854154	45.920001
3455.124885	537261.766409	45.925005
3452.948052	535801.385033	45.930010
3450.111891	534313.203683	45.935015
3447.529003	532813.936251	45.940020
3444.734766	531288.345962	45.945025
3442.473421	529743.559429	45.950029
3440.059005	528171.871950	45.955034
3436.778601	526583.812594	45.960039
3433.921448	524980.434287	45.965044
3431.137639	523363.903293	45.970049
3427.854503	521725.034351	45.975053
3425.311600	520074.259538	45.980058
3421.980933	518413.880976	45.985063
3418.971179	516734.398034	45.990068
3415.929797	515049.420743	45.995073
3412.486671	513337.124976	46.000077
3409.628336	511627.249047	46.005082
3406.168513	509919.879822	46.010087
3403.340397	508173.368166	46.015092
3400.167058	506432.142260	46.020097
3396.786008	504673.179359	46.025101
3393.508640	502904.044348	46.030106
3389.863295	501131.721859	46.035111
3386.844016	499346.266120	46.040116
3383.312984	497554.009494	46.045121
3379.417940	495749.829444	46.050125
3376.445851	493940.186051	46.055130
3372.764925	492148.358345	46.060135
3369.498098	490324.387766	46.065140
3365.937679	488514.182070	46.070145
3362.349658	486693.107808	46.075149
3358.832943	484862.965798	46.080154
3355.127585	483038.092778	46.085159
3351.417256	481196.332283	46.090164
3348.182645	479367.318709	46.095169
3344.694312	477528.176664	46.100173
3340.812445	475684.890466	46.105178
3336.875110	473838.570124	46.110183
3333.581717	472003.161737	46.115188
3329.721618	470160.505698	46.120193
3326.243481	468307.974994	46.125197
3323.081587	466461.053892	46.130202
3318.754304	464599.948059	46.135207
3315.000255	462744.667221	46.140212
3311.370318	460901.912584	46.145217
3307.292294	459057.966589	46.150221
3303.824588	457199.609794	46.155226
3299.979797	455347.084575	46.160231
3296.281544	453497.073372	46.165236
3292.591014	451662.305319	46.170241
3288.392134	449818.011713	46.175245
3285.075064	447965.998971	46.180250
3281.203643	446128.516309	46.185255
3277.312734	444277.938969	46.190260
3273.641806	442441.523854	46.195265
3269.854162	440597.398795	46.200269
3265.936289	438760.406591	46.205274
3262.039500	436915.431178	46.210279
3258.596044	435082.213451	46.215284
3254.414546	433266.062093	46.220289
3250.749797	431427.161453	46.225293
3247.184606	429599.272246	46.230298
3243.069095	427772.871187	46.235303
3239.191981	425954.223387	46.240308
3235.345661	424138.650709	46.245313
3231.528869	422329.552303	46.250317
3228.216511	420514.334285	46.255322
3224.160345	418700.949510	46.260327
3220.059819	416892.890901	46.265332
3215.978275	415092.382802	46.270337
3212.283648	413286.438205	46.275341
3208.865579	411490.189498	46.280346
3204.695840	409690.764870	46.285351
3200.570476	407896.005092	46.290356
3197.113898	406121.593351	46.295361
3193.016668	404339.784181	46.300365
3189.297334	402562.646747	46.305370
3185.464707	400788.484280	46.310375
3181.865384	399013.793718	46.315380
3177.971271	397248.048310	46.320385
3174.111558	395473.790280	46.325389
3170.120038	393706.476442	46.330394
3165.942762	391959.113896	46.335399
3162.421939	390192.078945	46.340404
3158.401318	388447.893277	46.345409
3154.674041	386710.165534	46.350413
3150.839182	384955.323519	46.355418
3146.795446	383235.356608	46.360423
3143.049912	381507.737015	46.365428
3139.373940	379785.705418	46.370433
3135.457602	378061.414454	46.375437
3131.641603	376335.141862	46.380442
3127.824569	374618.969133	46.385447
3124.176031	372905.506655	46.390452
3120.490133	371193.823092	46.395457
3116.879962	369491.040910	46.400461
3113.033398	367800.743161	46.405466
3109.077120	366114.198822	46.410471
3104.847598	364395.507512	46.415476
3101.230315	362719.028832	46.420481
3097.300244	361020.726335	46.425485
3093.913148	359345.546315	46.430490
3090.048876	357660.513020	46.435495
3086.132613	355985.663370	46.440500
3082.396694	354310.644521	46.445505
3078.666127	352654.701319	46.450509
3074.908035	350986.983469	46.455514
3070.899530	349328.573771	46.460519
3067.432618	347666.309285	46.465524
3063.444728	346014.060043	46.470529
3059.571359	344364.457773	46.475533
3055.967292	342720.327490	46.480538
