Thu Aug 25 12:37:46 2022

Number of Points = 9925

Depth (nm)	Load (N)	Time (s)
1.696161	99.225707	0.000000
1.772105	103.434230	0.005005
1.904567	107.083402	0.010010
1.889171	107.582470	0.015014
1.894619	87.602309	0.020019
1.555676	82.403492	0.025024
1.319711	83.345246	0.030029
1.063552	80.329118	0.035034
0.726999	64.996368	0.040038
0.631639	61.100832	0.045043
0.597865	60.220211	0.050048
0.556661	57.705085	0.055053
0.113039	49.770200	0.060058
-0.191409	45.856807	0.065062
-0.438424	33.553599	0.070067
-0.705340	28.061938	0.075072
-1.492724	23.167520	0.080077
-1.328383	23.255609	0.085082
-1.924437	11.263370	0.090086
-2.050766	17.034826	0.095091
-2.240377	19.114596	0.100096
-2.466865	9.253778	0.105101
-2.558826	-4.007007	0.110106
-3.436194	6.121556	0.115110
-3.188866	5.835974	0.120115
-3.637585	-0.244126	0.125120
-4.409035	8.007553	0.130125
-4.514236	6.875534	0.135130
-5.116812	8.804871	0.140134
-4.842855	6.243536	0.145139
-5.140541	8.318092	0.150144
-5.056708	5.954225	0.155149
-5.066555	-3.358397	0.160154
-5.935617	6.246845	0.165158
-6.254691	-2.672477	0.170163
-6.410906	-1.607182	0.175168
-6.687573	-4.075914	0.180173
-6.404321	-1.880411	0.185178
-6.776998	0.860792	0.190182
-6.915229	-3.619636	0.195187
-7.465028	-3.327905	0.200192
-7.655481	1.517120	0.205197
-8.100817	3.690740	0.210202
-8.834561	6.403095	0.215206
-8.654712	-6.969878	0.220211
-9.229946	5.639189	0.225216
-9.685337	3.508507	0.230221
-9.264728	-2.945082	0.235226
-9.751232	5.948485	0.240230
-9.529902	-3.413013	0.245235
-9.499541	-1.665105	0.250240
-10.013742	-4.216843	0.255245
-10.585438	-9.812598	0.260250
-11.013542	-1.817200	0.265254
-10.515981	-2.366617	0.270259
-10.935860	-10.390615	0.275264
-11.805064	5.548492	0.280269
-12.215165	-2.103719	0.285274
-12.627337	1.671894	0.290278
-12.234423	-1.888843	0.295283
-12.519811	6.672656	0.300288
-12.394511	4.488954	0.305293
-12.849213	-4.146524	0.310298
-13.492040	-3.925638	0.315302
-13.745620	-8.204493	0.320307
-13.936608	-2.919623	0.325312
-14.433025	2.688351	0.330317
-14.015292	-1.891842	0.335322
-14.314880	3.587216	0.340326
-15.029654	-6.314145	0.345331
-15.151172	-0.293512	0.350336
-15.502765	-10.125225	0.355341
-15.233542	-20.171262	0.360346
-15.537440	-5.640025	0.365350
-15.886697	-1.077003	0.370355
-16.801877	-4.749160	0.375360
-16.847241	-1.293612	0.380365
-16.822398	2.919730	0.385370
-17.193247	3.971199	0.390374
-16.594511	3.905804	0.395379
-17.352774	-2.116303	0.400384
-18.081599	-7.029376	0.405389
-18.056999	-4.473808	0.410394
-18.661260	10.335458	0.415398
-18.327893	-0.973489	0.420403
-18.765658	-1.898376	0.425408
-19.721818	5.727345	0.430413
-19.666569	3.323666	0.435418
-19.902684	7.830997	0.440422
-19.462599	-8.914187	0.445427
-19.660043	3.939405	0.450432
-19.953978	-1.016501	0.455437
-20.303470	-4.106574	0.460442
-21.224076	3.545213	0.465446
-21.305447	4.253933	0.470451
-21.167934	-1.158716	0.475456
-21.575878	-4.302906	0.480461
-21.758727	-3.926300	0.485466
-22.460771	-4.528203	0.490470
-22.610120	0.395802	0.495475
-22.442243	-3.411250	0.500480
-22.687103	7.026335	0.505485
-22.641774	-0.817456	0.510490
-23.082046	2.222240	0.515494
-23.597442	3.419745	0.520499
-23.924007	-2.881973	0.525504
-24.353417	10.355983	0.530509
-24.628058	3.030561	0.535514
-24.806784	5.020038	0.540518
-24.443839	1.365919	0.545523
-25.056070	3.236658	0.550528
-25.661495	4.780463	0.555533
-25.685169	-3.223358	0.560538
-25.900957	-5.508639	0.565542
-25.560267	-1.714947	0.570547
-26.038587	0.960551	0.575552
-27.332590	10.869659	0.580557
-27.242698	0.867528	0.585562
-27.477103	4.545686	0.590566
-27.374816	4.026564	0.595571
-27.193889	4.956777	0.600576
-27.583629	4.631808	0.605581
-27.354309	0.457623	0.610586
-27.921373	-6.160751	0.615590
-28.157918	-2.700559	0.620595
-29.111411	-3.743955	0.625600
-29.807621	8.887232	0.630605
-29.974523	1.804359	0.635610
-29.410239	4.158309	0.640614
-29.729152	1.851220	0.645619
-29.471669	0.466222	0.650624
-29.823297	-0.886613	0.655629
-30.398803	-2.814975	0.660634
-31.050541	-3.076746	0.665638
-31.299416	1.274394	0.670643
-31.247292	-2.811914	0.675648
-31.370281	5.527985	0.680653
-31.896845	-2.381222	0.685658
-32.525316	-3.753954	0.690662
-32.926585	0.149664	0.695667
-32.707321	1.937577	0.700672
-32.761825	-0.955107	0.705677
-32.879574	3.334360	0.710682
-33.116334	-5.186567	0.715686
-33.488265	3.233465	0.720691
-33.792153	-4.264541	0.725696
-34.560415	0.636216	0.730701
-34.027439	-8.960770	0.735706
-34.462302	1.946344	0.740710
-35.108118	1.863979	0.745715
-35.802076	-5.601381	0.750720
-35.752358	9.045302	0.755725
-35.626041	0.726912	0.760730
-35.943617	-0.593293	0.765734
-36.128617	9.252782	0.770739
-35.760369	0.735133	0.775744
-36.260502	0.177525	0.780749
-36.661855	2.122790	0.785754
-37.175871	0.634048	0.790758
-37.079142	4.152754	0.795763
-37.351068	0.215295	0.800768
-38.228705	5.199630	0.805773
-38.390457	2.181381	0.810778
-38.468423	10.232653	0.815782
-38.618569	3.710303	0.820787
-38.644264	-1.961511	0.825792
-38.990657	-1.328325	0.830797
-39.188918	-2.866541	0.835802
-39.314495	-4.333888	0.840806
-39.716724	-12.832048	0.845811
-39.816887	-7.295655	0.850816
-40.781086	0.979894	0.855821
-41.226807	-4.278093	0.860826
-41.601022	2.959052	0.865830
-41.650235	3.627931	0.870835
-41.542177	-2.023711	0.875840
-42.052009	-0.074103	0.880845
-41.520460	-2.574558	0.885850
-41.792400	-4.971262	0.890854
-42.011251	-3.022955	0.895859
-42.310413	-6.022836	0.900864
-42.924816	-0.551400	0.905869
-42.964354	-6.594367	0.910874
-43.013475	-1.183029	0.915878
-43.787100	-8.828894	0.920883
-44.444185	-6.444926	0.925888
-45.037688	-7.633310	0.930893
-44.420219	-8.068639	0.935898
-44.633473	-11.309770	0.940902
-44.905216	-10.450999	0.945907
-44.847421	-2.110957	0.950912
-45.014432	3.900986	0.955917
-45.552771	-11.010932	0.960922
-46.141348	-6.195278	0.965926
-46.045883	-7.868102	0.970931
-46.211468	0.864447	0.975936
-46.195693	-0.786400	0.980941
-46.975062	3.081550	0.985946
-47.647421	3.265937	0.990950
-47.398850	10.446631	0.995955
-47.182530	9.093392	1.000960
-47.680192	6.222688	1.005965
-48.481094	-5.304000	1.010970
-48.860626	-0.043371	1.015974
-48.899223	5.312535	1.020979
-48.752620	3.527294	1.025984
-49.274922	1.539977	1.030989
-49.014746	1.999027	1.035994
-49.169750	-6.142402	1.040998
-49.867029	1.059941	1.046003
-50.104015	0.957811	1.051008
-50.658555	2.841658	1.056013
-50.418713	-6.155741	1.061018
-50.637518	3.433035	1.066022
-51.481147	6.703613	1.071027
-51.659310	-5.876105	1.076032
-52.133612	7.096797	1.081037
-51.795381	5.648526	1.086042
-51.973759	6.350299	1.091046
-52.297417	11.893242	1.096051
-51.993465	-3.027270	1.101056
-53.026618	15.411591	1.106061
-53.058451	10.667718	1.111066
-53.636102	7.385604	1.116070
-53.770748	2.442706	1.121075
-53.558795	2.741634	1.126080
-55.004576	9.017220	1.131085
-55.173954	5.430690	1.136090
-55.112569	-7.123285	1.141094
-54.932406	1.922085	1.146099
-55.000555	-6.650568	1.151104
-55.840149	11.292888	1.156109
-55.555290	3.490660	1.161114
-55.636368	-2.140838	1.166118
-55.628773	5.928662	1.171123
-56.142112	3.186967	1.176128
-56.444597	9.447928	1.181133
-56.789092	-0.717091	1.186138
-57.311477	4.787385	1.191142
-57.983024	5.132997	1.196147
-57.934358	6.020659	1.201152
-58.392330	16.137298	1.206157
-57.988597	5.741141	1.211162
-58.654964	2.156553	1.216166
-58.467397	3.240750	1.221171
-58.063051	-1.312036	1.226176
-59.291814	6.195049	1.231181
-59.579368	4.449361	1.236186
-59.919018	5.378884	1.241190
-59.977558	5.008349	1.246195
-59.742291	-2.786107	1.251200
-60.313736	12.615967	1.256205
-60.749757	14.607796	1.261210
-60.775072	1.757352	1.266214
-61.078411	-0.539520	1.271219
-61.229691	7.235334	1.276224
-62.364344	12.889533	1.281229
-62.621407	4.571102	1.286234
-62.316349	6.680930	1.291238
-62.376417	5.510202	1.296243
-62.499365	9.094966	1.301248
-63.163493	5.348676	1.306253
-62.757470	3.203247	1.311258
-62.949991	-1.841312	1.316262
-63.802064	1.506519	1.321267
-63.621212	-1.552755	1.326272
-64.529788	0.443514	1.331277
-64.221021	-5.299687	1.336282
-64.534615	2.215860	1.341286
-65.570635	7.247161	1.346291
-65.323875	7.081889	1.351296
-65.837488	12.221160	1.356301
-65.668702	6.949143	1.361306
-66.057589	4.216422	1.366310
-65.806213	7.666603	1.371315
-66.126503	-1.189248	1.376320
-67.112816	10.028903	1.381325
-67.078753	5.211431	1.386330
-67.400659	4.945438	1.391334
-67.333509	3.128353	1.396339
-67.361271	4.382330	1.401344
-67.736841	6.291920	1.406349
-68.189907	3.642021	1.411354
-68.467716	-1.075961	1.416358
-68.984644	8.141912	1.421363
-68.847138	1.175860	1.426368
-69.186849	14.466199	1.431373
-69.088626	4.041984	1.436378
-69.450562	-3.105237	1.441382
-69.874572	3.817006	1.446387
-69.993989	0.776307	1.451392
-70.322157	-1.946945	1.456397
-71.443458	-1.685884	1.461402
-71.609186	4.161341	1.466406
-71.586714	3.034629	1.471411
-71.577416	4.697251	1.476416
-71.897995	-0.561360	1.481421
-71.913705	-3.064651	1.486426
-72.148692	2.312535	1.491430
-72.423217	3.674780	1.496435
-71.668889	-0.815786	1.501440
-72.798588	8.118452	1.506445
-73.055720	11.743224	1.511450
-73.140032	6.814586	1.516454
-73.719341	6.114362	1.521459
-73.869396	7.602637	1.526464
-74.679958	0.196679	1.531469
-74.542128	1.139971	1.536474
-74.916558	2.938651	1.541478
-74.695817	-1.107639	1.546483
-74.878291	-4.594038	1.551488
-75.695623	7.758733	1.556493
-75.697256	2.159079	1.561498
-75.623758	-2.294409	1.566502
-76.306046	2.314468	1.571507
-76.842286	-1.413893	1.576512
-77.180453	6.032739	1.581517
-77.100797	8.750525	1.586522
-77.134342	4.870628	1.591526
-77.507195	2.882042	1.596531
-77.014328	-4.687019	1.601536
-77.615706	6.436013	1.606541
-78.156633	-2.258714	1.611546
-78.575819	2.334248	1.616550
-79.142669	2.233186	1.621555
-79.066794	-14.473901	1.626560
-78.934443	-2.149721	1.631565
-79.421849	-9.305753	1.636570
-80.093115	-8.722902	1.641574
-80.147316	5.152280	1.646579
-80.282468	2.759453	1.651584
-80.472002	-6.297215	1.656589
-80.398416	5.343315	1.661594
-80.995134	5.240605	1.666598
-81.580134	3.120745	1.671603
-81.650404	-6.758205	1.676608
-81.543159	0.523720	1.681613
-81.594227	-1.287495	1.686618
-82.090923	-3.769204	1.691622
-83.175721	-0.783539	1.696627
-83.333310	-9.908486	1.701632
-83.595903	7.451008	1.706637
-83.016561	2.073534	1.711642
-83.388966	-2.715047	1.716646
-83.606077	4.200088	1.721651
-83.432885	-2.847484	1.726656
-84.154573	-0.757111	1.731661
-84.622093	-3.116841	1.736666
-84.592364	-2.270505	1.741670
-85.132498	3.334828	1.746675
-84.847271	2.204910	1.751680
-85.086129	12.356815	1.756685
-85.620429	5.869352	1.761690
-85.876631	3.599896	1.766694
-86.070512	-5.316886	1.771699
-86.714455	-3.229204	1.776704
-87.136507	4.993037	1.781709
-87.509524	3.371474	1.786714
-87.442481	-2.530004	1.791718
-87.934303	7.329341	1.796723
-87.568226	-5.610896	1.801728
-87.589135	-5.421016	1.806733
-87.457269	2.505622	1.811738
-88.340168	-2.301044	1.816742
-88.801751	-2.592607	1.821747
-88.793016	-13.939260	1.826752
-89.185939	-1.222727	1.831757
-89.407270	0.868339	1.836762
-89.958846	-3.164502	1.841766
-90.717834	-2.444518	1.846771
-90.511893	-3.910026	1.851776
-90.715577	2.506294	1.856781
-90.469738	-1.237043	1.861786
-90.563513	-0.501070	1.866790
-91.428572	-1.985423	1.871795
-91.507972	-8.800424	1.876800
-92.177443	2.624341	1.881805
-92.331583	3.319153	1.886810
-92.123486	-3.746543	1.891814
-92.406770	0.198700	1.896819
-92.344214	-2.297872	1.901824
-93.455868	-2.231309	1.906829
-93.190483	3.535708	1.911834
-93.489186	7.916804	1.916838
-94.171349	9.618171	1.921843
-93.802986	4.504709	1.926848
-93.999513	11.388146	1.931853
-94.582028	6.091485	1.936858
-94.921935	6.372479	1.941862
-95.532989	3.984620	1.946867
-95.524341	11.870457	1.951872
-95.495325	9.211460	1.956877
-95.668853	2.221378	1.961882
-95.632738	3.566587	1.966886
-96.492018	6.630812	1.971891
-96.820453	-2.960913	1.976896
-96.855988	5.710128	1.981901
-96.926127	-1.419538	1.986906
-96.815177	0.575169	1.991910
-97.225037	-3.764615	1.996915
-98.140754	-2.590478	2.006912
-97.467390	-2.170247	2.016909
-97.207674	-5.267991	2.026906
-96.565741	0.773687	2.036902
-95.927576	-0.865977	2.046899
-95.789445	1.218857	2.056896
-95.065392	-3.240942	2.066893
-94.533550	3.872867	2.076890
-94.470638	-0.119039	2.086886
-93.456925	3.377656	2.096883
-93.112885	-3.262239	2.106880
-92.219125	0.231077	2.116877
-91.710207	-3.824378	2.126874
-91.767006	-0.172614	2.136870
-91.207024	0.423774	2.146867
-90.341367	0.104285	2.156864
-90.050358	0.907545	2.166861
-89.704457	5.351519	2.176858
-88.763050	6.851155	2.186854
-88.673114	-1.871356	2.196851
-88.145543	4.387816	2.206848
-87.455990	-4.343119	2.216845
-87.136756	1.340478	2.226842
-86.346189	4.577534	2.236838
-85.972331	1.794524	2.246835
-85.825606	0.855923	2.256832
-85.115190	0.161616	2.266829
-84.570378	0.475279	2.276826
-83.855510	-0.108852	2.286822
-83.269596	1.202565	2.296819
-83.124693	-1.446367	2.306816
-83.017979	1.951695	2.316813
-82.111172	4.746051	2.326810
-81.591859	0.540079	2.336806
-80.658229	8.455748	2.346803
-80.570703	3.272054	2.356800
-80.391622	-2.543705	2.366797
-79.429201	-1.379982	2.376794
-78.775988	2.806764	2.386790
-78.523629	5.466081	2.396787
-77.990590	3.846058	2.406784
-77.480635	0.794634	2.416781
-76.977184	2.391405	2.426778
-76.655442	2.024096	2.436774
-76.292531	1.444429	2.446771
-75.672852	5.820164	2.456768
-75.005763	6.726055	2.466765
-73.973812	3.976144	2.476762
-73.676108	5.161661	2.486758
-73.599447	2.631126	2.496755
-73.736219	6.038831	2.506752
-72.473648	-0.339510	2.516749
-71.884415	1.481405	2.526746
-71.141568	-0.713187	2.536742
-70.944726	-1.722997	2.546739
-71.070797	6.868734	2.556736
-69.850664	3.059799	2.566733
-69.563177	3.033646	2.576730
-68.763203	0.684383	2.586726
-68.159862	6.906343	2.596723
-67.887478	1.066458	2.606720
-67.740476	1.103499	2.616717
-67.099628	-2.494289	2.626714
-66.324796	5.360731	2.636710
-66.219999	8.537349	2.646707
-65.508285	0.889499	2.656704
-65.048442	-2.014688	2.666701
-64.641044	3.043709	2.676698
-63.743899	4.753024	2.686694
-63.661255	9.349123	2.696691
-62.814940	8.722223	2.706688
-62.393693	-2.326690	2.716685
-62.156953	-3.554995	2.726682
-61.236418	-0.566383	2.736678
-60.828848	6.094900	2.746675
-60.617802	0.717623	2.756672
-59.732398	0.426722	2.766669
-59.438490	3.244255	2.776666
-59.334646	4.903641	2.786662
-58.278969	4.408663	2.796659
-57.831929	3.340643	2.806656
-57.418705	-1.719853	2.816653
-57.052504	-3.659024	2.826650
-56.518576	3.356261	2.836646
-56.093412	4.445779	2.846643
-55.096510	3.586209	2.856640
-54.759673	1.623128	2.866637
-54.779431	0.225938	2.876634
-53.729328	0.634659	2.886630
-53.509795	5.320183	2.896627
-53.344048	2.417728	2.906624
-52.366726	-2.572765	2.916621
-52.136848	-1.202391	2.926618
-51.151581	0.448767	2.936614
-50.476909	-2.916734	2.946611
-50.830517	0.068781	2.956608
-50.136784	-4.744228	2.966605
-49.208861	-8.266619	2.976602
-48.826932	1.474623	2.986598
-48.586157	-2.855599	2.996595
-47.908085	1.365269	3.006592
-47.619618	0.090846	3.016589
-46.849253	-4.838707	3.026586
-46.244189	1.078874	3.036582
-46.105044	-3.295611	3.046579
-45.410387	0.586870	3.056576
-44.882580	-2.394489	3.066573
-44.578979	-0.687207	3.076570
-43.716252	-5.232089	3.086566
-43.572643	-8.235612	3.096563
-42.936384	-5.924717	3.106560
-42.181005	-4.433942	3.116557
-41.789372	-5.493279	3.126554
-41.687159	2.878950	3.136550
-41.156709	-7.296917	3.146547
-40.493451	0.011717	3.156544
-39.479724	-3.235847	3.166541
-38.921470	-0.592781	3.176538
-38.960241	1.716178	3.186534
-38.856876	1.782231	3.196531
-37.995633	-7.891100	3.206528
-37.323535	-1.727429	3.216525
-36.748013	-4.868319	3.226522
-36.139294	1.739273	3.236518
-35.803059	3.406597	3.246515
-35.770895	-3.181265	3.256512
-34.678347	-4.451795	3.266509
-34.423998	3.139491	3.276506
-33.925470	-0.847812	3.286502
-32.873302	-0.049771	3.296499
-32.871109	6.763731	3.306496
-32.803612	4.364512	3.316493
-31.735081	7.409135	3.326490
-31.160583	2.488095	3.336486
-31.169494	5.558985	3.346483
-30.928682	-2.233659	3.356480
-30.255661	2.564544	3.366477
-29.248616	5.067602	3.376474
-29.241416	0.580741	3.386470
-28.246930	-2.673312	3.396467
-27.549055	4.341632	3.406464
-27.319896	-4.801840	3.416461
-27.105993	1.981656	3.426458
-25.886548	4.612993	3.436454
-25.891530	5.187033	3.446451
-25.507008	9.409551	3.456448
-24.517407	-2.910009	3.466445
-24.245970	4.206597	3.476442
-24.268270	1.023160	3.486438
-23.449239	4.049856	3.496435
-22.995456	-0.690711	3.506432
-22.126561	-1.932532	3.516429
-21.271423	-0.748824	3.526426
-21.464486	2.987650	3.536422
-21.324048	5.499780	3.546419
-20.344368	4.915343	3.556416
-19.988214	0.690587	3.566413
-19.425808	5.439600	3.576410
-18.796448	-0.167947	3.586406
-18.515016	-8.521320	3.596403
-17.417782	-10.600373	3.606400
-16.891228	-4.486755	3.616397
-16.665969	-12.454356	3.626394
-16.837073	-7.815332	3.636390
-16.279782	-12.549939	3.646387
-15.462210	-12.114283	3.656384
-14.499596	-10.896730	3.666381
-14.237534	-4.735335	3.676378
-14.140793	-2.118157	3.686374
-13.489251	-3.363936	3.696371
-13.047633	-6.892491	3.706368
-12.155902	-6.740886	3.716365
-11.511756	-2.834648	3.726362
-11.208114	-6.465130	3.736358
-11.169127	-2.666813	3.746355
-10.104598	-2.101956	3.756352
-9.509739	-3.212141	3.766349
-9.209146	-3.740860	3.776346
-9.104671	-7.150067	3.786342
-8.356802	-6.244157	3.796339
-8.331364	-5.377109	3.806336
-7.196421	-2.105304	3.816333
-6.818561	-5.718904	3.826330
-6.432835	1.104196	3.836326
-5.490522	3.759951	3.846323
-5.341105	0.137793	3.856320
-4.959439	3.290039	3.866317
-4.406788	9.190498	3.876314
-4.053001	6.540514	3.886310
-3.663382	22.321586	3.896307
-3.173960	23.622788	3.906304
-2.402713	42.812841	3.916301
-2.331286	42.871228	3.926298
-1.845876	64.858925	3.936294
-1.642135	72.717934	3.946291
-0.750059	88.803646	3.956288
-0.215619	115.706526	3.966285
0.000000	126.123193	3.971290
0.217538	122.226074	3.976294
0.693309	139.178951	3.981299
0.627540	142.944611	3.986304
0.893390	137.119502	3.991309
0.589096	143.820561	3.996314
0.656516	136.368720	4.001318
0.399693	153.319334	4.006323
0.651304	148.977105	4.011328
1.117828	156.576135	4.016333
0.807940	169.751189	4.021338
1.189797	167.577891	4.026342
0.919609	168.838226	4.031347
1.185905	173.905966	4.036352
1.332089	165.748902	4.041357
0.998890	168.986987	4.046362
1.295381	162.081381	4.051366
0.662156	162.712055	4.056371
1.042289	166.771691	4.061376
1.052310	169.139742	4.066381
1.396646	173.451764	4.071386
1.555047	182.639848	4.076390
0.992229	160.714323	4.081395
0.887010	157.041776	4.086400
1.171761	165.476056	4.091405
1.421598	172.824302	4.096410
1.353932	174.600242	4.101414
1.075791	164.342466	4.106419
1.060267	177.737163	4.111424
1.074540	178.671352	4.116429
0.926255	180.146709	4.121434
1.330478	181.231774	4.126438
1.465079	179.960930	4.131443
1.294925	184.252324	4.136448
1.634036	172.879090	4.141453
1.200670	180.631781	4.146458
1.727174	179.891162	4.151462
1.536792	184.362898	4.156467
1.529302	179.118448	4.161472
1.393069	163.130960	4.166477
0.879575	164.676192	4.171482
0.893681	176.655196	4.176486
1.205413	182.117621	4.181491
1.246152	184.322671	4.186496
1.474685	178.149052	4.191501
1.448535	181.516202	4.196506
1.560328	182.798948	4.201510
1.631691	182.243537	4.206515
1.400858	177.420064	4.211520
1.527579	174.340766	4.216525
1.854120	184.252325	4.221530
2.056657	179.082537	4.226534
1.660454	179.350203	4.231539
1.606245	173.492972	4.236544
1.685376	169.399228	4.241549
1.253096	172.409225	4.246554
1.701398	181.317766	4.251558
1.152156	184.301798	4.256563
1.321172	180.399615	4.261568
1.521539	177.640976	4.266573
1.412468	184.241859	4.271578
1.412747	177.385822	4.276582
1.445353	176.146777	4.281587
1.172441	177.069014	4.286592
1.811814	173.830299	4.291597
1.439706	175.400836	4.296602
1.745934	178.589357	4.301606
1.407018	180.189496	4.306611
1.630958	187.915134	4.311616
1.870582	200.266949	4.316621
1.582276	206.054353	4.321626
2.210894	195.192572	4.326630
1.975365	190.762142	4.331635
1.817787	179.969768	4.336640
2.015488	174.617239	4.341645
1.790159	184.279903	4.346650
1.889036	169.831140	4.351654
1.623318	179.718432	4.356659
1.726905	175.560743	4.361664
1.526211	181.372377	4.366669
1.930164	202.924065	4.371674
2.026174	206.208804	4.376678
2.481030	200.727389	4.381683
1.871398	186.943287	4.386688
1.859409	179.127378	4.391693
1.764128	181.499275	4.396698
1.977647	176.005060	4.401702
1.886657	195.074780	4.406707
2.133089	206.451085	4.411712
2.303843	200.789554	4.416717
1.399038	201.899384	4.421722
1.869520	186.373642	4.426726
2.239613	201.732766	4.431731
2.081182	205.503466	4.436736
2.255986	203.523958	4.441741
2.083843	212.007701	4.446746
2.101526	204.193460	4.451750
2.258884	204.542075	4.456755
2.062578	205.433328	4.461760
1.823488	190.986881	4.466765
2.070221	204.546154	4.471770
1.981215	205.936294	4.476774
1.983398	210.270296	4.481779
2.070553	196.984461	4.486784
2.443194	210.033623	4.491789
2.051790	206.703302	4.496794
2.143431	202.012796	4.501798
1.925014	205.565102	4.506803
2.194375	215.858965	4.511808
2.115465	210.340954	4.516813
2.181600	208.245593	4.521818
2.421897	198.042611	4.526822
2.242181	204.746320	4.531827
2.051603	209.607240	4.536832
2.219245	205.670464	4.541837
2.012878	214.687924	4.546842
2.115781	205.898535	4.551846
2.160094	212.737991	4.556851
2.193162	221.287662	4.561856
2.604899	215.705430	4.566861
2.435898	218.332494	4.571866
1.959812	209.114958	4.576870
2.317704	221.454585	4.581875
2.182634	219.422386	4.586880
2.784042	226.348569	4.591885
2.417499	227.282315	4.596890
2.723751	232.353303	4.601894
2.887128	232.878149	4.606899
2.134376	225.744604	4.611904
2.648010	221.826382	4.616909
2.357123	229.559934	4.621914
2.720209	227.870468	4.626918
2.494290	235.283791	4.631923
2.304613	238.771487	4.636928
2.827389	231.352666	4.641933
2.668304	231.931200	4.646938
2.824385	227.334997	4.651942
2.254266	221.289660	4.656947
2.364091	224.581729	4.661952
2.463723	232.190820	4.666957
2.651959	226.915689	4.671962
2.459329	228.382178	4.676966
2.518403	227.553441	4.681971
2.330724	232.828371	4.686976
2.560117	233.507391	4.691981
2.616291	238.693495	4.696986
2.704270	235.544326	4.701990
2.935361	229.613900	4.706995
2.611919	235.397327	4.712000
2.902177	237.965092	4.717005
2.621294	241.758150	4.722010
2.715015	235.051968	4.727014
2.763565	236.632532	4.732019
2.777614	230.944924	4.737024
3.041139	230.846629	4.742029
2.506802	237.004790	4.747034
2.958397	231.621955	4.752038
2.985448	237.850347	4.757043
2.351874	230.596886	4.762048
2.370999	231.039928	4.767053
2.675751	240.182965	4.772058
2.977775	258.640674	4.777062
3.382944	250.556890	4.782067
3.002972	247.281719	4.787072
3.057515	236.876861	4.792077
2.796776	234.873841	4.797082
2.819697	242.507610	4.802086
2.942655	245.240796	4.807091
2.762079	249.593951	4.812096
2.648056	262.668782	4.817101
3.201823	255.615261	4.822106
3.063470	257.791432	4.827110
3.530123	265.785965	4.832115
2.880912	256.380390	4.837120
3.104017	250.568270	4.842125
3.166067	252.358696	4.847130
3.286520	256.462203	4.852134
2.715365	248.414331	4.857139
2.910771	252.582025	4.862144
3.068394	253.901888	4.867149
2.864016	262.580533	4.872154
2.740917	269.382965	4.877158
2.775361	262.540525	4.882163
3.090038	258.691434	4.887168
3.447503	254.535077	4.892173
3.227754	265.889547	4.897178
3.376059	262.493636	4.902182
3.203880	266.548082	4.907187
3.001885	261.033521	4.912192
3.237493	255.067578	4.917197
2.790071	259.646046	4.922202
2.866977	267.075211	4.927206
3.111167	266.226959	4.932211
3.380269	284.541155	4.937216
3.450581	279.876117	4.942221
3.604464	284.822295	4.947226
3.214479	267.719680	4.952230
3.078239	269.525356	4.957235
2.569813	288.562503	4.962240
3.179025	282.667730	4.967245
3.404013	297.730128	4.972250
3.763299	292.719248	4.977254
3.721811	290.982431	4.982259
3.577630	287.031218	4.987264
3.519471	277.074274	4.992269
3.600897	293.244347	4.997274
3.522442	294.313296	5.002278
3.790722	278.066168	5.007283
3.372500	278.232881	5.012288
3.444231	267.730398	5.017293
3.638451	280.696834	5.022298
3.531208	281.067926	5.027302
3.536323	279.966062	5.032307
3.523261	289.722078	5.037312
3.515937	290.143955	5.042317
3.183935	294.622089	5.047322
3.422873	291.851061	5.052326
3.771038	290.872621	5.057331
3.404735	285.108545	5.062336
3.869693	282.140752	5.067341
3.649821	299.310345	5.072346
3.656031	296.230926	5.077350
3.756537	298.451937	5.082355
3.930750	289.730429	5.087360
3.724605	282.875057	5.092365
4.114843	295.658928	5.097370
3.691267	293.463112	5.102374
3.593502	283.445930	5.107379
3.379320	293.736505	5.112384
3.775717	290.130871	5.117389
3.508808	297.895498	5.122394
3.503792	290.916858	5.127398
3.592440	295.427162	5.132403
3.582897	299.003708	5.137408
3.554544	288.137237	5.142413
3.453877	297.638059	5.147418
3.658810	299.247912	5.152422
3.872865	296.540895	5.157427
3.756700	293.974204	5.162432
3.976805	290.095631	5.167437
3.696691	293.417170	5.172442
3.774848	301.342872	5.177446
4.193057	306.605152	5.182451
3.556875	307.559002	5.187456
3.666817	308.259905	5.192461
4.213574	320.161877	5.197466
3.835237	315.753790	5.202470
4.004332	316.198648	5.207475
4.094571	320.528371	5.212480
4.096237	310.255145	5.217485
4.115138	319.287983	5.222490
3.931344	317.861367	5.227494
3.943296	318.938299	5.232499
3.746302	323.559805	5.237504
4.140322	321.710456	5.242509
4.104532	319.077384	5.247514
4.227339	316.973130	5.252518
4.116647	321.242585	5.257523
4.093600	322.688840	5.262528
4.778074	319.038064	5.267533
4.109911	313.248507	5.272538
4.053812	300.456449	5.277542
4.286171	309.133128	5.282547
4.044724	323.604228	5.287552
4.321582	313.341667	5.292557
4.305531	320.718979	5.297562
3.933597	310.361917	5.302566
4.291691	309.021245	5.307571
3.987147	313.640616	5.312576
3.909050	320.635337	5.317581
3.673978	326.427094	5.322586
3.936702	319.150224	5.327590
4.323974	326.942082	5.332595
3.956992	331.318135	5.337600
3.918647	328.438684	5.342605
4.346855	322.701975	5.347610
4.111285	314.705898	5.352614
4.155956	329.401098	5.357619
4.394407	338.962706	5.362624
4.392303	340.086134	5.367629
4.444851	346.098594	5.372634
4.737537	345.315509	5.377638
4.599977	345.688189	5.382643
4.070106	342.262476	5.387648
4.359908	335.462257	5.392653
4.403683	341.023664	5.397658
4.420740	342.602844	5.402662
4.570796	341.063806	5.407667
4.298098	331.051859	5.412672
4.557170	328.723770	5.417677
3.974268	341.378567	5.422682
4.515322	340.262332	5.427686
4.646300	330.816737	5.432691
4.558271	334.108188	5.437696
4.669787	333.805915	5.442701
4.628767	340.987827	5.447706
4.507432	347.903910	5.452710
4.647521	335.017811	5.457715
4.343073	343.085738	5.462720
4.842907	332.073207	5.467725
4.552533	342.628853	5.472730
4.849887	341.294532	5.477734
4.659876	339.232961	5.482739
4.355560	348.749899	5.487744
4.514857	337.727444	5.492749
4.744778	338.425369	5.497754
4.708184	341.471476	5.502758
4.621903	342.766285	5.507763
4.681721	344.307127	5.512768
4.557747	336.790276	5.517773
4.444404	344.859899	5.522778
4.230888	345.459620	5.527782
4.857649	349.471165	5.532787
4.855593	356.925395	5.537792
5.189559	363.352522	5.542797
4.732789	343.982345	5.547802
4.572914	341.637636	5.552806
4.745865	348.510773	5.557811
4.579174	352.940873	5.562816
5.060056	358.623628	5.567821
4.970646	353.322358	5.572826
4.726870	365.164720	5.577830
4.841780	362.144190	5.582835
4.509506	368.875027	5.587840
4.712758	360.351420	5.592845
4.824764	370.211273	5.597850
4.862678	366.712413	5.602854
5.059279	367.637028	5.607859
4.995748	362.423451	5.612864
5.190927	360.193956	5.617869
4.998686	366.232121	5.622874
5.009267	369.194910	5.627878
5.148233	358.128170	5.632883
5.102076	370.227480	5.637888
5.174002	361.480835	5.642893
5.369663	359.570810	5.647898
5.058372	359.897943	5.652902
5.263297	352.101758	5.657907
5.048819	369.621757	5.662912
5.247914	359.558020	5.667917
4.940631	372.865696	5.672922
4.901006	359.476215	5.677926
5.134457	367.899646	5.682931
4.994589	369.247146	5.687936
5.248233	358.494640	5.692941
5.043441	365.854086	5.697946
4.956770	360.428995	5.702950
5.207363	369.491997	5.707955
4.712578	373.018033	5.712960
4.841889	377.832041	5.717965
5.289635	382.944180	5.722970
5.075085	389.466750	5.727974
5.184115	387.709504	5.732979
5.174178	394.642953	5.737984
5.204390	384.051992	5.742989
4.929365	391.333865	5.747994
5.096846	389.222604	5.752998
5.220150	386.127986	5.758003
5.573222	392.694503	5.763008
5.562116	394.467930	5.768013
5.446280	386.956110	5.773018
5.421304	384.545966	5.778022
5.661883	382.571952	5.783027
5.552612	391.495192	5.788032
5.638227	391.149519	5.793037
5.675964	391.431457	5.798042
5.659603	393.003223	5.803046
5.777716	394.076181	5.808051
5.892255	389.657292	5.813056
5.638781	380.828740	5.818061
5.464962	383.231951	5.823066
5.506536	387.195984	5.828070
5.600199	393.891732	5.833075
5.515192	398.422943	5.838080
5.543123	390.037526	5.843085
5.569997	389.552356	5.848090
5.643897	399.994013	5.853094
5.532977	387.150369	5.858099
5.595254	397.913393	5.863104
5.210362	390.114689	5.868109
5.167670	394.427292	5.873114
5.467457	389.944576	5.878118
5.684151	390.318701	5.883123
5.351035	391.231398	5.888128
5.616890	392.480529	5.893133
5.574614	395.960980	5.898138
5.696255	397.264345	5.903142
5.851374	391.598876	5.908147
5.527214	395.594904	5.913152
5.493314	398.178680	5.918157
5.601860	399.104437	5.923162
5.602048	410.854820	5.928166
5.813189	406.911185	5.933171
5.685842	414.492640	5.938176
6.170195	413.024607	5.943181
6.046543	408.288684	5.948186
5.559813	402.986375	5.953190
5.731241	394.268417	5.958195
5.820040	416.477198	5.963200
6.050841	416.491601	5.968205
6.377155	405.661240	5.973210
5.647667	400.605780	5.978214
5.781114	391.577391	5.983219
5.702846	406.197001	5.988224
6.249315	403.690992	5.993229
6.192650	406.382742	5.998234
5.568544	405.452225	6.003238
5.651078	388.557040	6.008243
5.649776	402.430580	6.013248
5.842961	408.474811	6.018253
6.210404	407.085209	6.023258
5.914630	419.223663	6.028262
6.110325	412.321099	6.033267
5.818795	412.759034	6.038272
5.815829	394.396567	6.043277
5.749227	399.181164	6.048282
5.869315	409.375138	6.053286
5.814022	415.537399	6.058291
5.710148	413.237691	6.063296
6.078456	411.401854	6.068301
6.250229	407.995910	6.073306
5.997872	405.074047	6.078310
5.860582	390.978491	6.083315
5.738320	395.031472	6.088320
5.597428	411.923037	6.093325
6.317214	410.930658	6.098330
5.908748	403.784227	6.103334
5.997559	389.333700	6.108339
5.539331	395.584396	6.113344
5.837842	400.295969	6.118349
6.003031	402.557479	6.123354
5.695153	405.054466	6.128358
5.692731	407.671277	6.133363
5.968882	417.679449	6.138368
6.016213	415.916048	6.143373
5.945460	423.431691	6.148378
5.862579	420.495926	6.153382
6.164233	414.209526	6.158387
5.723173	409.048760	6.163392
5.681362	405.173232	6.168397
6.382940	410.818261	6.173402
5.771634	408.066535	6.178406
5.722897	402.831646	6.183411
6.124380	415.844802	6.188416
5.626178	409.490732	6.193421
5.538807	407.178948	6.198426
5.632421	418.902043	6.203430
5.953976	410.518068	6.208435
5.652927	426.352709	6.213440
6.080952	425.488303	6.218445
5.939638	418.369613	6.223450
5.893332	420.914206	6.228454
6.154222	419.025593	6.233459
5.928595	420.275800	6.238464
5.769819	424.084566	6.243469
5.702935	427.505602	6.248474
5.778761	419.100012	6.253478
5.838569	419.590470	6.258483
5.774212	428.240929	6.263488
5.869933	422.464531	6.268493
6.189592	427.087373	6.273498
5.785050	425.590929	6.278502
5.889044	421.265436	6.283507
5.820785	426.151543	6.288512
5.734833	420.359316	6.293517
5.737271	429.752303	6.298522
5.684715	430.013587	6.303526
6.190611	427.665796	6.308531
5.628750	424.580445	6.313536
5.744341	424.056064	6.318541
5.656909	426.366650	6.323546
5.790496	439.127560	6.328550
6.006120	424.074990	6.333555
5.968900	428.155784	6.338560
6.294007	430.025237	6.343565
5.926016	431.054135	6.348570
5.786520	433.796833	6.353574
6.266362	421.642071	6.358579
5.844286	420.717865	6.363584
5.822526	421.518504	6.368589
5.877219	427.739468	6.373594
5.806511	430.667546	6.378598
5.956344	428.290119	6.383603
5.994165	432.906500	6.388608
6.041608	427.488851	6.393613
6.056615	430.384516	6.398618
6.080331	436.214857	6.403622
6.198030	425.689260	6.408627
5.933280	424.844810	6.413632
5.922762	431.654975	6.418637
6.183384	424.302460	6.423642
6.060988	429.266654	6.428646
5.779257	416.535176	6.433651
5.877600	414.298699	6.438656
5.626123	415.189115	6.443661
5.892411	428.641089	6.448666
6.046204	422.200678	6.453670
6.111933	423.705799	6.458675
5.804442	420.286358	6.463680
5.667130	419.516857	6.468685
6.112523	417.770183	6.473690
5.772512	418.544753	6.478694
5.804144	413.471280	6.483699
5.730963	435.483995	6.488704
5.626162	425.613372	6.493709
5.933625	422.274753	6.498714
5.703548	430.925867	6.503718
5.829711	426.612718	6.508723
5.833715	423.660176	6.513728
6.084104	422.848912	6.518733
5.985672	427.233533	6.523738
5.763096	426.240104	6.528742
6.001061	422.210003	6.533747
5.797240	431.053161	6.538752
6.041179	431.571719	6.543757
6.342772	421.979117	6.548762
6.185794	424.335402	6.553766
5.840513	412.939529	6.558771
5.640652	418.146818	6.563776
5.955807	416.350946	6.568781
5.683642	415.124835	6.573786
5.853616	429.455626	6.578790
6.477952	419.473928	6.583795
5.984163	416.716443	6.588800
5.818516	408.987786	6.593805
5.662347	392.800730	6.598810
5.892992	411.551363	6.603814
5.782222	413.830801	6.608819
5.884822	420.436572	6.613824
6.307076	412.261451	6.618829
5.844156	408.186141	6.623834
5.900868	400.299259	6.628838
5.753700	391.390769	6.633843
5.534326	402.846510	6.638848
6.066035	417.860951	6.643853
6.260100	410.148702	6.648858
5.973153	419.201036	6.653862
6.111552	403.056405	6.658867
6.082255	402.004219	6.663872
5.929306	405.087551	6.668877
5.928228	399.658529	6.673882
5.665437	404.964260	6.678886
6.041918	398.137782	6.683891
5.685535	408.732285	6.688896
5.518104	409.713938	6.693901
5.483834	399.541206	6.698906
5.620805	406.603505	6.703910
5.918334	417.563804	6.708915
5.455170	422.546587	6.713920
5.275274	429.389616	6.718925
6.004225	433.419972	6.723930
5.995106	429.719655	6.728934
6.391999	428.562726	6.733939
5.776542	429.399436	6.738944
5.742083	431.173363	6.743949
6.049669	421.162196	6.748954
5.821173	426.437250	6.753958
6.217131	417.722067	6.758963
6.262624	420.277588	6.763968
6.095295	422.980352	6.768973
6.060359	423.995032	6.773978
5.643722	413.907511	6.778982
6.164711	422.725689	6.783987
5.712649	416.000547	6.788992
5.951141	412.631607	6.793997
5.854454	422.309046	6.799002
6.071754	423.616408	6.804006
5.903946	401.998864	6.809011
5.703655	401.853014	6.814016
5.581193	402.666266	6.819021
5.838566	412.952631	6.824026
6.214234	422.321937	6.829030
6.200121	418.325005	6.834035
5.797930	407.627769	6.839040
5.659698	409.342020	6.844045
5.623671	410.609977	6.849050
6.040982	418.533214	6.854054
5.985869	421.765739	6.859059
6.196316	421.137908	6.864064
5.821016	406.791722	6.869069
5.648683	410.719671	6.874074
5.900786	424.477592	6.879078
6.043928	410.844296	6.884083
5.916788	410.085856	6.889088
5.382233	408.306057	6.894093
5.288790	406.571042	6.899098
5.532231	415.369426	6.904102
5.725146	426.238551	6.909107
5.337231	425.982889	6.914112
5.655423	427.752183	6.919117
5.660703	419.677192	6.924122
5.910337	432.587599	6.929126
5.949528	430.607168	6.934131
5.949513	424.981814	6.939136
5.652642	423.889291	6.944141
6.087776	428.519352	6.949146
5.760294	436.372624	6.954150
6.029981	436.172121	6.959155
6.127078	438.143740	6.964160
5.696554	427.979292	6.969165
5.904092	417.743351	6.974170
6.048706	421.305260	6.979174
5.667524	421.722440	6.984179
5.712307	429.125067	6.989184
6.222046	441.374615	6.994189
6.449118	431.493120	6.999194
5.686593	428.878982	7.004198
5.967020	422.624380	7.009203
5.793442	425.185751	7.014208
5.923773	418.533877	7.019213
6.037262	417.715588	7.024218
5.720328	416.686321	7.029222
5.859723	420.616052	7.034227
5.885206	423.769509	7.039232
5.860076	418.239844	7.044237
5.735857	412.709886	7.049242
5.682369	413.335157	7.054246
5.801772	422.111849	7.059251
6.084119	418.229823	7.064256
5.570309	427.450587	7.069261
5.753825	430.123693	7.074266
6.011195	441.058660	7.079270
6.534749	440.248889	7.084275
5.894456	426.482059	7.089280
5.574988	410.595827	7.094285
6.114326	415.279162	7.099290
5.614145	417.167186	7.104294
5.759102	415.543517	7.109299
6.227743	423.433403	7.114304
6.075302	419.072157	7.119309
5.916608	412.218791	7.124314
6.090369	419.832166	7.129318
5.687711	416.066959	7.134323
5.936742	416.685961	7.139328
5.876147	417.385114	7.144333
5.950302	416.819767	7.149338
5.812844	421.270614	7.154342
6.033568	416.800279	7.159347
5.893675	414.123391	7.164352
5.810232	426.453213	7.169357
5.956339	415.673228	7.174362
5.815916	421.127475	7.179366
6.170052	415.500421	7.184371
6.067213	409.416607	7.189376
5.910488	414.050810	7.194381
5.815618	418.811367	7.199386
5.659980	420.629589	7.204390
5.701071	411.849785	7.209395
5.889691	418.024451	7.214400
5.818217	422.699084	7.219405
6.014756	415.179439	7.224410
5.775999	417.409327	7.229414
5.763987	413.067209	7.234419
5.590096	418.612122	7.239424
6.049882	425.358088	7.244429
6.078588	416.494798	7.249434
6.037015	431.852181	7.254438
5.954611	419.393198	7.259443
5.906233	423.937659	7.264448
5.389538	421.576078	7.269453
5.794924	422.711598	7.274458
5.886021	426.183813	7.279462
6.167142	432.682522	7.284467
6.044754	425.418491	7.289472
5.951990	434.108206	7.294477
6.396693	421.743809	7.299482
5.842274	421.340224	7.304486
6.245131	426.035454	7.309491
6.098558	426.434859	7.314496
5.779164	419.397855	7.319501
5.997780	423.644213	7.324506
5.721421	414.306689	7.329510
6.316003	413.912908	7.334515
6.382322	422.378371	7.339520
6.112391	416.254295	7.344525
6.103774	411.335828	7.349530
6.014001	415.757055	7.354534
6.056700	405.259040	7.359539
5.965215	394.035392	7.364544
5.606455	393.531548	7.369549
5.823132	392.440823	7.374554
5.544135	404.450085	7.379558
6.010658	409.290363	7.384563
6.298810	406.653980	7.389568
6.106291	402.106023	7.394573
6.184273	386.815616	7.399578
5.906411	392.054101	7.404582
5.738520	377.030021	7.409587
5.940287	389.476486	7.414592
5.910336	392.303257	7.419597
6.090623	379.581675	7.424602
5.922659	390.839523	7.429606
5.813539	385.750144	7.434611
5.761776	389.994564	7.439616
5.644002	388.500650	7.444621
5.949756	382.368646	7.449626
5.657866	387.596672	7.454630
5.820923	387.267340	7.459635
5.811787	386.813123	7.464640
5.633535	407.722272	7.469645
6.213980	405.821558	7.474650
5.872033	407.039368	7.479654
5.983474	403.032259	7.484659
6.348694	403.304017	7.489664
5.953629	396.563624	7.494669
5.901713	378.405000	7.499674
5.662747	386.408902	7.504678
5.749158	381.042109	7.509683
5.732303	384.885580	7.514688
5.890273	397.516087	7.519693
6.132570	389.748832	7.524698
5.812056	392.023165	7.529702
5.963899	385.839343	7.534707
6.012012	386.796715	7.539712
5.920243	389.639499	7.544717
6.024424	378.084640	7.549722
5.566240	391.960152	7.554726
5.780100	392.863080	7.559731
6.089154	379.915674	7.564736
5.747087	385.230657	7.569741
6.410309	378.033385	7.574746
5.884878	383.070206	7.579750
5.920675	376.736887	7.584755
5.970635	381.927169	7.589760
5.811286	383.882014	7.594765
5.871666	379.588674	7.599770
6.027465	386.916942	7.604774
6.101055	388.768849	7.609779
6.028569	377.469466	7.614784
5.877172	395.229550	7.619789
5.953963	379.537529	7.624794
6.106208	385.404664	7.629798
5.577331	391.979648	7.634803
5.716399	391.207974	7.639808
5.616863	398.443372	7.644813
6.109648	388.681623	7.649818
5.695949	390.502310	7.654822
5.608329	393.189417	7.659827
5.501729	393.984364	7.664832
5.689033	403.221818	7.669837
6.246986	399.170061	7.674842
6.055335	405.527693	7.679846
5.846918	393.139094	7.684851
5.930059	387.456429	7.689856
5.535514	386.534239	7.694861
5.990184	393.442350	7.699866
6.405913	406.674735	7.704870
5.917413	392.697483	7.709875
5.839040	382.458902	7.714880
5.763574	384.403767	7.719885
6.050045	384.273402	7.724890
5.828155	391.546950	7.729894
5.771306	383.681032	7.734899
5.771835	386.180316	7.739904
5.631884	386.834952	7.744909
5.998440	389.574287	7.749914
5.805988	401.389649	7.754918
6.164799	388.981782	7.759923
6.125348	380.385459	7.764928
5.493285	390.441000	7.769933
5.817861	389.728848	7.774938
5.464174	394.716617	7.779942
5.847821	407.409851	7.784947
6.098077	403.865058	7.789952
6.085034	413.368032	7.794957
6.343206	408.774769	7.799962
5.612214	399.226905	7.804966
6.129366	401.790782	7.809971
5.812714	392.912010	7.814976
5.473842	404.478226	7.819981
6.323426	397.988920	7.824986
6.060796	396.543012	7.829990
6.040243	389.573095	7.834995
5.770278	394.443340	7.840000
5.645938	387.657369	7.845005
5.746918	377.147075	7.850010
5.988595	386.689220	7.855014
5.670992	395.138891	7.860019
5.902227	403.069128	7.865024
6.384789	404.113459	7.870029
6.277598	387.238511	7.875034
5.859341	390.888604	7.880038
5.804425	385.369943	7.885043
5.945531	385.021904	7.890048
5.390748	384.491824	7.895053
5.722741	377.514133	7.900058
5.839521	384.253713	7.905062
5.817958	393.871909	7.910067
6.347654	407.127568	7.915072
5.643408	389.507749	7.920077
5.596979	387.154751	7.925082
5.745904	404.377395	7.930086
5.924980	406.930967	7.935091
6.256900	411.026688	7.940096
5.785705	410.217749	7.945101
