Thu Aug 25 12:21:23 2022

Number of Points = 9925

Depth (nm)	Load (N)	Time (s)
1.551823	100.853709	0.000000
1.942089	98.514636	0.005005
1.697026	112.362876	0.010010
1.703362	109.824528	0.015014
1.722048	103.361170	0.020019
1.356700	98.403829	0.025024
1.471316	93.700319	0.030029
1.390340	91.226274	0.035034
1.401329	73.384067	0.040038
1.196195	68.202314	0.045043
1.021267	61.940151	0.050048
0.531152	39.861122	0.055053
-0.175615	39.434011	0.060058
-0.253008	32.365637	0.065062
-0.296310	26.294835	0.070067
-1.120144	16.483388	0.075072
-1.327071	20.249029	0.080077
-1.788224	14.151952	0.085082
-1.701644	13.258852	0.090086
-1.694869	0.631244	0.095091
-2.361236	5.734369	0.100096
-2.646085	-9.637967	0.105101
-2.792735	2.511654	0.110106
-2.817750	2.490251	0.115110
-3.344289	-4.760833	0.120115
-3.621403	9.592221	0.125120
-3.680249	-1.370460	0.130125
-4.322640	2.055283	0.135130
-4.703648	4.025876	0.140134
-4.846938	4.532370	0.145139
-5.583795	9.067574	0.150144
-5.662309	0.604174	0.155149
-5.513638	8.955318	0.160154
-5.561522	15.265005	0.165158
-5.521408	8.137101	0.170163
-6.123250	13.362995	0.175168
-6.376504	4.420772	0.180173
-6.843132	11.438310	0.185178
-7.054404	7.842578	0.190182
-6.909743	7.506688	0.195187
-7.217210	19.181645	0.200192
-7.840384	4.115409	0.205197
-8.022616	12.262138	0.210202
-8.423476	1.264459	0.215206
-8.016488	0.995034	0.220211
-8.443145	12.891142	0.225216
-8.855341	5.077973	0.230221
-9.750255	2.361314	0.235226
-10.057929	0.321435	0.240230
-9.637300	3.602765	0.245235
-10.163018	0.957972	0.250240
-9.664838	-0.300176	0.255245
-10.073977	3.126986	0.260250
-10.911556	-0.740770	0.265254
-10.865640	-0.627753	0.270259
-11.185001	5.933274	0.275264
-11.408620	3.054485	0.280269
-11.995580	4.895996	0.285274
-12.283414	2.805552	0.290278
-12.061357	2.084213	0.295283
-12.409180	13.316236	0.300288
-12.748968	-3.300342	0.305293
-12.698860	0.848964	0.310298
-13.557387	11.275155	0.315302
-13.756608	13.574769	0.320307
-14.296048	10.340504	0.325312
-14.119013	13.780227	0.330317
-14.396553	11.881157	0.335322
-14.476664	11.972792	0.340326
-14.416589	7.325307	0.345331
-14.608876	10.107888	0.350336
-15.139984	6.062397	0.355341
-15.190298	7.171255	0.360346
-15.744070	9.694101	0.365350
-15.627150	-1.134768	0.370355
-16.276515	15.462768	0.375360
-16.760807	1.747844	0.380365
-17.370166	6.016298	0.385370
-17.360604	3.876092	0.390374
-16.989491	4.431700	0.395379
-17.232482	10.113895	0.400384
-17.106249	2.501101	0.405389
-18.028911	4.385721	0.410394
-18.854466	9.093011	0.415398
-18.464934	2.359613	0.420403
-18.872604	13.806657	0.425408
-18.791459	9.203326	0.430413
-18.742172	5.569933	0.435418
-19.204929	0.194450	0.440422
-19.698784	9.902278	0.445427
-20.277371	8.971031	0.450432
-20.065100	5.530399	0.455437
-20.561823	0.634801	0.460442
-21.510812	6.380159	0.465446
-21.229569	-0.943710	0.470451
-21.856070	6.370958	0.475456
-21.377502	1.015661	0.480461
-21.651186	2.134207	0.485466
-21.585946	6.853781	0.490470
-21.767186	5.974171	0.495475
-22.624269	7.595416	0.500480
-22.700391	-1.140439	0.505485
-22.811839	11.949632	0.510490
-23.207863	13.185424	0.515494
-23.580110	4.989511	0.520499
-24.703163	4.039172	0.525504
-24.738101	1.383920	0.530509
-24.154139	3.234952	0.535514
-24.294993	4.253592	0.540518
-24.195383	-4.731259	0.545523
-24.654424	0.690556	0.550528
-24.845684	-4.983728	0.555533
-25.227771	-1.203302	0.560538
-25.885088	-2.685359	0.565542
-25.813344	10.009011	0.570547
-26.774903	14.389601	0.575552
-27.172482	7.403045	0.580557
-26.686865	1.844163	0.585562
-26.996072	0.355018	0.590566
-27.119980	-5.532300	0.595571
-27.549524	8.797180	0.600576
-27.206383	-0.915529	0.605581
-28.179952	4.156638	0.610586
-28.678241	3.291904	0.615590
-28.793309	7.138061	0.620595
-28.848587	5.545853	0.625600
-28.477000	9.391687	0.630605
-29.116089	7.451193	0.635610
-29.778511	14.062813	0.640614
-30.033201	4.842407	0.645619
-30.735473	13.209825	0.650624
-30.710964	-3.618854	0.655629
-30.815603	-0.071726	0.660634
-31.003720	7.895589	0.665638
-30.569762	3.059809	0.670643
-30.880528	10.483195	0.675648
-30.579094	5.579593	0.680653
-31.487203	6.114177	0.685658
-31.593835	11.078981	0.690662
-32.614571	-0.609341	0.695667
-32.937722	6.107304	0.700672
-33.214066	11.937094	0.705677
-33.350811	4.106077	0.710682
-33.512229	7.291945	0.715686
-33.216819	0.937127	0.720691
-33.592871	13.024621	0.725696
-33.573588	5.147010	0.730701
-34.239991	7.545136	0.735706
-34.856036	5.382733	0.740710
-34.701550	7.196655	0.745715
-34.718326	9.122833	0.750720
-34.803188	2.245468	0.755725
-35.599297	6.236301	0.760730
-36.637570	7.180422	0.765734
-36.115544	3.061669	0.770739
-36.587817	7.166275	0.775744
-36.466026	-8.503890	0.780749
-36.296857	-2.009922	0.785754
-36.893258	6.875578	0.790758
-37.376158	1.617148	0.795763
-37.594413	11.626642	0.800768
-37.445360	-0.751172	0.805773
-37.903103	8.992125	0.810778
-38.459650	5.418858	0.815782
-38.737899	7.578995	0.820787
-39.024293	-2.664658	0.825792
-39.146562	4.675406	0.830797
-39.426485	5.687363	0.835802
-39.555343	9.288909	0.840806
-38.997985	-4.693626	0.845811
-39.981774	-3.258170	0.850816
-40.242600	3.246228	0.855821
-40.668893	5.777573	0.860826
-40.429980	10.251636	0.865830
-41.282586	8.654646	0.870835
-42.335790	6.114653	0.875840
-41.760882	8.837135	0.880845
-42.488347	10.074241	0.885850
-42.085674	15.721707	0.890854
-42.043949	9.852725	0.895859
-42.379782	12.202219	0.900864
-42.013095	3.523529	0.905869
-43.160513	6.980952	0.910874
-43.554075	10.658775	0.915878
-43.640072	5.629218	0.920883
-44.507070	3.936409	0.925888
-44.224099	4.439387	0.930893
-43.831590	5.352309	0.935898
-44.288130	9.935341	0.940902
-44.752435	6.069211	0.945907
-45.447911	1.809034	0.950912
-45.127344	1.635407	0.955917
-45.206912	9.873615	0.960922
-45.531578	11.313362	0.965926
-45.943094	1.443653	0.970931
-46.510362	0.301828	0.975936
-46.404112	4.995992	0.980941
-46.679039	5.459838	0.985946
-47.265187	10.819315	0.990950
-47.577963	1.117633	0.995955
-47.923346	16.161592	1.000960
-47.924578	-0.365662	1.005965
-48.246031	5.575598	1.010970
-48.267804	13.001158	1.015974
-48.315665	18.640125	1.020979
-48.257905	13.249520	1.025984
-48.789286	10.580307	1.030989
-49.198658	7.999544	1.035994
-49.433533	14.661231	1.040998
-49.455082	5.363166	1.046003
-50.540671	12.654860	1.051008
-50.471719	3.507132	1.056013
-50.224546	9.422569	1.061018
-50.810622	6.951752	1.066022
-50.798813	4.384088	1.071027
-51.481845	3.330005	1.076032
-51.832866	7.608602	1.081037
-51.875938	0.246965	1.086042
-52.234171	6.747644	1.091046
-52.223406	7.337567	1.096051
-52.381223	8.276608	1.101056
-52.759686	-0.218883	1.106061
-53.450994	7.371696	1.111066
-53.878673	5.024756	1.116070
-53.556802	-2.710437	1.121075
-53.894398	10.911773	1.126080
-54.105663	9.119381	1.131085
-53.753424	8.096069	1.136090
-54.704333	10.728600	1.141094
-54.817022	7.278775	1.146099
-55.147739	8.431569	1.151104
-55.010385	6.578224	1.156109
-55.131841	-0.964119	1.161114
-56.291942	14.527036	1.166118
-56.495440	7.054492	1.171123
-56.822029	7.880773	1.176128
-57.044037	15.805944	1.181133
-57.080658	9.462021	1.186138
-56.909959	10.504611	1.191142
-57.434374	7.226867	1.196147
-57.314874	4.465159	1.201152
-57.247937	7.691176	1.206157
-58.131929	2.853099	1.211162
-58.091022	6.965880	1.216166
-58.272121	3.947554	1.221171
-59.434548	5.926694	1.226176
-60.031240	8.472086	1.231181
-59.439532	6.177388	1.236186
-59.788882	15.922687	1.241190
-59.810538	4.701080	1.246195
-59.834618	4.110056	1.251200
-60.096319	11.348584	1.256205
-59.802042	10.603272	1.261210
-60.676786	17.055174	1.266214
-60.986695	10.444025	1.271219
-61.375038	9.751891	1.276224
-61.721608	20.366788	1.281229
-62.194473	15.505417	1.286234
-62.523638	15.721497	1.291238
-62.342228	14.601566	1.296243
-62.672770	10.078563	1.301248
-62.532257	7.035152	1.306253
-62.630377	18.136300	1.311258
-63.345581	16.207735	1.316262
-63.651046	8.852409	1.321267
-64.158393	13.013134	1.326272
-64.111985	6.763770	1.331277
-64.213212	3.097015	1.336282
-64.616775	4.166311	1.341286
-65.398325	0.270800	1.346291
-65.582474	11.287347	1.351296
-65.230890	13.244391	1.356301
-65.774472	9.166058	1.361306
-65.889511	13.853768	1.366310
-65.652008	5.027642	1.371315
-66.107000	7.474901	1.376320
-66.620824	0.408491	1.381325
-67.188411	6.236458	1.386330
-67.636705	9.211013	1.391334
-67.575626	7.660684	1.396339
-67.276899	6.772307	1.401344
-67.406724	3.780748	1.406349
-67.914184	6.473509	1.411354
-68.896740	4.884230	1.416358
-69.071348	13.741606	1.421363
-68.949069	10.115758	1.426368
-69.112726	4.563699	1.431373
-68.814103	-5.328692	1.436378
-69.728359	-2.414003	1.441382
-69.921087	3.288787	1.446387
-70.379062	6.584398	1.451392
-70.174716	-0.170601	1.456397
-70.080960	4.433770	1.461402
-71.193109	12.409833	1.466406
-71.741231	2.457129	1.471411
-71.633712	11.434811	1.476416
-72.055766	9.482459	1.481421
-72.412168	5.757612	1.486426
-72.701795	11.073791	1.491430
-72.456362	7.352716	1.496435
-72.270426	10.863806	1.501440
-72.334056	9.943623	1.506445
-72.209491	11.806524	1.511450
-73.170935	10.963746	1.516454
-73.191788	6.490295	1.521459
-73.684429	11.050512	1.526464
-74.255468	8.621632	1.531469
-74.514282	8.304671	1.536474
-74.863729	16.585168	1.541478
-74.776516	1.407635	1.546483
-74.900085	6.574407	1.551488
-75.657549	6.509587	1.556493
-75.915749	9.571415	1.561498
-76.579539	10.143650	1.566502
-75.939685	12.507939	1.571507
-76.624511	13.295442	1.576512
-76.602034	9.729525	1.581517
-76.833122	15.624990	1.586522
-76.690168	12.603342	1.591526
-76.725553	11.182024	1.596531
-78.339825	10.818027	1.601536
-78.056991	15.883155	1.606541
-77.933235	15.715055	1.611546
-77.918457	13.200709	1.616550
-78.384966	15.833272	1.621555
-79.175474	14.337287	1.626560
-79.352835	8.379250	1.631565
-79.618900	14.764250	1.636570
-79.385617	12.845252	1.641574
-79.575680	6.171035	1.646579
-80.508678	14.024115	1.651584
-80.543906	13.146937	1.656589
-80.805768	19.585063	1.661594
-80.766535	12.049175	1.666598
-80.882183	3.414428	1.671603
-81.448962	14.883237	1.676608
-82.017233	5.895470	1.681613
-82.234431	13.462382	1.686618
-82.555980	16.287365	1.691622
-82.264145	9.439560	1.696627
-82.666175	16.617820	1.701632
-82.879443	21.678428	1.706637
-82.856853	17.134893	1.711642
-83.614218	15.972236	1.716646
-83.788949	12.468858	1.721651
-84.117426	20.591047	1.726656
-83.782282	13.182798	1.731661
-83.955742	2.750609	1.736666
-84.752402	6.219512	1.741670
-84.929366	9.645097	1.746675
-85.502727	16.318694	1.751680
-85.713017	16.392762	1.756685
-85.608186	16.066277	1.761690
-85.967223	13.487119	1.766694
-85.433332	13.200970	1.771699
-86.617094	13.759770	1.776704
-86.909475	12.638149	1.781709
-86.397988	13.804508	1.786714
-87.102535	16.430077	1.791718
-87.267076	4.756299	1.796723
-87.943212	3.979549	1.801728
-88.314581	9.697677	1.806733
-88.605710	2.972859	1.811738
-88.777967	12.408832	1.816742
-88.470942	7.273400	1.821747
-88.643864	5.620534	1.826752
-88.763521	9.404134	1.831757
-89.785542	5.929119	1.836762
-89.882150	9.642669	1.841766
-89.794289	7.607254	1.846771
-90.121421	15.305287	1.851776
-90.554809	12.873822	1.856781
-90.382669	17.503879	1.861786
-91.016718	19.599547	1.866790
-90.795952	10.681129	1.871795
-91.296844	12.458539	1.876800
-91.889204	11.355449	1.881805
-92.233991	11.877699	1.886810
-92.602375	7.787735	1.891814
-92.617138	6.553011	1.896819
-92.813526	13.626280	1.901824
-92.751388	5.874836	1.906829
-92.937942	8.052242	1.911834
-93.179088	18.691745	1.916838
-93.511634	9.828392	1.921843
-94.008037	17.198610	1.926848
-94.115967	14.874335	1.931853
-94.034744	7.271759	1.936858
-94.619454	20.426496	1.941862
-94.832961	8.437686	1.946867
-95.458322	20.909096	1.951872
-95.648138	18.806459	1.956877
-96.066988	16.224019	1.961882
-96.392308	23.425063	1.966886
-96.035062	13.621554	1.971891
-95.743168	17.641224	1.976896
-96.628000	9.380104	1.981901
-96.802714	5.332560	1.986906
-97.233749	9.573075	1.991910
-97.086519	8.993173	1.996915
-98.243099	12.408564	2.006912
-97.587599	8.409432	2.016909
-97.047273	2.838112	2.026906
-96.392880	9.204196	2.036902
-96.072883	4.563888	2.046899
-95.559166	9.133699	2.056896
-94.712963	12.362116	2.066893
-94.750579	5.202422	2.076890
-93.769410	11.159342	2.086886
-93.158618	10.113270	2.096883
-93.437631	6.352438	2.106880
-92.342550	8.388778	2.116877
-92.227851	13.946112	2.126874
-91.529866	12.902217	2.136870
-90.527808	9.051520	2.146867
-90.514984	12.153932	2.156864
-90.594382	11.710187	2.166861
-89.679267	5.234336	2.176858
-88.611748	7.455559	2.186854
-88.092725	9.816583	2.196851
-87.822955	3.622419	2.206848
-87.853603	7.710493	2.216845
-87.063197	5.023867	2.226842
-86.504798	0.558446	2.236838
-85.913054	4.324080	2.246835
-85.192726	5.690548	2.256832
-85.048658	6.003738	2.266829
-84.984619	6.994705	2.276826
-83.876002	3.707020	2.286822
-83.291042	5.408312	2.296819
-82.400254	6.393277	2.306816
-82.499736	8.597792	2.316813
-82.204709	-0.612906	2.326810
-81.316650	7.446184	2.336806
-80.778530	13.130407	2.346803
-80.590927	5.051605	2.356800
-80.331079	5.432182	2.366797
-79.559196	3.198287	2.376794
-78.550563	-2.421069	2.386790
-78.124068	3.800161	2.396787
-77.718863	4.693321	2.406784
-77.867140	8.660444	2.416781
-76.391887	3.183380	2.426778
-76.328931	6.455333	2.436774
-76.450148	8.070876	2.446771
-75.610657	0.561503	2.456768
-74.880239	7.872352	2.466765
-74.799557	5.170224	2.476762
-73.600863	0.097626	2.486758
-73.639494	-4.290082	2.496755
-72.453473	-2.974410	2.506752
-72.325022	0.721269	2.516749
-72.092275	1.090254	2.526746
-71.704217	0.180455	2.536742
-70.796862	2.867101	2.546739
-70.623568	2.200028	2.556736
-69.795634	1.455721	2.566733
-69.329199	-2.596146	2.576730
-69.003048	-3.055921	2.586726
-68.589560	-0.253876	2.596723
-67.993736	-2.821311	2.606720
-66.987278	1.069409	2.616717
-66.461143	1.756720	2.626714
-66.377235	0.432080	2.636710
-65.920445	2.609620	2.646707
-65.485991	-1.133127	2.656704
-65.057474	-0.718790	2.666701
-64.538389	-4.357589	2.676698
-63.575259	-0.387219	2.686694
-63.561934	2.252615	2.696691
-63.393514	2.343410	2.706688
-62.316930	4.309793	2.716685
-61.837831	5.837606	2.726682
-60.927815	0.293891	2.736678
-60.586501	-2.376216	2.746675
-60.520772	-0.352811	2.756672
-60.454907	0.112016	2.766669
-59.207020	-8.833002	2.776666
-59.014797	-0.813767	2.786662
-58.574683	-8.985983	2.796659
-57.880114	0.478251	2.806656
-57.259049	-2.552471	2.816653
-56.382372	-2.046798	2.826650
-56.377916	2.466596	2.836646
-56.373352	-0.739956	2.846643
-55.537456	7.371661	2.856640
-54.603668	10.516668	2.866637
-54.455023	4.078555	2.876634
-53.381920	8.605068	2.886630
-53.203323	11.513613	2.896627
-53.224124	8.225503	2.906624
-52.763071	8.799469	2.916621
-52.357760	3.800502	2.926618
-50.852193	1.445313	2.936614
-50.543049	7.190758	2.946611
-50.486842	3.824058	2.956608
-50.076967	1.070349	2.966605
-49.437192	6.336334	2.976602
-49.022232	3.277718	2.986598
-48.166538	7.448658	2.996595
-47.933412	6.366732	3.006592
-47.454533	8.192354	3.016589
-46.581458	1.412650	3.026586
-46.247106	9.929140	3.036582
-46.189682	10.563183	3.046579
-45.472057	9.167755	3.056576
-45.010512	12.440612	3.066573
-44.176601	11.543316	3.076570
-43.641003	8.225044	3.086566
-43.257541	9.226150	3.096563
-42.888724	9.285545	3.106560
-41.893525	11.302698	3.116557
-41.899120	13.191562	3.126554
-41.474154	8.807236	3.136550
-40.513793	12.546796	3.146547
-40.213709	9.645563	3.156544
-40.546808	19.451399	3.166541
-39.420375	16.103904	3.176538
-38.769778	8.804691	3.186534
-37.996866	15.674902	3.196531
-37.810728	13.824226	3.206528
-37.696197	12.602492	3.216525
-36.836835	14.254458	3.226522
-36.352898	13.310629	3.236518
-35.809941	17.188453	3.246515
-34.857769	13.776397	3.256512
-34.837721	13.909449	3.266509
-34.584930	15.985909	3.276506
-33.838500	12.172102	3.286502
-33.154807	15.910665	3.296499
-32.779668	15.158113	3.306496
-32.211875	5.622736	3.316493
-31.984245	4.421295	3.326490
-31.385848	13.659856	3.336486
-30.509230	20.954145	3.346483
-30.348465	16.687242	3.356480
-30.198362	23.236894	3.366477
-28.872079	12.920595	3.376474
-28.521336	9.944900	3.386470
-28.743145	12.627916	3.396467
-28.021754	9.834898	3.406464
-27.362733	12.782208	3.416461
-26.667342	8.608935	3.426458
-26.334952	9.111196	3.436454
-25.908705	7.808942	3.446451
-25.119689	10.238539	3.456448
-24.909532	12.480069	3.466445
-24.440378	12.001057	3.476442
-23.380361	10.871930	3.486438
-23.145321	10.312392	3.496435
-23.239035	14.749306	3.506432
-22.059800	14.288913	3.516429
-21.646419	17.509131	3.526426
-21.591113	9.099427	3.536422
-20.429737	13.070422	3.546419
-19.865606	1.495555	3.556416
-19.742391	8.445390	3.566413
-19.750015	4.312579	3.576410
-18.666112	9.287234	3.586406
-18.070881	11.218172	3.596403
-18.024570	15.224500	3.606400
-17.546837	9.843552	3.616397
-17.080246	10.020676	3.626394
-15.962063	14.229689	3.636390
-15.451307	11.216251	3.646387
-15.506166	9.773970	3.656384
-14.425597	13.101891	3.666381
-13.828542	7.337950	3.676378
-13.992712	8.361508	3.686374
-13.392761	3.240179	3.696371
-12.732336	5.838811	3.706368
-12.734235	13.844124	3.716365
-11.181804	8.880830	3.726362
-10.883554	12.096913	3.736358
-10.706404	15.407998	3.746355
-10.846094	10.782694	3.756352
-9.931751	12.296168	3.766349
-9.423387	4.879859	3.776346
-8.096279	6.924205	3.786342
-7.813469	5.004531	3.796339
-8.189195	4.952505	3.806336
-7.706956	6.476662	3.816333
-6.760811	7.893287	3.826330
-6.280620	9.658518	3.836326
-5.399805	5.145749	3.846323
-5.000638	10.702865	3.856320
-5.171694	9.399166	3.866317
-4.410843	9.999020	3.876314
-4.061376	17.600823	3.886310
-3.267803	21.388699	3.896307
-3.084968	23.637680	3.906304
-2.590351	41.391746	3.916301
-2.115496	44.630849	3.926298
-1.545672	56.946690	3.936294
-1.138455	65.721060	3.946291
-0.861978	81.634000	3.956288
-0.465500	99.881843	3.966285
0.000000	116.045953	3.971290
0.158013	118.359211	3.976294
0.441476	126.793696	3.981299
0.605388	141.084082	3.986304
0.965952	150.813137	3.991309
0.862377	144.916254	3.996314
0.700426	143.112955	4.001318
1.038508	147.688577	4.006323
1.072891	148.382372	4.011328
0.807980	145.171506	4.016333
0.902258	149.873914	4.021338
0.954651	155.886363	4.026342
1.007708	149.860532	4.031347
0.945225	146.168691	4.036352
0.943197	152.648414	4.041357
1.524446	151.943556	4.046362
0.765505	153.476668	4.051366
1.116918	179.794869	4.056371
1.540409	178.260508	4.061376
1.556871	178.814742	4.066381
1.362313	158.907068	4.071386
0.532024	153.424607	4.076390
0.975921	161.621997	4.081395
0.890168	174.483535	4.086400
1.370749	173.569822	4.091405
1.719062	175.676098	4.096410
0.895667	186.815064	4.101414
1.237347	182.053807	4.106419
1.258004	184.284190	4.111424
1.201852	178.212185	4.116429
1.088421	175.534404	4.121434
1.033315	178.507491	4.126438
1.391509	171.987749	4.131443
1.405026	180.575288	4.136448
1.463483	177.244146	4.141453
1.605547	178.474733	4.146458
1.234438	174.758476	4.151462
1.672695	183.744542	4.156467
1.522125	181.237096	4.161472
1.484481	175.845570	4.166477
1.275589	177.751247	4.171482
1.582947	181.448996	4.176486
1.801690	179.677794	4.181491
1.508970	180.033698	4.186496
1.659851	185.692201	4.191501
1.702090	177.529338	4.196506
1.386362	185.349047	4.201510
1.481032	182.414030	4.206515
1.573451	196.190474	4.211520
1.663914	190.747233	4.216525
1.393499	185.047323	4.221530
1.287266	188.964902	4.226534
1.456426	188.906748	4.231539
1.399430	192.873561	4.236544
1.405000	184.583562	4.241549
1.182631	193.312472	4.246554
1.423541	193.897979	4.251558
2.125230	198.201505	4.256563
1.500990	194.844448	4.261568
1.499062	196.837923	4.266573
1.968098	200.168655	4.271578
1.516360	200.498854	4.276582
1.625610	201.174594	4.281587
1.457931	210.182847	4.286592
1.524243	212.561106	4.291597
1.994492	209.396392	4.296602
1.656726	212.458066	4.301606
2.065147	217.076469	4.306611
1.913262	220.197605	4.311616
1.975840	222.332838	4.316621
1.961985	207.487336	4.321626
2.064181	207.278321	4.326630
1.798608	203.244962	4.331635
1.929618	202.809967	4.336640
1.893757	208.415478	4.341645
2.153366	210.801415	4.346650
1.327827	214.657696	4.351654
2.044332	206.677078	4.356659
2.267713	207.198892	4.361664
2.226573	205.370330	4.366669
1.654514	193.817218	4.371674
2.058310	210.898498	4.376678
1.912488	206.821065	4.381683
1.906426	208.302656	4.386688
1.820512	214.846165	4.391693
2.159821	217.184814	4.396698
1.679112	217.627121	4.401702
2.079861	208.246961	4.406707
1.616155	213.663243	4.411712
1.760907	207.161113	4.416717
1.309367	206.668697	4.421722
1.618487	220.977524	4.426726
1.754858	219.671647	4.431731
2.143030	229.235066	4.436736
1.922569	239.713276	4.441741
1.855748	242.555329	4.446746
2.104459	245.104332	4.451750
2.433580	241.047389	4.456755
2.587658	236.669857	4.461760
2.423734	239.239219	4.466765
2.491093	240.165136	4.471770
2.355996	240.338154	4.476774
1.988823	223.178317	4.481779
2.154810	232.893611	4.486784
2.035497	237.483974	4.491789
2.390072	233.065537	4.496794
1.914311	246.526079	4.501798
2.243946	236.729934	4.506803
2.205375	246.255821	4.511808
2.126133	238.384051	4.516813
2.244167	243.981279	4.521818
2.220840	255.789042	4.526822
2.137648	240.182411	4.531827
2.099838	244.975144	4.536832
2.324250	244.076254	4.541837
2.622162	245.035651	4.546842
2.407579	240.972148	4.551846
2.314688	244.549123	4.556851
2.235005	241.201647	4.561856
2.423610	252.802193	4.566861
2.416118	244.077609	4.571866
1.931396	245.476012	4.576870
2.621199	255.134555	4.581875
2.845505	261.945854	4.586880
2.488753	252.643230	4.591885
2.555441	244.843506	4.596890
2.645044	243.905627	4.601894
1.958440	233.550532	4.606899
2.492204	260.140840	4.611904
2.557560	262.288298	4.616909
2.730075	264.089931	4.621914
2.467590	267.585914	4.626918
2.691498	264.912212	4.631923
2.748023	265.874630	4.636928
2.369407	257.891569	4.641933
2.577683	262.063610	4.646938
2.865538	260.863710	4.651942
3.053162	262.432018	4.656947
2.654112	268.543713	4.661952
2.736877	269.071743	4.666957
2.516064	274.041856	4.671962
2.473559	275.370972	4.676966
2.953244	265.121025	4.681971
2.815883	267.464763	4.686976
2.485201	275.846847	4.691981
2.881978	264.989785	4.696986
2.776104	262.190583	4.701990
3.094522	266.475083	4.706995
3.228216	267.099538	4.712000
2.901607	260.908528	4.717005
2.979349	257.988806	4.722010
2.605972	253.235163	4.727014
2.973578	260.881398	4.732019
2.906684	263.441888	4.737024
2.839116	268.204488	4.742029
2.925114	266.979267	4.747034
2.999591	267.378880	4.752038
2.675396	257.001788	4.757043
2.894782	261.444175	4.762048
2.402697	262.359672	4.767053
2.710099	267.471649	4.772058
3.076453	261.130933	4.777062
2.925658	266.140694	4.782067
2.958005	279.047079	4.787072
2.808279	273.138402	4.792077
3.102106	268.346654	4.797082
2.816697	270.140942	4.802086
2.796911	261.373983	4.807091
2.418023	269.140349	4.812096
2.547452	280.006692	4.817101
3.038250	283.514366	4.822106
3.008581	291.513931	4.827110
3.051477	286.963978	4.832115
3.065794	291.166416	4.837120
2.979532	287.696574	4.842125
3.052351	294.623372	4.847130
3.040463	296.618419	4.852134
2.988636	282.965230	4.857139
2.846953	290.099644	4.862144
2.965270	302.628738	4.867149
3.057153	299.058214	4.872154
2.915597	298.441294	4.877158
2.873321	298.027120	4.882163
2.982859	309.909015	4.887168
3.335623	321.967948	4.892173
4.027079	323.618673	4.897178
3.644269	316.522109	4.902182
3.389828	308.212680	4.907187
3.212287	303.956694	4.912192
3.230717	297.363590	4.917197
2.991114	302.001292	4.922202
3.182588	308.292561	4.927206
3.647863	313.585464	4.932211
3.157865	309.036742	4.937216
3.238254	316.889358	4.942221
3.558771	317.193473	4.947226
3.422900	327.908421	4.952230
3.425884	321.577161	4.957235
3.535365	323.078623	4.962240
3.422266	325.304671	4.967245
3.880443	320.164450	4.972250
3.264726	322.880544	4.977254
3.414991	321.847734	4.982259
3.639343	318.715202	4.987264
3.269654	316.219922	4.992269
3.188023	322.550825	4.997274
3.137879	323.308492	5.002278
3.108347	318.826828	5.007283
3.691889	320.832989	5.012288
3.524248	326.335797	5.017293
3.606351	322.833240	5.022298
3.763510	318.724128	5.027302
3.759425	328.029517	5.032307
3.654205	319.209475	5.037312
3.829515	319.064934	5.042317
3.947887	325.487889	5.047322
3.598258	324.422670	5.052326
3.727747	320.820939	5.057331
3.690976	324.604276	5.062336
3.892240	321.813889	5.067341
3.922656	321.663576	5.072346
3.676287	315.627656	5.077350
3.617546	320.727414	5.082355
3.685933	327.952317	5.087360
3.685522	325.414996	5.092365
3.834573	321.240714	5.097370
3.622344	330.458492	5.102374
3.908989	326.541065	5.107379
3.497156	320.303275	5.112384
3.363064	324.889648	5.117389
3.629121	335.804222	5.122394
3.761293	330.047514	5.127398
3.748889	332.431794	5.132403
3.811247	331.368464	5.137408
3.822018	323.384474	5.142413
3.817587	338.739125	5.147418
3.517877	337.862240	5.152422
3.660291	342.250267	5.157427
4.200795	351.944912	5.162432
4.202594	351.840212	5.167437
4.337523	349.566425	5.172442
3.436667	340.187653	5.177446
3.821006	347.356731	5.182451
3.869446	352.066375	5.187456
3.833578	356.400080	5.192461
4.357307	348.025654	5.197466
4.337259	357.773329	5.202470
4.143403	357.446180	5.207475
4.231016	349.994316	5.212480
3.636302	359.749773	5.217485
4.326792	356.268947	5.222490
4.379543	361.566387	5.227494
4.737209	345.406524	5.232499
4.272210	335.405795	5.237504
4.103472	342.028768	5.242509
4.079208	334.505852	5.247514
3.777164	334.227294	5.252518
4.095318	330.263800	5.257523
3.719298	335.501861	5.262528
3.877915	350.963855	5.267533
4.610053	359.287021	5.272538
4.384708	360.679594	5.277542
4.222362	354.946877	5.282547
4.173643	360.351966	5.287552
4.274701	350.427055	5.292557
4.273315	354.122595	5.297562
4.215566	366.233223	5.302566
4.496435	360.162135	5.307571
4.623302	360.518740	5.312576
4.213347	359.947035	5.317581
4.532269	360.444393	5.322586
4.454903	349.462251	5.327590
4.057376	347.379460	5.332595
4.060724	351.887357	5.337600
3.942404	355.987204	5.342605
4.087463	355.730342	5.347610
3.981542	360.305983	5.352614
4.110473	357.606019	5.357619
4.391000	350.503585	5.362624
4.470725	358.185477	5.367629
4.301158	356.614307	5.372634
4.296685	354.488913	5.377638
4.309094	361.222718	5.382643
4.477748	375.889044	5.387648
4.320159	376.065587	5.392653
4.912694	370.587918	5.397658
4.897403	378.531484	5.402662
4.642895	368.424988	5.407667
4.925827	361.227259	5.412672
4.185009	360.112597	5.417677
3.977852	363.255074	5.422682
4.364047	374.210960	5.427686
4.587728	373.922796	5.432691
4.245802	371.587677	5.437696
4.241191	378.520311	5.442701
5.222154	377.328866	5.447706
4.419649	389.923205	5.452710
4.669270	376.092995	5.457715
4.531217	382.818745	5.462720
4.206291	390.820322	5.467725
4.402972	385.629304	5.472730
4.363014	387.647742	5.477734
4.777959	384.156299	5.482739
4.699154	394.042917	5.487744
4.687411	401.318371	5.492749
4.857902	398.817537	5.497754
4.937891	407.685842	5.502758
4.565497	394.959174	5.507763
4.677577	397.902938	5.512768
5.135465	413.052334	5.517773
5.241246	402.892531	5.522778
4.499555	397.737803	5.527782
4.652416	390.658520	5.532787
4.280788	401.676213	5.537792
4.342468	404.324148	5.542797
4.455359	414.000403	5.547802
4.723609	411.961988	5.552806
5.086436	409.257007	5.557811
4.798816	414.610957	5.562816
4.405186	422.509415	5.567821
5.247161	421.709913	5.572826
4.851447	428.849382	5.577830
5.075216	430.313964	5.582835
5.248234	419.760793	5.587840
4.666234	424.860308	5.592845
5.280679	429.541401	5.597850
4.763145	431.435351	5.602854
5.116928	436.321807	5.607859
5.159365	437.188362	5.612864
5.148279	445.719771	5.617869
4.966770	438.044275	5.622874
5.202686	441.775419	5.627878
5.448490	431.726541	5.632883
4.854829	419.237010	5.637888
4.734896	428.702974	5.642893
5.222864	434.881393	5.647898
5.111183	435.768932	5.652902
5.130428	439.540353	5.657907
5.298751	438.378153	5.662912
4.982968	438.585811	5.667917
5.275838	434.430098	5.672922
5.588396	440.164592	5.677926
5.259805	442.212442	5.682931
5.623939	438.820701	5.687936
5.368841	434.390169	5.692941
5.623257	428.323204	5.697946
4.846447	416.726095	5.702950
5.253982	424.416766	5.707955
5.254624	434.550391	5.712960
5.396969	432.867067	5.717965
5.109430	435.060347	5.722970
4.904211	443.106468	5.727974
4.778909	442.534453	5.732979
4.956477	436.375119	5.737984
5.293062	440.960543	5.742989
5.201734	433.055779	5.747994
5.146674	437.860757	5.752998
4.941621	442.363365	5.758003
5.138343	468.364536	5.763008
5.452643	462.044561	5.768013
5.187571	459.355694	5.773018
5.242635	469.882620	5.778022
5.664837	474.584354	5.783027
5.546758	467.490544	5.788032
5.262781	469.626322	5.793037
5.615031	467.087509	5.798042
5.612375	465.183285	5.803046
5.614394	462.496863	5.808051
5.672639	469.229854	5.813056
5.471858	467.970458	5.818061
5.307539	462.541744	5.823066
5.764972	467.250612	5.828070
5.721085	459.563035	5.833075
5.551166	464.904886	5.838080
5.329390	467.081538	5.843085
5.439976	467.231883	5.848090
5.495629	474.651834	5.853094
5.385794	476.988123	5.858099
5.790668	469.011924	5.863104
5.529647	483.922836	5.868109
5.854872	480.815601	5.873114
5.736951	486.683999	5.878118
5.843169	481.649500	5.883123
5.796847	476.474383	5.888128
5.614334	477.660932	5.893133
5.898603	477.644855	5.898138
5.968441	476.830287	5.903142
5.830520	477.076517	5.908147
5.542445	477.770229	5.913152
5.497561	484.712379	5.918157
6.237002	490.864070	5.923162
6.188196	496.012943	5.928166
5.818988	481.194417	5.933171
6.250869	478.965836	5.938176
5.689703	483.726736	5.943181
5.643825	471.239927	5.948186
5.898889	479.084228	5.953190
5.702394	490.457359	5.958195
5.550929	505.370106	5.963200
5.757994	504.689063	5.968205
5.837473	491.018305	5.973210
5.696159	496.551842	5.978214
5.562777	498.645043	5.983219
6.105830	496.183901	5.988224
6.038168	504.774824	5.993229
6.062232	500.192966	5.998234
5.742355	496.376862	6.003238
5.933292	497.109419	6.008243
5.978588	494.400392	6.013248
5.532671	503.202445	6.018253
5.959278	498.241131	6.023258
5.739081	500.256184	6.028262
5.863540	500.505598	6.033267
6.059871	495.804998	6.038272
6.403806	501.116968	6.043277
5.730426	496.198288	6.048282
6.193044	502.320589	6.053286
6.413252	499.985963	6.058291
6.159514	495.830457	6.063296
5.749057	498.397354	6.068301
6.071778	491.516050	6.073306
6.182774	502.629033	6.078310
5.880446	495.200239	6.083315
5.753883	493.078139	6.088320
6.019657	503.708114	6.093325
5.873289	497.716577	6.098330
6.030836	503.972102	6.103334
5.487056	496.666563	6.108339
5.956839	498.953168	6.113344
5.913541	504.224570	6.118349
6.066690	489.074248	6.123354
6.016878	495.805198	6.128358
5.977066	502.243509	6.133363
6.268764	496.151696	6.138368
6.055063	501.025842	6.143373
6.049015	493.696163	6.148378
6.272591	499.833770	6.153382
6.021136	499.680164	6.158387
6.034582	497.273528	6.163392
6.053049	495.745652	6.168397
5.783950	492.541706	6.173402
5.582312	500.277235	6.178406
5.967879	486.365527	6.183411
5.921545	493.424970	6.188416
5.948677	497.913358	6.193421
5.896210	497.962697	6.198426
5.815530	511.168540	6.203430
6.187252	504.387124	6.208435
5.841994	500.783810	6.213440
6.226959	496.430151	6.218445
6.089095	494.420556	6.223450
5.953347	500.816950	6.228454
5.927598	503.975321	6.233459
6.286437	501.109595	6.238464
5.614043	504.287025	6.243469
6.098826	499.705748	6.248474
5.942091	503.738879	6.253478
6.010623	499.324065	6.258483
6.224590	501.119227	6.263488
5.981610	499.224181	6.268493
6.332049	501.592762	6.273498
6.011193	505.088445	6.278502
6.110029	508.176675	6.283507
6.263738	500.689081	6.288512
6.087543	503.804584	6.293517
5.954961	500.228060	6.298522
6.041292	503.694746	6.303526
6.030207	504.939860	6.308531
6.240120	494.709904	6.313536
5.624740	495.236594	6.318541
5.942884	496.439615	6.323546
5.797982	514.290548	6.328550
6.223381	512.173714	6.333555
6.091529	497.498323	6.338560
5.806982	492.847759	6.343565
5.771887	503.129395	6.348570
5.997505	505.182167	6.353574
6.173619	501.933772	6.358579
6.464565	497.348065	6.363584
5.758293	489.887649	6.368589
5.789800	486.269599	6.373594
5.767584	489.000296	6.378598
5.985274	501.982208	6.383603
6.083049	499.910381	6.388608
5.735014	498.863885	6.393613
6.183109	495.905079	6.398618
5.816981	499.771696	6.403622
5.744414	496.755260	6.408627
6.179223	501.733445	6.413632
5.764296	501.459915	6.418637
6.220320	495.924501	6.423642
6.100860	503.156761	6.428646
6.045527	499.726325	6.433651
6.160933	493.023040	6.438656
5.300173	494.034279	6.443661
6.128581	487.390127	6.448666
6.200989	502.210845	6.453670
5.649662	511.285689	6.458675
6.026650	508.319039	6.463680
5.935671	514.708423	6.468685
6.163798	497.606912	6.473690
6.442220	503.074685	6.478694
5.942132	492.133377	6.483699
5.747726	479.407235	6.488704
5.877241	494.389847	6.493709
6.189145	491.582098	6.498714
5.909751	490.546994	6.503718
5.748484	485.437342	6.508723
6.131119	489.170819	6.513728
5.932482	494.545653	6.518733
5.830203	495.691157	6.523738
5.792200	501.509073	6.528742
5.859817	497.423441	6.533747
6.400212	499.638870	6.538752
5.808033	508.166441	6.543757
5.392791	504.453865	6.548762
5.668120	501.541111	6.553766
5.620891	507.392113	6.558771
6.101770	504.621163	6.563776
5.702613	507.932957	6.568781
5.849666	515.256345	6.573786
6.109536	514.775842	6.578790
5.915174	513.743232	6.583795
6.509931	507.259073	6.588800
5.928900	508.697895	6.593805
6.237388	502.654071	6.598810
6.384079	507.917853	6.603814
6.189160	509.925782	6.608819
5.804654	507.496074	6.613824
6.191563	511.035891	6.618829
6.426197	500.197765	6.623834
6.157572	492.403013	6.628838
6.042207	486.520520	6.633843
6.126632	473.880411	6.638848
5.799643	489.212962	6.643853
5.808721	484.832778	6.648858
5.350084	475.808599	6.653862
5.583468	489.101262	6.658867
6.086981	490.968119	6.663872
5.887094	495.416144	6.668877
6.091653	500.177298	6.673882
6.097952	509.278668	6.678886
5.837695	507.452768	6.683891
6.043546	501.276325	6.688896
6.017878	511.768467	6.693901
5.989078	497.466082	6.698906
6.290304	494.381588	6.703910
6.108139	491.657580	6.708915
6.265778	478.237183	6.713920
6.106979	478.901148	6.718925
5.895877	468.297400	6.723930
5.694433	481.427228	6.728934
5.736947	472.289727	6.733939
5.657143	479.889096	6.738944
5.767269	501.306830	6.743949
6.238699	496.230923	6.748954
6.013987	502.565325	6.753958
6.111903	500.854153	6.758963
6.447894	494.208057	6.763968
5.835661	489.083639	6.768973
5.702007	476.512500	6.773978
6.050192	490.457910	6.778982
5.761160	491.135953	6.783987
5.969675	491.625304	6.788992
5.934283	506.785628	6.793997
6.004347	497.166057	6.799002
6.067924	508.014382	6.804006
5.926822	503.913995	6.809011
6.161285	493.632735	6.814016
6.099858	491.038510	6.819021
5.938418	481.777931	6.824026
5.892788	476.504627	6.829030
5.669531	485.926698	6.834035
6.314062	492.985463	6.839040
5.952631	494.525922	6.844045
6.081665	478.771931	6.849050
5.993267	481.927459	6.854054
6.076562	488.466703	6.859059
6.311049	485.848260	6.864064
6.282587	483.935423	6.869069
6.228623	481.836751	6.874074
5.726637	475.119474	6.879078
5.802006	479.306063	6.884083
5.929833	470.677227	6.889088
5.578101	478.951970	6.894093
5.546642	477.893839	6.899098
5.923440	484.947093	6.904102
6.197534	491.358363	6.909107
6.192878	479.532659	6.914112
5.902470	485.959607	6.919117
6.243000	479.018569	6.924122
5.835012	480.930162	6.929126
6.063696	483.703806	6.934131
6.081382	482.669613	6.939136
6.316323	488.353007	6.944141
6.230400	477.989074	6.949146
6.167334	479.530241	6.954150
6.182701	474.563763	6.959155
5.954952	470.264983	6.964160
5.950593	478.406202	6.969165
5.961994	474.519214	6.974170
6.213260	472.398030	6.979174
5.816692	487.238431	6.984179
6.297831	469.812558	6.989184
5.918328	484.150398	6.994189
5.355097	474.411762	6.999194
6.184126	472.095645	7.004198
5.837536	471.798753	7.009203
6.061629	476.044298	7.014208
5.970978	484.562881	7.019213
6.186488	478.986061	7.024218
6.017290	481.600578	7.029222
5.880376	479.834451	7.034227
6.032238	467.044572	7.039232
5.819963	476.778137	7.044237
6.072655	477.159323	7.049242
6.221418	475.278831	7.054246
5.847440	474.499000	7.059251
6.134108	479.108073	7.064256
6.101551	484.744792	7.069261
5.970430	466.465702	7.074266
6.121591	475.639272	7.079270
5.888064	479.042172	7.084275
5.744763	469.272544	7.089280
5.786338	472.720925	7.094285
5.889291	480.854822	7.099290
6.124643	471.579536	7.104294
5.892919	465.807033	7.109299
5.726870	465.336317	7.114304
5.967873	468.104864	7.119309
5.984279	467.273357	7.124314
6.283127	471.940634	7.129318
5.943429	476.280844	7.134323
6.196796	473.599332	7.139328
5.855559	484.014348	7.144333
5.722632	482.627257	7.149338
6.263976	482.301974	7.154342
6.064591	477.606432	7.159347
6.273858	474.020644	7.164352
5.905595	477.017537	7.169357
6.152668	470.429675	7.174362
6.199257	482.055785	7.179366
5.698654	467.647010	7.184371
5.824862	464.612090	7.189376
5.671620	472.583640	7.194381
5.802037	467.985126	7.199386
6.137141	469.324696	7.204390
6.010419	484.227221	7.209395
6.249023	475.302609	7.214400
6.125789	470.164856	7.219405
6.117005	470.235825	7.224410
6.033815	461.902655	7.229414
5.682487	448.808807	7.234419
5.973343	464.104643	7.239424
6.347078	470.430690	7.244429
5.917146	457.757285	7.249434
5.836364	451.676391	7.254438
5.605829	454.022098	7.259443
6.203401	467.181751	7.264448
6.184784	480.706886	7.269453
6.149791	466.367531	7.274458
6.103781	462.926150	7.279462
5.866240	462.147088	7.284467
5.796851	450.844086	7.289472
5.505570	463.304590	7.294477
5.737005	459.076238	7.299482
6.331194	476.004552	7.304486
6.072351	474.776399	7.309491
6.209489	471.515133	7.314496
5.839820	466.400174	7.319501
5.838099	463.483378	7.324506
5.799168	466.017369	7.329510
5.514715	477.027777	7.334515
5.942910	480.456713	7.339520
5.794769	483.365331	7.344525
6.390363	478.848956	7.349530
5.950676	479.044390	7.354534
5.911544	484.979539	7.359539
6.288646	480.073444	7.364544
6.128444	473.691767	7.369549
6.164368	462.739262	7.374554
6.108498	459.312082	7.379558
5.766702	454.354114	7.384563
6.067525	456.784249	7.389568
6.276735	456.741966	7.394573
6.092703	443.615581	7.399578
6.090167	446.396973	7.404582
5.854766	445.408764	7.409587
6.046650	447.887605	7.414592
5.573562	440.349544	7.419597
5.615888	445.294294	7.424602
6.003283	461.568445	7.429606
5.734127	470.687644	7.434611
6.266817	469.246883	7.439616
6.178094	466.413323	7.444621
6.286088	468.962259	7.449626
5.915815	461.414408	7.454630
5.455750	454.174866	7.459635
6.050317	455.138415	7.464640
6.003286	472.157702	7.469645
5.909663	456.846752	7.474650
5.890173	465.907847	7.479654
5.830165	467.970566	7.484659
6.076950	476.097744	7.489664
5.838051	476.533807	7.494669
5.827241	472.090301	7.499674
6.273209	474.886848	7.504678
6.467701	471.936143	7.509683
6.195092	453.261610	7.514688
5.621272	447.561696	7.519693
5.758085	448.805780	7.524698
6.030330	456.131675	7.529702
5.731870	464.312640	7.534707
5.932844	469.817848	7.539712
6.031127	473.583219	7.544717
5.919755	471.281567	7.549722
6.099008	474.607134	7.554726
5.610138	476.784507	7.559731
6.122428	473.948528	7.564736
5.633573	480.166116	7.569741
6.329634	468.341363	7.574746
6.197708	470.734897	7.579750
5.996001	472.611005	7.584755
5.917552	458.439820	7.589760
5.824403	463.813936	7.594765
6.045170	468.072656	7.599770
6.052162	481.356492	7.604774
5.690995	476.800197	7.609779
6.411503	466.202346	7.614784
5.722449	475.282932	7.619789
5.849674	469.571248	7.624794
6.099929	476.112802	7.629798
6.293844	474.101846	7.634803
6.069366	459.406197	7.639808
5.841492	458.568672	7.644813
5.661334	461.899929	7.649818
6.040422	463.729329	7.654822
5.838327	480.519814	7.659827
6.248887	474.880796	7.664832
5.685941	462.212410	7.669837
5.790396	459.418188	7.674842
5.917173	472.594661	7.679846
5.693327	472.699327	7.684851
5.963985	476.130799	7.689856
5.915522	470.740878	7.694861
5.951987	467.273919	7.699866
6.020718	472.954876	7.704870
6.141874	476.384461	7.709875
6.478800	468.725800	7.714880
6.113400	478.632059	7.719885
6.312147	458.605476	7.724890
5.991331	456.665681	7.729894
5.905325	452.252945	7.734899
6.184719	443.780713	7.739904
5.935052	447.334835	7.744909
6.085845	436.468754	7.749914
5.965217	442.397675	7.754918
5.669224	445.430696	7.759923
5.788552	445.446790	7.764928
5.597797	447.482535	7.769933
5.831476	465.539863	7.774938
6.056222	468.908923	7.779942
5.723499	486.928465	7.784947
5.928460	477.177035	7.789952
5.692454	476.112987	7.794957
6.038295	470.113942	7.799962
6.464998	471.388539	7.804966
6.047533	473.618000	7.809971
6.051733	474.066595	7.814976
5.868455	479.138453	7.819981
5.898322	479.870936	7.824986
6.160845	473.869125	7.829990
5.991549	471.753724	7.834995
5.959109	471.372807	7.840000
5.775084	470.012706	7.845005
6.204439	474.121683	7.850010
5.851871	470.573305	7.855014
5.827017	477.724291	7.860019
6.322160	481.981154	7.865024
6.017557	473.318829	7.870029
5.971289	458.826218	7.875034
5.534830	466.275815	7.880038
5.711259	470.108037	7.885043
6.231047	468.340259	7.890048
6.040128	477.769915	7.895053
6.148931	481.701322	7.900058
6.176979	478.362233	7.905062
6.093221	471.595247	7.910067
6.369997	460.864439	7.915072
5.992831	454.678119	7.920077
6.197077	451.925210	7.925082
5.853310	455.620631	7.930086
5.768833	451.147543	7.935091
5.821002	450.756534	7.940096
5.762402	454.717329	7.945101
5.851979	449.979683	7.950106
5.740405	454.293635	7.955110
5.526988	477.233217	7.960115
5.850828	468.972313	7.965120
5.605661	478.733180	7.970125
