Thu Aug 25 12:32:07 2022

Number of Points = 9926

Depth (nm)	Load (N)	Time (s)
1.500252	106.155718	0.000000
1.562536	97.844235	0.005005
1.574820	98.908530	0.010010
1.345569	103.364275	0.015014
2.000209	91.653835	0.020019
1.503690	85.619245	0.025024
0.999041	83.423588	0.030029
1.053143	67.694351	0.035034
0.551372	64.242229	0.040038
0.583265	52.869835	0.045043
0.203543	51.695488	0.050048
0.004532	46.234396	0.055053
-0.232872	28.222335	0.060058
-0.373129	28.652464	0.065062
-0.399889	12.470873	0.070067
-0.901879	10.322265	0.075072
-1.174617	0.851599	0.080077
-1.678901	-10.629735	0.085082
-1.888403	-11.172686	0.090086
-2.155964	-16.211730	0.095091
-2.932949	-18.301428	0.100096
-3.578809	-9.484054	0.105101
-3.528459	-14.069872	0.110106
-4.029953	-4.553780	0.115110
-3.998988	-22.427503	0.120115
-3.512785	-7.295477	0.125120
-3.930194	-6.562495	0.130125
-4.308801	-3.949993	0.135130
-4.750774	1.355305	0.140134
-5.146217	-19.555258	0.145139
-5.277058	-11.600028	0.150144
-5.964437	-11.634669	0.155149
-6.376031	-19.520671	0.160154
-6.590279	-12.061738	0.165158
-6.620989	-17.128401	0.170163
-6.714290	-14.839013	0.175168
-6.767467	-9.461758	0.180173
-6.860733	-19.238944	0.185178
-7.010471	-11.619276	0.190182
-7.294200	-21.369782	0.195187
-7.734393	-14.682206	0.200192
-7.948307	-17.742815	0.205197
-8.105361	-14.554423	0.210202
-8.930452	-19.142278	0.215206
-9.687542	-19.618413	0.220211
-9.249539	-22.512247	0.225216
-9.071263	-15.383736	0.230221
-9.421747	-14.155040	0.235226
-9.755263	-13.656666	0.240230
-9.525644	-14.097577	0.245235
-10.049571	-9.598853	0.250240
-11.008417	-16.367726	0.255245
-11.290485	-12.074578	0.260250
-11.323202	-2.843906	0.265254
-11.331779	-17.041478	0.270259
-11.067347	-13.419252	0.275264
-11.791864	-11.758627	0.280269
-12.049656	-17.026991	0.285274
-12.470263	-13.287940	0.290278
-12.570363	-19.245400	0.295283
-12.644845	-17.313303	0.300288
-12.816354	-16.270837	0.305293
-13.619086	-14.550501	0.310298
-13.775156	-9.464008	0.315302
-14.092381	-10.255836	0.320307
-13.913160	-8.240102	0.325312
-14.177251	-13.972552	0.330317
-14.330415	-16.840199	0.335322
-15.217786	-7.564205	0.340326
-14.840843	-10.040349	0.345331
-14.975320	-16.435349	0.350336
-15.821977	-19.175354	0.355341
-16.227839	-17.488727	0.360346
-16.592009	-9.212200	0.365350
-16.503802	-14.541105	0.370355
-16.547428	-12.623333	0.375360
-17.011284	-15.980138	0.380365
-16.851085	-13.626066	0.385370
-16.840595	-7.904446	0.390374
-17.834187	-19.018039	0.395379
-18.166716	-21.319743	0.400384
-18.358367	-16.613655	0.405389
-17.934764	-17.739858	0.410394
-18.181924	-12.765644	0.415398
-18.824718	-18.549487	0.420403
-19.511772	-6.713763	0.425408
-19.812019	-14.022426	0.430413
-19.820119	-13.749046	0.435418
-19.897968	-10.218723	0.440422
-19.984740	-22.689281	0.445427
-19.900762	-19.133696	0.450432
-20.424175	-13.679599	0.455437
-20.564692	-17.624905	0.460442
-20.688734	-11.464591	0.465446
-21.296035	-10.027975	0.470451
-22.155277	-14.319413	0.475456
-22.470426	-12.593215	0.480461
-22.359146	-13.306650	0.485466
-22.930735	-17.734906	0.490470
-22.569602	-26.108975	0.495475
-22.413433	-17.205300	0.500480
-22.714462	-12.659244	0.505485
-23.119470	-18.005780	0.510490
-23.868960	-9.365159	0.515494
-24.137707	-21.180781	0.520499
-24.266865	-6.926776	0.525504
-24.251269	-10.130914	0.530509
-24.198066	-14.220469	0.535514
-25.039643	-5.831173	0.540518
-25.457511	-18.009410	0.545523
-25.485512	-8.994616	0.550528
-25.655518	-12.005158	0.555533
-25.505081	-26.129559	0.560538
-25.975190	-9.224692	0.565542
-26.334793	-19.684646	0.570547
-26.608415	-13.817271	0.575552
-26.947881	-10.356688	0.580557
-27.055427	-19.827914	0.585562
-27.387184	-11.433080	0.590566
-27.733097	-16.067540	0.595571
-28.147228	-17.926187	0.600576
-28.342434	-21.942016	0.605581
-28.115339	-11.382153	0.610586
-28.474005	-12.569284	0.615590
-28.847700	-10.903515	0.620595
-29.538057	-20.235966	0.625600
-29.844114	-9.254043	0.630605
-29.815284	-23.720060	0.635610
-30.120817	-16.781501	0.640614
-29.962439	-18.305909	0.645619
-30.074179	-16.602091	0.650624
-30.293369	-10.344611	0.655629
-30.722512	-15.801261	0.660634
-31.220446	-11.550220	0.665638
-31.340295	-19.760343	0.670643
-31.437054	-14.385752	0.675648
-32.125130	-10.484569	0.680653
-32.467414	-26.426857	0.685658
-33.012606	-19.115389	0.690662
-33.294786	-23.532042	0.695667
-32.912263	-21.389978	0.700672
-33.293321	-13.974512	0.705677
-32.779956	-26.542262	0.710682
-33.008699	-27.733930	0.715686
-33.526995	-26.659274	0.720691
-34.259573	-19.631658	0.725696
-34.712162	-13.948213	0.730701
-34.254354	-18.654820	0.735706
-35.227075	-17.777880	0.740710
-36.013901	-22.833634	0.745715
-35.639399	-17.941010	0.750720
-35.740626	-13.480044	0.755725
-35.912322	-13.734688	0.760730
-36.142357	-13.834659	0.765734
-36.311723	-15.750640	0.770739
-36.260211	-17.533550	0.775744
-37.125990	-7.757901	0.780749
-37.277073	-22.891755	0.785754
-37.321856	-11.368640	0.790758
-37.619968	-15.393656	0.795763
-37.430150	-19.621674	0.800768
-38.134313	-13.702658	0.805773
-38.436911	-13.680527	0.810778
-38.979954	-15.344969	0.815782
-39.009689	-23.635648	0.820787
-38.848402	-19.854895	0.825792
-39.482560	-12.997721	0.830797
-39.845212	-13.238264	0.835802
-40.446603	-22.217656	0.840806
-40.424888	-16.671804	0.845811
-40.601951	-15.609485	0.850816
-40.779722	-9.488209	0.855821
-40.760249	-15.739651	0.860826
-40.980597	-11.212564	0.865830
-41.149211	-15.694469	0.870835
-41.586425	-17.166684	0.875840
-42.163201	-19.888861	0.880845
-41.943602	-19.214561	0.885850
-42.144836	-13.073791	0.890854
-42.482188	-14.855882	0.895859
-43.139010	-17.480096	0.900864
-43.331684	-15.390274	0.905869
-43.360600	-21.033019	0.910874
-43.772677	-4.444126	0.915878
-44.004139	-10.238635	0.920883
-44.332234	-13.607219	0.925888
-44.880329	-10.490434	0.930893
-44.739188	-5.836488	0.935898
-44.955181	-10.437521	0.940902
-44.969456	-13.662288	0.945907
-44.937062	-21.339442	0.950912
-45.970044	-11.423701	0.955917
-46.695513	-16.805445	0.960922
-46.410478	-2.439168	0.965926
-46.216909	-8.189544	0.970931
-46.137953	-13.248079	0.975936
-46.465012	-4.974201	0.980941
-47.015222	-10.892773	0.985946
-47.424583	-18.355178	0.990950
-47.447945	-13.257843	0.995955
-47.545808	-20.224890	1.000960
-48.645944	-6.410369	1.005965
-48.704020	-14.987676	1.010970
-49.330736	-8.384767	1.015974
-49.447879	-17.484328	1.020979
-49.082312	-14.263930	1.025984
-49.433310	-13.145883	1.030989
-49.665073	-23.464511	1.035994
-49.671684	-10.318045	1.040998
-50.128399	-17.728737	1.046003
-50.633317	-25.324863	1.051008
-51.236231	-10.841608	1.056013
-50.882799	-16.984025	1.061018
-51.344702	-16.582592	1.066022
-50.782791	-19.891312	1.071027
-51.174232	-18.412588	1.076032
-52.174108	-16.386112	1.081037
-51.980529	-20.453367	1.086042
-52.401253	-10.092557	1.091046
-52.575449	-14.314159	1.096051
-53.551305	-15.334979	1.101056
-53.847900	-14.418445	1.106061
-53.952865	-8.460437	1.111066
-54.121143	-9.949481	1.116070
-53.941823	-9.063225	1.121075
-54.171988	-11.643560	1.126080
-54.263630	-8.557166	1.131085
-54.111459	-13.984677	1.136090
-54.870807	-19.867311	1.141094
-55.242004	-17.740025	1.146099
-55.593237	-20.412120	1.151104
-55.749136	-13.031934	1.156109
-55.295958	-18.000407	1.161114
-55.967004	-8.366002	1.166118
-56.401752	-8.063736	1.171123
-56.587806	-5.481405	1.176128
-56.795669	-10.466525	1.181133
-56.763664	-5.801807	1.186138
-57.806886	-7.833965	1.191142
-58.274860	-7.893489	1.196147
-58.381648	-3.210187	1.201152
-58.372890	-10.092703	1.206157
-58.046321	-12.864675	1.211162
-58.393757	-9.200362	1.216166
-59.266854	-9.648825	1.221171
-59.856604	-8.803415	1.226176
-59.852999	-7.949738	1.231181
-59.574351	-12.118910	1.236186
-60.131093	-11.965208	1.241190
-59.887065	-13.718172	1.246195
-60.014088	-9.683435	1.251200
-60.864641	0.694110	1.256205
-60.895732	-7.659637	1.261210
-61.438364	-4.021685	1.266214
-61.458782	-14.019092	1.271219
-61.459398	-12.649062	1.276224
-62.206897	-13.474708	1.281229
-62.539679	-11.688798	1.286234
-63.007426	0.884523	1.291238
-63.295398	-10.918596	1.296243
-62.723688	-6.695950	1.301248
-62.992947	-5.597037	1.306253
-63.370437	-15.051275	1.311258
-63.183623	-12.036986	1.316262
-64.053207	-10.685822	1.321267
-64.455488	-12.957612	1.326272
-64.571839	-17.197768	1.331277
-64.571869	-17.213554	1.336282
-64.729262	-18.394255	1.341286
-65.503091	-17.077077	1.346291
-65.740166	-13.091536	1.351296
-66.115098	-8.375711	1.356301
-65.812917	-8.445179	1.361306
-66.103216	-1.452054	1.366310
-66.126780	-10.936440	1.371315
-66.533838	-8.145473	1.376320
-67.135509	0.095505	1.381325
-67.217388	-3.909610	1.386330
-67.319519	-1.248678	1.391334
-67.869476	-6.911024	1.396339
-68.279173	-3.116731	1.401344
-68.768275	-4.128398	1.406349
-68.486186	-7.709651	1.411354
-68.250269	-6.968305	1.416358
-68.524239	-11.209075	1.421363
-68.290099	-16.548188	1.426368
-69.631965	-3.037473	1.431373
-69.762597	-8.689592	1.436378
-69.839504	-2.935296	1.441382
-70.429419	-9.189330	1.446387
-70.990662	-18.817252	1.451392
-71.721559	-14.653094	1.456397
-71.257086	-0.954014	1.461402
-71.339466	-11.020807	1.466406
-71.558450	-12.365864	1.471411
-71.320081	-12.036190	1.476416
-72.045034	-7.977366	1.481421
-71.633945	-21.361160	1.486426
-72.791986	-10.318508	1.491430
-72.884413	-12.496481	1.496435
-73.160755	-18.404175	1.501440
-73.551984	-5.267045	1.506445
-73.178558	-6.505611	1.511450
-73.593486	-6.361474	1.516454
-73.821241	-6.218191	1.521459
-74.505659	-12.969944	1.526464
-75.018314	-3.249623	1.531469
-74.861508	-3.416535	1.536474
-74.969547	-7.563082	1.541478
-75.008292	-2.102667	1.546483
-75.363995	-10.968696	1.551488
-75.924710	-10.700475	1.556493
-76.200709	-10.220603	1.561498
-76.669463	-10.128143	1.566502
-76.529509	-14.712180	1.571507
-76.347491	-4.271805	1.576512
-77.042559	-8.550996	1.581517
-77.539002	-12.396237	1.586522
-77.816633	-8.217678	1.591526
-77.567837	-11.626035	1.596531
-77.679380	-15.613843	1.601536
-77.975523	-6.961997	1.606541
-78.412358	-12.237105	1.611546
-79.295801	-10.010570	1.616550
-79.188774	-7.635514	1.621555
-79.267356	-14.798570	1.626560
-79.264030	-5.893092	1.631565
-79.256106	-10.465933	1.636570
-80.072233	-9.237038	1.641574
-80.528408	-7.517215	1.646579
-80.748413	-10.437662	1.651584
-80.689071	-9.488315	1.656589
-80.727826	-11.930961	1.661594
-81.178309	-10.240504	1.666598
-81.882569	-6.162774	1.671603
-82.021074	-6.118898	1.676608
-82.124332	-2.900969	1.681613
-82.008746	-6.297944	1.686618
-82.054868	-5.569353	1.691622
-82.599823	-9.799298	1.696627
-83.283096	-12.995168	1.701632
-83.411845	-3.550138	1.706637
-83.447204	-16.209083	1.711642
-83.869525	-10.014688	1.716646
-83.899768	-8.064211	1.721651
-84.429781	-19.041621	1.726656
-84.845711	-10.633600	1.731661
-85.104229	-18.106982	1.736666
-85.266979	-8.539568	1.741670
-85.536553	-10.816333	1.746675
-85.579458	-17.804644	1.751680
-85.748096	-10.381333	1.756685
-85.487984	-18.454836	1.761690
-86.325345	-13.464074	1.766694
-86.622279	-13.053687	1.771699
-86.730212	-10.546872	1.776704
-86.870415	-5.814043	1.781709
-87.465623	-15.509409	1.786714
-87.823458	-8.714514	1.791718
-88.402566	-10.132855	1.796723
-88.456659	-13.373528	1.801728
-88.468000	-3.829837	1.806733
-88.258424	-14.695346	1.811738
-88.443725	-13.986076	1.816742
-88.810650	-13.204054	1.821747
-89.477108	-21.290556	1.826752
-90.069088	-11.516682	1.831757
-90.207952	-17.806585	1.836762
-89.887806	-19.191826	1.841766
-90.289072	-21.030339	1.846771
-90.232457	-15.489958	1.851776
-90.607552	-5.642498	1.856781
-91.262442	-10.086170	1.861786
-91.617772	-14.709658	1.866790
-91.838323	-17.155455	1.871795
-91.720690	-20.160443	1.876800
-91.840452	-16.901965	1.881805
-91.819639	-22.201322	1.886810
-92.270346	-22.579925	1.891814
-92.931002	-16.977773	1.896819
-92.705393	-23.517774	1.901824
-93.134739	-14.152199	1.906829
-93.764904	-22.630365	1.911834
-94.166651	-14.496651	1.916838
-94.531728	-15.891581	1.921843
-93.946630	-23.642681	1.926848
-94.518360	-16.652921	1.931853
-94.614674	-17.033271	1.936858
-95.171119	-21.337342	1.941862
-95.926914	-13.872650	1.946867
-96.177488	-20.287417	1.951872
-95.902638	-14.395254	1.956877
-95.800029	-18.407126	1.961882
-95.735939	-9.833875	1.966886
-96.296520	-17.209305	1.971891
-96.860906	-11.831044	1.976896
-97.460418	-6.004352	1.981901
-97.521726	-22.218450	1.986906
-97.392772	-14.041343	1.991910
-97.475411	-9.434595	1.996915
-97.842731	-9.167729	2.006912
-97.845712	-12.148112	2.016909
-97.750996	-17.345427	2.026906
-96.874397	-14.527168	2.036902
-96.408454	-14.128120	2.046899
-95.921546	-17.277131	2.056896
-94.962398	-13.591156	2.066893
-94.521465	-12.260022	2.076890
-95.157221	-12.106495	2.086886
-93.882733	-15.385250	2.096883
-93.490662	-17.097057	2.106880
-92.469136	-11.855960	2.116877
-91.997964	-13.744886	2.126874
-92.115858	-17.388341	2.136870
-91.757728	-14.675740	2.146867
-90.972004	-11.656339	2.156864
-90.361877	-17.004108	2.166861
-89.694594	-17.659809	2.176858
-89.533342	-9.480405	2.186854
-88.959105	-17.866811	2.196851
-88.340438	-10.262761	2.206848
-87.882843	-13.923532	2.216845
-86.904798	-13.858150	2.226842
-86.667101	-13.192088	2.236838
-86.635023	-13.174884	2.246835
-85.854759	-17.849227	2.256832
-85.246233	-16.100860	2.266829
-84.814227	-18.097690	2.276826
-83.829437	-14.982769	2.286822
-83.666313	-21.470596	2.296819
-83.842033	-14.537192	2.306816
-83.132122	-12.921920	2.316813
-82.055479	-15.742020	2.326810
-81.931486	-17.725432	2.336806
-81.001777	-12.270375	2.346803
-80.746997	-11.448598	2.356800
-80.517264	-12.634454	2.366797
-79.642373	-14.174825	2.376794
-79.392823	-9.535022	2.386790
-79.247798	-8.765740	2.396787
-78.183922	-10.880586	2.406784
-77.942906	-18.115550	2.416781
-76.790051	-11.836982	2.426778
-76.535806	-22.799357	2.436774
-76.427874	-11.953810	2.446771
-76.370259	-15.833841	2.456768
-75.429407	-15.027699	2.466765
-75.033759	-12.881678	2.476762
-74.181752	-14.922144	2.486758
-73.935282	-10.969273	2.496755
-72.751711	-15.253813	2.506752
-72.637201	-14.558945	2.516749
-72.307305	-13.200907	2.526746
-72.088762	-14.286807	2.536742
-71.163497	-15.287040	2.546739
-70.859366	-13.858442	2.556736
-70.443140	-19.612984	2.566733
-69.925818	-12.480895	2.576730
-69.603088	-12.005552	2.586726
-68.618975	-9.093262	2.596723
-68.153124	-11.801816	2.606720
-68.078015	-10.137760	2.616717
-67.082614	-13.274580	2.626714
-67.014925	-9.851229	2.636710
-66.155273	-6.523459	2.646707
-65.845460	-13.439754	2.656704
-65.303039	-7.803632	2.666701
-64.453143	-13.040083	2.676698
-64.141119	-6.145086	2.686694
-63.970593	-10.679540	2.696691
-63.483834	-13.581439	2.706688
-62.617269	-10.752098	2.716685
-62.468093	-12.470194	2.726682
-61.548246	-11.762129	2.736678
-61.297748	-9.184716	2.746675
-60.782627	-12.182925	2.756672
-59.684262	-11.018158	2.766669
-59.669297	-9.575927	2.776666
-59.665844	-11.058947	2.786662
-59.112011	-14.487707	2.796659
-58.175465	-14.764278	2.806656
-57.777437	-7.227021	2.816653
-56.963422	-15.692181	2.826650
-56.793619	-10.618563	2.836646
-56.640772	-11.092286	2.846643
-55.457095	-11.087632	2.856640
-55.050510	-9.500856	2.866637
-55.109737	-13.866262	2.876634
-54.236148	-8.282029	2.886630
-53.876504	-13.172399	2.896627
-52.922897	-15.779981	2.906624
-52.361888	-10.789836	2.916621
-52.475238	-14.136231	2.926618
-52.020598	-6.997483	2.936614
-50.944935	-17.800299	2.946611
-50.829370	-13.611505	2.956608
-50.338497	-7.517476	2.966605
-49.347066	-9.392885	2.976602
-49.448964	-8.195272	2.986598
-48.966230	-13.481898	2.996595
-47.932133	-10.602779	3.006592
-47.766181	-10.464000	3.016589
-47.520070	-16.448481	3.026586
-46.848648	-14.361507	3.036582
-46.312742	-9.741229	3.046579
-45.314612	-13.391659	3.056576
-45.246872	-17.989202	3.066573
-44.948359	-14.678045	3.076570
-43.865410	-16.168650	3.086566
-43.591098	-12.704814	3.096563
-43.813549	-13.392163	3.106560
-42.611221	-9.997708	3.116557
-42.094290	-15.229503	3.126554
-41.691641	-8.719338	3.136550
-40.978016	-11.859523	3.146547
-40.610674	-7.003756	3.156544
-40.559804	-14.959700	3.166541
-39.433524	-17.277555	3.176538
-39.293537	-16.881284	3.186534
-38.810822	-13.713030	3.196531
-37.684257	-12.289750	3.206528
-37.557979	-13.639960	3.216525
-37.437186	-19.677663	3.226522
-36.825282	-13.010219	3.236518
-36.187175	-16.281121	3.246515
-35.968030	-10.125508	3.256512
-34.950534	-14.868697	3.266509
-34.528671	-3.217021	3.276506
-34.636694	-8.015109	3.286502
-33.602942	-7.508621	3.296499
-33.181929	-9.807838	3.306496
-32.606518	-9.482958	3.316493
-32.107670	-10.882042	3.326490
-31.741121	-5.693529	3.336486
-31.298727	-13.641129	3.346483
-30.497235	-7.345510	3.356480
-30.028851	-8.286824	3.366477
-29.767001	-8.384817	3.376474
-28.860350	-8.210041	3.386470
-28.333283	-15.195222	3.396467
-28.195347	-12.825085	3.406464
-27.918716	-14.597997	3.416461
-27.231014	-17.908347	3.426458
-26.916585	-11.412869	3.436454
-25.943437	-9.081730	3.446451
-25.277359	-13.098282	3.456448
-25.384933	-9.368701	3.466445
-25.042605	-13.838208	3.476442
-23.969188	-18.346236	3.486438
-23.863781	-14.827424	3.496435
-23.068679	-10.919331	3.506432
-22.789201	-15.581729	3.516429
-22.395082	-7.156869	3.526426
-21.533794	-9.702467	3.536422
-21.352654	-17.802367	3.546419
-20.616520	-10.473306	3.556416
-20.055132	-16.988693	3.566413
-19.773744	-8.948482	3.576410
-18.965525	-13.006312	3.586406
-18.611264	-13.435565	3.596403
-18.312245	-8.477225	3.606400
-17.504241	-14.454713	3.616397
-17.163401	-16.991622	3.626394
-16.919435	-14.961215	3.636390
-16.069346	-7.501120	3.646387
-15.510033	-17.133305	3.656384
-15.268920	-13.683272	3.666381
-14.288413	-15.012104	3.676378
-14.116015	-15.051732	3.686374
-13.964983	-13.114468	3.696371
-12.790527	-13.016496	3.706368
-12.397702	-9.469857	3.716365
-12.417690	-23.056563	3.726362
-11.938043	-15.547931	3.736358
-11.129060	-16.992438	3.746355
-10.639802	-18.833510	3.756352
-9.596210	-18.658014	3.766349
-9.526312	-18.966684	3.776346
-9.604147	-15.530034	3.786342
-8.697490	-13.460907	3.796339
-8.182956	-12.429570	3.806336
-7.732326	-15.290960	3.816333
-6.735498	-15.722690	3.826330
-6.667671	-9.099872	3.836326
-6.440381	-12.087827	3.846323
-5.546538	-11.388353	3.856320
-5.029990	-9.004677	3.866317
-4.801077	-8.584324	3.876314
-4.190687	0.031570	3.886310
-4.092215	7.574593	3.896307
-3.433052	8.957072	3.906304
-2.962471	21.557816	3.916301
-2.175436	26.116586	3.926298
-1.969224	38.052340	3.936294
-1.766753	55.326465	3.946291
-1.347657	65.366204	3.956288
-0.649246	80.082243	3.966285
-0.105566	100.302880	3.976282
0.000000	117.043089	3.981286
0.526102	129.093786	3.986291
0.562765	136.459684	3.991296
0.408650	141.254845	3.996301
0.585187	146.311415	4.001306
0.563974	158.881326	4.006310
0.924013	160.495422	4.011315
1.448906	169.186394	4.016320
1.112986	167.169936	4.021325
1.260783	164.365837	4.026330
1.169515	169.435899	4.031334
1.057868	167.061595	4.036339
1.088881	172.874973	4.041344
1.191930	170.656857	4.046349
1.187047	174.134655	4.051354
1.109422	173.343242	4.056358
1.553698	164.165110	4.061363
1.104763	170.512435	4.066368
1.060971	171.898737	4.071373
0.905098	171.853584	4.076378
0.962393	181.873851	4.081382
1.087471	191.728478	4.086387
1.190211	199.125177	4.091392
1.569228	195.563499	4.096397
1.790288	210.553755	4.101402
1.377719	202.443176	4.106406
1.599459	200.219115	4.111411
1.402507	200.490450	4.116416
1.519408	183.422478	4.121421
1.446838	189.660220	4.126426
1.569910	185.746336	4.131430
1.404610	179.273835	4.136435
1.313531	195.964484	4.141440
1.464635	200.041114	4.146445
1.719009	196.821672	4.151450
1.524490	198.225264	4.156454
1.529451	189.299453	4.161459
1.130733	190.551539	4.166464
1.484270	200.886073	4.171469
1.577057	201.409408	4.176474
1.473361	205.200091	4.181478
2.000034	195.765420	4.186483
1.753287	203.716760	4.191488
1.846646	209.738683	4.196493
1.691341	205.985471	4.201498
1.314291	200.748382	4.206502
1.765963	205.701748	4.211507
1.801650	209.663585	4.216512
1.679335	201.846055	4.221517
1.680992	202.098926	4.226522
1.736641	210.056673	4.231526
2.057472	199.894941	4.236531
1.747182	184.539075	4.241536
1.523135	181.584423	4.246541
1.676096	197.373122	4.251546
1.734234	203.137966	4.256550
1.905388	198.609097	4.261555
1.798611	206.848559	4.266560
2.000503	218.184477	4.271565
1.797530	199.432847	4.276570
1.720158	207.990409	4.281574
2.063407	203.981911	4.286579
1.691134	207.400218	4.291584
1.793834	207.380991	4.296589
2.309052	204.788239	4.301594
1.555730	205.899731	4.306598
1.575704	200.796591	4.311603
1.772312	207.704017	4.316608
1.935618	206.874854	4.321613
1.634793	201.081648	4.326618
1.550412	216.372870	4.331622
1.627950	218.259028	4.336627
1.670889	217.787249	4.341632
1.892260	203.018791	4.346637
2.048308	206.420759	4.351642
1.451760	213.844772	4.356646
1.715253	214.667232	4.361651
2.180985	218.710389	4.366656
2.216852	229.597757	4.371661
2.425902	239.258917	4.376666
2.229678	230.788556	4.381670
2.064959	216.083743	4.386675
1.852309	225.684417	4.391680
1.835990	231.252125	4.396685
2.434462	231.617134	4.401690
2.066729	237.521483	4.406694
2.331299	239.191674	4.411699
2.417456	237.979122	4.416704
1.543083	231.817020	4.421709
1.922585	236.500124	4.426714
2.210267	244.649325	4.431718
2.383477	234.080425	4.436723
1.841482	245.941045	4.441728
2.055018	243.202564	4.446733
2.076775	240.532097	4.451738
2.034267	245.990017	4.456742
2.055913	244.828701	4.461747
2.463821	243.904263	4.466752
2.196132	248.748886	4.471757
2.468332	246.513749	4.476762
1.882829	242.128733	4.481766
1.919307	241.509268	4.486771
2.283852	249.326883	4.491776
2.128247	261.598380	4.496781
2.467362	263.288531	4.501786
2.584558	271.556206	4.506790
2.544711	269.120018	4.511795
2.414628	272.123898	4.516800
2.717458	265.188870	4.521805
2.684712	251.763674	4.526810
2.255149	247.857270	4.531814
2.058372	257.847784	4.536819
2.140350	255.139406	4.541824
2.543820	260.090848	4.546829
2.608992	262.716115	4.551834
2.369608	267.508851	4.556838
2.347976	268.277909	4.561843
2.136290	270.595373	4.566848
2.161225	266.282388	4.571853
2.558864	269.399739	4.576858
2.206625	267.882544	4.581862
2.543608	258.841399	4.586867
2.501345	265.308541	4.591872
2.127465	265.512684	4.596877
2.641078	273.844801	4.601882
2.583634	293.535889	4.606886
2.948534	289.720136	4.611891
2.777232	290.534792	4.616896
2.629789	300.406868	4.621901
3.249536	286.506083	4.626906
2.602485	284.165031	4.631910
2.987849	272.199266	4.636915
3.043158	272.696837	4.641920
2.716613	268.638243	4.646925
2.968704	266.988395	4.651930
2.854861	270.075152	4.656934
2.760157	267.448240	4.661939
2.592850	276.342634	4.666944
2.410013	271.306052	4.671949
2.675444	264.614170	4.676954
2.432772	269.556120	4.681958
2.652972	281.341634	4.686963
2.872039	289.394036	4.691968
2.896443	284.644525	4.696973
3.029345	294.491655	4.701978
2.900502	298.441324	4.706982
3.022094	288.491097	4.711987
3.130456	290.002266	4.716992
3.136893	294.835589	4.721997
3.116065	282.427251	4.727002
2.464928	279.045947	4.732006
2.733130	274.096885	4.737011
2.656216	283.236552	4.742016
2.738149	295.186110	4.747021
2.742077	295.397498	4.752026
2.892692	297.240576	4.757030
3.150025	288.749744	4.762035
2.892867	291.169250	4.767040
2.534014	298.809160	4.772045
2.950961	296.519699	4.777050
3.059154	290.871191	4.782054
3.000119	294.461903	4.787059
2.753729	296.557013	4.792064
2.893961	311.882727	4.797069
3.555154	307.644052	4.802074
2.966470	318.610348	4.807078
3.420052	316.536612	4.812083
3.539666	320.396737	4.817088
3.021743	304.032405	4.822093
2.962106	297.685676	4.827098
3.022427	298.872174	4.832102
3.455304	315.499823	4.837107
3.273147	317.670295	4.842112
3.232757	326.820081	4.847117
3.343143	317.855540	4.852122
3.479644	327.575572	4.857126
3.465670	308.101339	4.862131
3.116194	305.982583	4.867136
3.115068	300.446114	4.872141
3.505031	313.350351	4.877146
3.371745	319.543866	4.882150
3.462979	318.248253	4.887155
3.230193	301.703203	4.892160
3.453645	310.843280	4.897165
3.216554	309.121375	4.902170
3.330602	321.113376	4.907174
3.521338	313.844708	4.912179
3.358798	323.057924	4.917184
3.032287	319.571964	4.922189
3.366988	315.526814	4.927194
3.495411	326.406068	4.932198
3.190164	325.596528	4.937203
3.333636	326.516893	4.942208
3.333283	322.862768	4.947213
3.653349	317.449978	4.952218
3.440992	321.105848	4.957222
3.687182	319.691042	4.962227
3.607904	316.204311	4.967232
3.745620	318.353138	4.972237
3.773744	314.947658	4.977242
3.502139	325.051176	4.982246
4.164186	319.964462	4.987251
3.549185	318.219508	4.992256
3.424883	326.370021	4.997261
3.427282	326.208317	5.002266
3.411956	322.721056	5.007270
3.665763	322.355444	5.012275
3.154463	324.235795	5.017280
3.116191	316.294313	5.022285
3.057475	319.461028	5.027290
3.374268	337.733088	5.032294
3.631078	342.929000	5.037299
3.798695	350.834464	5.042304
3.697769	351.653916	5.047309
3.645637	348.934898	5.052314
4.167518	355.952772	5.057318
3.975745	354.644550	5.062323
4.109848	355.237348	5.067328
3.905606	353.159107	5.072333
3.841636	351.406909	5.077338
3.893231	347.978762	5.082342
3.890358	348.507598	5.087347
4.172990	351.551232	5.092352
3.803580	334.451742	5.097357
3.882148	336.208035	5.102362
3.791732	334.216368	5.107366
3.841290	335.717772	5.112371
4.032668	344.521199	5.117376
4.032947	351.813791	5.122381
3.614880	345.690888	5.127386
3.834135	358.296030	5.132390
3.824221	352.555273	5.137395
3.952835	348.055178	5.142400
3.923339	360.696133	5.147405
3.894030	346.612254	5.152410
3.758913	363.964871	5.157414
3.818543	357.536158	5.162419
3.713368	361.925068	5.167424
3.696002	347.304630	5.172429
3.765033	344.996908	5.177434
3.890044	354.987680	5.182438
4.040820	361.655569	5.187443
4.228592	366.957220	5.192448
3.954162	375.852629	5.197453
4.044797	376.398453	5.202458
4.105592	389.705504	5.207462
3.980319	378.373347	5.212467
4.254196	375.574770	5.217472
4.382602	385.631467	5.222477
4.782839	372.207946	5.227482
4.328369	367.973215	5.232486
4.284775	362.104851	5.237491
4.454749	354.371174	5.242496
4.244044	352.578690	5.247501
4.290851	351.011620	5.252506
4.247378	364.183126	5.257510
3.913535	358.005893	5.262515
4.585015	358.264551	5.267520
4.168218	352.812177	5.272525
4.483151	351.029086	5.277530
4.163820	357.602948	5.282534
4.282193	354.303545	5.287539
4.368139	350.515667	5.292544
4.339194	359.698479	5.297549
4.522013	371.907534	5.302554
4.223901	369.464340	5.307558
4.201600	372.214062	5.312563
4.678753	378.707431	5.317568
4.246627	378.632793	5.322573
4.658085	381.757490	5.327578
4.378086	384.436857	5.332582
4.407703	383.831117	5.337587
4.462079	388.122267	5.342592
4.158229	376.160014	5.347597
4.455151	378.046618	5.352602
4.520168	378.840070	5.357606
4.754840	379.682873	5.362611
4.627975	377.317253	5.367616
4.541712	378.159719	5.372621
4.617335	374.452549	5.377626
4.710678	375.580092	5.382630
4.573339	385.165887	5.387635
4.616570	383.254517	5.392640
4.358807	381.953469	5.397645
4.608109	380.101563	5.402650
4.644768	379.978785	5.407654
4.679055	375.601032	5.412659
4.535996	381.416441	5.417664
4.715481	381.869248	5.422669
4.750817	375.608855	5.427674
4.655288	387.269897	5.432678
4.507375	389.938061	5.437683
4.779296	376.268879	5.442688
4.630859	384.913592	5.447693
4.893657	374.495093	5.452698
4.545401	381.070332	5.457702
4.440134	382.643456	5.462707
4.511030	372.106325	5.467712
4.520944	382.624522	5.472717
4.424977	381.880267	5.477722
4.614244	402.618014	5.482726
4.948741	406.055337	5.487731
5.186030	413.234887	5.492736
5.184781	413.728668	5.497741
5.135774	400.046475	5.502746
4.452656	391.199898	5.507750
4.792214	398.227373	5.512755
4.696759	403.956234	5.517760
4.806231	409.248019	5.522765
5.262663	405.553945	5.527770
5.036569	409.471419	5.532774
5.092401	403.995598	5.537779
5.094322	402.650696	5.542784
4.933145	409.563638	5.547789
5.239375	403.548699	5.552794
4.958441	407.025501	5.557798
5.077344	403.526685	5.562803
5.415695	403.328162	5.567808
5.081878	397.948196	5.572813
4.822324	385.232333	5.577818
4.540783	389.066740	5.582822
4.563767	398.725500	5.587827
5.018936	400.555673	5.592832
5.082104	407.404990	5.597837
5.254760	403.090974	5.602842
5.289184	407.654180	5.607846
5.217192	408.019837	5.612851
5.379132	400.714516	5.617856
5.056478	411.145628	5.622861
4.979228	402.533155	5.627866
5.035640	420.963159	5.632870
5.431396	398.722716	5.637875
4.985172	401.988128	5.642880
4.906880	407.670008	5.647885
5.260517	407.320391	5.652890
5.102101	409.354272	5.657894
5.149931	400.601977	5.662899
4.957049	398.512459	5.667904
5.292237	411.494954	5.672909
5.630283	417.905726	5.677914
5.463851	412.189474	5.682918
5.342327	406.213081	5.687923
5.461659	401.426518	5.692928
5.138697	409.260173	5.697933
5.309060	406.961876	5.702938
5.786160	425.351282	5.707942
5.402725	408.658889	5.712947
5.345498	402.631293	5.717952
5.296505	406.062262	5.722957
5.315202	407.584327	5.727962
5.184497	428.324780	5.732966
5.323230	429.726796	5.737971
5.471561	420.933433	5.742976
5.579861	427.712409	5.747981
5.647056	426.721119	5.752986
5.299654	432.014890	5.757990
5.632495	432.554405	5.762995
5.737403	427.694163	5.768000
4.808981	430.832646	5.773005
5.314355	420.951930	5.778010
5.306946	426.695479	5.783014
5.328184	425.065968	5.788019
5.621919	425.187655	5.793024
5.217472	426.310937	5.798029
5.692337	434.386603	5.803034
5.339643	444.907865	5.808038
5.837553	455.957102	5.813043
5.622181	462.422963	5.818048
5.513314	462.196432	5.823053
6.102679	464.514965	5.828058
5.780349	468.725948	5.833062
5.704353	456.531783	5.838067
5.554143	452.651167	5.843072
5.636977	470.086800	5.848077
5.962040	461.759286	5.853082
5.509792	459.928704	5.858086
5.563372	462.172991	5.863091
5.962369	456.374460	5.868096
5.552748	469.128836	5.873101
5.643457	462.673069	5.878106
5.701448	464.663558	5.883110
5.635355	463.300834	5.888115
5.515487	464.294106	5.893120
5.625215	461.578185	5.898125
5.800429	459.861268	5.903130
5.535971	464.449172	5.908134
5.658832	468.030402	5.913139
6.016975	477.098839	5.918144
6.118302	485.185596	5.923149
6.100593	487.963091	5.928154
6.020534	482.609781	5.933158
6.276987	474.815045	5.938163
6.110524	465.090191	5.943168
5.792861	464.250951	5.948173
5.591121	470.448916	5.953178
5.808470	480.444274	5.958182
5.739011	485.384455	5.963187
5.858715	485.425840	5.968192
6.111068	487.759213	5.973197
6.445027	485.422619	5.978202
6.129512	477.072074	5.983206
5.896836	473.799178	5.988211
6.119407	477.206594	5.993216
6.261089	480.212222	5.998221
6.433863	483.592640	6.003226
6.314565	479.374971	6.008230
6.003529	489.275947	6.013235
6.274436	485.566631	6.018240
6.051185	485.294745	6.023245
6.496517	483.883527	6.028250
6.139075	472.404183	6.033254
6.135719	468.114566	6.038259
5.791485	465.571014	6.043264
5.864020	467.182728	6.048269
5.967906	479.793378	6.053274
6.439971	481.902494	6.058278
6.041225	468.619905	6.063283
5.806232	460.339012	6.068288
5.852211	477.356472	6.073293
6.029276	479.008758	6.078298
6.195544	483.617767	6.083302
6.030026	482.286439	6.088307
6.251232	483.925482	6.093312
5.705488	485.051923	6.098317
6.368323	477.120745	6.103322
6.300597	490.378403	6.108326
5.879767	486.556001	6.113331
6.094950	480.960273	6.118336
6.205377	483.917013	6.123341
6.231964	491.727575	6.128346
5.965258	488.811194	6.133350
6.171228	491.999745	6.138355
6.312474	488.807469	6.143360
5.826895	491.721548	6.148365
6.131291	488.307550	6.153370
5.981886	483.458664	6.158374
5.742543	485.805800	6.163379
6.169417	488.314314	6.168384
5.952366	496.210509	6.173389
6.401578	484.465560	6.178394
6.145602	492.440620	6.183398
6.124467	491.358760	6.188403
6.228035	491.535555	6.193408
5.977296	485.607856	6.198413
6.022006	481.810592	6.203418
5.921955	486.233532	6.208422
6.472705	490.798120	6.213427
6.203761	487.002542	6.218432
6.163381	494.630602	6.223437
6.155128	487.279144	6.228442
5.965766	480.718551	6.233446
6.043868	484.692787	6.238451
6.064877	484.806585	6.243456
6.017557	489.816067	6.248461
6.300479	487.357751	6.253466
6.443879	481.785926	6.258470
6.114129	470.197838	6.263475
5.907403	470.726979	6.268480
6.176043	470.909549	6.273485
6.308785	459.230021	6.278490
6.290860	461.368450	6.283494
5.881402	470.367322	6.288499
6.179370	458.383489	6.293504
6.140177	462.781069	6.298509
6.317386	462.218642	6.303514
5.997276	471.200351	6.308518
6.180109	467.103031	6.313523
6.388220	459.154520	6.318528
6.098026	462.936512	6.323533
6.226234	461.609785	6.328538
6.014056	463.829272	6.333542
6.252955	470.790287	6.338547
6.257117	461.320284	6.343552
6.101153	465.090736	6.348557
6.417611	465.189881	6.353562
6.327697	466.048743	6.358566
5.953435	462.073512	6.363571
6.479898	462.937041	6.368576
5.954101	464.231203	6.373581
6.008652	464.747882	6.378586
5.793722	461.760116	6.383590
6.013588	469.293605	6.388595
5.807708	466.845438	6.393600
5.601436	472.038012	6.398605
5.815526	470.340314	6.403610
5.772865	464.104765	6.408614
6.136389	456.625464	6.413619
5.974415	461.703524	6.418624
5.850008	468.132987	6.423629
5.960371	475.930416	6.428634
6.048076	480.409360	6.433638
6.095149	486.454448	6.438643
6.094760	485.872389	6.443648
5.812672	489.295602	6.448653
5.994460	488.574265	6.453658
6.064950	491.704947	6.458662
5.973408	492.178076	6.463667
6.047611	475.885330	6.468672
5.994402	486.888055	6.473677
6.043143	483.169255	6.478682
6.212164	486.556589	6.483686
6.390789	483.377439	6.488691
6.221075	485.511179	6.493696
6.065266	490.898338	6.498701
6.328937	477.024722	6.503706
6.413467	484.854677	6.508710
6.099096	479.572882	6.513715
5.984832	464.644818	6.518720
5.799445	482.698308	6.523725
6.453149	479.318169	6.528730
6.132081	474.790420	6.533734
6.075819	467.905249	6.538739
5.984496	464.939246	6.543744
5.852472	470.749791	6.548749
6.333428	476.287120	6.553754
6.233004	482.526164	6.558758
5.794945	469.885667	6.563763
6.059462	472.100069	6.568768
6.272614	490.062649	6.573773
6.328370	486.668625	6.578778
6.263350	481.230699	6.583782
6.199262	479.927772	6.588787
6.022731	471.700991	6.593792
5.704975	474.047755	6.598797
6.256555	475.666672	6.603802
6.112285	475.974050	6.608806
5.913775	468.639754	6.613811
6.440367	466.674788	6.618816
6.010128	470.744487	6.623821
5.882625	464.512740	6.628826
5.955270	464.618447	6.633830
6.438788	469.747237	6.638835
6.353004	473.057430	6.643840
6.162676	472.498804	6.648845
6.190718	466.900764	6.653850
5.907273	458.899553	6.658854
5.692628	468.624059	6.663859
5.878257	471.575342	6.668864
5.846217	481.590792	6.673869
6.000269	485.992901	6.678874
5.650141	492.881695	6.683878
6.107727	486.884144	6.688883
6.348289	480.876304	6.693888
6.087546	497.315400	6.698893
6.348113	484.078198	6.703898
6.139945	494.345884	6.708902
6.080216	497.822847	6.713907
6.397300	487.459053	6.718912
6.302216	489.229913	6.723917
6.335989	478.597293	6.728922
6.366661	473.524037	6.733926
5.943150	472.280590	6.738931
6.056760	466.726092	6.743936
6.044449	469.205338	6.748941
5.700047	461.428818	6.753946
5.807702	472.928364	6.758950
6.077535	482.507364	6.763955
6.120468	485.262701	6.768960
6.114273	488.579410	6.773965
5.871727	493.261967	6.778970
6.296258	493.600450	6.783974
6.129022	493.348262	6.788979
6.560775	482.672267	6.793984
6.047728	480.534824	6.798989
5.768547	468.505368	6.803994
6.012806	475.028935	6.808998
6.378532	483.928504	6.814003
6.382724	473.540974	6.819008
5.850594	474.861439	6.824013
6.034894	470.184905	6.829018
6.231643	472.748457	6.834022
6.255417	472.260691	6.839027
5.968148	465.051038	6.844032
5.894119	473.345605	6.849037
6.532553	469.869781	6.854042
6.267707	473.945205	6.859046
5.893862	472.349117	6.864051
6.108819	458.635013	6.869056
6.302362	471.253755	6.874061
6.362131	471.829729	6.879066
5.915559	471.931365	6.884070
5.905420	472.208236	6.889075
6.201707	465.302630	6.894080
6.075066	474.269847	6.899085
6.143188	469.282476	6.904090
6.160934	467.995203	6.909094
6.041428	468.906159	6.914099
6.271657	466.639605	6.919104
6.123955	465.242210	6.924109
6.417380	464.487563	6.929114
6.189395	466.399470	6.934118
6.013651	466.452344	6.939123
6.311654	460.397545	6.944128
5.939831	466.327920	6.949133
6.376627	464.633295	6.954138
6.430144	474.287313	6.959142
6.016833	475.136732	6.964147
6.056729	461.257060	6.969152
6.032086	466.332587	6.974157
6.183538	470.364931	6.979162
6.334095	469.759222	6.984166
6.348209	471.237717	6.989171
6.349135	463.524152	6.994176
6.148055	470.544613	6.999181
5.968216	455.433836	7.004186
6.190096	459.154578	7.009190
5.766818	459.372790	7.014195
5.961976	450.119646	7.019200
6.026006	464.884777	7.024205
6.045858	455.099098	7.029210
5.863303	473.917785	7.034214
5.893410	466.332528	7.039219
5.904188	466.552336	7.044224
6.204064	468.321424	7.049229
6.066196	468.036160	7.054234
6.201855	468.948266	7.059238
5.931860	474.751955	7.064243
6.037308	467.740204	7.069248
6.072824	474.619190	7.074253
6.286780	475.332361	7.079258
5.795020	463.187515	7.084262
5.495153	461.893057	7.089267
6.037732	460.732367	7.094272
6.471097	465.685511	7.099277
6.232187	464.808621	7.104282
6.329263	464.043608	7.109286
6.141814	464.582384	7.114291
6.295133	461.451497	7.119296
5.889608	466.656306	7.124301
6.042679	462.307378	7.129306
6.215199	465.982070	7.134310
6.126660	461.734275	7.139315
6.462608	462.061327	7.144320
6.166163	470.204074	7.149325
6.206926	462.731048	7.154330
6.248431	467.913273	7.159334
5.880760	472.393960	7.164339
6.204730	463.253508	7.169344
6.023694	470.248682	7.174349
5.917834	476.861909	7.179354
6.334226	466.270590	7.184358
6.130347	467.533296	7.189363
6.149132	473.807445	7.194368
6.047097	466.986395	7.199373
6.188914	468.435390	7.204378
6.080879	470.401272	7.209382
5.825887	465.268370	7.214387
6.258859	463.292762	7.219392
5.947542	473.756937	7.224397
6.199252	466.450179	7.229402
6.315296	471.456207	7.234406
5.956287	476.394295	7.239411
6.218003	481.640100	7.244416
6.235714	467.567741	7.249421
6.239388	474.284031	7.254426
6.379684	467.421849	7.259430
5.836766	455.395758	7.264435
6.199229	443.183524	7.269440
5.881279	455.559686	7.274445
6.135957	452.172468	7.279450
6.029026	457.713314	7.284454
6.097372	467.703536	7.289459
6.223371	474.650604	7.294464
6.190814	461.918103	7.299469
5.975377	450.517767	7.304474
6.256112	452.220248	7.309478
6.110888	449.506309	7.314483
6.342188	443.813153	7.319488
5.889086	443.691179	7.324493
5.779017	432.157283	7.329498
5.835665	441.333054	7.334502
5.688401	467.337608	7.339507
6.073691	463.461675	7.344512
5.815921	462.812373	7.349517
6.129360	462.949957	7.354522
6.325598	461.179125	7.359526
6.081407	469.794589	7.364531
6.116152	472.858100	7.369536
6.179535	477.347182	7.374541
6.119985	469.753825	7.379546
5.983909	473.169977	7.384550
6.062325	469.231389	7.389555
6.383329	470.737732	7.394560
6.067859	470.654306	7.399565
6.044848	470.537713	7.404570
6.199714	467.314832	7.409574
5.756339	464.021164	7.414579
6.236489	464.312967	7.419584
6.083936	470.259609	7.424589
6.041692	471.117329	7.429594
6.004496	470.449287	7.434598
5.742968	474.960801	7.439603
6.192861	459.067964	7.444608
5.902296	467.019958	7.449613
6.148749	465.728489	7.454618
6.040459	461.562886	7.459622
6.160445	466.824565	7.464627
6.308931	467.361328	7.469632
6.319787	477.496608	7.474637
6.147295	466.118008	7.479642
6.204826	466.457044	7.484646
6.192392	471.325010	7.489651
5.475204	464.625656	7.494656
5.458871	468.291971	7.499661
5.930745	472.068462	7.504666
6.381389	464.316072	7.509670
6.004854	471.955662	7.514675
6.282551	466.878506	7.519680
6.599935	470.267902	7.524685
6.582781	471.722822	7.529690
6.295119	474.295832	7.534694
6.115577	471.875176	7.539699
5.980132	463.316085	7.544704
6.303064	471.463030	7.549709
6.228779	474.486676	7.554714
6.281925	471.599279	7.559718
5.979981	462.031699	7.564723
6.007733	455.085912	7.569728
5.951643	477.421962	7.574733
6.288678	465.289630	7.579738
6.022157	452.577974	7.584742
5.846388	462.536837	7.589747
6.497330	459.751937	7.594752
6.142157	462.588630	7.599757
6.052177	454.152137	7.604762
6.264339	452.669884	7.609766
5.887543	450.549064	7.614771
6.171257	436.438215	7.619776
5.899223	454.891241	7.624781
6.400432	465.342001	7.629786
6.173248	448.726332	7.634790
5.932288	449.165921	7.639795
5.993711	434.865270	7.644800
6.091451	451.839794	7.649805
6.234748	456.971265	7.654810
6.149042	444.272415	7.659814
5.903478	453.062096	7.664819
6.087257	443.431078	7.669824
6.068902	446.214995	7.674829
6.006513	453.511120	7.679834
5.929697	446.600703	7.684838
6.229005	464.502300	7.689843
6.352255	476.733416	7.694848
6.251311	459.803720	7.699853
5.800545	452.224209	7.704858
6.222425	456.793161	7.709862
5.867782	451.928983	7.714867
6.065076	454.046346	7.719872
6.166374	461.332646	7.724877
6.365164	458.530002	7.729882
6.304419	443.685322	7.734886
5.896527	439.054123	7.739891
6.102536	441.736446	7.744896
5.988324	441.058324	7.749901
5.872603	436.757845	7.754906
6.141806	454.025054	7.759910
6.026352	468.685428	7.764915
6.081950	463.677874	7.769920
6.052059	469.181342	7.774925
5.990673	465.046355	7.779930
5.984575	468.382028	7.784934
6.233402	470.054707	7.789939
6.107802	470.514188	7.794944
6.098171	476.204315	7.799949
6.168795	465.141975	7.804954
6.303918	478.478576	7.809958
6.242769	462.513942	7.814963
6.203198	451.598593	7.819968
6.038296	446.464236	7.824973
5.872203	443.497297	7.829978
6.035788	450.258128	7.834982
6.038183	458.461617	7.839987
6.283888	455.237160	7.844992
6.095519	453.545573	7.849997
