Thu Aug 25 12:29:24 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.551019	97.165359	0.000000
0.867379	102.396129	0.005005
0.488404	106.995523	0.010010
0.373001	100.992931	0.015014
0.397238	102.368534	0.020019
-0.456189	88.777786	0.025024
-0.078871	79.638631	0.030029
-0.226060	73.365780	0.035034
-0.146469	60.441956	0.040038
-0.945503	50.977761	0.045043
-1.177757	49.868862	0.050048
-0.884508	49.468568	0.055053
-1.882101	29.854494	0.060058
-1.878583	26.604752	0.065062
-2.136800	16.151004	0.070067
-2.540350	11.209157	0.075072
-2.755439	2.340032	0.080077
-3.020187	3.235723	0.085082
-3.444690	-4.357231	0.090086
-3.491494	-5.941273	0.095091
-4.135418	-1.240283	0.100096
-4.060547	-9.009553	0.105101
-4.798390	-3.711717	0.110106
-4.827008	-11.031337	0.115110
-4.960846	-5.008725	0.120115
-5.505983	-6.128708	0.125120
-6.194098	-11.152512	0.130125
-6.295193	-2.702101	0.135130
-6.077602	-8.408816	0.140134
-6.667220	-6.683940	0.145139
-6.867268	-4.706890	0.150144
-6.652562	-8.287109	0.155149
-7.456380	-11.128774	0.160154
-7.815081	-12.768351	0.165158
-7.831705	-4.011635	0.170163
-8.317359	2.100904	0.175168
-7.960712	-1.289583	0.180173
-8.005815	0.153824	0.185178
-8.414910	-6.096944	0.190182
-9.154171	3.355131	0.195187
-9.572012	-4.681792	0.200192
-9.508954	-6.396943	0.205197
-9.101970	-2.063092	0.210202
-9.728817	-4.486396	0.215206
-10.252255	-3.132557	0.220211
-11.276073	-2.117933	0.225216
-11.008802	3.775396	0.230221
-11.078057	1.252071	0.235226
-11.039104	-7.096868	0.240230
-11.026721	-7.937209	0.245235
-11.664316	2.577777	0.250240
-12.161402	-10.628963	0.255245
-12.626346	-9.923368	0.260250
-12.691781	-11.944252	0.265254
-12.686802	-3.975534	0.270259
-12.860542	-8.114985	0.275264
-12.694090	-5.176630	0.280269
-13.576006	-4.943542	0.285274
-14.239819	-0.672869	0.290278
-14.137039	-8.785035	0.295283
-14.442598	-5.712612	0.300288
-14.214475	-10.864156	0.305293
-14.736646	-1.310056	0.310298
-14.941370	-1.103978	0.315302
-15.215959	0.014718	0.320307
-15.732240	-1.562204	0.325312
-15.641938	-3.357554	0.330317
-15.657913	-2.538807	0.335322
-16.364588	-9.144745	0.340326
-16.464123	-14.729003	0.345331
-16.990131	-4.127101	0.350336
-16.783837	-17.042246	0.355341
-17.045553	-8.031996	0.360346
-17.364395	-8.162378	0.365350
-18.232376	-5.979434	0.370355
-18.637347	-10.582528	0.375360
-18.393372	-13.816155	0.380365
-18.542250	-5.329784	0.385370
-18.374245	2.205269	0.390374
-18.497129	-7.019983	0.395379
-18.961041	-5.991847	0.400384
-19.333074	-11.343585	0.405389
-19.764463	-0.164883	0.410394
-20.204770	-7.138424	0.415398
-19.754009	-7.930393	0.420403
-20.602903	-4.484936	0.425408
-20.881516	-14.154020	0.430413
-21.448819	4.512445	0.435418
-21.301456	-13.297294	0.440422
-21.244874	-8.494092	0.445427
-21.659961	-5.705065	0.450432
-21.986684	-14.265623	0.455437
-22.660195	-6.177942	0.460442
-22.703694	-13.931827	0.465446
-22.574802	-6.583639	0.470451
-22.680214	-10.689503	0.475456
-22.600531	-10.746286	0.480461
-23.809585	-1.154165	0.485466
-24.243693	-11.937839	0.490470
-24.089490	-16.868991	0.495475
-24.307530	-11.861409	0.500480
-24.682235	-2.422164	0.505485
-24.348757	-10.304720	0.510490
-24.834566	-10.652549	0.515494
-25.078612	-15.540285	0.520499
-25.345396	0.200072	0.525504
-25.594647	-10.982726	0.530509
-26.338819	-1.001537	0.535514
-27.048240	-5.034909	0.540518
-27.043570	-10.803175	0.545523
-26.476256	-9.525327	0.550528
-26.739204	-13.878590	0.555533
-26.948033	-1.152882	0.560538
-27.143083	-3.131312	0.565542
-27.644643	-8.165362	0.570547
-27.915901	-11.745367	0.575552
-28.181460	-11.729073	0.580557
-28.562036	-5.313461	0.585562
-28.463895	-7.802902	0.590566
-29.029672	-9.495453	0.595571
-29.876146	-7.594289	0.600576
-30.193954	-6.965531	0.605581
-29.868702	-8.911589	0.610586
-29.428622	-15.162527	0.615590
-29.825742	-6.070950	0.620595
-30.303721	-6.843950	0.625600
-30.648139	-8.688244	0.630605
-31.039721	-14.739271	0.635610
-31.326398	-3.750925	0.640614
-31.199713	-16.419477	0.645619
-31.920965	-6.394426	0.650624
-32.196470	-16.677763	0.655629
-32.470499	-10.633188	0.660634
-32.701811	-10.122386	0.665638
-32.555554	-20.380056	0.670643
-33.020833	-6.911818	0.675648
-33.468623	-19.420754	0.680653
-33.927424	-23.401641	0.685658
-34.059966	-15.218392	0.690662
-33.473746	-16.664337	0.695667
-33.841979	-8.567542	0.700672
-34.313640	-8.246872	0.705677
-35.108509	4.877547	0.710682
-35.439841	-2.559159	0.715686
-34.898465	-6.434171	0.720691
-35.775860	-12.254054	0.725696
-35.391215	-13.693726	0.730701
-36.159982	-12.924706	0.735706
-36.834084	-14.907168	0.740710
-36.793159	-17.144033	0.745715
-37.228523	-10.147199	0.750720
-37.077965	-14.663328	0.755725
-37.327130	-7.138846	0.760730
-37.254779	-10.108300	0.765734
-37.032045	-12.247102	0.770739
-37.747135	-5.076722	0.775744
-37.979313	-12.247386	0.780749
-38.482541	-7.891144	0.785754
-39.217678	-16.950855	0.790758
-39.785362	-15.194613	0.795763
-39.531805	-3.373426	0.800768
-39.028045	-7.865804	0.805773
-39.756116	-13.702756	0.810778
-39.922849	-11.458844	0.815782
-39.931307	-17.316799	0.820787
-40.653105	-6.991105	0.825792
-40.999957	-20.850959	0.830797
-41.678734	-8.095916	0.835802
-41.560346	-13.394780	0.840806
-41.986453	-14.394206	0.845811
-41.913188	-4.844820	0.850816
-41.841165	-11.231079	0.855821
-42.175677	-15.709169	0.860826
-42.497261	-9.843804	0.865830
-42.820019	-16.408650	0.870835
-43.201353	-10.562397	0.875840
-43.113880	-17.862236	0.880845
-43.310527	-10.187797	0.885850
-43.973042	-9.378478	0.890854
-44.504118	-10.769581	0.895859
-45.212244	-2.692293	0.900864
-44.180191	-15.964613	0.905869
-44.478516	-14.415091	0.910874
-44.651762	-5.561072	0.915878
-44.547817	-13.249473	0.920883
-45.781168	-5.978906	0.925888
-46.001874	-14.011907	0.930893
-46.153319	-2.491093	0.935898
-46.691999	-4.940864	0.940902
-46.364482	-10.614182	0.945907
-46.707792	-5.833743	0.950912
-47.112512	-10.604554	0.955917
-47.498045	-15.618814	0.960922
-48.008406	-2.516833	0.965926
-47.584459	-8.711462	0.970931
-47.613440	-6.723252	0.975936
-48.119165	-17.884839	0.980941
-48.975804	-13.691523	0.985946
-49.310602	-15.644890	0.990950
-49.258593	-11.353502	0.995955
-49.313140	-8.136912	1.000960
-49.303553	-14.314070	1.005965
-49.548320	-9.770536	1.010970
-50.047351	-13.963419	1.015974
-50.600346	-11.747570	1.020979
-50.734663	-10.274366	1.025984
-50.484315	-21.408885	1.030989
-50.791893	-13.112789	1.035994
-51.676710	-11.654869	1.040998
-51.783835	-8.445860	1.046003
-52.048107	-6.224629	1.051008
-52.352706	-6.879261	1.056013
-52.364903	-6.330026	1.061018
-52.501700	-8.032844	1.066022
-52.479341	-10.624305	1.071027
-53.188942	-8.535777	1.076032
-53.452406	-15.423125	1.081037
-53.816647	-11.164592	1.086042
-53.761955	-12.239352	1.091046
-53.773036	-4.926181	1.096051
-54.188438	0.561581	1.101056
-54.498472	-8.064867	1.106061
-55.099788	-16.917753	1.111066
-55.555501	-11.547064	1.116070
-55.368712	-6.308684	1.121075
-55.902916	-10.802940	1.126080
-55.747743	-13.440521	1.131085
-55.739213	-9.363782	1.136090
-56.364884	-10.834975	1.141094
-56.691999	-16.991013	1.146099
-57.102048	-10.846032	1.151104
-56.979373	-9.315018	1.156109
-57.076563	5.512915	1.161114
-57.167032	-2.524678	1.166118
-57.920857	-10.047039	1.171123
-58.301765	-9.490651	1.176128
-58.421033	-14.758604	1.181133
-58.436861	2.264879	1.186138
-58.569503	-8.594502	1.191142
-59.095508	-5.696346	1.196147
-59.830229	-5.578065	1.201152
-59.495785	-11.015186	1.206157
-59.884639	-2.269752	1.211162
-59.761132	-4.336060	1.216166
-60.628183	-7.057081	1.221171
-61.091693	-5.557605	1.226176
-61.271070	-5.614926	1.231181
-61.137774	-9.055837	1.236186
-61.488313	-15.037362	1.241190
-61.531914	-9.076348	1.246195
-61.583981	-11.241695	1.251200
-61.676832	-9.158056	1.256205
-62.319405	-8.054467	1.261210
-62.884571	-12.910867	1.266214
-62.852076	-2.795109	1.271219
-62.796660	4.099521	1.276224
-62.995945	-13.750809	1.281229
-63.869746	-12.582516	1.286234
-64.144550	-13.463279	1.291238
-64.052524	-9.541992	1.296243
-64.360433	-8.465531	1.301248
-64.184692	-11.989023	1.306253
-64.797753	-5.426252	1.311258
-65.605561	-0.013045	1.316262
-65.680849	-1.782449	1.321267
-65.983013	-0.839765	1.326272
-65.749247	-4.334385	1.331277
-66.244008	-2.630696	1.336282
-66.084913	-4.133104	1.341286
-66.343940	-11.293231	1.346291
-67.159604	1.492758	1.351296
-67.019492	-4.236619	1.356301
-67.396972	0.637761	1.361306
-67.595897	-7.430292	1.366310
-67.750059	-5.219986	1.371315
-67.796464	-8.427096	1.376320
-68.639764	-4.178919	1.381325
-69.129598	-3.320725	1.386330
-68.719972	6.182288	1.391334
-68.868688	-4.854910	1.396339
-69.132377	-9.533922	1.401344
-69.785972	-12.892664	1.406349
-70.188908	-2.499871	1.411354
-70.525668	-5.810183	1.416358
-70.181962	-9.891504	1.421363
-70.584357	-4.003984	1.426368
-70.219390	-9.059910	1.431373
-71.125099	0.095541	1.436378
-71.844756	-3.907749	1.441382
-71.841315	-3.148992	1.446387
-72.103546	-3.240786	1.451392
-71.860059	-0.064566	1.456397
-71.869873	-1.708188	1.461402
-72.830407	-7.957965	1.466406
-72.933809	-4.676773	1.471411
-73.197582	0.246229	1.476416
-73.161881	-12.759243	1.481421
-73.157888	-17.173311	1.486426
-73.803654	1.530751	1.491430
-74.181474	-5.310207	1.496435
-74.552482	2.280825	1.501440
-74.325012	-7.489701	1.506445
-74.932762	4.362042	1.511450
-75.359119	-7.340332	1.516454
-75.560739	-10.001101	1.521459
-76.379428	-7.148833	1.526464
-75.653404	-10.056195	1.531469
-75.844138	-0.436970	1.536474
-76.227975	-2.088424	1.541478
-76.340957	-6.841671	1.546483
-76.941388	-7.260123	1.551488
-77.167508	-8.888832	1.556493
-77.247868	-5.642888	1.561498
-77.855040	2.073734	1.566502
-77.729193	-6.836146	1.571507
-78.225713	-11.617879	1.576512
-78.659202	-8.398861	1.581517
-78.432171	-6.808269	1.586522
-78.925897	-3.253945	1.591526
-79.287527	-18.899001	1.596531
-79.655545	-3.990677	1.601536
-79.423710	-8.367681	1.606541
-80.029906	-2.375461	1.611546
-80.485070	-7.195313	1.616550
-80.610708	-4.192210	1.621555
-80.031806	-3.280014	1.626560
-80.696341	-6.314338	1.631565
-81.535934	0.698383	1.636570
-82.159465	-12.592934	1.641574
-81.788851	-8.854506	1.646579
-82.334120	-5.848926	1.651584
-81.786869	-5.675253	1.656589
-81.900497	2.647406	1.661594
-82.061965	-4.493207	1.666598
-82.948623	-6.559418	1.671603
-83.420535	4.141578	1.676608
-83.185663	-5.462429	1.681613
-83.561901	-11.360832	1.686618
-83.747111	-3.564798	1.691622
-84.486018	-6.021156	1.696627
-85.061888	-3.684661	1.701632
-84.993779	-15.553092	1.706637
-85.177185	-10.291509	1.711642
-85.030203	-12.440589	1.716646
-84.667524	-5.907321	1.721651
-85.461841	-7.393215	1.726656
-86.056393	-17.585425	1.731661
-86.339605	-11.438172	1.736666
-86.829850	-11.380342	1.741670
-86.581197	-11.292759	1.746675
-87.212236	-11.247670	1.751680
-86.663874	-17.180217	1.756685
-87.175886	-13.417385	1.761690
-87.705280	-9.151955	1.766694
-87.658269	-13.515816	1.771699
-87.676241	-5.480232	1.776704
-88.399070	-15.649179	1.781709
-89.281451	-7.794525	1.786714
-89.682421	-10.673994	1.791718
-89.529394	-18.708602	1.796723
-90.012368	-6.623319	1.801728
-89.480969	-7.769612	1.806733
-89.535544	-8.115406	1.811738
-89.737530	-11.298137	1.816742
-90.069774	-14.362380	1.821747
-90.758244	-5.003689	1.826752
-90.869209	-12.060463	1.831757
-91.156020	-16.476420	1.836762
-91.316879	-9.187241	1.841766
-91.663427	-10.404774	1.846771
-92.607330	-4.748780	1.851776
-92.281793	-12.614269	1.856781
-92.695241	-9.154781	1.861786
-92.750686	-1.549922	1.866790
-92.483367	-14.398694	1.871795
-92.805285	-9.624773	1.876800
-93.543133	-21.623175	1.881805
-93.651528	-11.972567	1.886810
-94.072302	-11.416258	1.891814
-94.117377	-20.052575	1.896819
-94.363026	-12.133180	1.901824
-94.751559	-22.949288	1.906829
-95.161051	-20.325654	1.911834
-95.542659	-10.939119	1.916838
-95.677284	-16.922834	1.921843
-95.610241	-11.675186	1.926848
-95.908696	-22.768000	1.931853
-96.274753	-14.073602	1.936858
-96.248932	-18.032345	1.941862
-96.797011	-17.247281	1.946867
-97.256816	-13.989338	1.951872
-97.255565	-13.347298	1.956877
-97.165916	-9.843256	1.961882
-97.547141	-11.922224	1.966886
-97.298333	-19.241012	1.971891
-98.285924	-7.522749	1.976896
-98.661853	-12.908670	1.981901
-98.680007	-7.505302	1.986906
-98.927431	-9.086381	1.991910
-99.085309	-15.025324	1.996915
-99.724216	-6.215800	2.006912
-99.027281	-6.581608	2.016909
-98.896398	-4.980210	2.026906
-98.264438	-11.322990	2.036902
-97.756444	-9.869382	2.046899
-97.691651	-13.950175	2.056896
-96.646130	-12.926084	2.066893
-96.240508	-12.124843	2.076890
-95.855544	-19.319070	2.086886
-95.026027	-14.662508	2.096883
-94.868168	-9.758149	2.106880
-94.215704	-13.988046	2.116877
-93.452653	-9.964133	2.126874
-93.323116	-11.451135	2.136870
-92.979892	-11.913573	2.146867
-91.797906	-8.889805	2.156864
-92.049998	-11.077282	2.166861
-91.130253	-18.526367	2.176858
-90.342779	-10.578203	2.186854
-90.509596	-6.424424	2.196851
-89.951940	-8.193920	2.206848
-89.553954	-0.453984	2.216845
-88.172134	-1.452964	2.226842
-87.972593	-0.565577	2.236838
-87.790702	-6.191603	2.246835
-87.503178	-8.232384	2.256832
-86.734268	1.923489	2.266829
-86.499072	-7.600957	2.276826
-85.537525	-9.617472	2.286822
-84.906382	-3.732391	2.296819
-84.840486	-3.578002	2.306816
-84.454144	-11.339486	2.316813
-83.832016	-6.286126	2.326810
-83.009259	-13.951266	2.336806
-81.932801	-5.595382	2.346803
-82.570929	-9.813124	2.356800
-82.068585	-5.767364	2.366797
-81.023291	-5.620718	2.376794
-80.728117	-5.144292	2.386790
-80.204135	-5.980344	2.396787
-79.329545	-4.704553	2.406784
-79.284631	-5.253296	2.416781
-79.106379	-2.512575	2.426778
-78.379938	-4.701325	2.436774
-77.718411	-12.363377	2.446771
-77.021650	-13.936090	2.456768
-76.760045	-12.139764	2.466765
-76.393839	-17.978400	2.476762
-75.448325	-3.481798	2.486758
-75.465743	-5.664866	2.496755
-74.359510	-9.813810	2.506752
-73.884205	-5.469206	2.516749
-73.800818	-8.551887	2.526746
-73.445207	-10.346745	2.536742
-72.387224	-14.253709	2.546739
-72.417591	-7.910182	2.556736
-71.849931	-12.212322	2.566733
-71.261223	-5.854924	2.576730
-70.592160	-13.743069	2.586726
-69.858138	-11.517086	2.596723
-69.360160	-11.965758	2.606720
-69.172071	-11.938220	2.616717
-68.892524	-11.481519	2.626714
-68.506989	-9.200931	2.636710
-67.503196	-13.609421	2.646707
-66.564253	-13.116657	2.656704
-66.440267	-12.686267	2.666701
-65.974043	-8.796405	2.676698
-66.248409	-14.110185	2.686694
-65.690655	-15.290483	2.696691
-64.447286	-18.250810	2.706688
-63.812889	-10.585933	2.716685
-63.615214	-14.921965	2.726682
-63.523548	-14.397812	2.736678
-62.466408	-18.868512	2.746675
-61.926560	-20.457818	2.756672
-62.065682	-17.702214	2.766669
-60.806945	-18.327109	2.776666
-60.550353	-20.613298	2.786662
-60.400422	-16.309580	2.796659
-59.653102	-18.511103	2.806656
-59.363826	-21.828782	2.816653
-58.391701	-21.566131	2.826650
-57.793643	-18.172098	2.836646
-57.736399	-22.353077	2.846643
-57.313436	-15.108067	2.856640
-56.512721	-4.624557	2.866637
-56.192175	-8.495169	2.876634
-55.672493	-7.673783	2.886630
-54.902851	-11.161765	2.896627
-54.634082	-14.197466	2.906624
-54.044934	-13.117701	2.916621
-53.664421	-9.312610	2.926618
-53.476480	-9.817240	2.936614
-52.489742	-11.698315	2.946611
-51.957845	-5.050078	2.956608
-51.902948	-3.462115	2.966605
-50.531987	-8.792947	2.976602
-50.429588	-3.984432	2.986598
-50.086811	-12.407498	2.996595
-49.950102	-12.739374	3.006592
-49.120867	-8.405876	3.016589
-48.911223	-15.205170	3.026586
-47.779617	-12.316053	3.036582
-47.643818	-14.684686	3.046579
-47.289783	-17.518335	3.056576
-46.546006	-9.743881	3.066573
-46.090832	-13.683103	3.076570
-45.902527	-15.328200	3.086566
-45.189059	-14.052503	3.096563
-44.628663	-19.538261	3.106560
-43.622545	-19.553366	3.116557
-43.197014	-12.232728	3.126554
-43.239687	-14.529048	3.136550
-42.912066	-11.273203	3.146547
-42.208424	-13.056067	3.156544
-41.783226	-8.066881	3.166541
-40.834245	-9.808991	3.176538
-40.293734	-8.097546	3.186534
-40.386118	-12.632052	3.196531
-39.684729	-10.106346	3.206528
-39.081467	-11.426821	3.216525
-38.628288	-4.905631	3.226522
-37.671590	-12.183109	3.236518
-37.564532	-14.106914	3.246515
-37.335492	-13.775347	3.256512
-36.116227	-16.202870	3.266509
-36.065572	-15.558250	3.276506
-35.868585	-13.530052	3.286502
-35.198674	-20.509167	3.296499
-34.665451	-15.128261	3.306496
-34.122365	-12.311655	3.316493
-32.894160	-9.843150	3.326490
-32.941832	-11.796564	3.336486
-32.490833	-5.176830	3.346483
-32.690806	-15.456720	3.356480
-31.633622	-16.243266	3.366477
-31.010596	-13.714785	3.376474
-30.081602	-15.485440	3.386470
-29.729441	-17.723247	3.396467
-29.840004	-17.224428	3.406464
-29.714134	-14.510344	3.416461
-29.020304	-12.230541	3.426458
-27.496536	-16.774352	3.436454
-27.411743	-14.909140	3.446451
-27.277073	-15.848915	3.456448
-26.042411	-16.983217	3.466445
-26.217965	-16.486886	3.476442
-25.805464	-19.491253	3.486438
-25.372679	-15.447263	3.496435
-24.657277	-15.096866	3.506432
-23.675320	-18.275989	3.516429
-23.238843	-14.739426	3.526426
-22.879167	-15.251956	3.536422
-22.589322	-11.233085	3.546419
-22.317708	-15.577535	3.556416
-21.335046	-12.633398	3.566413
-21.093685	-15.028075	3.576410
-20.449565	-17.511199	3.586406
-19.805644	-16.373490	3.596403
-19.535461	-11.629278	3.606400
-19.325497	-8.494379	3.616397
-18.451745	-7.129752	3.626394
-18.141191	-9.335699	3.636390
-17.409788	-16.698251	3.646387
-17.138359	-14.010141	3.656384
-16.527958	-13.377196	3.666381
-15.461026	-15.679479	3.676378
-15.547946	-16.365956	3.686374
-15.264054	-15.862418	3.696371
-14.886905	-13.966985	3.706368
-13.897151	-13.333289	3.716365
-13.546493	-8.646035	3.726362
-12.693950	-12.216696	3.736358
-12.546292	-16.158419	3.746355
-12.326357	-19.652135	3.756352
-11.362840	-13.065188	3.766349
-10.957075	-21.624832	3.776346
-10.731048	-15.631922	3.786342
-9.440234	-16.670482	3.796339
-9.225925	-18.341827	3.806336
-9.218429	-19.100118	3.816333
-8.822388	-17.641635	3.826330
-7.934731	-22.541938	3.836326
-7.479118	-15.590309	3.846323
-6.655843	-15.700306	3.856320
-6.564238	-6.204911	3.866317
-6.623558	-9.544001	3.876314
-5.610872	-9.427082	3.886310
-5.204768	-7.057846	3.896307
-4.684703	-1.792080	3.906304
-4.505470	1.702431	3.916301
-3.625150	18.594644	3.926298
-3.182616	26.840808	3.936294
-3.042563	34.475462	3.946291
-2.351336	51.805983	3.956288
-2.118021	58.044867	3.966285
-1.587978	85.629569	3.976282
-1.133141	99.525239	3.986278
-0.711874	117.924499	3.996275
0.000000	140.771496	4.001280
0.332832	141.551417	4.006285
0.296999	152.089266	4.011290
0.294361	143.370282	4.016294
0.588776	142.571166	4.021299
0.489981	144.915186	4.026304
0.828618	164.509235	4.031309
0.774900	170.538336	4.036314
1.044828	172.223466	4.041318
0.757638	171.929933	4.046323
0.911450	168.036514	4.051328
1.066872	167.778037	4.056333
0.710231	166.270999	4.061338
0.859121	149.511233	4.066342
0.693124	157.927597	4.071347
0.841834	168.306825	4.076352
1.234436	174.240687	4.081357
0.899007	174.014824	4.086362
0.986378	172.526803	4.091366
0.699475	169.303556	4.096371
0.824569	174.213134	4.101376
0.984111	167.427114	4.106381
1.082860	182.392182	4.111386
1.252657	170.308368	4.116390
0.876482	180.231999	4.121395
0.671406	171.895901	4.126400
0.804633	169.536981	4.131405
0.919420	183.917400	4.136410
1.005181	171.938502	4.141414
1.164098	177.118031	4.146419
1.050766	174.898983	4.151424
1.128810	179.211651	4.156429
0.688538	178.926284	4.161434
0.993846	185.050999	4.166438
0.820558	189.624513	4.171443
0.984693	180.082106	4.176448
1.174381	181.349534	4.181453
1.265232	175.472790	4.186458
1.099641	177.719711	4.191462
1.343108	184.123037	4.196467
1.043843	174.558325	4.201472
1.256352	163.606788	4.206477
0.875249	187.027919	4.211482
1.334861	173.990686	4.216486
1.077265	174.496118	4.221491
0.999773	183.939514	4.226496
1.513430	191.787491	4.231501
1.368210	204.497053	4.236506
1.532752	198.855532	4.241510
1.658614	185.731376	4.246515
1.328030	181.170359	4.251520
1.387816	172.723158	4.256525
1.222286	188.558551	4.261530
1.032602	181.574139	4.266534
1.329366	195.362900	4.271539
1.391663	203.316404	4.276544
1.750367	203.775895	4.281549
1.422194	192.678098	4.286554
1.244696	177.389987	4.291558
1.347100	183.973605	4.296563
1.627247	196.287480	4.301568
1.775668	200.604945	4.306573
1.343516	183.221168	4.311578
1.528182	184.464073	4.316582
1.587035	185.381837	4.321587
1.364648	172.888065	4.326592
1.549222	182.027805	4.331597
1.313937	194.257919	4.336602
1.597301	199.709026	4.341606
1.442004	201.293103	4.346611
1.533298	212.314113	4.351616
1.430983	216.341832	4.356621
1.440049	211.423866	4.361626
1.955700	196.220128	4.366630
1.861908	208.266729	4.371635
1.504493	202.520324	4.376640
1.789170	205.775553	4.381645
1.493050	213.484658	4.386650
1.823979	206.934365	4.391654
1.827423	201.691411	4.396659
1.634626	212.715803	4.401664
1.704559	201.970082	4.406669
1.518239	210.111241	4.411674
1.549916	210.533385	4.416678
1.855052	206.720653	4.421683
1.707179	206.525515	4.426688
1.814489	203.939695	4.431693
1.973726	205.692792	4.436698
1.809478	199.254889	4.441702
1.898488	203.274775	4.446707
1.794910	197.830290	4.451712
1.993785	209.005286	4.456717
1.619421	216.802583	4.461722
1.507746	200.343026	4.466726
2.148861	204.804762	4.471731
1.638676	203.796348	4.476736
2.106846	201.283703	4.481741
1.786027	210.613376	4.486746
1.790073	213.593033	4.491750
1.690003	213.988362	4.496755
1.776023	221.631269	4.501760
2.021555	216.407329	4.506765
2.055129	208.536865	4.511770
2.071089	202.684501	4.516774
2.065914	211.895115	4.521779
1.876200	209.254591	4.526784
1.784754	217.466310	4.531789
1.944561	217.222964	4.536794
1.761103	208.070366	4.541798
1.934475	214.547961	4.546803
2.060383	229.613218	4.551808
2.439962	227.532072	4.556813
2.067750	219.883372	4.561818
2.447495	206.972526	4.566822
2.121886	208.526340	4.571827
1.782805	213.030924	4.576832
2.292782	208.319217	4.581837
2.216214	217.841581	4.586842
2.014064	212.219543	4.591846
2.491313	218.333149	4.596851
2.081238	215.065916	4.601856
2.177250	218.793640	4.606861
2.361262	222.630964	4.611866
2.483426	213.262796	4.616870
2.093829	204.819550	4.621875
1.782106	208.598501	4.626880
2.158078	221.656690	4.631885
2.201257	229.926417	4.636890
2.206544	234.494110	4.641894
2.219830	231.850250	4.646899
2.170677	238.603169	4.651904
2.378843	238.054848	4.656909
2.343041	242.530904	4.661914
2.421409	234.197823	4.666918
2.201969	242.160685	4.671923
2.334209	241.133871	4.676928
2.497737	232.164179	4.681933
2.541746	235.988640	4.686938
2.315498	228.642938	4.691942
2.694655	238.334359	4.696947
2.301329	239.490655	4.701952
2.522395	231.780633	4.706957
2.529991	235.158376	4.711962
2.356791	236.552269	4.716966
2.316528	242.237596	4.721971
2.389424	250.205279	4.726976
2.596131	245.291139	4.731981
2.443433	239.531628	4.736986
2.508394	233.162205	4.741990
2.561661	232.182567	4.746995
2.478598	233.483243	4.752000
2.881274	236.628239	4.757005
2.430824	242.124730	4.762010
2.500136	236.048858	4.767014
2.584183	239.712021	4.772019
2.935799	247.281687	4.777024
2.919308	232.632701	4.782029
2.403202	237.462424	4.787034
2.642704	238.301266	4.792038
2.404250	240.584921	4.797043
2.738456	240.124421	4.802048
2.841740	241.092176	4.807053
2.318843	246.865778	4.812058
2.812684	244.219390	4.817062
2.915960	248.632527	4.822067
2.860330	243.057126	4.827072
3.015913	236.053398	4.832077
2.477199	238.751098	4.837082
2.691184	229.349553	4.842086
2.491874	242.042306	4.847091
2.577311	254.067184	4.852096
2.984095	247.925777	4.857101
2.875292	252.928972	4.862106
3.020409	254.216045	4.867110
3.516590	258.678356	4.872115
3.057708	256.181240	4.877120
2.722749	241.939654	4.882125
2.791618	233.323320	4.887130
2.614323	242.693798	4.892134
2.447254	249.822705	4.897139
2.590373	264.961227	4.902144
3.030124	262.943417	4.907149
2.679511	266.086220	4.912154
3.280126	266.925432	4.917158
3.127596	258.258352	4.922163
2.853009	261.677149	4.927168
3.265507	254.607850	4.932173
3.127773	266.053925	4.937178
3.069479	268.378959	4.942182
3.091062	263.066705	4.947187
3.071581	270.678706	4.952192
3.153758	265.227242	4.957197
3.083499	260.631744	4.962202
3.111098	264.281610	4.967206
3.113227	273.453146	4.972211
3.246179	272.290175	4.977216
3.539884	261.136028	4.982221
3.490783	266.500039	4.987226
3.036918	268.323894	4.992230
3.229536	265.664586	4.997235
3.395879	265.635354	5.002240
3.332846	260.940646	5.007245
2.954408	266.596707	5.012250
3.014733	265.429297	5.017254
3.228898	269.809246	5.022259
3.151017	272.314522	5.027264
3.458848	267.188376	5.032269
3.053189	275.224723	5.037274
3.201418	267.288812	5.042278
3.055246	267.972944	5.047283
2.962981	267.326160	5.052288
3.511304	259.628126	5.057293
3.180110	259.923626	5.062298
3.163320	267.725032	5.067302
3.123216	262.166176	5.072307
3.433240	273.434530	5.077312
3.124897	277.089577	5.082317
3.589796	286.055733	5.087322
3.517378	292.204865	5.092326
3.913538	291.247431	5.097331
3.001879	288.036627	5.102336
3.371159	276.990853	5.107341
3.839678	297.355651	5.112346
3.488374	288.378008	5.117350
3.586834	280.785253	5.122355
3.141348	273.777608	5.127360
3.383123	287.211218	5.132365
3.506671	295.000139	5.137370
3.636456	289.674089	5.142374
3.522122	290.742382	5.147379
3.289619	298.046080	5.152384
3.835775	298.542643	5.157389
3.480442	294.624565	5.162394
3.350018	294.448838	5.167398
3.622021	292.849620	5.172403
3.111689	290.841459	5.177408
3.304749	288.368743	5.182413
3.562478	294.320614	5.187418
3.345439	289.121671	5.192422
3.459743	299.544333	5.197427
3.925241	307.314485	5.202432
4.479274	296.344158	5.207437
3.968562	307.304522	5.212442
4.155065	302.308109	5.217446
3.665122	296.155323	5.222451
3.766470	296.496949	5.227456
3.869245	292.700086	5.232461
3.660009	298.247387	5.237466
3.691157	301.229140	5.242470
4.068100	293.712971	5.247475
3.792621	304.269475	5.252480
3.921317	293.622061	5.257485
3.883101	297.139874	5.262490
3.972810	299.122178	5.267494
3.520005	292.609227	5.272499
3.515469	294.543021	5.277504
3.865533	291.507857	5.282509
3.781887	297.829597	5.287514
3.716722	292.901092	5.292518
4.008972	309.297629	5.297523
3.999946	311.640260	5.302528
4.153050	302.953745	5.307533
3.920560	302.518759	5.312538
3.876242	296.387902	5.317542
4.063843	297.551260	5.322547
4.033361	312.596797	5.327552
4.168891	312.705273	5.332557
3.809331	313.596851	5.337562
4.033169	314.915887	5.342566
4.313536	319.301295	5.347571
4.046303	326.218132	5.352576
4.337299	326.697727	5.357581
3.841904	320.308500	5.362586
3.981004	308.349628	5.367590
4.099509	319.584743	5.372595
3.903236	315.916990	5.377600
4.143429	314.734050	5.382605
3.997441	317.835310	5.387610
3.994383	315.741338	5.392614
4.271593	322.582362	5.397619
4.317978	327.441038	5.402624
4.369314	317.254993	5.407629
4.421329	319.850658	5.412634
4.289277	325.718075	5.417638
4.290128	315.590562	5.422643
4.274766	320.107728	5.427648
4.521818	314.421604	5.432653
4.321782	322.992078	5.437658
4.277811	318.095048	5.442662
4.488772	317.530468	5.447667
4.325418	326.440052	5.452672
4.273296	322.205536	5.457677
4.293947	323.040706	5.462682
3.980662	330.578541	5.467686
4.081036	323.871336	5.472691
4.059307	326.766463	5.477696
4.242857	319.963969	5.482701
4.225178	329.970721	5.487706
4.105117	328.565809	5.492710
4.289572	316.954173	5.497715
4.150017	333.111497	5.502720
4.547033	337.301458	5.507725
4.513848	339.328333	5.512730
4.784439	334.983137	5.517734
4.786254	337.713223	5.522739
4.483517	324.795326	5.527744
4.432833	329.039613	5.532749
4.305422	324.766271	5.537754
4.845925	330.575770	5.542758
4.840687	327.485536	5.547763
4.459038	323.489315	5.552768
4.831679	318.795933	5.557773
4.673449	322.598316	5.562778
4.402738	319.116235	5.567782
4.563371	323.653283	5.572787
4.493823	330.703668	5.577792
4.844060	328.611288	5.582797
4.894652	337.269053	5.587802
4.613229	332.500974	5.592806
4.825379	327.203137	5.597811
4.268916	316.539672	5.602816
4.471652	327.068719	5.607821
4.352551	339.812251	5.612826
4.998799	328.884405	5.617830
5.421661	345.016896	5.622835
4.676924	343.675056	5.627840
5.015785	335.411847	5.632845
4.916888	351.240108	5.637850
5.008876	335.381280	5.642854
5.386191	322.413783	5.647859
4.499919	329.475070	5.652864
4.471229	325.296994	5.657869
4.451861	329.685074	5.662874
4.733016	332.706756	5.667878
4.795625	337.040863	5.672883
5.012646	336.570248	5.677888
4.724654	335.726332	5.682893
4.834456	343.587032	5.687898
4.604527	341.240696	5.692902
4.433529	345.725305	5.697907
4.589821	351.446310	5.702912
4.809957	336.389997	5.707917
4.523098	335.422515	5.712922
4.598213	351.381703	5.717926
5.202327	352.520934	5.722931
5.364748	365.052692	5.727936
5.502549	360.408750	5.732941
5.097980	348.902037	5.737946
4.736123	340.884659	5.742950
5.035927	349.889369	5.747955
5.024888	362.685590	5.752960
5.330521	362.390919	5.757965
5.045655	365.792363	5.762970
4.845399	359.591003	5.767974
5.263919	361.268690	5.772979
4.692391	367.233452	5.777984
5.002089	358.164863	5.782989
5.076943	366.290482	5.787994
5.033088	365.873396	5.792998
5.064872	356.228242	5.798003
4.650982	364.863881	5.803008
5.130601	355.537711	5.808013
5.164426	366.235619	5.813018
5.190387	369.306783	5.818022
5.350888	358.467681	5.823027
5.007507	367.918032	5.828032
5.290704	367.930604	5.833037
5.235519	365.322763	5.838042
5.520078	366.467770	5.843046
5.536889	374.127914	5.848051
5.293651	369.046951	5.853056
5.331858	361.552189	5.858061
5.312316	367.572837	5.863066
5.348708	360.065705	5.868070
5.552353	355.281731	5.873075
4.874750	371.574013	5.878080
5.202837	369.434479	5.883085
5.411539	384.958304	5.888090
5.471532	385.097599	5.893094
5.563585	381.536521	5.898099
5.505424	389.164124	5.903104
5.788088	388.101078	5.908109
5.707676	386.455826	5.913114
5.414941	389.096025	5.918118
5.594828	381.265837	5.923123
5.402351	380.501869	5.928128
5.729768	379.703901	5.933133
5.598017	388.178284	5.938138
5.525539	367.665896	5.943142
5.669686	373.895023	5.948147
5.102641	386.319621	5.953152
5.775146	379.873938	5.958157
5.722390	383.118793	5.963162
5.291029	394.130054	5.968166
5.734851	387.198167	5.973171
5.326988	400.059753	5.978176
5.424402	386.633015	5.983181
5.350631	403.628002	5.988186
5.813226	384.645312	5.993190
5.847917	386.326191	5.998195
5.516903	399.536412	6.003200
5.758450	390.079842	6.008205
5.779158	400.871577	6.013210
5.761962	394.701635	6.018214
5.818903	390.446850	6.023219
5.458102	397.027190	6.028224
5.612190	391.089846	6.033229
5.712750	391.937810	6.038234
5.324676	399.503211	6.043238
5.857855	394.898554	6.048243
5.888431	396.453526	6.053248
6.026481	390.882535	6.058253
5.843727	386.953215	6.063258
5.801830	389.478181	6.068262
5.736762	397.850370	6.073267
5.458307	396.141231	6.078272
5.842112	384.979218	6.083277
5.640992	391.645271	6.088282
5.773582	389.495235	6.093286
5.758231	391.418079	6.098291
5.628979	395.111530	6.103296
5.495997	388.693969	6.108301
5.839595	388.314254	6.113306
5.537843	380.923371	6.118310
5.762811	383.843131	6.123315
5.542098	388.772148	6.128320
5.745847	379.495517	6.133325
5.575422	389.260473	6.138330
5.533573	392.117634	6.143334
5.959205	379.572805	6.148339
5.362662	385.430759	6.153344
5.595960	386.473065	6.158349
5.867984	395.978872	6.163354
5.223430	392.662921	6.168358
5.586418	405.780229	6.173363
5.615399	414.166164	6.178368
5.719118	413.409571	6.183373
5.941887	423.084466	6.188378
6.035700	408.718617	6.193382
5.531891	392.794897	6.198387
5.569339	396.459066	6.203392
5.807560	404.154136	6.208397
5.788741	399.300600	6.213402
5.882824	398.536026	6.218406
5.981798	394.629003	6.223411
5.749507	393.577036	6.228416
5.795617	383.344315	6.233421
5.536387	390.108059	6.238426
5.440491	388.575967	6.243430
6.121436	393.319419	6.248435
5.665048	387.749816	6.253440
5.967882	384.484750	6.258445
5.715601	395.559704	6.263450
5.797329	384.581065	6.268454
6.116738	392.301376	6.273459
5.535635	395.986527	6.278464
5.746615	384.032161	6.283469
5.862901	393.065647	6.288474
5.765187	392.815190	6.293478
5.809563	384.765782	6.298483
5.636700	394.692478	6.303488
5.976761	383.818901	6.308493
5.772328	385.970690	6.313498
5.977444	388.956838	6.318502
6.374432	386.354079	6.323507
5.320664	395.026713	6.328512
6.035834	387.451183	6.333517
5.761108	388.354783	6.338522
5.559565	395.008248	6.343526
5.747646	391.144214	6.348531
5.247504	401.523999	6.353536
5.926800	390.496023	6.358541
5.852553	393.231707	6.363546
5.405235	393.304952	6.368550
5.373757	390.845256	6.373555
5.592785	398.574969	6.378560
5.842631	378.733419	6.383565
5.712250	397.110370	6.388570
5.871710	394.782113	6.393574
5.867098	384.655417	6.398579
5.401581	400.987264	6.403584
5.398542	394.998605	6.408589
5.458691	394.182399	6.413594
5.552490	394.841593	6.418598
5.801292	388.228170	6.423603
5.895235	390.956484	6.428608
5.708129	389.305802	6.433613
5.606094	399.623210	6.438618
5.597494	391.901646	6.443622
5.775979	383.448402	6.448627
5.578677	395.119033	6.453632
5.888897	391.650323	6.458637
5.684252	389.296856	6.463642
5.689742	387.672946	6.468646
5.953701	385.885151	6.473651
5.655302	392.569610	6.478656
5.687428	391.023786	6.483661
5.619244	394.274224	6.488666
5.697282	391.316468	6.493670
6.050807	393.795298	6.498675
5.720569	391.097668	6.503680
5.646349	378.994997	6.508685
5.727042	390.653707	6.513690
5.546610	383.367203	6.518694
6.093847	388.356235	6.523699
5.506465	393.890045	6.528704
5.581106	386.585721	6.533709
5.598055	389.041354	6.538714
5.469333	395.101266	6.543718
5.594362	393.933201	6.548723
5.586603	393.956558	6.553728
5.821467	394.223481	6.558733
5.695999	383.704424	6.563738
5.465649	392.912447	6.568742
5.458313	393.160369	6.573747
5.723103	408.134413	6.578752
6.046606	416.879173	6.583757
6.003719	414.955950	6.588762
5.657332	399.349253	6.593766
5.940051	387.465904	6.598771
5.594624	398.220089	6.603776
5.694785	392.155149	6.608781
5.715975	401.981841	6.613786
5.724020	397.608163	6.618790
5.749047	389.691500	6.623795
5.324160	398.680064	6.628800
5.600607	396.124664	6.633805
5.786324	412.199457	6.638810
5.525401	409.063847	6.643814
5.742421	415.882699	6.648819
5.789619	419.330204	6.653824
5.759803	416.974650	6.658829
5.924086	401.572684	6.663834
5.664877	394.795240	6.668838
5.529594	391.908872	6.673843
5.754614	403.079894	6.678848
5.802451	406.321647	6.683853
5.766027	405.827463	6.688858
5.856717	395.992721	6.693862
5.720943	408.871794	6.698867
5.545379	401.489605	6.703872
5.686837	394.886670	6.708877
5.682855	396.355306	6.713882
5.623876	401.119777	6.718886
5.776034	405.898626	6.723891
5.682275	414.234188	6.728896
5.859120	411.846255	6.733901
5.849076	407.440606	6.738906
5.283705	407.943646	6.743910
5.808188	405.735369	6.748915
6.106876	411.190468	6.753920
6.101785	403.306993	6.758925
6.092243	392.969088	6.763930
5.856705	390.696392	6.768934
5.720421	396.453761	6.773939
5.952331	396.417420	6.778944
5.985688	396.266652	6.783949
5.994164	402.599306	6.788954
5.969336	396.908297	6.793958
5.702523	396.554617	6.798963
5.691995	397.401004	6.803968
5.671462	389.978710	6.808973
5.960820	393.739453	6.813978
5.502841	394.352219	6.818982
6.108828	386.395154	6.823987
5.865484	400.164292	6.828992
5.863455	384.870658	6.833997
5.603922	380.883765	6.839002
5.807182	387.796513	6.844006
5.504871	376.166190	6.849011
5.598825	381.014264	6.854016
5.928646	386.549900	6.859021
5.681982	391.318465	6.864026
5.562588	393.292412	6.869030
5.785822	381.896126	6.874035
5.713831	395.973778	6.879040
5.936110	382.847026	6.884045
5.835635	369.906898	6.889050
5.479102	375.663967	6.894054
5.662678	385.522156	6.899059
5.812912	386.435104	6.904064
5.659634	386.544538	6.909069
5.427809	391.203208	6.914074
5.427571	392.253630	6.919078
5.778355	394.856280	6.924083
5.667699	397.562867	6.929088
5.658712	399.399291	6.934093
5.789408	395.253174	6.939098
5.551872	391.193228	6.944102
5.567443	388.906499	6.949107
5.713793	394.372806	6.954112
5.735795	396.150589	6.959117
5.608835	398.470579	6.964122
5.129048	402.636580	6.969126
5.484527	395.205991	6.974131
5.231611	407.122630	6.979136
5.453528	398.789128	6.984141
5.531720	410.309034	6.989146
5.379104	422.592792	6.994150
5.933016	422.157977	6.999155
5.777889	430.250055	7.004160
6.043002	420.153846	7.009165
5.773220	412.669353	7.014170
5.640576	410.503922	7.019174
5.844709	396.174584	7.024179
5.499324	403.847196	7.029184
5.645072	406.874287	7.034189
6.035749	412.394069	7.039194
5.580929	407.972684	7.044198
5.830557	403.779457	7.049203
5.315007	400.626794	7.054208
5.958778	411.371534	7.059213
5.884243	419.824312	7.064218
5.566334	407.680708	7.069222
5.905410	398.563202	7.074227
5.492154	393.072262	7.079232
5.699663	408.627934	7.084237
5.814720	428.902726	7.089242
5.649920	410.277745	7.094246
5.955618	409.211089	7.099251
5.634307	411.156562	7.104256
5.845978	400.391678	7.109261
5.766607	399.233491	7.114266
5.656989	411.007456	7.119270
5.861695	394.675323	7.124275
5.738214	403.964686	7.129280
5.839501	388.790905	7.134285
5.730817	403.409000	7.139290
6.247420	401.107044	7.144294
5.934393	391.411490	7.149299
5.887175	398.363487	7.154304
6.040733	392.843851	7.159309
5.800696	401.711702	7.164314
5.534807	401.867255	7.169318
5.897207	399.662228	7.174323
6.337925	404.297785	7.179328
6.053254	405.807236	7.184333
5.721846	388.309395	7.189338
5.536872	377.467463	7.194342
5.852989	370.558755	7.199347
5.739416	385.528786	7.204352
5.699020	383.336250	7.209357
5.538738	379.030079	7.214362
5.580047	395.969062	7.219366
5.980357	394.431991	7.224371
5.828067	395.351210	7.229376
5.664321	380.402465	7.234381
5.546206	373.818061	7.239386
5.721251	375.457966	7.244390
6.260212	382.859128	7.249395
5.347224	379.069534	7.254400
5.828931	370.926300	7.259405
5.562024	377.830450	7.264410
5.673423	379.926427	7.269414
5.769497	379.250129	7.274419
5.300669	382.278594	7.279424
5.754418	387.630294	7.284429
5.875825	399.491443	7.289434
5.990775	405.411936	7.294438
5.637789	386.506410	7.299443
5.538474	393.956961	7.304448
5.844579	398.502874	7.309453
5.732785	397.916094	7.314458
5.576150	393.599857	7.319462
5.702516	387.185955	7.324467
5.858430	399.876948	7.329472
5.684393	401.868950	7.334477
5.542850	397.575658	7.339482
5.738575	397.706341	7.344486
5.777538	401.768916	7.349491
5.495354	401.949168	7.354496
5.978786	399.570150	7.359501
5.827889	403.058181	7.364506
5.417951	396.503674	7.369510
5.641633	402.207808	7.374515
5.767325	399.071737	7.379520
5.740675	394.883834	7.384525
5.690148	393.885647	7.389530
5.867497	395.202482	7.394534
5.912705	391.702526	7.399539
5.744785	395.386217	7.404544
5.700181	384.683642	7.409549
5.804055	390.688125	7.414554
5.638270	392.245388	7.419558
5.674402	380.973332	7.424563
5.513985	393.647444	7.429568
5.783079	395.085948	7.434573
5.906105	398.781003	7.439578
5.616108	396.374466	7.444582
5.829026	390.399431	7.449587
5.764832	399.594078	7.454592
5.913612	381.562253	7.459597
5.581271	377.928461	7.464602
5.392134	381.840105	7.469606
6.036301	386.864570	7.474611
5.928147	387.352921	7.479616
5.775775	376.009160	7.484621
5.556747	378.640974	7.489626
5.208895	380.106536	7.494630
5.780959	387.717654	7.499635
5.900582	392.647133	7.504640
5.805151	391.899597	7.509645
5.744890	395.158286	7.514650
5.390673	393.714125	7.519654
5.763624	387.334356	7.524659
5.436419	398.066703	7.529664
5.902679	394.681114	7.534669
5.707774	398.770839	7.539674
5.512397	400.165056	7.544678
5.694081	399.453197	7.549683
5.675193	407.808664	7.554688
5.733851	396.691260	7.559693
5.482453	398.287248	7.564698
5.753410	406.284081	7.569702
5.729055	402.434346	7.574707
6.049347	416.744788	7.579712
5.828652	407.281538	7.584717
6.085057	402.818323	7.589722
5.784327	407.095478	7.594726
5.514377	391.375570	7.599731
5.608070	394.173528	7.604736
5.837541	393.229550	7.609741
6.044555	399.062849	7.614746
5.554580	388.252879	7.619750
5.587091	385.723045	7.624755
5.371496	399.484671	7.629760
5.581995	394.490800	7.634765
5.555960	394.428433	7.639770
5.777033	399.996932	7.644774
6.123310	395.117832	7.649779
5.620430	410.329218	7.654784
5.889749	396.106728	7.659789
5.682012	404.222856	7.664794
5.794215	402.566406	7.669798
5.756257	404.283981	7.674803
5.815641	397.285771	7.679808
5.962096	390.973127	7.684813
5.540020	384.483802	7.689818
5.429171	394.647561	7.694822
5.890327	391.613957	7.699827
5.544616	403.795076	7.704832
5.469718	394.976557	7.709837
5.366421	402.677679	7.714842
5.536867	405.587002	7.719846
5.799650	398.651838	7.724851
5.213104	405.299189	7.729856
5.375315	401.110168	7.734861
5.654474	403.844266	7.739866
5.713958	402.645341	7.744870
6.163926	398.420725	7.749875
5.845509	410.002772	7.754880
5.788857	409.043510	7.759885
5.889073	403.510082	7.764890
6.046892	404.893254	7.769894
5.876437	400.791157	7.774899
5.301703	415.093131	7.779904
5.648907	401.288715	7.784909
5.814173	396.134248	7.789914
5.951201	402.889696	7.794918
5.865924	404.760220	7.799923
5.814528	401.430427	7.804928
6.069358	399.688354	7.809933
5.791285	400.643100	7.814938
5.861695	399.872744	7.819942
5.478179	386.752318	7.824947
5.327365	399.073744	7.829952
6.171103	404.104911	7.834957
6.038795	404.268009	7.839962
5.516755	388.381951	7.844966
5.987450	384.483130	7.849971
5.678026	390.504911	7.854976
5.591043	383.361957	7.859981
5.720949	384.009165	7.864986
5.399725	387.065125	7.869990
5.988768	397.356513	7.874995
5.718168	399.433248	7.880000