5.918809	482.311159	7.975142
5.881778	486.791825	7.980160
5.748383	479.971014	7.985178
6.167041	475.711395	7.990195
5.799125	482.235192	7.995213
5.945466	481.666303	8.000230
5.681516	486.422362	8.005248
5.810390	483.827053	8.010266
5.427437	480.261070	8.015283
6.080406	489.780678	8.020301
6.147850	491.048185	8.025318
6.041188	483.317480	8.030336
6.014624	486.518421	8.035354
5.743482	479.807555	8.040371
6.105609	491.616484	8.045389
6.160650	489.701765	8.050406
6.044815	495.403439	8.055424
5.785375	489.003157	8.060442
6.245682	495.021653	8.065459
6.059885	500.497609	8.070477
6.204922	498.051242	8.075494
6.098393	491.122077	8.080512
5.842090	500.452804	8.085530
6.256316	497.579256	8.090547
6.036612	503.571760	8.095565
6.109442	502.613606	8.100582
6.038894	502.343785	8.105600
5.842446	511.175995	8.110618
5.925718	510.269853	8.115635
6.272486	515.409907	8.120653
6.297345	507.415590	8.125670
6.438732	510.347226	8.130688
6.088481	511.875837	8.135706
6.267134	505.223873	8.140723
6.005084	494.428011	8.145741
6.325298	512.510876	8.150758
6.567215	491.064225	8.155776
6.275134	493.328482	8.160794
6.247397	482.852516	8.165811
6.188648	482.486173	8.170829
6.208290	482.148573	8.175846
6.563271	481.332402	8.180864
6.053023	483.031246	8.185882
6.359609	486.924749	8.190899
5.866401	487.446978	8.195917
5.947230	486.938846	8.200934
6.134049	483.608632	8.205952
6.357125	488.521909	8.210970
5.962426	485.371170	8.215987
6.006210	492.512110	8.221005
5.781662	481.915505	8.226022
6.431175	501.127019	8.231040
6.012001	515.308444	8.236058
6.776097	517.075862	8.241075
6.506177	510.270119	8.246093
6.100754	495.451024	8.251110
6.210419	498.375006	8.256128
5.615266	495.555471	8.261146
6.105325	500.177614	8.266163
5.981760	523.477082	8.271181
5.958520	511.697061	8.276198
6.471300	512.326753	8.281216
6.323018	517.762123	8.286234
6.415108	516.097214	8.291251
6.182423	518.569916	8.296269
6.291533	514.055834	8.301286
6.350023	513.576448	8.306304
5.925653	513.153784	8.311322
5.965725	509.985411	8.316339
6.414818	515.999360	8.321357
6.276993	520.388531	8.326374
6.393042	512.039101	8.331392
6.113664	519.663026	8.336410
6.302245	518.790875	8.341427
5.890623	515.731144	8.346445
6.006932	514.125556	8.351462
6.675407	525.113344	8.356480
6.546887	528.623754	8.361498
6.303719	526.209807	8.366515
6.616492	516.661915	8.371533
6.230782	514.974040	8.376550
6.356441	512.401321	8.381568
6.426734	509.464897	8.386586
6.589282	502.121187	8.391603
6.630557	505.093754	8.396621
6.027816	515.097301	8.401638
6.316164	510.387881	8.406656
5.872536	517.501059	8.411674
6.584624	532.486692	8.416691
6.767186	534.894334	8.421709
6.395014	538.174682	8.426726
6.387981	534.360440	8.431744
6.631910	536.878386	8.436762
6.592465	525.675246	8.441779
6.465356	515.041264	8.446797
6.373491	522.582162	8.451814
6.807775	526.597675	8.456832
6.352039	514.768653	8.461850
6.152813	511.211745	8.466867
6.454167	516.595598	8.471885
6.455586	534.545401	8.476902
6.513925	524.327321	8.481920
6.237695	540.395611	8.486938
6.510867	536.982430	8.491955
7.137282	533.816856	8.496973
6.561005	540.666808	8.501990
6.304736	520.872911	8.507008
6.013164	533.229255	8.512026
6.482810	537.662104	8.517043
6.985985	529.731686	8.522061
6.272242	540.402728	8.527078
6.496011	529.401339	8.532096
6.554402	533.179107	8.537114
6.118153	541.771197	8.542131
6.208802	539.784622	8.547149
6.093278	544.649983	8.552166
6.552298	532.519833	8.557184
6.447331	539.131838	8.562202
6.747530	536.358200	8.567219
6.406278	536.765104	8.572237
6.285933	540.589813	8.577255
6.424164	540.861630	8.582272
6.734957	556.850581	8.587290
6.533437	561.511672	8.592307
6.804222	562.873555	8.597325
6.556629	571.660160	8.602343
7.224069	568.055811	8.607360
6.547183	552.225172	8.612378
6.367607	552.095508	8.617395
6.680808	549.168354	8.622413
6.725148	566.947363	8.627431
7.183447	547.076189	8.632448
6.907436	550.527663	8.637466
6.804474	541.164816	8.642483
6.429570	541.576993	8.647501
6.022691	540.141739	8.652519
6.820922	540.723551	8.657536
6.480099	549.887668	8.662554
6.869831	558.830026	8.667571
7.194085	559.009581	8.672589
6.502277	553.582729	8.677607
6.915111	548.367805	8.682624
6.753021	544.243343	8.687642
6.826903	540.328061	8.692659
6.896613	531.935389	8.697677
6.824934	539.908628	8.702695
7.118599	537.599913	8.707712
6.963810	547.287140	8.712730
6.803202	542.976257	8.717747
6.798732	531.044960	8.722765
6.633479	546.063929	8.727783
6.682972	529.396826	8.732800
6.604044	546.740698	8.737818
6.573049	543.633947	8.742835
7.033474	539.806422	8.747853
6.626876	545.282273	8.752871
6.740839	536.832172	8.757888
7.308837	542.612907	8.762906
6.731502	535.555523	8.767923
6.920412	541.717544	8.772941
7.195798	546.269194	8.777959
6.953686	532.983433	8.782976
6.843273	535.743089	8.787994
6.542942	537.629952	8.793011
7.130643	534.552494	8.798029
6.802446	545.595471	8.803047
6.900864	537.258259	8.808064
6.988985	539.901603	8.813082
6.994177	535.990772	8.818099
6.896983	533.250998	8.823117
6.978379	546.139043	8.828135
6.946369	532.031419	8.833152
6.731972	537.448752	8.838170
7.054180	544.069565	8.843187
7.037412	540.711279	8.848205
6.767855	548.131708	8.853223
6.692994	553.710217	8.858240
6.661728	538.327538	8.863258
6.634859	537.009466	8.868275
7.081257	540.941035	8.873293
6.938357	535.396626	8.878311
6.728586	534.552176	8.883328
6.973695	537.915685	8.888346
7.127230	540.693946	8.893363
7.001878	536.159791	8.898381
6.890361	538.351582	8.903399
6.548606	548.737128	8.908416
7.000581	550.057997	8.913434
6.979630	554.637146	8.918451
7.130200	556.295572	8.923469
6.869400	554.534474	8.928487
7.071533	568.646995	8.933504
6.976992	565.730076	8.938522
6.990044	563.190773	8.943539
7.331533	558.170059	8.948557
6.680704	566.495983	8.953575
6.831465	565.847505	8.958592
7.013255	568.731795	8.963610
6.870741	576.088148	8.968627
6.828877	572.929447	8.973645
7.079140	576.453101	8.978663
6.877361	568.813001	8.983680
7.525465	562.649188	8.988698
7.140254	576.837963	8.993715
7.191627	568.801595	8.998733
7.153944	583.983643	9.003751
7.493366	570.493129	9.008768
7.168108	577.363724	9.013786
7.062454	571.248583	9.018803
6.990014	568.353447	9.023821
6.740482	581.015660	9.028839
6.948304	570.291297	9.033856
7.042148	571.314834	9.038874
6.904690	573.046793	9.043891
7.366833	562.793823	9.048909
6.613387	567.623444	9.053927
7.276912	570.141922	9.058944
7.401846	571.583462	9.063962
7.005900	572.418655	9.068979
7.314904	559.513580	9.073997
7.494450	573.935754	9.079015
7.311175	566.674604	9.084032
7.225914	571.475271	9.089050
6.982971	580.573574	9.094067
6.859906	582.360083	9.099085
7.253578	577.230203	9.104103
6.646233	572.295036	9.109120
7.226505	571.686558	9.114138
6.973226	579.025554	9.119155
7.273341	590.307781	9.124173
7.222490	599.139313	9.129191
6.906904	600.984391	9.134208
7.143094	596.974237	9.139226
7.288666	605.210110	9.144243
7.242691	593.395727	9.149261
7.104473	601.559299	9.154279
6.896939	601.156306	9.159296
7.731057	597.484810	9.164314
7.564938	602.698939	9.169331
7.313294	600.355737	9.174349
7.576012	598.626216	9.179367
7.546716	603.231931	9.184384
7.497734	603.839194	9.189402
7.095381	600.396145	9.194419
7.526638	597.649301	9.199437
7.433489	605.834215	9.204455
7.475649	605.755014	9.209472
7.363441	598.432225	9.214490
7.077661	599.843445	9.219507
7.254475	607.550563	9.224525
7.573210	604.455276	9.229543
6.943015	608.899525	9.234560
7.500603	596.189002	9.239578
7.291102	600.573645	9.244595
7.528824	599.911540	9.249613
7.321437	595.794165	9.254631
7.475407	605.180583	9.259648
7.493539	596.328906	9.264666
7.411641	600.598881	9.269683
7.513188	600.317873	9.274701
7.514045	606.572496	9.279719
7.359760	610.339422	9.284736
7.360817	599.530675	9.289754
7.661831	607.521288	9.294771
7.747873	606.845080	9.299789
7.508054	605.206921	9.304807
7.276621	603.463307	9.309824
7.246908	601.426157	9.314842
7.186647	599.381171	9.319859
7.520243	606.514616	9.324877
7.062988	605.838327	9.329895
7.101090	599.561798	9.334912
7.407803	602.136188	9.339930
7.551709	618.618399	9.344947
7.723058	630.848630	9.349965
7.670975	622.916809	9.354983
7.677105	607.089557	9.360000
7.511457	604.524598	9.365018
7.216035	614.536852	9.370035
7.197361	611.784763	9.375053
7.637128	618.724854	9.380071
7.522386	630.570723	9.385088
7.809936	620.837380	9.390106
7.722731	634.225274	9.395123
7.942855	634.575779	9.400141
7.592162	628.224458	9.405159
7.707724	620.424161	9.410176
7.422483	608.363236	9.415194
7.534502	613.417025	9.420211
8.139251	621.328496	9.425229
7.881122	602.901256	9.430247
7.812544	600.611421	9.435264
7.866664	605.667967	9.440282
7.798597	605.135825	9.445299
7.463975	595.269608	9.450317
7.538010	609.206572	9.455335
7.440557	605.488533	9.460352
7.720323	600.000955	9.465370
7.565781	599.580192	9.470387
7.685717	609.950239	9.475405
7.851692	611.565232	9.480423
7.462504	617.041533	9.485440
7.904815	612.699280	9.490458
8.033786	622.518812	9.495475
8.007696	613.446838	9.500493
7.766798	605.421533	9.505511
7.698523	597.826774	9.510528
7.844716	598.198329	9.515546
7.322866	610.063791	9.520563
7.669542	613.897392	9.525581
7.945431	630.904887	9.530599
7.363566	623.930228	9.535616
8.032375	622.080273	9.540634
8.052815	628.909346	9.545651
7.779368	631.502058	9.550669
7.903395	637.109391	9.555687
7.773990	620.381871	9.560704
8.133695	613.969740	9.565722
7.782383	612.058717	9.570739
7.706018	612.099073	9.575757
7.685455	617.397697	9.580775
7.365959	622.572747	9.585792
7.923110	624.413627	9.590810
7.688802	634.400537	9.595827
7.570152	631.414802	9.600845
7.996486	617.153246	9.605863
7.687342	624.696673	9.610880
7.683182	624.321774	9.615898
7.448555	632.598295	9.620915
7.780219	633.126983	9.625933
7.963823	621.062017	9.630951
8.109215	622.181621	9.635968
7.903103	622.349603	9.640986
8.277202	627.314994	9.646003
7.439933	632.927779	9.651021
7.959435	625.035786	9.656039
7.860903	634.370265	9.661056
7.577730	632.274995	9.666074
7.870113	650.264531	9.671091
8.169377	653.853106	9.676109
8.112442	655.837543	9.681127
7.847737	666.798063	9.686144
7.927418	660.256222	9.691162
8.237288	661.432108	9.696179
8.591129	652.221691	9.701197
8.429314	636.221912	9.706215
7.495081	638.353273	9.711232
7.921923	636.534917	9.716250
7.897867	642.837638	9.721267
8.294181	659.346610	9.726285
8.468774	649.280657	9.731303
8.308836	638.071079	9.736320
8.022009	615.722516	9.741338
8.406804	621.087016	9.746355
8.268643	625.930699	9.751373
7.868721	623.178383	9.756391
7.685783	632.759615	9.761408
8.214599	624.828294	9.766426
8.111239	633.993116	9.771443
7.789764	633.510145	9.776461
8.127706	625.116427	9.781479
7.938963	630.072178	9.786496
8.030778	636.009604	9.791514
8.203046	654.948924	9.796531
8.080149	652.765423	9.801549
8.374363	651.927208	9.806567
8.149473	661.663350	9.811584
7.994122	649.399010	9.816602
8.139516	655.643627	9.821619
8.141754	659.136731	9.826637
8.200692	644.516153	9.831655
8.328013	657.422329	9.836672
8.373807	656.058150	9.841690
8.173474	662.401120	9.846707
8.059367	663.147976	9.851725
8.081667	649.164295	9.856743
8.467034	664.923909	9.861760
8.247651	663.860053	9.866778
8.410220	653.698151	9.871795
8.295785	653.179584	9.876813
8.273220	658.850918	9.881831
8.472832	662.625521	9.886848
8.132969	654.480002	9.891866
8.027852	655.834517	9.896883
8.286682	660.174197	9.901901
8.671144	657.447298	9.906919
7.859904	654.582700	9.911936
8.034386	645.804330	9.916954
8.362658	656.539392	9.921971
8.024743	657.103565	9.926989
8.401018	658.142814	9.932007
8.584638	654.592164	9.937024
8.309707	664.639105	9.942042
8.392639	660.996932	9.947059
8.000693	658.527383	9.952077
8.205822	651.268459	9.957095
8.442369	658.085773	9.962112
8.736330	647.710784	9.967130
8.943331	659.143344	9.972147
8.321282	654.122095	9.977165
8.413591	650.740387	9.982183
8.444598	655.021087	9.987200
8.638721	656.742126	9.992218
8.094612	656.505477	9.997235
8.166169	655.102547	10.002253
8.431749	654.060536	10.007271
8.590838	660.047390	10.012288
8.413290	655.429865	10.017306
8.242576	661.929140	10.022323
8.187855	664.399224	10.027341
8.556970	669.933452	10.032359
8.436380	672.536934	10.037376
8.459708	677.219629	10.042394
8.538644	678.365428	10.047411
8.113766	684.289153	10.052429
8.877242	679.836603	10.057447
8.658320	694.087779	10.062464
8.558042	688.113766	10.067482
8.782500	677.235255	10.072499
8.654713	684.406309	10.077517
8.759071	676.153307	10.082535
8.900060	663.220834	10.087552
8.338058	661.166093	10.092570
8.352596	666.124716	10.097587
7.975011	667.193721	10.102605
8.232153	672.559303	10.107623
8.745702	687.901222	10.112640
8.719954	687.545483	10.117658
8.864008	681.728850	10.122675
8.587688	683.656146	10.127693
8.620881	677.582330	10.132711
8.754814	681.966830	10.137728
8.634354	686.874028	10.142746
8.274505	680.243257	10.147763
8.446606	682.425340	10.152781
8.832352	677.770044	10.157799
8.446361	684.968931	10.162816
8.408263	671.925656	10.167834
8.738361	685.844650	10.172851
8.416762	684.541189	10.177869
8.770365	677.088578	10.182887
8.648491	687.386104	10.187904
8.691320	700.712648	10.192922
8.837228	707.209667	10.197939
8.995011	706.408606	10.202957
9.051954	704.537747	10.207975
8.923741	683.716903	10.212992
8.579935	691.789652	10.218010
8.906050	679.064846	10.223027
8.525995	693.830417	10.228045
8.539635	696.741075	10.233063
8.799987	696.327885	10.238080
8.836319	695.940329	10.243098
9.497998	704.303665	10.248115
8.903450	699.183421	10.253133
8.854034	699.162749	10.258151
9.021096	687.068773	10.263168
8.574713	696.262127	10.268186
8.682109	682.574354	10.273203
8.521628	702.361122	10.278221
8.608665	705.465408	10.283239
8.733486	718.671821	10.288256
8.153880	716.146460	10.293274
9.051712	709.826705	10.298291
8.708043	711.641480	10.303309
9.143956	708.351091	10.308327
9.111927	718.634558	10.313344
8.927912	702.167983	10.318362
9.041680	696.889421	10.323379
9.002430	714.564910	10.328397
9.484311	703.942694	10.333415
9.752068	709.660073	10.338432
9.646259	705.987504	10.343450
8.814082	691.790533	10.348467
8.750803	689.585063	10.353485
8.881691	695.358596	10.358503
8.849529	708.472834	10.363520
8.613295	703.722480	10.368538
9.252200	709.773027	10.373555
9.005364	712.124896	10.378573
8.995902	708.468788	10.383591
8.873504	710.201557	10.388608
8.978785	709.503395	10.393626
9.463151	706.088649	10.398643
9.010131	704.840492	10.403661
9.339992	703.640084	10.408679
9.211387	713.727241	10.413696
9.344000	710.923031	10.418714
9.168509	706.677555	10.423731
9.322906	709.017050	10.428749
9.066866	700.293487	10.433767
9.207386	711.158984	10.438784
9.089291	722.017672	10.443802
9.368862	704.960905	10.448819
9.524198	713.113247	10.453837
9.224334	700.596959	10.458855
9.196446	689.780069	10.463872
9.059378	689.233489	10.468890
9.007829	676.599417	10.473907
9.157340	701.743499	10.478925
9.178585	711.662009	10.483943
9.393378	706.228760	10.488960
9.277111	717.491102	10.493978
9.847914	702.720848	10.498995
9.245742	696.396282	10.504013
9.180352	683.884293	10.509031
9.421876	682.246448	10.514048
9.135964	678.359107	10.519066
9.086335	674.706144	10.524083
9.232147	683.746743	10.529101
9.238488	676.471619	10.534119
9.506371	687.916748	10.539136
9.282054	688.172790	10.544154
9.372304	686.132613	10.549171
9.539146	684.093059	10.554189
9.353169	686.504817	10.559207
9.339445	683.893952	10.564224
9.123940	682.548621	10.569242
9.757188	688.382297	10.574259
9.375908	690.212430	10.579277
9.340427	687.317796	10.584295
9.812516	677.053736	10.589312
9.247981	687.108195	10.594330
9.157742	678.361820	10.599347
9.026723	682.380736	10.604365
9.415682	697.155206	10.609383
9.591469	692.819980	10.614400
9.333555	709.422038	10.619418
9.931576	697.260531	10.624435
9.909935	700.656399	10.629453
9.490190	688.401900	10.634471
9.940272	678.781915	10.639488
9.236919	678.478697	10.644506
9.539551	669.992661	10.649523
9.638081	679.807526	10.654541
9.466951	681.153453	10.659559
9.829342	672.793751	10.664576
9.742183	679.462977	10.669594
9.910523	675.924184	10.674611
9.227760	676.955800	10.679629
9.407116	677.233798	10.684647
9.669286	675.965103	10.689664
9.566691	676.975243	10.694682
9.929517	677.145600	10.699699
9.447191	678.316224	10.704717
9.294352	676.837999	10.709735
9.570544	681.493699	10.714752
9.268986	679.843116	10.719770
9.262259	670.288398	10.724787
9.417465	679.769335	10.729805
9.477798	695.475762	10.734823
9.418582	693.048749	10.739840
9.776406	699.162267	10.744858
9.761638	704.194921	10.749875
9.789450	700.551910	10.754893
9.765345	706.737896	10.759911
9.852444	701.387772	10.764928
9.804182	711.449717	10.769946
9.832068	686.508176	10.774963
9.464027	684.719686	10.779981
9.625144	692.634428	10.784999
9.610004	703.536933	10.790016
10.023897	708.183688	10.795034
10.068464	700.514400	10.800051
9.791353	682.869535	10.805069
9.481559	677.821446	10.810087
10.067928	687.253766	10.815104
9.270778	696.148629	10.820122
9.744751	694.935109	10.825139
9.724579	699.025023	10.830157
9.846466	705.708842	10.835175
9.847877	704.660882	10.840192
9.846250	710.117512	10.845210
9.724432	694.878274	10.850227
9.580876	704.529113	10.855245
9.547822	703.189907	10.860263
9.760104	704.273789	10.865280
9.381957	712.443446	10.870298
9.772551	704.508501	10.875315
9.749323	702.530284	10.880333
9.663772	707.267916	10.885351
9.812796	709.885964	10.890368
10.140355	724.401833	10.895386
9.938621	721.151390	10.900403
9.870753	713.168354	10.905421
9.705818	719.641497	10.910439
10.080388	722.817500	10.915456
10.176259	732.610720	10.920474
9.832668	722.086273	10.925491
10.062495	731.451405	10.930509
9.933676	731.711418	10.935527
10.103189	731.167294	10.940544
10.037198	737.375633	10.945562
10.032433	733.725095	10.950579
10.443520	737.362439	10.955597
9.828403	721.458854	10.960615
10.184658	712.124951	10.965632
9.712306	725.822569	10.970650
9.986180	723.791486	10.975667
10.282909	729.251868	10.980685
10.045123	722.261129	10.985703
10.449555	722.115698	10.990720
10.399625	724.831193	10.995738
9.658989	712.349245	11.000755
9.780509	715.495467	11.005773
10.107751	727.013372	11.010791
10.026707	728.076943	11.015808
9.738844	723.817512	11.020826
9.925270	729.184723	11.025843
10.141136	730.795065	11.030861
10.304530	734.370231	11.035879
10.313146	718.485686	11.040896
10.308704	731.280016	11.045914
9.683140	722.383966	11.050931
10.322639	728.964602	11.055949
10.418878	725.415005	11.060967
10.755950	721.549964	11.065984
10.089172	729.061107	11.071002
10.266892	727.057714	11.076019
10.483053	719.531945	11.081037
9.880275	723.817292	11.086055
10.315402	734.280037	11.091072
9.731599	728.817273	11.096090
9.936686	731.259282	11.101107
10.380263	734.011063	11.106125
10.309060	734.833251	11.111143
10.405068	723.842293	11.116160
9.878652	728.159857	11.121178
10.305039	741.789252	11.126195
10.411127	747.812842	11.131213
10.277443	766.560376	11.136231
10.488078	752.780634	11.141248
10.331489	756.661561	11.146266
10.863141	753.327761	11.151283
10.729971	742.205442	11.156301
10.202581	729.882574	11.161319
10.439686	721.488832	11.166336
10.290396	728.290887	11.171354
10.515281	732.800005	11.176371
11.056493	735.558579	11.181389
10.635603	732.213084	11.186407
10.568338	719.177500	11.191424
10.248096	738.440229	11.196442
10.632908	723.484504	11.201459
10.267246	720.139825	11.206477
10.318114	726.146813	11.211495
10.462241	722.110031	11.216512
10.271425	728.000253	11.221530
10.120017	733.272075	11.226547
10.875962	745.606449	11.231565
10.526139	744.553558	11.236583
11.057883	751.078502	11.241600
10.850850	741.545663	11.246618
10.546319	732.378401	11.251635
10.657434	727.491566	11.256653
10.501266	723.694339	11.261671
10.386025	728.417694	11.266688
10.558944	736.229620	11.271706
10.343079	748.848806	11.276723
10.503654	746.526203	11.281741
10.618660	754.369302	11.286759
10.980092	740.666928	11.291776
10.549988	755.964257	11.296794
10.369058	751.697532	11.301811
10.900706	751.150315	11.306829
10.486650	749.731947	11.311847
10.546623	743.511901	11.316864
10.664612	757.994362	11.321882
10.408696	755.001711	11.326899
10.454695	745.321926	11.331917
10.769437	752.360555	11.336935
10.871597	750.643553	11.341952
10.895073	756.314015	11.346970
10.836183	764.130716	11.351987
11.195830	755.922885	11.357005
10.788820	758.571256	11.362023
10.813535	751.081783	11.367040
11.174340	752.735690	11.372058
10.972909	757.422064	11.377075
11.238889	749.393014	11.382093
10.873152	748.547745	11.387111
10.681100	742.809001	11.392128
11.036551	747.692141	11.397146
10.715599	752.135309	11.402163
11.035469	742.295850	11.407181
10.530473	756.112214	11.412199
10.970287	751.224364	11.417216
10.721524	757.212038	11.422234
10.623530	754.358745	11.427251
11.168757	746.522630	11.432269
10.678497	749.455444	11.437287
10.657287	746.646927	11.442304
10.615570	746.183236	11.447322
10.834017	747.332426	11.452339
10.512924	761.886843	11.457357
10.992215	779.954522	11.462375
10.979613	777.447610	11.467392
11.454572	784.953455	11.472410
11.175441	784.804674	11.477427
11.548461	776.771464	11.482445
11.170347	761.793234	11.487463
11.338638	750.661545	11.492480
10.816160	755.858970	11.497498
10.906850	749.520500	11.502515
11.207898	752.540769	11.507533
11.077335	745.817243	11.512551
11.059742	745.816832	11.517568
10.932672	746.849746	11.522586
10.935242	778.095054	11.527603
11.340722	775.216521	11.532621
11.366291	776.487453	11.537639
11.302094	768.854113	11.542656
11.166891	755.813368	11.547674
10.791959	757.333243	11.552691
11.487546	768.610425	11.557709
11.058076	777.936870	11.562727
11.352190	777.947581	11.567744
11.379124	772.430137	11.572762
10.971456	770.199721	11.577779
11.219875	767.595108	11.582797
11.011729	782.292791	11.587815
10.815168	781.086496	11.592832
11.267232	778.191197	11.597850
11.394894	771.405111	11.602867
11.260517	776.368163	11.607885
11.007004	778.822073	11.612903
10.753492	773.370661	11.617920
11.361428	792.450148	11.622938
10.980807	777.999319	11.627955
11.177493	769.473031	11.632973
11.511123	781.040464	11.637991
11.600007	782.374060	11.643008
11.502039	783.314053	11.648026
11.315419	783.374840	11.653043
11.701808	771.893384	11.658061
11.470500	782.492135	11.663079
11.077634	775.014431	11.668096
11.090719	768.565036	11.673114
10.897405	785.220159	11.678131
11.055663	800.349599	11.683149
11.034792	813.528417	11.688167
11.176272	811.581185	11.693184
11.344827	806.331877	11.698202
11.541812	803.403956	11.703219
11.309043	800.262503	11.708237
11.479198	807.838207	11.713255
11.483380	810.434782	11.718272
11.611719	799.732203	11.723290
11.364898	812.088039	11.728307
11.206543	812.235916	11.733325
11.240240	834.640142	11.738343
11.340794	827.375441	11.743360
11.484028	833.885549	11.748378
11.274692	839.213816	11.753395
11.710739	828.188450	11.758413
11.736322	838.191558	11.763431
11.885500	839.222220	11.768448
12.391998	829.160966	11.773466
11.827870	841.806382	11.778483
11.748873	828.946127	11.783501
12.142395	825.630800	11.788519
11.686524	814.688387	11.793536
11.815983	812.642052	11.798554
11.587927	807.123524	11.803571
11.642962	807.361044	11.808589
12.036560	810.303706	11.813607
11.863838	809.702748	11.818624
11.850620	802.661011	11.823642
11.739556	804.795958	11.828659
11.394050	801.299782	11.833677
11.586108	809.509530	11.838695
12.001691	818.261775	11.843712
12.185855	805.297188	11.848730
11.916085	813.557208	11.853747
11.778218	801.570892	11.858765
11.774341	804.904036	11.863783
11.993497	797.800646	11.868800
11.919866	803.265431	11.873818
11.873215	818.221863	11.878835
12.036743	805.295223	11.883853
11.654216	809.823792	11.888871
12.137180	812.859750	11.893888
11.532791	807.109852	11.898906
11.532259	815.501258	11.903923
11.599229	821.139679	11.908941
12.077461	819.751913	11.913959
11.797057	828.341812	11.918976
11.851614	824.622001	11.923994
11.552455	831.838900	11.929011
11.720451	822.367178	11.934029
11.882999	832.765392	11.939047
11.990564	833.486991	11.944064
11.808859	827.348964	11.949082
11.972801	841.155257	11.954099
11.932622	831.845537	11.959117
12.046467	820.005963	11.964135
11.940887	835.741665	11.969152
12.421736	825.917964	11.974170
11.860376	830.461934	11.979187
12.304817	829.997808	11.984205
12.353117	831.741712	11.989223
12.148043	824.698470	11.994240
12.071539	826.720706	11.999258
12.197688	830.225987	12.004275
12.317076	820.976479	12.009293
12.553749	821.355953	12.014311
12.456032	832.902641	12.019328
12.488222	823.496379	12.024346
12.360465	833.163746	12.029363
12.041788	823.866108	12.034381
12.235109	821.645663	12.039399
12.233384	829.219904	12.044416
12.014424	823.668388	12.049434
12.180935	829.774057	12.054451
12.390445	821.239423	12.059469
12.100796	824.816164	12.064487
12.067815	834.654875	12.069504
12.159931	820.338226	12.074522
12.517365	823.826203	12.079539
12.484190	829.350929	12.084557
12.040865	821.729631	12.089575
12.116713	827.770609	12.094592
12.541578	838.260270	12.099610
12.250835	842.102275	12.104627
12.429222	840.266023	12.109645
12.579942	834.795437	12.114663
12.306534	841.569645	12.119680
12.465616	831.553357	12.124698
12.448826	834.860127	12.129715
12.073548	832.154411	12.134733
12.614030	839.372300	12.139751
12.687373	850.639731	12.144768
12.479476	844.325919	12.149786
12.443293	834.715768	12.154803
12.388604	855.281398	12.159821
12.219161	844.701189	12.164839
12.002829	851.627406	12.169856
12.753004	852.658577	12.174874
12.920877	853.689466	12.179891
12.429146	849.512440	12.184909
12.965749	841.844894	12.189927
12.827347	842.036982	12.194944
12.966302	842.150899	12.199962
12.747015	845.158037	12.204979
12.571882	830.788578	12.209997
12.789289	825.903998	12.215015
12.052774	829.301444	12.220032
12.596522	839.602065	12.225050
12.744252	844.385234	12.230067
12.776773	850.767526	12.235085
12.702823	842.128973	12.240103
12.801408	859.741983	12.245120
12.611849	843.244588	12.250138
12.700464	845.973107	12.255155
12.974920	852.617297	12.260173
12.785664	852.391316	12.265191
12.546652	853.400750	12.270208
12.518616	841.810612	12.275226
13.024116	858.533037	12.280243
12.453207	853.330149	12.285261
12.697189	846.355394	12.290279
12.675547	859.367108	12.295296
12.677488	854.696162	12.300314
12.935343	855.656147	12.305331
12.499667	852.177244	12.310349
12.791953	844.311290	12.315367
12.325861	850.175255	12.320384
12.516771	854.699194	12.325402
12.906381	871.603893	12.330419
12.997315	880.164037	12.335437
13.053607	872.120450	12.340455
12.681040	880.652229	12.345472
12.859394	870.550848	12.350490
12.847753	879.370063	12.355507
12.451534	879.659352	12.360525
12.850140	879.852508	12.365543
12.879059	874.852279	12.370560
13.074210	875.809466	12.375578
13.098387	884.777707	12.380595
13.010409	885.605686	12.385613
13.083446	888.298783	12.390631
13.123218	885.733156	12.395648
12.991655	880.792784	12.400666
13.117117	875.632259	12.405683
12.793574	877.346066	12.410701
13.118734	874.451700	12.415719
12.771088	880.145636	12.420736
13.197683	873.716621	12.425754
12.931536	878.359517	12.430771
12.962318	888.219826	12.435789
13.542643	892.244099	12.440807
13.037524	897.748117	12.445824
13.315525	893.456789	12.450842
13.346635	887.064488	12.455859
13.117877	885.938971	12.460877
13.255808	881.906280	12.465895
13.381095	886.068121	12.470912
13.141904	884.442461	12.475930
13.259953	893.253985	12.480947
13.313376	897.998295	12.485965
13.366482	886.925596	12.490983
13.074469	896.937473	12.496000
13.588347	899.469980	12.501018
13.348025	890.705990	12.506035
13.289549	898.547931	12.511053
13.134349	899.859818	12.516071
13.107760	908.877051	12.521088
13.350770	911.328922	12.526106
13.407838	913.696318	12.531123
13.334972	908.443780	12.536141
13.387507	908.981498	12.541159
13.097745	910.005197	12.546176
13.289494	910.502167	12.551194
13.303053	912.292549	12.556211
13.501318	919.627207	12.561229
13.643427	909.588288	12.566247
13.491609	912.468100	12.571264
13.648762	905.244993	12.576282
13.293489	912.303457	12.581299
13.064304	913.525951	12.586317
13.231235	908.538802	12.591335
13.176574	910.885833	12.596352
13.745235	926.061531	12.601370
13.977573	932.765999	12.606387
13.669482	927.929013	12.611405
13.524153	916.549711	12.616423
13.294132	921.366841	12.621440
13.309419	933.160979	12.626458
13.537256	935.832984	12.631475
13.140682	936.614641	12.636493
14.005906	947.701254	12.641511
13.434684	947.604548	12.646528
13.693805	943.899998	12.651546
13.767189	943.333059	12.656563
13.318621	936.151197	12.661581
13.603218	938.325153	12.666599
13.552583	941.167025	12.671616
13.803310	941.216092	12.676634
13.812177	929.743193	12.681651
13.728155	936.973764	12.686669
13.594203	940.229482	12.691687
13.665889	936.863575	12.696704
13.746107	931.817421	12.701722
13.774685	939.248103	12.706739
13.976447	958.391409	12.711757
14.002542	957.970737	12.716775
14.029206	953.633567	12.721792
13.836444	949.523285	12.726810
13.419948	942.718252	12.731827
14.012433	964.728971	12.736845
13.930368	967.831396	12.741863
14.042978	972.351854	12.746880
14.124177	962.565450	12.751898
13.884639	964.622714	12.756915
13.947785	961.460114	12.761933
13.971529	955.485515	12.766951
14.174703	967.531107	12.771968
13.557731	963.004443	12.776986
14.056521	963.667905	12.782003
13.869234	968.049156	12.787021
13.898112	952.874450	12.792039
14.261845	968.341072	12.797056
14.316641	963.930063	12.802074
14.117435	962.878807	12.807091
14.187293	968.510511	12.812109
14.389556	957.597437	12.817127
14.311689	961.917360	12.822144
14.348288	970.612295	12.827162
14.524334	963.846958	12.832179
14.143594	950.478464	12.837197
13.940732	942.210359	12.842215
14.279397	946.708016	12.847232
13.989799	960.645424	12.852250
14.271523	951.689154	12.857267
14.294570	954.800353	12.862285
14.317954	955.954874	12.867303
14.277282	961.518686	12.872320
14.479983	961.266005	12.877338
14.843119	960.622108	12.882355
13.760074	948.382994	12.887373
14.355049	951.742258	12.892391
14.404923	960.166860	12.897408
13.859511	957.800210	12.902426
14.384289	971.013573	12.907443
14.253047	966.925206	12.912461
14.407673	971.164522	12.917479
14.307616	964.742252	12.922496
14.292323	965.268507	12.927514
14.878957	955.828953	12.932531
14.404330	963.155450	12.937549
14.402611	962.385680	12.942567
14.434154	961.752712	12.947584
14.277063	965.135139	12.952602
14.663779	958.352575	12.957619
14.482113	967.514058	12.962637
14.411251	958.464703	12.967655
14.536076	963.339856	12.972672
14.163404	966.522528	12.977690
14.579487	964.245072	12.982707
14.398283	966.927522	12.987725
14.499755	961.890654	12.992743
14.434734	963.806963	12.997760
14.532728	957.820730	13.002778
14.576251	964.633691	13.007795
14.777381	986.323897	13.012813
14.676197	981.729037	13.017831
14.622759	986.543763	13.022848
14.946910	996.569608	13.027866
15.059524	978.437348	13.032883
14.680183	980.213556	13.037901
14.685537	961.665766	13.042919
14.422691	966.538545	13.047936
14.541089	986.190411	13.052954
14.926797	990.396681	13.057971
14.750359	995.511553	13.062989
14.783456	988.778072	13.068007
14.790362	988.918992	13.073024
14.885440	991.756976	13.078042
14.880946	990.555288	13.083059
14.461079	990.273918	13.088077
14.536403	989.245919	13.093095
14.643494	984.722568	13.098112
14.396410	992.256425	13.103130
14.599302	989.270743	13.108147
14.394063	996.012238	13.113165
14.392339	1000.594800	13.118183
14.713300	1016.999143	13.123200
15.074460	1028.641320	13.128218
15.178736	1019.706507	13.133235
15.393378	1011.597020	13.138253
15.019311	1020.343700	13.143271
15.418829	1024.279566	13.148288
14.884716	1023.880394	13.153306
14.906408	1012.822006	13.158323
15.177715	1026.198203	13.163341
15.135000	1014.480863	13.168359
15.726396	1010.478081	13.173376
14.879156	1005.627717	13.178394
15.060557	1005.245827	13.183411
15.111210	1016.172929	13.188429
15.430047	1014.182107	13.193447
15.247872	1005.771874	13.198464
14.605623	1007.137991	13.203482
14.966345	1008.545778	13.208499
14.748433	1022.898044	13.213517
14.750200	1017.292948	13.218535
15.453339	1012.856083	13.223552
15.485893	1015.754361	13.228570
15.337250	1017.623817	13.233587
15.081676	1017.992059	13.238605
15.532794	1021.496955	13.243623
15.276696	1015.222193	13.248640
15.187078	1018.685578	13.253658
15.355214	1018.129038	13.258675
15.477338	1011.955966	13.263693
15.139833	1024.064220	13.268711
15.450090	1020.219096	13.273728
15.548548	1018.433220	13.278746
15.293153	1019.726101	13.283763
14.998238	1019.298919	13.288781
15.281063	1024.379711	13.293799
15.111501	1021.938383	13.298816
15.800585	1046.682823	13.303834
15.414116	1040.491597	13.308851
15.686953	1050.380343	13.313869
15.664060	1044.315190	13.318887
15.816380	1028.385762	13.323904
15.477655	1023.064391	13.328922
15.540856	1012.741127	13.333939
15.530576	1023.324324	13.338957
15.257296	1026.415693	13.343975
15.292595	1026.602658	13.348992
15.610350	1041.517960	13.354010
15.760910	1041.715269	13.359027
15.914051	1043.158740	13.364045
15.713250	1041.448153	13.369063
16.050766	1047.609156	13.374080
15.839282	1045.471045	13.379098
15.814775	1031.737400	13.384115
15.560067	1030.158339	13.389133
15.364060	1043.431040	13.394151
15.493017	1039.188277	13.399168
15.547325	1051.777968	13.404186
15.596436	1039.083686	13.409203
15.820338	1041.724765	13.414221
15.638930	1044.173725	13.419239
15.642967	1039.369855	13.424256
15.775635	1045.225276	13.429274
15.657807	1045.073309	13.434291
15.258579	1046.240402	13.439309
15.463306	1062.233802	13.444327
15.902520	1058.996483	13.449344
15.856415	1075.423678	13.454362
15.950588	1069.816711	13.459379
15.635755	1073.757215	13.464397
15.476771	1073.873634	13.469415
15.879794	1072.084215	13.474432
15.676872	1070.556998	13.479450
15.790451	1080.833638	13.484467
15.796916	1080.573832	13.489485
16.158500	1074.492610	13.494503
16.462176	1074.624903	13.499520
16.331930	1074.951418	13.504538
16.202689	1071.771604	13.509555
16.140429	1078.847340	13.514573
16.154628	1077.008387	13.519591
16.467611	1071.771087	13.524608
16.261651	1073.968272	13.529626
16.054846	1073.795532	13.534643
15.953767	1067.278708	13.539661
15.897075	1076.464847	13.544679
15.927213	1065.181037	13.549696
16.153398	1074.581634	13.554714
16.250527	1071.183312	13.559731
15.660048	1074.759898	13.564749
15.738978	1087.247925	13.569767
16.283473	1097.785268	13.574784
15.834267	1099.556656	13.579802
15.876987	1101.992597	13.584819
16.142200	1103.629957	13.589837
16.148523	1095.322694	13.594855
16.423037	1099.937740	13.599872
16.403629	1103.352270	13.604890
16.032963	1101.232782	13.609907
16.780547	1099.360971	13.614925
16.366786	1095.190605	13.619943
16.582164	1096.936760	13.624960
16.315085	1100.655189	13.629978
16.848211	1103.809573	13.634995
16.819258	1098.966675	13.640013
16.356287	1102.412832	13.645031
16.749364	1099.794974	13.650048
16.827693	1100.025692	13.655066
16.530589	1106.106264	13.660083
16.471789	1101.776137	13.665101
16.398954	1103.507489	13.670119
16.971205	1097.636254	13.675136
16.506298	1097.049507	13.680154
16.202953	1093.180586	13.685171
16.374953	1096.006534	13.690189
16.431279	1095.161391	13.695207
16.647466	1109.603504	13.700224
16.928849	1115.864845	13.705242
16.878413	1118.520517	13.710259
16.708701	1104.411927	13.715277
16.519397	1101.711744	13.720295
17.206564	1103.166223	13.725312
16.930696	1097.967528	13.730330
16.599981	1091.152153	13.735347
16.796161	1096.041410	13.740365
16.912288	1098.658358	13.745383
16.846637	1090.081501	13.750400
17.127535	1094.108554	13.755418
16.841195	1089.773055	13.760435
17.092767	1091.560877	13.765453
16.607457	1092.252300	13.770471
16.875607	1091.437085	13.775488
16.823343	1097.962141	13.780506
16.776893	1096.918501	13.785523
16.954445	1102.315618	13.790541
16.674803	1124.964966	13.795559
16.949450	1115.214442	13.800576
17.132541	1119.146369	13.805594
17.140372	1122.566102	13.810611
17.202071	1113.325482	13.815629
17.426356	1130.587697	13.820647
17.567243	1101.206486	13.825664
16.939601	1105.391673	13.830682
17.032707	1097.645180	13.835699
16.986852	1081.311246	13.840717
17.095719	1091.184679	13.845735
16.918886	1087.258066	13.850752
17.296106	1108.024563	13.855770
17.057846	1110.507686	13.860787
17.300856	1107.200111	13.865805
17.043879	1122.975566	13.870823
17.548325	1123.029063	13.875840
17.198746	1124.668076	13.880858
17.163696	1126.677539	13.885875
17.602378	1123.869491	13.890893
17.512075	1124.855639	13.895911
16.947780	1094.859076	13.900928
17.186454	1110.477963	13.905946
17.061569	1120.378569	13.910963
17.303249	1119.090963	13.915981
17.192051	1128.749583	13.920999
17.529323	1115.107516	13.926016
17.278949	1118.318390	13.931034
16.853886	1120.297440	13.936051
17.362972	1121.539976	13.941069
17.483470	1125.885665	13.946087
17.357987	1127.366486	13.951104
17.523985	1125.746746	13.956122
17.188454	1130.911831	13.961139
17.546968	1120.718964	13.966157
16.881746	1128.062766	13.971175
17.363539	1140.304667	13.976192
17.853205	1143.639441	13.981210
17.642716	1149.122619	13.986227
17.854933	1145.655756	13.991245
17.627205	1150.362132	13.996263
17.616700	1147.722292	14.001280
17.815494	1148.880901	14.006298
17.439647	1155.623939	14.011315
18.099536	1155.021905	14.016333
17.542782	1150.747695	14.021351
17.736462	1145.895149	14.026368
18.190401	1150.608331	14.031386
17.553107	1150.802849	14.036403
17.729431	1144.343521	14.041421
17.497716	1151.256484	14.046439
17.883704	1141.882985	14.051456
18.129827	1145.596754	14.056474
17.780334	1147.488226	14.061491
17.835693	1134.903352	14.066509
17.809096	1147.994949	14.071527
17.796808	1145.074515	14.076544
18.233361	1137.769667	14.081562
17.506014	1142.017822	14.086579
17.703006	1149.557907	14.091597
17.832140	1151.588987	14.096615
17.967196	1147.970108	14.101632
17.816588	1146.500961	14.106650
18.093438	1152.217058	14.111667
18.259661	1139.466485	14.116685
17.783083	1142.772767	14.121703
17.738491	1139.721693	14.126720
18.191764	1139.357165	14.131738
17.574425	1156.688155	14.136755
17.767923	1157.970674	14.141773
18.481708	1162.816720	14.146791
18.077667	1168.043043	14.151808
18.401361	1174.935265	14.156826
18.310265	1162.979250	14.161843
18.014841	1162.492181	14.166861
18.375278	1164.695309	14.171879
18.037695	1172.464333	14.176896
18.687266	1165.795146	14.181914
18.091602	1153.447966	14.186931
18.349083	1151.113285	14.191949
18.432758	1166.077991	14.196967
18.152287	1166.235536	14.201984
18.366724	1172.431646	14.207002
18.220553	1168.071010	14.212019
18.331049	1166.355819	14.217037
18.559493	1171.243197	14.222055
18.590249	1166.201572	14.227072
18.467792	1161.843534	14.232090
18.419546	1164.391569	14.237107
18.545927	1168.297678	14.242125
18.369858	1166.043547	14.247143
18.557922	1167.939160	14.252160
18.357657	1171.561925	14.257178
18.547509	1172.444219	14.262195
18.698957	1176.425299	14.267213
18.644655	1182.966484	14.272231
18.595959	1159.494304	14.277248
18.610347	1163.045565	14.282266
18.232077	1166.083978	14.287283
18.315775	1169.463430	14.292301
18.204387	1177.367433	14.297319
18.434506	1165.231695	14.302336
18.307591	1168.934488	14.307354
18.120202	1172.870825	14.312371
18.757638	1184.917952	14.317389
18.781204	1185.068886	14.322407
18.539609	1193.151092	14.327424
19.087444	1188.265135	14.332442
18.698247	1204.610503	14.337459
18.669324	1202.910841	14.342477
18.470508	1195.727612	14.347495
18.998646	1195.837360	14.352512
18.904460	1199.888490	14.357530
18.697659	1199.273923	14.362547
18.995231	1190.469690	14.367565
18.950802	1197.350170	14.372583
18.645377	1197.205503	14.377600
19.054919	1195.639119	14.382618
18.906887	1192.648426	14.387635
18.830850	1194.585421	14.392653
18.882316	1194.915026	14.397671
19.021602	1201.855088	14.402688
18.825022	1185.071291	14.407706
18.682707	1219.574857	14.412723
19.166244	1213.168359	14.417741
19.371711	1219.144977	14.422759
19.198177	1224.212121	14.427776
19.474946	1206.378967	14.432794
19.097458	1214.046960	14.437811
18.663292	1217.346611	14.442829
18.951027	1219.883039	14.447847
19.152052	1226.838684	14.452864
19.361852	1217.738911	14.457882
19.519650	1221.412885	14.462899
19.422563	1224.429342	14.467917
19.630669	1213.590939	14.472935
19.604277	1222.213812	14.477952
19.833436	1217.128462	14.482970
19.113357	1207.256025	14.487987
18.929749	1190.596427	14.493005
19.870142	1204.805223	14.498023
19.570125	1204.953207	14.503040
19.385186	1194.372064	14.508058
19.666070	1198.648458	14.513075
19.575546	1186.187394	14.518093
19.537779	1188.288811	14.523111
19.041926	1191.680175	14.528128
19.413186	1189.119372	14.533146
19.717247	1197.466389	14.538163
19.613164	1192.253374	14.543181
19.832237	1191.531054	14.548199
19.455447	1196.945625	14.553216
19.514558	1187.967311	14.558234
19.546949	1199.740009	14.563251
19.942528	1209.224592	14.568269
19.906527	1192.409317	14.573287
19.221014	1198.654921	14.578304
19.716578	1190.630730	14.583322
19.848820	1205.676225	14.588339
20.012038	1211.331248	14.593357
20.145662	1190.923236	14.598375
19.373508	1198.668840	14.603392
19.110547	1198.631133	14.608410
19.981215	1214.053255	14.613427
19.852101	1217.453437	14.618445
19.504795	1218.596626	14.623463
19.811543	1227.978369	14.628480
19.803911	1213.181559	14.633498
19.642794	1228.882125	14.638515
19.967070	1216.027836	14.643533
20.063163	1217.909461	14.648551
19.916324	1212.529565	14.653568
19.736662	1217.673408	14.658586
19.632585	1221.423128	14.663603
20.072226	1216.923355	14.668621
20.057755	1210.462340	14.673639
19.550324	1211.794723	14.678656
