Thu Aug 25 12:40:25 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
1.964159	96.103975	0.000000
1.600983	90.725514	0.005005
1.888663	77.563431	0.010010
1.632278	88.040903	0.015014
1.778358	78.941147	0.020019
1.228829	79.299339	0.025024
1.152015	72.540903	0.030029
0.995389	61.308745	0.035034
0.316662	57.640716	0.040038
0.335094	50.835727	0.045043
-0.165804	37.917453	0.050048
-0.019728	36.107042	0.055053
-0.716395	30.195555	0.060058
-0.804772	26.640680	0.065062
-1.262172	20.561992	0.070067
-1.174255	14.461141	0.075072
-2.071225	23.776602	0.080077
-1.999608	11.072366	0.085082
-2.103527	16.324682	0.090086
-2.534682	10.460186	0.095091
-2.865937	4.023217	0.100096
-3.318543	5.502012	0.105101
-3.130915	7.130430	0.110106
-3.797405	-2.345005	0.115110
-4.290137	8.270691	0.120115
-4.748990	-4.097317	0.125120
-4.547476	0.388964	0.130125
-4.453739	10.064884	0.135130
-4.937748	8.378510	0.140134
-5.293979	4.346750	0.145139
-5.549543	-2.225462	0.150144
-6.266559	2.610383	0.155149
-6.270763	-3.479192	0.160154
-6.813391	-4.238890	0.165158
-6.398602	-0.228952	0.170163
-6.368949	-2.698162	0.175168
-6.546372	-0.386123	0.180173
-7.193706	1.335154	0.185178
-7.838061	6.314640	0.190182
-8.360795	-7.660039	0.195187
-7.819827	-1.528007	0.200192
-8.439491	-5.439394	0.205197
-7.910421	-1.643516	0.210202
-8.540171	-5.733657	0.215206
-9.129998	-5.264748	0.220211
-9.196660	-1.900712	0.225216
-9.577408	-1.012145	0.230221
-9.580799	-9.585397	0.235226
-10.610536	-5.637029	0.240230
-10.536870	-2.522771	0.245235
-10.785270	3.369112	0.250240
-11.061001	-2.696902	0.255245
-10.900045	1.276877	0.260250
-11.152247	-2.363055	0.265254
-11.386312	-4.360673	0.270259
-11.634681	3.612959	0.275264
-12.144845	-0.350387	0.280269
-12.155562	-10.121556	0.285274
-12.265198	-9.063496	0.290278
-13.365257	-3.677253	0.295283
-13.039980	-4.250234	0.300288
-13.668327	-8.970182	0.305293
-13.371663	-9.298234	0.310298
-13.641662	-8.398545	0.315302
-13.873842	-4.306221	0.320307
-13.887833	-0.032948	0.325312
-14.809742	5.084938	0.330317
-14.857382	-6.243345	0.335322
-15.072981	1.962433	0.340326
-14.938178	4.254026	0.345331
-15.384952	2.909833	0.350336
-16.341637	-5.090110	0.355341
-16.778915	-4.426803	0.360346
-16.665650	6.236310	0.365350
-16.694741	-7.271546	0.370355
-16.723267	-7.773273	0.375360
-17.009874	6.859738	0.380365
-16.790804	-9.869743	0.385370
-17.177257	-1.181615	0.390374
-17.881852	-1.609050	0.395379
-18.206036	-7.139122	0.400384
-18.622094	3.356990	0.405389
-18.451399	-1.450192	0.410394
-18.303173	1.623910	0.415398
-18.938342	4.798612	0.420403
-18.822374	-0.654893	0.425408
-19.263635	-4.654344	0.430413
-19.461096	-13.437632	0.435418
-20.230495	-4.192793	0.440422
-20.673933	0.239517	0.445427
-20.768867	-6.247129	0.450432
-20.941962	-4.853258	0.455437
-20.715415	-8.697915	0.460442
-21.185000	0.262668	0.465446
-22.371399	0.644717	0.470451
-22.436215	-5.030398	0.475456
-22.524166	-4.703400	0.480461
-22.407595	-12.868338	0.485466
-22.289155	-0.994321	0.490470
-22.536509	7.548630	0.495475
-22.485353	-1.517227	0.500480
-22.827290	6.838063	0.505485
-23.249702	-3.352657	0.510490
-23.457421	1.321130	0.515494
-24.381720	9.811962	0.520499
-24.851922	1.175807	0.525504
-25.122855	-1.594320	0.530509
-24.960230	-1.195851	0.535514
-25.184522	-3.213983	0.540518
-25.575504	-2.785720	0.545523
-25.369190	-5.159223	0.550528
-25.304678	5.755138	0.555533
-25.563315	0.458404	0.560538
-26.224823	4.095978	0.565542
-26.552628	-3.588047	0.570547
-26.730423	-0.709637	0.575552
-27.545262	8.868196	0.580557
-27.603934	1.834862	0.585562
-27.823283	-1.066733	0.590566
-27.936907	4.987530	0.595571
-28.108601	2.306259	0.600576
-28.410872	6.532954	0.605581
-28.366063	-2.266152	0.610586
-28.332213	-3.283854	0.615590
-29.244524	-4.586740	0.620595
-29.362398	0.544370	0.625600
-29.988282	1.930093	0.630605
-30.044522	1.385252	0.635610
-29.853624	-5.079741	0.640614
-30.364902	0.565428	0.645619
-30.257502	-9.828525	0.650624
-30.916091	-6.213556	0.655629
-31.356316	-9.444373	0.660634
-31.672085	-10.983098	0.665638
-31.707526	-10.072705	0.670643
-31.542204	-10.582658	0.675648
-31.824135	-5.473301	0.680653
-32.094673	-3.871172	0.685658
-32.605079	-7.669962	0.690662
-33.107929	-6.657858	0.695667
-32.795574	-4.799048	0.700672
-33.991704	3.193370	0.705677
-33.863558	-7.143723	0.710682
-34.463179	-7.492691	0.715686
-34.490245	-4.698010	0.720691
-34.081140	-11.073804	0.725696
-34.425744	-7.621927	0.730701
-34.070234	-8.974767	0.735706
-34.392713	-1.796285	0.740710
-35.512970	3.115399	0.745715
-35.563925	1.642748	0.750720
-35.966478	2.338580	0.755725
-36.013073	4.139739	0.760730
-36.632229	-5.102661	0.765734
-37.469907	-1.595672	0.770739
-37.386920	-1.937700	0.775744
-37.198355	8.457350	0.780749
-37.250629	-3.012576	0.785754
-37.145586	1.580568	0.790758
-37.505553	7.923368	0.795763
-37.273545	-1.955438	0.800768
-38.294675	-2.716089	0.805773
-38.369149	5.154365	0.810778
-38.775030	2.879948	0.815782
-39.500504	-0.821869	0.820787
-39.710235	1.912850	0.825792
-39.962779	1.604412	0.830797
-40.200146	-4.214509	0.835802
-40.093687	-2.456316	0.840806
-40.264782	-4.384705	0.845811
-39.632477	-8.476437	0.850816
-40.787196	5.235897	0.855821
-41.331546	-11.158826	0.860826
-41.311940	3.884945	0.865830
-41.483748	-0.257965	0.870835
-41.738492	-12.012537	0.875840
-42.438469	-4.145319	0.880845
-42.453074	-3.352085	0.885850
-42.569975	-6.576616	0.890854
-43.277805	-0.346992	0.895859
-42.796486	-12.400393	0.900864
-42.859124	6.497068	0.905869
-43.668171	0.131806	0.910874
-44.432455	0.840024	0.915878
-44.454453	-0.074014	0.920883
-44.157746	-0.582408	0.925888
-44.664094	-4.935490	0.930893
-44.764520	1.942444	0.935898
-45.286819	1.435828	0.940902
-45.635657	-2.024445	0.945907
-45.734055	-1.344632	0.950912
-45.890252	2.707313	0.955917
-45.643005	-4.902298	0.960922
-45.881609	8.046398	0.965926
-46.868847	2.990378	0.970931
-47.085921	-5.489280	0.975936
-47.301239	5.010179	0.980941
-47.223519	-7.508334	0.985946
-47.212235	-6.450238	0.990950
-47.987579	5.696705	0.995955
-48.279871	2.449034	1.000960
-48.994935	-2.510425	1.005965
-48.892949	-0.596506	1.010970
-49.078275	6.677548	1.015974
-49.256865	-1.235501	1.020979
-48.941134	-4.040601	1.025984
-49.057766	3.127775	1.030989
-50.099861	-2.049362	1.035994
-50.549567	5.417978	1.040998
-50.604778	12.250866	1.046003
-50.461657	1.496970	1.051008
-50.488261	10.011660	1.056013
-50.991898	3.696619	1.061018
-51.285977	4.033769	1.066022
-51.949478	6.694056	1.071027
-52.182695	1.171877	1.076032
-52.226596	2.947303	1.081037
-51.968289	-1.098485	1.086042
-52.512654	-3.477752	1.091046
-52.980003	0.951978	1.096051
-52.941345	0.161313	1.101056
-53.604858	1.144809	1.106061
-53.654727	0.507221	1.111066
-53.374543	0.890432	1.116070
-54.702647	7.312162	1.121075
-54.670873	-3.699532	1.126080
-54.723565	0.668390	1.131085
-55.190108	7.780864	1.136090
-54.917273	7.222426	1.141094
-55.124809	-3.179130	1.146099
-55.931823	-4.084059	1.151104
-56.482432	-0.805547	1.156109
-56.438587	4.518523	1.161114
-56.492405	-6.637944	1.166118
-56.851495	7.234463	1.171123
-56.200335	-8.977422	1.176128
-56.664190	3.687024	1.181133
-57.370872	10.938366	1.186138
-57.815782	-1.646956	1.191142
-58.073293	0.959207	1.196147
-58.219530	-4.396264	1.201152
-58.095290	6.325237	1.206157
-58.432784	-3.072025	1.211162
-58.933345	6.776102	1.216166
-59.388756	-3.431589	1.221171
-59.765468	-2.062761	1.226176
-59.233850	0.634890	1.231181
-59.715332	-4.541501	1.236186
-60.535182	-7.149685	1.241190
-60.770818	0.113267	1.246195
-60.625074	-13.545361	1.251200
-60.911563	-1.376946	1.256205
-61.041955	-5.007487	1.261210
-61.022191	1.791503	1.266214
-61.706116	10.244672	1.271219
-62.099324	-5.496690	1.276224
-62.692669	1.265490	1.281229
-62.532931	2.449022	1.286234
-62.758535	-0.068777	1.291238
-62.841542	-1.457310	1.296243
-62.976313	-10.247254	1.301248
-63.759106	-2.563211	1.306253
-63.963509	-5.505111	1.311258
-63.995290	-2.481900	1.316262
-64.063520	-4.081557	1.321267
-64.056915	-6.515516	1.326272
-64.442819	-2.807231	1.331277
-64.770856	-4.755320	1.336282
-65.007800	-8.144538	1.341286
-65.428594	-5.107830	1.346291
-65.291553	-7.147775	1.351296
-66.019558	-7.514590	1.356301
-66.529818	-7.567509	1.361306
-66.630232	-6.688064	1.366310
-66.804204	-2.386562	1.371315
-66.719860	-13.820937	1.376320
-67.059542	-11.746066	1.381325
-67.319554	-6.469301	1.386330
-67.695982	-6.707707	1.391334
-68.449474	-7.690624	1.396339
-68.403043	-7.115762	1.401344
-68.853480	-3.669448	1.406349
-68.979831	-2.950454	1.411354
-68.425516	-2.012247	1.416358
-68.831251	-0.809714	1.421363
-69.038348	-7.990627	1.426368
-69.447338	-3.060677	1.431373
-69.760730	-6.013972	1.436378
-69.924717	-7.544841	1.441382
-70.710351	0.952734	1.446387
-70.635888	-7.639040	1.451392
-71.213764	-3.492549	1.456397
-71.444083	1.083538	1.461402
-70.962392	-4.572803	1.466406
-71.812377	-1.633359	1.471411
-72.132806	-5.281579	1.476416
-72.844733	-7.770630	1.481421
-72.697309	-2.535559	1.486426
-72.944869	-9.729113	1.491430
-73.054523	-4.494890	1.496435
-72.933086	-8.531885	1.501440
-73.087073	-0.718579	1.506445
-73.734396	3.786809	1.511450
-73.886686	-11.707557	1.516454
-74.462355	-4.676066	1.521459
-74.351649	-5.240737	1.526464
-74.765746	-0.351115	1.531469
-74.810968	1.076504	1.536474
-75.381400	-6.427129	1.541478
-75.993988	0.145077	1.546483
-75.658547	-5.978731	1.551488
-75.908906	2.928519	1.556493
-76.050811	-5.281340	1.561498
-76.009040	-10.166394	1.566502
-76.842859	-4.821864	1.571507
-77.192280	-9.357719	1.576512
-77.479468	3.187294	1.581517
-77.418267	-8.651582	1.586522
-76.961420	-11.760367	1.591526
-77.843406	-6.867036	1.596531
-78.373004	-10.580555	1.601536
-78.601397	-3.628789	1.606541
-78.972085	1.614700	1.611546
-78.739475	-8.283176	1.616550
-78.931035	-3.045610	1.621555
-79.501133	-6.910972	1.626560
-79.890030	5.415862	1.631565
-80.164243	-1.343248	1.636570
-80.305171	-7.003269	1.641574
-80.371770	4.849119	1.646579
-80.408105	-1.428407	1.651584
-80.994730	2.286021	1.656589
-81.559072	8.762085	1.661594
-81.032954	-4.212666	1.666598
-81.535892	9.647480	1.671603
-81.613831	1.354829	1.676608
-82.427839	3.526172	1.681613
-82.823809	9.453833	1.686618
-82.758680	0.034612	1.691622
-82.958295	13.252446	1.696627
-83.098375	-5.233590	1.701632
-83.325037	-0.876376	1.706637
-83.947146	-1.547684	1.711642
-84.032147	-3.853394	1.716646
-84.484742	10.406989	1.721651
-84.411664	-0.136612	1.726656
-84.784132	2.050966	1.731661
-84.543831	-6.541484	1.736666
-85.259588	0.863138	1.741670
-85.774126	3.259639	1.746675
-86.085578	-0.522865	1.751680
-85.743229	-2.724695	1.756685
-85.918344	-2.099301	1.761690
-86.176827	-3.900100	1.766694
-87.230816	-1.371615	1.771699
-87.316541	3.555140	1.776704
-87.587242	4.141728	1.781709
-87.937411	0.071061	1.786714
-87.584691	-5.321462	1.791718
-87.961077	2.143878	1.796723
-87.737733	-4.446420	1.801728
-88.352363	-4.416545	1.806733
-88.865337	2.146380	1.811738
-88.833022	-2.889054	1.816742
-89.153307	-2.057414	1.821747
-89.288231	4.914511	1.826752
-90.082430	8.645647	1.831757
-90.497421	0.829755	1.836762
-90.725683	4.121035	1.841766
-90.573311	3.714350	1.846771
-90.516654	-3.754665	1.851776
-90.954700	2.638332	1.856781
-90.982711	3.484286	1.861786
-90.889582	2.938188	1.866790
-91.812524	3.367550	1.871795
-92.047007	0.904928	1.876800
-92.263354	3.925422	1.881805
-92.301773	2.890570	1.886810
-92.979304	-0.363171	1.891814
-93.782394	6.191431	1.896819
-93.921151	-0.791383	1.901824
-93.621212	-6.204109	1.906829
-93.501035	0.604454	1.911834
-93.479022	-0.101344	1.916838
-94.046173	2.645087	1.921843
-94.717171	-4.241672	1.926848
-95.106359	-0.263951	1.931853
-95.237162	-0.885693	1.936858
-94.965090	-0.887190	1.941862
-95.271099	3.745050	1.946867
-95.193782	0.132584	1.951872
-96.035631	-0.137296	1.956877
-96.390474	-1.037144	1.961882
-96.274097	-3.548415	1.966886
-96.858646	0.181507	1.971891
-96.940291	-11.179401	1.976896
-97.135690	-2.511722	1.981901
-98.205578	4.527611	1.986906
-98.228056	-2.049478	1.991910
-98.424129	4.758021	1.996915
-98.315526	-3.160199	2.006912
-97.833967	5.041840	2.016909
-97.153340	5.299499	2.026906
-97.309239	5.080016	2.036902
-96.826248	3.990646	2.046899
-96.103348	4.609147	2.056896
-95.635478	7.396378	2.066893
-94.925016	6.958779	2.076890
-94.449797	8.132443	2.086886
-94.288876	6.944652	2.096883
-93.588577	13.762933	2.106880
-93.049106	12.075499	2.116877
-92.469996	14.512681	2.126874
-91.365190	7.741025	2.136870
-91.332301	2.344270	2.146867
-91.410602	3.430437	2.156864
-90.660041	8.799487	2.166861
-90.154828	4.678209	2.176858
-89.573033	4.764453	2.186854
-88.857973	1.604986	2.196851
-88.749406	2.436958	2.206848
-88.294505	1.184096	2.216845
-87.814481	5.860605	2.226842
-86.659989	0.326117	2.236838
-86.126186	4.652075	2.246835
-85.802682	0.559270	2.256832
-86.009708	0.522029	2.266829
-85.030214	-4.687263	2.276826
-84.778529	1.716634	2.286822
-83.977847	2.303941	2.296819
-83.397496	0.385189	2.306816
-83.060089	3.443120	2.316813
-82.209460	1.922343	2.326810
-81.712269	1.454807	2.336806
-81.641508	6.509058	2.346803
-81.393528	3.394269	2.356800
-80.769765	-4.502606	2.366797
-79.964334	-4.587619	2.376794
-79.248205	2.408745	2.386790
-78.784099	-0.698728	2.396787
-78.825737	-0.049128	2.406784
-77.969432	1.479807	2.416781
-77.805727	-2.033592	2.426778
-76.593713	1.226251	2.436774
-76.078383	1.601679	2.446771
-76.239587	-3.264149	2.456768
-75.948880	-1.120734	2.466765
-74.911875	-3.107871	2.476762
-74.663146	-1.056080	2.486758
-73.536387	-0.709934	2.496755
-73.013436	1.165842	2.506752
-73.277269	-5.575087	2.516749
-72.771585	2.319063	2.526746
-72.102452	-3.633550	2.536742
-71.668845	-1.886326	2.546739
-70.475329	-1.436599	2.556736
-70.344960	2.341188	2.566733
-70.330399	-3.702096	2.576730
-69.568235	0.283972	2.586726
-68.947290	0.243707	2.596723
-68.767009	-4.026228	2.606720
-67.998464	1.574423	2.616717
-67.705786	-2.988723	2.626714
-66.663389	-0.443568	2.636710
-66.416845	3.211478	2.646707
-66.040393	-8.505037	2.656704
-65.418713	-2.700809	2.666701
-64.848247	-3.392069	2.676698
-64.565226	1.933033	2.686694
-63.972082	-3.583187	2.696691
-63.449091	1.910222	2.706688
-63.241752	-7.362756	2.716685
-62.107093	6.480192	2.726682
-62.146657	5.333319	2.736678
-61.474677	1.052863	2.746675
-60.781579	-1.501277	2.756672
-60.663889	0.843479	2.766669
-59.840071	5.111327	2.776666
-59.528992	1.726890	2.786662
-59.142570	0.117293	2.796659
-58.010670	-5.347127	2.806656
-57.307949	0.754849	2.816653
-57.367237	6.244462	2.826650
-57.497908	3.325219	2.836646
-56.458825	-4.975687	2.846643
-56.277547	0.789843	2.856640
-55.193073	1.006402	2.866637
-54.709220	0.119638	2.876634
-54.369503	2.521472	2.886630
-54.207921	1.365257	2.896627
-53.224599	5.978747	2.906624
-53.060494	-0.436430	2.916621
-52.613995	-0.797819	2.926618
-51.999441	-3.171758	2.936614
-51.467138	-0.796932	2.946611
-50.270438	0.399902	2.956608
-50.157834	-0.792988	2.966605
-50.233347	0.473307	2.976602
-49.657108	-1.166031	2.986598
-48.900261	-2.038549	2.996595
-48.558280	-3.286387	3.006592
-47.335680	-8.175804	3.016589
-47.363827	1.718519	3.026586
-47.308121	4.741396	3.036582
-46.653671	-6.191881	3.046579
-45.687137	-1.376189	3.056576
-45.549247	-8.104037	3.066573
-44.804457	-2.841785	3.076570
-44.288509	-8.032294	3.086566
-44.065778	-4.516068	3.096563
-43.350536	-9.199276	3.106560
-43.159262	-3.026665	3.116557
-42.271639	-7.198355	3.126554
-41.625492	-8.997533	3.136550
-41.441876	-5.091874	3.146547
-41.012479	-3.362996	3.156544
-40.076328	-2.277390	3.166541
-40.131615	-3.725910	3.176538
-39.575958	1.974626	3.186534
-39.033435	0.277215	3.196531
-38.383808	-3.527733	3.206528
-37.597598	2.374265	3.216525
-37.379204	2.571306	3.226522
-36.966956	0.225899	3.236518
-36.431042	2.967626	3.246515
-35.631842	-3.154253	3.256512
-35.667560	-5.784264	3.266509
-35.122884	-4.044938	3.276506
-34.163982	4.354747	3.286502
-34.152376	3.367750	3.296499
-33.132147	4.075885	3.306496
-32.827885	-0.172296	3.316493
-32.705394	4.186437	3.326490
-31.780172	4.478636	3.336486
-31.313789	0.262074	3.346483
-31.005538	-0.375427	3.356480
-30.158607	-0.473273	3.366477
-30.135093	-1.040817	3.376474
-29.335976	-1.368757	3.386470
-28.311990	4.958487	3.396467
-28.000085	-0.833615	3.406464
-28.127112	-3.148378	3.416461
-27.764954	-1.139700	3.426458
-26.777033	-5.666060	3.436454
-26.517359	-0.714268	3.446451
-25.581927	-1.909371	3.456448
-25.198789	1.258607	3.466445
-25.162480	5.985639	3.476442
-24.114770	-3.349325	3.486438
-23.833451	-2.861201	3.496435
-23.490417	-3.339425	3.506432
-22.727073	-7.988988	3.516429
-22.169611	-4.081715	3.526426
-22.192271	0.410634	3.536422
-21.359300	-3.860198	3.546419
-21.052075	-4.345483	3.556416
-20.159173	-6.002758	3.566413
-19.456168	-0.404502	3.576410
-19.472213	1.365661	3.586406
-19.290748	3.827139	3.596403
-17.937859	2.541284	3.606400
-18.228724	1.025138	3.616397
-17.368675	1.615821	3.626394
-16.800578	2.515177	3.636390
-16.462119	0.273198	3.646387
-15.408430	0.953918	3.656384
-15.181873	-2.255716	3.666381
-15.118869	3.994018	3.676378
-14.697518	-2.949309	3.686374
-13.634490	-1.196165	3.696371
-13.345108	-1.146461	3.706368
-12.436865	4.980342	3.716365
-12.156519	0.583853	3.726362
-12.308267	-1.426095	3.736358
-11.295605	1.564052	3.746355
-10.629410	-4.087156	3.756352
-10.430989	1.583825	3.766349
-9.531273	-0.518010	3.776346
-8.904388	3.609638	3.786342
-9.139862	-3.617248	3.796339
-8.499231	2.836588	3.806336
-7.544583	1.565616	3.816333
-7.643162	5.388782	3.826330
-6.735078	5.452419	3.836326
-6.170597	4.210901	3.846323
-6.137239	4.550977	3.856320
-5.486279	-2.555039	3.866317
-4.974286	6.380344	3.876314
-3.923848	6.823989	3.886310
-3.496417	5.144611	3.896307
-3.452403	8.840899	3.906304
-3.259250	0.612347	3.916301
-2.986544	13.453125	3.926298
-2.125553	33.316654	3.936294
-1.821865	43.827421	3.946291
-1.169024	56.798738	3.956288
-0.728818	68.834027	3.966285
-0.441294	81.862602	3.976282
0.113461	101.609463	3.986278
0.000000	113.155533	3.991283
0.286530	122.212843	3.996288
1.003444	131.905085	4.001293
1.368243	141.883459	4.006298
1.148421	143.718101	4.011302
1.346449	141.048481	4.016307
1.066691	151.785919	4.021312
1.279367	145.314295	4.026317
1.759843	162.374094	4.031322
1.576470	152.148992	4.036326
1.682647	153.233359	4.041331
1.199149	153.492620	4.046336
1.578794	157.131610	4.051341
1.922750	154.170202	4.056346
1.558390	147.089792	4.061350
1.882857	141.973737	4.066355
1.676548	140.775354	4.071360
1.687455	144.307600	4.076365
1.617580	143.378909	4.081370
1.892514	144.354576	4.086374
1.574732	138.377360	4.091379
1.642785	148.870473	4.096384
1.530702	144.098067	4.101389
1.699294	147.387305	4.106394
1.756026	152.244326	4.111398
1.711013	153.649779	4.116403
1.687941	152.302462	4.121408
1.679237	147.928313	4.126413
1.451497	151.029711	4.131418
1.671276	153.488345	4.136422
1.908561	149.857110	4.141427
1.330243	152.307913	4.146432
1.821446	154.126064	4.151437
1.923645	170.235892	4.156442
1.945647	172.788793	4.161446
2.020468	168.673638	4.166451
1.712177	163.422599	4.171456
1.967630	171.443917	4.176461
2.183499	155.587987	4.181466
2.117817	152.485116	4.186470
1.931295	150.486358	4.191475
1.482110	155.384683	4.196480
1.232399	151.228631	4.201485
1.470760	168.579475	4.206490
2.253896	175.872703	4.211494
2.191034	169.915647	4.216499
2.101363	177.301337	4.221504
1.803388	177.553676	4.226509
2.015574	174.419919	4.231514
1.832216	177.232791	4.236518
2.077674	169.895470	4.241523
1.707903	182.845864	4.246528
2.349244	167.815449	4.251533
2.610347	161.108439	4.256538
2.280259	177.599220	4.261542
2.322536	165.949850	4.266547
1.796295	166.858057	4.271552
2.137044	162.172884	4.276557
2.632172	175.212388	4.281562
2.081105	158.717310	4.286566
1.755143	149.175783	4.291571
1.922884	161.453479	4.296576
2.048212	159.583031	4.301581
2.221484	171.081575	4.306586
2.131264	182.349325	4.311590
2.308304	167.673235	4.316595
2.186142	177.272341	4.321600
2.471711	169.191572	4.326605
2.791262	167.913959	4.331610
1.981920	169.034204	4.336614
2.533299	171.757264	4.341619
2.255224	174.626105	4.346624