3052.119630	341076.259009	46.485543
3048.607459	339441.876534	46.490548
3044.555019	337803.994356	46.495553
3040.839116	336169.342256	46.500557
3037.383422	334533.915468	46.505562
3033.098892	332916.196974	46.510567
3029.436399	331286.663266	46.515572
3025.212542	329673.324926	46.520577
3021.734707	328055.936925	46.525581
3018.048060	326445.688848	46.530586
3014.432959	324856.962166	46.535591
3010.560448	323249.058399	46.540596
3006.958551	321638.633341	46.545601
3003.199547	320052.035223	46.550605
2999.929389	318456.168450	46.555610
2995.891589	316861.203112	46.560615
2992.141250	315278.704889	46.565620
2988.175561	313693.895026	46.570625
2984.602856	312110.546853	46.575629
2980.989126	310524.174471	46.580634
2977.320313	308957.683255	46.585639
2973.147401	307374.933768	46.590644
2969.869767	305804.056582	46.595649
2965.828228	304242.513783	46.600653
2962.068093	302672.404784	46.605658
2958.450480	301121.849524	46.610663
2954.721145	299566.176655	46.615668
2951.340669	298007.859895	46.620673
2947.275605	296459.559114	46.625677
2943.827968	294908.065469	46.630682
2939.934906	293367.494959	46.635687
2936.356613	291820.242701	46.640692
2932.168618	290281.192619	46.645697
2928.789079	288742.029276	46.650701
2925.185210	287205.588072	46.655706
2921.596766	285690.645815	46.660711
2918.029718	284153.950353	46.665716
2914.172634	282627.958867	46.670721
2910.347611	281109.338299	46.675725
2906.742297	279571.455084	46.680730
2902.708666	278043.511464	46.685735
2899.216975	276535.235990	46.690740
2895.622494	275019.691534	46.695745
2891.927995	273510.474707	46.700749
2888.155639	271999.791784	46.705754
2884.578757	270500.001110	46.710759
2881.106245	268983.770953	46.715764
2877.049048	267477.360129	46.720769
2873.565575	265992.964228	46.725773
2870.083830	264489.626128	46.730778
2866.416372	263003.203857	46.735783
2862.582298	261495.523973	46.740788
2859.226576	260006.644348	46.745793
2855.279434	258516.845187	46.750797
2851.703348	257027.453763	46.755802
2847.988940	255553.244559	46.760807
2843.925609	254065.194568	46.765812
2840.410798	252586.771453	46.770817
2836.675876	251118.503982	46.775821
2833.114461	249638.022391	46.780826
2829.459383	248172.950143	46.785831
2825.554743	246715.265013	46.790836
2822.116747	245248.327316	46.795841
2818.739689	243782.209988	46.800845
2815.415563	242322.492593	46.805850
2811.659387	240853.639797	46.810855
2807.777863	239397.558037	46.815860
2804.350088	237924.028403	46.820865
2800.130632	236475.931690	46.825869
2796.808001	235033.164725	46.830874
2792.819593	233585.657807	46.835879
2789.275669	232132.219235	46.840884
2785.851066	230682.731587	46.845889
2781.775363	229244.421979	46.850893
2778.048853	227814.333159	46.855898
2774.528900	226379.677243	46.860903
2771.067697	224939.764927	46.865908
2767.375114	223514.457236	46.870913
2763.659806	222085.257184	46.875917
2759.784696	220659.598410	46.880922
2756.048110	219242.044834	46.885927
2752.435476	217812.198803	46.890932
2748.819649	216394.123569	46.895937
2745.242190	214988.093386	46.900941
2741.870466	213579.922075	46.905946
2737.947407	212169.601408	46.910951
2734.282758	210755.171728	46.915956
2730.912282	209349.336863	46.920961
2727.230092	207945.137446	46.925965
2723.861538	206536.644156	46.930970
2720.188704	205130.576027	46.935975
2716.679834	203732.030385	46.940980
2713.025157	202322.999780	46.945985
2709.142793	200930.900675	46.950989
2705.605307	199524.956028	46.955994
2701.844779	198139.686779	46.960999
2698.337176	196744.662468	46.966004
2695.019928	195343.408169	46.971009
2690.948248	193960.010565	46.976013
2687.490913	192570.903584	46.981018
2683.764367	191192.371355	46.986023
2679.944536	189810.406277	46.991028
2676.630265	188422.241647	46.996033
2672.929163	187048.924293	47.001037
2669.293730	185673.831790	47.006042
2665.489706	184295.702830	47.011047
2662.063176	182920.818638	47.016052
2658.593800	181541.479205	47.021057
2654.275811	180178.512606	47.026061
2651.006908	178807.534535	47.031066
2647.535120	177452.625116	47.036071
2644.042513	176087.415758	47.041076