6.031889	404.531680	7.950106
5.835713	403.227223	7.955110
5.905864	403.387022	7.960115
6.169212	403.010337	7.965120
5.821561	405.352200	7.970125
6.281784	388.609412	7.975142
6.035484	391.961491	7.980160
5.691966	386.091899	7.985178
5.424176	383.915303	7.990195
5.592077	395.072944	7.995213
5.988871	404.481150	8.000230
5.908642	402.010080	8.005248
5.912818	407.673958	8.010266
6.323414	401.872396	8.015283
6.168296	405.147076	8.020301
6.238515	390.490140	8.025318
5.964155	382.858268	8.030336
5.782849	385.938235	8.035354
6.203149	386.159498	8.040371
5.738071	393.468462	8.045389
5.804525	382.280301	8.050406
5.717152	392.174609	8.055424
6.026465	393.404170	8.060442
5.811028	392.301795	8.065459
6.087983	399.052693	8.070477
6.132156	396.098236	8.075494
5.824770	395.537278	8.080512
5.760238	404.626452	8.085530
6.189239	403.473597	8.090547
6.058597	405.024553	8.095565
6.185470	406.560407	8.100582
6.101831	416.466766	8.105600
6.078845	409.780096	8.110618
5.836601	390.914995	8.115635
5.851729	391.341750	8.120653
6.048497	409.731031	8.125670
6.379788	413.592211	8.130688
5.928831	414.243471	8.135706
6.398764	417.562228	8.140723
5.870178	406.142240	8.145741
6.057654	389.904830	8.150758
6.275470	404.024224	8.155776
6.070271	400.821664	8.160794
6.295543	390.839359	8.165811
5.634948	392.769989	8.170829
6.321550	394.637859	8.175846
6.518684	399.473095	8.180864
5.714244	393.117149	8.185882
5.982134	384.232687	8.190899
5.870223	392.556117	8.195917
5.941161	399.541263	8.200934
5.956799	398.734036	8.205952
5.652566	417.514243	8.210970
5.831545	408.223983	8.215987
5.730981	420.566088	8.221005
6.039551	413.666524	8.226022
6.295406	417.952929	8.231040
6.163101	419.194882	8.236058
6.614750	409.719889	8.241075
6.579900	411.801783	8.246093
6.185243	417.386145	8.251110
6.521768	413.985097	8.256128
6.028645	413.058770	8.261146
6.477525	408.478799	8.266163
6.024791	405.630598	8.271181
6.347933	408.480055	8.276198
6.310586	407.434981	8.281216
6.169842	414.014648	8.286234
6.373135	411.874689	8.291251
6.075751	416.099455	8.296269
6.155592	415.108602	8.301286
6.208974	408.053366	8.306304
6.346115	409.357241	8.311322
6.424162	411.310995	8.316339
6.481300	415.764232	8.321357
6.363916	412.380655	8.326374
6.352162	402.463884	8.331392
6.178382	415.492790	8.336410
6.260306	409.480794	8.341427
6.385057	409.278157	8.346445
6.169198	409.659054	8.351462
6.019103	404.810020	8.356480
6.000706	416.299816	8.361498
6.165621	408.640132	8.366515
6.435684	408.660877	8.371533
6.425550	414.522656	8.376550
6.493694	406.792930	8.381568
6.414976	410.061952	8.386586
6.503634	406.396788	8.391603
6.464652	407.766127	8.396621
6.394981	405.763611	8.401638
6.039066	408.018884	8.406656
6.036867	414.251800	8.411674
6.565977	404.998200	8.416691
6.574894	416.139739	8.421709
6.308197	412.628080	8.426726
6.418501	403.708339	8.431744
6.110761	410.907452	8.436762
6.292168	406.167421	8.441779
6.435844	411.923051	8.446797
6.542320	414.506659	8.451814
6.422628	411.038238	8.456832
6.269193	414.363148	8.461850
6.149593	406.009596	8.466867
6.204209	412.299880	8.471885
6.167426	407.136449	8.476902
6.506681	401.481763	8.481920
6.250995	407.789107	8.486938
6.384924	402.267575	8.491955
6.385447	407.114684	8.496973
5.927816	407.864817	8.501990
6.279329	411.457745	8.507008
6.397791	415.071409	8.512026
6.229962	410.856303	8.517043
6.541970	413.322502	8.522061
6.771867	423.580522	8.527078
6.738228	404.862600	8.532096
6.631231	416.180089	8.537114
6.949983	405.372099	8.542131
6.362877	416.534441	8.547149
6.333152	411.997899	8.552166
6.673812	404.815604	8.557184
6.245315	416.107726	8.562202
6.157805	412.170366	8.567219
6.231722	405.503228	8.572237
6.259315	420.536052	8.577255
6.374002	425.504132	8.582272
6.466602	432.971884	8.587290
6.729988	430.320741	8.592307
6.598264	435.529401	8.597325
6.349352	433.845295	8.602343
6.793731	437.840239	8.607360
6.878476	437.940511	8.612378
6.440659	431.328296	8.617395
6.737520	432.673419	8.622413
6.164737	432.715769	8.627431
6.953745	433.220087	8.632448
6.485436	444.849821	8.637466
6.938294	438.300021	8.642483
6.954004	430.083044	8.647501
6.468647	428.155123	8.652519
6.634269	416.519063	8.657536
6.502544	415.103772	8.662554
6.492525	418.813306	8.667571
6.538219	421.791441	8.672589
6.766127	432.182320	8.677607
6.554190	434.762172	8.682624
6.302919	441.002564	8.687642
6.293088	439.419853	8.692659
6.182408	442.930571	8.697677
6.138894	448.235865	8.702695
6.627957	437.871380	8.707712
6.518632	441.022128	8.712730
6.464456	435.381738	8.717747
6.639309	442.041353	8.722765
6.422291	447.089813	8.727783
6.674899	458.941113	8.732800
6.811270	460.503886	8.737818
6.519431	465.816535	8.742835
6.927006	461.574379	8.747853
6.826566	462.981753	8.752871
6.958601	457.615134	8.757888
6.520634	456.430858	8.762906
6.669138	458.730179	8.767923
7.133188	462.706267	8.772941
6.598242	447.333069	8.777959
6.873632	436.273082	8.782976
7.170834	436.939662	8.787994
6.811007	431.201997	8.793011
6.787402	435.156657	8.798029
6.682305	446.732639	8.803047
6.660171	432.358378	8.808064
6.660871	438.988475	8.813082
6.580053	431.925854	8.818099
6.770729	446.901591	8.823117
6.717174	463.313612	8.828135
7.095503	458.580583	8.833152
7.208929	458.591156	8.838170
6.882482	448.281858	8.843187
6.878299	443.949587	8.848205
6.502054	437.712726	8.853223
6.775221	442.211016	8.858240
6.831462	452.518352	8.863258
6.818840	455.448826	8.868275
7.222310	461.340490	8.873293
6.703420	460.014260	8.878311
7.165552	458.638462	8.883328
6.808683	445.916613	8.888346
6.578892	440.180661	8.893363
6.735995	441.096408	8.898381
7.293366	460.164535	8.903399
7.196379	450.819662	8.908416
6.903378	442.430146	8.913434
6.643368	436.654750	8.918451
6.925178	434.767571	8.923469
6.954638	447.562688	8.928487
7.040035	454.264726	8.933504
7.247220	460.799363	8.938522
7.028607	446.597885	8.943539
6.990397	441.295814	8.948557
6.730907	444.097710	8.953575
6.650233	437.173918	8.958592
6.949465	448.737044	8.963610
7.064284	462.418191	8.968627
6.904304	460.025879	8.973645
7.124271	461.297847	8.978663
7.163008	463.873140	8.983680
7.284996	462.787319	8.988698
7.120579	449.394692	8.993715
6.903494	445.815294	8.998733
6.786428	455.259859	9.003751
7.390430	450.734467	9.008768
6.970883	448.821478	9.013786
7.023343	448.740618	9.018803
7.513325	438.467507	9.023821
6.995756	441.123648	9.028839
7.138530	435.862649	9.033856
7.095689	440.249508	9.038874
6.570871	443.727284	9.043891
7.148700	439.190217	9.048909
7.079281	458.053595	9.053927
7.020669	455.942044	9.058944
6.907862	457.294552	9.063962
7.113350	461.023976	9.068979
7.279646	460.650729	9.073997
6.938238	465.516714	9.079015
7.191380	465.615848	9.084032
7.530328	462.716179	9.089050
7.090152	466.587793	9.094067
7.275856	447.270577	9.099085
7.117734	442.874064	9.104103
7.055237	441.268046	9.109120
7.364657	455.963257	9.114138
6.961952	454.562019	9.119155
7.233609	450.113945	9.124173
7.343660	463.499198	9.129191
6.932884	454.089881	9.134208
7.315673	462.023412	9.139226
6.998673	460.384686	9.144243
7.090685	455.996316	9.149261
7.746825	466.869223	9.154279
7.026303	452.942037	9.159296
7.366575	464.489275	9.164314
7.363513	462.403734	9.169331
7.301697	442.765546	9.174349
7.243803	444.989908	9.179367
7.153493	438.531523	9.184384
7.291640	445.089595	9.189402
7.135581	460.501517	9.194419
7.244153	460.175183	9.199437
7.215084	458.601796	9.204455
7.214961	453.416829	9.209472
7.535952	463.777363	9.214490
7.425226	471.011904	9.219507
7.457377	468.166614	9.224525
6.936715	463.546036	9.229543
6.982987	463.873241	9.234560
7.431060	459.416458	9.239578
7.335670	458.844374	9.244595
6.978387	459.771288	9.249613
7.029055	464.982937	9.254631
7.161176	471.197983	9.259648
7.203158	468.139717	9.264666
7.370550	469.419922	9.269683
7.320472	464.772949	9.274701
7.390824	474.639434	9.279719
7.221888	474.132520	9.284736
7.133459	469.895493	9.289754
7.139957	475.830425	9.294771
7.383469	475.744878	9.299789
7.330510	477.501417	9.304807
7.392694	476.563819	9.309824
7.618990	473.511387	9.314842
7.374336	470.788362	9.319859
7.004664	465.506660	9.324877
7.168471	481.436522	9.329895
7.769439	494.094792	9.334912
8.168074	486.366898	9.339930
7.474422	475.540767	9.344947
7.496445	471.794513	9.349965
7.482765	463.591593	9.354983
7.325717	455.764587	9.360000
7.335290	457.044272	9.365018
7.177349	471.730672	9.370035
7.397820	480.970888	9.375053
7.384075	488.925536	9.380071
7.180861	494.145413	9.385088
7.636503	493.357605	9.390106
7.521878	499.627100	9.395123
7.729956	485.996203	9.400141
7.493750	488.175926	9.405159
7.589823	494.683804	9.410176
7.993478	484.181198	9.415194
7.832561	488.151072	9.420211
7.856992	480.443941	9.425229
7.819871	469.543350	9.430247
7.143268	466.720748	9.435264
7.595052	461.253537	9.440282
7.313292	468.846230	9.445299
7.796664	482.479115	9.450317
7.863132	484.513585	9.455335
7.590391	476.632113	9.460352
7.818041	460.400968	9.465370
7.324286	468.424504	9.470387
7.449298	470.266765	9.475405
7.733684	480.112342	9.480423
7.746379	487.756736	9.485440
7.837027	482.462866	9.490458
7.525665	484.720635	9.495475
7.540583	484.071306	9.500493
7.622593	492.635796	9.505511
7.759532	492.847811	9.510528
7.918178	482.131132	9.515546
7.873078	484.410298	9.520563
7.857169	486.220992	9.525581
7.460492	473.401219	9.530599
7.465308	478.853583	9.535616
7.947043	473.962338	9.540634
7.758101	486.113211	9.545651
7.665176	499.202092	9.550669
7.665658	491.738548	9.555687
7.579709	497.927812	9.560704
7.916564	494.728667	9.565722
7.758433	499.322950	9.570739
7.793378	491.532118	9.575757
7.813726	494.769854	9.580775
7.651455	495.890276	9.585792
7.856138	492.898031	9.590810
7.833190	490.834536	9.595827
7.839975	493.632589	9.600845
7.858004	491.035659	9.605863
7.804534	499.157481	9.610880
7.660563	499.366172	9.615898
7.452256	494.684022	9.620915
7.644219	486.786540	9.625933
7.587097	492.807184	9.630951
7.264965	499.936005	9.635968
7.620203	492.666185	9.640986
7.613199	507.654010	9.646003
7.841009	504.566622	9.651021
8.084139	500.116694	9.656039
7.592294	506.883948	9.661056
7.888722	502.261569	9.666074
7.505576	508.112396	9.671091
7.875628	519.724431	9.676109
7.896794	517.051267	9.681127
7.634741	512.582660	9.686144
8.055244	509.843773	9.691162
8.161846	520.938514	9.696179
8.109007	514.332220	9.701197
8.276492	511.367891	9.706215
7.632095	522.987396	9.711232
8.001632	511.480269	9.716250
8.222893	508.457022	9.721267
8.090613	510.715138	9.726285
8.263072	519.385388	9.731303
8.279180	510.802242	9.736320
8.121538	495.612881	9.741338
7.745138	487.757113	9.746355
7.785812	492.014135	9.751373
8.077641	491.889460	9.756391
7.950936	511.632863	9.761408
8.206801	509.068094	9.766426
8.349702	517.231739	9.771443
7.657674	502.088230	9.776461
8.352995	505.340133	9.781479
7.949965	511.635885	9.786496
8.205452	501.490996	9.791514
8.102119	495.435415	9.796531
8.231887	506.785291	9.801549
8.238858	495.745233	9.806567
7.677031	496.944036	9.811584
8.235253	502.991347	9.816602
8.041229	508.635819	9.821619
8.095921	516.914269	9.826637
8.565484	517.351877	9.831655
8.120474	503.532961	9.836672
7.882947	495.529200	9.841690
7.923026	498.198962	9.846707
7.787178	514.005392	9.851725
8.361180	504.946676	9.856743
8.226484	515.028346	9.861760
8.598394	510.532992	9.866778
8.084404	518.846896	9.871795
7.985392	517.183477	9.876813
7.925138	518.142751	9.881831
8.189099	519.474100	9.886848
8.120230	519.497457	9.891866
8.053995	511.690911	9.896883
8.247486	520.824922	9.901901
8.436510	519.233137	9.906919
8.300744	510.724279	9.911936
8.045764	507.068756	9.916954
8.108054	517.886418	9.921971
7.975108	518.484698	9.926989
8.025045	512.550262	9.932007
7.890929	525.961195	9.937024
8.239777	518.436747	9.942042
8.215807	518.844385	9.947059
8.171235	522.205906	9.952077
8.476808	532.632012	9.957095
8.575051	533.093085	9.962112
8.085832	514.089826	9.967130
8.306804	531.090053	9.972147
8.584400	528.446137	9.977165
8.214356	516.638322	9.982183
8.381878	528.771241	9.987200
8.382416	529.102457	9.992218
8.764170	535.480384	9.997235
8.428056	530.392218	10.002253
8.103878	516.393416	10.007271
8.151963	527.200686	10.012288
8.291221	528.119233	10.017306
8.361101	530.809576	10.022323
8.475012	548.445127	10.027341
8.553529	535.998977	10.032359
8.634697	541.332100	10.037376
8.625341	534.523328	10.042394
8.688924	520.318601	10.047411
8.323115	507.519214	10.052429
8.475926	510.180781	10.057447
8.225666	521.659637	10.062464
8.398802	529.405143	10.067482
8.795838	538.554609	10.072499
8.388752	527.743506	10.077517
8.632914	534.480659	10.082535
8.552232	535.051816	10.087552
8.739510	528.190147	10.092570
8.405197	517.364493	10.097587
8.062647	521.517465	10.102605
8.447964	536.368107	10.107623
8.706821	538.504983	10.112640
8.516600	541.456986	10.117658
8.777286	541.646456	10.122675
8.743713	546.303286	10.127693
8.861451	531.493622	10.132711
8.493187	523.816443	10.137728
8.857844	518.441761	10.142746
8.606316	505.955826	10.147763
8.867797	520.582862	10.152781
8.598173	507.531720	10.157799
8.519050	510.968080	10.162816
8.379319	515.947646	10.167834
8.675697	504.161655	10.172851
8.536837	512.312639	10.177869
8.415234	527.621392	10.182887
8.236083	538.353820	10.187904
8.007772	539.273154	10.192922
8.450895	536.600147	10.197939
8.588230	535.808561	10.202957
8.839776	545.088122	10.207975
8.480866	549.477192	10.212992
8.619003	537.466665	10.218010
8.983771	543.623195	10.223027
8.947613	538.062000	10.228045
8.928016	538.058702	10.233063
9.013394	546.297644	10.238080
8.731900	543.308982	10.243098
8.696733	532.348086	10.248115
8.780978	543.493681	10.253133
8.875305	544.946284	10.258151
8.891545	541.014731	10.263168
8.475111	549.966612	10.268186
8.530600	538.698020	10.273203
8.764528	546.244661	10.278221
8.788890	536.965936	10.283239
8.903376	549.176607	10.288256
8.688582	539.515633	10.293274
8.484427	544.050867	10.298291
8.840045	540.511105	10.303309
8.717551	543.070647	10.308327
8.515738	541.426488	10.313344
8.910428	563.603417	10.318362
9.013853	560.753258	10.323379
8.862985	560.650607	10.328397
8.912161	552.819649	10.333415
9.207321	558.002485	10.338432
9.070352	562.157970	10.343450
8.963659	538.244305	10.348467
8.823857	540.585653	10.353485
9.174445	549.672975	10.358503
8.746904	537.454435	10.363520
9.084155	547.784068	10.368538
9.122932	544.297104	10.373555
9.127048	544.738212	10.378573
8.979518	542.448080	10.383591
9.233621	542.982563	10.388608
8.899688	539.301533	10.393626
9.040000	530.847239	10.398643
9.132122	540.770310	10.403661
9.043351	534.011850	10.408679
9.063074	542.986907	10.413696
9.056840	531.645941	10.418714
9.111813	532.309452	10.423731
9.096748	539.270257	10.428749
9.130427	535.935572	10.433767
8.968957	538.229822	10.438784
8.896464	539.945246	10.443802
9.460463	531.882157	10.448819
9.065685	534.276077	10.453837
8.812954	530.392980	10.458855
9.394856	533.965614	10.463872
9.219009	540.651812	10.468890
9.113796	537.925864	10.473907
9.076194	543.160832	10.478925
9.146365	537.576666	10.483943
8.891658	544.057472	10.488960
9.128174	538.519825	10.493978
9.395013	528.328962	10.498995
9.071144	535.719999	10.504013
8.882331	542.695406	10.509031
9.470316	536.238006	10.514048
9.173533	536.899827	10.519066
9.470539	535.186981	10.524083
9.204992	542.830813	10.529101
8.924281	539.772602	10.534119
9.805723	536.226194	10.539136
9.313600	543.754049	10.544154
9.142942	535.575692	10.549171
9.464255	537.819546	10.554189
9.163108	539.302554	10.559207
9.361355	540.208704	10.564224
9.213311	537.877627	10.569242
9.661560	527.948672	10.574259
9.141699	537.314380	10.579277
8.844992	539.105960	10.584295
9.108391	540.923390	10.589312
9.201733	549.476664	10.594330
9.548172	552.543399	10.599347
9.390292	551.933766	10.604365
9.468419	547.105739	10.609383
9.031799	542.146926	10.614400
9.004955	562.408067	10.619418
9.202931	563.001837	10.624435
9.462230	570.882182	10.629453
9.501992	565.211254	10.634471
9.708992	561.221405	10.639488
9.590747	565.326621	10.644506
9.538097	564.113523	10.649523
9.652240	570.385069	10.654541
9.298725	547.311634	10.659559
9.525652	546.849991	10.664576
9.208393	550.210061	10.669594
9.292742	559.440088	10.674611
9.603410	569.082781	10.679629
9.630768	559.371232	10.684647
9.791194	553.858126	10.689664
9.581683	555.853794	10.694682
9.560193	544.890748	10.699699
9.551331	542.010848	10.704717
9.438044	532.352908	10.709735
9.387351	527.652366	10.714752
9.104795	546.019059	10.719770
9.234162	549.624730	10.724787
9.277018	565.548372	10.729805
9.247220	554.318380	10.734823
9.229806	556.148252	10.739840
9.746586	561.744487	10.744858
9.376610	560.265529	10.749875
9.644381	556.973056	10.754893
9.494550	563.557357	10.759911
9.901407	559.053360	10.764928
9.453414	559.527435	10.769946
9.298949	562.344452	10.774963
9.788858	559.067667	10.779981
9.801047	557.894903	10.784999
9.743095	554.890149	10.790016
9.482767	557.436575	10.795034
9.390038	566.072659	10.800051
9.709707	561.134200	10.805069
9.734318	567.388215	10.810087
9.793934	566.671921	10.815104
9.425016	576.541016	10.820122
9.541013	575.045874	10.825139
9.956416	586.149077	10.830157
10.123747	584.349247	10.835175
9.760047	572.669788	10.840192
9.312998	568.050272	10.845210
9.769347	585.307160	10.850227
9.314543	580.382743	10.855245
9.557655	583.453050	10.860263
9.814344	587.366982	10.865280
9.750657	587.711417	10.870298
9.702161	594.002143	10.875315
10.034436	594.199332	10.880333
9.891166	590.226488	10.885351
10.106301	587.705959	10.890368
10.067385	594.926142	10.895386
9.761021	593.377255	10.900403
9.843397	578.983345	10.905421
9.830646	583.453887	10.910439
10.296475	579.401390	10.915456
10.140125	581.284591	10.920474
10.195513	581.973286	10.925491
10.226012	582.006319	10.930509
9.539872	574.091747	10.935527
10.105668	575.047607	10.940544
10.099149	577.096679	10.945562
9.878886	564.694166	10.950579
9.984616	561.720569	10.955597
9.815699	575.061253	10.960615
10.014639	577.576749	10.965632
10.042655	573.384568	10.970650
10.053323	588.931423	10.975667
10.228255	574.709208	10.980685
9.945874	571.140014	10.985703
9.949346	561.116628	10.990720
9.817133	563.024447	10.995738
9.604456	587.379389	11.000755
9.941054	586.408258	11.005773
9.895313	586.336472	11.010791
9.961570	578.322946	11.015808
10.322014	582.662432	11.020826
10.236073	586.270287	11.025843
10.349659	576.560998	11.030861
10.022260	587.376643	11.035879
10.585094	590.624073	11.040896
10.309369	582.077150	11.045914
10.058047	584.776803	11.050931
10.441328	583.189290	11.055949
9.898804	571.840805	11.060967
10.145362	576.141329	11.065984
10.125596	584.384140	11.071002
10.180648	586.814884	11.076019
9.943381	579.353841	11.081037
9.906720	592.964148	11.086055
10.352753	578.282889	11.091072
10.009455	583.496338	11.096090
9.864305	585.633404	11.101107
9.952368	573.971524	11.106125
9.941246	586.511168	11.111143
10.041889	576.829153	11.116160
10.107842	579.255032	11.121178
10.294789	579.897868	11.126195
10.271191	570.800208	11.131213
10.521610	574.860287	11.136231
10.267578	581.053823	11.141248
10.016897	579.051246	11.146266
10.056277	580.982675	11.151283
10.363775	589.489791	11.156301
10.276014	605.071017	11.161319
10.404749	605.454732	11.166336
10.861504	606.090008	11.171354
10.720650	600.702987	11.176371
10.443481	581.792663	11.181389
10.147796	588.589173	11.186407
10.389230	580.059052	11.191424
10.268924	581.873489	11.196442
10.157142	587.795433	11.201459
10.790643	579.645694	11.206477
10.313956	587.496195	11.211495
10.459737	590.117851	11.216512
10.246734	596.317588	11.221530
10.544856	616.524719	11.226547
10.765418	604.646399	11.231565
10.361254	601.231980	11.236583
10.481302	613.861545	11.241600
10.601936	605.015824	11.246618
10.598546	608.074264	11.251635
10.484082	589.655990	11.256653
10.311202	604.723534	11.261671
10.527216	611.559801	11.266688
10.729652	615.845156	11.271706
10.612476	614.389701	11.276723
11.003871	610.042747	11.281741
10.656318	603.463662	11.286759
10.572507	589.774278	11.291776
10.499525	582.208599	11.296794
10.382476	591.612207	11.301811
10.538456	598.625131	11.306829
10.568103	611.262546	11.311847
10.725984	616.612075	11.316864
10.660478	609.906745	11.321882
10.643350	612.232038	11.326899
11.143176	607.293741	11.331917
10.766887	598.989784	11.336935
10.665062	589.484651	11.341952
10.397850	595.967435	11.346970
10.782308	600.363122	11.351987
10.637882	604.257855	11.357005
10.811739	605.650665	11.362023
10.739646	609.341562	11.367040
10.973491	608.298167	11.372058
10.684240	606.926477	11.377075
10.689255	589.540363	11.382093
10.929530	610.684354	11.387111
10.810296	605.224516	11.392128
10.813980	600.973025	11.397146
10.781453	604.818667	11.402163
11.331226	599.146714	11.407181
10.867875	593.999571	11.412199
10.791286	594.503818	11.417216
10.783050	577.548979	11.422234
10.599861	582.888821	11.427251
10.412727	582.867591	11.432269
10.774226	607.965728	11.437287
10.758434	609.968920	11.442304
10.995761	604.311205	11.447322
10.883739	615.415013	11.452339
10.783654	602.857944	11.457357
10.707271	612.138428	11.462375
10.871050	610.181362	11.467392
11.347806	609.068350	11.472410
11.304373	609.936630	11.477427
11.138428	611.347968	11.482445
10.752888	616.201973	11.487463
10.981175	609.176058	11.492480
10.810180	609.360582	11.497498
10.992451	613.374542	11.502515
10.859058	601.611642	11.507533
10.838656	606.209620	11.512551
10.525431	614.747732	11.517568
10.952390	612.787300	11.522586
10.878665	616.109226	11.527603
11.161171	611.132394	11.532621
10.992640	610.877877	11.537639
11.057929	612.495981	11.542656
10.975639	609.226789	11.547674
10.847102	604.636253	11.552691
10.771425	617.204968	11.557709
11.148751	624.754421	11.562727
10.883338	630.842461	11.567744
11.163239	638.984696	11.572762
11.290015	641.363185	11.577779
11.078925	632.623074	11.582797
10.694082	634.800857	11.587815
11.088882	639.030832	11.592832
11.367061	625.183718	11.597850
11.107207	631.908359	11.602867
11.238544	632.859711	11.607885
11.051429	633.441236	11.612903
10.783709	627.474482	11.617920
11.101359	626.578901	11.622938
11.210396	636.227976	11.627955
10.722626	635.042022	11.632973
11.224750	641.322232	11.637991
11.100003	660.137687	11.643008
11.562538	659.901058	11.648026
11.514695	660.826836	11.653043
11.892384	650.770014	11.658061
11.752222	642.927656	11.663079
11.164307	642.211828	11.668096
11.590649	632.513466	11.673114
11.164355	634.672496	11.678131
11.917509	636.832923	11.683149
11.772524	629.874951	11.688167
11.322908	630.380840	11.693184
11.507814	622.285589	11.698202
11.594775	624.796546	11.703219
10.949671	616.648306	11.708237
11.295024	625.313610	11.713255
11.551252	629.085613	11.718272
11.733363	619.100477	11.723290
11.671103	624.497123	11.728307
11.566192	628.644445	11.733325
11.694570	624.187219	11.738343
11.721307	627.256721	11.743360
11.611969	622.947195	11.748378
11.461499	624.608573	11.753395
11.795309	621.315209	11.758413
11.966533	623.273322	11.763431
11.961799	628.165495	11.768448
11.539202	614.595445	11.773466
11.693865	610.355010	11.778483
11.294451	607.479487	11.783501
11.580953	610.325250	11.788519
11.740436	617.388126	11.793536
11.582726	616.005293	11.798554
11.682649	621.442799	11.803571
11.558853	624.037270	11.808589
11.455187	628.686168	11.813607
11.506895	627.333639	11.818624
11.526820	618.169176	11.823642
11.618965	618.646986	11.828659
11.506762	625.623045	11.833677
11.377834	618.394319	11.838695
11.725251	629.132661	11.843712
11.623942	624.578879	11.848730
11.757637	628.294341	11.853747
11.439284	624.860161	11.858765
11.474099	618.183290	11.863783
11.415198	635.028652	11.868800
11.759448	639.705204	11.873818
11.864423	664.742627	11.878835
11.907909	652.267171	11.883853
12.069257	657.736089	11.888871
11.731439	635.742521	11.893888
11.822179	633.045816	11.898906
11.748033	636.143750	11.903923
11.756431	643.407032	11.908941
12.034776	644.190184	11.913959
11.513598	657.671328	11.918976
11.699438	660.103681	11.923994
11.968344	658.821260	11.929011
12.063003	654.056886	11.934029
12.030244	655.160181	11.939047
12.379047	660.565016	11.944064
12.006535	652.607580	11.949082
11.842400	653.602072	11.954099
11.832317	653.805566	11.959117
11.784623	644.175158	11.964135
11.910251	649.491880	11.969152
11.994877	647.484096	11.974170
12.012495	651.908871	11.979187
11.961536	641.114484	11.984205
12.258309	647.142848	11.989223
12.072265	654.341927	11.994240
12.115460	646.508709	11.999258
11.995021	646.022593	12.004275
12.235879	647.622660	12.009293
12.161934	652.027067	12.014311
11.946650	653.594462	12.019328
12.027718	653.146202	12.024346
11.984837	645.430612	12.029363
12.084636	659.022745	12.034381
12.095867	656.133367	12.039399
11.926824	648.992964	12.044416
12.267666	644.672858	12.049434
12.324593	650.833477	12.054451
12.141978	658.227679	12.059469
12.473398	653.732322	12.064487
12.401841	655.283509	12.069504
12.206853	659.214578	12.074522
12.328647	650.829400	12.079539
12.259550	650.666600	12.084557
12.176779	649.000624	12.089575
12.382114	652.834254	12.094592
12.318581	646.885994	12.099610
12.381746	651.256296	12.104627
12.089090	662.461018	12.109645
12.364238	650.618296	12.114663
12.166848	648.881916	12.119680
12.387013	645.921934	12.124698
12.270756	646.688017	12.129715
12.518971	655.374867	12.134733
12.385732	649.715239	12.139751
12.270065	651.222843	12.144768
12.283312	648.361553	12.149786
12.838577	651.162057	12.154803
12.363727	652.337775	12.159821
12.504235	640.077499	12.164839
12.291097	646.542362	12.169856
12.297392	643.265595	12.174874
12.478149	647.317670	12.179891
12.197972	648.737441	12.184909
12.418326	644.117477	12.189927
12.335566	651.404513	12.194944
12.350219	641.884258	12.199962
12.596111	658.637706	12.204979
12.608302	673.275524	12.209997
12.485338	668.434790	12.215015
12.989966	674.417974	12.220032
12.390106	658.048060	12.225050
12.647537	662.621456	12.230067
12.555533	675.789218	12.235085
12.537617	670.499678	12.240103
12.609523	670.425239	12.245120
12.742020	669.056892	12.250138
12.866493	676.687010	12.255155
12.405864	673.354008	12.260173
12.721186	666.648949	12.265191
12.436127	674.198064	12.270208
12.977744	674.804268	12.275226
13.081947	673.178422	12.280243
12.849077	671.021565	12.285261
12.872771	656.242312	12.290279
12.656069	654.234402	12.295296
12.530187	656.084435	12.300314
12.953301	661.180981	12.305331
12.805633	654.886139	12.310349
12.867943	650.922096	12.315367
12.888705	653.762166	12.320384
12.556895	653.728890	12.325402
13.175252	662.632304	12.330419
13.069206	660.285164	12.335437
13.006519	647.513921	12.340455
12.726637	648.984139	12.345472
12.483729	640.618238	12.350490
12.990913	650.678310	12.355507
13.087441	656.495055	12.360525
12.856916	652.854604	12.365543
13.317719	657.800078	12.370560
12.832234	647.332545	12.375578
12.890643	648.819187	12.380595
12.520488	650.038462	12.385613
12.896283	661.510835	12.390631
13.044795	666.580980	12.395648
13.003395	671.289561	12.400666
13.125698	674.924767	12.405683
12.926888	673.674601	12.410701
12.942150	674.476884	12.415719
12.876983	663.675243	12.420736
12.570900	675.232371	12.425754
13.213712	673.692549	12.430771
13.060169	675.086170	12.435789
12.870026	670.609411	12.440807
13.058747	664.075667	12.445824
12.958238	667.966688	12.450842
13.439960	663.343638	12.455859
13.135714	659.471740	12.460877
13.237503	667.376807	12.465895
13.229636	665.711717	12.470912
12.645590	669.643784	12.475930
12.689747	664.587518	12.480947
12.936642	673.564918	12.485965
13.187388	676.122804	12.490983
13.409940	687.840111	12.496000
13.085510	695.698362	12.501018
13.169755	694.880373	12.506035
13.515029	703.072356	12.511053
13.549798	691.787979	12.516071
13.183404	681.847722	12.521088
13.089203	676.327136	12.526106
13.400250	684.799028	12.531123
13.313287	690.234278	12.536141
12.851272	694.159855	12.541159
13.517122	697.410100	12.546176
13.487449	697.042306	12.551194
13.645125	683.999825	12.556211
13.564816	687.237588	12.561229
13.671689	683.692591	12.566247
13.596525	672.368646	12.571264
13.004807	673.692064	12.576282
13.423496	670.117149	12.581299
13.270504	678.314605	12.586317
13.569991	685.330325	12.591335
13.684460	691.598707	12.596352
13.582334	674.999314	12.601370
13.512360	682.786133	12.606387
13.521167	692.438320	12.611405
13.635938	693.827772	12.616423
13.489675	683.225018	12.621440
13.367826	692.181306	12.626458
13.601130	687.950623	12.631475
13.579702	691.182317	12.636493
13.465653	681.120472	12.641511
13.498869	678.284450	12.646528
13.561761	687.902914	12.651546
13.818066	683.192100	12.656563
13.834571	687.490826	12.661581
13.508635	690.025459	12.666599
13.511198	680.324041	12.671616
13.619733	692.261187	12.676634
13.856484	688.616944	12.681651
13.580383	688.505511	12.686669
13.862642	695.571272	12.691687
13.866098	681.303254	12.696704
13.692812	682.860915	12.701722
13.762889	684.093267	12.706739
13.724037	689.688237	12.711757
13.912744	683.826676	12.716775
14.199120	683.728101	12.721792
13.480814	683.695421	12.726810
14.001167	690.076934	12.731827
13.987413	682.019093	12.736845
13.883357	679.753689	12.741863
14.022326	685.746831	12.746880
13.771121	692.047261	12.751898
14.026809	681.731825	12.756915
13.655047	683.595138	12.761933
13.614476	691.986425	12.766951
13.868603	682.441251	12.771968
13.983173	681.454410	12.776986
14.108971	680.238591	12.782003
14.015106	683.020885	12.787021
13.661244	679.216717	12.792039
14.025075	670.597947	12.797056
13.735953	690.329126	12.802074
13.957741	675.793375	12.807091
14.038335	685.484803	12.812109
14.081217	683.619255	12.817127
13.713342	683.051986	12.822144
13.797990	690.618923	12.827162
14.285675	686.042269	12.832179
14.284728	688.702708	12.837197
13.951456	692.229416	12.842215
14.209544	681.175144	12.847232
13.977022	695.415821	12.852250
14.187541	696.152798	12.857267
14.402834	699.094939	12.862285
13.889121	691.008130	12.867303
14.539753	691.789759	12.872320
14.055967	692.663922	12.877338
14.123736	700.435479	12.882355
14.446847	701.666056	12.887373
14.298995	703.216578	12.892391
14.201859	690.955632	12.897408
14.222884	690.917566	12.902426
14.455997	694.765789	12.907443
14.071233	692.711623	12.912461
14.303353	692.773027	12.917479
14.592091	704.407391	12.922496
14.388254	703.593514	12.927514
14.410052	699.872494	12.932531
14.245992	697.935226	12.937549
14.493066	703.352857	12.942567
14.710582	699.070996	12.947584
14.427462	692.478626	12.952602
14.315402	692.114273	12.957619
14.543029	693.684859	12.962637
14.732359	697.476826	12.967655
14.430064	690.338350	12.972672
14.415770	689.346452	12.977690
14.338485	695.512335	12.982707
14.769818	692.942138	12.987725
14.460104	695.512100	12.992743
14.781079	692.896078	12.997760
14.355925	693.615887	13.002778
14.494058	696.794180	13.007795
14.671298	713.227075	13.012813
14.469554	707.369878	13.017831
14.407136	704.533057	13.022848
14.764314	707.086895	13.027866
14.730739	708.752056	13.032883
14.918223	711.749050	13.037901
14.740471	710.053768	13.042919
14.633037	700.865036	13.047936
14.162149	688.763637	13.052954
14.313814	702.063653	13.057971
14.782046	699.424558	13.062989
14.695045	711.345016	13.068007
14.915277	705.693104	13.073024
14.643914	705.719785	13.078042
14.488152	715.609208	13.083059
14.471947	698.563984	13.088077
14.868487	701.039071	13.093095
14.867140	696.163495	13.098112
14.813993	707.267602	13.103130
14.722278	709.169092	13.108147
14.690055	708.129509	13.113165
14.690983	701.697758	13.118183
14.617869	704.864970	13.123200
14.636238	717.832432	13.128218
15.025570	720.406481	13.133235
15.083510	723.259671	13.138253
14.829605	713.800390	13.143271
15.069645	721.320902	13.148288
14.889880	731.343483	13.153306
14.942026	727.620858	13.158323
15.020240	721.129654	13.163341
14.911809	734.022321	13.168359
15.183977	724.729919	13.173376
14.938795	726.888986	13.178394
15.118677	717.308089	13.183411
15.251093	723.160258	13.188429
15.171244	722.913935	13.193447
15.160440	716.222085	13.198464
15.227367	719.910158	13.203482
14.856990	711.946049	13.208499
15.329496	722.986741	13.213517
14.977541	730.110859	13.218535
15.107891	719.363757	13.223552
15.451952	729.348446	13.228570
15.086195	734.581237	13.233587
15.494729	720.978714	13.238605
15.030543	725.176038	13.243623
15.355475	724.904163	13.248640
15.290265	732.137989	13.253658
15.435493	731.812219	13.258675
15.184396	713.317394	13.263693
15.114661	711.008739	13.268711
15.077356	720.775464	13.273728
15.330039	724.166188	13.278746
14.823752	725.157487	13.283763
15.114187	717.370708	13.288781
15.124169	727.237324	13.293799
15.144404	725.148102	13.298816
14.946465	725.570379	13.303834
14.943363	732.968044	13.308851
15.513078	738.300421	13.313869
15.483627	751.594138	13.318887
15.509294	748.468952	13.323904
15.558623	750.379905	13.328922
15.685750	755.696424	13.333939
15.895875	744.829510	13.338957
15.809472	732.686774	13.343975
15.892441	729.723028	13.348992
15.845749	721.717667	13.354010
15.687499	721.622483	13.359027
15.730720	720.362795	13.364045
15.478998	724.700400	13.369063
15.773462	725.313772	13.374080
15.328025	731.120782	13.379098
15.671093	723.855930	13.384115
15.471681	724.874888	13.389133
15.341100	722.228625	13.394151
15.537599	717.669184	13.399168
15.840490	719.379459	13.404186
15.489789	715.871434	13.409203
15.439606	717.627561	13.414221
15.547924	739.833800	13.419239
15.986012	748.762347	13.424256
15.980349	748.245622	13.429274
15.606265	756.026472	13.434291
15.917590	743.007212	13.439309
15.821056	752.407691	13.444327
15.805004	750.229476	13.449344
16.012895	747.678501	13.454362
15.887059	746.012952	13.459379
16.155269	736.090000	13.464397
15.587259	735.074402	13.469415
15.696795	737.960536	13.474432
16.127778	748.490196	13.479450
15.678537	745.019695	13.484467
15.975879	745.433800	13.489485
16.008097	750.152959	13.494503
15.895045	742.366270	13.499520
16.336140	748.703418	13.504538
15.918420	741.813381	13.509555
16.057233	742.993942	13.514573
16.269276	747.312539	13.519591
16.283953	741.377240	13.524608
16.143248	726.065106	13.529626
15.799919	722.559080	13.534643
16.197870	725.636710	13.539661
16.435217	735.982106	13.544679
16.008417	717.760959	13.549696
16.112421	718.887012	13.554714
16.177044	735.091419	13.559731
16.328868	729.055740	13.564749
15.788982	725.646783	13.569767
16.016093	737.653743	13.574784
16.267785	740.252516	13.579802
15.887429	737.067871	13.584819
16.019097	740.143043	13.589837
16.533274	742.006409	13.594855
16.394599	751.486074	13.599872
16.362718	738.649979	13.604890
16.295389	750.548446	13.609907
16.567097	749.019426	13.614925
16.120106	745.106757	13.619943
16.083830	742.770765	13.624960
16.433274	738.998402	13.629978
15.977687	744.371503	13.634995
16.354771	735.116307	13.640013
16.145544	742.726153	13.645031
16.064613	737.162443	13.650048
16.464619	747.886306	13.655066
16.343353	748.621620	13.660083
16.718638	757.711491	13.665101
16.553349	748.396098	13.670119
16.304661	753.503255	13.675136
16.823003	745.971090	13.680154
16.417262	741.408172	13.685171
16.044886	749.832539	13.690189
16.264282	753.550378	13.695207
16.138475	773.410696	13.700224
16.626180	775.862042	13.705242
16.833082	778.922277	13.710259
16.894785	764.635599	13.715277
17.504448	766.591306	13.720295
17.144420	770.406245	13.725312
16.958764	759.935850	13.730330
16.682467	751.871775	13.735347
16.592816	745.368994	13.740365
16.418677	738.153614	13.745383
16.726558	759.381864	13.750400
17.169666	758.062675	13.755418
16.720314	768.698720	13.760435
16.690819	755.366774	13.765453
16.883815	750.334501	13.770471
16.901672	764.113123	13.775488
16.910514	760.659209	13.780506
16.999000	768.888300	13.785523
17.011574	748.780526	13.790541
16.567699	745.899322	13.795559
16.743532	765.150634	13.800576
16.964592	764.901345	13.805594
16.923222	766.981146	13.810611
16.704498	767.725419	13.815629
16.918708	767.710734	13.820647
16.700174	765.295997	13.825664
17.215791	768.771768	13.830682
17.120914	768.660343	13.835699
16.687088	761.069073	13.840717
16.648589	763.391422	13.845735
16.660597	775.832900	13.850752
16.931698	777.226268	13.855770
16.978014	774.479697	13.860787
16.744522	779.114262	13.865805
17.526363	791.905352	13.870823
17.376710	786.368174	13.875840
17.468669	767.134728	13.880858
17.295950	769.045759	13.885875
17.653534	773.149054	13.890893
17.415437	770.320812	13.895911
17.359565	774.264823	13.900928
17.399406	770.790271	13.905946
17.307556	772.745438	13.910963
17.073187	767.805366	13.915981
17.288938	773.685521	13.920999
17.387571	774.228591	13.926016
17.654299	766.634854	13.931034
17.409719	770.147680	13.936051
17.264256	776.958594	13.941069
17.447934	762.356160	13.946087
16.918465	776.359402	13.951104
16.971939	769.982511	13.956122
17.278366	773.816108	13.961139
17.144707	764.928100	13.966157
17.270582	775.316231	13.971175
17.308938	789.555567	13.976192
17.847706	785.415857	13.981210
17.698403	787.297975	13.986227
17.834110	786.143713	13.991245
17.690240	779.725155	13.996263
17.409054	774.170718	14.001280
17.822291	774.039643	14.006298
17.598767	772.840679	14.011315
17.340600	771.685014	14.016333
17.699096	774.178695	14.021351
17.333245	777.240305	14.026368
17.724098	783.623207	14.031386
17.615052	782.355814	14.036403
17.915714	784.684987	14.041421
18.291289	787.643056	14.046439
17.654210	786.480485	14.051456
17.565876	784.181046	14.056474
17.461103	788.258955	14.061491
17.348724	798.359379	14.066509
17.717563	783.585904	14.071527
17.598424	791.819133	14.076544
17.824761	785.932708	14.081562
17.597178	790.500078	14.086579
17.848960	789.930393	14.091597
17.708026	779.563433	14.096615
17.602048	790.325573	14.101632
17.946269	786.961120	14.106650
18.072681	791.147975	14.111667
17.896397	791.424849	14.116685
18.182415	785.002050	14.121703
18.164316	790.549618	14.126720
17.986951	785.083054	14.131738
18.235267	781.402266	14.136755
18.138156	789.603641	14.141773
18.005219	783.757728	14.146791
17.796802	789.956813	14.151808
17.578915	786.033486	14.156826
17.913126	792.216982	14.161843
18.012933	806.014355	14.166861
18.379669	804.426259	14.171879
18.275063	804.322670	14.176896
18.003404	809.846856	14.181914
18.615131	807.043250	14.186931
18.064742	807.741659	14.191949
18.080684	808.894138	14.196967
18.398974	808.026851	14.201984
18.241283	804.457009	14.207002
18.032194	800.888909	14.212019
18.162709	816.956833	14.217037
18.299530	800.966830	14.222055
18.081045	805.715816	14.227072
18.087239	801.574338	14.232090
18.313604	802.258344	14.237107
18.620051	805.842634	14.242125
18.424717	809.597063	14.247143
18.486197	813.708890	14.252160
18.396441	804.208063	14.257178
18.223367	805.759389	14.262195
18.079656	805.646148	14.267213
18.557099	798.495913	14.272231
18.441181	807.552317	14.277248
18.263206	806.724915	14.282266
18.939779	809.083557	14.287283
18.516709	816.089461	14.292301
18.509890	803.779572	14.297319
18.589880	819.811233	14.302336
18.780409	809.032558	14.307354
18.870891	818.186018	14.312371
18.876252	810.368123	14.317389
18.711711	799.553567	14.322407
18.709650	802.946350	14.327424
18.690033	796.782874	14.332442
18.825434	800.302444	14.337459
18.491270	805.170541	14.342477
18.843356	796.124358	14.347495
18.600366	808.422774	14.352512
18.862442	828.941910	14.357530
19.039544	824.502248	14.362547
18.741110	814.970994	14.367565
18.939386	819.260207	14.372583
19.085109	828.209355	14.377600
18.965337	820.395282	14.382618
18.831678	812.144728	14.387635
18.689035	816.948107	14.392653
18.976642	821.668296	14.397671
19.158295	828.642575	14.402688
18.801369	830.093320	14.407706
19.218089	825.780217	14.412723
19.207079	831.042662	14.417741
19.059232	822.743833	14.422759
19.306954	831.579171	14.427776
18.964858	809.567123	14.432794
18.878885	805.534760	14.437811
18.882259	819.214707	14.442829
19.043073	824.696384	14.447847
19.135615	832.937493	14.452864
18.921945	829.764584	14.457882
19.381519	822.238440	14.462899
19.511930	828.687411	14.467917
18.924578	824.231822	14.472935
19.435273	823.246025	14.477952
19.316285	836.304522	14.482970
19.484930	825.270488	14.487987
19.150565	827.759123	14.493005
19.307700	817.304414	14.498023
19.250457	828.049474	14.503040
18.913609	834.435956	14.508058
19.130296	824.984935	14.513075
19.129235	826.591364	14.518093
19.170687	823.100771	14.523111
19.213501	822.869942	14.528128
18.964034	826.535024	14.533146
19.377722	829.998375	14.538163
19.451570	850.193573	14.543181
19.459751	844.641114	14.548199
19.564096	851.075242	14.553216
19.719675	849.289851	14.558234
19.560306	845.868588	14.563251
19.672633	854.289645	14.568269
19.900449	850.580496	14.573287
19.891100	828.582563	14.578304
19.351863	824.494979	14.583322
19.518011	821.660198	14.588339
19.580986	833.468876	14.593357
19.765750	834.007921	14.598375
20.012480	842.480498	14.603392
19.898228	836.448602	14.608410
19.831778	830.557543	14.613427
19.434849	823.746268	14.618445
19.766438	829.409474	14.623463
19.863986	835.759454	14.628480
19.974197	841.788713	14.633498
20.129600	842.919344	14.638515
19.582729	836.787971	14.643533
19.414200	841.002115	14.648551
19.985232	846.078695	14.653568
19.739193	847.587808	14.658586
19.887553	847.845375	14.663603
19.641831	840.385547	14.668621
19.462775	846.204506	14.673639
20.002524	842.039383	14.678656
19.726297	842.161501	14.683674
20.102170	843.462718	14.688691
19.982465	844.276688	14.693709