1.987326	167.423004	4.351629
2.332628	166.486209	4.356634
2.501097	165.096224	4.361638
2.409223	174.317256	4.366643
2.284531	179.335590	4.371648
2.374472	171.760041	4.376653
2.310879	181.830869	4.381658
2.211586	174.398864	4.386662
2.862146	167.067676	4.391667
2.407732	173.637307	4.396672
2.329055	167.388497	4.401677
2.360888	162.489131	4.406682
2.436142	173.791061	4.411686
2.428741	165.310102	4.416691
2.225610	178.746919	4.421696
2.422448	167.320106	4.426701
2.644348	166.611456	4.431706
2.276411	180.820751	4.436710
2.302973	164.184543	4.441715
2.213822	178.669697	4.446720
2.247067	170.517730	4.451725
2.266940	159.118650	4.456730
2.078830	165.649716	4.461734
2.165676	165.335554	4.466739
2.139467	183.544124	4.471744
2.662180	191.115447	4.476749
2.593527	187.956087	4.481754
2.663417	194.133524	4.486758
2.739941	198.826104	4.491763
2.988849	197.015384	4.496768
2.535001	194.954101	4.501773
2.615916	200.503382	4.506778
2.860061	203.720680	4.511782
2.792396	201.155957	4.516787
2.720036	191.913198	4.521792
2.736396	195.893858	4.526797
2.688790	192.414820	4.531802
2.747989	202.621446	4.536806
2.943039	194.773151	4.541811
2.872823	202.238061	4.546816
3.298270	202.541571	4.551821
2.999221	192.084630	4.556826
2.564859	178.899560	4.561830
2.457782	178.894196	4.566835
2.264476	190.247706	4.571840
2.515435	189.904666	4.576845
2.819880	195.058249	4.581850
2.449623	202.981464	4.586854
2.514896	195.042770	4.591859
3.033746	209.056194	4.596864
2.941668	196.833061	4.601869
3.135704	196.796336	4.606874
2.973469	194.420440	4.611878
3.162992	199.769203	4.616883
2.980520	199.949661	4.621888
2.894604	191.256363	4.626893
2.670573	203.861231	4.631898
2.677533	199.649132	4.636902
3.089265	185.391842	4.641907
3.001622	204.144740	4.646912
3.244509	205.808812	4.651917
3.012038	200.159898	4.656922
3.214786	195.980400	4.661926
3.214053	196.872711	4.666931
3.185865	200.401601	4.671936
2.958814	199.551319	4.676941
3.310957	202.286618	4.681946
2.867396	200.644507	4.686950
3.209364	199.521569	4.691955
3.120441	196.197703	4.696960
3.037637	192.205317	4.701965
3.206906	198.642435	4.706970
3.253368	209.474329	4.711974
3.185680	207.811291	4.716979
3.287360	206.966450	4.721984
3.222866	212.411965	4.726989
3.024593	209.276074	4.731994
3.080332	218.046888	4.736998
3.408990	225.550553	4.742003
3.705733	223.191326	4.747008
3.346713	217.846977	4.752013
3.204818	211.639694	4.757018
3.175434	214.776464	4.762022
3.382008	213.658920	4.767027
3.401432	219.224169	4.772032
3.392007	232.143449	4.777037
3.389655	222.133557	4.782042
3.454394	226.616015	4.787046
3.835422	222.142819	4.792051
3.064050	205.584137	4.797056
2.985115	211.205924	4.802061
3.275128	227.659705	4.807066
3.191474	221.724872	4.812070
3.627873	211.478559	4.817075
3.485643	229.506035	4.822080
3.739220	221.787764	4.827085
3.807145	211.972513	4.832090
3.385088	221.305415	4.837094
3.623969	217.914365	4.842099
3.567266	224.915252	4.847104
3.373426	221.481267	4.852109
3.619350	216.216144	4.857114
3.971524	227.889177	4.862118
3.791469	209.738201	4.867123
3.239134	203.699636	4.872128
3.592301	212.958527	4.877133
3.783211	223.245770	4.882138
3.150634	220.019735	4.887142
3.666491	217.528099	4.892147
3.641135	222.249303	4.897152
3.688881	224.298298	4.902157
3.650498	220.368549	4.907162
3.358335	231.057358	4.912166
3.905348	221.954823	4.917171
3.608651	227.787907	4.922176
3.356141	227.723071	4.927181
3.481488	227.102314	4.932186
3.158349	227.763563	4.937190
3.523948	225.225866	4.942195
3.612367	239.547204	4.947200
3.932844	249.703429	4.952205
4.098524	239.755785	4.957210
3.384720	253.519447	4.962214
3.853449	241.812701	4.967219
3.848204	255.370432	4.972224
3.561951	251.454204	4.977229
3.885064	249.268014	4.982234
3.719439	256.244851	4.987238
3.904678	250.024265	4.992243
3.945815	256.937068	4.997248
3.840234	247.724795	5.002253
4.190255	249.780216	5.007258
3.959335	256.666042	5.012262
4.019497	248.879987	5.017267
4.041804	247.822950	5.022272
3.901996	253.935186	5.027277
4.063428	249.914012	5.032282
3.852662	250.124213	5.037286
4.331763	243.598155	5.042291
3.727679	252.791912	5.047296
3.880387	252.720533	5.052301
3.913258	239.746954	5.057306
3.732620	253.825718	5.062310
4.110207	250.450894	5.067315
3.584878	254.880278	5.072320
3.831332	254.553762	5.077325
3.955992	249.307629	5.082330
3.631003	269.091217	5.087334
4.332709	263.381337	5.092339
4.576601	271.822135	5.097344
4.286977	261.790790	5.102349
4.390181	254.042282	5.107354
4.069141	249.644278	5.112358
3.689672	240.639441	5.117363
3.713504	254.097701	5.122368
3.884771	271.323113	5.127373
4.189247	266.352527	5.132378
4.173291	279.266537	5.137382
4.337816	266.487450	5.142387
4.238767	281.486775	5.147392
4.270013	274.119699	5.152397
4.153215	267.418074	5.157402
3.972276	276.956840	5.162406
4.223690	271.852194	5.167411
3.893494	269.913899	5.172416
4.207691	288.774770	5.177421
4.751245	287.667699	5.182426
4.145805	287.572737	5.187430
4.210693	295.829618	5.192435
4.274933	304.738350	5.197440
4.372540	304.112445	5.202445
4.401139	302.469114	5.207450
4.429928	305.157015	5.212454
4.748096	297.868362	5.217459
4.785013	295.442266	5.222464
4.773445	304.078132	5.227469
4.533666	278.548938	5.232474
4.175939	283.686072	5.237478
4.533846	289.679208	5.242483
4.342242	291.626504	5.247488
4.381044	299.140814	5.252493
4.642864	301.931411	5.257498
4.335996	299.824939	5.262502
4.888516	295.780444	5.267507
4.771971	297.570445	5.272512
4.475363	295.936939	5.277517
4.732916	291.837418	5.282522
4.352188	297.987417	5.287526
4.318049	300.564952	5.292531
4.511977	305.245492	5.297536
4.676023	296.209251	5.302541
4.667666	296.925588	5.307546
4.672456	298.339068	5.312550
4.776293	301.106960	5.317555
4.544689	306.145244	5.322560
4.439986	303.959639	5.327565
4.572019	307.105936	5.332570
4.995604	311.355018	5.337574
4.661629	315.472855	5.342579
4.475043	304.599586	5.347584
4.507239	312.899563	5.352589
4.726029	305.348062	5.357594
4.915677	318.802537	5.362598
4.882923	322.253072	5.367603
4.924098	321.164600	5.372608
4.817781	321.564085	5.377613
4.756111	326.287842	5.382618
4.919346	335.586048	5.387622
5.136009	322.646887	5.392627
4.997625	314.129432	5.397632
4.665921	312.419164	5.402637
5.062760	317.675368	5.407642
5.196745	320.131649	5.412646
5.142462	313.723938	5.417651
4.823703	314.188347	5.422656
4.805540	312.235960	5.427661
5.382912	318.261159	5.432666
4.967139	304.949695	5.437670
4.988553	305.892325	5.442675
5.080008	307.716178	5.447680
4.842781	306.003763	5.452685
5.085036	307.436985	5.457690
5.094776	323.586749	5.462694
4.987444	323.018265	5.467699
5.372783	327.279670	5.472704
4.868209	327.684607	5.477709
5.411012	313.514248	5.482714
5.280547	324.503650	5.487718
4.532661	318.802575	5.492723
5.005785	332.804279	5.497728
5.192562	329.294818	5.502733
5.215471	340.744263	5.507738
4.976239	346.040023	5.512742
5.308350	338.717531	5.517747
5.553461	338.081170	5.522752
5.391102	339.378470	5.527757
5.271621	325.188481	5.532762
5.392629	337.960850	5.537766
5.372058	334.395289	5.542771
4.945437	331.640010	5.547776
5.277647	339.329833	5.552781
5.247478	344.893399	5.557786
5.427737	332.140274	5.562790
5.538762	340.241247	5.567795
5.309696	338.916700	5.572800
5.199004	343.781023	5.577805
5.134170	342.835712	5.582810
5.410692	343.219507	5.587814
5.779901	340.538856	5.592819
5.368917	337.784291	5.597824
5.278827	338.507108	5.602829
5.599249	329.927250	5.607834
5.166611	339.204922	5.612838
5.323341	335.589434	5.617843
5.674177	344.804466	5.622848
5.660491	337.754458	5.627853
5.813020	334.187086	5.632858
5.714992	340.716757	5.637862
5.441073	331.192288	5.642867
5.372875	329.905812	5.647872
5.658970	332.781197	5.652877
5.588592	329.856205	5.657882
5.591302	340.356505	5.662886
5.557313	333.850693	5.667891
5.615943	332.129886	5.672896
5.288474	338.872679	5.677901
5.290683	323.382278	5.682906
5.420529	338.402737	5.687910
5.115990	327.563754	5.692915
4.988701	333.702530	5.697920
5.396415	343.560396	5.702925
6.079863	352.312020	5.707930
5.888438	360.109206	5.712934
5.657910	337.071573	5.717939
5.431843	337.673323	5.722944
5.586039	352.196422	5.727949
5.611458	362.054084	5.732954
5.873627	365.221131	5.737958
5.633944	369.703866	5.742963
5.979305	361.806636	5.747968
5.898546	371.930882	5.752973
5.760963	356.237723	5.757978
5.943847	365.013998	5.762982
5.857611	361.028440	5.767987
5.997329	368.087195	5.772992
5.790329	368.689123	5.777997
5.935807	352.660545	5.783002
5.754901	361.272350	5.788006
5.725059	365.323563	5.793011
5.985180	363.805306	5.798016
5.711868	370.204260	5.803021
5.887936	360.264413	5.808026
5.694815	366.742553	5.813030
5.937540	362.309974	5.818035
6.123645	362.075172	5.823040
5.828705	366.313458	5.828045
6.119466	360.927369	5.833050
5.696072	361.354388	5.838054
5.948266	370.977203	5.843059
5.814335	354.622234	5.848064
5.618432	365.378300	5.853069
6.029437	359.229872	5.858074
6.144983	367.716136	5.863078
5.900799	367.276663	5.868083
5.963684	370.326235	5.873088
5.797625	377.309515	5.878093
6.586196	381.052163	5.883098
6.127380	399.192689	5.888102
6.116595	393.622878	5.893107
6.233217	395.673756	5.898112
6.411913	399.331626	5.903117
6.203466	391.470533	5.908122
6.025328	382.120860	5.913126
6.304608	379.988980	5.918131
6.364041	385.873886	5.923136
5.736729	376.170640	5.928141
6.426952	382.301569	5.933146
6.138845	394.723617	5.938150
6.364049	390.844283	5.943155
6.588114	393.954028	5.948160
6.322305	390.702134	5.953165
6.380401	378.480657	5.958170
6.283369	386.446566	5.963174
6.419859	378.752902	5.968179
6.683734	369.941434	5.973184
6.150585	376.716468	5.978189
6.478394	361.934336	5.983194
6.154447	373.197698	5.988198
6.627462	382.498012	5.993203
6.451539	367.646101	5.998208
6.174372	373.185100	6.003213
6.410226	378.640556	6.008218
6.552502	386.796766	6.013222
6.071795	386.378532	6.018227
6.276899	390.133506	6.023232
6.518231	389.561011	6.028237
6.564558	381.596728	6.033242
6.505984	392.552760	6.038246
6.402288	394.135109	6.043251
6.519878	387.823832	6.048256
6.055942	386.640488	6.053261
6.296115	380.885823	6.058266
6.593464	382.677424	6.063270
6.412009	386.173416	6.068275
6.689463	390.695356	6.073280
6.459311	384.255063	6.078285
6.099810	368.508077	6.083290
6.400576	380.391750	6.088294
6.395137	392.193691	6.093299
6.503084	392.743109	6.098304
6.466983	393.245492	6.103309
6.280079	383.859224	6.108314
6.321779	394.147798	6.113318
6.298741	386.947372	6.118323
6.568299	390.549874	6.123328
6.401212	392.945768	6.128333
6.283461	382.577370	6.133338
6.340509	393.018566	6.138342
6.490584	394.146692	6.143347
6.726632	393.429489	6.148352
6.509205	383.177951	6.153357
6.370642	371.585255	6.158362
6.194003	375.520263	6.163366
6.471311	384.617119	6.168371
6.597056	375.276785	6.173376
6.250524	373.654257	6.178381
6.701763	378.088852	6.183386
6.038889	370.953881	6.188390
6.467972	372.781789	6.193395
6.741504	384.505213	6.198400
6.546035	373.396006	6.203405
6.256888	367.331966	6.208410
6.177603	364.224862	6.213414
6.004180	366.868524	6.218419
6.432463	372.227387	6.223424
6.436104	387.935229	6.228429
6.858840	380.180895	6.233434
6.429395	372.781553	6.238438
6.411281	361.948293	6.243443
6.254106	359.087517	6.248448
6.367571	376.663780	6.253453
6.268344	368.880500	6.258458
6.686198	374.532070	6.263462
6.774443	375.492707	6.268467
6.197753	366.945823	6.273472
5.853723	363.320202	6.278477
6.639964	372.365786	6.283482
6.623441	376.987568	6.288486
6.153442	377.431381	6.293491
6.548000	369.472654	6.298496
6.325018	372.687243	6.303501
6.406887	372.263123	6.308506
6.326416	371.956190	6.313510
6.267186	372.870330	6.318515
6.590315	373.876425	6.323520
6.409547	371.500245	6.328525
6.802665	377.348685	6.333530
6.453619	360.400978	6.338534
6.255740	369.752617	6.343539
6.257881	361.896508	6.348544
6.147502	359.920598	6.353549
6.491080	368.659042	6.358554
6.538004	383.923490	6.363558
6.287555	373.730917	6.368563
6.177427	376.823417	6.373568
6.452835	380.295284	6.378573
6.660689	383.265196	6.383578
6.396864	376.687809	6.388582
6.446612	370.235304	6.393587
6.254011	361.533328	6.398592
6.042215	377.081922	6.403597
6.259993	384.840315	6.408602
6.318640	386.299148	6.413606
6.139358	388.235032	6.418611
6.493835	382.671271	6.423616
6.318254	388.131081	6.428621
6.371280	383.051160	6.433626
6.397076	388.299080	6.438630
6.526119	389.072988	6.443635
6.713441	384.905355	6.448640
6.514873	392.849210	6.453645
6.792485	385.484617	6.458650
6.719814	394.000383	6.463654
6.539256	380.920933	6.468659
6.246906	366.052464	6.473664
5.973445	365.038598	6.478669
6.430994	374.632403	6.483674
6.368720	385.490932	6.488678
6.625831	380.995982	6.493683
6.325752	388.228060	6.498688
6.517538	390.127952	6.503693
6.258707	378.060538	6.508698
6.340859	376.854909	6.513702
6.222034	384.488867	6.518707
6.297378	379.759798	6.523712
6.231108	387.686087	6.528717
6.252793	382.516162	6.533722
6.287262	392.271180	6.538726
5.940560	386.703382	6.543731
6.506989	381.416467	6.548736
6.355645	390.245122	6.553741
6.421887	386.583689	6.558746
6.330807	382.216062	6.563750
6.186427	385.687262	6.568755
6.296863	388.969839	6.573760
5.927506	391.650530	6.578765
6.505145	389.652241	6.583770
6.395194	385.749489	6.588774
6.143131	385.213171	6.593779
6.595598	386.977304	6.598784
6.468329	390.287633	6.603789
6.128280	388.553354	6.608794
6.606599	388.959317	6.613798
6.283081	384.368674	6.618803
6.709739	387.835827	6.623808
6.453783	390.799315	6.628813
6.924878	384.230166	6.633818
6.909303	383.527078	6.638822
6.591501	388.284655	6.643827
6.724593	391.244135	6.648832
6.557015	389.052552	6.653837
6.551411	385.975029	6.658842
6.491094	383.921669	6.663846
6.505318	384.463624	6.668851
6.584998	375.991068	6.673856
6.162983	376.658323	6.678861
6.780906	376.355862	6.683866
6.393338	363.185470	6.688870
5.860271	364.227637	6.693875
6.510661	374.828962	6.698880
6.601323	385.739461	6.703885
6.422429	374.472629	6.708890
6.530164	374.373495	6.713894
6.328876	369.548565	6.718899
6.540753	373.685296	6.723904
6.047959	370.231683	6.728909
6.471742	368.308123	6.733914
6.628310	373.589334	6.738918
6.257019	375.852702	6.743923
6.552811	371.974967	6.748928
6.364800	371.444433	6.753933
6.231678	368.896269	6.758938
6.544674	361.674841	6.763942
5.986956	382.023377	6.768947
6.753795	375.888796	6.773952
6.509421	379.255437	6.778957
6.605730	376.728273	6.783962
6.332558	374.277983	6.788966
6.017878	375.577005	6.793971
6.225435	384.067843	6.798976
6.297518	386.505358	6.803981
6.763282	385.885044	6.808986
6.333456	383.962347	6.813990
6.509017	392.603738	6.818995
6.506446	386.244848	6.824000
6.260711	375.194138	6.829005
6.715205	382.118156	6.834010
6.319772	372.679143	6.839014
6.316926	374.369078	6.844019
6.482325	369.701835	6.849024
6.069084	364.603224	6.854029
6.471130	380.229653	6.859034
6.341135	384.495884	6.864038
5.853017	384.974175	6.869043
6.478993	382.060294	6.874048
6.267189	395.267672	6.879053
6.282981	384.533492	6.884058
6.495777	388.758670	6.889062
6.343445	393.566254	6.894067
6.438558	386.147995	6.899072
6.391501	387.996722	6.904077
6.655514	387.692763	6.909082
6.633290	394.289673	6.914086
6.507210	390.936789	6.919091
7.026823	385.451560	6.924096
6.128776	380.134668	6.929101
6.453521	371.051065	6.934106
6.702984	370.926560	6.939110
6.480147	371.493003	6.944115
6.434526	362.543365	6.949120
6.484484	365.740498	6.954125
6.862603	364.311323	6.959130
6.417978	363.922238	6.964134
6.003645	369.792782	6.969139
6.215589	367.152587	6.974144
6.247742	366.540100	6.979149
6.303475	363.329582	6.984154
6.470603	368.700888	6.989158
6.224281	364.607531	6.994163
6.464788	361.184560	6.999168
6.491188	374.221720	7.004173
6.593585	369.374518	7.009178
6.459203	368.917841	7.014182
6.169256	365.954477	7.019187
6.337201	360.692038	7.024192
6.362586	367.831983	7.029197
6.316384	372.040789	7.034202
6.484207	380.091751	7.039206
6.463979	388.694213	7.044211
6.479587	373.400991	7.049216
6.264747	374.684369	7.054221
6.573731	379.770855	7.059226
6.444909	367.550197	7.064230
6.148818	370.877482	7.069235
6.272924	377.454622	7.074240
6.458522	380.162259	7.079245
6.593421	379.293222	7.084250
6.291249	375.072569	7.089254
6.278868	379.978447	7.094259
6.550758	388.557286	7.099264
6.470094	393.777594	7.104269
6.247327	377.281496	7.109274
6.579326	384.325950	7.114278
6.370811	374.674148	7.119283
6.363549	380.053798	7.124288
6.567191	382.663693	7.129293
6.188100	379.533956	7.134298
6.657609	385.560259	7.139302
6.116089	379.940728	7.144307
6.735597	381.397107	7.149312
6.089929	385.266397	7.154317
6.519023	388.144696	7.159322
6.490417	386.940601	7.164326
6.277667	386.186147	7.169331
6.446755	377.566701	7.174336
6.469521	380.948435	7.179341
6.174487	377.875133	7.184346
6.323233	378.661772	7.189350
6.118250	385.511945	7.194355
6.300751	385.628892	7.199360
6.595242	399.778863	7.204365
6.472178	403.892149	7.209370
6.319954	399.271499	7.214374
6.360944	403.909588	7.219379
6.736129	394.637731	7.224384
6.542324	404.836657	7.229389
6.467446	386.703824	7.234394
6.461966	388.090445	7.239398
6.222221	392.911725	7.244403
7.050395	380.221568	7.249408
6.366983	379.882552	7.254413
6.333413	368.896681	7.259418
6.493330	365.122497	7.264422
6.279994	362.112328	7.269427
6.197155	362.043053	7.274432
6.356682	357.977860	7.279437
6.265684	367.157724	7.284442
6.492584	372.310854	7.289446
6.473127	383.871371	7.294451
6.623523	374.717004	7.299456
6.252735	373.190028	7.304461
6.362393	375.457135	7.309466
6.494744	359.332529	7.314470
6.238876	375.403730	7.319475
6.338518	368.782053	7.324480
6.459536	384.749918	7.329485
6.721539	383.538255	7.334490
6.190857	374.667776	7.339494
5.850363	374.037744	7.344499
6.626633	382.673597	7.349504
6.351998	392.575126	7.354509
6.514878	394.444745	7.359514
6.498124	393.956982	7.364518
6.490481	393.458299	7.369523
6.571328	388.222154	7.374528
6.778453	379.153811	7.379533
6.405597	374.906267	7.384538
6.378259	369.022674	7.389542
6.556037	365.517780	7.394547
6.473714	359.702918	7.399552
6.211842	367.216909	7.404557
6.028581	373.895992	7.409562
6.332105	365.053003	7.414566
6.341134	371.483652	7.419571
6.450245	382.774082	7.424576
6.270167	386.086357	7.429581
6.278659	383.095213	7.434586
6.602816	388.258419	7.439590
6.529009	386.833610	7.444595
6.253292	372.978118	7.449600
6.450352	378.683267	7.454605
6.452848	379.328302	7.459610
6.465340	369.622892	7.464614
6.321473	368.854482	7.469619
6.427356	372.460479	7.474624
6.547727	377.725216	7.479629
6.313570	375.439660	7.484634
6.523523	358.572052	7.489638
6.358978	368.095642	7.494643
6.810005	365.671093	7.499648
6.446330	361.270250	7.504653
6.336744	366.279942	7.509658
6.353032	366.549484	7.514662
6.294041	365.486196	7.519667
6.303349	358.505344	7.524672
6.121930	362.573979	7.529677
6.157722	374.394759	7.534682
6.563742	373.505389	7.539686
6.555461	382.207218	7.544691
6.414234	386.870688	7.549696
6.316253	377.024392	7.554701
6.205563	379.955626	7.559706
6.998956	381.770748	7.564710
6.057543	378.564598	7.569715
6.472094	368.324783	7.574720
6.343444	372.255435	7.579725
6.567309	378.766323	7.584730
6.230078	366.467586	7.589734
6.399971	366.092952	7.594739
6.454925	372.152566	7.599744
6.641739	378.640785	7.604749
6.352205	364.354020	7.609754
6.624625	359.660519	7.614758
6.441099	371.370124	7.619763
6.386414	361.051970	7.624768
6.617880	358.573237	7.629773
6.523850	369.531647	7.634778
6.532460	362.234521	7.639782
6.141655	366.677657	7.644787
6.422404	366.535595	7.649792
6.415453	365.296470	7.654797
6.449953	362.560688	7.659802
6.669950	359.669290	7.664806
6.316432	360.664341	7.669811
6.306271	356.632063	7.674816
6.769346	361.602649	7.679821
6.554724	356.665913	7.684826
6.680436	353.605787	7.689830
6.681463	366.830419	7.694835
6.348293	363.763094	7.699840
6.601690	361.553012	7.704845
6.279142	359.521758	7.709850
6.514566	361.765995	7.714854
6.453430	368.207636	7.719859
6.582704	367.019935	7.724864
6.667283	356.676800	7.729869
6.452028	369.286737	7.734874
6.538404	360.705569	7.739878
6.085704	368.113415	7.744883
6.409841	360.459962	7.749888
6.610552	365.076178	7.754893
6.610049	365.079426	7.759898
6.426304	354.303760	7.764902
6.206756	362.861508	7.769907