2640.489083	174728.539956	47.046081
2636.762343	173360.484583	47.051085
2632.975669	171992.666026	47.056090
2629.462321	170646.164396	47.061095
2625.844283	169287.826590	47.066100
2622.167484	167929.981500	47.071105
2618.730077	166579.673229	47.076109
2615.148014	165234.098007	47.081114
2611.321950	163876.673507	47.086119
2607.828775	162528.147233	47.091124
2604.002765	161186.599591	47.096129
2600.609667	159841.372287	47.101133
2596.661972	158497.037088	47.106138
2593.010016	157159.468826	47.111143
2589.473708	155833.812075	47.116148
2585.986655	154493.134479	47.121153
2582.167517	153166.691770	47.126157
2578.630284	151828.629783	47.131162
2575.161638	150513.686651	47.136167
2571.498915	149178.711915	47.141172
2567.923758	147861.012068	47.146177
2564.062486	146546.392961	47.151181
2560.826913	145179.055081	47.156186
2557.300984	143814.598611	47.161191
2553.719227	142499.912883	47.166196
2549.841443	141185.181266	47.171201
2546.160578	139867.299104	47.176205
2542.777076	138557.956508	47.181210
2538.594779	137254.920235	47.186215
2535.119745	135935.907309	47.191220
2531.438674	134645.601347	47.196225
2527.580014	133340.577893	47.201229
2524.288241	132039.918326	47.206234
2520.843556	130753.695638	47.211239
2516.957280	129459.744679	47.216244
2513.423660	128169.085046	47.221249
2509.807907	126885.817044	47.226253
2506.526387	125594.485312	47.231258
2502.749946	124313.217744	47.236263
2498.872535	123022.824030	47.241268
2495.249569	121743.382333	47.246273
2491.636853	120467.465172	47.251277
2488.206769	119185.597012	47.256282
2484.484843	117916.330381	47.261287
2480.887734	116641.364383	47.266292
2477.416021	115372.970690	47.271297
2473.770399	114112.518345	47.276301
2470.054225	112832.870088	47.281306
2466.334342	111581.633421	47.286311
2462.523614	110314.066360	47.291316
2459.035119	109060.110386	47.296321
2455.015306	107800.815769	47.301325
2451.263638	106552.712013	47.306330
2448.055068	105317.471508	47.311335
2444.472002	104069.877097	47.316340
2441.113106	102817.717919	47.321345
2436.960377	101581.033748	47.326349
2433.950339	100351.729035	47.331354
2430.235185	99115.730433	47.336359
2426.290136	97866.635647	47.341364
2422.811647	96642.425870	47.346369
2419.213586	95415.143219	47.351373
2415.555814	94191.247403	47.356378
2411.592551	92962.402845	47.361383
2408.098359	91738.171979	47.366388
2404.436277	90525.147233	47.371393
2400.376627	89311.445664	47.376397
2397.050156	88092.596558	47.381402
2393.330862	86890.464033	47.386407
2389.930608	85687.695565	47.391412
2386.402049	84481.147619	47.396417
2382.684236	83295.195214	47.401421
2378.976485	82093.196176	47.406426
2375.304569	80889.489536	47.411431
2371.562973	79697.441734	47.416436
2367.898828	78514.082068	47.421441
2363.984806	77341.709024	47.426445
2360.826226	76149.265538	47.431450
2356.964798	74980.846204	47.436455
2353.609416	73801.743943	47.441460
2349.913406	72633.972025	47.446465
2346.084737	71469.040196	47.451469
2342.404485	70297.838787	47.456474
2338.938823	69134.489911	47.461479
2335.296770	67976.933850	47.466484
2331.442538	66806.189872	47.471489
2327.760725	65653.524437	47.476493
2323.979450	64499.739899	47.481498
2320.611595	63356.098340	47.486503
2316.639465	62212.552723	47.491508
2313.255883	61085.512248	47.496513
2309.611945	59950.669535	47.501517
2305.913730	58808.850459	47.506522
2301.917604	57681.522775	47.511527
2298.464740	56548.953319	47.516532
2295.224352	55428.776285	47.521537
2291.163361	54315.156376	47.526541
2287.810797	53179.596888	47.531546
2284.069937	52062.556431	47.536551
2280.219669	50965.638423	47.541556
2277.092721	49847.656451	47.546561
2273.073538	48744.475991	47.551565
2269.726588	47647.414790	47.556570
2265.695211	46558.155958	47.561575
2261.937330	45467.086518	47.566580
2258.287057	44369.349872	47.571585
2254.256227	43287.358201	47.576589
2250.735630	42195.726185	47.581594
2247.048317	41130.558224	47.586599
2243.287152	40060.786812	47.591604
2239.747376	38995.433216	47.596609
2235.977930	37942.562251	47.601613
2232.849446	36872.728341	47.606618
2228.750088	35812.969821	47.611623
2224.999265	34764.942746	47.616628