5.598812	451.937099	7.855002
5.955583	465.033312	7.860006
5.813231	469.646379	7.865011
6.119485	468.086106	7.870016
6.050767	472.830009	7.875021
5.845797	466.632546	7.880026
6.437216	467.631434	7.885030
6.086949	471.369055	7.890035
6.547433	466.218966	7.895040
6.523729	474.344292	7.900045
6.311955	461.187442	7.905050
5.997091	446.180090	7.910054
5.834304	435.103717	7.915059
5.887005	442.745646	7.920064
6.252415	450.563215	7.925069
6.074693	451.571878	7.930074
6.281794	452.070982	7.935078
6.064559	438.054441	7.940083
6.058178	446.455458	7.945088
5.602246	451.351776	7.950093
5.907748	465.433649	7.955098
6.541307	468.064806	7.960102
6.037598	467.817880	7.965107
6.636501	463.490850	7.970112
6.074869	449.686452	7.975117
5.994169	439.400830	7.980122
6.130998	442.980084	7.985139
6.505139	444.915936	7.990157
6.335953	435.102792	7.995174
5.857999	445.112059	8.000192
6.016621	436.159570	8.005210
5.925233	434.870586	8.010227
5.595573	441.486259	8.015245
6.310183	452.725617	8.020262
6.136983	462.904892	8.025280
5.886518	460.504753	8.030298
6.223293	458.533306	8.035315
6.151475	469.602407	8.040333
6.766398	465.239484	8.045350
6.439633	450.035720	8.050368
6.270335	448.992469	8.055386
6.344334	435.979143	8.060403
6.218325	438.110121	8.065421
6.201156	442.884358	8.070438
6.150356	439.272681	8.075456
6.011352	435.340313	8.080474
5.957342	431.738608	8.085491
6.228016	442.937064	8.090509
6.255849	440.622710	8.095526
6.462880	435.932389	8.100544
6.322206	437.049508	8.105562
6.073852	433.203701	8.110579
6.135432	434.128187	8.115597
6.135600	433.932531	8.120614
6.189708	432.279927	8.125632
5.895387	440.660447	8.130650
5.793931	442.838071	8.135667
6.066169	459.883930	8.140685
6.645222	460.585329	8.145702
6.466226	466.117066	8.150720
6.181052	454.280302	8.155738
6.509532	447.955195	8.160755
6.331873	453.590859	8.165773
6.321907	443.531860	8.170790
6.218079	442.759214	8.175808
6.000941	444.866602	8.180826
6.675840	442.785375	8.185843
5.975330	446.363348	8.190861
6.486583	440.984739	8.195878
6.425845	449.341288	8.200896
6.120708	446.870822	8.205914
6.338583	444.640299	8.210931
6.302015	445.258275	8.215949
6.236045	448.907239	8.220966
6.517407	465.658188	8.225984
6.761815	452.245769	8.231002
6.552820	447.039967	8.236019
6.175671	455.461874	8.241037
6.213587	443.451419	8.246054
6.538520	446.572082	8.251072
6.251189	447.595417	8.256090
6.284304	441.982458	8.261107
6.147624	441.095040	8.266125
6.141266	446.258899	8.271142
6.414857	462.095889	8.276160
6.329218	468.540796	8.281178
6.532846	460.183996	8.286195
6.317221	463.111649	8.291213
6.470948	467.796001	8.296230
6.250067	462.001928	8.301248
6.465357	461.949289	8.306266
6.401949	463.679147	8.311283
6.345997	466.736416	8.316301
6.296823	459.659443	8.321318
6.451234	457.845956	8.326336
6.624152	472.231296	8.331354
6.688833	464.817750	8.336371
6.746845	469.245702	8.341389
6.400152	457.570052	8.346406
6.721240	456.200659	8.351424
6.044163	450.736840	8.356442
6.241431	453.176927	8.361459
6.600072	458.119500	8.366477
6.612310	462.633517	8.371494
6.531705	454.949252	8.376512
6.548272	464.694857	8.381530
6.358103	460.518039	8.386547
6.149719	465.416915	8.391565
6.220697	461.650455	8.396582
6.534230	463.636830	8.401600
6.261199	460.848910	8.406618
6.791189	466.080216	8.411635
6.630111	467.828533	8.416653
6.662771	463.339093	8.421670
6.689055	462.839546	8.426688
6.488248	473.313484	8.431706
6.169205	469.806945	8.436723
6.464264	466.002219	8.441741
6.438210	466.747935	8.446758
6.545372	457.715137	8.451776
6.592938	453.971281	8.456794
6.740807	459.903077	8.461811
6.493944	466.537344	8.466829
6.278832	464.377815	8.471846
6.419640	449.596247	8.476864
6.495377	458.537325	8.481882
6.623273	453.338696	8.486899
6.310106	460.516675	8.491917
6.450993	458.399197	8.496934
6.722192	464.917579	8.501952
6.390675	480.802058	8.506970
6.669006	476.261500	8.511987
6.460095	484.350950	8.517005
6.560622	480.895433	8.522022
6.599034	477.724202	8.527040
6.534457	490.338510	8.532058
6.710261	486.129591	8.537075
6.550166	494.460703	8.542093
6.311411	499.626276	8.547110
6.656691	481.713672	8.552128
6.554607	497.540128	8.557146
6.569447	493.643603	8.562163
6.586023	497.601532	8.567181
6.612814	488.824306	8.572199
6.811394	488.641742	8.577216
6.694786	494.195271	8.582234
6.689634	494.596889	8.587251
6.453112	489.739368	8.592269
6.407887	496.985831	8.597287
7.050727	485.514879	8.602304
6.531684	491.579580	8.607322
6.572787	486.445033	8.612339
6.943248	497.239729	8.617357
6.868958	498.507395	8.622375
6.793007	493.482704	8.627392
6.875726	496.578211	8.632410
6.788399	483.959353	8.637427
6.707010	493.442614	8.642445
6.442602	495.207123	8.647463
6.902206	503.800902	8.652480
6.470476	507.481940	8.657498
7.010970	510.723473	8.662515
7.073855	512.458794	8.667533
7.072189	501.827266	8.672551
6.722751	490.937811	8.677568
6.665279	498.744767	8.682586
6.889707	506.703215	8.687603
7.033237	509.984854	8.692621
7.070819	500.779901	8.697639
6.786309	485.689405	8.702656
6.651788	496.083544	8.707674
6.630846	497.292359	8.712691
7.043371	511.147887	8.717709
6.919658	514.244184	8.722727
7.305173	504.975246	8.727744
6.961780	502.936796	8.732762
6.801958	497.259376	8.737779
6.702804	497.609452	8.742797
6.659388	491.838056	8.747815
6.839858	496.461421	8.752832
6.908579	520.500870	8.757850
6.977660	519.461289	8.762867
6.881262	520.710331	8.767885
6.869427	519.090142	8.772903
6.735248	518.543153	8.777920
6.700249	519.870936	8.782938
6.738772	521.392326	8.787955
7.033017	515.369203	8.792973
6.740784	521.281614	8.797991
7.003053	526.214060	8.803008
6.989062	518.648717	8.808026
6.962701	513.811908	8.813043
7.381737	520.843630	8.818061
7.013294	519.115215	8.823079
7.052647	522.182807	8.828096
6.700281	525.270750	8.833114
6.865627	513.770453	8.838131
7.086564	519.520408	8.843149
6.926659	530.249901	8.848167
6.968258	507.666958	8.853184
6.934238	520.285967	8.858202
7.134300	515.644054	8.863219
7.080273	517.845814	8.868237
7.041887	521.244320	8.873255
7.320826	518.268923	8.878272
6.711763	522.728824	8.883290
7.029640	510.472489	8.888307
6.912180	526.705320	8.893325
6.769252	527.415702	8.898343
7.085391	517.352904	8.903360
6.936242	522.810555	8.908378
6.844929	532.055552	8.913395
7.083035	543.855617	8.918413
6.953417	550.641957	8.923431
7.506451	558.081886	8.928448
7.332771	549.560100	8.933466
7.074744	534.500128	8.938483
6.621954	530.509607	8.943501
7.092253	552.333935	8.948519
7.271600	545.741828	8.953536
7.146397	549.892396	8.958554
7.142028	553.216151	8.963571
7.308780	552.580985	8.968589
7.343942	559.328887	8.973607
7.306311	551.173946	8.978624
7.227415	558.021770	8.983642
7.102694	555.011783	8.988659
7.488273	539.633216	8.993677
7.589230	547.497420	8.998695
7.033442	531.098714	9.003712
7.112033	522.793034	9.008730
6.928968	531.118295	9.013747
7.168366	542.044005	9.018765
7.391802	549.636557	9.023783
7.577611	541.661205	9.028800
7.387145	544.272507	9.033818
7.253538	538.092352	9.038835
7.094424	532.493704	9.043853
7.327934	543.016398	9.048871
7.271501	536.565377	9.053888
7.445693	539.428810	9.058906
7.129394	533.422448	9.063923
7.351890	534.987597	9.068941
7.194959	540.194009	9.073959
7.545211	537.983759	9.078976
6.933384	537.072953	9.083994
7.300450	544.829190	9.089011
7.227862	548.034246	9.094029
7.608808	553.462498	9.099047
7.245401	548.284016	9.104064
7.293666	556.607757	9.109082
7.303539	552.601545	9.114099
7.904458	551.251417	9.119117
7.509735	540.107098	9.124135
7.463080	535.683715	9.129152
7.156406	525.598576	9.134170
7.143056	521.239406	9.139187
7.379296	531.430307	9.144205
7.400737	546.388547	9.149223
7.313854	549.548506	9.154240
7.410400	548.072278	9.159258
7.243879	555.363016	9.164275
7.543502	558.033231	9.169293
7.364806	559.329883	9.174311
7.178304	551.450731	9.179328
7.594139	555.267222	9.184346
7.296937	551.242852	9.189363
7.707570	552.857419	9.194381
7.443756	553.858141	9.199399
7.009035	548.772883	9.204416
7.583457	543.141350	9.209434
7.328726	543.500024	9.214451
7.434394	548.567465	9.219469
7.242660	548.588067	9.224487
7.378716	546.304079	9.229504
7.597529	545.831169	9.234522
7.326346	549.389231	9.239539
7.372143	548.757237	9.244557
7.257359	547.885318	9.249575
7.011300	546.715233	9.254592
7.544180	561.340889	9.259610
7.691077	576.481468	9.264627
7.976185	566.511866	9.269645
7.719212	560.881205	9.274663
7.754690	566.357278	9.279680
7.877593	551.486914	9.284698
7.673558	554.308625	9.289715
7.917894	550.234119	9.294733
7.737459	551.587848	9.299751
7.671609	548.584418	9.304768
7.553626	549.836844	9.309786
7.629048	554.492462	9.314803
7.764718	546.354551	9.319821
7.736840	557.801828	9.324839
7.601302	550.997125	9.329856
7.500237	546.620135	9.334874
7.524184	548.017579	9.339891
7.745334	543.085178	9.344909
7.408155	557.894490	9.349927
7.278065	547.459781	9.354944
7.575992	547.965392	9.359962
7.584145	553.597220	9.364979
7.581073	556.033996	9.369997
7.332788	557.392045	9.375015
7.235949	556.529936	9.380032
7.595405	562.624274	9.385050
7.689318	573.680095	9.390067
7.768670	577.953253	9.395085
7.821161	579.961607	9.400103
7.864085	587.213230	9.405120
8.064752	574.738532	9.410138
7.556474	574.654096	9.415155
7.939512	570.983886	9.420173
7.574715	565.594179	9.425191
7.876340	581.998080	9.430208
7.928537	577.540264	9.435226
7.492530	579.940736	9.440243
7.536136	564.457939	9.445261
7.574526	579.921632	9.450279
7.858169	568.607892	9.455296
7.663694	577.954282	9.460314
7.622329	575.133203	9.465331
7.880307	576.468735	9.470349
7.619354	583.499727	9.475367
7.677855	576.052389	9.480384
7.805868	583.656750	9.485402
7.764702	588.343268	9.490419
7.865018	585.096047	9.495437
7.646484	584.221447	9.500455
7.916951	586.224050	9.505472
7.953444	583.898853	9.510490
7.989593	595.724284	9.515507
8.217443	583.163271	9.520525
8.110271	579.033380	9.525543
7.926618	585.541023	9.530560
8.081512	575.074269	9.535578
8.148937	578.841214	9.540595
8.212273	576.041599	9.545613
8.283854	576.412262	9.550631
7.977590	569.564875	9.555648
7.655545	566.929785	9.560666
7.928361	578.765460	9.565683
7.980889	580.272037	9.570701
7.944941	576.017380	9.575719
7.959414	588.455270	9.580736
7.933360	575.952978	9.585754
7.662013	584.752842	9.590771
8.062380	582.967077	9.595789
7.879605	581.521987	9.600807
7.713428	585.133031	9.605824
7.999167	574.756229	9.610842
7.909173	578.582552	9.615859
8.120290	572.348374	9.620877
8.143064	583.784575	9.625895
8.061374	584.892462	9.630912
8.430294	581.464301	9.635930
7.858622	585.075763	9.640947
8.005234	578.135324	9.645965
7.814107	580.787760	9.650983
7.791460	585.405104	9.656000
8.088766	577.323904	9.661018
7.961920	575.999440	9.666035
7.926021	576.134480	9.671053
7.933699	573.741216	9.676071
7.913000	573.394194	9.681088
8.461114	567.388081	9.686106
7.867075	567.437003	9.691123
7.806276	574.846883	9.696141
8.011202	579.497996	9.701159
8.083331	604.202895	9.706176
8.175661	592.351071	9.711194
8.258192	599.031607	9.716211
8.266920	600.948990	9.721229
8.113563	579.987023	9.726247
8.284806	586.186597	9.731264
8.685454	581.276555	9.736282
8.021126	579.578714	9.741299
8.324449	576.132429	9.746317
8.112242	566.449030	9.751335
7.943782	570.139323	9.756352
8.176104	571.286372	9.761370
8.408420	575.223139	9.766387
7.919341	573.283247	9.771405
8.423611	580.169094	9.776423
8.303857	587.739695	9.781440
8.568260	571.954054	9.786458
8.159621	575.603085	9.791475
8.008984	568.863858	9.796493
8.017981	579.005185	9.801511
8.162765	597.945686	9.806528
8.587578	599.838901	9.811546
8.113757	603.068963	9.816563
7.905783	602.871203	9.821581
7.879119	606.974787	9.826599
8.250485	608.485059	9.831616
8.653142	602.549063	9.836634
8.403137	605.204416	9.841651
8.321605	599.587280	9.846669
8.657003	602.939859	9.851687
8.386412	607.021702	9.856704
8.416920	604.486002	9.861722
8.219552	607.436064	9.866739
8.483603	605.176196	9.871757
8.335278	597.231081	9.876775
8.012675	604.470555	9.881792
8.400110	592.648234	9.886810
8.337765	598.448911	9.891827
8.202891	602.493710	9.896845
8.398727	594.766071	9.901863
8.323447	606.990820	9.906880
8.398452	599.657650	9.911898
8.579358	602.557911	9.916915
8.673105	601.978363	9.921933
8.548314	606.801064	9.926951
8.308058	609.192959	9.931968
8.383331	607.095212	9.936986
8.457000	601.794584	9.942003
8.288691	602.616243	9.947021
8.391315	607.147693	9.952039
8.118179	605.420114	9.957056
8.065118	601.199690	9.962074
8.240789	616.493584	9.967091
8.986327	622.312856	9.972109
8.947307	618.219616	9.977127
8.824813	614.385607	9.982144
8.700927	607.140402	9.987162
8.744436	608.307569	9.992179
8.544643	596.873896	9.997197
8.532591	604.023688	10.002215
8.757632	605.629469	10.007232
8.485167	601.490758	10.012250
8.441952	597.666423	10.017267
8.479422	606.850255	10.022285
8.688276	600.228258	10.027303
8.382097	604.321988	10.032320
8.834522	594.162054	10.037338
8.917393	597.169192	10.042355
8.277367	602.214630	10.047373
8.529154	599.265565	10.052391
8.587645	598.675762	10.057408
8.316322	599.734467	10.062426
8.630726	603.617354	10.067443
8.378163	610.536588	10.072461
8.970051	609.516074	10.077479
9.069006	618.608228	10.082496
8.703168	619.142101	10.087514
8.506108	614.638123	10.092531
8.820866	615.036958	10.097549
8.924635	615.784430	10.102567
8.653813	614.129071	10.107584
8.703750	605.859400	10.112602
8.566641	608.604362	10.117619
8.915187	620.709066	10.122637
9.075722	623.536782	10.127655
8.874049	616.076544	10.132672
8.433037	601.982456	10.137690
8.868813	611.230115	10.142707
8.542506	610.915197	10.147725
8.707417	613.111067	10.152743
9.117905	622.927582	10.157760
9.033488	613.034787	10.162778
8.523644	613.726922	10.167795
8.798294	613.990030	10.172813
8.693906	626.730592	10.177831
8.258897	621.146742	10.182848
8.892639	628.949594	10.187866
8.747307	626.772801	10.192883
8.930977	624.572861	10.197901
9.127508	625.286865	10.202919
8.741012	625.893402	10.207936
8.790369	630.963378	10.212954
8.776507	628.055931	10.217971
8.675165	632.565696	10.222989
8.763957	626.508455	10.228007
8.970803	635.870891	10.233024
8.869299	626.173269	10.238042
8.913891	627.737898	10.243059
8.497970	641.035366	10.248077
9.378303	630.716848	10.253095
8.882692	628.585469	10.258112
8.973438	630.802429	10.263130
9.067608	630.658314	10.268147
9.035317	620.157746	10.273165
9.013265	620.593573	10.278183
9.366727	626.288085	10.283200
8.941280	618.032932	10.288218
9.019959	625.364175	10.293235
8.908467	627.095270	10.298253
8.912003	621.231270	10.303271
9.012543	615.614003	10.308288
8.817952	624.764777	10.313306
9.073388	624.989870	10.318323
9.145978	626.335518	10.323341
9.400067	620.280782	10.328359
9.136709	626.561087	10.333376
9.126660	623.507876	10.338394
9.280377	615.821541	10.343411
9.122226	629.450996	10.348429
9.219664	623.840525	10.353447
8.844321	622.012194	10.358464
9.080249	628.132220	10.363482
9.329886	632.261946	10.368499
9.011989	629.231722	10.373517
9.363456	620.324665	10.378535
9.098918	618.709347	10.383552
9.255796	621.796412	10.388570
8.913297	617.965315	10.393587
9.018385	624.194203	10.398605
9.388729	615.785962	10.403623
9.423730	625.847503	10.408640
8.993257	625.719318	10.413658
9.152968	619.723551	10.418675
8.909909	622.377818	10.423693
9.078238	616.241847	10.428711
9.200149	634.128778	10.433728
9.394289	640.694012	10.438746
9.396018	634.385322	10.443763
9.059428	628.350549	10.448781
9.316108	643.827433	10.453799
9.236484	651.060414	10.458816
9.258982	651.937386	10.463834
9.455106	655.602131	10.468851
9.625324	645.262323	10.473869
9.358613	629.184306	10.478887
9.146815	628.725214	10.483904
8.837830	626.249014	10.488922
9.228709	635.109245	10.493939
9.396891	655.340019	10.498957
9.610231	650.860093	10.503975
9.595609	656.094735	10.508992
9.315266	659.161948	10.514010
9.958431	650.692011	10.519027
9.305576	644.631045	10.524045
9.437978	629.569780	10.529063
9.036914	635.376203	10.534080
9.299574	647.011544	10.539098
9.731840	649.178152	10.544115
9.499280	650.707313	10.549133
9.168303	641.780940	10.554151
9.569890	652.520360	10.559168
9.630025	664.884877	10.564186
9.875491	661.545472	10.569203
9.579765	641.312640	10.574221
9.586699	631.645362	10.579239
9.526648	632.427970	10.584256
9.383047	633.624455	10.589274
9.393510	625.660760	10.594291
9.371551	640.868875	10.599309
9.601294	637.134307	10.604327
9.443660	626.435624	10.609344
9.360293	641.154745	10.614362
9.833466	636.302752	10.619379
9.458033	647.261743	10.624397
9.821892	653.961336	10.629415
9.531314	634.115869	10.634432
9.309265	632.146755	10.639450
9.719347	640.000435	10.644467
9.721183	655.274262	10.649485
9.554943	644.905120	10.654503
9.896158	645.817361	10.659520
9.643826	639.876679	10.664538
9.797568	627.226260	10.669555
9.727418	634.744928	10.674573
9.804692	624.372357	10.679591
9.695269	628.160710	10.684608
9.428849	625.819852	10.689626
9.764566	622.983864	10.694643
9.674231	630.269008	10.699661
9.396786	626.897930	10.704679
9.380601	632.483104	10.709696
9.541428	642.632237	10.714714
10.166598	647.286950	10.719731
10.058672	649.579222	10.724749
10.028956	640.766593	10.729767
9.559356	630.845777	10.734784
9.620254	632.281620	10.739802
9.620365	618.096313	10.744819
9.823116	633.938244	10.749837
9.717808	643.176023	10.754855
9.797068	648.705222	10.759872
9.523985	655.842284	10.764890
9.782006	652.396772	10.769907
9.806736	663.555007	10.774925
9.724951	653.952111	10.779943
9.745480	647.227060	10.784960
9.720288	652.447578	10.789978
10.095282	655.468916	10.794995
9.984522	660.008566	10.800013
9.876185	657.352602	10.805031
9.841574	656.834189	10.810048
9.733567	650.312313	10.815066
10.323828	656.402078	10.820083
9.826513	658.954177	10.825101
9.782130	655.969456	10.830119
9.590204	656.154189	10.835136
9.671797	653.171821	10.840154
9.656188	646.704897	10.845171
9.604790	649.843535	10.850189
9.493535	658.151292	10.855207
10.048659	651.383504	10.860224
9.784022	661.290041	10.865242
10.174196	661.733864	10.870259
9.932913	661.901084	10.875277
10.056215	666.536607	10.880295
10.319013	652.256466	10.885312
10.189467	657.610101	10.890330
10.493195	656.139272	10.895347
9.996236	657.126036	10.900365
9.953949	662.342924	10.905383
10.272538	649.527805	10.910400
10.080128	664.570143	10.915418
10.551609	656.695148	10.920435
9.944792	652.583565	10.925453
9.958027	658.949933	10.930471
10.073936	654.863967	10.935488
10.133711	653.204144	10.940506
10.247861	647.935029	10.945523
10.218335	651.991735	10.950541
9.971638	658.073781	10.955559
10.058222	653.228706	10.960576
10.009599	656.158626	10.965594
9.859520	650.864639	10.970611
9.862137	651.754193	10.975629
9.868417	670.748030	10.980647
10.254422	675.897816	10.985664
10.408781	677.615665	10.990682
10.572726	671.915863	10.995699
10.159355	659.590963	11.000717
9.799076	656.267573	11.005735
10.176565	672.037978	11.010752
10.062699	678.941819	11.015770
10.089668	674.295427	11.020787
10.328150	680.866352	11.025805
10.157168	684.254107	11.030823
10.683739	671.980742	11.035840
10.268222	674.845075	11.040858
10.426395	679.620305	11.045875
10.315241	674.048812	11.050893
10.083183	690.814143	11.055911
10.418667	683.957680	11.060928
10.160281	685.206867	11.065946
10.664879	678.200833	11.070963
10.538016	674.342250	11.075981
10.548452	683.101167	11.080999
10.636933	665.272796	11.086016
10.303285	674.508499	11.091034
10.279478	671.400631	11.096051
10.268653	670.966853	11.101069
10.215817	673.774360	11.106087
10.399089	670.236415	11.111104
10.619422	676.134839	11.116122
10.502123	677.295648	11.121139
10.223933	679.261150	11.126157
10.350512	676.700920	11.131175
10.805489	673.625332	11.136192
10.560636	673.452284	11.141210
10.581321	674.323230	11.146227
10.564972	675.745933	11.151245
10.528924	674.255755	11.156263
10.503355	676.169053	11.161280
10.541309	682.891318	11.166298
10.278341	675.352296	11.171315
10.730320	683.401403	11.176333
10.400985	685.078273	11.181351
10.726087	682.319679	11.186368
10.667474	677.020820	11.191386
10.933136	674.536628	11.196403
10.672643	674.656365	11.201421
10.779772	683.857725	11.206439
10.953063	672.715844	11.211456
10.706388	665.713916	11.216474
10.152353	654.338866	11.221491
10.703591	666.459180	11.226509
10.656683	676.218002	11.231527
10.627827	674.660425	11.236544
10.589721	677.071149	11.241562
10.765162	684.068519	11.246579
11.054069	682.536895	11.251597
10.555275	678.427316	11.256615
10.685195	667.478426	11.261632
10.467835	680.489191	11.266650
10.697689	679.954587	11.271667
10.284126	679.552353	11.276685
10.508495	673.104624	11.281703
10.734841	668.259738	11.286720
10.562381	676.952634	11.291738
10.396976	678.373445	11.296755
11.049586	671.322132	11.301773
10.970115	677.393762	11.306791
10.651543	667.373523	11.311808
10.542793	670.028844	11.316826
10.488413	667.377047	11.321843
10.827544	670.965740	11.326861
10.668656	686.706590	11.331879
10.642129	692.886695	11.336896
10.855276	693.282517	11.341914
10.573029	703.359093	11.346931
10.952271	698.531269	11.351949
10.861607	700.915517	11.356967
10.725973	695.366788	11.361984
10.705214	699.412663	11.367002
10.674638	696.166995	11.372019
10.956428	697.757582	11.377037
10.586073	704.111483	11.382055
10.871517	697.966602	11.387072
10.999340	705.315424	11.392090
10.939328	700.250308	11.397107
10.719841	703.838170	11.402125
10.956566	707.726939	11.407143
11.076488	691.127540	11.412160
10.958863	700.420928	11.417178
10.861312	696.065440	11.422195
11.276101	709.684083	11.427213
11.241501	713.205109	11.432231
11.215155	709.406508	11.437248
11.367675	698.561356	11.442266
11.012300	706.796931	11.447283
10.815023	703.362786	11.452301
10.683114	707.886827	11.457319
10.909745	714.652125	11.462336
11.269340	713.857351	11.467354
11.208136	721.220018	11.472371
10.950892	719.543587	11.477389
10.945113	722.694025	11.482407
11.324190	721.829925	11.487424
11.286425	733.389316	11.492442
11.486401	727.645982	11.497459
11.359698	725.601957	11.502477
11.254284	714.746715	11.507495
11.330676	703.361221	11.512512
10.977843	703.520673	11.517530
10.901363	697.839598	11.522547
11.203284	710.885789	11.527565
11.534599	724.337640	11.532583
11.667758	712.466716	11.537600
11.619186	709.738263	11.542618
11.325167	708.951224	11.547635
11.416437	707.557860	11.552653
10.998617	701.135001	11.557671
11.754081	704.434407	11.562688
11.199865	706.238032	11.567706
11.310553	711.740236	11.572723
11.276277	710.978771	11.577741
11.247003	708.335658	11.582759
11.347933	713.479628	11.587776
11.093721	702.319503	11.592794
11.193653	709.246663	11.597811
11.576644	725.129862	11.602829
11.236619	722.538591	11.607847
11.676634	726.098866	11.612864
11.728533	709.203993	11.617882
11.384896	706.783705	11.622899
11.268587	696.561344	11.627917
11.467115	714.016627	11.632935
11.799454	715.592984	11.637952
11.641691	714.336470	11.642970
11.563355	707.238722	11.647987
11.758054	700.297013	11.653005
11.447061	698.408099	11.658023
11.541995	693.747898	11.663040
11.446236	694.356222	11.668058
11.323177	696.780259	11.673075
11.307892	690.092362	11.678093
11.231279	696.857829	11.683111
11.005760	710.800859	11.688128
11.416870	721.949085	11.693146
11.318829	726.906483	11.698163
11.359194	726.455216	11.703181
11.032457	734.900912	11.708199
11.070650	722.552554	11.713216
11.847375	733.548828	11.718234
11.698136	738.539497	11.723251
11.752674	724.702186	11.728269
11.621629	723.009138	11.733287
11.473700	725.591710	11.738304
11.654457	741.405624	11.743322
11.661069	745.204223	11.748339
12.063729	742.695401	11.753357
11.873833	736.038001	11.758375
11.858339	728.700024	11.763392
11.819743	720.762908	11.768410
11.397273	725.562854	11.773427
11.603231	726.019763	11.778445
12.060014	738.571494	11.783463
12.072935	734.668905	11.788480
12.287239	728.052319	11.793498
11.905725	725.947232	11.798515
12.187439	723.419493	11.803533
11.995025	719.874129	11.808551
11.792766	721.272315	11.813568
12.218574	725.680575	11.818586
11.592156	725.497882	11.823603
12.180474	721.382066	11.828621
12.004563	725.433321	11.833639
11.900915	721.302846	11.838656
11.801337	724.206048	11.843674
11.571280	730.127720	11.848691
11.989525	714.185305	11.853709
11.957452	718.848342	11.858727
11.967780	723.122882	11.863744
12.144891	716.736191	11.868762
11.976660	715.901039	11.873779
12.279608	711.722639	11.878797
12.009828	728.702200	11.883815
11.758019	726.409533	11.888832
12.076922	711.691363	11.893850
11.666116	725.215310	11.898867
11.963660	723.937950	11.903885
11.766314	718.503025	11.908903
12.027683	714.135478	11.913920
12.319844	719.991104	11.918938
12.114402	722.200834	11.923955
11.591182	715.434721	11.928973
11.871387	721.693009	11.933991
12.051285	722.769386	11.939008
12.104096	718.582839	11.944026
11.806982	721.848351	11.949043
11.987914	740.729691	11.954061
12.199900	743.451535	11.959079
12.218194	741.624632	11.964096
12.529308	743.766053	11.969114
12.256846	748.372087	11.974131
12.446149	742.179138	11.979149
12.395813	729.727880	11.984167
12.359580	721.768303	11.989184
12.368951	714.492708	11.994202
12.259252	715.412486	11.999219
12.125369	717.042957	12.004237
11.871133	721.955398	12.009255
11.842971	728.628079	12.014272
12.545210	731.102694	12.019290
12.357046	746.838715	12.024307
12.138947	749.145106	12.029325
12.420071	749.505032	12.034343
12.659566	752.986276	12.039360
12.356333	745.620791	12.044378
12.147978	749.380488	12.049395
12.373973	746.309207	12.054413
12.483695	746.481393	12.059431
12.260320	749.508138	12.064448
12.493508	744.018371	12.069466
12.379894	749.562042	12.074483
12.556493	737.362402	12.079501
12.305493	741.785190	12.084519
12.252110	745.258672	12.089536
12.626061	753.581969	12.094554
12.400529	749.596817	12.099571
12.507984	741.693614	12.104589
12.339817	742.010326	12.109607
12.424715	747.592321	12.114624
12.406751	736.003837	12.119642
12.249000	748.613991	12.124659
12.324490	743.306724	12.129677
12.300702	738.453673	12.134695
12.391281	743.570871	12.139712
12.496483	743.806881	12.144730
12.346891	745.869007	12.149747
12.110482	742.693451	12.154765
12.709906	753.979450	12.159783
12.660744	765.038872	12.164800
13.139764	761.972126	12.169818
12.560806	758.970159	12.174835
12.307573	750.549104	12.179853
12.405578	751.288018	12.184871
12.459203	766.418125	12.189888
12.515520	765.263765	12.194906
12.544001	774.262898	12.199923
12.897776	768.659556	12.204941
12.461843	772.811523	12.209959
12.855793	779.604280	12.214976
12.657254	775.485504	12.219994
12.591915	780.005444	12.225011
12.878672	772.522261	12.230029
12.780105	770.836743	12.235047
13.058600	772.184855	12.240064
13.052180	768.067537	12.245082
12.836261	767.293504	12.250099
12.711716	770.336326	12.255117
12.862548	769.280766	12.260135
12.871017	772.785588	12.265152
13.131644	771.403555	12.270170
13.108936	767.380309	12.275187
12.957387	766.088103	12.280205
13.084038	767.021345	12.285223
12.824974	770.688006	12.290240
12.980649	772.342541	12.295258
13.242985	775.877016	12.300275
12.985911	761.886527	12.305293
13.324846	761.388479	12.310311
12.690369	755.946292	12.315328
13.211566	759.563282	12.320346
12.756669	768.518227	12.325363
13.070646	773.698263	12.330381
13.417405	764.176486	12.335399
13.019576	756.658560	12.340416
13.033663	750.849668	12.345434
12.781760	754.941239	12.350451
13.108108	763.587582	12.355469
13.150120	767.749870	12.360487
12.923376	767.684438	12.365504
12.975446	767.117727	12.370522
13.122068	764.011542	12.375539
12.980670	767.849115	12.380557
13.204820	770.606927	12.385575
12.955942	766.937856	12.390592
13.000870	773.602258	12.395610
13.258540	770.226206	12.400627
13.064967	771.989111	12.405645
13.358602	763.999922	12.410663
13.204122	761.733026	12.415680
13.361260	766.445325	12.420698
13.308676	770.884369	12.425715
13.012534	765.789959	12.430733
13.242415	764.138186	12.435751
13.223828	770.250802	12.440768
13.378625	766.395405	12.445786
13.558746	781.773951	12.450803
13.162843	773.608771	12.455821
13.304998	768.751802	12.460839
13.156565	775.332891	12.465856
13.056683	763.668861	12.470874
13.351257	759.785254	12.475891
13.259941	769.671006	12.480909
13.128826	764.481311	12.485927
13.661626	773.104779	12.490944
13.270039	767.419404	12.495962
13.699026	768.680819	12.500979
13.138839	778.141419	12.505997
13.365894	769.105458	12.511015
13.127557	780.257646	12.516032
13.673806	775.873852	12.521050
13.389990	776.470617	12.526067
13.395829	769.848809	12.531085
13.752791	774.542424	12.536103
13.331512	780.156400	12.541120
13.498257	786.170555	12.546138
13.670370	799.401252	12.551155
13.531855	787.642274	12.556173
13.557947	783.040173	12.561191
13.633412	797.658797	12.566208
13.571273	799.625175	12.571226
13.469778	788.194914	12.576243
13.517295	808.274352	12.581261
13.801554	801.943427	12.586279
13.637447	808.668996	12.591296
13.805147	806.149641	12.596314
13.962905	797.443263	12.601331
13.555394	792.615604	12.606349
13.717562	789.191396	12.611367
13.341124	796.590862	12.616384
13.708271	796.514430	12.621402
13.697938	797.873083	12.626419
13.659496	800.315435	12.631437
13.846374	799.402550	12.636455
13.869524	808.165848	12.641472
13.855320	806.366122	12.646490
13.963017	800.971740	12.651507
13.519127	806.715500	12.656525
13.548644	788.426027	12.661543
13.541139	811.269128	12.666560
13.794915	801.578862	12.671578
13.831118	799.408318	12.676595
13.757237	800.922097	12.681613
14.025850	795.322622	12.686631
13.706378	806.111995	12.691648
13.590373	798.912814	12.696666
13.813131	789.069624	12.701683
13.593998	797.072453	12.706701
14.332171	808.046411	12.711719
13.984160	802.183783	12.716736
13.820343	802.988967	12.721754
14.040557	802.080327	12.726771
14.052607	800.131319	12.731789
13.838354	795.383835	12.736807
13.846634	812.300973	12.741824
14.089068	812.685898	12.746842
14.146711	817.429578	12.751859
13.970951	826.306102	12.756877
14.104740	816.811354	12.761895
14.328567	826.843423	12.766912
14.342004	816.136757	12.771930
14.212488	806.039480	12.776947
14.012109	795.981714	12.781965
14.504635	797.750733	12.786983
14.580985	801.197588	12.792000
14.242010	791.152072	12.797018
14.211792	782.487776	12.802035
14.032540	790.869365	12.807053
14.339005	787.996909	12.812071
14.291029	786.211944	12.817088
14.005854	795.294945	12.822106
14.094037	788.325711	12.827123
13.831212	793.526697	12.832141
14.618127	810.239785	12.837159
14.335510	805.231608	12.842176
14.191398	795.903491	12.847194
14.299189	789.038481	12.852211
14.554280	798.945714	12.857229
14.414740	792.226754	12.862247
14.130025	785.003519	12.867264
14.211782	800.287039	12.872282
14.415232	810.041421	12.877299
14.546880	813.164031	12.882317
14.562736	810.870440	12.887335
14.332120	806.362204	12.892352
14.189357	804.166051	12.897370
14.755924	818.991770	12.902387
14.473792	818.994977	12.907405
14.862746	808.434608	12.912423
14.493648	800.934252	12.917440
14.225873	798.940725	12.922458
14.516032	797.052286	12.927475
14.300048	811.577729	12.932493
14.566276	803.056325	12.937511
14.500597	813.383056	12.942528
14.609925	809.430632	12.947546
14.976298	806.204801	12.952563
14.476167	813.513201	12.957581
14.687822	805.360111	12.962599
14.580293	819.676062	12.967616
14.601644	823.488148	12.972634
14.824530	817.665455	12.977651
14.757565	819.023515	12.982669
14.925060	810.504954	12.987687
14.564315	820.704350	12.992704
14.605705	812.221326	12.997722
14.699230	812.945165	13.002739
14.354575	817.679293	13.007757
14.565698	814.225319	13.012775
14.641687	815.829227	13.017792
14.503614	811.732527	13.022810
14.801944	814.447166	13.027827
14.723385	825.315569	13.032845
14.524127	810.236688	13.037863
14.921018	820.131182	13.042880
14.874278	825.064790	13.047898
14.960947	814.283535	13.052915
14.723717	817.018969	13.057933
14.524261	812.379615	13.062951
14.921440	820.203839	13.067968
14.505596	808.103287	13.072986
14.960211	823.296849	13.078003
15.183281	838.476208	13.083021
15.321104	831.600166	13.088039
14.976777	824.992175	13.093056
14.549943	816.920185	13.098074
15.129694	820.979297	13.103091
15.123130	835.102715	13.108109
15.380367	826.828864	13.113127
15.057472	814.325577	13.118144
15.066673	809.741895	13.123162
15.328039	806.030739	13.128179
15.046514	808.880411	13.133197
14.860190	805.330919	13.138215
14.886050	806.324138	13.143232
14.735234	822.369957	13.148250
15.299538	826.336817	13.153267
14.944656	835.923071	13.158285
15.068701	834.376238	13.163303
15.096145	833.055982	13.168320
14.920513	836.545480	13.173338
15.606991	832.098676	13.178355
15.143276	837.520501	13.183373
14.968239	836.399229	13.188391
15.488743	832.013144	13.193408
15.421619	831.764910	13.198426
15.423215	827.646323	13.203443
15.349241	830.627581	13.208461
15.735681	830.226231	13.213479
15.340282	831.301234	13.218496
15.107149	840.587545	13.223514
15.558494	829.411468	13.228531
15.340277	827.672107	13.233549
15.374320	828.967005	13.238567
15.422267	836.006501	13.243584
14.860611	832.152891	13.248602
15.382639	834.763055	13.253619
15.381143	834.902174	13.258637
15.158667	836.978885	13.263655
15.240293	837.354292	13.268672
15.151816	837.712168	13.273690
15.062610	827.561226	13.278707
15.288467	829.902210	13.283725
15.352027	839.268268	13.288743
15.844450	855.569944	13.293760
15.947028	848.661547	13.298778
15.785127	834.731828	13.303795
15.665616	829.840101	13.308813
15.502563	820.991469	13.313831
15.633109	821.832586	13.318848
15.361043	827.562054	13.323866
15.505763	827.836056	13.328883
15.666772	844.470517	13.333901
15.718520	839.848602	13.338919
16.252867	845.391766	13.343936
15.773540	845.492142	13.348954
15.633436	836.693556	13.353971
15.643728	823.301762	13.358989
15.906822	822.121312	13.364007
15.761921	823.983894	13.369024
15.368435	822.729591	13.374042
15.834657	837.151322	13.379059
15.919231	844.024135	13.384077
15.981051	854.305667	13.389095
15.806297	834.239856	13.394112
16.008115	834.438639	13.399130
15.701246	823.649609	13.404147
15.854624	841.228857	13.409165
16.042727	847.485842	13.414183
16.017715	839.521298	13.419200
15.694624	831.896954	13.424218
15.827411	847.276661	13.429235
15.901090	858.843920	13.434253
16.487489	859.872393	13.439271
16.122795	843.771665	13.444288
15.539687	835.803047	13.449306
15.936741	831.272200	13.454323
15.955760	841.244847	13.459341
15.852492	851.523841	13.464359
16.174346	848.011485	13.469376
15.962126	849.663709	13.474394
15.946782	848.649960	13.479411
16.046522	843.783838	13.484429
16.307168	844.509896	13.489447
15.997617	837.157986	13.494464
15.701818	855.732286	13.499482
16.155030	849.160275	13.504499
16.433590	850.814499	13.509517
16.177960	855.938636	13.514535
16.109852	849.751267	13.519552
16.310714	854.854374	13.524570
16.166886	848.161311	13.529587
15.850779	847.939465	13.534605
15.929756	852.329513	13.539623
16.391701	841.328495	13.544640
16.131774	845.216214	13.549658
15.913746	851.218094	13.554675
16.378756	851.397730	13.559693
16.537605	877.484301	13.564711
16.719256	853.692381	13.569728
16.770377	857.162134	13.574746
16.583922	838.698162	13.579763
16.382680	845.748303	13.584781
16.484381	842.090560	13.589799
16.264198	841.714827	13.594816
16.271645	845.554342	13.599834
16.657597	839.295834	13.604851
16.505738	850.800594	13.609869
16.329743	846.678269	13.614887
16.694771	844.014381	13.619904
16.626658	840.828218	13.624922
16.607791	847.073449	13.629939
16.567082	841.225776	13.634957
16.477089	839.270661	13.639975
16.771925	834.661154	13.644992
16.431621	844.576492	13.650010
16.619828	843.148995	13.655027
16.651582	839.192939	13.660045
16.589044	843.021328	13.665063
16.582882	833.901953	13.670080
16.677802	841.454805	13.675098
16.788631	841.554234	13.680115
16.825310	845.913039	13.685133
16.551105	840.101950	13.690151
17.148049	847.614017	13.695168
16.601126	848.690671	13.700186
16.429757	844.293063	13.705203
16.807770	847.500156	13.710221
16.748568	856.626679	13.715239
16.793807	863.098560	13.720256
16.993228	863.177796	13.725274
16.496680	857.111202	13.730291
16.950334	860.129718	13.735309
16.620085	860.194113	13.740327
17.167390	855.854316	13.745344
16.965939	863.961703	13.750362
17.108124	861.402157	13.755379
17.444951	858.294557	13.760397
16.830119	862.048536	13.765415
16.976837	859.611358	13.770432
17.130585	859.997556	13.775450
16.937416	847.906270	13.780467
16.996376	858.781550	13.785485
16.698037	861.274098	13.790503
17.046013	860.017229	13.795520
17.163907	870.990582	13.800538
16.892129	866.308896	13.805555
16.985549	866.818156	13.810573
16.890760	861.846806	13.815591
17.074272	854.849986	13.820608
17.259505	863.644721	13.825626
17.057272	862.202657	13.830643
17.120594	863.284685	13.835661
16.715647	861.009681	13.840679
17.020604	855.391870	13.845696
17.050587	870.150225	13.850714
16.967721	874.032299	13.855731
17.703419	875.236200	13.860749
17.333300	887.504180	13.865767
17.580422	873.819618	13.870784
17.419751	867.899212	13.875802
17.207398	856.350575	13.880819
17.126620	864.817757	13.885837
17.107204	880.281300	13.890855
17.412618	876.102476	13.895872
17.345577	880.815215	13.900890
17.130364	882.467911	13.905907
17.568753	878.407109	13.910925
17.318523	889.611722	13.915943
17.276287	883.609637	13.920960
17.224723	884.084809	13.925978
17.457745	875.092042	13.930995
17.455588	873.135785	13.936013
17.251291	883.301236	13.941031
17.642282	885.133510	13.946048
17.935897	889.594082	13.951066
17.474305	887.981210	13.956083
17.556163	873.360009	13.961101
17.437826	882.360109	13.966119
17.561363	882.261885	13.971136
17.582275	882.678364	13.976154
17.562827	889.018376	13.981171
17.439857	889.545762	13.986189
17.389263	902.398013	13.991207
17.675603	907.301548	13.996224
18.078758	908.317709	14.001242
17.896639	917.722302	14.006259
18.043210	911.305612	14.011277
17.568768	901.839845	14.016295
17.884204	901.553761	14.021312
17.676336	906.250702	14.026330
17.773486	915.756706	14.031347
17.874457	898.601498	14.036365
17.952763	914.166527	14.041383
18.166567	901.724257	14.046400
18.301021	894.965484	14.051418
17.730315	886.329016	14.056435
18.162116	883.692531	14.061453
17.805650	883.827306	14.066471
17.826755	883.858742	14.071488
18.022562	887.107013	14.076506
17.952561	900.520889	14.081523
18.319491	886.792299	14.086541
17.821412	907.500139	14.091559
18.117617	895.669821	14.096576
18.369999	895.188487	14.101594
18.266787	897.445337	14.106611
18.272067	876.767438	14.111629
17.482630	877.531792	14.116647
17.925169	886.115808	14.121664
18.234502	895.686388	14.126682
18.308071	895.293031	14.131699
18.545311	888.552871	14.136717
18.118606	904.357964	14.141735
18.113413	895.222627	14.146752
18.174498	897.999696	14.151770
18.038067	901.085428	14.156787
18.250705	894.822497	14.161805
17.973592	899.738571	14.166823
18.105239	900.945597	14.171840
18.253244	901.279046	14.176858
17.933898	894.704986	14.181875
18.533834	895.172756	14.186893
18.175114	896.608093	14.191911
18.143415	900.093987	14.196928
18.348501	895.684722	14.201946
18.211687	905.520872	14.206963
18.289628	910.062578	14.211981
18.368129	917.116255	14.216999
18.356357	923.489791	14.222016
18.611371	933.561215	14.227034
18.423542	930.235999	14.232051
18.689859	927.104721	14.237069
18.895430	925.788108	14.242087
18.768898	933.224215	14.247104
18.518312	917.569452	14.252122
18.576493	928.934053	14.257139
19.153032	920.420780	14.262157
19.008133	908.385007	14.267175
18.947852	897.655128	14.272192
18.781518	897.927373	14.277210
18.268137	899.017708	14.282227
18.665193	886.799205	14.287245
18.537417	894.374348	14.292263
18.665699	896.326681	14.297280
19.249292	910.464991	14.302298
18.741044	911.971095	14.307315
18.912231	895.647500	14.312333
18.613873	902.018593	14.317351
18.605089	899.425890	14.322368
19.082496	909.232079	14.327386
18.966001	922.880478	14.332403
18.905924	912.595533	14.337421
18.976281	897.685776	14.342439
18.979138	907.285446	14.347456
19.092883	910.316203	14.352474
18.644563	897.112975	14.357491
18.975607	910.066386	14.362509
19.051779	921.352423	14.367527
18.917008	913.850019	14.372544
19.201341	917.857609	14.377562
18.907049	920.371622	14.382579
19.013919	912.575734	14.387597
18.945894	920.113123	14.392615
19.043215	921.369711	14.397632
19.213596	912.216323	14.402650
19.147988	924.319851	14.407667
19.363020	913.272268	14.412685
19.248726	919.100124	14.417703
19.160182	920.657236	14.422720
19.557777	913.563733	14.427738
19.087621	923.941278	14.432755
19.067314	912.763308	14.437773
19.270571	925.477972	14.442791
19.256273	923.012363	14.447808
19.409680	918.314540	14.452826
18.962421	922.862797	14.457843
19.128460	919.185490	14.462861
19.441485	920.307293	14.467879
19.208230	918.500850	14.472896
19.357990	917.035190	14.477914
19.234812	919.686497	14.482931
19.514559	917.266338	14.487949
19.468037	916.203821	14.492967
19.377680	913.907924	14.497984
19.630011	907.976445	14.503002
19.336418	918.278986	14.508019
19.491246	912.662588	14.513037
19.259480	911.297732	14.518055
19.663577	911.502692	14.523072
19.866542	904.928844	14.528090
19.303131	916.526531	14.533107
19.753957	922.650859	14.538125
19.709368	930.758946	14.543143
19.455395	927.216873	14.548160
19.610859	928.022532	14.553178
19.486297	932.586505	14.558195
19.745267	940.732243	14.563213
19.805160	938.841997	14.568231
19.818253	940.793447	14.573248
20.040462	941.250973	14.578266
20.108058	935.067558	14.583283
19.923692	933.149311	14.588301
20.073455	919.924943	14.593319
19.454441	912.362709	14.598336
19.676345	921.552520	14.603354
19.584094	930.523310	14.608371
20.055644	931.102717	14.613389
20.018759	938.550028	14.618407
