Thu Aug 25 12:26:43 2022

Number of Points = 9926

Depth (nm)	Load (N)	Time (s)
1.566640	114.611786	0.000000
1.336296	96.570057	0.005005
1.054587	86.993146	0.010010
1.238567	88.046302	0.015014
0.907469	79.340842	0.020019
1.143083	87.887203	0.025024
1.011900	87.689431	0.030029
0.982083	70.505328	0.035034
0.527427	70.256998	0.040038
0.258084	56.087542	0.045043
-0.134090	50.207416	0.050048
-0.177646	47.648403	0.055053
-0.288797	35.668812	0.060058
-0.926761	41.909602	0.065062
-0.767741	32.678118	0.070067
-1.546631	22.343909	0.075072
-1.929358	20.929539	0.080077
-1.993102	26.181846	0.085082
-2.809363	27.616346	0.090086
-3.323644	23.878243	0.095091
-3.546430	30.579162	0.100096
-3.536293	24.110826	0.105101
-3.539022	22.592623	0.110106
-3.293520	21.848613	0.115110
-3.425451	24.653365	0.120115
-4.285900	26.638954	0.125120
-4.793858	28.901510	0.130125
-4.860839	19.635841	0.135130
-4.987003	29.975760	0.140134
-5.139494	27.629972	0.145139
-5.544025	24.633974	0.150144
-6.087715	24.029436	0.155149
-6.388512	28.869633	0.160154
-6.519238	36.125606	0.165158
-6.258178	19.253483	0.170163
-6.686513	28.308804	0.175168
-6.795565	22.207157	0.180173
-7.604448	29.920560	0.185178
-7.878067	39.109834	0.190182
-7.767502	28.231299	0.195187
-7.977535	21.433628	0.200192
-7.787064	34.337202	0.205197
-8.434458	30.139063	0.210202
-8.950757	29.824462	0.215206
-9.059996	27.528845	0.220211
-9.547037	24.615379	0.225216
-9.002792	32.417327	0.230221
-9.356259	31.210344	0.235226
-10.473237	17.597674	0.240230
-10.524081	21.908324	0.245235
-10.852180	21.599037	0.250240
-10.907314	26.131822	0.255245
-10.813518	20.083815	0.260250
-11.165453	19.888994	0.265254
-11.654207	18.912016	0.270259
-11.887728	21.824434	0.275264
-12.050583	22.865491	0.280269
-12.276235	23.106464	0.285274
-12.468852	36.114355	0.290278
-12.987186	22.325627	0.295283
-13.463071	18.543545	0.300288
-13.568346	31.031545	0.305293
-13.562901	16.379306	0.310298
-13.633856	20.851294	0.315302
-13.568545	17.142603	0.320307
-14.425130	17.703897	0.325312
-14.866158	26.261332	0.330317
-15.388128	20.613526	0.335322
-15.347395	23.859460	0.340326
-15.310629	29.681315	0.345331
-15.067055	15.839653	0.350336
-15.220878	20.457502	0.355341
-15.842044	23.835618	0.360346
-16.733920	27.733879	0.365350
-16.618145	19.708243	0.370355
-16.792990	23.313821	0.375360
-16.956644	24.889678	0.380365
-17.707312	18.439311	0.385370
-17.982788	31.156459	0.390374
-18.212361	25.545095	0.395379
-18.222178	25.777561	0.400384
-18.426106	31.001214	0.405389
-17.983287	23.531776	0.410394
-18.347661	32.817523	0.415398
-19.017361	14.607439	0.420403
-19.540708	25.661320	0.425408
-19.692655	29.962502	0.430413
-19.493749	23.401315	0.435418
-19.991896	27.544769	0.440422
-20.654458	26.987330	0.445427
-21.023025	29.674136	0.450432
-21.158764	17.198538	0.455437
-21.020528	22.510945	0.460442
-21.297479	30.476362	0.465446
-21.023966	25.504345	0.470451
-21.817767	26.520875	0.475456
-22.478388	26.165613	0.480461
-22.166163	26.667160	0.485466
-22.555603	26.978090	0.490470
-22.490792	21.051683	0.495475
-23.066275	13.438081	0.500480
-23.282382	20.321447	0.505485
-23.229688	10.780769	0.510490
-23.845677	23.133649	0.515494
-23.974713	20.818988	0.520499
-24.534368	23.545224	0.525504
-25.161587	20.451243	0.530509
-24.785385	23.015026	0.535514
-24.974214	20.545219	0.540518
-25.172435	18.437552	0.545523
-24.933647	19.713070	0.550528
-26.252436	20.046228	0.555533
-26.433442	17.784004	0.560538
-26.958223	21.251422	0.565542
-27.063314	23.960219	0.570547
-26.818385	30.727058	0.575552
-26.933102	21.842194	0.580557
-26.888910	14.308668	0.585562
-27.576735	28.552078	0.590566
-27.875069	36.460735	0.595571
-27.980824	30.431337	0.600576
-28.390186	21.557838	0.605581
-28.378737	15.247488	0.610586
-29.210981	27.020486	0.615590
-29.511308	20.926665	0.620595
-29.638466	22.791032	0.625600
-29.826011	19.903408	0.630605
-29.849987	14.399040	0.635610
-29.781430	20.465847	0.640614
-30.170948	19.036723	0.645619
-30.291840	21.434784	0.650624
-30.922775	21.100181	0.655629
-31.035665	22.702885	0.660634
-31.383770	24.991015	0.665638
-31.610758	17.667657	0.670643
-32.351302	22.143319	0.675648
-32.549815	21.279054	0.680653
-32.833623	19.213271	0.685658
-32.921757	28.284890	0.690662
-32.894677	18.985504	0.695667
-32.957257	20.646763	0.700672
-32.863436	26.734923	0.705677
-33.321299	20.207041	0.710682
-34.290418	27.100828	0.715686
-34.108049	19.099561	0.720691
-34.280585	27.330189	0.725696
-34.427157	27.758090	0.730701
-34.293862	28.366766	0.735706
-35.282889	30.318721	0.740710
-35.817768	24.470458	0.745715
-36.136688	20.239840	0.750720
-36.004094	27.391274	0.755725
-35.674694	24.770665	0.760730
-35.973273	25.696946	0.765734
-36.530623	15.742487	0.770739
-37.257738	25.527992	0.775744
-37.667369	34.795521	0.780749
-37.510637	28.582626	0.785754
-37.750676	33.239297	0.790758
-37.630358	24.456811	0.795763
-37.835832	24.030235	0.800768
-38.647466	28.507547	0.805773
-38.495567	26.604448	0.810778
-38.738393	30.625640	0.815782
-38.463647	20.784410	0.820787
-39.634840	14.627728	0.825792
-40.060429	21.980515	0.830797
-39.827994	13.863838	0.835802
-39.970200	27.629449	0.840806
-40.261285	17.221981	0.845811
-40.342649	20.256090	0.850816
-41.245507	20.214032	0.855821
-41.345096	13.649000	0.860826
-41.751062	23.529716	0.865830
-41.984261	17.517128	0.870835
-41.650019	11.618112	0.875840
-41.647565	11.301325	0.880845
-42.323035	22.144922	0.885850
-43.335157	25.391308	0.890854
-42.999373	18.330949	0.895859
-43.483520	14.942471	0.900864
-43.015830	9.664788	0.905869
-42.937519	16.350159	0.910874
-44.140226	21.657538	0.915878
-44.322231	23.998736	0.920883
-44.841229	20.280359	0.925888
-44.777131	21.118176	0.930893
-44.700332	21.615481	0.935898
-45.033187	23.651284	0.940902
-44.914759	19.282537	0.945907
-45.507259	14.354469	0.950912
-46.366856	20.582523	0.955917
-46.036616	18.815997	0.960922
-45.936516	18.116915	0.965926
-46.632590	10.012848	0.970931
-47.355932	28.178549	0.975936
-47.733023	16.101441	0.980941
-47.343574	20.997997	0.985946
-47.803176	18.232096	0.990950
-47.600715	16.713382	0.995955
-47.520078	16.384345	1.000960
-48.282817	20.180115	1.005965
-48.717841	14.313047	1.010970
-48.818538	19.393970	1.015974
-49.207891	20.283855	1.020979
-49.858483	18.478024	1.025984
-49.737443	16.589253	1.030989
-50.138636	9.891146	1.035994
-50.660090	23.966114	1.040998
-50.543340	21.875534	1.046003
-51.014723	18.912162	1.051008
-51.103689	21.096412	1.056013
-50.927893	23.637811	1.061018
-50.972199	18.962368	1.066022
-51.491935	14.826493	1.071027
-51.889341	15.768259	1.076032
-51.996538	33.210999	1.081037
-52.260059	21.900704	1.086042
-53.059167	24.367068	1.091046
-53.331901	18.847894	1.096051
-53.749361	20.925427	1.101056
-53.926775	18.384230	1.106061
-54.018683	8.679552	1.111066
-53.660286	25.748774	1.116070
-53.690536	14.379787	1.121075
-53.807098	15.214273	1.126080
-54.111268	20.526396	1.131085
-54.503687	19.857029	1.136090
-55.115093	29.026456	1.141094
-55.908942	23.354815	1.146099
-55.891123	18.008414	1.151104
-56.488234	21.727612	1.156109
-56.485953	19.828975	1.161114
-57.135023	20.383068	1.166118
-57.162395	18.463767	1.171123
-56.916658	22.468516	1.176128
-57.084387	23.908970	1.181133
-56.833341	19.222051	1.186138
-57.284616	26.404857	1.191142
-57.679204	21.948815	1.196147
-58.117582	24.760454	1.201152
-58.393258	31.137464	1.206157
-58.432735	25.588067	1.211162
-58.967367	29.654981	1.216166
-59.420752	29.931639	1.221171
-59.737386	23.565128	1.226176
-59.899293	22.574905	1.231181
-60.310556	23.423931	1.236186
-60.029730	29.631485	1.241190
-60.236329	25.933762	1.246195
-60.585432	24.539436	1.251200
-61.150118	25.118272	1.256205
-61.110251	20.223996	1.261210
-61.413536	29.784906	1.266214
-61.333412	26.187789	1.271219
-62.040700	28.630276	1.276224
-62.718621	26.743306	1.281229
-62.892671	23.701708	1.286234
-63.023769	34.346119	1.291238
-63.177311	26.482905	1.296243
-62.679997	20.115408	1.301248
-62.929351	23.976270	1.306253
-62.914517	14.963545	1.311258
-63.852329	31.286747	1.316262
-64.115335	27.332106	1.321267
-64.509844	25.315308	1.326272
-65.234984	33.717946	1.331277
-65.528779	26.237377	1.336282
-65.377633	35.647991	1.341286
-65.322805	20.747572	1.346291
-66.036674	23.317640	1.351296
-66.174453	26.980685	1.356301
-65.733042	30.034122	1.361306
-65.914022	29.293661	1.366310
-66.710729	27.286098	1.371315
-67.176758	26.330873	1.376320
-67.418703	22.452028	1.381325
-67.218771	19.952945	1.386330
-67.260619	32.212704	1.391334
-68.339444	19.214166	1.396339
-68.311509	21.475011	1.401344
-68.561773	29.955100	1.406349
-68.512747	17.447393	1.411354
-68.926782	23.020340	1.416358
-68.858069	13.540429	1.421363
-69.620421	16.089619	1.426368
-70.309976	24.888474	1.431373
-70.323924	10.046297	1.436378
-70.617791	20.716204	1.441382
-70.548474	14.311368	1.446387
-70.648273	20.404552	1.451392
-70.909431	22.837246	1.456397
-70.470913	12.593873	1.461402
-70.944520	24.029100	1.466406
-71.481465	19.301136	1.471411
-71.948337	22.196333	1.476416
-72.401862	29.882531	1.481421
-72.441564	20.505026	1.486426
-73.133731	29.835804	1.491430
-72.957359	28.188299	1.496435
-72.843384	20.697623	1.501440
-73.648550	18.533200	1.506445
-73.953484	11.513127	1.511450
-74.738925	27.515058	1.516454
-74.674214	23.252804	1.521459
-74.767428	20.461133	1.526464
-74.960543	27.948338	1.531469
-74.755673	18.769794	1.536474
-74.854603	31.266285	1.541478
-74.915564	32.712156	1.546483
-75.547808	14.730334	1.551488
-75.722691	19.588764	1.556493
-75.922603	18.398853	1.561498
-76.229064	21.294225	1.566502
-77.017871	16.207094	1.571507
-77.284294	18.694396	1.576512
-77.800162	31.379604	1.581517
-77.675897	23.219763	1.586522
-77.813937	24.424611	1.591526
-77.654867	17.752610	1.596531
-78.030850	17.931720	1.601536
-78.573735	23.622933	1.606541
-78.888895	16.085606	1.611546
-79.168716	20.960478	1.616550
-79.403522	27.891067	1.621555
-79.048700	20.321524	1.626560
-79.476455	26.823602	1.631565
-80.060698	21.014718	1.636570
-80.660213	28.192279	1.641574
-80.290273	32.996980	1.646579
-80.871472	23.460713	1.651584
-81.142793	25.689355	1.656589
-80.982286	12.069526	1.661594
-81.705880	13.220592	1.666598
-82.622610	21.612117	1.671603
-82.208303	36.609816	1.676608
-82.297531	17.717165	1.681613
-81.940259	25.580036	1.686618
-82.250088	24.094136	1.691622
-82.552637	18.971941	1.696627
-82.975202	24.106463	1.701632
-83.365421	23.009646	1.706637
-83.465489	14.663497	1.711642
-84.443914	14.335892	1.716646
-84.947958	19.900795	1.721651
-84.708706	19.885426	1.726656
-85.160796	22.832092	1.731661
-84.411652	11.859840	1.736666
-84.974564	32.158084	1.741670
-85.273646	25.035851	1.746675
-85.996006	22.893255	1.751680
-86.760995	26.784293	1.756685
-86.135176	26.034472	1.761690
-86.799884	24.661127	1.766694
-86.642087	22.447056	1.771699
-86.693459	30.848523	1.776704
-87.113800	28.769335	1.781709
-87.568677	24.025348	1.786714
-88.232648	29.324248	1.791718
-88.422233	32.131706	1.796723
-88.716074	30.599008	1.801728
-88.629138	21.919833	1.806733
-88.218279	23.658769	1.811738
-88.399753	29.302844	1.816742
-89.075668	15.238271	1.821747
-89.767286	17.811180	1.826752
-90.014109	26.958280	1.831757
-89.971239	17.972800	1.836762
-89.998359	24.981576	1.841766
-90.841768	22.573210	1.846771
-91.169175	19.868856	1.851776
-91.474993	30.521657	1.856781
-91.349502	17.752034	1.861786
-91.342366	20.917808	1.866790
-91.288761	18.514420	1.871795
-91.431800	20.741944	1.876800
-92.374382	29.751292	1.881805
-92.294773	14.954565	1.886810
-92.639192	27.008628	1.891814
-93.075395	26.485330	1.896819
-93.613375	24.165147	1.901824
-93.958139	26.421117	1.906829
-93.787255	25.859639	1.911834
-93.921780	30.120125	1.916838
-94.227586	21.698643	1.921843
-93.944369	27.092734	1.926848
-94.809468	30.195866	1.931853
-94.885304	19.650271	1.936858
-95.494833	24.893183	1.941862
-95.240890	24.375639	1.946867
-95.501766	25.884472	1.951872
-96.089958	28.928396	1.956877
-96.258644	17.362804	1.961882
-96.944005	25.243514	1.966886
-96.937850	27.159759	1.971891
-97.062771	26.992646	1.976896
-97.211884	8.615592	1.981901
-97.693690	12.598296	1.986906
-98.190460	20.601313	1.991910
-98.813044	26.921948	1.996915
-98.269618	28.609986	2.006912
-97.654366	24.246493	2.016909
-97.365000	19.658466	2.026906
-97.327571	20.029517	2.036902
-96.792219	14.240363	2.046899
-96.063196	21.190282	2.056896
-95.732497	19.060331	2.066893
-94.512881	12.444866	2.076890
-94.773477	19.467488	2.086886
-94.544181	17.961645	2.096883
-93.433073	21.474815	2.106880
-93.203973	21.438865	2.116877
-92.258975	23.137568	2.126874
-92.004991	22.220236	2.136870
-92.132390	26.564202	2.146867
-91.633127	25.228299	2.156864
-90.026468	19.030524	2.166861
-89.974897	23.926154	2.176858
-89.758978	22.172150	2.186854
-89.346097	23.155946	2.196851
-88.485447	23.774974	2.206848
-87.933571	22.510023	2.216845
-87.598919	20.864127	2.226842
-86.345439	20.167151	2.236838
-86.656095	22.439576	2.246835
-86.342964	23.958522	2.256832
-85.595811	23.245849	2.266829
-85.041859	18.274241	2.276826
-84.678899	22.202415	2.286822
-83.848174	22.677245	2.296819
-83.350701	21.104039	2.306816
-83.612804	15.243435	2.316813
-82.803112	18.125925	2.326810
-81.635146	24.275306	2.336806
-81.243395	26.383817	2.346803
-80.977843	22.730855	2.356800
-80.855666	25.793935	2.366797
-80.289057	24.482326	2.376794
-79.434110	28.225706	2.386790
-79.066427	21.873610	2.396787
-78.198699	27.512503	2.406784
-78.043516	25.248495	2.416781
-77.872940	26.723256	2.426778
-76.825913	25.646815	2.436774
-76.561262	25.095278	2.446771
-76.009508	29.931543	2.456768
-75.006228	24.810332	2.466765
-74.877592	24.397315	2.476762
-74.859050	27.172524	2.486758
-74.096438	20.505122	2.496755
-73.758246	21.047625	2.506752
-72.871207	24.567398	2.516749
-72.440206	18.116683	2.526746
-72.514389	23.003508	2.536742
-71.440859	21.945090	2.546739
-70.974918	19.173058	2.556736
-70.595817	20.893911	2.566733
-69.984812	26.275258	2.576730
-69.584995	25.594836	2.586726
-69.037927	21.403586	2.596723
-68.229644	22.509160	2.606720
-67.922576	18.846527	2.616717
-67.844219	23.791813	2.626714
-67.140503	26.681409	2.636710
-66.411811	24.441579	2.646707
-65.450376	19.694393	2.656704
-65.187767	18.753536	2.666701
-65.337079	12.634504	2.676698
-64.852716	17.221566	2.686694
-63.957609	27.417813	2.696691
-63.648583	29.073620	2.706688
-62.521708	20.926796	2.716685
-62.078549	25.162354	2.726682
-62.115895	23.701459	2.736678
-61.768582	24.701866	2.746675
-60.972020	26.794466	2.756672
-60.816375	29.424648	2.766669
-59.846622	24.825045	2.776666
-59.373577	21.839657	2.786662
-59.313964	24.177609	2.796659
-58.304773	24.352047	2.806656
-57.878827	26.360167	2.816653
-57.525361	24.505416	2.826650
-56.768994	20.601321	2.836646
-56.545088	24.392895	2.846643
-56.213233	22.661907	2.856640
-55.200991	19.766263	2.866637
-55.131861	23.233631	2.876634
-54.533863	18.055550	2.886630
-53.833646	22.893895	2.896627
-53.691082	19.101815	2.906624
-52.690215	19.039972	2.916621
-51.890808	22.595654	2.926618
-52.117610	19.602715	2.936614
-51.956379	22.228854	2.946611
-51.021596	17.530195	2.956608
-50.494211	23.643737	2.966605
-49.405066	25.272343	2.976602
-49.215834	18.438192	2.986598
-49.279217	25.512280	2.996595
-48.902810	19.412241	3.006592
-48.068487	15.359717	3.016589
-47.602748	11.174878	3.026586
-46.567052	14.649185	3.036582
-46.349882	19.069040	3.046579
-46.270313	17.105152	3.056576
-44.956623	20.060731	3.066573
-44.648754	18.301824	3.076570
-44.629795	15.530139	3.086566
-44.267667	15.916838	3.096563
-43.582473	20.637162	3.106560
-42.893845	18.067824	3.116557
-42.037091	18.747656	3.126554
-41.767622	11.657013	3.136550
-41.660246	16.920869	3.146547
-41.231815	19.825089	3.156544
-40.496643	18.978082	3.166541
-39.577281	16.496136	3.176538
-39.096758	9.163350	3.186534
-39.079832	13.674768	3.196531
-38.970875	19.641629	3.206528
-37.875427	15.016000	3.216525
-37.502832	19.158078	3.226522
-36.454091	21.531115	3.236518
-36.527401	17.566952	3.246515
-36.236623	15.915261	3.256512
-35.241402	19.177334	3.266509
-34.391407	18.860367	3.276506
-34.641008	20.245741	3.286502
-34.096088	14.543787	3.296499
-33.332010	15.133602	3.306496
-33.121782	14.378350	3.316493
-32.420237	13.717178	3.326490
-31.760091	13.284238	3.336486
-31.535844	10.876363	3.346483
-30.749153	15.162633	3.356480
-30.170334	20.396971	3.366477
-30.216550	19.292260	3.376474
-28.764515	17.952794	3.386470
-28.981054	13.253968	3.396467
-28.814907	12.949116	3.406464
-27.667852	12.249816	3.416461
-27.042856	6.224873	3.426458
-27.172914	13.227041	3.436454
-26.870076	11.934591	3.446451
-26.189999	16.291419	3.456448
-24.999353	15.309691	3.466445
-24.562987	10.784164	3.476442
-24.371147	14.438211	3.486438
-24.106954	11.514061	3.496435
-23.504167	16.469043	3.506432
-23.074273	20.389902	3.516429
-22.004853	9.017757	3.526426
-21.430569	13.080717	3.536422
-21.408929	15.462632	3.546419
-21.366920	17.429541	3.556416
-20.288600	12.727401	3.566413
-19.918130	15.181372	3.576410
-19.464821	13.900191	3.586406
-18.774419	12.889139	3.596403
-18.320876	15.434632	3.606400
-17.923447	14.599364	3.616397
-16.939513	18.103961	3.626394
-16.514762	17.970833	3.636390
-16.892455	12.524312	3.646387
-16.226170	19.439723	3.656384
-15.384607	15.563463	3.666381
-14.922389	25.013418	3.676378
-13.758708	13.322392	3.686374
-13.568628	18.158308	3.696371
-13.697848	14.459497	3.706368
-13.128172	11.056660	3.716365
-12.188834	15.860710	3.726362
-12.010175	10.938404	3.736358
-11.098868	17.546161	3.746355
-11.114794	22.560075	3.756352
-10.506965	16.655027	3.766349
-9.543081	13.361486	3.776346
-9.290279	15.456926	3.786342
-9.053104	20.279128	3.796339
-7.925700	21.366386	3.806336
-7.730706	23.036894	3.816333
-7.791938	16.989588	3.826330
-7.074413	22.518977	3.836326
-6.454297	24.027842	3.846323
-5.599392	27.229543	3.856320
-5.327183	24.842662	3.866317
-4.950838	14.963439	3.876314
-4.380844	27.922279	3.886310
-3.884981	29.555151	3.896307
-3.423905	31.047754	3.906304
-2.987618	54.022006	3.916301
-2.690224	49.321839	3.926298
-2.336178	57.879599	3.936294
-1.920652	71.540587	3.946291
-1.332235	83.495552	3.956288
-0.892089	97.688063	3.966285
-0.520338	120.609157	3.976282
0.000000	124.587148	3.981286
0.039681	135.942025	3.986291
0.355367	147.377053	3.991296
0.414467	153.957920	3.996301
0.825338	170.623598	4.001306
0.956003	167.543720	4.006310
1.161638	162.993593	4.011315
1.003066	170.655784	4.016320
0.955388	158.558596	4.021325
0.924395	172.648587	4.026330
0.844685	171.484122	4.031334
0.774841	169.653717	4.036339
0.901270	177.831246	4.041344
1.190597	166.361464	4.046349
1.129217	173.527534	4.051354
0.766712	165.719140	4.056358
1.267290	169.652359	4.061363
1.046397	165.700576	4.066368
1.124773	168.864708	4.071373
1.151175	168.642244	4.076378
1.167523	177.817794	4.081382
0.987144	166.108392	4.086387
0.899877	171.487815	4.091392
1.039088	165.885063	4.096397
1.065863	171.129558	4.101402
1.236304	167.125951	4.106406
0.852619	175.968705	4.111411
1.039173	174.231006	4.116416
1.129179	164.418640	4.121421
0.735958	174.553711	4.126426
1.035726	186.763221	4.131430
1.488459	192.763567	4.136435
1.378577	198.810938	4.141440
1.421690	196.231996	4.146445
1.216464	191.366582	4.151450
1.404966	196.016263	4.156454
1.254618	183.375154	4.161459
1.346691	188.710665	4.166464
1.173228	194.233315	4.171469
1.286001	201.871988	4.176474
1.054385	201.370407	4.181478
1.685730	195.930986	4.186483
1.447447	198.050067	4.191488
1.522509	193.273615	4.196493
1.397312	190.531218	4.201498
1.436341	202.547472	4.206502
1.655361	189.437193	4.211507
1.376863	194.432130	4.216512
1.715648	191.167778	4.221517
1.251124	188.798091	4.226522
1.301384	192.491821	4.231526
1.400123	191.565153	4.236531
1.602945	206.352534	4.241536
1.850909	208.196112	4.246541
1.873702	204.481389	4.251546
1.419599	185.338828	4.256550
1.110147	188.184074	4.261555
1.463724	200.967300	4.266560
1.598728	197.567195	4.271565
1.720795	198.617404	4.276570
2.067985	197.610679	4.281574
1.750789	189.162418	4.286579
1.068687	196.470045	4.291584
1.455658	197.095929	4.296589
1.666934	196.689473	4.301594
1.594079	206.236522	4.306598
1.867286	195.300764	4.311603
1.555080	195.083897	4.316608
1.955658	184.995066	4.321613
1.976541	201.810463	4.326618
1.553420	197.615109	4.331622
1.880968	197.541615	4.336627
1.774687	195.315115	4.341632
1.604470	187.062128	4.346637
1.674874	200.171298	4.351642
1.669966	200.440963	4.356646
1.602135	197.370034	4.361651
1.752363	202.940049	4.366656
2.162492	196.459599	4.371661
1.926720	196.341489	4.376666
1.764450	197.043938	4.381670
1.920901	190.600073	4.386675
1.664713	196.607091	4.391680
1.860021	192.143996	4.396685
1.927936	202.304909	4.401690
1.560513	202.188443	4.406694
1.656953	200.717963	4.411699
1.890069	207.834740	4.416704
2.135593	201.921087	4.421709
1.829905	198.950702	4.426714
1.541178	203.836511	4.431718
1.802275	197.195912	4.436723
1.532129	214.623238	4.441728
1.969830	223.052578	4.446733
2.052229	220.100478	4.451738
2.430532	226.925592	4.456742
2.206670	231.051427	4.461747
1.944261	237.075251	4.466752
2.440231	223.877261	4.471757
2.323818	220.060958	4.476762
2.116892	207.026895	4.481766
2.141188	209.089017	4.486771
1.651746	213.275442	4.491776
1.792047	218.777413	4.496781
2.099419	228.423089	4.501786
2.115443	221.963250	4.506790
2.336398	226.408536	4.511795
1.863006	232.772304	4.516800
2.349431	230.310563	4.521805
1.763049	227.203816	4.526810
2.111589	230.996354	4.531814
2.193350	226.320085	4.536819
2.288639	213.441149	4.541824
2.085458	222.910549	4.546829
2.428933	236.834349	4.551834
1.943926	238.362497	4.556838
2.198540	233.763548	4.561843
2.282456	223.705328	4.566848
2.429547	227.412368	4.571853
2.217064	233.203739	4.576858
1.917661	228.375217	4.581862
2.615590	242.525063	4.586867
2.222497	249.613420	4.591872
2.666000	248.585274	4.596877
2.636812	259.707409	4.601882
2.280525	244.387148	4.606886
2.368202	245.445911	4.611891
2.556822	252.433635	4.616896
2.576231	246.700930	4.621901
2.413970	238.601698	4.626906
2.615652	238.532106	4.631910
2.362825	232.674379	4.636915
2.253977	236.437341	4.641920
2.412815	241.930088	4.646925
2.457466	255.343894	4.651930
2.464861	254.358768	4.656934
2.601210	248.269214	4.661939
2.386169	254.677933	4.666944
2.866157	248.594649	4.671949
2.482258	248.433307	4.676954
2.694209	250.750774	4.681958
2.836022	248.729008	4.686963
2.579233	253.366214	4.691968
2.495924	246.757413	4.696973
2.412910	255.198751	4.701978
2.410407	250.871041	4.706982
2.628106	252.618123	4.711987
2.390701	258.549451	4.716992
2.738162	252.933026	4.721997
2.879141	255.366018	4.727002
2.493299	252.664451	4.732006
2.637166	243.536474	4.737011
2.690937	252.848570	4.742016
2.163372	245.012219	4.747021
2.459126	271.680973	4.752026
2.562316	280.491787	4.757030
2.703346	278.539745	4.762035
2.726569	284.888997	4.767040
3.213398	277.124652	4.772045
3.285315	284.852020	4.777050
2.908431	276.444707	4.782054
3.109424	276.897251	4.787059
2.944087	263.378897	4.792064
2.691524	259.134658	4.797069
3.044070	279.555515	4.802074
2.652235	267.414098	4.807078
3.026251	268.462801	4.812083
2.941366	288.572550	4.817088
2.698316	284.583082	4.822093
2.968316	285.635428	4.827098
2.895548	279.796931	4.832102
3.050968	277.985004	4.837107
3.092193	289.039177	4.842112
3.107259	287.923131	4.847117
3.051743	285.071724	4.852122
3.148360	279.393351	4.857126
2.901939	282.788730	4.862131
2.852264	289.465786	4.867136
3.065274	277.239086	4.872141
3.122381	281.381021	4.877146
2.958344	282.830408	4.882150
3.179310	278.043728	4.887155
2.754939	284.912370	4.892160
3.020886	282.500986	4.897165
3.170993	288.532962	4.902170
2.906768	279.544839	4.907174
2.973622	284.115525	4.912179
2.906425	287.274013	4.917184
3.217255	296.862235	4.922189
3.173884	290.288289	4.927194
2.870788	293.914016	4.932198
3.408940	297.265565	4.937203
3.423985	307.975832	4.942208
3.598500	303.111000	4.947213
3.221174	297.943486	4.952218
3.173622	288.377235	4.957222
3.555370	291.958935	4.962227
3.534436	294.714700	4.967232
3.236902	281.859297	4.972237
2.906943	278.152371	4.977242
3.426907	300.739537	4.982246
3.545843	303.340508	4.987251
3.477795	304.129440	4.992256
3.651890	298.391465	4.997261
3.299142	281.773457	5.002266
3.251903	278.651831	5.007270
3.681415	279.258398	5.012275
3.555991	290.250095	5.017280
3.539150	275.607461	5.022285
3.204435	278.197248	5.027290
3.369493	287.317916	5.032294
3.517666	295.074470	5.037299
3.590490	312.774027	5.042304
3.487180	302.245216	5.047309
3.640817	308.501275	5.052314
3.763965	310.820008	5.057318
3.572033	295.859936	5.062323
3.222851	296.531562	5.067328
3.379412	304.865783	5.072333
3.504906	310.205585	5.077338
3.008941	306.005799	5.082342
3.203545	311.739740	5.087347
3.314689	311.070555	5.092352
3.370620	304.708839	5.097357
3.367177	314.688004	5.102362
3.599820	324.468829	5.107366
3.926716	326.780951	5.112371
3.761423	325.171133	5.117376
3.642562	318.751376	5.122381
3.733237	328.383601	5.127386
4.005744	328.495905	5.132390
4.162018	309.982088	5.137395
3.655881	317.983542	5.142400
3.407471	312.286451	5.147405
3.891044	307.180203	5.152410
3.338182	310.509703	5.157414
3.989480	320.237586	5.162419
4.081352	334.976018	5.167424
3.780187	322.953237	5.172429
3.771277	318.800524	5.177434
3.787326	322.360434	5.182438
4.025270	336.322993	5.187443
4.097788	339.851912	5.192448
4.078651	322.944308	5.197453
3.713519	327.022695	5.202458
3.603817	325.850264	5.207462
3.996670	332.505457	5.212467
3.598870	341.717507	5.217472
3.883234	339.110237	5.222477
3.885276	333.190396	5.227482
3.834875	343.034563	5.232486
3.957347	337.064214	5.237491
3.684835	336.936039	5.242496
4.146445	335.265962	5.247501
3.964097	338.198886	5.252506
3.763189	339.261742	5.257510
4.010062	344.794512	5.262515
3.967242	345.475087	5.267520
3.945133	330.656060	5.272525
4.220921	333.846239	5.277530
3.899400	338.110788	5.282534
4.024166	336.123321	5.287539
3.883019	342.352812	5.292544
4.412455	347.929897	5.297549
4.503301	347.795412	5.302554
4.486817	344.222858	5.307558
4.170548	339.697511	5.312563
4.223708	344.447531	5.317568
4.153507	335.830784	5.322573
4.458256	340.446471	5.327578
4.127093	339.786473	5.332582
3.771146	339.633406	5.337587
4.273162	347.132058	5.342592
4.475399	348.742365	5.347597
4.177899	340.528232	5.352602
4.262023	337.768835	5.357606
3.923698	332.794520	5.362611
4.421149	363.778889	5.367616
4.521804	363.307502	5.372621
4.602478	367.448929	5.377626
4.634263	360.319005	5.382630
4.442018	348.124114	5.387635
4.537422	342.515515	5.392640
3.894393	332.501529	5.397645
4.453333	346.129059	5.402650
4.117984	352.983779	5.407654
4.488060	356.133878	5.412659
4.522987	363.500073	5.417664
4.518422	360.726094	5.422669
4.379359	359.358941	5.427674
4.096158	365.610697	5.432678
4.775069	355.468670	5.437683
4.575926	366.070159	5.442688
4.508015	352.871837	5.447693
4.506491	365.869010	5.452698
4.506678	365.160260	5.457702
4.526107	367.102937	5.462707
4.654839	368.322958	5.467712
4.905610	363.063341	5.472717
4.965218	361.345514	5.477722
4.514067	358.565575	5.482726
4.810075	352.811645	5.487731
4.680830	363.300939	5.492736
4.321054	358.592574	5.497741
4.668887	357.810371	5.502746
4.399779	365.012228	5.507750
4.688356	362.980109	5.512755
4.686505	359.705822	5.517760
4.507849	366.608764	5.522765
5.039548	368.736940	5.527770
5.105488	360.782235	5.532774
5.010419	362.695395	5.537779
4.733109	363.374745	5.542784
4.663883	369.089930	5.547789
4.896580	366.342052	5.552794
4.688791	373.236905	5.557798
4.827251	362.287356	5.562803
4.466780	371.822609	5.567808
4.561081	361.563363	5.572813
4.830976	367.544959	5.577818
4.479135	374.601591	5.582822
4.253372	366.670442	5.587827
4.279456	367.087117	5.592832
4.701609	375.775234	5.597837
4.787155	384.098472	5.602842
4.838958	394.562582	5.607846
5.077197	394.870084	5.612851
5.112896	395.981295	5.617856
5.186495	385.563924	5.622861
5.310775	398.474970	5.627866
4.789056	390.713569	5.632870
4.896339	383.201639	5.637875
4.870091	392.728830	5.642880
5.621699	389.953430	5.647885
5.090205	375.176211	5.652890
5.068963	372.120099	5.657894
4.766098	366.921915	5.662899
4.987617	384.386269	5.667904
5.205481	397.162425	5.672909
4.956756	386.093188	5.677914
5.097811	402.304638	5.682918
5.229848	398.414567	5.687923
5.065130	388.797016	5.692928
5.118462	398.346543	5.697933
5.253709	392.323553	5.702938
5.180421	395.878492	5.707942
5.312505	385.255801	5.712947
5.183063	387.569827	5.717952
5.389674	386.860371	5.722957
5.079621	385.323849	5.727962
5.251966	391.017010	5.732966
5.667233	378.774370	5.737971
5.265725	384.895970	5.742976
5.193823	383.537275	5.747981
5.280549	388.857864	5.752986
4.848022	394.247156	5.757990
4.949260	384.040596	5.762995
4.996478	396.606203	5.768000
5.429636	385.645267	5.773005
5.139148	390.398522	5.778010
5.075452	399.194414	5.783014
5.123892	389.818717	5.788019
4.803275	392.915687	5.793024
5.109135	403.665869	5.798029
5.393215	416.415845	5.803034
5.264581	418.612687	5.808038
5.721330	412.744965	5.813043
5.567105	407.207097	5.818048
5.999402	419.396003	5.823053
5.764355	411.390356	5.828058
5.228708	402.558595	5.833062
5.332553	397.423230	5.838067
5.968599	407.248466	5.843072
5.899025	401.874510	5.848077
5.542373	388.983999	5.853082
5.153395	394.043758	5.858086
5.452062	392.829486	5.863091
5.365494	404.090418	5.868096
5.610362	411.066227	5.873101
5.679516	413.181456	5.878106
5.675982	422.698777	5.883110
6.043433	405.395158	5.888115
5.262671	406.460283	5.893120
5.744857	405.422904	5.898125
5.544732	411.984370	5.903130
5.770433	415.517777	5.908134
5.966222	412.459293	5.913139
5.683685	407.093392	5.918144
5.692723	403.466206	5.923149
5.738914	402.873635	5.928154
5.771019	413.100391	5.933158
5.711194	409.224559	5.938163
5.572848	417.348769	5.943168
5.404816	417.786368	5.948173
5.592918	421.531317	5.953178
5.908554	416.802535	5.958182
5.823860	412.962238	5.963187
5.885071	422.178341	5.968192
5.807812	414.821866	5.973197
6.056049	418.702927	5.978202
5.788683	418.561291	5.983206
6.043485	416.594571	5.988211
5.744317	420.067844	5.993216
5.939668	418.528064	5.998221
6.140023	413.621188	6.003226
5.768255	419.608423	6.008230
6.146871	408.469354	6.013235
6.081311	413.063983	6.018240
5.799045	408.014423	6.023245
5.674648	408.805861	6.028250
5.844477	417.176022	6.033254
6.398249	409.442260	6.038259
5.688204	412.612905	6.043264
5.913638	406.610582	6.048269
6.135766	402.934189	6.053274
5.619103	395.769957	6.058278
5.604920	395.307071	6.063283
5.848394	409.354245	6.068288
5.880637	415.664164	6.073293
5.985845	414.015119	6.078298
5.743730	418.431765	6.083302
5.541835	406.039025	6.088307
5.491592	419.208390	6.093312
5.760060	420.760869	6.098317
5.791693	414.576931	6.103322
5.648723	424.236325	6.108326
5.949730	413.631444	6.113331
5.697942	420.681909	6.118336
5.683844	416.406597	6.123341
5.796893	416.429988	6.128346
5.649014	416.412002	6.133350
5.980741	416.565649	6.138355
6.142924	406.589978	6.143360
6.043653	419.475952	6.148365
6.121359	417.986243	6.153370
6.169764	414.251645	6.158374
5.961097	418.615592	6.163379
5.772242	405.423525	6.168384
5.867146	418.813762	6.173389
5.911140	418.117128	6.178394
5.765797	414.738760	6.183398
6.212710	413.763857	6.188403
5.656339	416.385229	6.193408
5.952709	420.622590	6.198413
5.968495	415.924970	6.203418
5.677840	414.369587	6.208422
5.674327	403.708019	6.213427
5.596529	415.426338	6.218432
5.725584	420.072737	6.223437
5.836432	417.214225	6.228442
5.688996	415.022621	6.233446
5.896077	413.803714	6.238451
6.111802	423.577753	6.243456
5.877421	429.021433	6.248461
6.060819	419.893501	6.253466
5.636488	432.453920	6.258470
6.204445	415.846557	6.263475
6.050553	417.996734	6.268480
5.770027	421.679063	6.273485
5.734618	420.175439	6.278490
5.922527	416.381016	6.283494
5.929808	409.625079	6.288499
6.082183	424.192750	6.293504
5.949864	420.261835	6.298509
5.910057	416.629644	6.303514
5.779022	416.558397	6.308518
6.109963	424.925465	6.313523
5.885439	418.797480	6.318528
5.783966	424.305759	6.323533
6.031667	417.474183	6.328538
5.705898	411.805000	6.333542
6.172610	414.936805	6.338547
5.845440	424.065062	6.343552
6.084966	413.659644	6.348557
6.096845	409.921277	6.353562
6.181552	415.637669	6.358566
6.054839	401.780956	6.363571
5.484607	389.705373	6.368576
5.474203	399.894488	6.373581
5.453615	412.027794	6.378586
5.950217	422.222907	6.383590
6.010699	409.760581	6.388595
6.100271	413.460852	6.393600
5.930413	417.334653	6.398605
6.090847	414.927128	6.403610
5.721802	419.110555	6.408614
6.022950	408.008935	6.413619
5.952749	413.101012	6.418624
5.959598	405.497239	6.423629
6.212688	408.883982	6.428634
5.616518	397.692001	6.433638
5.691619	387.486370	6.438643
5.604805	402.025059	6.443648
5.777017	410.341058	6.448653
6.128457	411.776130	6.453658
5.613604	411.701744	6.458662
6.318974	409.499910	6.463667
6.037714	408.863730	6.468672
5.501667	402.974390	6.473677
5.991233	400.676653	6.478682
5.569626	404.146960	6.483686
5.927431	405.919563	6.488691
5.751568	409.806959	6.493696
5.396710	416.038322	6.498701
5.802438	408.735891	6.503706
5.916402	410.999127	6.508710
5.695101	406.781592	6.513715
5.646103	413.388984	6.518720
5.877062	409.404316	6.523725
5.824565	410.798271	6.528730
5.752310	414.001867	6.533734
6.248366	412.864236	6.538739
6.298636	417.826705	6.543744
5.964277	419.695104	6.548749
5.610064	420.351704	6.553754
5.844627	422.656159	6.558758
5.897976	420.388800	6.563763
5.710309	419.174794	6.568768
5.996697	413.811502	6.573773
6.044613	414.269051	6.578778
6.056491	425.315250	6.583782
5.981645	418.059638	6.588787
6.059561	412.292403	6.593792
6.011141	410.031499	6.598797
6.300024	411.248577	6.603802
6.216143	406.209064	6.608806
5.967741	389.777090	6.613811
6.007662	395.940264	6.618816
5.949289	388.517564	6.623821
5.676558	388.822867	6.628826
5.625878	391.295399	6.633830
5.796304	387.114571	6.638835
5.794590	395.350244	6.643840
5.429392	396.767882	6.648845
5.959706	401.455812	6.653850
5.764348	413.480457	6.658854
6.327701	414.866508	6.663859
6.236688	408.878963	6.668864
5.567943	408.505979	6.673869
5.645523	393.127102	6.678874
6.313547	395.344655	6.683878
5.812150	397.495493	6.688883
5.469414	404.335571	6.693888
5.809675	399.634573	6.698893
6.103834	406.580511	6.703898
5.852557	414.323772	6.708902
5.766444	395.537789	6.713907
5.989298	403.693986	6.718912
5.895419	400.225298	6.723917
6.114622	399.615111	6.728922
5.851819	395.701481	6.733926
5.914092	394.011708	6.738931
5.612638	391.559494	6.743936
5.456635	396.218911	6.748941
5.803308	406.972192	6.753946
6.067565	412.878755	6.758950
6.177738	410.513908	6.763955
5.540617	405.811019	6.768960
5.825206	410.686152	6.773965
6.055191	413.149514	6.778970
6.090116	414.093164	6.783974
5.805362	411.663641	6.788979
5.714432	405.081285	6.793984
5.697365	402.673098	6.798989
5.795860	412.952729	6.803994
5.755095	413.376714	6.808998
6.079924	410.617558	6.814003
5.382717	416.608325	6.819008
5.662824	422.091618	6.824013
5.778763	417.191640	6.829018
6.031495	417.224784	6.834022
5.943705	414.647338	6.839027
5.991520	414.449991	6.844032
5.899688	417.599706	6.849037
6.068654	419.338621	6.854042
5.881133	416.333866	6.859046
5.859348	412.863371	6.864051
5.846232	417.978144	6.869056
5.961513	417.824011	6.874061
5.894639	411.335962	6.879066
5.888268	420.958133	6.884070
6.236245	414.749940	6.889075
6.192640	419.784068	6.894080
5.871083	406.119236	6.899085
6.118607	402.641349	6.904090
5.725107	400.029545	6.909094
6.024322	397.935643	6.914099
5.693176	403.448262	6.919104
5.623276	396.157082	6.924109
5.895907	398.167661	6.929114
5.708452	405.315611	6.934118
5.845556	401.576609	6.939123
5.661584	417.826344	6.944128
6.093593	418.805856	6.949133
5.938142	422.361019	6.954138
5.814713	419.289271	6.959142
5.894471	424.835595	6.964147
6.137495	426.287655	6.969152
5.785047	406.274695	6.974157
5.575778	399.631787	6.979162
5.848765	405.429409	6.984166
6.089788	411.099161	6.989171
5.841122	413.191419	6.994176
5.923368	411.403600	6.999181
5.852463	403.122296	7.004186
5.463201	414.531903	7.009190
5.880484	416.469199	7.014195
6.551096	410.726161	7.019200
6.061762	399.890771	7.024205
6.194710	392.039451	7.029210
5.534175	397.315770	7.034214
5.751881	399.483655	7.039219
5.837909	390.345683	7.044224
5.592435	393.769408	7.049229
6.187635	394.875214	7.054234
5.643223	398.431202	7.059238
5.960195	390.174554	7.064243
6.120420	394.398438	7.069248
6.146992	389.553600	7.074253
6.089821	382.298396	7.079258
5.471773	394.939762	7.084262
5.571283	385.404202	7.089267
5.603154	394.599578	7.094272
5.767334	405.052414	7.099277
6.032490	410.231155	7.104282
6.036909	408.771913	7.109286
5.600344	402.737269	7.114291
6.101291	403.601574	7.119296
6.014680	396.736964	7.124301
5.959774	393.306464	7.129306
5.736877	395.280785	7.134310
5.729765	387.745648	7.139315
5.738003	399.001213	7.144320
6.071302	405.653110	7.149325
6.012934	399.505426	7.154330
5.574492	401.295216	7.159334
5.711636	403.906004	7.164339
5.981214	418.021862	7.169344
5.597273	417.718152	7.174349
5.814459	423.926330	7.179354
6.102558	412.355340	7.184358
5.950046	420.102112	7.189363
5.963217	422.349504	7.194368
6.304309	418.771530	7.199373
6.212059	401.119153	7.204378
5.945335	400.120020	7.209382
6.117405	399.292586	7.214387
5.940636	401.136291	7.219392
5.643744	393.200455	7.224397
5.607998	389.586616	7.229402
5.537483	395.523479	7.234406
5.701064	391.106436	7.239411
5.607978	386.909947	7.244416
6.215434	407.423892	7.249421
6.028688	398.369784	7.254426
5.681234	405.432069	7.259430
5.659549	396.405886	7.264435
5.605403	406.883439	7.269440
5.894911	410.704247	7.274445
6.116462	407.755624	7.279450
5.925885	418.358966	7.284454
5.888558	415.552146	7.289459
5.560218	422.522856	7.294464
5.734497	421.562194	7.299469
6.231415	418.915282	7.304474
5.662453	430.650455	7.309478
5.962084	426.009602	7.314483
6.037344	422.982655	7.319488
5.694168	419.562515	7.324493
6.175902	422.002253	7.329498
5.696737	427.680444	7.334502
6.005526	416.080899	7.339507
6.057745	420.786794	7.344512
5.739721	409.481622	7.349517
6.061853	395.833005	7.354522
5.651886	398.089742	7.359526
5.834746	393.464030	7.364531
5.746479	410.053110	7.369536
6.044310	417.795761	7.374541
6.041858	416.581209	7.379546
5.851769	412.497992	7.384550
6.042741	398.721223	7.389555
5.510011	396.694395	7.394560
5.411392	406.134854	7.399565
6.088697	409.284283	7.404570
6.030126	419.183556	7.409574
5.683240	422.110636	7.414579
6.142200	420.393509	7.419584
5.993994	421.884720	7.424589
6.215067	416.677198	7.429594
6.049045	403.025964	7.434598
5.851656	404.759003	7.439603
5.980900	398.958419	7.444608
5.845805	391.367401	7.449613
5.675284	397.639479	7.454618
5.763731	402.947147	7.459622
5.833869	400.095017	7.464627
5.742959	397.973654	7.469632
5.672284	400.800504	7.474637
6.061356	418.453780	7.479642
5.999156	415.043402	7.484646
5.648264	392.989545	7.489651
5.705881	409.182436	7.494656
5.776794	424.490551	7.499661
5.912238	419.359721	7.504666
5.703403	421.274892	7.509670
6.044540	420.819610	7.514675
6.187564	415.526238	7.519680
5.997198	414.568925	7.524685
5.936249	397.515938	7.529690
5.554457	403.197847	7.534694
5.955801	403.590529	7.539699
6.013088	408.444326	7.544704
5.814089	408.684292	7.549709
5.769307	403.860121	7.554714
5.831301	408.940976	7.559718
6.107352	412.254518	7.564723
6.042290	401.928467	7.569728
5.730330	394.564480	7.574733
5.833711	391.213586	7.579738
5.724236	400.298231	7.584742
5.922480	402.826678	7.589747
5.983958	398.656590	7.594752
5.951505	399.167860	7.599757
5.718486	392.462236	7.604762
5.769096	399.101473	7.609766
6.216599	413.015440	7.614771
5.998203	395.060123	7.619776
5.576662	400.754588	7.624781
5.782474	388.361257	7.629786
5.625221	401.518900	7.634790
6.064653	405.436442	7.639795
6.361971	403.709841	7.644800
5.875331	395.841699	7.649805
6.028740	387.775199	7.654810
5.475171	388.649699	7.659814
5.751252	386.331627	7.664819
5.755394	396.565919	7.669824
5.987830	410.624314	7.674829
6.070050	393.893756	7.679834
5.858603	401.032808	7.684838
5.930394	387.591104	7.689843
5.916703	391.285403	7.694848
6.013185	404.517191	7.699853
5.934856	388.159814	7.704858
5.466994	394.158933	7.709862
5.808582	388.730051	7.714867
5.873009	399.442127	7.719872
5.851464	398.493166	7.724877
6.230715	394.225833	7.729882
5.934772	395.746517	7.734886
5.841180	391.489994	7.739891
5.632908	392.709033	7.744896
5.826351	402.053108	7.749901
6.175006	393.206188	7.754906
5.804783	392.030278	7.759910
5.792342	392.367566	7.764915
6.084930	394.745185	7.769920
5.398684	393.381503	7.774925
5.755586	393.104089	7.779930
5.402479	405.261016	7.784934
5.727953	409.993698	7.789939
6.079482	424.321353	7.794944
6.166228	423.817342	7.799949
6.287794	420.305402	7.804954
6.124299	413.595204	7.809958
6.018971	396.602957	7.814963
5.746377	398.132638	7.819968
5.890970	401.055477	7.824973
5.776378	398.093083	7.829978
5.759707	391.679435	7.834982
5.859698	391.894701	7.839987
5.896426	394.590825	7.844992
5.897262	399.867926	7.849997
6.197429	395.869253	7.855002
6.243986	393.046129	7.860006
5.936633	383.324377	7.865011
5.884802	395.383471	7.870016
6.204125	399.778585	7.875021
6.043526	404.416578	7.880026
6.031594	399.666357	7.885030
5.822538	398.594911	7.890035
5.508492	392.832147	7.895040
5.875856	399.269891	7.900045
5.896518	390.819219	7.905050
5.926439	388.701071	7.910054
5.686163	393.724877	7.915059
6.107046	382.250163	7.920064