6.508551	360.903277	7.774912
6.278666	362.926183	7.779917
6.431296	369.657042	7.784922
5.945643	360.918722	7.789926
6.274797	371.510265	7.794931
6.455169	356.820843	7.799936
6.257338	371.430752	7.804941
6.256978	369.219299	7.809946
6.699028	360.541274	7.814950
6.533117	365.512333	7.819955
6.394037	364.382497	7.824960
6.523590	366.921739	7.829965
6.183188	363.536001	7.834970
6.521080	356.010111	7.839974
6.754333	371.808515	7.844979
6.414021	366.742770	7.849984
6.515361	368.508132	7.854989
6.192638	363.186526	7.859994
6.707144	366.412115	7.864998
6.368212	354.303483	7.870003
6.140868	361.527317	7.875008
6.345602	358.097297	7.880013
6.031926	359.747345	7.885018
6.559494	358.914864	7.890022
6.081226	363.257804	7.895027
6.583060	366.118375	7.900032
6.578267	362.490224	7.905037
6.411159	365.142387	7.910042
6.613549	360.402910	7.915046
6.648407	357.809445	7.920051
6.649115	357.961203	7.925056
6.510420	347.918817	7.930061
6.367142	339.759628	7.935066
6.631350	331.353096	7.940070
6.313842	338.094329	7.945075
6.305768	345.312276	7.950080
6.485352	336.055277	7.955085
6.001807	331.885199	7.960090
6.365436	341.009637	7.965094
6.427274	363.722532	7.970099
6.480148	359.588626	7.975104
6.536650	358.266791	7.980109
6.619707	362.749578	7.985114
6.561021	349.293543	7.990118
5.986939	342.206157	7.995136
5.941048	341.102528	8.000154
6.215574	357.958571	8.005171
6.373531	359.435966	8.010189
6.176326	361.372945	8.015206
6.203540	367.058512	8.020224
6.654806	361.648275	8.025242
6.459606	361.284396	8.030259
6.137139	366.084336	8.035277
6.708215	360.380777	8.040294
6.434284	367.473658	8.045312
6.504139	366.512836	8.050330
6.610103	361.500680	8.055347
6.460130	367.911430	8.060365
6.484209	363.839895	8.065382
6.202802	370.498454	8.070400
5.992946	364.832046	8.075418
6.442777	356.733334	8.080435
5.897694	361.874261	8.085453
6.313687	364.611397	8.090470
6.185020	367.086740	8.095488
6.531712	376.581741	8.100506
6.954519	378.301659	8.105523
6.383218	375.188084	8.110541
6.416895	366.880020	8.115558
6.272996	377.168245	8.120576
6.821962	387.051275	8.125594
6.804511	390.610555	8.130611
6.329185	380.599232	8.135629
6.679474	364.951764	8.140646
6.612777	365.501853	8.145664
6.479829	362.862388	8.150682
6.475180	374.151258	8.155699
6.660831	374.731236	8.160717
6.477275	358.558356	8.165734
6.305902	374.648005	8.170752
6.880517	382.595691	8.175770
6.732191	389.129266	8.180787
6.457387	374.674778	8.185805
6.546192	380.902956	8.190822
6.773803	391.798846	8.195840
6.813149	373.861671	8.200858
6.456389	373.526260	8.205875
6.481882	365.771736	8.210893
6.828200	378.794932	8.215910
6.635866	386.802828	8.220928
6.571386	374.158350	8.225946
6.750087	370.687426	8.230963
6.454162	379.670899	8.235981
6.682924	378.221283	8.240998
6.649579	393.266856	8.246016
6.747743	389.966336	8.251034
6.945205	378.675658	8.256051
6.311940	372.775791	8.261069
6.603444	373.411767	8.266086
7.028294	386.428975	8.271104
6.970780	377.160065	8.276122
6.776334	365.246001	8.281139
6.790381	368.203903	8.286157
6.673626	367.796175	8.291174
6.634071	362.781573	8.296192
6.608694	365.524749	8.301210
6.705274	363.897031	8.306227
6.643498	372.338893	8.311245
6.802278	370.035565	8.316262
6.576286	375.697692	8.321280
6.417974	378.057762	8.326298
7.103682	381.352236	8.331315
6.985630	384.605389	8.336333
6.668280	374.897517	8.341350
6.628125	376.639480	8.346368
7.048832	385.763133	8.351386
6.815430	365.003274	8.356403
6.610410	372.741757	8.361421
6.580510	372.563413	8.366438
7.061301	378.193694	8.371456
6.899837	381.087581	8.376474
6.817757	367.956723	8.381491
6.478509	374.905208	8.386509
6.844164	375.965060	8.391526
6.717776	386.490384	8.396544
6.564952	392.832164	8.401562
6.758283	386.812247	8.406579
6.834464	391.152108	8.411597
7.008512	387.372646	8.416614
6.657122	389.116038	8.421632
6.968234	384.298947	8.426650
7.231977	383.405574	8.431667
7.121661	388.708759	8.436685
6.862556	385.379011	8.441702
7.029788	380.060609	8.446720
6.730189	370.747582	8.451738
6.835968	366.533860	8.456755
6.984515	373.797230	8.461773
7.068873	373.534713	8.466790
6.848452	372.755069	8.471808
6.856011	371.381137	8.476826
6.992215	367.645477	8.481843
6.602838	373.137546	8.486861
6.863098	381.131330	8.491878
7.249010	379.928486	8.496896
6.734793	387.223122	8.501914
7.192742	379.773213	8.506931
7.065797	376.239726	8.511949
6.858964	373.286793	8.516966
6.953212	378.030912	8.521984
7.133993	378.308701	8.527002
6.844483	366.125513	8.532019
6.714590	374.259318	8.537037
6.814916	380.094377	8.542054
7.338850	386.623604	8.547072
7.130909	396.783021	8.552090
7.037266	375.792971	8.557107
7.055350	379.226763	8.562125
7.083402	376.397970	8.567143
6.903598	368.533602	8.572160
6.786244	369.751182	8.577178
7.230346	376.532751	8.582195
7.140182	388.330482	8.587213
7.105802	383.438137	8.592231
7.265361	372.522626	8.597248
6.990380	362.694514	8.602266
6.778088	363.608237	8.607283
6.787568	361.596542	8.612301
7.105153	380.803208	8.617319
7.295223	379.810927	8.622336
7.238515	386.879248	8.627354
7.512806	370.659866	8.632371
6.806059	374.532267	8.637389
6.635173	377.680090	8.642407
6.812018	381.767495	8.647424
6.785655	388.834217	8.652442
6.991961	379.729094	8.657459
7.184914	398.614486	8.662477
6.966861	399.936206	8.667495
7.349747	399.869909	8.672512
7.083117	398.769305	8.677530
7.356112	387.277441	8.682547
7.044276	388.762176	8.687565
7.041817	389.901795	8.692583
7.036786	385.929489	8.697600
6.805852	392.286662	8.702618
7.280051	393.364221	8.707635
7.157150	398.410609	8.712653
7.061583	391.738533	8.717671
7.294467	392.090208	8.722688
7.275801	387.179621	8.727706
7.232608	386.021919	8.732723
7.205448	392.972005	8.737741
7.138876	391.562350	8.742759
7.152722	388.511722	8.747776
6.980204	387.872893	8.752794
7.334010	392.759382	8.757811
7.271710	386.009513	8.762829
7.252314	396.022626	8.767847
7.445386	391.164068	8.772864
6.835899	400.313444	8.777882
7.309887	392.838927	8.782899
6.929706	395.110687	8.787917
6.839274	392.486646	8.792935
6.750994	396.669242	8.797952
6.935360	415.631735	8.802970
7.200191	413.630517	8.807987
7.303861	418.975922	8.813005
7.526105	420.307551	8.818023
7.678453	420.397294	8.823040
7.608875	414.955041	8.828058
7.493336	418.952567	8.833075
7.364014	408.845991	8.838093
7.165342	406.879527	8.843111
7.391850	405.663788	8.848128
7.096533	409.796776	8.853146
7.227152	417.444820	8.858163
7.454832	427.775839	8.863181
7.310147	423.181630	8.868199
7.627416	417.378967	8.873216
7.512490	428.697772	8.878234
7.360698	404.340131	8.883251
7.300960	409.133631	8.888269
7.424085	428.777911	8.893287
7.833362	419.312766	8.898304
7.272501	410.911645	8.903322
7.182392	398.239607	8.908339
7.371361	408.425204	8.913357
7.211984	428.940556	8.918375
7.522433	422.460470	8.923392
7.661129	425.278933	8.928410
7.424473	420.642330	8.933427
7.212605	411.517506	8.938445
7.365985	418.944237	8.943463
7.672677	414.635908	8.948480
7.310229	419.902868	8.953498
7.469823	422.168953	8.958515
7.704184	418.711390	8.963533
7.613945	427.880408	8.968551
7.362091	403.850866	8.973568
7.213456	425.532163	8.978586
7.215728	416.569441	8.983603
7.310598	422.421148	8.988621
7.269384	427.136012	8.993639
7.397516	413.473573	8.998656
7.461416	425.278747	9.003674
7.181466	423.037842	9.008691
7.422538	420.260872	9.013709
7.052328	416.692909	9.018727
7.138941	423.031897	9.023744
7.747843	437.415154	9.028762
7.715351	430.026288	9.033779
7.578088	425.118495	9.038797
7.505619	429.304932	9.043815
7.703189	418.014213	9.048832
7.881233	421.416638	9.053850
7.827285	420.614064	9.058867
7.385015	420.345698	9.063885
7.622470	422.025235	9.068903
7.506318	408.871282	9.073920
7.632379	420.720362	9.078938
7.590308	422.446851	9.083955
7.631644	422.326772	9.088973
7.468771	412.651479	9.093991
7.723845	410.292033	9.099008
7.571864	417.940175	9.104026
7.515807	419.432173	9.109043
7.529389	412.635691	9.114061
7.558014	426.185218	9.119079
7.602304	431.909155	9.124096
7.841597	444.229653	9.129114
7.763271	442.181214	9.134131
8.011164	435.379569	9.139149
7.965233	422.602763	9.144167
7.659458	415.382953	9.149184
7.505469	411.661195	9.154202
7.593551	422.967124	9.159219
7.681788	410.033608	9.164237
7.152645	424.954922	9.169255
7.605066	433.691784	9.174272
7.732092	448.311494	9.179290
7.708975	451.877985	9.184307
8.133759	443.237210	9.189325
8.115144	448.696456	9.194343
7.841183	446.868015	9.199360
7.565874	427.010888	9.204378
7.710570	429.582262	9.209395
7.813533	440.617630	9.214413
7.553993	455.035985	9.219431
7.904872	451.676923	9.224448
7.945732	451.225563	9.229466
7.659750	449.294864	9.234483
7.823341	446.129248	9.239501
7.912798	445.499862	9.244519
7.835615	449.497697	9.249536
7.623833	446.397206	9.254554
7.782423	454.517404	9.259571
7.950367	446.065191	9.264589
7.953434	454.317053	9.269607
7.765476	446.946228	9.274624
8.056896	450.532864	9.279642
7.873428	462.174852	9.284659
8.308072	447.492383	9.289677
7.827411	457.972273	9.294695
7.915796	449.229570	9.299712
7.962228	437.634319	9.304730
7.843427	447.085529	9.309747
7.956419	447.680050	9.314765
7.975708	449.343279	9.319783
7.917382	436.568406	9.324800
7.969976	436.156233	9.329818
7.811228	437.462352	9.334835
8.128783	422.968661	9.339853
7.901659	425.976983	9.344871
8.227368	426.374075	9.349888
8.118381	423.891790	9.354906
8.020748	423.487376	9.359923
7.931003	422.478975	9.364941
7.792214	422.974091	9.369959
7.675817	415.652026	9.374976
8.220853	436.180093	9.379994
7.952888	433.473411	9.385011
8.019914	429.625503	9.390029
7.919249	436.994217	9.395047
7.981792	436.343802	9.400064
8.214182	439.393737	9.405082
8.167635	446.652991	9.410099
8.073551	429.535076	9.415117
7.696359	435.441815	9.420135
8.073190	435.736224	9.425152
8.284300	441.601282	9.430170
8.121340	445.562063	9.435187
8.132371	432.542799	9.440205
7.961192	439.906783	9.445223
8.300407	438.720719	9.450240
7.931516	430.374716	9.455258
7.991809	451.104981	9.460275
8.384897	438.972582	9.465293
8.099094	442.665435	9.470311
8.004890	428.993639	9.475328
7.981824	439.720554	9.480346
8.135895	448.759786	9.485363
8.289316	442.430527	9.490381
7.846168	445.624176	9.495399
7.990246	449.647303	9.500416
8.408942	436.302234	9.505434
8.201358	449.806739	9.510451
8.265110	445.454417	9.515469
7.997981	446.203169	9.520487
7.977624	442.110176	9.525504
8.305420	450.301690	9.530522
8.306833	455.448535	9.535539
8.201581	451.479294	9.540557
8.219334	452.155008	9.545575
8.207230	448.224821	9.550592
7.999416	446.587985	9.555610
8.134176	454.929666	9.560627
8.298378	445.417700	9.565645
8.493737	448.167329	9.570663
8.209802	447.053654	9.575680
8.211860	444.288884	9.580698
8.018512	451.116710	9.585715
8.460446	450.700338	9.590733
8.412422	444.674037	9.595751
8.325817	446.574761	9.600768
8.124900	445.675295	9.605786
8.037622	452.555929	9.610803
8.284325	448.563102	9.615821
8.395192	451.269165	9.620839
8.194108	446.002140	9.625856
8.550606	443.800366	9.630874
8.403947	448.708480	9.635891
8.382824	441.447216	9.640909
8.293462	451.853170	9.645927
8.232697	448.871026	9.650944
8.524734	453.574708	9.655962
8.076197	451.306566	9.660979
8.125244	440.465132	9.665997
7.946124	444.693529	9.671015
8.104958	447.196419	9.676032
8.341675	457.406120	9.681050
8.607187	466.866553	9.686067
8.667554	462.874516	9.691085
8.467088	454.448464	9.696103
8.398050	452.199755	9.701120
8.330518	440.956869	9.706138
8.253616	461.487739	9.711155
8.619918	461.259940	9.716173
8.569604	457.035939	9.721191
8.573473	446.801176	9.726208
8.198633	460.609603	9.731226
8.192268	457.808281	9.736243
8.424808	465.045905	9.741261
8.646096	465.727599	9.746279
8.569986	473.348098	9.751296
8.503209	465.936188	9.756314
8.527430	477.608760	9.761331
8.520776	471.326662	9.766349
8.556446	469.503353	9.771367
8.065775	475.427886	9.776384
8.495169	469.964240	9.781402
8.465880	468.990545	9.786419
8.690182	477.747392	9.791437
8.728352	476.267670	9.796455
8.499356	477.035695	9.801472
8.917978	477.090029	9.806490
8.687990	473.430658	9.811507
8.612576	473.676007	9.816525
8.533277	465.666462	9.821543
8.438867	477.193520	9.826560
8.400188	467.861652	9.831578
8.187556	483.553924	9.836595
8.177941	471.440418	9.841613
8.268549	472.354024	9.846631
8.268992	476.238718	9.851648
8.437265	482.088410	9.856666
8.457268	488.949094	9.861683
8.710957	498.550250	9.866701
8.615500	492.938460	9.871719
8.985571	503.979354	9.876736
8.984634	496.733839	9.881754
8.916138	494.895291	9.886771
8.574233	477.876118	9.891789
8.764826	481.825693	9.896807
8.884179	480.380588	9.901824
8.551056	480.843038	9.906842
8.607326	479.275274	9.911859
8.848480	487.237386	9.916877
8.665761	483.062527	9.921895
8.817398	495.046503	9.926912
8.763270	483.492224	9.931930
8.393382	489.104349	9.936947
9.107720	492.848790	9.941965
9.132727	492.904837	9.946983
9.066193	483.725647	9.952000
9.220087	481.580859	9.957018
9.007487	480.112026	9.962035
8.746369	480.162411	9.967053
8.967028	478.897091	9.972071
8.463731	485.069755	9.977088
8.668802	481.430578	9.982106
8.595592	483.679499	9.987123
8.790136	479.726394	9.992141
8.886269	472.797036	9.997159
8.240277	479.941945	10.002176
8.958683	490.293941	10.007194
8.830439	494.271385	10.012211
9.120027	496.823222	10.017229
9.105421	491.700533	10.022247
8.572509	491.500016	10.027264
9.031647	491.084103	10.032282
9.126510	490.968261	10.037299
8.750728	497.682679	10.042317
8.865948	495.742762	10.047335
8.731159	492.295687	10.052352
8.822139	492.467629	10.057370
9.045695	492.887039	10.062387
9.097212	487.362675	10.067405
9.145576	491.350315	10.072423
8.965386	499.425786	10.077440
8.990427	499.630149	10.082458
8.785767	497.667769	10.087475
8.876962	497.621928	10.092493
9.186097	490.356235	10.097511
8.864191	489.750276	10.102528
8.898165	486.191554	10.107546
9.030348	488.364113	10.112563
8.780695	493.263131	10.117581
8.686798	493.079034	10.122599
8.715306	499.382972	10.127616
8.392043	494.655779	10.132634
8.772588	502.911636	10.137651
8.992850	520.603149	10.142669
9.544327	516.291156	10.147687
9.081823	532.549637	10.152704
9.216807	520.145200	10.157722
9.261486	513.766683	10.162739
9.193218	511.259071	10.167757
8.986287	497.383980	10.172775
9.180550	510.446875	10.177792
9.044579	519.834543	10.182810
9.278403	523.010499	10.187827
9.023410	517.647758	10.192845
9.350844	515.453685	10.197863
9.067540	514.999466	10.202880
9.313227	519.025623	10.207898
9.058747	511.567365	10.212915
9.234882	531.184517	10.217933
9.364482	523.135904	10.222951
9.049954	515.895334	10.227968
8.829304	519.843080	10.232986
9.217984	521.019253	10.238003
9.209837	527.979036	10.243021
9.386081	530.924175	10.248039
9.345445	528.071407	10.253056
9.149186	522.554296	10.258074
9.361983	523.338308	10.263091
9.400617	523.067175	10.268109
9.073461	515.651859	10.273127
9.102094	530.681526	10.278144
9.521503	522.754762	10.283162
9.288333	523.747503	10.288179
8.927172	527.717266	10.293197
9.368929	521.677316	10.298215
9.130950	519.893722	10.303232
9.305118	515.666093	10.308250
9.702964	522.016312	10.313267
9.063948	523.325104	10.318285
9.691393	522.216950	10.323303
9.378771	521.634781	10.328320
9.362117	521.460671	10.333338
9.713158	520.774519	10.338355
9.472039	523.775582	10.343373
9.132004	510.281096	10.348391
9.669006	516.969268	10.353408
9.156597	523.840801	10.358426
9.372280	511.587827	10.363443
9.212605	524.576801	10.368461
9.567399	518.092889	10.373479
9.253546	526.381817	10.378496
9.264252	521.065807	10.383514
9.499252	521.035304	10.388531
9.320954	516.992286	10.393549
9.260178	518.519745	10.398567
9.125512	518.458800	10.403584
9.261421	525.572735	10.408602
9.457908	535.470050	10.413619
9.577188	543.362920	10.418637
9.813807	538.387047	10.423655
9.647996	532.234006	10.428672
9.271979	529.159233	10.433690
9.338120	528.577678	10.438707
9.694821	542.855369	10.443725
9.918129	541.636966	10.448743
9.414710	523.901446	10.453760
9.344548	533.730087	10.458778
10.268543	528.024829	10.463795
9.439316	527.675079	10.468813
9.570154	521.213632	10.473831
9.516637	524.248418	10.478848
9.389106	528.721215	10.483866
9.790182	535.238189	10.488883
9.884471	545.672227	10.493901
9.705105	533.080350	10.498919
9.781531	527.956011	10.503936
9.613979	523.362202	10.508954
9.923045	514.528087	10.513971
9.468839	523.160893	10.518989
10.085267	513.319262	10.524007
9.918303	519.514980	10.529024
9.620664	519.735188	10.534042
9.873093	514.551719	10.539059
9.555636	512.098930	10.544077
9.518517	513.537475	10.549095
9.434124	512.294703	10.554112
9.631599	512.096511	10.559130
10.121434	521.663836	10.564147
9.697494	530.026819	10.569165
9.551219	523.264809	10.574183
9.823499	535.861066	10.579200
9.602044	536.716273	10.584218
9.681127	542.946032	10.589235
9.806901	541.269543	10.594253
9.869184	548.404490	10.599271
10.197895	548.573897	10.604288
9.818889	539.721346	10.609306
9.920991	531.752776	10.614323
9.885995	531.508958	10.619341
9.785208	536.129044	10.624359
9.572904	539.409616	10.629376
9.716539	545.604015	10.634394
9.765818	545.624701	10.639411
10.059355	552.035455	10.644429
9.898674	550.365978	10.649447
9.846861	548.070377	10.654464
9.757771	533.570883	10.659482
10.272578	547.258920	10.664499
9.874540	560.657650	10.669517
10.109657	546.078947	10.674535
10.060908	547.270010	10.679552
9.854595	551.603679	10.684570
10.141952	548.150411	10.689587
10.139713	557.397225	10.694605
10.207149	550.806846	10.699623
9.882244	546.367073	10.704640
9.990023	551.620356	10.709658
10.034387	547.794908	10.714675
10.263520	553.303731	10.719693
9.808597	539.650498	10.724711
10.195432	544.093200	10.729728
9.773010	545.999214	10.734746
9.707048	547.000472	10.739763
9.656487	553.313662	10.744781
10.181925	553.430156	10.749799
10.183334	551.962499	10.754816
9.742986	551.898956	10.759834
9.884111	558.623924	10.764851
9.453265	552.805890	10.769869
9.788410	555.278015	10.774887
9.914001	551.616563	10.779904
9.805573	568.741089	10.784922
10.266630	576.886536	10.789939
9.901605	575.971750	10.794957
10.181488	579.774814	10.799975
10.535803	574.894098	10.804992
10.346121	575.453996	10.810010
10.440458	578.528741	10.815027
10.529267	562.742189	10.820045
10.250206	558.285763	10.825063
10.115854	554.816517	10.830080
9.958940	565.274146	10.835098
10.118655	559.609731	10.840115
10.257791	564.757119	10.845133
10.280793	563.055706	10.850151
10.468175	562.104862	10.855168
10.341096	562.680197	10.860186
10.431801	551.008508	10.865203
10.238906	552.651344	10.870221
10.129865	547.496099	10.875239
10.168537	553.558624	10.880256
10.048179	572.319721	10.885274
10.435579	569.223157	10.890291
10.486435	570.578496	10.895309
10.428696	579.278598	10.900327
10.551139	574.434213	10.905344
10.300369	567.461342	10.910362
10.294881	557.777089	10.915379
10.309448	561.192531	10.920397
10.141875	573.094031	10.925415
10.402608	575.022398	10.930432
9.922922	585.893528	10.935450
10.520850	572.665441	10.940467
10.519635	577.301495	10.945485
10.151119	575.033421	10.950503
10.465219	574.296250	10.955520
10.571295	572.269396	10.960538
10.609071	570.294269	10.965555
10.422479	571.513243	10.970573
10.334600	573.180652	10.975591
10.562357	569.689381	10.980608
10.615039	579.145351	10.985626
10.446975	567.668829	10.990643
10.388508	577.612426	10.995661
10.355612	577.655455	11.000679
10.303710	575.536589	11.005696
10.319404	582.467411	11.010714
10.340698	570.292191	11.015731
10.528846	571.228389	11.020749
10.292487	571.117105	11.025767
9.995299	578.769132	11.030784
10.650560	593.621776	11.035802
10.592320	594.776460	11.040819
10.787784	594.969901	11.045837
10.598727	602.399869	11.050855
10.747403	600.009733	11.055872
10.891096	605.446752	11.060890
10.775991	580.152162	11.065907
10.495464	587.602768	11.070925
10.434782	577.829323	11.075943
10.849428	579.433775	11.080960
10.593140	590.973647	11.085978
10.299410	589.356571	11.090995
10.792152	593.328257	11.096013
10.422647	601.584914	11.101031
10.886701	608.868373	11.106048
10.709836	604.307561	11.111066
10.907066	603.105863	11.116083
10.981283	602.614559	11.121101
10.529497	597.642389	11.126119
10.945301	605.264765	11.131136
10.746954	605.844956	11.136154
10.799663	603.495102	11.141171
