Thu Aug 25 12:34:47 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
1.410421	100.151472	0.000000
1.163523	106.520831	0.005005
1.317249	100.045775	0.010010
1.154636	101.953663	0.015014
1.214521	90.772964	0.020019
1.004644	80.732367	0.025024
0.497296	78.619331	0.030029
0.198766	61.426699	0.035034
0.107139	60.191332	0.040038
-0.754463	52.540268	0.045043
-0.596812	46.137383	0.050048
-0.891127	40.656367	0.055053
-1.112165	43.731339	0.060058
-1.833153	34.868676	0.065062
-1.526577	39.113830	0.070067
-1.887874	34.560802	0.075072
-2.338079	33.435403	0.080077
-2.669383	27.814654	0.085082
-3.573122	26.051635	0.090086
-3.705024	26.315875	0.095091
-3.898356	25.830438	0.100096
-3.909216	34.023079	0.105101
-3.948542	33.377470	0.110106
-3.906072	32.601986	0.115110
-4.635335	30.669260	0.120115
-4.509123	17.940627	0.125120
-4.936677	25.084910	0.130125
-5.324574	30.039988	0.135130
-5.279959	24.758973	0.140134
-5.949289	25.512381	0.145139
-6.320188	17.898343	0.150144
-6.967496	28.171214	0.155149
-7.266040	24.956119	0.160154
-7.046577	20.672768	0.165158
-7.028230	34.720116	0.170163
-7.216532	21.610488	0.175168
-7.315659	19.743547	0.180173
-7.423248	25.588013	0.185178
-8.170699	31.994645	0.190182
-8.568399	24.862531	0.195187
-8.443096	14.804257	0.200192
-8.747378	27.139935	0.205197
-9.039735	23.768847	0.210202
-9.317836	16.092814	0.215206
-9.779574	22.859637	0.220211
-9.708365	26.084970	0.225216
-9.817522	22.644048	0.230221
-10.287220	18.338964	0.235226
-10.721450	19.153611	0.240230
-11.375880	23.777125	0.245235
-11.155422	21.992988	0.250240
-11.285580	30.134716	0.255245
-11.375261	27.589250	0.260250
-11.535280	24.115168	0.265254
-12.174876	29.068554	0.270259
-12.362415	13.155722	0.275264
-12.845593	19.758225	0.280269
-12.741896	18.631462	0.285274
-12.823940	11.737798	0.290278
-14.011841	22.702810	0.295283
-14.071387	22.012913	0.300288
-13.913179	19.830405	0.305293
-13.975788	28.053298	0.310298
-14.559901	22.525946	0.315302
-14.424872	24.070814	0.320307
-14.348325	30.756464	0.325312
-14.909821	27.554095	0.330317
-15.777207	23.678317	0.335322
-15.815213	21.254470	0.340326
-16.039949	32.615905	0.345331
-16.178444	24.449759	0.350336
-15.988794	25.144509	0.355341
-16.482159	27.717981	0.360346
-17.215615	22.486113	0.365350
-17.600591	27.861512	0.370355
-17.317011	15.282232	0.375360
-17.515186	22.580400	0.380365
-17.301477	16.928044	0.385370
-17.854088	24.250109	0.390374
-18.738813	30.017024	0.395379
-18.321895	26.885980	0.400384
-18.621978	28.926131	0.405389
-19.288209	25.072620	0.410394
-19.506912	26.302752	0.415398
-20.250907	34.673539	0.420403
-19.844881	16.902324	0.425408
-19.933606	25.091342	0.430413
-20.345869	29.142238	0.435418
-20.279963	26.044046	0.440422
-21.091978	30.578358	0.445427
-21.085903	33.393117	0.450432
-21.757643	32.005037	0.455437
-21.694465	35.861217	0.460442
-21.425860	25.587495	0.465446
-21.596742	32.932010	0.470451
-22.321098	22.820199	0.475456
-23.249000	29.938476	0.480461
-23.080338	24.185609	0.485466
-23.320903	22.663533	0.490470
-23.645688	28.282602	0.495475
-23.491846	33.959557	0.500480
-23.083616	29.975658	0.505485
-24.153622	26.555573	0.510490
-24.397835	25.049887	0.515494
-24.492773	28.532206	0.520499
-24.622056	28.302490	0.525504
-25.162111	28.975532	0.530509
-26.056900	21.734646	0.535514
-26.125980	20.628627	0.540518
-26.105369	26.288490	0.545523
-25.739190	26.708807	0.550528
-26.066104	29.309984	0.555533
-26.749934	28.790669	0.560538
-27.105885	24.350704	0.565542
-27.504893	28.696916	0.570547
-27.520637	31.021547	0.575552
-27.464683	28.756983	0.580557
-27.574125	20.551486	0.585562
-27.540513	23.985189	0.590566
-28.371781	33.027711	0.595571
-28.530049	18.157496	0.600576
-28.843581	23.135721	0.605581
-29.592769	26.755353	0.610586
-29.420147	28.278511	0.615590
-30.214690	23.008760	0.620595
-30.348828	20.286763	0.625600
-30.419068	19.146125	0.630605
-30.223959	29.030738	0.635610
-30.192057	19.604030	0.640614
-30.661335	25.486183	0.645619
-30.938981	14.393223	0.650624
-31.619840	22.959756	0.655629
-31.883368	18.119332	0.660634
-32.186357	27.085405	0.665638
-32.370445	28.946030	0.670643
-32.372323	25.175087	0.675648
-32.539174	20.835208	0.680653
-32.490908	23.662336	0.685658
-33.234869	22.639916	0.690662
-33.659285	35.845473	0.695667
-33.561166	23.361687	0.700672
-33.560336	29.809261	0.705677
-33.932552	23.438788	0.710682
-34.482878	29.286186	0.715686
-34.621563	25.166519	0.720691
-34.851248	23.335854	0.725696
-35.213081	20.836196	0.730701
-35.372377	17.456916	0.735706
-35.710129	20.562827	0.740710
-36.089355	27.149044	0.745715
-36.062471	18.545701	0.750720
-36.050093	18.391865	0.755725
-37.040279	16.338675	0.760730
-37.486276	18.743374	0.765734
-37.623977	20.802374	0.770739
-37.941143	11.015913	0.775744
-37.954493	16.266641	0.780749
-37.643084	23.152768	0.785754
-37.977563	22.933057	0.790758
-38.148492	34.684695	0.795763
-38.077237	24.302692	0.800768
-38.899634	19.549835	0.805773
-39.044534	21.442284	0.810778
-39.062256	24.083599	0.815782
-39.820987	22.879995	0.820787
-40.318102	18.082500	0.825792
-40.593715	14.518966	0.830797
-40.828467	28.618617	0.835802
-40.712683	13.354290	0.840806
-40.938584	18.749054	0.845811
-40.751315	16.017827	0.850816
-41.121722	16.980663	0.855821
-41.698487	24.768421	0.860826
-41.909399	16.037824	0.865830
-42.118876	27.355734	0.870835
-41.927747	17.973682	0.875840
-42.578708	21.868989	0.880845
-43.431294	26.128083	0.885850
-43.504494	15.923742	0.890854
-43.930258	22.874755	0.895859
-43.839028	26.514565	0.900864
-43.624017	22.269877	0.905869
-43.779558	31.098953	0.910874
-44.537255	18.227247	0.915878
-45.289071	25.510922	0.920883
-45.298242	16.407029	0.925888
-45.502739	18.201247	0.930893
-45.148460	21.141779	0.935898
-45.253476	23.382319	0.940902
-45.574791	26.846325	0.945907
-45.821627	22.288024	0.950912
-46.435705	19.055933	0.955917
-46.858905	27.101205	0.960922
-46.623966	20.904520	0.965926
-47.365864	23.792182	0.970931
-47.532895	15.984854	0.975936
-47.525128	26.977659	0.980941
-48.043637	21.101511	0.985946
-48.189917	26.195899	0.990950
-48.346564	23.322405	0.995955
-48.843907	27.807412	1.000960
-49.026102	27.196845	1.005965
-49.142672	30.916672	1.010970
-49.445086	26.363915	1.015974
-49.531351	29.231106	1.020979
-49.413197	23.353276	1.025984
-50.426422	23.822049	1.030989
-50.734791	24.113940	1.035994
-50.801658	20.742324	1.040998
-51.130412	23.682311	1.046003
-50.916047	25.211583	1.051008
-51.308698	28.721567	1.056013
-52.253413	21.342976	1.061018
-52.098888	24.536270	1.066022
-52.588148	29.149724	1.071027
-52.436514	15.850802	1.076032
-52.772740	19.389909	1.081037
-52.715496	23.098318	1.086042
-52.614412	14.945260	1.091046
-53.361780	20.466025	1.096051
-53.485918	16.410521	1.101056
-53.694221	12.981974	1.106061
-54.985281	17.018705	1.111066
-55.147722	21.675862	1.116070
-54.744749	20.147865	1.121075
-55.075749	21.167803	1.126080
-55.412198	27.304391	1.131085
-55.713826	23.339971	1.136090
-55.823041	19.424498	1.141094
-55.539477	24.116175	1.146099
-55.941412	22.654187	1.151104
-56.419613	25.946621	1.156109
-56.799007	21.383782	1.161114
-57.086612	16.793906	1.166118
-57.258454	21.838515	1.171123
-57.280452	26.609709	1.176128
-57.638410	25.441386	1.181133
-58.148745	28.542703	1.186138
-58.363082	21.559036	1.191142
-58.655634	34.576250	1.196147
-58.574393	19.842517	1.201152
-58.772586	20.408210	1.206157
-58.772971	33.354334	1.211162
-59.414174	19.347569	1.216166
-59.883037	28.823687	1.221171
-59.748045	23.525351	1.226176
-60.245600	16.712613	1.231181
-61.092976	28.911923	1.236186
-61.573325	23.460067	1.241190
-61.031958	25.251313	1.246195
-61.282115	20.949799	1.251200
-61.460202	23.499182	1.256205
-62.019853	22.881319	1.261210
-61.545091	22.952426	1.266214
-62.122882	28.845256	1.271219
-62.348279	24.071625	1.276224
-63.127520	23.380602	1.281229
-63.163007	30.716554	1.286234
-62.996569	14.991875	1.291238
-63.547536	25.926692	1.296243
-63.424498	26.540129	1.301248
-64.319872	27.680136	1.306253
-64.988754	25.592423	1.311258
-64.749688	24.162874	1.316262
-64.965474	29.730063	1.321267
-64.963671	29.090665	1.326272
-65.080035	23.208454	1.331277
-65.414981	33.868982	1.336282
-65.188705	35.959538	1.341286
-66.307434	29.370678	1.346291
-66.535840	27.413263	1.351296
-66.566494	26.582798	1.356301
-66.940250	37.341159	1.361306
-66.509138	31.097914	1.366310
-66.831100	27.146171	1.371315
-67.535775	30.913855	1.376320
-67.844293	32.417490	1.381325
-68.020680	26.225143	1.386330
-67.978111	21.795504	1.391334
-68.700389	37.433205	1.396339
-69.410701	32.359066	1.401344
-69.352777	34.267192	1.406349
-69.495162	20.682143	1.411354
-69.758184	23.716234	1.416358
-69.758335	29.983626	1.421363
-69.744649	21.641780	1.426368
-69.711357	22.914685	1.431373
-69.908661	33.718162	1.436378
-70.312952	25.463953	1.441382
-70.803346	24.515700	1.446387
-71.345767	19.260234	1.451392
-72.076489	23.971634	1.456397
-72.557075	22.904785	1.461402
-72.182736	16.464796	1.466406
-72.274707	24.337943	1.471411
-72.253719	18.737933	1.476416
-72.376645	29.842964	1.481421
-72.739143	21.965024	1.486426
-73.002541	17.406158	1.491430
-73.725182	22.457977	1.496435
-73.520909	27.203207	1.501440
-74.231132	30.123874	1.506445
-74.457244	34.518927	1.511450
-73.960711	22.466264	1.516454
-74.879420	27.972751	1.521459
-75.081067	23.701601	1.526464
-75.570984	28.675827	1.531469
-75.607840	26.118922	1.536474
-75.099052	25.314663	1.541478
-76.031477	23.141695	1.546483
-76.289166	21.524228	1.551488
-76.607138	26.544278	1.556493
-76.962559	29.368222	1.561498
-76.728346	27.550291	1.566502
-77.308323	27.625314	1.571507
-78.121804	22.083290	1.576512
-78.320699	23.234389	1.581517
-78.693232	23.242105	1.586522
-78.345989	18.502136	1.591526
-78.848085	27.508896	1.596531
-78.616813	28.140175	1.601536
-78.784779	23.756179	1.606541
-78.784842	22.566581	1.611546
-79.478428	20.947812	1.616550
-79.934301	21.674105	1.621555
-79.982606	18.245799	1.626560
-79.804913	28.167936	1.631565
-80.328132	27.389342	1.636570
-80.854282	16.841526	1.641574
-81.644797	19.790591	1.646579
-81.498408	20.362403	1.651584
-81.296598	21.877823	1.656589
-81.725062	18.547049	1.661594
-81.805753	22.928804	1.666598
-82.499194	26.182199	1.671603
-82.697818	14.807944	1.676608
-82.887787	18.463339	1.681613
-83.019966	27.956302	1.686618
-82.972593	21.621329	1.691622
-83.369326	30.000976	1.696627
-83.676485	27.979972	1.701632
-84.368681	18.049796	1.706637
-84.707565	19.308252	1.711642
-84.384477	20.456654	1.716646
-84.710709	24.677568	1.721651
-84.351380	25.940515	1.726656
-85.254391	17.495538	1.731661
-85.438003	23.858113	1.736666
-85.554791	17.991789	1.741670
-86.561339	20.908267	1.746675
-86.839658	26.102438	1.751680
-86.473014	27.930551	1.756685
-87.154230	19.615335	1.761690
-87.124838	18.190167	1.766694
-87.676875	28.618952	1.771699
-87.504796	32.407445	1.776704
-87.476632	25.942602	1.781709
-87.884256	27.857236	1.786714
-88.486795	17.663076	1.791718
-88.756238	20.527330	1.796723
-88.625620	25.651096	1.801728
-88.925095	21.126357	1.806733
-89.118517	24.203327	1.811738
-89.611740	16.804619	1.816742
-90.273996	17.487321	1.821747
-90.389640	24.114492	1.826752
-90.344348	23.436643	1.831757
-90.550616	18.375280	1.836762
-90.131746	17.025125	1.841766
-90.519475	31.408171	1.846771
-91.269324	27.624718	1.851776
-92.127289	19.090425	1.856781
-92.098123	19.829301	1.861786
-91.972944	17.408360	1.866790
-92.381316	29.187704	1.871795
-92.278438	29.184203	1.876800
-93.138732	17.609905	1.881805
-93.429430	20.812848	1.886810
-93.523163	20.454176	1.891814
-93.203129	28.538012	1.896819
-93.273198	19.608179	1.901824
-93.457997	23.006500	1.906829
-94.473797	28.449107	1.911834
-94.444020	12.976801	1.916838
-94.915201	27.259025	1.921843
-95.261752	28.040955	1.926848
-95.708656	21.824561	1.931853
-95.786206	20.792637	1.936858
-96.054301	24.194519	1.941862
-96.072748	21.872012	1.946867
-96.156702	29.794524	1.951872
-96.386524	26.242799	1.956877
-96.598774	37.656059	1.961882
-97.066759	25.428662	1.966886
-97.855792	27.045555	1.971891
-97.890719	23.422163	1.976896
-97.842157	20.484879	1.981901
-98.055321	32.657581	1.986906
-97.767373	28.240112	1.991910
-98.516222	30.005734	1.996915
-99.139630	29.739684	2.006912
-98.462599	27.206984	2.016909
-98.301581	34.005142	2.026906
-97.795368	27.282855	2.036902
-96.681428	31.926473	2.046899
-96.686156	32.963016	2.056896
-96.549041	26.463290	2.066893
-95.809634	31.700955	2.076890
-95.079336	22.570868	2.086886
-94.148683	20.536956	2.096883
-93.973076	26.252604	2.106880
-93.800970	26.532841	2.116877
-93.456035	36.001155	2.126874
-92.885065	28.007932	2.136870
-91.730827	25.441640	2.146867
-91.366073	21.221914	2.156864
-91.329985	25.961564	2.166861
-90.589953	24.413685	2.176858
-90.128097	30.543813	2.186854
-90.000153	29.316758	2.196851
-89.148854	23.946907	2.206848
-88.674899	26.254762	2.216845
-87.509588	27.966444	2.226842
-87.164208	29.277580	2.236838
-87.102629	31.707072	2.246835
-87.017810	21.534548	2.256832
-85.964285	27.061948	2.266829
-85.491346	35.277927	2.276826
-85.433543	28.752614	2.286822
-84.553876	22.861966	2.296819
-84.189693	20.457484	2.306816
-83.510444	28.818531	2.316813
-82.917950	22.862007	2.326810
-83.028854	20.329228	2.336806
-81.759521	24.840792	2.346803
-81.287463	25.191239	2.356800
-81.211049	27.973201	2.366797
-80.888883	29.421022	2.376794
-80.090025	28.662215	2.386790
-79.413543	22.001948	2.396787
-78.796339	22.402512	2.406784
-78.678198	35.223059	2.416781
-78.187163	27.438765	2.426778
-77.439629	22.997503	2.436774
-77.213317	27.254351	2.446771
-76.774848	25.975472	2.456768
-76.011935	27.667845	2.466765
-75.767534	25.769974	2.476762
-74.912677	29.063523	2.486758
-74.389870	16.294461	2.496755
-74.244882	26.031687	2.506752
-73.356401	25.990601	2.516749
-72.880005	17.704924	2.526746
-72.979783	23.143773	2.536742
-71.948687	23.720238	2.546739
-71.846501	17.210149	2.556736
-70.971327	22.790838	2.566733
-70.347636	27.425746	2.576730
-70.252137	25.285111	2.586726
-69.621133	24.948581	2.596723
-69.045764	21.164691	2.606720
-68.586346	19.622770	2.616717
-67.872906	25.545584	2.626714
-67.599595	28.036934	2.636710
-67.186859	26.587858	2.646707
-66.435659	24.762632	2.656704
-66.108466	23.282611	2.666701
-65.561053	25.680327	2.676698
-64.796050	28.215011	2.686694
-64.718589	23.555626	2.696691
-64.028285	22.813829	2.706688
-63.267577	22.799100	2.716685
-63.012195	25.134869	2.726682
-62.868953	25.730076	2.736678
-61.889367	24.144664	2.746675
-61.326599	26.093313	2.756672
-61.304979	28.899701	2.766669
-60.610349	27.894298	2.776666
-60.122650	29.233820	2.786662
-58.830372	24.615336	2.796659
-58.610087	26.604978	2.806656
-58.460850	23.366197	2.816653
-58.639589	32.951412	2.826650
-57.813897	34.253814	2.836646
-57.124756	26.666563	2.846643
-56.153881	21.974896	2.856640
-55.868914	24.562622	2.866637
-55.820356	25.391243	2.876634
-54.979583	23.577325	2.886630
-54.456799	29.834126	2.896627
-54.077673	24.677644	2.906624
-53.311747	29.746433	2.916621
-53.113775	31.552671	2.926618
-52.492490	33.181707	2.936614
-51.891505	30.594402	2.946611
-51.359944	29.392804	2.956608
-51.000648	26.165457	2.966605
-50.044794	28.416814	2.976602
-49.778768	21.725828	2.986598
-49.727468	21.790578	2.996595
-49.514499	25.564842	3.006592
-48.568271	18.561370	3.016589
-48.035378	23.508281	3.026586
-47.018708	26.614921	3.036582
-47.151746	27.129873	3.046579
-46.722102	26.910426	3.056576
-45.718106	22.565197	3.066573
-45.549623	32.539501	3.076570
-45.124899	27.581782	3.086566
-44.059734	29.594266	3.096563
-43.905482	26.642968	3.106560
-43.789576	24.461121	3.116557
-42.885519	28.938062	3.126554
-42.715174	26.614637	3.136550
-41.976441	26.539997	3.146547
-41.295739	28.435324	3.156544
-40.948953	28.175008	3.166541
-40.607063	29.128730	3.176538
-39.761966	20.516017	3.186534
-39.626087	25.148166	3.196531
-39.019453	31.502704	3.206528
-38.419713	31.918679	3.216525
-38.079854	33.728029	3.226522
-37.299795	29.531928	3.236518
-37.032228	23.224004	3.246515
-36.535816	22.056425	3.256512
-35.719768	30.183802	3.266509
-35.408642	31.560496	3.276506
-35.172128	29.027131	3.286502
-34.427522	29.490099	3.296499
-33.865813	25.568965	3.306496
-33.380024	27.003822	3.316493
-32.443389	29.264528	3.326490
-32.497936	29.345863	3.336486
-32.052936	29.149354	3.346483
-31.907033	27.257413	3.356480
-30.859413	29.975901	3.366477
-30.375086	30.919978	3.376474
-29.656568	27.186517	3.386470
-29.228611	38.140205	3.396467
-28.900700	32.776335	3.406464
-28.780167	28.867305	3.416461
-27.849167	30.431977	3.426458
-27.741884	27.285299	3.436454
-26.794591	29.091340	3.446451
-26.401014	28.601946	3.456448
-26.156854	31.173894	3.466445
-25.300949	31.099903	3.476442
-25.232933	31.849448	3.486438
-24.290770	29.569817	3.496435
-24.064626	23.350747	3.506432
-23.492843	30.657922	3.516429
-22.386112	28.282814	3.526426
-22.496693	32.538600	3.536422
-22.179569	28.611439	3.546419
-21.171200	28.646607	3.556416
-21.072629	24.056773	3.566413
-20.583560	27.147882	3.576410
-19.756178	29.045571	3.586406
-19.578626	32.080953	3.596403
-19.031132	28.149375	3.606400
-18.105504	29.828931	3.616397
-17.908356	27.995485	3.626394
-17.722237	38.996571	3.636390
-16.487767	31.738857	3.646387
-16.198915	33.109538	3.656384
-16.338450	29.418655	3.666381
-15.262870	30.441154	3.676378
-14.876214	28.609693	3.686374
-14.571925	31.286261	3.696371
-13.993133	29.136425	3.706368
-13.343474	33.688077	3.716365
-12.388444	31.960798	3.726362
-12.354569	33.219375	3.736358
-12.000526	30.132235	3.746355
-11.811062	28.879702	3.756352
-10.783642	26.529694	3.766349
-10.540904	25.550749	3.776346
-9.677010	31.088869	3.786342
-9.344714	25.388525	3.796339
-9.010694	26.321307	3.806336
-7.806392	24.383910	3.816333
-7.645863	23.306973	3.826330
-7.659073	23.926694	3.836326
-7.202713	24.935342	3.846323
-6.334221	26.240546	3.856320
-6.064555	21.398990	3.866317
-5.144137	23.326452	3.876314
-4.470820	18.161891	3.886310
-4.611777	29.309254	3.896307
-4.258867	29.589676	3.906304
-3.648208	34.340676	3.916301
-3.241716	46.298765	3.926298
-2.792770	56.793015	3.936294
-1.964712	60.280848	3.946291
-1.860440	75.412944	3.956288
-1.466747	87.664506	3.966285
-0.816156	97.731209	3.976282
-0.429636	113.392491	3.986278
0.000000	123.565893	3.991283
-0.066972	136.433945	3.996288
0.600687	148.003649	4.001293
0.537297	151.566472	4.006298
0.225183	148.900814	4.011302
0.525261	142.156037	4.016307
0.740922	155.349981	4.021312
1.239501	167.227766	4.026317
1.197415	152.604989	4.031322
0.917532	150.605002	4.036326
0.896224	156.983326	4.041331
0.705632	148.651276	4.046336
0.687143	148.964188	4.051341
0.452727	158.008169	4.056346
1.289917	172.231051	4.061350
1.423637	174.487989	4.066355
1.380735	176.494188	4.071360
0.871608	160.369016	4.076365
1.046937	167.460024	4.081370
1.272158	161.964008	4.086374
1.044559	155.017163	4.091379
0.765182	158.218356	4.096384
1.175764	162.058098	4.101389
1.091926	173.524099	4.106394
1.342720	174.297861	4.111398
1.197512	160.890310	4.116403
0.974494	164.705939	4.121408
1.291318	161.748745	4.126413
1.432228	164.194382	4.131418
0.818091	158.418588	4.136422
1.319235	162.168210	4.141427
1.400794	174.696639	4.146432
1.267985	162.201478	4.151437
1.278875	158.172239	4.156442
1.264527	155.988277	4.161446
1.112064	152.376943	4.166451
1.183395	171.437021	4.171456
1.846212	167.631504	4.176461
1.317608	158.536153	4.181466
0.987684	157.211565	4.186470
1.222556	150.622535	4.191475
1.391516	160.169633	4.196480
1.340662	164.581552	4.201485
1.514859	170.081355	4.206490
1.165752	173.271329	4.211494
1.555975	176.054396	4.216499
1.233995	174.908897	4.221504
1.699850	181.324797	4.226509
1.128105	172.388060	4.231514
1.381106	170.032492	4.236518
1.665178	176.663536	4.241523
1.243430	183.095120	4.246528
1.694678	175.020001	4.251533
1.913469	179.813623	4.256538
1.296408	166.385084	4.261542
1.550659	159.388050	4.266547
1.439700	167.678695	4.271552
1.531334	165.841962	4.276557
1.413789	171.235614	4.281562
1.104585	173.887821	4.286566
1.594393	176.101622	4.291571
1.747722	184.347702	4.296576
1.830325	174.862345	4.301581
1.678133	182.064787	4.306586
1.581425	174.708280	4.311590
2.076332	168.012062	4.316595
1.914301	170.682337	4.321600
1.797705	158.538983	4.326605
1.155839	156.159110	4.331610
1.302519	172.344159	4.336614
1.847776	168.639320	4.341619
1.604472	183.246642	4.346624
1.635045	178.413876	4.351629
1.617710	182.845859	4.356634
1.943104	179.890483	4.361638
2.134456	182.359857	4.366643
1.953297	185.580468	4.371648
1.912698	174.197159	4.376653
1.281033	177.336492	4.381658
1.880894	176.685643	4.386662
2.109512	174.893885	4.391667
1.601483	183.347992	4.396672
1.788611	183.983032	4.401677
1.917719	182.181555	4.406682
1.611084	177.123210	4.411686
1.806065	177.263469	4.416691
1.453875	188.331760	4.421696
1.986235	167.788103	4.426701
1.840411	179.178398	4.431706
1.479358	179.051433	4.436710
1.976617	173.863971	4.441715
1.597740	179.390321	4.446720
1.864537	180.079317	4.451725
1.654136	184.367542	4.456730
1.700008	195.215278	4.461734
1.700866	207.180565	4.466739
1.881670	207.607786	4.471744
2.339328	202.784029	4.476749
2.190902	208.451452	4.481754
1.898164	212.448860	4.486758
2.163521	206.380223	4.491763
2.397278	208.450647	4.496768
2.604546	205.656146	4.501773
2.309707	203.997022	4.506778
1.835287	187.439276	4.511782
2.367229	190.443752	4.516787
2.175326	191.799411	4.521792
2.171942	183.324116	4.526797
2.106403	183.043280	4.531802
2.002066	194.585274	4.536806
2.495770	201.224611	4.541811
1.798954	197.119584	4.546816
1.929367	198.279209	4.551821
1.974610	198.170843	4.556826
2.213365	204.815325	4.561830
2.228076	203.427243	4.566835
1.329398	211.847657	4.571840
1.801228	204.386240	4.576845
1.775393	210.607103	4.581850
2.465483	220.388960	4.586854
2.607206	224.210730	4.591859
2.614380	232.327869	4.596864
2.490888	217.477345	4.601869
2.206918	209.292777	4.606874
2.210755	207.801993	4.611878
2.538795	207.269663	4.616883
2.428007	223.571030	4.621888
2.173671	205.608861	4.626893
2.281652	218.212275	4.631898
2.495540	227.670111	4.636902
3.094365	222.457230	4.641907
2.821039	216.764060	4.646912
2.516621	214.125660	4.651917
2.528212	210.409516	4.656922
2.259303	210.451613	4.661926
2.507022	204.952059	4.666931
2.397325	215.858984	4.671936
2.261861	206.958278	4.676941
2.762052	214.764042	4.681946
2.340227	221.771462	4.686950
2.228746	220.178522	4.691955
2.490535	232.814796	4.696960
2.496985	225.027648	4.701965
2.553413	235.329582	4.706970
2.732754	239.756074	4.711974
3.069222	226.225546	4.716979
2.674111	239.148249	4.721984
2.685653	231.458378	4.726989
3.013731	240.063087	4.731994
2.765979	230.142237	4.736998
2.633906	214.242680	4.742003
2.354631	223.663887	4.747008
2.695414	233.851663	4.752013
2.748461	239.133185	4.757018
2.612782	230.017362	4.762022
2.697373	230.269831	4.767027
2.714374	233.301212	4.772032
2.729128	227.328781	4.777037
2.892333	234.677983	4.782042
2.452779	234.936645	4.787046
2.877806	226.606179	4.792051
2.697766	236.584492	4.797056
2.849954	237.259810	4.802061
3.227966	231.907514	4.807066
2.854325	228.884484	4.812070
2.923699	235.362524	4.817075
2.879947	225.140791	4.822080
2.900642	227.424936	4.827085
3.131766	228.337826	4.832090
2.772428	226.274349	4.837094
2.860695	236.742140	4.842099
2.926700	230.034005	4.847104
2.824109	228.227697	4.852109
3.162847	231.366857	4.857114
2.763184	236.469369	4.862118
3.216803	222.373152	4.867123
3.130586	227.882137	4.872128
2.750834	223.369917	4.877133
2.795203	227.368294	4.882138
2.783338	236.500833	4.887142
3.088545	230.217134	4.892147
2.738449	231.736789	4.897152
2.379819	237.256821	4.902157
3.406047	250.488353	4.907162
3.145915	255.255792	4.912166
3.706949	241.645774	4.917171
2.893306	252.229577	4.922176
3.368484	251.364139	4.927181
3.211047	250.629459	4.932186
3.178401	247.761808	4.937190
3.293486	242.729120	4.942195
3.149789	239.366334	4.947200
3.283495	241.654922	4.952205
3.407158	236.177959	4.957210
3.084401	238.721566	4.962214
3.115714	239.694237	4.967219
3.316057	245.180475	4.972224
3.171009	248.803569	4.977229
3.504219	258.287018	4.982234
3.217601	259.894808	4.987238
3.457297	247.948672	4.992243
3.512551	255.030054	4.997248
3.603098	251.725479	5.002253
3.420021	239.497571	5.007258
2.923472	234.412019	5.012262
3.634589	233.857632	5.017267
3.321631	255.793790	5.022272
3.611605	252.556046	5.027277
3.398205	247.198331	5.032282
3.566009	255.420030	5.037286
3.313241	245.458827	5.042291
3.382224	255.717676	5.047296
3.271433	254.456824	5.052301
3.634809	254.168896	5.057306
3.220217	257.846879	5.062310
3.419006	250.159300	5.067315
3.192234	263.833941	5.072320
3.207623	255.735326	5.077325
3.474473	253.538931	5.082330
3.111918	255.766068	5.087334
3.454516	250.972981	5.092339
3.138362	258.520687	5.097344
3.352606	257.629693	5.102349
3.876328	264.226385	5.107354
3.651833	278.916260	5.112358
3.763702	268.318937	5.117363
3.391430	263.413223	5.122368
3.707819	273.117619	5.127373
3.647540	263.600817	5.132378
3.714762	272.240085	5.137382
4.021721	269.524868	5.142387
3.933780	262.413728	5.147392
3.585760	254.207536	5.152397
3.953870	250.881619	5.157402
3.231365	256.366919	5.162406
4.110626	254.387787	5.167411
3.717866	271.388284	5.172416
4.105159	269.331207	5.177421
3.773227	252.728927	5.182426
3.559456	256.470359	5.187430
3.771865	258.392272	5.192435
3.642261	269.049245	5.197440
3.632632	269.851159	5.202445
3.513749	275.776572	5.207450
3.602587	278.034228	5.212454
4.109747	271.266448	5.217459
4.064212	278.537640	5.222464
3.872877	271.683145	5.227469
3.990549	277.546184	5.232474
3.872203	283.895464	5.237478
3.956677	272.815205	5.242483
3.744958	269.450416	5.247488
3.645908	282.415350	5.252493
3.930516	280.912207	5.257498
3.884563	272.949748	5.262502
3.679351	273.924678	5.267507
3.870694	284.344709	5.272512
3.937990	280.195872	5.277517
3.988117	278.248570	5.282522
4.230901	288.837717	5.287526
4.427750	280.960600	5.292531
4.264967	285.345793	5.297536
4.261608	281.106784	5.302541
4.108733	274.888515	5.307546
3.809986	277.184752	5.312550
3.859442	267.796289	5.317555
3.863478	284.544800	5.322560
4.242737	291.486845	5.327565
4.491650	293.675129	5.332570
4.273124	296.423879	5.337574
4.444030	283.232466	5.342579
4.255055	283.012098	5.347584
4.010857	280.332615	5.352589
4.287403	278.884520	5.357594
4.250257	286.303100	5.362598
4.254275	270.309402	5.367603
4.219797	289.531719	5.372608
4.151335	286.309000	5.377613
4.509496	293.456834	5.382618
4.417294	293.793953	5.387622
4.774015	284.540840	5.392627
4.358246	283.498615	5.397632
4.191847	283.546798	5.402637
4.163427	281.652931	5.407642
4.221330	278.293354	5.412646
4.629424	288.625642	5.417651
4.272877	294.044123	5.422656
4.466133	293.567710	5.427661
4.580441	300.374098	5.432666
4.014937	299.719171	5.437670
4.683231	300.193403	5.442675
4.805841	308.393733	5.447680
4.343721	298.072990	5.452685
4.358280	296.561536	5.457690
4.487822	304.393776	5.462694
4.750862	303.393892	5.467699
4.190183	296.730137	5.472704
4.306268	308.554050	5.477709
4.640324	302.851110	5.482714
4.607471	312.395108	5.487718
4.553667	305.781647	5.492723
4.420672	312.076284	5.497728
4.706944	307.247714	5.502733
4.762166	305.609664	5.507738
4.777317	304.841612	5.512742
4.659165	307.590456	5.517747
4.698212	309.378182	5.522752
4.822523	301.749708	5.527757
4.963741	304.657233	5.532762
4.764836	310.155425	5.537766
4.657443	295.884454	5.542771
4.827228	301.644421	5.547776
4.572866	297.868686	5.552781
4.717847	297.747856	5.557786
4.679503	306.489104	5.562790
5.031035	301.830647	5.567795
4.951461	300.049199	5.572800
4.724111	300.951669	5.577805
4.746928	289.137564	5.582810
4.405587	301.634265	5.587814
4.837802	304.432920	5.592819
4.646342	309.610401	5.597824
4.563024	308.462301	5.602829
4.861921	306.235568	5.607834
4.361882	305.766540	5.612838
5.070049	304.481774	5.617843
4.732401	306.806257	5.622848
4.658953	302.201731	5.627853
4.842228	311.404976	5.632858
4.392480	308.691254	5.637862
4.907642	318.060805	5.642867
5.072465	327.532709	5.647872
5.288369	328.251832	5.652877
5.211489	315.086564	5.657882
4.661918	317.482218	5.662886
4.795696	302.274933	5.667891
5.134442	319.116568	5.672896
5.099483	321.732155	5.677901
5.163167	312.382570	5.682906
4.748198	317.664676	5.687910
5.288375	318.355138	5.692915
5.362177	329.904110	5.697920
5.332034	323.315411	5.702925
5.036699	320.071284	5.707930
4.766293	317.101666	5.712934
5.574828	315.402534	5.717939
4.798834	318.801790	5.722944
5.036100	322.861716	5.727949
5.262807	323.398809	5.732954
5.344480	335.060449	5.737958
5.428079	332.801006	5.742963
5.333350	334.122468	5.747968
4.821246	314.286468	5.752973
5.216927	314.313023	5.757978
5.280718	327.673262	5.762982
5.407974	322.939206	5.767987
5.518743	331.255299	5.772992
5.094602	318.457655	5.777997
5.739221	329.654595	5.783002
4.948310	318.967732	5.788006
5.126531	318.139327	5.793011
5.465028	332.481604	5.798016
5.501812	337.082319	5.803021
5.241209	335.288102	5.808026
5.148312	331.657907	5.813030
5.442014	329.539555	5.818035
5.162694	333.256471	5.823040
5.341216	326.470558	5.828045
5.286983	326.713142	5.833050
5.068359	332.015110	5.838054
4.970501	334.238749	5.843059
5.017724	338.742914	5.848064
5.091734	332.520714	5.853069
5.490616	337.071022	5.858074
5.583647	352.369281	5.863078
5.857076	351.162119	5.868083
5.363385	360.272136	5.873088
5.572844	360.599957	5.878093
5.621445	347.351728	5.883098
5.494234	351.933848	5.888102
5.877157	345.770812	5.893107
5.741266	339.217658	5.898112
5.382807	331.528768	5.903117
5.344209	332.638951	5.908122
5.535901	347.288984	5.913126
5.632546	347.004881	5.918131
5.614016	353.825775	5.923136
5.709388	357.370091	5.928141
5.734575	352.171120	5.933146
5.636404	361.019847	5.938150
5.943575	346.747157	5.943155
5.591776	354.661164	5.948160
5.864699	351.252064	5.953165
5.836511	351.038141	5.958170
5.507241	350.314560	5.963174
5.786048	355.921419	5.968179
5.751893	355.426851	5.973184
5.564207	350.697840	5.978189
5.738210	353.166793	5.983194
5.314864	356.561425	5.988198
5.825490	352.941070	5.993203
5.499038	348.512218	5.998208
5.415578	353.432340	6.003213
5.501803	355.775838	6.008218
5.233085	357.355521	6.013222
5.868485	367.278910	6.018227
5.931924	379.845124	6.023232
6.040373	374.376831	6.028237
6.276568	379.294333	6.033242
6.014214	373.286176	6.038246
5.915512	361.127224	6.043251
5.917745	362.844792	6.048256
5.824599	354.358169	6.053261
5.938077	355.542604	6.058266
5.826328	367.335813	6.063270
5.992002	351.753321	6.068275
5.844367	355.405316	6.073280
5.562254	355.924054	6.078285
5.840377	353.684752	6.083290
5.793200	350.098011	6.088294
5.965862	348.606075	6.093299
6.107412	357.062892	6.098304
5.818176	354.899829	6.103309
6.247282	355.566566	6.108314
5.833442	349.373339	6.113318
6.080439	355.826758	6.118323
5.864279	361.767440	6.123328
5.701314	351.089740	6.128333
5.769645	344.014194	6.133338
5.581279	357.357015	6.138342
5.937897	357.525735	6.143347
6.259418	347.762402	6.148352
6.333194	355.508488	6.153357
6.211351	349.566910	6.158362
6.013537	357.595999	6.163366
5.979695	347.477049	6.168371
6.053633	337.116586	6.173376
5.534970	330.610754	6.178381
5.872123	335.645306	6.183386
5.463363	345.431720	6.188390
5.673650	342.174807	6.193395
5.863971	352.500124	6.198400
5.768959	344.959780	6.203405
5.763833	354.967701	6.208410
5.839532	355.866984	6.213414
5.799313	357.433012	6.218419
5.827260	363.639174	6.223424
5.793936	361.698611	6.228429
6.162080	356.597766	6.233434
6.041434	358.976842	6.238438
6.236206	345.617125	6.243443
5.887915	340.299500	6.248448
5.515297	342.933192	6.253453
5.788630	345.345451	6.258458
5.337568	358.324464	6.263462
5.720219	357.416571	6.268467
5.879014	360.735811	6.273472
5.737542	364.915200	6.278477
6.114718	363.176079	6.283482
5.920601	369.809350	6.288486
5.984154	359.649823	6.293491
5.882191	366.012385	6.298496
6.050531	360.525220	6.303501
5.867176	356.346034	6.308506
5.695535	358.948239	6.313510
5.779227	359.286274	6.318515
6.052178	363.963890	6.323520
5.638839	349.914822	6.328525
5.986243	351.372659	6.333530
5.904264	357.830165	6.338534
5.927904	349.511912	6.343539
5.611692	348.169341	6.348544
6.094554	355.300826	6.353549
6.086632	342.833428	6.358554
5.643534	343.953204	6.363558
5.387110	337.656222	6.368563
5.656567	347.178183	6.373568
5.647119	366.472593	6.378573
6.317829	363.624437	6.383578
6.043342	365.815642	6.388582
5.740775	354.321400	6.393587
5.567708	355.490619	6.398592
5.677939	360.168419	6.403597
5.976873	358.514326	6.408602
5.914541	366.813263	6.413606
5.850853	352.541727	6.418611
6.119531	358.909490	6.423616
5.631170	350.503775	6.428621
5.268852	354.388727	6.433626
5.160094	363.201147	6.438630
5.146363	359.137755	6.443635
5.746656	364.719556	6.448640
6.010404	365.092656	6.453645
5.772208	366.259425	6.458650
5.790387	368.648389	6.463654
5.854153	365.990244	6.468659
5.841769	361.376136	6.473664
5.742981	359.031369	6.478669
5.792610	356.796229	6.483674
5.480791	366.592777	6.488678
5.698057	362.018618	6.493683
5.968692	378.611548	6.498688
6.035428	370.229584	6.503693
5.964973	369.063646	6.508698
5.542216	367.209409	6.513702
5.938673	355.830274	6.518707
5.874416	363.265789	6.523712
5.775777	353.552465	6.528717
6.291834	359.425879	6.533722
5.743564	364.140414	6.538726
5.988298	357.122648	6.543731
5.976128	355.722948	6.548736
5.731626	361.788295	6.553741
5.957855	358.785151	6.558746
5.880801	362.248915	6.563750
5.574626	357.756770	6.568755
5.741417	362.865480	6.573760
5.556191	368.643127	6.578765
5.855854	362.958212	6.583770
5.849891	371.855773	6.588774
5.903320	355.591660	6.593779
5.811016	360.203115	6.598784
5.566053	363.977931	6.603789
6.078226	366.049044	6.608794
5.545416	365.983790	6.613798
5.834428	367.033153	6.618803
6.303188	373.233528	6.623808
5.902047	366.709268	6.628813
5.840538	366.291754	6.633818
5.961802	364.330133	6.638822
5.948765	364.664341	6.643827
5.765665	363.617294	6.648832
5.792320	362.338063	6.653837
5.841441	352.762943	6.658842
5.678080	355.088598	6.663846
5.754225	358.310054	6.668851
5.704555	360.136996	6.673856
5.432876	366.567279	6.678861
6.159777	377.957006	6.683866
5.806063	370.204078	6.688870
5.795600	365.390347	6.693875
5.785448	367.451549	6.698880
6.038936	381.917918	6.703885
6.056224	362.308974	6.708890
5.760341	371.941673	6.713894
5.655281	363.928321	6.718899
5.846971	361.446291	6.723904
5.855628	363.811435	6.728909
5.863521	365.562919	6.733914
5.805443	369.210376	6.738918
5.684979	372.510097	6.743923
5.847715	368.374760	6.748928
5.824507	380.695118	6.753933
5.909889	369.728553	6.758938
5.634656	369.126222	6.763942
6.103024	379.964822	6.768947
6.183908	383.134919	6.773952
5.887230	369.504165	6.778957
6.064627	369.254866	6.783962
5.628100	367.516685	6.788966
5.864682	358.804387	6.793971
6.200116	362.564197	6.798976
5.755111	371.568514	6.803981
5.782800	359.437217	6.808986
5.635298	377.819943	6.813990
5.771019	368.155315	6.818995
5.693892	366.408279	6.824000
5.663304	370.136852	6.829005
5.853187	361.840003	6.834010
5.481779	368.266930	6.839014
5.841343	377.755806	6.844019
5.924534	383.380667	6.849024
5.924285	379.349960	6.854029
5.866480	371.310219	6.859034
6.138417	369.660354	6.864038
5.983577	371.652475	6.869043
6.045571	367.827158	6.874048
5.547113	364.402872	6.879053
5.700081	353.878154	6.884058
5.819703	372.127270	6.889062
5.675108	370.555324	6.894067
5.595083	373.105211	6.899072
5.819696	382.118513	6.904077
6.310058	382.823111	6.909082
5.876511	377.907983	6.914086
5.805583	364.191241	6.919091
5.934769	374.023102	6.924096
5.643399	365.845948	6.929101
5.979796	359.323194	6.934106
5.906496	372.632178	6.939110
6.030332	367.882827	6.944115
5.808378	363.130708	6.949120
5.587040	370.002367	6.954125
6.012199	364.636317	6.959130
5.578723	369.222134	6.964134
5.786995	362.282847	6.969139
5.821209	358.955440	6.974144
5.552581	374.709024	6.979149
5.961324	366.396865	6.984154
5.737347	378.115914	6.989158
5.774480	375.164542	6.994163
5.993953	382.245555	6.999168
5.712772	375.971421	7.004173
6.087638	364.282445	7.009178
5.952311	366.027894	7.014182
5.573698	370.367829	7.019187
5.702273	367.924161	7.024192
5.790158	378.730625	7.029197
6.139302	384.421387	7.034202
6.019234	377.717040	7.039206
6.105269	359.872231	7.044211
6.011095	360.940502	7.049216
5.748138	370.064994	7.054221
5.846966	364.341941	7.059226
5.641102	357.189127	7.064230
5.823062	360.884396	7.069235
5.999495	364.919061	7.074240
5.634866	370.212278	7.079245
5.890617	361.085680	7.084250
5.666265	369.913051	7.089254
5.725413	361.494314	7.094259
5.760133	353.297712	7.099264
5.661821	364.569947	7.104269
6.027764	359.159392	7.109274
5.656467	354.006723	7.114278
5.954246	358.519093	7.119283
6.036842	369.620614	7.124288
5.856298	372.888619	7.129293
6.026612	362.595301	7.134298
5.957218	370.234108	7.139302
5.646471	363.746308	7.144307
5.950133	358.848558	7.149312
5.725789	372.374202	7.154317
5.803376	365.642054	7.159322
6.038304	364.738323	7.164326
5.749669	370.585957	7.169331
6.217523	365.956716	7.174336
5.892673	358.964916	7.179341
6.475286	364.558978	7.184346
5.845801	368.662967	7.189350
5.899248	369.290485	7.194355
6.556122	367.551834	7.199360
6.094754	366.858441	7.204365
6.018007	360.922449	7.209370
5.681912	348.354603	7.214374
5.750248	354.769573	7.219379
6.138549	353.917743	7.224384
5.702160	359.829654	7.229389
5.716442	342.160624	7.234394
5.724936	355.137234	7.239398
5.874079	362.333665	7.244403
5.761769	367.536727	7.249408
6.170542	363.878544	7.254413
6.009344	352.877856	7.259418
5.603261	341.241652	7.264422
5.487520	343.021996	7.269427
5.698018	348.342156	7.274432
5.561427	361.186476	7.279437
5.922973	365.211120	7.284442
5.651640	366.449521	7.289446
5.950454	362.893990	7.294451
6.157857	362.836148	7.299456
5.903826	375.531196	7.304461
6.019933	364.173835	7.309466
6.055263	359.900271	7.314470
5.393062	355.524022	7.319475
5.937821	366.765106	7.324480
5.629196	363.532544	7.329485
5.809863	360.599815	7.334490
5.564911	361.565157	7.339494
5.391005	359.058150	7.344499
5.600813	370.256802	7.349504
5.533957	367.464096	7.354509
5.797234	368.780088	7.359514
5.704557	369.851289	7.364518
5.716371	378.973864	7.369523
5.689653	383.530755	7.374528
5.781209	369.427875	7.379533
5.699686	366.618484	7.384538
5.691677	377.035002	7.389542
5.587154	373.305378	7.394547
5.885038	384.892044	7.399552
6.164113	384.819808	7.404557
6.424595	374.158007	7.409562
5.965054	374.524208	7.414566
5.837613	373.996799	7.419571
5.668603	362.981510	7.424576
5.741076	367.117886	7.429581
6.056908	359.519492	7.434586
5.873270	362.120414	7.439590
5.919629	371.566609	7.444595
6.002617	361.745728	7.449600
5.619570	365.096080	7.454605
5.917338	374.771811	7.459610
6.001713	367.747528	7.464614
6.072196	364.082236	7.469619
5.786691	366.025225	7.474624
5.843752	366.709126	7.479629
6.047765	367.860394	7.484634
5.821367	364.713027	7.489638
5.979157	364.469965	7.494643
5.749651	369.466758	7.499648
5.654507	372.259464	7.504653
5.959189	370.250121	7.509658
5.621657	368.483773	7.514662
5.514636	369.535075	7.519667
5.905295	360.969482	7.524672
5.717238	362.552346	7.529677
5.977718	362.391273	7.534682
5.998474	364.340062	7.539686
5.757441	361.966960	7.544691
6.076875	363.663304	7.549696
6.094425	364.954520	7.554701
5.990987	358.839209	7.559706
5.699375	360.571179	7.564710
5.833395	364.378366	7.569715
5.786147	364.575562	7.574720
5.598630	363.579829	7.579725
6.107995	361.627004	7.584730
5.774457	366.225636	7.589734
5.923711	370.201284	7.594739
6.186537	370.061989	7.599744
5.896424	363.226100	7.604749
5.719652	355.521387	7.609754
5.879229	360.276879	7.614758
5.631539	360.505480	7.619763
5.811514	362.169889	7.624768
5.709624	369.029160	7.629773
5.863623	363.085488	7.634778
6.005965	365.246185	7.639782
5.909758	375.948610	7.644787
5.951286	364.634572	7.649792
5.443432	370.361526	7.654797
6.445485	360.849072	7.659802
6.178182	377.377586	7.664806
6.023028	364.787706	7.669811
5.720023	344.314621	7.674816
6.019844	359.953817	7.679821
5.807639	345.987135	7.684826
5.769555	343.069700	7.689830
5.554744	344.599806	7.694835
6.291787	342.775829	7.699840
5.755459	344.818228	7.704845
5.506303	337.694351	7.709850
6.353722	357.430310	7.714854
5.842007	345.383538	7.719859
5.727013	341.598612	7.724864
5.565291	337.431859	7.729869
5.729001	351.915435	7.734874
6.023882	353.226474	7.739878
5.928922	347.081365	7.744883
5.671717	342.559405	7.749888
5.399123	342.893150	7.754893
5.873686	348.197247	7.759898
5.667746	359.622387	7.764902
5.987051	373.572226	7.769907
6.008856	361.210891	7.774912
6.012183	359.669554	7.779917
5.993743	355.812549	7.784922
5.957233	344.602501	7.789926
5.819214	340.378249	7.794931
5.986561	332.806294	7.799936
5.668583	336.279327	7.804941
5.701028	337.561880	7.809946
5.784637	343.851065	7.814950
5.678727	362.176636	7.819955
6.074688	356.505110	7.824960
5.754886	355.055531	7.829965
5.748379	342.116503	7.834970
5.777790	345.395900	7.839974
5.647102	357.786867	7.844979
6.133619	352.041041	7.849984
5.937351	367.688367	7.854989
5.876144	361.310169	7.859994
5.956745	340.621957	7.864998
5.597214	340.004360	7.870003
6.178170	342.270342	7.875008
6.036481	350.312781	7.880013
5.788557	339.869867	7.885018
5.761110	341.813550	7.890022
5.553237	342.750935	7.895027
5.618419	341.332789	7.900032
5.657114	347.467657	7.905037
5.998312	352.340226	7.910042
6.033409	371.241675	7.915046