5.834507	391.220697	7.885005
5.668211	395.084471	7.890010
5.524900	399.684981	7.895014
5.631759	397.576942	7.900019
5.777552	401.799953	7.905024
5.983450	402.580791	7.910029
5.941479	389.185382	7.915034
5.457434	384.082032	7.920038
5.513123	384.687083	7.925043
5.499922	397.736774	7.930048
5.077398	396.429868	7.935053
5.737107	395.222323	7.940058
5.553792	402.486717	7.945062
5.577371	398.537722	7.950067
5.652068	405.476948	7.955072
5.478137	407.041816	7.960077
5.364164	411.242253	7.965082
5.387196	405.173574	7.970086
5.757458	409.529100	7.975091
5.776087	405.410032	7.980096
5.821598	408.804014	7.985101
5.777336	407.273322	7.990106
5.688541	415.750479	7.995110
5.705131	409.069025	8.000115
5.777523	398.536948	8.005133
5.898284	404.416135	8.010150
5.792403	405.183790	8.015168
5.578840	403.551005	8.020186
5.661715	404.207036	8.025203
5.523488	400.211406	8.030221
5.544605	398.513450	8.035238
5.656369	409.348590	8.040256
5.734627	417.743271	8.045274
5.784008	414.223166	8.050291
5.550408	413.129998	8.055309
5.982035	409.748816	8.060326
5.746426	419.726375	8.065344
5.984945	426.656922	8.070362
6.497873	406.423857	8.075379
5.915346	403.517150	8.080397
5.401401	404.919934	8.085414
5.487889	400.699750	8.090432
5.867066	405.411843	8.095450
5.903934	403.837648	8.100467
5.762935	405.816306	8.105485
5.859187	403.011528	8.110502
5.770889	400.668005	8.115520
5.430161	402.479143	8.120538
6.204661	410.666904	8.125555
5.948549	409.933866	8.130573
5.859482	409.341909	8.135590
5.939003	413.927388	8.140608
5.477595	412.406017	8.145626
6.021216	398.741602	8.150643
5.975851	401.784545	8.155661
5.610507	401.964856	8.160678
5.771804	398.146357	8.165696
5.859256	418.070742	8.170714
5.975507	426.771895	8.175731
6.025547	429.840919	8.180749
6.121132	423.243014	8.185766
5.770206	406.553522	8.190784
5.543899	419.723253	8.195802
5.982967	415.138558	8.200819
6.384752	430.201172	8.205837
5.706593	417.889494	8.210854
5.733845	419.093875	8.215872
6.058155	422.628003	8.220890
6.204244	419.521928	8.225907
6.062810	411.683081	8.230925
5.617943	401.868937	8.235942
5.727575	417.823058	8.240960
5.691660	428.252165	8.245978
6.299814	422.078873	8.250995
6.177309	421.687813	8.256013
6.158822	434.657737	8.261030
6.220676	418.588360	8.266048
6.200502	416.126866	8.271066
6.139667	402.453015	8.276083
6.073505	403.066126	8.281101
5.965960	405.023763	8.286118
6.207152	405.541381	8.291136
5.714163	414.609379	8.296154
6.042800	405.857451	8.301171
5.889964	409.497893	8.306189
6.007215	401.025236	8.311206
6.303385	389.463466	8.316224
6.078704	409.424124	8.321242
6.180357	396.886138	8.326259
6.283157	403.639129	8.331277
6.345399	402.180878	8.336294
6.050999	399.591941	8.341312
5.755450	400.370378	8.346330
6.216312	399.427175	8.351347
6.047166	399.144407	8.356365
5.876078	401.888316	8.361382
5.848064	405.490266	8.366400
5.686065	408.649312	8.371418
5.790667	399.831505	8.376435
6.460185	410.692863	8.381453
6.441020	414.119861	8.386470
6.553926	402.798232	8.391488
6.318008	403.775607	8.396506
6.129137	400.841936	8.401523
6.066715	408.933612	8.406541
5.865957	404.556465	8.411558
5.789371	406.357775	8.416576
5.469721	410.248412	8.421594
6.028021	414.881950	8.426611
6.444526	428.070889	8.431629
6.282495	435.139937	8.436646
6.512118	425.245347	8.441664
5.987873	418.394270	8.446682
6.424200	403.052019	8.451699
6.255794	413.255727	8.456717
6.186793	414.418385	8.461734
6.236194	405.303115	8.466752
5.918619	415.725852	8.471770
6.037804	414.713108	8.476787
6.284343	416.290225	8.481805
6.509235	422.481302	8.486822
6.384542	411.720751	8.491840
6.301433	406.264834	8.496858
6.407516	400.681448	8.501875
6.428111	397.888525	8.506893
6.299033	404.232885	8.511910
6.153039	403.804480	8.516928
5.889497	414.297645	8.521946
5.964317	408.409890	8.526963
6.155991	422.268360	8.531981
6.172363	425.143845	8.536998
6.269412	424.166126	8.542016
6.367048	438.683118	8.547034
6.476000	432.704801	8.552051
6.605779	427.811962	8.557069
6.001242	415.924245	8.562087
6.481233	418.610326	8.567104
6.045017	432.952185	8.572122
6.381659	431.271060	8.577139
6.258238	435.702151	8.582157
6.143752	436.155579	8.587175
6.396171	433.881743	8.592192
6.066024	434.615110	8.597210
6.145153	427.590599	8.602227
6.333467	433.850526	8.607245
6.168400	434.169870	8.612263
6.505054	425.413520	8.617280
6.346886	440.570188	8.622298
6.512763	434.005447	8.627315
6.463910	435.903399	8.632333
6.123131	443.369681	8.637351
6.481087	433.893630	8.642368
6.127254	435.839367	8.647386
5.989004	438.515021	8.652403
5.531738	435.976843	8.657421
6.028585	453.672269	8.662439
6.366176	451.590210	8.667456
6.528110	463.168595	8.672474
6.591969	461.893121	8.677491
6.666102	461.442848	8.682509
6.237448	460.657947	8.687527
6.374344	458.629423	8.692544
6.459960	462.352434	8.697562
6.522441	462.765512	8.702579
6.734336	454.988050	8.707597
6.432585	458.339413	8.712615
6.564343	454.405610	8.717632
6.378941	459.064166	8.722650
6.426174	456.636286	8.727667
6.741676	455.135194	8.732685
6.545481	462.361082	8.737703
6.748031	457.459989	8.742720
6.566642	439.134461	8.747738
6.284987	434.990885	8.752755
6.446458	442.580442	8.757773
6.407511	452.019127	8.762791
6.902019	457.514729	8.767808
6.396691	440.609558	8.772826
6.433708	447.287666	8.777843
6.511721	457.241353	8.782861
6.810195	454.108241	8.787879
6.470457	450.301962	8.792896
6.860499	454.018299	8.797914
6.644001	445.430657	8.802931
6.923012	427.370672	8.807949
6.301953	438.267001	8.812967
6.188896	432.657981	8.817984
6.173247	446.362762	8.823002
6.597409	463.258554	8.828019
7.258915	453.179517	8.833037
6.569144	460.454337	8.838055
7.042589	452.727412	8.843072
6.879203	446.050156	8.848090
6.706874	444.224716	8.853107
6.535595	440.937992	8.858125
6.137638	444.367542	8.863143
6.382144	436.121080	8.868160
6.586612	450.037526	8.873178
6.784595	461.963708	8.878195
6.948216	454.783938	8.883213
6.664468	455.465855	8.888231
7.033710	451.415950	8.893248
6.681890	442.707503	8.898266
6.599819	436.030133	8.903283
6.551888	440.357880	8.908301
6.697554	453.485133	8.913319
7.229830	453.329148	8.918336
6.590576	439.922618	8.923354
6.637807	438.779137	8.928371
6.712643	430.937953	8.933389
6.323145	433.690842	8.938407
6.914234	444.769635	8.943424
6.719969	453.904456	8.948442
6.880430	454.538865	8.953459
7.073767	453.107407	8.958477
6.744809	450.605926	8.963495
6.610363	436.697433	8.968512
6.678430	436.838239	8.973530
6.576706	450.660651	8.978547
6.660724	449.672349	8.983565
7.044347	455.541925	8.988583
6.941781	452.881898	8.993600
6.743838	458.047342	8.998618
6.883744	450.852355	9.003635
7.218811	454.249105	9.008653
6.936078	442.427714	9.013671
6.960815	435.411721	9.018688
6.716093	430.060013	9.023706
6.443050	434.123232	9.028723
6.865836	440.734584	9.033741
7.009057	454.051566	9.038759
6.887201	445.736271	9.043776
6.890243	446.849775	9.048794
6.695205	451.118524	9.053811
7.126747	456.248454	9.058829
7.024667	456.037227	9.063847
7.038188	442.604157	9.068864
6.962154	436.033137	9.073882
6.601850	426.985205	9.078899
7.007277	432.627298	9.083917
7.066576	445.389385	9.088935
7.098768	427.737297	9.093952
6.925769	423.617724	9.098970
6.445059	434.410011	9.103987
6.940669	439.198543	9.109005
6.837699	455.085024	9.114023
6.961639	447.340279	9.119040
6.907084	447.178410	9.124058
6.869924	445.991347	9.129075
7.089691	446.834212	9.134093
7.099123	450.553378	9.139111
6.925019	458.687821	9.144128
6.964592	453.629229	9.149146
7.019122	460.755874	9.154163
7.026895	445.139910	9.159181
7.167697	457.097138	9.164199
6.814333	448.912787	9.169216
7.181054	445.204101	9.174234
6.914508	454.864638	9.179251
7.312175	446.108186	9.184269
7.119243	458.774104	9.189287
7.183430	445.304692	9.194304
6.951298	448.752441	9.199322
6.843323	460.972710	9.204339
6.879598	455.027864	9.209357
6.869371	455.966724	9.214375
7.010875	452.842427	9.219392
7.026982	447.058532	9.224410
7.032549	454.233870	9.229427
7.041070	449.732404	9.234445
7.086198	457.497985	9.239463
6.978735	462.283185	9.244480
7.080995	451.736357	9.249498
6.901306	453.304520	9.254515
7.118838	456.479848	9.259533
6.762691	455.358542	9.264551
6.467504	452.204838	9.269568
7.021435	457.675350	9.274586
6.418578	473.198362	9.279603
7.201183	469.888409	9.284621
7.222620	477.380002	9.289639
7.203773	471.409074	9.294656
7.241525	470.203960	9.299674
6.996769	476.673766	9.304691
7.325190	482.034454	9.309709
7.056835	478.002392	9.314727
7.203779	477.461816	9.319744
7.107719	477.177063	9.324762
6.758907	477.840774	9.329779
7.087674	472.465470	9.334797
6.969007	483.630246	9.339815
6.905968	477.783003	9.344832
7.440232	494.595302	9.349850
7.358661	514.271725	9.354867
7.627332	498.087822	9.359885
6.885523	491.469619	9.364903
6.878113	493.824983	9.369920
7.632034	498.948596	9.374938
7.539136	503.239223	9.379955
7.979744	488.104510	9.384973
7.624389	491.805102	9.389991
7.228001	477.347488	9.395008
7.678209	477.844983	9.400026
7.259814	485.386558	9.405043
7.020689	468.414406	9.410061
7.400314	478.219863	9.415079
7.190196	473.967240	9.420096
7.668424	473.346357	9.425114
7.212630	475.762505	9.430131
7.328134	466.725207	9.435149
7.254800	469.927176	9.440167
6.951335	468.797616	9.445184
7.387560	471.828229	9.450202
7.178272	476.815577	9.455219
7.408740	482.971088	9.460237
7.408591	488.970233	9.465255
7.342706	490.738317	9.470272
7.560345	488.144878	9.475290
7.413441	499.149988	9.480307
7.405446	484.726188	9.485325
7.524815	494.029637	9.490343
7.548361	482.772451	9.495360
7.934093	478.442248	9.500378
7.231310	480.319588	9.505395
7.141631	468.556293	9.510413
7.489314	483.264514	9.515431
7.538350	494.112690	9.520448
7.854016	492.289680	9.525466
7.642223	483.051194	9.530483
7.441607	484.158740	9.535501
7.188965	482.036614	9.540519
7.392881	484.876413	9.545536
7.650167	487.616332	9.550554
7.555536	500.929591	9.555571
7.726032	493.890738	9.560589
7.697043	481.919112	9.565607
7.683771	480.611540	9.570624
7.324028	479.411901	9.575642
7.161836	472.485142	9.580659
7.612007	486.732345	9.585677
7.622634	500.884327	9.590695
7.629242	500.207950	9.595712
7.815451	497.859274	9.600730
7.204295	492.362990	9.605747
7.480387	503.652119	9.610765
7.604270	501.363699	9.615783
7.824583	512.229231	9.620800
8.163190	499.786590	9.625818
7.623927	495.822216	9.630835
7.592510	485.927468	9.635853
7.565632	487.897721	9.640871
7.547780	495.963517	9.645888
7.609759	493.536477	9.650906
7.552623	500.030543	9.655923
7.815245	505.777085	9.660941
8.020790	502.582786	9.665959
7.236792	503.191607	9.670976
7.556054	502.936454	9.675994
7.366911	493.918474	9.681011
7.349768	512.322490	9.686029
7.791543	512.376342	9.691047
7.698892	509.332904	9.696064
7.539632	506.583923	9.701082
7.760043	508.704780	9.706099
7.716361	506.884423	9.711117
7.466155	513.781126	9.716135
7.806100	512.124722	9.721152
8.042731	508.733049	9.726170
7.681393	522.690866	9.731187
7.551516	512.464393	9.736205
7.936509	507.048712	9.741223
7.659978	509.323168	9.746240
7.754049	499.983102	9.751258
8.008728	508.365963	9.756275
7.861644	502.206834	9.761293
7.714627	501.472477	9.766311
7.581783	505.087716	9.771328
8.099556	502.740738	9.776346
8.049853	512.749180	9.781363
7.908933	510.716842	9.786381
7.768728	504.477741	9.791399
7.850436	507.043203	9.796416
8.234105	509.832752	9.801434
7.826462	510.616134	9.806451
7.844701	504.415323	9.811469
7.916511	508.610718	9.816487
7.809962	512.420652	9.821504
8.146862	506.169913	9.826522
7.688624	508.128860	9.831539
7.485921	508.065941	9.836557
7.796551	499.644989	9.841575
7.539400	508.250053	9.846592
7.738046	514.577817	9.851610
8.054877	531.582008	9.856627
7.845536	531.971406	9.861645
8.277411	526.396895	9.866663
8.044551	538.135015	9.871680
8.392325	526.378880	9.876698
7.805379	517.338009	9.881715
7.677617	503.737682	9.886733
7.627635	515.585988	9.891751
7.799679	523.401139	9.896768
8.052956	527.536549	9.901786
7.712959	526.592587	9.906803
8.276689	529.997706	9.911821
8.185723	527.859710	9.916839
7.804353	532.299683	9.921856
8.247277	525.997612	9.926874
8.180501	531.470727	9.931891
8.015729	538.249913	9.936909
7.977284	527.235939	9.941927
7.987326	526.745214	9.946944
7.942342	533.511941	9.951962
8.132740	528.341336	9.956979
8.001950	532.764138	9.961997
8.383218	524.328951	9.967015
8.051185	534.384797	9.972032
8.081199	527.926515	9.977050
8.358113	532.017196	9.982067
7.912250	529.527710	9.987085
8.195489	530.370101	9.992103
8.033914	533.746852	9.997120
8.296123	528.564995	10.002138
8.111237	533.043610	10.007155
8.170692	531.604720	10.012173
8.003752	522.201396	10.017191
8.050333	533.046825	10.022208
7.847475	530.086922	10.027226
7.839819	533.149224	10.032243
8.064220	536.052093	10.037261
8.033679	541.715192	10.042279
7.922517	553.683561	10.047296
8.392603	549.261230	10.052314
8.488738	562.295338	10.057331
8.219070	565.584890	10.062349
8.222406	566.111379	10.067367
8.073452	566.898412	10.072384
8.507432	569.509675	10.077402
8.689729	567.079552	10.082419
8.491640	557.785231	10.087437
8.143881	540.523920	10.092455
8.287708	540.236294	10.097472
8.171491	538.165369	10.102490
8.768378	553.686665	10.107507
8.554346	557.687017	10.112525
8.499711	547.641239	10.117543
8.423991	546.425497	10.122560
8.645603	540.161252	10.127578
8.501117	537.996927	10.132595
8.043889	523.615079	10.137613
8.163196	527.487458	10.142631
8.322316	544.484814	10.147648
8.229278	530.247870	10.152666
8.030773	538.884785	10.157683
8.310128	552.625477	10.162701
8.636231	556.216155	10.167719
8.537057	555.960290	10.172736
8.592785	548.084180	10.177754
8.286425	544.405194	10.182771
8.177143	550.475106	10.187789
8.521372	552.860588	10.192807
8.601303	566.032937	10.197824
8.661277	557.783774	10.202842
8.552967	552.293892	10.207859
8.077299	543.162990	10.212877
8.585263	546.974479	10.217895
8.537024	564.310454	10.222912
8.507976	556.943081	10.227930
8.879479	552.867553	10.232947
8.376957	552.779026	10.237965
8.526820	556.447810	10.242983
8.338764	553.801162	10.248000
8.746391	556.334502	10.253018
8.784068	560.623619	10.258035
8.415372	558.093635	10.263053
8.800297	560.510612	10.268071
8.489468	557.649673	10.273088
8.653086	554.108485	10.278106
8.474102	551.911694	10.283123
8.659703	561.466732	10.288141
8.215591	558.251136	10.293159
8.602150	558.468274	10.298176
8.724599	571.018586	10.303194
8.452469	564.913742	10.308211
8.500123	559.506718	10.313229
8.367887	557.845397	10.318247
8.192595	555.316670	10.323264
8.324533	553.803305	10.328282
8.432560	561.218252	10.333299
8.160209	563.889689	10.338317
8.478241	563.107712	10.343335
8.519849	571.501896	10.348352
8.925694	580.804686	10.353370
9.018741	589.329674	10.358387
8.925267	583.657577	10.363405
9.230254	576.910043	10.368423
8.658198	562.874357	10.373440
8.370568	561.057503	10.378458
8.445748	570.266931	10.383475
8.722232	576.500471	10.388493
9.076751	583.311920	10.393511
9.038167	591.384164	10.398528
8.744876	569.257526	10.403546
8.734994	563.736440	10.408563
8.764383	567.717590	10.413581
8.999251	568.924166	10.418599
8.616609	576.119353	10.423616
8.913997	584.356703	10.428634
8.608456	581.602227	10.433651
8.607810	584.108021	10.438669
8.941311	579.741796	10.443687
8.975496	581.825568	10.448704
8.868932	581.605575	10.453722
9.312389	578.301403	10.458739
9.002571	572.133035	10.463757
9.197536	562.960163	10.468775
8.681388	554.220604	10.473792
8.570512	561.341646	10.478810
8.814525	563.061182	10.483827
8.701123	578.226732	10.488845
8.798163	575.131471	10.493863
9.124331	585.219917	10.498880
8.762745	585.563742	10.503898
9.319783	577.782641	10.508915
9.108224	582.177085	10.513933
9.125108	577.191441	10.518951
9.213691	586.951041	10.523968
8.943588	572.943776	10.528986
9.040008	569.807588	10.534003
8.625896	569.632626	10.539021
9.066447	571.712687	10.544039
9.027231	582.331748	10.549056
9.040844	589.657358	10.554074
9.045413	579.166786	10.559091
9.273807	585.199582	10.564109
9.294389	579.443345	10.569127
8.891854	577.698141	10.574144
8.902699	582.224996	10.579162
8.945366	577.815977	10.584179
8.916355	592.173057	10.589197
8.966867	582.760877	10.594215
8.980449	581.600569	10.599232
9.020563	586.570961	10.604250
9.248634	584.916300	10.609267
9.116656	586.584296	10.614285
9.379358	588.755341	10.619303
9.389297	588.895789	10.624320
9.070173	591.082255	10.629338
9.193589	578.190440	10.634355
8.818390	591.443585	10.639373
9.262689	584.532209	10.644391
9.121491	581.344887	10.649408
9.108375	589.984339	10.654426
9.192898	588.415284	10.659443
9.099944	586.833012	10.664461
9.288930	577.651603	10.669479
9.341113	587.123418	10.674496
9.562497	587.729351	10.679514
8.950764	582.520307	10.684531
8.930441	583.561741	10.689549
9.274332	577.650707	10.694567
9.283870	579.662601	10.699584
8.919036	580.306736	10.704602
9.218034	577.842547	10.709619
9.030105	589.046643	10.714637
9.104253	589.208589	10.719655
9.585749	601.510164	10.724672
9.506112	593.595282	10.729690
9.202009	583.048930	10.734707
9.390325	592.729791	10.739725
9.632616	597.043662	10.744743
9.336381	588.711441	10.749760
9.568673	578.828971	10.754778
9.413135	574.829703	10.759795
9.535866	575.918151	10.764813
9.381959	575.923325	10.769831
9.720602	582.219711	10.774848
9.512989	579.790718	10.779866
9.619045	583.027716	10.784883
9.220369	585.103570	10.789901
9.342240	581.499491	10.794919
9.525517	580.744938	10.799936
9.840757	588.114806	10.804954
9.851321	588.715901	10.809971
10.008390	583.957599	10.814989
9.481246	581.603916	10.820007
9.689336	584.007577	10.825024
9.405800	578.914369	10.830042
9.827200	574.849953	10.835059
9.453974	579.878794	10.840077
9.734705	579.544471	10.845095
9.672384	580.381047	10.850112
9.404828	590.344771	10.855130
9.834680	579.632931	10.860147
9.445052	582.417420	10.865165
9.500924	581.733322	10.870183
9.785620	583.941945	10.875200
9.430374	582.075723	10.880218
10.063629	574.449939	10.885235
9.567596	567.360855	10.890253
9.248021	569.165539	10.895271
9.665501	571.870906	10.900288
9.249336	575.587354	10.905306
9.828473	568.061570	10.910323
9.225990	574.697912	10.915341
9.509912	585.291592	10.920359
9.551336	582.728905	10.925376
9.350566	589.908225	10.930394
9.551056	580.371562	10.935411
9.864726	587.249373	10.940429
9.951120	588.135232	10.945447
9.594107	585.316237	10.950464
9.355831	592.709716	10.955482
9.753038	582.962351	10.960499
9.504497	581.821021	10.965517
9.339011	586.179846	10.970535
9.999298	600.570943	10.975552
9.729480	609.499932	10.980570
9.628279	602.825496	10.985587
9.669586	610.755844	10.990605
9.467602	611.387087	10.995623
9.427472	606.094788	11.000640
9.411408	607.593147	11.005658
9.544311	608.853571	11.010675
9.578222	606.143736	11.015693
9.652220	606.390912	11.020711
9.550815	620.427998	11.025728
9.639366	631.105964	11.030746
10.088020	629.808057	11.035763
9.914976	632.397674	11.040781
10.016648	638.204190	11.045799
10.246651	633.115711	11.050816
9.737725	627.234139	11.055834
9.884371	609.343033	11.060851
9.799490	619.609510	11.065869
9.830278	626.777810	11.070887
10.313376	635.023956	11.075904
9.995525	629.532167	11.080922
10.097032	615.580253	11.085939
10.325180	604.369828	11.090957
10.222527	609.788628	11.095975
10.362629	608.191930	11.100992
10.012490	607.650339	11.106010
10.400511	608.583614	11.111027
10.165894	611.223900	11.116045
9.812382	604.819369	11.121063
9.898025	604.430406	11.126080
9.990245	611.832071	11.131098
9.956786	610.079529	11.136115
9.947289	607.206082	11.141133
10.229633	611.983895	11.146151
10.445433	607.945373	11.151168
10.041848	612.997915	11.156186
10.399021	602.966478	11.161203
9.931252	620.983620	11.166221
9.982512	613.922376	11.171239
10.143896	604.808393	11.176256
10.277519	615.955814	11.181274
9.914179	620.232038	11.186291
10.337589	617.492732	11.191309
9.981194	616.639697	11.196327
10.169029	607.196521	11.201344
9.939722	612.038721	11.206362
10.044710	605.016399	11.211379
9.848516	605.608865	11.216397
9.760146	627.126306	11.221415
10.198656	630.516351	11.226432
10.123067	635.448081	11.231450
10.384445	640.910839	11.236467
10.242637	632.532311	11.241485
10.115472	635.685940	11.246503
10.136377	626.931627	11.251520
10.182203	645.269109	11.256538
10.165139	634.450535	11.261555
10.211560	631.722957	11.266573
9.839663	636.871526	11.271591
10.216103	630.620860	11.276608
10.015208	639.545377	11.281626
10.191015	641.550162	11.286643
10.274227	645.595480	11.291661
10.023574	659.577086	11.296679
10.364971	659.940156	11.301696
10.277631	670.210204	11.306714
10.748205	663.755429	11.311731
10.531620	661.103768	11.316749
10.516776	660.162503	11.321767
10.738804	657.988074	11.326784
10.594778	654.043789	11.331802
10.541363	644.332280	11.336819
10.734552	637.861016	11.341837
10.145237	642.305194	11.346855
10.454685	635.402305	11.351872
10.431823	638.956157	11.356890
10.172295	645.254769	11.361907
10.653523	651.472035	11.366925
10.710474	667.008600	11.371943
10.637110	641.205615	11.376960
10.350195	644.576779	11.381978
10.517683	650.824266	11.386995
10.801267	654.831881	11.392013
10.619149	660.181095	11.397031
10.716670	642.875165	11.402048
10.667305	643.230032	11.407066
10.638121	640.621595	11.412083
10.491893	634.670570	11.417101
10.458714	644.755392	11.422119
10.600249	638.582554	11.427136
10.467922	646.716848	11.432154
10.791006	654.644091	11.437171
10.557557	654.731156	11.442189
10.522081	663.424638	11.447207
10.648177	656.073942	11.452224
10.724946	667.877243	11.457242
10.499854	671.554305	11.462259
10.802091	673.091160	11.467277
10.428800	671.407637	11.472295
10.786921	667.602423	11.477312
10.806137	667.997038	11.482330
10.750108	663.300505	11.487347
11.037931	662.677891	11.492365
10.570656	667.308082	11.497383
10.871448	659.554472	11.502400
10.923282	655.831963	11.507418
10.774722	665.657164	11.512435
10.980660	655.914481	11.517453
10.935162	657.938163	11.522471
11.051033	653.299906	11.527488
10.551025	652.018091	11.532506
10.652480	659.755999	11.537523
10.805547	664.285838	11.542541
10.690074	662.647127	11.547559
11.006326	660.303301	11.552576
10.543549	664.273223	11.557594
10.738875	659.512062	11.562611
10.908741	652.883500	11.567629
10.426848	664.098988	11.572647
10.774086	668.595249	11.577664
10.814520	660.746731	11.582682
10.463519	667.697156	11.587699
10.640963	671.986492	11.592717
10.594189	688.315655	11.597735
11.032612	679.060398	11.602752
11.062457	684.483707	11.607770
11.174161	687.110768	11.612787
11.394165	678.299988	11.617805
11.386765	697.305427	11.622823
11.048204	677.237026	11.627840
10.947947	667.390833	11.632858
10.890217	667.806972	11.637875
11.128217	674.292729	11.642893
11.380149	681.341195	11.647911
11.190330	674.522827	11.652928
11.047042	660.767023	11.657946
10.960303	648.889539	11.662963
11.056612	651.960819	11.667981
10.812138	663.199068	11.672999
11.140533	670.121940	11.678016
11.219440	682.350949	11.683034
10.881560	685.925766	11.688051
11.263511	683.615824	11.693069
11.065765	681.324126	11.698087
11.040957	685.137069	11.703104
11.445111	681.378289	11.708122
11.123206	688.049607	11.713139
11.733506	688.092835	11.718157
11.267690	692.580792	11.723175
11.349452	687.559706	11.728192
11.489665	680.613887	11.733210
11.374794	680.335234	11.738227
11.322195	668.777436	11.743245
11.030498	671.025886	11.748263
11.376011	677.052986	11.753280
11.260268	669.541360	11.758298
11.451992	673.052130	11.763315
11.087076	669.363357	11.768333
11.044945	689.229453	11.773351
11.251330	683.081153	11.778368
11.679062	678.113160	11.783386
11.178630	683.660579	11.788403
11.749168	677.316369	11.793421
11.349510	687.117807	11.798439
11.257205	692.569725	11.803456
11.517410	688.413774	11.808474
11.398581	683.869087	11.813491
11.468006	684.075955	11.818509
11.558566	683.257029	11.823527
11.637315	682.338968	11.828544
11.462063	676.092675	11.833562
11.561084	691.477502	11.838579
11.629817	681.099894	11.843597
11.447968	671.376935	11.848615
11.228166	670.669754	11.853632
11.322137	677.989121	11.858650
11.560513	679.665371	11.863667
11.835840	680.527944	11.868685
11.444990	691.306305	11.873703
11.658874	684.263735	11.878720
11.765915	688.952270	11.883738
11.409633	687.013616	11.888755
11.856759	676.813409	11.893773
11.535912	680.726383	11.898791
11.608236	690.094111	11.903808
11.717500	683.282528	11.908826
11.500975	682.432821	11.913843
11.598415	675.547355	11.918861
11.354529	682.190668	11.923879
11.158982	679.560954	11.928896
11.416486	671.618461	11.933914
11.362385	673.750790	11.938931
11.627520	676.404303	11.943949
11.242158	685.395614	11.948967
11.352574	685.684422	11.953984
11.797266	689.540569	11.959002
11.487595	709.783122	11.964019
12.297014	700.545466	11.969037
12.055757	705.559977	11.974055
11.734462	694.126313	11.979072
11.452378	680.565809	11.984090
11.643585	697.507791	11.989107
12.022922	707.266082	11.994125
12.078697	707.418285	11.999143
11.766703	693.625772	12.004160
11.983228	697.542917	12.009178
11.896364	698.525355	12.014195
11.906028	678.058410	12.019213
11.811025	677.792422	12.024231
11.801007	686.005401	12.029248
12.258641	693.258328	12.034266
12.043866	698.950343	12.039283
11.750316	691.652759	12.044301
11.800482	686.138005	12.049319
11.848695	691.369090	12.054336
11.994815	691.415618	12.059354
12.295003	707.526335	12.064371
12.028396	696.563785	12.069389
11.753721	698.746456	12.074407
11.989728	700.672387	12.079424
11.866659	699.050642	12.084442
12.107667	704.866907	12.089459
12.132395	705.563618	12.094477
12.136930	703.906100	12.099495
11.879079	712.830109	12.104512
12.110804	720.115287	12.109530
12.346520	716.641667	12.114547
12.403898	708.459114	12.119565
11.858298	695.773021	12.124583
12.017347	703.299953	12.129600
12.233551	707.434902	12.134618
12.374270	712.727238	12.139635
12.067171	692.347777	12.144653
12.134117	697.086778	12.149671
12.276849	692.368562	12.154688
12.052192	686.196278	12.159706
12.042071	700.597822	12.164723
12.405268	701.822171	12.169741
12.300084	707.171969	12.174759
12.127321	702.569455	12.179776
12.211130	703.499906	12.184794
11.926138	705.371769	12.189811
12.103110	705.050545	12.194829
12.316320	709.615153	12.199847
12.186796	703.806655	12.204864
12.343378	704.088230	12.209882
12.361918	703.482560	12.214899
12.187617	695.118561	12.219917
12.315243	700.311959	12.224935
12.140143	704.015909	12.229952
12.296780	708.889184	12.234970
12.194435	708.346635	12.239987
12.328868	706.337404	12.245005
11.985411	709.521778	12.250023
12.053075	710.470539	12.255040
12.555734	707.176003	12.260058
12.412394	713.611069	12.265075
12.576671	713.888283	12.270093
12.092812	715.349491	12.275111
12.452986	723.687522	12.280128
12.943717	724.374336	12.285146
12.913636	716.293845	12.290163
12.747292	712.529769	12.295181
12.616914	711.420410	12.300199
12.507502	710.266741	12.305216
12.467163	701.544077	12.310234
12.585445	711.961813	12.315251
12.744427	699.749149	12.320269
12.748585	708.461691	12.325287
12.374360	701.157808	12.330304
12.807289	701.831587	12.335322
12.284323	700.294588	12.340339
12.596457	695.079615	12.345357
12.641034	697.111279	12.350375
12.049902	700.902503	12.355392
12.145222	699.754627	12.360410
12.173104	715.728134	12.365427
12.646217	718.311198	12.370445
13.021816	726.788825	12.375463
12.917499	726.344415	12.380480
13.082952	737.307042	12.385498
13.097792	731.065660	12.390515
13.142811	721.742631	12.395533
12.971440	698.968723	12.400551
12.642614	698.105052	12.405568
12.737054	696.581772	12.410586
12.588740	705.911494	12.415603
12.566236	702.980109	12.420621
12.993230	708.255993	12.425639
13.038939	716.999898	12.430656
12.743653	692.014253	12.435674
12.730278	703.093241	12.440691
12.923434	711.223904	12.445709
12.901406	707.124793	12.450727
12.868894	716.729867	12.455744
12.962185	703.612307	12.460762
12.524593	705.287172	12.465779
13.077006	719.385998	12.470797
13.159879	727.533948	12.475815
12.997851	724.327774	12.480832
12.917622	721.440144	12.485850
13.176835	732.309183	12.490867
12.618771	715.055406	12.495885
12.917239	713.664260	12.500903
12.441704	732.241309	12.505920
13.141101	722.503326	12.510938
12.923605	728.934237	12.515955
12.983637	726.983999	12.520973
13.183530	729.335316	12.525991
12.957819	736.379746	12.531008
13.219942	729.462144	12.536026
13.007100	735.987004	12.541043
12.954879	734.360467	12.546061
13.116001	729.194390	12.551079
13.133715	731.952949	12.556096
13.287821	728.637281	12.561114
12.983672	733.772107	12.566131
13.494843	728.630081	12.571149
13.401058	723.361933	12.576167
12.994433	732.558571	12.581184
13.222818	727.934224	12.586202
13.388514	729.009638	12.591219
13.015020	730.286297	12.596237
13.494392	724.202508	12.601255
13.181564	722.329625	12.606272
13.230824	719.270228	12.611290
13.024639	732.784175	12.616307
13.062789	723.948217	12.621325
12.973885	730.504149	12.626343
12.966142	724.121140	12.631360
13.138897	720.909849	12.636378
13.650272	732.884940	12.641395
13.260223	733.504627	12.646413
13.187067	732.499911	12.651431
13.186570	745.180063	12.656448
13.571098	740.502846	12.661466
13.661015	742.682046	12.666483
13.575182	743.951505	12.671501
13.506037	735.138664	12.676519
13.367197	740.051931	12.681536
13.511714	731.767351	12.686554
13.732020	737.530065	12.691571
13.428255	735.056155	12.696589
13.455370	723.713051	12.701607
13.458729	733.381942	12.706624
13.604743	730.865963	12.711642
13.553053	738.432240	12.716659
13.581907	749.258487	12.721677
13.797059	737.119048	12.726695
13.409639	741.885069	12.731712
13.295460	729.106111	12.736730
13.620254	732.981054	12.741747
13.855783	738.861305	12.746765
13.849388	744.100961	12.751783
13.664143	739.456212	12.756800
13.551099	739.155180	12.761818
13.871760	733.771601	12.766835
13.532596	734.348602	12.771853
13.650378	732.730142	12.776871
13.790915	750.784650	12.781888
13.936611	744.630058	12.786906
13.692087	732.026156	12.791923
13.440857	736.038687	12.796941
13.877340	738.157276	12.801959
13.970117	739.745890	12.806976
13.671816	745.577239	12.811994
13.415690	741.003556	12.817011
13.714018	742.244382	12.822029
14.074488	741.234841	12.827047
13.954098	744.510504	12.832064
13.912066	744.943120	12.837082
14.078000	745.756564	12.842099
13.815128	744.415496	12.847117
13.947909	732.247941	12.852135
13.680046	744.736453	12.857152
13.717994	738.870146	12.862170
13.906665	744.003499	12.867187
13.615470	743.316968	12.872205
13.902445	741.832946	12.877223
13.789611	742.819456	12.882240
13.821905	738.430958	12.887258
13.981963	733.899367	12.892275
13.682927	743.123335	12.897293
14.109562	736.299876	12.902311
13.890065	741.175287	12.907328
13.884709	744.123656	12.912346
14.288516	743.208311	12.917363
14.257500	737.851429	12.922381
14.185325	730.181471	12.927399
13.815208	741.158586	12.932416
13.800367	739.996409	12.937434
14.210146	728.845811	12.942451
13.977612	732.864881	12.947469
14.394915	737.441700	12.952487
14.241654	743.625866	12.957504
13.805330	736.991265	12.962522
14.072263	757.427553	12.967539
14.389345	766.684389	12.972557
14.149838	759.431958	12.977575
14.288136	766.791754	12.982592
14.289501	762.922496	12.987610
14.185022	766.220916	12.992627
14.132492	770.978656	12.997645
14.225892	760.208971	13.002663
14.078347	764.366210	13.007680
14.431373	767.987427	13.012698
14.090994	769.710183	13.017715
13.995461	760.885685	13.022733
14.147183	756.355394	13.027751
14.291695	766.033745	13.032768
14.192629	767.908041	13.037786
14.313395	761.391274	13.042803
13.999676	775.190347	13.047821
14.575969	768.251909	13.052839
14.367315	776.442401	13.057856
14.560862	775.888204	13.062874
14.513624	771.559497	13.067891
14.425191	779.308274	13.072909
14.527357	782.637437	13.077927
14.867216	784.597600	13.082944
14.407176	776.663343	13.087962
14.676881	769.331125	13.092979
14.934458	769.798850	13.097997
14.785964	757.687971	13.103015
14.816407	755.931715	13.108032
14.802468	756.170580	13.113050
14.652815	755.780610	13.118067
14.622630	762.226367	13.123085
14.714469	760.350037	13.128103
14.567358	768.552974	13.133120
14.688946	766.589931	13.138138
14.861630	760.102900	13.143155
14.669169	758.135414	13.148173
15.020752	753.103592	13.153191
15.096500	757.762334	13.158208
14.497279	759.550891	13.163226
14.597495	755.666146	13.168243
14.410439	763.405123	13.173261
14.285802	758.290122	13.178279
14.478269	767.803169	13.183296
14.550705	762.202852	13.188314
14.994467	769.429581	13.193331
14.872128	785.578168	13.198349
14.935790	774.232461	13.203367
14.889523	780.570291	13.208384
14.797430	777.473070	13.213402
14.928151	773.914904	13.218419
14.542539	782.111034	13.223437
14.728631	790.482684	13.228455
14.952984	784.094846	13.233472
14.780501	785.554611	13.238490
15.053011	788.427893	13.243507
14.890549	785.871875	13.248525
14.970937	778.260045	13.253543
15.299933	790.834955	13.258560
15.010646	791.883829	13.263578
15.359231	789.001585	13.268595
14.972315	789.119007	13.273613
15.332244	779.364752	13.278631
15.356615	789.323873	13.283648
14.972432	786.540661	13.288666
15.434726	788.762510	13.293683
15.049962	790.132458	13.298701
15.394648	785.003877	13.303719
15.157340	771.641417	13.308736
14.884506	763.292824	13.313754
15.078927	771.035151	13.318771
14.941143	792.213392	13.323789
14.919496	785.643190	13.328807
15.120502	782.566318	13.333824
15.172325	794.897478	13.338842
15.476010	785.858938	13.343859
15.126987	784.777520	13.348877
15.148990	782.590235	13.353895
15.262441	798.184334	13.358912
15.298025	787.641443	13.363930
15.291264	778.014071	13.368947
15.011729	788.623570	13.373965
14.969472	791.644001	13.378983
14.964789	788.116514	13.384000
15.347748	801.333077	13.389018
15.803780	800.478975	13.394035
15.332738	796.166170	13.399053
15.211763	793.556313	13.404071
15.859667	794.073337	13.409088
15.203735	798.575328	13.414106
15.611178	798.300044	13.419123
15.507393	807.900555	13.424141
15.528922	813.927970	13.429159
15.752364	802.525653	13.434176
15.573667	795.894846	13.439194
15.852231	780.892573	13.444211
15.521988	781.998356	13.449229
15.459216	773.260238	13.454247
15.458534	784.173185	13.459264
15.592436	786.433862	13.464282
15.973356	785.137090	13.469299
15.776254	793.944323	13.474317
15.566295	782.729845	13.479335
15.546784	777.443733	13.484352
15.653412	782.321707	13.489370
15.673888	772.929912	13.494387
15.955749	777.408042	13.499405
15.495661	778.540481	13.504423
15.662593	785.267789	13.509440
15.572042	783.789265	13.514458
15.552255	794.654718	13.519475
15.371921	806.899183	13.524493
15.578052	803.404936	13.529511
15.867278	808.112295	13.534528
15.630893	808.288183	13.539546
15.810040	808.326381	13.544563
15.945518	809.359197	13.549581
15.747346	808.765386	13.554599
15.872301	806.483072	13.559616
15.473327	816.180331	13.564634
16.029411	799.660788	13.569651
15.526929	808.001474	13.574669
16.036565	809.363834	13.579687
15.819641	802.461301	13.584704
15.847748	811.362646	13.589722
16.357466	818.758944	13.594739
15.921158	805.882078	13.599757
15.803265	815.276519	13.604775
16.108151	825.422085	13.609792
16.145603	833.798108	13.614810
16.326105	823.860501	13.619827
16.205531	812.325884	13.624845
16.063582	810.845943	13.629863
16.430564	806.436548	13.634880
15.985533	805.663663	13.639898
15.767944	798.167940	13.644915
16.174522	821.425825	13.649933
16.522096	823.135472	13.654951
16.402099	818.568842	13.659968
15.843792	815.885491	13.664986
16.127425	816.178720	13.670003
16.061789	829.837979	13.675021
16.354193	828.403592	13.680039
16.396792	826.058439	13.685056
16.022757	833.321808	13.690074
16.078579	824.833329	13.695091
16.307691	821.326010	13.700109
16.336500	833.095908	13.705127
16.358233	830.381635	13.710144
16.448690	820.584372	13.715162
16.679895	830.845628	13.720179
16.976781	829.637759	13.725197
16.650044	825.438038	13.730215
16.525420	822.860307	13.735232
16.395906	826.856945	13.740250
16.656122	826.112418	13.745267
16.566337	826.946997	13.750285
16.576124	818.203799	13.755303
16.695541	817.380346	13.760320
16.456321	809.332580	13.765338
16.466171	798.326652	13.770355
16.332287	812.558328	13.775373
16.339107	815.946618	13.780391
16.644983	825.823783	13.785408
16.635241	828.356283	13.790426
16.699978	819.989487	13.795443
16.724376	828.613708	13.800461
16.412505	817.765473	13.805479
16.705197	821.099506	13.810496
16.522260	830.639847	13.815514
16.816636	823.553053	13.820531
16.954865	824.642243	13.825549
16.963392	820.983290	13.830567
16.996717	825.004907	13.835584
16.775199	830.281450	13.840602
16.509608	824.112376	13.845619
16.649819	825.299086	13.850637
16.600898	823.694115	13.855655
17.021971	818.604049	13.860672
16.928400	825.514200	13.865690
16.958518	820.561129	13.870707
16.748310	828.650903	13.875725
16.555628	828.614814	13.880743
16.884275	821.162886	13.885760
16.900496	820.494458	13.890778
16.966323	811.016642	13.895795
16.901052	814.542460	13.900813
16.811738	818.709524	13.905831
16.919913	817.288224	13.910848
16.661263	828.225837	13.915866
16.901503	811.869378	13.920883
17.073134	821.597160	13.925901
16.613150	818.882624	13.930919
17.109481	821.427351	13.935936
17.060545	836.308461	13.940954
17.255129	840.737165	13.945971
17.528233	841.789445	13.950989
17.167009	824.495253	13.956007
17.580857	817.187769	13.961024
17.270546	820.098724	13.966042
17.326065	821.620599	13.971059
17.278168	830.363446	13.976077
16.864071	827.771109	13.981095
17.278159	814.641075	13.986112
16.978369	820.021397	13.991130
17.456210	824.071198	13.996147
17.012954	831.496892	14.001165
16.967930	845.178179	14.006183
17.605884	838.252144	14.011200
17.576967	842.586477	14.016218
17.618059	841.118881	14.021235
17.550543	833.959395	14.026253
16.997969	824.505878	14.031271
17.553190	828.527777	14.036288
17.488034	841.012998	14.041306
17.782304	846.536940	14.046323
17.744385	831.262316	14.051341
17.077931	824.524881	14.056359
17.426464	827.525115	14.061376
17.401081	846.164298	14.066394
17.268028	841.422981	14.071411
17.560482	835.617753	14.076429
17.319182	846.902956	14.081447
17.456257	841.538641	14.086464
17.617597	842.785160	14.091482
17.470036	848.037497	14.096499
17.618190	848.727498	14.101517
17.497300	846.587841	14.106535
17.768036	840.621910	14.111552
17.677464	851.362787	14.116570
17.881538	845.148521	14.121587
17.596870	846.995100	14.126605
17.682323	848.490197	14.131623
17.876931	842.400492	14.136640
17.515201	842.359332	14.141658
17.573138	847.166057	14.146675
17.870033	840.814171	14.151693
17.200632	849.373536	14.156711
17.799203	848.336151	14.161728
17.917174	853.398562	14.166746
17.863986	864.815251	14.171763
18.015804	857.536182	14.176781
17.476028	852.404146	14.181799
18.029628	853.472440	14.186816
18.165105	858.784577	14.191834
18.223594	858.428265	14.196851
17.973932	851.385673	14.201869
17.972324	847.908186	14.206887
18.165742	843.342937	14.211904
17.843811	844.488448	14.216922
17.798879	850.933391	14.221939
18.302887	861.426480	14.226957
18.287570	876.602161	14.231975
18.129844	855.807784	14.236992
18.013662	849.167162	14.242010
18.222343	849.980226	14.247027
18.206040	858.367839	14.252045
18.259905	866.189034	14.257063
17.984641	846.022161	14.262080
17.925415	849.638558	14.267098
17.769428	860.844131	14.272115
17.936809	859.624993	14.277133
18.361117	859.186118	14.282151
18.326823	855.252998	14.287168
18.264618	864.828090	14.292186
18.108718	871.583921	14.297203
18.559294	860.925473	14.302221
18.507594	870.647246	14.307239
18.397879	868.597355	14.312256
18.323388	859.785290	14.317274
17.854580	864.668238	14.322291
18.238721	861.852996	14.327309
18.159018	862.184219	14.332327
18.251257	857.802079	14.337344
18.437209	874.795546	14.342362
18.222567	885.978766	14.347379
18.580381	884.313218	14.352397
18.625964	893.738892	14.357415
18.378980	893.521960	14.362432
18.600318	881.845363	14.367450
18.670651	891.566963	14.372467
18.419090	889.390969	14.377485
18.611166	891.143922	14.382503
18.709319	893.100942	14.387520
19.111581	892.088000	14.392538
18.785684	891.331160	14.397555
18.873461	883.263685	14.402573
18.582409	890.182712	14.407591
19.394987	887.723223	14.412608
18.654125	865.224524	14.417626
18.674168	852.853642	14.422643
19.120032	855.895436	14.427661
18.507332	858.115308	14.432679
18.535496	854.721518	14.437696
18.703485	858.699953	14.442714
18.885208	867.267985	14.447731
19.166704	871.629430	14.452749
19.179224	880.075654	14.457767
18.982601	862.698831	14.462784
18.826994	863.310192	14.467802
18.718924	857.113270	14.472819
18.984341	871.405508	14.477837
19.226174	877.300597	14.482855
19.472465	861.457547	14.487872
18.865858	855.550177	14.492890
18.833330	851.506327	14.497907
18.855174	853.270168	14.502925
19.116931	862.914423	14.507943
18.947489	868.327987	14.512960
19.310591	871.477426	14.517978
18.989869	874.475228	14.522995
19.141285	873.558395	14.528013
19.338975	881.183491	14.533031
18.979080	867.635036	14.538048
19.106576	879.935464	14.543066
19.210041	873.831627	14.548083
19.416462	876.604824	14.553101
19.207371	882.453798	14.558119
19.152768	875.326986	14.563136
19.293206	871.789368	14.568154
18.838707	877.755687	14.573171
19.452755	876.122578	14.578189
19.443064	884.963609	14.583207
19.222170	878.942149	14.588224
19.207659	876.050509	14.593242
19.207357	877.439121	14.598259
19.368679	870.603532	14.603277
19.110111	874.958075	14.608295
19.144705	879.007908	14.613312
19.163963	876.754769	14.618330
18.682187	884.060286	14.623347
19.434998	893.207892	14.628365
19.162684	903.254587	14.633383
19.254810	899.740312	14.638400
19.442646	901.427658	14.643418
19.561566	901.386929	14.648435