19.936776	837.255739	14.698727
19.950447	846.370755	14.703744
19.702261	851.960703	14.708762
20.262308	858.705292	14.713779
20.337397	867.659215	14.718797
20.443023	861.700159	14.723815
20.643549	854.227212	14.728832
20.236022	852.577385	14.733850
20.022962	840.703731	14.738867
20.155396	843.321205	14.743885
20.108929	841.062537	14.748903
20.022464	852.547499	14.753920
20.035730	862.685078	14.758938
20.285909	863.617823	14.763955
20.340996	867.266755	14.768973
20.424690	863.283536	14.773991
20.446925	864.245682	14.779008
20.329413	870.717734	14.784026
20.512806	875.069253	14.789043
20.397306	875.806824	14.794061
20.202935	868.228484	14.799079
20.636982	861.113427	14.804096
20.384619	868.215683	14.809114
20.525687	861.260139	14.814131
20.554690	870.271778	14.819149
20.410003	870.183936	14.824167
20.510102	855.831208	14.829184
20.518667	867.036200	14.834202
20.964716	867.120893	14.839219
20.747747	868.619141	14.844237
20.742144	875.247232	14.849255
20.872208	867.217267	14.854272
20.440753	870.254458	14.859290
20.709017	869.641162	14.864307
20.552050	869.107114	14.869325
20.485403	877.502574	14.874343
20.582742	871.661579	14.879360
20.448598	865.661192	14.884378
20.404793	870.474346	14.889395
20.981352	880.744588	14.894413
20.572100	885.965303	14.899431
21.132485	889.260512	14.904448
20.559175	888.769605	14.909466
21.139156	883.648259	14.914483
21.177486	886.188963	14.919501
20.860994	889.899275	14.924519
21.272187	884.466699	14.929536
21.140120	881.151606	14.934554
20.931433	883.396493	14.939571
20.897526	874.824164	14.944589
21.110651	872.928767	14.949607
21.167998	883.813698	14.954624
20.921949	883.416685	14.959642
21.163457	880.320775	14.964659
21.322764	878.563200	14.969677
21.110328	884.886025	14.974695
21.316467	876.661098	14.979712
21.263668	883.858327	14.984730
21.087875	868.403244	14.989747
21.039075	873.160376	14.994765
21.169957	874.821877	14.999783
21.665201	874.614835	15.004800
20.843665	879.448859	15.009818
21.274964	869.282528	15.014835
21.466910	877.687965	15.019853
21.510806	876.150446	15.024871
21.314333	873.628095	15.029888
21.489550	879.801818	15.034906
21.373984	875.755140	15.039923
21.514351	874.262468	15.044941
21.161271	874.636471	15.049959
21.475077	876.976220	15.054976
21.379000	877.335203	15.059994
21.327617	876.573171	15.065011
21.256956	882.523484	15.070029
21.185789	882.218993	15.075047
21.780681	879.765157	15.080064
21.466661	886.649860	15.085082
21.954195	892.888264	15.090099
21.894385	886.112509	15.095117
21.428333	872.422836	15.100135
21.780339	872.096224	15.105152
21.521355	878.975457	15.110170
21.731185	901.623590	15.115187
21.933406	900.594601	15.120205
21.416376	898.030952	15.125223
21.884668	893.170103	15.130240
21.955700	901.689172	15.135258
21.988357	907.026850	15.140275
21.844054	897.193688	15.145293
21.714007	900.095295	15.150311
22.294894	894.664531	15.155328
21.877114	895.563075	15.160346
21.861766	901.807689	15.165363
22.130252	901.607774	15.170381
21.908250	906.117493	15.175399
21.959756	894.915573	15.180416
22.094175	893.351246	15.185434
21.777216	898.847842	15.190451
21.829684	904.314961	15.195469
21.723173	907.376986	15.200487
21.758449	903.202525	15.205504
21.962565	897.527831	15.210522
21.672657	907.694002	15.215539
21.772312	897.863643	15.220557
21.967557	903.305235	15.225575
22.545371	921.976175	15.230592
22.474372	929.883185	15.235610
22.257797	905.585449	15.240627
22.019066	901.021569	15.245645
22.338043	910.334939	15.250663
22.489376	913.198774	15.255680
22.742959	917.160604	15.260698
22.216853	912.228330	15.265715
22.465148	902.614524	15.270733
22.161416	905.805280	15.275751
22.597030	910.524395	15.280768
22.893806	924.915857	15.285786
22.444299	901.427807	15.290803
22.501912	885.065126	15.295821
22.466959	897.820164	15.300839
22.584146	895.027756	15.305856
22.516766	906.598128	15.310874
22.613051	913.980296	15.315891
22.829551	911.964444	15.320909
22.487988	903.190992	15.325927
22.492428	911.745746	15.330944
22.919347	915.904484	15.335962
22.976718	917.123064	15.340979
22.728012	897.245410	15.345997
22.591985	900.349928	15.351015
22.841519	901.083957	15.356032
23.023725	910.806925	15.361050
22.834592	906.639221	15.366067
23.020594	893.169266	15.371085
22.514831	908.245041	15.376103
22.619643	914.814820	15.381120
23.109805	914.308769	15.386138
22.993289	919.212225	15.391155
23.301048	920.189600	15.396173
22.877465	927.773149	15.401191
23.068434	915.908727	15.406208
22.557417	917.342595	15.411226
22.722501	920.702901	15.416243
22.852650	918.489136	15.421261
23.126691	924.281312	15.426279
22.758351	922.041506	15.431296
22.789362	918.704011	15.436314
22.999973	926.756248	15.441331
22.973344	920.297178	15.446349
22.783234	916.801821	15.451367
22.909672	938.680416	15.456384
23.004753	937.784978	15.461402
23.173881	945.666995	15.466419
23.581649	939.616392	15.471437
23.241376	948.562849	15.476455
23.472992	937.474697	15.481472
23.448848	936.304445	15.486490
23.339845	934.090277	15.491507
23.643459	932.884452	15.496525
23.516236	939.326491	15.501543
23.436904	940.389763	15.506560
23.572458	934.419682	15.511578
23.416815	941.064994	15.516595
23.804161	938.672071	15.521613
23.581299	935.920312	15.526631
23.477335	937.732225	15.531648
23.818222	934.219942	15.536666
23.471417	927.804722	15.541683
23.535547	918.286035	15.546701
23.755305	928.990911	15.551719
23.676317	937.700763	15.556736
23.561634	933.593973	15.561754
23.553523	940.538066	15.566771
23.775607	935.049896	15.571789
23.853557	939.137081	15.576807
23.509208	930.376676	15.581824
23.581448	936.266746	15.586842
23.307816	937.600306	15.591859
23.898433	933.663881	15.596877
23.500803	937.853981	15.601895
23.508017	937.016493	15.606912
23.573504	932.688967	15.611930
23.891741	947.547307	15.616947
23.702168	956.227156	15.621965
23.777439	957.764832	15.626983
23.783419	957.899540	15.632000
24.222202	952.440530	15.637018
24.353501	962.676439	15.642035
24.315989	949.557047	15.647053
24.291304	951.179812	15.652071
24.164366	955.980767	15.657088
24.192589	954.158514	15.662106
24.074937	958.554065	15.667123
24.002810	953.970380	15.672141
24.227697	958.905564	15.677159
24.034555	953.349900	15.682176
24.132176	951.863918	15.687194
23.896795	956.839657	15.692211
24.226277	942.583466	15.697229
24.074947	954.280632	15.702247
24.450924	957.102965	15.707264
24.303581	951.205605	15.712282
24.395563	950.954447	15.717299
24.630449	952.135749	15.722317
24.114101	949.262711	15.727335
24.174187	949.325824	15.732352
24.627175	966.754026	15.737370
24.682110	968.358006	15.742387
24.503096	952.925446	15.747405
24.680986	959.527974	15.752423
24.187341	968.738317	15.757440
24.913636	965.948296	15.762458
24.490380	984.413224	15.767475
24.889990	977.158347	15.772493
25.039781	978.835830	15.777511
24.941328	966.846304	15.782528
25.000605	957.202123	15.787546
24.552447	950.667073	15.792563
24.710746	947.297006	15.797581
24.727860	954.868323	15.802599
24.864596	954.446049	15.807616
24.915938	958.319653	15.812634
25.011867	963.637966	15.817651
24.694921	963.327800	15.822669
24.755067	969.257647	15.827687
24.806715	978.291039	15.832704
25.231765	977.861461	15.837722
25.200716	974.899759	15.842739
24.970943	981.477804	15.847757
25.046603	977.751443	15.852775
25.009069	978.997520	15.857792
25.395392	969.251597	15.862810
25.098358	975.922231	15.867827
24.912047	970.592713	15.872845
25.312697	970.877027	15.877863
25.258257	975.373133	15.882880
25.293109	975.894644	15.887898
25.056910	981.006220	15.892915
25.560309	973.059728	15.897933
25.519931	965.245776	15.902951
25.310060	960.017785	15.907968
25.416176	965.479672	15.912986
25.090193	971.274355	15.918003
25.486853	967.784886	15.923021
25.688618	977.934023	15.928039
25.207571	974.765110	15.933056
25.413828	966.953541	15.938074
25.131273	975.868878	15.943091
25.313769	970.055535	15.948109
25.424025	975.358984	15.953127
25.018251	976.596483	15.958144
25.127297	970.643167	15.963162
25.440350	972.364498	15.968179
25.856583	979.100107	15.973197
25.737656	974.075617	15.978215
25.091596	978.427729	15.983232
25.810265	988.331779	15.988250
25.969177	1001.690846	15.993267
25.697977	999.221211	15.998285
25.753779	988.192132	16.003303
25.708554	988.789307	16.008320
25.952979	990.344665	16.013338
25.749675	993.781639	16.018355
26.345527	994.354112	16.023373
26.295645	991.654139	16.028391
26.084062	982.797165	16.033408
25.814935	967.631179	16.038426
25.935785	973.333762	16.043443
25.589394	988.097451	16.048461
26.051838	988.542500	16.053479
25.843218	990.216178	16.058496
26.095263	993.843745	16.063514
26.051895	986.238539	16.068531
26.296839	985.688855	16.073549
26.234843	992.900192	16.078567
26.055343	995.320404	16.083584
26.037563	987.405070	16.088602
26.008007	984.449444	16.093619
26.149469	989.321966	16.098637
26.361420	981.664136	16.103655
26.169232	984.881612	16.108672
26.581872	983.418856	16.113690
26.399400	987.508983	16.118707
26.131363	992.818059	16.123725
26.275022	989.235679	16.128743
26.068981	989.810712	16.133760
26.167653	994.775149	16.138778
26.138147	1007.532568	16.143795
26.034543	1009.050936	16.148813
26.551867	997.409888	16.153831
26.605259	1007.017389	16.158848
26.432891	1008.423452	16.163866
26.505522	1003.488863	16.168883
26.550330	1008.035701	16.173901
26.852432	999.820929	16.178919
26.555012	1005.548030	16.183936
26.555584	997.475178	16.188954
26.681191	1000.933205	16.193971
26.508689	996.194818	16.198989
26.753477	999.804588	16.204007
26.910405	1020.766462	16.209024
27.303755	1013.004456	16.214042
27.084597	1008.822497	16.219059
26.695430	995.003916	16.224077
26.471446	999.832711	16.229095
26.904365	1020.221157	16.234112
26.961203	1019.303304	16.239130
27.396101	1016.713569	16.244147
27.093229	1030.564739	16.249165
27.494952	1024.865356	16.254183
27.052381	1007.571052	16.259200
27.161505	1005.524676	16.264218
27.035267	996.098891	16.269235
27.102821	1006.234358	16.274253
27.243668	1013.407611	16.279271
27.203385	1021.218328	16.284288
27.326411	1024.922921	16.289306
27.309659	1030.126363	16.294323
27.008172	1033.727053	16.299341
27.146180	1023.496132	16.304359
27.121875	1033.759618	16.309376
27.443168	1022.856183	16.314394
27.443562	1031.597825	16.319411
27.334698	1025.252589	16.324429
27.307912	1013.122413	16.329447
27.186263	1029.141672	16.334464
27.742512	1013.391884	16.339482
27.807120	1020.659137	16.344499
27.641976	1020.438796	16.349517
27.403515	1018.099731	16.354535
27.458135	1020.334939	16.359552
27.435537	1018.208211	16.364570
27.752368	1016.230278	16.369587
27.326970	1019.945055	16.374605
27.772113	1019.521797	16.379623
27.648754	1029.128600	16.384640
27.929604	1035.850727	16.389658
28.095578	1033.378865	16.394675
27.640294	1035.523549	16.399693
27.910349	1030.494903	16.404711
28.017611	1044.995052	16.409728
27.862641	1038.960000	16.414746
28.255131	1034.631709	16.419763
28.069870	1027.411642	16.424781
28.218494	1016.895033	16.429799
27.753186	1021.988867	16.434816
28.159464	1024.708632	16.439834
28.373692	1024.469878	16.444851
27.789642	1021.263445	16.449869
27.973359	1023.913937	16.454887
28.358736	1033.598828	16.459904
28.124478	1042.301499	16.464922
28.191179	1042.603423	16.469939
28.348473	1045.523151	16.474957
28.247319	1042.566110	16.479975
28.028169	1047.125911	16.484992
28.068707	1038.415605	16.490010
28.729603	1031.804592	16.495027
28.358697	1049.851122	16.500045
28.489165	1044.443547	16.505063
28.246027	1045.898571	16.510080
28.120511	1041.225396	16.515098
28.763944	1046.461109	16.520115
28.815672	1045.932228	16.525133
28.925100	1043.920514	16.530151
28.755037	1034.514199	16.535168
28.421530	1037.176301	16.540186
28.307976	1035.723399	16.545203
28.296708	1039.789871	16.550221
28.456551	1041.459473	16.555239
28.382449	1033.341499	16.560256
28.283814	1040.306126	16.565274
28.714170	1040.822478	16.570291
28.717106	1055.806051	16.575309
28.647108	1055.722285	16.580327
28.832875	1061.540960	16.585344
29.054764	1069.493663	16.590362
29.363215	1059.273887	16.595379
28.817831	1070.417472	16.600397
29.331928	1047.292661	16.605415
29.203950	1049.253518	16.610432
29.239581	1046.293980	16.615450
29.410093	1033.252389	16.620467
28.817902	1031.789271	16.625485
29.019140	1027.396270	16.630503
29.285773	1039.046941	16.635520
28.759387	1028.437264	16.640538
29.074516	1032.219061	16.645555
29.203058	1050.540797	16.650573
29.233780	1061.461567	16.655591
29.431916	1043.183198	16.660608
29.284088	1054.065666	16.665626
29.617745	1051.996728	16.670643
29.379145	1049.717642	16.675661
29.227916	1051.372866	16.680679
29.286006	1050.943976	16.685696
29.331939	1056.661480	16.690714
29.327231	1051.028923	16.695731
28.976574	1062.129371	16.700749
29.661982	1068.696605	16.705767
29.748335	1044.442738	16.710784
29.502747	1054.643074	16.715802
29.524239	1043.628805	16.720819
29.360006	1048.423004	16.725837
29.438290	1043.727365	16.730855
29.559788	1055.618542	16.735872
29.822748	1071.195719	16.740890
29.900101	1066.866301	16.745907
29.555402	1079.512206	16.750925
29.659983	1083.134493	16.755943
30.090938	1065.147835	16.760960
29.663846	1077.582581	16.765978
29.998057	1081.459230	16.770995
29.725829	1080.820155	16.776013
29.766841	1078.001783	16.781031
29.810005	1078.143290	16.786048
30.488272	1075.275569	16.791066
30.468870	1070.604695	16.796083
30.197684	1073.222324	16.801101
30.077104	1070.643871	16.806119
29.797607	1074.070706	16.811136
29.887663	1077.461733	16.816154
30.108834	1075.097984	16.821171
29.701377	1074.764126	16.826189
30.227815	1070.989210	16.831207
30.417053	1064.313225	16.836224
30.164027	1077.632747	16.841242
30.532348	1082.324580	16.846259
30.578670	1091.327306	16.851277
30.204334	1078.181694	16.856295
30.359398	1078.299357	16.861312
30.421181	1092.926594	16.866330
30.701959	1089.969666	16.871347
30.843416	1096.783087	16.876365
30.459806	1077.819482	16.881383
30.672335	1073.718198	16.886400
30.357532	1085.772430	16.891418
30.891511	1088.506912	16.896435
30.888821	1089.523470	16.901453
30.901682	1076.108907	16.906471
30.774357	1069.921186	16.911488
30.716180	1066.925848	16.916506
30.538932	1064.832812	16.921523
30.816961	1078.914905	16.926541
30.493752	1087.050853	16.931559
30.594271	1088.751846	16.936576
30.612309	1101.959486	16.941594
30.633143	1094.612425	16.946611
30.737767	1100.500632	16.951629
30.689472	1092.489044	16.956647
30.978830	1088.615567	16.961664
31.259432	1094.346809	16.966682
31.204600	1092.995158	16.971699
31.475589	1089.954555	16.976717
31.634812	1089.449857	16.981735
31.473872	1085.302941	16.986752
31.632838	1091.296243	16.991770
31.203720	1081.488668	16.996787
31.134778	1088.480220	17.001805
31.307475	1087.957632	17.006823
31.206548	1079.626084	17.011840
31.244361	1087.052200	17.016858
31.382288	1083.615870	17.021875
31.175029	1085.759570	17.026893
31.091543	1090.850406	17.031911
31.490148	1100.167179	17.036928
31.916470	1109.407029	17.041946
31.640306	1098.682364	17.046963
31.645041	1099.382171	17.051981
31.691157	1094.262359	17.056999
31.731637	1082.462431	17.062016
31.512856	1100.384190	17.067034
31.855962	1105.714313	17.072051
32.071579	1117.881126	17.077069
31.704303	1103.434165	17.082087
32.093431	1093.877088	17.087104
31.657823	1095.763069	17.092122
32.001364	1097.444922	17.097139
32.213424	1105.184581	17.102157
31.933926	1088.943960	17.107175
31.774693	1078.175740	17.112192
31.645824	1089.181494	17.117210
32.152815	1099.304969	17.122227
31.939284	1108.222181	17.127245
31.558133	1104.854551	17.132263
32.324105	1103.986539	17.137280
32.045650	1104.680222	17.142298
32.323023	1103.194467	17.147315
32.334163	1099.632828	17.152333
32.134267	1103.934001	17.157351
32.411584	1099.355489	17.162368
32.222655	1104.377641	17.167386
32.404602	1103.951435	17.172403
32.218826	1101.171749	17.177421
32.340413	1095.150152	17.182439
32.363753	1099.249086	17.187456
32.302086	1108.148815	17.192474
32.414210	1100.961022	17.197491
32.256218	1104.810650	17.202509
32.140860	1098.624200	17.207527
32.434304	1117.573436	17.212544
32.539917	1127.043429	17.217562
32.354543	1120.681744	17.222579
32.738328	1118.819544	17.227597
32.540844	1122.145175	17.232615
32.634296	1122.379791	17.237632
32.472292	1131.901183	17.242650
32.805632	1120.430896	17.247667
32.595549	1120.100828	17.252685
32.810961	1122.206712	17.257703
32.887958	1121.582349	17.262720
32.906042	1124.224092	17.267738
32.876100	1125.670966	17.272755
33.120296	1126.636221	17.277773
32.965607	1142.686007	17.282791
33.473302	1144.783970	17.287808
32.991920	1137.758581	17.292826
32.781765	1126.670098	17.297843
33.057968	1146.546741	17.302861
32.816641	1148.216091	17.307879
33.230579	1143.332133	17.312896
33.086395	1144.355083	17.317914
33.094020	1151.672344	17.322931
33.577968	1141.207269	17.327949
33.044643	1145.734266	17.332967
33.153805	1132.503393	17.337984
33.351126	1146.001722	17.343002
33.532842	1144.328974	17.348019
33.571434	1138.869492	17.353037
33.405292	1142.985499	17.358055
33.753535	1137.193472	17.363072
33.299795	1137.933554	17.368090
33.568531	1156.290240	17.373107
33.879152	1148.585320	17.378125
34.168491	1153.093882	17.383143
33.860984	1141.354750	17.388160
33.769108	1146.125015	17.393178
33.700686	1136.046296	17.398195
34.104537	1136.377451	17.403213
33.907475	1138.854083	17.408231
34.149012	1133.170296	17.413248
33.900806	1143.680371	17.418266
34.058732	1141.070895	17.423283
34.236717	1140.664245	17.428301
33.851229	1135.915009	17.433319
34.194008	1136.350409	17.438336
34.063789	1134.663418	17.443354
34.018965	1135.737074	17.448371
33.688725	1135.908682	17.453389
34.104629	1154.239152	17.458407
34.075955	1158.279975	17.463424
34.381652	1161.492060	17.468442
34.521470	1155.559108	17.473459
34.778430	1151.731719	17.478477
34.396185	1168.921743	17.483495
34.446733	1162.422091	17.488512
34.609920	1165.748026	17.493530
34.564753	1164.303334	17.498547
34.651529	1156.305269	17.503565
34.430511	1158.176571	17.508583
34.575540	1146.309726	17.513600
34.665914	1158.259498	17.518618
34.497106	1162.577905	17.523635
34.958940	1149.752524	17.528653
34.521131	1148.760682	17.533671
34.608607	1153.042089	17.538688
35.070910	1152.530930	17.543706
34.828558	1151.757780	17.548723
34.731904	1144.921425	17.553741
34.492572	1153.498709	17.558759
34.502963	1151.221626	17.563776
34.595122	1146.564812	17.568794
34.133077	1156.429881	17.573811
34.611795	1154.505466	17.578829
34.481977	1180.441960	17.583847
34.848316	1167.956586	17.588864
34.976192	1173.512961	17.593882
34.704016	1181.732477	17.598899
34.994250	1173.768801	17.603917
35.034267	1181.702711	17.608935
34.877381	1186.328533	17.613952
35.186131	1196.902859	17.618970
35.360508	1197.086927	17.623987
35.487692	1198.256717	17.629005
35.242999	1201.949531	17.634023
35.703232	1206.223042	17.639040
35.652905	1207.830913	17.644058
35.801724	1214.674783	17.649075
35.989980	1199.285455	17.654093
35.248203	1182.549115	17.659111
35.724225	1189.228099	17.664128
36.078735	1192.284215	17.669146
35.821470	1180.082735	17.674163
35.684326	1168.733470	17.679181
35.569137	1169.471005	17.684199
35.395155	1162.119724	17.689216
35.922001	1182.354781	17.694234
36.202804	1191.333443	17.699251
35.992361	1184.445471	17.704269
36.033839	1179.414726	17.709287
35.932729	1166.314606	17.714304
36.133034	1174.277049	17.719322
35.897208	1174.342344	17.724339
36.113671	1166.873081	17.729357
36.307944	1180.274081	17.734375
36.177570	1189.153056	17.739392
36.148630	1178.121358	17.744410
35.978729	1197.231640	17.749427
36.400417	1190.967327	17.754445
36.384755	1191.212728	17.759463
36.384917	1192.295119	17.764480
36.518780	1197.206760	17.769498
36.322468	1190.698436	17.774515
36.230931	1185.382407	17.779533
36.339012	1179.233507	17.784551
36.060348	1185.891872	17.789568
36.466367	1178.904161	17.794586
36.348949	1186.237872	17.799603
36.433363	1184.034395	17.804621
36.501605	1184.465472	17.809639
36.412445	1187.647906	17.814656
36.208137	1179.392471	17.819674
36.723879	1202.390701	17.824691
36.517176	1207.257871	17.829709
36.606913	1213.858526	17.834727
36.965105	1209.339902	17.839744
36.967682	1207.303884	17.844762
36.967901	1207.417404	17.849779
37.213228	1207.413625	17.854797
36.884712	1213.316083	17.859815
36.629969	1212.099888	17.864832
36.924432	1207.225165	17.869850
36.756097	1206.317335	17.874867
37.020384	1207.077469	17.879885
36.810927	1206.125587	17.884903
36.524752	1205.362456	17.889920
36.980380	1219.492577	17.894938
36.727131	1220.630453	17.899955
37.369296	1224.398922	17.904973
37.326533	1235.883596	17.909991
37.342088	1234.820717	17.915008
37.489416	1232.468518	17.920026
37.078350	1237.184672	17.925043
37.566563	1232.528902	17.930061
37.105225	1230.492980	17.935079
37.439728	1234.240226	17.940096
37.656877	1227.111669	17.945114
37.377954	1239.412854	17.950131
37.808947	1241.904712	17.955149
37.795185	1247.751554	17.960167
37.625818	1257.883257	17.965184
37.989571	1262.765210	17.970202
37.668174	1268.534022	17.975219
37.694536	1265.522250	17.980237
37.867633	1258.012405	17.985255
37.884228	1249.526661	17.990272
38.058730	1254.170010	17.995290
38.220329	1261.321176	18.000307
38.365874	1244.366857	18.005325
38.284610	1245.007557	18.010343
38.126743	1248.809858	18.015360
38.284476	1247.661584	18.020378
38.031472	1247.237248	18.025395
38.413407	1249.313901	18.030413
38.120473	1246.674061	18.035431
38.020776	1243.142382	18.040448
38.659027	1244.702334	18.045466
38.224501	1249.311710	18.050483
38.477538	1240.728963	18.055501
38.280455	1237.682774	18.060519
37.935429	1244.540912	18.065536
38.232482	1233.849436	18.070554
37.957918	1234.438369	18.075571
38.169329	1262.085670	18.080589
38.555581	1268.352701	18.085607
38.476666	1271.561948	18.090624
39.003656	1262.245123	18.095642
38.805892	1271.245155	18.100659
38.920842	1268.033303	18.105677
38.973116	1263.212289	18.110695
38.919077	1270.744395	18.115712
39.037953	1264.808376	18.120730
38.817564	1266.480767	18.125747
38.916534	1267.654983	18.130765
38.818250	1268.563448	18.135783
38.700125	1264.911572	18.140800
38.931620	1266.285937	18.145818
39.087919	1266.510709	18.150835
39.074066	1267.197655	18.155853
39.320923	1282.947960	18.160871
39.342022	1288.325434	18.165888
39.448060	1288.188838	18.170906
39.607177	1280.214099	18.175923
39.481276	1272.877331	18.180941
39.499152	1264.179933	18.185959
39.253625	1276.157164	18.190976
39.889062	1267.110534	18.195994
39.444611	1274.034755	18.201011
39.653808	1271.275212	18.206029
39.533698	1262.186010	18.211047
39.472985	1273.234848	18.216064
39.533090	1273.484159	18.221082
39.819246	1287.369477	18.226099
39.730187	1289.065477	18.231117
39.791920	1283.065819	18.236135
39.826530	1299.253349	18.241152
40.203536	1277.850760	18.246170
39.960525	1289.496235	18.251187
39.715589	1284.046415	18.256205
39.993894	1287.130267	18.261223
39.993399	1291.665340	18.266240
40.174900	1273.764896	18.271258
39.877200	1283.216107	18.276275
39.953037	1276.153854	18.281293
40.137095	1278.573949	18.286311
39.668479	1290.226368	18.291328
40.177470	1283.784237	18.296346
40.241940	1279.150663	18.301363
40.109445	1274.740460	18.306381
39.989824	1291.390820	18.311399
39.645853	1303.187827	18.316416
40.376625	1299.898420	18.321434
40.448806	1303.355409	18.326451
40.450929	1305.005565	18.331469
40.414106	1304.395873	18.336487
40.377922	1311.057320	18.341504
40.463177	1307.389349	18.346522
40.341869	1311.381602	18.351539
40.478700	1326.820968	18.356557
40.944436	1322.679956	18.361575
40.947147	1331.916862	18.366592
40.811106	1324.764705	18.371610
40.973730	1330.725955	18.376627
40.817331	1326.458346	18.381645
41.138873	1321.942280	18.386663
40.952470	1330.874287	18.391680
41.047263	1326.299069	18.396698
41.273397	1323.865080	18.401715
41.163436	1329.957403	18.406733
41.153214	1323.596607	18.411751
41.091754	1339.770822	18.416768
41.425678	1322.461854	18.421786
41.705901	1315.730494	18.426803
41.214175	1321.655402	18.431821
41.351350	1314.820218	18.436839
41.304576	1327.056687	18.441856
41.338594	1318.994230	18.446874
41.348943	1327.702898	18.451891
41.228097	1328.848439	18.456909
41.762058	1332.536052	18.461927
41.904598	1350.666548	18.466944
41.727809	1337.161578	18.471962
41.770681	1339.389198	18.476979
41.572717	1339.167684	18.481997
41.734472	1337.248728	18.487015
42.059321	1350.701983	18.492032
41.704097	1349.943352	18.497050
41.993702	1344.327710	18.502067
41.901842	1348.201743	18.507085
42.354734	1338.975386	18.512103
42.275454	1346.116988	18.517120
42.282937	1355.428900	18.522138
42.337134	1345.482336	18.527155
42.090935	1343.191779	18.532173
42.342612	1330.074136	18.537191
42.123925	1340.301979	18.542208
41.996773	1338.027486	18.547226
42.404354	1337.133562	18.552243
42.526086	1341.949310	18.557261
42.331029	1341.894604	18.562279
42.392294	1342.819102	18.567296
42.512541	1340.344895	18.572314
42.206507	1335.037181	18.577331
42.580462	1347.532807	18.582349
42.694736	1342.257072	18.587367
42.237060	1340.138509	18.592384
42.099566	1345.509289	18.597402
41.892801	1349.208814	18.602419
43.022398	1363.501708	18.607437
42.695564	1357.256779	18.612455
42.922536	1364.909005	18.617472
43.103062	1371.833179	18.622490
43.161113	1367.216367	18.627507
42.770569	1364.421382	18.632525
42.642684	1361.045581	18.637543
42.819063	1368.570030	18.642560
42.876436	1371.079417	18.647578
42.834582	1358.941898	18.652595
43.205346	1374.830667	18.657613
43.363796	1371.189087	18.662631
42.949353	1383.700960	18.667648
43.020291	1382.165473	18.672666
43.454167	1376.350485	18.677683
43.298779	1391.857782	18.682701
43.109706	1384.751782	18.687719
43.311616	1383.533459	18.692736
43.440174	1385.173281	18.697754
43.873150	1381.160470	18.702771
43.824938	1381.524587	18.707789
43.673031	1381.305323	18.712807
43.628465	1372.882753	18.717824
43.486538	1379.421932	18.722842
44.209109	1371.832263	18.727859
43.813358	1379.660959	18.732877
43.750563	1376.701008	18.737895
43.687158	1376.673013	18.742912
43.851174	1399.092262	18.747930
44.135230	1404.365453	18.752947
43.946291	1401.904964	18.757965
44.382112	1400.113483	18.762983
44.140338	1401.792393	18.768000
44.066584	1386.765860	18.773018
44.695649	1392.631959	18.778035
44.119326	1393.747877	18.783053
44.360129	1393.833173	18.788071
44.409801	1392.509309	18.793088
44.324088	1393.276949	18.798106
44.749997	1393.569939	18.803123
44.792543	1401.582448	18.808141
44.551782	1400.594433	18.813159
44.369375	1395.541898	18.818176
44.167539	1396.002671	18.823194
44.644245	1388.962777	18.828211
44.415896	1389.440328	18.833229
44.351713	1395.456071	18.838247
44.637499	1410.525019	18.843264
44.573970	1418.866593	18.848282
45.160816	1420.895383	18.853299
45.079095	1426.077560	18.858317
44.841832	1420.658055	18.863335
44.815659	1422.470452	18.868352
44.773840	1423.300648	18.873370
45.193243	1419.507715	18.878387
44.632602	1425.594939	18.883405
44.739655	1422.579966	18.888423
44.916495	1434.314395	18.893440
45.028143	1438.996044	18.898458
45.094969	1437.991395	18.903475
45.280029	1440.767976	18.908493
45.544784	1444.037023	18.913511
45.764202	1451.412747	18.918528
45.724425	1441.745952	18.923546
45.937578	1442.201670	18.928563
45.742943	1446.640961	18.933581
45.801854	1443.725050	18.938599
45.780357	1427.210157	18.943616
45.269597	1439.333199	18.948634
45.783542	1434.127368	18.953651
45.731913	1438.973460	18.958669
45.503009	1434.360563	18.963687
45.900719	1426.291570	18.968704
45.408987	1435.842693	18.973722
45.959357	1443.071882	18.978739
46.137968	1463.450185	18.983757
46.163180	1465.305031	18.988775
46.255807	1469.342699	18.993792
46.253966	1463.744279	18.998810
46.550679	1458.888070	19.003827
46.300196	1457.033690	19.008845
46.388274	1463.113966	19.013863
46.578462	1461.408303	19.018880
46.361082	1467.732108	19.023898
46.846377	1458.273385	19.028915
46.607426	1456.010081	19.033933
46.400294	1464.494102	19.038951
46.518825	1463.961055	19.043968
46.679991	1468.360386	19.048986
46.741906	1465.421908	19.054003
46.794839	1464.845487	19.059021
46.846710	1465.963976	19.064039
46.636461	1462.512694	19.069056
46.469851	1465.618945	19.074074
46.453123	1465.214392	19.079091
46.410398	1476.191106	19.084109
46.636264	1478.797191	19.089127
46.800505	1484.098646	19.094144
46.438227	1494.222836	19.099162
47.087544	1480.761903	19.104179
47.119228	1489.767122	19.109197
47.305449	1491.508378	19.114215
47.210600	1483.614366	19.119232
47.093136	1504.278956	19.124250
47.410291	1502.786937	19.129267
47.418144	1517.558678	19.134285
47.407391	1512.469748	19.139303
47.898840	1504.389190	19.144320
47.727733	1509.859963	19.149338
47.971018	1497.936464	19.154355
47.750940	1500.675541	19.159373
47.531091	1496.114860	19.164391
47.781154	1503.552079	19.169408
47.669507	1510.017130	19.174426
47.723017	1501.446583	19.179443
47.738373	1505.272293	19.184461
47.591485	1507.621189	19.189479
48.124534	1503.977698	19.194496
47.844681	1497.804258	19.199514
48.100975	1502.611591	19.204531
48.145218	1509.797023	19.209549
48.148851	1526.595556	19.214567
48.377462	1528.629990	19.219584
48.160896	1530.756265	19.224602
48.335759	1522.939905	19.229619
48.182931	1525.624265	19.234637
48.473484	1522.621552	19.239655
48.717559	1521.516541	19.244672
48.477988	1525.833498	19.249690
48.846597	1522.540831	19.254707
48.413205	1515.643478	19.259725
48.422152	1532.501148	19.264743
48.410043	1519.011266	19.269760
48.187681	1527.813298	19.274778
48.747255	1524.774748	19.279795
48.684326	1528.492802	19.284813
48.735697	1538.735253	19.289831
49.274140	1550.173251	19.294848
48.926113	1552.948162	19.299866
49.194563	1554.395660	19.304883
49.112585	1550.255199	19.309901
48.993796	1540.862675	19.314919
49.363526	1544.522412	19.319936
49.147984	1543.315833	19.324954
49.307397	1542.675387	19.329971
49.158120	1537.829070	19.334989
49.390723	1540.860163	19.340007
49.286542	1538.162302	19.345024
49.448542	1541.324384	19.350042
49.320866	1535.171272	19.355059
49.307068	1535.533156	19.360077
49.273002	1543.939604	19.365095
49.763341	1547.706684	19.370112
49.485244	1557.038197	19.375130
49.521934	1572.490310	19.380147
49.962639	1571.430231	19.385165
49.696949	1568.344239	19.390183
50.072718	1568.266372	19.395200
50.200354	1568.337840	19.400218
49.701669	1566.762189	19.405235
50.252439	1565.735362	19.410253
49.499003	1575.195010	19.415271
50.184003	1564.988538	19.420288
49.772370	1565.011946	19.425306
49.850032	1576.537934	19.430323
50.146051	1590.608145	19.435341
50.012584	1598.600981	19.440359
50.447969	1594.717140	19.445376
50.495325	1599.311069	19.450394
50.206063	1582.020590	19.455411
50.537106	1577.985835	19.460429
50.712838	1587.246260	19.465447
50.888717	1588.944962	19.470464
50.817344	1582.189690	19.475482
50.632736	1585.374525	19.480499
50.892001	1585.958729	19.485517
50.839122	1597.363165	19.490535
51.249405	1594.310122	19.495552
51.289602	1604.030470	19.500570
51.086421	1594.341855	19.505587
51.158293	1596.501845	19.510605
50.907526	1598.194806	19.515623
51.392452	1603.392401	19.520640
51.009647	1599.191758	19.525658
51.204158	1594.408334	19.530675
51.419729	1593.459270	19.535693
51.381123	1605.388522	19.540711
51.853858	1598.844656	19.545728
51.242347	1597.832662	19.550746
51.588634	1602.856308	19.555763
51.855702	1586.554848	19.560781
51.479367	1597.628089	19.565799
51.790782	1600.577413	19.570816
51.573589	1600.743936	19.575834
51.392120	1607.267301	19.580851
51.809866	1596.985913	19.585869
51.597845	1600.487486	19.590887
52.021600	1600.417881	19.595904
51.619978	1604.564576	19.600922
51.650778	1617.262486	19.605939
51.837379	1618.467179	19.610957
51.747800	1631.663668	19.615975
52.220664	1625.719408	19.620992
51.889993	1620.491212	19.626010
51.600707	1623.124379	19.631027
52.288010	1630.341659	19.636045
52.393080	1636.431956	19.641063
52.209873	1635.955646	19.646080
52.347620	1650.009674	19.651098
52.546566	1650.038411	19.656115
52.742507	1652.444071	19.661133
52.638394	1646.186237	19.666151
52.425718	1645.010761	19.671168
52.752929	1646.082967	19.676186
52.919305	1642.850368	19.681203
52.925344	1633.889542	19.686221
52.909633	1643.634451	19.691239
52.865483	1631.594943	19.696256
52.689392	1641.254519	19.701274
53.060724	1655.189899	19.706291
53.300089	1659.671705	19.711309
53.169521	1666.777285	19.716327
53.501883	1661.612463	19.721344
53.663091	1664.654764	19.726362
53.497065	1663.803356	19.731379
53.501371	1664.721015	19.736397
53.488244	1661.601747	19.741415
53.311693	1654.651476	19.746432
52.821421	1668.510407	19.751450
53.129669	1668.607230	19.756467
53.524174	1661.422310	19.761485
53.700928	1666.507252	19.766503
53.766416	1657.496073	19.771520
53.837676	1661.095294	19.776538
53.649398	1677.598971	19.781555
53.679725	1675.211393	19.786573
53.752809	1688.202547	19.791591
53.885666	1682.967985	19.796608
54.154848	1678.475814	19.801626
54.103007	1685.452296	19.806643
54.139233	1683.022765	19.811661
54.292959	1676.449953	19.816679
54.162222	1675.984358	19.821696
54.333854	1673.571486	19.826714
54.362944	1677.079482	19.831731
54.502979	1676.085441	19.836749
54.391241	1686.571295	19.841767
54.525089	1705.006488	19.846784
54.812432	1704.380709	19.851802
54.716884	1712.841053	19.856819
54.870767	1697.617638	19.861837
54.638341	1704.515117	19.866855
54.744727	1702.418594	19.871872
54.786652	1706.975530	19.876890
54.725165	1706.095117	19.881907
54.816440	1700.447318	19.886925
54.887730	1696.077671	19.891943
54.986115	1705.066236	19.896960
55.328985	1706.678822	19.901978
55.166785	1708.004446	19.906995
55.346182	1708.661132	19.912013
55.030037	1713.485621	19.917031
55.030853	1715.827182	19.922048
55.172640	1723.515000	19.927066
55.135814	1733.806097	19.932083
55.742605	1723.801150	19.937101
55.519496	1728.948758	19.942119
55.623587	1719.899939	19.947136
55.608140	1729.969921	19.952154
55.496952	1722.895767	19.957171
55.744287	1728.970118	19.962189
55.751478	1718.349017	19.967207
55.981965	1734.818695	19.972224
56.072043	1745.888384	19.977242
55.942180	1749.443390	19.982259
56.527338	1749.149670	19.987277
56.235379	1743.647112	19.992295
56.197688	1740.705259	19.997312
56.075937	1742.359084	20.002330
56.308232	1746.665283	20.007347
56.220525	1738.586992	20.012365
56.097827	1742.560622	20.017383
56.318319	1742.257760	20.022400
56.848203	1739.435278	20.027418
56.780729	1743.046784	20.032435
56.581637	1743.765927	20.037453
56.889244	1736.818668	20.042471
56.922218	1733.840497	20.047488
56.856897	1735.283496	20.052506
56.998774	1737.877530	20.057523
57.042524	1735.579366	20.062541
56.934446	1744.941147	20.067559
56.734815	1748.661727	20.072576
57.152183	1742.366341	20.077594
56.792662	1748.005570	20.082611
56.947387	1747.135464	20.087629
57.405877	1764.405787	20.092647
57.160306	1760.180449	20.097664
57.468285	1767.028000	20.102682
57.189648	1762.454369	20.107699
57.563241	1757.993160	20.112717
57.257654	1769.910698	20.117735
57.220247	1755.711345	20.122752
57.482209	1758.829400	20.127770
57.366212	1774.409757	20.132787
57.825644	1782.104641	20.137805
57.532086	1788.134361	20.142823
57.677181	1794.126917	20.147840
57.901917	1793.675057	20.152858
57.342155	1792.796962	20.157875
57.413918	1786.202236	20.162893
57.957220	1798.232961	20.167911
57.657163	1817.686209	20.172928
58.023197	1813.380815	20.177946
57.503220	1817.580817	20.182963
57.981848	1831.133426	20.187981
58.164936	1828.687179	20.192999
58.359676	1839.705811	20.198016
59.152154	1831.574788	20.203034
58.760010	1838.752979	20.208051
59.248600	1825.973422	20.213069
59.001677	1826.157228	20.218087
59.135211	1838.599342	20.223104
59.457678	1826.524355	20.228122
58.967919	1824.148810	20.233139
59.106071	1804.054890	20.238157
59.187127	1808.160723	20.243175
59.116026	1800.641572	20.248192
59.230028	1808.753529	20.253210
59.284478	1802.799022	20.258227
59.280199	1800.366354	20.263245
59.390838	1797.890434	20.268263
59.035529	1803.648949	20.273280
59.410716	1807.336290	20.278298
59.539474	1819.498255	20.283315
59.367925	1820.490815	20.288333
59.723753	1826.557669	20.293351
59.288527	1823.277273	20.298368
59.519580	1826.441211	20.303386
59.561751	1827.728511	20.308403
59.770054	1827.228729	20.313421
59.478823	1824.534882	20.318439
59.437922	1833.570583	20.323456
59.810693	1828.838068	20.328474
59.873649	1848.408055	20.333491
60.069223	1857.974801	20.338509
59.993688	1849.275974	20.343527
59.979948	1858.926011	20.348544
59.957064	1849.881241	20.353562
59.773187	1855.862238	20.358579
60.039670	1858.708185	20.363597
60.702202	1868.930817	20.368615
60.456066	1874.375584	20.373632
60.423028	1871.319364	20.378650
60.334463	1876.281822	20.383667
60.740186	1872.983278	20.388685
61.170825	1867.525270	20.393703
60.237320	1867.867142	20.398720
61.064325	1865.515678	20.403738
60.921441	1866.033502	20.408755
60.861586	1861.886347	20.413773
61.209711	1867.332687	20.418791
61.325749	1878.859169	20.423808
61.338544	1885.885566	20.428826
61.305698	1892.063835	20.433843
61.473979	1896.793540	20.438861
61.629938	1887.263107	20.443879
61.601803	1882.520801	20.448896
61.428864	1873.676265	20.453914
61.401340	1889.517434	20.458931
61.438703	1886.099863	20.463949
61.905362	1886.626337	20.468967
61.689964	1885.744781	20.473984
61.661900	1884.066961	20.479002
61.900173	1887.119318	20.484019
61.747481	1892.076047	20.489037
61.837097	1891.462305	20.494055
61.703431	1903.258314	20.499072
62.067583	1886.486904	20.504090
62.194458	1894.937734	20.509107
61.966787	1914.537546	20.514125
62.300324	1908.548747	20.519143
62.345336	1922.967837	20.524160
62.124057	1913.752132	20.529178
62.367425	1923.289333	20.534195
62.205617	1917.191933	20.539213
62.691505	1911.116143	20.544231
62.661209	1908.772749	20.549248
62.564712	1915.061991	20.554266
62.713756	1915.300533	20.559283
62.913097	1930.165697	20.564301
63.042737	1925.177739	20.569319
62.928498	1933.603243	20.574336
63.169792	1926.981903	20.579354
63.026913	1930.908240	20.584371
63.227457	1928.831655	20.589389
63.174458	1929.568945	20.594407
63.295130	1935.035161	20.599424
63.714699	1918.166670	20.604442
63.284544	1920.973439	20.609459
63.089178	1930.472077	20.614477
63.545999	1912.205946	20.619495
63.600521	1926.203798	20.624512
63.569874	1922.209854	20.629530
63.469042	1924.128680	20.634547
63.362298	1921.409070	20.639565
64.124242	1925.862721	20.644583
63.739442	1940.778387	20.649600
64.195692	1942.041848	20.654618
64.316201	1946.981037	20.659635
63.857323	1949.085359	20.664653
63.966911	1947.862528	20.669671
63.940716	1941.377772	20.674688
64.142169	1943.044098	20.679706
64.195348	1940.914856	20.684723
64.257974	1942.552435	20.689741
64.452419	1943.484503	20.694759
64.352962	1945.431520	20.699776
64.340547	1952.215723	20.704794
64.372275	1971.825453	20.709811
64.190329	1965.813249	20.714829
64.562387	1967.014158	20.719847
64.327958	1974.259218	20.724864
64.765460	1969.841597	20.729882
65.373274	1984.999442	20.734899
65.179079	1998.780679	20.739917
65.288574	2004.157142	20.744935
65.183202	1997.410196	20.749952
65.129855	1999.697159	20.754970
65.337724	1993.450289	20.759987
65.283374	2000.521968	20.765005
65.030753	1991.563616	20.770023
64.965381	1992.675259	20.775040
65.298754	1985.528193	20.780058
65.282635	2005.492621	20.785075
65.554133	2006.661948	20.790093
65.533887	2016.925362	20.795111
65.429782	2024.317294	20.800128
65.569703	2021.858847	20.805146
65.692313	2023.666931	20.810163
65.612367	2035.328369	20.815181
66.218994	2033.412229	20.820199
66.216134	2044.174746	20.825216
66.210355	2037.046080	20.830234
66.865278	2040.938971	20.835251
66.737008	2040.867485	20.840269
66.745285	2039.401724	20.845287
66.598214	2044.865738	20.850304
66.719225	2028.069169	20.855322
66.721040	2031.190158	20.860339
66.902027	2041.087517	20.865357
66.770097	2029.951499	20.870375
66.863080	2037.571354	20.875392
66.808753	2037.756547	20.880410
67.120469	2021.984225	20.885427
66.930015	2034.477236	20.890445
67.230786	2027.126963	20.895463
67.072979	2028.196281	20.900480
67.147160	2021.474847	20.905498
67.201197	2022.548848	20.910515
67.083144	2024.274707	20.915533
67.269530	2037.911133	20.920551
67.199268	2044.739151	20.925568
67.401169	2052.998406	20.930586
67.339542	2050.467383	20.935603
67.190288	2055.379433	20.940621
67.627435	2044.630811	20.945639
67.865371	2050.937137	20.950656
67.306009	2056.254294	20.955674
67.584158	2064.649942	20.960691
67.703309	2082.996300	20.965709
68.118634	2078.910357	20.970727
68.072450	2087.820772	20.975744
67.983427	2083.002739	20.980762
67.867691	2082.231800	20.985779
68.056090	2089.704173	20.990797
68.088068	2095.777674	20.995815
68.396063	2099.207339	21.000832
68.245857	2105.167364	21.005850
68.534301	2106.229893	21.010867
68.207747	2104.680875	21.015885
68.719451	2107.715679	21.020903
68.643872	2108.289242	21.025920
68.727494	2128.007787	21.030938
68.880999	2113.349015	21.035955
68.995949	2113.592902	21.040973
69.236302	2126.826433	21.045991
69.193275	2128.780408	21.051008
68.915211	2132.216686	21.056026
69.421423	2124.007297	21.061043
69.184332	2121.816205	21.066061
69.459155	2107.794891	21.071079
69.720942	2112.153368	21.076096
69.206476	2122.153419	21.081114
69.604390	2126.174965	21.086131
69.728949	2143.330702	21.091149
69.820153	2146.601822	21.096167
69.918071	2145.639603	21.101184
69.895789	2151.207185	21.106202
70.384326	2142.653389	21.111219
70.160955	2151.070844	21.116237