6.188408	353.227876	7.920051
5.833028	346.022561	7.925056
5.398251	338.212745	7.930061
5.780174	345.404335	7.935066
6.046101	365.199773	7.940070
5.771359	350.546847	7.945075
5.775117	341.285731	7.950080
6.004309	354.211942	7.955085
5.660340	346.463826	7.960090
5.603739	349.085972	7.965094
5.540576	361.618225	7.970099
6.135742	353.887479	7.975104
6.122659	365.883531	7.980109
5.889251	358.757178	7.985114
5.899632	346.106573	7.990118
5.841843	346.392691	7.995136
6.032768	334.421403	8.000154
5.557882	338.759183	8.005171
5.948493	343.914392	8.010189
5.725781	341.393097	8.015206
5.620970	345.619247	8.020224
6.160009	352.029279	8.025242
5.969485	353.087868	8.030259
5.727818	347.874535	8.035277
6.056329	353.926241	8.040294
5.822122	354.947493	8.045312
5.810593	339.934225	8.050330
5.975625	356.031038	8.055347
5.801020	353.031998	8.060365
5.859294	356.976982	8.065382
5.808741	359.749302	8.070400
6.033210	361.468692	8.075418
5.828639	368.610611	8.080435
6.103387	354.824242	8.085453
6.192659	355.542353	8.090470
5.699665	344.164200	8.095488
5.861795	358.156588	8.100506
6.109765	368.863024	8.105523
6.003237	359.213620	8.110541
6.106453	344.864011	8.115558
5.882447	341.724392	8.120576
5.807747	345.563979	8.125594
5.885762	352.980346	8.130611
5.908351	366.963046	8.135629
6.055944	370.496415	8.140646
5.794965	367.577177	8.145664
5.970258	369.774479	8.150682
6.024581	374.783574	8.155699
6.342994	371.328594	8.160717
6.031075	361.515714	8.165734
5.749502	363.885582	8.170752
6.035763	364.042662	8.175770
6.050637	361.402089	8.180787
6.236702	352.953366	8.185805
6.142559	360.418800	8.190822
5.988941	357.331266	8.195840
6.167263	347.700353	8.200858
5.776590	351.791416	8.205875
6.160226	356.793089	8.210893
6.489390	350.215395	8.215910
5.762728	345.866988	8.220928
6.010185	346.913757	8.225946
5.950013	353.111567	8.230963
6.199258	356.565891	8.235981
5.976369	359.314721	8.240998
6.057268	361.391115	8.246016
5.965202	359.572014	8.251034
5.951751	363.575574	8.256051
6.138295	359.298673	8.261069
5.888981	360.189752	8.266086
5.844867	366.110500	8.271104
6.508778	351.436354	8.276122
5.967933	359.255795	8.281139
5.985597	363.857228	8.286157
6.150370	362.092558	8.291174
6.278079	367.566671	8.296192
6.414722	359.662165	8.301210
6.068058	361.215425	8.306227
6.164758	371.437489	8.311245
6.112952	355.985556	8.316262
6.072739	362.224423	8.321280
6.069015	363.443089	8.326298
6.183265	364.636960	8.331315
6.134461	370.536355	8.336333
6.071514	365.184563	8.341350
6.243256	366.151679	8.346368
6.265335	359.786195	8.351386
5.887706	363.004230	8.356403
5.848018	361.142209	8.361421
5.912729	364.180487	8.366438
5.468696	370.921277	8.371456
6.499840	382.120384	8.376474
6.154597	391.726905	8.381491
5.948568	389.177743	8.386509
6.692204	383.661700	8.391526
6.336783	386.699538	8.396544
6.442645	381.804123	8.401562
6.245277	378.171183	8.406579
6.130284	375.620383	8.411597
6.370111	359.018242	8.416614
6.158000	358.587544	8.421632
6.502184	368.556239	8.426650
6.534895	366.998449	8.431667
6.347511	360.706808	8.436685
6.318965	360.282063	8.441702
6.027692	366.661251	8.446720
6.031822	355.164177	8.451738
6.316902	373.283965	8.456755
6.330367	378.163766	8.461773
6.634024	381.568545	8.466790
6.323194	370.433229	8.471808
6.213936	364.318690	8.476826
6.232017	368.298377	8.481843
6.830360	377.271062	8.486861
6.722755	374.046930	8.491878
6.271470	370.286521	8.496896
6.422872	365.346105	8.501914
6.482198	365.264192	8.506931
6.044612	362.527256	8.511949
5.916560	357.886244	8.516966
6.226828	372.003752	8.521984
6.492617	380.410017	8.527002
6.576525	394.421000	8.532019
6.632044	382.720200	8.537037
6.517192	364.286486	8.542054
6.285568	370.612149	8.547072
6.201049	357.759368	8.552090
5.696722	363.064269	8.557107
6.443475	382.727474	8.562125
6.697307	384.918784	8.567143
6.605152	397.168044	8.572160
6.380036	380.219016	8.577178
6.911309	386.993189	8.582195
6.697331	386.234585	8.587213
6.359635	375.832454	8.592231
6.482324	377.671932	8.597248
6.622491	375.541893	8.602266
6.739593	368.681843	8.607283
6.394501	365.378159	8.612301
6.361145	362.177108	8.617319
6.400899	366.194424	8.622336
6.286398	364.154779	8.627354
6.570461	384.310196	8.632371
6.378555	388.985496	8.637389
6.628273	387.008701	8.642407
6.585129	391.632292	8.647424
6.375049	389.061675	8.652442
6.761253	384.870247	8.657459
6.596561	386.193030	8.662477
7.015482	385.594035	8.667495
6.360028	373.026353	8.672512
6.277484	375.456555	8.677530
6.564341	381.262337	8.682547
6.599973	384.548168	8.687565
6.994813	380.822440	8.692583
6.455717	379.584610	8.697600
6.630670	374.769887	8.702618
6.679116	373.582010	8.707635
6.390279	381.930011	8.712653
6.638911	386.397433	8.717671
6.590637	394.442665	8.722688
6.692465	386.928604	8.727706
6.541102	386.169657	8.732723
6.714509	395.559220	8.737741
6.711468	378.957244	8.742759
6.518320	377.781974	8.747776
6.539870	388.075781	8.752794
6.730506	389.292398	8.757811
6.512400	387.814929	8.762829
6.656453	389.026222	8.767847
6.775289	386.817474	8.772864
6.373083	388.114356	8.777882
6.444992	391.716391	8.782899
6.208092	393.208275	8.787917
6.394184	387.486102	8.792935
6.356713	392.301305	8.797952
6.616582	388.186475	8.802970
7.060072	388.669209	8.807987
6.563940	392.966150	8.813005
6.636639	396.697448	8.818023
6.832042	392.015215	8.823040
6.693953	402.744290	8.828058
6.710577	390.620396	8.833075
6.576012	395.797946	8.838093
7.215171	387.038378	8.843111
6.649525	389.749399	8.848128
6.646888	394.562300	8.853146
6.541671	389.769381	8.858163
6.307865	392.551483	8.863181
6.808183	398.620466	8.868199
7.072936	408.033593	8.873216
6.776568	407.720236	8.878234
6.999759	404.090824	8.883251
6.789578	399.585743	8.888269
6.689259	396.534031	8.893287
6.823242	396.516158	8.898304
6.680905	406.551635	8.903322
7.254274	412.479792	8.908339
6.831750	405.259315	8.913357
6.809972	398.348431	8.918375
6.826501	407.144052	8.923392
6.517319	399.549218	8.928410
6.615125	407.773536	8.933427
6.855097	413.536182	8.938445
6.999447	408.382268	8.943463
7.202007	409.473944	8.948480
6.617449	413.036830	8.953498
7.038263	412.926680	8.958515
6.849471	417.358507	8.963533
7.018715	409.003909	8.968551
7.284658	417.318651	8.973568
6.948410	399.102623	8.978586
6.741941	396.149593	8.983603
6.476164	407.952700	8.988621
6.976511	401.143042	8.993639
7.060056	415.450739	8.998656
6.613630	409.022945	9.003674
6.864178	408.377748	9.008691
6.858075	411.149423	9.013709
6.847154	410.945973	9.018727
6.788407	416.001198	9.023744
6.664187	413.312985	9.028762
7.064761	403.461029	9.033779
6.568326	419.263913	9.038797
7.193709	413.908399	9.043815
7.138073	410.603534	9.048832
6.968267	417.238260	9.053850
7.394968	405.782241	9.058867
7.154020	408.956778	9.063885
7.014270	404.630006	9.068903
6.854759	413.967601	9.073920
6.749517	412.642857	9.078938
7.138063	410.395004	9.083955
6.730345	412.456444	9.088973
6.677722	402.912178	9.093991
7.155888	405.418630	9.099008
7.138443	409.716312	9.104026
7.059850	407.235542	9.109043
6.974543	406.857559	9.114061
7.033178	412.004842	9.119079
7.179229	404.303967	9.124096
7.160883	406.986042	9.129114
7.040954	410.671786	9.134131
6.894344	402.969430	9.139149
7.146841	420.226537	9.144167
7.396113	429.187671	9.149184
7.314429	423.059325	9.154202
7.640756	410.618653	9.159219
7.221339	407.440214	9.164237
7.226992	397.596490	9.169255
7.329843	405.135218	9.174272
6.702900	410.124835	9.179290
6.867515	409.960153	9.184307
7.249384	406.321658	9.189325
7.298601	406.796741	9.194343
7.443407	396.457852	9.199360
6.977197	408.226092	9.204378
7.417853	397.708307	9.209395
6.940885	406.417150	9.214413
7.192883	405.437215	9.219431
7.478888	403.975433	9.224448
7.170492	404.850525	9.229466
7.033055	418.549074	9.234483
7.062778	407.366688	9.239501
7.013512	413.547032	9.244519
7.441942	422.353861	9.249536
7.348418	424.732142	9.254554
7.343326	429.327691	9.259571
7.330171	422.481717	9.264589
7.326280	417.407831	9.269607
7.097621	418.658588	9.274624
7.461276	426.658228	9.279642
7.457765	422.534164	9.284659
6.868865	414.266793	9.289677
7.291320	427.543115	9.294695
7.411149	427.196105	9.299712
6.872797	427.460297	9.304730
7.078502	425.894331	9.309747
6.880150	439.400472	9.314765
7.293827	424.714981	9.319783
7.282476	423.236672	9.324800
6.984941	428.247265	9.329818
7.453706	431.607249	9.334835
7.385904	437.462306	9.339853
7.263620	432.608934	9.344871
7.488590	424.356050	9.349888
7.159853	435.780882	9.354906
7.553470	425.314631	9.359923
7.231744	428.274614	9.364941
7.260920	420.749832	9.369959
7.299651	434.076813	9.374976
7.196057	433.089476	9.379994
7.542297	447.068866	9.385011
7.826636	445.948164	9.390029
7.364557	431.926893	9.395047
7.766846	415.229819	9.400064
7.304265	432.987136	9.405082
7.713425	431.184168	9.410099
7.698755	432.070044	9.415117
7.603028	429.449946	9.420135
7.697469	419.617545	9.425152
7.343597	429.809254	9.430170
7.659914	425.209051	9.435187
7.715912	430.927946	9.440205
7.801959	435.319870	9.445223
7.514703	431.524281	9.450240
7.240479	443.764230	9.455258
7.168453	430.073161	9.460275
7.601644	437.052067	9.465293
7.616334	434.351553	9.470311
7.177820	426.414060	9.475328
7.515159	425.499647	9.480346
7.768605	433.380859	9.485363
7.523308	427.729420	9.490381
7.339724	429.437013	9.495399
7.610209	427.172941	9.500416
7.541125	434.309437	9.505434
7.356500	430.191658	9.510451
7.607096	438.215328	9.515469
7.930997	447.937941	9.520487
8.127289	428.871593	9.525504
7.740312	429.408709	9.530522
7.710046	426.652125	9.535539
7.760269	432.169956	9.540557
7.681156	424.958781	9.545575
7.769194	430.921960	9.550592
7.738452	429.544518	9.555610
7.717530	436.095964	9.560627
7.610943	432.117434	9.565645
7.369474	438.684502	9.570663
8.084995	427.009649	9.575680
8.047021	433.686841	9.580698
7.915107	429.500844	9.585715
8.100694	425.217766	9.590733
7.886137	430.530933	9.595751
7.790986	429.965146	9.600768
7.359920	436.192695	9.605786
7.589874	431.861639	9.610803
7.561336	432.702351	9.615821
7.218362	440.973655	9.620839
7.755723	435.575122	9.625856
7.276175	438.970083	9.630874
7.585919	429.990712	9.635891
7.579651	435.441657	9.640909
7.534981	445.253573	9.645927
7.871313	448.492302	9.650944
7.875981	453.654365	9.655962
7.968724	462.176143	9.660979
8.018863	461.237300	9.665997
7.719239	445.420181	9.671015
7.896406	442.804660	9.676032
7.698830	450.270559	9.681050
7.907883	452.481517	9.686067
8.034268	446.077569	9.691085
7.579337	450.456429	9.696103
8.122912	459.557656	9.701120
7.708586	444.272900	9.706138
7.989089	445.481752	9.711155
7.959332	441.920366	9.716173
7.625498	445.159956	9.721191
7.924567	456.249753	9.726208
7.850116	459.376123	9.731226
7.879582	463.025847	9.736243
7.609599	452.464741	9.741261
7.896497	458.620831	9.746279
7.878061	454.000488	9.751296
7.922852	463.971965	9.756314
7.633539	463.222005	9.761331
7.757354	464.947709	9.766349
7.738468	461.656012	9.771367
8.018781	460.681105	9.776384
7.790060	466.324702	9.781402
8.153870	464.828634	9.786419
7.989949	462.257086	9.791437
8.194070	466.425393	9.796455
8.393003	462.591489	9.801472
8.246823	459.155637	9.806490
8.112168	469.641221	9.811507
8.019947	467.702214	9.816525
7.908930	457.838868	9.821543
8.267008	459.900247	9.826560
8.171759	458.460327	9.831578
7.949185	461.000842	9.836595
8.053392	467.965034	9.841613
7.770418	463.297775	9.846631
8.068614	461.603707	9.851648
8.312919	461.054159	9.856666
7.840651	459.717491	9.861683
8.281729	465.243520	9.866701
8.140577	460.727608	9.871719
8.279457	465.874957	9.876736
8.114882	462.899573	9.881754
7.985540	464.254692	9.886771
8.087287	450.495356	9.891789
7.920786	462.699505	9.896807
7.903220	457.836031	9.901824
8.178459	464.230632	9.906842
8.007936	462.894023	9.911859
8.293418	464.190458	9.916877
8.021940	464.952472	9.921895
8.342323	457.991110	9.926912
8.471710	457.336493	9.931930
8.130340	451.283538	9.936947
8.196171	456.571717	9.941965
8.035939	460.724527	9.946983
8.343927	454.620322	9.952000
8.328201	457.402979	9.957018
8.204177	469.063997	9.962035
8.372137	467.128406	9.967053
7.825941	475.381075	9.972071
8.319693	462.320851	9.977088
8.365182	461.278596	9.982106
8.556829	463.470192	9.987123
8.473708	460.213806	9.992141
7.925523	465.178474	9.997159
8.477320	452.282730	10.002176
8.215707	467.720665	10.007194
8.037970	459.442500	10.012211
8.137589	462.973936	10.017229
7.988674	466.077260	10.022247
8.183140	467.545745	10.027264
8.624873	474.968290	10.032282
8.252732	485.153425	10.037299
8.621266	476.988475	10.042317
7.996601	473.782223	10.047335
8.340194	485.152236	10.052352
8.186086	485.605531	10.057370
8.616227	486.080892	10.062387
8.738245	479.649214	10.067405
7.994377	482.766865	10.072423
8.460964	488.137427	10.077440
8.232332	480.567808	10.082458
8.397138	481.091054	10.087475
8.529444	485.923862	10.092493
8.359970	484.839548	10.097511
8.311531	479.750533	10.102528
8.547973	485.311787	10.107546
8.745364	482.639444	10.112563
8.788844	487.965847	10.117581
8.739054	489.636703	10.122599
8.226940	470.327859	10.127616
8.342512	472.727034	10.132634
8.107829	482.814892	10.137651
8.463661	483.172509	10.142669
8.300147	486.836696	10.147687
8.273086	480.661902	10.152704
8.294570	476.982029	10.157722
8.377211	480.064854	10.162739
8.710580	479.188930	10.167757
8.453399	484.480390	10.172775
8.528234	486.933285	10.177792
8.648414	481.398133	10.182810
8.478341	491.983952	10.187827
8.321696	488.748548	10.192845
8.466248	493.879238	10.197863
8.439123	492.106752	10.202880
8.828291	489.902972	10.207898
8.255504	489.576120	10.212915
8.742566	491.822418	10.217933
8.349280	498.135586	10.222951
8.649713	502.225696	10.227968
8.910504	504.182404	10.232986
8.701067	505.234497	10.238003
8.824832	500.011200	10.243021
8.575337	499.759924	10.248039
8.602443	491.888301	10.253056
8.628426	497.375237	10.258074
8.767004	506.975441	10.263091
8.832964	514.570487	10.268109
8.795264	508.943300	10.273127
8.754525	504.481071	10.278144
8.823192	494.053070	10.283162
8.508465	493.695251	10.288179
8.857668	507.311310	10.293197
8.505646	509.524979	10.298215
8.774943	515.838480	10.303232
8.799300	508.762536	10.308250
8.518668	518.002398	10.313267
8.564417	509.815425	10.318285
8.601179	520.457215	10.323303
8.681061	514.739020	10.328320
8.916044	519.372715	10.333338
8.746892	519.140408	10.338355
9.041940	505.581115	10.343373
9.021006	508.522385	10.348391
8.934322	517.520422	10.353408
9.174112	507.838767	10.358426
8.748104	512.279382	10.363443
8.947204	505.548442	10.368461
9.055092	515.194484	10.373479
8.948879	499.567917	10.378496
9.076889	495.255974	10.383514
9.026277	500.281546	10.388531
8.857732	505.246703	10.393549
8.910010	509.217907	10.398567
8.798643	508.386417	10.403584
9.188474	516.826960	10.408602
8.930475	504.733393	10.413619
8.638233	515.821201	10.418637
8.821680	516.035417	10.423655
9.009132	515.718836	10.428672
9.202600	515.123603	10.433690
8.998523	512.081817	10.438707
9.029791	500.160679	10.443725
8.742542	508.742017	10.448743
8.789714	514.591709	10.453760
9.010459	510.088508	10.458778
8.885637	508.814162	10.463795
8.781309	507.154756	10.468813
9.218066	509.787632	10.473831
8.828099	517.154315	10.478848
9.223778	517.745530	10.483866
9.063595	510.471283	10.488883
8.989254	510.170473	10.493901
8.937536	516.338613	10.498919
9.046031	506.608103	10.503936
9.027766	507.844837	10.508954
9.121220	511.525570	10.513971
8.837837	503.399635	10.518989
8.900074	509.464713	10.524007
9.060310	507.164258	10.529024
9.079551	500.063872	10.534042
8.879633	506.012235	10.539059
8.841543	516.340706	10.544077
9.432726	534.308556	10.549095
9.519800	523.824006	10.554112
9.466747	510.865199	10.559130
9.356159	516.809036	10.564147
9.477686	507.941166	10.569165
9.475262	505.489473	10.574183
8.834253	508.464781	10.579200
9.172614	504.444923	10.584218
9.500468	514.817042	10.589235
9.568442	499.150560	10.594253
9.448821	493.028134	10.599271
9.165010	512.256511	10.604288
9.250133	515.291617	10.609306
9.226407	511.208570	10.614323
9.066104	515.288821	10.619341
9.124807	509.188942	10.624359
9.162430	501.438742	10.629376
9.379311	504.238609	10.634394
9.029010	511.984081	10.639411
9.057186	506.034151	10.644429
9.104000	509.179398	10.649447
9.136053	527.316897	10.654464
9.668835	528.524097	10.659482
9.501322	534.842929	10.664499
9.382150	520.771018	10.669517
9.454894	516.294161	10.674535
9.377855	510.060916	10.679552
9.204356	512.751538	10.684570
9.577531	527.578830	10.689587
9.434924	527.465439	10.694605
9.194108	519.686275	10.699623
9.053552	530.431592	10.704640
9.440622	531.999291	10.709658
9.530579	531.776879	10.714675
9.632345	545.763093	10.719693
9.708656	538.211942	10.724711
9.730851	538.666016	10.729728
9.760451	524.738048	10.734746
9.562009	519.186535	10.739763
9.485657	511.154390	10.744781
9.253629	513.579630	10.749799
9.260189	510.044098	10.754816
9.359842	518.851996	10.759834
9.305722	526.617339	10.764851
9.417288	544.082839	10.769869
9.557993	535.966182	10.774887
9.724216	536.650152	10.779904
9.654182	533.076124	10.784922
9.273503	531.056075	10.789939
9.543726	532.739911	10.794957
9.713858	531.163731	10.799975
9.176203	537.499534	10.804992
9.353163	532.949540	10.810010
9.757530	537.108579	10.815027
9.856883	538.396314	10.820045
9.506808	540.133158	10.825063
9.471534	537.989563	10.830080
9.445663	535.844495	10.835098
9.479473	548.758926	10.840115
9.296633	542.135151	10.845133
9.508452	538.176137	10.850151
9.471392	537.254108	10.855168
9.421914	546.849085	10.860186
9.620747	557.323494	10.865203
9.729260	567.004180	10.870221
10.005636	567.497324	10.875239
10.005342	573.180903	10.880256
10.076611	553.275639	10.885274
9.927811	545.674548	10.890291
9.884761	537.072289	10.895309
9.582751	532.004055	10.900327
9.498426	545.688068	10.905344
9.490986	539.592230	10.910362
9.928269	559.768019	10.915379
9.915732	568.994305	10.920397
10.228145	554.472895	10.925415
9.601138	547.391696	10.930432
9.821336	543.772192	10.935450
9.939154	541.680348	10.940467
9.976850	553.019439	10.945485
10.153518	533.242849	10.950503
9.613355	536.685195	10.955520
9.817741	535.198321	10.960538
9.889999	537.036250	10.965555
9.606454	544.190613	10.970573
10.240168	545.486141	10.975591
9.741369	556.596870	10.980608
9.904381	556.864781	10.985626
10.157640	560.211220	10.990643
9.696859	556.404922	10.995661
10.030623	547.904563	11.000679
9.811875	559.671999	11.005696
9.607874	562.673518	11.010714
10.196011	567.718950	11.015731
10.134549	566.447295	11.020749
10.272296	570.231553	11.025767
10.364366	569.630115	11.030784
10.100866	554.858115	11.035802
9.840790	543.496990	11.040819
9.751190	548.282533	11.045837
9.924589	545.086924	11.050855
10.032855	562.313120	11.055872
10.434706	562.745579	11.060890
10.089701	571.007795	11.065907
9.937325	563.934273	11.070925
10.046039	559.963007	11.075943
9.917090	566.086461	11.080960
9.951354	567.191892	11.085978
10.300886	561.778570	11.090995
9.933860	569.419390	11.096013
10.027786	567.668955	11.101031
9.966918	566.280444	11.106048
9.877662	570.163385	11.111066
10.090573	570.432945	11.116083
9.796445	575.032792	11.121101
9.997321	560.478361	11.126119
10.075363	574.682907	11.131136
10.047315	572.191039	11.136154
10.095497	567.260429	11.141171
10.052801	570.343973	11.146189
10.145015	568.600119	11.151207
10.277283	567.099296	11.156224
10.384837	589.169759	11.161242
10.108435	575.627365	11.166259
10.385201	578.973279	11.171277
10.106228	569.290821	11.176295
10.229118	583.769213	11.181312
10.039669	578.822184	11.186330
10.634938	583.497275	11.191347
10.325122	588.269995	11.196365
10.883546	582.864962	11.201383
10.452684	574.992475	11.206400
9.953992	563.662411	11.211418
10.127773	564.405158	11.216435
10.274005	577.503966	11.221453
10.742668	572.750469	11.226471
10.375330	583.364094	11.231488
10.356340	580.921298	11.236506
10.317014	582.180271	11.241523
10.403541	592.877423	11.246541
10.584086	585.221558	11.251559
10.715115	584.705534	11.256576
10.636740	573.877650	11.261594
10.701986	563.882487	11.266611
10.301504	567.056802	11.271629
10.360198	562.471683	11.276647
10.439676	562.478129	11.281664
10.302387	563.055021	11.286682
10.301241	565.314706	11.291699
10.495339	578.636387	11.296717
10.542436	581.431311	11.301735
10.732196	582.483978	11.306752
10.861768	582.103881	11.311770
10.869656	572.493239	11.316787
10.672715	565.433011	11.321805
10.520989	561.117544	11.326823
10.362325	565.550998	11.331840
10.045908	564.079451	11.336858
10.562183	557.702736	11.341875
10.534001	579.412604	11.346893
10.728914	577.214004	11.351911
10.560431	584.830034	11.356928
10.625681	583.800455	11.361946
10.789112	586.438297	11.366963
10.725587	594.208299	11.371981
10.628374	592.206945	11.376999
10.599812	585.401193	11.382016
10.692773	593.490657	11.387034
10.962049	584.037869	11.392051
10.854313	586.841274	11.397069
10.910318	584.001721	11.402087
10.686145	570.713078	11.407104
10.454301	565.715890	11.412122
11.066658	570.195798	11.417139
10.416212	574.725241	11.422157
10.650882	574.432818	11.427175
10.716628	582.242521	11.432192
10.497524	573.134500	11.437210
10.754003	576.666629	11.442227
10.813740	590.511141	11.447245
10.709187	588.659259	11.452263
10.800920	593.646776	11.457280
10.535394	590.191728	11.462298
10.827045	585.355509	11.467315
10.741080	586.931058	11.472333
10.895902	587.765138	11.477351
10.634198	589.062110	11.482368
10.473172	588.386718	11.487386
10.664069	578.406574	11.492403
10.669972	590.716342	11.497421
10.535500	595.701431	11.502439
10.945578	608.960893	11.507456
10.874533	610.186968	11.512474
11.351872	609.881770	11.517491
11.139834	611.644330	11.522509
11.311158	601.701954	11.527527
10.997426	592.933796	11.532544
10.895157	589.718255	11.537562
11.300085	585.710040	11.542579
11.090958	585.496618	11.547597
11.072137	579.724440	11.552615
11.167025	577.762417	11.557632
10.864514	586.087408	11.562650
10.861507	577.109629	11.567667
10.776530	590.812714	11.572685
10.744082	580.665592	11.577703
10.658359	596.076079	11.582720
10.738677	610.002587	11.587738
11.326902	612.955727	11.592755
11.077610	617.422328	11.597773
10.909199	615.703525	11.602791
11.029226	617.956855	11.607808
11.084092	618.036584	11.612826
11.104132	609.979825	11.617843
11.122172	614.470811	11.622861
11.273239	608.498437	11.627879
11.221274	609.604758	11.632896
10.836542	614.613285	11.637914
11.296830	620.843251	11.642931
10.921417	611.488303	11.647949
11.445250	616.925674	11.652967
11.496495	617.195319	11.657984
11.249443	617.394937	11.663002
11.289048	612.948494	11.668019
11.035882	616.828725	11.673037
11.039227	613.098017	11.678055
11.367200	607.422972	11.683072
11.181796	621.097635	11.688090
11.610518	610.319664	11.693107
11.400067	613.394785	11.698125
11.446806	612.418598	11.703143
11.036078	613.855685	11.708160
11.081646	610.519148	11.713178
11.018888	610.771941	11.718195
11.107081	621.771805	11.723213
11.307699	631.886218	11.728231
11.614104	633.018442	11.733248
11.728512	644.373974	11.738266
11.634525	627.798640	11.743283
11.298395	622.581091	11.748301
11.278673	614.123462	11.753319
11.417152	614.521450	11.758336
11.238069	633.077143	11.763354
11.570266	631.349330	11.768371
11.904554	622.236630	11.773389
11.318870	610.071258	11.778407
11.563812	610.181166	11.783424
11.229238	613.603938	11.788442
11.458378	620.100493	11.793459
11.589357	627.805320	11.798477
11.535204	635.636987	11.803495
11.719834	640.329096	11.808512
11.508011	639.737401	11.813530
11.861116	633.379913	11.818547
11.784292	621.586084	11.823565
11.360440	613.794531	11.828583
11.366281	613.620011	11.833600
11.861470	618.007836	11.838618
12.016998	613.587412	11.843635
11.730852	604.139586	11.848653
11.451576	592.279667	11.853671
11.653954	601.437583	11.858688
11.607815	602.217944	11.863706
11.564165	602.720207	11.868723
11.704787	607.381332	11.873741
11.695224	627.971192	11.878759
11.932805	622.714247	11.883776
11.361827	627.938150	11.888794
11.618008	619.673975	11.893811
11.617442	629.535886	11.898829
11.590358	627.252142	11.903847
11.817299	629.599174	11.908864
11.672994	629.246208	11.913882
11.837982	626.421131	11.918899
11.691818	625.939069	11.923917
11.574488	628.482053	11.928935
11.794607	631.865255	11.933952
11.671148	627.646329	11.938970
11.643272	623.314598	11.943987
11.923260	631.548345	11.949005
11.474353	637.964951	11.954023
11.707202	639.607316	11.959040
11.548694	631.117776	11.964058
11.795577	638.671905	11.969075
12.210643	660.552264	11.974093
11.829039	644.769903	11.979111
12.221326	644.462250	11.984128
12.180854	647.797923	11.989146
11.589664	633.607375	11.994163
11.982106	636.622752	11.999181
11.876233	644.033338	12.004199
12.020567	644.263152	12.009216
12.347120	646.774460	12.014234
11.839274	635.363734	12.019251
11.917787	647.346584	12.024269
12.042335	657.441372	12.029287
12.242630	657.731845	12.034304
11.855998	650.508800	12.039322
12.005964	652.511291	12.044339
12.059445	652.581770	12.049357
11.828964	664.089182	12.054375
12.137445	660.430576	12.059392
12.062668	664.203971	12.064410
12.127444	654.079444	12.069427
12.409398	663.726696	12.074445
12.062007	659.871051	12.079463
12.171822	658.402141	12.084480
12.198921	663.153651	12.089498
12.454739	661.601905	12.094515
12.392496	651.632980	12.099533
11.927367	653.305811	12.104551
12.541509	651.663209	12.109568
12.169136	659.730938	12.114586
12.171704	651.569600	12.119603
12.368715	654.580887	12.124621
12.323737	654.748844	12.129639
12.436410	655.684206	12.134656
12.209925	657.060871	12.139674
12.177553	646.333032	12.144691
12.827875	660.163960	12.149709
12.080046	637.833895	12.154727
12.359484	632.851254	12.159744
12.000058	631.481113	12.164762
12.086164	644.305369	12.169779
12.557678	647.750172	12.174797
12.267365	650.481207	12.179815
12.507189	649.073978	12.184832
12.699083	646.292020	12.189850
12.590922	651.225665	12.194867
12.627293	642.563575	12.199885
12.279459	644.293766	12.204903
12.487675	646.053600	12.209920
12.312167	645.276334	12.214938
12.222627	651.220074	12.219955
12.632105	644.743297	12.224973
12.292379	660.603891	12.229991
12.599743	653.196370	12.235008
12.360377	652.126152	12.240026
12.537969	653.799267	12.245043
12.519526	653.253011	12.250061
12.574707	650.353617	12.255079
12.496841	651.542894	12.260096
12.745316	665.746056	12.265114
12.235013	648.345995	12.270131
12.499963	649.901281	12.275149
12.677922	657.466217	12.280167
12.680570	655.556507	12.285184
12.291970	652.695086	12.290202
12.416170	656.008115	12.295219
12.841706	650.967865	12.300237
12.524627	660.002073	12.305255
12.460889	653.451114	12.310272
12.521609	656.354368	12.315290
12.316565	653.956492	12.320307
12.192489	659.520638	12.325325
12.396165	669.716644	12.330343
12.992314	668.799538	12.335360
12.820060	672.840672	12.340378
12.914504	677.966643	12.345395
13.149057	677.273450	12.350413
12.930975	680.005796	12.355431
13.037674	666.390685	12.360448
12.495940	669.325218	12.365466
12.554115	670.695153	12.370483
12.799632	673.077150	12.375501
12.816796	691.075136	12.380519
12.684957	675.619688	12.385536
12.892088	678.907105	12.390554
12.940785	680.212253	12.395571
12.923849	681.568711	12.400589
12.589789	681.608393	12.405607
12.904035	680.527172	12.410624
12.854473	681.955014	12.415642
12.956844	686.398091	12.420659
13.037601	679.789769	12.425677
12.715803	683.513510	12.430695
12.741398	684.648709	12.435712
13.110818	679.860240	12.440730
12.868990	681.788421	12.445747
13.257080	680.903914	12.450765
12.990616	686.370457	12.455783
13.203843	680.886937	12.460800
13.344371	676.976931	12.465818
12.808772	682.170061	12.470835
12.780457	680.211551	12.475853
12.629350	680.853728	12.480871
12.669912	681.973959	12.485888
13.483950	675.045620	12.490906
13.284685	680.536347	12.495923
12.945847	672.393777	12.500941
13.221307	681.780124	12.505959
13.212265	683.804376	12.510976
13.232104	679.140108	12.515994
13.186380	684.218614	12.521011
13.636140	675.826253	12.526029
13.468993	686.105615	12.531047
13.222858	682.328775	12.536064
13.572644	675.350100	12.541082
13.360528	671.492192	12.546099
13.539399	669.113057	12.551117
12.998845	672.463972	12.556135
12.991290	664.673443	12.561152
13.491458	667.233291	12.566170
13.282685	672.290003	12.571187
13.520682	670.908306	12.576205
13.568510	670.105514	12.581223
13.546277	667.950392	12.586240
13.411747	667.065719	12.591258
13.220137	672.845577	12.596275
13.402019	673.205208	12.601293
13.062019	674.438713	12.606311
13.254280	676.052728	12.611328
13.579391	670.125647	12.616346
13.126086	672.935872	12.621363
13.202438	666.160988	12.626381
12.913838	675.294883	12.631399
13.265489	681.895341	12.636416
13.493487	682.771610	12.641434
13.500806	692.250468	12.646451
13.599155	694.267362	12.651469
13.680244	690.628599	12.656487
13.636391	690.468176	12.661504
14.092408	689.437326	12.666522
13.577454	694.583043	12.671539
14.024160	691.445573	12.676557
13.508115	672.061386	12.681575
13.328135	669.113627	12.686592
13.729890	676.589858	12.691610
13.571347	686.972014	12.696627
13.901825	682.921794	12.701645
13.695770	681.688564	12.706663
13.709855	666.308091	12.711680
13.777833	668.588516	12.716698
13.747401	675.779012	12.721715
13.425130	663.777459	12.726733
13.461332	675.328300	12.731751
13.534603	691.171550	12.736768
13.764457	688.765489	12.741786
13.714061	691.004505	12.746803
13.602923	693.985184	12.751821
13.757865	701.850391	12.756839
13.769140	699.144061	12.761856
13.763470	696.560307	12.766874
13.694656	693.535166	12.771891
13.640851	689.128587	12.776909
13.758717	689.084837	12.781927
13.940628	690.242882	12.786944
14.044668	692.845865	12.791962
13.472888	691.325954	12.796979
13.664842	687.571991	12.801997
13.926770	702.012915	12.807015
13.552684	704.952745	12.812032
13.925174	694.454934	12.817050
13.940379	693.931807	12.822067
13.935037	691.546818	12.827085
13.619739	695.944885	12.832103
13.726506	711.899669	12.837120
14.307372	711.852804	12.842138
14.208451	721.812228	12.847155
14.583907	710.512367	12.852173
14.331488	696.647386	12.857191
13.915530	696.138165	12.862208
14.389919	680.376290	12.867226
14.374081	690.862322	12.872243
14.016063	686.241475	12.877261
13.942499	686.947242	12.882279
14.027505	693.639976	12.887296
14.155658	686.910617	12.892314
14.339179	687.629753	12.897331
14.228971	684.472243	12.902349
14.115474	685.758624	12.907367
14.113389	689.896176	12.912384
14.267978	689.707817	12.917402
13.949151	692.187706	12.922419
13.997699	681.611270	12.927437
14.195390	703.140732	12.932455
14.261907	708.984300	12.937472
14.487712	711.684972	12.942490
14.253008	704.491750	12.947507
14.297395	702.023228	12.952525
14.615115	706.820734	12.957543
14.319287	698.349521	12.962560
14.208955	683.689115	12.967578
14.364426	690.071006	12.972595
14.641751	703.212483	12.977613
14.696085	689.397275	12.982631
14.322670	694.839553	12.987648
14.481469	688.155884	12.992666
14.249884	686.904564	12.997683
14.429673	684.613646	13.002701
14.331833	684.291268	13.007719
14.308391	714.899932	13.012736
14.974917	700.398661	13.017754
14.882337	697.462450	13.022771
14.450021	692.051668	13.027789
14.726398	687.855288	13.032807
14.129336	699.069864	13.037824
14.401744	694.261877	13.042842
14.303668	699.111905	13.047859
14.817303	704.449916	13.052877
14.771777	713.618329	13.057895
14.524572	705.780123	13.062912
14.708603	700.563103	13.067930
14.488920	708.206143	13.072947
14.673822	709.152281	13.077965
14.906274	707.963954	13.082983
14.681893	712.606557	13.088000
14.315229	693.006438	13.093018
14.649122	704.782056	13.098035
14.967537	709.901346	13.103053
15.082184	713.730280	13.108071
14.624798	709.734068	13.113088
14.630649	696.503965	13.118106
14.859239	703.038506	13.123123
14.806101	714.395087	13.128141
14.746986	709.282433	13.133159
14.957976	716.611845	13.138176
15.174107	711.522337	13.143194
14.713809	699.886368	13.148211
14.730169	696.197785	13.153229
14.889166	706.000025	13.158247
14.564337	707.019717	13.163264
14.868841	705.766452	13.168282
14.904555	704.615261	13.173299
14.987546	704.226681	13.178317
14.741576	706.739338	13.183335
14.539504	706.300747	13.188352
14.787177	708.007068	13.193370
14.736232	707.926651	13.198387
14.788531	708.653725	13.203405
14.656653	707.591909	13.208423
14.580222	712.321784	13.213440
14.882362	719.643227	13.218458
15.099631	725.955488	13.223475
14.871672	737.323695	13.228493
15.077255	728.754972	13.233511
14.851275	723.984039	13.238528
15.378589	732.100186	13.243546
15.066433	726.364453	13.248563
15.415517	735.755072	13.253581
15.486658	725.941933	13.258599
15.464531	744.517332	13.263616
15.577640	714.879108	13.268634
15.181450	706.029140	13.273651
15.128426	705.403094	13.278669
15.064826	696.652499	13.283687
14.889223	699.479178	13.288704
15.445400	711.630228	13.293722
15.394985	723.952067	13.298739
15.055605	723.938933	13.303757
15.379079	723.642061	13.308775
15.417683	722.695545	13.313792
15.235291	725.210866	13.318810
15.226580	719.945144	13.323827
15.273536	723.453326	13.328845
15.550623	726.174368	13.333863
15.458377	722.354473	13.338880
15.317978	724.869526	13.343898
15.578510	725.652337	13.348915
15.852234	728.474892	13.353933
15.693653	720.550211	13.358951
15.375433	712.836738	13.363968
15.272856	698.692658	13.368986
15.509862	726.650682	13.374003
15.465646	725.079667	13.379021
15.840654	720.236664	13.384039
15.481537	714.388371	13.389056
15.399527	707.407909	13.394074
15.603760	707.735636	13.399091
15.568357	722.090619	13.404109
15.566737	728.503448	13.409127
15.276823	730.000510	13.414144
15.191437	734.258422	13.419162
15.999344	732.777959	13.424179
15.529997	736.669995	13.429197
15.812018	720.761499	13.434215
15.588121	737.042670	13.439232
15.982359	743.535493	13.444250
15.978401	734.321097	13.449267
15.662186	728.153652	13.454285
15.958873	729.502001	13.459303
15.669416	730.083805	13.464320
15.851613	720.628810	13.469338
15.954063	731.544458	13.474355
15.506924	725.214490	13.479373
15.814844	729.742138	13.484391
15.636772	731.950670	13.489408
15.846661	723.744192	13.494426
15.629353	719.795569	13.499443
15.811612	720.047844	13.504461
15.964116	718.689005	13.509479
15.977223	724.925956	13.514496
15.826972	720.644934	13.519514
15.633774	718.481879	13.524531
15.450873	722.868676	13.529549
15.689306	716.986719	13.534567
15.636349	727.339732	13.539584
15.766982	733.605609	13.544602
16.139272	739.757886	13.549619
15.872986	743.791678	13.554637
15.846597	743.322405	13.559655
15.733439	745.422937	13.564672
15.656256	744.390419	13.569690
15.783787	748.952646	13.574707
15.914513	750.544751	13.579725
15.907536	743.950151	13.584743
16.018623	746.353221	13.589760
15.860250	744.424549	13.594778
16.083322	745.970626	13.599795
16.000758	761.469123	13.604813
16.537030	759.368496	13.609831
16.584376	761.667945	13.614848
16.287864	752.849673	13.619866
16.301622	747.526774	13.624883
16.031920	739.158745	13.629901
16.449083	740.194728	13.634919
16.291171	738.625746	13.639936
16.312982	743.696844	13.644954
16.221334	738.040167	13.649971
16.387637	751.827082	13.654989
16.722713	749.701175	13.660007
16.293173	749.203548	13.665024
16.152299	744.760103	13.670042
16.789509	746.803029	13.675059
16.576461	755.060432	13.680077
16.335663	743.380577	13.685095
16.321284	738.125205	13.690112
16.382608	741.533309	13.695130
16.689015	742.892758	13.700147
16.440859	751.054675	13.705165
16.642497	737.983214	13.710183
16.549446	738.764621	13.715200
16.424362	743.988123	13.720218
16.627372	736.719994	13.725235
16.162581	755.219593	13.730253
16.841311	754.791320	13.735271
17.008446	763.923284	13.740288
16.639225	757.975574	13.745306
16.562143	744.130421	13.750323
16.404394	751.637543	13.755341
17.083895	749.669110	13.760359
16.951919	747.303955	13.765376
16.803429	739.712200	13.770394
16.695271	735.446670	13.775411
16.481354	739.671072	13.780429
16.666444	739.607322	13.785447
16.544788	745.451983	13.790464
16.603405	758.122837	13.795482
16.878329	751.067499	13.800499
16.889656	755.736298	13.805517
16.800251	758.628376	13.810535
17.119989	758.972721	13.815552
16.798167	754.611274	13.820570
16.969650	759.747289	13.825587
16.787103	757.011357	13.830605
17.026429	749.775404	13.835623
17.042368	755.690028	13.840640
16.928381	755.815149	13.845658
17.193658	749.250475	13.850675
16.833105	740.284452	13.855693
17.050199	737.760463	13.860711
17.069777	741.954594	13.865728
17.036348	742.530999	13.870746
17.186639	740.897949	13.875763
16.645394	736.204811	13.880781
16.895782	748.517407	13.885799
17.035062	752.664383	13.890816
17.063983	754.843642	13.895834
17.327084	748.569644	13.900851
17.120725	760.972746	13.905869
17.235120	763.384767	13.910887
17.256112	762.829174	13.915904
16.821938	761.978821	13.920922
17.433752	749.635196	13.925939
17.226966	765.885310	13.930957
17.159356	761.304150	13.935975
17.270176	745.009043	13.940992
17.355018	760.367701	13.946010
17.245948	742.750047	13.951027
17.044939	758.557435	13.956045
17.069830	760.248174	13.961063
17.804278	753.322809	13.966080
17.163416	758.084326	13.971098
17.097284	750.549091	13.976115
17.035671	753.850226	13.981133
16.833419	756.330794	13.986151
17.054960	753.247527	13.991168
17.119876	771.269670	13.996186
17.551419	776.462774	14.001203
17.341805	778.493216	14.006221
17.596403	779.393724	14.011239
17.803630	782.075227	14.016256
17.471516	788.890156	14.021274
17.617681	776.704678	14.026291
17.507410	779.868274	14.031309
17.558203	790.022030	14.036327
17.498280	777.332351	14.041344
17.659821	781.412730	14.046362
17.639573	766.738141	14.051379
17.679517	777.644676	14.056397
17.517640	767.975320	14.061415
18.095301	771.154206	14.066432
17.424236	780.114548	14.071450
17.721978	782.778713	14.076467
17.926502	782.528881	14.081485
17.659146	777.369939	14.086503
18.092197	776.771874	14.091520
17.661540	791.750578	14.096538
17.807066	771.868149	14.101555
17.462930	784.775695	14.106573
17.254064	785.950792	14.111591
17.570626	773.628164	14.116608
17.693899	786.068000	14.121626
17.887525	782.184367	14.126643
17.634974	781.182479	14.131661
17.466922	778.520013	14.136679
18.094892	780.671688	14.141696
17.979211	793.373032	14.146714
17.725422	780.101495	14.151731
18.091394	790.133286	14.156749
17.757782	794.389078	14.161767
18.463700	797.513160	14.166784
18.102275	789.645476	14.171802
18.153396	785.250835	14.176819
18.163985	777.504752	14.181837
18.074146	776.347982	14.186855
18.265514	772.278511	14.191872
17.939776	786.429725	14.196890
17.982149	771.107845	14.201907
18.121174	769.142041	14.206925
17.967069	779.618231	14.211943
18.393489	791.426746	14.216960
18.550842	797.259267	14.221978
18.208639	776.165674	14.226995
17.985728	777.431334	14.232013
17.934937	784.091730	14.237031
18.343894	794.069450	14.242048
18.365149	801.961959	14.247066
18.617821	797.103389	14.252083
18.380624	799.797722	14.257101
17.982309	794.545684	14.262119
18.320994	798.459455	14.267136
18.145433	799.272726	14.272154
18.649085	800.020605	14.277171
18.746139	797.367092	14.282189
18.524606	801.005719	14.287207
18.863029	791.554611	14.292224
18.508517	778.194715	14.297242
18.510700	779.137928	14.302259
18.368803	772.248875	14.307277
18.026289	785.758930	14.312295
18.481123	783.910902	14.317312
18.304620	788.104207	14.322330
18.379953	791.065154	14.327347
18.564497	798.935234	14.332365
18.688867	800.847077	14.337383
18.815232	798.984240	14.342400
18.722812	804.486666	14.347418
18.868958	791.272381	14.352435
18.559552	799.472319	14.357453
18.340310	808.573324	14.362471
18.790369	796.400178	14.367488
18.907212	796.056785	14.372506
18.893798	807.678603	14.377523
18.991281	802.885372	14.382541
18.650149	798.028319	14.387559
18.917813	799.087728	14.392576
18.729118	799.240334	14.397594
18.720968	805.035672	14.402611
19.135181	797.024367	14.407629
18.983380	802.463513	14.412647
19.036607	805.825560	14.417664
18.978224	808.435073	14.422682
19.126144	798.938069	14.427699
19.209931	793.326472	14.432717
18.995186	805.188117	14.437735
19.442278	792.968101	14.442752
19.290054	783.224641	14.447770
18.677536	778.732008	14.452787
18.895294	781.509691	14.457805
18.928118	794.048912	14.462823
18.942405	790.445842	14.467840
19.127441	797.119786	14.472858
18.798968	794.940047	14.477875
19.033655	790.788045	14.482893
18.752281	797.847493	14.487911
19.179637	797.742629	14.492928
18.946841	800.183806	14.497946
19.044070	796.753933	14.502963
18.892012	797.790742	14.507981
18.868045	797.179075	14.512999
19.474360	797.342819	14.518016
19.100657	798.641574	14.523034
19.322500	805.644272	14.528051
19.333849	812.619993	14.533069
19.435666	820.316850	14.538087
19.339562	800.702623	14.543104
19.429686	804.428120	14.548122
19.016571	802.271109	14.553139
19.245673	815.486497	14.558157
19.550798	825.616204	14.563175
19.469974	819.465496	14.568192
19.541376	819.817193	14.573210
19.610489	818.550308	14.578227
20.086258	821.644182	14.583245
19.726845	816.370263	14.588263
19.527419	805.712684	14.593280
19.045442	803.219321	14.598298
19.378638	819.397503	14.603315
19.631804	816.116764	14.608333
19.676898	825.485632	14.613351
19.751016	821.901584	14.618368
19.803468	825.746598	14.623386
19.463184	826.882328	14.628403
19.811083	826.051449	14.633421
19.859934	822.566034	14.638439
19.669553	825.019504	14.643456
19.814019	820.509243	14.648474
19.710016	822.033989	14.653491
19.981764	824.547598	14.658509
19.519045	826.491468	14.663527
19.583811	820.239052	14.668544
19.679696	816.077233	14.673562
19.581564	820.393968	14.678579