5.743972	392.488203	7.925069
6.199396	390.344517	7.930074
5.717832	394.178564	7.935078
5.739835	387.758858	7.940083
5.686240	388.991628	7.945088
5.530646	406.116449	7.950093
5.909059	391.313712	7.955098
5.628120	399.463420	7.960102
5.905139	391.627492	7.965107
5.731235	398.023490	7.970112
5.472090	398.794910	7.975117
6.052740	400.292147	7.980122
5.506595	404.086735	7.985139
5.847650	404.620242	7.990157
6.091589	421.373771	7.995174
5.860171	413.952951	8.000192
6.006103	405.971245	8.005210
5.938002	400.796986	8.010227
5.504271	396.891824	8.015245
5.623347	410.139930	8.020262
5.823828	418.073620	8.025280
6.146484	419.503089	8.030298
6.225966	416.846085	8.035315
6.119957	414.615770	8.040333
6.105554	405.475778	8.045350
5.623718	412.512842	8.050368
6.094074	407.036467	8.055386
5.935639	408.579183	8.060403
6.113943	390.560270	8.065421
6.086442	402.701578	8.070438
5.653382	395.530106	8.075456
5.805848	396.705377	8.080474
6.066560	411.540727	8.085491
5.851522	422.218759	8.090509
6.098708	421.795001	8.095526
5.964467	420.468499	8.100544
6.145384	427.142956	8.105562
6.009522	422.433736	8.110579
6.043075	409.698132	8.115597
6.381727	413.327812	8.120614
5.964181	406.968090	8.125632
6.028874	393.713230	8.130650
5.752381	400.364672	8.135667
5.835057	406.704224	8.140685
6.019999	402.976677	8.145702
5.440546	420.187413	8.150720
5.979197	417.022972	8.155738
5.900054	416.621942	8.160755
5.885529	432.728023	8.165773
6.180147	428.904392	8.170790
6.002815	432.980989	8.175808
6.363071	420.115295	8.180826
6.234511	425.591717	8.185843
6.198504	424.612736	8.190861
6.305922	424.207721	8.195878
6.275682	424.944568	8.200896
6.124062	420.550238	8.205914
5.906896	424.585737	8.210931
5.968349	423.793455	8.215949
6.158997	428.528752	8.220966
5.923937	420.698251	8.225984
6.132918	423.171153	8.231002
6.287782	430.449286	8.236019
6.021085	425.842615	8.241037
6.165019	422.500180	8.246054
6.281476	433.934153	8.251072
6.598263	422.100891	8.256090
6.318624	430.769366	8.261107
6.002751	426.429171	8.266125
6.397993	423.729004	8.271142
6.238003	429.235597	8.276160
6.125212	402.959483	8.281178
5.981822	410.527332	8.286195
5.774969	424.284100	8.291213
6.025025	426.453925	8.296230
5.665908	428.463580	8.301248
6.161537	429.711317	8.306266
5.903201	431.036161	8.311283
5.788081	425.657825	8.316301
6.341386	428.875185	8.321318
5.960667	425.791675	8.326336
6.145893	427.267924	8.331354
5.855229	433.624956	8.336371
5.987109	435.582928	8.341389
6.408130	440.733407	8.346406
6.242743	448.487753	8.351424
6.583751	442.277407	8.356442
6.755425	433.887718	8.361459
6.218447	427.262683	8.366477
6.266607	427.412899	8.371494
6.618359	439.248660	8.376512
6.341098	424.570460	8.381530
5.999064	433.870397	8.386547
5.921325	428.953255	8.391565
6.165646	430.839961	8.396582
6.516244	434.300518	8.401600
6.443280	431.799940	8.406618
6.279959	429.651185	8.411635
6.034372	423.854641	8.416653
6.335642	435.789827	8.421670
6.323981	436.978193	8.426688
6.329569	434.228625	8.431706
6.540361	441.201358	8.436723
6.223401	440.102297	8.441741
6.391090	436.049247	8.446758
6.253473	444.465106	8.451776
6.377604	439.484775	8.456794
6.417065	440.791362	8.461811
6.345469	443.888887	8.466829
6.510864	443.354869	8.471846
6.101418	435.753654	8.476864
6.494746	445.001494	8.481882
6.703894	442.014906	8.486899
6.101380	446.148656	8.491917
6.261636	443.923955	8.496934
5.921938	453.255093	8.501952
6.288136	449.448645	8.506970
6.798936	448.352430	8.511987
6.239466	451.236068	8.517005
6.403457	455.432758	8.522022
6.438543	452.025322	8.527040
6.332499	452.430069	8.532058
6.275856	447.206664	8.537075
5.938140	455.136335	8.542093
6.595723	439.134550	8.547110
6.604751	444.892373	8.552128
6.543685	441.888163	8.557146
6.789795	445.327224	8.562163
6.379663	449.355095	8.567181
6.506178	439.391442	8.572199
6.470582	452.121023	8.577216
6.556288	444.921899	8.582234
6.996459	449.599171	8.587251
6.386210	452.960974	8.592269
6.615510	450.271024	8.597287
6.228165	445.695874	8.602304
6.316984	446.587635	8.607322
6.832509	447.579794	8.612339
6.389955	444.862571	8.617357
6.965991	445.359262	8.622375
6.944275	453.195239	8.627392
6.738540	448.471714	8.632410
6.605441	446.141499	8.637427
6.613502	454.259986	8.642445
6.613983	442.492049	8.647463
6.735401	451.697290	8.652480
6.606232	446.636725	8.657498
6.588104	445.588670	8.662515
6.275131	444.419557	8.667533
6.430564	449.065705	8.672551
6.473019	445.451991	8.677568
6.403183	453.790963	8.682586
6.714757	448.112239	8.687603
6.227605	457.229800	8.692621
6.406819	444.231511	8.697639
6.716089	448.929293	8.702656
6.606119	458.252842	8.707674
6.865132	455.760205	8.712691
6.483830	451.704807	8.717709
6.745714	443.471391	8.722727
6.792392	451.927804	8.727744
6.744579	442.505853	8.732762
6.827487	447.740868	8.737779
6.795243	440.730636	8.742797
6.901391	442.866208	8.747815
6.832309	447.134127	8.752832
6.906832	447.554764	8.757850
7.206696	444.781177	8.762867
6.647406	454.140409	8.767885
6.507758	449.523293	8.772903
6.626058	441.886723	8.777920
6.689824	441.169815	8.782938
6.737231	436.627534	8.787955
6.860905	446.024920	8.792973
6.588280	437.673285	8.797991
6.622635	451.114574	8.803008
6.348222	446.553287	8.808026
6.715979	439.202677	8.813043
6.631540	448.111971	8.818061
6.476130	458.777526	8.823079
6.454414	449.944766	8.828096
6.324191	453.830953	8.833114
6.930700	455.995424	8.838131
6.598713	460.373966	8.843149
6.876611	466.910167	8.848167
6.964493	476.089118	8.853184
6.705080	475.504895	8.858202
6.989609	471.771197	8.863219
6.870703	471.187050	8.868237
6.773875	455.297142	8.873255
6.520150	456.371960	8.878272
6.946159	465.867151	8.883290
6.841955	469.641968	8.888307
6.619506	477.190675	8.893325
7.035455	465.988779	8.898343
7.069042	466.223329	8.903360
6.828261	470.900003	8.908378
7.133488	463.382457	8.913395
6.878339	469.014424	8.918413
6.846253	471.947975	8.923431
6.734238	477.241941	8.928448
7.052388	471.660008	8.933466
6.983954	473.134980	8.938483
6.412311	476.642214	8.943501
6.768853	472.060956	8.948519
6.627222	474.828637	8.953536
6.399714	474.971553	8.958554
6.657585	473.694063	8.963571
6.550807	475.995542	8.968589
6.855866	469.667743	8.973607
6.914660	478.254813	8.978624
7.017753	492.483772	8.983642
7.167973	485.971948	8.988659
7.021568	481.191782	8.993677
6.765603	480.976243	8.998695
6.770319	490.868812	9.003712
7.214203	495.173134	9.008730
7.511889	491.841310	9.013747
6.867161	485.087970	9.018765
6.696340	470.800149	9.023783
7.039107	482.444845	9.028800
6.908024	494.245843	9.033818
7.089327	491.175248	9.038835
7.123289	495.572199	9.043853
6.948934	496.259047	9.048871
6.789692	494.926990	9.053888
7.044709	494.016014	9.058906
7.274493	500.831163	9.063923
6.843005	508.889157	9.068941
7.314050	497.978407	9.073959
7.273364	489.902829	9.078976
7.535867	507.786451	9.083994
7.033209	485.938889	9.089011
6.800110	488.929185	9.094029
7.363319	489.225918	9.099047
7.365561	483.766061	9.104064
6.655459	483.817335	9.109082
7.043773	479.376261	9.114099
7.336442	490.350322	9.119117
7.462151	495.891066	9.124135
6.987112	482.490335	9.129152
7.200264	493.079230	9.134170
7.365177	496.076593	9.139187
7.167304	489.303730	9.144205
7.576754	476.783734	9.149223
7.430184	475.323462	9.154240
6.903084	474.367776	9.159258
6.962872	473.701982	9.164275
6.911036	478.308030	9.169293
7.471273	480.063193	9.174311
7.299821	469.811698	9.179328
6.799892	477.343922	9.184346
7.017406	492.457503	9.189363
7.024576	492.740372	9.194381
7.304398	492.866915	9.199399
7.204109	492.232513	9.204416
6.823667	495.858115	9.209434
7.363406	494.157768	9.214451
7.429867	498.095197	9.219469
7.257859	501.994252	9.224487
7.706309	497.808837	9.229504
7.489758	502.961400	9.234522
7.330318	493.263426	9.239539
7.563039	492.068769	9.244557
7.439740	506.039724	9.249575
7.240281	493.252208	9.254592
7.422643	496.824343	9.259610
6.995030	495.420727	9.264627
7.091095	497.207594	9.269645
7.074392	492.880468	9.274663
7.554049	482.271332	9.279680
7.235933	495.660584	9.284698
7.364349	495.144982	9.289715
7.424020	499.200238	9.294733
7.467745	493.049077	9.299751
7.261153	487.473617	9.304768
6.776932	499.916922	9.309786
7.271789	495.661120	9.314803
7.354354	498.377899	9.319821
7.132736	493.363364	9.324839
7.219886	485.627516	9.329856
7.262174	495.599406	9.334874
7.353068	497.683726	9.339891
7.718454	499.567249	9.344909
7.586206	498.739041	9.349927
7.650388	486.506663	9.354944
7.225208	494.554195	9.359962
7.395575	493.053731	9.364979
7.565989	498.082548	9.369997
7.432635	497.330252	9.375015
7.466447	499.679133	9.380032
7.083464	503.043205	9.385050
7.291853	498.368389	9.390067
7.620048	512.874517	9.395085
7.900873	508.219906	9.400103
7.884924	495.760238	9.405120
7.609926	498.561442	9.410138
7.486304	499.287678	9.415155
7.674466	490.406235	9.420173
6.931042	494.057151	9.425191
7.677186	497.329515	9.430208
7.714134	493.833418	9.435226
7.425923	490.792206	9.440243
7.480983	488.896403	9.445261
7.316347	497.284962	9.450279
7.304919	499.076049	9.455296
7.534395	517.406663	9.460314
7.499535	511.996791	9.465331
7.760206	523.714337	9.470349
7.727586	528.569849	9.475367
7.749166	519.266372	9.480384
7.562065	528.346424	9.485402
7.725612	522.962266	9.490419
8.041197	519.308899	9.495437
7.725869	513.015173	9.500455
8.057173	492.883064	9.505472
7.506240	494.925936	9.510490
7.617421	499.818868	9.515507
7.714848	501.018549	9.520525
7.552196	499.453499	9.525543
7.660021	493.109259	9.530560
7.779524	495.675084	9.535578
7.622940	497.788712	9.540595
7.806607	492.552887	9.545613
7.891517	495.281921	9.550631
8.164153	493.115345	9.555648
7.585984	499.836180	9.560666
7.586416	498.636894	9.565683
7.720592	496.006022	9.570701
7.448794	497.538105	9.575719
7.530436	491.201124	9.580736
7.682774	498.192506	9.585754
7.531211	499.664726	9.590771
7.764663	509.190110	9.595789
8.169635	524.649885	9.600807
7.836486	515.745968	9.605824
7.666963	509.116978	9.610842
7.569129	505.708267	9.615859
7.461864	506.416161	9.620877
7.599045	524.915877	9.625895
8.080266	508.402027	9.630912
7.806141	516.722544	9.635930
7.774432	525.740378	9.640947
7.967620	523.475794	9.645965
7.769891	527.953236	9.650983
8.115461	517.112626	9.656000
7.873125	527.249049	9.661018
8.157175	523.196683	9.666035
8.324327	520.219818	9.671053
7.791954	506.083290	9.676071
7.897321	498.458190	9.681088
7.588046	503.779914	9.686106
7.866030	509.293648	9.691123
8.117142	516.837600	9.696141
7.599781	518.196723	9.701159
8.133464	510.021676	9.706176
8.225671	521.661475	9.711194
7.900351	508.426613	9.716211
8.180475	500.685769	9.721229
7.536284	502.471858	9.726247
7.716775	505.084933	9.731264
8.219901	518.916724	9.736282
7.941207	522.911393	9.741299
8.064247	518.404578	9.746317
7.975918	517.143458	9.751335
8.144499	517.505178	9.756352
8.130847	515.197265	9.761370
7.619759	499.523701	9.766387
7.950205	506.108488	9.771405
8.031020	512.325294	9.776423
8.160159	515.495521	9.781440
7.752491	525.058250	9.786458
7.640589	526.492700	9.791475
7.908806	515.853558	9.796493
7.685640	520.344451	9.801511
7.869352	522.499436	9.806528
7.965686	517.981026	9.811546
8.019402	522.832476	9.816563
7.952796	524.496512	9.821581
7.780836	524.665439	9.826599
8.089780	524.036344	9.831616
8.131666	526.904666	9.836634
7.864673	525.021450	9.841651
8.191520	521.710297	9.846669
7.910309	531.168010	9.851687
8.390795	534.289502	9.856704
8.191334	536.248908	9.861722
8.127252	525.598709	9.866739
8.115735	525.004046	9.871757
7.909797	535.002228	9.876775
7.805137	537.338096	9.881792
7.897432	549.015768	9.886810
7.886295	545.738632	9.891827
8.451269	536.955916	9.896845
8.182743	551.388314	9.901863
8.060797	552.180560	9.906880
7.929776	548.470931	9.911898
8.018942	555.936133	9.916915
8.025735	545.861793	9.921933
7.827815	554.568016	9.926951
8.146824	557.743215	9.931968
8.007290	556.742578	9.936986
8.275418	569.146945	9.942003
8.650584	563.653880	9.947021
8.298995	565.558229	9.952039
8.505820	553.757888	9.957056
8.362788	549.494723	9.962074
8.318500	553.963909	9.967091
8.558421	537.730833	9.972109
8.425780	559.270850	9.977127
8.128798	551.333230	9.982144
8.136068	551.417271	9.987162
8.257514	545.395923	9.992179
8.532890	544.589052	9.997197
8.278588	557.712734	10.002215
8.667760	555.407972	10.007232
8.311306	548.877682	10.012250
8.248843	549.307161	10.017267
8.372367	546.611680	10.022285
8.377957	545.140185	10.027303
8.033482	540.936986	10.032320
8.304137	555.553149	10.037338
8.098975	564.639205	10.042355
8.344522	573.269642	10.047373
8.351455	574.240511	10.052391
8.231010	566.262602	10.057408
8.346229	568.207419	10.062426
8.261601	574.929849	10.067443
8.704112	564.036153	10.072461
8.300821	563.562832	10.077479
8.214225	558.618640	10.082496
8.662221	578.000668	10.087514
8.731967	571.308919	10.092531
8.485790	572.455144	10.097549
8.591276	569.292274	10.102567
8.369211	564.315658	10.107584
8.740336	571.607302	10.112602
8.384127	567.790941	10.117619
8.513134	570.156473	10.122637
8.804371	575.879589	10.127655
8.538406	575.144911	10.132672
8.346277	579.962313	10.137690
8.175705	575.858090	10.142707
8.602719	565.825195	10.147725
8.452155	576.625760	10.152743
8.246519	576.402334	10.157760
8.467880	569.936137	10.162778
8.322835	567.134411	10.167795
8.909898	566.745759	10.172813
8.328821	579.065439	10.177831
8.614362	568.827492	10.182848
8.855473	570.515901	10.187866
8.367339	575.818334	10.192883
8.705610	576.159781	10.197901
8.763488	587.006588	10.202919
8.517662	587.452174	10.207936
8.906999	582.253526	10.212954
8.808051	586.841737	10.217971
8.621927	577.084782	10.222989
8.640900	577.056537	10.228007
8.524324	593.819377	10.233024
8.888762	596.536188	10.238042
8.577526	596.373488	10.243059
9.097269	592.148479	10.248077
8.720803	595.508391	10.253095
8.659593	583.175674	10.258112
8.756561	582.516674	10.263130
8.915559	589.437621	10.268147
8.787047	581.565109	10.273165
8.657810	579.628745	10.278183
8.720102	588.272124	10.283200
8.756629	595.234352	10.288218
8.415396	593.949737	10.293235
8.830145	606.952848	10.298253
8.947474	601.474923	10.303271
8.671175	604.525655	10.308288
8.770365	600.063580	10.313306
9.011908	605.377927	10.318323
9.099387	596.985575	10.323341
9.284627	609.336686	10.328359
8.890801	593.988648	10.333376
8.913819	585.656894	10.338394
9.171978	580.819625	10.343411
8.618041	582.878756	10.348429
8.631514	585.088824	10.353447
9.083647	591.496787	10.358464
8.844917	585.228904	10.363482
8.814017	596.045445	10.368499
9.388538	601.083558	10.373517
9.084373	586.352636	10.378535
8.875937	582.964396	10.383552
9.062654	578.898865	10.388570
8.225552	583.334488	10.393587
8.857891	587.063354	10.398605
9.309710	595.809806	10.403623
9.156390	596.947795	10.408640
9.083500	585.749834	10.413658
8.759003	588.814426	10.418675
8.894868	592.425423	10.423693
9.202579	601.958157	10.428711
9.096370	607.819294	10.433728
9.100068	593.889036	10.438746
8.990818	602.840164	10.443763
9.126208	599.492723	10.448781
9.493324	595.998524	10.453799
8.902623	592.304104	10.458816
8.881439	586.680629	10.463834
8.983668	594.519339	10.468851
9.229006	585.619423	10.473869
9.033468	594.047583	10.478887
9.129483	596.364640	10.483904
8.906510	595.765236	10.488922
8.990951	608.835881	10.493939
9.455034	609.722502	10.498957
8.957612	607.313649	10.503975
9.048854	607.422403	10.508992
9.398381	596.792564	10.514010
8.968778	605.771796	10.519027
9.052919	605.550304	10.524045
9.012617	609.741170	10.529063
9.054070	610.485727	10.534080
9.143234	603.850883	10.539098
8.996358	605.565372	10.544115
9.374977	615.181677	10.549133
9.214749	605.559504	10.554151
8.996221	601.841484	10.559168
9.543836	603.207320	10.564186
9.463069	609.471567	10.569203
9.461612	603.501015	10.574221
9.539770	600.074179	10.579239
9.063077	599.801705	10.584256
9.775568	603.723143	10.589274
9.059502	608.843549	10.594291
9.039729	606.381949	10.599309
9.313375	594.504840	10.604327
9.158274	610.317528	10.609344
9.631118	601.164209	10.614362
8.880310	606.103866	10.619379
9.217981	603.800855	10.624397
9.112848	603.877261	10.629415
9.260400	605.482504	10.634432
9.796683	600.024143	10.639450
9.289140	608.876734	10.644467
9.207369	610.098187	10.649485
9.334445	599.657834	10.654503
9.195172	604.542699	10.659520
9.406542	593.486387	10.664538
9.023749	601.805034	10.669555
8.975842	609.878713	10.674573
9.116921	614.814329	10.679591
9.196638	627.074689	10.684608
9.478619	621.820268	10.689626
9.483992	631.040627	10.694643
9.513062	634.538978	10.699661
9.626546	625.211579	10.704679
9.554145	627.993683	10.709696
9.586913	626.874528	10.714714
9.862921	633.568876	10.719731
9.830566	633.832695	10.724749
9.968424	624.908574	10.729767
9.364042	619.294415	10.734784
9.457254	608.411239	10.739802
9.158892	610.282007	10.744819
9.415957	614.470464	10.749837
9.595088	624.935380	10.754855
9.601861	631.570926	10.759872
9.589216	619.981653	10.764890
9.748156	628.729828	10.769907
9.744056	632.107144	10.774925
9.965713	627.616407	10.779943
9.562626	615.188910	10.784960
9.806973	605.279287	10.789978
9.653657	599.357776	10.794995
9.525447	600.494987	10.800013
9.463971	606.642603	10.805031
9.445960	615.617311	10.810048
9.935884	616.755503	10.815066
9.880023	625.136546	10.820083
9.493205	619.706048	10.825101
9.588931	616.617282	10.830119
9.422831	621.089791	10.835136
9.864448	617.760638	10.840154
9.521575	632.144790	10.845171
9.537605	622.829506	10.850189
9.995767	620.176256	10.855207
10.123533	634.000677	10.860224
10.062106	627.443067	10.865242
9.320622	623.990016	10.870259
9.754630	629.892749	10.875277
9.983731	630.175563	10.880295
9.710971	626.358737	10.885312
9.692331	623.552975	10.890330
9.692987	628.318094	10.895347
9.733335	629.346846	10.900365
10.155111	619.327365	10.905383
9.766639	624.683625	10.910400
9.927782	620.906113	10.915418
9.971971	623.016700	10.920435
10.011032	624.910341	10.925453
10.074547	623.202546	10.930471
10.130785	622.584641	10.935488
10.072747	627.841792	10.940506
10.399035	622.662478	10.945523
9.755113	607.653414	10.950541
9.557680	602.988507	10.955559
9.057924	615.074564	10.960576
9.088370	620.949008	10.965594
9.580766	629.108452	10.970611
9.499178	635.947192	10.975629
9.919667	624.652969	10.980647
9.933079	637.457053	10.985664
10.240599	650.366545	10.990682
10.227246	639.979728	10.995699
9.724471	643.356284	11.000717
10.185397	632.825733	11.005735
9.677357	640.747458	11.010752
9.917845	645.181515	11.015770
10.383756	646.052073	11.020787
10.133745	659.777914	11.025805
10.086975	636.299774	11.030823
9.872050	641.187036	11.035840
10.340890	641.754178	11.040858
9.928596	638.334751	11.045875
9.974964	646.772371	11.050893
9.995248	651.815286	11.055911
10.262837	660.817853	11.060928
10.001710	654.676530	11.065946
10.131745	651.995792	11.070963
9.996836	665.249168	11.075981
10.131488	657.821383	11.080999
10.043478	652.072659	11.086016
9.999568	657.494862	11.091034
10.328762	663.814816	11.096051
10.109010	663.183347	11.101069
10.123368	655.503012	11.106087
9.939525	666.823241	11.111104
10.015218	657.429163	11.116122
10.265481	656.632533	11.121139
10.221068	658.144782	11.126157
9.934774	661.092948	11.131175
10.142539	666.649290	11.136192
10.302372	658.226638	11.141210
10.453666	666.669918	11.146227
10.251243	665.571831	11.151245
10.413151	658.982373	11.156263
10.127527	667.001805	11.161280
10.117173	658.523767	11.166298
10.276862	657.226933	11.171315
9.958219	659.053547	11.176333
10.138710	657.396849	11.181351
10.345825	681.777648	11.186368
10.100160	683.605453	11.191386
10.410541	675.408513	11.196403
10.070275	685.004948	11.201421
10.378483	671.323565	11.206439
10.495497	678.872818	11.211456
10.625597	679.268973	11.216474
10.641027	691.454243	11.221491
10.366410	685.365516	11.226509
10.372509	693.134125	11.231527
10.202888	688.834067	11.236544
10.629771	693.819599	11.241562
10.726104	684.602154	11.246579
10.502732	688.004369	11.251597
10.720802	681.286183	11.256615
10.578207	680.418562	11.261632
10.834201	685.897926	11.266650
10.541910	666.005339	11.271667
10.477770	661.666670	11.276685
10.514677	653.339020	11.281703
10.435177	669.890995	11.286720
10.422274	671.852743	11.291738
10.462818	679.543365	11.296755
10.192068	690.511152	11.301773
10.419244	679.256650	11.306791
10.232082	687.172301	11.311808
10.279117	689.787379	11.316826
10.710388	678.945867	11.321843
10.634125	685.603911	11.326861
10.423317	682.042455	11.331879
10.540249	675.223353	11.336896
10.820778	675.229866	11.341914
11.082178	680.156116	11.346931
10.540545	684.737973	11.351949
10.612795	678.809496	11.356967
10.607072	685.645836	11.361984
10.286855	687.198144	11.367002
10.432401	682.132339	11.372019
10.596496	692.328252	11.377037
10.981257	687.101889	11.382055
10.718106	685.432647	11.387072
10.473159	682.832748	11.392090
10.902009	688.587987	11.397107
10.898960	697.128047	11.402125
10.848536	689.934374	11.407143
10.577448	685.760667	11.412160
10.778892	701.823685	11.417178
10.927779	700.976666	11.422195
10.740917	712.136450	11.427213
11.184953	702.479508	11.432231
11.169025	693.611007	11.437248
10.529127	692.344777	11.442266
10.886088	671.555195	11.447283
10.657683	686.732497	11.452301
10.636380	686.903066	11.457319
11.082811	698.739945	11.462336
10.993550	705.109698	11.467354
11.201647	701.668796	11.472371
10.822598	696.508456	11.477389
10.754938	670.145982	11.482407
10.653687	687.032740	11.487424
10.928579	704.081486	11.492442
10.880346	705.114654	11.497459
11.162057	709.381322	11.502477
10.833067	703.263239	11.507495
11.327205	704.741604	11.512512
10.929738	709.916261	11.517530
11.311162	695.765796	11.522547
10.958135	705.664042	11.527565
10.896762	707.974216	11.532583
11.247534	701.273100	11.537600
11.341290	711.741976	11.542618
11.267001	692.869243	11.547635
10.798295	682.809367	11.552653
10.728458	687.727557	11.557671
11.468062	695.564277	11.562688
11.076072	697.907316	11.567706
10.774097	693.533320	11.572723
10.884894	707.104836	11.577741
11.137748	711.174054	11.582759
11.365352	707.827924	11.587776
11.188221	699.953510	11.592794
11.727048	700.743218	11.597811
11.132580	696.232013	11.602829
11.206134	681.713229	11.607847
11.163178	687.791699	11.612864
11.200706	703.864622	11.617882
11.301032	699.913586	11.622899
11.089648	700.066600	11.627917
10.984494	706.164289	11.632935
11.191608	711.102210	11.637952
11.073689	709.394432	11.642970
11.248778	703.370939	11.647987
11.277484	697.768014	11.653005
11.292423	709.653572	11.658023
11.264025	700.720749	11.663040
11.011446	704.619849	11.668058
11.354235	705.124692	11.673075
11.413291	706.137894	11.678093
11.152293	700.804422	11.683111
11.368873	700.701034	11.688128
11.016300	710.330968	11.693146
11.731466	694.600802	11.698163
11.455089	705.705180	11.703181
11.038941	702.510407	11.708199
11.320305	705.975554	11.713216
11.283888	702.396237	11.718234
11.272230	708.706496	11.723251
11.520578	708.323575	11.728269
11.347376	697.078145	11.733287
11.389976	699.589777	11.738304
10.896764	711.400319	11.743322
11.472219	719.073420	11.748339
11.437446	736.353752	11.753357
11.151660	725.031269	11.758375
11.773601	736.114838	11.763392
11.577162	730.739683	11.768410
11.622506	724.342035	11.773427
11.587274	731.214574	11.778445
11.266172	730.901940	11.783463
11.647430	733.966432	11.788480
11.155745	733.746796	11.793498
11.377072	726.501063	11.798515
11.373534	728.111055	11.803533
11.191957	733.403372	11.808551
11.750238	734.821196	11.813568
11.568657	735.417666	11.818586
11.523202	726.405452	11.823603
11.711134	726.754678	11.828621
11.625476	735.105727	11.833639
11.647131	720.737055	11.838656
11.589239	734.675850	11.843674
11.814694	729.004219	11.848691
11.455952	723.831222	11.853709
11.521906	729.854773	11.858727
11.925540	737.535868	11.863744
11.534680	735.050341	11.868762
11.900672	744.286841	11.873779
11.891343	746.367958	11.878797
11.865358	737.523102	11.883815
11.575720	721.297092	11.888832
11.895912	743.703656	11.893850
11.619950	740.726754	11.898867
11.702078	746.886632	11.903885
11.628962	755.797461	11.908903
12.269333	750.966533	11.913920
12.107605	752.888492	11.918938
11.909159	728.017034	11.923955
11.934761	730.973148	11.928973
11.621204	735.228947	11.933991
12.012787	738.588469	11.939008
12.057953	745.798712	11.944026
11.940918	736.122364	11.949043
11.989651	731.923783	11.954061
11.774404	728.047431	11.959079
11.764513	720.140494	11.964096
11.871239	737.581694	11.969114
12.041196	750.799990	11.974131
12.191515	757.776012	11.979149
11.850724	753.670015	11.984167
12.160027	746.779720	11.989184
12.295116	753.227949	11.994202
12.202825	738.088162	11.999219
11.942700	728.440549	12.004237
11.812389	729.076323	12.009255
11.858645	733.465095	12.014272
12.079692	747.293923	12.019290
12.312295	748.699660	12.024307
12.392564	741.479177	12.029325
12.030725	731.172155	12.034343
11.990794	742.741284	12.039360
11.903674	750.382511	12.044378
12.146638	751.152306	12.049395
12.009235	751.438896	12.054413
11.928750	746.667265	12.059431
12.061795	743.525293	12.064448
11.830319	747.957584	12.069466
11.974909	750.364881	12.074483
11.991763	745.170898	12.079501
11.841092	745.494282	12.084519
12.306449	741.069476	12.089536
12.163399	759.275669	12.094554
12.059598	744.074565	12.099571
12.005013	750.117008	12.104589
12.366916	767.534036	12.109607
12.525248	762.756540	12.114624
12.379374	759.898109	12.119642
11.954263	754.107494	12.124659
12.725939	756.151451	12.129677
12.315282	758.210242	12.134695
12.472067	752.896503	12.139712
12.383893	744.907145	12.144730
12.090719	751.138451	12.149747
12.454600	750.920465	12.154765
12.031119	759.823075	12.159783
12.250193	770.546907	12.164800
12.565645	777.004754	12.169818
12.560351	780.631595	12.174835
12.351831	775.482383	12.179853
12.269219	779.664139	12.184871
12.375434	773.765023	12.189888
12.505271	778.964379	12.194906
12.658018	783.008273	12.199923
12.819366	773.909984	12.204941
12.689684	775.637575	12.209959
12.673960	771.701550	12.214976
12.447799	765.504217	12.219994
12.179150	771.195198	12.225011
12.666075	781.337424	12.230029
12.382243	788.542427	12.235047
12.594556	780.092560	12.240064
12.798560	774.370627	12.245082
12.506644	778.938628	12.250099
12.778330	786.378485	12.255117
12.686834	787.812915	12.260135
12.739108	780.379051	12.265152
12.618953	782.925663	12.270170
12.445969	782.356290	12.275187
12.775830	777.946393	12.280205
12.530798	784.914940	12.285223
12.517921	782.550066	12.290240
12.405454	781.690343	12.295258
12.607183	781.586125	12.300275
12.548150	780.282527	12.305293
12.767010	782.460440	12.310311
13.011266	771.247386	12.315328
12.834391	784.655749	12.320346
12.737746	776.083878	12.325363
13.208568	781.037304	12.330381
12.852774	772.313533	12.335399
13.246595	776.117682	12.340416
12.843719	783.126739	12.345434
12.558265	785.241656	12.350451
12.718532	785.999163	12.355469
12.766301	776.249634	12.360487
12.614544	784.942424	12.365504
13.074773	779.451745	12.370522
12.674803	771.246138	12.375539
13.021117	776.888105	12.380557
12.933355	781.111694	12.385575
13.011744	777.867826	12.390592
13.300512	779.353128	12.395610
12.902887	783.126647	12.400627
13.111135	782.595372	12.405645
12.786955	784.586969	12.410663
12.998400	783.215745	12.415680
12.916140	774.726827	12.420698
12.963910	773.949297	12.425715
13.503557	771.614619	12.430733
13.483069	780.413072	12.435751
13.398373	767.604222	12.440768
13.371537	771.575265	12.445786
13.271192	768.908515	12.450803
13.414159	758.961042	12.455821
12.651578	755.574385	12.460839
12.966757	749.970741	12.465856
12.988631	760.596076	12.470874
13.146888	772.213066	12.475891
13.272482	771.581133	12.480909
13.087342	788.695726	12.485927
13.137385	776.749389	12.490944
13.491000	774.630052	12.495962
13.409340	774.769053	12.500979
13.305302	757.904857	12.505997
12.784868	765.380452	12.511015
13.161570	763.459472	12.516032
13.528742	772.692646	12.521050
13.413550	775.784436	12.526067
13.530836	771.893843	12.531085
12.911706	764.337963	12.536103
13.138115	765.309169	12.541120
12.972513	768.566647	12.546138
13.053566	779.012306	12.551155
13.526961	770.486824	12.556173
13.240285	774.829939	12.561191
13.155563	774.682241	12.566208
13.339757	775.458089	12.571226
13.310288	783.197595	12.576243
13.506495	774.478854	12.581261
13.355204	773.047699	12.586279
12.954042	775.348003	12.591296
13.189604	779.811268	12.596314
13.014403	783.246979	12.601331
13.271996	791.733623	12.606349
12.956744	801.512394	12.611367
13.359708	809.042146	12.616384
13.543242	797.674486	12.621402
13.499944	806.359760	12.626419
13.535349	795.479217	12.631437
13.602442	799.012668	12.636455
13.997459	795.299463	12.641472
13.747338	800.473150	12.646490
13.509058	806.755835	12.651507
13.623283	808.132786	12.656525
13.720158	809.802793	12.661543
13.491846	805.552928	12.666560
13.516565	805.145083	12.671578
13.309226	805.966499	12.676595
13.639372	796.930113	12.681613
13.689016	806.938895	12.686631
13.632601	806.808852	12.691648
13.967135	801.180068	12.696666
13.967458	806.181973	12.701683
13.927931	791.084368	12.706701
13.636390	803.873236	12.711719
13.578871	804.456582	12.716736
13.628075	797.607019	12.721754
13.666367	803.177335	12.726771
13.800482	803.456098	12.731789
13.716819	806.318890	12.736807
13.451001	806.985366	12.741824
13.686094	807.686968	12.746842
13.004821	798.329367	12.751859
13.569389	813.470895	12.756877
13.800889	818.367154	12.761895
14.292993	830.553573	12.766912
14.233513	817.106415	12.771930
13.728810	813.632005	12.776947
13.869724	785.352654	12.781965
13.749055	802.176290	12.786983
14.150367	811.946938	12.792000
14.474689	808.790764	12.797018
14.014564	808.266379	12.802035
13.982128	795.869046	12.807053
13.721196	802.363562	12.812071
13.529052	802.283187	12.817088
14.085078	825.536534	12.822106
14.083474	830.759656	12.827123
14.128895	822.714618	12.832141
13.992980	830.066876	12.837159
14.128553	825.718967	12.842176
14.400293	820.232561	12.847194
13.942848	821.187839	12.852211
14.017418	809.767816	12.857229
13.994906	821.971743	12.862247
14.014965	817.421027	12.867264
14.335385	820.147925	12.872282
14.221830	816.116764	12.877299
14.058159	813.586162	12.882317
14.152509	825.008072	12.887335
14.218222	828.952003	12.892352
14.625688	828.979654	12.897370
14.606570	833.113603	12.902387
14.116347	815.637669	12.907405
14.449040	811.340930	12.912423
14.125584	815.083899	12.917440
14.125694	813.247165	12.922458
14.271420	826.633417	12.927475
14.466314	823.320793	12.932493
14.352077	817.875928	12.937511
14.444140	822.759321	12.942528
14.539407	823.586975	12.947546
14.387662	824.772069	12.952563
14.381396	824.574207	12.957581
14.383741	818.265314	12.962599
14.400573	824.230320	12.967616
14.364870	824.775535	12.972634
14.729014	828.530695	12.977651
14.502588	816.444610	12.982669
14.524320	803.846279	12.987687
14.195555	797.478817	12.992704
14.335225	812.507036	12.997722
14.313755	817.925772	13.002739
14.543540	812.789927	13.007757
14.488801	823.200084	13.012775
14.308364	819.580191	13.017792
14.263968	815.714921	13.022810
14.340626	824.267800	13.027827
14.541340	819.145976	13.032845
14.058602	811.275213	13.037863
14.086245	822.758066	13.042880
14.822434	821.209948	13.047898
14.683371	840.627437	13.052915
14.297112	840.040985	13.057933
14.959567	843.418047	13.062951
14.885493	844.840283	13.067968
14.713296	834.998953	13.072986
14.753032	836.185605	13.078003
14.814425	828.040231	13.083021
14.486396	823.831232	13.088039
14.810790	838.912582	13.093056
15.010905	834.134832	13.098074
14.437510	826.139411	13.103091
14.617216	827.985791	13.108109
15.002359	840.176352	13.113127
15.041381	844.503168	13.118144
15.066868	838.499914	13.123162
14.593956	829.567245	13.128179
15.080498	838.349401	13.133197
14.934392	833.812092	13.138215
14.841415	835.000602	13.143232
14.892122	835.617486	13.148250
15.143021	838.478357	13.153267
15.082615	824.958754	13.158285
15.027117	824.490893	13.163303
14.605163	826.052841	13.168320
14.791507	819.752988	13.173338
14.609392	836.157092	13.178355
14.867991	843.277128	13.183373
15.010148	835.381031	13.188391
15.249375	841.282796	13.193408
15.254904	832.025853	13.198426
15.165671	839.616956	13.203443
15.054861	844.200779	13.208461
15.214417	838.905515	13.213479
14.976574	843.455593	13.218496
14.929730	837.646710	13.223514
15.192731	844.298994	13.228531
14.897393	837.108921	13.233549
15.035963	833.180265	13.238567
15.183999	840.667922	13.243584
15.371380	833.149751	13.248602
15.367395	836.937345	13.253619
15.042012	831.067963	13.258637
15.056455	838.604952	13.263655
14.657633	843.054018	13.268672
15.126785	838.533919	13.273690
15.302550	837.793136	13.278707
14.981225	837.057653	13.283725
15.368886	837.375588	13.288743
15.129508	836.661980	13.293760
15.053174	847.091313	13.298778
15.466368	855.114947	13.303795
15.373078	865.903557	13.308813
15.725751	862.042336	13.313831
15.883719	866.763936	13.318848
15.548206	845.249509	13.323866
15.314668	835.417790	13.328883
15.284087	841.749996	13.333901
15.383608	836.419957	13.338919
14.990871	838.315003	13.343936
15.339896	851.366461	13.348954
15.326247	858.668016	13.353971
15.590485	858.572940	13.358989
15.426806	859.046687	13.364007
15.254454	861.696164	13.369024
15.506644	863.042036	13.374042
15.825681	856.784496	13.379059
15.580796	857.466629	13.384077
15.628761	848.180938	13.389095
15.204619	862.022580	13.394112
15.924062	855.080606	13.399130
15.600983	855.285835	13.404147
15.519788	862.187717	13.409165
15.787316	847.392252	13.414183
15.368426	847.524130	13.419200
15.331870	845.289191	13.424218
15.466408	849.424316	13.429235
15.409157	853.958725	13.434253
15.855626	867.667120	13.439271
16.120144	872.996882	13.444288
15.700348	871.734022	13.449306
15.703043	856.819096	13.454323
16.004730	871.585293	13.459341
15.778012	866.492555	13.464359
15.768194	869.978110	13.469376
15.880233	866.754200	13.474394
16.055398	864.220995	13.479411
15.727738	866.323600	13.484429
15.938211	870.964390	13.489447
16.210109	872.433408	13.494464
16.128357	863.351071	13.499482
16.219920	859.407685	13.504499
16.100180	859.410640	13.509517
15.958318	851.511698	13.514535
15.682054	857.462677	13.519552
15.685539	847.379218	13.524570
15.833825	855.649488	13.529587
15.803183	878.130125	13.534605
16.429287	869.804733	13.539623
15.944136	880.642125	13.544640
15.917033	879.374543	13.549658
15.976308	884.013779	13.554675
16.198320	884.597512	13.559693
16.383103	878.215832	13.564711
16.173435	881.978857	13.569728
16.425571	879.802823	13.574746
16.190839	887.744951	13.579763
16.069725	881.521652	13.584781
16.252001	877.803892	13.589799
16.249550	886.643753	13.594816
15.831054	881.069813	13.599834
15.943192	879.357532	13.604851
15.829241	882.957236	13.609869
15.872505	881.577641	13.614887
16.063325	880.219109	13.619904
16.035917	877.424149	13.624922
16.155279	878.361640	13.629939
16.072618	891.613309	13.634957
16.412996	899.096100	13.639975
16.679227	914.464341	13.644992
16.648686	890.367935	13.650010
16.320359	883.757374	13.655027
16.196299	892.401695	13.660045
16.565072	896.093028	13.665063
16.541337	900.912534	13.670080
16.824560	901.104820	13.675098
16.630368	882.036076	13.680115
16.480697	886.976297	13.685133
16.538684	877.521761	13.690151
16.363968	874.850868	13.695168
16.141783	877.574427	13.700186
16.549585	887.624969	13.705203
16.609351	899.402642	13.710221
16.864111	901.597036	13.715239
16.318788	904.121917	13.720256
16.609222	901.005751	13.725274
16.744757	902.079567	13.730291
16.735005	900.518927	13.735309
16.742472	904.910663	13.740327
16.880656	904.535531	13.745344
16.548185	906.638894	13.750362
16.839894	902.683074	13.755379
16.389813	897.230844	13.760397
17.023575	900.950088	13.765415
17.014025	910.523228	13.770432
16.614008	907.739306	13.775450
17.143133	910.869025	13.780467
16.989361	901.570732	13.785485
17.011339	895.747891	13.790503
16.632497	892.499901	13.795520
16.528377	901.866945	13.800538
16.774858	899.890614	13.805555
16.554309	901.263220	13.810573
16.808986	905.335353	13.815591
16.873438	899.619466	13.820608
16.859832	901.919024	13.825626
17.298942	906.631300	13.830643
16.509400	905.202304	13.835661
16.861037	891.450832	13.840679
16.990204	896.713445	13.845696
16.775536	899.789284	13.850714
16.756037	895.923251	13.855731
16.762218	902.246563	13.860749
16.775743	901.360782	13.865767
16.827982	916.011462	13.870784
17.160981	919.661067	13.875802
17.282753	925.609666	13.880819
17.387914	925.242864	13.885837
17.456068	924.307497	13.890855
17.125046	916.671696	13.895872
17.230843	909.904743	13.900890
17.306827	897.796468	13.905907
17.401486	907.107124	13.910925
17.205931	903.158220	13.915943
17.142625	904.840709	13.920960
17.040957	905.670819	13.925978
17.104914	913.342095	13.930995
17.189986	928.363186	13.936013
17.136985	925.035734	13.941031
17.335933	932.856284	13.946048
17.884999	934.575375	13.951066
17.940658	927.854141	13.956083
17.578992	921.024724	13.961101
17.482678	906.873205	13.966119
17.172895	904.630573	13.971136
17.123602	906.711659	13.976154
17.584524	899.642913	13.981171
17.483042	923.182446	13.986189
17.442879	929.014404	13.991207
17.756297	926.522646	13.996224
17.440053	923.523622	14.001242
17.422123	921.863274	14.006259
17.348300	929.833859	14.011277
17.587621	927.218009	14.016295
17.568641	927.230424	14.021312
17.475749	927.175523	14.026330
17.808978	919.041166	14.031347
17.550553	919.655993	14.036365
17.735815	924.502722	14.041383
17.632837	920.684477	14.046400
17.700561	925.950414	14.051418
17.877840	921.330856	14.056435
17.899560	929.059250	14.061453
17.732013	932.351776	14.066471
17.953436	923.218752	14.071488
17.634872	929.775993	14.076506
17.817816	924.937793	14.081523
17.336016	922.441241	14.086541
17.493553	919.689882	14.091559
17.664441	926.142032	14.096576
17.274173	928.219739	14.101594
17.609782	914.896799	14.106611
17.656574	933.603608	14.111629
17.609594	944.949906	14.116647
18.113409	942.712341	14.121664
18.016167	955.631822	14.126682
18.209099	944.710728	14.131699
18.053079	942.472403	14.136717
18.192201	944.924765	14.141735
18.173305	927.671522	14.146752
18.021245	929.052334	14.151770
18.210346	925.579651	14.156787
17.761573	927.764356	14.161805
18.111279	922.581288	14.166823
18.117273	913.463087	14.171840
17.730797	925.692552	14.176858
18.133437	933.891447	14.181875
18.482198	940.003304	14.186893
18.488618	941.359287	14.191911
17.871191	936.561278	14.196928
17.907515	931.752361	14.201946
18.385384	943.581322	14.206963
18.339748	948.817689	14.211981
18.463668	946.838464	14.216999
18.504040	947.826205	14.222016
18.185099	931.412088	14.227034
18.457618	926.944866	14.232051
18.046099	927.495317	14.237069
18.171539	939.786598	14.242087
18.315605	941.114703	14.247104
18.248004	947.111915	14.252122
18.491627	944.015699	14.257139
18.381373	948.766722	14.262157
18.553331	953.079048	14.267175
18.865137	935.862347	14.272192
18.606487	942.053595	14.277210
18.541038	940.328106	14.282227
18.299513	934.496044	14.287245
18.522215	942.041473	14.292263
18.809541	941.513583	14.297280
18.641610	950.272105	14.302298
18.552582	934.582522	14.307315
18.278142	942.862259	14.312333
18.266259	951.119798	14.317351
18.537288	948.776692	14.322368
18.336527	948.397861	14.327386
18.519351	945.083950	14.332403
18.393554	949.076848	14.337421
18.182367	949.248768	14.342439
18.802520	945.361401	14.347456
18.630329	948.108696	14.352474
18.754164	940.101812	14.357491
18.826464	943.268398	14.362509
18.623452	951.666338	14.367527
18.948506	944.924980	14.372544
18.924399	947.068397	14.377562
18.662158	939.497550	14.382579
18.759209	951.080065	14.387597
18.781416	968.092914	14.392615
19.186657	961.477844	14.397632
18.731521	969.546060	14.402650
19.053311	962.921974	14.407667
18.840719	976.159349	14.412685
19.273001	974.873433	14.417703
19.154868	967.813334	14.422720
18.635578	971.258811	14.427738
18.899355	971.239547	14.432755
19.287708	971.260726	14.437773
19.037605	971.896342	14.442791
19.258673	964.117214	14.447808
19.022760	969.070970	14.452826
19.028423	974.292995	14.457843
19.412125	968.656456	14.462861
18.949946	976.063050	14.467879
19.029406	969.183434	14.472896
18.891205	967.851200	14.477914
18.568203	966.396440	14.482931
18.929273	964.133900	14.487949
18.767816	965.288966	14.492967
19.008276	965.314381	14.497984
19.014944	982.844083	14.503002
19.359360	979.697355	14.508019
19.501818	983.386295	14.513037
19.561189	992.109223	14.518055
19.445260	972.946067	14.523072
19.098461	963.946232	14.528090
19.025634	983.814254	14.533107
19.561028	998.569185	14.538125
19.577269	996.739372	14.543143
19.791813	986.622766	14.548160
19.405058	991.069978	14.553178
19.774655	986.287725	14.558195
19.755688	976.015203	14.563213
19.324336	970.064546	14.568231
19.537436	962.406590	14.573248
19.638287	966.603826	14.578266
19.598971	959.200018	14.583283
19.486358	956.699266	14.588301
19.329690	970.502240	14.593319
19.426494	977.234264	14.598336
19.504641	984.950684	14.603354
19.441000	992.645142	14.608371
19.783120	994.305143	14.613389
19.278095	996.359812	14.618407
19.500279	998.530919	14.623424
19.380661	993.370870	14.628442
19.522061	989.558504	14.633459
19.853163	993.164240	14.638477
19.590847	998.778560	14.643495
19.606897	994.124283	14.648512
19.945009	1000.594442	14.653530
19.953796	1012.392801	14.658547
19.988435	1005.182517	14.663565
19.968865	1000.603249	14.668583
20.226774	997.791969	14.673600
19.883573	999.758166	14.678618
19.767503	990.920987	14.683635