70.093127	2145.334214	21.121255
70.285702	2143.176796	21.126272
70.501464	2148.091649	21.131290
70.322965	2131.752197	21.136307
70.175803	2141.880919	21.141325
69.793791	2145.425011	21.146343
70.099589	2160.737630	21.151360
70.305196	2161.377603	21.156378
70.494803	2155.322902	21.161395
70.894124	2163.163081	21.166413
70.709852	2173.973035	21.171431
70.744729	2171.256447	21.176448
70.749480	2172.568572	21.181466
70.653474	2189.623198	21.186483
70.749864	2193.641503	21.191501
70.944622	2197.167831	21.196519
70.802089	2189.915350	21.201536
71.034955	2192.476259	21.206554
71.518467	2211.507341	21.211571
71.169936	2208.153324	21.216589
71.273248	2213.931641	21.221607
71.758274	2213.902935	21.226624
72.097438	2215.935909	21.231642
72.153410	2210.362914	21.236659
72.002301	2217.481398	21.241677
71.967767	2211.212466	21.246695
72.211300	2210.397858	21.251712
72.086955	2212.942146	21.256730
72.269506	2207.324072	21.261747
72.134662	2208.632821	21.266765
72.054699	2211.772966	21.271783
72.675997	2207.493764	21.276800
72.309927	2206.291785	21.281818
72.817992	2204.870795	21.286835
72.614461	2207.165533	21.291853
72.776674	2200.749004	21.296871
72.981269	2198.075256	21.301888
72.644044	2197.329546	21.306906
72.465947	2203.483337	21.311923
72.736735	2203.740682	21.316941
72.513380	2214.045498	21.321959
73.151415	2229.097822	21.326976
72.954747	2229.851321	21.331994
72.907311	2226.510092	21.337011
72.895221	2232.003512	21.342029
72.790165	2231.243518	21.347047
73.326061	2233.163613	21.352064
73.163146	2242.300694	21.357082
73.308301	2253.756578	21.362099
73.246500	2254.987608	21.367117
73.394219	2251.054017	21.372135
73.405020	2256.726911	21.377152
73.504423	2263.913472	21.382170
73.751064	2263.300365	21.387187
73.861830	2264.864154	21.392205
73.792362	2270.527536	21.397223
73.932096	2264.606856	21.402240
73.841235	2269.017466	21.407258
73.720404	2272.015688	21.412275
74.193384	2282.836352	21.417293
74.469813	2290.203491	21.422311
74.579421	2285.960253	21.427328
74.504490	2292.501891	21.432346
74.615942	2288.204711	21.437363
74.652191	2285.737222	21.442381
74.665771	2286.921728	21.447399
74.919463	2282.684322	21.452416
74.662792	2287.357621	21.457434
75.143190	2302.374739	21.462451
75.073418	2308.218078	21.467469
75.069417	2312.924387	21.472487
75.251865	2317.137540	21.477504
74.878518	2314.232401	21.482522
75.228266	2304.513581	21.487539
75.425496	2312.726346	21.492557
75.287964	2313.208627	21.497575
75.485717	2327.215911	21.502592
75.225425	2335.708671	21.507610
75.485042	2335.014626	21.512627
75.791551	2326.050565	21.517645
75.933492	2342.439992	21.522663
75.788918	2332.849102	21.527680
76.059740	2349.723320	21.532698
76.319079	2348.947259	21.537715
76.395943	2356.535058	21.542733
76.304790	2357.253093	21.547751
76.518674	2355.461576	21.552768
76.269099	2355.986661	21.557786
76.311591	2351.081673	21.562803
76.344967	2355.857884	21.567821
76.338059	2360.820306	21.572839
76.828868	2357.161173	21.577856
76.856187	2353.741931	21.582874
76.736692	2375.869118	21.587891
77.132993	2380.582163	21.592909
76.534582	2388.692378	21.597927
77.014145	2372.467378	21.602944
76.844446	2380.841814	21.607962
76.877415	2377.667859	21.612979
77.059722	2380.669103	21.617997
77.232279	2400.178335	21.623015
77.161414	2396.875462	21.628032
77.188694	2402.299644	21.633050
77.155868	2407.149363	21.638067
77.433775	2408.361899	21.643085
77.832635	2423.994711	21.648103
78.181713	2429.093901	21.653120
77.914591	2441.406683	21.658138
78.287665	2433.360039	21.663155
78.106818	2428.543675	21.668173
77.976596	2428.084290	21.673191
78.321166	2429.800830	21.678208
78.504392	2420.704544	21.683226
78.380982	2420.730134	21.688243
78.349648	2420.031172	21.693261
78.351370	2421.201764	21.698279
78.447879	2425.415782	21.703296
78.456747	2441.797744	21.708314
78.625005	2439.549418	21.713331
78.782461	2442.444102	21.718349
78.719240	2448.652570	21.723367
79.169399	2458.321776	21.728384
78.751331	2457.405664	21.733402
78.912797	2454.419867	21.738419
79.167219	2465.622058	21.743437
78.929048	2484.592911	21.748455
79.552890	2474.629065	21.753472
79.234510	2476.361104	21.758490
79.326087	2478.256156	21.763507
79.668307	2473.989055	21.768525
79.592488	2488.288660	21.773543
80.167883	2494.412871	21.778560
80.050151	2490.350385	21.783578
80.275457	2496.721970	21.788595
80.636036	2488.235401	21.793613
80.309874	2495.693877	21.798631
80.648974	2489.546209	21.803648
80.434921	2492.129839	21.808666
80.674246	2504.028767	21.813683
80.601203	2498.453804	21.818701
80.480535	2492.564379	21.823719
80.478107	2486.429190	21.828736
80.661024	2488.644481	21.833754
80.505869	2494.008901	21.838771
80.748439	2491.720521	21.843789
80.871792	2494.200791	21.848807
80.771348	2493.613650	21.853824
81.070625	2510.246852	21.858842
80.701468	2511.339842	21.863859
81.272586	2512.983023	21.868877
80.701202	2511.693256	21.873895
80.659408	2521.651033	21.878912
81.151972	2531.821773	21.883930
81.052582	2543.877947	21.888947
81.645111	2540.969783	21.893965
81.809646	2552.801558	21.898983
81.850733	2565.886733	21.904000
82.181735	2570.382817	21.909018
82.007511	2563.214053	21.914035
82.327802	2558.132928	21.919053
81.986438	2565.846306	21.924071
82.296887	2570.828500	21.929088
82.584051	2557.603408	21.934106
82.265417	2559.193468	21.939123
82.478303	2550.004097	21.944141
82.187360	2556.926850	21.949159
82.607469	2573.481212	21.954176
82.900397	2579.302531	21.959194
82.831812	2581.055411	21.964211
83.232121	2577.565065	21.969229
82.849751	2584.123414	21.974247
83.121666	2578.737404	21.979264
83.152609	2589.236147	21.984282
83.227544	2586.364883	21.989299
83.076390	2579.874225	21.994317
83.119336	2582.616441	21.999335
83.423920	2566.409213	22.004352
83.344710	2578.080356	22.009370
83.643488	2584.175345	22.014387
83.856982	2594.724394	22.019405
83.991636	2596.413872	22.024423
83.819621	2595.512858	22.029440
83.852387	2597.448697	22.034458
83.574502	2601.983374	22.039475
83.935769	2603.249142	22.044493
83.737063	2606.774073	22.049511
83.780072	2604.258139	22.054528
84.089718	2620.047127	22.059546
84.070864	2627.094553	22.064563
84.092728	2624.966981	22.069581
84.486637	2642.191459	22.074599
84.697538	2642.107861	22.079616
84.704133	2650.423240	22.084634
84.689992	2648.471738	22.089651
84.608692	2644.867464	22.094669
84.660507	2652.535060	22.099687
84.973803	2657.175967	22.104704
85.359889	2661.404639	22.109722
85.005390	2678.058364	22.114739
85.359695	2671.876690	22.119757
85.260467	2672.274075	22.124775
85.566678	2672.488004	22.129792
85.621832	2682.455930	22.134810
85.911195	2692.851124	22.139827
86.070049	2695.313235	22.144845
85.889081	2700.555514	22.149863
85.919468	2698.486565	22.154880
85.856346	2691.663302	22.159898
86.100315	2688.516202	22.164915
86.193471	2688.542580	22.169933
86.469082	2688.600339	22.174951
86.730560	2691.058997	22.179968
86.636747	2691.313506	22.184986
86.542089	2696.037275	22.190003
86.735597	2706.586366	22.195021
86.863691	2717.123618	22.200039
86.597217	2718.067973	22.205056
86.719677	2711.010477	22.210074
86.736226	2720.369020	22.215091
86.833523	2715.105012	22.220109
87.340069	2725.137957	22.225127
87.219640	2723.038978	22.230144
87.290432	2732.089192	22.235162
86.947294	2736.277478	22.240179
87.233737	2727.287957	22.245197
87.338244	2741.600542	22.250215
87.151571	2754.402764	22.255232
87.542208	2754.025887	22.260250
87.877162	2763.678591	22.265267
87.671269	2757.196445	22.270285
88.155641	2761.766391	22.275303
87.723997	2768.935356	22.280320
88.146489	2782.674229	22.285338
88.302016	2792.007879	22.290355
88.506150	2778.315894	22.295373
88.624593	2781.860606	22.300391
88.540983	2781.804212	22.305408
88.879505	2782.401292	22.310426
88.539542	2776.385165	22.315443
89.129957	2768.771436	22.320461
89.008226	2776.756643	22.325479
88.901682	2783.445440	22.330496
89.004245	2800.362224	22.335514
89.109487	2803.157837	22.340531
89.644435	2796.591171	22.345549
89.230677	2807.535299	22.350567
89.394548	2800.610152	22.355584
89.937065	2797.507788	22.360602
89.472302	2807.197434	22.365619
89.686695	2808.265296	22.370637
89.722115	2811.523184	22.375655
89.470451	2811.916048	22.380672
89.861590	2812.896251	22.385690
89.734253	2821.617747	22.390707
89.959839	2823.176221	22.395725
89.971385	2831.850712	22.400743
89.954096	2833.630298	22.405760
90.283761	2838.262375	22.410778
90.229325	2852.120209	22.415795
90.523501	2840.288848	22.420813
90.669586	2854.402481	22.425831
90.567991	2848.838195	22.430848
90.685004	2858.878588	22.435866
90.908466	2870.461469	22.440883
90.967591	2866.718371	22.445901
91.252647	2875.053351	22.450919
91.090054	2872.399157	22.455936
91.578673	2881.961569	22.460954
91.513296	2875.583614	22.465971
91.665995	2863.641844	22.470989
91.831346	2873.857731	22.476007
91.646776	2883.942231	22.481024
91.856011	2882.290264	22.486042
92.067357	2890.314867	22.491059
92.386772	2887.660903	22.496077
92.313649	2890.572848	22.501095
92.085648	2898.363292	22.506112
92.496822	2890.714471	22.511130
92.426236	2885.988020	22.516147
92.511478	2882.177703	22.521165
92.198478	2892.348609	22.526183
92.272847	2897.670876	22.531200
92.908553	2904.903075	22.536218
92.671268	2916.936916	22.541235
92.839791	2919.315483	22.546253
92.938216	2914.796104	22.551271
92.781909	2915.814739	22.556288
93.187354	2925.614296	22.561306
92.972811	2941.978059	22.566323
93.261861	2944.041063	22.571341
93.187680	2936.881726	22.576359
93.346239	2946.789411	22.581376
93.527708	2941.022938	22.586394
93.364313	2957.927882	22.591411
93.985444	2963.316005	22.596429
93.935454	2965.927654	22.601447
93.611264	2966.619099	22.606464
93.533831	2961.259302	22.611482
93.772628	2980.449477	22.616499
93.808856	2986.582580	22.621517
94.007850	2977.837040	22.626535
94.198701	2995.213606	22.631552
94.548082	3001.692180	22.636570
94.400409	3007.248109	22.641587
94.897320	3010.080235	22.646605
95.370792	3001.853487	22.651623
95.116188	3005.115817	22.656640
95.224492	3001.579609	22.661658
95.168087	3005.476849	22.666675
95.060931	3000.339476	22.671693
95.586254	2999.587999	22.676711
95.112663	3000.605848	22.681728
95.569084	3005.527420	22.686746
95.605983	3019.942348	22.691763
95.894501	3022.223224	22.696781
95.825637	3034.145538	22.701799
95.619158	3039.508691	22.706816
95.939676	3027.818268	22.711834
95.722948	3035.076759	22.716851
95.780144	3035.193990	22.721869
96.388390	3049.263774	22.726887
96.384462	3062.163832	22.731904
96.721408	3058.029983	22.736922
96.441534	3066.074812	22.741939
96.487625	3058.044402	22.746957
96.681205	3050.082419	22.751975
96.432676	3058.510550	22.756992
96.846589	3072.127896	22.762010
97.022885	3085.694105	22.767027
97.002369	3080.454761	22.772045
97.307390	3080.949788	22.777063
97.085703	3085.081251	22.782080
97.092284	3077.817675	22.787098
97.343968	3091.766606	22.792115
97.571977	3100.044347	22.797133
97.478742	3094.642799	22.802151
97.323325	3110.123174	22.807168
97.641881	3117.544022	22.812186
97.798411	3125.959223	22.817203
97.739902	3123.585372	22.822221
97.900499	3124.933118	22.827239
98.068820	3140.126081	22.832256
98.076982	3148.302569	22.837274
98.672705	3148.092399	22.842291
98.530094	3148.221997	22.847309
98.615940	3150.266361	22.852327
98.694929	3154.906232	22.857344
98.966948	3166.248134	22.862362
98.852834	3170.318576	22.867379
99.043662	3174.281274	22.872397
99.168770	3167.715560	22.877415
99.009270	3175.965672	22.882432
98.958152	3172.921532	22.887450
99.440710	3178.612337	22.892467
99.255303	3196.556203	22.897485
99.677894	3190.477280	22.902503
99.593261	3198.444235	22.907520
99.972769	3195.149563	22.912538
100.032255	3215.917800	22.917555
100.079271	3221.219198	22.922573
100.398517	3215.936053	22.927591
99.754518	3224.208437	22.932608
100.263500	3218.747222	22.937626
100.610957	3219.475480	22.942643
100.243512	3218.564020	22.947661
100.701241	3238.001075	22.952679
100.620589	3237.363465	22.957696
100.789840	3245.997667	22.962714
101.037079	3238.273383	22.967731
100.907532	3246.480959	22.972749
101.453762	3244.571006	22.977767
101.648984	3262.414272	22.982784
101.457637	3258.880772	22.987802
101.568399	3267.754556	22.992819
101.727689	3268.944704	22.997837
101.597529	3260.203252	23.002855
101.922954	3267.370585	23.007872
101.941118	3270.722791	23.012890
101.981934	3260.628920	23.017907
101.769732	3263.739465	23.022925
102.251345	3256.795926	23.027943
101.961302	3275.327546	23.032960
102.319488	3280.690681	23.037978
102.406209	3283.981648	23.042995
102.685416	3289.082563	23.048013
102.580937	3286.065702	23.053031
102.385636	3291.506085	23.058048
102.242592	3283.517832	23.063066
102.716410	3293.448910	23.068083
102.667906	3307.410320	23.073101
102.934060	3308.684730	23.078119
102.975156	3330.743739	23.083136
103.214903	3338.865093	23.088154
103.439287	3330.674065	23.093171
103.287755	3339.017691	23.098189
103.617249	3336.769244	23.103207
103.642850	3345.132466	23.108224
103.793327	3347.488667	23.113242
104.225138	3356.558385	23.118259
104.231172	3358.299649	23.123277
104.429723	3354.095883	23.128295
104.250137	3356.327045	23.133312
104.134419	3356.329336	23.138330
104.703613	3374.578096	23.143347
104.497677	3379.262664	23.148365
104.540282	3378.848771	23.153383
104.717825	3378.603115	23.158400
104.743155	3375.748966	23.163418
105.263069	3388.434622	23.168435
105.366461	3397.940881	23.173453
105.483317	3393.775156	23.178471
105.568579	3402.981255	23.183488
105.522152	3406.157384	23.188506
105.430797	3399.767532	23.193523
105.594343	3404.640410	23.198541
105.580342	3414.594325	23.203559
106.141194	3420.670634	23.208576
105.884286	3425.306386	23.213594
106.480857	3419.174881	23.218611
106.449830	3430.251954	23.223629
106.419243	3424.840492	23.228647
106.466985	3431.044538	23.233664
106.535930	3426.700090	23.238682
106.962053	3419.149707	23.243699
106.369356	3429.541485	23.248717
107.232620	3450.862668	23.253735
107.073096	3452.948665	23.258752
106.955272	3452.241119	23.263770
107.217461	3458.465234	23.268787
107.367353	3463.494926	23.273805
107.422462	3449.832094	23.278823
107.480106	3455.261305	23.283840
107.591840	3476.738135	23.288858
107.887805	3476.991558	23.293875
108.084992	3482.152723	23.298893
107.722905	3483.538197	23.303911
107.905814	3482.401622	23.308928
107.809778	3482.164106	23.313946
108.034543	3493.961813	23.318963
108.120815	3515.474242	23.323981
107.992013	3502.512477	23.328999
108.358105	3504.058468	23.334016
108.464531	3523.538245	23.339034
108.550323	3527.195534	23.344051
108.473238	3530.963562	23.349069
108.741097	3531.196138	23.354087
108.763679	3535.336779	23.359104
108.716394	3548.780549	23.364122
109.214436	3554.557426	23.369139
109.159870	3558.189366	23.374157
109.095590	3549.816210	23.379175
109.319012	3565.799446	23.384192
109.457745	3580.962696	23.389210
109.878257	3579.088187	23.394227
109.867038	3589.250079	23.399245
110.069381	3589.448733	23.404263
110.471674	3600.492742	23.409280
110.196775	3610.951619	23.414298
110.334925	3602.906545	23.419315
110.545819	3603.536275	23.424333
110.759018	3610.247878	23.429351
110.655367	3611.340367	23.434368
110.605451	3620.422563	23.439386
110.804305	3613.703099	23.444403
110.726521	3626.779260	23.449421
110.992691	3622.912034	23.454439
111.340478	3627.083811	23.459456
111.311461	3645.259281	23.464474
111.740970	3652.767127	23.469491
111.634495	3653.089915	23.474509
111.849174	3651.070892	23.479527
111.978517	3643.964610	23.484544
111.838319	3651.009352	23.489562
112.066299	3644.626197	23.494579
111.922971	3668.620935	23.499597
112.113460	3673.502290	23.504615
112.424348	3677.064374	23.509632
112.433244	3673.938151	23.514650
112.623388	3675.019335	23.519667
112.834094	3696.345198	23.524685
112.890512	3694.821259	23.529703
113.355581	3700.496034	23.534720
113.103916	3695.267475	23.539738
113.344654	3692.878230	23.544755
113.147948	3698.113792	23.549773
113.291663	3700.325908	23.554791
113.538918	3703.506580	23.559808
113.310155	3721.751297	23.564826
113.441769	3720.581711	23.569843
113.495341	3731.165951	23.574861
113.485771	3732.897070	23.579879
114.103982	3739.769370	23.584896
114.026703	3748.196241	23.589914
114.255869	3742.226348	23.594931
114.250860	3758.570647	23.599949
114.378509	3771.106554	23.604967
114.334380	3762.199875	23.609984
114.618370	3762.048010	23.615002
115.048974	3781.278426	23.620019
114.561957	3799.216482	23.625037
114.822177	3794.646285	23.630055
115.321942	3795.940946	23.635072
115.160898	3804.687133	23.640090
115.547051	3823.015526	23.645107
115.429166	3820.496224	23.650125
115.444523	3822.409672	23.655143
115.922037	3823.947704	23.660160
116.001612	3824.222409	23.665178
116.128675	3837.717988	23.670195
116.197984	3844.199713	23.675213
116.260249	3845.310410	23.680231
116.584707	3839.922109	23.685248
116.283319	3838.122797	23.690266
116.434331	3839.216433	23.695283
116.231873	3839.699455	23.700301
116.485114	3864.913806	23.705319
116.654656	3856.958392	23.710336
116.971688	3869.631985	23.715354
117.169963	3866.435027	23.720371
117.309548	3887.816447	23.725389
117.395170	3900.374810	23.730407
117.595167	3896.514738	23.735424
117.569506	3908.831719	23.740442
118.011277	3894.625049	23.745459
117.770681	3893.333853	23.750477
117.947779	3901.058104	23.755495
118.246862	3905.158666	23.760512
118.244025	3918.655718	23.765530
118.310588	3915.662456	23.770547
118.323981	3916.370486	23.775565
118.298036	3919.420397	23.780583
118.545869	3922.954533	23.785600
118.584632	3944.342346	23.790618
118.900500	3937.326669	23.795635
119.072949	3940.667454	23.800653
118.978165	3953.737043	23.805671
119.113036	3956.966932	23.810688
119.260168	3960.264340	23.815706
119.280737	3966.081435	23.820723
119.357275	3977.779581	23.825741
119.705786	3982.670984	23.830759
119.930938	3989.661775	23.835776
120.020924	3987.292953	23.840794
119.857526	3985.986499	23.845811
120.033187	3998.515042	23.850829
120.228913	4016.886091	23.855847
120.536402	4008.457635	23.860864
120.476913	4016.581986	23.865882
120.798453	4018.542177	23.870899
121.084218	4043.085682	23.875917
121.091139	4045.619129	23.880935
121.130438	4035.572411	23.885952
120.908001	4046.922892	23.890970
121.251797	4039.868080	23.895987
121.520611	4059.610225	23.901005
121.376278	4068.281323	23.906023
121.516302	4062.918695	23.911040
121.522750	4070.249953	23.916058
121.726709	4083.919896	23.921075
122.041437	4089.242735	23.926093
122.143479	4095.053419	23.931111
122.182326	4088.478792	23.936128
122.361572	4100.470255	23.941146
122.316821	4106.275533	23.946163
122.679464	4114.561055	23.951181
123.029778	4111.583278	23.956199
123.054784	4112.589355	23.961216
123.111845	4123.899252	23.966234
123.565810	4136.864064	23.971251
123.282743	4134.752523	23.976269
123.254669	4132.007627	23.981287
123.779589	4132.644994	23.986304
123.359631	4138.092419	23.991322
123.455030	4151.631069	23.996339
124.146527	4158.258474	24.001357
124.152048	4159.958862	24.006375
124.491950	4157.067933	24.011392
123.937061	4159.948239	24.016410
124.196095	4165.687005	24.021427
124.415557	4167.388596	24.026445
124.224976	4185.583607	24.031463
124.607830	4181.896839	24.036480
124.685306	4190.012435	24.041498
124.962248	4200.565111	24.046515
124.939056	4213.074453	24.051533
124.911318	4215.644918	24.056551
125.058652	4223.680143	24.061568
125.477743	4225.786053	24.066586
125.692032	4233.772916	24.071603
125.802458	4242.281084	24.076621
125.894455	4248.298560	24.081639
126.261092	4244.548035	24.086656
125.934035	4252.357733	24.091674
125.920720	4245.967981	24.096691
126.142001	4261.784877	24.101709
126.255665	4270.017941	24.106727
126.519235	4270.967713	24.111744
126.747825	4270.455221	24.116762
127.103801	4283.539652	24.121779
127.049849	4288.071228	24.126797
126.661595	4292.109114	24.131815
127.169021	4293.326858	24.136832
127.413027	4304.752776	24.141850
127.133670	4313.599811	24.146867
127.449879	4309.778262	24.151885
127.304872	4318.721039	24.156903
127.539766	4329.766471	24.161920
127.793034	4341.702306	24.166938
127.985733	4353.101572	24.171955
128.220748	4364.547875	24.176973
127.926582	4365.802826	24.181991
128.405497	4363.534002	24.187008
128.808120	4379.130046	24.192026
128.850001	4394.716334	24.197043
129.176361	4392.622918	24.202061
128.931240	4395.435791	24.207079
129.148641	4388.867803	24.212096
128.968765	4396.976464	24.217114
129.338685	4409.339129	24.222131
129.680415	4413.076446	24.227149
129.577569	4412.322324	24.232167
129.581293	4431.516147	24.237184
129.993399	4439.058612	24.242202
129.997794	4448.997586	24.247219
129.883082	4437.762690	24.252237
130.112447	4453.458541	24.257255
130.419458	4459.275108	24.262272
130.516986	4464.073391	24.267290
130.575546	4476.453317	24.272307
130.786240	4483.945287	24.277325
130.678843	4499.990646	24.282343
131.169363	4493.556594	24.287360
131.528694	4491.394872	24.292378
131.229427	4503.269023	24.297395
131.618008	4511.250798	24.302413
131.381989	4520.870794	24.307431
131.784107	4513.753003	24.312448
131.805805	4518.812542	24.317466
131.913678	4531.576184	24.322483
132.083051	4532.540728	24.327501
132.301246	4538.503807	24.332519
132.614583	4538.091665	24.337536
132.742685	4557.231413	24.342554
132.856672	4567.393176	24.347571
132.943618	4555.934067	24.352589
132.749078	4560.219435	24.357607
132.864987	4563.114658	24.362624
133.478276	4566.484345	24.367642
133.222422	4579.630122	24.372659
133.698939	4580.044667	24.377677
133.733033	4580.841018	24.382695
133.607747	4586.043550	24.387712
133.937920	4582.115593	24.392730
133.622653	4590.911570	24.397747
134.193265	4587.473078	24.402765
134.106559	4602.978682	24.407783
134.234695	4608.580271	24.412800
134.488556	4613.360414	24.417818
134.345011	4620.222978	24.422835
134.846819	4632.290518	24.427853
134.365349	4642.668714	24.432871
134.680435	4643.468393	24.437888
134.735539	4660.839418	24.442906
134.708804	4666.960860	24.447923
135.383439	4677.883951	24.452941
135.484282	4685.680457	24.457959
135.552632	4695.379121	24.462976
136.257665	4699.188998	24.467994
136.178571	4708.235274	24.473011
136.585360	4716.817183	24.478029
136.480546	4717.641615	24.483047
136.767903	4712.959617	24.488064
136.622774	4708.872514	24.493082
136.560081	4704.365307	24.498099
136.635521	4719.769851	24.503117
136.482394	4740.661526	24.508135
136.986325	4736.946209	24.513152
137.397688	4744.725658	24.518170
137.268575	4762.494954	24.523187
137.599322	4757.645165	24.528205
137.682323	4765.416092	24.533223
137.616464	4766.597423	24.538240
137.776622	4783.434437	24.543258
138.035052	4789.991036	24.548275
138.159224	4788.342757	24.553293
138.495218	4796.954734	24.558311
138.396898	4809.807692	24.563328
138.749423	4813.158305	24.568346
138.677401	4823.671318	24.573363
139.041599	4815.653426	24.578381
139.189005	4832.334656	24.583399
139.239659	4845.776668	24.588416
139.535140	4843.034636	24.593434
139.172955	4855.401822	24.598451
139.364420	4854.749931	24.603469
139.491068	4868.467299	24.608487
139.790278	4867.463934	24.613504
139.961132	4873.819639	24.618522
140.185443	4897.938325	24.623539
140.422833	4903.384001	24.628557
140.348086	4895.179160	24.633575
140.573383	4898.079396	24.638592
140.514403	4904.534250	24.643610
140.695664	4923.009492	24.648627
141.044612	4924.327867	24.653645
141.100574	4928.652989	24.658663
140.969713	4937.937918	24.663680
141.048334	4947.628794	24.668698
141.120314	4954.347239	24.673715
141.486071	4962.680011	24.678733
141.814453	4973.054624	24.683751
141.956747	4974.730504	24.688768
142.252691	4979.624101	24.693786
142.522831	5002.122742	24.698803
143.092908	4998.741076	24.703821
142.559020	4996.078449	24.708839
142.564382	5000.664041	24.713856
142.619865	5003.808700	24.718874
142.816056	4998.844195	24.723891
142.987101	5018.296513	24.728909
143.334518	5023.112614	24.733927
143.460023	5028.642143	24.738944
143.427393	5016.825847	24.743962
143.104554	5037.312000	24.748979
143.762711	5040.406440	24.753997
143.732885	5050.568907	24.759015
143.767204	5063.322349	24.764032
144.181987	5073.058482	24.769050
143.790711	5070.878553	24.774067
144.466912	5081.088257	24.779085
144.371737	5096.841821	24.784103
144.426663	5107.518191	24.789120
145.020042	5102.238906	24.794138
144.811574	5125.586044	24.799155
145.187394	5127.282171	24.804173
145.713179	5130.163778	24.809191
145.491886	5136.388459	24.814208
145.818192	5143.442763	24.819226
145.887440	5151.566391	24.824243
145.753078	5159.507273	24.829261
146.199930	5154.301435	24.834279
146.152651	5166.007117	24.839296
146.645483	5172.779661	24.844314
146.333646	5172.108754	24.849331
146.725222	5181.861206	24.854349
147.184289	5204.627220	24.859367
146.858659	5204.378300	24.864384
147.205748	5198.316857	24.869402
147.103535	5203.762165	24.874419
147.427353	5224.781696	24.879437
147.255433	5227.640047	24.884455
147.609508	5240.327735	24.889472
147.738045	5248.994524	24.894490
148.133838	5259.301921	24.899507
148.108354	5267.623525	24.904525
148.524193	5272.700442	24.909543
148.705063	5275.080544	24.914560
148.646734	5287.927573	24.919578
148.494142	5286.130055	24.924595
148.688092	5294.215270	24.929613
149.022942	5303.869351	24.934631
148.908167	5313.265588	24.939648
149.409672	5321.312103	24.944666
149.257916	5335.164980	24.949683
149.262837	5342.556965	24.954701
149.460382	5347.090439	24.959719
149.461574	5367.715595	24.964736
149.959704	5357.706747	24.969754
149.695143	5380.952517	24.974771
149.974826	5389.734585	24.979789
150.293739	5397.904439	24.984807
150.506672	5409.089703	24.989824
150.807557	5414.822309	24.994842
150.860763	5434.501870	24.999859
150.965336	5439.346657	25.004877
150.786750	5443.339319	25.009895
151.252796	5463.288838	25.014912
151.679281	5463.768066	25.019930
151.677387	5459.768836	25.024947
151.666321	5475.395910	25.029965
152.502394	5482.228435	25.034983
152.541881	5492.348723	25.040000
152.824439	5491.540490	25.045018
152.867364	5492.218701	25.050035
152.531790	5490.023681	25.055053
153.156030	5476.112334	25.060071
153.374475	5495.314674	25.065088
153.210068	5497.890947	25.070106
153.366549	5510.347778	25.075123
153.197515	5512.555450	25.080141
153.689584	5514.687961	25.085159
153.327336	5526.487412	25.090176
153.910259	5527.418789	25.095194
153.683419	5533.811776	25.100211
154.090420	5545.894778	25.105229
154.058378	5552.361423	25.110247
154.247919	5566.710266	25.115264
154.369502	5565.340110	25.120282
154.285160	5587.007985	25.125299
155.073048	5591.212285	25.130317
155.140841	5588.565790	25.135335
155.147068	5613.878086	25.140352
155.175603	5611.256678	25.145370
155.453576	5616.418424	25.150387
155.314471	5637.681414	25.155405
155.842957	5639.066417	25.160423
155.963958	5645.707990	25.165440
156.202806	5665.816435	25.170458
156.375426	5667.171961	25.175475
156.236637	5676.682630	25.180493
156.632106	5688.316128	25.185511
156.735936	5701.283250	25.190528
156.931724	5702.287914	25.195546
157.016402	5713.992214	25.200563
157.206097	5733.600208	25.205581
157.299616	5722.063578	25.210599
157.462839	5739.863786	25.215616
157.981272	5748.962175	25.220634
158.050721	5754.769026	25.225651
157.841509	5764.391788	25.230669
157.980042	5766.342964	25.235687
158.219791	5774.815805	25.240704
158.525626	5778.798940	25.245722
158.615171	5788.043456	25.250739
158.639874	5799.930826	25.255757
159.005591	5809.270983	25.260775
159.258565	5824.446617	25.265792
159.226792	5825.452214	25.270810
159.708871	5833.268404	25.275827
159.618107	5849.596445	25.280845
159.659799	5849.321536	25.285863
159.897804	5847.383852	25.290880
160.061733	5856.506265	25.295898
160.486631	5877.737997	25.300915
160.320874	5882.574745	25.305933
160.900698	5880.551940	25.310951
160.681512	5900.707147	25.315968
160.995380	5901.251382	25.320986
161.446987	5908.636750	25.326003
161.279745	5909.385783	25.331021
161.682521	5917.760546	25.336039
161.780785	5935.021851	25.341056
161.851787	5937.510798	25.346074
161.843105	5941.312800	25.351091
162.024226	5956.263047	25.356109
162.394851	5953.660602	25.361127
162.730710	5962.200549	25.366144
162.478603	5961.359259	25.371162
162.893326	5977.715553	25.376179
162.553784	5994.328923	25.381197
163.105428	5993.712112	25.386215
162.949875	5992.252758	25.391232
163.093435	6005.756830	25.396250
163.376736	6010.980988	25.401267
163.365687	6014.382471	25.406285
163.679443	6029.277274	25.411303
163.484989	6036.321964	25.416320
163.268581	6038.723368	25.421338
163.923708	6057.002409	25.426355
164.390176	6073.606378	25.431373
164.877984	6082.182555	25.436391
164.492015	6096.893456	25.441408
164.611755	6099.437924	25.446426
165.018242	6111.957015	25.451443
165.288098	6123.755681	25.456461
165.804786	6118.636492	25.461479
165.579032	6135.876142	25.466496
165.670038	6141.562938	25.471514
166.122543	6151.880898	25.476531
166.100688	6155.078910	25.481549
166.521418	6166.282593	25.486567
166.533812	6180.546026	25.491584
166.368667	6174.308813	25.496602
166.711622	6174.876911	25.501619
167.304844	6186.091464	25.506637
167.234583	6188.997172	25.511655
167.120576	6200.259395	25.516672
167.432645	6212.979596	25.521690
167.723500	6220.005149	25.526707
167.858680	6231.240979	25.531725
168.116239	6239.196692	25.536743
168.505439	6244.811551	25.541760
168.601934	6256.208140	25.546778
168.397373	6253.298009	25.551795
168.779089	6264.469983	25.556813
168.831759	6274.326625	25.561831
169.198601	6275.680180	25.566848
169.159882	6281.592535	25.571866
169.459025	6295.574377	25.576883
169.222849	6304.346155	25.581901
169.574371	6307.466759	25.586919
169.642485	6322.154054	25.591936
169.809439	6332.943018	25.596954
170.136786	6344.205635	25.601971
170.078593	6356.339956	25.606989
170.755715	6352.278351	25.612007
170.470511	6362.213226	25.617024
170.636139	6374.157811	25.622042
171.054458	6378.439136	25.627059
170.872745	6403.406306	25.632077
170.958447	6408.156445	25.637095
171.177661	6425.437145	25.642112
171.488955	6441.645903	25.647130
171.580554	6442.089234	25.652147
171.611811	6460.977820	25.657165
172.178189	6468.591668	25.662183
172.253991	6478.814144	25.667200
172.442005	6491.762324	25.672218
172.920730	6486.462729	25.677236
173.059776	6512.648838	25.682253
173.332629	6520.403397	25.687271
173.327273	6513.487572	25.692288
173.343888	6529.363754	25.697306
173.743706	6526.169487	25.702324
173.500721	6541.063536	25.707341
174.059853	6545.427016	25.712359
174.177112	6563.639300	25.717376
174.393177	6576.103306	25.722394
174.586890	6564.610431	25.727412
174.747107	6571.129394	25.732429
174.991898	6592.661660	25.737447
175.297011	6592.156062	25.742464
174.961390	6598.317069	25.747482
175.264446	6593.584784	25.752500
175.624797	6602.168546	25.757517
175.906356	6608.775846	25.762535
176.183305	6616.046807	25.767552
175.861024	6621.833224	25.772570
176.258385	6617.575470	25.777588
176.253301	6635.781737	25.782605
176.320779	6640.197009	25.787623
176.701053	6651.719856	25.792640
176.797007	6668.698097	25.797658
176.945130	6671.389728	25.802676
177.287590	6685.390337	25.807693
177.087504	6694.686999	25.812711
177.395800	6698.944597	25.817728
177.459651	6718.955341	25.822746
178.002660	6723.504488	25.827764
178.310971	6734.792426	25.832781
178.444793	6745.981432	25.837799
178.467195	6750.927832	25.842816
178.374039	6769.242735	25.847834
178.649348	6769.534176	25.852852
178.885807	6782.929562	25.857869
179.069258	6790.044768	25.862887
179.386253	6800.652659	25.867904
179.578696	6815.668127	25.872922
179.742659	6823.045264	25.877940
180.033377	6830.168937	25.882957
180.247519	6839.432347	25.887975
180.533820	6848.119376	25.892992
180.851619	6864.611609	25.898010
180.774539	6859.970377	25.903028
180.858045	6878.961699	25.908045
181.177022	6883.473375	25.913063
181.308815	6885.248942	25.918080
181.256960	6910.370084	25.923098
181.393225	6913.041511	25.928116
181.443103	6926.349426	25.933133
182.037965	6936.945433	25.938151
182.422038	6934.691163	25.943168
182.158654	6937.100041	25.948186
182.241904	6961.524512	25.953204
182.767852	6967.708513	25.958221
183.146077	6972.018358	25.963239
183.393068	6983.827475	25.968256
182.883006	6995.957241	25.973274
183.487115	6992.560418	25.978292
184.033952	7009.594615	25.983309
183.887134	7012.875491	25.988327
183.901646	7025.475556	25.993344
184.074126	7032.510496	25.998362
184.214407	7043.411392	26.003380
184.238535	7042.981371	26.008397
184.611714	7056.746996	26.013415
184.747391	7076.854212	26.018432
184.824344	7090.562091	26.023450
185.285041	7094.000362	26.028468
185.529088	7101.434517	26.033485
185.555173	7113.347776	26.038503
185.467558	7123.356284	26.043520
185.799759	7138.227002	26.048538
185.917597	7155.511643	26.053556
186.257315	7160.269537	26.058573
185.910871	7167.717302	26.063591
186.514694	7182.024608	26.068608
186.330888	7198.744099	26.073626
187.017683	7202.405840	26.078644
186.952312	7212.843413	26.083661
187.147772	7232.107999	26.088679
187.500095	7242.464369	26.093696
187.721158	7245.390901	26.098714
187.886389	7255.593484	26.103732
188.136155	7268.924001	26.108749
188.014108	7272.283123	26.113767
188.338555	7282.350285	26.118784
188.597453	7295.600467	26.123802
188.933989	7305.877265	26.128820
188.984767	7313.325998	26.133837
189.055990	7326.517208	26.138855
189.187441	7341.394284	26.143872
189.074453	7348.666641	26.148890
189.459349	7362.762142	26.153908
189.622476	7377.391198	26.158925
189.988291	7403.341004	26.163943
190.644336	7414.410721	26.168960
190.607279	7421.911143	26.173978
190.826999	7429.882772	26.178996
190.866395	7436.780866	26.184013
191.175096	7457.600126	26.189031
191.563480	7460.449968	26.194048
191.415591	7471.210000	26.199066
191.729918	7470.939711	26.204084
192.094182	7474.759373	26.209101
192.412168	7498.617408	26.214119
192.680764	7509.381669	26.219136
192.857147	7520.820196	26.224154
192.854417	7516.779608	26.229172
193.476363	7531.892540	26.234189
193.397629	7545.950318	26.239207
193.501146	7548.251285	26.244224
193.462007	7553.924181	26.249242
193.811409	7563.728714	26.254260
194.152617	7572.593748	26.259277
193.842196	7590.965602	26.264295
194.126391	7598.557833	26.269312
194.184963	7604.755287	26.274330
194.382469	7624.007334	26.279348
194.795245	7633.063235	26.284365
194.806562	7654.835370	26.289383
195.473582	7660.031458	26.294400
195.307606	7675.728869	26.299418
195.603457	7684.399012	26.304436
195.596311	7694.111091	26.309453
195.813543	7709.211803	26.314471
196.251614	7716.669481	26.319488
196.165717	7741.200408	26.324506
196.511034	7752.981987	26.329524
196.828127	7756.395526	26.334541
196.844953	7767.363547	26.339559
196.952455	7780.735663	26.344576
197.237261	7799.952119	26.349594
197.865426	7806.720231	26.354612
197.823001	7819.178220	26.359629
197.937789	7828.675531	26.364647
198.132272	7845.424741	26.369664
198.394397	7856.739547	26.374682
198.336237	7859.166906	26.379700
198.823521	7875.598768	26.384717
198.966324	7882.761807	26.389735
199.286310	7896.227003	26.394752
199.584367	7905.847181	26.399770
199.479310	7906.444482	26.404788
200.061639	7918.691011	26.409805
200.120282	7932.879101	26.414823
200.347061	7930.178951	26.419840
200.212314	7940.312096	26.424858
200.764315	7944.121389	26.429876
200.943507	7951.670232	26.434893
200.596389	7962.550157	26.439911
201.029382	7977.194240	26.444928
201.372831	7976.471078	26.449946
201.527558	7993.160353	26.454964
201.698184	7999.444568	26.459981
201.820198	8014.816170	26.464999
202.055446	8030.053234	26.470016
202.039959	8037.193775	26.475034
202.271085	8049.763762	26.480052
202.806265	8054.068219	26.485069
202.965215	8072.370176	26.490087
203.023077	8085.339867	26.495104
203.206441	8100.806114	26.500122
203.452394	8113.032855	26.505140
203.702080	8128.062526	26.510157
203.531134	8150.905642	26.515175
203.767472	8160.327253	26.520192
204.167427	8167.898428	26.525210
203.942393	8181.471313	26.530228
204.451073	8197.925367	26.535245
204.759459	8211.720950	26.540263
204.815638	8231.908178	26.545280
205.398386	8244.205372	26.550298
205.383625	8260.804626	26.555316
205.790258	8274.493308	26.560333
205.905131	8292.174120	26.565351
206.089429	8302.355353	26.570368
206.703928	8314.268764	26.575386
206.658774	8323.194687	26.580404
206.865274	8334.755285	26.585421
207.252581	8346.243366	26.590439
207.351202	8351.503440	26.595456
207.461257	8373.687167	26.600474
207.409658	8378.389867	26.605492
207.575324	8387.118622	26.610509
207.787648	8409.494742	26.615527
208.331273	8427.320044	26.620544
208.316622	8446.265212	26.625562
208.716828	8463.623658	26.630580
208.860393	8469.062997	26.635597
208.970077	8487.710898	26.640615
209.175362	8488.442716	26.645632
209.330639	8512.390693	26.650650
209.636860	8533.312584	26.655668
210.300636	8535.904766	26.660685
210.508635	8553.460737	26.665703
210.408643	8551.831456	26.670720
210.982588	8567.435808	26.675738
211.064169	8573.835198	26.680756
211.133419	8583.930423	26.685773
211.065692	8605.911804	26.690791
211.463199	8610.708381	26.695808
211.803429	8625.446440	26.700826
211.849564	8640.056937	26.705844
212.228966	8642.557925	26.710861
212.440312	8651.926873	26.715879
212.537571	8664.196216	26.720896
213.019768	8675.259202	26.725914
212.933878	8684.147479	26.730932
213.305359	8695.006817	26.735949
213.315046	8701.003921	26.740967
213.819221	8706.623628	26.745984
214.152771	8726.600611	26.751002
214.156729	8741.274625	26.756020
214.515220	8731.266895	26.761037
214.599884	8743.269901	26.766055
214.850511	8751.527724	26.771072
214.986923	8760.801121	26.776090
215.236554	8766.343905	26.781108
215.570322	8781.398822	26.786125
215.691547	8799.009663	26.791143
215.822293	8794.370117	26.796160
215.648165	8814.998182	26.801178
215.559591	8824.543648	26.806196
216.144078	8831.931485	26.811213
216.256947	8850.853932	26.816231
216.368735	8884.558717	26.821248
216.405500	8881.111518	26.826266
216.887421	8901.734780	26.831284
217.174508	8920.301653	26.836301
217.438221	8936.838943	26.841319
217.854947	8957.993425	26.846336
217.929156	8965.022397	26.851354
218.039982	8976.478409	26.856372
218.694878	8990.043484	26.861389
218.662976	9003.267831	26.866407
219.122401	9022.467673	26.871424
219.640729	9019.497530	26.876442
219.523379	9049.793947	26.881460
219.542614	9053.595374	26.886477
220.036501	9060.785960	26.891495
220.282782	9075.397018	26.896512
220.168556	9079.333019	26.901530
220.295235	9099.093388	26.906548
220.513996	9103.065633	26.911565
220.434175	9134.893899	26.916583
221.013609	9145.787228	26.921600
221.770904	9155.683417	26.926618
221.647584	9170.532415	26.931636
221.909647	9183.963421	26.936653
221.848904	9195.607467	26.941671
222.006663	9217.607921	26.946688
222.486232	9217.289626	26.951706
222.446973	9249.721090	26.956724
223.066834	9254.012566	26.961741
222.695371	9267.719687	26.966759
223.207522	9278.405781	26.971776
223.765344	9296.810641	26.976794
223.557281	9310.198566	26.981812
224.376521	9325.664098	26.986829
224.390204	9329.232811	26.991847
224.668765	9346.690074	26.996864
225.428694	9354.129570	27.001882
224.938661	9371.334698	27.006900
225.258244	9374.141945	27.011917
225.434297	9387.589730	27.016935
225.614539	9411.058201	27.021952
225.948395	9406.503505	27.026970
225.892613	9439.888242	27.031988
226.377976	9444.046124	27.037005
226.851922	9464.838600	27.042023
227.303508	9471.944411	27.047040
227.370991	9471.037100	27.052058
226.901063	9490.597714	27.057076
227.154674	9505.972038	27.062093
227.436003	9517.259593	27.067111
227.343229	9534.124792	27.072128
227.814821	9556.205934	27.077146
228.049324	9567.437708	27.082164
228.264029	9586.597538	27.087181
228.498210	9600.399466	27.092199
228.663220	9630.160046	27.097216
229.386833	9633.027177	27.102234
229.339202	9648.183591	27.107252
229.470009	9662.696379	27.112269
229.864252	9669.606020	27.117287
229.780395	9684.253488	27.122304
230.247315	9694.296491	27.127322
230.648214	9709.935231	27.132340
230.745321	9723.597698	27.137357
231.179013	9731.849381	27.142375
230.822656	9750.186357	27.147392
231.534207	9759.007056	27.152410
231.562428	9776.507097	27.157428
231.715141	9791.714335	27.162445
232.292938	9807.448583	27.167463
232.305042	9823.590359	27.172480
232.692894	9837.946192	27.177498
232.795401	9843.165034	27.182516
233.101193	9855.610884	27.187533
233.514414	9886.842226	27.192551
233.406497	9893.334904	27.197568
234.095937	9904.890290	27.202586
234.242530	9919.290296	27.207604
234.056320	9937.733412	27.212621
234.495060	9941.680850	27.217639
234.353871	9967.003255	27.222656
234.657974	9977.911791	27.227674
235.007878	10008.903819	27.232692
235.348284	10024.233400	27.237709
235.802862	10034.168011	27.242727
235.693267	10050.862653	27.247744
236.167522	10052.041801	27.252762
236.282190	10081.084778	27.257780
236.821220	10098.852419	27.262797
237.231969	10114.076331	27.267815
237.345510	10131.680164	27.272832
237.701261	10140.935677	27.277850
237.789190	10153.062220	27.282868
238.112544	10160.141023	27.287885
238.539284	10175.911877	27.292903
238.640503	10195.481634	27.297920
238.947233	10192.162405	27.302938
239.126460	10210.627480	27.307956
239.442269	10216.539227	27.312973
239.531310	10236.073046	27.317991
239.907069	10241.479688	27.323008
240.076647	10250.574973	27.328026
240.202590	10258.998242	27.333044
240.760578	10282.737011	27.338061
241.174855	10285.785320	27.343079
241.072136	10303.701050	27.348096