19.686592	822.523440	14.683597
19.432918	826.113459	14.688615
19.817503	816.238536	14.693632
19.736660	823.377029	14.698650
19.486351	821.945595	14.703667
19.597280	831.080087	14.708685
20.027539	842.913282	14.713703
19.706902	829.759481	14.718720
20.084416	840.654190	14.723738
19.834520	848.440879	14.728755
20.338867	844.388627	14.733773
19.898782	851.286769	14.738791
20.058880	840.089996	14.743808
20.435349	847.090575	14.748826
20.246541	843.831742	14.753843
20.560405	832.853882	14.758861
20.595253	848.826369	14.763879
20.516187	842.362949	14.768896
20.307950	840.565157	14.773914
20.217765	848.004927	14.778931
20.409962	836.938829	14.783949
20.348795	841.697905	14.788967
20.533017	832.050028	14.793984
20.506198	825.385923	14.799002
20.092345	824.059008	14.804019
20.352128	831.907846	14.809037
20.103887	834.676499	14.814055
20.387615	833.319182	14.819072
20.308836	833.549242	14.824090
20.024209	838.349640	14.829107
20.445064	829.668244	14.834125
20.184919	841.925194	14.839143
20.317852	831.628939	14.844160
20.357077	836.280765	14.849178
20.115227	839.304040	14.854195
20.461507	841.925895	14.859213
20.521918	833.057972	14.864231
20.274755	838.370057	14.869248
20.355260	850.223342	14.874266
20.939497	864.632835	14.879283
20.857179	852.921765	14.884301
20.914513	863.030356	14.889319
21.171594	845.083830	14.894336
20.896278	834.251931	14.899354
20.589592	826.959482	14.904371
20.632669	833.526293	14.909389
20.574053	838.310215	14.914407
20.705473	832.110469	14.919424
20.713836	842.065774	14.924442
20.605126	853.645748	14.929459
20.963161	857.338748	14.934477
20.854117	859.539636	14.939495
20.662127	859.440291	14.944512
20.853289	858.138502	14.949530
20.812583	863.863220	14.954547
20.998250	850.469128	14.959565
21.272627	860.764621	14.964583
21.201005	856.512272	14.969600
21.276991	851.116475	14.974618
21.179240	864.285279	14.979635
21.049812	854.039586	14.984653
21.211969	855.825593	14.989671
21.196407	856.355020	14.994688
21.067237	858.417048	14.999706
21.247247	861.254308	15.004723
21.687093	849.003831	15.009741
21.244970	841.379144	15.014759
21.086292	830.434296	15.019776
20.979793	828.828849	15.024794
21.232451	839.604263	15.029811
21.388883	849.205010	15.034829
21.483940	859.525442	15.039847
21.257428	858.367990	15.044864
21.475063	847.506184	15.049882
21.175495	848.203186	15.054899
21.413786	849.030513	15.059917
21.368835	863.030496	15.064935
21.481795	858.275851	15.069952
21.660295	853.447821	15.074970
21.174164	859.251794	15.079987
21.366495	848.132018	15.085005
21.352368	854.767760	15.090023
21.180380	850.780449	15.095040
21.134070	846.555695	15.100058
21.222211	856.388054	15.105075
21.599867	845.845163	15.110093
21.311310	857.005189	15.115111
21.232822	859.857703	15.120128
21.410760	860.214800	15.125146
21.669942	875.255905	15.130163
21.515278	873.591727	15.135181
21.610079	883.782824	15.140199
21.615696	877.432357	15.145216
21.860369	874.045641	15.150234
21.603630	875.423906	15.155251
21.868327	879.863690	15.160269
22.298928	877.344100	15.165287
21.703503	867.711060	15.170304
21.980698	874.509451	15.175322
21.881358	878.460311	15.180339
21.951030	880.352330	15.185357
22.165206	877.263884	15.190375
22.144718	876.531748	15.195392
22.029959	876.271978	15.200410
21.904646	869.121510	15.205427
22.042414	867.537749	15.210445
21.907568	867.060218	15.215463
21.592340	870.224384	15.220480
21.921136	872.344049	15.225498
21.791428	879.540715	15.230515
21.946399	880.523111	15.235533
21.842273	867.972838	15.240551
21.840672	879.905280	15.245568
22.295117	870.732601	15.250586
22.174219	871.849739	15.255603
21.982271	875.723589	15.260621
22.388191	876.404732	15.265639
21.947505	877.227988	15.270656
21.949752	876.975133	15.275674
21.926593	895.904305	15.280691
22.149016	897.482056	15.285709
22.281554	898.878227	15.290727
21.954690	896.461535	15.295744
22.662797	891.818763	15.300762
22.496268	910.038258	15.305779
22.559474	896.650695	15.310797
22.450777	897.942650	15.315815
22.556787	895.120460	15.320832
22.685145	892.910159	15.325850
22.555966	914.008246	15.330867
22.619733	898.641878	15.335885
22.723724	896.653147	15.340903
22.553886	905.459278	15.345920
22.567650	902.048774	15.350938
22.531293	902.707694	15.355955
22.739378	901.759861	15.360973
22.775641	895.881119	15.365991
22.526365	900.070073	15.371008
23.184397	895.775977	15.376026
22.525456	897.334027	15.381043
22.588727	894.288157	15.386061
22.936388	889.670301	15.391079
22.638262	895.173427	15.396096
22.943417	898.843163	15.401114
23.093721	906.384135	15.406131
22.996689	904.221769	15.411149
22.907567	890.514091	15.416167
22.892698	897.992576	15.421184
22.845267	900.496243	15.426202
22.851994	898.121959	15.431219
22.895712	898.919813	15.436237
23.076406	901.034284	15.441255
22.705121	900.899914	15.446272
22.845675	895.241520	15.451290
23.128420	896.285949	15.456307
23.206275	897.412975	15.461325
23.109040	896.298381	15.466343
22.791188	894.874368	15.471360
22.980786	895.210703	15.476378
23.023455	903.021006	15.481395
22.840980	901.197080	15.486413
23.211691	909.893274	15.491431
23.233489	918.625204	15.496448
23.650003	916.931492	15.501466
23.262660	925.402478	15.506483
23.552630	920.762096	15.511501
23.534382	901.870871	15.516519
23.317568	898.625884	15.521536
23.391485	892.239464	15.526554
23.127232	898.813425	15.531571
23.249933	904.711372	15.536589
23.353272	904.452145	15.541607
23.653996	915.917516	15.546624
23.678858	914.247297	15.551642
23.172419	905.730087	15.556659
23.587880	911.913530	15.561677
23.519404	909.913949	15.566695
23.649993	918.417393	15.571712
23.585972	910.288461	15.576730
23.341928	919.825758	15.581747
23.710359	918.123801	15.586765
23.586199	912.513188	15.591783
23.520538	914.931350	15.596800
23.558738	911.589600	15.601818
23.623296	909.603890	15.606835
23.118218	908.622625	15.611853
23.373949	907.276001	15.616871
23.556587	922.171346	15.621888
23.984349	933.888227	15.626906
23.902947	937.224055	15.631923
23.732788	934.063271	15.636941
24.198884	928.953472	15.641959
23.913568	947.942709	15.646976
24.010257	928.926149	15.651994
23.834427	928.985220	15.657011
23.979557	930.420447	15.662029
24.296279	927.416913	15.667047
24.135111	926.788868	15.672064
24.144106	934.841150	15.677082
24.317109	937.805753	15.682099
24.113334	935.836836	15.687117
24.233842	925.605591	15.692135
23.865903	934.161904	15.697152
24.180394	927.497935	15.702170
24.203749	927.560512	15.707187
24.127175	936.415163	15.712205
24.509927	927.660793	15.717223
24.584464	934.569856	15.722240
24.094652	930.193660	15.727258
24.360837	927.175953	15.732275
24.201702	930.602855	15.737293
24.476057	927.274595	15.742311
24.704253	937.400640	15.747328
24.549081	924.353389	15.752346
24.632031	921.702068	15.757363
24.462882	926.137253	15.762381
24.844962	926.421341	15.767399
24.229534	920.875074	15.772416
24.476870	921.786195	15.777434
24.471913	932.949172	15.782451
24.335431	925.907730	15.787469
24.591139	928.240828	15.792487
24.749222	932.836186	15.797504
24.567526	933.085528	15.802522
24.788955	934.732866	15.807539
24.431875	935.249531	15.812557
24.944364	924.767521	15.817575
24.691214	937.342181	15.822592
24.650776	932.482160	15.827610
24.787008	935.471460	15.832627
24.633571	933.059148	15.837645
25.046400	925.063783	15.842663
24.640203	940.887701	15.847680
24.388137	925.861133	15.852698
24.549545	927.438979	15.857715
24.749517	933.959154	15.862733
25.050147	940.700249	15.867751
25.012926	953.985870	15.872768
25.193357	945.304217	15.877786
25.108510	927.745702	15.882803
24.949439	941.088274	15.887821
25.427866	946.160473	15.892839
25.050125	932.428554	15.897856
24.813988	929.568446	15.902874
25.028122	939.393734	15.907891
25.179264	951.034045	15.912909
25.175469	950.255107	15.917927
25.048073	955.602111	15.922944
25.209141	949.741668	15.927962
25.340034	954.218213	15.932979
24.798527	953.422537	15.937997
25.117036	948.342168	15.943015
25.354304	947.380293	15.948032
25.072199	957.592615	15.953050
25.352464	948.002212	15.958067
25.260398	947.659989	15.963085
25.542836	951.036645	15.968103
25.444694	952.159690	15.973120
25.163480	951.187530	15.978138
25.371294	964.892366	15.983155
25.522365	971.757893	15.988173
25.517698	973.364919	15.993191
25.831906	973.684888	15.998208
25.665135	978.062909	16.003226
25.824976	959.695995	16.008243
25.845759	974.733510	16.013261
25.684883	969.030801	16.018279
25.664605	977.068752	16.023296
25.671198	972.611614	16.028314
25.780306	969.795238	16.033331
25.766792	976.058539	16.038349
25.697475	972.749402	16.043367
25.888390	977.080848	16.048384
25.938231	971.831124	16.053402
25.995047	966.738103	16.058419
25.837891	967.273938	16.063437
26.064900	959.045736	16.068455
25.988750	963.845062	16.073472
26.213665	961.089440	16.078490
26.217148	959.005994	16.083507
25.973130	961.433172	16.088525
26.601682	953.501826	16.093543
25.910419	961.335627	16.098560
26.291061	955.525986	16.103578
26.346940	961.494382	16.108595
26.244448	970.248968	16.113613
26.401115	967.207387	16.118631
26.066970	960.531422	16.123648
26.123342	964.659879	16.128666
26.426065	959.739773	16.133683
26.011507	958.299347	16.138701
25.875162	960.599201	16.143719
25.929214	962.528390	16.148736
26.105869	969.948495	16.153754
26.471250	966.877369	16.158771
26.031249	974.646561	16.163789
26.445957	972.943659	16.168807
26.514030	988.081075	16.173824
26.524801	985.740860	16.178842
26.684449	982.080262	16.183859
26.343056	981.777103	16.188877
26.717772	983.545598	16.193895
26.392805	987.364573	16.198912
26.667586	988.318736	16.203930
26.962235	981.809336	16.208947
26.600762	983.623749	16.213965
26.701016	984.835634	16.218983
26.742135	979.079182	16.224000
26.451847	985.136538	16.229018
26.746674	986.819719	16.234035
26.641659	977.750421	16.239053
26.527531	985.411754	16.244071
26.545511	985.112251	16.249088
26.862549	987.041265	16.254106
26.917100	976.646753	16.259123
26.761259	983.954854	16.264141
26.889976	975.473796	16.269159
27.018387	978.079314	16.274176
26.994092	983.037781	16.279194
27.069314	981.738369	16.284211
26.606782	1000.799610	16.289229
26.947127	1006.341592	16.294247
27.147656	1007.903848	16.299264
26.920668	1006.831669	16.304282
27.079101	1007.311748	16.309299
27.030524	1005.905496	16.314317
27.420038	1002.445568	16.319335
27.281169	1003.379334	16.324352
27.490473	1009.834958	16.329370
27.448745	1007.127417	16.334387
27.507606	1017.393651	16.339405
27.609741	1007.793255	16.344423
27.597758	1008.429424	16.349440
27.217476	1010.243630	16.354458
27.615876	1002.692312	16.359475
27.120372	1014.386642	16.364493
27.179879	1009.040717	16.369511
27.638373	998.207356	16.374528
27.356901	1010.780193	16.379546
27.652068	1002.383498	16.384563
27.732318	1006.631303	16.389581
27.266531	1003.987048	16.394599
27.771828	1005.555203	16.399616
27.776158	1010.326153	16.404634
27.829014	1011.870520	16.409651
27.528252	1010.661573	16.414669
27.812135	1013.078633	16.419687
28.170947	1017.380626	16.424704
27.528949	1017.717868	16.429722
27.902920	1025.470004	16.434739
28.104756	1029.124397	16.439757
28.020968	1028.679888	16.444775
28.155578	1025.300920	16.449792
27.825284	1019.678388	16.454810
28.015720	1021.766100	16.459827
28.171371	1022.896723	16.464845
28.030724	1019.049633	16.469863
27.922082	1020.439420	16.474880
27.880791	1028.398635	16.479898
28.369442	1026.715702	16.484915
28.065064	1022.692289	16.489933
27.792031	1025.865650	16.494951
28.210671	1025.282460	16.499968
28.188802	1030.518276	16.504986
28.038531	1017.066239	16.510003
27.955513	1029.188265	16.515021
28.299079	1035.130547	16.520039
28.376209	1027.667425	16.525056
28.235168	1026.531284	16.530074
28.322276	1019.628346	16.535091
28.440677	1020.670129	16.540109
28.174973	1032.053906	16.545127
28.441794	1037.818861	16.550144
28.498471	1049.246814	16.555162
28.616863	1035.560161	16.560179
28.726277	1046.238220	16.565197
28.691361	1049.569941	16.570215
28.664763	1035.410533	16.575232
28.564411	1045.865833	16.580250
28.929346	1034.078257	16.585267
28.916510	1045.185733	16.590285
28.737157	1030.053008	16.595303
28.707973	1016.364244	16.600320
28.803480	1030.919875	16.605338
28.800774	1039.718822	16.610355
28.923534	1041.659346	16.615373
28.699508	1045.131152	16.620391
28.889361	1039.196739	16.625408
29.039004	1049.139492	16.630426
29.265935	1034.877245	16.635443
29.078682	1036.399272	16.640461
28.962173	1038.774924	16.645479
29.365293	1037.607174	16.650496
29.148569	1040.364608	16.655514
29.035231	1045.589514	16.660531
28.950195	1041.869408	16.665549
29.025961	1041.194768	16.670567
29.324502	1026.268043	16.675584
28.945258	1040.531985	16.680602
29.248804	1040.386558	16.685619
29.347406	1048.327019	16.690637
29.157413	1046.138174	16.695655
29.297787	1038.712476	16.700672
29.270015	1045.495598	16.705690
29.195437	1043.941935	16.710707
29.329072	1047.001090	16.715725
29.090643	1048.928777	16.720743
29.298117	1041.735566	16.725760
29.401952	1049.255478	16.730778
29.433198	1057.474745	16.735795
29.428223	1057.986740	16.740813
29.347003	1070.146383	16.745831
29.571970	1069.644030	16.750848
29.446655	1067.189423	16.755866
29.510274	1063.452334	16.760883
29.658724	1066.805823	16.765901
29.525342	1064.882667	16.770919
29.839940	1063.580459	16.775936
29.375899	1067.266603	16.780954
29.190599	1051.418408	16.785971
29.776046	1073.080073	16.790989
29.658695	1083.765281	16.796007
30.110304	1080.727964	16.801024
29.894886	1080.446092	16.806042
30.129489	1086.320255	16.811059
30.129925	1080.286115	16.816077
30.219751	1095.306603	16.821095
30.294836	1088.086778	16.826112
29.977126	1091.058863	16.831130
30.229451	1082.435308	16.836147
30.511344	1072.380670	16.841165
30.146009	1078.484530	16.846183
30.327239	1080.182363	16.851200
30.414991	1080.329528	16.856218
30.470110	1075.640693	16.861235
30.433793	1076.429004	16.866253
30.405523	1069.032872	16.871271
30.079852	1055.223271	16.876288
30.618607	1059.566511	16.881306
30.536803	1066.266586	16.886323
30.409592	1060.549105	16.891341
30.578947	1068.898221	16.896359
30.407263	1049.112521	16.901376
30.443225	1062.645538	16.906394
30.721326	1071.078605	16.911411
30.719893	1081.392192	16.916429
30.366915	1072.399567	16.921447
30.576452	1072.196283	16.926464
30.321953	1068.218695	16.931482
30.624687	1070.557067	16.936499
30.962617	1070.895413	16.941517
30.508580	1080.001784	16.946535
30.910304	1067.952796	16.951552
30.536479	1076.074588	16.956570
30.574216	1070.242895	16.961587
30.716929	1081.436478	16.966605
30.788129	1074.933651	16.971623
30.667357	1075.148202	16.976640
30.600087	1074.792624	16.981658
30.651514	1095.868941	16.986675
31.079609	1097.332432	16.991693
31.208223	1096.330767	16.996711
31.268234	1097.246001	17.001728
31.036602	1100.535968	17.006746
31.154799	1102.628696	17.011763
31.341684	1097.294347	17.016781
31.280938	1099.705452	17.021799
31.551371	1098.470123	17.026816
31.370173	1093.007248	17.031834
31.532340	1096.926652	17.036851
31.569022	1098.334702	17.041869
30.909896	1101.060472	17.046887
31.191563	1097.232406	17.051904
31.238241	1101.091008	17.056922
31.182150	1096.757271	17.061939
31.547963	1094.124724	17.066957
31.257152	1105.701833	17.071975
30.971582	1103.165030	17.076992
31.236165	1102.299855	17.082010
31.539414	1120.281854	17.087027
31.495575	1115.384446	17.092045
31.510476	1117.180928	17.097063
32.004697	1122.970244	17.102080
31.681883	1126.953017	17.107098
31.741937	1119.019149	17.112115
32.028113	1120.495411	17.117133
31.828310	1129.372621	17.122151
31.877186	1129.475383	17.127168
32.083935	1123.525672	17.132186
31.608485	1123.729520	17.137203
31.910956	1121.681263	17.142221
31.693538	1121.333430	17.147239
31.730313	1118.708250	17.152256
31.849364	1122.729091	17.157274
31.932391	1133.610158	17.162291
32.485144	1144.162008	17.167309
32.311658	1147.853139	17.172327
32.555831	1132.669749	17.177344
32.440932	1116.860960	17.182362
32.201915	1118.245934	17.187379
32.703957	1109.466474	17.192397
32.688480	1111.106765	17.197415
32.503056	1105.117517	17.202432
32.091443	1103.316846	17.207450
32.097011	1111.811568	17.212467
32.161985	1103.656025	17.217485
32.044147	1117.235271	17.222503
32.533511	1124.193025	17.227520
32.794154	1128.005486	17.232538
32.640528	1137.714930	17.237555
32.781560	1132.397222	17.242573
32.672965	1137.107001	17.247591
32.597692	1129.033382	17.252608
32.858916	1129.762454	17.257626
32.742664	1127.344289	17.262643
32.843682	1122.976463	17.267661
32.442646	1134.217402	17.272679
32.560460	1131.308116	17.277696
32.978479	1128.140351	17.282714
32.960875	1143.865694	17.287731
33.438604	1136.267176	17.292749
33.289666	1136.385152	17.297767
33.107041	1128.643941	17.302784
32.791179	1120.428135	17.307802
32.778715	1137.415020	17.312819
33.156151	1132.060273	17.317837
33.178718	1136.907297	17.322855
33.249155	1126.803706	17.327872
33.306413	1135.362925	17.332890
33.003733	1134.125867	17.337907
33.255933	1127.042383	17.342925
32.974838	1131.791811	17.347943
32.789944	1124.742096	17.352960
33.021339	1121.865511	17.357978
32.970580	1137.857982	17.362995
33.001790	1139.525675	17.368013
33.537266	1153.220345	17.373031
33.094776	1151.613861	17.378048
33.425848	1159.694679	17.383066
33.229252	1158.308450	17.388083
33.660497	1152.203633	17.393101
33.498433	1149.505457	17.398119
33.644852	1151.155101	17.403136
33.563264	1147.589071	17.408154
33.781348	1154.450482	17.413171
33.874163	1150.244884	17.418189
33.689117	1146.489931	17.423207
33.311037	1150.500303	17.428224
33.984166	1145.367474	17.433242
33.524954	1149.848161	17.438259
33.750144	1170.496543	17.443277
34.012680	1176.300086	17.448295
34.158357	1175.586085	17.453312
34.390368	1174.473538	17.458330
34.122476	1188.294105	17.463347
34.284941	1168.111928	17.468365
33.906063	1159.609323	17.473383
34.219534	1171.476816	17.478400
34.345486	1161.910476	17.483418
34.330436	1173.595906	17.488435
34.100143	1170.782182	17.493453
34.149936	1163.067659	17.498471
34.056354	1165.534412	17.503488
34.339983	1171.470351	17.508506
34.324435	1174.748567	17.513523
34.398324	1166.717834	17.518541
34.487811	1169.597729	17.523559
34.452621	1176.038070	17.528576
34.823480	1172.088714	17.533594
34.446695	1176.711132	17.538611
34.510008	1173.374865	17.543629
34.564489	1172.529982	17.548647
34.440818	1172.123277	17.553664
34.586013	1171.949010	17.558682
34.437684	1177.043732	17.563699
34.827612	1167.230897	17.568717
34.666816	1166.268261	17.573735
34.651191	1171.623064	17.578752
34.723780	1168.118083	17.583770
34.523891	1175.878144	17.588787
34.714901	1179.824606	17.593805
34.908030	1196.419563	17.598823
34.936644	1199.217480	17.603840
35.095683	1190.589554	17.608858
35.031390	1199.025833	17.613875
35.281365	1196.824843	17.618893
34.921496	1192.620731	17.623911
35.188903	1196.378496	17.628928
35.412197	1190.688110	17.633946
34.932320	1199.299958	17.638963
35.101030	1195.483258	17.643981
35.410980	1196.229945	17.648999
35.407166	1192.282481	17.654016
35.175202	1188.105669	17.659034
34.875224	1189.579098	17.664051
35.096804	1196.077048	17.669069
35.245531	1190.975874	17.674087
35.245285	1200.412005	17.679104
35.450392	1202.882460	17.684122
35.487902	1214.177818	17.689139
35.207669	1215.701805	17.694157
35.808408	1220.070089	17.699175
35.662516	1223.924174	17.704192
35.487035	1208.086925	17.709210
35.525163	1217.078383	17.714227
35.607839	1219.473345	17.719245
35.802173	1216.987571	17.724263
35.459881	1223.150988	17.729280
35.656222	1215.369299	17.734298
35.619010	1231.624826	17.739315
36.225820	1244.585689	17.744333
36.392249	1236.357383	17.749351
36.126253	1244.456045	17.754368
36.444387	1229.264141	17.759386
36.023088	1223.094052	17.764403
36.627774	1216.368729	17.769421
36.647744	1213.799818	17.774439
36.140111	1216.148408	17.779456
36.276402	1204.289244	17.784474
36.072650	1212.933577	17.789491
35.643680	1215.481288	17.794509
35.929511	1228.773304	17.799527
36.591353	1229.562692	17.804544
36.695669	1228.220834	17.809562
36.243472	1234.044856	17.814579
36.289307	1230.402040	17.819597
36.560162	1235.175474	17.824615
36.446370	1234.672542	17.829632
36.571873	1236.054064	17.834650
36.837571	1234.043115	17.839667
36.619496	1239.060418	17.844685
36.591057	1229.647624	17.849703
36.305966	1241.097688	17.854720
36.770814	1231.920040	17.859738
36.792840	1233.147355	17.864755
36.530405	1232.412085	17.869773
37.106850	1238.141218	17.874791
36.920513	1244.655759	17.879808
37.158740	1245.864980	17.884826
37.163424	1241.808873	17.889843
37.064608	1236.572896	17.894861
37.174466	1225.001890	17.899879
36.697000	1231.776642	17.904896
37.174773	1232.872589	17.909914
36.946947	1247.343352	17.914931
37.198475	1250.592360	17.919949
37.462458	1242.396106	17.924967
37.234203	1256.870100	17.929984
37.130889	1251.868360	17.935002
37.250291	1246.642372	17.940019
37.066622	1257.653665	17.945037
37.691385	1251.389102	17.950055
36.889686	1254.951456	17.955072
37.620082	1249.658142	17.960090
37.555793	1248.039731	17.965107
37.507508	1251.815411	17.970125
37.534779	1248.964476	17.975143
37.397519	1259.062754	17.980160
37.594053	1255.386853	17.985178
37.424390	1249.925279	17.990195
37.904270	1261.343868	17.995213
37.958315	1266.501585	18.000231
37.877166	1264.832164	18.005248
37.843667	1268.958993	18.010266
37.668400	1268.721321	18.015283
37.891788	1274.603615	18.020301
38.097666	1271.049328	18.025319
38.054665	1275.584759	18.030336
38.134355	1270.062020	18.035354
38.282017	1275.858345	18.040371
38.029295	1277.068748	18.045389
38.591025	1269.277126	18.050407
37.975298	1273.640350	18.055424
38.135215	1263.263878	18.060442
38.344803	1260.624224	18.065459
38.486374	1263.855748	18.070477
38.621249	1261.458182	18.075495
38.280169	1270.316569	18.080512
38.418573	1266.630839	18.085530
38.500714	1263.686094	18.090547
38.102147	1264.622691	18.095565
38.772979	1257.492501	18.100583
38.337630	1273.213979	18.105600
38.432000	1261.414995	18.110618
38.633403	1271.299267	18.115635
38.494629	1268.606892	18.120653
38.590427	1260.364395	18.125671
38.874298	1267.325998	18.130688
38.669410	1279.946987	18.135706
38.602253	1281.712159	18.140723
38.500407	1285.101750	18.145741
38.745171	1290.340050	18.150759
38.855348	1289.887235	18.155776
38.833551	1283.648221	18.160794
39.027648	1280.360874	18.165811
38.826387	1287.650967	18.170829
39.371786	1281.105328	18.175847
38.917164	1293.692869	18.180864
39.198583	1292.522080	18.185882
39.021205	1283.678565	18.190899
39.369143	1290.750065	18.195917
39.590881	1302.288023	18.200935
39.361180	1292.717374	18.205952
39.202737	1290.034389	18.210970
39.289872	1303.606910	18.215987
39.638452	1314.951427	18.221005
39.659162	1308.980309	18.226023
39.855600	1300.797766	18.231040
39.877292	1295.855326	18.236058
39.770653	1288.736479	18.241075
39.264514	1280.600905	18.246093
39.476365	1290.325756	18.251111
39.730862	1306.450438	18.256128
39.731642	1299.728181	18.261146
40.014440	1309.909002	18.266163
39.758994	1315.919983	18.271181
39.631084	1308.810772	18.276199
40.041764	1312.015921	18.281216
39.670187	1310.477209	18.286234
39.774525	1297.764579	18.291251
39.822589	1303.128379	18.296269
39.931737	1302.170779	18.301287
40.147098	1318.128028	18.306304
40.124130	1312.520370	18.311322
40.456277	1310.568432	18.316339
40.013768	1308.542199	18.321357
40.342849	1299.041794	18.326375
40.351879	1298.901483	18.331392
40.185903	1309.360907	18.336410
40.447577	1306.432210	18.341427
39.872585	1316.305602	18.346445
40.691176	1318.888245	18.351463
40.832128	1322.078849	18.356480
40.726067	1332.399507	18.361498
40.561107	1328.212163	18.366515
40.546444	1330.789655	18.371533
40.902297	1323.746660	18.376551
40.913981	1319.582137	18.381568
40.924883	1328.309664	18.386586
40.618604	1328.259781	18.391603
40.641070	1326.469975	18.396621
41.207369	1322.808713	18.401639
41.346840	1328.319150	18.406656
40.835945	1336.099605	18.411674
41.036636	1323.690609	18.416691
40.906488	1325.970601	18.421709
41.087291	1311.870001	18.426727
40.904633	1320.637318	18.431744
40.930223	1324.357256	18.436762
40.998150	1314.361254	18.441779
41.040750	1332.365370	18.446797
41.040868	1321.837169	18.451815
41.041863	1329.433274	18.456832
41.315979	1342.446334	18.461850
41.456936	1343.276312	18.466867
41.283091	1343.180432	18.471885
41.228977	1337.025360	18.476903
41.375167	1345.128918	18.481920
40.951682	1347.584265	18.486938
41.304429	1341.624231	18.491955
41.447963	1354.613577	18.496973
41.773376	1351.813746	18.501991
42.099288	1356.992013	18.507008
41.964818	1357.442251	18.512026
41.898062	1335.105587	18.517043
41.912752	1342.241943	18.522061
42.024451	1339.178942	18.527079
41.790850	1337.615454	18.532096
41.701395	1355.760209	18.537114
42.043502	1348.429013	18.542131
42.068774	1355.775163	18.547149
42.333306	1359.959464	18.552167
42.230166	1352.467644	18.557184
42.195460	1357.939106	18.562202
42.322581	1355.236617	18.567219
42.346874	1351.502473	18.572237
42.215888	1353.747886	18.577255
42.188546	1348.765775	18.582272
42.359129	1352.115850	18.587290
42.382315	1352.519295	18.592307
42.297795	1359.513406	18.597325
42.680688	1354.823638	18.602343
42.430181	1347.743088	18.607360
42.634079	1357.563899	18.612378
42.714366	1351.491910	18.617395
42.666654	1361.386860	18.622413
42.626081	1361.920220	18.627431
42.490628	1352.366332	18.632448
42.297469	1357.764786	18.637466
42.831313	1361.098976	18.642483
42.874170	1378.803286	18.647501
42.847468	1378.738003	18.652519
42.607154	1369.225782	18.657536
42.861444	1378.508514	18.662554
43.143810	1381.225675	18.667571
42.919028	1380.190998	18.672589
43.270960	1375.654404	18.677607
43.439540	1377.029187	18.682624
42.905039	1376.222924	18.687642
42.937821	1382.015192	18.692659
43.034648	1378.345420	18.697677
43.089161	1384.920110	18.702695
43.569808	1402.742052	18.707712
43.556066	1397.918749	18.712730
43.531433	1398.847260	18.717747
43.814593	1393.352566	18.722765
43.105673	1395.764275	18.727783
43.881483	1390.744683	18.732800
43.756818	1398.941197	18.737818
43.934795	1398.408327	18.742835
44.020404	1397.722664	18.747853
43.906562	1392.182870	18.752871
43.718618	1392.278555	18.757888
43.438013	1388.109316	18.762906
43.789193	1389.569105	18.767923
43.809971	1391.797056	18.772941
43.781018	1386.616363	18.777959
44.102995	1385.780054	18.782976
43.504518	1393.441706	18.787994
43.713208	1401.374544	18.793011
44.018173	1411.690812	18.798029
44.168966	1421.494731	18.803047
44.310183	1424.587479	18.808064
44.212731	1426.022882	18.813082
44.491699	1412.241352	18.818099
44.418308	1418.990735	18.823117
44.212984	1418.151831	18.828135
44.466455	1411.333134	18.833152
44.484801	1411.585854	18.838170
44.434111	1413.544128	18.843187
44.507457	1410.881615	18.848205
44.387356	1416.574766	18.853223
45.043614	1424.743617	18.858240
44.749263	1438.016233	18.863258
45.251627	1434.857292	18.868275
44.957134	1423.191714	18.873293
44.791424	1420.926431	18.878311
45.280501	1416.980592	18.883328
45.316916	1415.936548	18.888346
44.916965	1407.001607	18.893363
45.313688	1413.563719	18.898381
44.894667	1409.211026	18.903399
44.953478	1400.563987	18.908416
45.020283	1426.375339	18.913434
45.274282	1433.679374	18.918451
45.023357	1442.176567	18.923469
45.219507	1446.551491	18.928487
45.507591	1436.558798	18.933504
45.399268	1444.771708	18.938522
45.301817	1441.287003	18.943539
45.374151	1438.725635	18.948557
45.245648	1437.495981	18.953575
45.391761	1441.487407	18.958592
45.391138	1435.005170	18.963610
45.047530	1433.506248	18.968627
45.577045	1450.216003	18.973645
45.764700	1462.605197	18.978663
46.075146	1465.172798	18.983680
45.913464	1471.948658	18.988698
45.902110	1451.020188	18.993715
45.887141	1456.558019	18.998733
45.792545	1452.066119	19.003751
46.171696	1457.226607	19.008768
46.221306	1449.029130	19.013786
46.045347	1454.219782	19.018803
46.240104	1460.314916	19.023821
46.419442	1457.490617	19.028839
46.542361	1455.931223	19.033856
46.112313	1455.670347	19.038874
46.601255	1453.286712	19.043891
46.371950	1458.081763	19.048909
46.116284	1454.470359	19.053927
46.467891	1450.811149	19.058944
46.079777	1456.669386	19.063962
46.910583	1464.801440	19.068979
46.723332	1470.132728	19.073997
46.452785	1473.198475	19.079015
46.544910	1471.239943	19.084032
46.288248	1488.000322	19.089050
46.323994	1480.600302	19.094067
46.653040	1480.810656	19.099085
46.601876	1481.576063	19.104103
46.945320	1484.198460	19.109120
46.937608	1502.153823	19.114138
47.476979	1506.856857	19.119155
47.033262	1500.586036	19.124173
47.013246	1500.828989	19.129191
47.409216	1505.914268	19.134208
47.585486	1510.939292	19.139226
47.218872	1502.649206	19.144243
47.487770	1497.904675	19.149261
47.280505	1499.871710	19.154279
47.483639	1505.031385	19.159296
47.377400	1505.868541	19.164314
47.779106	1503.757356	19.169331
47.850524	1503.244334	19.174349
47.920574	1503.971815	19.179367
47.553248	1503.303462	19.184384
47.804828	1506.902820	19.189402
47.814882	1493.602037	19.194419
47.781204	1490.388210	19.199437
48.111546	1503.402047	19.204455
48.181079	1495.330822	19.209472
47.897624	1495.564553	19.214490
47.497644	1495.867036	19.219507
47.536286	1503.406821	19.224525
47.472325	1507.323873	19.229543
47.772554	1507.674448	19.234560
47.886227	1517.768272	19.239578
48.089523	1524.957206	19.244595
48.238516	1523.617793	19.249613
48.106940	1526.393520	19.254631
48.417462	1525.398046	19.259648
48.419187	1525.549226	19.264666
48.437550	1520.424200	19.269683
48.440565	1516.712291	19.274701
48.358940	1523.680764	19.279719
48.180116	1518.141644	19.284736
48.330856	1531.691749	19.289754
48.761176	1541.398288	19.294771
48.806825	1542.618767	19.299789
49.020578	1548.133414	19.304807
48.938890	1539.195882	19.309824
49.003196	1540.082062	19.314842
49.135060	1536.239503	19.319859
48.593062	1530.732032	19.324877
48.489823	1539.673214	19.329895
48.705508	1532.345971	19.334912
49.073614	1543.791722	19.339930
48.965151	1540.097275	19.344947
49.100507	1542.307293	19.349965
48.960421	1555.262322	19.354983
49.609952	1563.451227	19.360000
49.368827	1570.078617	19.365018
49.232438	1576.279324	19.370035
49.941570	1568.937874	19.375053
49.575837	1565.930701	19.380071
49.779838	1569.360793	19.385088
49.786510	1566.244777	19.390106
49.706845	1554.116244	19.395123
49.544215	1558.506380	19.400141
49.579688	1570.461878	19.405159
49.799113	1564.207064	19.410176
49.715458	1563.263878	19.415194
49.978632	1558.857916	19.420211
49.980543	1561.202459	19.425229
49.602259	1558.929436	19.430247
49.756592	1566.151305	19.435264
49.736061	1568.704503	19.440282
49.696310	1581.486033	19.445299
50.253559	1574.815349	19.450317
49.964689	1588.011474	19.455335
50.220540	1586.068305	19.460352
50.250378	1577.444657	19.465370
50.302560	1592.534580	19.470387
50.488946	1587.165448	19.475405
50.346543	1589.788238	19.480423
50.678049	1595.353882	19.485440
51.027275	1602.242258	19.490458
50.498000	1594.577248	19.495475
50.781578	1596.603096	19.500493
50.785837	1597.457660	19.505511
51.078316	1611.607344	19.510528
51.009142	1606.710614	19.515546
51.114522	1603.468668	19.520563
51.310461	1601.866261	19.525581
50.984814	1598.625572	19.530599
50.907249	1597.043925	19.535616
50.997351	1611.105390	19.540634
51.256203	1611.926377	19.545651
51.411518	1603.507131	19.550669
50.676216	1612.241249	19.555687
51.121214	1608.207595	19.560704
51.628564	1595.535759	19.565722
51.165198	1602.680844	19.570739
51.446091	1595.545340	19.575757
51.539013	1600.974789	19.580775
51.265251	1599.982487	19.585792
51.287013	1600.244143	19.590810
51.529873	1621.934904	19.595827
52.178210	1624.193956	19.600845
51.861797	1626.635721	19.605863
52.081497	1629.239656	19.610880
52.185122	1622.242375	19.615898
51.800969	1612.032999	19.620915
52.109448	1605.729501	19.625933
51.822715	1618.066890	19.630951
52.056815	1619.658657	19.635968
52.315228	1620.719568	19.640986
51.927817	1623.011501	19.646003
51.920030	1622.949566	19.651021
51.898309	1621.684233	19.656039
51.945976	1616.734478	19.661056
52.291285	1614.149253	19.666074
51.926695	1624.879832	19.671091
52.248614	1632.309013	19.676109
52.501460	1643.649804	19.681127
52.447186	1645.075305	19.686144
52.716208	1639.453356	19.691162
52.366376	1648.026107	19.696179
52.675422	1642.300051	19.701197
52.244151	1656.642064	19.706215
52.657620	1648.769361	19.711232
52.684204	1654.136632	19.716250
52.732893	1662.533336	19.721267
52.659894	1667.635330	19.726285
53.289760	1666.444641	19.731303
53.051213	1673.892219	19.736320
53.208086	1665.138166	19.741338
53.181511	1676.573252	19.746355
53.230994	1661.151660	19.751373
53.169350	1664.920052	19.756391
53.300318	1670.782242	19.761408
53.798922	1664.287981	19.766426
53.241598	1677.220102	19.771443
53.587447	1677.620341	19.776461
53.647561	1681.338100	19.781479
53.665744	1687.047543	19.786496
53.738294	1685.985198	19.791514
53.547296	1690.247259	19.796531
53.560087	1689.853877	19.801549
53.919964	1691.271301	19.806567
54.007215	1686.883403	19.811584
54.325247	1676.658654	19.816602
53.997026	1681.974219	19.821619
53.985001	1680.341269	19.826637
54.192488	1673.816872	19.831655
53.964472	1682.430517	19.836672
54.196917	1682.207859	19.841690
54.027748	1680.432262	19.846707
54.231345	1686.390381	19.851725
54.317122	1699.701469	19.856743
54.325517	1695.704641	19.861760
54.511992	1697.859330	19.866778
54.416948	1699.382746	19.871795
54.689343	1701.344083	19.876813
54.794017	1698.663996	19.881831
54.722965	1696.024065	19.886848
54.781385	1697.570776	19.891866
54.579418	1699.827352	19.896883
55.021573	1703.633591	19.901901
54.869706	1697.818777	19.906919
54.667547	1690.840974	19.911936
55.064841	1698.226814	19.916954
54.916349	1720.717511	19.921971
55.161192	1726.482978	19.926989
55.000308	1714.332345	19.932007
54.972956	1717.489426	19.937024
55.127590	1721.766774	19.942042
55.427092	1716.755444	19.947059
55.383717	1718.826220	19.952077
55.400860	1716.784730	19.957095
55.333066	1714.040138	19.962112
55.685208	1715.114774	19.967130
55.632143	1724.808780	19.972147
55.702962	1721.865735	19.977165
55.540387	1718.227068	19.982183
55.399894	1733.268397	19.987200
55.789725	1741.475981	19.992218
55.830955	1753.891475	19.997235
55.633169	1740.515768	20.002253
56.233766	1745.941464	20.007271
56.179992	1748.288444	20.012288
56.183476	1738.936656	20.017306
55.938067	1739.151805	20.022323
56.032354	1745.063950	20.027341
56.068110	1742.347315	20.032359
55.975917	1740.733231	20.037376
56.638255	1752.000466	20.042394
56.446855	1763.900115	20.047411
56.426983	1767.273796	20.052429
56.562793	1761.319209	20.057447
56.619113	1764.075002	20.062464
56.765564	1760.567801	20.067482
56.599957	1762.777661	20.072499
56.843533	1758.469400	20.077517
56.659268	1765.504545	20.082535
56.768875	1764.288057	20.087552
56.928455	1758.676907	20.092570
56.680709	1758.220195	20.097587
57.030035	1767.497708	20.102605
57.262022	1779.529861	20.107623
57.080636	1794.271516	20.112640
57.437298	1783.535695	20.117658
57.411904	1790.255605	20.122675
57.171579	1787.354986	20.127693
57.451355	1786.316976	20.132711
57.189104	1784.088864	20.137728
57.614747	1774.333224	20.142746
57.773126	1783.523890	20.147763
57.600456	1778.267765	20.152781
57.725268	1784.052056	20.157799
57.322967	1784.465367	20.162816
57.451691	1785.631819	20.167834
57.545688	1799.819061	20.172851
57.845767	1798.364433	20.177869
57.879268	1799.732009	20.182887
58.161199	1806.356436	20.187904
58.073376	1805.833639	20.192922
57.898369	1806.747859	20.197939
58.173194	1803.217381	20.202957
58.178394	1806.037997	20.207975
58.531677	1826.644977	20.212992
58.458525	1825.851621	20.218010
58.489540	1826.847180	20.223027
58.547049	1835.990557	20.228045
58.733853	1828.945447	20.233063
58.407738	1836.447840	20.238080
58.879244	1825.817084	20.243098
58.448291	1817.906184	20.248115
58.978917	1829.904206	20.253133
58.699256	1817.816296	20.258151
59.008441	1824.231319	20.263168
59.191721	1825.733231	20.268186
58.995596	1822.923517	20.273203
58.808153	1820.705772	20.278221
59.307735	1824.039106	20.283239
59.210150	1825.083218	20.288256
58.877525	1815.036077	20.293274
59.173221	1833.464976	20.298291
59.128893	1850.479622	20.303309
59.088163	1847.471977	20.308327
59.481376	1850.853542	20.313344
59.708731	1843.511720	20.318362
59.798536	1851.977815	20.323379
59.214153	1844.176154	20.328397
59.325726	1848.438188	20.333415
59.464544	1848.015589	20.338432
60.033951	1855.778498	20.343450
59.899045	1870.541337	20.348467
59.932148	1871.637564	20.353485
59.993893	1866.111141	20.358503
59.983555	1872.645675	20.363520
60.125782	1875.239692	20.368538
60.139579	1877.538230	20.373555
59.912361	1871.716228	20.378573
60.200659	1867.110582	20.383591
60.084253	1883.136095	20.388608
60.243025	1880.002507	20.393626
60.422190	1890.162025	20.398643
60.263472	1894.406453	20.403661
60.753966	1882.150495	20.408679
60.540017	1879.927428	20.413696
60.555636	1895.471489	20.418714
60.222536	1892.995670	20.423731
60.550770	1904.924459	20.428749
61.237371	1909.380457	20.433767
61.153187	1911.195699	20.438784
61.204736	1914.305736	20.443802
61.242672	1914.498586	20.448819
61.490712	1924.789353	20.453837
61.557774	1910.125395	20.458855
61.493997	1913.663784	20.463872
61.644533	1906.267696	20.468890
61.421993	1918.020836	20.473907
61.262219	1910.480847	20.478925
61.560063	1909.872374	20.483943
61.238931	1914.451543	20.488960
61.649121	1908.472856	20.493978
61.768017	1908.564652	20.498995
61.486439	1916.120065	20.504013
61.502835	1908.946978	20.509031
61.466108	1914.393678	20.514048
61.725358	1927.914458	20.519066
61.974215	1932.082414	20.524083
62.093495	1934.613759	20.529101
61.993619	1922.920518	20.534119
62.149375	1926.462386	20.539136
62.326283	1929.811580	20.544154
62.645463	1923.515764	20.549171
62.070703	1934.288923	20.554189
61.961061	1934.006243	20.559207
62.172547	1943.870372	20.564224
62.770671	1951.502583	20.569242
62.789628	1950.966208	20.574259
62.354236	1961.319888	20.579277
62.712700	1955.977339	20.584295
62.495845	1958.065854	20.589312
62.463454	1961.892846	20.594330
63.021516	1970.560208	20.599347
62.967240	1981.816779	20.604365
63.179432	1978.513846	20.609383
63.538207	1984.523497	20.614400
63.523842	1981.369677	20.619418
63.536652	1977.520429	20.624435
63.429066	1976.972319	20.629453
63.454369	1973.360972	20.634471
63.411824	1973.983028	20.639488
63.388870	1975.608790	20.644506
63.572164	1967.683642	20.649523
63.493253	1975.623924	20.654541
63.783358	1970.194243	20.659559
63.604544	1965.885835	20.664576
63.486490	1974.517107	20.669594
63.527000	1972.342530	20.674611
63.340616	1985.740655	20.679629
63.858219	1984.908388	20.684647
63.886752	1987.450802	20.689664
63.881068	2005.412663	20.694682
64.220166	1991.564459	20.699699
63.983013	2000.043978	20.704717
64.303420	1998.996434	20.709735
64.386536	2000.750757	20.714752
64.614241	2010.034827	20.719770
64.905854	2016.768277	20.724787
64.838000	2017.558414	20.729805
64.726929	2006.876805	20.734823
64.943556	2006.678715	20.739840
64.717862	2014.471585	20.744858
65.045399	2010.708729	20.749875
65.122653	2015.850402	20.754893
65.193302	2011.543927	20.759911
65.218182	2012.628827	20.764928
65.312348	2016.439158	20.769946
65.532726	2011.307590	20.774963
65.368607	2009.884645	20.779981
64.986289	2005.144173	20.784999
65.098565	2018.053684	20.790016
65.080751	2014.742597	20.795034
65.394070	2009.277708	20.800051
65.066572	2012.466085	20.805069
65.433772	2011.038797	20.810087
65.543030	2034.259578	20.815104
65.648940	2034.678482	20.820122
65.498221	2033.389146	20.825139
65.097987	2042.462323	20.830157
65.776161	2039.651304	20.835175
66.046229	2054.420278	20.840192
65.597765	2065.467241	20.845210
65.988091	2064.175191	20.850227
65.696005	2071.785968	20.855245
66.076734	2061.257666	20.860263
66.122503	2063.317671	20.865280
66.242960	2073.975679	20.870298
66.661166	2074.216258	20.875315
66.576262	2085.162087	20.880333
66.818976	2086.023499	20.885351
67.119948	2078.322882	20.890368
67.167359	2074.319857	20.895386
67.175398	2069.966368	20.900403
66.888710	2082.382969	20.905421
67.371490	2077.251299	20.910439
67.221074	2072.575469	20.915456
66.797370	2078.559412	20.920474
67.072023	2080.100683	20.925491
67.167989	2079.457557	20.930509
67.246029	2086.237119	20.935527
67.323707	2074.929403	20.940544
67.183124	2088.209967	20.945562
67.772456	2071.560951	20.950579
67.124696	2080.373103	20.955597
67.310115	2072.267682	20.960615
67.005948	2083.301516	20.965632
67.010917	2096.417259	20.970650
67.506781	2097.396812	20.975667
67.438731	2111.189934	20.980685
67.512484	2112.219842	20.985703
68.174060	2116.114879	20.990720
67.825232	2120.269215	20.995738
68.390700	2124.416016	21.000755
68.114792	2126.599016	21.005773
68.017489	2119.159613	21.010791
68.356313	2116.136641	21.015808
68.323113	2130.129462	21.020826
67.972831	2128.855604	21.025843
68.216882	2137.521748	21.030861
68.523695	2149.993744	21.035879
68.916447	2147.924917	21.040896
68.666295	2155.456570	21.045914
68.842780	2144.272197	21.050931
68.523707	2145.351028	21.055949
68.843262	2145.594440	21.060967
68.963274	2142.823514	21.065984
68.716797	2145.996065	21.071002
69.337288	2153.615391	21.076019
69.167994	2164.246259	21.081037
69.609226	2172.319747	21.086055
69.821722	2175.265747	21.091072
69.381892	2175.438771	21.096090
69.808396	2168.075084	21.101107
69.611295	2166.982369	21.106125
69.829202	2170.650259	21.111143
69.908804	2168.535811	21.116160
69.941984	2171.617210	21.121178