2221.302855	33724.337046	47.621633
2217.596361	32684.145484	47.626637
2214.045300	31643.790982	47.631642
2210.362745	30614.086475	47.636647
2206.162552	29597.740104	47.641652
2202.346846	28569.647330	47.646657
2198.283064	27539.857836	47.651661
2194.435326	26531.155050	47.656666
2190.836227	25535.053268	47.661671
2186.635828	24553.445217	47.666676
2183.070295	23567.198805	47.671681
2179.011074	22601.110075	47.676685
2175.417651	21625.074865	47.681690
2171.541994	20670.675739	47.686695
2167.341414	19732.392984	47.691700
2163.419622	18789.234269	47.696705
2159.454201	17865.971268	47.701709
2155.152125	16959.822521	47.706714
2149.761312	16082.160571	47.711719
2144.556862	15229.106040	47.716724
2139.068435	14400.108814	47.721729
2134.342164	13596.123060	47.726733
2129.357680	12823.517093	47.731738
2124.029999	12082.170710	47.736743
2119.027378	11376.705452	47.741748
2114.212939	10681.275436	47.746753
2109.312476	10032.183750	47.751757
2104.607971	9403.944104	47.756762
2099.107354	8832.867278	47.761767
2093.272770	8287.717096	47.766772
2088.174510	7770.428688	47.771777
2083.049838	7285.031122	47.776781
2078.090521	6834.910105	47.781786
2073.160700	6424.730446	47.786791
2068.308950	6029.606110	47.791796
2063.798909	5658.884826	47.796801
2059.329057	5320.077908	47.801805
2055.378897	5003.630355	47.806810
2051.290207	4699.564662	47.811815
2047.757020	4397.654480	47.816820
2044.443421	4126.641843	47.821825
2040.593253	3869.580795	47.826829
2036.928544	3607.393300	47.831834
2033.911970	3363.629374	47.836839
2029.877474	3116.933270	47.841844
2027.163298	2878.685163	47.846849
2023.617403	2641.579739	47.851853
2020.436246	2405.483542	47.856858
2016.905917	2181.187368	47.861863
2013.372735	1956.669784	47.866868
2010.510237	1731.705174	47.871873
2007.266138	1513.324237	47.876877
2004.180484	1291.393272	47.881882
2000.673213	1074.346623	47.886887
1997.220965	864.621717	47.891892
1993.679811	636.853546	47.896897
1989.949785	431.350397	47.901901
1986.230934	232.621657	47.906906
1979.448528	114.795536	47.911911
1968.104945	146.528762	47.916916
1960.312958	152.316559	47.921921
1955.282194	147.620809	47.926925
1952.725755	138.785587	47.931930
1951.111665	139.363994	47.936935
1948.695182	140.510893	47.941940
1946.675556	141.244509	47.946945
1943.875205	141.217585	47.951949
1941.138466	143.360584	47.956954
1937.658195	142.231472	47.961959
1934.142674	147.277340	47.966964
1931.129245	138.656007	47.971969
1927.585368	139.653452	47.976973
1924.349269	144.519554	47.981978
1920.876363	149.546102	47.986983
1917.460794	144.670393	47.991988
1914.505501	140.481980	47.996993
1911.400462	132.722898	48.001997
1907.573868	138.083210	48.007002
1903.835643	133.330767	48.012007
1900.461597	134.181420	48.017012
1897.669340	138.231411	48.022017
1894.151574	142.625892	48.027021
1890.520893	140.767343	48.032026
1887.707256	140.280595	48.037031
1884.213687	140.719676	48.042036
1880.507542	135.775556	48.047041
1876.646274	142.001864	48.052045
1873.713502	132.842738	48.057050
1869.944916	143.765479	48.062055
1866.425802	136.226235	48.067060
1863.549235	134.705279	48.072065
1860.316674	130.588749	48.077069
1856.935744	133.215397	48.082074
1853.519493	131.797880	48.087079
1849.645955	136.330307	48.092084
1846.784792	139.483076	48.097089
1843.062648	146.684229	48.102093
1839.208341	140.377555	48.107098
1835.940306	141.825420	48.112103
1832.424995	147.716026	48.117108
1829.200632	135.087536	48.122113
1825.398930	138.203993	48.127117
1822.576023	142.021511	48.132122
1818.375856	130.966290	48.137127
1815.239477	134.291851	48.142132
1812.100180	129.717808	48.147137
1808.392046	136.938922	48.152141
1804.715659	137.419294	48.157146
1801.479377	139.982194	48.162151
1797.466680	138.211936	48.167156
1794.454510	134.057774	48.172161
1790.940629	135.465030	48.177165
1787.713886	130.616772	48.182170
1784.034149	132.910544	48.187175
1780.443502	135.645966	48.192180
1777.327609	128.100609	48.197185
1773.747035	132.096820	48.202189
1770.210185	138.224934	48.207194
1766.743040	134.274863	48.212199
1763.262665	134.430339	48.217204