20.085857	1226.177427	14.683674
19.994426	1233.904754	14.688691
19.887702	1247.220422	14.693709
20.384808	1231.416679	14.698727
20.155916	1232.036372	14.703744
20.541951	1240.954406	14.708762
20.081785	1235.781391	14.713779
19.868738	1239.538720	14.718797
20.585554	1237.911565	14.723815
20.177791	1232.411594	14.728832
19.931566	1233.084497	14.733850
20.197809	1227.545197	14.738867
20.079377	1233.083406	14.743885
19.996497	1230.757860	14.748903
19.828383	1236.736212	14.753920
20.316614	1225.008130	14.758938
20.394231	1236.278290	14.763955
20.235287	1245.922363	14.768973
20.634545	1253.392930	14.773991
20.586680	1260.090929	14.779008
20.547759	1248.903033	14.784026
20.328465	1236.522073	14.789043
20.593504	1256.040803	14.794061
20.753810	1254.273617	14.799079
20.635668	1248.119173	14.804096
20.487490	1240.075899	14.809114
20.643077	1235.996180	14.814131
20.723612	1247.840264	14.819149
20.805718	1240.306879	14.824167
20.382129	1230.350103	14.829184
20.635073	1233.033999	14.834202
20.700133	1240.575859	14.839219
20.860036	1244.315781	14.844237
20.673263	1243.167883	14.849255
20.470389	1249.438873	14.854272
20.443070	1253.719387	14.859290
20.485212	1262.441998	14.864307
20.603531	1254.697799	14.869325
20.890696	1248.767039	14.874343
20.957498	1257.523654	14.879360
20.644828	1256.266089	14.884378
20.642155	1269.369805	14.889395
20.853212	1262.033964	14.894413
20.966572	1256.515453	14.899431
21.044546	1257.674064	14.904448
20.735163	1257.747774	14.909466
20.952468	1258.852995	14.914483
21.173001	1263.119926	14.919501
21.268374	1251.270338	14.924519
20.682677	1252.091108	14.929536
20.905304	1268.192344	14.934554
21.308840	1261.981406	14.939571
21.149493	1249.354351	14.944589
20.991136	1253.336651	14.949607
20.801668	1262.919241	14.954624
21.204839	1277.736149	14.959642
21.500178	1282.379539	14.964659
21.378220	1277.661621	14.969677
21.589345	1266.131570	14.974695
21.183805	1263.872354	14.979712
21.249165	1268.678011	14.984730
21.224755	1257.096504	14.989747
21.231254	1253.993222	14.994765
21.277721	1261.544316	14.999783
21.333809	1267.159336	15.004800
21.419001	1281.871429	15.009818
21.185589	1279.989198	15.014835
21.528853	1275.529759	15.019853
21.781644	1276.601018	15.024871
21.680770	1281.420100	15.029888
21.409014	1273.326743	15.034906
21.312639	1266.155838	15.039923
21.660007	1276.563224	15.044941
21.766053	1273.924039	15.049959
21.538004	1270.930090	15.054976
21.483680	1267.258806	15.059994
21.480404	1279.217031	15.065011
21.643780	1280.497966	15.070029
21.669195	1275.457147	15.075047
21.454563	1282.594709	15.080064
21.734731	1283.181981	15.085082
22.008963	1272.137515	15.090099
21.616000	1275.064635	15.095117
21.774978	1271.681832	15.100135
21.658180	1274.376328	15.105152
21.789374	1271.436549	15.110170
21.914085	1268.002309	15.115187
22.007571	1275.527105	15.120205
21.529918	1275.835470	15.125223
21.591656	1269.084773	15.130240
21.732149	1278.741909	15.135258
21.694144	1272.129919	15.140275
21.817747	1279.031441	15.145293
21.746484	1275.050375	15.150311
21.480812	1283.420425	15.155328
21.592179	1282.317332	15.160346
21.709040	1296.292305	15.165363
21.926654	1309.389939	15.170381
22.327489	1293.200425	15.175399
22.210054	1291.401010	15.180416
22.335632	1300.334636	15.185434
22.416196	1297.380694	15.190451
22.194910	1301.798912	15.195469
22.071677	1293.647560	15.200487
22.432488	1300.887477	15.205504
22.184070	1289.489375	15.210522
22.245791	1288.539233	15.215539
22.279252	1295.183477	15.220557
22.291460	1284.934320	15.225575
22.087481	1293.837524	15.230592
22.085578	1294.077660	15.235610
22.464832	1289.003488	15.240627
22.158537	1294.646892	15.245645
22.685988	1297.432960	15.250663
22.585059	1300.437408	15.255680
22.909960	1296.599399	15.260698
22.242709	1293.860460	15.265715
22.537207	1298.907943	15.270733
22.603807	1295.463867	15.275751
22.825261	1306.866175	15.280768
22.149242	1282.349684	15.285786
22.073753	1291.949146	15.290803
22.462571	1295.309219	15.295821
22.464229	1294.409514	15.300839
22.166711	1299.805383	15.305856
22.409562	1302.598172	15.310874
22.300064	1299.023892	15.315891
22.540166	1306.888660	15.320909
22.603985	1294.479080	15.325927
22.629584	1297.829788	15.330944
22.358202	1319.111578	15.335962
23.101702	1321.396724	15.340979
22.917878	1331.653832	15.345997
22.966111	1329.478149	15.351015
23.044703	1327.477598	15.356032
22.995282	1324.253673	15.361050
23.086255	1310.312366	15.366067
22.556283	1305.645745	15.371085
22.967777	1314.506177	15.376103
23.032915	1317.620313	15.381120
22.729827	1330.736428	15.386138
22.990906	1316.304544	15.391155
23.200832	1328.327230	15.396173
23.245307	1315.292640	15.401191
23.209368	1320.145741	15.406208
23.048583	1317.870261	15.411226
23.355838	1315.994835	15.416243
22.567939	1313.110688	15.421261
23.028804	1320.874598	15.426279
23.506149	1318.114114	15.431296
23.120010	1324.906166	15.436314
23.574184	1315.925851	15.441331
23.366640	1325.334576	15.446349
23.193654	1314.770423	15.451367
23.336262	1324.045387	15.456384
23.059100	1321.844947	15.461402
23.736070	1308.272589	15.466419
23.459226	1320.819678	15.471437
23.252254	1323.102261	15.476455
23.697149	1317.083647	15.481472
23.237900	1319.036515	15.486490
23.290267	1311.798103	15.491507
23.288709	1312.628341	15.496525
23.151101	1318.908064	15.501543
22.922707	1316.176102	15.506560
23.403858	1314.349171	15.511578
23.395046	1302.339143	15.516595
23.034831	1312.194674	15.521613
23.360928	1308.530050	15.526631
23.551668	1325.381129	15.531648
23.233716	1332.329764	15.536666
23.688186	1338.355775	15.541683
24.027475	1344.633372	15.546701
23.670357	1342.309753	15.551719
23.684173	1344.440976	15.556736
23.618553	1344.129342	15.561754
23.782432	1340.136666	15.566771
24.084397	1346.918747	15.571789
24.381004	1340.276396	15.576807
24.368613	1337.346479	15.581824
23.745880	1328.676906	15.586842
23.744049	1317.874488	15.591859
23.766938	1331.346643	15.596877
23.949124	1339.454037	15.601895
24.467035	1336.971226	15.606912
23.896457	1334.453827	15.611930
23.807671	1313.812270	15.616947
24.350723	1326.855771	15.621965
23.892907	1322.307233	15.626983
24.209257	1336.216266	15.632000
24.081423	1335.125401	15.637018
23.576246	1331.928701	15.642035
23.758599	1337.564987	15.647053
24.391892	1338.279976	15.652071
24.460363	1337.079456	15.657088
24.190160	1347.025048	15.662106
24.056889	1339.503275	15.667123
24.315317	1342.767017	15.672141
24.132440	1344.717613	15.677159
24.156392	1344.313047	15.682176
23.990481	1342.672706	15.687194
24.044543	1337.384375	15.692211
24.204426	1341.383107	15.697229
24.062671	1340.146095	15.702247
24.083246	1349.913580	15.707264
24.204786	1360.943399	15.712282
24.852001	1362.874393	15.717299
24.323378	1364.260602	15.722317
24.218684	1367.742196	15.727335
24.381557	1369.821665	15.732352
24.357237	1376.648568	15.737370
24.492141	1367.147029	15.742387
24.700157	1368.465159	15.747405
24.123772	1376.707204	15.752423
24.762102	1364.999697	15.757440
24.539126	1367.237454	15.762458
24.865209	1366.810797	15.767475
25.089167	1361.457968	15.772493
24.910122	1367.494883	15.777511
24.971978	1363.499252	15.782528
24.523708	1367.416543	15.787546
24.947227	1367.621583	15.792563
24.768094	1372.339339	15.797581
24.658424	1375.730191	15.802599
24.917442	1370.766357	15.807616
24.772646	1379.240594	15.812634
24.912360	1381.273198	15.817651
25.156273	1392.845617	15.822669
25.147878	1394.102980	15.827687
25.286702	1386.592206	15.832704
24.990987	1372.563108	15.837722
25.195006	1361.365480	15.842739
24.697483	1367.212445	15.847757
24.365650	1386.534492	15.852775
24.789248	1382.946098	15.857792
24.522143	1393.746486	15.862810
24.780780	1396.167573	15.867827
24.935853	1390.342672	15.872845
25.541043	1403.256568	15.877863
25.600577	1402.836958	15.882880
25.059683	1391.797053	15.887898
25.330860	1389.652707	15.892915
25.248732	1402.699539	15.897933
25.222782	1411.716925	15.902951
25.451683	1410.368182	15.907968
25.357053	1420.642926	15.912986
25.779083	1416.136396	15.918003
25.762552	1414.649375	15.923021
25.467890	1400.863097	15.928039
25.804950	1395.577747	15.933056
25.679049	1388.269402	15.938074
25.333307	1379.641614	15.943091
25.515544	1385.940677	15.948109
25.578330	1403.588236	15.953127
25.578678	1410.436534	15.958144
25.240433	1411.811854	15.963162
25.892570	1408.607386	15.968179
25.750090	1419.072670	15.973197
25.579407	1415.435366	15.978215
25.518422	1419.954734	15.983232
25.547002	1414.351624	15.988250
25.444052	1415.841562	15.993267
25.603105	1409.750933	15.998285
25.878342	1410.168563	16.003303
25.833572	1409.607499	16.008320
25.716737	1408.098323	16.013338
25.656617	1405.119067	16.018355
25.963238	1420.329932	16.023373
25.719690	1437.214447	16.028391
26.496965	1436.076440	16.033408
26.377414	1438.288533	16.038426
25.976210	1420.927480	16.043443
25.545659	1422.307795	16.048461
25.824160	1433.720181	16.053479
26.017282	1432.137192	16.058496
26.096700	1432.973683	16.063514
26.567065	1435.001825	16.068531
26.182205	1426.190788	16.073549
26.375520	1423.582091	16.078567
26.441056	1427.826007	16.083584
26.234375	1429.518399	16.088602
26.652451	1428.651276	16.093619
26.442172	1429.848750	16.098637
26.497104	1426.668420	16.103655
26.369710	1422.345807	16.108672
26.443104	1431.385508	16.113690
26.516822	1430.162068	16.118707
26.685747	1430.182928	16.123725
26.486651	1426.319691	16.128743
26.766428	1428.986789	16.133760
26.443024	1434.863301	16.138778
26.340711	1430.375803	16.143795
26.613566	1434.277957	16.148813
26.523035	1436.993608	16.153831
26.636018	1431.809632	16.158848
26.776632	1426.062727	16.163866
26.701653	1433.143752	16.168883
26.822561	1428.775921	16.173901
26.639093	1437.032173	16.178919
26.690379	1430.674388	16.183936
26.445637	1426.868798	16.188954
26.665645	1429.848230	16.193971
26.852922	1423.292409	16.198989
26.413347	1428.827344	16.204007
27.027910	1415.312023	16.209024
26.838851	1414.451661	16.214042
26.656164	1423.922817	16.219059
26.843189	1427.058902	16.224077
26.895350	1448.223878	16.229095
27.104789	1457.598898	16.234112
27.149399	1445.577247	16.239130
27.098124	1451.187055	16.244147
26.800168	1444.199147	16.249165
27.245565	1450.226617	16.254183
27.252680	1449.095666	16.259200
27.406322	1459.814390	16.264218
27.076265	1459.335895	16.269235
27.200471	1451.363461	16.274253
26.802716	1454.663761	16.279271
26.826270	1449.500103	16.284288
27.040482	1451.678840	16.289306
27.100069	1454.787558	16.294323
27.188063	1461.334953	16.299341
27.296597	1475.305058	16.304359
27.446735	1479.355842	16.309376
27.289643	1466.482117	16.314394
27.375881	1477.183010	16.319411
27.761711	1470.943215	16.324429
27.499420	1481.080153	16.329447
27.664742	1474.420451	16.334464
28.035011	1480.500730	16.339482
27.810032	1478.191104	16.344499
27.930695	1474.741679	16.349517
27.658389	1466.875548	16.354535
27.878624	1449.959920	16.359552
27.713905	1447.637701	16.364570
27.920080	1451.575553	16.369587
27.491753	1446.362771	16.374605
27.557797	1447.453833	16.379623
27.822360	1460.039272	16.384640
27.816616	1466.036443	16.389658
27.614197	1474.374580	16.394675
27.861147	1471.760629	16.399693
27.770478	1473.469563	16.404711
27.900083	1472.647636	16.409728
28.219080	1469.738362	16.414746
27.544327	1475.556323	16.419763
28.233734	1473.251760	16.424781
28.253145	1472.955204	16.429799
28.123693	1468.045898	16.434816
28.139602	1473.042402	16.439834
27.806639	1480.511020	16.444851
28.304708	1471.795161	16.449869
27.863270	1475.282197	16.454887
28.142213	1462.526357	16.459904
27.801527	1473.903234	16.464922
28.225148	1485.242421	16.469939
28.253739	1493.506500	16.474957
28.702084	1494.288346	16.479975
28.933821	1496.675790	16.484992
28.855372	1477.149630	16.490010
28.177383	1471.912839	16.495027
28.653192	1469.685927	16.500045
28.028591	1476.262923	16.505063
28.246893	1476.459091	16.510080
28.473563	1487.270536	16.515098
28.874880	1500.702461	16.520115
28.997828	1490.760898	16.525133
28.578230	1482.185659	16.530151
28.348249	1487.956028	16.535168
28.203592	1484.182083	16.540186
28.605486	1491.115827	16.545203
28.382883	1482.127853	16.550221
28.884244	1493.114023	16.555239
28.895347	1503.877198	16.560256
28.984165	1493.395002	16.565274
29.063377	1499.987971	16.570291
29.219569	1499.840405	16.575309
28.685064	1503.562945	16.580327
28.451334	1496.959446	16.585344
29.169919	1499.551491	16.590362
28.748908	1498.503395	16.595379
28.632074	1492.074096	16.600397
28.846717	1499.804076	16.605415
29.100139	1492.155377	16.610432
28.976340	1496.236462	16.615450
28.851587	1495.388112	16.620467
28.959491	1511.475983	16.625485
28.833246	1526.644303	16.630503
28.993244	1520.165307	16.635520
29.311738	1507.583127	16.640538
28.963174	1514.839599	16.645555
29.417030	1524.899071	16.650573
29.104225	1521.747938	16.655591
29.216790	1523.172558	16.660608
29.773431	1518.042125	16.665626
29.573219	1523.672136	16.670643
29.505893	1512.665258	16.675661
29.240132	1518.627444	16.680679
29.385470	1519.674527	16.685696
29.926579	1520.397657	16.690714
29.896129	1515.125671	16.695731
29.772331	1511.938614	16.700749
29.301957	1517.522585	16.705767
29.528133	1514.154455	16.710784
29.550084	1509.205636	16.715802
29.360768	1515.263145	16.720819
29.599995	1513.142726	16.725837
29.750880	1528.737863	16.730855
29.389533	1535.491394	16.735872
29.989363	1541.845009	16.740890
29.885909	1539.636261	16.745907
30.140506	1529.213280	16.750925
30.018414	1531.801342	16.755943
29.964385	1536.509006	16.760960
30.063679	1526.656340	16.765978
29.852377	1541.216277	16.770995
30.293613	1532.291532	16.776013
29.938462	1537.974227	16.781031
30.134631	1543.554762	16.786048
30.310101	1533.055810	16.791066
29.980173	1534.660220	16.796083
30.256601	1526.941626	16.801101
30.843191	1535.209819	16.806119
29.928609	1528.372143	16.811136
30.293093	1522.100960	16.816154
30.474916	1529.236465	16.821171
30.276949	1528.879289	16.826189
30.290606	1537.312994	16.831207
30.481402	1530.349464	16.836224
30.573892	1526.841324	16.841242
30.251372	1529.653302	16.846259
30.431020	1531.739629	16.851277
30.569619	1536.865258	16.856295
30.278356	1538.700306	16.861312
30.678136	1529.785214	16.866330
30.471740	1531.326085	16.871347
30.255736	1528.368076	16.876365
30.183477	1532.996542	16.881383
30.510951	1523.824526	16.886400
30.641372	1521.803208	16.891418
30.128437	1536.009596	16.896435
30.436195	1549.389941	16.901453
30.847798	1552.512953	16.906471
30.634738	1560.332064	16.911488
30.843540	1561.372362	16.916506
30.735472	1556.639570	16.921523
30.720547	1554.076106	16.926541
30.968107	1561.573727	16.931559
31.066076	1562.707133	16.936576
30.997298	1558.877100	16.941594
31.252646	1559.989004	16.946611
31.107757	1559.238484	16.951629
31.095080	1555.172433	16.956647
31.177806	1559.438935	16.961664
31.319791	1553.306748	16.966682
31.182658	1561.404311	16.971699
31.131200	1556.268155	16.976717
31.031842	1552.701703	16.981735
31.014282	1554.768437	16.986752
31.114292	1557.160749	16.991770
30.868300	1555.630770	16.996787
30.853772	1549.709309	17.001805
31.530029	1563.259157	17.006823
31.405011	1574.261463	17.011840
31.354128	1572.249611	17.016858
31.393649	1575.535071	17.021875
31.743807	1580.400336	17.026893
31.531023	1579.758288	17.031911
31.529618	1579.001067	17.036928
31.322776	1566.475908	17.041946
31.373263	1570.053153	17.046963
31.296288	1572.788793	17.051981
31.208954	1572.953951	17.056999
31.569763	1580.446460	17.062016
31.676958	1582.143338	17.067034
31.580038	1597.206132	17.072051
32.195983	1595.490606	17.077069
32.058423	1589.055051	17.082087
31.781111	1593.753531	17.087104
32.237014	1587.127158	17.092122
31.859699	1590.124463	17.097139
32.492164	1587.847744	17.102157
32.004628	1571.759298	17.107175
31.930227	1566.995981	17.112192
32.774606	1574.220208	17.117210
32.453086	1566.052459	17.122227
32.117814	1565.729419	17.127245
32.108879	1554.391460	17.132263
32.022928	1553.499156	17.137280
32.322446	1556.870115	17.142298
32.401927	1563.141157	17.147315
32.392585	1556.890662	17.152333
32.097025	1555.564118	17.157351
32.312579	1558.061409	17.162368
32.056321	1555.478950	17.167386
32.045863	1567.271227	17.172403
32.532262	1579.569517	17.177421
32.530627	1578.203231	17.182439
32.324643	1582.975743	17.187456
33.032418	1580.081281	17.192474
32.326544	1579.945702	17.197491
32.427292	1584.281973	17.202509
32.357121	1578.110431	17.207527
32.367163	1582.877501	17.212544
32.602986	1574.751818	17.217562
32.468452	1582.350342	17.222579
32.130104	1571.941341	17.227597
32.831986	1592.796395	17.232615
32.717658	1607.631541	17.237632
33.208165	1591.415085	17.242650
33.036662	1604.788508	17.247667
33.146463	1595.934598	17.252685
32.969360	1575.849402	17.257703
32.755854	1585.410683	17.262720
32.896287	1594.563046	17.267738
32.991072	1602.706345	17.272755
32.910868	1603.993909	17.277773
32.986336	1595.429415	17.282791
32.722021	1601.265163	17.287808
32.938968	1603.970536	17.292826
33.075564	1604.987434	17.297843
33.156453	1602.888657	17.302861
33.292333	1599.566219	17.307879
32.834570	1606.833525	17.312896
33.414243	1607.585333	17.317914
33.577457	1625.236310	17.322931
33.099259	1615.038554	17.327949
33.104067	1624.931742	17.332967
33.056969	1632.014789	17.337984
33.482288	1629.297125	17.343002
33.788229	1629.656298	17.348019
33.208947	1637.652749	17.353037
33.641532	1627.668908	17.358055
33.683516	1625.390022	17.363072
33.436991	1624.065258	17.368090
33.771445	1625.089029	17.373107
33.620620	1622.319618	17.378125
34.070510	1615.119791	17.383143
33.840375	1633.791821	17.388160
33.816274	1628.212678	17.393178
34.031872	1621.011686	17.398195
33.793403	1619.811899	17.403213
34.030340	1619.077295	17.408231
34.025261	1624.812470	17.413248
34.200928	1613.713807	17.418266
34.023196	1624.159486	17.423283
34.268462	1615.741956	17.428301
34.235249	1615.352652	17.433319
34.243323	1617.860368	17.438336
34.027760	1610.591228	17.443354
34.207270	1613.173074	17.448371
34.057060	1620.496345	17.453389
34.413616	1619.840834	17.458407
33.961432	1617.866605	17.463424
33.959495	1623.516076	17.468442
34.074959	1636.456377	17.473459
34.331254	1639.098783	17.478477
34.935504	1637.927912	17.483495
34.836897	1648.881942	17.488512
34.658371	1646.811182	17.493530
34.777402	1641.720876	17.498547
34.844843	1645.579517	17.503565
34.793971	1632.644846	17.508583
34.294083	1630.564475	17.513600
34.424667	1635.486249	17.518618
34.794164	1637.369266	17.523635
34.822327	1640.082131	17.528653
35.044358	1644.377322	17.533671
34.598424	1646.994048	17.538688
34.599214	1640.991257	17.543706
34.701417	1640.284075	17.548723
34.674142	1641.907349	17.553741
34.956500	1646.271988	17.558759
34.444893	1639.639387	17.563776
34.662415	1645.257636	17.568794
34.862185	1633.602889	17.573811
34.557252	1644.175812	17.578829
34.838881	1652.990485	17.583847
35.089716	1659.932184	17.588864
34.979077	1670.806057	17.593882
35.044849	1672.020259	17.598899
35.172348	1666.019699	17.603917
35.064264	1652.977206	17.608935
35.127972	1681.396229	17.613952
35.058385	1660.593465	17.618970
35.449590	1661.797705	17.623987
35.337719	1664.021246	17.629005
35.523136	1670.177893	17.634023
35.643772	1676.193205	17.639040
35.609855	1665.032669	17.644058
35.435789	1667.288047	17.649075
35.510462	1675.058970	17.654093
35.748284	1686.875545	17.659111
35.602949	1697.909514	17.664128
36.132319	1689.239142	17.669146
36.208658	1681.712787	17.674163
35.967280	1679.487760	17.679181
35.754433	1664.861592	17.684199
35.969783	1659.869805	17.689216
35.837793	1664.084762	17.694234
35.806621	1656.834053	17.699251
36.230824	1665.336044	17.704269
35.680090	1658.103619	17.709287
35.627775	1667.712276	17.714304
35.814266	1682.831728	17.719322
36.328045	1679.491094	17.724339
36.159295	1689.275804	17.729357
36.033789	1692.274700	17.734375
35.953676	1694.016717	17.739392
36.341511	1689.357678	17.744410
36.630295	1691.348026	17.749427
36.373755	1682.478884	17.754445
36.424190	1677.828529	17.759463
36.544152	1683.058111	17.764480
36.490910	1688.324299	17.769498
36.312852	1678.903190	17.774515
35.906328	1689.447873	17.779533
36.587892	1681.523718	17.784551
36.534741	1686.606845	17.789568
36.096174	1683.671058	17.794586
36.268655	1677.025939	17.799603
36.130092	1698.659774	17.804621
36.473987	1706.025591	17.809639
35.945680	1713.979374	17.814656
36.636228	1709.667399	17.819674
36.591758	1707.219001	17.824691
36.701598	1714.529970	17.829709
36.880064	1705.529540	17.834727
36.796282	1721.019593	17.839744
36.451898	1732.924262	17.844762
36.506907	1734.938619	17.849779
36.739055	1737.165076	17.854797
36.874351	1741.426541	17.859815
37.120302	1740.621088	17.864832
36.928786	1736.961735	17.869850
37.415700	1732.867863	17.874867
37.202864	1733.387220	17.879885
37.516619	1732.018848	17.884903
37.567383	1735.258392	17.889920
37.358275	1726.397576	17.894938
37.575274	1725.590349	17.899955
37.521820	1729.142883	17.904973
37.582706	1725.172571	17.909991
37.523986	1721.094760	17.915008
37.444222	1732.822262	17.920026
37.533542	1726.044979	17.925043
37.564770	1732.244742	17.930061
37.539301	1734.101284	17.935079
37.194089	1729.282518	17.940096
37.138371	1730.739834	17.945114
37.628530	1733.620183	17.950131
37.847669	1748.832411	17.955149
38.117319	1739.521015	17.960167
37.599857	1739.665199	17.965184
37.570780	1740.831146	17.970202
37.846705	1744.824411	17.975219
37.711600	1754.625977	17.980237
37.611860	1749.680377	17.985255
37.667235	1751.391703	17.990272
38.087885	1748.630570	17.995290
38.284112	1742.145818	18.000307
38.184427	1761.236223	18.005325
38.249844	1745.212472	18.010343
38.370801	1747.812979	18.015360
38.196408	1755.847036	18.020378
38.299536	1756.711387	18.025395
37.966699	1761.327087	18.030413
38.192825	1745.685277	18.035431
38.298720	1754.691647	18.040448
38.066190	1752.929154	18.045466
38.342941	1765.954737	18.050483
38.479815	1772.406221	18.055501
38.746953	1769.400877	18.060519
38.631242	1777.166957	18.065536
38.660739	1783.837252	18.070554
38.580200	1777.455815	18.075571
38.518674	1781.767063	18.080589
38.820062	1773.940305	18.085607
38.736583	1776.216220	18.090624
38.831401	1777.675202	18.095642
38.972555	1772.360473	18.100659
38.845800	1767.384386	18.105677
38.558929	1772.803976	18.110695
39.264073	1777.780944	18.115712
38.835269	1784.153794	18.120730
39.189215	1771.427011	18.125747
39.133527	1767.695874	18.130765
38.752070	1775.102779	18.135783
38.892972	1769.011717	18.140800
38.637861	1763.689646	18.145818
39.107806	1779.654759	18.150835
39.497695	1791.412861	18.155853
39.298516	1794.527465	18.160871
39.135678	1792.056574	18.165888
39.076762	1796.916560	18.170906
39.848096	1791.742945	18.175923
39.580486	1799.024719	18.180941
39.843529	1796.092601	18.185959
39.594992	1791.511151	18.190976
39.224087	1792.127864	18.195994
39.530611	1791.767383	18.201011
39.912210	1799.594418	18.206029
39.888129	1793.759585	18.211047
39.597887	1792.242830	18.216064
39.719766	1791.718763	18.221082
39.750292	1787.570146	18.226099
39.672726	1793.619708	18.231117
39.452850	1794.749277	18.236135
39.753137	1792.120612	18.241152
39.310547	1794.651622	18.246170
39.796420	1784.318498	18.251187
40.141256	1808.833894	18.256205
40.125269	1815.230443	18.261223
39.919306	1821.227543	18.266240
39.920826	1821.672290	18.271258
40.356961	1818.937124	18.276275
40.455736	1813.979339	18.281293
40.247868	1812.673752	18.286311
40.474947	1813.935278	18.291328
39.991712	1829.589003	18.296346
40.693084	1821.608031	18.301363
40.276843	1824.002365	18.306381
40.703843	1828.426442	18.311399
40.916385	1826.284920	18.316416
40.375283	1816.213676	18.321434
40.742783	1821.685398	18.326451
40.310001	1819.338853	18.331469
40.532756	1826.045160	18.336487
40.645310	1814.255629	18.341504
40.231665	1819.792932	18.346522
40.758090	1821.099081	18.351539
41.000382	1819.502043	18.356557
40.488424	1826.143572	18.361575
40.839809	1818.545662	18.366592
40.391444	1821.295345	18.371610
41.070071	1840.860374	18.376627
41.062871	1841.861944	18.381645
40.958799	1846.006293	18.386663
41.321362	1843.831795	18.391680
41.299317	1842.686452	18.396698
40.884435	1841.719430	18.401715
41.444341	1839.744402	18.406733
41.430510	1839.478297	18.411751
41.299452	1840.325692	18.416768
41.199715	1850.115457	18.421786
41.462476	1833.009757	18.426803
41.730266	1844.095860	18.431821
41.469515	1838.080329	18.436839
41.755268	1840.377301	18.441856
41.712745	1842.365923	18.446874
41.474929	1843.687667	18.451891
41.475735	1840.430532	18.456909
41.487800	1842.221240	18.461927
42.008513	1845.342989	18.466944
41.504281	1838.450365	18.471962
41.654698	1836.410100	18.476979
41.481667	1841.714038	18.481997
41.647321	1841.252543	18.487015
41.576291	1847.048619	18.492032
41.629508	1856.495665	18.497050
41.731289	1862.406690	18.502067
42.088993	1866.750110	18.507085
41.716461	1867.834169	18.512103
42.053475	1868.895426	18.517120
41.582810	1869.016498	18.522138
41.767718	1859.109207	18.527155
41.945253	1879.759556	18.532173
41.980121	1891.715370	18.537191
42.273421	1892.168054	18.542208
42.100352	1896.692479	18.547226
42.320709	1890.248078	18.552243
42.409289	1884.954177	18.557261
42.543853	1901.372759	18.562279
42.437875	1888.171964	18.567296
42.613398	1883.785998	18.572314
42.702231	1886.748188	18.577331
42.512077	1883.773446	18.582349
42.516779	1888.109059	18.587367
42.844133	1885.630784	18.592384
43.212176	1887.248950	18.597402
42.870481	1891.828198	18.602419
42.748226	1893.444285	18.607437
42.792526	1897.862065	18.612455
42.988301	1882.676202	18.617472
42.973588	1885.455786	18.622490
43.203611	1888.102346	18.627507
42.975590	1888.848164	18.632525
42.757141	1888.399508	18.637543
42.962588	1898.100455	18.642560
43.069196	1906.327253	18.647578
43.257118	1905.991664	18.652595
43.367142	1906.959091	18.657613
43.525509	1903.124955	18.662631
43.545400	1903.153387	18.667648
43.362573	1898.343849	18.672666
43.369288	1897.159280	18.677683
43.505052	1897.289485	18.682701
43.573507	1899.980297	18.687719
43.617945	1898.994958	18.692736
43.510042	1903.745876	18.697754
43.532096	1901.583694	18.702771
43.397182	1894.115598	18.707789
43.249945	1898.683316	18.712807
43.489418	1909.354146	18.717824
43.667427	1911.324003	18.722842
43.392250	1919.411796	18.727859
43.786126	1926.845618	18.732877
43.506293	1920.312306	18.737895
43.685047	1917.585891	18.742912
43.580645	1943.541571	18.747930
44.012093	1955.324830	18.752947
44.140159	1951.192453	18.757965
44.310518	1953.292910	18.762983
44.562329	1942.068497	18.768000
44.421435	1949.548244	18.773018
44.365996	1946.596568	18.778035
44.799770	1947.535364	18.783053
44.243807	1946.435796	18.788071
44.550997	1942.833972	18.793088
44.556022	1949.303021	18.798106
44.724520	1942.304953	18.803123
44.691105	1936.332671	18.808141
44.465557	1944.523160	18.813159
45.238238	1937.342063	18.818176
45.025059	1946.647847	18.823194
45.158717	1945.437073	18.828211
44.856563	1935.675485	18.833229
45.003872	1934.513069	18.838247
44.905914	1927.705089	18.843264
45.354126	1926.268295	18.848282
44.477782	1917.388842	18.853299
44.697639	1924.130356	18.858317
44.321267	1938.012684	18.863335
44.865805	1938.801573	18.868352
44.755774	1948.662437	18.873370
44.943250	1940.888171	18.878387
45.378757	1954.176216	18.883405
45.189729	1966.678436	18.888423
45.253788	1959.359030	18.893440
45.488060	1968.042414	18.898458
45.203163	1966.076651	18.903475
45.556164	1967.870763	18.908493
45.177002	1974.295866	18.913511
45.421318	1971.439242	18.918528
45.071820	1972.383990	18.923546
45.404626	1971.618572	18.928563
45.786907	1965.069873	18.933581
45.701695	1972.730266	18.938599
45.624600	1966.291414	18.943616
45.561070	1963.281038	18.948634
45.857544	1980.690566	18.953651
45.917617	1982.625256	18.958669
45.998743	1987.327643	18.963687
46.056477	1985.178797	18.968704
46.199715	1986.819571	18.973722
45.794873	1988.830261	18.978739
45.998447	1987.113033	18.983757
45.668127	1982.181404	18.988775
46.195124	1980.022155	18.993792
46.712791	1979.218305	18.998810
46.218937	1983.171275	19.003827
46.461389	1973.362210	19.008845
46.001145	1979.115161	19.013863
46.551286	1981.957749	19.018880
46.702595	1986.260947	19.023898
46.253753	1972.842391	19.028915
46.355787	1978.040152	19.033933
46.177307	1994.873966	19.038951
46.575817	2010.149839	19.043968
46.855336	2007.622233	19.048986
46.702479	2009.322025	19.054003
46.636510	1996.657719	19.059021
46.763915	2011.373267	19.064039
47.008574	2006.768140	19.069056
46.882197	1998.244547	19.074074
46.950774	2008.175296	19.079091
47.510000	2000.970810	19.084109
46.963892	2006.642541	19.089127
46.951504	1997.507754	19.094144
47.091523	2011.571183	19.099162
46.716020	2010.670570	19.104179
47.032551	2013.612886	19.109197
47.185608	2034.721718	19.114215
47.255881	2034.634951	19.119232
47.538604	2028.906617	19.124250
47.278170	2036.130554	19.129267
47.568807	2026.541146	19.134285
47.754092	2028.497252	19.139303
47.878794	2023.832015	19.144320
47.813157	2026.957296	19.149338
47.870657	2024.638056	19.154355
47.615890	2028.219035	19.159373
47.709966	2026.897684	19.164391
48.122913	2024.630058	19.169408
48.038783	2019.224313	19.174426
47.908370	2022.833148	19.179443
47.956211	2024.444687	19.184461
47.991277	2028.314796	19.189479
47.880635	2023.153062	19.194496
48.296679	2024.949927	19.199514
48.318619	2026.436127	19.204531
48.205825	2017.244473	19.209549
48.127774	2028.956119	19.214567
48.111961	2037.356804	19.219584
48.186691	2042.887090	19.224602
48.066725	2054.021452	19.229619
48.268488	2058.282047	19.234637
48.130039	2049.968619	19.239655
48.412519	2051.354036	19.244672
48.438983	2051.270977	19.249690
48.426950	2058.307669	19.254707
48.667719	2041.397736	19.259725
48.393129	2059.622703	19.264743
48.755491	2064.075903	19.269760
48.911344	2070.193136	19.274778
48.762427	2071.062276	19.279795
49.037689	2071.713467	19.284813
48.801071	2075.749238	19.289831
48.659098	2072.558616	19.294848
48.625965	2072.219787	19.299866
48.830750	2081.548523	19.304883
48.911890	2062.078778	19.309901
49.222526	2078.741356	19.314919
48.848493	2092.629750	19.319936
49.080621	2084.883142	19.324954
49.329410	2091.254085	19.329971
49.487196	2101.413924	19.334989
49.793066	2096.410990	19.340007
49.440767	2094.181196	19.345024
49.815092	2094.371864	19.350042
49.541885	2095.295196	19.355059
49.684370	2078.574209	19.360077
49.665663	2087.846440	19.365095
49.413897	2092.686225	19.370112
49.761829	2086.471093	19.375130
49.635398	2091.729931	19.380147
49.981288	2082.548434	19.385165
50.056152	2101.059544	19.390183
49.988860	2119.460392	19.395200
50.001304	2111.306346	19.400218
50.161216	2113.796653	19.405235
50.515966	2107.195408	19.410253
50.209259	2106.949938	19.415271
50.303176	2111.931242	19.420288
50.270339	2111.854318	19.425306
50.084804	2117.788350	19.430323
50.706600	2109.406278	19.435341
50.193530	2105.611022	19.440359
50.562957	2104.704151	19.445376
50.615711	2108.457888	19.450394
50.053424	2110.783615	19.455411
50.440141	2113.333069	19.460429
50.321860	2106.562921	19.465447
50.398714	2123.874443	19.470464
50.519476	2125.812265	19.475482
50.573855	2141.274721	19.480499
50.524849	2130.154132	19.485517
50.915412	2132.065463	19.490535
51.046911	2139.669881	19.495552
51.130202	2122.096525	19.500570
50.864622	2132.979174	19.505587
50.901620	2134.908028	19.510605
51.444942	2140.304960	19.515623
51.386405	2159.572393	19.520640
51.632266	2147.657607	19.525658
51.407080	2144.423201	19.530675
51.571465	2151.858357	19.535693
51.654309	2161.679650	19.540711
51.615960	2146.126271	19.545728
51.674471	2143.282952	19.550746
51.693336	2150.065510	19.555763
51.256705	2148.316019	19.560781
51.949410	2146.853527	19.565799
51.496736	2152.829426	19.570816
52.021712	2143.206396	19.575834
51.956277	2146.565215	19.580851
51.969238	2149.129048	19.585869
51.992185	2148.390079	19.590887
51.934836	2158.656248	19.595904
52.510301	2155.119655	19.600922
52.197329	2156.071313	19.605939
52.053873	2152.423280	19.610957
52.089383	2146.645272	19.615975
52.295344	2153.202843	19.620992
52.281761	2152.867261	19.626010
52.523953	2153.422642	19.631027
52.183226	2151.759118	19.636045
52.333112	2150.798273	19.641063
52.210813	2159.755386	19.646080
52.285706	2153.210595	19.651098
52.433540	2148.873088	19.656115
52.131256	2164.135804	19.661133
52.636641	2170.406607	19.666151
52.544794	2173.592829	19.671168
52.511228	2175.185577	19.676186
52.726878	2183.095592	19.681203
52.645866	2175.297013	19.686221
53.132314	2179.055404	19.691239
52.855761	2193.070624	19.696256
53.023546	2191.358985	19.701274
53.601311	2198.186549	19.706291
53.227055	2200.110411	19.711309
53.555120	2199.664490	19.716327
53.277141	2201.787881	19.721344
53.138441	2192.044728	19.726362
53.564361	2196.765738	19.731379
53.248523	2198.102886	19.736397
53.634408	2199.551015	19.741415
53.209891	2203.695157	19.746432
53.541551	2200.761691	19.751450
53.456472	2207.292291	19.756467
53.283920	2204.778679	19.761485
53.390447	2208.905896	19.766503
53.325301	2220.019147	19.771520
53.890824	2218.210471	19.776538
54.074876	2229.483517	19.781555
53.843154	2228.844412	19.786573
53.553084	2230.786648	19.791591
53.613531	2229.413742	19.796608
53.998634	2227.298790	19.801626
53.962172	2244.726021	19.806643
53.986509	2250.182208	19.811661
54.292779	2246.103901	19.816679
54.168023	2246.723091	19.821696
54.457439	2248.785993	19.826714
54.448418	2246.379308	19.831731
54.103692	2243.517094	19.836749
54.172325	2247.356741	19.841767
54.492024	2260.013008	19.846784
54.660302	2262.874443	19.851802
54.559370	2270.553206	19.856819
54.526556	2264.015782	19.861837
54.868021	2254.939042	19.866855
54.858296	2269.325962	19.871872
54.867572	2266.439840	19.876890
55.091022	2260.250465	19.881907
54.906526	2266.660951	19.886925
55.288392	2281.497812	19.891943
55.251441	2285.158334	19.896960
55.658000	2283.090511	19.901978
55.133332	2274.256772	19.906995
54.998081	2292.232905	19.912013
55.352187	2283.734889	19.917031
55.739588	2284.295929	19.922048
55.771691	2281.059059	19.927066
55.836977	2282.832005	19.932083
55.683352	2289.259756	19.937101
56.104256	2282.225166	19.942119
55.819400	2272.236602	19.947136
55.839300	2255.367385	19.952154
56.006224	2254.100882	19.957171
55.656247	2262.162674	19.962189
56.157830	2267.720833	19.967207
56.119387	2285.905874	19.972224
55.431274	2273.367254	19.977242
56.098940	2269.443777	19.982259
55.759087	2277.346186	19.987277
55.952848	2273.692635	19.992295
55.845248	2274.403819	19.997312
55.988166	2279.263874	20.002330
56.210933	2290.470927	20.007347
56.036368	2297.318564	20.012365
56.638452	2299.335640	20.017383
56.527403	2302.029388	20.022400
56.435114	2293.487689	20.027418
56.862037	2295.576394	20.032435
56.508231	2305.522989	20.037453
56.695812	2298.417643	20.042471
56.295861	2306.626152	20.047488
56.179692	2302.036456	20.052506
56.861000	2321.055589	20.057523
56.624301	2322.882166	20.062541
56.766338	2325.444738	20.067559
56.905436	2330.040293	20.072576
56.903136	2316.753504	20.077594
57.044016	2334.452865	20.082611
56.857310	2349.340992	20.087629
57.382211	2343.104357	20.092647
57.214325	2353.902398	20.097664
57.441260	2341.816864	20.102682
57.378015	2345.708757	20.107699
57.652846	2349.383564	20.112717
58.030333	2340.291669	20.117735
58.182678	2339.762813	20.122752
57.915479	2343.393143	20.127770
57.856938	2346.637300	20.132787
57.601591	2343.445456	20.137805
57.927537	2338.704421	20.142823
57.939426	2345.765883	20.147840
58.064447	2337.912861	20.152858
58.147273	2338.799359	20.157875
57.992427	2345.527149	20.162893
58.155382	2361.818617	20.167911
58.252884	2369.254875	20.172928
58.371526	2375.015090	20.177946
58.614875	2381.178686	20.182963
58.214415	2372.233911	20.187981
58.405960	2373.873465	20.192999
58.593888	2375.908098	20.198016
58.805606	2372.674631	20.203034
59.193910	2371.016795	20.208051
58.653360	2367.001704	20.213069
58.552448	2363.523704	20.218087
59.069396	2370.209371	20.223104
58.883805	2365.980861	20.228122
58.835760	2358.918721	20.233139
58.791197	2366.901148	20.238157
59.061093	2356.730936	20.243175
58.888678	2364.402003	20.248192
59.012179	2371.130378	20.253210
58.912635	2373.036465	20.258227
59.138002	2393.367458	20.263245
59.233196	2385.762108	20.268263
59.243763	2386.704115	20.273280
59.551651	2389.449014	20.278298
59.566224	2389.645553	20.283315
59.195877	2391.205871	20.288333
59.251420	2399.005354	20.293351
59.494962	2390.893875	20.298368
59.755579	2405.907641	20.303386
59.830311	2403.109081	20.308403
59.991867	2423.055592	20.313421
59.964368	2402.680917	20.318439
60.127936	2405.997592	20.323456
60.038033	2403.152236	20.328474
59.999190	2409.738787	20.333491
59.846358	2412.009868	20.338509
60.282809	2406.168959	20.343527
60.404038	2414.665124	20.348544
59.990100	2415.998722	20.353562
60.231404	2407.878118	20.358579
60.085090	2410.788866	20.363597
60.018087	2416.852763	20.368615
60.355327	2422.443032	20.373632
60.358387	2437.118445	20.378650
60.305655	2430.451524	20.383667
60.507222	2434.276697	20.388685
60.800294	2444.645930	20.393703
60.885637	2462.085849	20.398720
61.123879	2462.013793	20.403738
61.071021	2457.309986	20.408755
61.121046	2457.340010	20.413773
61.145811	2445.273458	20.418791
61.328025	2458.099742	20.423808
60.990905	2452.181184	20.428826
61.188347	2446.519734	20.433843
61.634555	2451.303912	20.438861
61.493410	2451.354420	20.443879
61.475956	2452.348162	20.448896
60.792189	2446.679596	20.453914
61.257252	2453.714284	20.458931
61.712277	2479.545214	20.463949
61.722610	2470.270914	20.468967
61.976314	2470.906562	20.473984
61.978434	2474.210671	20.479002
62.174079	2471.718236	20.484019
61.825137	2465.934083	20.489037
62.113959	2468.139129	20.494055
62.381337	2465.790105	20.499072
62.071617	2464.052259	20.504090
62.589736	2467.559572	20.509107
62.113523	2474.186268	20.514125
62.449998	2471.270942	20.519143
62.469419	2470.961744	20.524160
62.236370	2474.236421	20.529178
62.162217	2473.013986	20.534195
62.016942	2489.656849	20.539213
62.453709	2481.698111	20.544231
62.866654	2484.843172	20.549248
62.314167	2491.642787	20.554266
62.688803	2487.844077	20.559283
63.156747	2500.025962	20.564301
62.976009	2495.272746	20.569319
62.604475	2489.791956	20.574336
62.834042	2512.846157	20.579354
63.322071	2517.554365	20.584371
63.262571	2519.507848	20.589389
63.396053	2513.973175	20.594407
63.054951	2511.523800	20.599424
62.789974	2515.396838	20.604442
63.568829	2512.686777	20.609459
63.168195	2514.539057	20.614477
63.566142	2514.129523	20.619495
63.562078	2528.092842	20.624512
63.914106	2537.032636	20.629530
64.127794	2537.138014	20.634547
64.235333	2542.458165	20.639565
64.423737	2524.318781	20.644583
64.141037	2523.883331	20.649600
63.827703	2514.621846	20.654618
63.624094	2507.738670	20.659635
64.100814	2526.521806	20.664653
63.895727	2529.646930	20.669671
63.904131	2531.069015	20.674688
63.955585	2533.156609	20.679706
64.447011	2539.413950	20.684723
64.056015	2538.869221	20.689741
64.105129	2554.828371	20.694759
64.263942	2557.615589	20.699776
64.429057	2562.759451	20.704794
64.464071	2569.091467	20.709811
64.390110	2565.558706	20.714829
64.891720	2569.185403	20.719847
64.843183	2574.217560	20.724864
64.901019	2588.117574	20.729882
65.347875	2590.982757	20.734899
65.258987	2585.460809	20.739917
65.094454	2582.914326	20.744935
65.349895	2581.154199	20.749952
65.395040	2586.244273	20.754970
65.405797	2576.976163	20.759987
65.407826	2582.814683	20.765005
65.244471	2570.218885	20.770023
65.302724	2578.797586	20.775040
65.480232	2578.605644	20.780058
65.869382	2578.061773	20.785075
65.857429	2590.277879	20.790093
66.059216	2605.215813	20.795111
65.990470	2598.090543	20.800128
66.027801	2602.566399	20.805146
66.142763	2601.592066	20.810163
65.779722	2609.031144	20.815181
66.103902	2605.928354	20.820199
65.936604	2602.283964	20.825216
65.808705	2600.198847	20.830234
66.089321	2598.100223	20.835251
66.073770	2609.818236	20.840269
66.207636	2610.999740	20.845287
66.665681	2624.404687	20.850304
66.468844	2623.204619	20.855322
66.220590	2617.344674	20.860339
66.362305	2625.695704	20.865357
66.744483	2638.244608	20.870375
67.094074	2645.871882	20.875392
66.624212	2649.177381	20.880410
67.159829	2642.718035	20.885427
67.128465	2649.947357	20.890445
67.404133	2666.934731	20.895463
67.565455	2650.178701	20.900480
67.317465	2656.823361	20.905498
67.623219	2648.263315	20.910515
67.543949	2652.353465	20.915533
67.439451	2656.037269	20.920551
67.842133	2642.330144	20.925568
67.658097	2641.172256	20.930586
67.758896	2641.383694	20.935603
68.113262	2640.318195	20.940621
67.165103	2642.997966	20.945639
67.645053	2641.019602	20.950656
67.601030	2648.989444	20.955674
68.137274	2647.693456	20.960691
67.964985	2656.380906	20.965709
67.622332	2676.037426	20.970727
67.982737	2673.153036	20.975744
67.980167	2675.580508	20.980762
68.328201	2663.030768	20.985779
68.025906	2675.273484	20.990797
68.274003	2674.745398	20.995815
68.707314	2682.062892	21.000832
68.626837	2688.353078	21.005850
68.759243	2687.754745	21.010867
68.534804	2693.029113	21.015885
68.505297	2691.199999	21.020903
68.918527	2689.740224	21.025920
68.839021	2685.113123	21.030938
69.041438	2695.162154	21.035955
68.685040	2695.502035	21.040973
68.949762	2698.269526	21.045991
69.374574	2708.482557	21.051008
69.353167	2713.106514	21.056026
68.983700	2710.945611	21.061043
69.597115	2714.747346	21.066061
69.246657	2719.448109	21.071079