19.256064	889.972756	14.653453
19.265161	901.629021	14.658471
19.400043	907.708137	14.663488
20.063304	921.136496	14.668506
20.007953	919.781835	14.673523
19.848370	908.253268	14.678541
19.638751	906.395752	14.683559
19.741845	898.041845	14.688576
19.593458	906.011512	14.693594
19.524772	905.252242	14.698611
19.799943	916.923635	14.703629
20.318069	923.340346	14.708647
19.899387	915.159702	14.713664
19.983588	905.483295	14.718682
19.855438	912.089624	14.723699
19.904826	905.997404	14.728717
19.818130	904.284733	14.733735
19.589749	905.541823	14.738752
19.931618	912.475303	14.743770
19.940534	928.770714	14.748787
20.442919	920.294275	14.753805
20.431718	918.475099	14.758823
19.978483	906.948359	14.763840
20.338838	893.583686	14.768858
20.131132	902.430504	14.773875
20.161146	892.557463	14.778893
19.912681	887.603840	14.783911
20.003788	897.454734	14.788928
20.053471	901.461182	14.793946
19.945104	909.535035	14.798963
20.306868	913.012900	14.803981
20.102799	916.509991	14.808999
20.143767	921.060615	14.814016
19.974119	915.558140	14.819034
19.928884	922.609080	14.824051
20.076862	924.081763	14.829069
20.345040	915.329592	14.834087
20.275003	915.990665	14.839104
20.574036	916.057418	14.844122
20.398264	919.382816	14.849139
20.528759	913.505107	14.854157
20.859116	915.469929	14.859175
20.567312	911.703377	14.864192
20.861256	910.410757	14.869210
20.246150	916.790422	14.874227
20.380767	913.354695	14.879245
20.725627	915.806402	14.884263
20.262431	910.734935	14.889280
20.685548	905.635058	14.894298
20.669259	910.787949	14.899315
20.860034	910.660222	14.904333
20.528312	919.835753	14.909351
20.580041	913.765254	14.914368
20.789214	920.441813	14.919386
20.653543	916.013316	14.924403
20.656848	916.388339	14.929421
20.567148	911.491885	14.934439
20.565801	922.452359	14.939456
20.758941	913.746659	14.944474
20.875810	912.895199	14.949491
20.664978	912.391732	14.954509
21.065085	918.476634	14.959527
20.866684	908.285917	14.964544
20.851208	910.528989	14.969562
20.886053	916.213521	14.974579
20.812262	915.189958	14.979597
20.856577	914.545528	14.984615
20.862824	918.864902	14.989632
20.973020	920.674869	14.994650
20.957953	915.687825	14.999667
20.709463	915.698350	15.004685
20.740868	908.387633	15.009703
20.589708	919.977500	15.014720
20.603327	917.034108	15.019738
20.535600	923.119727	15.024755
20.979978	925.723103	15.029773
20.868993	934.116119	15.034791
20.801620	942.697969	15.039808
20.992811	941.951629	15.044826
21.096682	949.357920	15.049843
21.134630	938.577881	15.054861
21.223360	944.421239	15.059879
20.925593	953.862870	15.064896
21.327811	946.538221	15.069914
21.102259	946.835491	15.074931
21.078207	942.720863	15.079949
21.178271	951.330133	15.084967
21.218703	958.664315	15.089984
22.014000	962.790644	15.095002
21.693151	953.849871	15.100019
21.596071	956.661165	15.105037
21.867133	949.413870	15.110055
21.619583	946.684965	15.115072
22.188300	936.566548	15.120090
22.027670	941.874609	15.125107
22.165705	939.514489	15.130125
21.883675	915.129221	15.135143
21.536168	917.828265	15.140160
21.392019	904.709889	15.145178
21.034054	918.071029	15.150195
21.526882	922.086946	15.155213
21.931999	924.996280	15.160231
21.370865	927.078690	15.165248
21.745919	918.944099	15.170266
21.737185	938.480187	15.175283
21.807356	932.072272	15.180301
21.980459	928.179226	15.185319
21.661435	915.160826	15.190336
21.732362	913.653835	15.195354
21.834347	917.137688	15.200371
21.853554	916.269971	15.205389
21.766648	917.539610	15.210407
21.459964	923.441759	15.215424
21.580147	940.540269	15.220442
21.733757	933.743734	15.225459
21.639757	932.960025	15.230477
21.580458	938.643536	15.235495
21.557863	935.248216	15.240512
21.583769	934.660319	15.245530
22.051335	942.186352	15.250547
21.818336	943.485194	15.255565
21.803148	951.778001	15.260583
22.033265	966.792226	15.265600
22.233625	959.893681	15.270618
22.021231	968.495109	15.275635
21.774727	964.958137	15.280653
22.073168	961.512513	15.285671
22.189121	956.937282	15.290688
22.251307	951.325887	15.295706
22.298910	963.339084	15.300723
22.313806	960.193510	15.305741
22.255336	956.096895	15.310759
22.608647	958.752415	15.315776
22.637426	955.623602	15.320794
22.339308	953.366529	15.325811
22.268869	956.325131	15.330829
22.219206	956.414959	15.335847
22.380358	961.678922	15.340864
22.171125	964.384710	15.345882
22.342894	950.765515	15.350899
22.188741	960.004764	15.355917
22.525683	962.482965	15.360935
21.948837	951.960192	15.365952
22.675490	952.111427	15.370970
22.500754	955.496630	15.375987
22.711972	947.614917	15.381005
22.295076	943.331462	15.386023
21.965546	961.368313	15.391040
22.531744	968.042601	15.396058
22.788518	977.406827	15.401075
22.582525	983.249037	15.406093
22.899536	980.709388	15.411111
22.625475	982.914087	15.416128
22.989656	979.218314	15.421146
23.121125	971.181825	15.426163
23.152512	973.310263	15.431181
23.144440	961.174088	15.436199
22.613440	955.986997	15.441216
22.787257	942.973411	15.446234
22.840437	959.006291	15.451251
22.875483	962.794136	15.456269
23.298048	966.716929	15.461287
22.971622	961.018093	15.466304
22.830783	959.657888	15.471322
22.936980	956.857778	15.476339
22.990414	969.605380	15.481357
23.395008	974.206344	15.486375
23.066425	976.668898	15.491392
22.931500	959.632614	15.496410
22.955888	964.646602	15.501427
22.919293	967.025536	15.506445
22.913428	969.068290	15.511463
23.118797	977.799931	15.516480
22.971297	970.097490	15.521498
22.983089	969.527582	15.526515
23.074503	971.286847	15.531533
23.321961	973.637057	15.536551
22.789096	977.305597	15.541568
22.786762	973.143378	15.546586
23.244197	974.220435	15.551603
23.346451	989.352544	15.556621
23.360738	985.500148	15.561639
23.415997	998.017106	15.566656
23.616898	999.658232	15.571674
23.947484	987.708825	15.576691
23.526972	977.615986	15.581709
23.503036	964.507133	15.586727
23.423253	973.542230	15.591744
23.526288	964.030101	15.596762
23.661207	959.780106	15.601779
23.348491	970.903005	15.606797
23.203604	969.729630	15.611815
23.336595	987.930729	15.616832
23.877203	978.469957	15.621850
24.032414	987.496645	15.626867
23.844583	982.659729	15.631885
24.139808	980.524287	15.636903
23.847312	976.423309	15.641920
23.769192	965.462619	15.646938
23.866695	959.318660	15.651955
23.937126	959.231879	15.656973
23.516896	961.610958	15.661991
23.775440	967.007989	15.667008
23.758538	971.463549	15.672026
23.798082	985.276864	15.677043
23.646760	993.767748	15.682061
24.352683	997.775542	15.687079
23.957781	999.721460	15.692096
23.865758	1003.314624	15.697114
23.810186	995.559898	15.702131
23.993490	996.061358	15.707149
24.329108	995.850975	15.712167
23.918335	998.976518	15.717184
23.920190	984.724342	15.722202
24.130241	994.780721	15.727219
24.147247	1003.658654	15.732237
24.055693	999.687135	15.737255
24.082314	999.379996	15.742272
23.757123	997.408032	15.747290
24.146955	990.287281	15.752307
24.004608	995.573559	15.757325
24.065375	991.947413	15.762343
24.129513	1007.224367	15.767360
24.391808	1014.953010	15.772378
24.789075	1022.247090	15.777395
24.463966	1017.327529	15.782413
24.838129	1011.840808	15.787431
24.286351	1007.165052	15.792448
24.359306	990.702094	15.797466
24.681376	993.652853	15.802483
24.091345	994.524791	15.807501
24.749101	1007.029410	15.812519
24.827875	1012.486180	15.817536
24.422582	1006.572464	15.822554
24.645684	1008.907558	15.827571
24.877689	1009.253063	15.832589
24.827198	1006.723652	15.837607
24.883299	1004.306931	15.842624
24.350543	992.789438	15.847642
24.749556	993.597935	15.852659
24.853157	1011.166178	15.857677
24.685382	1007.250783	15.862695
24.706263	1013.508745	15.867712
24.817437	1004.815844	15.872730
25.148585	1005.000645	15.877747
24.995583	1014.498523	15.882765
24.851397	1013.201956	15.887783
25.151871	1015.745840	15.892800
24.641434	1007.677361	15.897818
24.926351	1005.641363	15.902835
25.125380	1005.685915	15.907853
25.094306	1003.645777	15.912871
24.955088	1007.590326	15.917888
24.868545	1020.312557	15.922906
25.218266	1003.654742	15.927923
24.932088	1013.842529	15.932941
25.009170	1012.852128	15.937959
25.054438	1013.507762	15.942976
24.968211	1018.330809	15.947994
25.094706	1009.774363	15.953011
24.823740	1008.346178	15.958029
24.984638	1011.344284	15.963047
25.067467	1012.536842	15.968064
25.082013	1019.922444	15.973082
25.207046	1023.907646	15.978099
25.374661	1036.766797	15.983117
25.439402	1038.230440	15.988135
25.525220	1034.726595	15.993152
25.074557	1037.053647	15.998170
25.518670	1041.490643	16.003187
25.343208	1042.262915	16.008205
25.283137	1035.168454	16.013223
25.334752	1036.167085	16.018240
25.312119	1045.032314	16.023258
25.266933	1028.471064	16.028275
25.267001	1032.327521	16.033293
25.592553	1033.873379	16.038311
25.554897	1044.142169	16.043328
25.574763	1057.131783	16.048346
25.763937	1056.369975	16.053363
25.582456	1054.003095	16.058381
25.799031	1054.007027	16.063399
25.459081	1047.991540	16.068416
25.841553	1050.254332	16.073434
25.807795	1043.111563	16.078451
25.487768	1054.955198	16.083469
25.542857	1059.478398	16.088487
25.896196	1040.288970	16.093504
25.595153	1053.489811	16.098522
26.023949	1046.246165	16.103539
26.143308	1043.412420	16.108557
25.815368	1045.647660	16.113575
25.952763	1043.290782	16.118592
25.899844	1056.730466	16.123610
26.417212	1057.858101	16.128627
26.365657	1057.881952	16.133645
26.253457	1046.472106	16.138663
26.148865	1046.135030	16.143680
25.774011	1053.073561	16.148698
26.413088	1052.935555	16.153715
26.392458	1066.556384	16.158733
26.774555	1056.751168	16.163751
26.726053	1048.531398	16.168768
26.244350	1053.088206	16.173786
26.463913	1038.568343	16.178803
26.622196	1035.898918	16.183821
26.326469	1037.611547	16.188839
26.308876	1045.371431	16.193856
26.349302	1042.673133	16.198874
26.467646	1039.946847	16.203891
26.318149	1041.791203	16.208909
26.517165	1041.008918	16.213927
26.450162	1042.007199	16.218944
26.255159	1037.190327	16.223962
26.351030	1046.923790	16.228979
26.358445	1064.298869	16.233997
26.663733	1069.827465	16.239015
26.528989	1064.821260	16.244032
26.643509	1069.316215	16.249050
26.818176	1062.304889	16.254067
26.841831	1068.997947	16.259085
26.892916	1067.210023	16.264103
27.034735	1063.915154	16.269120
26.598807	1063.907708	16.274138
26.885315	1064.680185	16.279155
27.023647	1069.853079	16.284173
26.986515	1066.677767	16.289191
27.205384	1067.867950	16.294208
26.924685	1072.222852	16.299226
27.146629	1064.269978	16.304243
26.964913	1066.220372	16.309261
27.010801	1068.627423	16.314279
26.813073	1074.604070	16.319296
26.926753	1073.298656	16.324314
26.826443	1066.532386	16.329331
26.954485	1072.196054	16.334349
26.579799	1070.033016	16.339367
26.961511	1084.509181	16.344384
27.210994	1091.580286	16.349402
27.430483	1090.248824	16.354419
27.603935	1095.712876	16.359437
27.445876	1091.597119	16.364455
27.447302	1087.393257	16.369472
27.290928	1084.182975	16.374490
27.436467	1088.834025	16.379507
27.461278	1089.369788	16.384525
27.582622	1096.675571	16.389543
27.679019	1082.061358	16.394560
27.630264	1096.788019	16.399578
27.521711	1088.129504	16.404595
27.505253	1095.542086	16.409613
27.657982	1095.432942	16.414631
27.997448	1081.127794	16.419648
26.984509	1081.434821	16.424666
27.518491	1086.315350	16.429683
27.548530	1084.514943	16.434701
27.464842	1081.694070	16.439719
27.462601	1088.031422	16.444736
27.835454	1093.726170	16.449754
27.895395	1088.118240	16.454771
27.979913	1091.065208	16.459789
27.698850	1089.733275	16.464807
27.870234	1080.525963	16.469824
27.802802	1088.580861	16.474842
27.636412	1084.668386	16.479859
27.850448	1080.137718	16.484877
27.779842	1083.639178	16.489895
28.077639	1094.751708	16.494912
27.493452	1097.595161	16.499930
27.683968	1100.137350	16.504947
28.052332	1105.832804	16.509965
28.153654	1114.284162	16.514983
28.153941	1108.938043	16.520000
28.134195	1117.370499	16.525018
27.945250	1106.846819	16.530035
27.784000	1104.410489	16.535053
27.714865	1104.970439	16.540071
28.439080	1108.116993	16.545088
28.648113	1131.119048	16.550106
28.690665	1110.706416	16.555123
28.384829	1106.768447	16.560141
28.056079	1112.538411	16.565159
28.520877	1096.780842	16.570176
28.222352	1105.578872	16.575194
28.490122	1125.450549	16.580211
28.748678	1126.350487	16.585229
28.800537	1121.520162	16.590247
28.745139	1114.481743	16.595264
28.632427	1111.359292	16.600282
28.833180	1101.336305	16.605299
28.552200	1098.341209	16.610317
28.544856	1100.349495	16.615335
28.852902	1102.507188	16.620352
28.647155	1101.220259	16.625370
28.790867	1104.827003	16.630387
28.979456	1100.325563	16.635405
28.917503	1107.893605	16.640423
28.823923	1097.070960	16.645440
28.676136	1099.552541	16.650458
28.860087	1110.310524	16.655475
29.321878	1120.018255	16.660493
28.854654	1114.410859	16.665511
29.270693	1119.016380	16.670528
29.012714	1107.206446	16.675546
28.964547	1108.362730	16.680563
29.302487	1115.281125	16.685581
28.836887	1112.624229	16.690599
29.345100	1114.125696	16.695616
29.123439	1131.628252	16.700634
29.216117	1130.225135	16.705651
29.164820	1127.380245	16.710669
29.242987	1132.556272	16.715687
29.197051	1120.700483	16.720704
29.159174	1136.113455	16.725722
29.121191	1135.709135	16.730739
29.332433	1131.425051	16.735757
29.582154	1127.983873	16.740775
29.705358	1127.724717	16.745792
29.065534	1125.347586	16.750810
29.748938	1133.183876	16.755827
29.687335	1120.816132	16.760845
29.079819	1133.118283	16.765863
29.522094	1121.160756	16.770880
29.650459	1124.899299	16.775898
29.137198	1128.864608	16.780915
29.476618	1117.863652	16.785933
29.405038	1130.151261	16.790951
29.527463	1141.281829	16.795968
29.576835	1145.058001	16.800986
29.559987	1146.625957	16.806003
30.250896	1147.578080	16.811021
29.724203	1154.253254	16.816039
29.731499	1155.195717	16.821056
29.914154	1142.685544	16.826074
29.564672	1148.023255	16.831091
30.209530	1147.250010	16.836109
30.154824	1145.879452	16.841127
30.578898	1146.390531	16.846144
30.104702	1148.096417	16.851162
29.903478	1150.797823	16.856179
30.244339	1146.534454	16.861197
29.895137	1148.107144	16.866215
29.889260	1139.060122	16.871232
30.102617	1147.219379	16.876250
29.633301	1147.504350	16.881267
30.255582	1137.595185	16.886285
30.220730	1140.974286	16.891303
30.330906	1135.781360	16.896320
30.193537	1144.995984	16.901338
30.368387	1146.814779	16.906355
30.326648	1135.753607	16.911373
30.362673	1139.935823	16.916391
30.235295	1145.412309	16.921408
30.225833	1153.581232	16.926426
30.579318	1164.893370	16.931443
30.701932	1162.822823	16.936461
30.687040	1160.906367	16.941479
30.740232	1155.119588	16.946496
30.724851	1167.218532	16.951514
30.595664	1170.113787	16.956531
31.039755	1161.797851	16.961549
30.385890	1153.082728	16.966567
30.749463	1157.472411	16.971584
30.888738	1166.536401	16.976602
30.605404	1174.438966	16.981619
30.776499	1171.373027	16.986637
30.783726	1185.276769	16.991655
30.655809	1156.350936	16.996672
30.820218	1163.877223	17.001690
30.811768	1162.755044	17.006707
31.113877	1165.465956	17.011725
30.882303	1162.182233	17.016743
30.696014	1166.216244	17.021760
30.971124	1177.187209	17.026778
30.856786	1167.911006	17.031795
31.325521	1154.336648	17.036813
30.931197	1170.272569	17.041831
31.245765	1180.341080	17.046848
31.072423	1177.717281	17.051866
31.454539	1185.632358	17.056883
31.637915	1175.529999	17.061901
31.236774	1181.803647	17.066919
31.292162	1177.610245	17.071936
31.498101	1183.296458	17.076954
31.576751	1183.662838	17.081971
31.666926	1187.909166	17.086989
31.340731	1175.519722	17.092007
31.598026	1181.728079	17.097024
31.508575	1191.070923	17.102042
31.722793	1189.389975	17.107059
31.938816	1180.465960	17.112077
31.285664	1171.602389	17.117095
31.619581	1173.752881	17.122112
31.815403	1174.239762	17.127130
31.368207	1185.203977	17.132147
31.876721	1190.817539	17.137165
31.704252	1184.523292	17.142183
31.965984	1181.430526	17.147200
32.044240	1183.226589	17.152218
31.650846	1180.201752	17.157235
32.261603	1174.974567	17.162253
31.858656	1184.000441	17.167271
31.743914	1186.218074	17.172288
32.042028	1174.693364	17.177306
31.684056	1183.327172	17.182323
31.792197	1182.631705	17.187341
31.574047	1181.564471	17.192359
31.834911	1179.992984	17.197376
32.520147	1194.872977	17.202394
32.142553	1204.917400	17.207411
32.176406	1203.611859	17.212429
32.090066	1205.664094	17.217447
32.158545	1211.838926	17.222464
32.363440	1204.011742	17.227482
32.068298	1207.955516	17.232499
32.603191	1202.708651	17.237517
32.400229	1205.246230	17.242535
32.393389	1199.408881	17.247552
32.526504	1196.001738	17.252570
32.612588	1196.461631	17.257587
32.764759	1192.347738	17.262605
32.276406	1197.991253	17.267623
32.657161	1196.662920	17.272640
32.561931	1196.188671	17.277658
32.540220	1205.344178	17.282675
32.733707	1207.510365	17.287693
32.647845	1197.920406	17.292711
32.611124	1201.615401	17.297728
32.572545	1193.210968	17.302746
32.591909	1201.220758	17.307763
32.898706	1194.990276	17.312781
32.767719	1199.558445	17.317799
32.559417	1221.114328	17.322816
33.210493	1211.557227	17.327834
32.926526	1224.140117	17.332851
33.033010	1214.150773	17.337869
33.273969	1226.746098	17.342887
33.174934	1221.270335	17.347904
33.344315	1218.217280	17.352922
33.393007	1228.485270	17.357939
33.579643	1208.021548	17.362957
33.310085	1200.975623	17.367975
33.152175	1193.773348	17.372992
33.243170	1190.183452	17.378010
33.265438	1196.659018	17.383027
33.468251	1200.695192	17.388045
33.453673	1203.064396	17.393063
33.532841	1213.296043	17.398080
33.557125	1221.084158	17.403098
33.407584	1215.739391	17.408115
33.407724	1222.657104	17.413133
33.541706	1224.144629	17.418151
33.683681	1218.621639	17.423168
33.846874	1212.770268	17.428186
33.374530	1216.953254	17.433203
33.560253	1217.337573	17.438221
33.563315	1219.265345	17.443239
33.571414	1220.311830	17.448256
33.688247	1207.578388	17.453274
33.223441	1215.282179	17.458291
33.636391	1203.215579	17.463309
33.782924	1219.997794	17.468327
33.434066	1232.837018	17.473344
33.726263	1239.563807	17.478362
33.805860	1238.465699	17.483379
34.219817	1241.913360	17.488397
34.184844	1239.548748	17.493415
33.728500	1237.379547	17.498432
34.357112	1232.790198	17.503450
34.179518	1228.832108	17.508467
34.365886	1235.408214	17.513485
34.626156	1239.735205	17.518503
34.200972	1244.280050	17.523520
34.628742	1233.356702	17.528538
33.894966	1233.755694	17.533555
34.255928	1236.968654	17.538573
34.390851	1245.979716	17.543591
34.404542	1245.886044	17.548608
34.308494	1233.154378	17.553626
34.628128	1241.009840	17.558643
34.270101	1236.489864	17.563661
34.195119	1239.761658	17.568679
34.035628	1238.284430	17.573696
34.746607	1243.800013	17.578714
34.240462	1252.958859	17.583731
34.679365	1263.156264	17.588749
34.307218	1254.816687	17.593767
34.363742	1253.696945	17.598784
34.756126	1252.202679	17.603802
34.864571	1252.185683	17.608819
34.904718	1249.837703	17.613837
34.845145	1252.854613	17.618855
34.585554	1261.564565	17.623872
34.874133	1236.205801	17.628890
34.787745	1256.732735	17.633907
34.854990	1259.177492	17.638925
35.239568	1267.313134	17.643943
35.039293	1269.174936	17.648960
35.500349	1267.344851	17.653978
35.421909	1268.341780	17.658995
35.715651	1252.535132	17.664013
35.384851	1241.863179	17.669031
34.931094	1247.551783	17.674048
35.167784	1248.811772	17.679066
34.946140	1248.527747	17.684083
35.447224	1262.395199	17.689101
35.577686	1266.436411	17.694119
35.513934	1270.331322	17.699136
35.423414	1274.754310	17.704154
35.512885	1271.436045	17.709171
35.827334	1277.910046	17.714189
35.887000	1275.637902	17.719207
35.837214	1268.270328	17.724224
35.924513	1257.968374	17.729242
35.500694	1242.037469	17.734259
35.685673	1252.249404	17.739277
35.794962	1255.034724	17.744295
35.827302	1272.787965	17.749312
35.888502	1267.233433	17.754330
36.097611	1268.513524	17.759347
35.970132	1264.351909	17.764365
36.278365	1267.869790	17.769383
35.625062	1265.264370	17.774400
36.021541	1263.065694	17.779418
36.258850	1264.372926	17.784435
36.177859	1268.974306	17.789453
36.207778	1262.929197	17.794471
36.192446	1270.868713	17.799488
36.186057	1274.385395	17.804506
36.582457	1273.202934	17.809523
36.585307	1265.511523	17.814541
36.276206	1248.839934	17.819559
36.071403	1262.748553	17.824576
36.340208	1270.100734	17.829594
36.036912	1262.340522	17.834611
35.906340	1268.000589	17.839629
36.411625	1271.332958	17.844647
36.474198	1273.507041	17.849664
36.517439	1260.482123	17.854682
36.506374	1265.015740	17.859699
36.236556	1275.579821	17.864717
36.663239	1270.258369	17.869735
36.018614	1278.293328	17.874752
36.756591	1281.551371	17.879770
36.890525	1297.032240	17.884787
36.682662	1299.318127	17.889805
37.067449	1297.638849	17.894823
36.608824	1305.575248	17.899840
36.534464	1290.930812	17.904858
36.501866	1297.064704	17.909875
36.467495	1293.494430	17.914893
36.734343	1290.441871	17.919911
37.313644	1312.679223	17.924928
37.299185	1297.283756	17.929946
36.995361	1291.644390	17.934963
37.182153	1300.798838	17.939981
37.306057	1304.064730	17.944999
37.181254	1309.938509	17.950016
37.172066	1312.000758	17.955034
37.359729	1313.429386	17.960051
37.132415	1319.562234	17.965069
37.403178	1308.467773	17.970087
37.149926	1319.455334	17.975104
37.396101	1319.918550	17.980122
37.335446	1309.068526	17.985139
37.195825	1313.587582	17.990157
37.181623	1305.371787	17.995175
37.220617	1314.735598	18.000192
37.526454	1321.766405	18.005210
37.596624	1332.043714	18.010227
37.366778	1336.188733	18.015245
37.735740	1339.230037	18.020263
37.948174	1338.994769	18.025280
38.350118	1332.714617	18.030298
37.967132	1332.146588	18.035315
38.100740	1334.814497	18.040333
38.090133	1329.028190	18.045351
37.921675	1335.647302	18.050368
38.160226	1320.581417	18.055386
38.317405	1329.970901	18.060403
38.158149	1333.574665	18.065421
38.035389	1317.621770	18.070439
37.976579	1321.247664	18.075456
38.145484	1321.505228	18.080474
38.066809	1323.183876	18.085491
38.274865	1327.856753	18.090509
37.856643	1336.844070	18.095527
38.036759	1322.374340	18.100544
37.786717	1325.017146	18.105562
38.292102	1328.374758	18.110579
38.367715	1348.926911	18.115597
38.789530	1342.662579	18.120615
38.418127	1354.192556	18.125632
38.455026	1339.104599	18.130650
38.582302	1345.033571	18.135667
38.352137	1345.325257	18.140685
38.777610	1342.219434	18.145703
38.597704	1339.883827	18.150720
38.385670	1343.884041	18.155738
39.067290	1344.881815	18.160755
38.699080	1344.040061	18.165773
38.730579	1341.033836	18.170791
39.023823	1351.456092	18.175808
38.846028	1336.777330	18.180826
39.061094	1343.462592	18.185843
38.627665	1343.104446	18.190861
39.042365	1350.645248	18.195879
39.039677	1363.433484	18.200896
39.225539	1369.747777	18.205914
39.347552	1368.463127	18.210931
39.223022	1374.643008	18.215949
39.517741	1366.299887	18.220967
39.528752	1362.804542	18.225984
39.536538	1362.765446	18.231002
39.733900	1365.104621	18.236019
39.078756	1362.310119	18.241037
39.601462	1360.101122	18.246055
39.397691	1363.601408	18.251072
39.567022	1363.009961	18.256090
39.445134	1360.059324	18.261107
39.536431	1366.129645	18.266125
39.376880	1361.985655	18.271143
39.504966	1364.799606	18.276160
39.411821	1365.278116	18.281178
39.363812	1354.356652	18.286195
39.377607	1370.301394	18.291213
39.405677	1372.443024	18.296231
39.747399	1384.659741	18.301248
39.768831	1386.398452	18.306266
39.775690	1381.161680	18.311283
39.844018	1394.055581	18.316301
40.212992	1384.043951	18.321319
40.040642	1377.282539	18.326336
40.109278	1378.874993	18.331354
40.025412	1386.443430	18.336371
40.197666	1386.634196	18.341389
40.275836	1383.264030	18.346407
40.598957	1387.158315	18.351424
40.141695	1379.955528	18.356442
40.343282	1376.837437	18.361459
40.266426	1368.249562	18.366477
40.432737	1372.203127	18.371495
40.242569	1379.917610	18.376512
40.373173	1399.924697	18.381530
40.614171	1398.567752	18.386547
40.625845	1406.783975	18.391565
40.916905	1409.824873	18.396583
41.040389	1413.081384	18.401600
40.659809	1411.108583	18.406618
41.013742	1399.975787	18.411635
40.588954	1410.968188	18.416653
40.876913	1403.323571	18.421671
40.989180	1407.213025	18.426688
40.886226	1408.071785	18.431706
41.223659	1398.519544	18.436723
40.899412	1403.149603	18.441741
41.133892	1405.637609	18.446759
40.888064	1396.637520	18.451776
40.845546	1397.388976	18.456794
41.191741	1393.825331	18.461811
40.936218	1397.803967	18.466829
41.367572	1401.327832	18.471847
41.321048	1399.618287	18.476864
41.252473	1396.911766	18.481882
41.431720	1396.154656	18.486899
41.178411	1398.482391	18.491917
41.275555	1391.792363	18.496935
41.263865	1405.699240	18.501952
41.195210	1418.327430	18.506970
41.501933	1426.166061	18.511987
41.645921	1424.751727	18.517005
41.666281	1420.939312	18.522023
41.806477	1418.345251	18.527040
41.613350	1419.577917	18.532058
41.867547	1416.618841	18.537075
41.433109	1430.235351	18.542093
41.836941	1423.187979	18.547111
41.854638	1425.343864	18.552128
42.030813	1428.169226	18.557146
41.854603	1415.229073	18.562163
41.585672	1423.577635	18.567181
42.065854	1430.552766	18.572199
42.235219	1436.522514	18.577216
41.966715	1448.932718	18.582234
42.207257	1454.263287	18.587251
41.937192	1457.824473	18.592269
42.194471	1441.862419	18.597287
41.826273	1446.328955	18.602304
42.003989	1443.719544	18.607322
42.754325	1437.911814	18.612339
42.288015	1452.211861	18.617357
42.017631	1439.740902	18.622375
42.578779	1431.627418	18.627392
42.317636	1439.573962	18.632410
42.793858	1447.632209	18.637427
42.959224	1472.288949	18.642445
42.683954	1455.693921	18.647463
42.655363	1455.095609	18.652480
42.889933	1470.447248	18.657498
42.984056	1462.959212	18.662515
42.702145	1468.624117	18.667533
42.513553	1471.897974	18.672551
42.927151	1465.628575	18.677568
42.969841	1470.381050	18.682586
43.126504	1465.420597	18.687603
43.023063	1465.755549	18.692621
42.963991	1466.055146	18.697639
42.832253	1466.340880	18.702656
42.665267	1469.153739	18.707674
42.910239	1466.265532	18.712691
43.287475	1476.933490	18.717709
43.264051	1485.666512	18.722727
43.176506	1489.262227	18.727744
43.478925	1484.127447	18.732762
43.800721	1487.475982	18.737779
44.035533	1485.889616	18.742797
43.651363	1490.443875	18.747815
43.838874	1483.850113	18.752832
43.577749	1482.139468	18.757850
43.623457	1468.457575	18.762867
43.261173	1484.174149	18.767885
43.799182	1490.711036	18.772903
43.639202	1484.853403	18.777920
43.858973	1487.697191	18.782938
43.794938	1480.183433	18.787955
43.754177	1483.831780	18.792973
43.619788	1481.937169	18.797991
43.837861	1480.697424	18.803008
43.786340	1486.414604	18.808026
44.024147	1490.379086	18.813043
43.970027	1504.500980	18.818061
44.057217	1507.463379	18.823079
44.284210	1502.703346	18.828096
44.011017	1510.806451	18.833114
44.414670	1501.347927	18.838131
44.416712	1509.164900	18.843149
44.384070	1497.003807	18.848167
44.527868	1498.111103	18.853184
44.282574	1504.492996	18.858202
44.303188	1503.593470	18.863219
44.439310	1502.098307	18.868237
44.375594	1517.244244	18.873255
44.537398	1521.668786	18.878272
44.748554	1530.415572	18.883290
45.052451	1515.061561	18.888307
44.893736	1523.771615	18.893325
44.907065	1522.907945	18.898343
44.924283	1518.325948	18.903360
45.074834	1524.311297	18.908378
45.104180	1525.613260	18.913395
44.963000	1518.916342	18.918413
45.044125	1522.466701	18.923431
45.513343	1515.049270	18.928448
44.882697	1522.851762	18.933466
45.073373	1522.329552	18.938483
45.051779	1517.996646	18.943501
45.070422	1522.964351	18.948519
45.344389	1518.307413	18.953536
45.321114	1522.467449	18.958554
45.319609	1518.996127	18.963571
45.529261	1514.721669	18.968589
45.597160	1525.700067	18.973607
45.519768	1518.393523	18.978624
45.547172	1526.998675	18.983642
45.733543	1518.416826	18.988659
45.541447	1517.364424	18.993677
45.762277	1540.538737	18.998695
45.953193	1532.697819	19.003712
45.804480	1544.486532	19.008730
46.230151	1541.658369	19.013747
46.150125	1524.442521	19.018765
45.792377	1527.231626	19.023783
46.108781	1527.478708	19.028800
45.884599	1549.128995	19.033818
46.076987	1540.483074	19.038835
46.132285	1537.974884	19.043853
46.134831	1547.776894	19.048871
46.746983	1545.623292	19.053888
46.324442	1545.683177	19.058906
46.070268	1540.323146	19.063923
46.263965	1545.945118	19.068941
46.174724	1535.831618	19.073959
46.930287	1534.135254	19.078976
46.379269	1543.200286	19.083994
46.504232	1539.658650	19.089011
46.451997	1545.521136	19.094029
46.481007	1548.991299	19.099047
46.783332	1538.068485	19.104064
46.487228	1547.525947	19.109082
46.780233	1539.211417	19.114099
46.745702	1551.774392	19.119117
46.702143	1561.659376	19.124135
46.843414	1565.260283	19.129152
46.892176	1574.969856	19.134170
47.036955	1570.058576	19.139187
46.673224	1566.426235	19.144205
46.466957	1564.003206	19.149223
47.009794	1574.796764	19.154240
47.216746	1576.780997	19.159258
47.410345	1596.068341	19.164275
47.522731	1591.603967	19.169293
47.195214	1593.346875	19.174311
47.230774	1586.281395	19.179328
47.226863	1588.904613	19.184346
47.429201	1589.216906	19.189363
47.211344	1592.230269	19.194381
47.380884	1589.738888	19.199399
47.694887	1584.532834	19.204416
47.419972	1588.375687	19.209434
47.476629	1591.058846	19.214451
48.015758	1600.082502	19.219469
48.026306	1610.552358	19.224487
47.833015	1595.213056	19.229504
47.878382	1599.315016	19.234522
47.979383	1598.383955	19.239539
48.226289	1607.459710	19.244557
48.249120	1608.327176	19.249575
47.888101	1607.389603	19.254592
48.295946	1612.435217	19.259610
48.312090	1615.560252	19.264627
48.187880	1608.478768	19.269645
48.119388	1609.874966	19.274663
47.966052	1597.347686	19.279680
48.319010	1604.863555	19.284698
48.241468	1608.757544	19.289715
48.387766	1602.091297	19.294733
48.401445	1616.559282	19.299751
48.568801	1596.849258	19.304768
48.421931	1606.229718	19.309786
48.447574	1604.464663	19.314803
48.555717	1616.610833	19.319821
48.745283	1636.271257	19.324839
48.837784	1630.323523	19.329856
48.831142	1630.286687	19.334874
48.745033	1626.945370	19.339891
49.013690	1629.500641	19.344909
48.489369	1628.336173	19.349927
48.855022	1624.144551	19.354944
48.831685	1624.151358	19.359962
48.826699	1631.275171	19.364979
49.629641	1636.590268	19.369997
49.216246	1651.904720	19.375015
49.592405	1650.646507	19.380032
49.736813	1654.603567	19.385050
49.560294	1639.703437	19.390067
49.343481	1625.447139	19.395085
49.315962	1637.665074	19.400103
49.736247	1637.715991	19.405120
49.971428	1646.092976	19.410138
49.774456	1649.655372	19.415155
49.934035	1640.156117	19.420173
49.653119	1644.236620	19.425191
49.787843	1642.552306	19.430208
49.954482	1646.935095	19.435226
49.652879	1639.379591	19.440243
50.151619	1643.906017	19.445261
49.721711	1648.852511	19.450279
49.978160	1639.274960	19.455296
49.874763	1651.056643	19.460314
49.825869	1657.502498	19.465331
50.161511	1652.204666	19.470349
50.297821	1646.922286	19.475367
50.107119	1643.928731	19.480384
50.065449	1645.759410	19.485402
50.231338	1660.405566	19.490419
50.604639	1658.882698	19.495437
50.044430	1668.138591	19.500455
50.349434	1661.273877	19.505472
50.340489	1665.201315	19.510490
50.304643	1664.575729	19.515507
50.591168	1665.812161	19.520525
50.491469	1685.161335	19.525543
50.835743	1691.886448	19.530560
50.823283	1692.582712	19.535578
50.758208	1696.121297	19.540595
50.990707	1689.343676	19.545613
50.868962	1693.146773	19.550631
51.329845	1686.607942	19.555648
51.178638	1689.696090	19.560666
50.946769	1687.807261	19.565683
51.114988	1673.642087	19.570701
50.916473	1689.052299	19.575719
51.087820	1683.379389	19.580736
51.318941	1689.831880	19.585754
51.153285	1700.657618	19.590771
51.398329	1702.137251	19.595789
51.282771	1706.602139	19.600807
51.514669	1707.228559	19.605824
51.519978	1713.640694	19.610842
51.411230	1703.205088	19.615859
51.749715	1703.556017	19.620877
51.465666	1696.370146	19.625895
51.814028	1697.915646	19.630912
51.889032	1698.749694	19.635930
51.901231	1693.092248	19.640947
51.624063	1698.649178	19.645965
51.764711	1713.763262	19.650983
51.799966	1724.197754	19.656000
52.228447	1727.747384	19.661018
51.905584	1732.563513	19.666035
52.406500	1731.468797	19.671053
52.311477	1731.843462	19.676071
52.620493	1725.726066	19.681088
52.528495	1732.450117	19.686106
52.223456	1727.909089	19.691123
52.318972	1726.196194	19.696141
52.282152	1729.440007	19.701159
52.374254	1719.380046	19.706176
52.529325	1725.740318	19.711194
52.482145	1732.391070	19.716211
52.639813	1733.988543	19.721229
52.744509	1745.551482	19.726247
52.771003	1750.208733	19.731264
53.154501	1748.179300	19.736282
52.902649	1755.042020	19.741299
52.978335	1747.673527	19.746317
52.781642	1744.257990	19.751335
52.914228	1743.006374	19.756352
53.308297	1736.294945	19.761370
53.058454	1735.077998	19.766387
53.182741	1743.371411	19.771405
53.135957	1749.870621	19.776423
53.468070	1737.535445	19.781440
53.394297	1748.422560	19.786458
53.222079	1773.220973	19.791475
53.572472	1777.123696	19.796493
53.462051	1779.650013	19.801511
53.516978	1772.972770	19.806528
53.764933	1768.635443	19.811546
53.586090	1775.262656	19.816563
53.661242	1769.390182	19.821581
54.045190	1766.464373	19.826599
53.781299	1770.043589	19.831616
54.363456	1769.144438	19.836634
54.156593	1783.287327	19.841651
54.207874	1766.801803	19.846669
54.273277	1773.801028	19.851687
54.414471	1767.946611	19.856704
54.530837	1778.829203	19.861722
54.224927	1777.734653	19.866739
54.375363	1774.346780	19.871757
54.178966	1769.908648	19.876775
54.370451	1778.046373	19.881792
54.574750	1772.314620	19.886810
54.213131	1776.827546	19.891827
54.408738	1767.316266	19.896845
54.329741	1790.572594	19.901863
54.447307	1793.072661	19.906880
54.768383	1789.989431	19.911898
55.047247	1798.653152	19.916915
55.055683	1792.828995	19.921933
54.884490	1794.840938	19.926951
54.821681	1800.257011	19.931968
54.826684	1788.257091	19.936986
54.785012	1794.793388	19.942003
55.100133	1795.927513	19.947021
54.903194	1806.038646	19.952039
55.370265	1816.642237	19.957056
55.677602	1809.619302	19.962074
55.256595	1821.321462	19.967091
55.467277	1819.284382	19.972109
55.635277	1823.092607	19.977127
55.258476	1822.482562	19.982144
55.425780	1806.947718	19.987162
55.465799	1820.253486	19.992179
55.279454	1810.672630	19.997197
55.776111	1812.554692	20.002215
55.797244	1812.971125	20.007232
55.932268	1813.473862	20.012250
55.600203	1817.016428	20.017267
55.611954	1818.027660	20.022285
55.595533	1832.418479	20.027303
55.745434	1835.658305	20.032320
55.738286	1828.937114	20.037338
55.773590	1834.785979	20.042355
55.708258	1838.406688	20.047373
55.600053	1854.026969	20.052391
55.786789	1861.619486	20.057408
56.341426	1855.495123	20.062426
56.165899	1861.683162	20.067443
56.298363	1871.796376	20.072461
56.773368	1879.365828	20.077479
56.764171	1881.232471	20.082496
57.139964	1878.169057	20.087514
56.838209	1886.712337	20.092531
57.105491	1862.113470	20.097549
57.172563	1861.714766	20.102567
56.949999	1863.861007	20.107584
57.161329	1855.401327	20.112602
57.285480	1862.047377	20.117619
57.156596	1848.910135	20.122637
57.136564	1851.924106	20.127655
57.264286	1856.344603	20.132672
57.318077	1867.546342	20.137690
57.035935	1880.896318	20.142707
57.547213	1880.907732	20.147725
57.535165	1866.243595	20.152743
57.631395	1880.209676	20.157760
57.566607	1881.245528	20.162778
57.805841	1881.107048	20.167795
57.794315	1879.508746	20.172813
57.974703	1873.080071	20.177831
58.041522	1880.457838	20.182848
57.869690	1871.130313	20.187866
57.508857	1875.554772	20.192883
57.264546	1874.592586	20.197901
57.875303	1872.095159	20.202919
57.617126	1871.075182	20.207936
58.146895	1885.838092	20.212954
58.104415	1896.338515	20.217971
58.267346	1901.312124	20.222989
58.481440	1891.816818	20.228007
58.599015	1901.357985	20.233024
58.533229	1897.120279	20.238042
58.108060	1899.178338	20.243059
58.340324	1905.927394	20.248077
58.748927	1890.051695	20.253095
58.758566	1903.409624	20.258112
58.665119	1897.847566	20.263130
58.759713	1901.405359	20.268147
58.400172	1903.241682	20.273165
58.726630	1896.035823	20.278183
58.695852	1905.792753	20.283200
59.133298	1914.744132	20.288218
59.044731	1926.567856	20.293235
59.150170	1923.613069	20.298253
59.243532	1924.718826	20.303271
59.070958	1930.767561	20.308288
59.358399	1916.520396	20.313306
59.261062	1913.821458	20.318323
59.049014	1922.076125	20.323341
59.268805	1922.780195	20.328359
59.107571	1919.188643	20.333376
59.223540	1915.481073	20.338394
59.538075	1920.579268	20.343411
59.356011	1930.858566	20.348429
59.517310	1937.388363	20.353447
59.558861	1947.632636	20.358464
59.902167	1946.281715	20.363482
60.012536	1942.871683	20.368499
59.649992	1942.802238	20.373517
60.274492	1945.967726	20.378535
59.526288	1949.373530	20.383552
60.042531	1952.294030	20.388570
60.010464	1966.977763	20.393587
60.117529	1970.391594	20.398605
60.350186	1972.939930	20.403623
60.254958	1976.710529	20.408640
60.248222	1959.116681	20.413658
60.175499	1961.271016	20.418675
60.265064	1960.780417	20.423693
60.560279	1973.740181	20.428711
60.440760	1992.316405	20.433728
60.552086	1989.348061	20.438746
60.926382	1991.858429	20.443763
60.572784	1990.351584	20.448781
60.938116	1993.049563	20.453799
60.572588	1991.888595	20.458816
60.964002	1986.884908	20.463834
61.377758	1997.481180	20.468851
61.342410	2000.557540	20.473869
61.638655	1999.917785	20.478887
61.329274	1998.047379	20.483904
61.545280	1985.588202	20.488922
61.442338	1988.539441	20.493939
61.765461	1996.135895	20.498957
61.767219	1996.186111	20.503975
61.771724	1989.671334	20.508992
61.726134	1989.075667	20.514010
61.514650	1998.337057	20.519027
61.518873	2005.213405	20.524045
62.045829	1986.718499	20.529063
62.192841	1998.953519	20.534080
62.187161	1992.714912	20.539098
62.086358	1992.456124	20.544115
62.252060	2007.500254	20.549133
62.115014	1994.219006	20.554151
62.453548	1997.290441	20.559168
62.202330	1993.883399	20.564186
62.087902	1990.732657	20.569203
61.983122	1995.221177	20.574221
62.327742	1987.188710	20.579239
61.935838	1991.958917	20.584256
62.203852	2020.207683	20.589274
62.372244	2019.610051	20.594291
62.194836	2033.183589	20.599309
62.535211	2030.864214	20.604327
62.745100	2044.538040	20.609344
62.944439	2041.047774	20.614362
63.267504	2049.193412	20.619379
63.203724	2050.775112	20.624397
63.376459	2051.325601	20.629415
63.382552	2044.201437	20.634432
63.550260	2049.464695	20.639450
63.502247	2046.445560	20.644467
63.290571	2036.846459	20.649485
63.084692	2028.054403	20.654503
63.089682	2044.938470	20.659520
63.597423	2036.025135	20.664538
63.556770	2035.387666	20.669555
63.048005	2038.730724	20.674573
63.632158	2037.746035	20.679591
63.439907	2048.724484	20.684608
63.349018	2050.013763	20.689626
63.848603	2062.969976	20.694643
63.674737	2064.540520	20.699661
63.650918	2066.362133	20.704679
63.897177	2067.153587	20.709696
63.664105	2072.343934	20.714714
64.022776	2077.258519	20.719731
64.288995	2084.519916	20.724749
64.344339	2092.404538	20.729767
64.172093	2089.452201	20.734784
64.208909	2089.714692	20.739802
64.376625	2090.045044	20.744819
64.421618	2092.338755	20.749837
64.574740	2086.586516	20.754855
64.553204	2106.716068	20.759872
64.744163	2103.100860	20.764890
64.945874	2105.133315	20.769907
64.879905	2115.580738	20.774925
65.326217	2112.171694	20.779943
65.196227	2125.605318	20.784960
65.339111	2120.236556	20.789978
65.377981	2108.268989	20.794995
65.342225	2116.006935	20.800013
65.323343	2105.389744	20.805031
65.163085	2110.739120	20.810048
65.464266	2110.714020	20.815066
65.436081	2106.517714	20.820083
65.313802	2113.934672	20.825101
65.704879	2103.638292	20.830119
65.896840	2124.958966	20.835136
65.818880	2125.611855	20.840154
66.017659	2135.645395	20.845171
66.135219	2135.604878	20.850189
66.160258	2124.365362	20.855207
66.065369	2127.451073	20.860224
65.945886	2126.709176	20.865242
66.288470	2127.681217	20.870259
65.894970	2130.068882	20.875277
66.119029	2129.519334	20.880295
66.175749	2132.944240	20.885312
65.844402	2133.946123	20.890330
66.542308	2134.635259	20.895347
66.858289	2146.487272	20.900365
66.877171	2146.490620	20.905383
66.786263	2158.930297	20.910400
66.637665	2151.218050	20.915418
67.071359	2144.408736	20.920435
66.944313	2161.998467	20.925453
66.885181	2151.289717	20.930471
67.343197	2156.763164	20.935488
67.052380	2154.514260	20.940506
67.232695	2159.579899	20.945523
66.772259	2152.822299	20.950541
67.192897	2153.955697	20.955559
67.008881	2153.375401	20.960576
67.021707	2158.864945	20.965594
66.932479	2176.066880	20.970611
66.878131	2172.676300	20.975629
66.928371	2174.524194	20.980647
67.114394	2185.276188	20.985664
67.220756	2197.157920	20.990682
67.655180	2205.352460	20.995699
67.696429	2205.516420	21.000717
67.915293	2212.368686	21.005735
67.912129	2213.710510	21.010752
67.997431	2218.974104	21.015770
68.535469	2222.601353	21.020787
68.203124	2230.294289	21.025805
68.202426	2233.330543	21.030823
68.450990	2226.105197	21.035840
68.034943	2233.602947	21.040858
68.610859	2228.387234	21.045875
68.654083	2218.400931	21.050893
68.647297	2218.222092	21.055911
68.852630	2226.913322	21.060928
68.455337	2221.057911	21.065946
68.588993	2220.680328	21.070963
68.579961	2225.422171	21.075981