241.645374	10298.442413	27.353114
241.438353	10318.480530	27.358132
241.761046	10329.888398	27.363149
241.976167	10334.344573	27.368167
241.962723	10355.365954	27.373184
242.279565	10357.296003	27.378202
243.022377	10375.148811	27.383220
242.656268	10397.968418	27.388237
242.792762	10400.485598	27.393255
242.560850	10421.304466	27.398272
242.902762	10439.854794	27.403290
243.367812	10469.108715	27.408308
243.635615	10477.326725	27.413325
244.351158	10491.527532	27.418343
244.139638	10508.576401	27.423360
244.393943	10521.112857	27.428378
244.710069	10534.324815	27.433396
244.818306	10560.407800	27.438413
245.414047	10574.785313	27.443431
245.627055	10584.117086	27.448448
245.837024	10592.464192	27.453466
246.009856	10601.480200	27.458484
246.313140	10618.985303	27.463501
246.341893	10624.942149	27.468519
246.355072	10647.708957	27.473536
247.203326	10668.898826	27.478554
247.453132	10679.743655	27.483572
247.369257	10693.128901	27.488589
247.990685	10697.875158	27.493607
248.299612	10728.707451	27.498624
248.531128	10737.404893	27.503642
248.496602	10741.319284	27.508660
248.951635	10752.334089	27.513677
248.985920	10764.987271	27.518695
249.074894	10788.089707	27.523712
249.121528	10804.504784	27.528730
249.637781	10808.629719	27.533748
250.056326	10831.427976	27.538765
250.335681	10846.947778	27.543783
250.464456	10862.560648	27.548800
250.415421	10874.522819	27.553818
250.855876	10899.938508	27.558836
250.887101	10917.214958	27.563853
251.401177	10933.834789	27.568871
251.289988	10960.975760	27.573888
251.799418	10980.899192	27.578906
252.371355	10990.291771	27.583924
252.795312	11020.039260	27.588941
253.254374	11025.369930	27.593959
253.167342	11039.501110	27.598976
253.561816	11047.547964	27.603994
253.920530	11058.641190	27.609012
253.994805	11079.905408	27.614029
254.339261	11090.413573	27.619047
254.365768	11109.209746	27.624064
254.496472	11112.198414	27.629082
254.907219	11130.928101	27.634100
255.008758	11152.658614	27.639117
255.220813	11162.205542	27.644135
255.533637	11190.404533	27.649152
255.722958	11202.837951	27.654170
256.159490	11225.640186	27.659188
256.102042	11243.941267	27.664205
256.594279	11255.266304	27.669223
256.963218	11273.525881	27.674240
257.194063	11283.158341	27.679258
257.553398	11302.439367	27.684276
257.184114	11318.073801	27.689293
257.545171	11340.543815	27.694311
257.990635	11365.605695	27.699328
258.786263	11382.803877	27.704346
258.777559	11395.416854	27.709364
258.904144	11413.067212	27.714381
259.586470	11419.566090	27.719399
259.535286	11445.665805	27.724416
260.145000	11452.949697	27.729434
260.469987	11465.185207	27.734452
260.527048	11484.078014	27.739469
260.629637	11486.809059	27.744487
260.314465	11500.988954	27.749504
261.042663	11521.677583	27.754522
261.355917	11535.342247	27.759540
261.392150	11562.723079	27.764557
262.181853	11569.546218	27.769575
262.387531	11581.592088	27.774592
262.486503	11589.634944	27.779610
262.682286	11592.581916	27.784628
262.933430	11623.475255	27.789645
263.038253	11619.173788	27.794663
263.139798	11645.609833	27.799680
263.472149	11654.257170	27.804698
264.119830	11668.232678	27.809716
264.248646	11682.071595	27.814733
264.158029	11700.368843	27.819751
264.389866	11723.443734	27.824768
264.866666	11737.225023	27.829786
265.253357	11753.824488	27.834804
265.159615	11775.374745	27.839821
265.568212	11786.681629	27.844839
265.482021	11819.664864	27.849856
265.671075	11829.443091	27.854874
266.169743	11857.487661	27.859892
266.237015	11887.848161	27.864909
266.765548	11901.533050	27.869927
267.122018	11922.087731	27.874944
267.298202	11940.918127	27.879962
267.611144	11958.650325	27.884980
267.968805	11984.958309	27.889997
268.434211	12001.858280	27.895015
268.678594	12018.256070	27.900032
268.776622	12033.972621	27.905050
269.565475	12046.410571	27.910068
269.233895	12077.111739	27.915085
269.702053	12091.510407	27.920103
270.278628	12099.011314	27.925120
270.354421	12124.103695	27.930138
270.541853	12134.567572	27.935156
271.067382	12160.704247	27.940173
271.253793	12172.570361	27.945191
271.624893	12182.500249	27.950208
271.774087	12216.157805	27.955226
272.019224	12219.071883	27.960244
272.417175	12243.570817	27.965261
272.665593	12257.899827	27.970279
272.810778	12274.967045	27.975296
272.764948	12297.842985	27.980314
273.325715	12306.590627	27.985332
273.459114	12337.172011	27.990349
273.653614	12350.840082	27.995367
274.126725	12365.200290	28.000384
274.146902	12390.885934	28.005402
274.507554	12411.664700	28.010420
274.880992	12429.558388	28.015437
275.015950	12449.532568	28.020455
275.740789	12470.421714	28.025472
275.731686	12482.760747	28.030490
276.377816	12497.785520	28.035508
276.253849	12514.503545	28.040525
276.733092	12526.241906	28.045543
277.159170	12550.149473	28.050560
277.116463	12576.195740	28.055578
277.598875	12572.611740	28.060596
277.668546	12591.977359	28.065613
277.994897	12612.246988	28.070631
278.512929	12634.160280	28.075648
278.674477	12656.603120	28.080666
279.038679	12669.445898	28.085684
279.037774	12693.853161	28.090701
279.306880	12698.070919	28.095719
279.908005	12726.299679	28.100736
279.736222	12746.833800	28.105754
280.134613	12753.579728	28.110772
280.436997	12776.850119	28.115789
280.685331	12783.237460	28.120807
281.171378	12803.220174	28.125824
281.322365	12811.905929	28.130842
281.618633	12832.644718	28.135860
281.702604	12845.885198	28.140877
281.919667	12860.030103	28.145895
282.019899	12879.485966	28.150912
282.662046	12900.808545	28.155930
282.543675	12921.735542	28.160948
283.088471	12954.350332	28.165965
283.125315	12973.244637	28.170983
283.610995	12991.405489	28.176000
283.663499	13008.513151	28.181018
283.987801	13022.843487	28.186036
284.486753	13063.047829	28.191053
284.685433	13078.225264	28.196071
284.920477	13093.226486	28.201088
285.032022	13114.243997	28.206106
285.400280	13145.749912	28.211124
285.570624	13170.945714	28.216141
286.017128	13201.125756	28.221159
286.290045	13212.082113	28.226176
286.559111	13243.581623	28.231194
287.129261	13267.890697	28.236212
287.276251	13298.064126	28.241229
287.701936	13316.812597	28.246247
288.333147	13336.719450	28.251264
288.167583	13355.930062	28.256282
288.798546	13370.342100	28.261300
289.061034	13403.661906	28.266317
289.389496	13410.974831	28.271335
289.683864	13430.833493	28.276352
290.034014	13446.353823	28.281370
289.938582	13465.695669	28.286388
290.562444	13484.691167	28.291405
290.895825	13505.500671	28.296423
291.319738	13523.318013	28.301440
291.379099	13542.553581	28.306458
291.806305	13551.644844	28.311476
292.138240	13577.921180	28.316493
292.392915	13593.917657	28.321511
293.017691	13613.882655	28.326528
293.076267	13627.626627	28.331546
293.415768	13649.903814	28.336564
293.448664	13666.424588	28.341581
294.085452	13683.135003	28.346599
294.616235	13696.331349	28.351616
294.510199	13719.755302	28.356634
294.536448	13731.164303	28.361652
294.884654	13745.027209	28.366669
295.481835	13772.683385	28.371687
295.544962	13780.325400	28.376704
295.523768	13802.719271	28.381722
296.001362	13826.418265	28.386740
296.248021	13843.688907	28.391757
296.412591	13873.604694	28.396775
296.763774	13892.220134	28.401792
296.863892	13917.914271	28.406810
297.257523	13940.887571	28.411828
297.371660	13962.941465	28.416845
297.991939	13987.013069	28.421863
298.391290	14015.032187	28.426880
298.451286	14033.646008	28.431898
298.799471	14055.698086	28.436916
298.774798	14081.197240	28.441933
299.350743	14106.191790	28.446951
299.882234	14119.072510	28.451968
300.224855	14144.981614	28.456986
300.370432	14162.164162	28.462004
300.632923	14176.463998	28.467021
300.778994	14206.999039	28.472039
301.185317	14215.092768	28.477056
301.314267	14242.630329	28.482074
302.010803	14267.678838	28.487092
302.040968	14281.102445	28.492109
302.504530	14304.646327	28.497127
302.640354	14321.432621	28.502144
303.394513	14353.031679	28.507162
303.498633	14362.167627	28.512180
303.772784	14381.837803	28.517197
304.150431	14406.415353	28.522215
304.536413	14419.246433	28.527232
304.764287	14438.153325	28.532250
304.726633	14446.806216	28.537268
305.362313	14480.363158	28.542285
305.411266	14492.173304	28.547303
306.081368	14511.257333	28.552320
306.169188	14548.074179	28.557338
306.141235	14569.216211	28.562356
306.661491	14584.486595	28.567373
306.817513	14606.689423	28.572391
307.179983	14625.888079	28.577408
307.617087	14655.497113	28.582426
307.867463	14678.850621	28.587444
308.532312	14700.326422	28.592461
308.111388	14727.647631	28.597479
308.884168	14751.374177	28.602496
309.191953	14781.919547	28.607514
309.682090	14809.069734	28.612532
309.653533	14838.057186	28.617549
310.085439	14855.384999	28.622567
310.442802	14885.452192	28.627584
310.601737	14909.755143	28.632602
310.774768	14932.622075	28.637620
311.418772	14943.366549	28.642637
311.682331	14969.475495	28.647655
312.341941	14992.038884	28.652672
312.599255	15018.224673	28.657690
312.604024	15041.563407	28.662708
313.155406	15060.117047	28.667725
313.446311	15083.123608	28.672743
313.829322	15102.578504	28.677760
314.080215	15135.404147	28.682778
314.202462	15158.171922	28.687796
314.651345	15173.460275	28.692813
314.849451	15204.408811	28.697831
315.385101	15214.412422	28.702848
315.602648	15244.366274	28.707866
315.502124	15279.006381	28.712884
316.130651	15293.767679	28.717901
316.379342	15323.726251	28.722919
316.474771	15348.974567	28.727936
316.735273	15381.211681	28.732954
317.102216	15403.063404	28.737972
317.538869	15426.129663	28.742989
317.649563	15448.034211	28.748007
317.975476	15473.391870	28.753024
318.598993	15499.473579	28.758042
318.739830	15539.224438	28.763060
319.195881	15554.540398	28.768077
319.570748	15583.885843	28.773095
319.819585	15603.501234	28.778112
319.976875	15632.182838	28.783130
320.171166	15668.201886	28.788148
320.736090	15685.190622	28.793165
321.168226	15713.456608	28.798183
321.514356	15724.292401	28.803200
321.475865	15743.820292	28.808218
322.095605	15779.406533	28.813236
322.246924	15799.697502	28.818253
322.515491	15820.102779	28.823271
322.728269	15845.484968	28.828288
323.233134	15871.295198	28.833306
323.898357	15887.636723	28.838324
324.232940	15909.803617	28.843341
324.341265	15949.513041	28.848359
324.413044	15963.417703	28.853376
325.016314	15987.011260	28.858394
325.415236	16015.365013	28.863412
325.861123	16032.420080	28.868429
325.857920	16061.857063	28.873447
326.406929	16078.813898	28.878464
326.763244	16112.540645	28.883482
326.565758	16135.808162	28.888500
326.938195	16153.774998	28.893517
327.280182	16185.122650	28.898535
327.902413	16220.046043	28.903552
328.513973	16249.345954	28.908570
328.374070	16270.899045	28.913588
328.939192	16293.320848	28.918605
328.838552	16329.681072	28.923623
329.391857	16344.486550	28.928640
330.025998	16379.152530	28.933658
330.231887	16404.201738	28.938676
330.707673	16426.988282	28.943693
330.804278	16454.824669	28.948711
331.215253	16473.869132	28.953728
331.876483	16503.606998	28.958746
331.733675	16520.688385	28.963764
332.102698	16551.713390	28.968781
332.216244	16582.491039	28.973799
332.834484	16610.659706	28.978816
332.977295	16629.146209	28.983834
333.630062	16675.824829	28.988852
334.233456	16703.724324	28.993869
334.058540	16730.431824	28.998887
334.447720	16760.755971	29.003904
334.904569	16778.621730	29.008922
335.083833	16815.829733	29.013940
335.736239	16839.053407	29.018957
336.340044	16872.568997	29.023975
336.418480	16888.368421	29.028992
336.904555	16918.437587	29.034010
337.030213	16945.335194	29.039028
337.415766	16965.799167	29.044045
337.440416	17003.540282	29.049063
338.000177	17022.182951	29.054080
338.505539	17053.721208	29.059098
338.777951	17070.336898	29.064116
339.323069	17104.787553	29.069133
339.438552	17132.129218	29.074151
339.795594	17154.391944	29.079168
340.203038	17182.894535	29.084186
340.381382	17217.030126	29.089204
340.595096	17230.307013	29.094221
341.643512	17253.011155	29.099239
341.388877	17283.076888	29.104256
341.820855	17290.135033	29.109274
342.014658	17321.400350	29.114292
342.368280	17349.873715	29.119309
343.043068	17386.187110	29.124327
343.485564	17405.612910	29.129344
343.649147	17420.894048	29.134362
343.667806	17449.855923	29.139380
344.366901	17463.897143	29.144397
344.373172	17481.881513	29.149415
344.631064	17505.720554	29.154432
345.041644	17530.754953	29.159450
345.258001	17565.731727	29.164468
345.690229	17584.723420	29.169485
346.069032	17608.019306	29.174503
346.075238	17643.262881	29.179520
346.547245	17667.694002	29.184538
346.557773	17708.635299	29.189556
347.218186	17730.269968	29.194573
347.466239	17757.737050	29.199591
347.697643	17788.959327	29.204608
348.462485	17816.048623	29.209626
348.599466	17856.711410	29.214644
349.259918	17884.278326	29.219661
349.573624	17911.470009	29.224679
350.214398	17936.222494	29.229696
350.628563	17959.892313	29.234714
350.437561	17991.124224	29.239732
351.331524	18015.622356	29.244749
351.410728	18043.602739	29.249767
351.660082	18066.338243	29.254784
352.210872	18092.090554	29.259802
352.548182	18127.321048	29.264820
352.704115	18152.566713	29.269837
353.095034	18185.274533	29.274855
353.118128	18213.504017	29.279872
353.752161	18241.486221	29.284890
354.294057	18271.978342	29.289908
354.727245	18300.655439	29.294925
354.832817	18334.564326	29.299943
355.047176	18370.136717	29.304960
355.995973	18395.700736	29.309978
356.221043	18428.908767	29.314996
356.346988	18451.619829	29.320013
356.410890	18487.512931	29.325031
356.652010	18508.961443	29.330048
357.086573	18547.317339	29.335066
357.636277	18573.133636	29.340084
357.737740	18604.560790	29.345101
358.154434	18643.759929	29.350119
358.621769	18673.316704	29.355136
359.129201	18708.749041	29.360154
359.461048	18736.305464	29.365172
359.883898	18764.700566	29.370189
360.247617	18794.671774	29.375207
360.631654	18832.398054	29.380224
360.808158	18860.193790	29.385242
360.974496	18889.052544	29.390260
361.491416	18916.656045	29.395277
362.100548	18956.387953	29.400295
362.209116	18988.812826	29.405312
363.033033	19016.058808	29.410330
363.213173	19047.935554	29.415348
363.550888	19073.191844	29.420365
363.935210	19099.868700	29.425383
364.369520	19132.129066	29.430400
364.720308	19153.295758	29.435418
364.933962	19189.874296	29.440436
365.519671	19216.096468	29.445453
366.133159	19246.073471	29.450471
366.129196	19278.105788	29.455488
366.184697	19306.830891	29.460506
366.604422	19337.223778	29.465524
367.347243	19371.470586	29.470541
367.547047	19402.782535	29.475559
367.647550	19416.015471	29.480576
368.812574	19453.968107	29.485594
368.468413	19479.521270	29.490612
368.864460	19512.104156	29.495629
369.394865	19529.483923	29.500647
369.743484	19561.859510	29.505664
370.353639	19591.249992	29.510682
370.532606	19617.138380	29.515700
371.038045	19641.851057	29.520717
371.391596	19669.721300	29.525735
371.471212	19701.178912	29.530752
371.966512	19723.050161	29.535770
371.612207	19750.039462	29.540788
371.887802	19791.651233	29.545805
372.651190	19818.636142	29.550823
373.132186	19862.913711	29.555840
373.361585	19897.570404	29.560858
373.474721	19938.645623	29.565876
374.133366	19971.504047	29.570893
374.549405	20008.020821	29.575911
375.005748	20042.515860	29.580928
375.513265	20077.015580	29.585946
375.600506	20111.214738	29.590964
376.272701	20139.042055	29.595981
376.649865	20172.595680	29.600999
376.780195	20206.908301	29.606016
377.009642	20240.624180	29.611034
377.767871	20277.327948	29.616052
377.914607	20316.945503	29.621069
378.320292	20355.347381	29.626087
379.092622	20400.048080	29.631104
379.458802	20431.386156	29.636122
379.913487	20470.077542	29.641140
380.177428	20495.410407	29.646157
380.662533	20530.224031	29.651175
380.703269	20562.794817	29.656192
381.217379	20592.062843	29.661210
381.173384	20623.433882	29.666228
381.588161	20668.292291	29.671245
382.257013	20700.708053	29.676263
382.502043	20741.600012	29.681280
383.199357	20771.275577	29.686298
383.317668	20809.723356	29.691316
383.618634	20855.661509	29.696333
384.350560	20891.921940	29.701351
384.786222	20931.640799	29.706368
385.121969	20957.057787	29.711386
385.757264	21006.722354	29.716404
385.998149	21035.142934	29.721421
386.271054	21057.555985	29.726439
386.719562	21096.003149	29.731456
387.279969	21132.069742	29.736474
388.013990	21159.459164	29.741492
387.976199	21188.700793	29.746509
388.399581	21224.087661	29.751527
388.637287	21261.228639	29.756544
389.090373	21294.386854	29.761562
389.993490	21326.646902	29.766580
389.876447	21351.219130	29.771597
390.484662	21386.552064	29.776615
390.677230	21424.894631	29.781632
391.460198	21450.994118	29.786650
391.677014	21485.169046	29.791668
392.111139	21519.859715	29.796685
392.036178	21542.921756	29.801703
392.661666	21587.408045	29.806720
393.126868	21616.483058	29.811738
393.600350	21638.423046	29.816756
393.880906	21662.901789	29.821773
394.350221	21685.897700	29.826791
394.420211	21726.566371	29.831808
394.768131	21751.230551	29.836826
395.105252	21777.577230	29.841844
395.188035	21820.714704	29.846861
395.894490	21856.614414	29.851879
396.246489	21896.468376	29.856896
396.677682	21924.196957	29.861914
397.183630	21963.881609	29.866932
397.215162	21999.666139	29.871949
397.914357	22023.763816	29.876967
398.155299	22065.809176	29.881984
398.887148	22108.978306	29.887002
399.329165	22139.270932	29.892020
399.274863	22177.546206	29.897037
400.176674	22210.376600	29.902055
400.454050	22248.303072	29.907072
401.009666	22275.191205	29.912090
401.516789	22306.554415	29.917108
401.349352	22351.166621	29.922125
402.297314	22374.808715	29.927143
402.335224	22418.396840	29.932160
402.832744	22452.485236	29.937178
403.123704	22490.877644	29.942196
403.421818	22534.450543	29.947213
403.996075	22567.547680	29.952231
404.043891	22605.460240	29.957248
404.732589	22647.177619	29.962266
405.309300	22691.863599	29.967284
405.773977	22726.551596	29.972301
406.031981	22759.123559	29.977319
406.093629	22801.495554	29.982336
406.424536	22838.814460	29.987354
407.073793	22882.977664	29.992372
407.247225	22933.502975	29.997389
407.797814	22970.699252	30.002407
408.201927	23008.740025	30.007424
408.735454	23048.371973	30.012442
409.077406	23085.240955	30.017460
409.552426	23137.381473	30.022477
410.195016	23159.991764	30.027495
410.434638	23202.785394	30.032512
410.426749	23251.241950	30.037530
411.081632	23291.891719	30.042548
411.514900	23331.173421	30.047565
412.231538	23375.320844	30.052583
412.503611	23405.901108	30.057600
413.431372	23453.996749	30.062618
413.624053	23491.521787	30.067636
413.922554	23532.215229	30.072653
414.782033	23567.828658	30.077671
414.686834	23608.223723	30.082688
415.642302	23650.185789	30.087706
415.778169	23672.199867	30.092724
416.180974	23706.254692	30.097741
416.493859	23746.244873	30.102759
416.884976	23780.118395	30.107776
417.435990	23810.314343	30.112794
418.211237	23848.229072	30.117812
418.062992	23891.053333	30.122829
418.444473	23912.081297	30.127847
418.751779	23958.524869	30.132864
419.545160	24003.660127	30.137882
419.973683	24042.836543	30.142900
420.243708	24074.966411	30.147917
420.360839	24114.115907	30.152935
421.076373	24156.040785	30.157952
421.219331	24190.440470	30.162970
421.776120	24214.038596	30.167988
422.290464	24268.343488	30.173005
422.639606	24287.885512	30.178023
423.248820	24325.081452	30.183040
423.435070	24358.785817	30.188058
424.134293	24387.310027	30.193076
424.070789	24428.346373	30.198093
424.751353	24451.571498	30.203111
425.094554	24495.855725	30.208128
425.183501	24535.907837	30.213146
425.712785	24572.345766	30.218164
426.319720	24614.762584	30.223181
426.273389	24651.436168	30.228199
426.591578	24706.556604	30.233216
427.288187	24746.330687	30.238234
427.701200	24800.286351	30.243252
428.379925	24841.137766	30.248269
428.522515	24886.781409	30.253287
429.095571	24935.075204	30.258304
429.675761	24968.036360	30.263322
430.039145	25001.530788	30.268340
430.578478	25058.380753	30.273357
431.267186	25088.070441	30.278375
431.358394	25128.319291	30.283392
431.821693	25171.037852	30.288410
432.078796	25212.341567	30.293428
432.668166	25265.942228	30.298445
432.899522	25311.193741	30.303463
433.299033	25353.840523	30.308480
433.979107	25399.318983	30.313498
434.610009	25437.979793	30.318516
434.814422	25481.434747	30.323533
435.479552	25516.115143	30.328551
435.820796	25559.858509	30.333568
436.133935	25605.622424	30.338586
436.610600	25648.194545	30.343604
437.118740	25703.212117	30.348621
437.814898	25748.037890	30.353639
438.074285	25786.719640	30.358656
438.349538	25834.367040	30.363674
439.188258	25867.175415	30.368692
439.281158	25923.756466	30.373709
440.106932	25952.477959	30.378727
440.271723	25996.793431	30.383744
440.734926	26030.754256	30.388762
441.662460	26069.951262	30.393780
441.738324	26109.199580	30.398797
441.932657	26155.052869	30.403815
442.732416	26199.629574	30.408832
442.815728	26242.403601	30.413850
443.464648	26288.786401	30.418868
444.011586	26338.004066	30.423885
444.174413	26364.194482	30.428903
444.571534	26420.880956	30.433920
445.260309	26462.536745	30.438938
445.749749	26495.457732	30.443956
446.238215	26548.748952	30.448973
446.887991	26589.374597	30.453991
447.409603	26626.291459	30.459008
447.649574	26671.702672	30.464026
448.122245	26702.401894	30.469044
448.699639	26741.288469	30.474061
449.048309	26785.867597	30.479079
449.347932	26819.084293	30.484096
449.798763	26861.340678	30.489114
450.727017	26889.977930	30.494132
450.804483	26932.887054	30.499149
451.208067	26970.252811	30.504167
451.475915	26999.549847	30.509184
451.699428	27040.830954	30.514202
452.334735	27085.157271	30.519220
452.677079	27126.337775	30.524237
453.017731	27165.976448	30.529255
453.741086	27206.655009	30.534272
453.701897	27255.600120	30.539290
454.375075	27276.465821	30.544308
455.139909	27330.594347	30.549325
455.336364	27381.873023	30.554343
455.845036	27413.869699	30.559360
456.434775	27467.103223	30.564378
456.697743	27503.177320	30.569396
457.032803	27553.587771	30.574413
457.214293	27600.527142	30.579431
457.917940	27643.169029	30.584448
458.588824	27693.501944	30.589466
459.155950	27739.711254	30.594484
459.442861	27784.460257	30.599501
459.835841	27829.148501	30.604519
460.273806	27873.197734	30.609536
460.835001	27927.637849	30.614554
461.138183	27973.054705	30.619572
461.670230	28018.960430	30.624589
462.482409	28074.429818	30.629607
462.884523	28116.930304	30.634624
463.245215	28173.083784	30.639642
463.885775	28205.914342	30.644660
464.012925	28254.007777	30.649677
464.620234	28302.576024	30.654695
465.157206	28346.149354	30.659712
465.606808	28392.871570	30.664730
466.381531	28434.385200	30.669748
466.782815	28485.419657	30.674765
467.194589	28523.185188	30.679783
467.633293	28569.220543	30.684800
468.094068	28613.318365	30.689818
468.390354	28662.271185	30.694836
468.983579	28711.398845	30.699853
469.303443	28760.329243	30.704871
470.282684	28795.161993	30.709888
470.679725	28838.416959	30.714906
471.039187	28880.780331	30.719924
471.663467	28925.232470	30.724941
472.476856	28982.442391	30.729959
472.586330	29017.057774	30.734976
472.767947	29059.063789	30.739994
473.178361	29099.365310	30.745012
473.704458	29155.312263	30.750029
474.190577	29201.455389	30.755047
475.141341	29248.948079	30.760064
475.273523	29292.352943	30.765082
475.691182	29332.957198	30.770100
475.938523	29379.561635	30.775117
476.274959	29418.510014	30.780135
477.022056	29460.738014	30.785152
477.511421	29517.330138	30.790170
477.963807	29564.117795	30.795188
478.391897	29609.367002	30.800205
478.846299	29661.982671	30.805223
479.339342	29705.660587	30.810240
479.925736	29751.384685	30.815258
480.225801	29805.029963	30.820276
481.088741	29855.982874	30.825293
481.327100	29898.500054	30.830311
481.665448	29946.501156	30.835328
482.109781	29983.063231	30.840346
482.842730	30022.140285	30.845364
483.083571	30068.911651	30.850381
483.589650	30125.104583	30.855399
484.096993	30159.488892	30.860416
484.579474	30203.966004	30.865434
484.984344	30253.695768	30.870452
485.156606	30293.657645	30.875469
485.782920	30342.708161	30.880487
486.319033	30385.982524	30.885504
486.722332	30443.361877	30.890522
487.400190	30479.319328	30.895540
487.982578	30529.894309	30.900557
488.139203	30588.709738	30.905575
488.712366	30635.670550	30.910592
489.272022	30681.369287	30.915610
489.733159	30736.211800	30.920628
490.218231	30784.963090	30.925645
490.820108	30837.716693	30.930663
491.279357	30890.555984	30.935680
491.927192	30946.956521	30.940698
492.249961	30996.802074	30.945716
493.099684	31038.094278	30.950733
493.075113	31095.934391	30.955751
494.037190	31147.564014	30.960768
494.534739	31190.884028	30.965786
494.828382	31238.142851	30.970804
495.193141	31296.365058	30.975821
495.538423	31352.618113	30.980839
496.254386	31401.777206	30.985856
496.874266	31456.704228	30.990874
497.539776	31508.861650	30.995892
497.856699	31549.852697	31.000909
497.897596	31612.810929	31.005927
498.668653	31658.933876	31.010944
499.355857	31720.425702	31.015962
499.387921	31772.126678	31.020980
500.200814	31821.366409	31.025997
500.361106	31887.657341	31.031015
501.312519	31935.623920	31.036032
501.921615	31996.939140	31.041050
501.994197	32051.599425	31.046068
502.645121	32104.898566	31.051085
503.185851	32163.038737	31.056103
503.878815	32217.975285	31.061120
504.071648	32273.401238	31.066138
504.921843	32323.502423	31.071156
505.756040	32377.108619	31.076173
506.239184	32442.446699	31.081191
506.343817	32481.860711	31.086208
507.228425	32537.937661	31.091226
507.588636	32588.166800	31.096244
508.497111	32626.734470	31.101261
508.818076	32681.749467	31.106279
509.224872	32728.380700	31.111296
509.875910	32781.934435	31.116314
510.176584	32824.182307	31.121332
510.990546	32864.522772	31.126349
511.436103	32928.780848	31.131367
511.787355	32971.874588	31.136384
512.214196	33021.070136	31.141402
512.691009	33069.107332	31.146420
513.410231	33120.242492	31.151437
513.709917	33177.335811	31.156455
514.286277	33217.853260	31.161472
514.679886	33282.955093	31.166490
515.078158	33323.519606	31.171508
515.888981	33373.825463	31.176525
516.487242	33421.338659	31.181543
516.688321	33469.729750	31.186560
517.440197	33519.444568	31.191578
517.750830	33571.586851	31.196596
518.465978	33612.266672	31.201613
518.274214	33665.923052	31.206631
518.812869	33715.880368	31.211648
519.848565	33768.617687	31.216666
520.409332	33823.003808	31.221684
520.919513	33864.563426	31.226701
521.304819	33919.514685	31.231719
521.474088	33958.466126	31.236736
522.380641	34023.730167	31.241754
522.918344	34071.115220	31.246772
523.180990	34113.605572	31.251789
523.631846	34187.470571	31.256807
524.203909	34230.216178	31.261824
524.739416	34286.934153	31.266842
525.186773	34351.518741	31.271860
526.067412	34397.289137	31.276877
526.570592	34453.525781	31.281895
526.679649	34501.478423	31.286912
527.266083	34562.646619	31.291930
527.617503	34621.537703	31.296948
528.269784	34681.096293	31.301965
528.828297	34749.900891	31.306983
529.367019	34806.215101	31.312000
530.057104	34868.398552	31.317018
530.500670	34930.949579	31.322036
531.200692	34979.695933	31.327053
531.597586	35046.876563	31.332071
532.225431	35089.760596	31.337088
532.752292	35159.102595	31.342106
533.358640	35210.058173	31.347124
534.234347	35275.628084	31.352141
534.470879	35339.306596	31.357159
535.202320	35391.678313	31.362176
535.837278	35442.433957	31.367194
536.070690	35511.500599	31.372212
537.185157	35566.335608	31.377229
537.867339	35619.309959	31.382247
537.811355	35661.113530	31.387264
538.730764	35710.257165	31.392282
539.183136	35770.672114	31.397300
539.844034	35818.010166	31.402317
540.365644	35881.184070	31.407335
540.899080	35935.282715	31.412352
541.442519	35989.095391	31.417370
541.839461	36041.653882	31.422388
542.289381	36094.343314	31.427405
542.679935	36153.896442	31.432423
543.453619	36212.719478	31.437440
543.994800	36261.417772	31.442458
544.339638	36311.898448	31.447476
545.205528	36370.846589	31.452493
545.502164	36433.937225	31.457511
546.255592	36484.860173	31.462528
546.844375	36542.530634	31.467546
547.007328	36591.807425	31.472564
547.981213	36650.612959	31.477581
548.443244	36712.116664	31.482599
548.861652	36765.925587	31.487616
549.501381	36817.309767	31.492634
550.155262	36869.969168	31.497652
550.777667	36924.290347	31.502669
550.840111	36979.344348	31.507687
551.432856	37037.053461	31.512704
552.202116	37089.151520	31.517722
552.353364	37152.633801	31.522740
552.846976	37194.721049	31.527757
553.401511	37248.060900	31.532775
553.779237	37308.245271	31.537792
554.866897	37358.827074	31.542810
555.016677	37412.818809	31.547828
555.821958	37470.280803	31.552845
556.001011	37529.168970	31.557863
556.760425	37576.780048	31.562880
557.376095	37638.401464	31.567898
557.931930	37699.671983	31.572916
558.485546	37754.025008	31.577933
559.240158	37806.329457	31.582951
559.432926	37872.090183	31.587968
560.432020	37931.407498	31.592986
560.713894	37981.851376	31.598004
561.361777	38049.160223	31.603021
561.971021	38091.300678	31.608039
562.316931	38158.568628	31.613056
562.840005	38214.660297	31.618074
563.427910	38282.984740	31.623092
563.920475	38346.088248	31.628109
564.756344	38402.466576	31.633127
565.064971	38462.007319	31.638144
565.888664	38524.313279	31.643162
566.525355	38592.397079	31.648180
566.992756	38647.973714	31.653197
567.624895	38710.379773	31.658215
568.030077	38766.725323	31.663232
568.848371	38825.497940	31.668250
568.866316	38897.334827	31.673268
569.521017	38951.497966	31.678285
570.575735	39016.279769	31.683303
571.028527	39085.665040	31.688320
571.676976	39144.629548	31.693338
572.191383	39212.538406	31.698356
573.110311	39268.779505	31.703373
573.558519	39329.767951	31.708391
574.109185	39389.260687	31.713408
574.443238	39447.067358	31.718426
575.194725	39511.543984	31.723444
575.996208	39573.565533	31.728461
576.502975	39633.843683	31.733479
576.829958	39695.724873	31.738496
577.965809	39749.232827	31.743514
578.365074	39815.529964	31.748532
578.926331	39868.660211	31.753549
579.753130	39921.881808	31.758567
579.836355	39980.418521	31.763584
580.800709	40037.843456	31.768602
581.423664	40114.212646	31.773620
581.768671	40161.287188	31.778637
582.233641	40234.026095	31.783655
583.008363	40285.751550	31.788672
583.923118	40345.303717	31.793690
584.239410	40408.232123	31.798708
584.599227	40464.924371	31.803725
585.161810	40518.656811	31.808743
585.262776	40596.595674	31.813760
586.235761	40652.465069	31.818778
586.819451	40719.513976	31.823796
587.072513	40783.509550	31.828813
588.195288	40847.647379	31.833831
588.533898	40902.826204	31.838848
589.546895	40958.449784	31.843866
589.637993	41023.546594	31.848884
590.409315	41098.213657	31.853901
591.395112	41151.881372	31.858919
591.617436	41211.341956	31.863936
592.388473	41265.372463	31.868954
592.810729	41317.054366	31.873972
592.987316	41371.311049	31.878989
593.696503	41428.792254	31.884007
594.196283	41496.286757	31.889024
595.442731	41548.333451	31.894042
595.743044	41603.387217	31.899060
596.326269	41662.210626	31.904077
596.742124	41716.424364	31.909095
597.164740	41786.056957	31.914112
597.985125	41843.053799	31.919130
598.401105	41906.242856	31.924148
598.836541	41969.536570	31.929165
599.639559	42034.701974	31.934183
599.803008	42095.097594	31.939200
600.577337	42161.052147	31.944218
601.473284	42235.886979	31.949236
601.842094	42303.606865	31.954253
602.483085	42369.563949	31.959271
602.860337	42441.628167	31.964288
603.734972	42516.663363	31.969306
604.138265	42587.674033	31.974324
604.822555	42649.374773	31.979341
605.448664	42713.817213	31.984359
605.983661	42796.053838	31.989376
606.860879	42860.166425	31.994394
607.577635	42930.060164	31.999412
608.023835	43001.887705	32.004429
608.891296	43056.375564	32.009447
609.324405	43131.665423	32.014464
609.957271	43199.991864	32.019482
610.672457	43269.621263	32.024500
611.339819	43341.642976	32.029517
611.781249	43399.019444	32.034535
612.514704	43469.000820	32.039552
612.860548	43545.608752	32.044570
613.557703	43621.738133	32.049588
614.248928	43690.006340	32.054605
614.959875	43754.855989	32.059623
615.423188	43831.301025	32.064640
615.970040	43899.965682	32.069658
616.624532	43970.112812	32.074676
617.320151	44046.553831	32.079693
618.266773	44112.398656	32.084711
618.651776	44186.826712	32.089728
619.698302	44251.840319	32.094746
620.093502	44315.741627	32.099764
620.936578	44393.602956	32.104781
621.692504	44455.164659	32.109799
621.911619	44514.906614	32.114816
622.272226	44589.687738	32.119834
623.014307	44660.512808	32.124852
623.869189	44731.725275	32.129869
624.858453	44794.902357	32.134887
625.094825	44865.807276	32.139904
625.710169	44937.557638	32.144922
626.457740	45003.221192	32.149940
627.318448	45077.179194	32.154957
627.662378	45125.086816	32.159975
628.449113	45200.132181	32.164992
629.116303	45271.774282	32.170010
629.735338	45343.247033	32.175028
630.296001	45409.466087	32.180045
631.226827	45471.661080	32.185063
631.370798	45533.555643	32.190080
631.764421	45605.810978	32.195098
632.765914	45667.128804	32.200116
633.559881	45722.608874	32.205133
634.137087	45779.995495	32.210151
634.609866	45846.400400	32.215168
634.821480	45907.671784	32.220186
635.869899	45965.870714	32.225204
636.328978	46030.095852	32.230221
636.913586	46099.071312	32.235239
637.280106	46165.734186	32.240256
638.031983	46239.390431	32.245274
638.576963	46307.866653	32.250292
639.089850	46377.278040	32.255309
639.572568	46436.484060	32.260327
640.266056	46509.650571	32.265344
641.114891	46586.259707	32.270362
641.694494	46662.702505	32.275380
641.886720	46740.680224	32.280397
642.966997	46810.079997	32.285415
643.655061	46892.832777	32.290432
644.140925	46961.212690	32.295450
644.869495	47027.720186	32.300468
645.401595	47113.420925	32.305485
646.043651	47189.571038	32.310503
646.659451	47274.278701	32.315520
647.052350	47352.340970	32.320538
648.026013	47429.173810	32.325556
648.620241	47525.089778	32.330573
649.411905	47588.103196	32.335591
650.064438	47672.275171	32.340608
650.734949	47751.377154	32.345626
651.405419	47824.133966	32.350644
651.767387	47909.826392	32.355661
652.578984	47986.610579	32.360679
653.322580	48077.817535	32.365696
653.912887	48154.592657	32.370714
654.977726	48230.135958	32.375732
655.192749	48310.158975	32.380749
655.901964	48374.724848	32.385767
656.581082	48469.037184	32.390784
657.325419	48548.288536	32.395802
658.264109	48628.914252	32.400820
658.770997	48715.586624	32.405837
659.759380	48777.901892	32.410855
660.327874	48862.534290	32.415872
660.646574	48944.947459	32.420890
661.786855	49018.944146	32.425908
662.127577	49100.424384	32.430925
663.174297	49181.636178	32.435943
663.621514	49248.928131	32.440960
664.472287	49336.466392	32.445978
665.299421	49395.588206	32.450996
665.825917	49476.110629	32.456013
666.805946	49544.490489	32.461031
667.241015	49622.800658	32.466048
667.604623	49696.060693	32.471066
668.435564	49770.544811	32.476084
668.948114	49853.456020	32.481101
670.040758	49930.613970	32.486119
670.584464	50002.695252	32.491136
671.228721	50073.767658	32.496154
672.216737	50145.102806	32.501172
672.595205	50230.484962	32.506189
673.381758	50292.563882	32.511207
674.019909	50369.864076	32.516224
674.929516	50439.130772	32.521242
675.443258	50519.911925	32.526260
675.970450	50597.388437	32.531277
676.550850	50664.745921	32.536295
677.160184	50735.148815	32.541312
677.876868	50800.175896	32.546330
678.889364	50865.732620	32.551348
679.428457	50941.088770	32.556365
680.066466	51003.275116	32.561383
680.591568	51074.021254	32.566400
680.936073	51154.445153	32.571418
681.605150	51215.203540	32.576436
682.346391	51286.055679	32.581453
683.144218	51358.272227	32.586471
684.033141	51439.187653	32.591488
684.375752	51512.475708	32.596506
685.105518	51592.575036	32.601524
685.657577	51672.278525	32.606541
686.256973	51740.958611	32.611559
687.015055	51818.061351	32.616576
687.735984	51894.195715	32.621594
688.264276	51963.969612	32.626612
688.787875	52058.789211	32.631629
689.525379	52137.819832	32.636647
690.521515	52231.079132	32.641664
691.168165	52309.093148	32.646682
691.936284	52383.108266	32.651700
692.707979	52472.284331	32.656717
693.269627	52550.230203	32.661735
694.261081	52628.444399	32.666752
694.819214	52718.578704	32.671770
695.475490	52792.384830	32.676788
696.068777	52876.781223	32.681805
696.633189	52967.453369	32.686823
697.736360	53046.625960	32.691840
698.225213	53131.419297	32.696858
699.141709	53212.247957	32.701876
699.637011	53296.376446	32.706893
700.325285	53379.152466	32.711911
701.124914	53451.571370	32.716928
701.941973	53541.902423	32.721946
702.747553	53626.673258	32.726964
703.093945	53713.066688	32.731981
703.872180	53796.981799	32.736999
705.023918	53880.566610	32.742016
705.760262	53953.901892	32.747034
706.262696	54040.107550	32.752052
707.058933	54127.944484	32.757069
707.783431	54208.256078	32.762087
708.629298	54285.435448	32.767104
709.261940	54370.147442	32.772122
710.090947	54443.735520	32.777140
710.768707	54524.454188	32.782157
711.660051	54605.734546	32.787175
711.971148	54684.030477	32.792192
712.587864	54766.512479	32.797210
713.658884	54845.829046	32.802228
714.036499	54937.392345	32.807245
714.981770	55013.172599	32.812263
715.830962	55095.353545	32.817280
716.153904	55177.218492	32.822298
717.150155	55261.104655	32.827316
717.480821	55350.480910	32.832333
718.032999	55433.798042	32.837351
719.127273	55519.872099	32.842368
719.752479	55609.234843	32.847386
720.564905	55683.690050	32.852404
720.996753	55774.507629	32.857421
721.667526	55857.054562	32.862439
722.354107	55940.599236	32.867456
723.006875	56026.130378	32.872474
723.726296	56114.796762	32.877492
724.542767	56211.232631	32.882509
725.028821	56293.196110	32.887527
725.993289	56374.888758	32.892544
726.518796	56461.188182	32.897562
727.451638	56529.564169	32.902580
727.897117	56619.325906	32.907597
728.813506	56708.178824	32.912615
729.460545	56798.137505	32.917632
729.930491	56875.017061	32.922650
731.002134	56960.802393	32.927668
731.540807	57046.329728	32.932685
732.738750	57128.817478	32.937703
733.241202	57222.439557	32.942720
733.691187	57310.298137	32.947738
734.519840	57402.198968	32.952756
735.208314	57489.565163	32.957773
735.567521	57573.419952	32.962791
736.959485	57673.176629	32.967808
737.552971	57765.178961	32.972826
738.209846	57853.336236	32.977844
738.674747	57957.087401	32.982861
739.360466	58046.778861	32.987879
740.174555	58136.323967	32.992896
741.155871	58222.241860	32.997914
742.163448	58318.295479	33.002932
742.621481	58420.999044	33.007949
743.073579	58510.690830	33.012967
744.356593	58599.543941	33.017984
744.605321	58696.933131	33.023002
745.888590	58791.306138	33.028020
746.678436	58899.789165	33.033037
747.105767	58991.834831	33.038055
748.274762	59069.776521	33.043072
749.049417	59169.186637	33.048090
749.774202	59253.344440	33.053108
750.930195	59344.024084	33.058125
751.023934	59433.015841	33.063143
752.256006	59523.025960	33.068160
753.150704	59626.546049	33.073178
753.629633	59712.408630	33.078196
754.699697	59801.204533	33.083213
755.249590	59894.905450	33.088231
756.113234	59985.468686	33.093248
757.094432	60075.659383	33.098266
757.721540	60170.716492	33.103284
758.727829	60257.087072	33.108301
759.022911	60342.917356	33.113319
760.016301	60435.360885	33.118336
760.761397	60537.775211	33.123354
761.808168	60611.449310	33.128372
762.209013	60708.050445	33.133389
762.816917	60797.352764	33.138407
763.618937	60884.643732	33.143424
764.448372	60976.760494	33.148442
765.240981	61065.294254	33.153460
766.074900	61158.759287	33.158477
766.163642	61252.189443	33.163495
767.443781	61339.824937	33.168512
768.019523	61435.553305	33.173530
768.801916	61527.812425	33.178548
769.678260	61626.153113	33.183565
770.461654	61727.154761	33.188583
771.589739	61817.695994	33.193600
772.215544	61915.463035	33.198618
772.938194	62004.080747	33.203636
773.841575	62088.726716	33.208653
774.130743	62188.155436	33.213671
775.069107	62280.525873	33.218688
775.879645	62372.777403	33.223706
776.760560	62467.195902	33.228724
777.506254	62548.386431	33.233741
778.065001	62637.399232	33.238759
779.083073	62718.028568	33.243776
779.036044	62804.060236	33.248794
779.922487	62890.028322	33.253812
781.197769	62979.417589	33.258829
781.662874	63078.062653	33.263847
782.710054	63175.192587	33.268864
783.458387	63271.325151	33.273882
784.212192	63362.101546	33.278900
784.987471	63443.841120	33.283917
785.560102	63553.632099	33.288935
786.653205	63648.661240	33.293952
786.739421	63743.310303	33.298970
787.819365	63850.079369	33.303988
788.804300	63943.873087	33.309005
789.210040	64041.543648	33.314023
789.804516	64136.431143	33.319040
790.574883	64244.351921	33.324058
791.528237	64357.131920	33.329076
792.311306	64462.411684	33.334093
792.837197	64569.162942	33.339111
794.138084	64675.337469	33.344128
795.114219	64783.798123	33.349146
795.452439	64890.782720	33.354164