69.647897	2713.760958	21.076096
69.728635	2716.696148	21.081114
69.528431	2710.683461	21.086131
69.465592	2712.899449	21.091149
69.216956	2718.695226	21.096167
69.869628	2730.109784	21.101184
69.752033	2736.263775	21.106202
69.890874	2734.553463	21.111219
70.379492	2738.548346	21.116237
69.817157	2735.723301	21.121255
69.979328	2733.513817	21.126272
69.988316	2752.790243	21.131290
70.421807	2750.992735	21.136307
70.260440	2754.928494	21.141325
70.078817	2768.815666	21.146343
70.522458	2753.770136	21.151360
70.535710	2758.533859	21.156378
70.677935	2775.488588	21.161395
70.704328	2771.495044	21.166413
70.571960	2780.050053	21.171431
71.265207	2773.799520	21.176448
71.100096	2775.605457	21.181466
70.992503	2777.995742	21.186483
70.986455	2777.119263	21.191501
71.271563	2771.608097	21.196519
71.610341	2776.087265	21.201536
71.383886	2781.538721	21.206554
71.333006	2783.986400	21.211571
71.752174	2784.125866	21.216589
71.778601	2799.940447	21.221607
72.029475	2799.850631	21.226624
71.602672	2793.311620	21.231642
71.859089	2794.319283	21.236659
71.806918	2799.560380	21.241677
72.181453	2802.200216	21.246695
72.192433	2796.760397	21.251712
72.330412	2793.358507	21.256730
72.073321	2797.034686	21.261747
72.138538	2797.460008	21.266765
72.276664	2805.518160	21.271783
72.151300	2798.568959	21.276800
72.084675	2805.362002	21.281818
72.127784	2809.612916	21.286835
72.499512	2808.462627	21.291853
72.010468	2821.681553	21.296871
72.370136	2830.333085	21.301888
72.402646	2827.569480	21.306906
72.274613	2824.247136	21.311923
72.666248	2841.629965	21.316941
72.992130	2850.106898	21.321959
73.532856	2847.784434	21.326976
73.479659	2850.377670	21.331994
73.551550	2853.699324	21.337011
73.532283	2847.629836	21.342029
73.162113	2859.895936	21.347047
73.351787	2856.331282	21.352064
73.390030	2848.513727	21.357082
73.158107	2854.852948	21.362099
73.506124	2849.196187	21.367117
73.299854	2865.994138	21.372135
73.865643	2866.763963	21.377152
74.250599	2873.360034	21.382170
74.085223	2869.279735	21.387187
73.906474	2869.718033	21.392205
74.198517	2878.983015	21.397223
74.145679	2874.017132	21.402240
74.366593	2870.807385	21.407258
74.022314	2869.542028	21.412275
74.496611	2873.775899	21.417293
74.156417	2878.661309	21.422311
74.604190	2886.787762	21.427328
74.333896	2899.552699	21.432346
74.609738	2906.812896	21.437363
74.631136	2890.583557	21.442381
74.758418	2900.884344	21.447399
75.181815	2893.650289	21.452416
75.313827	2890.003132	21.457434
74.836630	2891.267769	21.462451
74.866923	2882.681335	21.467469
74.988876	2907.700271	21.472487
75.755723	2906.664817	21.477504
75.230033	2919.210974	21.482522
75.448268	2913.669213	21.487539
75.628238	2920.540444	21.492557
75.519844	2912.985706	21.497575
75.547258	2916.355370	21.502592
75.390929	2920.037880	21.507610
75.733371	2917.203609	21.512627
76.056521	2917.048814	21.517645
75.862644	2937.480826	21.522663
75.818131	2935.098547	21.527680
76.118112	2934.691729	21.532698
76.322091	2939.068966	21.537715
76.254311	2934.278998	21.542733
76.117437	2936.664423	21.547751
75.958503	2929.098660	21.552768
76.302597	2943.481183	21.557786
76.308412	2958.844640	21.562803
76.378879	2955.614263	21.567821
76.482258	2958.154577	21.572839
76.434406	2944.924961	21.577856
76.533569	2963.379497	21.582874
76.642408	2974.876260	21.587891
76.852534	2979.997409	21.592909
76.688319	2982.567027	21.597927
77.009346	2989.652899	21.602944
77.374435	2979.574735	21.607962
77.401958	2985.718699	21.612979
77.283919	3002.367237	21.617997
77.469112	3000.719075	21.623015
77.233507	3007.573388	21.628032
77.391070	3005.191002	21.633050
77.481394	3016.103638	21.638067
77.440298	2997.911361	21.643085
77.653836	3008.605847	21.648103
78.234337	3019.517436	21.653120
78.103579	3024.628881	21.658138
77.956661	3028.934869	21.663155
78.352013	3024.801400	21.668173
78.130619	3025.031761	21.673191
78.228309	3026.556675	21.678208
78.507714	3024.776971	21.683226
78.251234	3029.567244	21.688243
78.383384	3020.945848	21.693261
77.786237	3017.381346	21.698279
78.476277	3029.566669	21.703296
78.530431	3052.336579	21.708314
79.023733	3042.948440	21.713331
78.932167	3048.325186	21.718349
78.970572	3053.438542	21.723367
78.885460	3052.318783	21.728384
79.082456	3051.432572	21.733402
79.011413	3074.966993	21.738419
79.308844	3076.678397	21.743437
79.411343	3072.432990	21.748455
78.870377	3075.759173	21.753472
79.411285	3064.343583	21.758490
79.485822	3085.888885	21.763507
79.763947	3098.855255	21.768525
79.727206	3092.684268	21.773543
80.074747	3088.002781	21.778560
80.137803	3089.978155	21.783578
80.038721	3086.234604	21.788595
79.986880	3078.418439	21.793613
80.639889	3082.608579	21.798631
80.349441	3081.805050	21.803648
80.384354	3080.650703	21.808666
80.517887	3088.930637	21.813683
80.464583	3081.474509	21.818701
80.605596	3098.088861	21.823719
80.830413	3114.232444	21.828736
81.021013	3113.318827	21.833754
80.725661	3118.689647	21.838771
81.270454	3104.858908	21.843789
81.062063	3114.126667	21.848807
80.769629	3119.430749	21.853824
81.245079	3111.134272	21.858842
81.712131	3108.308854	21.863859
81.614353	3095.118512	21.868877
81.365696	3116.525114	21.873895
81.214068	3116.353173	21.878912
81.271436	3100.424163	21.883930
81.581970	3124.025114	21.888947
81.731024	3128.407847	21.893965
81.605904	3133.565783	21.898983
81.548937	3131.510521	21.904000
81.803423	3135.766269	21.909018
81.632887	3154.600972	21.914035
82.092993	3159.897630	21.919053
81.994956	3164.962957	21.924071
81.914551	3170.672552	21.929088
82.273468	3160.345911	21.934106
81.807258	3170.806120	21.939123
82.397764	3177.976096	21.944141
82.611439	3192.041533	21.949159
82.531155	3187.035676	21.954176
83.240884	3188.729838	21.959194
82.753258	3193.928805	21.964211
83.025270	3186.431134	21.969229
83.389530	3193.421939	21.974247
82.842592	3191.569686	21.979264
83.073996	3182.787476	21.984282
83.212783	3209.417031	21.989299
83.105705	3202.000841	21.994317
83.450112	3202.745399	21.999335
83.559578	3211.073347	22.004352
83.343758	3205.700502	22.009370
83.503545	3207.641796	22.014387
83.766902	3209.547926	22.019405
83.868693	3208.433593	22.024423
84.008380	3224.502239	22.029440
83.803717	3232.292351	22.034458
83.661912	3231.279307	22.039475
83.934131	3230.851583	22.044493
84.367635	3234.006182	22.049511
84.027368	3229.170453	22.054528
84.252965	3238.417624	22.059546
84.736004	3250.013749	22.064563
84.736642	3258.207269	22.069581
85.053004	3260.758444	22.074599
84.592990	3264.797917	22.079616
84.984369	3245.126787	22.084634
84.988064	3252.549701	22.089651
85.165481	3258.989055	22.094669
85.413487	3246.290458	22.099687
84.924815	3258.913113	22.104704
85.122846	3252.762100	22.109722
85.419171	3262.904048	22.114739
85.689602	3266.696515	22.119757
85.710764	3273.169824	22.124775
85.569245	3269.871604	22.129792
85.862974	3270.242198	22.134810
85.414304	3273.604457	22.139827
85.676786	3282.823779	22.144845
85.914889	3282.666524	22.149863
85.485774	3267.220744	22.154880
85.596363	3279.291867	22.159898
85.332632	3295.783594	22.164915
86.239336	3306.865189	22.169933
86.331162	3305.806068	22.174951
86.862098	3314.806596	22.179968
86.718681	3315.943215	22.184986
86.759481	3317.764287	22.190003
86.677225	3316.912347	22.195021
86.822230	3311.874315	22.200039
86.723805	3314.077014	22.205056
87.134298	3306.415565	22.210074
87.022362	3314.481560	22.215091
86.709984	3323.106059	22.220109
86.947676	3331.041534	22.225127
87.018457	3337.661749	22.230144
87.097524	3337.115940	22.235162
87.516789	3346.749452	22.240179
87.482203	3361.911268	22.245197
88.197550	3357.964311	22.250215
88.006804	3367.835439	22.255232
88.164342	3353.550712	22.260250
88.219326	3357.569487	22.265267
87.960018	3358.796860	22.270285
88.049766	3359.117352	22.275303
87.818935	3363.237720	22.280320
88.103925	3359.721160	22.285338
88.372423	3362.901635	22.290355
88.414660	3380.658511	22.295373
88.936286	3381.144904	22.300391
88.713280	3388.634954	22.305408
88.885330	3383.586352	22.310426
88.528527	3382.951018	22.315443
88.100957	3382.572961	22.320461
88.763519	3383.958904	22.325479
88.717116	3407.578274	22.330496
88.943877	3411.090393	22.335514
89.312345	3415.031660	22.340531
89.043394	3418.870792	22.345549
89.090625	3417.875464	22.350567
89.580979	3423.842906	22.355584
89.158980	3436.682490	22.360602
89.396373	3444.580186	22.365619
89.429312	3444.811735	22.370637
89.588329	3443.814674	22.375655
89.495087	3445.483164	22.380672
90.028560	3452.204525	22.385690
90.088173	3462.140638	22.390707
89.916596	3465.090232	22.395725
90.079072	3467.009039	22.400743
90.500606	3474.896836	22.405760
90.324253	3473.504123	22.410778
90.614231	3480.538241	22.415795
90.917069	3491.563059	22.420813
91.137387	3489.584252	22.425831
90.684121	3493.348120	22.430848
90.817988	3497.341942	22.435866
91.141597	3487.771845	22.440883
90.948640	3482.180707	22.445901
91.272865	3479.074607	22.450919
91.107618	3498.644256	22.455936
91.241705	3506.258316	22.460954
91.836723	3515.365688	22.465971
91.854198	3522.373078	22.470989
91.678948	3512.360338	22.476007
91.712629	3523.291624	22.481024
91.741777	3515.503613	22.486042
91.640108	3507.303687	22.491059
91.771791	3524.431213	22.496077
92.279413	3531.996230	22.501095
91.997227	3533.015727	22.506112
92.403151	3534.514487	22.511130
92.548578	3531.205981	22.516147
92.102957	3537.200164	22.521165
92.729293	3537.540749	22.526183
92.409854	3558.987369	22.531200
92.579566	3560.971335	22.536218
93.002637	3554.469332	22.541235
92.593175	3564.235957	22.546253
93.149028	3558.489601	22.551271
93.221261	3572.684810	22.556288
93.443753	3575.983002	22.561306
93.368221	3587.111347	22.566323
93.140338	3592.803148	22.571341
93.656836	3588.183439	22.576359
93.542685	3590.410730	22.581376
93.530792	3583.484480	22.586394
94.013636	3590.387422	22.591411
93.910867	3601.911426	22.596429
93.915673	3607.541526	22.601447
94.342073	3605.287383	22.606464
94.114774	3610.022735	22.611482
94.020729	3606.022626	22.616499
94.020619	3614.216424	22.621517
94.180605	3611.290694	22.626535
94.425764	3623.331493	22.631552
94.373217	3637.650462	22.636570
94.940433	3636.763034	22.641587
94.485147	3635.145722	22.646605
94.952628	3643.282057	22.651623
94.822720	3639.404343	22.656640
95.016503	3655.237641	22.661658
95.101996	3655.953346	22.666675
95.114518	3669.447813	22.671693
95.585566	3666.179800	22.676711
95.468597	3665.064994	22.681728
94.960574	3669.740185	22.686746
95.488887	3662.874459	22.691763
95.782637	3677.770469	22.696781
95.937165	3680.845760	22.701799
95.892015	3679.943800	22.706816
96.009186	3677.365649	22.711834
95.923212	3682.871117	22.716851
95.818365	3679.099939	22.721869
96.058088	3691.331016	22.726887
95.903433	3701.464959	22.731904
96.271340	3697.149416	22.736922
96.458938	3702.056514	22.741939
96.615246	3717.605356	22.746957
96.505226	3735.935637	22.751975
96.850498	3737.349228	22.756992
96.777289	3734.210662	22.762010
96.730231	3731.137439	22.767027
97.024589	3745.250637	22.772045
97.775443	3753.936017	22.777063
97.293265	3758.424113	22.782080
97.053439	3755.715660	22.787098
97.346271	3749.155084	22.792115
97.570634	3755.773485	22.797133
97.854278	3763.742983	22.802151
97.777924	3786.770991	22.807168
97.802109	3780.574442	22.812186
98.308366	3774.873665	22.817203
97.831988	3776.949410	22.822221
98.689122	3775.072807	22.827239
98.584814	3775.565746	22.832256
98.374187	3783.710539	22.837274
98.711046	3785.071793	22.842291
98.545804	3799.702086	22.847309
98.854688	3806.783871	22.852327
98.804325	3800.273891	22.857344
99.254278	3801.806808	22.862362
99.493306	3796.201550	22.867379
99.378560	3799.612590	22.872397
99.504016	3796.285070	22.877415
99.427948	3789.671805	22.882432
99.434435	3796.428515	22.887450
99.448984	3794.327253	22.892467
99.475448	3817.986243	22.897485
99.646362	3817.580692	22.902503
99.576295	3826.325283	22.907520
99.835519	3818.800948	22.912538
99.921324	3824.027037	22.917555
99.802121	3835.282318	22.922573
100.216778	3845.639625	22.927591
100.407317	3849.375294	22.932608
100.127939	3845.394699	22.937626
100.686134	3854.034559	22.942643
100.428259	3859.200874	22.947661
100.619614	3860.023099	22.952679
100.692352	3874.710858	22.957696
101.016955	3877.507028	22.962714
101.263109	3877.746211	22.967731
100.951836	3877.274167	22.972749
100.904665	3883.190255	22.977767
101.427409	3890.273288	22.982784
101.200331	3894.977116	22.987802
101.358362	3889.561275	22.992819
100.936661	3894.699609	22.997837
101.098477	3910.781180	23.002855
101.394792	3920.352197	23.007872
101.618526	3922.251987	23.012890
101.817441	3923.773744	23.017907
101.996703	3940.449162	23.022925
101.831619	3954.331494	23.027943
102.317947	3949.605949	23.032960
102.012933	3951.149846	23.037978
102.434183	3958.163584	23.042995
102.599927	3969.383774	23.048013
103.106121	3983.498690	23.053031
102.717871	3968.967569	23.058048
103.060609	3976.328191	23.063066
103.558257	3966.497005	23.068083
103.390535	3973.896568	23.073101
103.472458	3972.567512	23.078119
103.478988	3966.626175	23.083136
103.540730	3964.618504	23.088154
103.772940	3961.757154	23.093171
103.719410	3967.563793	23.098189
103.834858	3987.680234	23.103207
103.849102	3984.265944	23.108224
103.748460	3999.009375	23.113242
103.841252	3990.690385	23.118259
104.087423	3988.123544	23.123277
104.290166	4000.805674	23.128295
104.469522	4010.028923	23.133312
104.380899	4013.344374	23.138330
104.607750	4019.492180	23.143347
104.440794	4028.990643	23.148365
104.574095	4017.676195	23.153383
104.635168	4022.565327	23.158400
104.583745	4045.106830	23.163418
105.278222	4043.697580	23.168435
105.091782	4050.481455	23.173453
105.315377	4043.477101	23.178471
105.290031	4061.958578	23.183488
105.340981	4063.793918	23.188506
105.291542	4069.113864	23.193523
105.430077	4074.265479	23.198541
105.530943	4092.124341	23.203559
105.880871	4086.397458	23.208576
105.787333	4098.472701	23.213594
106.282703	4090.434640	23.218611
106.238192	4097.653974	23.223629
106.492506	4114.289385	23.228647
106.677425	4114.528696	23.233664
106.460551	4117.409738	23.238682
106.707601	4114.372438	23.243699
106.276441	4123.015925	23.248717
106.797039	4132.283621	23.253735
107.709077	4140.814524	23.258752
107.224255	4151.180361	23.263770
107.599156	4143.180089	23.268787
107.370827	4140.753853	23.273805
107.339408	4139.316286	23.278823
107.797433	4136.930868	23.283840
107.570534	4134.848456	23.288858
107.740406	4138.678959	23.293875
107.653151	4155.500492	23.298893
107.376116	4165.836939	23.303911
107.387057	4161.119535	23.308928
107.606527	4182.892793	23.313946
107.670895	4187.393214	23.318963
108.107869	4194.193102	23.323981
108.270236	4209.400524	23.328999
108.554924	4213.604450	23.334016
108.609296	4218.216919	23.339034
108.837137	4218.547356	23.344051
109.225831	4216.529466	23.349069
108.876785	4213.557133	23.354087
108.485687	4222.652071	23.359104
108.672687	4235.835547	23.364122
109.408772	4228.195299	23.369139
109.263178	4239.208764	23.374157
109.452517	4258.616359	23.379175
109.817029	4260.503598	23.384192
109.744078	4267.099326	23.389210
109.762371	4265.420385	23.394227
109.728053	4266.360053	23.399245
110.013368	4282.567800	23.404263
110.537872	4284.900284	23.409280
110.335604	4288.486105	23.414298
110.474899	4285.071105	23.419315
110.764659	4278.709676	23.424333
110.492831	4294.654360	23.429351
110.732618	4296.535892	23.434368
110.772582	4301.750362	23.439386
110.829572	4315.023706	23.444403
111.268558	4313.326196	23.449421
111.023382	4314.014822	23.454439
111.167963	4318.199690	23.459456
110.963070	4326.820449	23.464474
111.491869	4326.765998	23.469491
111.880573	4337.351761	23.474509
111.722849	4331.151959	23.479527
112.336130	4330.370916	23.484544
111.805728	4345.939505	23.489562
111.829276	4355.556645	23.494579
112.078913	4356.552836	23.499597
111.937935	4365.599189	23.504615
112.621659	4367.152348	23.509632
112.585016	4384.499603	23.514650
113.008764	4385.708407	23.519667
113.015333	4377.765741	23.524685
112.793128	4382.743541	23.529703
113.254943	4383.706492	23.534720
112.990917	4388.959144	23.539738
113.181588	4385.614987	23.544755
113.466203	4413.066239	23.549773
113.482065	4411.548644	23.554791
113.831327	4411.459192	23.559808
113.645450	4416.030440	23.564826
113.637621	4411.019205	23.569843
113.610462	4422.007912	23.574861
114.021467	4435.882423	23.579879
113.835384	4435.734804	23.584896
114.517337	4435.075570	23.589914
114.320080	4441.883380	23.594931
114.945704	4445.077538	23.599949
113.963742	4457.175420	23.604967
114.316377	4455.257849	23.609984
114.768626	4468.734522	23.615002
114.739824	4468.044600	23.620019
114.867620	4472.670882	23.625037
114.892889	4489.961191	23.630055
114.776220	4483.947449	23.635072
114.970372	4493.313823	23.640090
115.319563	4503.845901	23.645107
115.401230	4511.162420	23.650125
115.090658	4527.413241	23.655143
115.843613	4527.554095	23.660160
115.959091	4535.654445	23.665178
115.914101	4528.862434	23.670195
116.342744	4542.317609	23.675213
115.997379	4564.233478	23.680231
116.825215	4562.547623	23.685248
116.791296	4559.907796	23.690266
116.996260	4556.845452	23.695283
117.293339	4561.517834	23.700301
116.724339	4563.191521	23.705319
117.316296	4561.694133	23.710336
117.226798	4554.991154	23.715354
117.116848	4554.774789	23.720371
117.210119	4557.910331	23.725389
117.254022	4575.557640	23.730407
117.631981	4572.171481	23.735424
117.946001	4584.221072	23.740442
117.819647	4579.831248	23.745459
117.404367	4587.231968	23.750477
117.734985	4608.410686	23.755495
117.738976	4601.348986	23.760512
117.884430	4615.555636	23.765530
118.459751	4627.671637	23.770547
118.381294	4632.447064	23.775565
118.180667	4645.132868	23.780583
118.334251	4640.086812	23.785600
118.770207	4658.165191	23.790618
118.944150	4665.842938	23.795635
119.046843	4666.597023	23.800653
118.947667	4671.767112	23.805671
119.094136	4677.103890	23.810688
119.475360	4682.586967	23.815706
119.420243	4691.556900	23.820723
119.649527	4687.105019	23.825741
119.974164	4707.855507	23.830759
120.217510	4710.339418	23.835776
120.019202	4712.611595	23.840794
120.137765	4714.546886	23.845811
120.639585	4707.792243	23.850829
120.104572	4717.146711	23.855847
120.230049	4728.342115	23.860864
120.581367	4741.481275	23.865882
120.359098	4746.140376	23.870899
121.087731	4747.295127	23.875917
120.677721	4764.878005	23.880935
120.655645	4770.831484	23.885952
121.220743	4766.427981	23.890970
121.343179	4774.300078	23.895987
121.753538	4783.515938	23.901005
121.339922	4789.281402	23.906023
121.790035	4786.969742	23.911040
121.989066	4796.427048	23.916058
121.875328	4815.538661	23.921075
122.502991	4809.146205	23.926093
122.669853	4816.029681	23.931111
122.427686	4813.450851	23.936128
122.385764	4808.643709	23.941146
122.066536	4809.691173	23.946163
122.744299	4821.958551	23.951181
122.653995	4827.550269	23.956199
122.587599	4839.624907	23.961216
122.596220	4847.887338	23.966234
122.773840	4852.496442	23.971251
123.176963	4844.551417	23.976269
123.258043	4862.455172	23.981287
123.848591	4880.064481	23.986304
123.817546	4886.638085	23.991322
124.070996	4888.164007	23.996339
124.750073	4888.411137	24.001357
124.610711	4895.276332	24.006375
124.379404	4880.378984	24.011392
124.685504	4880.927601	24.016410
124.654400	4888.902717	24.021427
125.035149	4877.185966	24.026445
124.640761	4879.327900	24.031463
124.404107	4890.943140	24.036480
124.833555	4900.474879	24.041498
124.200324	4909.993190	24.046515
124.769775	4918.496069	24.051533
124.738428	4937.645406	24.056551
125.155107	4943.214548	24.061568
125.468936	4937.928659	24.066586
125.183805	4957.992141	24.071603
125.886741	4961.196377	24.076621
125.659134	4958.990875	24.081639
126.049972	4968.572891	24.086656
126.080495	4977.071847	24.091674
126.089737	4990.078544	24.096691
126.317967	4986.466399	24.101709
126.340358	4988.353656	24.106727
126.845142	5001.784617	24.111744
127.334259	5007.216167	24.116762
127.380605	5015.065568	24.121779
127.593442	5014.025269	24.126797
127.535320	5008.693467	24.131815
127.325709	5010.254069	24.136832
127.246977	5010.869295	24.141850
127.438380	5017.420721	24.146867
127.515530	5028.437644	24.151885
128.031590	5038.135810	24.156903
127.786249	5034.408457	24.161920
127.821492	5043.942057	24.166938
127.580845	5053.061184	24.171955
128.076923	5056.758705	24.176973
128.070084	5069.648028	24.181991
128.489357	5082.656840	24.187008
128.535037	5084.357376	24.192026
128.577750	5090.708007	24.197043
129.002418	5103.406645	24.202061
129.343702	5120.398673	24.207079
129.176389	5117.741783	24.212096
128.918011	5116.781617	24.217114
128.956405	5130.061625	24.222131
129.294980	5134.942302	24.227149
129.676572	5141.227233	24.232167
129.382727	5156.686848	24.237184
130.010091	5158.211031	24.242202
130.038178	5167.733191	24.247219
130.400297	5161.445348	24.252237
130.437235	5179.987648	24.257255
129.957158	5195.713216	24.262272
130.873573	5197.425706	24.267290
131.013557	5195.655012	24.272307
131.432007	5191.296480	24.277325
131.408249	5198.686611	24.282343
131.687243	5217.342542	24.287360
131.535680	5216.103638	24.292378
131.460643	5219.372987	24.297395
131.395466	5218.527750	24.302413
131.622385	5213.488986	24.307431
131.731193	5222.764940	24.312448
131.839372	5238.215301	24.317466
132.217478	5245.709791	24.322483
131.999324	5241.684572	24.327501
132.547761	5251.431443	24.332519
132.793822	5261.771784	24.337536
133.084433	5259.548188	24.342554
133.079304	5269.015629	24.347571
133.053020	5272.479372	24.352589
133.170905	5260.822499	24.357607
133.248988	5271.047115	24.362624
133.529812	5259.538328	24.367642
133.802251	5261.165476	24.372659
133.988579	5255.220802	24.377677
133.409124	5256.324842	24.382695
133.288869	5275.845160	24.387712
133.590818	5286.861742	24.392730
133.657917	5291.904945	24.397747
133.561835	5304.767380	24.402765
133.895714	5308.152608	24.407783
133.974257	5327.720750	24.412800
134.269094	5331.800240	24.417818
134.252274	5343.700145	24.422835
134.314606	5355.710764	24.427853
134.687727	5348.385763	24.432871
134.489922	5369.932252	24.437888
135.042946	5377.146863	24.442906
134.898134	5393.827038	24.447923
135.258021	5398.006834	24.452941
135.605788	5412.532795	24.457959
135.995948	5426.720680	24.462976
135.791740	5419.593425	24.467994
136.131416	5435.979927	24.473011
136.540013	5439.378727	24.478029
136.758540	5444.294079	24.483047
136.522381	5442.490749	24.488064
136.701126	5435.682288	24.493082
136.545783	5447.127310	24.498099
136.885285	5463.649599	24.503117
137.078582	5464.294824	24.508135
137.287090	5473.002875	24.513152
137.353168	5459.352683	24.518170
137.020027	5476.630633	24.523187
137.469679	5490.708235	24.528205
137.537945	5489.785259	24.533223
137.776937	5502.090275	24.538240
138.204990	5519.176407	24.543258
137.877600	5523.665932	24.548275
138.135386	5530.453362	24.553293
138.268963	5530.606039	24.558311
138.436778	5545.232901	24.563328
138.763159	5546.955794	24.568346
138.799111	5558.497182	24.573363
138.619827	5569.930248	24.578381
139.179395	5575.410910	24.583399
139.132331	5588.363722	24.588416
139.592579	5579.976969	24.593434
139.306643	5594.981155	24.598451
139.559078	5599.433522	24.603469
139.742115	5609.061059	24.608487
140.195980	5605.104091	24.613504
140.354019	5617.267191	24.618522
140.517399	5627.298714	24.623539
140.445117	5627.830877	24.628557
140.805728	5619.680682	24.633575
140.954172	5624.951139	24.638592
140.563656	5620.564570	24.643610
141.036234	5638.622404	24.648627
140.922183	5647.220083	24.653645
141.297711	5649.645536	24.658663
141.241682	5654.872276	24.663680
141.276980	5663.658061	24.668698
141.565054	5674.446615	24.673715
141.606128	5673.392153	24.678733
141.730206	5675.443480	24.683751
142.033500	5685.724589	24.688768
142.184767	5693.046462	24.693786
142.403351	5702.138158	24.698803
142.264553	5701.007704	24.703821
142.516356	5709.298717	24.708839
142.426551	5729.480807	24.713856
142.659985	5727.685951	24.718874
142.622526	5723.992177	24.723891
142.539753	5742.083457	24.728909
143.229764	5748.604381	24.733927
143.186938	5759.492177	24.738944
143.496834	5772.180853	24.743962
143.654095	5773.077958	24.748979
143.525383	5775.932819	24.753997
144.000537	5786.073418	24.759015
143.662471	5794.576837	24.764032
143.645646	5798.575836	24.769050
143.990293	5821.723546	24.774067
144.124694	5828.359956	24.779085
144.549790	5836.851160	24.784103
144.757318	5859.294359	24.789120
145.022954	5843.346103	24.794138
144.854388	5864.333013	24.799155
145.023491	5881.100189	24.804173
145.455637	5884.261787	24.809191
145.294383	5887.844650	24.814208
145.906944	5902.619935	24.819226
146.340690	5903.653662	24.824243
146.208307	5901.875065	24.829261
146.632248	5902.635694	24.834279
146.554804	5903.225494	24.839296
146.472867	5911.729877	24.844314
147.147106	5926.520772	24.849331
147.185051	5927.878517	24.854349
147.060591	5936.121253	24.859367
147.346471	5941.480755	24.864384
147.493793	5936.176473	24.869402
147.670974	5940.214556	24.874419
147.477848	5949.168847	24.879437
147.890993	5953.141554	24.884455
147.369720	5958.166635	24.889472
147.772394	5967.687347	24.894490
147.827157	5979.238680	24.899507
148.069226	5989.908360	24.904525
148.245685	5989.830195	24.909543
148.222252	6015.810581	24.914560
148.395122	6010.082430	24.919578
148.791698	6024.749599	24.924595
149.044014	6036.519401	24.929613
149.322176	6031.450289	24.934631
149.336799	6040.754041	24.939648
149.693504	6053.492401	24.944666
149.765159	6065.255801	24.949683
149.708906	6063.654664	24.954701
150.204862	6062.156420	24.959719
149.969387	6067.288278	24.964736
150.008335	6077.333229	24.969754
150.133174	6082.575949	24.974771
150.201886	6092.957174	24.979789
150.627584	6095.996707	24.984807
150.199566	6114.404452	24.989824
150.572580	6121.467628	24.994842
151.302415	6130.716198	24.999859
151.121611	6147.519497	25.004877
151.122473	6140.729173	25.009895
151.118158	6155.838064	25.014912
151.989368	6166.706017	25.019930
151.688712	6164.931659	25.024947
151.643227	6180.277464	25.029965
152.175357	6186.832752	25.034983
152.160946	6197.760552	25.040000
152.373678	6196.985373	25.045018
152.138181	6212.206292	25.050035
152.580704	6220.729669	25.055053
153.084127	6223.555014	25.060071
153.237635	6220.642511	25.065088
153.166352	6240.332962	25.070106
153.747260	6245.984108	25.075123
153.806607	6249.226273	25.080141
153.959820	6245.833983	25.085159
153.791580	6242.422605	25.090176
153.991286	6243.969692	25.095194
154.164650	6262.494872	25.100211
154.108201	6276.462965	25.105229
153.963827	6262.093833	25.110247
154.541357	6282.629715	25.115264
154.181956	6298.274184	25.120282
154.895761	6291.716199	25.125299
154.521345	6303.606458	25.130317
154.768021	6310.638992	25.135335
154.985883	6326.335102	25.140352
155.210576	6342.696238	25.145370
155.080613	6353.168715	25.150387
155.370600	6365.305327	25.155405
155.922921	6373.192844	25.160423
156.156559	6377.439998	25.165440
156.017694	6397.804133	25.170458
156.148813	6407.815884	25.175475
156.573070	6411.196630	25.180493
156.585551	6419.654889	25.185511
156.628192	6431.937628	25.190528
156.857055	6434.190444	25.195546
157.028869	6446.626579	25.200563
157.132472	6465.914214	25.205581
157.144425	6466.234324	25.210599
157.587896	6477.592489	25.215616
157.660406	6488.721507	25.220634
158.027183	6492.038667	25.225651
158.188027	6511.023798	25.230669
159.002750	6512.414576	25.235687
158.784643	6518.067870	25.240704
158.716353	6515.092207	25.245722
158.837446	6523.135738	25.250739
158.988316	6529.141616	25.255757
159.251363	6538.507720	25.260775
159.265939	6540.639436	25.265792
159.450469	6556.299927	25.270810
160.015338	6556.650218	25.275827
159.709909	6551.994388	25.280845
159.998824	6558.376408	25.285863
159.998544	6574.182670	25.290880
159.983374	6582.351750	25.295898
160.206974	6581.240229	25.300915
160.618727	6606.013657	25.305933
160.759631	6609.075797	25.310951
161.069437	6613.879303	25.315968
161.188168	6622.586183	25.320986
160.897681	6639.145098	25.326003
161.068969	6636.179235	25.331021
161.199601	6645.247297	25.336039
161.886528	6665.769628	25.341056
161.706265	6682.967937	25.346074
162.184172	6668.024313	25.351091
161.919953	6692.556507	25.356109
162.050564	6698.672947	25.361127
162.407553	6705.760958	25.366144
162.320505	6718.701890	25.371162
163.009285	6725.479067	25.376179
162.759269	6729.940977	25.381197
162.810434	6745.704601	25.386215
162.915829	6757.567335	25.391232
163.154244	6753.987977	25.396250
163.665040	6766.712164	25.401267
163.785088	6783.481538	25.406285
163.661010	6787.945830	25.411303
163.909084	6784.295501	25.416320
164.048595	6807.467126	25.421338
164.180856	6818.628023	25.426355
164.192738	6825.078792	25.431373
164.453996	6837.397004	25.436391
164.912659	6837.861804	25.441408
164.797733	6843.265423	25.446426
164.897760	6859.450825	25.451443
165.770012	6866.865412	25.456461
165.307299	6867.357757	25.461479
165.605722	6883.180625	25.466496
165.481150	6896.114933	25.471514
165.791231	6899.100108	25.476531
165.839582	6916.859470	25.481549
165.955232	6916.554063	25.486567
166.064507	6929.426504	25.491584
166.655838	6939.543232	25.496602
166.746715	6953.504543	25.501619
166.905967	6961.147676	25.506637
167.002611	6966.783365	25.511655
167.516383	6979.564059	25.516672
167.549475	6991.706607	25.521690
167.594875	7004.462832	25.526707
167.739494	7010.798164	25.531725
168.223218	7016.966725	25.536743
168.341820	7021.879216	25.541760
167.936378	7029.055231	25.546778
168.506198	7044.144357	25.551795
168.865121	7054.016595	25.556813
168.878405	7066.430633	25.561831
169.266545	7069.829790	25.566848
169.095828	7081.606557	25.571866
169.606164	7081.387689	25.576883
169.612192	7101.471036	25.581901
169.714460	7096.287128	25.586919
170.174438	7106.336134	25.591936
169.967584	7124.741807	25.596954
170.697848	7127.724329	25.601971
170.568144	7128.035075	25.606989
170.721308	7127.976341	25.612007
170.801393	7141.074488	25.617024
170.819027	7151.202289	25.622042
171.081781	7151.139015	25.627059
171.429899	7171.512949	25.632077
171.343726	7185.476918	25.637095
171.237408	7184.562267	25.642112
171.507845	7206.766804	25.647130
171.638322	7209.960113	25.652147
171.949244	7226.892561	25.657165
171.897447	7243.736631	25.662183
172.366785	7252.609868	25.667200
172.672460	7262.506345	25.672218
173.309309	7265.449858	25.677236
173.489787	7268.502752	25.682253
173.100919	7273.513755	25.687271
173.514354	7284.930795	25.692288
173.764903	7292.821791	25.697306
174.077000	7297.789280	25.702324
174.039450	7292.766128	25.707341
173.887006	7306.052354	25.712359
174.035222	7314.183535	25.717376
174.606495	7325.547460	25.722394
174.444814	7323.520756	25.727412
174.261212	7337.108640	25.732429
174.411104	7339.323430	25.737447
175.075014	7355.300963	25.742464
174.894448	7371.584443	25.747482
175.309481	7370.190328	25.752500
175.437256	7373.017881	25.757517
175.712526	7387.282114	25.762535
175.917606	7402.933793	25.767552
175.868979	7408.731283	25.772570
175.732857	7427.432403	25.777588
176.247913	7431.278976	25.782605
176.194238	7450.166092	25.787623
176.512910	7458.671568	25.792640
177.124469	7478.862507	25.797658
177.020873	7483.402682	25.802676
177.109032	7485.917603	25.807693
176.949920	7488.370240	25.812711
177.264985	7498.959909	25.817728
177.476353	7528.769799	25.822746
177.646549	7526.946796	25.827764
178.435044	7553.162051	25.832781
178.362118	7561.795221	25.837799
178.834563	7572.401318	25.842816
178.816271	7569.490262	25.847834
179.189589	7585.254648	25.852852
179.182797	7590.351100	25.857869
179.346556	7595.203002	25.862887
179.298113	7597.423639	25.867904
179.838232	7620.877640	25.872922
179.312512	7624.783126	25.877940
180.054755	7623.126212	25.882957
179.613021	7647.450708	25.887975
180.313237	7660.351048	25.892992
180.522747	7679.342389	25.898010
180.950762	7681.093765	25.903028
181.418305	7689.111944	25.908045
181.338536	7704.372836	25.913063
181.378215	7700.780232	25.918080
180.892281	7713.206618	25.923098
181.360067	7729.508806	25.928116
181.470674	7741.447126	25.933133
182.240275	7757.796767	25.938151
182.157105	7762.324339	25.943168
182.534783	7774.299767	25.948186
182.351793	7786.650328	25.953204
182.923325	7786.213504	25.958221
182.738174	7799.675689	25.963239
183.566651	7802.854462	25.968256
183.908836	7810.122015	25.973274
183.437115	7806.300119	25.978292
183.683538	7813.273286	25.983309
183.451476	7831.169014	25.988327
184.017802	7839.869490	25.993344
184.126718	7859.470300	25.998362
184.138758	7869.457304	26.003380
184.771254	7878.191631	26.008397
184.242638	7901.974431	26.013415
184.827689	7899.104555	26.018432
184.549352	7917.168625	26.023450
185.034813	7922.942589	26.028468
185.660901	7936.372494	26.033485
185.245476	7949.754052	26.038503
186.105435	7967.617743	26.043520
185.864115	7980.501644	26.048538
186.262086	7977.354830	26.053556
186.198073	7984.837628	26.058573
186.416096	8007.344948	26.063591
186.485534	8010.955221	26.068608
186.456232	8016.377340	26.073626
186.786969	8025.594687	26.078644
187.370486	8041.632770	26.083661
187.559727	8066.960786	26.088679
187.580079	8066.313541	26.093696
187.418601	8080.965599	26.098714
187.379564	8095.162809	26.103732
188.621574	8101.481294	26.108749
188.436247	8120.844340	26.113767
188.730823	8123.907916	26.118784
188.937120	8130.098217	26.123802
189.130278	8140.540029	26.128820
188.918552	8148.974220	26.133837
188.957229	8146.960236	26.138855
189.018501	8165.836388	26.143872
189.642201	8175.942417	26.148890
189.766855	8196.365122	26.153908
190.081496	8184.966028	26.158925
190.550189	8217.890664	26.163943
190.534820	8221.533207	26.168960
190.569867	8235.548434	26.173978
191.101595	8248.049373	26.178996
191.173379	8254.456530	26.184013
191.542288	8254.281911	26.189031
191.670831	8257.093694	26.194048
192.038578	8275.284208	26.199066
192.078203	8285.491271	26.204084
192.355750	8275.575465	26.209101
192.410008	8293.512025	26.214119
192.718436	8297.539539	26.219136
192.545078	8308.998631	26.224154
192.759383	8318.426950	26.229172
193.009084	8331.057371	26.234189
192.781434	8338.398620	26.239207
193.323669	8358.980242	26.244224
193.372466	8366.454993	26.249242
193.475460	8379.307330	26.254260
194.199916	8385.533355	26.259277
193.861921	8406.120328	26.264295
194.286986	8409.769681	26.269312
194.541641	8430.459578	26.274330
194.835567	8445.536251	26.279348
194.901814	8449.333382	26.284365
194.738438	8459.856486	26.289383
195.261435	8467.601118	26.294400
195.309544	8490.994392	26.299418
195.389251	8508.507272	26.304436
195.659568	8518.406806	26.309453
195.669221	8542.364986	26.314471
196.059965	8551.361666	26.319488
196.272597	8563.076161	26.324506
196.672262	8583.531982	26.329524
196.730275	8590.111900	26.334541
197.078476	8611.699767	26.339559
197.494324	8618.185750	26.344576
197.567325	8627.724765	26.349594
197.438701	8639.742187	26.354612
197.837522	8648.844994	26.359629
197.989517	8661.434118	26.364647
198.327195	8677.981689	26.369664
198.584631	8686.705701	26.374682
198.670186	8698.512805	26.379700
199.006207	8698.703256	26.384717
199.062750	8709.507768	26.389735
199.058274	8724.085222	26.394752
199.486769	8735.867038	26.399770
199.431315	8753.811760	26.404788
199.822330	8760.570045	26.409805
200.102744	8760.128296	26.414823
199.988478	8771.013276	26.419840
200.140929	8788.682356	26.424858
200.280900	8800.086349	26.429876
201.044216	8799.221654	26.434893
200.881455	8815.775132	26.439911
200.880293	8831.851826	26.444928
201.219178	8835.732613	26.449946
201.340689	8863.099261	26.454964
201.910208	8863.382579	26.459981
201.871009	8880.895496	26.464999
201.866232	8889.872216	26.470016
201.962940	8897.983749	26.475034
202.457177	8919.659600	26.480052
203.006110	8924.978768	26.485069
202.776599	8943.288764	26.490087
203.081515	8959.507053	26.495104
203.339659	8962.124992	26.500122
203.550394	8989.411546	26.505140
203.617321	8993.353915	26.510157
203.904623	9016.786152	26.515175
203.530582	9019.181100	26.520192
204.102655	9035.970108	26.525210
204.611624	9063.055343	26.530228
204.556446	9064.832038	26.535245
205.186683	9089.770326	26.540263
205.287450	9095.541782	26.545280
205.566441	9102.024117	26.550298
205.951660	9119.972773	26.555316
206.483707	9125.935569	26.560333
206.514811	9129.665728	26.565351
206.309269	9140.022173	26.570368
206.841585	9161.487120	26.575386
206.686048	9154.814907	26.580404
207.149921	9172.656574	26.585421
207.248284	9182.381338	26.590439
207.267708	9186.801623	26.595456
207.525109	9199.684013	26.600474
207.888535	9212.038323	26.605492
207.795509	9227.270971	26.610509
207.654940	9238.997024	26.615527
208.145824	9242.601502	26.620544
208.197000	9265.856350	26.625562
208.531823	9290.077124	26.630580
209.061862	9300.498388	26.635597
209.600940	9321.930889	26.640615
209.754148	9325.695632	26.645632
210.308606	9342.465577	26.650650
210.282896	9355.881809	26.655668
210.356269	9349.502024	26.660685
210.023887	9359.234372	26.665703
210.624895	9371.235838	26.670720
210.843919	9379.609420	26.675738
211.114678	9397.655208	26.680756
210.904055	9398.701689	26.685773
211.221112	9416.329793	26.690791
211.227062	9434.224506	26.695808
211.726549	9445.664136	26.700826
211.419441	9464.302531	26.705844
211.897421	9480.045823	26.710861
212.308097	9490.953177	26.715879
212.478613	9505.235456	26.720896
212.975681	9515.958795	26.725914
212.927551	9533.577916	26.730932
213.253316	9551.122693	26.735949
213.233796	9560.285172	26.740967
213.486060	9579.609599	26.745984
214.167838	9583.443141	26.751002
213.988423	9584.519474	26.756020
214.324772	9602.501511	26.761037
214.296722	9610.759194	26.766055
214.730361	9615.531460	26.771072
214.613592	9634.399108	26.776090
214.910622	9645.043353	26.781108
215.609428	9660.815351	26.786125
215.653572	9669.052277	26.791143
215.923868	9685.257680	26.796160
215.703483	9687.423410	26.801178
216.040927	9703.008939	26.806196
216.331883	9719.173245	26.811213
216.798466	9733.567186	26.816231
216.517088	9749.066570	26.821248
216.380432	9752.737886	26.826266
217.081532	9769.068471	26.831284
217.606544	9786.168640	26.836301
217.553613	9807.612354	26.841319
217.749275	9824.442101	26.846336
218.123268	9833.454660	26.851354
218.384554	9844.372996	26.856372
218.354432	9868.108625	26.861389
218.466937	9874.585739	26.866407
218.792896	9894.543055	26.871424
219.052481	9904.372392	26.876442
219.265492	9930.996918	26.881460
219.769801	9932.622898	26.886477
219.716269	9943.075954	26.891495
219.744940	9960.658188	26.896512
220.542068	9974.460616	26.901530
220.441318	9996.575094	26.906548
220.766983	10003.224091	26.911565
221.142743	10023.899949	26.916583
221.277174	10035.296095	26.921600
221.521024	10035.109484	26.926618
221.506106	10057.952580	26.931636
221.728134	10067.617387	26.936653
222.563112	10079.740531	26.941671
222.039712	10094.810816	26.946688
222.742801	10107.845035	26.951706
222.601886	10126.230718	26.956724
223.083903	10145.080856	26.961741
223.411248	10147.309232	26.966759
223.224070	10166.674693	26.971776
223.282325	10174.072910	26.976794
223.356624	10193.656347	26.981812
224.022550	10208.518304	26.986829
224.197774	10235.010255	26.991847
224.260991	10236.762198	26.996864
224.812067	10265.516039	27.001882
225.175386	10276.226039	27.006900
225.015225	10292.032100	27.011917
225.353955	10305.935005	27.016935
225.577433	10323.831225	27.021952
226.177062	10332.060359	27.026970
226.558625	10348.211018	27.031988
226.532340	10355.073151	27.037005
226.794433	10371.886670	27.042023
226.677453	10376.619094	27.047040
227.238238	10392.814336	27.052058
227.412777	10411.056157	27.057076
227.533589	10419.540317	27.062093
227.598314	10427.689101	27.067111
227.695701	10452.008575	27.072128
228.391605	10458.710247	27.077146
228.318050	10482.039828	27.082164
228.442994	10497.233049	27.087181
228.809135	10497.393546	27.092199
229.031168	10514.980741	27.097216
229.223369	10526.563902	27.102234
229.314627	10545.175698	27.107252
229.510110	10560.250565	27.112269
229.907620	10564.627734	27.117287
230.011728	10586.843431	27.122304
230.349030	10585.653875	27.127322
230.408719	10607.939705	27.132340
230.936821	10619.792369	27.137357
231.256850	10627.910718	27.142375
231.031260	10645.157682	27.147392
231.611929	10657.545229	27.152410
231.834001	10672.066612	27.157428
231.580266	10691.269377	27.162445
231.965099	10710.100579	27.167463
232.710010	10721.919343	27.172480
232.818243	10733.749444	27.177498
233.034478	10765.508807	27.182516
232.770761	10773.443961	27.187533
233.032493	10782.657705	27.192551
233.644945	10811.917452	27.197568
233.952040	10806.984605	27.202586
234.032800	10827.773877	27.207604
234.237971	10847.438537	27.212621
234.364485	10867.200794	27.217639
234.633587	10879.646771	27.222656
235.073564	10891.731285	27.227674
235.325345	10910.798246	27.232692
235.498671	10931.910991	27.237709
235.765512	10945.459357	27.242727
236.008171	10964.805668	27.247744
236.147218	10977.044738	27.252762
236.425663	10986.423316	27.257780
236.904420	11005.022227	27.262797
237.046322	11010.055274	27.267815
237.037215	11027.691790	27.272832
237.447505	11040.551503	27.277850
237.847696	11062.702435	27.282868
237.738385	11081.387232	27.287885
238.004668	11091.566639	27.292903
238.520352	11114.608927	27.297920
238.835523	11121.345224	27.302938
239.373810	11135.978467	27.307956
239.598684	11152.185944	27.312973
239.850331	11159.127977	27.317991