69.153914	2231.830613	21.080999
69.077807	2248.014303	21.086016
69.098433	2249.235627	21.091034
69.630319	2248.284365	21.096051
68.915561	2245.650550	21.101069
69.169963	2239.576254	21.106087
69.484754	2243.768706	21.111104
69.069621	2246.014595	21.116122
69.763414	2243.838656	21.121139
69.447124	2246.138492	21.126157
69.485154	2242.051712	21.131175
69.197184	2257.403836	21.136192
69.475045	2257.000503	21.141210
69.991966	2258.620641	21.146227
69.950767	2261.637997	21.151245
69.949482	2271.406285	21.156263
69.953232	2265.333378	21.161280
69.997763	2269.410374	21.166298
70.636250	2257.708557	21.171315
70.302402	2274.387128	21.176333
70.348082	2269.964597	21.181351
70.647920	2282.261082	21.186368
70.273648	2294.489605	21.191386
70.898920	2279.507508	21.196403
70.790784	2286.635118	21.201421
70.633563	2292.100847	21.206439
70.967624	2292.603976	21.211456
70.467949	2288.844448	21.216474
70.916991	2284.065201	21.221491
71.237087	2286.631445	21.226509
71.034464	2289.052346	21.231527
71.276488	2284.438090	21.236544
70.668786	2287.013983	21.241562
71.101365	2289.935023	21.246579
71.339012	2304.336911	21.251597
71.274435	2304.299682	21.256615
71.561943	2301.284747	21.261632
71.406390	2312.604777	21.266650
71.487078	2308.927903	21.271667
71.488302	2310.044963	21.276685
71.447432	2307.700070	21.281703
71.677453	2315.336496	21.286720
71.606050	2341.350775	21.291738
71.973894	2331.155745	21.296755
71.701574	2335.295022	21.301773
72.072139	2330.988849	21.306791
71.994370	2329.331451	21.311808
72.049022	2323.427291	21.316826
72.048888	2337.948519	21.321843
72.149316	2347.382147	21.326861
72.107380	2350.803615	21.331879
72.366329	2350.182316	21.336896
72.316175	2353.150593	21.341914
72.414401	2345.611050	21.346931
72.895142	2360.602962	21.351949
73.105483	2362.921299	21.356967
73.273816	2366.950516	21.361984
72.969696	2356.229529	21.367002
73.151719	2362.166042	21.372019
72.848196	2372.057484	21.377037
72.916923	2372.422288	21.382055
73.356625	2374.789907	21.387072
73.282441	2376.436388	21.392090
73.420720	2376.439967	21.397107
73.355559	2380.562579	21.402125
73.125687	2370.991398	21.407143
73.392465	2380.793494	21.412160
73.610508	2396.142204	21.417178
73.944292	2392.933793	21.422195
73.970336	2393.368407	21.427213
73.811540	2401.337212	21.432231
74.314656	2404.079945	21.437248
73.817912	2400.853317	21.442266
74.196369	2394.453391	21.447283
74.637840	2398.206269	21.452301
74.278982	2394.127982	21.457319
74.350904	2395.372840	21.462336
74.454450	2404.130602	21.467354
74.697760	2396.738736	21.472371
74.213105	2403.751796	21.477389
74.519771	2422.072326	21.482407
74.790948	2414.316290	21.487424
74.604716	2416.015047	21.492442
74.579563	2417.082593	21.497459
74.806716	2417.634036	21.502477
75.052976	2420.590601	21.507495
75.122214	2419.721285	21.512512
75.101236	2442.581164	21.517530
75.336107	2445.656295	21.522547
75.285690	2442.309233	21.527565
75.483104	2440.984290	21.532583
75.686957	2441.106996	21.537600
75.540162	2441.104741	21.542618
75.671083	2434.450063	21.547635
75.538245	2438.172996	21.552653
75.321854	2437.335805	21.557671
75.568130	2437.268809	21.562688
75.736356	2466.957322	21.567706
75.729782	2461.009056	21.572723
75.636353	2461.806406	21.577741
75.605178	2470.001424	21.582759
76.080739	2472.066763	21.587776
76.381871	2489.062657	21.592794
76.556817	2486.500872	21.597811
76.394642	2487.327931	21.602829
76.513034	2483.926010	21.607847
76.682746	2478.789648	21.612864
76.781508	2493.270258	21.617882
76.702191	2484.656984	21.622899
76.757878	2486.305220	21.627917
76.909703	2499.840153	21.632935
77.240065	2508.404623	21.637952
77.134365	2517.709672	21.642970
77.391928	2504.479842	21.647987
77.498931	2509.320357	21.653005
77.275021	2504.917913	21.658023
77.526868	2506.541730	21.663040
77.525511	2509.186775	21.668058
77.352642	2506.171343	21.673075
77.761262	2506.160973	21.678093
77.673686	2505.085823	21.683111
77.820443	2506.098036	21.688128
77.714753	2501.913780	21.693146
78.097525	2505.713752	21.698163
77.769471	2501.583272	21.703181
77.423290	2509.979155	21.708199
78.144579	2512.731910	21.713216
78.054744	2526.008047	21.718234
77.967103	2527.199011	21.723251
78.201319	2532.660296	21.728269
77.716047	2534.260732	21.733287
78.338878	2533.187901	21.738304
77.925780	2550.564024	21.743322
78.599219	2549.398047	21.748339
78.471821	2550.787765	21.753357
78.713453	2564.078277	21.758375
79.216256	2569.185036	21.763392
79.072251	2569.797790	21.768410
79.009540	2570.085350	21.773427
78.701466	2575.590581	21.778445
78.983998	2576.136509	21.783463
79.334897	2567.149647	21.788480
79.137148	2571.564503	21.793498
79.260318	2590.037043	21.798515
79.572590	2599.942596	21.803533
80.046970	2601.610461	21.808551
79.779819	2591.754638	21.813568
79.991367	2611.983951	21.818586
79.870847	2594.700829	21.823603
80.298054	2603.704657	21.828621
80.198815	2588.968374	21.833639
80.076237	2593.971126	21.838656
80.319673	2597.032316	21.843674
79.998384	2592.405240	21.848691
80.379629	2586.225740	21.853709
80.267125	2604.006148	21.858727
80.369467	2611.757388	21.863744
80.494874	2616.778105	21.868762
80.525469	2623.716836	21.873779
81.014701	2610.652627	21.878797
80.624651	2616.341145	21.883815
80.620592	2613.059380	21.888832
80.746452	2622.091493	21.893850
81.010022	2636.836764	21.898867
80.799658	2635.263235	21.903885
80.971542	2641.397111	21.908903
81.539386	2638.934713	21.913920
81.335205	2637.180314	21.918938
81.529895	2637.042497	21.923955
81.390953	2649.758311	21.928973
81.432428	2655.461294	21.933991
81.667697	2647.922247	21.939008
81.967694	2659.082749	21.944026
82.042659	2668.571033	21.949043
81.924918	2665.180824	21.954061
82.051639	2664.154150	21.959079
82.274572	2657.557567	21.964096
82.229992	2669.684191	21.969114
82.117084	2666.249038	21.974131
82.618447	2672.542767	21.979149
82.207103	2682.116718	21.984167
82.439437	2677.671156	21.989184
82.279208	2691.696986	21.994202
82.528300	2684.092635	21.999219
82.777013	2686.439721	22.004237
82.605091	2688.578123	22.009255
82.854086	2696.773536	22.014272
83.105641	2705.195795	22.019290
83.082294	2707.781190	22.024307
82.913603	2710.723911	22.029325
83.077218	2713.090645	22.034343
82.835106	2709.375891	22.039360
83.239929	2707.147332	22.044378
83.212186	2720.233982	22.049395
83.678468	2724.008292	22.054413
83.287089	2733.411865	22.059431
83.764790	2728.031497	22.064448
83.923117	2726.864153	22.069466
83.706362	2731.439834	22.074483
83.644472	2723.881032	22.079501
83.781485	2744.819686	22.084519
83.749455	2743.817880	22.089536
84.354274	2755.290489	22.094554
84.305815	2759.139139	22.099571
84.251619	2756.076668	22.104589
84.314951	2773.652949	22.109607
84.581317	2784.099190	22.114624
84.792353	2778.426031	22.119642
84.774630	2780.022672	22.124659
85.257914	2776.737117	22.129677
84.896042	2788.481135	22.134695
85.193409	2777.119641	22.139712
85.379175	2770.677180	22.144730
85.158670	2779.968789	22.149747
85.234103	2764.365453	22.154765
85.249136	2778.913066	22.159783
85.576141	2787.380354	22.164800
86.031339	2802.215673	22.169818
85.508920	2792.980469	22.174835
85.679984	2804.397976	22.179853
85.412687	2801.873872	22.184871
86.049305	2795.723727	22.189888
85.731595	2789.906159	22.194906
85.606288	2795.657409	22.199923
86.302543	2808.775879	22.204941
86.332216	2822.049291	22.209959
86.324108	2828.148307	22.214976
86.335472	2819.034613	22.219994
86.296746	2819.450979	22.225011
86.585802	2810.606246	22.230029
86.168283	2827.595117	22.235047
86.695157	2838.262539	22.240064
86.982744	2840.265843	22.245082
86.677326	2850.697551	22.250099
87.219440	2842.217147	22.255117
87.260945	2844.656686	22.260135
87.108787	2843.389638	22.265152
87.782031	2842.463545	22.270170
87.118372	2845.247121	22.275187
87.238976	2839.357709	22.280205
87.462637	2858.682732	22.285223
87.415827	2862.654238	22.290240
87.578141	2860.574121	22.295258
87.689359	2874.955245	22.300275
88.071087	2858.435887	22.305293
87.726815	2868.106737	22.310311
87.670711	2868.857227	22.315328
87.795002	2886.383037	22.320346
87.904504	2884.740435	22.325363
88.348714	2889.278882	22.330381
88.311672	2895.521326	22.335399
88.625025	2897.949843	22.340416
88.620795	2890.306189	22.345434
88.519342	2896.022172	22.350451
89.016083	2907.745370	22.355469
89.041028	2920.644008	22.360487
88.556459	2912.444360	22.365504
88.697429	2918.633673	22.370522
89.094980	2926.057896	22.375539
89.168190	2914.690404	22.380557
88.938449	2922.133999	22.385575
88.944486	2926.239268	22.390592
89.485309	2942.803513	22.395610
89.670069	2940.947117	22.400627
89.570135	2937.639284	22.405645
89.305377	2935.155794	22.410663
89.624191	2935.645551	22.415680
89.687186	2934.871874	22.420698
89.716535	2955.852891	22.425715
89.772057	2958.479621	22.430733
89.819493	2967.445289	22.435751
90.010820	2959.938246	22.440768
90.142417	2964.992809	22.445786
90.243769	2982.004687	22.450803
90.655592	2979.064851	22.455821
90.809093	2985.851905	22.460839
90.817839	2996.726846	22.465856
91.036829	2978.793640	22.470874
90.660908	2990.606270	22.475891
90.933596	2976.666734	22.480909
91.137403	2991.023976	22.485927
91.177305	3004.368513	22.490944
91.317449	3004.943076	22.495962
91.352161	2998.735666	22.500979
91.658382	3006.672914	22.505997
91.502825	3000.438501	22.511015
91.534707	3007.374022	22.516032
92.154663	2993.111788	22.521050
91.599022	3008.809483	22.526067
91.606928	3003.404794	22.531085
91.701759	3025.549745	22.536103
92.047657	3024.902178	22.541120
92.207052	3022.469004	22.546138
91.935946	3028.827071	22.551155
92.056505	3026.027547	22.556173
92.135399	3029.376557	22.561191
92.367507	3047.213878	22.566208
92.251793	3044.031590	22.571226
92.668825	3051.635874	22.576243
92.364932	3049.161656	22.581261
92.228519	3066.854735	22.586279
92.802403	3064.994175	22.591296
93.007298	3070.337125	22.596314
92.683524	3087.529332	22.601331
92.824965	3086.367768	22.606349
93.602924	3096.910788	22.611367
93.445771	3089.802318	22.616384
93.951111	3091.837816	22.621402
93.827404	3099.722525	22.626419
93.714631	3093.651814	22.631437
93.868318	3099.643511	22.636455
94.185446	3094.755315	22.641472
93.896640	3099.733750	22.646490
93.912850	3124.757001	22.651507
94.194034	3116.711880	22.656525
94.718750	3114.849550	22.661543
94.228155	3121.238880	22.666560
94.424615	3114.592622	22.671578
94.649485	3116.337504	22.676595
94.805602	3117.471378	22.681613
94.963055	3115.505619	22.686631
94.969735	3110.413558	22.691648
95.076755	3103.696099	22.696666
94.972337	3123.672491	22.701683
95.140167	3133.023377	22.706701
95.274980	3129.088514	22.711719
95.149751	3140.016094	22.716736
95.410685	3132.491762	22.721754
95.342163	3132.846522	22.726771
95.519540	3125.029129	22.731789
95.771625	3140.335266	22.736807
95.624724	3147.570288	22.741824
96.105980	3150.319721	22.746842
95.758665	3169.469408	22.751859
95.781831	3163.049126	22.756877
95.949518	3157.294266	22.761895
95.804514	3162.016626	22.766912
96.351192	3174.180362	22.771930
96.248911	3189.882935	22.776947
96.760286	3186.062657	22.781965
96.760722	3195.812239	22.786983
96.543128	3196.262949	22.792000
97.015455	3191.432475	22.797018
96.836564	3190.377903	22.802035
96.893958	3194.610906	22.807053
97.026102	3205.637077	22.812071
96.939521	3222.864845	22.817088
96.999778	3216.454515	22.822106
97.333196	3211.923548	22.827123
97.263968	3228.653071	22.832141
97.640486	3235.847155	22.837159
97.566381	3243.730468	22.842176
97.984778	3232.163508	22.847194
98.110728	3238.901318	22.852211
97.847949	3242.272335	22.857229
97.850910	3251.248268	22.862247
98.078065	3259.762985	22.867264
98.162514	3262.268446	22.872282
98.119114	3265.829192	22.877299
98.343056	3262.596808	22.882317
98.645317	3272.917772	22.887335
98.829612	3287.830653	22.892352
98.967413	3288.187811	22.897370
98.745367	3293.474622	22.902387
98.615818	3291.657965	22.907405
99.180220	3284.638373	22.912423
98.744592	3298.666788	22.917440
99.396251	3306.568986	22.922458
99.428125	3312.668214	22.927475
99.563051	3316.636597	22.932493
99.588329	3312.194914	22.937511
99.560632	3314.493857	22.942528
99.760526	3320.876079	22.947546
99.878818	3332.027592	22.952563
99.754835	3332.119606	22.957581
100.089223	3336.347120	22.962599
100.215186	3347.980352	22.967616
100.178677	3335.619777	22.972634
100.760725	3348.052686	22.977651
100.815997	3353.539100	22.982669
100.892918	3339.248047	22.987687
100.806989	3357.946666	22.992704
101.053148	3361.815568	22.997722
100.709653	3358.555285	23.002739
100.761891	3366.046416	23.007757
100.955821	3349.294062	23.012775
100.737868	3364.778188	23.017792
101.009843	3364.694541	23.022810
101.269525	3374.870733	23.027827
101.091489	3383.430052	23.032845
101.184149	3385.126235	23.037863
101.553150	3402.238610	23.042880
101.621896	3414.130195	23.047898
101.768002	3415.199376	23.052915
101.712024	3423.815342	23.057933
101.847649	3408.643901	23.062951
101.906713	3416.168702	23.067968
102.134579	3431.822917	23.072986
102.199722	3440.874422	23.078003
102.118696	3447.414327	23.083021
102.539256	3436.888475	23.088039
102.667216	3440.681225	23.093056
102.797679	3435.620180	23.098074
102.963122	3457.457906	23.103091
102.862079	3454.854005	23.108109
103.080313	3452.572527	23.113127
102.966802	3454.594553	23.118144
103.298303	3451.351596	23.123162
103.376337	3464.554778	23.128179
103.267738	3484.974106	23.133197
103.471960	3483.777430	23.138215
103.295372	3484.733043	23.143232
103.729327	3494.673684	23.148250
104.046520	3495.034303	23.153267
103.899394	3519.382991	23.158285
104.249075	3512.924055	23.163303
104.426440	3507.498979	23.168320
104.297655	3509.062584	23.173338
104.355345	3510.571723	23.178355
104.323127	3514.427459	23.183373
104.874185	3518.308597	23.188391
105.174439	3524.754075	23.193408
104.943972	3525.702350	23.198426
104.985731	3534.697596	23.203443
105.008427	3533.283164	23.208461
105.083940	3526.084412	23.213479
105.452328	3528.829494	23.218496
105.388331	3541.935045	23.223514
105.326203	3545.956445	23.228531
105.829949	3552.098609	23.233549
105.724644	3554.810593	23.238567
105.756939	3562.421714	23.243584
105.906649	3544.956467	23.248602
106.070931	3562.707080	23.253619
105.765935	3573.300108	23.258637
105.818034	3580.005427	23.263655
105.786576	3580.202885	23.268672
106.133359	3589.598568	23.273690
106.338481	3593.234069	23.278707
106.529668	3600.365802	23.283725
106.480149	3604.186391	23.288743
106.755817	3621.108435	23.293760
107.132012	3627.703026	23.298778
107.318214	3629.839088	23.303795
107.281620	3630.687555	23.308813
107.668803	3630.061908	23.313831
107.603108	3628.386716	23.318848
107.529041	3627.419854	23.323866
107.942757	3621.411671	23.328883
107.644314	3639.206446	23.333901
107.887402	3650.944620	23.338919
107.909518	3656.250098	23.343936
108.033317	3657.467979	23.348954
107.849493	3665.403384	23.353971
107.712977	3665.746712	23.358989
108.195321	3666.810575	23.364007
108.211941	3674.342134	23.369024
108.226552	3680.971298	23.374042
108.401588	3672.942562	23.379059
108.579246	3693.879105	23.384077
109.079505	3703.377055	23.389095
109.080080	3707.931558	23.394112
109.191328	3707.740524	23.399130
109.200680	3703.721034	23.404147
109.106121	3698.193312	23.409165
109.259231	3706.006508	23.414183
109.408121	3723.541902	23.419200
109.527195	3732.288408	23.424218
109.575465	3721.419863	23.429235
109.777037	3728.957188	23.434253
109.812328	3723.308112	23.439271
110.115268	3738.082836	23.444288
110.037487	3743.258798	23.449306
110.090122	3746.754091	23.454323
110.098727	3755.562104	23.459341
110.322813	3759.125228	23.464359
110.674956	3773.639765	23.469376
110.338265	3783.035312	23.474394
110.674864	3779.671557	23.479411
110.742963	3783.887240	23.484429
111.249473	3792.655140	23.489447
111.209789	3802.461836	23.494464
111.239118	3800.610767	23.499482
111.549007	3795.291098	23.504499
111.515790	3804.351882	23.509517
111.696352	3805.589287	23.514535
111.861570	3816.130884	23.519552
111.814241	3819.632383	23.524570
112.053117	3830.825284	23.529587
111.893187	3829.666699	23.534605
112.085091	3821.477436	23.539623
112.547493	3838.499839	23.544640
112.502522	3838.137585	23.549658
113.069038	3842.155253	23.554675
112.474401	3842.068495	23.559693
112.829501	3843.193337	23.564711
112.839236	3831.993032	23.569728
112.995859	3843.050478	23.574746
113.136709	3855.290882	23.579763
113.060576	3861.230460	23.584781
113.297864	3851.869374	23.589799
113.431036	3858.937702	23.594816
113.700739	3868.566552	23.599834
113.645828	3862.426545	23.604851
113.400085	3879.364236	23.609869
113.786102	3884.729555	23.614887
114.008990	3885.139678	23.619904
114.022160	3894.224803	23.624922
114.210005	3905.918140	23.629939
114.010124	3930.133607	23.634957
114.423457	3919.359255	23.639975
114.549907	3916.138873	23.644992
114.394177	3933.731665	23.650010
114.761206	3933.671001	23.655027
114.447487	3931.106663	23.660045
114.649310	3940.291667	23.665063
115.132734	3952.914048	23.670080
115.172227	3960.887192	23.675098
115.377318	3965.889489	23.680115
115.051759	3973.316961	23.685133
115.542403	3973.000202	23.690151
115.780774	3980.080503	23.695168
115.631390	3992.038206	23.700186
115.930222	3993.449635	23.705203
116.316674	3992.824091	23.710221
116.213138	3988.351922	23.715239
116.131929	3988.617150	23.720256
116.537094	4006.803918	23.725274
116.709237	4004.362303	23.730291
116.632265	4022.668812	23.735309
116.946035	4016.875011	23.740327
116.947000	4012.736823	23.745344
116.929749	4017.234224	23.750362
117.102572	4010.225201	23.755379
117.277515	4026.345900	23.760397
117.072055	4029.209370	23.765415
117.240193	4031.143145	23.770432
117.024157	4035.700102	23.775450
117.397389	4046.764769	23.780467
117.591866	4066.370264	23.785485
117.736225	4070.103762	23.790503
117.732000	4061.376966	23.795520
117.943273	4088.233265	23.800538
118.197619	4084.967565	23.805555
118.323483	4088.056900	23.810573
117.959335	4092.681266	23.815591
118.363914	4106.916405	23.820608
118.652037	4124.622915	23.825626
119.061033	4119.975722	23.830643
118.688761	4122.884280	23.835661
119.306397	4135.463667	23.840679
119.172490	4142.974813	23.845696
119.282765	4137.042409	23.850714
119.884264	4138.920928	23.855731
119.589453	4149.629483	23.860749
119.527118	4145.930454	23.865767
120.052320	4153.928593	23.870784
120.184139	4163.926408	23.875802
120.416363	4165.566080	23.880819
120.302460	4170.915113	23.885837
120.485502	4162.506136	23.890855
120.585700	4160.905910	23.895872
120.306411	4169.863389	23.900890
120.767223	4173.427386	23.905907
120.663122	4188.894377	23.910925
120.967417	4188.805665	23.915943
121.083293	4190.277338	23.920960
120.858316	4192.821936	23.925978
121.121128	4205.990397	23.930995
121.225347	4208.751720	23.936013
121.435009	4217.241223	23.941031
121.378706	4213.878973	23.946048
121.567020	4240.259317	23.951066
121.756423	4237.092144	23.956083
121.468543	4239.065821	23.961101
121.735457	4245.955525	23.966119
122.191200	4265.008961	23.971136
121.989923	4264.630152	23.976154
122.343842	4263.873970	23.981171
122.360824	4281.803030	23.986189
122.745316	4284.482577	23.991207
122.815716	4294.796261	23.996224
122.788476	4295.106698	24.001242
123.322881	4302.677343	24.006259
123.523774	4319.943182	24.011277
123.156719	4321.165411	24.016295
123.636644	4319.448865	24.021312
123.355965	4316.636249	24.026330
123.858317	4318.606075	24.031347
123.990213	4346.633609	24.036365
123.863576	4342.591091	24.041383
124.014106	4341.904648	24.046400
124.228482	4351.877007	24.051418
124.368385	4340.794879	24.056435
124.181191	4344.747668	24.061453
124.538724	4365.641025	24.066471
124.744439	4362.786921	24.071488
124.617823	4367.898113	24.076506
124.725149	4374.711862	24.081523
124.988022	4371.517374	24.086541
124.564677	4388.019363	24.091559
125.083874	4397.363204	24.096576
125.104277	4399.897796	24.101594
125.777620	4419.144568	24.106611
125.833252	4423.498080	24.111629
125.468205	4426.042560	24.116647
125.818348	4422.162064	24.121664
126.033958	4431.168395	24.126682
126.355802	4433.419031	24.131699
126.386281	4442.318643	24.136717
126.436458	4443.469201	24.141735
126.560863	4442.644806	24.146752
126.412854	4446.916595	24.151770
126.384544	4458.132804	24.156787
126.699621	4460.876913	24.161805
126.795197	4476.865248	24.166823
127.349983	4471.926827	24.171840
127.347239	4497.018071	24.176858
127.611212	4495.051259	24.181875
127.762018	4497.666442	24.186893
127.773580	4505.909346	24.191911
128.036675	4492.228983	24.196928
127.901562	4505.561011	24.201946
127.896977	4521.505104	24.206963
127.990622	4520.401442	24.211981
128.147652	4523.400744	24.216999
128.417385	4533.866411	24.222016
128.352508	4545.937498	24.227034
128.556953	4546.060130	24.232051
128.611686	4549.006021	24.237069
128.607210	4566.869281	24.242087
129.400257	4562.502710	24.247104
129.271050	4578.775714	24.252122
129.311654	4573.627424	24.257139
129.243959	4588.555604	24.262157
129.580265	4600.813237	24.267175
130.121919	4594.140769	24.272192
129.503294	4596.586113	24.277210
129.873560	4616.199383	24.282227
130.206973	4619.278389	24.287245
130.090050	4617.185004	24.292263
130.567497	4615.967547	24.297280
130.398792	4629.762620	24.302298
130.563913	4639.250440	24.307315
130.633587	4637.547634	24.312333
130.770282	4649.145299	24.317351
130.779821	4646.463928	24.322368
131.332242	4659.748329	24.327386
131.124072	4663.511926	24.332403
131.413966	4660.609866	24.337421
131.370341	4680.215449	24.342439
131.702342	4688.474520	24.347456
131.409346	4696.159174	24.352474
131.602308	4695.301932	24.357491
131.827905	4708.085181	24.362509
131.841333	4719.651698	24.367527
132.129742	4724.426509	24.372544
132.488156	4740.809498	24.377562
132.503212	4749.547538	24.382579
132.652762	4736.721259	24.387597
133.115646	4751.383371	24.392615
132.976713	4754.599531	24.397632
133.133651	4766.771743	24.402650
133.536853	4773.561385	24.407667
133.612646	4773.098122	24.412685
133.380671	4778.702570	24.417703
133.810444	4772.126478	24.422720
134.212226	4791.169983	24.427738
134.412790	4796.498341	24.432755
133.966181	4800.037330	24.437773
134.257193	4790.844112	24.442791
134.279807	4792.380950	24.447808
134.162136	4798.620898	24.452826
134.143497	4816.584474	24.457843
134.815748	4813.916045	24.462861
134.202074	4818.832207	24.467879
134.677155	4833.915450	24.472896
134.944402	4854.078571	24.477914
134.993447	4851.081640	24.482931
134.945393	4859.656011	24.487949
135.088457	4879.478770	24.492967
135.454553	4882.006619	24.497984
135.807737	4898.169611	24.503002
135.863617	4902.889359	24.508019
136.233269	4897.878819	24.513037
135.963183	4910.411586	24.518055
136.598871	4920.362445	24.523072
136.790430	4923.391126	24.528090
136.713050	4933.946127	24.533107
136.940327	4930.122652	24.538125
136.739115	4937.493155	24.543143
137.340652	4956.085716	24.548160
137.340337	4954.936773	24.553178
137.673855	4959.114303	24.558195
137.696871	4957.709181	24.563213
137.524335	4957.767771	24.568231
137.469632	4966.592602	24.573248
137.971469	4977.154738	24.578266
137.738041	4982.873112	24.583283
137.807245	4979.765678	24.588301
138.094221	4999.828017	24.593319
138.211848	5002.524229	24.598336
138.592924	5012.527653	24.603354
139.010846	5025.400945	24.608371
138.995602	5030.371767	24.613389
138.882385	5036.251250	24.618407
138.803938	5036.749646	24.623424
139.012732	5050.864685	24.628442
139.107808	5057.816343	24.633459
139.302854	5059.222022	24.638477
139.339306	5079.061700	24.643495
139.382354	5090.200831	24.648512
139.704151	5084.894707	24.653530
139.899845	5101.473969	24.658547
140.393015	5101.579783	24.663565
140.161848	5111.540289	24.668583
140.272490	5119.225016	24.673600
140.943873	5134.375609	24.678618
140.835323	5137.337706	24.683635
141.071431	5138.957920	24.688653
141.041741	5146.942423	24.693671
141.145558	5159.940777	24.698688
141.277508	5161.795115	24.703706
141.115882	5164.405680	24.708723
141.385178	5178.779650	24.713741
141.624957	5186.958699	24.718759
141.953145	5191.762124	24.723776
141.975370	5194.290228	24.728794
142.260099	5212.658061	24.733811
142.583484	5208.677424	24.738829
142.463055	5218.286041	24.743847
142.542065	5215.028670	24.748864
142.565765	5227.013729	24.753882
142.753510	5237.896692	24.758899
142.772408	5240.876718	24.763917
142.898125	5248.357115	24.768935
143.120701	5259.297766	24.773952
143.154547	5269.807126	24.778970
143.298949	5277.985375	24.783987
143.698610	5274.365255	24.789005
143.871138	5294.938280	24.794023
144.056920	5302.478735	24.799040
144.304261	5293.831888	24.804058
144.511620	5310.614693	24.809075
144.801773	5309.161380	24.814093
144.547730	5321.448855	24.819111
145.047775	5317.238495	24.824128
145.337325	5318.061198	24.829146
145.037407	5321.583617	24.834163
144.995661	5328.872475	24.839181
145.510624	5338.883514	24.844199
145.575660	5341.123992	24.849216
145.538755	5341.937864	24.854234
145.848951	5367.552629	24.859251
146.355973	5365.222515	24.864269
146.080522	5369.422942	24.869287
146.163838	5372.313982	24.874304
146.409494	5373.885372	24.879322
146.291448	5392.196534	24.884339
147.006629	5392.936776	24.889357
146.868520	5396.623258	24.894375
146.852334	5390.643970	24.899392
147.237303	5406.584627	24.904410
147.428837	5421.662275	24.909427
147.520612	5421.752061	24.914445
147.621224	5424.271073	24.919463
147.416840	5445.020112	24.924480
147.952845	5444.828808	24.929498
147.957168	5448.944386	24.934515
147.720049	5447.052820	24.939533
147.829330	5467.948457	24.944551
148.021455	5478.209019	24.949568
148.400766	5489.431448	24.954586
148.379326	5494.602237	24.959603
148.935729	5498.530322	24.964621
149.038393	5521.327360	24.969639
149.006221	5518.876518	24.974656
149.190392	5520.025092	24.979674
148.883181	5533.416397	24.984691
149.397680	5544.163123	24.989709
149.870122	5558.186745	24.994727
149.981169	5567.213178	24.999744
150.170670	5568.824949	25.004762
150.201481	5577.923934	25.009779
150.824303	5583.334734	25.014797
150.724014	5586.014666	25.019815
150.728464	5594.584313	25.024832
151.000467	5596.085304	25.029850
150.892590	5605.815267	25.034867
151.260135	5612.563461	25.039885
151.419597	5627.204369	25.044903
151.479418	5623.195488	25.049920
151.700572	5623.527009	25.054938
151.524603	5630.852799	25.059955
151.487535	5636.054486	25.064973
151.809689	5648.040413	25.069991
152.045367	5661.242591	25.075008
152.186909	5662.533589	25.080026
152.414679	5668.669209	25.085043
152.126544	5675.122405	25.090061
152.139069	5685.505921	25.095079
152.675353	5696.331398	25.100096
153.014298	5702.755810	25.105114
152.795232	5726.124360	25.110131
153.083628	5725.428895	25.115149
153.333955	5737.353530	25.120167
153.558822	5763.411528	25.125184
154.130157	5758.252362	25.130202
153.838034	5772.676875	25.135219
154.168445	5765.588828	25.140237
154.553551	5778.079520	25.145255
154.604063	5793.760401	25.150272
154.450446	5782.256192	25.155290
154.671309	5795.151430	25.160307
154.751123	5802.917036	25.165325
155.173818	5811.664326	25.170343
154.953063	5812.740617	25.175360
155.731468	5828.039173	25.180378
155.472447	5835.712667	25.185395
155.946955	5834.940691	25.190413
156.027695	5835.720370	25.195431
155.935952	5848.680405	25.200448
156.084238	5853.815234	25.205466
156.126715	5866.533284	25.210483
156.626243	5865.984671	25.215501
156.745503	5882.333550	25.220519
156.786580	5887.156887	25.225536
157.250293	5875.259174	25.230554
157.263184	5889.187740	25.235571
157.432081	5900.796941	25.240589
157.197512	5912.387282	25.245607
157.387026	5916.341370	25.250624
157.887585	5925.714175	25.255642
157.637913	5937.780407	25.260659
158.041294	5940.255215	25.265677
158.044510	5941.024947	25.270695
158.127094	5959.507276	25.275712
158.359981	5961.197517	25.280730
158.505519	5979.531107	25.285747
159.299926	5993.867649	25.290765
159.134634	5992.659255	25.295783
158.915256	5991.187855	25.300800
159.361970	6000.894278	25.305818
159.527098	6014.483416	25.310835
159.434022	6022.620284	25.315853
160.196796	6035.853799	25.320871
160.003008	6040.518253	25.325888
160.096303	6039.506100	25.330906
160.542470	6040.471609	25.335923
160.491997	6056.866176	25.340941
160.667125	6060.724690	25.345959
160.462518	6073.124880	25.350976
160.875850	6074.957327	25.355994
160.628854	6082.307051	25.361011
161.012504	6094.312049	25.366029
161.225237	6106.160739	25.371047
161.334985	6121.220209	25.376064
162.003337	6118.631130	25.381082
162.317870	6132.847241	25.386099
162.195368	6139.306218	25.391117
162.341495	6143.207175	25.396135
162.125680	6150.428927	25.401152
162.617011	6162.884301	25.406170
162.644623	6174.108587	25.411187
163.067903	6174.449492	25.416205
163.057080	6178.914851	25.421223
163.046915	6181.852233	25.426240
163.306179	6191.970093	25.431258
163.392873	6196.890539	25.436275
163.269935	6199.514129	25.441293
163.841361	6208.560301	25.446311
163.542745	6221.183665	25.451328
164.130541	6226.366546	25.456346
164.334150	6242.140627	25.461363
164.117210	6250.110751	25.466381
164.384309	6254.185343	25.471399
164.447960	6276.746362	25.476416
164.733366	6274.794946	25.481434
165.114845	6289.448955	25.486451
165.116873	6293.451438	25.491469
165.320987	6308.429986	25.496487
165.353841	6309.599159	25.501504
165.490503	6331.365923	25.506522
165.368985	6342.054922	25.511539
165.728248	6348.741551	25.516557
166.131578	6351.992996	25.521575
166.020160	6359.378412	25.526592
166.708116	6375.790166	25.531610
166.672341	6386.314231	25.536627
166.812666	6417.011122	25.541645
167.140358	6411.984650	25.546663
167.651097	6416.879761	25.551680
167.685151	6413.723926	25.556698
167.848451	6434.192347	25.561715
168.167398	6449.654954	25.566733
168.307077	6441.223315	25.571751
167.927323	6455.264332	25.576768
168.043079	6459.387934	25.581786
168.656984	6462.858956	25.586803
168.394258	6472.130644	25.591821
169.261987	6488.132360	25.596839
169.089243	6488.977033	25.601856
168.874188	6493.165096	25.606874
169.084853	6502.965590	25.611891
169.243352	6521.275594	25.616909
169.510950	6521.372566	25.621927
169.796222	6535.959767	25.626944
169.871696	6545.146940	25.631962
169.712699	6554.001501	25.636979
170.036791	6574.151304	25.641997
170.002844	6574.601730	25.647015
170.375469	6596.290803	25.652032
170.945780	6599.055235	25.657050
171.195197	6613.275607	25.662067
171.127758	6622.958735	25.667085
171.264385	6627.480025	25.672103
171.161980	6635.227177	25.677120
171.290316	6640.930429	25.682138
171.673286	6662.681097	25.687156
171.533786	6679.595263	25.692173
172.169911	6692.123021	25.697191
172.193496	6711.404564	25.702208
172.650990	6713.088100	25.707226
173.115384	6719.155435	25.712244
172.962277	6736.759981	25.717261
173.247029	6736.140817	25.722279
173.506255	6745.507656	25.727296
173.897940	6745.774603	25.732314
173.657817	6749.824592	25.737332
173.979805	6758.155624	25.742349
174.521889	6753.442728	25.747367
174.074520	6758.525913	25.752384
174.462030	6759.443828	25.757402
174.759971	6774.161823	25.762420
174.811836	6789.287733	25.767437
174.987496	6787.189300	25.772455
175.059847	6786.155134	25.777472
175.003847	6792.209313	25.782490
175.414962	6805.811010	25.787508
175.225502	6814.196937	25.792525
175.538328	6818.611749	25.797543
175.747353	6837.908569	25.802560
175.998306	6835.166960	25.807578
176.480429	6844.508401	25.812596
175.880229	6860.494175	25.817613
176.125897	6871.744707	25.822631
176.562733	6891.451016	25.827648
176.935290	6899.398521	25.832666
177.271085	6904.295916	25.837684
177.225604	6912.839275	25.842701
177.546198	6921.189541	25.847719
177.336714	6931.971585	25.852736
177.617031	6933.818647	25.857754
177.797836	6948.173147	25.862772
177.413065	6959.162610	25.867789
178.076369	6973.627799	25.872807
178.250571	6993.915193	25.877824
178.229933	7002.824060	25.882842
178.532942	7009.128287	25.887860
178.743338	7029.968824	25.892877
179.071538	7037.658157	25.897895
179.517485	7048.353373	25.902912
179.716725	7071.828574	25.907930
179.806185	7077.007690	25.912948
179.613923	7079.437065	25.917965
180.157976	7091.780636	25.922983
180.101407	7097.257287	25.928000
180.448575	7108.296333	25.933018
180.484387	7120.239691	25.938036
180.488592	7138.498716	25.943053
181.069459	7134.758298	25.948071
181.046337	7150.344537	25.953088
181.106369	7168.392801	25.958106
181.681150	7168.485853	25.963124
181.179937	7179.619966	25.968141
181.725653	7193.993258	25.973159
182.193282	7200.053933	25.978176
181.978121	7211.269530	25.983194
182.691995	7228.369361	25.988212
182.544450	7243.391136	25.993229
182.674768	7248.996401	25.998247
183.119580	7255.988813	26.003264
183.344045	7270.305155	26.008282
183.339194	7284.430132	26.013300
183.277339	7302.402914	26.018317
183.751129	7308.768885	26.023335
184.177356	7314.646667	26.028352
184.147455	7325.394492	26.033370
184.724667	7325.566089	26.038388
184.679400	7347.580388	26.043405
184.715470	7350.665404	26.048423
184.983024	7363.516549	26.053440
185.042779	7371.854216	26.058458
185.426330	7364.479419	26.063476
185.000221	7377.685487	26.068493
185.262295	7389.732480	26.073511
185.336215	7399.472795	26.078528
185.363112	7418.337838	26.083546
185.970110	7431.672540	26.088564
186.126172	7446.757411	26.093581
186.259023	7451.364734	26.098599
186.884495	7466.047757	26.103616
186.628540	7472.850120	26.108634
187.361758	7479.106055	26.113652
187.178921	7483.418730	26.118669
187.452986	7502.292493	26.123687
187.655227	7518.500392	26.128704
187.685572	7518.918671	26.133722
188.142567	7528.093921	26.138740
188.379782	7548.798250	26.143757
188.084841	7541.160307	26.148775
188.425862	7554.255793	26.153792
188.654933	7570.926772	26.158810
188.634770	7572.678907	26.163828
189.075836	7590.828900	26.168845
189.304479	7598.088926	26.173863
189.243539	7603.531685	26.178880
189.567340	7618.344172	26.183898
189.799288	7616.214729	26.188916
189.826130	7641.394038	26.193933
190.309415	7648.055400	26.198951
190.363233	7657.360174	26.203968
190.324434	7675.635938	26.208986
190.606594	7681.536408	26.214004
190.773539	7695.827364	26.219021
190.879637	7709.455417	26.224039
191.223883	7720.391108	26.229056
191.458161	7732.215374	26.234074
191.830833	7744.485208	26.239092
191.528572	7754.685585	26.244109
192.058513	7770.722402	26.249127
192.377841	7783.152157	26.254144
192.457075	7797.886291	26.259162
193.053994	7807.680642	26.264180
193.232729	7811.444249	26.269197
193.029394	7824.012739	26.274215
193.545678	7841.273535	26.279232
193.347445	7848.771015	26.284250
193.529185	7856.152146	26.289268
193.773544	7868.571604	26.294285
193.866368	7885.646216	26.299303
193.987439	7899.707737	26.304320
194.383125	7908.529721	26.309338
194.954850	7926.154445	26.314356
195.053099	7932.595251	26.319373
195.237118	7942.908976	26.324391
195.764038	7952.600715	26.329408
195.161055	7955.849088	26.334426
195.670862	7968.321740	26.339444
195.510669	7990.007530	26.344461
195.932159	7996.429291	26.349479
196.467854	8013.819805	26.354496
196.447129	8018.833337	26.359514
196.512052	8041.014310	26.364532
196.741646	8047.889201	26.369549
196.974592	8051.053990	26.374567
197.361354	8065.755946	26.379584
197.344322	8072.584241	26.384602
197.592083	8086.764970	26.389620
197.665357	8095.454441	26.394637
197.952354	8110.743496	26.399655
197.997986	8121.022173	26.404672
197.852539	8137.815478	26.409690
198.675219	8145.999247	26.414708
198.642790	8159.873488	26.419725
198.832795	8175.335647	26.424743
198.924720	8181.809102	26.429760
199.267244	8204.133052	26.434778
199.473043	8215.390652	26.439796
199.621113	8220.813477	26.444813
200.045762	8240.188485	26.449831
200.015806	8237.137080	26.454848
200.100670	8260.726426	26.459866
200.525429	8262.557310	26.464884
200.706339	8274.393441	26.469901
200.999334	8293.953302	26.474919
201.082265	8298.947513	26.479936
201.716816	8311.830226	26.484954
201.515126	8324.727138	26.489972
201.789308	8317.953169	26.494989
201.822710	8340.714038	26.500007
202.074224	8349.113662	26.505024
202.024585	8362.324594	26.510042
202.322149	8377.672201	26.515060
202.347178	8393.861274	26.520077
202.693444	8405.718942	26.525095
202.852311	8412.014662	26.530112
203.141098	8435.720670	26.535130
203.281008	8448.911441	26.540148
203.672257	8468.143535	26.545165
203.936448	8484.352049	26.550183
204.273452	8491.636496	26.555200
204.153056	8501.745649	26.560218
204.722984	8511.471989	26.565236
205.057367	8516.512111	26.570253
204.814786	8539.518517	26.575271
205.290309	8549.373325	26.580288
205.334792	8569.442827	26.585306
205.289340	8580.910497	26.590324
205.656007	8603.534236	26.595341
206.018087	8608.806833	26.600359
206.458463	8622.001171	26.605376
206.224472	8635.310636	26.610394
206.512549	8641.835610	26.615412
206.909796	8651.011311	26.620429
206.785175	8668.711104	26.625447
207.606150	8676.317612	26.630464
207.605322	8690.954498	26.635482
207.731610	8703.585603	26.640500
208.009015	8716.909728	26.645517
207.848894	8725.168791	26.650535
208.256312	8739.467083	26.655552
208.032634	8754.183131	26.660570
208.661225	8773.896143	26.665588
208.908633	8793.094279	26.670605
208.854177	8809.517172	26.675623
209.301550	8814.508103	26.680640
209.416053	8834.238571	26.685658
210.011304	8844.908287	26.690676
210.366155	8864.869500	26.695693
210.605148	8877.154715	26.700711
210.783506	8874.433653	26.705728
210.772242	8893.681887	26.710746
210.814194	8902.130379	26.715764
210.993379	8917.436991	26.720781
211.145191	8921.811233	26.725799
211.690027	8939.832636	26.730816
211.726346	8955.909927	26.735834
211.626379	8965.798282	26.740852
211.992394	8971.354519	26.745869
212.087449	8983.987550	26.750887
212.663221	8992.557677	26.755904
212.698675	9007.154398	26.760922
212.953328	9026.635794	26.765940
213.252723	9035.574434	26.770957
213.238449	9046.724939	26.775975
213.422696	9054.693406	26.780992
213.827191	9076.572998	26.786010
214.014303	9082.236226	26.791028
214.192792	9090.811805	26.796045
214.091523	9104.372337	26.801063
214.687035	9116.260875	26.806080
215.032588	9121.889823	26.811098
214.951407	9138.276148	26.816116
214.906962	9145.371185	26.821133
215.302156	9164.893854	26.826151
215.941609	9175.342143	26.831168
215.511950	9195.941247	26.836186
215.708030	9204.637257	26.841204
216.311099	9216.186846	26.846221
216.583649	9245.238563	26.851239
216.803640	9249.545371	26.856256
217.084700	9266.711743	26.861274
217.050742	9275.724823	26.866292
217.517510	9290.528883	26.871309
217.581043	9302.030441	26.876327
217.736177	9313.463982	26.881344
217.938449	9323.046280	26.886362
218.346578	9346.235902	26.891380
218.481969	9350.944336	26.896397
218.367830	9374.193708	26.901415
218.961048	9391.342868	26.906432
219.146398	9405.888004	26.911450
219.409949	9411.226783	26.916468
219.676431	9427.391561	26.921485
219.608688	9443.854982	26.926503
219.786398	9459.989492	26.931520
220.148852	9473.982820	26.936538
220.435644	9492.534571	26.941556
220.975383	9491.493341	26.946573
220.452258	9510.301439	26.951591
221.354451	9520.759281	26.956608
221.248114	9546.160950	26.961626
221.949651	9551.008073	26.966644
221.836631	9566.455716	26.971661
221.936641	9586.517617	26.976679
222.438407	9600.242943	26.981696
222.553476	9613.937295	26.986714
222.949226	9626.391048	26.991732
223.220519	9638.507526	26.996749
223.292238	9645.193043	27.001767
223.677189	9660.846916	27.006784
223.702640	9667.640725	27.011802
223.542762	9680.096308	27.016820
223.995187	9691.953957	27.021837
224.195935	9716.793101	27.026855
224.394371	9734.061255	27.031872
224.721354	9750.977763	27.036890
224.960658	9765.887299	27.041908
225.533744	9779.052201	27.046925
225.765486	9787.266133	27.051943
225.732443	9792.733578	27.056960
226.018340	9804.105890	27.061978
225.965609	9820.279969	27.066996
226.194962	9841.616412	27.072013
226.280819	9858.753920	27.077031
226.797128	9873.796962	27.082048
227.256338	9883.869741	27.087066
227.171378	9897.532489	27.092084
227.712719	9910.658254	27.097101
227.740152	9926.327312	27.102119
227.738594	9933.011782	27.107136
227.610835	9948.831466	27.112154
227.860435	9959.631753	27.117172
228.338784	9978.071888	27.122189
228.672445	10004.112513	27.127207
229.026896	10016.816119	27.132224
229.507678	10032.322681	27.137242
229.378724	10052.670388	27.142260
229.688808	10060.824807	27.147277
229.550447	10066.179376	27.152295
229.951576	10077.960057	27.157312
230.308899	10103.324580	27.162330
230.715816	10119.578469	27.167348
230.928184	10130.179455	27.172365
230.926855	10141.754840	27.177383
231.357788	10151.058621	27.182400
231.320021	10161.695652	27.187418
231.674612	10187.821663	27.192436
232.025442	10199.433483	27.197453
231.703346	10217.509843	27.202471
232.322379	10229.543813	27.207488
232.595331	10249.708790	27.212506
232.464872	10269.425476	27.217524
233.132144	10278.698612	27.222541
233.604605	10304.878944	27.227559
233.526208	10319.532417	27.232576
233.621189	10337.259383	27.237594
234.012570	10349.723778	27.242612
234.658813	10360.414800	27.247629
234.924868	10375.765837	27.252647
234.881085	10381.958200	27.257664
235.409820	10396.589246	27.262682
235.458358	10405.997263	27.267700
236.259621	10416.907160	27.272717
236.131112	10436.355329	27.277735
236.122781	10437.755398	27.282752
236.246635	10454.439137	27.287770
236.483742	10469.706376	27.292788
237.106947	10483.697507	27.297805
236.675912	10500.749230	27.302823
237.055054	10514.810192	27.307840
237.206192	10530.419330	27.312858
237.461497	10540.319170	27.317876
237.875835	10556.954337	27.322893