19.739066	936.012389	14.623424
19.866158	932.439012	14.628442
20.163838	937.324999	14.633459
20.194170	930.869709	14.638477
20.151516	939.596045	14.643495
19.845857	936.844720	14.648512
20.052858	935.019790	14.653530
19.994385	941.189207	14.658547
20.258597	938.853532	14.663565
19.957084	934.220669	14.668583
20.012189	939.554924	14.673600
20.002566	935.860954	14.678618
19.785197	941.603980	14.683635
19.812914	938.456433	14.688653
19.839705	939.512631	14.693671
19.864167	943.087565	14.698688
20.332496	950.111735	14.703706
20.180883	961.332500	14.708723
20.195350	953.910839	14.713741
20.283091	958.728738	14.718759
20.516789	958.221927	14.723776
20.584647	963.270164	14.728794
20.355464	960.156553	14.733811
20.372901	951.708774	14.738829
20.810190	961.404511	14.743847
20.747870	954.963729	14.748864
20.475104	941.562546	14.753882
20.418687	937.636063	14.758899
20.436234	942.859437	14.763917
20.610246	936.918128	14.768935
20.301639	937.282094	14.773952
20.443573	948.904990	14.778970
20.429017	956.572875	14.783987
20.402796	961.711592	14.789005
21.005120	960.837750	14.794023
20.878729	960.081240	14.799040
20.631846	959.454063	14.804058
20.584171	963.261214	14.809075
20.688169	957.365584	14.814093
20.930654	960.016410	14.819111
20.585153	964.924281	14.824128
20.882287	956.372716	14.829146
20.792370	961.956921	14.834163
20.976486	964.872518	14.839181
21.151442	946.143522	14.844199
20.972413	938.035806	14.849216
20.750794	933.469321	14.854234
20.906273	938.734200	14.859251
20.161575	939.545195	14.864269
20.614341	945.211628	14.869287
20.567165	953.149715	14.874304
20.885890	949.287530	14.879322
20.919607	957.863050	14.884339
20.868241	964.135505	14.889357
21.241155	957.471893	14.894375
20.845718	966.505984	14.899392
20.874023	964.320878	14.904410
20.873541	959.653466	14.909427
20.793231	962.266504	14.914445
21.238035	950.734765	14.919463
21.120105	963.190506	14.924480
20.927248	962.864138	14.929498
20.944619	955.404151	14.934515
20.796435	956.560350	14.939533
21.214232	967.199589	14.944551
21.158371	974.769810	14.949568
21.196681	973.517271	14.954586
21.324383	988.601246	14.959603
21.191651	984.285914	14.964621
21.509065	977.703575	14.969639
21.502922	984.786320	14.974656
21.557730	979.816745	14.979674
21.095971	975.316278	14.984691
21.441099	981.479278	14.989709
21.606073	975.877050	14.994727
21.463144	982.122831	14.999744
21.522834	981.709556	15.004762
21.551768	982.967396	15.009779
21.399559	983.196403	15.014797
21.393439	978.479376	15.019815
21.406575	978.420540	15.024832
21.799092	975.720768	15.029850
21.528546	974.974219	15.034867
21.812157	983.425391	15.039885
22.101170	976.585565	15.044903
21.845141	960.054288	15.049920
21.728267	959.283663	15.054938
21.654429	941.685580	15.059955
21.684262	947.342538	15.064973
21.790227	946.915702	15.069991
21.280992	955.939215	15.075008
21.522072	959.265614	15.080026
21.781977	967.041983	15.085043
21.896553	978.886939	15.090061
22.287276	975.291183	15.095079
21.812681	961.407203	15.100096
21.283139	958.258600	15.105114
21.844517	964.482388	15.110131
21.450913	976.687836	15.115149
21.881415	971.110280	15.120167
21.604602	972.636933	15.125184
21.790386	974.141600	15.130202
22.139729	971.237151	15.135219
21.764069	982.603488	15.140237
22.009252	972.381136	15.145255
21.836042	970.372772	15.150272
21.880596	976.721722	15.155290
21.897755	976.311956	15.160307
21.988175	982.398097	15.165325
22.459035	979.455672	15.170343
22.134499	986.881798	15.175360
22.068210	974.486519	15.180378
22.094282	971.209834	15.185395
21.911335	984.401624	15.190413
22.584704	985.492221	15.195431
22.133290	992.565837	15.200448
22.395093	997.618411	15.205466
22.512262	998.294371	15.210483
22.367879	993.340222	15.215501
22.181600	984.558265	15.220519
22.355335	986.225770	15.225536
22.432623	994.854443	15.230554
22.587390	995.988424	15.235571
22.334780	997.621743	15.240589
22.913424	989.196471	15.245607
22.705211	986.666561	15.250624
22.651280	980.543198	15.255642
22.681541	974.018475	15.260659
22.559186	965.188641	15.265677
22.617530	954.856715	15.270695
22.643531	968.820499	15.275712
22.360809	965.279768	15.280730
22.715722	965.984750	15.285747
22.414070	963.545223	15.290765
22.517938	954.705197	15.295783
22.577706	963.538575	15.300800
22.708020	974.683618	15.305818
22.972303	981.831291	15.310835
22.399142	980.639841	15.315853
22.694257	981.474116	15.320871
22.651281	988.064006	15.325888
22.831941	987.208892	15.330906
22.773137	987.199198	15.335923
23.019283	1002.195198	15.340941
22.641213	992.518618	15.345959
22.776923	996.505331	15.350976
22.868841	997.459808	15.355994
23.072531	991.150907	15.361011
23.139473	999.314135	15.366029
22.860756	984.556830	15.371047
22.802126	987.191722	15.376064
22.530995	1000.220612	15.381082
22.686985	991.643806	15.386099
22.722701	998.571672	15.391117
23.206618	997.302963	15.396135
23.199949	989.837261	15.401152
23.136286	995.912834	15.406170
23.400086	993.340527	15.411187
23.079539	995.562012	15.416205
23.096933	989.124508	15.421223
22.814000	998.614367	15.426240
22.825615	1010.147266	15.431258
23.186576	1011.794907	15.436275
23.138113	1018.458253	15.441293
23.424322	1006.118178	15.446311
23.530630	1011.419185	15.451328
23.293746	1019.639494	15.456346
23.700101	1007.438387	15.461363
23.608501	1013.821306	15.466381
23.700982	1008.094724	15.471399
23.790961	1013.142665	15.476416
23.436108	1013.662204	15.481434
23.914335	1000.695588	15.486451
23.582874	1006.364990	15.491469
23.773478	997.164208	15.496487
23.334215	984.631696	15.501504
23.344726	996.448786	15.506522
23.599802	995.083386	15.511539
23.388374	1009.453638	15.516557
23.730999	1002.466545	15.521575
23.847320	1007.617656	15.526592
23.411514	1007.619693	15.531610
23.821252	1011.948490	15.536627
23.699609	1005.539076	15.541645
23.516248	1002.030107	15.546663
23.828753	1003.991458	15.551680
23.593790	1005.590453	15.556698
23.978098	1008.206443	15.561715
23.418994	1012.661791	15.566733
23.359573	1007.902613	15.571751
23.754524	1013.593906	15.576768
23.422326	1004.497124	15.581786
23.915922	1016.143862	15.586803
23.933533	1027.865185	15.591821
24.292618	1037.970857	15.596839
24.036614	1027.151642	15.601856
23.796378	1038.228548	15.606874
24.075980	1027.562105	15.611891
24.209626	1037.176068	15.616909
24.022007	1027.220315	15.621927
24.094058	1038.844751	15.626944
23.786273	1034.348547	15.631962
24.180629	1027.981357	15.636979
24.162957	1032.478114	15.641997
24.181927	1026.308598	15.647015
24.049669	1026.809040	15.652032
24.045316	1024.969878	15.657050
24.385593	1031.231488	15.662067
24.205751	1029.445067	15.667085
24.276103	1029.721257	15.672103
24.224169	1025.588920	15.677120
24.254733	1029.570023	15.682138
24.194868	1021.210063	15.687155
24.153543	1039.457498	15.692173
24.445597	1043.640637	15.697191
24.709527	1047.010811	15.702208
24.606782	1056.661822	15.707226
24.623404	1054.974008	15.712243
24.579359	1050.878299	15.717261
24.719357	1046.933641	15.722279
24.817045	1045.753846	15.727296
24.615801	1053.002888	15.732314
24.705066	1052.212585	15.737331
24.789107	1057.810591	15.742349
24.817343	1046.359838	15.747367
25.112377	1042.873738	15.752384
24.840421	1030.832542	15.757402
24.950411	1028.770332	15.762419
24.734585	1026.929589	15.767437
24.529211	1023.632351	15.772455
24.938002	1019.601402	15.777472
24.717595	1028.844791	15.782490
24.871802	1039.866208	15.787507
25.126017	1045.996137	15.792525
25.022178	1042.020255	15.797543
25.002244	1035.866299	15.802560
25.094396	1037.849555	15.807578
25.128719	1031.964816	15.812595
24.955584	1024.029710	15.817613
24.834320	1030.325763	15.822631
24.964688	1040.296854	15.827648
25.175404	1042.596057	15.832666
25.372991	1047.428328	15.837683
25.555519	1044.338560	15.842701
25.006748	1034.960108	15.847719
24.937537	1027.551527	15.852736
25.176462	1040.112358	15.857754
25.221074	1037.798454	15.862771
25.054887	1045.887774	15.867789
25.308792	1046.226725	15.872807
25.473496	1040.529843	15.877824
25.084174	1050.995785	15.882842
25.266803	1038.299523	15.887859
25.316497	1046.553840	15.892877
25.253205	1045.686451	15.897895
25.081188	1043.636866	15.902912
25.305488	1049.544261	15.907930
25.449362	1041.906623	15.912947
25.635271	1045.519401	15.917965
24.993369	1049.290283	15.922983
25.075248	1051.303553	15.928000
25.517996	1070.191559	15.933018
25.659060	1068.604169	15.938035
25.510922	1068.163493	15.943053
25.632629	1064.682455	15.948071
25.914522	1066.752753	15.953088
25.850418	1070.502540	15.958106
25.856443	1068.851099	15.963123
25.998631	1064.801950	15.968141
25.982206	1070.863836	15.973159
25.894014	1069.359704	15.978176
25.954283	1066.721443	15.983194
25.863801	1065.309191	15.988211
25.973860	1068.454164	15.993229
25.878700	1072.978851	15.998247
26.014165	1056.941578	16.003264
25.941847	1065.151903	16.008282
25.776286	1055.318914	16.013299
25.766288	1061.562831	16.018317
25.831054	1074.081544	16.023335
26.145917	1063.639934	16.028352
26.008194	1068.016651	16.033370
26.046992	1063.011691	16.038387
26.079546	1064.082772	16.043405
25.739306	1071.274703	16.048423
26.079467	1074.140622	16.053440
25.575310	1060.589406	16.058458
25.933547	1069.404476	16.063475
26.350871	1079.302226	16.068493
26.104666	1089.486984	16.073511
26.605083	1084.728435	16.078528
26.275366	1091.388538	16.083546
26.551949	1089.331778	16.088563
26.402030	1080.058072	16.093581
26.395281	1093.269673	16.098599
26.403979	1087.982237	16.103616
26.361609	1090.365282	16.108634
26.614630	1079.226435	16.113651
26.554400	1084.843898	16.118669
26.332218	1092.506502	16.123687
26.756505	1083.777159	16.128704
26.685659	1085.410410	16.133722
26.764890	1083.103698	16.138739
26.462724	1093.221486	16.143757
26.834801	1087.823465	16.148775
26.751814	1089.588009	16.153792
26.811028	1087.991351	16.158810
26.718290	1084.250411	16.163827
26.736278	1088.807868	16.168845
26.887301	1089.743621	16.173863
26.603461	1078.597370	16.178880
26.851484	1086.003258	16.183898
26.875452	1085.652384	16.188915
26.709348	1084.384526	16.193933
26.555655	1085.863495	16.198951
26.709347	1077.826663	16.203968
26.667720	1080.222214	16.208986
26.381524	1086.610402	16.214003
26.771217	1093.640638	16.219021
26.809067	1104.850743	16.224039
27.660114	1105.395944	16.229056
27.170896	1113.251878	16.234074
27.350740	1110.405523	16.239091
27.280588	1107.014498	16.244109
27.370703	1118.847600	16.249127
27.434197	1109.332152	16.254144
27.645313	1088.609135	16.259162
27.162166	1077.270043	16.264179
27.163010	1086.194767	16.269197
27.090697	1086.272398	16.274215
27.449670	1089.987460	16.279232
27.525344	1102.062661	16.284250
27.054013	1097.655182	16.289267
27.376243	1093.000291	16.294285
27.062383	1109.406437	16.299303
27.012279	1093.063684	16.304320
27.154546	1100.612383	16.309338
27.263924	1103.624922	16.314355
27.427702	1101.705759	16.319373
27.291111	1104.671627	16.324391
27.563370	1106.137510	16.329408
27.841869	1122.693861	16.334426
27.815653	1132.522275	16.339443
27.779833	1105.775466	16.344461
27.861080	1101.363462	16.349479
27.840125	1095.752458	16.354496
27.599894	1103.604091	16.359514
27.461885	1108.337477	16.364531
28.020801	1113.750642	16.369549
27.806540	1123.090948	16.374567
28.131358	1129.506498	16.379584
28.136601	1128.350649	16.384602
27.994828	1121.161687	16.389619
28.094986	1108.847535	16.394637
27.859001	1118.891850	16.399655
28.155495	1115.916761	16.404672
28.122250	1116.079792	16.409690
27.664152	1121.106335	16.414707
27.920657	1120.741118	16.419725
28.191814	1135.098978	16.424743
27.883273	1131.246669	16.429760
28.071448	1130.118964	16.434778
28.033608	1133.059897	16.439795
28.378455	1119.508163	16.444813
28.235356	1125.015543	16.449831
28.132910	1122.737291	16.454848
28.248074	1124.224634	16.459866
28.112870	1129.544581	16.464883
28.229490	1127.263565	16.469901
28.588504	1124.704723	16.474919
28.413623	1121.109193	16.479936
28.303708	1128.640610	16.484954
27.941903	1128.943485	16.489971
28.543055	1139.222732	16.494989
28.891022	1155.553628	16.500007
28.737601	1149.218571	16.505024
28.751588	1144.252190	16.510042
28.479263	1138.708960	16.515059
28.834852	1120.131366	16.520077
28.740080	1124.517146	16.525095
28.849496	1116.342063	16.530112
28.632417	1112.295543	16.535130
28.208774	1117.872123	16.540147
28.965531	1120.644375	16.545165
28.927470	1149.245878	16.550183
29.068969	1132.686871	16.555200
28.767580	1123.717748	16.560218
28.826772	1138.408630	16.565235
28.956472	1140.531186	16.570253
29.166167	1141.675506	16.575271
29.126911	1142.959820	16.580288
28.816479	1119.377192	16.585306
28.758408	1131.148311	16.590323
29.218428	1141.370775	16.595341
29.099129	1152.280475	16.600359
29.103934	1149.007090	16.605376
29.237256	1147.307295	16.610394
28.908780	1148.696886	16.615411
29.427354	1134.568796	16.620429
28.965158	1149.496017	16.625447
29.049417	1143.546611	16.630464
29.241752	1134.743130	16.635482
29.098308	1135.381031	16.640499
29.223351	1142.758873	16.645517
29.308809	1141.038174	16.650535
29.501754	1139.777175	16.655552
29.655605	1136.130136	16.660570
29.524108	1143.223116	16.665587
29.198186	1129.031680	16.670605
29.421128	1140.443187	16.675623
29.278809	1140.541255	16.680640
29.574486	1132.365385	16.685658
29.472862	1135.066996	16.690675
29.427166	1137.690416	16.695693
29.783600	1144.997290	16.700711
29.519894	1155.124866	16.705728
29.593778	1144.708342	16.710746
29.430372	1157.486932	16.715763
29.759411	1156.962022	16.720781
29.508020	1157.206571	16.725799
29.649589	1159.529246	16.730816
29.996998	1151.973285	16.735834
30.079628	1153.345803	16.740851
30.017977	1152.399255	16.745869
29.710113	1161.078886	16.750887
29.941819	1162.014625	16.755904
29.817043	1153.529070	16.760922
29.794277	1159.449965	16.765939
29.632570	1151.304722	16.770957
30.140503	1163.589957	16.775975
30.171544	1167.261738	16.780992
30.201186	1167.320240	16.786010
30.456306	1180.203690	16.791027
30.371266	1167.902735	16.796045
29.870371	1162.338503	16.801063
30.009851	1169.054512	16.806080
30.501408	1167.715165	16.811098
30.474664	1174.110072	16.816115
30.462080	1172.915986	16.821133
30.546686	1170.337015	16.826151
30.532692	1175.382357	16.831168
30.704017	1174.405617	16.836186
30.554271	1172.472451	16.841203
30.528419	1148.444398	16.846221
30.607679	1146.510070	16.851239
30.493449	1147.493698	16.856256
30.366183	1152.108644	16.861274
30.204400	1171.044136	16.866291
30.712097	1165.426023	16.871309
30.931192	1163.801152	16.876327
30.529030	1172.997351	16.881344
30.961807	1171.029722	16.886362
30.454100	1172.674621	16.891379
30.982386	1169.265564	16.896397
30.444062	1169.094308	16.901415
30.329174	1169.042906	16.906432
30.756670	1172.295957	16.911450
30.689438	1173.748763	16.916467
30.523996	1163.669535	16.921485
30.444942	1172.310166	16.926503
30.937396	1195.255312	16.931520
31.213474	1200.848522	16.936538
31.307183	1203.999236	16.941555
31.138515	1196.524115	16.946573
31.630611	1193.471028	16.951591
31.075131	1181.231148	16.956608
31.273210	1176.330592	16.961626
31.056845	1168.926073	16.966643
31.394843	1188.105179	16.971661
31.151420	1189.935897	16.976679
31.332149	1191.738030	16.981696
31.451137	1178.098558	16.986714
31.286816	1199.117370	16.991731
31.045486	1195.693186	16.996749
31.402977	1184.862964	17.001767
31.347049	1186.575939	17.006784
31.607653	1186.143804	17.011802
31.374936	1184.513980	17.016819
31.444091	1185.907547	17.021837
31.287741	1189.914816	17.026855
31.178938	1190.301130	17.031872
31.578452	1185.618327	17.036890
31.489905	1189.734897	17.041907
31.537638	1194.432892	17.046925
31.826390	1198.616584	17.051943
31.558088	1213.229448	17.056960
31.785200	1207.541670	17.061978
31.999094	1218.459169	17.066995
31.996576	1212.949383	17.072013
31.929508	1211.937407	17.077031
32.085139	1209.864870	17.082048
32.308499	1207.194723	17.087066
31.959691	1210.553632	17.092083
32.127775	1200.886044	17.097101
31.844801	1193.974804	17.102119
31.859403	1212.784871	17.107136
32.248191	1204.764799	17.112154
32.337721	1214.351054	17.117171
31.940537	1216.789708	17.122189
32.162135	1209.307084	17.127207
32.158022	1212.331111	17.132224
32.319048	1206.521141	17.137242
32.159282	1201.114894	17.142259
32.260541	1203.273472	17.147277
32.290269	1206.793985	17.152295
31.859235	1214.524078	17.157312
32.371599	1208.128868	17.162330
32.103815	1205.459932	17.167347
32.113148	1203.391382	17.172365
32.293822	1219.625469	17.177383
32.484861	1220.684351	17.182400
32.363473	1222.518043	17.187418
32.451644	1232.899810	17.192435
32.700551	1228.720290	17.197453
33.074221	1227.427812	17.202471
32.705112	1232.061735	17.207488
32.844598	1225.090604	17.212506
32.286530	1221.652924	17.217523
32.084555	1219.235615	17.222541
32.835752	1220.121523	17.227559
32.477769	1225.586860	17.232576
32.967349	1224.793791	17.237594
32.805856	1221.133024	17.242611
32.582107	1220.798868	17.247629
32.793666	1238.097984	17.252647
33.024224	1255.230033	17.257664
33.080753	1253.665340	17.262682
33.146087	1248.167004	17.267699
33.074101	1253.142557	17.272717
33.196687	1256.676933	17.277735
33.290644	1255.273639	17.282752
33.231514	1253.985852	17.287770
33.408380	1254.542012	17.292787
33.476308	1246.635311	17.297805
33.667936	1250.793206	17.302823
33.562573	1249.642056	17.307840
33.545309	1243.487610	17.312858
33.559198	1237.864789	17.317875
33.100446	1233.275419	17.322893
33.591569	1233.675040	17.327911
33.391101	1241.492101	17.332928
33.758127	1238.316586	17.337946
33.778779	1243.959298	17.342963
33.752217	1244.219116	17.347981
33.711899	1237.153071	17.352999
33.710872	1245.544819	17.358016
33.418591	1237.580946	17.363034
33.944054	1236.839060	17.368051
33.723459	1240.881653	17.373069
33.766664	1239.035018	17.378087
33.775996	1243.593870	17.383104
33.555631	1243.543215	17.388122
33.560890	1235.516945	17.393139
33.525951	1247.401285	17.398157
33.572410	1246.955363	17.403175
33.497029	1249.315197	17.408192
34.011806	1259.260898	17.413210
34.140046	1267.518790	17.418227
34.250112	1259.971567	17.423245
34.423475	1269.244905	17.428263
33.895648	1263.236721	17.433280
34.150256	1261.123423	17.438298
34.266949	1263.835031	17.443315
34.522609	1275.648612	17.448333
34.063139	1251.331741	17.453351
34.110277	1263.847038	17.458368
34.243794	1261.976782	17.463386
34.313207	1267.129007	17.468403
34.532840	1259.308988	17.473421
34.411237	1259.432213	17.478439
33.780151	1272.287316	17.483456
33.947845	1264.472277	17.488474
34.229222	1277.856631	17.493491
34.033460	1288.229265	17.498509
34.658634	1288.762524	17.503527
34.792539	1291.458816	17.508544
35.019965	1294.127832	17.513562
35.176863	1293.159658	17.518579
34.926613	1291.535726	17.523597
35.114813	1286.737677	17.528615
35.119621	1293.717839	17.533632
35.206974	1272.824644	17.538650
34.899296	1262.947533	17.543667
34.371993	1261.445910	17.548685
34.936773	1266.927634	17.553703
35.041605	1285.881437	17.558720
35.120970	1280.535533	17.563738
35.109447	1285.340669	17.568755
34.771536	1291.260489	17.573773
35.063903	1286.515549	17.578791
34.931301	1294.315688	17.583808
35.247687	1282.996367	17.588826
35.215538	1273.697796	17.593843
35.422316	1281.116540	17.598861
35.100730	1283.025787	17.603879
35.016020	1285.235604	17.608896
34.801621	1279.661162	17.613914
34.905440	1283.757081	17.618931
34.846508	1303.872691	17.623949
35.074325	1301.271263	17.628967
35.106075	1306.732368	17.633984
35.290594	1311.648812	17.639002
35.489182	1306.378898	17.644019
35.238341	1309.141786	17.649037
35.927526	1318.662548	17.654055
35.795546	1326.285871	17.659072
35.899971	1326.178016	17.664090
35.860179	1307.586434	17.669107
35.908950	1310.636907	17.674125
35.816394	1301.609727	17.679143
36.117521	1313.116396	17.684160
35.614035	1296.244867	17.689178
36.253776	1300.354656	17.694195
36.072253	1313.451788	17.699213
35.928308	1307.175152	17.704231
35.757210	1309.038732	17.709248
35.850532	1323.440387	17.714266
36.339213	1322.114103	17.719283
36.065963	1316.687731	17.724301
36.318298	1324.897804	17.729319
36.439019	1331.096086	17.734336
36.038781	1330.221513	17.739354
36.200863	1320.595828	17.744371
36.244850	1323.170509	17.749389
36.687095	1317.041876	17.754407
36.531868	1320.932229	17.759424
36.565209	1331.761317	17.764442
36.811815	1326.638514	17.769459
36.773599	1328.405534	17.774477
36.535179	1319.360172	17.779495
36.572459	1325.517875	17.784512
36.617990	1323.935964	17.789530
36.755566	1317.583657	17.794547
36.625324	1328.141715	17.799565
36.757999	1324.538983	17.804583
36.762091	1323.976615	17.809600
36.580778	1331.522460	17.814618
36.884808	1318.630247	17.819635
36.433676	1323.576857	17.824653
36.613273	1317.820748	17.829671
36.693554	1324.751226	17.834688
36.467458	1328.460172	17.839706
36.804295	1330.105312	17.844723
37.086132	1347.920563	17.849741
37.276892	1342.708672	17.854759
37.170450	1343.498578	17.859776
37.245456	1347.513816	17.864794
37.292769	1343.864492	17.869811
37.506048	1343.414521	17.874829
37.072413	1318.279282	17.879847
37.582946	1321.557222	17.884864
37.177794	1323.880368	17.889882
37.293732	1317.632441	17.894899
37.027263	1328.136102	17.899917
37.446388	1330.421625	17.904935
37.477712	1341.651837	17.909952
37.157633	1345.883616	17.914970
37.617935	1340.405423	17.919987
37.086958	1344.739676	17.925005
37.322657	1352.242284	17.930023
37.621305	1347.123945	17.935040
37.588782	1340.924518	17.940058
37.566605	1344.809809	17.945075
37.432849	1348.715739	17.950093
37.613365	1349.246083	17.955111
37.671314	1357.666515	17.960128
37.609213	1361.037336	17.965146
37.699692	1376.638732	17.970163
37.736864	1375.531516	17.975181
37.928159	1372.244651	17.980199
37.806068	1369.918951	17.985216
37.925174	1361.609689	17.990234
38.224928	1366.893117	17.995251
38.177854	1366.711165	18.000269
38.316765	1364.530772	18.005287
38.115289	1370.934190	18.010304
38.179705	1373.688721	18.015322
38.403008	1363.239191	18.020339
38.147406	1366.539342	18.025357
38.045624	1363.137444	18.030375
38.318817	1374.307690	18.035392
38.557943	1386.284887	18.040410
38.806076	1389.228395	18.045427
38.107187	1391.253576	18.050445
38.297082	1390.980844	18.055463
38.749067	1387.182898	18.060480
38.505352	1390.859902	18.065498
38.809441	1390.679736	18.070515
38.732650	1393.292286	18.075533
38.414754	1386.528459	18.080551
38.615702	1385.736422	18.085568
38.515136	1391.442356	18.090586
38.686599	1393.195466	18.095603
38.601242	1389.857265	18.100621
38.538397	1379.111718	18.105639
39.167659	1395.651238	18.110656
39.028186	1397.737100	18.115674
39.466966	1400.903215	18.120691
39.038649	1393.121538	18.125709
39.016975	1388.520454	18.130727
39.206191	1399.438774	18.135744
39.176032	1397.486847	18.140762
39.652174	1398.169698	18.145779
39.781441	1388.564898	18.150797
39.696633	1380.492712	18.155815
39.431766	1372.398247	18.160832
39.203907	1370.650874	18.165850
39.229187	1369.390880	18.170867
39.355300	1373.571693	18.175885
39.499418	1362.048930	18.180903
39.429555	1372.177816	18.185920
39.482069	1394.033921	18.190938
39.634827	1394.300361	18.195955
39.309100	1401.057786	18.200973
39.685999	1403.378338	18.205991
39.865376	1402.343517	18.211008
39.388760	1406.091731	18.216026
39.646190	1398.136336	18.221043
39.523484	1398.748905	18.226061
39.483880	1402.649563	18.231079
39.611042	1401.313642	18.236096
39.783642	1404.855992	18.241114
39.979664	1407.719301	18.246131
39.774974	1425.251081	18.251149
39.548230	1426.189233	18.256167
40.217936	1425.967563	18.261184
39.910593	1422.244396	18.266202
40.302081	1418.686305	18.271219
39.847798	1427.354290	18.276237
40.043674	1425.168121	18.281255
40.375154	1432.194989	18.286272
39.928718	1430.510260	18.291290
40.291839	1415.506862	18.296307
40.513107	1433.495797	18.301325
40.185986	1448.383167	18.306343
40.805710	1449.169762	18.311360
40.811136	1449.143692	18.316378
40.935141	1452.627390	18.321395
41.042359	1433.472977	18.326413
40.915406	1425.479961	18.331431
41.023667	1417.276518	18.336448
41.038714	1426.650486	18.341466
41.078246	1418.473591	18.346483
41.075245	1422.905029	18.351501
41.107390	1419.456890	18.356519
41.087795	1414.757638	18.361536
40.946257	1418.194568	18.366554
40.887357	1414.732291	18.371571
40.776665	1415.040008	18.376589
40.597673	1424.561146	18.381607
40.959111	1417.413148	18.386624
40.690445	1412.850755	18.391642
41.052601	1413.885996	18.396659
41.109895	1427.037315	18.401677
41.152305	1441.317648	18.406695
41.305409	1445.595239	18.411712
41.228819	1451.010244	18.416730
41.279493	1443.847806	18.421747
41.558042	1449.658468	18.426765
41.086843	1442.565173	18.431783
41.536477	1427.664980	18.436800
41.538796	1443.472760	18.441818
41.761049	1446.458204	18.446835
41.610797	1448.725649	18.451853
41.479391	1443.011915	18.456871
41.306951	1436.007519	18.461888
41.259614	1444.258287	18.466906
41.639327	1453.142769	18.471923
41.766543	1460.678200	18.476941
41.524248	1463.218856	18.481959
41.640925	1456.992856	18.486976
41.564998	1456.805955	18.491994
42.040000	1451.233903	18.497011
41.757393	1453.389537	18.502029
41.188062	1465.799581	18.507047
41.691673	1475.037064	18.512064
42.063727	1486.415963	18.517082
42.248545	1477.708170	18.522099
42.262331	1481.909763	18.527117
42.110737	1484.082745	18.532135
42.515298	1477.685395	18.537152
42.318967	1476.355969	18.542170
42.555570	1482.918018	18.547187
42.312285	1475.252489	18.552205
42.289930	1479.705908	18.557223
42.707840	1477.604871	18.562240
42.548678	1490.850114	18.567258
42.722555	1492.486086	18.572275
42.469495	1480.858211	18.577293
42.727135	1492.368654	18.582311
42.711545	1493.125397	18.587328
42.627660	1492.822972	18.592346
42.853626	1498.645045	18.597363
42.960311	1493.809217	18.602381
42.963458	1500.480437	18.607399
43.099956	1497.577693	18.612416
43.160602	1493.339242	18.617434
43.137753	1499.209766	18.622451
43.510211	1493.969363	18.627469
43.314864	1486.823363	18.632487
43.184831	1467.245316	18.637504
43.251025	1479.912420	18.642522
43.121410	1481.939940	18.647539
43.510017	1485.012941	18.652557
43.190286	1501.994749	18.657575
43.736746	1492.444455	18.662592
43.139616	1488.624659	18.667610
43.565215	1494.232407	18.672627
43.824255	1497.814883	18.677645
43.375426	1497.055216	18.682663
43.523730	1492.553711	18.687680
43.803454	1496.663146	18.692698
43.551126	1494.256845	18.697715
43.490706	1488.917000	18.702733
43.604239	1500.951823	18.707751
43.518054	1491.355477	18.712768
43.527653	1493.244416	18.717786
43.219182	1485.996214	18.722803
43.725352	1499.102505	18.727821
43.669826	1519.669126	18.732839
43.643999	1518.669606	18.737856
43.962660	1520.996142	18.742874
43.889158	1519.164607	18.747891
44.211711	1513.707944	18.752909
43.916302	1523.720768	18.757927
44.133727	1520.338259	18.762944
44.183391	1520.112745	18.767962
44.098046	1516.316904	18.772979
44.422460	1525.093316	18.777997
44.249606	1541.140077	18.783015
44.676119	1539.795115	18.788032
44.556540	1545.690278	18.793050
44.630729	1541.512813	18.798067
44.802937	1540.504356	18.803085
44.416251	1532.794995	18.808103
44.536606	1530.974113	18.813120
44.753289	1541.686235	18.818138
44.639818	1546.693617	18.823155
44.918551	1543.809608	18.828173
44.761347	1549.502373	18.833191
45.182195	1541.963146	18.838208
45.225891	1538.926606	18.843226
44.903974	1538.257511	18.848243
44.982125	1532.141668	18.853261
44.910097	1538.688974	18.858279
44.964825	1533.892836	18.863296
45.078797	1540.562486	18.868314
44.809965	1536.962656	18.873331
45.049517	1535.495501	18.878349
44.856003	1545.624923	18.883367
45.023467	1558.165756	18.888384
45.198432	1567.246485	18.893402
45.322086	1565.668092	18.898419
45.590798	1558.461979	18.903437
45.466503	1560.962069	18.908455
45.479816	1558.201698	18.913472
45.553261	1566.200057	18.918490
45.366566	1560.554911	18.923507
45.557222	1559.414168	18.928525
45.473575	1564.618863	18.933543
45.580599	1557.185606	18.938560
45.842279	1564.258178	18.943578
45.711399	1578.433221	18.948595
46.054205	1579.499907	18.953613
46.004773	1587.877308	18.958631
46.332522	1579.516320	18.963648
46.186082	1579.069052	18.968666
46.477324	1575.539261	18.973683
46.487025	1561.834565	18.978701
46.364947	1565.243226	18.983719
46.427136	1552.152040	18.988736
46.466536	1551.934445	18.993754
46.289678	1556.323723	18.998771
46.582054	1547.532769	19.003789
46.236904	1552.929919	19.008807
46.280050	1548.640545	19.013824
46.132161	1549.168698	19.018842
46.385065	1561.396331	19.023859
46.538435	1564.509358	19.028877
46.116568	1581.415720	19.033895
46.481199	1572.177910	19.038912
46.783030	1571.837143	19.043930
46.660625	1579.320211	19.048947
47.001468	1577.262797	19.053965
46.884759	1579.764857	19.058983
46.868740	1577.529813	19.064000
46.896621	1573.419559	19.069018
46.710797	1574.578538	19.074035
46.898630	1578.232150	19.079053
46.785541	1575.633599	19.084071
47.009829	1583.964957	19.089088
47.375811	1597.891745	19.094106
47.021717	1611.341197	19.099123
47.294008	1603.181402	19.104141
47.136331	1607.678146	19.109159
47.341982	1602.627958	19.114176
47.430973	1598.987831	19.119194
47.497849	1596.187503	19.124211
47.634675	1588.358223	19.129229
47.431656	1601.036033	19.134247
47.755566	1598.220681	19.139264
47.607389	1601.245253	19.144282
47.426530	1598.669941	19.149299
47.637141	1592.678498	19.154317
47.657713	1595.278978	19.159335
47.795420	1595.733982	19.164352
47.814256	1599.240498	19.169370
47.989932	1618.234050	19.174387
48.080401	1611.636542	19.179405
48.220159	1618.466292	19.184423
48.189456	1624.865136	19.189440
48.511376	1623.681731	19.194458
47.871665	1616.289702	19.199475
47.885761	1614.529644	19.204493
47.877084	1613.855653	19.209511
47.955200	1619.994435	19.214528
47.874454	1620.250124	19.219546
48.239436	1617.797583	19.224563
48.145814	1621.148144	19.229581
48.312026	1632.565700	19.234599
48.309582	1649.990268	19.239616
48.645014	1646.365172	19.244634
48.254715	1642.232054	19.249651
48.815655	1646.499447	19.254669
48.635351	1646.874882	19.259687
48.716697	1642.920347	19.264704
49.109518	1633.741208	19.269722
48.976929	1646.199720	19.274739
48.932312	1645.158953	19.279757
48.833544	1647.472008	19.284775
48.778993	1643.216855	19.289792
48.915474	1635.012048	19.294810
48.806535	1649.117433	19.299827
48.751228	1650.861915	19.304845
49.320349	1663.563967	19.309863
49.456063	1666.938569	19.314880
49.506579	1660.094824	19.319898
49.145244	1673.911551	19.324915
49.589254	1667.732028	19.329933
49.277615	1673.426937	19.334951
49.814122	1664.578741	19.339968
49.670730	1664.014222	19.344986
49.469428	1664.061569	19.350003
49.785523	1664.059412	19.355021
49.682470	1656.987250	19.360039
49.511025	1661.015924	19.365056
49.726101	1663.197754	19.370074
49.772184	1653.678433	19.375091
49.803412	1649.715968	19.380109
49.830146	1663.932659	19.385127
49.849032	1658.362576	19.390144
50.322564	1655.129275	19.395162
49.652926	1665.898282	19.400179
49.795077	1658.323773	19.405197
50.191380	1672.536219	19.410215
50.313547	1683.556742	19.415232
50.428033	1684.716015	19.420250
50.068762	1697.607733	19.425267
50.186514	1688.601059	19.430285
50.407452	1694.663839	19.435303
50.288474	1687.379553	19.440320
50.281696	1678.846856	19.445338
49.838220	1696.845527	19.450355
50.340150	1699.872407	19.455373
50.394135	1706.822933	19.460391
50.398797	1716.877218	19.465408
51.023305	1711.155423	19.470426
50.646744	1713.950694	19.475443
51.026106	1708.611311	19.480461
51.034273	1711.014925	19.485479
50.892739	1715.496543	19.490496
51.067000	1707.828614	19.495514
51.037800	1709.938262	19.500531
51.037067	1698.078196	19.505549
51.018482	1706.106816	19.510567
51.099080	1727.804284	19.515584
51.392528	1724.365643	19.520602
51.339750	1740.075013	19.525619
51.553012	1722.803585	19.530637
51.140925	1729.533636	19.535655
51.142228	1727.494687	19.540672
51.467331	1726.152978	19.545690
51.392882	1728.989284	19.550707
51.338063	1729.755339	19.555725
51.879669	1727.180431	19.560743
51.957373	1726.881089	19.565760
51.782543	1719.507705	19.570778
51.834148	1727.373850	19.575795
51.906083	1719.800848	19.580813
52.141091	1713.546751	19.585831
51.916695	1719.805553	19.590848
52.108326	1717.156083	19.595866
51.930215	1723.398165	19.600883
51.914855	1727.112048	19.605901
52.370557	1732.188104	19.610919
52.254064	1743.444884	19.615936
52.443811	1735.159098	19.620954
52.471050	1742.167480	19.625971
52.514083	1729.984936	19.630989
52.477225	1722.615181	19.636007
52.474030	1745.818585	19.641024
52.448131	1731.068390	19.646042
52.323584	1741.758352	19.651059
52.671563	1737.632625	19.656077
52.845462	1743.516587	19.661095
52.493307	1741.097488	19.666112
52.869018	1740.931347	19.671130
52.848595	1741.303826	19.676147
52.758012	1747.551140	19.681165
52.807944	1735.676798	19.686183
52.721178	1741.983476	19.691200
52.906782	1745.192476	19.696218
52.938557	1744.196543	19.701235
53.217482	1756.985157	19.706253
53.350955	1766.558512	19.711271
53.367153	1776.838255	19.716288
53.227274	1772.022047	19.721306
53.575640	1768.836741	19.726323
53.487199	1773.575159	19.731341
53.533304	1766.792029	19.736359
53.510097	1771.024734	19.741376
53.130039	1759.214590	19.746394
53.535958	1767.034708	19.751411
53.598312	1765.800438	19.756429
53.727015	1758.196434	19.761447
53.583875	1769.520525	19.766464
53.787400	1762.965212	19.771482
53.779195	1776.095490	19.776499
53.724923	1778.758219	19.781517
53.800175	1770.966911	19.786535
53.796432	1783.294871	19.791552
53.959387	1780.075492	19.796570
53.760351	1786.696440	19.801587
53.847683	1781.677363	19.806605
54.669220	1789.328225	19.811623
54.644454	1799.671207	19.816640
54.350779	1775.617998	19.821658
54.374458	1787.395676	19.826675
54.468977	1797.928264	19.831693
54.438508	1796.591763	19.836711
54.500249	1811.118687	19.841728
54.832828	1806.379935	19.846746
54.511135	1806.941638	19.851763
54.294201	1803.188445	19.856781
54.757369	1798.473419	19.861799
54.736352	1817.135059	19.866816
54.705118	1801.296819	19.871834
54.969634	1812.557067	19.876851
54.957551	1821.045498	19.881869
55.382134	1824.248630	19.886887
55.470156	1833.882795	19.891904
55.239151	1812.739028	19.896922
55.275719	1812.632334	19.901939
55.359842	1821.086755	19.906957
55.721417	1822.055836	19.911975
55.542952	1824.725406	19.916992
55.433942	1821.864231	19.922010
55.599463	1812.875259	19.927027
55.410057	1823.531247	19.932045
55.390034	1817.547460	19.937063
55.149540	1826.283132	19.942080
55.625702	1818.457395	19.947098
55.486896	1814.698271	19.952115
55.548178	1828.433122	19.957133
55.837950	1822.315585	19.962151
55.744939	1833.199488	19.967168
55.542674	1830.457071	19.972186
56.293003	1842.455474	19.977203
55.960970	1848.301966	19.982221
56.338842	1842.116967	19.987239
56.219489	1852.462175	19.992256
56.435804	1851.112252	19.997274
56.623600	1846.096353	20.002291
56.474717	1843.036281	20.007309
56.743303	1839.320628	20.012327
56.411994	1842.007835	20.017344
56.564035	1842.236523	20.022362
56.671368	1839.969497	20.027379
56.416148	1845.021261	20.032397
56.447617	1846.777415	20.037415
56.053094	1849.566052	20.042432
56.448750	1850.990573	20.047450
56.936117	1865.009013	20.052467
56.845621	1871.076463	20.057485
57.073928	1862.203869	20.062503
57.206786	1862.965773	20.067520
57.128941	1863.183139	20.072538
56.955045	1861.200029	20.077555
56.829602	1867.263484	20.082573
57.094532	1855.042933	20.087591
57.117048	1862.093131	20.092608
57.068789	1879.449356	20.097626
57.311961	1881.033479	20.102643
57.553077	1888.652238	20.107661
57.543816	1875.679314	20.112679
57.517024	1882.592069	20.117696
57.409900	1877.240489	20.122714
57.886197	1883.477934	20.127731
57.547863	1884.177955	20.132749
57.781798	1872.388311	20.137767
57.517103	1883.990312	20.142784
57.847663	1894.842606	20.147802
57.766023	1903.932150	20.152819
58.105354	1901.518306	20.157837
58.534700	1900.340145	20.162855
58.352967	1905.478250	20.167872
58.358706	1904.186565	20.172890
58.230249	1900.031298	20.177907
58.076811	1913.348544	20.182925
58.703859	1906.228171	20.187943
58.436095	1907.292703	20.192960
58.491907	1902.259595	20.197978
58.391604	1903.787074	20.202995
58.501814	1921.844397	20.208013
58.757995	1927.125351	20.213031
58.839928	1929.274422	20.218048
58.807406	1934.180860	20.223066
58.911984	1932.507587	20.228083
58.618871	1937.243399	20.233101
59.215527	1928.496111	20.238119
59.229304	1935.923275	20.243136
59.332555	1928.783966	20.248154
59.436370	1925.217196	20.253171
59.299214	1929.054352	20.258189
59.024757	1924.265500	20.263207
59.185141	1927.478485	20.268224
59.205223	1927.213416	20.273242
59.254926	1919.435515	20.278259
59.063341	1936.580705	20.283277
59.618170	1943.515974	20.288295
59.444531	1945.929167	20.293312
59.457011	1948.256391	20.298330
59.738349	1946.192479	20.303347
59.691513	1956.425392	20.308365
59.781351	1948.751652	20.313383
59.725928	1947.728340	20.318400
59.627083	1951.467973	20.323418
60.007260	1958.427456	20.328435
59.941621	1969.714282	20.333453
60.389535	1970.313212	20.338471
60.172101	1972.461851	20.343488
60.034478	1977.444732	20.348506
60.210952	1971.780428	20.353523
60.110802	1973.639272	20.358541
60.632299	1969.435810	20.363559
60.600993	1965.281087	20.368576
60.434085	1971.332138	20.373594
60.712708	1974.274124	20.378611
60.479190	1972.464456	20.383629
60.939761	1968.485151	20.388647
60.536737	1992.531057	20.393664
60.835480	1998.840546	20.398682
60.836621	1986.437156	20.403699
60.920483	1997.555399	20.408717
60.680003	1986.370225	20.413735
60.917304	1991.155502	20.418752
60.886004	1995.326407	20.423770
60.711400	2000.308776	20.428787
60.880823	2006.610124	20.433805
61.234377	2012.314538	20.438823
61.572892	2014.963102	20.443840
61.677344	2019.532498	20.448858
61.718044	2017.790324	20.453875
61.288117	2016.336497	20.458893
61.444899	2012.862405	20.463911
61.616827	2018.216551	20.468928
61.781620	2031.853283	20.473946
61.960737	2028.814379	20.478963
62.192913	2034.020225	20.483981
62.337728	2030.967758	20.488999
62.106933	2032.045441	20.494016
62.581096	2031.245289	20.499034
62.505307	2024.566372	20.504051
62.732265	2020.330144	20.509069
62.368529	2011.752223	20.514087
62.207858	2006.822435	20.519104
62.327341	2010.613087	20.524122
62.520928	2013.050811	20.529139
62.422388	2019.170068	20.534157
62.799517	2022.405920	20.539175
62.561006	2028.654415	20.544192
62.730786	2019.494246	20.549210
62.963135	2031.195206	20.554227
62.804269	2028.427023	20.559245
62.729792	2033.018143	20.564263
63.148292	2025.977739	20.569280
62.791542	2038.910334	20.574298
63.136033	2022.987783	20.579315
62.959342	2031.928170	20.584333
63.164424	2032.325289	20.589351
63.502223	2041.970928	20.594368
63.359227	2048.718902	20.599386
63.495248	2053.636837	20.604403
63.386263	2045.161009	20.609421
63.661113	2052.449479	20.614439
63.392732	2047.252512	20.619456
63.280355	2049.836015	20.624474
63.482883	2038.240546	20.629491
63.317439	2046.061937	20.634509
63.399125	2045.929236	20.639527
63.616010	2053.075298	20.644544
63.712833	2073.546095	20.649562
63.508606	2075.992502	20.654579
63.853819	2082.569316	20.659597
63.717245	2077.326441	20.664615
64.079067	2075.698065	20.669632
64.161616	2089.445564	20.674650
64.448753	2083.277854	20.679667
64.382141	2094.583848	20.684685
64.669994	2102.375271	20.689703
64.703023	2092.463255	20.694720
64.527262	2099.326843	20.699738
64.921203	2085.192287	20.704755
64.645248	2090.651345	20.709773
64.834284	2087.872829	20.714791
64.631816	2089.580445	20.719808
64.690380	2091.657451	20.724826
64.652190	2081.605109	20.729843
64.630991	2088.229865	20.734861
65.038712	2098.909235	20.739879
65.222707	2113.909595	20.744896
65.319997	2108.863618	20.749914
65.457332	2113.295331	20.754931
65.631202	2110.282484	20.759949
65.460575	2104.738798	20.764967
65.662115	2107.307843	20.769984
65.501268	2105.931780	20.775002
65.598588	2107.453562	20.780019
65.561558	2114.317512	20.785037
65.495761	2114.160578	20.790055
65.674582	2109.796160	20.795072
65.674527	2110.260138	20.800090
66.018153	2119.377844	20.805107
66.211681	2130.491611	20.810125
66.163233	2128.769706	20.815143
66.381218	2134.362845	20.820160
66.211486	2141.137134	20.825178
66.217659	2134.274908	20.830195
66.099455	2129.909681	20.835213
66.114702	2132.690969	20.840231
66.456579	2125.214370	20.845248
66.279681	2130.500116	20.850266
66.375353	2128.263285	20.855283
66.503086	2143.777455	20.860301
66.418596	2150.222786	20.865319
67.031957	2157.707592	20.870336
66.881160	2157.819616	20.875354
67.086254	2162.262818	20.880371
67.190070	2148.656547	20.885389
66.748302	2160.384307	20.890407
67.024101	2157.447008	20.895424
66.986353	2162.114465	20.900442
67.062446	2164.406503	20.905459
67.049474	2171.680151	20.910477
67.046549	2182.373412	20.915495
67.454914	2175.527058	20.920512
67.283472	2180.802495	20.925530
67.480442	2174.345898	20.930547
67.587895	2175.269601	20.935565
67.454073	2183.114500	20.940583
67.967343	2194.336016	20.945600
67.832493	2202.099027	20.950618
67.760529	2199.951573	20.955635
68.009533	2202.724653	20.960653
68.039320	2199.510283	20.965671
68.308658	2197.530281	20.970688
68.144008	2201.403363	20.975706
68.337233	2202.010645	20.980723
68.226490	2204.098410	20.985741
68.134478	2207.843338	20.990759
68.159869	2204.872674	20.995776
68.342461	2192.115637	21.000794
68.432359	2214.042631	21.005811
68.549049	2220.863601	21.010829
68.798289	2220.815111	21.015847
68.660470	2216.771700	21.020864
68.339469	2234.287775	21.025882
68.738197	2227.695398	21.030899
68.921938	2218.627622	21.035917
68.576192	2225.991303	21.040935