19.979749	993.522847	14.688653
19.990434	1004.942201	14.693671
20.133013	1005.825567	14.698688
20.242027	999.679781	14.703706
19.925157	1000.489964	14.708723
20.460774	986.807424	14.713741
20.271891	986.603459	14.718759
20.209209	989.387252	14.723776
20.041932	984.869000	14.728794
19.890880	981.026717	14.733811
20.085173	985.338707	14.738829
19.850466	1006.686968	14.743847
19.977668	1006.480816	14.748864
20.346990	1012.081383	14.753882
20.246547	1014.732238	14.758899
20.714823	1016.053734	14.763917
20.343040	1012.564770	14.768935
20.459292	1003.056856	14.773952
20.742801	999.054962	14.778970
20.154411	994.725766	14.783987
20.536987	980.230908	14.789005
20.233140	982.777926	14.794023
20.458681	977.809960	14.799040
19.903784	982.365566	14.804058
20.319856	1005.170854	14.809075
20.504656	1004.747391	14.814093
20.126457	1017.082921	14.819111
20.389127	1006.245538	14.824128
20.132017	1009.993932	14.829146
20.309639	1005.333272	14.834163
20.587239	999.258904	14.839181
20.299787	1016.459174	14.844199
20.347781	1000.918481	14.849216
20.518168	1008.592057	14.854234
20.755591	1006.576107	14.859251
20.514155	1004.834004	14.864269
20.619404	1014.982516	14.869287
20.592660	1007.867056	14.874304
20.798777	1018.665653	14.879322
20.842497	1039.244480	14.884339
20.983496	1022.344797	14.889357
20.527861	1020.289108	14.894375
20.762950	1017.598168	14.899392
20.752329	1013.071144	14.904410
20.884047	1031.404980	14.909427
20.886342	1025.623051	14.914445
21.048038	1031.230908	14.919463
20.919217	1025.027701	14.924480
20.767198	1021.621070	14.929498
20.999029	1035.704057	14.934515
21.042824	1024.503317	14.939533
20.903291	1036.517439	14.944551
21.057816	1025.050036	14.949568
20.537583	1022.250216	14.954586
21.037905	1032.570372	14.959603
21.248640	1023.877636	14.964621
21.053314	1024.163839	14.969639
20.986427	1021.251963	14.974656
20.914808	1024.384307	14.979674
21.032327	1030.721778	14.984691
21.480051	1027.202243	14.989709
21.043197	1029.896341	14.994727
21.377084	1022.809581	14.999744
21.454356	1025.224307	15.004762
21.323148	1021.871220	15.009779
21.175242	1017.930604	15.014797
20.962512	1029.943566	15.019815
21.278528	1028.679019	15.024832
21.349401	1029.144424	15.029850
21.325544	1035.062226	15.034867
21.248118	1027.582308	15.039885
21.294709	1029.168693	15.044903
21.425023	1028.725364	15.049920
21.571913	1025.262431	15.054938
20.889444	1035.976195	15.059955
21.596001	1025.356436	15.064973
21.530479	1025.912640	15.069991
21.260713	1020.987552	15.075008
21.585215	1026.901265	15.080026
21.439117	1030.458697	15.085043
21.480327	1046.439831	15.090061
21.508542	1043.958029	15.095079
21.628881	1057.695578	15.100096
21.933529	1046.040535	15.105114
21.846735	1060.501674	15.110131
21.909877	1039.031852	15.115149
21.438603	1029.139442	15.120167
21.478599	1045.411106	15.125184
21.629332	1049.436441	15.130202
21.331995	1052.209671	15.135219
22.013688	1046.012012	15.140237
22.136492	1048.621583	15.145255
22.127676	1049.462399	15.150272
22.000039	1049.864231	15.155290
21.709332	1050.701875	15.160307
21.968215	1048.297542	15.165325
21.942659	1051.416362	15.170343
21.910896	1041.089002	15.175360
22.037937	1051.038456	15.180378
21.782976	1050.270475	15.185395
22.172378	1042.218781	15.190413
21.967667	1050.800073	15.195431
21.984432	1053.694508	15.200448
22.240051	1046.064568	15.205466
22.173027	1042.572031	15.210483
22.557247	1045.314215	15.215501
22.280264	1029.388905	15.220519
21.892278	1021.326475	15.225536
21.766744	1020.086928	15.230554
21.918907	1041.983697	15.235571
22.044764	1039.982068	15.240589
21.812657	1050.142430	15.245607
21.859624	1045.846221	15.250624
22.044755	1048.184089	15.255642
22.032146	1052.976646	15.260659
22.118359	1043.280910	15.265677
22.250552	1044.850728	15.270695
21.655179	1046.143214	15.275712
22.356553	1062.778338	15.280730
22.371697	1076.608124	15.285747
22.316554	1070.510124	15.290765
22.573322	1073.619428	15.295783
22.003474	1074.939476	15.300800
22.783545	1065.617862	15.305818
22.238257	1076.587873	15.310835
22.391663	1076.765787	15.315853
22.666982	1078.464666	15.320871
22.357311	1074.057067	15.325888
22.829356	1077.041121	15.330906
22.371754	1076.986557	15.335923
22.310882	1069.308363	15.340941
22.715303	1070.119149	15.345959
22.406171	1070.833446	15.350976
22.574310	1069.326972	15.355994
22.748512	1092.668896	15.361011
22.797615	1091.370423	15.366029
22.937296	1081.596859	15.371047
22.688347	1094.448690	15.376064
23.027364	1087.793455	15.381082
22.693986	1092.330161	15.386099
23.151692	1090.652081	15.391117
22.951026	1085.372158	15.396135
23.083559	1069.164894	15.401152
23.101253	1064.216846	15.406170
22.816814	1075.597276	15.411187
22.955344	1069.838169	15.416205
23.031494	1066.376845	15.421223
23.061266	1063.986315	15.426240
23.326700	1063.872116	15.431258
23.145399	1066.238996	15.436275
22.948096	1069.192220	15.441293
22.758479	1064.895203	15.446311
22.631782	1068.758879	15.451328
22.787646	1079.407592	15.456346
23.257805	1091.294666	15.461363
22.905727	1091.343491	15.466381
23.152043	1089.711155	15.471399
22.938050	1096.551881	15.476416
23.116357	1092.664281	15.481434
22.854566	1091.660677	15.486451
22.901457	1079.825087	15.491469
23.419912	1094.071500	15.496487
23.226407	1115.716399	15.501504
23.747560	1117.941667	15.506522
23.568359	1106.703230	15.511539
23.669337	1098.254878	15.516557
23.557884	1085.093378	15.521575
23.109178	1087.760939	15.526592
23.463568	1090.539363	15.531610
23.240410	1094.765304	15.536627
23.531724	1094.183136	15.541645
23.738842	1118.160579	15.546663
23.835056	1108.980804	15.551680
23.614039	1095.886957	15.556698
23.430897	1101.293239	15.561715
23.549784	1110.028991	15.566733
23.910398	1112.755949	15.571751
23.867982	1117.108215	15.576768
23.778744	1109.740568	15.581786
23.529435	1096.168304	15.586803
23.927748	1098.513804	15.591821
23.968318	1101.884210	15.596839
23.552162	1095.230525	15.601856
23.955899	1098.054869	15.606874
23.592085	1101.696921	15.611891
24.216162	1113.077043	15.616909
23.990783	1106.996236	15.621927
24.197900	1100.629913	15.626944
23.918770	1081.514301	15.631962
23.710611	1086.088192	15.636979
24.020900	1092.865707	15.641997
23.964252	1104.952097	15.647015
23.959985	1113.577755	15.652032
24.044540	1115.107706	15.657050
24.173287	1110.107531	15.662067
24.000247	1104.924261	15.667085
24.097025	1107.440086	15.672103
24.103666	1113.271083	15.677120
24.074303	1107.118538	15.682138
24.331453	1103.486833	15.687155
23.972478	1109.416139	15.692173
24.302154	1103.494526	15.697191
24.113376	1109.485531	15.702208
24.029008	1099.857517	15.707226
24.098429	1103.658914	15.712243
24.181508	1105.362668	15.717261
24.432481	1099.336620	15.722279
24.662680	1104.725480	15.727296
24.509066	1103.433521	15.732314
24.363246	1096.813220	15.737331
24.319369	1103.873454	15.742349
24.516187	1105.281670	15.747367
24.182208	1103.109078	15.752384
24.049329	1098.178300	15.757402
24.652992	1110.852374	15.762419
24.359396	1120.239752	15.767437
24.649447	1121.544997	15.772455
24.651228	1130.684125	15.777472
24.490006	1128.153094	15.782490
24.725903	1126.421399	15.787507
24.900032	1127.899446	15.792525
25.187721	1124.528046	15.797543
24.753907	1135.871957	15.802560
24.889852	1126.736442	15.807578
25.017513	1135.022696	15.812595
24.643613	1121.858107	15.817613
24.674732	1114.424263	15.822631
24.416068	1129.818125	15.827648
24.649214	1122.472547	15.832666
25.042174	1123.133649	15.837683
24.816491	1128.985272	15.842701
24.970392	1127.963874	15.847719
24.906879	1121.292799	15.852736
24.855732	1120.451854	15.857754
25.117011	1126.943565	15.862771
25.262139	1137.268939	15.867789
25.309686	1125.830857	15.872807
25.200643	1133.709218	15.877824
25.203017	1127.128805	15.882842
25.157820	1127.852245	15.887859
25.289433	1122.892643	15.892877
25.172424	1124.902311	15.897895
24.977197	1138.660962	15.902912
25.043890	1129.965496	15.907930
25.053526	1132.157298	15.912947
24.580598	1131.754832	15.917965
25.150873	1128.926149	15.922983
25.070473	1142.136624	15.928000
25.511967	1154.943438	15.933018
25.412966	1153.207406	15.938035
25.313153	1151.815493	15.943053
25.448844	1146.820531	15.948071
25.301181	1156.494340	15.953088
25.415876	1151.174454	15.958106
25.558501	1153.471658	15.963123
25.427228	1153.018816	15.968141
25.670261	1152.191740	15.973159
25.444163	1162.076662	15.978176
25.783037	1156.144123	15.983194
25.618871	1153.515718	15.988211
25.564007	1157.330287	15.993229
25.798908	1151.180504	15.998247
25.676121	1161.753002	16.003264
25.693915	1157.887381	16.008282
25.789316	1155.038421	16.013299
25.679987	1155.794002	16.018317
25.649350	1152.614486	16.023335
25.376321	1152.496288	16.028352
25.792159	1151.001492	16.033370
25.864849	1150.617682	16.038387
25.649334	1147.672267	16.043405
26.005361	1156.162598	16.048423
25.986786	1169.682151	16.053440
26.000519	1163.680628	16.058458
25.819420	1170.124898	16.063475
26.322776	1163.718449	16.068493
26.530436	1156.913353	16.073511
26.182567	1150.239480	16.078528
26.181705	1141.797596	16.083546
26.240461	1135.940511	16.088563
25.866947	1141.234618	16.093581
26.291231	1152.772306	16.098599
26.417046	1159.408332	16.103616
26.197109	1157.826951	16.108634
26.341497	1154.247618	16.113651
26.174069	1165.407795	16.118669
26.723482	1165.416364	16.123687
26.412704	1165.988908	16.128704
26.250074	1157.720689	16.133722
26.621527	1155.664787	16.138739
26.470988	1150.358055	16.143757
26.425484	1139.941270	16.148775
26.341066	1149.646193	16.153792
26.514614	1158.701617	16.158810
26.638031	1152.184283	16.163827
26.418465	1160.117843	16.168845
26.644776	1152.770168	16.173863
26.341166	1162.515752	16.178880
26.482852	1163.484476	16.183898
26.709405	1162.278119	16.188915
26.342724	1163.522158	16.193933
26.441969	1158.327770	16.198951
26.459386	1169.963931	16.203968
26.301831	1156.462454	16.208986
26.584459	1164.071173	16.214003
26.610141	1166.658107	16.219021
26.965806	1165.403118	16.224039
26.744552	1186.970398	16.229056
26.554494	1189.319731	16.234074
26.923429	1178.408789	16.239091
27.150039	1188.203860	16.244109
27.028114	1176.533514	16.249127
27.269209	1185.783502	16.254144
27.069287	1191.400729	16.259162
27.051672	1187.184034	16.264179
26.986104	1189.965154	16.269197
27.170025	1184.902663	16.274215
27.133975	1185.709882	16.279232
27.029107	1179.679598	16.284250
27.207784	1180.188078	16.289267
27.198230	1182.076772	16.294285
27.299496	1170.276784	16.299303
27.008694	1179.196684	16.304320
27.401236	1176.642001	16.309338
27.519434	1184.623640	16.314355
27.285237	1179.285824	16.319373
27.182514	1179.222995	16.324391
27.103636	1185.970000	16.329408
27.079975	1178.456347	16.334426
27.204832	1175.470221	16.339443
27.218833	1178.336706	16.344461
27.363273	1179.996139	16.349479
27.061141	1187.854282	16.354496
27.101772	1204.141770	16.359514
27.946131	1205.420136	16.364531
27.297026	1200.655421	16.369549
27.206311	1209.061133	16.374567
27.561522	1208.718266	16.379584
27.541594	1209.554519	16.384602
28.214540	1200.379013	16.389619
27.781811	1212.530711	16.394637
27.955169	1206.368461	16.399655
27.727328	1200.928654	16.404672
28.039587	1200.358981	16.409690
28.111230	1210.405569	16.414707
27.859998	1201.949234	16.419725
27.928525	1197.494971	16.424743
28.377958	1205.121756	16.429760
28.230032	1213.394419	16.434778
28.096449	1214.993271	16.439795
27.957173	1207.463006	16.444813
28.099573	1203.372719	16.449831
28.378760	1193.078605	16.454848
27.831867	1200.599552	16.459866
28.289461	1199.385397	16.464883
28.238359	1205.291745	16.469901
28.205835	1198.407496	16.474919
28.429706	1202.995779	16.479936
28.414144	1200.015871	16.484954
28.299981	1189.704491	16.489971
28.374760	1200.104042	16.494989
28.191101	1207.602795	16.500007
28.559972	1203.880980	16.505024
28.588376	1207.862400	16.510042
28.448473	1190.470067	16.515059
28.394683	1202.606570	16.520077
28.219708	1196.372663	16.525095
28.441935	1191.853294	16.530112
28.211756	1193.438876	16.535130
28.533329	1198.608314	16.540147
28.202466	1198.524424	16.545165
28.082587	1201.140481	16.550183
28.488839	1198.526841	16.555200
27.919203	1209.216717	16.560218
28.550666	1203.718016	16.565235
28.397094	1217.725829	16.570253
28.517685	1225.195855	16.575271
28.359872	1222.465455	16.580288
28.255148	1233.669501	16.585306
28.243102	1219.810652	16.590323
28.309423	1221.479173	16.595341
28.867489	1237.963340	16.600359
29.083670	1242.117324	16.605376
28.781740	1248.069297	16.610394
29.236044	1239.761186	16.615411
29.194195	1254.089204	16.620429
29.126593	1235.505192	16.625447
29.333330	1227.772378	16.630464
28.985223	1227.549173	16.635482
29.033018	1215.830119	16.640499
28.931913	1222.574309	16.645517
29.164734	1228.928500	16.650535
29.648486	1232.254740	16.655552
29.257667	1232.606290	16.660570
29.554078	1219.712157	16.665587
29.139425	1214.301615	16.670605
29.248800	1213.855250	16.675623
29.439534	1217.612417	16.680640
29.230245	1225.503369	16.685658
29.530848	1223.673161	16.690675
29.461711	1244.490820	16.695693
29.355226	1234.209771	16.700711
29.352596	1241.699111	16.705728
29.587173	1237.916276	16.710746
29.676269	1241.055036	16.715763
29.643246	1241.366306	16.720781
29.261154	1238.368077	16.725799
29.944281	1234.063671	16.730816
29.663440	1242.287743	16.735834
29.825150	1229.288471	16.740851
29.668507	1237.467834	16.745869
29.593994	1237.832944	16.750887
29.495387	1233.382767	16.755904
29.668755	1239.171904	16.760922
30.301407	1225.963144	16.765939
30.071068	1230.000888	16.770957
30.016318	1229.738032	16.775975
30.032837	1226.500620	16.780992
29.864242	1237.850380	16.786010
30.292619	1231.389381	16.791027
30.091090	1233.803635	16.796045
29.888484	1235.593189	16.801063
29.925642	1230.402197	16.806080
29.863158	1235.347789	16.811098
29.982559	1231.308437	16.816115
30.054892	1239.549759	16.821133
30.193343	1236.949669	16.826151
30.429912	1229.398378	16.831168
30.117413	1232.972454	16.836186
30.324242	1239.378061	16.841203
30.242800	1233.296749	16.846221
30.063370	1235.754880	16.851239
30.197846	1231.059895	16.856256
29.804796	1235.656480	16.861274
30.145409	1233.100458	16.866291
30.346201	1237.260008	16.871309
30.038046	1250.528338	16.876327
30.371959	1259.877434	16.881344
30.356600	1261.192671	16.886362
30.704781	1262.952738	16.891379
30.603052	1256.836727	16.896397
30.572337	1257.662048	16.901415
30.607217	1256.599329	16.906432
30.293488	1254.726511	16.911450
30.230975	1255.881873	16.916467
30.457273	1256.477571	16.921485
30.338656	1254.002965	16.926503
30.521073	1256.442275	16.931520
30.725819	1271.075664	16.936538
30.877539	1283.615538	16.941555
30.522138	1279.593761	16.946573
30.744939	1289.320054	16.951591
31.072781	1271.917476	16.956608
30.639126	1281.633005	16.961626
31.279859	1283.902677	16.966643
31.343861	1283.157296	16.971661
31.236585	1274.883506	16.976679
31.081136	1274.901524	16.981696
30.761216	1280.278795	16.986714
31.163711	1277.069266	16.991731
31.258527	1275.182930	16.996749
31.005925	1278.861244	17.001767
31.297709	1278.004433	17.006784
31.352509	1273.650135	17.011802
31.441550	1267.709364	17.016819
31.500323	1269.943979	17.021837
31.349963	1270.895348	17.026855
31.297472	1267.823381	17.031872
31.327745	1274.480731	17.036890
31.163180	1271.571495	17.041907
31.229131	1273.767115	17.046925
31.040783	1272.900321	17.051943
31.508996	1276.109080	17.056960
31.756605	1295.425453	17.061978
31.841672	1294.228632	17.066995
31.748428	1301.703791	17.072013
31.505907	1300.394188	17.077031
31.793134	1294.119389	17.082048
31.962121	1293.499575	17.087066
32.169023	1289.291862	17.092083
32.037981	1268.063635	17.097101
31.791531	1267.130202	17.102119
31.890729	1258.830381	17.107136
31.869604	1261.632953	17.112154
31.818128	1261.659927	17.117171
31.600745	1265.856600	17.122189
32.111928	1286.788519	17.127207
32.194862	1293.917324	17.132224
32.024146	1291.125817	17.137242
32.292948	1293.062431	17.142259
32.103974	1288.743168	17.147277
31.939209	1297.346723	17.152295
31.778822	1300.827550	17.157312
31.972224	1287.283610	17.162330
32.256938	1296.081837	17.167347
32.016547	1293.929272	17.172365
32.013389	1292.216081	17.177383
32.251868	1281.278178	17.182400
31.916855	1287.557250	17.187418
31.985185	1280.720286	17.192435
32.588262	1290.557418	17.197453
32.311162	1305.828083	17.202471
32.537561	1300.241334	17.207488
32.395877	1307.777736	17.212506
32.481163	1311.485169	17.217523
32.953285	1310.732650	17.222541
32.498433	1316.670735	17.227559
32.421617	1309.455700	17.232576
32.627441	1312.105952	17.237594
32.592613	1313.888163	17.242611
32.549951	1305.477998	17.247629
32.335304	1319.160932	17.252647
32.471951	1307.989650	17.257664
32.580984	1308.019879	17.262682
32.802934	1307.697890	17.267699
32.845206	1309.165052	17.272717
32.740355	1313.138970	17.277735
32.991973	1325.508582	17.282752
33.118330	1335.559291	17.287770
33.093909	1348.372969	17.292787
33.423275	1339.683585	17.297805
33.161475	1322.853041	17.302823
33.256420	1310.236569	17.307840
33.094818	1314.863186	17.312858
33.279590	1312.811268	17.317875
33.390280	1311.878684	17.322893
33.380811	1312.527104	17.327911
33.577144	1304.881096	17.332928
33.349248	1311.932373	17.337946
33.456810	1317.040700	17.342963
33.680334	1305.025801	17.347981
33.353793	1304.827620	17.352999
33.353915	1293.990172	17.358016
33.226658	1308.363174	17.363034
32.966448	1302.887381	17.368051
33.477317	1305.859080	17.373069
33.551531	1319.531472	17.378087
33.619399	1325.804242	17.383104
33.592768	1325.937780	17.388122
33.267519	1313.112577	17.393139
33.560701	1319.510994	17.398157
34.014326	1327.544289	17.403175
33.848218	1320.021335	17.408192
33.975123	1315.513714	17.413210
34.130864	1319.588821	17.418227
33.849492	1323.306366	17.423245
33.953656	1327.944996	17.428263
33.630642	1323.043946	17.433280
33.942294	1323.496881	17.438298
33.522264	1320.271044	17.443315
33.757389	1314.547219	17.448333
33.757439	1332.491726	17.453351
33.855856	1340.716384	17.458368
33.956844	1344.869505	17.463386
34.096758	1352.172450	17.468403
34.391221	1347.035787	17.473421
34.602943	1350.291058	17.478439
34.383377	1346.449962	17.483456
34.383463	1340.598847	17.488474
34.286250	1348.103050	17.493491
34.459643	1345.942455	17.498509
34.652621	1342.443837	17.503527
34.657814	1350.102416	17.508544
34.893795	1342.241890	17.513562
34.310302	1349.831751	17.518579
34.560257	1342.874784	17.523597
34.345727	1344.139179	17.528615
34.307880	1341.699245	17.533632
34.581548	1346.948819	17.538650
34.297432	1347.390953	17.543667
34.500883	1346.882506	17.548685
34.439959	1342.293850	17.553703
34.860575	1342.612945	17.558720
34.894151	1341.594607	17.563738
34.671877	1339.322429	17.568755
34.822298	1337.796618	17.573773
34.772891	1349.500172	17.578791
34.884116	1357.331497	17.583808
34.778306	1364.502526	17.588826
34.795673	1370.896837	17.593843
34.998254	1364.007248	17.598861
35.009530	1376.171544	17.603879
34.972777	1374.321592	17.608896
35.290231	1366.808066	17.613914
35.073036	1362.499518	17.618931
35.110453	1368.120642	17.623949
35.176597	1367.583213	17.628967
35.493287	1360.101368	17.633984
35.600986	1368.144697	17.639002
35.154488	1360.567824	17.644019
35.306689	1365.953204	17.649037
34.985900	1363.437672	17.654055
35.257466	1362.634520	17.659072
35.646760	1359.556437	17.664090
34.975990	1366.863323	17.669107
35.689835	1380.669084	17.674125
35.817100	1390.618693	17.679143
35.588144	1389.313269	17.684160
35.561961	1385.773239	17.689178
35.167161	1394.703227	17.694195
35.923223	1383.068761	17.699213
35.933131	1387.068898	17.704231
35.807198	1375.922934	17.709248
36.298962	1376.723207	17.714266
35.731475	1389.694587	17.719283
36.004826	1387.887569	17.724301
36.336215	1386.491197	17.729319
36.135403	1378.266728	17.734336
36.069442	1381.827454	17.739354
35.809839	1381.543041	17.744371
36.061464	1382.365159	17.749389
36.105259	1397.459387	17.754407
36.227455	1382.708343	17.759424
36.106086	1379.959585	17.764442
36.223182	1390.582999	17.769459
36.150908	1386.677790	17.774477
35.840700	1384.798095	17.779495
36.278692	1381.788121	17.784512
35.829522	1388.315497	17.789530
36.273794	1399.676637	17.794547
36.496897	1405.180314	17.799565
36.500984	1402.654902	17.804583
36.655878	1407.787399	17.809600
36.919443	1414.654413	17.814618
36.428200	1416.624913	17.819635
36.429744	1406.790761	17.824653
36.689225	1402.161356	17.829671
36.651118	1407.936342	17.834688
36.773252	1408.911298	17.839706
36.602876	1405.646330	17.844723
36.591702	1405.430295	17.849741
36.846886	1404.907430	17.854759
36.514142	1404.921666	17.859776
37.149577	1400.940286	17.864794
37.013730	1407.910904	17.869811
36.369159	1402.564731	17.874829
36.694301	1415.585631	17.879847
36.731902	1432.167303	17.884864
36.987586	1424.445671	17.889882
36.821403	1429.678974	17.894899
37.142810	1432.645665	17.899917
37.192962	1429.895273	17.904935
37.025412	1432.944884	17.909952
37.156240	1426.366327	17.914970
37.104838	1420.043550	17.919987
37.290711	1425.628808	17.925005
37.178906	1431.964481	17.930023
37.540643	1447.245632	17.935040
38.000160	1444.156533	17.940058
37.219289	1433.548667	17.945075
37.691068	1424.313044	17.950093
37.579722	1425.668579	17.955111
37.147184	1433.550418	17.960128
37.790801	1445.483138	17.965146
37.909719	1458.662618	17.970163
37.975913	1451.829079	17.975181
37.522022	1445.774490	17.980199
38.080673	1449.388852	17.985216
38.573566	1445.164697	17.990234
37.888918	1435.750478	17.995251
37.758374	1428.906745	18.000269
37.976451	1428.648479	18.005287
37.691415	1417.028780	18.010304
37.958736	1430.705716	18.015322
38.132704	1447.707868	18.020339
38.187023	1448.807066	18.025357
38.162890	1442.448449	18.030375
37.877899	1448.905941	18.035392
38.175045	1452.520248	18.040410
38.002871	1449.855181	18.045427
38.213917	1443.996227	18.050445
38.047433	1449.614607	18.055463
38.232371	1454.508870	18.060480
38.044840	1449.854812	18.065498
37.964511	1454.364585	18.070515
38.376876	1451.964555	18.075533
38.421120	1458.253697	18.080551
38.537007	1465.954945	18.085568
38.774384	1454.029299	18.090586
38.740904	1463.587550	18.095603
38.847776	1468.800174	18.100621
39.096338	1467.849137	18.105639
38.840221	1470.843200	18.110656
39.092318	1465.384923	18.115674
38.815690	1447.631893	18.120691
38.748896	1449.223457	18.125709
39.003722	1443.865750	18.130727
38.985565	1458.897150	18.135744
39.100101	1446.432154	18.140762
39.224843	1453.096862	18.145779
39.040131	1449.000963	18.150797
38.892808	1442.800509	18.155815
39.091608	1463.573288	18.160832
39.135545	1464.276464	18.165850
38.957897	1472.986268	18.170867
38.907371	1467.903623	18.175885
39.280797	1463.019655	18.180903
39.002692	1459.762087	18.185920
39.215813	1465.784920	18.190938
38.983759	1460.620261	18.195955
39.073487	1469.985634	18.200973
39.435836	1470.585272	18.205991
39.530901	1491.077677	18.211008
39.639363	1485.632431	18.216026
39.580486	1494.471965	18.221043
39.569818	1488.755036	18.226061
39.418116	1484.685517	18.231079
39.179078	1483.870838	18.236096
39.306321	1486.173651	18.241114
39.201334	1483.785244	18.246131
38.921814	1494.685465	18.251149
39.730890	1502.944027	18.256167
39.734469	1514.257517	18.261184
39.559724	1515.664020	18.266202
39.912491	1515.766521	18.271219
39.579889	1516.768546	18.276237
39.997107	1506.806093	18.281255
39.789696	1510.063944	18.286272
39.962656	1522.244035	18.291290
40.217470	1534.868923	18.296307
40.453855	1538.824142	18.301325
40.514702	1531.571669	18.306343
40.135131	1526.480598	18.311360
40.330941	1525.023402	18.316378
40.409106	1536.568229	18.321395
40.354762	1535.702518	18.326413
40.413915	1532.051253	18.331431
40.572332	1537.410464	18.336448
40.647137	1529.600356	18.341466
40.911825	1527.608480	18.346483
40.898939	1526.114552	18.351501
41.203873	1522.285919	18.356519
40.624563	1509.926433	18.361536
40.593401	1497.534724	18.366554
40.520701	1498.754816	18.371571
40.559894	1515.787617	18.376589
40.936242	1514.684006	18.381607
40.786715	1524.642341	18.386624
40.594275	1520.399308	18.391642
41.158929	1524.634466	18.396659
41.101483	1526.978845	18.401677
41.343993	1521.465247	18.406695
40.998988	1524.186054	18.411712
41.068794	1531.717817	18.416730
41.041294	1519.694766	18.421747
40.639330	1521.771215	18.426765
40.835196	1520.844211	18.431783
40.508482	1528.876776	18.436800
40.879723	1529.651756	18.441818
40.726124	1550.959554	18.446835
41.092531	1552.855657	18.451853
41.295716	1546.268875	18.456871
41.363558	1564.995138	18.461888
41.940425	1567.893424	18.466906
42.106152	1561.842706	18.471923
41.854705	1549.075201	18.476941
41.987426	1532.731782	18.481959
41.836123	1537.691373	18.486976
41.679691	1546.069669	18.491994
41.794082	1536.460773	18.497011
41.900819	1545.369064	18.502029
42.155480	1535.432064	18.507047
41.636905	1539.032175	18.512064
41.772708	1543.883666	18.517082
41.936799	1532.767907	18.522099
41.768958	1541.734996	18.527117
41.636760	1548.026565	18.532135
42.450981	1561.406466	18.537152
42.213152	1561.159666	18.542170
42.488156	1566.323885	18.547187
42.307525	1568.381441	18.552205
42.611739	1558.730169	18.557223
42.175297	1570.336709	18.562240
42.220822	1566.157372	18.567258
42.273743	1563.643223	18.572275
42.012703	1567.711099	18.577293
42.393487	1559.666837	18.582311
42.259202	1573.337374	18.587328
42.233069	1564.564718	18.592346
42.564887	1566.819710	18.597363
42.583171	1571.168887	18.602381
42.758211	1564.873700	18.607399
42.538990	1572.081518	18.612416
42.445256	1567.488476	18.617434
42.507616	1573.456067	18.622451
42.361275	1588.794852	18.627469
42.766160	1585.985702	18.632487
42.598153	1586.946163	18.637504
42.455836	1580.132621	18.642522
42.718834	1585.156708	18.647539
42.650069	1607.360198	18.652557
42.977221	1595.436173	18.657575
43.215942	1611.184885	18.662592
42.999705	1614.346302	18.667610
43.299440	1607.671783	18.672627
43.333388	1611.898590	18.677645
43.786260	1619.133674	18.682663
43.562670	1616.053739	18.687680
43.402940	1612.215834	18.692698
43.950040	1606.263148	18.697715
43.407723	1602.832344	18.702733
43.551228	1603.396843	18.707751
43.749849	1604.659644	18.712768
43.772307	1606.003696	18.717786
43.798452	1605.317885	18.722803
43.686194	1602.289940	18.727821
43.766156	1606.825132	18.732839
43.786019	1615.283142	18.737856
43.724209	1606.689633	18.742874
43.806275	1594.406356	18.747891
43.905411	1603.341114	18.752909
43.875122	1594.117792	18.757927
43.705784	1608.213591	18.762944
43.723702	1601.109834	18.767962
44.110140	1590.312670	18.772979
43.978248	1592.996942	18.777997
44.284324	1610.619212	18.783015
44.360361	1628.990790	18.788032
44.446254	1620.380445	18.793050
44.602240	1616.076486	18.798067
44.097839	1613.330897	18.803085
44.834461	1619.271761	18.808103
44.384785	1612.234949	18.813120
44.035661	1620.618222	18.818138
44.599135	1623.386065	18.823155
44.383305	1621.242235	18.828173
44.287766	1622.181877	18.833191
44.453932	1616.112136	18.838208
44.491194	1623.330284	18.843226
44.708388	1620.793545	18.848243
44.302309	1635.784881	18.853261
44.856174	1631.055643	18.858279
44.610000	1644.926812	18.863296
44.694775	1648.599680	18.868314
45.039558	1648.873856	18.873331
45.030209	1654.625479	18.878349
44.836997	1651.061070	18.883367
45.140068	1655.031115	18.888384
44.867741	1657.298718	18.893402
44.701947	1649.983871	18.898419
45.048791	1654.470950	18.903437
45.186863	1660.985316	18.908455
45.268617	1661.082940	18.913472
45.391466	1666.198439	18.918490
45.854367	1667.277819	18.923507
45.587824	1656.052719	18.928525
45.269806	1659.501504	18.933543
45.554847	1666.617729	18.938560
45.510846	1682.038395	18.943578
45.661431	1675.712285	18.948595
45.530741	1673.425715	18.953613
45.878638	1673.030335	18.958631
45.794512	1677.218849	18.963648
45.857018	1680.330293	18.968666
45.870529	1678.194708	18.973683
45.759208	1688.039844	18.978701
45.748919	1675.367016	18.983719
46.053243	1668.925298	18.988736
45.738394	1682.280207	18.993754
45.766908	1674.505693	18.998771
45.719634	1680.228551	19.003789
46.006774	1684.857542	19.008807
46.045713	1693.637666	19.013824
46.074277	1701.365321	19.018842
46.410300	1695.865422	19.023859
46.251031	1700.504396	19.028877
46.057915	1700.165376	19.033895
46.157680	1691.388713	19.038912
46.124538	1698.128745	19.043930
46.472740	1705.462320	19.048947
46.379213	1701.733950	19.053965
46.418087	1701.882477	19.058983
46.974770	1722.094526	19.064000
46.787414	1727.975055	19.069018
47.205102	1718.814032	19.074035
47.058235	1719.168395	19.079053
46.869731	1719.437758	19.084071
47.251082	1708.994791	19.089088
46.939430	1706.117996	19.094106
46.928940	1692.990725	19.099123
46.987651	1705.618055	19.104141
47.152025	1707.624729	19.109159
47.039784	1708.194585	19.114176
47.145031	1712.605916	19.119194
47.390071	1715.300581	19.124211
47.206802	1716.853609	19.129229
47.094583	1715.883342	19.134247
47.452195	1705.254737	19.139264
46.841381	1711.621352	19.144282
47.391567	1700.157803	19.149299
47.710458	1707.123565	19.154317
47.397799	1702.198695	19.159335
47.358102	1707.942466	19.164352
47.532055	1728.839373	19.169370
47.813961	1721.713144	19.174387
47.774280	1734.690444	19.179405
47.655022	1740.743355	19.184423
48.139915	1740.386474	19.189440
48.240306	1745.533919	19.194458
48.293529	1725.961577	19.199475
48.178890	1723.416851	19.204493
47.810069	1730.354663	19.209511
47.783662	1729.396198	19.214528
47.749413	1728.517861	19.219546
47.673985	1721.936795	19.224563
47.783482	1730.459715	19.229581
48.212013	1734.672068	19.234599
48.424790	1725.587331	19.239616
47.870675	1749.574429	19.244634
48.171865	1740.646256	19.249651
48.413826	1753.775115	19.254669
48.393324	1753.191286	19.259687
48.455022	1757.066620	19.264704
48.294107	1754.308220	19.269722
48.764618	1759.205164	19.274739
48.683387	1756.106056	19.279757
48.586028	1758.971145	19.284775
48.966559	1754.237473	19.289792
48.230051	1761.258153	19.294810
48.499688	1755.800197	19.299827
49.054931	1769.287107	19.304845
49.148347	1787.103825	19.309863
49.444959	1779.426125	19.314880
48.973054	1790.533403	19.319898
48.767037	1782.647256	19.324915
49.269572	1777.578863	19.329933
49.165461	1784.115438	19.334951
49.459399	1781.784417	19.339968
49.306027	1781.038357	19.344986
49.774940	1781.015359	19.350003
49.423091	1778.154318	19.355021
49.590177	1784.146600	19.360039
49.894881	1776.745361	19.365056
49.179265	1774.891269	19.370074
49.370297	1777.237778	19.375091
49.408949	1777.402119	19.380109
49.597041	1774.727899	19.385127
49.957943	1769.284043	19.390144
49.732080	1779.712099	19.395162
50.066091	1769.699418	19.400179
50.038812	1772.408353	19.405197
49.917171	1777.666339	19.410215
50.260335	1773.929499	19.415232
50.037744	1775.674898	19.420250
49.720942	1771.545968	19.425267
49.791203	1772.617440	19.430285
49.973623	1794.327344	19.435303
50.325321	1791.261392	19.440320
50.096499	1792.859436	19.445338
50.050006	1797.872109	19.450355
50.279040	1789.195073	19.455373
50.320448	1789.406323	19.460391
50.416366	1796.662691	19.465408
50.203229	1798.737990	19.470426
50.305038	1805.112914	19.475443
50.545524	1812.005790	19.480461
50.569246	1816.808639	19.485479
50.617385	1820.443099	19.490496
50.454307	1824.145368	19.495514
50.824703	1819.381707	19.500531
50.645755	1809.935397	19.505549
51.038774	1811.868387	19.510567
50.932049	1814.012228	19.515584
51.023606	1836.831553	19.520602
51.220836	1835.762299	19.525619
51.214265	1843.653321	19.530637
51.437668	1839.187258	19.535655
51.644394	1837.295954	19.540672
51.423238	1839.801731	19.545690
51.525216	1842.206385	19.550707
51.424765	1820.900121	19.555725
51.136421	1838.511599	19.560743
51.549886	1832.472472	19.565760
51.410748	1842.157939	19.570778
51.582978	1832.520887	19.575795
51.788081	1830.670866	19.580813
51.444755	1837.475329	19.585831
51.697144	1832.963698	19.590848
51.588130	1836.051545	19.595866
51.443924	1831.504216	19.600883
51.788010	1833.410159	19.605901
51.768511	1835.092183	19.610919
52.232822	1850.913067	19.615936
52.279723	1855.740699	19.620954
51.962212	1854.307095	19.625971
52.317730	1844.464583	19.630989
52.116443	1854.898300	19.636007
52.351797	1854.533174	19.641024
52.212722	1864.944526	19.646042
52.340185	1856.352803	19.651059
52.471657	1852.352449	19.656077
52.068951	1858.001655	19.661095
52.218954	1856.911396	19.666112
52.584703	1855.676873	19.671130
52.524957	1854.493236	19.676147
52.741932	1852.410965	19.681165
52.336831	1856.649809	19.686183
52.670543	1867.763467	19.691200
53.102540	1875.112387	19.696218
52.903168	1877.011958	19.701235
53.294579	1876.612914	19.706253
52.890628	1875.770401	19.711271
52.926245	1873.457748	19.716288
53.061629	1879.161520	19.721306
53.127009	1883.585451	19.726323
52.990686	1872.674350	19.731341
53.098738	1885.590741	19.736359
53.167458	1878.204342	19.741376
53.007530	1879.662203	19.746394
53.124976	1876.140600	19.751411
53.348792	1882.395443	19.756429
53.221856	1900.590804	19.761447
53.355493	1896.110387	19.766464
53.717711	1903.012630	19.771482
53.498402	1907.591631	19.776499
53.940999	1905.928471	19.781517
53.851885	1904.695779	19.786535
53.490611	1901.646833	19.791552
53.859956	1901.349082	19.796570
53.534460	1900.061902	19.801587
54.099538	1908.444096	19.806605
54.041699	1919.473955	19.811623
54.284734	1917.005715	19.816640
54.050291	1930.262997	19.821658
54.362272	1925.420092	19.826675
54.563497	1917.009301	19.831693
54.577249	1915.034607	19.836711
54.457150	1916.776584	19.841728
54.460676	1918.366640	19.846746
54.600426	1914.914124	19.851763
54.985086	1916.267728	19.856781
54.481475	1924.069390	19.861799
54.596284	1923.473824	19.866816
54.566821	1922.427459	19.871834
54.521551	1927.130686	19.876851
54.420760	1913.127404	19.881869
54.412836	1921.798209	19.886887
54.523134	1926.590679	19.891904
54.766450	1932.324898	19.896922
55.012748	1945.349070	19.901939
54.955325	1948.065911	19.906957
54.966619	1940.104618	19.911975
54.989221	1935.606871	19.916992
55.058097	1939.023496	19.922010
55.407146	1943.627076	19.927027
55.623141	1940.307786	19.932045
55.335778	1943.332071	19.937063
55.464846	1941.793774	19.942080
55.347826	1939.725949	19.947098
55.517027	1936.369807	19.952115
55.397885	1947.311452	19.957133
55.435974	1945.184608	19.962151
55.501043	1957.713283	19.967168
55.671668	1964.973794	19.972186
55.383433	1957.987295	19.977203
55.798136	1955.261763	19.982221
55.348642	1971.320605	19.987239
55.824717	1974.746028	19.992256
55.683038	1980.957178	19.997274
55.664098	1988.575626	20.002291
55.919955	1982.482242	20.007309
55.930731	1992.018060	20.012327
56.161126	1990.037820	20.017344
56.338020	1988.823410	20.022362
56.347006	2002.579131	20.027379
56.800332	2002.129356	20.032397
56.908734	2010.075026	20.037415
56.476816	2004.446024	20.042432
56.758362	1998.279177	20.047450
56.612320	1997.181640	20.052467
57.011275	2000.306703	20.057485
57.180733	2002.637685	20.062503
56.990144	1988.459051	20.067520
57.040769	1987.125559	20.072538
57.109514	1992.088671	20.077555
57.091967	1987.944365	20.082573
56.623725	1988.055574	20.087591
57.331015	1996.967834	20.092608
57.443069	1998.679759	20.097626
57.523940	2001.835722	20.102643
57.861293	1995.211975	20.107661
57.120702	1996.861814	20.112679
57.518331	1990.885081	20.117696
57.648136	1993.433729	20.122714
57.426786	2002.084359	20.127731
57.531541	1996.803653	20.132749
57.602572	1999.762327	20.137767
57.584981	1999.124382	20.142784
58.132358	1984.363036	20.147802
57.518585	1994.227097	20.152819
57.503574	1991.209098	20.157837
57.521635	1998.357817	20.162855
57.976078	1998.886237	20.167872
58.153853	2011.731831	20.172890
57.752979	2014.975898	20.177907
58.194842	2019.501835	20.182925
57.734572	2024.825572	20.187943
58.037365	2023.837605	20.192960
58.183836	2017.849716	20.197978
57.938930	2022.524282	20.202995
58.548269	2023.637551	20.208013
58.889682	2033.907443	20.213031
58.776356	2031.930554	20.218048
58.659903	2025.519918	20.223066
58.358543	2011.213442	20.228083
58.322383	2028.047082	20.233101
58.534138	2032.145136	20.238119
58.620969	2043.048256	20.243136
58.924955	2037.966714	20.248154
58.825888	2043.382199	20.253171
59.122879	2045.450190	20.258189
59.206363	2042.741823	20.263207
59.095245	2041.263242	20.268224
58.895295	2040.672802	20.273242
59.059904	2049.499688	20.278259
59.279852	2055.808852	20.283277
59.756136	2059.262663	20.288295
59.442299	2065.844823	20.293312
59.848291	2057.900540	20.298330
59.401060	2066.637088	20.303347
59.861744	2051.699907	20.308365
59.813135	2056.665643	20.313383
59.542129	2056.676516	20.318400
59.575479	2057.829534	20.323418
59.720683	2060.577766	20.328435
59.555709	2048.389692	20.333453
59.519566	2048.303803	20.338471
59.779798	2061.688822	20.343488
60.239063	2058.782711	20.348506
60.148392	2060.870413	20.353523
59.652916	2062.851111	20.358541
59.799121	2071.292697	20.363559
60.098346	2084.927264	20.368576
60.265572	2087.880349	20.373594
60.254678	2086.032584	20.378611
60.767670	2082.982341	20.383629
60.464150	2080.470312	20.388647
60.579758	2080.420613	20.393664
60.795887	2081.974218	20.398682
60.702346	2085.315324	20.403699
60.754362	2099.585127	20.408717
60.768809	2111.610560	20.413735
60.796817	2100.790347	20.418752
61.042976	2095.724162	20.423770
60.583334	2106.618257	20.428787
61.125417	2105.027862	20.433805
61.212340	2103.991655	20.438823
60.949126	2106.797571	20.443840
61.364113	2093.483416	20.448858
61.339357	2102.898618	20.453875
61.242630	2105.769975	20.458893
61.401533	2105.063345	20.463911
61.506769	2118.491626	20.468928
61.484060	2121.891075	20.473946
61.591413	2124.459040	20.478963
61.696492	2116.397762	20.483981
62.000474	2121.806931	20.488999
61.454144	2120.099861	20.494016
61.858566	2105.471276	20.499034
61.789640	2116.013804	20.504051
61.810211	2114.722884	20.509069
61.807105	2120.599921	20.514087
62.023985	2141.389591	20.519104
62.629534	2138.993922	20.524122
62.137559	2143.792442	20.529139
62.322133	2146.468242	20.534157
62.349658	2141.316368	20.539175
62.244183	2143.939773	20.544192
62.573796	2138.276629	20.549210
62.262784	2132.574991	20.554227
62.815981	2146.813650	20.559245
62.858897	2125.844352	20.564263
62.545369	2133.935084	20.569280
62.913861	2137.945485	20.574298
63.096427	2133.523621	20.579315
62.885167	2146.992042	20.584333
63.371228	2149.936214	20.589351
62.880980	2143.366331	20.594368
63.428883	2142.119032	20.599386
63.277973	2164.642220	20.604403
63.401581	2168.476383	20.609421
63.392150	2165.198682	20.614439
63.199485	2163.496163	20.619456
63.108420	2161.026581	20.624474
63.259371	2155.277806	20.629491
63.326749	2155.286160	20.634509
63.877704	2154.776900	20.639527
63.491369	2164.188819	20.644544
63.523533	2152.326423	20.649562
63.625667	2160.844390	20.654579
63.251558	2163.333147	20.659597
63.663710	2172.585251	20.664615
63.900019	2185.731093	20.669632
63.599754	2181.615257	20.674650
63.858902	2179.223359	20.679667
64.017335	2177.109194	20.684685
64.041645	2185.229077	20.689703
63.743507	2202.937127	20.694720
64.292513	2200.985848	20.699738
64.145170	2208.892773	20.704755
64.417027	2217.636661	20.709773
64.621464	2203.250787	20.714791
64.521684	2217.355102	20.719808
64.600690	2208.429947	20.724826
64.795517	2218.394680	20.729843
64.792373	2229.476125	20.734861
65.143310	2226.492278	20.739879
65.286106	2237.484586	20.744896
65.266971	2235.445575	20.749914
65.479858	2232.164592	20.754931
65.284347	2219.261601	20.759949
65.378384	2205.284375	20.764967
65.244088	2205.693586	20.769984
65.207497	2212.058778	20.775002
65.679768	2215.658429	20.780019
65.552559	2221.132029	20.785037
65.638577	2217.208150	20.790055
65.364822	2223.768307	20.795072
65.651915	2224.704840	20.800090
65.488314	2220.447653	20.805107
65.445258	2222.641532	20.810125
65.860891	2216.390481	20.815143
65.642330	2235.692538	20.820160
65.863686	2245.615257	20.825178
66.192756	2238.699203	20.830195
66.046486	2252.365822	20.835213
66.055016	2245.017107	20.840231
66.392000	2252.415787	20.845248
66.511492	2245.674591	20.850266
66.472901	2249.411096	20.855283
66.472756	2243.594439	20.860301
66.493081	2252.630239	20.865319
66.438182	2250.934531	20.870336
66.315946	2250.521273	20.875354
66.454876	2246.589098	20.880371
66.222773	2266.893787	20.885389
66.768700	2269.831755	20.890407
66.907133	2279.290916	20.895424
66.524227	2276.702926	20.900442
66.780065	2268.112986	20.905459
66.555761	2281.583552	20.910477
67.045356	2286.670175	20.915495
66.896872	2292.150286	20.920512
67.314071	2288.117694	20.925530
67.631778	2289.181990	20.930547
67.443452	2294.611534	20.935565
67.597646	2292.431742	20.940583
67.285797	2291.379100	20.945600
67.765289	2301.283499	20.950618
67.789651	2302.030805	20.955635
67.505047	2311.900276	20.960653
67.830686	2299.666725	20.965671
67.899221	2308.265772	20.970688
67.915331	2317.393792	20.975706
68.287388	2310.874956	20.980723
68.109596	2316.182925	20.985741
68.163678	2309.010100	20.990759
68.467750	2309.558935	20.995776
68.378082	2305.144963	21.000794
68.222643	2308.287506	21.005811
68.131825	2304.463904	21.010829
68.395300	2301.553713	21.015847
68.581999	2304.696306	21.020864
68.417324	2302.582251	21.025882
68.544332	2322.281580	21.030899
68.436640	2324.630778	21.035917
68.696371	2331.773327	21.040935
68.790958	2334.655776	21.045952
68.858278	2332.432781	21.050970
69.122615	2337.204384	21.055987
69.035295	2349.043929	21.061005
69.009377	2334.918123	21.066023
69.390203	2346.349775	21.071040
69.194944	2356.448291	21.076058
69.299436	2362.182306	21.081075