238.138993	10584.528737	27.327911
237.914191	10602.707055	27.332928
238.137650	10610.613210	27.337946
238.349547	10635.009776	27.342964
239.023550	10657.183704	27.347981
239.180512	10676.123245	27.352999
239.350291	10695.108161	27.358016
240.075030	10714.669242	27.363034
240.075968	10721.925118	27.368052
240.519710	10738.606361	27.373069
240.456806	10752.010515	27.378087
240.641470	10773.749716	27.383104
240.872403	10778.910862	27.388122
241.245587	10809.613279	27.393140
241.455939	10817.208977	27.398157
242.065955	10829.579450	27.403175
241.973779	10846.322640	27.408192
242.073050	10858.473173	27.413210
242.441181	10880.458466	27.418228
243.088605	10880.928559	27.423245
243.170859	10898.654892	27.428263
243.288112	10919.991182	27.433280
243.987732	10933.118134	27.438298
243.929716	10950.440218	27.443316
244.004009	10953.276711	27.448333
244.123420	10971.796160	27.453351
244.496161	10980.503216	27.458368
244.757361	10987.405822	27.463386
244.320850	11013.877948	27.468404
245.065623	11029.786048	27.473421
245.239005	11039.648465	27.478439
245.437795	11057.110400	27.483456
245.627109	11067.207155	27.488474
245.800598	11092.049239	27.493492
246.159753	11097.120919	27.498509
246.491842	11121.022491	27.503527
246.618335	11137.362244	27.508544
247.004455	11151.204718	27.513562
247.155344	11174.174829	27.518580
247.700774	11183.303309	27.523597
247.779540	11195.599366	27.528615
247.921594	11226.824947	27.533632
248.132198	11235.216497	27.538650
248.668518	11251.015348	27.543668
248.755453	11263.666982	27.548685
248.902253	11284.118077	27.553703
249.383928	11306.073452	27.558720
249.585425	11306.363961	27.563738
249.751359	11328.776159	27.568756
249.996220	11337.130813	27.573773
250.322830	11364.942718	27.578791
250.421742	11380.816514	27.583808
250.571945	11392.965731	27.588826
250.811665	11418.666226	27.593844
250.866440	11436.795237	27.598861
251.446762	11452.552630	27.603879
251.415415	11473.878093	27.608896
251.758683	11483.142593	27.613914
252.117994	11517.028114	27.618932
252.376042	11531.541412	27.623949
252.577368	11553.790451	27.628967
252.878523	11568.540167	27.633984
253.197920	11586.820487	27.639002
253.583998	11609.760602	27.644020
254.144577	11626.076988	27.649037
254.379405	11651.513322	27.654055
254.680453	11661.346594	27.659072
254.594451	11670.223723	27.664090
254.532580	11690.329025	27.669108
255.514001	11712.137120	27.674125
255.819302	11716.892162	27.679143
255.863459	11736.144110	27.684160
256.060388	11748.150455	27.689178
256.505941	11771.343541	27.694196
256.821493	11778.496859	27.699213
257.167406	11794.903859	27.704231
256.875478	11804.558532	27.709248
257.130065	11818.516835	27.714266
257.545923	11840.761026	27.719284
257.653314	11845.461845	27.724301
258.218708	11864.370181	27.729319
258.585220	11889.871467	27.734336
258.709517	11894.572808	27.739354
259.006327	11921.240788	27.744372
259.006615	11929.798221	27.749389
259.531884	11947.860336	27.754407
259.663821	11957.612891	27.759424
260.095122	11971.022597	27.764442
259.654255	11991.800194	27.769460
260.011228	12006.639400	27.774477
260.189729	12023.840160	27.779495
260.304218	12056.719787	27.784512
260.980447	12072.459520	27.789530
260.971561	12087.381365	27.794548
261.452978	12099.002329	27.799565
261.540617	12129.303231	27.804583
262.065486	12145.398303	27.809600
262.251566	12160.498077	27.814618
262.585825	12180.759734	27.819636
262.799452	12199.401418	27.824653
263.215995	12211.098927	27.829671
263.415955	12224.121910	27.834688
263.779363	12247.720018	27.839706
264.029899	12257.173106	27.844724
263.999953	12265.422805	27.849741
264.493193	12283.588152	27.854759
264.479683	12310.324241	27.859776
264.756415	12323.669993	27.864794
264.973367	12339.731364	27.869812
265.467275	12359.134542	27.874829
265.861447	12374.283993	27.879847
265.632948	12399.364453	27.884864
266.194277	12410.401526	27.889882
266.550860	12430.325226	27.894900
266.661308	12453.319021	27.899917
267.019241	12469.263683	27.904935
267.239345	12496.146593	27.909952
267.728135	12512.958146	27.914970
267.823188	12535.284990	27.919988
268.056505	12547.942976	27.925005
268.460470	12562.993152	27.930023
268.708696	12578.790884	27.935040
269.102503	12597.894203	27.940058
269.564372	12621.903666	27.945076
269.999025	12648.557397	27.950093
269.979303	12653.906745	27.955111
270.266191	12671.779532	27.960128
270.467241	12681.354268	27.965146
270.614418	12702.157366	27.970164
270.976158	12722.058461	27.975181
271.098855	12728.478145	27.980199
271.113600	12747.498892	27.985216
271.986642	12773.518865	27.990234
272.008084	12793.482816	27.995252
272.088390	12804.434421	28.000269
272.678860	12819.076638	28.005287
272.724237	12847.882155	28.010304
273.229750	12869.582990	28.015322
273.175946	12884.885132	28.020340
273.525923	12902.426148	28.025357
273.647157	12925.043036	28.030375
273.962139	12951.371728	28.035392
274.114691	12974.485878	28.040410
274.395437	12992.887302	28.045428
274.747016	13021.139849	28.050445
275.389242	13032.657252	28.055463
275.637714	13062.533397	28.060480
276.195233	13074.831474	28.065498
276.292226	13094.142845	28.070516
276.510941	13112.914109	28.075533
276.704606	13133.419869	28.080551
276.761729	13150.293294	28.085568
277.316114	13173.572112	28.090586
277.542806	13188.590555	28.095604
277.469711	13211.014011	28.100621
278.235009	13219.521664	28.105639
278.175512	13245.565210	28.110656
278.888239	13264.843461	28.115674
278.989534	13274.699393	28.120692
279.206525	13305.913517	28.125709
279.532687	13311.398346	28.130727
279.588063	13340.755691	28.135744
279.963186	13351.475109	28.140762
280.566175	13363.387293	28.145780
280.645565	13384.523874	28.150797
280.700880	13397.311368	28.155815
280.771268	13413.554510	28.160832
281.321282	13429.334100	28.165850
281.784218	13449.987501	28.170868
281.671489	13468.848933	28.175885
281.757923	13487.028637	28.180903
281.990791	13519.882787	28.185920
282.443518	13534.632403	28.190938
282.798165	13546.081482	28.195956
283.201864	13585.054479	28.200973
283.185887	13600.458644	28.205991
283.762773	13630.783207	28.211008
283.926013	13640.670680	28.216026
284.206310	13663.209844	28.221044
284.237873	13682.412059	28.226061
284.782200	13705.948908	28.231079
284.437365	13735.941161	28.236096
285.465760	13758.502204	28.241114
285.862592	13784.253941	28.246132
286.098781	13805.767500	28.251149
286.670962	13817.267934	28.256167
286.969113	13853.974741	28.261184
287.156268	13859.699412	28.266202
287.386177	13882.647804	28.271220
287.832451	13900.698899	28.276237
288.310402	13924.956984	28.281255
288.110573	13942.727203	28.286272
288.085926	13961.774285	28.291290
288.898475	13977.317405	28.296308
288.678073	14007.552713	28.301325
288.991166	14027.652286	28.306343
289.412037	14054.139617	28.311360
290.044994	14080.442173	28.316378
290.229421	14092.486704	28.321396
290.337656	14122.076990	28.326413
290.975050	14147.431511	28.331431
290.931705	14167.918669	28.336448
291.408353	14181.528121	28.341466
291.934102	14202.883079	28.346484
292.233216	14224.624114	28.351501
292.134353	14248.489776	28.356519
292.569080	14274.034120	28.361536
292.675599	14288.225878	28.366554
292.926957	14314.307460	28.371572
293.353390	14333.113712	28.376589
293.634350	14354.355595	28.381607
294.179247	14382.800955	28.386624
293.934547	14402.549317	28.391642
294.324064	14431.625456	28.396660
294.645743	14451.695708	28.401677
295.115668	14477.913817	28.406695
295.306623	14503.878794	28.411712
295.460025	14521.906878	28.416730
295.745141	14539.980667	28.421748
296.498118	14568.358970	28.426765
296.799026	14597.016570	28.431783
297.065168	14616.656708	28.436800
296.970297	14633.817387	28.441818
297.285505	14668.763978	28.446836
298.045652	14688.380494	28.451853
298.244908	14691.115861	28.456871
298.360395	14713.918952	28.461888
298.386764	14743.943067	28.466906
298.899659	14767.287188	28.471924
298.994970	14791.915822	28.476941
299.795010	14814.163333	28.481959
299.862610	14830.218626	28.486976
299.985467	14845.990510	28.491994
300.585290	14870.142279	28.497012
300.654447	14898.707148	28.502029
301.215525	14902.538624	28.507047
301.330064	14939.655271	28.512064
301.451008	14953.046228	28.517082
301.806143	14972.795963	28.522100
302.038014	15012.619942	28.527117
302.448154	15023.814875	28.532135
302.550408	15049.330223	28.537152
303.058168	15071.838582	28.542170
303.441202	15091.230343	28.547188
303.666568	15116.458044	28.552205
304.212569	15142.112451	28.557223
304.513415	15165.783995	28.562240
304.839397	15178.353422	28.567258
304.840849	15197.211307	28.572276
305.172628	15223.231000	28.577293
305.904785	15249.661756	28.582311
305.740280	15269.736386	28.587328
306.271657	15289.120902	28.592346
306.713065	15312.072625	28.597364
306.697493	15342.934883	28.602381
307.131211	15366.926960	28.607399
307.074976	15390.070429	28.612416
307.628491	15410.136956	28.617434
308.335322	15432.229240	28.622452
308.301699	15457.024210	28.627469
308.673347	15487.011195	28.632487
308.993379	15508.497749	28.637504
309.199423	15528.931506	28.642522
309.672763	15547.324182	28.647540
310.111295	15572.834926	28.652557
310.295655	15603.460993	28.657575
310.359932	15621.889393	28.662592
310.663452	15653.930768	28.667610
311.346601	15673.964631	28.672628
311.171953	15693.554905	28.677645
311.647230	15717.288241	28.682663
311.993952	15751.976045	28.687680
312.227580	15775.469369	28.692698
313.003743	15797.424880	28.697716
313.028091	15832.997142	28.702733
313.591044	15850.062181	28.707751
313.519819	15879.850691	28.712768
314.130128	15909.447211	28.717786
314.423633	15922.360162	28.722804
314.373698	15957.303134	28.727821
314.810712	15980.306880	28.732839
315.100186	16008.560949	28.737856
315.631961	16031.698359	28.742874
316.009491	16053.375498	28.747892
316.143290	16078.536688	28.752909
316.747225	16109.341036	28.757927
316.827961	16135.312856	28.762944
317.306489	16149.791990	28.767962
317.927765	16176.102424	28.772980
317.765333	16205.283510	28.777997
318.409284	16221.780304	28.783015
318.754905	16232.366996	28.788032
318.773321	16271.029967	28.793050
319.180008	16285.138284	28.798068
319.486985	16313.506922	28.803085
319.762434	16331.296497	28.808103
320.380917	16349.082890	28.813120
320.446234	16378.497033	28.818138
320.573867	16399.942078	28.823156
320.594975	16420.162549	28.828173
321.103404	16439.934002	28.833191
321.364225	16475.423031	28.838208
321.648164	16505.137922	28.843226
321.815474	16530.714535	28.848244
322.292640	16559.502226	28.853261
322.514016	16572.635375	28.858279
323.172724	16600.538734	28.863296
323.142363	16630.151442	28.868314
323.495197	16647.736517	28.873332
324.381659	16690.654705	28.878349
324.412550	16708.435559	28.883367
324.793065	16728.461078	28.888384
324.925191	16761.905110	28.893402
325.363340	16776.694263	28.898420
325.755775	16805.849352	28.903437
326.040601	16828.236767	28.908455
326.340161	16859.904903	28.913472
326.668133	16887.623594	28.918490
326.989499	16911.000328	28.923508
326.905121	16936.048361	28.928525
327.173217	16968.994509	28.933543
327.814009	16991.875946	28.938560
328.064815	17031.148387	28.943578
328.657926	17053.494090	28.948596
329.162150	17094.135694	28.953613
329.180042	17116.937972	28.958631
329.416005	17142.656254	28.963648
329.677958	17172.697794	28.968666
330.208598	17193.050885	28.973684
330.607592	17228.162731	28.978701
330.901565	17256.247359	28.983719
331.210258	17276.730064	28.988736
331.595765	17308.635003	28.993754
331.974037	17339.385068	28.998772
332.834283	17360.318433	29.003789
332.980536	17388.641180	29.008807
333.070777	17406.536566	29.013824
333.345820	17449.798592	29.018842
334.186732	17474.304391	29.023860
334.353219	17500.052983	29.028877
334.677857	17528.259549	29.033895
334.973837	17542.926262	29.038912
335.135688	17577.519962	29.043930
335.525642	17596.265640	29.048948
335.738561	17625.917571	29.053965
336.353255	17645.607284	29.058983
336.715621	17672.437281	29.064000
336.921873	17696.158342	29.069018
337.475255	17719.237539	29.074036
337.586549	17745.557352	29.079053
337.920414	17770.092412	29.084071
338.334226	17793.585240	29.089088
338.579456	17822.632256	29.094106
338.700194	17849.329776	29.099124
338.663511	17873.815614	29.104141
338.971832	17913.693628	29.109159
339.235061	17930.292590	29.114176
339.684912	17982.973039	29.119194
340.396376	18014.670146	29.124212
340.805872	18046.806291	29.129229
341.048025	18078.160061	29.134247
341.719816	18105.719242	29.139264
341.751538	18128.697433	29.144282
341.930398	18157.332071	29.149300
342.845800	18183.438075	29.154317
342.803027	18213.895380	29.159335
343.474975	18232.591184	29.164352
343.722023	18262.510397	29.169370
344.126994	18280.161444	29.174388
344.531486	18305.835918	29.179405
344.687527	18327.449224	29.184423
345.000749	18341.488399	29.189440
345.521868	18373.266450	29.194458
345.506944	18389.985187	29.199476
346.089749	18414.216728	29.204493
346.168612	18445.034398	29.209511
346.607881	18464.108026	29.214528
346.694755	18496.459710	29.219546
347.048956	18526.173014	29.224564
347.560284	18550.782346	29.229581
347.849217	18590.930128	29.234599
348.571306	18612.145518	29.239616
348.630264	18651.091181	29.244634
348.509958	18676.469288	29.249652
349.371194	18697.290229	29.254669
349.495036	18734.924447	29.259687
350.019847	18761.269309	29.264704
349.962047	18789.449164	29.269722
350.320583	18817.999770	29.274740
350.497317	18850.047348	29.279757
350.876706	18893.201476	29.284775
351.244266	18920.834741	29.289792
351.586655	18971.835215	29.294810
352.162974	18992.164090	29.299828
352.806683	19029.723762	29.304845
352.917831	19069.413905	29.309863
353.810954	19093.085939	29.314880
354.004766	19122.029228	29.319898
354.338038	19159.802041	29.324916
354.974286	19188.107517	29.329933
354.834846	19222.416488	29.334951
355.189706	19245.705498	29.339968
355.302004	19285.882379	29.344986
356.039814	19308.258561	29.350004
356.504013	19344.318022	29.355021
357.067901	19380.974775	29.360039
357.121811	19400.690933	29.365056
357.133406	19442.305447	29.370074
357.413142	19469.618394	29.375092
357.738057	19494.359205	29.380109
358.225911	19551.845921	29.385127
358.458882	19571.635291	29.390144
359.176436	19616.349136	29.395162
359.882252	19650.286371	29.400180
359.759574	19682.110539	29.405197
360.086462	19715.544937	29.410215
360.811705	19745.322021	29.415232
361.001121	19780.717707	29.420250
361.448820	19810.835315	29.425268
362.224889	19842.171468	29.430285
362.164958	19864.117255	29.435303
362.911913	19894.592474	29.440320
362.904002	19935.181238	29.445338
363.253659	19957.347287	29.450356
363.570682	19986.544234	29.455373
363.854384	20024.572888	29.460391
364.327115	20062.451962	29.465408
364.586278	20093.679942	29.470426
365.138990	20118.480633	29.475444
365.654895	20157.376672	29.480461
365.949664	20189.123635	29.485479
366.301242	20223.945037	29.490496
366.832189	20253.532192	29.495514
367.266605	20279.413078	29.500532
367.503427	20304.800534	29.505549
367.510739	20333.572643	29.510567
368.286628	20351.401241	29.515584
368.533116	20380.799370	29.520602
368.527507	20408.006683	29.525620
369.105283	20433.448310	29.530637
369.244242	20476.422450	29.535655
369.889314	20489.109623	29.540672
370.251590	20528.245283	29.545690
370.653318	20551.427413	29.550708
370.899545	20582.209595	29.555725
371.047914	20615.787221	29.560743
371.257508	20652.388119	29.565760
371.892234	20691.348743	29.570778
372.314163	20719.746871	29.575796
372.860818	20751.783844	29.580813
372.939950	20790.869603	29.585831
373.323877	20817.119253	29.590848
373.692868	20854.188394	29.595866
374.137243	20891.018334	29.600884
374.772967	20922.220238	29.605901
374.696183	20946.817294	29.610919
375.263986	20986.035404	29.615936
375.652681	21017.750038	29.620954
376.039308	21054.671469	29.625972
376.411364	21084.550140	29.630989
376.603117	21133.507367	29.636007
376.512382	21165.234150	29.641024
376.980308	21205.081235	29.646042
377.421097	21242.032444	29.651060
377.993809	21286.867562	29.656077
378.840584	21332.601318	29.661095
379.185007	21359.300179	29.666112
379.477292	21398.416938	29.671130
379.798636	21424.809892	29.676148
380.614588	21461.115117	29.681165
380.540850	21499.531177	29.686183
381.342851	21530.126687	29.691200
381.518668	21559.360723	29.696218
381.741598	21590.944278	29.701236
382.491745	21620.120035	29.706253
382.555712	21668.131848	29.711271
383.169604	21700.873843	29.716288
383.438194	21745.852419	29.721306
383.862924	21782.832431	29.726324
384.166832	21815.206135	29.731341
384.198198	21854.333072	29.736359
385.063629	21883.156269	29.741376
385.236823	21923.853450	29.746394
385.495018	21960.076353	29.751412
386.326443	21994.610883	29.756429
386.106426	22033.069846	29.761447
386.286099	22060.812785	29.766464
387.082013	22110.056922	29.771482
387.531149	22145.567824	29.776500
387.951135	22187.345321	29.781517
388.188243	22219.711193	29.786535
388.507383	22263.393982	29.791552
388.889407	22300.154170	29.796570
389.517346	22337.823739	29.801588
390.074306	22369.482591	29.806605
390.411240	22410.774375	29.811623
390.751902	22455.105062	29.816640
391.192723	22492.703132	29.821658
391.424004	22527.737009	29.826676
391.952948	22557.195238	29.831693
392.144378	22599.552833	29.836711
392.631988	22638.230713	29.841728
393.185689	22663.792731	29.846746
393.291885	22706.163904	29.851764
393.662485	22728.317149	29.856781
393.987184	22767.968650	29.861799
393.844668	22809.020410	29.866816
394.714171	22836.643743	29.871834
394.511930	22882.362143	29.876852
395.529342	22912.907094	29.881869
395.919845	22956.510719	29.886887
396.407997	23003.334520	29.891904
396.601008	23025.408489	29.896922
397.060448	23073.551325	29.901940
397.644587	23110.433013	29.906957
397.796403	23150.870651	29.911975
398.271525	23185.216620	29.916992
398.735599	23225.599180	29.922010
398.941458	23267.810596	29.927028
399.653992	23305.967966	29.932045
400.116127	23345.738112	29.937063
400.051277	23383.284368	29.942080
401.063396	23418.052163	29.947098
401.216913	23461.302220	29.952116
401.740634	23498.478456	29.957133
402.260335	23545.197480	29.962151
402.613595	23577.654795	29.967168
402.995761	23611.624263	29.972186
402.915696	23653.470526	29.977204
403.606259	23686.557669	29.982221
404.186830	23735.972271	29.987239
404.300019	23771.652445	29.992256
405.005365	23808.592271	29.997274
405.111849	23852.330812	30.002292
405.657820	23879.936758	30.007309
406.215533	23935.459948	30.012327
406.429651	23969.311001	30.017344
407.278876	24002.057845	30.022362
407.807682	24058.224165	30.027380
407.931714	24098.352101	30.032397
408.145540	24120.796867	30.037415
408.909732	24156.792842	30.042432
409.170971	24193.638637	30.047450
409.227242	24248.286998	30.052468
409.992001	24287.228000	30.057485
410.784932	24312.236464	30.062503
410.933797	24358.383524	30.067520
411.671662	24395.230868	30.072538
411.533103	24431.128595	30.077556
412.009363	24459.416133	30.082573
412.276475	24493.733738	30.087591
413.030768	24536.070471	30.092608
413.563091	24579.882929	30.097626
413.866368	24617.260083	30.102644
414.330895	24649.537398	30.107661
414.990396	24682.940717	30.112679
415.359856	24729.736597	30.117696
415.644407	24758.098822	30.122714
416.048741	24791.049357	30.127732
416.154539	24836.389024	30.132749
416.619856	24862.599673	30.137767
417.201971	24907.296121	30.142784
417.371841	24944.214483	30.147802
417.809159	24993.875815	30.152820
418.296876	25023.053435	30.157837
418.723377	25066.940408	30.162855
418.899266	25114.311001	30.167872
419.721053	25142.937207	30.172890
419.988396	25183.455648	30.177908
420.254550	25222.710398	30.182925
420.535822	25251.648934	30.187943
421.036700	25289.002706	30.192960
421.355437	25330.613041	30.197978
421.622409	25357.740178	30.202996
422.172758	25402.177269	30.208013
422.636074	25451.696623	30.213031
422.842807	25494.146421	30.218048
423.283285	25518.023460	30.223066
423.475205	25571.466027	30.228084
424.448452	25614.200491	30.233101
424.994949	25655.434546	30.238119
425.180256	25693.192412	30.243136
425.709570	25737.740976	30.248154
425.924075	25779.861521	30.253172
426.459698	25821.862335	30.258189
426.952838	25850.951826	30.263207
427.112717	25900.589328	30.268224
427.690269	25934.133962	30.273242
428.119622	25981.782891	30.278260
428.354235	26026.959696	30.283277
428.592408	26067.370719	30.288295
429.091876	26121.082571	30.293312
429.816092	26163.528562	30.298330
430.497740	26215.720589	30.303348
430.975400	26249.445715	30.308365
431.361619	26294.706814	30.313383
431.738398	26341.498966	30.318400
432.585667	26371.323757	30.323418
432.715304	26413.345150	30.328436
433.001382	26454.773310	30.333453
433.334457	26491.738458	30.338471
433.663825	26538.475290	30.343488
434.452126	26589.867871	30.348506
434.575621	26636.036753	30.353524
435.066087	26678.014817	30.358541
435.690166	26720.724151	30.363559
435.857686	26768.378020	30.368576
436.275768	26816.334050	30.373594
437.339440	26855.492334	30.378612
437.885562	26898.839965	30.383629
438.214929	26935.743300	30.388647
438.636021	26984.116397	30.393664
439.090320	27020.911834	30.398682
439.483620	27055.043377	30.403700
439.992478	27092.607803	30.408717
440.535611	27136.809660	30.413735
441.049035	27173.602434	30.418752
441.405202	27211.323724	30.423770
441.746350	27254.666296	30.428788
441.976305	27291.844986	30.433805
442.924566	27334.195133	30.438823
443.072777	27384.280523	30.443840
443.660767	27423.824115	30.448858
443.521176	27448.679156	30.453876
444.013862	27492.478856	30.458893
444.814188	27537.690504	30.463911
445.176369	27581.605644	30.468928
445.597416	27622.819108	30.473946
446.158098	27664.301530	30.478964
446.422198	27697.891859	30.483981
446.584970	27741.566793	30.488999
447.195814	27787.263755	30.494016
447.713226	27835.396247	30.499034
447.967056	27878.178646	30.504052
448.358119	27926.034072	30.509069
449.242608	27970.683604	30.514087
449.391648	28018.267442	30.519104
449.591628	28049.011451	30.524122
450.368839	28099.372995	30.529140
450.402690	28138.492791	30.534157
450.888636	28176.530537	30.539175
451.106103	28232.498065	30.544192
452.174657	28267.632002	30.549210
452.524419	28316.923300	30.554228
452.849233	28349.064057	30.559245
453.727139	28397.710278	30.564263
454.072513	28444.430013	30.569280
454.450786	28472.909172	30.574298
454.673346	28516.342526	30.579316
454.713074	28564.918162	30.584333
455.371932	28603.112922	30.589351
455.943290	28655.435936	30.594368
456.707225	28686.990134	30.599386
456.978871	28749.220892	30.604404
456.948793	28788.528926	30.609421
457.875626	28835.973876	30.614439
458.010412	28890.445451	30.619456
458.734503	28932.511662	30.624474
459.417555	28981.259321	30.629492
459.790876	29027.375515	30.634509
459.921258	29072.234060	30.639527
460.021165	29130.915193	30.644544
460.740097	29163.608635	30.649562
461.511515	29221.369438	30.654580
461.728588	29275.367708	30.659597
462.421717	29333.115803	30.664615
463.025672	29375.347123	30.669632
463.401385	29417.765985	30.674650
464.246910	29473.436249	30.679668
464.129557	29519.554546	30.684685
464.781738	29565.602985	30.689703
465.210228	29619.657540	30.694720
465.970093	29664.785409	30.699738
466.298666	29711.308378	30.704756
466.511686	29757.141577	30.709773
467.076070	29808.273912	30.714791
467.590271	29856.089267	30.719808
468.013216	29904.323586	30.724826
468.654614	29961.683308	30.729844
468.887001	30011.850425	30.734861
469.699531	30060.080980	30.739879
470.211490	30114.964491	30.744896
470.560532	30153.343407	30.749914
471.018580	30211.080212	30.754932
471.518870	30261.888679	30.759949
471.799127	30309.729084	30.764967
472.479550	30353.549738	30.769984
473.179132	30405.117516	30.775002
473.929768	30456.987175	30.780020
473.942787	30505.862352	30.785037
474.180767	30544.644997	30.790055
474.741638	30600.065779	30.795072
475.414694	30643.003196	30.800090
475.960476	30698.831180	30.805108
475.983361	30753.255661	30.810125
476.847724	30792.364202	30.815143
476.936031	30848.131489	30.820160
477.184295	30893.133563	30.825178
478.355049	30959.408702	30.830196
478.869259	31009.413985	30.835213
479.033426	31042.222585	30.840231
479.746218	31094.415847	30.845248
480.115644	31150.765755	30.850266
480.398225	31198.057865	30.855284
481.224680	31251.535978	30.860301
481.553627	31281.727269	30.865319
481.819369	31330.994678	30.870336
482.480008	31383.177870	30.875354
483.229759	31418.898152	30.880372
483.349012	31462.701577	30.885389
483.891126	31505.560143	30.890407
484.372254	31551.273134	30.895424
484.421871	31604.943369	30.900442
485.299500	31652.307677	30.905460
485.613605	31702.984470	30.910477
486.428246	31753.570345	30.915495
486.432643	31807.911974	30.920512
487.019098	31862.377522	30.925530
487.509299	31902.817451	30.930548
487.758227	31960.446472	30.935565
488.619991	31992.224314	30.940583
488.898382	32050.493801	30.945600
489.441105	32107.166859	30.950618
490.070716	32154.400464	30.955636
490.312983	32212.505369	30.960653
491.026583	32263.816366	30.965671
491.709545	32314.272500	30.970688
492.022167	32381.008997	30.975706
492.679892	32424.312851	30.980724
492.915308	32476.628602	30.985741
493.617173	32526.361576	30.990759
493.699279	32570.767415	30.995776
494.361937	32632.714673	31.000794
494.934744	32690.958798	31.005812
495.188873	32752.565782	31.010829
495.797575	32812.302962	31.015847
496.582599	32858.793096	31.020864
496.930286	32919.911758	31.025882
497.917846	32971.440792	31.030900
498.057878	33028.773702	31.035917
498.411644	33081.382213	31.040935
498.950022	33127.949508	31.045952
499.604239	33190.102047	31.050970
499.971552	33244.978531	31.055988
500.478074	33301.698426	31.061005
501.214195	33356.043266	31.066023
501.532689	33406.356802	31.071040
501.954994	33469.747729	31.076058
503.074728	33512.178535	31.081076
503.422348	33571.528850	31.086093
503.989586	33620.615337	31.091111
504.158165	33675.290142	31.096128
504.651109	33728.548648	31.101146
505.532489	33778.035191	31.106164
505.544044	33833.493691	31.111181
506.373912	33885.732492	31.116199
506.912644	33941.709341	31.121216
507.263438	33997.083526	31.126234
508.172619	34044.347150	31.131252
508.440190	34102.680930	31.136269
508.918176	34156.094599	31.141287
509.265844	34211.944027	31.146304
509.653037	34260.529111	31.151322
510.562817	34314.975679	31.156340
510.779617	34376.074810	31.161357
511.556107	34420.691926	31.166375
512.022269	34467.772982	31.171392
512.054163	34533.554979	31.176410
512.714211	34581.143346	31.181428
513.241397	34641.821594	31.186445
513.758287	34700.168555	31.191463
514.221119	34755.419694	31.196480
514.505544	34811.135187	31.201498
515.188158	34868.893934	31.206516
515.450617	34925.688035	31.211533
515.785014	34971.678044	31.216551
516.460225	35027.111602	31.221568
516.874488	35087.372540	31.226586
517.791584	35145.474685	31.231604
518.188000	35195.362971	31.236621
518.662822	35254.944680	31.241639
519.287418	35305.556230	31.246656
519.271793	35372.094369	31.251674
520.252249	35433.361472	31.256692
520.853890	35486.392401	31.261709
521.231890	35537.770264	31.266727
521.687354	35584.653142	31.271744
521.848677	35660.307463	31.276762
522.527738	35716.014105	31.281780
523.266546	35780.165404	31.286797
523.708165	35840.392577	31.291815
524.219679	35906.122674	31.296832
524.708934	35968.157464	31.301850
525.823466	36022.557383	31.306868
525.990183	36091.073626	31.311885
526.635907	36143.840041	31.316903
527.543019	36203.578009	31.321920
527.569000	36263.624873	31.326938
528.529176	36321.609670	31.331956
528.841396	36388.858414	31.336973
529.418657	36438.632765	31.341991
529.987742	36486.119505	31.347008
530.215101	36551.010842	31.352026
531.318105	36607.747337	31.357044
531.382736	36667.643847	31.362061
532.228049	36722.233153	31.367079
532.597403	36776.808617	31.372096
532.906656	36839.076474	31.377114
533.787904	36898.744558	31.382132
534.595409	36965.108153	31.387149
534.893319	37029.496667	31.392167
535.558302	37075.312970	31.397184
535.991497	37141.305744	31.402202
536.795442	37192.949695	31.407220
537.110302	37250.235005	31.412237
537.303443	37308.146584	31.417255
537.966996	37365.839202	31.422272
538.284330	37434.683944	31.427290
538.691106	37496.521084	31.432308
539.559497	37561.814638	31.437325
540.146783	37629.112721	31.442343
540.761735	37684.587915	31.447360
541.251040	37756.473688	31.452378
541.760206	37795.499096	31.457396
542.418509	37870.798825	31.462413
542.882051	37924.780681	31.467431
543.479576	37988.126004	31.472448
543.820070	38053.320343	31.477466
543.948981	38104.901470	31.482484
544.493939	38173.086877	31.487501
545.341162	38242.837711	31.492519
546.140088	38314.676854	31.497536
546.635449	38382.839072	31.502554
547.351865	38436.036396	31.507572
547.680389	38502.467107	31.512589
548.218499	38568.726071	31.517607
548.958008	38632.974330	31.522624
549.191942	38693.343219	31.527642
549.963752	38762.652226	31.532660
550.624794	38822.676331	31.537677
551.242613	38888.778343	31.542695
551.958449	38944.886018	31.547712
551.653299	38995.082742	31.552730
552.661125	39051.897515	31.557748
553.043123	39111.921858	31.562765
553.830620	39167.892408	31.567783
554.591921	39217.751873	31.572800
554.803422	39291.709949	31.577818
555.688608	39345.003234	31.582836
556.072713	39397.394896	31.587853
556.517135	39452.825451	31.592871
557.217343	39515.153634	31.597888
557.525486	39579.946569	31.602906
557.922225	39623.369184	31.607924
558.517417	39695.554699	31.612941
559.270608	39762.744900	31.617959
559.927932	39818.269525	31.622976
560.628087	39883.090507	31.627994
560.978721	39950.148283	31.633012
561.756729	40018.309319	31.638029
561.887313	40078.363057	31.643047
562.646928	40136.806938	31.648064
562.883624	40209.050302	31.653082
563.334611	40267.245626	31.658100
564.053738	40332.944055	31.663117
564.304011	40414.691469	31.668135
565.315329	40475.594964	31.673152
565.832223	40546.884849	31.678170
566.205166	40614.358583	31.683188
566.918810	40695.547494	31.688205
567.145507	40759.079147	31.693223
568.141238	40823.110341	31.698240
568.670597	40908.281710	31.703258
569.233677	40963.741792	31.708276
569.968191	41035.581043	31.713293
570.587508	41109.753365	31.718311
571.135800	41190.299603	31.723328
571.587957	41254.771369	31.728346
572.415763	41317.527440	31.733364
573.106592	41388.881369	31.738381
573.132857	41452.244032	31.743399
574.144541	41517.229783	31.748416
574.800830	41591.012135	31.753434
575.206880	41654.258977	31.758452
575.889957	41719.916616	31.763469
576.425888	41802.067194	31.768487
577.148686	41859.028794	31.773504
577.489336	41941.621588	31.778522
577.986001	42001.996423	31.783540
578.725682	42070.005403	31.788557
579.157003	42134.388139	31.793575
580.062213	42209.607274	31.798592
580.176197	42270.953563	31.803610
580.916216	42345.806889	31.808628
581.739861	42408.826047	31.813645
582.465700	42490.829275	31.818663
582.854086	42546.782432	31.823680
583.534313	42625.915437	31.828698
584.165455	42689.610697	31.833716
584.418194	42752.340746	31.838733
585.245649	42824.278806	31.843751
585.776077	42892.626695	31.848768
586.454610	42953.519606	31.853786
586.830426	43030.342470	31.858804
587.858677	43089.144294	31.863821
587.830540	43161.641231	31.868839
588.481583	43225.866230	31.873856
588.858070	43309.717230	31.878874
589.602670	43370.980453	31.883892
590.465734	43447.418516	31.888909
590.847987	43522.319201	31.893927
591.842748	43583.834796	31.898944
592.170926	43645.771221	31.903962
592.498418	43699.004295	31.908980
593.271089	43760.321123	31.913997
593.770250	43841.517255	31.919015
594.597656	43894.773709	31.924032
594.896805	43972.332929	31.929050
595.645725	44034.223517	31.934068
596.379903	44093.662322	31.939085
596.397240	44182.829288	31.944103
597.481991	44240.644869	31.949120
598.064170	44311.468600	31.954138
598.558270	44371.084904	31.959156
598.956374	44445.619332	31.964173
599.232601	44513.727365	31.969191
600.109728	44590.432823	31.974208
600.522460	44665.946157	31.979226
601.221216	44748.461678	31.984244
601.802457	44819.900751	31.989261
602.102937	44898.468751	31.994279
603.063681	44975.402809	31.999296
603.635788	45063.619782	32.004314
603.957836	45137.004494	32.009332
604.811799	45207.130621	32.014349
605.220085	45297.562876	32.019367
606.204941	45368.326887	32.024384
607.068633	45455.462307	32.029402
607.475802	45531.846064	32.034420
608.304773	45598.605661	32.039437
608.950849	45680.633121	32.044455
609.624808	45744.634045	32.049472
610.317571	45829.558320	32.054490
611.007989	45900.313186	32.059508
611.503111	45971.895931	32.064525
612.162154	46050.525671	32.069543
612.877736	46124.136640	32.074560
613.610075	46194.468350	32.079578
614.503978	46269.924370	32.084596
615.018296	46335.078008	32.089613
615.604154	46397.804070	32.094631
615.926174	46470.003830	32.099648
616.672611	46546.040564	32.104666
617.185820	46608.924091	32.109684
617.807765	46674.314897	32.114701
618.567758	46759.276425	32.119719
619.008602	46826.252272	32.124736
619.720821	46903.858138	32.129754
620.267382	46979.813761	32.134772
621.043711	47041.556517	32.139789
621.707361	47121.764500	32.144807
622.036700	47192.213038	32.149824
622.472790	47271.501917	32.154842
623.510365	47347.008620	32.159860
624.218593	47418.695422	32.164877
624.572276	47496.213959	32.169895
625.327547	47563.231308	32.174912
625.991509	47633.198613	32.179930
626.719841	47709.937993	32.184948
627.398863	47771.021045	32.189965
627.738566	47854.426596	32.194983
628.474543	47931.330014	32.200000
629.273106	47999.493292	32.205018
629.826003	48078.703426	32.210036
630.616052	48136.461290	32.215053
630.980230	48209.311612	32.220071
631.793629	48286.419206	32.225088
632.471464	48348.630127	32.230106
632.762890	48422.258042	32.235124
633.785275	48477.873615	32.240141
634.065632	48551.990833	32.245159
634.559223	48615.401769	32.250176
634.656128	48685.903978	32.255194
635.125317	48761.883989	32.260212
636.130526	48834.724486	32.265229
636.989002	48896.345527	32.270247
637.575292	48976.363369	32.275264
638.106858	49057.762979	32.280282
638.872557	49134.488641	32.285300
639.949682	49203.130685	32.290317
640.246928	49283.587130	32.295335
640.708975	49352.224716	32.300352
641.660046	49420.399981	32.305370
642.134293	49503.885376	32.310388
643.332149	49578.773303	32.315405
643.481443	49655.799703	32.320423
644.113860	49729.593529	32.325440
644.870969	49801.248513	32.330458
645.404815	49876.203435	32.335476
646.236685	49939.659958	32.340493
646.756868	50033.155806	32.345511
647.358042	50105.772566	32.350528
648.206366	50180.299602	32.355546
648.618667	50256.692071	32.360564
649.353339	50335.090634	32.365581
649.758260	50419.387423	32.370599
650.391780	50496.809008	32.375616
651.054141	50574.454116	32.380634
651.927835	50660.677776	32.385652
652.813502	50729.183519	32.390669
653.141246	50824.389431	32.395687
654.220145	50898.015832	32.400704
654.522000	50964.804089	32.405722
655.039030	51060.152163	32.410740
655.823634	51142.101617	32.415757
656.316496	51222.749312	32.420775
657.124695	51299.336315	32.425792
658.122395	51385.296481	32.430810
658.538740	51461.154453	32.435828
659.389845	51538.589734	32.440845
659.899976	51621.817724	32.445863
660.821748	51707.189857	32.450880
661.576278	51777.497271	32.455898
662.219868	51863.172970	32.460916
662.696388	51934.935447	32.465933
663.529236	52013.109167	32.470951
664.363916	52094.060696	32.475968
664.834229	52167.096715	32.480986
665.791167	52244.163418	32.486004
666.263038	52325.672456	32.491021
666.953519	52393.947910	32.496039
667.580392	52485.861319	32.501056
668.276175	52549.333638	32.506074
668.944641	52633.559210	32.511092
669.619482	52705.255027	32.516109
670.211366	52785.671144	32.521127
670.898623	52869.217543	32.526144
671.565835	52934.739277	32.531162
672.017373	53020.702408	32.536180
673.083875	53102.190632	32.541197
673.410286	53185.560535	32.546215
674.187948	53256.463599	32.551232
674.795129	53333.765845	32.556250
675.670949	53412.968971	32.561268
676.348386	53500.113455	32.566285
677.069025	53573.563942	32.571303
677.762028	53645.886263	32.576320
678.231608	53717.459114	32.581338
678.792557	53791.599738	32.586356
679.549120	53846.839520	32.591373
680.086477	53918.199866	32.596391
680.815517	53994.181602	32.601408
681.576803	54068.304378	32.606426
681.786724	54144.045155	32.611444
682.404504	54220.791770	32.616461
683.126632	54309.330780	32.621479
683.878803	54392.264907	32.626496
684.707980	54471.972499	32.631514
684.912343	54556.049811	32.636532
685.752123	54636.224590	32.641549
686.414187	54735.102425	32.646567
687.156410	54824.235079	32.651584
688.074224	54896.570321	32.656602
688.887124	54988.065669	32.661620
688.822059	55067.079952	32.666637
689.960692	55160.436142	32.671655
690.446324	55246.085608	32.676672
691.434552	55338.061126	32.681690
691.721596	55430.956860	32.686708
692.557630	55517.400452	32.691725
693.751815	55605.016015	32.696743
694.117106	55694.571689	32.701760
695.126062	55782.881418	32.706778
695.918042	55865.877742	32.711796
696.167389	55955.680383	32.716813
696.828165	56047.134009	32.721831
698.006945	56138.373961	32.726848
698.945523	56231.923898	32.731866
699.497026	56312.219084	32.736884
700.261892	56394.354449	32.741901
700.773770	56477.118293	32.746919
701.455448	56577.209501	32.751936
702.482259	56665.285528	32.756954
703.068799	56749.532231	32.761972
703.578315	56825.025759	32.766989
704.128600	56915.936732	32.772007
704.582727	57008.261806	32.777024
705.678213	57104.885436	32.782042
706.438574	57201.448013	32.787060
706.818106	57286.817606	32.792077
708.012208	57388.515469	32.797095
708.383825	57489.291936	32.802112
709.048717	57566.814080	32.807130
710.017519	57648.510405	32.812148
710.783721	57735.574200	32.817165
711.518445	57836.048416	32.822183
712.049203	57927.238417	32.827200
713.032212	58016.592087	32.832218
713.725618	58100.617916	32.837236
714.169331	58193.227641	32.842253
715.236975	58286.233698	32.847271
715.906000	58377.422730	32.852288
716.768888	58452.429290	32.857306
717.138489	58548.267278	32.862324
717.658917	58642.347774	32.867341
718.544189	58720.870794	32.872359
719.033561	58828.805608	32.877376
720.082214	58914.158440	32.882394
720.687187	59002.201453	32.887412
721.527055	59102.702430	32.892429
722.145985	59181.933247	32.897447
722.914631	59270.863052	32.902464
724.095953	59359.722228	32.907482
724.447161	59444.540524	32.912500
724.995175	59530.258747	32.917517
726.008584	59606.365637	32.922535
726.821406	59686.137396	32.927552
727.336883	59767.652331	32.932570
728.006451	59856.346598	32.937588
728.425290	59938.497546	32.942605
729.152122	60017.790135	32.947623
729.853684	60113.734204	32.952640
731.204492	60194.518423	32.957658
731.510091	60284.986611	32.962676
732.111954	60367.958531	32.967693
732.962909	60462.696894	32.972711
733.391489	60551.349128	32.977728
734.139991	60634.969954	32.982746
734.903321	60737.426582	32.987764
735.574707	60832.409708	32.992781
736.631984	60923.876608	32.997799
737.455833	61022.026896	33.002816
738.189126	61115.931652	33.007834
738.784811	61202.724358	33.012852
739.012247	61295.291084	33.017869
740.144613	61387.444253	33.022887
740.929770	61486.203806	33.027904
741.932456	61579.859249	33.032922
742.596789	61681.278169	33.037940
743.102952	61776.366765	33.042957
743.871877	61873.718775	33.047975
744.558847	61977.509194	33.052992
745.436104	62073.186502	33.058010
746.063481	62163.155408	33.063028
746.974035	62272.495363	33.068045
747.957547	62365.517418	33.073063
748.563493	62470.474709	33.078080
749.402823	62564.805152	33.083098
750.391229	62654.504069	33.088116
750.779236	62750.368217	33.093133
751.805433	62841.739457	33.098151
752.094209	62950.268173	33.103168
752.984052	63039.730693	33.108186
753.807197	63141.156026	33.113204
754.479227	63253.449688	33.118221
755.704427	63336.498542	33.123239
756.350527	63447.455052	33.128256
756.949642	63539.098305	33.133274
757.662671	63635.073217	33.138292
758.760590	63734.989218	33.143309
759.641082	63831.204548	33.148327
760.121623	63940.302616	33.153344
760.772451	64034.541515	33.158362
761.624507	64130.572523	33.163380
762.495926	64231.659183	33.168397
762.645042	64328.161878	33.173415
763.391543	64432.339361	33.178432
764.551466	64533.198460	33.183450
765.367816	64635.878089	33.188468
766.089239	64744.745667	33.193485
767.410144	64835.666521	33.198503
767.738007	64929.161642	33.203520
768.439973	65023.320263	33.208538
769.284877	65130.296189	33.213556
770.240925	65231.284972	33.218573
771.117847	65334.325160	33.223591
771.449423	65427.277068	33.228608
772.125951	65512.685570	33.233626
773.054887	65611.280616	33.238644
773.771270	65719.133862	33.243661
774.701365	65820.578573	33.248679
775.614798	65915.872341	33.253696
776.862327	66015.919573	33.258714
777.086319	66109.049106	33.263732
777.771497	66190.507816	33.268749
778.662112	66271.383793	33.273767
779.369409	66365.267984	33.278784
780.145570	66455.330255	33.283802
780.916611	66556.498903	33.288820
781.181111	66657.892895	33.293837
782.324326	66743.042508	33.298855
782.777887	66844.857169	33.303872
783.835380	66937.523639	33.308890
784.352584	67038.670631	33.313908
784.916079	67143.805973	33.318925
786.040988	67242.009415	33.323943
786.676347	67348.495630	33.328960
787.688118	67444.666132	33.333978
788.335344	67552.322682	33.338996