68.925174	2240.012782	21.045952
68.905970	2250.131071	21.050970
69.047001	2244.181874	21.055987
69.015869	2242.883317	21.061005
68.924329	2248.676478	21.066023
69.320615	2256.378390	21.071040
69.522302	2264.221256	21.076058
69.723063	2261.731237	21.081075
69.985462	2277.265453	21.086093
69.917958	2273.892729	21.091111
69.747786	2266.789812	21.096128
69.670974	2267.066986	21.101146
70.013181	2268.136966	21.106163
70.089546	2263.046883	21.111181
70.152930	2263.826003	21.116199
70.354976	2265.394512	21.121216
70.336176	2264.441190	21.126234
70.397188	2260.344525	21.131251
70.620305	2260.814570	21.136269
70.298691	2266.296614	21.141287
70.295191	2268.519076	21.146304
70.694824	2282.785141	21.151322
70.554691	2283.794981	21.156339
70.696161	2283.384645	21.161357
70.651939	2287.743851	21.166375
71.038564	2279.502716	21.171392
71.084059	2285.918262	21.176410
70.925734	2287.183439	21.181427
71.348970	2277.121815	21.186445
70.923065	2282.541301	21.191463
71.171193	2290.282221	21.196480
71.059833	2301.724755	21.201498
71.528292	2301.045417	21.206515
71.637006	2306.292779	21.211533
71.641166	2314.788366	21.216551
71.815240	2306.675202	21.221568
71.762721	2309.457666	21.226586
71.813752	2301.168105	21.231603
72.035692	2304.636626	21.236621
71.384653	2306.061058	21.241639
71.733254	2302.257028	21.246656
71.315718	2302.909507	21.251674
71.585500	2310.309340	21.256691
71.862387	2331.717985	21.261709
71.956696	2333.069829	21.266727
72.389727	2326.935988	21.271744
72.469144	2326.860451	21.276762
72.130774	2323.306072	21.281779
72.100251	2343.449958	21.286797
72.115189	2351.123287	21.291815
72.471806	2344.543777	21.296832
72.877247	2346.989384	21.301850
72.626575	2359.151280	21.306867
72.798649	2355.895653	21.311885
72.813865	2360.662171	21.316903
72.923334	2357.346919	21.321920
72.664071	2362.746632	21.326938
72.912387	2366.053227	21.331955
73.010678	2373.123315	21.336973
73.514768	2379.432327	21.341991
73.472747	2384.946348	21.347008
73.435263	2383.096456	21.352026
73.537414	2379.668726	21.357043
73.477019	2370.837959	21.362061
73.403867	2377.903348	21.367079
73.606807	2374.055846	21.372096
73.830572	2381.787997	21.377114
73.626547	2400.270612	21.382131
74.031595	2386.620122	21.387149
73.834444	2397.766860	21.392167
74.066639	2405.100031	21.397184
74.066971	2396.881490	21.402202
74.309664	2403.528140	21.407219
74.407807	2392.295970	21.412237
74.431866	2399.686997	21.417255
74.510260	2397.383406	21.422272
74.063861	2399.526938	21.427290
74.226939	2401.439268	21.432307
74.661623	2411.035211	21.437325
74.634700	2417.992377	21.442343
74.534106	2425.213577	21.447360
74.590187	2419.864670	21.452378
74.994707	2414.328617	21.457395
75.172111	2414.739550	21.462413
74.974062	2443.286124	21.467431
75.218313	2445.109995	21.472448
75.310700	2441.330298	21.477466
75.297518	2443.462771	21.482483
75.431375	2432.206045	21.487501
75.328394	2446.550987	21.492519
75.907456	2450.863079	21.497536
75.728680	2442.145507	21.502554
75.499814	2445.103959	21.507571
75.791826	2443.328682	21.512589
75.744152	2449.459052	21.517607
75.792916	2443.994508	21.522624
76.151257	2463.055020	21.527642
76.040460	2462.248659	21.532659
76.276371	2450.398362	21.537677
76.397769	2456.577992	21.542695
76.363314	2463.204963	21.547712
76.540025	2446.194214	21.552730
76.061921	2453.376732	21.557747
76.416133	2450.767962	21.562765
76.501053	2459.784349	21.567783
76.887872	2474.267191	21.572800
77.163261	2484.364705	21.577818
77.051978	2484.101272	21.582835
76.931011	2474.560347	21.587853
77.070274	2479.856628	21.592871
76.934176	2480.910031	21.597888
76.749094	2479.884911	21.602906
77.101515	2472.308677	21.607923
77.384956	2478.488175	21.612941
77.198110	2482.487884	21.617959
77.455918	2495.255085	21.622976
77.393679	2507.425432	21.627994
77.700294	2501.677450	21.633011
77.951540	2495.076522	21.638029
77.911194	2507.499085	21.643047
77.487239	2506.211555	21.648064
78.171932	2502.364295	21.653082
77.579162	2505.212496	21.658099
77.899440	2488.598980	21.663117
77.681214	2491.865073	21.668135
78.030519	2512.542991	21.673152
78.279817	2519.671537	21.678170
78.192948	2525.520865	21.683187
77.887981	2524.404060	21.688205
77.967239	2521.017763	21.693223
78.310642	2519.509011	21.698240
78.503724	2536.029557	21.703258
78.674173	2549.075599	21.708275
78.566299	2549.048342	21.713293
78.453597	2547.560549	21.718311
78.581287	2544.365497	21.723328
78.921029	2549.112782	21.728346
78.666538	2568.253639	21.733363
79.017437	2568.858324	21.738381
79.119442	2565.941876	21.743399
79.095937	2569.695083	21.748416
79.740873	2582.521627	21.753434
79.572985	2598.196127	21.758451
80.065154	2601.874860	21.763469
80.174608	2604.155415	21.768487
80.053819	2590.833335	21.773504
80.103132	2562.253075	21.778522
79.662862	2566.863768	21.783539
80.450553	2575.306155	21.788557
80.274780	2583.659628	21.793575
79.684041	2585.854201	21.798592
80.419091	2588.412320	21.803610
80.458978	2590.656431	21.808627
80.617722	2582.220462	21.813645
80.680083	2589.327825	21.818663
80.491880	2595.821126	21.823680
80.724828	2593.755255	21.828698
80.787750	2585.416357	21.833715
80.959089	2587.494689	21.838733
80.900070	2585.313599	21.843751
80.801254	2590.896548	21.848768
81.229557	2591.694257	21.853786
81.210459	2608.011400	21.858803
81.463327	2601.807854	21.863821
81.135653	2615.525342	21.868839
81.464751	2612.923640	21.873856
81.167012	2614.870318	21.878874
81.401725	2621.461488	21.883891
81.083760	2613.835575	21.888909
81.350649	2628.974874	21.893927
81.426211	2628.066716	21.898944
81.596122	2641.766233	21.903962
81.556178	2645.900769	21.908979
81.772035	2653.650058	21.913997
81.838259	2655.811146	21.919015
82.138866	2659.100135	21.924032
82.495683	2661.562872	21.929050
82.406344	2671.708167	21.934067
82.569763	2660.339357	21.939085
82.790628	2662.990672	21.944103
82.368986	2663.255597	21.949120
82.802544	2664.664780	21.954138
82.606066	2666.324168	21.959155
83.332560	2680.245817	21.964173
82.786563	2691.703040	21.969191
82.952467	2688.407290	21.974208
83.203074	2682.241944	21.979226
83.036741	2685.181169	21.984243
83.082124	2683.703315	21.989261
83.391467	2682.136764	21.994279
83.090135	2683.781020	21.999296
83.453466	2683.910337	22.004314
83.450992	2677.453246	22.009331
83.275769	2690.048563	22.014349
83.876010	2711.482748	22.019367
83.621098	2707.722690	22.024384
83.918574	2697.825720	22.029402
83.893282	2712.846746	22.034419
83.679787	2713.691357	22.039437
84.063972	2706.962214	22.044455
84.297969	2719.695432	22.049472
84.790564	2717.629898	22.054490
84.341944	2731.650478	22.059507
84.439842	2733.317407	22.064525
84.580719	2733.046026	22.069543
84.682271	2728.046551	22.074560
84.921968	2719.761955	22.079578
85.105269	2729.350111	22.084595
84.918679	2724.484154	22.089613
84.772888	2726.526972	22.094631
85.025389	2726.626311	22.099648
85.062330	2713.172119	22.104666
84.839207	2726.428292	22.109683
85.074051	2744.312263	22.114701
85.476755	2746.086091	22.119719
85.303167	2756.475033	22.124736
85.805412	2747.300280	22.129754
85.840037	2755.153755	22.134771
85.407564	2749.275308	22.139789
85.697641	2757.814682	22.144807
85.468254	2764.999385	22.149824
86.058510	2765.796978	22.154842
86.265704	2769.716077	22.159859
85.982063	2770.177159	22.164877
86.096707	2764.863161	22.169895
85.857595	2777.386487	22.174912
86.522717	2784.093342	22.179930
86.225400	2789.028874	22.184947
86.620069	2797.043734	22.189965
86.449066	2797.556605	22.194983
86.306991	2800.290053	22.200000
86.967637	2815.096386	22.205018
86.861517	2819.247642	22.210035
86.776155	2823.783858	22.215053
86.861105	2823.344491	22.220071
87.221940	2817.149205	22.225088
87.382864	2815.482804	22.230106
87.394181	2818.428936	22.235123
87.213167	2831.908990	22.240141
87.643214	2830.957909	22.245159
87.596015	2841.049353	22.250176
87.694950	2835.728327	22.255194
87.755302	2838.306974	22.260211
87.930062	2845.740853	22.265229
87.913328	2835.094521	22.270247
87.760857	2850.921478	22.275264
88.037446	2865.705963	22.280282
88.422464	2869.515162	22.285299
88.264391	2873.027551	22.290317
88.677154	2868.380116	22.295335
88.212849	2866.931602	22.300352
88.765551	2851.995151	22.305370
88.625813	2851.972885	22.310387
88.524569	2865.184815	22.315405
89.009978	2876.657308	22.320423
89.079804	2887.225966	22.325440
88.809665	2890.604418	22.330458
88.916960	2884.385708	22.335475
89.205143	2881.118109	22.340493
89.054155	2878.796738	22.345511
89.075473	2884.616608	22.350528
89.234632	2885.200846	22.355546
89.368692	2898.997706	22.360563
89.180782	2901.678382	22.365581
89.538152	2903.064803	22.370599
89.671443	2896.592676	22.375616
89.853858	2906.250502	22.380634
90.011513	2922.669642	22.385651
90.065627	2934.733674	22.390669
90.486256	2927.402217	22.395687
90.345911	2926.455278	22.400704
90.321828	2917.037812	22.405722
90.654476	2916.988880	22.410739
90.544606	2923.290121	22.415757
90.564089	2916.747444	22.420775
90.493778	2920.896269	22.425792
90.638131	2935.060820	22.430810
91.040280	2946.947241	22.435827
91.007119	2949.272277	22.440845
91.192110	2946.513202	22.445863
91.114670	2941.828926	22.450880
91.385993	2945.349803	22.455898
91.483184	2952.502352	22.460915
91.024133	2952.290241	22.465933
91.640806	2947.323624	22.470951
91.477431	2968.704163	22.475968
91.537370	2974.675822	22.480986
91.458798	2966.270543	22.486003
91.492737	2969.512995	22.491021
92.114591	2976.422387	22.496039
92.045891	2986.542531	22.501056
92.159857	2992.426826	22.506074
92.370330	2991.724761	22.511091
92.102150	3002.292787	22.516109
92.263978	2994.550510	22.521127
92.387022	2992.968934	22.526144
92.408639	3006.316373	22.531162
93.024028	3009.272049	22.536179
92.913881	3017.836376	22.541197
92.858146	3014.638417	22.546215
92.796678	3026.329247	22.551232
93.032342	3021.854706	22.556250
93.121463	3024.836025	22.561267
92.899836	3028.026997	22.566285
93.287058	3035.784321	22.571303
93.481720	3048.321937	22.576320
93.257257	3051.412358	22.581338
93.462118	3044.193565	22.586355
93.520935	3053.479462	22.591373
93.730822	3056.946861	22.596391
93.824810	3071.362439	22.601408
93.869670	3069.010360	22.606426
93.937539	3073.235415	22.611443
94.009864	3072.823270	22.616461
94.237565	3086.630853	22.621479
94.143189	3089.306370	22.626496
94.500500	3098.952679	22.631514
94.553862	3100.762338	22.636531
94.346099	3091.616588	22.641549
94.825820	3085.632990	22.646567
94.964764	3105.063118	22.651584
95.159131	3107.289402	22.656602
95.233761	3113.599679	22.661619
95.418191	3109.404579	22.666637
95.544241	3107.374336	22.671655
95.459125	3108.205164	22.676672
95.625541	3102.409521	22.681690
95.865444	3109.561867	22.686707
95.519727	3119.763361	22.691725
96.062534	3104.989221	22.696743
95.953050	3108.588730	22.701760
96.153969	3104.555172	22.706778
95.929674	3108.371511	22.711795
96.237785	3109.525792	22.716813
96.150947	3106.102284	22.721831
96.142795	3107.795332	22.726848
96.130246	3104.811526	22.731866
96.532966	3105.531206	22.736883
96.322302	3125.486408	22.741901
96.751333	3125.965248	22.746919
96.332818	3135.736283	22.751936
96.652400	3139.177044	22.756954
96.996392	3129.717581	22.761971
96.922870	3146.270988	22.766989
96.966769	3158.456707	22.772007
96.991769	3160.763190	22.777024
96.961779	3150.970934	22.782042
97.060856	3162.267419	22.787059
97.539535	3170.995222	22.792077
97.502797	3172.134098	22.797095
97.574986	3177.769343	22.802112
97.877950	3177.463093	22.807130
97.909366	3174.421888	22.812147
97.625957	3173.099663	22.817165
97.503093	3188.278402	22.822183
97.918997	3202.829869	22.827200
98.100861	3208.261721	22.832218
98.187146	3200.458599	22.837235
98.529519	3211.988435	22.842253
98.484226	3213.772530	22.847271
98.783922	3215.089106	22.852288
98.591444	3220.046204	22.857306
98.943941	3222.446573	22.862323
98.824746	3218.526268	22.867341
99.159390	3227.557571	22.872359
99.484387	3238.992304	22.877376
98.984054	3241.557851	22.882394
99.523891	3239.585859	22.887411
99.099395	3245.911256	22.892429
99.038216	3237.563094	22.897447
99.623789	3248.881258	22.902464
99.190752	3260.529453	22.907482
99.759573	3261.522961	22.912499
99.657245	3270.903655	22.917517
99.695403	3272.336961	22.922535
100.173515	3294.400136	22.927552
100.040244	3286.132684	22.932570
100.245224	3290.020682	22.937587
100.419078	3295.655817	22.942605
100.595276	3302.161717	22.947623
100.839489	3317.595525	22.952640
100.925441	3317.089708	22.957658
101.009742	3317.960284	22.962675
100.867696	3322.537068	22.967693
100.833961	3315.529143	22.972711
101.149545	3315.650167	22.977728
101.043788	3323.336507	22.982746
101.536313	3333.469918	22.987763
101.264476	3345.553729	22.992781
101.425310	3339.601071	22.997799
101.383003	3340.756611	23.002816
101.358561	3339.109736	23.007834
102.030029	3346.702724	23.012851
101.902134	3364.454765	23.017869
101.921969	3358.492628	23.022887
102.255016	3363.673590	23.027904
102.395228	3359.624237	23.032922
102.086907	3358.296431	23.037939
101.955258	3363.458665	23.042957
102.235569	3368.063978	23.047975
102.582269	3387.203045	23.052992
102.802789	3394.440605	23.058010
102.714739	3384.240689	23.063027
103.019305	3383.312397	23.068045
103.023253	3375.130720	23.073063
103.452426	3389.680259	23.078080
103.333918	3412.174774	23.083098
103.710105	3395.008786	23.088115
103.635352	3409.956077	23.093133
103.716628	3399.562341	23.098151
104.073704	3409.073133	23.103168
103.837353	3405.338426	23.108186
103.859015	3403.848448	23.113203
104.059989	3405.066879	23.118221
104.072788	3395.858013	23.123239
104.193963	3414.278089	23.128256
104.088657	3425.976046	23.133274
104.269573	3424.549493	23.138291
104.441848	3436.342844	23.143309
104.664184	3432.896086	23.148327
104.768687	3428.003270	23.153344
104.317153	3449.041298	23.158362
104.813636	3450.207122	23.163379
104.788303	3458.679462	23.168397
104.732715	3451.334028	23.173415
105.010405	3466.961566	23.178432
105.129330	3476.200388	23.183450
105.368400	3481.620204	23.188467
105.462306	3490.010751	23.193485
105.280597	3489.026074	23.198503
105.442016	3502.648669	23.203520
105.664344	3509.270513	23.208538
106.059166	3507.226524	23.213555
106.045327	3510.883722	23.218573
105.874571	3532.035672	23.223591
106.732306	3529.963344	23.228608
106.437738	3528.696497	23.233626
106.618616	3528.204209	23.238643
106.322765	3532.069723	23.243661
106.471726	3528.063150	23.248679
106.794219	3537.475270	23.253696
106.919172	3553.477163	23.258714
107.004690	3549.780375	23.263731
106.972317	3552.234773	23.268749
107.243149	3553.789464	23.273767
107.428478	3560.862164	23.278784
107.549409	3578.278738	23.283802
107.910972	3575.195211	23.288819
107.999638	3573.543218	23.293837
107.939394	3572.084997	23.298855
108.123269	3576.506624	23.303872
108.079292	3579.076472	23.308890
108.107076	3571.329700	23.313907
108.181685	3566.574095	23.318925
108.285704	3580.827537	23.323943
108.504539	3588.239036	23.328960
108.481698	3600.706953	23.333978
108.570612	3593.641829	23.338995
108.520507	3596.278922	23.344013
108.480084	3598.368455	23.349031
108.831710	3600.838451	23.354048
108.899258	3616.833612	23.359066
109.238665	3615.732565	23.364083
109.363524	3616.530519	23.369101
109.400072	3623.541332	23.374119
109.757820	3625.742084	23.379136
109.330960	3621.570043	23.384154
109.830585	3633.369051	23.389171
109.905669	3638.142309	23.394189
109.600548	3642.577437	23.399207
109.725819	3640.200061	23.404224
109.752516	3641.467906	23.409242
109.979477	3654.013508	23.414259
110.209389	3655.527274	23.419277
109.975240	3666.402831	23.424295
110.611835	3666.830232	23.429312
110.520348	3684.024524	23.434330
110.783223	3685.896107	23.439347
110.715560	3686.872574	23.444365
111.095041	3692.867004	23.449383
111.427875	3689.737458	23.454400
111.508987	3695.286245	23.459418
111.160739	3691.250219	23.464435
111.476266	3705.202332	23.469453
111.831002	3717.926809	23.474471
111.940713	3711.391803	23.479488
111.837392	3718.683386	23.484506
112.208560	3710.945883	23.489523
112.244950	3707.796494	23.494541
112.101587	3714.564084	23.499559
112.005572	3713.872134	23.504576
111.856695	3725.252007	23.509594
112.271680	3734.864371	23.514611
112.431315	3741.805444	23.519629
112.498298	3758.933947	23.524647
112.919402	3766.361176	23.529664
112.101730	3774.272871	23.534682
112.396952	3769.612060	23.539699
112.686144	3780.860209	23.544717
112.748695	3787.182082	23.549735
113.139220	3797.609495	23.554752
113.242671	3815.142665	23.559770
113.415655	3813.348030	23.564787
113.762332	3816.323849	23.569805
113.551347	3833.464408	23.574823
113.670830	3833.900232	23.579840
114.039515	3837.121959	23.584858
114.237206	3840.866026	23.589875
114.372927	3848.811454	23.594893
114.663852	3842.702526	23.599911
114.640350	3857.774725	23.604928
115.051066	3870.591543	23.609946
114.797260	3876.082384	23.614963
115.071209	3865.651882	23.619981
115.122747	3870.482548	23.624999
115.416706	3865.790347	23.630016
115.344384	3867.742872	23.635034
115.326168	3858.342934	23.640051
115.511947	3863.676524	23.645069
115.347486	3858.323868	23.650087
115.765623	3870.202083	23.655104
115.846819	3885.633509	23.660122
115.817459	3881.418068	23.665139
116.084003	3880.454677	23.670157
115.812587	3884.600509	23.675175
116.291330	3898.640831	23.680192
116.211096	3905.297597	23.685210
116.371570	3909.284236	23.690227
116.787141	3916.248407	23.695245
116.178448	3913.926014	23.700263
116.647243	3909.376854	23.705280
116.271896	3919.321459	23.710298
116.883091	3927.826861	23.715315
117.357148	3938.844138	23.720333
117.068024	3931.572973	23.725351
117.203241	3928.771046	23.730368
117.401069	3940.371341	23.735386
117.198292	3955.200258	23.740403
117.420156	3952.084897	23.745421
117.473445	3966.457063	23.750439
117.854532	3973.114176	23.755456
117.935397	3980.017179	23.760474
117.841328	3984.835968	23.765491
118.391281	3985.403208	23.770509
118.246829	4004.389461	23.775527
118.438919	4012.073618	23.780544
118.671309	4023.832684	23.785562
118.898266	4005.190212	23.790579
118.798466	4012.916944	23.795597
118.867816	4033.441616	23.800615
119.577641	4031.799583	23.805632
119.528664	4027.899665	23.810650
119.538621	4038.276367	23.815667
119.639474	4027.655100	23.820685
119.520381	4029.277235	23.825703
119.673704	4028.754531	23.830720
119.589061	4039.736301	23.835738
119.893805	4044.921894	23.840755
120.288177	4050.892016	23.845773
120.150314	4059.262323	23.850791
120.337565	4061.019538	23.855808
120.490462	4073.753793	23.860826
120.471430	4079.027998	23.865843
120.860194	4083.815358	23.870861
121.011882	4083.570673	23.875879
121.071598	4074.186822	23.880896
121.023583	4080.977486	23.885914
120.935054	4096.309426	23.890931
121.316820	4100.766463	23.895949
121.278960	4111.838796	23.900967
121.791266	4103.258349	23.905984
121.393702	4110.359457	23.911002
121.336405	4130.796762	23.916019
121.693286	4137.129461	23.921037
121.664703	4138.841588	23.926055
121.715724	4141.500794	23.931072
122.170409	4156.005922	23.936090
121.999263	4166.789840	23.941107
122.498812	4169.830148	23.946125
122.816663	4180.670034	23.951143
123.019715	4182.263808	23.956160
123.019781	4186.547092	23.961178
122.991034	4187.517489	23.966195
123.570283	4190.677884	23.971213
123.170427	4192.735417	23.976231
123.504460	4200.507892	23.981248
123.811852	4202.975433	23.986266
123.772766	4208.372762	23.991283
124.015659	4200.206936	23.996301
124.286970	4204.488763	24.001319
123.906084	4201.104802	24.006336
124.213159	4204.421472	24.011354
124.354133	4204.440447	24.016371
124.746377	4201.857037	24.021389
124.269552	4205.599536	24.026407
124.283574	4215.757909	24.031424
124.620636	4226.029812	24.036442
124.053455	4227.232919	24.041459
124.496349	4233.255472	24.046477
124.525336	4254.111830	24.051495
125.088349	4252.546440	24.056512
125.321052	4254.287083	24.061530
125.168246	4272.009194	24.066547
125.412693	4279.985125	24.071565
125.137284	4281.612833	24.076583
125.563694	4287.249745	24.081600
125.863580	4298.963694	24.086618
125.817403	4305.924603	24.091635
125.804145	4302.003247	24.096653
126.140623	4314.090247	24.101671
126.436110	4331.824251	24.106688
126.407284	4324.609997	24.111706
126.515000	4324.861447	24.116723
126.425754	4341.623577	24.121741
126.810622	4348.879963	24.126759
126.607958	4348.495090	24.131776
127.035842	4359.317845	24.136794
127.122849	4371.264049	24.141811
127.707207	4361.879923	24.146829
127.493098	4378.181867	24.151847
127.738453	4380.283534	24.156864
127.973898	4375.691907	24.161882
127.847468	4395.827853	24.166899
128.151889	4392.061877	24.171917
128.159852	4405.144187	24.176935
128.069666	4399.407272	24.181952
128.238497	4411.075540	24.186970
128.532725	4416.793174	24.191987
128.604357	4415.655122	24.197005
128.525865	4425.875453	24.202023
128.735777	4440.062477	24.207040
128.705861	4442.298814	24.212058
129.298131	4450.886342	24.217075
129.462833	4467.608803	24.222093
129.542218	4474.701615	24.227111
129.679388	4479.986186	24.232128
130.067319	4474.502615	24.237146
129.885726	4471.740770	24.242163
130.120176	4472.565784	24.247181
130.462808	4494.171867	24.252199
130.306620	4495.556806	24.257216
130.582108	4497.060348	24.262234
130.493697	4505.306323	24.267251
130.490293	4490.443029	24.272269
130.484071	4508.372828	24.277287
130.464626	4526.446757	24.282304
130.887337	4528.388083	24.287322
130.657875	4539.676926	24.292339
131.251473	4547.973896	24.297357
131.330656	4558.037027	24.302375
131.502109	4567.249237	24.307392
131.660555	4571.040638	24.312410
131.662410	4578.805344	24.317427
131.788581	4578.504677	24.322445
131.971420	4592.102641	24.327463
132.101444	4605.907748	24.332480
132.389700	4603.908744	24.337498
132.246207	4611.118596	24.342515
132.614030	4614.855108	24.347533
132.663000	4625.257598	24.352551
132.841557	4631.170186	24.357568
133.074335	4623.157269	24.362586
133.052599	4641.749338	24.367603
133.488921	4639.360979	24.372621
133.558406	4655.353595	24.377639
133.815366	4656.074083	24.382656
134.565046	4651.603841	24.387674
133.998420	4661.900779	24.392691
134.257603	4653.044081	24.397709
134.100104	4652.980401	24.402727
134.240806	4655.912875	24.407744
134.429165	4649.920755	24.412762
134.159601	4661.001313	24.417779
134.443380	4667.961171	24.422797
134.634516	4682.078726	24.427815
134.731466	4680.775709	24.432832
134.890248	4682.190229	24.437850
134.919555	4707.541927	24.442867
134.833714	4708.290871	24.447885
135.157692	4709.486966	24.452903
135.143640	4721.477641	24.457920
135.701764	4723.981730	24.462938
135.582868	4727.541997	24.467955
135.825573	4738.173034	24.472973
135.678444	4750.727500	24.477991
136.057571	4751.968618	24.483008
136.117484	4753.960494	24.488026
135.970227	4773.184728	24.493043
136.481528	4780.591932	24.498061
136.707407	4786.386678	24.503079
136.888139	4799.076047	24.508096
136.813819	4807.575629	24.513114
136.684729	4818.050317	24.518131
137.457676	4821.171010	24.523149
137.565316	4826.933789	24.528167
137.519238	4825.564786	24.533184
137.615163	4835.511812	24.538202
137.815496	4840.221572	24.543219
138.249939	4851.236143	24.548237
138.331968	4850.910823	24.553255
138.153775	4858.441862	24.558272
138.435583	4852.034156	24.563290
138.570968	4875.014690	24.568307
138.659061	4880.951001	24.573325
138.936238	4881.242199	24.578343
138.584578	4879.649603	24.583360
139.076785	4890.191136	24.588378
139.225526	4902.711979	24.593395
139.415358	4907.044617	24.598413
139.639524	4906.435033	24.603431
139.880127	4918.714224	24.608448
139.949762	4922.649031	24.613466
140.163521	4933.231056	24.618483
140.140299	4937.259328	24.623501
140.242196	4933.768026	24.628519
139.772740	4935.953336	24.633536
140.238751	4941.151802	24.638554
140.251181	4956.421300	24.643571
140.622081	4971.997656	24.648589
141.329152	4977.098391	24.653607
141.134145	4985.531737	24.658624
141.278146	4984.653776	24.663642
141.104182	4984.576892	24.668659
141.375123	5005.257315	24.673677
141.365269	4999.229847	24.678695
141.502896	5013.668542	24.683712
141.785805	5023.460114	24.688730
142.290301	5035.742233	24.693747
142.261258	5040.506921	24.698765
142.338183	5033.070641	24.703783
142.338455	5028.174786	24.708800
142.706730	5037.889860	24.713818
142.686482	5051.794606	24.718835
142.686482	5062.413352	24.723853
142.916841	5050.281296	24.728871
142.931490	5069.240577	24.733888
143.750224	5080.280309	24.738906
143.535192	5088.981993	24.743923
143.087469	5083.398729	24.748941
143.769204	5080.163782	24.753959
143.892966	5103.730393	24.758976
144.152164	5110.482781	24.763994
144.104388	5109.941048	24.769011
144.128433	5103.478939	24.774029
144.070432	5111.840373	24.779047
144.416419	5128.285670	24.784064
144.515117	5131.837179	24.789082
144.652435	5149.678833	24.794099
144.690832	5155.572514	24.799117
145.189131	5156.526681	24.804135
145.032695	5164.796237	24.809152
145.376777	5180.137072	24.814170
145.391588	5191.716334	24.819187
145.449189	5187.644797	24.824205
145.882600	5197.763266	24.829223
145.634926	5219.993002	24.834240
146.153906	5214.447644	24.839258
146.363390	5218.625761	24.844275
146.569649	5242.940368	24.849293
146.440225	5240.596374	24.854311
146.715694	5243.255300	24.859328
146.830831	5254.992498	24.864346
146.497091	5273.990789	24.869363
146.422741	5264.576823	24.874381
147.108887	5285.479768	24.879399
147.252096	5288.976985	24.884416
147.544007	5308.155075	24.889434
147.706895	5322.337528	24.894451
147.645258	5325.778460	24.899469
148.053352	5328.801729	24.904487
148.307957	5340.258289	24.909504
148.461794	5347.522862	24.914522
148.746802	5346.079854	24.919539
148.422945	5342.311103	24.924557
148.980708	5362.937528	24.929575
148.839588	5375.213697	24.934592
149.437374	5369.476019	24.939610
149.475165	5375.300421	24.944627
149.780128	5393.403302	24.949645
149.941718	5395.641320	24.954663
150.016171	5399.143017	24.959680
150.186387	5396.108106	24.964698
150.116153	5394.285133	24.969715
150.142367	5407.011760	24.974733
150.484616	5408.072461	24.979751
150.663546	5428.669925	24.984768
150.654264	5421.284873	24.989786
151.062817	5421.050436	24.994803
150.913102	5420.360519	24.999821
151.212274	5440.213132	25.004839
150.947635	5443.534369	25.009856
151.236009	5445.847230	25.014874
151.682967	5453.706722	25.019891
151.381728	5470.989224	25.024909
151.298108	5469.847020	25.029927
151.719485	5483.531389	25.034944
151.789198	5492.665308	25.039962
152.209980	5496.848265	25.044979
152.381876	5527.242032	25.049997
152.862520	5527.188857	25.055015
152.654338	5535.858112	25.060032
152.698701	5528.540372	25.065050
152.807866	5528.062426	25.070067
152.826042	5546.598658	25.075085
153.036190	5551.600635	25.080103
153.001927	5550.763202	25.085120
153.197808	5570.183893	25.090138
153.564516	5565.539839	25.095155
153.711525	5583.901248	25.100173
154.262877	5590.219774	25.105191
154.218383	5603.427959	25.110208
154.246732	5606.965329	25.115226
154.289576	5599.262685	25.120243
154.636841	5624.954115	25.125261
155.100417	5613.069250	25.130279
155.060707	5618.845894	25.135296
155.048043	5634.047288	25.140314
155.430694	5648.211349	25.145331
154.880494	5652.480171	25.150349
155.332969	5663.653401	25.155367
155.607986	5670.877021	25.160384
155.942945	5677.983926	25.165402
156.386340	5684.439353	25.170419
156.107168	5708.685423	25.175437
156.676777	5705.237498	25.180455
156.443499	5714.472660	25.185472
156.506098	5718.162520	25.190490
156.571523	5718.553197	25.195507
156.686656	5733.305342	25.200525
156.934385	5746.777205	25.205543
157.265928	5754.089860	25.210560
157.500299	5763.482221	25.215578
157.798531	5775.184756	25.220595
157.449068	5786.878285	25.225613
157.862529	5790.118604	25.230631
158.162480	5798.383237	25.235648
158.224761	5811.050830	25.240666
158.553903	5804.351274	25.245683
158.277581	5806.850507	25.250701
158.600015	5830.462692	25.255719
159.057175	5833.566748	25.260736
159.121075	5833.588332	25.265754
159.664779	5852.882227	25.270771
159.727223	5872.709263	25.275789
160.074358	5865.530201	25.280807
160.180952	5873.196974	25.285824
160.055631	5866.265548	25.290842
160.117923	5869.074763	25.295859
159.928503	5878.486226	25.300877
160.190375	5888.704560	25.305895
160.365805	5900.922019	25.310912
160.041033	5911.989885	25.315930
160.704370	5918.511953	25.320947
160.552607	5933.880596	25.325965
160.992753	5943.218715	25.330983
161.094703	5946.485768	25.336000
161.065193	5965.225612	25.341018
161.428942	5977.221058	25.346035
161.601009	5991.891887	25.351053
161.950140	5995.057090	25.356071
162.262828	5997.110518	25.361088
162.583869	6004.058737	25.366106
162.715784	6014.556354	25.371123
162.699138	6032.801800	25.376141
162.793377	6019.626606	25.381159
162.710196	6021.659979	25.386176
163.069097	6038.012529	25.391194
163.393527	6046.314477	25.396211
163.280725	6056.686305	25.401229
163.360020	6044.526751	25.406247
163.801876	6060.724271	25.411264
163.868935	6067.904867	25.416282
164.178552	6070.331280	25.421299
163.924148	6080.737933	25.426317
164.038908	6093.463792	25.431335
164.577489	6094.373822	25.436352
164.609005	6112.539196	25.441370
165.036483	6113.441378	25.446387
164.641138	6125.549531	25.451405
164.809108	6127.672997	25.456423
165.180627	6137.618595	25.461440
165.262137	6159.314914	25.466458
165.072477	6163.849358	25.471475
165.230972	6179.791484	25.476493
165.474862	6181.713657	25.481511
166.077412	6195.212339	25.486528
165.554582	6213.761396	25.491546
165.929596	6227.841870	25.496563
166.608024	6243.576326	25.501581
166.773043	6254.813894	25.506599
167.000250	6261.448607	25.511616
167.006133	6273.563449	25.516634
167.713905	6282.376827	25.521651
167.632608	6300.957817	25.526669
167.695823	6289.735029	25.531687
168.117161	6291.594689	25.536704
168.011318	6302.587453	25.541722
168.375915	6309.494241	25.546739
168.521605	6315.118944	25.551757
168.560593	6321.552721	25.556775
168.389836	6330.409051	25.561792
168.652491	6343.146639	25.566810
168.720845	6347.312401	25.571827
168.972137	6359.679278	25.576845
168.966893	6380.360333	25.581863
169.620256	6390.637574	25.586880
169.634059	6399.105148	25.591898
169.675658	6399.032366	25.596915
170.047346	6417.643526	25.601933
170.251791	6428.957101	25.606951
170.328255	6417.331245	25.611968
170.107076	6444.684972	25.616986
170.626704	6458.083194	25.622003
170.647466	6472.307746	25.627021
170.950530	6480.591142	25.632039
171.304027	6481.476522	25.637056
171.640517	6488.785541	25.642074
171.727655	6505.862958	25.647091
171.834733	6508.725235	25.652109
171.941311	6515.580976	25.657127
172.090872	6520.955746	25.662144
171.842947	6539.556768	25.667162
172.049544	6543.577800	25.672180
172.369704	6555.529947	25.677197
172.480198	6563.752000	25.682215
172.981952	6579.545993	25.687232
172.865734	6589.681894	25.692250
173.107592	6589.486190	25.697268
173.352550	6616.243110	25.702285
173.715531	6617.205933	25.707303
173.800201	6628.525769	25.712320
173.925363	6639.283663	25.717338
174.469509	6644.091557	25.722356
174.604177	6647.173670	25.727373
174.486378	6650.415295	25.732391
174.837227	6653.615070	25.737408
174.934423	6668.118230	25.742426
175.244781	6660.329036	25.747444
175.658319	6664.990084	25.752461
175.228645	6674.060770	25.757479
175.593455	6689.551156	25.762496
175.642878	6697.789151	25.767514
176.223417	6695.485273	25.772532
176.340391	6695.886837	25.777549
175.957359	6714.976417	25.782567
176.042477	6720.484460	25.787584
175.926880	6737.928481	25.792602
176.185901	6745.338131	25.797620
176.821076	6759.318278	25.802637
176.509522	6781.537813	25.807655
177.195952	6792.896065	25.812672
177.108242	6806.115042	25.817690
177.481209	6799.310397	25.822708
177.692067	6811.289304	25.827725
177.819821	6833.339059	25.832743
178.108517	6835.516303	25.837760
178.202995	6853.959823	25.842778
178.747336	6859.045551	25.847796
178.359220	6864.766677	25.852813
178.577393	6876.877071	25.857831
178.925749	6881.441053	25.862848
178.868491	6890.863896	25.867866
179.334874	6910.698223	25.872884
179.616798	6924.500227	25.877901
179.594632	6940.310314	25.882919
179.795577	6943.887198	25.887936
179.747492	6954.426179	25.892954
180.228664	6962.656636	25.897972
180.195627	6980.744588	25.902989
180.245312	6988.887966	25.908007
180.794112	7001.322317	25.913024
180.727859	7024.027761	25.918042
181.165479	7030.172037	25.923060
181.367207	7039.885860	25.928077
181.442055	7059.308148	25.933095
181.483928	7069.814161	25.938112
181.916205	7077.237844	25.943130
181.929332	7082.138516	25.948148
182.544607	7098.098274	25.953165
182.409817	7110.500887	25.958183
182.863216	7110.976033	25.963200
183.034060	7118.080799	25.968218
183.202809	7137.715758	25.973236
183.114606	7141.862030	25.978253
183.268706	7143.738390	25.983271
183.660120	7152.895348	25.988288
183.793985	7166.581824	25.993306
183.845408	7180.022356	25.998324
184.218456	7190.621775	26.003341
184.373664	7194.347935	26.008359
184.584237	7193.652016	26.013376
184.741160	7219.830102	26.018394
184.804406	7226.737094	26.023412
185.168112	7238.057788	26.028429
184.963780	7248.368859	26.033447
185.442350	7247.924550	26.038464
185.324213	7261.884190	26.043482
185.460318	7272.160883	26.048500
186.007337	7277.707225	26.053517
186.499764	7299.179509	26.058535
186.590065	7302.672774	26.063552
186.422498	7310.250506	26.068570
186.384227	7317.201848	26.073588
186.664380	7324.728387	26.078605
187.085839	7329.852440	26.083623
187.161100	7353.372716	26.088640
187.020927	7355.573013	26.093658
187.537285	7363.627662	26.098676
188.003424	7381.855637	26.103693
187.721965	7387.484448	26.108711
188.043766	7395.140241	26.113728
188.392159	7412.073391	26.118746
188.452801	7410.286539	26.123764
188.600584	7423.522734	26.128781
188.694410	7436.865258	26.133799
188.967002	7446.044135	26.138816
189.130380	7455.899936	26.143834
189.324866	7466.637982	26.148852
189.601179	7483.137354	26.153869
189.425278	7496.042314	26.158887
189.642838	7508.121649	26.163904
190.014283	7533.287905	26.168922
189.850332	7541.114567	26.173940
190.541753	7550.076345	26.178957
190.684989	7565.778975	26.183975
191.276404	7578.393306	26.188992
191.713921	7586.075249	26.194010
191.629293	7586.912514	26.199028
191.739710	7598.093161	26.204045
191.838375	7608.606369	26.209063
192.105577	7608.681347	26.214080
191.828536	7617.870647	26.219098
192.103872	7633.549482	26.224116
192.434717	7656.929080	26.229133
192.931174	7665.242699	26.234151
192.546023	7664.333858	26.239168
193.158462	7687.318951	26.244186
193.102514	7700.745114	26.249204
193.240945	7706.380852	26.254221
193.413464	7733.684284	26.259239
193.558697	7731.918876	26.264256
194.224197	7753.819191	26.269274
194.445615	7762.258024	26.274292
194.829625	7767.662730	26.279309
194.810432	7778.166085	26.284327
194.973959	7782.812918	26.289344
195.220678	7798.834181	26.294362
195.519645	7803.627124	26.299380
195.460030	7801.496014	26.304397
195.344794	7823.117776	26.309415
195.644010	7831.048796	26.314432
195.833315	7850.880189	26.319450
195.824860	7863.010951	26.324468
196.560331	7874.829439	26.329485
196.583811	7885.979681	26.334503
196.692487	7899.149732	26.339520
196.985889	7924.489758	26.344538
197.143847	7927.656835	26.349556
197.206361	7932.827819	26.354573
197.605674	7947.638248	26.359591
197.921268	7955.121609	26.364608
197.778326	7981.455092	26.369626
198.354822	7990.154111	26.374644
198.776891	7993.469250	26.379661
198.939547	8004.998709	26.384679
198.645650	8006.380224	26.389696
199.108640	8032.887208	26.394714
199.203578	8034.820285	26.399732
199.800956	8027.860066	26.404749
199.633335	8057.986028	26.409767
199.359874	8061.703749	26.414784
199.925428	8070.477134	26.419802
200.122744	8084.350090	26.424820
200.388803	8085.236623	26.429837
200.539757	8103.700959	26.434855
200.658083	8104.209686	26.439872
201.113475	8109.770636	26.444890
200.966241	8122.223233	26.449908
201.380909	8138.212165	26.454925
201.344501	8154.694830	26.459943
201.634614	8157.961214	26.464960
202.201701	8163.255271	26.469978
201.891887	8169.078186	26.474996
202.236848	8191.215506	26.480013
202.224700	8201.105517	26.485031
202.700627	8212.879642	26.490048
203.006005	8211.720524	26.495066
203.086486	8243.639047	26.500084
203.130961	8247.884751	26.505101
203.169484	8264.674644	26.510119
203.564582	8280.240554	26.515136
203.852727	8288.947002	26.520154
203.568689	8312.095416	26.525172
204.243519	8325.675905	26.530189
204.406725	8338.253655	26.535207
204.665251	8349.727269	26.540224
204.822275	8359.909734	26.545242
204.862562	8380.873197	26.550260
204.977285	8391.801078	26.555277
205.037391	8410.137881	26.560295
205.523622	8425.064520	26.565312
206.012073	8439.832966	26.570330
205.969580	8453.721668	26.575348
206.493295	8470.697782	26.580365
206.533697	8483.733715	26.585383
206.818029	8503.926624	26.590400
207.141755	8518.922997	26.595418
207.030435	8532.484723	26.600436
207.480146	8538.529741	26.605453
207.449749	8554.112025	26.610471
207.650553	8561.452599	26.615488
208.033857	8577.307910	26.620506
208.317439	8595.796160	26.625524
208.560872	8600.670628	26.630541
208.703633	8614.571472	26.635559
209.064328	8635.001978	26.640576
209.367863	8631.772009	26.645594
209.218687	8652.159280	26.650612
209.732164	8650.696017	26.655629
209.674980	8680.275280	26.660647
209.900690	8680.167332	26.665664
210.274486	8696.864050	26.670682
210.268229	8710.160027	26.675700
210.608784	8716.111702	26.680717
210.494935	8739.647580	26.685735
211.018047	8750.154931	26.690752
210.920866	8757.684340	26.695770
211.201193	8777.770829	26.700788
211.786909	8782.231801	26.705805
211.763398	8809.712762	26.710823
212.006453	8825.192447	26.715840
212.738817	8835.010364	26.720858
212.639809	8850.897266	26.725876
212.821092	8862.421185	26.730893
212.757417	8861.338787	26.735911
213.146384	8880.865327	26.740928
213.361161	8881.879908	26.745946
213.309846	8903.998073	26.750964
213.707022	8906.679517	26.755981
213.935249	8928.716031	26.760999
214.053779	8938.244982	26.766016
214.358046	8948.969850	26.771034
214.367430	8962.645584	26.776052
214.661100	8957.983716	26.781069
215.405196	8980.940324	26.786087
215.234407	8997.694211	26.791104
215.437422	9000.630250	26.796122
215.758321	9017.673370	26.801140
215.837190	9021.380287	26.806157
215.925575	9046.062527	26.811175
215.989684	9053.405767	26.816192
216.466797	9077.427272	26.821210
216.790187	9085.212969	26.826228
217.021867	9086.660617	26.831245
217.171488	9103.111822	26.836263
216.939199	9113.005233	26.841280
217.744585	9125.072471	26.846298
217.613718	9140.064788	26.851316
218.026350	9153.570144	26.856333
218.449655	9163.701864	26.861351
218.390576	9189.578746	26.866368
218.844608	9196.235817	26.871386
218.929955	9207.314016	26.876404
218.889583	9215.459852	26.881421
218.927311	9232.137082	26.886439
219.576542	9249.103720	26.891456
219.750636	9257.904267	26.896474
219.827565	9283.466345	26.901492
219.625534	9291.028181	26.906509
220.366857	9307.803637	26.911527
220.584178	9333.912105	26.916544
220.962146	9340.596930	26.921562
221.071121	9353.199652	26.926580
221.494046	9372.876098	26.931597
221.674316	9383.876385	26.936615
221.356922	9396.880605	26.941632
221.887846	9412.789282	26.946650
221.955980	9435.833404	26.951668
222.506918	9446.592537	26.956685
223.040988	9458.996128	26.961703
223.239672	9479.812881	26.966720
223.471373	9484.869388	26.971738
223.524671	9490.519008	26.976756
223.422480	9504.632545	26.981773
224.078687	9509.177372	26.986791
224.135955	9527.853558	26.991808
224.305735	9532.240950	26.996826
224.436788	9547.116787	27.001844
224.874889	9554.000654	27.006861
225.044975	9568.901968	27.011879
224.988626	9591.883693	27.016896
225.328042	9598.884072	27.021914
225.438186	9616.642746	27.026932
225.660335	9630.967629	27.031949
225.748477	9641.812004	27.036967
226.080797	9665.361247	27.041984
226.394754	9679.851755	27.047002
226.625776	9693.976382	27.052020
227.146627	9709.523794	27.057037
227.287903	9712.302278	27.062055
227.322199	9741.411076	27.067072
227.508741	9747.579811	27.072090
227.853683	9775.844339	27.077108
227.743577	9780.537699	27.082125
228.065583	9789.204818	27.087143
228.316690	9817.935615	27.092160
228.455264	9818.845364	27.097178
228.517225	9836.056094	27.102196
228.845081	9858.914813	27.107213
229.500908	9867.037120	27.112231
229.264956	9889.573738	27.117248
229.766092	9895.143851	27.122266
229.932016	9913.670790	27.127284
230.295018	9929.786188	27.132301
230.638744	9942.519876	27.137319
230.663628	9963.923258	27.142336
230.698010	9974.460507	27.147354
231.190137	9988.857039	27.152372
231.406918	9996.602986	27.157389
231.458824	10009.533991	27.162407
231.838871	10031.787993	27.167424
232.322994	10039.732042	27.172442
232.385280	10057.792273	27.177460
232.256821	10069.873809	27.182477
232.567295	10078.088200	27.187495
232.805633	10100.917035	27.192512
233.055081	10112.225817	27.197530
233.353792	10133.697007	27.202548
233.590113	10160.349894	27.207565
233.934510	10177.744030	27.212583
234.027630	10190.836049	27.217600
234.229062	10202.114518	27.222618
234.489830	10228.015354	27.227636
234.858972	10242.993376	27.232653
235.058303	10261.685930	27.237671
235.290781	10279.981784	27.242688
235.683731	10297.412630	27.247706
235.690093	10305.583195	27.252724
236.005917	10333.916279	27.257741
236.487384	10349.975593	27.262759
236.692475	10359.719050	27.267776
236.874729	10378.976427	27.272794
237.289316	10376.461301	27.277812
237.445542	10405.413102	27.282829
237.712824	10407.811997	27.287847
237.901174	10421.725994	27.292864