69.223915	2361.966873	21.086093
69.513997	2357.149377	21.091111
69.461054	2357.097679	21.096128
69.763734	2356.586285	21.101146
69.779768	2354.753209	21.106163
69.680732	2362.873561	21.111181
69.509657	2362.657318	21.116199
69.879436	2377.799138	21.121216
70.172910	2378.813582	21.126234
70.407492	2374.907422	21.131251
70.263850	2386.519109	21.136269
70.514786	2384.750223	21.141287
70.583270	2375.495243	21.146304
70.473662	2375.900590	21.151322
70.867222	2372.559714	21.156339
70.530204	2375.232054	21.161357
70.527334	2373.581836	21.166375
70.566584	2381.109275	21.171392
70.640151	2377.080005	21.176410
70.755879	2366.757177	21.181427
70.643088	2384.859285	21.186445
70.853897	2373.773560	21.191463
70.648551	2385.019338	21.196480
71.085800	2399.689814	21.201498
71.328819	2399.648557	21.206515
71.176892	2407.947646	21.211533
71.138871	2393.441801	21.216551
70.990944	2398.871359	21.221568
71.193275	2403.034098	21.226586
71.191599	2403.271042	21.231603
71.028261	2420.497395	21.236621
71.447079	2424.361108	21.241639
71.554218	2414.326804	21.246656
71.601160	2425.283748	21.251674
71.901644	2420.833870	21.256691
71.888834	2412.768836	21.261709
72.117082	2434.576487	21.266727
72.158292	2441.604980	21.271744
72.121757	2438.877484	21.276762
72.308258	2436.436968	21.281779
72.363591	2444.293306	21.286797
72.359037	2438.101699	21.291815
72.613015	2434.530191	21.296832
72.463411	2439.035283	21.301850
72.778225	2432.437001	21.306867
72.524011	2443.078186	21.311885
72.467741	2437.279728	21.316903
72.712255	2429.976023	21.321920
72.083353	2430.456419	21.326938
72.659269	2441.857566	21.331955
72.613852	2451.121538	21.336973
73.143160	2452.061164	21.341991
73.296569	2456.591378	21.347008
73.304629	2451.679173	21.352026
73.354991	2451.093687	21.357043
73.228376	2453.871943	21.362061
73.479706	2450.253505	21.367079
73.797718	2450.301495	21.372096
73.256532	2455.982050	21.377114
73.491521	2453.407690	21.382131
73.403425	2457.603320	21.387149
73.502862	2473.879593	21.392167
73.747974	2476.284000	21.397184
73.449863	2476.166561	21.402202
73.804847	2474.741163	21.407219
73.749774	2482.365482	21.412237
73.632423	2497.400668	21.417255
74.096565	2508.535319	21.422272
73.884835	2510.096030	21.427290
74.017085	2500.720531	21.432307
74.063763	2518.621046	21.437325
74.212150	2521.438285	21.442343
74.518969	2526.345309	21.447360
74.547344	2520.994357	21.452378
74.620129	2518.959850	21.457395
74.870043	2525.873617	21.462413
75.025396	2531.220982	21.467431
75.414355	2534.533918	21.472448
75.370502	2532.546089	21.477466
75.480383	2526.011442	21.482483
75.099416	2524.426760	21.487501
75.202091	2518.836927	21.492519
75.928396	2542.662345	21.497536
75.731895	2539.199269	21.502554
75.866444	2526.727232	21.507571
75.402249	2525.919373	21.512589
75.681231	2527.715661	21.517607
75.586064	2539.638621	21.522624
75.477119	2541.277914	21.527642
75.618885	2541.946869	21.532659
75.698932	2545.270333	21.537677
75.625162	2538.556149	21.542695
75.846872	2546.512711	21.547712
75.714186	2565.277748	21.552730
75.967430	2558.051527	21.557747
76.284657	2565.450277	21.562765
76.136996	2562.001637	21.567783
76.388133	2575.666205	21.572800
76.137470	2584.113401	21.577818
76.663295	2595.673989	21.582835
76.994048	2588.849067	21.587853
77.015299	2595.394701	21.592871
77.065899	2593.051204	21.597888
76.333010	2593.472147	21.602906
76.688255	2587.899532	21.607923
76.871861	2598.525867	21.612941
76.968772	2609.383566	21.617959
76.859931	2617.653907	21.622976
77.019586	2628.082019	21.627994
77.597777	2618.930113	21.633011
77.757919	2615.133405	21.638029
77.750332	2616.715795	21.643047
77.913682	2615.695991	21.648064
77.844364	2618.458983	21.653082
77.533429	2605.283432	21.658099
77.998648	2608.511843	21.663117
77.970988	2607.913327	21.668135
78.154918	2608.916543	21.673152
77.772178	2611.722326	21.678170
77.944888	2618.701879	21.683187
78.225575	2634.839436	21.688205
77.984857	2639.210514	21.693223
78.241363	2631.668138	21.698240
78.301549	2627.470477	21.703258
78.375514	2623.292750	21.708275
78.437496	2637.949625	21.713293
78.594556	2649.722675	21.718311
78.766156	2661.064219	21.723328
78.832610	2664.639169	21.728346
79.050471	2661.701350	21.733363
79.003116	2662.226352	21.738381
78.698902	2659.761691	21.743399
79.164970	2645.905737	21.748416
78.812807	2654.681327	21.753434
79.134189	2671.522674	21.758451
79.497138	2674.498848	21.763469
79.696566	2677.642668	21.768487
79.606614	2669.510701	21.773504
79.437116	2680.659518	21.778522
79.829357	2671.442034	21.783539
80.107196	2671.688844	21.788557
79.853042	2680.051416	21.793575
80.349420	2665.868770	21.798592
79.950327	2676.359201	21.803610
79.998160	2672.498017	21.808627
80.024870	2677.960265	21.813645
79.773698	2691.905613	21.818663
80.285756	2695.530690	21.823680
79.970610	2692.906773	21.828698
80.112392	2704.025772	21.833715
80.770516	2705.412343	21.838733
80.650943	2719.965171	21.843751
80.704514	2715.743275	21.848768
80.815498	2719.623721	21.853786
80.642024	2718.410501	21.858803
81.166536	2723.428656	21.863821
81.017245	2711.048305	21.868839
81.114950	2718.610914	21.873856
80.843656	2727.474866	21.878874
81.324580	2736.508182	21.883891
81.532658	2737.536027	21.888909
81.653530	2745.369604	21.893927
81.784209	2741.072499	21.898944
82.027566	2748.719610	21.903962
81.833626	2742.260891	21.908979
81.798317	2741.780347	21.913997
81.613877	2745.394622	21.919015
82.185895	2742.846323	21.924032
82.036040	2735.866243	21.929050
82.060859	2744.898431	21.934067
81.917527	2750.955452	21.939085
82.086929	2755.581076	21.944103
82.309050	2759.737642	21.949120
82.589908	2766.353130	21.954138
82.327646	2760.141821	21.959155
82.932312	2756.862486	21.964173
82.768582	2767.158287	21.969191
82.993088	2764.194161	21.974208
82.957220	2762.694262	21.979226
82.875591	2765.490766	21.984243
82.899677	2756.532914	21.989261
83.061071	2777.818064	21.994279
83.314077	2784.769321	21.999296
83.307026	2789.343695	22.004314
83.175926	2785.258026	22.009331
83.238822	2786.119250	22.014349
83.272353	2792.906057	22.019367
83.709079	2781.958277	22.024384
83.442920	2786.102975	22.029402
83.327028	2797.139312	22.034419
84.137806	2798.312603	22.039437
83.758380	2803.017914	22.044455
83.742933	2804.929795	22.049472
83.578887	2807.089045	22.054490
83.826496	2808.801904	22.059507
84.190353	2808.268289	22.064525
84.221435	2829.788536	22.069543
84.281349	2830.628136	22.074560
84.193180	2829.186923	22.079578
84.173341	2832.825926	22.084595
84.349552	2832.391145	22.089613
84.425828	2843.690927	22.094631
84.727979	2851.982202	22.099648
84.804677	2848.757163	22.104666
84.941544	2854.107520	22.109683
85.245843	2842.069474	22.114701
85.297688	2851.564595	22.119719
85.823650	2844.945708	22.124736
85.523479	2857.033555	22.129754
85.600987	2852.189266	22.134771
85.574505	2852.865656	22.139789
85.671430	2870.117942	22.144807
85.898188	2873.345888	22.149824
85.917456	2867.611205	22.154842
85.856325	2866.396155	22.159859
85.735939	2871.023025	22.164877
85.960426	2868.532313	22.169895
86.236353	2867.277081	22.174912
85.987923	2865.460138	22.179930
86.017801	2886.393591	22.184947
86.464220	2883.438865	22.189965
86.403275	2887.835492	22.194983
86.400754	2890.619622	22.200000
86.429432	2897.063204	22.205018
86.819039	2902.121483	22.210035
86.903265	2887.050066	22.215053
86.779835	2900.757784	22.220071
87.351618	2918.377587	22.225088
87.612151	2913.706602	22.230106
87.110298	2916.752027	22.235123
87.180766	2912.521126	22.240141
87.199795	2913.891064	22.245159
87.342885	2907.013363	22.250176
87.413592	2914.062668	22.255194
87.329061	2910.260045	22.260211
87.891692	2910.269712	22.265229
87.616677	2923.136399	22.270247
87.736624	2933.895998	22.275264
88.122119	2938.418378	22.280282
88.105175	2933.061779	22.285299
88.231906	2932.606342	22.290317
88.052101	2944.684859	22.295335
88.075740	2940.256135	22.300352
88.453756	2944.773376	22.305370
88.194931	2946.635029	22.310387
88.712999	2954.109784	22.315405
88.719225	2961.418550	22.320423
88.723132	2961.392662	22.325440
88.880142	2966.013970	22.330458
88.736092	2962.167005	22.335475
89.053314	2960.210932	22.340493
88.515568	2958.925363	22.345511
88.986229	2962.014114	22.350528
88.921143	2969.135215	22.355546
89.238410	2979.917582	22.360563
89.340945	2978.897818	22.365581
89.425873	2988.719230	22.370599
89.443418	2984.294607	22.375616
89.357006	2975.701141	22.380634
89.157441	3001.641701	22.385651
89.779636	3002.686743	22.390669
89.859797	3017.552545	22.395687
89.862405	3011.359619	22.400704
89.924854	3006.492398	22.405722
90.020002	3029.438922	22.410739
90.263642	3036.328620	22.415757
90.716787	3043.886178	22.420775
90.593954	3031.166902	22.425792
90.779303	3034.486583	22.430810
90.437481	3030.661120	22.435827
90.676192	3028.382781	22.440845
90.582110	3036.622595	22.445863
90.793104	3045.521610	22.450880
91.136449	3044.350490	22.455898
90.959181	3063.747961	22.460915
91.353813	3058.775027	22.465933
91.049516	3061.994678	22.470951
90.763154	3058.633953	22.475968
91.656501	3066.198303	22.480986
91.478385	3082.373424	22.486003
91.503707	3079.926512	22.491021
91.793361	3078.385055	22.496039
91.659409	3075.502288	22.501056
92.026594	3072.190668	22.506074
91.948918	3087.813500	22.511091
92.334659	3088.867187	22.516109
92.562178	3099.783625	22.521127
92.559077	3100.945576	22.526144
92.450295	3097.964176	22.531162
92.288792	3106.568083	22.536179
92.409535	3098.639630	22.541197
92.631499	3097.361274	22.546215
92.706626	3095.146431	22.551232
92.716701	3111.434124	22.556250
92.921365	3122.950684	22.561267
93.019391	3122.187273	22.566285
93.435623	3119.988422	22.571303
93.035751	3121.079976	22.576320
93.534343	3113.654128	22.581338
93.442967	3114.769942	22.586355
93.505701	3119.810057	22.591373
93.672110	3134.504632	22.596391
93.795120	3141.927736	22.601408
93.752512	3144.282625	22.606426
93.943330	3140.518876	22.611443
93.867365	3137.538640	22.616461
94.127580	3141.645139	22.621479
94.053036	3147.581047	22.626496
94.432270	3138.141272	22.631514
94.195418	3154.622346	22.636531
94.545691	3153.289166	22.641549
94.436923	3159.470314	22.646567
94.614293	3162.507207	22.651584
94.968600	3154.176014	22.656602
94.559699	3163.055425	22.661619
94.653472	3162.889208	22.666637
94.423802	3173.343914	22.671655
94.616242	3177.669351	22.676672
95.131514	3178.797438	22.681690
94.978199	3194.324900	22.686707
95.207544	3198.388905	22.691725
95.352400	3207.446705	22.696743
95.318677	3210.630303	22.701760
95.534598	3215.245602	22.706778
95.626366	3203.483645	22.711795
95.942882	3202.749124	22.716813
95.756878	3206.685673	22.721831
95.548749	3214.678311	22.726848
95.915656	3220.276800	22.731866
96.041049	3237.474478	22.736883
96.146365	3234.961356	22.741901
96.730990	3239.569396	22.746919
96.718371	3241.168411	22.751936
96.611271	3245.720700	22.756954
96.770871	3258.005064	22.761971
96.707802	3257.023854	22.766989
97.355984	3251.897518	22.772007
97.128155	3259.091574	22.777024
97.294211	3251.837706	22.782042
97.317415	3257.688898	22.787059
97.294609	3251.865997	22.792077
97.228164	3254.429791	22.797095
96.893341	3260.100358	22.802112
98.086061	3263.988195	22.807130
97.807261	3273.491154	22.812147
97.933398	3275.734403	22.817165
97.966839	3275.650231	22.822183
98.083424	3276.900756	22.827200
97.915373	3270.582978	22.832218
97.914472	3284.448541	22.837235
98.347864	3290.500605	22.842253
98.557967	3293.500830	22.847271
98.548479	3292.899444	22.852288
98.472064	3301.931989	22.857306
98.515341	3299.709486	22.862323
98.479498	3302.855557	22.867341
98.485183	3297.779369	22.872359
98.597884	3319.410507	22.877376
99.030475	3320.867183	22.882394
98.856965	3329.526733	22.887411
99.290155	3327.647141	22.892429
99.208581	3335.667349	22.897447
99.129483	3344.719274	22.902464
99.753781	3348.251151	22.907482
99.474722	3362.971515	22.912499
99.395535	3346.760652	22.917517
99.957005	3357.501831	22.922535
99.989056	3368.966685	22.927552
100.132577	3375.143099	22.932570
100.274318	3376.541191	22.937587
100.231017	3389.899004	22.942605
100.390071	3376.769193	22.947623
100.101476	3376.991132	22.952640
100.318960	3381.912388	22.957658
100.475497	3388.569678	22.962675
100.682510	3394.976029	22.967693
101.225498	3394.799401	22.972711
100.972034	3395.312527	22.977728
101.054103	3387.986543	22.982746
101.106734	3391.857338	22.987763
100.848023	3412.060169	22.992781
101.383215	3422.556158	22.997799
101.225781	3428.994369	23.002816
101.410024	3423.643980	23.007834
101.189086	3428.163649	23.012851
101.276787	3440.361557	23.017869
101.926999	3448.311354	23.022887
101.802376	3459.254773	23.027904
101.888677	3446.672879	23.032922
101.623538	3450.009558	23.037939
101.776290	3455.259761	23.042957
102.453847	3469.457896	23.047975
102.019658	3471.580641	23.052992
102.149824	3479.028013	23.058010
102.574787	3482.284986	23.063027
102.759576	3497.867052	23.068045
103.292465	3512.340390	23.073063
102.852235	3507.940014	23.078080
103.274320	3494.292307	23.083098
103.183157	3495.401798	23.088115
103.202816	3504.924401	23.093133
103.171493	3488.980509	23.098151
103.497868	3503.404130	23.103168
103.602730	3512.285284	23.108186
103.709772	3527.283015	23.113203
103.746670	3523.922058	23.118221
103.995698	3519.214846	23.123239
103.552971	3523.441032	23.128256
104.219011	3511.724624	23.133274
104.409156	3526.005479	23.138291
104.391587	3531.301326	23.143309
104.639546	3536.647108	23.148327
104.372133	3535.328609	23.153344
104.702601	3536.441485	23.158362
104.520179	3536.829858	23.163379
104.444816	3540.761770	23.168397
104.994450	3547.411189	23.173415
104.593607	3564.505402	23.178432
104.855282	3558.240137	23.183450
105.204101	3561.351239	23.188467
104.841747	3569.459729	23.193485
105.347062	3586.494059	23.198503
105.720838	3595.071149	23.203520
105.622369	3594.751980	23.208538
105.912786	3591.515420	23.213555
105.794162	3591.524510	23.218573
106.264865	3593.761161	23.223591
106.416536	3613.581134	23.228608
106.123575	3607.977197	23.233626
106.250489	3618.941274	23.238643
106.203066	3619.374781	23.243661
106.647504	3609.785668	23.248679
106.398309	3628.472217	23.253696
106.505402	3634.818556	23.258714
106.875525	3636.165106	23.263731
106.742987	3641.766223	23.268749
106.901515	3628.629999	23.273767
106.713184	3649.172418	23.278784
106.939203	3654.998277	23.283802
107.260432	3660.698750	23.288819
107.191701	3664.405550	23.293837
107.754135	3660.438282	23.298855
107.631033	3683.299890	23.303872
107.763387	3690.440843	23.308890
107.965027	3690.718546	23.313907
107.812404	3692.014433	23.318925
108.028474	3687.593254	23.323943
107.991294	3690.846918	23.328960
108.250956	3711.066715	23.333978
108.364940	3710.689008	23.338995
108.373351	3712.988633	23.344013
108.695518	3711.899698	23.349031
108.711312	3717.180904	23.354048
108.935346	3719.497249	23.359066
108.907007	3719.179716	23.364083
108.684173	3734.103047	23.369101
109.089699	3743.978802	23.374119
109.321426	3735.616046	23.379136
109.016620	3742.361526	23.384154
109.210578	3737.479818	23.389171
109.379407	3745.438883	23.394189
109.379110	3749.119197	23.399207
109.233574	3757.405276	23.404224
109.454508	3766.565067	23.409242
109.921814	3775.187560	23.414259
110.189078	3785.126031	23.419277
110.044295	3785.063467	23.424295
110.385270	3789.984425	23.429312
110.321710	3801.306715	23.434330
110.562633	3806.628428	23.439347
110.164467	3801.880502	23.444365
110.483212	3803.367682	23.449383
110.885777	3812.757860	23.454400
111.145542	3832.138186	23.459418
111.300537	3833.559488	23.464435
111.098759	3837.795342	23.469453
111.515088	3830.994424	23.474471
112.004358	3828.196966	23.479488
111.710835	3822.630926	23.484506
111.988738	3824.983035	23.489523
112.002031	3819.230048	23.494541
112.091506	3833.021901	23.499559
111.991468	3847.168561	23.504576
112.174583	3842.168582	23.509594
112.471884	3848.917617	23.514611
112.135028	3847.909829	23.519629
112.582270	3835.305837	23.524647
112.407026	3855.537117	23.529664
112.423641	3869.652893	23.534682
112.837592	3867.397498	23.539699
113.016875	3872.416408	23.544717
113.155024	3876.741050	23.549735
113.160581	3884.751007	23.554752
113.510910	3890.216579	23.559770
113.557245	3897.279556	23.564787
113.575849	3903.781889	23.569805
113.590769	3905.679660	23.574823
113.632352	3905.568958	23.579840
113.833276	3894.035649	23.584858
113.957436	3900.893895	23.589875
113.774063	3913.431289	23.594893
114.330164	3911.693358	23.599911
114.149812	3922.251241	23.604928
114.185777	3922.469682	23.609946
114.297462	3926.056736	23.614963
114.215409	3948.277816	23.619981
114.735935	3939.645617	23.624999
114.629569	3948.698959	23.630016
114.682808	3967.824556	23.635034
115.043874	3965.507995	23.640051
115.232982	3969.483787	23.645069
115.445547	3968.456199	23.650087
115.507308	3960.489264	23.655104
115.264459	3967.960558	23.660122
115.834456	3982.911387	23.665139
115.520235	3992.644374	23.670157
115.778347	3996.741930	23.675175
115.810544	3998.725382	23.680192
116.017397	4001.852490	23.685210
115.791714	4015.614948	23.690227
115.888040	4014.854923	23.695245
116.213431	4016.751409	23.700263
116.162836	4030.151871	23.705280
116.588582	4040.674837	23.710298
116.730207	4038.051755	23.715315
116.957648	4041.488128	23.720333
117.243717	4043.772702	23.725351
116.937772	4050.846740	23.730368
117.192865	4071.250726	23.735386
117.437724	4072.992546	23.740403
117.442899	4070.431870	23.745421
117.608012	4073.436118	23.750439
117.358603	4074.349489	23.755456
117.199559	4083.553188	23.760474
117.952386	4086.310699	23.765491
117.986235	4100.386077	23.770509
118.158103	4096.937584	23.775527
118.425078	4105.768380	23.780544
118.611487	4117.929185	23.785562
118.880093	4121.147645	23.790579
118.726166	4123.109768	23.795597
118.868006	4112.576688	23.800615
118.997212	4119.828778	23.805632
118.520096	4119.420570	23.810650
119.236642	4124.828839	23.815667
118.839232	4136.067916	23.820685
119.115653	4133.919258	23.825703
119.471988	4143.648275	23.830720
119.594512	4165.761817	23.835738
119.937205	4154.023060	23.840755
119.708002	4163.057876	23.845773
119.622680	4163.800348	23.850791
119.996723	4180.451784	23.855808
120.405323	4187.221387	23.860826
120.001835	4178.538142	23.865843
120.392841	4190.774261	23.870861
120.466473	4199.054612	23.875879
120.855066	4209.062689	23.880896
120.801009	4218.480427	23.885914
121.037778	4208.614207	23.890931
121.014059	4212.522391	23.895949
121.205466	4219.183994	23.900967
121.795356	4225.817891	23.905984
121.285341	4239.233667	23.911002
121.508000	4236.847219	23.916019
121.477022	4243.085990	23.921037
121.546611	4241.279054	23.926055
121.791475	4254.996381	23.931072
121.794081	4270.831761	23.936090
122.466564	4272.872753	23.941107
122.277639	4257.581006	23.946125
122.168544	4274.008360	23.951143
122.636432	4284.521710	23.956160
122.556014	4289.139522	23.961178
122.680136	4287.106244	23.966195
122.971781	4291.943533	23.971213
122.851878	4292.991289	23.976231
122.967256	4304.598346	23.981248
123.292879	4317.176220	23.986266
123.366502	4303.023810	23.991283
123.081556	4311.275167	23.996301
123.249157	4320.004849	24.001319
123.641051	4330.905748	24.006336
123.540697	4337.120699	24.011354
124.132075	4346.996076	24.016371
124.213603	4359.586969	24.021389
124.232756	4363.712577	24.026407
124.298741	4361.202306	24.031424
124.444957	4360.103023	24.036442
124.337534	4353.724864	24.041459
124.840323	4369.930184	24.046477
124.739898	4377.139442	24.051495
125.212517	4373.287100	24.056512
124.649048	4385.391961	24.061530
124.984164	4378.133254	24.066547
125.329879	4399.716551	24.071565
125.389177	4412.292025	24.076583
125.772264	4408.100179	24.081600
125.653219	4402.939059	24.086618
125.326587	4403.675156	24.091635
125.821416	4419.342014	24.096653
125.685502	4428.886318	24.101671
126.093221	4434.235745	24.106688
126.176372	4447.647125	24.111706
126.346515	4452.582404	24.116723
126.568327	4470.719400	24.121741
126.563895	4467.058566	24.126759
126.940746	4463.154924	24.131776
127.030896	4473.901169	24.136794
127.319144	4481.482012	24.141811
127.130391	4490.428585	24.146829
127.286784	4491.003786	24.151847
127.393779	4484.740343	24.156864
127.364340	4502.654746	24.161882
127.910976	4507.095463	24.166899
127.665936	4505.015832	24.171917
127.743235	4514.735105	24.176935
128.017270	4516.103091	24.181952
128.089190	4531.877336	24.186970
128.309401	4531.195732	24.191987
128.289002	4533.168544	24.197005
128.278190	4554.883637	24.202023
128.746839	4556.208511	24.207040
128.837821	4568.715999	24.212058
129.081895	4567.140527	24.217075
129.144619	4572.010598	24.222093
129.039377	4589.277258	24.227111
129.235124	4585.992226	24.232128
129.383463	4591.344458	24.237146
129.578362	4608.573583	24.242163
129.760258	4610.536806	24.247181
129.486827	4621.826200	24.252199
129.975198	4625.196553	24.257216
129.970718	4630.613773	24.262234
130.089962	4637.062725	24.267251
130.548863	4642.710376	24.272269
130.579629	4654.403511	24.277287
131.026973	4663.922848	24.282304
131.261398	4673.311409	24.287322
131.481527	4670.448670	24.292339
131.191864	4653.038577	24.297357
131.242435	4655.701026	24.302375
131.438791	4653.981510	24.307392
131.638812	4676.793745	24.312410
131.640540	4683.693565	24.317427
131.925987	4691.757880	24.322445
131.790801	4693.852857	24.327463
132.128044	4687.925739	24.332480
132.018684	4694.820871	24.337498
132.215396	4702.226757	24.342515
132.482899	4704.697402	24.347533
132.401537	4720.817789	24.352551
132.209812	4711.106810	24.357568
132.657326	4729.701121	24.362586
132.670609	4732.950221	24.367603
133.002737	4736.401891	24.372621
132.586658	4741.511159	24.377639
132.823543	4757.316573	24.382656
133.254194	4754.256700	24.387674
133.224672	4771.906234	24.392691
133.824500	4786.755204	24.397709
133.664665	4799.652520	24.402727
133.923362	4793.008517	24.407744
133.602041	4798.491208	24.412762
133.866671	4814.194472	24.417779
134.391020	4809.999344	24.422797
134.274122	4822.773158	24.427815
134.443510	4832.440295	24.432832
134.660549	4846.029855	24.437850
135.018769	4850.765324	24.442867
135.346415	4846.294821	24.447885
135.012324	4840.103515	24.452903
135.387852	4860.262251	24.457920
135.222621	4871.547473	24.462938
135.421538	4875.405137	24.467955
135.789993	4867.370818	24.472973
135.594781	4885.583032	24.477991
136.110680	4895.303238	24.483008
135.975806	4892.919058	24.488026
135.882745	4893.943704	24.493043
136.261857	4917.201664	24.498061
136.313084	4926.467543	24.503079
136.318339	4919.471788	24.508096
136.496024	4944.412213	24.513114
136.617378	4957.555990	24.518131
136.893724	4957.964057	24.523149
137.160107	4976.157705	24.528167
137.705223	4971.078609	24.533184
137.378879	4979.964906	24.538202
137.351403	4983.899096	24.543219
138.051308	4986.807087	24.548237
137.676742	5011.515310	24.553255
138.038588	4999.387910	24.558272
138.389299	5000.548214	24.563290
138.196937	5015.407845	24.568307
138.699558	5020.262782	24.573325
138.677897	5027.750360	24.578343
138.801901	5021.910204	24.583360
139.008642	5034.507200	24.588378
138.775832	5038.520920	24.593395
139.270513	5045.144784	24.598413
139.342644	5063.501529	24.603431
139.793726	5050.829810	24.608448
139.665206	5053.053203	24.613466
139.670741	5075.220901	24.618483
139.996946	5076.214595	24.623501
139.798843	5082.236780	24.628519
140.108469	5081.317032	24.633536
140.516814	5091.464548	24.638554
140.117609	5103.853493	24.643571
140.498496	5102.196567	24.648589
140.435080	5118.131412	24.653607
140.874250	5123.943291	24.658624
140.937436	5133.030633	24.663642
140.734891	5129.542749	24.668659
141.113342	5136.181700	24.673677
141.097640	5150.357195	24.678695
141.460333	5149.804763	24.683712
141.532252	5166.876915	24.688730
141.513682	5175.879232	24.693747
141.767433	5173.159508	24.698765
141.655479	5185.661334	24.703783
141.945362	5202.206943	24.708800
142.481790	5204.051556	24.713818
142.495052	5211.195983	24.718835
142.674980	5204.930337	24.723853
142.667543	5212.197957	24.728871
142.767239	5220.976590	24.733888
143.111476	5228.473216	24.738906
142.687018	5230.623042	24.743923
142.983343	5238.565946	24.748941
143.098753	5251.843444	24.753959
143.371905	5259.941504	24.758976
143.642602	5283.213760	24.763994
143.708711	5293.942160	24.769011
144.149325	5290.037824	24.774029
144.212768	5299.898578	24.779047
144.280851	5313.950593	24.784064
144.429539	5307.509878	24.789082
144.224447	5310.392404	24.794099
144.610683	5330.985596	24.799117
144.670263	5335.954220	24.804135
144.894556	5336.771341	24.809152
145.327588	5349.746621	24.814170
145.175273	5362.554770	24.819187
145.484878	5365.546067	24.824205
145.679978	5366.367763	24.829223
145.841990	5379.473909	24.834240
146.446886	5383.624777	24.839258
146.210279	5393.074878	24.844275
145.967341	5391.664020	24.849293
146.045872	5395.300751	24.854311
146.052282	5405.669245	24.859328
146.593317	5414.577696	24.864346
146.849302	5433.922445	24.869363
147.041812	5435.435853	24.874381
147.138270	5434.227507	24.879399
147.242374	5431.202899	24.884416
147.618448	5456.308655	24.889434
147.534821	5480.154362	24.894451
148.098222	5459.951959	24.899469
148.300176	5456.694209	24.904487
148.223485	5467.523999	24.909504
148.228738	5467.804091	24.914522
148.131599	5495.790290	24.919539
148.655326	5495.698744	24.924557
148.531769	5490.765300	24.929575
148.733603	5506.996690	24.934592
148.806444	5514.529639	24.939610
148.704820	5523.257884	24.944627
148.937422	5523.290863	24.949645
149.249803	5533.573614	24.954663
148.991991	5553.560868	24.959680
149.308565	5560.588467	24.964698
149.332903	5568.037494	24.969715
150.008032	5571.397708	24.974733
149.968542	5587.809026	24.979751
149.809750	5598.380283	24.984768
150.069788	5603.424902	24.989786
149.980029	5620.715364	24.994803
150.450689	5620.906762	24.999821
150.825877	5639.671168	25.004839
150.792114	5645.696200	25.009856
151.203780	5646.468198	25.014874
150.818438	5657.819956	25.019891
151.395448	5672.436476	25.024909
151.512413	5672.992641	25.029927
151.646856	5689.493598	25.034944
152.159265	5696.872527	25.039962
151.987834	5708.765320	25.044979
152.136226	5699.934907	25.049997
151.897465	5705.764794	25.055015
152.397176	5727.208744	25.060032
153.126298	5721.409302	25.065050
152.830598	5738.675319	25.070067
153.017012	5746.619880	25.075085
153.161258	5737.098784	25.080103
153.282057	5753.513549	25.085120
153.621906	5751.433687	25.090138
153.229472	5768.617029	25.095155
153.675962	5759.421060	25.100173
153.673807	5776.442253	25.105191
153.650950	5778.406114	25.110208
153.895227	5784.614915	25.115226
154.065171	5806.467328	25.120243
154.236679	5817.492036	25.125261
154.608488	5814.797916	25.130279
154.592573	5835.814545	25.135296
154.828983	5846.425046	25.140314
154.802930	5846.012416	25.145331
154.963106	5848.048624	25.150349
155.430962	5864.781609	25.155367
155.283471	5870.063766	25.160384
155.900888	5882.600168	25.165402
155.634353	5896.275739	25.170419
155.879744	5891.281229	25.175437
155.809680	5896.336608	25.180455
156.333317	5915.074883	25.185472
156.446998	5920.707572	25.190490
156.540980	5929.380112	25.195507
156.795937	5942.254287	25.200525
156.964920	5945.930622	25.205543
157.221789	5952.200642	25.210560
157.440440	5966.684138	25.215578
157.032220	5971.581013	25.220595
157.579420	5972.072941	25.225613
157.729538	5979.259362	25.230631
157.768963	5993.108044	25.235648
158.071322	5991.169768	25.240666
157.966216	6008.134700	25.245683
158.202934	6023.912828	25.250701
158.488612	6025.822066	25.255719
158.624464	6026.896144	25.260736
159.173149	6045.172903	25.265754
159.098668	6052.429263	25.270771
159.090482	6054.779135	25.275789
159.405753	6062.949872	25.280807
159.527382	6081.991212	25.285824
159.613568	6083.590781	25.290842
159.791348	6084.219506	25.295859
159.383241	6095.511965	25.300877
159.910582	6095.953344	25.305895
159.996856	6121.544203	25.310912
160.526307	6134.880592	25.315930
160.301568	6137.668464	25.320947
160.464498	6149.392360	25.325965
161.014266	6156.317364	25.330983
160.972881	6160.474959	25.336000
161.052073	6177.985706	25.341018
161.339510	6186.438654	25.346035
161.438177	6198.794532	25.351053
161.499842	6196.395173	25.356071
161.793724	6218.266542	25.361088
162.072435	6211.451583	25.366106
162.109571	6230.948262	25.371123
162.140003	6238.402921	25.376141
162.800526	6246.257640	25.381159
162.815177	6246.990847	25.386176
162.903782	6258.726457	25.391194
163.041064	6272.560020	25.396211
163.077746	6270.508654	25.401229
163.411288	6262.469727	25.406247
163.407125	6286.288250	25.411264
163.868999	6289.574680	25.416282
163.726164	6292.804321	25.421299
163.891136	6302.375069	25.426317
163.802767	6307.891162	25.431335
163.979423	6325.320487	25.436352
164.383206	6325.446611	25.441370
164.853109	6344.761968	25.446387
164.881931	6354.796024	25.451405
164.819758	6339.144896	25.456423
164.708478	6354.548504	25.461440
165.182736	6374.352513	25.466458
165.444743	6377.641861	25.471475
165.230885	6385.605213	25.476493
165.700818	6391.605246	25.481511
165.577063	6406.079596	25.486528
166.060984	6412.336302	25.491546
166.241049	6427.230278	25.496563
166.432215	6432.112293	25.501581
166.433320	6437.907990	25.506599
166.570585	6461.404686	25.511616
166.663188	6467.072413	25.516634
166.780513	6469.494222	25.521651
166.931588	6490.397050	25.526669
167.532299	6505.193621	25.531687
167.455803	6518.827256	25.536704
167.697551	6523.928662	25.541722
167.747932	6525.707504	25.546739
167.842348	6544.005420	25.551757
168.405162	6540.280560	25.556775
168.287393	6562.671413	25.561792
168.550685	6570.244410	25.566810
168.922786	6579.429290	25.571827
168.981456	6594.146696	25.576845
168.979699	6593.689204	25.581863
169.112984	6610.819382	25.586880
169.293814	6620.981298	25.591898
169.438521	6627.247025	25.596915
169.244136	6638.178022	25.601933
170.040398	6641.317425	25.606951
169.896444	6652.123726	25.611968
170.207646	6668.897775	25.616986
170.502271	6673.912018	25.622003
170.361717	6686.687679	25.627021
170.944951	6696.679263	25.632039
171.129635	6702.986105	25.637056
171.003672	6721.012508	25.642074
171.101606	6733.776095	25.647091
171.333994	6726.592538	25.652109
171.919679	6741.953576	25.657127
171.983755	6767.678246	25.662144
172.246801	6758.002265	25.667162
172.714679	6760.659626	25.672180
172.716729	6783.174035	25.677197
173.135618	6783.499836	25.682215
173.046032	6785.022827	25.687232
172.978335	6779.556243	25.692250
173.039102	6786.662274	25.697268
172.862151	6808.488147	25.702285
173.249080	6811.562277	25.707303
173.350140	6822.781726	25.712320
173.700245	6836.408745	25.717338
173.792416	6841.022259	25.722356
173.954049	6858.145070	25.727373
174.452330	6860.109483	25.732391
174.619728	6862.921267	25.737408
175.204939	6870.911175	25.742426
175.114585	6863.273025	25.747444
174.954391	6875.751991	25.752461
174.971930	6879.480652	25.757479
174.853913	6896.798840	25.762496
175.248371	6904.499801	25.767514
175.853923	6919.507462	25.772532
176.209840	6931.574138	25.777549
176.033059	6919.902369	25.782567
176.061612	6939.675794	25.787584
175.930805	6943.642377	25.792602
176.228647	6944.593269	25.797620
176.268191	6968.478437	25.802637
176.621707	6976.151116	25.807655
176.843933	6992.513218	25.812672
177.041853	7010.861679	25.817690
177.347588	7013.995917	25.822708
177.161300	7029.891690	25.827725
177.760627	7029.128508	25.832743
177.663342	7045.190295	25.837760
177.733737	7049.939864	25.842778
178.245322	7064.886599	25.847796
178.197207	7087.415553	25.852813
178.398475	7085.379353	25.857831
178.345400	7104.780599	25.862848
178.609573	7120.886847	25.867866
178.713952	7135.098731	25.872884
178.847559	7146.253298	25.877901
179.306806	7162.357434	25.882919
179.512489	7173.311309	25.887936
179.823019	7186.970044	25.892954
180.000185	7189.079508	25.897972
180.148055	7199.944591	25.902989
180.496016	7211.895891	25.908007
180.675001	7221.278664	25.913024
180.522210	7223.862854	25.918042
180.973814	7242.212844	25.923060
180.799423	7250.776519	25.928077
181.512373	7274.547116	25.933095
181.483202	7281.219140	25.938112
181.474934	7280.308050	25.943130
181.960771	7292.439847	25.948148
181.741376	7314.437131	25.953165
182.035570	7318.422451	25.958183
182.316056	7322.662476	25.963200
182.475250	7341.683452	25.968218
182.949285	7358.173749	25.973236
182.744755	7366.480171	25.978253
183.149987	7380.474637	25.983271
183.176924	7391.718673	25.988288
183.388651	7403.000064	25.993306
183.869223	7414.763401	25.998324
184.199727	7416.725748	26.003341
184.229048	7424.269456	26.008359
184.428407	7438.899201	26.013376
184.452186	7453.894261	26.018394
184.718503	7447.548023	26.023412
184.758896	7460.327442	26.028429
184.948891	7479.356363	26.033447
185.259164	7491.193784	26.038464
185.151989	7500.504721	26.043482
185.830009	7508.180456	26.048500
185.675420	7521.625019	26.053517
185.626566	7524.881192	26.058535
185.785564	7538.311367	26.063552
186.099707	7561.235598	26.068570
186.513049	7563.945820	26.073588
186.602252	7556.111932	26.078605
186.724205	7577.323629	26.083623
187.168137	7586.235730	26.088640
187.113803	7586.547288	26.093658
187.701720	7596.046138	26.098676
188.040458	7616.633559	26.103693
187.981830	7620.611078	26.108711
187.894940	7620.365789	26.113728
188.324777	7629.879951	26.118746
188.703748	7629.466970	26.123764
188.578932	7640.687576	26.128781
188.855072	7638.664843	26.133799
188.858640	7661.139045	26.138816
188.962120	7672.456501	26.143834
189.112980	7677.569311	26.148852
189.094028	7690.323459	26.153869
189.252812	7696.915676	26.158887
189.389565	7727.463703	26.163904
189.647901	7736.878506	26.168922
189.987366	7740.831570	26.173940
189.807365	7756.749083	26.178957
190.378946	7771.131357	26.183975
190.719648	7787.586102	26.188992
190.468618	7806.305607	26.194010
191.328993	7805.681453	26.199028
191.300412	7818.658191	26.204045
191.445349	7838.401719	26.209063
191.543353	7851.260781	26.214080
191.861674	7861.998526	26.219098
192.081349	7866.816474	26.224116
192.178349	7887.887212	26.229133
192.221772	7892.900102	26.234151
192.476607	7906.545997	26.239168
192.609796	7929.893667	26.244186
192.995709	7935.294902	26.249204
192.972604	7950.152485	26.254221
192.961297	7964.730409	26.259239
193.246765	7976.793023	26.264256
193.822424	7996.301918	26.269274
194.253629	8005.459311	26.274292
194.176644	8021.976543	26.279309
194.485352	8036.333908	26.284327
194.869787	8037.640672	26.289344
195.147978	8043.298753	26.294362
195.409779	8051.791308	26.299380
195.551595	8070.083314	26.304397
195.460428	8069.399854	26.309415
195.654264	8082.692370	26.314432
195.665547	8098.936961	26.319450
196.250418	8095.972356	26.324468
196.068245	8118.577239	26.329485
196.030596	8118.883035	26.334503
196.738921	8139.400512	26.339520
196.656462	8151.675577	26.344538
197.236988	8155.268942	26.349556
197.247437	8173.610045	26.354573
197.019926	8179.287406	26.359591
197.692418	8194.683420	26.364608
198.176623	8199.684168	26.369626
198.113345	8199.694055	26.374644
198.229436	8215.745531	26.379661
198.440902	8228.227170	26.384679
199.193971	8220.026960	26.389696
198.618092	8245.389849	26.394714
198.958867	8256.809402	26.399732
199.249395	8268.183162	26.404749
199.286603	8281.992869	26.409767
199.495252	8289.199440	26.414784
199.810787	8295.697858	26.419802
199.620174	8300.305524	26.424820
200.060128	8323.438306	26.429837
200.280377	8325.844238	26.434855
200.910924	8339.371609	26.439872
200.651871	8342.452484	26.444890
201.145677	8339.603136	26.449908
201.440457	8363.014438	26.454925
201.093411	8370.731151	26.459943
201.335322	8374.952207	26.464960
201.646385	8396.602474	26.469978
201.927982	8395.898491	26.474996
202.087739	8419.605689	26.480013
202.239023	8424.747054	26.485031
202.508924	8433.958345	26.490048
202.046408	8448.635750	26.495066
202.981236	8466.497672	26.500084
202.891394	8480.485289	26.505101
202.936348	8495.490505	26.510119
203.212780	8503.835746	26.515136
203.274445	8529.487476	26.520154
203.494632	8532.881637	26.525172
203.689575	8558.310469	26.530189
203.976593	8566.878240	26.535207
204.339442	8588.934209	26.540224
204.437581	8600.038381	26.545242
204.571283	8618.101726	26.550260
205.249169	8632.389091	26.555277
205.475883	8646.264098	26.560295
205.758684	8652.148963	26.565312
205.575392	8670.981857	26.570330
206.218587	8675.080130	26.575348
206.601287	8691.671176	26.580365
206.547252	8702.496158	26.585383
207.284534	8707.965708	26.590400
206.888838	8713.057083	26.595418
206.948310	8720.208262	26.600436
207.511672	8732.521455	26.605453
207.345659	8742.678891	26.610471
207.839891	8749.922989	26.615488
207.687930	8763.424870	26.620506
208.128152	8780.284817	26.625524
208.262486	8793.236716	26.630541
208.268959	8816.965278	26.635559
208.739131	8820.563435	26.640576
208.635041	8841.647817	26.645594
209.161472	8844.829885	26.650612
209.252817	8866.534066	26.655629
209.228553	8889.696078	26.660647
209.651561	8888.578428	26.665664
209.772136	8916.857749	26.670682
209.846699	8924.420239	26.675700
210.117892	8944.975520	26.680717
210.408464	8964.211219	26.685735
210.803085	8962.753873	26.690752
211.132622	8988.563179	26.695770
211.187877	8997.732603	26.700788
211.616533	9001.372030	26.705805
211.827250	9025.008873	26.710823
212.325887	9026.247305	26.715840
212.299033	9030.201204	26.720858
212.063789	9051.738914	26.725876
212.763772	9061.678771	26.730893
212.682548	9070.402338	26.735911
212.960476	9083.057262	26.740928
212.934685	9093.016116	26.745946
213.039147	9109.240679	26.750964
213.179688	9119.201905	26.755981
213.562276	9128.556910	26.760999
213.949000	9137.342963	26.766016
214.018933	9152.458458	26.771034
214.128685	9160.672245	26.776052
214.456468	9176.097822	26.781069
214.994954	9193.280580	26.786087
214.877859	9202.717059	26.791104
215.180519	9220.470366	26.796122
214.879874	9219.623928	26.801140
215.538558	9235.594443	26.806157
215.379587	9261.606948	26.811175
215.880737	9275.808837	26.816192
215.835224	9298.681059	26.821210
216.160695	9308.253484	26.826228
216.487131	9322.315442	26.831245
216.747721	9332.434784	26.836263
217.255569	9344.586588	26.841280
217.015913	9361.244157	26.846298
217.562318	9380.361277	26.851316
217.915662	9390.245108	26.856333
217.956482	9407.322904	26.861351
218.498318	9421.679554	26.866368
218.554336	9434.461044	26.871386
218.820917	9445.012062	26.876404
219.353562	9454.649985	26.881421
219.274030	9470.894216	26.886439
219.510853	9478.491502	26.891456
219.495809	9492.840726	26.896474
219.626120	9501.660807	26.901492
219.882180	9514.003718	26.906509
220.446120	9533.582377	26.911527
220.443506	9536.121258	26.916544
220.362776	9552.406793	26.921562
220.326090	9565.111333	26.926580
220.729162	9586.587552	26.931597
221.032811	9599.384037	26.936615
221.825923	9614.399246	26.941632
221.643562	9633.267697	26.946650
222.276871	9649.760351	26.951668
222.314957	9660.969286	26.956685
222.499389	9683.714395	26.961703
222.875463	9688.808268	26.966720
223.307082	9705.187328	26.971738
223.050214	9715.176399	26.976756
223.494218	9725.829234	26.981773
223.997367	9738.645080	26.986791
223.811147	9751.534198	26.991808
223.999309	9762.331327	26.996826
224.017511	9774.155975	27.001844
224.432723	9785.059630	27.006861
224.809829	9803.929017	27.011879
224.818979	9814.817367	27.016896
224.976354	9832.205661	27.021914
225.115940	9855.431612	27.026932
225.801961	9866.864379	27.031949
225.466394	9891.756137	27.036967
226.244320	9899.098329	27.041984
226.333360	9914.091468	27.047002
226.554450	9927.071611	27.052020
227.028760	9936.393712	27.057037
227.029925	9948.063269	27.062055
227.103585	9959.585708	27.067072
227.512275	9971.137763	27.072090
227.874411	9984.013758	27.077108
227.916755	9990.347182	27.082125
228.137068	10003.387491	27.087143
228.407719	10024.439765	27.092160
228.732206	10028.323049	27.097178
228.687862	10040.722842	27.102196
228.946784	10048.648429	27.107213
228.942936	10062.854254	27.112231
229.081835	10078.903766	27.117248
229.434004	10097.600541	27.122266
229.674750	10117.063102	27.127284
230.029047	10124.446488	27.132301
230.039369	10149.252828	27.137319
230.603296	10154.156372	27.142336
230.830783	10163.125730	27.147354
230.854307	10187.415389	27.152372
231.050896	10204.693692	27.157389
231.220996	10214.827690	27.162407
231.742169	10234.214868	27.167424
231.905225	10242.392365	27.172442
231.765056	10264.150229	27.177460
232.060474	10273.121628	27.182477
232.406769	10292.880425	27.187495
232.584613	10315.557872	27.192512
232.990240	10328.553592	27.197530
232.933979	10349.379587	27.202548
233.338783	10359.315865	27.207565
233.582842	10373.874617	27.212583
234.208938	10395.244209	27.217600
234.415857	10405.561992	27.222618
234.219696	10426.119500	27.227636
234.828049	10438.692010	27.232653
234.855303	10459.160878	27.237671
235.189117	10466.664437	27.242688
235.549383	10472.613526	27.247706
235.904543	10497.975704	27.252724
236.159319	10509.293290	27.257741
236.324417	10520.883846	27.262759
236.701160	10540.527623	27.267776
236.958426	10545.368799	27.272794
236.837100	10562.169931	27.277812
237.455612	10571.987593	27.282829
237.804031	10582.169637	27.287847
237.551164	10602.303642	27.292864
237.862536	10608.484617	27.297882
237.902288	10631.774536	27.302900
237.961318	10639.614860	27.307917
238.272223	10671.337141	27.312935
238.396726	10681.958481	27.317952
238.732155	10696.727355	27.322970
238.571246	10725.296643	27.327988
