Thu Aug 25 12:24:03 2022

Number of Points = 9926

Depth (nm)	Load (N)	Time (s)
1.632816	98.275455	0.000000
1.562110	91.617293	0.005005
1.335330	93.335950	0.010010
1.591362	89.594216	0.015014
1.396367	96.294002	0.020019
0.997995	85.365466	0.025024
0.719260	72.953367	0.030029
0.973171	68.098322	0.035034
0.731133	54.702881	0.040038
0.228931	42.566263	0.045043
-0.279194	29.424504	0.050048
-0.260477	20.015704	0.055053
-0.528126	21.212409	0.060058
-0.632964	7.200720	0.065062
-0.891543	6.538877	0.070067
-1.446695	0.912109	0.075072
-1.354404	-8.258267	0.080077
-1.979817	-7.464252	0.085082
-2.392653	-15.587370	0.090086
-2.509145	-11.215794	0.095091
-3.367865	-15.089729	0.100096
-3.497658	-19.890957	0.105101
-3.873655	-20.066166	0.110106
-3.958743	-19.375793	0.115110
-4.228355	-14.243072	0.120115
-4.288445	-22.633427	0.125120
-4.036219	-21.562472	0.130125
-4.831691	-20.172337	0.135130
-4.721548	-19.635941	0.140134
-5.340566	-13.616406	0.145139
-5.779355	-17.587773	0.150144
-6.199167	-18.167404	0.155149
-6.769768	-15.787446	0.160154
-6.431968	-28.207489	0.165158
-6.890004	-25.383261	0.170163
-6.984675	-20.521560	0.175168
-6.681305	-28.345601	0.180173
-7.351704	-22.805237	0.185178
-7.880739	-19.147307	0.190182
-8.599300	-12.814782	0.195187
-8.749689	-15.831590	0.200192
-8.619372	-25.871620	0.205197
-8.579948	-25.283014	0.210202
-8.773590	-22.984266	0.215206
-8.382621	-22.428595	0.220211
-9.326478	-26.918774	0.225216
-9.575824	-19.030436	0.230221
-10.203771	-28.967475	0.235226
-9.903603	-27.828103	0.240230
-10.117211	-18.581787	0.245235
-11.022942	-19.404822	0.250240
-11.240789	-22.243381	0.255245
-11.053900	-17.330882	0.260250
-11.323643	-23.268116	0.265254
-11.690673	-21.853361	0.270259
-12.117443	-29.483907	0.275264
-12.612780	-25.935662	0.280269
-13.210394	-19.188656	0.285274
-12.340017	-26.155576	0.290278
-12.872756	-23.417719	0.295283
-13.434061	-25.237517	0.300288
-13.162108	-30.228240	0.305293
-13.353331	-17.334461	0.310298
-13.597720	-27.489786	0.315302
-14.219335	-25.000595	0.320307
-14.514022	-17.886600	0.325312
-14.569394	-26.065720	0.330317
-14.920340	-20.176775	0.335322
-15.270770	-23.244496	0.340326
-15.907615	-23.059294	0.345331
-16.079416	-25.655130	0.350336
-16.024412	-21.528726	0.355341
-16.341456	-22.602186	0.360346
-15.990695	-24.346591	0.365350
-16.289119	-17.678100	0.370355
-16.807288	-26.493389	0.375360
-17.600755	-27.723154	0.380365
-17.809855	-8.198506	0.385370
-17.631785	-22.289298	0.390374
-18.048307	-26.185058	0.395379
-17.909160	-26.048675	0.400384
-17.816150	-26.177146	0.405389
-18.734291	-22.027980	0.410394
-18.689646	-21.819843	0.415398
-19.115310	-18.991194	0.420403
-19.386828	-17.929926	0.425408
-20.300237	-26.442841	0.430413
-20.560423	-23.836273	0.435418
-20.380580	-18.773976	0.440422
-20.742136	-25.487760	0.445427
-20.601649	-19.039900	0.450432
-20.515154	-24.776685	0.455437
-21.082705	-21.985917	0.460442
-21.492816	-19.409641	0.465446
-21.790562	-18.578381	0.470451
-22.182189	-10.768988	0.475456
-22.045648	-27.061570	0.480461
-22.170048	-11.349863	0.485466
-22.626948	-19.934308	0.490470
-23.267764	-22.469312	0.495475
-23.432387	-18.416063	0.500480
-23.569446	-11.870929	0.505485
-23.239154	-15.757155	0.510490
-23.568958	-22.346201	0.515494
-24.178092	-22.051446	0.520499
-24.370660	-18.012801	0.525504
-24.248474	-24.232905	0.530509
-25.180385	-10.903529	0.535514
-25.850061	-27.670901	0.540518
-25.947295	-21.733124	0.545523
-26.147080	-11.182342	0.550528
-25.990162	-17.471165	0.555533
-26.346640	-14.185121	0.560538
-26.429368	-20.338318	0.565542
-26.516830	-22.804999	0.570547
-26.462716	-19.260586	0.575552
-27.237382	-21.385475	0.580557
-27.666361	-11.890277	0.585562
-27.564538	-20.657177	0.590566
-27.717623	-28.105978	0.595571
-27.983891	-18.671079	0.600576
-28.349800	-16.006816	0.605581
-28.585545	-27.561872	0.610586
-28.913023	-27.004364	0.615590
-28.512140	-24.941138	0.620595
-29.673151	-22.664823	0.625600
-29.994457	-33.377566	0.630605
-30.612053	-17.829034	0.635610
-30.562242	-20.889864	0.640614
-30.808500	-16.982011	0.645619
-30.364265	-26.020859	0.650624
-30.694141	-15.519299	0.655629
-31.020524	-13.933742	0.660634
-31.516779	-27.298775	0.665638
-31.388402	-13.996329	0.670643
-31.745868	-21.137862	0.675648
-32.220722	-24.398057	0.680653
-33.313559	-21.132678	0.685658
-33.205558	-26.195788	0.690662
-33.261013	-25.203175	0.695667
-33.439862	-22.239193	0.700672
-33.498913	-27.333076	0.705677
-33.477022	-24.460658	0.710682
-33.236968	-25.466383	0.715686
-34.025502	-17.790955	0.720691
-34.534848	-26.806940	0.725696
-34.970953	-27.017022	0.730701
-35.418469	-20.894646	0.735706
-35.157810	-20.922836	0.740710
-35.336363	-28.399283	0.745715
-35.767255	-24.895936	0.750720
-36.196893	-20.684105	0.755725
-36.466834	-16.089171	0.760730
-36.446999	-22.812094	0.765734
-36.659386	-22.804128	0.770739
-36.880584	-17.381601	0.775744
-37.422909	-17.824976	0.780749
-37.989794	-11.554181	0.785754
-37.969674	-22.276133	0.790758
-37.935775	-17.289045	0.795763
-38.290179	-5.470679	0.800768
-37.939868	-20.316122	0.805773
-38.631803	-20.318439	0.810778
-39.071377	-21.711221	0.815782
-39.475698	-16.073339	0.820787
-39.610344	-20.756746	0.825792
-39.438870	-13.557604	0.830797
-39.896786	-19.383094	0.835802
-40.102867	-19.771586	0.840806
-40.767482	-21.496102	0.845811
-41.206034	-19.139996	0.850816
-41.132241	-17.908206	0.855821
-41.326155	-17.355806	0.860826
-41.356568	-22.748407	0.865830
-41.215995	-23.570865	0.870835
-42.434677	-19.529629	0.875840
-42.414708	-16.884700	0.880845
-42.926402	-12.163300	0.885850
-42.913947	-21.049074	0.890854
-42.930462	-27.035472	0.895859
-43.145680	-18.140083	0.900864
-43.462411	-23.604879	0.905869
-43.720799	-18.322058	0.910874
-43.844714	-29.897797	0.915878
-44.096913	-21.569253	0.920883
-44.269916	-21.494693	0.925888
-44.290823	-19.770338	0.930893
-45.260543	-12.658141	0.935898
-45.418292	-21.245163	0.940902
-45.718234	-28.797501	0.945907
-45.856328	-20.151479	0.950912
-45.668997	-23.474301	0.955917
-46.703010	-21.192573	0.960922
-46.958292	-30.463498	0.965926
-47.182469	-28.912938	0.970931
-47.408644	-14.368533	0.975936
-47.353354	-28.822893	0.980941
-47.389143	-11.040162	0.985946
-47.200488	-23.651971	0.990950
-47.556380	-16.961821	0.995955
-48.434799	-11.872912	1.000960
-48.476020	-14.710671	1.005965
-48.381081	-19.581911	1.010970
-48.734648	-23.104718	1.015974
-49.496022	-22.077426	1.020979
-50.168991	-15.166751	1.025984
-50.088071	-11.490496	1.030989
-50.379855	-9.644604	1.035994
-50.349245	-12.221535	1.040998
-50.319022	-17.234496	1.046003
-50.636090	-12.793528	1.051008
-50.701409	-16.905667	1.056013
-51.540222	-19.039485	1.061018
-51.575457	-19.283904	1.066022
-51.716386	-13.953047	1.071027
-51.783160	-16.653924	1.076032
-51.918832	-19.910317	1.081037
-52.925718	-12.276604	1.086042
-52.945570	-18.657951	1.091046
-52.885632	-15.424498	1.096051
-53.289672	-12.219585	1.101056
-53.443481	-16.036285	1.106061
-54.116884	-12.941027	1.111066
-54.550453	-14.492936	1.116070
-54.669005	-18.147481	1.121075
-54.866514	-15.731067	1.126080
-54.577111	-21.471171	1.131085
-55.046267	-11.599519	1.136090
-54.874251	-14.720626	1.141094
-55.132962	-21.608711	1.146099
-55.740956	-9.687338	1.151104
-55.975475	-9.274108	1.156109
-56.362718	-25.516254	1.161114
-56.262938	-8.381186	1.166118
-57.047277	-19.401032	1.171123
-57.369544	-16.104529	1.176128
-57.644458	-16.279755	1.181133
-57.843542	-14.989390	1.186138
-57.830374	-16.949819	1.191142
-58.187403	-14.799475	1.196147
-57.995054	-12.333416	1.201152
-57.897642	-10.595962	1.206157
-58.876343	-19.649136	1.211162
-58.901346	-18.082327	1.216166
-58.890126	-15.932736	1.221171
-59.677670	-8.741514	1.226176
-60.421390	-22.374656	1.231181
-60.744408	-19.919594	1.236186
-60.398486	-24.355595	1.241190
-60.322373	-20.071149	1.246195
-60.892189	-18.510723	1.251200
-60.491142	-22.262501	1.256205
-60.847820	-7.741936	1.261210
-61.545156	-17.763014	1.266214
-61.483683	-19.534859	1.271219
-62.235263	-11.222977	1.276224
-62.172240	-11.811822	1.281229
-63.289957	-15.407885	1.286234
-63.461875	-14.900059	1.291238
-63.196874	-15.337054	1.296243
-63.419266	-17.102386	1.301248
-63.586052	-21.932616	1.306253
-63.792204	-14.633177	1.311258
-63.891222	-21.365949	1.316262
-64.040815	-16.464006	1.321267
-64.460239	-13.497128	1.326272
-65.025819	-19.312074	1.331277
-65.202949	-21.653973	1.336282
-65.079140	-17.895855	1.341286
-65.166692	-16.936177	1.346291
-65.790270	-17.683194	1.351296
-66.348782	-23.492918	1.356301
-66.411555	-16.839206	1.361306
-66.476543	-23.314718	1.366310
-66.856707	-23.903722	1.371315
-66.875610	-10.119456	1.376320
-67.479007	-17.168668	1.381325
-68.153748	-13.225313	1.386330
-68.099621	-16.157105	1.391334
-68.169513	-19.461770	1.396339
-68.687877	-20.965590	1.401344
-68.480417	-23.045047	1.406349
-68.388014	-10.015376	1.411354
-68.486709	-13.321856	1.416358
-68.856060	-18.395592	1.421363
-69.568921	-16.581798	1.426368
-69.547377	-21.375098	1.431373
-70.199003	-17.821344	1.436378
-70.855855	-15.374084	1.441382
-70.890018	-12.185998	1.446387
-71.084974	-22.766680	1.451392
-70.982818	-18.536934	1.456397
-70.964175	-23.953038	1.461402
-70.940186	-15.006545	1.466406
-71.713868	-21.522872	1.471411
-72.057047	-11.044537	1.476416
-71.889708	-28.183495	1.481421
-72.745933	-15.435458	1.486426
-73.007636	-16.720067	1.491430
-73.320323	-20.325209	1.496435
-73.711661	-19.950681	1.501440
-73.736977	-19.038721	1.506445
-73.905510	-14.573571	1.511450
-73.737012	-23.755875	1.516454
-74.117201	-18.482443	1.521459
-75.031408	-19.307306	1.526464
-75.085079	-24.000235	1.531469
-75.244096	-20.150345	1.536474
-74.986121	-23.911343	1.541478
-75.266722	-22.513292	1.546483
-75.958642	-16.279854	1.551488
-76.059955	-25.046557	1.556493
-76.487761	-14.042436	1.561498
-76.793571	-15.756732	1.566502
-76.542197	-19.168683	1.571507
-76.981576	-15.850665	1.576512
-77.323018	-22.747931	1.581517
-78.123164	-20.180142	1.586522
-78.532897	-13.832731	1.591526
-78.556536	-20.770302	1.596531
-78.532290	-25.402673	1.601536
-78.049314	-19.634905	1.606541
-78.379212	-23.490449	1.611546
-78.997126	-15.563344	1.616550
-79.670484	-18.374817	1.621555
-80.354328	-15.841070	1.626560
-80.052962	-18.175687	1.631565
-79.916715	-18.753859	1.636570
-79.708784	-24.370465	1.641574
-80.186928	-28.092048	1.646579
-81.134867	-22.637907	1.651584
-81.176730	-28.028709	1.656589
-81.670440	-12.388857	1.661594
-81.786449	-16.812591	1.666598
-81.713495	-18.861482	1.671603
-81.656199	-14.646853	1.676608
-82.484833	-22.733280	1.681613
-82.693265	-9.976011	1.686618
-82.630276	-16.291244	1.691622
-82.639457	-22.807137	1.696627
-83.652960	-13.394358	1.701632
-83.765343	-30.635015	1.706637
-84.137540	-19.038498	1.711642
-84.166349	-22.270505	1.716646
-83.921075	-14.358432	1.721651
-84.398782	-20.003646	1.726656
-84.939266	-20.219516	1.731661
-85.511993	-14.833656	1.736666
-85.513270	-27.304967	1.741670
-85.495001	-21.056261	1.746675
-85.543035	-10.035715	1.751680
-85.658108	-23.178897	1.756685
-86.481382	-21.180122	1.761690
-86.884913	-18.209407	1.766694
-87.172952	-20.100493	1.771699
-87.204201	-10.101305	1.776704
-87.260360	-19.659696	1.781709
-87.356591	-17.382538	1.786714
-87.965447	-18.948108	1.791718
-88.252878	-18.412691	1.796723
-88.444094	-15.022827	1.801728
-88.756688	-18.975995	1.806733
-88.683381	-14.884098	1.811738
-89.528772	-21.085466	1.816742
-89.817583	-16.073125	1.821747
-90.294638	-16.782987	1.826752
-89.484225	-28.925902	1.831757
-89.958039	-13.422047	1.836762
-89.963655	-22.355605	1.841766
-90.061188	-15.544587	1.846771
-90.959583	-17.434947	1.851776
-91.630468	-20.610638	1.856781
-91.973919	-15.728939	1.861786
-91.671907	-22.815613	1.866790
-91.767746	-23.458659	1.871795
-91.771283	-19.848267	1.876800
-92.099051	-14.212889	1.881805
-93.202942	-24.556230	1.886810
-93.218956	-18.903265	1.891814
-93.207157	-20.698963	1.896819
-93.654981	-17.329002	1.901824
-93.308414	-21.246251	1.906829
-93.292047	-19.331585	1.911834
-94.036013	-20.433058	1.916838
-94.147166	-30.055592	1.921843
-94.781414	-19.550637	1.926848
-94.456332	-24.182690	1.931853
-95.493891	-23.703739	1.936858
-95.849142	-27.966596	1.941862
-96.080192	-20.476599	1.946867
-96.376071	-19.936694	1.951872
-95.826738	-22.142487	1.956877
-96.305049	-27.376316	1.961882
-96.274327	-28.690925	1.966886
-96.248520	-19.963020	1.971891
-97.138790	-14.277467	1.976896
-97.655530	-21.441491	1.981901
-97.719975	-14.635658	1.986906
-97.734287	-16.240604	1.991910
-98.171921	-20.598121	1.996915
-98.811112	-18.054558	2.006912
-98.229199	-10.318103	2.016909
-98.004423	-15.301439	2.026906
-96.898993	-12.012250	2.036902
-96.602398	-23.849292	2.046899
-96.496151	-24.600876	2.056896
-95.498646	-22.194433	2.066893
-95.320505	-26.090238	2.076890
-94.979858	-20.758358	2.086886
-94.227399	-28.212897	2.096883
-93.692745	-20.050892	2.106880
-92.815755	-22.497644	2.116877
-92.774375	-23.220057	2.126874
-92.399125	-22.338025	2.136870
-91.654595	-21.631064	2.146867
-91.209263	-23.908809	2.156864
-90.628126	-15.003315	2.166861
-89.557386	-23.077933	2.176858
-89.305751	-17.652909	2.186854
-89.476996	-17.635586	2.196851
-89.045041	-23.592221	2.206848
-88.687587	-23.980856	2.216845
-87.477987	-28.028779	2.226842
-86.890908	-26.483023	2.236838
-86.942789	-22.492972	2.246835
-86.005009	-25.962945	2.256832
-85.423688	-23.827075	2.266829
-85.289866	-18.396262	2.276826
-84.850733	-21.110191	2.286822
-83.872723	-26.547337	2.296819
-83.735256	-25.830785	2.306816
-83.622197	-21.752539	2.316813
-82.887502	-21.462186	2.326810
-81.794447	-19.406500	2.336806
-81.456209	-20.571403	2.346803
-81.144103	-21.358412	2.356800
-80.835036	-20.355135	2.366797
-79.968842	-23.820227	2.376794
-79.699586	-24.239391	2.386790
-79.040510	-25.340526	2.396787
-78.227931	-25.762462	2.406784
-77.944361	-24.143804	2.416781
-78.049720	-27.269761	2.426778
-77.396007	-28.141974	2.436774
-76.824671	-21.848382	2.446771
-75.746152	-22.812500	2.456768
-75.273533	-23.627827	2.466765
-75.203999	-16.112029	2.476762
-75.018639	-24.972913	2.486758
-74.218445	-16.887357	2.496755
-73.901598	-26.918756	2.506752
-72.878863	-18.129973	2.516749
-72.559463	-21.899026	2.526746
-72.649988	-19.965159	2.536742
-71.623749	-20.316035	2.546739
-71.217660	-15.415724	2.556736
-70.270175	-23.347484	2.566733
-70.098697	-24.590794	2.576730
-69.767093	-24.240449	2.586726
-68.998808	-20.049458	2.596723
-68.664810	-21.482960	2.606720
-68.337457	-13.054049	2.616717
-67.606749	-14.106219	2.626714
-67.159081	-17.942889	2.636710
-66.554146	-25.608731	2.646707
-65.912736	-25.810609	2.656704
-65.737386	-27.501186	2.666701
-65.344202	-26.355867	2.676698
-64.172536	-30.362998	2.686694
-64.290569	-30.458550	2.696691
-63.538839	-23.347420	2.706688
-62.602385	-29.297572	2.716685
-62.805900	-28.258328	2.726682
-62.491538	-31.139606	2.736678
-61.667729	-27.505346	2.746675
-61.340978	-33.074860	2.756672
-60.435499	-28.088074	2.766669
-60.018039	-24.010006	2.776666
-59.703152	-26.428868	2.786662
-58.785651	-26.385735	2.796659
-58.301558	-23.689766	2.806656
-58.358466	-24.672378	2.816653
-57.520733	-25.262978	2.826650
-57.143339	-36.035622	2.836646
-56.529298	-25.611573	2.846643
-55.616658	-24.823245	2.856640
-55.707648	-19.829207	2.866637
-55.413137	-31.447342	2.876634
-54.774113	-25.731391	2.886630
-53.991530	-26.855044	2.896627
-53.737933	-32.552480	2.906624
-52.846156	-23.248999	2.916621
-52.505651	-20.910666	2.926618
-52.489023	-18.860541	2.936614
-51.373591	-18.965630	2.946611
-51.164071	-19.274064	2.956608
-50.392371	-22.407568	2.966605
-49.911282	-23.740572	2.976602
-49.511749	-24.291022	2.986598
-49.426336	-24.709890	2.996595
-48.504038	-30.087618	3.006592
-48.264124	-26.631129	3.016589
-47.048893	-21.702377	3.026586
-46.715324	-38.284240	3.036582
-46.822182	-23.435855	3.046579
-46.298327	-27.506206	3.056576
-45.336486	-27.660088	3.066573
-45.347572	-29.368970	3.076570
-44.383710	-23.691244	3.086566
-43.518638	-23.510015	3.096563
-44.026552	-25.327952	3.106560
-43.346160	-23.137909	3.116557
-42.554082	-27.503711	3.126554
-42.368286	-23.880352	3.136550
-41.241583	-27.965967	3.146547
-40.965336	-24.242739	3.156544
-40.705236	-25.325707	3.166541
-39.713269	-29.276168	3.176538
-39.295210	-31.666845	3.186534
-39.094500	-29.984519	3.196531
-38.603239	-28.658162	3.206528
-37.818078	-24.726405	3.216525
-37.778269	-25.287014	3.226522
-37.072914	-29.442823	3.236518
-36.533941	-30.240034	3.246515
-36.117962	-24.596838	3.256512
-35.072112	-17.024937	3.266509
-34.860807	-19.582792	3.276506
-34.724961	-16.410936	3.286502
-34.386605	-24.510180	3.296499
-33.687724	-26.846656	3.306496
-32.919844	-21.340959	3.316493
-31.938432	-22.543282	3.326490
-31.706064	-24.755977	3.336486
-32.136265	-27.647305	3.346483
-31.508855	-22.566259	3.356480
-30.382120	-28.090060	3.366477
-29.598187	-26.353396	3.376474
-29.214637	-28.526423	3.386470
-28.801600	-21.900746	3.396467
-28.701257	-26.424258	3.406464
-28.403235	-25.035945	3.416461
-27.551074	-27.412277	3.426458
-27.102486	-28.398065	3.436454
-26.299130	-26.449034	3.446451
-26.118940	-20.588326	3.456448
-25.718849	-28.161882	3.466445
-25.073147	-26.381385	3.476442
-24.914031	-28.772671	3.486438
-23.502615	-28.791085	3.496435
-23.284044	-24.621663	3.506432
-23.269985	-32.869662	3.516429
-22.270566	-28.594506	3.526426
-21.854302	-30.965895	3.536422
-21.553638	-25.618241	3.546419
-21.187098	-22.263954	3.556416
-20.433592	-24.371403	3.566413
-20.336771	-17.338215	3.576410
-19.376020	-22.345000	3.586406
-18.947338	-17.796683	3.596403
-18.429254	-20.038307	3.606400
-17.680377	-20.586471	3.616397
-17.620861	-17.656080	3.626394
-17.204909	-14.664327	3.636390
-16.537964	-23.138172	3.646387
-16.189929	-21.361719	3.656384
-15.017096	-17.664928	3.666381
-14.548011	-15.616003	3.676378
-14.557410	-22.203570	3.686374
-14.345834	-18.394180	3.696371
-13.420719	-18.988964	3.706368
-13.030003	-20.415513	3.716365
-12.700397	-15.870678	3.726362
-11.917100	-20.010190	3.736358
-11.323173	-23.758901	3.746355
-10.788338	-21.283120	3.756352
-10.263590	-24.796078	3.766349
-10.286870	-25.714267	3.776346
-9.428091	-21.648321	3.786342
-8.840666	-28.677857	3.796339
-8.800907	-24.407557	3.806336
-7.929408	-20.242234	3.816333
-7.504617	-19.228576	3.826330
-7.044227	-18.629143	3.836326
-6.112819	-18.654708	3.846323
-5.884470	-18.772855	3.856320
-5.760181	-13.036432	3.866317
-4.864779	-4.528619	3.876314
-4.725462	-5.896772	3.886310
-4.270049	-0.478322	3.896307
-3.879241	12.533989	3.906304
-3.385007	30.405370	3.916301
-2.634283	41.080484	3.926298
-2.700279	47.087494	3.936294
-2.111679	63.059272	3.946291
-1.360494	77.542055	3.956288
-1.044211	96.974611	3.966285
-0.440083	112.573364	3.976282
0.000000	122.200299	3.981286
-0.318743	129.612354	3.986291
0.362276	132.580842	3.991296
0.449264	155.011087	3.996301
0.304718	150.575959	4.001306
0.843744	153.471786	4.006310
0.653161	153.061877	4.011315
0.882454	147.742429	4.016320
0.867244	153.702215	4.021325
0.571310	160.693088	4.026330
0.866132	144.280634	4.031334
0.702993	154.537870	4.036339
0.859544	147.954813	4.041344
0.976733	150.688941	4.046349
0.703042	154.110742	4.051354
1.202450	150.125217	4.056358
0.701567	154.414691	4.061363
1.063633	149.188335	4.066368
1.152646	153.644812	4.071373
0.966397	152.493900	4.076378
1.241882	148.192279	4.081382
0.572968	154.779678	4.086387
1.209245	150.408872	4.091392
0.863297	147.099971	4.096397
0.732155	161.914374	4.101402
0.980041	166.966065	4.106406
1.088469	180.151562	4.111411
1.480038	174.835153	4.116416
1.117499	177.286942	4.121421
0.711722	174.098142	4.126426
0.955934	183.927734	4.131430
1.206571	189.690853	4.136435
1.367337	178.750585	4.141440
1.403258	189.561953	4.146445
1.082089	183.825698	4.151450
1.044194	177.099088	4.156454
0.855898	189.040257	4.161459
1.206711	182.113535	4.166464
1.233334	185.599021	4.171469
1.346431	179.807381	4.176474
1.520673	183.902496	4.181478
1.466638	191.890040	4.186483
1.359347	184.709223	4.191488
1.390498	184.280391	4.196493
1.327459	184.141567	4.201498
1.446144	178.099113	4.206502
1.064761	187.390805	4.211507
0.823130	177.250749	4.216512
1.240381	184.835414	4.221517
0.823244	182.088159	4.226522
1.260326	184.930361	4.231526
1.252547	193.166925	4.236531
1.053645	184.114842	4.241536
1.103856	198.695215	4.246541
1.231663	189.190138	4.251546
1.557199	193.185619	4.256550
1.061351	207.541505	4.261555
1.136797	208.282664	4.266560
1.328906	213.706944	4.271565
1.027966	219.354011	4.276570
1.421150	209.307465	4.281574
1.114768	213.414615	4.286579
1.550006	204.307457	4.291584
1.614024	207.983244	4.296589
1.088837	217.604371	4.301594
1.561256	210.614291	4.306598
1.732337	218.247032	4.311603
1.803096	215.081638	4.316608
1.826781	211.376283	4.321613
1.455650	212.158939	4.326618
1.831391	209.363382	4.331622
1.450487	216.838996	4.336627
1.994341	216.298194	4.341632
1.678781	213.481235	4.346637
1.770183	218.516329	4.351642
1.899743	207.647372	4.356646
1.561317	218.428824	4.361651
1.546450	214.277087	4.366656
1.561087	216.884922	4.371661
1.919990	219.059162	4.376666
1.923778	221.298533	4.381670
1.795879	214.845443	4.386675
1.767814	213.524206	4.391680
1.962031	217.730096	4.396685
1.814022	218.506267	4.401690
2.124303	215.951922	4.406694
1.631321	225.428800	4.411699
1.481130	218.571071	4.416704
1.833125	211.852963	4.421709
1.879067	211.621132	4.426714
1.980813	217.176632	4.431718
1.769205	219.611105	4.436723
1.928153	212.736580	4.441728
2.011479	217.428085	4.446733
2.007427	219.067564	4.451738
2.136790	210.520862	4.456742
2.058588	214.785253	4.461747
1.989265	210.717980	4.466752
2.051204	214.482680	4.471757
1.926320	216.992151	4.476762
2.280858	215.259787	4.481766
1.791177	218.560416	4.486771
2.187867	207.073794	4.491776
2.211216	209.610660	4.496781
2.118271	219.581685	4.501786
2.353185	213.948120	4.506790
1.951854	214.074274	4.511795
1.996333	214.197017	4.516800
2.084210	207.001431	4.521805
1.875212	216.642620	4.526810
2.633806	208.652237	4.531814
2.332072	217.384128	4.536819
2.554765	210.271823	4.541824
2.293935	216.675080	4.546829
2.328024	217.011426	4.551834
2.250248	219.567301	4.556838
1.945652	230.811702	4.561843
2.228541	206.349195	4.566848
2.185566	216.638260	4.571853
2.177699	225.479138	4.576858
2.535267	219.614379	4.581862
2.114149	218.610994	4.586867
1.955680	219.524847	4.591872
2.048832	215.704202	4.596877
2.070743	222.616825	4.601882
2.559395	210.372300	4.606886
2.084562	210.968721	4.611891
2.268010	215.935608	4.616896
2.613754	221.936940	4.621901
2.510650	227.160702	4.626906
2.222845	221.317966	4.631910
2.455420	220.360857	4.636915
2.358738	217.240681	4.641920
2.548619	218.552376	4.646925
2.035770	224.058639	4.651930
2.163383	215.369839	4.656934
2.099061	216.297415	4.661939
2.182529	216.635515	4.666944
1.997252	220.391494	4.671949
2.335453	232.481157	4.676954
2.772402	233.453582	4.681958
2.472191	248.993747	4.686963
2.393862	245.370809	4.691968
2.721539	239.520218	4.696973
2.694028	239.875708	4.701978
2.660190	238.960341	4.706982
2.476680	246.038038	4.711987
2.447177	238.167958	4.716992
2.812555	245.390612	4.721997
2.548781	244.827652	4.727002
2.758854	240.675466	4.732006
2.330003	249.351358	4.737011
2.631583	240.423314	4.742016
3.009816	242.502778	4.747021
2.508757	247.991381	4.752026
2.858954	243.374308	4.757030
2.678411	244.089137	4.762035
2.247594	240.632162	4.767040
2.359010	239.273251	4.772045
2.740764	246.948926	4.777050
2.608579	245.852813	4.782054
2.471853	247.196701	4.787059
2.558477	247.221091	4.792064
2.768083	242.717796	4.797069
2.719895	245.436720	4.802074
3.056160	240.192234	4.807078
2.697778	237.109893	4.812083
2.501531	240.098792	4.817088
2.828031	248.384248	4.822093
2.371188	245.991222	4.827098
2.802449	253.197229	4.832102
3.020473	265.707547	4.837107
3.154197	266.436414	4.842112
3.117491	259.902578	4.847117
2.791844	251.762512	4.852122
2.489606	246.077056	4.857126
2.614568	255.330577	4.862131
2.923840	263.153660	4.867136
2.884834	263.362252	4.872141
3.011811	271.587231	4.877146
2.977441	264.451904	4.882150
3.038901	272.601726	4.887155
3.450361	271.426758	4.892160
3.285009	267.896546	4.897165
3.168550	265.766566	4.902170
3.459582	269.153692	4.907174
2.879409	255.485208	4.912179
3.104797	264.406619	4.917184
3.296129	273.744665	4.922189
3.034484	257.995108	4.927194
2.944776	255.278798	4.932198
3.306844	261.840743	4.937203
3.049521	265.940219	4.942208
2.766700	270.050018	4.947213
2.895605	264.777902	4.952218
3.138791	264.239915	4.957222
2.969898	272.074645	4.962227
3.138779	260.117474	4.967232
3.318090	264.360512	4.972237
3.086146	267.617603	4.977242
3.281967	272.263023	4.982246
2.849731	268.426608	4.987251
3.035578	266.024632	4.992256
3.132933	274.580125	4.997261
3.053438	271.789445	5.002266
3.162658	270.968723	5.007270
3.485836	285.256457	5.012275
3.550085	278.618210	5.017280
3.405612	264.391062	5.022285
3.069092	266.854605	5.027290
3.518021	272.792330	5.032294
3.275147	276.914854	5.037299
3.279333	288.857570	5.042304
3.634685	289.570695	5.047309
3.390770	289.991730	5.052314
3.548463	292.912526	5.057318
3.590777	295.436941	5.062323
3.174559	280.344345	5.067328
3.554064	287.166163	5.072333
3.158800	297.861654	5.077338
3.309739	291.795125	5.082342
3.394607	295.761897	5.087347
3.613210	295.759281	5.092352
3.633322	293.630047	5.097357
3.354337	293.281443	5.102362
3.473597	291.873842	5.107366
3.059776	295.124633	5.112371
3.453521	292.104776	5.117376
3.428067	289.416359	5.122381
3.294087	295.549828	5.127386
3.611554	292.769716	5.132390
3.378523	288.130115	5.137395
3.670123	294.453172	5.142400
3.736802	299.663009	5.147405
3.540327	301.392756	5.152410
3.841531	303.288140	5.157414
3.577475	301.785570	5.162419
3.602307	314.639409	5.167424
4.008506	317.562402	5.172429
3.836652	319.319932	5.177434
3.870236	301.388505	5.182438
3.781676	301.943389	5.187443
3.761514	296.384566	5.192448
3.792667	298.524745	5.197453
3.690530	298.170579	5.202458
3.871458	298.110590	5.207462
3.917262	296.869525	5.212467
3.667925	298.063379	5.217472
3.925180	303.452168	5.222477
3.872927	312.372812	5.227482
4.157120	300.090656	5.232486
3.568296	303.935191	5.237491
3.632860	305.019751	5.242496
4.036986	311.875687	5.247501
3.651177	314.584244	5.252506
4.242428	307.524888	5.257510
3.892547	318.713163	5.262515
4.324505	320.249534	5.267520
4.175239	317.321080	5.272525
3.689684	308.076561	5.277530
4.155039	307.086140	5.282534
4.320377	322.354105	5.287539
4.027802	312.762966	5.292544
3.895558	302.355759	5.297549
3.811431	307.972047	5.302554
4.072168	318.605897	5.307558
3.963034	319.822079	5.312563
4.068660	317.619331	5.317568
4.257479	316.346365	5.322573
4.003571	318.113587	5.327578
4.544988	315.605273	5.332582
3.905330	325.782241	5.337587
4.119543	319.993696	5.342592
4.146755	327.016262	5.347597
4.117103	324.369628	5.352602
4.346118	311.472839	5.357606
4.552215	317.205012	5.362611
4.275789	313.233441	5.367616
3.964770	304.325416	5.372621
4.207518	313.661755	5.377626
4.150867	311.671098	5.382630
4.099246	314.400062	5.387635
4.355063	312.382594	5.392640
4.410467	315.294110	5.397645
4.010989	315.774322	5.402650
4.321936	310.182598	5.407654
4.322594	315.684363	5.412659
4.295949	316.235875	5.417664
4.206947	313.604869	5.422669
3.910061	311.993544	5.427674
4.256723	313.809039	5.432678
4.155850	317.567633	5.437683
4.212832	317.751694	5.442688
4.275466	317.555213	5.447693
4.383341	318.139432	5.452698
4.445448	314.285665	5.457702
4.021173	316.373815	5.462707
4.343207	344.307309	5.467712
4.438494	340.505286	5.472717
4.332548	345.198006	5.477722
4.677403	344.416293	5.482726
4.813777	340.060491	5.487731
4.887102	344.620717	5.492736
4.763261	331.760216	5.497741
4.598045	324.740282	5.502746
4.273337	319.428489	5.507750
4.552315	325.076478	5.512755
4.559515	339.344159	5.517760
4.651491	344.091292	5.522765
4.660184	345.735112	5.527770
5.142633	342.910160	5.532774
4.812783	333.100219	5.537779
4.652418	324.946878	5.542784
4.716142	316.359790	5.547789
4.376394	317.991762	5.552794
4.396533	308.525639	5.557798
4.506697	324.669136	5.562803
4.859886	340.853665	5.567808
4.862317	347.522611	5.572813
4.473663	349.491286	5.577818
4.863988	345.605069	5.582822
4.664420	350.302968	5.587827
4.712608	353.506692	5.592832
4.859536	354.179709	5.597837
4.708419	351.096512	5.602842
4.866508	350.872419	5.607846
4.398722	354.286703	5.612851
4.591509	356.218063	5.617856
5.097721	351.712561	5.622861
4.781983	341.957353	5.627866
5.199932	341.951977	5.632870
5.120409	349.497487	5.637875
4.703133	348.724451	5.642880
4.555867	348.437468	5.647885
4.454656	359.941155	5.652890
4.587804	348.112912	5.657894
4.842672	359.563972	5.662899
4.560578	356.643667	5.667904
4.775655	365.411717	5.672909
5.158756	365.905359	5.677914
5.254414	366.931265	5.682918
5.014248	364.561223	5.687923
5.218905	364.177970	5.692928
4.960687	358.707047	5.697933
4.876613	358.217170	5.702938
5.463355	362.753906	5.707942
5.120528	364.756532	5.712947
5.030718	359.243404	5.717952
5.221118	355.882065	5.722957
5.029042	354.592844	5.727962
4.848478	354.488251	5.732966
5.250823	362.768205	5.737971
5.275549	369.193215	5.742976
5.311729	369.848783	5.747981
5.166837	360.955830	5.752986
5.254446	360.511821	5.757990
4.906012	348.879258	5.762995
5.345646	366.774548	5.768000
5.485022	365.629551	5.773005
5.112521	372.993179	5.778010
5.157353	354.629656	5.783014
5.574952	365.609124	5.788019
5.437031	360.340820	5.793024
5.587083	356.909871	5.798029
4.943351	349.949082	5.803034
5.526743	360.329919	5.808038
5.210148	347.572375	5.813043
5.280166	349.320486	5.818048
5.195282	352.377377	5.823053
5.192010	376.236270	5.828058
5.529557	367.792919	5.833062
5.784239	377.475443	5.838067
5.071015	372.604166	5.843072
5.452451	364.859473	5.848077
5.361800	369.382121	5.853082
5.885897	365.316748	5.858086
5.263773	365.695801	5.863091
5.333768	359.135720	5.868096
5.541117	364.722177	5.873101
6.001514	373.015186	5.878106
5.456404	359.258868	5.883110
5.197436	357.429622	5.888115
5.055052	363.232230	5.893120
5.380461	376.064329	5.898125
5.017895	375.769949	5.903130
5.568668	379.192332	5.908134
5.296476	383.888963	5.913139
5.487455	374.870611	5.918144
5.910503	372.595975	5.923149
5.707259	383.359510	5.928154
5.563629	380.297281	5.933158
5.650969	386.820058	5.938163
5.403099	382.932583	5.943168
5.639836	377.516986	5.948173
5.250470	378.979563	5.953178
5.590304	376.458531	5.958182
5.580082	383.154784	5.963187
5.658944	380.924583	5.968192
5.628904	379.053138	5.973197
5.290924	387.857232	5.978202
5.472330	395.200523	5.983206
5.481102	406.753448	5.988211
5.232975	402.097200	5.993216
5.444486	403.000550	5.998221
5.396429	407.171676	6.003226
5.722067	399.410400	6.008230
5.690686	399.149553	6.013235
5.990601	401.488085	6.018240
6.177376	394.666079	6.023245
6.019823	407.238506	6.028250
6.027854	393.923854	6.033254
5.800492	401.078088	6.038259
5.713629	405.093938	6.043264
5.920960	392.722520	6.048269
5.441243	399.856180	6.053274
5.566569	398.533043	6.058278
5.773399	394.232630	6.063283
6.186455	392.661927	6.068288
6.014141	389.338430	6.073293
5.931463	395.909995	6.078298
5.773399	396.222666	6.083302
6.173463	399.855331	6.088307
5.728130	402.275829	6.093312
5.999746	398.658142	6.098317
5.937685	405.128402	6.103322
5.632931	397.181153	6.108326
5.779326	392.709871	6.113331
5.603745	401.061409	6.118336
5.883277	397.464630	6.123341
5.685034	391.370517	6.128346
5.869016	397.416237	6.133350
5.657001	401.942089	6.138355
5.716245	402.742744	6.143360
5.563002	391.914821	6.148365
5.614529	398.079372	6.153370
5.768284	395.812125	6.158374
5.487957	393.856505	6.163379
5.711141	397.551686	6.168384
5.855794	405.346839	6.173389
5.314072	397.455702	6.178394
5.643407	394.297219	6.183398
5.598900	395.009723	6.188403
5.758578	398.034632	6.193408
6.007061	387.336762	6.198413
5.988059	393.597786	6.203418
5.790720	390.407926	6.208422
6.009284	398.631269	6.213427
5.620745	398.435872	6.218432
5.881906	390.020299	6.223437
5.792374	395.517237	6.228442
5.665469	393.496448	6.233446
6.031229	403.395705	6.238451
5.682930	402.630843	6.243456
5.711149	396.498082	6.248461
5.434054	403.717058	6.253466
5.556514	401.268047	6.258470
5.676828	393.472504	6.263475
5.763490	386.783248	6.268480
5.997422	388.692346	6.273485
5.713117	389.334851	6.278490
5.736655	395.136783	6.283494
5.713904	391.755049	6.288499
5.566604	397.533128	6.293504
5.807880	386.896501	6.298509
5.913024	390.588028	6.303514
5.896826	398.737419	6.308518
5.525922	392.838042	6.313523
5.694130	394.013939	6.318528
5.766999	391.772020	6.323533
5.824780	392.500136	6.328538
5.796868	388.087804	6.333542
5.821657	392.029209	6.338547
5.458273	396.369964	6.343552
5.526321	407.198577	6.348557
5.686658	400.336417	6.353562
6.004642	401.242068	6.358566
5.866971	402.114705	6.363571
5.949339	402.513095	6.368576
5.818168	399.170494	6.373581
5.945121	403.589452	6.378586
6.165183	397.034318	6.383590
6.291453	388.896150	6.388595
5.881272	395.993603	6.393600
5.889779	391.581892	6.398605
5.882497	388.539428	6.403610
5.798871	372.799843	6.408614
5.742926	384.391368	6.413619
5.697611	379.007306	6.418624
5.492691	383.054305	6.423629
5.577180	395.921002	6.428634
5.852589	397.782472	6.433638
5.791749	399.883292	6.438643
5.765700	403.098657	6.443648
6.067263	394.214832	6.448653
5.365806	393.442026	6.453658
5.966076	388.064381	6.458662
5.877291	403.422854	6.463667
5.856955	390.071520	6.468672
5.739925	382.224581	6.473677
5.515936	386.062592	6.478682
5.542843	396.264879	6.483686
5.445584	394.508371	6.488691
5.632368	394.308256	6.493696
6.054503	399.645930	6.498701
5.841120	399.195295	6.503706
5.958830	390.394063	6.508710
6.050223	391.809791	6.513715
5.550641	396.899566	6.518720
5.949853	382.527025	6.523725
5.618020	381.392580	6.528730
6.013164	383.725681	6.533734
5.438907	388.415857	6.538739
5.572668	400.642072	6.543744
5.919335	402.239272	6.548749
6.060592	398.831840	6.553754
5.525868	387.655557	6.558758
5.822940	382.825303	6.563763
5.373345	392.700441	6.568768
5.867629	394.274511	6.573773
5.776013	399.227598	6.578778
5.790986	397.523109	6.583782
5.754640	396.051293	6.588787
5.813971	404.606479	6.593792
5.898943	398.512283	6.598797
5.950161	398.225838	6.603802
5.507784	392.593930	6.608806
5.693984	393.776499	6.613811
5.888399	399.523184	6.618816
6.158279	390.808845	6.623821
5.605593	385.991506	6.628826
5.606460	375.648823	6.633830
5.808486	380.527422	6.638835
5.595138	386.648047	6.643840
5.884930	386.738684	6.648845
5.536012	388.283512	6.653850
5.769737	393.818388	6.658854
5.903339	396.508852	6.663859
5.880098	401.821395	6.668864
5.948677	383.523725	6.673869
5.611444	381.406176	6.678874
5.433932	377.124857	6.683878
5.599389	390.659087	6.688883
5.706097	392.936139	6.693888
5.895621	383.187166	6.698893
5.830272	394.732714	6.703898
5.914346	402.002671	6.708902
6.040748	393.386742	6.713907
5.846019	386.690954	6.718912
5.860506	367.746864	6.723917
5.768705	375.427188	6.728922
5.875161	368.782295	6.733926
5.946216	367.170265	6.738931
5.686489	377.357339	6.743936
6.001958	367.439942	6.748941
5.582180	375.095723	6.753946
5.591761	375.603594	6.758950
5.821913	367.506108	6.763955
5.625348	372.624331	6.768960
5.420769	364.848067	6.773965
5.547506	377.841012	6.778970
5.496847	386.144497	6.783974
5.558868	388.033072	6.788979
5.960977	396.145395	6.793984
6.130864	384.536004	6.798989
5.525553	395.849772	6.803994
5.668064	392.932538	6.808998
5.836164	397.322900	6.814003
5.386381	390.651254	6.819008
5.659929	395.806559	6.824013
5.951654	396.956775	6.829018
6.112906	399.620761	6.834022
5.703120	391.360933	6.839027
6.191010	392.227307	6.844032
5.893962	381.080229	6.849037
5.508485	383.545131	6.854042
5.738618	381.053942	6.859046
5.754725	386.720991	6.864051
5.712302	388.622767	6.869056
6.089593	379.315787	6.874061
5.702387	377.098498	6.879066
5.774795	379.206912	6.884070
6.075971	370.240901	6.889075
5.683795	375.177797	6.894080
5.522474	369.150675	6.899085
5.631862	377.207611	6.904090
5.437096	370.157487	6.909094
5.842915	380.705366	6.914099
5.849380	391.730284	6.919104
6.157369	395.488109	6.924109
5.665862	386.140076	6.929114
5.894290	379.134375	6.934118
5.710031	376.135462	6.939123
5.553470	381.367644	6.944128
5.772096	379.612266	6.949133
5.789370	380.802319	6.954138
5.788699	384.462967	6.959142
5.246365	384.652344	6.964147
5.532908	391.023685	6.969152
6.187730	393.942538	6.974157
5.865686	394.654234	6.979162
5.690262	395.836513	6.984166
5.880254	400.574631	6.989171
5.989809	391.803151	6.994176
5.921467	383.413897	6.999181
6.001555	380.661473	7.004186
5.764482	379.173652	7.009190
5.837026	379.083187	7.014195
5.752011	378.330858	7.019200
5.756531	375.251746	7.024205
5.598216	380.778439	7.029210
5.906941	379.208265	7.034214
5.578836	374.045687	7.039219
5.620016	375.627472	7.044224
6.112747	366.811787	7.049229
5.669384	371.933876	7.054234
5.846743	371.516934	7.059238
5.761353	367.445814	7.064243
5.621129	377.924219	7.069248
5.631058	365.526800	7.074253
5.312554	378.010527	7.079258
5.621835	375.968856	7.084262
5.943002	380.363706	7.089267
5.560537	389.016579	7.094272
5.730950	389.853600	7.099277
5.909070	383.630917	7.104282
5.685532	389.136194	7.109286
5.623075	395.328095	7.114291
6.037186	397.003314	7.119296
5.844440	388.054569	7.124301
5.539696	385.229560	7.129306
5.678722	387.783128	7.134310
5.695384	389.128305	7.139315
5.694277	388.732997	7.144320
5.760036	386.144172	7.149325
5.716342	402.583936	7.154330
5.913799	393.678457	7.159334
5.717067	389.703873	7.164339
5.672427	391.324416	7.169344
5.911572	392.448068	7.174349
5.950653	398.655699	7.179354
5.926188	385.849193	7.184358
5.996003	375.789943	7.189363
5.696216	386.831204	7.194368
5.830940	375.065973	7.199373
5.483619	375.345020	7.204378
5.483936	369.960140	7.209382
5.777533	386.005348	7.214387
5.883455	395.423280	7.219392
5.918163	394.310500	7.224397
5.720815	394.566049	7.229402
5.750953	386.740344	7.234406
6.003142	372.700902	7.239411
5.229207	377.207221	7.244416
5.464334	385.079941	7.249421
5.338390	387.991408	7.254426
5.952643	391.068481	7.259430
5.667096	388.838427	7.264435
5.917205	402.311945	7.269440
5.662227	404.284992	7.274445
5.513566	404.643647	7.279450
5.327422	394.061329	7.284454
5.584651	402.718387	7.289459
5.618219	402.599226	7.294464
5.787525	398.795085	7.299469
5.457314	403.200248	7.304474
5.487817	396.785549	7.309478
5.583070	400.121116	7.314483
5.440060	409.315461	7.319488
5.951898	417.986419	7.324493
6.043270	428.441222	7.329498
5.827272	423.365472	7.334502
5.675777	415.466970	7.339507
5.686368	408.599795	7.344512
5.796401	402.941444	7.349517
5.587788	405.805754	7.354522
6.090630	418.543643	7.359526
5.852124	411.351655	7.364531
5.561972	413.406146	7.369536
5.587557	404.401038	7.374541
5.505441	403.423622	7.379546
5.765667	420.654198	7.384550
6.113511	421.612121	7.389555
6.029714	426.567154	7.394560
5.634084	407.775867	7.399565
5.596371	405.184269	7.404570
5.707630	403.072378	7.409574
5.834946	402.267798	7.414579
5.989410	407.365833	7.419584
6.124788	399.650186	7.424589
5.425430	403.676580	7.429594
5.738166	406.079545	7.434598
6.001473	407.082350	7.439603
5.710025	408.728910	7.444608
5.765332	394.694988	7.449613
5.899917	400.988899	7.454618
5.970660	403.856896	7.459622
5.958002	397.429977	7.464627
5.757947	400.315092	7.469632
5.929927	398.873911	7.474637
5.792251	406.827199	7.479642
5.450558	394.348808	7.484646
6.248974	404.221406	7.489651
6.034689	393.146776	7.494656
5.699921	392.313353	7.499661
5.782375	401.965926	7.504666
5.764422	395.416447	7.509670
5.952518	398.591931	7.514675
5.913976	406.225959	7.519680
6.172446	396.336459	7.524685
6.104516	395.692187	7.529690
5.670323	384.402076	7.534694
5.939048	381.208799	7.539699
5.304790	382.076982	7.544704
5.983571	383.350054	7.549709
5.782729	389.095389	7.554714
5.772117	389.713995	7.559718
5.951181	382.674898	7.564723
5.753044	379.583244	7.569728
5.762621	372.602344	7.574733
5.688432	373.977573	7.579738
5.159626	380.745585	7.584742
5.868367	388.082182	7.589747
5.801608	398.163101	7.594752
6.270853	398.402795	7.599757
6.046204	393.274623	7.604762
5.792696	380.526155	7.609766
5.774832	373.584356	7.614771
5.644309	375.370217	7.619776
5.685213	373.218733	7.624781
5.314995	385.871923	7.629786
5.533975	395.189882	7.634790
5.663299	389.082413	7.639795
5.565245	395.343168	7.644800
6.014465	397.712092	7.649805
5.638474	403.484874	7.654810
5.731879	396.376933	7.659814
5.800033	398.425904	7.664819
5.580096	397.372004	7.669824
5.999006	399.517881	7.674829
5.912657	399.721237	7.679834
5.812468	392.684760	7.684838
5.968334	396.479075	7.689843
5.845979	393.926051	7.694848
5.941601	389.668374	7.699853
5.519186	389.101790	7.704858
5.356950	387.045409	7.709862
5.483473	398.965866	7.714867
5.542251	396.843217	7.719872
6.143436	391.993786	7.724877
5.887657	398.140047	7.729882
5.721856	398.071107	7.734886
5.961243	400.210310	7.739891
5.983894	400.073877	7.744896
5.857833	390.795136	7.749901
5.595620	384.315571	7.754906
5.807887	395.491748	7.759910
5.723331	388.253502	7.764915
5.851100	400.895117	7.769920
5.354698	398.125446	7.774925
5.453933	400.353049	7.779930
5.810713	405.716784	7.784934
5.559453	407.967666	7.789939
5.498309	400.178404	7.794944
5.714425	399.157425	7.799949
5.473493	395.319483	7.804954
5.552858	389.298937	7.809958
5.471962	395.091921	7.814963