789.037074	67661.281803	33.344013
789.998576	67758.442761	33.349031
790.776270	67867.422519	33.354048
791.936368	67973.006030	33.359066
792.410212	68078.944375	33.364084
793.072276	68176.704666	33.369101
793.985035	68274.824975	33.374119
794.519855	68392.734856	33.379136
795.571173	68500.465063	33.384154
796.043693	68613.364534	33.389172
796.920309	68716.842637	33.394189
797.937116	68817.221875	33.399207
798.899450	68926.120204	33.404224
799.415811	69050.507252	33.409242
800.402142	69162.505500	33.414260
801.216180	69275.291057	33.419277
802.072532	69370.416627	33.424295
802.840963	69486.870189	33.429312
803.132924	69593.938669	33.434330
804.264347	69700.375897	33.439348
805.315528	69819.224553	33.444365
806.234277	69929.526997	33.449383
806.915048	70037.194965	33.454400
807.814824	70150.262172	33.459418
808.664691	70261.425330	33.464436
809.285032	70368.496226	33.469453
810.592697	70470.216748	33.474471
811.360974	70590.487336	33.479488
812.151499	70696.317108	33.484506
812.867054	70797.561704	33.489524
813.892100	70904.824718	33.494541
814.499902	71015.547716	33.499559
815.126917	71122.190038	33.504576
815.985045	71228.492641	33.509594
817.331119	71335.909788	33.514612
817.589212	71456.251566	33.519629
818.816812	71550.807665	33.524647
819.822779	71667.107080	33.529664
820.337391	71774.086275	33.534682
821.044918	71878.147990	33.539700
822.250282	71988.034249	33.544717
822.870567	72087.158265	33.549735
823.873520	72202.662587	33.554752
824.929853	72309.293146	33.559770
825.664631	72415.125888	33.564788
826.138696	72517.377492	33.569805
827.325398	72623.444277	33.574823
827.631153	72715.463758	33.579840
828.391405	72820.166873	33.584858
829.317228	72929.011548	33.589876
829.838750	73050.560576	33.594893
831.031118	73141.910733	33.599911
832.152126	73247.635649	33.604928
832.750629	73347.895061	33.609946
833.590368	73447.787756	33.614964
834.187686	73541.411032	33.619981
835.314531	73649.239212	33.624999
835.854451	73754.208491	33.630016
836.450678	73851.316248	33.635034
837.624017	73960.633029	33.640052
838.267790	74072.135804	33.645069
838.965515	74177.056697	33.650087
839.449182	74289.801429	33.655104
840.125804	74398.729115	33.660122
841.352471	74498.894477	33.665140
842.050382	74629.657027	33.670157
843.101609	74736.412088	33.675175
843.882719	74851.911950	33.680192
844.848839	74976.490797	33.685210
845.566068	75077.232090	33.690228
846.592318	75199.636514	33.695245
847.151379	75315.768478	33.700263
847.998741	75435.757252	33.705280
849.050773	75554.283125	33.710298
849.864894	75673.366126	33.715316
850.580719	75799.710695	33.720333
851.622489	75908.308619	33.725351
852.807271	76033.149443	33.730368
853.544464	76146.837615	33.735386
854.740222	76242.454025	33.740404
854.988719	76382.542650	33.745421
856.004060	76496.391409	33.750439
856.980644	76608.333905	33.755456
857.627168	76743.675046	33.760474
858.532391	76845.508224	33.765492
859.614906	76963.731447	33.770509
860.114615	77093.029447	33.775527
861.463351	77215.962512	33.780544
861.622618	77344.757621	33.785562
862.900630	77458.024538	33.790580
863.695961	77586.049778	33.795597
864.848596	77715.235808	33.800615
865.852206	77825.608207	33.805632
866.290758	77956.173999	33.810650
867.350589	78067.476015	33.815668
868.429131	78195.041693	33.820685
869.256412	78316.325775	33.825703
870.570281	78426.259282	33.830720
870.877935	78556.721729	33.835738
872.123050	78675.800989	33.840756
872.993761	78782.397462	33.845773
873.544162	78901.852515	33.850791
874.785646	79024.367052	33.855808
875.597030	79140.577084	33.860826
876.281863	79255.692561	33.865844
877.124580	79374.090371	33.870861
878.477529	79502.594616	33.875879
879.233080	79620.576381	33.880896
880.030340	79747.040376	33.885914
881.096794	79852.989528	33.890932
881.832197	79971.356006	33.895949
882.693418	80089.728624	33.900967
883.717549	80207.784843	33.905984
884.319360	80321.536775	33.911002
885.649274	80440.825699	33.916020
886.069378	80553.428776	33.921037
887.194366	80672.066624	33.926055
888.213652	80786.122490	33.931072
888.744011	80904.106926	33.936090
889.648470	81005.208025	33.941108
890.393658	81123.400466	33.946125
891.121393	81237.858568	33.951143
892.448152	81341.656753	33.956160
893.149437	81460.503642	33.961178
893.997267	81568.406656	33.966196
894.848511	81685.381212	33.971213
895.549115	81788.860979	33.976231
896.437200	81909.897756	33.981248
897.501720	82035.798075	33.986266
898.292850	82150.211941	33.991284
899.020803	82261.722019	33.996301
899.842167	82388.257476	34.001319
901.162177	82506.112293	34.006336
901.605930	82623.889406	34.011354
902.549946	82753.372145	34.016372
903.138082	82890.741539	34.021389
904.154973	83012.776489	34.026407
905.122156	83134.604344	34.031424
905.630167	83268.617734	34.036442
906.844273	83396.515288	34.041460
907.588084	83538.652944	34.046477
908.628601	83666.743608	34.051495
909.930752	83789.091991	34.056512
910.364581	83921.181410	34.061530
911.796511	84057.575340	34.066548
912.353242	84197.692858	34.071565
913.315883	84323.112385	34.076583
914.244708	84454.328470	34.081600
915.036604	84588.835764	34.086618
915.978195	84725.030869	34.091636
917.007505	84867.903344	34.096653
917.717156	85004.148753	34.101671
918.779057	85138.552975	34.106688
919.585381	85284.617614	34.111706
920.707355	85408.420299	34.116724
921.983599	85558.277568	34.121741
922.744724	85686.965835	34.126759
923.993484	85817.517097	34.131776
924.689680	85963.120867	34.136794
925.922107	86084.273402	34.141812
926.761522	86220.060684	34.146829
927.738513	86365.901283	34.151847
928.885430	86486.308558	34.156864
929.732033	86631.372560	34.161882
930.760991	86756.640161	34.166900
931.746953	86878.569567	34.171917
932.574860	87009.939719	34.176935
934.017230	87143.850092	34.181952
934.379909	87271.898077	34.186970
935.317863	87392.810674	34.191988
936.199781	87522.717332	34.197005
937.343534	87664.166271	34.202023
938.350863	87787.249304	34.207040
939.215339	87934.458610	34.212058
939.910348	88059.365851	34.217076
940.931180	88201.863102	34.222093
941.937830	88335.365548	34.227111
942.982255	88457.761232	34.232128
943.793546	88597.986733	34.237146
945.082038	88724.540048	34.242164
945.956595	88856.380013	34.247181
946.499661	88985.395668	34.252199
947.841094	89124.666203	34.257216
948.781766	89251.884534	34.262234
949.566940	89379.533299	34.267252
950.714449	89514.501758	34.272269
951.298384	89652.448601	34.277287
952.639261	89768.846764	34.282304
953.141970	89902.156322	34.287322
953.957146	90013.226163	34.292340
955.102149	90143.812805	34.297357
955.913206	90269.585620	34.302375
956.794674	90389.429316	34.307392
957.996275	90529.716833	34.312410
958.937020	90647.017521	34.317428
959.696040	90776.374616	34.322445
960.688792	90909.104955	34.327463
961.362435	91027.944468	34.332480
962.299600	91170.912557	34.337498
963.552121	91312.539188	34.342516
964.158780	91445.940690	34.347533
965.041476	91585.750729	34.352551
965.874155	91718.205496	34.357568
966.858231	91869.217689	34.362586
968.053562	92003.708183	34.367604
969.274831	92143.049519	34.372621
970.127127	92280.129831	34.377639
971.043199	92428.861362	34.382656
971.469654	92563.994367	34.387674
972.679768	92715.380946	34.392692
973.837673	92859.501150	34.397709
974.512429	93008.438051	34.402727
975.781508	93156.217934	34.407744
976.817732	93307.444539	34.412762
978.059462	93457.967938	34.417780
978.969242	93598.746240	34.422797
979.922064	93742.813972	34.427815
980.961020	93895.069717	34.432832
981.846808	94040.898506	34.437850
982.844992	94181.919131	34.442868
983.896377	94329.117631	34.447885
984.647784	94483.373294	34.452903
985.930962	94625.010434	34.457920
986.785994	94774.827585	34.462938
988.076914	94925.502529	34.467956
989.007523	95076.716290	34.472973
989.763555	95232.077721	34.477991
990.912329	95379.646217	34.483008
991.709179	95533.735181	34.488026
992.842769	95680.331434	34.493044
994.031574	95832.522498	34.498061
995.350240	95983.667211	34.503079
996.190730	96125.710047	34.508096
997.204254	96274.026466	34.513114
998.356586	96426.606403	34.518132
999.329118	96565.410798	34.523149
1000.310898	96717.524472	34.528167
1001.480125	96868.151749	34.533184
1002.166743	97008.625432	34.538202
1003.428925	97157.274687	34.543220
1004.645243	97296.690625	34.548237
1005.799313	97445.890576	34.553255
1006.842599	97593.232428	34.558272
1007.747712	97732.901832	34.563290
1009.104510	97865.566941	34.568308
1010.161944	98001.410647	34.573325
1010.495250	98144.720890	34.578343
1011.863711	98288.478199	34.583360
1013.137953	98429.043628	34.588378
1013.851004	98566.160644	34.593396
1014.783836	98715.781485	34.598413
1015.364714	98853.414830	34.603431
1016.409858	98994.145377	34.608448
1016.956195	99140.710115	34.613466
1018.332588	99298.783347	34.618484
1019.660549	99423.105065	34.623501
1020.689434	99570.623075	34.628519
1021.691704	99705.202209	34.633536
1022.705219	99843.088980	34.638554
1023.447129	99978.863672	34.643572
1024.628695	100115.432177	34.648589
1025.464852	100251.383418	34.653607
1026.570285	100392.414883	34.658624
1027.686296	100542.814206	34.663642
1028.097961	100678.174445	34.668660
1029.498534	100820.720935	34.673677
1030.096479	100966.436426	34.678695
1031.159431	101118.139864	34.683712
1032.106852	101265.843137	34.688730
1032.996069	101428.972826	34.693748
1034.066316	101574.287443	34.698765
1035.105857	101736.330155	34.703783
1036.268913	101891.165709	34.708800
1037.411914	102054.322161	34.713818
1037.900957	102224.504247	34.718836
1039.314242	102364.988868	34.723853
1040.481690	102524.416332	34.728871
1041.522136	102685.588744	34.733888
1042.335336	102859.450865	34.738906
1043.465552	103021.181395	34.743924
1044.637820	103179.622312	34.748941
1045.534270	103343.457657	34.753959
1046.717475	103517.442794	34.758976
1047.544318	103671.806792	34.763994
1048.498116	103842.177981	34.769012
1050.018531	104001.519227	34.774029
1050.551544	104168.078136	34.779047
1051.708455	104336.695669	34.784064
1053.001995	104508.006034	34.789082
1054.288046	104674.969412	34.794100
1055.251169	104846.536101	34.799117
1056.450887	105018.573803	34.804135
1057.823683	105177.576028	34.809152
1058.966893	105332.861771	34.814170
1059.899257	105507.112033	34.819188
1061.317711	105667.694375	34.824205
1061.987070	105826.404022	34.829223
1063.200738	105994.703946	34.834240
1064.417773	106153.278654	34.839258
1065.539978	106313.263747	34.844276
1066.610677	106480.421891	34.849293
1067.422784	106651.983302	34.854311
1068.562883	106805.019182	34.859328
1069.996621	106972.566698	34.864346
1070.749145	107137.812423	34.869364
1072.130543	107284.130138	34.874381
1073.440357	107451.559906	34.879399
1074.413337	107609.215845	34.884416
1075.439909	107768.449180	34.889434
1076.388423	107932.932559	34.894452
1077.679447	108083.414369	34.899469
1078.515828	108242.641620	34.904487
1079.827188	108408.363881	34.909504
1080.734674	108565.539874	34.914522
1082.095065	108722.645671	34.919540
1083.475998	108876.946470	34.924557
1084.544220	109044.548561	34.929575
1085.329517	109195.963985	34.934592
1086.534547	109353.058898	34.939610
1087.288267	109516.489673	34.944628
1088.548205	109666.539341	34.949645
1089.567882	109830.272331	34.954663
1090.656216	109982.658209	34.959680
1092.118230	110127.542261	34.964698
1092.583274	110284.579646	34.969716
1093.814559	110424.517229	34.974733
1094.660416	110578.706369	34.979751
1095.582702	110721.052270	34.984768
1096.613428	110874.807944	34.989786
1097.442266	111036.407832	34.994804
1098.913173	111193.279083	34.999821
1099.844113	111351.465699	35.004839
1101.013021	111517.377080	35.009856
1102.104102	111675.159602	35.014874
1102.794234	111848.109864	35.019892
1104.282397	112002.800665	35.024909
1105.065975	112171.590822	35.029927
1105.649969	112331.560853	35.034944
1107.120550	112504.696464	35.039962
1108.198283	112683.233661	35.044980
1109.404448	112853.419319	35.049997
1110.946266	113024.301494	35.055015
1112.150450	113191.178939	35.060032
1112.858904	113373.569417	35.065050
1114.162966	113537.198767	35.070068
1115.376193	113704.089836	35.075085
1115.901996	113885.928074	35.080103
1117.298149	114060.186164	35.085120
1118.190847	114233.572691	35.090138
1119.528145	114427.119674	35.095156
1120.981708	114598.403538	35.100173
1121.922021	114788.818470	35.105191
1122.860239	114956.772946	35.110208
1124.306931	115140.565944	35.115226
1125.349295	115319.540118	35.120244
1126.805156	115485.893977	35.125261
1127.733298	115673.195290	35.130279
1128.555645	115854.958779	35.135296
1130.248586	116036.092209	35.140314
1131.229562	116222.677746	35.145332
1132.704493	116396.566715	35.150349
1133.608990	116582.633314	35.155367
1134.533624	116758.106787	35.160384
1135.952512	116933.199295	35.165402
1137.097899	117122.122760	35.170420
1138.176736	117287.643128	35.175437
1139.513388	117472.466882	35.180455
1140.379719	117655.817722	35.185472
1141.619887	117840.569595	35.190490
1142.506186	118024.857720	35.195508
1143.913034	118201.797203	35.200525
1145.043084	118390.539148	35.205543
1146.026021	118570.362617	35.210560
1147.477683	118748.464585	35.215578
1148.584912	118937.314286	35.220596
1149.813293	119115.224600	35.225613
1150.975170	119301.023261	35.230631
1151.750103	119480.655251	35.235648
1153.090296	119664.195262	35.240666
1154.067110	119847.754980	35.245684
1155.561556	120031.158428	35.250701
1156.619734	120216.292761	35.255719
1157.618384	120402.236449	35.260736
1158.969306	120586.337297	35.265754
1160.055391	120766.015344	35.270772
1161.159439	120945.475763	35.275789
1162.732498	121132.182920	35.280807
1163.377337	121323.108238	35.285824
1165.070360	121505.599591	35.290842
1165.939321	121685.671048	35.295860
1167.568805	121860.245664	35.300877
1168.675311	122028.864654	35.305895
1169.836878	122209.082982	35.310912
1170.949650	122366.488449	35.315930
1171.737467	122547.629450	35.320948
1172.859779	122698.882223	35.325965
1173.954104	122883.757105	35.330983
1174.964902	123053.346874	35.336000
1176.164828	123224.024112	35.341018
1177.339344	123410.702962	35.346036
1178.492333	123585.829157	35.351053
1180.126380	123769.570723	35.356071
1180.920160	123953.064091	35.361088
1182.050026	124133.625935	35.366106
1183.100269	124320.759808	35.371124
1184.187642	124500.315055	35.376141
1185.247051	124678.175515	35.381159
1186.372066	124872.366504	35.386176
1187.809886	125064.187841	35.391194
1188.810145	125261.038995	35.396212
1190.104859	125443.623403	35.401229
1191.363482	125630.451600	35.406247
1192.627121	125832.212050	35.411264
1193.937454	126024.476526	35.416282
1194.961786	126220.135984	35.421300
1196.224355	126409.035059	35.426317
1197.342856	126603.920392	35.431335
1198.251059	126810.359317	35.436352
1199.795228	127000.016295	35.441370
1200.965144	127208.255851	35.446388
1202.144669	127395.142504	35.451405
1203.265201	127602.389485	35.456423
1204.152895	127811.627784	35.461440
1205.972020	128014.111227	35.466458
1207.462699	128209.364512	35.471476
1208.388178	128403.298882	35.476493
1209.642632	128610.770955	35.481511
1210.483450	128808.869260	35.486528
1211.931395	129016.110038	35.491546
1213.348805	129219.918251	35.496564
1214.538998	129417.469895	35.501581
1215.632948	129631.582418	35.506599
1217.040430	129834.227857	35.511616
1218.525791	130027.828268	35.516634
1219.467685	130232.502423	35.521652
1220.378269	130434.847858	35.526669
1222.155242	130640.662041	35.531687
1223.070231	130841.968280	35.536704
1224.156548	131054.249327	35.541722
1225.347709	131265.499943	35.546740
1226.711305	131469.175029	35.551757
1228.133880	131680.099607	35.556775
1229.040169	131885.535792	35.561792
1230.748010	132089.540551	35.566810
1231.912429	132292.844639	35.571828
1233.253071	132493.914261	35.576845
1234.838499	132698.461256	35.581863
1235.509431	132911.768031	35.586880
1237.008056	133115.721493	35.591898
1238.268337	133318.406254	35.596916
1239.340562	133523.354635	35.601933
1240.825771	133719.357017	35.606951
1241.730125	133927.937218	35.611968
1243.552778	134120.690902	35.616986
1245.060653	134331.665583	35.622004
1246.025290	134528.146374	35.627021
1247.194903	134729.874680	35.632039
1248.219428	134933.098567	35.637056
1249.875291	135128.699729	35.642074
1250.937751	135319.762982	35.647092
1252.106862	135508.792716	35.652109
1253.516452	135682.849991	35.657127
1254.589784	135874.586427	35.662144
1255.527016	136057.144975	35.667162
1256.904428	136250.434287	35.672180
1258.329991	136437.371999	35.677197
1259.505605	136625.542444	35.682215
1260.559314	136829.062100	35.687232
1261.669104	137016.812994	35.692250
1263.217047	137221.970158	35.697268
1264.211555	137417.862314	35.702285
1265.380330	137613.766090	35.707303
1266.402373	137818.297573	35.712320
1267.607192	138025.618567	35.717338
1268.960543	138244.414600	35.722356
1269.810972	138454.864015	35.727373
1271.222720	138663.614830	35.732391
1272.596722	138878.172005	35.737408
1273.764184	139083.270009	35.742426
1275.073372	139313.892772	35.747444
1276.618396	139537.169953	35.752461
1277.669260	139750.893328	35.757479
1278.847527	139969.305975	35.762496
1279.984007	140186.533230	35.767514
1281.330682	140425.759857	35.772532
1282.723214	140636.121398	35.777549
1284.487260	140847.517126	35.782567
1285.572807	141089.656085	35.787584
1287.094739	141311.536448	35.792602
1287.927553	141538.894046	35.797620
1289.246167	141763.790719	35.802637
1290.869846	141979.337992	35.807655
1292.267218	142207.282969	35.812672
1293.296933	142434.233175	35.817690
1294.738861	142657.883590	35.822708
1295.954574	142886.418576	35.827725
1297.832584	143099.100750	35.832743
1298.805911	143345.075890	35.837760
1300.023152	143562.863975	35.842778
1301.321626	143786.046964	35.847796
1302.995623	144021.686248	35.852813
1304.241013	144240.475530	35.857831
1305.342561	144471.954777	35.862848
1306.486632	144698.021664	35.867866
1307.987768	144919.248788	35.872884
1309.279759	145153.366663	35.877901
1311.053864	145374.007282	35.882919
1311.931997	145606.516666	35.887936
1313.047108	145822.591664	35.892954
1314.466175	146056.998406	35.897972
1315.875199	146293.007022	35.902989
1317.315599	146514.491713	35.908007
1318.558484	146748.396097	35.913024
1320.169478	146977.801538	35.918042
1321.358591	147200.927751	35.923060
1322.594059	147435.521783	35.928077
1324.517950	147662.456969	35.933095
1325.550202	147895.485595	35.938112
1326.819528	148114.934947	35.943130
1328.188187	148353.104283	35.948148
1329.495631	148585.026677	35.953165
1330.900291	148799.875552	35.958183
1332.355235	149027.816592	35.963200
1333.081885	149252.737423	35.968218
1334.939803	149483.143242	35.973236
1336.070956	149709.614694	35.978253
1337.456860	149938.408158	35.983271
1338.854512	150156.208386	35.988288
1339.915540	150362.422416	35.993306
1342.024663	150564.500149	35.998324
1342.897925	150788.566658	36.003341
1343.736157	151007.371783	36.008359
1345.414016	151213.708264	36.013376
1346.906190	151425.113927	36.018394
1348.062867	151642.881636	36.023412
1349.312587	151874.750985	36.028429
1350.893218	152091.832109	36.033447
1351.845073	152302.589461	36.038464
1352.859685	152520.002032	36.043482
1354.418866	152750.772999	36.048500
1355.304756	152985.014190	36.053517
1357.257934	153213.491257	36.058535
1358.669954	153445.062435	36.063552
1360.050111	153677.528131	36.068570
1361.637916	153897.242771	36.073588
1362.569792	154149.799183	36.078605
1363.929516	154365.933487	36.083623
1365.608656	154605.820359	36.088640
1366.931962	154839.302517	36.093658
1368.179089	155066.729633	36.098676
1369.339798	155312.882746	36.103693
1371.089481	155541.807166	36.108711
1372.166850	155783.329131	36.113728
1373.462963	156022.215464	36.118746
1375.395013	156261.917239	36.123764
1376.574763	156509.265690	36.128781
1378.015101	156742.635565	36.133799
1379.049914	156985.832121	36.138816
1380.513324	157226.055464	36.143834
1382.403351	157471.595627	36.148852
1383.797232	157719.613797	36.153869
1384.971816	157954.591471	36.158887
1386.336585	158200.166038	36.163904
1387.907757	158443.284528	36.168922
1389.383338	158680.414147	36.173940
1390.840284	158931.156849	36.178957
1392.177111	159168.119646	36.183975
1393.837514	159412.865702	36.188992
1395.183987	159651.250717	36.194010
1396.830182	159885.285996	36.199028
1398.031221	160134.270885	36.204045
1399.773109	160369.448287	36.209063
1401.072752	160607.285682	36.214080
1402.337650	160844.875500	36.219098
1403.837235	161082.035913	36.224116
1405.208230	161329.234230	36.229133
1406.892625	161564.133074	36.234151
1408.267825	161804.261054	36.239168
1409.672722	162041.858815	36.244186
1411.250967	162279.430319	36.249204
1412.938384	162517.874323	36.254221
1414.505961	162749.710669	36.259239
1416.038542	162980.943910	36.264256
1417.260707	163222.827757	36.269274
1419.188885	163457.009723	36.274292
1420.187348	163689.001953	36.279309
1421.470027	163913.700988	36.284327
1423.071800	164136.725722	36.289344
1424.264705	164369.616719	36.294362
1425.910205	164597.828923	36.299380
1427.184367	164828.880529	36.304397
1428.366780	165050.082184	36.309415
1430.310022	165289.689585	36.314432
1431.742963	165517.201774	36.319450
1433.280356	165737.816855	36.324468
1434.292496	165959.848001	36.329485
1435.621353	166174.656708	36.334503
1436.898981	166386.858593	36.339520
1438.553425	166603.445990	36.344538
1439.850624	166806.694935	36.349556
1441.023561	167039.268049	36.354573
1442.273861	167259.259990	36.359591
1443.703462	167481.586169	36.364608
1444.563236	167712.153638	36.369626
1446.410884	167937.856677	36.374644
1447.434815	168177.376692	36.379661
1448.891008	168418.962951	36.384679
1450.573069	168670.558043	36.389696
1452.014513	168902.930177	36.394714
1453.053820	169135.454879	36.399732
1454.094921	169394.555244	36.404749
1455.777632	169635.043550	36.409767
1457.573762	169885.621919	36.414784
1458.939322	170139.798386	36.419802
1460.183515	170385.182758	36.424820
1461.596752	170649.574882	36.429837
1462.979115	170900.361117	36.434855
1464.575110	171160.244245	36.439872
1465.901617	171419.408597	36.444890
1467.538112	171679.325266	36.449908
1468.609891	171949.616281	36.454925
1470.219285	172208.218442	36.459943
1472.052484	172477.566796	36.464960
1473.477049	172745.342039	36.469978
1475.232048	173002.298761	36.474996
1476.081927	173273.225935	36.480013
1477.967708	173534.887533	36.485031
1479.650459	173806.333779	36.490048
1480.853502	174080.040088	36.495066
1482.585042	174341.842776	36.500084
1483.960274	174615.409688	36.505101
1485.543107	174879.599243	36.510119
1487.169260	175147.211376	36.515136
1488.873837	175416.539067	36.520154
1490.615619	175676.541333	36.525172
1491.647155	175956.096615	36.530189
1493.663468	176219.816312	36.535207
1495.539097	176486.644562	36.540224
1496.893795	176745.479028	36.545242
1498.415640	177011.678611	36.550260
1499.999197	177291.482121	36.555277
1501.057447	177538.835216	36.560295
1502.674050	177796.539834	36.565312
1503.958373	178062.678289	36.570330
1505.489640	178331.699595	36.575348
1507.193457	178602.040786	36.580365
1508.853250	178874.294509	36.585383
1510.265290	179134.981212	36.590400
1511.774224	179409.571369	36.595418
1513.517538	179669.115701	36.600436
1514.955222	179934.600885	36.605453
1516.671106	180203.827579	36.610471
1518.485223	180462.753575	36.615488
1519.914224	180731.467984	36.620506
1521.342974	180983.903114	36.625524
1522.945633	181247.893229	36.630541
1524.576573	181508.349332	36.635559
1526.386455	181771.597356	36.640576
1527.397873	182037.968084	36.645594
1528.953423	182292.012404	36.650612
1530.428334	182564.306080	36.655629
1531.552123	182829.188334	36.660647
1533.618129	183087.498020	36.665664
1534.783775	183329.033838	36.670682
1536.422238	183586.726007	36.675700
1537.883946	183828.673903	36.680717
1539.447768	184075.406785	36.685735
1541.118387	184325.755606	36.690752
1542.338955	184589.408337	36.695770
1543.930729	184897.959904	36.700788
1545.248605	185155.782517	36.705805
1546.545759	185408.529199	36.710823
1548.342376	185656.524883	36.715840
1549.654626	185920.065124	36.720858
1551.323621	186177.733756	36.725876
1552.725642	186448.373098	36.730893
1554.455477	186712.408772	36.735911
1556.190737	186982.006753	36.740928
1557.426177	187257.931940	36.745946
1558.930935	187516.696323	36.750964
1560.270509	187787.374242	36.755981
1561.781508	188066.026936	36.760999
1563.320327	188349.832151	36.766016
1564.518499	188624.115646	36.771034
1566.396037	188907.158080	36.776052
1567.843222	189199.336395	36.781069
1569.759868	189477.929139	36.786087
1571.190263	189764.955318	36.791104
1572.362914	190058.067807	36.796122
1574.156677	190337.723279	36.801140
1575.870324	190631.971761	36.806157
1577.211113	190920.310235	36.811175
1579.027342	191209.438618	36.816192
1580.306193	191518.692824	36.821210
1582.202847	191815.989052	36.826228
1583.785024	192112.573204	36.831245
1585.495694	192406.928098	36.836263
1587.050859	192688.633039	36.841280
1588.459263	192997.515080	36.846298
1589.894631	193294.734642	36.851316
1591.732832	193598.369097	36.856333
1593.165362	193908.214806	36.861351
1594.937064	194208.279557	36.866368
1596.686258	194515.892655	36.871386
1598.009993	194812.802946	36.876404
1599.576332	195113.765529	36.881421
1601.383795	195420.025320	36.886439
1603.070381	195727.117560	36.891456
1604.812188	196034.151039	36.896474
1606.489725	196330.526632	36.901492
1607.734778	196646.580516	36.906509
1609.742354	196954.971493	36.911527
1611.752492	197244.489312	36.916544
1613.579518	197564.467591	36.921562
1615.099128	197866.484839	36.926580
1616.857934	198153.554411	36.931597
1618.283560	198457.365687	36.936615
1620.307434	198735.986872	36.941632
1622.134603	199048.957370	36.946650
1623.588724	199341.563678	36.951668
1625.353567	199636.128664	36.956685
1626.929835	199936.693198	36.961703
1628.321464	200217.270310	36.966720
1629.804463	200520.339934	36.971738
1631.413679	200819.757845	36.976756
1633.293619	201112.783360	36.981773
1634.813570	201406.703998	36.986791
1636.925196	201698.170126	36.991808
1638.731813	201996.111287	36.996826
1639.874235	202284.656388	37.001844
1641.618344	202573.590442	37.006861
1643.219740	202842.301488	37.011879
1645.046963	203112.095302	37.016896
1646.241062	203390.930308	37.021914
1647.686723	203663.782147	37.026932
1649.739622	203947.538705	37.031949
1651.129877	204220.450821	37.036967
1652.892049	204498.919123	37.041984
1654.217499	204784.645154	37.047002
1655.991900	205066.313093	37.052020
1657.647567	205350.921335	37.057037
1659.395602	205641.840837	37.062055
1660.878521	205927.493026	37.067072
1662.130535	206211.022487	37.072090
1663.763768	206501.376875	37.077108
1665.685684	206796.513048	37.082125
1666.932309	207105.549156	37.087143
1668.636267	207402.879504	37.092160
1670.076339	207709.701499	37.097178
1671.922251	208015.114020	37.102196
1673.704603	208314.440119	37.107213
1675.054023	208627.145630	37.112231
1676.899414	208934.998112	37.117248
1678.393980	209244.658704	37.122266
1680.091930	209565.439901	37.127284
1682.142198	209875.471549	37.132301
1683.654212	210203.802017	37.137319
1685.578270	210515.352959	37.142336
1687.174850	210834.601936	37.147354
1689.010312	211154.804625	37.152372
1690.733994	211466.159345	37.157389
1692.422887	211791.923633	37.162407
1694.211843	212102.608311	37.167424
1696.047952	212435.463240	37.172442
1697.334259	212748.818385	37.177460
1699.523865	213069.094679	37.182477
1701.229761	213402.428241	37.187495
1702.981917	213710.554448	37.192512
1704.624146	214031.552395	37.197530
1706.424506	214355.904575	37.202548
1707.892994	214675.964933	37.207565
1709.755955	215001.552654	37.212583
1711.657554	215325.813600	37.217600
1713.255457	215654.542589	37.222618
1715.189115	215976.436473	37.227636
1716.635083	216296.400010	37.232653
1718.033935	216631.257804	37.237671
1720.436399	216954.628654	37.242688
1722.363038	217286.838522	37.247706
1723.860870	217621.376659	37.252724
1725.354746	217933.661792	37.257741
1727.276391	218262.595949	37.262759
1729.289934	218578.585302	37.267776
1730.806614	218918.252853	37.272794
1732.163557	219257.361291	37.277812
1734.413928	219564.371873	37.282829
1735.869181	219902.322063	37.287847
1737.402764	220229.438040	37.292864
1739.675073	220563.450057	37.297882
1741.219604	220885.128119	37.302900
1743.127836	221205.860237	37.307917
1744.739637	221544.472486	37.312935
1746.745572	221866.154873	37.317952
1748.503095	222189.908547	37.322970
1749.935631	222520.470637	37.327988
1752.042816	222848.564650	37.333005
1753.410553	223179.365658	37.338023
1755.368433	223495.975111	37.343040
1756.820503	223830.726062	37.348058
1758.644323	224139.862372	37.353076
1760.499455	224446.377190	37.358093
1761.699284	224759.370999	37.363111
1763.941029	225067.552828	37.368128
1765.575307	225383.171504	37.373146
1767.300913	225706.422518	37.378164
1769.194691	226007.012164	37.383181
1770.797846	226332.771913	37.388199
1772.457258	226633.626832	37.393216
1774.471446	226964.021957	37.398234
1775.887685	227276.702351	37.403252
1777.499382	227595.423685	37.408269
1779.253729	227932.184931	37.413287
1781.159824	228248.954767	37.418304
1782.742370	228589.400931	37.423322
1784.573850	228914.387792	37.428340
1786.122349	229260.427983	37.433357
1787.927347	229594.437217	37.438375
1789.567308	229934.950186	37.443392
1791.690013	230269.620771	37.448410
1793.107152	230619.186758	37.453428
1794.809450	230969.317660	37.458445
1796.788866	231326.187889	37.463463
1798.501280	231670.829598	37.468480
1800.137312	232027.600758	37.473498
1801.914239	232396.899204	37.478516
1803.940564	232739.509679	37.483533
1805.736292	233103.647725	37.488551
1807.327497	233466.064653	37.493568
1809.591029	233827.182131	37.498586
1811.168970	234185.561390	37.503604
1813.214967	234546.864778	37.508621
1815.153653	234913.113002	37.513639
1817.001618	235273.125776	37.518656
1819.159370	235642.362130	37.523674
1820.631101	236007.920331	37.528692
1822.852510	236365.155476	37.533709
1824.695581	236726.920526	37.538727
1826.432956	237090.810253	37.543744
1828.770486	237452.014516	37.548762
1830.159839	237818.498288	37.553780
1832.089361	238177.555492	37.558797
1833.968730	238554.097775	37.563815
1835.789784	238906.617002	37.568832
1837.646117	239273.635683	37.573850
1839.318560	239647.236768	37.578868
1841.557614	239994.684796	37.583885
1843.420876	240368.255065	37.588903
1845.122272	240731.536389	37.593920
1847.224846	241087.946352	37.598938
1848.732291	241463.704632	37.603956
1850.951189	241814.582870	37.608973
1853.012037	242180.346215	37.613991
1854.587152	242552.078547	37.619008
1856.550567	242903.884293	37.624026
1858.492938	243270.629814	37.629044
1860.581896	243633.007885	37.634061
1862.360287	244003.639133	37.639079
1864.146583	244368.425835	37.644096
1866.093065	244731.002200	37.649114
1868.088882	245096.821787	37.654132
1869.993332	245451.604794	37.659149
1871.760892	245807.399309	37.664167
1873.348704	246172.213882	37.669184
1875.372324	246533.962066	37.674202
1876.989602	246900.777472	37.679220
1879.152936	247258.158570	37.684237
1880.721251	247623.684691	37.689255
1882.659366	247964.943646	37.694272
1884.759575	248311.866738	37.699290
1886.544647	248660.133985	37.704308
1888.389103	249000.186291	37.709325
1890.546969	249335.540265	37.714343
1892.008167	249686.701173	37.719360
1893.789989	250028.666388	37.724378
1895.413514	250384.195002	37.729396
1897.634768	250734.980732	37.734413
1899.371336	251092.446060	37.739431
1901.128939	251447.163879	37.744448
1903.135931	251805.245725	37.749466
1904.656619	252162.843992	37.754484
1906.455497	252530.533201	37.759501
1908.410597	252891.922839	37.764519
1910.172978	253266.626817	37.769536
1912.162154	253644.571153	37.774554
1913.830151	254026.349580	37.779572
1915.630053	254399.952475	37.784589
1917.759348	254783.612588	37.789607
1919.388310	255161.964847	37.794624
1921.658700	255555.405639	37.799642
1923.339581	255934.052439	37.804660
1925.351479	256321.689161	37.809677
1927.547750	256710.667548	37.814695
1929.056315	257111.081197	37.819712
1931.434867	257490.528763	37.824730
1933.115490	257890.176421	37.829748
1935.407614	258287.999876	37.834765
1937.367008	258685.061295	37.839783
1939.225523	259083.127831	37.844800
1941.359912	259484.375748	37.849818
1943.203472	259880.054342	37.854836
1945.383331	260265.163270	37.859853
1947.780892	260659.279338	37.864871
1949.753626	261072.256616	37.869888
1951.824608	261454.610001	37.874906
1953.614983	261851.509361	37.879924
1955.502309	262241.534184	37.884941
1957.857570	262636.742164	37.889959
1959.859777	263035.483711	37.894976
1961.820215	263428.413822	37.899994
1963.959128	263830.661574	37.905012
1965.735784	264210.333631	37.910029
1967.523158	264610.499864	37.915047
1969.719472	265000.440895	37.920064
1971.555149	265400.825103	37.925082
1973.499399	265797.888880	37.930100
1975.666687	266195.932152	37.935117
1977.443039	266597.184454	37.940135
1979.509328	266993.030640	37.945152
1981.529044	267389.644471	37.950170
1983.814190	267782.811754	37.955188
1985.265979	268186.775135	37.960205
1987.624661	268595.369780	37.965223
1989.501481	268989.865878	37.970240
1991.636793	269394.809260	37.975258
1993.217952	269799.761381	37.980276
1995.457111	270204.862741	37.985293
1997.734262	270602.718005	37.990311
1999.702358	271003.642181	37.995328
2001.696739	271399.557142	38.000346
2003.670663	271803.600690	38.005364
2005.759265	272193.452770	38.010381
2007.824999	272595.395720	38.015399
2009.684971	272998.105505	38.020416
2011.808311	273393.788041	38.025434
2013.419195	273795.821917	38.030452
2015.370123	274167.070709	38.035469
2017.866861	274543.997471	38.040487
2019.429638	274918.808364	38.045504
2021.457260	275298.801857	38.050522
2023.284620	275682.786722	38.055540
2025.215731	276075.312011	38.060557
2027.241886	276457.941488	38.065575
2028.959430	276844.375998	38.070592
2031.247165	277235.747760	38.075610
2033.123497	277629.569125	38.080628
2035.047604	278020.765295	38.085645
2037.074342	278425.783880	38.090663
2039.141709	278836.431702	38.095680
2041.180872	279236.136461	38.100698
2042.968880	279633.135753	38.105716
2044.898155	280045.754027	38.110733
2046.866619	280456.078368	38.115751
2048.725461	280878.302206	38.120768
2051.234962	281295.012822	38.125786
2053.154104	281713.387860	38.130804
2055.130465	282141.807569	38.135821
2057.219056	282564.874444	38.140839
2059.311639	282986.059047	38.145856
2061.068121	283409.325214	38.150874
2063.212549	283842.279214	38.155892
2065.614332	284286.871166	38.160909
2067.491260	284714.376634	38.165927
2069.507176	285156.915716	38.170944
2071.644134	285582.115107	38.175962
2073.678609	286028.251386	38.180980
2075.898895	286470.546764	38.185997
2078.122693	286910.197861	38.191015
2080.262590	287347.015249	38.196032
2082.148837	287795.092661	38.201050
2084.689034	288237.783197	38.206068
2086.690166	288665.777135	38.211085
2088.858058	289117.254604	38.216103
2091.156552	289572.060096	38.221120
2093.183741	290013.345946	38.226138
2095.357584	290452.650665	38.231156
2097.566309	290888.798396	38.236173
2099.933194	291334.109697	38.241191
2101.940789	291777.620504	38.246208
2104.097864	292216.966122	38.251226
2106.263588	292657.221260	38.256244
2108.662437	293096.319574	38.261261
2110.794212	293534.999455	38.266279
2112.678381	293974.070306	38.271296
2114.739313	294420.117686	38.276314
2117.200658	294864.550319	38.281332
2118.905227	295305.518153	38.286349
2121.287882	295743.634588	38.291367
2123.565686	296203.928240	38.296384
2125.661709	296636.674997	38.301402
2127.910469	297075.208452	38.306420
2130.113639	297510.749886	38.311437
2132.490463	297947.860216	38.316455
2134.423846	298400.065905	38.321472
2136.261984	298837.482051	38.326490
2138.324240	299278.845456	38.331508
2140.450120	299717.935941	38.336525
2143.054198	300162.050815	38.341543
2145.197868	300607.173396	38.346560
2147.287244	301048.975213	38.351578
2149.030292	301484.912640	38.356596
2151.560459	301926.232100	38.361613
2153.435917	302372.372052	38.366631
2155.669783	302810.709621	38.371648
2157.960970	303226.543282	38.376666
2160.050996	303643.572819	38.381684
2161.824933	304067.273898	38.386701
2164.318554	304480.019696	38.391719
2166.004808	304903.651475	38.396736
2168.451181	305325.409325	38.401754
2170.576682	305758.205137	38.406772
2172.118794	306182.737269	38.411789
2174.052653	306606.341500	38.416807
2176.072762	307049.016910	38.421824
2178.654886	307483.173283	38.426842
2180.286436	307925.267105	38.431860
2182.159176	308378.766800	38.436877
2184.871610	308826.166077	38.441895
2186.821464	309283.782651	38.446912
2188.922079	309745.178612	38.451930
2191.284997	310211.250119	38.456948
2193.357671	310667.235319	38.461965
2195.712394	311128.197514	38.466983
2197.747969	311591.464065	38.472000
2199.985993	312059.364447	38.477018
2202.511633	312528.915663	38.482036
2204.465721	312996.191217	38.487053
2206.854905	313466.794916	38.492071
2208.936904	313949.040380	38.497088
2211.057003	314412.214906	38.502106
2213.222298	314898.345782	38.507124
2215.361899	315368.461425	38.512141
2217.702721	315853.057259	38.517159
2220.035238	316343.080132	38.522176
2222.216265	316830.405889	38.527194
2224.604208	317310.892704	38.532212
2226.651702	317803.761020	38.537229
2229.228015	318296.845620	38.542247
2231.362250	318780.680503	38.547264
2234.197652	319268.206819	38.552282
2236.129803	319761.908525	38.557300
2238.506598	320258.148753	38.562317
2240.879934	320737.585033	38.567335
2243.130072	321236.422059	38.572352
2245.318839	321729.604163	38.577370
2247.806324	322217.506556	38.582388
2250.087148	322710.510530	38.587405
2252.822088	323198.870281	38.592423
2254.827458	323692.311731	38.597440
2257.492130	324168.669169	38.602458
2259.912296	324648.814609	38.607476
2262.127800	325135.659564	38.612493
2264.467401	325617.886822	38.617511
2266.695060	326108.219686	38.622528
2268.850708	326578.260122	38.627546
2271.302269	327068.165699	38.632564
2273.612622	327556.793417	38.637581
2275.986709	328040.863716	38.642599
2278.252722	328519.667853	38.647616
2280.679512	328993.189304	38.652634
2282.865189	329480.950149	38.657652
2284.719244	329962.794832	38.662669
2287.497024	330430.992363	38.667687
2289.823484	330931.955978	38.672704
2292.005102	331395.617851	38.677722
2294.159224	331882.313257	38.682740
2296.194097	332364.429430	38.687757
2298.272877	332848.765017	38.692775
2301.027504	333337.732457	38.697792
2303.004689	333832.421374	38.702810
2305.667884	334312.740135	38.707828
2307.372548	334794.039765	38.712845
2309.805643	335258.350513	38.717863
2312.103399	335725.593717	38.722880
2314.151041	336191.246709	38.727898
2316.675241	336654.815370	38.732916
2318.938186	337121.336016	38.737933
2321.345590	337584.556017	38.742951
2323.506014	338053.312836	38.747968
2325.729589	338526.923617	38.752986
2327.716384	338993.437949	38.758004
2330.010652	339473.315414	38.763021
2332.455530	339960.543546	38.768039
2334.673739	340445.111985	38.773056
2336.671984	340937.393023	38.778074
2339.125962	341431.269785	38.783092
2341.249657	341935.412042	38.788109
2343.971239	342423.856226	38.793127
2345.966400	342938.097907	38.798144
2348.613514	343434.553580	38.803162
2350.707292	343934.715174	38.808180
2353.006588	344447.111528	38.813197
2355.482969	344955.922156	38.818215
2357.875533	345472.751773	38.823232
2360.410792	345984.682294	38.828250
2363.116350	346485.851801	38.833268
2364.964334	347014.889625	38.838285
2367.331710	347530.854741	38.843303
2369.618002	348057.144921	38.848320
2372.102488	348580.073998	38.853338
2374.753078	349103.247723	38.858356
2376.977427	349632.869499	38.863373
2379.218927	350160.274081	38.868391
2381.863509	350700.436782	38.873408
2384.253838	351227.648630	38.878426
2386.895191	351754.077328	38.883444
2389.047755	352286.912342	38.888461
2391.502091	352819.184216	38.893479
2394.394162	353354.268980	38.898496
2396.872834	353892.122121	38.903514
2399.386387	354421.746542	38.908532
2401.343138	354956.088524	38.913549
2404.301272	355495.284328	38.918567
2406.397373	356027.203195	38.923584
2408.748084	356569.390777	38.928602
2411.773392	357092.222675	38.933620
2413.783157	357635.965877	38.938637
2416.108630	358183.807327	38.943655
2418.341159	358718.472189	38.948672
2420.704126	359260.711735	38.953690
2423.652347	359796.132879	38.958708
2425.677126	360346.491820	38.963725
2428.234860	360892.473712	38.968743
2431.147243	361447.869734	38.973760
2433.171215	361990.493306	38.978778
2435.883123	362527.930273	38.983796
2438.239172	363067.161952	38.988813
2440.632476	363609.875490	38.993831
2443.195307	364159.952952	38.998848
2445.719084	364704.222496	39.003866
2448.197810	365249.477302	39.008884
2450.512870	365800.880385	39.013901
2453.145100	366348.396673	39.018919
2455.668824	366882.665823	39.023936
2458.164930	367428.079473	39.028954
2460.509116	367974.317378	39.033972
2462.729015	368526.721918	39.038989
2465.190831	369064.710224	39.044007
2467.694144	369617.631953	39.049024
2470.293460	370149.217900	39.054042
2473.168607	370677.405967	39.059060
2475.103834	371188.932085	39.064077
2477.454251	371708.441139	39.069095
2479.900425	372214.902324	39.074112
2482.084534	372735.456928	39.079130
2484.713797	373253.474477	39.084148
2486.863528	373781.412741	39.089165