239.401615	11169.122621	27.323008
240.220580	11186.692716	27.328026
239.893310	11199.143918	27.333044
240.048449	11222.201771	27.338061
240.524116	11233.734648	27.343079
240.934427	11254.055960	27.348096
241.219158	11272.268726	27.353114
241.300719	11284.403328	27.358132
241.523224	11298.082042	27.363149
242.123193	11310.438581	27.368167
242.277476	11324.086952	27.373184
242.204255	11336.687904	27.378202
242.639568	11353.216243	27.383220
242.760212	11372.108443	27.388237
243.197744	11382.276970	27.393255
243.102032	11401.995662	27.398272
243.689897	11418.891709	27.403290
243.717648	11427.842449	27.408308
243.908794	11443.919682	27.413325
244.205501	11455.518623	27.418343
243.877825	11467.057502	27.423360
244.054507	11488.533478	27.428378
244.740414	11501.874503	27.433396
244.453318	11525.090421	27.438413
245.066269	11529.257240	27.443431
245.550500	11555.348991	27.448448
245.493112	11578.421629	27.453466
245.925864	11591.530815	27.458484
246.346375	11608.374309	27.463501
246.413186	11627.767797	27.468519
246.508037	11643.276115	27.473536
246.988698	11659.829197	27.478554
246.905175	11677.626393	27.483572
247.252204	11702.606230	27.488589
247.416159	11710.825285	27.493607
247.481926	11733.162021	27.498624
248.204773	11744.738592	27.503642
248.229369	11770.697396	27.508660
248.451639	11790.423520	27.513677
249.304718	11797.817857	27.518695
249.299537	11820.652100	27.523712
249.705579	11835.218192	27.528730
249.926104	11841.110675	27.533748
249.530000	11870.334293	27.538765
250.438144	11895.103333	27.543783
250.443644	11905.560865	27.548800
250.770041	11923.474067	27.553818
251.082328	11945.005107	27.558836
250.879747	11961.539180	27.563853
251.529226	11983.822665	27.568871
251.850687	11989.576231	27.573888
252.511863	12008.153877	27.578906
252.943017	12014.651285	27.583924
252.537056	12037.479104	27.588941
253.025834	12046.171608	27.593959
253.203146	12060.202152	27.598976
253.268189	12092.123225	27.603994
253.803600	12097.830678	27.609012
253.650086	12118.692812	27.614029
254.541443	12132.368403	27.619047
254.052365	12147.071803	27.624064
254.644377	12163.232112	27.629082
255.157592	12173.120801	27.634100
255.021957	12209.567027	27.639117
255.694990	12218.357058	27.644135
255.733966	12239.732310	27.649152
255.450796	12260.412813	27.654170
256.267113	12268.444656	27.659188
256.304846	12298.510416	27.664205
256.270275	12308.459728	27.669223
256.764145	12327.098635	27.674240
257.121154	12356.546068	27.679258
257.294802	12363.579712	27.684276
257.678901	12390.190399	27.689293
257.667114	12405.485528	27.694311
257.952057	12424.182523	27.699328
258.260276	12441.467502	27.704346
258.978446	12460.984015	27.709364
258.719115	12481.683130	27.714381
258.901399	12493.269059	27.719399
259.689933	12514.325099	27.724416
259.649957	12536.155151	27.729434
260.204463	12550.774328	27.734452
260.151878	12577.709473	27.739469
260.734635	12590.382181	27.744487
260.744500	12598.742603	27.749504
260.811827	12621.395932	27.754522
261.645359	12636.119884	27.759540
261.661276	12647.779337	27.764557
261.962755	12659.517220	27.769575
262.374082	12667.631626	27.774592
262.386720	12686.065226	27.779610
262.627542	12702.309434	27.784628
262.688126	12724.329212	27.789645
262.817399	12741.610920	27.794663
263.570935	12753.754883	27.799680
263.670240	12772.781303	27.804698
264.077007	12798.154285	27.809716
263.841066	12807.573301	27.814733
264.275260	12821.949432	27.819751
264.552039	12834.746027	27.824768
264.930316	12857.199348	27.829786
265.211219	12873.090056	27.834804
265.303375	12901.281934	27.839821
265.635148	12904.002584	27.844839
266.081941	12923.783142	27.849856
266.035494	12949.565220	27.854874
266.754994	12965.412561	27.859892
266.668428	12985.643054	27.864909
267.161118	12997.070139	27.869927
267.454564	13017.831667	27.874944
267.660357	13041.464867	27.879962
268.394383	13052.446807	27.884980
268.047521	13071.682369	27.889997
268.378269	13082.452763	27.895015
268.776053	13101.208542	27.900032
268.901285	13119.735453	27.905050
268.956833	13139.849110	27.910068
269.340650	13179.910616	27.915085
269.688279	13190.940537	27.920103
270.063936	13209.241987	27.925120
269.802405	13243.511991	27.930138
270.475031	13244.025569	27.935156
270.485548	13263.063232	27.940173
271.036834	13278.839292	27.945191
271.954791	13312.435166	27.950208
271.880812	13330.380845	27.955226
271.752664	13344.984418	27.960244
272.419888	13367.440450	27.965261
272.974307	13363.055582	27.970279
272.924389	13395.776883	27.975296
272.719558	13402.431245	27.980314
273.571166	13415.555038	27.985332
273.498827	13444.983001	27.990349
273.800690	13465.617381	27.995367
274.155506	13484.326585	28.000384
274.320083	13508.680531	28.005402
274.391210	13523.101440	28.010420
274.886480	13550.375315	28.015437
274.760555	13571.013664	28.020455
275.430289	13591.893722	28.025472
275.676852	13618.088719	28.030490
276.066049	13631.585113	28.035508
276.347152	13661.444378	28.040525
276.675177	13676.191490	28.045543
277.159162	13692.032124	28.050560
276.959334	13710.920021	28.055578
277.126924	13735.671698	28.060596
277.670290	13752.564182	28.065613
277.969512	13771.863458	28.070631
278.096264	13793.353033	28.075648
278.564480	13821.910546	28.080666
279.197116	13832.930933	28.085684
279.304607	13853.147740	28.090701
279.440685	13867.328197	28.095719
279.619494	13880.128213	28.100736
279.680183	13912.005663	28.105754
280.182414	13925.816156	28.110772
280.180632	13947.417625	28.115789
280.895582	13961.349567	28.120807
281.087514	13985.990382	28.125824
280.987786	13997.018216	28.130842
281.260987	14004.396897	28.135860
281.658904	14031.288796	28.140877
281.646436	14056.075413	28.145895
282.290701	14066.538290	28.150912
282.043504	14097.996884	28.155930
283.031778	14116.661168	28.160948
282.852920	14141.953992	28.165965
282.650523	14159.336320	28.170983
283.490389	14185.767600	28.176000
283.563522	14217.150945	28.181018
284.138942	14240.152957	28.186036
284.270077	14266.793276	28.191053
284.861429	14289.600206	28.196071
285.342700	14316.687888	28.201088
285.754359	14328.949587	28.206106
285.548479	14349.013890	28.211124
286.050232	14366.807193	28.216141
286.383007	14389.635801	28.221159
286.775461	14406.719889	28.226176
286.825215	14426.027328	28.231194
287.137246	14443.916744	28.236212
287.588981	14465.684617	28.241229
288.231418	14492.254630	28.246247
288.432771	14507.912833	28.251264
288.506365	14530.892747	28.256282
288.942653	14547.401625	28.261300
288.981495	14570.345974	28.266317
289.346476	14595.743697	28.271335
289.736711	14615.354865	28.276352
289.911615	14634.914513	28.281370
290.093493	14642.241427	28.286388
290.296778	14672.439761	28.291405
290.456095	14693.220973	28.296423
290.856830	14717.940562	28.301440
291.115685	14736.280731	28.306458
291.929163	14773.413799	28.311476
291.783074	14777.656039	28.316493
292.232651	14806.546404	28.321511
292.965832	14823.050070	28.326528
293.023033	14840.089160	28.331546
293.448557	14870.445645	28.336564
293.766836	14881.853818	28.341581
293.943497	14904.754872	28.346599
294.038560	14913.046117	28.351616
294.088887	14931.851817	28.356634
294.428906	14958.836210	28.361652
294.820250	14980.743620	28.366669
294.990564	15014.630171	28.371687
295.438852	15024.075741	28.376704
295.926078	15048.295839	28.381722
295.972388	15070.642708	28.386740
296.013581	15093.596792	28.391757
296.193071	15127.750559	28.396775
296.796079	15152.356909	28.401792
297.065782	15175.553223	28.406810
297.504192	15197.273487	28.411828
297.997009	15219.095792	28.416845
297.932571	15240.193737	28.421863
298.001320	15255.753311	28.426880
298.459298	15290.767014	28.431898
299.091148	15313.338271	28.436916
299.278476	15331.393336	28.441933
299.681416	15345.536246	28.446951
299.981263	15353.814553	28.451968
300.343305	15376.361826	28.456986
300.702044	15398.454846	28.462004
301.133351	15411.718509	28.467021
300.822974	15423.342342	28.472039
301.462787	15445.410336	28.477056
301.415551	15464.415025	28.482074
301.909507	15492.538320	28.487092
302.342784	15511.710975	28.492109
302.407130	15539.930062	28.497127
302.734291	15559.924764	28.502144
302.834433	15584.597812	28.507162
303.065643	15609.048226	28.512180
303.625867	15621.265377	28.517197
303.825002	15657.015135	28.522215
304.141809	15673.970083	28.527232
304.291913	15702.289675	28.532250
304.656402	15729.375547	28.537268
305.164185	15752.329970	28.542285
305.486878	15784.052637	28.547303
305.936110	15805.996142	28.552320
306.253964	15823.860672	28.557338
306.229830	15853.148979	28.562356
306.514190	15864.818882	28.567373
306.665906	15902.544200	28.572391
307.590350	15931.867220	28.577408
307.720821	15944.464581	28.582426
308.316760	15965.952586	28.587444
308.838411	15988.797735	28.592461
308.943131	16018.018732	28.597479
309.215344	16024.245530	28.602496
309.308442	16049.106625	28.607514
309.362793	16083.414349	28.612532
310.052274	16100.361831	28.617549
310.082919	16127.513194	28.622567
310.374595	16136.547985	28.627584
310.724062	16165.456083	28.632602
311.040617	16192.995458	28.637620
311.067634	16223.767101	28.642637
311.496840	16251.551064	28.647655
311.562799	16282.117717	28.652672
311.839583	16316.659482	28.657690
312.722122	16341.466776	28.662708
313.195391	16354.961405	28.667725
313.606749	16393.414521	28.672743
313.696807	16416.229874	28.677760
314.412630	16432.952431	28.682778
314.192832	16452.117783	28.687796
314.636158	16474.359874	28.692813
314.717172	16504.564454	28.697831
315.135603	16527.167417	28.702848
315.533072	16547.613275	28.707866
315.894041	16582.211816	28.712884
316.324680	16597.952675	28.717901
316.513518	16627.575185	28.722919
316.545852	16647.073939	28.727936
316.795180	16672.344081	28.732954
317.143723	16698.416773	28.737972
317.917907	16722.992011	28.742989
318.306918	16756.942133	28.748007
318.475666	16780.310968	28.753024
318.655718	16802.259875	28.758042
318.903029	16824.722589	28.763060
319.691736	16842.735407	28.768077
319.963198	16868.902526	28.773095
320.115905	16888.404778	28.778112
320.688969	16907.787506	28.783130
320.348931	16938.011343	28.788148
321.056961	16950.041945	28.793165
321.372194	16979.834710	28.798183
321.461827	17002.436040	28.803200
321.614384	17027.592305	28.808218
321.929229	17048.105333	28.813236
322.359854	17070.962869	28.818253
322.279605	17101.841155	28.823271
322.821351	17130.373136	28.828288
323.186407	17154.472894	28.833306
323.800124	17184.377148	28.838324
324.414208	17210.339446	28.843341
324.241118	17228.301137	28.848359
324.527966	17253.885184	28.853376
325.239647	17274.266800	28.858394
325.268735	17301.331617	28.863412
325.268005	17329.607738	28.868429
326.006249	17355.721349	28.873447
326.055895	17386.826115	28.878464
326.503920	17402.296424	28.883482
326.697166	17429.973751	28.888500
327.205963	17452.307793	28.893517
327.332314	17478.738527	28.898535
327.958524	17504.869889	28.903552
328.321930	17542.350464	28.908570
328.506188	17573.668185	28.913588
329.505277	17581.901094	28.918605
329.168682	17606.275577	28.923623
329.718340	17644.491573	28.928640
329.802560	17664.232760	28.933658
329.993626	17696.705691	28.938676
330.735137	17717.822236	28.943693
331.141388	17751.802993	28.948711
331.272699	17781.802691	28.953728
331.818547	17804.965234	28.958746
331.999241	17826.940473	28.963764
332.287543	17848.355582	28.968781
332.535087	17882.588855	28.973799
332.886610	17913.249179	28.978816
333.515035	17938.629006	28.983834
333.574174	17968.513948	28.988852
333.715809	17986.856628	28.993869
334.123471	18017.603085	28.998887
334.469118	18044.183444	29.003904
334.829968	18079.953420	29.008922
334.719826	18103.408602	29.013940
335.749649	18135.416052	29.018957
336.092889	18180.943223	29.023975
336.270943	18203.500515	29.028992
336.865317	18229.372507	29.034010
336.930469	18264.999616	29.039028
337.786254	18282.131451	29.044045
337.955210	18305.979071	29.049063
338.159111	18333.131659	29.054080
338.490852	18355.008023	29.059098
339.047318	18384.588269	29.064116
339.175511	18400.715967	29.069133
339.419008	18427.439205	29.074151
339.923747	18456.035796	29.079168
340.636065	18480.828288	29.084186
341.011175	18492.596126	29.089204
340.776963	18524.050424	29.094221
341.286962	18550.694179	29.099239
341.406259	18568.352282	29.104256
341.878948	18591.072354	29.109274
341.846420	18624.731675	29.114292
342.191930	18658.679310	29.119309
342.866825	18686.636771	29.124327
343.164884	18716.396990	29.129344
343.740468	18727.672374	29.134362
343.840419	18765.834669	29.139380
344.221348	18785.239901	29.144397
344.560808	18809.680567	29.149415
344.906193	18830.190698	29.154432
345.605087	18853.191529	29.159450
345.797492	18874.673334	29.164468
345.948160	18897.229402	29.169485
345.793825	18921.520119	29.174503
346.540671	18946.004543	29.179520
346.778745	18964.118233	29.184538
346.978995	18998.379832	29.189556
347.370009	19020.531962	29.194573
347.700815	19055.228093	29.199591
348.098902	19086.565297	29.204608
348.708284	19107.754600	29.209626
348.487801	19145.121240	29.214644
349.093211	19174.259089	29.219661
349.770330	19202.741326	29.224679
349.393749	19240.240003	29.229696
349.828380	19262.922596	29.234714
350.361697	19293.493439	29.239732
350.940508	19330.678369	29.244749
351.758431	19367.800642	29.249767
351.804922	19397.525491	29.254784
352.478536	19420.410913	29.259802
352.785603	19438.179385	29.264820
353.032934	19466.261803	29.269837
353.646391	19488.752380	29.274855
353.640453	19518.245543	29.279872
354.074819	19537.839011	29.284890
354.357729	19578.242386	29.289908
354.595876	19597.512843	29.294925
355.054790	19624.949501	29.299943
355.463536	19660.045168	29.304960
355.923032	19681.612382	29.309978
355.913024	19716.249348	29.314996
356.267957	19750.026819	29.320013
356.648966	19768.895985	29.325031
356.513524	19797.980227	29.330048
356.862240	19839.485810	29.335066
357.380920	19873.256798	29.340084
358.209868	19908.293405	29.345101
358.785161	19926.664751	29.350119
359.109236	19962.879891	29.355136
359.258833	19986.315600	29.360154
359.632900	20018.441509	29.365172
360.174250	20049.056503	29.370189
360.468900	20085.263842	29.375207
360.732419	20125.513428	29.380224
361.236912	20144.445750	29.385242
361.304958	20180.726669	29.390260
361.305544	20216.436949	29.395277
361.874122	20245.689575	29.400295
362.080575	20284.488922	29.405312
362.776334	20304.471852	29.410330
363.297034	20341.301349	29.415348
363.497123	20373.353999	29.420365
363.867911	20409.486827	29.425383
363.857284	20434.015953	29.430400
365.021700	20461.090541	29.435418
365.662181	20499.607506	29.440436
364.968008	20526.865907	29.445453
365.877767	20557.461897	29.450471
366.363595	20585.925569	29.455488
366.742341	20615.998272	29.460506
367.310990	20644.929248	29.465524
367.464455	20666.210613	29.470541
367.668684	20684.855619	29.475559
368.044888	20728.153185	29.480576
368.775304	20745.009870	29.485594
368.544815	20763.173348	29.490612
369.236384	20793.936571	29.495629
369.821202	20822.012295	29.500647
369.834721	20854.120226	29.505664
370.216819	20871.296953	29.510682
370.701606	20896.298754	29.515700
370.862816	20936.344883	29.520717
371.804209	20950.609736	29.525735
371.062752	20981.629316	29.530752
371.784142	21005.001948	29.535770
372.215222	21034.037186	29.540788
372.542145	21072.951905	29.545805
373.074555	21106.969286	29.550823
373.114772	21131.061659	29.555840
373.721759	21162.559016	29.560858
373.433372	21210.239365	29.565876
374.405451	21240.864570	29.570893
374.968392	21281.044345	29.575911
375.185226	21320.735021	29.580928
375.665327	21353.636320	29.585946
375.873996	21378.833631	29.590964
376.274673	21425.452460	29.595981
376.942568	21451.393027	29.600999
376.700563	21488.072442	29.606016
377.528963	21513.033840	29.611034
377.974808	21547.457294	29.616052
377.976207	21586.468246	29.621069
378.563203	21619.018356	29.626087
378.794173	21647.144365	29.631104
378.996401	21677.094690	29.636122
379.871200	21727.658633	29.641140
380.187418	21769.817883	29.646157
380.956955	21791.800116	29.651175
380.665132	21830.490994	29.656192
381.488469	21860.476999	29.661210
381.553421	21900.394829	29.666228
381.750904	21925.929482	29.671245
382.494497	21970.056848	29.676263
383.457754	22005.790179	29.681280
383.594778	22039.858463	29.686298
384.144632	22063.455103	29.691316
384.169118	22095.683390	29.696333
385.015323	22127.915709	29.701351
385.268052	22161.776515	29.706368
384.845972	22188.880839	29.711386
385.765345	22214.789337	29.716404
386.028366	22263.390541	29.721421
386.456268	22284.504285	29.726439
386.603651	22319.266500	29.731456
387.101500	22369.183416	29.736474
387.598478	22397.294099	29.741492
387.805016	22435.130869	29.746509
388.541476	22465.744335	29.751527
388.715091	22496.641898	29.756544
389.098852	22539.259805	29.761562
389.689104	22565.157127	29.766580
389.772251	22599.948852	29.771597
390.604898	22629.378498	29.776615
390.343194	22659.181813	29.781632
390.897122	22690.942676	29.786650
391.667796	22730.865374	29.791668
391.446389	22772.769743	29.796685
392.287219	22811.537873	29.801703
392.117222	22848.884656	29.806720
392.545896	22885.183558	29.811738
393.055319	22917.337216	29.816756
393.333043	22952.610923	29.821773
393.868570	22987.793758	29.826791
394.736348	23031.347956	29.831808
394.880865	23058.156180	29.836826
395.412583	23084.910108	29.841844
395.044002	23119.078397	29.846861
395.807890	23151.413744	29.851879
396.381381	23193.535718	29.856896
396.661852	23230.604123	29.861914
397.103282	23260.039113	29.866932
396.780923	23301.094679	29.871949
398.024815	23345.184653	29.876967
398.186787	23386.113976	29.881984
398.543109	23417.711058	29.887002
399.060217	23459.362167	29.892020
399.666696	23495.046642	29.897037
399.871965	23534.806748	29.902055
400.612197	23573.175051	29.907072
400.634055	23605.526258	29.912090
401.420815	23641.833642	29.917108
401.797226	23676.296942	29.922125
402.194754	23703.426601	29.927143
402.470570	23741.476177	29.932160
402.755948	23774.317202	29.937178
403.393953	23807.134644	29.942196
403.468466	23850.644268	29.947213
403.883742	23887.458961	29.952231
404.548784	23919.520349	29.957248
404.831934	23968.173113	29.962266
405.231058	24004.327016	29.967284
405.619230	24051.680695	29.972301
406.287183	24077.719482	29.977319
406.654899	24115.249820	29.982336
407.265992	24151.604606	29.987354
407.486455	24181.549525	29.992372
407.999316	24230.034236	29.997389
408.509896	24253.108794	30.002407
408.480226	24292.389009	30.007424
409.121983	24327.804028	30.012442
409.702855	24368.094671	30.017460
409.601176	24399.809282	30.022477
410.661800	24436.997866	30.027495
410.765224	24474.507079	30.032512
411.616406	24517.157108	30.037530
411.766907	24550.652490	30.042548
411.701630	24573.577475	30.047565
412.325530	24608.332232	30.052583
412.521695	24654.984340	30.057600
412.836757	24702.357328	30.062618
413.679252	24727.074100	30.067636
413.640727	24768.006054	30.072653
414.645846	24805.557917	30.077671
414.749122	24844.439208	30.082688
415.213006	24887.289723	30.087706
416.053831	24927.357501	30.092724
416.002926	24969.069125	30.097741
416.408869	25000.199594	30.102759
416.552286	25050.867580	30.107776
417.227535	25082.948192	30.112794
418.067023	25116.930653	30.117812
418.254871	25162.030582	30.122829
418.985351	25203.778293	30.127847
419.134268	25233.603272	30.132864
419.414390	25274.012359	30.137882
419.783859	25303.809216	30.142900
420.626859	25332.931562	30.147917
420.830542	25366.280936	30.152935
421.530529	25391.096688	30.157952
421.704426	25435.200880	30.162970
422.167869	25452.419385	30.167988
422.274229	25493.494435	30.173005
422.906947	25533.381144	30.178023
423.108075	25572.058916	30.183040
423.312818	25596.655459	30.188058
424.273466	25626.473952	30.193076
424.612129	25673.150338	30.198093
424.932847	25712.681797	30.203111
425.160488	25748.227387	30.208128
425.320825	25781.773836	30.213146
425.960770	25810.227164	30.218164
426.228782	25852.181378	30.223181
426.790191	25891.896686	30.228199
427.332459	25936.064353	30.233216
427.457606	25978.755368	30.238234
428.117971	26016.060134	30.243252
428.063957	26057.989375	30.248269
428.689420	26100.223077	30.253287
429.665144	26145.340836	30.258304
429.825189	26191.041505	30.263322
430.246788	26224.541445	30.268340
430.475940	26273.138718	30.273357
430.975044	26310.083760	30.278375
431.708769	26347.586212	30.283392
431.788836	26398.646709	30.288410
432.558317	26437.875449	30.293428
433.165304	26476.194331	30.298445
433.388784	26516.444131	30.303463
433.799512	26564.849338	30.308480
434.173415	26605.107353	30.313498
434.838930	26637.299409	30.318516
435.179776	26675.154737	30.323533
435.203511	26721.541577	30.328551
436.109436	26767.139355	30.333568
436.369903	26811.795491	30.338586
436.683724	26841.179873	30.343604
436.998016	26891.035668	30.348621
437.952851	26930.267931	30.353639
438.384315	26969.556966	30.358656
438.318319	27020.028832	30.363674
439.322741	27058.817473	30.368692
439.798041	27097.379369	30.373709
440.093658	27141.341804	30.378727
440.632715	27171.671043	30.383744
441.060120	27221.231834	30.388762
441.803640	27257.211219	30.393780
441.678157	27294.319090	30.398797
442.294102	27337.909434	30.403815
442.725479	27372.895043	30.408832
443.228899	27417.337482	30.413850
443.845109	27459.979976	30.418868
444.425598	27502.331092	30.423885
444.778545	27534.864273	30.428903
445.217315	27570.923551	30.433920
445.327952	27624.889774	30.438938
446.096740	27660.050566	30.443956
446.334362	27699.889658	30.448973
446.729043	27739.546213	30.453991
447.211252	27784.460497	30.459008
447.712351	27819.221053	30.464026
448.091375	27868.784677	30.469044
448.500945	27904.368752	30.474061
448.980683	27951.021959	30.479079
449.127636	27988.897460	30.484096
449.625106	28028.784982	30.489114
450.475595	28061.835215	30.494132
450.946553	28105.070670	30.499149
451.089625	28138.718524	30.504167
451.709862	28175.717512	30.509184
451.595303	28220.517646	30.514202
452.427192	28253.950346	30.519220
452.831121	28287.987396	30.524237
453.430177	28335.235903	30.529255
454.018571	28378.756939	30.534272
454.437105	28416.356825	30.539290
454.408636	28460.726828	30.544308
454.904934	28491.210108	30.549325
455.036959	28534.107669	30.554343
456.012540	28575.937710	30.559360
456.387344	28617.059192	30.564378
456.497381	28677.165816	30.569396
457.282103	28717.388941	30.574413
457.361632	28762.273633	30.579431
458.112032	28813.323670	30.584448
458.559954	28859.200141	30.589466
459.571181	28904.944237	30.594484
459.381889	28946.078882	30.599501
459.742375	28994.004691	30.604519
460.428008	29029.838247	30.609536
460.618058	29084.977899	30.614554
461.425114	29129.610379	30.619572
462.446606	29168.349796	30.624589
462.589103	29211.518935	30.629607
463.224167	29251.494746	30.634624
463.364435	29304.904502	30.639642
463.643355	29343.792166	30.644660
464.710603	29391.273185	30.649677
464.754458	29445.406366	30.654695
465.506358	29477.671552	30.659712
465.795097	29535.047264	30.664730
466.347253	29575.738335	30.669748
466.901187	29616.732624	30.674765
467.116294	29668.462819	30.679783
467.767372	29695.074060	30.684800
468.520123	29762.497917	30.689818
469.001046	29798.320630	30.694836
469.532364	29831.019156	30.699853
469.637321	29879.676063	30.704871
470.361607	29917.306662	30.709888
470.507052	29973.011946	30.714906
471.046838	30009.344149	30.719924
472.132149	30054.838996	30.724941
471.930354	30102.324467	30.729959
472.402281	30147.378283	30.734976
472.617703	30189.924882	30.739994
473.410009	30236.749251	30.745012
473.739264	30277.160553	30.750029
474.177132	30327.801845	30.755047
475.003067	30370.777864	30.760064
475.270191	30421.085810	30.765082
475.689352	30460.743787	30.770100
476.424367	30504.379108	30.775117
476.196150	30556.294749	30.780135
477.171368	30600.575365	30.785152
477.521995	30652.659762	30.790170
478.139365	30703.710039	30.795188
478.577888	30753.277618	30.800205
478.809574	30801.436410	30.805223
479.435329	30839.153659	30.810240
480.194978	30874.245537	30.815258
480.555687	30928.453081	30.820276
481.464591	30972.612129	30.825293
481.520594	31013.813612	30.830311
482.002987	31052.337579	30.835328
482.565735	31108.783397	30.840346
483.014222	31153.008622	30.845364
483.368676	31191.464384	30.850381
483.757288	31230.572316	30.855399
484.550877	31268.074410	30.860416
484.398933	31314.360055	30.865434
484.782746	31357.502198	30.870452
485.345864	31401.444488	30.875469
486.033334	31449.217309	30.880487
486.848453	31492.728375	30.885504
486.876580	31550.276925	30.890522
487.586921	31586.161627	30.895540
488.471937	31628.688482	30.900557
488.249328	31684.784741	30.905575
488.976635	31732.798523	30.910592
489.624275	31773.510571	30.915610
489.929197	31818.524636	30.920628
490.466008	31876.986939	30.925645
490.744387	31924.110559	30.930663
491.423311	31976.165818	30.935680
492.036221	32016.953322	30.940698
492.392732	32071.038064	30.945716
492.990185	32117.258689	30.950733
493.050701	32179.431535	30.955751
493.987344	32225.858473	30.960768
494.390120	32283.167028	30.965786
494.954443	32326.687510	30.970804
495.547635	32376.949115	30.975821
495.646442	32430.442952	30.980839
496.363312	32481.399824	30.985856
496.848246	32529.485013	30.990874
497.250410	32578.392499	30.995892
497.787233	32638.374222	31.000909
498.224913	32693.794460	31.005927
499.009674	32740.081958	31.010944
499.505421	32793.761113	31.015962
500.258115	32844.643715	31.020980
500.543515	32888.253308	31.025997
501.056333	32948.068981	31.031015
501.355291	32996.696467	31.036032
501.895141	33049.579099	31.041050
502.639886	33102.884970	31.046068
503.085170	33154.903894	31.051085
503.578461	33199.164371	31.056103
504.113928	33245.188564	31.061120
504.732604	33308.807321	31.066138
504.931887	33359.935909	31.071156
505.831639	33406.149968	31.076173
506.018428	33467.276321	31.081191
506.564782	33519.817714	31.086208
507.100783	33562.434786	31.091226
507.315302	33617.159024	31.096244
508.320307	33654.252954	31.101261
508.780588	33717.221262	31.106279
509.380606	33765.917178	31.111296
510.084225	33821.418866	31.116314
510.478161	33869.919693	31.121332
510.831353	33926.646194	31.126349
511.493143	33976.274966	31.131367
512.263600	34014.866759	31.136384
512.572135	34056.376090	31.141402
512.798659	34106.598109	31.146420
513.418015	34155.418346	31.151437
513.763438	34213.556757	31.156455
514.509700	34262.426913	31.161472
515.094277	34307.554260	31.166490
515.358609	34359.288373	31.171508
516.080160	34401.467113	31.176525
516.528602	34449.379057	31.181543
516.951691	34492.300212	31.186560
517.539882	34536.428508	31.191578
518.200742	34587.108420	31.196596
518.344445	34628.821727	31.201613
518.490777	34676.414789	31.206631
519.426848	34734.531673	31.211648
519.504289	34776.590752	31.216666
520.115418	34827.987173	31.221684
520.732890	34880.628304	31.226701
521.244258	34932.748750	31.231719
521.754858	34996.693018	31.236736
522.100862	35035.707233	31.241754
522.399409	35101.082363	31.246772
523.058819	35154.912615	31.251789
523.873903	35207.397152	31.256807
524.302010	35262.383046	31.261824
524.707037	35326.256323	31.266842
525.075425	35380.499455	31.271860
526.184763	35434.070261	31.276877
526.543714	35499.481417	31.281895
527.399974	35550.411238	31.286912
527.592423	35608.621697	31.291930
528.136255	35665.696052	31.296948
528.445569	35707.632136	31.301965
529.084958	35768.340160	31.306983
529.819296	35824.689575	31.312000
530.303388	35883.854144	31.317018
531.082461	35943.295152	31.322036
531.595882	35996.511776	31.327053
531.973228	36046.152012	31.332071
532.227805	36109.305079	31.337088
533.030820	36159.871637	31.342106
533.676286	36216.387763	31.347124
533.999368	36269.799281	31.352141
534.379815	36332.743601	31.357159
534.979979	36386.889764	31.362176
535.904476	36440.258099	31.367194
536.365422	36500.755876	31.372212
537.231395	36550.991018	31.377229
537.380530	36608.439554	31.382247
537.862800	36666.790881	31.387264
538.846838	36728.370855	31.392282
539.347107	36775.584364	31.397300
539.705775	36835.403544	31.402317
540.165909	36891.975778	31.407335
540.268342	36945.562656	31.412352
541.350439	36995.309711	31.417370
541.766455	37057.852223	31.422388
542.307880	37107.614663	31.427405
542.801103	37168.298974	31.432423
543.264269	37230.606961	31.437440
543.771774	37275.158275	31.442458
544.477790	37346.275061	31.447476
545.100174	37398.257678	31.452493
545.182175	37459.721772	31.457511
546.038128	37524.726139	31.462528
546.654712	37577.393039	31.467546
547.340122	37639.180492	31.472564
547.558674	37684.656885	31.477581
547.895060	37753.505840	31.482599
548.476244	37817.422206	31.487616
549.285189	37875.769922	31.492634
549.424928	37934.677910	31.497652
550.134475	37990.208516	31.502669
550.890717	38054.344790	31.507687
551.162219	38121.630489	31.512704
551.721333	38170.355535	31.517722
552.769406	38231.506108	31.522740
553.258156	38288.766823	31.527757
553.644294	38332.270623	31.532775
554.380388	38387.665297	31.537792
554.621402	38441.803334	31.542810
554.775081	38507.338029	31.547828
555.647283	38562.648596	31.552845
556.530237	38614.890561	31.557863
556.903171	38675.604284	31.562880
557.726033	38732.978268	31.567898
558.039442	38789.540527	31.572916
558.260236	38836.131999	31.577933
558.462663	38901.672901	31.582951
559.430894	38952.877853	31.587968
560.574551	39014.938970	31.592986
560.614247	39086.248066	31.598004
561.421794	39149.430962	31.603021
561.921262	39206.730373	31.608039
562.291492	39268.160792	31.613056
562.765785	39328.247039	31.618074
563.805642	39397.598161	31.623092
564.634289	39447.536036	31.628109
564.551624	39505.148751	31.633127
565.135354	39568.152901	31.638144
566.030483	39625.922676	31.643162
566.212865	39693.859630	31.648180
566.734314	39759.081217	31.653197
567.410116	39819.238448	31.658215
568.072461	39885.102385	31.663232
568.725971	39952.567934	31.668250
568.988610	40021.353434	31.673268
570.183482	40080.962099	31.678285
570.387860	40141.560861	31.683303
570.873550	40210.609266	31.688320
571.718485	40269.609202	31.693338
572.282060	40342.111551	31.698356
572.936069	40401.755208	31.703373
573.448596	40462.787252	31.708391
573.782252	40530.557659	31.713408
574.489118	40588.644073	31.718426
574.910290	40653.675336	31.723444
575.497412	40713.393564	31.728461
576.507057	40782.671615	31.733479
576.559199	40846.458407	31.738496
577.499844	40916.171428	31.743514
577.649002	40986.508269	31.748532
578.955270	41045.235664	31.753549
579.208486	41117.257930	31.758567
579.973300	41171.567378	31.763584
580.533107	41228.514801	31.768602
581.059372	41306.262952	31.773620
581.512960	41365.428333	31.778637
582.255510	41430.854294	31.783655
582.887924	41497.328620	31.788672
583.719134	41550.458544	31.793690
584.106510	41618.622358	31.798708
584.378091	41683.933093	31.803725
585.042481	41740.688373	31.808743
585.405313	41802.228273	31.813760
586.428156	41868.579327	31.818778
586.903180	41933.549026	31.823796
587.459850	41995.957230	31.828813
588.120997	42057.508045	31.833831
588.570833	42125.499201	31.838848
589.472126	42181.674578	31.843866
589.892500	42245.591180	31.848884
590.554626	42308.628891	31.853901
590.817458	42365.954666	31.858919
591.469048	42434.642542	31.863936
591.899407	42488.242308	31.868954
592.763036	42556.555807	31.873972
593.164178	42603.658356	31.878989
594.103623	42675.730044	31.884007
594.133769	42732.947738	31.889024
595.076676	42790.604530	31.894042
595.786517	42851.479480	31.899060
596.048108	42911.090209	31.904077
597.019467	42972.942873	31.909095
597.310471	43037.596761	31.914112
597.809535	43098.265046	31.919130
598.639567	43154.745018	31.924148
599.446037	43222.993627	31.929165
599.625775	43280.866099	31.934183
600.212880	43358.782735	31.939200
600.622058	43421.996065	31.944218
601.325341	43483.386121	31.949236
601.553215	43557.937763	31.954253
602.597512	43620.356409	31.959271
602.986901	43694.440444	31.964288
603.713495	43766.024014	31.969306
604.300540	43842.588738	31.974324
604.852310	43917.691765	31.979341
605.578647	43979.946157	31.984359
606.182032	44054.921382	31.989376
606.925361	44120.494342	31.994394
607.115557	44180.828105	31.999412
608.156019	44268.127128	32.004429
608.368591	44326.794185	32.009447
609.320995	44406.542271	32.014464
609.915979	44479.483427	32.019482
610.302359	44548.257333	32.024500
611.206690	44629.436991	32.029517
611.925388	44699.089172	32.034535
612.379273	44774.324274	32.039552
613.099016	44836.537810	32.044570
613.203871	44904.673734	32.049588
614.172296	44983.295406	32.054605
615.056850	45058.628481	32.059623
615.635026	45131.144248	32.064640
616.801108	45204.150143	32.069658
617.014974	45274.395562	32.074676
617.897962	45336.812650	32.079693
618.737558	45399.641557	32.084711
619.057436	45468.782947	32.089728
619.273020	45525.738380	32.094746
620.216544	45596.142542	32.099764
620.924185	45661.187912	32.104781
621.460054	45728.974172	32.109799
621.596142	45802.390033	32.114816
622.427931	45877.866966	32.119834
623.038113	45945.794063	32.124852
624.006966	46023.666527	32.129869
624.915495	46081.583930	32.134887
625.428725	46155.017786	32.139904
626.059341	46223.252493	32.144922
626.843883	46292.304662	32.149940
627.243702	46358.285900	32.154957
628.180089	46421.823674	32.159975
628.641920	46484.683144	32.164992
629.243175	46543.497553	32.170010
629.705132	46609.109204	32.175028
630.367242	46682.122913	32.180045
630.795535	46733.613930	32.185063
631.291015	46815.789136	32.190080
632.072150	46880.769580	32.195098
632.459248	46953.567861	32.200116
633.122635	47015.043429	32.205133
633.807599	47079.887676	32.210151
634.451480	47148.660831	32.215168
634.982250	47210.651148	32.220186
635.362625	47273.114356	32.225204
636.151724	47348.141068	32.230221
637.067637	47408.774712	32.235239
637.366755	47483.492702	32.240256
638.069883	47552.555141	32.245274
638.824007	47617.168670	32.250292
639.497963	47688.209927	32.255309
639.887877	47758.410189	32.260327
640.467997	47836.419364	32.265344
641.550049	47906.094139	32.270362
642.280229	47974.248936	32.275380
642.404866	48045.737949	32.280397
643.054944	48115.898568	32.285415
643.719941	48186.025434	32.290432
644.456831	48257.071263	32.295450
645.082256	48334.322184	32.300468
645.549995	48410.750295	32.305485
646.279935	48488.637012	32.310503
646.858411	48558.829187	32.315520
647.819888	48640.134517	32.320538
648.361635	48708.333671	32.325556
648.846384	48794.921089	32.330573
649.253977	48872.037120	32.335591
650.043415	48945.866958	32.340608
650.705861	49032.509693	32.345626
651.644579	49111.352813	32.350644
651.856784	49190.373252	32.355661
652.719254	49273.157835	32.360679
653.170102	49351.679594	32.365696
653.893054	49436.960428	32.370714
654.497570	49506.145448	32.375732
654.962727	49603.652931	32.380749
656.025724	49677.524532	32.385767
656.827565	49768.412591	32.390784
657.557578	49847.961587	32.395802
657.998061	49934.376750	32.400820
658.350960	50022.735707	32.405837
659.416976	50092.539865	32.410855
660.132135	50174.161270	32.415872
660.699962	50250.092641	32.420890
661.508593	50334.945792	32.425908
662.273700	50419.812399	32.430925
663.385470	50493.343639	32.435943
663.757082	50573.457440	32.440960
664.545396	50648.805124	32.445978
665.027091	50733.660322	32.450996
665.148005	50815.206218	32.456013
666.031014	50893.703510	32.461031
666.889673	50959.164269	32.466048
667.189728	51048.623720	32.471066
668.334379	51134.066241	32.476084
668.618230	51213.702464	32.481101
669.715191	51294.205026	32.486119
670.278082	51380.068586	32.491136
671.386729	51464.233493	32.496154
671.797705	51530.405048	32.501172
672.861837	51603.276559	32.506189
673.138790	51678.929134	32.511207
673.761753	51764.310142	32.516224
674.735989	51841.397965	32.521242
675.489784	51908.693834	32.526260
676.281702	51987.228070	32.531277
676.675728	52062.237122	32.536295
677.542724	52130.851033	32.541312
677.507672	52205.522772	32.546330
678.450630	52268.018999	32.551348
679.340034	52348.652629	32.556365
680.083349	52414.648093	32.561383
680.663850	52485.301143	32.566400
680.754860	52560.643997	32.571418
681.987060	52636.903081	32.576436
682.210672	52717.205632	32.581453
682.730790	52785.135435	32.586471
683.573721	52865.487045	32.591488
684.192840	52943.406116	32.596506
684.609785	53019.142350	32.601524
684.780566	53107.984495	32.606541
685.867451	53190.823848	32.611559
686.721943	53275.528666	32.616576
687.267711	53363.800488	32.621594
687.808354	53447.960248	32.626612
688.127560	53546.152564	32.631629
689.672274	53635.610508	32.636647
690.358943	53720.210320	32.641664
691.068635	53815.374743	32.646682
691.450193	53898.662437	32.651700
692.107477	53988.868198	32.656717
693.212783	54075.694512	32.661735
693.640447	54157.912769	32.666752
694.494432	54235.128548	32.671770
695.396678	54333.125253	32.676788
696.057955	54419.661659	32.681805
696.936008	54509.233649	32.686823
697.704325	54594.633827	32.691840
698.259135	54677.542748	32.696858
699.074723	54754.829520	32.701876
699.384284	54850.699936	32.706893
700.492317	54939.883150	32.711911
700.966387	55024.963912	32.716928
701.896819	55114.257864	32.721946
702.597268	55190.690763	32.726964
703.001099	55282.238475	32.731981
703.536345	55371.285185	32.736999
704.602970	55454.129322	32.742016
705.224042	55541.372253	32.747034
706.310894	55638.035428	32.752052
706.803749	55735.329949	32.757069
707.895916	55804.868583	32.762087
708.649425	55880.092948	32.767104
709.206716	55966.689245	32.772122
710.254639	56052.474894	32.777140
710.862910	56135.981750	32.782157
711.292071	56211.004803	32.787175
712.002151	56296.129087	32.792192
712.950487	56387.260344	32.797210
713.586118	56466.675680	32.802228
714.179658	56544.496680	32.807245
714.954119	56625.479335	32.812263
715.822271	56712.523300	32.817280
715.966712	56794.282375	32.822298
717.376498	56876.780252	32.827316
717.672007	56972.300638	32.832333
718.600756	57054.627629	32.837351
718.996778	57132.272611	32.842368
719.448039	57222.757054	32.847386
720.501600	57304.679287	32.852404
721.174499	57388.319620	32.857421
721.911483	57486.842497	32.862439
722.247715	57574.922244	32.867456
723.266659	57667.135904	32.872474
723.819558	57751.884898	32.877492
724.683783	57846.870321	32.882509
725.390963	57927.178016	32.887527
726.322124	57997.684944	32.892544
727.018321	58089.463413	32.897562
727.913738	58164.773979	32.902580
728.353816	58242.497914	32.907597
728.700639	58325.293801	32.912615
729.627413	58408.682715	32.917632
729.579054	58507.396030	32.922650
730.882560	58591.410145	32.927668
731.695399	58687.147447	32.932685
732.416481	58769.734337	32.937703
732.898196	58862.435436	32.942720
733.632671	58958.996247	32.947738
734.399195	59048.944452	32.952756
735.466052	59132.548107	32.957773
735.328588	59220.948536	32.962791
736.513787	59317.959209	32.967808
736.997187	59429.403990	32.972826
737.892803	59520.289485	32.977844
738.978360	59613.076108	32.982861
739.445479	59707.339794	32.987879
740.036441	59806.363350	32.992896
740.961354	59906.676906	32.997914
741.775276	59997.766862	33.002932
742.404601	60096.437450	33.007949
743.232631	60201.793207	33.012967
744.035532	60300.146264	33.017984
744.645899	60401.789725	33.023002
745.686007	60504.049935	33.028020
746.303349	60602.908003	33.033037
747.189275	60706.617423	33.038055
747.813533	60796.372788	33.043072
748.679206	60899.206333	33.048090
749.328683	60999.877660	33.053108
750.741071	61101.284480	33.058125
751.379041	61185.088912	33.063143
751.815151	61280.521888	33.068160
752.334951	61392.615550	33.073178
753.612875	61481.789963	33.078196
754.847487	61577.599123	33.083213
755.291049	61675.520198	33.088231
756.039823	61750.320384	33.093248
756.861123	61853.177514	33.098266
757.357536	61942.362030	33.103284
758.244870	62048.514006	33.108301
759.078573	62137.526130	33.113319
760.078927	62230.658818	33.118336
760.411170	62332.879201	33.123354
761.179789	62409.216536	33.128372
761.987024	62509.362877	33.133389
762.744192	62612.049617	33.138407
763.475030	62710.771733	33.143424
764.622946	62801.636158	33.148442
765.035313	62895.072318	33.153460
766.412535	62987.471468	33.158477
766.461556	63083.199892	33.163495
767.579418	63179.508310	33.168512
768.023966	63270.376970	33.173530
768.414937	63371.655495	33.178548
769.889470	63470.485731	33.183565
770.283394	63559.002050	33.188583
771.208597	63660.337360	33.193600
771.783135	63761.538072	33.198618
773.116773	63856.688449	33.203636
773.957397	63955.594547	33.208653
774.315736	64043.649676	33.213671
775.247592	64135.154208	33.218688
776.141272	64227.507048	33.223706
776.597736	64325.050329	33.228724
777.189295	64398.680225	33.233741
777.775980	64487.853366	33.238759
778.898602	64580.361577	33.243776
779.530827	64663.203652	33.248794
780.219107	64761.585989	33.253812
780.784197	64859.430875	33.258829
781.663203	64954.371711	33.263847
782.949427	65051.604270	33.268864
783.264629	65148.742350	33.273882
783.884094	65237.184939	33.278900
785.229426	65332.510008	33.283917
785.473839	65435.003701	33.288935
786.602709	65526.697692	33.293952
786.882969	65637.739941	33.298970
787.829090	65730.450946	33.303988
788.688243	65830.412470	33.309005
789.097458	65936.491165	33.314023
790.414361	66050.779089	33.319040
791.018172	66153.846198	33.324058
791.832868	66249.213491	33.329076
792.982353	66341.806245	33.334093