5.613822	403.118471	7.819968
5.922871	399.827121	7.824973
5.580269	399.023400	7.829978
5.520661	395.875236	7.834982
6.176553	397.082292	7.839987
5.897119	397.622792	7.844992
6.106654	397.551992	7.849997
5.808446	402.863324	7.855002
5.285837	395.307722	7.860006
6.025550	403.471559	7.865011
5.696019	408.442942	7.870016
5.979325	403.725574	7.875021
5.892184	400.584887	7.880026
5.541855	399.380571	7.885030
5.608855	397.522394	7.890035
6.030045	397.681031	7.895040
5.962670	398.283220	7.900045
5.845553	400.250485	7.905050
5.582122	397.279792	7.910054
6.044911	403.572902	7.915059
6.118368	410.439556	7.920064
5.948399	397.927928	7.925069
6.086428	405.047060	7.930074
5.940052	415.403062	7.935078
5.842215	401.304542	7.940083
5.414870	394.958416	7.945088
5.788148	389.821985	7.950093
6.038287	406.876954	7.955098
5.799059	397.059107	7.960102
5.782162	384.754464	7.965107
5.613824	398.331508	7.970112
5.700298	390.519121	7.975117
5.941937	395.223835	7.980122
5.957422	391.418760	7.985139
5.885741	383.240803	7.990157
5.870101	386.701958	7.995174
5.857071	386.227477	8.000192
5.763699	381.685194	8.005210
5.832056	383.400679	8.010227
5.601648	377.917362	8.015245
5.540302	386.248695	8.020262
5.716245	380.067404	8.025280
5.545704	397.592786	8.030298
5.635515	399.992866	8.035315
6.003582	390.351161	8.040333
5.930606	400.574620	8.045350
6.053836	399.602271	8.050368
5.868291	394.780941	8.055386
5.862405	387.495219	8.060403
5.940611	386.608819	8.065421
5.714715	395.606556	8.070438
5.734048	383.826244	8.075456
6.089716	381.249067	8.080474
5.981312	398.221924	8.085491
5.830476	382.533046	8.090509
5.736630	389.193767	8.095526
5.784863	391.840197	8.100544
5.741571	389.707375	8.105562
6.058294	402.836188	8.110579
6.021370	395.444875	8.115597
5.862337	396.577460	8.120614
5.697347	391.674017	8.125632
5.948971	395.036494	8.130650
5.777516	404.559029	8.135667
6.021984	404.069449	8.140685
6.070730	409.963078	8.145702
5.601395	399.830888	8.150720
6.219582	408.352403	8.155738
5.965869	400.329189	8.160755
6.264807	397.745119	8.165773
5.942120	397.748339	8.170790
6.006267	392.499729	8.175808
5.800998	382.679620	8.180826
5.819261	392.484843	8.185843
5.763541	398.754592	8.190861
5.799333	407.477808	8.195878
5.803312	407.814847	8.200896
6.185537	405.331334	8.205914
6.112681	406.980585	8.210931
5.977109	404.568734	8.215949
5.595579	411.356588	8.220966
5.658212	404.861687	8.225984
5.848746	409.672765	8.231002
5.526473	408.423083	8.236019
6.248050	399.275086	8.241037
5.783248	411.914140	8.246054
5.445511	411.036105	8.251072
5.862648	410.311191	8.256090
5.793287	417.365711	8.261107
6.067302	425.947471	8.266125
5.928756	430.339907	8.271142
6.108358	425.388774	8.276160
6.206752	431.776397	8.281178
6.109223	439.393910	8.286195
6.296079	427.842938	8.291213
6.124674	432.562410	8.296230
6.074334	420.805613	8.301248
6.213599	409.558750	8.306266
5.724646	417.935006	8.311283
6.011370	420.118046	8.316301
5.955851	435.173417	8.321318
6.149742	431.987271	8.326336
6.306263	431.530405	8.331354
6.558154	428.376197	8.336371
6.150769	416.356613	8.341389
6.145799	416.215380	8.346406
5.933385	412.136703	8.351424
6.067490	409.714155	8.356442
5.968479	427.988898	8.361459
6.299704	418.952544	8.366477
6.141867	430.940765	8.371494
6.259491	434.769208	8.376512
6.246598	424.189953	8.381530
6.092852	429.919657	8.386547
6.579091	421.982466	8.391565
6.374670	408.757143	8.396582
6.195900	402.135967	8.401600
6.241274	392.765723	8.406618
5.919956	403.921175	8.411635
6.188712	402.294872	8.416653
5.979329	401.557670	8.421670
6.225690	412.242336	8.426688
6.307696	406.318747	8.431706
6.006066	421.264347	8.436723
6.124255	426.099387	8.441741
6.004779	432.095118	8.446758
6.403466	435.365135	8.451776
6.502617	431.051447	8.456794
6.107509	434.650961	8.461811
6.327945	428.377476	8.466829
6.317684	425.785044	8.471846
6.614088	437.885132	8.476864
6.294010	429.891238	8.481882
6.041469	425.935609	8.486899
6.613892	420.853503	8.491917
6.291661	423.362325	8.496934
6.290388	413.904707	8.501952
6.283342	415.136554	8.506970
6.262042	421.587108	8.511987
6.486372	418.210005	8.517005
6.548106	411.377576	8.522022
6.258975	413.717112	8.527040
6.393598	399.573996	8.532058
5.990512	409.300081	8.537075
6.743801	414.300694	8.542093
6.702609	410.529700	8.547110
6.276242	407.412340	8.552128
6.352924	399.529862	8.557146
6.237820	400.415727	8.562163
6.353823	397.869787	8.567181
6.389560	397.728487	8.572199
6.253131	402.799072	8.577216
6.110160	394.458713	8.582234
6.173792	413.957638	8.587251
6.375662	424.516739	8.592269
6.620373	428.672402	8.597287
6.508456	420.191468	8.602304
6.750277	425.212262	8.607322
6.401602	415.222102	8.612339
6.235604	402.505153	8.617357
6.364289	410.068275	8.622375
6.350373	422.475747	8.627392
6.700004	422.143256	8.632410
6.757360	426.845819	8.637427
6.199066	408.506804	8.642445
6.635596	405.538262	8.647463
6.064202	410.623353	8.652480
6.301044	414.489916	8.657498
6.482098	423.944607	8.662515
6.573183	418.240495	8.667533
6.536984	422.433858	8.672551
6.333070	424.861028	8.677568
6.804905	420.305916	8.682586
6.429934	426.792951	8.687603
6.399078	427.353196	8.692621
6.640398	431.026560	8.697639
6.180708	439.849515	8.702656
6.505346	435.014509	8.707674
6.331027	443.852713	8.712691
6.363966	435.844530	8.717709
6.494336	432.131857	8.722727
6.381378	436.845329	8.727744
6.419674	425.816245	8.732762
6.548326	432.590442	8.737779
6.329889	422.393682	8.742797
6.534428	423.128482	8.747815
6.417125	430.761712	8.752832
6.664384	421.274617	8.757850
6.329592	426.682397	8.762867
6.344144	422.968938	8.767885
6.526213	430.820347	8.772903
6.548748	437.210390	8.777920
6.744486	444.649414	8.782938
6.665473	444.510314	8.787955
6.869786	438.431853	8.792973
6.848361	430.384854	8.797991
6.424184	426.733824	8.803008
6.821385	423.361192	8.808026
6.523356	427.895378	8.813043
6.590503	432.246119	8.818061
6.463545	423.931639	8.823079
6.177938	438.881055	8.828096
6.469112	436.225613	8.833114
7.080169	451.107131	8.838131
7.071428	454.447299	8.843149
6.843242	450.500471	8.848167
6.436654	438.379762	8.853184
6.758062	443.422805	8.858202
6.717958	443.675235	8.863219
6.991381	455.794715	8.868237
6.871048	439.144811	8.873255
6.601437	442.188183	8.878272
6.667662	435.134138	8.883290
6.715760	438.478020	8.888307
7.295588	446.156662	8.893325
6.631632	434.426571	8.898343
6.303093	437.371880	8.903360
6.833247	442.893449	8.908378
6.862597	448.048525	8.913395
6.991036	450.761291	8.918413
6.777214	440.737365	8.923431
6.644782	435.462739	8.928448
7.007419	431.129858	8.933466
6.617008	436.445372	8.938483
7.011638	446.122228	8.943501
6.668060	440.252686	8.948519
6.566585	438.880046	8.953536
6.767013	439.931067	8.958554
6.947128	448.271933	8.963571
7.045775	449.241073	8.968589
7.143041	454.256122	8.973607
6.808588	451.077016	8.978624
6.709160	429.797492	8.983642
6.901116	443.305640	8.988659
7.053154	448.397312	8.993677
7.093646	452.209442	8.998695
6.608648	434.505848	9.003712
7.054563	435.420577	9.008730
6.719097	434.056197	9.013747
6.437965	444.757259	9.018765
6.812928	454.235232	9.023783
6.919339	464.250743	9.028800
6.999745	450.630472	9.033818
7.121319	459.595890	9.038835
6.595128	458.463360	9.043853
6.663309	456.685445	9.048871
6.738274	453.091900	9.053888
6.608453	454.989919	9.058906
6.783290	449.528292	9.063923
6.772866	460.508837	9.068941
7.044490	447.164717	9.073959
7.188738	461.425115	9.078976
7.173919	452.988912	9.083994
7.330908	450.316623	9.089011
6.822855	456.925504	9.094029
7.302395	453.416892	9.099047
6.861301	459.021216	9.104064
6.797633	452.337806	9.109082
6.996513	457.125499	9.114099
6.931726	455.885963	9.119117
7.214104	449.243008	9.124135
7.204241	445.637510	9.129152
7.171541	453.090239	9.134170
7.308206	454.523632	9.139187
6.989688	462.213648	9.144205
7.295003	449.656346	9.149223
7.150935	456.328117	9.154240
6.942683	453.754079	9.159258
6.683001	447.836676	9.164275
6.576782	453.388530	9.169293
7.015995	460.227686	9.174311
7.208276	457.486752	9.179328
7.173643	453.206643	9.184346
7.065871	448.827543	9.189363
6.893067	461.900557	9.194381
6.998936	452.486091	9.199399
7.117703	454.029584	9.204416
6.848344	450.799254	9.209434
7.131350	458.713754	9.214451
7.260448	479.767755	9.219469
7.474589	466.214879	9.224487
7.134123	460.960218	9.229504
7.084022	461.330978	9.234522
7.367741	463.546052	9.239539
7.088752	457.991428	9.244557
7.099753	447.490465	9.249575
7.210650	465.416781	9.254592
7.008940	471.340204	9.259610
7.014582	476.899785	9.264627
7.224521	487.135771	9.269645
7.593740	481.179779	9.274663
7.394465	481.163662	9.279680
6.992120	473.804325	9.284698
7.325698	476.734260	9.289715
7.065282	483.610461	9.294733
7.239516	483.627340	9.299751
7.210303	487.096952	9.304768
7.011719	483.991226	9.309786
7.124842	484.216493	9.314803
7.102283	492.541798	9.319821
7.729959	486.583179	9.324839
7.197532	494.499227	9.329856
7.204452	487.886794	9.334874
7.345781	487.684769	9.339891
7.172184	486.102521	9.344909
7.628274	483.339183	9.349927
7.453097	482.353624	9.354944
7.481148	484.548800	9.359962
7.483968	476.520071	9.364979
7.369954	490.609521	9.369997
7.354556	480.339891	9.375015
7.459009	482.945968	9.380032
7.247650	479.747571	9.385050
7.822334	475.065879	9.390067
7.533251	467.688798	9.395085
7.384034	460.725302	9.400103
7.604264	462.132980	9.405120
7.194028	465.211012	9.410138
7.204995	454.779477	9.415155
7.271739	470.405850	9.420173
7.530663	471.353034	9.425191
7.521888	477.539717	9.430208
7.282358	485.166875	9.435226
7.386888	479.713099	9.440243
7.168259	483.360710	9.445261
7.675985	478.613769	9.450279
7.485893	485.447395	9.455296
7.706522	483.279521	9.460314
7.615282	477.461947	9.465331
7.397372	483.517299	9.470349
7.606031	474.733649	9.475367
7.571653	481.268323	9.480384
7.403616	482.882002	9.485402
7.597675	483.851973	9.490419
7.602365	488.963587	9.495437
7.419666	472.891462	9.500455
7.352689	476.458507	9.505472
7.613510	484.723629	9.510490
7.755899	476.205979	9.515507
7.420067	476.637287	9.520525
7.419165	487.379674	9.525543
7.710684	479.122676	9.530560
7.333863	477.127306	9.535578
7.857064	477.114754	9.540595
7.508154	482.335417	9.545613
7.585167	478.280804	9.550631
7.562103	476.504560	9.555648
7.495508	481.229714	9.560666
7.568617	478.570563	9.565683
7.517068	481.838549	9.570701
7.263546	480.483417	9.575719
7.599490	476.972053	9.580736
7.343501	474.137251	9.585754
7.600077	479.995184	9.590771
6.880155	494.078586	9.595789
7.683591	485.122846	9.600807
7.549034	484.951423	9.605824
7.255835	492.646953	9.610842
7.463999	487.842805	9.615859
7.090471	501.057750	9.620877
7.808120	508.112072	9.625895
7.707088	506.067177	9.630912
7.873234	508.584698	9.635930
7.897139	512.664525	9.640947
7.695328	516.009709	9.645965
7.698449	515.712573	9.650983
7.974689	511.090256	9.656000
7.769898	510.781516	9.661018
8.403537	507.431783	9.666035
7.903099	503.934695	9.671053
7.718201	489.267220	9.676071
7.764871	482.004783	9.681088
7.326335	489.543204	9.686106
7.735031	493.742617	9.691123
7.865505	510.337329	9.696141
8.008590	498.291401	9.701159
7.815447	494.771413	9.706176
7.843276	507.456423	9.711194
8.071274	502.731214	9.716211
7.720613	500.125834	9.721229
8.045662	493.192158	9.726247
8.056699	495.440492	9.731264
7.664376	481.067453	9.736282
7.699863	484.634224	9.741299
7.674936	498.122747	9.746317
7.764232	506.682996	9.751335
7.550968	507.719944	9.756352
7.636089	509.032030	9.761370
7.914148	508.890632	9.766387
7.822118	512.774031	9.771405
7.699080	507.087661	9.776423
7.907041	506.537527	9.781440
8.029269	509.920300	9.786458
8.131940	507.758283	9.791475
8.072931	510.560388	9.796493
8.242590	511.395329	9.801511
7.932115	505.773041	9.806528
7.761865	511.600031	9.811546
8.235871	504.633544	9.816563
8.089013	506.625755	9.821581
8.121806	512.373595	9.826599
8.063671	500.179314	9.831616
8.005039	506.714642	9.836634
8.006801	498.023357	9.841651
7.793632	515.325162	9.846669
8.130922	510.832133	9.851687
8.074078	506.312497	9.856704
8.051202	514.846143	9.861722
8.335614	504.138208	9.866739
7.962013	512.581640	9.871757
8.161708	511.467917	9.876775
8.362788	505.446744	9.881792
7.709079	504.627679	9.886810
7.958502	502.568899	9.891827
7.912020	503.182088	9.896845
8.126314	494.239757	9.901863
8.030242	499.581754	9.906880
7.819219	513.231989	9.911898
7.993289	512.936472	9.916915
8.048171	506.988697	9.921933
8.001523	501.949917	9.926951
8.171551	499.054674	9.931968
7.671232	507.072994	9.936986
8.096500	494.370635	9.942003
7.863572	497.338842	9.947021
7.875200	504.175582	9.952039
8.149962	508.493812	9.957056
8.022652	520.751862	9.962074
8.205795	527.100995	9.967091
8.098557	541.312498	9.972109
8.018619	538.961339	9.977127
8.244686	533.826172	9.982144
7.970908	531.309727	9.987162
8.061727	528.490005	9.992179
8.080739	531.242020	9.997197
8.168734	534.071588	10.002215
8.080971	526.855443	10.007232
8.049658	533.244490	10.012250
7.917594	530.223006	10.017267
8.466735	538.809050	10.022285
8.141809	535.590567	10.027303
8.793971	538.363300	10.032320
8.195271	539.495354	10.037338
8.472412	540.764734	10.042355
8.459297	532.766879	10.047373
8.409672	546.931491	10.052391
9.026654	536.512253	10.057408
8.442866	547.137721	10.062426
8.677644	536.547996	10.067443
8.295736	526.985855	10.072461
8.249737	543.513575	10.077479
8.534424	535.888778	10.082496
8.594055	537.750811	10.087514
8.398478	520.506709	10.092531
8.108167	523.064192	10.097549
8.207917	519.264782	10.102567
8.283784	526.261877	10.107584
8.386210	542.113094	10.112602
8.549630	530.638311	10.117619
8.681501	534.183678	10.122637
8.468175	526.794704	10.127655
8.951958	518.226699	10.132672
8.466751	522.515684	10.137690
8.107225	518.620976	10.142707
8.800405	516.284386	10.147725
8.458864	503.130969	10.152743
8.265867	496.325796	10.157760
8.376139	515.075917	10.162778
8.685234	511.417275	10.167795
8.389493	516.711667	10.172813
8.273879	513.485639	10.177831
8.627415	513.256676	10.182848
8.043421	525.365379	10.187866
8.393646	518.083768	10.192883
8.434280	522.467087	10.197901
8.616147	521.324599	10.202919
8.897297	528.466255	10.207936
8.154548	535.840923	10.212954
8.255429	534.480751	10.217971
8.514850	529.949426	10.222989
8.534025	529.170096	10.228007
8.475384	530.596227	10.233024
8.353099	527.888789	10.238042
8.487837	533.393447	10.243059
8.149923	532.644820	10.248077
8.011567	536.437654	10.253095
8.547191	549.194609	10.258112
8.728217	556.358275	10.263130
8.961168	560.320154	10.268147
8.745503	561.884498	10.273165
8.596504	561.106270	10.278183
8.737718	551.522113	10.283200
8.985781	556.030729	10.288218
8.600401	541.019084	10.293235
8.629502	534.917551	10.298253
8.361483	554.004692	10.303271
8.656852	555.359579	10.308288
8.616857	555.179651	10.313306
8.438255	552.919688	10.318323
8.759254	551.736464	10.323341
8.760465	558.678998	10.328359
9.048514	554.162115	10.333376
8.571222	555.653842	10.338394
8.555805	555.892939	10.343411
9.131791	556.307615	10.348429
8.849411	558.813369	10.353447
9.155428	556.610017	10.358464
8.894357	561.586568	10.363482
8.925210	563.522539	10.368499
8.676653	552.872835	10.373517
8.502257	559.082340	10.378535
8.895968	552.229400	10.383552
8.798406	552.430875	10.388570
8.550947	557.320085	10.393587
8.710352	559.005542	10.398605
8.703925	567.975291	10.403623
8.644149	554.361126	10.408640
8.683671	559.899645	10.413658
8.599002	560.171683	10.418675
8.961197	554.166275	10.423693
8.642803	557.327763	10.428711
8.577332	554.248504	10.433728
8.825702	564.554252	10.438746
9.175052	573.556622	10.443763
9.084991	561.105371	10.448781
8.735500	563.637419	10.453799
8.816428	562.008973	10.458816
9.149167	581.153494	10.463834
9.009813	583.523233	10.468851
9.103680	570.336260	10.473869
8.814802	564.467574	10.478887
9.134720	570.148355	10.483904
8.918020	565.019437	10.488922
8.592454	574.405263	10.493939
9.268203	574.668611	10.498957
9.147773	580.645606	10.503975
9.134435	585.059487	10.508992
9.210547	589.004920	10.514010
8.874895	575.822125	10.519027
9.165503	575.590398	10.524045
9.318614	588.369444	10.529063
9.154147	573.865955	10.534080
9.077101	573.208997	10.539098
8.651935	568.958492	10.544115
9.171122	563.307178	10.549133
9.054898	576.257802	10.554151
9.295660	583.617247	10.559168
9.292007	582.551159	10.564186
9.111068	587.101753	10.569203
9.400570	577.330247	10.574221
9.220206	568.550699	10.579239
9.273207	554.609596	10.584256
9.063849	562.150009	10.589274
8.922427	564.381215	10.594291
9.286979	575.031681	10.599309
8.908937	579.105073	10.604327
9.291045	579.004176	10.609344
9.095907	584.386966	10.614362
9.036510	585.399811	10.619379
9.355411	578.798423	10.624397
9.456147	589.054733	10.629415
9.500204	588.729092	10.634432
9.280183	593.020725	10.639450
9.562646	586.213605	10.644467
9.191826	574.986599	10.649485
8.913098	569.974696	10.654503
9.175511	578.905484	10.659520
9.939968	578.265000	10.664538
9.352698	575.548359	10.669555
9.557003	562.438762	10.674573
9.365136	562.348901	10.679591
8.984703	558.381722	10.684608
9.183007	555.778683	10.689626
9.095293	563.423113	10.694643
9.381536	574.057446	10.699661
9.569476	587.910315	10.704679
9.494392	585.463715	10.709696
9.687336	577.982662	10.714714
9.094967	574.140203	10.719731
9.741397	566.158915	10.724749
9.353426	558.462778	10.729767
9.160392	548.738489	10.734784
9.489347	568.401137	10.739802
9.634099	575.674636	10.744819
9.615245	561.416584	10.749837
9.398644	559.935741	10.754855
9.289626	562.748846	10.759872
9.228705	563.818732	10.764890
9.284398	578.257200	10.769907
9.154864	575.516177	10.774925
9.502135	587.182366	10.779943
9.310865	585.041147	10.784960
9.364283	580.737745	10.789978
9.263321	586.670667	10.794995
9.412852	585.668940	10.800013
9.767244	589.930532	10.805031
9.631033	587.294695	10.810048
9.645637	588.605213	10.815066
9.280235	587.696789	10.820083
9.659641	587.018806	10.825101
9.407082	580.311295	10.830119
9.365534	583.877533	10.835136
9.737550	579.814545	10.840154
9.379987	591.007349	10.845171
9.635916	579.145657	10.850189
9.490084	580.367703	10.855207
9.574160	578.000308	10.860224
9.475860	589.294500	10.865242
9.572496	589.159436	10.870259
9.738462	597.597263	10.875277
9.590359	598.873314	10.880295
9.651449	610.638006	10.885312
10.196145	598.207195	10.890330
9.554524	598.629612	10.895347
9.987288	583.764298	10.900365
9.540671	574.546784	10.905383
9.745050	583.726507	10.910400
9.482510	576.468298	10.915418
9.557100	593.927063	10.920435
9.789999	604.405671	10.925453
9.555900	605.013545	10.930471
9.764809	615.391777	10.935488
10.119605	614.572482	10.940506
9.978437	612.874689	10.945523
9.952802	600.214501	10.950541
9.949855	609.060649	10.955559
9.335529	599.768413	10.960576
9.702094	600.626156	10.965594
9.684976	596.573642	10.970611
10.348495	606.558749	10.975629
9.947514	604.150586	10.980647
9.580332	606.802176	10.985664
10.138290	599.686799	10.990682
10.177295	606.045920	10.995699
9.791475	590.838643	11.000717
9.511770	595.900173	11.005735
9.639385	599.622945	11.010752
10.150333	604.898268	11.015770
9.986638	610.219335	11.020787
9.860099	614.095540	11.025805
9.959533	605.587714	11.030823
9.699797	606.609859	11.035840
10.089978	602.973208	11.040858
9.830602	608.189346	11.045875
9.633186	610.006454	11.050893
9.437260	608.203632	11.055911
9.806563	613.201350	11.060928
10.318417	610.255687	11.065946
9.849031	607.040890	11.070963
9.940836	607.594546	11.075981
10.048532	610.127551	11.080999
10.101652	604.924788	11.086016
9.946802	606.659487	11.091034
10.008717	611.860000	11.096051
9.779931	599.701856	11.101069
10.013382	613.992581	11.106087
9.897286	632.030369	11.111104
10.138179	631.008013	11.116122
9.906558	637.343275	11.121139
10.340248	629.174386	11.126157
10.386588	625.137169	11.131175
10.296716	624.703124	11.136192
10.255412	608.760200	11.141210
9.800161	615.313529	11.146227
10.016104	622.736839	11.151245
10.410869	629.166459	11.156263
10.438934	627.489486	11.161280
10.347785	621.274220	11.166298
9.941170	617.314286	11.171315
10.231302	621.882599	11.176333
10.481898	623.039380	11.181351
9.863375	620.428614	11.186368
10.215628	625.337488	11.191386
10.380489	623.591745	11.196403
10.652063	626.600848	11.201421
10.612164	614.899091	11.206439
10.296549	610.148574	11.211456
10.467164	606.511610	11.216474
9.984920	603.582850	11.221491
10.308948	606.391227	11.226509
10.107536	601.026375	11.231527
10.250983	617.322510	11.236544
10.511139	623.934164	11.241562
10.282911	633.311082	11.246579
10.045959	625.304076	11.251597
10.177768	628.761110	11.256615
10.158469	638.259929	11.261632
10.528697	626.023692	11.266650
10.509141	635.822351	11.271667
10.651654	625.351171	11.276685
10.927540	626.573417	11.281703
10.315502	627.657073	11.286720
10.093084	620.285263	11.291738
10.407983	633.657529	11.296755
10.393028	631.050023	11.301773
10.507257	630.347315	11.306791
10.663612	630.657328	11.311808
10.374261	628.509382	11.316826
10.517461	626.492478	11.321843
10.504365	628.713052	11.326861
10.596989	626.347468	11.331879
10.039260	637.199279	11.336896
10.345749	626.150141	11.341914
10.327765	634.512666	11.346931
10.770570	630.981372	11.351949
10.631393	633.849706	11.356967
10.569692	633.272392	11.361984
10.352219	630.327389	11.367002
10.577478	637.711376	11.372019
10.473617	627.004242	11.377037
10.915314	620.345729	11.382055
10.590944	633.316384	11.387072
10.834843	623.507817	11.392090
10.600195	624.781651	11.397107
10.767661	625.307674	11.402125
10.612557	629.257785	11.407143
10.537034	633.886548	11.412160
10.453823	624.403787	11.417178
10.501905	634.832474	11.422195
10.367011	625.929009	11.427213
10.581331	629.120652	11.432231
10.573130	632.877334	11.437248
10.947519	634.759488	11.442266
10.882080	631.828533	11.447283
10.788793	633.948064	11.452301
10.813368	625.360440	11.457319
10.405464	629.318602	11.462336
10.838291	629.288653	11.467354
11.110617	647.035224	11.472371
10.917921	641.334479	11.477389
10.678247	635.350762	11.482407
10.871255	631.375770	11.487424
10.761201	616.172601	11.492442
10.792044	632.445368	11.497459
10.941844	641.378053	11.502477
10.919414	635.981991	11.507495
10.877858	639.990053	11.512512
11.226552	635.779228	11.517530
11.177576	627.701743	11.522547
10.708120	624.837247	11.527565
10.636558	615.990136	11.532583
10.885623	627.902111	11.537600
11.135811	632.227378	11.542618
11.010212	627.598563	11.547635
10.590807	623.785798	11.552653
11.035240	625.546523	11.557671
10.819712	639.225962	11.562688
11.064496	644.741815	11.567706
11.349441	646.868357	11.572723
10.878942	643.950373	11.577741
11.140039	635.432983	11.582759
10.995681	644.815701	11.587776
10.982675	653.054378	11.592794
11.357944	642.919103	11.597811
11.060680	645.484005	11.602829
11.034082	634.534388	11.607847
11.143038	639.677045	11.612864
11.104324	632.872893	11.617882
10.733335	630.311704	11.622899
10.840223	643.864892	11.627917
11.219617	645.995571	11.632935
11.150457	650.932610	11.637952
11.090243	649.518775	11.642970
11.241595	646.159376	11.647987
10.906766	653.549073	11.653005
11.188831	653.526966	11.658023
10.837278	645.856643	11.663040
10.932190	641.477296	11.668058
11.106386	646.707564	11.673075
11.030842	646.463778	11.678093
11.227715	644.804535	11.683111
11.137804	644.872268	11.688128
11.057156	651.417410	11.693146
11.042670	648.083994	11.698163
11.272405	649.083099	11.703181
11.089863	649.143255	11.708199
11.328723	659.242265	11.713216
11.505362	667.706855	11.718234
11.418354	657.268462	11.723251
11.281229	662.443370	11.728269
11.460053	645.168889	11.733287
11.101837	646.121259	11.738304
11.427716	648.863081	11.743322
11.417066	657.303362	11.748339
11.421729	667.385422	11.753357
11.540673	658.751438	11.758375
11.470184	654.593664	11.763392
11.576257	645.844938	11.768410
11.554102	650.156075	11.773427
11.283678	646.051719	11.778445
11.750350	644.795172	11.783463
11.638055	648.602881	11.788480
11.619915	650.439241	11.793498
11.787261	644.155064	11.798515
11.613543	644.302200	11.803533
11.504035	639.544629	11.808551
11.484275	641.630550	11.813568
11.285571	641.961481	11.818586
11.233578	635.001618	11.823603
11.205642	646.388963	11.828621
11.655132	636.971054	11.833639
11.517213	645.014704	11.838656
11.409689	640.988967	11.843674
11.523760	642.315463	11.848691
11.413450	650.487333	11.853709
11.606694	648.393158	11.858727
11.584518	670.054908	11.863744
11.823178	663.888939	11.868762
11.452822	660.914236	11.873779
11.506727	660.766932	11.878797
11.717780	664.296763	11.883815
11.855002	665.477622	11.888832
11.766970	671.405390	11.893850
11.748006	663.992217	11.898867
11.926557	666.069160	11.903885
11.746788	656.308021	11.908903
11.389213	654.268590	11.913920
12.032404	660.902295	11.918938
11.604616	646.496808	11.923955
11.358795	656.652822	11.928973
11.730009	662.537035	11.933991
11.931593	664.279009	11.939008
11.547417	663.086345	11.944026
11.893600	663.259320	11.949043
11.866167	673.851341	11.954061
11.711774	666.547748	11.959079
11.642151	666.429266	11.964096
11.779806	670.377698	11.969114
11.835348	665.887749	11.974131
11.812594	673.534672	11.979149
11.793902	670.277650	11.984167
11.924222	669.449342	11.989184
11.541756	672.958560	11.994202
12.088117	669.174349	11.999219
12.022287	669.803198	12.004237
11.933078	661.416421	12.009255
11.794039	660.800730	12.014272
11.807179	668.031772	12.019290
12.231061	672.222536	12.024307
12.311796	670.985431	12.029325
11.971279	673.077430	12.034343
12.191524	667.201524	12.039360
12.003131	665.713096	12.044378
11.970563	662.429848	12.049395
12.062967	672.043728	12.054413
12.197389	663.653469	12.059431
12.054948	661.293152	12.064448
11.731058	672.016827	12.069466
12.393194	668.757275	12.074483
11.976040	665.991875	12.079501
12.030682	662.019621	12.084519
12.224191	665.593227	12.089536
12.514268	663.228258	12.094554
12.075675	658.465439	12.099571
12.164584	666.735491	12.104589
12.130089	661.748410	12.109607
12.539529	662.984447	12.114624
11.914642	669.883111	12.119642
12.135052	660.469523	12.124659
12.090314	667.637050	12.129677
12.050373	660.934065	12.134695
12.451014	660.962808	12.139712
11.864432	665.403409	12.144730
12.026220	667.883765	12.149747
11.963775	669.007546	12.154765
11.918501	665.492758	12.159783
11.969340	672.758920	12.164800
11.943220	686.711677	12.169818
12.370648	680.819083	12.174835
12.326767	695.459439	12.179853
12.227771	681.857633	12.184871
12.517122	690.986229	12.189888
12.553905	684.482653	12.194906
12.414531	679.622453	12.199923
12.612666	685.912489	12.204941
12.511413	679.386361	12.209959
12.664091	682.994771	12.214976
12.275873	684.112789	12.219994
12.558702	680.215232	12.225011
12.256464	685.886233	12.230029
12.428878	683.782694	12.235047
12.618533	681.603871	12.240064
12.464919	683.212152	12.245082
12.720121	682.856583	12.250099
12.520116	684.289095	12.255117
12.562695	675.809079	12.260135
12.512251	680.071007	12.265152
12.309611	683.782425	12.270170
12.599173	681.805699	12.275187
12.560175	691.809407	12.280205
12.339649	691.973344	12.285223
12.239306	687.690852	12.290240
12.505519	685.184452	12.295258
12.485968	690.912149	12.300275
12.451269	680.351937	12.305293
12.521707	683.894337	12.310311
12.356577	677.122598	12.315328
12.620529	685.336831	12.320346
12.739970	685.539021	12.325363
12.787338	687.781687	12.330381
12.563621	687.917722	12.335399
12.555606	687.240476	12.340416
12.683830	686.119006	12.345434
12.774255	689.648808	12.350451
12.531458	693.751529	12.355469
12.658736	694.949726	12.360487
12.785586	686.958275	12.365504
12.738229	683.762547	12.370522
12.762403	681.748507	12.375539
12.715068	691.330642	12.380557
12.778428	697.275724	12.385575
13.035032	690.911274	12.390592
12.693202	683.662289	12.395610
13.481179	696.698548	12.400627
13.171887	691.470492	12.405645
12.954135	695.061204	12.410663
13.081347	687.628273	12.415680
12.552035	698.046479	12.420698
12.886039	691.382723	12.425715
12.738013	688.865486	12.430733
12.719585	694.271116	12.435751
12.920353	682.260207	12.440768
12.543698	684.828086	12.445786
12.816886	699.144211	12.450803
12.895091	717.924816	12.455821
12.990674	712.207282	12.460839
13.101432	709.475927	12.465856
13.152275	704.768954	12.470874
13.387548	705.593625	12.475891
13.283894	705.581460	12.480909
13.038713	696.928770	12.485927
13.195435	685.183537	12.490944
12.998871	676.100360	12.495962
12.755098	686.429639	12.500979
13.095157	696.932537	12.505997
13.156427	703.212465	12.511015
13.397470	703.395602	12.516032
12.971777	700.394849	12.521050
13.362911	694.012475	12.526067
13.106739	694.734264	12.531085
12.877606	705.487294	12.536103
13.376247	700.347243	12.541120
13.166442	703.002591	12.546138
13.261494	706.679995	12.551155
13.299711	713.335924	12.556173
13.087167	700.739664	12.561191
13.319343	707.545082	12.566208
13.254016	708.448409	12.571226
13.263624	700.308064	12.576243
13.178698	699.166340	12.581261
13.488581	708.477921	12.586279
13.716005	709.616247	12.591296
13.628870	704.558507	12.596314
13.326191	686.744044	12.601331
13.176148	683.346654	12.606349
12.971099	691.448180	12.611367
13.232696	693.262806	12.616384
13.302103	712.757997	12.621402
13.547257	705.574824	12.626419
13.654015	704.005435	12.631437
13.166683	706.322413	12.636455
13.936846	699.643966	12.641472
13.534186	707.202103	12.646490
13.716562	701.846516	12.651507
13.623318	700.885977	12.656525
12.913834	683.151035	12.661543
13.255851	697.216533	12.666560
13.298970	696.632261	12.671578
13.434517	704.156564	12.676595
13.566276	697.035343	12.681613
13.423611	695.975250	12.686631
13.405076	698.603785	12.691648
13.403182	697.651024	12.696666
13.353203	699.486066	12.701683
13.509330	703.674608	12.706701
13.704483	709.734746	12.711719
13.726614	694.283581	12.716736
13.727023	708.598271	12.721754
13.750848	704.719199	12.726771
13.688277	699.682858	12.731789
13.853130	706.293696	12.736807
13.835754	705.961900	12.741824
13.783989	702.820508	12.746842
13.555096	700.483198	12.751859
13.864251	700.781895	12.756877
13.443405	711.590214	12.761895
13.847975	705.477131	12.766912
13.472319	703.049206	12.771930
13.781558	698.263880	12.776947
13.686060	713.350996	12.781965
13.470645	706.924796	12.786983
13.835239	719.219520	12.792000
13.974981	728.826013	12.797018
14.099628	721.396627	12.802035
13.949825	716.020497	12.807053
13.650524	707.691862	12.812071
13.965944	699.948571	12.817088
13.815868	708.155101	12.822106
13.814047	717.742743	12.827123
14.069642	724.724380	12.832141
14.121076	725.246495	12.837159
14.205117	710.558791	12.842176
13.852062	711.437772	12.847194
13.766478	709.261044	12.852211
13.972514	710.222840	12.857229
14.154723	718.238456	12.862247
14.002937	718.110756	12.867264
13.990534	722.578173	12.872282
14.408008	727.413741	12.877299
14.377276	713.192143	12.882317
13.703926	714.215982	12.887335
14.171338	705.934477	12.892352
13.876910	711.793611	12.897370
14.251819	728.675278	12.902387
14.562442	728.175325	12.907405
14.061427	721.525623	12.912423
14.194758	710.831769	12.917440
13.758395	715.491843	12.922458
13.980597	727.288174	12.927475
14.181325	733.950206	12.932493
14.254246	736.589664	12.937511
14.264587	734.246425	12.942528
14.148942	735.990773	12.947546
14.184456	738.863311	12.952563
14.328688	739.916843	12.957581
14.092019	737.744849	12.962599
14.275283	729.545723	12.967616
14.431961	738.190200	12.972634
14.213528	730.319101	12.977651
14.354759	732.247264	12.982669
13.904449	733.173042	12.987687
14.189405	736.779672	12.992704
14.477287	731.972436	12.997722
14.448939	729.221847	13.002739
14.293094	731.657306	13.007757
14.252484	740.610407	13.012775
14.434299	733.812689	13.017792
14.205848	734.009426	13.022810
14.091590	726.355537	13.027827
14.396390	731.518029	13.032845
14.485529	750.442123	13.037863
14.744808	750.272107	13.042880
14.599149	737.248773	13.047898
14.400682	741.158366	13.052915
14.552305	734.485300	13.057933
14.628962	749.311942	13.062951
15.009126	746.282749	13.067968
14.673741	726.349505	13.072986
14.430115	722.064208	13.078003
14.576769	712.078323	13.083021
14.565399	723.453654	13.088039
14.171772	724.484160	13.093056
14.792275	738.259904	13.098074
14.843899	739.258518	13.103091
14.994739	738.638432	13.108109
14.653036	734.119189	13.113127
14.607255	721.357929	13.118144
14.542941	730.280025	13.123162
14.743763	739.532970	13.128179
15.463578	735.690010	13.133197
15.157502	729.366370	13.138215
15.008714	721.320260	13.143232
14.727065	711.019629	13.148250
14.884133	719.099145	13.153267
15.193445	705.837291	13.158285
14.941352	710.790385	13.163303
15.050803	716.018195	13.168320
15.102630	715.328416	13.173338
14.811989	708.052465	13.178355
14.814203	704.441867	13.183373
14.691724	715.364385	13.188391
14.921681	700.754813	13.193408
15.033871	703.710006	13.198426
14.689902	702.012421	13.203443
14.809565	700.491503	13.208461
14.791109	704.243495	13.213479
14.901107	710.512635	13.218496
15.245760	705.636551	13.223514
14.904608	704.929449	13.228531
14.891195	703.937467	13.233549
14.853082	709.178928	13.238567
15.149770	709.624746	13.243584
14.976680	711.075134	13.248602
14.789888	709.157262	13.253619
15.272460	719.284393	13.258637
15.119209	732.556513	13.263655
14.964180	735.496775	13.268672
15.407786	731.665534	13.273690
15.234069	739.285645	13.278707
15.255540	726.864140	13.283725
15.320155	730.940795	13.288743
15.286625	720.178404	13.293760
15.005010	718.998069	13.298778
14.562848	721.787655	13.303795
15.292100	730.910464	13.308813
15.588879	738.015043	13.313831
15.277960	736.889790	13.318848
15.218127	739.840384	13.323866
15.309862	749.299775	13.328883
15.595033	729.401843	13.333901
15.279892	737.148253	13.338919
15.327006	734.985445	13.343936
15.629900	744.178218	13.348954
15.100961	748.493043	13.353971
15.829790	731.113368	13.358989
15.328851	735.202895	13.364007
15.479013	740.853524	13.369024
15.780019	730.531020	13.374042
15.566126	739.432375	13.379059
15.389814	725.741663	13.384077
15.503883	731.136011	13.389095
15.573555	733.649745	13.394112
15.990781	738.561095	13.399130
15.694377	727.208723	13.404147
15.339167	710.380770	13.409165
15.442700	704.365347	13.414183
15.119321	710.636116	13.419200
15.534538	726.829810	13.424218
15.624716	741.540719	13.429235
15.865742	728.516766	13.434253
15.521945	736.943010	13.439271
15.772465	732.924270	13.444288
16.015530	736.335492	13.449306
15.623457	736.176012	13.454323
15.979548	728.300103	13.459341
15.562950	726.544467	13.464359
15.796430	716.857402	13.469376
15.409455	720.607177	13.474394
15.717633	730.985702	13.479411
15.692878	725.110293	13.484429
15.758014	737.975815	13.489447
15.787417	736.402764	13.494464
15.909653	732.088542	13.499482
15.389756	737.124629	13.504499
15.543803	731.587278	13.509517
15.411337	737.907040	13.514535
15.584786	739.082228	13.519552
15.738217	729.436100	13.524570
15.608544	733.375938	13.529587
15.830179	740.539628	13.534605
15.571477	748.024734	13.539623
16.183880	749.803337	13.544640
16.066031	748.045072	13.549658
16.115830	753.547327	13.554675
16.123734	750.952002	13.559693
16.155210	745.017283	13.564711
15.899873	744.489239	13.569728
16.172050	744.172035	13.574746
16.167874	746.716277	13.579763
16.088349	736.693232	13.584781
16.154007	737.617064	13.589799
16.012160	742.183663	13.594816
16.269346	742.357960	13.599834
15.934755	739.636417	13.604851
16.098932	744.612662	13.609869
16.019844	747.392703	13.614887
16.114150	752.566092	13.619904
16.169161	748.713681	13.624922
16.075724	754.762246	13.629939
16.056606	758.340783	13.634957
15.999856	754.695231	13.639975
16.160093	750.027911	13.644992
16.565883	755.376560	13.650010
16.255191	758.495850	13.655027
16.254504	756.839149	13.660045
16.397283	757.384823	13.665063
16.061853	755.487078	13.670080
16.242805	752.769964	13.675098
16.327751	762.558631	13.680115
16.589833	751.658386	13.685133
16.536214	752.010769	13.690151
16.047353	750.531542	13.695168
16.207988	757.461798	13.700186
16.099634	763.212899	13.705203
16.068259	752.841473	13.710221
16.404326	769.842874	13.715239
16.432172	777.368303	13.720256
16.877969	770.444004	13.725274
16.789135	773.910390	13.730291
16.584055	773.519639	13.735309
16.379361	769.149334	13.740327
16.686742	773.860152	13.745344
16.950928	767.513421	13.750362
16.764028	760.678789	13.755379
16.513566	754.460036	13.760397
16.512182	748.000287	13.765415
16.550922	759.595009	13.770432
16.738997	761.010905	13.775450
16.548693	768.037176	13.780467
16.479531	775.754530	13.785485
16.816626	768.263435	13.790503
16.784744	780.702373	13.795520
17.012756	776.611411	13.800538
17.044837	772.459629	13.805555
16.957662	765.555721	13.810573
16.902273	749.144661	13.815591
16.677184	744.108524	13.820608
16.749905	732.830859	13.825626
16.563289	753.849442	13.830643
16.666571	757.099531	13.835661
17.022942	765.122594	13.840679
16.839508	775.931624	13.845696
16.615608	759.540645	13.850714
16.586883	768.870596	13.855731
16.750341	769.087981	13.860749
16.840013	766.861697	13.865767
17.080367	766.082417	13.870784
17.266133	766.775991	13.875802
17.128117	770.518328	13.880819
17.116958	768.222634	13.885837
17.403702	771.469227	13.890855
16.985562	768.943808	13.895872
16.951171	765.670293	13.900890
17.037898	775.531273	13.905907
17.389849	776.798416	13.910925
17.396555	766.553560	13.915943
17.277149	774.105215	13.920960
17.480271	767.225251	13.925978
17.346650	775.426078	13.930995
17.422998	766.726131	13.936013
17.035387	752.721364	13.941031
16.869281	767.765940	13.946048
17.214952	771.120066	13.951066
17.432994	770.729292	13.956083
17.128353	770.931656	13.961101
17.502456	768.496704	13.966119
17.293936	779.256016	13.971136
17.563393	769.850465	13.976154
17.507376	777.988641	13.981171
17.401048	767.291277	13.986189
17.882601	760.023706	13.991207
17.270003	757.052227	13.996224
17.216191	747.104044	14.001242
17.340652	765.053782	14.006259
17.117777	771.400345	14.011277
17.330220	768.103935	14.016295
17.309805	767.652692	14.021312
17.419538	767.831157	14.026330
17.575130	776.942885	14.031347
17.577040	776.503923	14.036365
17.291157	773.809457	14.041383
17.444789	781.072182	14.046400
17.860100	771.015769	14.051418
17.319527	771.021567	14.056435
17.158077	772.053568	14.061453
17.252086	768.204510	14.066471
17.543831	782.820755	14.071488
17.451063	772.569390	14.076506
17.582286	786.825778	14.081523
17.505836	792.663409	14.086541
17.881838	787.498367	14.091559
17.565247	793.862776	14.096576
17.715324	798.620338	14.101594
17.716177	792.387442	14.106611
18.002212	797.054274	14.111629
17.952940	792.129432	14.116647
17.804943	798.095041	14.121664
18.028169	794.389835	14.126682
17.847792	798.441774	14.131699
17.866698	797.776085	14.136717
17.936785	790.699203	14.141735
17.859949	795.170423	14.146752
17.887148	785.824911	14.151770
18.013254	794.714048	14.156787
17.821168	802.097221	14.161805
18.330992	791.072928	14.166823
17.879776	794.005957	14.171840
18.035301	787.010365	14.176858
18.009986	793.367007	14.181875
18.046805	796.835801	14.186893
18.278280	799.286323	14.191911
18.118192	797.806073	14.196928
17.943987	791.010466	14.201946
18.005626	785.228799	14.206963
17.789819	793.679198	14.211981
18.095047	786.458178	14.216999
17.881394	795.302718	14.222016
18.027615	793.881774	14.227034
17.803868	791.714060	14.232051
17.606385	797.494916	14.237069
18.282145	794.166935	14.242087
18.168413	793.361081	14.247104
18.370612	790.467063	14.252122
18.359188	782.932737	14.257139
18.045951	789.211412	14.262157
18.249554	783.723086	14.267175
18.375653	810.578355	14.272192
18.511350	804.775611	14.277210
18.330290	807.628444	14.282227
18.055185	801.539769	14.287245
18.403165	802.416214	14.292263
18.871358	813.325141	14.297280
18.823052	806.894814	14.302298
18.300191	796.044942	14.307315
18.398729	793.612137	14.312333
18.525846	782.957082	14.317351
18.472045	800.126895	14.322368
18.476345	801.319122	14.327386
18.567560	801.778201	14.332403
18.735321	810.701846	14.337421
18.969280	800.064756	14.342439
18.408751	792.534408	14.347456
18.120358	791.011145	14.352474
18.419033	799.248393	14.357491
18.337338	821.131092	14.362509
18.591275	812.422234	14.367527
18.361006	820.303706	14.372544
18.474134	815.189310	14.377562
18.840487	816.719290	14.382579
18.458234	821.269927	14.387597
19.015633	818.317095	14.392615
18.627792	814.808614	14.397632
18.802286	809.413204	14.402650
18.671055	808.130404	14.407667
18.741869	809.428976	14.412685
18.993360	804.330774	14.417703
18.926972	817.396843	14.422720
18.989127	803.959044	14.427738
18.750756	803.898558	14.432755
19.001005	821.371050	14.437773
19.045408	811.596792	14.442791
19.001927	814.964561	14.447808
19.052620	809.705314	14.452826
18.950243	805.208515	14.457843
18.804688	804.152024	14.462861
18.860815	806.402801	14.467879
19.406971	823.585933	14.472896
19.111470	819.179350	14.477914
19.297410	807.347407	14.482931
19.153598	816.695416	14.487949
19.048814	805.259322	14.492967
18.974490	811.115561	14.497984
19.000810	809.726025	14.503002
19.348588	819.344154	14.508019
19.021918	819.149178	14.513037
19.334380	815.202767	14.518055
19.326877	834.015858	14.523072
19.099677	824.221032	14.528090
19.652913	816.774948	14.533107
19.341719	812.979901	14.538125
19.416649	808.613112	14.543143
19.132599	810.794111	14.548160
19.549209	805.840453	14.553178
19.645263	799.829326	14.558195
19.179745	808.492426	14.563213
19.556600	802.270043	14.568231
19.317187	801.726879	14.573248
19.245016	801.996962	14.578266
19.516705	813.776129	14.583283
19.593394	820.848952	14.588301