69.844829	2161.529826	21.126195
70.084029	2156.174343	21.131213
70.265947	2164.480975	21.136231
69.904927	2161.589735	21.141248
69.896096	2161.688921	21.146266
69.817791	2160.075779	21.151283
70.048890	2154.888837	21.156301
70.033734	2163.791281	21.161319
70.263023	2175.906181	21.166336
69.955757	2185.431962	21.171354
70.012439	2185.975358	21.176371
70.162515	2191.484401	21.181389
69.920084	2203.878370	21.186407
70.525261	2206.646078	21.191424
70.558020	2213.565337	21.196442
70.962628	2220.713542	21.201459
70.950011	2216.413751	21.206477
70.933069	2215.207593	21.211495
71.304558	2233.227363	21.216512
71.026526	2239.649324	21.221530
71.535486	2226.216179	21.226547
71.508197	2236.723847	21.231565
71.332417	2237.663458	21.236583
71.710723	2227.728781	21.241600
71.478959	2239.947520	21.246618
71.699279	2234.304613	21.251635
71.728974	2227.684785	21.256653
71.461260	2233.776894	21.261671
71.462815	2222.083347	21.266688
71.612812	2231.386019	21.271706
72.087153	2235.461910	21.276723
72.210307	2251.421814	21.281741
72.037912	2256.492207	21.286759
72.141938	2251.707032	21.291776
72.211312	2259.573709	21.296794
72.192520	2249.240448	21.301811
72.228246	2261.556161	21.306829
72.160398	2262.112757	21.311847
72.465655	2257.403360	21.316864
72.620718	2257.858755	21.321882
72.576641	2249.994355	21.326899
72.795195	2265.200802	21.331917
72.700119	2281.308542	21.336935
73.193039	2269.181342	21.341952
72.888875	2284.678003	21.346970
73.240312	2276.325554	21.351987
73.014636	2279.999843	21.357005
72.951295	2278.598960	21.362023
73.084836	2266.944670	21.367040
73.076560	2280.898986	21.372058
73.358070	2279.649219	21.377075
73.606816	2275.945995	21.382093
73.318397	2278.121505	21.387111
73.760373	2286.864019	21.392128
73.255978	2295.792681	21.397146
73.838167	2302.231382	21.402163
73.851838	2292.814588	21.407181
73.457162	2305.699581	21.412199
73.566299	2298.177263	21.417216
73.838787	2303.212685	21.422234
73.982427	2314.331148	21.427251
74.065505	2325.149810	21.432269
74.174201	2330.693784	21.437287
74.394127	2319.644521	21.442304
74.336202	2323.014800	21.447322
74.290549	2328.564019	21.452339
74.119767	2323.992310	21.457357
74.534664	2336.658960	21.462375
74.631718	2338.338543	21.467392
74.547740	2353.624024	21.472410
75.099281	2344.621597	21.477427
74.902137	2349.588586	21.482445
74.932924	2354.466212	21.487463
75.356254	2352.193738	21.492480
75.125567	2362.250463	21.497498
75.034651	2354.216615	21.502515
75.305590	2353.804866	21.507533
75.413893	2359.708706	21.512551
75.401125	2366.398449	21.517568
75.397707	2371.492898	21.522586
75.801223	2365.666599	21.527603
75.733427	2360.987218	21.532621
75.532295	2369.868403	21.537639
75.686563	2363.153261	21.542656
75.508432	2364.939082	21.547674
75.477446	2373.648431	21.552691
75.759989	2390.861709	21.557709
75.950598	2384.576408	21.562727
76.010884	2382.404995	21.567744
76.082626	2383.403673	21.572762
76.225241	2394.011057	21.577779
76.251837	2401.284838	21.582797
76.484458	2415.087896	21.587815
76.787156	2413.585468	21.592832
76.931961	2419.815001	21.597850
77.105968	2410.180502	21.602867
76.898332	2412.826256	21.607885
76.519557	2412.282747	21.612903
77.016541	2408.935117	21.617920
77.154806	2416.270311	21.622938
76.465784	2409.848235	21.627955
77.020258	2422.994900	21.632973
76.919801	2434.252676	21.637991
77.447481	2440.917740	21.643008
77.435127	2440.367319	21.648026
77.608135	2438.932550	21.653043
77.771200	2427.668046	21.658061
77.839618	2440.660479	21.663079
78.146995	2434.934436	21.668096
77.911290	2433.857220	21.673114
78.050615	2435.653277	21.678131
78.184660	2429.200081	21.683149
78.074784	2443.261967	21.688167
77.918207	2424.595957	21.693184
78.175434	2435.153848	21.698202
78.170799	2430.496114	21.703219
78.386420	2435.335336	21.708237
78.041944	2448.278844	21.713255
78.518459	2448.036877	21.718272
78.475713	2453.970726	21.723290
78.317923	2461.245014	21.728307
78.632384	2461.448200	21.733325
78.553547	2455.975182	21.738343
78.717542	2468.078417	21.743360
78.670714	2472.128707	21.748378
78.731821	2481.997757	21.753395
78.953963	2474.009491	21.758413
78.969877	2476.781193	21.763431
79.190399	2477.377831	21.768448
79.273356	2484.380857	21.773466
79.352767	2494.414321	21.778483
79.433829	2494.092284	21.783501
79.368289	2507.131003	21.788519
79.600101	2503.534538	21.793536
80.010181	2497.211656	21.798554
79.823458	2498.001501	21.803571
79.898026	2503.825458	21.808589
79.631949	2513.035658	21.813607
80.003777	2516.089309	21.818624
80.574216	2523.195874	21.823642
80.531846	2525.168745	21.828659
80.588546	2525.895204	21.833677
80.379660	2521.626090	21.838695
80.546394	2516.925705	21.843712
81.012081	2516.546564	21.848730
80.910414	2512.478427	21.853747
80.507584	2518.768544	21.858765
80.750206	2529.256188	21.863783
80.700490	2518.769810	21.868800
80.672215	2517.139329	21.873818
80.663671	2534.193202	21.878835
80.950440	2542.969626	21.883853
80.556736	2548.753343	21.888871
80.810435	2542.644314	21.893888
81.250405	2549.234789	21.898906
81.226785	2559.243401	21.903923
81.476559	2565.049397	21.908941
82.158824	2566.359574	21.913959
81.749784	2564.539409	21.918976
81.652761	2571.706381	21.923994
81.551434	2578.072371	21.929011
81.783365	2564.837029	21.934029
81.973784	2579.041342	21.939047
82.120536	2587.154843	21.944064
81.899543	2583.793423	21.949082
81.829756	2590.148164	21.954099
82.130897	2586.430355	21.959117
82.100898	2592.523215	21.964135
82.087459	2601.409826	21.969152
82.391164	2605.607221	21.974170
82.441604	2621.635656	21.979187
82.851948	2608.170337	21.984205
82.768813	2615.350931	21.989223
82.530099	2613.867033	21.994240
83.083738	2617.816967	21.999258
83.074270	2630.518750	22.004275
83.433686	2623.777683	22.009293
83.332197	2627.688234	22.014311
83.537481	2627.343577	22.019328
83.592976	2624.071390	22.024346
83.524584	2626.562800	22.029363
83.514282	2617.847101	22.034381
83.353229	2626.936751	22.039399
83.664240	2623.580346	22.044416
83.783087	2614.393085	22.049434
83.753113	2626.204889	22.054451
84.031659	2626.637791	22.059469
83.844663	2642.930688	22.064487
84.108627	2650.508245	22.069504
84.359763	2654.666545	22.074522
84.071594	2649.683907	22.079539
84.495622	2646.912616	22.084557
84.377501	2649.238233	22.089575
84.385674	2651.244228	22.094592
84.549148	2652.856624	22.099610
84.622942	2675.411528	22.104627
84.560579	2671.403477	22.109645
85.276635	2673.566843	22.114663
85.180230	2676.927436	22.119680
85.305823	2676.055561	22.124698
84.870698	2677.222039	22.129715
85.033162	2675.722625	22.134733
85.003423	2676.162797	22.139751
85.387396	2682.099301	22.144768
85.429822	2686.792137	22.149786
84.906493	2694.404687	22.154803
85.284833	2702.201058	22.159821
85.588162	2708.229110	22.164839
85.634296	2712.561569	22.169856
86.010233	2721.103179	22.174874
85.872719	2725.442321	22.179891
85.909410	2724.502312	22.184909
85.951577	2715.816218	22.189927
86.210348	2717.751398	22.194944
86.826843	2725.352659	22.199962
86.124902	2727.807629	22.204979
86.496232	2732.739314	22.209997
86.563026	2735.730327	22.215015
86.505575	2746.271423	22.220032
86.975053	2738.553595	22.225050
86.878109	2743.845859	22.230067
86.742564	2754.506505	22.235085
87.121275	2750.662888	22.240103
86.774354	2766.542245	22.245120
87.142512	2756.226973	22.250138
87.658154	2764.364820	22.255155
86.869308	2764.030728	22.260173
87.427110	2761.819197	22.265191
86.952436	2770.453068	22.270208
87.439609	2760.059180	22.275226
87.535553	2795.611037	22.280243
87.755547	2783.602002	22.285261
87.866714	2789.565502	22.290279
87.699798	2787.069833	22.295296
88.161058	2801.566443	22.300314
88.246776	2806.050532	22.305331
88.293236	2811.014200	22.310349
88.602853	2805.972579	22.315367
88.507808	2812.596474	22.320384
88.633444	2809.291171	22.325402
88.587747	2804.232627	22.330419
88.698706	2804.840130	22.335437
88.916980	2798.196860	22.340455
88.752432	2810.632699	22.345472
88.727351	2797.267019	22.350490
89.102123	2809.220683	22.355507
88.899759	2824.597703	22.360525
89.135924	2831.131839	22.365543
89.291907	2826.783394	22.370560
89.280702	2829.063878	22.375578
89.417578	2828.505846	22.380595
89.370586	2831.167522	22.385613
89.425124	2835.583911	22.390631
89.380269	2856.633195	22.395648
89.966187	2851.437807	22.400666
90.164048	2868.948868	22.405683
90.307534	2863.084245	22.410701
90.216346	2866.052688	22.415719
89.867302	2861.581362	22.420736
90.343271	2858.214851	22.425754
89.878180	2869.476372	22.430771
90.145839	2872.461188	22.435789
90.531638	2880.751990	22.440807
90.664589	2889.117129	22.445824
90.977511	2879.612114	22.450842
90.455601	2883.714835	22.455859
90.630242	2887.373871	22.460877
90.839437	2893.334672	22.465895
90.752166	2902.580179	22.470912
91.110179	2909.363531	22.475930
90.960093	2916.390612	22.480947
91.330281	2908.445240	22.485965
91.715432	2902.003033	22.490983
91.362279	2912.798863	22.496000
91.527618	2918.602421	22.501018
91.854313	2926.451169	22.506035
91.971784	2923.873050	22.511053
91.929084	2927.143215	22.516071
91.908829	2936.192024	22.521088
91.898886	2932.529196	22.526106
92.151995	2929.128151	22.531123
92.456646	2949.210643	22.536141
92.652253	2951.992139	22.541159
92.593554	2959.680347	22.546176
92.450061	2950.524548	22.551194
92.281422	2954.246848	22.556211
92.592508	2954.191762	22.561229
92.689258	2952.434342	22.566247
93.091164	2979.622031	22.571264
93.027870	2981.531949	22.576282
92.716919	2975.479678	22.581299
93.005953	2984.252808	22.586317
93.315422	2978.668295	22.591335
92.974019	2981.776957	22.596352
93.368741	2993.828617	22.601370
93.181881	2995.723178	22.606387
93.555762	3004.558774	22.611405
93.787085	2995.773473	22.616423
93.652679	3008.851750	22.621440
93.910856	3015.202600	22.626458
94.233624	3023.216128	22.631475
94.284953	3024.003417	22.636493
94.418841	3019.169174	22.641511
94.159891	3026.484788	22.646528
94.462920	3020.099593	22.651546
94.462287	3028.387882	22.656563
94.223086	3028.703069	22.661581
94.902517	3027.649721	22.666599
94.978249	3047.405222	22.671616
95.156038	3049.482532	22.676634
94.839679	3059.370005	22.681651
95.025733	3042.776967	22.686669
95.434816	3042.791746	22.691687
95.431744	3040.137810	22.696704
94.848738	3035.134975	22.701722
95.154164	3039.780386	22.706739
94.983606	3041.991176	22.711757
95.676449	3048.539061	22.716775
95.227215	3068.682987	22.721792
95.814055	3067.451613	22.726810
95.564733	3075.176047	22.731827
95.741728	3076.704301	22.736845
96.068499	3076.933973	22.741863
96.175376	3085.928221	22.746880
96.069692	3082.820077	22.751898
96.069426	3086.099404	22.756915
96.094054	3081.067639	22.761933
96.558372	3099.111610	22.766951
96.589709	3107.600082	22.771968
96.458043	3114.551761	22.776986
96.730983	3109.130743	22.782003
96.753308	3119.609059	22.787021
97.242522	3128.486615	22.792039
97.451279	3139.614324	22.797056
97.383604	3139.807953	22.802074
97.397849	3146.348566	22.807091
97.703323	3140.859317	22.812109
97.687716	3137.617114	22.817127
97.545118	3139.277506	22.822144
98.038272	3130.659431	22.827162
97.741530	3131.447601	22.832179
98.063537	3132.444987	22.837197
98.064628	3135.149674	22.842215
97.734000	3150.045225	22.847232
98.076183	3158.582864	22.852250
98.064031	3152.067096	22.857267
98.452652	3161.588520	22.862285
98.450587	3161.197433	22.867303
98.526728	3176.931962	22.872320
98.407622	3184.203636	22.877338
98.516768	3181.178599	22.882355
98.605286	3189.052152	22.887373
99.063867	3188.863489	22.892391
98.897735	3200.602313	22.897408
98.996337	3209.471669	22.902426
99.684777	3207.324838	22.907443
99.163315	3202.145033	22.912461
99.411320	3202.342860	22.917479
99.548312	3220.169955	22.922496
99.555200	3221.541809	22.927514
100.008947	3226.321844	22.932531
99.547715	3238.798145	22.937549
99.993747	3228.435686	22.942567
100.244118	3231.173927	22.947584
100.414710	3246.584406	22.952602
100.411672	3244.930968	22.957619
100.334360	3252.852623	22.962637
100.642007	3246.444531	22.967655
100.638777	3247.312971	22.972672
100.903518	3250.389839	22.977690
100.757121	3244.037102	22.982707
100.908498	3250.414237	22.987725
100.867942	3252.812998	22.992743
100.934752	3274.811089	22.997760
100.977567	3278.733890	23.002778
101.477214	3270.401952	23.007795
101.394362	3272.939905	23.012813
101.367637	3269.910889	23.017831
101.518040	3281.445518	23.022848
101.709508	3289.744862	23.027866
101.959983	3295.913956	23.032883
101.636157	3299.758484	23.037901
101.972468	3298.673660	23.042919
101.958621	3304.312883	23.047936
101.885263	3310.952500	23.052954
101.925128	3306.663164	23.057971
102.265558	3323.641015	23.062989
102.243589	3322.217787	23.068007
102.276187	3328.402089	23.073024
101.932654	3328.257029	23.078042
102.757145	3342.242667	23.083059
102.754035	3350.995464	23.088077
102.748942	3341.265435	23.093095
102.737681	3345.367162	23.098112
102.937895	3366.751085	23.103130
103.534801	3382.852396	23.108147
103.248001	3379.135008	23.113165
103.735882	3381.305807	23.118183
103.646583	3372.573712	23.123200
103.628060	3374.094748	23.128218
103.763465	3384.839567	23.133235
104.015469	3403.349517	23.138253
104.149008	3388.108968	23.143271
104.449372	3396.066203	23.148288
104.231508	3401.147196	23.153306
104.563737	3391.345354	23.158323
104.281999	3399.734667	23.163341
104.619649	3406.032174	23.168359
104.911885	3415.493083	23.173376
104.565750	3413.915476	23.178394
105.059233	3410.659747	23.183411
105.037263	3414.157160	23.188429
104.989723	3405.292257	23.193447
105.336457	3410.742458	23.198464
105.231073	3422.632879	23.203482
105.619263	3429.626328	23.208499
105.307874	3437.234388	23.213517
105.730070	3436.511699	23.218535
105.658123	3437.974828	23.223552
105.513687	3449.928198	23.228570
106.111860	3452.179571	23.233587
106.367060	3462.167096	23.238605
106.376634	3459.021891	23.243623
106.263362	3464.452645	23.248640
106.189676	3476.448606	23.253658
106.391913	3470.060106	23.258675
106.220562	3470.629798	23.263693
106.434281	3477.839978	23.268711
106.818616	3486.134447	23.273728
106.586838	3497.015766	23.278746
107.134453	3493.912513	23.283763
106.964056	3490.432525	23.288781
107.167254	3508.637756	23.293799
107.507061	3512.555111	23.298816
107.602597	3521.579760	23.303834
107.962467	3513.168608	23.308851
108.038897	3513.794171	23.313869
107.861706	3519.626337	23.318887
108.243025	3512.789977	23.323904
107.641478	3512.290800	23.328922
107.661608	3514.547523	23.333939
107.917042	3521.290364	23.338957
108.083326	3528.441713	23.343975
108.152847	3531.340899	23.348992
108.357290	3545.133457	23.354010
108.410197	3534.220091	23.359027
108.463717	3557.789293	23.364045
108.494688	3564.876635	23.369063
109.038840	3571.918301	23.374080
108.474161	3568.875670	23.379098
109.222556	3576.459787	23.384115
109.370935	3586.495679	23.389133
109.445498	3587.007910	23.394151
109.579493	3584.973152	23.399168
109.434434	3594.104969	23.404186
109.768486	3587.301238	23.409203
109.453673	3584.639248	23.414221
109.378954	3593.996770	23.419239
109.986168	3604.276418	23.424256
110.002758	3606.129698	23.429274
110.099333	3615.217357	23.434291
109.952568	3615.145625	23.439309
110.308581	3634.340220	23.444327
110.224454	3634.501712	23.449344
110.516625	3642.615000	23.454362
110.601131	3641.844206	23.459379
110.611642	3655.001247	23.464397
110.840420	3669.736987	23.469415
110.809397	3671.026437	23.474432
110.701826	3674.669878	23.479450
111.442045	3686.648935	23.484467
111.442513	3688.245930	23.489485
111.198044	3692.425305	23.494503
111.266397	3690.605981	23.499520
111.608685	3707.536557	23.504538
112.070054	3710.816268	23.509555
111.956766	3714.773090	23.514573
112.154197	3717.368196	23.519591
111.980985	3719.083938	23.524608
112.229280	3730.710832	23.529626
112.307160	3735.281602	23.534643
112.653496	3732.787454	23.539661
112.572089	3744.825834	23.544679
112.771009	3734.394487	23.549696
112.831112	3742.020225	23.554714
113.006144	3750.713743	23.559731
113.130364	3760.750360	23.564749
113.064014	3765.125946	23.569767
113.314693	3767.068822	23.574784
113.332481	3773.369225	23.579802
113.679884	3781.360294	23.584819
113.641837	3789.427537	23.589837
113.883107	3792.441892	23.594855
114.176701	3790.236915	23.599872
113.767525	3796.676814	23.604890
114.007516	3799.470427	23.609907
114.685789	3806.219726	23.614925
114.191655	3810.873818	23.619943
114.779528	3797.859570	23.624960
114.548336	3808.191779	23.629978
114.961609	3812.526954	23.634995
114.782817	3810.001438	23.640013
115.075334	3814.229278	23.645031
115.430936	3828.279286	23.650048
115.162340	3845.422484	23.655066
114.984997	3832.086206	23.660083
115.242199	3834.245857	23.665101
115.572814	3835.620698	23.670119
115.885293	3843.973935	23.675136
115.492221	3857.115442	23.680154
115.673940	3852.226139	23.685171
115.932700	3851.699484	23.690189
115.613631	3847.478879	23.695207
115.656711	3856.865426	23.700224
115.724339	3868.688001	23.705242
115.779044	3875.137318	23.710259
116.413930	3879.081120	23.715277
116.635636	3901.346091	23.720295
117.173330	3898.897694	23.725312
116.694653	3899.995316	23.730330
116.989224	3906.321841	23.735347
116.807630	3902.553141	23.740365
116.882523	3916.953365	23.745383
117.215677	3923.946160	23.750400
117.138097	3930.466723	23.755418
117.467387	3927.441792	23.760435
117.628280	3941.755965	23.765453
117.544494	3948.498453	23.770471
117.762112	3940.027326	23.775488
118.011690	3948.889174	23.780506
118.030279	3954.229975	23.785523
118.613614	3961.647577	23.790541
118.481723	3977.999325	23.795559
118.341433	3972.447096	23.800576
118.452466	3979.569403	23.805594
118.442017	3978.197977	23.810611
118.873225	3983.458361	23.815629
119.033367	3991.579866	23.820647
119.239896	3993.100415	23.825664
119.079477	3999.580322	23.830682
119.141197	4001.410791	23.835699
119.462481	4005.851960	23.840717
119.670152	4023.050120	23.845735
119.635062	4020.495749	23.850752
119.558656	4015.899353	23.855770
119.500520	4023.726805	23.860787
119.918306	4040.655335	23.865805
120.180683	4049.370033	23.870823
120.461348	4047.810956	23.875840
120.561714	4047.403802	23.880858
121.052642	4068.588347	23.885875
120.772953	4071.977912	23.890893
120.653946	4080.733438	23.895911
120.995867	4085.389185	23.900928
121.197023	4092.528982	23.905946
121.006096	4081.757648	23.910963
121.432335	4080.504028	23.915981
121.337694	4102.752523	23.920999
121.606217	4098.323016	23.926016
121.805489	4099.181866	23.931034
121.611659	4104.909508	23.936051
122.274437	4098.653803	23.941069
121.749902	4110.613499	23.946087
122.396888	4113.277113	23.951104
122.240198	4124.481622	23.956122
122.544813	4120.147460	23.961139
122.432533	4115.020070	23.966157
122.218579	4126.994247	23.971175
122.494408	4136.824248	23.976192
122.651091	4151.871535	23.981210
122.359023	4156.705536	23.986227
123.146894	4164.138525	23.991245
122.770374	4174.294854	23.996263
122.960476	4175.748552	24.001280
123.047143	4183.281934	24.006298
123.466643	4196.583617	24.011315
123.727757	4195.646249	24.016333
123.458228	4201.587792	24.021351
123.711610	4212.052636	24.026368
123.789659	4227.629958	24.031386
124.113900	4225.104485	24.036403
124.159272	4226.489325	24.041421
124.254203	4249.358524	24.046439
124.760459	4248.887777	24.051456
124.528430	4248.251772	24.056474
124.624337	4245.648438	24.061491
125.179804	4250.466471	24.066509
124.983667	4254.600524	24.071527
125.182460	4263.265315	24.076544
125.538108	4274.269705	24.081562
125.533218	4275.463568	24.086579
125.514662	4274.052356	24.091597
125.423123	4275.553342	24.096615
125.181047	4282.822626	24.101632
125.949856	4295.473089	24.106650
125.595153	4298.763973	24.111667
126.188581	4301.224526	24.116685
125.991929	4316.434624	24.121703
126.396377	4320.080044	24.126720
126.574164	4324.360700	24.131738
126.903626	4321.878586	24.136755
126.861393	4324.628116	24.141773
126.946795	4338.758731	24.146791
127.349672	4346.406777	24.151808
127.277166	4348.757028	24.156826
127.566094	4350.365705	24.161843
127.492166	4350.213116	24.166861
127.537723	4360.426525	24.171879
127.987447	4369.752786	24.176896
128.100882	4378.285807	24.181914
127.705856	4380.743407	24.186931
127.794387	4377.497293	24.191949
127.894318	4381.389290	24.196967
128.464900	4389.569773	24.201984
128.320874	4400.242184	24.207002
128.093851	4392.152996	24.212019
128.752193	4402.298834	24.217037
128.841538	4428.006789	24.222055
129.179344	4432.581203	24.227072
129.606504	4431.873483	24.232090
129.181839	4442.709831	24.237107
129.577255	4431.928497	24.242125
129.685756	4434.935354	24.247143
129.400388	4455.645400	24.252160
129.667158	4445.550227	24.257178
129.758148	4461.766484	24.262195
129.746273	4455.546912	24.267213
129.842973	4469.751614	24.272231
129.818942	4479.717161	24.277248
130.402097	4478.801925	24.282266
130.560194	4505.575575	24.287283
130.633717	4499.844488	24.292301
130.700398	4501.169194	24.297319
131.123735	4505.335668	24.302336
130.972128	4502.938368	24.307354
130.960612	4530.000613	24.312371
131.230744	4526.230455	24.317389
131.234942	4529.777644	24.322407
131.283275	4537.004688	24.327424
131.758952	4548.545981	24.332442
131.497368	4563.381367	24.337459
131.959814	4559.685236	24.342477
132.668841	4574.128676	24.347495
132.368513	4575.779186	24.352512
132.419704	4573.656284	24.357530
132.146569	4590.207473	24.362547
132.459340	4579.214890	24.367565
132.517395	4588.810954	24.372583
132.960168	4606.717767	24.377600
132.811428	4598.584658	24.382618
132.942809	4607.370652	24.387635
133.167892	4614.797304	24.392653
133.125411	4623.597918	24.397671
133.540893	4637.067848	24.402688
133.867373	4624.539031	24.407706
133.849809	4627.130074	24.412723
133.832064	4629.869500	24.417741
133.774902	4646.219610	24.422759
133.827822	4653.256592	24.427776
134.172738	4648.120553	24.432794
134.212132	4666.172691	24.437811
134.622966	4661.357754	24.442829
134.617357	4669.764364	24.447847
134.644946	4676.353943	24.452864
135.274513	4683.793010	24.457882
135.071190	4693.723634	24.462899
135.139702	4696.307514	24.467917
135.524659	4705.401044	24.472935
135.293727	4701.049639	24.477952
135.575546	4716.257710	24.482970
135.807538	4728.263425	24.487987
135.504851	4730.987534	24.493005
135.734219	4733.912374	24.498023
135.891499	4751.636789	24.503040
136.187463	4747.540573	24.508058
136.077805	4773.718949	24.513075
136.585910	4773.677189	24.518093
136.984909	4776.717504	24.523111
136.321656	4778.194465	24.528128
137.246408	4800.678675	24.533146
137.090147	4802.019391	24.538163
137.401859	4807.488129	24.543181
137.615760	4813.123707	24.548199
137.853160	4822.230944	24.553216
137.818999	4827.649709	24.558234
137.926579	4830.154888	24.563251
138.110339	4823.150129	24.568269
138.278077	4828.303681	24.573287
138.127300	4844.763332	24.578304
138.702831	4850.165500	24.583322
138.708190	4854.384912	24.588339
138.694886	4849.096607	24.593357
138.891788	4859.434943	24.598375
138.768437	4878.355582	24.603392
139.039624	4870.573226	24.608410
138.754012	4877.202476	24.613427
139.252646	4892.480893	24.618445
139.746410	4902.103558	24.623463
139.542355	4902.369075	24.628480
139.810401	4904.719705	24.633498
139.757542	4923.367354	24.638515
140.216985	4926.145702	24.643533
140.523222	4934.664563	24.648551
140.439281	4938.916924	24.653568
140.658221	4937.263277	24.658586
140.828228	4951.567350	24.663603
140.981493	4954.021196	24.668621
141.155769	4957.652302	24.673639
140.665732	4956.753663	24.678656
141.214221	4965.357691	24.683674
141.378718	4982.986504	24.688691
141.190400	4988.770377	24.693709
141.313067	4988.265013	24.698727
141.659902	4997.067946	24.703744
141.984893	5007.859783	24.708762
141.772207	5007.631073	24.713779
141.969922	5014.853843	24.718797
142.213028	5029.882004	24.723815
142.145402	5038.500521	24.728832
142.560696	5042.977724	24.733850
142.756635	5053.540437	24.738867
142.372258	5058.161864	24.743885
143.092378	5058.838153	24.748903
142.724208	5066.758816	24.753920
143.296759	5071.091440	24.758938
143.353828	5086.729603	24.763955
143.381148	5085.093337	24.768973
143.578873	5088.023193	24.773991
143.785653	5100.856970	24.779008
143.977433	5101.991666	24.784026
144.199357	5117.900747	24.789043
144.316228	5119.580643	24.794061
144.655490	5133.703669	24.799079
144.763098	5138.513192	24.804096
144.929581	5128.225020	24.809114
144.608579	5134.187555	24.814131
144.760747	5149.962389	24.819149
145.118279	5158.770038	24.824167
145.162551	5160.653863	24.829184
145.119918	5172.535596	24.834202
145.667174	5180.423374	24.839219
145.403660	5186.891444	24.844237
145.957058	5196.182951	24.849255
146.153451	5212.689555	24.854272
146.081045	5211.403500	24.859290
145.862844	5212.359375	24.864307
146.031609	5241.348368	24.869325
146.508147	5239.480725	24.874343
146.434603	5249.025152	24.879360
146.858510	5266.449455	24.884378
146.756386	5266.430695	24.889395
146.793890	5265.171611	24.894413
147.191816	5275.535509	24.899431
147.569174	5291.748678	24.904448
147.673122	5301.101182	24.909466
147.940619	5316.978044	24.914483
148.135501	5318.974025	24.919501
148.555193	5314.040736	24.924519
147.899368	5322.820982	24.929536
148.674930	5342.254694	24.934554
148.786740	5342.300273	24.939571
148.709242	5346.706394	24.944589
148.939320	5339.261725	24.949607
148.880701	5356.379759	24.954624
149.107593	5369.422068	24.959642
148.869953	5364.124567	24.964659
149.059322	5378.002953	24.969677
149.482474	5388.823832	24.974695
149.563486	5395.503156	24.979712
149.750629	5407.633142	24.984730
150.118614	5417.796630	24.989747
150.031000	5420.405073	24.994765
150.444367	5425.135204	24.999783
150.259050	5447.996151	25.004800
150.579485	5443.978020	25.009818
150.713952	5457.309500	25.014835
150.839197	5463.637847	25.019853
151.152392	5463.834962	25.024871
151.060994	5475.721376	25.029888
151.604158	5478.142620	25.034906
151.000296	5494.399209	25.039923
151.387484	5494.603673	25.044941
151.553174	5500.455356	25.049959
152.008962	5514.664592	25.054976
151.935519	5518.656598	25.059994
152.156317	5525.074165	25.065011
152.165169	5547.544959	25.070029
152.580293	5544.708345	25.075047
152.510808	5551.262942	25.080064
152.831835	5561.680087	25.085082
153.173507	5568.233409	25.090099
153.468027	5574.992991	25.095117
153.830241	5568.695493	25.100135
153.695972	5566.873003	25.105152
153.621408	5578.024501	25.110170
153.756432	5591.958914	25.115187
153.697396	5601.141392	25.120205
154.147081	5592.064944	25.125223
154.144852	5607.611830	25.130240
154.615351	5625.777308	25.135258
154.696799	5628.596045	25.140275
154.303209	5629.781444	25.145293
154.807207	5645.321658	25.150311
155.078720	5654.042010	25.155328
155.073915	5660.412896	25.160346
155.341519	5666.258136	25.165363
155.398685	5685.347044	25.170381
155.684267	5680.046397	25.175399
155.546596	5689.089718	25.180416
155.302798	5704.005315	25.185434
156.111919	5703.648081	25.190451
155.752058	5729.759697	25.195469
156.303705	5737.056730	25.200487
156.345335	5738.884208	25.205504
156.564440	5760.245894	25.210522
157.120020	5774.010389	25.215539
156.955447	5778.682790	25.220557
157.166410	5785.534458	25.225575
157.156638	5795.422729	25.230592
157.388324	5796.544905	25.235610
158.018326	5807.330470	25.240627
157.974076	5811.103310	25.245645
158.266233	5810.198881	25.250663
158.378695	5811.945822	25.255680
158.195317	5826.852053	25.260698
158.485301	5828.369155	25.265715
158.589111	5848.489481	25.270733
158.705487	5846.258362	25.275751
158.815568	5853.624619	25.280768
159.036875	5871.873576	25.285786
159.342679	5878.110645	25.290803
159.432018	5894.025391	25.295821
159.783933	5884.822064	25.300839
160.118409	5896.812495	25.305856
159.827556	5901.668860	25.310874
160.518316	5904.306951	25.315891
160.315248	5918.594468	25.320909
160.360655	5919.070296	25.325927
160.652638	5930.284540	25.330944
161.039072	5943.801028	25.335962
161.168005	5939.986411	25.340979
160.876317	5943.943252	25.345997
161.254689	5948.347547	25.351015
161.078970	5969.316763	25.356032
161.580588	5980.242500	25.361050
161.705496	5970.149772	25.366067
161.829250	5995.513619	25.371085
162.016946	5992.447401	25.376103
162.371867	5999.699599	25.381120
162.224215	6001.105344	25.386138
162.441767	6020.242079	25.391155
162.420128	6025.204668	25.396173
162.611707	6023.141679	25.401191
162.998078	6038.075622	25.406208
162.889028	6049.324355	25.411226
162.914469	6043.751841	25.416243
162.564843	6067.333785	25.421261
163.647746	6071.065835	25.426279
163.576567	6081.857240	25.431296
163.435531	6092.912135	25.436314
163.762060	6101.987109	25.441331
163.793024	6120.446069	25.446349
164.172158	6133.389312	25.451367
164.444114	6146.813398	25.456384
164.395002	6151.540411	25.461402
164.733716	6153.144610	25.466419
164.969176	6178.604854	25.471437
165.265211	6180.231525	25.476455
165.441565	6182.959717	25.481472
165.436831	6197.743559	25.486490
165.705162	6200.024866	25.491507
165.776926	6213.881274	25.496525
165.754796	6221.322058	25.501543
166.302557	6238.800493	25.506560
166.296176	6237.200972	25.511578
166.699739	6244.287808	25.516595
166.837051	6264.144487	25.521613
166.897675	6257.505719	25.526631
166.943396	6266.769979	25.531648
166.926432	6269.651584	25.536666
167.614026	6290.438566	25.541683
167.053901	6302.960854	25.546701
167.540293	6317.850946	25.551719
167.791427	6307.053236	25.556736
167.909799	6325.438729	25.561754
168.148888	6336.806721	25.566771
168.637579	6344.536872	25.571789
168.719046	6349.682273	25.576807
169.126189	6359.458182	25.581824
169.112436	6377.949660	25.586842
169.343292	6373.276121	25.591859
169.348262	6371.857904	25.596877
169.263088	6385.824262	25.601895
169.788653	6397.668284	25.606912
169.739649	6403.673850	25.611930
170.105161	6416.508940	25.616947
170.103389	6427.719000	25.621965
170.279866	6415.667042	25.626983
170.631986	6437.106540	25.632000
170.423801	6448.345793	25.637018
170.799899	6457.763585	25.642035
170.835242	6462.546897	25.647053
170.917889	6477.954952	25.652071
171.324742	6478.481502	25.657088
171.724060	6499.427529	25.662106
171.803201	6504.522829	25.667123
171.613586	6518.401474	25.672141
171.718586	6522.896089	25.677159
171.829248	6537.671597	25.682176
172.173099	6545.285625	25.687194
172.565036	6557.254860	25.692212
172.626963	6571.968580	25.697229
172.710668	6575.636297	25.702247
173.272955	6589.984373	25.707264
173.152001	6596.582131	25.712282
173.286227	6594.818493	25.717300
173.651198	6614.952413	25.722317
173.635093	6616.972121	25.727335
173.925942	6616.377230	25.732352
173.935074	6641.715731	25.737370
174.010535	6647.755544	25.742388
174.252408	6656.992428	25.747405
174.624944	6676.544371	25.752423
174.752043	6671.924894	25.757440
174.721985	6677.681347	25.762458
174.864066	6680.313963	25.767476
175.291536	6698.228388	25.772493
175.116415	6706.640392	25.777511
175.791335	6714.764545	25.782528
175.609269	6725.943051	25.787546
175.990610	6728.746545	25.792564
176.255378	6728.345148	25.797581
176.247700	6749.017437	25.802599
176.206353	6749.970937	25.807616
176.515686	6763.537994	25.812634
177.173346	6769.401403	25.817652
176.795551	6780.825273	25.822669
177.014231	6791.110782	25.827687
177.092264	6801.636155	25.832704
176.861029	6813.400125	25.837722
177.538976	6820.829339	25.842740
177.619493	6832.162500	25.847757
177.635999	6851.306344	25.852775
177.904725	6860.535968	25.857792
177.905556	6878.091227	25.862810
178.451418	6882.971456	25.867828
178.723259	6896.452934	25.872845
178.838620	6908.468885	25.877863
179.036806	6910.979097	25.882880
179.034605	6938.876864	25.887898
179.313469	6946.015078	25.892916
179.876284	6958.705991	25.897933
179.743703	6975.717159	25.902951
180.158794	6973.922113	25.907968
180.341300	6980.415644	25.912986
180.428478	6994.898450	25.918004
180.588033	7004.303094	25.923021
180.683620	7013.945061	25.928039
181.157434	7011.070620	25.933056
181.295794	7025.646453	25.938074
181.560891	7031.448328	25.943092
181.917349	7038.909055	25.948109
182.054011	7056.455833	25.953127
182.212873	7055.269164	25.958144
182.227640	7059.711752	25.963162
182.113540	7071.842680	25.968180
182.333249	7083.504607	25.973197
182.477348	7089.385437	25.978215
182.580712	7100.374237	25.983232
182.613491	7115.639106	25.988250
183.285155	7119.631536	25.993268
183.344347	7134.260898	25.998285
183.419538	7147.694445	26.003303
183.865499	7162.465282	26.008320
183.816292	7169.939103	26.013338
183.916037	7166.990649	26.018356
184.363791	7183.096604	26.023373
184.404355	7200.759596	26.028391
184.373210	7198.418833	26.033408
184.412530	7218.355034	26.038426
184.758517	7222.382723	26.043444
185.155134	7239.377526	26.048461
185.556083	7256.908347	26.053479
185.470162	7251.820142	26.058496
185.497195	7270.448190	26.063514
185.722478	7280.382517	26.068532
186.006185	7299.885901	26.073549
186.138349	7309.108732	26.078567
186.425603	7310.181258	26.083584
186.682853	7330.837952	26.088602
186.746697	7337.448065	26.093620
187.087555	7339.765509	26.098637
186.991512	7346.792137	26.103655
187.640573	7354.740681	26.108672
187.737792	7364.120548	26.113690
187.808766	7368.238707	26.118708
187.792592	7369.324045	26.123725
188.071954	7387.896897	26.128743
188.289523	7381.608817	26.133760
188.085719	7410.356536	26.138778
188.488259	7421.295502	26.143796
188.967390	7423.225086	26.148813
188.887460	7440.591487	26.153831
188.884550	7449.374629	26.158848
189.072208	7469.966614	26.163866
189.380113	7476.806886	26.168884
189.736360	7493.918744	26.173901
189.435807	7505.678228	26.178919
190.175084	7512.892914	26.183936
190.491316	7530.677200	26.188954
190.155080	7539.146392	26.193972
190.564847	7534.997008	26.198989
190.650488	7546.361376	26.204007
191.050823	7578.405329	26.209024
190.945984	7589.543847	26.214042
191.316847	7600.958276	26.219060
191.558461	7615.464731	26.224077
191.531759	7618.354386	26.229095
192.019244	7639.316315	26.234112
192.265817	7649.468497	26.239130
192.204924	7664.694826	26.244148
192.662058	7674.274186	26.249165
192.390483	7692.668465	26.254183
192.835840	7694.571800	26.259200
193.712710	7714.124764	26.264218
193.401082	7725.346271	26.269236
194.357011	7724.975488	26.274253
194.130182	7729.171952	26.279271
194.575272	7747.873899	26.284288
194.650088	7757.146979	26.289306
194.380094	7749.912276	26.294324
194.979109	7756.823858	26.299341
194.881824	7776.166440	26.304359
195.279284	7782.105669	26.309376
195.031824	7780.714261	26.314394
195.198083	7804.757459	26.319412
195.541706	7804.356317	26.324429
195.520443	7836.795099	26.329447
195.930558	7838.606102	26.334464
196.026091	7855.860164	26.339482
196.209837	7862.044422	26.344500
196.752342	7869.466870	26.349517
196.732253	7895.493596	26.354535
196.539666	7895.160669	26.359552
196.769321	7910.711060	26.364570
197.146551	7927.810562	26.369588
197.596161	7938.985556	26.374605
197.729080	7952.918933	26.379623
197.795927	7960.378050	26.384640
198.011153	7977.619790	26.389658
198.026577	7995.940995	26.394676
198.402465	8000.971280	26.399693
198.641887	8019.238475	26.404711
199.265243	8027.551246	26.409728
199.179112	8038.699732	26.414746
199.329311	8052.943029	26.419764
199.504225	8063.321347	26.424781
199.823653	8068.543606	26.429799
199.954893	8077.921664	26.434816
200.467837	8082.665304	26.439834
200.210152	8085.237623	26.444852
200.524533	8085.579816	26.449869
200.289046	8108.145686	26.454887
200.626146	8109.257808	26.459904
201.010022	8132.550681	26.464922
200.674614	8138.898445	26.469940
201.682724	8146.974199	26.474957
201.679188	8168.774515	26.479975
201.671708	8181.991297	26.484992
201.963262	8193.980484	26.490010
202.051024	8203.466444	26.495028
202.756313	8218.001762	26.500045
202.377601	8226.667348	26.505063
203.001432	8236.192472	26.510080
202.953176	8251.597260	26.515098
202.992902	8262.388352	26.520116
203.521243	8283.843439	26.525133
203.744173	8286.763548	26.530151
203.905472	8305.340034	26.535168
204.456185	8308.799180	26.540186
204.152318	8324.572413	26.545204
204.597197	8335.189577	26.550221
204.941160	8348.474550	26.555239
204.914479	8357.950103	26.560256
205.121340	8368.408831	26.565274
205.160155	8375.673607	26.570292
205.455131	8387.675012	26.575309
205.599030	8412.603346	26.580327
205.344327	8420.536080	26.585344
206.151487	8431.592217	26.590362
206.172772	8458.301511	26.595380
206.598818	8460.599440	26.600397
206.864791	8480.552010	26.605415
206.841712	8483.892706	26.610432
206.992056	8494.221444	26.615450
207.656399	8508.753935	26.620468
208.192820	8527.767553	26.625485
207.934410	8533.266740	26.630503
208.252971	8537.469504	26.635520
208.645115	8548.322368	26.640538
208.819048	8567.740103	26.645556
209.040092	8560.323969	26.650573
208.792310	8570.449917	26.655591
209.419739	8576.246033	26.660608
209.675997	8580.553282	26.665626
209.637434	8611.010268	26.670644
210.029116	8617.872570	26.675661
210.054575	8621.474047	26.680679
210.059797	8636.883406	26.685696
210.553832	8643.559195	26.690714
210.463861	8657.673251	26.695732
210.874684	8673.533721	26.700749
210.804847	8681.822783	26.705767
210.659457	8703.017668	26.710784
211.062743	8708.924713	26.715802
211.266463	8733.379999	26.720820
211.660415	8751.112242	26.725837
211.700811	8772.120241	26.730855
212.201403	8781.734414	26.735872
212.306187	8794.839329	26.740890
212.505144	8809.141872	26.745908
212.461677	8824.375895	26.750925
212.928761	8837.474599	26.755943
213.139111	8843.967583	26.760960
213.474031	8865.744111	26.765978
213.936312	8874.546614	26.770996
213.928505	8886.706279	26.776013
213.989464	8891.618811	26.781031
213.952991	8909.551239	26.786048
214.814871	8912.005113	26.791066
214.683527	8941.470018	26.796084
214.895066	8948.584827	26.801101
215.201941	8956.073045	26.806119
215.140440	8975.070289	26.811136
215.772184	8981.478364	26.816154
216.083471	8995.334067	26.821172
215.877825	8998.829746	26.826189
216.295225	9013.543397	26.831207
216.097098	9030.882445	26.836224
216.627786	9035.310986	26.841242
216.335143	9052.560672	26.846260
216.845239	9075.282438	26.851277
217.390095	9088.391238	26.856295
217.186514	9103.372734	26.861312
217.363525	9106.167562	26.866330
217.689644	9132.511187	26.871348
217.750846	9154.056251	26.876365
218.278077	9163.912718	26.881383
218.378516	9192.988096	26.886400
218.603389	9196.548973	26.891418
218.660998	9224.210333	26.896436
218.955409	9229.683110	26.901453
219.489331	9246.487759	26.906471
219.863317	9273.165072	26.911488
220.018223	9277.387329	26.916506
220.133665	9287.797751	26.921524
220.456761	9303.937718	26.926541
220.531995	9320.741673	26.931559
220.761763	9337.622468	26.936576
221.091266	9342.448848	26.941594
221.204676	9365.697238	26.946612
221.362690	9373.332080	26.951629
221.928048	9390.605532	26.956647
221.787186	9397.807293	26.961664
222.116997	9408.439944	26.966682
222.137237	9434.891904	26.971700
222.450000	9447.317448	26.976717
222.858515	9461.003560	26.981735
223.036904	9477.526281	26.986752
223.199309	9488.579869	26.991770
223.254090	9507.351055	26.996788
223.707723	9526.653357	27.001805
223.933034	9532.560132	27.006823
224.013975	9552.928036	27.011840
224.458214	9565.775091	27.016858
224.740066	9582.262753	27.021876
224.755150	9601.270739	27.026893
225.283878	9608.386630	27.031911
225.335398	9633.040598	27.036928
225.922014	9637.561559	27.041946
225.755907	9652.458691	27.046964
225.835638	9662.625486	27.051981
226.236020	9678.898910	27.056999
226.428465	9695.558547	27.062016
226.755791	9714.388282	27.067034
226.925480	9713.446026	27.072052
227.551621	9734.347564	27.077069
227.604570	9746.946620	27.082087
227.723705	9758.966988	27.087104
227.805338	9765.117361	27.092122
227.930545	9781.254011	27.097140
228.363394	9800.853490	27.102157
228.690955	9802.102982	27.107175
228.444953	9819.743898	27.112192
228.876403	9825.883694	27.117210
229.371037	9838.520970	27.122228
229.477574	9863.330807	27.127245
229.600496	9867.564523	27.132263
229.686485	9889.823283	27.137280
230.378261	9884.312571	27.142298
230.475072	9906.323379	27.147316
230.189039	9921.009021	27.152333
230.772270	9931.902225	27.157351
231.360306	9943.672442	27.162368
231.548414	9951.258604	27.167386
231.647063	9956.544402	27.172404
231.255251	9968.828078	27.177421
231.553087	9983.324423	27.182439
231.619911	10015.244864	27.187456
231.832166	10017.756456	27.192474
231.885511	10041.333997	27.197492
232.323498	10064.368225	27.202509
233.044031	10081.169657	27.207527
233.339030	10106.051331	27.212544
233.429535	10127.198250	27.217562
233.556784	10149.956046	27.222580
233.783011	10160.046487	27.227597
234.098310	10174.925454	27.232615
233.965508	10186.101480	27.237632
234.600187	10201.530350	27.242650
234.862550	10221.940028	27.247668
235.124183	10251.939041	27.252685
235.668753	10256.526734	27.257703
235.820991	10270.604067	27.262720
235.901788	10279.290182	27.267738
236.072922	10294.946463	27.272756
236.031098	10316.085908	27.277773
236.677466	10325.693836	27.282791
236.753681	10342.261747	27.287808
236.822414	10358.600349	27.292826
237.508998	10371.015312	27.297844
237.226514	10391.418961	27.302861
237.942897	10405.215413	27.307879
238.031739	10422.419229	27.312896
238.220463	10447.617968	27.317914
238.882603	10452.443049	27.322932
238.505967	10464.086857	27.327949
239.446920	10483.212771	27.332967
239.222790	10502.871703	27.337984
239.598648	10507.700599	27.343002
239.802526	10524.416020	27.348020
240.138163	10539.295249	27.353037
240.670028	10559.265231	27.358055
240.343392	10571.466467	27.363072