793.298500	66457.689920	33.339111
794.423214	66556.935260	33.344128
795.004112	66673.246978	33.349146
795.889520	66783.844906	33.354164
796.889250	66892.798224	33.359181
796.942187	66995.315519	33.364199
798.285406	67087.551406	33.369216
799.228910	67205.999470	33.374234
799.948715	67312.719057	33.379252
800.710310	67415.247361	33.384269
801.235112	67527.506863	33.389287
802.115864	67626.452650	33.394304
803.361502	67747.863438	33.399322
804.076346	67847.374248	33.404340
804.716926	67955.527214	33.409357
805.639130	68048.845565	33.414375
806.435999	68158.975744	33.419392
807.423487	68277.941070	33.424410
808.245167	68377.943746	33.429428
809.141804	68489.819964	33.434445
809.585733	68598.664935	33.439463
810.721487	68700.924486	33.444480
811.404263	68812.278382	33.449498
812.458604	68910.454749	33.454516
813.051638	69021.070092	33.459533
814.069379	69129.384201	33.464551
814.691942	69229.016099	33.469568
815.834241	69342.712824	33.474586
816.451121	69455.010612	33.479604
817.669189	69548.079087	33.484621
818.023343	69651.129652	33.489639
819.061307	69750.381895	33.494656
820.188800	69860.271240	33.499674
820.835296	69965.297239	33.504692
821.733703	70060.456577	33.509709
822.205177	70173.502108	33.514727
823.191488	70270.966059	33.519744
824.113822	70388.247878	33.524762
825.134331	70487.290361	33.529780
825.733691	70579.332246	33.534797
826.433766	70692.686173	33.539815
827.466215	70792.335850	33.544832
828.309439	70899.221856	33.549850
828.817639	71004.514317	33.554868
829.963659	71092.065005	33.559885
830.543379	71199.816720	33.564903
831.479696	71307.665019	33.569920
832.509183	71399.135824	33.574938
832.596834	71491.919624	33.579956
833.521925	71584.901912	33.584973
834.765056	71700.606872	33.589991
835.201200	71800.265090	33.595008
836.057151	71896.362307	33.600026
836.760894	72005.896380	33.605044
838.188735	72108.022213	33.610061
838.789743	72221.752871	33.615079
839.592582	72317.239325	33.620096
840.241702	72421.451470	33.625114
841.151776	72522.228764	33.630132
841.825732	72624.423978	33.635149
842.729960	72741.630455	33.640167
843.791813	72842.321870	33.645184
844.747819	72955.138810	33.650202
845.102410	73060.007543	33.655220
845.808392	73168.570793	33.660237
846.587789	73284.393287	33.665255
847.638714	73406.557472	33.670272
848.533412	73520.995002	33.675290
849.385723	73633.514399	33.680308
850.546378	73742.274779	33.685325
851.247294	73853.286193	33.690343
851.771526	73967.859645	33.695360
852.632877	74084.648085	33.700378
853.495565	74205.642090	33.705396
854.597128	74321.469297	33.710413
855.459120	74437.435850	33.715431
856.562763	74555.138393	33.720448
857.478526	74668.741533	33.725466
858.178818	74784.063568	33.730484
859.461038	74892.328242	33.735501
860.181824	75010.029392	33.740519
860.974045	75119.220384	33.745536
862.071570	75241.499634	33.750554
862.625573	75355.402988	33.755572
863.776327	75458.383048	33.760589
864.700010	75587.987311	33.765607
865.331137	75700.043308	33.770624
866.224167	75805.978495	33.775642
866.552458	75931.776130	33.780660
867.816723	76044.735127	33.785677
868.386538	76170.407377	33.790695
869.449022	76279.155372	33.795712
870.660419	76393.150159	33.800730
871.099224	76512.143402	33.805748
872.443534	76628.195839	33.810765
873.174461	76752.768805	33.815783
873.982033	76874.302755	33.820800
875.040583	76983.687565	33.825818
875.519381	77098.268721	33.830836
876.615290	77219.239677	33.835853
877.658529	77342.106935	33.840871
878.389639	77456.485400	33.845888
878.977440	77579.311024	33.850906
879.670519	77699.359069	33.855924
880.960495	77807.444124	33.860941
881.566419	77941.264478	33.865959
882.293544	78061.498797	33.870976
883.267030	78188.282588	33.875994
884.231249	78310.431790	33.881012
884.927582	78433.028869	33.886029
886.102815	78557.743152	33.891047
887.256591	78676.874533	33.896064
887.943283	78806.759191	33.901082
888.601353	78915.758330	33.906100
889.869197	79035.608177	33.911117
890.036604	79149.701873	33.916135
890.797856	79262.714885	33.921152
891.884267	79370.673244	33.926170
892.831277	79502.433397	33.931188
893.813210	79614.159062	33.936205
894.971625	79736.993611	33.941223
895.501160	79857.114638	33.946240
896.764343	79971.787602	33.951258
897.778088	80091.200363	33.956276
898.620347	80210.133717	33.961293
899.552321	80337.263232	33.966311
900.323133	80447.555655	33.971328
901.121824	80554.474089	33.976346
901.927178	80689.290014	33.981364
902.909011	80798.309171	33.986381
903.142980	80936.877240	33.991399
904.515359	81065.968232	33.996416
905.429008	81188.594091	34.001434
906.082119	81332.977214	34.006452
907.537257	81455.025328	34.011469
908.696745	81583.619900	34.016487
909.297494	81705.663511	34.021504
910.622887	81827.492825	34.026522
910.811704	81966.225063	34.031540
911.935980	82085.857057	34.036557
912.756671	82222.730471	34.041575
913.666349	82354.243787	34.046592
914.909061	82489.075856	34.051610
915.570744	82613.381815	34.056628
916.814228	82735.962741	34.061645
917.780388	82881.217010	34.066663
918.357148	83016.523298	34.071680
919.244555	83144.546701	34.076698
919.721514	83275.941974	34.081716
920.834239	83401.612528	34.086733
921.772066	83535.306247	34.091751
922.873711	83686.600009	34.096768
923.993935	83814.057783	34.101786
924.931272	83956.065623	34.106804
925.578537	84091.251917	34.111821
926.900695	84227.524250	34.116839
927.543186	84366.260474	34.121856
928.911019	84493.226334	34.126874
929.518468	84624.341258	34.131892
930.626150	84764.945258	34.136909
931.542079	84904.325507	34.141927
932.161009	85036.973737	34.146944
933.907383	85168.698429	34.151962
934.485669	85309.223240	34.156980
935.816039	85436.503233	34.161997
936.847351	85563.741908	34.167015
937.333914	85708.236559	34.172032
938.321999	85835.635255	34.177050
939.268850	85973.368477	34.182068
940.037908	86094.390672	34.187085
941.226605	86224.256012	34.192103
942.299383	86363.530007	34.197120
943.049397	86489.169418	34.202138
944.010863	86630.362916	34.207156
945.018158	86753.340058	34.212173
945.936325	86891.829761	34.217191
946.853543	87030.510351	34.222208
947.751364	87156.889820	34.227226
949.013577	87293.566100	34.232244
950.015260	87423.960269	34.237261
950.917397	87550.758946	34.242279
951.329897	87681.132453	34.247296
952.302866	87804.993778	34.252314
953.101909	87933.584406	34.257332
954.384567	88053.925982	34.262349
955.504235	88182.467492	34.267367
956.100492	88312.967089	34.272384
957.278544	88421.819638	34.277402
957.941197	88559.115244	34.282420
958.741798	88692.372556	34.287437
959.754830	88821.225012	34.292455
960.911541	88943.174050	34.297472
961.699573	89083.988238	34.302490
962.781814	89225.200588	34.307508
963.534843	89354.007348	34.312525
964.718355	89482.531815	34.317543
965.471883	89624.101680	34.322560
966.375925	89751.974028	34.327578
967.111977	89904.459770	34.332596
968.139781	90042.516135	34.337613
969.448354	90185.117018	34.342631
970.261983	90323.347619	34.347648
971.358290	90449.849433	34.352666
972.262966	90600.994242	34.357684
973.073280	90746.742857	34.362701
974.012125	90890.558293	34.367719
974.990320	91035.141364	34.372736
976.282221	91184.986422	34.377754
977.131193	91329.907986	34.382772
978.137888	91474.222538	34.387789
978.748336	91616.445204	34.392807
979.868814	91768.157746	34.397824
981.077212	91918.856009	34.402842
982.628414	92069.906925	34.407860
983.311719	92215.923304	34.412877
984.207866	92345.594966	34.417895
985.166139	92503.078118	34.422912
986.253154	92644.052229	34.427930
987.155616	92799.783874	34.432948
988.098909	92952.037035	34.437965
989.326904	93092.433448	34.442983
990.141576	93237.787719	34.448000
991.239475	93381.970263	34.453018
992.548255	93542.965532	34.458036
993.695221	93676.241277	34.463053
994.527611	93819.275985	34.468071
995.381976	93962.181163	34.473088
996.573562	94113.640684	34.478106
998.245689	94269.246582	34.483124
998.803150	94407.193561	34.488141
999.592367	94536.536293	34.493159
1000.484669	94689.959477	34.498176
1001.281580	94835.286015	34.503194
1002.861376	94977.182329	34.508212
1003.733244	95119.101401	34.513229
1005.003288	95273.558424	34.518247
1005.415517	95412.052299	34.523264
1006.654977	95558.111490	34.528282
1007.695836	95701.882773	34.533300
1008.667080	95851.724712	34.538317
1009.746593	95993.818059	34.543335
1010.738667	96138.967991	34.548352
1011.773685	96271.701959	34.553370
1013.092821	96428.185166	34.558388
1013.626642	96568.832733	34.563405
1014.999314	96708.918595	34.568423
1015.626021	96854.547348	34.573440
1016.872333	96997.785333	34.578458
1017.750910	97153.060795	34.583476
1018.293702	97299.427292	34.588493
1019.113319	97434.735176	34.593511
1020.313188	97582.838205	34.598528
1021.008007	97712.145411	34.603546
1022.274117	97860.543603	34.608564
1023.745347	98013.296545	34.613581
1025.045175	98151.435281	34.618599
1025.172383	98289.111686	34.623616
1026.630219	98424.450620	34.628634
1027.398836	98569.469188	34.633652
1028.602220	98710.655250	34.638669
1029.554431	98867.005084	34.643687
1030.593956	99008.129369	34.648704
1031.664464	99151.746842	34.653722
1032.537572	99309.518389	34.658740
1033.468967	99468.016870	34.663757
1034.749425	99607.660840	34.668775
1035.332327	99761.993741	34.673792
1036.577603	99908.870693	34.678810
1037.487987	100072.484481	34.683828
1038.522433	100244.916013	34.688845
1039.383711	100392.045440	34.693863
1040.445400	100565.868961	34.698880
1041.127194	100719.240095	34.703898
1042.580727	100881.061401	34.708916
1043.957730	101041.716439	34.713933
1045.054164	101206.257645	34.718951
1045.781716	101377.285239	34.723968
1046.936213	101539.156622	34.728986
1048.182999	101698.643522	34.734004
1049.182162	101870.442569	34.739021
1050.393878	102027.058577	34.744039
1051.347904	102193.338606	34.749056
1052.658435	102346.568198	34.754074
1053.415251	102513.704819	34.759092
1054.510803	102675.831909	34.764109
1055.675649	102837.315010	34.769127
1056.404062	103005.853216	34.774144
1057.610032	103169.334736	34.779162
1059.048747	103335.709440	34.784180
1059.889080	103500.441646	34.789197
1061.429327	103661.882657	34.794215
1062.179179	103834.859350	34.799232
1063.365371	103992.426882	34.804250
1064.834023	104147.148834	34.809268
1065.705349	104316.127732	34.814285
1066.476115	104475.677141	34.819303
1067.242779	104653.321407	34.824320
1068.370408	104812.917978	34.829338
1069.395729	104977.755274	34.834356
1071.054081	105154.539845	34.839373
1072.053787	105313.055688	34.844391
1073.360568	105480.108340	34.849408
1074.351927	105637.726752	34.854426
1075.345165	105797.184172	34.859444
1076.350759	105967.608485	34.864461
1077.926683	106135.332295	34.869479
1078.982847	106293.602957	34.874496
1080.134966	106451.643769	34.879514
1081.071964	106611.912649	34.884532
1082.137194	106771.857879	34.889549
1083.546617	106920.718179	34.894567
1084.353418	107086.145148	34.899584
1085.136776	107246.035276	34.904602
1086.499771	107400.129222	34.909620
1087.457523	107566.232287	34.914637
1088.754158	107723.723750	34.919655
1089.973616	107872.275533	34.924672
1090.699905	108035.044060	34.929690
1092.060640	108181.279858	34.934708
1093.023557	108341.413238	34.939725
1094.155207	108476.108634	34.944743
1094.901843	108629.163279	34.949760
1096.340011	108780.905646	34.954778
1097.369185	108921.604194	34.959796
1098.331498	109077.848004	34.964813
1099.491436	109227.809809	34.969831
1100.594756	109378.846335	34.974848
1101.544824	109533.825986	34.979866
1102.870200	109673.580821	34.984884
1103.626048	109840.094099	34.989901
1105.124171	109998.426623	34.994919
1105.782155	110159.110635	34.999936
1107.080752	110315.522887	35.004954
1108.078876	110470.308914	35.009972
1108.899878	110641.520611	35.014989
1109.835769	110799.158489	35.020007
1111.174484	110971.673025	35.025024
1112.572855	111129.341418	35.030042
1113.607972	111295.310550	35.035060
1114.479686	111461.001671	35.040077
1115.767966	111624.421692	35.045095
1116.852942	111800.315308	35.050112
1117.909275	111972.473071	35.055130
1119.360541	112132.775478	35.060148
1120.398562	112301.183785	35.065165
1121.387416	112483.259326	35.070183
1122.770565	112641.012856	35.075200
1123.840228	112816.241682	35.080218
1124.916523	112983.378950	35.085236
1125.905119	113163.872664	35.090253
1127.254339	113327.227466	35.095271
1128.230974	113503.729751	35.100288
1129.265087	113676.190816	35.105306
1130.804604	113843.297572	35.110324
1131.906826	114007.670667	35.115341
1132.814294	114190.160683	35.120359
1133.968441	114356.886224	35.125376
1135.314806	114531.661458	35.130394
1136.351025	114693.118207	35.135412
1137.701966	114879.841762	35.140429
1138.652413	115047.794537	35.145447
1139.889212	115221.245793	35.150464
1140.710029	115399.582616	35.155482
1142.258755	115563.943503	35.160500
1142.969372	115746.040818	35.165517
1144.501515	115926.412302	35.170535
1145.825487	116109.163695	35.175552
1146.780485	116276.702774	35.180570
1148.210804	116448.417195	35.185588
1149.084776	116625.419801	35.190605
1150.578049	116800.664724	35.195623
1151.801754	116972.096804	35.200640
1152.757871	117152.082407	35.205658
1153.803286	117317.278164	35.210676
1154.778174	117492.417212	35.215693
1156.003228	117668.088690	35.220711
1157.001474	117837.378359	35.225728
1158.402027	118017.628300	35.230746
1159.792994	118197.297128	35.235764
1160.815943	118384.292490	35.240781
1161.817275	118558.214641	35.245799
1163.411602	118722.886648	35.250816
1164.130797	118901.763381	35.255834
1165.854640	119071.858231	35.260852
1166.350206	119243.998067	35.265869
1167.840487	119415.627784	35.270887
1169.488031	119572.430676	35.275904
1169.962092	119733.857560	35.280922
1171.055019	119906.135169	35.285940
1172.057994	120063.561045	35.290957
1173.343290	120223.467649	35.295975
1174.604395	120392.651366	35.300992
1175.303526	120575.636242	35.306010
1176.687990	120732.028371	35.311028
1177.816247	120909.404288	35.316045
1179.110079	121075.541439	35.321063
1180.069356	121249.938984	35.326080
1181.309523	121432.716335	35.331098
1182.102525	121606.025197	35.336116
1183.370290	121788.241733	35.341133
1184.497893	121969.593077	35.346151
1185.952243	122148.889800	35.351168
1186.823319	122336.372020	35.356186
1187.794697	122514.173006	35.361204
1189.294086	122702.776418	35.366221
1190.356894	122898.984388	35.371239
1191.961249	123084.528612	35.376256
1193.235975	123279.195677	35.381274
1194.077085	123453.583401	35.386292
1195.324335	123651.631031	35.391309
1196.954719	123854.009024	35.396327
1198.136031	124024.870012	35.401344
1199.115601	124220.387085	35.406362
1200.604931	124408.657606	35.411380
1201.429568	124599.722550	35.416397
1202.615535	124789.716926	35.421415
1204.120895	124981.679327	35.426432
1204.948733	125178.848648	35.431450
1206.340794	125363.510522	35.436468
1207.305621	125559.366220	35.441485
1208.956656	125755.496033	35.446503
1210.275378	125951.437764	35.451520
1211.308057	126155.265614	35.456538
1212.799776	126351.867262	35.461556
1213.492838	126538.711817	35.466573
1214.684167	126734.486924	35.471591
1216.057329	126935.169729	35.476608
1217.484470	127136.289104	35.481626
1218.756322	127324.175750	35.486644
1220.060642	127533.156902	35.491661
1220.922698	127727.415040	35.496679
1222.343915	127931.863245	35.501696
1223.727996	128135.341338	35.506714
1224.755882	128334.727401	35.511732
1226.084506	128527.875850	35.516749
1227.291424	128729.633691	35.521767
1228.508596	128918.639875	35.526784
1229.914156	129129.148336	35.531802
1230.946894	129321.483981	35.536820
1232.112997	129526.233624	35.541837
1233.682066	129723.321168	35.546855
1234.846997	129914.966353	35.551872
1236.201123	130124.789967	35.556890
1237.209498	130322.056867	35.561908
1238.355849	130525.532912	35.566925
1239.846350	130731.049585	35.571943
1241.553005	130928.374906	35.576960
1242.640007	131125.011463	35.581978
1244.012426	131310.844566	35.586996
1245.117043	131515.296125	35.592013
1246.046474	131713.990159	35.597031
1247.440163	131897.766926	35.602048
1248.550515	132104.986445	35.607066
1249.949544	132296.618250	35.612084
1251.354073	132489.315880	35.617101
1252.526041	132665.403209	35.622119
1253.590735	132853.029408	35.627136
1255.232148	133033.130496	35.632154
1256.125684	133215.975984	35.637172
1257.415203	133401.780197	35.642189
1258.140117	133584.653605	35.647207
1259.696432	133773.298002	35.652224
1260.940610	133966.813902	35.657242
1262.271566	134154.556204	35.662260
1263.239064	134356.453851	35.667277
1264.679812	134549.624278	35.672295
1265.749243	134742.549121	35.677312
1266.894170	134938.927160	35.682330
1268.007484	135143.914408	35.687348
1269.362674	135347.392748	35.692365
1270.432110	135560.154693	35.697383
1271.967670	135752.236823	35.702400
1273.375039	135961.115501	35.707418
1274.404625	136171.031381	35.712436
1276.011737	136376.238757	35.717453
1276.919258	136596.720865	35.722471
1278.124485	136794.391841	35.727488
1279.413740	137015.463385	35.732506
1280.953274	137228.578271	35.737524
1282.524917	137438.161289	35.742541
1283.388749	137668.223637	35.747559
1284.634316	137865.753290	35.752576
1286.075424	138083.075258	35.757594
1287.276723	138299.915477	35.762612
1288.790716	138517.786429	35.767629
1290.137978	138743.463694	35.772647
1291.771060	138955.099750	35.777664
1292.810747	139164.824547	35.782682
1294.211764	139369.963189	35.787700
1295.651786	139593.916777	35.792717
1296.377836	139814.861282	35.797735
1297.913671	140023.623863	35.802752
1299.725373	140240.859687	35.807770
1300.666959	140458.435755	35.812788
1302.080617	140674.987097	35.817805
1303.234226	140897.506794	35.822823
1304.738336	141113.906350	35.827840
1305.797457	141334.831095	35.832858
1307.698867	141546.639684	35.837876
1309.061960	141764.612536	35.842893
1309.810657	141985.131948	35.847911
1311.499468	142200.124084	35.852928
1312.720580	142414.263908	35.857946
1314.022410	142624.038880	35.862964
1315.478937	142849.730999	35.867981
1316.746718	143070.846675	35.872999
1318.024212	143285.463735	35.878016
1319.250641	143507.133567	35.883034
1320.299188	143725.722770	35.888052
1322.049343	143948.607137	35.893069
1323.279511	144163.717673	35.898087
1324.713651	144385.714259	35.903104
1325.838133	144604.396943	35.908122
1327.129652	144832.408402	35.913140
1328.802524	145046.044599	35.918157
1330.336026	145274.235932	35.923175
1331.619681	145491.361788	35.928192
1332.754181	145700.426998	35.933210
1334.676644	145921.909644	35.938228
1335.703721	146129.406892	35.943245
1337.306842	146344.138284	35.948263
1338.602397	146544.880935	35.953280
1339.421526	146751.753234	35.958298
1340.766738	146959.508637	35.963316
1342.465535	147156.408175	35.968333
1343.270097	147351.569933	35.973351
1344.911280	147551.856210	35.978368
1346.009542	147767.726002	35.983386
1347.091293	147974.460498	35.988404
1348.295037	148173.484883	35.993421
1349.622772	148397.393946	35.998439
1351.061222	148608.619124	36.003456
1351.751374	148822.665871	36.008474
1353.062605	149053.383698	36.013492
1354.660617	149273.484325	36.018509
1355.609142	149509.642745	36.023527
1356.915634	149736.124759	36.028544
1358.672433	149965.812085	36.033562
1360.227670	150188.499873	36.038580
1361.531210	150426.980376	36.043597
1362.556214	150659.603106	36.048615
1363.758781	150892.617917	36.053632
1365.514199	151123.909723	36.058650
1367.330085	151355.675394	36.063668
1368.639598	151595.657891	36.068685
1369.517453	151831.710500	36.073703
1371.308681	152061.655110	36.078720
1372.709126	152300.179342	36.083738
1374.119176	152535.009195	36.088756
1375.732032	152770.138329	36.093773
1377.022128	153005.179337	36.098791
1378.558490	153239.256118	36.103808
1379.852958	153481.952884	36.108826
1381.330966	153710.544242	36.113844
1382.833511	153947.764676	36.118861
1383.874317	154185.198007	36.123879
1385.322906	154424.485320	36.128896
1386.990491	154655.818123	36.133914
1388.425151	154896.328229	36.138932
1389.761503	155130.304424	36.143949
1391.031797	155369.001535	36.148967
1392.343596	155604.341784	36.153984
1394.155267	155853.264054	36.159002
1395.573487	156088.031032	36.164020
1396.546807	156327.578294	36.169037
1398.247711	156569.970503	36.174055
1400.033809	156797.408663	36.179072
1401.387212	157042.231110	36.184090
1402.840696	157280.628003	36.189108
1404.205729	157512.996923	36.194125
1405.186542	157766.068853	36.199143
1406.606185	157985.253700	36.204160
1408.357635	158238.676699	36.209178
1409.802711	158476.787651	36.214196
1411.551879	158711.589285	36.219213
1412.289259	158949.647816	36.224231
1413.931416	159186.283431	36.229248
1415.227802	159429.118595	36.234266
1416.410120	159668.925686	36.239284
1418.458750	159902.923268	36.244301
1419.347553	160147.742043	36.249319
1421.053064	160389.971019	36.254336
1422.751131	160623.010531	36.259354
1423.971541	160871.119147	36.264372
1425.553969	161096.116815	36.269389
1426.935830	161344.697146	36.274407
1428.371219	161583.545145	36.279424
1429.690435	161825.281464	36.284442
1430.931075	162062.308149	36.289460
1432.668156	162295.868206	36.294477
1434.146142	162530.561510	36.299495
1435.191097	162751.713381	36.304512
1436.743735	162976.646121	36.309530
1438.134593	163213.006001	36.314548
1439.018158	163437.080149	36.319565
1440.878433	163668.975350	36.324583
1442.376221	163895.202129	36.329600
1443.990576	164132.025471	36.334618
1445.138292	164361.343027	36.339636
1446.510615	164588.836034	36.344653
1447.799672	164827.871129	36.349671
1449.237805	165065.449047	36.354688
1450.638157	165306.702983	36.359706
1451.759156	165554.667155	36.364724
1453.270086	165790.534886	36.369741
1454.705606	166050.221310	36.374759
1455.650809	166304.487821	36.379776
1457.405652	166551.239082	36.384794
1459.000302	166810.954246	36.389812
1460.456795	167053.335531	36.394829
1462.098719	167312.004027	36.399847
1463.094784	167571.853797	36.404864
1464.941146	167821.312341	36.409882
1466.201571	168094.632155	36.414900
1467.928333	168346.510987	36.419917
1468.867915	168609.154032	36.424935
1471.005220	168875.432392	36.429952
1472.457632	169136.511533	36.434970
1473.994202	169407.583817	36.439988
1475.567268	169662.538620	36.445005
1477.391485	169924.248038	36.450023
1478.273233	170188.112077	36.455040
1480.079347	170447.756526	36.460058
1481.191808	170711.891055	36.465076
1482.657122	170972.746139	36.470093
1484.586241	171250.467992	36.475111
1485.953922	171514.997117	36.480128
1487.313680	171782.474245	36.485146
1488.896700	172051.783920	36.490164
1490.883558	172318.390219	36.495181
1491.894700	172591.067295	36.500199
1493.800455	172853.701058	36.505216
1495.634977	173115.419918	36.510234
1496.784504	173383.583094	36.515252
1498.180196	173651.289627	36.520269
1499.811802	173919.239498	36.525287
1501.344939	174173.542667	36.530304
1502.950159	174447.377610	36.535322
1504.497108	174721.921002	36.540340
1505.846434	174984.280688	36.545357
1507.501262	175252.878988	36.550375
1509.126170	175524.492327	36.555392
1510.709801	175787.376649	36.560410
1512.133746	176050.489976	36.565428
1513.660194	176307.619894	36.570445
1515.201749	176571.173604	36.575463
1516.802170	176844.953830	36.580480
1518.235885	177104.995946	36.585498
1519.980516	177379.872800	36.590516
1521.481725	177639.804404	36.595533
1522.959889	177897.175300	36.600551
1524.166571	178160.811763	36.605568
1526.109874	178431.749733	36.610586
1527.253463	178708.756687	36.615604
1529.100510	178960.764965	36.620621
1531.057889	179223.042674	36.625639
1532.328961	179493.708178	36.630656
1533.734747	179731.031741	36.635674
1535.310702	179991.618979	36.640692
1537.176511	180230.395727	36.645709
1538.198375	180473.140264	36.650727
1539.601166	180721.286377	36.655744
1540.956553	180956.132051	36.660762
1542.652375	181222.672580	36.665780
1544.144753	181468.774848	36.670797
1545.379225	181724.518640	36.675815
1547.104477	181987.424817	36.680832
1548.423368	182240.667777	36.685850
1549.797468	182504.138320	36.690868
1551.367064	182763.947017	36.695885
1553.110972	183031.882061	36.700903
1554.123214	183304.834292	36.705920
1555.620683	183571.971249	36.710938
1557.135951	183855.666125	36.715956
1558.644065	184122.244145	36.720973
1560.240827	184410.169462	36.725991
1561.447795	184691.425895	36.731008
1563.386917	184990.500237	36.736026
1564.977938	185329.633532	36.741044
1566.574772	185614.514386	36.746061
1568.148118	185894.700845	36.751079
1569.393374	186189.112232	36.756096
1570.890092	186471.801375	36.761114
1572.847524	186774.535545	36.766132
1574.146019	187056.038106	36.771149
1575.839298	187349.417433	36.776167
1577.462922	187645.551629	36.781184
1578.957533	187936.474480	36.786202
1580.670332	188247.785403	36.791220
1581.847846	188540.842272	36.796237
1584.112104	188830.402440	36.801255
1585.414451	189131.950309	36.806272
1587.264846	189440.525234	36.811290
1588.711444	189726.812066	36.816308
1590.402242	190027.590313	36.821325
1592.506783	190336.026274	36.826343
1593.746752	190639.645296	36.831360
1595.342438	190949.762735	36.836378
1597.250505	191247.487466	36.841396
1598.914986	191544.184238	36.846413
1600.480908	191826.444225	36.851431
1602.005153	192134.340651	36.856448
1604.114683	192431.350943	36.861466
1605.319674	192734.853707	36.866484
1607.370987	193028.572433	36.871501
1608.530259	193326.597200	36.876519
1610.088736	193620.902448	36.881536
1612.384702	193917.582249	36.886554
1613.727775	194215.250095	36.891572
1615.147752	194515.573701	36.896589
1616.790712	194810.833655	36.901607
1618.293576	195116.098877	36.906624
1619.996131	195413.763948	36.911642
1621.813054	195705.544058	36.916660
1623.560592	196019.333267	36.921677
1625.370446	196303.774737	36.926695
1626.991448	196606.078204	36.931712
1628.903626	196894.111865	36.936730
1630.245132	197200.778601	36.941748
1632.021661	197484.770413	36.946765
1633.778427	197785.480202	36.951783
1635.272762	198079.220784	36.956800
1636.712754	198365.730927	36.961818
1638.167207	198656.100434	36.966836
1639.677518	198959.772357	36.971853
1641.832252	199247.010557	36.976871
1643.363727	199526.523006	36.981888
1644.638815	199798.582466	36.986906
1646.419073	200084.458280	36.991924
1647.885747	200352.271946	36.996941
1649.580111	200627.671074	37.001959
1650.780280	200906.551902	37.006976
1652.868239	201180.620239	37.011994
1654.280311	201486.623898	37.017012
1656.014995	201772.027106	37.022029
1657.383327	202059.952151	37.027047
1659.334143	202364.907758	37.032064
1661.142752	202644.382049	37.037082
1662.565374	202938.904670	37.042100
1664.036161	203238.424536	37.047117
1665.908991	203531.378902	37.052135
1667.210495	203825.515451	37.057152
1669.326468	204123.691035	37.062170
1670.817517	204430.220767	37.067188
1672.200782	204738.952487	37.072205
1673.926917	205038.359006	37.077223
1675.393181	205355.309199	37.082240
1676.947899	205663.075601	37.087258
1678.713594	205961.054721	37.092276
1680.489913	206283.521051	37.097293
1682.187653	206606.254194	37.102311
1683.589494	206919.838225	37.107328
1685.370138	207238.062986	37.112346
1687.599916	207560.841274	37.117364
1689.138778	207882.000729	37.122381
1691.129885	208190.286651	37.127399
1692.968866	208522.196359	37.132416
1694.712307	208840.860981	37.137434
1696.539746	209142.899130	37.142452
1697.917562	209465.102016	37.147469
1699.942795	209770.437789	37.152487
1701.266242	210095.368124	37.157504
1702.943558	210421.412030	37.162522
1704.867026	210737.662890	37.167540
1706.424300	211062.405361	37.172557
1708.241739	211379.511846	37.177575
1710.208366	211720.804873	37.182592
1711.914791	212040.114142	37.187610
1713.800519	212360.894494	37.192628
1715.120064	212670.560796	37.197645
1717.386039	212996.286790	37.202663
1718.855743	213324.347833	37.207680
1720.475577	213639.785483	37.212698
1722.266184	213956.085823	37.217716
1723.979693	214287.767750	37.222733
1726.073116	214613.852509	37.227751
1727.588849	214938.833975	37.232768
1729.770207	215258.173524	37.237786
1731.258718	215577.291502	37.242804
1732.681452	215909.833228	37.247821
1734.535040	216235.397944	37.252839
1736.163366	216566.917245	37.257856
1737.980348	216889.007829	37.262874
1740.190281	217213.120254	37.267892
1741.241859	217539.471876	37.272909
1743.449583	217852.559760	37.277927
1745.477972	218193.162939	37.282944
1746.627749	218509.058761	37.287962
1748.866562	218829.534866	37.292980
1750.197667	219156.732810	37.297997
1752.435724	219479.673543	37.303015
1754.056087	219810.637135	37.308032
1755.913644	220132.596145	37.313050
1757.548268	220451.059016	37.318068
1759.133234	220763.636046	37.323085
1760.959086	221055.522015	37.328103
1762.457546	221373.396828	37.333120
1764.179057	221671.751933	37.338138
1766.123446	221975.102243	37.343156
1767.492096	222284.842932	37.348173
1769.361153	222601.770947	37.353191
1771.088572	222913.462553	37.358208
1772.715612	223230.987458	37.363226
1774.841443	223553.794622	37.368244
1776.282810	223862.304828	37.373261
1777.986326	224181.392952	37.378279
1779.198373	224505.613428	37.383296
1781.205894	224829.252171	37.388314
1783.071127	225165.335792	37.393332
1784.597935	225498.931969	37.398349
1786.468343	225833.363516	37.403367
1788.417082	226167.325520	37.408384
1790.148031	226512.448571	37.413402
1792.175516	226844.289658	37.418420
1793.735090	227179.379437	37.423437
1795.392445	227510.033556	37.428455
1797.328593	227866.784776	37.433472
1799.073662	228218.357986	37.438490
1800.881885	228553.662632	37.443508
1802.630253	228901.297520	37.448525
1804.549104	229246.644665	37.453543
1806.351757	229613.908155	37.458560
1807.607648	229959.993898	37.463578
1809.735823	230313.030727	37.468596
1811.435009	230683.282234	37.473613
1813.473172	231036.536059	37.478631
1815.217953	231401.953316	37.483648
1817.041556	231767.662888	37.488666
1819.152854	232119.736120	37.493684
1821.005079	232479.623290	37.498701
1822.841361	232837.785263	37.503719
1824.655109	233200.497825	37.508736
1826.363035	233569.526855	37.513754
1828.523895	233934.013656	37.518772
1830.468813	234293.808855	37.523789
1832.534340	234654.042167	37.528807
1834.624685	235026.820775	37.533824
1836.395245	235383.822544	37.538842
1838.441985	235740.780783	37.543860
1840.135664	236091.544627	37.548877
1842.088418	236444.985805	37.553895
1844.057742	236800.710382	37.558912
1846.190419	237157.272767	37.563930
1847.803797	237508.276439	37.568948
1849.299734	237867.655906	37.573965
1851.817415	238226.290814	37.578983
1853.437064	238579.959727	37.584000
1855.265937	238932.045882	37.589018
1856.961735	239287.531112	37.594036
1859.302995	239647.538338	37.599053
1860.674254	240001.015795	37.604071
1862.739190	240353.215703	37.609088
1864.243829	240711.853669	37.614106
1866.572479	241072.242056	37.619124
1868.295420	241442.708214	37.624141
1870.434248	241790.576075	37.629159
1872.194781	242145.056672	37.634176
1873.774409	242504.061422	37.639194
1875.954074	242857.560871	37.644212
1878.048827	243222.987123	37.649229
1879.494628	243573.120085	37.654247
1881.599143	243913.064430	37.659264
1883.426972	244259.630916	37.664282
1885.287755	244588.231813	37.669300
1886.419775	244931.629110	37.674317
1888.394559	245271.820224	37.679335
1890.748189	245610.935382	37.684352
1892.423805	245943.170299	37.689370
1893.846982	246290.457172	37.694388
1895.725694	246642.117615	37.699405
1897.455107	246988.999677	37.704423
1899.605535	247353.215994	37.709440
1901.171695	247709.876857	37.714458
1903.069608	248056.527338	37.719476
1904.814884	248422.329069	37.724493
1906.828910	248787.605345	37.729511
1908.645004	249156.010911	37.734528
1910.552922	249525.976259	37.739546
1912.360955	249891.587245	37.744564
1913.949714	250274.937042	37.749581
1915.757630	250652.510776	37.754599
1917.837741	251026.154524	37.759616
1919.442245	251412.649009	37.764634
1921.643907	251797.093154	37.769652
1923.414039	252192.552061	37.774669
1925.457622	252583.750457	37.779687
1927.111666	252977.498152	37.784704
1929.268818	253377.338677	37.789722
1931.349077	253770.001489	37.794740
1932.782330	254172.899668	37.799757
1935.151036	254562.466986	37.804775
1937.365659	254958.077450	37.809792
1939.267987	255381.296040	37.814810
1941.498727	255768.519218	37.819828
1942.953617	256179.257121	37.824845
1945.137814	256582.818144	37.829863
1947.274495	256981.305160	37.834880
1948.781173	257384.410882	37.839898
1951.055795	257789.020822	37.844916
1953.136357	258196.707914	37.849933
1955.464880	258613.651508	37.854951
1957.557624	259011.326150	37.859968
1959.255343	259417.214851	37.864986
1961.541521	259827.048765	37.870004
1963.412706	260238.394011	37.875021
1965.522337	260638.753010	37.880039
1967.895034	261029.417413	37.885056
1969.518399	261440.873361	37.890074
1971.861661	261826.612025	37.895092
1974.000455	262232.752041	37.900109
1975.833094	262640.716452	37.905127
1977.999307	263036.587707	37.910144
1979.638597	263433.657542	37.915162
1981.909551	263830.423876	37.920180
1984.384221	264227.436246	37.925197
1986.407439	264630.994570	37.930215
1988.376091	265025.847941	37.935232
1989.817457	265419.537744	37.940250
1992.070193	265817.162914	37.945268
1993.412114	266209.011085	37.950285
1996.284526	266612.758876	37.955303
1997.963996	267014.456587	37.960320
1999.866569	267409.590307	37.965338
2002.458825	267804.690702	37.970356
2004.407252	268201.058536	37.975373
2006.007377	268599.231697	37.980391
2008.055000	268979.960816	37.985408
2009.868629	269377.436923	37.990426
2012.324849	269782.760342	37.995444
2013.712809	270167.499081	38.000461
2015.935918	270554.594503	38.005479
2017.912864	270925.319914	38.010496
2019.853275	271303.516378	38.015514
2022.017745	271678.476100	38.020532
2023.511189	272050.212170	38.025549
2025.624905	272433.913278	38.030567
2027.787086	272810.138363	38.035584
2029.533012	273196.585718	38.040602
2031.884268	273584.333438	38.045620
2033.869750	273971.603279	38.050637
2035.253565	274360.235302	38.055655
2037.385546	274753.903943	38.060672
2038.985345	275148.593639	38.065690
2041.339771	275549.690203	38.070708
2043.310480	275956.355783	38.075725
2044.707776	276376.060986	38.080743
2047.616390	276776.429839	38.085760
2049.690724	277198.437388	38.090778
2051.475818	277611.955008	38.095796
2053.813137	278015.632182	38.100813
2055.688488	278436.622958	38.105831
2057.702631	278850.047344	38.110848
2059.521656	279289.606124	38.115866
2061.859790	279709.146138	38.120884
2063.911139	280131.674468	38.125901
2065.948906	280561.541569	38.130919
2067.794597	280973.431547	38.135936
2070.103715	281411.910741	38.140954
2072.189606	281847.197161	38.145972
2074.060112	282272.661780	38.150989
2076.120041	282707.693116	38.156007
2078.306166	283143.971732	38.161024
2080.711560	283581.990895	38.166042
2082.687349	284020.861729	38.171060
2084.880959	284465.231436	38.176077
2086.796664	284901.236660	38.181095
2089.298736	285342.276734	38.186112
2091.192179	285782.723567	38.191130
2093.318137	286216.148193	38.196148
2095.082604	286666.639482	38.201165
2097.511235	287118.268028	38.206183
2100.007543	287557.745497	38.211200
2101.731857	287999.245193	38.216218
2104.007451	288445.607030	38.221236
2106.183010	288898.532451	38.226253
2108.244210	289343.448901	38.231271
2110.274729	289783.238029	38.236288
2112.815845	290239.321411	38.241306
2115.079603	290679.397882	38.246324
2117.234919	291128.146425	38.251341
2119.382859	291565.340219	38.256359
2121.917572	292008.564064	38.261376
2123.844590	292462.086587	38.266394
2125.497966	292893.406988	38.271412
2128.151582	293346.174468	38.276429
2130.104747	293783.408170	38.281447
2132.460813	294216.487948	38.286464
2134.608670	294670.213122	38.291482
2136.437782	295115.860201	38.296500
2138.380081	295556.865421	38.301517
2140.932092	296005.794690	38.306535
2142.613307	296437.516447	38.311552
2145.205351	296889.910762	38.316570
2147.324953	297326.558691	38.321588
2149.455649	297773.483571	38.326605
2151.167223	298225.903415	38.331623
2153.696912	298668.849057	38.336640
2155.999983	299100.935529	38.341658
2158.152226	299530.909714	38.346676
2159.718828	299943.252186	38.351693
2161.879797	300364.079229	38.356711
2163.640268	300792.860837	38.361728
2165.872308	301221.184476	38.366746
2167.817202	301649.879642	38.371764
2169.779525	302079.203287	38.376781
2172.011311	302532.826066	38.381799
2173.882465	302961.319102	38.386816
2176.170873	303401.648999	38.391834
2178.361387	303852.829862	38.396852
2180.389597	304301.899883	38.401869
2182.201815	304758.107443	38.406887
2184.696523	305211.386526	38.411904
2187.038276	305678.875181	38.416922
2189.032245	306133.087450	38.421940
2191.623969	306588.344375	38.426957
2193.377356	307057.841454	38.431975
2195.371258	307518.387024	38.436992
2197.780385	307996.656736	38.442010
2200.282858	308466.404036	38.447028
2202.612043	308934.803299	38.452045
2204.507477	309410.068326	38.457063
2206.642613	309885.392723	38.462080
2208.995622	310372.023929	38.467098
2211.552985	310845.140728	38.472116
2213.754618	311320.795830	38.477133
2215.677103	311804.027940	38.482151
2218.046040	312293.200452	38.487168
2220.621394	312774.696091	38.492186
2222.933220	313255.872662	38.497204
2225.187406	313735.225911	38.502221
2226.993633	314230.303421	38.507239
2229.577703	314715.381373	38.512256
2231.723063	315198.974679	38.517274
2234.133243	315682.191476	38.522292
2236.450425	316173.335717	38.527309
2238.480284	316666.296000	38.532327
2241.057814	317157.008041	38.537344
2243.794475	317648.628732	38.542362
2245.976551	318141.295043	38.547380
2248.544417	318620.851682	38.552397
2250.561858	319106.072049	38.557415
2252.805421	319587.927307	38.562432
2255.095747	320082.686353	38.567450
2257.368184	320566.150237	38.572468
2259.974973	321046.891914	38.577485
2261.790415	321544.601163	38.582503
2264.509332	322034.728348	38.587520
2266.517318	322514.582787	38.592538
2269.366323	322995.061400	38.597556
2271.301701	323474.941553	38.602573
2273.647032	323963.962730	38.607591
2276.221699	324438.504696	38.612608
2278.572985	324932.613526	38.617626
2280.945980	325415.802628	38.622644
2283.069006	325896.462461	38.627661
2285.447503	326383.039124	38.632679
2287.758032	326852.519796	38.637696
2290.154713	327339.183532	38.642714
2292.400560	327810.134649	38.647732
2294.305230	328294.859335	38.652749
2296.577382	328785.533476	38.657767
2298.910195	329264.369363	38.662784
2300.940436	329758.900131	38.667802
2303.277618	330241.224452	38.672820
2305.795756	330723.717427	38.677837
2308.012626	331203.714582	38.682855
2310.263492	331671.574087	38.687872
2312.547978	332140.158306	38.692890
2314.360477	332605.512720	38.697908
2316.685327	333056.194686	38.702925
2318.900030	333533.017223	38.707943
2321.056721	334001.775973	38.712960
2323.252191	334466.134293	38.717978
2324.993918	334953.007360	38.722996
2327.876540	335431.705163	38.728013
2329.652072	335915.947554	38.733031
2331.906492	336409.265686	38.738048
2334.457278	336896.925070	38.743066
2336.274214	337410.970897	38.748084
2338.904296	337901.090194	38.753101
2341.273675	338410.875612	38.758119
2343.846290	338920.038648	38.763136
2345.661329	339417.747153	38.768154
2348.118529	339938.099090	38.773172
2350.445214	340439.644571	38.778189
2352.392115	340965.793251	38.783207
2355.012144	341480.390452	38.788224
2357.669810	342004.155160	38.793242
2359.757908	342545.728685	38.798260
2362.350441	343073.570659	38.803277
2364.365857	343611.791240	38.808295
2366.991058	344139.332821	38.813312
2369.464213	344676.399978	38.818330
2371.460559	345221.343947	38.823348
2373.802710	345741.905817	38.828365
2376.836203	346296.433452	38.833383
2379.038335	346844.057781	38.838400
2381.669451	347382.705481	38.843418
2383.997751	347928.212965	38.848436
2386.581911	348467.459014	38.853453
2388.733323	349014.218762	38.858471
2391.450271	349558.472129	38.863488
2393.825512	350098.636928	38.868506
2396.147768	350660.454428	38.873524
2398.884686	351204.372923	38.878541
2401.158101	351764.480135	38.883559
2403.469992	352299.623318	38.888576
2406.526917	352851.577155	38.893594
2408.777593	353403.267256	38.898612
2411.135313	353946.488606	38.903629
2413.387709	354513.903070	38.908647
2416.216553	355050.642964	38.913664
2418.810107	355596.283420	38.918682
2421.041981	356150.843704	38.923700
2423.480470	356699.480484	38.928717
2426.384651	357241.671857	38.933735
2428.794745	357801.371422	38.938752
2431.010268	358331.762384	38.943770
2433.408834	358889.542686	38.948788
2436.086203	359429.500119	38.953805
2438.634498	359991.799417	38.958823
2441.102540	360525.103596	38.963840
2443.651762	361077.040825	38.968858
2445.727944	361625.493391	38.973876
2448.461705	362163.846758	38.978893
2451.071261	362712.195863	38.983911
2453.321566	363248.907001	38.988928
2455.764728	363794.727533	38.993946
2458.149288	364353.066986	38.998964
2460.643065	364889.557965	39.003981
2463.262583	365433.495574	39.008999
2465.790885	365980.731773	39.014016
2468.175635	366531.173153	39.019034
2470.988966	367066.053271	39.024052
2473.317158	367584.299504	39.029069
2475.706028	368094.671238	39.034087
2478.216133	368605.065532	39.039104
2480.477550	369109.864111	39.044122
2482.388153	369642.733784	39.049140
2485.133078	370147.767559	39.054157
2487.556579	370663.661987	39.059175
2489.920599	371190.350124	39.064192
2492.628048	371709.956121	39.069210
2495.074819	372251.382897	39.074228
2497.051858	372778.126749	39.079245
2499.143983	373318.929297	39.084263