19.861937	817.764652	14.593319
19.564152	811.941460	14.598336
19.237063	814.933939	14.603354
19.445092	804.442922	14.608371
19.477887	829.851690	14.613389
19.808313	833.785734	14.618407
19.579589	825.540661	14.623424
19.597324	828.712647	14.628442
19.948329	827.818197	14.633459
19.860468	819.718315	14.638477
19.723579	805.175602	14.643495
19.841966	810.701843	14.648512
19.605398	809.167302	14.653530
19.740598	807.353604	14.658547
19.529648	815.061632	14.663565
19.726383	823.526304	14.668583
19.887693	827.830829	14.673600
19.840879	837.649649	14.678618
20.039136	830.461151	14.683635
19.707109	837.130955	14.688653
19.976631	833.585747	14.693671
19.587891	835.931476	14.698688
19.766436	827.991822	14.703706
19.626296	825.934083	14.708723
19.766729	831.390603	14.713741
19.849555	839.011587	14.718759
19.881187	837.255139	14.723776
19.660653	829.513714	14.728794
19.789866	828.559339	14.733811
19.637139	835.434581	14.738829
20.127064	836.863150	14.743847
20.148831	856.334404	14.748864
20.495723	845.717462	14.753882
20.367929	842.474348	14.758899
20.227343	838.955524	14.763917
20.210293	829.635858	14.768935
20.412044	831.917471	14.773952
20.231188	826.877536	14.778970
20.279290	830.221491	14.783987
20.171018	834.306322	14.789005
20.177810	832.225560	14.794023
20.277164	826.665191	14.799040
20.131905	832.920718	14.804058
20.677926	824.525856	14.809075
20.172628	828.546658	14.814093
20.428219	822.516838	14.819111
20.510366	827.010494	14.824128
20.220543	824.493364	14.829146
20.192762	828.729686	14.834163
20.519991	843.548706	14.839181
20.529534	843.228468	14.844199
20.978358	844.590893	14.849216
20.496919	835.937281	14.854234
20.648559	823.255471	14.859251
20.481663	828.334105	14.864269
20.593812	822.187904	14.869287
20.764514	822.883841	14.874304
20.359371	827.046742	14.879322
20.492885	812.789863	14.884339
20.445443	826.215890	14.889357
20.813490	836.547226	14.894375
20.975794	831.172655	14.899392
20.564169	836.116064	14.904410
20.716981	823.654979	14.909427
20.649345	820.408754	14.914445
20.675587	839.263901	14.919463
20.799447	839.828321	14.924480
20.512989	855.797553	14.929498
20.934561	837.506542	14.934515
20.904179	849.295191	14.939533
20.659527	843.198574	14.944551
21.104652	846.186834	14.949568
20.738221	849.857676	14.954586
21.064401	847.329236	14.959603
20.712162	856.807752	14.964621
20.935453	847.210576	14.969639
20.846647	844.418949	14.974656
20.556937	851.505009	14.979674
20.857906	848.324105	14.984691
20.749522	844.939091	14.989709
20.757700	843.290460	14.994727
20.868872	847.861625	14.999744
21.094930	869.058686	15.004762
21.242554	861.202759	15.009779
21.477623	871.431873	15.014797
20.896371	864.087781	15.019815
21.386681	868.173509	15.024832
21.362415	876.704391	15.029850
21.395810	865.224518	15.034867
21.030651	847.331320	15.039885
21.324587	852.019019	15.044903
21.236206	867.610084	15.049920
21.482798	868.470860	15.054938
21.367985	869.823766	15.059955
21.366193	866.958541	15.064973
21.462811	868.581281	15.069991
21.597549	866.837078	15.075008
21.241532	855.661225	15.080026
21.646408	848.541333	15.085043
21.563882	855.841089	15.090061
21.280891	845.641577	15.095079
21.273766	843.824929	15.100096
21.398733	854.784503	15.105114
21.352374	857.496317	15.110131
21.344606	867.864464	15.115149
21.503643	865.179170	15.120167
21.549177	863.401606	15.125184
21.375908	866.906486	15.130202
21.446573	859.958877	15.135219
21.644151	861.183941	15.140237
21.262057	868.824132	15.145255
21.215377	859.995091	15.150272
21.447560	875.356055	15.155290
21.836946	879.555430	15.160307
22.109468	889.889141	15.165325
21.666257	893.890762	15.170343
22.207035	888.081328	15.175360
22.032656	877.564976	15.180378
21.979951	865.827190	15.185395
21.782689	860.474232	15.190413
21.525173	859.801357	15.195431
22.199230	863.539555	15.200448
22.040070	869.172417	15.205466
21.879439	856.804600	15.210483
21.814172	867.197535	15.215501
22.051947	872.657752	15.220519
22.132617	873.481407	15.225536
21.947828	876.517874	15.230554
22.296137	869.271136	15.235571
22.319850	873.310050	15.240589
21.807608	872.191085	15.245607
22.197256	868.816399	15.250624
22.087611	881.841955	15.255642
22.255151	876.043666	15.260659
22.665708	882.354139	15.265677
21.961575	875.218645	15.270695
22.466449	871.125309	15.275712
22.594290	868.643720	15.280730
22.200378	859.313656	15.285747
22.593769	856.361269	15.290765
22.085359	864.885948	15.295783
22.056223	857.297561	15.300800
21.981335	870.478611	15.305818
22.543003	869.693165	15.310835
22.842527	870.050180	15.315853
22.427752	872.737668	15.320871
22.662665	877.298920	15.325888
22.419411	871.606022	15.330906
22.208766	870.364063	15.335923
22.653081	872.844364	15.340941
22.543682	890.935014	15.345959
23.196451	884.044515	15.350976
22.560415	877.908221	15.355994
22.510641	863.727356	15.361011
22.422603	861.109177	15.366029
22.341979	877.854073	15.371047
22.909101	871.077985	15.376064
22.959662	878.694574	15.381082
22.698817	871.426511	15.386099
23.060104	879.685544	15.391117
22.792996	882.378300	15.396135
23.018061	877.785997	15.401152
22.457698	875.241819	15.406170
22.964387	877.349427	15.411187
22.943327	881.177604	15.416205
22.853525	883.154606	15.421223
22.784946	871.965264	15.426240
22.702240	880.265460	15.431258
22.528772	886.089920	15.436275
22.767574	882.659970	15.441293
22.788040	886.352253	15.446311
22.820237	879.407507	15.451328
22.964976	879.034527	15.456346
22.805587	878.286316	15.461363
22.807597	877.004726	15.466381
22.822373	876.052500	15.471399
23.114427	884.937773	15.476416
23.258208	905.926859	15.481434
23.264378	908.721970	15.486451
23.159725	900.223890	15.491469
23.218688	905.996159	15.496487
23.477875	895.348748	15.501504
23.051725	893.215890	15.506522
23.058136	889.118597	15.511539
23.061940	899.421832	15.516557
23.351506	904.523645	15.521575
23.469856	894.740912	15.526592
23.489942	901.759518	15.531610
23.481045	900.280817	15.536627
23.483699	896.644864	15.541645
23.313262	905.810896	15.546663
23.609728	900.958089	15.551680
23.621953	903.395639	15.556698
23.432889	898.953425	15.561715
23.616710	892.221605	15.566733
23.699272	898.880124	15.571751
24.112449	893.119084	15.576768
23.355566	883.123189	15.581786
23.456308	892.101556	15.586803
23.455904	887.314201	15.591821
23.440549	896.402280	15.596839
23.954943	888.877045	15.601856
23.803316	894.186838	15.606874
23.460399	904.029997	15.611891
23.468612	896.543041	15.616909
23.392769	901.373897	15.621927
23.329478	897.558925	15.626944
23.336447	903.670704	15.631962
23.309479	900.935652	15.636979
24.099026	911.349317	15.641997
23.559218	924.319223	15.647015
24.024224	919.616731	15.652032
24.186574	926.549941	15.657050
23.818810	918.556985	15.662067
23.685236	920.244199	15.667085
23.727525	923.459693	15.672103
24.055969	922.398358	15.677120
23.845661	918.770520	15.682138
23.906706	918.880875	15.687155
24.190427	912.379552	15.692173
23.766863	914.689721	15.697191
24.360838	915.549721	15.702208
24.025458	907.968268	15.707226
23.958836	916.796143	15.712243
24.111169	931.797276	15.717261
24.426215	940.862014	15.722279
24.568983	934.389079	15.727296
24.207083	923.854742	15.732314
24.364912	923.804764	15.737331
24.341186	926.980108	15.742349
24.513769	933.324729	15.747367
24.379180	919.302277	15.752384
24.243490	925.862456	15.757402
24.506767	935.459173	15.762419
24.713137	937.273010	15.767437
24.801151	942.217062	15.772455
24.785057	917.092693	15.777472
24.781009	912.542590	15.782490
24.516557	921.887464	15.787507
24.782331	919.226465	15.792525
24.401397	918.976873	15.797543
24.345538	910.767792	15.802560
24.961987	914.552898	15.807578
24.606371	906.195122	15.812595
24.876986	907.743266	15.817613
24.520017	915.341670	15.822631
24.827804	904.733976	15.827648
24.580816	906.931270	15.832666
24.226278	918.644520	15.837683
24.938020	929.736270	15.842701
24.812698	929.023745	15.847719
24.879130	933.106473	15.852736
25.370187	938.284026	15.857754
24.984187	947.310281	15.862771
25.035616	933.956117	15.867789
24.943407	929.419823	15.872807
24.842212	925.329913	15.877824
25.021024	927.122820	15.882842
24.707828	931.590080	15.887859
25.200023	922.307344	15.892877
25.061376	934.138258	15.897895
24.980106	928.880716	15.902912
25.271795	943.418206	15.907930
25.267049	940.903731	15.912947
25.644158	925.223176	15.917965
25.449832	937.069128	15.922983
25.415735	927.436497	15.928000
25.390445	912.156677	15.933018
24.870178	914.033866	15.938035
25.081894	914.559277	15.943053
25.223359	921.590432	15.948071
25.234316	929.771833	15.953088
25.383905	929.104599	15.958106
25.282678	929.353989	15.963123
25.313865	923.573893	15.968141
25.153637	938.605069	15.973159
25.380821	928.710589	15.978176
25.559921	924.371633	15.983194
25.090607	932.905998	15.988211
25.600520	937.556725	15.993229
25.704990	932.241678	15.998247
25.358497	934.486124	16.003264
25.576916	926.735843	16.008282
25.836429	932.965856	16.013299
25.851899	930.410346	16.018317
25.377833	940.968360	16.023335
25.674619	944.030373	16.028352
25.778049	956.397739	16.033370
26.051825	964.235015	16.038387
25.896616	942.297732	16.043405
26.107038	939.856845	16.048423
25.664883	934.034141	16.053440
25.699310	935.237436	16.058458
25.938926	953.267153	16.063475
25.829021	950.355737	16.068493
25.804444	951.599835	16.073511
25.792158	957.541078	16.078528
26.091618	952.479501	16.083546
25.807791	964.238506	16.088563
25.852546	949.061291	16.093581
25.833766	962.006395	16.098599
25.785085	951.621786	16.103616
26.068868	962.098944	16.108634
25.783045	956.267519	16.113651
26.044407	952.389045	16.118669
26.190796	958.336985	16.123687
26.429241	971.443770	16.128704
26.991812	970.159553	16.133722
26.372283	960.691213	16.138739
26.381370	956.369419	16.143757
26.181180	952.373910	16.148775
25.997065	947.432282	16.153792
26.275049	956.471276	16.158810
26.464711	970.333641	16.163827
26.561573	972.969383	16.168845
26.489785	966.056674	16.173863
26.236206	974.165932	16.178880
26.911903	968.246970	16.183898
26.803248	970.526741	16.188915
26.354115	953.438713	16.193933
26.489669	957.977684	16.198951
26.428718	962.941926	16.203968
26.605681	967.367111	16.208986
26.563511	971.315382	16.214003
26.891669	972.971283	16.219021
27.162995	971.395022	16.224039
26.798475	978.057345	16.229056
26.935007	959.056619	16.234074
26.713721	955.578819	16.239091
26.660650	955.896405	16.244109
26.904313	966.689126	16.249127
26.704326	974.042049	16.254144
27.365860	973.370343	16.259162
26.715524	968.025222	16.264179
26.773893	964.942268	16.269197
27.260589	969.019119	16.274215
27.134605	967.489329	16.279232
27.083618	969.409765	16.284250
26.720532	964.657122	16.289267
26.925448	960.834829	16.294285
27.104478	962.835991	16.299303
27.029486	966.606364	16.304320
26.884456	963.845618	16.309338
26.749760	962.856845	16.314355
26.756319	953.760636	16.319373
27.177798	959.832736	16.324391
26.876245	961.950223	16.329408
27.274192	976.190219	16.334426
27.199562	989.920436	16.339443
27.281844	991.157262	16.344461
27.409350	985.507225	16.349479
27.018649	983.624426	16.354496
26.998163	981.601570	16.359514
26.883376	985.674833	16.364531
27.295194	992.262863	16.369549
27.622392	1000.117032	16.374567
27.667508	1012.641900	16.379584
27.951613	994.911920	16.384602
27.879125	985.335765	16.389619
27.844678	978.751723	16.394637
27.946739	986.593822	16.399655
27.851009	987.170561	16.404672
28.011920	976.046185	16.409690
28.054673	978.336950	16.414707
27.955315	985.958138	16.419725
27.943473	977.975663	16.424743
27.795347	975.849728	16.429760
28.180059	977.455743	16.434778
28.072989	979.769982	16.439795
28.049330	974.689595	16.444813
28.182628	977.758294	16.449831
28.139165	971.683760	16.454848
28.100568	978.528551	16.459866
28.141156	968.906286	16.464883
27.950296	957.360503	16.469901
28.014776	963.428577	16.474919
27.554339	976.849996	16.479936
27.908738	981.805972	16.484954
28.154442	974.628918	16.489971
28.022982	978.919390	16.494989
28.407519	970.404591	16.500007
28.107931	972.221964	16.505024
28.622088	970.109030	16.510042
28.055884	967.032414	16.515059
28.371794	979.300232	16.520077
28.086499	973.901071	16.525095
28.006024	979.016702	16.530112
28.248687	972.578595	16.535130
28.237414	981.195856	16.540147
28.079586	973.895830	16.545165
28.124574	980.907411	16.550183
28.440340	991.111327	16.555200
28.511654	991.844934	16.560218
28.392342	991.715300	16.565235
28.564433	999.477003	16.570253
28.841191	998.581555	16.575271
28.498471	1000.320480	16.580288
28.390064	990.134558	16.585306
28.529949	999.905280	16.590323
28.657076	1003.991138	16.595341
28.685327	1000.878183	16.600359
28.503068	1002.049158	16.605376
28.692173	1005.917019	16.610394
28.770338	996.796946	16.615411
28.584655	1000.325888	16.620429
28.670092	1004.017484	16.625447
28.869199	1017.158868	16.630464
28.837407	1018.088515	16.635482
29.066053	1022.802268	16.640499
29.171158	1023.915598	16.645517
29.075490	1022.658770	16.650535
29.495255	1021.270690	16.655552
29.503309	1008.330373	16.660570
29.205640	994.762611	16.665587
28.950111	991.163935	16.670605
29.004536	992.764894	16.675623
29.111734	1011.705371	16.680640
29.083340	1017.377753	16.685658
29.082113	1017.655658	16.690675
29.337924	1023.179370	16.695693
29.305975	1021.644309	16.700711
28.939658	1013.941423	16.705728
29.347852	1012.826562	16.710746
29.203239	1022.051724	16.715763
29.224203	1013.852650	16.720781
29.617663	1011.859610	16.725799
29.561648	1010.583946	16.730816
29.671927	1017.591623	16.735834
29.841108	1021.131243	16.740851
29.261140	1007.961158	16.745869
30.024034	1009.539482	16.750887
30.030841	1020.464022	16.755904
29.949082	1018.529659	16.760922
29.772730	1008.098746	16.765939
29.336993	1018.912738	16.770957
29.648344	1021.495946	16.775975
29.629778	1019.053055	16.780992
29.790993	1021.000210	16.786010
29.731373	1014.325422	16.791027
29.765257	1019.823942	16.796045
29.784672	1009.378135	16.801063
29.828226	1018.403397	16.806080
29.973141	1023.673079	16.811098
29.522388	1024.769357	16.816115
29.794771	1031.129935	16.821133
29.861941	1033.101294	16.826151
29.694957	1040.262876	16.831168
29.798417	1029.920656	16.836186
29.909203	1035.915227	16.841203
29.961326	1027.802785	16.846221
30.269532	1026.845603	16.851239
30.039179	1043.844492	16.856256
30.389448	1043.606569	16.861274
30.105860	1042.909369	16.866291
30.312666	1056.898505	16.871309
30.456025	1048.825409	16.876327
30.286031	1062.220320	16.881344
30.684008	1058.250991	16.886362
30.563181	1049.181004	16.891379
30.534695	1041.358902	16.896397
30.355158	1031.739533	16.901415
30.488516	1045.591843	16.906432
30.597149	1049.267190	16.911450
30.797797	1050.356085	16.916467
30.777193	1041.516557	16.921485
30.738576	1031.303897	16.926503
30.625182	1036.219570	16.931520
30.602411	1036.201043	16.936538
30.872141	1036.543796	16.941555
30.378806	1048.856401	16.946573
30.748435	1054.138222	16.951591
30.805250	1057.584999	16.956608
30.854009	1055.772196	16.961626
30.925128	1057.967006	16.966643
30.567282	1062.381333	16.971661
30.659288	1049.301598	16.976679
30.714601	1048.488181	16.981696
30.867756	1052.664648	16.986714
31.138000	1048.989894	16.991731
30.827325	1060.787884	16.996749
30.616881	1050.576888	17.001767
31.131192	1059.926053	17.006784
30.972738	1079.305864	17.011802
31.135845	1072.129088	17.016819
31.473112	1076.314586	17.021837
31.399108	1073.829879	17.026855
31.372695	1076.608030	17.031872
31.494360	1077.087593	17.036890
31.549713	1066.576161	17.041907
31.351438	1068.144135	17.046925
31.449848	1056.575056	17.051943
31.897515	1071.842466	17.056960
31.438299	1066.988090	17.061978
31.330363	1050.300956	17.066995
31.260064	1057.930246	17.072013
31.511721	1071.767197	17.077031
31.795574	1067.162479	17.082048
31.589983	1082.292403	17.087066
31.689388	1075.788341	17.092083
31.589602	1075.712452	17.097101
31.899462	1074.231133	17.102119
31.770890	1080.648238	17.107136
31.351598	1076.090568	17.112154
31.300425	1063.847472	17.117171
31.129249	1073.193590	17.122189
31.426646	1075.479184	17.127207
32.102008	1077.320543	17.132224
31.864208	1090.615644	17.137242
32.527203	1093.683423	17.142259
32.200090	1078.728467	17.147277
32.077396	1067.620066	17.152295
32.033459	1068.472722	17.157312
31.941589	1069.875699	17.162330
32.325752	1061.483995	17.167347
32.489385	1064.797270	17.172365
32.281477	1068.105640	17.177383
32.190596	1063.468116	17.182400
31.992936	1064.445844	17.187418
32.180223	1058.492921	17.192435
32.032070	1080.563080	17.197453
32.132572	1088.108816	17.202471
32.264220	1098.329018	17.207488
32.205510	1100.733528	17.212506
32.623593	1086.693782	17.217523
32.267560	1089.611944	17.222541
32.465137	1095.349934	17.227559
32.342784	1093.390364	17.232576
32.404076	1091.944833	17.237594
32.674297	1085.540239	17.242611
32.356785	1084.507517	17.247629
32.933711	1087.462545	17.252647
32.862822	1092.851268	17.257664
32.517524	1092.252098	17.262682
32.993737	1088.687080	17.267699
33.015840	1091.460788	17.272717
32.955938	1091.545912	17.277735
33.121062	1090.809964	17.282752
32.611831	1088.311393	17.287770
32.511208	1086.490434	17.292787
32.579976	1094.883764	17.297805
32.663883	1089.455125	17.302823
32.808441	1093.519337	17.307840
32.944107	1117.078831	17.312858
33.243643	1108.252229	17.317875
33.124717	1105.635697	17.322893
33.155630	1107.458107	17.327911
32.712192	1108.228187	17.332928
32.405323	1107.282161	17.337946
32.953817	1105.978050	17.342963
32.812616	1110.939127	17.347981
32.826788	1116.323997	17.352999
33.407988	1129.112101	17.358016
33.524557	1135.298308	17.363034
33.584058	1140.000724	17.368051
33.591088	1133.170278	17.373069
33.488660	1130.254504	17.378087
33.906563	1133.890880	17.383104
33.844529	1124.562329	17.388122
34.168685	1103.685859	17.393139
33.671105	1104.593813	17.398157
33.307642	1106.768354	17.403175
33.615094	1097.713293	17.408192
33.354710	1102.102891	17.413210
33.703679	1107.470018	17.418227
33.460998	1116.846298	17.423245
34.098091	1127.489110	17.428263
33.861812	1124.916209	17.433280
33.686344	1135.361280	17.438298
34.094280	1128.158746	17.443315
34.307653	1128.169495	17.448333
34.360188	1122.439639	17.453351
34.336815	1107.383420	17.458368
33.725744	1107.236155	17.463386
33.875568	1104.403942	17.468403
34.289902	1115.179481	17.473421
34.385804	1122.950020	17.478439
34.191999	1105.313744	17.483456
33.977714	1098.716807	17.488474
34.086181	1105.933091	17.493491
33.992719	1128.471279	17.498509
34.325995	1121.627592	17.503527
34.228833	1127.200327	17.508544
34.054463	1121.130473	17.513562
34.403783	1116.607006	17.518579
34.514042	1128.790382	17.523597
34.047577	1131.369237	17.528615
34.137049	1129.344916	17.533632
34.369618	1121.311460	17.538650
34.427496	1113.444236	17.543667
34.601750	1126.081498	17.548685
34.536330	1143.613233	17.553703
34.861369	1141.918085	17.558720
34.536577	1149.240139	17.563738
34.902256	1143.631632	17.568755
34.768137	1147.461801	17.573773
34.838774	1143.998188	17.578791
34.815261	1139.479480	17.583808
34.797789	1144.679964	17.588826
35.071085	1140.894257	17.593843
34.836704	1148.628191	17.598861
35.036692	1146.343549	17.603879
35.116322	1143.487613	17.608896
35.010535	1153.700865	17.613914
34.913223	1145.040567	17.618931
35.156057	1138.917963	17.623949
34.680901	1138.358073	17.628967
35.164813	1135.650241	17.633984
35.021244	1138.503564	17.639002
35.333019	1146.880936	17.644019
34.826843	1145.101421	17.649037
35.022820	1145.067557	17.654055
35.248894	1144.255784	17.659072
35.217435	1158.193967	17.664090
35.449221	1157.072021	17.669107
35.519383	1163.748361	17.674125
35.350689	1163.635929	17.679143
35.579696	1154.608910	17.684160
35.485336	1159.919277	17.689178
35.427020	1151.060357	17.694195
35.515315	1163.572253	17.699213
35.774454	1164.595185	17.704231
35.750100	1154.705276	17.709248
35.682404	1163.536597	17.714266
35.956821	1155.802691	17.719283
35.849892	1156.330695	17.724301
35.682171	1158.973205	17.729319
35.464224	1160.765181	17.734336
35.778460	1166.361836	17.739354
35.998678	1158.667979	17.744371
36.092134	1158.082117	17.749389
35.875395	1154.464706	17.754407
36.302908	1152.570460	17.759424
35.927125	1154.797431	17.764442
35.820171	1169.479618	17.769459
36.501730	1175.413211	17.774477
36.200823	1186.468118	17.779495
36.285061	1182.730959	17.784512
36.199346	1184.215033	17.789530
36.313581	1179.258155	17.794547
36.438666	1185.301030	17.799565
36.429912	1183.323652	17.804583
36.406865	1183.642849	17.809600
36.875745	1184.718130	17.814618
36.752327	1178.899056	17.819635
36.691602	1157.331724	17.824653
36.449568	1159.635572	17.829671
36.722909	1156.834493	17.834688
36.493405	1165.280901	17.839706
36.526092	1166.976803	17.844723
36.699999	1175.823927	17.849741
36.571639	1179.460691	17.854759
36.837973	1167.164622	17.859776
36.808474	1176.542246	17.864794
36.760489	1182.069422	17.869811
36.914626	1176.172148	17.874829
36.919942	1176.187092	17.879847
37.034153	1170.425467	17.884864
36.980645	1175.243430	17.889882
36.801976	1174.135299	17.894899
37.011767	1170.842387	17.899917
36.819063	1179.636496	17.904935
37.020659	1170.935665	17.909952
36.643051	1175.097487	17.914970
36.814467	1165.845949	17.919987
36.841359	1182.337594	17.925005
36.994543	1199.718365	17.930023
37.224289	1198.833429	17.935040
37.300821	1201.961555	17.940058
37.282107	1197.890218	17.945075
37.430993	1196.298407	17.950093
37.311340	1198.333770	17.955111
37.503307	1195.214065	17.960128
37.261846	1202.781869	17.965146
37.211360	1198.137980	17.970163
37.393905	1206.807036	17.975181
37.166354	1221.391391	17.980199
37.673699	1205.598665	17.985216
37.878267	1225.148982	17.990234
37.606671	1222.243918	17.995251
38.202293	1222.674474	18.000269
37.541599	1223.437571	18.005287
37.623515	1206.821534	18.010304
37.816165	1214.946196	18.015322
37.696429	1219.285383	18.020339
37.876092	1218.547153	18.025357
37.758652	1217.438893	18.030375
37.816059	1222.485651	18.035392
38.083483	1223.614589	18.040410
38.335951	1237.984890	18.045427
38.213977	1243.167060	18.050445
38.353296	1245.748852	18.055463
38.986493	1230.236198	18.060480
38.591008	1226.760390	18.065498
38.403307	1219.988824	18.070515
38.609109	1218.694215	18.075533
38.335519	1216.568973	18.080551
38.672725	1213.420198	18.085568
38.539636	1209.843319	18.090586
38.523549	1211.202874	18.095603
38.433745	1198.848969	18.100621
38.306400	1212.208908	18.105639
38.345357	1203.716585	18.110656
38.329081	1209.942568	18.115674
38.509766	1232.807175	18.120691
38.667159	1229.377291	18.125709
38.610020	1233.978082	18.130727
38.792202	1232.049680	18.135744
39.013888	1241.091328	18.140762
39.240229	1234.838728	18.145779
39.139422	1225.898063	18.150797
38.922104	1236.681119	18.155815
39.009930	1227.269072	18.160832
39.261074	1235.741195	18.165850
39.056693	1232.405863	18.170867
39.896053	1236.080373	18.175885
39.326059	1230.899314	18.180903
39.721344	1225.939416	18.185920
39.298931	1219.251962	18.190938
38.672165	1204.940314	18.195955
39.048846	1213.676790	18.200973
38.786540	1218.262383	18.205991
39.026442	1224.426142	18.211008
39.087880	1229.532233	18.216026
39.060826	1238.079504	18.221043
39.388475	1230.324601	18.226061
39.239482	1261.973288	18.231079
39.690664	1257.850407	18.236096
39.332664	1255.915116	18.241114
39.650088	1254.934387	18.246131
39.626328	1250.693410	18.251149
39.841290	1254.377387	18.256167
39.812846	1246.469979	18.261184
39.515503	1258.720461	18.266202
39.747843	1259.491968	18.271219
40.033726	1248.928531	18.276237
39.752222	1250.443286	18.281255
40.116531	1259.778189	18.286272
39.953435	1255.085655	18.291290
39.806600	1258.693770	18.296307
39.991861	1241.206258	18.301325
40.224815	1252.079729	18.306343
39.947840	1247.742721	18.311360
40.136466	1267.980414	18.316378
40.177405	1276.469712	18.321395
40.584523	1273.922220	18.326413
40.128958	1278.181489	18.331431
40.552619	1283.155102	18.336448
40.894381	1274.321802	18.341466
40.607615	1281.445442	18.346483
40.492777	1252.047186	18.351501
40.431985	1262.029381	18.356519
40.657961	1274.677579	18.361536
40.492965	1275.066357	18.366554
40.546585	1274.650841	18.371571
40.677346	1274.904915	18.376589
40.707366	1277.020982	18.381607
40.427980	1277.932628	18.386624
40.845353	1281.591210	18.391642
40.495810	1284.751391	18.396659
40.784641	1277.482249	18.401677
40.280662	1279.827154	18.406695
40.582524	1293.728998	18.411712
41.037243	1303.485275	18.416730
41.020661	1304.551414	18.421747
41.073121	1304.319121	18.426765
41.046869	1308.056682	18.431783
41.245048	1305.128497	18.436800
41.361306	1298.482853	18.441818
41.119324	1300.884544	18.446835
41.630319	1291.062167	18.451853
41.575742	1305.711012	18.456871
41.509868	1303.628956	18.461888
41.588831	1289.929373	18.466906
41.591024	1300.252028	18.471923
41.689583	1291.175948	18.476941
41.487882	1293.375661	18.481959
41.335224	1288.110262	18.486976
41.899566	1289.356791	18.491994
41.588089	1297.809793	18.497011
41.879597	1294.380975	18.502029
41.575574	1297.117446	18.507047
41.435697	1290.439350	18.512064
41.930762	1289.396071	18.517082
41.554841	1298.073772	18.522099
41.632326	1294.170385	18.527117
41.550095	1295.306771	18.532135
41.938802	1303.299766	18.537152
41.864537	1320.350205	18.542170
42.262659	1322.550620	18.547187
42.198623	1319.783440	18.552205
42.113785	1319.294938	18.557223
42.120628	1320.316381	18.562240
42.256255	1317.038219	18.567258
42.363497	1319.448316	18.572275
42.554403	1315.896396	18.577293
42.169207	1323.458367	18.582311
42.438355	1313.670713	18.587328
42.528769	1314.899977	18.592346
42.437214	1313.525714	18.597363
42.543273	1305.691884	18.602381
42.314200	1301.722912	18.607399
42.451501	1301.079681	18.612416
42.857693	1310.654211	18.617434
42.175935	1318.887516	18.622451
42.488716	1301.982746	18.627469
42.451938	1312.235771	18.632487
42.741938	1326.786463	18.637504
42.930225	1322.060949	18.642522
42.555542	1326.762010	18.647539
42.880586	1328.292197	18.652557
42.898819	1331.113887	18.657575
42.793548	1331.950918	18.662592
43.394630	1333.248501	18.667610
42.815512	1337.530298	18.672627
43.230410	1328.625551	18.677645
42.913211	1332.702203	18.682663
42.827845	1325.147674	18.687680
43.036516	1331.802375	18.692698
42.806343	1355.678288	18.697715
43.091573	1350.704040	18.702733
43.401698	1358.775646	18.707751
43.209186	1354.349637	18.712768
43.545431	1351.216768	18.717786
43.233105	1357.729036	18.722803
43.672632	1348.296537	18.727821
43.445641	1349.136859	18.732839
43.426192	1351.450041	18.737856
43.574754	1363.551833	18.742874
43.616630	1381.496196	18.747891
43.972186	1377.574471	18.752909
44.183879	1373.485930	18.757927
43.944009	1376.572137	18.762944
44.138475	1374.023234	18.767962
44.365585	1372.444399	18.772979
44.092918	1370.593559	18.777997
44.478061	1369.908339	18.783015
44.067160	1357.273260	18.788032
44.396395	1349.997758	18.793050
44.386343	1352.110645	18.798067
44.283594	1345.764394	18.803085
44.207273	1346.622137	18.808103
44.257258	1361.172591	18.813120
44.548080	1359.763662	18.818138
44.506348	1364.964854	18.823155
44.678990	1363.107364	18.828173
44.403460	1364.630661	18.833191
44.272897	1371.379554	18.838208
44.598827	1368.365068	18.843226
44.862393	1377.441251	18.848243
44.468140	1358.652656	18.853261
44.636800	1364.758195	18.858279
44.104468	1373.135377	18.863296
44.616288	1363.814624	18.868314
44.576108	1370.401028	18.873331
44.523124	1375.023295	18.878349
44.317389	1379.300252	18.883367
44.883686	1393.539455	18.888384
45.026104	1377.964706	18.893402
44.702041	1388.284877	18.898419
44.998558	1396.434375	18.903437
45.173229	1390.303430	18.908455
45.243519	1382.412052	18.913472
45.419918	1380.948463	18.918490
45.180311	1382.223126	18.923507
45.129946	1381.394692	18.928525
45.417021	1387.055636	18.933543
45.422689	1393.634864	18.938560
45.267590	1396.878214	18.943578
44.925112	1408.974917	18.948595
45.668376	1403.345042	18.953613
45.925207	1412.217163	18.958631
45.263332	1421.271098	18.963648
45.623535	1417.680010	18.968666
45.521796	1409.739830	18.973683
45.821032	1411.599129	18.978701
45.877881	1414.345352	18.983719
45.582114	1410.816013	18.988736
45.897114	1400.383629	18.993754
46.083025	1409.178493	18.998771
45.861868	1417.579529	19.003789
45.736856	1415.150105	19.008807
45.905121	1430.168097	19.013824
46.300970	1427.313067	19.018842
46.379525	1429.822352	19.023859
46.255721	1439.937600	19.028877
46.335773	1429.835513	19.033895
46.529020	1431.010802	19.038912
46.682907	1427.553026	19.043930
46.750204	1423.938397	19.048947
46.882634	1429.412135	19.053965
46.662194	1424.835843	19.058983
46.093758	1413.292114	19.064000
46.466252	1423.806141	19.069018
46.811309	1427.425589	19.074035
46.572924	1423.688432	19.079053
46.625292	1424.712216	19.084071
46.508245	1419.176100	19.089088
46.981137	1418.903182	19.094106
46.899257	1424.249543	19.099123
46.904308	1429.071024	19.104141
46.919682	1421.153518	19.109159
46.867710	1424.178735	19.114176
47.082704	1416.059534	19.119194
46.572977	1425.376824	19.124211
46.773951	1438.458264	19.129229
46.957754	1436.936703	19.134247
46.984381	1441.354002	19.139264
47.333655	1446.159427	19.144282
47.287344	1446.624292	19.149299
47.197579	1445.300233	19.154317
47.674186	1449.782738	19.159335
47.394176	1438.670351	19.164352
47.476045	1441.819774	19.169370
47.100071	1456.781041	19.174387
47.354929	1468.105667	19.179405
47.940840	1466.861945	19.184423
47.719650	1476.607446	19.189440
47.847572	1471.433739	19.194458
48.030219	1467.952514	19.199475
48.020570	1474.174394	19.204493
48.012938	1466.957936	19.209511
48.262118	1467.199772	19.214528
47.893930	1467.225896	19.219546
48.260709	1468.231981	19.224563
48.110658	1468.214460	19.229581
48.117970	1460.818931	19.234599
47.958387	1472.385226	19.239616
48.310818	1459.980788	19.244634
48.221837	1465.208348	19.249651
48.234378	1465.736579	19.254669
48.656913	1465.730338	19.259687
47.992944	1459.932745	19.264704
48.339268	1459.102119	19.269722
48.713766	1461.555573	19.274739
48.473607	1460.292948	19.279757
48.920678	1461.658855	19.284775
48.701174	1468.030382	19.289792
48.623824	1455.765871	19.294810
48.504393	1462.475183	19.299827
48.716081	1477.429604	19.304845
49.070208	1482.155380	19.309863
49.125610	1484.377953	19.314880
48.894408	1485.506132	19.319898
48.645992	1482.161873	19.324915
48.582333	1484.835465	19.329933
48.242814	1486.940024	19.334951
48.556421	1501.102133	19.339968
48.888469	1501.466692	19.344986
49.020462	1504.396824	19.350003
48.932998	1512.789581	19.355021
49.440864	1501.998702	19.360039
49.639060	1503.542467	19.365056
49.374102	1512.335435	19.370074
49.374412	1511.890394	19.375091
49.246757	1520.939579	19.380109
49.651610	1510.136431	19.385127
49.842904	1514.799361	19.390144
49.784133	1519.236371	19.395162
49.585555	1516.670129	19.400179
49.332617	1523.223648	19.405197
50.043042	1527.735814	19.410215
50.102150	1534.303566	19.415232
49.899187	1530.245241	19.420250
50.034345	1526.847188	19.425267
49.981029	1533.199013	19.430285
50.266158	1525.668406	19.435303
50.317261	1527.086889	19.440320
50.278050	1522.327535	19.445338
50.232859	1523.757949	19.450355
50.092983	1528.393870	19.455373
50.022095	1526.287326	19.460391
49.897276	1523.037308	19.465408
50.110628	1528.896049	19.470426
50.546764	1540.384833	19.475443
50.351550	1557.804759	19.480461
50.518146	1549.667833	19.485479
50.426744	1549.903068	19.490496
50.420905	1556.626178	19.495514
50.533438	1548.677612	19.500531
50.734121	1554.014457	19.505549
50.983472	1540.455253	19.510567
50.958043	1543.826642	19.515584
50.777518	1541.058743	19.520602
50.888045	1546.741087	19.525619
51.191675	1556.073029	19.530637
51.624970	1556.576368	19.535655
51.471036	1546.151095	19.540672
51.178082	1546.809247	19.545690
51.287001	1541.815231	19.550707
51.286648	1540.559211	19.555725
51.326829	1543.516359	19.560743
51.313355	1566.153024	19.565760
51.606867	1570.500137	19.570778
51.837630	1570.183098	19.575795
51.662941	1567.496336	19.580813
51.681583	1567.364017	19.585831
51.868121	1560.382201	19.590848
51.725098	1550.791547	19.595866
51.733999	1541.287553	19.600883
51.753189	1566.563796	19.605901
52.122984	1564.972056	19.610919
51.890171	1565.466144	19.615936
51.776310	1568.510550	19.620954
52.076886	1564.717325	19.625971
51.921762	1569.283058	19.630989
52.139687	1561.084434	19.636007
52.097815	1558.654588	19.641024
51.884739	1551.520780	19.646042
52.237458	1558.859932	19.651059
52.213768	1561.745035	19.656077
52.238440	1566.011185	19.661095
52.110579	1557.301821	19.666112
51.815860	1561.059406	19.671130
52.167066	1574.631830	19.676147
51.997327	1587.051900	19.681165
52.335370	1588.049871	19.686183
52.323193	1588.212730	19.691200
52.090836	1595.062868	19.696218
52.546303	1608.934579	19.701235
52.677869	1607.809373	19.706253
52.896246	1614.737229	19.711271
53.077717	1608.273768	19.716288
53.284460	1611.968576	19.721306
53.426168	1610.008604	19.726323
53.319671	1607.301683	19.731341
53.158541	1603.785926	19.736359
53.755436	1606.684264	19.741376
53.288652	1607.028809	19.746394
53.364111	1606.543587	19.751411
53.381299	1607.610766	19.756429
53.701953	1596.795510	19.761447
53.629242	1595.983191	19.766464
53.215428	1599.393350	19.771482
53.297354	1601.151011	19.776499
53.521482	1602.349876	19.781517
53.931885	1598.634116	19.786535
53.652415	1599.675186	19.791552
53.753532	1604.516378	19.796570
53.591019	1599.703735	19.801587
53.590337	1606.587010	19.806605
53.723682	1626.268852	19.811623
53.998178	1623.559044	19.816640
53.973275	1628.012866	19.821658
54.226250	1613.840779	19.826675
54.011791	1621.653850	19.831693
54.569010	1626.107991	19.836711
54.471526	1623.541674	19.841728
54.115040	1623.651175	19.846746
54.117999	1617.909993	19.851763
54.173482	1613.347229	19.856781
53.997673	1612.898220	19.861799
54.335003	1619.816909	19.866816
54.059367	1636.700372	19.871834
54.481661	1634.210416	19.876851
54.763134	1641.058965	19.881869
54.614623	1632.393828	19.886887
55.051055	1634.761860	19.891904
54.690438	1641.635266	19.896922
54.930942	1627.184241	19.901939
54.640263	1635.037663	19.906957
55.056312	1641.622117	19.911975
55.136943	1648.107639	19.916992
55.357067	1656.038839	19.922010
55.145942	1647.774846	19.927027
55.293404	1659.959066	19.932045
55.375850	1653.624719	19.937063
55.538981	1642.594261	19.942080
55.219803	1657.426869	19.947098
55.308581	1654.247509	19.952115
55.278920	1662.659684	19.957133
55.246715	1651.580926	19.962151
55.628763	1649.864177	19.967168
55.334495	1658.052705	19.972186
55.596493	1658.112644	19.977203
55.356442	1655.761175	19.982221
55.789820	1665.094937	19.987239
55.861266	1671.998497	19.992256
55.821855	1677.041617	19.997274
55.962212	1689.971783	20.002291
55.964732	1686.389342	20.007309
55.938128	1683.344826	20.012327
56.461053	1677.313864	20.017344
56.279982	1671.566782	20.022362
56.336184	1679.889769	20.027379
56.393363	1682.197300	20.032397
56.378607	1674.906131	20.037415
56.469702	1668.589359	20.042432
56.503949	1672.942401	20.047450
56.961495	1670.068200	20.052467
56.484953	1678.370506	20.057485
56.310369	1675.251341	20.062503
56.250502	1673.755314	20.067520
56.558418	1694.624933	20.072538
57.113453	1699.401346	20.077555
57.132089	1702.062076	20.082573
56.793341	1700.243646	20.087591
57.043940	1689.761222	20.092608
56.739022	1693.170117	20.097626
57.075077	1698.801394	20.102643
57.198008	1697.425056	20.107661
57.162055	1702.817957	20.112679
57.402012	1697.377308	20.117696
57.225811	1701.551879	20.122714
57.598116	1701.588224	20.127731
57.610361	1703.350500	20.132749
57.559483	1709.525270	20.137767
57.716865	1709.140826	20.142784
57.636165	1716.178699	20.147802
57.622240	1723.256609	20.152819
57.310575	1726.691816	20.157837
57.645442	1725.724110	20.162855
57.938533	1713.193087	20.167872
57.704483	1719.140924	20.172890
57.943113	1722.126973	20.177907
57.795495	1722.569845	20.182925
57.940482	1718.333878	20.187943
57.865028	1730.483640	20.192960
57.928551	1742.333909	20.197978
58.243926	1743.161861	20.202995
58.289331	1745.291353	20.208013
58.289419	1751.704320	20.213031
58.717733	1745.530359	20.218048
58.043484	1743.549881	20.223066
58.412533	1745.398278	20.228083
58.263897	1754.075304	20.233101
58.319711	1756.550326	20.238119
58.827510	1757.698447	20.243136
58.705097	1767.154058	20.248154
58.675761	1761.664057	20.253171
58.710034	1768.103234	20.258189
58.866976	1762.189548	20.263207
59.385201	1755.742705	20.268224
59.019697	1768.524952	20.273242
59.207499	1761.381904	20.278259
59.249073	1766.257717	20.283277
59.040042	1766.195784	20.288295
59.019882	1763.087125	20.293312
59.423432	1772.031118	20.298330
59.485685	1787.277472	20.303347
59.790933	1786.560571	20.308365
59.762606	1781.404943	20.313383
60.041973	1783.074879	20.318400
59.519223	1773.698243	20.323418
59.735850	1768.112896	20.328435
59.866116	1774.511787	20.333453
59.918839	1777.397577	20.338471
60.011580	1782.539950	20.343488
59.918441	1788.162755	20.348506
59.918088	1784.984713	20.353523
60.175019	1782.366002	20.358541
59.903381	1779.694396	20.363559
60.151943	1781.845715	20.368576
60.306962	1791.106384	20.373594
60.341414	1777.953078	20.378611
60.111344	1781.918343	20.383629
60.155904	1782.321639	20.388647
60.368506	1779.656221	20.393664
60.362119	1787.689244	20.398682
60.307322	1801.915624	20.403699
60.511165	1797.746162	20.408717
60.356165	1803.116716	20.413735
60.553731	1803.593876	20.418752
60.404185	1802.332809	20.423770
60.733639	1812.415125	20.428787
60.663121	1822.386531	20.433805
60.900074	1837.283644	20.438823
60.813346	1827.305299	20.443840
60.683790	1833.088469	20.448858
60.753986	1837.792549	20.453875
61.147575	1838.665060	20.458893
61.247040	1849.812290	20.463911
61.194572	1854.033786	20.468928
61.197705	1853.288473	20.473946
61.435397	1854.952321	20.478963
61.926662	1848.146728	20.483981
61.528690	1852.968346	20.488999
62.154606	1842.764723	20.494016
62.047977	1854.846866	20.499034
62.063935	1848.115741	20.504051
62.170626	1845.665736	20.509069
62.285557	1843.195504	20.514087
61.866946	1845.902669	20.519104
61.929941	1847.054210	20.524122
62.187559	1846.701399	20.529139
62.461710	1841.712972	20.534157
62.086215	1845.183449	20.539175
62.481726	1853.118818	20.544192
62.590305	1863.993211	20.549210
62.464959	1857.079081	20.554227
62.743051	1853.185170	20.559245
62.420732	1866.582456	20.564263
62.313787	1863.051846	20.569280
62.272760	1871.964550	20.574298
62.723559	1870.000308	20.579315
62.748626	1866.852985	20.584333
62.691884	1868.509313	20.589351
62.754611	1870.197419	20.594368
62.789026	1873.789884	20.599386
62.816492	1891.067940	20.604403
63.365902	1891.742460	20.609421
62.971439	1900.013072	20.614439
63.160869	1893.680814	20.619456
63.247007	1894.718270	20.624474
63.010175	1890.185454	20.629491
63.321897	1890.641576	20.634509
63.215561	1891.021175	20.639527
63.463195	1890.332234	20.644544
63.712171	1911.116660	20.649562
63.654624	1921.007189	20.654579
63.933935	1916.816407	20.659597
63.735199	1922.231721	20.664615
63.882924	1918.727476	20.669632
64.153201	1917.643639	20.674650
63.860967	1922.593886	20.679667
64.061213	1909.594402	20.684685
64.010969	1918.344460	20.689703
63.919369	1911.267220	20.694720
63.988041	1912.825002	20.699738
63.868321	1912.610210	20.704755
64.346778	1923.524527	20.709773
64.285358	1925.771770	20.714791
64.506337	1927.738066	20.719808
64.496895	1937.179223	20.724826
64.142162	1934.384903	20.729843
64.481073	1937.752937	20.734861
64.609200	1942.665734	20.739879
64.442792	1952.036810	20.744896
64.732314	1946.878676	20.749914
64.746489	1951.408513	20.754931
65.001823	1956.699043	20.759949
64.890097	1958.666973	20.764967
65.180261	1956.500655	20.769984
65.143255	1965.920897	20.775002
65.226870	1959.182287	20.780019
65.581931	1960.603678	20.785037
65.509931	1971.184514	20.790055
65.651471	1968.082045	20.795072
65.742606	1971.526778	20.800090
65.973139	1974.908642	20.805107
65.957036	1975.867441	20.810125
66.066280	1965.751011	20.815143
65.774109	1955.394498	20.820160
65.810781	1961.527233	20.825178
65.868474	1973.072433	20.830195
66.173386	1964.500209	20.835213
66.251884	1967.353586	20.840231
66.535838	1964.572813	20.845248
66.428620	1961.155844	20.850266
66.134879	1964.623003	20.855283
66.837579	1965.260885	20.860301
66.101889	1970.463673	20.865319
66.425231	1973.553266	20.870336
66.304723	1972.132991	20.875354
66.117936	1977.584322	20.880371
66.454636	1961.227492	20.885389
66.534067	1984.872685	20.890407
66.741588	1985.758576	20.895424
66.661210	1979.960902	20.900442
66.425235	1987.171542	20.905459
66.844730	1982.640022	20.910477
66.684291	1997.170308	20.915495
66.900420	1999.222586	20.920512
66.691752	2016.159033	20.925530
66.828337	2016.342774	20.930547
67.419824	2009.622411	20.935565
67.426813	2018.691779	20.940583
67.216185	2008.767463	20.945600
67.352455	2014.711029	20.950618
67.757095	2022.793377	20.955635
67.831584	2037.299513	20.960653
67.830679	2043.346638	20.965671
67.905625	2033.428062	20.970688
67.938771	2038.706087	20.975706
67.791593	2042.743635	20.980723
68.130489	2034.181834	20.985741
67.910732	2036.741098	20.990759
68.062509	2037.537888	20.995776
68.102314	2029.710966	21.000794
68.155659	2033.066950	21.005811
68.250305	2027.781523	21.010829
68.259470	2031.857695	21.015847
68.076298	2030.074820	21.020864
68.221241	2037.273141	21.025882
68.133879	2051.855143	21.030899
68.509102	2053.579520	21.035917
68.459356	2048.506072	21.040935