240.937459	10584.072886	27.368090
240.886301	10594.352261	27.373108
241.092763	10613.820712	27.378125
241.026177	10623.502591	27.383143
241.160068	10649.035416	27.388160
241.852271	10669.286678	27.393178
242.440350	10688.316520	27.398196
242.267424	10705.053240	27.403213
242.647190	10712.777037	27.408231
242.900880	10737.716544	27.413248
243.091098	10746.669914	27.418266
243.362639	10768.218623	27.423284
243.194189	10779.640560	27.428301
244.073955	10793.234883	27.433319
243.631952	10811.062156	27.438336
244.229555	10825.177495	27.443354
244.775609	10836.907493	27.448372
244.656997	10857.990112	27.453389
244.812868	10867.384663	27.458407
244.616242	10878.668984	27.463424
244.712491	10897.753984	27.468442
245.264015	10916.091963	27.473460
245.120364	10935.685061	27.478477
246.236082	10962.040196	27.483495
246.512523	10978.719395	27.488512
246.691912	10993.077201	27.493530
246.753096	11015.107524	27.498548
246.977317	11029.669893	27.503565
247.185256	11043.202291	27.508583
247.468544	11060.313080	27.513600
247.886758	11078.463701	27.518618
248.312362	11102.161087	27.523636
248.181791	11109.497670	27.528653
248.822124	11120.992045	27.533671
249.131594	11146.725389	27.538688
249.041871	11156.670091	27.543706
249.843208	11176.967961	27.548724
249.640910	11194.022321	27.553741
250.291297	11203.604813	27.558759
250.506106	11219.453955	27.563776
250.418703	11231.605511	27.568794
250.933748	11244.619460	27.573812
250.798122	11268.695477	27.578829
251.266618	11278.306502	27.583847
251.398839	11293.072945	27.588864
251.691097	11311.515080	27.593882
251.849177	11322.924087	27.598900
252.103793	11349.888309	27.603917
252.341240	11367.113919	27.608935
252.603038	11372.440871	27.613952
252.873280	11396.188228	27.618970
253.078351	11411.404369	27.623988
253.368891	11445.698332	27.629005
253.619947	11455.608755	27.634023
253.971418	11471.607215	27.639040
254.185700	11489.161805	27.644058
254.272791	11503.464991	27.649076
254.474257	11532.528179	27.654093
254.915465	11539.386964	27.659111
255.245957	11568.461572	27.664128
255.399828	11586.581469	27.669146
255.597653	11597.681278	27.674164
255.871575	11623.919760	27.679181
256.075069	11639.729979	27.684199
256.260193	11660.611189	27.689216
256.366922	11685.710759	27.694234
256.266220	11704.341145	27.699252
257.050017	11728.112676	27.704269
257.495669	11747.064862	27.709287
257.754297	11770.302962	27.714304
258.129391	11795.777456	27.719322
258.854241	11806.498004	27.724340
258.455068	11832.109627	27.729357
258.887586	11848.664102	27.734375
259.329807	11853.517688	27.739392
259.476928	11865.885532	27.744410
259.624130	11884.726723	27.749428
259.840805	11895.580610	27.754445
260.148335	11911.538963	27.759463
260.541267	11931.734269	27.764480
260.874639	11959.350153	27.769498
261.067561	11964.002833	27.774516
260.891985	11990.716432	27.779533
261.489505	11993.767913	27.784551
261.668056	12016.036800	27.789568
261.727453	12032.450949	27.794586
261.957573	12059.432657	27.799604
262.294633	12076.254908	27.804621
262.327150	12082.233743	27.809639
262.636233	12105.578033	27.814656
262.958351	12138.163115	27.819674
263.468863	12145.974388	27.824692
263.644456	12163.892498	27.829709
263.708938	12185.333169	27.834727
264.161884	12197.861737	27.839744
264.435840	12230.265056	27.844762
264.950611	12235.773670	27.849780
265.046889	12258.677817	27.854797
265.329828	12273.759304	27.859815
265.724100	12293.436909	27.864832
265.685594	12304.078383	27.869850
266.300594	12318.852106	27.874868
266.159242	12346.227143	27.879885
266.568062	12368.056174	27.884903
266.942486	12378.430903	27.889920
266.696514	12398.268911	27.894938
267.459910	12415.852028	27.899956
267.765849	12437.583575	27.904973
267.717947	12452.679138	27.909991
268.436859	12475.135492	27.915008
268.146603	12493.445831	27.920026
268.823146	12523.819257	27.925044
268.845939	12544.325830	27.930061
268.628772	12558.551165	27.935079
269.638618	12587.644081	27.940096
269.366825	12611.181042	27.945114
269.958082	12630.878667	27.950132
270.326928	12666.975196	27.955149
270.417363	12677.602996	27.960167
271.085740	12695.005471	27.965184
271.297351	12718.157369	27.970202
271.449475	12734.450234	27.975220
271.671188	12759.223747	27.980237
272.026883	12774.335289	27.985255
272.299763	12794.364011	27.990272
272.614939	12816.685072	27.995290
272.709550	12826.238619	28.000308
272.841014	12858.172705	28.005325
273.474094	12874.282981	28.010343
273.874229	12895.539245	28.015360
274.044689	12913.256764	28.020378
274.240682	12932.767149	28.025396
274.605448	12953.286911	28.030413
274.992154	12977.223280	28.035431
275.369193	12997.381164	28.040448
274.933589	13014.037919	28.045466
275.428931	13035.348901	28.050484
275.618777	13062.448877	28.055501
275.522924	13088.911533	28.060519
276.279974	13103.849940	28.065536
276.759615	13130.462506	28.070554
277.380486	13151.542373	28.075572
277.546256	13177.149419	28.080589
277.229522	13188.466563	28.085607
277.647184	13212.562594	28.090624
278.106429	13234.820526	28.095642
278.552006	13259.376463	28.100660
278.827956	13274.781956	28.105677
279.213503	13291.209266	28.110695
279.214388	13303.531484	28.115712
279.430669	13326.563390	28.120730
279.877744	13350.484459	28.125748
279.852321	13364.272981	28.130765
280.163233	13378.883588	28.135783
280.506756	13393.334356	28.140800
280.397597	13423.718622	28.145818
280.736145	13437.630187	28.150836
281.179671	13459.240299	28.155853
281.442748	13485.416747	28.160871
282.215449	13504.414208	28.165888
282.197547	13533.123244	28.170906
282.282921	13543.183881	28.175924
282.557372	13570.587131	28.180941
283.109966	13589.151771	28.185959
283.465842	13602.662833	28.190976
283.262341	13628.899936	28.195994
283.536207	13651.484251	28.201012
283.692725	13673.347996	28.206029
284.249107	13701.679945	28.211047
284.217414	13720.945742	28.216064
284.662810	13758.949289	28.221082
285.449099	13779.902886	28.226100
285.543831	13800.143745	28.231117
285.464675	13828.300688	28.236135
285.810092	13844.760028	28.241152
285.966358	13867.347231	28.246170
286.505500	13892.290406	28.251188
286.680577	13916.207425	28.256205
287.261117	13945.038086	28.261223
287.637943	13967.385582	28.266240
287.792058	13990.854373	28.271258
287.980799	14013.983012	28.276276
288.470275	14031.474748	28.281293
288.101178	14062.301829	28.286311
288.863210	14084.285944	28.291328
289.098300	14122.158940	28.296346
289.568349	14150.688252	28.301364
290.050793	14170.480323	28.306381
290.134574	14193.151904	28.311399
290.671879	14211.735339	28.316416
290.632365	14229.306965	28.321434
291.052364	14261.848785	28.326452
291.259264	14277.559615	28.331469
291.485705	14310.693986	28.336487
292.036828	14327.544711	28.341504
292.405792	14360.072586	28.346522
292.649223	14375.067192	28.351540
292.987654	14396.107418	28.356557
293.001054	14420.214620	28.361575
293.773550	14439.288847	28.366592
293.721137	14460.826195	28.371610
293.658069	14486.338208	28.376628
294.643209	14504.760191	28.381645
294.218412	14533.101802	28.386663
294.914785	14553.757681	28.391680
295.316406	14584.120631	28.396698
295.406565	14600.462701	28.401716
295.968601	14624.620021	28.406733
296.066874	14663.901969	28.411751
296.328772	14677.501156	28.416768
296.437944	14709.966103	28.421786
296.627921	14723.794505	28.426804
297.188546	14745.643551	28.431821
297.264693	14787.657912	28.436839
297.937676	14803.321430	28.441856
298.394690	14823.936142	28.446874
298.261979	14848.110987	28.451892
299.016716	14862.725850	28.456909
299.070770	14884.502813	28.461927
299.543445	14899.698789	28.466944
299.786783	14925.599226	28.471962
299.895409	14941.824999	28.476980
300.244925	14966.834027	28.481997
300.230463	14988.662899	28.487015
300.716748	15000.616460	28.492032
301.121246	15035.098035	28.497050
301.300969	15068.373686	28.502068
301.747191	15085.544708	28.507085
301.947788	15109.392902	28.512103
302.350923	15128.841508	28.517120
302.710178	15147.011590	28.522138
302.584446	15178.841417	28.527156
303.225164	15199.999407	28.532173
303.462746	15220.727879	28.537191
303.961164	15245.461284	28.542208
303.878709	15271.855385	28.547226
303.924402	15293.877312	28.552244
304.651320	15317.087458	28.557261
304.612550	15346.863678	28.562279
305.056303	15376.267477	28.567296
305.159079	15400.134514	28.572314
305.630179	15443.339138	28.577332
305.993019	15464.626225	28.582349
306.433388	15497.166959	28.587367
306.668421	15516.793892	28.592384
307.196730	15537.840374	28.597402
307.550050	15565.117276	28.602420
308.079196	15592.628817	28.607437
308.055746	15625.157149	28.612455
308.231228	15641.884695	28.617472
308.700255	15672.557808	28.622490
308.887917	15695.963429	28.627508
309.490234	15718.839844	28.632525
309.825406	15743.893193	28.637543
310.053940	15763.897244	28.642560
310.432081	15794.199466	28.647578
310.574704	15813.080009	28.652596
310.750339	15831.434264	28.657613
310.838027	15862.792777	28.662631
311.552677	15889.189199	28.667648
311.932991	15916.433946	28.672666
311.567626	15946.129602	28.677684
312.330765	15970.588754	28.682701
312.731481	16006.907706	28.687719
313.167401	16029.327320	28.692736
313.471101	16056.334752	28.697754
313.523784	16085.788265	28.702772
314.254632	16125.185731	28.707789
314.274796	16135.769614	28.712807
314.578983	16152.818556	28.717824
315.190547	16185.062014	28.722842
315.360627	16220.529975	28.727860
315.665305	16231.246217	28.732877
315.982641	16260.958594	28.737895
316.302395	16282.622879	28.742912
316.476013	16315.298380	28.747930
316.709994	16343.905846	28.752948
316.885308	16366.338250	28.757965
317.138216	16394.980728	28.762983
317.912543	16432.429548	28.768000
318.689114	16461.542832	28.773018
318.219723	16490.134355	28.778036
318.897024	16510.372100	28.783053
319.352010	16536.645847	28.788071
319.906267	16564.306455	28.793088
320.130749	16584.094057	28.798106
320.000773	16611.119665	28.803124
320.592953	16630.796022	28.808141
320.562038	16654.278108	28.813159
320.814423	16676.269240	28.818176
321.507472	16695.427658	28.823194
321.443914	16728.538987	28.828212
322.035918	16735.732956	28.833229
322.185828	16777.304234	28.838247
322.274553	16799.324301	28.843264
322.767018	16819.155447	28.848282
322.816112	16840.594280	28.853300
323.436610	16873.008054	28.858317
323.651182	16901.493045	28.863335
323.607722	16926.089240	28.868352
324.094792	16949.866416	28.873370
324.418272	16986.158252	28.878388
324.936378	17011.017191	28.883405
325.098933	17043.998884	28.888423
325.702565	17080.404942	28.893440
326.147611	17106.898966	28.898458
326.294973	17141.159277	28.903476
326.607688	17161.097897	28.908493
327.002756	17203.424498	28.913511
327.226048	17228.178284	28.918528
327.782808	17252.166019	28.923546
327.863176	17288.123787	28.928564
328.330321	17307.248711	28.933581
328.950654	17342.597666	28.938599
328.987129	17365.517298	28.943616
329.495848	17387.983946	28.948634
329.736389	17414.636772	28.953652
330.349173	17439.835202	28.958669
330.341028	17475.573443	28.963687
330.504953	17501.973063	28.968704
331.291709	17524.952242	28.973722
331.359312	17563.110951	28.978740
331.786458	17585.186296	28.983757
332.125132	17619.802844	28.988775
332.551410	17648.543213	28.993792
332.795666	17675.480098	28.998810
333.270125	17698.198851	29.003828
333.378890	17721.467671	29.008845
333.630654	17755.441066	29.013863
334.059582	17778.887231	29.018880
334.328132	17808.404315	29.023898
334.818306	17842.302614	29.028916
335.306724	17868.367619	29.033933
335.245689	17894.499775	29.038951
335.694847	17928.657347	29.043968
335.994979	17952.389229	29.048986
336.433242	17988.431218	29.054004
336.637056	18013.631283	29.059021
337.413023	18047.965303	29.064039
337.276363	18079.346760	29.069056
337.912652	18099.115628	29.074074
337.895003	18143.802191	29.079092
338.469641	18165.280199	29.084109
338.744780	18191.909721	29.089127
339.095436	18230.846684	29.094144
339.669904	18248.818567	29.099162
339.492687	18282.316771	29.104180
340.414144	18307.423756	29.109197
340.586914	18336.918743	29.114215
340.914084	18367.817366	29.119232
341.335405	18393.880953	29.124250
341.604927	18428.756163	29.129268
341.900654	18453.822366	29.134285
342.335304	18479.138500	29.139303
342.558267	18512.081637	29.144320
343.145620	18532.136589	29.149338
343.383816	18565.229055	29.154356
343.922209	18585.159060	29.159373
344.268392	18610.583987	29.164391
344.763042	18645.430639	29.169408
344.856630	18658.392487	29.174426
345.115990	18675.921345	29.179444
345.271839	18697.307600	29.184461
345.839775	18720.676269	29.189479
345.591935	18755.184547	29.194496
346.025636	18770.854041	29.199514
346.239272	18810.685474	29.204532
346.682184	18839.620851	29.209549
347.199185	18873.023961	29.214567
347.045151	18900.391362	29.219584
347.627239	18927.795121	29.224602
348.073336	18974.773798	29.229620
348.516770	19000.746285	29.234637
349.189090	19031.598215	29.239655
349.263123	19063.763251	29.244672
349.497578	19094.506969	29.249690
349.777061	19121.901541	29.254708
349.964565	19149.992887	29.259725
350.609444	19186.282717	29.264743
350.742721	19219.209508	29.269760
351.615904	19252.127860	29.274778
352.027240	19293.717273	29.279796
352.078362	19323.536066	29.284813
352.530181	19357.379834	29.289831
352.743734	19387.546038	29.294848
353.153849	19419.804328	29.299866
353.746360	19450.593607	29.304884
354.068157	19484.792814	29.309901
354.558978	19510.651152	29.314919
354.695947	19552.258821	29.319936
355.071667	19573.459963	29.324954
355.677647	19608.366713	29.329972
356.051754	19640.504647	29.334989
356.099535	19657.738993	29.340007
356.251537	19691.977795	29.345024
356.824417	19720.085412	29.350042
357.130239	19765.906490	29.355060
357.761179	19789.873106	29.360077
358.179793	19823.141620	29.365095
358.201427	19850.280653	29.370112
358.728993	19876.108446	29.375130
359.062115	19912.511640	29.380148
359.519541	19949.306108	29.385165
359.803152	19980.466832	29.390183
359.869728	20008.072902	29.395200
360.500962	20033.183352	29.400218
360.736073	20062.216272	29.405236
361.020392	20104.168484	29.410253
361.465750	20135.563163	29.415271
361.607922	20177.480934	29.420288
361.939494	20206.075638	29.425306
362.143972	20250.346810	29.430324
363.038224	20285.557114	29.435341
363.475845	20310.597156	29.440359
363.677418	20349.334238	29.445376
364.011095	20374.795011	29.450394
364.381409	20406.846341	29.455412
364.672949	20444.432231	29.460429
365.387190	20483.411505	29.465447
365.260358	20514.586823	29.470464
365.648724	20542.869843	29.475482
366.412677	20570.860295	29.480500
366.723259	20607.622134	29.485517
366.928873	20636.572067	29.490535
367.361148	20665.044254	29.495552
367.902759	20696.450027	29.500570
368.458057	20729.603893	29.505588
368.403057	20756.926777	29.510605
368.957124	20773.703695	29.515623
368.990951	20809.005487	29.520640
369.700011	20838.255961	29.525658
369.937693	20865.596334	29.530676
370.383414	20896.309785	29.535693
370.617521	20919.885017	29.540711
370.878525	20953.685609	29.545728
370.960485	20990.357605	29.550746
371.201930	21023.024059	29.555764
371.507869	21056.027980	29.560781
372.341543	21084.444219	29.565799
372.427858	21127.826012	29.570816
372.880131	21170.284942	29.575834
373.237113	21201.202324	29.580852
373.551295	21244.276984	29.585869
374.285779	21275.173261	29.590887
374.574285	21305.798242	29.595904
375.054794	21339.331326	29.600922
375.566618	21380.252289	29.605940
375.792743	21414.665717	29.610957
376.385565	21435.986512	29.615975
376.285098	21490.000954	29.620992
376.998592	21520.717664	29.626010
377.773987	21546.047577	29.631028
377.723479	21579.582104	29.636045
378.113090	21607.784317	29.641063
378.805221	21653.833619	29.646080
379.155594	21684.929716	29.651098
379.608254	21722.581267	29.656116
379.574660	21746.268924	29.661133
379.926696	21776.183309	29.666151
380.184824	21818.762506	29.671168
380.894963	21849.366517	29.676186
381.312957	21889.766142	29.681204
381.483322	21928.650226	29.686221
382.358404	21966.627837	29.691239
382.273316	21999.302821	29.696256
382.838579	22022.252490	29.701274
383.020942	22063.908902	29.706292
383.775109	22096.199836	29.711309
384.069043	22128.847258	29.716327
383.967555	22163.698752	29.721344
384.457541	22199.955224	29.726362
385.104242	22234.771794	29.731380
385.097040	22279.977950	29.736397
385.535130	22310.182968	29.741415
386.371935	22360.729245	29.746432
386.459309	22396.012843	29.751450
387.044594	22428.621441	29.756468
386.938844	22475.423204	29.761485
387.400439	22493.530409	29.766503
388.077080	22541.934845	29.771520
388.553514	22579.192526	29.776538
389.263536	22610.739258	29.781556
389.459212	22646.341241	29.786573
389.907684	22675.717403	29.791591
389.991846	22717.643329	29.796608
390.594238	22751.608363	29.801626
390.792896	22786.603505	29.806644
391.147811	22823.653194	29.811661
391.962956	22858.469751	29.816679
392.255221	22892.553113	29.821696
392.146862	22930.219005	29.826714
393.040007	22971.576415	29.831732
393.581970	23003.289115	29.836749
393.949303	23030.504746	29.841767
394.051663	23057.237432	29.846784
394.400654	23092.443371	29.851802
394.757347	23109.676574	29.856820
394.901093	23152.573546	29.861837
395.244001	23176.393507	29.866855
395.828793	23215.183597	29.871872
396.030142	23254.874274	29.876890
396.772265	23285.020514	29.881908
396.649442	23323.984845	29.886925
397.552547	23367.951345	29.891943
397.366146	23405.371270	29.896960
398.073267	23447.713010	29.901978
398.284263	23475.181228	29.906996
398.748341	23524.569236	29.912013
399.518095	23553.656239	29.917031
399.497437	23595.796326	29.922048
400.112462	23638.822741	29.927066
400.565683	23672.673689	29.932084
400.824224	23711.060857	29.937101
401.354444	23743.604406	29.942119
401.427707	23789.995733	29.947136
401.719250	23828.340042	29.952154
402.368094	23870.129384	29.957172
402.605917	23916.122386	29.962189
403.181058	23960.773501	29.967207
403.520152	24005.101484	29.972224
404.159421	24045.066384	29.977242
404.531748	24081.180408	29.982260
404.850099	24125.455031	29.987277
405.395278	24162.155113	29.992295
405.809486	24213.025065	29.997312
406.390022	24253.757919	30.002330
406.957397	24275.844092	30.007348
407.076645	24321.072980	30.012365
407.485861	24358.805839	30.017383
407.967665	24397.848181	30.022400
408.361182	24444.709062	30.027418
409.579628	24475.743065	30.032436
409.737546	24511.310049	30.037453
409.880177	24546.184338	30.042471
410.512358	24581.095759	30.047488
410.908237	24608.681924	30.052506
411.169886	24649.238025	30.057524
411.269532	24687.418127	30.062541
411.952852	24715.363872	30.067559
412.467955	24749.510292	30.072576
412.806344	24790.143132	30.077594
413.241340	24818.317506	30.082612
413.874855	24851.440725	30.087629
414.334921	24890.304161	30.092647
414.603255	24932.705134	30.097664
414.848902	24966.723497	30.102682
415.144004	24999.495507	30.107700
415.693244	25042.699555	30.112717
416.228522	25072.925131	30.117735
416.640958	25100.831686	30.122752
416.804395	25145.505690	30.127770
417.314153	25176.234680	30.132788
417.905656	25216.095641	30.137805
417.993716	25257.324777	30.142823
418.508879	25295.883335	30.147840
418.779741	25333.026674	30.152858
419.227945	25369.510321	30.157876
419.395967	25413.798690	30.162893
419.913557	25452.224452	30.167911
420.893966	25489.377018	30.172928
420.876702	25519.803570	30.177946
421.348618	25559.203631	30.182964
421.553901	25598.152580	30.187981
421.813643	25627.562640	30.192999
422.250485	25672.005388	30.198016
422.641351	25714.382494	30.203034
423.377537	25733.486099	30.208052
423.640375	25781.552394	30.213069
424.045305	25816.368837	30.218087
424.655989	25864.602044	30.223104
424.406895	25905.493473	30.228122
425.070328	25946.109332	30.233140
425.525588	25989.715652	30.238157
425.589882	26027.511987	30.243175
426.470635	26083.913149	30.248192
426.785403	26121.297543	30.253210
427.239402	26156.081606	30.258228
427.801203	26202.509414	30.263245
428.096108	26250.710842	30.268263
428.866354	26289.123903	30.273280
429.273117	26334.647240	30.278298
430.012922	26376.339066	30.283316
430.267620	26418.644174	30.288333
430.756800	26449.909222	30.293351
431.020576	26495.265711	30.298368
431.285075	26535.964202	30.303386
432.036687	26579.974110	30.308404
432.612758	26621.881694	30.313421
432.972078	26664.638625	30.318439
433.662228	26698.362753	30.323456
433.776165	26734.762176	30.328474
434.218593	26763.380522	30.333492
434.770894	26817.073217	30.338509
434.936911	26852.124792	30.343527
435.297504	26897.271086	30.348544
435.592863	26932.808166	30.353562
436.439455	26977.094795	30.358580
436.918164	27024.409707	30.363597
437.415069	27063.821425	30.368615
438.317598	27105.274371	30.373632
438.327809	27141.153537	30.378650
439.028984	27175.786868	30.383668
439.418905	27215.841357	30.388685
439.674562	27253.900741	30.393703
439.581913	27296.514900	30.398720
440.009156	27343.965025	30.403738
440.699288	27385.274838	30.408756
441.248713	27421.841137	30.413773
441.363737	27472.570227	30.418791
441.928545	27517.357246	30.423808
442.377458	27550.823512	30.428826
442.622712	27600.059842	30.433844
443.456801	27634.287583	30.438861
443.847972	27688.785244	30.443879
444.239351	27731.943913	30.448896
444.520751	27781.933489	30.453914
445.286247	27817.992612	30.458932
445.994732	27857.979505	30.463949
445.846873	27905.622146	30.468967
446.494341	27942.553261	30.473984
446.848336	27991.305776	30.479002
447.210645	28030.285359	30.484020
447.624837	28072.385625	30.489037
448.364946	28119.617893	30.494055
448.826239	28156.844025	30.499072
449.121749	28206.048661	30.504090
449.795664	28250.086996	30.509108
450.077692	28287.701727	30.514125
450.380535	28338.523643	30.519143
451.183491	28375.753546	30.524160
451.391555	28411.142536	30.529178
451.480774	28448.806724	30.534196
452.147274	28495.912334	30.539213
452.705537	28536.290692	30.544231
453.329664	28572.828391	30.549248
453.370801	28617.548146	30.554266
453.551135	28663.630463	30.559284
454.441553	28693.477128	30.564301
454.376247	28748.441004	30.569319
455.037469	28779.347676	30.574336
455.226059	28823.488545	30.579354
455.912561	28884.599049	30.584372
456.475299	28935.116259	30.589389
456.406310	28990.163530	30.594407
457.460358	29034.877245	30.599424
457.946438	29084.913794	30.604442
458.625900	29131.848169	30.609460
458.624601	29171.044900	30.614477
458.821634	29225.513848	30.619495
460.125089	29272.066362	30.624512
460.418046	29315.060473	30.629530
460.898145	29361.223824	30.634548
461.687557	29401.428618	30.639565
461.755006	29463.794565	30.644583
462.598699	29499.768553	30.649600
462.367522	29548.433111	30.654618
463.107131	29597.641057	30.659636
463.842716	29649.119047	30.664653
463.780646	29690.323771	30.669671
464.307190	29734.875108	30.674688
464.851383	29785.688086	30.679706
465.292509	29835.272053	30.684724
466.001910	29883.865936	30.689741
466.150736	29929.797992	30.694759
466.910597	29976.449889	30.699776
467.651819	30032.751076	30.704794
468.220729	30070.355742	30.709812
468.540134	30115.111019	30.714829
468.968942	30171.139131	30.719847
469.413541	30212.297143	30.724864
469.825107	30257.613535	30.729882
469.963078	30301.695964	30.734900
470.601889	30356.971052	30.739917
470.993290	30411.343152	30.744935
471.912459	30451.769886	30.749952
472.362410	30503.661388	30.754970
472.872500	30541.750232	30.759988
473.453882	30588.507324	30.765005
473.664391	30637.054690	30.770023
474.091420	30682.097767	30.775040
474.701283	30738.099056	30.780058
474.838216	30785.122170	30.785076
475.856890	30834.169247	30.790093
475.821136	30882.294288	30.795111
476.516120	30920.171544	30.800128
476.950167	30980.758862	30.805146
477.645602	31024.597476	30.810164
478.209964	31068.361889	30.815181
478.236688	31102.292004	30.820199
478.756935	31160.805504	30.825216
479.369182	31211.428000	30.830234
480.203888	31256.326290	30.835252
480.231935	31301.749286	30.840269
480.536841	31350.909381	30.845287
481.332226	31400.119205	30.850304
481.956316	31452.352464	30.855322
482.231898	31493.963049	30.860340
483.061523	31525.271020	30.865357
483.130392	31565.535987	30.870375
483.592323	31607.022785	30.875392
484.065983	31662.118601	30.880410
484.331822	31700.513343	30.885428
484.690168	31739.216078	30.890445
485.081607	31800.431994	30.895463
485.586869	31845.465341	30.900480
486.213472	31895.486679	30.905498
486.750765	31949.093977	30.910516
487.396134	31998.657450	30.915533
487.675959	32040.799500	30.920551
488.098460	32082.539974	30.925568
488.599949	32137.493606	30.930586
488.852766	32200.445647	30.935604
489.900825	32243.156872	30.940621
490.459716	32304.152058	30.945639
490.796018	32346.475539	30.950656
491.411309	32401.374109	30.955674
491.783380	32449.508433	30.960692
491.965822	32495.529402	30.965709
492.706563	32547.001136	30.970727
493.366683	32602.885775	30.975744
493.976157	32652.083420	30.980762
494.255389	32700.359303	30.985780
494.776822	32742.882184	30.990797
495.084149	32812.105374	30.995815
495.629190	32860.125041	31.000832
496.187538	32917.101222	31.005850
496.705278	32973.236747	31.010868
497.031775	33022.979036	31.015885
497.641888	33079.922263	31.020903
498.527372	33132.491796	31.025920
498.881551	33187.085601	31.030938
499.286207	33230.930143	31.035956
499.419241	33284.509345	31.040973
500.289325	33344.542093	31.045991
501.000292	33391.778316	31.051008
501.390641	33441.536885	31.056026
501.526657	33504.795640	31.061044
502.541721	33545.934113	31.066061
502.792973	33600.703173	31.071079
503.627952	33660.483105	31.076096
503.942890	33718.587033	31.081114
504.319002	33767.476112	31.086132
505.117896	33812.448733	31.091149
505.146164	33866.229175	31.096167
506.023575	33918.947357	31.101184
506.397851	33975.588536	31.106202
506.836017	34026.801489	31.111220
507.475784	34077.856542	31.116237
507.872798	34137.453524	31.121255
508.606935	34189.834441	31.126272
509.138442	34242.721416	31.131290
509.328099	34292.778976	31.136308
509.733008	34352.451199	31.141325
510.308270	34402.043978	31.146343
510.978936	34452.823226	31.151360
511.546132	34503.770546	31.156378
511.513961	34569.151623	31.161396
512.207735	34617.866466	31.166413
512.704116	34684.884881	31.171431
513.383817	34745.039956	31.176448
513.997642	34794.026957	31.181466
514.379536	34852.395394	31.186484
515.065214	34899.537794	31.191501
515.212885	34964.582108	31.196519
515.794910	35012.898061	31.201536
516.319756	35054.293298	31.206554
516.830631	35118.275874	31.211572
517.571585	35167.597906	31.216589
518.159293	35220.206641	31.221607
518.605820	35262.683112	31.226624
519.276416	35318.592284	31.231642
519.557894	35369.959487	31.236660
520.062974	35423.479517	31.241677
520.596851	35472.980119	31.246695
521.231706	35523.027761	31.251712
521.941658	35567.746163	31.256730
521.824837	35632.283850	31.261748
522.511618	35680.275090	31.266765
523.158320	35729.145289	31.271783
523.597510	35792.319133	31.276800
524.131777	35840.846787	31.281818
524.605011	35913.942813	31.286836
525.182623	35961.287865	31.291853
525.689885	36027.189630	31.296871
526.678912	36076.955475	31.301888
527.264041	36131.779953	31.306906
527.390796	36189.180322	31.311924
528.198659	36244.488702	31.316941
528.961130	36295.871328	31.321959
529.291199	36345.235154	31.326976
529.565797	36406.324655	31.331994
530.026905	36459.127007	31.337012
530.705867	36508.461859	31.342029
531.397541	36572.237114	31.347047
531.607341	36625.989785	31.352064
532.271069	36678.590217	31.357082
532.862236	36747.092575	31.362100
533.313737	36805.196207	31.367117
534.064614	36856.879195	31.372135
534.467064	36913.226595	31.377152
534.932769	36968.432355	31.382170
535.358316	37035.165740	31.387188
536.067155	37088.221720	31.392205
536.775366	37142.751285	31.397223
537.078648	37210.788018	31.402240
538.071359	37260.378989	31.407258
538.187413	37322.482392	31.412276
539.025063	37378.320211	31.417293
539.625660	37431.438258	31.422311
539.909073	37496.146525	31.427328
540.598373	37550.167883	31.432346
540.833322	37610.438642	31.437364
541.477580	37669.899284	31.442381
542.282751	37721.076291	31.447399
542.800302	37786.001702	31.452416
543.428622	37832.988833	31.457434
543.683542	37889.760289	31.462452
544.646730	37949.393081	31.467469
545.159526	37998.125022	31.472487
545.506300	38051.859808	31.477504
546.075071	38114.021063	31.482522
546.367008	38166.417777	31.487540
547.206639	38231.015843	31.492557
547.831933	38285.801597	31.497575
548.185234	38348.781420	31.502592
548.886877	38400.469510	31.507610
549.326906	38454.380407	31.512628
549.832491	38509.204448	31.517645
550.678201	38564.032273	31.522663
550.915208	38626.860377	31.527680
551.492020	38671.903336	31.532698
551.958984	38743.327831	31.537716
552.595170	38787.077984	31.542733
553.496595	38842.593418	31.547751
553.895785	38898.048528	31.552768
554.174839	38943.233545	31.557786
554.784136	39000.268614	31.562804
554.877205	39045.141479	31.567821
555.576610	39101.359558	31.572839
556.249480	39156.639663	31.577856
557.162434	39212.710753	31.582874
557.018789	39269.352209	31.587892
557.456870	39337.058330	31.592909
557.892434	39389.441834	31.597927
558.532651	39460.107965	31.602944
559.368541	39518.797442	31.607962
559.929144	39588.382389	31.612980
560.446178	39638.799580	31.617997
560.498662	39705.909531	31.623015
561.182651	39779.497931	31.628032
561.912576	39830.021356	31.633050
562.472373	39901.877818	31.638068
563.307485	39975.449538	31.643085
563.449202	40043.065139	31.648103
564.147075	40107.128142	31.653120
564.912778	40172.926216	31.658138
565.341041	40243.590141	31.663156
565.796659	40311.846763	31.668173
566.539015	40360.693523	31.673191
567.146734	40439.191145	31.678208
567.736716	40497.864856	31.683226
568.290272	40578.167585	31.688244
568.625338	40647.266310	31.693261
569.740595	40710.392944	31.698279
569.932136	40782.759018	31.703296
571.099827	40844.347305	31.708314
571.625987	40914.087340	31.713332
571.831418	40978.824528	31.718349
572.625458	41037.315940	31.723367
573.389647	41113.286955	31.728384
573.880798	41160.890960	31.733402
574.266754	41237.977849	31.738420
574.961249	41308.451726	31.743437
575.601733	41357.702472	31.748455
575.598960	41433.307716	31.753472
576.876943	41488.094184	31.758490
577.148674	41566.218387	31.763508
577.628672	41629.289045	31.768525
578.814519	41690.889520	31.773543
578.829312	41760.731307	31.778560
579.576657	41823.501337	31.783578
580.254446	41889.919194	31.788596
580.868806	41957.371805	31.793613
581.863615	42011.818117	31.798631
581.967904	42077.586354	31.803648
582.758793	42141.609116	31.808666
583.177369	42210.516258	31.813684
583.765280	42279.226323	31.818701
584.624462	42337.223977	31.823719
585.116533	42407.916503	31.828736
586.096359	42466.009450	31.833754
586.416800	42531.631338	31.838772
586.769129	42596.071977	31.843789
587.462962	42640.959320	31.848807
587.910297	42711.748374	31.853824
588.629795	42767.479376	31.858842
589.140917	42834.602960	31.863860
589.535574	42894.357295	31.868877
590.200272	42962.380675	31.873895
590.571734	43029.299018	31.878912
591.380600	43082.954831	31.883930
591.991327	43148.102974	31.888948
592.425598	43205.815247	31.893965
593.256592	43257.462940	31.898983
593.434554	43321.028496	31.904000
594.122685	43392.161524	31.909018
594.851934	43455.021253	31.914036
595.274892	43523.153791	31.919053
595.725460	43575.943424	31.924071
596.102575	43646.158208	31.929088
596.756830	43714.748482	31.934106
597.490127	43786.470278	31.939124
597.903894	43853.276948	31.944141
598.823372	43905.721937	31.949159
599.599092	43987.583626	31.954176
599.860404	44054.465378	31.959194
600.816944	44123.060172	31.964212
601.035774	44193.016826	31.969229
601.769237	44262.298506	31.974247
602.501865	44336.470134	31.979264
603.000100	44405.226130	31.984282
603.781288	44463.323793	31.989300
604.333493	44535.196545	31.994317
605.511688	44602.372807	31.999335
605.880401	44665.425255	32.004352
605.773350	44739.502004	32.009370
606.825842	44806.628985	32.014388
607.495824	44883.506955	32.019405
608.232225	44939.462152	32.024423
608.774386	45022.445902	32.029440
609.041989	45086.850090	32.034458
609.820833	45153.976690	32.039476
610.413847	45217.805257	32.044493
610.901494	45295.345769	32.049511
611.578818	45364.430906	32.054528
612.076958	45436.859036	32.059546
612.968932	45507.150853	32.064564
613.455096	45588.102224	32.069581
614.244588	45661.200269	32.074599
614.722480	45740.907291	32.079616
615.620244	45803.291775	32.084634
616.412322	45881.311681	32.089652
616.739519	45958.835329	32.094669
617.698428	46014.296565	32.099687
618.136010	46093.384878	32.104704
618.701778	46163.305993	32.109722
619.533100	46222.469457	32.114740
620.090551	46294.669648	32.119757
620.852783	46355.881268	32.124775
621.245939	46420.282261	32.129792
622.053326	46495.606989	32.134810
622.473822	46557.220610	32.139828
622.934233	46635.699940	32.144845
623.710293	46705.728975	32.149863
624.349655	46776.222468	32.154880
624.846876	46850.989643	32.159898
625.697697	46916.237672	32.164916
626.146810	46981.523496	32.169933
627.200484	47054.458157	32.174951
627.457729	47123.342444	32.179968
627.903045	47201.807121	32.184986
628.466323	47269.694980	32.190004
629.020906	47351.331522	32.195021
629.747057	47420.029400	32.200039
630.784574	47481.365438	32.205056
631.142150	47567.012896	32.210074
631.842365	47620.487817	32.215092
632.273115	47694.230649	32.220109
632.951239	47763.379936	32.225127
633.514922	47832.205727	32.230144
634.377619	47900.371228	32.235162
634.871903	47964.988523	32.240180
635.241028	48036.989674	32.245197
635.850756	48097.363147	32.250215
636.831246	48169.256318	32.255232
637.296512	48241.749185	32.260250
637.908793	48309.252876	32.265268
638.331147	48386.738284	32.270285
639.124458	48448.773145	32.275303
639.678752	48519.475165	32.280320
640.429556	48595.777372	32.285338
641.139856	48667.107065	32.290356
641.508048	48749.151080	32.295373
642.287659	48821.887586	32.300391
643.169914	48898.195523	32.305408
643.397554	48972.733504	32.310426
644.185330	49040.521883	32.315444
644.591169	49126.623160	32.320461
645.359784	49203.367481	32.325479
645.941250	49275.946654	32.330496
646.560242	49349.386964	32.335514
647.357772	49437.364091	32.340532
648.115077	49520.457136	32.345549
648.541540	49594.276360	32.350567
649.309501	49672.363665	32.355584
649.936395	49755.326134	32.360602
650.931100	49833.897291	32.365620
651.556891	49917.790589	32.370637
652.244890	49989.210135	32.375655
652.983043	50067.543877	32.380672
653.273753	50138.627497	32.385690
654.368332	50216.273215	32.390708
654.820351	50302.700669	32.395725
655.542341	50375.856055	32.400743
656.117400	50449.737001	32.405760
656.558371	50529.536141	32.410778
657.440329	50605.077867	32.415796
658.311372	50694.522526	32.420813
658.930570	50775.357581	32.425831
659.650231	50849.343703	32.430848
660.275161	50934.594870	32.435866
661.121311	51003.942733	32.440884
661.607074	51081.034984	32.445901
662.358899	51163.198350	32.450919
662.790219	51234.453135	32.455936
663.451315	51309.797635	32.460954
664.188416	51385.826495	32.465972
664.731886	51466.327807	32.470989
665.680402	51547.797347	32.476007
665.953214	51627.487392	32.481024
666.958327	51709.650989	32.486042
667.753188	51784.064912	32.491060
668.185521	51866.401020	32.496077
668.780218	51946.769420	32.501095
669.477412	52025.666693	32.506112
669.891392	52110.404704	32.511130
670.930087	52183.997091	32.516148
671.675190	52272.176702	32.521165
672.139044	52362.906462	32.526183
673.155956	52429.264138	32.531200
673.603802	52507.195978	32.536218
674.419297	52579.217318	32.541236
674.963601	52657.900215	32.546253
675.585329	52727.573107	32.551271
676.322356	52810.712752	32.556288
677.013381	52893.429601	32.561306
677.492932	52961.587787	32.566324
678.303934	53033.408736	32.571341
679.191021	53111.558554	32.576359
680.074731	53178.458103	32.581376
680.163906	53254.436315	32.586394
680.795511	53324.122089	32.591412
681.387116	53398.535013	32.596429
681.938945	53482.585629	32.601447
682.871348	53558.717532	32.606464
683.410376	53646.073969	32.611482
684.223759	53716.833521	32.616500
684.668092	53796.915408	32.621517
685.555311	53878.940551	32.626535
686.438347	53949.822786	32.631552
686.894193	54039.275663	32.636570
687.567180	54117.399069	32.641588
688.344780	54207.643845	32.646605
689.059886	54285.615663	32.651623
689.611677	54368.289888	32.656640
690.050504	54443.970372	32.661658
691.085069	54530.986693	32.666676
691.621798	54621.277096	32.671693
691.941508	54709.779267	32.676711
693.285196	54790.495735	32.681728
693.507179	54880.133965	32.686746
694.187500	54963.587516	32.691764
694.693988	55047.030612	32.696781
695.634645	55140.246752	32.701799
696.533856	55232.286323	32.706816
697.093538	55325.607150	32.711834
697.974652	55419.751343	32.716852
698.860678	55498.288935	32.721869
699.682250	55578.121580	32.726887
700.395070	55657.110834	32.731904
701.076639	55749.059915	32.736922
701.918811	55830.611563	32.741940
702.794403	55921.904391	32.746957
703.022235	56008.881586	32.751975
703.709062	56093.338010	32.756992
704.633641	56176.979066	32.762010
705.234640	56255.500500	32.767028
705.921143	56341.052723	32.772045
706.216370	56439.108937	32.777063
707.008075	56525.974393	32.782080
707.701300	56625.551248	32.787098
708.718779	56719.274164	32.792116
709.551830	56808.842927	32.797133
709.459222	56904.151747	32.802151
710.391427	56998.768828	32.807168
711.527502	57095.575823	32.812186
712.312005	57186.811789	32.817204
712.958879	57272.095061	32.822221
713.866745	57360.084567	32.827239
714.549325	57452.046351	32.832256
714.905235	57538.597641	32.837274
715.973575	57623.993372	32.842292
716.811227	57707.001475	32.847309
717.308265	57802.613915	32.852327
718.062050	57896.344735	32.857344
718.880624	57986.426481	32.862362
719.540368	58062.963576	32.867380
720.303033	58147.965984	32.872397
720.985608	58242.563746	32.877415
721.647857	58333.626985	32.882432
722.359558	58419.752284	32.887450
723.353565	58507.169170	32.892468
723.941176	58599.080568	32.897485
724.693351	58684.719438	32.902503
725.370324	58765.243567	32.907520
725.798475	58843.363769	32.912538
726.687566	58924.627399	32.917556
727.529282	59006.259500	32.922573
727.957631	59090.861843	32.927591
728.649201	59163.238951	32.932608
729.398525	59258.266953	32.937626
730.378275	59347.676571	32.942644
731.103673	59431.790512	32.947661
731.787877	59518.708879	32.952679
732.282676	59604.941967	32.957696
733.028802	59694.167904	32.962714
733.562684	59775.825470	32.967732
734.242906	59871.157845	32.972749
735.112398	59973.037531	32.977767
735.774622	60052.245309	32.982784
736.757459	60151.854602	32.987802
737.570844	60251.199666	32.992820
738.444933	60333.407147	32.997837
738.709024	60432.497153	33.002855
739.496970	60522.238606	33.007872
740.094921	60616.105574	33.012890
740.967571	60713.658202	33.017908
741.922648	60806.843313	33.022925
742.099462	60902.859874	33.027943
743.344079	60999.671752	33.032960
743.815226	61112.892251	33.037978
744.667358	61207.753465	33.042996
745.712931	61299.774204	33.048013
746.590766	61397.740184	33.053031
747.203059	61487.430371	33.058048
748.073699	61586.499666	33.063066
748.810398	61687.419748	33.068084
749.750392	61780.389346	33.073101
750.541619	61883.403311	33.078119
751.402649	61969.543028	33.083136
751.967403	62062.945932	33.088154
752.429389	62151.199773	33.093172
753.671055	62247.618198	33.098189
754.101166	62345.132625	33.103207
754.734249	62439.640384	33.108224
755.445682	62535.364326	33.113242
756.432008	62635.293289	33.118260
757.638982	62731.206263	33.123277
757.988995	62833.166444	33.128295
758.619667	62921.795423	33.133312
759.483460	63018.364639	33.138330
759.998418	63112.285721	33.143348
760.937558	63220.384466	33.148365
761.482444	63317.967023	33.153383
762.542344	63419.723477	33.158400
763.240052	63515.067164	33.163418
763.907202	63617.462011	33.168436
764.560871	63715.497553	33.173453
765.343348	63822.844762	33.178471
765.914514	63917.247528	33.183488
766.655623	64018.081403	33.188506
767.359179	64118.497401	33.193524
768.130370	64223.980514	33.198541
769.024185	64333.553577	33.203559
769.756008	64437.537013	33.208576
770.843371	64533.386997	33.213594
771.673187	64647.390404	33.218612
772.508770	64744.287233	33.223629
772.928396	64846.561246	33.228647
773.881388	64940.825759	33.233664
774.855208	65050.522363	33.238682
775.740811	65144.399335	33.243700
776.662404	65233.256823	33.248717
777.344649	65329.597454	33.253735
777.672061	65414.617022	33.258752
778.868561	65499.146240	33.263770
779.691131	65593.813479	33.268788
780.419414	65677.929116	33.273805
781.288706	65781.738280	33.278823
781.747122	65866.131053	33.283840
782.783441	65958.208370	33.288858
783.347220	66055.912534	33.293876
784.277002	66150.356129	33.298893
784.704198	66252.140788	33.303911
785.477854	66352.415393	33.308928
786.419552	66450.517749	33.313946
787.178801	66549.579765	33.318964
787.672404	66632.728619	33.323981
788.441427	66741.438913	33.328999
789.410108	66843.546352	33.334016
790.111724	66944.163800	33.339034
790.764822	67054.698052	33.344052
791.786649	67154.405100	33.349069
792.644308	67267.428189	33.354087
793.391484	67355.066752	33.359104
794.379757	67462.251522	33.364122
794.792171	67564.037387	33.369140
795.885159	67665.679093	33.374157
796.117422	67775.826473	33.379175