238.268268	10435.893017	27.297882
238.627284	10455.305918	27.302900
238.795014	10477.941037	27.307917
238.979798	10473.741060	27.312935
239.270225	10491.260770	27.317952
239.364493	10505.912636	27.322970
239.628581	10514.276574	27.327988
239.520404	10534.141645	27.333005
240.196706	10553.381801	27.338023
240.076232	10564.461473	27.343040
240.472986	10580.723708	27.348058
240.551077	10594.140430	27.353076
240.561269	10612.837704	27.358093
240.826912	10627.080758	27.363111
241.127680	10646.389311	27.368128
241.368539	10671.261369	27.373146
241.937767	10689.842726	27.378164
242.084123	10703.454073	27.383181
242.419593	10713.486728	27.388199
242.321152	10740.407596	27.393216
242.678085	10755.871047	27.398234
243.323885	10778.794756	27.403252
243.211520	10796.548360	27.408269
243.801106	10801.599683	27.413287
244.015281	10820.792521	27.418304
244.232110	10827.187371	27.423322
244.621884	10837.956771	27.428340
244.747934	10857.949685	27.433357
245.234207	10862.515157	27.438375
245.396274	10876.162059	27.443392
245.366799	10881.547200	27.448410
245.747633	10894.152579	27.453428
245.725742	10911.756343	27.458445
245.920506	10916.926385	27.463463
246.142036	10925.906586	27.468480
246.236349	10934.913035	27.473498
246.454178	10953.650747	27.478516
246.499054	10977.227728	27.483533
247.210438	10999.961453	27.488551
247.175579	11018.467261	27.493568
247.090067	11031.935186	27.498586
247.386425	11048.103039	27.503604
247.343557	11069.145701	27.508621
248.155214	11100.174645	27.513639
248.785940	11116.268073	27.518656
249.101895	11134.115936	27.523674
249.376602	11146.946514	27.528692
249.083396	11168.397944	27.533709
249.304544	11178.578221	27.538727
249.754910	11198.921711	27.543744
250.145774	11211.601517	27.548762
250.556075	11227.773778	27.553780
250.303246	11255.556341	27.558797
250.760084	11267.881668	27.563815
251.148637	11287.540258	27.568832
251.207002	11295.696793	27.573850
251.598476	11316.362242	27.578868
251.821548	11345.595526	27.583885
252.024700	11357.752249	27.588903
252.205300	11381.633714	27.593920
252.432603	11397.699011	27.598938
252.985143	11423.407384	27.603956
253.084999	11451.719153	27.608973
253.428746	11451.229574	27.613991
253.629440	11476.437389	27.619008
253.762971	11496.243508	27.624026
254.121407	11516.235454	27.629044
254.364319	11529.118639	27.634061
254.774337	11546.945844	27.639079
254.978917	11560.962348	27.644096
255.136280	11589.382150	27.649114
255.352380	11602.399051	27.654132
255.868112	11629.629164	27.659149
256.186631	11632.102292	27.664167
256.397107	11659.149755	27.669184
256.699771	11677.499133	27.674202
257.099315	11683.973016	27.679220
257.374990	11703.236065	27.684237
257.165626	11715.328175	27.689255
257.497361	11732.457334	27.694272
257.866787	11751.667855	27.699290
258.499825	11760.208224	27.704308
258.077085	11776.647239	27.709325
258.719182	11789.111248	27.714343
258.881526	11806.506997	27.719360
258.913513	11833.402681	27.724378
259.825938	11843.171887	27.729396
260.077138	11866.455570	27.734413
260.244878	11873.490015	27.739431
260.576888	11895.002216	27.744448
260.383190	11907.208831	27.749466
260.779757	11911.523365	27.754484
260.919846	11942.191559	27.759501
260.935598	11950.200324	27.764519
261.380533	11972.904342	27.769536
261.755734	11988.069119	27.774554
261.942697	12004.166516	27.779572
261.945151	12023.791628	27.784589
262.041904	12043.341990	27.789607
262.448964	12056.420867	27.794624
262.363875	12081.655313	27.799642
263.103196	12095.500030	27.804660
263.347324	12122.025012	27.809677
263.633799	12136.183846	27.814695
263.869784	12158.453469	27.819712
264.302093	12166.406544	27.824730
264.683048	12184.627315	27.829748
264.530235	12203.004347	27.834765
264.830884	12221.559828	27.839783
265.043556	12243.166909	27.844800
265.425115	12260.610840	27.849818
265.848731	12279.964985	27.854836
266.215637	12302.751096	27.859853
266.128154	12312.869812	27.864871
266.934853	12328.943033	27.869888
266.676355	12351.757702	27.874906
267.296458	12361.405609	27.879924
267.510675	12380.783187	27.884941
267.790469	12402.111520	27.889959
268.126721	12421.586863	27.894976
268.286697	12433.678414	27.899994
268.521517	12448.660296	27.905012
268.473775	12475.806222	27.910029
268.778601	12493.297125	27.915047
269.434883	12509.564587	27.920064
269.627158	12528.105768	27.925082
269.954978	12542.624741	27.930100
270.097731	12574.613526	27.935117
270.253066	12591.711102	27.940135
270.745198	12610.372757	27.945152
270.736896	12634.178034	27.950170
270.832011	12643.747275	27.955188
271.320333	12672.600017	27.960205
271.741375	12696.916006	27.965223
272.432525	12711.305562	27.970240
272.465971	12731.008658	27.975258
272.941157	12753.614141	27.980276
272.955612	12770.853948	27.985293
273.571828	12790.241604	27.990311
273.934768	12794.454242	27.995328
273.776363	12823.146419	28.000346
274.187643	12835.113598	28.005364
274.366284	12845.838279	28.010381
274.510062	12865.511599	28.015399
274.684399	12867.296952	28.020416
275.156116	12894.712632	28.025434
275.554307	12912.530351	28.030452
275.514820	12945.849370	28.035469
275.969098	12959.780430	28.040487
276.212685	12978.648754	28.045504
276.318855	13003.563940	28.050522
276.852343	13018.297380	28.055540
277.165227	13040.672840	28.060557
277.257383	13060.660769	28.065575
277.538167	13078.967570	28.070592
277.513369	13102.596017	28.075610
278.008023	13115.822963	28.080628
278.570919	13142.801555	28.085645
278.627382	13162.912027	28.090663
278.595993	13180.462550	28.095680
278.685204	13205.699612	28.100698
279.495775	13220.771918	28.105716
279.709326	13250.284386	28.110733
279.689567	13275.390186	28.115751
280.213217	13293.984421	28.120768
280.348415	13314.777474	28.125786
280.748482	13323.730852	28.130804
280.812904	13345.902431	28.135821
281.175921	13376.954883	28.140839
281.457104	13384.632140	28.145856
281.765800	13403.200152	28.150874
282.383504	13425.664111	28.155892
282.575053	13441.834647	28.160909
282.336637	13464.679087	28.165927
282.851755	13488.795035	28.170944
283.349125	13513.311702	28.175962
283.615602	13521.945037	28.180980
283.725291	13555.453343	28.185997
283.897984	13576.379762	28.191015
284.071374	13591.634287	28.196032
284.472678	13607.974220	28.201050
284.588348	13643.433403	28.206068
285.141469	13669.242647	28.211085
285.312820	13690.074660	28.216103
285.949631	13707.520997	28.221120
285.921116	13733.873042	28.226138
286.237365	13761.961731	28.231156
286.806564	13787.083320	28.236173
286.943274	13810.428386	28.241191
287.482652	13821.791883	28.246208
287.557864	13856.203008	28.251226
287.942295	13870.562546	28.256244
288.496347	13884.687092	28.261261
288.503223	13907.029400	28.266279
289.051806	13928.241553	28.271296
288.928821	13948.134636	28.276314
289.124009	13966.029361	28.281332
289.676609	13987.556759	28.286349
290.041051	14014.940335	28.291367
290.334073	14034.278837	28.296384
290.352509	14066.033803	28.301402
290.564175	14083.291279	28.306420
291.014979	14102.106153	28.311437
290.959398	14125.232237	28.316455
291.617995	14140.663844	28.321472
291.819557	14174.282014	28.326490
292.282671	14203.153668	28.331508
292.583830	14217.141222	28.336525
292.728809	14252.849598	28.341543
293.065241	14263.496675	28.346560
293.696754	14292.019954	28.351578
293.663029	14313.380602	28.356596
294.061984	14328.256146	28.361613
294.453960	14357.088647	28.366631
294.844349	14371.548692	28.371648
294.929574	14396.427928	28.376666
295.468532	14422.802567	28.381684
295.783019	14441.607549	28.386701
295.868932	14469.392282	28.391719
296.551940	14481.624279	28.396736
296.745751	14502.289437	28.401754
296.820496	14524.375500	28.406772
296.969112	14539.975749	28.411789
297.230382	14570.619735	28.416807
297.935221	14585.858129	28.421824
297.792063	14607.561541	28.426842
297.906962	14627.888638	28.431860
298.186657	14656.142281	28.436877
298.354296	14679.928872	28.441895
298.832908	14701.594998	28.446912
298.973735	14735.773199	28.451930
299.422889	14757.500850	28.456948
300.371966	14773.980212	28.461965
300.175740	14807.001742	28.466983
300.540556	14817.625733	28.472000
300.407578	14829.240436	28.477018
300.767024	14851.888659	28.482036
301.292429	14874.798310	28.487053
301.591077	14904.325278	28.492071
301.757839	14925.162518	28.497088
301.847165	14948.270056	28.502106
302.290292	14979.495752	28.507124
302.760768	14999.903349	28.512141
302.903884	15026.299773	28.517159
303.247793	15050.068688	28.522176
303.649464	15078.385963	28.527194
304.077639	15099.930953	28.532212
304.448966	15125.372709	28.537229
304.541911	15151.729791	28.542247
305.434077	15183.842438	28.547264
305.757213	15201.863561	28.552282
305.569352	15223.495715	28.557300
306.012964	15238.788187	28.562317
306.131504	15269.822014	28.567335
306.405671	15294.391732	28.572352
306.595494	15319.843228	28.577370
306.810322	15336.166483	28.582388
307.752613	15354.735055	28.587405
307.691115	15385.835172	28.592423
308.487251	15407.341819	28.597440
308.470820	15436.063058	28.602458
309.074869	15460.117040	28.607476
309.361477	15469.231332	28.612493
309.342184	15498.111029	28.617511
309.769625	15519.865057	28.622528
309.918104	15546.033957	28.627546
310.345112	15575.507111	28.632564
310.758118	15586.108191	28.637581
310.510724	15618.065291	28.642599
311.034568	15644.150258	28.647616
311.260589	15674.915235	28.652634
311.876757	15708.139526	28.657652
312.214622	15727.763289	28.662669
312.391943	15753.615274	28.667687
312.738682	15779.251253	28.672704
313.151446	15801.908040	28.677722
313.346912	15830.644052	28.682740
314.064995	15844.987555	28.687757
313.735464	15866.121490	28.692775
314.570930	15893.140243	28.697792
314.804943	15922.697856	28.702810
314.848533	15942.895390	28.707828
315.250651	15970.155846	28.712845
315.332246	15995.896816	28.717863
315.724844	16021.222726	28.722880
316.147228	16047.769473	28.727898
316.692465	16081.403484	28.732916
316.806845	16095.301651	28.737933
317.115852	16127.920989	28.742951
317.773398	16157.842166	28.747968
318.109439	16178.139424	28.752986
318.279763	16205.370197	28.758004
318.939926	16224.713414	28.763021
319.066490	16248.066202	28.768039
319.242507	16265.624967	28.773056
319.392038	16295.272190	28.778074
319.576978	16318.104246	28.783092
320.146527	16342.948042	28.788109
320.209789	16372.608897	28.793127
320.829273	16388.130574	28.798144
321.422797	16416.192362	28.803162
321.078272	16437.319794	28.808180
321.265557	16451.611086	28.813197
321.589644	16479.560405	28.818215
321.970252	16507.488278	28.823232
322.684560	16540.152215	28.828250
322.730146	16557.861177	28.833268
323.163834	16580.240814	28.838285
323.222464	16612.960206	28.843303
323.611767	16636.136491	28.848320
323.790299	16662.586468	28.853338
324.002179	16693.408984	28.858356
324.553006	16709.702883	28.863373
324.814139	16751.405249	28.868391
324.908042	16770.948268	28.873408
325.410180	16814.198607	28.878426
325.881691	16841.218853	28.883444
326.123841	16858.385614	28.888461
326.774506	16895.068335	28.893479
326.902957	16924.719827	28.898496
327.294091	16951.954968	28.903514
327.368006	16983.219647	28.908532
328.109080	17015.908626	28.913549
328.391885	17033.116553	28.918567
328.649427	17054.611502	28.923584
328.933459	17092.697590	28.928602
328.855968	17127.732317	28.933620
329.516349	17140.080118	28.938637
329.455743	17185.011375	28.943655
330.164751	17219.771455	28.948672
330.854710	17240.617690	28.953690
330.731552	17277.504476	28.958708
331.784026	17308.212092	28.963725
331.915676	17323.978350	28.968743
332.141834	17352.168537	28.973760
332.505556	17372.813326	28.978778
332.860266	17401.848916	28.983796
333.298689	17424.655210	28.988813
333.372970	17460.330081	28.993831
333.569063	17484.861128	28.998848
334.183280	17501.587981	29.003866
334.360769	17541.492080	29.008884
334.806064	17562.762346	29.013901
335.332524	17592.106138	29.018919
335.221876	17614.884951	29.023936
335.786763	17645.511547	29.028954
335.978102	17682.551996	29.033972
336.581129	17702.622675	29.038989
337.000993	17735.590614	29.044007
337.241823	17762.490349	29.049024
337.833011	17783.984384	29.054042
337.691467	17812.466583	29.059060
338.583683	17839.447595	29.064077
338.960595	17872.056083	29.069095
339.312814	17884.907491	29.074112
339.445956	17903.055667	29.079130
339.142939	17929.086886	29.084148
339.784695	17954.995418	29.089165
340.067274	17983.822068	29.094183
340.342079	18013.212236	29.099200
341.080130	18039.421672	29.104218
340.906746	18068.642064	29.109236
341.534655	18096.138650	29.114253
341.927923	18129.231457	29.119271
341.921259	18162.393285	29.124288
342.190934	18186.635722	29.129306
342.347329	18216.297447	29.134324
342.948229	18253.508580	29.139341
343.283793	18281.701932	29.144359
343.244188	18303.036332	29.149376
343.965942	18334.675530	29.154394
344.287563	18363.142842	29.159412
344.712051	18386.470495	29.164429
345.542367	18407.586614	29.169447
345.850819	18442.272646	29.174464
346.338829	18471.510075	29.179482
345.963716	18504.698612	29.184500
346.214896	18510.496808	29.189517
346.515890	18545.759100	29.194535
347.007111	18581.421260	29.199552
347.527335	18601.682736	29.204570
347.871042	18644.222808	29.209588
348.309538	18674.017937	29.214605
348.517907	18698.649678	29.219623
348.808272	18739.119784	29.224640
349.607442	18767.544472	29.229658
349.706819	18797.146518	29.234676
350.152108	18821.716032	29.239693
350.574934	18846.895600	29.244711
350.682774	18886.762828	29.249728
351.406565	18909.248185	29.254746
351.044548	18945.341600	29.259764
351.597291	18961.175900	29.264781
352.217554	18996.117330	29.269799
352.194965	19027.520454	29.274816
352.761561	19057.403507	29.279834
352.936437	19094.436586	29.284852
353.746834	19115.430240	29.289869
354.016993	19156.296084	29.294887
354.117871	19181.829773	29.299904
354.749656	19211.942931	29.304922
355.019042	19250.717874	29.309940
355.289111	19280.420273	29.314957
355.303850	19315.097005	29.319975
356.155268	19353.193415	29.324992
356.356212	19377.492325	29.330010
356.436368	19417.712458	29.335028
357.055572	19441.958568	29.340045
357.349945	19472.301883	29.345063
358.036549	19508.623793	29.350080
358.250609	19539.024018	29.355098
358.476953	19570.976593	29.360116
359.018562	19603.770677	29.365133
359.518445	19635.023437	29.370151
359.836212	19669.754418	29.375168
360.395161	19697.422021	29.380186
360.487984	19723.873795	29.385204
360.983501	19753.162515	29.390221
361.324630	19777.787457	29.395239
361.574431	19814.431078	29.400256
362.159628	19838.000655	29.405274
362.319709	19866.748188	29.410292
362.350743	19897.739949	29.415309
362.898374	19932.429072	29.420327
363.584364	19960.816367	29.425344
364.070677	19989.260253	29.430362
363.965752	20014.050134	29.435380
364.426278	20045.897303	29.440397
364.893867	20077.749735	29.445415
364.832751	20105.060133	29.450432
365.088915	20141.191597	29.455450
365.883337	20178.824682	29.460468
365.907192	20211.972568	29.465485
366.614899	20241.696328	29.470503
366.970810	20271.462603	29.475520
367.440912	20303.656192	29.480538
367.695271	20338.695248	29.485556
367.984230	20358.489315	29.490573
368.136408	20386.354292	29.495591
368.408592	20420.859968	29.500608
368.794182	20446.514982	29.505626
368.972918	20480.574166	29.510644
369.765606	20516.356911	29.515661
370.228581	20553.183343	29.520679
370.390081	20579.537055	29.525696
371.026942	20606.460813	29.530714
370.980627	20633.927585	29.535732
371.451968	20678.650869	29.540749
371.778585	20707.929562	29.545767
372.156791	20749.438911	29.550784
372.590055	20771.188443	29.555802
372.710882	20818.728084	29.560820
373.077560	20847.324640	29.565837
373.501915	20889.680042	29.570855
374.027549	20926.680592	29.575872
374.513645	20953.685307	29.580890
375.115048	21001.023742	29.585908
375.406618	21033.606644	29.590925
375.733562	21061.603163	29.595943
375.955724	21091.688598	29.600960
376.396896	21125.474005	29.605978
376.834051	21154.022056	29.610996
376.962494	21196.614024	29.616013
377.749399	21224.974705	29.621031
377.617468	21268.005678	29.626048
377.843331	21304.181934	29.631066
378.355121	21350.265215	29.636084
378.579554	21389.089331	29.641101
379.421319	21418.016688	29.646119
379.715811	21460.614808	29.651136
380.310697	21503.462942	29.656154
380.935783	21534.737025	29.661172
380.925487	21568.101055	29.666189
381.407556	21590.993840	29.671207
381.593751	21633.072211	29.676224
382.011740	21667.430857	29.681242
382.319191	21704.031053	29.686260
382.786932	21746.166662	29.691277
383.552762	21776.686114	29.696295
383.718504	21813.637283	29.701312
384.363354	21849.515115	29.706330
384.526098	21887.326239	29.711348
384.861792	21916.485247	29.716365
385.497829	21952.225633	29.721383
385.275768	21990.286791	29.726400
386.119583	22026.525543	29.731418
386.798276	22062.398460	29.736436
386.755573	22092.912353	29.741453
387.435023	22130.276514	29.746471
387.446086	22164.604981	29.751488
388.335422	22199.756400	29.756506
388.498198	22229.157795	29.761524
388.714396	22267.561561	29.766541
389.830470	22307.277789	29.771559
389.765194	22337.113154	29.776576
389.885751	22363.804242	29.781594
390.256228	22405.002334	29.786612
390.491978	22442.209103	29.791629
391.485493	22462.179273	29.796647
391.680660	22510.103105	29.801664
392.123228	22549.312377	29.806682
392.326703	22588.546540	29.811700
392.766561	22606.625744	29.816717
392.825056	22641.383614	29.821735
392.991094	22687.612630	29.826752
393.633604	22720.313952	29.831770
394.492445	22753.986166	29.836788
394.458797	22788.657622	29.841805
395.092519	22804.254857	29.846823
395.224086	22848.549704	29.851840
395.518911	22889.248808	29.856858
396.197036	22914.766421	29.861876
396.514268	22947.487472	29.866893
397.270604	22982.762219	29.871911
397.120934	23024.845596	29.876928
397.275302	23055.020459	29.881946
398.000775	23089.497703	29.886964
397.977259	23133.457284	29.891981
398.567724	23171.564045	29.896999
398.941359	23210.121907	29.902016
399.122518	23247.749478	29.907034
400.004546	23286.708113	29.912052
400.223732	23327.729600	29.917069
400.728102	23369.723895	29.922087
401.519625	23416.033566	29.927104
401.409551	23447.659632	29.932122
402.037975	23487.391415	29.937140
402.551091	23535.887198	29.942157
403.017074	23564.939748	29.947175
403.210642	23608.594643	29.952192
403.641612	23650.070205	29.957210
404.299205	23674.309192	29.962228
404.602916	23723.609187	29.967245
404.866653	23753.919640	29.972263
405.359893	23798.924584	29.977280
405.429830	23832.437825	29.982298
406.307801	23872.504128	29.987316
406.547725	23919.609138	29.992333
407.052620	23954.804923	29.997351
407.229414	24002.463484	30.002368
407.550157	24030.345092	30.007386
408.293000	24073.636912	30.012404
408.453062	24115.572956	30.017421
408.988211	24148.735802	30.022439
409.597295	24203.430201	30.027456
409.426656	24236.893328	30.032474
410.145899	24275.146331	30.037492
410.735709	24319.568566	30.042509
410.892902	24360.393337	30.047527
411.474347	24398.206835	30.052544
411.663084	24442.761679	30.057562
412.305646	24483.201017	30.062580
412.700542	24519.344001	30.067597
413.107124	24566.380189	30.072615
413.724196	24605.768395	30.077632
413.731436	24644.967817	30.082650
414.667515	24678.549031	30.087668
414.730051	24719.806455	30.092685
415.431015	24761.678084	30.097703
415.804301	24813.643075	30.102720
416.217185	24846.377530	30.107738
416.599190	24877.265206	30.112756
417.158235	24921.364969	30.117773
417.386324	24939.485779	30.122791
417.809470	24995.393247	30.127808
417.989836	25045.354103	30.132826
418.834096	25061.729058	30.137844
419.110394	25110.221508	30.142861
419.825934	25153.816967	30.147879
419.546951	25188.499403	30.152896
420.078205	25230.803059	30.157914
420.833732	25268.963798	30.162932
420.964554	25307.936599	30.167949
421.545018	25340.493934	30.172967
422.165891	25380.262254	30.177984
422.217231	25412.434915	30.183002
422.977815	25439.213130	30.188020
422.891853	25485.557593	30.193037
423.474130	25524.782414	30.198055
424.158538	25568.566925	30.203072
424.557157	25600.527493	30.208090
424.736084	25639.032045	30.213108
424.611740	25686.324649	30.218125
425.264009	25721.146531	30.223143
425.891267	25764.232584	30.228160
426.370350	25807.898095	30.233178
426.653033	25850.286226	30.238196
427.004482	25899.280720	30.243213
427.555697	25940.900179	30.248231
428.156157	25978.701031	30.253248
428.455223	26031.375989	30.258266
429.261320	26072.127869	30.263284
429.513521	26112.732747	30.268301
429.959529	26150.817236	30.273319
430.358987	26190.337430	30.278336
430.123032	26238.312415	30.283354
430.963480	26284.482000	30.288372
431.162364	26339.417097	30.293389
432.101833	26379.030040	30.298407
431.989821	26419.642020	30.303424
432.613881	26467.242673	30.308442
433.481731	26512.390937	30.313460
433.871100	26557.968180	30.318477
434.038858	26589.915911	30.323495
434.645546	26632.223328	30.328512
435.169168	26688.808650	30.333530
435.555425	26734.190848	30.338548
436.342506	26783.694392	30.343565
436.691787	26817.143557	30.348583
437.179541	26855.949667	30.353600
437.728356	26902.002012	30.358618
437.881008	26945.108035	30.363636
438.057921	26982.098575	30.368653
438.729662	27028.410048	30.373671
439.407231	27063.925519	30.378688
439.410096	27115.094875	30.383706
440.356135	27158.146604	30.388724
440.731885	27189.866768	30.393741
440.987936	27241.869002	30.398759
441.610586	27280.787524	30.403776
441.844201	27329.898737	30.408794
442.067315	27364.885473	30.413812
442.623176	27428.578327	30.418829
443.041483	27462.371689	30.423847
443.810721	27511.639624	30.428864
443.941145	27542.235789	30.433882
444.597529	27583.747340	30.438900
445.111301	27634.174319	30.443917
445.260977	27668.250279	30.448935
445.958842	27716.986322	30.453952
446.186863	27758.021753	30.458970
446.691797	27796.789043	30.463988
447.023359	27847.940356	30.469005
447.445372	27896.404005	30.474023
447.894823	27937.759069	30.479040
448.705503	27981.939856	30.484058
448.845147	28028.374871	30.489076
449.148895	28068.545774	30.494093
449.596259	28119.224539	30.499111
450.253816	28160.572742	30.504128
450.258337	28203.508683	30.509146
450.919579	28244.774310	30.514164
451.457649	28288.625536	30.519181
451.804838	28338.315536	30.524199
452.527206	28376.866568	30.529216
452.396444	28427.112024	30.534234
453.176190	28464.440643	30.539252
453.818024	28511.126776	30.544269
454.252838	28556.941562	30.549287
454.436998	28599.395096	30.554304
454.923655	28648.842774	30.559322
455.622670	28696.639167	30.564340
456.015367	28736.727919	30.569357
456.355727	28783.171132	30.574375
456.631455	28827.570275	30.579392
456.883016	28880.247396	30.584410
457.684758	28917.320559	30.589428
457.889153	28969.651325	30.594445
458.271068	29032.813855	30.599463
458.897500	29077.139645	30.604480
459.410965	29119.479465	30.609498
460.192601	29171.081909	30.614516
460.027969	29231.435629	30.619533
460.351515	29272.320067	30.624551
461.048935	29319.922208	30.629568
461.453728	29377.829410	30.634586
462.312907	29424.527827	30.639604
462.792364	29481.778875	30.644621
463.463378	29531.869842	30.649639
463.919452	29571.842838	30.654656
464.283346	29625.661043	30.659674
464.785991	29666.537175	30.664692
465.600376	29724.665652	30.669709
465.916587	29774.458795	30.674727
466.149606	29811.976639	30.679744
466.741644	29866.233829	30.684762
467.324457	29902.097777	30.689780
467.686622	29949.747565	30.694797
467.957085	30006.640887	30.699815
468.532929	30056.236012	30.704832
469.243997	30113.022688	30.709850
469.744809	30144.525557	30.714868
470.087727	30188.904468	30.719885
470.630714	30242.746802	30.724903
470.947601	30282.635513	30.729920
471.015925	30346.856283	30.734938
471.736941	30391.049981	30.739956
472.588783	30439.667231	30.744973
473.104210	30486.946575	30.749991
473.575180	30526.097301	30.755008
473.722110	30588.852580	30.760026
474.408365	30637.249694	30.765044
474.943323	30673.754625	30.770061
474.821470	30730.148772	30.775079
475.706400	30774.532546	30.780096
475.925286	30830.702916	30.785114
476.466694	30887.309681	30.790132
477.484781	30933.398722	30.795149
477.707736	30990.005074	30.800167
478.224446	31026.393375	30.805184
478.601221	31075.288818	30.810202
478.757956	31123.156808	30.815220
479.693778	31176.554422	30.820237
479.908830	31223.477908	30.825255
480.265668	31270.265503	30.830272
480.746670	31322.381893	30.835290
481.246489	31377.144257	30.840308
481.715632	31432.417306	30.845325
481.924549	31477.047544	30.850343
483.054642	31532.065614	30.855360
483.435264	31570.075584	30.860378
483.711215	31621.611631	30.865396
484.320364	31653.118791	30.870413
484.348590	31703.284084	30.875431
484.774912	31752.306115	30.880448
485.581995	31805.080684	30.885466
485.549470	31858.916203	30.890484
486.354764	31903.491877	30.895501
486.636797	31959.800806	30.900519
487.610096	32007.523968	30.905536
487.950118	32073.193157	30.910554
488.461542	32120.211325	30.915572
489.108287	32164.825035	30.920589
489.195254	32218.775525	30.925607
490.080661	32265.128537	30.930624
490.243231	32321.488762	30.935642
490.685591	32363.960149	30.940660
491.283860	32426.056005	30.945677
491.697024	32490.286273	30.950695
492.385071	32529.451026	30.955712
492.692693	32587.521489	30.960730
493.177134	32649.111104	30.965748
493.837704	32707.246737	30.970765
494.139186	32761.746661	30.975783
494.876308	32813.548488	30.980800
495.639064	32871.295567	30.985818
496.014565	32927.314287	30.990836
496.507074	32971.498680	30.995853
497.017814	33031.504757	31.000871
497.693498	33083.651951	31.005888
498.055374	33139.717628	31.010906
498.437377	33190.027061	31.015924
499.326210	33237.759942	31.020941
499.683856	33291.582286	31.025959
499.973554	33349.316262	31.030976
500.268932	33390.763251	31.035994
501.039702	33451.810915	31.041012
501.864441	33502.842044	31.046029
502.188537	33560.994810	31.051047
502.405211	33611.375403	31.056064
502.975576	33666.366639	31.061082
503.471493	33723.272721	31.066100
503.720848	33774.287148	31.071117
504.136604	33837.035362	31.076135
505.244932	33887.435021	31.081152
505.868432	33942.235305	31.086170
506.363047	33996.619665	31.091188
506.446917	34038.998851	31.096205
506.673612	34109.630029	31.101223
507.595045	34158.023758	31.106240
508.034796	34217.582791	31.111258
508.462490	34280.475873	31.116276
509.222367	34330.596073	31.121293
509.691929	34384.751422	31.126311
509.985124	34437.025104	31.131328
510.558767	34492.365724	31.136346
510.863149	34555.481262	31.141364
511.737139	34603.453504	31.146381
512.118460	34668.043154	31.151399
512.624826	34718.886831	31.156416
513.010922	34784.000870	31.161434
513.703764	34843.307053	31.166452
514.416721	34893.031281	31.171469
514.704671	34954.525634	31.176487
515.445350	35000.667086	31.181504
515.875381	35053.135831	31.186522
516.350557	35093.742362	31.191540
516.891250	35140.882832	31.196557
517.092981	35210.901956	31.201575
517.776988	35253.410876	31.206592
518.346597	35304.227084	31.211610
519.033658	35358.635387	31.216628
519.144710	35403.023722	31.221645
519.584073	35461.916086	31.226663
520.275535	35511.177235	31.231680
521.203933	35567.849824	31.236698
521.098513	35616.616377	31.241716
521.889156	35666.595816	31.246733
521.989233	35734.008547	31.251751
522.625339	35786.642841	31.256768
522.991279	35835.114763	31.261786
523.855440	35899.645181	31.266804
524.684133	35952.192814	31.271821
524.726683	36015.948068	31.276839
525.177451	36071.558652	31.281856
525.823261	36130.951673	31.286874
526.311140	36183.275037	31.291892
527.168691	36250.773104	31.296909
527.715211	36315.683336	31.301927
528.155151	36366.180937	31.306944
528.983821	36420.740503	31.311962
529.163514	36486.220885	31.316980
529.577027	36539.435698	31.321997
529.809139	36598.439540	31.327015
530.448931	36658.758168	31.332032
531.378986	36725.721549	31.337050
531.685707	36790.234472	31.342068
532.584796	36846.282721	31.347085
532.982625	36906.665238	31.352103
533.550900	36963.031185	31.357120
534.128222	37027.236859	31.362138
534.484991	37087.670580	31.367156
534.970414	37151.170149	31.372173
535.426964	37205.771030	31.377191
535.757117	37272.722580	31.382208
536.781646	37345.806857	31.387226
537.232263	37411.854687	31.392244
537.814649	37458.671250	31.397261
538.435815	37523.725216	31.402279
538.654486	37575.562969	31.407296
539.410634	37649.253109	31.412314
539.900102	37708.333520	31.417332
540.723771	37763.788916	31.422349
541.376804	37825.563180	31.427367
541.629350	37885.737229	31.432384
542.270473	37943.049208	31.437402
542.681594	37995.964472	31.442420
543.546277	38067.356200	31.447437
543.940242	38124.587223	31.452455
544.394778	38179.190890	31.457472
545.169703	38235.091472	31.462490
545.294760	38299.725907	31.467508
545.804822	38366.728567	31.472525
546.699249	38431.597030	31.477543
546.966659	38486.705067	31.482560
547.880357	38547.548917	31.487578
548.066203	38620.054282	31.492596
548.497687	38678.564638	31.497613
549.320173	38740.321305	31.502631
549.789794	38795.645091	31.507648
550.450424	38857.079627	31.512666
550.472430	38925.937479	31.517684
551.448252	38984.515183	31.522701
552.151578	39056.371806	31.527719
552.207529	39108.776262	31.532736
552.572727	39162.928429	31.537754
553.210050	39223.419053	31.542772
553.841947	39289.836326	31.547789
554.361467	39352.546528	31.552807
554.916701	39402.982602	31.557824
555.733475	39477.080547	31.562842
556.240475	39535.050162	31.567860
556.927021	39595.711191	31.572877
557.061778	39662.182167	31.577895
557.976932	39720.644879	31.582912
558.659262	39783.963245	31.587930
559.089466	39847.441442	31.592948
559.529589	39904.372698	31.597965
559.931705	39972.807528	31.602983
560.525281	40039.827574	31.608000
561.286500	40099.061675	31.613018
561.400734	40173.366885	31.618036
562.282047	40234.827675	31.623053
563.046920	40309.486798	31.628071
563.150433	40379.089078	31.633088
563.718155	40430.967533	31.638106
564.410685	40505.866335	31.643124
564.795496	40578.283821	31.648141
565.545894	40644.193361	31.653159
565.948012	40713.509609	31.658176
566.732469	40774.753083	31.663194
567.108976	40860.144307	31.668212
568.062018	40919.666817	31.673229
568.519898	40999.214634	31.678247
569.057618	41064.406128	31.683264
570.063408	41127.336206	31.688282
570.548336	41199.309994	31.693300
570.761455	41261.479158	31.698317
571.318878	41329.716820	31.703335
572.174044	41405.415432	31.708352
572.943396	41476.561326	31.713370
573.351115	41545.000195	31.718388
573.746873	41600.064377	31.723405
574.588947	41669.390638	31.728423
574.706308	41742.821540	31.733440
575.678075	41802.912744	31.738458
575.986641	41881.045091	31.743476
576.717903	41947.809069	31.748493
577.542896	42012.313254	31.753511
577.970799	42085.418369	31.758528
578.750451	42148.873805	31.763546
578.845903	42221.544423	31.768564
579.835762	42289.008947	31.773581
580.176797	42356.663842	31.778599
581.047524	42416.544849	31.783616
581.644204	42477.499909	31.788634
582.551411	42555.749612	31.793652
583.245312	42619.049056	31.798669
583.512540	42677.425062	31.803687
583.860060	42758.274171	31.808704
584.747653	42811.683088	31.813722
585.115042	42883.238031	31.818740
585.837584	42945.224631	31.823757
586.151230	43003.587902	31.828775
586.478645	43072.999178	31.833792
587.588773	43139.663148	31.838810
587.662379	43216.167170	31.843828
588.387995	43278.242773	31.848845
589.405651	43343.378492	31.853863
589.735341	43417.256089	31.858880
590.523043	43473.288243	31.863898
591.134339	43541.087861	31.868916
591.712622	43605.249491	31.873933
592.434077	43662.601833	31.878951
592.730408	43726.466404	31.883968
593.433673	43783.764980	31.888986
593.881308	43850.496890	31.894004
594.362964	43905.996134	31.899021
595.099776	43966.313453	31.904039
595.494947	44039.158147	31.909056
595.841951	44096.222353	31.914074
596.435906	44166.158261	31.919092
597.048335	44231.088051	31.924109
597.463200	44297.782155	31.929127
598.297190	44378.567294	31.934144
598.986711	44447.749033	31.939162
599.230072	44520.252192	31.944180
599.878896	44585.942706	31.949197
600.438301	44670.124453	31.954215
600.918095	44736.885605	31.959232
601.903259	44807.122811	31.964250
602.224585	44890.488714	31.969268
602.977883	44960.130149	31.974285
603.600623	45038.142159	31.979303
604.297546	45115.712674	31.984320
605.291658	45183.096762	31.989338
606.039086	45254.213926	31.994356
606.481138	45321.672238	31.999373
606.900106	45384.921392	32.004391
607.231179	45466.390172	32.009408
607.820414	45543.055461	32.014426
608.664817	45620.047949	32.019444
609.207996	45702.009409	32.024461
610.232299	45770.592450	32.029479
610.517427	45844.491369	32.034496
611.009630	45916.719682	32.039514
611.795411	45988.573298	32.044532
612.534926	46055.632972	32.049549
613.119140	46135.084495	32.054567
613.677594	46217.608453	32.059584
614.530751	46287.870966	32.064602
615.160628	46363.267474	32.069620
615.537676	46436.217678	32.074637
616.293702	46494.299358	32.079655
617.079983	46570.772805	32.084672
617.733318	46647.937904	32.089690
618.074599	46715.466779	32.094708
618.321318	46801.249054	32.099725
619.373902	46861.828362	32.104743
619.679902	46943.325378	32.109760
620.178191	47022.730215	32.114778
620.982004	47095.046343	32.119796
621.673379	47171.846672	32.124813
622.219431	47250.928513	32.129831
622.957918	47331.922678	32.134848
623.740364	47402.832362	32.139866
624.609727	47490.518858	32.144884
624.924962	47558.066973	32.149901
625.567261	47631.207231	32.154919
626.151191	47710.885751	32.159936
626.996378	47774.049533	32.164954
627.285331	47848.074592	32.169972
628.125176	47927.935219	32.174989
628.420413	47989.825530	32.180007
629.244444	48079.242208	32.185024
629.761705	48161.494994	32.190042
630.737969	48239.127377	32.195060
631.521713	48311.368272	32.200077
632.009761	48370.369793	32.205095
632.486297	48449.397090	32.210112
633.589553	48514.072536	32.215130
633.743936	48586.242044	32.220148
634.447060	48657.440104	32.225165
634.993314	48712.612065	32.230183
635.350936	48795.771549	32.235200
636.213736	48858.960884	32.240218
636.759469	48925.692430	32.245236
637.465716	49000.959186	32.250253
638.299756	49058.864376	32.255271
638.905766	49151.716892	32.260288
639.404727	49215.520953	32.265306
640.092621	49291.278705	32.270324
640.355255	49361.807693	32.275341
641.217372	49434.773780	32.280359
641.531622	49512.501505	32.285376
642.488430	49592.507800	32.290394
643.359277	49660.683730	32.295412
643.979227	49752.922774	32.300429
644.290228	49813.145211	32.305447
644.602574	49897.910183	32.310464
645.803521	49976.418032	32.315482
646.518658	50056.919338	32.320500
647.020383	50142.256623	32.325517
647.633159	50219.281961	32.330535
647.936007	50293.249462	32.335552
648.867153	50374.470978	32.340570
649.636780	50449.802147	32.345588
650.164338	50533.884048	32.350605
651.047940	50611.361803	32.355623
651.837809	50703.267999	32.360640
652.515995	50776.235501	32.365658
653.255472	50847.567517	32.370676
653.732969	50933.367081	32.375693
654.710610	51004.858430	32.380711
655.084768	51083.980404	32.385728
655.390609	51161.639064	32.390746
656.130567	51237.395050	32.395764
656.849449	51327.644402	32.400781
657.710997	51403.192063	32.405799
658.097611	51480.788520	32.410816
659.009808	51568.705333	32.415834
659.690758	51649.280802	32.420852
660.310275	51739.072748	32.425869
661.244156	51808.947247	32.430887
661.632489	51887.411666	32.435904
661.957233	51968.246505	32.440922
663.204389	52050.639301	32.445940
663.303574	52133.547533	32.450957
664.569779	52207.667661	32.455975
665.052910	52302.849002	32.460992
665.767925	52376.030897	32.466010
666.385189	52459.865259	32.471028
667.020983	52536.451731	32.476045
667.768748	52616.418939	32.481063
668.462068	52703.418809	32.486080
669.059595	52782.353368	32.491098
669.917628	52858.615010	32.496116
670.153446	52942.339984	32.501133
671.256186	53019.873698	32.506151
671.774908	53114.894567	32.511168
671.926460	53186.585256	32.516186
673.300348	53263.779900	32.521204
673.690219	53342.008489	32.526221
674.458280	53427.765385	32.531239
675.387547	53512.162135	32.536256
675.829429	53596.825355	32.541274
676.591452	53676.661052	32.546292
677.301126	53760.188167	32.551309
677.710306	53821.266205	32.556327
678.220423	53889.143984	32.561344
678.872335	53970.896359	32.566362
679.718644	54036.171669	32.571380
680.036973	54126.475550	32.576397
681.005138	54196.402423	32.581415
681.663529	54282.160617	32.586432
682.716895	54361.212602	32.591450
683.360008	54444.296927	32.596468
683.548156	54523.674800	32.601485
684.381565	54595.705967	32.606503
685.104968	54674.785360	32.611520
685.775509	54757.720937	32.616538
686.276145	54841.392190	32.621556
687.093605	54921.324664	32.626573
687.582132	55006.700736	32.631591
688.302129	55091.332079	32.636608
688.640346	55171.492329	32.641626
689.385643	55258.936475	32.646644
690.165841	55353.583656	32.651661
690.629518	55437.845019	32.656679
691.574976	55535.283242	32.661696
692.301689	55627.750205	32.666714
693.431872	55709.864020	32.671732
693.926322	55804.234981	32.676749
694.779196	55881.829870	32.681767
695.313375	55980.397534	32.686784
696.117349	56072.157965	32.691802
696.619485	56151.814858	32.696820
697.335584	56242.602423	32.701837
698.231188	56331.931919	32.706855
698.762976	56431.229623	32.711872
699.426100	56517.735602	32.716890
700.448591	56605.552645	32.721908
700.951724	56694.179164	32.726925
701.612952	56781.920522	32.731943
702.256587	56873.107886	32.736960
703.202392	56970.406338	32.741978
704.128891	57056.132525	32.746996
704.696912	57148.636544	32.752013
705.185419	57233.723108	32.757031
705.988011	57324.475906	32.762048
706.561864	57412.619320	32.767066
707.491970	57502.751560	32.772084
708.323990	57598.804555	32.777101
708.629915	57690.433976	32.782119
709.636319	57778.567952	32.787136
710.377631	57874.376753	32.792154
711.140499	57957.321617	32.797172
711.603478	58043.307451	32.802189
712.024840	58146.249836	32.807207
713.221305	58232.684782	32.812224
713.767994	58332.304452	32.817242
714.762943	58418.739974	32.822260
715.112311	58521.752192	32.827277
715.917084	58607.161166	32.832295
716.693601	58705.328597	32.837312
717.422912	58802.889863	32.842330
718.794957	58885.742508	32.847348
719.011980	58980.175682	32.852365
719.796363	59066.285705	32.857383
720.486375	59153.233648	32.862400
721.298453	59248.106355	32.867418
722.181888	59331.340853	32.872436
722.598868	59422.934105	32.877453
723.375551	59508.173413	32.882471
723.859857	59599.408656	32.887488
724.681160	59683.799750	32.892506
725.391726	59772.367072	32.897524
725.985015	59859.307359	32.902541
726.890065	59944.407823	32.907559
727.603694	60026.436988	32.912576
728.195950	60118.676351	32.917594
728.732738	60204.297461	32.922612
729.526289	60292.752394	32.927629
730.320289	60379.030114	32.932647
731.278404	60464.446897	32.937664
731.374360	60551.771355	32.942682
731.912735	60641.748697	32.947700
732.986276	60744.967049	32.952717
733.227998	60836.808248	32.957735
734.585242	60928.481431	32.962752
735.115821	61033.425483	32.967770
736.000722	61124.806226	32.972788
736.544439	61224.507776	32.977805
737.432611	61322.446669	32.982823
738.329453	61409.275274	32.987840
738.870046	61523.392151	32.992858
739.789905	61616.763230	32.997876
740.691827	61715.125647	33.002893
741.267571	61802.290774	33.007911
741.948266	61898.814827	33.012928
742.443781	61999.274016	33.017946
743.141178	62097.802916	33.022964
744.222019	62195.569499	33.027981
744.873604	62296.701784	33.032999
746.096834	62397.624687	33.038016
746.500271	62497.328008	33.043034
747.101243	62599.298730	33.048052
748.032542	62704.415005	33.053069
748.565269	62808.581268	33.058087
749.626086	62903.979854	33.063104
750.115543	63009.305878	33.068122
751.029375	63106.051330	33.073140
751.728378	63202.938419	33.078157
752.395233	63312.207196	33.083175
753.270246	63412.378428	33.088192
753.960240	63514.427577	33.093210
754.776762	63617.457573	33.098228
755.841965	63723.038300	33.103245
756.350371	63820.540050	33.108263
757.362647	63914.848555	33.113280
757.874439	64030.475481	33.118298
758.771479	64129.987733	33.123316
759.917058	64213.469838	33.128333
760.457148	64318.002085	33.133351
761.206005	64413.094420	33.138368
761.842716	64523.075918	33.143386
762.784867	64621.665075	33.148404
763.467682	64716.262423	33.153421
764.191318	64818.052033	33.158439
764.948559	64923.445452	33.163456
765.809790	65025.986734	33.168474
766.849905	65128.234517	33.173492
767.377509	65229.461365	33.178509
768.143558	65320.698813	33.183527
768.964588	65425.141004	33.188544
769.540914	65531.071775	33.193562
770.265740	65631.389317	33.198580
771.422484	65729.594648	33.203597
771.965479	65826.244023	33.208615
772.706465	65921.298946	33.213632
773.190914	66024.757989	33.218650
774.143216	66138.356556	33.223668
775.027441	66234.909731	33.228685
775.716581	66337.552910	33.233703
776.357746	66422.856088	33.238720
777.483510	66517.865649	33.243738
777.839848	66608.924958	33.248756
778.689333	66705.472693	33.253773
779.646816	66813.058601	33.258791
780.229605	66903.557988	33.263808
780.853161	66995.786144	33.268826
781.422953	67093.835389	33.273844
782.355396	67197.026424	33.278861
783.020533	67308.680730	33.283879
783.969518	67399.833665	33.288896
784.576446	67517.620653	33.293914
785.520243	67609.724891	33.298932
786.106577	67711.199331	33.303949
786.835053	67815.944398	33.308967
787.983002	67923.796401	33.313984