68.659649	2051.453998	21.045952
68.682506	2059.996997	21.050970
68.756390	2078.707121	21.055987
69.045836	2083.118117	21.061005
69.219239	2086.622572	21.066023
69.244097	2087.742230	21.071040
69.718925	2075.375002	21.076058
69.336850	2083.640601	21.081075
69.564552	2083.715385	21.086093
69.507167	2084.087319	21.091111
69.661501	2081.481483	21.096128
69.521256	2075.497482	21.101146
69.567130	2077.765807	21.106163
69.608040	2064.952133	21.111181
69.725135	2075.048932	21.116199
69.712561	2071.301508	21.121216
69.427064	2067.249679	21.126234
69.979412	2085.597646	21.131251
69.964415	2091.826891	21.136269
69.992905	2106.845258	21.141287
70.127621	2100.082808	21.146304
70.464907	2081.712212	21.151322
70.152276	2103.923018	21.156339
70.289202	2088.039220	21.161357
70.554789	2093.574358	21.166375
70.221573	2098.600507	21.171392
70.737331	2103.133854	21.176410
70.388283	2118.018862	21.181427
70.747915	2124.214672	21.186445
70.436352	2112.652334	21.191463
70.620182	2124.802769	21.196480
70.830343	2120.632243	21.201498
70.440461	2122.489123	21.206515
70.892388	2136.049350	21.211533
70.960770	2145.244874	21.216551
70.979963	2150.001212	21.221568
71.273309	2139.350869	21.226586
71.398826	2151.204320	21.231603
71.659615	2140.473863	21.236621
71.424445	2144.351637	21.241639
71.340640	2157.162614	21.246656
72.013075	2167.491220	21.251674
71.831864	2163.277852	21.256691
71.996135	2162.390505	21.261709
72.445068	2166.770223	21.266727
72.195006	2169.435248	21.271744
72.470440	2171.314139	21.276762
72.149205	2164.342210	21.281779
72.555647	2157.082692	21.286797
72.555488	2144.751962	21.291815
72.250111	2140.690607	21.296832
72.475405	2133.191214	21.301850
72.104747	2134.215039	21.306867
72.521942	2142.645798	21.311885
72.369157	2156.180853	21.316903
72.371787	2153.661896	21.321920
72.641691	2150.782302	21.326938
72.702827	2153.736267	21.331955
72.558678	2166.244254	21.336973
72.899152	2159.247557	21.341991
72.683120	2179.142548	21.347008
72.906072	2177.608480	21.352026
72.747506	2181.969763	21.357043
72.745428	2188.440034	21.362061
73.159067	2187.097016	21.367079
72.982351	2202.961880	21.372096
73.140311	2202.302758	21.377114
73.396615	2211.876008	21.382131
73.506871	2211.928164	21.387149
73.958267	2212.671708	21.392167
73.721013	2217.291501	21.397184
73.750571	2214.784097	21.402202
73.357164	2208.075945	21.407219
73.705814	2215.725303	21.412237
73.789980	2235.251402	21.417255
73.630410	2239.054230	21.422272
73.769681	2234.945281	21.427290
73.827390	2239.408404	21.432307
74.168763	2250.284433	21.437325
74.389753	2257.382558	21.442343
74.258858	2255.136993	21.447360
74.480488	2259.886892	21.452378
74.673029	2256.334532	21.457395
74.679947	2256.781609	21.462413
74.829533	2263.038781	21.467431
74.660865	2269.645644	21.472448
75.017118	2269.788660	21.477466
75.068713	2280.710107	21.482483
75.243712	2274.834454	21.487501
75.439669	2275.993595	21.492519
75.175249	2281.501366	21.497536
75.700060	2281.210837	21.502554
75.809276	2274.367103	21.507571
75.562864	2274.853870	21.512589
75.547407	2272.381916	21.517607
75.971977	2276.339407	21.522624
76.078376	2270.212547	21.527642
75.870040	2270.860622	21.532659
75.755416	2268.776623	21.537677
76.149012	2266.919141	21.542695
76.009795	2266.565375	21.547712
76.355594	2266.672155	21.552730
76.311060	2270.624239	21.557747
76.009337	2257.747333	21.562765
76.286648	2265.076500	21.567783
76.146019	2270.325010	21.572800
76.437548	2280.426157	21.577818
76.259845	2289.281579	21.582835
76.338296	2293.305926	21.587853
76.299157	2287.536408	21.592871
76.309913	2296.340215	21.597888
76.527697	2298.739438	21.602906
76.576483	2309.295237	21.607923
76.757373	2321.995426	21.612941
76.954453	2322.621014	21.617959
76.860928	2329.856815	21.622976
77.117590	2323.333976	21.627994
77.221601	2318.564596	21.633011
77.227275	2334.754484	21.638029
77.536984	2344.414120	21.643047
77.378925	2346.256795	21.648064
77.411417	2350.922731	21.653082
77.741574	2344.053823	21.658099
77.330448	2337.922808	21.663117
78.027140	2341.679875	21.668135
77.774535	2346.210579	21.673152
77.718547	2343.782838	21.678170
78.388743	2353.505933	21.683187
78.351445	2346.618848	21.688205
78.313323	2345.226665	21.693223
78.050693	2339.236501	21.698240
78.071199	2356.973731	21.703258
78.512181	2365.953187	21.708275
78.379804	2365.383732	21.713293
79.034181	2360.575455	21.718311
78.791059	2367.086712	21.723328
78.556930	2362.237742	21.728346
78.567213	2365.575286	21.733363
78.456102	2363.945204	21.738381
78.526884	2376.681620	21.743399
78.960698	2387.603216	21.748416
79.331594	2384.556269	21.753434
79.288266	2390.155678	21.758451
79.102317	2387.707263	21.763469
79.344907	2381.117174	21.768487
79.053572	2384.435698	21.773504
79.442531	2401.913254	21.778522
79.739875	2407.449826	21.783539
79.853007	2400.687489	21.788557
79.719764	2402.062333	21.793575
79.817170	2418.203207	21.798592
79.781455	2405.369734	21.803610
79.929071	2400.612438	21.808627
79.900664	2405.013348	21.813645
80.067464	2400.581281	21.818663
79.926632	2420.338512	21.823680
80.045760	2429.803970	21.828698
80.495489	2420.445061	21.833715
80.459724	2423.316413	21.838733
80.486427	2426.307379	21.843751
80.694973	2423.677220	21.848768
80.298992	2429.142525	21.853786
80.999164	2433.015843	21.858803
80.838368	2445.671813	21.863821
81.239104	2452.855475	21.868839
81.106341	2448.991089	21.873856
81.153108	2449.050038	21.878874
81.420379	2452.318930	21.883891
81.387784	2454.621689	21.888909
81.422027	2443.816082	21.893927
81.023734	2442.997923	21.898944
81.571235	2437.120667	21.903962
81.455567	2455.075007	21.908979
81.202694	2474.026103	21.913997
81.589668	2471.112336	21.919015
81.190525	2470.925534	21.924032
81.275115	2471.227891	21.929050
81.887114	2488.774740	21.934067
81.587278	2489.206760	21.939085
81.923310	2487.279371	21.944103
82.256369	2481.034870	21.949120
82.173792	2503.566767	21.954138
81.985330	2513.190924	21.959155
82.372222	2521.560331	21.964173
82.693922	2514.522252	21.969191
82.801457	2520.454708	21.974208
82.399992	2518.709141	21.979226
82.903957	2515.896971	21.984243
83.020804	2524.583272	21.989261
83.196724	2515.383989	21.994279
83.023280	2528.319739	21.999296
83.020482	2533.878125	22.004314
83.286182	2539.224015	22.009331
83.273490	2540.841942	22.014349
83.657618	2544.269286	22.019367
83.583984	2548.270175	22.024384
83.334968	2555.653517	22.029402
83.554937	2544.080216	22.034419
83.959347	2551.408524	22.039437
83.699119	2541.453808	22.044455
83.904754	2534.178260	22.049472
83.747312	2532.211403	22.054490
84.007860	2546.366873	22.059507
83.975433	2564.153630	22.064525
84.234589	2558.861210	22.069543
83.908464	2557.993865	22.074560
83.728700	2567.963864	22.079578
84.300844	2568.609602	22.084595
84.245584	2591.017396	22.089613
84.682836	2585.681284	22.094631
84.463641	2579.595863	22.099648
84.371432	2583.123093	22.104666
84.802030	2597.936844	22.109683
84.998780	2612.708342	22.114701
85.297820	2601.618131	22.119719
84.999250	2609.555272	22.124736
85.241563	2609.731923	22.129754
85.665639	2617.713656	22.134771
85.761062	2607.043549	22.139789
85.945409	2602.157355	22.144807
85.641046	2601.797894	22.149824
85.820353	2605.708669	22.154842
86.058287	2599.469562	22.159859
85.697761	2604.332853	22.164877
86.146354	2593.424365	22.169895
85.886578	2604.792467	22.174912
85.915603	2614.044896	22.179930
86.252567	2618.817851	22.184947
85.710938	2631.019165	22.189965
86.048004	2628.747579	22.194983
86.268939	2628.072264	22.200000
86.365479	2642.105166	22.205018
86.521276	2650.068978	22.210035
86.093141	2661.668643	22.215053
86.572361	2646.159963	22.220071
86.510266	2655.300443	22.225088
86.581009	2660.853658	22.230106
87.087312	2676.905452	22.235123
87.231663	2679.328857	22.240141
87.249366	2668.898133	22.245159
87.406088	2670.309628	22.250176
87.252564	2679.742186	22.255194
87.453900	2676.153648	22.260211
87.384012	2692.541910	22.265229
87.708199	2697.222203	22.270247
87.962098	2701.597893	22.275264
87.963102	2701.263179	22.280282
87.794478	2692.578587	22.285299
87.703103	2695.502881	22.290317
87.886563	2700.946921	22.295335
88.077376	2701.945932	22.300352
88.189116	2716.150100	22.305370
88.589791	2718.356605	22.310387
88.629220	2727.964109	22.315405
88.690258	2722.147196	22.320423
88.792842	2720.243733	22.325440
88.454814	2726.706865	22.330458
88.827666	2724.701091	22.335475
88.671192	2721.004482	22.340493
88.715848	2722.083205	22.345511
89.133723	2716.399756	22.350528
89.121079	2729.465109	22.355546
89.268508	2733.860644	22.360563
89.160429	2749.882513	22.365581
89.359428	2741.566384	22.370599
89.216504	2742.194758	22.375616
89.309890	2750.136831	22.380634
89.450522	2745.894994	22.385651
89.687818	2762.957956	22.390669
89.815913	2762.625423	22.395687
89.787698	2769.848011	22.400704
89.714612	2766.122548	22.405722
90.109542	2766.357351	22.410739
89.993828	2767.505387	22.415757
90.230394	2773.417712	22.420775
90.368040	2781.775792	22.425792
90.586655	2797.509806	22.430810
90.607015	2792.879654	22.435827
90.622675	2805.132646	22.440845
90.554427	2795.365488	22.445863
90.453251	2797.151953	22.450880
90.662240	2809.904897	22.455898
91.282022	2814.084419	22.460915
91.282291	2820.778639	22.465933
91.021897	2817.761090	22.470951
91.372375	2818.400538	22.475968
91.121621	2812.992249	22.480986
91.611433	2819.294153	22.486003
91.377878	2822.458519	22.491021
91.504563	2830.505877	22.496039
91.790063	2835.826661	22.501056
91.598380	2841.613575	22.506074
92.003153	2841.196663	22.511091
91.879126	2845.928280	22.516109
91.807334	2850.086757	22.521127
92.375332	2852.020882	22.526144
92.109938	2856.436938	22.531162
92.463001	2855.756694	22.536179
92.635987	2862.060908	22.541197
92.590554	2862.674012	22.546215
92.956050	2858.507385	22.551232
92.760539	2861.902513	22.556250
92.741659	2855.798239	22.561267
92.594737	2866.981546	22.566285
92.940178	2879.624788	22.571303
93.130728	2874.317775	22.576320
93.427924	2887.890190	22.581338
93.440251	2882.226041	22.586355
93.270146	2888.037994	22.591373
93.482550	2875.796553	22.596391
93.493309	2886.948856	22.601408
93.468732	2904.210789	22.606426
93.895186	2901.915697	22.611443
94.062054	2902.287232	22.616461
94.016181	2911.046556	22.621479
94.151986	2901.925954	22.626496
94.035668	2903.635897	22.631514
94.125223	2901.074812	22.636531
93.901278	2912.162903	22.641549
94.193456	2922.734585	22.646567
94.624545	2922.714385	22.651584
94.687985	2927.489246	22.656602
94.867591	2925.690474	22.661619
94.902965	2931.438687	22.666637
94.456583	2920.704938	22.671655
94.811379	2926.188483	22.676672
94.993813	2944.816221	22.681690
95.074493	2952.735124	22.686707
95.194191	2958.088234	22.691725
95.000209	2959.059172	22.696743
95.536628	2955.544330	22.701760
95.357102	2953.899663	22.706778
95.517764	2971.817537	22.711795
95.458436	2975.844685	22.716813
95.615731	2985.105614	22.721831
96.189570	2967.896417	22.726848
95.920710	2979.019993	22.731866
96.010251	2971.143840	22.736883
96.195456	2995.559686	22.741901
96.271479	3006.168438	22.746919
96.670332	2996.874015	22.751936
96.430019	3010.335049	22.756954
96.148440	3007.986749	22.761971
96.737252	2997.179143	22.766989
96.675589	3003.737948	22.772007
96.909044	3015.035345	22.777024
97.164040	3024.296769	22.782042
96.983538	3019.685403	22.787059
97.024934	3017.239157	22.792077
97.046536	3018.252072	22.797095
97.182096	3026.301284	22.802112
97.247110	3034.342614	22.807130
97.332315	3044.545953	22.812147
97.770139	3041.548381	22.817165
97.893715	3049.195484	22.822183
97.847023	3040.990303	22.827200
97.716705	3051.240037	22.832218
98.041698	3053.275382	22.837235
98.153182	3062.871776	22.842253
97.931428	3062.941233	22.847271
98.392655	3064.235616	22.852288
98.246925	3062.765549	22.857306
98.589363	3065.186378	22.862323
98.567908	3080.693129	22.867341
98.579205	3090.772356	22.872359
99.173459	3086.412027	22.877376
98.740305	3097.305760	22.882394
99.217610	3088.680746	22.887411
99.039571	3087.263083	22.892429
98.866256	3094.353879	22.897447
99.262606	3109.103981	22.902464
99.483400	3110.240350	22.907482
99.573307	3113.180497	22.912499
99.987684	3112.616888	22.917517
99.870098	3114.503799	22.922535
99.593721	3111.362455	22.927552
99.725265	3121.675358	22.932570
100.013544	3129.157816	22.937587
100.267312	3129.768241	22.942605
100.049513	3130.474639	22.947623
100.036969	3138.206230	22.952640
99.936380	3143.085752	22.957658
100.350409	3154.979882	22.962675
100.773948	3156.406426	22.967693
100.757855	3163.753522	22.972711
101.090282	3162.262191	22.977728
100.664196	3161.574600	22.982746
100.775739	3162.292527	22.987763
101.125780	3172.605946	22.992781
101.051759	3175.016287	22.997799
101.361660	3178.171322	23.002816
101.708441	3187.737230	23.007834
101.481889	3182.003101	23.012851
101.463632	3176.788682	23.017869
101.579878	3186.700020	23.022887
101.551852	3193.114749	23.027904
101.784368	3199.031005	23.032922
101.935468	3205.726987	23.037939
102.242482	3204.608915	23.042957
102.090125	3211.469223	23.047975
102.020675	3201.316971	23.052992
102.173267	3219.564605	23.058010
102.418772	3228.581433	23.063027
102.956193	3228.449888	23.068045
102.676060	3229.175525	23.073063
102.627960	3229.344027	23.078080
103.074659	3229.570727	23.083098
103.068620	3238.832127	23.088115
103.138965	3247.759625	23.093133
103.242887	3256.666086	23.098151
103.310225	3249.803294	23.103168
103.424115	3256.091654	23.108186
103.116290	3246.563787	23.113203
103.770652	3253.928974	23.118221
103.713756	3264.419827	23.123239
103.869399	3269.300271	23.128256
104.150586	3277.083747	23.133274
104.012458	3280.069116	23.138291
103.880200	3267.038686	23.143309
104.032694	3274.798135	23.148327
104.331204	3279.362666	23.153344
104.405455	3292.026592	23.158362
104.293489	3294.427112	23.163379
104.527632	3287.689673	23.168397
104.712768	3303.924908	23.173415
105.028733	3313.776620	23.178432
105.199337	3321.021937	23.183450
105.148165	3319.849505	23.188467
105.188567	3324.097827	23.193485
105.090756	3320.849563	23.198503
105.726300	3323.319195	23.203520
106.130881	3339.810460	23.208538
105.816214	3331.344128	23.213555
105.688009	3333.295850	23.218573
105.821389	3331.608438	23.223591
105.808385	3340.687917	23.228608
106.363082	3337.236421	23.233626
106.148978	3342.512534	23.238643
106.628998	3341.108535	23.243661
106.097500	3348.328141	23.248679
106.709605	3354.065039	23.253696
106.858284	3360.265922	23.258714
106.670630	3361.598862	23.263731
107.099275	3368.235640	23.268749
106.940241	3366.849696	23.273767
107.233199	3366.705950	23.278784
107.194285	3363.038135	23.283802
106.887266	3366.425576	23.288819
107.184432	3368.986103	23.293837
106.959825	3380.513308	23.298855
107.347779	3379.164761	23.303872
107.616047	3392.912529	23.308890
107.440290	3407.866135	23.313907
107.996217	3410.089437	23.318925
107.871530	3411.844927	23.323943
107.843285	3407.790364	23.328960
107.750600	3410.108971	23.333978
108.099318	3426.088280	23.338995
108.495728	3420.875107	23.344013
108.523138	3436.570198	23.349031
108.909890	3431.005031	23.354048
108.937725	3424.044203	23.359066
108.526249	3430.875752	23.364083
109.024712	3441.986709	23.369101
109.156781	3449.553744	23.374119
109.482359	3456.443424	23.379136
109.412687	3453.143384	23.384154
109.212258	3455.434689	23.389171
109.470897	3444.403949	23.394189
109.314613	3452.691608	23.399207
109.557719	3455.408963	23.404224
110.248460	3468.954879	23.409242
109.842100	3474.529436	23.414259
110.430816	3475.115804	23.419277
110.279562	3483.819320	23.424295
110.202728	3481.372598	23.429312
110.406161	3475.564696	23.434330
110.276035	3473.868053	23.439347
110.295569	3475.812426	23.444365
110.777166	3493.083996	23.449383
110.532483	3490.663569	23.454400
110.889492	3497.769282	23.459418
110.949258	3503.273977	23.464435
111.130233	3501.973630	23.469453
111.187808	3521.053938	23.474471
111.443644	3521.834493	23.479488
111.803658	3522.292565	23.484506
111.511265	3525.702994	23.489523
111.715898	3523.057510	23.494541
111.414468	3524.231533	23.499559
111.844632	3531.057512	23.504576
112.033431	3544.044550	23.509594
112.147565	3545.794199	23.514611
112.019361	3537.257526	23.519629
112.035039	3542.425102	23.524647
112.307185	3555.058208	23.529664
112.494917	3566.972283	23.534682
112.632161	3577.877942	23.539699
112.944158	3568.966124	23.544717
112.576409	3577.911921	23.549735
112.829257	3587.451727	23.554752
113.443113	3594.435174	23.559770
113.115164	3591.557487	23.564787
113.257891	3604.324531	23.569805
113.646536	3614.449090	23.574823
113.696552	3619.144172	23.579840
114.015775	3621.442462	23.584858
113.413331	3620.630978	23.589875
113.829024	3611.510358	23.594893
114.058081	3620.741433	23.599911
114.147666	3639.305526	23.604928
114.294352	3633.894693	23.609946
114.184187	3636.317070	23.614963
114.643179	3645.152313	23.619981
114.187049	3646.337955	23.624999
114.235933	3655.650933	23.630016
114.644663	3661.527108	23.635034
114.837044	3665.218280	23.640051
114.988048	3677.043492	23.645069
115.517126	3683.191202	23.650087
115.231807	3683.561002	23.655104
115.682962	3684.986420	23.660122
115.525527	3693.214399	23.665139
115.630539	3689.905885	23.670157
115.577945	3700.339502	23.675175
115.626455	3715.103565	23.680192
116.040772	3707.460281	23.685210
115.970455	3717.631552	23.690227
116.184310	3721.139459	23.695245
116.190391	3716.208299	23.700263
116.037326	3729.807702	23.705280
116.669917	3737.615232	23.710298
116.616962	3748.342473	23.715315
116.951532	3738.555885	23.720333
117.099297	3731.847596	23.725351
116.807421	3741.479138	23.730368
117.087032	3746.892649	23.735386
117.357049	3756.316226	23.740403
117.584032	3755.807210	23.745421
117.510400	3752.081628	23.750439
117.349065	3770.887174	23.755456
117.671784	3768.557727	23.760474
117.784305	3774.180493	23.765491
117.891747	3785.898972	23.770509
118.107331	3793.648761	23.775527
118.397666	3776.764131	23.780544
118.395162	3778.314289	23.785562
117.989155	3791.271594	23.790579
118.490248	3792.897516	23.795597
118.693109	3799.797086	23.800615
118.283429	3805.987752	23.805632
118.714288	3813.167242	23.810650
119.130963	3826.052498	23.815667
119.202397	3822.553527	23.820685
119.184741	3824.257567	23.825703
118.989150	3829.682426	23.830720
119.876472	3842.484489	23.835738
119.174965	3856.097314	23.840755
119.185469	3860.495638	23.845773
119.614146	3866.911651	23.850791
119.704097	3883.894598	23.855808
120.333240	3878.951001	23.860826
120.270834	3887.410377	23.865843
120.162039	3886.657264	23.870861
120.657564	3893.015468	23.875879
120.692327	3907.052719	23.880896
120.778479	3910.252408	23.885914
120.905470	3914.522022	23.890931
120.756745	3901.900886	23.895949
121.211112	3915.316884	23.900967
121.151826	3923.308644	23.905984
121.305812	3921.267592	23.911002
121.456014	3931.073015	23.916019
121.809939	3924.717434	23.921037
121.910874	3917.381982	23.926055
121.798660	3918.119213	23.931072
122.252236	3940.392145	23.936090
122.041676	3957.144480	23.941107
122.581929	3947.183519	23.946125
122.495590	3945.562037	23.951143
122.246152	3948.344008	23.956160
122.336442	3947.973188	23.961178
122.325731	3968.930087	23.966195
122.559690	3971.800461	23.971213
122.537381	3972.974972	23.976231
122.799116	3981.872848	23.981248
123.068621	3985.065919	23.986266
123.262791	3994.391030	23.991283
123.207605	4010.216344	23.996301
123.394926	4005.013669	24.001319
123.409524	4012.129041	24.006336
123.758697	4017.635898	24.011354
123.887616	4035.158937	24.016371
123.747801	4028.874361	24.021389
124.236041	4036.780391	24.026407
124.221440	4049.266227	24.031424
124.260354	4052.864734	24.036442
124.544327	4061.765479	24.041459
124.567752	4049.303497	24.046477
124.794289	4048.418932	24.051495
124.828765	4055.550146	24.056512
125.362630	4065.008302	24.061530
125.310999	4077.998670	24.066547
125.491309	4075.704121	24.071565
125.271053	4077.417831	24.076583
125.419127	4081.864097	24.081600
125.479181	4073.332397	24.086618
125.432907	4087.584494	24.091635
125.953026	4101.018737	24.096653
125.904793	4107.212850	24.101671
125.774547	4107.018616	24.106688
126.012860	4111.024637	24.111706
125.971433	4121.141106	24.116723
126.536722	4127.841981	24.121741
126.579166	4123.100711	24.126759
126.360247	4142.878369	24.131776
126.483308	4150.737499	24.136794
126.720575	4162.183369	24.141811
126.794803	4164.861005	24.146829
127.141730	4175.301744	24.151847
126.902831	4185.430247	24.156864
127.473193	4175.148803	24.161882
127.237536	4187.562048	24.166899
127.126437	4199.747463	24.171917
127.484334	4210.271728	24.176935
127.550637	4230.724461	24.181952
128.146489	4226.130039	24.186970
128.007796	4225.293216	24.191987
128.289909	4245.623775	24.197005
128.600546	4249.747910	24.202023
128.660281	4257.891617	24.207040
128.924760	4252.979801	24.212058
129.143186	4255.928408	24.217075
129.237589	4266.582366	24.222093
129.808050	4278.140244	24.227111
129.438153	4280.199373	24.232128
129.491334	4282.848760	24.237146
129.284784	4280.876778	24.242163
129.370990	4274.569332	24.247181
130.170342	4285.718895	24.252199
130.243726	4305.271018	24.257216
129.983205	4293.847633	24.262234
130.419732	4299.795418	24.267251
130.377858	4302.892132	24.272269
130.362425	4307.206248	24.277287
130.532071	4318.763817	24.282304
130.899488	4331.429887	24.287322
130.819194	4323.485062	24.292339
130.890911	4331.402817	24.297357
131.582873	4328.336816	24.302375
131.455561	4339.158123	24.307392
131.099524	4341.502324	24.312410
131.371128	4348.647006	24.317427
131.351061	4355.171375	24.322445
131.361039	4370.245027	24.327463
131.556546	4380.548629	24.332480
131.791902	4372.093487	24.337498
132.160973	4391.078563	24.342515
132.078891	4401.034264	24.347533
132.524548	4396.643249	24.352551
132.318047	4407.609574	24.357568
132.609270	4417.216405	24.362586
133.017081	4425.012105	24.367603
132.991003	4430.514748	24.372621
133.239359	4425.999969	24.377639
133.353149	4431.029326	24.382656
133.505800	4419.705267	24.387674
133.474436	4415.894015	24.392691
133.468519	4445.650931	24.397709
133.416709	4448.518805	24.402727
133.734793	4445.890135	24.407744
133.851249	4454.997236	24.412762
133.964968	4465.941837	24.417779
134.196724	4485.434620	24.422797
134.214946	4487.013156	24.427815
134.262875	4482.637084	24.432832
134.551189	4498.282749	24.437850
134.897090	4491.344282	24.442867
134.702092	4508.167284	24.447885
134.503941	4502.213643	24.452903
134.626978	4533.440357	24.457920
134.960937	4531.355260	24.462938
135.437035	4540.080942	24.467955
135.446478	4556.439522	24.472973
135.698323	4554.360973	24.477991
135.922654	4562.835714	24.483008
135.769169	4566.767489	24.488026
136.245383	4573.981212	24.493043
136.052847	4574.115537	24.498061
136.295059	4584.677082	24.503079
136.414388	4601.725541	24.508096
136.827671	4595.600323	24.513114
136.676544	4605.077696	24.518131
136.708524	4609.078275	24.523149
137.164002	4619.922079	24.528167
137.119761	4631.813224	24.533184
137.047292	4632.588447	24.538202
137.444900	4635.149204	24.543219
137.227878	4653.247860	24.548237
137.681615	4655.815609	24.553255
137.937971	4661.614976	24.558272
138.143462	4676.554088	24.563290
138.602751	4673.152015	24.568307
138.192815	4687.041739	24.573325
138.443166	4678.123257	24.578343
138.515717	4685.018328	24.583360
138.797354	4700.561049	24.588378
139.401956	4699.920249	24.593395
139.075491	4710.447856	24.598413
139.210397	4702.333420	24.603431
139.217477	4720.851571	24.608448
139.147314	4731.768323	24.613466
139.318921	4727.233929	24.618483
139.268753	4744.776241	24.623501
140.127255	4746.983878	24.628519
140.247767	4763.808190	24.633536
140.158079	4758.178377	24.638554
140.450984	4762.734695	24.643571
140.507280	4785.891603	24.648589
140.377441	4788.926425	24.653607
140.557153	4788.497388	24.658624
140.856117	4794.410071	24.663642
140.673224	4810.104575	24.668659
140.902523	4819.774982	24.673677
141.082842	4818.133741	24.678695
141.253413	4828.930766	24.683712
141.736849	4836.699014	24.688730
141.864218	4832.755484	24.693747
142.024305	4841.215167	24.698765
141.843106	4836.840185	24.703783
142.093715	4856.712354	24.708800
142.383088	4867.269832	24.713818
142.520074	4860.345015	24.718835
142.555133	4859.474628	24.723853
142.992288	4849.254712	24.728871
143.060945	4866.936352	24.733888
143.280990	4873.521142	24.738906
143.198975	4878.417158	24.743923
143.217252	4885.876359	24.748941
143.327927	4878.327506	24.753959
143.318821	4882.602888	24.758976
143.369357	4894.185797	24.763994
143.673573	4895.804790	24.769011
143.609143	4912.787633	24.774029
144.278289	4919.093749	24.779047
144.466720	4925.614066	24.784064
144.607664	4934.086261	24.789082
144.917536	4939.792107	24.794099
144.641336	4942.152285	24.799117
144.633714	4939.180003	24.804135
144.738302	4947.872546	24.809152
144.863484	4964.986716	24.814170
145.382055	4959.813945	24.819187
145.108979	4984.149598	24.824205
144.960539	4982.894443	24.829223
145.533750	4979.427119	24.834240
145.787442	5005.757290	24.839258
146.227843	5014.081598	24.844275
146.244226	5021.051884	24.849293
146.200723	5014.357306	24.854311
146.404033	5023.624696	24.859328
146.267343	5030.944093	24.864346
146.695394	5033.818952	24.869363
146.920264	5049.367708	24.874381
147.023297	5059.032772	24.879399
147.343824	5062.255921	24.884416
147.626298	5062.464190	24.889434
147.619660	5054.958895	24.894451
147.543419	5073.108513	24.899469
147.696000	5087.393370	24.904487
147.771185	5089.243970	24.909504
147.876532	5100.269178	24.914522
148.279238	5102.516703	24.919539
148.140039	5115.493121	24.924557
148.489092	5118.124686	24.929575
148.712094	5130.570883	24.934592
148.541047	5143.943727	24.939610
148.794722	5140.807369	24.944627
149.033097	5145.817406	24.949645
149.285491	5164.275480	24.954663
149.378343	5163.512818	24.959680
149.819172	5163.939337	24.964698
149.969911	5168.868412	24.969715
149.941998	5185.949956	24.974733
149.903852	5187.142809	24.979751
150.207662	5188.525147	24.984768
150.221751	5199.015465	24.989786
150.728670	5203.061720	24.994803
150.732559	5217.912909	24.999821
150.407784	5222.455631	25.004839
150.840543	5219.354336	25.009856
150.989098	5236.992252	25.014874
151.216561	5245.867710	25.019891
151.443329	5245.870060	25.024909
151.161010	5253.177637	25.029927
151.509288	5253.520804	25.034944
151.634805	5270.830919	25.039962
151.891870	5270.759077	25.044979
152.416578	5293.552839	25.049997
152.193761	5292.413483	25.055015
152.766444	5302.235531	25.060032
152.575105	5305.074892	25.065050
152.821966	5303.814605	25.070067
152.794494	5303.332787	25.075085
153.101462	5309.957780	25.080103
153.292618	5311.256765	25.085120
153.023674	5323.458189	25.090138
153.326393	5323.612785	25.095155
153.189773	5337.838978	25.100173
153.386007	5348.231400	25.105191
153.427460	5345.481797	25.110208
153.871715	5365.592498	25.115226
154.128009	5364.930487	25.120243
154.126767	5373.150536	25.125261
154.260128	5383.117213	25.130279
154.593407	5392.298141	25.135296
154.501499	5402.641037	25.140314
154.800223	5408.863309	25.145331
155.037108	5427.775478	25.150349
154.939267	5418.974317	25.155367
155.495883	5433.145642	25.160384
155.479666	5455.061575	25.165402
155.736453	5443.581676	25.170419
155.677667	5460.175877	25.175437
155.783027	5482.091736	25.180455
156.148890	5470.806226	25.185472
156.569649	5492.372805	25.190490
156.588377	5495.296081	25.195507
156.860230	5503.514441	25.200525
156.612702	5507.306474	25.205543
156.977310	5510.295519	25.210560
157.089790	5525.458238	25.215578
157.404574	5534.642135	25.220595
157.712741	5534.391828	25.225613
157.624434	5553.995875	25.230631
158.040182	5551.373846	25.235648
157.708032	5557.382494	25.240666
157.962688	5561.717727	25.245683
158.070244	5574.112867	25.250701
158.565909	5582.744445	25.255719
158.523670	5586.987303	25.260736
158.293493	5603.119201	25.265754
158.606044	5608.218758	25.270771
158.800352	5632.740898	25.275789
158.840057	5641.188246	25.280807
159.228637	5640.297161	25.285824
159.329162	5650.288069	25.290842
159.502148	5661.208320	25.295859
159.602720	5671.319185	25.300877
159.759641	5676.518903	25.305895
160.380841	5679.600358	25.310912
160.598425	5701.628323	25.315930
160.877883	5708.548186	25.320947
161.111002	5708.704220	25.325965
161.144095	5704.071332	25.330983
160.913423	5722.043760	25.336000
160.873559	5722.605579	25.341018
161.327910	5733.680665	25.346035
161.560938	5740.648852	25.351053
161.504575	5737.851380	25.356071
161.643219	5755.655499	25.361088
161.804851	5761.700497	25.366106
161.868675	5766.393971	25.371123
161.938073	5773.842370	25.376141
162.496198	5791.025227	25.381159
162.652250	5796.468181	25.386176
162.549782	5798.624474	25.391194
163.143466	5810.561655	25.396211
163.102734	5819.274224	25.401229
163.040016	5826.620230	25.406247
163.115781	5826.895617	25.411264
163.180436	5840.194163	25.416282
163.557069	5846.319149	25.421299
163.596828	5854.233103	25.426317
163.487271	5875.700126	25.431335
164.063587	5873.832605	25.436352
164.114863	5891.862043	25.441370
164.422081	5894.815949	25.446387
164.478369	5898.330025	25.451405
164.696400	5916.907887	25.456423
164.961859	5917.406095	25.461440
164.853293	5924.270031	25.466458
165.151776	5937.639345	25.471475
165.401077	5942.439546	25.476493
165.735616	5955.127684	25.481511
165.850502	5967.629271	25.486528
166.273018	5980.164747	25.491546
166.488148	5976.958526	25.496563
166.233596	5979.586922	25.501581
166.416174	5997.428587	25.506599
166.743088	5997.140613	25.511616
166.752776	6009.807077	25.516634
166.952689	6012.228540	25.521651
166.960118	6020.857897	25.526669
167.136486	6036.149927	25.531687
167.380335	6049.720443	25.536704
167.346065	6061.547821	25.541722
167.531106	6074.893969	25.546739
167.622641	6080.631223	25.551757
167.592768	6094.784458	25.556775
167.951966	6110.562459	25.561792
168.681643	6118.100119	25.566810
168.666850	6130.751560	25.571827
168.927551	6134.363085	25.576845
168.994609	6134.090565	25.581863
169.268669	6150.336511	25.586880
169.291128	6161.627887	25.591898
169.467704	6161.110923	25.596915
169.888869	6175.294576	25.601933
170.011250	6180.938640	25.606951
170.331005	6185.143866	25.611968
170.931099	6190.514217	25.616986
170.582261	6189.217767	25.622003
170.657796	6198.941407	25.627021
171.020919	6213.724499	25.632039
170.808045	6216.393751	25.637056
170.855276	6227.974867	25.642074
171.093871	6238.803109	25.647091
171.292776	6238.329996	25.652109
171.390625	6258.391776	25.657127
171.550234	6248.182998	25.662144
171.962100	6262.794341	25.667162
172.192534	6285.244004	25.672180
172.699872	6280.441971	25.677197
172.327228	6291.675367	25.682215
173.085576	6301.790863	25.687232
172.853405	6317.598552	25.692250
173.025973	6324.248127	25.697268
173.264442	6318.010827	25.702285
173.318869	6328.034581	25.707303
173.265059	6340.654398	25.712320
173.577668	6349.539152	25.717338
173.346801	6358.032376	25.722356
173.979453	6372.520828	25.727373
174.140256	6375.968114	25.732391
174.037913	6382.139906	25.737408
174.526912	6392.423922	25.742426
174.764730	6399.470531	25.747444
174.791276	6403.658606	25.752461
174.858798	6418.718620	25.757479
175.054698	6424.048188	25.762496
175.130452	6434.194931	25.767514
175.090768	6453.852302	25.772532
175.541126	6452.023400	25.777549
175.518751	6462.087670	25.782567
175.782261	6475.926908	25.787584
176.185279	6483.657953	25.792602
176.761729	6496.999913	25.797620
176.969361	6507.744774	25.802637
177.015006	6514.158600	25.807655
176.967588	6508.647897	25.812672
177.032685	6519.361428	25.817690
177.328377	6531.506765	25.822708
177.598246	6529.210509	25.827725
177.910543	6539.803249	25.832743
178.061951	6559.907478	25.837760
177.835462	6565.195926	25.842778
177.862971	6563.824705	25.847796
178.220135	6579.003630	25.852813
178.035135	6593.282571	25.857831
178.119643	6601.748598	25.862848
178.996938	6620.836319	25.867866
179.171901	6637.249750	25.872884
179.247073	6644.498717	25.877901
179.012409	6654.372214	25.882919
179.570883	6652.778903	25.887936
179.922850	6656.543548	25.892954
179.899327	6682.161919	25.897972
180.398558	6684.205112	25.902989
180.240252	6697.065680	25.908007
180.598828	6693.817922	25.913024
181.298836	6713.950022	25.918042
180.863456	6725.288215	25.923060
180.951713	6716.634060	25.928077
180.748841	6738.845945	25.933095
181.526469	6737.205667	25.938112
181.685516	6756.582836	25.943130
181.833578	6777.824300	25.948148
181.956347	6778.215457	25.953165
181.876370	6781.567952	25.958183
182.288925	6799.554311	25.963200
182.762666	6802.112924	25.968218
182.635212	6814.223719	25.973236
182.809307	6830.028182	25.978253
183.076437	6834.936316	25.983271
182.929440	6848.915911	25.988288
183.500459	6860.541645	25.993306
183.573446	6869.811448	25.998324
183.585483	6885.268834	26.003341
183.639148	6884.843715	26.008359
183.831530	6901.292536	26.013376
184.064123	6916.245019	26.018394
184.491809	6930.930183	26.023412
185.131106	6944.609884	26.028429
185.150247	6949.067580	26.033447
184.986754	6956.893889	26.038464
185.352539	6968.119347	26.043482
185.467943	6980.037517	26.048500
185.802742	6990.781680	26.053517
185.848004	7000.961926	26.058535
186.099100	7005.863147	26.063552
186.310056	7008.270387	26.068570
186.269610	7031.587352	26.073588
186.614695	7033.313787	26.078605
186.621551	7044.159868	26.083623
186.597937	7041.941096	26.088640
186.925045	7056.307485	26.093658
187.342969	7063.152503	26.098676
187.685324	7075.473992	26.103693
187.938493	7084.791443	26.108711
187.565164	7084.502664	26.113728
188.112795	7085.610186	26.118746
187.975611	7098.991775	26.123764
188.165286	7095.625188	26.128781
188.242459	7120.268690	26.133799
188.168731	7126.518329	26.138816
188.541429	7147.245174	26.143834
188.502064	7162.196265	26.148852
189.279605	7171.273765	26.153869
189.324077	7185.602452	26.158887
189.540841	7198.859211	26.163904
189.783753	7217.784913	26.168922
189.832731	7225.669602	26.173940
190.537058	7232.741313	26.178957
190.432464	7235.911487	26.183975
189.908686	7261.230200	26.188992
190.673506	7257.044226	26.194010
190.882571	7286.986753	26.199028
191.241578	7291.258697	26.204045
191.527311	7310.105175	26.209063
191.607102	7326.736178	26.214080
191.784601	7328.264751	26.219098
191.951406	7349.683885	26.224116
192.135340	7350.321187	26.229133
192.036193	7359.277251	26.234151
191.737004	7386.729790	26.239168
192.344887	7392.058239	26.244186
192.506485	7416.407939	26.249204
193.137177	7434.089247	26.254221
193.905025	7438.849648	26.259239
193.344720	7446.722544	26.264256
194.150378	7462.065556	26.269274
193.977684	7473.091553	26.274292
194.639338	7477.628670	26.279309
194.509074	7488.925844	26.284327
194.952529	7491.157816	26.289344
194.848023	7496.070680	26.294362
195.058173	7517.435864	26.299380
195.147437	7521.753277	26.304397
195.756176	7523.681544	26.309415
195.489357	7547.558687	26.314432
196.282843	7544.267905	26.319450
195.720619	7548.479023	26.324468
195.538345	7557.700766	26.329485
196.065483	7579.306807	26.334503
196.626091	7594.937724	26.339520
196.760333	7590.796794	26.344538
197.138960	7615.744160	26.349556
197.107032	7623.518570	26.354573
197.413808	7632.171242	26.359591
197.296611	7637.436560	26.364608
197.830000	7646.978744	26.369626
197.575012	7663.870859	26.374644
197.962158	7674.136826	26.379661
198.380083	7678.674292	26.384679
198.506161	7700.277007	26.389696
198.707863	7704.106451	26.394714
198.721861	7715.857875	26.399732
198.811421	7734.776562	26.404749
199.150828	7748.544885	26.409767
199.495615	7760.326600	26.414784
200.078136	7764.449986	26.419802
200.106754	7772.631702	26.424820
200.017194	7771.818585	26.429837
200.277224	7767.875746	26.434855
200.318746	7792.386820	26.439872
200.591545	7795.633720	26.444890
200.551375	7816.470198	26.449908
200.647586	7819.091257	26.454925
200.928536	7832.133209	26.459943
200.880615	7862.053788	26.464960
201.596346	7868.006363	26.469978
201.656322	7879.996939	26.474996
201.605389	7893.267722	26.480013
202.067654	7898.555991	26.485031
202.642971	7912.397977	26.490048
202.603451	7938.992976	26.495066
202.577195	7949.112336	26.500084
203.172891	7956.640181	26.505101
203.121905	7969.800529	26.510119
203.301996	7979.215123	26.515136
203.738850	7989.129358	26.520154
203.762835	7994.811494	26.525172
203.947221	7997.134628	26.530189
204.154030	8010.229363	26.535207
204.341675	8029.350824	26.540224
204.421993	8035.740806	26.545242
204.838310	8054.646516	26.550260
205.224509	8073.253883	26.555277
205.880166	8063.768293	26.560295
205.328453	8077.490196	26.565312
205.544067	8104.635840	26.570330
205.880554	8115.500367	26.575348
205.975415	8128.101273	26.580365
206.133189	8132.098700	26.585383
206.458002	8156.044955	26.590400
206.895083	8160.172274	26.595418
206.775215	8185.741526	26.600436
206.930943	8191.482012	26.605453
207.438039	8188.848465	26.610471
207.617249	8212.653433	26.615488
207.675686	8219.810928	26.620506
208.246762	8238.320043	26.625524
208.357297	8236.474752	26.630541
208.809348	8252.170591	26.635559
208.855787	8272.627787	26.640576
209.201299	8269.306033	26.645594
209.257657	8281.477392	26.650612
209.427238	8298.875014	26.655629
209.591925	8302.530425	26.660647
209.495751	8316.433710	26.665664
210.009146	8327.955746	26.670682
210.339574	8337.050201	26.675700
210.461453	8350.167953	26.680717
210.443869	8357.488953	26.685735
210.727462	8381.959729	26.690752
210.680395	8383.643543	26.695770
210.654296	8399.436513	26.700788
210.669152	8415.466181	26.705805
211.054876	8429.057272	26.710823
211.056834	8448.419784	26.715840
211.833482	8466.530694	26.720858
212.161507	8484.500371	26.725876
212.388850	8496.976588	26.730893
212.599426	8507.902114	26.735911
212.543614	8523.652487	26.740928
212.662132	8529.591495	26.745946
213.178291	8545.015495	26.750964
213.381298	8553.969002	26.755981
213.766102	8572.621291	26.760999
213.671695	8584.484964	26.766016
213.927461	8589.319578	26.771034
214.322087	8603.304049	26.776052
214.237275	8609.025518	26.781069
215.076551	8638.388458	26.786087
215.012351	8639.465642	26.791104
215.266071	8642.835655	26.796122
215.258315	8652.961973	26.801140
215.307054	8666.684959	26.806157
215.669742	8674.811583	26.811175
215.710689	8701.552929	26.816192
216.042102	8704.632949	26.821210
216.402099	8717.075904	26.826228
216.140146	8743.141763	26.831245
216.726908	8748.514963	26.836263
216.910562	8774.362669	26.841280
217.393123	8778.495632	26.846298
217.477993	8794.618848	26.851316
217.303676	8808.635773	26.856333
217.719756	8823.580002	26.861351
218.071406	8831.973630	26.866368
218.113790	8851.349174	26.871386
218.325795	8866.704273	26.876404
219.023850	8882.043230	26.881421
218.992263	8891.911361	26.886439
219.508992	8907.086153	26.891456
219.640652	8919.268235	26.896474
219.592860	8919.402009	26.901492
219.688229	8937.632737	26.906509
219.873713	8952.123821	26.911527
220.451753	8967.049108	26.916544
220.767942	8982.410083	26.921562
221.279652	8994.368500	26.926580
220.965821	9012.079315	26.931597
221.027713	9008.700829	26.936615
221.838584	9030.112573	26.941632
221.940190	9030.952269	26.946650
222.163644	9042.460185	26.951668
221.898266	9071.510648	26.956685
222.317981	9075.356740	26.961703
222.341292	9096.939297	26.966720
222.450474	9120.494348	26.971738
222.910273	9127.393567	26.976756
222.720360	9156.119769	26.981773
223.323702	9164.527793	26.986791
223.583053	9190.673634	26.991808
223.740424	9193.796787	26.996826
224.011597	9211.700302	27.001844
224.162894	9232.748328	27.006861
224.631784	9238.162239	27.011879
224.726550	9260.813584	27.016896
225.057006	9259.849356	27.021914
225.159156	9285.274835	27.026932
225.660306	9296.985676	27.031949
226.019397	9309.138699	27.036967
226.024132	9329.581492	27.041984
225.997507	9338.722903	27.047002
226.829607	9348.099198	27.052020
226.412966	9359.189787	27.057037
226.694093	9368.106192	27.062055
227.040703	9384.899311	27.067072
227.009161	9406.014064	27.072090
227.440905	9417.701124	27.077108
227.544653	9438.437943	27.082125
227.898349	9450.478241	27.087143
228.032357	9466.531194	27.092160
228.438015	9474.986116	27.097178
228.666039	9491.488491	27.102196
228.673921	9508.205335	27.107213
229.026999	9510.360155	27.112231
229.403919	9528.799943	27.117248
229.328176	9524.713581	27.122266
229.751435	9551.670946	27.127284
229.677336	9569.114247	27.132301
230.071366	9580.507370	27.137319
230.300479	9589.485704	27.142336
230.477679	9606.447644	27.147354
230.999050	9619.247964	27.152372
231.179717	9639.546715	27.157389
231.359001	9648.062437	27.162407
231.295968	9660.701747	27.167424
231.717259	9675.772141	27.172442
231.719005	9695.347529	27.177460
231.830984	9714.176315	27.182477
232.292774	9734.254316	27.187495
232.408484	9746.047924	27.192512
232.853984	9768.758608	27.197530
233.457678	9783.374269	27.202548
233.268881	9807.924084	27.207565
233.610099	9808.571567	27.212583
233.622193	9827.561356	27.217600
233.955166	9846.197786	27.222618
234.366414	9854.408886	27.227636
234.353558	9882.221241	27.232653
234.894025	9896.003870	27.237671
235.119674	9913.207934	27.242688
235.537149	9926.514141	27.247706
235.800599	9930.375421	27.252724
236.042285	9954.659075	27.257741
236.148266	9964.307306	27.262759
236.435654	9978.060179	27.267776
236.210302	9995.271821	27.272794
237.121780	10011.579183	27.277812
236.813660	10023.594075	27.282829
237.305864	10031.650488	27.287847
237.377022	10044.622668	27.292864