797.007378	67882.243263	33.384192
798.135195	67989.794619	33.389210
798.591021	68101.776249	33.394228
799.727546	68202.235550	33.399245
800.364426	68324.675246	33.404263
801.176241	68426.458965	33.409280
802.145531	68540.793526	33.414298
802.662562	68654.433252	33.419316
803.568240	68769.386648	33.424333
804.308692	68879.579467	33.429351
805.417453	68994.862986	33.434368
806.495201	69097.069937	33.439386
807.117127	69207.833597	33.444404
807.821056	69317.274152	33.449421
808.670063	69427.585275	33.454439
809.373630	69530.036155	33.459456
810.220473	69639.968591	33.464474
810.855498	69758.470426	33.469492
811.931991	69873.984528	33.474509
812.594376	69982.851825	33.479527
813.415094	70095.272507	33.484544
814.523509	70211.789935	33.489562
815.382780	70325.674661	33.494580
816.054588	70429.457501	33.499597
816.855823	70552.546855	33.504615
817.635382	70659.758542	33.509632
818.701889	70752.829782	33.514650
819.141669	70865.680705	33.519668
820.341007	70987.151982	33.524685
821.243564	71100.374723	33.529703
821.790950	71206.219185	33.534720
823.139365	71312.457911	33.539738
823.385259	71432.345426	33.544756
824.341216	71537.101364	33.549773
825.341570	71652.236278	33.554791
826.192350	71766.039927	33.559808
827.259749	71869.019256	33.564826
827.891303	71976.132833	33.569844
829.010153	72087.413470	33.574861
829.641852	72194.249268	33.579879
830.575660	72296.149281	33.584896
831.355854	72381.177816	33.589914
831.911396	72490.952491	33.594932
833.038253	72580.689672	33.599949
833.668725	72677.559705	33.604967
834.357853	72785.478147	33.609984
835.290061	72880.325807	33.615002
835.910979	72990.738269	33.620020
836.815080	73093.735266	33.625037
837.054283	73195.709500	33.630055
838.140427	73306.405072	33.635072
839.317005	73408.828647	33.640090
840.150564	73524.580450	33.645108
840.407925	73641.765598	33.650125
841.236495	73753.769979	33.655143
842.367309	73864.473537	33.660160
843.388219	73978.196692	33.665178
844.064412	74091.885642	33.670196
845.013892	74203.378982	33.675213
845.803906	74318.267051	33.680231
846.537459	74439.611743	33.685248
847.628319	74545.713736	33.690266
848.234019	74658.744794	33.695284
849.212658	74775.935955	33.700301
850.001386	74892.144019	33.705319
850.573500	75010.970541	33.710336
851.736818	75131.060372	33.715354
852.585246	75266.995753	33.720372
853.487508	75370.407129	33.725389
854.299950	75495.468326	33.730407
855.026045	75618.922229	33.735424
856.132805	75728.535185	33.740442
856.708389	75852.913092	33.745460
857.656738	75969.810161	33.750477
858.499745	76096.896116	33.755495
859.543143	76213.488003	33.760512
860.379437	76338.562021	33.765530
860.890766	76470.831986	33.770548
862.034612	76586.206325	33.775565
862.837058	76711.160679	33.780583
863.899222	76831.489229	33.785600
865.007913	76951.519666	33.790618
865.756178	77085.681010	33.795636
866.524687	77210.706302	33.800653
867.422047	77337.802198	33.805671
868.111088	77452.174637	33.810688
869.133782	77577.655854	33.815706
869.783155	77691.516111	33.820724
870.742863	77827.484852	33.825741
871.687708	77957.553201	33.830759
872.724980	78081.400237	33.835776
873.580473	78190.530355	33.840794
874.343730	78318.399217	33.845812
875.622572	78450.355860	33.850829
876.213305	78569.473667	33.855847
876.980810	78693.162994	33.860864
878.095891	78815.176868	33.865882
878.877581	78939.283139	33.870900
880.036305	79065.066546	33.875917
880.745488	79183.484337	33.880935
881.892843	79313.565368	33.885952
882.833707	79420.799317	33.890970
883.208289	79541.576765	33.895988
884.669401	79673.257316	33.901005
885.398426	79787.671169	33.906023
886.069751	79909.277912	33.911040
887.006510	80021.759832	33.916058
888.001538	80139.668176	33.921076
888.611831	80259.258926	33.926093
889.695222	80367.931169	33.931111
890.336826	80500.491434	33.936128
891.325122	80609.141497	33.941146
892.168121	80725.834512	33.946164
892.945674	80839.016130	33.951181
894.100286	80944.005293	33.956199
894.585206	81057.157594	33.961216
895.397286	81173.451883	33.966234
896.680164	81300.644929	33.971252
897.691487	81418.277364	33.976269
898.595432	81530.377712	33.981287
898.972786	81647.400859	33.986304
899.919621	81763.917213	33.991322
900.609822	81900.708230	33.996340
901.775118	82025.655025	34.001357
902.780470	82146.699679	34.006375
903.527554	82277.541324	34.011392
904.338216	82404.914644	34.016410
905.259821	82541.026337	34.021428
905.939148	82664.823023	34.026445
907.313654	82793.579561	34.031463
907.926026	82920.745503	34.036480
909.000428	83041.618444	34.041498
910.085628	83184.714398	34.046516
910.907343	83310.658266	34.051533
912.194637	83436.111656	34.056551
912.742878	83567.459179	34.061568
914.141977	83705.541659	34.066586
914.738763	83829.140916	34.071604
915.757070	83959.212901	34.076621
916.866357	84076.980381	34.081639
917.461179	84210.110162	34.086656
918.288892	84338.300380	34.091674
919.614621	84464.727930	34.096692
920.153540	84605.318927	34.101709
921.133647	84719.941464	34.106727
922.162256	84859.975520	34.111744
923.101891	84994.575493	34.116762
924.162835	85125.799167	34.121780
924.639024	85257.444454	34.126797
925.977452	85395.506527	34.131815
926.761874	85537.774276	34.136832
927.723199	85659.968435	34.141850
928.763598	85797.546875	34.146868
929.555481	85938.231450	34.151885
930.847939	86072.096903	34.156903
931.778076	86204.739840	34.161920
932.664788	86333.613934	34.166938
933.482284	86466.491121	34.171956
934.422887	86596.270322	34.176973
935.380285	86730.267289	34.181991
936.309094	86870.770182	34.187008
937.182383	87000.764470	34.192026
937.957356	87139.696034	34.197044
938.914829	87270.147211	34.202061
940.242930	87399.438435	34.207079
940.455984	87537.281324	34.212096
941.786496	87675.520158	34.217114
942.881773	87806.598435	34.222132
943.751964	87946.722796	34.227149
944.724918	88081.496518	34.232167
945.597873	88236.727702	34.237184
946.462235	88371.355001	34.242202
947.677594	88499.439431	34.247220
948.809748	88635.876245	34.252237
949.849520	88760.783041	34.257255
950.220746	88904.906017	34.262272
951.633195	89024.610305	34.267290
952.244523	89145.593767	34.272308
953.377661	89275.823511	34.277325
954.180737	89391.341135	34.282343
954.894165	89517.772302	34.287360
955.939233	89655.786244	34.292378
956.782741	89775.519260	34.297396
957.495507	89911.888172	34.302413
958.961032	90037.671491	34.307431
959.703736	90176.901143	34.312448
960.286614	90302.861792	34.317466
961.208127	90445.334495	34.322484
962.397114	90583.406213	34.327501
963.294222	90711.562633	34.332519
964.007056	90856.870872	34.337536
964.961102	91001.761824	34.342554
966.134625	91145.896689	34.347572
967.183648	91287.301460	34.352589
968.168831	91426.232758	34.357607
968.903493	91579.905978	34.362624
969.413147	91714.477082	34.367642
970.643794	91868.150149	34.372660
971.677185	92014.237577	34.377677
972.616399	92158.375914	34.382695
973.715025	92313.212598	34.387712
974.736299	92469.393007	34.392730
975.655319	92615.716691	34.397748
976.790426	92770.664053	34.402765
977.801642	92908.761505	34.407783
978.346620	93065.539195	34.412800
979.327522	93220.031329	34.417818
980.380755	93363.916668	34.422836
981.347697	93527.018811	34.427853
982.304123	93677.651200	34.432871
983.707258	93836.250413	34.437888
985.006292	93994.271007	34.442906
986.093475	94146.799167	34.447924
987.085578	94300.889354	34.452941
987.996262	94442.533158	34.457959
988.930568	94594.086101	34.462976
990.192133	94748.922201	34.467994
991.209249	94895.139937	34.473012
992.222685	95041.853285	34.478029
993.280479	95193.098273	34.483047
994.020851	95343.303578	34.488064
994.826853	95491.154305	34.493082
996.070406	95641.713239	34.498100
997.502046	95793.789912	34.503117
998.483525	95934.884346	34.508135
999.509824	96092.907589	34.513152
1000.517469	96250.871166	34.518170
1001.293541	96385.167361	34.523188
1002.264515	96537.002854	34.528205
1003.537347	96685.394573	34.533223
1004.641499	96833.864105	34.538240
1005.696955	96981.340523	34.543258
1006.354909	97123.327575	34.548276
1007.185253	97277.609847	34.553293
1008.210564	97419.236472	34.558311
1009.075618	97577.165620	34.563328
1010.149705	97732.121831	34.568346
1011.540676	97874.669341	34.573364
1012.146612	98034.796377	34.578381
1013.080952	98186.113074	34.583399
1014.290453	98334.560448	34.588416
1015.433373	98481.256834	34.593434
1016.354398	98634.314485	34.598452
1017.271789	98790.352558	34.603469
1018.529712	98936.120267	34.608487
1019.540231	99091.993099	34.613504
1020.455225	99230.513746	34.618522
1021.770853	99371.355604	34.623540
1022.678901	99508.750250	34.628557
1023.647301	99639.328238	34.633575
1024.676652	99781.230903	34.638592
1025.679821	99921.794468	34.643610
1026.339923	100060.929074	34.648628
1027.445971	100206.751657	34.653645
1028.956688	100344.283691	34.658663
1029.580939	100497.130407	34.663680
1030.310299	100649.048579	34.668698
1031.454275	100781.378574	34.673716
1031.877756	100940.420262	34.678733
1032.713292	101088.862775	34.683751
1034.198239	101255.676249	34.688768
1035.010143	101415.737071	34.693786
1036.122586	101572.087619	34.698804
1037.530844	101733.755505	34.703821
1038.509307	101889.925690	34.708839
1039.459035	102051.147114	34.713856
1040.532614	102215.659012	34.718874
1041.732856	102368.817308	34.723892
1042.803305	102543.055747	34.728909
1043.650644	102705.817827	34.733927
1045.119376	102856.679548	34.738944
1046.024840	103027.852765	34.743962
1047.110803	103174.553831	34.748980
1047.950649	103344.179455	34.753997
1049.344654	103510.473372	34.759015
1050.373284	103667.442855	34.764032
1051.125086	103838.695012	34.769050
1052.681979	103989.573423	34.774068
1053.384400	104151.300207	34.779085
1054.640576	104318.266359	34.784103
1055.704478	104490.284454	34.789120
1056.753649	104651.376108	34.794138
1057.380424	104803.253317	34.799156
1058.699162	104978.822290	34.804173
1060.043275	105147.503200	34.809191
1061.196325	105311.066936	34.814208
1062.137078	105468.996880	34.819226
1063.409076	105637.539366	34.824244
1064.687500	105801.415513	34.829261
1065.457504	105955.304234	34.834279
1066.653011	106123.429989	34.839296
1067.451675	106287.928826	34.844314
1068.761984	106453.857279	34.849332
1069.888970	106620.233682	34.854349
1070.564674	106780.518982	34.859367
1071.781805	106951.460423	34.864384
1072.864295	107115.741278	34.869402
1074.280631	107278.601173	34.874420
1075.042743	107447.929833	34.879437
1076.090441	107614.779960	34.884455
1077.316347	107775.554377	34.889472
1078.009257	107951.350734	34.894490
1079.394376	108097.633157	34.899508
1080.408187	108277.717713	34.904525
1081.831796	108442.915209	34.909543
1082.975348	108610.287717	34.914560
1084.096494	108774.342141	34.919578
1085.082021	108933.244736	34.924596
1086.269430	109105.368115	34.929613
1087.019952	109266.604283	34.934631
1088.323254	109420.615171	34.939648
1089.698096	109595.780451	34.944666
1090.673636	109747.206397	34.949684
1091.635563	109911.684195	34.954701
1092.645551	110055.281703	34.959719
1093.763869	110196.313871	34.964736
1094.502963	110350.379117	34.969754
1095.793564	110496.800501	34.974772
1096.853888	110666.592652	34.979789
1097.837948	110815.675752	34.984807
1098.708784	110964.231893	34.989824
1100.079145	111130.464895	34.994842
1101.077069	111292.267622	34.999860
1102.485420	111458.217207	35.004877
1103.085948	111618.219393	35.009895
1104.570169	111792.820409	35.014912
1105.538759	111959.602089	35.019930
1106.447443	112120.243103	35.024948
1107.465736	112277.925416	35.029965
1108.856700	112446.507508	35.034983
1110.074428	112618.503679	35.040000
1111.063647	112781.493940	35.045018
1112.382567	112942.886068	35.050036
1113.110750	113124.955015	35.055053
1114.259692	113288.404487	35.060071
1115.773315	113454.689229	35.065088
1116.760716	113636.428460	35.070106
1117.787634	113793.748233	35.075124
1119.078683	113969.277803	35.080141
1120.108293	114153.486140	35.085159
1121.080817	114319.453688	35.090176
1122.118699	114497.891758	35.095194
1123.317395	114668.150357	35.100212
1124.182291	114843.890347	35.105229
1125.381831	115021.088076	35.110247
1126.515021	115198.576074	35.115264
1127.857212	115395.348774	35.120282
1129.277218	115574.531280	35.125300
1129.916227	115745.909820	35.130317
1131.140126	115926.494531	35.135335
1132.331486	116102.519160	35.140352
1133.740656	116278.079282	35.145370
1134.709460	116464.109725	35.150388
1135.796759	116657.821529	35.155405
1136.971921	116830.186546	35.160423
1138.328060	117003.094793	35.165440
1139.331098	117191.228997	35.170458
1140.133796	117377.150452	35.175476
1141.427957	117558.822857	35.180493
1142.405261	117755.462168	35.185511
1143.904904	117934.706930	35.190528
1145.046068	118129.166234	35.195546
1146.229800	118306.876692	35.200564
1147.500233	118483.204506	35.205581
1148.325912	118668.824280	35.210599
1149.632576	118855.282935	35.215616
1150.775577	119041.412957	35.220634
1151.898779	119222.866394	35.225652
1153.104004	119411.436587	35.230669
1154.117587	119601.014426	35.235687
1155.801684	119783.524321	35.240704
1156.754744	119968.610372	35.245722
1157.855950	120156.718478	35.250740
1159.296154	120330.821046	35.255757
1160.562387	120521.759191	35.260775
1161.833393	120698.008284	35.265792
1162.759217	120880.007809	35.270810
1164.079642	121059.802624	35.275828
1165.528398	121235.823362	35.280845
1166.480543	121419.838230	35.285863
1167.844167	121582.528980	35.290880
1168.729947	121750.927508	35.295898
1169.654835	121921.971885	35.300916
1170.772140	122078.474717	35.305933
1172.235786	122247.190840	35.310951
1173.239762	122408.469790	35.315968
1174.488324	122585.492019	35.320986
1175.491297	122757.403100	35.326004
1176.453031	122928.801268	35.331021
1177.781985	123103.783507	35.336039
1178.848683	123276.448006	35.341056
1179.949359	123449.983260	35.346074
1181.123108	123626.197250	35.351092
1182.213887	123807.512095	35.356109
1183.261819	123992.817892	35.361127
1184.800414	124177.426113	35.366144
1185.803914	124357.006417	35.371162
1186.701067	124546.715104	35.376180
1188.249828	124714.920889	35.381197
1189.313516	124920.399699	35.386215
1190.744430	125091.657539	35.391232
1191.607032	125280.410904	35.396250
1192.993697	125477.836812	35.401268
1194.201210	125647.774508	35.406285
1195.095713	125856.633791	35.411303
1196.684903	126043.056776	35.416320
1197.400502	126235.973438	35.421338
1198.379865	126426.122046	35.426356
1200.018851	126620.545247	35.431373
1201.389624	126823.219808	35.436391
1202.936996	127013.815060	35.441408
1203.859105	127204.547132	35.446426
1204.924947	127409.784340	35.451444
1206.170129	127596.166700	35.456461
1207.416909	127795.287636	35.461479
1208.820630	127986.810634	35.466496
1209.949920	128192.967938	35.471514
1211.105342	128387.310171	35.476532
1212.788167	128577.739123	35.481549
1214.228960	128780.805554	35.486567
1215.550712	128957.425265	35.491584
1216.716622	129160.117864	35.496602
1217.892819	129340.098813	35.501620
1219.219373	129526.527750	35.506637
1219.957600	129726.003873	35.511655
1221.605867	129925.490723	35.516672
1222.512035	130114.322613	35.521690
1223.977618	130311.847860	35.526708
1225.293802	130497.597513	35.531725
1226.425790	130692.550309	35.536743
1227.706292	130881.301601	35.541760
1228.678776	131079.960688	35.546778
1229.996583	131274.582511	35.551796
1231.307117	131468.711502	35.556813
1232.393375	131661.848710	35.561831
1233.966613	131852.017577	35.566848
1235.118650	132050.437299	35.571866
1235.988327	132252.594496	35.576884
1237.636302	132437.044359	35.581901
1238.418761	132632.974164	35.586919
1239.860347	132832.291065	35.591936
1240.871977	133041.852588	35.596954
1242.367930	133235.731999	35.601972
1243.474673	133424.178892	35.606989
1244.846253	133633.661495	35.612007
1246.048899	133829.530832	35.617024
1247.550484	134020.836923	35.622042
1248.536612	134212.655957	35.627060
1249.984491	134403.426464	35.632077
1251.142401	134595.474032	35.637095
1252.385439	134783.359697	35.642112
1253.547787	134957.960348	35.647130
1254.556226	135131.900542	35.652148
1255.975381	135330.737245	35.657165
1256.963926	135518.678501	35.662183
1258.504648	135696.864663	35.667200
1259.920923	135899.803038	35.672218
1260.738579	136067.711056	35.677236
1262.177075	136262.818056	35.682253
1263.275787	136464.565062	35.687271
1264.466655	136657.136485	35.692288
1265.808284	136846.385749	35.697306
1266.729818	137047.122481	35.702324
1268.668646	137240.784805	35.707341
1269.567127	137442.047151	35.712359
1270.779853	137641.763750	35.717376
1272.171945	137850.666173	35.722394
1273.349066	138054.501724	35.727412
1274.517418	138253.085775	35.732429
1275.832338	138456.749228	35.737447
1277.324480	138654.535568	35.742464
1278.403202	138871.067749	35.747482
1279.745164	139067.610293	35.752500
1281.260722	139275.002262	35.757517
1282.120939	139489.667903	35.762535
1283.468039	139702.671971	35.767552
1284.857404	139902.167477	35.772570
1285.941809	140123.349283	35.777588
1287.298974	140336.506895	35.782605
1288.568191	140543.981026	35.787623
1290.099851	140771.390480	35.792640
1291.342906	140987.335464	35.797658
1292.716544	141207.220577	35.802676
1294.117406	141418.726305	35.807693
1295.314921	141628.119982	35.812711
1296.721441	141849.868458	35.817728
1297.991587	142055.191415	35.822746
1298.744266	142275.952726	35.827764
1300.500286	142487.331344	35.832781
1301.938379	142704.979438	35.837799
1303.052764	142927.958821	35.842816
1304.790439	143148.138345	35.847834
1305.939808	143374.782120	35.852852
1307.391113	143579.435796	35.857869
1308.680806	143806.072261	35.862887
1309.666964	144019.189772	35.867904
1311.517179	144239.508805	35.872922
1312.388057	144467.165706	35.877940
1314.230875	144682.106482	35.882957
1315.081869	144887.582904	35.887975
1316.392283	145118.943457	35.892992
1317.976149	145332.810631	35.898010
1319.036292	145559.897055	35.903028
1320.703132	145766.683535	35.908045
1321.941055	145994.619823	35.913063
1323.212834	146217.703360	35.918080
1324.877737	146429.303199	35.923098
1326.013230	146655.989212	35.928116
1327.413657	146857.706733	35.933133
1328.513976	147069.981420	35.938151
1329.619017	147307.260604	35.943168
1331.362310	147523.180801	35.948186
1332.537980	147748.799101	35.953204
1334.030845	147963.313344	35.958221
1335.395013	148180.856798	35.963239
1336.650926	148404.015636	35.968256
1337.961177	148617.088751	35.973274
1338.714689	148824.499964	35.978292
1340.547879	149036.858258	35.983309
1341.956777	149244.676237	35.988327
1342.854935	149438.752195	35.993344
1344.241640	149649.240765	35.998362
1345.214267	149876.918086	36.003380
1347.036226	150080.016237	36.008397
1348.636526	150288.252548	36.013415
1349.820234	150504.488203	36.018432
1351.005672	150709.960453	36.023450
1352.367458	150933.392470	36.028468
1353.606439	151146.753299	36.033485
1354.792078	151362.636627	36.038503
1355.883984	151595.532186	36.043520
1357.324258	151803.266176	36.048538
1358.684473	152045.007175	36.053556
1360.079024	152258.995325	36.058573
1361.483195	152494.232199	36.063591
1362.710757	152728.406035	36.068608
1364.285618	152959.391093	36.073626
1365.202709	153194.618286	36.078644
1366.698166	153422.152219	36.083661
1368.100867	153658.714364	36.088679
1369.576797	153905.979861	36.093696
1370.977901	154135.879829	36.098714
1372.431003	154367.714797	36.103732
1373.750982	154601.475678	36.108749
1375.167254	154844.590841	36.113767
1376.646693	155090.553373	36.118784
1378.085537	155321.721603	36.123802
1379.250202	155572.572020	36.128820
1380.671242	155798.921027	36.133837
1382.118820	156054.019975	36.138855
1383.753792	156286.113409	36.143872
1385.248448	156521.162190	36.148890
1386.479164	156773.048351	36.153908
1388.123024	157023.182504	36.158925
1389.435641	157255.545998	36.163943
1390.976212	157508.656248	36.168960
1392.348220	157737.673557	36.173978
1393.460443	157972.610179	36.178996
1395.011923	158219.044139	36.184013
1396.591395	158464.636841	36.189031
1397.879553	158707.292773	36.194048
1399.513666	158949.578136	36.199066
1400.793319	159199.384741	36.204084
1401.952119	159441.175152	36.209101
1403.277866	159681.074162	36.214119
1405.091376	159941.007256	36.219136
1406.667531	160183.941296	36.224154
1408.183803	160420.931465	36.229172
1409.496340	160655.910437	36.234189
1410.825079	160908.026794	36.239207
1412.179771	161146.581150	36.244224
1413.692068	161383.867555	36.249242
1415.241385	161634.124090	36.254260
1416.808104	161870.273864	36.259277
1418.656489	162111.979281	36.264295
1419.584017	162348.027722	36.269312
1421.307845	162590.858968	36.274330
1422.894866	162825.269715	36.279348
1424.353686	163070.645336	36.284365
1425.705876	163314.413471	36.289383
1427.060029	163551.262822	36.294400
1428.558193	163781.755101	36.299418
1429.695167	164024.937435	36.304436
1430.992294	164253.164805	36.309453
1432.770513	164482.181003	36.314471
1434.034628	164712.738529	36.319488
1435.585723	164928.359083	36.324506
1436.946106	165149.456936	36.329524
1438.274699	165367.830750	36.334541
1439.661301	165587.351566	36.339559
1440.742852	165820.074447	36.344576
1442.163957	166043.412985	36.349594
1443.824643	166270.841151	36.354612
1444.788425	166502.277022	36.359629
1446.350988	166739.942904	36.364647
1447.906791	166978.232796	36.369664
1449.458173	167212.473917	36.374682
1450.532979	167446.320630	36.379700
1452.031777	167684.990054	36.384717
1453.604423	167928.029163	36.389735
1454.771024	168181.201350	36.394752
1456.125224	168417.546929	36.399770
1457.515224	168670.178002	36.404788
1459.020496	168915.402208	36.409805
1460.659044	169159.425553	36.414823
1461.786383	169425.318098	36.419840
1463.862776	169674.543973	36.424858
1465.178666	169923.470718	36.429876
1466.210199	170179.020020	36.434893
1467.842788	170427.771924	36.439911
1469.164631	170698.882635	36.444928
1470.807036	170951.316999	36.449946
1472.490961	171211.630857	36.454964
1473.533448	171476.375868	36.459981
1475.704582	171728.082507	36.464999
1476.877145	171997.202338	36.470016
1478.525812	172258.363347	36.475034
1479.876234	172513.832560	36.480052
1481.113580	172787.414611	36.485069
1482.749985	173046.040653	36.490087
1484.098438	173312.407511	36.495104
1485.745481	173573.077983	36.500122
1487.625709	173847.299598	36.505140
1488.740839	174119.876894	36.510157
1490.541682	174381.910034	36.515175
1491.965804	174654.301115	36.520192
1493.726784	174909.104327	36.525210
1494.834331	175174.956404	36.530228
1496.535007	175448.754462	36.535245
1498.297287	175720.435891	36.540263
1499.821932	175981.895217	36.545280
1501.591004	176236.180672	36.550298
1503.121866	176510.250103	36.555316
1504.480704	176772.106119	36.560333
1506.191033	177033.247621	36.565351
1507.839804	177292.164636	36.570368
1509.011194	177547.271418	36.575386
1510.936038	177820.648515	36.580404
1512.453738	178081.569411	36.585421
1514.019787	178340.604134	36.590439
1515.136765	178604.230634	36.595456
1516.330784	178862.004476	36.600474
1518.284434	179124.460301	36.605492
1519.513176	179403.310179	36.610509
1521.373884	179669.464809	36.615527
1522.720009	179931.179983	36.620544
1524.208038	180204.683666	36.625562
1525.605755	180465.808169	36.630580
1527.044487	180734.114610	36.635597
1528.778253	180989.321101	36.640615
1530.306547	181262.974044	36.645632
1531.812640	181532.796154	36.650650
1533.343054	181802.691434	36.655668
1534.818768	182059.211164	36.660685
1536.479096	182303.308312	36.665703
1537.831245	182548.038484	36.670720
1538.971288	182801.183975	36.675738
1540.432385	183055.575210	36.680756
1541.951846	183313.056611	36.685773
1544.013399	183569.691892	36.690791
1545.406387	183820.768567	36.695808
1546.877878	184088.952387	36.700826
1548.329145	184339.005309	36.705844
1549.753968	184603.616585	36.710861
1551.172180	184912.500058	36.715879
1552.374001	185216.363924	36.720896
1553.928307	185486.240258	36.725914
1555.647475	185753.932568	36.730932
1556.854249	186028.131785	36.735949
1558.393121	186305.683264	36.740967
1559.687830	186584.188072	36.745984
1561.411206	186870.297173	36.751002
1563.241014	187157.330172	36.756020
1564.893538	187443.426503	36.761037
1566.436231	187722.530468	36.766055
1567.836931	188005.086341	36.771072
1569.710708	188287.924502	36.776090
1571.233640	188581.206854	36.781108
1572.231881	188886.967277	36.786125
1574.528156	189175.659767	36.791143
1575.977293	189474.823415	36.796160
1577.539569	189764.521284	36.801178
1579.349677	190050.345664	36.806196
1580.821141	190347.603077	36.811213
1582.251769	190634.758301	36.816231
1584.044079	190942.482754	36.821248
1585.568726	191228.278484	36.826266
1587.150841	191514.243707	36.831284
1588.717667	191815.299953	36.836301
1590.857294	192108.240690	36.841319
1592.344953	192422.011149	36.846336
1593.858048	192704.764066	36.851354
1595.620908	192999.645535	36.856372
1597.233895	193300.342553	36.861389
1598.860856	193600.276064	36.866407
1600.849236	193901.982586	36.871424
1602.253608	194182.926926	36.876442
1604.000322	194476.645861	36.881460
1605.614980	194780.190972	36.886477
1606.961622	195064.168960	36.891495
1608.820463	195360.895039	36.896512
1610.430334	195664.620700	36.901530
1612.067078	195950.409434	36.906548
1613.924646	196240.736458	36.911565
1615.516591	196535.576319	36.916583
1616.959319	196834.021767	36.921600
1618.909266	197119.027207	36.926618
1620.439482	197408.950615	36.931636
1622.113390	197714.143944	36.936653
1623.649496	198000.536759	36.941671
1625.172536	198279.032204	36.946688
1626.559565	198573.501818	36.951706
1628.582155	198864.316267	36.956724
1629.724017	199176.251118	36.961741
1631.693998	199461.562696	36.966759
1633.049248	199758.046291	36.971776
1634.494544	200068.893934	36.976794
1636.704613	200358.716519	36.981812
1638.153805	200655.364874	36.986829
1640.049458	200947.676315	36.991847
1641.369269	201239.290914	36.996864
1643.236190	201521.015095	37.001882
1644.863787	201790.355436	37.006900
1646.056042	202068.985399	37.011917
1647.618662	202348.472331	37.016935
1649.456797	202630.126601	37.021952
1650.773802	202918.873967	37.026970
1652.401693	203192.509415	37.031988
1653.977646	203490.717716	37.037005
1655.617769	203777.028013	37.042023
1657.255203	204068.318089	37.047040
1658.880189	204369.009562	37.052058
1660.416309	204656.023320	37.057076
1661.960157	204970.293487	37.062093
1664.040525	205258.035830	37.067111
1665.267534	205554.523702	37.072128
1667.113256	205853.709493	37.077146
1668.729764	206148.257441	37.082164
1669.858599	206463.077485	37.087181
1671.710543	206765.007105	37.092199
1673.178222	207082.620153	37.097216
1674.832561	207407.266500	37.102234
1676.707240	207720.752258	37.107252
1678.629820	208051.454287	37.112269
1680.183950	208366.616877	37.117287
1681.775220	208680.834149	37.122304
1683.691733	209005.670294	37.127322
1685.446924	209327.610729	37.132340
1686.950771	209658.939327	37.137357
1688.551155	209980.930208	37.142375
1690.150853	210305.182487	37.147392
1691.876653	210629.110578	37.152410
1693.671700	210959.480686	37.157428
1695.504147	211290.556623	37.162445
1697.360283	211622.162703	37.167463
1699.290657	211958.431785	37.172480
1700.667049	212287.014442	37.177498
1702.364093	212611.304867	37.182516
1704.276220	212941.481001	37.187533
1706.011730	213275.597266	37.192551
1707.777361	213608.591385	37.197568
1709.273395	213941.704224	37.202586
1710.967640	214269.603998	37.207604
1713.112478	214613.717341	37.212621
1714.840213	214941.561655	37.217639
1716.486779	215280.393375	37.222656
1718.116209	215616.865506	37.227674
1720.422521	215939.691748	37.232692
1721.731369	216275.173010	37.237709
1723.619661	216609.877940	37.242727
1725.482313	216937.677270	37.247744
1727.093977	217273.188071	37.252762
1728.946212	217599.033369	37.257780
1730.743459	217936.547871	37.262797
1732.553315	218267.862047	37.267815
1734.617275	218613.794727	37.272832
1736.092243	218941.198670	37.277850
1737.784345	219276.494843	37.282868
1739.616441	219604.021059	37.287885
1741.446876	219920.242907	37.292903
1743.144600	220254.319268	37.297920
1744.680162	220584.915391	37.302938
1746.852710	220911.525144	37.307956
1748.505267	221242.001586	37.312973
1750.101220	221579.168260	37.317991
1752.060672	221911.934062	37.323008
1753.510354	222229.384871	37.328026
1755.488054	222557.651471	37.333044
1757.140457	222880.405559	37.338061
1758.748120	223203.801812	37.343079
1760.434574	223503.814040	37.348096
1761.951907	223826.309980	37.353114
1763.715466	224128.342544	37.358132
1765.535860	224443.576366	37.363149
1766.937925	224767.614678	37.368167
1769.055535	225086.434811	37.373184
1770.461246	225410.142321	37.378202
1772.459163	225735.891100	37.383220
1774.211420	226061.602099	37.388237
1775.672535	226397.113807	37.393255
1777.833641	226708.534494	37.398272
1779.387786	227037.960005	37.403290
1781.004280	227372.151680	37.408308
1782.897765	227707.239905	37.413325
1784.468083	228042.810504	37.418343
1786.187182	228373.378552	37.423360
1788.069559	228726.479766	37.428378
1789.996421	229066.160580	37.433396
1791.154824	229411.931488	37.438413
1793.015806	229768.236622	37.443431
1794.883232	230117.300466	37.448448
1796.381211	230464.008598	37.453466
1798.320963	230822.104651	37.458484
1800.313873	231188.270679	37.463501
1802.177036	231541.704027	37.468519
1803.849757	231899.358638	37.473536
1805.575431	232264.625938	37.478554
1807.515386	232625.108948	37.483572
1809.643207	232996.968682	37.488589
1811.305160	233359.908080	37.493607
1813.253567	233723.462895	37.498624
1814.857240	234094.286076	37.503642
1816.704475	234453.994781	37.508660
1818.924997	234816.744049	37.513677
1820.684368	235188.710535	37.518695
1822.551871	235552.886215	37.523712
1824.607116	235928.286043	37.528730
1826.314227	236286.643281	37.533748
1828.141306	236662.306718	37.538765
1829.741580	237030.282541	37.543783
1832.337782	237395.942825	37.548800
1834.030838	237767.459850	37.553818
1835.747841	238132.545602	37.558836
1837.598280	238501.395185	37.563853
1839.500493	238871.176157	37.568871
1841.623733	239230.532065	37.573888
1843.534607	239612.860084	37.578906
1845.367346	239973.251263	37.583924
1847.593331	240343.919620	37.588941
1849.258383	240705.707863	37.593959
1851.304326	241061.923493	37.598976
1852.917680	241425.319243	37.603994
1854.776799	241785.373594	37.609012
1856.894775	242155.192557	37.614029
1858.818887	242520.443317	37.619047
1860.559300	242875.027543	37.624064
1862.396345	243237.953726	37.629082
1863.988971	243599.850648	37.634100
1866.159725	243967.067362	37.639117
1867.729163	244332.243704	37.644135
1869.916925	244704.384684	37.649152
1871.375975	245070.262911	37.654170
1873.543966	245429.374018	37.659188
1875.705051	245791.559307	37.664205
1877.125477	246153.199363	37.669223
1879.079247	246520.013655	37.674240
1881.106379	246887.781069	37.679258
1882.873522	247223.886013	37.684276
1884.708170	247561.859577	37.689293
1886.343735	247915.130574	37.694311
1888.406751	248257.487150	37.699328
1890.145890	248616.075076	37.704346
1891.732279	248961.172120	37.709364
1893.811562	249305.657902	37.714381
1895.207546	249669.860439	37.719399
1897.450222	250020.060106	37.724416
1899.024548	250391.142557	37.729434
1900.790425	250745.682840	37.734452
1902.992497	251107.292056	37.739469
1904.053728	251473.702114	37.744487
1906.401854	251836.861722	37.749504
1908.552830	252212.726841	37.754522
1909.985156	252592.132717	37.759540
1912.231537	252965.948889	37.764557
1913.859301	253356.930817	37.769575
1916.049942	253736.977148	37.774592
1917.514539	254126.229819	37.779610
1919.446162	254510.607475	37.784628
1921.232684	254893.787513	37.789645
1923.300799	255291.959995	37.794663
1925.602204	255687.326078	37.799680
1927.368800	256088.464537	37.804698
1929.476221	256467.322518	37.809716
1931.630521	256853.512958	37.814733
1933.345183	257256.738851	37.819751
1935.220238	257653.994580	37.824768
1937.091427	258054.704167	37.829786
1938.929131	258458.948401	37.834804
1941.324405	258858.277955	37.839821
1943.436749	259269.944314	37.844839
1945.225189	259668.350125	37.849856
1947.288565	260063.180935	37.854874
1949.281115	260459.799519	37.859892
1951.693642	260866.790504	37.864909
1953.301712	261269.410105	37.869927
1955.598894	261669.685257	37.874944
1957.164094	262075.204292	37.879962
1959.321119	262476.057283	37.884980
1961.704747	262874.612782	37.889997
1963.452456	263281.876788	37.895015
1965.482962	263680.255973	37.900032
1967.625190	264077.219219	37.905050
1969.459786	264477.099226	37.910068
1971.822646	264879.892153	37.915085
1973.415567	265279.502091	37.920103
1975.835316	265674.434671	37.925120
1977.778900	266085.416136	37.930138
1979.693400	266478.164113	37.935156
1981.975677	266869.202073	37.940173
1984.164345	267284.254818	37.945191
1985.661644	267671.907380	37.950208
1987.762328	268064.772244	37.955226
1989.806885	268468.870323	37.960244
1992.066581	268861.275245	37.965261
1993.758747	269270.098291	37.970279
1995.908775	269662.948768	37.975296
1998.248428	270057.139384	37.980314
1999.914787	270453.770236	37.985332
2002.229098	270857.282321	37.990349
2003.890709	271256.577133	37.995367
2006.026150	271642.995716	38.000384
2008.264713	272033.155272	38.005402
2010.013178	272434.234367	38.010420
2012.056338	272827.824156	38.015437
2014.078530	273216.310634	38.020455
2016.136409	273590.491335	38.025472
2018.108888	273966.613893	38.030490
2019.758008	274338.493329	38.035508
2022.194180	274704.863904	38.040525
2023.939685	275086.223201	38.045543
2025.722019	275457.467247	38.050560
2027.418869	275839.440152	38.055578
2029.559854	276228.732009	38.060596
2031.863628	276603.114502	38.065613
2033.593469	276994.828772	38.070631
2035.558225	277378.580898	38.075648
2037.386703	277769.666383	38.080666
2039.089998	278177.860597	38.085684
2041.523947	278567.780717	38.090701
2043.490952	278975.726276	38.095719
2045.544306	279382.107042	38.100736
2047.297666	279784.951881	38.105754
2048.704044	280194.400682	38.110772
2051.065357	280607.583195	38.115789
2053.280980	281042.168308	38.120807
2055.095200	281452.638281	38.125824
2057.044720	281874.689893	38.130842
2059.072542	282303.938682	38.135860
2061.603152	282729.652670	38.140877
2063.577191	283158.549217	38.145895
2065.533720	283597.450949	38.150912
2067.589927	284029.757452	38.155930
2069.567290	284454.734961	38.160948
2071.791103	284889.828519	38.165965
2073.413673	285330.091960	38.170983
2075.735682	285781.492098	38.176000
2077.982177	286216.751364	38.181018
2079.887867	286670.369038	38.186036
2081.957214	287119.082708	38.191053
2084.058029	287561.084906	38.196071
2086.266983	288011.141820	38.201088
2088.702833	288462.074225	38.206106
2090.363301	288919.345714	38.211124
2092.873854	289373.535552	38.216141
2094.958226	289825.351277	38.221159
2097.068340	290275.001515	38.226176
2099.787236	290728.006435	38.231194
2101.593606	291173.305135	38.236212
2103.694577	291624.546683	38.241229
2105.818038	292077.533329	38.246247
2107.904060	292524.200354	38.251264
2109.836780	292965.048408	38.256282
2112.289382	293429.805143	38.261300
2114.682056	293877.048911	38.266317
2116.984294	294337.962899	38.271335
2119.010377	294786.348901	38.276352
2121.546195	295233.610787	38.281370
2123.585452	295678.230339	38.286388
2125.446897	296120.640112	38.291405
2127.858393	296580.732246	38.296423
2130.098031	297019.800833	38.301440
2132.642780	297455.568643	38.306458
2134.626533	297909.446136	38.311476
2136.724914	298343.753651	38.316493
2138.464570	298788.827354	38.321511
2140.721765	299237.142232	38.326528
2143.122301	299674.184647	38.331546
2145.196978	300125.846520	38.336564
2147.762425	300560.418927	38.341581
2149.720134	301001.023319	38.346599
2151.449977	301446.102319	38.351616
2153.660836	301878.917155	38.356634
2155.582258	302326.522821	38.361652
2158.368652	302739.262094	38.366669
2160.334985	303151.618721	38.371687
2162.456679	303564.557039	38.376704
2164.344565	303976.970196	38.381722
2166.236945	304399.457073	38.386740
2168.341878	304811.042697	38.391757
2170.493383	305239.777472	38.396775
2172.445086	305667.397621	38.401792
2174.968071	306092.132574	38.406810
2176.899773	306518.784074	38.411828
2178.763613	306957.550432	38.416845
2181.058521	307394.595592	38.421863
2182.778602	307831.726836	38.426880
2185.028521	308281.462667	38.431898
2187.149816	308726.493367	38.436916
2189.626119	309176.693215	38.441933
2191.559326	309634.385395	38.446951
2193.629309	310089.234472	38.451968
2195.871904	310543.519232	38.456986
2198.168430	311010.202674	38.462004
2200.312288	311461.879864	38.467021
2202.594274	311939.597177	38.472039
2204.347840	312413.534471	38.477056
2207.267622	312881.853149	38.482074
2209.365847	313353.671178	38.487092
2211.462445	313824.900919	38.492109
2213.955143	314290.125076	38.497127
2215.893864	314761.547562	38.502144
2218.445455	315235.381809	38.507162
2220.259994	315714.402142	38.512180
2222.841477	316196.038273	38.517197
2224.937942	316673.050151	38.522215
2227.299002	317151.106784	38.527232
2229.438753	317631.603758	38.532250
2231.461217	318126.172877	38.537268
2234.011031	318613.522986	38.542285
2236.470310	319088.269580	38.547303
2238.449282	319582.194599	38.552320
2240.832993	320070.239516	38.557338
2243.190747	320566.580865	38.562356
2245.408497	321051.925354	38.567373
2248.080848	321540.263601	38.572391
2249.950406	322032.274302	38.577408
2252.570237	322509.444557	38.582426
2254.897971	323013.374329	38.587444
2257.443679	323495.340687	38.592461
2259.601452	323991.140111	38.597479
2261.671474	324471.317229	38.602496
2264.407773	324946.005383	38.607514
2266.772856	325450.812997	38.612532
2268.974077	325936.509044	38.617549
2271.268267	326411.502982	38.622567
2273.511955	326904.513338	38.627584
2275.706674	327378.724873	38.632602
2277.871400	327872.750514	38.637620
2280.087330	328348.773914	38.642637
2282.905471	328842.025602	38.647655
2284.898842	329337.632724	38.652672
2287.575673	329813.008153	38.657690
2289.398638	330300.866452	38.662708
2291.794636	330783.453599	38.667725
2294.139788	331276.951410	38.672743
2296.324244	331767.449129	38.677760
2298.599609	332248.362405	38.682778
2300.892944	332742.280681	38.687796
2303.347069	333235.685377	38.692813
2305.859056	333722.022394	38.697831
2307.984100	334192.762073	38.702848
2310.164968	334651.843687	38.707866
2312.522089	335116.269786	38.712884
2314.643290	335571.493648	38.717901
2316.958966	336029.801488	38.722919
2318.974443	336498.423658	38.727936
2321.292331	336963.238458	38.732954
2323.664291	337436.789793	38.737972
2325.754606	337910.353642	38.742989
2328.142613	338374.429192	38.748007
2330.390094	338857.848101	38.753024
2332.612068	339329.166022	38.758042
2334.719985	339814.039568	38.763060
2336.736790	340313.301546	38.768077
2339.041521	340799.272168	38.773095
2341.274540	341299.779870	38.778112
2343.794728	341806.271637	38.783130
2346.231650	342304.983101	38.788148
2348.512723	342808.226076	38.793165
2350.948059	343311.970183	38.798183
2352.760629	343842.305956	38.803200
2355.068978	344347.424227	38.808218
2357.421667	344870.812386	38.813236
2359.871084	345396.408976	38.818253
2362.622806	345910.335775	38.823271
2364.785581	346437.685413	38.828288
2367.257658	346957.548481	38.833306
2369.528465	347495.286735	38.838324
2371.746636	348021.943425	38.843341
2374.369450	348545.206705	38.848359
2376.567502	349091.450343	38.853376
2379.188816	349620.883729	38.858394
2381.487087	350166.764148	38.863412
2383.821649	350699.850738	38.868429
2386.333968	351240.177574	38.873447
2388.597988	351786.796726	38.878464
2391.076035	352326.121894	38.883482
2393.564951	352875.805841	38.888500
2396.140862	353425.568113	38.893517
2398.959623	353966.257353	38.898535
2401.178179	354514.104477	38.903552
2403.614202	355062.516487	38.908570
2406.094153	355612.306345	38.913588
2408.369165	356159.101826	38.918605
2411.132171	356698.713248	38.923623
2413.290544	357264.216050	38.928640
2415.927796	357807.883737	38.933658
2418.645137	358365.471212	38.938676
2420.978787	358914.794206	38.943693
2423.696216	359444.655959	38.948711
2425.993184	359994.750940	38.953728
2428.889126	360538.304018	38.958746
2431.242858	361086.697257	38.963764
2433.570392	361627.810171	38.968781
2436.429586	362173.240269	38.973799
2438.576769	362719.329314	38.978816
2440.845079	363251.804480	38.983834
2443.517240	363794.015137	38.988852
2445.743718	364343.609880	38.993869
2448.892728	364892.543116	38.998887
2451.355817	365429.712772	39.003904
2453.598199	365962.421372	39.008922
2455.948067	366492.366393	39.013940
2458.464042	367043.461225	39.018957
2461.185273	367587.645921	39.023975
2463.419635	368119.327456	39.028992
2466.199761	368646.327120	39.034010
2468.475392	369185.660286	39.039028
2470.904637	369722.653255	39.044045
2473.599092	370235.902801	39.049063
2476.041241	370742.898522	39.054080
2478.263815	371246.574792	39.059098
2481.062406	371756.156793	39.064116
2482.954532	372251.403857	39.069133
2485.416338	372752.253633	39.074151
2487.393944	373274.097524	39.079168
2489.525787	373794.969954	39.084186
2492.095005	374316.752113	39.089204
2494.177845	374854.333064	39.094221
2496.816358	375380.568169	39.099239
2499.668656	375919.299667	39.104256
2501.784912	376456.919536	39.109274
2504.442334	377002.727709	39.114292
2506.654388	377548.949054	39.119309
2509.271727	378084.988579	39.124327