10.830581	602.414136	11.146189
10.876851	601.188755	11.151207
10.929910	593.436124	11.156224
10.646596	599.621698	11.161242
10.479832	598.792611	11.166259
10.702282	606.129703	11.171277
10.600242	599.793078	11.176295
10.739718	596.997286	11.181312
10.696996	604.940812	11.186330
10.818610	600.046057	11.191347
10.708789	603.929120	11.196365
11.063168	606.401394	11.201383
10.785796	606.044072	11.206400
11.151132	603.272851	11.211418
10.975419	611.152011	11.216435
11.126044	601.443275	11.221453
10.825078	600.407998	11.226471
10.976939	592.075000	11.231488
10.834502	596.228258	11.236506
10.796030	591.611052	11.241523
10.974895	595.726591	11.246541
10.910424	591.179730	11.251559
10.973197	602.038460	11.256576
10.976424	600.352764	11.261594
11.141002	600.349074	11.266611
11.021764	589.088950	11.271629
10.869011	602.761703	11.276647
11.284756	591.913216	11.281664
11.077095	601.290068	11.286682
11.199469	592.737629	11.291699
11.161483	596.764069	11.296717
11.090610	593.269090	11.301735
11.025779	593.929347	11.306752
11.034355	603.130309	11.311770
11.110930	602.837451	11.316787
11.215747	594.783221	11.321805
11.123799	599.673337	11.326823
11.247885	592.827915	11.331840
11.092879	596.901092	11.336858
10.894936	605.007794	11.341875
10.893709	599.835641	11.346893
11.094845	605.995805	11.351911
10.935780	594.896552	11.356928
11.495117	615.905422	11.361946
11.057821	618.492271	11.366963
11.591900	608.600375	11.371981
11.200646	607.784371	11.376999
11.021282	594.330918	11.382016
11.341420	599.042859	11.387034
11.358791	610.527243	11.392051
11.241696	604.382323	11.397069
11.250019	614.943479	11.402087
11.297925	611.300499	11.407104
11.617526	612.171922	11.412122
11.433773	603.007880	11.417139
11.434996	591.441703	11.422157
11.066716	601.307623	11.427175
10.926460	596.397095	11.432192
11.356359	607.457081	11.437210
11.650984	620.456995	11.442227
11.455089	616.773318	11.447245
10.791133	616.877353	11.452263
11.366392	615.872044	11.457280
11.744331	619.520897	11.462298
11.300829	623.405753	11.467315
11.531945	619.610989	11.472333
11.601815	624.393708	11.477351
11.356358	626.877917	11.482368
11.914350	622.157780	11.487386
11.372558	615.555535	11.492403
11.481976	603.855634	11.497421
11.244840	609.144040	11.502439
11.128826	606.606027	11.507456
11.575156	618.998348	11.512474
11.095162	628.342145	11.517491
11.405031	626.024579	11.522509
11.298304	632.693735	11.527527
11.217958	621.219214	11.532544
11.465772	630.183891	11.537562
11.325335	626.702961	11.542579
11.229151	621.902285	11.547597
11.351349	638.492127	11.552615
11.728664	634.841711	11.557632
11.392905	636.077749	11.562650
11.445210	650.134976	11.567667
11.892465	642.087032	11.572685
11.784644	660.344484	11.577703
11.731983	644.999748	11.582720
11.777475	634.004119	11.587738
11.489535	632.771140	11.592755
11.567746	634.336792	11.597773
11.960757	645.879108	11.602791
11.848726	637.940886	11.607808
11.601834	622.137452	11.612826
11.421130	622.689633	11.617843
11.885940	624.832183	11.622861
11.877339	632.915543	11.627879
11.563562	640.402937	11.632896
11.921362	637.746501	11.637914
12.011171	638.126910	11.642931
11.865434	629.004236	11.647949
11.613445	626.386538	11.652967
12.080796	626.013518	11.657984
11.705184	618.059798	11.663002
11.610810	619.680892	11.668019
11.673200	623.612716	11.673037
11.600565	643.300527	11.678055
12.050357	651.974793	11.683072
12.335504	643.545148	11.688090
12.036062	640.953819	11.693107
12.147895	623.355331	11.698125
11.774806	615.909301	11.703143
11.440734	624.242467	11.708160
11.888802	631.449546	11.713178
11.622950	644.590942	11.718195
11.759260	640.650082	11.723213
11.855723	642.679934	11.728231
11.807127	644.205495	11.733248
12.268581	643.659829	11.738266
11.804145	653.297846	11.743283
11.988699	644.969169	11.748301
12.049346	646.190436	11.753319
11.752646	640.038930	11.758336
11.910952	633.775110	11.763354
11.740028	642.972659	11.768371
12.011761	641.711949	11.773389
12.185497	646.472087	11.778407
11.918453	639.132509	11.783424
11.991999	632.932462	11.788442
12.029923	645.407727	11.793459
11.966997	638.411708	11.798477
12.411773	639.168845	11.803495
12.055073	647.666514	11.808512
12.437626	639.098533	11.813530
11.830883	652.558434	11.818547
12.446352	642.726351	11.823565
12.229974	650.088036	11.828583
11.923745	647.822817	11.833600
12.262664	649.593775	11.838618
12.012914	650.832117	11.843635
11.968137	635.744929	11.848653
12.160253	636.440668	11.853671
11.997764	646.504743	11.858688
12.356276	644.990595	11.863706
11.929103	657.030654	11.868723
12.216564	666.197421	11.873741
12.407286	666.688251	11.878759
12.381402	672.581051	11.883776
12.658479	663.625641	11.888794
12.247818	653.752355	11.893811
12.040548	650.591161	11.898829
12.592652	660.429671	11.903847
12.479541	654.009555	11.908864
12.551651	646.193956	11.913882
12.465846	643.925759	11.918899
12.348832	651.293967	11.923917
12.349764	645.010619	11.928935
11.914249	645.100952	11.933952
12.219239	655.536755	11.938970
12.489873	669.723892	11.943987
12.338065	675.519657	11.949005
12.648116	673.056889	11.954023
12.350194	681.529585	11.959040
12.685806	671.965396	11.964058
12.608008	681.463955	11.969075
12.513366	672.509978	11.974093
12.474403	658.829350	11.979111
12.468480	663.264192	11.984128
12.788231	669.610921	11.989146
12.475655	668.069374	11.994163
12.560146	652.160343	11.999181
12.561837	659.317451	12.004199
12.846881	669.046331	12.009216
13.013222	647.141068	12.014234
12.832354	645.026621	12.019251
12.572260	642.804667	12.024269
12.875418	638.102364	12.029287
12.467260	639.889388	12.034304
12.634369	642.305802	12.039322
12.653431	646.774595	12.044339
12.389856	645.957519	12.049357
12.557982	642.920545	12.054375
12.525832	643.395803	12.059392
12.406425	642.941146	12.064410
12.564747	651.178241	12.069427
12.545441	659.086565	12.074445
13.230020	662.333932	12.079463
12.918819	656.973644	12.084480
12.884787	647.962846	12.089498
12.639221	643.823042	12.094515
12.542634	649.228295	12.099533
12.819594	639.010594	12.104551
12.475411	646.834115	12.109568
12.853753	655.024116	12.114586
13.003023	661.492227	12.119603
12.812350	661.250708	12.124621
12.876036	647.418306	12.129639
12.688399	653.926578	12.134656
13.071181	660.503269	12.139674
13.004124	665.187531	12.144691
12.735521	657.545232	12.149709
12.603684	653.744213	12.154727
12.549242	666.748360	12.159744
12.579722	668.895851	12.164762
12.866413	671.271442	12.169779
12.772290	675.382435	12.174797
12.843505	663.798933	12.179815
12.843105	675.993045	12.184832
12.815555	679.235227	12.189850
12.926640	671.252565	12.194867
12.797662	681.393460	12.199885
13.087209	666.304357	12.204903
13.233369	678.778465	12.209920
12.919192	676.378787	12.214938
13.019401	667.924459	12.219955
13.046480	680.079554	12.224973
13.256577	675.802077	12.229991
13.132363	682.824287	12.235008
12.921918	682.806772	12.240026
13.032845	683.903398	12.245043
12.859096	684.858435	12.250061
13.489815	675.519407	12.255079
13.205485	672.616435	12.260096
12.973695	675.328884	12.265114
13.256060	671.185252	12.270131
13.014819	670.146925	12.275149
13.261952	673.213525	12.280167
13.077233	680.936336	12.285184
12.964214	670.271635	12.290202
13.064986	683.557589	12.295219
13.062248	688.888188	12.300237
13.538950	686.487670	12.305255
13.595149	691.048486	12.310272
13.129674	681.174305	12.315290
13.280633	678.708061	12.320307
13.077431	681.728456	12.325325
13.460058	679.853920	12.330343
13.326239	679.376275	12.335360
13.088014	684.058958	12.340378
13.427681	691.175748	12.345395
13.131612	704.915216	12.350413
13.444403	695.477667	12.355431
13.351257	700.626775	12.360448
13.510614	702.735142	12.365466
13.734007	698.790093	12.370483
13.847476	689.888707	12.375501
13.631986	669.829432	12.380519
13.609857	671.417121	12.385536
13.488618	670.139084	12.390554
13.310455	671.587118	12.395571
13.153899	671.280293	12.400589
13.312400	670.185645	12.405607
13.551948	668.548123	12.410624
13.461800	674.324760	12.415642
13.124689	681.036342	12.420659
13.272915	696.217824	12.425677
13.848628	695.600606	12.430695
13.374214	696.552259	12.435712
13.671372	698.509647	12.440730
13.614834	704.378857	12.445747
13.589056	707.709130	12.450765
13.784513	706.854843	12.455783
13.730694	709.422647	12.460800
13.872144	699.478609	12.465818
14.040595	685.109054	12.470835
13.215402	685.632828	12.475853
13.274073	679.479277	12.480871
13.200747	699.053649	12.485888
13.358140	699.104733	12.490906
13.477671	700.944785	12.495923
13.592179	707.273191	12.500941
13.544028	697.437757	12.505959
13.653733	704.398078	12.510976
13.593320	697.502628	12.515994
13.621187	695.901426	12.521011
13.449138	699.440808	12.526029
13.610986	694.003236	12.531047
13.499634	715.903106	12.536064
13.933588	711.385418	12.541082
14.247879	728.443865	12.546099
13.812316	729.474640	12.551117
13.930340	715.523218	12.556135
13.776979	713.524374	12.561152
13.513207	722.073789	12.566170
13.989984	719.098897	12.571187
14.034144	727.650561	12.576205
13.917466	722.805732	12.581223
13.925128	719.304735	12.586240
13.838050	725.778343	12.591258
14.072188	719.149160	12.596275
14.117526	728.978746	12.601293
14.288108	725.947686	12.606311
14.053876	713.026605	12.611328
13.942872	706.877540	12.616346
14.084739	695.885708	12.621363
13.999086	706.774068	12.626381
14.154874	707.046311	12.631399
13.901286	705.271455	12.636416
13.799863	717.784382	12.641434
14.229085	717.818123	12.646451
13.969910	725.934473	12.651469
14.006406	727.803316	12.656487
13.978214	722.070461	12.661504
14.071548	733.139078	12.666522
14.081753	720.703560	12.671539
13.777857	716.115284	12.676557
13.917886	722.689008	12.681575
14.071274	725.625137	12.686592
13.880333	725.490957	12.691610
13.998917	720.034909	12.696627
14.505303	718.106264	12.701645
14.070602	709.719947	12.706663
14.107867	720.948820	12.711680
13.768967	725.252811	12.716698
14.450355	734.035998	12.721715
14.515170	742.521317	12.726733
14.331543	728.610836	12.731751
14.425302	729.640727	12.736768
14.252912	727.234607	12.741786
14.609482	723.202413	12.746803
14.026261	725.291431	12.751821
14.053217	725.511276	12.756839
14.414306	748.981346	12.761856
14.470077	750.339084	12.766874
14.550168	749.427131	12.771891
14.487213	751.463039	12.776909
14.274930	743.578347	12.781927
14.722739	742.555131	12.786944
14.566978	734.671055	12.791962
14.719062	732.308769	12.796979
14.425108	722.795857	12.801997
14.356126	721.070971	12.807015
14.241049	721.571847	12.812032
14.429235	738.893060	12.817050
14.616326	739.599058	12.822067
14.483620	754.628945	12.827085
14.836957	738.257990	12.832103
14.473715	727.563032	12.837120
14.227726	730.249311	12.842138
14.874583	733.944417	12.847155
14.800168	737.317030	12.852173
14.634449	723.918146	12.857191
14.504061	716.361463	12.862208
14.438783	734.583923	12.867226
14.732708	735.957995	12.872243
14.890788	738.486291	12.877261
14.736463	740.552292	12.882279
14.486455	744.435259	12.887296
14.469120	751.393412	12.892314
14.965293	751.943686	12.897331
14.874558	750.771318	12.902349
15.185417	741.359294	12.907367
14.897104	728.894803	12.912384
14.538373	729.907227	12.917402
14.825843	721.540299	12.922419
14.931901	742.847559	12.927437
14.700746	734.454585	12.932455
14.539136	736.133561	12.937472
14.654820	744.812883	12.942490
14.834310	745.977667	12.947507
14.997842	740.164273	12.952525
14.783346	753.588039	12.957543
14.809236	742.264054	12.962560
14.644860	756.311132	12.967578
14.391239	746.268022	12.972595
14.827055	751.066021	12.977613
14.899581	752.250720	12.982631
15.059460	739.640258	12.987648
14.703439	745.916168	12.992666
14.946479	737.726608	12.997683
14.773762	743.238492	13.002701
14.834858	756.596989	13.007719
14.914073	757.865847	13.012736
14.749308	762.647495	13.017754
15.328202	766.577320	13.022771
15.185826	775.088806	13.027789
15.284137	766.587391	13.032807
15.365048	763.182207	13.037824
14.804415	761.973009	13.042842
15.273263	764.818692	13.047859
15.353592	770.057406	13.052877
15.216561	769.375132	13.057895
15.217177	758.380146	13.062912
15.053445	759.172671	13.067930
15.448109	759.091905	13.072947
15.134098	754.214869	13.077965
15.094921	756.774074	13.082983
15.276653	755.593730	13.088000
15.125837	762.607515	13.093018
15.446674	767.003809	13.098035
15.646568	771.810376	13.103053
15.155754	754.050561	13.108071
15.588493	758.811175	13.113088
15.339598	747.003217	13.118106
14.736430	747.312323	13.123123
15.837958	761.842721	13.128141
15.590460	761.559611	13.133159
15.107691	750.362655	13.138176
15.098509	760.674174	13.143194
15.374001	776.694169	13.148211
15.513427	768.662841	13.153229
15.434467	768.943463	13.158247
15.484817	776.654731	13.163264
15.445080	773.710264	13.168282
15.452171	773.488251	13.173299
15.615327	775.693862	13.178317
15.433314	777.145664	13.183335
15.645290	774.243810	13.188352
15.574310	781.002095	13.193370
15.957484	769.925072	13.198387
15.628570	770.491012	13.203405
15.222452	759.853245	13.208423
15.412293	764.677164	13.213440
15.541337	768.649070	13.218458
15.455139	776.567926	13.223475
15.649432	771.847931	13.228493
15.488171	778.809711	13.233511
15.350291	770.850233	13.238528
14.914658	778.426206	13.243546
15.339432	768.769100	13.248563
15.364025	773.716743	13.253581
15.696033	800.006434	13.258599
15.976175	786.212595	13.263616
16.023004	796.051452	13.268634
15.696295	785.369670	13.273651
15.764401	782.146371	13.278669
15.732507	788.090643	13.283687
15.981495	790.017718	13.288704
15.868029	785.371186	13.293722
15.548488	797.110451	13.298739
15.573829	794.149473	13.303757
15.365366	792.941899	13.308775
15.772998	794.705262	13.313792
15.857073	793.521281	13.318810
16.191973	796.078686	13.323827
16.312113	794.993197	13.328845
15.852560	798.050621	13.333863
16.200744	789.639434	13.338880
15.973908	790.984650	13.343898
15.974505	792.209024	13.348915
15.810485	792.080092	13.353933
15.553991	791.195627	13.358951
16.263612	786.265497	13.363968
16.392544	782.341541	13.368986
16.071557	790.559124	13.374003
16.333906	792.692391	13.379021
16.354390	799.019784	13.384039
16.128743	791.787266	13.389056
16.475334	792.547171	13.394074
16.013222	797.302833	13.399091
16.168790	790.966803	13.404109
16.219889	799.744634	13.409127
16.191346	790.654008	13.414144
16.086619	794.384834	13.419162
15.905217	791.408911	13.424179
16.400335	784.246505	13.429197
16.244225	791.374741	13.434215
16.102332	780.114890	13.439232
16.073652	782.621961	13.444250
16.073801	781.965531	13.449267
15.923068	787.316192	13.454285
15.830352	785.191072	13.459303
16.057780	778.310452	13.464320
16.071729	793.008123	13.469338
16.267438	799.560527	13.474355
16.455362	799.887697	13.479373
16.461424	811.765306	13.484391
16.502029	807.340783	13.489408
16.438823	812.655647	13.494426
16.418441	822.501894	13.499443
16.810537	801.918080	13.504461
16.619176	800.480606	13.509479
16.544137	790.352685	13.514496
16.463953	782.822822	13.519514
16.470802	789.922370	13.524531
16.505673	784.144900	13.529549
16.657603	786.794088	13.534567
16.703116	780.674122	13.539584
16.493703	787.346802	13.544602
16.221425	788.752786	13.549619
16.503433	792.811185	13.554637
16.814810	811.217708	13.559655
16.716097	806.982272	13.564672
16.954812	801.677792	13.569690
16.801873	798.403916	13.574707
16.543918	790.396970	13.579725
16.375610	793.926317	13.584743
16.485579	795.019945	13.589760
16.660853	812.740888	13.594778
16.273878	815.525009	13.599795
16.617810	811.346453	13.604813
16.326611	814.267048	13.609831
16.562761	817.297524	13.614848
16.672339	815.538340	13.619866
16.638035	814.764229	13.624883
16.572308	809.520070	13.629901
16.681643	817.436710	13.634919
16.931296	822.951869	13.639936
17.322457	816.635723	13.644954
17.172574	817.719572	13.649971
17.402022	795.049996	13.654989
17.244631	807.944143	13.660007
17.129502	800.852097	13.665024
16.831890	799.715296	13.670042
17.133920	800.059302	13.675059
17.072327	802.789285	13.680077
16.869226	809.230608	13.685095
16.858906	806.218410	13.690112
17.122928	806.502099	13.695130
17.163607	807.701259	13.700147
17.612260	809.489754	13.705165
17.165488	816.041842	13.710183
17.210259	819.313745	13.715200
17.404070	806.798906	13.720218
16.987361	813.488295	13.725235
16.938507	805.271854	13.730253
17.200812	811.125857	13.735271
17.397684	802.107205	13.740288
17.417268	812.584663	13.745306
17.202572	806.101511	13.750323
17.046739	807.120020	13.755341
16.970033	809.729294	13.760359
17.440140	808.358596	13.765376
17.197219	806.395864	13.770394
17.204443	805.905583	13.775411
17.299331	810.236304	13.780429
17.062216	813.757500	13.785447
17.060767	809.459488	13.790464
17.302196	805.779835	13.795482
16.920918	813.410423	13.800499
16.878837	802.545177	13.805517
17.116368	821.405097	13.810535
17.356800	839.380947	13.815552
17.688513	828.444497	13.820570
17.491607	838.308942	13.825587
17.468006	831.511816	13.830605
17.922300	833.135327	13.835623
17.160979	821.704255	13.840640
17.613544	818.663712	13.845658
17.368833	832.461503	13.850675
17.820897	829.566205	13.855693
17.470587	826.547313	13.860711
17.509885	829.438218	13.865728
17.597702	825.899395	13.870746
17.900293	840.296258	13.875763
17.886788	817.797264	13.880781
17.532844	808.154849	13.885799
17.521724	808.664686	13.890816
17.435144	813.285773	13.895834
17.599820	827.843091	13.900851
17.560581	832.021260	13.905869
17.840132	832.876879	13.910887
17.558072	830.551044	13.915904
17.914480	825.786699	13.920922
17.973369	827.320682	13.925939
17.715584	819.610345	13.930957
17.706801	829.338012	13.935975
17.948268	832.850501	13.940992
17.935796	821.961669	13.946010
17.603670	828.517890	13.951027
17.675780	833.312936	13.956045
17.275532	829.730661	13.961063
17.418156	834.754504	13.966080
17.690790	829.356337	13.971098
17.960965	832.936912	13.976115
17.881833	823.301924	13.981133
17.788695	828.643573	13.986151
17.665924	837.688509	13.991168
18.364479	855.759857	13.996186
17.939153	855.318412	14.001203
18.156315	849.102100	14.006221
18.442010	849.638017	14.011239
18.454143	840.613577	14.016256
18.428024	827.312664	14.021274
17.764682	820.158181	14.026291
17.987062	822.950972	14.031309
18.361395	825.931396	14.036327
17.909796	824.825031	14.041344
18.118753	817.922044	14.046362
17.956193	827.904180	14.051379
18.293745	839.483714	14.056397
18.035204	838.198776	14.061415
18.193629	845.170453	14.066432
18.251130	841.147222	14.071450
18.386346	854.361634	14.076467
18.550101	840.204132	14.081485
18.377803	847.009876	14.086503
18.368855	851.296914	14.091520
18.488325	850.700682	14.096538
18.476701	843.456700	14.101555
18.499032	825.575387	14.106573
18.450057	827.214633	14.111591
18.367395	830.197232	14.116608
18.710328	818.832991	14.121626
17.864977	824.159952	14.126643
18.345309	835.679242	14.131661
18.676857	838.966177	14.136679
18.438504	843.251286	14.141696
18.747636	846.279800	14.146714
18.657184	840.692363	14.151731
18.619167	830.031594	14.156749
18.908512	821.560182	14.161767
18.806175	823.930475	14.166784
18.749064	815.128338	14.171802
18.193342	828.441519	14.176819
18.398084	829.327794	14.181837
18.340913	829.835379	14.186855
17.983043	838.727801	14.191872
18.625219	841.767249	14.196890
18.375124	851.371789	14.201907
18.372221	849.339888	14.206925
18.495247	843.125705	14.211943
18.710297	846.049037	14.216960
18.640986	850.323442	14.221978
18.358080	862.508295	14.226995
18.747392	858.398357	14.232013
19.109426	859.269457	14.237031
18.756081	859.962304	14.242048
18.658504	851.744008	14.247066
18.914572	857.469614	14.252083
18.974678	865.330873	14.257101
19.117220	852.783008	14.262119
18.868552	851.411314	14.267136
18.843838	848.123650	14.272154
19.019372	871.313682	14.277171
19.045840	866.313840	14.282189
19.224127	860.917823	14.287207
18.911491	858.622022	14.292224
19.205446	855.035116	14.297242
18.997364	852.842856	14.302259
18.799738	857.733821	14.307277
19.369543	865.546778	14.312295
19.022632	856.790026	14.317312
19.188309	858.449292	14.322330
19.502019	856.598160	14.327347
18.964331	856.704502	14.332365
19.343746	845.893112	14.337383
18.762790	840.429864	14.342400
19.358058	850.315367	14.347418
19.561167	856.178660	14.352435