237.600176	10060.188554	27.297882
238.128687	10080.786925	27.302900
238.057208	10101.757165	27.307917
238.220863	10111.592198	27.312935
238.535389	10137.613899	27.317952
238.974796	10156.278171	27.322970
239.176047	10165.163267	27.327988
239.038366	10191.022232	27.333005
239.733344	10193.843472	27.338023
239.566153	10219.457661	27.343040
239.911651	10234.887701	27.348058
239.972202	10251.104396	27.353076
240.598470	10269.827918	27.358093
240.745876	10284.136557	27.363111
241.121564	10301.238538	27.368128
241.104813	10313.735268	27.373146
241.592076	10335.761245	27.378164
241.661484	10348.598139	27.383181
241.918116	10364.616869	27.388199
242.551120	10387.210524	27.393216
242.369317	10403.105364	27.398234
243.275741	10424.017496	27.403252
243.477281	10439.609187	27.408269
243.379051	10438.765734	27.413287
243.831640	10456.765169	27.418304
244.080325	10465.788222	27.423322
244.167237	10471.006577	27.428340
244.418248	10495.491553	27.433357
244.920510	10502.299382	27.438375
244.790134	10501.558845	27.443392
244.871400	10523.206594	27.448410
245.221447	10527.417546	27.453428
245.331604	10540.065053	27.458445
245.523466	10563.249017	27.463463
245.826623	10577.587160	27.468480
245.831612	10592.603526	27.473498
246.316067	10605.722905	27.478516
246.557581	10621.179027	27.483533
246.612658	10639.360895	27.488551
247.130816	10663.172736	27.493568
247.565284	10676.779940	27.498586
247.589850	10684.736230	27.503604
247.539255	10711.002222	27.508621
247.778669	10723.815899	27.513639
248.303806	10745.015465	27.518656
248.121273	10760.860200	27.523674
248.523785	10776.976418	27.528692
248.468508	10805.118860	27.533709
248.666687	10819.097883	27.538727
249.463903	10839.178208	27.543744
249.376596	10864.837600	27.548762
249.723085	10880.463788	27.553780
249.973766	10900.702419	27.558797
250.208184	10928.862815	27.563815
250.567476	10949.908613	27.568832
251.065184	10972.918869	27.573850
251.403700	10975.183502	27.578868
251.303924	11003.099550	27.583885
251.550626	11018.463618	27.588903
252.125130	11032.740656	27.593920
252.397066	11054.981196	27.598938
252.628492	11071.373919	27.603956
252.922935	11090.753348	27.608973
252.913107	11103.950508	27.613991
253.395534	11114.743409	27.619008
253.688541	11136.140820	27.624026
253.841459	11158.706415	27.629044
254.493385	11177.344732	27.634061
254.383399	11192.726927	27.639079
254.703932	11204.009410	27.644096
254.783950	11225.380294	27.649114
255.262130	11241.466113	27.654132
255.513409	11259.027369	27.659149
255.923952	11269.597956	27.664167
256.155277	11276.786379	27.669184
256.000170	11290.401132	27.674202
256.468067	11309.087354	27.679220
256.686155	11331.409283	27.684237
256.696990	11354.635215	27.689255
257.224076	11369.633567	27.694272
257.177212	11399.774373	27.699290
257.657586	11412.127648	27.704308
257.905013	11435.045058	27.709325
257.773802	11454.570484	27.714343
258.270792	11469.213658	27.719360
258.564717	11491.574419	27.724378
258.742402	11514.468117	27.729396
259.233388	11533.848792	27.734413
259.706504	11549.815678	27.739431
260.238167	11566.161800	27.744448
260.284323	11585.719573	27.749466
260.605283	11589.963744	27.754484
260.545824	11610.415924	27.759501
260.922565	11620.142586	27.764519
261.528139	11645.517670	27.769536
261.450389	11657.402784	27.774554
261.833780	11670.737678	27.779572
262.117717	11683.554510	27.784589
262.203393	11695.328789	27.789607
262.507304	11704.789026	27.794624
262.490483	11727.053492	27.799642
262.752237	11740.802204	27.804660
262.959255	11755.964683	27.809677
263.433460	11768.489677	27.814695
263.701477	11778.915519	27.819712
263.510387	11802.003118	27.824730
264.208267	11822.526354	27.829748
264.087712	11845.981884	27.834765
264.244817	11873.884243	27.839783
265.020082	11886.005330	27.844800
265.383526	11910.146135	27.849818
265.493178	11918.692746	27.854836
265.853020	11945.761388	27.859853
265.644048	11960.528166	27.864871
266.196553	11972.886301	27.869888
266.580030	12001.902810	27.874906
266.495083	12017.477536	27.879924
266.879295	12035.397625	27.884941
267.236132	12058.636536	27.889959
267.773779	12070.763389	27.894976
268.040657	12099.100446	27.899994
268.062424	12109.666096	27.905012
268.511828	12124.314079	27.910029
268.861555	12152.792969	27.915047
269.332742	12170.955343	27.920064
269.255467	12177.390377	27.925082
269.362008	12190.664803	27.930100
269.773247	12212.745948	27.935117
269.788842	12226.239901	27.940135
270.637967	12248.179864	27.945152
270.948730	12279.914423	27.950170
270.933864	12289.279632	27.955188
271.624866	12307.350863	27.960205
271.408297	12325.959009	27.965223
271.938426	12333.457862	27.970240
272.199654	12360.697280	27.975258
272.296299	12371.513445	27.980276
272.475950	12385.152335	27.985293
272.648397	12415.127779	27.990311
273.046838	12428.366119	27.995328
273.339154	12458.487061	28.000346
273.393627	12469.335151	28.005364
273.828642	12483.256208	28.010381
274.083145	12515.821014	28.015399
274.556323	12537.517054	28.020416
274.410695	12558.463751	28.025434
274.658282	12578.755199	28.030452
275.045388	12603.332127	28.035469
275.177857	12631.523672	28.040487
276.023481	12636.759565	28.045504
276.043264	12655.362588	28.050522
276.351636	12679.699320	28.055540
276.776107	12698.460042	28.060557
276.681329	12725.556808	28.065575
277.031838	12739.450240	28.070592
277.397128	12761.873961	28.075610
277.775293	12786.155687	28.080628
278.492808	12800.256934	28.085645
278.329505	12822.097216	28.090663
279.129844	12836.185517	28.095680
278.977215	12852.939953	28.100698
279.360460	12881.190482	28.105716
279.555906	12889.364093	28.110733
279.646228	12917.970037	28.115751
279.997764	12928.964488	28.120768
280.168912	12937.584033	28.125786
280.525949	12958.550326	28.130804
280.945122	12971.447903	28.135821
280.638350	12999.029851	28.140839
281.460151	13018.578131	28.145856
281.598509	13045.487253	28.150874
282.060820	13051.721215	28.155892
282.092610	13060.005800	28.160909
282.104986	13090.856873	28.165927
282.970367	13115.706919	28.170944
282.933096	13139.277322	28.175962
283.225304	13155.949711	28.180980
283.231775	13164.582524	28.185997
283.724049	13194.787002	28.191015
284.104013	13209.933032	28.196032
284.746798	13235.724439	28.201050
284.510091	13254.775606	28.206068
285.273270	13270.262715	28.211085
285.315899	13295.178721	28.216103
285.296761	13307.093585	28.221120
286.018747	13336.280175	28.226138
286.047009	13358.684765	28.231156
286.200556	13369.347320	28.236173
286.596631	13409.205375	28.241191
286.657549	13431.784941	28.246208
286.986896	13448.448612	28.251226
287.260374	13471.563367	28.256244
287.944680	13497.797063	28.261261
287.971897	13519.084073	28.266279
288.486343	13547.984541	28.271296
288.953953	13572.543801	28.276314
288.944156	13587.820665	28.281332
289.505183	13611.307406	28.286349
289.771878	13637.294069	28.291367
290.024445	13652.160396	28.296384
290.266239	13661.394495	28.301402
290.520518	13693.598187	28.306420
290.934990	13705.028514	28.311437
291.141755	13733.601657	28.316455
291.281059	13750.503794	28.321472
291.880166	13768.467658	28.326490
291.975451	13797.219420	28.331508
292.696955	13810.086000	28.336525
292.871118	13837.098010	28.341543
292.743335	13860.209776	28.346560
293.229859	13879.922001	28.351578
293.296689	13895.174476	28.356596
294.146747	13910.541128	28.361613
294.118928	13944.311625	28.366631
294.221057	13963.446220	28.371648
294.477167	13973.805663	28.376666
294.942439	14009.065443	28.381684
295.419638	14017.050133	28.386701
295.658420	14050.299026	28.391719
296.279603	14068.654479	28.396736
296.313320	14083.151190	28.401754
296.245886	14105.407428	28.406772
296.430601	14127.374704	28.411789
296.520149	14152.196055	28.416807
297.106457	14168.826423	28.421824
297.603209	14198.924421	28.426842
297.670871	14222.362878	28.431860
298.423132	14246.524710	28.436877
298.455900	14264.631449	28.441895
298.943836	14290.325381	28.446912
299.131218	14300.755773	28.451930
299.327054	14328.093530	28.456948
299.877041	14336.269073	28.461965
300.145537	14371.740364	28.466983
300.050829	14380.487481	28.472000
300.317991	14407.498364	28.477018
300.525989	14429.774998	28.482036
300.985380	14440.017581	28.487053
301.541922	14462.915502	28.492071
301.768125	14485.170401	28.497088
302.133491	14514.818913	28.502106
301.918386	14531.287744	28.507124
302.242657	14555.378052	28.512141
302.582676	14585.425418	28.517159
302.940526	14608.278842	28.522176
303.479578	14627.645688	28.527194
303.561629	14656.340813	28.532212
304.080297	14672.176877	28.537229
304.448243	14694.747743	28.542247
304.662446	14720.677786	28.547264
304.940644	14736.760014	28.552282
304.994405	14766.603007	28.557300
305.534659	14781.011426	28.562317
305.973047	14808.668755	28.567335
306.073775	14838.109725	28.572352
306.197101	14868.583101	28.577370
306.588618	14895.174098	28.582388
307.135708	14916.036983	28.587405
307.552145	14937.094060	28.592423
307.559841	14960.830216	28.597440
307.732818	14980.826409	28.602458
308.014577	15016.549479	28.607476
309.074006	15042.865511	28.612493
309.129013	15061.872784	28.617511
309.127808	15081.368937	28.622528
309.598695	15114.248549	28.627546
309.708601	15139.677540	28.632564
310.450388	15160.914454	28.637581
310.743452	15188.377176	28.642599
310.845553	15214.862357	28.647616
311.377662	15234.249858	28.652634
311.789865	15254.591016	28.657652
311.889231	15277.773136	28.662669
312.244676	15297.554738	28.667687
312.658580	15329.265599	28.672704
313.151983	15342.816406	28.677722
313.456706	15361.952250	28.682740
313.680175	15389.062956	28.687757
313.757341	15410.843263	28.692775
314.169063	15438.363556	28.697792
314.505833	15451.841069	28.702810
314.723113	15481.485853	28.707828
314.839402	15510.849620	28.712845
315.713875	15524.672489	28.717863
315.774597	15551.303583	28.722880
315.926321	15571.013154	28.727898
316.058485	15602.020072	28.732916
316.735872	15618.119470	28.737933
316.920543	15644.282791	28.742951
317.076499	15669.443128	28.747968
317.906743	15682.704535	28.752986
317.843098	15717.276523	28.758004
318.075023	15733.265770	28.763021
318.364322	15761.860602	28.768039
318.822504	15793.230507	28.773056
319.264034	15810.601941	28.778074
319.215777	15839.868809	28.783092
319.772841	15861.621830	28.788109
320.239891	15895.381418	28.793127
320.386536	15924.829498	28.798144
320.882913	15944.886582	28.803162
321.096181	15962.666602	28.808180
321.271368	15975.058033	28.813197
321.620955	15998.242887	28.818215
322.034724	16026.629110	28.823232
322.293730	16040.479279	28.828250
322.297122	16073.683283	28.833268
322.725801	16089.376699	28.838285
323.171190	16114.890244	28.843303
323.597094	16140.631124	28.848320
323.693316	16158.129608	28.853338
324.019607	16190.670496	28.858356
324.576798	16213.481977	28.863373
324.847532	16231.281670	28.868391
324.898918	16268.887698	28.873408
325.331941	16288.320214	28.878426
325.323202	16314.963247	28.883444
325.969455	16335.821623	28.888461
326.165699	16373.961055	28.893479
326.316244	16406.750931	28.898496
326.910032	16433.653496	28.903514
327.196719	16468.358304	28.908532
327.292562	16502.028656	28.913549
327.820317	16520.372678	28.918567
328.410938	16563.251632	28.923584
328.722268	16579.071220	28.928602
329.076864	16606.823232	28.933620
329.384107	16633.170843	28.938637
330.224664	16647.963190	28.943655
330.305289	16682.748041	28.948672
330.556655	16703.125406	28.953690
330.900571	16735.977149	28.958708
331.082008	16757.079354	28.963725
331.830436	16782.972719	28.968743
331.655225	16796.218679	28.973760
332.182982	16822.503580	28.978778
332.667538	16845.718851	28.983796
332.840753	16869.355629	28.988813
333.203252	16898.654518	28.993831
333.163119	16925.369640	28.998848
334.061424	16952.064142	29.003866
333.826703	16983.718249	29.008884
334.168212	17007.695229	29.013901
334.305136	17038.842692	29.018919
334.943865	17072.242642	29.023936
335.003424	17097.363089	29.028954
335.713258	17130.050792	29.033972
336.060617	17157.747876	29.038989
336.283622	17186.273084	29.044007
336.375526	17218.198588	29.049024
336.976465	17251.415251	29.054042
337.690641	17284.854288	29.059060
337.594474	17304.402311	29.064077
338.368848	17325.121663	29.069095
338.224166	17361.639215	29.074112
338.729896	17387.492444	29.079130
338.775911	17418.939037	29.084148
339.245288	17458.203366	29.089165
340.051406	17476.245687	29.094183
340.574221	17508.609557	29.099200
340.741759	17525.633785	29.104218
340.893366	17559.748933	29.109236
341.398990	17590.965877	29.114253
342.087588	17616.083223	29.119271
342.090445	17639.229603	29.124288
342.280229	17655.435520	29.129306
342.929273	17678.322793	29.134324
342.850642	17701.538868	29.139341
343.302155	17719.396902	29.144359
343.743997	17750.605142	29.149376
344.142096	17769.330756	29.154394
344.546757	17784.568145	29.159412
344.894703	17806.201346	29.164429
345.206866	17826.191326	29.169447
345.649793	17862.516697	29.174464
345.778785	17878.934482	29.179482
346.132293	17898.867521	29.184500
346.011914	17923.802432	29.189517
346.548459	17945.867421	29.194535
346.825780	17979.243423	29.199552
347.239834	18005.036028	29.204570
347.630966	18039.209262	29.209588
347.723958	18066.404185	29.214605
348.474108	18094.127961	29.219623
348.525613	18123.805930	29.224640
348.953862	18159.533991	29.229658
349.395358	18181.614137	29.234676
349.713347	18206.449156	29.239693
350.180760	18239.852687	29.244711
350.595155	18280.176011	29.249728
351.058636	18289.762988	29.254746
351.574961	18322.539877	29.259764
351.574150	18351.739935	29.264781
352.090803	18372.090138	29.269799
351.943196	18411.870006	29.274816
352.635096	18431.106189	29.279834
353.149004	18456.523649	29.284852
353.458848	18500.445906	29.289869
354.049512	18524.139347	29.294887
354.259627	18544.449300	29.299904
354.741308	18569.676108	29.304922
354.743959	18598.162096	29.309940
355.033330	18625.661877	29.314957
355.583645	18646.998973	29.319975
355.655413	18684.110554	29.324992
356.050514	18709.313199	29.330010
356.464632	18744.438047	29.335028
356.715776	18777.535222	29.340045
357.156761	18796.179297	29.345063
357.317198	18841.136565	29.350080
357.512750	18875.809419	29.355098
358.341088	18900.521158	29.360116
358.140030	18936.298678	29.365133
358.905706	18966.453618	29.370151
359.225416	19005.649754	29.375168
359.894022	19040.912173	29.380186
360.013604	19064.395761	29.385204
360.237641	19085.992936	29.390221
360.944017	19122.153036	29.395239
361.007580	19164.333732	29.400256
361.352504	19190.574671	29.405274
361.837101	19221.570087	29.410292
362.242348	19249.842333	29.415309
362.828961	19276.127662	29.420327
363.054729	19319.104611	29.425344
363.329899	19341.205810	29.430362
364.528018	19367.812459	29.435380
364.449502	19398.277204	29.440397
364.863523	19423.142957	29.445415
365.306310	19452.780612	29.450432
365.440806	19481.127194	29.455450
365.659021	19508.601458	29.460468
366.020185	19542.845204	29.465485
366.659705	19556.044394	29.470503
366.896661	19591.855590	29.475520
367.199655	19620.194933	29.480538
367.595390	19636.686141	29.485556
367.373206	19669.094488	29.490573
367.958776	19694.287525	29.495591
368.462446	19726.778129	29.500608
368.443228	19757.682725	29.505626
368.981312	19783.224490	29.510644
369.424323	19816.716682	29.515661
369.809062	19841.720234	29.520679
370.134262	19881.966069	29.525696
370.371421	19897.041810	29.530714
370.750812	19937.026545	29.535732
371.107621	19972.080443	29.540749
371.296722	20005.341049	29.545767
371.958244	20041.800513	29.550784
372.248777	20068.101695	29.555802
372.903088	20108.928260	29.560820
372.743813	20145.680758	29.565837
373.529149	20180.099267	29.570855
373.472250	20217.638274	29.575872
373.819530	20244.354123	29.580890
374.433091	20277.409704	29.585908
374.496152	20311.827852	29.590925
374.906653	20351.701150	29.595943
375.822944	20395.715900	29.600960
375.920017	20422.060496	29.605978
376.482770	20461.467889	29.610996
376.507140	20500.688006	29.616013
377.220925	20526.651818	29.621031
377.602649	20562.859118	29.626048
377.940598	20609.751316	29.631066
378.894873	20634.565575	29.636084
378.757707	20666.058725	29.641101
379.213329	20691.507179	29.646119
379.419317	20728.051909	29.651136
380.287292	20773.035466	29.656154
380.653739	20805.764178	29.661172
380.795623	20831.135588	29.666189
381.297346	20862.453156	29.671207
381.522315	20905.149375	29.676224
382.163924	20936.116591	29.681242
382.469416	20962.081750	29.686260
382.898832	20996.279430	29.691277
383.119783	21036.525003	29.696295
383.833741	21073.970170	29.701312
383.412711	21097.218629	29.706330
384.637051	21131.595317	29.711348
384.892075	21170.072965	29.716365
385.156508	21196.373426	29.721383
385.638898	21235.763366	29.726400
385.686747	21264.429380	29.731418
386.269974	21293.567609	29.736436
386.669544	21327.094454	29.741453
387.157518	21355.540016	29.746471
387.392899	21395.840928	29.751488
387.660421	21427.745796	29.756506
388.274316	21452.519628	29.761524
388.806637	21496.982424	29.766541
388.948005	21529.608583	29.771559
389.536474	21560.275492	29.776576
389.575175	21604.455686	29.781594
390.143426	21625.673168	29.786612
390.420530	21660.906843	29.791629
391.377524	21702.251666	29.796647
391.659523	21730.268767	29.801664
391.715516	21763.420499	29.806682
392.205967	21794.216861	29.811700
392.600641	21831.353312	29.816717
392.873510	21860.503080	29.821735
393.361040	21877.234541	29.826752
393.146620	21920.823215	29.831770
393.684434	21949.192319	29.836788
394.051596	21982.472602	29.841805
394.393598	22013.829654	29.846823
395.052978	22052.384695	29.851840
395.177092	22087.624138	29.856858
395.398595	22124.440729	29.861876
395.798352	22161.703380	29.866893
396.071316	22202.878365	29.871911
397.016791	22236.915216	29.876928
396.848924	22279.037729	29.881946
397.338534	22322.466457	29.886964
398.019665	22362.080266	29.891981
398.130208	22403.268471	29.896999
398.346082	22438.930168	29.902016
399.082388	22481.265343	29.907034
399.719537	22516.564204	29.912052
400.477247	22561.069912	29.917069
400.659199	22603.555370	29.922087
401.101089	22634.518620	29.927104
401.780527	22666.841205	29.932122
401.921779	22695.437788	29.937140
402.379545	22740.054070	29.942157
402.487372	22769.761821	29.947175
403.259799	22801.773068	29.952192
403.492131	22834.298658	29.957210
404.007397	22871.633015	29.962228
404.291020	22919.139507	29.967245
404.618828	22942.948967	29.972263
405.058203	22981.104259	29.977280
405.550236	23017.589452	29.982298
406.228166	23058.955544	29.987316
406.413209	23086.490537	29.992333
406.723570	23132.994930	29.997351
407.154815	23163.651034	30.002368
407.600893	23198.690355	30.007386
408.036051	23233.731448	30.012404
408.295927	23273.495207	30.017421
408.624096	23313.513755	30.022439
409.142526	23352.472551	30.027456
409.248802	23398.996891	30.032474
410.057371	23443.370225	30.037492
410.099587	23480.748224	30.042509
410.584854	23514.088404	30.047527
411.216534	23546.489413	30.052544
411.440140	23597.343492	30.057562
412.007595	23643.202153	30.062580
412.219126	23685.015437	30.067597
412.631256	23716.452660	30.072615
413.252827	23761.374176	30.077632
413.365423	23808.113336	30.082650
414.349930	23843.284311	30.087668
414.419800	23886.390396	30.092685
414.959768	23927.280669	30.097703
415.529897	23969.954691	30.102720
416.040327	24005.250763	30.107738
416.375866	24036.125420	30.112756
416.726511	24074.909685	30.117773
416.945495	24111.464926	30.122791
417.386570	24150.993508	30.127808
418.030571	24196.487559	30.132826
418.630931	24226.903945	30.137844
419.051499	24268.477163	30.142861
419.167056	24302.236778	30.147879
419.932905	24340.476241	30.152896
420.041408	24384.917084	30.157914
420.695216	24410.389825	30.162932
420.780290	24446.650676	30.167949
421.534175	24473.498123	30.172967
421.979605	24504.337330	30.177984
422.261030	24540.024112	30.183002
422.607609	24567.472647	30.188020
423.098729	24606.950052	30.193037
423.507556	24640.759095	30.198055
423.859241	24665.925586	30.203072
423.970942	24709.330229	30.208090
424.572234	24742.205590	30.213108
425.095634	24779.668633	30.218125
425.171348	24824.374690	30.223143
425.650698	24854.425484	30.228160
425.999482	24907.247658	30.233178
426.696042	24950.485377	30.238196
426.816492	24981.749084	30.243213
426.721371	25021.609836	30.248231
427.775855	25070.100323	30.253248
427.923640	25114.372313	30.258266
428.166410	25148.359894	30.263284
428.659258	25199.618247	30.268301
429.223656	25247.629785	30.273319
429.541657	25288.999988	30.278336
430.188311	25344.696408	30.283354
430.769724	25384.388712	30.288372
431.239456	25429.849656	30.293389
431.588521	25473.351484	30.298407
432.324821	25514.896786	30.303424
432.620174	25557.882659	30.308442
433.600542	25605.823577	30.313460
433.580343	25643.613531	30.318477
434.262492	25679.536603	30.323495
434.485768	25716.119369	30.328512
434.862637	25768.920443	30.333530
435.550147	25801.626032	30.338548
435.723226	25828.307146	30.343565
435.812700	25882.771448	30.348583
436.873623	25927.698516	30.353600
437.229791	25969.866778	30.358618
437.338137	26008.648484	30.363636
438.186334	26058.184870	30.368653
438.665810	26095.334918	30.373671
439.493006	26131.627921	30.378688
439.389000	26165.475608	30.383706
439.905905	26199.308260	30.388724
440.112469	26245.558033	30.393741
440.255947	26299.964437	30.398759
441.169175	26338.551184	30.403776
441.329252	26383.323320	30.408794
441.577991	26426.615388	30.413812
442.182776	26472.752744	30.418829
442.848676	26519.392569	30.423847
443.220427	26570.471122	30.428864
443.816025	26609.076535	30.433882
444.107466	26646.219125	30.438900
444.700479	26688.503472	30.443917
445.064222	26733.971310	30.448935
445.539663	26772.374645	30.453952
446.367593	26823.325501	30.458970
446.790105	26864.998573	30.463988
446.955828	26904.272308	30.469005
447.528963	26946.705675	30.474023
448.415477	26980.747194	30.479040
448.785679	27026.593896	30.484058
448.952975	27064.009509	30.489076
449.412029	27089.155884	30.494093
449.798425	27138.817810	30.499111
450.442963	27167.620018	30.504128
450.683311	27213.797181	30.509146
450.865350	27236.724420	30.514164
451.577853	27283.181730	30.519181
451.659213	27322.406282	30.524199
452.257891	27347.411019	30.529216
452.735853	27390.662918	30.534234
452.703512	27428.104149	30.539252
453.509345	27465.268795	30.544269
453.799303	27524.471749	30.549287
454.391790	27550.735488	30.554304
454.854665	27608.963525	30.559322
455.396236	27644.532871	30.564340
455.783587	27676.460511	30.569357
456.138318	27719.650243	30.574375
456.351103	27765.706562	30.579392
457.041465	27817.718034	30.584410
457.145744	27867.229983	30.589428
458.078859	27903.269385	30.594445
458.051766	27953.560596	30.599463
458.659878	27999.795707	30.604480
459.285018	28058.246117	30.609498
459.216732	28105.029858	30.614516
459.957961	28138.653624	30.619533
460.374824	28191.258787	30.624551
460.803818	28245.524537	30.629568
461.486585	28289.839751	30.634586
462.048999	28356.378753	30.639604
462.580034	28395.711915	30.644621
462.885265	28442.393677	30.649639
463.620310	28492.914483	30.654656
464.102944	28538.020078	30.659674
464.513973	28584.533893	30.664692
465.220430	28632.050803	30.669709
465.495641	28677.732787	30.674727
465.852601	28720.361726	30.679744
466.248056	28762.472732	30.684762
466.743700	28820.560027	30.689780
467.505310	28868.106771	30.694797
467.618736	28913.264700	30.699815
468.297648	28953.132013	30.704832
468.919540	29012.148220	30.709850
469.213588	29053.156894	30.714868
469.799223	29105.434561	30.719885
470.473518	29147.268806	30.724903
470.855182	29190.419496	30.729920
471.287827	29232.506678	30.734938
471.658086	29290.545410	30.739956
472.081698	29325.636791	30.744973
472.387576	29383.268679	30.749991
473.043634	29433.962202	30.755008
473.598457	29470.556665	30.760026
474.081689	29526.732605	30.765044
474.631326	29568.776866	30.770061
474.899999	29614.070045	30.775079
475.124002	29666.228787	30.780096
475.821557	29714.065654	30.785114
476.107430	29763.522127	30.790132
476.725507	29811.371669	30.795149
476.775122	29861.415327	30.800167
477.345429	29912.907293	30.805184
477.901284	29956.462149	30.810202
478.618320	30019.986044	30.815220
479.431926	30067.540061	30.820237
479.964456	30122.837565	30.825255
480.287266	30170.841649	30.830272
481.124647	30210.920470	30.835290
480.817675	30257.126994	30.840308
482.128397	30302.555575	30.845325
482.260128	30351.614068	30.850343
482.779177	30378.619895	30.855360
483.412783	30422.662947	30.860378
483.869070	30473.011030	30.865396
484.443550	30504.635618	30.870413
484.844625	30546.085640	30.875431
485.365781	30587.744510	30.880448
485.943619	30622.516835	30.885466
486.291248	30662.464632	30.890484
486.852767	30697.745357	30.895501
487.110533	30747.537304	30.900519
487.346816	30786.308016	30.905536
488.188706	30833.713973	30.910554
488.450099	30872.613666	30.915572
488.702271	30924.815421	30.920589
489.026917	30970.892999	30.925607
489.689288	31019.364235	30.930624
489.961163	31069.654150	30.935642
490.408781	31130.947878	30.940660
490.970745	31188.285500	30.945677
491.532412	31238.511470	30.950695
491.928748	31280.045884	30.955712
492.584670	31336.724390	30.960730
493.052491	31397.901951	30.965748
493.427479	31445.932424	30.970765
493.754090	31502.239405	30.975783
494.521020	31556.511509	30.980800
495.205513	31611.985159	30.985818
495.209088	31662.640940	30.990836
496.337633	31705.629322	30.995853
496.650183	31763.500694	31.000871
496.830044	31819.376347	31.005888
497.888870	31867.060456	31.010906
498.271579	31912.954015	31.015924
499.021409	31969.328730	31.020941
499.096355	32022.932843	31.025959
499.576005	32076.555891	31.030976
500.298029	32131.563547	31.035994
500.834651	32186.088311	31.041012
501.433815	32228.225041	31.046029
502.214245	32290.272942	31.051047
502.668618	32338.760864	31.056064
503.260600	32381.777785	31.061082
503.216880	32433.827360	31.066100
504.204025	32485.683996	31.071117
504.520742	32530.109893	31.076135
504.816634	32578.047886	31.081152
505.300648	32625.545590	31.086170
505.405378	32688.579272	31.091188
505.981988	32739.002501	31.096205
507.108455	32793.992811	31.101223
507.141677	32846.208379	31.106240
507.764739	32899.084029	31.111258
508.116402	32952.691437	31.116276
508.848721	32998.747575	31.121293
509.120000	33058.430816	31.126311
509.459616	33113.640038	31.131328
510.753038	33161.081728	31.136346
510.666409	33224.172279	31.141364
511.412754	33276.049622	31.146381
511.934001	33338.463660	31.151399
512.524906	33385.623908	31.156416
512.811653	33439.666320	31.161434
513.505830	33495.408988	31.166452
514.316915	33545.316935	31.171469
514.849910	33597.323323	31.176487
515.422301	33646.820009	31.181504
515.699411	33690.363110	31.186522
515.698614	33740.556739	31.191540
516.234284	33787.220746	31.196557
516.986095	33850.068050	31.201575
517.268442	33905.212450	31.206592
518.131234	33945.376672	31.211610
518.283134	34004.297307	31.216628
519.079573	34050.971636	31.221645
519.535393	34101.581440	31.226663
519.668848	34148.966786	31.231680
520.640816	34200.716235	31.236698
521.018246	34252.552607	31.241716
521.371542	34309.160106	31.246733
522.072631	34362.501409	31.251751
522.244966	34419.554837	31.256768
522.739044	34472.517871	31.261786
523.334896	34539.425489	31.266804
523.727401	34591.121231	31.271821
524.533577	34649.011759	31.276839
525.134961	34714.509108	31.281856
525.560285	34766.358206	31.286874
525.783166	34830.966789	31.291892
526.453656	34895.827925	31.296909
527.300328	34954.819428	31.301927
527.594643	35014.561499	31.306944
528.234770	35072.662553	31.311962
528.563688	35127.701681	31.316980
529.621026	35189.872836	31.321997
530.308047	35242.700089	31.327015
530.325681	35301.891954	31.332032
531.446031	35352.059234	31.337050
531.706593	35416.537241	31.342068
532.077237	35470.849912	31.347085
533.008424	35517.506376	31.352103
533.173643	35591.389405	31.357120
534.150965	35637.931417	31.362138
534.151478	35709.937440	31.367156
534.732820	35760.727561	31.372173
535.727109	35814.709483	31.377191
536.388815	35870.855527	31.382208
537.025239	35926.354405	31.387226
537.698128	35980.285917	31.392244
537.991243	36036.464834	31.397261
538.818373	36072.288397	31.402279
538.981067	36145.446585	31.407296
539.594832	36194.424250	31.412314
539.878205	36244.376953	31.417332
540.518467	36303.581578	31.422349
541.401096	36353.364803	31.427367
541.607551	36408.439069	31.432384
542.158325	36457.408233	31.437402
542.659212	36520.865519	31.442420
543.338256	36574.102013	31.447437
543.771756	36632.404092	31.452455
544.067485	36695.160528	31.457472
544.700611	36750.453397	31.462490
545.449762	36804.071528	31.467508
545.686034	36864.883870	31.472525
546.594168	36923.498128	31.477543
546.946029	36987.580856	31.482560
547.321528	37028.820008	31.487578
547.890100	37094.304522	31.492596
548.274255	37153.165882	31.497613
548.915227	37211.013373	31.502631
549.451956	37275.472707	31.507648
550.198610	37334.341025	31.512666
550.700207	37394.923609	31.517684
551.212656	37462.093760	31.522701
551.967800	37511.924943	31.527719
552.405806	37573.042842	31.532736
553.077125	37615.444587	31.537754
553.823100	37666.055361	31.542772
554.018367	37724.890959	31.547789
554.633768	37764.911441	31.552807
554.852405	37823.300995	31.557824
555.792907	37881.350001	31.562842
555.914924	37939.457792	31.567860
556.524200	37999.671091	31.572877
557.086369	38044.373621	31.577895
557.525341	38121.801702	31.582912
557.905639	38181.349440	31.587930
558.580307	38240.452843	31.592948
559.399534	38298.269017	31.597965
559.958726	38365.232304	31.602983
560.080151	38428.602885	31.608000
560.970689	38488.691290	31.613018
561.725810	38553.651447	31.618036
562.225020	38612.644225	31.623053
562.951549	38671.576267	31.628071
563.237969	38742.731899	31.633088
564.036857	38791.332358	31.638106
564.312265	38852.580530	31.643124
564.870580	38915.327607	31.648141
565.815849	38972.733762	31.653159
566.080441	39042.331782	31.658176
566.694318	39104.343448	31.663194
567.405731	39174.681383	31.668212
567.597674	39243.842422	31.673229
568.154035	39294.657461	31.678247
568.783131	39362.251613	31.683264
569.873694	39422.741323	31.688282
570.382675	39491.600534	31.693300
570.873628	39569.942648	31.698317
571.672632	39617.950476	31.703335
572.087894	39691.220275	31.708352
572.883993	39751.263733	31.713370
573.317070	39811.199783	31.718388
573.784755	39879.940208	31.723405
574.642327	39929.792548	31.728423
574.877649	39998.588712	31.733440
576.027631	40059.481965	31.738458
576.467564	40110.652333	31.743476
576.838163	40170.390455	31.748493
577.341457	40239.518544	31.753511
577.898294	40306.589380	31.758528
578.633156	40364.841685	31.763546
579.143062	40424.615605	31.768564
579.498726	40505.018717	31.773581
580.722941	40540.749582	31.778599
581.021153	40604.029247	31.783616
581.223842	40664.376864	31.788634
582.044091	40737.289501	31.793652
582.336944	40805.288636	31.798669
583.149169	40870.038066	31.803687
583.619731	40933.076657	31.808704
584.176638	40985.685394	31.813722
584.860192	41059.796877	31.818740
585.503723	41119.216566	31.823757
586.066679	41182.032691	31.828775
586.512661	41247.732365	31.833792
586.824264	41312.972608	31.838810
587.556107	41382.694653	31.843828
588.139760	41458.790096	31.848845
589.267415	41510.703538	31.853863
589.563259	41582.391906	31.858880
590.209282	41647.365728	31.863898
590.861314	41695.824901	31.868916
591.238579	41769.942478	31.873933
591.916006	41825.924427	31.878951
592.102484	41880.136568	31.883968
593.007107	41943.236574	31.888986
593.637905	41996.886082	31.894004
593.820017	42060.264024	31.899021
594.989659	42123.019448	31.904039
595.384328	42197.717626	31.909056
595.996510	42256.032119	31.914074
596.188983	42311.983730	31.919092
596.787317	42379.136627	31.924109
597.443875	42436.597106	31.929127
597.980100	42510.293804	31.934144
598.664432	42572.449742	31.939162
599.214946	42643.083350	31.944180
599.541785	42722.056981	31.949197
600.342977	42783.518432	31.954215
600.983870	42856.687564	31.959232
601.640267	42929.291575	31.964250
602.383079	42983.628024	31.969268
602.703405	43063.849939	31.974285
603.538700	43136.021803	31.979303
603.996643	43212.617368	31.984320
605.100542	43277.081517	31.989338
605.488450	43356.345127	31.994356
606.077768	43426.159202	31.999373
606.874577	43494.087702	32.004391
607.093805	43558.077668	32.009408
608.056985	43633.267251	32.014426
609.002498	43696.422787	32.019444
609.138967	43765.372704	32.024461
609.671959	43828.884187	32.029479
610.420488	43893.291924	32.034496
611.143610	43980.007145	32.039514
612.010806	44043.334066	32.044532
612.395417	44121.506623	32.049549
613.244387	44183.995517	32.054567
613.581148	44249.183547	32.059584
614.227000	44309.528643	32.064602
614.713538	44381.727543	32.069620
615.284957	44464.034226	32.074637
615.998196	44529.606901	32.079655
616.742235	44605.833525	32.084672
617.031064	44675.572064	32.089690
618.005614	44746.778505	32.094708
618.441420	44824.420478	32.099725
619.270149	44879.855088	32.104743
620.106234	44953.816554	32.109760
620.416353	45027.936543	32.114778
621.183774	45090.023248	32.119796
621.440059	45171.053487	32.124813
621.912742	45241.846694	32.129831
623.036931	45315.473248	32.134848
623.976441	45383.075188	32.139866
624.690148	45451.212434	32.144884
624.594214	45517.408139	32.149901
625.460368	45585.736996	32.154919
626.293362	45665.508418	32.159936
626.948689	45735.939309	32.164954
627.761316	45794.927527	32.169972
628.229543	45866.305382	32.174989
628.462863	45930.470723	32.180007
629.268931	46009.665596	32.185024
629.976250	46072.612110	32.190042
630.916771	46146.624408	32.195060
631.230281	46217.863132	32.200077
631.692075	46279.184930	32.205095
632.461955	46349.100040	32.210112
632.959603	46418.906175	32.215130
633.696821	46476.541555	32.220148
634.165710	46545.555498	32.225165
634.638860	46605.193657	32.230183
635.202213	46672.029655	32.235200
635.425104	46740.133794	32.240218
636.190551	46809.298209	32.245236
636.918385	46890.874419	32.250253
637.349140	46964.134171	32.255271
638.208694	47039.781591	32.260288
638.719463	47121.544457	32.265306
639.415424	47184.982971	32.270324
640.183744	47264.086931	32.275341
640.539411	47334.449534	32.280359
641.119479	47417.208499	32.285376
641.503618	47500.960059	32.290394
642.752919	47571.607313	32.295412
643.045128	47655.259963	32.300429
643.721559	47747.285901	32.305447
644.733594	47821.001458	32.310464
645.142741	47892.274749	32.315482
645.994213	47974.727526	32.320500
646.786096	48058.436260	32.325517
647.261353	48135.798739	32.330535
647.667455	48211.672912	32.335552
648.665138	48298.697057	32.340570
649.366669	48381.307644	32.345588
649.755608	48461.069881	32.350605
650.648954	48531.434222	32.355623
650.959617	48613.157860	32.360640
651.705456	48692.510715	32.365658
652.137875	48771.950891	32.370676
653.337990	48861.779855	32.375693
653.850964	48943.510949	32.380711
654.504935	49020.930682	32.385728
655.093612	49109.078541	32.390746
656.061234	49184.690851	32.395764
656.737198	49271.104760	32.400781
657.245823	49350.402140	32.405799
658.073910	49420.773108	32.410816
658.543761	49516.299336	32.415834
659.621252	49591.357990	32.420852
660.228698	49662.801873	32.425869
660.710010	49749.785859	32.430887
661.417210	49817.937216	32.435904
662.044684	49905.949187	32.440922
662.914861	49980.959327	32.445940
663.220053	50061.233748	32.450957
663.791970	50143.934249	32.455975
664.824429	50226.132678	32.460992
665.079632	50311.180126	32.466010
666.395915	50381.357360	32.471028
666.826964	50469.187116	32.476045
667.117917	50551.148503	32.481063
667.861733	50624.174794	32.486080
668.751540	50711.876682	32.491098
669.519444	50791.423139	32.496116
669.839350	50871.672758	32.501133
670.396203	50952.163951	32.506151
671.428029	51032.701260	32.511168
672.013086	51122.629037	32.516186
672.593975	51201.168498	32.521204
673.376283	51288.610998	32.526221
673.831894	51368.739845	32.531239
675.018112	51444.407584	32.536256
675.503522	51530.998992	32.541274
675.645117	51608.045733	32.546292
676.458039	51686.828908	32.551309
677.015597	51755.015730	32.556327
677.936428	51845.311336	32.561344
678.379180	51925.020164	32.566362
679.270973	52001.564739	32.571380
680.064584	52079.542331	32.576397
680.352845	52165.432964	32.581415
681.170705	52233.953754	32.586432
681.747747	52315.313391	32.591450
682.466887	52400.928598	32.596468
683.239607	52480.397815	32.601485
683.772090	52565.321492	32.606503
684.822932	52642.722821	32.611520
685.362104	52737.441493	32.616538
685.897328	52804.027610	32.621556
686.871218	52897.887873	32.626573
687.644339	52978.953340	32.631591
688.509882	53054.474029	32.636608
688.752823	53151.253033	32.641626
689.419296	53229.235383	32.646644
690.125813	53309.489788	32.651661
691.125352	53397.994575	32.656679
692.044675	53470.432776	32.661696
692.533566	53560.239449	32.666714
693.012306	53645.042559	32.671732
693.794152	53719.648268	32.676749
694.174735	53808.605901	32.681767
695.182537	53893.713068	32.686784
695.869642	53983.882657	32.691802
696.409589	54064.893458	32.696820
696.849516	54153.779817	32.701837
697.621796	54246.481004	32.706855
698.294707	54342.324268	32.711872
698.823603	54432.583627	32.716890
700.012495	54517.386239	32.721908
700.350971	54604.151214	32.726925
701.479887	54702.759611	32.731943
702.036086	54781.542746	32.736960
702.633582	54879.830086	32.741978
703.455396	54971.102465	32.746996
704.290758	55056.304103	32.752013
705.266138	55156.609139	32.757031
705.936665	55239.691901	32.762048
707.029382	55324.328935	32.767066
708.115540	55399.790933	32.772084
708.571329	55477.604850	32.777101
709.062657	55569.279350	32.782119
710.049915	55650.598904	32.787136
710.393143	55734.120691	32.792154
711.359216	55817.716105	32.797172
712.071436	55896.820246	32.802189
712.516352	55977.953715	32.807207
713.294695	56061.452808	32.812224
713.884784	56142.671690	32.817242
714.778885	56220.957332	32.822260
715.646438	56296.367800	32.827277
715.940536	56392.373576	32.832295
716.769876	56477.511621	32.837312
717.584627	56566.095139	32.842330
718.073238	56645.882316	32.847348
718.975824	56735.553926	32.852365
719.431708	56817.954299	32.857383
720.669130	56906.783002	32.862400
721.152807	56993.451648	32.867418
721.755634	57079.063998	32.872436
722.518979	57163.467993	32.877453
722.934835	57243.787526	32.882471
723.975815	57329.357468	32.887488
724.315048	57418.138846	32.892506
725.168601	57500.618521	32.897524
725.803090	57587.069486	32.902541
726.049564	57677.973937	32.907559
727.038348	57750.850995	32.912576
727.664335	57853.677752	32.917594
728.433679	57937.716427	32.922612
728.759505	58019.653928	32.927629
729.616946	58119.926543	32.932647
730.602366	58203.001905	32.937664
731.164370	58301.467064	32.942682
731.796635	58389.193432	32.947700
732.921216	58477.988633	32.952717
733.352422	58574.424678	32.957735
734.319253	58658.036178	32.962752
734.934696	58754.545357	32.967770
735.583768	58853.948534	32.972788
736.670056	58942.580537	32.977805
737.388957	59041.992537	32.982823
738.259215	59122.721856	32.987840
738.797122	59218.586751	32.992858
739.536667	59312.338023	32.997876
740.342994	59406.395677	33.002893
740.698164	59509.062978	33.007911
741.630269	59592.702117	33.012928
742.424145	59688.294577	33.017946
743.167305	59792.009997	33.022964
744.188139	59883.567325	33.027981
744.805697	59978.061842	33.032999
745.870395	60074.588181	33.038016
746.382567	60168.125153	33.043034
747.154192	60267.502236	33.048052
747.723262	60368.247034	33.053069
748.394048	60459.500531	33.058087
749.023865	60562.331793	33.063104
749.934716	60667.967933	33.068122
750.856550	60761.303756	33.073140
751.668622	60862.423972	33.078157
752.010069	60971.777646	33.083175
752.989371	61066.264013	33.088192
753.844823	61161.738632	33.093210
754.230611	61261.585275	33.098228
755.316602	61358.974213	33.103245
755.898340	61459.968368	33.108263
757.337634	61564.772319	33.113280
758.054383	61662.220276	33.118298
758.618185	61767.352088	33.123316
759.448266	61858.699765	33.128333
759.787043	61963.772696	33.133351
760.818195	62051.190171	33.138368
761.724697	62151.914734	33.143386
762.137095	62259.509502	33.148404
763.187460	62355.300043	33.153421
763.728069	62460.508059	33.158439
764.742639	62550.240472	33.163456
765.245370	62656.550406	33.168474
765.991382	62759.473895	33.173492
766.791200	62857.350336	33.178509
767.436054	62960.923545	33.183527
768.198389	63061.687030	33.188544
769.182231	63158.427996	33.193562
769.967837	63272.311897	33.198580
770.793777	63366.900682	33.203597
771.825487	63473.067954	33.208615
772.562299	63574.280647	33.213632
773.083032	63674.242460	33.218650
773.903134	63774.955460	33.223668
774.818235	63862.479765	33.228685
775.263732	63964.879182	33.233703
776.269717	64056.891092	33.238720
776.863526	64154.482000	33.243738
777.534495	64241.089906	33.248756
778.294517	64348.284705	33.253773
778.981453	64433.865178	33.258791
779.909972	64532.797931	33.263808
780.700428	64625.921925	33.268826
781.385999	64732.275345	33.273844
782.162949	64815.089062	33.278861
783.095650	64925.861593	33.283879
783.656733	65018.142947	33.288896
784.480171	65112.713374	33.293914
785.426822	65223.504019	33.298932
786.221958	65315.471241	33.303949