2511.636579	378648.819441	39.129344
2514.305176	379198.557766	39.134362
2516.957119	379757.431298	39.139380
2519.270721	380319.157411	39.144397
2521.850191	380875.004274	39.149415
2524.142801	381437.266862	39.154432
2526.636019	382007.236164	39.159450
2529.221469	382582.522504	39.164468
2531.540217	383163.738802	39.169485
2534.285399	383742.823855	39.174503
2536.742516	384329.842373	39.179520
2539.090067	384899.567698	39.184538
2541.770694	385497.110098	39.189556
2544.368476	386081.964230	39.194573
2546.998856	386662.342851	39.199591
2549.565739	387266.698330	39.204608
2551.914217	387859.172133	39.209626
2554.547971	388452.954589	39.214644
2556.934732	389061.700637	39.219661
2559.974879	389659.847057	39.224679
2562.815139	390267.125198	39.229696
2564.740050	390867.543530	39.234714
2567.924992	391477.016488	39.239732
2570.529529	392074.260702	39.244749
2573.194836	392676.544103	39.249767
2575.954754	393282.038200	39.254784
2578.589771	393889.612511	39.259802
2581.146651	394492.373848	39.264820
2583.891715	395100.963498	39.269837
2586.751608	395704.406308	39.274855
2589.516924	396302.127851	39.279872
2591.790098	396909.378114	39.284890
2594.773952	397509.515570	39.289908
2597.229847	398111.947662	39.294925
2600.166515	398701.785724	39.299943
2602.985624	399297.195429	39.304960
2605.083819	399895.992845	39.309978
2608.206385	400499.929370	39.314996
2610.446202	401104.190640	39.320013
2613.257484	401701.716207	39.325031
2616.124727	402300.938306	39.330048
2618.519213	402901.990055	39.335066
2621.464094	403498.637996	39.340084
2623.759909	404091.778541	39.345101
2626.807003	404678.308262	39.350119
2629.208320	405285.925374	39.355136
2631.843684	405880.534591	39.360154
2634.694533	406466.339895	39.365172
2637.400000	407067.383874	39.370189
2640.448960	407664.512231	39.375207
2642.963275	408260.594944	39.380224
2645.093264	408847.917607	39.385242
2648.068569	409411.463653	39.390260
2650.773243	409968.561326	39.395277
2653.173338	410512.537924	39.400295
2655.751407	411075.091408	39.405312
2658.095487	411637.616361	39.410330
2660.988291	412197.561983	39.415348
2663.290210	412767.399826	39.420365
2666.028063	413327.947454	39.425383
2668.684740	413891.427183	39.430400
2670.919601	414469.020752	39.435418
2673.683873	415046.313581	39.440436
2676.143267	415626.622812	39.445453
2678.755052	416198.698231	39.450471
2681.612724	416794.896808	39.455488
2683.963937	417383.722760	39.460506
2686.665207	417972.123453	39.465524
2689.055440	418584.478421	39.470541
2691.779549	419184.574946	39.475559
2694.386907	419795.444372	39.480576
2697.076217	420410.682688	39.485594
2699.660705	421024.098624	39.490612
2702.246686	421647.609672	39.495629
2704.762317	422262.769387	39.500647
2707.836270	422898.908853	39.505664
2710.478475	423538.534342	39.510682
2713.311533	424162.435807	39.515700
2716.020015	424805.803209	39.520717
2718.726043	425435.954797	39.525735
2721.810279	426071.083245	39.530752
2724.482117	426708.227786	39.535770
2727.311643	427348.310083	39.540788
2729.871507	428001.456468	39.545805
2732.479983	428632.028376	39.550823
2735.629327	429279.631699	39.555840
2738.448223	429934.392643	39.560858
2741.167282	430587.732196	39.565876
2743.928218	431233.714652	39.570893
2746.925180	431889.898937	39.575911
2749.512738	432528.992027	39.580928
2752.304000	433188.298298	39.585946
2755.077968	433841.520445	39.590964
2758.044545	434501.613742	39.595981
2760.836210	435140.437183	39.600999
2763.625838	435805.971057	39.606016
2765.997636	436466.847864	39.611034
2769.054514	437114.962590	39.616052
2772.181241	437781.334955	39.621069
2774.939852	438438.141777	39.626087
2777.911105	439099.085956	39.631104
2780.680453	439758.017694	39.636122
2783.454437	440414.702753	39.641140
2786.703619	441063.056091	39.646157
2789.264080	441727.154590	39.651175
2791.837351	442386.529590	39.656192
2795.070655	443041.787475	39.661210
2798.103031	443688.719327	39.666228
2800.507258	444344.666795	39.671245
2803.487394	445001.712982	39.676263
2806.289679	445645.884604	39.681280
2808.931561	446302.128941	39.686298
2812.173703	446955.074179	39.691316
2814.865112	447604.395592	39.696333
2818.045592	448259.424522	39.701351
2820.459929	448911.317753	39.706368
2823.408104	449564.416759	39.711386
2826.133456	450206.923426	39.716404
2829.012957	450861.349223	39.721421
2831.726972	451505.881091	39.726439
2834.735396	452124.746634	39.731456
2837.239815	452739.226700	39.736474
2840.446134	453358.119188	39.741492
2842.834364	453969.141774	39.746509
2845.458710	454594.745440	39.751527
2848.407351	455219.973223	39.756544
2850.670780	455842.206757	39.761562
2853.650262	456472.735396	39.766580
2856.215067	457107.545748	39.771597
2858.642790	457756.284287	39.776615
2861.554245	458400.784402	39.781632
2863.976364	459060.880831	39.786650
2867.207550	459711.691223	39.791668
2869.763289	460376.308543	39.796685
2872.088922	461049.110746	39.801703
2875.096035	461717.944942	39.806720
2877.833647	462392.193898	39.811738
2880.679688	463077.902875	39.816756
2883.856106	463770.293093	39.821773
2886.461800	464466.527941	39.826791
2889.302618	465153.414567	39.831808
2892.256407	465862.653775	39.836826
2895.307139	466559.488753	39.841844
2898.105046	467270.861574	39.846861
2901.089592	467981.367683	39.851879
2904.024519	468694.877346	39.856896
2906.792492	469415.191132	39.861914
2909.973899	470132.382701	39.866932
2912.869527	470845.805224	39.871949
2915.667445	471576.811764	39.876967
2918.828856	472292.650971	39.881984
2921.569519	473033.333495	39.887002
2924.726857	473757.529666	39.892020
2927.673778	474488.633859	39.897037
2930.577452	475217.795741	39.902055
2933.694139	475944.622491	39.907072
2936.632127	476688.685578	39.912090
2940.089984	477420.886901	39.917108
2943.136756	478156.798645	39.922125
2946.379444	478896.829345	39.927143
2949.365848	479621.744268	39.932160
2951.792180	480356.592189	39.937178
2955.303747	481102.626324	39.942196
2958.570222	481827.647726	39.947213
2961.489395	482565.893196	39.952231
2964.708881	483291.357876	39.957248
2967.869844	484021.987989	39.962266
2970.736506	484747.490127	39.967284
2973.798195	485474.590401	39.972301
2976.447342	486205.549946	39.977319
2979.547564	486934.791992	39.982336
2982.645891	487671.405160	39.987354
2985.698956	488404.010194	39.992372
2988.982204	489126.116736	39.997389
2991.943677	489873.676442	40.002407
2995.253045	490591.528306	40.007424
2997.988987	491321.473123	40.012442
3000.885687	492043.450344	40.017460
3004.276630	492769.545867	40.022477
3006.945797	493499.596619	40.027495
3010.012958	494224.815952	40.032512
3012.931843	494957.525806	40.037530
3016.041227	495681.005786	40.042548
3019.428705	496409.391418	40.047565
3022.190654	497134.969165	40.052583
3025.207115	497857.903806	40.057600
3028.334833	498590.299915	40.062618
3031.256784	499305.324687	40.067636
3034.393446	500001.807431	40.072653
3037.105199	500687.551819	40.077671
3040.326101	501378.167020	40.082688
3043.178946	502067.649252	40.087706
3045.878269	502750.731067	40.092724
3048.934451	503445.399935	40.097741
3051.908783	504144.929226	40.102759
3054.582585	504837.627909	40.107776
3057.158271	505551.189899	40.112794
3060.142130	506255.394488	40.117812
3063.729243	506966.614155	40.122829
3066.086069	507701.233426	40.127847
3069.051717	508416.099712	40.132864
3072.123087	509157.624738	40.137882
3074.797173	509896.406201	40.142900
3077.917706	510633.620276	40.147917
3081.123007	511389.039737	40.152935
3083.789721	512133.287065	40.157952
3086.990231	512903.713140	40.162970
3089.846031	513669.574126	40.167988
3093.360176	514440.167422	40.173005
3095.999680	515211.407525	40.178023
3099.279091	515986.928924	40.183040
3102.476854	516773.832012	40.188058
3105.604437	517550.042789	40.193076
3108.820332	518334.791888	40.198093
3111.575000	519127.258805	40.203111
3114.974643	519912.239900	40.208128
3118.558516	520713.783337	40.213146
3121.664321	521515.002065	40.218164
3124.982717	522296.037421	40.223181
3128.051605	523100.936500	40.228199
3131.083220	523907.501461	40.233216
3134.158137	524705.770368	40.238234
3137.837698	525507.866086	40.243252
3140.853147	526311.474099	40.248269
3143.852369	527124.179095	40.253287
3147.113267	527930.664451	40.258304
3150.306911	528750.120841	40.263322
3153.624909	529557.351281	40.268340
3156.877092	530366.852536	40.273357
3159.825539	531187.801687	40.278375
3163.442606	531997.747145	40.283392
3166.534872	532804.158716	40.288410
3169.621575	533611.374477	40.293428
3172.983112	534421.760356	40.298445
3175.671366	535250.877226	40.303463
3179.539611	536060.578367	40.308480
3183.167116	536883.468467	40.313498
3185.967585	537693.584380	40.318516
3189.210352	538503.981078	40.323533
3192.397281	539332.302866	40.328551
3195.957950	540142.494797	40.333568
3199.385174	540957.222265	40.338586
3202.418857	541760.366749	40.343604
3205.431576	542576.860455	40.348621
3208.878963	543389.871239	40.353639
3212.392344	544198.805041	40.358656
3215.352236	545007.421602	40.363674
3218.761139	545831.717020	40.368692
3222.149398	546624.409484	40.373709
3225.008743	547462.325848	40.378727
3228.436295	548254.907285	40.383744
3231.727151	549069.776165	40.388762
3234.533826	549889.029358	40.393780
3238.138810	550687.894579	40.398797
3241.111804	551496.383150	40.403815
3244.519305	552293.168142	40.408832
3247.979865	553083.074128	40.413850
3250.855583	553842.139006	40.418868
3253.978216	554602.170172	40.423885
3256.747453	555372.684678	40.428903
3260.178850	556156.178067	40.433920
3263.401594	556926.722190	40.438938
3266.424496	557706.669471	40.443956
3269.533857	558490.310528	40.448973
3272.174977	559278.432744	40.453991
3275.600429	560066.580322	40.459008
3278.670664	560867.055920	40.464026
3282.083136	561676.190868	40.469044
3285.260967	562484.304900	40.474061
3287.858087	563311.338512	40.479079
3291.172133	564134.194528	40.484096
3294.564820	564961.638043	40.489114
3297.770315	565796.614164	40.494132
3300.814893	566644.825797	40.499149
3304.032544	567494.850994	40.504167
3307.052752	568346.797178	40.509184
3310.395781	569197.628522	40.514202
3313.618459	570068.390466	40.519220
3317.340204	570937.806763	40.524237
3320.298386	571815.985727	40.529255
3323.854754	572695.504978	40.534272
3327.692175	573574.912171	40.539290
3330.422567	574448.919424	40.544308
3333.991837	575336.088338	40.549325
3337.587473	576226.335468	40.554343
3340.909405	577120.507293	40.559360
3344.121184	578007.220970	40.564378
3347.478195	578904.546523	40.569396
3350.699069	579808.973826	40.574413
3354.132539	580720.646483	40.579431
3357.519288	581618.898556	40.584448
3361.340461	582528.761297	40.589466
3364.575929	583449.741059	40.594484
3368.170311	584350.688180	40.599501
3371.910218	585273.036042	40.604519
3375.577943	586181.570095	40.609536
3378.726117	587088.010244	40.614554
3381.649814	587998.958262	40.619572
3385.804283	588901.840851	40.624589
3388.957831	589815.298924	40.629607
3392.079023	590732.682224	40.634624
3395.840431	591646.089869	40.639642
3399.404459	592571.591000	40.644660
3402.716687	593484.012847	40.649677
3406.235101	594403.567467	40.654695
3409.860277	595308.990631	40.659712
3413.460336	596216.937524	40.664730
3416.630605	597141.453493	40.669748
3420.304502	598042.090763	40.674765
3423.602234	598962.532182	40.679783
3426.799706	599882.609034	40.684800
3430.383350	600801.446407	40.689818
3433.835308	601714.033786	40.694836
3437.419362	602631.461940	40.699853
3440.722479	603557.437252	40.704871
3444.276650	604468.768504	40.709888
3447.864662	605381.311489	40.714906
3450.833589	606305.945101	40.719924
3454.204493	607221.302727	40.724941
3457.844115	608142.423209	40.729959
3461.256753	609072.923851	40.734976
3464.711220	609993.008500	40.739994
3468.165708	610921.887265	40.745012
3471.902176	611818.629736	40.750016
3475.217575	612696.098759	40.755021
3478.425265	613508.125061	40.760026
3481.584024	614267.161029	40.765031
3484.603457	614993.424601	40.770036
3487.383902	615650.605335	40.775040
3490.558269	616258.307455	40.780045
3492.854228	616809.493014	40.785050
3495.538650	617307.271206	40.790055
3497.672355	617752.846093	40.795060
3499.816529	618146.986325	40.800064
3501.825970	618494.716944	40.805069
3503.822621	618786.031547	40.810074
3506.336792	619038.138279	40.815079
3507.978785	619242.914265	40.820084
3509.349242	619410.410000	40.825088
3510.968259	619540.745898	40.830093
3512.010894	619630.805198	40.835098
3513.795067	619680.482887	40.840103
3514.672020	619703.075947	40.845108
3515.652362	619692.581678	40.850112
3516.574646	619658.566934	40.855117
3517.249984	619603.508890	40.860122
3518.162522	619512.194443	40.865127
3519.113993	619419.823958	40.870132
3519.906136	619295.254375	40.875136
3520.166611	619141.290447	40.880141
3520.750014	618981.228489	40.885146
3521.609263	618798.388627	40.890151
3521.464988	618610.806018	40.895156
3521.681801	618401.029862	40.900160
3521.707409	618191.379102	40.905165
3522.238602	617960.309791	40.910170
3522.393724	617722.048794	40.915175
3522.541252	617472.790423	40.920180
3522.722660	617228.217597	40.925184
3523.079899	616974.116978	40.930189
3523.003051	616709.283934	40.935194
3523.018812	616437.283290	40.940199
3523.171962	616169.801416	40.945204
3523.220292	615881.538972	40.950208
3523.207868	615612.668785	40.955213
3523.056819	615325.171157	40.960218
3523.292962	615039.204113	40.965223
3522.528238	614751.036273	40.970228
3522.548062	614460.438315	40.975232
3522.639703	614168.471164	40.980237
3522.515744	613883.527220	40.985242
3522.317978	613592.588321	40.990247
3522.413413	613308.743526	40.995252
3521.984925	613005.326656	41.000256
3522.120149	612718.709606	41.005261
3521.701158	612437.320311	41.010266
3521.599085	612141.775309	41.015271
3521.150189	611852.125376	41.020276
3520.986422	611570.872070	41.025280
3520.750116	611297.672028	41.030285
3521.014123	611010.086511	41.035290
3520.912515	610728.450137	41.040295
3520.911330	610453.690597	41.045300
3520.496573	610167.337398	41.050304
3520.327656	609896.389319	41.055309
3519.581680	609609.172101	41.060314
3519.759554	609335.004465	41.065319
3519.396224	609078.467307	41.070324
3519.413183	608801.459970	41.075328
3519.257110	608535.374762	41.080333
3518.763520	608283.639142	41.085338
3518.619651	608007.985802	41.090343
3518.337390	607759.505204	41.095348
3518.251477	607497.983495	41.100352
3517.874514	607254.757238	41.105357
3517.634453	607010.903581	41.110362
3517.722988	606759.189567	41.115367
3517.333702	606509.194803	41.120372
3516.795977	606268.071221	41.125376
3516.813518	606036.159658	41.130381
3516.594497	605799.977689	41.135386
3516.678996	605572.047223	41.140391
3516.355298	605340.123314	41.145396
3515.929273	605107.759929	41.150400
3516.155106	604884.294745	41.155405
3515.338858	604655.634349	41.160410
3515.334545	604441.251120	41.165415
3515.087818	604234.306195	41.170420
3514.935499	604008.729798	41.175424
3514.721957	603808.725881	41.180429
3514.217723	603608.863618	41.185434
3514.458367	603388.065749	41.190439
3513.843801	603203.774373	41.195444
3513.948563	602999.902229	41.200448
3513.726390	602800.580766	41.205453
3513.449572	602615.425512	41.210458
3513.593402	602426.798382	41.215463
3513.145473	602246.116992	41.220468
3513.034279	602054.370311	41.225472
3512.814309	601871.595011	41.230477
3512.629870	601684.957482	41.235482
3512.733264	601501.274371	41.240487
3512.502684	601335.356789	41.245492
3512.526974	601162.390071	41.250496
3511.850877	600979.870638	41.255501
3511.740420	600816.328353	41.260506
3511.654710	600640.817686	41.265511
3511.897567	600488.025837	41.270516
3511.714699	600322.685323	41.275520
3511.635528	600160.279076	41.280525
3511.026960	600005.911511	41.285530
3511.199751	599837.904983	41.290535
3510.715465	599694.174867	41.295540
3510.825226	599535.283271	41.300544
3510.762275	599384.074847	41.305549
3510.502166	599237.950798	41.310554
3510.258715	599085.564929	41.315559
3510.026049	598941.284587	41.320564
3509.988439	598796.120771	41.325568
3509.964243	598666.020765	41.330573
3509.513274	598527.225347	41.335578
3509.770976	598384.012083	41.340583
3509.210956	598248.634171	41.345588
3509.342235	598109.541977	41.350592
3509.284364	597993.556430	41.355597
3508.879096	597868.962974	41.360602
3509.127340	597730.698571	41.365607
3509.235246	597622.643187	41.370612
3508.938222	597489.267045	41.375616
3509.135538	597369.079337	41.380621
3508.760299	597243.772882	41.385626
3508.612665	597107.464719	41.390631
3508.327736	596988.299337	41.395636
3508.330602	596880.002438	41.400640
3508.317236	596771.006009	41.405645
3508.051418	596654.637711	41.410650
3507.741441	596537.574062	41.415655
3507.773372	596435.727043	41.420660
3507.631690	596318.935086	41.425664
3507.540097	596225.016503	41.430669
3507.571120	596116.256747	41.435674
3507.713838	596005.775964	41.440679
3507.512091	595917.479947	41.445684
3507.125130	595799.919452	41.450688
3507.643381	595698.490054	41.455693
3507.038483	595603.143998	41.460698
3507.084873	595505.542069	41.465703
3507.342926	595411.361322	41.470708
3507.202620	595319.745781	41.475712
3507.213664	595222.146774	41.480717
3506.919113	595120.488390	41.485722
3506.864204	595022.146712	41.490727
3506.788620	594931.118622	41.495732
3506.568881	594840.412754	41.500736
3506.289297	594761.183325	41.505741
3505.934450	594673.652065	41.510746
3506.081632	594589.146487	41.515751
3506.128057	594512.418256	41.520756
3506.210443	594410.894478	41.525760
3506.182194	594336.029595	41.530765
3506.044865	594254.169994	41.535770
3506.158130	594172.921638	41.540775
3506.034272	594094.664516	41.545780
3505.772781	594010.668967	41.550784
3505.784826	593943.357327	41.555789
3505.878203	593874.830577	41.560794
3506.173818	593791.046699	41.565799
3505.844708	593704.404934	41.570804
3505.451682	593632.146362	41.575808
3505.362465	593552.677848	41.580813
3505.646751	593484.569501	41.585818
3505.634416	593409.294953	41.590823
3505.347312	593339.872647	41.595828
3505.106866	593275.751600	41.600832
3505.237792	593198.449773	41.605837
3505.273650	593138.491871	41.610842
3505.264575	593061.060680	41.615847
3504.769828	593005.492369	41.620852
3504.737586	592929.015481	41.625856
3505.023512	592875.077481	41.630861
3504.773861	592813.659786	41.635866
3504.979947	592746.610793	41.640871
3504.942656	592687.212758	41.645876
3504.891409	592624.310417	41.650880
3505.251463	592551.275661	41.655885
3505.101551	592497.203539	41.660890
3505.289575	592428.752900	41.665895
3504.739309	592362.921700	41.670900
3504.795240	592298.598194	41.675904
3504.684290	592233.799491	41.680909
3504.520511	592187.391709	41.685914
3504.638733	592105.826326	41.690919
3504.607748	592059.998318	41.695924
3504.260556	591996.437286	41.700928
3504.284551	591946.242286	41.705933
3504.336614	591894.890562	41.710938
3504.412770	591846.840872	41.715943
3504.314001	591782.989281	41.720948
3504.433242	591725.565122	41.725952
3504.109648	591664.553135	41.730957
3504.054680	591622.183384	41.735962
3504.163481	591561.203399	41.740967
3503.803113	591509.162910	41.745972
3504.260770	591461.703069	41.750976
3504.261167	591410.707759	41.755981
3503.992567	591367.118058	41.760986
3503.985065	591308.358949	41.765991
3504.049594	591258.254584	41.770996
3504.110049	591212.809419	41.776000
3504.198686	591165.105392	41.781005
3503.828424	591116.270611	41.786010
3503.983088	591058.687065	41.791015
3503.834091	591015.878766	41.796020
3503.585227	590967.725669	41.801024
3503.497522	590924.506658	41.806029
3503.470940	590889.944543	41.811034
3503.796402	590842.452542	41.816039
3503.914783	590802.457083	41.821044
3503.726105	590747.380274	41.826048
3503.979612	590701.552093	41.831053
3503.775612	590657.047668	41.836058
3503.810167	590613.658005	41.841063
3503.766798	590570.781325	41.846068
3503.724379	590532.112536	41.851072
3503.873020	590481.340135	41.856077
3503.639265	590434.384640	41.861082
3503.656955	590395.054686	41.866087
3503.357036	590353.018818	41.871092
3503.642892	590309.688843	41.876096
3503.737414	590262.430785	41.881101
3503.603981	590224.276110	41.886106
3503.716649	590174.760368	41.891111
3503.909999	590140.161465	41.896116
3503.776682	590094.791974	41.901120
3503.771510	590054.061557	41.906125
3503.266698	590001.184650	41.911130
3503.510894	589960.014093	41.916135
3503.571065	589914.262892	41.921140
3503.689320	589870.155744	41.926144
3503.793717	589828.455431	41.931149
3503.151153	589795.388928	41.936154
3503.547329	589739.113310	41.941159
3503.383608	589703.065785	41.946164
3503.611667	589668.860759	41.951168
3503.536499	589624.131521	41.956173
3503.426965	589592.283718	41.961178
3503.428164	589541.429741	41.966183
3503.436089	589509.413024	41.971188
3503.343922	589462.030340	41.976192
3503.232662	589417.055373	41.981197
3502.979653	589384.177224	41.986202
3503.170264	589358.544693	41.991207
3503.396075	589310.510397	41.996212
3502.975375	589277.908656	42.001216
3503.264178	589248.753265	42.006221
3503.288896	589206.712283	42.011226
3503.554396	589167.439325	42.016231
3503.126353	589124.216199	42.021236
3503.120258	589089.695218	42.026240
3503.243280	589049.141388	42.031245
3503.088027	589033.683284	42.036250
3503.213781	588977.195455	42.041255
3503.425833	588947.951042	42.046260
3502.780841	588904.911270	42.051264
3503.550487	588874.878019	42.056269
3503.012043	588842.143053	42.061274
3503.284206	588795.652499	42.066279
3503.175726	588772.169779	42.071284
3503.132532	588730.688730	42.076288
3503.117022	588702.781988	42.081293
3503.166250	588666.697716	42.086298
3503.194801	588623.100570	42.091303
3503.141301	588595.249597	42.096308
3502.984007	588568.166381	42.101312
3503.132187	588523.547996	42.106317
3503.001427	588500.118276	42.111322
3503.228835	588462.853006	42.116327
3502.646698	588423.258895	42.121332
3502.634648	588392.795330	42.126336
3502.876465	588345.906731	42.131341
3503.023161	588322.583576	42.136346
3502.964672	588285.512715	42.141351
3503.073375	588263.999267	42.146356
3503.009745	588228.482370	42.151360
3503.651363	588192.704780	42.156365
3503.104152	588156.561725	42.161370
3503.504428	588112.152782	42.166375
3503.134156	588082.546090	42.171380
3503.082630	588048.129110	42.176384
3502.994496	588004.898484	42.181389
3502.935348	587983.110063	42.186394
3503.048394	587938.945752	42.191399
3503.205655	587908.454360	42.196404
3502.674742	587872.007147	42.201408
3502.867286	587836.398809	42.206413
3502.979565	587826.058509	42.211418
3503.033760	587788.767894	42.216423
3502.992743	587755.150109	42.221428
3502.766280	587718.053457	42.226432
3503.055359	587677.869427	42.231437
3502.794063	587644.987291	42.236442
3503.186378	587619.118673	42.241447
3502.775850	587588.865479	42.246452
3503.138217	587553.079331	42.251456
3503.485244	587524.411322	42.256461
3502.768397	587495.057651	42.261466
3503.175852	587451.997909	42.266471
3502.905872	587426.883826	42.271476
3502.697443	587397.350186	42.276480
3503.074592	587363.415256	42.281485
3502.903144	587333.224199	42.286490
3502.896383	587292.182968	42.291495
3502.856263	587254.153571	42.296500
3502.577118	587235.154251	42.301504
3503.075221	587203.655452	42.306509
3502.852139	587180.738447	42.311514
3503.195132	587134.831072	42.316519
3502.982787	587106.149181	42.321524
3503.289917	587072.625201	42.326528
3503.320561	587025.713808	42.331533
3503.224013	586997.564782	42.336538
3503.010571	586958.859851	42.341543
3502.947295	586922.637029	42.346548
3502.537740	586898.295260	42.351552
3502.472484	586851.197648	42.356557
3502.547215	586839.158379	42.361562
3502.672408	586814.331907	42.366567
3503.018099	586781.352267	42.371572
3502.736988	586761.049433	42.376576
3502.720055	586719.406249	42.381581
3502.363622	586696.158261	42.386586
3502.565579	586666.157556	42.391591
3502.714499	586646.238322	42.396596
3502.795086	586615.504715	42.401600
3502.557787	586580.009580	42.406605
3502.659611	586552.179203	42.411610
3502.877808	586519.369052	42.416615
3502.780021	586484.102376	42.421620
3502.776471	586455.837179	42.426624
3502.987993	586425.032450	42.431629
3502.944947	586405.944654	42.436634
3503.025964	586368.244045	42.441639
3502.666434	586337.227638	42.446644
3502.273819	586299.951654	42.451648
3502.844692	586274.753578	42.456653
3502.765727	586250.709500	42.461658
3503.175388	586228.543571	42.466663
3502.749782	586201.396164	42.471668
3502.926705	586166.486458	42.476672
3502.817108	586122.550057	42.481677
3502.816209	586101.199824	42.486682
3502.597614	586064.948314	42.491687
3502.874010	586037.039215	42.496692
3502.508835	586010.332950	42.501696
3502.951447	585983.349984	42.506701
3502.759278	585958.821772	42.511706
3502.541435	585921.066101	42.516711
3502.738116	585902.491258	42.521716
3502.343239	585862.758295	42.526720
3502.374296	585830.727119	42.531725
3502.677486	585817.297783	42.536730
3502.637397	585787.933938	42.541735
3502.429697	585752.581841	42.546740
3502.479769	585734.881669	42.551744
3502.312358	585707.091228	42.556749
3502.043938	585683.225877	42.561754
3502.365826	585655.960256	42.566759
3502.575488	585641.091838	42.571764
3502.193629	585620.702386	42.576768
3502.410532	585586.987469	42.581773
3502.623660	585572.168536	42.586778
3502.159718	585545.777298	42.591783
3502.617918	585521.647640	42.596788
3502.309203	585502.449434	42.601792
3502.786879	585458.568917	42.606797
3502.466379	585445.487232	42.611802
3502.621513	585423.610070	42.616807
3502.557845	585390.790473	42.621812
3502.522287	585364.582434	42.626816
3502.535203	585328.693261	42.631821
3502.616190	585322.465465	42.636826
3502.543712	585297.666448	42.641831
3502.488599	585259.081098	42.646836
3502.615708	585241.769062	42.651840
3502.431770	585212.125425	42.656845
3502.624757	585189.590289	42.661850
3502.491742	585153.222129	42.666855
3502.382073	585128.629033	42.671860
3502.344103	585104.626146	42.676864
3502.410083	585077.800075	42.681869
3502.668047	585066.682544	42.686874
3502.780053	585031.578873	42.691879
3502.723714	584999.809543	42.696884
3502.337079	584975.008783	42.701888
3503.082220	584941.610288	42.706893
3502.714628	584910.139973	42.711898
3502.784845	584879.202611	42.716903
3502.708602	584859.315322	42.721908
3502.711981	584832.899428	42.726912
3502.812051	584799.851965	42.731917
3502.682044	584776.664735	42.736922
3502.872747	584745.607912	42.741927
3502.461924	584707.226598	42.746932
3502.673681	584687.293974	42.751936
3502.707839	584652.552132	42.756941
3502.443346	584639.159976	42.761946
3502.786267	584597.753201	42.766951
3502.455906	584560.762298	42.771956
3502.289016	584544.146749	42.776960
3502.715298	584521.022390	42.781965
3502.449298	584501.915998	42.786970
3502.329094	584467.849334	42.791975
3502.416521	584440.015835	42.796980
3502.264504	584428.560744	42.801985
3502.832450	584392.631863	42.806989
3502.370313	584373.104774	42.811994
3502.518949	584338.043283	42.816999
3502.404091	584319.464334	42.822004
3502.032758	584298.970516	42.827009
3502.378840	584279.166532	42.832013
3502.186026	584249.822437	42.837018
3502.616015	584229.754614	42.842023
3502.201551	584206.510392	42.847028
3502.276130	584186.046907	42.852033
3502.220093	584153.673553	42.857037
3502.090948	584144.470311	42.862042
3502.183212	584121.798346	42.867047
3502.249997	584102.087833	42.872052
3502.033053	584070.391043	42.877057
3501.835777	584045.608702	42.882061
3501.825325	584021.549014	42.887066
3502.198872	584020.989305	42.892071
3502.316678	583989.991868	42.897076
3502.237694	583974.715166	42.902081
3502.218609	583947.849502	42.907085
3502.144005	583936.030898	42.912090
3502.356764	583909.730434	42.917095
3501.619021	583881.172335	42.922100
3501.580817	583856.765726	42.927105
3502.313251	583847.026517	42.932109
3502.274187	583832.194533	42.937114
3502.118100	583808.808818	42.942119
3502.091776	583794.676594	42.947124
3502.236210	583779.364694	42.952129
3502.370152	583751.873082	42.957133
3502.421150	583738.430503	42.962138
3502.132906	583715.817185	42.967143
3502.288185	583686.667813	42.972148
3502.361668	583675.377200	42.977153
3502.500998	583647.583709	42.982157
3502.101377	583626.942668	42.987162
3502.106253	583605.386149	42.992167
3502.018693	583589.809475	42.997172
3501.957197	583566.608976	43.002177
3502.526238	583540.703101	43.007181
3501.872089	583522.106849	43.012186
3501.968901	583495.572871	43.017191
3502.273184	583483.443899	43.022196
3501.980574	583466.946632	43.027201
3502.214591	583449.615058	43.032205
3502.369748	583433.799698	43.037210
3502.056949	583414.047031	43.042215
3501.796052	583370.774940	43.047220
3501.876809	583366.751823	43.052225
3502.169223	583345.199975	43.057229
3501.825781	583334.375236	43.062234
3501.946882	583321.221974	43.067239
3502.027905	583296.594960	43.072244
3502.127108	583280.988652	43.077249
3502.139793	583253.414488	43.082253
3501.934571	583240.161749	43.087258
3502.424466	583219.832066	43.092263
3502.223912	583199.860941	43.097268
3501.813594	583175.310466	43.102273
3501.737623	583152.261751	43.107277
3501.893770	583144.065835	43.112282
3502.187937	583114.642578	43.117287
3502.404662	583102.226084	43.122292
3502.325839	583083.138091	43.127297
3501.838740	583055.942355	43.132301
3502.081775	583037.154892	43.137306
3501.907170	583025.501339	43.142311
3502.165985	583008.315592	43.147316
3502.178532	582990.616861	43.152321
3502.330136	582965.326351	43.157325
3502.083999	582941.401410	43.162330
3502.109943	582925.705786	43.167335
3501.989475	582907.877317	43.172340
3501.687366	582886.818578	43.177345
3501.807610	582877.124090	43.182349
3502.128891	582867.648830	43.187354
3502.464721	582849.147338	43.192359
3502.560166	582826.221543	43.197364
3502.242426	582798.898429	43.202369
3502.553788	582773.482238	43.207373
3502.275593	582756.079249	43.212378
3502.415370	582724.774015	43.217383
3502.321014	582709.698493	43.222388
3501.990044	582687.891879	43.227393
3502.197862	582654.018983	43.232397
3502.036938	582635.945729	43.237402
3501.892436	582621.680071	43.242407
3502.076221	582595.731939	43.247412
3502.034845	582578.542318	43.252417
3502.130726	582555.615892	43.257421
3502.005175	582550.571907	43.262426
3502.411814	582524.839443	43.267431
3502.484890	582503.019433	43.272436
3502.246734	582478.841566	43.277441
3502.448485	582457.101619	43.282445
3502.719577	582427.579869	43.287450
3502.284137	582407.894701	43.292455
3502.235021	582385.241264	43.297460
3502.025795	582359.053204	43.302465
3502.362602	582334.233648	43.307469
3502.158020	582329.302187	43.312474
3502.120977	582305.192771	43.317479
3502.460207	582283.380855	43.322484
3502.498017	582259.660722	43.327489
3502.459151	582222.616378	43.332493
3502.181262	582202.856078	43.337498
3502.302409	582186.994112	43.342503
3502.353951	582156.753919	43.347508
3501.888996	582143.741008	43.352513
3502.363382	582118.648780	43.357517
3501.870810	582105.890823	43.362522
3502.072712	582079.487419	43.367527
3502.125328	582057.569454	43.372532
3501.895385	582039.656422	43.377537
3502.093826	582015.810381	43.382541
3502.116051	582011.043868	43.387546
3501.961015	581982.941242	43.392551
3501.742885	581971.945159	43.397556
3502.119245	581949.174176	43.402561
3502.463526	581926.859396	43.407565
3502.025750	581909.229329	43.412570
3501.834072	581895.070380	43.417575
3501.981845	581871.332224	43.422580
3501.424111	581848.406234	43.427585
3501.958796	581838.846597	43.432589
3502.025833	581814.268599	43.437594
3501.551424	581798.348766	43.442599
3501.968413	581794.673617	43.447604
3501.759079	581772.194382	43.452609
3502.023031	581759.568447	43.457613
3501.563026	581737.529433	43.462618
3501.833879	581722.445608	43.467623
3502.101664	581721.350807	43.472628
3501.923576	581693.100633	43.477633
3502.238046	581680.667263	43.482637
3502.194052	581659.114581	43.487642
3502.085318	581650.106613	43.492647
3501.635714	581617.737194	43.497652
3501.802358	581605.126295	43.502657
3502.156019	581590.229900	43.507661
3501.854604	581571.274366	43.512666
3502.063073	581564.021740	43.517671
3502.345004	581532.891463	43.522676
3501.927940	581527.942720	43.527681
3501.946454	581493.945447	43.532685
3501.927547	581494.650316	43.537690
3502.176331	581480.071003	43.542695
3501.616485	581450.024734	43.547700
3501.841220	581439.911536	43.552705
3502.005163	581416.119736	43.557709
3502.003553	581405.791194	43.562714
3501.969445	581380.175112	43.567719
3501.862350	581355.673457	43.572724
3502.001253	581347.930167	43.577729
3501.978880	581316.295314	43.582733
3502.003859	581312.129750	43.587738
3502.031774	581287.255857	43.592743
3502.087532	581274.762197	43.597748
3501.877672	581248.972726	43.602753
3501.996079	581227.243393	43.607757
3501.974548	581225.341386	43.612762
3502.261420	581197.418383	43.617767
3502.024060	581183.867351	43.622772
3502.014831	581169.578669	43.627777
3501.746158	581145.352511	43.632781
3501.851626	581132.048666	43.637786
3501.692067	581107.755227	43.642791
3501.999345	581099.233327	43.647796
3501.852452	581088.877060	43.652801
3501.767742	581066.727896	43.657805
3501.821449	581047.866372	43.662810
3501.681878	581027.229942	43.667815
3502.122406	581023.601004	43.672820
3501.734964	581014.385381	43.677825
3501.938914	581000.464286	43.682829
3501.817686	580987.646981	43.687834
3501.492667	580952.197503	43.692839
3501.947223	580951.925840	43.697844
3501.940968	580926.454779	43.702849
3501.932485	580908.054015	43.707853
3501.702671	580907.337778	43.712858
3501.819835	580884.605130	43.717863
3501.772924	580872.377777	43.722868
3501.576663	580861.276884	43.727873
3501.668035	580823.806359	43.732877
3501.797039	580834.115457	43.737882
3501.774463	580822.084812	43.742887
3501.978928	580793.170829	43.747892
3501.855564	580782.008318	43.752897
3501.392558	580764.229938	43.757901
3501.578647	580752.868593	43.762906
3501.550559	580728.303057	43.767911
3502.162550	580724.697360	43.772916
3501.970988	580709.433735	43.777921
3502.011578	580681.898935	43.782925
3501.801309	580673.507760	43.787930
3502.259144	580655.334536	43.792935
3502.568562	580634.677328	43.797940
3501.839717	580615.385830	43.802945
3502.087262	580593.685211	43.807949
3501.937374	580570.993669	43.812954
3502.192238	580558.217359	43.817959
3502.021430	580535.478872	43.822964
3501.742361	580511.102521	43.827969
3502.025772	580485.735596	43.832973
3501.754569	580488.385433	43.837978
3502.190942	580463.395696	43.842983
3502.105802	580452.577884	43.847988
3501.972652	580432.190063	43.852993
3501.831432	580408.744673	43.857997
3501.690409	580399.740735	43.863002
3501.855276	580371.483719	43.868007
3502.231041	580365.608200	43.873012
3501.742967	580355.204294	43.878017
3501.883033	580332.918236	43.883021
3502.024063	580327.029248	43.888026
3502.040187	580296.939948	43.893031
3502.262128	580282.814564	43.898036
3502.014496	580255.775067	43.903041
3501.987462	580246.552606	43.908045
3501.785258	580225.523316	43.913050
3501.810075	580203.355305	43.918055
3502.070296	580200.807336	43.923060
3501.898942	580177.416314	43.928065
3502.300813	580154.236502	43.933069
3502.159452	580136.306539	43.938074
3502.057174	580110.898763	43.943079
3502.072692	580092.492896	43.948084
3501.733873	580083.770350	43.953089
3501.835232	580046.395932	43.958093
3501.611828	580040.714202	43.963098
3501.567526	580036.358406	43.968103
3501.644200	580016.939937	43.973108
3501.649923	580005.906902	43.978113
3501.894951	580001.455716	43.983117
3502.028592	579976.311628	43.988122
3501.878922	579961.040423	43.993127
3501.863147	579933.663018	43.998132
3501.483732	579921.486597	44.003137
3501.941196	579906.672014	44.008141
3501.753864	579895.167586	44.013146
3502.060864	579882.833669	44.018151
3501.986834	579867.249631	44.023156
3501.786632	579852.688229	44.028161
3501.984929	579836.108789	44.033165
3501.826185	579815.422955	44.038170
3501.907208	579805.631620	44.043175
3502.006513	579789.819790	44.048180
3501.894444	579770.029219	44.053185
3501.549752	579744.257325	44.058189
3501.563506	579741.597341	44.063194
3501.677716	579718.662182	44.068199
3501.607789	579698.363423	44.073204
3502.080611	579706.062307	44.078209
3501.778607	579684.796858	44.083213
3501.634193	579671.229444	44.088218
3501.617281	579658.344147	44.093223
3502.079249	579642.375117	44.098228
3501.955631	579642.193816	44.103233
3501.633318	579616.167388	44.108237
3501.614219	579600.674685	44.113242
3501.644494	579584.171284	44.118247
3501.543506	579570.145627	44.123252
3501.551812	579562.672251	44.128257
3501.659884	579537.180132	44.133261
3501.871804	579535.241340	44.138266
3501.942293	579511.610517	44.143271
3502.142823	579499.292821	44.148276
3501.702785	579489.682962	44.153281
3501.655970	579465.919935	44.158285
3501.747826	579451.914130	44.163290
3501.416025	579443.992358	44.168295
3501.879181	579430.881304	44.173300
3501.835261	579424.017781	44.178305
3502.077244	579398.604708	44.183309
3502.250574	579393.562706	44.188314
3501.911154	579364.228547	44.193319
3502.001600	579332.971598	44.198324
3501.960729	579327.862753	44.203329
3502.428304	579299.806440	44.208333
3502.194292	579284.798237	44.213338
3501.693174	579267.324306	44.218343
3501.834354	579256.770845	44.223348
3501.616527	579236.444216	44.228353
3501.806654	579217.006615	44.233357
3501.780649	579201.363988	44.238362
3501.711284	579176.450428	44.243367
3502.110627	579174.030927	44.248372
3501.484998	579161.240215	44.253377
3501.624281	579133.535704	44.258381
3501.665526	579130.871276	44.263386
3501.701644	579120.133511	44.268391
3501.486807	579092.083057	44.273396
3501.575142	579084.245798	44.278401
3501.636695	579086.342444	44.283405
3501.533836	579072.567203	44.288410
3501.960368	579053.292961	44.293415
3501.881008	579044.880087	44.298420
3501.780556	579035.016145	44.303425
3501.639840	579023.653977	44.308429
3500.956999	579015.335423	44.313434
3501.183950	579014.748253	44.318439
3501.565176	578999.693636	44.323444
3501.145317	578975.035019	44.328449
3501.614331	578966.787113	44.333453
3501.502509	578961.338138	44.338458
3501.307169	578964.979486	44.343463
3501.425221	578928.250665	44.348468
3501.356163	578922.794986	44.353473
3501.597163	578918.544604	44.358477
3501.728111	578911.001467	44.363482
3501.412627	578904.480983	44.368487
3501.569455	578888.809334	44.373492
3501.239165	578880.485715	44.378497
3501.698800	578882.269413	44.383501
3501.307429	578861.718474	44.388506
3501.302470	578845.871452	44.393511
3501.591384	578836.548279	44.398516
3501.547865	578833.245066	44.403521
3501.825660	578819.109097	44.408525
3501.834634	578805.065287	44.413530
3501.889215	578803.652480	44.418535
3501.692489	578772.539156	44.423540
3501.812674	578757.725628	44.428545
3501.966654	578752.987271	44.433549
3501.839028	578732.896380	44.438554
3501.587121	578724.008721	44.443559
3501.553533	578696.480605	44.448564
3501.432283	578688.074011	44.453569
3501.784659	578677.486987	44.458573
3501.616066	578674.754950	44.463578
3501.818216	578640.870698	44.468583
3502.023510	578636.475335	44.473588
3501.780586	578620.966108	44.478593
3501.697554	578597.206891	44.483597
3502.125356	578596.337540	44.488602
3501.794679	578566.097170	44.493607
3501.908399	578558.105117	44.498612
3501.638591	578548.367524	44.503617
3501.726095	578526.487291	44.508621
3502.009462	578512.550675	44.513626
3501.871028	578500.987006	44.518631
3501.758911	578476.931163	44.523636
3501.813963	578471.957389	44.528641
3501.444150	578446.687945	44.533645
3501.616256	578433.621224	44.538650
3501.752386	578427.932613	44.543655
3501.816421	578411.973884	44.548660
3501.697373	578392.181957	44.553665
3501.411400	578389.468200	44.558669
3501.709944	578378.337624	44.563674
3501.751866	578361.228754	44.568679
3501.521426	578353.039589	44.573684
3501.541114	578346.366073	44.578689
3501.754383	578326.020543	44.583693
3501.691725	578310.382396	44.588698
3501.689916	578296.088863	44.593703
3501.573852	578283.418092	44.598708
3501.410375	578274.817172	44.603713
3501.495456	578258.654319	44.608717
3502.062258	578260.772443	44.613722
3501.715041	578238.307606	44.618727
3501.748747	578221.049344	44.623732
3501.424276	578201.088576	44.628737
3501.340527	578188.362491	44.633741
3501.488012	578179.161189	44.638746
3501.061659	578184.945378	44.643751
3501.481695	578174.297149	44.648756
3501.416694	578162.470879	44.653761
3501.260852	578148.201237	44.658765
3501.614577	578145.387416	44.663770
3501.754523	578143.409484	44.668775
3501.703632	578119.945152	44.673780
3501.527737	578103.020401	44.678785
3501.666685	578092.566500	44.683789
3501.623131	578097.187492	44.688794
3501.791767	578072.735806	44.693799
3501.484499	578062.000551	44.698804
3501.135978	578059.597418	44.703809
3501.284561	578041.217517	44.708813
3501.150662	578026.693515	44.713818
3501.416659	578017.824638	44.718823
3501.516165	578010.335965	44.723828
3501.496003	578009.185517	44.728833
3501.736537	578002.376961	44.733837
3501.622264	577978.270226	44.738842
3501.344528	577973.047324	44.743847
3501.794537	577961.792347	44.748852
3501.868684	577954.407911	44.753857
3501.716031	577940.739367	44.758861
3501.771304	577932.705849	44.763866
3501.977046	577898.618166	44.768871
3501.706913	577885.168541	44.773876
3501.398281	577876.289073	44.778881
3501.919518	577851.731628	44.783885
3501.584272	577854.191471	44.788890
3501.657863	577840.938837	44.793895