1759.797122	138.313640	48.222209
1756.065402	143.149778	48.227213
1752.542306	140.521453	48.232218
1749.388088	132.254423	48.237223
1745.778193	134.929592	48.242228
1742.323951	130.623164	48.247233
1738.825964	130.094856	48.252237
1735.417560	134.586166	48.257242
1731.843561	135.952228	48.262247
1728.517084	135.821034	48.267252
1725.382455	134.906828	48.272257
1721.375749	136.198240	48.277261
1717.862537	127.943113	48.282266
1714.658789	129.498015	48.287271
1710.974958	129.182302	48.292276
1707.378697	129.691298	48.297281
1703.915029	136.877348	48.302285
1700.562477	128.448385	48.307290
1697.544086	129.186492	48.312295
1693.743956	138.304509	48.317300
1690.206428	128.215020	48.322305
1686.514563	125.831438	48.327309
1682.877771	132.225157	48.332314
1679.647132	129.899110	48.337319
1676.253597	134.679181	48.342324
1672.683118	124.139269	48.347329
1669.008976	133.585594	48.352333
1665.654904	124.147627	48.357338
1662.484828	133.404331	48.362343
1658.870221	137.738106	48.367348
1655.233573	125.813313	48.372353
1651.815193	125.800933	48.377357
1648.108803	119.721140	48.382362
1644.531861	116.604566	48.387367
1641.267535	129.299271	48.392372
1638.008737	127.585097	48.397377
1634.171108	131.833559	48.402381
1630.968726	131.524784	48.407386
1627.385521	130.301157	48.412391
1623.895480	133.751725	48.417396
1620.483267	130.217063	48.422401
1616.972308	136.008967	48.427405
1613.057985	137.244832	48.432410
1609.841724	128.212432	48.437415
1606.359857	131.022636	48.442420
1602.813631	126.651562	48.447425
1599.288964	141.892771	48.452429
1595.553929	134.542458	48.457434
1592.114463	130.755803	48.462439
1588.751251	134.332068	48.467444
1585.498549	128.564111	48.472449
1582.398238	131.577200	48.477453
1578.477009	126.353650	48.482458
1575.427795	128.412763	48.487463
1571.367009	135.322139	48.492468
1568.045793	135.022491	48.497473
1564.206443	125.894640	48.502477
1560.574908	127.383662	48.507482
1557.386787	129.768248	48.512487
1554.106610	133.752313	48.517492
1550.606760	129.086093	48.522497
1547.050593	130.117226	48.527501
1543.236152	132.391034	48.532506
1539.728217	124.410408	48.537511
1536.014244	135.378471	48.542516
1532.775774	123.970391	48.547521
1529.426652	128.503102	48.552525
1526.018208	136.537950	48.557530
1523.054996	132.173732	48.562535
1518.899182	130.501919	48.567540
1515.571538	123.176469	48.572545
1512.196069	126.580664	48.577549
1508.300081	136.571131	48.582554
1505.136809	132.314163	48.587559
1501.339142	131.086184	48.592564
1497.862261	126.305656	48.597569
1494.225055	124.653924	48.602573
1491.264209	127.698994	48.607578
1487.755497	128.662607	48.612583
1483.831833	119.411949	48.617588
1480.338926	122.682672	48.622593
1476.776638	131.918549	48.627597
1473.323715	127.526593	48.632602
1470.453021	120.028397	48.637607
1466.259089	129.410600	48.642612
1462.967940	123.734131	48.647617
1459.535351	122.721112	48.652621
1456.096120	122.164723	48.657626
1452.845209	123.069013	48.662631
1449.281967	124.382865	48.667636
1445.655529	118.455160	48.672641
1441.582595	123.300511	48.677645
1438.324474	127.436184	48.682650
1434.799620	116.765852	48.687655
1431.323710	121.799334	48.692660
1428.174159	124.842320	48.697665
1424.508930	126.491690	48.702669
1420.871306	118.363735	48.707674
1417.809852	122.845121	48.712679
1413.901039	129.290992	48.717684
1410.287129	115.527751	48.722689
1407.113312	122.453368	48.727693
1403.409307	128.645717	48.732698
1400.148300	123.809290	48.737703
1396.203685	119.712634	48.742708
1393.274119	120.838729	48.747713
1389.309727	123.778316	48.752717
1386.120891	119.553869	48.757722
1382.961688	116.982621	48.762727
1378.901505	125.571947	48.767732
1375.756780	119.284124	48.772737
1371.855091	118.268635	48.777741
1368.469895	122.582408	48.782746
1365.305355	122.176045	48.787751
1361.311375	123.272610	48.792756
1357.899840	112.040403	48.797761
1354.681452	122.187437	48.802765
1351.174997	120.312808	48.807770
1347.408142	120.544909	48.812775
1343.533216	119.272137	48.817780
1340.339596	110.093939	48.822785
1336.835933	116.498557	48.827789