786.680566	65422.179660	33.308967
787.473422	65526.012503	33.313984
788.469292	65626.806679	33.319002
789.216071	65736.978761	33.324020
789.974363	65842.154190	33.329037
790.877118	65945.952548	33.334055
791.444984	66054.761152	33.339072
792.496045	66161.519194	33.344090
793.074557	66278.659069	33.349108
793.993370	66367.540046	33.354125
794.786982	66470.357283	33.359143
795.551324	66576.357878	33.364160
796.073073	66679.148883	33.369178
796.747765	66793.648523	33.374196
797.616171	66909.561919	33.379213
798.367102	67023.525137	33.384231
799.182820	67133.673467	33.389248
800.450782	67246.208099	33.394266
800.973640	67366.983331	33.399284
802.002970	67475.687738	33.404301
802.470796	67585.075705	33.409319
803.375869	67700.246134	33.414336
804.635449	67808.573985	33.419354
805.490420	67919.245072	33.424372
806.153930	68025.710674	33.429389
807.040372	68150.282358	33.434407
807.762126	68257.442624	33.439424
808.882519	68358.785275	33.444442
809.700516	68465.329810	33.449460
810.666884	68573.871423	33.454477
811.559165	68693.676906	33.459495
812.030126	68787.834901	33.464512
813.149061	68891.718980	33.469530
813.421057	69009.109263	33.474548
814.636478	69100.739332	33.479565
815.145798	69213.053091	33.484583
815.852274	69337.101453	33.489600
816.940041	69444.994501	33.494618
817.335072	69542.960053	33.499636
818.439333	69672.393353	33.504653
819.105280	69791.251529	33.509671
820.201824	69897.941967	33.514688
820.825898	70003.554357	33.519706
821.639575	70118.851175	33.524724
822.572545	70236.371454	33.529741
823.391279	70348.008427	33.534759
824.123156	70457.379834	33.539776
824.918383	70568.400860	33.544794
825.842956	70680.858554	33.549812
827.224508	70789.800335	33.554829
827.544344	70900.415943	33.559847
828.213573	71014.498165	33.564864
829.454681	71117.624755	33.569882
830.196729	71225.591958	33.574900
831.035133	71335.304967	33.579917
831.881647	71433.529861	33.584935
832.366363	71537.207153	33.589952
833.474908	71641.091136	33.594970
834.217739	71743.234321	33.599988
835.021471	71840.340218	33.605005
835.592905	71945.740691	33.610023
836.461040	72061.721444	33.615040
837.329555	72159.780946	33.620058
838.232799	72265.232060	33.625076
838.789115	72375.132884	33.630093
839.832203	72486.807129	33.635111
840.495287	72606.406760	33.640128
841.262203	72714.528144	33.645146
842.035850	72836.239347	33.650164
842.861983	72946.999563	33.655181
844.073401	73073.646329	33.660199
844.655593	73188.929495	33.665216
845.661211	73292.760077	33.670234
846.072941	73411.554061	33.675252
847.042117	73532.477863	33.680269
847.897834	73650.228092	33.685287
849.160678	73773.260258	33.690304
849.988000	73882.567553	33.695322
850.595865	74012.226537	33.700340
851.520680	74136.060618	33.705357
852.619891	74257.562660	33.710375
853.260310	74368.927845	33.715392
854.327575	74495.527923	33.720410
854.870386	74611.507380	33.725428
855.640191	74735.444498	33.730445
856.714352	74857.725847	33.735463
857.270533	74975.744132	33.740480
858.655697	75092.113100	33.745498
859.205666	75226.005078	33.750516
860.206404	75351.352900	33.755533
860.915044	75473.162259	33.760551
861.738005	75597.741034	33.765568
863.170626	75719.298799	33.770586
863.521510	75856.835220	33.775604
864.577362	75966.457203	33.780621
865.416044	76098.699540	33.785639
866.078915	76227.081149	33.790656
867.486880	76349.076290	33.795674
868.371521	76479.159808	33.800692
869.345974	76598.791781	33.805709
870.118817	76711.627983	33.810727
870.984742	76829.795848	33.815744
872.061543	76948.273234	33.820762
872.615236	77071.368123	33.825780
873.474387	77196.239910	33.830797
874.565743	77323.850186	33.835815
875.452771	77439.357114	33.840832
876.620574	77552.781011	33.845850
877.116954	77685.768707	33.850868
877.931278	77794.713771	33.855885
879.056436	77919.179823	33.860903
879.864391	78044.316850	33.865920
881.162361	78158.520967	33.870938
881.861365	78274.440897	33.875956
882.562280	78402.003301	33.880973
883.436560	78520.329157	33.885991
884.223926	78639.454580	33.891008
885.188513	78756.665145	33.896026
886.226191	78888.294356	33.901044
887.247336	78999.327460	33.906061
888.141834	79113.763398	33.911079
888.711043	79231.696658	33.916096
889.939114	79331.246089	33.921114
890.842389	79450.483538	33.926132
891.590041	79551.198508	33.931149
892.388388	79664.752276	33.936167
892.788572	79782.828360	33.941184
893.876170	79889.851196	33.946202
894.833985	80007.828251	33.951220
895.970172	80115.173742	33.956237
896.668775	80235.878221	33.961255
897.004980	80359.123152	33.966272
898.444499	80463.153801	33.971290
899.193409	80599.207250	33.976308
900.070678	80713.867836	33.981325
901.178730	80829.024876	33.986343
901.852945	80957.325334	33.991360
902.413453	81081.159127	33.996378
903.144266	81205.346889	34.001396
904.260910	81326.117300	34.006413
905.223505	81450.966691	34.011431
906.120977	81584.543703	34.016448
906.874477	81717.066947	34.021466
907.728588	81846.344211	34.026484
908.569544	81977.030501	34.031501
909.962297	82112.508987	34.036519
910.745432	82242.483360	34.041536
911.867913	82379.589214	34.046554
912.585355	82507.408478	34.051572
913.333942	82640.367600	34.056589
914.257442	82774.795064	34.061607
915.210607	82912.601533	34.066624
916.104452	83033.350759	34.071642
917.135137	83170.740882	34.076660
918.258151	83310.727362	34.081677
918.680529	83440.370902	34.086695
919.613808	83582.783185	34.091712
920.688267	83721.993695	34.096730
921.791006	83859.629262	34.101748
922.808551	83998.457229	34.106765
923.501986	84132.724367	34.111783
924.167980	84266.907732	34.116800
925.674506	84409.576482	34.121818
926.483329	84553.596960	34.126836
927.434242	84689.169526	34.131853
928.374894	84825.517285	34.136871
929.397451	84965.134750	34.141888
930.315136	85092.465350	34.146906
931.442397	85241.736057	34.151924
932.260151	85373.531235	34.156941
933.509285	85508.858205	34.161959
933.927398	85641.528157	34.166976
935.241380	85775.173555	34.171994
936.113089	85914.629136	34.177012
937.027373	86048.832575	34.182029
938.337925	86183.798259	34.187047
939.134649	86316.057190	34.192064
940.224623	86450.678489	34.197082
940.879747	86589.550280	34.202100
942.083958	86728.083314	34.207117
943.197683	86845.303868	34.212135
943.595280	86991.136902	34.217152
944.615214	87112.985912	34.222170
945.349047	87245.664403	34.227188
946.395578	87392.082129	34.232205
947.493106	87525.858130	34.237223
948.588920	87665.223598	34.242240
949.535333	87785.122660	34.247258
950.471213	87930.394508	34.252276
951.227915	88074.085690	34.257293
952.477744	88189.389381	34.262311
953.475721	88316.594715	34.267328
953.808752	88434.830929	34.272346
955.350250	88561.318570	34.277364
955.927953	88683.332017	34.282381
956.820745	88819.059545	34.287399
957.850659	88951.597950	34.292416
958.545141	89073.746791	34.297434
959.950283	89200.689391	34.302452
960.203106	89335.898490	34.307469
961.726628	89469.667260	34.312487
962.190496	89608.912684	34.317504
963.052886	89744.940674	34.322522
964.062350	89887.092897	34.327540
964.887636	90021.315642	34.332557
965.812668	90163.533089	34.337575
966.921366	90310.006152	34.342592
967.685578	90456.863382	34.347610
968.771756	90600.717925	34.352628
969.851676	90750.657584	34.357645
970.782031	90890.875165	34.362663
971.728143	91049.848414	34.367680
972.311264	91198.511964	34.372698
973.725975	91337.895341	34.377716
974.734817	91499.028398	34.382733
975.759765	91642.137033	34.387751
976.751428	91794.693900	34.392768
977.811070	91939.750346	34.397786
978.708307	92080.561636	34.402804
979.315397	92240.620828	34.407821
980.778843	92383.600923	34.412839
981.769859	92542.232735	34.417856
982.707166	92694.878664	34.422874
983.842814	92843.945376	34.427892
984.569307	92998.083416	34.432909
985.561323	93144.448998	34.437927
986.747762	93289.491996	34.442944
987.777164	93438.869755	34.447962
988.741288	93602.391124	34.452980
990.047879	93752.056554	34.457997
991.054542	93908.715658	34.463015
991.658046	94060.140434	34.468032
992.586877	94206.216745	34.473050
994.020798	94362.925333	34.478068
994.915401	94512.177283	34.483085
995.922601	94669.537299	34.488103
996.759356	94821.943312	34.493120
997.916809	94976.987087	34.498138
999.229633	95134.086117	34.503156
999.800743	95289.350005	34.508173
1000.629388	95437.818148	34.513191
1001.969116	95600.010976	34.518208
1002.813355	95743.952852	34.523226
1004.154921	95899.923074	34.528244
1005.169973	96054.576183	34.533261
1006.567790	96206.356031	34.538279
1007.166485	96358.489898	34.543296
1008.447258	96500.769699	34.548314
1009.360437	96656.417784	34.553332
1010.541918	96803.531482	34.558349
1011.587053	96945.786802	34.563367
1012.288361	97094.675671	34.568384
1013.489191	97250.395731	34.573402
1014.640696	97388.770049	34.578420
1015.272911	97544.390430	34.583437
1016.707282	97689.820688	34.588455
1017.766487	97836.235752	34.593472
1018.574038	97983.667003	34.598490
1019.412708	98119.570796	34.603508
1020.179419	98269.633872	34.608525
1021.291551	98407.777921	34.613543
1022.495852	98542.929035	34.618560
1023.044341	98685.155792	34.623578
1024.151412	98821.426209	34.628596
1024.907755	98978.517364	34.633613
1026.198210	99130.480113	34.638631
1027.249099	99274.735245	34.643648
1028.156046	99420.268620	34.648666
1028.872845	99573.121946	34.653684
1029.792101	99733.588826	34.658701
1030.705583	99875.104460	34.663719
1032.118589	100035.153238	34.668736
1033.191868	100193.569865	34.673754
1033.983345	100353.527357	34.678772
1034.921151	100513.906450	34.683789
1035.984858	100677.321987	34.688807
1037.212619	100837.517820	34.693824
1038.368537	101004.330921	34.698842
1039.406173	101164.063681	34.703860
1040.508515	101315.584351	34.708877
1041.615325	101479.669092	34.713895
1042.451405	101645.470568	34.718912
1043.737973	101802.454322	34.723930
1044.726690	101961.678815	34.728948
1045.620217	102123.492701	34.733965
1046.704216	102291.578767	34.738983
1047.886722	102457.342770	34.744000
1048.545308	102635.678067	34.749018
1050.113326	102791.975856	34.754036
1051.074717	102954.353722	34.759053
1052.281193	103119.939784	34.764071
1053.140362	103289.093094	34.769088
1054.123677	103458.798377	34.774106
1055.619164	103621.438210	34.779124
1056.459589	103794.159813	34.784141
1057.441538	103955.030529	34.789159
1058.455688	104125.862814	34.794176
1059.298886	104291.777827	34.799194
1060.777842	104454.475014	34.804212
1061.908929	104636.880483	34.809229
1062.890835	104799.619120	34.814247
1064.008758	104975.714123	34.819264
1065.122614	105137.609565	34.824282
1066.549685	105303.171875	34.829300
1067.217945	105470.045686	34.834317
1068.508117	105635.225302	34.839335
1069.856464	105809.576801	34.844352
1070.534722	105973.674640	34.849370
1071.766167	106143.747675	34.854388
1072.776534	106309.849289	34.859405
1073.844991	106480.989282	34.864423
1074.761155	106643.823130	34.869440
1076.257995	106812.272927	34.874458
1077.083401	106979.991774	34.879476
1078.309115	107147.433203	34.884493
1079.205909	107309.081290	34.889511
1079.918578	107480.941350	34.894528
1081.248025	107651.146003	34.899546
1082.491626	107821.986282	34.904564
1083.878207	107996.596527	34.909581
1084.961802	108165.536098	34.914599
1086.152588	108318.266398	34.919616
1086.986736	108490.949382	34.924634
1088.535348	108651.056077	34.929652
1089.297586	108821.862511	34.934669
1089.992887	108979.111607	34.939687
1091.396570	109139.408086	34.944704
1092.443717	109289.349939	34.949722
1093.603387	109447.669738	34.954740
1094.491886	109608.873298	34.959757
1095.356169	109761.343995	34.964775
1096.707586	109911.912978	34.969792
1097.560415	110087.314713	34.974810
1098.614590	110240.467912	34.979828
1100.010540	110406.909200	34.984845
1100.805864	110565.811007	34.989863
1101.954333	110716.554693	34.994880
1102.708132	110897.910941	34.999898
1103.739582	111064.767470	35.004916
1104.969495	111235.360203	35.009933
1106.130227	111408.488272	35.014951
1107.431614	111577.600357	35.019968
1108.357754	111746.632489	35.024986
1109.385711	111923.119196	35.030004
1110.534660	112100.957497	35.035021
1111.678361	112274.688480	35.040039
1113.013223	112447.439209	35.045056
1114.340337	112623.235727	35.050074
1115.525272	112801.820112	35.055092
1116.510916	112972.307157	35.060109
1117.393238	113147.389551	35.065127
1118.556220	113314.464225	35.070144
1119.878898	113502.225331	35.075162
1120.752047	113670.754786	35.080180
1121.938593	113848.354824	35.085197
1123.166190	114033.292626	35.090215
1124.677050	114215.789962	35.095232
1125.457981	114388.662015	35.100250
1126.325984	114573.557379	35.105268
1127.374253	114765.096725	35.110285
1128.735094	114938.578145	35.115303
1130.067367	115114.614168	35.120320
1131.030710	115306.220355	35.125338
1132.521476	115489.056920	35.130356
1133.701593	115660.756318	35.135373
1134.451815	115844.395471	35.140391
1135.870617	116026.320063	35.145408
1137.012261	116205.359042	35.150426
1137.891379	116385.771756	35.155444
1139.349924	116572.969165	35.160461
1140.283638	116753.425842	35.165479
1141.833951	116935.562584	35.170496
1142.702906	117128.182253	35.175514
1143.805121	117306.192596	35.180532
1145.069054	117487.133824	35.185549
1146.194464	117666.080848	35.190567
1147.696204	117861.192737	35.195584
1148.328987	118040.764071	35.200602
1149.635172	118219.393676	35.205620
1150.454474	118405.190843	35.210637
1152.062280	118597.220323	35.215655
1153.195607	118775.904970	35.220672
1154.191575	118968.742429	35.225690
1155.441402	119148.805872	35.230708
1156.948170	119338.317993	35.235725
1157.785563	119513.805164	35.240743
1159.193352	119707.812278	35.245760
1160.145857	119882.724983	35.250778
1161.109574	120065.323720	35.255796
1162.362338	120253.370617	35.260813
1163.525313	120445.567772	35.265831
1165.044296	120626.268282	35.270848
1166.222527	120811.209044	35.275866
1167.053827	120987.363475	35.280884
1168.476439	121148.432267	35.285901
1169.837448	121331.672443	35.290919
1170.621175	121505.819709	35.295936
1171.445094	121678.286992	35.300954
1172.659832	121847.065828	35.305972
1173.902801	122023.046303	35.310989
1174.895237	122203.836532	35.316007
1175.950603	122380.913555	35.321024
1176.872500	122572.930554	35.326042
1177.878691	122748.608816	35.331060
1179.394633	122936.069219	35.336077
1180.343917	123118.506840	35.341095
1181.834681	123296.585396	35.346112
1182.767804	123501.049943	35.351130
1183.986497	123693.901216	35.356148
1185.523756	123883.988736	35.361165
1186.290659	124086.338351	35.366183
1187.496002	124280.564634	35.371200
1188.618529	124471.848928	35.376218
1189.962700	124670.153005	35.381236
1191.328053	124858.369094	35.386253
1192.110472	125064.577832	35.391271
1193.609440	125251.823350	35.396288
1194.920397	125452.978225	35.401306
1195.759242	125650.021424	35.406324
1197.431057	125854.635974	35.411341
1198.264654	126057.898422	35.416359
1199.599749	126251.707840	35.421376
1200.706065	126453.635503	35.426394
1201.998863	126667.130793	35.431412
1203.257709	126870.267249	35.436429
1204.619754	127070.039172	35.441447
1205.894133	127274.405822	35.446464
1207.247743	127476.033338	35.451482
1208.671568	127677.473218	35.456500
1209.904058	127865.457453	35.461517
1210.768103	128081.069786	35.466535
1212.172223	128274.662171	35.471552
1213.405663	128478.863506	35.476570
1214.547650	128682.318899	35.481588
1216.085467	128881.716723	35.486605
1217.314987	129089.080837	35.491623
1218.563430	129274.531351	35.496640
1219.689438	129487.217076	35.501658
1220.916926	129690.092983	35.506676
1222.472471	129889.848035	35.511693
1223.592678	130092.247823	35.516711
1224.706198	130295.131760	35.521728
1225.867433	130496.803823	35.526746
1226.698601	130702.626766	35.531764
1228.339062	130904.289162	35.536781
1229.471429	131109.115282	35.541799
1230.747439	131311.445669	35.546816
1232.394739	131510.686362	35.551834
1233.363159	131714.805087	35.556852
1234.904005	131922.235673	35.561869
1235.670658	132131.133424	35.566887
1237.155084	132319.808391	35.571904
1238.561154	132528.849030	35.576922
1239.892226	132718.412548	35.581940
1240.972086	132919.994400	35.586957
1242.052707	133120.929926	35.591975
1243.498849	133314.005486	35.596992
1244.709100	133523.728633	35.602010
1245.814920	133727.657558	35.607028
1247.255400	133923.084121	35.612045
1248.417693	134131.980167	35.617063
1249.406529	134320.398648	35.622080
1250.744033	134509.308979	35.627098
1251.692791	134707.785226	35.632116
1252.938999	134898.196130	35.637133
1253.954108	135098.655938	35.642151
1254.857399	135286.140156	35.647168
1256.787751	135489.351618	35.652186
1257.538689	135686.429221	35.657204
1259.008835	135882.519512	35.662221
1260.023596	136088.909799	35.667239
1261.068016	136293.646712	35.672256
1262.914065	136494.363295	35.677274
1264.120969	136700.294810	35.682292
1265.017896	136908.788369	35.687309
1266.121646	137129.166355	35.692327
1267.439985	137335.146714	35.697344
1268.679910	137543.513306	35.702362
1269.988529	137758.646604	35.707380
1271.338332	137979.205847	35.712397
1272.574717	138189.974333	35.717415
1273.663543	138408.888658	35.722432
1274.931763	138622.712471	35.727450
1276.405794	138845.743661	35.732468
1277.742910	139068.112054	35.737485
1278.399583	139300.727747	35.742503
1280.356896	139516.364015	35.747520
1281.633347	139737.488679	35.752538
1282.772695	139965.628416	35.757556
1284.731406	140182.435031	35.762573
1285.580636	140409.518204	35.767591
1287.004799	140626.182069	35.772608
1288.465287	140851.115721	35.777626
1289.741175	141072.195872	35.782644
1291.044593	141290.303015	35.787661
1292.081153	141527.489596	35.792679
1293.414138	141748.893864	35.797696
1294.811799	141970.923575	35.802714
1296.360823	142197.499469	35.807732
1297.866052	142424.768601	35.812749
1298.769081	142642.931772	35.817767
1300.350143	142879.519323	35.822784
1301.690576	143090.458013	35.827802
1302.838821	143328.181549	35.832820
1304.721612	143550.091672	35.837837
1305.532007	143771.992966	35.842855
1306.752192	143992.841143	35.847872
1308.096986	144214.952661	35.852890
1309.405461	144436.563171	35.857908
1311.228637	144660.784777	35.862925
1312.415571	144883.660086	35.867943
1313.347797	145114.597615	35.872960
1314.955761	145335.086359	35.877978
1316.065974	145563.840410	35.882996
1317.613149	145797.502433	35.888013
1318.990003	146021.507982	35.893031
1320.622679	146234.850993	35.898048
1321.945169	146451.860767	35.903066
1323.149040	146685.339406	35.908084
1324.966778	146898.338879	35.913101
1325.900742	147118.623461	35.918119
1327.103605	147344.273926	35.923136
1328.668364	147553.723676	35.928154
1329.672249	147786.565844	35.933172
1331.593339	147998.297048	35.938189
1332.813619	148226.639443	35.943207
1333.813683	148446.944639	35.948224
1335.163692	148658.184010	35.953242
1336.668605	148890.622599	35.958260
1337.749294	149104.672963	35.963277
1339.133092	149324.147449	35.968295
1340.319991	149525.527888	35.973312
1341.954149	149728.552648	35.978330
1342.867137	149940.614384	35.983348
1344.391587	150144.013290	35.988365
1345.501194	150354.560759	35.993383
1347.161098	150572.905479	35.998400
1348.398694	150773.724119	36.003418
1349.446976	150988.599394	36.008436
1351.072331	151207.675585	36.013453
1352.510605	151426.451901	36.018471
1353.532659	151645.192687	36.023488
1355.355389	151857.436795	36.028506
1356.189647	152073.428757	36.033524
1357.949557	152299.875949	36.038541
1358.823584	152517.716697	36.043559
1360.044832	152740.632257	36.048576
1361.298428	152963.010495	36.053594
1362.463948	153201.423170	36.058612
1363.937177	153434.419118	36.063629
1365.402882	153663.977111	36.068647
1366.835586	153899.723229	36.073664
1367.984352	154132.544331	36.078682
1369.456093	154375.928191	36.083700
1370.999628	154615.226983	36.088717
1372.012560	154845.546075	36.093735
1373.087923	155087.484359	36.098752
1374.862775	155322.268755	36.103770
1376.234097	155581.059050	36.108788
1377.736797	155828.531789	36.113805
1379.317453	156073.809900	36.118823
1380.591514	156310.212692	36.123840
1382.351322	156552.418039	36.128858
1383.925802	156801.521242	36.133876
1385.245119	157031.001190	36.138893
1386.366328	157277.422561	36.143911
1387.691548	157519.242849	36.148928
1389.329635	157752.738032	36.153946
1390.967789	157999.474991	36.158964
1392.213443	158236.892751	36.163981
1393.407390	158480.870202	36.168999
1395.015173	158729.011337	36.174016
1396.720567	158971.831607	36.179034
1398.273812	159216.733282	36.184052
1399.688951	159456.719076	36.189069
1401.059583	159698.337770	36.194087
1401.957787	159941.897575	36.199104
1403.468369	160173.619190	36.204122
1404.796925	160415.056816	36.209140
1406.372292	160657.624729	36.214157
1407.833957	160906.305256	36.219175
1409.059537	161156.128235	36.224192
1410.681597	161400.113597	36.229210
1412.364138	161637.272814	36.234228
1413.889131	161883.839756	36.239245
1415.178385	162121.367021	36.244263
1416.423463	162370.620374	36.249280
1418.144520	162594.154406	36.254298
1419.800228	162856.701471	36.259316
1421.218434	163093.056775	36.264333
1422.727545	163337.092521	36.269351
1424.064222	163589.281680	36.274368
1425.932486	163819.551190	36.279386
1427.209307	164061.023257	36.284404
1428.613013	164289.462679	36.289421
1430.151920	164528.724359	36.294439
1431.361378	164760.293689	36.299456
1432.765771	164981.396875	36.304474
1434.246692	165205.358199	36.309492
1435.456499	165427.242387	36.314509
1436.977628	165639.733941	36.319527
1438.079898	165861.407836	36.324544
1439.544919	166081.083092	36.329562
1440.777993	166308.616478	36.334580
1442.296707	166544.549192	36.339597
1443.675077	166766.195477	36.344615
1444.851619	166998.323487	36.349632
1446.294328	167230.436001	36.354650
1447.724630	167465.852403	36.359668
1449.069047	167702.946326	36.364685
1450.586983	167937.995073	36.369703
1451.051532	168195.797380	36.374720
1452.927052	168436.238804	36.379738
1454.271899	168691.073678	36.384756
1455.917680	168938.409153	36.389773
1457.530906	169190.156480	36.394791
1458.657032	169447.935901	36.399808
1460.305599	169697.533625	36.404826
1461.464131	169970.648076	36.409844
1462.764275	170221.559145	36.414861
1464.104290	170484.489231	36.419879
1465.496145	170751.437214	36.424896
1467.220620	171015.604136	36.429914
1468.719633	171295.272837	36.434932
1470.125233	171566.246674	36.439949
1471.472007	171827.834464	36.444967
1472.996460	172094.169654	36.449984
1474.974969	172361.260053	36.455002
1476.472313	172644.832155	36.460020
1478.152790	172912.783763	36.465037
1479.565906	173180.511486	36.470055
1480.568700	173463.414804	36.475072
1482.516839	173730.248001	36.480090
1483.873578	173995.358855	36.485108
1485.409022	174276.975410	36.490125
1486.985142	174538.434807	36.495143
1488.233881	174820.174333	36.500160
1490.183792	175088.370484	36.505178
1492.011193	175361.259620	36.510196
1493.242248	175636.223925	36.515213
1494.752198	175904.809074	36.520231
1496.805846	176190.109840	36.525248
1498.281299	176445.470523	36.530266
1499.662364	176723.348276	36.535284
1501.233668	176983.927330	36.540301
1503.044560	177246.552237	36.545319
1503.970395	177518.662569	36.550336
1505.796317	177782.302657	36.555354
1507.308417	178058.005520	36.560372
1508.613864	178323.989074	36.565389
1510.342279	178592.751741	36.570407
1511.743943	178869.261782	36.575424
1513.256008	179129.628028	36.580442
1514.676963	179399.482582	36.585460
1516.371603	179678.184283	36.590477
1518.020713	179946.303144	36.595495
1519.296247	180220.144975	36.600512
1521.238456	180482.886027	36.605530
1522.770550	180752.905034	36.610548
1523.893638	181027.966857	36.615565
1525.213237	181292.179169	36.620583
1526.755117	181556.916205	36.625600
1528.495835	181835.896665	36.630618
1530.083827	182108.425296	36.635636
1531.582936	182375.203197	36.640653
1533.239303	182648.052858	36.645671
1534.613864	182908.044967	36.650688
1536.389640	183160.584001	36.655706
1537.736590	183415.527485	36.660724
1539.114878	183672.016052	36.665741
1540.934326	183920.461034	36.670759
1542.224321	184181.663520	36.675776
1543.576435	184437.142222	36.680794
1544.964291	184688.374358	36.685812
1546.396177	184951.537771	36.690829
1547.920375	185283.036391	36.695847
1549.142934	185564.165923	36.700864
1550.636366	185837.456264	36.705882
1552.512660	186099.562509	36.710900
1553.958570	186378.754354	36.715917
1555.469945	186646.405350	36.720935
1556.929257	186932.022624	36.725952
1558.425126	187215.653777	36.730970
1560.256544	187500.884142	36.735988
1561.587519	187775.220911	36.741005
1563.409790	188050.370473	36.746023
1564.681155	188345.723618	36.751040
1566.409414	188636.154664	36.756058
1568.048315	188923.476256	36.761076
1569.225030	189214.274526	36.766093
1571.130112	189503.664144	36.771111
1572.509323	189793.314601	36.776128
1574.224222	190083.040252	36.781146
1576.106374	190373.146856	36.786164
1577.220349	190672.315331	36.791181
1579.024999	190967.083800	36.796199
1580.548875	191254.988012	36.801216
1582.169377	191551.793384	36.806234
1583.830161	191855.552947	36.811252
1585.470333	192147.987795	36.816269
1587.147785	192447.351902	36.821287
1588.998651	192745.140142	36.826304
1590.257304	193045.612662	36.831322
1592.359475	193335.641112	36.836340
1593.775192	193645.285598	36.841357
1595.674877	193937.379177	36.846375
1597.139683	194234.240674	36.851392
1598.548029	194535.861691	36.856410
1600.355671	194829.394124	36.861428
1602.031423	195130.720627	36.866445
1603.926927	195418.855531	36.871463
1605.521843	195712.956604	36.876480
1606.928726	196010.745536	36.881498
1608.783394	196297.898013	36.886516
1610.050057	196605.057896	36.891533
1611.902838	196898.206649	36.896551
1613.483612	197208.239850	36.901568
1615.067564	197496.427769	36.906586
1616.850209	197799.775394	36.911604
1618.559782	198098.003915	36.916621
1620.299192	198396.075949	36.921639
1621.649214	198691.440704	36.926656
1623.192265	198987.436268	36.931674
1624.988753	199286.110747	36.936692
1626.714736	199583.577532	36.941709
1628.223114	199878.741939	36.946727
1629.802020	200172.549539	36.951744
1631.657791	200469.616624	36.956762
1633.067343	200767.236721	36.961780
1634.507876	201074.479960	36.966797
1636.495793	201364.288319	36.971815
1638.008750	201666.415434	36.976832
1639.948886	201958.315268	36.981850
1641.557752	202245.009129	36.986868
1642.872289	202529.336283	36.991885
1644.592943	202809.789954	36.996903
1645.944092	203088.625318	37.001920
1647.407474	203374.099019	37.006938
1649.318223	203655.997584	37.011956
1650.872012	203940.924547	37.016973
1652.454170	204225.618871	37.021991
1653.877168	204506.172472	37.027008
1655.809828	204797.849339	37.032026
1657.909347	205092.574262	37.037044
1659.063408	205388.539900	37.042061
1660.572192	205680.868646	37.047079
1662.154102	205971.408153	37.052096
1663.765356	206267.532120	37.057114
1665.205709	206560.126822	37.062132
1666.662331	206869.790207	37.067149
1668.632043	207168.272590	37.072167
1670.231092	207479.870569	37.077184
1671.606747	207795.898675	37.082202
1673.785580	208105.704755	37.087220
1675.084777	208433.710575	37.092237
1676.985387	208726.566259	37.097255
1678.847946	209031.316974	37.102272
1680.293142	209355.439879	37.107290
1682.058359	209669.097749	37.112308
1683.978746	209988.523678	37.117325
1685.394892	210307.876481	37.122343
1687.182055	210635.097464	37.127360
1688.762190	210955.543107	37.132378
1690.461566	211262.633627	37.137396
1692.192576	211591.007655	37.142413
1693.880179	211910.929463	37.147431
1695.545491	212241.829432	37.152448
1697.409828	212567.567083	37.157466
1699.203875	212892.045884	37.162484
1701.154134	213222.394203	37.167501
1702.551279	213542.947382	37.172519
1704.748249	213867.694315	37.177536
1706.175298	214203.536432	37.182554
1707.818945	214520.215954	37.187572
1709.216208	214858.324254	37.192589
1711.022513	215185.267387	37.197607
1713.256901	215520.349219	37.202624
1714.681389	215846.793749	37.207642
1716.717854	216175.860967	37.212660
1718.378508	216513.929392	37.217677
1720.504959	216842.525742	37.222695
1722.495970	217176.376710	37.227712
1723.652679	217502.432445	37.232730
1725.554573	217826.974555	37.237748
1727.321489	218156.263111	37.242765
1728.905871	218475.418845	37.247783
1730.760185	218816.303699	37.252800
1732.617221	219138.414779	37.257818
1734.580795	219460.128284	37.262836
1736.035290	219800.669751	37.267853
1738.016849	220130.052748	37.272871
1739.651136	220453.545689	37.277888
1741.362011	220788.229943	37.282906
1743.661496	221104.302672	37.287924
1744.779191	221440.528016	37.292941
1746.697688	221751.300316	37.297959
1748.067371	222083.523393	37.302976
1749.707214	222418.524132	37.307994
1751.817898	222752.663743	37.313012
1753.590013	223083.299837	37.318029
1755.026062	223412.743782	37.323047
1757.041260	223736.101784	37.328064
1758.577101	224054.098368	37.333082
1760.407156	224365.189839	37.338100
1761.870480	224670.826034	37.343117
1763.273528	224983.152952	37.348135
1765.457105	225298.228398	37.353152
1767.092552	225617.327253	37.358170
1769.296006	225935.016203	37.363188
1770.695394	226251.763992	37.368205
1772.318009	226575.488353	37.373223
1774.183181	226906.364079	37.378240
1775.640064	227229.860260	37.383258
1777.524285	227552.908459	37.388276
1779.254768	227891.832797	37.393293
1780.705029	228221.757067	37.398311
1782.586948	228560.733768	37.403328
1784.262867	228893.264581	37.408346
1785.996931	229234.652209	37.413364
1787.633787	229586.699226	37.418381
1789.498164	229931.571980	37.423399
1791.070957	230274.610331	37.428416
1792.982665	230629.306749	37.433434
1794.850055	230976.896822	37.438452
1796.263504	231336.700862	37.443469
1798.335134	231701.736548	37.448487
1800.692868	232052.069180	37.453504
1802.006577	232405.638857	37.458522
1803.835426	232764.919799	37.463540
1805.726572	233126.502513	37.468557
1807.636090	233487.192966	37.473575
1809.349436	233854.950725	37.478592
1811.521772	234209.604209	37.483610
1813.125183	234571.205476	37.488628
1815.206844	234948.075505	37.493645
1816.899036	235305.648466	37.498663
1818.984975	235667.579754	37.503680
1820.710494	236034.520837	37.508698
1822.600084	236396.990244	37.513716
1824.404498	236766.306213	37.518733
1826.274199	237134.976492	37.523751
1828.493084	237497.063006	37.528768
1830.150544	237873.869453	37.533786
1832.131238	238231.699226	37.538804
1833.850467	238597.241377	37.543821
1835.771852	238979.263741	37.548839
1837.657765	239332.585240	37.553856
1839.506207	239703.491357	37.558874
1841.581511	240069.534843	37.563892
1843.132105	240435.482128	37.568909
1844.969206	240809.767187	37.573927
1846.945728	241169.804048	37.578944
1848.770061	241541.651338	37.583962
1850.838078	241902.206315	37.588980
1852.877134	242270.233835	37.593997
1854.494998	242643.839185	37.599015
1856.465458	243005.855755	37.604032
1858.283749	243377.904380	37.609050
1859.921484	243745.535116	37.614068
1862.369487	244115.502544	37.619085
1864.270324	244485.300930	37.624103
1865.901392	244838.324167	37.629120
1867.899452	245210.570151	37.634138
1869.619448	245576.584477	37.639156
1871.689414	245938.047088	37.644173
1873.365645	246310.087373	37.649191
1875.383600	246672.928515	37.654208
1877.344813	247038.800759	37.659226
1879.243277	247405.037746	37.664244
1881.054652	247765.064017	37.669261
1883.005612	248107.971871	37.674279
1884.820713	248447.674220	37.679296
1886.224590	248800.065240	37.684314
1888.114751	249144.250713	37.689332
1889.980733	249483.739858	37.694349
1891.310691	249840.738117	37.699367
1893.486229	250196.612615	37.704384
1895.468664	250553.685054	37.709402
1896.929908	250919.728975	37.714420
1899.031767	251279.778556	37.719437
1900.787277	251642.294689	37.724455
1903.109163	252003.146438	37.729472
1904.626663	252370.346643	37.734490
1906.320707	252738.915427	37.739508
1908.562171	253105.340107	37.744525
1910.149776	253490.002940	37.749543
1912.282830	253855.325029	37.754560
1914.465560	254241.797851	37.759578
1915.906513	254612.052570	37.764596
1918.044132	254992.129226	37.769613
1919.873695	255384.369443	37.774631
1921.989546	255761.450015	37.779648
1924.043017	256149.791990	37.784666
1925.692516	256521.050320	37.789684
1927.723871	256906.218391	37.794701
1929.459243	257297.070628	37.799719
1931.656770	257689.779819	37.804736
1933.754947	258085.221212	37.809754
1935.232327	258468.007350	37.814772
1937.355086	258865.753866	37.819789
1939.443274	259258.424390	37.824807
1941.401307	259656.270284	37.829824
1943.273252	260054.915726	37.834842
1945.280076	260461.488991	37.839860
1947.484550	260848.039980	37.844877
1949.365568	261253.715735	37.849895
1951.587864	261646.611251	37.854912
1953.584624	262039.820081	37.859930
1955.491647	262441.550496	37.864948
1957.586027	262833.928434	37.869965
1959.655335	263234.182762	37.874983
1961.295102	263632.496249	37.880000
1963.051414	264030.942407	37.885018
1965.223346	264429.474427	37.890036
1967.877117	264827.827936	37.895053
1969.519507	265236.599405	37.900071
1971.665683	265629.797005	37.905088
1973.569087	266022.319894	37.910106
1975.701635	266430.781260	37.915124
1978.266122	266821.013271	37.920141
1980.448815	267216.535588	37.925159
1982.261883	267612.850690	37.930176
1984.233737	268005.177166	37.935194
1985.958137	268396.651809	37.940212
1988.113842	268776.374173	37.945229
1990.063205	269182.287338	37.950247
1992.169367	269572.224258	37.955264
1994.107823	269957.283977	37.960282
1995.898476	270351.203627	37.965300
1998.177770	270743.140287	37.970317
2000.274175	271142.850107	37.975335
2002.256302	271533.178960	37.980352
2004.193070	271923.132223	37.985370
2006.053326	272309.794083	37.990388
2008.218460	272700.952602	37.995405
2009.751695	273094.265369	38.000423
2011.641795	273487.444299	38.005440
2013.625862	273884.086058	38.010458
2015.640683	274267.641865	38.015476
2017.476617	274635.376467	38.020493
2019.326284	275019.741934	38.025511
2021.591400	275394.847143	38.030528
2023.243470	275774.490874	38.035546
2024.983100	276147.947882	38.040564
2027.342044	276544.619720	38.045581
2029.465124	276936.171139	38.050599
2031.341010	277320.623108	38.055616
2032.913608	277700.422468	38.060634
2034.846138	278112.060318	38.065652
2037.118789	278517.420915	38.070669
2039.075544	278914.397604	38.075687
2040.949018	279321.594051	38.080704
2043.041230	279727.255782	38.085722
2044.777766	280144.449391	38.090740
2047.183651	280554.044530	38.095757
2049.077439	280975.221208	38.100775
2050.934635	281385.811764	38.105792
2052.872821	281814.620344	38.110810
2054.789552	282237.995416	38.115828
2056.955920	282662.877955	38.120845
2058.922862	283095.229516	38.125863
2061.280995	283529.421741	38.130880
2063.057100	283950.370806	38.135898
2065.184810	284393.151287	38.140916
2067.368338	284833.660212	38.145933
2069.338733	285263.661594	38.150951
2071.330561	285707.445170	38.155968
2073.750112	286159.563854	38.160986
2075.853697	286604.187379	38.166004
2078.321946	287043.723218	38.171021
2080.041031	287487.893132	38.176039
2082.215415	287933.233010	38.181056
2084.548368	288368.718437	38.186074
2086.525272	288817.206329	38.191092
2088.896358	289264.689939	38.196109
2090.604763	289704.072732	38.201127
2092.857501	290158.906618	38.206144
2095.150277	290603.726964	38.211162
2097.126321	291057.201127	38.216180
2099.119599	291507.800158	38.221197
2101.788554	291965.323289	38.226215
2103.763276	292409.926499	38.231232
2106.102908	292861.146910	38.236250
2107.973032	293312.361236	38.241268
2110.563090	293756.375858	38.246285
2112.468234	294205.064406	38.251303
2114.722391	294645.088032	38.256320
2117.041879	295100.585404	38.261338
2118.962050	295550.480008	38.266356
2121.138953	295989.591603	38.271373
2123.256517	296447.598078	38.276391
2125.425303	296887.922726	38.281408
2128.113889	297334.204982	38.286426
2130.089670	297782.042341	38.291444
2132.454370	298227.048046	38.296461
2134.545180	298668.818092	38.301479
2136.614242	299099.239971	38.306496
2138.771341	299539.494864	38.311514
2140.669302	299982.858567	38.316532
2142.847213	300434.755525	38.321549
2144.894608	300873.265157	38.326567
2146.908340	301316.472925	38.331584
2149.488833	301769.514256	38.336602
2151.567115	302219.457095	38.341620
2153.525441	302659.946098	38.346637
2155.701323	303095.041092	38.351655
2157.906696	303517.892258	38.356672
2160.235973	303931.175902	38.361690
2162.023412	304344.464865	38.366708
2164.204984	304759.744998	38.371725
2166.271712	305189.051844	38.376743
2168.310733	305602.494390	38.381760
2170.362746	306027.608098	38.386778
2172.227291	306467.165448	38.391796
2174.482630	306889.930162	38.396813
2176.743949	307325.432716	38.401831
2178.679515	307753.646743	38.406848
2181.049069	308201.917670	38.411866
2183.118921	308642.667413	38.416884
2184.955550	309082.992792	38.421901
2187.234946	309533.194674	38.426919
2189.150985	309982.103978	38.431936
2191.913212	310438.668853	38.436954
2193.410564	310897.102420	38.441972
2195.524383	311346.627904	38.446989
2197.592464	311813.313714	38.452007
2199.598314	312286.476681	38.457024
2201.723661	312760.225304	38.462042
2204.055268	313243.936580	38.467060
2206.767790	313728.166952	38.472077
2208.785648	314202.171449	38.477095
2211.030895	314672.861549	38.482112
2213.565835	315163.956932	38.487130
2215.222931	315642.291944	38.492148
2217.722298	316121.200717	38.497165
2219.994413	316598.921777	38.502183
2221.947962	317100.669668	38.507200
2224.378196	317585.714986	38.512218
2226.893813	318082.110660	38.517236
2229.268990	318574.919155	38.522253
2231.572372	319066.083832	38.527271
2233.930155	319549.266239	38.532288
2236.365024	320038.343835	38.537306
2238.388977	320536.742351	38.542324
2240.616625	321026.526246	38.547341
2242.911489	321513.401205	38.552359
2245.145970	322015.149766	38.557376
2248.038563	322503.772175	38.562394
2250.090990	323006.044877	38.567412
2252.029415	323490.288378	38.572429
2254.566417	323988.819535	38.577447
2256.847208	324485.177258	38.582464
2259.130269	324970.136063	38.587482
2261.796087	325468.147020	38.592500
2264.176518	325955.717648	38.597517
2266.475047	326447.126426	38.602535
2268.891055	326934.603547	38.607552
2271.322909	327419.433606	38.612570
2273.506464	327918.656793	38.617588
2275.962114	328393.652549	38.622605
2278.513657	328879.359407	38.627623
2280.823746	329366.188963	38.632640
2282.949417	329849.058208	38.637658
2285.694263	330320.357464	38.642676
2287.703013	330798.844225	38.647693
2289.771536	331283.708730	38.652711
2292.206786	331778.758755	38.657728
2294.495562	332251.475633	38.662746
2296.645306	332738.008685	38.667764
2298.970381	333208.323366	38.672781
2301.315295	333691.794837	38.677799
2303.534644	334185.071473	38.682816
2305.614517	334657.562575	38.687834
2307.785770	335138.556552	38.692852
2309.936703	335594.054392	38.697869
2312.176461	336065.335691	38.702887
2314.633880	336523.589707	38.707904
2316.809867	336975.870434	38.712922
2318.817090	337449.047321	38.717940
2320.701372	337914.627880	38.722957
2323.038098	338385.635722	38.727975
2325.370681	338869.320032	38.732992
2327.711424	339341.937995	38.738010
2329.822539	339834.292894	38.743028
2331.697811	340324.623467	38.748045
2334.287103	340802.636149	38.753063
2336.282582	341307.061232	38.758080
2339.044982	341807.630900	38.763098
2340.890733	342322.158796	38.768116
2343.543045	342828.868493	38.773133
2345.944577	343324.476632	38.778151
2348.191811	343847.059864	38.783168
2350.009783	344350.707656	38.788186
2352.601498	344871.141856	38.793204
2354.989569	345390.889892	38.798221
2357.317346	345917.055168	38.803239
2359.608365	346431.553106	38.808256
2362.214408	346954.767767	38.813274
2364.754480	347488.837630	38.818292
2367.033308	348020.987283	38.823309
2369.605008	348539.973098	38.828327
2371.612584	349087.666398	38.833344
2374.023578	349619.211763	38.838362
2376.445766	350166.086868	38.843380
2378.808158	350703.656802	38.848397
2381.700358	351243.695778	38.853415
2384.249545	351785.199217	38.858432
2386.516442	352329.602679	38.863450
2388.816317	352866.537811	38.868468
2391.027523	353415.545805	38.873485
2393.902476	353954.121977	38.878503
2395.879089	354506.747818	38.883520
2398.884406	355052.662304	38.888538
2401.406546	355614.132470	38.893556
2403.902368	356154.732941	38.898573
2406.265128	356684.520212	38.903591
2408.896004	357236.057409	38.908608
2411.437168	357781.844435	38.913626
2413.838337	358315.957750	38.918644
2415.948798	358866.685171	38.923661
2418.818564	359406.916475	38.928679
2421.422448	359965.632832	38.933696
2423.488810	360499.126426	38.938714
2426.202275	361037.071746	38.943732
2428.355109	361582.141361	38.948749
2431.001278	362125.831208	38.953767
2433.552201	362676.546662	38.958784
2435.553538	363214.842798	38.963802
2438.348978	363754.576240	38.968820
2440.736819	364305.261410	38.973837
2443.378508	364852.221693	38.978855
2445.781222	365401.870092	38.983872
2448.017776	365937.570333	38.988890
2451.160939	366487.918586	38.993908
2453.508685	367026.495531	38.998925
2456.240196	367565.635854	39.003943
2458.180774	368116.875815	39.008960
2460.630585	368650.667461	39.013978
2463.156060	369191.659012	39.018996
2465.419007	369733.036003	39.024013
2468.329969	370274.731967	39.029031
2470.588170	370807.549839	39.034048
2473.112935	371326.000040	39.039066
2475.682649	371835.160112	39.044084
2477.973792	372343.847662	39.049101
2480.180217	372859.227877	39.054119
2482.474033	373374.812790	39.059136