19.318856	852.136128	14.357453
19.205047	843.683691	14.362471
19.194465	855.298846	14.367488
19.297632	846.279075	14.372506
19.337674	860.291051	14.377523
19.634681	854.021202	14.382541
19.386771	847.928252	14.387559
19.438086	857.772752	14.392576
19.445922	853.280768	14.397594
19.248094	850.667174	14.402611
19.635478	848.280630	14.407629
19.506948	853.457417	14.412647
19.218554	861.228108	14.417664
19.632341	852.623574	14.422682
19.452451	854.523178	14.427699
19.095886	858.451268	14.432717
19.555506	846.863597	14.437735
19.501346	858.659153	14.442752
19.511234	854.337262	14.447770
19.590635	854.170191	14.452787
19.552292	859.121407	14.457805
19.633720	851.907025	14.462823
19.666003	860.280731	14.467840
19.708640	856.922552	14.472858
19.874905	861.040127	14.477875
19.544054	859.482491	14.482893
19.956930	854.409486	14.487911
19.521082	854.275806	14.492928
19.505529	855.745715	14.497946
19.463751	847.477652	14.502963
19.365179	853.429237	14.507981
19.687974	851.999565	14.512999
19.399655	854.919715	14.518016
19.538158	854.724448	14.523034
19.692387	872.227839	14.528051
20.040990	875.815070	14.533069
20.171288	868.308997	14.538087
19.834407	879.239981	14.543104
20.247731	873.485238	14.548122
20.097191	872.031895	14.553139
19.765905	874.977716	14.558157
19.921295	873.277621	14.563175
20.044673	879.611012	14.568192
20.044110	875.890364	14.573210
20.501780	877.825779	14.578227
20.305951	869.928985	14.583245
20.350471	849.128173	14.588263
19.811433	849.578712	14.593280
19.709267	851.175801	14.598298
20.299336	850.521614	14.603315
20.265337	866.018974	14.608333
20.644979	867.793041	14.613351
20.086907	861.003904	14.618368
20.310885	852.059876	14.623386
20.169159	850.715608	14.628403
19.766721	851.930550	14.633421
20.493889	861.729120	14.638439
20.155910	874.212947	14.643456
20.249545	874.640100	14.648474
20.404836	877.841048	14.653491
20.065053	890.299922	14.658509
20.585965	873.883653	14.663527
20.323114	877.153271	14.668544
20.523247	877.431192	14.673562
20.095305	879.432780	14.678579
20.483223	875.768032	14.683597
20.519203	876.320984	14.688615
20.152600	879.591079	14.693632
20.375715	873.869294	14.698650
20.132157	873.386746	14.703667
20.151841	875.971460	14.708685
20.419932	875.607565	14.713703
20.460458	882.881756	14.718720
20.348659	889.428724	14.723738
20.673311	890.485566	14.728755
20.803609	893.879783	14.733773
20.830129	888.990381	14.738791
20.843029	885.270778	14.743808
20.885861	889.215192	14.748826
21.026849	879.564621	14.753843
20.404531	880.738274	14.758861
20.971544	883.887338	14.763879
20.677987	878.047685	14.768896
20.713619	885.707658	14.773914
20.968874	890.287830	14.778931
20.759132	890.983425	14.783949
20.985780	887.811007	14.788967
21.175740	887.708665	14.793984
20.563977	884.440389	14.799002
20.960391	890.497471	14.804019
20.736254	897.759486	14.809037
21.087501	887.728823	14.814055
21.149854	888.533268	14.819072
20.907752	887.488750	14.824090
20.970264	886.907753	14.829107
20.834398	888.374424	14.834125
20.864153	892.188342	14.839143
21.088232	892.232135	14.844160
21.057050	892.476871	14.849178
21.170090	885.295392	14.854195
21.028637	890.029239	14.859213
20.987157	885.866870	14.864231
21.294406	894.380549	14.869248
21.159493	895.436811	14.874266
21.526353	884.526378	14.879283
21.256140	882.429056	14.884301
21.274176	889.807761	14.889319
21.488078	891.399514	14.894336
21.183629	894.947056	14.899354
21.276835	886.831397	14.904371
21.395028	891.783343	14.909389
21.033292	893.436884	14.914407
21.015352	891.347373	14.919424
20.849180	890.171037	14.924442
21.191201	894.317888	14.929459
21.093482	899.414120	14.934477
20.806926	899.446399	14.939495
21.290205	912.139254	14.944512
21.391293	918.605540	14.949530
21.197247	910.774722	14.954547
21.172250	917.456426	14.959565
21.359676	920.712308	14.964583
21.389381	910.735167	14.969600
21.217513	920.093954	14.974618
21.767392	917.341110	14.979635
21.603272	928.087262	14.984653
22.139313	921.596898	14.989671
21.789701	920.370404	14.994688
21.509640	915.529030	14.999706
21.682445	908.707413	15.004723
21.783106	913.034098	15.009741
21.377680	916.158801	15.014759
21.659636	915.634940	15.019776
21.969535	930.816538	15.024794
22.078850	939.421213	15.029811
22.168991	924.615604	15.034829
22.055886	917.529506	15.039847
22.141443	903.554621	15.044864
21.725276	909.780051	15.049882
21.922968	901.054715	15.054899
21.760570	900.875035	15.059917
22.147003	903.607421	15.064935
22.208598	895.884880	15.069952
21.706147	903.502933	15.074970
22.044843	902.335857	15.079987
22.135394	902.735091	15.085005
21.978086	910.327472	15.090023
22.485951	905.056531	15.095040
22.053182	907.727919	15.100058
22.047603	900.789085	15.105075
21.964800	906.185943	15.110093
21.982832	905.665564	15.115111
22.672402	918.657466	15.120128
22.215208	918.675455	15.125146
22.230552	900.451174	15.130163
22.052948	908.460150	15.135181
22.408493	919.541449	15.140199
22.695702	899.538854	15.145216
22.334498	892.431677	15.150234
22.388448	895.298207	15.155251
22.591133	909.710779	15.160269
22.325001	898.807995	15.165287
22.444097	904.520363	15.170304
22.352382	893.975267	15.175322
22.741997	899.960834	15.180339
22.698946	905.566061	15.185357
21.951414	902.208599	15.190375
22.703712	897.237039	15.195392
22.327116	901.038886	15.200410
22.379371	900.670937	15.205427
22.680672	900.781527	15.210445
22.214200	899.267227	15.215463
22.565601	917.784356	15.220480
22.837263	932.081996	15.225498
22.674660	934.234524	15.230515
22.154718	932.381455	15.235533
22.390537	930.533051	15.240551
22.565096	925.118664	15.245568
22.672721	926.846994	15.250586
22.436500	930.917192	15.255603
21.908613	932.988095	15.260621
22.667985	927.974392	15.265639
22.770025	931.256277	15.270656
23.179086	944.939099	15.275674
23.218200	935.806240	15.280691
22.922447	932.213883	15.285709
22.518379	931.333597	15.290727
23.335495	930.085248	15.295744
22.891671	926.440351	15.300762
23.064632	923.367859	15.305779
22.702461	930.799839	15.310797
22.846232	926.270759	15.315815
23.249958	932.033216	15.320832
22.787967	942.283240	15.325850
22.998554	946.447540	15.330867
23.243662	941.410265	15.335885
23.225375	958.177053	15.340903
23.576008	950.024188	15.345920
23.352310	947.212658	15.350938
23.116159	933.830963	15.355955
23.115149	916.899972	15.360973
22.834589	927.800070	15.365991
23.301201	934.944406	15.371008
23.348331	947.390036	15.376026
23.350056	950.419395	15.381043
23.328029	934.918128	15.386061
23.217821	944.049513	15.391079
23.211848	944.523833	15.396096
23.182566	938.188310	15.401114
23.568339	930.919900	15.406131
23.980754	938.325197	15.411149
23.643879	946.024624	15.416167
24.066078	942.411297	15.421184
23.713582	937.969436	15.426202
23.354531	916.935125	15.431219
23.611541	916.516160	15.436237
23.354249	923.404678	15.441255
23.306397	933.482511	15.446272
23.619296	940.745609	15.451290
23.688665	942.694533	15.456307
23.707660	943.026083	15.461325
23.303214	954.011880	15.466343
23.606955	949.886926	15.471360
23.849216	942.208644	15.476378
23.600256	946.539622	15.481395
23.644275	942.341752	15.486413
23.464513	951.244194	15.491431
23.669533	944.960323	15.496448
23.772387	956.873356	15.501466
23.427487	949.634211	15.506483
23.704871	944.156370	15.511501
23.825329	947.574230	15.516519
24.300622	954.884475	15.521536
23.989385	945.285787	15.526554
23.811855	943.312795	15.531571
23.732115	946.642099	15.536589
24.028774	961.169379	15.541607
24.178997	966.605486	15.546624
23.966584	964.944075	15.551642
24.275425	965.580513	15.556659
24.259623	965.409422	15.561677
24.068371	960.961227	15.566695
23.707404	959.143208	15.571712
24.150551	957.230759	15.576730
24.164053	968.548720	15.581747
24.410103	964.833596	15.586765
24.347012	963.287647	15.591783
24.428184	955.735586	15.596800
24.433588	967.007476	15.601818
24.662498	961.458328	15.606835
24.343498	948.149564	15.611853
24.043998	948.628847	15.616871
24.083750	950.828569	15.621888
24.495122	959.253381	15.626906
24.309855	961.213800	15.631923
24.430723	963.170436	15.636941
24.281634	961.802067	15.641959
24.419142	953.130317	15.646976
24.661491	963.872767	15.651994
24.370459	963.867877	15.657011
25.262730	955.081026	15.662029
24.898426	951.811836	15.667047
24.360972	958.898900	15.672064
24.066184	951.875969	15.677082
24.352797	951.023168	15.682099
24.484189	948.386381	15.687117
24.300394	956.592012	15.692135
24.592401	957.559297	15.697152
24.951664	955.445393	15.702170
24.837818	958.385561	15.707187
24.828045	955.133407	15.712205
24.597954	957.198680	15.717223
24.922003	954.774708	15.722240
24.925985	956.067991	15.727258
24.515524	962.623911	15.732275
25.480165	974.720674	15.737293
24.728846	979.130369	15.742311
24.975651	980.959976	15.747328
25.123351	979.901717	15.752346
24.884478	988.630398	15.757363
25.054515	994.615686	15.762381
25.094027	988.960501	15.767399
25.099715	989.193149	15.772416
25.098882	979.173417	15.777434
25.354505	986.874705	15.782451
25.341777	976.711668	15.787469
25.230315	981.721713	15.792487
25.076748	972.637959	15.797504
24.939927	975.581730	15.802522
25.263029	980.823494	15.807539
25.493116	979.761794	15.812557
25.425156	978.121931	15.817575
25.392536	978.035527	15.822592
25.140928	982.101836	15.827610
24.874016	979.161370	15.832627
25.407813	977.177910	15.837645
25.373923	981.342653	15.842663
25.119459	975.304336	15.847680
25.222493	974.890559	15.852698
25.038412	977.469343	15.857715
25.506619	976.304062	15.862733
25.197676	985.406644	15.867751
25.347116	996.043748	15.872768
25.762747	997.667021	15.877786
25.505137	1005.827434	15.882803
25.973737	999.391791	15.887821
25.779234	1008.706833	15.892839
25.812032	981.861060	15.897856
25.544354	983.657665	15.902874
25.700019	996.376664	15.907891
25.874526	995.560361	15.912909
25.857348	999.637281	15.917927
25.912085	992.382842	15.922944
25.971669	985.481103	15.927962
25.761770	980.281573	15.932979
25.596392	983.065715	15.937997
25.685980	999.500053	15.943015
26.167477	992.488024	15.948032
26.024634	1003.628527	15.953050
26.047119	1008.734360	15.958067
26.068371	1006.474590	15.963085
25.976968	1004.920450	15.968103
25.790840	1008.812400	15.973120
26.342241	1002.827695	15.978138
25.926506	1009.024689	15.983155
26.452271	996.183146	15.988173
26.144331	1002.423210	15.993191
26.238944	998.763365	15.998208
26.121694	993.978513	16.003226
25.996932	1003.364678	16.008243
26.099063	988.942152	16.013261
26.060364	998.876575	16.018279
26.068219	991.784119	16.023296
26.312805	992.926096	16.028314
25.984359	998.718082	16.033331
26.148258	993.472605	16.038349
26.273095	988.776059	16.043367
25.777367	1000.451542	16.048384
26.206375	1009.943454	16.053402
26.139875	1018.206477	16.058419
26.576090	1010.292645	16.063437
26.525319	1012.743247	16.068455
26.571241	1017.349939	16.073472
26.845806	1013.030722	16.078490
26.523158	1009.789709	16.083507
26.599524	1017.834683	16.088525
26.811433	1012.739472	16.093543
26.514488	1016.863386	16.098560
26.508715	1007.746990	16.103578
26.646074	1010.063973	16.108595
26.794193	1013.086185	16.113613
26.997616	1011.927672	16.118631
26.965497	1024.515164	16.123648
27.019332	1014.792966	16.128666
26.814667	1016.649131	16.133683
26.807880	1018.322810	16.138701
26.975579	1022.790500	16.143719
26.950946	1014.636441	16.148736
26.940670	1006.192952	16.153754
26.367341	1012.783875	16.158771
26.572623	1016.882750	16.163789
26.915788	1029.234717	16.168807
27.087881	1045.214348	16.173824
27.062237	1038.228110	16.178842
27.033433	1053.803715	16.183859
27.011307	1041.492962	16.188877
27.435148	1033.969232	16.193895
27.337910	1047.715680	16.198912
27.304386	1042.169754	16.203930
27.532442	1042.822008	16.208947
27.702673	1036.243748	16.213965
27.464234	1020.375518	16.218983
27.264733	1024.083370	16.224000
27.214436	1010.625159	16.229018
27.043840	1027.475838	16.234035
27.366709	1034.686918	16.239053
27.404399	1033.317681	16.244071
27.692570	1043.462852	16.249088
27.685057	1039.964170	16.254106
27.315109	1048.615585	16.259123
27.471726	1045.327877	16.264141
27.555549	1045.084370	16.269159
27.363697	1038.837401	16.274176
27.295941	1038.071677	16.279194
27.405682	1044.334678	16.284211
27.794105	1037.551814	16.289229
27.994775	1027.797135	16.294247
27.858425	1041.975749	16.299264
27.875952	1030.712853	16.304282
27.757778	1039.741391	16.309299
27.661735	1035.281416	16.314317
28.228212	1032.708994	16.319335
27.659377	1045.904468	16.324352
27.917050	1034.768048	16.329370
27.626769	1036.031702	16.334387
27.570637	1033.174969	16.339405
27.679556	1037.235297	16.344423
27.594568	1034.815440	16.349440
27.859041	1032.091516	16.354458
27.822394	1034.287439	16.359475
28.021667	1046.346376	16.364493
28.343033	1055.713163	16.369511
27.958800	1057.455452	16.374528
28.306893	1049.912024	16.379546
27.996509	1060.390832	16.384563
27.998080	1056.890723	16.389581
28.398017	1058.712126	16.394599
28.369596	1058.347346	16.399616
28.671260	1052.408065	16.404634
28.612183	1048.387274	16.409651
28.126718	1042.088474	16.414669
28.739453	1051.078241	16.419687
28.020062	1034.133459	16.424704
28.392113	1038.086287	16.429722
28.790333	1038.853894	16.434739
28.517932	1045.814255	16.439757
28.334847	1047.676510	16.444775
28.299341	1050.156284	16.449792
28.810819	1047.523049	16.454810
28.673814	1050.829786	16.459827
28.447156	1058.840204	16.464845
28.717209	1052.864849	16.469863
28.252621	1055.247748	16.474880
28.460189	1043.024084	16.479898
28.605261	1047.867719	16.484915
28.775475	1055.216337	16.489933
29.231439	1054.406427	16.494951
28.926922	1050.799640	16.499968
28.529494	1044.947803	16.504986
28.585757	1059.863132	16.510003
29.231621	1058.802557	16.515021
29.337941	1051.394841	16.520039
28.506694	1051.070639	16.525056
28.594023	1049.160281	16.530074
28.915813	1055.970743	16.535091
28.574907	1059.104297	16.540109
28.742987	1052.554771	16.545127
28.463521	1057.831006	16.550144
28.965358	1067.428305	16.555162
29.047244	1083.882864	16.560179
29.251435	1071.789101	16.565197
29.223451	1068.628144	16.570215
29.385720	1082.463351	16.575232
29.280354	1084.468070	16.580250
29.541532	1075.940990	16.585267
29.603743	1084.729845	16.590285
29.652533	1073.130656	16.595303
29.394628	1054.516674	16.600320
28.791480	1055.122432	16.605338
29.135446	1064.810739	16.610355
29.477579	1069.405748	16.615373
29.349558	1073.335946	16.620391
29.392162	1080.732972	16.625408
29.184664	1077.991469	16.630426
29.471903	1082.099609	16.635443
29.306799	1079.626025	16.640461
29.410752	1076.523292	16.645479
29.719117	1069.367942	16.650496
29.644413	1074.160809	16.655514
29.205070	1075.201661	16.660531
29.468247	1081.058773	16.665549
29.850094	1098.334214	16.670567
29.859620	1103.287466	16.675584
30.046687	1097.448179	16.680602
29.987400	1101.752631	16.685619
30.057061	1094.360110	16.690637
29.806654	1078.913435	16.695655
29.701991	1085.282628	16.700672
29.728986	1095.260461	16.705690
30.211420	1096.011720	16.710707
29.668842	1103.484662	16.715725
29.790789	1093.246808	16.720743
29.896818	1106.295562	16.725760
29.714391	1102.350890	16.730778
30.270181	1099.792757	16.735795
30.221102	1100.993377	16.740813
30.014617	1095.796434	16.745831
29.999370	1095.584228	16.750848
29.901985	1091.670417	16.755866
30.333230	1092.432852	16.760883
29.951659	1101.452196	16.765901
30.553062	1105.975034	16.770919
30.462643	1104.584837	16.775936
30.228025	1108.635889	16.780954
30.275179	1106.293151	16.785971
30.330781	1118.683923	16.790989
30.583759	1117.583914	16.796007
30.292513	1126.753225	16.801024
30.233116	1118.030193	16.806042
30.297965	1123.037900	16.811059
30.383205	1123.169721	16.816077
31.058860	1112.977648	16.821095
30.684099	1112.007552	16.826112
30.764587	1112.452550	16.831130
30.559660	1105.633234	16.836147
30.437324	1114.649839	16.841165
30.251145	1110.727844	16.846183
30.527185	1110.735094	16.851200
30.712020	1102.522928	16.856218
31.056626	1113.075873	16.861235
30.715543	1121.899531	16.866253
31.030719	1117.368794	16.871271
31.112269	1122.528522	16.876288
30.662996	1112.648406	16.881306
31.080804	1118.702215	16.886323
31.323946	1129.798101	16.891341
31.272013	1124.737884	16.896359
31.200694	1109.938484	16.901376
30.912312	1110.384470	16.906394
31.100113	1103.721379	16.911411
31.033356	1109.289359	16.916429
31.113943	1118.725463	16.921447
31.156394	1129.849637	16.926464
31.323487	1130.621903	16.931482
31.664638	1127.570362	16.936499
31.330351	1129.424755	16.941517
31.460255	1124.859927	16.946535
31.570294	1124.975239	16.951552
31.466247	1120.065204	16.956570
31.382517	1098.242752	16.961587
31.352591	1102.170211	16.966605
31.406533	1120.658416	16.971623
31.621481	1120.823564	16.976640
31.147549	1129.696443	16.981658
31.745907	1137.754363	16.986675
31.706808	1129.252214	16.991693
31.391526	1124.940178	16.996711
31.475726	1120.527683	17.001728
31.329390	1129.456535	17.006746
31.663190	1126.788008	17.011763
31.550104	1124.353606	17.016781
31.839324	1123.437271	17.021799
31.865410	1120.488746	17.026816
31.662997	1123.386011	17.031834
31.711311	1120.434003	17.036851
31.572171	1126.508803	17.041869
32.206084	1132.276287	17.046887
31.997604	1142.392028	17.051904
31.900628	1146.418367	17.056922
31.815560	1143.515656	17.061939
31.963523	1151.773542	17.066957
32.084778	1145.057744	17.071975
32.180628	1143.846648	17.076992
31.960527	1149.634331	17.082010
32.463328	1141.508033	17.087027
32.053066	1137.801027	17.092045
31.896686	1143.521918	17.097063
31.966929	1146.079814	17.102080
32.098012	1142.149131	17.107098
32.051902	1138.265147	17.112115
31.992141	1154.631507	17.117133
32.137017	1156.881057	17.122151
32.348241	1162.358161	17.127168
32.109919	1166.334064	17.132186
32.620664	1163.691459	17.137203
32.419608	1163.659848	17.142221
32.459570	1163.732489	17.147239
32.859974	1167.204363	17.152256
32.106295	1161.313629	17.157274
32.460801	1156.773564	17.162291
32.721198	1169.053387	17.167309
32.808451	1167.512268	17.172327
33.047386	1175.484504	17.177344
32.863129	1180.752169	17.182362
32.890041	1160.335617	17.187379
32.841942	1165.985900	17.192397
32.695384	1162.534226	17.197415
33.096269	1171.882304	17.202432
33.207944	1176.207328	17.207450
33.278633	1168.470621	17.212467
32.972204	1164.185592	17.217485
33.352593	1169.005014	17.222503
33.230418	1167.222144	17.227520
33.039295	1169.123541	17.232538
33.185406	1169.545636	17.237555
32.906344	1163.100841	17.242573
33.290971	1168.206786	17.247591
32.906833	1165.679142	17.252608
32.908900	1172.085294	17.257626
33.536433	1181.858628	17.262643
33.407549	1186.227656	17.267661
33.152764	1187.649864	17.272679
33.271555	1183.298208	17.277696
33.206695	1186.568419	17.282714
33.636121	1182.862391	17.287731
33.544112	1182.510728	17.292749
33.395089	1184.841044	17.297767
33.571457	1183.096607	17.302784
33.451955	1188.789643	17.307802
33.862610	1188.646410	17.312819
33.838498	1190.348068	17.317837
33.799596	1192.351853	17.322855
33.810639	1181.446495	17.327872
33.584517	1186.663915	17.332890
33.568410	1184.324767	17.337907
33.738600	1178.478629	17.342925
33.625722	1178.619400	17.347943
34.183312	1171.626939	17.352960
33.911556	1181.556951	17.357978
33.940080	1177.364610	17.362995
34.059930	1174.530776	17.368013
33.878044	1182.319633	17.373031
33.911885	1175.188318	17.378048
33.807054	1183.596282	17.383066
33.833431	1176.005375	17.388083
34.100502	1184.345603	17.393101
34.068361	1183.725776	17.398119
34.269347	1191.303166	17.403136
34.141441	1202.476167	17.408154
34.421594	1187.432280	17.413171
34.647923	1197.539890	17.418189
34.393031	1197.463063	17.423207
35.079613	1189.595135	17.428224
34.479041	1182.446447	17.433242
34.173706	1173.619906	17.438259
34.438921	1177.977679	17.443277
34.369034	1185.742678	17.448295
34.931420	1193.954588	17.453312
34.626522	1190.022773	17.458330
34.460833	1182.512450	17.463347
34.499574	1187.593695	17.468365
34.567757	1197.905970	17.473383
34.858643	1190.889014	17.478400
34.668467	1193.030113	17.483418
34.344897	1186.475516	17.488435
34.703068	1192.352496	17.493453
34.678620	1201.779854	17.498471
34.381279	1193.419124	17.503488
34.488689	1203.071984	17.508506
34.894186	1203.204123	17.513523