1333.116187	121.798033	48.832794
1330.235415	117.278606	48.837799
1326.560286	116.809811	48.842804
1322.930559	112.344352	48.847809
1319.698484	118.630530	48.852813
1315.932334	127.673732	48.857818
1312.562830	118.418667	48.862823
1308.647005	123.521052	48.867828
1305.117670	119.410048	48.872833
1301.917506	123.666403	48.877837
1298.541208	115.529233	48.882842
1295.400683	114.540156	48.887847
1291.420306	121.791383	48.892852
1288.174469	117.800525	48.897857
1284.860453	124.814562	48.902861
1280.941340	122.473039	48.907866
1277.522004	115.317067	48.912871
1273.907475	127.908480	48.917876
1270.251378	122.023456	48.922881
1267.017954	114.578953	48.927885
1263.172441	117.471502	48.932890
1260.393114	120.260424	48.937895
1256.354959	119.427698	48.942900
1252.926190	115.588879	48.947905
1249.438484	114.647840	48.952909
1246.090053	126.235807	48.957914
1242.774996	117.307612	48.962919
1239.001132	123.080671	48.967924
1236.069931	116.060274	48.972929
1231.775277	120.162116	48.977933
1228.368903	124.086936	48.982938
1224.904950	118.292077	48.987943
1221.576494	123.065256	48.992948
1218.033358	127.179171	48.997953
1214.565046	114.079779	49.002957
1210.907239	117.638998	49.007962
1207.304577	112.748564	49.012967
1203.841456	115.926126	49.017972
1200.411649	118.528989	49.022977
1196.878400	118.692938	49.027981
1193.199803	122.239600	49.032986
1190.086074	98.938410	49.037991
1186.110768	117.420363	49.042996
1182.664942	110.002820	49.048001
1179.584885	123.102212	49.053005
1176.220207	118.645938	49.058010
1172.694624	111.649016	49.063015
1169.197127	113.237415	49.068020
1165.689183	113.435379	49.073025
1162.043749	111.683822	49.078029
1157.754999	103.243469	49.083034
1154.557685	104.734257	49.088039
1150.805828	119.334062	49.093044
1147.917005	106.811546	49.098049
1144.703281	110.845436	49.103053
1141.023236	115.743284	49.108058
1138.052386	105.135059	49.113063
1134.243678	121.607247	49.118068
1130.302942	112.780221	49.123073
1126.708434	114.709694	49.128077
1123.162536	128.536939	49.133082
1120.021746	110.264124	49.138087
1116.296746	120.680357	49.143092
1113.114067	111.877029	49.148097
1109.368248	116.804168	49.153101
1105.744777	114.517676	49.158106
1102.261693	105.539922	49.163111
1099.038566	111.745663	49.168116
1095.861787	102.027087	49.173121
1092.059554	109.297944	49.178125
1088.331434	109.327924	49.183130
1084.937940	105.255856	49.188135
1081.131593	119.013148	49.193140
1077.517392	112.555330	49.198145
1074.113168	115.236489	49.203149
1070.721092	113.546542	49.208154
1067.575796	121.432742	49.213159
1063.834560	121.471112	49.218164
1060.458668	112.739185	49.223169
1057.124857	111.255260	49.228173
1053.563252	113.730108	49.233178
1049.939696	106.305648	49.238183
1046.045130	109.642560	49.243188
1042.865302	120.188597	49.248193
1039.059187	104.930689	49.253197
1035.259658	113.678636	49.258202
1032.408349	114.280047	49.263207
1029.022290	117.898025	49.268212
1025.356523	109.236810	49.273217
1022.242467	105.149490	49.278221
1018.358149	121.788571	49.283226
1015.065504	115.580994	49.288231
1011.053278	114.054606	49.293236
1007.981103	114.048355	49.298241
1004.680640	118.222422	49.303245
1000.950377	115.883088	49.308250
997.461634	108.519801	49.313255
993.907154	117.805205	49.318260
990.242920	105.211171	49.323265
987.038902	113.384996	49.328269
983.472186	124.697152	49.333274
979.893301	110.106056	49.338279
975.894594	122.124937	49.343284
972.727273	112.465037	49.348289
969.075269	118.804408	49.353293
965.487229	104.961412	49.358298
962.497555	107.504932	49.363303
958.911735	113.131579	49.368308
955.431147	105.991663	49.373313
951.618384	112.527054	49.378317
948.256023	112.370104	49.383322
944.629429	104.936675	49.388327
941.211633	115.171976	49.393332
937.701142	115.085681	49.398337
934.026406	113.079371	49.403341
930.491547	112.920962	49.408346
927.272473	115.247308	49.413351
923.751974	118.022655	49.418356
921.010681	108.770640	49.423361
917.238794	107.595808	49.428365
913.179453	119.880469	49.433370
909.788877	109.024839	49.438375
905.877008	113.263031	49.443380
902.499161	110.333877	49.448385