788.777022	68028.798004	33.319002
789.279674	68135.428605	33.324020
789.875567	68241.418198	33.329037
790.790271	68352.708703	33.334055
791.860207	68457.409240	33.339072
792.176203	68575.563217	33.344090
793.066075	68682.464701	33.349108
793.975450	68792.858804	33.354125
795.117035	68901.944291	33.359143
795.861034	69017.779084	33.364160
796.293224	69123.310362	33.369178
797.265959	69246.936742	33.374196
798.186700	69353.956472	33.379213
799.004830	69462.335118	33.384231
799.900688	69568.492130	33.389248
800.622104	69682.750393	33.394266
801.159752	69795.429558	33.399284
802.139999	69910.952722	33.404301
803.166022	70031.509695	33.409319
804.115082	70132.170620	33.414336
805.101323	70247.757660	33.419354
805.780307	70353.780859	33.424372
806.714871	70464.577051	33.429389
807.530280	70572.897416	33.434407
808.373240	70673.767012	33.439424
808.958170	70780.351253	33.444442
809.869348	70887.302782	33.449460
810.640835	70998.937324	33.454477
811.486638	71119.476871	33.459495
812.140280	71233.739857	33.464512
813.013300	71341.066496	33.469530
814.080743	71450.592198	33.474548
815.032839	71554.741034	33.479565
815.663009	71673.480427	33.484583
816.644185	71781.298535	33.489600
817.278807	71898.442412	33.494618
818.139759	72007.204842	33.499636
819.304014	72114.185054	33.504653
819.735697	72229.437021	33.509671
820.554978	72337.004106	33.514688
821.510446	72437.482871	33.519706
822.147655	72550.348241	33.524724
823.005079	72664.927482	33.529741
823.696904	72776.316033	33.534759
824.680731	72883.213611	33.539776
825.330379	72997.839488	33.544794
826.301966	73109.058967	33.549812
827.429806	73211.704883	33.554829
828.055883	73330.566332	33.559847
829.061161	73440.971293	33.564864
829.523096	73552.437087	33.569882
830.099956	73662.428733	33.574900
831.292098	73760.152197	33.579917
831.705215	73876.110845	33.584935
832.375942	73971.814118	33.589952
833.532568	74095.953770	33.594970
834.114042	74198.461036	33.599988
835.026140	74296.964967	33.605005
835.666304	74419.046343	33.610023
836.606877	74521.574613	33.615040
837.419220	74634.586033	33.620058
837.972023	74745.953893	33.625076
838.851153	74862.350498	33.630093
839.519651	74985.747354	33.635111
840.502729	75099.899343	33.640128
841.751980	75214.909489	33.645146
842.230851	75340.225036	33.650164
842.854138	75454.472863	33.655181
844.013060	75585.319905	33.660199
844.853024	75708.414535	33.665216
845.801384	75815.215346	33.670234
846.615248	75946.308172	33.675252
847.681411	76056.650998	33.680269
848.048471	76185.382810	33.685287
848.947073	76300.287797	33.690304
849.888972	76429.070092	33.695322
851.129851	76555.804703	33.700340
851.776952	76674.006217	33.705357
852.686914	76791.989736	33.710375
853.654939	76898.183671	33.715392
854.625619	77045.446612	33.720410
855.408568	77165.465814	33.725428
856.378659	77283.442040	33.730445
857.227465	77400.994386	33.735463
858.171275	77526.044502	33.740480
859.014639	77643.763426	33.745498
859.775756	77773.568473	33.750516
860.628229	77881.671869	33.755533
861.472206	78018.369265	33.760551
862.632245	78130.910044	33.765568
862.951996	78259.012928	33.770586
864.182665	78376.725016	33.775604
865.479596	78481.290023	33.780621
865.924462	78621.942127	33.785639
866.614765	78746.594082	33.790656
867.737002	78869.113976	33.795674
868.609407	79002.695307	33.800692
869.859295	79109.525088	33.805709
870.409070	79235.746837	33.810727
871.604544	79353.531937	33.815744
872.417708	79484.122340	33.820762
873.029822	79599.035296	33.825780
874.163122	79718.833379	33.830797
874.845598	79844.606365	33.835815
875.839525	79969.228935	33.840832
876.437993	80091.278789	33.845850
877.234816	80217.238257	33.850868
878.503656	80332.228771	33.855885
878.901983	80462.977398	33.860903
880.070944	80581.519332	33.865920
880.648173	80708.718992	33.870938
881.683037	80834.834008	33.875956
882.676545	80956.078272	33.880973
883.487292	81083.445778	33.885991
884.051366	81213.791859	33.891008
885.420671	81337.069425	33.896026
885.709069	81460.985565	33.901044
887.113148	81590.745747	33.906061
887.854729	81714.782090	33.911079
888.829084	81843.483096	33.916096
889.576324	81963.946709	33.921114
890.609879	82074.318613	33.926132
891.899964	82187.374863	33.931149
892.495070	82311.968905	33.936167
893.077824	82420.474204	33.941184
894.138770	82535.366896	33.946202
894.539858	82658.523082	33.951220
895.626031	82781.382475	33.956237
896.317802	82898.184319	33.961255
897.546264	83028.928871	33.966272
898.534774	83152.185272	33.971290
898.990875	83279.998303	33.976308
900.011545	83396.066472	33.981325
900.760067	83529.093165	33.986343
901.379005	83661.481883	33.991360
902.639049	83791.832188	33.996378
903.638721	83923.313554	34.001396
904.622033	84043.292841	34.006413
905.504593	84179.266570	34.011431
906.504998	84320.480993	34.016448
907.311292	84450.107056	34.021466
908.156322	84581.717017	34.026484
909.359598	84712.321140	34.031501
909.991995	84843.623466	34.036519
911.016898	84980.985207	34.041536
912.015221	85111.395141	34.046554
912.701213	85247.189269	34.051572
913.605694	85376.335269	34.056589
915.170081	85510.168388	34.061607
915.728440	85644.856588	34.066624
916.865175	85777.655466	34.071642
917.439867	85924.786047	34.076660
918.464316	86047.681726	34.081677
919.501128	86185.376772	34.086695
920.522395	86318.956513	34.091712
921.458614	86449.990434	34.096730
922.284491	86587.403603	34.101748
923.656704	86723.059152	34.106765
924.391806	86850.489453	34.111783
925.196821	86987.134761	34.116800
926.302526	87118.119791	34.121818
926.829884	87265.923490	34.126836
927.888520	87388.844794	34.131853
928.692762	87524.922465	34.136871
929.476715	87658.634176	34.141888
930.623628	87799.170885	34.146906
931.472552	87944.697261	34.151924
932.683579	88082.019094	34.156941
933.465653	88224.249732	34.161959
934.630567	88362.340454	34.166976
935.667502	88491.390733	34.171994
936.828974	88632.955629	34.177012
937.749601	88773.012803	34.182029
938.352097	88899.471544	34.187047
939.447066	89037.918533	34.192064
940.325555	89160.051649	34.197082
941.065227	89307.262000	34.202100
942.235666	89433.114476	34.207117
943.054181	89570.415934	34.212135
944.055108	89696.841017	34.217152
945.363815	89836.994505	34.222170
945.967493	89982.619943	34.227188
946.883965	90118.197647	34.232205
947.804332	90258.021025	34.237223
948.568067	90392.825444	34.242240
949.935112	90519.031910	34.247258
950.494581	90657.316758	34.252276
951.392616	90801.037017	34.257293
952.659018	90923.243316	34.262311
953.500956	91051.600081	34.267328
954.471908	91172.370792	34.272346
955.248976	91306.340717	34.277364
956.127954	91437.963236	34.282381
957.126723	91571.430678	34.287399
957.974244	91697.685389	34.292416
958.999291	91831.454041	34.297434
959.710476	91962.344646	34.302452
960.303846	92095.611702	34.307469
961.553426	92230.969280	34.312487
962.373548	92381.566117	34.317504
963.601821	92519.615314	34.322522
964.375783	92668.040759	34.327540
965.529989	92795.734933	34.332557
966.217255	92938.433622	34.337575
967.426476	93086.285953	34.342592
968.377575	93226.295632	34.347610
969.208308	93369.911804	34.352628
970.458802	93516.454224	34.357645
971.455571	93657.092463	34.362663
972.060430	93808.705985	34.367680
973.229276	93945.883639	34.372698
974.336970	94090.676621	34.377716
975.332692	94239.036896	34.382733
976.393112	94383.889351	34.387751
977.071662	94541.528397	34.392768
978.287905	94685.369180	34.397786
979.411903	94831.126403	34.402804
980.318159	94971.163679	34.407821
981.354922	95113.982470	34.412839
982.248996	95263.795901	34.417856
983.371718	95416.882629	34.422874
984.139666	95568.922856	34.427892
985.253968	95711.377315	34.432909
986.108695	95861.732158	34.437927
987.174189	96021.054697	34.442944
988.288560	96163.409790	34.447962
989.205596	96310.765471	34.452980
990.382574	96460.692441	34.457997
991.550284	96610.266639	34.463015
992.527269	96754.192417	34.468032
993.497238	96922.471279	34.473050
994.675422	97053.715888	34.478068
995.464991	97201.285830	34.483085
996.938088	97353.705973	34.488103
997.677529	97507.027667	34.493120
998.641539	97644.316973	34.498138
999.769278	97788.439347	34.503156
1000.776270	97937.322399	34.508173
1001.736203	98085.807854	34.513191
1002.731684	98239.688798	34.518208
1003.834489	98366.272848	34.523226
1005.011059	98516.780055	34.528244
1005.671231	98665.860249	34.533261
1006.832871	98810.159404	34.538279
1007.578883	98965.464701	34.543296
1008.807640	99106.179708	34.548314
1010.034830	99256.061271	34.553332
1010.710712	99400.401096	34.558349
1011.798085	99557.088342	34.563367
1012.889793	99701.681345	34.568384
1014.042291	99845.454115	34.573402
1014.585446	99997.030907	34.578420
1015.823140	100142.312967	34.583437
1017.041484	100292.796572	34.588455
1017.726827	100445.342058	34.593472
1018.739366	100580.759989	34.598490
1019.574918	100716.941510	34.603508
1020.529641	100868.749518	34.608525
1021.342480	101009.550588	34.613543
1022.298595	101153.867009	34.618560
1023.561829	101295.017167	34.623578
1024.752335	101448.857485	34.628596
1025.357170	101590.162710	34.633613
1026.770195	101736.020292	34.638631
1027.601612	101888.283392	34.643648
1028.811195	102020.354705	34.648666
1030.109915	102166.257448	34.653684
1030.674496	102323.648392	34.658701
1031.746068	102474.798928	34.663719
1032.901282	102621.550257	34.668736
1033.595686	102772.862634	34.673754
1034.508204	102925.003706	34.678772
1035.941427	103084.328899	34.683789
1037.057109	103230.264989	34.688807
1037.685795	103403.461548	34.693824
1039.058458	103556.750643	34.698842
1040.035320	103709.189521	34.703860
1040.822082	103859.351263	34.708877
1042.269346	104016.054140	34.713895
1042.949415	104178.063662	34.718912
1044.072734	104341.906459	34.723930
1045.168980	104503.180390	34.728948
1046.639517	104656.383120	34.733965
1047.533251	104813.138342	34.738983
1048.158161	104978.063945	34.744000
1049.581718	105145.337831	34.749018
1050.594498	105298.691223	34.754036
1051.742362	105462.966732	34.759053
1052.754729	105617.171169	34.764071
1053.800975	105775.834295	34.769088
1055.149708	105935.972387	34.774106
1056.259511	106103.794637	34.779124
1056.916534	106270.319162	34.784141
1058.238441	106424.415394	34.789159
1059.271751	106588.815712	34.794176
1060.446777	106755.185418	34.799194
1061.458534	106918.018348	34.804212
1062.748743	107078.843011	34.809229
1063.850782	107239.938814	34.814247
1064.575792	107390.468217	34.819264
1065.796227	107556.352837	34.824282
1067.261220	107721.413774	34.829300
1067.885730	107881.699699	34.834317
1069.011032	108034.591231	34.839335
1070.096012	108205.813362	34.844352
1071.300819	108367.785982	34.849370
1072.355066	108530.011183	34.854388
1073.195462	108694.844839	34.859405
1074.447457	108855.328677	34.864423
1075.378999	109030.028101	34.869440
1076.704889	109191.478352	34.874458
1077.714610	109346.105681	34.879476
1078.608743	109517.858696	34.884493
1079.530090	109676.026682	34.889511
1080.909477	109847.033230	34.894528
1081.961585	110014.084537	34.899546
1083.166346	110181.467816	34.904564
1084.349327	110338.266266	34.909581
1085.506539	110504.922997	34.914599
1086.221507	110670.990307	34.919616
1087.557011	110830.138514	34.924634
1089.110962	110996.469129	34.929652
1089.610315	111150.600905	34.934669
1090.896206	111306.715390	34.939687
1091.364356	111466.091007	34.944704
1092.374905	111627.830030	34.949722
1093.991293	111771.682107	34.954740
1094.997588	111938.090170	34.959757
1096.201761	112086.624312	34.964775
1096.972137	112243.850845	34.969792
1098.453853	112395.754313	34.974810
1099.392835	112555.834673	34.979828
1100.007349	112714.000783	34.984845
1101.495671	112874.237517	34.989863
1102.379070	113037.182247	34.994880
1103.017983	113197.299743	34.999898
1104.179831	113360.088189	35.004916
1105.493236	113534.902110	35.009933
1106.563624	113700.940465	35.014951
1107.543625	113869.783926	35.019968
1108.372593	114046.210751	35.024986
1109.978506	114218.179260	35.030004
1111.018416	114398.798147	35.035021
1111.944080	114573.183108	35.040039
1113.047958	114749.278571	35.045056
1114.254438	114921.820234	35.050074
1115.426104	115090.918340	35.055092
1116.540406	115274.155290	35.060109
1117.692530	115450.982178	35.065127
1118.746081	115629.347341	35.070144
1119.614235	115813.500645	35.075162
1121.255483	115982.503943	35.080180
1122.014734	116181.985046	35.085197
1123.615001	116359.900302	35.090215
1124.773779	116539.851487	35.095232
1125.939132	116720.855256	35.100250
1127.332139	116899.312876	35.105268
1128.240642	117068.638745	35.110285
1129.389246	117250.941443	35.115303
1130.116405	117426.106527	35.120320
1131.602860	117609.930879	35.125338
1132.618934	117793.335087	35.130356
1133.679221	117981.198074	35.135373
1135.181828	118165.885119	35.140391
1136.198294	118336.937505	35.145408
1137.369437	118521.995280	35.150426
1138.760638	118688.335441	35.155444
1139.683029	118878.165154	35.160461
1140.819954	119056.026126	35.165479
1142.121252	119245.709552	35.170496
1143.401587	119423.587834	35.175514
1144.240252	119601.612192	35.180532
1145.381642	119794.253517	35.185549
1146.435225	119977.193006	35.190567
1147.758450	120158.366010	35.195584
1148.490498	120336.385078	35.200602
1149.922378	120518.722455	35.205620
1151.144831	120705.837671	35.210637
1152.629232	120894.980448	35.215655
1153.536692	121071.821082	35.220672
1154.473404	121263.702583	35.225690
1156.060985	121434.032356	35.230708
1156.969866	121627.848159	35.235725
1158.234623	121807.858254	35.240743
1159.455160	121988.599166	35.245760
1160.348555	122171.282260	35.250778
1161.922490	122352.667220	35.255796
1162.710214	122547.178848	35.260813
1164.079980	122722.812828	35.265831
1165.208669	122913.594032	35.270848
1166.044848	123094.653884	35.275866
1167.915011	123269.412740	35.280884
1168.830679	123451.933330	35.285901
1170.155763	123617.251930	35.290919
1171.301140	123779.897226	35.295936
1172.256304	123949.689840	35.300954
1173.433721	124109.781561	35.305972
1174.641288	124288.289510	35.310989
1175.603747	124455.139926	35.316007
1177.043926	124629.921284	35.321024
1177.845636	124807.784637	35.326042
1179.134620	124989.099305	35.331060
1180.296806	125169.851057	35.336077
1181.561583	125341.554766	35.341095
1182.883666	125519.517384	35.346112
1183.848365	125702.624058	35.351130
1184.984731	125874.007573	35.356148
1186.130920	126062.745699	35.361165
1187.127212	126246.357328	35.366183
1188.599743	126423.716736	35.371200
1189.623290	126608.759328	35.376218
1190.917976	126792.605793	35.381236
1191.603127	126980.062797	35.386253
1192.822119	127179.413665	35.391271
1194.033925	127366.054118	35.396288
1195.044914	127568.966439	35.401306
1196.739558	127756.002482	35.406324
1197.725205	127961.026760	35.411341
1198.955643	128151.765814	35.416359
1200.360546	128344.571849	35.421376
1201.146809	128544.517166	35.426394
1202.707782	128737.922261	35.431412
1204.001486	128938.119885	35.436429
1204.962708	129140.032589	35.441447
1206.205316	129342.663470	35.446464
1207.651026	129544.730637	35.451482
1209.289022	129726.582318	35.456500
1210.241216	129930.263802	35.461517
1211.755087	130135.444325	35.466535
1212.839367	130322.320841	35.471552
1214.056583	130529.820848	35.476570
1215.276420	130724.354178	35.481588
1216.313500	130919.640223	35.486605
1217.203573	131110.851864	35.491623
1218.760649	131310.613354	35.496640
1219.549010	131519.009994	35.501658
1221.018490	131723.228025	35.506676
1222.771340	131925.550137	35.511693
1223.641593	132124.204794	35.516711
1224.827632	132328.393900	35.521728
1226.238224	132530.023764	35.526746
1227.475154	132737.861145	35.531764
1228.687143	132925.908928	35.536781
1229.976828	133134.958046	35.541799
1231.316219	133336.247462	35.546816
1232.711666	133549.773852	35.551834
1234.017374	133736.731852	35.556852
1235.099769	133939.701119	35.561869
1236.325315	134142.039824	35.566887
1237.553190	134336.296077	35.571904
1238.767955	134536.138487	35.576922
1240.499918	134728.096914	35.581940
1241.416353	134929.218634	35.586957
1242.530565	135138.342680	35.591975
1244.018664	135325.494479	35.596992
1245.147304	135531.610686	35.602010
1246.510953	135726.346570	35.607028
1247.742380	135931.712509	35.612045
1248.475615	136127.157896	35.617063
1250.025920	136326.384651	35.622080
1251.018348	136512.007329	35.627098
1252.545476	136685.352130	35.632116
1253.909730	136884.585056	35.637133
1255.080010	137072.517096	35.642151
1256.353306	137256.652160	35.647168
1257.265463	137455.742594	35.652186
1258.833048	137627.016125	35.657204
1259.529103	137825.926244	35.662221
1260.844918	138017.164150	35.667239
1262.081299	138209.811201	35.672256
1263.270481	138412.542532	35.677274
1264.491976	138614.343286	35.682292
1265.721963	138808.643546	35.687309
1266.718744	139028.768134	35.692327
1268.395911	139218.126943	35.697344
1269.411557	139426.372108	35.702362
1270.808276	139624.621773	35.707380
1272.221797	139834.468917	35.712397
1273.536356	140042.606536	35.717415
1274.966328	140246.704016	35.722432
1275.879230	140464.729020	35.727450
1277.263428	140668.759317	35.732468
1278.928586	140874.586686	35.737485
1279.750266	141086.625965	35.742503
1280.739110	141299.553763	35.747520
1281.964990	141517.788353	35.752538
1283.448820	141731.782764	35.757556
1284.348127	141958.154731	35.762573
1286.048247	142182.409857	35.767591
1287.594979	142388.147954	35.772608
1288.731074	142615.209298	35.777626
1290.098537	142835.267855	35.782644
1291.670175	143055.815786	35.787661
1292.816955	143276.621578	35.792679
1294.254830	143490.186628	35.797696
1295.698451	143712.508960	35.802714
1296.951372	143932.387244	35.807732
1298.218500	144150.119355	35.812749
1299.522150	144368.417827	35.817767
1301.131495	144584.296006	35.822784
1301.810656	144812.187704	35.827802
1303.341481	145023.764784	35.832820
1304.601089	145247.163447	35.837837
1306.085054	145468.586074	35.842855
1307.500386	145682.265481	35.847872
1308.908949	145910.796760	35.852890
1310.193879	146126.668806	35.857908
1311.649674	146346.855794	35.862925
1312.782546	146568.630052	35.867943
1314.352045	146791.707698	35.872960
1315.520945	146998.272594	35.877978
1316.870514	147221.399205	35.882996
1318.141508	147440.299736	35.888013
1319.319887	147671.857579	35.893031
1321.220668	147884.543516	35.898048
1322.346893	148099.509330	35.903066
1323.570164	148319.246023	35.908084
1325.036460	148538.882123	35.913101
1326.221859	148761.660177	35.918119
1327.901111	148974.651727	35.923136
1328.966063	149194.315276	35.928154
1330.356836	149410.996622	35.933172
1331.904009	149627.387806	35.938189
1333.329154	149842.516948	35.943207
1334.371119	150049.253232	35.948224
1335.651101	150279.270617	35.953242
1337.216855	150490.445405	35.958260
1338.759426	150701.954669	35.963277
1339.620995	150899.798973	35.968295
1341.286806	151100.323361	35.973312
1342.267862	151300.701797	35.978330
1343.364193	151499.539690	35.983348
1345.049979	151706.244930	35.988365
1346.347450	151918.228822	35.993383
1347.361199	152119.569827	35.998400
1348.716392	152331.939767	36.003418
1349.874999	152537.169284	36.008436
1351.198106	152754.775702	36.013453
1352.142549	152982.000749	36.018471
1353.491626	153197.637259	36.023488
1354.950973	153414.018972	36.028506
1355.989149	153646.246149	36.033524
1357.311309	153871.435368	36.038541
1358.342981	154105.506081	36.043559
1359.773128	154337.750882	36.048576
1361.238370	154568.277404	36.053594
1362.542159	154807.043342	36.058612
1363.869572	155036.463514	36.063629
1364.969327	155289.430291	36.068647
1367.056059	155525.956667	36.073664
1368.541776	155767.744749	36.078682
1369.465863	156017.365432	36.083700
1371.254309	156243.112920	36.088717
1372.631485	156485.504895	36.093735
1374.030587	156726.688432	36.098752
1375.502905	156970.425832	36.103770
1376.608464	157205.906521	36.108788
1378.279954	157451.303121	36.113805
1379.847509	157697.085145	36.118823
1381.377809	157932.159434	36.123840
1382.584288	158175.549792	36.128858
1383.981325	158418.009946	36.133876
1385.475303	158646.148473	36.138893
1387.143488	158910.378386	36.143911
1388.278352	159137.775158	36.148928
1389.905501	159379.936501	36.153946
1391.271339	159622.050827	36.158964
1392.629249	159861.958342	36.163981
1393.467769	160103.865089	36.168999
1395.321496	160349.371728	36.174016
1396.991538	160598.450134	36.179034
1398.105253	160844.163406	36.184052
1399.763362	161080.562696	36.189069
1400.824050	161322.134650	36.194087
1402.341670	161568.295330	36.199104
1403.768061	161814.369671	36.204122
1404.936168	162062.046969	36.209140
1406.821846	162307.619650	36.214157
1407.581491	162562.739104	36.219175
1409.290418	162810.499662	36.224192
1410.884090	163067.471120	36.229210
1412.271118	163314.903095	36.234228
1413.807109	163566.718236	36.239245
1415.503469	163822.508529	36.244263
1416.884451	164060.574474	36.249280
1418.244243	164306.160772	36.254298
1419.584463	164557.756388	36.259316
1421.580056	164790.078876	36.264333
1422.614818	165042.866790	36.269351
1423.989723	165286.740290	36.274368
1425.978838	165521.351665	36.279386
1427.024802	165765.570387	36.284404
1428.561429	165997.854577	36.289421
1429.676094	166242.940308	36.294439
1431.299031	166482.233855	36.299456
1432.677287	166732.891989	36.304474
1434.045152	166958.273418	36.309492
1435.544235	167169.732050	36.314509
1436.696052	167415.971505	36.319527
1438.065084	167628.315257	36.324544
1439.320946	167868.051903	36.329562
1440.637414	168101.583758	36.334580
1442.002934	168330.486993	36.339597
1443.276983	168581.282276	36.344615
1444.810705	168815.785522	36.349632
1446.205176	169062.652931	36.354650
1447.742504	169305.499213	36.359668
1448.740634	169548.748130	36.364685
1450.371916	169806.157771	36.369703
1452.043651	170058.064053	36.374720
1453.559586	170296.422123	36.379738
1454.579631	170558.793141	36.384756
1456.177486	170806.929710	36.389773
1457.317590	171064.814220	36.394791
1458.736203	171323.468664	36.399808
1460.393701	171578.594775	36.404826
1461.586432	171832.499333	36.409844
1463.476952	172099.310603	36.414861
1464.624819	172366.746947	36.419879
1466.242667	172631.075902	36.424896
1467.782425	172892.675263	36.429914
1469.184085	173162.576095	36.434932
1470.835056	173426.648612	36.439949
1472.363800	173708.632493	36.444967
1473.934435	173976.211349	36.449984
1475.720989	174233.687806	36.455002
1476.769010	174507.572260	36.460020
1478.360367	174770.833204	36.465037
1480.088450	175047.127271	36.470055
1481.720479	175308.364599	36.475072
1483.429148	175575.736696	36.480090
1484.740441	175840.962367	36.485108
1486.038919	176102.546490	36.490125
1487.799842	176379.652597	36.495143
1489.325657	176644.529804	36.500160
1490.990391	176906.008331	36.505178
1492.376917	177178.553460	36.510196
1494.052203	177445.695511	36.515213
1495.287758	177708.335756	36.520231
1497.052157	177982.119562	36.525248
1498.493898	178236.094127	36.530266
1500.321429	178514.212660	36.535284
1501.779048	178768.795831	36.540301
1503.105306	179047.451669	36.545319
1504.508722	179315.708728	36.550336
1506.570198	179565.501149	36.555354
1507.630419	179837.343761	36.560372
1509.196934	180109.057158	36.565389
1510.476105	180366.111015	36.570407
1512.275803	180643.275447	36.575424
1514.061419	180903.400893	36.580442
1515.399654	181172.080039	36.585460
1516.640613	181437.575030	36.590477
1518.307255	181702.648579	36.595495
1519.730816	181967.913315	36.600512
1521.569174	182241.622315	36.605530
1523.323940	182508.055850	36.610548
1524.606622	182775.960932	36.615565
1526.061906	183039.064824	36.620583
1527.377063	183309.277575	36.625600
1529.208007	183584.185302	36.630618
1530.599990	183915.801726	36.635636
1532.025723	184185.542412	36.640653
1533.514740	184451.108508	36.645671
1535.306609	184701.744118	36.650688
1536.899577	184947.763463	36.655706
1538.060418	185203.172503	36.660724
1539.520420	185446.292973	36.665741
1541.029559	185704.061674	36.670759
1542.293279	185961.463043	36.675776
1544.275193	186222.587946	36.680794
1545.754995	186476.197667	36.685812
1547.047156	186730.650151	36.690829
1548.379945	186990.481587	36.695847
1549.784991	187250.607143	36.700864
1551.268114	187524.817915	36.705882
1552.720430	187805.079338	36.710900
1554.167601	188069.365827	36.715917
1555.664184	188343.449557	36.720935
1557.399460	188631.872957	36.725952
1559.020360	188900.858629	36.730970
1560.468991	189176.983917	36.735988
1562.207289	189454.715550	36.741005
1563.564577	189743.353359	36.746023
1565.290429	190024.923750	36.751040
1566.666482	190307.108379	36.756058
1568.744460	190590.834857	36.761076
1569.720411	190870.391027	36.766093
1571.421819	191163.906173	36.771111
1573.129103	191453.890447	36.776128
1574.971552	191742.508034	36.781146
1576.446098	192031.285488	36.786164
1578.177517	192320.506034	36.791181
1579.775434	192600.070459	36.796199
1581.251348	192905.157030	36.801216
1583.169933	193178.296952	36.806234
1584.178792	193479.266859	36.811252
1585.937014	193778.392925	36.816269
1587.644773	194060.813687	36.821287
1589.314261	194357.745082	36.826304
1590.817284	194649.292751	36.831322
1592.225145	194956.198289	36.836340
1594.035172	195241.526704	36.841357
1595.790477	195537.202625	36.846375
1597.291775	195833.604774	36.851392
1599.329065	196131.320753	36.856410
1600.921968	196429.919762	36.861428
1602.281830	196724.796444	36.866445
1604.151603	197021.016422	36.871463
1605.675679	197318.129366	36.876480
1607.377075	197610.642858	36.881498
1609.312159	197907.819682	36.886516
1610.646391	198197.191173	36.891533
1612.381429	198495.797572	36.896551
1613.792998	198790.467081	36.901568
1615.351330	199086.917725	36.906586
1617.214387	199387.791995	36.911604
1618.679707	199682.378575	36.916621
1620.507312	199977.925085	36.921639
1621.828608	200266.616592	36.926656
1623.857676	200567.975142	36.931674
1625.506464	200868.199852	36.936692
1626.947216	201161.192609	36.941709
1628.920882	201457.938222	36.946727
1630.012272	201755.635303	36.951744
1631.854049	202045.493128	36.956762
1633.340931	202342.900695	36.961780
1634.990808	202644.144430	36.966797
1636.862674	202937.733167	36.971815
1638.821875	203238.624651	36.976832
1640.388980	203527.892785	36.981850
1642.094638	203821.178705	36.986868
1643.588874	204101.466584	36.991885
1645.194473	204372.897295	36.996903
1646.870245	204638.525572	37.001920
1648.491591	204919.912457	37.006938
1649.861776	205200.500751	37.011956
1651.442254	205477.017467	37.016973
1653.537701	205751.066091	37.021991
1654.452488	206028.907061	37.027008
1656.587614	206303.432852	37.032026
1657.672127	206588.081387	37.037044
1659.142098	206878.360250	37.042061
1660.539034	207180.209317	37.047079
1662.002390	207478.161721	37.052096
1664.292356	207773.902093	37.057114
1665.351169	208078.574202	37.062132
1667.287635	208381.153307	37.067149
1669.047463	208680.026161	37.072167
1670.306090	208984.845967	37.077184
1672.034559	209296.045052	37.082202
1673.811215	209610.082148	37.087220
1675.398642	209918.839937	37.092237
1677.361364	210230.790986	37.097255
1679.083318	210544.812347	37.102272
1680.883572	210860.523842	37.107290
1682.399447	211171.936200	37.112308
1684.034643	211498.724739	37.117325
1686.327861	211806.637460	37.122343
1687.318188	212129.971115	37.127360
1689.223791	212449.478354	37.132378
1690.766266	212773.386757	37.137396
1692.346386	213103.538883	37.142413
1694.204679	213421.606473	37.147431
1695.799755	213740.884118	37.152448
1697.832028	214067.714743	37.157466
1699.288949	214399.005140	37.162484
1701.015320	214725.757201	37.167501
1702.903043	215048.114842	37.172519
1704.705836	215382.527428	37.177536
1706.650336	215710.872005	37.182554
1708.847382	216034.452204	37.187572
1710.287692	216362.063255	37.192589
1712.202727	216681.318594	37.197607
1713.429955	217022.833963	37.202624
1715.461694	217330.868360	37.207642
1717.297180	217666.141238	37.212660
1719.021979	217989.491805	37.217677
1721.073045	218308.599853	37.222695
1722.320137	218637.258755	37.227712
1724.319337	218959.677781	37.232730
1725.989258	219283.367889	37.237748
1728.011586	219611.372489	37.242765
1729.769741	219937.665704	37.247783
1730.822049	220265.669970	37.252800
1732.936864	220585.226387	37.257818
1734.626263	220914.985703	37.262836
1735.959499	221249.271982	37.267853
1738.111684	221579.619609	37.272871
1739.687944	221911.454685	37.277888
1741.362807	222238.498460	37.282906
1743.365665	222573.874328	37.287924
1745.082255	222902.512184	37.292941
1747.091126	223226.811076	37.297959
1748.572289	223564.377319	37.302976
1750.583661	223888.498093	37.307994
1752.136666	224214.011644	37.313012
1753.605479	224547.464474	37.318029
1755.887407	224873.702342	37.323047
1757.243629	225199.449981	37.328064
1759.417701	225516.305230	37.333082
1761.094249	225823.102099	37.338100
1762.411353	226124.493327	37.343117
1764.436925	226433.902978	37.348135
1766.115182	226742.122152	37.353152
1767.515488	227051.477165	37.358170
1769.294719	227364.888300	37.363188
1770.791309	227689.241961	37.368205
1772.979937	228004.062359	37.373223
1774.561657	228331.222421	37.378240
1776.372466	228651.512865	37.383258
1777.980182	228977.220663	37.388276
1779.690846	229300.270237	37.393293
1781.348159	229631.254114	37.398311
1783.130465	229964.250638	37.403328
1784.927852	230300.343965	37.408346
1786.666624	230638.072182	37.413364
1788.374334	230974.966780	37.418381
1790.347730	231300.006796	37.423399
1791.682006	231646.892462	37.428416
1793.796189	231994.621249	37.433434
1795.351615	232343.682066	37.438452
1797.299796	232694.713528	37.443469
1799.285020	233045.916798	37.448487
1801.015709	233392.764792	37.453504
1803.258789	233740.091254	37.458522
1805.031487	234092.749670	37.463540
1806.980904	234444.973703	37.468557
1808.631812	234784.542267	37.473575
1810.402841	235133.745206	37.478592
1812.017539	235486.249400	37.483610
1814.062597	235842.394888	37.488628
1815.979139	236197.137551	37.493645
1817.857689	236545.484092	37.498663
1819.323790	236915.691189	37.503680
1821.328430	237272.146466	37.508698
1823.210273	237625.673766	37.513716
1824.783110	237991.798416	37.518733
1826.899160	238351.689986	37.523751
1828.995497	238706.173276	37.528768
1830.658947	239070.275607	37.533786
1832.599334	239425.595364	37.538804
1834.362164	239784.346529	37.543821
1836.831749	240141.716476	37.548839
1838.461748	240508.565776	37.553856
1839.898128	240855.706481	37.558874
1842.265585	241218.959147	37.563892
1843.594529	241591.137930	37.568909
1845.473669	241947.099018	37.573927
1847.123442	242311.681760	37.578944
1849.410345	242673.090470	37.583962
1851.344083	243041.692161	37.588980
1853.060130	243411.953122	37.593997
1855.163168	243766.606268	37.599015
1857.030456	244140.906839	37.604032
1858.726935	244502.506619	37.609050
1860.310440	244862.192843	37.614068
1862.177812	245230.394790	37.619085
1864.183489	245598.701448	37.624103
1866.006085	245970.211425	37.629120
1867.903533	246341.404159	37.634138
1869.945426	246696.112655	37.639156
1871.800067	247065.380089	37.644173
1873.821867	247429.717945	37.649191
1875.575039	247795.240229	37.654208
1877.377011	248164.208876	37.659226
1879.500822	248524.083143	37.664244
1881.558049	248882.061916	37.669261
1883.321044	249228.527939	37.674279
1885.332913	249571.982253	37.679296
1887.236902	249916.697454	37.684314
1888.933561	250247.447794	37.689332
1890.615924	250588.690772	37.694349
1892.293809	250932.016696	37.699367
1894.091565	251285.585529	37.704384
1896.093464	251632.821944	37.709402
1898.151715	251977.483175	37.714420
1899.926790	252330.341923	37.719437
1901.540180	252682.386888	37.724455
1903.204659	253047.555706	37.729472
1905.325940	253413.541197	37.734490
1906.993187	253768.496326	37.739508
1909.024288	254131.877745	37.744525
1910.841013	254501.388122	37.749543
1912.363960	254884.279209	37.754560
1914.166625	255255.212258	37.759578
1916.120813	255630.108581	37.764596
1917.989733	256016.269916	37.769613
1920.211281	256393.636980	37.774631
1921.962697	256764.472260	37.779648
1924.144455	257163.230975	37.784666
1926.413467	257545.134030	37.789684
1927.723066	257932.723422	37.794701
1930.114823	258309.728002	37.799719
1931.865083	258705.526665	37.804736
1933.706184	259098.871382	37.809754
1935.770216	259493.297556	37.814772
1937.786975	259894.232319	37.819789
1939.659055	260278.855976	37.824807
1941.683012	260681.463343	37.829824
1943.416717	261086.857932	37.834842
1945.498357	261472.206826	37.839860
1947.564107	261872.542850	37.844877
1949.608113	262284.463167	37.849895
1951.602719	262678.635257	37.854912
1953.654940	263072.923907	37.859930
1955.791807	263471.998392	37.864948
1957.840268	263881.245006	37.869965
1959.873777	264275.100361	37.874983
1961.828784	264664.928035	37.880000
1964.057924	265075.284681	37.885018
1966.268635	265465.120121	37.890036
1968.086525	265877.976201	37.895053
1970.141244	266268.950504	37.900071
1972.384488	266653.467886	37.905088
1974.170446	267062.946017	37.910106
1976.434055	267438.796194	37.915124
1978.258966	267843.870992	37.920141
1980.516622	268233.459569	37.925159
1982.277128	268614.971495	37.930176
1984.463085	269012.009775	37.935194
1986.510976	269403.201021	37.940212
1988.150540	269803.851738	37.945229
1990.050902	270194.326168	37.950247
1992.263296	270590.515382	37.955264
1994.303697	270985.205908	37.960282
1996.027291	271380.350619	37.965300
1998.142100	271777.921300	37.970317
1999.774958	272176.657671	37.975335
2002.283179	272576.220346	37.980352
2004.127848	272967.376989	37.985370
2006.196215	273351.766665	37.990388
2008.253253	273755.407142	37.995405
2010.200894	274154.999335	38.000423
2012.056820	274549.727830	38.005440
2014.016040	274940.501837	38.010458
2016.398696	275316.427083	38.015476
2017.952315	275690.397822	38.020493
2020.228787	276066.260025	38.025511
2022.069050	276442.849016	38.030528
2024.291037	276808.989607	38.035546
2025.783891	277183.242239	38.040564
2028.064792	277576.365698	38.045581
2029.661741	277958.928092	38.050599
2031.898876	278337.299785	38.055616
2033.779339	278732.664031	38.060634
2036.269178	279118.966424	38.065652
2037.764094	279514.793250	38.070669
2040.011413	279900.647085	38.075687
2041.833402	280305.560700	38.080704
2043.605275	280702.302903	38.085722
2045.923714	281098.576538	38.090740
2047.558426	281510.064590	38.095757
2048.895221	281912.988314	38.100775
2051.642289	282317.542900	38.105792
2053.549931	282743.658927	38.110810
2055.939008	283157.482715	38.115828
2058.069625	283581.044841	38.120845
2060.232518	283991.090079	38.125863
2062.466535	284405.413225	38.130880
2064.387624	284836.846988	38.135898
2066.456995	285250.022726	38.140916
2068.553491	285668.194085	38.145933
2070.611505	286091.218864	38.150951
2072.881824	286513.572950	38.155968
2075.007245	286943.615496	38.160986
2077.113014	287364.187066	38.166004
2079.134166	287799.775824	38.171021
2081.080599	288220.214475	38.176039
2083.530230	288649.357171	38.181056
2085.341623	289086.747514	38.186074
2087.315847	289498.413426	38.191092
2089.416947	289929.481017	38.196109
2091.827850	290373.218048	38.201127
2094.181779	290798.298653	38.206144
2096.128910	291237.557160	38.211162
2098.081635	291661.780561	38.216180
2100.048426	292100.268136	38.221197
2102.400239	292534.553749	38.226215
2104.678613	292972.732391	38.231232
2106.725408	293417.316883	38.236250
2109.070819	293852.051019	38.241268
2111.115726	294281.065622	38.246285
2113.392655	294720.196456	38.251303
2115.586279	295150.958698	38.256320
2117.551448	295587.465969	38.261338
2119.727384	296024.749414	38.266356
2121.800867	296458.237321	38.271373
2123.872114	296894.514996	38.276391
2126.210247	297323.080413	38.281408
2128.484050	297776.634206	38.286426
2130.643300	298200.016460	38.291444
2132.862534	298638.770870	38.296461
2134.569586	299068.030987	38.301479
2137.013899	299506.692541	38.306496
2139.147228	299955.757044	38.311514
2141.082378	300384.539618	38.316532
2143.498433	300822.408043	38.321549
2145.244566	301263.627152	38.326567
2147.683414	301700.114021	38.331584
2150.011944	302136.843050	38.336602
2152.268556	302579.570718	38.341620
2154.552110	303012.567883	38.346637
2156.511240	303433.503537	38.351655
2158.611923	303847.178952	38.356672
2160.840776	304256.160234	38.361690
2162.669574	304654.310910	38.366708
2164.714451	305069.939868	38.371725
2166.452397	305480.841254	38.376743
2168.855155	305898.438194	38.381760
2170.624190	306326.360451	38.386778
2172.851794	306749.815989	38.391796
2175.200156	307170.888411	38.396813
2177.201747	307598.585726	38.401831
2179.747913	308016.294856	38.406848
2181.563384	308457.492124	38.411866
2183.580071	308884.541351	38.416884
2185.581800	309320.802894	38.421901
2187.707358	309758.056418	38.426919
2189.927297	310209.378043	38.431936
2191.804326	310652.627013	38.436954
2194.145136	311100.977077	38.441972
2196.271709	311562.351472	38.446989
2198.493575	312017.818132	38.452007
2201.045921	312466.147528	38.457024
2202.900564	312940.139645	38.462042
2205.011786	313388.757602	38.467060
2207.480991	313851.350183	38.472077
2209.905651	314334.350152	38.477095
2212.349274	314785.110505	38.482112
2214.203302	315248.039002	38.487130
2216.519790	315715.788505	38.492148
2219.153478	316179.245336	38.497165
2220.768889	316652.094318	38.502183
2223.155347	317124.944555	38.507200
2225.400132	317600.984115	38.512218
2227.450737	318074.942602	38.517236
2230.068222	318554.263355	38.522253
2232.091335	319038.341157	38.527271
2234.515316	319519.483314	38.532288
2236.552520	319995.808394	38.537306
2238.890785	320470.330166	38.542324
2241.320218	320957.621733	38.547341
2243.573707	321446.559269	38.552359
2246.041482	321927.794378	38.557376
2248.294624	322401.978011	38.562394
2250.822590	322892.708194	38.567412
2253.303974	323385.419078	38.572429
2255.262213	323861.383082	38.577447
2257.763097	324339.438843	38.582464
2260.150639	324826.691903	38.587482
2262.434933	325301.649420	38.592500
2265.234397	325771.852231	38.597517
2267.008836	326261.873537	38.602535
2269.628949	326733.209609	38.607552
2271.980451	327207.652153	38.612570
2274.114868	327681.615594	38.617588
2276.717361	328164.177106	38.622605
2278.961454	328656.378986	38.627623
2281.109753	329118.753936	38.632640
2283.322387	329590.500366	38.637658
2285.503790	330062.474311	38.642676
2288.113447	330534.502379	38.647693
2289.848194	331029.113401	38.652711
2292.607157	331496.818929	38.657728
2294.665117	331983.172921	38.662746
2296.669749	332468.514323	38.667764
2299.267555	332937.318242	38.672781
2301.841573	333425.653218	38.677799
2304.113765	333887.393307	38.682816
2306.308948	334371.691095	38.687834
2308.598043	334844.299201	38.692852
2310.749068	335297.187804	38.697869
2313.204212	335749.313039	38.702887
2315.307952	336190.453561	38.707904
2317.187317	336649.912420	38.712922
2319.184226	337107.089614	38.717940
2321.552190	337570.696431	38.722957
2323.947165	338032.695125	38.727975
2326.585927	338503.882346	38.732992
2328.552252	338972.251733	38.738010
2330.859435	339446.471379	38.743028
2333.315403	339913.509016	38.748045
2334.866914	340389.559001	38.753063
2337.423848	340865.496025	38.758080
2339.533993	341356.713816	38.763098
2342.136706	341839.884059	38.768116
2344.533939	342333.401878	38.773133
2346.663492	342840.497393	38.778151
2348.876704	343337.402739	38.783168
2351.437617	343821.794587	38.788186
2353.480862	344333.345067	38.793204
2356.361432	344837.605497	38.798221
2358.144460	345344.363188	38.803239
2360.819906	345857.871316	38.808256
2363.325670	346358.135685	38.813274
2365.470150	346873.917560	38.818292
2367.715863	347385.491628	38.823309
2369.684421	347906.153756	38.828327
2372.582259	348422.275603	38.833344
2374.990889	348947.923888	38.838362
2377.219416	349485.027547	38.843380
2379.802287	350008.983434	38.848397
2381.788878	350542.760602	38.853415
2384.496312	351072.207332	38.858432
2387.085283	351607.115125	38.863450
2389.185778	352144.803319	38.868468
2392.453383	352670.789397	38.873485
2394.576180	353196.464170	38.878503
2397.211870	353729.554438	38.883520
2399.769389	354271.901554	38.888538
2402.157566	354787.697041	38.893556
2404.560662	355321.329162	38.898573
2406.855439	355862.168812	38.903591
2409.628333	356396.510578	38.908608
2412.234867	356926.027275	38.913626
2414.361512	357453.581977	38.918644
2417.322140	357978.893185	38.923661
2419.108188	358519.410983	38.928679
2421.917933	359039.302913	38.933696
2424.574804	359575.863478	38.938714
2426.753501	360110.436176	38.943732
2429.217181	360637.857637	38.948749
2431.472701	361172.145981	38.953767
2434.076963	361706.851807	38.958784
2436.669686	362243.932335	38.963802
2438.867603	362787.122410	38.968820
2441.637372	363308.796702	38.973837
2444.313431	363843.072545	38.978855
2446.317157	364374.808054	38.983872
2448.767209	364914.447245	38.988890
2451.331195	365441.893992	38.993908
2454.155555	365977.729459	38.998925
2456.593072	366507.153275	39.003943
2459.081847	367040.639316	39.008960
2461.300176	367573.878975	39.013978
2463.636951	368106.684696	39.018996
2466.376899	368635.945774	39.024013
2468.557655	369170.909831	39.029031
2471.387348	369689.697208	39.034048
2473.581635	370198.590944	39.039066
2476.183984	370707.183566	39.044084
2478.849350	371208.459778	39.049101
2481.213867	371707.899051	39.054119
2483.314189	372209.245581	39.059136
2485.871395	372714.007980	39.064154
2488.148235	373222.706716	39.069172