796.680722	64998.419772	33.359181
797.061277	65107.013062	33.364199
798.126097	65211.105915	33.369216
799.289123	65321.388281	33.374234
799.905794	65432.472098	33.379252
800.655349	65534.893588	33.384269
801.529515	65650.781362	33.389287
802.101187	65752.300903	33.394304
803.113144	65863.457665	33.399322
804.060028	65969.996961	33.404340
804.921852	66071.972514	33.409357
805.334674	66174.873509	33.414375
806.068770	66282.504762	33.419392
807.000621	66394.676739	33.424410
808.142891	66507.955910	33.429428
808.894196	66606.088766	33.434445
809.660966	66726.094675	33.439463
810.511863	66821.648533	33.444480
811.324211	66937.646818	33.449498
812.442543	67043.055743	33.454516
813.204299	67140.498880	33.459533
813.596056	67252.518599	33.464551
814.508588	67360.911569	33.469568
815.593162	67462.192977	33.474586
816.641304	67566.810934	33.479604
817.383273	67672.097764	33.484621
817.860741	67783.131301	33.489639
818.954630	67886.426404	33.494656
819.899692	67989.909851	33.499674
820.534652	68096.329562	33.504692
821.679849	68198.775759	33.509709
822.318779	68308.000708	33.514727
823.489833	68414.989966	33.519744
824.144389	68515.298102	33.524762
824.598921	68612.573308	33.529780
825.784182	68715.217903	33.534797
826.440897	68824.961471	33.539815
827.234845	68928.972571	33.544832
828.059481	69035.575405	33.549850
828.318785	69137.834780	33.554868
829.454209	69240.178992	33.559885
830.296038	69359.210285	33.564903
830.854405	69456.193786	33.569920
831.667769	69558.330066	33.574938
832.679262	69650.576559	33.579956
833.432342	69763.829683	33.584973
834.062408	69876.273043	33.589991
834.666477	69965.589315	33.595008
835.673684	70078.462073	33.600026
836.627536	70197.599971	33.605044
837.230136	70295.022928	33.610061
838.173920	70401.258089	33.615079
838.910065	70513.655921	33.620096
839.924010	70628.125754	33.625114
840.606431	70735.935638	33.630132
841.745219	70849.740984	33.635149
842.229033	70964.105322	33.640167
843.081512	71073.549072	33.645184
843.959658	71186.193516	33.650202
844.520254	71309.716830	33.655220
845.798273	71417.727549	33.660237
846.315661	71537.953094	33.665255
847.634525	71658.750278	33.670272
848.488171	71777.505751	33.675290
848.748400	71892.149770	33.680308
849.550719	72009.242491	33.685325
850.486015	72133.014958	33.690343
851.535495	72249.107462	33.695360
852.708289	72379.189338	33.700378
853.521580	72505.287793	33.705396
854.358634	72611.345934	33.710413
854.878235	72736.212234	33.715431
855.903222	72860.126042	33.720448
856.665685	72972.416237	33.725466
857.495131	73100.161553	33.730484
858.667891	73231.678864	33.735501
859.377070	73353.098547	33.740519
860.659376	73466.487373	33.745536
861.545869	73583.649852	33.750554
862.159419	73713.445835	33.755572
863.062004	73833.646792	33.760589
864.198400	73961.968819	33.765607
865.037324	74074.264343	33.770624
866.150672	74180.437460	33.775642
866.711205	74310.675300	33.780660
867.594096	74432.528676	33.785677
868.730802	74549.124203	33.790695
869.530129	74664.227725	33.795712
870.799045	74787.364936	33.800730
871.474935	74908.910881	33.805748
872.113064	75021.393806	33.810765
872.929586	75138.206689	33.815783
873.736890	75264.445755	33.820800
874.946706	75375.738614	33.825818
875.410516	75500.677195	33.830836
876.277060	75609.795358	33.835853
877.209102	75735.206392	33.840871
877.839306	75861.007285	33.845888
879.391590	75987.766437	33.850906
880.091373	76098.521430	33.855924
881.107034	76212.178924	33.860941
881.813947	76334.879148	33.865959
882.683656	76450.612624	33.870976
883.683836	76563.057925	33.875994
884.361933	76696.177049	33.881012
885.246918	76807.577312	33.886029
885.981807	76929.756458	33.891047
886.707288	77056.156006	33.896064
887.758111	77179.008862	33.901082
888.595436	77303.314508	33.906100
889.223123	77414.909549	33.911117
889.977378	77528.879484	33.916135
890.911261	77647.749654	33.921152
891.654188	77772.794289	33.926170
892.290021	77899.895843	33.931188
893.886438	78015.078761	33.936205
894.740790	78136.737848	33.941223
895.018130	78247.377660	33.946240
896.352587	78366.479587	33.951258
896.965564	78495.956464	33.956276
897.795881	78617.190704	33.961293
898.757956	78750.617370	33.966311
899.987384	78872.841733	33.971328
901.106736	78997.934331	33.976346
901.357176	79131.904997	33.981364
902.383850	79252.984589	33.986381
903.804309	79383.998799	33.991399
904.631555	79517.450268	33.996416
905.713142	79628.375073	34.001434
906.246958	79766.789252	34.006452
907.311080	79897.202884	34.011469
908.062867	80020.989375	34.016487
909.460885	80146.727645	34.021504
910.589996	80262.727896	34.026522
911.056736	80397.038186	34.031540
911.756136	80521.696612	34.036557
912.879438	80650.634844	34.041575
913.604825	80783.462168	34.046592
914.621496	80910.087097	34.051610
915.424581	81043.004840	34.056628
916.139716	81174.023858	34.061645
917.450139	81301.567453	34.066663
918.141319	81440.142634	34.071680
919.340066	81572.886899	34.076698
920.391308	81711.178977	34.081716
921.451108	81833.658238	34.086733
922.378896	81968.917439	34.091751
923.104584	82106.806304	34.096768
924.463528	82227.175202	34.101786
925.032459	82362.910588	34.106804
926.115087	82486.605441	34.111821
926.997916	82617.769607	34.116839
927.835271	82760.433553	34.121856
929.268764	82884.252586	34.126874
929.861797	83023.788492	34.131892
930.827737	83150.266675	34.136909
931.730927	83274.689931	34.141927
932.556855	83414.051901	34.146944
933.684227	83540.696599	34.151962
934.440422	83664.485688	34.156980
935.864833	83791.110326	34.161997
936.594534	83912.927983	34.167015
937.465628	84055.212983	34.172032
938.428981	84189.526830	34.177050
939.159732	84320.862003	34.182068
940.187035	84443.268866	34.187085
941.133025	84576.256766	34.192103
942.088752	84711.258487	34.197120
943.125646	84843.295712	34.202138
944.014156	84973.151953	34.207156
945.039995	85103.696876	34.212173
946.096922	85225.772962	34.217191
947.184790	85356.854190	34.222208
948.037646	85489.328668	34.227226
949.030727	85619.285478	34.232244
949.933080	85741.273892	34.237261
951.047088	85868.235029	34.242279
951.447342	85997.855511	34.247296
952.523300	86112.874141	34.252314
953.557114	86239.596015	34.257332
954.353442	86369.206822	34.262349
955.095237	86495.772779	34.267367
956.340259	86619.802105	34.272384
957.199354	86736.022978	34.277402
957.898156	86861.824248	34.282420
958.919460	86992.150250	34.287437
960.061224	87119.986868	34.292455
960.927283	87242.075939	34.297472
961.727545	87372.907117	34.302490
962.760340	87501.345387	34.307508
963.548511	87636.184132	34.312525
964.188360	87769.538678	34.317543
964.943212	87919.907868	34.322560
966.213951	88048.488684	34.327578
967.174378	88194.125506	34.332596
968.045318	88327.573114	34.337613
969.068710	88476.610459	34.342631
969.739290	88614.703666	34.347648
970.957745	88757.274018	34.352666
971.962482	88906.278421	34.357684
972.838776	89053.985675	34.362701
973.846731	89191.420424	34.367719
974.537472	89346.369230	34.372736
975.744839	89496.574166	34.377754
976.665012	89648.928606	34.382772
977.479146	89801.997464	34.387789
978.716112	89950.615863	34.392807
979.532865	90107.487928	34.397824
980.730325	90257.812295	34.402842
981.441023	90415.437645	34.407860
982.653777	90559.259508	34.412877
983.801514	90715.411212	34.417895
984.519289	90867.930261	34.422912
985.676797	91017.453545	34.427930
986.754039	91162.972468	34.432948
987.478667	91333.173070	34.437965
988.928576	91480.536286	34.442983
989.895478	91634.097495	34.448000
990.827157	91796.245491	34.453018
991.837592	91942.678490	34.458036
992.891093	92099.232311	34.463053
993.988232	92248.010645	34.468071
994.782072	92395.430317	34.473088
996.126661	92551.180410	34.478106
997.319188	92708.590138	34.483124
998.297988	92858.213825	34.488141
999.431169	93000.285242	34.493159
1000.093992	93154.991742	34.498176
1001.241658	93308.507717	34.503194
1002.494982	93449.662483	34.508212
1003.134741	93589.507031	34.513229
1004.300594	93738.484640	34.518247
1005.293332	93892.965741	34.523264
1006.002644	94055.718213	34.528282
1007.252730	94203.417353	34.533300
1008.321787	94352.679258	34.538317
1009.602130	94498.765300	34.543335
1010.578733	94656.358211	34.548352
1011.062128	94796.169313	34.553370
1012.318174	94953.935465	34.558388
1013.397181	95112.579404	34.563405
1014.468098	95241.868455	34.568423
1015.186394	95408.644803	34.573440
1015.929111	95554.084774	34.578458
1017.434645	95716.569159	34.583476
1018.489125	95856.004047	34.588493
1019.645605	96002.015114	34.593511
1020.555256	96143.223244	34.598528
1021.765416	96277.729990	34.603546
1022.560489	96419.502372	34.608564
1023.134072	96558.635383	34.613581
1024.483264	96693.147488	34.618599
1025.338944	96840.502521	34.623616
1026.559443	96983.617907	34.628634
1027.171671	97137.021057	34.633652
1027.983829	97285.069503	34.638669
1029.272954	97439.230142	34.643687
1030.275080	97592.840660	34.648704
1031.110189	97743.575101	34.653722
1032.362052	97893.661875	34.658740
1033.054441	98051.810680	34.663757
1034.178886	98210.513793	34.668775
1035.225941	98366.719770	34.673792
1036.329490	98525.554487	34.678810
1037.319356	98682.709061	34.683828
1038.161173	98845.883876	34.688845
1039.247182	99012.761067	34.693863
1039.996597	99169.511965	34.698880
1040.876533	99345.867721	34.703898
1042.649745	99512.779364	34.708916
1043.762534	99676.866771	34.713933
1044.533713	99841.274722	34.718951
1045.954329	100004.314069	34.723968
1046.762892	100172.622552	34.728986
1047.701275	100328.855054	34.734004
1048.728218	100506.106911	34.739021
1049.675008	100668.754698	34.744039
1050.944132	100840.886636	34.749056
1052.248380	101002.098227	34.754074
1053.070887	101176.533184	34.759092
1053.963226	101347.129342	34.764109
1055.351363	101521.553650	34.769127
1056.456947	101689.468460	34.774144
1057.756510	101860.561375	34.779162
1058.985375	102017.910195	34.784180
1059.783504	102193.457389	34.789197
1060.891494	102358.763473	34.794215
1062.070724	102521.295300	34.799232
1063.131320	102685.570795	34.804250
1064.420940	102849.570353	34.809268
1065.302276	103021.229226	34.814285
1066.234576	103185.958362	34.819303
1067.450763	103344.710145	34.824320
1068.418401	103525.613703	34.829338
1069.835949	103681.850490	34.834356
1070.793790	103861.311992	34.839373
1072.196891	104012.950079	34.844391
1073.145381	104193.517911	34.849408
1074.390270	104352.130515	34.854426
1075.505557	104511.626352	34.859444
1076.362905	104669.045870	34.864461
1077.617586	104834.341256	34.869479
1078.563404	104997.099186	34.874496
1079.632416	105164.517379	34.879514
1080.908675	105326.248832	34.884532
1081.802004	105486.126375	34.889549
1082.839053	105656.899446	34.894567
1083.772259	105816.138312	34.899584
1085.045973	105987.319785	34.904602
1085.947835	106140.491409	34.909620
1087.096205	106318.224341	34.914637
1088.222108	106476.852845	34.919655
1089.372306	106650.960721	34.924672
1090.038155	106811.932546	34.929690
1091.382277	106962.325050	34.934708
1092.323255	107115.139865	34.939725
1093.324512	107279.383610	34.944743
1094.615256	107427.389917	34.949760
1095.390704	107588.880797	34.954778
1096.583404	107738.691736	34.959796
1097.558497	107911.032767	34.964813
1098.735207	108067.061125	34.969831
1099.609037	108238.176932	34.974848
1100.643924	108403.600059	34.979866
1101.866640	108570.833288	34.984884
1102.935862	108738.547864	34.989901
1103.952589	108908.084843	34.994919
1105.226446	109076.263562	34.999936
1106.133351	109250.942530	35.004954
1107.250455	109414.518821	35.009972
1108.459961	109595.365892	35.014989
1109.399612	109772.946329	35.020007
1110.789641	109940.159909	35.025024
1111.522898	110116.962788	35.030042
1113.157879	110287.867999	35.035060
1113.991549	110473.673461	35.040077
1115.175437	110652.538965	35.045095
1116.643564	110831.754005	35.050112
1117.678272	111007.195242	35.055130
1118.456501	111179.671917	35.060148
1119.318462	111368.280301	35.065165
1120.568883	111549.156311	35.070183
1122.117299	111730.405090	35.075200
1123.179946	111912.808809	35.080218
1124.394169	112087.453646	35.085236
1125.503609	112270.029404	35.090253
1126.308382	112449.254950	35.095271
1128.039022	112634.639537	35.100288
1128.897546	112821.188880	35.105306
1130.292447	112991.434401	35.110324
1131.334957	113181.533240	35.115341
1132.399434	113359.099281	35.120359
1133.464451	113547.636561	35.125376
1134.336701	113723.129159	35.130394
1135.415264	113910.829142	35.135412
1137.003125	114097.296224	35.140429
1137.904286	114290.251243	35.145447
1139.289583	114462.217333	35.150464
1140.330146	114647.720216	35.155482
1141.540706	114831.218864	35.160500
1142.836511	115026.995026	35.165517
1143.647550	115215.783581	35.170535
1145.137077	115394.383700	35.175552
1146.133605	115576.004389	35.180570
1147.023916	115763.235963	35.185588
1148.883662	115952.688518	35.190605
1149.996392	116135.447945	35.195623
1151.150788	116313.584929	35.200640
1152.230659	116504.037545	35.205658
1153.491110	116677.365251	35.210676
1154.781860	116862.358062	35.215693
1155.944579	117043.262275	35.220711
1157.294168	117220.700776	35.225728
1158.055565	117406.134284	35.230746
1159.398951	117580.100053	35.235764
1160.431635	117764.402028	35.240781
1161.573983	117946.988062	35.245799
1163.159750	118121.768214	35.250816
1163.984421	118301.983014	35.255834
1165.246526	118484.641676	35.260852
1166.429592	118658.536019	35.265869
1167.532689	118835.411824	35.270887
1168.905439	119015.303192	35.275904
1170.123447	119180.860748	35.280922
1170.999267	119334.105128	35.285940
1172.088674	119501.434672	35.290957
1173.024400	119673.799452	35.295975
1174.304089	119841.633444	35.300992
1175.242517	120021.521407	35.306010
1176.407186	120175.573799	35.311028
1177.694888	120360.546026	35.316045
1178.412061	120537.845249	35.321063
1179.794846	120727.941755	35.326080
1180.857252	120907.662201	35.331098
1182.059503	121084.685018	35.336116
1183.298328	121262.552820	35.341133
1184.368124	121451.623610	35.346151
1185.847721	121637.003155	35.351168
1186.789558	121827.402377	35.356186
1188.086213	122008.385115	35.361204
1189.761198	122194.878395	35.366221
1190.324322	122393.065109	35.371239
1191.903596	122564.568095	35.376256
1192.846968	122764.866385	35.381274
1194.009678	122951.887429	35.386292
1195.196661	123138.550349	35.391309
1196.043547	123336.583179	35.396327
1197.452536	123528.744212	35.401344
1198.782885	123725.942132	35.406362
1199.942484	123933.887470	35.411380
1200.795334	124121.761719	35.416397
1202.008070	124330.994778	35.421415
1203.313778	124520.335022	35.426432
1204.730452	124735.526161	35.431450
1205.757821	124925.406641	35.436468
1207.239752	125133.574118	35.441485
1208.430443	125340.963632	35.446503
1209.888502	125530.246684	35.451520
1210.689096	125737.559731	35.456538
1211.836994	125929.493946	35.461556
1213.526576	126137.570608	35.466573
1214.717573	126348.733151	35.471591
1216.224026	126549.735956	35.476608
1217.346772	126746.448190	35.481626
1218.698994	126940.638788	35.486644
1219.919171	127142.983369	35.491661
1221.072446	127350.097080	35.496679
1222.505354	127534.825929	35.501696
1223.620442	127734.462100	35.506714
1225.091597	127937.380246	35.511732
1226.449628	128130.826943	35.516749
1227.312467	128335.555039	35.521767
1228.780863	128537.169719	35.526784
1230.173438	128728.266579	35.531802
1230.937691	128921.556118	35.536820
1232.871251	129122.149210	35.541837
1233.608462	129314.480516	35.546855
1235.024078	129506.465428	35.551872
1236.068980	129713.696570	35.556890
1237.325382	129901.914530	35.561908
1238.846048	130115.315588	35.566925
1240.104579	130296.734214	35.571943
1241.382184	130496.383364	35.576960
1242.588023	130688.571375	35.581978
1243.857465	130887.373515	35.586996
1245.058909	131084.943770	35.592013
1246.327228	131283.874796	35.597031
1247.491009	131476.352041	35.602048
1248.591535	131672.303976	35.607066
1250.108677	131859.817193	35.612084
1251.607653	132037.652723	35.617101
1252.330906	132225.367918	35.622119
1253.845871	132403.532339	35.627136
1254.830763	132590.319938	35.632154
1256.156139	132778.971030	35.637172
1257.451985	132953.987115	35.642189
1258.064187	133142.269230	35.647207
1260.093821	133329.429352	35.652224
1260.857092	133523.234483	35.657242
1261.779934	133721.900746	35.662260
1262.936573	133909.504511	35.667277
1264.008505	134111.207234	35.672295
1265.609723	134313.703568	35.677312
1266.766802	134512.095588	35.682330
1267.699251	134727.755693	35.687348
1268.806936	134932.451188	35.692365
1270.204243	135152.151905	35.697383
1271.588192	135354.268187	35.702400
1272.765236	135563.155894	35.707418
1274.170495	135773.468140	35.712436
1275.539223	135989.307069	35.717453
1276.656491	136205.059485	35.722471
1277.891376	136416.238887	35.727488
1279.460114	136638.762455	35.732506
1280.461615	136851.579310	35.737524
1281.611271	137068.028659	35.742541
1282.507460	137290.102296	35.747559
1283.899675	137510.310055	35.752576
1285.770135	137731.954121	35.757594
1286.696518	137961.678387	35.762612
1288.477991	138178.034013	35.767629
1289.750471	138405.853513	35.772647
1291.262142	138626.961550	35.777664
1292.431295	138849.317143	35.782682
1293.592914	139063.946463	35.787700
1295.436294	139272.391274	35.792717
1296.516879	139512.276791	35.797735
1297.770234	139728.544542	35.802752
1299.462170	139941.292749	35.807770
1300.410080	140175.453484	35.812788
1302.190602	140387.529892	35.817805
1303.029099	140610.732314	35.822823
1304.634997	140817.913894	35.827840
1306.222404	141052.638731	35.832858
1307.467432	141264.180966	35.837876
1308.756710	141477.189366	35.842893
1310.289612	141695.325873	35.847911
1311.445936	141917.773865	35.852928
1312.774460	142121.641256	35.857946
1313.886110	142349.974271	35.862964
1315.276205	142571.906370	35.867981
1316.496227	142793.561497	35.872999
1317.919166	143012.685627	35.878016
1319.776254	143224.343586	35.883034
1320.638882	143446.374869	35.888052
1322.212368	143656.721059	35.893069
1323.407077	143889.071434	35.898087
1324.536114	144100.847081	35.903104
1326.074904	144322.116440	35.908122
1327.425341	144541.779002	35.913140
1328.800814	144758.735214	35.918157
1329.793841	144974.444946	35.923175
1331.275437	145185.370363	35.928192
1332.608174	145409.951289	35.933210
1333.812886	145635.352850	35.938228
1335.007482	145847.861686	35.943245
1336.359833	146077.608210	35.948263
1337.711422	146291.680843	35.953280
1339.213488	146500.108084	35.958298
1340.429486	146717.237186	35.963316
1341.949819	146916.296224	35.968333
1343.427124	147127.826832	35.973351
1344.445476	147325.341365	35.978368
1345.549327	147530.941163	35.983386
1346.861195	147749.696912	35.988404
1348.292259	147958.229949	35.993421
1349.523300	148177.253982	35.998439
1350.695845	148400.502104	36.003456
1352.109856	148614.790262	36.008474
1353.124593	148835.564416	36.013492
1355.074598	149061.866860	36.018509
1356.014256	149293.786427	36.023527
1357.591967	149521.710338	36.028544
1359.384473	149735.067919	36.033562
1359.951526	149959.737419	36.038580
1361.555927	150181.706824	36.043597
1362.746927	150422.883377	36.048615
1364.002952	150643.373307	36.053632
1365.609509	150875.741082	36.058650
1366.913640	151124.481005	36.063668
1368.325508	151345.038221	36.068685
1369.649425	151578.354451	36.073703
1371.018990	151812.527690	36.078720
1372.746327	152052.307306	36.083738
1373.808269	152288.701326	36.088756
1375.098839	152532.397581	36.093773
1376.551275	152768.821365	36.098791
1377.806647	153006.317890	36.103808
1379.595357	153249.203036	36.108826
1380.847543	153499.573823	36.113844
1382.152555	153738.170031	36.118861
1383.322595	153976.344071	36.123879
1384.621893	154221.239484	36.128896
1386.812742	154462.543560	36.133914
1387.932862	154712.356396	36.138932
1389.278592	154950.138839	36.143949
1390.619263	155195.476219	36.148967
1392.160685	155447.942884	36.153984
1393.628306	155687.867323	36.159002
1394.937591	155946.097699	36.164020
1396.705230	156182.384640	36.169037
1397.832991	156422.644557	36.174055
1399.167071	156672.254554	36.179072
1400.793875	156917.732064	36.184090
1402.223414	157165.501141	36.189108
1403.495669	157402.759116	36.194125
1404.986957	157660.130594	36.199143
1406.383348	157899.338811	36.204160
1408.013674	158139.196890	36.209178
1409.273985	158395.693610	36.214196
1410.736982	158635.249765	36.219213
1412.077917	158888.143212	36.224231
1413.182791	159144.235764	36.229248
1415.000701	159386.278346	36.234266
1416.150933	159631.359005	36.239284
1417.529771	159887.767224	36.244301
1419.025505	160129.596529	36.249319
1420.550316	160380.474103	36.254336
1421.770306	160622.196123	36.259354
1423.095277	160883.072979	36.264372
1424.599839	161132.318983	36.269389
1426.534605	161383.339504	36.274407
1427.705098	161637.578400	36.279424
1429.300396	161881.569790	36.284442
1430.717688	162134.058092	36.289460
1432.452715	162378.575415	36.294477
1433.697566	162617.685741	36.299495
1435.119460	162842.956009	36.304512
1436.371580	163072.303658	36.309530
1437.863500	163316.913340	36.314548
1439.325545	163543.347770	36.319565
1440.710508	163776.676360	36.324583
1441.705311	164013.393243	36.329600
1443.352170	164246.682493	36.334618
1444.225021	164480.550772	36.339636
1445.749078	164735.101845	36.344653
1447.693020	164977.704344	36.349671
1448.347908	165231.060210	36.354688
1450.368488	165477.220200	36.359706
1451.592593	165736.976758	36.364724
1452.603563	165981.112785	36.369741
1454.355337	166237.360574	36.374759
1455.757487	166498.145960	36.379776
1457.409205	166753.852669	36.384794
1458.822525	167011.730686	36.389812
1460.360003	167263.813174	36.394829
1461.755311	167522.013308	36.399847
1462.921622	167784.237055	36.404864
1464.723999	168049.320606	36.409882
1466.193487	168316.450674	36.414900
1467.403193	168575.940690	36.419917
1469.105988	168842.998111	36.424935
1470.477971	169104.915171	36.429952
1472.198786	169377.774336	36.434970
1473.290674	169655.024623	36.439988
1475.031887	169913.852159	36.445005
1476.480588	170182.668390	36.450023
1478.055182	170452.583262	36.455040
1479.408714	170732.590064	36.460058
1481.214915	171004.578455	36.465076
1482.716982	171276.615434	36.470093
1484.327220	171543.849485	36.475111
1485.500989	171818.606281	36.480128
1487.083410	172083.370551	36.485146
1488.657575	172366.396300	36.490164
1490.336408	172637.851770	36.495181
1492.196758	172901.280183	36.500199
1493.211695	173178.034841	36.505216
1495.013772	173446.921582	36.510234
1496.581929	173720.137747	36.515252
1497.941456	173999.647599	36.520269
1499.436862	174261.169504	36.525287
1500.740520	174540.880469	36.530304
1502.520607	174812.543444	36.535322
1504.018506	175083.807065	36.540340
1505.489596	175362.186761	36.545357
1507.054047	175630.076772	36.550375
1509.012550	175908.229660	36.555392
1510.664232	176171.041176	36.560410
1512.092037	176452.948762	36.565428
1513.554293	176716.388469	36.570445
1515.236780	176978.854851	36.575463
1516.598574	177243.784949	36.580480
1518.692826	177512.182210	36.585498
1520.075564	177783.104398	36.590516
1521.032456	178044.443174	36.595533
1522.761474	178307.058743	36.600551
1524.308516	178581.208564	36.605568
1525.848009	178839.029913	36.610586
1526.937186	179123.691415	36.615604
1528.694411	179385.162918	36.620621
1530.120622	179668.401954	36.625639
1531.477656	179939.639606	36.630656
1533.067240	180193.063246	36.635674
1534.864190	180446.734517	36.640692
1536.474996	180712.067870	36.645709
1537.898362	180962.776696	36.650727
1539.565542	181219.264199	36.655744
1540.619260	181469.879867	36.660762
1542.402307	181733.411333	36.665780
1543.829819	181978.941026	36.670797
1545.463592	182235.563541	36.675815
1547.109201	182496.985196	36.680832
1548.467675	182749.664640	36.685850
1549.809042	183007.706516	36.690868
1551.065368	183278.131508	36.695885
1552.850340	183545.350480	36.700903
1554.241743	183805.951912	36.705920
1555.794375	184163.425276	36.710938
1557.155406	184436.122966	36.715956
1558.709542	184706.175086	36.720973
1560.110722	184984.811344	36.725991
1561.595190	185268.413559	36.731008
1563.305337	185548.018972	36.736026
1564.812109	185827.148991	36.741044
1566.324172	186126.750783	36.746061
1567.996139	186399.201867	36.751079
1569.710713	186699.383191	36.756096
1571.282529	186982.570030	36.761114
1573.037502	187265.373362	36.766132
1574.466157	187565.144683	36.771149
1576.105592	187852.387181	36.776167
1577.651138	188143.836096	36.781184
1578.954248	188431.005750	36.786202
1580.577555	188725.161818	36.791220
1582.018988	189023.207924	36.796237
1584.013695	189323.708237	36.801255
1585.698313	189624.207076	36.806272
1587.386162	189916.984540	36.811290
1589.299774	190219.887519	36.816308
1590.563028	190513.240947	36.821325
1591.919079	190797.309444	36.826343
1593.779205	191108.148009	36.831360
1595.434779	191396.235134	36.836378
1597.306283	191698.615080	36.841396
1598.793871	192002.046488	36.846413
1600.566194	192280.871608	36.851431
1602.249648	192583.587978	36.856448
1603.828937	192883.019279	36.861466
1605.813044	193169.433488	36.866484
1607.010696	193468.798899	36.871501
1608.930666	193772.776549	36.876519
1610.435419	194060.182206	36.881536
1612.217748	194352.422066	36.886554
1613.564831	194642.698598	36.891572
1615.436866	194945.695823	36.896589
1617.258369	195229.523675	36.901607
1618.971768	195528.711443	36.906624
1620.820976	195826.176717	36.911642
1622.201963	196107.408183	36.916660
1623.814822	196400.415620	36.921677
1625.511615	196692.851695	36.926695
1627.019680	196978.662688	36.931712
1628.615667	197271.445941	36.936730
1630.567237	197562.269007	36.941748
1631.942456	197856.053244	36.946765
1633.994076	198133.525861	36.951783
1635.667038	198424.241805	36.956800
1636.795152	198719.539709	36.961818
1638.683792	199001.027515	36.966836
1640.070590	199294.634910	36.971853
1641.685371	199574.210656	36.976871
1643.584335	199840.330126	36.981888
1645.125597	200116.971690	36.986906
1646.834785	200385.458755	36.991924
1648.240317	200660.268126	36.996941
1649.858732	200928.414652	37.001959
1651.572405	201195.784631	37.006976
1653.071478	201472.866902	37.011994
1655.002042	201751.914284	37.017012
1656.267253	202029.821523	37.022029
1657.680248	202311.414832	37.027047
1659.258584	202593.922603	37.032064
1660.846388	202885.980687	37.037082
1662.566570	203172.023518	37.042100
1663.895467	203465.393171	37.047117
1665.637293	203747.877137	37.052135
1667.482190	204058.821803	37.057152
1668.916126	204357.790393	37.062170
1671.128231	204649.321668	37.067188
1672.299048	204952.396783	37.072205
1674.109541	205245.185713	37.077223
1675.530513	205550.788265	37.082240
1677.073577	205857.159652	37.087258
1678.974354	206163.958162	37.092276
1680.506658	206483.287645	37.097293
1682.314097	206798.738683	37.102311
1683.960704	207098.668671	37.107328
1685.490540	207417.847475	37.112346
1687.254223	207725.609529	37.117364
1689.049462	208046.627502	37.122381
1690.489829	208361.553874	37.127399
1692.441126	208678.864812	37.132416
1694.172255	209002.281996	37.137434
1696.432477	209316.801855	37.142452
1697.903526	209651.565036	37.147469
1699.959779	209962.688154	37.152487
1701.728809	210266.946864	37.157504
1703.447045	210580.536917	37.162522
1705.581926	210887.203194	37.167540
1707.086426	211206.975029	37.172557
1708.943574	211521.027051	37.177575
1710.794070	211831.600164	37.182592
1712.279666	212145.710986	37.187610
1714.125392	212451.662029	37.192628
1715.766032	212764.123378	37.197645
1717.754614	213077.724549	37.202663
1719.350569	213387.322873	37.207680
1720.939217	213699.056528	37.212698
1722.975416	213999.491992	37.217716
1724.721319	214322.861879	37.222733
1726.991956	214622.067192	37.227751
1728.399293	214937.691643	37.232768
1729.656593	215246.734845	37.237786
1731.641372	215560.059296	37.242804
1733.098582	215879.969916	37.247821
1735.090099	216190.677184	37.252839
1736.522613	216504.393589	37.257856
1737.954459	216831.117088	37.262874
1740.262165	217141.927938	37.267892
1741.933627	217455.353531	37.272909
1743.257590	217761.542770	37.277927
1745.827854	218085.726362	37.282944
1747.278395	218403.683571	37.287962
1749.223026	218705.813181	37.292980
1750.945787	219037.598682	37.297997
1752.662335	219344.743466	37.303015
1754.489775	219653.166638	37.308032
1755.981018	219973.557028	37.313050
1757.812632	220277.153046	37.318068
1759.303824	220579.583057	37.323085
1761.220685	220877.119797	37.328103
1762.824294	221160.987475	37.333120
1764.581855	221470.463821	37.338138
1766.367526	221761.721156	37.343156
1767.603952	222065.614116	37.348173
1769.437356	222354.222104	37.353191
1771.310602	222664.137928	37.358208
1772.468506	222980.618388	37.363226
1774.224731	223287.351730	37.368244
1776.280802	223608.366096	37.373261
1777.890289	223935.547370	37.378279
1779.804956	224249.089738	37.383296
1781.344727	224575.113395	37.388314
1782.991269	224898.173489	37.393332
1784.949591	225225.478096	37.398349
1786.372139	225558.658677	37.403367
1788.452943	225887.011086	37.408384
1790.083105	226236.493983	37.413402
1791.673981	226549.807587	37.418420
1793.675329	226890.061466	37.423437
1795.244409	227228.909506	37.428455
1797.083805	227557.883817	37.433472
1798.823524	227917.968243	37.438490
1800.483540	228253.245292	37.443508
1802.674528	228607.517617	37.448525
1804.418117	228953.070050	37.453543
1806.330059	229308.884668	37.458560
1807.899663	229671.510203	37.463578
1809.718652	230009.200636	37.468596
1811.467584	230376.573781	37.473613
1813.410601	230726.489247	37.478631
1815.490698	231080.625566	37.483648
1817.300577	231448.344308	37.488666
1819.488131	231799.541984	37.493684
1821.198287	232154.040468	37.498701
1823.294003	232500.425365	37.503719
1825.266991	232860.140904	37.508736
1826.818430	233214.561946	37.513754
1828.865238	233564.383340	37.518772
1830.917793	233920.021070	37.523789
1832.515704	234280.861252	37.528807
1834.632588	234629.629337	37.533824
1836.030597	234991.567185	37.538842
1837.943899	235355.710429	37.543860
1839.725164	235704.733373	37.548877
1841.871559	236063.276077	37.553895
1843.826031	236425.913067	37.558912
1845.706616	236787.900765	37.563930
1847.437370	237139.267410	37.568948
1849.457693	237500.241763	37.573965
1850.874908	237856.813664	37.578983
1853.325433	238216.805388	37.584000
1854.700670	238574.958080	37.589018
1856.748883	238926.933612	37.594036
1858.360509	239278.951643	37.599053
1860.189095	239649.860870	37.604071
1862.267587	240010.035672	37.609088
1864.122087	240385.741118	37.614106
1866.034966	240737.964217	37.619124
1867.887492	241099.138257	37.624141
1869.923183	241473.010173	37.629159
1871.693872	241823.552022	37.634176
1873.480889	242200.179908	37.639194
1875.498226	242560.817982	37.644212
1877.676306	242921.608177	37.649229
1879.151406	243272.092545	37.654247
1881.703105	243620.451878	37.659264
1883.369135	243964.275098	37.664282
1885.325463	244306.858414	37.669300
1886.649988	244637.016403	37.674317
1888.106072	244973.885055	37.679335
1890.066238	245315.805660	37.684352
1892.223790	245670.091371	37.689370
1893.607084	246010.602301	37.694388
1895.655715	246370.848052	37.699405
1897.546808	246721.566383	37.704423
1899.242036	247061.696424	37.709440
1901.285197	247417.470193	37.714458
1902.903225	247773.055773	37.719476
1905.028348	248144.158427	37.724493
1906.663465	248512.263289	37.729511
1908.785575	248869.190350	37.734528
1910.307806	249242.518821	37.739546
1912.133402	249617.907394	37.744564
1914.313501	249984.628315	37.749581
1916.009500	250367.148092	37.754599
1918.113664	250742.058689	37.759616
1920.086433	251123.771308	37.764634
1921.806228	251498.968885	37.769652
1923.852536	251875.308358	37.774669
1925.646729	252261.974099	37.779687
1927.906311	252647.092731	37.784704
1929.875865	253038.047338	37.789722
1931.669029	253426.031113	37.794740
1933.741072	253802.514112	37.799757
1935.722124	254203.853019	37.804775
1937.879720	254590.684353	37.809792
1939.565389	254988.282423	37.814810
1941.756768	255390.550255	37.819828
1943.891310	255766.205330	37.824845
1945.373979	256156.668603	37.829863
1947.825513	256551.348110	37.834880
1949.376834	256941.468098	37.839898
1951.403707	257338.751754	37.844916
1953.603823	257732.908165	37.849933
1955.712752	258132.868978	37.854951
1958.016346	258524.009419	37.859968
1959.729504	258919.279690	37.864986
1961.628266	259309.160131	37.870004
1963.799271	259703.060774	37.875021
1965.663273	260105.542653	37.880039
1967.607846	260503.260701	37.885056
1969.492584	260900.199343	37.890074
1971.551429	261295.763167	37.895092
1973.761979	261691.149474	37.900109
1975.819224	262083.967587	37.905127
1977.565582	262479.271333	37.910144
1979.636836	262884.758899	37.915162
1981.592279	263282.211398	37.920180
1984.108202	263678.685750	37.925197
1986.071611	264079.740768	37.930215
1988.072750	264475.784690	37.935232
1990.041337	264872.619576	37.940250
1992.117885	265257.015872	37.945268
1994.080701	265654.255025	37.950285
1995.689999	266047.611098	37.955303
1998.418425	266432.840692	37.960320
2000.232944	266836.117885	37.965338
2001.800969	267221.424367	37.970356
2004.151323	267602.314569	37.975373
2006.215583	268012.049839	37.980391
2008.254236	268396.160464	37.985408
2010.130838	268788.219127	37.990426
2011.961822	269183.000886	37.995444
2014.141863	269573.891260	38.000461
2015.955247	269938.296550	38.005479
2017.938993	270305.442091	38.010496
2020.009195	270686.338165	38.015514
2021.701488	271064.955176	38.020532
2023.926576	271427.766185	38.025549
2026.059802	271811.923866	38.030567
2027.811420	272185.193355	38.035584
2029.597687	272569.122622	38.040602
2031.389387	272957.773180	38.045620
2033.612370	273340.589397	38.050637
2035.572287	273731.165674	38.055655
2037.450729	274115.378322	38.060672
2039.331954	274509.188669	38.065690
2041.085943	274904.769408	38.070708
2043.267630	275307.341503	38.075725
2045.137960	275719.610878	38.080743
2047.290303	276115.732929	38.085760
2049.172547	276526.726510	38.090778
2051.095510	276947.488981	38.095796
2053.652873	277358.093274	38.100813
2055.508731	277772.309754	38.105831
2057.637487	278192.525435	38.110848
2059.860994	278616.431709	38.115866
2061.493879	279043.780195	38.120884
2063.929861	279464.982022	38.125901
2065.730158	279887.703059	38.130919
2068.097760	280311.831235	38.135936
2070.272457	280731.644701	38.140954
2072.252620	281156.438114	38.145972
2074.796913	281591.196915	38.150989
2076.730409	282021.706281	38.156007
2078.541334	282446.340856	38.161024
2080.825911	282869.197417	38.166042
2082.958862	283306.701908	38.171060
2085.209551	283736.948118	38.176077
2087.450302	284183.673490	38.181095
2089.170218	284606.455551	38.186112
2091.808214	285035.363448	38.191130
2093.760767	285476.539055	38.196148
2095.886138	285904.886852	38.201165
2097.969163	286348.397872	38.206183
2100.179658	286781.627503	38.211200
2102.576686	287204.871392	38.216218
2104.096026	287647.497017	38.221236
2106.442976	288075.923094	38.226253
2108.467199	288517.143452	38.231271
2110.575505	288962.257928	38.236288
2112.809179	289398.716653	38.241306
2114.723709	289845.099466	38.246324
2117.106204	290277.491669	38.251341
2118.962370	290726.162557	38.256359
2121.153566	291160.482894	38.261376
2123.305431	291614.737817	38.266394
2125.354811	292061.362961	38.271412
2127.387354	292501.513013	38.276429
2130.117264	292947.415828	38.281447
2132.029560	293397.353269	38.286464
2134.142626	293834.815075	38.291482
2136.121561	294293.773990	38.296500
2138.568608	294730.770708	38.301517
2140.569970	295183.448078	38.306535
2142.900706	295620.634074	38.311552
2145.008889	296059.044851	38.316570
2147.102740	296509.310883	38.321588
2149.416836	296949.256729	38.326605
2151.407162	297394.860558	38.331623
2153.649498	297847.022260	38.336640
2155.687682	298270.930562	38.341658
2157.942300	298697.772107	38.346676
2159.903889	299109.830123	38.351693
2161.917634	299533.910323	38.356711
2163.989905	299951.225216	38.361728
2166.022070	300369.685590	38.366746
2168.192759	300808.150909	38.371764
2170.272199	301234.619292	38.376781
2172.538900	301655.393923	38.381799
2174.370547	302096.795760	38.386816
2176.761163	302514.548698	38.391834
2178.598877	302959.039434	38.396852
2180.974320	303392.983614	38.401869
2182.987140	303842.744944	38.406887
2184.788554	304286.468511	38.411904
2187.158168	304728.779381	38.416922
2189.065504	305200.274483	38.421940
2191.584820	305644.660907	38.426957
2193.379434	306110.377656	38.431975
2195.291894	306580.843777	38.436992
2197.887071	307028.912135	38.442010
2199.910188	307502.144443	38.447028
2201.855133	307970.917087	38.452045
2204.072546	308449.567241	38.457063
2206.535375	308929.088092	38.462080
2208.751134	309406.409254	38.467098
2211.129890	309892.482330	38.472116
2213.515460	310378.828634	38.477133
2215.548470	310864.641385	38.482151
2218.002147	311343.327437	38.487168
2220.401299	311816.534927	38.492186
2222.817864	312314.658634	38.497204
2224.612022	312789.727603	38.502221
2227.222077	313279.815959	38.507239
2229.580731	313759.888078	38.512256
2231.827183	314236.952589	38.517274
2233.651147	314742.985150	38.522292
2235.777137	315238.356452	38.527309
2238.109911	315736.253234	38.532327
2240.714981	316227.630431	38.537344
2243.373244	316711.304355	38.542362
2245.749839	317210.421428	38.547380
2247.736001	317704.188547	38.552397
2250.274073	318192.306181	38.557415
2252.038352	318689.649761	38.562432
2254.655608	319175.663123	38.567450
2256.885559	319675.561761	38.572468
2259.341795	320176.231246	38.577485
2261.746184	320665.610774	38.582503
2263.798874	321160.343195	38.587520
2266.240597	321650.872838	38.592538
2268.647897	322156.677872	38.597556
2271.042964	322640.301328	38.602573
2273.265371	323140.566381	38.607591
2275.267525	323627.640020	38.612608
2278.118216	324109.881054	38.617626
2280.514576	324598.962220	38.622644
2282.299665	325095.110783	38.627661
2285.159187	325591.491202	38.632679
2286.835877	326074.400186	38.637696
2289.266644	326570.607326	38.642714
2291.480231	327067.349754	38.647732
2293.726129	327554.465141	38.652749
2296.235608	328054.802499	38.657767
2298.404984	328551.457216	38.662784
2300.964249	329041.473701	38.667802
2303.142636	329538.393627	38.672820
2305.201960	330028.628186	38.677837
2307.790445	330507.560401	38.682855
2309.903750	330990.746962	38.687872
2312.279563	331456.026605	38.692890
2314.263616	331920.499350	38.697908
2316.310129	332393.353618	38.702925
2318.886282	332857.468633	38.707943
2320.615227	333342.968682	38.712960
2323.147636	333810.325901	38.717978
2325.154188	334297.977161	38.722996
2327.427880	334787.482775	38.728013
2329.752048	335273.016880	38.733031
2331.780469	335772.034923	38.738048
2334.351083	336262.387761	38.743066
2336.549662	336759.133599	38.748084
2338.941849	337257.719411	38.753101
2341.329739	337760.205225	38.758119
2343.411700	338270.112953	38.763136
2346.036581	338775.160100	38.768154
2347.935982	339291.575084	38.773172
2350.383522	339799.197246	38.778189
2353.041174	340309.011227	38.783207
2355.885139	340839.205575	38.788224
2357.929346	341352.270765	38.793242
2360.515114	341875.819605	38.798260
2362.882011	342393.612424	38.803277
2365.100492	342916.619756	38.808295
2367.570515	343447.264112	38.813312
2369.836395	343964.313760	38.818330
2372.445744	344482.595237	38.823348
2374.877157	345012.333809	38.828365
2377.379257	345534.927159	38.833383
2379.917891	346074.978867	38.838400
2382.246465	346596.365709	38.843418
2384.541235	347123.531334	38.848436
2387.474060	347649.270237	38.853453
2389.470303	348181.537317	38.858471
2391.754761	348718.695308	38.863488
2394.485641	349246.900016	38.868506
2397.202794	349770.179327	38.873524
2399.233578	350313.664497	38.878541
2402.049512	350844.695228	38.883559
2404.436727	351377.077396	38.888576
2406.856158	351905.693315	38.893594
2409.195403	352440.651521	38.898612
2411.926283	352972.421055	38.903629
2414.290250	353505.684216	38.908647
2416.083039	354048.103950	38.913664
2418.886781	354573.750630	38.918682
2421.687834	355116.982981	38.923700
2423.840771	355649.203460	38.928717
2426.400760	356188.145190	38.933735
2428.677932	356733.484736	38.938752
2431.272432	357266.749186	38.943770
2433.785969	357813.959257	38.948788
2435.953507	358351.910608	38.953805
2438.436696	358881.159259	38.958823
2440.465232	359429.683675	38.963840
2443.436916	359978.684327	38.968858
2446.022912	360512.070761	38.973876
2448.617069	361063.848171	38.978893
2450.786599	361593.858700	38.983911
2453.255706	362147.359199	38.988928
2455.526493	362681.060352	38.993946
2458.405769	363224.870679	38.998964
2460.656502	363765.043651	39.003981
2463.094846	364303.276537	39.008999
2465.389923	364850.138698	39.014016
2468.125843	365393.474983	39.019034
2470.634468	365935.974991	39.024052
2472.838413	366446.201347	39.029069
2475.281429	366957.242877	39.034087
2477.852562	367477.986261	39.039104
2480.390855	367985.674827	39.044122
2482.638052	368509.237520	39.049140
2485.036452	369025.773119	39.054157
2487.624599	369532.691331	39.059175
2489.665638	370048.706624	39.064192
2491.962763	370576.581410	39.069210
2494.454487	371103.326257	39.074228
2496.973827	371652.860487	39.079245
2499.318244	372180.748135	39.084263
2501.760554	372723.381525	39.089280