239.465284	10741.231586	27.333005
239.740379	10757.923429	27.338023
240.166033	10774.329625	27.343040
240.543209	10792.053812	27.348058
240.449984	10807.852977	27.353076
240.672674	10826.652862	27.358093
241.028567	10832.811150	27.363111
241.196705	10850.953361	27.368128
241.487443	10859.900515	27.373146
241.523915	10892.319777	27.378164
242.045068	10894.258951	27.383181
242.303543	10908.894800	27.388199
242.279093	10930.284819	27.393216
242.699619	10935.990956	27.398234
242.795309	10956.317028	27.403252
243.328805	10953.476865	27.408269
243.692017	10978.813173	27.413287
243.085281	10993.088887	27.418304
243.428782	10999.220753	27.423322
243.860695	11027.091376	27.428340
244.372836	11047.923832	27.433357
244.763799	11054.351410	27.438375
244.888120	11073.905829	27.443392
244.932982	11083.343144	27.448410
245.090757	11105.528949	27.453428
245.533004	11118.731042	27.458445
245.694183	11140.742687	27.463463
246.099054	11146.107162	27.468480
246.038329	11160.022756	27.473498
246.050383	11177.302445	27.478516
246.503387	11195.956105	27.483533
246.811503	11204.398641	27.488551
247.230681	11229.082367	27.493568
247.414627	11245.362645	27.498586
247.262145	11262.627139	27.503604
247.699754	11274.630170	27.508621
248.101836	11296.923181	27.513639
248.341908	11314.145174	27.518656
248.802951	11330.211605	27.523674
248.984389	11349.583694	27.528692
249.250236	11362.118911	27.533709
249.615141	11374.464949	27.538727
249.610376	11397.781737	27.543744
249.441818	11400.975239	27.548762
250.014632	11420.747108	27.553780
250.385396	11448.981594	27.558797
250.695603	11459.460608	27.563815
250.831576	11484.605846	27.568832
251.236213	11490.459895	27.573850
251.475698	11516.782558	27.578868
251.611921	11531.371734	27.583885
251.848728	11541.224441	27.588903
252.046643	11572.157582	27.593920
252.607313	11582.638479	27.598938
252.575352	11602.145303	27.603956
252.975920	11623.848453	27.608973
252.989471	11641.560938	27.613991
253.641388	11656.356776	27.619008
253.924211	11666.837037	27.624026
254.223313	11699.964923	27.629044
254.325790	11706.087414	27.634061
255.023618	11729.856622	27.639079
255.140889	11737.419876	27.644096
255.334882	11745.391090	27.649114
255.430411	11774.613337	27.654132
255.788687	11785.691283	27.659149
255.813101	11797.298352	27.664167
256.087593	11818.026796	27.669184
256.179785	11826.531857	27.674202
256.038436	11849.333788	27.679220
256.183724	11869.125737	27.684237
256.833317	11884.313678	27.689255
256.922201	11914.200305	27.694272
257.296399	11926.178953	27.699290
257.315463	11963.039409	27.704308
257.577808	11976.396599	27.709325
258.428604	11994.688752	27.714343
258.386408	12017.759552	27.719360
258.894240	12039.159022	27.724378
259.192090	12056.833677	27.729396
259.322707	12066.384362	27.734413
259.718704	12093.621169	27.739431
260.288033	12116.574188	27.744448
260.194130	12119.588753	27.749466
260.507882	12145.265949	27.754484
260.438556	12154.548011	27.759501
261.149865	12175.581038	27.764519
260.739764	12200.269636	27.769536
261.504328	12213.873573	27.774554
262.083747	12245.973278	27.779572
262.155191	12248.049361	27.784589
262.504999	12254.048024	27.789607
262.157356	12274.504967	27.794624
262.487369	12292.702156	27.799642
263.066998	12310.481324	27.804660
263.257531	12322.820566	27.809677
263.712314	12341.209830	27.814695
263.930489	12362.680307	27.819712
264.352004	12368.645669	27.824730
264.480419	12381.537824	27.829748
264.350141	12395.667324	27.834765
264.290455	12412.416240	27.839783
264.778373	12428.523611	27.844800
265.373947	12453.159207	27.849818
265.774842	12479.401089	27.854836
266.043798	12485.766170	27.859853
266.345839	12507.065781	27.864871
266.243556	12519.343655	27.869888
266.831592	12540.661660	27.874906
266.958012	12560.327819	27.879924
267.150561	12568.002770	27.884941
267.441104	12594.969457	27.889959
267.653432	12620.009513	27.894976
267.911027	12634.978419	27.899994
268.197589	12654.929060	27.905012
268.482972	12673.600972	27.910029
268.666627	12698.424572	27.915047
269.034228	12718.722582	27.920064
269.285732	12731.753588	27.925082
269.607580	12755.393518	27.930100
270.198713	12788.085992	27.935117
270.532771	12798.438859	27.940135
270.620834	12820.994445	27.945152
270.693352	12827.990413	27.950170
270.911363	12846.167787	27.955188
271.347612	12862.286781	27.960205
271.706838	12880.085224	27.965223
271.707276	12900.488315	27.970240
272.180150	12915.480562	27.975258
272.449737	12935.367842	27.980276
272.349854	12952.256164	27.985293
273.223832	12969.686686	27.990311
273.148005	12996.670286	27.995328
273.408183	13010.770658	28.000346
273.569135	13042.703586	28.005364
273.666992	13051.239891	28.010381
274.267620	13069.461755	28.015399
274.511685	13095.460636	28.020416
274.622213	13120.814147	28.025434
275.383019	13155.315439	28.030452
275.328864	13168.700948	28.035469
275.523029	13179.366469	28.040487
275.832849	13202.475149	28.045504
276.287180	13209.203022	28.050522
276.550770	13240.242293	28.055540
277.079921	13267.684150	28.060557
277.339142	13274.291028	28.065575
277.246690	13301.350297	28.070592
277.927837	13309.861664	28.075610
278.341728	13328.785678	28.080628
278.418792	13353.017346	28.085645
278.987084	13354.406229	28.090663
278.919049	13374.147906	28.095680
279.054654	13391.084995	28.100698
279.522698	13408.926892	28.105716
279.572211	13424.487983	28.110733
280.112284	13442.514423	28.115751
280.214881	13461.481017	28.120768
280.460647	13477.459844	28.125786
280.978266	13493.317149	28.130804
281.271184	13519.858452	28.135821
281.659374	13521.929268	28.140839
281.507777	13527.526868	28.145856
281.742326	13551.175151	28.150874
281.824811	13568.205985	28.155892
281.991473	13597.511487	28.160909
282.355662	13606.495814	28.165927
282.821553	13643.640086	28.170944
283.012329	13655.749624	28.175962
283.367408	13669.049273	28.180980
283.765429	13699.190305	28.185997
283.747743	13711.114629	28.191015
283.695955	13730.888869	28.196032
283.975739	13760.164269	28.201050
284.732388	13787.220698	28.206068
284.754278	13812.873243	28.211085
285.153528	13825.155505	28.216103
285.257205	13858.662014	28.221120
285.537110	13873.789467	28.226138
285.967451	13898.155973	28.231156
286.482290	13929.021216	28.236173
286.547742	13950.804801	28.241191
287.563666	13974.899664	28.246208
287.457574	13991.991999	28.251226
287.452649	14007.713683	28.256244
287.927492	14033.614536	28.261261
288.416499	14051.949575	28.266279
288.475885	14084.367562	28.271296
288.771331	14096.460984	28.276314
289.272023	14119.253494	28.281332
289.635783	14144.963466	28.286349
290.171944	14155.891774	28.291367
290.276171	14182.953068	28.296384
290.356620	14200.426923	28.301402
290.808945	14218.944724	28.306420
290.932192	14239.427915	28.311437
291.291444	14262.388026	28.316455
291.454401	14282.855569	28.321472
291.206790	14312.242857	28.326490
292.171759	14329.789867	28.331508
292.414916	14353.800986	28.336525
292.432216	14374.083006	28.341543
292.706628	14404.285574	28.346560
293.236469	14425.305321	28.351578
293.490340	14439.660397	28.356596
293.549760	14472.656980	28.361613
294.198633	14494.469805	28.366631
294.220217	14518.597953	28.371648
294.704451	14544.801216	28.376666
295.049903	14559.419955	28.381684
295.261981	14595.513116	28.386701
295.427130	14617.382907	28.391719
295.992620	14643.526204	28.396736
296.159094	14657.610897	28.401754
296.437116	14684.456186	28.406772
296.768038	14702.674498	28.411789
297.203265	14720.532243	28.416807
297.645389	14740.435442	28.421824
297.627861	14763.170941	28.426842
298.101069	14788.327740	28.431860
298.190053	14806.075577	28.436877
298.540242	14826.217501	28.441895
298.774649	14849.766356	28.446912
298.726939	14872.080352	28.451930
299.071032	14890.716824	28.456948
299.343446	14923.437637	28.461965
299.965394	14933.004389	28.466983
300.435087	14958.354616	28.472000
300.545528	14985.201312	28.477018
300.902010	14997.901605	28.482036
301.598896	15020.269680	28.487053
301.393622	15039.655587	28.492071
302.026008	15057.896496	28.497088
302.196504	15082.782119	28.502106
302.371762	15102.639068	28.507124
302.500678	15124.215080	28.512141
303.233278	15144.300594	28.517159
303.222514	15159.499867	28.522176
303.639908	15182.660425	28.527194
304.231311	15207.969810	28.532212
304.013570	15231.523640	28.537229
304.470730	15254.349594	28.542247
304.866503	15274.955435	28.547264
305.268756	15295.658192	28.552282
305.676662	15311.477352	28.557300
306.205189	15336.054556	28.562317
306.357676	15350.520948	28.567335
306.498407	15360.245412	28.572352
306.845970	15386.739697	28.577370
307.085252	15399.490199	28.582388
307.318616	15432.211683	28.587405
307.640107	15463.122331	28.592423
308.180268	15485.847126	28.597440
308.211014	15500.860143	28.602458
308.767820	15530.537030	28.607476
308.652439	15540.500681	28.612493
309.072867	15573.673170	28.617511
309.194650	15602.246569	28.622528
309.277585	15622.472254	28.627546
309.696008	15643.817158	28.632564
310.066853	15693.752701	28.637581
310.541218	15713.664498	28.642599
310.803397	15737.566991	28.647616
311.095906	15765.880170	28.652634
311.961041	15781.669155	28.657652
311.846256	15810.343088	28.662669
312.028044	15831.927406	28.667687
312.975154	15854.800505	28.672704
313.096664	15881.359309	28.677722
313.532928	15899.145351	28.682740
313.354214	15930.672035	28.687757
313.655727	15950.832243	28.692775
314.188580	15973.653515	28.697792
314.520068	16007.712408	28.702810
315.143446	16029.502557	28.707828
315.150019	16051.768360	28.712845
315.295536	16067.559763	28.717863
315.808773	16090.665347	28.722880
315.743729	16113.605710	28.727898
316.239837	16140.362026	28.732916
316.708546	16174.829268	28.737933
317.172230	16201.366498	28.742951
317.208598	16223.763647	28.747968
317.576438	16251.484587	28.752986
317.908643	16269.138825	28.758004
318.251192	16293.717964	28.763021
318.745508	16319.363032	28.768039
319.288246	16345.989150	28.773056
319.571385	16362.460417	28.778074
319.615766	16384.243754	28.783092
320.255992	16390.782557	28.788109
320.347811	16423.433147	28.793127
320.692615	16453.144672	28.798144
320.789404	16473.286961	28.803162
321.176929	16486.697199	28.808180
321.592731	16521.473406	28.813197
321.627025	16540.741176	28.818215
322.092382	16555.396354	28.823232
322.177175	16578.553845	28.828250
323.061511	16604.422465	28.833268
323.006685	16624.904514	28.838285
323.181964	16645.189455	28.843303
323.748674	16673.773712	28.848320
323.920954	16694.706673	28.853338
324.059131	16712.777053	28.858356
324.677463	16751.789125	28.863373
324.854778	16778.706815	28.868391
325.474451	16791.922975	28.873408
325.975406	16816.531663	28.878426
326.148248	16838.055340	28.883444
326.336349	16853.038445	28.888461
326.438799	16875.564975	28.893479
326.886434	16898.286987	28.898496
327.195543	16922.351004	28.903514
327.579277	16955.572688	28.908532
328.043120	16983.560756	28.913549
328.325205	17004.950639	28.918567
328.776735	17037.444846	28.923584
328.733797	17057.268506	28.928602
329.161530	17089.836018	28.933620
329.486582	17108.995638	28.938637
329.318902	17130.411892	28.943655
330.274075	17159.384541	28.948672
330.649297	17191.019185	28.953690
331.057115	17214.834368	28.958708
331.417494	17247.261084	28.963725
331.688791	17264.761528	28.968743
331.948647	17284.380058	28.973760
332.461017	17314.237227	28.978778
332.773698	17334.599287	28.983796
333.296090	17361.542701	28.988813
333.486083	17390.736635	28.993831
333.971885	17409.088029	28.998848
333.957551	17431.213401	29.003866
334.621720	17453.756851	29.008884
334.822918	17480.453830	29.013901
335.027843	17503.764180	29.018919
335.668352	17521.188071	29.023936
335.669033	17552.243926	29.028954
335.789312	17567.595138	29.033972
336.725439	17592.983175	29.038989
336.464976	17624.414872	29.044007
337.027239	17647.846307	29.049024
337.318666	17674.769480	29.054042
337.925842	17704.928271	29.059060
338.275742	17730.079812	29.064077
338.078327	17761.716646	29.069095
338.635182	17776.064661	29.074112
339.523012	17802.382881	29.079130
339.310363	17818.670880	29.084148
339.789814	17848.685649	29.089165
339.745446	17876.072335	29.094183
340.732423	17900.416751	29.099200
340.773119	17923.159491	29.104218
341.069791	17948.168034	29.109236
341.590098	17979.755972	29.114253
341.966521	18012.674219	29.119271
342.100737	18043.191909	29.124288
342.222707	18059.238170	29.129306
342.654236	18084.705895	29.134324
343.081588	18118.317586	29.139341
342.930256	18144.268376	29.144359
343.537371	18161.527503	29.149376
343.823867	18192.552246	29.154394
344.082932	18213.789133	29.159412
344.889014	18243.304803	29.164429
345.040158	18278.078245	29.169447
345.588670	18298.663398	29.174464
345.978716	18307.137322	29.179482
346.298345	18342.124555	29.184500
346.561228	18368.149747	29.189517
346.902506	18386.815317	29.194535
347.134664	18411.777705	29.199552
347.844237	18441.447782	29.204570
347.933531	18465.263856	29.209588
348.437981	18484.289336	29.214605
348.145181	18506.718575	29.219623
349.107892	18543.715530	29.224640
349.470999	18561.979837	29.229658
349.680665	18597.464897	29.234676
350.151588	18621.467773	29.239693
350.216922	18639.469230	29.244711
350.570831	18668.854211	29.249728
351.014969	18699.545503	29.254746
351.325148	18727.762330	29.259764
351.800633	18750.570602	29.264781
352.098930	18785.637787	29.269799
352.456380	18804.522346	29.274816
352.762128	18836.037884	29.279834
352.659133	18861.640898	29.284852
353.502147	18888.447765	29.289869
353.422434	18924.648431	29.294887
354.179528	18947.103252	29.299904
354.261386	18977.877002	29.304922
354.837003	19020.097140	29.309940
355.035025	19046.341886	29.314957
355.239900	19079.219314	29.319975
356.057480	19114.098345	29.324992
356.246484	19136.970899	29.330010
356.277322	19166.805261	29.335028
356.947566	19201.341091	29.340045
357.134901	19228.623887	29.345063
358.023309	19268.306323	29.350080
358.423385	19293.382531	29.355098
358.421854	19320.088520	29.360116
359.018531	19343.124902	29.365133
359.108103	19379.243032	29.370151
359.571736	19402.673082	29.375168
360.158851	19427.499037	29.380186
360.292023	19454.992807	29.385204
360.921795	19481.006241	29.390221
361.156442	19510.234268	29.395239
361.402952	19538.860273	29.400256
361.988426	19571.047113	29.405274
362.144402	19589.761817	29.410292
362.708939	19621.648756	29.415309
362.701373	19651.433011	29.420327
363.421275	19672.340263	29.425344
364.045417	19696.573185	29.430362
364.219996	19721.122960	29.435380
364.509304	19748.731682	29.440397
364.619690	19788.404366	29.445415
365.083756	19811.638980	29.450432
365.918315	19841.980283	29.455450
365.956284	19870.620485	29.460468
366.181494	19886.190857	29.465485
366.535069	19926.583899	29.470503
366.826243	19953.251220	29.475520
367.494968	19974.628036	29.480538
367.366103	20000.571451	29.485556
367.949736	20020.420022	29.490573
368.273579	20054.980032	29.495591
368.588137	20078.352108	29.500608
369.318424	20109.152430	29.505626
369.020996	20141.630143	29.510644
369.574587	20161.622563	29.515661
369.738814	20201.319240	29.520679
370.090233	20228.268135	29.525696
370.638792	20251.692218	29.530714
371.193454	20291.605922	29.535732
371.385136	20317.291043	29.540749
371.446358	20348.032269	29.545767
372.097801	20377.670171	29.550784
373.001345	20415.488684	29.555802
372.615693	20447.759582	29.560820
373.368293	20471.436289	29.565837
373.388635	20506.215228	29.570855
373.734151	20540.058730	29.575872
374.495542	20576.566659	29.580890
374.623085	20610.204330	29.585908
374.666614	20638.219265	29.590925
374.876305	20673.929226	29.595943
375.752240	20713.250085	29.600960
376.355977	20749.258607	29.605978
376.385219	20786.791454	29.610996
377.286167	20818.924611	29.616013
377.423866	20849.812601	29.621031
377.669747	20881.239714	29.626048
378.342497	20908.777369	29.631066
378.460840	20944.761185	29.636084
378.797362	20975.201212	29.641101
379.493918	21019.156924	29.646119
379.509569	21047.473775	29.651136
380.536987	21076.794784	29.656154
380.473830	21111.341449	29.661172
381.078796	21144.279718	29.666189
381.250830	21181.020093	29.671207
381.596054	21217.190016	29.676224
382.205706	21244.832804	29.681242
382.655561	21288.442329	29.686260
383.006282	21305.915004	29.691277
383.278861	21340.706452	29.696295
383.878600	21366.986156	29.701312
384.438740	21401.593660	29.706330
384.444602	21448.419736	29.711348
385.359416	21471.314011	29.716365
385.671723	21497.961161	29.721383
386.083329	21517.016775	29.726400
386.243970	21541.861662	29.731418
386.900883	21578.438365	29.736436
386.780824	21616.937653	29.741453
387.184565	21637.593232	29.746471
387.597520	21675.370960	29.751488
388.295846	21707.076045	29.756506
388.434644	21742.634759	29.761524
389.089551	21768.464050	29.766541
389.273881	21789.406904	29.771559
389.551600	21819.288760	29.776576
390.094852	21847.877964	29.781594
390.480877	21889.205120	29.786612
390.684330	21923.938916	29.791629
391.266409	21953.255165	29.796647
391.433523	21985.720011	29.801664
392.041068	22012.075177	29.806682
392.212389	22051.546990	29.811700
392.635236	22086.050823	29.816717
393.038793	22108.172884	29.821735
393.331272	22138.526821	29.826752
393.937698	22167.131866	29.831770
393.975832	22200.381844	29.836788
394.259253	22222.516531	29.841805
394.462605	22252.322227	29.846823
395.090276	22293.049997	29.851840
395.843862	22321.575345	29.856858
395.545042	22359.971379	29.861876
395.964284	22392.921867	29.866893
396.545601	22429.575175	29.871911
396.679267	22470.273267	29.876928
397.795368	22500.587214	29.881946
397.984132	22542.445826	29.886964
398.531495	22575.281764	29.891981
398.464516	22609.326122	29.896999
398.855637	22642.641610	29.902016
399.313308	22682.480558	29.907034
399.760981	22719.616621	29.912052
400.161483	22751.306840	29.917069
400.702310	22798.513596	29.922087
401.041383	22831.856510	29.927104
401.748073	22856.573280	29.932122
402.088332	22903.609492	29.937140
402.131795	22938.414357	29.942157
402.573897	22981.352685	29.947175
403.041135	23008.502082	29.952192
403.866884	23044.385225	29.957210
404.030253	23085.010412	29.962228
404.297629	23113.139124	29.967245
405.070999	23150.357678	29.972263
405.220669	23198.037394	29.977280
406.136505	23215.025132	29.982298
406.192339	23259.996139	29.987316
406.468607	23295.188545	29.992333
407.054231	23330.149301	29.997351
407.463718	23359.962284	30.002368
407.892304	23392.483259	30.007386
408.148420	23440.361735	30.012404
408.404003	23478.812105	30.017421
409.041765	23508.020822	30.022439
408.866682	23547.752078	30.027456
409.501955	23582.370579	30.032474
409.786523	23620.892515	30.037492
410.196682	23667.578339	30.042509
410.887989	23713.278658	30.047527
411.195398	23760.732792	30.052544
411.675591	23787.072347	30.057562
412.173542	23836.790735	30.062580
412.670643	23870.439241	30.067597
413.138560	23911.486039	30.072615
413.450095	23953.480047	30.077632
413.741919	23988.209923	30.082650
414.626724	24023.441002	30.087668
414.939143	24059.817142	30.092685
415.333438	24099.491905	30.097703
416.035308	24136.312737	30.102720
416.472990	24151.966937	30.107738
416.625301	24190.744506	30.112756
416.820604	24233.060641	30.117773
417.771121	24262.183557	30.122791
417.508951	24298.959786	30.127808
418.335723	24340.210355	30.132826
418.558161	24376.019769	30.137844
419.160423	24408.192899	30.142861
419.500656	24440.571431	30.147879
419.594288	24487.915424	30.152896
420.223174	24515.250098	30.157914
420.655159	24558.168122	30.162932
420.850532	24588.572597	30.167949
421.648364	24613.631170	30.172967
422.093419	24647.548238	30.177984
422.148570	24685.975446	30.183002
422.557351	24721.124326	30.188020
422.504240	24748.623018	30.193037
423.226401	24793.107601	30.198055
423.499981	24837.156971	30.203072
424.035306	24869.164376	30.208090
424.486460	24920.024003	30.213108
424.542617	24959.867187	30.218125
425.501572	25000.036700	30.223143
425.711847	25040.058133	30.228160
426.495135	25076.469798	30.233178
426.983802	25126.420349	30.238196
427.126888	25154.324928	30.243213
427.681122	25191.158184	30.248231
427.707784	25232.807663	30.253248
428.574433	25269.788042	30.258266
429.362386	25303.747307	30.263284
429.497766	25345.354711	30.268301
429.983044	25382.609907	30.273319
429.984434	25425.970099	30.278336
430.330357	25459.006645	30.283354
430.846247	25507.007360	30.288372
431.648924	25538.310367	30.293389
431.903424	25577.068283	30.298407
432.605777	25636.611833	30.303424
433.220642	25668.089818	30.308442
433.369636	25709.676881	30.313460
433.584851	25740.907901	30.318477
434.236420	25786.157811	30.323495
434.793757	25825.823085	30.328512
435.496894	25865.187521	30.333530
435.813858	25904.113241	30.338548
436.233325	25935.729689	30.343565
436.574605	25981.287759	30.348583
437.033350	26026.024887	30.353600
437.609973	26054.766570	30.358618
438.050075	26091.815271	30.363636
438.265168	26129.297447	30.368653
438.832260	26164.044845	30.373671
439.078077	26201.768827	30.378688
439.389515	26239.122354	30.383706
439.875731	26283.122617	30.388724
440.836264	26325.651934	30.393741
440.905314	26363.068936	30.398759
441.559162	26398.030673	30.403776
441.758919	26431.281308	30.408794
442.195144	26475.890236	30.413812
442.285895	26525.596886	30.418829
443.157606	26561.586574	30.423847
443.391596	26601.556824	30.428864
443.936161	26643.475700	30.433882
444.156860	26682.613922	30.438900
444.472151	26743.125151	30.443917
445.326092	26769.694487	30.448935
445.358253	26819.417354	30.453952
446.215307	26859.903590	30.458970
446.851176	26902.800987	30.463988
447.203417	26942.329927	30.469005
447.921079	26989.582039	30.474023
448.031035	27022.733944	30.479040
448.635547	27064.739106	30.484058
449.254804	27109.390282	30.489076
449.540491	27149.871785	30.494093
450.091447	27182.259633	30.499111
450.111005	27228.060507	30.504128
450.283899	27255.938031	30.509146
451.144180	27295.584016	30.514164
451.705688	27336.010047	30.519181
451.745938	27365.918400	30.524199
452.347868	27405.402810	30.529216
452.958395	27435.620132	30.534234
453.608420	27478.314273	30.539252
453.862584	27509.668326	30.544269
454.712633	27541.965657	30.549287
454.788066	27584.838507	30.554304
455.451080	27627.271784	30.559322
455.683429	27655.349121	30.564340
456.337440	27690.091841	30.569357
456.842620	27730.957277	30.574375
456.866219	27769.964127	30.579392
456.999960	27806.969135	30.584410
457.764803	27848.622133	30.589428
457.958191	27895.933186	30.594445
458.799895	27941.316140	30.599463
459.018717	27983.604832	30.604480
459.194630	28035.450848	30.609498
459.905912	28071.992957	30.614516
460.274397	28122.785083	30.619533
460.799532	28168.319258	30.624551
461.006613	28224.882436	30.629568
461.419219	28264.341278	30.634586
462.518127	28312.257310	30.639604
462.502102	28355.537987	30.644621
463.159564	28404.206020	30.649639
463.797033	28458.161481	30.654656
463.930908	28491.482685	30.659674
464.798108	28534.985689	30.664692
464.913655	28589.541550	30.669709
465.422883	28641.210477	30.674727
466.140016	28685.167122	30.679744
466.503956	28732.649342	30.684762
467.314298	28775.712981	30.689780
467.517676	28821.488632	30.694797
468.334841	28857.983958	30.699815
468.555589	28904.800025	30.704832
468.878240	28953.679828	30.709850
469.651472	28990.220197	30.714868
470.076084	29041.909708	30.719885
470.750666	29078.244451	30.724903
470.955949	29123.217711	30.729920
471.639927	29172.901098	30.734938
472.025217	29216.481030	30.739956
471.988042	29259.861741	30.744973
472.614173	29303.777076	30.749991
473.243341	29357.477041	30.755008
473.669678	29398.023137	30.760026
474.165582	29441.257525	30.765044
474.930988	29494.993399	30.770061
475.245711	29531.473804	30.775079
475.615419	29575.600554	30.780096
476.184392	29619.455985	30.785114
476.722660	29665.383338	30.790132
476.881887	29715.934051	30.795149
477.823134	29761.646793	30.800167
478.255025	29804.601195	30.805184
478.110648	29857.361659	30.810202
479.118249	29897.634382	30.815220
479.283499	29944.284511	30.820237
479.663041	29991.040249	30.825255
480.516706	30036.267939	30.830272
480.915558	30093.040107	30.835290
481.633222	30131.772057	30.840308
481.824857	30177.716915	30.845325
482.670745	30216.024375	30.850343
483.500933	30254.460792	30.855360
483.578976	30288.071789	30.860378
484.409372	30323.101093	30.865396
484.551833	30362.208028	30.870413
484.944304	30400.694312	30.875431
485.378376	30440.394181	30.880448
485.712055	30477.992178	30.885466
486.140223	30524.362222	30.890484
486.538838	30569.207211	30.895501
487.320834	30609.794806	30.900519
487.713071	30650.690064	30.905536
487.662620	30696.408489	30.910554
488.440736	30738.981890	30.915572
488.622368	30790.593731	30.920589
489.091553	30836.572438	30.925607
489.925391	30881.906230	30.930624
490.162196	30938.870460	30.935642
490.657132	30986.489069	30.940660
490.904710	31045.689739	30.945677
491.524749	31095.065368	30.950695
492.434516	31146.039356	30.955712
492.940532	31201.078299	30.960730
493.532541	31241.608387	30.965748
493.946271	31297.180413	30.970765
494.348538	31340.755845	30.975783
495.379312	31394.423488	30.980800
495.400282	31434.208928	30.985818
496.276118	31489.020025	30.990836
496.102036	31536.675142	30.995853
496.983929	31583.880497	31.000871
497.441133	31627.296203	31.005888
497.900296	31680.080562	31.010906
498.841239	31733.472350	31.015924
499.465504	31777.665072	31.020941
499.914596	31825.533013	31.025959
500.398721	31860.758234	31.030976
500.708387	31906.587282	31.035994
501.388568	31945.233666	31.041012
501.939449	31996.297561	31.046029
502.167208	32048.461622	31.051047
502.680891	32089.290115	31.056064
502.940535	32139.394792	31.061082
503.876981	32197.333932	31.066100
504.174114	32238.885725	31.071117
504.725175	32284.677795	31.076135
505.379174	32329.865900	31.081152
505.610347	32387.852812	31.086170
506.403939	32421.266675	31.091188
507.071465	32472.838192	31.096205
507.460593	32515.754326	31.101223
508.079077	32572.423004	31.106240
508.480903	32621.659414	31.111258
509.025545	32657.603539	31.116276
509.439466	32706.010062	31.121293
509.607460	32754.088532	31.126311
510.258238	32800.397171	31.131328
510.823437	32862.948227	31.136346
511.043672	32895.257766	31.141364
511.759722	32949.237916	31.146381
512.401914	32997.090942	31.151399
513.077547	33044.919873	31.156416
513.431076	33100.348073	31.161434
514.250039	33145.442560	31.166452
514.268334	33192.514960	31.171469
514.669031	33242.536962	31.176487
515.240945	33295.756621	31.181504
515.786045	33341.539292	31.186522
516.616470	33389.230964	31.191540
517.211202	33429.398182	31.196557
517.495623	33471.776311	31.201575
517.955457	33516.036395	31.206592
518.267218	33560.951998	31.211610
519.070307	33602.907749	31.216628
519.123259	33647.737626	31.221645
519.848778	33698.702452	31.226663
520.279757	33734.900154	31.231680
520.507356	33796.647021	31.236698
521.326236	33833.827338	31.241716
521.881384	33886.336685	31.246733
522.280466	33940.052905	31.251751
522.865912	33994.328063	31.256768
523.195268	34050.356865	31.261786
523.548801	34093.389281	31.266804
524.577516	34152.577555	31.271821
524.955115	34206.841556	31.276839
525.743452	34257.361640	31.281856
525.869987	34320.889861	31.286874
526.294778	34361.136055	31.291892
527.174886	34423.130300	31.296909
527.325247	34478.012267	31.301927
528.090959	34526.228783	31.306944
528.453644	34585.263357	31.311962
529.111820	34634.913238	31.316980
529.641826	34694.895602	31.321997
530.115610	34747.748614	31.327015
530.508635	34796.043085	31.332032
530.856238	34862.750247	31.337050
531.698378	34922.507333	31.342068
532.286536	34987.280386	31.347085
532.883660	35045.267881	31.352103
533.754384	35086.235960	31.357120
533.890719	35153.109903	31.362138
534.450590	35195.821396	31.367156
535.348441	35251.125734	31.372173
535.798493	35307.113668	31.377191
536.397157	35359.044476	31.382208
537.064675	35407.638784	31.387226
537.469879	35458.822420	31.392244
538.171817	35510.377018	31.397261
538.414335	35569.553288	31.402279
539.315828	35622.328846	31.407296
539.941390	35681.135610	31.412314
540.439378	35729.782499	31.417332
541.027314	35776.626001	31.422349
541.965122	35825.159963	31.427367
542.078494	35874.967628	31.432384
542.519180	35934.075936	31.437402
543.408390	35975.668822	31.442420
544.055785	36012.911447	31.447437
544.107231	36071.916700	31.452455
544.719832	36127.533565	31.457472
545.489068	36180.849719	31.462490
545.948954	36222.579882	31.467508
546.645260	36273.890610	31.472525
546.619440	36327.552962	31.477543
547.327862	36374.138628	31.482560
548.004620	36426.837562	31.487578
548.208870	36478.567301	31.492596
549.337803	36530.481149	31.497613
549.384406	36593.390032	31.502631
549.954055	36637.645761	31.507648
550.404665	36702.236908	31.512666
550.852369	36750.780183	31.517684
551.731290	36805.743745	31.522701
552.285314	36856.831550	31.527719
553.000734	36915.185009	31.532736
553.205552	36963.646664	31.537754
554.272063	37009.728675	31.542772
554.480030	37052.966936	31.547789
554.903951	37110.519249	31.552807
555.361952	37144.707694	31.557824
555.616179	37206.662641	31.562842
556.354545	37262.016148	31.567860
556.901468	37311.689698	31.572877
557.460275	37373.388750	31.577895
557.861511	37426.601235	31.582912
558.587012	37478.555278	31.587930
558.703923	37533.096230	31.592948
559.440189	37586.458993	31.597965
559.930056	37653.601567	31.602983
560.398209	37710.377086	31.608000
560.980466	37780.066634	31.613018
561.698940	37838.384185	31.618036
562.348980	37898.116458	31.623053
563.038585	37966.170946	31.628071
563.478196	38016.602799	31.633088
564.112275	38083.407945	31.638106
564.605880	38148.243332	31.643124
565.626594	38203.106060	31.648141
565.732359	38254.229450	31.653159
566.250562	38313.174084	31.658176
566.925123	38379.195985	31.663194
567.339620	38435.937553	31.668212
568.169438	38503.959131	31.673229
568.661549	38573.519914	31.678247
569.024805	38635.012901	31.683264
569.953031	38692.281773	31.688282
570.488000	38757.371789	31.693300
571.075487	38815.598668	31.698317
571.647970	38882.188272	31.703335
572.037062	38937.676675	31.708352
573.198692	39000.582379	31.713370
573.123475	39065.585491	31.718388
573.547079	39123.004100	31.723405
574.146075	39189.742272	31.728423
574.812512	39258.354648	31.733440
575.425529	39329.638031	31.738458
576.050442	39395.139587	31.743476
576.515896	39450.326436	31.748493
576.851091	39522.317992	31.753511
577.709942	39591.951088	31.758528
578.617530	39653.930885	31.763546
579.112813	39722.780231	31.768564
579.927925	39785.812050	31.773581
580.230162	39844.851593	31.778599
580.934581	39908.710602	31.783616
581.622234	39960.663893	31.788634
581.729401	40032.370312	31.793652
582.803401	40103.678901	31.798669
583.109496	40165.944088	31.803687
583.837154	40227.719702	31.808704
584.292700	40296.330435	31.813722
585.041740	40358.438260	31.818740
585.474152	40411.374928	31.823757
586.164007	40485.325268	31.828775
586.905281	40550.331423	31.833792
587.633959	40610.526861	31.838810
588.204311	40669.267342	31.843828
588.914979	40731.622566	31.848845
589.109332	40798.315202	31.853863
589.569790	40857.560384	31.858880
590.217389	40919.590824	31.863898
591.147702	40983.835020	31.868916
591.928076	41039.065112	31.873933
592.060744	41095.585800	31.878951
592.807376	41149.069551	31.883968
593.254542	41211.549631	31.888986
593.574511	41269.900865	31.894004
594.185166	41324.816729	31.899021
594.913721	41388.745856	31.904039
595.391537	41459.823360	31.909056
595.951071	41516.025291	31.914074
596.566094	41574.868724	31.919092
597.242925	41632.292223	31.924109
597.517780	41707.570302	31.929127
598.385364	41759.936097	31.934144
599.127508	41828.019736	31.939162
598.886298	41899.578107	31.944180
599.960614	41970.456321	31.949197
600.516945	42043.597953	31.954215
601.055328	42110.835227	31.959232
601.687840	42170.537694	31.964250
602.068522	42247.053366	31.969268
602.838082	42311.573294	31.974285
603.339802	42391.909732	31.979303
603.821084	42472.180089	31.984320
604.735813	42539.005530	31.989338
605.165596	42619.164311	31.994356
605.680308	42691.966735	31.999373
606.350997	42773.106674	32.004391
606.868773	42846.864209	32.009408
607.449436	42918.335111	32.014426
607.973262	42998.651316	32.019444
608.996804	43074.069803	32.024461
609.449533	43157.022645	32.029479
610.062155	43227.407938	32.034496
610.940578	43301.736698	32.039514
611.349518	43371.730561	32.044532
612.039029	43446.785166	32.049549
612.469362	43526.308293	32.054567
612.893453	43608.027554	32.059584
613.666055	43675.131694	32.064602
614.493258	43761.032660	32.069620
615.094389	43834.925907	32.074637
615.633909	43919.917415	32.079655
616.593193	43996.803936	32.084672
617.280814	44068.818425	32.089690
617.706009	44149.211163	32.094708
618.265384	44214.876499	32.099725
619.216572	44293.618670	32.104743
619.960849	44362.114596	32.109760
620.340666	44440.870864	32.114778
621.037486	44518.742792	32.119796
621.639713	44589.203601	32.124813
622.243184	44660.822018	32.129831
622.672241	44738.875810	32.134848
623.624058	44805.044399	32.139866
624.338168	44880.308725	32.144884
625.002150	44947.990363	32.149901
625.378937	45032.828147	32.154919
625.891367	45093.164541	32.159936
626.679959	45172.997992	32.164954
627.439649	45257.896850	32.169972
628.299502	45314.219512	32.174989
628.880719	45378.720904	32.180007
629.378231	45468.481863	32.185024
630.024355	45533.751609	32.190042
630.488617	45602.541891	32.195060
630.821081	45684.283089	32.200077
631.476874	45750.595718	32.205095
632.278459	45830.865960	32.210112
632.939171	45899.999614	32.215130
633.727698	45965.874579	32.220148
634.485600	46016.673443	32.225165
635.145904	46087.926935	32.230183
635.535661	46158.451250	32.235200
635.804929	46220.372294	32.240218
636.336522	46292.829555	32.245236
637.207637	46366.378893	32.250253
637.498224	46433.699636	32.255271
638.424961	46513.516210	32.260288
639.179298	46573.843993	32.265306
639.662204	46656.855683	32.270324
640.098112	46727.083543	32.275341
640.724125	46807.138035	32.280359
641.019840	46889.730735	32.285376
641.974973	46962.111159	32.290394
642.542696	47049.615276	32.295412
643.461313	47121.710922	32.300429
644.100542	47207.091475	32.305447
644.677787	47283.928881	32.310464
645.480834	47359.035727	32.315482
645.573506	47447.609009	32.320500
646.465742	47521.247362	32.325517
647.346116	47607.040827	32.330535
647.742614	47692.442239	32.335552
648.546656	47773.307347	32.340570
649.149643	47853.584235	32.345588
650.097566	47935.110645	32.350605
650.352212	48018.175711	32.355623
650.920382	48102.267491	32.360640
651.794528	48180.832860	32.365658
652.402531	48263.539806	32.370676
653.198022	48345.034615	32.375693
653.879479	48424.086514	32.380711
654.229309	48515.793314	32.385728
655.304477	48593.132883	32.390746
655.953312	48686.621951	32.395764
656.449164	48765.065099	32.400781
657.488453	48847.497835	32.405799
657.905797	48935.431329	32.410816
658.800594	49008.574269	32.415834
659.447482	49096.548355	32.420852
659.777922	49175.164328	32.425869
660.651095	49254.688891	32.430887
661.410718	49344.949251	32.435904
662.248778	49422.233851	32.440922
662.896815	49505.147800	32.445940
663.439494	49578.328719	32.450957
663.882856	49669.582597	32.455975
664.804764	49747.323355	32.460992
665.650399	49829.220516	32.466010
665.936566	49913.413721	32.471028
666.563932	49993.947374	32.476045
667.373309	50070.960254	32.481063
668.230156	50168.415166	32.486080
668.834819	50240.329387	32.491098
669.725801	50312.205320	32.496116
670.006818	50399.849401	32.501133
670.837431	50484.174547	32.506151
671.624519	50564.413108	32.511168
672.330445	50642.064162	32.516186
672.811145	50726.242518	32.521204
673.706451	50804.522495	32.526221
674.697412	50886.444939	32.531239
674.666236	50954.253297	32.536256
675.567900	51030.343788	32.541274
676.282311	51123.225050	32.546292
676.840540	51197.129982	32.551309
677.939049	51272.880400	32.556327
678.225716	51350.112274	32.561344
679.100308	51421.190634	32.566362
679.448579	51489.099315	32.571380
679.463520	51575.979592	32.576397
680.800428	51644.005984	32.581415
681.430946	51727.993667	32.586432
682.100665	51809.077492	32.591450
682.402776	51891.680839	32.596468
683.038080	51976.617805	32.601485
684.151676	52059.588218	32.606503
684.222162	52147.765416	32.611520
685.422746	52217.200588	32.616538
685.895239	52308.643790	32.621556
686.528754	52403.403168	32.626573
687.199056	52490.652467	32.631591
687.717147	52577.558918	32.636608
688.707898	52664.132232	32.641626
689.109759	52751.013234	32.646644
689.757007	52843.424624	32.651661
690.750122	52927.866062	32.656679
691.247274	53019.137325	32.661696
691.884285	53111.019830	32.666714
692.516569	53211.072798	32.671732
693.424161	53298.009512	32.676749
694.060267	53400.511608	32.681767
695.036833	53488.286175	32.686784
695.915035	53564.318991	32.691802
696.372295	53662.692721	32.696820
697.140312	53759.423519	32.701837
697.835918	53845.477882	32.706855
698.247041	53940.689616	32.711872
698.876534	54027.710545	32.716890
700.029813	54129.533646	32.721908
700.684131	54225.689313	32.726925
701.327042	54313.133182	32.731943
702.155221	54401.333064	32.736960
702.806094	54486.162757	32.741978
703.698450	54586.516231	32.746996
704.249308	54683.917651	32.752013
705.258734	54760.566604	32.757031
705.856025	54859.062606	32.762048
706.278668	54945.429509	32.767066
707.283241	55035.882355	32.772084
707.845359	55131.594161	32.777101
709.089824	55211.821309	32.782119
709.440226	55306.908815	32.787136
709.912658	55395.604772	32.792154
710.860671	55483.815227	32.797172
711.446185	55573.943375	32.802189
712.492973	55667.113295	32.807207
713.046233	55755.905521	32.812224
713.915532	55840.484342	32.817242
714.380150	55936.467796	32.822260
714.975424	56019.969993	32.827277
716.007288	56112.568079	32.832295
717.055616	56203.138753	32.837312
717.599094	56290.719382	32.842330
718.504317	56374.497046	32.847348
718.804970	56464.654177	32.852365
719.693582	56550.561536	32.857383
720.623200	56637.696906	32.862400
721.120824	56720.476364	32.867418
722.024254	56803.154584	32.872436
722.505909	56897.500039	32.877453
723.837867	56975.200508	32.882471
724.300408	57061.233379	32.887488
724.580352	57149.712822	32.892506
725.729104	57225.740296	32.897524
726.179690	57308.877241	32.902541
726.787991	57372.198858	32.907559
727.608175	57460.107505	32.912576
728.176200	57539.847137	32.917594
728.810240	57628.931115	32.922612
729.462728	57712.873278	32.927629
730.283668	57793.074142	32.932647
730.942807	57880.243713	32.937664
731.358908	57953.432492	32.942682
731.975369	58051.527224	32.947700
733.118716	58144.248596	32.952717
734.001420	58236.966836	32.957735
734.568847	58328.241091	32.962752
735.222428	58424.628942	32.967770
736.077772	58506.010366	32.972788
736.998894	58596.578321	32.977805
737.529792	58674.903403	32.982823
738.474527	58776.183975	32.987840
738.964824	58873.504284	32.992858
739.548412	58956.088059	32.997876
739.871952	59050.751503	33.002893
740.986051	59144.145875	33.007911
741.723874	59242.011211	33.012928
742.343192	59346.693438	33.017946
743.193001	59435.997118	33.022964
743.543258	59547.824131	33.027981
744.703722	59640.143441	33.032999
745.522910	59734.928141	33.038016
745.881583	59843.235899	33.043034
746.961026	59938.436371	33.048052
747.709467	60040.860637	33.053069
748.477306	60140.541507	33.058087
749.400938	60236.729662	33.063104
750.130453	60353.855967	33.068122
750.505387	60444.680892	33.073140
751.544038	60544.283016	33.078157
752.587209	60642.580879	33.083175
753.040455	60745.858210	33.088192
753.982351	60856.199632	33.093210
755.035728	60943.983066	33.098228
755.442436	61043.800113	33.103245
756.264897	61138.577065	33.108263
757.288209	61242.748363	33.113280
757.837076	61339.328683	33.118298
758.973721	61436.557958	33.123316
759.297297	61539.593056	33.128333
760.326703	61634.187583	33.133351
761.278443	61726.636047	33.138368
761.779246	61827.106192	33.143386
762.797206	61922.304982	33.148404
763.252014	62031.525192	33.153421
764.076801	62117.860989	33.158439
764.956780	62230.281913	33.163456
765.599709	62325.028224	33.168474
766.174504	62420.013457	33.173492
766.746909	62524.931779	33.178509
767.765764	62613.676104	33.183527
768.525283	62710.431353	33.188544
769.323028	62824.292186	33.193562
770.499225	62917.235364	33.198580
771.292220	63020.874131	33.203597
771.669117	63122.457760	33.208615
772.580315	63210.284153	33.213632
773.157842	63317.446023	33.218650
774.220721	63409.623790	33.223668
774.888108	63512.600563	33.228685
775.311150	63612.463359	33.233703
776.069019	63695.415546	33.238720
776.607689	63799.635474	33.243738
777.600729	63899.353180	33.248756
778.345615	63990.266092	33.253773
779.521983	64080.839545	33.258791
780.634293	64174.227895	33.263808
780.995585	64269.297907	33.268826
781.682707	64354.314536	33.273844
782.736400	64453.379200	33.278861
783.107797	64544.555191	33.283879
784.022459	64644.883234	33.288896
784.840536	64747.835145	33.293914
785.563218	64840.729860	33.298932
786.375256	64951.052780	33.303949
786.938978	65035.274334	33.308967
787.523682	65128.609561	33.313984
788.545800	65248.403759	33.319002
789.436358	65343.774805	33.324020
790.314242	65441.326096	33.329037
791.067649	65535.478444	33.334055
792.067043	65643.679444	33.339072
792.649673	65751.066133	33.344090