2490.296737	373733.518942	39.074189
2492.571226	374261.757739	39.079207
2495.043058	374768.649100	39.084224
2497.661171	375289.644515	39.089242
2500.118924	375821.371069	39.094260
2502.346761	376353.959089	39.099277
2505.192352	376886.186600	39.104295
2507.177985	377424.339072	39.109312
2509.678886	377956.649838	39.114330
2512.235815	378512.093716	39.119348
2514.454474	379054.685645	39.124365
2516.993696	379604.106024	39.129383
2519.351947	380160.407498	39.134400
2522.062665	380734.245587	39.139418
2524.171660	381290.258063	39.144436
2527.034977	381849.230655	39.149453
2529.529561	382422.457427	39.154471
2531.919731	382999.284184	39.159488
2534.889240	383562.685872	39.164506
2537.316606	384138.898704	39.169524
2539.893874	384714.239362	39.174541
2542.120544	385294.357501	39.179559
2545.005335	385883.729224	39.184576
2547.948039	386457.858893	39.189594
2550.161175	387050.524428	39.194612
2553.025643	387627.956838	39.199629
2555.689452	388215.206672	39.204647
2558.265724	388802.608262	39.209664
2561.089922	389382.867493	39.214682
2563.490291	389968.749702	39.219700
2566.188956	390559.381924	39.224717
2568.824462	391148.186874	39.229735
2571.468443	391734.849615	39.234752
2574.204936	392315.053183	39.239770
2576.669813	392914.374060	39.244788
2579.569194	393499.080765	39.249805
2582.154337	394092.834684	39.254823
2584.790605	394680.591648	39.259840
2587.323955	395268.907175	39.264858
2589.378322	395866.446569	39.269876
2592.389061	396462.808838	39.274893
2594.868874	397053.569186	39.279911
2597.315981	397652.622039	39.284928
2600.349011	398244.531549	39.289946
2602.869028	398842.631415	39.294964
2605.615250	399439.010139	39.299981
2608.016797	400041.957185	39.304999
2610.611146	400632.001773	39.310016
2613.334564	401226.566476	39.315034
2615.778837	401837.001652	39.320052
2618.244683	402430.360750	39.325069
2620.901246	403037.542116	39.330087
2623.702870	403649.340722	39.335104
2626.555264	404250.689525	39.340122
2629.181396	404853.980800	39.345140
2631.793929	405455.082002	39.350157
2634.286573	406051.631460	39.355175
2636.578318	406653.965209	39.360192
2639.268070	407259.458968	39.365210
2642.116816	407882.469717	39.370228
2645.068555	408476.403011	39.375245
2647.711050	409050.989776	39.380263
2650.182788	409636.061702	39.385280
2653.126066	410196.910440	39.390298
2655.561120	410766.222849	39.395316
2657.883674	411328.303270	39.400333
2660.730465	411908.145838	39.405351
2663.298692	412484.373995	39.410368
2666.008625	413047.715158	39.415386
2668.176294	413634.649392	39.420404
2670.476324	414213.503757	39.425421
2673.357395	414805.808190	39.430439
2675.652175	415402.234501	39.435456
2678.195814	415999.465051	39.440474
2680.731365	416615.546384	39.445492
2683.413117	417223.646059	39.450509
2686.223270	417834.236947	39.455527
2688.426197	418452.592530	39.460544
2691.279465	419075.076352	39.465562
2693.681075	419705.400402	39.470580
2696.214468	420341.854391	39.475597
2699.230575	420972.701264	39.480615
2701.720269	421606.544127	39.485632
2704.502994	422243.962417	39.490650
2707.540542	422898.968134	39.495668
2709.781645	423548.161540	39.500685
2712.536973	424194.675207	39.505703
2715.382935	424856.827672	39.510720
2718.217826	425516.937875	39.515738
2721.269717	426172.341334	39.520756
2724.211943	426826.072261	39.525773
2726.923575	427483.255539	39.530791
2729.678827	428146.931519	39.535808
2732.487727	428800.517551	39.540826
2735.312238	429464.593634	39.545844
2738.166421	430129.249328	39.550861
2741.044330	430793.373444	39.555879
2743.633470	431455.852340	39.560896
2746.494610	432115.537044	39.565914
2749.316668	432789.306118	39.570932
2752.249709	433450.197863	39.575949
2755.189367	434122.234532	39.580967
2758.068525	434799.159120	39.585984
2761.125226	435452.382866	39.591002
2763.653867	436107.233421	39.596020
2766.705615	436772.287712	39.601037
2769.976041	437429.402328	39.606055
2772.557042	438095.140884	39.611072
2775.573676	438750.935762	39.616090
2778.389304	439404.667895	39.621108
2781.267299	440070.795596	39.626125
2784.001419	440722.928502	39.631143
2786.551373	441386.989457	39.636160
2789.409895	442033.348762	39.641178
2792.600894	442690.544477	39.646196
2795.810659	443351.956920	39.651213
2798.430091	443993.638201	39.656231
2800.891222	444653.605768	39.661248
2803.886002	445309.829728	39.666266
2807.067192	445962.869749	39.671284
2809.616170	446616.540800	39.676301
2812.935782	447264.462283	39.681319
2815.319030	447916.647966	39.686336
2818.239078	448551.052212	39.691354
2821.307860	449211.668438	39.696372
2823.754033	449844.939818	39.701389
2826.578222	450496.963113	39.706407
2829.335559	451149.175039	39.711424
2832.557746	451772.310296	39.716442
2835.098306	452404.516848	39.721460
2837.739740	453012.906888	39.726477
2840.643289	453626.384235	39.731495
2843.043564	454249.611276	39.736512
2846.034619	454852.229276	39.741530
2848.802345	455481.665007	39.746548
2851.195541	456104.524334	39.751565
2854.304335	456724.422965	39.756583
2856.967601	457352.192317	39.761600
2859.411202	457989.865433	39.766618
2862.582117	458632.448113	39.771636
2864.878314	459263.990548	39.776653
2868.061932	459906.523668	39.781671
2870.700585	460557.898410	39.786688
2873.406020	461219.834621	39.791706
2875.940271	461873.648040	39.796724
2879.159214	462548.319231	39.801741
2882.041481	463206.567963	39.806759
2884.702704	463886.116668	39.811776
2887.761676	464553.013537	39.816794
2890.355343	465241.145129	39.821812
2892.684717	465930.298707	39.826829
2895.766116	466608.158012	39.831847
2898.734628	467307.949819	39.836864
2901.717435	468009.626616	39.841882
2904.355661	468712.336306	39.846900
2907.431023	469425.236645	39.851917
2910.367912	470121.837632	39.856935
2913.466783	470845.213316	39.861952
2916.252978	471563.058663	39.866970
2919.158058	472274.096574	39.871988
2922.124029	472995.380542	39.877005
2924.965624	473707.727038	39.882023
2927.980704	474442.956292	39.887040
2931.181133	475173.887881	39.892058
2934.403401	475898.581634	39.897076
2937.475501	476641.616581	39.902093
2940.404226	477364.222833	39.907111
2943.635363	478084.530991	39.912128
2946.870904	478818.717977	39.917146
2949.551020	479550.991972	39.922164
2952.714460	480280.283483	39.927181
2955.942220	480998.241601	39.932199
2958.771105	481721.470529	39.937216
2961.979922	482445.412907	39.942234
2965.032790	483173.175882	39.947252
2967.844121	483899.682789	39.952269
2971.240361	484619.816078	39.957287
2974.053572	485351.444478	39.962304
2976.966220	486065.741172	39.967322
2980.437926	486790.698724	39.972340
2983.173336	487528.885850	39.977357
2986.466800	488245.036498	39.982375
2989.119710	488966.945847	39.987392
2992.072543	489689.932522	39.992410
2995.169381	490412.408842	39.997428
2998.248472	491147.042027	40.002445
3001.600183	491864.473008	40.007463
3004.450011	492588.092288	40.012480
3007.779892	493303.393000	40.017498
3010.886011	494030.427530	40.022516
3013.677371	494757.526128	40.027533
3016.814107	495474.766878	40.032551
3019.828545	496192.696893	40.037568
3022.563405	496900.213911	40.042586
3025.874964	497620.696316	40.047604
3028.647788	498339.314610	40.052621
3031.517437	499047.613241	40.057639
3034.492194	499735.977925	40.062656
3037.312852	500420.861071	40.067674
3040.736525	501109.593899	40.072692
3043.267014	501794.860215	40.077709
3046.141736	502479.587269	40.082727
3049.215149	503164.804305	40.087744
3052.296379	503870.972066	40.092762
3055.257023	504554.379121	40.097780
3057.547979	505268.350883	40.102797
3060.917620	505972.105499	40.107815
3063.809285	506683.446965	40.112832
3066.983824	507402.406018	40.117850
3070.476960	508111.418407	40.122868
3072.761577	508836.732114	40.127885
3076.003264	509567.643607	40.132903
3078.816944	510293.855774	40.137920
3081.926320	511030.747673	40.142938
3085.245668	511763.896342	40.147956
3087.944785	512504.093981	40.152973
3091.355408	513253.846761	40.157991
3094.318298	513995.733969	40.163008
3097.173058	514758.516321	40.168026
3100.049840	515515.571243	40.173044
3103.223434	516283.750089	40.178061
3106.431025	517050.070632	40.183079
3109.675036	517822.727115	40.188096
3112.708361	518596.378115	40.193114
3115.970617	519380.555569	40.198132
3118.779052	520154.152909	40.203149
3122.236764	520935.143599	40.208167
3125.352337	521721.972452	40.213184
3128.200826	522515.681943	40.218202
3131.574476	523302.679279	40.223220
3134.774033	524106.943192	40.228237
3138.485662	524897.713023	40.233255
3141.201494	525693.012879	40.238272
3144.017682	526499.704059	40.243290
3147.466013	527296.953303	40.248308
3150.664223	528110.569687	40.253325
3153.833141	528909.020779	40.258343
3157.193074	529724.420568	40.263360
3160.034958	530537.590359	40.268378
3163.661825	531333.812677	40.273396
3166.667669	532150.371542	40.278413
3170.116147	532961.235850	40.283431
3173.297841	533777.413458	40.288448
3176.701307	534582.960818	40.293466
3179.961772	535395.659455	40.298484
3182.646914	536217.131744	40.303501
3186.078935	537019.810498	40.308519
3189.178748	537835.190263	40.313536
3192.638238	538661.403532	40.318554
3196.411374	539475.819703	40.323572
3199.450257	540292.606757	40.328589
3203.034660	541104.939832	40.333607
3205.958169	541904.979458	40.338624
3209.119740	542716.621990	40.343642
3212.032919	543524.487651	40.348660
3215.222934	544352.476276	40.353677
3218.775687	545155.721117	40.358695
3221.616088	545977.335019	40.363712
3224.834246	546780.677254	40.368730
3228.324296	547602.783691	40.373748
3231.344703	548425.460296	40.378765
3234.705972	549241.107702	40.383783
3238.490499	550056.233374	40.388800
3241.524093	550878.091084	40.393818
3244.908529	551660.829323	40.398836
3247.363204	552446.219437	40.403853
3251.019072	553226.207025	40.408871
3254.278086	554000.190595	40.413888
3257.502922	554769.618307	40.418906
3260.714913	555535.289563	40.423924
3263.842648	556313.956540	40.428941
3266.662094	557083.299107	40.433959
3269.662279	557863.388525	40.438976
3272.517467	558659.685478	40.443994
3276.219016	559450.184609	40.449012
3279.128819	560256.587712	40.454029
3282.730546	561051.354443	40.459047
3285.973910	561850.832732	40.464064
3288.721116	562665.362422	40.469082
3292.109030	563476.830069	40.474100
3295.453664	564301.070439	40.479117
3298.433380	565124.808742	40.484135
3301.986922	565966.277521	40.489152
3305.244847	566803.424888	40.494170
3308.327494	567636.433103	40.499188
3311.640299	568484.065485	40.504205
3315.005050	569327.071350	40.509223
3318.475538	570178.759537	40.514240
3321.643796	571036.688827	40.519258
3324.973278	571894.077943	40.524276
3328.261743	572753.611111	40.529293
3331.284253	573616.373813	40.534311
3335.248524	574484.828590	40.539328
3338.063279	575354.547180	40.544346
3341.284479	576236.893990	40.549364
3345.177965	577120.367196	40.554381
3348.686221	578000.329055	40.559399
3352.046320	578885.347122	40.564416
3355.446884	579773.939965	40.569434
3358.910643	580662.401862	40.574452
3362.306794	581552.253426	40.579469
3365.504121	582438.863987	40.584487
3369.360290	583331.900638	40.589504
3372.474747	584230.530577	40.594522
3376.231738	585109.088478	40.599540
3379.501092	586002.649273	40.604557
3382.820045	586892.829989	40.609575
3386.752379	587778.693407	40.614592
3389.878281	588670.707935	40.619610
3393.377445	589569.736917	40.624628
3396.762147	590464.661310	40.629645
3400.368111	591353.081045	40.634663
3403.857116	592251.088186	40.639680
3407.596897	593161.020605	40.644698
3411.019654	594052.592126	40.649716
3413.883434	594948.521985	40.654733
3417.317260	595841.690030	40.659751
3421.210304	596741.502940	40.664768
3424.406503	597647.290608	40.669786
3428.064387	598537.399315	40.674804
3431.533152	599435.201061	40.679821
3434.647970	600330.085680	40.684839
3438.634415	601221.362937	40.689856
3441.969141	602124.845223	40.694874
3445.647302	603022.106233	40.699892
3448.944344	603916.803995	40.704909
3452.107623	604822.423826	40.709927
3455.985763	605698.712083	40.714944
3459.238034	606597.176393	40.719962
3462.442800	607492.426517	40.724980
3466.206304	608395.642306	40.729997
3469.138018	609290.678007	40.735015
3473.024839	610158.225867	40.740020
3476.254221	611005.100340	40.745024
3479.766969	611802.814138	40.750029
3482.675197	612547.018229	40.755034
3485.702354	613236.711432	40.760039
3488.958367	613869.338378	40.765044
3491.527908	614456.948683	40.770048
3493.969866	614983.019440	40.775053
3496.713663	615465.734963	40.780058
3499.256191	615878.943039	40.785063
3501.806485	616237.411796	40.790068
3503.603030	616555.258347	40.795072
3505.538217	616814.907274	40.800077
3507.720898	617050.875152	40.805082
3508.972911	617215.128075	40.810087
3511.053973	617351.566397	40.815092
3511.908081	617452.018178	40.820096
3513.906536	617517.213094	40.825101
3514.927159	617546.484246	40.830106
3516.062185	617540.710520	40.835111
3517.547096	617508.949097	40.840116
3518.071673	617453.353290	40.845120
3519.063959	617365.654608	40.850125
3519.483633	617249.312766	40.855130
3520.425416	617119.496200	40.860135
3521.115355	616959.235632	40.865140
3521.507956	616787.075937	40.870144
3522.209852	616607.269212	40.875149
3522.449064	616406.742918	40.880154
3522.835367	616179.103765	40.885159
3522.973056	615956.445834	40.890164
3522.921460	615725.716400	40.895168
3523.065741	615475.909638	40.900173
3523.565601	615223.642090	40.905178
3523.558621	614976.995212	40.910183
3524.369885	614699.775782	40.915188
3524.303283	614429.233677	40.920192
3524.133599	614138.806751	40.925197
3524.411066	613860.897894	40.930202
3523.738248	613566.934168	40.935207
3524.115815	613265.999235	40.940212
3523.959012	612979.485966	40.945216
3524.017779	612673.784190	40.950221
3523.750654	612380.122398	40.955226
3523.862518	612079.943568	40.960231
3523.633356	611767.960141	40.965236
3523.440181	611480.010194	40.970240
3523.778824	611168.769514	40.975245
3523.427707	610864.177162	40.980250
3523.096982	610559.822495	40.985255
3523.339610	610260.819441	40.990260
3522.500900	609960.026460	40.995264
3522.498554	609653.493143	41.000269
3522.397173	609364.368773	41.005274
3522.156793	609073.957701	41.010279
3521.931769	608773.783911	41.015284
3522.061615	608483.898310	41.020288
3521.511101	608181.007333	41.025293
3521.432250	607891.337620	41.030298
3521.061223	607598.654396	41.035303
3521.054940	607298.253079	41.040308
3520.896452	607024.727054	41.045312
3520.542929	606759.877763	41.050317
3519.979185	606471.244159	41.055322
3519.752068	606197.956961	41.060327
3519.605355	605916.595996	41.065332
3519.517016	605656.379136	41.070336
3519.365953	605387.210673	41.075341
3518.867539	605118.039458	41.080346
3518.545187	604857.188651	41.085351
3518.550874	604607.036611	41.090356
3518.329373	604356.563811	41.095360
3518.071648	604093.882485	41.100365
3517.905974	603852.194611	41.105370
3517.594769	603596.113571	41.110375
3517.500902	603350.449948	41.115380
3517.393924	603118.793217	41.120384
3517.197297	602880.540162	41.125389
3517.080083	602637.065034	41.130394
3516.723945	602402.779149	41.135399
3516.578910	602165.202216	41.140404
3516.697306	601945.344198	41.145408
3516.012053	601700.784961	41.150413
3516.091651	601481.723946	41.155418
3516.110404	601256.061645	41.160423
3515.601282	601031.027517	41.165428
3515.391793	600826.361725	41.170432
3515.285304	600610.314463	41.175437
3515.113980	600394.773383	41.180442
3514.855408	600191.404166	41.185447
3514.873675	599980.679972	41.190452
3514.308031	599780.554175	41.195456
3514.377897	599569.613434	41.200461
3514.305035	599374.458408	41.205466
3513.676157	599182.990772	41.210471
3513.799567	598985.395100	41.215476
3513.637767	598794.448056	41.220480
3513.235771	598589.067843	41.225485
3513.294100	598418.654087	41.230490
3512.923027	598234.337576	41.235495
3513.001972	598049.747239	41.240500
3512.352156	597875.730789	41.245504
3512.403058	597700.100004	41.250509
3512.571769	597533.209210	41.255514
3511.781190	597367.567184	41.260519
3512.039458	597189.993002	41.265524
3511.806002	597041.131109	41.270528
3511.291425	596868.929389	41.275533
3511.531430	596710.425852	41.280538
3511.211900	596554.811297	41.285543
3511.327373	596391.415650	41.290548
3511.133234	596243.337503	41.295552
3510.841129	596086.109502	41.300557
3511.047652	595932.606715	41.305562
3510.983165	595787.906850	41.310567
3510.607551	595637.995912	41.315572
3510.082052	595492.012089	41.320576
3510.296079	595353.171532	41.325581
3510.352363	595207.793902	41.330586
3509.675785	595072.494052	41.335591
3509.855985	594929.747293	41.340596
3509.430183	594803.418677	41.345600
3509.623994	594669.229566	41.350605
3509.517360	594532.030919	41.355610
3509.336119	594412.269840	41.360615
3509.600017	594282.772373	41.365620
3508.946228	594158.625185	41.370624
3508.837075	594035.192706	41.375629
3508.882961	593911.484151	41.380634
3508.571066	593789.482813	41.385639
3508.412969	593670.561179	41.390644
3508.526637	593562.263521	41.395648
3508.179899	593445.372207	41.400653
3508.139464	593331.987732	41.405658
3507.908519	593231.353439	41.410663
3508.515911	593113.007119	41.415668
3508.314847	593014.569879	41.420672
3508.024616	592898.114517	41.425677
3507.928320	592794.349692	41.430682
3507.324012	592684.702856	41.435687
3507.264388	592573.917895	41.440692
3507.513770	592483.920328	41.445696
3507.547709	592393.705240	41.450701
3507.417940	592289.690310	41.455706
3507.336467	592199.040820	41.460711
3507.404802	592094.141496	41.465716
3507.233003	591991.282318	41.470720
3507.432191	591896.078216	41.475725
3507.063506	591803.015805	41.480730
3506.694387	591720.421906	41.485735
3507.067882	591616.071306	41.490740
3507.070781	591531.213720	41.495744
3506.643792	591441.313142	41.500749
3506.349728	591343.876957	41.505754
3506.413291	591272.082326	41.510759
3506.560800	591188.602063	41.515764
3506.361907	591111.136604	41.520768
3506.643537	591025.580217	41.525773
3506.404822	590943.110239	41.530778
3505.899102	590854.469450	41.535783
3506.549571	590765.146219	41.540788
3506.284804	590697.256512	41.545792
3505.834415	590620.127413	41.550797
3506.067443	590541.888971	41.555802
3506.009866	590473.264095	41.560807
3506.066507	590387.387125	41.565812
3505.579228	590315.972817	41.570816
3505.739747	590242.252412	41.575821
3505.772266	590160.986514	41.580826
3505.367278	590093.415515	41.585831
3505.455498	590014.193889	41.590836
3505.686595	589952.033569	41.595840
3505.687915	589884.297542	41.600845
3505.793785	589812.536668	41.605850
3505.178986	589753.563602	41.610855
3505.440599	589682.729442	41.615860
3505.449319	589607.174671	41.620864
3505.148055	589532.870286	41.625869
3505.564009	589476.239679	41.630874
3505.027977	589414.196189	41.635879
3505.100154	589334.771675	41.640884
3505.985488	589288.838890	41.645888
3505.224201	589206.938355	41.650893
3505.140946	589153.891366	41.655898
3505.036071	589096.087590	41.660903
3504.940504	589024.904124	41.665908
3505.025534	588957.299514	41.670912
3505.093424	588898.665996	41.675917
3505.245395	588835.058573	41.680922
3504.661784	588786.146545	41.685927
3504.468546	588720.938928	41.690932
3504.440700	588667.029088	41.695936
3504.423995	588615.271818	41.700941
3504.764866	588560.451995	41.705946
3504.464949	588503.527360	41.710951
3504.510467	588447.750999	41.715956
3504.375185	588390.549496	41.720960
3504.650036	588337.743171	41.725965
3504.483302	588284.103677	41.730970
3504.557800	588236.689740	41.735975
3504.844615	588175.662997	41.740980
3504.952468	588131.350116	41.745984
3504.801688	588074.600348	41.750989
3504.492619	588003.694093	41.755994
3504.126253	587961.859902	41.760999
3504.077153	587907.699061	41.766004
3503.952827	587862.619622	41.771008
3504.146204	587809.572914	41.776013
3504.308539	587766.252231	41.781018
3504.235766	587715.802305	41.786023
3504.567051	587666.190975	41.791028
3504.623228	587621.382982	41.796032
3504.091202	587567.045381	41.801037
3504.153403	587506.701442	41.806042
3503.758294	587463.015689	41.811047
3503.865000	587419.251312	41.816052
3503.740996	587385.745718	41.821056
3503.985081	587331.636396	41.826061
3504.003282	587287.734988	41.831066
3503.380550	587256.862707	41.836071
3503.864014	587210.933857	41.841076
3503.829445	587165.236137	41.846080
3503.512632	587122.037904	41.851085
3503.771767	587087.569455	41.856090
3503.654913	587046.745115	41.861095
3504.037489	587001.883544	41.866100
3503.722839	586961.340375	41.871104
3503.861071	586909.500639	41.876109
3503.936804	586872.704804	41.881114
3503.663456	586838.569382	41.886119
3503.846105	586783.414531	41.891124
3503.612441	586749.322740	41.896128
3503.763389	586713.065874	41.901133
3503.834545	586667.098958	41.906138
3503.614718	586633.255218	41.911143
3503.650926	586588.245630	41.916148
3503.389211	586558.768286	41.921152
3503.403480	586512.258334	41.926157
3503.595968	586476.695816	41.931162
3503.251961	586445.126140	41.936167
3503.841298	586404.740277	41.941172
3503.812399	586360.792380	41.946176
3503.474438	586319.749296	41.951181
3503.788733	586278.804559	41.956186
3503.607712	586238.037337	41.961191
3503.720289	586195.620298	41.966196
3503.524807	586154.103258	41.971200
3503.476022	586115.018910	41.976205
3503.758121	586081.746526	41.981210
3503.485710	586042.245813	41.986215
3503.769722	586001.655600	41.991220
3503.691755	585971.195689	41.996224
3503.065476	585939.568438	42.001229
3503.376857	585897.469994	42.006234
3503.098474	585873.406257	42.011239
3503.540792	585829.482793	42.016244
3503.356089	585800.442432	42.021248
3503.304050	585761.758284	42.026253
3503.182761	585721.080031	42.031258
3503.170941	585692.714036	42.036263
3503.634783	585651.994173	42.041268
3503.544898	585616.573238	42.046272
3503.376902	585587.279097	42.051277
3503.367360	585545.630432	42.056282
3503.237587	585512.320462	42.061287
3503.505278	585472.081681	42.066292
3503.308051	585441.037483	42.071296
3503.578122	585391.675985	42.076301
3503.379416	585363.588957	42.081306
3503.371657	585341.937694	42.086311
3503.308952	585306.260896	42.091316
3503.122394	585276.567850	42.096320
3503.006992	585230.223075	42.101325
3502.886370	585202.173548	42.106330
3502.964517	585178.002419	42.111335
3503.572875	585144.074712	42.116340
3503.154817	585116.622811	42.121344
3503.120206	585084.098621	42.126349
3503.440831	585054.927159	42.131354
3503.112808	585024.553822	42.136359
3503.280091	584978.314158	42.141364
3502.820158	584945.605430	42.146368
3503.139742	584908.915230	42.151373
3503.582463	584883.383244	42.156378
3503.319752	584849.791296	42.161383
3503.492569	584809.063674	42.166388
3503.056378	584769.884708	42.171392
3502.805294	584733.984872	42.176397
3502.965813	584714.361160	42.181402
3502.857084	584686.960071	42.186407
3503.373506	584653.646717	42.191412
3503.301907	584625.287299	42.196416
3503.107523	584585.067373	42.201421
3503.242261	584560.284534	42.206426
3503.319787	584535.610833	42.211431
3503.304429	584492.505439	42.216436
3502.986353	584463.181624	42.221440
3502.934159	584432.663273	42.226445
3503.187839	584396.883927	42.231450
3503.151626	584371.926884	42.236455
3503.224238	584333.518958	42.241460
3502.993760	584303.529381	42.246464
3502.571558	584274.772729	42.251469
3503.183122	584249.263002	42.256474
3502.842698	584218.388101	42.261479
3502.862174	584198.986023	42.266484
3503.119441	584164.759292	42.271488
3502.957887	584133.054156	42.276493
3502.809630	584099.191378	42.281498
3502.961331	584076.259503	42.286503
3503.357693	584052.687804	42.291508
3503.117923	584029.065117	42.296512
3503.018111	583996.046616	42.301517
3503.018275	583962.912131	42.306522
3503.078812	583932.073998	42.311527
3503.257144	583899.513005	42.316532
3502.539129	583871.603590	42.321536
3502.723789	583855.182781	42.326541
3503.018562	583819.244745	42.331546
3502.992091	583797.493099	42.336551
3503.417134	583761.935541	42.341556
3502.856691	583725.178445	42.346560
3502.810732	583694.406422	42.351565
3502.839220	583662.219056	42.356570
3502.805707	583639.716260	42.361575
3503.298091	583611.717221	42.366580
3502.622639	583588.562731	42.371584
3502.611046	583551.017436	42.376589
3502.791395	583519.658118	42.381594
3503.036081	583500.119340	42.386599
3503.049933	583467.532652	42.391604
3503.027264	583446.030368	42.396608
3503.235153	583410.204840	42.401613
3503.253958	583386.039042	42.406618
3502.885275	583344.488293	42.411623
3502.897097	583315.962060	42.416628
3502.849303	583286.241930	42.421632
3502.523209	583245.035064	42.426637
3502.672653	583241.452415	42.431642
3502.732393	583210.461990	42.436647
3502.791721	583175.059972	42.441652
3502.506504	583158.561185	42.446656
3502.377982	583134.969315	42.451661
3502.600328	583114.731503	42.456666
3502.123506	583092.246757	42.461671
3502.784285	583059.056408	42.466676
3502.874053	583049.166391	42.471680
3502.464950	583023.011277	42.476685
3502.814680	582991.473580	42.481690
3502.502229	582981.445851	42.486695
3502.810561	582952.421132	42.491700
3502.619649	582920.967752	42.496704
3502.375508	582896.491057	42.501709
3503.027122	582878.140882	42.506714
3502.609825	582857.902328	42.511719
3502.645109	582825.210123	42.516724
3502.415671	582813.214073	42.521728
3502.686575	582770.909441	42.526733
3502.926547	582752.071942	42.531738
3502.596430	582728.510715	42.536743
3502.780483	582706.322934	42.541748
3503.127511	582682.806153	42.546752
3502.685713	582663.573746	42.551757
3502.733185	582628.322227	42.556762
3502.869983	582612.508657	42.561767
3502.610644	582583.521578	42.566772
3502.727695	582562.697605	42.571776
3502.623734	582538.849946	42.576781
3503.021925	582507.253156	42.581786
3502.659057	582488.108372	42.586791
3502.483557	582446.774706	42.591796
3502.619242	582436.676424	42.596800
3502.340435	582410.850428	42.601805
3502.817476	582389.969852	42.606810
3502.739873	582365.766754	42.611815
3502.883339	582336.615785	42.616820
3502.717106	582316.888475	42.621824
3502.545945	582275.603624	42.626829
3502.747321	582251.055848	42.631834
3502.447194	582234.708413	42.636839
3502.430436	582217.965704	42.641844
3502.647442	582199.682348	42.646848
3502.474447	582168.173882	42.651853
3502.673933	582146.534060	42.656858
3502.576198	582125.943386	42.661863
3502.192250	582101.837735	42.666868
3502.427783	582078.788328	42.671872
3502.663758	582062.707784	42.676877
3502.968434	582034.884504	42.681882
3502.391311	582032.367646	42.686887
3502.409497	581988.495150	42.691892
3502.572742	581975.634610	42.696896
3502.359946	581960.025168	42.701901
3502.533807	581931.169200	42.706906
3502.100276	581907.622385	42.711911
3502.634204	581887.283478	42.716916
3502.600773	581867.233780	42.721920
3502.048846	581846.613313	42.726925
3502.307124	581821.704726	42.731930
3502.374347	581813.271118	42.736935
3502.653439	581786.002726	42.741940
3502.562741	581763.555178	42.746944
3502.506551	581746.266401	42.751949
3502.658930	581713.251770	42.756954
3502.803456	581693.324351	42.761959
3502.553293	581660.823736	42.766964
3502.902099	581652.947648	42.771968
3502.752276	581618.726518	42.776973
3503.150694	581595.399948	42.781978
3502.649549	581573.567703	42.786983
3502.994154	581542.678480	42.791988
3502.818026	581517.436008	42.796993
3502.665279	581481.209349	42.801997
3502.798144	581454.063278	42.807002
3503.236963	581437.198027	42.812007
3502.946680	581404.652792	42.817012
3503.109488	581383.067352	42.822017
3502.791009	581353.685170	42.827021
3502.973998	581319.661786	42.832026
3502.424669	581297.335128	42.837031
3502.831948	581261.521601	42.842036
3502.781386	581251.300933	42.847041
3502.580517	581224.056050	42.852045
3502.966978	581201.081503	42.857050
3502.457527	581175.790078	42.862055
3502.299907	581144.075726	42.867060
3502.418061	581121.042676	42.872065
3502.532685	581098.962807	42.877069
3502.932569	581082.303668	42.882074
3502.760975	581058.463387	42.887079
3502.648546	581036.719736	42.892084
3502.590038	581014.466200	42.897089
3502.384645	580982.307581	42.902093
3502.709770	580953.726269	42.907098
3502.552196	580928.028277	42.912103
3502.736843	580916.867981	42.917108
3502.818363	580886.820326	42.922113
3502.802959	580863.005349	42.927117
3502.576717	580836.766319	42.932122
3502.603970	580810.537740	42.937127
3502.406713	580789.157860	42.942132
3502.630209	580764.001623	42.947137
3502.325505	580744.594007	42.952141
3502.708143	580715.301095	42.957146
3502.478060	580698.489151	42.962151
3502.215109	580661.023468	42.967156
3502.153529	580654.514545	42.972161
3502.446866	580629.296942	42.977165
3502.049265	580615.920786	42.982170
3502.147263	580600.912698	42.987175
3502.388480	580583.074181	42.992180
3502.430920	580560.503092	42.997185
3502.222529	580539.575761	43.002189
3502.514523	580526.643270	43.007194
3502.273818	580505.771070	43.012199
3502.597846	580490.727499	43.017204
3502.769652	580470.342324	43.022209
3502.607403	580435.668187	43.027213
3502.502072	580417.181564	43.032218
3502.004782	580386.771745	43.037223
3502.278594	580375.296101	43.042228
3502.085466	580357.876132	43.047233
3502.381211	580336.568740	43.052237
3502.379039	580320.322324	43.057242
3501.881294	580301.295121	43.062247
3502.004655	580284.427294	43.067252
3502.345364	580264.817652	43.072257
3501.721249	580255.939346	43.077261
3501.846140	580240.374976	43.082266
3502.217359	580224.320772	43.087271
3502.309238	580212.823257	43.092276
3502.332811	580196.572636	43.097281
3502.126609	580191.339674	43.102285
3502.326216	580166.837705	43.107290
3502.531395	580138.172757	43.112295
3502.510530	580114.808335	43.117300
3502.508188	580101.520202	43.122305
3501.795343	580079.868537	43.127309
3502.145049	580052.735285	43.132314
3502.403064	580055.402841	43.137319
3502.258887	580031.706503	43.142324
3502.497430	580015.722886	43.147329
3501.721841	579993.027797	43.152333
3501.987302	579967.712761	43.157338
3501.866363	579962.115339	43.162343
3502.046682	579956.119796	43.167348
3502.083189	579920.109180	43.172353
3502.106377	579925.571520	43.177357
3502.261482	579899.320802	43.182362
3502.186079	579891.660227	43.187367
3502.091151	579875.929126	43.192372
3501.898815	579842.962819	43.197377
3502.263860	579836.637455	43.202381
3502.383997	579818.365321	43.207386
3502.232564	579808.309532	43.212391
3501.980329	579791.299088	43.217396
3502.012097	579764.766452	43.222401
3501.930606	579758.811733	43.227405
3502.273517	579740.905821	43.232410
3501.793794	579728.594517	43.237415
3501.742526	579717.169015	43.242420
3502.475925	579710.635554	43.247425
3502.214461	579694.629348	43.252429
3502.502809	579670.664034	43.257434
3502.058213	579637.836850	43.262439
3502.113440	579630.707296	43.267444
3502.252590	579603.204685	43.272449
3502.171836	579592.285142	43.277453
3502.151619	579573.733661	43.282458
3502.209594	579564.597723	43.287463
3502.122711	579560.699801	43.292468
3502.191966	579535.113568	43.297473
3502.334051	579519.194466	43.302477
3502.668526	579491.109415	43.307482
3502.413136	579478.662467	43.312487
3502.408412	579448.323517	43.317492
3502.615403	579436.105128	43.322497
3502.116104	579411.460015	43.327501
3502.651204	579394.877513	43.332506
3502.616041	579384.401976	43.337511
3502.692468	579357.560497	43.342516
3502.393704	579336.745323	43.347521
3502.496197	579328.454763	43.352525
3502.404574	579286.043064	43.357530
3502.380480	579280.480308	43.362535
3502.467635	579251.380186	43.367540
3502.560654	579234.114318	43.372545
3502.306062	579213.091410	43.377549
3502.680446	579188.961163	43.382554
3502.672758	579170.657800	43.387559
3502.933139	579138.922525	43.392564
3502.912842	579117.912959	43.397569
3502.766083	579090.654380	43.402573
3502.874088	579059.995850	43.407578
3502.773929	579042.509134	43.412583
3502.948691	579013.595297	43.417588
3502.783826	578978.917025	43.422593
3502.535845	578961.252689	43.427597
3502.909025	578922.076879	43.432602
3502.588770	578904.975410	43.437607
3502.329239	578885.106122	43.442612
3502.608915	578859.284839	43.447617
3502.473687	578836.888483	43.452621
3502.658003	578806.317628	43.457626
3502.501862	578795.208483	43.462631
3502.540838	578776.947330	43.467636
3502.730702	578755.352562	43.472641
3502.509699	578737.834108	43.477645
3502.353452	578706.864857	43.482650
3502.403247	578680.928644	43.487655
3502.347511	578667.095476	43.492660
3502.516615	578646.005261	43.497665
3502.668461	578621.908580	43.502669
3502.561978	578601.362883	43.507674
3502.389696	578579.774238	43.512679
3502.506273	578559.895726	43.517684
3502.898287	578531.046982	43.522689
3502.667856	578510.570647	43.527693
3502.611844	578479.835859	43.532698
3502.549558	578459.032228	43.537703
3502.503702	578434.163604	43.542708
3502.594138	578413.336012	43.547713
3502.175245	578387.572693	43.552717
3502.524942	578363.946057	43.557722
3502.557725	578349.346359	43.562727
3502.531079	578325.327095	43.567732
3502.772051	578301.867786	43.572737
3502.442734	578275.839438	43.577741
3502.226177	578256.413694	43.582746
3502.594983	578238.200406	43.587751
3502.371504	578215.164598	43.592756
3502.090472	578189.429423	43.597761
3501.691261	578178.407816	43.602765
3502.061491	578150.363960	43.607770
3501.977021	578148.621796	43.612775
3501.859264	578129.681928	43.617780
3502.150926	578123.517536	43.622785
3501.865536	578113.481156	43.627789
3502.117506	578097.693314	43.632794
3502.393932	578087.970319	43.637799
3502.319809	578064.660079	43.642804
3502.162279	578051.092834	43.647809
3501.878159	578024.555288	43.652813
3502.136819	578018.947700	43.657818
3502.003072	578006.680707	43.662823
3502.128436	577987.552127	43.667828
3502.351332	577963.593385	43.672833
3502.531254	577961.007379	43.677837
3502.169112	577939.547486	43.682842
3502.179892	577924.449121	43.687847
3501.865428	577884.424226	43.692852
3502.162482	577884.929525	43.697857
3502.042498	577868.697953	43.702861
3502.182071	577846.457272	43.707866
3501.751342	577835.640874	43.712871
3501.738059	577808.458607	43.717876
3501.936332	577797.092438	43.722881
3501.950798	577800.801732	43.727885
3502.288629	577772.109970	43.732890
3501.730341	577768.586049	43.737895
3502.114549	577752.726893	43.742900
3501.995168	577730.927712	43.747905
3501.878464	577718.607582	43.752909
3501.933479	577724.116182	43.757914
3501.950780	577700.339486	43.762919
3501.937401	577680.329259	43.767924
3501.703475	577679.061792	43.772929
3501.835014	577650.201343	43.777933
3502.224739	577636.397573	43.782938
3502.005337	577634.877048	43.787943
3501.661513	577612.561002	43.792948
3502.262044	577598.623917	43.797953
3501.782700	577594.285093	43.802957
3502.233405	577562.365121	43.807962
3502.267959	577543.350292	43.812967
3502.206681	577527.510303	43.817972
3501.950457	577515.863802	43.822977
3502.113352	577508.064021	43.827981
3502.485393	577492.106084	43.832986
3502.180056	577481.821468	43.837991
3502.105744	577455.400243	43.842996
3502.422018	577435.789460	43.848001
3502.086248	577430.525293	43.853005
3502.471004	577406.590215	43.858010
3502.072490	577395.918826	43.863015
3502.044511	577371.947881	43.868020
3501.886525	577356.674503	43.873025
3501.908831	577348.194380	43.878029
3502.229659	577322.965015	43.883034
3502.030035	577307.196500	43.888039
3502.024534	577300.225427	43.893044
3502.192907	577282.342870	43.898049
3501.710619	577278.656436	43.903053
3502.049277	577257.035518	43.908058
3502.165297	577244.377535	43.913063
3501.840542	577228.427838	43.918068
3502.173000	577212.224900	43.923073
3501.907419	577181.770099	43.928077
3502.050145	577181.145912	43.933082
3502.276601	577171.881363	43.938087
3502.249932	577143.545928	43.943092
3502.509777	577125.097075	43.948097
3502.288516	577107.224991	43.953101
3502.515901	577091.740530	43.958106
3501.983901	577064.436913	43.963111
3502.026635	577053.495580	43.968116
3501.798499	577029.304397	43.973121
3501.944136	577018.497421	43.978125
3502.302734	577007.606983	43.983130
3502.444369	576992.587224	43.988135
3502.259336	576966.834228	43.993140
3502.388217	576947.653164	43.998145
3501.959655	576942.102314	44.003149
3502.160156	576928.026300	44.008154
3502.149381	576908.917162	44.013159
3502.121482	576891.766902	44.018164
3502.303372	576868.664950	44.023169
3501.908876	576861.302976	44.028173
3502.057266	576846.733406	44.033178
3501.651171	576824.174721	44.038183
3501.882562	576815.511030	44.043188
3501.914573	576805.072733	44.048193
3502.044255	576788.650084	44.053197
3502.297380	576766.188869	44.058202
3502.068992	576759.954549	44.063207
3501.767189	576731.259801	44.068212
3502.032208	576725.148970	44.073217
3501.828792	576718.710082	44.078221
3501.955723	576692.957847	44.083226
3501.798800	576685.157332	44.088231
3501.975267	576674.646170	44.093236
3501.821511	576654.405253	44.098241
3501.611360	576640.493397	44.103245
3502.078146	576633.999848	44.108250
3501.953514	576626.194244	44.113255
3501.913242	576615.466104	44.118260
3502.077175	576602.097653	44.123265
3502.089871	576592.765723	44.128269
3501.790737	576563.969807	44.133274
3502.077308	576559.260034	44.138279
3501.722044	576548.480750	44.143284
3501.715849	576519.337956	44.148289
3501.844983	576519.719088	44.153293
3502.212689	576515.046774	44.158298
3502.394012	576498.314660	44.163303
3502.033563	576478.707677	44.168308
3502.110873	576465.804060	44.173313
3502.004929	576449.417752	44.178317
3502.278692	576429.310242	44.183322
3502.218545	576411.211213	44.188327
3501.666591	576387.169591	44.193332
3502.137987	576377.565126	44.198337
3501.867370	576364.164001	44.203341
3501.957928	576340.473295	44.208346
3502.232807	576339.075968	44.213351
3501.959413	576307.666931	44.218356
3502.022731	576296.571155	44.223361
3502.063994	576298.169932	44.228365
3502.020183	576274.449930	44.233370
3502.116552	576262.696841	44.238375
3502.169645	576239.764219	44.243380
3502.541536	576224.105486	44.248385
3502.094293	576212.286838	44.253389
3502.224224	576179.660645	44.258394
3502.225181	576189.442306	44.263399
3502.272995	576151.762408	44.268404
3502.306836	576146.389689	44.273409
3502.271079	576126.631005	44.278413
3502.272361	576106.966822	44.283418
3502.313596	576097.278876	44.288423
3502.312617	576075.156986	44.293428
3502.254552	576048.529254	44.298433
3502.175922	576036.853450	44.303437
3501.716021	576026.792313	44.308442
3501.825935	575996.676903	44.313447
3501.824863	575988.701047	44.318452
3501.986851	575975.733467	44.323457
3501.972046	575974.281056	44.328461
3502.015535	575948.740818	44.333466
3501.783510	575949.780398	44.338471
3501.996399	575937.105801	44.343476
3502.333860	575911.770344	44.348481
3501.968224	575905.155690	44.353485
3502.058792	575882.316810	44.358490
3501.917043	575865.985412	44.363495
3501.881719	575872.412004	44.368500
3502.348543	575849.263415	44.373505
3502.166806	575830.881473	44.378509
3502.613303	575809.993387	44.383514
3502.322941	575787.213865	44.388519
3502.102699	575779.522947	44.393524
3502.339359	575751.594318	44.398529
3501.993640	575738.304516	44.403533
3502.080708	575714.613038	44.408538
3501.993171	575705.045216	44.413543
3501.880481	575693.424545	44.418548
3502.133751	575672.415916	44.423553
3502.020258	575666.765009	44.428557
3502.212399	575651.083416	44.433562
3501.948364	575629.754254	44.438567
3501.975645	575625.285290	44.443572
3501.991893	575612.340077	44.448577
3501.838099	575584.321576	44.453581
3501.954821	575574.621380	44.458586
3501.628838	575569.856459	44.463591
3501.652411	575542.261618	44.468596
3501.862958	575529.035105	44.473601
3501.710147	575534.828099	44.478605
3501.750539	575523.333819	44.483610
3501.791198	575506.070396	44.488615
3502.080439	575488.166093	44.493620
3502.326723	575493.344891	44.498625
3501.940322	575468.924257	44.503629
3501.982589	575459.787429	44.508634
3502.143998	575456.702084	44.513639
3501.622486	575430.245672	44.518644
3501.747801	575411.213047	44.523649
3501.990796	575411.626586	44.528653
3502.251766	575388.308568	44.533658
3502.363774	575374.946779	44.538663
3501.801655	575357.275694	44.543668
3502.207115	575330.322968	44.548673
3501.911450	575330.369216	44.553677
3501.928085	575308.794902	44.558682
3501.964371	575290.678995	44.563687
3501.910823	575283.814517	44.568692
3501.940337	575274.880201	44.573697
3501.843401	575260.547600	44.578701
3501.996958	575248.734347	44.583706
3502.143562	575239.480696	44.588711
3501.982646	575216.980785	44.593716
3501.945218	575205.799351	44.598721
3502.200722	575204.756089	44.603725
3501.940381	575174.295025	44.608730
3502.109619	575171.258546	44.613735
3502.190042	575147.767586	44.618740
3502.223510	575125.688614	44.623745
3502.056717	575125.413710	44.628749
3502.019980	575091.907405	44.633754
3502.116280	575082.912329	44.638759
3501.967419	575068.587601	44.643764
3501.599962	575046.420646	44.648769
3501.807037	575043.629058	44.653773
3501.616943	575039.344349	44.658778
3502.221413	575028.865081	44.663783
3501.736229	574998.689532	44.668788
3501.943710	574997.703927	44.673793
3501.887533	574994.351462	44.678797
3502.079285	574967.230606	44.683802
3502.197450	574966.860982	44.688807
3502.052454	574940.444894	44.693812
3502.408696	574925.539337	44.698817
3501.836406	574907.267111	44.703821
3502.017832	574877.237869	44.708826
3502.048980	574872.015470	44.713831
3501.836905	574855.844107	44.718836
3502.305781	574830.335174	44.723841
3501.487559	574839.694208	44.728845
3501.899366	574828.843524	44.733850
3502.183448	574826.491366	44.738855
3501.663573	574819.448660	44.743860