2484.915903	373889.655459	39.064154
2487.505055	374407.910930	39.069172
2489.683302	374931.389020	39.074189
2492.321617	375452.783669	39.079207
2494.480712	375993.901934	39.084224
2497.119889	376521.507806	39.089242
2499.511769	377059.654926	39.094260
2501.740070	377595.916911	39.099277
2504.677365	378132.031877	39.104295
2506.850674	378676.209398	39.109312
2509.212735	379223.157869	39.114330
2511.842707	379775.676301	39.119348
2514.092268	380327.761354	39.124365
2516.822179	380875.428416	39.129383
2519.374300	381447.021586	39.134400
2521.549361	382006.250623	39.139418
2524.447190	382571.711626	39.144436
2526.664749	383148.283662	39.149453
2529.134598	383709.734366	39.154471
2531.747073	384290.043186	39.159488
2534.373207	384856.104127	39.164506
2537.215480	385448.202614	39.169524
2539.655887	386023.788452	39.174541
2542.418637	386604.451324	39.179559
2544.844735	387184.545696	39.184576
2547.143372	387774.471460	39.189594
2549.565097	388356.514430	39.194612
2552.303090	388951.483820	39.199629
2554.769623	389538.480233	39.204647
2557.474965	390133.071816	39.209664
2560.014811	390716.534606	39.214682
2562.793600	391322.935103	39.219700
2565.238002	391922.435810	39.224717
2567.842450	392519.871350	39.229735
2570.640452	393120.147954	39.234752
2572.969267	393728.381527	39.239770
2575.849757	394336.260288	39.244788
2578.488081	394932.972520	39.249805
2581.118016	395537.012163	39.254823
2583.560705	396133.522433	39.259840
2586.312843	396740.246191	39.264858
2589.068118	397339.917173	39.269876
2591.705043	397950.222111	39.274893
2594.553814	398553.694803	39.279911
2597.498731	399165.995349	39.284928
2599.939851	399766.969428	39.289946
2602.283437	400358.579016	39.294964
2605.149065	400965.074138	39.299981
2607.982945	401566.699266	39.304999
2610.433506	402170.747409	39.310016
2613.082270	402762.348692	39.315034
2615.947183	403368.021186	39.320052
2618.090165	403972.170958	39.325069
2621.098038	404581.533788	39.330087
2623.556715	405175.784102	39.335104
2625.984165	405778.828912	39.340122
2629.151973	406380.577825	39.345140
2631.173908	406981.022275	39.350157
2634.683248	407584.557583	39.355175
2637.542631	408195.919885	39.360192
2640.300239	408790.786153	39.365210
2643.011342	409391.209311	39.370228
2644.983821	409965.219483	39.375245
2647.698826	410536.315799	39.380263
2650.383625	411108.970284	39.385280
2652.773035	411673.561234	39.390298
2655.624793	412234.017956	39.395316
2657.685102	412793.875690	39.400333
2660.453519	413351.281111	39.405351
2662.909350	413926.325044	39.410368
2665.216232	414509.824547	39.415386
2667.626124	415084.996290	39.420404
2670.461506	415681.279929	39.425421
2673.076590	416264.025612	39.430439
2675.644964	416860.520167	39.435456
2678.066118	417459.398050	39.440474
2680.940495	418052.574004	39.445492
2683.458274	418656.864896	39.450509
2686.022111	419282.675474	39.455527
2688.569476	419891.224749	39.460544
2690.902836	420510.004924	39.465562
2693.881392	421137.110734	39.470580
2696.336386	421758.110123	39.475597
2698.882180	422390.909005	39.480615
2701.398712	423027.687518	39.485632
2704.412323	423679.537290	39.490650
2706.770714	424315.440764	39.495668
2709.434628	424967.202812	39.500685
2712.337479	425620.625461	39.505703
2714.890369	426280.451757	39.510720
2717.679925	426946.488148	39.515738
2720.426874	427596.382654	39.520756
2723.147990	428274.619315	39.525773
2725.840044	428932.162625	39.530791
2729.194339	429604.947114	39.535808
2731.452574	430285.765301	39.540826
2734.493403	430950.970976	39.545844
2737.055560	431622.395171	39.550861
2739.949078	432297.130742	39.555879
2742.957282	432988.856721	39.560896
2745.601365	433669.244110	39.565914
2748.383894	434337.305787	39.570932
2751.203139	435028.280964	39.575949
2754.063353	435702.448280	39.580967
2757.303925	436381.737020	39.585984
2760.088717	437069.056380	39.591002
2762.648976	437738.095409	39.596020
2765.668289	438426.592185	39.601037
2768.483576	439096.553869	39.606055
2771.375039	439786.839886	39.611072
2774.068650	440471.372290	39.616090
2777.526917	441144.444181	39.621108
2780.238668	441825.842610	39.626125
2782.959822	442504.133283	39.631143
2785.899719	443167.413401	39.636160
2788.734769	443850.536631	39.641178
2791.643412	444520.137326	39.646196
2794.378984	445199.437932	39.651213
2797.438552	445873.561721	39.656231
2800.525018	446536.495313	39.661248
2802.976811	447218.946862	39.666266
2806.007649	447886.637494	39.671284
2808.816947	448557.721438	39.676301
2811.714885	449212.961534	39.681319
2814.816706	449883.849327	39.686336
2817.404243	450554.590471	39.691354
2820.241949	451222.136968	39.696372
2822.778206	451888.897794	39.701389
2825.714083	452551.128350	39.706407
2828.512202	453222.644733	39.711424
2831.047475	453871.661691	39.716442
2833.932270	454512.270828	39.721460
2836.883627	455157.793061	39.726477
2839.184730	455790.420704	39.731495
2842.158529	456422.465952	39.736512
2844.816420	457066.095937	39.741530
2847.759513	457699.008073	39.746548
2850.582443	458359.774812	39.751565
2853.185825	458992.945027	39.756583
2855.794363	459644.510993	39.761600
2858.243966	460306.876239	39.766618
2861.276311	460953.481670	39.771636
2863.986298	461621.911514	39.776653
2866.612829	462294.213372	39.781671
2869.554963	462968.810639	39.786688
2872.443719	463648.737408	39.791706
2875.372212	464322.172764	39.796724
2878.235722	465006.791072	39.801741
2880.923666	465700.741626	39.806759
2883.736794	466396.056259	39.811776
2886.228154	467093.712578	39.816794
2889.271314	467795.137270	39.821812
2891.945128	468503.802763	39.826829
2894.652681	469223.175570	39.831847
2897.747410	469927.628687	39.836864
2900.457989	470662.824860	39.841882
2903.412713	471388.872445	39.846900
2906.389745	472116.397059	39.851917
2909.624672	472851.563888	39.856935
2912.657665	473581.938764	39.861952
2915.455832	474319.477119	39.866970
2918.615046	475053.648060	39.871988
2921.666738	475793.801792	39.877005
2924.633341	476527.179168	39.882023
2927.639521	477278.715240	39.887040
2930.371603	478015.236769	39.892058
2933.643751	478748.010379	39.897076
2936.477399	479500.325153	39.902093
2939.325336	480249.325685	39.907111
2942.392894	480999.264200	39.912128
2945.751520	481757.436870	39.917146
2948.757541	482503.936312	39.922164
2952.173212	483242.877864	39.927181
2954.852358	483980.135790	39.932199
2958.159811	484730.008444	39.937216
2961.123621	485483.223842	39.942234
2964.197116	486228.122491	39.947252
2967.202073	486966.093623	39.952269
2970.198045	487705.642675	39.957287
2973.417526	488448.848719	39.962304
2975.890132	489197.877764	39.967322
2979.037255	489941.022141	39.972340
2982.152667	490696.475110	39.977357
2985.267912	491439.349288	39.982375
2988.540343	492175.312837	39.987392
2991.488087	492930.428000	39.992410
2994.588614	493670.071631	39.997428
2997.642794	494418.296589	40.002445
3000.732851	495152.178066	40.007463
3003.645230	495894.207757	40.012480
3006.658086	496641.168926	40.017498
3009.698695	497373.538115	40.022516
3012.732935	498123.089036	40.027533
3015.850740	498858.442964	40.032551
3019.081111	499601.494292	40.037568
3021.878265	500341.857378	40.042586
3024.797544	501074.261446	40.047604
3027.860464	501819.943489	40.052621
3030.585566	502544.904989	40.057639
3033.864770	503249.009507	40.062656
3036.475298	503955.800859	40.067674
3039.254617	504650.756086	40.072692
3042.216374	505367.386204	40.077709
3044.830107	506075.833380	40.082727
3048.187258	506785.235903	40.087744
3050.855292	507505.980135	40.092762
3053.828679	508231.871875	40.097780
3057.089864	508953.757495	40.102797
3059.668876	509690.400988	40.107815
3062.809035	510419.171948	40.112832
3065.763674	511162.117699	40.117850
3068.716858	511906.331782	40.122868
3071.839262	512652.692447	40.127885
3074.758843	513406.990326	40.132903
3077.964127	514163.264165	40.137920
3080.932833	514921.142631	40.142938
3084.177886	515688.439181	40.147956
3087.314637	516456.162284	40.152973
3089.930979	517231.967681	40.157991
3093.142319	518001.000077	40.163008
3096.270542	518788.702132	40.168026
3099.120863	519558.105062	40.173044
3102.420788	520347.499299	40.178061
3105.333921	521154.800527	40.183079
3108.597385	521943.503902	40.188096
3111.903222	522744.014342	40.193114
3114.898456	523544.676239	40.198132
3117.993663	524342.711828	40.203149
3121.434959	525155.015612	40.208167
3124.471843	525948.291135	40.213184
3127.733728	526774.742260	40.218202
3130.839940	527575.545633	40.223220
3134.092418	528385.419819	40.228237
3137.235218	529204.503474	40.233255
3140.735552	530021.119321	40.238272
3143.863274	530847.134127	40.243290
3147.130369	531652.584825	40.248308
3150.435290	532468.525242	40.253325
3153.676794	533294.115442	40.258343
3157.065672	534104.014223	40.263360
3160.565372	534917.459661	40.268378
3163.318389	535728.008222	40.273396
3166.876658	536542.747071	40.278413
3169.612318	537369.961451	40.283431
3173.180000	538182.636274	40.288448
3176.348402	539015.347932	40.293466
3179.628596	539831.425201	40.298484
3183.061728	540648.529868	40.303501
3185.767822	541464.992623	40.308519
3189.305672	542272.792065	40.313536
3192.667728	543095.970684	40.318554
3195.810127	543917.072322	40.323572
3198.620221	544733.656594	40.328589
3202.374045	545556.761780	40.333607
3205.808906	546366.067560	40.338624
3208.831730	547196.451394	40.343642
3212.083796	548014.355043	40.348660
3215.590549	548829.757118	40.353677
3218.617619	549658.068118	40.358695
3221.859063	550468.889046	40.363712
3225.105424	551274.340205	40.368730
3228.350425	552083.498594	40.373748
3231.749624	552903.408079	40.378765
3234.745904	553719.966116	40.383783
3238.126602	554528.438328	40.388800
3241.486949	555358.613649	40.393818
3244.555671	556145.371754	40.398836
3247.773711	556930.050037	40.403853
3250.665153	557696.886776	40.408871
3253.803854	558471.803714	40.413888
3256.893570	559250.035021	40.418906
3260.024364	560026.204560	40.423924
3263.259297	560795.042023	40.428941
3266.584013	561589.616179	40.433959
3269.702151	562364.481437	40.438976
3272.939508	563169.682747	40.443994
3275.413338	563957.867799	40.449012
3278.978841	564768.667799	40.454029
3281.957934	565581.205771	40.459047
3285.421613	566400.271511	40.464064
3288.440732	567213.840615	40.469082
3291.246393	568037.049504	40.474100
3294.779213	568862.539201	40.479117
3297.815133	569704.568333	40.484135
3301.216095	570535.765678	40.489152
3304.225624	571381.229872	40.494170
3307.338663	572241.530897	40.499188
3310.999979	573099.378879	40.504205
3314.548033	573959.531797	40.509223
3317.342868	574834.799473	40.514240
3320.879189	575701.276914	40.519258
3323.962460	576571.260800	40.524276
3327.489774	577444.709955	40.529293
3330.730831	578334.193922	40.534311
3334.015761	579215.196521	40.539328
3337.697072	580108.071665	40.544346
3341.048853	581009.578864	40.549364
3344.102855	581901.407382	40.554381
3347.576837	582797.948752	40.559399
3351.234495	583696.938486	40.564416
3354.434414	584597.376112	40.569434
3357.841435	585503.856500	40.574452
3361.276562	586413.406578	40.579469
3364.865901	587329.554567	40.584487
3368.151384	588235.076921	40.589504
3371.725494	589145.426142	40.594522
3375.408567	590062.427873	40.599540
3379.015626	590966.321825	40.604557
3382.402671	591875.420343	40.609575
3385.724864	592785.600968	40.614592
3389.151033	593698.485339	40.619610
3392.850369	594610.649432	40.624628
3396.587851	595529.322260	40.629645
3399.731825	596433.674841	40.634663
3403.040698	597352.006852	40.639680
3406.868438	598261.988681	40.644698
3409.946926	599175.004688	40.649716
3413.640473	600082.203579	40.654733
3416.946912	600991.131566	40.659751
3420.455471	601904.890527	40.664768
3424.575567	602813.881781	40.669786
3428.131413	603738.652439	40.674804
3431.194730	604627.936381	40.679821
3434.694178	605529.151122	40.684839
3437.672320	606437.603228	40.689856
3441.014616	607348.811730	40.694874
3444.757982	608263.817489	40.699892
3447.995471	609176.924946	40.704909
3451.585606	610099.322194	40.709927
3455.312738	611016.776770	40.714944
3458.870038	611924.201387	40.719962
3462.032868	612833.102180	40.724980
3465.564608	613740.567126	40.729997
3468.845377	614649.684538	40.735015
3472.725188	615552.089822	40.740020
3476.256534	616406.110923	40.745024
3479.497391	617226.075733	40.750029
3482.919000	617966.500665	40.755034
3485.438110	618672.588119	40.760039
3488.350399	619316.665758	40.765044
3491.583334	619892.862171	40.770048
3493.701488	620436.830022	40.775053
3496.219819	620930.105992	40.780058
3498.488164	621353.569306	40.785063
3501.168184	621740.889084	40.790068
3503.033341	622070.235862	40.795072
3505.088467	622354.793150	40.800077
3507.039005	622579.778176	40.805082
3508.786527	622777.971620	40.810087
3510.569112	622925.266824	40.815092
3512.139825	623037.285804	40.820096
3512.996794	623113.259263	40.825101
3514.145833	623147.937039	40.830106
3515.137716	623156.571219	40.835111
3516.221808	623130.034000	40.840116
3517.382723	623087.753868	40.845120
3517.981552	623030.729411	40.850125
3518.653536	622919.907909	40.855130
3519.640504	622816.227363	40.860135
3520.293717	622684.481025	40.865140
3520.785138	622516.750035	40.870144
3521.035398	622352.200291	40.875149
3521.906426	622166.224746	40.880154
3522.251099	621958.601959	40.885159
3522.565663	621749.231396	40.890164
3522.882285	621525.271517	40.895168
3522.486190	621280.589527	40.900173
3523.173625	621031.536317	40.905178
3523.681971	620785.451928	40.910183
3523.451864	620517.747665	40.915188
3523.605455	620250.675520	40.920192
3523.514193	619972.344630	40.925197
3523.627863	619693.474317	40.930202
3524.013310	619413.904221	40.935207
3523.727040	619128.486109	40.940212
3523.966091	618828.389146	40.945216
3523.640713	618545.258576	40.950221
3523.899364	618228.652920	40.955226
3523.680894	617928.950080	40.960231
3523.116642	617631.340912	40.965236
3523.350518	617328.501323	40.970240
3523.090171	617025.280075	40.975245
3522.891168	616718.941806	40.980250
3522.822342	616438.509663	40.985255
3522.530787	616125.271432	40.990260
3522.877629	615819.919727	40.995264
3522.333852	615520.645245	41.000269
3522.024296	615218.976207	41.005274
3521.771013	614920.837901	41.010279
3521.544880	614621.636881	41.015284
3521.809346	614331.797090	41.020288
3521.269847	614044.923756	41.025293
3520.663617	613751.004638	41.030298
3520.599187	613460.041484	41.035303
3520.664833	613180.347101	41.040308
3520.698726	612900.449971	41.045312
3519.958255	612627.165055	41.050317
3520.316568	612342.502536	41.055322
3519.920361	612070.148604	41.060327
3519.673317	611790.964600	41.065332
3519.489154	611512.563025	41.070336
3519.285425	611239.256712	41.075341
3519.029061	610974.351237	41.080346
3518.632496	610717.560945	41.085351
3518.779900	610446.278440	41.090356
3518.046976	610184.977051	41.095360
3518.151972	609930.438644	41.100365
3517.958996	609672.290005	41.105370
3517.566459	609429.268271	41.110375
3517.618088	609174.119229	41.115380
3517.642605	608926.069452	41.120384
3516.974533	608680.822520	41.125389
3516.775829	608438.497060	41.130394
3516.479009	608209.134668	41.135399
3516.073854	607973.032110	41.140404
3516.005533	607743.973676	41.145408
3515.379832	607527.451422	41.150413
3515.338085	607298.478910	41.155418
3515.295320	607077.654532	41.160423
3515.360786	606861.160221	41.165428
3515.366653	606646.921611	41.170432
3514.976486	606432.340272	41.175437
3514.358228	606212.287569	41.180442
3514.367697	606011.791512	41.185447
3514.298438	605807.301853	41.190452
3514.331767	605595.738421	41.195456
3513.798002	605393.464288	41.200461
3513.887987	605191.638986	41.205466
3513.694757	605009.065147	41.210471
3513.710992	604818.600648	41.215476
3513.254929	604613.647501	41.220480
3512.975570	604435.779894	41.225485
3513.169680	604236.020983	41.230490
3512.864937	604060.052128	41.235495
3512.959683	603881.866350	41.240500
3512.520226	603699.558058	41.245504
3511.845530	603516.482752	41.250509
3512.017680	603346.681747	41.255514
3511.911379	603181.374857	41.260519
3511.898451	603009.095374	41.265524
3512.049159	602832.434021	41.270528
3511.200903	602667.485136	41.275533
3511.036656	602510.733512	41.280538
3510.855473	602336.367457	41.285543
3510.746501	602192.112845	41.290548
3510.910885	602034.351862	41.295552
3510.794694	601891.445383	41.300557
3510.656817	601730.824505	41.305562
3510.578798	601577.898803	41.310567
3510.192933	601428.922588	41.315572
3510.435304	601287.102835	41.320576
3509.907331	601147.453532	41.325581
3509.985006	601005.155220	41.330586
3509.836796	600854.732307	41.335591
3509.552624	600712.686775	41.340596
3509.065360	600582.382828	41.345600
3508.424355	600455.004242	41.350605
3508.942225	600320.685987	41.355610
3509.140590	600199.679770	41.360615
3508.743182	600084.271084	41.365620
3508.542973	599949.709959	41.370624
3508.511199	599843.050830	41.375629
3508.667706	599712.385143	41.380634
3508.506256	599593.680628	41.385639
3508.313551	599481.637041	41.390644
3508.455292	599360.429768	41.395648
3508.235513	599252.792905	41.400653
3508.032579	599125.429780	41.405658
3507.833413	599009.727987	41.410663
3507.656679	598899.778119	41.415668
3508.321846	598791.998192	41.420672
3508.050937	598686.265752	41.425677
3507.532257	598564.702009	41.430682
3507.579794	598459.117742	41.435687
3507.295162	598359.892013	41.440692
3507.501969	598262.140425	41.445696
3507.284111	598157.645910	41.450701
3507.320104	598052.459864	41.455706
3507.020778	597952.081156	41.460711
3506.907978	597863.487258	41.465716
3507.050138	597762.386904	41.470720
3506.872229	597670.497358	41.475725
3506.548193	597570.669585	41.480730
3506.905683	597479.595841	41.485735
3506.417064	597387.802470	41.490740
3506.648286	597296.196163	41.495744
3506.170720	597213.711805	41.500749
3506.183073	597124.391207	41.505754
3506.088956	597035.086498	41.510759
3506.168001	596950.260046	41.515764
3506.040621	596861.159337	41.520768
3505.728942	596800.325227	41.525773
3505.489402	596707.786049	41.530778
3505.676547	596631.902437	41.535783
3505.399578	596553.136739	41.540788
3506.139221	596484.876392	41.545792
3505.705396	596408.287136	41.550797
3505.638955	596327.333831	41.555802
3505.828272	596256.704593	41.560807
3505.386566	596175.808793	41.565812
3505.735082	596097.442636	41.570816
3505.071895	596017.080963	41.575821
3505.051630	595956.346659	41.580826
3505.307202	595884.102267	41.585831
3505.351836	595820.102318	41.590836
3505.171970	595745.221116	41.595840
3505.459480	595675.423901	41.600845
3505.361105	595610.343424	41.605850
3504.928973	595537.352923	41.610855
3504.890137	595457.039621	41.615860
3505.087242	595401.375768	41.620864
3504.862977	595341.120507	41.625869
3504.529263	595268.513372	41.630874
3504.919043	595209.713713	41.635879
3504.693587	595146.603214	41.640884
3505.050048	595085.504578	41.645888
3504.707886	595022.812199	41.650893
3504.740531	594952.248849	41.655898
3504.487754	594892.295961	41.660903
3504.734786	594838.874835	41.665908
3504.317960	594770.183332	41.670912
3504.622051	594718.705719	41.675917
3504.530100	594653.868769	41.680922
3504.532111	594596.578615	41.685927
3504.571976	594542.988075	41.690932
3504.475016	594471.590458	41.695936
3504.618507	594424.543502	41.700941
3504.223222	594358.149627	41.705946
3504.643968	594312.461068	41.710951
3504.271748	594257.531272	41.715956
3504.403832	594193.157296	41.720960
3504.674404	594133.669204	41.725965
3504.285138	594074.434176	41.730970
3504.453053	594022.173189	41.735975
3504.224570	593977.335908	41.740980
3504.389249	593916.711285	41.745984
3504.214365	593859.795396	41.750989
3504.538751	593803.502306	41.755994
3504.779288	593745.619384	41.760999
3504.260480	593690.659498	41.766004
3504.025727	593628.693359	41.771008
3504.160078	593583.346951	41.776013
3504.195916	593531.705212	41.781018
3504.337544	593470.931409	41.786023
3504.233909	593425.972125	41.791028
3503.989798	593362.653631	41.796032
3503.991284	593318.629066	41.801037
3504.014801	593262.830925	41.806042
3504.127373	593206.066952	41.811047
3503.796788	593161.242202	41.816052
3503.752545	593111.814709	41.821056
3503.787940	593074.144709	41.826061
3504.065459	593019.958424	41.831066
3504.056611	592970.424572	41.836071
3503.410372	592919.888229	41.841076
3503.372907	592872.612291	41.846080
3502.893239	592829.261970	41.851085
3503.495703	592784.890822	41.856090
3504.053076	592745.184665	41.861095
3503.361063	592704.171050	41.866100
3503.952024	592663.607851	41.871104
3503.621662	592620.083077	41.876109
3503.650676	592576.852563	41.881114
3503.355612	592531.669002	41.886119
3503.401503	592489.587528	41.891124
3503.846068	592441.633269	41.896128
3503.256551	592405.060382	41.901133
3503.481421	592356.689287	41.906138
3503.692067	592314.080477	41.911143
3503.463491	592279.905114	41.916148
3503.660052	592235.795509	41.921152
3503.439253	592197.411129	41.926157
3503.553389	592144.498205	41.931162
3503.554719	592110.386541	41.936167
3503.108630	592081.904755	41.941172
3502.970627	592026.275688	41.946176
3503.422772	591989.338175	41.951181
3503.239324	591951.297710	41.956186
3503.174585	591908.830523	41.961191
3503.071764	591875.335488	41.966196
3503.235309	591832.682038	41.971200
3503.035989	591795.845701	41.976205
3503.248573	591756.340064	41.981210
3503.212015	591711.613552	41.986215
3502.768986	591681.376994	41.991220
3503.440249	591639.895716	41.996224
3503.566003	591604.761143	42.001229
3503.282424	591570.642210	42.006234
3503.254735	591518.650043	42.011239
3503.487922	591486.804433	42.016244
3503.654366	591441.844689	42.021248
3503.416773	591404.762526	42.026253
3503.112047	591366.688854	42.031258
3503.170091	591321.244614	42.036263
3503.074333	591296.312739	42.041268
3503.056119	591244.568235	42.046272
3503.204714	591219.597982	42.051277
3503.423397	591179.237665	42.056282
3503.446525	591143.416303	42.061287
3502.924675	591105.024981	42.066292
3503.005627	591062.631862	42.071296
3503.070187	591035.570321	42.076301
3503.087966	590994.739765	42.081306
3503.154843	590957.808843	42.086311
3502.991735	590928.828893	42.091316
3503.268018	590882.346764	42.096320
3502.693383	590838.702656	42.101325
3502.898987	590809.664744	42.106330
3503.064019	590766.656158	42.111335
3503.187806	590746.798538	42.116340
3502.576060	590697.097956	42.121344
3502.717263	590682.547766	42.126349
3502.692310	590650.389357	42.131354
3502.683422	590609.661703	42.136359
3502.695924	590586.364469	42.141364
3502.611217	590554.165017	42.146368
3502.197069	590528.128889	42.151373
3502.601880	590495.101269	42.156378
3502.686494	590470.690359	42.161383
3502.897105	590443.854989	42.166388
3502.838881	590404.937805	42.171392
3502.748151	590373.440130	42.176397
3502.803154	590339.314454	42.181402
3503.093320	590311.314051	42.186407
3502.670641	590286.631337	42.191412
3502.914979	590247.315593	42.196416
3502.936724	590211.641644	42.201421
3502.700942	590179.665086	42.206426
3502.936964	590146.512489	42.211431
3503.012905	590120.248461	42.216436
3503.182619	590090.562929	42.221440
3502.787000	590058.009801	42.226445
3502.639669	590021.910756	42.231450
3503.157711	589991.919999	42.236455
3502.805119	589957.957037	42.241460
3503.208264	589923.024115	42.246464
3502.590135	589890.455164	42.251469
3502.381990	589849.455184	42.256474
3502.861188	589822.977089	42.261479
3502.943321	589799.166260	42.266484
3503.239020	589761.844762	42.271488
3503.035102	589730.713613	42.276493
3502.998799	589695.948859	42.281498
3503.040289	589656.562472	42.286503
3502.980536	589626.811334	42.291508
3502.816940	589589.210328	42.296512
3502.381023	589554.357283	42.301517
3502.782151	589528.692309	42.306522
3502.917157	589494.250842	42.311527
3502.722631	589477.496900	42.316532
3502.313178	589438.581034	42.321536
3502.300797	589410.074462	42.326541
3502.457732	589380.639491	42.331546
3502.388387	589363.966010	42.336551
3502.120886	589334.346749	42.341556
3502.470478	589313.148509	42.346560
3502.448191	589293.110637	42.351565
3502.208172	589256.522488	42.356570
3502.262245	589236.472575	42.361575
3502.273366	589217.681933	42.366580
3502.894420	589188.474508	42.371584
3502.797471	589162.435595	42.376589
3502.764574	589137.438793	42.381594
3502.681636	589106.938286	42.386599
3502.028085	589071.917287	42.391604
3502.501790	589043.333760	42.396608
3502.416464	589010.628752	42.401613
3502.681116	588980.424283	42.406618
3502.990266	588964.192064	42.411623
3502.169654	588936.061117	42.416628
3502.633128	588906.125990	42.421632
3502.683109	588876.806580	42.426637
3502.488453	588847.224702	42.431642
3502.842499	588824.972596	42.436647
3502.608636	588794.394590	42.441652
3503.125737	588767.156406	42.446656
3502.887924	588740.988182	42.451661
3502.558938	588706.065576	42.456666
3502.603379	588668.629270	42.461671
3502.389167	588647.618080	42.466676
3502.376036	588610.140465	42.471680
3502.699070	588585.337280	42.476685
3502.057312	588561.636891	42.481690
3502.411871	588533.120753	42.486695
3502.421851	588517.485811	42.491700
3502.505605	588483.449996	42.496704
3502.388395	588458.665237	42.501709
3502.472690	588433.147415	42.506714
3502.703013	588406.153587	42.511719
3502.272958	588376.156253	42.516724
3502.037327	588345.627363	42.521728
3502.537258	588329.163940	42.526733
3502.547996	588314.630961	42.531738
3502.390449	588282.386015	42.536743
3502.289858	588252.286725	42.541748
3502.159368	588228.756221	42.546752
3502.495467	588204.000230	42.551757
3502.637125	588182.431420	42.556762
3502.537916	588158.294570	42.561767
3502.304857	588126.111073	42.566772
3502.385305	588113.521171	42.571776
3502.051613	588081.904473	42.576781
3502.478114	588055.229867	42.581786
3502.531867	588023.602539	42.586791
3502.293923	588001.190744	42.591796
3502.597540	587983.805409	42.596800
3502.448295	587952.410046	42.601805
3502.649961	587928.626527	42.606810
3502.581498	587893.610463	42.611815
3502.069656	587870.990667	42.616820
3502.500143	587840.706992	42.621824
3502.407317	587822.130621	42.626829
3502.648596	587801.146803	42.631834
3503.088822	587765.349259	42.636839
3502.744953	587734.885680	42.641844
3503.181169	587702.746632	42.646848
3502.571856	587666.511506	42.651853
3502.218690	587635.447770	42.656858
3502.634392	587605.065528	42.661863
3502.447494	587580.039098	42.666868
3502.363729	587546.828316	42.671872
3502.840530	587517.288174	42.676877
3502.672443	587502.631729	42.681882
3502.887017	587482.703817	42.686887
3502.316322	587453.878486	42.691892
3502.544126	587422.322422	42.696896
3502.575415	587385.885989	42.701901
3502.419688	587374.434621	42.706906
3502.570521	587343.241147	42.711911
3502.134885	587307.829582	42.716916
3502.558598	587279.750361	42.721920
3501.940656	587255.542258	42.726925
3501.953358	587233.590822	42.731930
3502.344604	587201.507438	42.736935
3502.509333	587192.260871	42.741940
3502.535644	587162.289060	42.746944
3502.900457	587136.824567	42.751949
3502.738672	587114.799943	42.756954
3502.631805	587087.655100	42.761959
3502.322193	587054.127325	42.766964
3502.490130	587027.991763	42.771968
3501.915300	586998.714843	42.776973
3501.893890	586983.032486	42.781978
3502.339561	586958.156305	42.786983
3501.914414	586936.673632	42.791988
3502.298040	586915.465398	42.796993
3502.051764	586885.284865	42.801997
3502.282101	586867.859092	42.807002
3502.308487	586848.210012	42.812007
3502.113836	586837.816572	42.817012
3502.013372	586803.102687	42.822017
3502.239141	586787.832442	42.827021
3502.099920	586761.694144	42.832026
3501.758508	586747.264235	42.837031
3501.984720	586724.125745	42.842036
3501.947146	586696.267480	42.847041
3502.169930	586678.241200	42.852045
3501.969540	586660.130698	42.857050
3502.174449	586641.205070	42.862055
3501.930880	586635.279378	42.867060
3502.168595	586603.969973	42.872065
3502.077770	586583.135959	42.877069
3501.944101	586555.492819	42.882074
3502.320185	586534.535605	42.887079
3502.275012	586519.257224	42.892084
3502.190733	586498.422024	42.897089
3502.477606	586471.765373	42.902093
3502.061330	586447.373591	42.907098
3502.274303	586424.537236	42.912103
3501.574772	586409.060295	42.917108
3502.143668	586377.698468	42.922113
3502.088544	586373.597497	42.927117
3501.955506	586342.946706	42.932122
3502.098281	586328.741251	42.937127
3501.862605	586302.667047	42.942132
3501.849364	586281.118686	42.947137
3501.843146	586267.337382	42.952141
3502.003648	586248.217546	42.957146
3501.921504	586221.367384	42.962151
3501.795520	586211.513904	42.967156
3502.131505	586187.855941	42.972161
3502.029500	586165.820050	42.977165
3501.983943	586154.801235	42.982170
3502.502081	586126.353461	42.987175
3502.072955	586111.084413	42.992180
3502.146850	586087.166496	42.997185
3502.122689	586079.602416	43.002189
3502.209532	586048.114531	43.007194
3502.523194	586027.216221	43.012199
3502.232205	586005.309787	43.017204
3502.176717	585977.502604	43.022209
3502.462178	585971.995034	43.027213
3502.200843	585942.265310	43.032218
3502.427131	585904.139516	43.037223
3501.939998	585888.829105	43.042228
3502.116081	585861.236021	43.047233
3501.665180	585834.542792	43.052237
3502.071157	585819.243023	43.057242
3502.305683	585802.165732	43.062247
3502.176215	585780.083236	43.067252
3502.183694	585748.506654	43.072257
3502.149662	585735.380584	43.077261
3502.150999	585707.363351	43.082266
3502.242198	585683.742565	43.087271
3502.422916	585676.547139	43.092276
3502.149881	585649.274330	43.097281
3502.190139	585626.312946	43.102285
3502.266899	585603.646531	43.107290
3502.315698	585580.182511	43.112295
3502.251978	585563.602557	43.117300
3502.484215	585539.758929	43.122305
3502.419150	585518.016681	43.127309
3502.539961	585497.999563	43.132314
3502.635944	585470.919226	43.137319
3501.949239	585437.645910	43.142324
3501.934803	585410.632806	43.147329
3502.021874	585387.412995	43.152333
3502.074241	585368.158162	43.157338
3502.262986	585351.889270	43.162343
3502.072629	585320.693231	43.167348
3502.313645	585305.468655	43.172353
3501.984752	585286.072792	43.177357
3502.261089	585260.417274	43.182362
3502.436833	585238.737068	43.187367
3501.799900	585218.487042	43.192372
3501.745694	585196.842701	43.197377
3502.250127	585179.221022	43.202381
3502.229690	585158.974754	43.207386
3502.408126	585132.782895	43.212391
3502.329839	585104.325462	43.217396
3502.491922	585082.045609	43.222401
3502.393159	585060.508210	43.227405
3501.836562	585040.145048	43.232410
3502.299215	585014.459828	43.237415
3501.872499	584998.737734	43.242420
3501.785973	584974.541723	43.247425
3502.052455	584951.142571	43.252429
3501.886366	584946.456929	43.257434
3502.337003	584924.733129	43.262439
3502.059762	584899.764790	43.267444
3502.234578	584875.577828	43.272449
3502.295415	584854.215568	43.277453
3501.864445	584834.784737	43.282458
3501.531448	584807.017960	43.287463
3501.930224	584799.136257	43.292468
3502.275976	584782.992349	43.297473
3502.205792	584764.507475	43.302477
3502.460821	584744.818870	43.307482
3502.510004	584712.731536	43.312487
3502.187808	584697.393665	43.317492
3502.313029	584659.830709	43.322497
3502.489919	584643.712994	43.327501
3501.988103	584632.463222	43.332506
3502.373527	584596.312993	43.337511
3502.034514	584576.215700	43.342516
3502.172903	584551.582593	43.347521
3502.208637	584523.707328	43.352525
3501.953232	584510.915148	43.357530
3502.421025	584483.673995	43.362535
3502.250795	584465.454885	43.367540
3502.297845	584443.743101	43.372545
3502.658615	584410.653785	43.377549
3502.559521	584387.160203	43.382554
3502.129703	584361.061589	43.387559
3502.096100	584336.605265	43.392564
3502.321773	584315.416692	43.397569
3502.388598	584288.187611	43.402573
3502.046599	584280.170711	43.407578
3501.970308	584246.848467	43.412583
3501.959296	584226.949890	43.417588
3501.763287	584207.932353	43.422593
3501.917482	584193.571965	43.427597
3501.675448	584174.110423	43.432602
3502.198314	584144.052709	43.437607
3502.236304	584135.224391	43.442612
3502.351373	584113.601576	43.447617
3502.616686	584084.686762	43.452621
3502.235939	584058.178736	43.457626
3502.046224	584035.300097	43.462631
3501.870926	584028.961290	43.467636
3502.198309	584000.688211	43.472641
3501.883617	583981.688836	43.477645
3501.927747	583951.855820	43.482650
3502.179917	583937.880806	43.487655
3501.953429	583913.503820	43.492660
3502.012122	583897.303233	43.497665
3501.970033	583871.493736	43.502669
3502.025127	583867.725493	43.507674
3502.132521	583835.275596	43.512679
3501.741516	583822.303295	43.517684
3502.077136	583800.244356	43.522689
3502.222131	583776.360408	43.527693
3502.004823	583759.801734	43.532698
3502.160190	583736.116593	43.537703
3502.096428	583722.240823	43.542708
3501.844074	583687.641051	43.547713
3501.924536	583684.620717	43.552717
3501.979812	583663.908690	43.557722
3502.127044	583638.169308	43.562727
3501.841001	583623.826869	43.567732
3502.250112	583610.979884	43.572737
3502.063080	583582.736020	43.577741
3502.089870	583566.640192	43.582746
3502.371740	583546.494078	43.587751
3501.973255	583519.686743	43.592756
3502.177472	583494.289026	43.597761
3502.126037	583476.701393	43.602765
3502.533925	583460.194922	43.607770
3502.090628	583435.750509	43.612775
3502.102888	583417.300607	43.617780
3502.169989	583389.517823	43.622785
3501.905637	583371.060956	43.627789
3501.910634	583346.195347	43.632794
3502.320435	583322.369279	43.637799
3502.165033	583307.655087	43.642804
3502.153334	583288.256228	43.647809
3501.906479	583258.366559	43.652813
3501.865747	583242.932518	43.657818
3502.048986	583225.458190	43.662823
3502.328033	583203.106113	43.667828
3502.405639	583186.600734	43.672833
3502.408112	583158.927734	43.677837
3501.660841	583134.229379	43.682842
3502.193709	583112.088096	43.687847
3502.268064	583089.868052	43.692852
3502.292536	583068.808798	43.697857
3502.142533	583039.805771	43.702861
3502.419434	583022.617273	43.707866
3502.412130	583005.773972	43.712871
3502.075599	582967.625699	43.717876
3502.194631	582951.163624	43.722881
3502.424152	582931.876824	43.727885
3502.399303	582907.365819	43.732890
3502.228868	582882.576722	43.737895
3502.218234	582866.285189	43.742900
3502.249877	582839.609486	43.747905
3502.483644	582808.340000	43.752909
3501.967713	582794.784413	43.757914
3502.264614	582767.264935	43.762919
3502.204995	582752.083826	43.767924
3501.897289	582722.603282	43.772929
3502.174797	582706.817938	43.777933
3501.878502	582680.694453	43.782938
3501.997460	582668.744007	43.787943
3502.067557	582644.568511	43.792948
3501.880927	582615.519958	43.797953
3502.069859	582595.386637	43.802957
3501.799546	582587.106617	43.807962
3502.011396	582560.402067	43.812967
3502.169584	582545.036220	43.817972
3501.960794	582532.384847	43.822977
3502.449483	582509.597517	43.827981
3501.926139	582489.926295	43.832986
3502.242666	582470.274145	43.837991
3502.044827	582441.828504	43.842996
3502.100891	582416.050386	43.848001
3502.385340	582396.854335	43.853005
3501.740009	582382.065091	43.858010
3501.917189	582355.766547	43.863015
3502.234217	582335.111374	43.868020
3501.840705	582309.704101	43.873025
3502.185544	582294.509269	43.878029
3502.020699	582277.739619	43.883034
3502.195054	582249.235296	43.888039
3501.867736	582225.822911	43.893044
3501.995234	582204.645629	43.898049
3501.843856	582200.207191	43.903053
3501.430510	582179.565634	43.908058
3502.019576	582167.190203	43.913063
3501.962992	582150.303163	43.918068
3501.879274	582130.963661	43.923073
3502.114012	582114.331842	43.928077
3502.061942	582101.505066	43.933082
3501.816734	582071.812464	43.938087
3502.170505	582058.821920	43.943092
3502.077605	582042.140939	43.948097
3502.071900	582015.118124	43.953101
3502.073193	581995.915507	43.958106
3502.051177	581961.374575	43.963111
3502.138636	581961.812133	43.968116
3502.312069	581929.045479	43.973121
3502.448434	581906.713085	43.978125
3501.848350	581876.473788	43.983130
3502.034584	581853.882804	43.988135
3501.913873	581836.102833	43.993140
3502.310537	581825.461779	43.998145
3502.397636	581797.822273	44.003149
3501.908126	581769.821598	44.008154
3502.327624	581756.268908	44.013159
3501.881272	581733.576018	44.018164
3501.952608	581707.793860	44.023169
3501.857647	581692.616818	44.028173
3501.770465	581677.588955	44.033178
3501.772299	581656.430268	44.038183
3502.387968	581649.314636	44.043188
3501.998529	581620.997108	44.048193
3502.056379	581594.264161	44.053197
3502.133606	581584.625449	44.058202
3502.245542	581560.541319	44.063207
3502.238786	581548.709594	44.068212
3501.628638	581524.637990	44.073217
3501.790924	581506.311857	44.078221
3502.063375	581475.333389	44.083226
3501.910452	581461.769547	44.088231
3501.594766	581447.378764	44.093236
3501.604570	581420.753187	44.098241
3501.561398	581413.690262	44.103245
3501.909447	581405.162265	44.108250
3501.594207	581378.537261	44.113255
3501.843344	581374.988532	44.118260
3501.856464	581357.437568	44.123265
3501.934592	581337.269140	44.128269
3501.704623	581319.856397	44.133274
3501.666079	581293.940033	44.138279
3501.967100	581291.335828	44.143284
3501.802069	581265.338891	44.148289
3502.014739	581249.210625	44.153293
3501.705935	581235.019050	44.158298
3501.585109	581205.254535	44.163303
3501.991091	581210.004550	44.168308
3501.618726	581175.465793	44.173313
3501.907293	581168.100147	44.178317
3501.556957	581151.458066	44.183322
3501.783965	581125.850780	44.188327
3501.665458	581122.860853	44.193332
3501.278561	581100.809198	44.198337
3501.732171	581080.982732	44.203341
3501.577639	581072.382626	44.208346
3501.748517	581066.539543	44.213351
3501.452311	581045.476422	44.218356
3501.585900	581040.040285	44.223361
3501.879322	581030.818565	44.228365
3501.371545	581009.688168	44.233370
3501.690840	580989.732113	44.238375
3501.505413	580981.838746	44.243380
3501.535786	580969.047909	44.248385
3501.619913	580943.863672	44.253389
3501.526859	580946.686148	44.258394
3501.658892	580926.909680	44.263399
3501.519482	580918.607940	44.268404
3501.410394	580908.997766	44.273409
3501.770194	580902.272653	44.278413
3501.017319	580887.046931	44.283418
3501.318864	580861.577809	44.288423
3501.376351	580866.984157	44.293428
3501.329168	580863.581873	44.298433
3501.532810	580852.418501	44.303437
3501.713748	580833.436494	44.308442
3501.760682	580827.662805	44.313447
3501.473895	580808.703732	44.318452
3501.420181	580795.675129	44.323457
3501.763204	580783.236340	44.328461
3501.326576	580770.768992	44.333466
3501.318435	580737.275062	44.338471
3501.435328	580741.669333	44.343476
3501.215934	580732.778246	44.348481
3501.762429	580732.241527	44.353485
3501.452266	580709.424956	44.358490
3501.369403	580692.740370	44.363495
3501.579937	580695.716022	44.368500
3501.570564	580683.883782	44.373505
3501.622141	580658.352986	44.378509
3501.810823	580660.529776	44.383514
3501.681954	580636.380997	44.388519
3501.591974	580614.733244	44.393524
3501.254871	580614.384794	44.398529
3501.210089	580603.560867	44.403533
3501.120340	580588.431640	44.408538
3501.604799	580566.242701	44.413543
3501.660069	580562.122301	44.418548
3501.705695	580573.798567	44.423553
3502.006674	580541.609592	44.428557
3501.322018	580526.071846	44.433562
3501.768878	580517.126575	44.438567
3501.832733	580496.708132	44.443572
3501.408578	580490.707050	44.448577
3501.562448	580472.631245	44.453581
3501.599035	580453.520723	44.458586
3501.649194	580444.787842	44.463591
3501.843413	580437.637039	44.468596
3501.536129	580410.807887	44.473601
3502.016517	580400.252671	44.478605
3501.701224	580388.568229	44.483610
3501.635007	580370.877673	44.488615
3501.583355	580365.069011	44.493620
3501.280606	580348.368137	44.498625
3501.431331	580331.345625	44.503629
3501.786461	580318.252547	44.508634
3501.478426	580310.377868	44.513639
3501.112439	580283.156428	44.518644
3500.971043	580271.845834	44.523649
3501.339212	580258.850937	44.528653
3501.539846	580271.155171	44.533658
3501.550474	580262.077313	44.538663
3501.413702	580251.116989	44.543668
3501.632596	580246.970893	44.548673
3501.680112	580225.200596	44.553677
3501.871025	580218.551618	44.558682
3501.534107	580201.254125	44.563687
3501.440818	580199.313050	44.568692
3501.479823	580189.328086	44.573697
3501.944161	580167.241789	44.578701
3501.904681	580159.776326	44.583706
3501.578555	580130.492326	44.588711
3501.674794	580115.985268	44.593716
3501.496972	580108.591543	44.598721
3501.913238	580082.300375	44.603725
3501.871552	580083.610673	44.608730
3501.721153	580064.127549	44.613735
3501.788569	580045.312380	44.618740
3501.725558	580044.770624	44.623745
3502.034221	580011.174833	44.628749
3501.494744	580002.834657	44.633754
3501.818413	579983.728594	44.638759
3501.772347	579964.128693	44.643764
3501.727531	579948.139084	44.648769
3501.613263	579932.310749	44.653773
3501.785725	579917.189762	44.658778
3501.758492	579903.554216	44.663783
3501.631114	579877.297405	44.668788
3501.329389	579869.020253	44.673793
3501.754833	579850.549957	44.678797
3501.555560	579837.191957	44.683802
3501.364984	579812.549566	44.688807
3502.039364	579811.040029	44.693812
3501.656185	579801.622184	44.698817
3501.817242	579777.025037	44.703821
3501.475319	579770.609532	44.708826
3501.486975	579763.837866	44.713831
3501.699395	579748.208933	44.718836
3501.644152	579738.238297	44.723841