898.948568	101.879320	49.453389
895.410086	114.942977	49.458394
892.323571	109.737735	49.463399
888.716991	104.759464	49.468404
885.547461	112.614700	49.473409
882.075753	106.625045	49.478413
877.981823	109.490196	49.483418
875.041856	105.593971	49.488423
871.390038	111.262620	49.493428
867.594071	103.763997	49.498433
864.068648	107.739210	49.503437
860.618317	113.955286	49.508442
857.315815	112.017273	49.513447
853.405364	114.619584	49.518452
850.195101	113.859878	49.523457
846.755221	108.687840	49.528461
843.082182	116.536510	49.533466
839.868012	104.783249	49.538471
836.072675	111.638656	49.543476
832.567263	114.563534	49.548481
829.422313	112.467980	49.553485
825.852650	111.859475	49.558490
822.617284	110.793659	49.563495
818.393040	110.480650	49.568500
814.924933	102.433998	49.573505
811.572341	113.589277	49.578509
808.296737	117.980978	49.583514
804.876776	103.026565	49.588519
801.176937	108.174403	49.593524
797.766209	102.526417	49.598529
794.403908	108.304780	49.603533
790.365598	109.335751	49.608538
787.235320	104.823946	49.613543
783.285135	111.596051	49.618548
780.064564	111.356846	49.623553
777.009134	107.557831	49.628557
772.902419	108.928555	49.633562
769.751478	118.770937	49.638567
766.214723	123.080159	49.643572
762.286952	110.157341	49.648577
759.377512	105.610963	49.653581
755.529131	110.478355	49.658586
752.153138	113.683554	49.663591
748.274098	109.418731	49.668596
744.998859	113.664859	49.673601
741.770224	105.432040	49.678605
738.248822	112.712824	49.683610
734.723675	108.905123	49.688615
730.983428	117.517335	49.693620
727.883185	116.724625	49.698625
724.547585	107.584736	49.703629
720.522772	111.771083	49.708634
717.084827	104.007655	49.713639
713.578899	111.956747	49.718644
709.940945	114.320286	49.723649
706.381106	100.732439	49.728653
702.773886	111.320174	49.733658
699.632116	105.911686	49.738663
696.059171	111.169405	49.743668
692.519158	109.369889	49.748673
689.146798	105.095350	49.753677
685.465093	112.470859	49.758682
682.205270	113.756453	49.763687
678.520533	114.346119	49.768692
675.056135	109.374146	49.773697
671.541259	106.621567	49.778701
667.999119	112.105428	49.783706
664.662825	101.007294	49.788711
661.038788	99.904328	49.793716
657.407700	96.489743	49.798721
654.045960	106.127876	49.803725
650.128498	113.369475	49.808730
647.200458	103.343211	49.813735
643.688204	109.233691	49.818740
640.162285	107.770514	49.823745
636.944653	110.615589	49.828749
632.794263	103.738901	49.833754
629.503208	100.903831	49.838759
626.021036	106.776950	49.843764
622.358045	114.532368	49.848769
619.201153	100.678977	49.853773
615.439681	113.793449	49.858778
612.377709	99.814464	49.863783
608.429034	106.257362	49.868788
604.633962	106.418244	49.873793
601.378091	105.051996	49.878797
598.070697	111.457743	49.883802
594.632951	103.273555	49.888807
590.730752	111.566323	49.893812
587.031944	107.630856	49.898817
583.769182	112.896983	49.903821
580.013421	110.141037	49.908826
577.117542	106.190555	49.913831
573.675078	107.963539	49.918836
569.925965	111.413899	49.923841
566.490231	110.287806	49.928845
562.893543	115.666351	49.933850
559.313489	111.319987	49.938855
555.981065	110.563700	49.943860
552.836308	105.937191	49.948865
549.195467	103.473312	49.953869
545.211074	104.211204	49.958874
541.609761	114.035593	49.963879
538.331392	111.432688	49.968884
535.108919	112.475199	49.973889
531.853070	107.141591	49.978893
527.878401	113.401930	49.983898
524.566653	105.005049	49.988903
520.512684	109.319430	49.993908
517.142083	112.150537	49.998913
513.743732	113.480032	50.003917
510.380437	112.241375	50.008922
506.831171	104.710613	50.013927
503.508447	111.248504	50.018932
500.281803	109.966301	50.023937
496.305734	98.835573	50.028941
492.272345	105.671437	50.033946
489.482528	98.955052	50.038951
485.986920	91.146980	50.043956
482.049328	101.976348	50.048961
478.984036	111.906627	50.053965
475.524422	107.841995	50.058970
472.166830	104.454253	50.063975
468.677929	100.596695	50.068980
464.753524	98.629687	50.073985
461.340037	98.990292	50.078989
457.394198	106.268040	50.083994