2504.570858	373268.910963	39.094298
2507.016413	373817.324168	39.099316
2509.358912	374364.906435	39.104333
2511.705746	374914.275754	39.109351
2513.997512	375478.564208	39.114368
2516.455867	376020.698817	39.119386
2519.104152	376584.959028	39.124404
2521.830483	377161.253327	39.129421
2524.063873	377723.021218	39.134439
2526.680254	378297.610932	39.139456
2529.043582	378869.897356	39.144474
2531.942372	379444.620642	39.149492
2534.197473	380032.527425	39.154509
2536.941073	380592.077486	39.159527
2539.528611	381186.618526	39.164544
2541.737860	381773.733439	39.169562
2544.853942	382356.108984	39.174580
2546.880292	382949.633620	39.179597
2549.511641	383534.818955	39.184615
2552.273561	384141.370570	39.189632
2554.897190	384737.824763	39.194650
2557.832555	385333.811022	39.199668
2559.756743	385929.232351	39.204685
2562.481256	386525.147540	39.209703
2565.284965	387134.305221	39.214720
2567.689793	387730.343086	39.219738
2570.546636	388324.371600	39.224756
2572.927435	388938.286479	39.229773
2575.595970	389531.328049	39.234791
2578.142134	390145.642849	39.239808
2580.842912	390765.336342	39.244826
2583.769471	391367.661214	39.249844
2586.316744	391973.929443	39.254861
2589.187205	392575.119255	39.259879
2591.889862	393186.193744	39.264896
2594.366978	393799.566443	39.269914
2596.691554	394395.733153	39.274932
2599.622508	395015.788212	39.279949
2602.415820	395612.256312	39.284967
2605.110415	396217.331341	39.289984
2607.427091	396822.652528	39.295002
2610.448049	397418.178947	39.300020
2613.235150	398032.608977	39.305037
2615.899554	398629.932214	39.310055
2618.577131	399233.919914	39.315072
2621.225084	399837.441013	39.320090
2624.117501	400433.113153	39.325108
2626.673192	401029.784307	39.330125
2629.452319	401632.073877	39.335143
2632.470514	402232.133894	39.340160
2634.668239	402821.273126	39.345178
2637.206042	403411.558603	39.350196
2639.804646	404009.461219	39.355213
2642.553896	404594.773752	39.360231
2645.311524	405184.219530	39.365248
2648.066207	405757.102424	39.370266
2650.888057	406312.754836	39.375284
2653.310968	406874.983576	39.380301
2655.844218	407430.703892	39.385319
2658.635610	407985.104929	39.390336
2660.810892	408559.979786	39.395354
2663.434530	409115.441290	39.400372
2665.883042	409683.160462	39.405389
2668.305669	410252.437433	39.410407
2671.254491	410826.980215	39.415424
2673.594659	411413.087489	39.420442
2676.207712	411988.360415	39.425460
2678.713192	412579.469416	39.430477
2681.500528	413161.766404	39.435495
2684.193720	413763.386508	39.440512
2686.642846	414346.058404	39.445530
2689.352780	414946.428612	39.450548
2692.045400	415559.834907	39.455565
2694.550933	416159.090057	39.460583
2697.289674	416764.513075	39.465600
2699.694801	417377.456473	39.470618
2702.380982	417990.186333	39.475636
2704.840261	418626.754684	39.480653
2707.267644	419254.357111	39.485671
2710.264046	419892.825786	39.490688
2712.894804	420523.948716	39.495706
2715.545942	421162.078301	39.500724
2718.035054	421819.125686	39.505741
2721.137307	422460.431362	39.510759
2723.820725	423101.883592	39.515776
2726.519793	423758.077501	39.520794
2729.423874	424407.544146	39.525812
2731.836865	425062.881119	39.530829
2734.874787	425717.998002	39.535847
2737.717291	426385.965371	39.540864
2740.349037	427060.161660	39.545882
2743.082232	427724.057191	39.550900
2745.853187	428394.900746	39.555917
2748.606500	429061.225538	39.560935
2751.664997	429726.064860	39.565952
2754.458397	430403.458611	39.570970
2757.161475	431081.196976	39.575988
2759.847371	431750.019162	39.581005
2762.405515	432424.650608	39.586023
2766.008231	433096.922165	39.591040
2768.575140	433777.620504	39.596058
2771.534269	434449.339352	39.601076
2774.201810	435131.894580	39.606093
2776.901057	435802.293001	39.611111
2779.804160	436474.455166	39.616128
2782.694883	437154.124306	39.621146
2785.217329	437817.557275	39.626164
2788.275021	438501.750008	39.631181
2790.849650	439181.547528	39.636199
2794.038228	439871.328706	39.641216
2796.826691	440548.668918	39.646234
2800.102520	441220.300996	39.651252
2803.034124	441903.884381	39.656269
2805.783908	442576.459124	39.661287
2808.693647	443237.164707	39.666304
2811.452340	443908.578416	39.671322
2814.433673	444579.831832	39.676340
2816.688068	445253.699719	39.681357
2819.677681	445925.054135	39.686375
2823.000626	446602.190030	39.691392
2825.193924	447275.285832	39.696410
2828.567316	447941.960770	39.701428
2830.853186	448594.894536	39.706445
2833.630390	449241.264449	39.711463
2836.818628	449875.125475	39.716480
2839.143193	450530.709542	39.721498
2842.214934	451161.766187	39.726516
2844.618317	451796.944039	39.731533
2847.345189	452443.761387	39.736551
2849.957633	453092.188515	39.741568
2852.700311	453753.545455	39.746586
2855.901485	454402.993427	39.751604
2858.619271	455060.519075	39.756621
2861.105615	455721.993411	39.761639
2863.814188	456379.016629	39.766656
2866.341705	457064.156751	39.771674
2869.763151	457740.398581	39.776692
2872.568095	458414.943973	39.781709
2875.203054	459094.586729	39.786727
2878.354167	459788.554873	39.791744
2880.905384	460476.179961	39.796762
2883.612589	461163.450237	39.801780
2886.769302	461869.948206	39.806797
2889.329112	462562.331827	39.811815
2892.650017	463264.356321	39.816832
2895.709911	463972.144026	39.821850
2898.269517	464669.536991	39.826868
2901.415947	465389.309127	39.831885
2904.394167	466101.055690	39.836903
2907.354350	466816.860663	39.841920
2910.149876	467527.061549	39.846938
2913.328473	468248.016617	39.851956
2915.789742	468972.482151	39.856973
2918.963395	469693.980081	39.861991
2922.088788	470419.236337	39.867008
2925.071342	471150.786644	39.872026
2928.103466	471861.419075	39.877044
2931.309309	472593.626153	39.882061
2934.161542	473320.510562	39.887079
2937.035952	474051.745533	39.892096
2939.847249	474781.696748	39.897114
2943.580564	475514.092343	39.902132
2946.873292	476248.439130	39.907149
2949.566024	476980.577446	39.912167
2952.493714	477697.774410	39.917184
2955.220280	478431.000147	39.922202
2958.629107	479159.296746	39.927220
2961.741988	479889.269343	39.932237
2964.810833	480614.527713	39.937255
2968.166570	481342.580438	39.942272
2970.612958	482059.301567	39.947290
2973.986610	482790.811773	39.952308
2976.794232	483509.324714	39.957325
2980.399346	484234.834946	39.962343
2983.416745	484952.492333	39.967360
2986.223553	485683.349990	39.972378
2989.153365	486398.384120	39.977396
2992.366015	487120.041198	39.982413
2995.106779	487845.214050	39.987431
2998.246015	488567.166878	39.992448
3001.440856	489290.033818	39.997466
3004.686265	490012.606545	40.002484
3007.728083	490721.325455	40.007501
3010.642409	491436.779954	40.012519
3013.591891	492148.014794	40.017536
3016.698263	492868.608800	40.022554
3019.896904	493583.664619	40.027572
3023.058793	494278.549592	40.032589
3025.655072	495007.932255	40.037607
3028.752435	495715.700876	40.042624
3031.690726	496423.863289	40.047642
3034.639310	497112.405453	40.052660
3037.672964	497788.970603	40.057677
3040.295173	498470.401678	40.062695
3043.363331	499142.418551	40.067712
3046.315457	499829.473344	40.072730
3048.847550	500502.920754	40.077748
3051.893655	501199.359006	40.082765
3054.478595	501900.164230	40.087783
3057.686074	502591.074641	40.092800
3060.482225	503306.524397	40.097818
3063.093303	504010.896582	40.102836
3066.212122	504734.376906	40.107853
3068.874915	505459.703332	40.112871
3072.276776	506187.996799	40.117888
3075.043117	506925.307856	40.122906
3077.833382	507678.273342	40.127924
3080.970927	508424.755487	40.132941
3083.463108	509183.371968	40.137959
3086.753303	509934.881177	40.142976
3089.823037	510702.630993	40.147994
3092.866928	511482.212477	40.153012
3095.932069	512257.623032	40.158029
3098.590198	513040.094588	40.163047
3101.763688	513819.675606	40.168064
3105.292489	514615.046956	40.173082
3108.363608	515415.421825	40.178100
3111.266036	516209.240259	40.183117
3114.366985	517013.589819	40.188135
3117.773432	517817.844266	40.193152
3120.937582	518621.134000	40.198170
3123.846111	519432.710199	40.203188
3127.627882	520245.207044	40.208205
3130.052489	521060.380236	40.213223
3133.600867	521869.850326	40.218240
3136.503983	522699.625057	40.223258
3139.905400	523530.426243	40.228276
3143.233550	524348.876378	40.233293
3145.983853	525172.642281	40.238311
3149.646602	526003.399007	40.243328
3152.904675	526845.922731	40.248346
3155.852350	527674.124061	40.253364
3159.610509	528506.516768	40.258381
3163.147530	529344.215531	40.263399
3165.894368	530159.030901	40.268416
3169.125583	530999.383550	40.273434
3172.268377	531824.629850	40.278452
3175.477553	532648.457424	40.283469
3178.926093	533497.753624	40.288487
3182.142045	534322.176359	40.293504
3185.316994	535148.761752	40.298522
3188.441216	535982.179674	40.303540
3192.249152	536813.729576	40.308557
3195.254382	537660.259220	40.313575
3198.653087	538477.006595	40.318592
3202.191005	539317.068291	40.323610
3204.514472	540140.200475	40.328628
3208.213298	540960.303798	40.333645
3211.732482	541796.489637	40.338663
3215.153864	542630.226503	40.343680
3218.599503	543439.920920	40.348698
3221.451926	544276.546903	40.353716
3225.066422	545088.666406	40.358733
3228.217298	545918.864198	40.363751
3231.211809	546740.252636	40.368768
3234.541223	547550.900702	40.373786
3237.742284	548385.388639	40.378804
3241.122971	549201.536987	40.383821
3243.885825	550012.863221	40.388839
3247.179298	550802.841726	40.393856
3250.508076	551580.579263	40.398874
3253.577607	552363.973036	40.403892
3256.282949	553140.304152	40.408909
3259.546124	553923.516501	40.413927
3262.692530	554726.496615	40.418944
3266.178855	555511.425434	40.423962
3269.183651	556317.880044	40.428980
3272.207726	557111.096319	40.433997
3275.038670	557915.916544	40.439015
3278.223643	558728.394150	40.444032
3281.316614	559539.778248	40.449050
3284.906414	560359.346290	40.454068
3288.335219	561190.606083	40.459085
3291.407579	562026.171228	40.464103
3294.400087	562861.539116	40.469120
3297.723496	563702.205366	40.474138
3301.189236	564544.441688	40.479156
3304.584513	565399.899955	40.484173
3307.555987	566256.913920	40.489191
3310.835299	567106.255047	40.494208
3314.251023	567957.715552	40.499226
3317.409279	568829.380688	40.504244
3320.589717	569690.713184	40.509261
3323.807875	570581.960954	40.514279
3327.247037	571468.799872	40.519296
3330.642886	572344.114634	40.524314
3334.025619	573238.832810	40.529332
3337.174907	574130.013775	40.534349
3340.575860	575030.292566	40.539367
3343.971400	575922.394442	40.544384
3347.408127	576820.973332	40.549402
3351.227143	577724.923556	40.554420
3354.438000	578623.193017	40.559437
3357.904452	579538.407044	40.564455
3361.108167	580445.984394	40.569472
3364.876745	581344.397016	40.574490
3368.548301	582253.453511	40.579508
3371.857742	583160.491542	40.584525
3375.411584	584072.116540	40.589543
3378.954589	584977.718012	40.594560
3382.095212	585880.007997	40.599578
3385.365707	586804.547330	40.604596
3389.033390	587707.403383	40.609613
3392.535011	588628.452519	40.614631
3395.902138	589548.045006	40.619648
3399.515816	590446.233269	40.624666
3403.030137	591364.048747	40.629684
3406.478099	592271.154266	40.634701
3409.888410	593179.737497	40.639719
3413.449925	594094.064314	40.644736
3417.154233	595005.742900	40.649754
3420.298622	595927.969085	40.654772
3423.811865	596826.135882	40.659789
3427.204623	597741.772734	40.664807
3430.996845	598653.972071	40.669824
3434.112640	599555.563413	40.674842
3437.996491	600473.631464	40.679860
3441.518954	601371.458272	40.684877
3444.708708	602271.705585	40.689895
3448.763578	603184.117442	40.694912
3452.189835	604087.664067	40.699930
3455.333471	604980.447152	40.704948
3458.895944	605879.873530	40.709965
3462.181067	606780.611765	40.714983
3465.814439	607683.860613	40.720000
3469.508814	608580.136255	40.725018
3473.064409	609458.132794	40.730023
3476.362779	610299.654300	40.735028
3479.891664	611083.421118	40.740032
3482.551433	611833.216303	40.745037
3485.649710	612515.898089	40.750042
3488.243047	613157.871704	40.755047
3491.442855	613733.678151	40.760052
3494.267102	614249.980086	40.765056
3496.871549	614715.509012	40.770061
3499.215393	615134.176716	40.775066
3501.281942	615491.348290	40.780071
3503.843701	615797.204570	40.785076
3505.969397	616061.490944	40.790080
3507.150374	616286.489055	40.795085
3509.178812	616456.479881	40.800090
3510.939440	616598.325582	40.805095
3512.315540	616688.858897	40.810100
3513.877111	616757.575033	40.815104
3514.805468	616777.468227	40.820109
3516.361883	616768.379997	40.825114
3517.373413	616719.699844	40.830119
3518.425267	616651.474278	40.835124
3519.253763	616556.048426	40.840128
3519.849144	616448.564743	40.845133
3520.698255	616305.809116	40.850138
3521.138545	616148.922731	40.855143
3521.749391	615959.023748	40.860148
3522.226831	615766.243415	40.865152
3522.524505	615567.290331	40.870157
3522.977415	615333.674224	40.875162
3523.455747	615105.946265	40.880167
3523.902246	614855.476997	40.885172
3523.508625	614589.388543	40.890176
3523.520959	614331.826686	40.895181
3524.229470	614055.705134	40.900186
3524.167399	613791.593111	40.905191
3524.504299	613503.717861	40.910196
3524.730445	613207.803528	40.915200
3524.223958	612920.443387	40.920205
3524.701152	612612.074785	40.925210
3524.472605	612316.955308	40.930215
3524.305308	611996.220382	40.935220
3524.368571	611691.788030	40.940224
3523.964692	611386.869585	40.945229
3524.183636	611070.444776	40.950234
3524.219066	610768.439027	40.955239
3523.720712	610450.857028	40.960244
3523.928212	610143.355553	40.965248
3523.691254	609826.663276	40.970253
3523.877719	609515.845787	40.975258
3523.392967	609207.724192	40.980263
3523.219458	608881.090949	40.985268
3523.379756	608576.350161	40.990272
3522.798367	608270.365884	40.995277
3522.589263	607960.813238	41.000282
3522.593767	607657.819957	41.005287
3521.942297	607341.015394	41.010292
3521.972430	607041.751219	41.015296
3521.474140	606745.011931	41.020301
3521.740554	606434.888715	41.025306
3521.306229	606146.375767	41.030311
3521.266554	605862.795513	41.035316
3520.795306	605565.217568	41.040320
3520.448857	605283.370216	41.045325
3520.585233	604992.434475	41.050330
3520.563387	604704.617158	41.055335
3519.816162	604418.756397	41.060340
3519.783434	604142.232295	41.065344
3519.757869	603879.309040	41.070349
3519.679377	603608.781971	41.075354
3519.089983	603329.321053	41.080359
3518.628823	603059.590033	41.085364
3518.681145	602787.519951	41.090368
3518.223464	602530.034335	41.095373
3518.216385	602261.562717	41.100378
3517.760953	602020.527990	41.105383
3517.585794	601762.678960	41.110388
3517.631925	601518.701675	41.115392
3517.324860	601263.713532	41.120397
3517.135713	601017.258957	41.125402
3516.908490	600778.011615	41.130407
3516.877358	600543.683133	41.135412
3517.149591	600305.698268	41.140416
3516.811483	600056.941974	41.145421
3516.435785	599815.293300	41.150426
3515.968504	599596.228161	41.155431
3515.794430	599356.289308	41.160436
3515.391389	599133.550370	41.165440
3515.249379	598927.235030	41.170445
3514.956639	598699.463832	41.175450
3514.895148	598504.040496	41.180455
3514.663633	598283.859862	41.185460
3514.502775	598066.366936	41.190464
3514.229885	597864.356561	41.195469
3513.978550	597645.417259	41.200474
3513.763621	597448.796793	41.205479
3513.643152	597273.586151	41.210484
3513.607891	597074.577527	41.215488
3513.247493	596880.021953	41.220493
3512.919596	596689.413147	41.225498
3512.864944	596507.370162	41.230503
3512.786056	596331.035865	41.235508
3512.455013	596144.974150	41.240512
3511.877402	595962.452764	41.245517
3512.056680	595791.677212	41.250522
3511.991424	595629.099162	41.255527
3511.869624	595454.810019	41.260532
3511.664556	595289.093918	41.265536
3511.375998	595124.540034	41.270541
3511.539168	594956.307446	41.275546
3510.969190	594803.911197	41.280551
3511.481004	594647.036909	41.285556
3511.097212	594480.084176	41.290560
3510.840125	594325.028035	41.295565
3510.643190	594168.357652	41.300570
3510.576075	594030.445164	41.305575
3510.508670	593871.296183	41.310580
3510.467558	593725.011980	41.315584
3510.108358	593590.044253	41.320589
3510.566212	593434.612980	41.325594
3509.833003	593287.529461	41.330599
3510.047295	593147.958864	41.335604
3509.794649	593014.569939	41.340608
3509.744604	592880.045770	41.345613
3509.530192	592745.245081	41.350618
3509.138235	592609.468690	41.355623
3508.770299	592477.142931	41.360628
3508.722553	592347.620563	41.365632
3508.727367	592243.884609	41.370637
3508.725269	592114.702918	41.375642
3508.571271	591990.853044	41.380647
3508.273764	591873.886695	41.385652
3508.187969	591755.884134	41.390656
3508.464005	591641.179907	41.395661
3508.008909	591521.729730	41.400666
3508.218497	591409.888722	41.405671
3508.234319	591303.336716	41.410676
3507.745676	591188.146064	41.415680
3507.578270	591091.990176	41.420685
3507.848923	590971.468620	41.425690
3507.737096	590877.606523	41.430695
3507.602644	590770.521673	41.435700
3507.282687	590666.169994	41.440704
3507.272751	590560.516402	41.445709
3507.301269	590454.755566	41.450714
3507.141498	590363.401379	41.455719
3507.007548	590267.533485	41.460724
3506.967567	590166.990812	41.465728
3506.961593	590080.469817	41.470733
3506.778365	589970.579055	41.475738
3506.533282	589877.931484	41.480743
3506.450639	589787.662575	41.485748
3506.684809	589697.343385	41.490752
3506.656659	589615.030650	41.495757
3506.834244	589521.812928	41.500762
3506.328041	589436.517324	41.505767
3506.636772	589355.903546	41.510772
3506.455840	589263.240671	41.515776
3506.141600	589176.259586	41.520781
3506.252786	589091.916928	41.525786
3505.991568	589012.341669	41.530791
3505.907575	588930.884234	41.535796
3506.030659	588845.435483	41.540800
3506.277284	588761.620238	41.545805
3506.192839	588687.175854	41.550810
3505.549175	588605.402611	41.555815
3505.615783	588523.818356	41.560820
3506.114615	588459.202391	41.565824
3505.356093	588384.610768	41.570829
3505.588438	588297.938036	41.575834
3505.530162	588224.388324	41.580839
3505.480579	588160.507722	41.585844
3505.527082	588082.481000	41.590848
3505.061629	588020.418399	41.595853
3505.235748	587949.837051	41.600858
3505.279655	587883.985931	41.605863
3505.307245	587806.260839	41.610868
3505.415796	587741.150401	41.615872
3505.281380	587673.271348	41.620877
3505.187653	587607.790845	41.625882
3504.788441	587546.767512	41.630887
3504.805350	587483.423757	41.635892
3505.255845	587408.135292	41.640896
3504.832084	587352.576922	41.645901
3504.844214	587280.463067	41.650906
3504.813878	587224.341411	41.655911
3505.112406	587152.783293	41.660916
3505.072432	587091.500791	41.665920
3504.491196	587034.111208	41.670925
3504.565451	586968.650709	41.675930
3504.628958	586918.576611	41.680935
3504.732759	586859.475357	41.685940
3504.587670	586798.107406	41.690944
3504.121703	586739.695951	41.695949
3504.234083	586685.253120	41.700954
3504.420366	586633.103784	41.705959
3503.998486	586579.896606	41.710964
3504.118280	586527.205883	41.715968
3503.955842	586474.358560	41.720973
3504.156051	586427.518400	41.725978
3504.366719	586381.578506	41.730983
3504.120658	586329.294838	41.735988
3503.959283	586275.193457	41.740992
3504.069550	586243.301512	41.745997
3504.374339	586181.909879	41.751002
3503.986112	586132.955263	41.756007
3503.847833	586071.932984	41.761012
3504.138900	586028.384710	41.766016
3503.542692	585982.619393	41.771021
3504.039372	585931.019602	41.776026
3503.905432	585884.880896	41.781031
3503.819585	585842.042350	41.786036
3504.023680	585787.430344	41.791040
3503.611782	585742.186520	41.796045
3503.903522	585699.037787	41.801050
3503.506718	585655.896283	41.806055
3503.433829	585606.338685	41.811060
3503.739931	585568.499951	41.816064
3503.293831	585534.938694	41.821069
3503.649059	585490.476076	41.826074
3503.700172	585446.862756	41.831079
3503.615225	585408.332783	41.836084
3503.859014	585365.089987	41.841088
3503.769068	585331.322064	41.846093
3503.983094	585274.300105	41.851098
3503.972978	585236.208924	41.856103
3503.519720	585183.801794	41.861108
3503.616733	585123.439146	41.866112
3503.631899	585095.869262	41.871117
3503.767358	585051.990570	41.876122
3503.489875	585007.574779	41.881127
3503.763071	584961.368528	41.886132
3503.877092	584929.823029	41.891136
3503.574707	584887.215087	41.896141
3503.607813	584835.983349	41.901146
3503.460356	584796.809384	41.906151
3503.379230	584751.509748	41.911156
3503.484575	584709.388742	41.916160
3503.539794	584669.781643	41.921165
3503.760728	584627.742502	41.926170
3503.595469	584583.157071	41.931175
3503.148957	584536.460039	41.936180
3503.503908	584503.021013	41.941184
3503.449832	584474.307505	41.946189
3503.373567	584425.396721	41.951194
3503.904255	584390.426106	41.956199
3503.647749	584344.199811	41.961204
3503.560570	584297.044576	41.966208
3503.543453	584257.246791	41.971213
3503.251898	584212.178328	41.976218
3503.041578	584183.538611	41.981223
3503.599569	584139.339580	41.986228
3503.433751	584103.725030	41.991232
3503.642876	584072.212326	41.996237
3503.284014	584020.386398	42.001242
3503.294344	583983.290219	42.006247
3503.809086	583943.558535	42.011252
3503.906377	583897.475562	42.016256
3503.705890	583856.151014	42.021261
3503.570410	583809.602777	42.026266
3503.701836	583773.790304	42.031271
3503.629704	583722.720207	42.036276
3503.458662	583692.318553	42.041280
3503.095864	583658.838777	42.046285
3503.070729	583605.404710	42.051290
3503.176648	583583.080436	42.056295
3503.009262	583547.113420	42.061300
3503.712054	583507.400895	42.066304
3503.171011	583471.742694	42.071309
3503.172859	583427.176573	42.076314
3503.288089	583391.465648	42.081319
3503.268051	583358.382548	42.086324
3503.619209	583316.819342	42.091328
3503.312833	583281.324361	42.096333
3503.362903	583242.414755	42.101338
3503.360087	583198.450012	42.106343
3503.044755	583169.523278	42.111348
3503.081598	583125.652307	42.116352
3502.772825	583091.460511	42.121357
3503.319275	583069.467384	42.126362
3503.514492	583036.099005	42.131367
3503.261668	582994.729268	42.136372
3503.510104	582949.170151	42.141376
3503.374960	582913.296286	42.146381
3503.435199	582876.740034	42.151386
3503.570686	582828.440768	42.156391
3503.272257	582800.613349	42.161396
3503.168967	582760.372419	42.166400
3503.181342	582728.786361	42.171405
3502.879951	582680.705144	42.176410
3503.144285	582653.090179	42.181415
3503.295937	582621.331638	42.186420
3503.451586	582591.176675	42.191424
3502.874983	582548.101181	42.196429
3503.014168	582502.005818	42.201434
3503.531807	582474.802019	42.206439
3503.115894	582438.469154	42.211444
3503.404052	582402.477318	42.216448
3503.197681	582366.813350	42.221453
3502.961055	582325.338297	42.226458
3503.314781	582303.072963	42.231463
3502.820703	582255.521368	42.236468
3502.979551	582222.457029	42.241472
3502.681295	582196.031857	42.246477
3502.806649	582165.379107	42.251482
3502.850960	582131.881177	42.256487
3502.603608	582101.386787	42.261492
3503.019497	582074.348319	42.266496
3502.952694	582041.418986	42.271501
3502.969231	581997.145608	42.276506
3502.676347	581966.958785	42.281511
3502.617877	581946.161006	42.286516
3502.974235	581914.268158	42.291520
3502.648467	581881.779930	42.296525
3502.579979	581845.240386	42.301530
3502.693603	581818.850197	42.306535
3502.397745	581791.120102	42.311540
3502.551214	581765.325210	42.316544
3502.737396	581749.151637	42.321549
3502.853050	581718.699717	42.326554
3502.636556	581688.450052	42.331559
3502.767804	581659.098571	42.336564
3503.026792	581626.468040	42.341568
3502.648061	581603.914696	42.346573
3502.757676	581570.705689	42.351578
3502.741432	581537.014868	42.356583
3502.368013	581509.947998	42.361588
3502.949246	581492.559094	42.366592
3503.091515	581468.219296	42.371597
3502.919294	581441.923034	42.376602
3502.859564	581403.575644	42.381607
3502.722298	581374.566222	42.386612
3503.030840	581330.094107	42.391616
3502.615655	581307.144736	42.396621
3502.741024	581266.862618	42.401626
3502.758598	581240.586347	42.406631
3502.697867	581217.330678	42.411636
3502.761534	581186.133314	42.416640
3502.761098	581167.079916	42.421645
3502.752634	581129.174827	42.426650
3502.584518	581111.250642	42.431655
3502.633123	581076.144337	42.436660
3502.716477	581044.843216	42.441664
3502.268560	581010.566441	42.446669
3502.637193	580998.625261	42.451674
3502.851937	580964.595740	42.456679
3502.825871	580944.442852	42.461684
3502.946521	580910.979434	42.466688
3502.620330	580883.703080	42.471693
3502.367273	580848.041508	42.476698
3502.671237	580822.321179	42.481703
3502.628368	580800.866961	42.486708
3502.877621	580767.633717	42.491712
3502.758955	580748.547939	42.496717
3502.795297	580711.787696	42.501722
3502.607965	580677.318724	42.506727
3502.332789	580650.986534	42.511732
3502.523194	580622.876635	42.516736
3502.390645	580601.887338	42.521741
3502.707515	580575.662989	42.526746
3503.008521	580555.859410	42.531751
3502.736028	580528.523644	42.536756
3502.333313	580483.256741	42.541760
3502.285062	580464.711047	42.546765
3502.552212	580438.444003	42.551770
3502.868832	580421.445801	42.556775
3502.657322	580406.535897	42.561780
3502.681496	580365.313588	42.566784
3502.645714	580341.901749	42.571789
3502.356053	580310.506437	42.576794
3502.686857	580286.084428	42.581799
3502.819803	580261.191849	42.586804
3503.243277	580232.944239	42.591808
3502.827406	580201.768929	42.596813
3502.633635	580169.706344	42.601818
3502.736426	580134.438154	42.606823
3502.554312	580115.712222	42.611828
3502.833365	580090.946858	42.616832
3502.814455	580057.352249	42.621837
3502.515325	580015.226416	42.626842
3502.797939	579996.427633	42.631847
3502.659621	579965.158122	42.636852
3502.724153	579937.467336	42.641856
3502.643296	579911.704767	42.646861
3502.801772	579888.111165	42.651866
3503.231173	579844.516843	42.656871
3502.838467	579827.227450	42.661876
3502.465571	579787.770058	42.666880
3502.320424	579764.925716	42.671885
3502.529502	579737.863746	42.676890
3503.008786	579712.314032	42.681895
3502.286440	579694.574493	42.686900
3502.636022	579656.157076	42.691904
3502.538829	579631.650098	42.696909
3502.636034	579610.171681	42.701914
3502.575586	579584.605755	42.706919
3502.360856	579553.447327	42.711924
3502.491359	579528.202455	42.716928
3502.615548	579509.477766	42.721933
3502.531060	579484.868182	42.726938
3502.515834	579458.743267	42.731943
3502.479557	579438.940281	42.736948
3502.518825	579395.455340	42.741952
3501.999620	579379.839928	42.746957
3502.301639	579354.517701	42.751962
3502.724631	579337.701814	42.756967
3502.704214	579313.232281	42.761972
3502.785082	579266.831694	42.766976
3502.949532	579251.359973	42.771981
3502.675427	579222.015271	42.776986
3502.240941	579187.931360	42.781991
3502.183428	579169.585551	42.786996
3502.632843	579142.685164	42.792001
3502.406849	579131.436741	42.797005
3502.541596	579109.048794	42.802010
3502.773000	579083.586542	42.807015
3502.200017	579052.482716	42.812020
3502.653038	579020.115104	42.817025
3502.681789	578992.427562	42.822029
3502.339512	578967.656533	42.827034
3502.417628	578946.831779	42.832039
3502.356845	578934.153112	42.837044
3502.439359	578901.040665	42.842049
3502.401552	578871.206741	42.847053
3502.474422	578849.530060	42.852058
3502.779195	578824.808014	42.857063
3502.406092	578802.348389	42.862068
3502.507992	578782.823545	42.867073
3502.318647	578755.871628	42.872077
3501.951258	578728.094903	42.877082
3502.259717	578700.362910	42.882087
3502.339047	578691.072379	42.887092
3502.155772	578669.435391	42.892097
3501.590717	578657.386912	42.897101
3502.005597	578629.738410	42.902106
3502.076701	578610.719599	42.907111
3502.072034	578598.382842	42.912116
3502.160697	578564.315543	42.917121
3501.766229	578554.045767	42.922125
3501.790597	578529.015836	42.927130
3502.204104	578515.460108	42.932135
3501.906367	578497.602120	42.937140
3501.867092	578471.578957	42.942145
3502.041493	578468.492318	42.947149
3501.780923	578446.114688	42.952154
3502.280448	578426.326449	42.957159
3502.554159	578416.604079	42.962164
3502.227948	578393.735076	42.967169
3502.101220	578369.831776	42.972173
3502.093192	578355.489148	42.977178
3501.856993	578329.747206	42.982183
3502.273725	578317.595029	42.987188
3502.371267	578300.678002	42.992193
3502.788987	578283.058899	42.997197
3502.464637	578263.449321	43.002202
3502.374318	578233.922825	43.007207
3502.330790	578204.188320	43.012212
3503.009415	578178.754402	43.017217
3502.711197	578150.514038	43.022221
3502.215147	578130.479680	43.027226
3502.300280	578106.091308	43.032231
3502.343918	578082.662305	43.037236
3502.366441	578062.195675	43.042241
3502.116038	578042.172910	43.047245
3502.014699	578020.722474	43.052250
3502.181041	577980.522368	43.057255
3502.258770	577985.776429	43.062260
3502.406489	577948.789036	43.067265
3502.139709	577935.338955	43.072269
3502.123196	577910.915893	43.077274
3502.282259	577891.380555	43.082279
3502.036215	577877.475765	43.087284
3502.002623	577856.666444	43.092289
3501.971669	577833.198423	43.097293
3501.694107	577810.772020	43.102298
3501.718124	577795.169771	43.107303
3501.643715	577787.056106	43.112308
3502.101775	577766.420536	43.117313
3501.805168	577750.667724	43.122317
3501.975035	577741.813656	43.127322
3502.206545	577718.755769	43.132327
3502.027529	577699.072323	43.137332
3502.023163	577690.496233	43.142337
3501.898644	577653.450110	43.147341
3502.178383	577636.904848	43.152346
3502.513641	577633.241113	43.157351
3501.990613	577608.695947	43.162356
3502.297834	577595.657291	43.167361
3502.570964	577571.388835	43.172365
3502.424099	577548.490063	43.177370
3502.371317	577524.172140	43.182375
3502.186344	577504.188340	43.187380
3502.299404	577484.157913	43.192385
3502.368724	577457.363055	43.197389
3502.010651	577433.644392	43.202394
3502.545752	577416.005579	43.207399
3502.107835	577397.515697	43.212404
3502.143770	577365.058031	43.217409
3501.868144	577350.103897	43.222413
3502.251728	577337.053004	43.227418
3502.272506	577307.857801	43.232423
3501.961635	577297.072216	43.237428
3502.092311	577273.226649	43.242433
3502.050047	577250.561706	43.247437
3502.251338	577231.219249	43.252442
3502.093539	577212.735429	43.257447
3502.203284	577205.445247	43.262452
3502.284476	577173.230743	43.267457
3502.168026	577152.332749	43.272461
3501.693461	577140.820223	43.277466
3502.522377	577120.225809	43.282471
3502.127269	577090.292513	43.287476
3502.105038	577072.940926	43.292481
3502.264167	577065.492455	43.297485
3502.189388	577034.555912	43.302490
3502.325791	577017.580713	43.307495
3502.570097	576993.365673	43.312500
3502.346980	576971.129712	43.317505
3502.300784	576958.948119	43.322509
3502.011175	576937.926315	43.327514
3501.998966	576904.020213	43.332519
3502.183900	576897.319994	43.337524
3502.236960	576862.901965	43.342529
3502.601590	576855.471390	43.347533
3502.291767	576839.970160	43.352538
3502.303363	576809.069653	43.357543
3501.916079	576794.031910	43.362548
3501.830215	576776.539330	43.367553
3501.760798	576749.714310	43.372557
3502.130106	576745.142078	43.377562
3502.066648	576714.253042	43.382567
3501.602014	576700.330799	43.387572
3502.069267	576695.341949	43.392577
3501.889120	576670.941765	43.397581
3501.845497	576657.104134	43.402586
3501.882793	576628.907800	43.407591
3502.125813	576622.098015	43.412596
3502.216941	576594.444950	43.417601
3502.149574	576591.445754	43.422605
3501.905913	576572.773657	43.427610
3502.045498	576546.818382	43.432615
3501.868184	576534.205373	43.437620
3502.220169	576510.173104	43.442625
3502.108631	576489.925207	43.447629
3502.120607	576473.971871	43.452634
3502.134363	576454.456748	43.457639
3501.930041	576439.139118	43.462644
3502.113406	576414.631387	43.467649
3501.855973	576394.707097	43.472653
3501.608307	576369.213247	43.477658
3502.099048	576355.642844	43.482663
3502.042260	576346.321487	43.487668
3501.772167	576328.154737	43.492673
3502.122903	576317.967053	43.497677
3502.487183	576289.417775	43.502682
3501.715056	576274.389334	43.507687
3501.675277	576255.484185	43.512692
3501.958236	576237.732458	43.517697
3502.209873	576225.904811	43.522701
3502.203211	576214.067369	43.527706
3502.495857	576197.016343	43.532711
3502.078997	576179.173274	43.537716
3501.925610	576149.249840	43.542721
3502.313426	576138.203423	43.547725
3502.186150	576102.306361	43.552730
3502.461717	576088.869602	43.557735
3501.961353	576074.851839	43.562740
3502.219256	576043.509414	43.567745
3502.325958	576019.614771	43.572749
3502.180827	575993.251255	43.577754
3502.473797	575984.276232	43.582759
3502.478245	575972.035487	43.587764
3502.632752	575938.050243	43.592769
3502.329326	575918.483447	43.597773
3502.054676	575890.233698	43.602778
3502.209002	575867.083751	43.607783
3502.285148	575846.705026	43.612788
3502.352638	575827.932883	43.617793
3502.165500	575802.679108	43.622797
3501.946246	575790.172148	43.627802
3501.884235	575755.517895	43.632807
3501.924633	575749.040249	43.637812
3502.376118	575734.572269	43.642817
3501.979753	575717.628231	43.647821
3502.002994	575707.942679	43.652826
3502.043798	575670.111688	43.657831
3502.059670	575664.691299	43.662836
3502.268154	575645.796481	43.667841
3502.406339	575625.257160	43.672845
3501.894345	575602.210834	43.677850
3502.016846	575585.988133	43.682855
3501.698766	575559.951632	43.687860
3501.895382	575544.720601	43.692865
3501.814173	575534.499404	43.697869
3501.925559	575516.071041	43.702874
3502.009365	575498.700446	43.707879
3502.110929	575487.698144	43.712884
3502.362773	575469.348079	43.717889
3502.111876	575457.297191	43.722893
3501.807774	575439.084153	43.727898
3502.276233	575414.228681	43.732903
3501.978446	575393.857426	43.737908
3501.772430	575369.709293	43.742913
3502.070622	575357.271460	43.747917
3502.276387	575338.577220	43.752922
3502.130995	575316.225498	43.757927
3501.923533	575304.568990	43.762932
3502.145229	575278.447456	43.767937
3502.273132	575256.654896	43.772941
3502.297953	575248.172713	43.777946
3502.138475	575204.251074	43.782951
3502.137835	575204.802958	43.787956
3502.083523	575176.567139	43.792961
3501.852879	575162.405735	43.797965
3501.712852	575151.139866	43.802970
3502.174109	575124.980527	43.807975
3501.918090	575120.555566	43.812980
3501.647254	575089.042307	43.817985
3501.903200	575074.704389	43.822989
3501.730888	575061.687601	43.827994
3501.785303	575037.648547	43.832999
3501.920867	575038.931668	43.838004
3501.987260	575011.880601	43.843009
3502.240109	575007.225541	43.848013
3502.052720	574995.565576	43.853018
3501.907885	574974.718138	43.858023
3501.932109	574965.683984	43.863028
3501.941969	574953.090107	43.868033
3502.088611	574931.344159	43.873037
3501.740076	574912.986710	43.878042
3502.081806	574883.283522	43.883047
3501.711286	574883.592232	43.888052
3501.747358	574864.823398	43.893057
3502.094589	574842.443895	43.898061
3502.077188	574836.376113	43.903066
3501.831515	574812.132646	43.908071
3502.092356	574799.348856	43.913076
3501.970031	574776.239920	43.918081
3502.147879	574762.766693	43.923085
3501.607093	574742.331909	43.928090
3502.006261	574712.067429	43.933095
3501.908439	574712.383682	43.938100
3502.053932	574691.189316	43.943105
3501.778355	574677.887210	43.948109
3501.761271	574665.949431	43.953114
3501.684073	574636.361256	43.958119
3501.817974	574622.643882	43.963124
3501.922964	574612.643591	43.968129
3502.135842	574591.940205	43.973133
3501.971605	574584.590820	43.978138
3501.887837	574550.688818	43.983143
3502.127205	574547.691295	43.988148
3502.325753	574528.595482	43.993153
3502.314980	574507.525542	43.998157
3501.793313	574488.993786	44.003162
3501.937979	574469.454761	44.008167
3501.941695	574456.058561	44.013172
3501.701640	574429.304860	44.018177
3502.087535	574414.243400	44.023181
3501.736562	574406.872920	44.028186
3501.609583	574389.583743	44.033191
3501.667260	574383.453809	44.038196
3501.795889	574373.299098	44.043201
3501.667387	574348.584779	44.048205
3501.792097	574343.648453	44.053210
3501.761137	574323.685091	44.058215
3502.303206	574318.282138	44.063220
3501.833076	574292.667849	44.068225
3502.361855	574278.938500	44.073229
3502.050296	574266.042905	44.078234
3501.907121	574248.856387	44.083239
3501.853918	574221.019379	44.088244
3501.551883	574212.637687	44.093249
3501.955738	574199.178630	44.098253
3501.834958	574180.834555	44.103258
3501.744201	574166.148311	44.108263
3501.799471	574160.470181	44.113268
3501.688208	574132.692204	44.118273
3501.955984	574126.980837	44.123277
3501.824458	574120.529134	44.128282
3502.039650	574093.452608	44.133287
3501.968426	574087.693872	44.138292
3502.081312	574052.304635	44.143297
3501.967886	574050.666619	44.148301
3501.447490	574028.722178	44.153306
3501.777261	574012.464817	44.158311
3501.773005	574008.903167	44.163316
3501.898888	573987.660377	44.168321
3501.698864	573962.003112	44.173325
3501.299896	573961.613869	44.178330
3501.526880	573955.457237	44.183335
3501.533857	573939.902482	44.188340
3501.922352	573914.403971	44.193345
3501.692265	573906.111149	44.198349
3501.566218	573893.938724	44.203354
3501.689924	573875.305069	44.208359
3501.998402	573866.727332	44.213364
3501.393410	573858.643604	44.218369
3501.809200	573831.785961	44.223373
3501.860666	573838.952659	44.228378
3501.907943	573821.334330	44.233383
3502.037556	573807.466120	44.238388
3501.450818	573795.164914	44.243393
3501.616481	573786.860311	44.248397
3501.367514	573768.334912	44.253402
3501.343038	573751.982036	44.258407
3501.381977	573750.169635	44.263412
3501.492569	573742.927260	44.268417
3501.542098	573731.279124	44.273421
3501.554716	573721.894574	44.278426
3501.866565	573707.445839	44.283431
3501.849471	573699.019221	44.288436
3501.495602	573685.226443	44.293441
3501.774414	573666.166803	44.298445
3501.605983	573664.587503	44.303450
3501.528935	573647.791128	44.308455
3501.535923	573628.723745	44.313460
3501.657707	573634.876092	44.318465
3501.913595	573631.123133	44.323469
3501.763558	573599.737357	44.328474
3501.512556	573573.936657	44.333479
3501.506848	573584.624674	44.338484
3501.144760	573563.708246	44.343489
3501.263659	573551.196112	44.348493
3501.094087	573539.682381	44.353498
3501.586486	573529.771096	44.358503
3501.634853	573530.917498	44.363508
3501.434746	573520.261491	44.368513
3501.833205	573501.885319	44.373517
3501.256000	573499.316226	44.378522
3501.514823	573489.692295	44.383527
3501.884587	573498.164173	44.388532
3501.749340	573469.485169	44.393537
3502.321620	573455.145926	44.398541
3501.966706	573444.313349	44.403546
3501.943615	573427.809263	44.408551
3501.909656	573410.353522	44.413556
3501.656582	573385.204995	44.418561
3501.799099	573375.197746	44.423565
3501.483799	573367.168727	44.428570
3501.875563	573344.729132	44.433575
3501.799506	573338.167960	44.438580
3501.173803	573323.514074	44.443585
3501.589739	573313.815258	44.448589
3501.406510	573299.945158	44.453594
3501.514976	573290.846322	44.458599
3501.369115	573292.123463	44.463604
3501.004493	573280.639960	44.468609
3501.488524	573275.245591	44.473613
3501.337084	573262.373993	44.478618
3501.458502	573245.696524	44.483623
3501.433869	573240.130776	44.488628
3501.735864	573239.280692	44.493633
3501.858261	573220.646166	44.498637
3501.782466	573205.705456	44.503642
3501.581411	573195.199821	44.508647
3501.499792	573189.291723	44.513652
3501.864721	573172.525902	44.518657
3501.977741	573166.537189	44.523661
3501.841173	573150.100615	44.528666
3501.752209	573128.337862	44.533671
3501.959222	573117.617832	44.538676
3501.263337	573100.214914	44.543681
3501.722304	573080.373479	44.548685
3501.565802	573071.516597	44.553690
3502.026486	573069.186565	44.558695
3501.727423	573051.370300	44.563700
3501.726692	573037.270642	44.568705
3502.014400	573028.344283	44.573709
3501.471525	573011.218370	44.578714
3501.606477	572988.416803	44.583719
3501.732405	572988.898831	44.588724
3501.677779	572982.233748	44.593729
3501.859396	572959.475005	44.598733
3501.652803	572953.937563	44.603738
3501.780880	572944.885562	44.608743
3501.652164	572917.107333	44.613748
3501.929428	572915.107010	44.618753
3501.191719	572896.706766	44.623757
3501.485463	572879.198978	44.628762
3501.608480	572865.431004	44.633767
3501.735731	572869.375093	44.638772
3501.991803	572854.783463	44.643777
3501.668350	572834.261070	44.648781
3501.619659	572823.580737	44.653786
3501.756413	572814.627632	44.658791
3501.885350	572797.747618	44.663796
3501.678638	572786.339283	44.668801
3501.833837	572767.548352	44.673805
3501.517994	572745.770155	44.678810
3502.030906	572738.464246	44.683815
3501.317822	572727.536438	44.688820
3501.780479	572711.657872	44.693825
3501.629770	572704.305148	44.698829
3502.012457	572702.639557	44.703834
3502.031344	572678.099266	44.708839
3501.801509	572669.303712	44.713844
3501.361243	572655.523185	44.718849
3501.358996	572627.875013	44.723853
3501.580226	572623.625355	44.728858
3501.615124	572614.186227	44.733863
3501.636456	572617.043028	44.738868
3501.771202	572596.398396	44.743873
3501.705870	572584.967756	44.748877