3501.700725	579722.784133	44.728845
3501.707206	579699.314217	44.733850
3501.715452	579695.000259	44.738855
3501.746392	579680.201957	44.743860
3501.656373	579655.142318	44.748865
3501.948516	579652.840008	44.753869
3501.580649	579638.103996	44.758874
3501.830582	579617.253668	44.763879
3501.985973	579608.353237	44.768884
3501.977658	579583.932584	44.773889
3501.581870	579571.808534	44.778893
3501.339231	579561.415705	44.783898
3501.443109	579548.210558	44.788903
3501.753352	579541.993855	44.793908
3501.187456	579526.285692	44.798913
3501.322799	579504.249513	44.803917
3501.456413	579503.125363	44.808922
3501.381832	579498.673832	44.813927
3501.593198	579498.239601	44.818932
3501.475218	579472.381550	44.823937
3501.604128	579464.086923	44.828941
3501.295316	579457.766356	44.833946
3501.617255	579433.394042	44.838951
3501.752945	579416.773670	44.843956
3501.455533	579408.595796	44.848961
3501.627474	579397.135031	44.853965
3501.728087	579387.841798	44.858970
3501.867408	579370.067369	44.863975
3501.771251	579355.539249	44.868980
3501.771568	579338.287988	44.873985
3501.579447	579326.332425	44.878989
3501.597348	579307.072408	44.883994
3501.605644	579285.206105	44.888999
3501.331113	579284.496782	44.894004
3501.355027	579268.044109	44.899009
3501.572592	579249.103824	44.904013
3501.296927	579239.317648	44.909018
3501.458215	579238.690638	44.914023
3501.459359	579215.421134	44.919028
3501.513997	579209.946298	44.924033
3501.637881	579202.103607	44.929037
3501.476284	579201.527072	44.934042
3501.201999	579171.530347	44.939047
3501.559174	579166.559840	44.944052
3501.620558	579156.319703	44.949057
3501.415313	579134.837535	44.954061
3501.356344	579124.465734	44.959066
3501.417000	579115.680019	44.964071
3501.462174	579110.808412	44.969076
3501.509234	579104.783060	44.974081
3501.682223	579071.155495	44.979085
3501.774470	579079.465985	44.984090
3501.145292	579047.217502	44.989095
3501.508045	579036.328339	44.994100
3501.695413	579022.808617	44.999105
3501.858251	579012.101135	45.004109
3501.747153	579008.256921	45.009114
3501.614801	578986.712921	45.014119
3501.829893	578973.590009	45.019124
3501.694933	578952.898912	45.024129
3502.086038	578941.152664	45.029133
3501.867557	578926.944011	45.034138
3501.700012	578913.830696	45.039143
3501.894557	578892.937523	45.044148
3501.682842	578880.031676	45.049153
3501.898381	578863.397998	45.054157
3501.595980	578843.384836	45.059162
3501.910055	578818.159840	45.064167
3501.468434	578817.426455	45.069172
3500.996952	578800.498873	45.074177
3501.336459	578775.019047	45.079181
3501.092566	578784.585940	45.084186
3501.605562	578775.127427	45.089191
3501.876505	578770.721892	45.094196
3501.553070	578751.765034	45.099201
3502.115708	578742.499339	45.104205
3501.442595	578728.311354	45.109210
3501.418940	578706.649517	45.114215
3501.443441	578694.258197	45.119220
3501.224831	578686.418534	45.124225
3501.475893	578658.946196	45.129229
3501.154158	578655.786764	45.134234
3501.098389	578651.231649	45.139239
3501.466016	578644.554111	45.144244
3501.395522	578645.016496	45.149249
3501.443776	578622.641127	45.154253
3501.065118	578619.891800	45.159258
3501.304414	578608.971370	45.164263
3501.417510	578606.997752	45.169268
3501.259434	578591.525423	45.174273
3501.678123	578581.329206	45.179277
3501.275130	578569.656557	45.184282
3501.699260	578557.302916	45.189287
3501.588494	578537.961381	45.194292
3501.586971	578532.244230	45.199297
3501.873957	578528.036702	45.204301
3501.652238	578508.963225	45.209306
3501.809991	578489.228560	45.214311
3501.890116	578481.642968	45.219316
3501.353416	578453.791748	45.224321
3501.401073	578443.954327	45.229325
3501.422439	578446.558935	45.234330
3501.467323	578430.051596	45.239335
3501.541792	578408.474147	45.244340
3501.754061	578401.870905	45.249345
3501.685057	578382.773338	45.254349
3501.714574	578364.713555	45.259354
3501.794654	578364.199501	45.264359
3501.649413	578342.255045	45.269364
3501.367856	578322.438302	45.274369
3501.666178	578313.012960	45.279373
3501.327797	578315.222457	45.284378
3501.576949	578271.499720	45.289383
3501.814771	578270.509619	45.294388
3501.780668	578274.978625	45.299393
3501.719724	578249.359590	45.304397
3501.515548	578242.319818	45.309402
3501.446534	578235.459528	45.314407
3501.573633	578215.077170	45.319412
3501.535925	578207.559968	45.324417
3502.019447	578190.732933	45.329421
3501.614047	578170.784819	45.334426
3501.402399	578152.511624	45.339431
3501.450636	578157.218576	45.344436
3501.239500	578134.431392	45.349441
3501.696009	578121.018969	45.354445
3501.367935	578111.340301	45.359450
3501.369722	578099.002026	45.364455
3501.715844	578088.214852	45.369460
3501.739081	578081.841591	45.374465
3501.793228	578065.131647	45.379469
3501.841793	578051.732759	45.384474
3501.531329	578022.541073	45.389479
3502.037835	578028.681084	45.394484
3501.929120	578006.981033	45.399489
3501.808801	577976.204699	45.404493
3501.946533	577960.735408	45.409498
3501.557885	577946.552107	45.414503
3501.827218	577934.021360	45.419508
3501.705730	577919.545484	45.424513
3501.765384	577899.674649	45.429517
3501.600995	577886.359010	45.434522
3501.701824	577867.033390	45.439527
3501.925678	577859.073819	45.444532
3501.478833	577841.739683	45.449537
3501.578248	577824.370279	45.454541
3501.308919	577818.494006	45.459546
3501.492877	577803.067426	45.464551
3501.635513	577790.004610	45.469556
3501.821783	577781.298521	45.474561
3501.349777	577761.059151	45.479565
3501.296477	577739.349918	45.484570
3501.569209	577736.598850	45.489575
3501.572120	577728.122009	45.494580
3501.391406	577712.551689	45.499585
3501.521049	577687.954852	45.504589
3501.383650	577704.427587	45.509594
3501.395057	577693.792673	45.514599
3501.700045	577664.052431	45.519604
3501.223244	577650.785350	45.524609
3501.568678	577644.863036	45.529613
3501.613345	577638.385860	45.534618
3501.816723	577615.532816	45.539623
3501.878955	577609.704913	45.544628
3501.732811	577593.928397	45.549633
3501.689446	577585.508839	45.554637
3501.450911	577574.762415	45.559642
3501.503092	577556.747942	45.564647
3502.065038	577536.647469	45.569652
3501.494379	577534.830711	45.574657
3501.394041	577513.830591	45.579661
3501.342416	577499.242936	45.584666
3501.303208	577497.343090	45.589671
3501.689703	577479.978431	45.594676
3501.467066	577476.702854	45.599681
3501.510421	577458.890232	45.604685
3501.636302	577446.180737	45.609690
3501.464746	577432.364103	45.614695
3501.372032	577404.842116	45.619700
3501.163578	577402.868397	45.624705
3501.537263	577396.289488	45.629709
3501.532525	577390.020521	45.634714
3501.506769	577375.177872	45.639719
3501.407744	577365.512906	45.644724
3501.139870	577361.090739	45.649729
3501.304639	577350.882944	45.654733
3501.409070	577327.844152	45.659738
3501.215793	577315.585665	45.664743
3501.687447	577311.148184	45.669748
3501.498306	577312.431699	45.674753
3501.909212	577286.385589	45.679757
3501.783296	577272.912730	45.684762
3501.622267	577261.602148	45.689767
3501.907505	577237.331107	45.694772
3501.455620	577221.351070	45.699777
3501.622130	577208.534637	45.704781
3501.423075	577193.869314	45.709786
3501.792699	577186.689015	45.714791
3501.753521	577174.255808	45.719796
3501.564198	577153.218765	45.724801
3501.372376	577133.686837	45.729805
3501.799173	577134.322336	45.734810
3501.637196	577118.798419	45.739815
3501.726997	577106.696086	45.744820
3501.589226	577080.283841	45.749825
3501.409482	577006.929033	45.754829
3501.688820	576903.707082	45.759834
3500.707276	576743.749230	45.764839
3500.579875	576538.660833	45.769844
3500.173240	576308.280320	45.774849
3500.033376	576004.213105	45.779853
3499.591976	575663.614327	45.784858
3499.106819	575280.520665	45.789863
3498.223116	574834.163131	45.794868
3497.820240	574371.156325	45.799873
3496.979590	573863.143413	45.804877
3496.425259	573301.675976	45.809882
3495.659834	572696.458167	45.814887
3494.490297	572039.132928	45.819892
3493.751345	571356.560056	45.824897
3492.669057	570620.751054	45.829901
3491.569860	569855.083931	45.834906
3490.353287	569039.741689	45.839911
3489.141788	568188.097699	45.844916
3487.843674	567295.941427	45.849921
3485.848959	566369.584600	45.854925
3484.560846	565409.502780	45.859930
3483.269302	564405.705729	45.864935
3481.659766	563364.358333	45.869940
3479.715378	562298.260539	45.874945
3477.961305	561184.871711	45.879949
3475.881895	560053.897091	45.884954
3473.917443	558890.241961	45.889959
3472.383321	557685.205982	45.894964
3469.965710	556455.212738	45.899969
3467.986900	555197.435073	45.904973
3465.691802	553914.495809	45.909978
3463.997709	552599.508609	45.914983
3461.847200	551258.711664	45.919988
3458.757323	549894.937727	45.924993
3456.656534	548493.246339	45.929997
3453.906356	547082.746367	45.935002
3451.398705	545646.146136	45.940007
3448.788210	544188.521266	45.945012
3446.645678	542712.743951	45.950017
3444.018797	541213.926436	45.955021
3441.156427	539695.091789	45.960026
3438.395262	538151.903607	45.965031
3435.479207	536590.634876	45.970036
3432.598528	535031.132754	45.975041
3430.016034	533435.349897	45.980045
3427.290830	531830.279044	45.985050
3424.081403	530213.403179	45.990055
3420.900977	528568.321980	45.995060
3417.743646	526924.290102	46.000065
3415.010914	525256.261298	46.005069
3411.711269	523590.126726	46.010074
3408.684931	521904.292613	46.015079
3405.562002	520209.443407	46.020084
3401.909180	518494.859471	46.025089
3399.076047	516783.207472	46.030093
3395.515554	515061.322407	46.035098
3392.457037	513319.329398	46.040103
3388.795282	511580.539630	46.045108
3385.333147	509828.995102	46.050113
3382.268298	508070.461761	46.055117
3378.783671	506301.434327	46.060122
3375.055181	504536.361686	46.065127
3371.728519	502763.036564	46.070132
3368.182006	500984.885060	46.075137
3364.565917	499198.703923	46.080141
3361.253618	497404.988546	46.085146
3357.684124	495610.539247	46.090151
3354.168540	493807.836705	46.095156
3350.493227	492010.899191	46.100161
3346.870026	490188.388329	46.105165
3343.292561	488391.407768	46.110170
3339.553756	486592.977588	46.115175
3336.066214	484773.434061	46.120180
3332.011995	482970.689665	46.125185
3328.602943	481153.184540	46.130189
3325.009613	479334.789996	46.135194
3321.151262	477517.490960	46.140199
3317.571148	475706.157863	46.145204
3313.285760	473898.673287	46.150209
3310.068220	472072.972944	46.155213
3306.247881	470259.751998	46.160218
3302.156366	468453.907510	46.165223
3299.025508	466640.129438	46.170228
3294.919403	464831.617042	46.175233
3291.366914	463015.134357	46.180237
3287.328402	461209.561090	46.185242
3283.586050	459403.649060	46.190247
3280.259348	457589.335588	46.195252
3276.366152	455783.068124	46.200257
3272.636157	453968.692999	46.205261
3268.808435	452162.598988	46.210266
3265.135224	450350.070619	46.215271
3261.211909	448550.813675	46.220276
3256.942119	446751.077043	46.225281
3253.363667	444950.041537	46.230285
3249.807276	443156.472575	46.235290
3245.835847	441374.088672	46.240295
3241.788234	439570.019832	46.245300
3238.130392	437782.129503	46.250305
3234.495625	435987.481321	46.255309
3230.691834	434218.277194	46.260314
3226.570085	432435.229240	46.265319
3222.903182	430654.024624	46.270324
3218.724207	428890.020141	46.275329
3214.985715	427106.023376	46.280333
3211.593410	425349.438273	46.285338
3207.463093	423587.188915	46.290343
3203.959505	421821.799420	46.295348
3200.114691	420064.778742	46.300353
3196.397651	418302.417382	46.305357
3192.509611	416547.743699	46.310362
3188.839821	414799.280144	46.315367
3185.146979	413035.258754	46.320372
3181.237637	411288.067853	46.325377
3177.297024	409544.393738	46.330381
3173.311052	407809.770350	46.335386
3169.706976	406069.320083	46.340391
3165.437457	404328.229717	46.345396
3161.845702	402604.455875	46.350401
3158.195893	400868.940294	46.355405
3154.075242	399148.643240	46.360410
3150.433405	397443.725401	46.365415
3146.928624	395713.944172	46.370420
3142.986840	394006.642946	46.375425
3138.846773	392297.271568	46.380429
3135.821617	390594.560564	46.385434
3131.061152	388889.844918	46.390439
3127.841676	387182.511566	46.395444
3124.104579	385489.157426	46.400449
3120.216828	383792.539747	46.405453
3116.372397	382103.522034	46.410458
3112.254073	380421.775687	46.415463
3108.990351	378734.987808	46.420468
3105.244078	377055.710729	46.425473
3101.388036	375373.272112	46.430477
3097.775903	373696.862942	46.435482
3093.670976	372024.162145	46.440487
3089.919616	370346.249667	46.445492
3086.011468	368694.809159	46.450497
3082.155280	367025.835497	46.455501
3078.476277	365378.765440	46.460506
3074.658031	363736.146426	46.465511
3071.187714	362076.864159	46.470516
3066.760178	360438.857904	46.475521
3063.020644	358790.870662	46.480525
3059.411362	357159.369655	46.485530
3055.585935	355525.986124	46.490535
3051.821145	353902.954171	46.495540
3047.972872	352282.571725	46.500545
3044.371750	350657.238821	46.505549
3040.530484	349033.666922	46.510554
3036.697203	347429.131249	46.515559
3033.174917	345819.867934	46.520564
3029.395092	344214.102204	46.525569
3025.822186	342607.211684	46.530573
3022.038191	341008.416421	46.535578
3017.871293	339417.618262	46.540583
3014.428527	337823.380899	46.545588
3010.475778	336219.794530	46.550593
3006.738562	334629.150825	46.555597
3003.205114	333054.938588	46.560602
2999.553305	331460.917152	46.565607
2996.039381	329874.972478	46.570612
2992.037992	328298.272648	46.575617
2988.423723	326728.037534	46.580621
2984.681096	325150.180564	46.585626
2981.236124	323577.558150	46.590631
2977.363025	322004.332433	46.595636
2973.576825	320444.568834	46.600641
2969.966751	318876.401410	46.605645
2966.337434	317308.613010	46.610650
2962.371019	315749.650684	46.615655
2958.655662	314194.233662	46.620660
2955.011345	312653.510951	46.625665
2951.212748	311097.035796	46.630669
2947.555995	309556.315385	46.635674
2943.620357	308018.541416	46.640679
2940.255671	306469.051088	46.645684
2936.146839	304938.792572	46.650689
2932.610801	303403.537752	46.655693
2928.890499	301857.729959	46.660698
2925.382888	300333.808615	46.665703
2921.643025	298810.084441	46.670708
2917.981911	297288.215026	46.675713
2914.185759	295765.231306	46.680717
2910.633219	294247.489302	46.685722
2907.115588	292734.895648	46.690727
2903.113309	291217.681571	46.695732
2899.629779	289712.898978	46.700737
2896.054001	288191.879111	46.705741
2892.155641	286685.690117	46.710746
2888.390504	285192.404151	46.715751
2885.403112	283682.186700	46.720756
2881.130045	282173.741551	46.725761
2877.167644	280666.820000	46.730765
2873.365071	279167.404210	46.735770
2869.508160	277670.767846	46.740775
2866.431396	276180.065852	46.745780
2862.610704	274696.556188	46.750785
2858.994183	273216.170644	46.755789
2855.170067	271731.183112	46.760794
2851.576381	270250.692237	46.765799
2848.150211	268775.294531	46.770804
2844.455839	267300.017390	46.775809
2840.613917	265822.678305	46.780813
2837.262420	264352.319874	46.785818
2833.455950	262880.942350	46.790823
2830.009847	261407.986052	46.795828
2826.031452	259958.292641	46.800833
2822.617462	258485.777752	46.805837
2819.024762	257026.591800	46.810842
2815.285402	255568.812825	46.815847
2811.471685	254099.111369	46.820852
2807.764452	252650.464404	46.825857
2804.193623	251204.736159	46.830861
2800.430032	249733.557566	46.835866
2796.723918	248292.765045	46.840871
2792.960115	246849.321171	46.845876
2789.465112	245415.170881	46.850881
2785.548819	243971.118318	46.855885
2782.225364	242533.177664	46.860890
2778.563402	241097.089413	46.865895
2775.093578	239666.260503	46.870900
2771.292947	238222.792740	46.875905
2767.686193	236801.089154	46.880909
2764.019757	235376.383838	46.885914
2760.534594	233944.743051	46.890919
2756.735859	232532.095759	46.895924
2753.018360	231104.889394	46.900929
2749.576431	229685.481422	46.905933
2745.872340	228260.483568	46.910938
2741.950816	226849.959135	46.915943
2738.319135	225437.783999	46.920948
2734.518578	224028.131109	46.925953
2730.994545	222617.365824	46.930957
2727.522732	221215.278544	46.935962
2723.510628	219814.805804	46.940967
2720.167827	218406.131835	46.945972
2716.446363	217013.820435	46.950977
2713.229911	215607.324213	46.955981
2709.302512	214214.544089	46.960986
2705.485490	212823.611104	46.965991
2702.077657	211429.385466	46.970996
2698.161265	210038.607721	46.976001
2694.346398	208655.207037	46.981005
2691.286008	207270.244398	46.986010
2687.608821	205893.281676	46.991015
2684.050167	204505.281825	46.996020
2680.273521	203136.477403	47.001025
2676.823450	201748.811625	47.006029
2673.032734	200361.592163	47.011034
2669.067732	198998.274151	47.016039
2665.810624	197619.526365	47.021044
2662.157538	196260.717160	47.026049
2658.267671	194888.384559	47.031053
2654.839122	193532.495688	47.036058
2651.038545	192169.548846	47.041063
2647.551517	190806.746218	47.046068
2643.712140	189440.118157	47.051073
2640.164492	188086.855267	47.056077
2636.801775	186735.591762	47.061082
2633.082136	185387.074987	47.066087
2629.541640	184031.290715	47.071092
2625.695039	182680.869220	47.076097
2621.788563	181331.418187	47.081101
2618.425015	179986.968850	47.086106
2614.657198	178661.877711	47.091111
2611.169784	177308.449031	47.096116
2607.599856	175965.646707	47.101121
2603.726444	174639.539671	47.106125
2600.561882	173304.266779	47.111130
2596.869838	171976.100594	47.116135
2593.140049	170640.248965	47.121140
2589.439608	169319.679444	47.126145
2585.584840	167984.964582	47.131149
2581.736937	166668.832764	47.136154
2578.321863	165349.323069	47.141159
2574.765558	164038.961994	47.146164
2570.979105	162732.417516	47.151169
2567.419842	161423.967101	47.156173
2564.109815	160103.349245	47.161178
2560.263755	158805.421909	47.166183
2556.634805	157487.531434	47.171188
2552.962966	156191.350743	47.176193
2549.045292	154891.367934	47.181197
2545.748693	153587.219121	47.186202
2541.848274	152295.615408	47.191207
2538.502360	151000.136955	47.196212
2534.732780	149720.624169	47.201217
2530.769660	148426.512308	47.206221
2527.404214	147157.559499	47.211226
2523.801605	145787.652946	47.216231
2520.392490	144496.122113	47.221236
2517.050419	143225.137694	47.226241
2513.335788	141941.774723	47.231245
2509.724539	140661.406457	47.236250
2505.970198	139392.723416	47.241255
2502.478758	138113.027938	47.246260
2498.968063	136832.950582	47.251265
2494.968563	135568.277044	47.256269
2491.781128	134308.892884	47.261274
2487.955169	133031.147156	47.266279
2484.232857	131764.959993	47.271284
2480.648000	130512.551711	47.276289
2476.660511	129249.506975	47.281293
2473.871957	127987.482451	47.286298
2469.719381	126735.223391	47.291303
2466.050223	125473.781587	47.296308
2462.590553	124236.460499	47.301313
2459.164519	122987.547565	47.306317
2455.469099	121737.482242	47.311322
2451.443030	120500.378370	47.316327
2448.270487	119253.795110	47.321332
2444.381851	118011.560746	47.326337
2440.868532	116771.457301	47.331341
2437.479316	115531.845841	47.336346
2433.577806	114293.334957	47.341351
2430.160693	113062.991191	47.346356
2426.719314	111829.285393	47.351361
2422.544814	110618.558400	47.356365
2419.168104	109388.562959	47.361370
2415.439687	108154.762598	47.366375
2411.879011	106933.476368	47.371380
2408.010523	105721.688700	47.376385
2404.475790	104503.930056	47.381389
2400.942015	103301.329047	47.386394
2396.974695	102091.721045	47.391399
2393.587879	100878.710922	47.396404
2389.909438	99681.462760	47.401409
2386.252321	98483.365799	47.406413
2382.685285	97283.062649	47.411418
2378.797415	96087.607973	47.416423
2375.362401	94903.704857	47.421428
2371.423758	93723.000648	47.426433
2367.772922	92532.270564	47.431437
2364.475168	91348.354932	47.436442
2360.510580	90174.983341	47.441447
2356.937244	89007.085083	47.446452
2353.350750	87836.617305	47.451457
2349.322710	86665.400965	47.456461
2346.372362	85489.781489	47.461466
2342.526843	84333.214378	47.466471
2338.822651	83171.196481	47.471476
2335.151170	82018.493525	47.476481
2331.840783	80872.055703	47.481485
2328.027280	79711.542944	47.486490
2323.976087	78563.194247	47.491495
2320.396007	77426.033972	47.496500
2316.819284	76277.121945	47.501505
2312.964161	75154.615066	47.506509
2309.620468	74013.737517	47.511514
2305.666397	72889.219705	47.516519
2302.209592	71758.157546	47.521524
2298.422269	70627.741416	47.526529
2294.545645	69512.706510	47.531533
2290.917970	68404.447409	47.536538
2286.925054	67303.053323	47.541543
2283.887292	66185.465959	47.546548
2280.275218	65082.457414	47.551553
2276.320295	63984.044184	47.556557
2272.906185	62880.244002	47.561562
2269.101956	61802.351874	47.566567
2265.721181	60704.557761	47.571572
2261.478179	59615.768183	47.576577
2257.981779	58535.914612	47.581581
2254.672943	57459.810664	47.586586
2251.035239	56390.309726	47.591591
2247.050093	55311.298466	47.596596
2243.664539	54243.928700	47.601601
2239.902314	53180.021978	47.606605
2236.325798	52121.824717	47.611610
2232.194041	51063.356152	47.616615
2229.101523	50001.512680	47.621620
2225.048375	48942.595746	47.626625
2221.722181	47903.872571	47.631629
2217.929682	46859.504279	47.636634
2213.764382	45834.820586	47.641639
2210.170403	44790.605443	47.646644
2206.397510	43768.205792	47.651649
2202.658732	42740.996557	47.656653
2199.068062	41714.915035	47.661658
2194.934476	40716.117058	47.666663
2191.683970	39698.794811	47.671668
2187.826819	38704.547112	47.676673
2184.064583	37712.105274	47.681677
2180.224241	36713.616320	47.686682
2176.583195	35734.692863	47.691687
2172.863504	34749.062926	47.696692
2168.996989	33779.183550	47.701697
2165.206889	32809.108561	47.706701
2161.674701	31848.741591	47.711706
2157.808634	30893.211628	47.716711
2154.095138	29930.248777	47.721716
2150.126494	28983.169291	47.726721
2146.133034	28051.694365	47.731725
2142.350310	27102.118711	47.736730
2138.525904	26192.772492	47.741735
2134.971406	25275.130873	47.746740
2131.339524	24362.579965	47.751745
2127.447849	23450.136446	47.756749
2123.455032	22560.018553	47.761754
2119.881841	21664.382390	47.766759
2115.853505	20788.501561	47.771764
2112.043490	19899.202924	47.776769
2108.207013	19034.423475	47.781773
2104.229487	18172.643169	47.786778
2100.014839	17325.479805	47.791783
2096.072027	16484.704285	47.796788
2092.078433	15666.445815	47.801793
2087.468308	14849.718113	47.806797
2083.266590	14067.986019	47.811802
2078.328371	13303.982477	47.816807
2073.293897	12563.490850	47.821812
2068.470261	11847.483017	47.826817
2063.943582	11151.216374	47.831821
2059.224274	10466.427176	47.836826
2054.235675	9810.979720	47.841831
2050.140491	9171.381725	47.846836
2045.283254	8570.978329	47.851841
2040.680516	7974.305266	47.856845
2036.165854	7411.630792	47.861850
2031.516264	6876.653563	47.866855
2026.489623	6371.491621	47.871860
2021.568802	5901.646615	47.876865
2016.160254	5463.610398	47.881869
2011.481568	5040.604029	47.886874
2006.256121	4656.272947	47.891879
2001.559996	4284.202613	47.896884
1997.170806	3952.793688	47.901889
1992.951195	3637.699164	47.906893
1989.034853	3336.777134	47.911898
1984.502949	3063.318544	47.916903
1980.640027	2789.167691	47.921908
1977.123799	2535.733767	47.926913
1972.994253	2289.737188	47.931917
1969.612696	2065.355312	47.936922
1965.726397	1843.735239	47.941927
1962.506207	1626.560480	47.946932
1958.774498	1419.669325	47.951937
1955.380944	1225.826716	47.956941
1952.082073	1027.472193	47.961946
1948.427871	845.938129	47.966951
1944.770510	666.095944	47.971956
1941.121062	490.895772	47.976961
1937.182525	340.692836	47.981965
1933.007271	195.131606	47.986970
1926.827114	112.120915	47.991975
1918.303974	117.577102	47.996980
1912.077831	123.521763	48.001985
1907.654937	126.491828	48.006989
1904.590893	117.087486	48.011994
1902.186792	115.790019	48.016999
1900.087000	128.349975	48.022004
1897.757481	127.648293	48.027009
1894.755900	121.205016	48.032013
1892.016904	122.111363	48.037018
1888.570987	124.770362	48.042023
1885.084388	127.163638	48.047028
1882.056114	121.705331	48.052033
1878.643432	126.988277	48.057037
1875.382431	129.599360	48.062042
1871.927766	130.408892	48.067047
1868.492358	116.604836	48.072052
1865.186817	119.093174	48.077057
1861.974460	130.789501	48.082061
1858.402545	121.774704	48.087066
1854.977091	120.940805	48.092071
1851.762796	119.529685	48.097076
1848.185026	114.359867	48.102081
1844.805790	116.125735	48.107085
1842.148335	114.390191	48.112090
1838.787871	119.022717	48.117095
1834.663007	120.993858	48.122100
1831.413327	100.175033	48.127105
1827.596512	116.759147	48.132109
1824.771877	113.860171	48.137114
1821.079571	116.016732	48.142119
1817.844799	113.798887	48.147124
1814.461880	109.215538	48.152129
1811.184259	126.319576	48.157133
1808.210835	119.232830	48.162138
1804.044439	119.008457	48.167143
1800.854624	113.009135	48.172148
1797.280754	113.027405	48.177153
1793.296020	119.981809	48.182157
1790.040594	118.001328	48.187162
1787.023499	120.181952	48.192167
1783.372849	122.933135	48.197172
1780.204390	118.515554	48.202177
1776.401450	124.353158	48.207181
1773.403186	114.340608	48.212186
1769.542976	119.551246	48.217191
1766.087722	121.588469	48.222196
1762.766769	112.328794	48.227201
1759.005300	122.310853	48.232205
1755.646442	119.498665	48.237210
1752.357509	115.258140	48.242215
1748.915667	119.571225	48.247220
1745.594187	126.178233	48.252225
1741.764025	124.623079	48.257229
1738.330935	117.832927	48.262234
1734.643868	115.170189	48.267239
1731.247136	118.447975	48.272244
1728.371647	116.151785	48.277249
1724.582865	115.881003	48.282253
1721.349775	118.921206	48.287258
1717.415634	121.808528	48.292263
1713.975891	113.573560	48.297268
1710.802764	117.154887	48.302273
1707.117029	122.746374	48.307277
1703.911764	113.462289	48.312282
1700.331321	116.999794	48.317287
1696.764777	112.306016	48.322292
1693.140927	117.346807	48.327297
1689.736716	110.150352	48.332301
1686.270355	113.293512	48.337306
1682.912813	112.366784	48.342311
1679.706141	120.904756	48.347316
1675.990191	108.100176	48.352321
1671.963680	115.118104	48.357325
1668.803221	114.954655	48.362330
1665.757457	112.757901	48.367335
1661.824087	119.669507	48.372340
1658.375151	112.226957	48.377345
1655.244662	109.568893	48.382349
1651.741632	107.712634	48.387354
1648.039396	101.318996	48.392359
1644.302115	105.099368	48.397364
1640.700505	108.535798	48.402369
1637.312300	110.799853	48.407373
1634.134451	101.982921	48.412378
1630.615148	106.605560	48.417383
1627.185483	107.885831	48.422388
1623.698886	103.056183	48.427393
1620.337607	112.931349	48.432397
1616.815372	94.948949	48.437402
1612.954337	105.047866	48.442407
1609.500676	113.007562	48.447412
1606.326408	95.726860	48.452417
1602.420254	109.208639	48.457421
1599.135665	105.470539	48.462426
1595.659947	109.200498	48.467431
1591.985503	95.449816	48.472436
1588.760317	91.575874	48.477441
1585.209497	107.226205	48.482445
1581.802805	88.684732	48.487450
1578.486893	96.426714	48.492455
1574.647246	96.708127	48.497460
1571.277669	107.932388	48.502465
1567.815560	106.114049	48.507469
1564.386680	96.251246	48.512474
1560.625792	91.113372	48.517479
1557.260399	100.473489	48.522484
1554.207944	103.292472	48.527489
1550.340288	111.272688	48.532493
1546.759704	109.615271	48.537498
1543.225447	102.654371	48.542503
1539.505770	113.019096	48.547508
1536.270655	102.581796	48.552513
1532.671871	108.023680	48.557517
1529.364251	98.170386	48.562522
1525.868757	105.813940	48.567527
1522.456509	105.534921	48.572532
1519.334440	95.345699	48.577537
1515.350025	101.993247	48.582541
1511.779888	98.363151	48.587546
1508.145839	98.346648	48.592551
1504.894973	106.154403	48.597556
1501.649789	96.655188	48.602561
1497.943545	107.128552	48.607565
1494.336732	105.364527	48.612570
1490.424638	103.025014	48.617575
1487.349987	105.167270	48.622580
1484.151467	100.453940	48.627585
1480.109547	97.862666	48.632589
1476.857399	106.961466	48.637594
1473.366752	104.970454	48.642599
1469.905382	107.128953	48.647604
1466.375665	97.187060	48.652609
1462.816236	107.080622	48.657613
1459.928926	96.202932	48.662618
1455.907469	99.822198	48.667623
1452.063043	98.705999	48.672628
1449.014148	94.507112	48.677633
1445.245990	96.052401	48.682637
1441.731192	103.733802	48.687642
1438.081840	100.552739	48.692647
1435.076408	98.318110	48.697652
1431.910064	99.503443	48.702657
1427.951731	97.946329	48.707661
1424.880433	96.550933	48.712666
1420.770882	99.079831	48.717671
1416.822056	93.180481	48.722676
1413.953884	91.066746	48.727681
1410.099443	92.568605	48.732685
1407.108756	101.363896	48.737690
1403.793510	99.601724	48.742695
1399.490786	106.590209	48.747700
1396.436971	103.012216	48.752705
1392.743212	96.199736	48.757709
1389.430503	97.594658	48.762714
1385.857437	96.015221	48.767719
1382.428723	94.932055	48.772724
1378.962704	90.482105	48.777729
1375.307765	95.107070	48.782733
1371.973815	92.522081	48.787738
1368.438445	101.152702	48.792743
1364.711924	99.185998	48.797748
1361.409742	99.418161	48.802753
1358.400715	102.746103	48.807757
1355.040257	93.334598	48.812762
1351.537301	98.979838	48.817767
1347.215195	98.618674	48.822772
1343.731271	96.234346	48.827777
1340.412632	95.981865	48.832781
1336.953674	91.347325	48.837786
1333.426273	98.192318	48.842791
1329.488493	95.581642	48.847796
1326.136955	100.772909	48.852801
1322.466600	104.909915	48.857805
1319.446898	97.093428	48.862810
1316.443409	85.838510	48.867815
1312.512290	98.596592	48.872820
1308.762915	99.528375	48.877825
1305.341959	102.341838	48.882829
1301.791249	102.125699	48.887834
1298.526075	95.072160	48.892839
1294.587647	98.988542	48.897844
1291.177437	94.586838	48.902849
1287.886217	99.430146	48.907853
1284.570473	95.640090	48.912858
1280.952774	92.991985	48.917863
1277.564937	95.619934	48.922868
1274.048606	95.749606	48.927873
1270.142388	97.857583	48.932877
1267.227631	96.450387	48.937882
1263.514452	97.806799	48.942887
1259.948534	101.009972	48.947892
1256.374133	88.964910	48.952897
1252.629923	101.469121	48.957901
1249.229932	97.012048	48.962906
1246.026759	97.428070	48.967911
1242.457522	97.534398	48.972916
1239.224833	95.974498	48.977921
1235.612538	86.722697	48.982925
1232.200846	90.284554	48.987930
1228.197883	91.328833	48.992935
1224.843083	93.448582	48.997940
1221.370268	88.559989	49.002945
1217.661311	99.964012	49.007949
1214.383142	97.468425	49.012954
1210.705512	99.066069	49.017959
1207.170544	95.247086	49.022964
1203.806654	95.118796	49.027969
1200.254762	97.800928	49.032973
1196.863972	104.716327	49.037978
1193.513233	93.284859	49.042983
1189.673024	97.514940	49.047988
1186.729929	92.163773	49.052993
1182.838722	91.751043	49.057997
1179.322785	86.619278	49.063002
1175.896568	90.955396	49.068007
1172.385715	106.498319	49.073012
1169.412547	88.094832	49.078017
1165.765005	94.075980	49.083021
1161.738747	96.066748	49.088026
1158.324318	91.643610	49.093031
1154.585816	94.196782	49.098036
1151.371997	98.211749	49.103041
1147.990535	95.434961	49.108045
1144.406021	89.042095	49.113050
1140.913966	99.538971	49.118055
1136.881474	93.440872	49.123060
1133.790883	97.192940	49.128065
1130.249011	89.186190	49.133069
1126.871342	99.785387	49.138074
1123.556781	101.054133	49.143079
1119.950342	94.996908	49.148084
1116.627420	85.639744	49.153089
1113.003303	91.057248	49.158093
1109.318642	88.859463	49.163098
1105.747127	94.898332	49.168103
1102.388566	97.398366	49.173108
1099.107511	88.471259	49.178113
1095.336428	93.750424	49.183117
1091.554030	91.643879	49.188122
1088.157145	95.437586	49.193127
1084.781657	90.587595	49.198132
1081.582755	86.377521	49.203137
1077.524906	79.948062	49.208141
1074.301357	88.643838	49.213146
1070.674961	83.769861	49.218151
1067.320337	95.934709	49.223156
1064.424470	88.870902	49.228161
1060.351296	85.781661	49.233165
1057.054436	89.591354	49.238170
1053.630650	90.197006	49.243175
1049.942875	97.263349	49.248180
1046.385941	90.458076	49.253185
1042.780997	99.251545	49.258189
1039.174331	90.081209	49.263194
1035.597992	91.454246	49.268199
1032.099583	81.814544	49.273204
1028.950642	92.634218	49.278209
1025.201780	95.293464	49.283213
1021.370468	89.423354	49.288218
1018.029295	91.832106	49.293223
1014.604726	93.181388	49.298228
1011.676601	80.661933	49.303233
1008.089032	83.080792	49.308237
1004.409661	81.467525	49.313242
1001.012333	86.938142	49.318247
997.143393	88.777792	49.323252
993.496098	87.146852	49.328257
989.949363	91.226648	49.333261
986.652211	89.316257	49.338266
983.464754	86.009275	49.343271
980.033991	91.883774	49.348276
976.449207	85.557464	49.353281
972.676705	91.384231	49.358285
969.380046	97.668014	49.363290
965.950778	82.949106	49.368295
962.543223	97.257832	49.373300
958.751323	89.875610	49.378305
954.960980	87.703927	49.383309
951.591069	86.080192	49.388314
948.336590	84.470023	49.393319
944.399783	86.741105	49.398324
940.890153	82.064039	49.403329
937.662352	98.910468	49.408333
934.346698	94.826297	49.413338
930.654779	90.883303	49.418343
927.245953	88.699350	49.423348
923.957675	74.980300	49.428353
920.202405	83.186723	49.433357
916.449382	88.333406	49.438362
913.095062	83.081532	49.443367
909.450652	85.629551	49.448372
906.278914	84.338640	49.453377
902.593849	93.549660	49.458381
899.203067	85.073261	49.463386
895.757055	78.706277	49.468391
892.536920	93.295722	49.473396
888.712004	87.889750	49.478401
884.826667	90.279348	49.483405
881.446032	96.974945	49.488410
878.158074	84.125904	49.493415
874.840039	98.401652	49.498420
871.508024	89.963517	49.503425
867.850928	96.161399	49.508429
864.037516	88.491520	49.513434
860.476876	84.515346	49.518439
856.884322	93.715058	49.523444
853.685032	86.369807	49.528449
850.104626	84.427890	49.533453
847.057955	86.189462	49.538458
843.446705	84.211248	49.543463
839.811141	90.541808	49.548468
836.603173	85.181624	49.553473
832.319351	91.841491	49.558477
828.918511	78.336264	49.563482
825.842459	75.397881	49.568487
822.057676	92.106915	49.573492
818.646036	89.796892	49.578497
815.007766	92.979908	49.583501
811.224580	84.533357	49.588506
807.841234	87.097481	49.593511
804.573012	87.976259	49.598516
801.796883	79.210663	49.603521
797.960179	84.088914	49.608525
793.925529	77.608503	49.613530
790.775184	82.806388	49.618535
786.999615	82.204869	49.623540
783.747577	85.169223	49.628545
779.844683	85.470344	49.633549
776.746533	82.219058	49.638554
773.385857	86.427980	49.643559
769.126486	97.880359	49.648564
765.992452	79.198540	49.653569
762.507348	86.378770	49.658573
759.108951	89.305941	49.663578
755.650022	86.313641	49.668583
752.037266	97.547707	49.673588
748.689979	82.050430	49.678593
745.250977	78.061584	49.683597
741.540406	84.669680	49.688602
738.269592	80.227387	49.693607
734.527873	83.160872	49.698612
730.988587	83.047564	49.703617
727.312333	81.332680	49.708621
723.589463	81.387331	49.713626
720.412273	81.226813	49.718631
716.874264	73.903029	49.723636
714.265863	75.940861	49.728641
710.405657	79.816737	49.733645
706.877742	87.494077	49.738650
703.082207	74.547441	49.743655
699.249238	85.872949	49.748660
695.954045	81.276300	49.753665
692.907333	78.387153	49.758669
688.896860	81.362744	49.763674
685.129435	79.744415	49.768679
681.965393	79.458463	49.773684
678.770279	76.279347	49.778689
675.231792	76.561409	49.783693
671.591619	78.488748	49.788698
667.962364	78.060520	49.793703
663.997062	76.182120	49.798708
661.081023	75.822535	49.803713
657.418303	81.663856	49.808717
653.609679	77.236219	49.813722
650.250146	73.231804	49.818727
647.199100	86.007276	49.823732
643.809130	86.996926	49.828737
640.143013	82.217941	49.833741
636.461683	80.060960	49.838746
633.187969	73.932864	49.843751
629.237892	73.950369	49.848756
626.082160	73.232861	49.853761
622.495463	77.477229	49.858765
618.602851	74.957871	49.863770
615.685113	68.805672	49.868775
611.977829	87.236375	49.873780
608.388393	76.193749	49.878785
605.020719	80.555683	49.883789
601.590845	77.277320	49.888794
598.138695	81.064022	49.893799
594.324797	82.167540	49.898804
591.106166	72.348186	49.903809
587.285851	79.036797	49.908813
583.657987	88.166190	49.913818
580.131057	87.867504	49.918823
576.464143	92.209877	49.923828
573.240797	82.736116	49.928833
569.797549	89.479578	49.933837
566.536081	80.625566	49.938842
563.376323	78.152808	49.943847
559.156579	82.550131	49.948852
556.083722	77.953519	49.953857
552.122674	87.321768	49.958861
548.627678	87.014930	49.963866
545.486897	69.935166	49.968871
542.018021	84.867363	49.973876
538.599941	76.521955	49.978881
534.996325	79.120671	49.983885
531.718025	78.235729	49.988890
528.169122	73.479568	49.993895
524.074854	76.965065	49.998900
521.029649	81.314487	50.003905
517.298473	78.912260	50.008909
513.614120	72.791582	50.013914
510.271624	77.722249	50.018919
506.320451	86.582762	50.023924
503.109601	78.261859	50.028929
499.919115	81.510898	50.033933
496.256551	85.514092	50.038938
493.264672	76.209762	50.043943
489.511583	83.685155	50.048948
486.326910	75.534169	50.053953
482.732510	86.101038	50.058957
478.751328	83.070426	50.063962
475.298029	81.871226	50.068967
471.784404	80.542269	50.073972
468.590151	72.800921	50.078977
464.713168	79.479470	50.083981
461.289718	84.356394	50.088986
457.695744	77.380017	50.093991
453.985536	88.920498	50.098996
450.913048	71.637093	50.104001
447.175673	75.715297	50.109005
443.900414	84.998314	50.114010
440.494478	79.406703	50.119015
436.870577	81.948522	50.124020
433.165490	67.719190	50.129025
430.067075	74.174559	50.134029
426.322421	77.073820	50.139034
422.608267	70.214364	50.144039
419.018267	79.470754	50.149044
415.883723	74.260593	50.154049
412.193011	77.376040	50.159053
408.833411	76.608283	50.164058
405.308258	67.877910	50.169063
401.531998	83.203141	50.174068
398.058011	70.291726	50.179073
394.822939	79.410271	50.184077
391.264452	72.168938	50.189082
387.616372	76.381876	50.194087
384.108810	70.584746	50.199092
380.679892	75.696672	50.204097
377.280640	75.469818	50.209101
373.554078	78.337792	50.214106
370.463437	73.924373	50.219111
366.671130	79.118537	50.224116
363.164561	70.157480	50.229121
359.787027	76.900203	50.234125
356.092560	75.479397	50.239130
352.911898	77.179856	50.244135
349.242436	70.006547	50.249140
346.022104	70.147151	50.254145
342.119783	75.061160	50.259149
338.596472	73.430053	50.264154
335.136679	69.356050	50.269159
331.266248	85.388923	50.274164
328.019595	74.390819	50.279169
324.806516	72.957896	50.284173
321.446810	75.629218	50.289178
317.627567	74.588645	50.294183
314.160345	79.896422	50.299188
310.989716	71.053610	50.304193
307.186030	81.365410	50.309197
303.390829	81.934605	50.314202
300.009608	67.869749	50.319207
296.306860	79.273063	50.324212
293.241371	73.352938	50.329217
289.787269	79.250295	50.334221
286.041345	75.702029	50.339226
282.883582	72.295749	50.344231
278.961411	73.099982	50.349236
275.535124	66.138555	50.354241
272.103957	73.775565	50.359245
268.702646	75.453669	50.364250
265.571591	76.472502	50.369255
261.485301	75.644632	50.374260
258.097174	69.775065	50.379265
254.709552	69.448359	50.384269
251.140345	69.254505	50.389274
247.657862	63.912257	50.394279
244.252519	76.012484	50.399284
240.660919	70.152652	50.404289
237.216892	69.996142	50.409293
233.365647	71.282833	50.414298
230.389754	68.325814	50.419303
226.839854	75.022814	50.424308
223.143553	73.317614	50.429313
219.116679	70.832128	50.434317
215.548173	71.188676	50.439322
212.553393	72.239963	50.444327
208.570815	84.541365	50.449332
205.663148	77.568322	50.454337
202.384298	73.193944	50.459341
198.891112	77.930021	50.464346
195.335422	73.557887	50.469351
191.381525	75.525070	50.474356
188.093762	73.164257	50.479361
184.409889	72.741619	50.484365
181.044390	76.847090	50.489370
177.731889	66.204229	50.494375
173.815791	73.271830	50.499380
170.617058	73.342675	50.504385
166.896623	76.168642	50.509389
163.208548	74.879797	50.514394
159.791422	68.916740	50.519399
156.710017	73.850913	50.524404
153.271158	66.774451	50.529409
149.700296	70.627365	50.534413
145.926392	82.149445	50.539418
142.497154	66.292004	50.544423
138.858930	73.423654	50.549428
135.600654	69.615561	50.554433
131.755934	73.258285	50.559437
128.617930	68.380980	50.564442
124.903278	71.762882	50.569447
121.484351	74.187288	50.574452
118.026506	69.040555	50.579457
114.326724	74.384835	50.584461
111.028437	71.475204	50.589466
107.757281	67.359092	50.594471
103.665353	73.327965	50.599476
100.638377	70.435944	50.604481
97.021157	72.502282	50.609485
93.114804	68.495184	50.614490
90.018942	67.822273	50.619495
86.405134	70.751790	50.624500
82.926140	71.442383	50.629505
79.419707	72.915564	50.634509
76.066613	73.874338	50.639514
72.908658	63.995094	50.644519
68.936791	69.413657	50.649524
65.581246	61.495276	50.654529
61.611045	57.026797	50.659533
58.100480	59.184008	50.664538
55.002880	63.541777	50.669543
51.493396	69.349813	50.674548
48.131574	63.023801	50.679553
44.460797	67.683351	50.684557
40.722239	66.411961	50.689562
37.131222	67.607344	50.694567
33.904106	70.058678	50.699572
30.739215	61.724462	50.704577
26.826902	62.903750	50.709581
23.195305	68.218397	50.714586
19.675945	61.515282	50.719591
16.043119	63.989059	50.724596
13.199712	61.568187	50.729601
9.190260	64.069339	50.734605
5.749897	70.201921	50.739610
2.600915	62.257533	50.744615