793.178674	65854.555317	33.349108
794.383188	65960.705893	33.354125
795.128447	66062.604576	33.359143
795.964619	66171.960352	33.364160
796.474306	66266.457477	33.369178
797.622106	66362.038991	33.374196
798.416606	66475.359680	33.379213
799.234937	66571.500081	33.384231
800.001764	66678.804858	33.389248
800.377718	66786.696804	33.394266
801.407507	66904.173967	33.399284
802.341273	67005.540384	33.404301
803.364612	67102.461113	33.409319
804.267627	67207.404123	33.414336
804.645221	67314.183683	33.419354
805.787878	67417.152566	33.424372
806.542269	67525.349265	33.429389
807.338201	67631.165547	33.434407
808.247484	67726.618559	33.439424
808.842054	67836.848738	33.444442
809.969676	67934.313471	33.449460
810.792586	68047.586015	33.454477
811.606788	68152.097239	33.459495
812.565562	68256.351972	33.464512
813.286135	68363.993964	33.469530
814.486928	68461.544214	33.474548
815.164743	68562.431310	33.479565
815.771260	68662.551141	33.484583
816.841390	68762.624090	33.489600
817.467764	68868.541655	33.494618
818.322949	68974.854398	33.499636
818.935198	69073.835166	33.504653
819.753435	69178.508210	33.509671
820.767462	69277.939737	33.514688
821.372185	69384.692300	33.519706
822.599754	69494.475831	33.524724
823.259645	69590.494016	33.529741
823.652542	69697.230373	33.534759
824.862285	69800.628845	33.539776
825.456026	69903.617610	33.544794
826.436052	70005.438154	33.549812
827.250557	70114.212502	33.554829
828.155691	70224.176245	33.559847
829.223183	70313.788323	33.564864
829.404375	70420.269503	33.569882
830.526093	70514.775003	33.574900
831.500254	70621.512775	33.579917
832.367498	70718.009230	33.584935
833.018260	70807.460287	33.589952
833.786938	70916.080503	33.594970
834.959466	70996.167134	33.599988
835.551559	71093.505947	33.605005
836.343544	71202.326337	33.610023
837.172941	71294.714703	33.615040
837.570100	71396.429285	33.620058
838.553611	71494.417540	33.625076
839.261620	71597.781359	33.630093
839.940726	71705.722275	33.635111
841.199514	71810.419195	33.640128
841.844421	71917.226452	33.645146
842.383712	72020.187721	33.650164
843.282003	72131.971681	33.655181
844.248564	72239.451806	33.660199
845.479038	72352.324580	33.665216
846.006036	72466.156588	33.670234
846.787648	72566.624904	33.675252
847.403331	72687.701418	33.680269
848.611855	72807.596394	33.685287
849.384317	72903.634388	33.690304
850.237798	73019.672168	33.695322
851.423132	73134.037248	33.700340
852.439298	73243.717551	33.705357
853.120306	73357.402599	33.710375
853.959369	73461.956444	33.715392
854.557076	73578.252031	33.720410
855.850759	73683.774184	33.725428
856.518825	73795.892515	33.730445
857.879875	73906.674172	33.735463
858.672871	74019.685854	33.740480
859.429770	74132.766998	33.745498
860.271797	74238.324063	33.750516
861.227629	74345.548372	33.755533
862.134156	74453.502826	33.760551
863.465500	74559.807865	33.765568
863.809691	74670.118569	33.770586
864.539196	74769.767333	33.775604
865.632664	74885.572960	33.780621
866.189239	74996.193748	33.785639
867.436595	75097.928669	33.790656
868.124980	75214.153810	33.795674
868.771308	75328.194647	33.800692
869.816733	75439.665397	33.805709
870.752272	75561.819514	33.810727
871.788157	75663.196998	33.815744
872.166835	75765.969824	33.820762
872.951308	75880.270034	33.825780
874.317227	75990.578151	33.830797
875.078932	76099.765260	33.835815
876.039496	76219.156938	33.840832
876.639837	76326.900806	33.845850
877.648019	76441.244354	33.850868
878.969066	76555.919420	33.855885
879.707459	76671.408256	33.860903
880.882651	76778.962562	33.865920
881.407549	76899.362847	33.870938
882.305119	77002.249108	33.875956
883.421857	77113.386198	33.880973
883.979887	77219.924107	33.885991
884.717279	77317.275437	33.891008
885.495037	77442.110295	33.896026
886.253101	77559.107290	33.901044
887.710586	77667.266959	33.906061
887.826483	77782.528585	33.911079
888.696189	77890.109755	33.916096
889.577505	78006.683977	33.921114
890.500257	78121.554653	33.926132
891.357551	78229.937197	33.931149
892.216803	78345.578851	33.936167
893.464639	78457.448291	33.941184
893.802516	78558.616433	33.946202
895.298422	78673.792390	33.951220
895.718659	78786.312157	33.956237
896.615527	78902.342979	33.961255
897.608801	79023.109956	33.966272
898.661790	79134.391878	33.971290
899.591085	79245.718953	33.976308
900.590014	79354.780515	33.981325
900.919442	79484.040227	33.986343
901.545457	79590.855363	33.991360
902.752782	79716.025977	33.996378
903.086892	79850.531632	34.001396
904.654654	79965.156931	34.006413
905.374227	80101.326443	34.011431
906.052417	80230.940424	34.016448
906.796784	80351.891504	34.021466
908.039767	80488.272341	34.026484
909.001994	80609.849231	34.031501
909.621747	80744.707214	34.036519
910.794471	80871.763509	34.041536
911.620400	80995.403209	34.046554
913.029698	81130.342133	34.051572
913.660782	81261.463273	34.056589
914.479518	81388.780047	34.061607
915.427390	81518.522455	34.066624
916.494965	81645.079245	34.071642
917.367424	81774.923329	34.076660
918.668254	81898.403944	34.081677
919.365870	82050.259138	34.086695
920.229292	82175.013106	34.091712
921.428483	82299.524997	34.096730
922.494429	82436.285082	34.101748
923.262519	82559.750634	34.106765
924.409850	82697.398826	34.111783
925.102443	82818.545977	34.116800
926.022468	82935.806210	34.121818
927.044576	83073.539181	34.126836
928.188344	83193.451595	34.131853
929.104194	83325.107869	34.136871
930.041074	83454.658121	34.141888
931.304473	83580.597353	34.146906
931.794378	83705.581232	34.151924
932.612499	83840.739654	34.156941
933.769831	83965.810227	34.161959
934.682905	84092.338741	34.166976
935.575118	84219.365249	34.171994
936.631773	84345.669660	34.177012
937.644753	84484.171111	34.182029
938.505348	84608.315264	34.187047
939.707377	84738.995549	34.192064
940.400215	84860.632802	34.197082
941.080463	84988.557539	34.202100
942.658960	85116.304185	34.207117
943.248788	85246.398363	34.212135
943.923361	85361.641484	34.217152
945.252854	85493.901837	34.222170
945.784810	85628.936043	34.227188
946.777629	85751.594488	34.232205
947.746677	85889.590006	34.237223
948.925400	86026.628306	34.242240
949.550590	86142.743940	34.247258
950.338032	86284.444608	34.252276
951.695513	86412.370955	34.257293
952.809455	86545.861009	34.262311
953.546342	86651.671475	34.267328
954.553700	86767.248216	34.272346
955.190785	86892.260815	34.277364
956.382264	87000.877956	34.282381
957.300041	87136.276909	34.287399
957.752024	87254.781126	34.292416
959.329220	87374.681021	34.297434
960.117645	87504.196580	34.302452
961.071233	87621.280454	34.307469
961.736112	87751.754212	34.312487
962.579973	87890.272988	34.317504
963.724158	88016.680992	34.322522
964.543499	88148.412260	34.327540
965.639818	88274.778172	34.332557
966.517295	88409.682371	34.337575
967.284284	88541.322200	34.342592
968.333331	88675.060183	34.347610
969.434296	88823.972924	34.352628
970.394084	88958.828713	34.357645
971.438851	89089.134822	34.362663
972.424752	89231.072043	34.367680
973.760478	89356.872801	34.372698
974.208610	89504.649182	34.377716
975.189669	89636.970044	34.382733
976.486261	89771.054389	34.387751
977.227184	89915.821375	34.392768
978.587069	90053.952595	34.397786
979.121325	90203.075006	34.402804
980.400704	90339.420492	34.407821
981.501914	90481.548367	34.412839
982.279775	90618.645350	34.417856
983.354407	90752.946267	34.422874
984.030126	90901.010730	34.427892
985.034158	91042.915662	34.432909
986.194514	91184.530631	34.437927
987.386165	91332.313643	34.442944
988.739922	91476.840088	34.447962
989.462573	91610.566217	34.452980
990.387013	91743.729021	34.457997
991.595289	91891.829014	34.463015
992.526254	92042.039070	34.468032
993.761318	92172.252683	34.473050
994.622028	92313.476228	34.478068
995.638335	92453.725473	34.483085
996.652974	92588.728334	34.488103
997.359651	92743.299001	34.493120
998.763282	92883.185382	34.498138
999.478412	93018.287730	34.503156
1000.863082	93150.155158	34.508173
1001.777426	93298.472762	34.513191
1002.702995	93435.521282	34.518208
1003.842288	93570.508948	34.523226
1005.082394	93714.430023	34.528244
1005.928542	93849.223980	34.533261
1007.530791	93985.598620	34.538279
1008.087338	94116.535129	34.543296
1009.053229	94255.076655	34.548314
1009.879407	94390.319733	34.553332
1011.052772	94527.296275	34.558349
1012.357820	94666.901976	34.563367
1012.988973	94801.201368	34.568384
1014.139643	94935.052409	34.573402
1015.111478	95083.686459	34.578420
1016.177701	95211.999985	34.583437
1017.337648	95346.675262	34.588455
1018.356632	95490.854685	34.593472
1019.014765	95612.921205	34.598490
1020.032901	95742.917652	34.603508
1021.159871	95872.694784	34.608525
1022.295626	95998.237292	34.613543
1022.971762	96126.438179	34.618560
1024.171113	96255.875986	34.623578
1024.807648	96385.085539	34.628596
1026.056068	96522.122456	34.633613
1026.958595	96654.802782	34.638631
1027.597566	96792.481371	34.643648
1028.803794	96920.691229	34.648666
1029.376981	97065.758959	34.653684
1030.585898	97203.654339	34.658701
1031.786979	97346.064396	34.663719
1032.421787	97493.824540	34.668736
1033.657375	97641.592724	34.673754
1034.547407	97794.613153	34.678772
1035.551723	97938.248282	34.683789
1036.607078	98092.410521	34.688807
1037.621249	98237.845568	34.693824
1038.980447	98390.301000	34.698842
1039.991318	98550.100983	34.703860
1040.604039	98702.129660	34.708877
1041.895030	98849.222874	34.713895
1042.932816	99005.078319	34.718912
1044.187203	99160.089263	34.723930
1045.079903	99313.040467	34.728948
1046.006399	99465.023625	34.733965
1047.137706	99627.713228	34.738983
1048.253960	99780.555583	34.744000
1049.740664	99927.863954	34.749018
1050.679120	100090.357881	34.754036
1051.528795	100246.908008	34.759053
1052.613786	100395.713977	34.764071
1053.493363	100559.956323	34.769088
1054.661906	100723.913377	34.774106
1056.209755	100883.564763	34.779124
1057.094987	101025.787003	34.784141
1058.329306	101185.032541	34.789159
1059.069641	101345.864890	34.794176
1060.134104	101492.840749	34.799194
1061.259133	101654.514534	34.804212
1062.377667	101814.579987	34.809229
1064.046680	101963.276300	34.814247
1064.719463	102124.731599	34.819264
1065.715492	102279.696413	34.824282
1066.833544	102433.045356	34.829300
1068.076070	102600.512157	34.834317
1069.025073	102746.839722	34.839335
1069.848980	102909.974133	34.844352
1071.024455	103059.855699	34.849370
1072.156620	103228.889762	34.854388
1073.185818	103385.515482	34.859405
1074.253936	103539.105575	34.864423
1074.982703	103713.758636	34.869440
1076.230428	103860.196477	34.874458
1077.744631	104030.772356	34.879476
1078.472349	104188.640880	34.884493
1079.966811	104344.145878	34.889511
1080.694438	104509.522049	34.894528
1081.661989	104661.877782	34.899546
1083.193183	104825.646213	34.904564
1084.106868	104983.882418	34.909581
1085.580117	105146.659800	34.914599
1086.401064	105305.127581	34.919616
1087.400717	105461.260423	34.924634
1088.653596	105611.749897	34.929652
1089.567688	105769.660038	34.934669
1091.070080	105920.238613	34.939687
1091.686390	106073.632040	34.944704
1092.929919	106212.789802	34.949722
1093.822477	106363.947652	34.954740
1094.601490	106515.225388	34.959757
1095.907702	106666.193014	34.964775
1096.773091	106819.702956	34.969792
1097.893370	106970.282585	34.974810
1098.937922	107123.157183	34.979828
1100.071249	107283.347808	34.984845
1101.002304	107437.116515	34.989863
1101.539530	107601.725964	34.994880
1103.109705	107758.807093	34.999898
1104.178055	107932.071851	35.004916
1105.037381	108103.810479	35.009933
1106.242865	108262.066886	35.014951
1107.334836	108444.016794	35.019968
1108.373938	108607.474581	35.024986
1109.505165	108778.007336	35.030004
1110.480623	108957.429307	35.035021
1111.652380	109119.587949	35.040039
1112.534648	109308.714616	35.045056
1113.916183	109473.961607	35.050074
1114.908460	109652.040302	35.055092
1116.129613	109842.296144	35.060109
1117.652668	110006.166585	35.065127
1118.289496	110190.517511	35.070144
1119.604178	110367.027577	35.075162
1120.913997	110541.243927	35.080180
1122.187104	110726.132109	35.085197
1123.544556	110895.409601	35.090215
1124.482832	111083.142028	35.095232
1125.428166	111247.311568	35.100250
1126.631326	111438.872347	35.105268
1127.544162	111611.735726	35.110285
1129.064605	111793.065154	35.115303
1130.023062	111985.212494	35.120320
1131.179320	112162.288909	35.125338
1132.556889	112346.078467	35.130356
1133.237385	112524.474000	35.135373
1134.581028	112705.201600	35.140391
1135.432809	112901.365458	35.145408
1136.588072	113077.495347	35.150426
1137.984843	113259.942214	35.155444
1139.057545	113450.303922	35.160461
1140.209993	113638.561508	35.165479
1141.529800	113824.067088	35.170496
1142.636959	114007.476200	35.175514
1143.694580	114188.496934	35.180532
1144.704289	114375.055802	35.185549
1146.039148	114565.356919	35.190567
1147.295433	114751.143487	35.195584
1148.374741	114936.578207	35.200602
1149.565494	115125.750625	35.205620
1150.248984	115316.360528	35.210637
1151.770947	115506.649900	35.215655
1152.919493	115701.158846	35.220672
1154.318408	115890.759187	35.225690
1155.541514	116077.661074	35.230708
1156.788979	116253.702982	35.235725
1157.861103	116442.012838	35.240743
1159.033147	116630.891448	35.245760
1159.813577	116816.052571	35.250778
1160.748559	117000.023505	35.255796
1162.281272	117203.396838	35.260813
1163.062617	117382.028425	35.265831
1164.062246	117583.812992	35.270848
1165.643947	117782.158926	35.275866
1167.139303	117962.710929	35.280884
1167.940426	118151.287396	35.285901
1168.778932	118312.841544	35.290919
1170.019484	118507.629678	35.295936
1171.092224	118694.872522	35.300954
1172.418642	118870.203964	35.305972
1173.490692	119063.587978	35.310989
1175.200376	119245.254116	35.316007
1175.930820	119420.009096	35.321024
1176.746696	119611.419127	35.326042
1177.946169	119788.702711	35.331060
1179.027450	119989.497813	35.336077
1180.507178	120178.307833	35.341095
1181.502172	120374.513847	35.346112
1182.774810	120568.964919	35.351130
1184.009964	120760.556017	35.356148
1184.415465	120963.796002	35.361165
1185.803377	121163.432889	35.366183
1187.103117	121371.266570	35.371200
1187.978250	121566.419107	35.376218
1189.434129	121776.412365	35.381236
1190.452590	121994.606581	35.386253
1191.434303	122191.686409	35.391271
1192.837001	122408.744500	35.396288
1193.868167	122620.064611	35.401306
1195.217077	122828.177370	35.406324
1196.410123	123050.828134	35.411341
1197.900182	123261.420161	35.416359
1198.916357	123488.160526	35.421376
1200.140418	123696.576458	35.426394
1201.486643	123911.875555	35.431412
1202.647111	124140.411128	35.436429
1203.895592	124343.054414	35.441447
1205.233637	124560.578347	35.446464
1206.193419	124772.441140	35.451482
1207.744018	124990.733350	35.456500
1208.845763	125218.941686	35.461517
1210.304011	125430.996302	35.466535
1211.147429	125643.795286	35.471552
1212.333087	125866.817990	35.476570
1213.866947	126085.575409	35.481588
1215.010858	126307.820472	35.486605
1216.221248	126515.415700	35.491623
1217.875141	126747.542483	35.496640
1218.849529	126968.193721	35.501658
1220.526157	127178.129824	35.506676
1221.558526	127396.414474	35.511693
1223.074019	127598.296232	35.516711
1224.476558	127816.182582	35.521728
1225.254036	128041.843746	35.526746
1226.790580	128241.263980	35.531764
1228.127650	128464.962091	35.536781
1229.807849	128670.083914	35.541799
1230.728518	128879.144594	35.546816
1231.817841	129089.905427	35.551834
1232.791157	129296.942598	35.556852
1234.272550	129513.011056	35.561869
1235.328488	129727.776930	35.566887
1236.802540	129941.793289	35.571904
1237.699980	130150.495918	35.576922
1239.061537	130358.086494	35.581940
1240.500905	130578.290530	35.586957
1241.729122	130791.030058	35.591975
1242.999882	131006.897963	35.596992
1244.265326	131215.776546	35.602010
1246.036273	131425.998099	35.607028
1246.886312	131646.997701	35.612045
1248.047029	131857.151919	35.617063
1249.040303	132052.855773	35.622080
1250.141235	132251.817301	35.627098
1252.033635	132461.047822	35.632116
1252.652119	132656.889180	35.637133
1254.533504	132856.365715	35.642151
1255.259360	133037.117737	35.647168
1256.596656	133247.466689	35.652186
1257.772099	133455.837131	35.657204
1258.866978	133663.574027	35.662221
1259.994940	133865.825054	35.667239
1261.104792	134064.298487	35.672256
1262.582382	134284.578635	35.677274
1263.886296	134493.822065	35.682292
1265.274444	134703.713128	35.687309
1266.105905	134920.328833	35.692327
1267.301550	135130.163195	35.697344
1268.567136	135348.146898	35.702362
1269.951122	135573.752202	35.707380
1271.047988	135793.591749	35.712397
1272.404239	136008.442798	35.717415
1273.640517	136230.470627	35.722432
1275.056835	136460.770453	35.727450
1276.465130	136684.334397	35.732468
1277.624901	136909.258080	35.737485
1278.893344	137131.577103	35.742503
1280.257012	137361.407462	35.747520
1281.615893	137590.935150	35.752538
1282.643946	137798.371487	35.757556
1284.118212	138041.157209	35.762573
1285.453447	138269.841705	35.767591
1286.882656	138493.055774	35.772608
1287.959188	138717.633220	35.777626
1289.573986	138954.855988	35.782644
1290.775090	139182.068451	35.787661
1292.045367	139407.367594	35.792679
1293.488319	139638.922635	35.797696
1294.763464	139873.030518	35.802714
1295.768706	140103.869516	35.807732
1296.904051	140337.455859	35.812749
1298.230693	140563.728837	35.817767
1299.908467	140801.712407	35.822784
1301.397612	141040.856177	35.827802
1302.790426	141268.695792	35.832820
1304.028135	141502.068699	35.837837
1305.058352	141739.016045	35.842855
1306.486502	141969.404340	35.847872
1307.876307	142208.937456	35.852890
1308.934818	142437.545578	35.857908
1310.849244	142672.836074	35.862925
1311.776085	142919.933062	35.867943
1313.181441	143147.386025	35.872960
1314.651940	143385.744608	35.877978
1316.164879	143624.034234	35.882996
1317.192658	143846.637828	35.888013
1318.653943	144087.996458	35.893031
1320.047207	144314.352454	35.898048
1321.098568	144550.954579	35.903066
1322.737485	144777.997645	35.908084
1324.275917	145012.355365	35.913101
1325.326120	145248.745171	35.918119
1326.624711	145479.474582	35.923136
1328.011932	145716.321488	35.928154
1329.396937	145952.027535	35.933172
1330.811865	146181.713831	35.938189
1332.154036	146416.616407	35.943207
1333.602827	146641.032120	35.948224
1334.788691	146884.706363	35.953242
1335.937763	147109.437561	35.958260
1337.551407	147336.940148	35.963277
1338.810188	147554.497475	35.968295
1340.237842	147770.506150	35.973312
1341.265852	147992.937333	35.978330
1342.682779	148211.069184	35.983348
1343.966687	148426.658803	35.988365
1345.130397	148646.342534	35.993383
1347.030239	148862.078675	35.998400
1347.829456	149092.343757	36.003418
1349.019699	149311.099486	36.008436
1350.607717	149543.172380	36.013453
1352.364087	149757.551043	36.018471
1353.580083	149985.990370	36.023488
1354.904271	150210.288414	36.028506
1355.758708	150433.937397	36.033524
1357.415472	150670.700899	36.038541
1358.661832	150896.169051	36.043559
1360.054926	151127.378003	36.048576
1360.815750	151368.689401	36.053594
1362.518838	151599.001346	36.058612
1364.202773	151831.056278	36.063629
1365.037330	152079.061479	36.068647
1366.860007	152315.234863	36.073664
1368.393500	152563.259753	36.078682
1369.459133	152796.887972	36.083700
1371.112017	153040.808863	36.088717
1372.706495	153273.277298	36.093735
1373.911080	153509.755558	36.098752
1375.083634	153752.624937	36.103770
1376.709398	153996.643048	36.108788
1377.905317	154243.623758	36.113805
1379.222676	154485.826184	36.118823
1380.799691	154728.395204	36.123840
1381.772827	154985.721737	36.128858
1383.369090	155227.299678	36.133876
1384.828064	155472.238754	36.138893
1386.372720	155725.810406	36.143911
1387.580455	155978.141049	36.148928
1388.760697	156225.196117	36.153946
1390.108657	156487.307237	36.158964
1391.586169	156727.577005	36.163981
1392.993139	156997.869242	36.168999
1394.367669	157255.993432	36.174016
1395.721164	157505.400638	36.179034
1397.272630	157764.921151	36.184052
1398.805125	158018.923427	36.189069
1400.104411	158281.659380	36.194087
1401.565676	158524.020863	36.199104
1403.105358	158797.740765	36.204122
1403.918785	159048.787658	36.209140
1405.870906	159314.510802	36.214157
1407.421585	159574.064523	36.219175
1408.903503	159822.610512	36.224192
1410.239275	160080.993930	36.229210
1411.666397	160350.904306	36.234228
1413.068448	160591.315359	36.239245
1414.522231	160848.858259	36.244263
1415.860710	161103.639914	36.249280
1417.892920	161365.334718	36.254298
1419.038937	161620.110480	36.259316
1420.472333	161859.962820	36.264333
1421.836466	162120.800406	36.269351
1423.218958	162375.948418	36.274368
1424.917818	162634.006068	36.279386
1426.414870	162898.660153	36.284404
1427.967274	163143.500838	36.289421
1429.256168	163401.194025	36.294439
1430.592478	163648.482671	36.299456
1432.020228	163898.094026	36.304474
1433.537768	164143.426335	36.309492
1435.046682	164372.446195	36.314509
1436.511135	164604.279683	36.319527
1437.815303	164841.027156	36.324544
1438.762145	165074.085952	36.329562
1440.467829	165318.796378	36.334580
1441.635767	165540.801661	36.339597
1443.286300	165792.073807	36.344615
1444.994672	166038.817842	36.349632
1446.168612	166282.472256	36.354650
1446.939237	166527.384143	36.359668
1448.625548	166780.419131	36.364685
1449.793942	167031.771254	36.369703
1451.734814	167283.104946	36.374720
1452.611999	167540.637030	36.379738
1454.015754	167803.712360	36.384756
1455.777013	168059.889057	36.389773
1456.836906	168334.091907	36.394791
1458.463710	168595.205307	36.399808
1459.535782	168863.174028	36.404826
1460.527223	169133.911641	36.409844
1462.567082	169402.010217	36.414861
1463.939685	169687.063438	36.419879
1465.549894	169963.840045	36.424896
1467.019478	170246.658234	36.429914
1468.247073	170524.588799	36.434932
1469.849482	170792.494263	36.439949
1470.888419	171085.096568	36.444967
1472.414873	171372.722465	36.449984
1474.147478	171653.409716	36.455002
1475.822909	171942.512772	36.460020
1477.317278	172225.474199	36.465037
1478.769484	172515.680960	36.470055
1480.234929	172794.509553	36.475072
1482.059546	173083.022143	36.480090
1483.288678	173377.050982	36.485108
1484.891407	173666.133760	36.490125
1486.544726	173961.330085	36.495143
1488.101912	174232.568758	36.500160
1489.547618	174527.774283	36.505178
1490.707119	174814.276714	36.510196
1492.654535	175105.545618	36.515213
1493.814610	175401.713308	36.520231
1495.908145	175676.098219	36.525248
1497.345800	175968.148387	36.530266
1498.696674	176252.416414	36.535284
1500.842596	176541.475235	36.540301
1501.843839	176829.723741	36.545319
1503.409765	177122.100731	36.550336
1504.955013	177401.580321	36.555354
1505.766553	177698.775805	36.560372
1507.808415	177989.328890	36.565389
1509.152289	178287.331991	36.570407
1511.379108	178579.432739	36.575424
1513.019640	178853.746478	36.580442
1514.193957	179147.131336	36.585460
1515.706194	179428.197270	36.590477
1517.396353	179717.084109	36.595495
1519.024453	179994.832006	36.600512
1520.565109	180285.928279	36.605530
1521.738370	180582.822905	36.610548
1523.572901	180857.975957	36.615565
1525.216981	181141.794967	36.620583
1526.955348	181422.349138	36.625600
1528.624110	181705.988228	36.630618
1529.584131	181995.580702	36.635636
1531.181735	182284.998082	36.640653
1533.077809	182556.184379	36.645671
1534.344424	182828.130324	36.650688
1535.698086	183097.066388	36.655706
1536.855621	183354.096551	36.660724
1538.515777	183629.284978	36.665741
1540.243379	183902.330129	36.670759
1541.696678	184176.765106	36.675776
1543.250310	184450.931151	36.680794
1544.412340	184736.995154	36.685812
1546.299540	185071.890427	36.690829
1547.513688	185354.595349	36.695847
1548.692077	185636.011293	36.700864
1550.760402	185920.311236	36.705882
1551.995162	186206.240981	36.710900
1553.649968	186483.368377	36.715917
1554.891553	186772.498925	36.720935
1556.396504	187066.262557	36.725952
1558.110137	187360.705528	36.730970
1559.641514	187660.283164	36.735988
1561.480977	187952.218889	36.741005
1562.967838	188252.109920	36.746023
1564.285062	188556.879696	36.751040
1565.781746	188843.639058	36.756058
1567.350289	189147.888519	36.761076
1568.928572	189448.632064	36.766093
1570.443408	189750.884945	36.771111
1571.951331	190057.940344	36.776128
1573.428257	190368.405049	36.781146
1575.023439	190685.024358	36.786164
1576.829338	190991.832377	36.791181
1578.565054	191305.865911	36.796199
1579.901914	191615.136586	36.801216
1581.885794	191930.707745	36.806234
1583.088400	192238.730987	36.811252
1584.887055	192557.609435	36.816269
1586.634290	192866.438026	36.821287
1588.224254	193183.826684	36.826304
1589.971332	193491.742398	36.831322
1591.366757	193807.766003	36.836340
1593.211722	194124.278848	36.841357
1595.256474	194430.905559	36.846375
1596.664887	194744.744901	36.851392
1598.550202	195057.824511	36.856410
1599.927918	195361.560409	36.861428
1602.001171	195669.531763	36.866445
1603.541034	195977.917501	36.871463
1604.802822	196288.150948	36.876480
1606.793444	196589.939317	36.881498
1608.229951	196911.577472	36.886516
1609.745543	197214.305158	36.891533
1611.718641	197521.940605	36.896551
1613.118662	197840.766943	36.901568
1615.114601	198140.728782	36.906586
1616.272923	198460.203913	36.911604
1618.188418	198774.988876	36.916621
1620.518891	199070.302455	36.921639
1621.355859	199376.011127	36.926656
1623.170954	199679.179524	36.931674
1624.754696	199991.148427	36.936692
1626.325089	200285.871973	36.941709
1628.174086	200595.488933	36.946727
1629.812363	200905.825314	36.951744
1631.387682	201200.702136	36.956762
1633.196230	201509.844480	36.961780
1634.672139	201816.499204	36.966797
1636.546104	202123.778038	36.971815
1638.198158	202429.999834	36.976832
1639.907223	202727.855812	36.981850
1641.394468	203026.178839	36.986868
1642.866480	203313.175187	36.991885
1644.554356	203601.763964	36.996903
1645.917191	203874.349574	37.001920
1647.953737	204156.787996	37.006938
1649.242090	204448.184074	37.011956
1650.749683	204742.188163	37.016973
1652.498968	205026.679618	37.021991
1653.900031	205325.121327	37.027008
1655.799713	205618.887518	37.032026
1657.564499	205913.437325	37.037044
1658.930933	206205.763621	37.042061
1660.876132	206504.756936	37.047079
1661.926742	206810.901898	37.052096
1663.775597	207093.958002	37.057114
1665.289517	207404.019555	37.062132
1667.075076	207708.526542	37.067149
1668.590749	208019.884212	37.072167
1670.260081	208330.532360	37.077184
1672.006718	208646.579699	37.082202
1673.768570	208958.966997	37.087220
1675.272443	209268.168842	37.092237
1677.140475	209584.299987	37.097255
1678.633915	209908.822437	37.102272
1680.466335	210214.747771	37.107290
1681.931584	210534.906013	37.112308
1683.509569	210857.307890	37.117325
1685.262101	211182.959867	37.122343
1687.006999	211513.135228	37.127360
1689.035028	211833.384682	37.132378
1690.821347	212172.216891	37.137396
1692.418841	212482.499998	37.142413
1694.074246	212806.365272	37.147431
1695.784309	213136.954275	37.152448
1697.229882	213463.952274	37.157466
1698.762709	213800.183866	37.162484
1700.826205	214132.572986	37.167501
1702.812434	214462.993010	37.172519
1704.471194	214791.991155	37.177536
1706.163840	215123.118193	37.182554
1708.022216	215455.337337	37.187572
1709.548852	215783.010575	37.192589
1711.535267	216114.117840	37.197607
1713.263448	216449.787648	37.202624
1715.414996	216774.620213	37.207642
1716.997899	217099.440371	37.212660
1718.663173	217432.072252	37.217677
1720.127612	217759.248531	37.222695
1721.982446	218088.497846	37.227712
1723.598605	218422.840088	37.232730
1726.099366	218759.025596	37.237748
1727.459185	219088.962630	37.242765
1729.185869	219411.983345	37.247783
1731.146566	219751.403974	37.252800
1733.098872	220071.417416	37.257818
1734.913316	220404.078359	37.262836
1736.316691	220725.117914	37.267853
1738.112748	221051.913657	37.272871
1739.731055	221377.517936	37.277888
1741.441629	221706.257980	37.282906
1743.446166	222037.213080	37.287924
1744.869781	222363.203769	37.292941
1746.812601	222696.455060	37.297959
1748.096773	223022.289890	37.302976
1750.071479	223352.665665	37.307994
1751.839444	223681.575006	37.313012
1752.810869	224019.551276	37.318029
1754.735533	224348.309156	37.323047
1756.815667	224685.400677	37.328064
1758.602967	225005.542707	37.333082
1760.219895	225325.228729	37.338100
1761.840920	225650.985688	37.343117
1763.470677	225955.427244	37.348135
1765.315666	226280.259989	37.353152
1767.108401	226591.865361	37.358170
1768.859887	226925.604111	37.363188
1770.329030	227251.130676	37.368205
1772.020491	227576.851039	37.373223
1773.909627	227910.212440	37.378240
1775.631616	228239.230428	37.383258
1777.042414	228569.821279	37.388276
1778.731686	228912.562411	37.393293
1780.819060	229244.368213	37.398311
1782.682287	229603.416704	37.403328
1784.100157	229943.710373	37.408346
1785.655609	230283.702937	37.413364
1787.295239	230633.564345	37.418381
1789.004596	230985.523215	37.423399
1790.960963	231349.611765	37.428416
1792.993468	231701.265669	37.433434
1795.304849	232071.674662	37.438452
1796.799961	232420.795648	37.443469
1798.363905	232760.429990	37.448487
1800.160391	233135.974252	37.453504
1802.563481	233498.772190	37.458522
1804.751016	233851.746897	37.463540
1805.965780	234217.600892	37.468557
1807.755794	234564.819789	37.473575
1809.914348	234932.303786	37.478592
1812.015421	235292.251538	37.483610
1813.359352	235650.589998	37.488628
1815.327628	236026.790875	37.493645
1817.273861	236382.824287	37.498663
1818.638057	236738.262535	37.503680
1820.421375	237118.555834	37.508698
1822.744990	237476.866242	37.513716
1824.314375	237854.423202	37.518733
1826.464440	238219.441111	37.523751
1828.163948	238593.166308	37.528768
1830.312030	238954.906612	37.533786
1832.439724	239322.517874	37.538804
1833.752486	239697.775615	37.543821
1835.778364	240064.106288	37.548839
1837.528386	240444.451502	37.553856
1839.371150	240811.978384	37.558874
1841.652891	241180.731632	37.563892
1843.152150	241557.761245	37.568909
1845.182723	241917.077311	37.573927
1847.151667	242293.956105	37.578944
1849.020279	242666.099619	37.583962
1851.030532	243024.756731	37.588980
1852.574932	243397.559485	37.593997
1854.593961	243756.874556	37.599015
1856.785075	244127.720477	37.604032
1858.629136	244502.125679	37.609050
1860.490574	244872.894888	37.614068
1861.821781	245242.781101	37.619085
1864.090334	245602.663684	37.624103
1865.974748	245973.782950	37.629120
1867.410275	246343.600013	37.634138
1869.646737	246719.463895	37.639156
1871.272922	247097.810376	37.644173
1873.290338	247468.550314	37.649191
1875.162501	247834.587370	37.654208
1877.022797	248211.015151	37.659226
1879.171989	248578.201262	37.664244
1880.693593	248939.693070	37.669261
1882.453416	249293.145123	37.674279
1884.254055	249644.862703	37.679296
1886.166806	250005.071740	37.684314
1888.308090	250352.035121	37.689332
1890.045746	250697.308177	37.694349
1891.997546	251043.004222	37.699367
1893.672786	251413.458912	37.704384
1895.388640	251776.971648	37.709402
1897.173224	252127.822650	37.714420
1898.781709	252496.761077	37.719437
1900.698316	252864.685120	37.724455
1902.490598	253236.945988	37.729472
1903.947878	253607.912043	37.734490
1906.120631	253981.737174	37.739508
1907.885475	254374.879464	37.744525
1909.949788	254748.516326	37.749543
1911.556273	255144.576989	37.754560
1913.309124	255531.164339	37.759578
1915.516448	255919.406753	37.764596
1917.350300	256315.479213	37.769613
1919.600474	256706.201928	37.774631
1921.328541	257097.614786	37.779648
1923.290144	257499.531275	37.784666
1925.231982	257886.615520	37.789684
1927.316150	258298.670603	37.794701
1929.072747	258694.493769	37.799719
1931.473260	259103.499386	37.804736
1933.296833	259500.604877	37.809754
1935.382714	259908.996572	37.814772
1937.038320	260309.630892	37.819789
1938.905063	260713.786829	37.824807
1941.097551	261130.615835	37.829824
1943.176237	261538.037720	37.834842
1944.964311	261936.004034	37.839860
1946.980209	262355.954934	37.844877
1949.055475	262756.972145	37.849895
1951.196892	263165.648223	37.854912
1953.020872	263577.471167	37.859930
1955.382572	263984.865082	37.864948
1957.413939	264398.303357	37.869965
1959.028954	264794.609852	37.874983
1961.438523	265201.864538	37.880000
1963.299467	265609.940018	37.885018
1965.780676	266009.204967	37.890036
1967.647334	266427.537418	37.895053
1969.867618	266833.976969	37.900071
1971.893834	267223.072541	37.905088
1973.851187	267635.061409	37.910106
1975.862345	268015.495260	37.915124
1977.945295	268426.445146	37.920141
1980.118910	268822.394122	37.925159
1982.284119	269224.412888	37.930176
1984.196935	269622.050157	37.935194
1986.594034	270016.054235	37.940212
1987.865159	270405.305619	37.945229
1990.281976	270792.801417	37.950247
1992.283956	271191.535373	37.955264
1994.476076	271598.771331	37.960282
1996.806691	271982.618205	37.965300
1998.345874	272373.241294	37.970317
2000.669237	272763.054209	37.975335
2002.543204	273149.811843	37.980352
2004.340083	273543.487734	37.985370
2006.771487	273930.332377	37.990388
2008.657593	274323.177971	37.995405
2010.385036	274710.713271	38.000423
2012.722141	275088.907079	38.005440
2014.427441	275477.610469	38.010458
2015.988689	275841.700272	38.015476
2018.552704	276214.190007	38.020493
2020.347342	276566.456252	38.025511
2022.538617	276932.017080	38.030528
2024.471048	277312.041470	38.035546
2026.185025	277676.708485	38.040564
2028.105881	278047.563312	38.045581
2029.818218	278410.830389	38.050599
2032.035033	278790.345938	38.055616
2033.665036	279176.223996	38.060634
2035.811151	279572.380478	38.065652
2037.849922	279957.327161	38.070669
2039.801326	280345.104341	38.075687
2041.550738	280740.732616	38.080704
2043.310805	281133.665293	38.085722
2045.547264	281544.652831	38.090740
2047.335410	281944.153859	38.095757
2049.022372	282356.390888	38.100775
2051.030812	282764.283688	38.105792
2053.069153	283195.379296	38.110810
2055.309729	283597.949087	38.115828
2057.349122	284020.558028	38.120845
2059.543618	284445.400130	38.125863
2061.774237	284869.345209	38.130880
2063.633898	285296.392852	38.135898
2065.721021	285727.439676	38.140916
2068.216389	286152.655760	38.145933
2069.542468	286587.066401	38.150951
2071.964863	287014.878444	38.155968
2073.954479	287447.986202	38.160986
2076.308407	287882.786149	38.166004
2078.468779	288323.199665	38.171021
2079.995650	288766.273851	38.176039
2082.969200	289189.237174	38.181056
2084.358274	289644.387769	38.186074
2086.959524	290074.868476	38.191092
2089.052258	290512.535247	38.196109
2091.257075	290962.902163	38.201127
2093.619638	291402.500948	38.206144
2095.803497	291840.017164	38.211162
2098.137983	292284.895227	38.216180
2100.079932	292723.179284	38.221197
2102.184098	293165.522544	38.226215
2104.072352	293588.981078	38.231232
2106.185169	294039.187315	38.236250
2108.569322	294474.037985	38.241268
2110.998265	294920.075007	38.246285
2112.828998	295368.436443	38.251303
2115.232887	295802.030119	38.256320
2116.934073	296249.821078	38.261338
2119.044353	296689.420307	38.266356
2121.230175	297126.237037	38.271373
2123.041554	297579.814205	38.276391
2125.794859	298019.810293	38.281408
2127.614717	298471.220999	38.286426
2130.014038	298920.836448	38.291444
2132.293155	299368.004512	38.296461
2134.219174	299804.333233	38.301479
2136.610650	300246.043784	38.306496
2138.355485	300691.253699	38.311514
2140.686418	301143.070220	38.316532
2143.102638	301581.288088	38.321549
2144.903275	302029.143732	38.326567
2146.889340	302474.478807	38.331584
2149.134964	302928.121310	38.336602
2151.147995	303368.900629	38.341620
2153.304051	303812.014653	38.346637
2155.584705	304267.086991	38.351655
2157.525151	304682.431032	38.356672
2159.508058	305118.808657	38.361690
2161.302925	305544.829886	38.366708
2163.657466	305967.764689	38.371725
2165.587830	306405.180229	38.376743
2167.917215	306841.793421	38.381760
2170.258731	307270.202126	38.386778
2172.045402	307708.517162	38.391796
2174.176324	308150.531108	38.396813
2176.226324	308584.101361	38.401831
2178.551193	309035.214712	38.406848
2180.617988	309486.313494	38.411866
2182.510868	309942.866994	38.416884
2184.448372	310399.282279	38.421901
2186.604479	310859.542363	38.426919
2188.831474	311315.142172	38.431936
2191.019940	311797.266615	38.436954
2192.913228	312267.503431	38.441972
2195.306032	312728.901171	38.446989
2197.528047	313208.518581	38.452007
2199.666931	313680.200154	38.457024
2201.716231	314165.925812	38.462042
2203.865682	314653.331071	38.467060
2206.377098	315137.248331	38.472077
2208.633196	315624.651881	38.477095
2210.990081	316105.994325	38.482112
2213.335883	316598.753527	38.487130
2215.404847	317094.773592	38.492148
2218.058488	317585.595749	38.497165
2220.147136	318067.441128	38.502183
2222.464604	318559.599268	38.507200
2224.842542	319043.748721	38.512218
2227.340636	319531.553577	38.517236
2229.640566	320025.245834	38.522253
2231.997976	320508.696941	38.527271
2234.172118	321004.554563	38.532288
2236.635782	321484.070158	38.537306
2238.852894	321979.300670	38.542324
2241.138419	322458.858445	38.547341
2243.305634	322950.202992	38.552359
2245.940058	323441.367168	38.557376
2248.465903	323938.277007	38.562394
2250.378600	324426.319928	38.567412
2252.607969	324904.741801	38.572429
2254.908180	325402.430435	38.577447
2257.606922	325873.866076	38.582464
2259.927148	326367.556244	38.587482
2262.379225	326852.364901	38.592500
2264.828721	327339.806761	38.597517
2266.566492	327828.140523	38.602535
2269.008321	328308.543845	38.607552
2271.494957	328788.071714	38.612570
2273.637196	329282.540088	38.617588
2276.301381	329752.286141	38.622605
2278.260019	330237.308083	38.627623
2280.890157	330718.185163	38.632640
2282.702301	331211.665875	38.637658
2284.954624	331693.883714	38.642676
2287.287172	332180.522430	38.647693
2289.533173	332663.388599	38.652711
2292.154219	333161.918065	38.657728
2294.405546	333646.800285	38.662746
2296.812389	334130.890904	38.667764
2299.074241	334606.956621	38.672781
2301.110713	335090.407829	38.677799
2303.734345	335577.616559	38.682816
2305.812462	336059.222223	38.687834
2308.117097	336534.749126	38.692852
2310.827589	336988.620496	38.697869
2312.718556	337457.478290	38.702887
2314.963336	337908.392601	38.707904
2317.011614	338364.709266	38.712922
2319.249633	338823.197137	38.717940
2321.939894	339277.195117	38.722957
2323.828436	339751.578066	38.727975
2326.074877	340205.075658	38.732992
2328.230968	340675.346323	38.738010
2330.484750	341157.541106	38.743028
2332.621986	341625.823761	38.748045
2335.278967	342108.272100	38.753063
2337.345408	342587.585249	38.758080
2339.605325	343082.407778	38.763098
2341.712483	343579.047717	38.768116
2343.959897	344077.788806	38.773133
2346.348430	344568.689726	38.778151
2348.556004	345058.521432	38.783168
2351.232702	345564.325011	38.788186
2353.151334	346075.235280	38.793204
2355.838419	346580.743059	38.798221
2358.015239	347086.449828	38.803239
2360.465325	347603.491746	38.808256
2362.754574	348117.710783	38.813274
2365.248474	348642.032535	38.818292
2367.627284	349163.777605	38.823309
2369.928631	349685.146164	38.828327
2372.480899	350204.159803	38.833344
2374.687921	350728.645179	38.838362
2376.685118	351245.244214	38.843380
2379.845576	351775.902161	38.848397
2382.293734	352309.527762	38.853415
2384.709900	352837.089990	38.858432
2387.144460	353363.854666	38.863450
2389.376773	353906.082003	38.868468
2392.339601	354432.087117	38.873485
2394.683787	354959.321042	38.878503
2396.894460	355475.336330	38.883520
2399.489803	356012.856580	38.888538
2402.159383	356547.415269	38.893556
2404.554556	357068.597468	38.898573
2407.087620	357603.209954	38.903591
2409.520177	358131.136670	38.908608
2412.031350	358662.058485	38.913626
2414.252742	359196.032829	38.918644
2417.117053	359721.202894	38.923661
2419.571156	360247.872805	38.928679
2421.894090	360772.019324	38.933696
2424.581205	361302.917941	38.938714
2426.541745	361829.916094	38.943732
2429.311852	362352.545561	38.948749
2431.597792	362882.540966	38.953767
2434.309192	363414.513234	38.958784
2436.942465	363935.716781	38.963802
2439.338381	364478.870597	38.968820
2441.691087	364994.219402	38.973837
2444.257066	365525.542436	38.978855
2446.685655	366045.979964	38.983872
2449.368990	366572.196918	38.988890
2451.872024	367095.416802	38.993908
2454.413596	367608.307286	38.998925
2456.549746	368141.524455	39.003943
2458.920965	368657.539589	39.008960
2461.488743	369178.835910	39.013978
2463.931986	369711.139296	39.018996
2466.573964	370235.723888	39.024013
2469.079847	370763.259182	39.029031
2471.323860	371275.090711	39.034048
2474.047818	371764.971644	39.039066
2476.184346	372272.798298	39.044084
2478.648020	372761.182094	39.049101
2480.788411	373255.333720	39.054119
2483.468234	373751.494920	39.059136
2485.701327	374249.161089	39.064154
2488.061998	374749.813030	39.069172
2490.487140	375258.425902	39.074189
2492.791315	375781.260299	39.079207
2495.125936	376292.629226	39.084224
2497.793666	376809.940160	39.089242
2500.391580	377334.446353	39.094260
2502.559084	377848.522257	39.099277