3501.703612	572576.537985	44.753882
3501.973755	572551.255636	44.758887
3501.928512	572530.187410	44.763892
3501.644665	572522.955741	44.768897
3501.749284	572496.243948	44.773901
3501.561689	572495.470348	44.778906
3501.834452	572481.527963	44.783911
3501.147751	572465.828731	44.788916
3501.399690	572449.029331	44.793921
3502.034899	572451.940745	44.798925
3501.790297	572449.118692	44.803930
3501.745033	572430.709800	44.808935
3501.980578	572410.049073	44.813940
3501.690868	572399.707098	44.818945
3502.089404	572376.812920	44.823949
3501.771635	572372.848149	44.828954
3502.082176	572358.397908	44.833959
3501.659768	572335.080003	44.838964
3501.743245	572331.453932	44.843969
3501.721437	572303.657490	44.848973
3501.671758	572294.080778	44.853978
3501.802876	572297.271759	44.858983
3502.090358	572288.796479	44.863988
3501.861672	572263.742015	44.868993
3501.656006	572245.006635	44.873997
3502.162328	572220.338977	44.879002
3501.643021	572205.817550	44.884007
3501.922907	572206.426087	44.889012
3501.847393	572177.834844	44.894017
3502.138929	572164.742209	44.899021
3502.059955	572150.051512	44.904026
3502.130456	572133.982544	44.909031
3501.751846	572122.550233	44.914036
3501.966240	572099.684285	44.919041
3502.006765	572077.246922	44.924045
3501.742350	572063.438184	44.929050
3501.622394	572049.556664	44.934055
3501.791076	572044.813192	44.939060
3501.695742	572027.063832	44.944065
3501.679498	571994.247623	44.949069
3501.743437	571999.155362	44.954074
3501.859940	571987.946604	44.959079
3501.912445	571969.471501	44.964084
3501.792152	571959.755001	44.969089
3501.888727	571929.931872	44.974093
3501.991567	571918.122999	44.979098
3501.563990	571909.508314	44.984103
3501.717108	571890.515535	44.989108
3501.540925	571884.370631	44.994113
3502.094021	571876.104433	44.999117
3501.964058	571864.783538	45.004122
3501.411067	571838.223188	45.009127
3501.570826	571836.491960	45.014132
3501.620765	571813.550783	45.019137
3501.742390	571794.713314	45.024141
3501.677758	571790.608401	45.029146
3501.615109	571778.172882	45.034151
3501.571554	571751.984334	45.039156
3501.634058	571757.143315	45.044161
3501.813231	571742.763015	45.049165
3501.560272	571729.604454	45.054170
3501.612534	571721.215709	45.059175
3501.670881	571708.510285	45.064180
3501.189671	571707.682165	45.069185
3501.356412	571685.876676	45.074189
3501.632339	571672.585187	45.079194
3502.037527	571679.145938	45.084199
3501.709301	571658.571983	45.089204
3501.527304	571642.240696	45.094209
3501.510555	571623.524943	45.099213
3501.320762	571628.020859	45.104218
3501.461301	571624.586376	45.109223
3501.724522	571615.763109	45.114228
3501.429278	571601.657529	45.119233
3501.667234	571583.152808	45.124237
3501.661241	571589.175691	45.129242
3501.785402	571560.902968	45.134247
3501.750149	571546.907226	45.139252
3500.916343	571537.452459	45.144257
3501.136258	571534.959028	45.149261
3501.574270	571545.679962	45.154266
3501.547847	571522.750138	45.159271
3501.767465	571507.761016	45.164276
3501.547277	571500.619109	45.169281
3501.620431	571485.351752	45.174285
3501.090670	571469.927708	45.179290
3501.407166	571460.142499	45.184295
3501.596061	571454.241394	45.189300
3501.493295	571453.103171	45.194305
3501.515519	571441.958800	45.199309
3501.340144	571421.109601	45.204314
3501.613342	571411.531856	45.209319
3501.621717	571419.359210	45.214324
3501.490666	571409.342818	45.219329
3501.443512	571378.135559	45.224333
3501.478561	571384.101950	45.229338
3501.457235	571373.666899	45.234343
3501.436761	571365.891476	45.239348
3501.412080	571356.059145	45.244353
3501.913028	571335.154245	45.249357
3501.307167	571331.434882	45.254362
3501.473298	571321.321770	45.259367
3501.969812	571314.519366	45.264372
3501.434362	571304.365363	45.269377
3501.583102	571281.909518	45.274381
3501.215196	571288.340429	45.279386
3501.374291	571275.719143	45.284391
3501.429210	571255.034378	45.289396
3501.429897	571245.950759	45.294401
3501.803515	571241.476027	45.299405
3501.347623	571241.497054	45.304410
3501.116721	571220.003764	45.309415
3501.684216	571211.734839	45.314420
3501.387221	571199.385509	45.319425
3501.515092	571192.490108	45.324429
3501.553555	571202.972716	45.329434
3501.444115	571179.402775	45.334439
3501.589029	571156.746541	45.339444
3501.477459	571160.126337	45.344449
3501.555346	571150.227610	45.349453
3501.369446	571138.212143	45.354458
3501.324205	571117.141303	45.359463
3501.507184	571116.962085	45.364468
3501.701961	571115.877685	45.369473
3501.683460	571103.283972	45.374477
3501.625186	571087.334032	45.379482
3501.942103	571082.817917	45.384487
3501.494816	571074.356235	45.389492
3501.351682	571049.235538	45.394497
3501.428994	571020.416758	45.399501
3501.571748	571022.150889	45.404506
3501.067695	571030.359732	45.409511
3501.688515	571036.736589	45.414516
3501.636137	571013.358128	45.419521
3501.629270	570992.331245	45.424525
3501.380836	570995.431368	45.429530
3501.175274	570972.126955	45.434535
3501.503587	570963.142453	45.439540
3501.330452	570963.119276	45.444545
3501.521852	570949.589230	45.449549
3501.686873	570959.148927	45.454554
3501.368844	570943.490324	45.459559
3501.532481	570921.784235	45.464564
3501.603866	570917.908675	45.469569
3502.274657	570908.117796	45.474573
3501.738687	570892.894684	45.479578
3501.605851	570879.465430	45.484583
3501.689952	570871.974441	45.489588
3501.413015	570844.816565	45.494593
3502.135658	570830.801838	45.499597
3502.064106	570823.084216	45.504602
3501.725533	570806.625649	45.509607
3501.565570	570788.984839	45.514612
3501.423074	570794.878919	45.519617
3501.362891	570775.767071	45.524621
3501.324910	570761.118363	45.529626
3501.613061	570746.067343	45.534631
3501.937117	570750.834582	45.539636
3501.760501	570735.956579	45.544641
3501.919078	570713.899578	45.549645
3502.094857	570708.050327	45.554650
3501.730586	570688.885497	45.559655
3501.986468	570671.179497	45.564660
3501.294240	570654.324310	45.569665
3501.175454	570625.886504	45.574669
3501.710431	570622.440247	45.579674
3501.641870	570622.701846	45.584679
3501.570652	570619.551104	45.589684
3501.487019	570608.071154	45.594689
3501.753481	570584.039719	45.599693
3501.662938	570569.800485	45.604698
3501.643752	570564.684269	45.609703
3501.719687	570545.600945	45.614708
3501.100516	570540.578513	45.619713
3501.779016	570529.330657	45.624717
3501.476489	570531.535977	45.629722
3501.491325	570522.951452	45.634727
3501.784480	570498.765101	45.639732
3501.341665	570495.321099	45.644737
3501.296848	570482.128558	45.649741
3501.471302	570465.840240	45.654746
3501.598808	570456.184097	45.659751
3501.709032	570454.912101	45.664756
3501.484988	570460.718724	45.669761
3501.487958	570435.724403	45.674765
3501.169753	570424.782824	45.679770
3501.832459	570412.834686	45.684775
3501.834788	570412.683699	45.689780
3501.431432	570394.026370	45.694785
3501.581161	570359.121782	45.699789
3501.572448	570365.346490	45.704794
3501.808732	570355.422314	45.709799
3501.583674	570335.331730	45.714804
3501.754863	570329.934703	45.719809
3501.797778	570316.678068	45.724813
3501.737908	570309.159028	45.729818
3501.352909	570288.691854	45.734823
3501.770591	570274.623747	45.739828
3501.160187	570218.908684	45.744833
3501.268490	570098.436603	45.749837
3500.902110	569949.980988	45.754842
3500.784833	569749.235364	45.759847
3500.567934	569513.869065	45.764852
3500.113883	569211.777500	45.769857
3500.328911	568870.872917	45.774861
3498.931055	568485.133613	45.779866
3498.639724	568057.443067	45.784871
3498.213474	567584.577065	45.789876
3497.381422	567064.664709	45.794881
3496.392550	566509.358648	45.799885
3495.551224	565905.050062	45.804890
3494.542744	565242.391098	45.809895
3494.043633	564560.131746	45.814900
3492.914347	563849.407751	45.819905
3491.708779	563063.522985	45.824909
3489.859440	562265.933747	45.829914
3488.471136	561414.525222	45.834919
3487.475031	560514.319794	45.839924
3485.556902	559610.974810	45.844929
3484.659148	558657.212557	45.849933
3482.945044	557666.120343	45.854938
3480.858679	556638.674848	45.859943
3479.570924	555568.904927	45.864948
3477.263006	554470.753779	45.869953
3476.190511	553348.334591	45.874957
3473.925907	552197.697636	45.879962
3471.760282	551003.602334	45.884967
3470.414240	549786.235271	45.889972
3467.891760	548539.063803	45.894977
3466.206001	547248.287791	45.899981
3463.546136	545939.272897	45.904986
3461.029571	544603.741341	45.909991
3458.801715	543240.505518	45.914996
3456.542509	541866.762225	45.920001
3453.885925	540453.836686	45.925005
3451.286371	539031.635940	45.930010
3448.907161	537583.222796	45.935015
3446.421790	536113.421626	45.940020
3443.637523	534617.776031	45.945025
3440.780957	533105.455199	45.950029
3438.436572	531581.649453	45.955034
3435.520820	530031.771157	45.960039
3432.641361	528466.997824	45.965044
3429.633263	526886.595434	45.970049
3426.954645	525291.092274	45.975053
3423.792064	523681.467615	45.980058
3420.584599	522043.994394	45.985063
3417.847627	520409.422550	45.990068
3414.890647	518758.812052	45.995073
3411.416486	517091.700655	46.000077
3408.765660	515416.897308	46.005082
3405.569622	513722.363369	46.010087
3402.318445	512024.000062	46.015092
3398.690823	510312.074425	46.020097
3395.741522	508585.863109	46.025101
3392.550521	506868.759270	46.030106
3389.009476	505133.291007	46.035111
3385.757771	503383.540616	46.040116
3382.072012	501636.975340	46.045121
3378.653834	499872.544984	46.050125
3375.149335	498111.750158	46.055130
3371.855831	496340.716343	46.060135
3368.289626	494565.019643	46.065140
3364.642045	492784.831896	46.070145
3361.335037	490992.462199	46.075149
3357.823710	489210.415573	46.080154
3354.257513	487415.339394	46.085159
3350.423556	485616.255233	46.090164
3346.791811	483823.597712	46.095169
3343.530046	482018.296446	46.100173
3339.718815	480218.784520	46.105178
3336.076510	478424.245602	46.110183
3332.793883	476607.107543	46.115188
3328.678519	474792.218089	46.120193
3325.465895	472986.234054	46.125197
3321.797513	471177.440411	46.130202
3318.027703	469360.725859	46.135207
3314.715055	467539.086794	46.140212
3310.438496	465726.805501	46.145217
3306.955322	463903.126299	46.150221
3303.631753	462078.567096	46.155226
3299.479828	460266.943595	46.160231
3295.917350	458435.050075	46.165236
3291.756752	456634.227036	46.170241
3288.132357	454801.908407	46.175245
3284.160608	452991.621343	46.180250
3280.105179	451181.566932	46.185255
3276.736135	449370.765774	46.190260
3272.901153	447569.930169	46.195265
3268.977629	445763.359734	46.200269
3265.334720	443954.389364	46.205274
3261.593124	442149.510950	46.210279
3257.759648	440342.091162	46.215284
3253.914611	438545.794667	46.220289
3250.042175	436740.010697	46.225293
3246.206912	434947.222367	46.230298
3242.530754	433169.290444	46.235303
3238.789718	431373.166471	46.240308
3234.613692	429581.101303	46.245313
3230.971815	427792.692569	46.250317
3227.001283	426006.557064	46.255322
3223.121524	424237.737034	46.260327
3219.478060	422456.559181	46.265332
3215.249511	420701.783008	46.270337
3211.802635	418928.583829	46.275341
3207.760973	417157.659578	46.280346
3203.798812	415397.832121	46.285351
3200.359987	413643.051703	46.290356
3196.422946	411892.618445	46.295361
3192.698229	410139.372956	46.300365
3189.140435	408386.113100	46.305370
3184.964553	406639.203082	46.310375
3181.399747	404889.016571	46.315380
3177.550510	403158.222900	46.320385
3173.608306	401416.706619	46.325389
3170.115892	399681.686809	46.330394
3165.810314	397940.016041	46.335399
3161.985086	396216.006777	46.340404
3158.397942	394491.581079	46.345409
3154.595206	392776.100682	46.350413
3150.476162	391053.288523	46.355418
3146.959593	389347.649441	46.360423
3143.280444	387634.657452	46.365428
3139.202282	385939.559951	46.370433
3135.492799	384231.011932	46.375437
3131.820869	382529.402550	46.380442
3127.943992	380839.901817	46.385447
3124.199963	379132.214950	46.390452
3119.896293	377447.666813	46.395457
3116.489681	375761.297292	46.400461
3112.669022	374081.186242	46.405466
3108.894519	372409.092948	46.410471
3105.413125	370719.553075	46.415476
3101.223961	369054.333711	46.420481
3097.855278	367373.949153	46.425485
3093.654715	365708.433832	46.430490
3089.888562	364059.778625	46.435495
3086.178534	362392.218146	46.440500
3082.300803	360743.343900	46.445505
3078.527990	359097.259696	46.450509
3074.819648	357453.007679	46.455514
3070.746665	355809.563475	46.460519
3067.340533	354163.691539	46.465524
3063.719836	352529.256422	46.470529
3060.008624	350904.538449	46.475533
3056.306388	349268.145520	46.480538
3052.553480	347626.213069	46.485543
3048.621976	345997.829028	46.490548
3044.613169	344378.022779	46.495553
3040.875201	342747.698133	46.500557
3037.323932	341141.067332	46.505562
3033.695459	339527.992591	46.510567
3030.070089	337917.590675	46.515572
3026.069707	336310.634164	46.520577
3022.456556	334706.623866	46.525581
3018.641520	333105.348124	46.530586
3014.908820	331498.853945	46.535591
3011.171394	329903.738842	46.540596
3007.064397	328316.933668	46.545601
3003.879104	326717.049550	46.550605
2999.728008	325138.773162	46.555610
2996.119616	323551.752465	46.560615
2992.418112	321970.129668	46.565620
2988.876000	320390.127079	46.570625
2984.672557	318818.158304	46.575629
2981.313219	317249.740833	46.580634
2978.077264	315683.563882	46.585639
2974.476145	314117.847592	46.590644
2970.295392	312549.140491	46.595649
2966.257554	310988.908205	46.600653
2962.992137	309415.322395	46.605658
2959.041585	307875.790780	46.610663
2955.598643	306303.481260	46.615668
2951.570525	304760.251765	46.620673
2947.972908	303210.545967	46.625677
2944.396949	301671.632897	46.630682
2940.410661	300119.275725	46.635687
2937.049956	298571.256060	46.640692
2933.279118	297032.904106	46.645697
2929.645644	295505.332252	46.650701
2925.983718	293965.252023	46.655706
2922.367074	292440.906810	46.660711
2918.584482	290894.606534	46.665716
2915.109681	289376.577850	46.670721
2911.267598	287846.987510	46.675725
2907.748560	286322.096722	46.680730
2903.867685	284804.355924	46.685735
2900.388361	283271.701813	46.690740
2896.933624	281763.094723	46.695745
2892.764104	280240.488710	46.700749
2889.220266	278719.968609	46.705754
2885.050553	277210.336832	46.710759
2881.561892	275687.660722	46.715764
2878.182432	274185.028036	46.720769
2874.412785	272681.130709	46.725773
2870.640093	271180.899602	46.730778
2866.598881	269696.141102	46.735783
2863.330489	268184.221155	46.740788
2859.447947	266701.630958	46.745793
2855.638511	265213.888700	46.750797
2852.332511	263722.888420	46.755802
2848.451453	262250.928348	46.760807
2845.034548	260766.423579	46.765812
2841.154237	259285.511771	46.770817
2837.603490	257803.842530	46.775821
2833.729967	256334.073400	46.780826
2830.055570	254863.569055	46.785831
2826.788971	253392.272149	46.790836
2823.056818	251931.550896	46.795841
2819.412061	250462.270527	46.800845
2816.455893	248990.424239	46.805850
2812.229884	247526.888046	46.810855
2808.651917	246053.204503	46.815860
2804.985007	244599.363247	46.820865
2801.090147	243122.626335	46.825869
2797.789982	241671.051295	46.830874
2793.728268	240222.413830	46.835879
2790.455783	238763.610613	46.840884
2786.711126	237311.419585	46.845889
2782.956425	235865.591030	46.850893
2779.429072	234418.957376	46.855898
2775.706808	232967.714127	46.860903
2772.341247	231519.416397	46.865908
2768.560172	230068.811769	46.870913
2764.682267	228633.883202	46.875917
2761.235784	227201.916224	46.880922
2757.490008	225760.342253	46.885927
2753.869219	224331.432015	46.890932
2750.173010	222897.975023	46.895937
2746.267067	221470.511715	46.900941
2742.986366	220038.036941	46.905946
2739.440072	218618.977459	46.910951
2735.473039	217183.024735	46.915956
2731.765772	215768.225432	46.920961
2728.510256	214346.840082	46.925965
2724.913497	212922.508148	46.930970
2721.044131	211512.665547	46.935975
2717.774687	210095.273520	46.940980
2713.637382	208681.233622	46.945985
2710.087411	207274.368320	46.950989
2706.934238	205862.101352	46.955994
2702.892612	204459.711424	46.960999
2699.724226	203049.503676	46.966004
2696.052230	201648.426353	46.971009
2691.740686	200243.462005	46.976013
2688.283384	198841.661312	46.981018
2684.285787	197444.261638	46.986023
2681.145004	196050.866753	46.991028
2677.164984	194664.722012	46.996033
2673.490442	193285.445085	47.001037
2670.158225	191894.899111	47.006042
2666.120420	190513.697677	47.011047
2662.404741	189126.885191	47.016052
2658.889866	187762.518122	47.021057
2655.459343	186370.322322	47.026061
2652.033913	184996.758331	47.031066
2648.270705	183636.201266	47.036071
2644.862275	182260.227664	47.041076
2640.587610	180898.083034	47.046081
2637.074112	179533.700592	47.051085
2634.030985	178164.962254	47.056090
2630.141157	176798.847684	47.061095
2626.805894	175438.015350	47.066100
2623.109015	174081.501357	47.071105
2619.445860	172728.926013	47.076109
2615.945306	171365.680951	47.081114
2612.394672	170009.838744	47.086119
2608.587055	168651.451990	47.091124
2605.026035	167298.487610	47.096129
2601.220526	165951.875563	47.101133
2597.801748	164604.783804	47.106138
2593.941136	163264.534197	47.111143
2590.349473	161911.885107	47.116148
2586.933295	160571.366722	47.121153
2583.486312	159228.361477	47.126157
2579.628881	157889.407802	47.131162
2576.058823	156555.860502	47.136167
2572.155922	155216.184410	47.141172
2568.614454	153883.100374	47.146177
2564.957774	152544.465804	47.151181
2561.942700	151213.716510	47.156186
2557.817086	149878.299053	47.161191
2554.419088	148548.883415	47.166196
2550.573404	147226.938791	47.171201
2547.233966	145861.455178	47.176205
2543.823596	144499.963449	47.181210
2539.815584	143182.894290	47.186215
2536.228155	141855.551598	47.191220
2532.759849	140534.040824	47.196225
2529.168995	139226.898848	47.201229
2525.618191	137906.656795	47.206234
2521.879135	136605.488606	47.211239
2518.717875	135292.842478	47.216244
2514.953845	133986.842045	47.221249
2510.881541	132673.982182	47.226253
2507.393337	131357.393725	47.231258
2503.636143	130061.697855	47.236263
2499.865244	128760.611818	47.241268
2496.763532	127462.132257	47.246273
2492.933354	126168.424135	47.251277
2489.369224	124866.956533	47.256282
2485.574100	123571.188292	47.261287
2482.178473	122286.667590	47.266292
2478.530044	121004.606272	47.271297
2474.745482	119708.199660	47.276301
2471.173802	118417.894574	47.281306
2467.797834	117147.185663	47.286311
2464.260936	115859.657986	47.291316
2460.601952	114576.122960	47.296321
2457.004817	113307.016397	47.301325
2453.439078	112024.738690	47.306330
2449.606363	110745.599806	47.311335
2446.418226	109471.504239	47.316340
2442.693634	108210.277340	47.321345
2438.569959	106930.585226	47.326349
2435.175084	105656.610745	47.331354
2431.908278	104399.049375	47.336359
2427.966229	103135.335723	47.341364
2424.553887	101862.931003	47.346369
2420.873546	100612.262969	47.351373
2417.145397	99345.051202	47.356378
2413.440100	98104.308273	47.361383
2409.789531	96850.133447	47.366388
2406.283220	95595.591698	47.371393
2402.400263	94347.246052	47.376397
2399.310099	93102.524337	47.381402
2395.070457	91868.376093	47.386407
2391.431637	90613.243780	47.391412
2387.746934	89384.128679	47.396417
2383.639951	88148.929912	47.401421
2380.439848	86922.330731	47.406426
2376.965177	85712.938222	47.411431
2373.533407	84471.232910	47.416436
2369.627328	83266.405309	47.421441
2365.624580	82042.640429	47.426445
2362.679367	80829.064213	47.431450
2359.005043	79616.962612	47.436455
2355.381684	78404.994572	47.441460
2351.925981	77191.732522	47.446465
2347.695087	75981.617116	47.451469
2344.347571	74783.837180	47.456474
2340.408360	73599.015914	47.461479
2337.184634	72384.611953	47.466484
2333.904514	71197.292682	47.471489
2330.167042	70000.981980	47.476493
2326.596551	68805.125184	47.481498
2322.774687	67620.147888	47.486503
2318.897455	66436.414415	47.491508
2315.501370	65246.846332	47.496513
2311.590700	64054.050592	47.501517
2308.172302	62883.416124	47.506522
2303.981478	61716.397071	47.511527
2300.877213	60541.565064	47.516532
2297.101398	59376.685732	47.521537
2293.292616	58214.202179	47.526541
2289.770718	57042.452676	47.531546
2286.461323	55891.842707	47.536551
2282.240858	54725.423108	47.541556
2278.739354	53577.955738	47.546561
2275.087284	52429.267142	47.551565
2271.493622	51274.009194	47.556570
2267.783858	50147.866580	47.561575
2264.257372	48995.965570	47.566580
2260.942612	47857.161497	47.571585
2257.157554	46729.992904	47.576589
2253.903174	45581.665381	47.581594
2249.818572	44458.950392	47.586599
2245.962324	43336.021300	47.591604
2242.505141	42212.445947	47.596609
2238.717974	41086.461961	47.601613
2235.129391	39976.856697	47.606618
2231.217969	38869.653415	47.611623
2227.611048	37751.129619	47.616628
2224.090003	36646.026718	47.621633
2220.145021	35553.186604	47.626637
2216.315047	34460.143601	47.631642
2212.566086	33368.589442	47.636647
2209.027781	32290.001471	47.641652
2204.971925	31210.821098	47.646657
2201.267951	30147.219284	47.651661
2197.494542	29075.799371	47.656666
2193.689129	28022.208858	47.661671
2189.521663	26966.004401	47.666676
2185.499098	25919.532809	47.671681
2181.437010	24884.728842	47.676685
2178.031301	23858.517046	47.681690
2173.663386	22845.343574	47.686695
2169.925072	21835.379200	47.691700
2166.196176	20849.194329	47.696705
2161.844524	19855.649906	47.701709
2157.882597	18880.248022	47.706714
2153.935645	17926.623385	47.711719
2149.139169	16990.937236	47.716724
2143.884093	16083.148205	47.721729
2137.714008	15213.187357	47.726733
2132.303568	14379.039956	47.731738
2126.600981	13581.264961	47.736743
2121.188123	12808.039987	47.741748
2115.909880	12060.358351	47.746753
2110.973670	11358.113220	47.751757
2106.270745	10671.062408	47.756762
2101.147629	10039.182987	47.761767
2097.042820	9413.354013	47.766772
2092.089699	8816.081359	47.771777
2087.681508	8243.225781	47.776781
2083.470063	7686.663956	47.781786
2078.642368	7176.520125	47.786791
2074.119006	6690.042141	47.791796
2069.523109	6223.732944	47.796801
2064.589836	5795.146615	47.801805
2060.068608	5385.152576	47.806810
2055.774316	4997.683784	47.811815
2051.127438	4635.082713	47.816820
2046.840599	4285.049646	47.821825
2042.394101	3975.756540	47.826829
2038.070265	3664.607798	47.831834
2034.191292	3374.637445	47.836839
2030.470591	3105.028609	47.841844
2026.684027	2843.930283	47.846849
2022.687122	2590.741349	47.851853
2019.331534	2346.609734	47.856858
2015.890073	2129.346160	47.861863
2012.377798	1899.319451	47.866868
2009.021208	1670.527476	47.871873
2005.848669	1460.662403	47.876877
2002.666008	1244.308770	47.881882
1999.082197	1034.918031	47.886887
1995.419222	832.515502	47.891892
1992.111760	640.633482	47.896897
1988.380472	443.555123	47.901901
1984.805043	256.430203	47.906906
1979.437250	115.681566	47.911911
1969.105360	125.290056	47.916916
1961.394814	129.255391	47.921921
1955.608825	140.740588	47.926925
1952.394183	137.488077	47.931930
1950.439039	136.088649	47.936935
1948.480659	139.467124	47.941940
1946.139461	128.854899	47.946945
1943.785415	135.338899	47.951949
1940.852306	131.400079	47.956954
1937.764289	143.159152	47.961959
1934.123202	134.550559	47.966964
1931.029152	130.883706	47.971969
1927.252409	134.679603	47.976973
1924.436252	128.751418	47.981978
1921.226001	143.196736	47.986983
1917.547657	133.540421	47.991988
1914.132944	137.497977	47.996993
1910.963528	148.886972	48.001997
1908.078129	131.342522	48.007002
1904.483878	143.430761	48.012007
1900.784090	144.806946	48.017012
1897.198736	131.133836	48.022017
1893.828982	147.920049	48.027021
1891.038566	136.394178	48.032026
1887.676690	139.786638	48.037031
1884.011729	137.417724	48.042036
1881.234435	137.108770	48.047041
1877.146795	140.795144	48.052045
1873.863909	133.275831	48.057050
1869.686631	138.333519	48.062055
1866.256468	138.854417	48.067060
1863.827574	138.965523	48.072065
1860.120355	142.370904	48.077069
1856.992141	130.942204	48.082074
1853.659537	135.269751	48.087079
1849.579149	138.502571	48.092084
1846.268307	137.166614	48.097089
1842.842312	142.230135	48.102093
1839.399186	134.530262	48.107098
1836.009011	138.234057	48.112103
1832.735744	141.312102	48.117108
1829.156043	138.562861	48.122113
1825.255108	138.429760	48.127117
1822.553202	142.845286	48.132122
1818.892985	131.110703	48.137127
1815.324066	135.377164	48.142132
1811.910062	133.472053	48.147137
1808.278217	138.441243	48.152141
1805.155281	132.712968	48.157146
1801.490124	140.550643	48.162151
1798.310370	139.709892	48.167156
1794.606215	134.556643	48.172161
1790.865782	135.942389	48.177165
1787.832622	132.769103	48.182170
1784.180732	139.323354	48.187175
1780.043274	136.636106	48.192180
1777.287417	122.159350	48.197185
1773.646248	133.581060	48.202189
1770.573754	133.058899	48.207194
1766.949394	130.981075	48.212199
1763.470762	140.175329	48.217204
1759.623623	135.629779	48.222209
1756.098613	131.919693	48.227213
1752.925912	127.436284	48.232218
1749.391280	131.956832	48.237223
1746.045072	140.130595	48.242228
1742.540191	141.574410	48.247233
1738.833239	133.627956	48.252237
1735.505638	132.158615	48.257242
1732.484082	142.401342	48.262247
1729.040221	141.554488	48.267252
1725.322306	136.567939	48.272257
1720.937207	138.798100	48.277261
1717.654332	129.269814	48.282266
1714.434165	131.861843	48.287271
1710.825478	133.676263	48.292276
1708.174141	130.677370	48.297281
1704.599845	132.641437	48.302285
1700.701590	131.818249	48.307290
1697.172923	133.965008	48.312295
1693.410169	135.531455	48.317300
1690.656048	128.097145	48.322305
1686.553951	133.601886	48.327309
1683.585961	133.202605	48.332314
1679.547898	127.158841	48.337319
1676.219786	132.934768	48.342324
1672.990926	129.570680	48.347329
1668.948108	131.288537	48.352333
1666.088657	130.790015	48.357338
1662.378063	133.727739	48.362343
1659.040511	133.009808	48.367348
1655.890228	121.223973	48.372353
1651.367302	134.606080	48.377357
1648.160187	133.459604	48.382362
1644.571305	139.447201	48.387367
1641.156031	132.303047	48.392372
1637.876330	135.806108	48.397377
1634.435873	123.518352	48.402381
1631.156621	121.152444	48.407386
1627.535952	127.796766	48.412391
1624.095908	124.532188	48.417396
1620.660638	120.042464	48.422401
1616.791673	128.165190	48.427405
1613.292710	130.351620	48.432410
1609.522842	126.733698	48.437415
1606.340359	120.385214	48.442420
1603.047200	118.217650	48.447425
1599.945993	124.024523	48.452429
1596.176698	125.794513	48.457434
1592.475610	121.298946	48.462439
1588.628630	124.947754	48.467444
1585.666622	111.939724	48.472449
1581.563872	126.800031	48.477453
1578.672447	123.563501	48.482458
1575.082592	113.608755	48.487463
1571.531382	118.049689	48.492468
1568.340901	113.755796	48.497473
1564.188299	130.974635	48.502477
1561.056541	119.587746	48.507482
1557.677620	121.100493	48.512487
1553.768701	126.847132	48.517492
1550.802580	113.567670	48.522497
1547.024140	120.742919	48.527501
1543.735550	120.830466	48.532506
1539.896172	115.410583	48.537511
1536.398638	123.392938	48.542516
1532.699845	117.751732	48.547521
1529.911248	129.150792	48.552525
1526.302437	120.812581	48.557530
1522.549278	124.956103	48.562535
1518.816004	129.188266	48.567540
1515.975711	126.915045	48.572545
1512.177768	127.310122	48.577549
1508.512004	119.518683	48.582554
1505.106486	118.960142	48.587559
1501.442785	124.994291	48.592564
1498.109102	114.404682	48.597569
1494.359115	117.117668	48.602573
1491.456539	120.501628	48.607578
1487.726056	121.575869	48.612583
1484.153780	121.084566	48.617588
1481.111640	118.963176	48.622593
1476.953224	122.831617	48.627597
1473.553007	114.011518	48.632602
1469.954451	117.362049	48.637607
1466.052971	118.039110	48.642612
1463.465867	119.772804	48.647617
1459.737606	117.853732	48.652621
1456.276682	118.790876	48.657626
1452.819221	121.553004	48.662631
1448.709499	119.823361	48.667636
1445.594871	119.567328	48.672641
1442.346941	124.451225	48.677645
1438.709921	115.187306	48.682650
1435.232047	114.912203	48.687655
1431.269777	118.506344	48.692660
1428.004125	110.519435	48.697665
1424.627078	123.880437	48.702669
1421.373582	110.782057	48.707674
1418.011681	113.057828	48.712679
1413.594874	119.697114	48.717684
1410.785451	116.855935	48.722689
1406.713195	121.713846	48.727693
1403.462958	110.437325	48.732698
1400.497626	116.760827	48.737703
1396.668123	118.097378	48.742708
1393.348975	112.918835	48.747713
1389.724641	126.195166	48.752717
1386.086618	122.534550	48.757722
1382.461243	112.262740	48.762727
1378.686880	124.809569	48.767732
1375.231370	112.480000	48.772737
1371.584118	117.439078	48.777741
1368.818475	110.601485	48.782746
1365.381892	106.488562	48.787751
1361.758072	121.884573	48.792756
1358.415861	111.331163	48.797761
1354.687267	110.453080	48.802765
1351.510634	119.723547	48.807770
1347.799807	112.037314	48.812775
1344.423173	115.998566	48.817780
1340.668505	99.618708	48.822785
1336.795404	111.450154	48.827789
1333.531047	115.542533	48.832794
1330.079926	116.240898	48.837799
1326.228273	122.674689	48.842804
1323.637029	106.891012	48.847809
1319.795468	109.776585	48.852813
1316.188092	112.018047	48.857818
1312.689723	108.161593	48.862823
1308.940140	112.545075	48.867828
1305.412183	104.276570	48.872833
1301.792477	110.984110	48.877837
1298.504489	105.231241	48.882842
1295.219496	108.260655	48.887847
1291.622765	112.509482	48.892852
1288.532131	105.283023	48.897857
1284.529515	107.276314	48.902861
1280.895685	112.353544	48.907866
1277.428142	117.059889	48.912871
1273.637163	123.594933	48.917876
1270.704317	104.941388	48.922881
1267.066004	113.439407	48.927885
1263.408096	113.391869	48.932890
1260.576026	109.095765	48.937895
1256.722323	105.870773	48.942900
1253.010556	109.558642	48.947905
1249.552963	109.546191	48.952909
1246.231651	107.022485	48.957914
1242.647495	110.706201	48.962919
1239.037158	116.428349	48.967924
1235.631273	120.840312	48.972929
1231.845153	112.314851	48.977933
1228.638038	110.921738	48.982938
1225.262842	103.024830	48.987943
1221.513607	111.657288	48.992948
1218.021980	104.904927	48.997953
1214.462478	111.150644	49.002957
1210.906702	104.031835	49.007962
1207.727808	107.648954	49.012967
1203.933078	112.213550	49.017972
1200.936752	113.470360	49.022977
1197.240248	116.690780	49.027981
1193.297306	105.102010	49.032986
1189.945945	110.201488	49.037991
1186.431187	112.865102	49.042996
1183.216349	96.888045	49.048001
1179.639573	110.020928	49.053005
1175.810836	110.803774	49.058010
1172.688628	105.597651	49.063015
1169.388869	103.864716	49.068020
1165.792993	95.771426	49.073025
1161.649448	100.852559	49.078029
1158.269201	107.013280	49.083034
1154.912330	110.930366	49.088039
1151.160495	110.125605	49.093044
1148.152316	103.892383	49.098049
1144.530127	103.497607	49.103053
1141.010039	107.623750	49.108058
1137.526651	104.410437	49.113063
1134.114221	110.237678	49.118068
1130.471675	104.948515	49.123073
1126.714026	105.473474	49.128077
1123.263033	100.878838	49.133082
1119.986223	104.419562	49.138087
1116.664740	109.932007	49.143092
1113.076750	105.181649	49.148097
1109.957903	111.136943	49.153101
1106.367028	105.070895	49.158106
1102.724059	106.368861	49.163111
1098.989588	112.414214	49.168116
1095.892329	112.253652	49.173121
1092.254549	105.274284	49.178125
1088.186780	109.172975	49.183130
1085.056607	115.281913	49.188135
1081.100371	103.211219	49.193140
1078.332133	95.266806	49.198145
1074.346668	107.451281	49.203149
1071.070222	106.249415	49.208154
1067.533612	101.604930	49.213159
1063.911809	109.793534	49.218164
1060.494759	96.331785	49.223169
1056.694872	111.565597	49.228173
1053.422969	106.588602	49.233178
1049.924072	100.372135	49.238183
1046.469876	112.138080	49.243188
1043.192441	111.667218	49.248193
1039.406075	111.279202	49.253197
1035.688892	101.461702	49.258202
1032.377926	100.347514	49.263207
1028.941626	104.058771	49.268212
1025.750710	94.367695	49.273217
1021.996670	99.761225	49.278221
1018.413254	101.296675	49.283226
1015.271590	105.420558	49.288231
1011.191746	104.705175	49.293236
1008.117513	98.232409	49.298241
1004.392146	111.970743	49.303245
1000.764265	104.009086	49.308250
997.623216	99.271059	49.313255
993.783235	97.581642	49.318260
990.386085	94.076471	49.323265
987.076588	105.728021	49.328269
983.267153	110.529119	49.333274
979.949689	96.577244	49.338279
976.295756	99.401927	49.343284
972.916593	97.118339	49.348289
969.298826	100.639726	49.353293
965.878501	105.560241	49.358298
962.685947	98.137893	49.363303
958.943482	102.115414	49.368308
955.439916	103.793410	49.373313
952.036429	102.636788	49.378317
948.460763	98.919136	49.383322
945.199985	92.874243	49.388327
941.389222	103.212216	49.393332
938.016293	97.817646	49.398337
934.036280	97.766883	49.403341
930.780417	103.889213	49.408346
927.340750	96.714384	49.413351
924.179547	103.590697	49.418356
920.453052	99.450576	49.423361
916.973845	102.833226	49.428365
913.004697	99.537873	49.433370
909.677990	96.072324	49.438375
906.220273	102.479371	49.443380
902.839517	94.985276	49.448385
899.310295	94.838632	49.453389
895.717397	99.488792	49.458394
892.702762	103.054974	49.463399
888.750275	106.571854	49.468404
885.373670	100.405911	49.473409
881.526184	99.521322	49.478413
878.250546	95.680788	49.483418
874.783239	100.403040	49.488423
871.001941	111.302746	49.493428
868.074634	104.506463	49.498433
864.460966	101.895798	49.503437
860.637797	106.550391	49.508442
857.377263	96.857629	49.513447
853.636643	99.360568	49.518452
850.435422	96.935265	49.523457
846.701856	103.663940	49.528461
843.393403	109.794532	49.533466
840.219112	105.476225	49.538471
836.478917	109.064289	49.543476
832.861130	102.066088	49.548481
829.114924	98.587164	49.553485
825.547837	109.649496	49.558490
822.242633	105.680731	49.563495
818.808390	117.646098	49.568500
815.165399	103.612391	49.573505
811.883645	102.996751	49.578509
807.914952	100.821359	49.583514
804.822345	100.777226	49.588519
801.143539	112.417053	49.593524
798.385311	104.673653	49.598529
794.634550	99.556608	49.603533
790.652856	93.093150	49.608538
787.551009	94.856997	49.613543
783.645905	93.813791	49.618548
780.003898	91.147488	49.623553
776.760144	96.999041	49.628557
773.333847	97.222311	49.633562
769.913999	96.925708	49.638567
765.923937	106.254091	49.643572
762.525569	99.386080	49.648577
759.289391	99.044901	49.653581
756.205027	95.424401	49.658586
752.449359	95.044350	49.663591
748.487484	105.263679	49.668596
745.045444	100.310286	49.673601
741.635786	95.661877	49.678605
738.186931	101.137432	49.683610
734.953107	105.266339	49.688615
730.983757	102.746230	49.693620
727.850292	97.997625	49.698625
724.393595	96.624792	49.703629
720.769282	98.160428	49.708634
717.320064	92.613379	49.713639
713.692392	100.050024	49.718644
709.977187	98.837903	49.723649
706.656748	103.379021	49.728653
703.006237	94.313720	49.733658
699.941495	99.213435	49.738663
696.126157	93.448480	49.743668
692.842079	98.404692	49.748673
689.485945	100.306472	49.753677
685.540917	100.841966	49.758682
681.991502	95.465648	49.763687
678.330332	95.083484	49.768692
675.114516	94.818241	49.773697
671.909219	95.332808	49.778701
668.134480	87.274087	49.783706
664.556488	92.168766	49.788711
660.785637	91.876554	49.793716
657.662021	98.244010	49.798721
654.464144	101.250492	49.803725
650.963335	103.174943	49.808730
647.412797	84.735511	49.813735
643.398482	97.196721	49.818740
640.035976	93.097798	49.823745
636.566991	101.958635	49.828749
632.712934	88.166900	49.833754
629.547401	83.821997	49.838759
626.251689	88.893947	49.843764
622.559428	87.203701	49.848769
619.152254	83.526241	49.853773
615.471698	99.741233	49.858778
612.353342	89.282825	49.863783
608.393513	96.708247	49.868788
605.303664	100.808319	49.873793
601.740232	100.562740	49.878797
598.088432	101.821151	49.883802
594.707639	99.091867	49.888807
591.063406	92.139052	49.893812
587.691565	101.187171	49.898817
584.104562	89.840379	49.903821
580.278921	104.429772	49.908826
577.044222	89.468538	49.913831
573.660468	102.194855	49.918836
570.030693	94.391887	49.923841
566.621804	104.126032	49.928845
562.897393	99.783258	49.933850
559.391986	94.814559	49.938855
556.090520	99.555236	49.943860
552.566501	97.247039	49.948865
549.361538	97.850183	49.953869
545.487422	101.380234	49.958874
542.400351	93.087316	49.963879
538.758599	95.998838	49.968884
534.878438	100.219546	49.973889
531.293562	95.355055	49.978893
527.773827	97.826686	49.983898
524.436613	96.928768	49.988903
520.603751	101.208514	49.993908
517.292579	89.499011	49.998913
514.250980	92.756310	50.003917
510.515472	95.192140	50.008922
507.543754	92.288089	50.013927
503.662574	99.995466	50.018932
499.848798	100.418732	50.023937
496.481061	92.353293	50.028941
492.947784	94.159498	50.033946
489.512528	95.934533	50.038951
486.071780	91.202515	50.043956
482.693230	97.075270	50.048961
479.136675	103.194210	50.053965
475.412747	102.489760	50.058970
471.753588	90.508911	50.063975
468.094723	94.831026	50.068980
464.921346	92.572350	50.073985
461.796930	96.219129	50.078989
458.032600	107.828159	50.083994
454.508729	90.703952	50.088999
450.378331	99.883579	50.094004
447.322993	90.601793	50.099009
444.059307	89.255787	50.104013
440.383779	91.862585	50.109018
437.169051	99.551020	50.114023
433.403060	89.232096	50.119028
429.992490	92.892067	50.124033
426.644461	91.185952	50.129037
422.567126	92.675600	50.134042
419.333459	86.224876	50.139047
415.739709	97.965384	50.144052
412.064466	95.051339	50.149057
409.041508	93.917578	50.154061
405.279625	90.419151	50.159066
402.142271	96.298446	50.164071
398.264247	92.846688	50.169076
394.835805	92.042204	50.174081
391.700037	86.066544	50.179085
387.563207	95.085848	50.184090
384.753514	88.932563	50.189095
380.858663	99.859696	50.194100
377.273147	91.606958	50.199105
373.622983	94.292067	50.204109
370.544989	100.095635	50.209114
367.058562	91.523656	50.214119
363.313070	88.199853	50.219124
360.097617	91.500252	50.224129
356.593520	88.806199	50.229133
352.902393	95.632801	50.234138
349.502189	84.804204	50.239143
345.913054	93.313783	50.244148
342.518118	87.859635	50.249153
338.914321	81.523873	50.254157
335.061424	91.495311	50.259162
331.298379	81.587274	50.264167
328.210233	91.432593	50.269172
324.761387	86.040682	50.274177
321.516292	90.880172	50.279181
318.035409	98.081982	50.284186
314.624322	88.776885	50.289191
310.940553	89.559520	50.294196
307.504819	89.670547	50.299201
303.948934	80.862709	50.304205
300.169213	93.492929	50.309210
296.898375	82.188509	50.314215
293.142849	86.826388	50.319220
289.692318	78.967008	50.324225
286.557273	84.586542	50.329229
282.754925	88.219350	50.334234
279.182158	80.825215	50.339239
275.636303	89.252106	50.344244
272.004420	86.644546	50.349249
268.700166	76.183780	50.354253
265.214980	86.157749	50.359258
262.036578	82.308556	50.364263
258.289304	88.523883	50.369268
255.173338	83.168443	50.374273
251.385301	86.008076	50.379277
247.293798	82.833444	50.384282
244.257852	78.677203	50.389287
240.983964	75.358675	50.394292
237.221425	85.243221	50.399297
233.732333	82.062812	50.404301
230.119908	88.437361	50.409306
226.769922	86.358304	50.414311
223.388655	85.612937	50.419316
219.699710	86.690653	50.424321
216.273266	87.534257	50.429325
212.554812	87.205552	50.434330
209.473787	88.934689	50.439335
205.327978	91.906320	50.444340
202.168978	84.890329	50.449345
198.674867	79.926350	50.454349
194.775544	86.434441	50.459354
191.775044	79.944124	50.464359
188.371443	80.695575	50.469364
184.283047	82.117459	50.474369
181.537876	83.392190	50.479373
177.912260	79.065759	50.484378
174.475308	81.603646	50.489383
170.450468	79.582880	50.494388
166.921051	80.119929	50.499393
163.392252	82.979097	50.504397
160.051291	88.317716	50.509402
156.661928	83.792927	50.514407
153.115162	84.152365	50.519412
149.682081	81.545352	50.524417
146.363479	79.730333	50.529421
142.049903	86.043914	50.534426
139.171051	77.807138	50.539431
135.118108	85.010040	50.544436
131.911176	87.394848	50.549441
129.183947	86.002883	50.554445
126.031655	82.636876	50.559450
122.342494	80.785007	50.564455
118.179321	91.564438	50.569460
114.409883	90.215534	50.574465
110.862581	79.049430	50.579469
107.462359	81.252556	50.584474
104.302106	81.871000	50.589479
100.569879	85.312559	50.594484
96.923948	80.498961	50.599489
93.784739	82.888991	50.604493
89.827998	79.854677	50.609498
86.694481	78.807956	50.614503
83.050335	84.238393	50.619508
79.614829	87.687258	50.624513
76.210093	84.373476	50.629517
72.660070	90.988244	50.634522
68.736833	84.826042	50.639527
65.828141	82.949996	50.644532
62.315474	82.959277	50.649537
58.503591	81.246887	50.654541
55.052174	78.604822	50.659546
51.475401	73.280535	50.664551
47.937055	84.455643	50.669556
44.173075	76.866952	50.674561
41.468326	73.285327	50.679565
37.835170	80.517409	50.684570
34.132775	86.441049	50.689575
30.686832	86.151984	50.694580
26.869886	84.465712	50.699585
23.640820	82.437396	50.704589
19.815334	92.967803	50.709594
16.521855	85.659747	50.714599
12.854941	80.362254	50.719604
9.533553	82.619504	50.724609
6.221686	82.018375	50.729613
2.262661	86.941355	50.734618