2501.565099	373865.091503	39.089280
2504.747070	374407.576899	39.094298
2506.432740	374962.218027	39.099316
2509.233459	375506.210517	39.104333
2511.452876	376062.037662	39.109351
2513.973252	376628.243386	39.114368
2516.694545	377195.368359	39.119386
2518.854599	377760.998513	39.124404
2521.540355	378323.140040	39.129421
2524.357853	378899.003601	39.134439
2526.579276	379475.454446	39.139456
2529.319967	380048.341298	39.144474
2531.460143	380629.794778	39.149492
2534.263714	381219.971178	39.154509
2536.963490	381796.979941	39.159527
2539.422356	382386.474570	39.164544
2542.330766	382963.829916	39.169562
2544.451819	383560.467345	39.174580
2547.575038	384142.295973	39.179597
2550.212600	384734.140018	39.184615
2552.466484	385323.421896	39.189632
2554.814893	385923.792433	39.194650
2557.913641	386521.144493	39.199668
2560.447914	387110.264848	39.204685
2562.946767	387720.925901	39.209703
2565.431356	388314.279762	39.214720
2568.412776	388904.984364	39.219738
2570.641554	389513.769912	39.224756
2573.388553	390113.521606	39.229773
2575.979653	390708.978846	39.234791
2578.511041	391318.254745	39.239808
2581.299555	391922.715506	39.244826
2583.716197	392525.143415	39.249844
2586.492798	393126.740560	39.254861
2589.294095	393721.483597	39.259879
2591.972003	394337.850359	39.264896
2594.700559	394936.169441	39.269914
2597.499718	395547.575068	39.274932
2600.102581	396150.541082	39.279949
2602.770591	396750.646570	39.284967
2605.268370	397351.674672	39.289984
2608.490265	397951.409860	39.295002
2610.597961	398547.811116	39.300020
2613.288933	399144.763994	39.305037
2616.012209	399746.505297	39.310055
2618.697478	400353.298683	39.315072
2621.854623	400948.714980	39.320090
2624.219978	401543.936048	39.325108
2626.851696	402143.705857	39.330125
2629.753025	402740.684737	39.335143
2632.445837	403327.609069	39.340160
2635.021340	403917.876825	39.345178
2637.277841	404510.203428	39.350196
2639.596479	405105.693012	39.355213
2642.666545	405691.434284	39.360231
2645.367041	406286.782247	39.365248
2648.125359	406844.558021	39.370266
2650.252114	407413.348559	39.375284
2652.964530	407975.556106	39.380301
2655.681334	408546.401125	39.385319
2657.913276	409115.586899	39.390336
2660.593267	409681.348521	39.395354
2663.313580	410260.142775	39.400372
2665.484182	410829.141912	39.405389
2668.269920	411401.166726	39.410407
2670.380996	412002.675392	39.415424
2672.932263	412572.328230	39.420442
2675.872730	413177.468740	39.425460
2678.601139	413772.609209	39.430477
2680.783103	414376.468744	39.435495
2683.252046	414995.795631	39.440512
2686.593402	415598.629934	39.445530
2689.035829	416218.279471	39.450548
2691.879143	416828.440381	39.455565
2694.678055	417427.817453	39.460583
2696.933822	418067.369689	39.465600
2699.995558	418670.868044	39.470618
2702.565565	419300.977049	39.475636
2704.919827	419933.578774	39.480653
2707.946913	420565.044592	39.485671
2710.622691	421192.753408	39.490688
2713.600991	421830.964411	39.495706
2716.061226	422473.838119	39.500724
2718.638896	423109.897681	39.505741
2721.421358	423755.158384	39.510759
2723.723937	424407.552236	39.515776
2727.131365	425065.263302	39.520794
2729.742556	425716.100519	39.525812
2732.453528	426366.850558	39.530829
2735.298401	427016.901365	39.535847
2738.169026	427682.295110	39.540864
2740.841326	428345.625083	39.545882
2743.563066	429012.463663	39.550900
2745.954500	429677.612841	39.555917
2749.148494	430333.869639	39.560935
2751.863398	431009.436895	39.565952
2754.892092	431667.898950	39.570970
2757.315726	432336.592192	39.575988
2760.432665	433003.435739	39.581005
2763.341715	433676.909314	39.586023
2766.304965	434354.798131	39.591040
2768.931679	435025.186217	39.596058
2771.797516	435697.787493	39.601076
2774.275753	436370.476323	39.606093
2777.716388	437034.805336	39.611111
2780.319324	437716.673939	39.616128
2783.560443	438372.701016	39.621146
2786.105444	439050.943410	39.626164
2788.882747	439730.337609	39.631181
2791.591386	440388.449239	39.636199
2794.275560	441066.092000	39.641216
2797.631919	441734.966827	39.646234
2800.609880	442399.330527	39.651252
2803.425028	443074.606591	39.656269
2806.426506	443739.827791	39.661287
2809.224449	444404.602255	39.666304
2812.404344	445060.100700	39.671322
2814.900334	445725.329137	39.676340
2818.208553	446376.770462	39.681357
2820.657976	447029.484331	39.686375
2823.298603	447696.234257	39.691392
2826.427994	448357.833426	39.696410
2829.268267	449014.908930	39.701428
2831.926736	449651.437773	39.706445
2834.990724	450275.005068	39.711463
2837.366262	450908.554461	39.716480
2839.698787	451524.972375	39.721498
2842.936386	452152.889923	39.726516
2845.671944	452784.852097	39.731533
2848.572960	453400.863521	39.736551
2850.656064	454036.719706	39.741568
2853.859475	454677.021870	39.746586
2856.827234	455312.491622	39.751604
2859.314063	455952.203023	39.756621
2862.216401	456595.510616	39.761639
2864.830158	457254.788836	39.766656
2867.525928	457904.540717	39.771674
2870.328632	458560.862853	39.776692
2872.937218	459229.857498	39.781709
2875.967387	459892.098847	39.786727
2878.588487	460588.289516	39.791744
2881.534889	461249.078508	39.796762
2884.077355	461937.859161	39.801780
2886.982595	462627.362470	39.806797
2889.933668	463314.661001	39.811815
2892.702730	464022.494179	39.816832
2895.631038	464714.733995	39.821850
2898.459680	465408.575195	39.826868
2901.081252	466125.322565	39.831885
2903.912243	466838.071774	39.836903
2907.065772	467554.876233	39.841920
2910.137923	468274.890567	39.846938
2913.018356	469015.734153	39.851956
2915.987030	469742.459253	39.856973
2918.613796	470460.632087	39.861991
2921.574726	471185.680615	39.867008
2924.747664	471928.515450	39.872026
2927.756103	472669.829330	39.877044
2930.713978	473400.427415	39.882061
2933.996413	474139.815941	39.887079
2936.448691	474886.409489	39.892096
2939.848945	475625.560118	39.897114
2943.183125	476374.618647	39.902132
2945.970481	477120.450786	39.907149
2949.000017	477859.354415	39.912167
2952.051479	478610.922909	39.917184
2955.370621	479341.042140	39.922202
2958.520008	480080.982677	39.927220
2960.935693	480832.897632	39.932237
2964.355450	481568.693821	39.937255
2967.533846	482316.033718	39.942272
2970.004129	483057.955689	39.947290
2973.638660	483806.362178	39.952308
2976.916024	484544.458789	39.957325
2980.049817	485278.159034	39.962343
2982.792193	486019.644614	39.967360
2985.451670	486760.351670	39.972378
2989.000114	487503.604360	39.977396
2991.838535	488240.786020	39.982413
2995.104872	488978.167336	39.987431
2998.092471	489714.951981	39.992448
3001.198034	490455.510365	39.997466
3004.313371	491195.728703	40.002484
3007.009726	491930.184321	40.007501
3010.218596	492660.646043	40.012519
3012.937306	493396.587534	40.017536
3016.392681	494128.248326	40.022554
3019.233353	494855.739532	40.027572
3022.257059	495596.660673	40.032589
3025.400436	496320.608747	40.037607
3028.472722	497053.141686	40.042624
3031.224847	497781.862084	40.047642
3034.271739	498473.348112	40.052660
3036.852481	499175.999343	40.057677
3040.067278	499871.369784	40.062695
3043.125446	500575.338691	40.067712
3046.068169	501269.778776	40.072730
3048.970754	501970.785015	40.077748
3051.635239	502673.102971	40.082765
3054.946572	503374.782303	40.087783
3058.044596	504088.990942	40.092800
3060.439080	504807.953720	40.097818
3063.658570	505529.518777	40.102836
3066.452844	506258.409399	40.107853
3069.565131	506974.886495	40.112871
3072.484251	507714.801760	40.117888
3075.614639	508457.814593	40.122906
3078.703141	509198.732353	40.127924
3081.201131	509955.296833	40.132941
3084.529070	510697.808299	40.137959
3087.825743	511459.548583	40.142976
3090.930262	512227.915998	40.147994
3094.308713	512982.670005	40.153012
3096.888974	513747.112682	40.158029
3100.056035	514503.627200	40.163047
3103.160497	515284.697953	40.168064
3106.183320	516073.681223	40.173082
3109.338907	516851.738663	40.178100
3111.977936	517641.546312	40.183117
3115.539073	518423.472655	40.188135
3118.664648	519217.586893	40.193152
3121.619204	520019.422117	40.198170
3125.282924	520809.387944	40.203188
3128.205653	521617.767759	40.208205
3131.430150	522423.840541	40.213223
3134.562536	523226.612836	40.218240
3137.746756	524027.469583	40.223258
3141.375148	524820.119061	40.228276
3144.623842	525631.270275	40.233293
3147.694736	526435.868387	40.238311
3151.032782	527250.121812	40.243328
3154.328195	528053.330283	40.248346
3157.538372	528854.242587	40.253364
3160.174839	529667.149960	40.258381
3164.008803	530470.075889	40.263399
3167.412986	531298.632723	40.268416
3170.437399	532099.676251	40.273434
3173.351194	532905.709135	40.278452
3176.645573	533721.373477	40.283469
3179.971566	534524.328506	40.288487
3183.170119	535331.169381	40.293504
3186.590312	536156.248910	40.298522
3190.126853	536965.996263	40.303540
3193.114365	537778.187450	40.308557
3196.653112	538582.912329	40.313575
3200.370734	539391.523178	40.318592
3203.166861	540200.126006	40.323610
3206.861678	540996.391997	40.328628
3209.673155	541797.964455	40.333645
3213.158190	542596.921682	40.338663
3216.563199	543395.288466	40.343680
3219.612377	544192.806878	40.348698
3223.158489	544985.581037	40.353716
3226.220734	545790.219031	40.358733
3229.483757	546583.637513	40.363751
3232.761767	547379.360079	40.368768
3235.806172	548169.600858	40.373786
3239.668802	548967.937868	40.378804
3242.195794	549758.056878	40.383821
3245.357193	550534.536560	40.388839
3248.972437	551298.711294	40.393856
3251.379059	552054.302771	40.398874
3254.856837	552802.460141	40.403892
3257.865130	553561.373019	40.408909
3261.149723	554316.284859	40.413927
3264.456751	555071.647099	40.418944
3267.225832	555833.812549	40.423962
3270.687293	556603.038526	40.428980
3274.059382	557367.718435	40.433997
3277.345556	558136.572242	40.439015
3280.648316	558921.058234	40.444032
3283.460272	559697.952812	40.449050
3286.723319	560481.239317	40.454068
3290.353209	561269.927499	40.459085
3293.167977	562053.680574	40.464103
3296.357206	562862.369551	40.469120
3299.422060	563673.877261	40.474138
3303.029792	564477.830917	40.479156
3306.468638	565284.960813	40.484173
3309.342272	566098.433044	40.489191
3312.742258	566923.533772	40.494208
3315.976160	567749.653106	40.499226
3319.107196	568572.074321	40.504244
3322.590608	569404.594957	40.509261
3325.553264	570230.979022	40.514279
3328.875815	571085.479823	40.519296
3332.103525	571935.877096	40.524314
3335.603836	572782.064095	40.529332
3339.319017	573648.223132	40.534349
3342.078930	574512.813849	40.539367
3345.398071	575372.146991	40.544384
3348.893416	576247.048014	40.549402
3352.373933	577102.170922	40.554420
3355.973718	577978.921805	40.559437
3359.071251	578861.935343	40.564455
3362.313860	579737.553412	40.569472
3365.736876	580629.929516	40.574490
3369.141628	581506.783109	40.579508
3372.687725	582395.046781	40.584525
3375.823773	583286.853244	40.589543
3379.554319	584174.394506	40.594560
3382.884293	585073.475475	40.599578
3386.531136	585975.632442	40.604596
3389.908363	586870.058951	40.609613
3393.392273	587766.094672	40.614631
3396.666606	588661.289506	40.619648
3399.847296	589561.222500	40.624666
3403.800326	590469.304784	40.629684
3407.303347	591365.938539	40.634701
3410.184899	592266.041949	40.639719
3414.507044	593163.596390	40.644736
3417.621077	594069.606502	40.649754
3421.309274	594970.504805	40.654772
3424.664508	595858.043389	40.659789
3428.283809	596769.138369	40.664807
3431.876067	597667.475114	40.669824
3435.332305	598560.463715	40.674842
3438.800134	599459.116389	40.679860
3442.207097	600358.700035	40.684877
3445.315586	601248.069363	40.689895
3448.594583	602153.259205	40.694912
3451.715406	603055.600012	40.699930
3455.171007	603954.116936	40.704948
3459.318645	604869.564148	40.709965
3462.300791	605780.771258	40.714983
3466.449481	606689.220704	40.720000
3469.573836	607592.960563	40.725018
3473.227377	608476.633353	40.730023
3476.662985	609318.168474	40.735028
3480.260570	610122.905764	40.740032
3483.493115	610867.435944	40.745037
3486.825189	611565.698710	40.750042
3489.527782	612180.321994	40.755047
3492.196817	612756.569960	40.760052
3494.688176	613279.924964	40.765056
3497.475080	613746.222342	40.770061
3500.037208	614163.948677	40.775066
3502.294494	614515.228800	40.780071
3504.387648	614817.890900	40.785076
3505.857329	615091.903087	40.790080
3507.981277	615305.131711	40.795085
3509.607450	615484.348895	40.800090
3511.595769	615615.528436	40.805095
3512.795364	615703.849793	40.810100
3514.002388	615765.981681	40.815104
3515.453452	615790.293141	40.820109
3516.057990	615792.197669	40.825114
3517.622887	615749.423244	40.830119
3518.565237	615682.157467	40.835124
3519.336661	615585.031664	40.840128
3520.361061	615473.221915	40.845133
3520.729445	615335.774635	40.850138
3521.492375	615173.624075	40.855143
3522.307064	614995.219291	40.860148
3522.576240	614818.845879	40.865152
3522.805475	614600.190883	40.870157
3523.151240	614379.713523	40.875162
3523.825657	614146.783854	40.880167
3524.219241	613903.095836	40.885172
3523.734899	613651.741237	40.890176
3523.859711	613385.388699	40.895181
3524.034596	613116.621811	40.900186
3524.229340	612841.295874	40.905191
3524.715325	612563.767244	40.910196
3524.288684	612263.326628	40.915200
3524.504068	611972.025815	40.920205
3524.376829	611676.620476	40.925210
3524.239409	611371.908488	40.930215
3524.417294	611071.838010	40.935220
3524.572425	610766.662121	40.940224
3524.969608	610456.438977	40.945229
3524.895605	610147.930168	40.950234
3524.325260	609823.387793	40.955239
3523.897759	609510.714462	40.960244
3523.793113	609205.032298	40.965248
3524.038860	608887.033699	40.970253
3523.430289	608573.509784	40.975258
3523.476359	608263.074763	40.980263
3523.296492	607952.515603	40.985268
3523.103138	607636.647402	40.990272
3523.180290	607325.128753	40.995277
3522.631814	607017.950099	41.000282
3522.198139	606700.189898	41.005287
3522.553872	606401.304983	41.010292
3522.158573	606102.778915	41.015296
3522.050915	605803.999121	41.020301
3521.523285	605512.730297	41.025306
3521.523617	605208.263339	41.030311
3521.710681	604906.409781	41.035316
3520.809626	604622.928808	41.040320
3520.441026	604330.350989	41.045325
3520.589001	604047.340665	41.050330
3520.283846	603771.848680	41.055335
3519.965752	603491.698004	41.060340
3520.152292	603210.960494	41.065344
3519.858935	602925.836930	41.070349
3519.408652	602651.789030	41.075354
3519.229111	602385.097768	41.080359
3518.823128	602118.435070	41.085364
3518.327489	601854.832263	41.090368
3518.119381	601585.072271	41.095373
3518.337715	601341.963660	41.100378
3518.355305	601095.477510	41.105383
3517.476019	600830.457398	41.110388
3517.114329	600589.524019	41.115392
3517.103332	600336.517885	41.120397
3516.906252	600100.552672	41.125402
3516.189056	599867.366360	41.130407
3516.383874	599642.491569	41.135412
3516.276440	599415.707026	41.140416
3516.282153	599179.889614	41.145421
3515.612475	598948.527559	41.150426
3515.849410	598731.035282	41.155431
3515.710744	598511.744996	41.160436
3515.069511	598292.428582	41.165440
3515.036078	598065.102719	41.170445
3514.957479	597852.197295	41.175450
3514.556640	597653.806567	41.180455
3514.648585	597448.826575	41.185460
3514.501445	597236.019562	41.190464
3514.146138	597025.093296	41.195469
3513.845385	596843.794725	41.200474
3513.692511	596639.838675	41.205479
3513.122150	596449.813383	41.210484
3512.923325	596273.195685	41.215488
3513.319588	596082.562052	41.220493
3513.223475	595891.601384	41.225498
3512.966060	595706.521106	41.230503
3513.075929	595511.064834	41.235508
3512.861313	595337.238187	41.240512
3512.584505	595158.661181	41.245517
3512.379422	594987.581511	41.250522
3512.282414	594812.375813	41.255527
3512.317159	594640.652137	41.260532
3511.530016	594481.974662	41.265536
3511.643810	594303.973272	41.270541
3511.144263	594138.985695	41.275546
3510.642874	593980.306151	41.280551
3510.958507	593826.154188	41.285556
3510.451217	593681.894863	41.290560
3510.349618	593524.598449	41.295565
3510.474639	593384.343128	41.300570
3510.188563	593234.784300	41.305575
3510.138207	593091.046580	41.310580
3510.272983	592954.841057	41.315584
3510.054728	592802.260381	41.320589
3509.456168	592673.027863	41.325594
3509.276545	592537.417142	41.330599
3509.748049	592406.561557	41.335604
3509.457883	592282.635647	41.340608
3509.459861	592145.038072	41.345613
3509.586518	592018.088611	41.350618
3509.496517	591880.351746	41.355623
3509.115241	591764.148184	41.360628
3509.023677	591634.773789	41.365632
3509.048606	591503.626358	41.370637
3509.003154	591384.110115	41.375642
3508.697359	591257.419641	41.380647
3508.961410	591141.859876	41.385652
3507.934546	591029.907176	41.390656
3508.388875	590900.238217	41.395661
3508.489881	590790.561415	41.400666
3508.325552	590676.716813	41.405671
3508.434762	590551.506159	41.410676
3508.094139	590453.467539	41.415680
3507.920442	590333.057901	41.420685
3507.558873	590221.944660	41.425690
3507.814535	590118.799848	41.430695
3507.414767	590010.796587	41.435700
3507.622484	589909.310576	41.440704
3507.745869	589805.482038	41.445709
3507.245034	589713.774489	41.450714
3507.348052	589604.436019	41.455719
3507.051772	589507.584318	41.460724
3507.069765	589419.099928	41.465728
3507.347634	589314.290562	41.470733
3507.218474	589232.190789	41.475738
3506.730218	589131.908564	41.480743
3506.908320	589040.790622	41.485748
3506.816977	588955.476132	41.490752
3506.835292	588848.899048	41.495757
3506.784697	588758.866704	41.500762
3506.511726	588664.258578	41.505767
3506.445564	588583.547018	41.510772
3506.219658	588505.615728	41.515776
3506.225314	588417.375613	41.520781
3506.595270	588340.402245	41.525786
3506.409169	588256.149327	41.530791
3506.361766	588166.712866	41.535796
3506.041913	588078.621098	41.540800
3506.214601	587995.713126	41.545805
3505.775448	587927.231616	41.550810
3506.066950	587850.116707	41.555815
3505.811050	587759.757390	41.560820
3505.855313	587686.789048	41.565824
3506.451169	587606.467836	41.570829
3505.447624	587535.165621	41.575834
3505.809995	587461.143800	41.580839
3505.610528	587374.831536	41.585844
3505.669082	587314.286344	41.590848
3505.305145	587221.884820	41.595853
3505.271835	587155.740430	41.600858
3505.340024	587100.354227	41.605863
3505.287633	587033.109573	41.610868
3505.434471	586974.853936	41.615872
3505.546934	586896.357055	41.620877
3505.348670	586818.108643	41.625882
3505.381170	586759.067887	41.630887
3505.341367	586688.461411	41.635892
3505.491641	586612.863282	41.640896
3505.253751	586544.942988	41.645901
3505.108385	586492.644174	41.650906
3504.968719	586429.819692	41.655911
3505.172565	586355.263855	41.660916
3504.742904	586292.233329	41.665920
3505.167326	586228.467507	41.670925
3504.782599	586156.708683	41.675930
3504.526703	586102.119843	41.680935
3505.177072	586034.909522	41.685940
3504.719960	585983.158186	41.690944
3505.094841	585912.030786	41.695949
3504.709053	585865.079181	41.700954
3504.486131	585799.507517	41.705959
3504.888887	585741.556126	41.710964
3504.291975	585688.472007	41.715968
3504.650175	585628.020968	41.720973
3504.768807	585584.297252	41.725978
3504.637594	585526.378075	41.730983
3504.033453	585450.238261	41.735988
3504.412207	585408.879001	41.740992
3504.463125	585353.135780	41.745997
3504.182802	585307.267967	41.751002
3504.072591	585250.095873	41.756007
3504.344438	585202.687756	41.761012
3504.294868	585164.702615	41.766016
3504.490627	585104.574816	41.771021
3504.107795	585049.098346	41.776026
3504.056459	585005.048024	41.781031
3504.167469	584959.117574	41.786036
3504.166458	584908.643180	41.791040
3504.304495	584847.921511	41.796045
3504.402719	584805.751722	41.801050
3504.202955	584747.087273	41.806055
3504.029191	584688.769319	41.811060
3504.193147	584649.495890	41.816064
3504.023581	584592.379766	41.821069
3504.116388	584539.232366	41.826074
3503.791796	584501.638798	41.831079
3503.837242	584460.328067	41.836084
3503.481754	584412.112339	41.841088
3503.738789	584366.407208	41.846093
3503.490455	584334.214780	41.851098
3503.908919	584289.336242	41.856103
3503.482777	584251.557185	41.861108
3503.886274	584214.801220	41.866112
3504.136409	584162.830449	41.871117
3503.597299	584116.296323	41.876122
3503.731668	584066.398418	41.881127
3504.180670	584012.791764	41.886132
3503.584988	583982.557464	41.891136
3503.580159	583934.485329	41.896141
3503.507197	583886.574020	41.901146
3503.597993	583858.387584	41.906151
3503.536375	583819.196579	41.911156
3503.314222	583776.521504	41.916160
3503.602393	583731.360284	41.921165
3503.747757	583699.605738	41.926170
3503.180352	583653.826013	41.931175
3503.593731	583599.922139	41.936180
3503.165973	583566.251614	41.941184
3503.339843	583525.468720	41.946189
3503.384601	583495.132956	41.951194
3503.414319	583453.871029	41.956199
3503.461261	583408.696067	41.961204
3503.491511	583373.349169	41.966208
3503.396829	583337.470248	41.971213
3503.451635	583297.507219	41.976218
3503.224453	583257.036683	41.981223
3503.453645	583219.903596	41.986228
3503.284773	583179.724449	41.991232
3503.539909	583136.069903	41.996237
3503.235070	583114.811477	42.001242
3503.393723	583078.290524	42.006247
3503.192532	583037.313795	42.011252
3503.073636	583004.495646	42.016256
3502.887680	582971.437219	42.021261
3503.252415	582938.041939	42.026266
3503.533563	582904.308695	42.031271
3503.439393	582868.277766	42.036276
3503.413351	582833.840334	42.041280
3503.735137	582790.374533	42.046285
3503.380728	582750.473492	42.051290
3503.362779	582714.680814	42.056295
3503.352452	582672.369411	42.061300
3503.383265	582641.131063	42.066304
3503.414203	582596.556882	42.071309
3503.478438	582559.547628	42.076314
3503.311909	582524.278904	42.081319
3503.286534	582483.272630	42.086324
3503.246001	582451.643820	42.091328
3503.223865	582411.138121	42.096333
3503.259022	582386.917296	42.101338
3503.427865	582352.698571	42.106343
3503.588253	582302.237117	42.111348
3503.055434	582277.152266	42.116352
3503.692498	582226.064451	42.121357
3503.671561	582189.267815	42.126362
3503.542051	582159.356708	42.131367
3503.414265	582119.016862	42.136372
3502.916303	582079.185969	42.141376
3503.248188	582047.798602	42.146381
3502.918283	582013.857345	42.151386
3502.927118	581975.099998	42.156391
3503.146212	581943.328871	42.161396
3503.244632	581912.980365	42.166400
3502.886154	581880.346737	42.171405
3502.743482	581859.311223	42.176410
3503.169113	581819.284869	42.181415
3502.910675	581782.874973	42.186420
3503.129228	581757.420786	42.191424
3502.911628	581715.238395	42.196429
3502.609986	581688.461498	42.201434
3503.127088	581673.138546	42.206439
3503.250871	581626.089147	42.211444
3502.840690	581598.276086	42.216448
3502.718381	581556.579581	42.221453
3502.857801	581542.819665	42.226458
3503.214884	581513.382270	42.231463
3503.027909	581467.533981	42.236468
3503.081715	581447.018501	42.241472
3503.309279	581408.776512	42.246477
3502.855231	581373.599200	42.251482
3502.952343	581343.249337	42.256487
3503.523722	581304.000577	42.261492
3503.010387	581283.573456	42.266496
3503.286021	581239.055829	42.271501
3503.164149	581201.720141	42.276506
3502.939360	581176.534490	42.281511
3503.123814	581140.755213	42.286516
3502.985902	581120.670228	42.291520
3503.031650	581084.862313	42.296525
3502.917782	581051.586303	42.301530
3503.114883	581017.559598	42.306535
3503.139270	580976.489815	42.311540
3502.797533	580948.764702	42.316544
3503.135783	580919.479102	42.321549
3502.915076	580874.786895	42.326554
3502.970889	580854.621000	42.331559
3503.114115	580813.181039	42.336564
3502.927612	580785.581677	42.341568
3502.772089	580760.584821	42.346573
3502.930619	580733.031674	42.351578
3502.534661	580705.565143	42.356583
3502.816979	580668.615757	42.361588
3502.594583	580648.242264	42.366592
3502.803449	580602.027651	42.371597
3502.882664	580583.913483	42.376602
3502.524401	580551.727192	42.381607
3502.932060	580532.809441	42.386612
3502.491228	580514.826604	42.391616
3502.863626	580491.401355	42.396621
3503.294775	580453.425111	42.401626
3502.991480	580429.954932	42.406631
3502.747522	580395.995273	42.411636
3502.581800	580376.565163	42.416640
3502.649212	580336.689750	42.421645
3502.744048	580317.870683	42.426650
3502.634012	580287.399881	42.431655
3502.570431	580257.373038	42.436660
3502.802278	580234.119655	42.441664
3502.491427	580207.440904	42.446669
3503.057651	580175.008703	42.451674
3502.863392	580153.326124	42.456679
3502.863951	580115.416039	42.461684
3502.750455	580091.865328	42.466688
3502.836778	580051.685063	42.471693
3502.870141	580031.922351	42.476698
3502.994569	580000.160459	42.481703
3502.962609	579970.579212	42.486708
3502.447368	579951.353435	42.491712
3502.845877	579915.837628	42.496717
3502.948711	579894.108098	42.501722
3502.564960	579870.147846	42.506727
3503.051991	579831.207956	42.511732
3502.776809	579802.115605	42.516736
3502.795761	579774.531756	42.521741
3502.870635	579745.033502	42.526746
3502.622396	579726.618099	42.531751
3502.776013	579691.440744	42.536756
3502.345332	579667.988867	42.541760
3502.408508	579627.860838	42.546765
3502.442985	579615.468931	42.551770
3502.825286	579594.046161	42.556775
3503.094222	579560.304653	42.561780
3502.956372	579532.243237	42.566784
3503.267504	579505.716306	42.571789
3503.008589	579476.369818	42.576794
3502.502828	579429.459676	42.581799
3502.617307	579402.762648	42.586804
3502.990603	579383.647726	42.591808
3502.864396	579359.345217	42.596813
3502.876580	579323.486725	42.601818
3502.921258	579296.800356	42.606823
3502.894213	579266.113184	42.611828
3502.593023	579235.819832	42.616832
3502.686470	579214.541789	42.621837
3502.505095	579186.285706	42.626842
3502.417431	579157.312803	42.631847
3502.658952	579129.542113	42.636852
3502.412599	579114.335000	42.641856
3502.640189	579084.760973	42.646861
3502.674161	579057.674503	42.651866
3502.880148	579041.644322	42.656871
3503.127136	579002.939668	42.661876
3502.335590	578981.448479	42.666880
3502.592414	578958.840490	42.671885
3502.990969	578929.339627	42.676890
3502.766405	578896.726430	42.681895
3502.743617	578876.719691	42.686900
3502.740402	578847.231269	42.691904
3502.912134	578798.507411	42.696909
3502.872448	578781.762990	42.701914
3502.579125	578754.927558	42.706919
3502.783350	578715.376014	42.711924
3502.749837	578688.901021	42.716928
3502.619455	578669.462403	42.721933
3502.802848	578639.292281	42.726938
3502.733000	578621.800052	42.731943
3502.981376	578594.277722	42.736948
3502.563408	578575.937099	42.741952
3502.566227	578537.870835	42.746957
3503.017202	578514.328848	42.751962
3502.594542	578485.306263	42.756967
3502.855475	578456.226890	42.761972
3502.363795	578436.994807	42.766976
3502.410544	578409.654001	42.771981
3502.739116	578386.632414	42.776986
3502.439948	578360.148018	42.781991
3502.618137	578323.808980	42.786996
3502.200145	578309.881442	42.792001
3502.596386	578291.112142	42.797005
3502.710676	578261.302880	42.802010
3502.515814	578229.485552	42.807015
3502.820296	578213.639402	42.812020
3502.951956	578185.733080	42.817025
3502.828325	578146.682166	42.822029
3502.891433	578113.670628	42.827034
3502.698557	578084.861852	42.832039
3502.903899	578055.288580	42.837044
3502.676509	578026.585358	42.842049
3502.341132	577995.742276	42.847053
3502.288410	577970.171374	42.852058
3502.395290	577963.032611	42.857063
3502.570716	577933.965248	42.862068
3502.477736	577924.349935	42.867073
3502.660117	577895.331540	42.872077
3502.861794	577866.109430	42.877082
3502.530562	577858.387066	42.882087
3502.074238	577820.791384	42.887092
3501.883685	577790.827901	42.892097
3501.939319	577777.126590	42.897101
3502.501423	577754.669069	42.902106
3502.175172	577731.748505	42.907111
3502.359202	577714.265322	42.912116
3502.275424	577694.968191	42.917121
3502.495753	577676.425989	42.922125
3502.594598	577651.332230	42.927130
3502.266483	577626.907043	42.932135
3502.516278	577600.034084	42.937140
3502.829278	577590.706116	42.942145
3502.495737	577563.171908	42.947149
3502.468671	577528.166458	42.952154
3502.468827	577505.896604	42.957159
3502.869347	577477.695700	42.962164
3502.510573	577451.770200	42.967169
3502.561156	577418.507783	42.972173
3502.624888	577406.058694	42.977178
3502.462680	577383.964454	42.982183
3502.891974	577354.053374	42.987188
3502.388052	577327.899488	42.992193
3502.640965	577308.749688	42.997197
3502.552903	577280.574511	43.002202
3502.756926	577258.874195	43.007207
3503.024112	577231.245259	43.012212
3502.859184	577198.015878	43.017217
3502.529054	577168.022389	43.022221
3502.522004	577141.840551	43.027226
3502.647132	577110.421446	43.032231
3502.594353	577099.795958	43.037236
3502.462989	577079.702660	43.042241
3502.322295	577053.842464	43.047245
3502.022670	577018.677394	43.052250
3501.909913	577007.609760	43.057255
3502.049362	576976.338520	43.062260
3502.550196	576972.598556	43.067265
3502.448148	576948.838783	43.072269
3502.199645	576916.123229	43.077274
3502.189186	576888.035253	43.082279
3502.333816	576878.682857	43.087284
3503.076771	576863.568818	43.092289
3502.408468	576829.413834	43.097293
3502.383039	576789.389788	43.102298
3502.713553	576783.419166	43.107303
3502.886239	576745.872021	43.112308
3502.744214	576731.397761	43.117313
3502.396829	576707.124061	43.122317
3502.896122	576669.826568	43.127322
3502.454854	576657.957207	43.132327
3502.741949	576625.407881	43.137332
3502.570832	576602.811881	43.142337
3502.484831	576573.129764	43.147341
3502.435103	576555.530838	43.152346
3502.452163	576532.604309	43.157351
3502.609875	576500.576465	43.162356
3502.478257	576478.375333	43.167361
3502.573155	576460.302191	43.172365
3502.781397	576432.780831	43.177370
3502.514902	576402.022913	43.182375
3502.642858	576375.416883	43.187380
3502.087022	576357.997092	43.192385
3502.644784	576337.242946	43.197389
3502.610481	576313.220424	43.202394
3502.306984	576289.290096	43.207399
3502.834706	576260.564628	43.212404
3502.735813	576236.602202	43.217409
3502.397075	576209.868088	43.222413
3502.730447	576182.477044	43.227418
3502.548144	576157.825205	43.232423
3502.702144	576133.221064	43.237428
3502.769810	576110.285763	43.242433
3502.638417	576071.931124	43.247437
3502.742494	576044.224444	43.252442
3502.479328	576021.641664	43.257447
3502.725368	575996.170049	43.262452
3502.228309	575972.871275	43.267457
3502.361049	575942.802149	43.272461
3502.127435	575932.655305	43.277466
3502.035592	575914.660644	43.282471
3502.359394	575894.193081	43.287476
3502.252683	575875.398050	43.292481
3502.261369	575856.133465	43.297485
3502.144695	575830.216531	43.302490
3502.099133	575819.990022	43.307495
3502.235086	575794.836150	43.312500
3502.350344	575775.303942	43.317505
3502.532165	575750.895278	43.322509
3502.253227	575733.682053	43.327514
3502.264466	575711.055751	43.332519
3502.275706	575684.065012	43.337524
3502.148940	575677.462979	43.342529
3502.391481	575646.773912	43.347533
3502.434301	575625.547139	43.352538
3502.538797	575607.471127	43.357543
3502.593800	575576.710856	43.362548
3502.546514	575559.461151	43.367553
3502.594129	575531.260375	43.372557
3502.599952	575495.039462	43.377562
3502.330837	575481.737285	43.382567
3503.115054	575448.655347	43.387572
3502.328833	575425.250143	43.392577
3502.637255	575392.794255	43.397581
3502.446385	575361.720668	43.402586
3502.299666	575354.017893	43.407591
3502.370205	575317.485291	43.412596
3502.105662	575293.295917	43.417601
3501.981656	575276.810280	43.422605
3502.478268	575267.552024	43.427610
3501.817246	575254.611848	43.432615
3502.285668	575224.086989	43.437620
3502.306985	575223.180630	43.442625
3502.315139	575191.021941	43.447629
3502.619438	575181.643176	43.452634
3502.470283	575151.766513	43.457639
3502.713973	575124.888600	43.462644
3502.564881	575102.737653	43.467649
3502.314858	575066.956706	43.472653
3502.385492	575047.681055	43.477658
3502.587264	575028.736049	43.482663
3502.676957	574997.517261	43.487668
3502.490642	574980.890426	43.492673
3502.522722	574958.460031	43.497677
3502.312340	574933.258045	43.502682
3502.628915	574904.562138	43.507687
3502.670462	574879.772168	43.512692
3502.195653	574860.832313	43.517697
3502.264424	574835.686806	43.522701
3502.291842	574825.197139	43.527706
3502.266834	574799.163166	43.532711
3502.420831	574771.947250	43.537716
3502.251226	574748.945934	43.542721
3502.174041	574731.298279	43.547725
3502.612109	574705.643224	43.552730
3502.295920	574691.394245	43.557735
3502.294787	574659.486343	43.562740
3502.065967	574655.458334	43.567745
3502.225186	574620.414713	43.572749
3502.172008	574590.521559	43.577754
3501.839611	574586.008014	43.582759
3502.189278	574565.283150	43.587764
3502.067720	574563.094644	43.592769
3502.411163	574532.135923	43.597773
3502.345213	574520.807671	43.602778
3501.997432	574497.331991	43.607783
3502.611766	574473.354658	43.612788
3502.355298	574461.805276	43.617793
3502.040639	574433.156684	43.622797
3502.186024	574413.567240	43.627802
3501.716215	574398.589340	43.632807
3502.229824	574374.527203	43.637812
3502.070899	574356.339857	43.642817
3502.270445	574335.738385	43.647821
3502.338588	574316.211019	43.652826
3502.085141	574299.493332	43.657831
3502.253524	574275.785984	43.662836
3502.231470	574265.654735	43.667841
3502.136657	574237.021448	43.672845
3501.877113	574221.157520	43.677850
3501.989136	574219.434149	43.682855
3502.593480	574185.774583	43.687860
3502.209448	574167.622124	43.692865
3502.221142	574139.724524	43.697869
3502.478627	574125.385146	43.702874
3502.183717	574106.967796	43.707879
3502.136029	574083.544686	43.712884
3502.406727	574068.952310	43.717889
3502.175083	574035.673851	43.722893
3502.508667	574008.729062	43.727898
3502.229364	573997.483811	43.732903
3502.263460	573976.255303	43.737908
3501.956058	573962.756625	43.742913
3501.997693	573950.006135	43.747917
3502.389156	573928.571151	43.752922
3502.193895	573915.004711	43.757927
3502.512870	573891.975444	43.762932
3502.062897	573867.862177	43.767937
3502.112068	573840.911278	43.772941
3502.256673	573831.606537	43.777946
3502.184326	573817.368507	43.782951
3502.235681	573797.391309	43.787956
3502.051757	573774.239726	43.792961
3502.458285	573761.933720	43.797965
3502.256416	573733.667114	43.802970
3502.187853	573724.947526	43.807975
3502.188903	573693.036558	43.812980
3502.058239	573677.653461	43.817985
3501.927893	573656.399886	43.822989
3502.479303	573641.361681	43.827994
3501.941909	573615.856656	43.832999
3502.202133	573587.316747	43.838004
3502.384563	573586.987168	43.843009
3502.100439	573555.722491	43.848013
3502.254190	573531.614476	43.853018
3502.104672	573514.678680	43.858023
3502.426545	573493.705330	43.863028
3501.997352	573469.036037	43.868033
3501.907714	573459.717435	43.873037
3502.178734	573430.523165	43.878042
3502.075682	573421.858911	43.883047
3502.546860	573398.905201	43.888052
3502.159633	573386.271298	43.893057
3502.102351	573354.117617	43.898061
3502.307116	573338.781974	43.903066
3502.159010	573328.619416	43.908071
3501.753400	573292.556119	43.913076
3502.266412	573283.644921	43.918081
3502.101081	573261.693610	43.923085
3502.391208	573240.524051	43.928090
3502.087362	573226.020411	43.933095
3502.208341	573210.747869	43.938100
3502.152364	573191.689559	43.943105
3502.290719	573172.199423	43.948109
3501.908391	573148.023869	43.953114
3501.961651	573132.962516	43.958119
3501.999182	573113.588396	43.963124
3501.806221	573094.551336	43.968129
3501.546781	573085.459680	43.973133
3501.828085	573071.466489	43.978138
3501.547205	573070.356316	43.983143
3501.914365	573055.647205	43.988148
3501.897566	573035.880028	43.993153
3501.683210	573026.480214	43.998157
3501.819340	573005.334291	44.003162
3501.971366	572994.271499	44.008167
3501.656781	572978.564964	44.013172
3501.564554	572960.465303	44.018177
3501.867298	572949.830503	44.023181
3501.724365	572947.645024	44.028186
3501.480570	572937.798139	44.033191
3501.976407	572916.997241	44.038196
3501.812309	572910.901201	44.043201
3501.881393	572886.002208	44.048205
3501.957013	572867.223847	44.053210
3501.596365	572865.122564	44.058215
3502.290597	572855.831458	44.063220
3502.132659	572845.268579	44.068225
3502.081878	572822.796731	44.073229
3502.235473	572800.744492	44.078234
3501.979892	572785.680782	44.083239
3502.442548	572753.594654	44.088244
3501.893927	572747.056854	44.093249
3502.310528	572722.454425	44.098253
3502.220460	572711.379026	44.103258
3501.935082	572698.327002	44.108263
3501.847718	572672.247711	44.113268
3502.139225	572659.657424	44.118273
3502.255954	572640.671547	44.123277
3502.013820	572614.415603	44.128282
3501.903065	572598.475960	44.133287
3502.010570	572571.763824	44.138292
3502.008119	572570.409356	44.143297
3501.731281	572545.513517	44.148301
3501.833768	572540.178471	44.153306
3501.668795	572531.473037	44.158311
3502.170291	572514.183077	44.163316
3502.135431	572506.109616	44.168321
3501.723584	572483.392465	44.173325
3502.062513	572457.095498	44.178330
3501.869980	572448.544848	44.183335
3502.107205	572428.486004	44.188340
3502.153222	572417.439224	44.193345
3502.132235	572401.685992	44.198349
3502.077026	572380.217560	44.203354
3502.002057	572367.734424	44.208359
3502.137979	572341.770008	44.213364
3501.906065	572327.354333	44.218369
3502.108817	572317.788363	44.223373
3501.731855	572295.968629	44.228378
3501.795997	572280.954628	44.233383
3501.769562	572269.116142	44.238388
3501.760409	572251.504171	44.243393
3501.829159	572233.378186	44.248397
3501.978966	572230.243550	44.253402
3502.134182	572208.440814	44.258407
3502.212409	572193.173591	44.263412
3502.166775	572178.728606	44.268417
3501.979683	572156.678198	44.273421
3502.266749	572141.629163	44.278426
3502.149535	572115.051449	44.283431
3502.267862	572098.974931	44.288436
3502.008866	572072.419282	44.293441
3501.988081	572063.239315	44.298445
3502.051420	572049.830941	44.303450
3502.002979	572032.274954	44.308455
3502.260822	572004.132900	44.313460
3502.037103	571988.159879	44.318465
3501.931770	571968.354506	44.323469
3502.023577	571951.228106	44.328474
3501.729550	571938.026014	44.333479
3502.085293	571923.467775	44.338484
3501.881535	571909.448625	44.343489
3501.959351	571894.130883	44.348493
3502.220290	571883.351080	44.353498
3502.096774	571866.760037	44.358503
3502.069866	571847.142922	44.363508
3501.973434	571815.643382	44.368513
3502.150528	571804.174056	44.373517
3501.973098	571774.142359	44.378522
3502.121649	571777.882829	44.383527
3501.857061	571753.786264	44.388532
3502.077906	571742.059122	44.393537
3501.693253	571732.132845	44.398541
3501.702101	571706.437763	44.403546
3501.776311	571692.224341	44.408551
3502.114727	571693.124903	44.413556
3501.646660	571672.924075	44.418561
3501.417913	571643.452071	44.423565
3501.993997	571641.003383	44.428570
3501.685401	571646.471413	44.433575
3502.064052	571613.140627	44.438580
3501.882486	571605.340379	44.443585
3501.566387	571603.131526	44.448589
3501.880788	571572.671126	44.453594
3501.796000	571563.249843	44.458599
3501.878414	571548.332388	44.463604
3502.154979	571535.090810	44.468609
3501.916766	571526.295688	44.473613
3502.358838	571507.457798	44.478618
3502.121065	571489.930573	44.483623
3502.287671	571472.390289	44.488628
3502.371668	571449.944845	44.493633
3502.065807	571427.259198	44.498637
3502.008260	571400.871227	44.503642
3501.753771	571391.476332	44.508647
3501.845670	571380.270821	44.513652
3501.929015	571359.130097	44.518657
3501.833147	571345.695600	44.523661
3502.021338	571332.969451	44.528666
3501.579690	571318.384545	44.533671
3501.492671	571309.063771	44.538676
3501.486015	571305.652234	44.543681
3501.760956	571289.550092	44.548685
3502.017312	571266.123829	44.553690
3501.965313	571269.644894	44.558695
3501.770743	571244.231496	44.563700
3501.861668	571237.592839	44.568705
3501.676952	571209.919494	44.573709
3501.805502	571208.293459	44.578714
3501.635053	571200.942862	44.583719
3501.880996	571187.003076	44.588724
3502.133420	571188.017495	44.593729
3501.586684	571166.372691	44.598733
3501.925306	571153.773381	44.603738
3501.895198	571137.066303	44.608743
3502.175576	571109.219634	44.613748
3502.213543	571094.208163	44.618753
3502.192680	571071.226325	44.623757
3502.024844	571061.265566	44.628762
3501.810659	571034.951423	44.633767
3501.728147	571015.743059	44.638772
3502.078753	571016.691959	44.643777
3501.461550	570997.266036	44.648781
3501.887644	570970.249414	44.653786
3502.034233	570975.295299	44.658791
3501.768575	570958.574597	44.663796
3501.617119	570933.304325	44.668801
3501.518239	570930.258398	44.673805
3502.067863	570923.146358	44.678810
3501.853009	570910.382375	44.683815
3502.040687	570890.830443	44.688820
3502.292975	570872.924538	44.693825
3501.978764	570853.852498	44.698829
3501.928630	570836.194561	44.703834
3501.923723	570824.050089	44.708839
3502.023531	570799.643606	44.713844
3501.799580	570790.243440	44.718849
3501.714237	570779.315984	44.723853
3501.984949	570756.839990	44.728858
3501.446109	570763.900236	44.733863
3501.813869	570729.665210	44.738868
3501.473983	570718.325803	44.743873
3501.530822	570717.915407	44.748877
3501.850849	570697.137956	44.753882
3501.723400	570686.668682	44.758887