2505.012659	378371.688032	39.104295
2507.457353	378897.960544	39.109312
2509.561577	379435.699721	39.114330
2512.009434	379981.758272	39.119348
2514.990854	380511.435391	39.124365
2517.273876	381052.963476	39.129383
2519.664333	381605.759807	39.134400
2522.401257	382143.065722	39.139418
2524.699976	382698.436497	39.144436
2527.711457	383253.303924	39.149453
2529.970105	383805.795175	39.154471
2532.777731	384361.404949	39.159488
2535.340162	384914.584464	39.164506
2537.778778	385490.233879	39.169524
2539.979592	386036.506653	39.174541
2543.034239	386607.779886	39.179559
2545.293452	387180.329383	39.184576
2547.986410	387753.506967	39.189594
2550.659523	388317.077700	39.194612
2552.992469	388887.905288	39.199629
2555.831488	389462.894367	39.204647
2558.295172	390034.029545	39.209664
2560.961943	390609.727762	39.214682
2563.603492	391189.163531	39.219700
2566.609334	391767.009513	39.224717
2569.284130	392344.235309	39.229735
2571.365060	392920.527592	39.234752
2574.133832	393497.964359	39.239770
2577.098218	394078.495799	39.244788
2579.516171	394655.909003	39.249805
2581.974121	395231.378140	39.254823
2584.756496	395817.464966	39.259840
2587.537392	396388.400434	39.264858
2589.950782	396975.225125	39.269876
2592.930420	397558.706765	39.274893
2595.385639	398142.610301	39.279911
2597.559590	398721.531818	39.284928
2600.971544	399297.663759	39.289946
2603.257849	399880.790966	39.294964
2605.943798	400457.615113	39.299981
2608.724076	401046.912215	39.304999
2611.110566	401618.793830	39.310016
2614.307650	402197.063536	39.315034
2616.693375	402786.225873	39.320052
2619.371466	403358.372699	39.325069
2621.744562	403935.664378	39.330087
2624.434463	404519.875718	39.335104
2627.160899	405098.701915	39.340122
2629.595352	405681.759150	39.345140
2632.620224	406259.294248	39.350157
2635.143161	406837.145946	39.355175
2637.799324	407422.501458	39.360192
2640.748242	408010.072771	39.365210
2642.791284	408595.392027	39.370228
2645.836193	409164.499659	39.375245
2648.070270	409717.174410	39.380263
2650.882341	410269.340080	39.385280
2653.768095	410808.578883	39.390298
2656.591938	411359.045561	39.395316
2658.726965	411896.857046	39.400333
2661.250631	412449.720799	39.405351
2663.400543	413000.352375	39.410368
2666.342373	413565.668112	39.415386
2668.739779	414138.085565	39.420404
2670.980091	414694.476961	39.425421
2673.856064	415256.520941	39.430439
2676.075707	415845.714064	39.435456
2679.053439	416419.395788	39.440474
2681.447783	416995.682148	39.445492
2683.835484	417583.586686	39.450509
2686.484775	418182.408933	39.455527
2689.109633	418780.762717	39.460544
2692.224641	419379.427291	39.465562
2694.677738	419987.685696	39.470580
2697.246084	420593.531443	39.475597
2700.175151	421199.353606	39.480615
2702.611129	421821.264977	39.485632
2705.172718	422435.654135	39.490650
2707.932235	423056.567295	39.495668
2710.307390	423688.493832	39.500685
2713.352425	424316.857829	39.505703
2716.246119	424948.866336	39.510720
2719.024468	425581.884300	39.515738
2721.817029	426209.976186	39.520756
2724.659191	426836.069044	39.525773
2727.472761	427483.884750	39.530791
2729.606333	428127.792206	39.535808
2732.955115	428762.389778	39.540826
2735.729556	429407.217109	39.545844
2738.415052	430056.586538	39.550861
2741.384143	430695.579022	39.555879
2743.907156	431349.227551	39.560896
2746.671240	431991.697379	39.565914
2749.610981	432640.233950	39.570932
2752.425041	433308.680693	39.575949
2755.292386	433953.899743	39.580967
2758.103007	434610.324901	39.585984
2761.087039	435259.120596	39.591002
2763.874895	435910.956954	39.596020
2766.545852	436565.113783	39.601037
2769.633860	437213.523829	39.606055
2772.252681	437878.456752	39.611072
2775.178397	438530.737754	39.616090
2778.179615	439183.893861	39.621108
2780.639410	439834.939602	39.626125
2783.854970	440482.005128	39.631143
2786.767405	441140.411650	39.636160
2789.532253	441788.765394	39.641178
2792.472446	442423.935475	39.646196
2795.183650	443093.013408	39.651213
2798.396666	443734.409942	39.656231
2801.081399	444383.746157	39.661248
2803.812705	445024.162936	39.666266
2806.884195	445675.665802	39.671284
2809.675973	446323.704457	39.676301
2812.310792	446964.775393	39.681319
2815.337854	447615.205843	39.686336
2818.149994	448250.547641	39.691354
2820.839464	448903.155993	39.696372
2823.883665	449542.152722	39.701389
2826.929543	450182.237286	39.706407
2829.497527	450833.431187	39.711424
2832.578131	451455.439513	39.716442
2835.363603	452065.708717	39.721460
2838.150331	452671.816928	39.726477
2840.717648	453270.012733	39.731495
2843.442417	453881.339484	39.736512
2845.907050	454473.351699	39.741530
2849.012422	455090.634531	39.746548
2851.560727	455699.401645	39.751565
2854.421247	456314.610004	39.756583
2856.754040	456941.538488	39.761600
2859.564711	457568.975271	39.766618
2862.638539	458202.959689	39.771636
2865.090740	458833.384362	39.776653
2868.147814	459471.564051	39.781671
2870.861228	460124.660642	39.786688
2873.290476	460758.702099	39.791706
2875.980648	461413.317437	39.796724
2878.754133	462067.137708	39.801741
2881.734587	462739.266516	39.806759
2884.278770	463411.890950	39.811776
2886.949428	464083.308407	39.816794
2890.232054	464762.322264	39.821812
2892.849282	465456.597579	39.826829
2895.517665	466137.165220	39.831847
2898.477625	466834.356453	39.836864
2901.694057	467528.149197	39.841882
2904.605922	468233.208592	39.846900
2907.140019	468937.086496	39.851917
2910.222061	469643.067822	39.856935
2913.231358	470360.982861	39.861952
2916.000241	471076.382494	39.866970
2919.336522	471784.551620	39.871988
2921.973579	472510.347731	39.877005
2924.859114	473216.659199	39.882023
2927.983619	473940.751908	39.887040
2931.078560	474665.925994	39.892058
2933.917924	475391.964465	39.897076
2937.163328	476123.704343	39.902093
2940.386801	476843.869614	39.907111
2942.924023	477589.415812	39.912128
2946.610167	478315.894710	39.917146
2949.880956	479025.972903	39.922164
2952.465560	479760.370683	39.927181
2955.601257	480482.148536	39.932199
2958.268187	481217.876667	39.937216
2961.363088	481939.845834	39.942234
2964.785533	482669.239169	39.947252
2967.567659	483406.660396	39.952269
2970.842225	484125.577409	39.957287
2973.885622	484862.435042	39.962304
2976.746528	485589.309847	39.967322
2979.893409	486310.412396	39.972340
2982.639035	487044.038068	39.977357
2985.570537	487776.743092	39.982375
2989.003589	488498.000080	39.987392
2991.747332	489237.414510	39.992410
2995.071277	489969.599962	39.997428
2997.846393	490691.611098	40.002445
3001.249102	491416.712940	40.007463
3004.104165	492145.743419	40.012480
3006.715998	492876.790927	40.017498
3010.578263	493603.578527	40.022516
3013.275845	494330.915664	40.027533
3016.298314	495051.167328	40.032551
3019.340202	495780.444128	40.037568
3022.289637	496501.945779	40.042586
3025.581361	497228.493893	40.047604
3028.172991	497951.088111	40.052621
3031.621343	498663.343902	40.057639
3034.368525	499359.868342	40.062656
3037.154121	500054.340075	40.067674
3040.454904	500731.181945	40.072692
3042.920422	501427.651446	40.077709
3045.936027	502109.657659	40.082727
3048.902790	502803.466047	40.087744
3051.804630	503497.804722	40.092762
3054.861856	504201.093121	40.097780
3058.152457	504911.103592	40.102797
3060.796023	505615.041303	40.107815
3063.496298	506320.293857	40.112832
3066.286231	507038.276574	40.117850
3069.777325	507762.049766	40.122868
3072.466560	508491.394685	40.127885
3075.456561	509208.229769	40.132903
3078.549008	509960.022023	40.137920
3081.447115	510702.750607	40.142938
3084.751325	511438.636584	40.147956
3087.368739	512204.364721	40.152973
3090.342169	512946.157351	40.157991
3093.572278	513717.640532	40.163008
3096.388796	514486.781954	40.168026
3099.956043	515247.064293	40.173044
3103.259914	516034.697724	40.178061
3106.337567	516801.406303	40.183079
3109.321100	517567.935796	40.188096
3112.444071	518348.476226	40.193114
3115.608586	519127.708669	40.198132
3118.829104	519926.239589	40.203149
3121.921496	520701.371573	40.208167
3125.135852	521492.472592	40.213184
3128.349923	522288.602988	40.218202
3131.604850	523064.829743	40.223220
3134.688425	523865.861845	40.228237
3137.867337	524655.324329	40.233255
3140.854201	525456.225653	40.238272
3144.133489	526263.262793	40.243290
3147.245947	527057.365587	40.248308
3150.857481	527873.596647	40.253325
3153.985462	528678.600705	40.258343
3157.335496	529481.059420	40.263360
3160.188633	530280.683718	40.268378
3163.807584	531082.600166	40.273396
3166.443597	531904.758875	40.278413
3169.630377	532719.598428	40.283431
3173.433413	533526.557459	40.288448
3176.464052	534347.143458	40.293466
3179.995482	535144.855111	40.298484
3182.988955	535961.779070	40.303501
3186.298129	536767.958992	40.308519
3189.741214	537573.263864	40.313536
3192.752665	538391.936873	40.318554
3196.293849	539195.115814	40.323572
3199.128268	540003.021719	40.328589
3203.066081	540805.032529	40.333607
3206.227284	541608.016892	40.338624
3209.219774	542421.714361	40.343642
3212.751779	543230.859192	40.348660
3215.876012	544029.027740	40.353677
3219.248988	544830.517667	40.358695
3222.465521	545626.863464	40.363712
3225.758372	546437.592733	40.368730
3229.172122	547223.973104	40.373748
3231.999808	548028.149912	40.378765
3235.102983	548831.729489	40.383783
3239.103177	549627.894684	40.388800
3241.926579	550440.088115	40.393818
3244.973714	551216.992602	40.398836
3248.247753	551983.583584	40.403853
3251.612918	552742.792000	40.408871
3254.506069	553497.614865	40.413888
3257.539977	554260.539652	40.418906
3260.759382	555014.264053	40.423924
3263.873818	555778.934571	40.428941
3266.854574	556545.882701	40.433959
3270.411134	557313.393216	40.438976
3272.955150	558098.452161	40.443994
3276.561115	558870.865885	40.449012
3279.590360	559663.863354	40.454029
3282.961177	560463.367946	40.459047
3286.060058	561249.484112	40.464064
3288.855790	562056.786158	40.469082
3292.106105	562865.464431	40.474100
3295.694272	563674.234399	40.479117
3298.553271	564496.185005	40.484135
3302.017598	565312.874538	40.489152
3305.011933	566145.254982	40.494170
3308.442455	566969.795798	40.499188
3311.902679	567804.638089	40.504205
3314.704999	568645.681212	40.509223
3318.273770	569492.400589	40.514240
3321.082539	570344.232444	40.519258
3324.436153	571197.968049	40.524276
3328.226982	572067.138065	40.529293
3331.499623	572932.619019	40.534311
3334.954438	573780.039010	40.539328
3338.327435	574664.239342	40.544346
3341.432575	575533.701080	40.549364
3344.739947	576411.970165	40.554381
3348.043129	577304.830093	40.559399
3351.776498	578183.794337	40.564416
3355.237243	579079.289423	40.569434
3358.650747	579960.664738	40.574452
3362.285232	580854.289121	40.579469
3365.194246	581736.702504	40.584487
3368.635831	582628.413361	40.589504
3372.364987	583525.357338	40.594522
3375.955709	584423.549692	40.599540
3379.003078	585315.054171	40.604557
3382.490993	586213.815591	40.609575
3386.131064	587120.726784	40.614592
3389.169535	588016.460476	40.619610
3392.622090	588923.700208	40.624628
3396.489150	589822.503450	40.629645
3399.741486	590718.929356	40.634663
3402.794418	591622.756518	40.639680
3406.731485	592541.207661	40.644698
3410.191328	593450.212785	40.649716
3413.408406	594345.441557	40.654733
3417.074950	595260.703758	40.659751
3420.789425	596162.045132	40.664768
3424.032486	597071.823217	40.669786
3427.311983	597976.723443	40.674804
3431.190019	598884.647913	40.679821
3434.876568	599792.823376	40.684839
3438.110527	600698.694428	40.689856
3441.731169	601605.824188	40.694874
3445.299828	602506.544082	40.699892
3448.916149	603402.586812	40.704909
3451.421918	604304.165334	40.709927
3455.558157	605206.707787	40.714944
3459.073448	606105.925265	40.719962
3462.255769	607008.907964	40.724980
3466.210486	607917.277837	40.729997
3469.414185	608816.057063	40.735015
3473.138871	609706.726004	40.740020
3476.153885	610542.823923	40.745024
3479.268591	611335.839097	40.750029
3482.535006	612081.223844	40.755034
3485.520077	612791.653989	40.760039
3488.991945	613425.676861	40.765044
3491.629876	614001.557842	40.770048
3494.090784	614531.000020	40.775053
3496.586214	615003.681744	40.780058
3499.011137	615424.575231	40.785063
3501.326633	615782.498421	40.790068
3503.450949	616103.057819	40.795072
3505.227915	616381.783843	40.800077
3507.285781	616597.943345	40.805082
3508.704038	616790.361972	40.810087
3511.008614	616931.218948	40.815092
3512.115242	617033.034936	40.820096
3513.544957	617097.871955	40.825101
3514.686391	617132.722076	40.830106
3515.669308	617132.018731	40.835111
3516.898152	617098.546952	40.840116
3517.574864	617054.817643	40.845120
3518.350951	616967.698582	40.850125
3519.450109	616851.495288	40.855130
3519.587999	616727.245613	40.860135
3520.670561	616579.659679	40.865140
3521.170141	616426.765636	40.870144
3521.764232	616233.225825	40.875149
3522.428726	616042.020084	40.880154
3522.435992	615832.522341	40.885159
3522.965125	615602.198203	40.890164
3523.323964	615374.694174	40.895168
3523.114454	615130.930602	40.900173
3523.737615	614878.384300	40.905178
3523.747310	614612.532407	40.910183
3523.378138	614335.486473	40.915188
3523.679348	614071.374102	40.920192
3523.694810	613798.351989	40.925197
3523.924277	613513.641971	40.930202
3523.640776	613233.703052	40.935207
3524.434881	612935.141523	40.940212
3523.998141	612643.112536	40.945216
3523.891353	612334.425794	40.950221
3524.001525	612025.595725	40.955226
3523.165112	611729.953233	40.960231
3522.986428	611432.399372	40.965236
3523.246643	611144.667993	40.970240
3523.188577	610831.927933	40.975245
3523.238705	610534.962004	40.980250
3522.706189	610234.628240	40.985255
3522.750532	609924.794478	40.990260
3522.602494	609632.283638	40.995264
3522.333838	609327.031223	41.000269
3522.452756	609029.510566	41.005274
3522.022886	608722.014830	41.010279
3521.969047	608428.754616	41.015284
3521.598777	608131.234269	41.020288
3521.547241	607838.606962	41.025293
3521.464809	607546.676361	41.030298
3521.047872	607256.090213	41.035303
3520.939306	606961.446062	41.040308
3520.697330	606680.520062	41.045312
3520.485754	606393.779041	41.050317
3520.561967	606107.485276	41.055322
3519.990492	605830.989670	41.060327
3519.765838	605559.935328	41.065332
3519.415959	605282.740028	41.070336
3519.357009	605014.547058	41.075341
3519.741950	604742.675549	41.080346
3519.059543	604477.718019	41.085351
3518.720275	604211.599333	41.090356
3518.530906	603949.403071	41.095360
3518.475968	603686.278519	41.100365
3518.176263	603435.294433	41.105370
3517.809056	603177.059332	41.110375
3517.576355	602917.745957	41.115380
3517.454476	602675.922912	41.120384
3517.159959	602425.914424	41.125389
3517.028797	602184.331609	41.130394
3516.458494	601947.415870	41.135399
3516.732830	601707.360003	41.140404
3515.934220	601470.619248	41.145408
3515.778386	601255.693306	41.150413
3515.955647	601030.000552	41.155418
3515.646875	600809.383833	41.160423
3515.708778	600585.751540	41.165428
3515.418800	600372.930526	41.170432
3515.226684	600150.279612	41.175437
3515.212726	599931.750553	41.180442
3514.732664	599716.843673	41.185447
3514.724887	599509.517049	41.190452
3514.499003	599307.276128	41.195456
3514.114800	599090.038823	41.200461
3514.162190	598896.307095	41.205466
3513.395791	598695.540527	41.210471
3513.494292	598501.693418	41.215476
3513.346195	598321.047383	41.220480
3512.984357	598125.413046	41.225485
3513.068722	597939.767983	41.230490
3513.019241	597759.998043	41.235495
3512.540476	597580.041824	41.240500
3512.598837	597400.148763	41.245504
3512.535332	597227.481245	41.250509
3512.529010	597035.576156	41.255514
3512.647945	596862.824092	41.260519
3512.175736	596676.743147	41.265524
3511.926589	596514.056713	41.270528
3511.367991	596341.051556	41.275533
3511.661735	596169.512609	41.280538
3511.409117	596018.135217	41.285543
3511.163093	595856.189269	41.290548
3511.035629	595701.482982	41.295552
3510.855052	595546.532370	41.300557
3510.561012	595393.349859	41.305562
3510.312043	595241.660364	41.310567
3510.378923	595094.476282	41.315572
3509.987720	594942.754677	41.320576
3509.870565	594798.850286	41.325581
3510.163576	594666.297718	41.330586
3509.798395	594527.987141	41.335591
3509.984931	594383.228389	41.340596
3509.693912	594257.172238	41.345600
3509.287203	594119.013081	41.350605
3509.302377	593993.206426	41.355610
3509.147710	593862.366534	41.360615
3509.045874	593735.823901	41.365620
3508.973123	593605.218464	41.370624
3508.886817	593476.416573	41.375629
3509.103638	593363.592813	41.380634
3508.626417	593237.303292	41.385639
3508.530849	593108.698756	41.390644
3508.647225	592991.679568	41.395648
3508.232442	592867.930321	41.400653
3508.350532	592760.575102	41.405658
3508.072597	592649.373860	41.410663
3508.327409	592526.016861	41.415668
3507.924397	592409.272854	41.420672
3507.772978	592303.357675	41.425677
3508.087496	592188.001773	41.430682
3508.068122	592078.056519	41.435687
3507.776997	591968.803805	41.440692
3507.382141	591869.784875	41.445696
3507.537533	591770.729103	41.450701
3507.626626	591663.768168	41.455706
3507.288380	591563.234783	41.460711
3507.213618	591457.599826	41.465716
3506.831077	591361.880452	41.470720
3506.844434	591264.144654	41.475725
3506.756001	591167.525966	41.480730
3506.765085	591085.318596	41.485735
3506.131671	590988.683305	41.490740
3506.204915	590911.674524	41.495744
3506.422084	590819.964444	41.500749
3506.577621	590730.216996	41.505754
3506.302980	590651.707737	41.510759
3506.375677	590553.104550	41.515764
3506.464010	590475.589315	41.520768
3506.368650	590389.335014	41.525773
3506.374521	590306.571116	41.530778
3505.996772	590228.325383	41.535783
3506.005907	590141.651970	41.540788
3506.015487	590061.941690	41.545792
3505.429161	589986.332004	41.550797
3505.098643	589897.405110	41.555802
3505.392604	589837.989596	41.560807
3506.088890	589767.187965	41.565812
3505.737492	589687.731757	41.570816
3505.508738	589614.318140	41.575821
3505.386519	589531.167502	41.580826
3505.375998	589469.843569	41.585831
3504.815260	589399.787170	41.590836
3504.717684	589335.419796	41.595840
3504.932794	589278.368390	41.600845
3505.307257	589204.557067	41.605850
3504.971217	589148.493008	41.610855
3504.954198	589078.349526	41.615860
3504.902404	589019.284192	41.620864
3504.658007	588950.979203	41.625869
3504.846767	588886.414079	41.630874
3504.594449	588835.696588	41.635879
3504.721664	588778.155230	41.640884
3504.665028	588711.322553	41.645888
3504.753716	588649.677823	41.650893
3504.745379	588588.348552	41.655898
3504.589193	588525.137977	41.660903
3504.812540	588465.575647	41.665908
3505.057361	588409.316738	41.670912
3504.850368	588351.725147	41.675917
3505.073576	588282.841764	41.680922
3504.386442	588224.723258	41.685927
3504.833200	588164.272505	41.690932
3504.831520	588114.063649	41.695936
3504.537610	588054.028723	41.700941
3504.355136	587984.054349	41.705946
3504.181311	587941.287821	41.710951
3504.414640	587883.574799	41.715956
3504.105135	587828.552067	41.720960
3504.160629	587774.824981	41.725965
3504.201024	587716.389574	41.730970
3504.063211	587671.411476	41.735975
3504.298082	587626.324820	41.740980
3504.352109	587565.932133	41.745984
3504.231560	587507.370427	41.750989
3504.369460	587456.385033	41.755994
3504.025076	587399.561546	41.760999
3504.209716	587358.941627	41.766004
3504.663779	587314.420762	41.771008
3504.251019	587253.848751	41.776013
3504.269157	587186.694317	41.781018
3504.460497	587154.491614	41.786023
3504.193711	587093.444868	41.791028
3503.827485	587036.673012	41.796032
3503.679322	586993.197145	41.801037
3504.098894	586940.862334	41.806042
3503.771544	586893.605385	41.811047
3504.247459	586845.521051	41.816052
3503.861047	586804.687647	41.821056
3503.902573	586758.825783	41.826061
3504.205639	586704.754019	41.831066
3503.769656	586659.216961	41.836071
3503.799978	586601.729340	41.841076
3503.959019	586562.563816	41.846080
3503.735551	586515.238869	41.851085
3504.100763	586463.411429	41.856090
3503.752667	586421.868966	41.861095
3503.772801	586375.156847	41.866100
3503.751214	586325.494134	41.871104
3503.613283	586289.481322	41.876109
3503.536648	586236.468943	41.881114
3503.444420	586201.551285	41.886119
3503.523453	586164.451669	41.891124
3504.050264	586120.165148	41.896128
3503.626965	586068.459101	41.901133
3503.685897	586022.691657	41.906138
3503.755217	585995.416231	41.911143
3503.952436	585946.218774	41.916148
3503.909605	585886.683943	41.921152
3503.724450	585844.762974	41.926157
3503.853292	585802.291560	41.931162
3503.713656	585765.325012	41.936167
3503.296759	585712.162800	41.941172
3503.425383	585677.108699	41.946176
3503.418831	585633.154188	41.951181
3503.723233	585593.862225	41.956186
3503.386922	585552.314607	41.961191
3503.637324	585509.321844	41.966196
3503.483361	585478.320959	41.971200
3503.210515	585439.870501	41.976205
3503.426453	585393.374179	41.981210
3503.394016	585350.575374	41.986215
3503.255218	585323.280683	41.991220
3503.291374	585276.811972	41.996224
3503.421149	585245.565582	42.001229
3503.831880	585194.326478	42.006234
3503.438648	585155.793595	42.011239
3503.572438	585104.296628	42.016244
3503.774468	585070.782916	42.021248
3503.517145	585031.827366	42.026253
3503.687567	584984.734948	42.031258
3503.445838	584942.518622	42.036263
3503.871375	584903.556112	42.041268
3503.821315	584863.715459	42.046272
3503.618341	584819.036525	42.051277
3503.813657	584773.643529	42.056282
3503.420707	584737.164224	42.061287
3503.499214	584696.751495	42.066292
3503.866546	584645.917611	42.071296
3503.536662	584607.222518	42.076301
3503.824215	584556.250314	42.081306
3503.417471	584512.454116	42.086311
3503.717097	584464.386879	42.091316
3503.675862	584430.458109	42.096320
3503.576574	584388.718640	42.101325
3503.401191	584339.471961	42.106330
3503.093947	584306.987931	42.111335
3503.360356	584265.140696	42.116340
3503.228050	584220.498402	42.121344
3503.022028	584193.261530	42.126349
3503.445458	584154.146311	42.131354
3502.965294	584120.184944	42.136359
3503.455743	584083.164342	42.141364
3503.280386	584048.703956	42.146368
3502.975790	584014.414049	42.151373
3503.277391	583983.337714	42.156378
3503.233784	583946.299884	42.161383
3503.337789	583910.742702	42.166388
3503.179347	583867.757292	42.171392
3502.913236	583829.801412	42.176397
3503.271770	583796.560117	42.181402
3503.123107	583766.305490	42.186407
3502.999952	583726.923296	42.191412
3503.296174	583683.916219	42.196416
3502.956836	583652.788760	42.201421
3503.200099	583609.238245	42.206426
3503.547891	583583.517433	42.211431
3502.991700	583545.405399	42.216436
3502.990059	583503.847821	42.221440
3503.060880	583466.589966	42.226445
3503.277265	583427.053357	42.231450
3503.416287	583406.979383	42.236455
3502.912529	583361.739969	42.241460
3502.837757	583328.565000	42.246464
3502.618746	583301.127423	42.251469
3502.887619	583261.331358	42.256474
3502.647107	583232.393033	42.261479
3502.865430	583204.686321	42.266484
3503.145635	583174.513416	42.271488
3502.879853	583140.264844	42.276493
3502.872994	583115.250094	42.281498
3502.531280	583078.406340	42.286503
3502.711297	583043.536322	42.291508
3502.836260	583017.548231	42.296512
3503.071521	582991.743366	42.301517
3502.833732	582960.848734	42.306522
3502.951728	582933.959149	42.311527
3502.903554	582899.074214	42.316532
3502.799710	582855.976048	42.321536
3502.746658	582831.719873	42.326541
3502.896878	582797.104401	42.331546
3502.823362	582770.144087	42.336551
3502.798025	582736.708940	42.341556
3502.996557	582711.059561	42.346560
3502.342107	582689.704579	42.351565
3502.599154	582652.615394	42.356570
3502.507844	582627.211667	42.361575
3502.795683	582595.732499	42.366580
3502.963995	582565.074077	42.371584
3503.074198	582543.298466	42.376589
3503.178193	582502.522749	42.381594
3502.698411	582472.165924	42.386599
3502.809392	582429.634126	42.391604
3503.053210	582398.061006	42.396608
3502.401895	582374.799785	42.401613
3502.876160	582343.090212	42.406618
3502.541812	582316.821326	42.411623
3502.544269	582291.502439	42.416628
3502.925706	582263.065965	42.421632
3502.608746	582229.073239	42.426637
3502.994267	582207.304062	42.431642
3502.717433	582180.323955	42.436647
3502.806537	582141.404270	42.441652
3503.163615	582117.182682	42.446656
3502.969597	582078.156625	42.451661
3502.871925	582040.168242	42.456666
3502.561026	582014.997981	42.461671
3502.554089	581991.885899	42.466676
3502.798786	581971.642384	42.471680
3502.312660	581932.160105	42.476685
3502.826805	581906.208832	42.481690
3502.587966	581886.141026	42.486695
3502.812996	581854.619430	42.491700
3502.843129	581829.796534	42.496704
3502.560593	581800.259364	42.501709
3502.545580	581767.120493	42.506714
3502.815269	581735.290747	42.511719
3502.811772	581707.915788	42.516724
3502.781563	581687.714729	42.521728
3502.656071	581656.498057	42.526733
3502.975981	581623.707507	42.531738
3502.519830	581592.341790	42.536743
3502.509848	581561.357486	42.541748
3502.773956	581545.923498	42.546752
3502.307058	581519.472879	42.551757
3502.627614	581482.770956	42.556762
3502.924784	581458.807991	42.561767
3502.672188	581432.223382	42.566772
3502.716023	581398.322114	42.571776
3502.809566	581382.814284	42.576781
3502.956747	581342.930055	42.581786
3502.612531	581319.819156	42.586791
3502.560738	581282.573098	42.591796
3502.850721	581256.404648	42.596800
3502.985331	581232.065483	42.601805
3503.134003	581198.799041	42.606810
3502.798999	581166.861631	42.611815
3502.687146	581136.293189	42.616820
3502.484865	581097.214820	42.621824
3502.275304	581076.188285	42.626829
3502.667360	581053.563422	42.631834
3502.561115	581037.083516	42.636839
3502.378252	581009.785012	42.641844
3502.616497	580973.645827	42.646848
3502.695891	580953.275870	42.651853
3502.774139	580922.977971	42.656858
3502.519748	580892.130286	42.661863
3502.390747	580867.931816	42.666868
3502.650561	580845.377344	42.671872
3502.658282	580828.728886	42.676877
3502.877177	580788.530598	42.681882
3502.711889	580762.733012	42.686887
3502.396698	580726.077828	42.691892
3502.684926	580707.780768	42.696896
3502.356059	580680.153277	42.701901
3502.651684	580651.425228	42.706906
3502.605868	580631.024110	42.711911
3502.501815	580602.308273	42.716916
3502.677928	580569.135939	42.721920
3502.730648	580541.899741	42.726925
3502.885515	580513.694777	42.731930
3502.584996	580486.964959	42.736935
3502.555098	580449.562248	42.741940
3502.878988	580434.117371	42.746944
3502.700263	580402.905487	42.751949
3502.479787	580361.821601	42.756954
3502.655565	580341.535742	42.761959
3502.593288	580313.915807	42.766964
3502.243912	580286.290539	42.771968
3502.417128	580268.512184	42.776973
3502.600219	580245.818056	42.781978
3502.514624	580215.092534	42.786983
3502.257727	580193.620419	42.791988
3502.646899	580181.123549	42.796993
3502.754289	580149.264481	42.801997
3502.602283	580126.572350	42.807002
3502.461777	580088.734406	42.812007
3502.253938	580072.118511	42.817012
3502.306157	580045.884089	42.822017
3502.297637	580027.682447	42.827021
3502.328168	579995.082765	42.832026
3501.961707	579978.942842	42.837031
3502.476167	579951.482574	42.842036
3502.838541	579928.007578	42.847041
3502.395476	579908.870747	42.852045
3502.640158	579880.800576	42.857050
3502.418044	579855.210349	42.862055
3502.343915	579821.623586	42.867060
3502.320394	579800.264666	42.872065
3502.098356	579783.249383	42.877069
3502.359455	579756.379860	42.882074
3502.387098	579735.664731	42.887079
3502.167146	579708.368822	42.892084
3502.306221	579692.550631	42.897089
3501.733087	579663.905698	42.902093
3502.203666	579639.560670	42.907098
3502.293347	579623.048034	42.912103
3501.884078	579600.896524	42.917108
3502.021854	579590.293763	42.922113
3502.059473	579577.550289	42.927117
3502.273310	579545.723001	42.932122
3502.150581	579535.160912	42.937127
3502.152921	579525.782817	42.942132
3502.431384	579495.600172	42.947137
3502.001074	579467.534184	42.952141
3502.362660	579444.760372	42.957146
3502.420066	579427.349818	42.962151
3502.563399	579409.123426	42.967156
3502.122205	579385.371718	42.972161
3501.931646	579356.014249	42.977165
3502.104290	579337.632711	42.982170
3502.607641	579319.299741	42.987175
3502.558717	579292.026223	42.992180
3502.656548	579272.302244	42.997185
3502.212260	579249.503566	43.002189
3502.427331	579217.825597	43.007194
3502.375803	579189.649544	43.012199
3502.235425	579177.735833	43.017204
3502.376336	579152.137387	43.022209
3502.026080	579114.930718	43.027213
3502.546410	579101.910639	43.032218
3502.546197	579082.803452	43.037223
3502.148203	579054.681220	43.042228
3502.315079	579026.019257	43.047233
3501.984220	579020.704858	43.052237
3502.154672	578992.744357	43.057242
3502.421443	578970.235152	43.062247
3502.599595	578953.055736	43.067252
3502.431029	578923.342632	43.072257
3502.324832	578899.788272	43.077261
3501.834257	578880.556793	43.082266
3502.105572	578869.029752	43.087271
3501.843948	578849.160613	43.092276
3502.331640	578826.365826	43.097281
3502.076125	578819.585164	43.102285
3502.563462	578781.795080	43.107290
3502.503012	578769.717984	43.112295
3502.253696	578744.430364	43.117300
3502.020761	578710.814925	43.122305
3502.259550	578698.891579	43.127309
3502.526503	578674.275370	43.132314
3502.739127	578657.090110	43.137319
3502.147296	578627.442386	43.142324
3502.489718	578592.382536	43.147329
3502.419779	578580.958699	43.152333
3502.432848	578547.504920	43.157338
3502.564616	578527.974931	43.162343
3502.735420	578503.674293	43.167348
3502.199052	578471.309234	43.172353
3502.009798	578452.431132	43.177357
3502.380222	578425.942541	43.182362
3502.528340	578408.616523	43.187367
3502.405216	578388.373839	43.192372
3502.119573	578362.439039	43.197377
3502.494421	578341.065200	43.202381
3502.355959	578308.737772	43.207386
3502.042896	578301.865483	43.212391
3502.278857	578276.400631	43.217396
3502.843529	578255.849569	43.222401
3502.211766	578231.021803	43.227405
3502.342952	578210.036884	43.232410
3501.882271	578192.103547	43.237415
3502.102779	578160.020495	43.242420
3502.021049	578143.382005	43.247425
3502.118921	578127.066494	43.252429
3502.319904	578100.001767	43.257434
3502.061792	578077.472511	43.262439
3501.953404	578061.791005	43.267444
3502.117567	578035.935593	43.272449
3501.765062	578023.301487	43.277453
3502.255914	578002.911967	43.282458
3502.153083	578001.423366	43.287463
3501.969563	577974.568909	43.292468
3501.902494	577940.824911	43.297473
3501.863221	577935.263786	43.302477
3501.741166	577907.647230	43.307482
3501.913274	577902.554599	43.312487
3501.957494	577887.952412	43.317492
3502.410449	577862.201919	43.322497
3502.202858	577855.563643	43.327501
3502.479913	577821.213776	43.332506
3501.696361	577797.161109	43.337511
3501.921673	577785.138587	43.342516
3502.543874	577762.972638	43.347521
3501.905827	577747.223024	43.352525
3502.103485	577727.681337	43.357530
3502.075051	577703.059014	43.362535
3502.302420	577682.559634	43.367540
3502.367096	577656.718899	43.372545
3501.871757	577655.743021	43.377549
3502.125433	577630.625028	43.382554
3502.046332	577614.838003	43.387559
3502.065957	577590.960272	43.392564
3502.228371	577562.495884	43.397569
3501.795587	577541.999134	43.402573
3502.080089	577527.659857	43.407578
3501.859970	577520.772555	43.412583
3501.994255	577510.168368	43.417588
3502.189449	577501.661255	43.422593
3501.785907	577475.040624	43.427597
3502.240442	577441.765310	43.432602
3502.383676	577428.100039	43.437607
3501.974400	577413.818916	43.442612
3502.058726	577395.799098	43.447617
3501.652610	577379.561286	43.452621
3501.828209	577361.376670	43.457626
3502.133656	577347.033889	43.462631
3501.857969	577336.092365	43.467636
3501.577585	577303.132162	43.472641
3501.846463	577293.861000	43.477645
3501.777328	577280.830647	43.482650
3502.110013	577271.348859	43.487655
3502.104109	577254.897826	43.492660
3501.986634	577234.702328	43.497665
3502.360684	577213.175991	43.502669
3502.391544	577193.007387	43.507674
3502.103391	577160.750201	43.512679
3501.857477	577153.967022	43.517684
3502.168663	577121.164598	43.522689
3502.265948	577118.240144	43.527693
3501.945103	577086.790398	43.532698
3502.394340	577083.309323	43.537703
3501.908655	577047.320755	43.542708
3502.189630	577036.542712	43.547713
3502.092433	577014.186795	43.552717
3502.260339	576996.554545	43.557722
3501.609281	576967.563743	43.562727
3502.471599	576958.199533	43.567732
3502.473936	576933.119271	43.572737
3502.299168	576914.938545	43.577741
3502.472085	576893.392879	43.582746
3502.444985	576877.446206	43.587751
3501.720123	576856.442098	43.592756
3502.203527	576829.129513	43.597761
3502.676598	576822.484536	43.602765
3502.308662	576791.843889	43.607770
3502.090312	576756.113555	43.612775
3501.985811	576750.110593	43.617780
3501.989664	576727.236701	43.622785
3501.813151	576713.419903	43.627789
3502.377511	576692.615230	43.632794
3502.370695	576668.388543	43.637799
3502.338585	576651.990884	43.642804
3502.192136	576627.785938	43.647809
3502.162791	576604.114406	43.652813
3502.219698	576583.338700	43.657818
3502.497912	576553.649779	43.662823
3502.282714	576539.537845	43.667828
3502.236777	576515.015973	43.672833
3501.856975	576492.402225	43.677837
3502.332920	576483.499321	43.682842
3502.238021	576460.038381	43.687847
3502.328141	576439.156893	43.692852
3502.642828	576411.568699	43.697857
3502.362846	576382.167235	43.702861
3502.345593	576358.744108	43.707866
3502.326595	576330.957069	43.712871
3502.028406	576307.427265	43.717876
3502.137890	576294.066866	43.722881
3501.918274	576281.811316	43.727885
3502.065019	576261.121296	43.732890
3501.974634	576246.086551	43.737895
3501.885443	576227.791007	43.742900
3502.375498	576207.247871	43.747905
3502.162597	576196.395743	43.752909
3502.238708	576178.224766	43.757914
3502.222559	576152.593857	43.762919
3502.230570	576131.875124	43.767924
3502.103668	576104.355211	43.772929
3502.318534	576092.282349	43.777933
3501.923760	576073.432363	43.782938
3501.905408	576059.188725	43.787943
3501.622823	576041.976549	43.792948
3502.180346	576022.626460	43.797953
3501.738964	576006.241676	43.802957
3501.567182	575990.818002	43.807962
3501.642235	575967.780942	43.812967
3501.712402	575961.499432	43.817972
3502.152793	575934.693045	43.822977
3501.749323	575918.402535	43.827981
3501.929395	575909.595598	43.832986
3502.416390	575890.808116	43.837991
3502.073432	575875.661866	43.842996
3502.444294	575840.438483	43.848001
3502.317320	575833.134262	43.853005
3502.108380	575803.017871	43.858010
3502.286875	575775.549740	43.863015
3502.354775	575759.837455	43.868020
3502.291370	575736.219587	43.873025
3502.214858	575726.599811	43.878029
3502.209337	575698.909435	43.883034
3502.477009	575671.978929	43.888039
3502.398887	575654.232542	43.893044
3502.204237	575623.461285	43.898049
3502.001348	575608.292777	43.903053
3502.335329	575590.983524	43.908058
3502.073118	575568.801025	43.913063
3501.961741	575565.206466	43.918068
3501.857495	575541.243411	43.923073
3502.058469	575517.684086	43.928077
3501.961881	575501.094165	43.933082
3502.129583	575472.523327	43.938087
3502.143074	575461.785596	43.943092
3501.962673	575431.312584	43.948097
3502.055188	575430.946930	43.953101
3501.798449	575409.164592	43.958106
3501.724335	575393.875331	43.963111
3501.646598	575389.322290	43.968116
3501.872235	575356.578267	43.973121
3501.832191	575346.450797	43.978125
3502.064365	575332.919579	43.983130
3501.766385	575302.865936	43.988135
3501.695675	575299.967273	43.993140
3502.024081	575291.186833	43.998145
3501.797872	575270.302462	44.003149
3501.915919	575249.414403	44.008154
3501.910535	575226.689407	44.013159
3501.583904	575213.797244	44.018164
3502.165303	575206.030704	44.023169
3502.139995	575191.736889	44.028173
3501.785850	575174.534572	44.033178
3501.873924	575149.888441	44.038183
3501.809632	575131.537055	44.043188
3502.049133	575123.422565	44.048193
3502.126279	575097.072319	44.053197
3502.064499	575080.677009	44.058202
3502.164421	575050.660826	44.063207
3502.339930	575037.890636	44.068212
3502.298961	575012.160676	44.073217
3501.851691	574997.079717	44.078221
3501.930804	574972.033251	44.083226
3502.030068	574953.806513	44.088231
3501.932048	574948.804948	44.093236
3502.133394	574921.883022	44.098241
3501.928876	574914.339483	44.103245
3501.875562	574893.226709	44.108250
3502.195893	574887.507520	44.113255
3501.981054	574870.935158	44.118260
3502.393672	574835.100084	44.123265
3501.819949	574827.714542	44.128269
3501.673718	574810.930689	44.133274
3502.016475	574797.883236	44.138279
3501.783827	574775.042350	44.143284
3501.777323	574755.427084	44.148289
3501.522156	574758.426948	44.153293
3501.620488	574735.082714	44.158298
3501.853139	574720.597467	44.163303
3501.474788	574709.920277	44.168308
3501.806623	574684.683157	44.173313
3501.570621	574682.512553	44.178317
3501.583188	574680.604109	44.183322
3501.949172	574667.352195	44.188327
3501.742563	574654.390459	44.193332
3502.154279	574636.064194	44.198337
3501.632211	574611.763122	44.203341
3501.473982	574596.285248	44.208346
3501.606135	574594.307924	44.213351
3501.595718	574582.519520	44.218356
3501.692019	574554.509396	44.223361
3501.257715	574548.406304	44.228365
3501.687788	574552.703870	44.233370
3501.668911	574535.147142	44.238375
3501.807729	574510.240830	44.243380
3501.813477	574495.790767	44.248385
3501.621308	574486.238184	44.253389
3501.753720	574464.543697	44.258394
3501.861241	574461.215590	44.263399
3501.928922	574444.197067	44.268404
3501.784734	574419.836508	44.273409
3501.466013	574409.450736	44.278413
3501.988757	574392.461339	44.283418
3501.722500	574373.136871	44.288423
3501.443251	574366.708413	44.293428
3501.567706	574358.310334	44.298433
3501.878483	574345.518216	44.303437
3502.065313	574328.430722	44.308442
3501.952720	574315.052527	44.313447
3501.286210	574298.650276	44.318452
3501.450107	574287.285857	44.323457
3501.566165	574285.210653	44.328461
3501.775068	574265.861892	44.333466
3502.119507	574240.722156	44.338471
3501.684224	574236.575747	44.343476
3501.958811	574219.374025	44.348481
3501.917647	574216.721325	44.353485
3501.808643	574191.802882	44.358490
3501.861013	574167.009674	44.363495
3501.598022	574172.569692	44.368500
3501.834410	574154.972468	44.373505
3501.605991	574131.527553	44.378509
3501.639195	574116.269956	44.383514
3501.906408	574105.089893	44.388519
3501.663562	574094.792315	44.393524
3501.751858	574071.448282	44.398529
3501.712430	574067.942341	44.403533
3501.915951	574051.504063	44.408538
3501.709307	574042.103885	44.413543
3501.888096	574028.880490	44.418548
3501.894209	574001.485169	44.423553
3501.891266	573987.838581	44.428557
3501.787732	573972.050265	44.433562
3502.045597	573956.004737	44.438567
3501.814360	573953.030476	44.443572
3501.867587	573933.504793	44.448577
3502.153745	573915.849244	44.453581
3501.715667	573896.350129	44.458586
3501.902447	573879.362312	44.463591
3501.433063	573880.589652	44.468596
3501.657164	573857.023253	44.473601
3501.948517	573840.320071	44.478605
3502.069226	573829.814896	44.483610
3501.968285	573794.006640	44.488615
3501.955443	573796.667831	44.493620
3501.713158	573770.414605	44.498625
3501.789936	573758.762233	44.503629
3501.612606	573736.111294	44.508634
3501.734924	573729.368826	44.513639
3501.629285	573709.064806	44.518644
3501.376154	573694.905061	44.523649
3501.263679	573696.126799	44.528653
3501.817154	573695.337810	44.533658
3501.857569	573662.166271	44.538663
3501.819188	573667.039156	44.543668
3501.803226	573646.269435	44.548673
3502.020135	573626.617286	44.553677
3501.696787	573608.906020	44.558682
3501.892991	573592.267523	44.563687
3502.002309	573584.473333	44.568692
3502.133487	573566.991994	44.573697
3501.862044	573551.931787	44.578701
3501.823461	573541.501422	44.583706
3502.178649	573515.806477	44.588711
3501.772278	573503.577098	44.593716
3501.727290	573491.993663	44.598721
3502.261184	573473.646423	44.603725
3501.834247	573467.641941	44.608730
3501.687007	573438.914502	44.613735
3501.570760	573422.374776	44.618740
3501.609184	573412.383833	44.623745
3501.518849	573410.340735	44.628749
3501.679299	573384.926814	44.633754
3501.916813	573378.166129	44.638759
3502.145712	573367.693789	44.643764
3501.804943	573339.447934	44.648769
3501.687721	573331.839512	44.653773
3501.851344	573316.660803	44.658778
3501.747888	573291.990393	44.663783
3502.079311	573291.135740	44.668788
3501.651381	573252.215802	44.673793
3501.653868	573248.652879	44.678797
3501.748686	573241.061425	44.683802
3501.764945	573218.680246	44.688807
3501.751947	573203.328291	44.693812
3502.044941	573184.215422	44.698817
3502.285257	573166.616053	44.703821
3502.254859	573153.775578	44.708826
3502.304662	573133.245520	44.713831
3502.065344	573115.018578	44.718836
3501.823231	573085.803309	44.723841
3501.686313	573077.445142	44.728845
3501.588475	573074.700680	44.733850
3501.861511	573038.781398	44.738855
3501.835264	573034.219357	44.743860
3501.755957	573017.974330	44.748865
3501.747018	572996.248955	44.753869
3501.787669	572987.913140	44.758874
3501.881777	572972.142710	44.763879
3501.344934	572961.689350	44.768884
3501.718446	572944.721122	44.773889