2489.409701	374315.916558	39.094183
2491.359516	374860.991627	39.099200
2493.697741	375399.256170	39.104218
2496.499444	375939.970847	39.109236
2498.848308	376491.739986	39.114253
2501.302222	377033.551052	39.119271
2504.161621	377590.765497	39.124288
2506.578292	378144.845785	39.129306
2509.154505	378685.666865	39.134324
2511.336767	379256.554907	39.139341
2513.799884	379814.088541	39.144359
2516.022071	380382.336944	39.149376
2518.385928	380949.689672	39.154394
2521.216955	381524.352782	39.159412
2523.674777	382101.417004	39.164429
2525.713177	382686.663909	39.169447
2528.572857	383270.958625	39.174464
2530.869455	383867.484493	39.179482
2533.644170	384453.816913	39.184500
2536.191371	385043.058432	39.189517
2538.577944	385633.096442	39.194535
2541.572189	386240.625425	39.199552
2543.582412	386841.937640	39.204570
2546.421637	387439.130202	39.209588
2549.054124	388045.304682	39.214605
2551.675365	388654.124872	39.219623
2554.377712	389269.753936	39.224640
2556.596659	389871.517428	39.229658
2559.690191	390475.154956	39.234676
2562.383870	391091.904507	39.239693
2564.850984	391700.065870	39.244711
2567.433727	392311.839639	39.249728
2569.988766	392924.513714	39.254746
2573.115717	393540.627039	39.259764
2575.316037	394154.135482	39.264781
2578.085646	394770.273180	39.269799
2580.826870	395380.880991	39.274816
2583.345036	395994.039368	39.279834
2585.975132	396605.240636	39.284852
2588.507899	397220.541873	39.289869
2591.452781	397842.697894	39.294887
2594.344219	398450.519938	39.299904
2596.884437	399055.495774	39.304922
2599.520740	399666.818840	39.309940
2602.313585	400281.442078	39.314957
2604.886254	400898.006837	39.319975
2607.482177	401503.669313	39.324992
2609.766778	402123.688096	39.330010
2612.618435	402720.674168	39.335028
2615.065587	403350.250538	39.340045
2617.574602	403959.303058	39.345063
2620.568519	404574.488136	39.350080
2623.412611	405186.086820	39.355098
2625.933597	405787.902011	39.360116
2628.454939	406411.612430	39.365133
2631.140431	407015.646050	39.370151
2634.131740	407631.304285	39.375168
2636.698937	408241.547013	39.380186
2639.063492	408856.712620	39.385204
2641.816958	409470.737702	39.390221
2644.487839	410076.663276	39.395239
2647.190412	410650.490522	39.400256
2649.715947	411239.558768	39.405274
2652.359395	411802.639264	39.410292
2654.682558	412393.529150	39.415309
2656.952256	412975.254708	39.420327
2659.784570	413551.767257	39.425344
2662.358854	414142.519320	39.430362
2664.763244	414734.192176	39.435380
2667.355165	415332.293933	39.440397
2669.958313	415927.089312	39.445415
2672.156996	416529.012497	39.450432
2675.171303	417141.665413	39.455450
2677.684262	417752.355831	39.460468
2680.184568	418357.214254	39.465485
2682.721585	418979.750473	39.470503
2685.704331	419603.867312	39.475520
2687.857575	420237.248548	39.480538
2690.875567	420873.408234	39.485556
2693.248807	421503.024737	39.490573
2695.873157	422150.685556	39.495591
2698.644320	422785.712296	39.500608
2701.131071	423436.489020	39.505626
2703.896977	424082.195698	39.510644
2706.773527	424729.533036	39.515661
2709.145092	425390.680580	39.520679
2712.130830	426049.587027	39.525696
2714.943135	426711.228994	39.530714
2717.977373	427369.578989	39.535732
2720.829197	428036.479081	39.540749
2723.449413	428709.711828	39.545767
2726.353979	429373.626905	39.550784
2728.750256	430036.183880	39.555802
2731.809920	430707.460225	39.560820
2734.676464	431374.852001	39.565837
2737.233501	432051.720710	39.570855
2739.805209	432729.675530	39.575872
2742.779183	433419.218095	39.580890
2745.607206	434092.031467	39.585908
2748.640566	434777.473450	39.590925
2751.378072	435450.253602	39.595943
2754.126146	436128.870105	39.600960
2757.117307	436812.275314	39.605978
2759.657314	437492.644418	39.610996
2762.743182	438175.025871	39.616013
2765.268109	438864.038537	39.621031
2768.392215	439541.261820	39.626048
2771.126136	440219.229028	39.631066
2773.935759	440908.071815	39.636084
2777.108230	441586.880767	39.641101
2779.902962	442273.604318	39.646119
2783.035012	442950.197723	39.651136
2785.707471	443636.182763	39.656154
2788.657223	444302.855061	39.661172
2791.622552	444980.107244	39.666189
2794.439285	445660.589986	39.671207
2797.384200	446328.553037	39.676224
2799.969034	446998.517474	39.681242
2803.016490	447667.172869	39.686260
2805.874435	448342.801899	39.691277
2808.494291	449013.241809	39.696295
2811.074256	449681.996687	39.701312
2814.040661	450361.320035	39.706330
2816.664012	451030.219775	39.711348
2819.601597	451709.243911	39.716365
2822.548544	452380.920134	39.721383
2825.652763	453050.476447	39.726400
2828.133791	453733.684631	39.731418
2831.346427	454382.677543	39.736436
2833.941617	455020.789142	39.741453
2836.728520	455659.907528	39.746471
2839.448215	456286.899015	39.751488
2841.757535	456932.152950	39.756506
2844.741360	457579.397230	39.761524
2847.440294	458216.921259	39.766541
2850.226249	458870.507305	39.771559
2852.968244	459512.316911	39.776576
2855.456426	460173.318452	39.781594
2858.283895	460836.108503	39.786612
2861.026146	461494.142918	39.791629
2863.787179	462168.497305	39.796647
2866.921973	462834.743966	39.801664
2869.997745	463505.464015	39.806682
2872.669737	464177.683644	39.811700
2874.968942	464855.332841	39.816717
2877.948829	465541.071209	39.821735
2880.740081	466233.621122	39.826752
2883.543372	466931.689181	39.831770
2886.230851	467624.550572	39.836788
2889.286519	468335.281821	39.841805
2891.562215	469046.507969	39.846823
2894.962068	469748.600645	39.851840
2898.080328	470472.443863	39.856858
2900.756684	471196.677203	39.861876
2903.914673	471908.095179	39.866893
2906.617676	472636.496367	39.871911
2909.661870	473361.332271	39.876928
2912.688284	474089.718410	39.881946
2915.654172	474824.686041	39.886964
2918.406060	475552.897679	39.891981
2921.851574	476290.546556	39.896999
2924.984567	477009.305641	39.902016
2927.785864	477755.305585	39.907034
2930.533005	478487.316061	39.912052
2933.607301	479222.215467	39.917069
2936.590779	479978.264105	39.922087
2939.923236	480713.557661	39.927104
2942.538367	481464.300375	39.932122
2945.486637	482197.316479	39.937140
2948.708125	482946.532481	39.942157
2951.693517	483692.322733	39.947175
2955.069523	484423.554535	39.952192
2957.778971	485166.696729	39.957210
2960.663805	485912.496401	39.962228
2963.719940	486667.402487	39.967245
2967.183901	487411.577702	39.972263
2970.191949	488144.805923	39.977280
2972.979034	488896.369502	39.982298
2976.284396	489646.404462	39.987316
2979.080872	490377.643884	39.992333
2982.143036	491133.284450	39.997351
2985.437948	491872.432070	40.002368
2988.316493	492612.615635	40.007386
2990.910600	493354.771084	40.012404
2994.551061	494100.402044	40.017421
2997.621455	494838.380636	40.022439
3000.753012	495568.760255	40.027456
3003.757341	496320.119226	40.032474
3006.873354	497056.620653	40.037492
3010.053089	497789.098089	40.042509
3012.781644	498523.522484	40.047527
3015.775138	499253.539457	40.052544
3018.855872	499992.415793	40.057562
3021.874950	500726.180547	40.062580
3024.984280	501464.524555	40.067597
3028.105044	502205.295203	40.072615
3031.103499	502916.354569	40.077632
3034.153449	503627.873987	40.082650
3036.877253	504316.965887	40.087668
3039.904319	505004.970825	40.092685
3042.548068	505709.305042	40.097703
3045.143286	506400.480106	40.102720
3048.236062	507110.209266	40.107738
3051.080247	507816.067961	40.112756
3054.015429	508529.372811	40.117773
3057.016711	509260.841170	40.122791
3060.054042	509980.243866	40.127808
3063.138846	510703.827295	40.132826
3065.545961	511430.446698	40.137844
3069.192875	512163.573685	40.142861
3071.957530	512904.947040	40.147879
3074.875146	513655.811546	40.152896
3077.813209	514398.888187	40.157914
3080.742621	515166.313109	40.162932
3083.832976	515923.815263	40.167949
3086.486997	516694.063838	40.172967
3089.779238	517464.118986	40.177984
3092.504530	518243.167562	40.183002
3095.535229	519034.389205	40.188020
3098.862172	519822.251146	40.193037
3101.873648	520621.727103	40.198055
3104.925075	521416.123511	40.203072
3108.205477	522216.618727	40.208090
3111.171170	523020.231078	40.213108
3114.156829	523818.767006	40.218125
3117.452509	524643.787416	40.223143
3120.682291	525451.282020	40.228160
3123.784329	526265.881652	40.233178
3126.803249	527091.295483	40.238196
3130.266166	527910.760999	40.243213
3132.915463	528726.635747	40.248231
3136.004292	529566.349974	40.253248
3139.503905	530396.202354	40.258266
3142.383802	531236.042748	40.263284
3145.727037	532079.974810	40.268301
3148.866878	532924.134796	40.273319
3152.386835	533761.602415	40.278336
3156.084048	534609.682375	40.283354
3159.419651	535445.060880	40.288372
3163.075353	536282.593968	40.293389
3165.924678	537120.047624	40.298407
3169.519398	537949.448961	40.303424
3172.837025	538772.615597	40.308442
3175.804825	539607.226575	40.313460
3178.589059	540434.483982	40.318477
3182.597990	541266.865121	40.323495
3185.683273	542105.858806	40.328512
3188.708314	542932.462458	40.333530
3191.989776	543768.704803	40.338548
3195.270845	544591.947423	40.343565
3198.577132	545430.933794	40.348583
3201.619081	546252.849441	40.353600
3205.313721	547084.640194	40.358618
3208.183599	547925.832702	40.363636
3211.714837	548749.160469	40.368653
3215.226269	549581.813860	40.373671
3218.375174	550404.237511	40.378688
3221.606921	551225.389304	40.383706
3224.759575	552057.929625	40.388724
3228.208717	552871.365133	40.393741
3231.079318	553696.216317	40.398759
3234.421750	554517.277933	40.403776
3237.513796	555330.653497	40.408794
3240.387378	556161.149681	40.413812
3244.204295	556972.546165	40.418829
3247.073705	557763.789188	40.423847
3250.053502	558546.493492	40.428864
3253.418623	559324.626308	40.433882
3256.709982	560118.252072	40.438900
3259.707093	560890.126399	40.443917
3263.291940	561690.865220	40.448935
3266.195628	562479.382724	40.453952
3269.470621	563260.125136	40.458970
3272.233802	564063.785748	40.463988
3275.422822	564849.744684	40.469005
3278.988128	565665.840818	40.474023
3282.104562	566485.905882	40.479040
3285.281888	567287.776478	40.484058
3288.523137	568117.570921	40.489076
3291.366920	568934.550559	40.494093
3294.609881	569757.667639	40.499111
3298.098401	570600.260608	40.504128
3301.411908	571439.064610	40.509146
3304.568256	572279.232932	40.514164
3308.258496	573124.911213	40.519181
3311.687695	573969.266067	40.524199
3315.051536	574816.620625	40.529216
3318.286984	575662.580601	40.534234
3321.493535	576526.443590	40.539252
3324.708329	577371.327528	40.544269
3328.024925	578237.993166	40.549287
3331.420424	579105.279504	40.554304
3334.877826	579969.787632	40.559322
3338.252683	580844.694359	40.564340
3341.893653	581711.138653	40.569357
3345.190874	582587.620020	40.574375
3348.534547	583467.874593	40.579392
3351.922510	584344.051868	40.584410
3355.347861	585223.002940	40.589428
3358.726335	586106.239834	40.594445
3362.173062	586986.195387	40.599463
3365.274435	587886.276562	40.604480
3368.868993	588764.865311	40.609498
3372.120302	589660.227630	40.614516
3375.833203	590550.346560	40.619533
3379.577060	591443.085162	40.624551
3382.876742	592328.224778	40.629568
3386.275072	593215.423954	40.634586
3389.605476	594112.450768	40.639604
3393.024166	594996.601260	40.644621
3396.898901	595898.886679	40.649639
3399.945657	596798.927408	40.654656
3403.559212	597688.765656	40.659674
3406.716366	598580.547466	40.664692
3410.684018	599468.132676	40.669709
3414.047477	600359.131992	40.674727
3417.318411	601262.150349	40.679744
3421.219485	602150.217148	40.684762
3424.219974	603036.602035	40.689780
3427.852379	603941.926632	40.694797
3431.280741	604833.430932	40.699815
3434.550766	605731.070330	40.704832
3438.120089	606621.998745	40.709850
3441.491475	607526.899672	40.714868
3445.266855	608414.147957	40.719885
3448.676744	609314.544769	40.724903
3451.993544	610217.619772	40.729920
3455.661395	611103.653207	40.734938
3459.003453	612001.728026	40.739956
3462.620055	612900.029232	40.744973
3465.874277	613784.296902	40.749991
3469.169762	614675.808976	40.755008
3473.022832	615560.008762	40.760013
3475.670731	616413.517043	40.765018
3479.199388	617190.662359	40.770023
3482.521729	617931.154886	40.775028
3485.338728	618633.500619	40.780032
3488.372560	619269.667898	40.785037
3490.901008	619861.612853	40.790042
3493.499716	620396.015886	40.795047
3496.343266	620867.564240	40.800052
3498.619324	621295.124487	40.805056
3501.043885	621670.099528	40.810061
3503.141270	621987.325512	40.815066
3504.985178	622252.989480	40.820071
3506.895144	622480.829727	40.825076
3508.551787	622667.253092	40.830080
3510.178817	622820.417212	40.835085
3511.610172	622930.311676	40.840090
3513.097738	623000.244517	40.845095
3514.666627	623032.360063	40.850100
3515.177198	623020.095011	40.855104
3516.614675	622993.002803	40.860109
3517.890772	622956.147549	40.865114
3518.614570	622865.692839	40.870119
3519.428546	622745.009007	40.875124
3519.833718	622624.986900	40.880128
3520.591234	622470.597957	40.885133
3521.146654	622318.036137	40.890138
3521.305453	622126.927296	40.895143
3522.241112	621929.600010	40.900148
3522.142138	621724.239364	40.905152
3522.396067	621491.248425	40.910157
3522.973367	621257.402257	40.915162
3522.996934	621026.034696	40.920167
3523.254974	620761.257884	40.925172
3523.315087	620508.293652	40.930176
3523.400497	620233.539244	40.935181
3523.640680	619966.945630	40.940186
3524.015631	619680.441146	40.945191
3524.002274	619397.236345	40.950196
3523.805613	619115.800686	40.955200
3524.289947	618816.514539	40.960205
3524.017320	618515.938769	40.965210
3523.930407	618220.121400	40.970215
3523.778777	617913.213065	40.975220
3523.950093	617608.043592	40.980224
3523.726780	617292.632985	40.985229
3523.351419	616988.929141	40.990234
3523.249366	616680.625928	40.995239
3523.371211	616372.278204	41.000244
3522.909389	616067.810281	41.005248
3523.112698	615757.132038	41.010253
3522.744105	615458.228324	41.015258
3522.579970	615145.789382	41.020263
3522.615023	614851.302600	41.025268
3522.223748	614542.778884	41.030272
3522.073843	614231.558830	41.035277
3521.573467	613937.878746	41.040282
3521.707019	613635.793217	41.045287
3521.840942	613330.349374	41.050292
3521.472958	613035.472565	41.055296
3521.051590	612737.396059	41.060301
3520.633108	612449.258817	41.065306
3520.717170	612164.984320	41.070311
3520.645058	611879.726347	41.075316
3520.161688	611591.324840	41.080320
3519.881642	611308.233141	41.085325
3519.949330	611038.379046	41.090330
3519.512414	610757.446480	41.095335
3519.485564	610480.292210	41.100340
3518.947663	610203.210276	41.105344
3519.017233	609936.576866	41.110349
3518.691834	609675.248869	41.115354
3518.388884	609404.809300	41.120359
3518.103188	609140.010856	41.125364
3517.848639	608888.853416	41.130368
3518.213673	608629.141036	41.135373
3517.621197	608373.072625	41.140378
3517.450880	608127.134613	41.145383
3517.085095	607867.167040	41.150388
3516.891706	607628.972992	41.155392
3516.837368	607387.600579	41.160397
3516.676081	607157.643423	41.165402
3516.167374	606917.331345	41.170407
3516.140309	606679.889576	41.175412
3515.541815	606451.585622	41.180416
3515.691349	606225.760856	41.185421
3515.427337	606009.250241	41.190426
3515.174282	605780.427174	41.195431
3514.976380	605559.994816	41.200436
3514.597662	605352.092830	41.205440
3514.764370	605131.194090	41.210445
3514.284459	604931.053827	41.215450
3514.599768	604722.780525	41.220455
3514.249129	604505.851651	41.225460
3513.929109	604309.726896	41.230464
3513.575032	604110.151452	41.235469
3513.140547	603909.934284	41.240474
3512.756861	603718.961810	41.245479
3513.002039	603535.743169	41.250484
3513.228045	603350.722960	41.255488
3512.760877	603157.401459	41.260493
3512.460043	602980.513103	41.265498
3512.142551	602789.813408	41.270503
3512.427418	602617.981399	41.275508
3512.113884	602455.147443	41.280512
3512.111598	602269.393050	41.285517
3511.786143	602095.496011	41.290522
3511.756595	601929.356639	41.295527
3511.499123	601761.748911	41.300532
3511.116676	601597.110702	41.305536
3511.089973	601432.264141	41.310541
3510.908184	601268.640346	41.315546
3510.764150	601120.272629	41.320551
3510.675396	600954.727559	41.325556
3510.417802	600812.679326	41.330560
3510.572896	600655.149297	41.335565
3510.480447	600515.323451	41.340570
3510.292374	600363.398284	41.345575
3509.827602	600217.670560	41.350580
3509.650679	600072.246177	41.355584
3509.862307	599930.813355	41.360589
3509.734793	599788.680831	41.365594
3509.853386	599658.771301	41.370599
3509.458448	599511.270920	41.375604
3509.121421	599387.586062	41.380608
3509.213284	599250.918108	41.385613
3508.707767	599129.959608	41.390618
3508.712886	598994.853653	41.395623
3509.190717	598869.083048	41.400628
3508.732271	598755.221164	41.405632
3508.544788	598616.085675	41.410637
3508.109560	598502.918262	41.415642
3508.458794	598376.010483	41.420647
3508.346287	598256.232006	41.425652
3508.403750	598142.983702	41.430656
3508.339804	598018.589239	41.435661
3508.178735	597905.172292	41.440666
3507.533261	597790.978769	41.445671
3507.688689	597684.268541	41.450676
3507.757322	597567.007178	41.455680
3507.617482	597457.387003	41.460685
3507.358559	597359.900182	41.465690
3507.266252	597261.685488	41.470695
3507.397260	597154.072530	41.475700
3507.237399	597056.567421	41.480704
3507.430221	596944.887240	41.485709
3507.150784	596850.903654	41.490714
3507.088071	596738.009536	41.495719
3507.242643	596644.356815	41.500724
3506.728645	596549.105421	41.505728
3506.693957	596451.725374	41.510733
3506.461432	596368.645395	41.515738
3506.040534	596268.720385	41.520743
3506.301425	596180.604791	41.525748
3506.357569	596102.284426	41.530752
3506.184272	595999.363946	41.535757
3506.519422	595918.945657	41.540762
3506.150003	595839.988867	41.545767
3506.512685	595746.395820	41.550772
3506.063944	595667.249851	41.555776
3506.225684	595563.621810	41.560781
3505.766311	595483.925319	41.565786
3505.695733	595410.326651	41.570791
3505.592317	595323.863288	41.575796
3505.779676	595252.777040	41.580800
3506.097611	595177.113000	41.585805
3505.899617	595100.026788	41.590810
3505.360828	595012.477196	41.595815
3505.656591	594939.268686	41.600820
3505.389348	594868.901940	41.605824
3505.174741	594789.262125	41.610829
3505.386224	594719.670874	41.615834
3505.398287	594646.604857	41.620839
3505.468558	594570.574593	41.625844
3505.591363	594491.580905	41.630848
3505.448754	594415.432575	41.635853
3505.329898	594350.247466	41.640858
3505.333718	594272.723069	41.645863
3505.645654	594193.347043	41.650868
3505.141952	594125.516372	41.655872
3505.119446	594050.899166	41.660877
3504.943272	593993.884068	41.665882
3504.705103	593926.461351	41.670887
3504.882238	593868.839452	41.675892
3505.003822	593796.651962	41.680896
3505.313923	593724.434513	41.685901
3504.785439	593661.663116	41.690906
3504.914166	593590.024025	41.695911
3504.707956	593522.393424	41.700916
3504.380054	593467.753165	41.705920
3504.211759	593406.326307	41.710925
3504.506164	593345.427776	41.715930
3504.450199	593298.457150	41.720935
3504.737297	593238.210253	41.725940
3504.342759	593181.575545	41.730944
3504.657210	593116.365242	41.735949
3504.386423	593057.456679	41.740954
3504.689510	593001.012471	41.745959
3504.339849	592942.766726	41.750964
3504.096433	592882.350326	41.755968
3503.787539	592826.351473	41.760973
3503.913379	592776.194653	41.765978
3503.882470	592721.003273	41.770983
3503.857154	592673.824761	41.775988
3503.900149	592627.036065	41.780992
3504.036881	592579.531278	41.785997
3503.876775	592526.162262	41.791002
3503.824483	592477.083743	41.796007
3503.864096	592426.588145	41.801012
3503.689393	592371.868244	41.806016
3504.033168	592330.040136	41.811021
3503.990978	592279.957349	41.816026
3503.654526	592226.714587	41.821031
3504.126773	592178.404226	41.826036
3503.999138	592129.035351	41.831040
3503.679957	592069.177197	41.836045
3503.592508	592024.960879	41.841050
3503.613581	591986.237410	41.846055
3504.116648	591933.012220	41.851060
3503.983113	591896.316241	41.856064
3503.742113	591833.689529	41.861069
3503.736607	591787.906584	41.866074
3503.502952	591735.897608	41.871079
3503.951711	591704.018960	41.876084
3503.627075	591653.326202	41.881088
3503.534269	591607.606228	41.886093
3503.417325	591550.819308	41.891098
3503.646248	591508.304654	41.896103
3503.625931	591462.472544	41.901108
3503.426295	591419.223040	41.906112
3503.611066	591372.506895	41.911117
3503.628663	591332.879926	41.916122
3503.314077	591293.505116	41.921127
3503.506584	591249.642591	41.926132
3503.389701	591216.298001	41.931136
3503.565896	591163.170195	41.936141
3503.409429	591123.469475	41.941146
3503.313693	591073.138953	41.946151
3503.630277	591036.820526	41.951156
3503.205282	591005.326877	41.956160
3503.071153	590951.495107	41.961165
3503.118954	590915.168191	41.966170
3503.497748	590869.621832	41.971175
3503.516973	590832.848241	41.976180
3502.994762	590781.981872	41.981184
3503.236811	590746.375468	41.986189
3503.469907	590711.221217	41.991194
3503.118643	590665.788125	41.996199
3503.355463	590626.675350	42.001204
3503.113228	590588.338687	42.006208
3504.009846	590556.987801	42.011213
3503.497352	590509.374962	42.016218
3502.813420	590464.293611	42.021223
3503.411990	590422.518450	42.026228
3503.180555	590393.998640	42.031232
3503.028676	590349.484910	42.036237
3502.940930	590311.974786	42.041242
3503.080134	590275.230634	42.046247
3503.330228	590238.368824	42.051252
3503.044816	590206.099527	42.056256
3503.106535	590168.114645	42.061261
3502.935639	590125.857434	42.066266
3502.995006	590086.469844	42.071271
3503.293824	590049.900372	42.076276
3502.863089	590027.272431	42.081280
3503.005143	589982.210234	42.086285
3503.105127	589949.729621	42.091290
3503.284329	589907.166321	42.096295
3503.456864	589869.213163	42.101300
3502.903608	589835.932515	42.106304
3503.012870	589802.347789	42.111309
3503.027196	589765.771727	42.116314
3503.125950	589731.386804	42.121319
3502.685966	589676.644551	42.126324
3502.467417	589656.387537	42.131328
3502.676997	589616.774344	42.136333
3502.794293	589597.667164	42.141338
3502.785817	589560.442646	42.146343
3502.952360	589536.217237	42.151348
3502.710890	589507.696649	42.156352
3502.937216	589462.518906	42.161357
3502.754811	589431.934678	42.166362
3502.936400	589403.798605	42.171367
3502.572647	589358.913086	42.176372
3502.553962	589336.870619	42.181376
3502.826669	589301.906000	42.186381
3502.990896	589270.966508	42.191386
3503.142285	589243.886914	42.196391
3502.933840	589206.041089	42.201396
3502.737117	589167.441739	42.206400
3503.005876	589130.773650	42.211405
3502.781336	589103.301535	42.216410
3502.528488	589067.867173	42.221415
3502.993104	589031.318442	42.226420
3502.613440	589003.419381	42.231424
3502.951731	588962.080110	42.236429
3502.667848	588932.863166	42.241434
3502.987765	588910.817003	42.246439
3503.217128	588868.291878	42.251444
3502.891591	588843.841213	42.256448
3502.991831	588798.630304	42.261453
3503.030915	588769.262218	42.266458
3502.689803	588741.055818	42.271463
3503.511128	588703.197570	42.276468
3502.981675	588659.838235	42.281472
3503.047556	588624.001847	42.286477
3503.071397	588592.831832	42.291482
3503.111275	588554.894802	42.296487
3503.133632	588513.603210	42.301492
3502.655838	588479.504867	42.306496
3502.737113	588445.168696	42.311501
3503.064752	588416.405940	42.316506
3502.532355	588379.810446	42.321511
3502.666051	588347.971153	42.326516
3502.513395	588323.341962	42.331520
3502.634579	588284.238793	42.336525
3503.012681	588263.635354	42.341530
3503.087831	588225.841983	42.346535
3502.637516	588186.527154	42.351540
3502.564182	588155.972375	42.356544
3502.962877	588121.234797	42.361549
3502.435922	588092.955543	42.366554
3502.630809	588067.018714	42.371559
3502.420179	588026.563435	42.376564
3502.524722	588001.542540	42.381568
3502.863112	587966.112362	42.386573
3502.975709	587946.802568	42.391578
3502.779677	587912.057074	42.396583
3502.955690	587874.998361	42.401588
3502.961123	587851.846683	42.406592
3502.807303	587803.364078	42.411597
3502.828412	587783.767634	42.416602
3502.819345	587739.872269	42.421607
3502.866622	587710.700478	42.426612
3502.638444	587673.052824	42.431616
3502.843746	587640.248155	42.436621
3502.978959	587621.084580	42.441626
3502.804989	587589.341271	42.446631
3502.805617	587542.637363	42.451636
3502.709287	587514.439613	42.456640
3502.720300	587483.619198	42.461645
3502.530148	587461.549611	42.466650
3502.434498	587425.884855	42.471655
3502.784529	587387.243802	42.476660
3502.410089	587355.881936	42.481664
3502.417572	587330.373546	42.486669
3502.566078	587300.332917	42.491674
3502.634004	587280.477684	42.496679
3502.572748	587246.711246	42.501684
3502.621158	587228.362354	42.506688
3502.499139	587187.839983	42.511693
3502.858914	587171.597185	42.516698
3502.253684	587140.170548	42.521703
3502.913697	587108.145118	42.526708
3502.534439	587079.439221	42.531712
3502.679167	587049.097808	42.536717
3502.764238	587018.515067	42.541722
3502.541556	586997.802698	42.546727
3502.583278	586961.413348	42.551732
3502.567883	586931.046523	42.556736
3502.397427	586890.530617	42.561741
3502.749240	586867.523153	42.566746
3502.522844	586841.148115	42.571751
3502.638723	586815.270770	42.576756
3502.326538	586788.558212	42.581760
3502.870453	586750.485971	42.586765
3502.772914	586728.199956	42.591770
3502.851179	586697.266571	42.596775
3502.595943	586661.373680	42.601780
3502.728257	586640.154094	42.606784
3502.825996	586604.306066	42.611789
3502.917302	586573.470522	42.616794
3502.379803	586545.339227	42.621799
3502.726380	586511.857566	42.626804
3502.408883	586485.295443	42.631808
3502.374302	586449.668057	42.636813
3502.648782	586429.478284	42.641818
3502.382832	586401.053582	42.646823
3502.014814	586365.578281	42.651828
3502.293985	586349.096276	42.656832
3502.633402	586322.080241	42.661837
3502.369861	586297.564026	42.666842
3502.345501	586272.910130	42.671847
3502.567499	586245.110383	42.676852
3502.401561	586223.485555	42.681856
3502.349575	586187.759800	42.686861
3502.553116	586161.967436	42.691866
3502.493220	586138.571738	42.696871
3502.693273	586106.665397	42.701876
3502.167359	586083.292314	42.706880
3502.574796	586047.644633	42.711885
3502.292558	586026.488661	42.716890
3502.279176	585994.715596	42.721895
3502.300249	585969.953676	42.726900
3502.026452	585948.495520	42.731904
3502.398818	585922.776437	42.736909
3502.156592	585890.537655	42.741914
3502.148514	585866.481724	42.746919
3502.184350	585846.227943	42.751924
3502.078871	585833.714597	42.756928
3502.422146	585809.453257	42.761933
3501.807370	585773.563528	42.766938
3502.296181	585763.663657	42.771943
3501.911650	585735.907313	42.776948
3502.077295	585717.838272	42.781952
3501.913629	585695.159523	42.786957
3502.104378	585679.241652	42.791962
3501.859028	585660.234364	42.796967
3501.803828	585638.791546	42.801972
3502.114777	585618.093372	42.806977
3502.254401	585600.579528	42.811981
3501.898958	585577.479431	42.816986
3501.757848	585554.195418	42.821991
3502.103531	585529.481995	42.826996
3502.143085	585513.136432	42.832001
3502.242440	585474.928765	42.837005
3502.201598	585475.386233	42.842010
3501.790940	585445.778759	42.847015
3502.312854	585430.761058	42.852020
3502.038250	585408.299541	42.857025
3502.095512	585380.974443	42.862029
3502.027913	585357.277547	42.867034
3502.043974	585342.539290	42.872039
3501.950143	585318.946655	42.877044
3502.452723	585307.690935	42.882049
3502.321753	585278.089405	42.887053
3502.220354	585259.159159	42.892058
3501.938202	585234.342731	42.897063
3502.183116	585201.725029	42.902068
3502.099173	585187.152563	42.907073
3502.232797	585165.929910	42.912077
3502.173759	585139.073491	42.917082
3502.178006	585117.419867	42.922087
3502.075263	585097.687589	42.927092
3502.273844	585071.342080	42.932097
3502.154222	585046.098834	42.937101
3502.233861	585024.633732	42.942106
3502.040552	585000.153745	42.947111
3502.509610	584982.637537	42.952116
3502.365000	584962.861438	42.957121
3502.193921	584934.067220	42.962125
3502.292949	584906.985027	42.967130
3502.311084	584881.118382	42.972135
3502.274568	584857.215049	42.977140
3502.444618	584827.715613	42.982145
3502.271414	584805.788370	42.987149
3502.420485	584779.850893	42.992154
3502.253300	584758.975222	42.997159
3502.173037	584734.426844	43.002164
3502.254752	584710.554833	43.007169
3501.928920	584692.811555	43.012173
3502.060019	584664.420510	43.017178
3502.568743	584653.965158	43.022183
3502.123077	584624.561430	43.027188
3502.354989	584605.728322	43.032193
3502.570066	584574.316418	43.037197
3502.715200	584547.526880	43.042202
3502.347131	584513.900203	43.047207
3502.344567	584489.289004	43.052212
3502.585086	584468.950551	43.057217
3502.395308	584439.155443	43.062221
3502.481205	584408.665522	43.067226
3502.063890	584384.519933	43.072231
3501.868972	584356.279308	43.077236
3501.986707	584341.523811	43.082241
3502.334388	584320.667069	43.087245
3502.741791	584299.049056	43.092250
3502.574428	584269.801374	43.097255
3502.411405	584240.603062	43.102260
3502.064902	584213.588806	43.107265
3501.958851	584181.273570	43.112269
3502.196347	584163.491496	43.117274
3502.008790	584147.580416	43.122279
3502.440493	584120.995675	43.127284
3502.274763	584101.572212	43.132289
3502.403365	584074.683851	43.137293
3502.391110	584046.764766	43.142298
3501.809764	584011.214913	43.147303
3502.226083	584003.179521	43.152308
3501.971148	583978.907396	43.157313
3502.371721	583965.711269	43.162317
3502.221597	583948.240083	43.167322
3502.198162	583919.119350	43.172327
3502.292380	583886.822067	43.177332
3502.192466	583882.376266	43.182337
3501.943382	583847.275223	43.187341
3502.413013	583839.080991	43.192346
3502.111104	583808.399386	43.197351
3502.386258	583788.605676	43.202356
3501.943964	583757.695232	43.207361
3502.167752	583737.658815	43.212365
3502.104491	583705.285360	43.217370
3501.899619	583679.500874	43.222375
3502.521830	583661.106426	43.227380
3502.002554	583642.790136	43.232385
3502.488046	583619.454183	43.237389
3502.313795	583597.875594	43.242394
3502.245395	583571.417835	43.247399
3502.032087	583529.342154	43.252404
3502.122417	583515.291650	43.257409
3502.302968	583490.098157	43.262413
3502.269124	583474.813762	43.267418
3501.760095	583452.585401	43.272423
3501.933631	583416.113526	43.277428
3501.367526	583407.679847	43.282433
3502.035797	583392.285578	43.287437
3501.959684	583369.036890	43.292442
3501.562633	583358.471260	43.297447
3501.998634	583332.886558	43.302452
3501.638326	583312.539632	43.307457
3501.708830	583299.745225	43.312461
3501.959339	583292.587464	43.317466
3501.950686	583288.879119	43.322471
3502.144070	583252.854780	43.327476
3501.729606	583245.700680	43.332481
3501.628539	583219.999150	43.337485
3501.939430	583202.905891	43.342490
3501.598433	583183.207415	43.347495
3501.621756	583157.436162	43.352500
3501.566549	583158.698076	43.357505
3501.787015	583135.703321	43.362509
3501.629142	583116.276888	43.367514
3501.723141	583110.597296	43.372519
3502.102737	583090.485214	43.377524
3501.611489	583067.601579	43.382529
3501.736693	583052.742922	43.387533
3501.766524	583036.645851	43.392538
3501.362238	583032.698476	43.397543
3501.810381	583007.261518	43.402548
3501.578744	582994.864916	43.407553
3501.467624	582980.544429	43.412557
3501.732542	582969.874939	43.417562
3502.105366	582950.214852	43.422567
3502.045503	582920.645978	43.427572
3501.869085	582913.003252	43.432577
3501.670915	582889.521969	43.437581
3501.529638	582864.828552	43.442586
3502.029688	582856.879505	43.447591
3502.221967	582833.537597	43.452596
3502.133322	582820.516847	43.457601
3501.820709	582798.156189	43.462605
3501.879279	582776.940657	43.467610
3501.631441	582766.401263	43.472615
3501.805803	582743.112097	43.477620
3501.761479	582735.699265	43.482625
3501.632373	582700.625939	43.487629
3501.740492	582697.250076	43.492634
3501.766642	582686.768040	43.497639
3501.554112	582657.974332	43.502644
3501.641828	582661.369716	43.507649
3501.655046	582642.717841	43.512653
3501.785687	582623.095033	43.517658
3501.627657	582616.201236	43.522663
3501.707241	582587.863020	43.527668
3502.139295	582588.497351	43.532673
3501.895377	582562.265142	43.537677
3502.102822	582536.513789	43.542682
3501.704849	582521.686070	43.547687
3501.882520	582491.778105	43.552692
3502.073342	582481.821612	43.557697
3501.597705	582463.496530	43.562701
3502.085239	582450.034327	43.567706
3501.709417	582441.520020	43.572711
3502.147598	582407.209369	43.577716
3501.719216	582397.349599	43.582721
3501.835716	582369.355996	43.587725
3501.815501	582358.229139	43.592730
3501.974746	582332.885928	43.597735
3502.044925	582325.103973	43.602740
3501.589887	582301.360780	43.607745
3502.136847	582285.983939	43.612749
3502.091703	582267.992317	43.617754
3501.744027	582247.691582	43.622759
3502.181023	582232.331858	43.627764
3501.748626	582208.685197	43.632769
3501.945208	582184.589206	43.637773
3501.904799	582167.599400	43.642778
3501.871513	582153.817168	43.647783
3501.869879	582122.983649	43.652788
3501.944899	582122.971915	43.657793
3502.115132	582091.359395	43.662797
3501.882091	582077.407750	43.667802
3501.837559	582054.702854	43.672807
3502.249145	582035.185491	43.677812
3501.854918	582013.738458	43.682817
3501.996332	581989.149298	43.687821
3502.411404	581971.386069	43.692826
3502.407235	581960.456851	43.697831
3502.152584	581933.873866	43.702836
3501.765008	581910.470244	43.707841
3502.025956	581883.305162	43.712845
3501.547437	581870.745339	43.717850
3501.744626	581848.052367	43.722855
3501.894910	581835.394204	43.727860
3501.622998	581820.646108	43.732865
3501.528469	581798.449878	43.737869
3501.590603	581791.922249	43.742874
3501.792023	581781.712782	43.747879
3501.834021	581756.988233	43.752884
3501.529974	581748.913409	43.757889
3501.592707	581723.734303	43.762893
3501.625032	581707.885596	43.767898
3501.464871	581705.253305	43.772903
3501.551905	581679.468642	43.777908
3501.494013	581668.647810	43.782913
3501.617273	581658.550724	43.787917
3501.740157	581653.567807	43.792922
3501.735840	581623.736082	43.797927
3501.492126	581605.824562	43.802932
3501.566447	581596.737843	43.807937
3501.570488	581578.988103	43.812941
3501.400094	581561.917409	43.817946
3501.088269	581562.417400	43.822951
3501.498284	581538.186358	43.827956
3501.673416	581534.298276	43.832961
3501.778118	581522.047992	43.837965
3501.866357	581502.580241	43.842970
3501.767152	581499.336702	43.847975
3501.864113	581477.260309	43.852980
3501.543188	581463.672600	43.857985
3501.599112	581457.346302	43.862989
3501.894001	581424.258350	43.867994
3501.708403	581400.069978	43.872999
3501.948121	581385.692575	43.878004
3501.748606	581371.885214	43.883009
3501.967159	581360.569608	43.888013
3501.781811	581335.879659	43.893018
3501.788879	581337.382744	43.898023
3502.309191	581319.451601	43.903028
3501.720201	581300.941744	43.908033
3501.829751	581275.503600	43.913037
3501.819180	581248.579968	43.918042
3501.634046	581246.152032	43.923047
3501.482184	581218.197469	43.928052
3501.658435	581211.200395	43.933057
3501.411010	581200.709577	43.938061
3502.029733	581176.194416	43.943066
3501.914727	581165.281739	43.948071
3501.878753	581145.531935	43.953076
3501.697717	581140.145033	43.958081
3501.681053	581121.043995	43.963085
3501.721357	581096.217955	43.968090
3501.501564	581088.931730	43.973095
3501.607654	581070.413107	43.978100
3501.757150	581049.731599	43.983105
3501.926659	581037.019378	43.988109
3501.944414	581019.768010	43.993114
3501.678732	581006.522091	43.998119
3501.897424	580985.328232	44.003124
3501.757119	580966.547105	44.008129
3501.693975	580952.266628	44.013133
3501.758484	580925.280332	44.018138
3501.731741	580917.612824	44.023143
3502.000415	580901.174455	44.028148
3501.764434	580873.031603	44.033153
3501.695257	580862.963877	44.038157
3501.950213	580843.418763	44.043162
3501.560624	580831.896836	44.048167
3501.879977	580816.202551	44.053172
3501.681680	580790.360139	44.058177
3501.865950	580777.795740	44.063181
3502.116228	580768.480266	44.068186
3501.775229	580746.170028	44.073191
3501.905144	580719.273291	44.078196
3501.984009	580699.354312	44.083201
3501.691498	580676.936069	44.088205
3501.819040	580660.017978	44.093210
3501.335705	580654.477524	44.098215
3501.740810	580638.318297	44.103220
3501.417725	580635.159646	44.108225
3501.563820	580613.424853	44.113229
3501.541446	580608.363889	44.118234
3501.322631	580590.396689	44.123239
3501.524059	580572.313619	44.128244
3501.612491	580573.402942	44.133249
3501.692560	580551.076629	44.138253
3501.635341	580545.018216	44.143258
3501.555166	580540.367405	44.148263
3501.618441	580508.867377	44.153268
3501.606233	580497.436536	44.158273
3501.825769	580486.771754	44.163277
3501.651939	580463.482083	44.168282
3501.659457	580455.357604	44.173287
3501.637919	580436.406581	44.178292
3501.638465	580424.773095	44.183297
3501.471508	580413.917943	44.188301
3501.578517	580397.052806	44.193306
3501.665684	580386.709486	44.198311
3501.529863	580365.068422	44.203316
3501.609291	580353.623108	44.208321
3501.906443	580327.351154	44.213325
3501.968357	580319.518939	44.218330
3501.500403	580301.540073	44.223335
3501.991643	580282.408336	44.228340
3501.830018	580277.469280	44.233345
3501.774422	580248.093170	44.238349
3501.733846	580247.146758	44.243354
3501.743159	580225.833748	44.248359
3501.817074	580201.852914	44.253364
3501.789066	580187.114655	44.258369
3501.751071	580172.277646	44.263373
3501.636518	580164.823925	44.268378
3501.624936	580143.413733	44.273383
3501.502708	580120.767164	44.278388
3501.469289	580119.468604	44.283393
3501.110723	580093.900350	44.288397
3501.723412	580077.958586	44.293402
3501.674028	580078.919066	44.298407
3501.971306	580056.758386	44.303412
3501.712537	580041.905571	44.308417
3501.566079	580025.831680	44.313421
3501.795721	580008.044158	44.318426
3501.677320	579981.234600	44.323431
3502.071266	579978.665710	44.328436
3501.650787	579974.820051	44.333441
3501.601091	579944.990904	44.338445
3501.603879	579921.020584	44.343450
3501.668370	579909.777732	44.348455
3502.178394	579905.435560	44.353460
3501.854822	579884.926130	44.358465
3501.981262	579874.576194	44.363469
3501.918741	579843.344679	44.368474
3501.353305	579838.819580	44.373479
3501.731440	579814.639913	44.378484
3501.021763	579798.403007	44.383489
3501.617740	579793.194859	44.388493
3501.870169	579790.046288	44.393498
3501.826778	579770.295196	44.398503
3501.942047	579746.507504	44.403508
3501.933385	579737.582678	44.408513
3501.386646	579712.243549	44.413517
3501.862648	579702.641162	44.418522
3501.748471	579672.620776	44.423527
3501.617727	579650.425905	44.428532
3501.977396	579649.216282	44.433537
3501.812370	579630.135873	44.438541
3501.923442	579609.507840	44.443546
3501.577064	579594.467531	44.448551
3501.645714	579581.017198	44.453556
3501.558962	579560.720886	44.458561
3501.354885	579542.950277	44.463565
3501.725347	579538.479337	44.468570
3501.538323	579530.234151	44.473575
3501.676108	579502.430577	44.478580
3501.467377	579499.203573	44.483585
3501.386715	579485.926911	44.488589
3501.861658	579462.734312	44.493594
3501.365554	579458.298513	44.498599
3501.740600	579442.041955	44.503604
3501.749232	579432.562549	44.508609
3501.585797	579415.537609	44.513613
3501.336313	579397.824014	44.518618
3500.950007	579381.485794	44.523623
3501.541453	579377.481732	44.528628
3501.328875	579372.349642	44.533633
3501.601136	579366.188929	44.538637
3501.671460	579333.681497	44.543642
3501.458766	579325.289725	44.548647
3501.563523	579319.907406	44.553652
3502.211663	579310.729114	44.558657
3501.766487	579289.084167	44.563661
3501.829775	579275.885050	44.568666
3501.405139	579265.520399	44.573671
3501.687767	579243.861886	44.578676
3501.399497	579230.416777	44.583681
3501.520419	579209.284969	44.588685
3501.413381	579207.747064	44.593690
3501.422710	579198.618395	44.598695
3501.551723	579169.160427	44.603700
3501.731921	579159.503519	44.608705
3501.674341	579148.930929	44.613709
3501.807477	579138.278364	44.618714
3501.450904	579131.413431	44.623719
3501.874577	579105.168967	44.628724
3502.058948	579092.402052	44.633729
3501.712662	579076.307878	44.638733
3501.849439	579043.538461	44.643738
3501.705545	579033.681357	44.648743
3501.581709	579020.360739	44.653748
3501.841344	578990.580978	44.658753
3501.904683	578990.370469	44.663757
3502.134270	578965.710682	44.668762
3501.827693	578953.973219	44.673767
3501.947056	578924.616415	44.678772
3502.009255	578917.084074	44.683777
3501.979467	578888.452602	44.688781
3501.984333	578870.798708	44.693786
3501.532648	578854.319481	44.698791
3501.841352	578830.248839	44.703796
3501.798594	578824.939494	44.708801
3501.712706	578799.425937	44.713805
3501.462340	578785.222094	44.718810
3501.528963	578782.804408	44.723815
3501.948995	578756.860604	44.728820
3501.499181	578753.219707	44.733825
3501.704016	578734.431003	44.738829
3501.979096	578706.052313	44.743834
3502.112904	578704.526838	44.748839
3501.730601	578674.946892	44.753844
3501.765921	578667.067521	44.758849