3501.811123	570675.965010	44.763892
3501.931815	570676.096693	44.768897
3501.735383	570656.152720	44.773901
3501.828155	570644.946353	44.778906
3501.897681	570622.652110	44.783911
3501.739141	570606.315648	44.788916
3501.931679	570594.491381	44.793921
3501.521953	570591.092454	44.798925
3501.554660	570576.131314	44.803930
3501.480097	570558.476767	44.808935
3502.093762	570543.675703	44.813940
3502.087946	570546.436948	44.818945
3501.969500	570531.047685	44.823949
3502.024865	570509.156941	44.828954
3502.036014	570496.306974	44.833959
3502.260371	570470.575422	44.838964
3501.800968	570465.327250	44.843969
3501.405082	570442.101644	44.848973
3501.760237	570427.842730	44.853978
3501.538797	570431.741862	44.858983
3502.036892	570417.761722	44.863988
3501.799972	570402.892694	44.868993
3501.551331	570393.144739	44.873997
3502.006252	570378.267902	44.879002
3501.658932	570360.856446	44.884007
3502.150448	570346.074223	44.889012
3501.965827	570331.297305	44.894017
3501.465967	570322.341399	44.899021
3502.164319	570298.693493	44.904026
3501.777371	570301.213245	44.909031
3501.951263	570274.334789	44.914036
3501.400162	570254.445561	44.919041
3501.697638	570256.958705	44.924045
3501.962666	570231.019499	44.929050
3501.760935	570230.398560	44.934055
3501.753646	570207.312485	44.939060
3501.780350	570194.760886	44.944065
3501.800346	570179.048369	44.949069
3502.355111	570170.379181	44.954074
3501.676120	570155.880080	44.959079
3501.896023	570131.202449	44.964084
3502.151018	570123.583888	44.969089
3501.952002	570097.465975	44.974093
3501.942515	570079.649946	44.979098
3501.872012	570085.282255	44.984103
3501.929245	570049.186516	44.989108
3502.051116	570046.959079	44.994113
3502.385394	570029.089230	44.999117
3502.373533	570005.551750	45.004122
3502.058629	569981.760452	45.009127
3502.342408	569961.940960	45.014132
3502.471252	569954.492581	45.019137
3501.909830	569934.303264	45.024141
3502.301153	569914.015159	45.029146
3502.347397	569902.514195	45.034151
3502.031173	569882.236263	45.039156
3501.866135	569856.212870	45.044161
3501.953494	569849.724540	45.049165
3502.204273	569820.875546	45.054170
3502.144204	569807.383454	45.059175
3502.530866	569783.331494	45.064180
3502.118587	569771.952271	45.069185
3501.860145	569748.653578	45.074189
3502.062876	569730.402297	45.079194
3502.005968	569721.928779	45.084199
3502.045421	569695.220560	45.089204
3501.591808	569677.523528	45.094209
3501.801584	569669.610585	45.099213
3501.960652	569647.952944	45.104218
3502.019285	569640.465145	45.109223
3501.763591	569626.501501	45.114228
3501.622039	569603.234430	45.119233
3501.910569	569597.467393	45.124237
3501.767575	569580.574921	45.129242
3501.514389	569565.958310	45.134247
3501.250441	569545.822187	45.139252
3502.043200	569547.103633	45.144257
3501.707942	569545.700450	45.149261
3502.056397	569515.179066	45.154266
3501.426512	569513.269818	45.159271
3501.843463	569499.301249	45.164276
3502.231024	569489.151908	45.169281
3501.991952	569476.841844	45.174285
3501.759745	569465.634937	45.179290
3501.673793	569432.370443	45.184295
3502.198119	569423.504682	45.189300
3502.128367	569420.654571	45.194305
3501.743251	569401.189646	45.199309
3501.836565	569381.047576	45.204314
3501.765312	569372.475657	45.209319
3501.745308	569350.393710	45.214324
3502.097834	569339.647395	45.219329
3501.610705	569321.804472	45.224333
3501.559656	569302.487929	45.229338
3501.606802	569293.546086	45.234343
3501.659431	569288.468290	45.239348
3501.855955	569277.394949	45.244353
3501.375634	569255.535363	45.249357
3501.837501	569246.829813	45.254362
3501.258393	569253.294947	45.259367
3501.663405	569238.775798	45.264372
3501.658996	569216.038635	45.269377
3501.804421	569211.197268	45.274381
3501.663204	569199.473935	45.279386
3501.653578	569189.787977	45.284391
3501.801381	569163.613717	45.289396
3501.801768	569163.563451	45.294401
3501.586891	569162.191594	45.299405
3501.766481	569142.236394	45.304410
3502.306056	569124.684408	45.309415
3502.243467	569108.381003	45.314420
3501.901067	569092.472680	45.319425
3501.836181	569077.273869	45.324429
3502.118115	569057.653886	45.329434
3501.876414	569048.857398	45.334439
3501.891971	569037.661533	45.339444
3501.847634	569012.771836	45.344449
3501.576503	568997.404383	45.349453
3501.816004	568997.216345	45.354458
3501.686100	568975.953978	45.359463
3501.819332	568950.132876	45.364468
3501.774142	568952.248124	45.369473
3501.459494	568941.906909	45.374477
3502.137722	568913.139400	45.379482
3501.737755	568910.290589	45.384487
3501.788077	568898.486811	45.389492
3502.135321	568890.451452	45.394497
3501.527767	568875.287014	45.399501
3501.907852	568864.385362	45.404506
3501.737811	568847.496039	45.409511
3501.753798	568819.735346	45.414516
3501.872853	568813.542652	45.419521
3501.664873	568807.099905	45.424525
3502.003816	568777.280791	45.429530
3501.867980	568773.989087	45.434535
3501.773380	568747.550601	45.439540
3501.982045	568736.625431	45.444545
3501.651307	568733.163400	45.449549
3502.266818	568725.136184	45.454554
3501.877793	568704.767158	45.459559
3501.581580	568690.708315	45.464564
3501.794525	568663.368221	45.469569
3501.809798	568658.848148	45.474573
3501.899733	568646.335169	45.479578
3501.984519	568641.503043	45.484583
3501.692257	568620.415989	45.489588
3501.599580	568607.580140	45.494593
3501.813207	568599.816451	45.499597
3501.778097	568573.920429	45.504602
3501.613938	568575.803360	45.509607
3501.470495	568573.767706	45.514612
3502.035993	568556.712772	45.519617
3501.698118	568530.010637	45.524621
3501.653021	568538.049185	45.529626
3501.827214	568521.908720	45.534631
3501.504075	568498.015237	45.539636
3501.709489	568497.079566	45.544641
3501.729331	568490.400237	45.549645
3501.649289	568471.488407	45.554650
3501.996833	568455.872919	45.559655
3501.795674	568437.532137	45.564660
3501.819954	568430.701488	45.569665
3501.640278	568410.399606	45.574669
3502.008901	568404.970837	45.579674
3501.777586	568395.469459	45.584679
3501.929458	568375.115684	45.589684
3501.946881	568372.402277	45.594689
3501.610434	568365.527586	45.599693
3501.993684	568343.932841	45.604698
3501.625327	568333.699869	45.609703
3501.581531	568311.218064	45.614708
3501.953264	568296.953924	45.619713
3501.785581	568286.689538	45.624717
3501.736869	568276.657535	45.629722
3501.929462	568249.018452	45.634727
3502.068688	568238.254260	45.639732
3501.706442	568223.652989	45.644737
3501.602200	568213.880603	45.649741
3501.870687	568201.088236	45.654746
3501.571756	568187.229996	45.659751
3501.656138	568180.590596	45.664756
3501.983683	568166.584195	45.669761
3501.935713	568165.537513	45.674765
3502.090616	568133.888163	45.679770
3501.966935	568122.863772	45.684775
3502.183914	568100.541585	45.689780
3501.863450	568081.767098	45.694785
3501.663534	568075.774469	45.699789
3501.419787	568060.602277	45.704794
3501.865738	568051.446528	45.709799
3502.017026	568027.026108	45.714804
3502.146195	568030.268847	45.719809
3501.653422	568005.396877	45.724813
3502.006772	567990.382244	45.729818
3501.787380	567975.356730	45.734823
3501.942562	567938.787262	45.739828
3501.263559	567885.932778	45.744833
3501.587241	567785.432015	45.749837
3501.126277	567635.002906	45.754842
3500.973606	567426.339953	45.759847
3500.504632	567182.881980	45.764852
3500.152826	566885.682298	45.769857
3499.940867	566543.469004	45.774861
3499.163266	566157.402762	45.779866
3498.762032	565737.474171	45.784871
3498.404215	565256.015109	45.789876
3497.448262	564724.165222	45.794881
3496.733504	564160.968898	45.799885
3496.033676	563548.729906	45.804890
3494.910150	562909.757202	45.809895
3493.628840	562199.908065	45.814900
3492.671382	561481.828553	45.819905
3491.359419	560698.109322	45.824909
3490.206230	559890.853893	45.829914
3488.570827	559044.835310	45.834919
3487.663738	558165.031043	45.839924
3486.364667	557236.987552	45.844929
3484.986425	556266.674800	45.849933
3483.593515	555260.304110	45.854938
3482.002587	554227.796166	45.859943
3480.115536	553147.295721	45.864948
3478.372770	552040.838890	45.869953
3475.994164	550898.536819	45.874957
3474.614537	549722.738591	45.879962
3472.539885	548530.041344	45.884967
3470.236260	547292.056411	45.889972
3468.099148	546031.641834	45.894977
3465.930716	544749.325196	45.899981
3463.809467	543431.154299	45.904986
3461.720476	542093.017931	45.909991
3459.725541	540710.750397	45.914996
3457.128370	539316.298490	45.920001
3454.589464	537896.119031	45.925005
3452.286780	536454.504724	45.930010
3449.543501	534985.363632	45.935015
3446.729572	533501.516742	45.940020
3444.565862	531988.045002	45.945025
3441.510620	530475.089942	45.950029
3439.199452	528913.095215	45.955034
3436.204643	527348.402263	45.960039
3433.536727	525768.411416	45.965044
3430.411903	524170.973825	45.970049
3427.142082	522553.214037	45.975053
3424.141020	520918.689175	45.980058
3421.316479	519291.397111	45.985063
3418.264530	517628.966476	45.990068
3415.362826	515952.195509	45.995073
3412.418773	514282.637181	46.000077
3409.234340	512581.250615	46.005082
3406.025889	510869.624560	46.010087
3402.698551	509159.623101	46.015092
3400.160757	507426.189358	46.020097
3396.185862	505684.545548	46.025101
3392.927838	503954.079639	46.030106
3389.535098	502188.913230	46.035111
3386.136989	500427.669857	46.040116
3382.704637	498651.380356	46.045121
3379.282905	496883.656344	46.050125
3376.036697	495084.999862	46.055130
3372.257714	493302.415218	46.060135
3368.702855	491501.556470	46.065140
3365.504261	489704.920923	46.070145
3361.856458	487901.122219	46.075149
3358.463823	486093.635553	46.080154
3354.772897	484289.266588	46.085159
3351.729009	482474.127713	46.090164
3347.841822	480663.406521	46.095169
3343.827874	478830.968316	46.100173
3340.389440	477009.599698	46.105178
3336.486043	475194.414072	46.110183
3333.248236	473367.848220	46.115188
3329.376573	471546.231184	46.120193
3325.802828	469713.796233	46.125197
3322.177187	467878.130924	46.130202
3318.515536	466044.948305	46.135207
3314.848960	464216.572652	46.140212
3311.079432	462373.799708	46.145217
3307.318812	460545.648522	46.150221
3303.838096	458709.516755	46.155226
3299.514453	456872.309142	46.160231
3296.054123	455045.450528	46.165236
3292.172321	453219.935102	46.170241
3287.907745	451382.901770	46.175245
3284.651189	449557.721593	46.180250
3280.738943	447750.127812	46.185255
3276.604775	445910.843641	46.190260
3273.331719	444094.786571	46.195265
3269.259683	442277.156108	46.200269
3265.539072	440454.785171	46.205274
3261.459914	438644.855137	46.210279
3258.056055	436829.732392	46.215284
3254.094276	435022.427566	46.220289
3250.363072	433208.076778	46.225293
3246.836635	431397.324834	46.230298
3242.849694	429591.291827	46.235303
3238.860656	427788.793874	46.240308
3235.499009	425985.274626	46.245313
3231.472062	424193.660828	46.250317
3227.923471	422393.297420	46.255322
3223.502501	420598.337191	46.260327
3219.696300	418801.401208	46.265332
3215.808786	417006.148882	46.270337
3212.079345	415230.294094	46.275341
3208.207630	413439.554856	46.280346
3204.569437	411670.592139	46.285351
3200.705418	409894.469796	46.290356
3197.138133	408119.932665	46.295361
3193.025408	406345.186378	46.300365
3189.807954	404588.120198	46.305370
3185.487593	402824.087489	46.310375
3181.425003	401062.922741	46.315380
3177.597642	399308.742190	46.320385
3174.071750	397564.888116	46.325389
3170.318469	395802.261935	46.330394
3166.036588	394063.394192	46.335399
3162.468939	392320.887673	46.340404
3158.877795	390582.879554	46.345409
3154.557203	388847.197810	46.350413
3151.132285	387108.868087	46.355418
3147.268590	385385.389753	46.360423
3143.693215	383654.030316	46.365428
3139.768513	381934.542927	46.370433
3135.618089	380219.192100	46.375437
3132.265759	378505.483417	46.380442
3128.419727	376802.509555	46.385447
3124.425237	375091.068995	46.390452
3120.987647	373389.085484	46.395457
3116.761630	371679.702182	46.400461
3112.806403	369971.314359	46.405466
3109.159643	368284.292543	46.410471
3105.079468	366604.225153	46.415476
3101.518065	364919.227122	46.420481
3097.680006	363248.023030	46.425485
3094.341029	361563.330675	46.430490
3089.873393	359881.692905	46.435495
3086.663774	358210.209875	46.440500
3082.713766	356556.516541	46.445505
3078.860451	354889.808145	46.450509
3075.448837	353221.569563	46.455514
3071.067681	351569.993824	46.460519
3067.344016	349919.603273	46.465524
3064.103357	348263.333816	46.470529
3060.001128	346623.717443	46.475533
3056.287948	344976.409020	46.480538
3052.494572	343335.643953	46.485543
3048.943867	341699.670199	46.490548
3045.481393	340057.096536	46.495553
3041.125818	338435.260305	46.500557
3037.547665	336799.903932	46.505562
3033.788102	335175.997642	46.510567
3030.180398	333553.980152	46.515572
3026.015390	331934.726672	46.520577
3022.482874	330322.808817	46.525581
3019.314099	328705.756235	46.530586
3015.218312	327100.050676	46.535591
3011.455357	325489.268255	46.540596
3007.835811	323890.279454	46.545601
3004.095340	322287.101003	46.550605
3000.235305	320678.766477	46.555610
2996.423571	319083.644340	46.560615
2992.339009	317490.643460	46.565620
2989.009043	315894.541153	46.570625
2985.602478	314319.563852	46.575629
2981.744041	312722.898277	46.580634
2977.761825	311145.205559	46.585639
2973.805898	309576.031887	46.590644
2970.451911	307993.149535	46.595649
2966.583241	306433.378627	46.600653
2962.872999	304857.908647	46.605658
2959.437459	303297.719093	46.610663
2955.367517	301728.776188	46.615668
2951.658525	300166.144469	46.620673
2947.909459	298615.131308	46.625677
2944.147582	297066.444009	46.630682
2940.712133	295519.114295	46.635687
2936.776036	293974.825246	46.640692
2933.447552	292429.586440	46.645697
2929.613189	290886.576614	46.650701
2926.050377	289341.576800	46.655706
2922.118565	287804.259710	46.660711
2918.191092	286261.941506	46.665716
2915.009435	284730.850834	46.670721
2911.067385	283193.709390	46.675725
2907.560855	281668.330238	46.680730
2903.588541	280141.667859	46.685735
2899.298442	278619.504816	46.690740
2895.822672	277096.623982	46.695745
2892.108562	275585.412169	46.700749
2888.530119	274069.975264	46.705754
2885.257778	272570.249503	46.710759
2881.640415	271056.470854	46.715764
2877.881193	269547.501165	46.720769
2873.794689	268053.403073	46.725773
2870.542516	266553.981947	46.730778
2866.736010	265054.930330	46.735783
2863.658941	263558.569275	46.740788
2859.853360	262059.754652	46.745793
2855.925694	260572.321787	46.750797
2852.532055	259078.445347	46.755802
2848.786473	257587.101096	46.760807
2845.030706	256091.971831	46.765812
2841.431285	254609.432535	46.770817
2837.739801	253127.783152	46.775821
2834.241789	251645.299037	46.780826
2830.469175	250167.198525	46.785831
2826.600353	248681.790585	46.790836
2822.755770	247204.592198	46.795841
2819.037476	245733.143489	46.800845
2815.600821	244263.524483	46.805850
2811.034974	242797.128176	46.810855
2808.020368	241334.605858	46.815860
2804.163849	239883.081772	46.820865
2800.681920	238433.427139	46.825869
2797.013694	236978.497364	46.830874
2793.754167	235535.391465	46.835879
2790.056982	234083.969509	46.840884
2786.538673	232633.864848	46.845889
2782.225580	231185.026769	46.850893
2778.910325	229746.268090	46.855898
2774.879458	228312.101579	46.860903
2771.550147	226874.843899	46.865908
2768.024769	225437.998072	46.870913
2764.389643	224009.675954	46.875917
2760.711789	222577.489816	46.880922
2757.262114	221146.135252	46.885927
2753.235083	219705.424031	46.890932
2749.421123	218283.605676	46.895937
2745.825187	216862.928207	46.900941
2742.279473	215435.803401	46.905946
2738.778389	214037.736232	46.910951
2734.984257	212611.730276	46.915956
2731.419404	211199.065658	46.920961
2727.627463	209788.149768	46.925965
2724.229595	208363.274121	46.930970
2720.381935	206971.203597	46.935975
2716.633987	205562.317330	46.940980
2713.506274	204168.318587	46.945985
2709.410178	202766.382638	46.950989
2705.972110	201365.398716	46.955994
2702.466912	199965.939294	46.960999
2698.945362	198567.207591	46.966004
2695.274698	197173.299681	46.971009
2691.601082	195775.916663	46.976013
2687.765685	194387.868134	46.981018
2684.109024	193002.963938	46.986023
2680.740061	191610.823102	46.991028
2677.546524	190230.130118	46.996033
2673.517477	188852.308875	47.001037
2670.119645	187452.378887	47.006042
2665.910464	186076.555803	47.011047
2662.465137	184696.404352	47.016052
2659.187239	183319.352152	47.021057
2655.563645	181945.225339	47.026061
2651.408813	180563.078954	47.031066
2648.073887	179194.625857	47.036071
2644.235243	177820.441817	47.041076
2640.744073	176465.232459	47.046081
2636.948333	175101.983240	47.051085
2633.675320	173725.817341	47.056090
2629.756205	172373.505424	47.061095
2626.361257	171020.995141	47.066100
2622.829449	169656.717340	47.071105
2619.013534	168308.650279	47.076109
2615.404416	166959.557846	47.081114
2611.936619	165600.591558	47.086119
2608.107663	164253.966492	47.091124
2604.566456	162898.044415	47.096129
2600.627730	161565.581581	47.101133
2596.946318	160221.307354	47.106138
2593.406540	158883.874496	47.111143
2589.697566	157550.799018	47.116148
2586.259624	156207.070720	47.121153
2582.451243	154878.715797	47.126157
2578.879977	153545.034491	47.131162
2575.207001	152237.870889	47.136167
2571.739073	150905.292060	47.141172
2568.183269	149580.241965	47.146177
2564.324708	148254.190106	47.151181
2560.891544	146935.027255	47.156186
2557.400526	145583.318969	47.161191
2553.837087	144229.507247	47.166196
2550.443210	142906.879117	47.171201
2546.461763	141599.671994	47.176205
2543.137587	140281.162404	47.181210
2539.186420	138976.680533	47.186215
2535.779985	137668.103639	47.191220
2531.883154	136358.151697	47.196225
2528.456112	135061.610665	47.201229
2524.712516	133759.673331	47.206234
2520.972393	132458.345912	47.211239
2517.622193	131164.793835	47.216244
2513.909092	129864.862440	47.221249
2510.469404	128581.832648	47.226253
2506.838020	127294.076563	47.231258
2502.855853	125997.460859	47.236263
2499.148274	124721.892728	47.241268
2495.651740	123422.204899	47.246273
2491.787559	122158.697672	47.251277
2488.537307	120881.679579	47.256282
2484.787256	119609.753819	47.261287
2481.027212	118337.172123	47.266292
2477.759049	117065.204491	47.271297
2473.696753	115796.290525	47.276301
2470.831334	114527.639471	47.281306
2467.034396	113254.918327	47.286311
2463.083424	111995.082070	47.291316
2460.025987	110723.999883	47.296321
2455.809076	109465.972557	47.301325
2452.362507	108211.874369	47.306330
2449.094352	106951.958310	47.311335
2445.420957	105692.545821	47.316340
2441.612420	104442.086581	47.321345
2437.819685	103191.861925	47.326349
2434.572548	101937.798230	47.331354
2430.823282	100685.538477	47.336359
2427.218880	99438.604059	47.341364
2423.909331	98201.839076	47.346369
2420.050970	96965.347481	47.351373
2416.270377	95724.837934	47.356378
2412.588238	94487.056036	47.361383
2408.711118	93256.114203	47.366388
2405.429694	92024.594648	47.371393
2401.358940	90797.555688	47.376397
2398.102959	89567.923276	47.381402
2394.277656	88355.887477	47.386407
2390.695810	87127.524655	47.391412
2387.052020	85920.896263	47.396417
2382.976296	84706.902818	47.401421
2379.914937	83493.716265	47.406426
2376.517606	82284.546005	47.411431
2372.482275	81077.876864	47.416436
2368.626207	79873.987574	47.421441
2364.804066	78683.925456	47.426445
2361.335184	77489.769592	47.431450
2357.758262	76301.613358	47.436455
2353.996117	75109.118462	47.441460
2350.544353	73934.088465	47.446465
2346.891053	72763.509633	47.451469
2343.271496	71574.158945	47.456474
2339.323400	70392.772710	47.461479
2335.646827	69231.115008	47.466484
2332.502899	68061.433691	47.471489
2328.478022	66900.220579	47.476493
2324.891862	65734.199127	47.481498
2321.114521	64583.621089	47.486503
2317.465455	63430.631854	47.491508
2313.752631	62274.449819	47.496513
2309.979719	61131.575526	47.501517
2306.603425	59987.809931	47.506522
2302.862016	58853.336936	47.511527
2298.901614	57717.186985	47.516532
2295.324526	56581.157291	47.521537
2291.481770	55455.342761	47.526541
2288.062027	54334.704916	47.531546
2284.189260	53216.830062	47.536551
2280.699265	52108.756001	47.541556
2277.230396	50988.912984	47.546561
2273.122635	49885.741729	47.551565
2269.421601	48780.827880	47.556570
2265.421100	47690.120150	47.561575
2261.761718	46603.635213	47.566580
2258.168622	45504.317571	47.571585
2253.924160	44439.825845	47.576589
2250.503916	43359.059685	47.581594
2246.862109	42301.348291	47.586599
2243.113696	41240.844402	47.591604
2239.154323	40182.231689	47.596609
2235.214864	39148.527172	47.601613
2231.626243	38104.685678	47.606618
2227.809266	37072.848802	47.611623
2223.546925	36042.639878	47.616628
2220.029136	35024.408252	47.621633
2215.724156	34015.336844	47.626637
2211.692432	33021.742924	47.631642
2207.281093	32052.131061	47.636647
2202.910132	31084.712671	47.641652
2198.346734	30136.420011	47.646657
2193.624891	29217.682847	47.651661
2188.777700	28319.930985	47.656666
2183.763142	27432.807901	47.661671
2178.836732	26582.302560	47.666676
2174.203937	25747.640015	47.671681
2169.268625	24955.738102	47.676685
2164.822258	24166.154015	47.681690
2160.453726	23415.545507	47.686695
2156.016275	22666.591431	47.691700
2152.010070	21947.340809	47.696705
2147.236639	21237.301332	47.701709
2143.377840	20556.593539	47.706714
2139.128383	19904.430538	47.711719
2135.370470	19235.749880	47.716724
2131.468960	18598.112686	47.721729
2127.480935	17981.708796	47.726733
2124.063153	17365.349210	47.731738
2120.145723	16762.206844	47.736743
2116.170751	16159.592604	47.741748
2112.475100	15579.042743	47.746753
2108.879635	15004.767311	47.751757
2104.990814	14434.237354	47.756762
2101.156214	13880.534706	47.761767
2097.597947	13338.798062	47.766772
2093.947759	12793.611790	47.771777
2090.602465	12272.926160	47.776781
2087.464020	11729.532993	47.781786
2083.649958	11205.179626	47.786791
2079.491312	10676.744614	47.791796
2076.457516	10163.795847	47.796801
2072.497931	9648.312158	47.801805
2069.002234	9137.502367	47.806810
2065.326440	8637.313199	47.811815
2061.399716	8150.499164	47.816820
2057.980472	7669.844332	47.821825
2053.636048	7193.860118	47.826829
2049.125527	6738.239663	47.831834
2044.397023	6301.616037	47.836839
2039.754150	5886.105152	47.841844
2035.573735	5474.999969	47.846849
2031.305747	5092.096165	47.851853
2027.001405	4719.775947	47.856858
2022.515104	4359.767169	47.861863
2018.068696	4021.002626	47.866868
2014.395132	3692.294024	47.871873
2010.320067	3374.476443	47.876877
2006.631853	3064.979927	47.881882
2002.752173	2772.947589	47.886887
1998.768320	2485.632012	47.891892
1995.024143	2199.375157	47.896897
1990.936747	1945.102791	47.901901
1987.375576	1676.453102	47.906906
1983.991846	1416.028356	47.911911
1980.040762	1189.832703	47.916916
1976.746139	933.580689	47.921921
1972.687567	706.781497	47.926925
1969.138385	469.325430	47.931930
1964.805700	269.357029	47.936935
1958.981146	118.688878	47.941940
1946.959978	148.228144	47.946945
1938.752801	162.455646	47.951949
1934.036311	147.912373	47.956954
1930.588960	149.761640	47.961959
1928.686928	151.407056	47.966964
1927.253019	151.935155	47.971969
1925.024021	150.157851	47.976973
1923.015916	143.040237	47.981978
1919.969742	150.806368	47.986983
1916.653471	143.102506	47.991988
1913.415117	140.556152	47.996993
1909.712588	143.549532	48.001997
1906.135977	139.186289	48.007002
1902.981456	148.339316	48.012007
1899.749916	145.560939	48.017012
1896.631724	141.926412	48.022017
1893.123969	144.734290	48.027021
1890.233669	140.867946	48.032026
1886.966360	148.618067	48.037031
1883.261419	146.132081	48.042036
1880.083009	145.376575	48.047041
1876.376315	144.479109	48.052045
1873.126520	143.146304	48.057050
1869.348112	136.748675	48.062055
1866.233739	147.138810	48.067060
1863.638889	144.618323	48.072065
1859.723264	148.385403	48.077069
1855.862196	146.521824	48.082074
1852.617245	139.167503	48.087079
1849.317194	142.673736	48.092084
1845.826495	135.873580	48.097089
1842.530677	142.802412	48.102093
1839.119996	142.643265	48.107098
1836.231999	149.505117	48.112103
1832.439206	150.304297	48.117108
1828.994781	140.579855	48.122113
1825.076302	145.736313	48.127117
1821.952063	146.921265	48.132122
1818.596709	145.718895	48.137127
1814.862244	145.059920	48.142132
1812.012594	141.604863	48.147137
1808.252206	143.316490	48.152141
1804.713349	139.981949	48.157146
1801.024743	139.739755	48.162151
1797.571386	149.354033	48.167156
1793.980857	137.342878	48.172161
1790.988099	132.812378	48.177165
1787.398670	131.798515	48.182170
1784.271191	135.840918	48.187175
1780.176044	141.176902	48.192180
1777.323903	135.444293	48.197185
1773.665116	143.527793	48.202189
1770.218607	136.897926	48.207194
1766.733596	136.940265	48.212199
1762.916746	139.552942	48.217204
1759.689736	139.412534	48.222209
1756.195676	149.264151	48.227213
1752.950886	145.133780	48.232218
1749.116138	149.910156	48.237223
1745.529312	149.459060	48.242228
1742.245952	145.885234	48.247233
1738.880222	135.170895	48.252237
1735.477212	146.406676	48.257242
1731.531353	134.232858	48.262247
1728.795975	140.884179	48.267252
1725.516699	138.312653	48.272257
1721.553961	141.264559	48.277261
1717.562164	133.786724	48.282266
1714.484011	143.683992	48.287271
1711.210106	146.379398	48.292276
1707.590078	134.578549	48.297281
1703.571244	146.284048	48.302285
1701.124467	132.078581	48.307290
1697.563848	134.882137	48.312295
1693.700878	141.988356	48.317300
1690.457772	134.722397	48.322305
1686.909822	138.042842	48.327309
1683.152984	138.918707	48.332314
1679.694359	142.687092	48.337319
1675.628965	147.942525	48.342324
1672.422610	125.626850	48.347329
1669.129062	136.541782	48.352333
1666.006068	134.319149	48.357338
1662.476598	137.804391	48.362343
1658.945852	144.823825	48.367348
1655.657305	136.663300	48.372353
1651.999058	131.547289	48.377357
1648.515645	128.919154	48.382362
1644.961549	129.991096	48.387367
1641.627694	150.264605	48.392372
1638.094121	133.416616	48.397377
1634.076873	142.059306	48.402381
1630.770068	130.177835	48.407386
1627.049635	121.183236	48.412391
1623.351667	126.991792	48.417396
1620.115793	135.546992	48.422401
1616.627641	134.836884	48.427405
1613.898579	130.167093	48.432410
1610.225674	133.393221	48.437415
1606.379331	134.264139	48.442420
1603.493532	135.437146	48.447425
1599.168691	139.641694	48.452429
1596.107705	142.477818	48.457434
1592.864706	138.068808	48.462439
1588.812805	146.530273	48.467444
1585.180115	133.263450	48.472449
1581.995781	130.613839	48.477453
1578.370147	128.520528	48.482458
1575.204950	131.847540	48.487463
1571.656999	136.974561	48.492468
1568.397218	135.380823	48.497473
1564.603449	134.130097	48.502477
1561.226506	136.098176	48.507482
1557.517212	131.518550	48.512487
1553.987339	132.615206	48.517492
1550.810653	131.609594	48.522497
1546.908927	130.628878	48.527501
1543.334860	124.639179	48.532506
1539.865147	126.349695	48.537511
1536.330528	139.273450	48.542516
1533.036051	132.214913	48.547521
1529.652268	132.497758	48.552525
1526.176093	124.714678	48.557530
1523.199409	122.133828	48.562535
1519.269370	129.620762	48.567540
1515.680877	125.819529	48.572545
1511.671905	128.728124	48.577549
1508.874494	127.577737	48.582554
1505.090714	124.518934	48.587559
1501.306066	136.716187	48.592564
1498.058302	125.841120	48.597569
1494.414164	120.128170	48.602573
1491.142760	126.107286	48.607578
1487.657981	126.481884	48.612583
1484.236225	129.111911	48.617588
1480.822751	126.944299	48.622593
1477.139941	124.958054	48.627597
1473.662887	124.600607	48.632602
1470.135829	128.563267	48.637607
1466.605682	123.721517	48.642612
1463.255467	119.044598	48.647617
1459.482883	135.413043	48.652621
1456.035665	129.925551	48.657626
1452.717252	119.384275	48.662631
1448.966922	129.605111	48.667636
1445.746621	120.269712	48.672641
1442.228270	126.765231	48.677645
1438.947847	128.718240	48.682650
1435.232255	128.217807	48.687655
1431.232769	123.933601	48.692660
1427.989255	130.949264	48.697665
1424.703080	128.034068	48.702669
1421.192248	127.121932	48.707674
1417.636390	123.619355	48.712679
1414.145414	133.714183	48.717684
1410.811862	124.614826	48.722689
1407.429930	132.136226	48.727693
1403.676207	119.742676	48.732698
1400.415968	119.664533	48.737703
1396.981580	128.475489	48.742708
1393.204083	126.051674	48.747713
1389.463676	126.804848	48.752717
1385.609270	124.905613	48.757722
1382.557620	128.819193	48.762727
1379.088672	129.703888	48.767732
1376.160622	126.447908	48.772737
1372.386945	127.506859	48.777741
1368.739114	132.801440	48.782746
1365.169934	124.991856	48.787751
1361.477584	123.396299	48.792756
1358.304720	118.565105	48.797761
1354.512381	114.049188	48.802765
1351.078434	120.503046	48.807770
1348.029475	117.047701	48.812775
1343.754055	130.232995	48.817780
1340.715894	117.047244	48.822785
1337.052727	119.645503	48.827789
1334.075176	124.740253	48.832794
1330.570766	122.729302	48.837799
1326.531164	126.452697	48.842804
1323.080903	120.336140	48.847809
1319.565310	124.252759	48.852813
1315.684742	131.181514	48.857818
1312.054831	125.953638	48.862823
1308.901646	115.649156	48.867828
1306.186436	111.322153	48.872833
1302.075219	121.260994	48.877837
1298.607180	120.914853	48.882842
1295.271669	119.950007	48.887847
1291.462806	120.650659	48.892852
1288.066263	119.530852	48.897857
1284.496104	118.669183	48.902861
1281.272124	120.603913	48.907866
1277.787951	126.505663	48.912871
1274.070760	125.167133	48.917876
1270.716290	124.556446	48.922881
1267.393201	131.568791	48.927885
1263.923241	126.765155	48.932890
1260.345946	120.763424	48.937895
1256.596396	133.050162	48.942900
1253.367851	121.719767	48.947905
1249.595734	120.339225	48.952909
1245.842826	118.613986	48.957914
1242.499112	125.015785	48.962919
1238.744476	125.717459	48.967924
1235.746735	115.879063	48.972929
1232.171611	120.323894	48.977933
1228.645444	120.518397	48.982938
1225.625235	121.434137	48.987943
1221.760500	129.167214	48.992948
1218.096932	125.222825	48.997953
1214.462425	128.803749	49.002957
1211.058179	127.568114	49.007962
1207.754622	118.590702	49.012967
1203.990381	126.001162	49.017972
1200.597028	121.865778	49.022977
1197.101717	127.389640	49.027981
1193.494426	117.371436	49.032986
1190.490883	115.740878	49.037991
1186.571631	119.214526	49.042996
1183.508176	119.102484	49.048001
1179.977837	115.548550	49.053005
1175.707741	116.970035	49.058010
1172.464724	117.348024	49.063015
1168.875692	120.820601	49.068020
1165.971075	112.964016	49.073025
1162.198460	120.148004	49.078029
1159.001703	118.497084	49.083034
1155.066411	125.111750	49.088039
1151.362573	120.104328	49.093044
1147.740540	111.477367	49.098049
1144.743297	117.135240	49.103053
1141.314173	114.150779	49.108058
1137.827747	109.555424	49.113063
1133.714367	116.432097	49.118068
1130.482189	113.714204	49.123073
1126.853968	115.199735	49.128077
1123.177799	119.654094	49.133082
1120.311143	119.909900	49.138087
1116.801959	119.769586	49.143092
1113.367145	113.176127	49.148097
1109.575691	125.972506	49.153101
1105.828566	116.593178	49.158106
1102.510195	109.677770	49.163111
1098.960542	120.019147	49.168116
1095.694741	110.279726	49.173121
1092.384414	120.779791	49.178125
1088.626180	111.860964	49.183130
1085.031843	113.850576	49.188135
1081.415375	119.311183	49.193140
1078.191968	114.946758	49.198145
1074.811501	118.563885	49.203149
1071.050610	113.894468	49.208154
1067.577242	108.446035	49.213159
1063.810845	118.935253	49.218164
1060.414651	106.685224	49.223169
1057.289972	112.695270	49.228173
1053.333450	111.046282	49.233178
1050.351765	116.821968	49.238183
1046.332742	118.571199	49.243188
1043.104767	113.704459	49.248193
1039.400010	121.978866	49.253197
1036.012850	124.353681	49.258202
1032.484198	116.999816	49.263207
1028.562244	116.092083	49.268212
1025.453963	104.508847	49.273217
1022.225476	119.852546	49.278221
1018.479581	116.012883	49.283226
1015.002782	120.107028	49.288231
1011.416925	126.287376	49.293236
1008.070523	114.830011	49.298241
1004.465189	124.474608	49.303245
1001.180639	120.005887	49.308250
997.636648	110.544187	49.313255
993.925818	117.142744	49.318260
990.284577	113.001965	49.323265
987.163344	119.900521	49.328269
983.425087	120.178943	49.333274
980.174657	116.612899	49.338279
976.419060	120.832969	49.343284
973.020001	117.707821	49.348289
969.584394	121.067858	49.353293
966.062099	115.396168	49.358298
962.879653	104.280160	49.363303
958.432449	122.611495	49.368308
955.845575	122.443886	49.373313
952.096334	116.155994	49.378317
948.208981	126.676846	49.383322
944.814392	113.847639	49.388327
941.572506	114.681115	49.393332
937.952329	114.653161	49.398337
933.928674	118.554545	49.403341
930.764166	114.335980	49.408346
927.536839	117.926012	49.413351
923.983183	118.355889	49.418356
920.121569	114.211680	49.423361
916.821224	113.548351	49.428365
913.678498	109.345365	49.433370
910.405962	111.806678	49.438375
906.430018	118.228477	49.443380
903.139653	118.715211	49.448385
899.277661	115.273434	49.453389
896.279697	116.448386	49.458394
892.838970	104.714781	49.463399
888.865716	115.062433	49.468404
885.296811	105.626834	49.473409
881.849295	120.761248	49.478413
878.243159	115.903164	49.483418
874.942866	119.963389	49.488423
871.159455	114.493981	49.493428
868.002109	98.375291	49.498433
864.791211	107.277941	49.503437
860.817246	108.548787	49.508442
856.858805	102.160823	49.513447
853.846216	110.630622	49.518452
850.546381	112.862109	49.523457
846.659907	111.379415	49.528461
843.420910	109.194212	49.533466
840.340149	108.139017	49.538471
836.398369	109.256135	49.543476
832.713475	100.515779	49.548481
829.318206	111.057681	49.553485
825.819674	110.567790	49.558490
822.049161	107.412284	49.563495
818.826905	113.197228	49.568500
815.736043	111.169175	49.573505
812.109733	104.321092	49.578509
808.553671	112.391949	49.583514
805.048925	112.371280	49.588519
801.535998	112.709402	49.593524
797.847401	101.701202	49.598529
794.184370	102.281135	49.603533
790.617109	104.573502	49.608538
787.307662	104.689938	49.613543
783.462844	111.398133	49.618548
779.929847	108.553467	49.623553
776.843427	117.348066	49.628557
773.447381	114.146594	49.633562
769.798699	109.292058	49.638567
766.131888	112.017644	49.643572
763.080104	102.928236	49.648577
759.052690	109.373965	49.653581
755.799218	103.521064	49.658586
752.251103	101.583623	49.663591
748.660637	115.028839	49.668596
745.303380	96.277603	49.673601
741.941613	105.580402	49.678605
738.663112	105.413596	49.683610
734.855717	104.304549	49.688615
731.122889	106.847495	49.693620
727.878748	106.684803	49.698625
724.471211	106.218666	49.703629
720.714785	99.811788	49.708634
717.420807	102.709961	49.713639
713.571215	106.628465	49.718644
710.325399	100.287161	49.723649
706.700893	111.532556	49.728653
703.360566	108.929835	49.733658
699.707455	107.780822	49.738663
696.328475	107.917671	49.743668
692.350672	104.908581	49.748673
688.992411	106.848712	49.753677
685.632493	103.189197	49.758682
682.278364	109.557987	49.763687
678.747585	105.463320	49.768692
675.738460	103.381387	49.773697
672.078035	102.622677	49.778701
667.854030	103.407573	49.783706
664.828554	99.974104	49.788711
661.152406	97.968165	49.793716
657.891616	97.510709	49.798721
654.174403	95.156861	49.803725
650.404756	100.461262	49.808730
647.274038	103.248467	49.813735
643.565870	113.504064	49.818740
640.292092	102.858087	49.823745
636.780490	102.095067	49.828749
633.114919	102.760883	49.833754
630.011632	104.955334	49.838759
625.992716	105.625870	49.843764
622.386149	104.713211	49.848769
618.904726	107.403490	49.853773
615.469443	106.887956	49.858778
612.103735	100.986253	49.863783
608.620476	116.948911	49.868788
605.777415	103.935418	49.873793
601.886696	105.943151	49.878797
597.962531	105.175157	49.883802
594.635065	105.025562	49.888807
590.867783	107.877682	49.893812
587.890360	103.939999	49.898817
584.291501	109.847271	49.903821
580.314137	118.433444	49.908826
576.976111	107.778572	49.913831
573.628250	104.019137	49.918836
570.233953	102.595522	49.923841
566.757835	108.119740	49.928845
562.951368	109.427753	49.933850
559.711575	108.033727	49.938855
555.760549	111.762534	49.943860
552.469141	106.225708	49.948865
549.649544	107.192497	49.953869
545.890132	110.635030	49.958874
542.196551	103.050954	49.963879
538.468692	105.096481	49.968884
535.274337	104.271157	49.973889
531.564270	100.850046	49.978893
528.062283	107.507800	49.983898
524.828710	99.981400	49.988903
521.017561	107.554455	49.993908
517.085721	107.755816	49.998913
514.245481	106.789613	50.003917
510.545769	111.371263	50.008922
507.146431	91.503607	50.013927
503.617431	109.466631	50.018932
500.065207	106.147361	50.023937
496.889090	97.153471	50.028941
493.193596	111.134065	50.033946
489.770004	104.732109	50.038951
485.910294	110.946030	50.043956
482.592996	95.978890	50.048961
478.852702	99.184333	50.053965
475.092218	107.698604	50.058970
471.950385	100.512200	50.063975
468.599735	103.343403	50.068980
464.878085	101.569302	50.073985
461.806592	103.458268	50.078989
457.881136	97.565212	50.083994
454.553953	101.819609	50.088999
451.018851	109.833510	50.094004
447.677799	104.918278	50.099009
444.164221	97.182669	50.104013
440.240243	106.000973	50.109018
436.772012	99.501630	50.114023
433.567846	118.182597	50.119028
430.330793	105.930087	50.124033
426.495674	109.954005	50.129037
422.702806	96.383847	50.134042
419.362173	102.763259	50.139047
415.641328	104.690677	50.144052
412.533676	100.814587	50.149057
409.487394	100.719094	50.154061
405.533835	111.927537	50.159066
401.741842	110.515661	50.164071
398.424545	100.771963	50.169076
394.946811	100.601687	50.174081
391.189339	105.246212	50.179085
387.995564	98.843106	50.184090
384.680288	92.395761	50.189095
380.906727	109.226524	50.194100
377.664107	100.632246	50.199105
374.127196	102.815609	50.204109
370.402852	102.092346	50.209114
367.006821	99.599725	50.214119
363.134683	99.469096	50.219124
359.619252	99.776143	50.224129
356.349264	106.502017	50.229133
353.222035	99.041291	50.234138
349.904940	105.784037	50.239143
346.165525	114.029297	50.244148
342.463361	97.053402	50.249153
338.580938	107.741353	50.254157
334.985628	106.703661	50.259162
331.865090	105.215109	50.264167
328.397194	103.407645	50.269172
325.445054	106.030939	50.274177
321.336060	107.563614	50.279181
317.705762	105.914472	50.284186
314.483342	93.140874	50.289191
311.135128	102.729578	50.294196
307.453686	101.423814	50.299201
303.983129	94.871112	50.304205
300.323070	109.203717	50.309210
296.975484	98.933297	50.314215
293.350131	95.385127	50.319220
289.433961	93.587791	50.324225
286.161925	100.548125	50.329229
282.741859	107.885995	50.334234
279.589875	95.683513	50.339239
276.136055	97.192667	50.344244
272.637560	94.228915	50.349249
269.045004	91.843052	50.354253
265.403381	95.713332	50.359258
261.884113	94.363200	50.364263
258.120993	110.727288	50.369268
254.475999	94.084177	50.374273
251.238556	98.020861	50.379277
247.640350	107.942980	50.384282
244.391444	97.717238	50.389287
240.545149	99.256252	50.394292
237.066202	102.873268	50.399297
233.865627	94.772347	50.404301
230.225952	89.850208	50.409306
227.189670	87.478459	50.414311
222.723009	96.169881	50.419316
219.673223	99.599448	50.424321
216.220010	103.531982	50.429325
212.814193	102.208389	50.434330
209.465104	91.969887	50.439335
206.112671	93.466349	50.444340
202.527604	95.511787	50.449345
198.670292	102.095600	50.454349
195.044763	99.366918	50.459354
192.152746	96.004466	50.464359
188.535229	102.579190	50.469364
184.608322	107.414855	50.474369
181.358970	106.421106	50.479373
177.636525	96.870699	50.484378
174.454935	92.000207	50.489383
170.280164	101.794374	50.494388
167.135469	89.189008	50.499393
163.870495	94.730902	50.504397
160.132825	102.801943	50.509402
156.745845	102.867482	50.514407
153.458001	100.269413	50.519412
149.908500	95.513517	50.524417
146.395712	100.198895	50.529421
142.525735	100.488807	50.534426
139.139636	98.339575	50.539431
135.251298	98.777900	50.544436
132.290018	95.992636	50.549441
128.845211	101.240013	50.554445
125.449031	103.660853	50.559450
121.589578	97.675365	50.564455
117.861526	106.365015	50.569460
114.457040	100.064639	50.574465
111.197580	101.935714	50.579469
107.641549	103.869073	50.584474
104.624715	100.105425	50.589479
100.697436	97.743601	50.594484
97.453428	100.248178	50.599489
93.923032	105.205256	50.604493
89.497453	104.968468	50.609498
86.694407	95.685353	50.614503
82.976935	99.779560	50.619508
79.559328	96.531133	50.624513
76.559079	95.618619	50.629517
72.770218	106.396409	50.634522
69.422404	89.912491	50.639527
65.238307	102.767526	50.644532
62.063024	103.999004	50.649537
58.903301	110.850067	50.654541
54.807370	108.299551	50.659546
51.671794	98.587655	50.664551
47.993554	101.840495	50.669556
44.407319	103.750137	50.674561
41.422383	102.230956	50.679565
37.605636	100.329574	50.684570
34.471404	105.202456	50.689575
30.557506	100.585965	50.694580
27.281129	105.503267	50.699585
23.585935	97.973483	50.704589
19.594475	101.338685	50.709594
16.621269	96.410296	50.714599
13.240691	98.366822	50.719604
9.932730	99.786786	50.724609
6.125807	102.623205	50.729613
2.422316	97.511851	50.734618