3501.488926	572939.187270	44.778893
3501.846542	572930.450620	44.783898
3501.692823	572900.719279	44.788903
3501.425964	572907.033183	44.793908
3501.730486	572897.150721	44.798913
3501.177862	572878.119355	44.803917
3501.317889	572873.481079	44.808922
3501.593590	572870.627994	44.813927
3501.225379	572875.452424	44.818932
3501.134391	572859.008283	44.823937
3501.227857	572841.029944	44.828941
3501.501273	572831.403177	44.833946
3501.709308	572814.661337	44.838951
3501.368331	572821.739546	44.843956
3501.366299	572815.869003	44.848961
3501.826242	572804.055395	44.853965
3501.681975	572781.598093	44.858970
3501.722330	572776.473577	44.863975
3501.112730	572757.952699	44.868980
3501.021119	572745.372223	44.873985
3501.741810	572737.381520	44.878989
3501.243274	572732.341228	44.883994
3501.887358	572731.839085	44.888999
3501.617268	572727.164506	44.894004
3501.572127	572704.541020	44.899009
3501.560007	572707.503424	44.904013
3501.488825	572692.460946	44.909018
3501.753404	572662.111624	44.914023
3501.615126	572658.219270	44.919028
3501.625595	572645.672904	44.924033
3501.611861	572626.556871	44.929037
3501.662080	572624.391301	44.934042
3501.672724	572611.493617	44.939047
3501.639022	572599.154821	44.944052
3502.068047	572579.367345	44.949057
3501.925927	572571.812484	44.954061
3501.604445	572544.264141	44.959066
3501.917535	572529.462450	44.964071
3501.802548	572528.727709	44.969076
3502.078388	572513.379848	44.974081
3501.945288	572484.296527	44.979085
3501.916042	572477.878088	44.984090
3501.782755	572457.024175	44.989095
3501.589564	572447.771107	44.994100
3501.658109	572429.896373	44.999105
3501.987856	572430.647675	45.004109
3501.560429	572410.793075	45.009114
3501.779339	572388.880380	45.014119
3501.584269	572374.659728	45.019124
3501.274260	572358.198922	45.024129
3501.840933	572358.060128	45.029133
3501.444874	572338.300858	45.034138
3501.396645	572314.874196	45.039143
3501.724487	572310.708133	45.044148
3501.639033	572302.391530	45.049153
3502.087441	572287.468010	45.054157
3501.529579	572277.167843	45.059162
3501.534384	572269.840715	45.064167
3501.914057	572264.110938	45.069172
3501.837549	572245.756786	45.074177
3501.991152	572245.381483	45.079181
3501.663590	572220.392515	45.084186
3502.200449	572198.730835	45.089191
3501.409977	572192.029790	45.094196
3501.298037	572166.003378	45.099201
3501.442925	572157.751022	45.104205
3501.435541	572157.350702	45.109210
3501.796640	572154.734995	45.114215
3501.158924	572137.472021	45.119220
3501.474656	572122.619209	45.124225
3501.267323	572111.109925	45.129229
3501.012881	572110.045690	45.134234
3501.762842	572102.852871	45.139239
3501.326982	572092.884732	45.144244
3501.743132	572071.793675	45.149249
3501.392799	572068.787352	45.154253
3501.585072	572065.244570	45.159258
3501.579944	572048.986561	45.164263
3501.338110	572034.923339	45.169268
3501.563991	572032.228379	45.174273
3501.521721	572024.808090	45.179277
3501.278819	572009.390101	45.184282
3501.720548	571989.499253	45.189287
3501.719679	571986.538640	45.194292
3501.834119	571975.480734	45.199297
3501.713096	571951.914160	45.204301
3501.324042	571952.175682	45.209306
3501.544046	571931.566666	45.214311
3501.399612	571934.750684	45.219316
3501.791033	571923.850156	45.224321
3501.451995	571905.235404	45.229325
3501.566067	571900.149152	45.234330
3501.990894	571894.863771	45.239335
3501.846670	571867.085346	45.244340
3501.611013	571858.992630	45.249345
3501.802408	571841.499227	45.254349
3501.720621	571817.123322	45.259354
3501.416484	571804.625211	45.264359
3501.585043	571801.387151	45.269364
3501.542635	571786.389159	45.274369
3502.053667	571771.003532	45.279373
3502.057418	571765.783918	45.284378
3502.032812	571743.105128	45.289383
3501.597399	571733.989711	45.294388
3501.348242	571721.482914	45.299393
3501.369473	571696.137170	45.304397
3501.416298	571691.161703	45.309402
3502.065915	571683.081016	45.314407
3501.700881	571664.971765	45.319412
3501.776793	571651.560960	45.324417
3502.091191	571641.123853	45.329421
3501.714529	571629.690737	45.334426
3501.639217	571608.073454	45.339431
3501.554376	571615.112367	45.344436
3501.919866	571588.006330	45.349441
3501.925926	571578.169386	45.354445
3501.273048	571565.926266	45.359450
3501.669428	571555.576632	45.364455
3501.786107	571538.295180	45.369460
3501.783366	571524.244132	45.374465
3501.868885	571520.416769	45.379469
3501.698888	571505.789640	45.384474
3502.090316	571488.766265	45.389479
3501.725831	571478.284587	45.394484
3501.441750	571439.637055	45.399489
3501.862244	571432.545510	45.404493
3501.771142	571428.544991	45.409498
3502.084291	571403.152961	45.414503
3501.418730	571399.693895	45.419508
3501.498996	571385.428963	45.424513
3501.770202	571368.875863	45.429517
3501.242271	571367.653571	45.434522
3501.414466	571350.162418	45.439527
3501.703688	571349.063302	45.444532
3501.944008	571334.070701	45.449537
3501.898291	571316.964855	45.454541
3501.185891	571313.814193	45.459546
3501.693568	571278.956748	45.464551
3501.637148	571275.402416	45.469556
3501.759290	571269.009815	45.474561
3501.647431	571245.440347	45.479565
3501.409622	571239.906961	45.484570
3501.717368	571231.427737	45.489575
3501.467304	571233.825501	45.494580
3501.814661	571212.442504	45.499585
3502.121397	571196.385452	45.504589
3501.489717	571190.612503	45.509594
3501.645848	571159.874657	45.514599
3501.970083	571156.812820	45.519604
3501.563291	571141.067977	45.524609
3501.404835	571112.085487	45.529613
3501.526889	571113.722505	45.534618
3501.564523	571101.822606	45.539623
3501.260169	571094.994724	45.544628
3501.662235	571088.106591	45.549633
3501.653668	571071.747355	45.554637
3501.862855	571061.426540	45.559642
3502.067751	571048.346163	45.564647
3501.640281	571026.833018	45.569652
3501.817475	571017.671442	45.574657
3501.986121	571010.769567	45.579661
3501.846631	570988.358167	45.584666
3501.826027	570969.892849	45.589671
3501.584805	570959.843099	45.594676
3501.581174	570939.718933	45.599681
3501.853965	570922.612890	45.604685
3501.681513	570915.513349	45.609690
3501.633170	570893.187886	45.614695
3501.821081	570900.987583	45.619700
3501.418117	570881.076300	45.624705
3501.491367	570866.008831	45.629709
3501.286711	570859.616903	45.634714
3501.996450	570856.946402	45.639719
3501.967061	570849.071654	45.644724
3501.439333	570827.373058	45.649729
3501.833201	570815.065863	45.654733
3501.511152	570809.595623	45.659738
3501.905606	570785.644933	45.664743
3502.070901	570781.955413	45.669748
3501.634232	570752.664195	45.674753
3501.460713	570744.209660	45.679757
3501.380635	570727.760737	45.684762
3501.766307	570717.010523	45.689767
3501.714439	570705.224578	45.694772
3501.852519	570689.644868	45.699777
3502.018818	570683.947662	45.704781
3501.679768	570661.867943	45.709786
3501.719475	570656.290888	45.714791
3501.497081	570645.234165	45.719796
3501.894405	570620.780806	45.724801
3501.435364	570601.329491	45.729805
3501.504003	570616.425263	45.734810
3501.679145	570593.913715	45.739815
3501.563894	570574.508985	45.744820
3501.752997	570545.019032	45.749825
3501.881703	570474.885922	45.754829
3501.132234	570369.606960	45.759834
3501.305296	570211.634480	45.764839
3500.969603	570024.026699	45.769844
3500.742665	569766.381927	45.774849
3500.155574	569470.741602	45.779853
3499.819303	569131.586297	45.784858
3499.656402	568736.274897	45.789863
3498.970064	568303.182605	45.794868
3498.005992	567828.702567	45.799873
3497.454343	567296.406081	45.804877
3496.526859	566740.045613	45.809882
3495.778852	566132.770456	45.814887
3494.900379	565481.901596	45.819892
3493.960660	564798.216770	45.824897
3492.585855	564054.551535	45.829901
3491.617772	563290.637311	45.834906
3490.401116	562465.440068	45.839911
3489.118569	561619.351018	45.844916
3487.798983	560738.296782	45.849921
3486.556517	559791.156750	45.854925
3484.990815	558833.491582	45.859930
3483.188929	557821.222473	45.864935
3482.131272	556791.616676	45.869940
3479.934117	555713.155244	45.874945
3478.185278	554614.122645	45.879949
3475.994785	553470.979816	45.884954
3474.515470	552304.143410	45.889959
3472.326931	551105.735489	45.894964
3470.492196	549877.692553	45.899969
3468.450638	548607.925789	45.904973
3466.042250	547314.601192	45.909978
3463.906408	545999.724204	45.914983
3461.660566	544652.785964	45.919988
3459.271870	543289.778108	45.924993
3457.038297	541900.135026	45.929997
3454.461211	540476.127869	45.935002
3452.218306	539037.264505	45.940007
3449.574797	537567.450733	45.945012
3446.945785	536080.956222	45.950017
3444.299848	534576.069478	45.955021
3441.841442	533055.622558	45.960026
3438.734924	531506.449351	45.965031
3436.039801	529953.703629	45.970036
3433.126207	528377.439817	45.975041
3430.646246	526776.641913	45.980045
3427.164400	525157.823233	45.985050
3424.081362	523520.457001	45.990055
3421.531459	521888.046847	45.995060
3418.205442	520234.495799	46.000065
3415.474902	518572.837579	46.005069
3412.053139	516888.654326	46.010074
3409.321387	515203.500452	46.015079
3405.772907	513497.445713	46.020084
3402.438505	511778.541476	46.025089
3399.478252	510059.770106	46.030093
3396.169670	508333.125856	46.035098
3392.837854	506588.568886	46.040103
3389.193580	504842.938394	46.045108
3386.192313	503085.541093	46.050113
3382.793036	501316.789195	46.055117
3379.447471	499543.674666	46.060122
3376.336289	497763.241734	46.065127
3372.871483	495972.552444	46.070132
3369.290052	494170.254902	46.075137
3365.799317	492362.877838	46.080141
3362.500456	490560.807553	46.085146
3358.529823	488740.496598	46.090151
3355.044192	486933.024257	46.095156
3351.231636	485117.812458	46.100161
3347.717023	483291.933150	46.105165
3344.428855	481471.058703	46.110170
3340.505070	479642.592991	46.115175
3336.740709	477826.777695	46.120180
3333.086770	475994.310697	46.125185
3329.947961	474169.186476	46.130189
3326.162327	472340.670766	46.135194
3322.456915	470500.105417	46.140199
3318.647512	468665.468141	46.145204
3314.945801	466823.985097	46.150209
3311.707204	464995.275045	46.155213
3307.901127	463151.936751	46.160218
3304.116540	461302.424535	46.165223
3300.368799	459477.041907	46.170228
3296.503613	457630.484605	46.175233
3292.622411	455777.812063	46.180237
3289.039016	453954.655572	46.185242
3284.916698	452111.350578	46.190247
3281.449768	450284.861704	46.195252
3277.405318	448457.061732	46.200257
3273.808905	446616.247477	46.205261
3269.675249	444786.876252	46.210266
3266.150266	442957.835288	46.215271
3262.232901	441134.651346	46.220276
3258.245515	439306.184606	46.225281
3254.598698	437491.316397	46.230285
3250.827651	435673.254678	46.235290
3246.930975	433852.202957	46.240295
3243.394970	432051.546444	46.245300
3239.021529	430242.493356	46.250305
3235.601040	428429.020039	46.255309
3231.712765	426639.022769	46.260314
3228.048315	424823.283474	46.265319
3224.049350	423027.660400	46.270324
3220.218549	421230.484394	46.275329
3216.725764	419423.972508	46.280333
3212.841469	417645.304554	46.285338
3209.184479	415848.701673	46.290343
3205.234316	414049.710341	46.295348
3201.321457	412264.307135	46.300353
3197.840032	410490.000520	46.305357
3194.152520	408700.312969	46.310362
3190.189101	406918.183913	46.315367
3186.337168	405137.163303	46.320372
3182.437471	403367.374981	46.325377
3178.760882	401582.749048	46.330381
3174.821253	399819.187417	46.335386
3171.151764	398052.099925	46.340391
3167.085466	396292.300845	46.345396
3163.130226	394544.028285	46.350401
3159.109032	392795.486089	46.355405
3155.132840	391046.861264	46.360410
3151.376728	389298.102379	46.365415
3147.927035	387562.880743	46.370420
3143.641070	385836.098375	46.375425
3140.104934	384095.598487	46.380429
3136.152573	382376.958362	46.385434
3132.202359	380643.779931	46.390439
3128.857390	378930.784291	46.395444
3124.863312	377221.283838	46.400449
3121.386963	375503.186103	46.405453
3117.583964	373795.063284	46.410458
3113.813327	372075.524896	46.415463
3109.887564	370370.383765	46.420468
3106.089656	368672.689408	46.425473
3102.357903	366976.966276	46.430477
3098.089830	365284.885435	46.435482
3094.607759	363595.174765	46.440487
3091.060836	361908.223057	46.445492
3087.241214	360220.964191	46.450497
3083.128891	358538.612226	46.455501
3079.311086	356868.142706	46.460506
3075.609695	355187.906439	46.465511
3072.133946	353518.830146	46.470516
3068.367109	351860.158738	46.475521
3064.798181	350189.753652	46.480525
3060.908956	348527.269929	46.485530
3056.918422	346866.523325	46.490535
3053.373869	345205.370300	46.495540
3049.451073	343561.001261	46.500545
3046.168835	341903.053636	46.505549
3042.408434	340258.934724	46.510554
3038.579908	338613.732933	46.515559
3034.422650	336969.931259	46.520564
3030.250787	335331.194830	46.525569
3026.848124	333693.893182	46.530573
3022.815393	332071.471813	46.535578
3018.809270	330444.780539	46.540583
3015.336163	328833.148046	46.545588
3012.077956	327214.827817	46.550593
3008.466464	325598.328793	46.555597
3004.445469	323978.649611	46.560602
3000.821329	322367.799547	46.565607
2997.066430	320767.160642	46.570612
2993.335478	319151.879933	46.575617
2989.465500	317552.920359	46.580621
2985.541230	315951.367029	46.585626
2982.168398	314361.756419	46.590631
2978.824691	312761.907950	46.595636
2974.894430	311172.020211	46.600641
2971.350754	309578.303496	46.605645
2967.309223	307997.310499	46.610650
2963.713386	306405.610494	46.615655
2960.145510	304820.803349	46.620660
2956.498014	303234.458089	46.625665
2952.533611	301660.941487	46.630669
2948.849097	300082.015338	46.635674
2945.187429	298516.733215	46.640679
2941.484438	296943.803086	46.645684
2937.380007	295377.102951	46.650689
2934.002374	293815.821463	46.655693
2930.372260	292268.182389	46.660698
2926.287313	290701.381504	46.665703
2923.063282	289157.851862	46.670708
2918.905028	287602.364414	46.675713
2915.478147	286043.874363	46.680717
2912.071750	284499.372331	46.685722
2908.037665	282951.853317	46.690727
2904.079977	281415.261404	46.695732
2900.673083	279880.969523	46.700737
2896.896232	278330.969538	46.705741
2893.234484	276794.465422	46.710746
2889.373942	275271.329724	46.715751
2885.981962	273731.363957	46.720756
2882.220641	272209.302218	46.725761
2878.599052	270681.895739	46.730765
2874.676246	269171.850716	46.735770
2871.000278	267650.080284	46.740775
2867.385281	266125.678938	46.745780
2864.006213	264623.498605	46.750785
2860.437672	263103.042556	46.755789
2856.758782	261603.463558	46.760794
2853.074935	260095.716411	46.765799
2849.122232	258590.258328	46.770804
2845.496693	257081.903838	46.775809
2841.869373	255580.764267	46.780813
2838.092843	254088.697331	46.785818
2834.159528	252586.095949	46.790823
2830.760081	251095.747416	46.795828
2827.028831	249611.039480	46.800833
2823.434679	248133.122197	46.805837
2819.527897	246647.754063	46.810842
2816.225281	245161.745031	46.815847
2812.635876	243676.585036	46.820852
2808.644676	242205.001493	46.825857
2804.938324	240730.690211	46.830861
2801.301339	239260.383829	46.835866
2797.544367	237784.230997	46.840871
2794.240887	236313.960195	46.845876
2790.339749	234866.596996	46.850881
2787.000048	233386.515431	46.855885
2783.067097	231936.219013	46.860890
2779.554734	230473.246199	46.865895
2775.666137	229015.448731	46.870900
2772.277663	227564.040190	46.875905
2768.720876	226112.198302	46.880909
2764.966591	224665.302353	46.885914
2761.143586	223220.454941	46.890919
2757.851286	221770.278910	46.895924
2754.037120	220330.704947	46.900929
2749.992222	218887.858568	46.905933
2746.386361	217456.127566	46.910938
2742.765747	216017.577108	46.915943
2739.269702	214576.846967	46.920948
2735.543295	213152.101589	46.925953
2732.143687	211709.126568	46.930957
2728.284058	210298.320503	46.935962
2724.791793	208862.861916	46.940967
2721.581388	207435.568194	46.945972
2717.762967	206017.597797	46.950977
2714.253758	204588.713741	46.955981
2710.583371	203168.702420	46.960986
2706.671901	201740.157169	46.965991
2703.454942	200318.060052	46.970996
2699.707324	198901.864689	46.976001
2696.063313	197488.874819	46.981005
2692.458847	196090.790150	46.986010
2688.922817	194671.546309	46.991015
2685.449134	193245.915816	46.996020
2681.857239	191839.699013	47.001025
2678.369014	190431.317578	47.006029
2674.409683	189015.871032	47.011034
2670.550761	187605.672236	47.016039
2667.134333	186205.353606	47.021044
2663.519463	184801.647079	47.026049
2660.039102	183394.883351	47.031053
2656.215394	182012.256339	47.036058
2652.430256	180613.474567	47.041063
2648.800979	179210.615765	47.046068
2644.787545	177831.060605	47.051073
2641.761250	176437.623809	47.056077
2637.795375	175046.686841	47.061082
2634.250290	173664.593619	47.066087
2630.937335	172286.498185	47.071092
2627.194621	170902.244160	47.076097
2623.556704	169520.468770	47.081101
2619.680844	168145.821471	47.086106
2616.026294	166778.561622	47.091111
2613.134747	165397.283675	47.096116
2608.898078	164029.265515	47.101121
2605.495383	162648.543782	47.106125
2601.582897	161289.874347	47.111130
2597.990403	159925.265275	47.116135
2594.627545	158560.000937	47.121140
2590.775443	157200.061745	47.126145
2587.027281	155838.202583	47.131149
2583.249852	154476.888573	47.136154
2579.722503	153127.835837	47.141159
2576.248609	151777.088836	47.146164
2572.436815	150433.808479	47.151169
2569.108597	149084.606344	47.156173
2565.168340	147743.372599	47.161178
2562.025371	146353.006683	47.166183
2558.379539	144971.053140	47.171188
2554.417089	143629.611336	47.176193
2550.984393	142287.028390	47.181197
2547.193505	140967.414909	47.186202
2543.783140	139623.896540	47.191207
2540.409811	138288.921765	47.196212
2536.255145	136961.320772	47.201217
2532.972307	135635.784280	47.206221
2529.404269	134313.142460	47.211226
2525.455072	132988.322130	47.216231
2522.360344	131663.713126	47.221236
2518.805281	130351.631589	47.226241
2514.841536	129021.731360	47.231245
2511.215145	127697.302280	47.236250
2507.757294	126385.709854	47.241255
2503.890942	125068.995544	47.246260
2500.190965	123769.887482	47.251265
2496.733674	122454.199062	47.256269
2493.261154	121144.394063	47.261274
2489.215927	119833.832238	47.266279
2486.081160	118531.781679	47.271284
2482.115021	117241.299407	47.276289
2478.796847	115929.333553	47.281293
2474.958915	114635.741877	47.286298
2471.259897	113336.960721	47.291303
2467.908001	112048.661112	47.296308
2463.694578	110763.873471	47.301313
2460.415568	109484.567342	47.306317
2457.124170	108200.682042	47.311322
2453.212200	106913.508733	47.316327
2449.916996	105631.905889	47.321332
2446.413599	104349.532152	47.326337
2443.034646	103063.514199	47.331341
2438.979731	101790.095469	47.336346
2435.304414	100511.556985	47.341351
2431.775432	99235.905391	47.346356
2428.262654	97965.309090	47.351361
2424.693204	96698.915195	47.356365
2420.827914	95433.634889	47.361370
2417.427922	94166.096289	47.366375
2413.106754	92899.109341	47.371380
2409.213057	91637.863885	47.376385
2406.318354	90385.929681	47.381389
2402.458257	89146.726236	47.386394
2398.882932	87885.892765	47.391399
2395.643155	86635.846686	47.396404
2391.814190	85395.181876	47.401409
2388.248724	84150.679615	47.406413
2384.658833	82900.988592	47.411418
2380.788541	81662.421796	47.416423
2377.356796	80423.294398	47.421428
2373.237887	79202.746068	47.426433
2369.891388	77967.334087	47.431437
2366.206706	76748.070618	47.436442
2362.336109	75518.819781	47.441447
2359.094788	74293.348589	47.446452
2355.283285	73078.498600	47.451457
2351.873025	71856.492232	47.456461
2348.155318	70637.790061	47.461466
2344.389776	69436.895532	47.466471
2340.915357	68228.367741	47.471476
2337.141395	67023.847154	47.476481
2333.506481	65821.030738	47.481485
2329.733493	64622.285099	47.486490
2326.264908	63425.281395	47.491495
2322.554324	62234.287659	47.496500
2318.692959	61042.460632	47.501505
2315.207954	59865.779971	47.506509
2311.647820	58681.730415	47.511514
2307.861239	57504.277807	47.516519
2304.327655	56314.704940	47.521524
2300.515006	55145.525025	47.526529
2296.763199	53980.104404	47.531533
2293.180997	52805.915382	47.536538
2289.481992	51649.223244	47.541543
2286.210247	50483.323559	47.546548
2282.290576	49330.124208	47.551553
2278.472052	48174.613579	47.556557
2274.969788	47035.532532	47.561562
2270.960841	45892.852279	47.566567
2267.791826	44750.212585	47.571572
2263.415013	43613.857155	47.576577
2260.083645	42481.188128	47.581581
2256.445106	41344.199115	47.586586
2252.347132	40237.927546	47.591591
2248.854599	39109.565838	47.596596
2245.354575	37997.208708	47.601601
2241.536319	36896.648797	47.606605
2237.963245	35785.558371	47.611610
2233.788041	34688.660675	47.616615
2230.273584	33591.095093	47.621620
2226.307272	32507.468372	47.626625
2222.171698	31422.884664	47.631629
2218.751194	30358.443459	47.636634
2215.026903	29290.422411	47.641639
2211.182423	28222.507131	47.646644
2206.883255	27176.478595	47.651649
2202.948290	26122.260177	47.656653
2199.377899	25081.592156	47.661658
2194.925845	24060.800631	47.666663
2190.937957	23046.285713	47.671668
2186.208061	22064.411780	47.676673
2182.091486	21080.273241	47.681677
2176.346360	20150.705411	47.686682
2171.035365	19235.542718	47.691687
2165.899621	18355.674848	47.696692
2160.552822	17496.280099	47.701697
2155.557158	16667.309407	47.706701
2150.629589	15871.763990	47.711706
2145.945558	15110.844122	47.716711
2141.080144	14364.740776	47.721716
2136.212474	13654.156253	47.726721
2131.760452	12952.654543	47.731725
2127.137036	12294.493203	47.736730
2122.742953	11658.131344	47.741735
2118.373090	11046.286614	47.746740
2114.235277	10457.689579	47.751745
2109.553593	9886.201273	47.756749
2104.262708	9345.647502	47.761754
2099.437838	8838.471972	47.766759
2094.788714	8352.838182	47.771764
2090.359322	7889.937192	47.776769
2085.341376	7460.056953	47.781773
2080.913818	7052.373032	47.786778
2077.028333	6661.261049	47.791783
2072.860018	6300.439143	47.796788
2068.760921	5937.296828	47.801793
2064.504766	5609.650879	47.806797
2060.856191	5289.102839	47.811802
2057.164798	4979.007400	47.816807
2053.472152	4673.721330	47.821812
2049.939790	4377.858389	47.826817
2046.507219	4090.750380	47.831821
2043.470249	3825.910404	47.836826
2039.530212	3537.624752	47.841831
2036.325422	3256.737718	47.846836
2032.446889	3000.686573	47.851841
2029.592829	2733.179074	47.856845
2025.948474	2486.876231	47.861850
2022.712567	2227.555434	47.866855
2019.634224	1967.001844	47.871860
2015.903820	1721.343113	47.876865
2012.701597	1466.831134	47.881869
2009.657475	1222.546300	47.886874
2005.399532	976.360169	47.891879
2001.869536	731.607525	47.896884
1997.842966	511.168221	47.901889
1994.176678	290.434814	47.906893
1989.161739	107.903212	47.911898
1976.444694	134.153351	47.916903
1967.299383	143.705918	47.921908
1961.679564	156.288295	47.926913
1959.063152	154.128646	47.931917
1956.955580	151.582484	47.936922
1954.739254	152.413332	47.941927
1953.104842	145.563086	47.946932
1950.362224	147.245100	47.951937
1947.382142	151.463703	47.956941
1944.897479	141.427645	47.961946
1941.233825	158.323127	47.966951
1937.760478	148.198161	47.971956
1934.665195	142.630074	47.976961
1931.304696	143.674771	47.981965
1927.943913	144.096237	47.986970
1924.458351	158.844088	47.991975
1920.960958	150.213057	47.996980
1918.091156	144.084495	48.001985
1914.343960	148.173202	48.006989
1911.510600	146.341752	48.011994
1908.213309	150.189212	48.016999
1904.414609	150.796275	48.022004
1900.928496	150.987419	48.027009
1897.827356	153.032442	48.032013
1894.594265	144.834640	48.037018
1890.870961	152.156217	48.042023
1887.975102	134.518562	48.047028
1883.984675	150.367334	48.052033
1880.357389	140.336090	48.057037
1877.337419	145.440496	48.062042
1873.490867	149.449849	48.067047
1870.261106	139.669622	48.072052
1866.839745	146.001132	48.077057
1863.555017	149.052517	48.082061
1860.314913	134.316192	48.087066
1857.114304	141.891345	48.092071
1853.808324	143.639396	48.097076
1850.256545	142.790442	48.102081
1846.603484	149.155053	48.107085
1843.117952	137.573513	48.112090
1839.771307	146.715474	48.117095
1836.135503	140.988393	48.122100
1832.395338	141.304740	48.127105
1828.958042	147.882369	48.132109
1825.717467	142.517395	48.137114
1822.379300	144.773541	48.142119
1818.871071	144.803654	48.147124
1815.433706	142.886415	48.152129
1811.783398	145.830506	48.157133
1808.363739	140.297406	48.162138
1805.012045	145.086737	48.167143
1801.638807	143.782742	48.172148
1798.016921	145.273355	48.177153
1794.754938	150.826953	48.182157
1791.317884	142.597834	48.187162
1787.766941	142.204362	48.192167
1784.597464	138.160249	48.197172
1780.911037	139.199049	48.202177
1776.912523	133.804009	48.207181
1773.787467	138.083305	48.212186
1770.188888	137.159443	48.217191
1766.713833	132.255141	48.222196
1763.106667	133.620073	48.227201
1759.832695	135.284046	48.232205
1756.860168	138.470103	48.237210
1753.024874	147.315226	48.242215
1749.566543	137.634095	48.247220
1746.036817	135.133373	48.252225
1742.298789	138.733470	48.257229
1739.115399	128.458815	48.262234
1734.828917	137.858614	48.267239
1732.278660	129.231309	48.272244
1728.734089	134.965189	48.277249
1725.204846	137.827083	48.282253
1721.870136	136.393697	48.287258
1717.863506	143.886215	48.292263
1714.478640	129.337133	48.297268
1711.169900	136.812180	48.302273
1707.515277	135.621859	48.307277
1704.627031	133.368780	48.312282
1700.235583	141.506835	48.317287
1696.893888	132.373800	48.322292
1693.643816	139.317641	48.327297
1690.505572	136.176690	48.332301
1686.834494	137.513684	48.337306
1683.524091	142.280767	48.342311
1680.041167	135.276948	48.347316
1676.263864	134.248210	48.352321
1672.728649	143.925935	48.357325
1669.351189	137.645949	48.362330
1665.307524	152.538142	48.367335
1662.199867	133.585942	48.372340
1658.914268	135.330862	48.377345
1655.774152	134.395401	48.382349
1652.021466	135.568005	48.387354
1648.017880	139.671612	48.392359
1645.226144	135.720292	48.397364
1641.155199	135.259556	48.402369
1637.302267	136.134635	48.407373
1634.088351	129.661388	48.412378
1631.070460	135.591283	48.417383
1627.834920	129.792152	48.422388
1624.147369	143.401051	48.427393
1620.662524	133.600737	48.432397
1617.400495	136.610673	48.437402
1613.121368	134.603783	48.442407
1609.840765	131.804687	48.447412
1606.491970	138.067960	48.452417
1602.815981	139.681004	48.457421
1599.659845	136.637798	48.462426
1596.003290	138.067465	48.467431
1592.487490	134.115589	48.472436
1588.754603	134.699809	48.477441
1584.992086	129.894354	48.482445
1581.822463	128.027044	48.487450
1578.264423	138.208246	48.492455
1575.150749	128.732683	48.497460
1571.859198	133.490517	48.502465
1568.319324	130.140381	48.507469
1564.721452	121.553713	48.512474
1561.041588	136.290902	48.517479
1557.333442	139.490905	48.522484
1553.532106	130.989868	48.527489
1550.523037	141.493288	48.532493
1547.806752	127.896355	48.537498
1543.543080	134.141483	48.542503
1540.158126	130.238752	48.547508
1536.617478	135.139991	48.552513
1532.648499	136.251577	48.557517
1529.040028	130.678535	48.562522
1525.829760	131.943459	48.567527
1522.488491	126.746223	48.572532
1519.332666	125.544341	48.577537
1516.112988	130.819298	48.582541
1512.446062	124.439150	48.587546
1508.743612	140.448580	48.592551
1504.852410	134.736299	48.597556
1501.108788	126.292694	48.602561
1498.109873	132.267108	48.607565
1494.771359	125.914658	48.612570
1490.823753	138.134244	48.617575
1487.649517	131.987040	48.622580
1483.664393	131.449659	48.627585
1480.435184	131.002772	48.632589
1477.507806	134.371664	48.637594
1473.483092	132.252246	48.642599
1470.207315	123.820850	48.647604
1466.715276	135.352189	48.652609
1463.063779	136.999414	48.657613
1459.750468	127.567801	48.662618
1455.949824	138.992423	48.667623
1452.558854	122.818220	48.672628
1449.142799	128.437151	48.677633
1445.390661	130.429172	48.682637
1442.228334	129.063813	48.687642
1438.514887	135.067828	48.692647
1435.334713	133.354081	48.697652
1431.398075	129.373226	48.702657
1427.725194	133.184697	48.707661
1424.853876	127.787384	48.712666
1420.932897	130.868884	48.717671
1417.782892	135.392630	48.722676
1414.405100	124.335438	48.727681
1410.582993	132.897012	48.732685
1407.373448	128.653656	48.737690
1403.435431	132.389576	48.742695
1400.087305	122.887508	48.747700
1396.660998	123.575672	48.752705
1392.860487	128.011420	48.757709
1389.536933	122.355874	48.762714
1386.194275	134.303620	48.767719
1382.590198	130.710499	48.772724
1378.880171	128.152714	48.777729
1375.497088	133.279279	48.782733
1372.240104	125.781469	48.787738
1368.468935	127.665762	48.792743
1364.986735	132.045367	48.797748
1361.858395	136.379072	48.802753
1357.981767	137.732538	48.807757
1354.725096	127.580244	48.812762
1351.219107	131.254882	48.817767
1347.744551	126.540494	48.822772
1344.354391	133.481041	48.827777
1340.403977	134.241776	48.832781
1337.289001	118.207930	48.837786
1333.639215	132.700012	48.842791
1330.088840	119.755768	48.847796
1326.611015	122.733128	48.852801
1322.939453	133.277021	48.857805
1320.102695	131.155208	48.862810
1316.043794	132.435981	48.867815
1312.432158	125.734044	48.872820
1309.232407	126.987897	48.877825
1305.674275	127.820116	48.882829
1301.989368	124.834479	48.887834
1298.273105	131.212308	48.892839
1294.936850	130.753765	48.897844
1291.575500	130.561748	48.902849
1288.144428	137.524536	48.907853
1284.590384	124.017726	48.912858
1280.695567	128.031670	48.917863
1277.326924	125.214836	48.922868
1274.029046	131.489211	48.927873
1270.396113	129.631258	48.932877
1266.976007	129.173195	48.937882
1263.230441	135.495512	48.942887
1260.054956	122.967183	48.947892
1256.988992	130.391686	48.952897
1253.049685	133.026856	48.957901
1249.623908	125.954159	48.962906
1246.133871	138.855173	48.967911
1242.851287	128.488678	48.972916
1239.174001	134.958504	48.977921
1235.491503	134.740849	48.982925
1232.240564	126.963732	48.987930
1228.655976	135.975409	48.992935
1224.930829	130.465051	48.997940
1221.613370	125.862164	49.002945
1218.005640	132.384382	49.007949
1214.365329	133.492096	49.012954
1210.725246	128.237353	49.017959
1207.430712	127.829257	49.022964
1204.358025	125.282499	49.027969
1200.230112	133.411115	49.032973
1197.210207	116.910026	49.037978
1193.559052	129.244637	49.042983
1189.632745	125.584980	49.047988
1186.829267	129.165509	49.052993
1182.956913	133.815063	49.057997
1179.884524	118.916757	49.063002
1176.163080	132.793662	49.068007
1172.450889	127.869768	49.073012
1168.883059	132.202728	49.078017
1165.396284	126.269095	49.083021
1162.377584	123.486105	49.088026
1158.397627	128.772618	49.093031
1154.967155	120.068172	49.098036
1151.315116	130.520469	49.103041
1147.767400	128.124030	49.108045
1144.702541	133.283103	49.113050
1141.014352	131.073176	49.118055
1137.634159	129.280112	49.123060
1134.416599	125.550647	49.128065
1130.518540	125.436385	49.133069
1127.416453	122.834144	49.138074
1123.376366	135.992147	49.143079
1119.718218	127.481547	49.148084
1116.372124	127.151159	49.153089
1112.844517	126.700491	49.158093
1109.609942	123.318555	49.163098
1106.158036	125.962895	49.168103
1102.184042	131.017538	49.173108
1099.025318	124.928166	49.178113
1095.590733	121.299135	49.183117
1092.304040	124.471280	49.188122
1088.490843	125.587124	49.193127
1085.392515	127.960975	49.198132
1081.621331	131.911343	49.203137
1077.926369	128.319919	49.208141
1074.536648	123.570211	49.213146
1070.596972	129.302874	49.218151
1067.299014	128.246783	49.223156
1063.682183	123.146653	49.228161
1060.444002	127.263518	49.233165
1057.136798	128.230549	49.238170
1053.270068	126.172001	49.243175
1050.170773	125.100630	49.248180
1046.621618	126.554807	49.253185
1042.844693	129.224746	49.258189
1039.767099	119.962055	49.263194
1036.130560	120.809812	49.268199
1032.294796	123.096654	49.273204
1028.808488	126.122900	49.278209
1025.077774	131.797552	49.283213
1021.887272	112.004427	49.288218
1018.521560	130.900414	49.293223
1014.926735	123.598015	49.298228
1011.408902	123.949461	49.303233
1007.801709	126.134086	49.308237
1004.445186	120.661025	49.313242
1000.659730	124.749699	49.318247
997.692588	123.698784	49.323252
994.093856	129.264196	49.328257
990.051278	119.583131	49.333261
986.765464	117.120439	49.338266
983.344206	132.443709	49.343271
980.310004	123.917740	49.348276
976.719103	117.456317	49.353281
973.031544	121.861871	49.358285
969.288508	115.497041	49.363290
965.773625	123.605683	49.368295
961.941200	124.917579	49.373300
959.074279	115.315048	49.378305
955.729696	123.764029	49.383309
952.453156	115.503813	49.388314
948.296515	125.949753	49.393319
944.569677	121.265538	49.398324
941.246558	134.627714	49.403329
937.228225	125.948967	49.408333
934.318026	119.229116	49.413338
931.150495	127.425752	49.418343
927.382141	118.157371	49.423348
923.977618	117.529311	49.428353
920.421418	115.150110	49.433357
916.983658	120.105036	49.438362
913.116805	120.678849	49.443367
909.983781	126.392832	49.448372
906.117009	114.593013	49.453377
902.749609	117.496276	49.458381
899.395606	115.670726	49.463386
895.283049	118.921628	49.468391
892.086343	116.539932	49.473396
889.075259	116.198297	49.478401
885.234799	114.135708	49.483405
881.926879	113.271072	49.488410
878.330888	120.952671	49.493415
874.645798	115.005923	49.498420
871.554551	117.992507	49.503425
867.885483	126.732771	49.508429
864.437053	121.264668	49.513434
860.658836	118.315970	49.518439
857.616158	120.140166	49.523444
853.861623	112.692007	49.528449
850.251897	123.463633	49.533453
846.646320	113.157388	49.538458
843.553989	116.169460	49.543463
839.672437	115.850250	49.548468
836.430777	110.488990	49.553473
832.392361	110.912528	49.558477
829.330835	109.984018	49.563482
825.603289	119.761684	49.568487
822.469261	121.192066	49.573492
819.085116	118.238626	49.578497
815.048026	120.155276	49.583501
811.562167	113.927419	49.588506
808.029859	119.830505	49.593511
804.503831	118.031929	49.598516
801.353192	113.336645	49.603521
798.231976	117.871876	49.608525
794.402240	114.206766	49.613530
790.717621	111.714848	49.618535
787.610261	117.263491	49.623540
783.787660	122.541320	49.628545
779.825794	118.264147	49.633549
776.688697	107.916214	49.638554
773.291381	112.643386	49.643559
769.910122	106.022678	49.648564
766.292288	111.531040	49.653569
762.513423	122.208953	49.658573
759.286702	109.486396	49.663578
755.719260	106.862248	49.668583
752.190441	114.653590	49.673588
749.076561	109.285010	49.678593
745.054970	109.497141	49.683597
741.674660	109.896754	49.688602
737.891462	115.766384	49.693607
734.633457	111.578328	49.698612
731.282611	112.973090	49.703617
727.725016	110.584694	49.708621
724.272359	93.272082	49.713626
720.628146	108.045006	49.718631
717.223378	103.576218	49.723636
713.568096	105.480574	49.728641
710.219797	106.577547	49.733645
707.075983	99.179357	49.738650
702.879230	109.119121	49.743655
699.383814	105.088484	49.748660
695.798344	113.369611	49.753665
692.715125	110.802536	49.758669
689.273100	111.502902	49.763674
685.802137	108.066397	49.768679
682.293003	108.856370	49.773684
678.658270	109.862168	49.778689
675.058220	107.208358	49.783693
671.900080	103.998119	49.788698
668.039920	110.382869	49.793703
664.526401	99.290337	49.798708
661.452038	111.155099	49.803713
657.734840	105.457093	49.808717
653.928842	109.400410	49.813722
650.818381	103.509309	49.818727
646.947680	105.358841	49.823732
643.639230	99.729708	49.828737
640.020101	116.090117	49.833741
636.556444	95.900221	49.838746
633.089886	102.485933	49.843751
629.731656	92.852920	49.848756
626.287094	102.538864	49.853761
622.486548	105.601806	49.858765
619.098297	102.212488	49.863770
615.805200	114.953088	49.868775
612.261348	110.509287	49.873780
608.473404	107.176242	49.878785
604.630951	109.850280	49.883789
601.697737	106.038523	49.888794
597.869150	109.612072	49.893799
594.789242	105.842274	49.898804
591.266334	94.434873	49.903809
586.894492	105.759365	49.908813
583.597028	111.116373	49.913818
580.788556	107.709033	49.918823
577.315402	104.301391	49.923828
573.865266	99.675251	49.928833
570.228546	101.127497	49.933837
566.608385	100.321371	49.938842
563.005367	100.385766	49.943847
559.447110	104.736412	49.948852
556.151022	102.458993	49.953857
552.463007	109.614098	49.958861
548.985294	100.642079	49.963866
545.323306	110.795544	49.968871
541.700469	107.019050	49.973876
538.541140	105.302355	49.978881
534.766777	110.082330	49.983885
531.809207	104.002813	49.988890
528.027342	107.287495	49.993895
524.525958	111.293885	49.998900
520.880270	104.578657	50.003905
517.341333	111.767373	50.008909
514.054192	111.912029	50.013914
510.440129	104.843836	50.018919
506.712136	108.392174	50.023924
503.845146	105.648930	50.028929
500.302597	113.157761	50.033933
496.462645	108.823663	50.038938
492.813254	107.120465	50.043943
489.139135	109.261978	50.048948
485.827572	99.700812	50.053953
481.955715	114.427202	50.058957
479.102065	109.138192	50.063962
475.608929	108.698188	50.068967
472.118772	113.164751	50.073972
468.809429	112.196085	50.078977
465.126306	114.990758	50.083981
461.568316	111.612269	50.088986
458.206231	103.527023	50.093991
454.078801	112.529035	50.098996
450.780924	106.202291	50.104001
447.239489	110.177016	50.109005
444.309038	105.108860	50.114010
440.426183	106.321296	50.119015
436.869142	113.753323	50.124020
433.626197	107.433800	50.129025
429.722610	103.723476	50.134029
426.441093	102.858037	50.139034
422.634457	97.696174	50.144039
419.458268	103.046892	50.149044
416.435262	102.071361	50.154049
412.444887	110.529896	50.159053
408.631189	105.223610	50.164058
405.232653	113.035784	50.169063
401.804801	110.469012	50.174068
398.229975	111.724967	50.179073
394.755954	111.149122	50.184077
391.478551	98.934561	50.189082
387.755725	116.209792	50.194087
384.175928	104.520328	50.199092
380.525539	104.494139	50.204097
377.201744	106.334047	50.209101
374.124069	104.598294	50.214106
370.316435	105.618642	50.219111
366.814539	113.706449	50.224116
363.248154	110.949418	50.229121
360.110731	111.314290	50.234125
356.724235	106.178395	50.239130
353.022965	106.773961	50.244135
349.310669	106.599293	50.249140
345.853954	101.053620	50.254145
342.234186	105.603805	50.259149
338.939952	103.708997	50.264154
335.449431	103.907724	50.269159
331.443847	111.324624	50.274164
328.445660	111.936618	50.279169
324.491294	106.478398	50.284173
321.392372	105.337620	50.289178
317.558890	112.474465	50.294183
314.167236	105.399998	50.299188
310.956646	112.053290	50.304193
307.173088	104.511865	50.309197
304.095764	101.067642	50.314202
300.658753	102.352667	50.319207
296.731066	113.541261	50.324212
292.996907	112.677173	50.329217
289.795326	109.306203	50.334221
286.375839	97.718233	50.339226
282.819452	109.880057	50.344231
278.885727	105.760070	50.349236
276.272804	99.531750	50.354241
271.844718	113.813822	50.359245
268.524275	109.009304	50.364250
265.015985	106.508973	50.369255
261.759610	99.302608	50.374260
258.493728	100.709539	50.379265
254.710518	109.746290	50.384269
251.392590	106.077183	50.389274
247.971913	99.510335	50.394279
244.041254	112.119948	50.399284
241.325074	106.344416	50.404289
237.016566	121.158271	50.409293
233.822283	111.471272	50.414298
230.081516	109.083305	50.419303
226.625733	108.703988	50.424308
223.419016	109.858053	50.429313
219.745328	107.336195	50.434317
216.121016	100.358333	50.439322
212.857528	108.807475	50.444327
209.050650	108.407236	50.449332
205.628663	97.376522	50.454337
201.848700	104.125370	50.459341
198.680677	106.988149	50.464346
195.403604	105.021106	50.469351
191.747569	103.426646	50.474356
188.339107	102.843777	50.479361
184.304840	114.928638	50.484365
180.959581	108.289890	50.489370
177.787737	110.900173	50.494375
174.102688	115.463814	50.499380
170.749195	102.486151	50.504385
166.707513	110.620620	50.509389
163.445330	100.327360	50.514394
160.196772	102.987632	50.519399
156.440397	101.427890	50.524404
153.263366	102.352701	50.529409
150.102272	111.171802	50.534413
146.412506	96.636475	50.539418
142.512750	101.727311	50.544423
138.870400	110.780001	50.549428
135.237592	103.031546	50.554433
132.257127	103.634501	50.559437
128.664150	106.298123	50.564442
125.335282	110.179552	50.569447
121.514688	110.214937	50.574452
118.053426	107.523802	50.579457
114.177274	110.494388	50.584461
111.076736	112.236139	50.589466
107.868300	107.581822	50.594471
104.302062	108.048768	50.599476
101.012994	104.979483	50.604481
96.987453	107.112934	50.609485
93.336865	100.278453	50.614490
89.808575	105.121287	50.619495
86.497883	104.213091	50.624500
83.248023	100.492261	50.629505
79.756661	101.292338	50.634509
76.084990	101.484747	50.639514
72.547233	104.677580	50.644519
68.835211	102.478174	50.649524
65.414368	93.064040	50.654529
61.960595	108.054084	50.659533
58.781587	108.115528	50.664538
55.300754	99.245473	50.669543
51.649940	108.160311	50.674548
47.861475	100.648260	50.679553
44.330120	97.857408	50.684557
41.173879	91.752265	50.689562
37.634094	106.069251	50.694567
33.832871	102.555051	50.699572
30.194345	98.850847	50.704577
26.829911	104.199545	50.709581
23.513384	106.199794	50.714586
20.258294	103.283408	50.719591
16.598440	108.896697	50.724596
13.316203	111.660375	50.729601
9.463612	109.647535	50.734605
6.047810	106.835428	50.739610
2.414105	111.894130	50.744615