3501.972778	578647.726685	44.763853
3502.385798	578623.589139	44.768858
3501.545279	578610.731133	44.773863
3501.356275	578593.357868	44.778868
3501.788108	578595.296443	44.783873
3501.718055	578565.165870	44.788877
3501.866324	578551.300630	44.793882
3501.638929	578534.785866	44.798887
3501.807566	578508.981092	44.803892
3501.664184	578498.972977	44.808897
3501.436575	578483.762140	44.813901
3501.809630	578466.250658	44.818906
3501.247887	578465.686483	44.823911
3501.632117	578446.768945	44.828916
3501.721772	578429.702933	44.833921
3501.451605	578421.068698	44.838925
3501.401509	578400.764543	44.843930
3501.664069	578386.078782	44.848935
3501.335184	578376.199863	44.853940
3501.400965	578380.703360	44.858945
3501.635312	578356.994396	44.863949
3501.587709	578328.213813	44.868954
3501.503978	578333.292390	44.873959
3501.120814	578313.290911	44.878964
3501.446516	578296.237948	44.883969
3501.759478	578291.574889	44.888973
3501.661127	578282.261690	44.893978
3501.482089	578258.918064	44.898983
3501.698540	578250.057163	44.903988
3501.942021	578245.605563	44.908993
3501.526359	578223.402237	44.913997
3501.304694	578209.393789	44.919002
3500.920898	578201.128224	44.924007
3501.327667	578178.144236	44.929012
3501.521768	578172.095395	44.934017
3501.719847	578170.309031	44.939021
3501.600486	578148.911856	44.944026
3501.183887	578127.711570	44.949031
3501.366848	578119.507807	44.954036
3501.720808	578121.859875	44.959041
3501.169886	578109.256941	44.964045
3501.357657	578093.178164	44.969050
3501.528180	578092.399184	44.974055
3501.291919	578072.675235	44.979060
3501.300296	578065.451662	44.984065
3501.372417	578045.930230	44.989069
3501.435539	578042.660302	44.994074
3501.419274	578041.960674	44.999079
3501.915388	578027.037312	45.004084
3501.621632	578009.729668	45.009089
3501.673756	577998.787754	45.014093
3501.815093	577971.732137	45.019098
3501.667087	577965.736666	45.024103
3501.558851	577947.396823	45.029108
3501.519915	577930.952014	45.034113
3501.861597	577923.826709	45.039117
3501.745381	577905.738821	45.044122
3501.802314	577886.921661	45.049127
3501.690366	577871.641752	45.054132
3501.260110	577848.085762	45.059137
3501.785295	577834.361334	45.064141
3501.783174	577827.189403	45.069146
3501.644026	577806.095599	45.074151
3501.514533	577800.598703	45.079156
3501.357820	577787.582687	45.084161
3501.126951	577774.528092	45.089165
3501.151374	577754.411738	45.094170
3501.617588	577757.398364	45.099175
3501.855753	577733.035455	45.104180
3501.706850	577713.999401	45.109185
3501.706635	577711.742402	45.114189
3501.661676	577696.000375	45.119194
3501.643866	577677.445328	45.124199
3501.717608	577658.173748	45.129204
3501.335392	577646.747669	45.134209
3501.488772	577620.040415	45.139213
3501.518205	577609.101667	45.144218
3501.382883	577618.752886	45.149223
3501.609240	577598.805310	45.154228
3501.391272	577587.002396	45.159233
3501.278797	577568.411811	45.164237
3501.831051	577562.507280	45.169242
3501.190479	577552.927139	45.174247
3501.614954	577538.164799	45.179252
3501.505198	577523.736740	45.184257
3501.618261	577513.085767	45.189261
3501.536222	577498.201929	45.194266
3501.316939	577496.881961	45.199271
3501.682951	577482.981359	45.204276
3501.381107	577465.272878	45.209281
3501.418268	577458.947244	45.214285
3501.889520	577440.515980	45.219290
3501.526062	577426.478558	45.224295
3501.566952	577403.098763	45.229300
3501.427984	577401.716071	45.234305
3501.885684	577374.609555	45.239309
3501.763810	577359.982549	45.244314
3501.657835	577348.462822	45.249319
3501.597027	577329.512657	45.254324
3501.888773	577332.376201	45.259329
3501.579857	577298.266924	45.264333
3501.608989	577292.293558	45.269338
3501.741212	577282.592374	45.274343
3501.529669	577260.555855	45.279348
3501.559814	577257.792436	45.284353
3501.204668	577245.458866	45.289357
3501.365406	577222.360908	45.294362
3501.485954	577206.341528	45.299367
3501.394329	577194.919716	45.304372
3501.747982	577208.357050	45.309377
3501.416395	577180.320126	45.314381
3501.597346	577164.792829	45.319386
3501.493283	577156.432599	45.324391
3501.279814	577136.502800	45.329396
3501.406255	577117.422687	45.334401
3501.138241	577114.956638	45.339405
3501.420356	577106.536000	45.344410
3501.323024	577094.312436	45.349415
3501.649925	577076.605366	45.354420
3501.240053	577070.750670	45.359425
3501.230815	577067.341293	45.364429
3501.235080	577063.979964	45.369434
3501.211277	577044.321305	45.374439
3501.507522	577030.330732	45.379444
3501.173171	577031.386180	45.384449
3501.476587	577029.232054	45.389453
3501.328152	576999.661269	45.394458
3501.279557	576986.828057	45.399463
3501.426606	576989.363194	45.404468
3501.509324	576991.406792	45.409473
3501.532303	576970.687344	45.414477
3501.074735	576942.418722	45.419482
3501.318690	576945.741273	45.424487
3501.525171	576927.149920	45.429492
3501.847763	576916.315147	45.434497
3501.880171	576902.917418	45.439501
3501.675600	576884.390254	45.444506
3501.362581	576872.450966	45.449511
3501.515564	576853.516735	45.454516
3501.557807	576853.610446	45.459521
3501.823016	576824.024693	45.464525
3501.945826	576814.826178	45.469530
3501.448231	576805.524002	45.474535
3501.436808	576777.686821	45.479540
3501.453853	576765.344697	45.484545
3501.599227	576756.393409	45.489549
3501.468091	576728.875784	45.494554
3501.508613	576733.283573	45.499559
3501.657900	576716.506593	45.504564
3501.353659	576700.101452	45.509569
3501.389923	576689.461704	45.514573
3501.569816	576669.068294	45.519578
3501.191789	576675.447649	45.524583
3501.647897	576655.011033	45.529588
3501.636808	576653.558095	45.534593
3501.533493	576645.448171	45.539597
3501.881410	576616.250229	45.544602
3501.463779	576616.315511	45.549607
3501.453138	576598.259168	45.554612
3501.722340	576576.396955	45.559617
3501.555255	576567.544525	45.564621
3501.595266	576563.374876	45.569626
3501.248689	576541.759344	45.574631
3501.507572	576530.934160	45.579636
3501.680060	576531.458965	45.584641
3501.703982	576507.979636	45.589645
3501.394962	576484.552305	45.594650
3501.607405	576481.960844	45.599655
3501.400071	576461.978725	45.604660
3501.374098	576447.536182	45.609665
3501.227687	576450.568775	45.614669
3501.023683	576438.762466	45.619674
3501.278939	576436.063978	45.624679
3501.311333	576414.840413	45.629684
3501.391107	576413.172592	45.634689
3501.656221	576390.758875	45.639693
3501.474065	576381.507357	45.644698
3501.105082	576373.288281	45.649703
3501.438448	576353.121117	45.654708
3501.724806	576351.922614	45.659713
3501.572464	576328.420302	45.664717
3501.666639	576318.021961	45.669722
3501.738072	576320.819883	45.674727
3501.776306	576285.298870	45.679732
3501.351508	576276.135359	45.684737
3501.288710	576264.657931	45.689741
3501.454427	576261.271122	45.694746
3501.032751	576246.739693	45.699751
3501.737032	576227.367085	45.704756
3501.205161	576223.788341	45.709761
3501.367628	576219.047631	45.714765
3501.872776	576193.034434	45.719770
3501.204981	576186.416985	45.724775
3501.628587	576182.989837	45.729780
3501.578455	576150.542155	45.734785
3501.237709	576146.933507	45.739789
3501.437710	576131.702785	45.744794
3501.508420	576134.199888	45.749799
3501.674978	576108.189263	45.754804
3501.643215	576103.579195	45.759809
3501.320105	576097.860913	45.764813
3501.246375	576055.885599	45.769818
3501.278040	576007.322198	45.774823
3501.099015	575905.416892	45.779828
3501.571005	575743.261254	45.784833
3500.745483	575542.477811	45.789837
3500.126440	575290.889635	45.794842
3499.661076	574997.230868	45.799847
3499.619851	574658.997635	45.804852
3498.941285	574270.782851	45.809857
3498.358128	573841.849253	45.814861
3498.273251	573362.294856	45.819866
3497.254260	572851.254245	45.824871
3496.959147	572285.180358	45.829876
3495.815258	571672.289996	45.834881
3494.436523	571015.139521	45.839885
3493.864177	570322.040515	45.844890
3492.745732	569596.360095	45.849895
3491.561584	568813.622063	45.854900
3490.281964	568005.444985	45.859905
3489.142871	567145.731539	45.864909
3487.960903	566255.736497	45.869914
3486.388337	565318.887701	45.874919
3484.683565	564348.942728	45.879924
3483.536402	563350.154786	45.884929
3481.665977	562300.618622	45.889933
3479.947950	561232.531023	45.894938
3477.752766	560124.988345	45.899943
3476.116847	558977.415904	45.904948
3474.127354	557805.872177	45.909953
3472.234064	556606.009127	45.914957
3470.384920	555378.982645	45.919962
3467.957300	554111.915608	45.924967
3465.793930	552817.230063	45.929972
3464.085141	551509.466019	45.934977
3461.105202	550165.964470	45.939981
3459.123376	548798.929492	45.944986
3456.607973	547406.833394	45.949991
3454.064597	545989.639620	45.954996
3451.519922	544545.475123	45.960001
3449.134565	543092.465745	45.965005
3446.517082	541605.666693	45.970010
3443.656798	540111.685340	45.975015
3441.318346	538589.567439	45.980020
3438.498586	537048.771242	45.985025
3435.712496	535493.086108	45.990029
3432.996033	533904.681711	45.995034
3429.869250	532316.195974	46.000039
3427.400725	530701.430762	46.005044
3423.785675	529082.263440	46.010049
3420.639550	527451.742386	46.015053
3417.667506	525797.670497	46.020058
3414.555069	524149.761611	46.025063
3411.966747	522469.875720	46.030068
3408.623158	520787.377916	46.035073
3405.335367	519090.248140	46.040077
3402.205262	517383.153717	46.045082
3399.058234	515674.285787	46.050087
3395.850406	513938.898021	46.055092
3392.508473	512191.918059	46.060097
3388.804685	510454.558267	46.065101
3385.921540	508706.011200	46.070106
3382.396211	506947.814304	46.075111
3378.764476	505165.403425	46.080116
3375.450813	503400.176988	46.085121
3371.734393	501629.649847	46.090125
3368.137317	499834.260254	46.095130
3364.501398	498044.358699	46.100135
3361.225285	496237.827634	46.105140
3357.623727	494442.333869	46.110145
3354.306774	492654.152281	46.115149
3350.724111	490843.883432	46.120154
3346.678378	489040.085416	46.125159
3343.286429	487228.899793	46.130164
3339.733148	485419.697029	46.135169
3335.899281	483606.890316	46.140173
3332.681123	481797.362890	46.145178
3328.693604	479993.203702	46.150183
3325.205303	478171.577039	46.155188
3321.172591	476351.848053	46.160193
3317.709743	474527.627221	46.165197
3313.934041	472705.119193	46.170202
3310.338221	470884.805242	46.175207
3306.443916	469068.886245	46.180212
3302.745500	467257.136203	46.185217
3298.870115	465427.311934	46.190221
3295.219694	463610.606180	46.195226
3291.246410	461795.677579	46.200231
3287.804003	459988.668315	46.205236
3284.252089	458175.970399	46.210241
3280.201012	456359.466235	46.215245
3276.616616	454539.764285	46.220250
3272.837417	452727.243254	46.225255
3268.978400	450914.194763	46.230260
3265.119818	449098.734534	46.235265
3261.495055	447287.307482	46.240269
3257.710409	445486.459153	46.245274
3253.422108	443680.499028	46.250279
3249.602720	441873.731751	46.255284
3245.778545	440079.350886	46.260289
3241.857697	438289.423146	46.265293
3238.331596	436495.313073	46.270298
3234.222765	434714.906108	46.275303
3230.762503	432916.701941	46.280308
3227.102530	431132.095032	46.285313
3222.815694	429358.927533	46.290317
3219.103627	427589.160334	46.295322
3215.081783	425817.054448	46.300327
3211.512595	424040.717273	46.305332
3207.860314	422273.920669	46.310337
3203.650523	420509.796835	46.315341
3199.979441	418751.370789	46.320346
3196.226223	416993.620922	46.325351
3192.172471	415235.162985	46.330356
3188.590200	413492.208212	46.335361
3184.602143	411739.538586	46.340365
3181.374837	409985.644638	46.345370
3176.968146	408243.107202	46.350375
3173.271579	406503.010263	46.355380
3169.259497	404767.850013	46.360385
3165.823671	403029.269499	46.365389
3162.234630	401305.499107	46.370394
3158.104805	399590.412796	46.375399
3154.524262	397857.858339	46.380404
3150.673941	396138.110116	46.385409
3146.353060	394419.072131	46.390413
3142.763280	392708.172344	46.395418
3138.929182	391000.997317	46.400423
3135.242696	389289.669219	46.405428
3131.595997	387594.743181	46.410433
3127.605724	385892.215494	46.415437
3124.134411	384181.290832	46.420442
3119.974777	382494.811454	46.425447
3116.240159	380804.930402	46.430452
3112.489415	379118.751664	46.435457
3108.496776	377436.769598	46.440461
3104.979882	375761.312215	46.445466
3100.945243	374083.621922	46.450471
3096.944828	372403.867181	46.455476
3093.663992	370750.519959	46.460481
3089.887701	369080.004276	46.465485
3086.059968	367426.368982	46.470490
3082.246322	365765.648739	46.475495
3078.469653	364103.429833	46.480500
3074.419487	362455.592309	46.485505
3070.735140	360810.223296	46.490509
3066.823131	359174.634434	46.495514
3063.031858	357531.949580	46.500519
3059.630208	355884.973219	46.505524
3055.979252	354263.213283	46.510529
3051.889600	352632.872495	46.515533
3048.424924	351006.265340	46.520538
3044.794489	349384.050958	46.525543
3040.788679	347754.620477	46.530548
3037.204041	346146.501549	46.535553
3033.257569	344519.776941	46.540557
3029.955055	342910.036500	46.545562
3026.173770	341294.498642	46.550567
3022.628190	339689.910752	46.555572
3018.600359	338075.230438	46.560577
3014.694940	336478.768621	46.565581
3010.680291	334872.081621	46.570586
3007.143090	333279.314685	46.575591
3003.154886	331681.922026	46.580596
3000.049284	330093.938978	46.585601
2996.177990	328512.852965	46.590605
2992.351218	326909.922706	46.595610
2988.493294	325339.035674	46.600615
2985.031059	323752.279526	46.605620
2981.224511	322170.375322	46.610625
2977.487428	320611.577167	46.615629
2973.854264	319040.900982	46.620634
2970.041843	317473.045593	46.625639
2966.183828	315901.732275	46.630644
2962.541259	314340.838818	46.635649
2958.719875	312781.904776	46.640653
2955.438110	311223.622969	46.645658
2951.558189	309673.373775	46.650663
2947.757943	308120.568469	46.655668
2944.186645	306571.139315	46.660673
2940.850549	305024.730282	46.665677
2937.027682	303468.119690	46.670682
2933.003447	301922.972360	46.675687
2929.617317	300371.877406	46.680692
2926.038717	298834.436024	46.685697
2922.198900	297302.032491	46.690701
2918.703536	295761.133924	46.695706
2914.882760	294232.768650	46.700711
2911.064761	292694.690575	46.705716
2907.548998	291160.318971	46.710721
2903.692057	289629.170135	46.715725
2900.289904	288111.456134	46.720730
2896.472457	286597.361049	46.725735
2892.636863	285070.174420	46.730740
2889.357828	283545.896091	46.735745
2884.905143	282037.425368	46.740749
2881.202732	280522.746254	46.745754
2877.717952	279016.505656	46.750759
2874.086765	277494.523436	46.755764
2870.497278	275998.016951	46.760769
2866.866501	274499.910441	46.765773
2863.158295	272989.007043	46.770778
2859.326127	271488.815965	46.775783
2855.751072	270003.276651	46.780788
2852.323942	268510.738527	46.785793
2848.163493	267020.735956	46.790797
2845.245179	265534.310513	46.795802
2841.216829	264054.377463	46.800807
2837.545355	262573.858457	46.805812
2833.541285	261091.843494	46.810817
2829.997829	259611.265101	46.815821
2826.763528	258130.696276	46.820826
2823.011096	256669.341206	46.825831
2819.364738	255178.590494	46.830836
2816.017530	253711.307739	46.835841
2812.226496	252245.098027	46.840845
2808.492874	250770.308170	46.845850
2804.819725	249317.320654	46.850855
2801.358167	247831.638287	46.855860
2797.794108	246369.440890	46.860865
2794.076642	244915.202358	46.865869
2790.413171	243442.684589	46.870874
2786.350837	241995.331125	46.875879
2782.894327	240534.299666	46.880884
2778.971932	239074.300842	46.885889
2775.508345	237630.370081	46.890893
2771.908957	236177.463753	46.895898
2768.203304	234729.534764	46.900903
2764.939270	233285.046500	46.905908
2761.461874	231845.044517	46.910913
2757.521436	230401.367621	46.915917
2754.276560	228958.139585	46.920922
2750.146845	227524.038572	46.925927
2746.601941	226078.078198	46.930932
2743.086982	224642.784206	46.935937
2739.443929	223206.619089	46.940941
2736.111478	221769.005582	46.945946
2731.625511	220350.599532	46.950951
2728.057628	218914.962600	46.955956
2724.589715	217488.965883	46.960961
2721.177044	216068.210913	46.965965
2717.604535	214640.583407	46.970970
2713.349389	213222.083801	46.975975
2709.836516	211811.089059	46.980980
2706.278937	210394.097271	46.985985
2703.000205	208981.704340	46.990989
2699.753149	207566.054432	46.995994
2695.782005	206166.087307	47.000999
2692.127467	204756.885905	47.006004
2688.189197	203345.421241	47.011009
2684.758426	201940.789494	47.016013
2681.284186	200536.379488	47.021018
2677.610123	199146.070373	47.026023
2673.796747	197740.948250	47.031028
2670.274473	196336.685167	47.036033
2666.323041	194942.231207	47.041037
2663.197832	193562.432647	47.046042
2659.365140	192174.941497	47.051047
2655.559650	190785.348003	47.056052
2652.298675	189397.850114	47.061057
2648.458221	188020.340034	47.066061
2645.124281	186634.033673	47.071066
2641.357023	185245.979787	47.076071
2637.531708	183861.315015	47.081076
2634.400232	182485.702455	47.086081
2630.407168	181105.992091	47.091085
2626.878507	179730.405487	47.096090
2623.048714	178358.018877	47.101095
2619.356554	176983.238903	47.106100
2615.912663	175611.434100	47.111105
2612.321950	174240.782636	47.116109
2608.623936	172879.095294	47.121114
2605.040886	171529.927340	47.126119
2601.060563	170161.839798	47.131124
2597.665832	168805.422540	47.136129
2594.104795	167453.550137	47.141133
2590.675572	166099.569906	47.146138
2586.877118	164753.120314	47.151143
2583.357997	163393.454297	47.156148
2579.726688	162049.082324	47.161153
2575.887736	160703.421587	47.166157
2572.184485	159357.424560	47.171162
2568.602311	158017.750635	47.176167
2565.433075	156679.734355	47.181172
2561.714259	155323.698178	47.186177
2557.967628	153993.087456	47.191181
2554.529293	152652.011049	47.196186
2550.768018	151324.124919	47.201191
2547.051041	149987.686616	47.206196
2543.317408	148652.619982	47.211201
2540.076021	147339.307853	47.216205
2536.708528	145943.286451	47.221210
2532.754706	144589.054323	47.226215
2528.989207	143267.199013	47.231220
2525.473656	141940.377415	47.236225
2521.954982	140625.170505	47.241229
2518.193794	139302.161802	47.246234
2514.651201	137983.048890	47.251239
2510.802810	136674.669589	47.256244
2507.221200	135358.423519	47.261249
2503.397889	134063.167711	47.266253
2500.129279	132745.689508	47.271258
2496.500613	131447.680806	47.276263
2492.831564	130140.354878	47.281268
2489.323519	128850.940741	47.286273
2485.699702	127550.683212	47.291277
2481.998327	126257.321272	47.296282
2478.376476	124967.357981	47.301287
2474.799909	123668.563725	47.306292
2471.330648	122367.912411	47.311297
2467.512600	121093.391354	47.316301
2464.302150	119801.699333	47.321306
2460.494758	118522.695315	47.326311
2457.003380	117227.445858	47.331316
2453.473914	115943.894602	47.336321
2449.456643	114672.187513	47.341325
2446.182232	113369.930085	47.346330
2442.521947	112086.063154	47.351335
2439.110445	110817.104052	47.356340
2435.047776	109551.038179	47.361345
2431.340892	108275.439943	47.366349
2428.099191	106998.328252	47.371354
2423.978283	105743.469978	47.376359
2420.774015	104481.154354	47.381364
2417.575715	103217.448645	47.386369
2413.317117	101950.092533	47.391373
2409.848949	100698.168064	47.396378
2406.195502	99436.597441	47.401383
2402.800623	98176.764017	47.406388
2399.027945	96924.130785	47.411393
2395.355474	95674.225512	47.416397
2391.730635	94418.567717	47.421402
2388.120232	93184.942091	47.426407
2384.297187	91943.114232	47.431412
2380.550733	90697.462178	47.436417
2376.675350	89465.273531	47.441421
2373.648431	88238.339047	47.446426
2369.679626	87002.976057	47.451431
2366.181584	85781.095890	47.456436
2362.435906	84556.002688	47.461441
2359.112462	83335.163614	47.466445
2355.453292	82106.489929	47.471450
2351.617711	80893.050551	47.476455
2347.961804	79679.444822	47.481460
2344.596201	78465.935322	47.486465
2340.335370	77262.868274	47.491469
2337.245668	76044.151498	47.496474
2333.653594	74846.178772	47.501479
2329.777900	73647.693993	47.506484
2326.226128	72440.120256	47.511489
2322.637360	71243.844505	47.516493
2319.235114	70052.266322	47.521498
2315.075929	68872.230450	47.526503
2311.695103	67667.617109	47.531508
2308.059465	66485.983117	47.536513
2304.508166	65305.323580	47.541517
2300.617146	64133.708733	47.546522
2297.220996	62954.302537	47.551527
2293.310571	61785.009014	47.556532
2289.983914	60612.131741	47.561537
2286.153808	59443.355184	47.566541
2282.732070	58274.576907	47.571546
2278.832247	57111.227908	47.576551
2275.086649	55959.896443	47.581556
2271.835654	54810.693751	47.586561
2267.905538	53647.352717	47.591565
2264.284241	52501.453955	47.596570
2260.530845	51349.935166	47.601575
2257.066449	50210.385308	47.606580
2253.820034	49061.006634	47.611585
2250.027575	47929.606615	47.616589
2246.294360	46792.995457	47.621594
2242.547184	45660.648200	47.626599
2238.679350	44534.071588	47.631604
2235.220633	43415.319316	47.636609
2231.140862	42293.537125	47.641613
2227.857485	41170.628267	47.646618
2223.953494	40062.476024	47.651623
2220.254887	38955.780697	47.656628
2216.660364	37841.688771	47.661633
2212.897403	36752.259083	47.666637
2209.068747	35648.390794	47.671642
2205.409933	34569.369812	47.676647
2201.621020	33473.449335	47.681652
2197.838963	32398.215711	47.686657
2194.511081	31319.347186	47.691661
2190.974441	30250.060840	47.696666
2186.766349	29183.108354	47.701671
2182.798361	28120.457276	47.706676
2179.573935	27054.487899	47.711681
2175.470330	26000.921791	47.716685
2171.955215	24955.257283	47.721690
2168.159994	23925.061027	47.726695
2164.040359	22878.566286	47.731700
2160.527465	21847.146718	47.736705
2156.448999	20829.140281	47.741709
2152.633976	19807.211456	47.746714
2148.870579	18809.973257	47.751719
2145.310589	17808.434498	47.756724
2141.038983	16820.592977	47.761729
2136.985411	15850.329229	47.766733
2133.164747	14868.726480	47.771738
2129.039053	13909.271070	47.776743
2124.938480	12964.297081	47.781748
2120.897172	12033.933369	47.786753
2116.518654	11119.113767	47.791757
2112.375229	10201.987772	47.796762
2107.837053	9312.903271	47.801767
2103.096733	8450.765957	47.806772
2098.239071	7614.001745	47.811777
2092.374279	6820.426283	47.816781
2086.274158	6063.618468	47.821786
2078.776729	5385.954517	47.826791
2071.586801	4756.253050	47.831796
2065.009951	4165.037344	47.836801
2058.744303	3625.894784	47.841805
2052.775265	3145.433424	47.846810
2046.706491	2701.617558	47.851815
2041.299771	2302.349781	47.856820
2036.178972	1942.294278	47.861825
2031.011266	1611.394655	47.866829
2027.229201	1320.299988	47.871834
2022.649097	1066.391684	47.876839
2018.459121	814.969763	47.881844
2014.616803	583.407504	47.886849
2010.442673	389.787636	47.891853
2006.854835	213.068014	47.896858
2001.697866	91.165344	47.901863
1991.330741	124.220219	47.906868
1984.398759	120.998919	47.911873
1979.915396	126.895471	47.916877
1977.745337	118.404763	47.921882
1976.205160	117.652316	47.926887
1974.085631	121.549609	47.931892
1972.316801	122.936891	47.936897
1969.954717	125.217455	47.941901
1967.261139	121.136795	47.946906
1963.915575	118.660981	47.951911
1960.433954	127.922138	47.956916
1957.421590	118.247083	47.961921
1954.206437	121.363507	47.966925
1950.941841	122.216036	47.971930
1947.583914	121.188034	47.976935
1944.035610	125.039981	47.981940
1941.337384	122.700165	47.986945
1937.848100	124.673053	47.991949
1934.669322	118.371384	47.996954
1931.452055	124.680454	48.001959
1927.715538	123.059950	48.006964
1924.596368	117.685452	48.011969
1921.306171	130.861967	48.016973
1918.473226	117.349593	48.021978
1914.669663	123.098663	48.026983
1910.912325	131.706936	48.031988
1907.971400	125.497771	48.036993
1904.780186	127.670805	48.041997
1901.598849	125.760948	48.047002
1898.186227	130.158005	48.052007
1894.167438	137.997257	48.057012
1890.764813	123.507822	48.062017
1886.945516	119.774191	48.067021
1883.703476	122.163997	48.072026
1880.679473	132.786783	48.077031
1877.310622	124.287536	48.082036
1873.977177	121.639007	48.087041
1870.079065	130.826156	48.092045
1866.939532	126.375537	48.097050
1863.705336	114.561679	48.102055
1860.375141	136.122295	48.107060
1857.053153	126.236290	48.112065
1853.358585	125.545743	48.117069
1849.648431	117.666246	48.122074
1845.743923	127.578918	48.127079
1842.364180	124.260585	48.132084
1839.691113	117.471677	48.137089
1835.868937	121.796796	48.142093
1832.649946	126.372381	48.147098
1829.504060	123.216778	48.152103
1825.614298	119.522673	48.157108
1822.307324	120.932379	48.162113
1818.553952	121.032513	48.167117
1815.415768	121.922249	48.172122
1811.769317	116.408838	48.177127
1807.835749	113.648599	48.182132
1805.134256	109.686290	48.187137
1801.521527	117.509474	48.192141
1798.253592	123.753739	48.197146
1794.249370	116.676441	48.202151
1790.681486	125.546170	48.207156
1787.267882	113.915448	48.212161
1784.089902	116.222488	48.217165
1780.544263	118.561757	48.222170
1777.247807	114.632451	48.227175
1773.432547	122.544289	48.232180
1769.959457	115.459815	48.237185
1766.612531	129.803199	48.242189
1763.271011	127.393259	48.247194
1760.211579	128.065038	48.252199
1756.606634	123.605033	48.257204
1752.988470	116.315474	48.262209
1749.343399	122.334027	48.267213
1746.210230	113.117731	48.272218
1742.128081	119.964006	48.277223
1738.581930	116.975480	48.282228
1735.430333	114.254248	48.287233
1731.706731	124.942252	48.292237
1728.749453	110.250324	48.297242
1725.097771	109.160798	48.302247
1721.335571	120.050999	48.307252
1717.852671	117.906817	48.312257
1714.323851	116.525976	48.317261
1710.643660	122.398174	48.322266
1707.704456	118.833770	48.327271
1703.991317	121.689670	48.332276
1700.630998	118.270270	48.337281
1696.896142	124.622437	48.342285
1693.713515	111.762845	48.347290
1690.292321	114.180744	48.352295
1686.456610	124.269359	48.357300
1682.948052	113.681786	48.362305
1679.318719	119.634620	48.367309
1676.211940	124.572345	48.372314
1672.497522	117.718671	48.377319
1669.202723	122.549779	48.382324
1666.098578	115.176645	48.387329
1662.341005	120.247864	48.392333
1658.857828	121.935139	48.397338
1655.332748	123.293608	48.402343
1651.440118	123.649720	48.407348
1648.113399	122.996591	48.412353
1644.389346	127.350711	48.417357
1640.954855	119.108612	48.422362
1637.741562	127.397691	48.427367
1634.532609	132.288143	48.432372
1631.190964	120.127354	48.437377
1626.791887	127.285870	48.442381
1623.675809	116.541980	48.447386
1620.260785	115.845732	48.452391
1616.891213	120.691721	48.457396
1613.694001	109.659974	48.462401
1609.728683	119.161438	48.467405
1606.151642	121.151329	48.472410
1602.703290	122.896449	48.477415
1599.346187	122.814416	48.482420
1595.941434	121.385725	48.487425
1592.177958	122.670793	48.492429
1588.954542	110.823726	48.497434
1585.264521	119.646183	48.502439
1581.696931	116.971126	48.507444
1578.658518	118.111078	48.512449
1574.762323	120.280649	48.517453
1571.421975	113.077400	48.522458
1567.797484	118.441038	48.527463
1564.411451	114.731476	48.532468
1560.902510	110.788048	48.537473
1557.321512	118.065322	48.542477
1554.072857	115.033467	48.547482
1550.384696	114.044628	48.552487
1546.576873	122.771637	48.557492
1543.576811	116.043497	48.562497
1539.526326	122.821609	48.567501
1536.343015	115.321705	48.572506
1532.949884	122.095010	48.577511
1529.184029	120.074278	48.582516
1526.362653	106.664661	48.587521
1522.482222	113.827456	48.592525
1519.045578	121.294124	48.597530
1515.695102	118.455392	48.602535
1511.530073	118.813064	48.607540
1508.127842	111.790373	48.612545
1504.544923	123.449857	48.617549
1501.669482	114.797605	48.622554
1498.281696	122.816628	48.627559
1494.520694	113.654405	48.632564
1490.789574	107.467830	48.637569
1487.010083	114.836304	48.642573
1483.795742	106.702190	48.647578
1480.664611	108.378712	48.652583
1476.955513	110.886036	48.657588
1473.703510	101.982687	48.662593
1469.760466	113.761818	48.667597
1466.460908	110.842368	48.672602
1462.919025	118.284393	48.677607
1459.130546	115.302265	48.682612
1456.301520	111.350531	48.687617
1452.472837	110.896263	48.692621
1448.775411	114.385718	48.697626
1445.030864	109.523739	48.702631
1441.935783	105.458628	48.707636
1438.652094	103.634550	48.712641
1435.092590	107.140385	48.717645
1431.467789	95.052497	48.722650
1428.150878	111.672348	48.727655
1424.790259	117.412351	48.732660
1421.107047	112.031406	48.737665
1416.930217	109.189180	48.742669
1413.678306	110.207572	48.747674
1410.303879	103.474807	48.752679
1406.972624	111.921608	48.757684
1403.853948	103.551084	48.762689
1399.919655	108.279882	48.767693
1396.617562	106.639036	48.772698
1393.061358	113.203780	48.777703
1389.511202	100.461969	48.782708
1385.653874	107.583223	48.787713
1382.196324	112.253220	48.792717
1378.905857	103.466663	48.797722
1375.793437	106.741179	48.802727
1372.159281	116.330086	48.807732
1368.368262	111.434283	48.812737
1364.593025	115.239673	48.817741
1361.173912	112.348466	48.822746
1358.347701	108.497565	48.827751
1354.611539	111.319221	48.832756
1351.164849	109.988933	48.837761
1347.383026	108.189077	48.842765
1343.473124	104.703976	48.847770
1340.305651	103.118008	48.852775
1336.823011	106.440997	48.857780
1333.596449	99.862291	48.862785
1329.855011	108.964954	48.867789
1326.883440	113.289969	48.872794
1323.282502	106.928060	48.877799
1319.302131	115.036727	48.882804
1315.680587	112.196208	48.887809
1312.194077	109.005517	48.892813
1308.918438	112.504923	48.897818
1305.408770	110.140451	48.902823
1302.202781	116.894014	48.907828
1298.761547	104.268072	48.912833
1294.931677	109.069147	48.917837
1291.446136	99.474754	48.922842
1287.845334	104.445620	48.927847
1284.247116	111.276405	48.932852
1280.873974	101.946000	48.937857
1277.140891	112.660917	48.942861
1273.754474	109.413441	48.947866
1270.004225	115.046800	48.952871
1266.444502	112.361141	48.957876
1263.738215	112.354513	48.962881
1260.335136	109.242531	48.967885
1256.488678	108.563328	48.972890
1252.835842	111.897169	48.977895
1249.020316	119.062550	48.982900
1246.125398	104.819821	48.987905
1242.491314	111.554993	48.992909
1239.211101	104.886642	48.997914
1235.494221	104.990771	49.002919
1231.923181	105.451728	49.007924
1228.513809	99.176933	49.012929
1224.963941	111.865874	49.017933
1221.148696	107.875615	49.022938
1218.058280	101.709082	49.027943
1214.376459	103.604775	49.032948
1210.890029	96.832678	49.037953
1207.145857	108.150472	49.042957
1203.830427	109.257970	49.047962
1200.324744	118.504105	49.052967
1196.636528	116.591576	49.057972
1193.607439	103.619582	49.062977
1189.887612	108.270586	49.067981
1186.507829	103.721779	49.072986
1183.213248	105.186694	49.077991
1179.226022	113.951389	49.082996
1176.018476	101.937503	49.088001
1172.083758	112.437239	49.093005
1168.891550	111.782197	49.098010
1165.411287	104.585200	49.103015
1161.637823	108.067674	49.108020
1157.918188	101.439676	49.113025
1154.795312	106.092149	49.118029
1151.446327	111.805098	49.123034
1148.232526	108.438895	49.128039
1144.579041	105.334522	49.133044
1141.160384	102.041524	49.138049
1137.272965	103.336671	49.143053
1133.775061	109.670899	49.148058
1130.582896	105.399630	49.153063
1127.064042	106.459906	49.158068
1123.535871	98.697780	49.163073
1119.520377	102.142228	49.168077
1115.937145	105.651883	49.173082
1112.521716	107.214837	49.178087
1109.242027	103.713429	49.183092
1106.273373	97.888550	49.188097
1102.120243	100.225074	49.193101
1098.870842	100.689508	49.198106
1095.438432	102.751843	49.203111
1091.808641	105.443042	49.208116
1088.533255	102.627515	49.213121
1084.746449	95.162169	49.218125
1081.243042	104.411138	49.223130
1078.049410	104.737131	49.228135
1074.041237	105.687371	49.233140
1070.552092	101.434148	49.238145
1067.027837	105.912202	49.243149
1063.932953	98.319550	49.248154
1060.538684	111.879529	49.253159
1056.883362	107.440351	49.258164
1053.727878	99.445896	49.263169
1049.769902	100.049759	49.268173
1046.064737	100.487490	49.273178
1042.869003	103.117075	49.278183
1039.144275	106.750152	49.283188
1035.705495	95.155356	49.288193
1032.225371	103.910304	49.293197
1028.911186	101.376124	49.298202
1025.463414	104.241332	49.303207
1021.677914	99.983907	49.308212
1018.199292	101.050578	49.313217
1014.387565	106.880311	49.318221
1011.260340	94.955167	49.323226
1007.845355	100.039401	49.328231
1004.258840	104.612647	49.333236
1000.937623	98.545609	49.338241
997.140248	98.722545	49.343245
993.606862	94.748368	49.348250
990.388981	99.842876	49.353255
986.666357	99.919525	49.358260
983.413735	94.620052	49.363265
979.570060	107.962506	49.368269
976.506284	95.967330	49.373274
972.804132	93.079460	49.378279
969.175923	90.142050	49.383284
965.557980	96.944380	49.388289
962.171339	99.426708	49.393293
959.147709	99.390759	49.398298
955.571429	98.150512	49.403303
951.676385	97.747964	49.408308
948.343970	99.459329	49.413313
944.730660	102.483363	49.418317
940.744017	98.412495	49.423322
937.702042	95.671210	49.428327
933.907202	92.740922	49.433332
931.112460	92.140788	49.438337
927.293546	96.279040	49.443341
923.660636	90.184911	49.448346
920.260898	96.168467	49.453351
916.401588	102.299917	49.458356
913.156487	95.863487	49.463361
909.552717	98.727849	49.468365
905.877125	91.688106	49.473370
902.744193	102.315481	49.478375
899.191394	99.606738	49.483380
896.020934	92.092429	49.488385
892.212335	93.726512	49.493389
888.754883	96.545824	49.498394
885.103549	98.569743	49.503399
881.243795	101.781087	49.508404
877.967891	99.987627	49.513409
874.472896	97.469163	49.518413
871.134723	102.076334	49.523418
867.912932	102.998437	49.528423
864.015699	106.946496	49.533428
860.927140	95.986649	49.538433
857.444021	103.021009	49.543437
853.861979	98.867843	49.548442
850.411368	98.370434	49.553447
846.385222	93.151010	49.558452
842.969779	94.011695	49.563457
839.547106	110.739972	49.568461
835.925158	95.383717	49.573466
832.499292	98.514482	49.578471
829.000534	104.254142	49.583476
826.161231	92.869298	49.588481
822.097547	104.325821	49.593485
818.480828	96.786507	49.598490
814.936702	102.106163	49.603495
811.249240	97.336763	49.608500
808.171051	87.068192	49.613505
804.639890	99.523348	49.618509
801.313243	98.905304	49.623514
797.726015	97.246048	49.628519
793.886271	109.423663	49.633524
790.597339	98.267429	49.638529
787.105053	97.697475	49.643533
783.566821	95.356663	49.648538
780.150552	92.278572	49.653543
776.420474	107.783153	49.658548
773.141348	98.672369	49.663553
769.377705	107.791337	49.668557
766.015354	101.898516	49.673562
762.381161	103.818556	49.678567
759.558775	105.456445	49.683572
756.005703	101.513921	49.688577
752.090692	113.133855	49.693581
748.388161	104.272884	49.698586
745.100738	98.918840	49.703591
741.247191	111.914895	49.708596
738.209425	101.035730	49.713601
734.574107	96.115827	49.718605
730.932653	103.386997	49.723610
727.582656	104.196345	49.728615
723.818370	100.628601	49.733620
720.225541	92.971695	49.738625
716.886655	91.488719	49.743629
713.660865	100.457033	49.748634
710.311554	95.100042	49.753639
706.437938	97.547985	49.758644
703.109803	90.507706	49.763649
699.461018	90.373587	49.768653
695.894206	92.631117	49.773658
692.731406	94.126179	49.778663
689.236578	96.707801	49.783668
685.912095	96.703236	49.788673
681.851540	98.601491	49.793677
678.036894	93.007335	49.798682
674.732265	85.058544	49.803687
671.642282	96.811884	49.808692
668.633528	85.944034	49.813697
664.534092	89.566323	49.818701
660.876380	90.221403	49.823706
657.523417	91.160955	49.828711
654.099080	90.077368	49.833716
650.365854	93.607511	49.838721
646.883735	87.315881	49.843725
643.337961	92.167609	49.848730
639.947891	91.395040	49.853735
636.258393	97.420901	49.858740
632.920882	100.534733	49.863745
629.057766	86.301546	49.868749
625.751126	80.789213	49.873754
622.489924	87.893291	49.878759
618.733271	88.320271	49.883764
615.787166	85.083190	49.888769
612.045564	98.216769	49.893773
608.206834	91.693099	49.898778
604.855713	96.109390	49.903783
601.579524	101.428285	49.908788
598.019942	88.457385	49.913793
594.556281	95.662786	49.918797
590.730025	91.089232	49.923802
587.367747	92.628225	49.928807
583.528281	97.348800	49.933812
580.711979	92.560125	49.938817
577.217244	87.529691	49.943821
573.436292	89.286123	49.948826
569.583585	87.940624	49.953831
566.116548	87.426913	49.958836
563.078781	81.942099	49.963841
559.533356	97.484248	49.968845
555.762371	89.440866	49.973850
552.159358	88.072087	49.978855
548.611425	96.992821	49.983860
545.394624	94.975091	49.988865
541.590193	87.977841	49.993869
538.218344	89.065929	49.998874
535.174381	95.974659	50.003879
531.216105	101.457353	50.008884
527.844844	92.917938	50.013889
524.384515	95.927655	50.018893
520.898500	94.148253	50.023898
517.190592	90.752109	50.028903
513.776774	97.778886	50.033908
510.549898	93.206404	50.038913
506.954261	95.069881	50.043917
503.608361	87.978686	50.048922
499.823606	84.490182	50.053927
495.936187	99.823321	50.058932
492.488920	84.060243	50.063937
489.516878	96.098876	50.068941
485.904169	94.646220	50.073946
482.256908	87.257383	50.078951
478.807942	91.483394	50.083956
475.536178	86.990726	50.088961
471.367517	102.437528	50.093965
468.007307	94.899328	50.098970
464.944303	86.226240	50.103975
461.459208	92.666240	50.108980
458.023115	84.975418	50.113985
454.280311	99.203902	50.118989
450.684302	88.624280	50.123994
447.130332	90.304082	50.128999
443.615912	97.188448	50.134004
440.045067	83.915673	50.139009
436.668965	88.408698	50.144013
433.107210	94.572811	50.149018
430.073695	88.780491	50.154023
426.414794	95.801390	50.159028
423.213377	96.223740	50.164033
419.709047	93.232354	50.169037
415.802831	90.500074	50.174042
411.849689	92.033603	50.179047
407.844023	102.804129	50.184052
405.306944	92.938194	50.189057
401.953737	89.122707	50.194061
398.411171	97.887623	50.199066
394.957775	87.519811	50.204071
391.018458	88.864520	50.209076
387.933912	89.838057	50.214081
383.938466	97.677323	50.219085
380.414826	89.636412	50.224090
377.108874	89.407593	50.229095
373.534550	91.751842	50.234100
370.381766	96.023248	50.239105
366.499640	106.113208	50.244109
363.072912	106.216528	50.249114
360.044205	83.111246	50.254119
356.318340	97.897095	50.259124
352.775267	93.231835	50.264129
349.320829	96.651984	50.269133
345.325021	97.780933	50.274138
341.898956	90.218306	50.279143
338.583494	97.223404	50.284148
335.367759	99.327998	50.289153
331.924704	97.981709	50.294157
328.286829	96.026855	50.299162
324.800748	89.561979	50.304167
321.005278	90.175498	50.309172
317.550017	83.920937	50.314177
313.792924	96.905169	50.319181
310.617873	98.073246	50.324186
307.367221	85.958946	50.329191
303.553867	97.056889	50.334196
300.327175	91.117708	50.339201
296.641755	95.099247	50.344205
292.757331	99.200547	50.349210
289.726234	90.364343	50.354215
286.207481	99.347030	50.359220
282.783808	86.294891	50.364225
278.706205	90.897861	50.369229
275.551696	93.106780	50.374234
272.316013	95.780837	50.379239
268.679016	94.085302	50.384244
265.655732	83.248377	50.389249
261.306372	88.453913	50.394253
257.601761	90.245971	50.399258
254.390889	81.225975	50.404263
250.698131	81.886709	50.409268
247.409709	82.107615	50.414273
244.356033	86.812790	50.419277
241.195681	85.305193	50.424282
237.443019	86.152488	50.429287
233.525070	87.383185	50.434292
230.111811	90.970934	50.439297
226.504820	93.475382	50.444301
223.265095	90.426808	50.449306
219.609091	72.387024	50.454311
215.587559	86.323874	50.459316
212.232487	83.767943	50.464321
208.795375	83.692614	50.469325
205.256176	87.812633	50.474330
201.985083	78.292727	50.479335
198.377994	99.628021	50.484340
195.232172	85.785747	50.489345
191.545968	89.745301	50.494349
187.896548	87.188035	50.499354
184.774721	84.671506	50.504359
181.098909	93.764251	50.509364
177.500039	88.285229	50.514369
173.501762	100.345502	50.519373
170.282435	94.727927	50.524378
167.000387	90.290779	50.529383
163.396522	93.611017	50.534388
159.913562	90.477188	50.539393
156.929852	90.087236	50.544397
153.213911	86.366645	50.549402
150.013621	78.942748	50.554407
145.633330	89.022236	50.559412
142.460184	82.878582	50.564417
138.704697	94.916646	50.569421
135.662391	89.739593	50.574426
132.204530	85.431246	50.579431
128.629582	92.458079	50.584436
125.205400	83.857539	50.589441
121.358609	87.519573	50.594445
117.513986	88.071277	50.599450
114.499352	83.740955	50.604455
110.672276	91.487506	50.609460
107.260938	85.919025	50.614465
104.116830	90.913661	50.619469
100.436855	84.387516	50.624474
97.436714	87.831494	50.629479
93.454892	88.297135	50.634484
89.983892	78.128388	50.639489
86.375995	85.957667	50.644493
82.555272	88.327976	50.649498
79.255833	81.577708	50.654503
75.795102	92.962167	50.659508
72.613032	84.890035	50.664513
69.141255	89.673425	50.669517
65.602108	84.656502	50.674522
61.987345	76.911600	50.679527
58.256630	78.109875	50.684532
54.612068	79.876789	50.689537
51.213750	81.114738	50.694541
48.033583	83.337246	50.699546
44.670042	77.827746	50.704551
40.630761	84.604652	50.709556
37.188283	84.014536	50.714561
33.841974	77.420330	50.719565
30.433031	82.212871	50.724570
27.123405	75.983082	50.729575
23.155057	87.121218	50.734580
20.219468	80.215891	50.739585
16.284168	78.250827	50.744589
12.964895	85.803955	50.749594
9.183449	78.097849	50.754599
5.699720	90.431899	50.759604
2.632040	78.077110	50.764609