454.258555	100.963095	50.088999
450.865151	91.364151	50.094004
447.514848	100.649370	50.099009
444.007866	97.557126	50.104013
440.422077	100.874383	50.109018
436.899632	91.400063	50.114023
433.063756	99.106687	50.119028
429.518682	96.520292	50.124033
426.218752	93.148850	50.129037
422.766460	104.857686	50.134042
419.209727	99.349791	50.139047
416.011086	100.005793	50.144052
412.360178	97.875747	50.149057
409.031524	108.106723	50.154061
405.260061	106.979496	50.159066
401.942733	102.740748	50.164071
398.242493	99.365579	50.169076
394.573323	106.096975	50.174081
390.654062	97.036008	50.179085
387.378939	96.656791	50.184090
384.579932	88.575137	50.189095
381.006644	109.417775	50.194100
377.230622	102.612296	50.199105
374.128831	103.212013	50.204109
370.397115	100.759282	50.209114
367.015937	95.378937	50.214119
363.368960	101.600662	50.219124
359.673889	99.651563	50.224129
356.201044	96.247122	50.229133
352.516889	94.837323	50.234138
348.926717	91.622108	50.239143
345.607943	92.841122	50.244148
342.171716	98.014270	50.249153
338.844494	99.411781	50.254157
335.297041	92.143413	50.259162
332.073603	103.531687	50.264167
328.154632	99.630824	50.269172
324.873548	94.829608	50.274177
321.288225	100.956268	50.279181
317.584643	101.327567	50.284186
314.243712	100.094974	50.289191
310.646302	97.754110	50.294196
306.892685	100.357384	50.299201
303.842866	99.000100	50.304205
300.214372	99.153999	50.309210
296.958378	98.955318	50.314215
292.900132	99.831440	50.319220
289.595219	99.051962	50.324225
286.428152	98.519813	50.329229
282.570011	101.133143	50.334234
279.710288	97.398570	50.339239
275.675763	93.591765	50.344244
271.747587	96.440698	50.349249
268.647748	97.577987	50.354253
265.148086	102.596584	50.359258
261.442293	99.668438	50.364263
258.593265	96.400435	50.369268
254.609491	107.559825	50.374273
251.263401	105.306166	50.379277
246.992652	102.292520	50.384282
243.849275	96.087196	50.389287
240.451706	95.951843	50.394292
237.028418	103.201599	50.399297
233.860897	92.431577	50.404301
230.120640	101.094574	50.409306
226.752790	92.820515	50.414311
223.251649	91.590910	50.419316
219.465701	96.632223	50.424321
216.167687	97.427251	50.429325
212.259861	99.083443	50.434330
209.096729	92.568017	50.439335
205.646233	97.243571	50.444340
202.036397	101.064561	50.449345
198.853676	93.973237	50.454349
195.106651	97.372793	50.459354
191.457116	86.444187	50.464359
187.865416	95.685039	50.469364
184.196459	90.862389	50.474369
181.364084	97.295085	50.479373
177.408593	96.010127	50.484378
174.453442	93.321931	50.489383
170.818356	94.362771	50.494388
166.889196	95.509795	50.499393
163.497766	92.019915	50.504397
159.820947	99.989624	50.509402
156.760393	98.377809	50.514407
153.274419	100.433012	50.519412
149.320981	98.337820	50.524417
146.121314	96.874354	50.529421
142.826901	103.904634	50.534426
138.935831	102.024303	50.539431
135.323102	107.054332	50.544436
132.328492	101.420535	50.549441
128.709810	93.745805	50.554445
124.908443	102.902470	50.559450
121.377020	102.500230	50.564455
118.075932	96.724629	50.569460
114.293921	104.448243	50.574465
111.077541	93.217693	50.579469
107.310833	99.967634	50.584474
104.483221	103.204202	50.589479
100.397649	107.678735	50.594484
96.628236	103.327442	50.599489
93.584651	92.072993	50.604493
89.873389	103.246692	50.609498
86.748569	87.980664	50.614503
82.802998	100.526182	50.619508
79.254685	95.814392	50.624513
76.089446	91.887313	50.629517
72.568442	94.508021	50.634522
68.837343	95.820211	50.639527
65.780542	92.812621	50.644532
61.975722	97.009063	50.649537
58.556403	89.584709	50.654541
54.546848	96.078486	50.659546
51.348637	94.001058	50.664551
47.846200	94.885124	50.669556
44.376268	100.721720	50.674561
40.988871	92.419172	50.679565
37.331886	104.815090	50.684570
33.732269	93.223840	50.689575
30.856634	101.068068	50.694580
26.916578	102.735718	50.699585
23.866317	94.839102	50.704589
20.329523	102.470546	50.709594
16.486908	88.747037	50.714599
13.164945	91.064499	50.719604
9.113508	100.763424	50.724609
5.234276	92.189939	50.729613
1.867242	93.375512	50.734618