3502.128647	577819.549016	44.798900
3501.897110	577803.083912	44.803905
3501.526832	577783.982207	44.808909
3501.658472	577769.817607	44.813914
3501.874605	577772.542364	44.818919
3501.961758	577742.635691	44.823924
3501.684217	577743.130448	44.828929
3501.846428	577720.183681	44.833933
3501.798602	577697.570640	44.838938
3501.598888	577687.269617	44.843943
3501.499982	577682.169091	44.848948
3501.761963	577669.990245	44.853953
3502.041869	577654.247471	44.858957
3501.650205	577636.904336	44.863962
3501.145380	577609.397054	44.868967
3501.722684	577600.980749	44.873972
3501.181956	577606.883428	44.878977
3501.376296	577605.197839	44.883981
3501.776350	577589.135250	44.888986
3501.473246	577565.709184	44.893991
3501.871399	577560.430584	44.898996
3501.199288	577558.579498	44.904001
3501.540230	577527.228181	44.909005
3501.267550	577519.747206	44.914010
3501.602977	577523.857774	44.919015
3501.719180	577515.262704	44.924020
3500.879155	577485.349817	44.929025
3501.050202	577480.507941	44.934029
3501.519791	577475.468921	44.939034
3501.112267	577480.247381	44.944039
3501.641808	577463.512325	44.949044
3501.466144	577470.561781	44.954049
3501.821706	577440.512028	44.959053
3501.635629	577435.224387	44.964058
3501.572064	577427.510029	44.969063
3501.844091	577403.090877	44.974068
3501.706746	577398.949227	44.979073
3501.388324	577391.324844	44.984077
3501.640069	577362.093633	44.989082
3501.581869	577361.099539	44.994087
3501.346877	577349.800562	44.999092
3501.672764	577350.301317	45.004097
3501.896708	577325.187302	45.009101
3501.560726	577315.158028	45.014106
3501.435990	577318.086658	45.019111
3501.357279	577283.941257	45.024116
3501.224594	577272.224943	45.029121
3501.664812	577266.588523	45.034125
3501.605344	577264.641611	45.039130
3501.291908	577253.154167	45.044135
3501.471765	577220.222108	45.049140
3501.647356	577226.364112	45.054145
3501.334140	577220.544502	45.059149
3501.833632	577213.293718	45.064154
3501.393358	577191.944811	45.069159
3501.617545	577189.903384	45.074164
3501.735789	577182.461388	45.079169
3501.737352	577157.933508	45.084173
3501.874390	577139.955204	45.089178
3501.590214	577137.140540	45.094183
3501.903916	577109.654545	45.099188
3501.684562	577105.475447	45.104193
3501.537979	577088.394101	45.109197
3501.565276	577076.100822	45.114202
3501.691916	577066.701231	45.119207
3501.639777	577048.351081	45.124212
3501.473181	577040.752882	45.129217
3501.627156	577029.041660	45.134221
3501.257446	577021.023767	45.139226
3501.320282	577023.170760	45.144231
3501.478811	577010.204822	45.149236
3501.526060	576996.403555	45.154241
3501.629694	576979.784522	45.159245
3501.838990	576983.965167	45.164250
3501.526061	576969.718578	45.169255
3502.021562	576946.015891	45.174260
3501.430855	576942.797659	45.179265
3501.778317	576907.129856	45.184269
3501.446970	576902.667230	45.189274
3501.211958	576898.390183	45.194279
3501.605596	576897.776851	45.199284
3501.742950	576878.293281	45.204289
3501.658043	576869.628836	45.209293
3501.609745	576859.303379	45.214298
3501.582519	576835.632016	45.219303
3501.905128	576823.492936	45.224308
3501.403086	576820.963051	45.229313
3501.361273	576814.248076	45.234317
3501.828958	576782.473584	45.239322
3501.648399	576783.605304	45.244327
3501.918008	576771.875737	45.249332
3501.896053	576757.733872	45.254337
3501.756241	576740.199492	45.259341
3501.834457	576718.567983	45.264346
3501.602214	576705.261497	45.269351
3501.535234	576688.668706	45.274356
3501.575941	576690.568418	45.279361
3501.683167	576665.019726	45.284365
3502.028702	576657.642172	45.289370
3501.724605	576641.437505	45.294375
3501.946393	576607.544035	45.299380
3501.914816	576613.518118	45.304385
3501.899567	576591.198719	45.309389
3501.766682	576575.518966	45.314394
3501.509386	576568.687046	45.319399
3501.918465	576531.955032	45.324404
3501.847497	576523.338302	45.329409
3501.372826	576514.935160	45.334413
3501.962267	576504.058224	45.339418
3501.503496	576490.034470	45.344423
3502.024736	576481.174643	45.349428
3501.470475	576455.678723	45.354433
3501.282524	576443.669211	45.359437
3502.080628	576437.825946	45.364442
3501.659779	576424.749259	45.369447
3501.983306	576405.536738	45.374452
3501.912116	576404.343941	45.379457
3501.618674	576381.666319	45.384461
3501.760015	576371.661902	45.389466
3501.691926	576367.759854	45.394471
3501.912806	576333.063102	45.399476
3501.555619	576327.049249	45.404481
3501.430143	576314.879345	45.409485
3501.389239	576295.874096	45.414490
3501.472089	576279.809066	45.419495
3501.570431	576273.774134	45.424500
3501.759599	576275.450058	45.429505
3501.817422	576257.081424	45.434509
3501.630834	576251.943790	45.439514
3501.659205	576239.248126	45.444519
3501.591896	576211.969989	45.449524
3501.622969	576204.340322	45.454529
3501.151609	576193.679085	45.459533
3501.883301	576191.507979	45.464538
3501.617720	576169.828835	45.469543
3501.438858	576162.332284	45.474548
3501.472214	576145.773168	45.479553
3501.311719	576137.320627	45.484557
3501.499564	576126.807090	45.489562
3501.263834	576120.473158	45.494567
3501.346228	576107.066611	45.499572
3501.475399	576110.056188	45.504577
3501.589403	576073.569461	45.509581
3501.515326	576066.808919	45.514586
3501.276219	576076.828818	45.519591
3501.795658	576065.460769	45.524596
3501.245586	576040.314395	45.529601
3501.411683	576035.773656	45.534605
3501.613947	576026.963339	45.539610
3500.940003	576034.894210	45.544615
3501.223689	576035.150808	45.549620
3501.133538	576012.540987	45.554625
3501.114006	575992.679099	45.559629
3501.406715	575989.723794	45.564634
3501.001230	575988.683540	45.569639
3501.841222	575982.833496	45.574644
3501.398851	575975.277686	45.579649
3501.352110	575957.476714	45.584653
3501.485897	575951.235412	45.589658
3501.383757	575948.241495	45.594663
3501.568126	575941.189655	45.599668
3501.833040	575927.503540	45.604673
3501.631529	575905.964363	45.609677
3501.304822	575905.313100	45.614682
3501.247947	575903.415711	45.619687
3501.568938	575869.203523	45.624692
3501.503862	575870.618266	45.629697
3501.668059	575859.405874	45.634701
3501.615003	575848.127105	45.639706
3501.419489	575839.027674	45.644711
3501.789259	575823.318456	45.649716
3501.680864	575818.870706	45.654721
3501.470731	575799.740579	45.659725
3501.528137	575787.441184	45.664730
3501.587046	575785.224685	45.669735
3501.420132	575772.157703	45.674740
3501.485378	575752.031312	45.679745
3501.549866	575739.530098	45.684749
3501.451487	575737.739498	45.689754
3501.368145	575735.545227	45.694759
3501.077889	575719.587891	45.699764
3501.052473	575708.003669	45.704769
3501.718830	575707.347645	45.709773
3501.816289	575704.824112	45.714778
3501.458351	575695.950617	45.719783
3501.483861	575664.543090	45.724788
3501.504120	575667.198654	45.729793
3501.474561	575656.919328	45.734797
3501.746542	575643.934081	45.739802
3501.074408	575622.066608	45.744807
3501.492531	575612.620236	45.749812
3501.296134	575611.396762	45.754817
3501.249608	575596.655289	45.759821
3501.268998	575531.235943	45.764826
3501.143525	575430.923067	45.769831
3501.102985	575275.061129	45.774836
3500.704776	575069.235507	45.779841
3500.438174	574821.845567	45.784845
3500.222174	574539.573913	45.789850
3499.929515	574213.406901	45.794855
3499.770345	573814.859478	45.799860
3498.616182	573378.320219	45.804865
3498.170137	572900.808899	45.809869
3497.460937	572380.665751	45.814874
3496.558956	571812.404067	45.819879
3495.651204	571195.485603	45.824884
3494.733389	570567.293278	45.829889
3493.920061	569868.883311	45.834893
3492.496649	569139.355616	45.839898
3491.463641	568378.598141	45.844903
3490.387267	567567.596258	45.849908
3488.980579	566714.818771	45.854913
3487.596342	565825.021477	45.859917
3486.348325	564901.893997	45.864922
3483.826582	563954.838684	45.869927
3482.657733	562962.446948	45.874932
3480.776212	561938.289975	45.879937
3479.697285	560873.433071	45.884941
3477.807993	559782.886665	45.889946
3475.727830	558653.585396	45.894951
3474.160135	557491.437926	45.899956
3471.942090	556316.063298	45.904961
3469.782850	555089.455508	45.909965
3468.042972	553844.312188	45.914970
3465.379202	552574.705835	45.919975
3463.062997	551261.780266	45.924980
3460.975783	549934.147478	45.929985
3458.496694	548578.978115	45.934989
3456.304330	547200.934859	45.939994
3453.501108	545816.345267	45.944999
3451.095919	544394.770600	45.950004
3448.549624	542958.014608	45.955009
3445.537969	541482.880357	45.960013
3443.050783	540010.107247	45.965018
3440.150897	538505.322792	45.970023
3437.300414	536999.546845	45.975028
3434.724014	535465.614958	45.980033
3431.715519	533920.190224	45.985037
3429.050869	532359.724644	45.990042
3426.273876	530773.711202	45.995047
3423.236907	529168.711274	46.000052
3420.238158	527556.306544	46.005057
3416.910323	525928.846135	46.010061
3414.162634	524285.578958	46.015066
3410.657033	522631.042517	46.020071
3407.695265	520977.476465	46.025076
3404.457371	519318.106415	46.030081
3401.295980	517636.697361	46.035085
3398.393022	515950.503911	46.040090
3394.899881	514245.643130	46.045095
3391.810311	512526.542276	46.050100
3388.120698	510810.297705	46.055105
3384.542577	509087.520909	46.060109
3380.851334	507344.375230	46.065114
3377.845471	505627.643781	46.070119
3374.723362	503881.058371	46.075124
3371.496641	502132.813405	46.080129
3367.608840	500370.128482	46.085133
3364.206749	498602.359239	46.090138
3360.222343	496847.540722	46.095143
3357.398623	495054.268435	46.100148
3353.511266	493281.847685	46.105153
3349.759098	491497.329418	46.110157
3346.152744	489709.092141	46.115162
3342.754582	487929.247688	46.120167
3339.073829	486136.712859	46.125172
3335.405988	484353.413636	46.130177
3331.575005	482574.885669	46.135181
3328.224531	480777.939654	46.140186
3324.184399	478990.042581	46.145191
3320.677053	477190.741119	46.150196
3316.801130	475406.963377	46.155201
3312.891802	473610.000752	46.160205
3309.246184	471809.713157	46.165210
3305.437848	470028.213158	46.170215
3301.924055	468229.634437	46.175220
3298.244499	466443.731811	46.180225
3294.509231	464663.968917	46.185229
3290.279068	462865.732539	46.190234
3286.742974	461073.267360	46.195239
3283.084638	459291.004964	46.200244
3279.289498	457514.094633	46.205249
3275.514104	455732.748103	46.210253
3271.783227	453952.326352	46.215258
3267.310539	452170.676352	46.220263
3263.623332	450392.217499	46.225268
3259.716460	448623.640141	46.230273
3256.233444	446851.987760	46.235277
3252.403222	445087.356717	46.240282
3248.359582	443328.868640	46.245287
3244.732721	441566.602942	46.250292
3241.121518	439808.929320	46.255297
3237.468157	438061.684816	46.260301
3233.781767	436299.643831	46.265306
3229.595530	434551.147271	46.270311
3225.997049	432798.397422	46.275316
3222.496535	431045.930366	46.280321
3218.100195	429302.670202	46.285325
3214.041840	427549.320589	46.290330
3210.280178	425802.207813	46.295335
3206.444957	424068.236056	46.300340
3202.894287	422341.219904	46.305345
3198.890528	420619.756798	46.310349
3195.275384	418893.120734	46.315354
3191.482236	417170.730598	46.320359
3187.648366	415439.382141	46.325364
3183.885983	413729.892344	46.330369
3180.149777	412006.567864	46.335373
3176.177637	410294.505402	46.340378
3172.608319	408585.340333	46.345383
3168.597507	406881.337374	46.350388
3164.658852	405176.076662	46.355393
3160.828330	403471.633872	46.360397
3157.297967	401782.848240	46.365402
3153.804148	400097.789376	46.370407
3149.888252	398404.401582	46.375412
3145.864451	396713.648846	46.380417
3142.198230	395029.926880	46.385421
3138.255817	393347.499910	46.390426
3133.951317	391672.728470	46.395431
3130.533810	389996.383207	46.400436
3126.674404	388339.260848	46.405441
3122.537347	386666.381883	46.410445
3119.246734	384999.758866	46.415450
3115.082209	383355.227911	46.420455
3111.454335	381685.140411	46.425460
3107.647259	380048.849337	46.430465
3103.837450	378406.894882	46.435469
3100.078609	376754.620981	46.440474
3096.154240	375114.919750	46.445479
3092.690513	373477.917498	46.450484
3088.899135	371852.096331	46.455489
3085.144499	370217.409813	46.460493
3081.357818	368596.504015	46.465498
3077.085333	366975.810126	46.470503
3073.670266	365359.031994	46.475508
3069.743087	363748.951836	46.480513
3065.865999	362125.943153	46.485517
3062.514672	360518.874718	46.490522
3058.451881	358921.183682	46.495527
3055.144040	357310.176714	46.500532
3051.429802	355717.372226	46.505537
3047.461131	354120.916875	46.510541
3043.709013	352524.168960	46.515546
3039.737386	350942.729115	46.520551
3036.609860	349339.243358	46.525556
3032.697297	347752.326384	46.530561
3028.818183	346170.082529	46.535565
3025.202060	344588.613006	46.540570
3021.373683	343010.586658	46.545575
3018.085233	341437.311219	46.550580
3013.873526	339861.312411	46.555585
3010.031506	338292.865463	46.560589
3006.428389	336715.005359	46.565594
3002.318171	335154.220837	46.570599
2998.806319	333597.829387	46.575604
2995.480993	332042.743155	46.580609
2991.741905	330480.816330	46.585613
2988.218961	328929.704504	46.590618
2984.379828	327382.014807	46.595623
2980.884494	325815.184040	46.600628
2976.895534	324270.806590	46.605633
2972.956055	322728.602093	46.610637
2969.522997	321178.705713	46.615642
2965.610436	319637.859410	46.620647
2962.398986	318110.561790	46.625652
2958.421947	316558.091251	46.630657
2954.421803	315028.546175	46.635661
2950.882786	313500.887585	46.640666
2947.160192	311976.896783	46.645671
2943.885437	310457.824918	46.650676
2939.721633	308932.736522	46.655681
2936.156322	307410.509647	46.660685
2932.255989	305879.966718	46.665690
2928.661210	304383.101194	46.670695
2925.331592	302867.572033	46.675700
2921.544683	301362.123803	46.680705
2917.495161	299846.264594	46.685709
2914.043047	298340.501783	46.690714
2909.997763	296838.303622	46.695719
2907.028627	295330.654084	46.700724
2903.236995	293832.079514	46.705729
2899.064571	292339.457747	46.710733
2895.372916	290850.924323	46.715738
2891.771647	289362.697513	46.720743
2888.639208	287873.649781	46.725748
2884.629375	286384.501564	46.730753
2881.027944	284909.283571	46.735757
2877.387662	283419.757611	46.740762
2873.486417	281940.118927	46.745767
2870.219983	280458.950264	46.750772
2866.072756	278978.577079	46.755777
2862.032738	277494.441023	46.760781
2858.722611	276022.027440	46.765786
2855.265409	274547.394729	46.770791
2851.564774	273089.374980	46.775796
2847.857369	271629.421684	46.780801
2844.091474	270164.029734	46.785805
2841.038912	268704.180867	46.790810
2837.022412	267255.180205	46.795815
2833.386496	265792.933554	46.800820
2829.574487	264335.276762	46.805825
2825.972728	262891.139377	46.810829
2822.596086	261427.288585	46.815834
2818.619200	259979.122883	46.820839
2815.055403	258532.606379	46.825844
2811.522419	257085.482263	46.830849
2807.649772	255649.345373	46.835853
2804.204408	254200.316664	46.840858
2800.429833	252762.249743	46.845863
2796.656310	251327.479403	46.850868
2792.757227	249897.146814	46.855873
2788.751321	248472.039371	46.860877
2785.376044	247040.149222	46.865882
2781.950431	245621.295474	46.870887
2778.254128	244201.608083	46.875892
2774.563790	242791.027957	46.880897
2770.868984	241374.786008	46.885901
2767.653838	239952.832582	46.890906
2763.547178	238550.622028	46.895911
2760.234705	237126.352355	46.900916
2756.349556	235723.865665	46.905921
2752.736217	234318.504353	46.910925
2749.356714	232910.580635	46.915930
2745.863351	231511.534165	46.920935
2742.248148	230107.791958	46.925940
2738.529435	228697.467086	46.930945
2734.542948	227304.093830	46.935949
2730.837568	225899.622028	46.940954
2727.240913	224508.147563	46.945959
2723.861950	223117.658130	46.950964
2720.596493	221722.745779	46.955969
2716.668019	220328.957529	46.960973
2712.870345	218938.767716	46.965978
2709.172535	217555.823865	46.970983
2705.371693	216181.024245	46.975988
2701.799703	214799.622062	46.980993
2698.327898	213429.135097	46.985997
2694.839813	212041.846850	46.991002
2691.326291	210671.709004	46.996007
2687.772837	209290.378024	47.001012
2683.966047	207912.888835	47.006017
2680.345682	206540.624908	47.011021
2676.806652	205175.258623	47.016026
2672.892961	203809.705385	47.021031
2669.672469	202444.333617	47.026036
2666.036918	201083.137364	47.031041
2662.256478	199715.684336	47.036045
2659.017242	198351.774598	47.041050
2654.928191	196992.135574	47.046055
2651.706824	195624.937416	47.051060
2647.970291	194271.992494	47.056065
2644.071489	192911.981832	47.061069
2640.451110	191552.909917	47.066074
2637.225983	190207.746337	47.071079
2633.515493	188845.969147	47.076084
2629.927730	187494.247782	47.081089
2626.437836	186147.569894	47.086093
2622.838792	184789.212969	47.091098
2619.123303	183445.941505	47.096103
2615.514359	182095.567551	47.101108
2611.912588	180750.991784	47.106113
2608.050125	179413.020324	47.111117
2604.779961	178066.395531	47.116122
2600.953707	176728.433777	47.121127
2597.371868	175388.087120	47.126132
2594.065040	174061.417320	47.131137
2589.793100	172730.566757	47.136141
2586.610668	171374.235775	47.141146
2582.516346	170058.425110	47.146151
2579.144350	168735.969102	47.151156
2575.688891	167410.418901	47.156161
2572.126265	166092.725978	47.161165
2568.661535	164763.459614	47.166170
2564.571966	163439.077619	47.171175
2561.152147	162124.507305	47.176180
2557.737665	160806.360795	47.181185
2554.058378	159487.557611	47.186189
2550.470929	158173.629967	47.191194
2546.434787	156856.186298	47.196199
2542.960648	155541.687339	47.201204
2539.457107	154239.274630	47.206209
2535.309478	152937.908449	47.211213
2531.667112	151628.781193	47.216218
2528.280156	150349.766850	47.221223
2524.337122	149053.817303	47.226228
2520.631265	147763.690126	47.231233
2517.164923	146477.285451	47.236237
2513.991577	145190.027038	47.241242
2510.182866	143879.144340	47.246247
2506.711320	142540.263296	47.251252
2503.410179	141257.782687	47.256257
2499.709306	139985.157150	47.261261
2496.207415	138687.915538	47.266266
2492.469651	137410.008410	47.271271
2488.846591	136126.329890	47.276276
2485.355306	134853.493005	47.281281
2481.550843	133577.598789	47.286285
2478.076761	132304.093749	47.291290
2474.398573	131034.588276	47.296295
2470.338287	129764.988981	47.301300
2467.247058	128497.667179	47.306305
2463.610022	127237.909796	47.311309
2459.932506	125967.741694	47.316314
2456.360808	124712.133896	47.321319
2452.632944	123446.694467	47.326324
2449.200874	122183.296337	47.331329
2445.575409	120936.374495	47.336333
2442.072808	119663.390260	47.341338
2438.355472	118407.941692	47.346343
2434.682283	117151.128724	47.351348
2431.634336	115904.534297	47.356353
2427.546753	114657.457543	47.361357
2423.977099	113397.944788	47.366362
2420.399627	112161.172385	47.371367
2416.973292	110919.396683	47.376372
2413.121193	109669.657623	47.381377
2409.829511	108433.008024	47.386381
2405.828342	107183.368190	47.391386
2402.562038	105956.121418	47.396391
2398.860062	104722.135182	47.401396
2395.243399	103487.265436	47.406401
2391.262752	102253.260878	47.411405
2387.969664	101023.389223	47.416410
2384.063134	99788.956966	47.421415
2380.509736	98564.404444	47.426420
2377.248182	97343.907115	47.431425
2373.371162	96133.376589	47.436429
2369.680004	94899.506035	47.441434
2365.876209	93696.390644	47.446439
2361.998613	92481.058555	47.451444
2358.538599	91274.527696	47.456449
2354.691930	90070.976828	47.461453
2351.517644	88866.936916	47.466458
2348.141554	87671.222745	47.471463
2343.945512	86468.888279	47.476468
2340.722446	85270.071577	47.481473
2336.649604	84076.213786	47.486477
2333.482074	82888.018294	47.491482
2329.790451	81705.505179	47.496487
2326.210060	80517.892470	47.501492
2322.352775	79341.474281	47.506497
2318.855530	78156.539902	47.511501
2315.115150	76976.418874	47.516506
2311.250831	75808.102599	47.521511
2308.129198	74638.386926	47.526516
2304.680026	73460.239731	47.531521
2300.884374	72297.271205	47.536525
2297.410125	71124.081831	47.541530
2293.618856	69962.662772	47.546535
2289.764425	68798.150123	47.551540
2286.274038	67636.489330	47.556545
2282.627282	66487.797395	47.561549
2279.367065	65328.991634	47.566554
2275.498148	64171.603406	47.571559
2272.118262	63014.502825	47.576564
2268.360531	61873.888733	47.581569
2264.562618	60718.902129	47.586573
2261.126559	59575.811508	47.591578
2257.529564	58439.259213	47.596583
2253.654194	57304.497775	47.601588
2250.008574	56164.563523	47.606593
2246.470167	55035.268624	47.611597
2243.162898	53894.945540	47.616602
2239.071741	52778.203307	47.621607
2235.272119	51641.460288	47.626612
2232.177615	50525.405395	47.631617
2228.395584	49413.603086	47.636621
2224.488633	48284.481872	47.641626
2220.841893	47174.117807	47.646631
2217.327364	46065.087400	47.651636
2213.694538	44970.113817	47.656641
2209.777288	43867.501334	47.661645
2206.157393	42763.469987	47.666650
2202.496011	41673.691156	47.671655
2198.810665	40594.317879	47.676660
2195.103914	39503.772323	47.681665
2191.549882	38424.193999	47.686669
2187.977899	37338.224780	47.691674
2184.352590	36261.599534	47.696679
2180.762218	35184.572878	47.701684
2176.773472	34117.386693	47.706689
2172.789116	33063.703805	47.711693
2169.629998	31989.250578	47.716698
2165.323310	30947.760444	47.721703
2161.779514	29903.167417	47.726708
2157.722668	28859.626259	47.731713
2153.873290	27816.701204	47.736717
2150.511629	26781.242730	47.741722
2146.434296	25761.472562	47.746727
2142.566858	24735.277293	47.751732
2138.691177	23730.511758	47.756737
2135.089290	22723.143615	47.761741
2131.280792	21727.274208	47.766746
2127.468248	20738.372799	47.771751
2123.738451	19758.236623	47.776756
2119.551046	18775.015930	47.781761
2115.679021	17811.214351	47.786765
2112.046673	16855.384028	47.791770
2107.932345	15916.680510	47.796775
2104.207279	14969.960372	47.801780
2100.018549	14042.318772	47.806785
2095.235204	13137.227821	47.811789
2091.489515	12242.271995	47.816794
2085.932721	11383.475187	47.821799
2080.319160	10554.125608	47.826804
2075.192866	9736.382286	47.831809
2070.222356	8960.626195	47.836813
2065.215730	8214.082024	47.841818
2059.758852	7483.033428	47.846823
2055.262230	6792.786811	47.851828
2050.625569	6127.875317	47.856833
2045.055024	5499.490867	47.861837
2039.733689	4903.697704	47.866842
2033.504699	4367.895377	47.871847
2028.050566	3857.420549	47.876852
2022.986338	3377.688683	47.881857
2017.300218	2956.973906	47.886861
2012.553056	2550.433943	47.891866
2007.422434	2167.517372	47.896871
2002.788884	1823.766360	47.901876
1998.613296	1499.092906	47.906881
1994.411087	1214.856190	47.911885
1990.505538	929.052529	47.916890
1986.329160	662.741297	47.921895
1982.397287	431.204823	47.926900
1978.336083	209.670364	47.931905
1969.996466	119.325189	47.936909
1957.972883	169.524674	47.941914
1951.456081	173.009011	47.946919
1947.105600	173.449283	47.951924
1946.065860	167.477260	47.956929
1944.551808	168.675950	47.961933
1943.137580	172.731786	47.966938
1941.248258	177.757332	47.971943
1938.676455	177.159959	47.976948
1936.043117	170.766569	47.981953
1932.348864	169.832297	47.986957
1929.707099	174.830050	47.991962
1925.767860	168.308810	47.996967
1922.431396	169.859117	48.001972
1919.600572	162.148843	48.006977
1916.245337	177.645127	48.011981
1913.089877	165.727125	48.016986
1909.799402	166.545720	48.021991
1906.798403	169.900710	48.026996
1903.595576	166.488196	48.032001
1899.958317	173.827946	48.037005
1896.746492	167.857296	48.042010
1893.548016	174.217200	48.047015
1890.289925	169.709157	48.052020
1886.669126	163.188726	48.057025
1882.784872	167.264084	48.062029
1879.806932	163.772093	48.067034
1876.940904	168.801786	48.072039
1873.165571	170.354344	48.077044
1870.099819	166.730560	48.082049
1866.270297	171.379506	48.087053
1862.515612	161.861736	48.092058
1859.024174	169.181840	48.097063
1855.691553	169.497669	48.102068
1852.441123	169.012842	48.107073
1849.263585	169.880223	48.112077
1845.791293	175.675532	48.117082
1842.775995	171.411093	48.122087
1839.344015	160.798767	48.127092
1835.952655	161.601534	48.132097
1831.881782	169.347688	48.137101
1828.772364	161.731663	48.142106
1825.140130	165.514495	48.147111
1822.027638	172.031807	48.152116
1818.518971	161.111944	48.157121
1814.488987	167.750689	48.162125
1811.313706	166.558071	48.167130
1808.345023	154.807048	48.172135
1804.699720	156.902443	48.177140
1801.239171	162.313098	48.182145
1797.545313	158.003003	48.187149
1794.459824	161.921750	48.192154
1790.882606	161.494411	48.197159
1787.259397	160.220035	48.202164
1783.892462	164.448592	48.207169
1780.294187	163.698677	48.212173
1776.859703	160.588221	48.217178
1774.000900	166.097709	48.222183
1769.928281	163.327572	48.227188
1766.472637	157.920326	48.232193
1762.944201	164.205343	48.237197
1759.713384	167.156563	48.242202
1756.379482	164.565061	48.247207
1752.573087	167.334270	48.252212
1749.414187	157.745461	48.257217
1745.445337	164.089915	48.262221
1742.458761	162.776036	48.267226
1738.714242	161.599759	48.272231
1734.932899	164.184714	48.277236
1731.729662	156.067706	48.282241
1728.255899	156.187360	48.287245
1724.786876	159.476432	48.292250
1721.541854	157.013406	48.297255
1718.072579	159.302749	48.302260
1714.652011	154.620879	48.307265
1711.005937	165.863063	48.312269
1707.533339	165.210566	48.317274
1703.777841	165.643246	48.322279
1700.319740	155.253375	48.327284
1697.415298	152.591520	48.332289
1693.359330	163.170175	48.337293
1690.156837	159.169209	48.342298
1687.105207	165.968099	48.347303
1682.960026	162.219076	48.352308
1679.639462	159.616023	48.357313
1675.542279	166.034371	48.362317
1672.423447	162.051955	48.367322
1669.079732	163.312402	48.372327
1665.500927	158.278818	48.377332
1662.131375	149.219736	48.382337
1658.784898	159.794930	48.387341
1655.402781	156.641521	48.392346
1652.020070	153.057926	48.397351
1648.041104	159.596988	48.402356
1644.864107	151.804946	48.407361
1641.143037	155.642868	48.412365
1637.921159	154.875224	48.417370
1634.237704	158.469974	48.422375
1630.397081	156.850023	48.427380
1627.073501	155.054237	48.432385
1623.673897	161.129300	48.437389
1620.487761	163.292101	48.442394
1617.050796	160.935082	48.447399
1613.218922	164.053184	48.452404
1609.758818	153.356775	48.457409
1606.540698	158.147399	48.462413
1602.954705	153.241519	48.467418
1599.107284	146.079622	48.472423
1595.712385	154.893828	48.477428
1592.442028	156.183946	48.482433
1588.892981	159.941177	48.487437
1585.289510	152.598729	48.492442
1581.998434	152.895488	48.497447
1578.550531	156.852031	48.502452
1574.943434	157.122322	48.507457
1571.360803	154.367331	48.512461
1568.278819	145.911865	48.517466
1564.564288	150.226525	48.522471
1560.630788	147.368265	48.527476
1557.285203	143.462513	48.532481
1553.800788	154.334571	48.537485
1550.267434	144.013498	48.542490
1546.568195	143.871105	48.547495
1543.105361	145.624809	48.552500
1540.242702	138.954228	48.557505
1536.902310	147.778897	48.562509
1533.293562	145.470945	48.567514
1529.620771	147.017065	48.572519
1525.745167	149.737070	48.577524
1522.533581	146.670917	48.582529
1518.864236	151.209479	48.587533
1515.857717	153.581482	48.592538
1512.220443	150.774954	48.597543
1508.380781	155.232608	48.602548
1504.780348	141.179253	48.607553
1501.146381	152.011454	48.612557
1497.896577	141.532127	48.617562
1494.841848	154.162469	48.622567
1490.961971	152.061488	48.627572
1487.488367	149.166076	48.632577
1484.037798	149.962404	48.637581
1480.525769	146.016292	48.642586
1477.027191	151.546889	48.647591
1473.575626	154.687770	48.652596
1469.792943	151.957803	48.657601
1466.509484	162.301713	48.662605
1463.196316	151.446325	48.667610
1459.800381	155.587763	48.672615
1456.056087	157.736736	48.677620
1452.495286	147.837625	48.682625
1448.714588	164.359220	48.687629
1445.650792	152.559952	48.692634
1442.178609	152.673129	48.697639
1438.422672	148.107136	48.702644
1435.105145	143.428228	48.707649
1431.441770	152.528114	48.712653
1428.077401	140.336138	48.717658
1424.387678	143.258043	48.722663
1420.703800	152.316847	48.727668
1417.972290	146.131988	48.732673
1414.237250	141.657651	48.737677
1410.542854	141.046305	48.742682
1407.051008	147.585126	48.747687
1403.278714	147.248573	48.752692
1400.250318	146.273547	48.757697
1396.609961	153.734145	48.762701
1392.938790	148.734114	48.767706
1389.629781	144.458859	48.772711
1385.451873	140.044366	48.777716
1382.973664	149.433319	48.782721
1379.046876	149.171580	48.787725
1375.870885	140.781526	48.792730
1372.234374	146.596341	48.797735
1368.699488	144.738808	48.802740
1365.257719	136.251156	48.807745
1361.103113	147.927371	48.812749
1357.962257	138.854768	48.817754
1354.665724	134.488989	48.822759
1350.973294	140.296743	48.827764
1347.486606	133.375894	48.832769
1343.847360	134.454910	48.837773
1340.646520	142.780046	48.842778
1337.269476	144.264119	48.847783
1333.474539	139.163264	48.852788
1329.934164	137.116776	48.857793
1326.440771	145.620593	48.862797
1322.677510	134.076418	48.867802
1319.634603	139.928041	48.872807
1316.449459	139.186392	48.877812
1313.064402	145.423780	48.882817
1308.957706	143.197027	48.887821
1305.549669	138.706348	48.892826
1302.007746	135.983056	48.897831
1298.179343	137.449211	48.902836
1295.181254	141.518925	48.907841
1291.506252	149.557627	48.912845
1287.973898	138.967594	48.917850
1284.228725	143.992673	48.922855
1280.678897	141.001702	48.927860
1277.555129	134.305648	48.932865
1273.852659	154.361666	48.937869
1270.446001	147.858594	48.942874
1266.889655	152.347911	48.947879
1263.518687	149.733914	48.952884
1260.274700	139.497391	48.957889
1256.417587	149.504031	48.962893
1252.851177	144.857826	48.967898
1249.534148	144.355148	48.972903
1246.136882	148.344994	48.977908
1242.754629	142.686018	48.982913
1238.771873	147.659720	48.987917
1235.151261	141.658403	48.992922
1232.048837	148.000269	48.997927
1228.434159	148.910963	49.002932
1225.394808	135.807642	49.007937
1221.981145	147.529261	49.012941
1218.221291	138.218254	49.017946
1214.557755	140.762802	49.022951
1210.470475	141.624099	49.027956
1207.460903	140.636696	49.032961
1203.465874	137.914773	49.037965
1200.309938	138.010163	49.042970
1197.065299	144.896331	49.047975
1193.348271	139.229672	49.052980
1190.362297	137.248307	49.057985
1186.618600	141.197492	49.062989
1182.714731	144.488370	49.067994
1179.765954	133.946235	49.072999
1175.870162	144.623354	49.078004
1172.668632	129.438351	49.083009
1168.980613	138.630751	49.088013
1165.241357	135.349937	49.093018
1161.824675	137.460380	49.098023
1158.190565	140.519205	49.103028
1154.956256	136.282967	49.108033
1151.858323	139.115481	49.113037
1147.954602	133.968463	49.118042
1144.553698	133.551720	49.123047
1140.481721	129.475106	49.128052
1137.295940	135.197281	49.133057
1133.778485	137.681021	49.138061
1130.965477	144.474320	49.143066
1127.648710	138.390679	49.148071
1123.459274	135.484088	49.153076
1120.035754	136.307944	49.158081
1116.297551	140.056973	49.163085
1112.835650	143.338795	49.168090
1109.654798	133.611320	49.173095
1105.857952	131.794900	49.178100
1102.547377	129.665065	49.183105
1098.675074	139.424186	49.188109
1095.330291	133.990363	49.193114
1091.774010	126.397136	49.198119
1088.336060	136.474240	49.203124
1085.332395	138.510554	49.208129
1081.446764	144.997228	49.213133
1078.097256	140.105161	49.218138
1074.222448	135.994542	49.223143
1070.692035	144.187846	49.228148
1067.378854	136.793850	49.233153
1064.131428	141.456331	49.238157
1060.596338	126.184399	49.243162
1056.772876	133.354218	49.248167
1053.379006	136.590605	49.253172
1050.007847	130.271900	49.258177
1046.491038	128.044659	49.263181
1042.911220	130.914686	49.268186
1039.048903	132.898786	49.273191
1035.989676	133.380893	49.278196
1032.720560	132.899263	49.283201
1028.688696	132.369375	49.288205
1025.284562	129.513886	49.293210
1022.046556	130.046135	49.298215
1018.344522	127.974457	49.303220
1015.159525	126.941816	49.308225
1011.059433	133.933496	49.313229
1007.881038	138.015699	49.318234
1004.550440	138.239743	49.323239
1000.799598	141.405487	49.328244
997.572921	137.724942	49.333249
993.653417	143.422833	49.338253
990.416374	136.159320	49.343258
987.014130	134.265346	49.348263
983.188022	130.143980	49.353268
980.088224	129.496650	49.358273
976.226542	137.792468	49.363277
972.676938	129.242778	49.368282
969.523782	135.735024	49.373287
965.699494	131.654510	49.378292
962.289646	120.833480	49.383297
958.852825	133.504760	49.388301
955.382316	125.831724	49.393306
951.642092	128.113121	49.398311
948.673284	123.072915	49.403316
945.064828	123.843530	49.408321
941.336110	134.497720	49.413325
937.979051	133.881194	49.418330
934.353821	125.963470	49.423335
930.735418	139.824309	49.428340
927.218505	129.931230	49.433345
923.680529	129.997945	49.438349
920.064104	122.638843	49.443354
916.880200	122.972828	49.448359
913.578144	124.236489	49.453364
910.153083	129.692468	49.458369
906.091582	133.096718	49.463373
902.620785	136.440115	49.468378
899.237918	131.490069	49.473383
895.329281	139.530671	49.478388
892.118140	127.976190	49.483393
888.699753	135.452803	49.488397
885.254419	137.972793	49.493402
882.285763	131.157690	49.498407
878.438704	135.926775	49.503412
874.953426	127.873265	49.508417
871.220864	138.926720	49.513421
867.579580	123.361464	49.518426
864.406910	128.290711	49.523431
860.520471	135.903899	49.528436
857.437193	135.279333	49.533441
853.981961	134.143528	49.538445
850.504592	125.329479	49.543450
846.605044	130.435828	49.548455
843.004292	137.127914	49.553460
839.769925	128.959199	49.558465
836.013993	128.250143	49.563469
832.327888	130.893275	49.568474
829.407636	129.967940	49.573479
825.414166	144.311492	49.578484
822.245021	128.903280	49.583489
818.731784	133.123395	49.588493
815.635157	134.244189	49.593498
811.875111	134.500746	49.598503
808.058536	135.658349	49.603508
805.062293	135.978804	49.608513
800.753388	138.526483	49.613517
797.287214	145.320902	49.618522
794.359580	136.525193	49.623527
790.424717	136.160555	49.628532
787.733454	141.394098	49.633537
783.714804	132.481337	49.638541
780.226772	135.403525	49.643546
776.757289	133.615073	49.648551
773.181557	132.365289	49.653556
769.899888	124.928522	49.658561
766.094943	124.869421	49.663565
762.751075	127.857625	49.668570
758.940544	125.265199	49.673575
755.635805	128.952805	49.678580
752.388669	128.948729	49.683585
748.655897	132.750824	49.688589
745.013190	124.737845	49.693594
741.462730	130.216680	49.698599
737.851323	125.245542	49.703604
734.873939	120.500990	49.708609
731.443007	127.922663	49.713613
727.829368	119.822884	49.718618
724.279086	117.819315	49.723623
720.441110	130.306699	49.728628
717.305647	127.656031	49.733633
713.606161	121.895093	49.738637
709.967345	119.645963	49.743642
706.731505	123.057035	49.748647
703.009063	123.826610	49.753652
699.782316	121.104823	49.758657
695.862214	120.120974	49.763661
692.477855	118.521710	49.768666
689.034955	118.665375	49.773671
685.257086	125.821850	49.778676
682.353646	119.888805	49.783681
679.006661	116.239881	49.788685
675.220788	109.258614	49.793690
671.736896	110.079429	49.798695
668.063538	123.847691	49.803700
664.680490	119.286920	49.808705
661.293022	123.253270	49.813709
657.745648	114.595812	49.818714
654.222925	114.157197	49.823719
650.312613	115.819931	49.828724
647.241597	116.329320	49.833729
643.668274	122.026903	49.838733
639.808277	122.783244	49.843738
636.566711	116.295723	49.848743
633.483466	123.849637	49.853748
629.877546	107.975258	49.858753
625.871463	122.248062	49.863757
622.229548	113.520005	49.868762
619.143546	119.511439	49.873767
615.321518	107.831303	49.878772
611.959531	109.161402	49.883777
608.387266	120.898511	49.888781
604.944810	125.231000	49.893786
601.836356	116.065059	49.898791
597.848329	126.522677	49.903796
594.534176	124.542290	49.908801
591.052391	113.248643	49.913805
587.684189	114.943560	49.918810
584.275162	107.722981	49.923815
580.214607	124.272769	49.928820
576.900727	114.389194	49.933825
573.193520	111.926204	49.938829
569.951376	116.736702	49.943834
566.755395	111.621485	49.948839
563.069173	120.639775	49.953844
559.584531	119.182820	49.958849
555.932674	125.057251	49.963853
552.503297	118.599179	49.968858
549.284612	118.207900	49.973863
544.993851	120.518729	49.978868
542.017479	124.506156	49.983873
538.309740	126.570649	49.988877
534.770901	116.871023	49.993882
531.431471	124.174020	49.998887
527.543799	120.011883	50.003892
524.709200	118.744199	50.008897
521.281595	118.426781	50.013901
517.399677	117.335789	50.018906
513.923324	120.253076	50.023911
510.466548	122.158049	50.028916
506.892710	116.443968	50.033921
503.408485	120.226206	50.038925
499.935193	118.805462	50.043930
496.432025	126.137280	50.048935
492.665353	130.083987	50.053940
489.378135	124.385130	50.058945
486.374856	115.142653	50.063949
482.444467	121.095537	50.068954
478.986683	120.542414	50.073959
475.046772	128.869637	50.078964
471.997469	116.543350	50.083969
468.167249	126.112581	50.088973
464.901173	129.632874	50.093978
461.548473	118.818946	50.098983
457.994047	134.261274	50.103988
454.661524	121.340266	50.108993
451.108762	114.376376	50.113997
447.132445	117.397307	50.119002
443.974243	122.751525	50.124007
439.775094	116.932935	50.129012
436.970943	124.085679	50.134017
433.804602	116.197556	50.139021
429.940549	111.614147	50.144026
426.567784	109.064035	50.149031
422.802128	115.380282	50.154036
419.284848	112.681964	50.159041
415.405638	118.804028	50.164045
412.377740	116.842150	50.169050
409.016864	115.808800	50.174055
405.175694	114.743113	50.179060
401.848193	105.817219	50.184065
397.875397	114.962708	50.189069
394.481520	123.324652	50.194074
391.484458	116.583797	50.199079
387.964672	115.733535	50.204084
384.594529	114.325154	50.209089
381.064923	113.827613	50.214093
377.386143	111.499462	50.219098
373.855586	114.023489	50.224103
370.357412	118.880483	50.229108
366.741366	109.329078	50.234113
363.451532	119.535038	50.239117
360.023193	111.732281	50.244122
356.470709	112.592434	50.249127
352.525486	123.809067	50.254132
349.178935	114.215454	50.259137
346.049297	117.113293	50.264141
342.190678	128.743478	50.269146
338.457861	121.994505	50.274151
335.006727	122.459136	50.279156
331.880424	116.352323	50.284161
328.381904	115.036842	50.289165
324.706122	120.718947	50.294170
321.673777	121.880455	50.299175
318.123436	121.569686	50.304180
314.554679	118.518802	50.309185
310.777429	126.377675	50.314189
306.657182	125.561393	50.319194
303.835447	123.418560	50.324199
300.130847	116.209602	50.329204
296.952065	110.183794	50.334209
293.287286	118.002904	50.339213
289.651486	114.991008	50.344218
286.086334	101.486437	50.349223
282.153196	111.764715	50.354228
279.421012	110.810102	50.359233
275.908110	114.185621	50.364237
272.144058	117.097444	50.369242
268.886615	112.482361	50.374247
264.609961	125.478370	50.379252
262.037895	116.282333	50.384257
258.112712	120.633614	50.389261
254.681933	119.279075	50.394266
251.103162	111.987156	50.399271
247.566146	118.707418	50.404276
244.166965	118.240121	50.409281
240.836879	110.551742	50.414285
236.969782	107.269217	50.419290
233.782908	105.338637	50.424295
230.221980	116.542564	50.429300
226.792938	118.063644	50.434305
222.976086	112.656683	50.439309
219.693112	118.071644	50.444314
216.181471	109.503713	50.449319
213.087694	110.804595	50.454324
209.511546	103.233875	50.459329
205.709385	119.097885	50.464333
201.891644	111.580831	50.469338
198.460080	108.426249	50.474343
195.206557	114.317498	50.479348
191.848764	106.896077	50.484353
187.907163	115.827947	50.489357
184.591561	107.055313	50.494362
181.126938	107.370255	50.499367
177.181258	110.313733	50.504372
173.954734	105.807743	50.509377
170.813665	114.696465	50.514381
166.827516	102.934713	50.519386
163.871054	99.854414	50.524391
159.930369	111.092543	50.529396
156.658015	107.267625	50.534401
153.192385	112.527723	50.539405
149.393673	111.265672	50.544410
145.938669	109.041771	50.549415
142.700416	117.031395	50.554420
139.138306	108.645415	50.559425
135.998519	116.743002	50.564429
132.383069	110.662286	50.569434
128.749424	112.595110	50.574439
124.901255	109.806386	50.579444
121.493205	108.018068	50.584449
118.192172	110.977635	50.589453
114.327309	117.559479	50.594458
110.825445	111.274314	50.599463
107.172593	108.916910	50.604468
103.995556	112.597380	50.609473
100.352551	103.667270	50.614477
97.055721	110.517632	50.619482
93.755276	106.276359	50.624487
90.353695	114.728187	50.629492
86.781966	118.084520	50.634497
83.051691	105.804995	50.639501
79.635135	102.790482	50.644506
76.613680	108.272083	50.649511
72.716219	112.277408	50.654516
68.898633	117.428163	50.659521
65.103571	120.544246	50.664525
61.733501	112.204145	50.669530
58.304964	104.977368	50.674535
55.046445	113.792774	50.679540
51.846530	113.300661	50.684545
48.145707	112.690875	50.689549
44.242067	111.777508	50.694554
40.933689	112.355930	50.699559
37.222640	112.260283	50.704564
34.346986	118.462543	50.709569
30.360368	112.430537	50.714573
27.115908	107.573075	50.719578
23.522436	114.121923	50.724583
19.987018	116.112168	50.729588
16.460057	112.248104	50.734593
13.154241	111.016456	50.739597
9.140080	104.817935	50.744602
5.759650	102.879804	50.749607
2.136241	112.255437	50.754612