35.180984	1211.629638	17.518541
34.938768	1228.943021	17.523559
35.001612	1218.730135	17.528576
34.828494	1210.690772	17.533594
35.421796	1219.693137	17.538611
35.314733	1224.869823	17.543629
35.199892	1223.805346	17.548647
35.486562	1219.023421	17.553664
35.209657	1220.013583	17.558682
35.423396	1198.668282	17.563699
35.668398	1201.138843	17.568717
35.123930	1195.691859	17.573735
35.358575	1191.735471	17.578752
35.147780	1198.351713	17.583770
35.255438	1208.790357	17.588787
35.724727	1216.840133	17.593805
35.309451	1222.292334	17.598823
35.383538	1216.309758	17.603840
35.378421	1217.636045	17.608858
35.415151	1210.923999	17.613875
35.558633	1221.524300	17.618893
35.268400	1221.172134	17.623911
35.466800	1214.049735	17.628928
35.533520	1218.953031	17.633946
35.721716	1219.841919	17.638963
35.908580	1226.174954	17.643981
35.612340	1242.537419	17.648999
36.034816	1237.996152	17.654016
35.891677	1242.660927	17.659034
36.109670	1234.181565	17.664051
36.354169	1235.736996	17.669069
35.920331	1238.560083	17.674087
36.300011	1233.268104	17.679104
35.921944	1236.325458	17.684122
35.973420	1237.949002	17.689139
36.232514	1236.601867	17.694157
36.254143	1238.293207	17.699175
36.464560	1232.999345	17.704192
36.295661	1239.384969	17.709210
36.285306	1236.868181	17.714227
36.464547	1238.358096	17.719245
36.350807	1244.706676	17.724263
36.560768	1232.201633	17.729280
36.338514	1225.403921	17.734298
36.034564	1233.035194	17.739315
36.400294	1237.263621	17.744333
36.272879	1240.187026	17.749351
36.473935	1235.876118	17.754368
36.181437	1233.425628	17.759386
36.516058	1246.656427	17.764403
36.947739	1251.707685	17.769421
36.823180	1260.671061	17.774439
36.836806	1254.432848	17.779456
36.672202	1256.718277	17.784474
36.747941	1256.621206	17.789491
37.102655	1255.530496	17.794509
36.855603	1259.854938	17.799527
37.238555	1260.634416	17.804544
37.122661	1265.733600	17.809562
37.301882	1257.859925	17.814579
37.461141	1254.221459	17.819597
37.382531	1238.608868	17.824615
37.104563	1233.811261	17.829632
36.946206	1235.142624	17.834650
37.128653	1235.136135	17.839667
37.284249	1231.343608	17.844685
37.203979	1252.178881	17.849703
37.361870	1253.198755	17.854720
37.155215	1262.004575	17.859738
37.054296	1260.874795	17.864755
37.375567	1256.784897	17.869773
37.298388	1259.040848	17.874791
37.182083	1254.703917	17.879808
37.540812	1249.216394	17.884826
37.392277	1258.473869	17.889843
37.698097	1252.372920	17.894861
37.414610	1263.100105	17.899879
37.629255	1254.693844	17.904896
37.875274	1261.977020	17.909914
37.405841	1253.914633	17.914931
37.732591	1250.407721	17.919949
37.696852	1264.248846	17.924967
37.920477	1277.421317	17.929984
37.879472	1275.079745	17.935002
38.012493	1280.531267	17.940019
37.816393	1284.254420	17.945037
37.763575	1281.176214	17.950055
38.099672	1276.074095	17.955072
38.279363	1271.965348	17.960090
38.029514	1284.874325	17.965107
38.239705	1280.460985	17.970125
38.225932	1278.582222	17.975143
37.985569	1287.907751	17.980160
38.053648	1273.638659	17.985178
38.051018	1280.036118	17.990195
38.094283	1273.291464	17.995213
37.942894	1290.391854	18.000231
38.108362	1276.258985	18.005248
38.161280	1282.054430	18.010266
38.350042	1294.213014	18.015283
38.704280	1289.590904	18.020301
38.209390	1298.883731	18.025319
38.746651	1296.457867	18.030336
38.547323	1297.019297	18.035354
38.404486	1295.305926	18.040371
38.604051	1298.253852	18.045389
38.675262	1292.041319	18.050407
38.557133	1296.052070	18.055424
38.828703	1295.192143	18.060442
38.830140	1294.952074	18.065459
38.897913	1290.485304	18.070477
38.936394	1298.653110	18.075495
39.161613	1303.938709	18.080512
39.411935	1290.650945	18.085530
39.073313	1294.522667	18.090547
39.067497	1291.904171	18.095565
39.241371	1298.362347	18.100583
38.697970	1301.660218	18.105600
38.945326	1287.037967	18.110618
38.951836	1306.572093	18.115635
39.098974	1307.300154	18.120653
39.172145	1314.051836	18.125671
39.030032	1320.505878	18.130688
39.277120	1314.114297	18.135706
39.040486	1312.131588	18.140723
39.684117	1302.998504	18.145741
39.369513	1306.494066	18.150759
39.400524	1306.735374	18.155776
39.141732	1311.879052	18.160794
39.254194	1328.316421	18.165811
39.807168	1326.743347	18.170829
39.897028	1336.878730	18.175847
39.859928	1334.419769	18.180864
40.068732	1332.998452	18.185882
39.634677	1340.085244	18.190899
40.002707	1332.462833	18.195917
40.499677	1329.841298	18.200935
40.308350	1333.418540	18.205952
40.136594	1307.683653	18.210970
39.932221	1306.361788	18.215987
39.661288	1309.714805	18.221005
39.809059	1324.139472	18.226023
39.790911	1334.216033	18.231040
39.924176	1316.528295	18.236058
40.096042	1325.079172	18.241075
40.205117	1322.003998	18.246093
40.346738	1323.297835	18.251111
40.069119	1332.966907	18.256128
40.423588	1323.828623	18.261146
40.010595	1331.748432	18.266163
40.278348	1322.071449	18.271181
40.481253	1318.129475	18.276199
40.477048	1321.263970	18.281216
40.655534	1332.180757	18.286234
40.371447	1328.709572	18.291251
40.472149	1331.480482	18.296269
40.737817	1334.736805	18.301287
40.729847	1348.393756	18.306304
41.104334	1348.593874	18.311322
40.726806	1342.644143	18.316339
40.672397	1334.623995	18.321357
40.922924	1344.226105	18.326375
40.759722	1341.988880	18.331392
41.213793	1331.130787	18.336410
40.773957	1351.056798	18.341427
40.891094	1352.802615	18.346445
41.241527	1350.671114	18.351463
41.474754	1352.130488	18.356480
41.214474	1341.437962	18.361498
41.188009	1340.577390	18.366515
40.947236	1344.089795	18.371533
41.392177	1350.423466	18.376551
41.063048	1348.127028	18.381568
41.744880	1340.616399	18.386586
41.006541	1350.354510	18.391603
41.110898	1345.815719	18.396621
41.165182	1339.902479	18.401639
40.813771	1340.068001	18.406656
41.410493	1344.831485	18.411674
41.492601	1364.700981	18.416691
41.148477	1365.891039	18.421709
41.714938	1365.139547	18.426727
41.602054	1375.754859	18.431744
42.062550	1367.224816	18.436762
41.696937	1369.715328	18.441779
41.754303	1370.889820	18.446797
41.590230	1363.770503	18.451815
41.527843	1366.147231	18.456832
41.835252	1358.591113	18.461850
41.981906	1363.926911	18.466867
42.043925	1369.900846	18.471885
42.082816	1370.197727	18.476903
41.881133	1379.949606	18.481920
42.309633	1386.683513	18.486938
42.409118	1397.874661	18.491955
42.275511	1391.160831	18.496973
42.452099	1393.051978	18.501991
42.282380	1390.168802	18.507008
42.634354	1384.104760	18.512026
42.349844	1384.038884	18.517043
42.433955	1390.287086	18.522061
42.446660	1378.409319	18.527079
42.539718	1382.364909	18.532096
42.451794	1383.025657	18.537114
42.499913	1377.047096	18.542131
42.060731	1386.684704	18.547149
42.487777	1387.990632	18.552167
42.481796	1395.534262	18.557184
42.505825	1385.800752	18.562202
42.582024	1393.337817	18.567219
42.557183	1405.258534	18.572237
42.715515	1398.139184	18.577255
42.789288	1401.766427	18.582272
42.733072	1403.555189	18.587290
42.734845	1402.002195	18.592307
42.901353	1410.803272	18.597325
42.697254	1402.301597	18.602343
43.196127	1408.071394	18.607360
43.207358	1399.570699	18.612378
43.076923	1396.340525	18.617395
43.404171	1406.176811	18.622413
42.968686	1400.292947	18.627431
43.206892	1416.376167	18.632448
43.809378	1423.521505	18.637466
43.525681	1425.033473	18.642483
43.365444	1414.511429	18.647501
43.511342	1417.941174	18.652519
43.415478	1424.649950	18.657536
43.823735	1422.506225	18.662554
43.812329	1422.088278	18.667571
44.146583	1426.037647	18.672589
43.965788	1410.251560	18.677607
43.422216	1404.674977	18.682624
43.603134	1403.251712	18.687642
44.028065	1423.970160	18.692659
44.059999	1420.443131	18.697677
44.369157	1411.532818	18.702695
44.204442	1421.935363	18.707712
43.983017	1399.995254	18.712730
44.016272	1399.380953	18.717747
43.910084	1413.485706	18.722765
44.476462	1411.847406	18.727783
44.177026	1426.455838	18.732800
44.066494	1418.898901	18.737818
44.113400	1422.400964	18.742835
44.085600	1419.934223	18.747853
44.363092	1414.942237	18.752871
44.009528	1426.879756	18.757888
44.232886	1419.229479	18.762906
44.087949	1420.426203	18.767923
43.590142	1427.617696	18.772941
44.379969	1426.626069	18.777959
44.698500	1436.801424	18.782976
44.769735	1435.247012	18.787994
44.906999	1441.414317	18.793011
44.433385	1434.838953	18.798029
44.615712	1434.873511	18.803047
44.773784	1444.092511	18.808064
44.452490	1444.281717	18.813082
44.982219	1442.421929	18.818099
44.710952	1463.953278	18.823117
45.095580	1462.264551	18.828135
45.199557	1467.468205	18.833152
45.147359	1463.998533	18.838170
45.192702	1462.719587	18.843187
45.303535	1459.552591	18.848205
45.821085	1462.819969	18.853223
45.302880	1472.754039	18.858240
45.249940	1464.572650	18.863258
45.229149	1457.705413	18.868275
45.092788	1469.103978	18.873293
45.326827	1461.253185	18.878311
45.242109	1456.141205	18.883328
45.434125	1462.233665	18.888346
45.486636	1450.680987	18.893363
45.242699	1461.364222	18.898381
45.627346	1461.991959	18.903399
45.694744	1480.295382	18.908416
46.001534	1477.410120	18.913434
45.799361	1466.973515	18.918451
45.823640	1485.596139	18.923469
45.902086	1473.253551	18.928487
45.898513	1478.543490	18.933504
45.730929	1476.515227	18.938522
46.085565	1477.535849	18.943539
45.905873	1478.775893	18.948557
46.300678	1472.127572	18.953575
46.159901	1484.877586	18.958592
46.117007	1486.096197	18.963610
45.773486	1480.507182	18.968627
45.977427	1483.482857	18.973645
46.339776	1475.062819	18.978663
46.230406	1476.295001	18.983680
46.716648	1476.780583	18.988698
46.657632	1472.627135	18.993715
46.642216	1475.315270	18.998733
46.557084	1476.158629	19.003751
46.661279	1478.360943	19.008768
46.889086	1471.224367	19.013786
46.649079	1466.562767	19.018803
46.597203	1469.502777	19.023821
46.634183	1475.546945	19.028839
46.669036	1490.974096	19.033856
46.855100	1502.132808	19.038874
47.103348	1500.279244	19.043891
46.894995	1504.979552	19.048909
46.995042	1499.876482	19.053927
46.767936	1507.031906	19.058944
46.804417	1500.821586	19.063962
47.380101	1496.619186	19.068979
47.031982	1499.580368	19.073997
47.248496	1496.434679	19.079015
47.361211	1491.216012	19.084032
47.376285	1500.463758	19.089050
47.323841	1490.218285	19.094067
47.634880	1501.496278	19.099085
47.554856	1498.961965	19.104103
47.120582	1505.171501	19.109120
47.171988	1514.849083	19.114138
47.797424	1523.568845	19.119155
47.913367	1529.206165	19.124173
47.782553	1522.883187	19.129191
47.674553	1525.005138	19.134208
47.701425	1529.037406	19.139226
47.665256	1512.957156	19.144243
48.067072	1534.828123	19.149261
47.994918	1523.607371	19.154279
47.816753	1525.210115	19.159296
48.184665	1531.959882	19.164314
47.969756	1524.122595	19.169331
48.027736	1523.861039	19.174349
47.892494	1530.452942	19.179367
48.159367	1529.824126	19.184384
48.192023	1539.813944	19.189402
48.268533	1540.748751	19.194419
48.467599	1531.038234	19.199437
48.633234	1545.655951	19.204455
48.812099	1550.058905	19.209472
48.473495	1551.939265	19.214490
48.554223	1535.676570	19.219507
48.905288	1537.010194	19.224525
48.520714	1536.571811	19.229543
48.467825	1534.484545	19.234560
48.264270	1539.843706	19.239578
48.409212	1532.369777	19.244595
48.372252	1533.688453	19.249613
48.496587	1540.283874	19.254631
48.804083	1555.658895	19.259648
48.912897	1567.435697	19.264666
48.954718	1562.515310	19.269683
49.071588	1565.018621	19.274701
48.943169	1560.743477	19.279719
48.904892	1555.292816	19.284736
49.007206	1568.740142	19.289754
48.865517	1564.287185	19.294771
49.099765	1568.851889	19.299789
49.226586	1582.017661	19.304807
49.566789	1582.636585	19.309824
49.540368	1586.601473	19.314842
49.644377	1588.753334	19.319859
49.738451	1590.682678	19.324877
49.331143	1588.903412	19.329895
49.790363	1589.374296	19.334912
49.810007	1587.771146	19.339930
49.914815	1578.280509	19.344947
49.860373	1586.134785	19.349965
49.726182	1583.997131	19.354983
50.017677	1575.594460	19.360000
49.517493	1576.821605	19.365018
49.821573	1579.582780	19.370035
49.992614	1585.956294	19.375053
49.935851	1583.064856	19.380071
50.117682	1580.896625	19.385088
50.079440	1577.939167	19.390106
49.955166	1571.356358	19.395123
50.107749	1589.425629	19.400141
50.232563	1596.775272	19.405159
50.733792	1593.171526	19.410176
50.636386	1597.400015	19.415194
50.647225	1599.727430	19.420211
50.974067	1599.288042	19.425229
50.686355	1602.823632	19.430247
51.065289	1607.204722	19.435264
50.589650	1595.030918	19.440282
50.705386	1592.538508	19.445299
51.267674	1609.593661	19.450317
50.762277	1600.722509	19.455335
51.040281	1596.219568	19.460352
50.584219	1601.533099	19.465370
50.743119	1598.633117	19.470387
50.843924	1600.993776	19.475405
50.804354	1595.350790	19.480423
51.113806	1598.057475	19.485440
50.744928	1599.134654	19.490458
51.184256	1597.077565	19.495475
51.174506	1609.807138	19.500493
51.201987	1616.682863	19.505511
51.361744	1617.626723	19.510528
51.120078	1628.028819	19.515546
51.401120	1629.849975	19.520563
51.509409	1622.801496	19.525581
51.449315	1618.449358	19.530599
51.600546	1617.851281	19.535616
51.421629	1627.148422	19.540634
51.401861	1614.388756	19.545651
51.603041	1624.607852	19.550669
51.373240	1645.050421	19.555687
51.774847	1651.750772	19.560704
51.743936	1656.360198	19.565722
52.344971	1642.521736	19.570739
52.430849	1645.029915	19.575757
52.230651	1649.653239	19.580775
52.262001	1650.929661	19.585792
52.342238	1643.131290	19.590810
52.431193	1637.988891	19.595827
52.537806	1642.845025	19.600845
52.477907	1645.581183	19.605863
52.783971	1639.682048	19.610880
52.656751	1645.613136	19.615898
52.534371	1646.566486	19.620915
52.775367	1645.553535	19.625933
52.431921	1649.836365	19.630951
52.485125	1643.310934	19.635968
52.657323	1644.811454	19.640986
52.591905	1639.778453	19.646003
53.029897	1634.843315	19.651021
52.834138	1641.274318	19.656039
52.692371	1638.254170	19.661056
52.856494	1653.979962	19.666074
52.617745	1633.538216	19.671091
52.871962	1633.653035	19.676109
52.870873	1636.755538	19.681127
53.018732	1659.360762	19.686144
53.046267	1663.777987	19.691162
53.147497	1665.933449	19.696179
53.236212	1661.273946	19.701197
53.071836	1661.577432	19.706215
53.060557	1666.035454	19.711232
53.257960	1665.218691	19.716250
53.224666	1660.272174	19.721267
53.466785	1672.189114	19.726285
53.675503	1686.787573	19.731303
53.895360	1681.031326	19.736320
53.709808	1683.932352	19.741338
53.958325	1683.909200	19.746355
54.101508	1682.311934	19.751373
54.033499	1688.230604	19.756391
54.186876	1679.925268	19.761408
54.112746	1682.909827	19.766426
54.123831	1683.252098	19.771443
54.392814	1674.786632	19.776461
54.142964	1689.580023	19.781479
54.388576	1669.718794	19.786496
54.214016	1682.909767	19.791514
54.241851	1680.314346	19.796531
54.406163	1683.697074	19.801549
54.421586	1686.689695	19.806567
54.347197	1682.926794	19.811584
54.315539	1677.913740	19.816602
54.061267	1678.253403	19.821619
54.262310	1685.332349	19.826637
54.578006	1697.793232	19.831655
54.563055	1698.480429	19.836672
54.462702	1697.697692	19.841690
54.646017	1704.539568	19.846707
54.505960	1701.089927	19.851725
54.326215	1709.901218	19.856743
54.886037	1722.932976	19.861760
55.153177	1727.773451	19.866778
55.290528	1732.927770	19.871795
55.453815	1732.375141	19.876813
55.613252	1724.135110	19.881831
55.361062	1724.155692	19.886848
55.140047	1730.436039	19.891866
55.368913	1727.613443	19.896883
55.748491	1714.052635	19.901901
55.530792	1726.098461	19.906919
55.408751	1731.287108	19.911936
55.318375	1723.588021	19.916954
55.288907	1723.813563	19.921971
55.428056	1721.522607	19.926989
55.662591	1738.140055	19.932007
56.162478	1738.958043	19.937024
56.014888	1754.631769	19.942042
56.005857	1752.884766	19.947059
56.323999	1743.572069	19.952077
55.948417	1739.868970	19.957095
55.879699	1744.427535	19.962112
55.848902	1741.538315	19.967130
55.868149	1739.449190	19.972147
56.193899	1740.142974	19.977165
55.904521	1746.781198	19.982183
56.094560	1744.665313	19.987200
56.448371	1742.460650	19.992218
56.131401	1741.869650	19.997235
56.461273	1750.137184	20.002253
56.317662	1762.982519	20.007271
56.413987	1768.111716	20.012288
56.692448	1756.513972	20.017306
56.539490	1759.839119	20.022323
56.770028	1763.078934	20.027341
56.804485	1760.706539	20.032359
56.649569	1762.605481	20.037376
56.892489	1765.448856	20.042394
56.806698	1773.371245	20.047411
56.898478	1769.424491	20.052429
57.096139	1773.654132	20.057447
57.326692	1781.567989	20.062464
57.159266	1778.775914	20.067482
57.325904	1783.707895	20.072499
57.671170	1779.573091	20.077517
57.434047	1781.516475	20.082535
57.427167	1775.038282	20.087552
57.286792	1772.860546	20.092570
57.090652	1780.686611	20.097587
57.469144	1782.129574	20.102605
57.485525	1797.742932	20.107623
57.345450	1798.598069	20.112640
57.803417	1796.698994	20.117658
57.919613	1803.980641	20.122675
57.855602	1798.268832	20.127693
58.138364	1802.011745	20.132711
58.061890	1797.712625	20.137728
58.412668	1798.374086	20.142746
58.205533	1798.475977	20.147763
58.281345	1789.273812	20.152781
58.226050	1806.097689	20.157799
57.963355	1797.838550	20.162816
58.304883	1799.044294	20.167834
58.491259	1812.810014	20.172851
58.750730	1818.036748	20.177869
58.750577	1817.342455	20.182887
58.957015	1816.634730	20.187904
58.611081	1814.542848	20.192922
58.745687	1813.221487	20.197939
59.075363	1806.712644	20.202957
58.752706	1822.189782	20.207975
58.851207	1816.556654	20.212992
59.246871	1813.802591	20.218010
59.165685	1818.284228	20.223027
59.214946	1809.177737	20.228045
59.127242	1817.504415	20.233063
58.854052	1809.925457	20.238080
59.037893	1819.999049	20.243098
58.627330	1816.781128	20.248115
59.460059	1831.853176	20.253133
59.383156	1831.189843	20.258151
59.050336	1839.630679	20.263168
59.631027	1844.084367	20.268186
59.191439	1845.475615	20.273203
59.482406	1838.584636	20.278221
59.368285	1831.561454	20.283239
59.156188	1842.227302	20.288256
59.496920	1854.435047	20.293274
59.706186	1866.455100	20.298291
60.114886	1863.493847	20.303309
59.930816	1858.716075	20.308327
59.978425	1857.828092	20.313344
60.374821	1859.599638	20.318362
60.403899	1864.565818	20.323379
60.427505	1852.263121	20.328397
60.412612	1856.254666	20.333415
60.080577	1859.917178	20.338432
60.211802	1860.442615	20.343450
60.543408	1868.889826	20.348467
60.341846	1861.047143	20.353485
60.534420	1872.681625	20.358503
60.688139	1882.725256	20.363520
60.677672	1875.086172	20.368538
60.611174	1887.168381	20.373555
60.964643	1879.036744	20.378573
60.939051	1875.783745	20.383591
60.740095	1874.057018	20.388608
61.389997	1870.698187	20.393626
61.110302	1871.635167	20.398643
61.295853	1874.231910	20.403661
61.303459	1871.699595	20.408679
61.195111	1888.396153	20.413696
61.374931	1872.957128	20.418714
61.006548	1875.142009	20.423731
61.362659	1881.391951	20.428749
61.716584	1888.169295	20.433767
61.347660	1904.474318	20.438784
61.507406	1898.616959	20.443802
61.679786	1902.547613	20.448819
61.822527	1896.503558	20.453837
61.975952	1901.579662	20.458855
61.856290	1902.428451	20.463872
61.941162	1894.774421	20.468890
62.127327	1897.213271	20.473907
61.896982	1904.183154	20.478925
61.967813	1897.250897	20.483943
61.978360	1901.020701	20.488960
62.014185	1889.716524	20.493978
61.698673	1919.533603	20.498995
61.964998	1921.536989	20.504013
62.282999	1923.428130	20.509031
62.041454	1928.430414	20.514048
62.313143	1916.073026	20.519066
62.185560	1937.465657	20.524083
62.227699	1947.731948	20.529101
62.761309	1954.026695	20.534119
62.841543	1952.016360	20.539136
62.955061	1946.705911	20.544154
62.730262	1948.994545	20.549171
63.160088	1946.759011	20.554189
63.161775	1945.591020	20.559207
63.101588	1945.906591	20.564224
63.143991	1934.484582	20.569242
62.832073	1946.851453	20.574259
63.130461	1954.413908	20.579277
63.276939	1960.561013	20.584295
63.432751	1963.859913	20.589312
63.481665	1966.989356	20.594330
63.371319	1966.091399	20.599347
63.431045	1966.192508	20.604365
63.523181	1964.745237	20.609383
63.223866	1964.517562	20.614400
63.236794	1968.867717	20.619418