3501.841451	574800.005436	44.748865
3501.612557	574772.096995	44.753869
3501.672185	574757.036908	44.758874
3501.610881	574758.702108	44.763879
3501.703749	574754.824578	44.768884
3501.846097	574739.249843	44.773889
3502.009675	574723.972784	44.778893
3501.701960	574709.722603	44.783898
3502.057978	574710.971383	44.788903
3501.816394	574686.626752	44.793908
3502.067807	574673.693868	44.798913
3501.465084	574664.807737	44.803917
3501.592017	574659.118738	44.808922
3501.646410	574635.329763	44.813927
3501.548435	574630.930157	44.818932
3502.003770	574622.029096	44.823937
3501.676482	574624.237595	44.828941
3501.511925	574606.402838	44.833946
3501.752455	574589.056597	44.838951
3501.674176	574585.406445	44.843956
3501.820686	574570.232188	44.848961
3501.793339	574565.068962	44.853965
3501.742031	574543.252955	44.858970
3501.364852	574537.040658	44.863975
3501.573797	574533.997802	44.868980
3501.693724	574528.360003	44.873985
3501.685025	574515.567942	44.878989
3501.936028	574498.219925	44.883994
3501.637898	574489.235867	44.888999
3501.375881	574493.541350	44.894004
3501.788599	574486.101790	44.899009
3501.735390	574470.707768	44.904013
3501.812510	574459.056151	44.909018
3501.768372	574453.443963	44.914023
3501.849223	574449.166842	44.919028
3502.165553	574423.329645	44.924033
3502.087059	574416.619051	44.929037
3502.116429	574397.499376	44.934042
3501.825513	574377.576832	44.939047
3501.893902	574367.682472	44.944052
3501.658490	574359.792270	44.949057
3501.636600	574351.567655	44.954061
3501.630435	574338.072601	44.959066
3501.439003	574331.229099	44.964071
3501.469417	574333.582419	44.969076
3501.954414	574319.458677	44.974081
3501.436749	574308.000230	44.979085
3502.031735	574292.053091	44.984090
3501.512180	574299.208506	44.989095
3501.255699	574287.207493	44.994100
3501.753890	574279.854779	44.999105
3501.400418	574255.024994	45.004109
3501.525532	574240.756728	45.009114
3501.876829	574244.464709	45.014119
3501.721196	574243.686321	45.019124
3502.187230	574229.966805	45.024129
3501.890918	574209.492919	45.029133
3501.317801	574205.970173	45.034138
3501.752992	574199.831380	45.039143
3501.813121	574188.131969	45.044148
3501.700494	574172.897346	45.049153
3501.901765	574167.748370	45.054157
3502.010349	574153.382235	45.059162
3501.705314	574139.883495	45.064167
3501.895552	574130.622116	45.069172
3502.087204	574128.133748	45.074177
3502.109367	574113.831245	45.079181
3502.448035	574097.422181	45.084186
3502.027498	574081.934537	45.089191
3502.065056	574056.039738	45.094196
3502.239336	574042.917503	45.099201
3501.766985	574032.455141	45.104205
3501.792607	573999.889128	45.109210
3501.665415	574005.929762	45.114215
3501.683061	574005.023922	45.119220
3501.959263	573978.288875	45.124225
3501.952385	573969.710427	45.129229
3502.079615	573960.809970	45.134234
3502.256734	573948.991677	45.139239
3502.105398	573929.146867	45.144244
3501.676101	573912.857592	45.149249
3501.486341	573901.799027	45.154253
3501.865437	573885.684376	45.159258
3501.866854	573879.713569	45.164263
3501.768336	573881.635581	45.169268
3501.967070	573854.510967	45.174273
3501.800751	573846.308563	45.179277
3501.622541	573837.455759	45.184282
3501.828032	573826.485851	45.189287
3501.691047	573802.373829	45.194292
3502.391191	573790.774649	45.199297
3502.142050	573792.017792	45.204301
3501.893848	573763.457620	45.209306
3501.927845	573756.026616	45.214311
3501.974620	573737.003453	45.219316
3501.815236	573711.439697	45.224321
3501.385819	573718.079644	45.229325
3501.606582	573707.107234	45.234330
3501.771964	573701.311396	45.239335
3501.721129	573675.931287	45.244340
3502.191963	573662.210336	45.249345
3501.967833	573666.660730	45.254349
3501.936246	573645.542348	45.259354
3501.853672	573632.158746	45.264359
3501.433471	573625.601450	45.269364
3501.992017	573621.450037	45.274369
3502.030587	573598.765194	45.279373
3502.131200	573589.868607	45.284378
3501.989410	573567.512944	45.289383
3502.018685	573551.201634	45.294388
3502.175391	573540.941523	45.299393
3501.951530	573530.891420	45.304397
3501.973699	573510.466830	45.309402
3502.112701	573500.711199	45.314407
3501.517349	573483.192890	45.319412
3501.906718	573463.112210	45.324417
3501.824371	573460.616356	45.329421
3501.671502	573461.292558	45.334426
3502.139527	573444.460929	45.339431
3501.554225	573430.403052	45.344436
3502.266923	573419.002234	45.349441
3501.433976	573397.607263	45.354445
3501.921975	573392.312763	45.359450
3502.235356	573388.952224	45.364455
3501.638575	573369.928700	45.369460
3501.808655	573348.627712	45.374465
3501.578122	573347.559916	45.379469
3501.826553	573343.206005	45.384474
3501.919400	573341.987303	45.389479
3501.879148	573321.622306	45.394484
3501.990657	573300.531087	45.399489
3501.814637	573296.895798	45.404493
3501.900598	573277.163276	45.409498
3501.945721	573264.060332	45.414503
3502.115706	573261.274108	45.419508
3501.794621	573233.627161	45.424513
3501.750035	573231.526763	45.429517
3501.849566	573217.813147	45.434522
3501.869722	573207.523906	45.439527
3501.745565	573191.788002	45.444532
3501.840490	573183.795160	45.449537
3501.792447	573171.158260	45.454541
3501.891442	573153.280011	45.459546
3502.242548	573138.172206	45.464551
3501.474953	573132.672460	45.469556
3501.855990	573117.911185	45.474561
3501.615433	573108.967203	45.479565
3501.974474	573091.951384	45.484570
3501.743665	573091.435550	45.489575
3501.774803	573085.359325	45.494580
3501.820412	573056.450379	45.499585
3501.708610	573052.654441	45.504589
3502.069271	573051.594549	45.509594
3502.159768	573024.535050	45.514599
3501.671834	573018.188696	45.519604
3502.429741	573005.375441	45.524609
3501.676134	572999.823266	45.529613
3501.947597	572973.839252	45.534618
3502.040269	572972.971780	45.539623
3501.842295	572957.397623	45.544628
3502.023408	572940.208683	45.549633
3501.572867	572944.594398	45.554637
3501.751448	572923.742881	45.559642
3501.982423	572892.345843	45.564647
3501.550319	572893.015552	45.569652
3502.283789	572884.571433	45.574657
3501.892917	572868.224467	45.579661
3501.865762	572841.734880	45.584666
3501.804106	572848.468372	45.589671
3501.448289	572824.840081	45.594676
3501.588218	572817.592614	45.599681
3501.234696	572821.662141	45.604685
3501.426614	572813.402986	45.609690
3501.987605	572816.576880	45.614695
3501.691278	572821.440313	45.619700
3500.947878	572785.880003	45.624705
3501.372055	572777.333623	45.629709
3501.477243	572764.521781	45.634714
3501.767051	572764.677216	45.639719
3501.538093	572762.204128	45.644724
3501.932884	572758.328896	45.649729
3501.333792	572745.677312	45.654733
3501.450626	572732.261474	45.659738
3501.728865	572724.139295	45.664743
3501.365747	572715.113805	45.669748
3501.434625	572712.092361	45.674753
3501.622821	572726.112911	45.679757
3501.472937	572705.111628	45.684762
3501.371829	572682.547147	45.689767
3501.719725	572696.542767	45.694772
3501.596753	572681.056863	45.699777
3501.718386	572687.711618	45.704781
3501.573946	572675.892093	45.709786
3501.605129	572655.765627	45.714791
3501.255509	572639.813311	45.719796
3501.985891	572641.907022	45.724801
3501.532283	572638.465452	45.729805
3501.461556	572639.781183	45.734810
3501.579004	572617.282763	45.739815
3501.532949	572614.630513	45.744820
3501.631170	572589.575924	45.749825
3501.566553	572535.041417	45.754829
3501.600447	572433.573396	45.759834
3501.350567	572273.989980	45.764839
3500.881171	572079.612951	45.769844
3500.890986	571827.347828	45.774849
3500.531223	571536.744526	45.779853
3500.221360	571198.701233	45.784858
3499.993801	570800.762354	45.789863
3499.111084	570369.335851	45.794868
3498.507233	569884.546951	45.799873
3497.538287	569365.562979	45.804877
3496.558261	568802.435464	45.809882
3495.961887	568198.007752	45.814887
3495.201427	567559.638181	45.819892
3494.177717	566857.917170	45.824897
3492.849805	566125.022528	45.829901
3492.038598	565349.974635	45.834906
3490.835660	564544.305801	45.839911
3489.763505	563692.611732	45.844916
3487.963586	562787.835066	45.849921
3486.556376	561864.645064	45.854925
3485.258150	560895.405467	45.859930
3483.229159	559902.690996	45.864935
3481.801607	558870.211482	45.869940
3480.139160	557801.504109	45.874945
3478.430995	556710.850368	45.879949
3476.097570	555575.118734	45.884954
3474.664206	554406.974357	45.889959
3472.267718	553212.529930	45.894964
3469.986562	551994.273622	45.899969
3468.356174	550751.813408	45.904973
3466.075822	549464.028138	45.909978
3463.842551	548150.204255	45.914983
3461.372160	546824.760900	45.919988
3459.338139	545463.297766	45.924993
3456.617189	544076.441568	45.929997
3454.374917	542675.371223	45.935002
3451.898994	541242.685929	45.940007
3449.177986	539793.422103	45.945012
3446.569259	538314.233843	45.950017
3444.049089	536835.110983	45.955021
3441.092841	535303.587485	45.960026
3438.478467	533783.657574	45.965031
3435.582259	532236.959298	45.970036
3432.435518	530675.060198	45.975041
3429.739061	529105.047507	45.980045
3426.813364	527502.548443	45.985050
3424.272917	525905.083095	45.990055
3421.102644	524287.826235	45.995060
3417.888497	522631.988042	46.000065
3415.016721	520991.915442	46.005069
3411.477329	519323.123056	46.010074
3408.520492	517660.687154	46.015079
3404.945879	515979.796766	46.020084
3402.337244	514291.894768	46.025089
3398.671596	512578.842425	46.030093
3395.637815	510871.127762	46.035098
3392.467397	509147.289141	46.040103
3389.020148	507422.626835	46.045108
3385.793531	505683.292675	46.050113
3382.278182	503941.672379	46.055117
3378.684557	502180.628619	46.060122
3375.267537	500412.731709	46.065127
3371.423305	498654.477601	46.070132
3368.449265	496881.642028	46.075137
3364.553047	495106.516083	46.080141
3361.044601	493332.934583	46.085146
3357.604901	491543.226197	46.090151
3353.675866	489763.683232	46.095156
3350.404266	487965.949378	46.100161
3346.735447	486190.341271	46.105165
3343.193005	484395.816730	46.110170
3339.485961	482603.736945	46.115175
3335.785198	480819.332557	46.120180
3332.502431	479007.270136	46.125185
3328.341052	477208.176838	46.130189
3324.779041	475406.613103	46.135194
3321.449824	473617.347535	46.140199
3317.306516	471814.107946	46.145204
3314.003658	470004.722561	46.150209
3310.135227	468211.762029	46.155213
3306.219158	466397.474642	46.160218
3302.930716	464593.766195	46.165223
3298.718994	462801.997015	46.170228
3295.192677	460988.025450	46.175233
3291.321637	459195.165040	46.180237
3287.475643	457395.991095	46.185242
3283.889035	455590.719544	46.190247
3279.847542	453795.100569	46.195252
3276.310855	451988.843267	46.200257
3272.100840	450208.223227	46.205261
3268.425784	448424.608615	46.210266
3264.862138	446621.408511	46.215271
3261.046663	444845.362180	46.220276
3257.548892	443050.205112	46.225281
3253.647138	441272.815205	46.230285
3249.783737	439486.892639	46.235290
3245.934094	437694.567831	46.240295
3242.004586	435918.399010	46.245300
3238.235744	434135.656531	46.250305
3234.505871	432368.400427	46.255309
3230.895724	430591.033169	46.260314
3226.764886	428822.759544	46.265319
3222.956851	427061.677586	46.270324
3219.279398	425294.033573	46.275329
3215.390263	423536.102233	46.280333
3211.436398	421773.669448	46.285338
3207.442960	420019.153245	46.290343
3203.713313	418280.875934	46.295348
3200.232365	416533.237077	46.300353
3196.659108	414777.861151	46.305357
3192.587541	413037.532614	46.310362
3188.998491	411290.597081	46.315367
3184.932194	409555.820761	46.320372
3181.372727	407823.263146	46.325377
3177.129678	406077.435513	46.330381
3173.704975	404351.841770	46.335386
3169.752728	402626.706215	46.340391
3165.866186	400907.113492	46.345396
3161.650429	399182.470588	46.350401
3158.278893	397473.199811	46.355405
3154.601134	395763.395922	46.360410
3150.707339	394046.903988	46.365415
3146.447403	392350.499760	46.370420
3143.168841	390658.900152	46.375425
3138.867702	388957.367261	46.380429
3135.109733	387262.639361	46.385434
3131.363795	385569.292774	46.390439
3127.406448	383884.447875	46.395444
3123.662235	382208.066558	46.400449
3119.838188	380530.446284	46.405453
3115.768853	378865.555919	46.410458
3112.243062	377189.148596	46.415463
3108.478757	375536.293996	46.420468
3104.750809	373870.124535	46.425473
3101.237910	372209.382774	46.430477
3096.977780	370546.600384	46.435482
3093.330814	368897.519512	46.440487
3089.546446	367265.716295	46.445492
3085.592305	365613.215620	46.450497
3081.879751	363979.207586	46.455501
3078.382421	362338.036061	46.460506
3074.502770	360703.415103	46.465511
3070.551878	359083.506668	46.470516
3066.967277	357445.918554	46.475521
3063.321849	355824.823861	46.480525
3059.374443	354199.396487	46.485530
3055.800011	352580.308696	46.490535
3052.188259	350975.100075	46.495540
3048.424703	349354.227063	46.500545
3044.422837	347745.361276	46.505549
3041.040284	346147.964619	46.510554
3037.479336	344537.604318	46.515559
3033.218363	342934.015290	46.520564
3029.802830	341327.371850	46.525569
3026.155857	339726.844582	46.530573
3022.450843	338128.568394	46.535578
3018.742746	336534.901032	46.540583
3014.644487	334948.066312	46.545588
3010.990820	333352.091077	46.550593
3007.267179	331772.667312	46.555597
3003.493277	330189.523544	46.560602
2999.747233	328605.674930	46.565607
2996.094264	327038.612629	46.570612
2992.688851	325465.650440	46.575617
2989.159616	323891.629187	46.580621
2985.360941	322323.263106	46.585626
2981.510642	320746.959893	46.590631
2977.416884	319182.695777	46.595636
2974.147506	317622.164453	46.600641
2970.505457	316071.050218	46.605645
2966.380912	314508.915030	46.610650
2962.888061	312941.665812	46.615655
2958.825630	311408.830202	46.620660
2955.498680	309847.685840	46.625665
2951.599748	308317.091912	46.630669
2947.704951	306780.163855	46.635674
2943.949035	305240.571018	46.640679
2940.442974	303701.656084	46.645684
2936.932932	302160.431089	46.650689
2933.238621	300640.823709	46.655693
2929.150797	299114.235854	46.660698
2925.811681	297584.841601	46.665703
2921.962177	296067.372400	46.670708
2918.174893	294538.730043	46.675713
2914.601383	293022.843716	46.680717
2910.917008	291512.282151	46.685722
2907.315617	289995.968389	46.690727
2903.513526	288493.319678	46.695732
2900.019845	286982.848738	46.700737
2896.039768	285474.735975	46.705741
2892.351766	283971.457388	46.710746
2888.750750	282477.017783	46.715751
2885.203269	280975.689894	46.720756
2881.510035	279492.099523	46.725761
2878.023360	277983.420031	46.730765
2874.073398	276491.002120	46.735770
2870.781118	274995.627156	46.740775
2866.580271	273513.174276	46.745780
2863.294989	272018.915961	46.750785
2859.384220	270538.428759	46.755789
2855.369230	269060.505277	46.760794
2852.064299	267586.037622	46.765799
2848.163219	266115.434734	46.770804
2844.593227	264642.772179	46.775809
2841.079947	263180.316548	46.780813
2837.041357	261720.113151	46.785818
2833.998719	260248.733938	46.790823
2830.020096	258788.942008	46.795828
2826.770210	257331.565152	46.800833
2823.011797	255866.407540	46.805837
2819.214882	254406.282163	46.810842
2815.619052	252939.717947	46.815847
2812.098824	251500.325936	46.820852
2808.468245	250038.399418	46.825857
2804.665007	248591.639965	46.830861
2800.758955	247137.728206	46.835866
2797.256651	245686.645256	46.840871
2793.844309	244245.291874	46.845876
2790.199841	242805.060221	46.850881
2785.694849	241371.142977	46.855885
2782.412086	239933.639127	46.860890
2779.050822	238502.048777	46.865895
2775.248120	237063.491435	46.870900
2771.933510	235637.993586	46.875905
2767.819691	234222.344604	46.880909
2764.281289	232797.177696	46.885914
2761.079571	231365.383346	46.890919
2757.118031	229946.439212	46.895924
2753.947361	228522.377096	46.900929
2749.776387	227109.013942	46.905933
2746.273808	225695.596234	46.910938
2742.541060	224273.427434	46.915943
2739.011628	222866.254007	46.920948
2735.653221	221445.658235	46.925953
2731.606236	220041.624949	46.930957
2727.947742	218634.145999	46.935962
2724.442704	217225.780266	46.940967
2720.506591	215829.965508	46.945972
2716.800593	214417.233453	46.950977
2713.632136	213024.339013	46.955981
2710.097399	211629.113578	46.960986
2706.246964	210231.218845	46.965991
2702.520634	208838.991250	46.970996
2699.200831	207448.796191	46.976001
2695.366593	206069.437427	46.981005
2691.724848	204683.181146	46.986010
2688.337645	203285.790814	46.991015
2684.444270	201909.704422	46.996020
2680.711125	200522.601920	47.001025
2677.413229	199145.145845	47.006029
2673.255192	197762.972232	47.011034
2669.760895	196390.359405	47.016039
2666.301136	195023.535271	47.021044
2663.199189	193650.022325	47.026049
2659.148944	192274.507658	47.031053
2655.280673	190907.867180	47.036058
2651.937924	189540.447133	47.041063
2648.137632	188182.384133	47.046068
2644.664796	186820.110428	47.051073
2641.213667	185449.320243	47.056077
2637.353652	184096.589721	47.061082
2633.867593	182731.723952	47.066087
2630.318064	181375.850459	47.071092
2626.411119	180021.122002	47.076097
2622.945506	178661.888883	47.081101
2619.288037	177323.534657	47.086106
2616.101897	175959.704345	47.091111
2612.226291	174615.087367	47.096116
2608.535601	173258.586430	47.101121
2604.935565	171920.667930	47.106125
2601.213823	170577.126993	47.111130
2597.839464	169238.838650	47.116135
2593.953953	167894.099122	47.121140
2590.486535	166553.838412	47.126145
2586.836042	165227.379363	47.131149
2583.078220	163890.881802	47.136154
2579.666947	162554.293191	47.141159
2575.712178	161218.746133	47.146164
2572.266977	159891.305883	47.151169
2568.899039	158565.765401	47.156173
2565.219003	157249.058806	47.161178
2561.622773	155922.911730	47.166183
2557.631435	154592.834619	47.171188
2554.122779	153279.397008	47.176193
2550.577418	151952.722101	47.181197
2546.901985	150639.830330	47.186202
2543.577418	149322.410293	47.191207
2539.805246	148018.441315	47.196212
2535.940219	146701.590458	47.201217
2532.635280	145402.677945	47.206221
2528.705262	144007.853271	47.211226
2525.407121	142704.338989	47.216231
2521.481876	141402.751162	47.221236
2518.079698	140099.322317	47.226241
2514.714887	138802.895203	47.231245
2510.899255	137504.793026	47.236250
2507.743862	136206.420228	47.241255
2503.476317	134925.547144	47.246260
2499.929901	133628.046912	47.251265
2496.248901	132336.495388	47.256269
2492.486420	131043.633461	47.261274
2489.308968	129757.600310	47.266279
2485.454567	128486.644987	47.271284
2481.980757	127212.666610	47.276289
2478.718644	125921.981094	47.281293
2474.802295	124650.491213	47.286298
2471.361564	123368.970144	47.291303
2467.685174	122089.943367	47.296308
2463.800420	120817.412926	47.301313
2460.288272	119554.276354	47.306317
2456.552530	118288.621892	47.311322
2453.566554	117015.465836	47.316327
2449.876210	115738.724513	47.321332
2445.765032	114478.330418	47.326337
2442.314492	113218.155875	47.331341
2438.546912	111948.500504	47.336346
2435.070148	110699.454021	47.341351
2431.109134	109448.327671	47.346356
2427.715774	108201.530347	47.351361
2424.375888	106949.862182	47.356365
2420.596913	105712.101021	47.361370
2417.064261	104455.494640	47.366375
2413.008620	103215.401821	47.371380
2409.548083	101968.004071	47.376385
2406.073275	100731.523035	47.381389
2402.387764	99497.663685	47.386394
2399.253405	98265.811345	47.391399
2394.903618	97039.445249	47.396404
2391.224204	95802.588017	47.401409
2387.961240	94576.884563	47.406413
2383.948470	93360.508697	47.411418
2380.644813	92134.107602	47.416423
2376.593786	90916.995831	47.421428
2373.386231	89703.371379	47.426433
2369.472083	88496.881792	47.431437
2366.038326	87278.944285	47.436442
2362.460598	86073.771265	47.441447
2358.897183	84870.487757	47.446452
2355.209023	83674.489216	47.451457
2351.484512	82460.749561	47.456461
2347.722131	81270.465082	47.461466
2344.601823	80066.069541	47.466471
2340.543030	78878.892157	47.471476
2337.071945	77679.226985	47.476481
2333.499692	76490.869435	47.481485
2329.561488	75316.679178	47.486490
2326.057995	74129.861721	47.491495
2322.417259	72952.387943	47.496500
2318.809853	71777.779839	47.501505
2315.384753	70601.544690	47.506509
2311.538050	69433.369953	47.511514
2307.863986	68253.432207	47.516519
2304.066214	67093.087042	47.521524
2300.535472	65922.025288	47.526529
2296.900773	64770.925724	47.531533
2292.982201	63613.017511	47.536538
2289.909630	62465.324544	47.541543
2286.093432	61317.546881	47.546548
2282.588800	60167.882574	47.551553
2278.821064	59020.610350	47.556557
2275.051987	57876.196943	47.561562
2271.996711	56739.263914	47.566567
2268.118736	55602.354661	47.571572
2264.437984	54465.106979	47.576577
2260.776674	53330.746589	47.581581
2256.811679	52199.412812	47.586586
2253.561697	51064.342506	47.591591
2249.971147	49943.659610	47.596596
2246.094589	48827.509530	47.601601
2242.842406	47708.119279	47.606605
2238.882123	46584.277447	47.611610
2235.506230	45472.995217	47.616615
2231.506648	44371.783857	47.621620
2227.553357	43258.342376	47.626625
2224.092275	42164.543414	47.631629
2220.403001	41071.062502	47.636634
2216.939673	39966.035559	47.641639
2213.013192	38878.534385	47.646644
2209.195732	37801.055878	47.651649
2205.731092	36715.169697	47.656653
2201.411906	35643.367708	47.661658
2198.259706	34564.977623	47.666663
2194.612134	33499.739280	47.671668
2190.659178	32447.202962	47.676673
2187.183000	31381.728115	47.681677
2183.220362	30331.587739	47.686682
2179.700901	29283.693592	47.691687
2175.484559	28252.729346	47.696692
2171.680436	27213.140866	47.701697
2167.878936	26173.250078	47.706701
2163.592183	25154.200917	47.711706
2160.155072	24133.023806	47.716711
2155.763491	23142.121989	47.721716
2152.515384	22143.881072	47.726721
2148.765647	21153.794859	47.731725
2145.039453	20177.424210	47.736730
2141.157756	19200.416866	47.741735
2136.517351	18243.914814	47.746740
2132.667444	17298.989649	47.751745
2128.717297	16349.458585	47.756749
2124.595905	15439.914048	47.761754
2120.223705	14524.679591	47.766759
2114.518862	13652.633582	47.771764
2109.249097	12804.494462	47.776769
2104.418495	11976.355017	47.781773
2098.729457	11180.201853	47.786778
2094.204907	10411.184560	47.791783
2089.437928	9674.379065	47.796788
2084.503539	8954.000076	47.801793
2080.131164	8260.161742	47.806797
2075.569458	7596.691440	47.811802
2070.995145	6941.779796	47.816807
2066.704547	6317.075102	47.821812
2062.330467	5710.184591	47.826817
2058.448154	5123.833142	47.831821
2054.481530	4549.998065	47.836826
2050.113673	3991.844870	47.841831
2045.834981	3468.101600	47.846836
2042.065760	2949.302868	47.851841
2038.135559	2443.568216	47.856845
2033.704095	1959.293722	47.861850
2029.905364	1479.233220	47.866855
2025.674357	1030.276141	47.871860
2021.198680	593.894541	47.876865
2016.072345	193.114259	47.881869
2000.141769	105.646341	47.886874
1984.155250	138.118899	47.891879
1974.729692	144.241491	47.896884
1970.187451	147.040414	47.901889
1969.234992	138.052312	47.906893
1968.741034	147.991321	47.911898
1968.362212	136.654477	47.916903
1967.202687	138.544418	47.921908
1965.567755	138.474402	47.926913
1963.090583	135.865899	47.931917
1959.970072	137.100886	47.936922
1957.377163	133.320892	47.941927
1953.737680	132.972911	47.946932
1950.111663	138.700557	47.951937
1947.114126	124.109775	47.956941
1943.716928	137.954823	47.961946
1940.341547	130.339316	47.966951
1937.183221	129.574354	47.971956
1934.130862	135.879806	47.976961
1931.297467	130.906719	47.981965
1927.864533	128.482588	47.986970
1924.622159	124.877003	47.991975
1921.663350	134.360129	47.996980
1917.681155	132.420594	48.001985
1914.728384	123.533546	48.006989
1910.814959	133.991816	48.011994
1907.862961	121.156184	48.016999
1904.883401	140.172034	48.022004
1901.128100	132.347066	48.027009
1897.375559	124.762122	48.032013
1894.288310	124.580853	48.037018
1890.918596	127.123554	48.042023
1887.538144	122.704337	48.047028
1884.277061	128.355908	48.052033
1880.569620	131.087507	48.057037
1876.848583	129.569041	48.062042
1873.376843	136.044541	48.067047
1870.285312	131.728816	48.072052
1867.002382	134.473085	48.077057
1864.094501	129.356647	48.082061
1860.665299	133.351376	48.087066
1857.624246	133.545711	48.092071
1853.937620	132.784352	48.097076
1850.146656	136.278861	48.102081
1846.435906	127.811016	48.107085
1842.548762	131.934361	48.112090
1839.411145	126.002813	48.117095
1836.537488	130.179536	48.122100
1832.815634	126.244045	48.127105
1829.507095	123.439805	48.132109
1825.307277	128.725755	48.137114
1822.240951	130.338290	48.142119
1819.480992	130.273507	48.147124
1815.708258	130.123602	48.152129
1812.072133	124.529511	48.157133
1808.391424	131.271853	48.162138
1804.940066	128.660818	48.167143
1801.426914	126.100584	48.172148
1797.846646	128.185869	48.177153
1795.423878	126.669911	48.182157
1791.007225	129.914334	48.187162
1787.667482	132.914295	48.192167
1784.507521	130.093145	48.197172
1780.902118	127.696056	48.202177
1777.836970	132.152703	48.207181
1773.520371	127.971781	48.212186
1770.184535	129.772043	48.217191
1767.078695	120.826746	48.222196
1763.760874	124.411755	48.227201
1760.172647	125.988921	48.232205
1756.302371	129.423104	48.237210
1753.144349	131.024697	48.242215
1749.828044	131.157734	48.247220
1746.219962	122.787765	48.252225
1742.909806	122.081427	48.257229
1739.565484	130.599839	48.262234
1735.688137	123.009187	48.267239
1732.344489	126.088871	48.272244
1728.587181	131.093626	48.277249
1725.113074	121.310614	48.282253
1721.804571	132.234263	48.287258
1718.038641	120.291735	48.292263
1714.832865	129.971742	48.297268
1711.196966	133.075024	48.302273
1707.694169	117.728170	48.307277
1704.153868	124.353652	48.312282
1700.798526	122.018700	48.317287
1697.641466	125.546930	48.322292
1693.765803	131.282082	48.327297
1690.733484	123.208014	48.332301
1686.949913	134.281954	48.337306
1683.432781	127.685339	48.342311
1680.014818	121.202924	48.347316
1676.281237	127.747930	48.352321
1672.892075	120.501692	48.357325
1669.381773	132.697156	48.362330
1665.757841	131.609671	48.367335
1662.081015	132.308536	48.372340
1659.079500	128.364782	48.377345
1655.726144	120.926281	48.382349
1652.628602	126.466894	48.387354
1648.648834	127.807977	48.392359
1644.907337	119.345035	48.397364
1641.269884	125.852860	48.402369
1638.241019	115.867322	48.407373
1634.576149	118.690417	48.412378
1631.427993	110.748404	48.417383
1628.144478	111.404708	48.422388
1624.286337	114.071389	48.427393
1620.688910	112.093902	48.432397
1616.799537	108.820648	48.437402
1613.321936	114.101205	48.442407
1609.995871	117.497718	48.447412
1606.446629	117.268617	48.452417
1603.099281	112.483650	48.457421
1599.626172	114.425674	48.462426
1596.238844	117.259128	48.467431
1593.129610	117.299694	48.472436
1588.978899	122.476799	48.477441
1585.618515	116.687780	48.482445
1581.948499	123.033036	48.487450
1578.670098	122.375567	48.492455
1575.485206	114.467797	48.497460
1571.657623	117.585305	48.502465
1568.761606	111.274351	48.507469
1564.790509	115.781095	48.512474
1560.940315	111.400721	48.517479
1557.485987	120.815935	48.522484
1553.790423	114.481428	48.527489
1551.000932	114.990828	48.532493
1547.379822	120.619742	48.537498
1543.601418	113.649622	48.542503
1540.300000	112.748990	48.547508
1536.710066	110.808328	48.552513
1533.398318	111.358346	48.557517
1529.765537	118.928515	48.562522
1525.999748	112.418347	48.567527
1522.786745	110.551573	48.572532
1519.290412	108.109038	48.577537
1516.282908	109.940246	48.582541
1512.557566	108.947787	48.587546
1508.808683	109.841487	48.592551
1505.279029	108.894332	48.597556
1501.195471	120.160805	48.602561
1497.952630	104.922074	48.607565
1494.355392	118.637156	48.612570
1491.242266	117.020519	48.617575
1488.022084	113.762798	48.622580
1484.131025	114.988816	48.627585
1480.854618	109.145566	48.632589
1477.430875	114.038075	48.637594
1473.746793	115.680962	48.642599
1470.780361	105.764819	48.647604
1466.578195	106.555474	48.652609
1463.433612	113.014676	48.657613
1460.069172	114.696122	48.662618
1456.501391	104.491289	48.667623
1452.849304	113.681212	48.672628
1449.035257	118.030534	48.677633
1445.684706	112.692458	48.682637
1441.781749	110.835629	48.687642
1438.853470	109.702616	48.692647
1435.544970	106.914329	48.697652
1431.765714	106.199264	48.702657
1428.394303	104.736976	48.707661
1424.725817	103.707176	48.712666
1421.276460	110.777254	48.717671
1418.166064	105.490186	48.722676
1414.402588	114.422303	48.727681
1410.718099	105.333604	48.732685
1407.281030	105.561588	48.737690
1403.926569	109.845312	48.742695
1400.296298	113.953907	48.747700
1396.606533	116.790471	48.752705
1393.398266	111.233986	48.757709
1389.657023	118.463662	48.762714
1386.235925	114.209186	48.767719
1382.917314	113.928244	48.772724
1379.013442	115.434723	48.777729
1376.004888	117.440146	48.782733
1372.212502	114.983895	48.787738
1368.838327	114.974252	48.792743
1365.576263	110.024160	48.797748
1362.026884	120.245258	48.802753
1358.490774	112.247016	48.807757
1355.013988	107.381163	48.812762
1351.358159	105.242074	48.817767
1347.648800	110.207805	48.822772
1344.125595	105.801648	48.827777
1340.662083	106.802602	48.832781
1337.127100	114.547346	48.837786
1333.830430	112.962657	48.842791
1330.387684	108.151596	48.847796
1326.483228	116.286382	48.852801
1323.114504	109.907139	48.857805
1319.973392	110.813337	48.862810
1316.522813	115.235524	48.867815
1312.967209	120.202510	48.872820
1309.173791	119.999083	48.877825
1305.919733	112.162360	48.882829
1302.245118	110.538768	48.887834
1298.808160	109.453789	48.892839
1295.967647	106.816923	48.897844
1291.835742	111.851983	48.902849
1288.120559	99.582186	48.907853
1284.395206	115.981303	48.912858
1281.193162	112.293701	48.917863
1277.470769	108.361686	48.922868
1274.190403	117.069519	48.927873
1271.341962	109.416091	48.932877
1267.296454	118.167774	48.937882
1263.938209	110.904210	48.942887
1260.204760	113.763478	48.947892
1256.746799	114.709806	48.952897
1253.225005	107.611058	48.957901
1249.836229	110.995350	48.962906
1246.268675	113.300296	48.967911
1242.702583	116.256760	48.972916
1239.332788	112.642891	48.977921
1235.969638	114.820927	48.982925
1232.159313	107.757866	48.987930
1228.758317	111.710400	48.992935
1225.465280	113.270011	48.997940
1221.846157	116.098740	49.002945
1218.495492	113.288657	49.007949
1214.471116	115.506939	49.012954
1210.880264	114.781447	49.017959
1207.606440	108.675301	49.022964
1204.402567	112.362861	49.027969
1201.244565	112.351072	49.032973
1197.296193	116.712019	49.037978
1193.538249	111.956684	49.042983
1190.066705	118.631664	49.047988
1186.300097	114.662314	49.052993
1183.513170	107.575101	49.057997
1180.111534	107.541348	49.063002
1176.514235	114.894091	49.068007
1172.860382	107.034590	49.073012
1168.954971	110.199227	49.078017
1165.674697	104.556025	49.083021
1161.738411	108.544926	49.088026
1158.590449	109.610438	49.093031
1155.111479	112.512162	49.098036
1151.710498	104.796584	49.103041
1148.396074	96.902942	49.108045
1144.814958	109.217175	49.113050
1141.311728	106.380385	49.118055
1137.918422	104.896318	49.123060
1134.215513	110.788107	49.128065
1131.215739	99.463096	49.133069
1127.490030	106.813808	49.138074
1123.587355	103.672561	49.143079
1120.491562	101.562945	49.148084
1116.238226	107.113801	49.153089
1113.145063	109.879205	49.158093
1109.685235	102.777146	49.163098
1106.124257	102.901246	49.168103
1102.514827	102.245144	49.173108
1099.202168	113.982679	49.178113
1095.743664	110.743428	49.183117
1092.072726	104.648881	49.188122
1088.511205	106.481529	49.193127
1085.299632	103.921808	49.198132
1082.141055	110.506688	49.203137
1078.485812	102.815131	49.208141
1074.800831	108.634528	49.213146
1071.059636	105.958412	49.218151
1067.736169	109.756487	49.223156
1063.990700	98.228710	49.228161
1060.823137	97.174408	49.233165
1057.290037	101.856370	49.238170
1053.749700	99.167798	49.243175
1050.016793	104.820697	49.248180
1046.168912	104.935954	49.253185
1043.369232	96.218268	49.258189
1039.862487	112.981853	49.263194
1036.320570	103.728633	49.268199
1032.909645	94.929481	49.273204
1028.932500	102.686591	49.278209
1025.961612	99.614637	49.283213
1022.411761	101.549886	49.288218
1018.285356	112.351810	49.293223
1014.865873	98.457110	49.298228
1011.306217	104.889666	49.303233
1008.136029	99.979113	49.308237
1004.497762	101.510590	49.313242
1001.082150	108.335056	49.318247
997.907652	108.060157	49.323252
994.093284	116.354956	49.328257
990.889318	103.752155	49.333261
987.310238	106.818308	49.338266
983.480300	106.177796	49.343271
979.804589	107.272212	49.348276
976.334266	107.233467	49.353281
973.433705	101.565689	49.358285
969.354942	100.046639	49.363290
965.958066	97.721623	49.368295
962.844701	96.424747	49.373300
959.192900	104.276476	49.378305
955.521241	96.865962	49.383309
952.389942	108.081579	49.388314
948.566659	113.115905	49.393319
945.082533	109.906035	49.398324
941.370318	111.363692	49.403329
938.072474	98.342176	49.408333
935.178550	105.910728	49.413338
931.051490	115.149866	49.418343
927.683845	99.573437	49.423348
924.040284	99.115741	49.428353
921.033752	98.979085	49.433357
916.706336	97.973563	49.438362
913.185141	95.538318	49.443367
910.240964	102.311137	49.448372
906.578592	101.369168	49.453377
902.761760	97.834921	49.458381
899.514038	103.354951	49.463386
895.533901	109.900844	49.468391
892.197107	101.830472	49.473396
889.287933	111.094059	49.478401
886.354870	103.659671	49.483405
882.226036	101.673930	49.488410
878.436049	108.218528	49.493415
874.570762	95.934476	49.498420
871.157705	109.823350	49.503425
868.117589	97.966920	49.508429
864.807241	96.881258	49.513434
861.122454	97.679744	49.518439
857.826737	96.829079	49.523444
853.884644	100.815840	49.528449
850.786592	99.494457	49.533453
847.236764	98.126757	49.538458
843.471941	93.970616	49.543463
840.344605	100.332365	49.548468
836.293129	100.017674	49.553473
832.758040	103.251002	49.558477
829.030296	102.505964	49.563482
825.740970	97.250300	49.568487
822.608140	98.376826	49.573492
818.955718	104.846117	49.578497
815.759702	102.619421	49.583501
812.016175	92.771447	49.588506
808.506029	105.925716	49.593511
805.228224	101.108023	49.598516
801.444606	102.143474	49.603521
798.213909	100.143681	49.608525
794.716977	103.703246	49.613530
790.681788	107.517947	49.618535
787.445210	101.282750	49.623540
783.645256	112.005158	49.628545
780.474429	99.251731	49.633549
777.023409	108.185736	49.638554
773.667336	100.488599	49.643559
770.222024	100.180254	49.648564
766.341714	101.499784	49.653569
762.856840	108.948945	49.658573
759.436744	107.402774	49.663578
755.802626	100.875499	49.668583
752.274267	91.787973	49.673588
748.715197	99.087401	49.678593
745.426250	91.215251	49.683597
742.046689	88.340273	49.688602
738.827482	100.775108	49.693607
735.325845	94.546641	49.698612
731.366630	99.352391	49.703617
727.659666	93.535738	49.708621
724.245356	102.919593	49.713626
720.703120	107.229772	49.718631
717.596127	100.417482	49.723636
713.710741	85.779641	49.728641
710.334758	87.149929	49.733645
707.012109	91.625040	49.738650
703.227241	98.042342	49.743655
700.069577	96.369674	49.748660
695.984228	102.868839	49.753665
692.579198	93.493103	49.758669
689.645690	95.765390	49.763674
686.181833	99.133149	49.768679
682.623012	102.715100	49.773684
678.622252	101.348483	49.778689
675.423140	96.502699	49.783693
671.793670	95.587310	49.788698
668.423183	95.349544	49.793703
664.963013	101.326864	49.798708
661.129819	98.307822	49.803713
657.944347	96.199756	49.808717
654.441981	101.168110	49.813722
650.765732	101.936866	49.818727
647.287411	107.648113	49.823732
643.798892	99.917990	49.828737
640.781164	89.162322	49.833741
636.933498	96.035577	49.838746
633.708787	96.240072	49.843751
630.032292	94.186771	49.848756
626.065065	104.182439	49.853761
622.518822	93.585479	49.858765
618.864301	97.647518	49.863770
615.414951	103.063169	49.868775
612.385277	95.577580	49.873780
608.659638	94.610838	49.878785
605.300099	99.560002	49.883789
601.689017	103.128021	49.888794
598.312075	93.909282	49.893799
595.021732	93.621027	49.898804
591.419991	94.571129	49.903809
587.606116	82.845505	49.908813
584.719274	83.433704	49.913818
581.047430	91.741112	49.918823
577.304966	85.427048	49.923828
573.659637	89.111171	49.928833
570.067714	88.180451	49.933837
566.510874	95.207501	49.938842
562.927576	89.532910	49.943847
559.496273	89.171831	49.948852
555.853928	90.555417	49.953857
553.026372	95.965451	49.958861
549.495395	89.479068	49.963866
545.889364	88.642318	49.968871
542.641533	89.726836	49.973876
538.586272	99.922984	49.978881
535.042030	105.663575	49.983885
531.530352	92.160049	49.988890
528.047321	85.719952	49.993895
524.704858	84.614137	49.998900
521.206361	84.216140	50.003905
517.484649	88.298229	50.008909
514.067477	94.771904	50.013914
510.197721	92.989371	50.018919
507.471297	90.334895	50.023924
503.847995	101.096159	50.028929
500.689889	91.656526	50.033933
497.020357	97.400933	50.038938
493.282775	90.753944	50.043943
489.308900	92.059768	50.048948
485.698723	98.718709	50.053953
482.863112	88.750842	50.058957
479.075074	91.422794	50.063962
475.456659	95.175506	50.068967
472.397101	93.576140	50.073972
468.531176	97.373950	50.078977
465.284500	81.313746	50.083981
461.783822	89.328625	50.088986
458.340403	87.745097	50.093991
454.957669	78.938631	50.098996
450.857365	84.060818	50.104001
447.613238	89.472850	50.109005
444.148529	86.949853	50.114010
440.386181	91.484431	50.119015
437.198425	76.186981	50.124020
433.773747	83.721723	50.129025
430.514438	85.064344	50.134029
426.738799	86.003783	50.139034
422.534699	83.694687	50.144039
419.650532	85.718879	50.149044
416.162622	96.022357	50.154049
413.030158	86.006104	50.159053
408.981711	77.838614	50.164058
405.304098	89.867595	50.169063
401.920814	94.947096	50.174068
398.401596	100.873641	50.179073
395.363978	91.291794	50.184077
391.899601	92.960783	50.189082
388.021750	80.213893	50.194087
384.312357	84.249809	50.199092
380.465376	87.984573	50.204097
378.115687	81.183519	50.209101
374.397827	85.787083	50.214106
370.530982	88.857404	50.219111
367.294246	88.592474	50.224116
363.806580	89.970889	50.229121
360.052305	82.526143	50.234125
356.312051	81.738970	50.239130
352.801877	84.313662	50.244135
349.862804	82.097513	50.249140
345.940412	84.989882	50.254145
342.303101	83.816426	50.259149
338.706768	77.008184	50.264154
335.602004	91.772712	50.269159
332.001898	83.958976	50.274164
328.829246	86.423858	50.279169
325.108257	85.431198	50.284173
321.546519	93.544275	50.289178
318.003458	96.193736	50.294183
314.755075	84.702379	50.299188
311.298625	82.608418	50.304193
307.369258	78.687108	50.309197
304.244459	76.582328	50.314202
300.409548	82.295760	50.319207
297.104355	82.022596	50.324212
293.035778	89.107752	50.329217
289.955439	85.439430	50.334221
286.552972	79.891665	50.339226
282.815996	77.088682	50.344231
279.566820	78.015314	50.349236
275.730073	84.083387	50.354241
272.379932	74.354405	50.359245
269.306647	73.323581	50.364250
265.382541	74.523628	50.369255
262.429557	77.245188	50.374260
258.528060	80.055225	50.379265
255.081099	79.861233	50.384269
251.224502	84.122743	50.389274
247.556287	86.092640	50.394279
244.358192	75.270493	50.399284
240.902676	78.747833	50.404289
237.699796	73.855365	50.409293
233.948586	79.954345	50.414298
230.610204	75.608294	50.419303
227.069922	80.519455	50.424308
223.380765	80.888606	50.429313
219.924765	77.715764	50.434317
216.598370	72.826835	50.439322
212.852482	81.538272	50.444327
209.723682	82.113875	50.449332
205.914451	80.733291	50.454337
202.128288	81.832661	50.459341
198.945052	78.610769	50.464346
195.048227	82.995663	50.469351
192.021931	75.788137	50.474356
188.160418	81.024885	50.479361
184.831878	81.733029	50.484365
181.377292	80.540508	50.489370
177.658213	72.375328	50.494375
173.962072	76.586419	50.499380
171.151375	80.987830	50.504385
167.710888	68.596497	50.509389
163.811612	85.573622	50.514394
160.240052	83.225672	50.519399
156.558032	77.443348	50.524404
153.017040	78.548623	50.529409
150.170883	82.439899	50.534413
146.927633	79.391946	50.539418
143.050073	82.932278	50.544423
139.538128	86.681089	50.549428
135.898691	78.633166	50.554433
132.076502	74.562271	50.559437
128.756417	75.512722	50.564442
125.090380	80.984628	50.569447
122.240815	73.648202	50.574452
118.591317	80.373538	50.579457
114.607361	75.334569	50.584461
111.193721	62.499299	50.589466
107.788503	74.526816	50.594471
104.737743	77.830059	50.599476
100.581362	82.546724	50.604481
97.328124	78.636645	50.609485
93.767437	82.295032	50.614490
90.119194	81.585309	50.619495
86.615148	74.250195	50.624500
83.077661	79.271702	50.629505
79.857758	75.723406	50.634509
76.384745	79.137108	50.639514
72.661501	80.780337	50.644519
69.509766	76.047604	50.649524
65.799863	79.564864	50.654529
62.491862	70.202706	50.659533
58.858259	74.400880	50.664538
55.178394	74.183347	50.669543
52.142128	74.165538	50.674548
48.190939	80.916021	50.679553
44.805775	77.773284	50.684557
41.086903	77.036682	50.689562
37.686845	77.148643	50.694567
34.394074	73.007502	50.699572
30.502654	77.511839	50.704577
26.961688	70.555865	50.709581
23.807055	73.119268	50.714586
20.096517	74.953517	50.719591
16.518592	72.239631	50.724596
13.227766	84.859867	50.729601
9.746025	84.139909	50.734605
6.037620	82.680341	50.739610
2.546526	84.002486	50.744615