63.744832	1979.073655	20.624435
63.875232	1989.376638	20.629453
64.089830	1986.682479	20.634471
63.871978	1987.044845	20.639488
64.163819	1988.892750	20.644506
64.283677	1986.080881	20.649523
64.185095	1992.219051	20.654541
64.444980	1989.580917	20.659559
64.178802	1988.697906	20.664576
64.167198	1983.971980	20.669594
64.330928	1985.328679	20.674611
64.541933	1988.110813	20.679629
65.087542	1990.726907	20.684647
64.494325	1991.122834	20.689664
64.817918	1985.899389	20.694682
64.820789	1995.401786	20.699699
65.136850	2004.817246	20.704717
65.110924	1998.597595	20.709735
64.798639	2010.194492	20.714752
65.007234	1998.345588	20.719770
64.883554	2007.227141	20.724787
64.989375	2017.742290	20.729805
65.051415	2009.798277	20.734823
64.945835	2008.984784	20.739840
65.311115	2000.545107	20.744858
65.401869	2003.787930	20.749875
65.302256	2020.966117	20.754893
65.668181	2019.147717	20.759911
65.827524	2028.852851	20.764928
65.761037	2028.727563	20.769946
65.728684	2030.872438	20.774963
65.655080	2018.903619	20.779981
65.586706	2019.558170	20.784999
65.586838	2028.982113	20.790016
65.569399	2019.680822	20.795034
65.660073	2033.985611	20.800051
65.725129	2046.299799	20.805069
66.279973	2047.339585	20.810087
66.307586	2058.444568	20.815104
66.255197	2047.864226	20.820122
66.359687	2056.981476	20.825139
66.474032	2049.808795	20.830157
66.660579	2036.956539	20.835175
66.434218	2051.339417	20.840192
66.872936	2047.366650	20.845210
66.506858	2056.462944	20.850227
66.575954	2078.014291	20.855245
66.755489	2065.292512	20.860263
66.783664	2081.046290	20.865280
66.894320	2082.960466	20.870298
67.126196	2078.420448	20.875315
66.967763	2081.563461	20.880333
67.334122	2072.684888	20.885351
67.492689	2079.028972	20.890368
67.411748	2075.961347	20.895386
67.520402	2067.987913	20.900403
67.320032	2075.060471	20.905421
67.475605	2068.581968	20.910439
67.486356	2075.577265	20.915456
67.777402	2090.784898	20.920474
67.909401	2097.467693	20.925491
68.243653	2099.794999	20.930509
68.226507	2088.199172	20.935527
67.929927	2079.279283	20.940544
68.132316	2083.268396	20.945562
68.013130	2080.806414	20.950579
67.853661	2090.937103	20.955597
68.162605	2082.105394	20.960615
68.554956	2085.588181	20.965632
68.292081	2088.987418	20.970650
68.521289	2089.573256	20.975667
68.606115	2085.008935	20.980685
68.786965	2086.119943	20.985703
68.405555	2087.824012	20.990720
68.349262	2087.615069	20.995738
68.519710	2090.933792	21.000755
68.444921	2092.662411	21.005773
68.676985	2074.923729	21.010791
68.357592	2086.619627	21.015808
68.447365	2107.858476	21.020826
68.921641	2107.380199	21.025843
68.674276	2110.754918	21.030861
69.226369	2109.617455	21.035879
69.259212	2111.546981	21.040896
69.123960	2109.794470	21.045914
69.040094	2128.179064	21.050931
68.697171	2138.196499	21.055949
69.293106	2137.443518	21.060967
69.625833	2134.917037	21.065984
69.612149	2140.549611	21.071002
69.716910	2140.577387	21.076019
69.539617	2148.946659	21.081037
69.866018	2149.024925	21.086055
69.647558	2159.354258	21.091072
69.865075	2159.812531	21.096090
69.900744	2150.105188	21.101107
69.980568	2156.827741	21.106125
70.180975	2146.829479	21.111143
69.982585	2160.412732	21.116160
70.087723	2171.657131	21.121178
70.481022	2176.029800	21.126195
70.743739	2182.707927	21.131213
70.869299	2172.134348	21.136231
70.718225	2180.004023	21.141248
70.932400	2178.597580	21.146266
71.269244	2185.586014	21.151283
70.983496	2172.305842	21.156301
71.280517	2171.085252	21.161319
71.199378	2179.739301	21.166336
71.113928	2177.562378	21.171354
71.138897	2174.077322	21.176371
71.084649	2180.038182	21.181389
71.158783	2173.133707	21.186407
71.043439	2172.388014	21.191424
70.799778	2170.699823	21.196442
71.096657	2179.809085	21.201459
71.229293	2198.475438	21.206477
71.534869	2201.094454	21.211495
71.650316	2195.998242	21.216512
71.533720	2202.032000	21.221530
71.661025	2190.962632	21.226547
71.546925	2209.531942	21.231565
72.098538	2221.343949	21.236583
71.876548	2226.756699	21.241600
72.249712	2225.448430	21.246618
72.163452	2225.105313	21.251635
72.208774	2223.453899	21.256653
72.045382	2221.970896	21.261671
72.300429	2217.701793	21.266688
72.153127	2219.094616	21.271706
72.852774	2235.601782	21.276723
72.456546	2247.688552	21.281741
72.682196	2247.489087	21.286759
72.711957	2245.537124	21.291776
72.675243	2250.630494	21.296794
72.996383	2240.935185	21.301811
72.809778	2244.622330	21.306829
72.881997	2246.037571	21.311847
73.366939	2245.412440	21.316864
72.966515	2246.863859	21.321882
73.153193	2237.823992	21.326899
73.259864	2244.296197	21.331917
73.100391	2251.646465	21.336935
73.421382	2263.201116	21.341952
72.927706	2276.941184	21.346970
73.409580	2263.427058	21.351987
73.112730	2276.407231	21.357005
73.364413	2277.586056	21.362023
73.844775	2288.260453	21.367040
73.745406	2290.621005	21.372058
73.908333	2300.013271	21.377075
74.022031	2297.776728	21.382093
74.095612	2288.344262	21.387111
74.318754	2292.951922	21.392128
73.988732	2291.043698	21.397146
74.060277	2288.037361	21.402163
74.236734	2299.226481	21.407181
74.408108	2318.660133	21.412199
74.694373	2307.111311	21.417216
74.782845	2308.085313	21.422234
74.854621	2300.341636	21.427251
74.770262	2318.212058	21.432269
74.911161	2320.998916	21.437287
74.976352	2308.897695	21.442304
75.088373	2306.595135	21.447322
75.159709	2309.563320	21.452339
75.431528	2314.295914	21.457357
75.096157	2317.738114	21.462375
75.170728	2308.037214	21.467392
75.110377	2312.948095	21.472410
75.423751	2312.166788	21.477427
75.212720	2335.201513	21.482445
75.291662	2323.599948	21.487463
75.677306	2331.761175	21.492480
75.367187	2341.773583	21.497498
76.000603	2325.313117	21.502515
75.903741	2343.605284	21.507533
75.359061	2340.701797	21.512551
75.750893	2342.259493	21.517568
75.844853	2364.110274	21.522586
75.972067	2363.702147	21.527603
76.141235	2361.043455	21.532621
76.382504	2365.313746	21.537639
76.215103	2364.361585	21.542656
76.164220	2376.627887	21.547674
76.540826	2377.859737	21.552691
76.465703	2385.165282	21.557709
76.815999	2391.561497	21.562727
76.679044	2377.383618	21.567744
76.624418	2383.669684	21.572762
76.538319	2383.642150	21.577779
76.805932	2392.942317	21.582797
76.789472	2402.416396	21.587815
77.038380	2404.665586	21.592832
76.871822	2408.437995	21.597850
76.839876	2408.910110	21.602867
77.210559	2423.272334	21.607885
77.400883	2427.042487	21.612903
77.778768	2427.002224	21.617920
77.626218	2430.974434	21.622938
77.564348	2428.020538	21.627955
78.106703	2427.386406	21.632973
77.975038	2428.492744	21.637991
78.114127	2430.629743	21.643008
77.989852	2431.280443	21.648026
78.082962	2428.968206	21.653043
78.014500	2433.211293	21.658061
78.113273	2425.558016	21.663079
78.218957	2429.521329	21.668096
78.325727	2448.412922	21.673114
78.230405	2439.253018	21.678131
78.519982	2445.889162	21.683149
78.549533	2447.137518	21.688167
78.816158	2437.043505	21.693184
78.475096	2443.090419	21.698202
78.869911	2435.488596	21.703219
78.759511	2447.720085	21.708237
78.806371	2446.200966	21.713255
78.930576	2453.525808	21.718272
78.946641	2467.637483	21.723290
78.808350	2470.237709	21.728307
79.085640	2461.473898	21.733325
78.914149	2466.771499	21.738343
79.141444	2474.414747	21.743360
79.350637	2476.578642	21.748378
79.487927	2487.875012	21.753395
79.902447	2487.254594	21.758413
79.596315	2489.278299	21.763431
79.862579	2473.496979	21.768448
79.746060	2483.428635	21.773466
79.935913	2498.620907	21.778483
80.374067	2500.543784	21.783501
80.170061	2502.463118	21.788519
80.517692	2508.215942	21.793536
80.552798	2513.320226	21.798554
80.658312	2506.723163	21.803571
80.842934	2502.237786	21.808589
80.716663	2509.655548	21.813607
80.487517	2506.914057	21.818624
80.896013	2506.376643	21.823642
80.780072	2506.599961	21.828659
81.174023	2499.452730	21.833677
81.041243	2509.626814	21.838695
81.053607	2502.069103	21.843712
80.903961	2501.723286	21.848730
80.911876	2507.766044	21.853747
81.001127	2508.257047	21.858765
81.065929	2530.071568	21.863783
81.160104	2531.189872	21.868800
81.314170	2527.747644	21.873818
81.417794	2533.696511	21.878835
81.583726	2550.988251	21.883853
81.553097	2552.672121	21.888871
81.575290	2556.452862	21.893888
81.701105	2560.132153	21.898906
81.674612	2556.964387	21.903923
81.685994	2565.051800	21.908941
81.985340	2580.804561	21.913959
82.248637	2588.278098	21.918976
82.202563	2587.291136	21.923994
82.102711	2589.752798	21.929011
82.503321	2591.312299	21.934029
82.393343	2601.198808	21.939047
82.658958	2598.906865	21.944064
82.854384	2606.807655	21.949082
82.690681	2609.134141	21.954099
82.964483	2599.234595	21.959117
82.833683	2599.674861	21.964135
83.029783	2605.372553	21.969152
83.349558	2613.405359	21.974170
83.265983	2598.489871	21.979187
83.414388	2618.773294	21.984205
83.076982	2627.966379	21.989223
83.645815	2626.141380	21.994240
83.373414	2632.518463	21.999258
83.821800	2633.230945	22.004275
83.897498	2614.443139	22.009293
83.860397	2629.071410	22.014311
83.974044	2614.977171	22.019328
83.709496	2627.879944	22.024346
84.110529	2630.736560	22.029363
84.516632	2620.248167	22.034381
84.050372	2625.702463	22.039399
84.221076	2619.344482	22.044416
84.648581	2630.399791	22.049434
84.281637	2623.630527	22.054451
84.824378	2631.669438	22.059469
84.840765	2646.207284	22.064487
84.394483	2641.416729	22.069504
84.410895	2649.064686	22.074522
84.499480	2646.402797	22.079539
84.988113	2637.599476	22.084557
84.737635	2648.013009	22.089575
84.880571	2668.546681	22.094592
85.157975	2671.331145	22.099610
85.191876	2668.797754	22.104627
85.220036	2674.540717	22.109645
84.855940	2675.756077	22.114663
85.341691	2683.835502	22.119680
85.193525	2700.832574	22.124698
85.698077	2698.888236	22.129715
85.917187	2699.617705	22.134733
85.828190	2707.086519	22.139751
85.844400	2697.609173	22.144768
86.162226	2708.482876	22.149786
86.061569	2718.320647	22.154803
86.341947	2724.566972	22.159821
86.093355	2721.370850	22.164839
86.369663	2724.853008	22.169856
86.483465	2714.299890	22.174874
86.291984	2709.753451	22.179891
86.981759	2717.251754	22.184909
86.505209	2726.810711	22.189927
86.774446	2727.548109	22.194944
87.343418	2742.356104	22.199962
86.981356	2749.113392	22.204979
87.051185	2741.423486	22.209997
86.836985	2745.973535	22.215015
87.081461	2748.135091	22.220032
87.126893	2746.268992	22.225050
87.342165	2755.959445	22.230067
87.365906	2767.548368	22.235085
87.333011	2771.839617	22.240103
87.562334	2767.965781	22.245120
87.565300	2770.651229	22.250138
87.553129	2786.298324	22.255155
88.049815	2788.126845	22.260173
87.864715	2796.043150	22.265191
88.147469	2799.464344	22.270208
88.044121	2795.658404	22.275226
87.607186	2796.957776	22.280243
88.188900	2802.105907	22.285261
88.358618	2811.194384	22.290279
88.282106	2807.160147	22.295296
88.695060	2802.443238	22.300314
88.601567	2815.694931	22.305331
88.587110	2817.527790	22.310349
88.843003	2832.132415	22.315367
89.078282	2831.527445	22.320384
89.303558	2835.323769	22.325402
89.126261	2839.388319	22.330419
89.305876	2833.603294	22.335437
89.238013	2835.144683	22.340455
89.055742	2827.352209	22.345472
89.494115	2826.955290	22.350490
89.321045	2850.142534	22.355507
89.833460	2850.879712	22.360525
89.748783	2862.747646	22.365543
90.019295	2862.654771	22.370560
90.023789	2856.941361	22.375578
89.827011	2855.927496	22.380595
90.081224	2856.152794	22.385613
90.026014	2862.101406	22.390631
89.974456	2859.464598	22.395648
90.084940	2875.648044	22.400666
90.022099	2881.039211	22.405683
90.444338	2879.565399	22.410701
90.636808	2880.138083	22.415719
90.802524	2895.741622	22.420736
90.954944	2899.669311	22.425754
90.990933	2897.665802	22.430771
91.215135	2903.400217	22.435789
91.135122	2906.152341	22.440807
91.302059	2907.555952	22.445824
91.261807	2901.546543	22.450842
91.220843	2908.291457	22.455859
91.288418	2896.987987	22.460877
91.136717	2912.281463	22.465895
91.333294	2923.029107	22.470912
91.381871	2927.702154	22.475930
91.635033	2923.619397	22.480947
91.703317	2926.506101	22.485965
91.970038	2941.910795	22.490983
91.811904	2951.896572	22.496000
92.303739	2940.362482	22.501018
92.543973	2951.661952	22.506035
92.497700	2946.363619	22.511053
92.372603	2953.128043	22.516071
92.161122	2955.648275	22.521088
92.636414	2964.802578	22.526106
92.676522	2972.304930	22.531123
92.719219	2965.865884	22.536141
92.991695	2982.377542	22.541159
92.896540	2972.867000	22.546176
93.386229	2982.091649	22.551194
93.372765	2994.551350	22.556211
93.422805	3000.148958	22.561229
93.605745	3000.975637	22.566247
93.651781	3000.043658	22.571264
93.687579	2995.429977	22.576282
93.823667	2999.104592	22.581299
93.944132	2986.350388	22.586317
93.784186	2987.559033	22.591335
93.810727	3000.176593	22.596352
94.037422	2992.379942	22.601370
93.887751	3014.727334	22.606387
94.292515	3019.571849	22.611405
94.452338	3023.877151	22.616423
94.368814	3026.806592	22.621440
94.309985	3026.096196	22.626458
94.061659	3029.401798	22.631475
94.691393	3035.394654	22.636493
94.884269	3045.641112	22.641511
94.563450	3054.115350	22.646528
95.308074	3053.951351	22.651546
95.111168	3060.878565	22.656563
94.955960	3053.678280	22.661581
94.810937	3052.189173	22.666599
95.138947	3061.537037	22.671616
95.074930	3067.354534	22.676634
95.139292	3071.245557	22.681651
95.337874	3069.226025	22.686669
95.481771	3077.807372	22.691687
95.254074	3097.361200	22.696704
95.816513	3097.279400	22.701722
95.935922	3099.681530	22.706739
96.061688	3094.927478	22.711757
96.156377	3092.466567	22.716775
96.331572	3100.452805	22.721792
96.262288	3105.257988	22.726810
96.475331	3115.150983	22.731827
96.387368	3126.101140	22.736845
96.580939	3112.514771	22.741863
96.602211	3113.865469	22.746880
96.947952	3114.695054	22.751898
97.221384	3129.947358	22.756915
96.778930	3137.111915	22.761933
96.975511	3134.821252	22.766951
97.151948	3143.744719	22.771968
97.294758	3139.111079	22.776986
97.404706	3137.559925	22.782003
97.292307	3133.887893	22.787021
97.797115	3145.392221	22.792039
97.891240	3168.219230	22.797056
98.093619	3162.888189	22.802074
98.075836	3162.392294	22.807091
98.509839	3164.148614	22.812109
98.421849	3161.040877	22.817127
98.105718	3167.181967	22.822144
98.240998	3159.652067	22.827162
98.228404	3169.514161	22.832179
98.031355	3161.758577	22.837197
98.266877	3170.524456	22.842215
98.612803	3181.681262	22.847232
98.454522	3168.434039	22.852250
98.806632	3177.055406	22.857267
98.727510	3201.535069	22.862285
98.940691	3204.746304	22.867303
98.971230	3212.149255	22.872320
98.937221	3207.546456	22.877338
99.293879	3222.681643	22.882355
99.287643	3233.726373	22.887373
99.299481	3228.504072	22.892391
99.535698	3234.814306	22.897408
99.629114	3234.048486	22.902426
100.133005	3246.758713	22.907443
99.985626	3252.753456	22.912461
99.848832	3258.102665	22.917479
100.148432	3264.213603	22.922496
100.172111	3263.102050	22.927514
100.197391	3263.707253	22.932531
100.396251	3269.265848	22.937549
100.652983	3272.176740	22.942567
100.721593	3276.341736	22.947584
100.755205	3277.813608	22.952602
100.990451	3277.732570	22.957619
100.967522	3274.914465	22.962637
101.277796	3276.570243	22.967655
100.919890	3282.231853	22.972672
100.849965	3291.522243	22.977690
101.241619	3297.817615	22.982707
101.148405	3302.591881	22.987725
101.545375	3307.876417	22.992743
101.775229	3317.085134	22.997760
101.989032	3326.539404	23.002778
102.159850	3326.187551	23.007795
101.637532	3329.289944	23.012813
102.350465	3323.721053	23.017831
102.522078	3325.414342	23.022848
102.363439	3326.130426	23.027866
102.483313	3326.114807	23.032883
102.395867	3324.480937	23.037901
102.613811	3320.097450	23.042919
102.715779	3328.527672	23.047936
102.490692	3325.311978	23.052954
102.420434	3337.619843	23.057971
102.490283	3344.439091	23.062989
102.807988	3340.216721	23.068007
102.952586	3361.091800	23.073024
103.255490	3378.135621	23.078042
103.230686	3381.204265	23.083059
103.246543	3375.214315	23.088077
103.372424	3376.226703	23.093095
103.282812	3387.688594	23.098112
103.689010	3395.692429	23.103130
103.911338	3401.572486	23.108147
104.232780	3400.998187	23.113165
104.221493	3400.977867	23.118183
104.259023	3409.153093	23.123200
104.378301	3388.738478	23.128218
104.241737	3404.737007	23.133235
103.957652	3416.036851	23.138253
104.460326	3420.515787	23.143271
104.852366	3415.792528	23.148288
104.602273	3422.175862	23.153306
104.846580	3438.831228	23.158323
104.690405	3458.348990	23.163341
105.064638	3449.045569	23.168359
104.996316	3447.430785	23.173376
105.184738	3456.131589	23.178394
105.444850	3464.054184	23.183411
105.490711	3478.016791	23.188429
105.915225	3476.337417	23.193447
105.792787	3473.061427	23.198464
105.821620	3477.251639	23.203482
105.740167	3476.456392	23.208499
105.825956	3494.800017	23.213517
105.791635	3497.017969	23.218535
105.976005	3508.907301	23.223552
106.273031	3516.764166	23.228570
106.416492	3521.103714	23.233587
106.338097	3530.228269	23.238605
106.479851	3521.305271	23.243623
106.748178	3533.541286	23.248640
107.089648	3540.169706	23.253658
107.294119	3548.205213	23.258675
107.254127	3551.503520	23.263693
107.536817	3551.263545	23.268711
107.717980	3553.962224	23.273728
107.235910	3541.320966	23.278746
107.919251	3544.947831	23.283763
107.520888	3543.842412	23.288781
108.046325	3554.980794	23.293799
108.109866	3548.977003	23.298816
108.345454	3561.486452	23.303834
108.331719	3568.713419	23.308851
108.390362	3569.086151	23.313869
108.770241	3572.665875	23.318887
108.686111	3574.228814	23.323904
108.355528	3567.762815	23.328922
108.954258	3568.511754	23.333939
108.786755	3567.490104	23.338957
108.653957	3569.537271	23.343975
108.815036	3573.495314	23.348992
108.565969	3586.582566	23.354010
108.815583	3594.771994	23.359027
108.931993	3606.182808	23.364045
109.203715	3597.523480	23.369063
109.360628	3616.440004	23.374080
109.691277	3628.473783	23.379098
110.008434	3622.805836	23.384115
109.940333	3628.229613	23.389133
109.783572	3627.102118	23.394151
110.162709	3618.059817	23.399168
109.812611	3617.265621	23.404186
110.051963	3624.175202	23.409203
109.742994	3636.694267	23.414221
109.943003	3644.250755	23.419239
110.281077	3641.436005	23.424256
110.308558	3661.158780	23.429274
110.859948	3661.457472	23.434291
110.272013	3665.327721	23.439309
110.906716	3669.615593	23.444327
111.172087	3683.499779	23.449344
111.261393	3688.185581	23.454362
111.295047	3681.665632	23.459379
111.164382	3691.202468	23.464397
111.539960	3687.573813	23.469415
111.650641	3702.533310	23.474432
111.757318	3701.127812	23.479450
112.050567	3707.151518	23.484467
112.070483	3712.072297	23.489485
112.196283	3707.270735	23.494503
112.384389	3707.638969	23.499520
112.329316	3708.812293	23.504538
112.391500	3724.341235	23.509555
112.454607	3738.023582	23.514573
112.540508	3743.533738	23.519591
113.234990	3736.250561	23.524608
113.027593	3734.405033	23.529626
113.161499	3730.498597	23.534643
113.033944	3745.785838	23.539661
113.046060	3757.755979	23.544679
113.294949	3760.137912	23.549696
113.440493	3759.253431	23.554714
113.508629	3761.382768	23.559731
113.250869	3778.802035	23.564749
113.932029	3784.269445	23.569767
113.926557	3781.385400	23.574784
113.777369	3789.694211	23.579802
113.946290	3786.527178	23.584819
113.886093	3806.285942	23.589837
114.245715	3810.206619	23.594855
114.654813	3802.409451	23.599872
114.569032	3817.532390	23.604890
114.644916	3809.938929	23.609907
114.680702	3832.296150	23.614925
114.971490	3835.766787	23.619943
115.145624	3840.777069	23.624960
114.901204	3844.341027	23.629978
115.196837	3841.756998	23.634995
115.402538	3855.262432	23.640013
115.852986	3860.554535	23.645031
115.544629	3859.643315	23.650048
115.660331	3863.283424	23.655066
115.761069	3864.353438	23.660083
116.063251	3870.909227	23.665101
115.986730	3882.691329	23.670119
116.303464	3880.457502	23.675136
116.226046	3884.626579	23.680154
116.310254	3890.320115	23.685171
116.505210	3884.478693	23.690189
116.284276	3887.890631	23.695207
116.564226	3895.295819	23.700224
116.768830	3914.845928	23.705242
116.778662	3901.663363	23.710259
117.103987	3914.108496	23.715277
117.531021	3926.468262	23.720295
117.465099	3918.120503	23.725312
117.371604	3941.400837	23.730330
117.982500	3942.889638	23.735347
117.820285	3926.785949	23.740365
118.137306	3929.756943	23.745383
117.837493	3930.564607	23.750400
117.840067	3929.762488	23.755418
118.095748	3929.905507	23.760435
118.112025	3935.477131	23.765453
118.381038	3944.023507	23.770471
118.600181	3949.465504	23.775488
118.472908	3958.623183	23.780506
118.871429	3954.037653	23.785523
118.656250	3958.976393	23.790541
118.463059	3968.049712	23.795559
118.904587	3967.251419	23.800576
118.879525	3978.956081	23.805594
118.941461	3989.854867	23.810611
119.315744	3995.259948	23.815629
119.455215	4008.668555	23.820647
119.527728	4006.539259	23.825664
119.323239	4019.604057	23.830682
119.822893	4028.707741	23.835699
119.759342	4039.348454	23.840717
119.948364	4038.539214	23.845735
120.345022	4049.660203	23.850752
120.416602	4051.962636	23.855770
120.678016	4055.185406	23.860787
120.638892	4055.245199	23.865805
120.647716	4055.840382	23.870823
120.649463	4064.602290	23.875840
121.054692	4079.108775	23.880858
121.154920	4074.576261	23.885875
121.433587	4067.455947	23.890893
121.266228	4080.451843	23.895911
120.976643	4090.941771	23.900928
121.469801	4102.568480	23.905946
122.034279	4110.538368	23.910963
122.175058	4104.017266	23.915981
121.971095	4099.986926	23.920999
121.981591	4114.984554	23.926016
122.397882	4126.190894	23.931034
122.358246	4126.203421	23.936051
122.711208	4131.930681	23.941069
122.346520	4127.341578	23.946087
122.477725	4133.340312	23.951104
122.216411	4159.554277	23.956122
122.208176	4151.503546	23.961139
122.886719	4174.458058	23.966157
123.013011	4185.365817	23.971175
123.137196	4178.891479	23.976192
123.463199	4188.505382	23.981210
123.929477	4194.249630	23.986227
123.984902	4203.634480	23.991245
123.876267	4211.643583	23.996263
123.991567	4213.105890	24.001280
124.071267	4212.427402	24.006298
124.224174	4203.246651	24.011315
124.534913	4202.339425	24.016333
124.470899	4202.144292	24.021351
124.520287	4217.830326	24.026368
124.777804	4224.367989	24.031386
124.849817	4224.097885	24.036403
125.052722	4227.819099	24.041421
124.857671	4228.411508	24.046439
125.074233	4213.371911	24.051456
124.996546	4232.824550	24.056474
125.291783	4246.458288	24.061491
125.450642	4240.985398	24.066509
125.343565	4252.722025	24.071527
125.526562	4246.655098	24.076544
125.762319	4256.090633	24.081562
125.922992	4273.075515	24.086579
126.192403	4277.212440	24.091597
125.987307	4272.661425	24.096615
126.119938	4269.184350	24.101632
126.514805	4298.452152	24.106650
126.359870	4297.280139	24.111667
126.772803	4299.185072	24.116685
126.667065	4306.742391	24.121703
126.967868	4321.439036	24.126720
126.585994	4325.333954	24.131738
126.936153	4336.468717	24.136755
127.373154	4340.699346	24.141773
127.647571	4350.223567	24.146791
127.508488	4350.703048	24.151808
127.568017	4347.177438	24.156826
127.724117	4356.420336	24.161843
127.930982	4362.707156	24.166861
128.357818	4374.445439	24.171879
128.203908	4371.433044	24.176896
128.684902	4369.580608	24.181914
128.674433	4376.261318	24.186931
129.044776	4374.404122	24.191949
128.747749	4386.069587	24.196967
129.143221	4395.536989	24.201984
129.098296	4391.159708	24.207002
128.836103	4394.524544	24.212019
129.325510	4387.181703	24.217037
129.068710	4403.067377	24.222055
129.634592	4412.978404	24.227072
129.666170	4422.591212	24.232090
129.482835	4424.545385	24.237107
129.990076	4434.351978	24.242125
129.855392	4439.287705	24.247143
129.938296	4447.386850	24.252160
129.851071	4459.398269	24.257178
130.170449	4466.462929	24.262195
130.440529	4462.216198	24.267213
130.184382	4475.295729	24.272231
131.004060	4481.183560	24.277248
130.809810	4490.639239	24.282266
130.972615	4496.740463	24.287283
131.125571	4501.586953	24.292301
131.438347	4510.953739	24.297319
131.602117	4515.340848	24.302336
131.775911	4514.862249	24.307354
131.592102	4522.892735	24.312371
132.257443	4527.201268	24.317389
132.015125	4545.976138	24.322407
131.872842	4539.590765	24.327424
132.445342	4535.429212	24.332442
132.105229	4560.554485	24.337459
132.717273	4553.002976	24.342477
133.016477	4567.921025	24.347495
132.816846	4573.166831	24.352512
132.671054	4568.451782	24.357530
132.741437	4580.429120	24.362547
133.429495	4582.505623	24.367565
133.664918	4587.497041	24.372583
133.203444	4596.180264	24.377600
133.704581	4583.147501	24.382618
133.568712	4589.377618	24.387635
133.867314	4602.938498	24.392653
133.711478	4611.469680	24.397671
134.040088	4614.195922	24.402688
134.258223	4615.061356	24.407706
134.099388	4625.739434	24.412723
134.842812	4629.357111	24.417741
134.920289	4640.402209	24.422759
134.992144	4643.875738	24.427776
134.639051	4644.489762	24.432794
134.945547	4650.391762	24.437811
135.214451	4651.934205	24.442829
135.375375	4667.151773	24.447847
135.271335	4664.033665	24.452864
135.420818	4658.300129	24.457882
135.468866	4677.954500	24.462899
135.852921	4689.541865	24.467917
135.704865	4699.400761	24.472935
135.851087	4699.333667	24.477952
136.105198	4705.231266	24.482970
135.981571	4718.407000	24.487987
136.579919	4717.315804	24.493005
136.573711	4721.246647	24.498023
136.746943	4737.724953	24.503040
136.967479	4737.857703	24.508058
136.777086	4744.077475	24.513075
137.021832	4759.727058	24.518093
136.864912	4757.804072	24.523111
137.153869	4769.924056	24.528128
137.320183	4774.364491	24.533146
137.537624	4788.815740	24.538163
137.790913	4783.103780	24.543181
137.987111	4806.254609	24.548199
138.076184	4818.061879	24.553216
138.413340	4818.892893	24.558234
138.350836	4816.951952	24.563251
138.463334	4821.255629	24.568269
138.908508	4842.767136	24.573287
138.895929	4837.415622	24.578304
139.253052	4839.585038	24.583322
138.860793	4835.760799	24.588339
139.344213	4849.210838	24.593357
139.090709	4865.320512	24.598375
139.475805	4862.652882	24.603392
140.068278	4869.697010	24.608410
140.031198	4881.271561	24.613427
139.876079	4886.860860	24.618445
140.177918	4890.333127	24.623463
140.466378	4889.129487	24.628480
140.234090	4881.621738	24.633498
140.727652	4903.876994	24.638515
140.590415	4915.186325	24.643533
140.699862	4925.165986	24.648551
141.054608	4924.826325	24.653568
141.106120	4934.136407	24.658586
141.343974	4944.761995	24.663603
141.453844	4947.696168	24.668621
141.694132	4942.336573	24.673639
141.340964	4950.987213	24.678656
141.355025	4958.857472	24.683674
141.698927	4973.794106	24.688691
141.939875	4977.594742	24.693709
142.330677	4989.613690	24.698727
142.039534	4996.742640	24.703744
142.247204	4990.330692	24.708762
142.371839	5001.583267	24.713779
142.741816	5009.066349	24.718797
142.845669	5027.029903	24.723815
142.946458	5023.320931	24.728832
143.369741	5023.415607	24.733850
143.423659	5041.386999	24.738867
143.453259	5045.978339	24.743885
143.564644	5045.244352	24.748903
143.745206	5047.716076	24.753920
144.063180	5043.950978	24.758938
143.631146	5064.271257	24.763955
143.953442	5077.734083	24.768973
144.135508	5075.704293	24.773991
144.267338	5086.469680	24.779008
144.296244	5094.375551	24.784026
144.640714	5108.399954	24.789043
144.601756	5112.395987	24.794061
145.054709	5124.152760	24.799079
144.919095	5133.921557	24.804096
145.195722	5128.171112	24.809114
145.322355	5137.785189	24.814131
145.599992	5136.217065	24.819149
146.033001	5143.601943	24.824167
146.162333	5150.172650	24.829184
145.886062	5155.986189	24.834202
146.168381	5170.503335	24.839219
146.148734	5172.015271	24.844237
146.538329	5175.132933	24.849255
146.281650	5192.442899	24.854272
146.692022	5194.424090	24.859290
146.852858	5201.498093	24.864307
147.034843	5204.553587	24.869325
147.144246	5218.905309	24.874343
147.365377	5229.849343	24.879360
147.362078	5230.313887	24.884378
147.478080	5236.814111	24.889395
147.777950	5247.029270	24.894413
148.073103	5245.720392	24.899431
147.828591	5251.522672	24.904448
148.120907	5263.159498	24.909466
148.110474	5272.545748	24.914483
148.359123	5280.420430	24.919501
148.676640	5288.274856	24.924519
148.648118	5288.932750	24.929536
148.926792	5298.131671	24.934554
148.916909	5314.759139	24.939571
149.106478	5320.613387	24.944589
149.452525	5328.722205	24.949607
149.253078	5332.708706	24.954624
149.760061	5349.125808	24.959642
149.837909	5355.168028	24.964659
150.011670	5359.064500	24.969677
150.383863	5368.346661	24.974695
150.261921	5378.135543	24.979712
150.292401	5379.260848	24.984730
150.730074	5389.100955	24.989747
151.037337	5394.589559	24.994765
151.513913	5397.838838	24.999783
151.409802	5413.452094	25.004800
151.116842	5401.944706	25.009818
151.374125	5402.182188	25.014835
151.634119	5421.163359	25.019853
152.021509	5428.072534	25.024871
151.831913	5428.818800	25.029888
151.976567	5431.911747	25.034906
152.289007	5434.962626	25.039923
152.160225	5453.082998	25.044941
152.402021	5447.514682	25.049959
152.665296	5459.080424	25.054976
152.793449	5455.401800	25.059994
153.142375	5470.596900	25.065011
152.764661	5478.683436	25.070029
153.074045	5468.176997	25.075047
153.001767	5482.778355	25.080064
153.276317	5493.395357	25.085082
153.551682	5502.383405	25.090099
153.370009	5498.829071	25.095117
153.773627	5515.417193	25.100135
153.794772	5526.231747	25.105152
154.092585	5526.251386	25.110170
154.249812	5541.198791	25.115187
154.283314	5550.180560	25.120205
154.770743	5553.339781	25.125223
154.702682	5565.067982	25.130240
154.928178	5583.123510	25.135258
154.842748	5576.125943	25.140275
154.758774	5588.456418	25.145293
155.451613	5595.033705	25.150311
155.403574	5607.563747	25.155328
155.516530	5616.744598	25.160346
155.935186	5632.351903	25.165363
155.708806	5635.657690	25.170381
156.200551	5638.105997	25.175399
156.240603	5663.286868	25.180416
156.437494	5664.562893	25.185434
156.620074	5672.646967	25.190451
156.360835	5684.143190	25.195469
156.904752	5678.912588	25.200487
157.422461	5706.427236	25.205504
157.419770	5700.114287	25.210522
157.925875	5716.623403	25.215539
157.711372	5713.920163	25.220557
158.219304	5715.226380	25.225575
158.017547	5727.878444	25.230592
158.175764	5735.934796	25.235610
158.399861	5741.827965	25.240627
158.264512	5747.837425	25.245645
158.439091	5757.813650	25.250663
158.640280	5768.035092	25.255680
158.802538	5766.513402	25.260698
158.822510	5786.302790	25.265715
159.165027	5794.879561	25.270733
159.258855	5792.064871	25.275751
159.127339	5809.870354	25.280768
159.690574	5822.263741	25.285786
159.745779	5817.996699	25.290803
160.161376	5841.022926	25.295821
160.238585	5846.639253	25.300839
160.473504	5849.926473	25.305856
160.430279	5849.617579	25.310874
160.824674	5864.581757	25.315891
160.625673	5876.633716	25.320909
160.930317	5873.707068	25.325927
160.743558	5892.499869	25.330944
161.030199	5903.765500	25.335962
161.422096	5907.902551	25.340979
161.623720	5931.161287	25.345997
161.877005	5928.728812	25.351015
161.703841	5934.873684	25.356032
162.111720	5948.109088	25.361050
162.311420	5955.114160	25.366067
162.592063	5958.277438	25.371085
162.628478	5958.016043	25.376103
163.016299	5968.170477	25.381120
163.094661	5973.837171	25.386138
163.691107	5973.298635	25.391155
163.361523	5976.617495	25.396173
163.462673	5970.711187	25.401191
163.099871	5983.151902	25.406208
163.644869	5991.409781	25.411226
163.834906	5993.577104	25.416243
163.972086	6007.360038	25.421261
164.009126	6018.251311	25.426279
164.382661	6026.188826	25.431296
164.569547	6027.816844	25.436314
164.626073	6039.516360	25.441331
164.649988	6048.641930	25.446349
165.076346	6046.747384	25.451367
165.081554	6051.371208	25.456384
164.917923	6067.742496	25.461402
165.452839	6077.567742	25.466419
165.465285	6079.904951	25.471437
165.657576	6083.129444	25.476455
166.062417	6097.325086	25.481472
165.963951	6116.603051	25.486490
166.448203	6124.466442	25.491507
166.462618	6127.785101	25.496525
166.551221	6137.351998	25.501543
166.416294	6138.657944	25.506560
166.514657	6159.287780	25.511578
166.918337	6174.313893	25.516595
166.778979	6192.180954	25.521613
167.369677	6195.248348	25.526631
167.421419	6214.165108	25.531648
167.667994	6218.324996	25.536666
168.048197	6228.982698	25.541683
168.028412	6241.032073	25.546701
167.923252	6244.394740	25.551719
168.259300	6266.584792	25.556736
168.458463	6270.613221	25.561754
168.995061	6275.169637	25.566771
168.747977	6292.479137	25.571789
169.226662	6292.669320	25.576807
169.761329	6299.382132	25.581824
169.872649	6305.653025	25.586842
169.606395	6324.727049	25.591859
169.615012	6319.750596	25.596877
169.756734	6321.464636	25.601895
170.228312	6337.585124	25.606912
170.354381	6345.795151	25.611930
170.688502	6359.443322	25.616947
170.730796	6372.019714	25.621965
170.750704	6376.543457	25.626983
170.936979	6380.261406	25.632000
171.523633	6395.934592	25.637018
171.597778	6400.418276	25.642035
171.293064	6400.592291	25.647053
171.546189	6419.253580	25.652071
171.801703	6419.661823	25.657088
171.724058	6433.008368	25.662106
172.343860	6447.195860	25.667123
172.400723	6460.792838	25.672141
172.562528	6450.574131	25.677159
172.701945	6470.803284	25.682176
172.560769	6476.899129	25.687194
172.843359	6486.893557	25.692212
172.665580	6489.841474	25.697229
173.354275	6510.186656	25.702247
173.567703	6524.406303	25.707264
173.716843	6533.960766	25.712282
174.523435	6533.461903	25.717300
174.195379	6551.867125	25.722317
174.447541	6553.424984	25.727335
174.509991	6553.711948	25.732352
174.322533	6561.257745	25.737370
174.775262	6576.601659	25.742388
174.739914	6594.111878	25.747405
175.139370	6590.030645	25.752423
175.171468	6599.262539	25.757440
175.173104	6614.453018	25.762458
175.501377	6610.297698	25.767476
175.766663	6633.948272	25.772493
175.704282	6643.498047	25.777511
176.049855	6652.440937	25.782528
176.164401	6667.238106	25.787546
176.200312	6667.560798	25.792564
177.112742	6682.760176	25.797581
177.020938	6700.680261	25.802599
177.384848	6699.688825	25.807616
177.170746	6710.682991	25.812634
177.869992	6703.328456	25.817652
177.594454	6711.860426	25.822669
177.683287	6728.678907	25.827687
178.019414	6717.166841	25.832704
177.740395	6743.141042	25.837722
178.182398	6744.236687	25.842740
178.490553	6751.026191	25.847757
178.428182	6770.179225	25.852775
179.000794	6775.699285	25.857792
178.542704	6787.448330	25.862810
179.150034	6797.107934	25.867828
179.484832	6811.785479	25.872845
179.457434	6811.682442	25.877863
179.714106	6824.553874	25.882880
179.801908	6826.112251	25.887898
180.014551	6844.272057	25.892916
180.356944	6857.237417	25.897933
180.350549	6862.822957	25.902951
180.549758	6864.859515	25.907968
180.865469	6886.062240	25.912986
180.807063	6887.659312	25.918004
181.043976	6911.393611	25.923021
181.218488	6917.269672	25.928039
181.249508	6927.376360	25.933056
181.722033	6943.800297	25.938074
181.700987	6948.744150	25.943092
181.654168	6960.106870	25.948109
182.081684	6973.510414	25.953127
182.506649	6981.752823	25.958144
182.643265	6997.332870	25.963162
182.726319	6993.417923	25.968180
183.008348	7005.635187	25.973197
183.161269	7020.688652	25.978215
183.374313	7026.075704	25.983232
183.734889	7038.192290	25.988250
183.497403	7039.476483	25.993268
184.192856	7046.596880	25.998285
183.988531	7071.817967	26.003303
184.414097	7064.749249	26.008320
184.419028	7081.906360	26.013338
184.789857	7091.060180	26.018356
185.388411	7099.916303	26.023373
185.027295	7107.404291	26.028391
185.508620	7106.249222	26.033408
185.497594	7125.160969	26.038426
185.456772	7127.948627	26.043444
185.890124	7126.703207	26.048461
185.955766	7148.204279	26.053479
186.272581	7147.324378	26.058496
186.144668	7167.728769	26.063514
186.527942	7175.311683	26.068532
186.860243	7178.969035	26.073549
186.851986	7186.995281	26.078567
187.267074	7198.329982	26.083584
187.371830	7209.833271	26.088602
187.627164	7220.912046	26.093620
187.487073	7217.543435	26.098637
187.835602	7221.902254	26.103655
187.841992	7234.642708	26.108672
188.042069	7240.735855	26.113690
188.414623	7252.228786	26.118708
188.705320	7257.392226	26.123725
188.413271	7269.185016	26.128743
188.878575	7263.941032	26.133760
188.551631	7283.707458	26.138778
188.634861	7292.707545	26.143796
189.321577	7317.555762	26.148813
189.428449	7322.905866	26.153831
189.474778	7323.785721	26.158848
189.174528	7342.995559	26.163866
189.841963	7356.358640	26.168884
190.162062	7371.383045	26.173901
190.569089	7390.084350	26.178919
190.607966	7393.251028	26.183936
190.825518	7413.380582	26.188954
191.065278	7431.233649	26.193972
191.410514	7435.558308	26.198989
191.468682	7445.702068	26.204007
191.741996	7452.061627	26.209024
192.004089	7463.322594	26.214042
192.106947	7481.408675	26.219060
192.346772	7486.302334	26.224077
192.305647	7498.033861	26.229095
192.917998	7502.660802	26.234112
192.770769	7517.196592	26.239130
192.867352	7530.080971	26.244148
193.552523	7530.886011	26.249165
193.349326	7542.279901	26.254183
193.688508	7555.940799	26.259200
193.473390	7569.360215	26.264218
194.038146	7576.138239	26.269236
194.257661	7593.849414	26.274253
194.167985	7609.850585	26.279271
194.756616	7617.439395	26.284288
194.904730	7622.663159	26.289306
194.886824	7640.575738	26.294324
195.050868	7649.231852	26.299341
195.262981	7666.132900	26.304359
195.736070	7670.806958	26.309376
195.759509	7679.611394	26.314394
195.615392	7680.003349	26.319412
196.162950	7701.085453	26.324429
196.245000	7712.024347	26.329447
196.596141	7720.815351	26.334464
196.684636	7730.414664	26.339482
196.791591	7748.440381	26.344500
196.890671	7750.132823	26.349517
196.893316	7778.706797	26.354535
197.278560	7783.464099	26.359552
197.812738	7797.947031	26.364570
197.538871	7813.134302	26.369588
198.086170	7824.691771	26.374605
198.454088	7848.277315	26.379623
198.572448	7840.501894	26.384640
198.829368	7866.621022	26.389658
198.983732	7883.521846	26.394676
199.556482	7876.698113	26.399693
199.332262	7895.473566	26.404711
199.637594	7904.344446	26.409728
199.756196	7905.497143	26.414746
199.648399	7922.442229	26.419764
199.826981	7924.920970	26.424781
200.273840	7936.086983	26.429799
200.456780	7955.944729	26.434816
200.663229	7967.502015	26.439834
200.396894	7977.456966	26.444852
200.744394	7980.925832	26.449869
200.941185	8002.388410	26.454887
201.119597	8009.700683	26.459904
201.486658	8023.247062	26.464922
201.492547	8044.266034	26.469940
202.054567	8048.007543	26.474957
201.849706	8069.343697	26.479975
202.123287	8077.124123	26.484992
202.517516	8094.735794	26.490010
202.526737	8103.956240	26.495028
202.624371	8113.465922	26.500045
203.395061	8126.409280	26.505063
203.772136	8138.975474	26.510080
204.002089	8157.436945	26.515098
203.746409	8158.051598	26.520116
204.177442	8171.370224	26.525133
204.145825	8180.338223	26.530151
204.263751	8189.267013	26.535168
204.475933	8202.629418	26.540186
204.878857	8212.915331	26.545204
205.163063	8225.123592	26.550221
205.166614	8238.411365	26.555239
205.244721	8256.603111	26.560256
205.740141	8261.586377	26.565274
205.244310	8275.315478	26.570292
206.127012	8282.659596	26.575309
206.112728	8306.163530	26.580327
206.502422	8324.732742	26.585344
206.757703	8329.340062	26.590362
206.850104	8346.538316	26.595380
207.163621	8353.823245	26.600397
207.140025	8380.975231	26.605415
207.622596	8386.209959	26.610432
207.642992	8405.168607	26.615450
208.063068	8420.951708	26.620468
208.164582	8431.906921	26.625485
208.407514	8441.106708	26.630503
208.500581	8459.542568	26.635520
208.199550	8463.997128	26.640538
208.583392	8485.509893	26.645556
209.062260	8503.080280	26.650573
209.279473	8514.948782	26.655591
209.425609	8529.070019	26.660608
209.927776	8552.026095	26.665626
209.829145	8561.753027	26.670644
210.519495	8571.788897	26.675661
210.795036	8583.376788	26.680679
211.052622	8605.417778	26.685696
210.964617	8601.592434	26.690714
211.139945	8621.079538	26.695732
211.650845	8619.092566	26.700749
211.855240	8635.638948	26.705767
211.903213	8638.378194	26.710784
212.390893	8644.328878	26.715802
212.175716	8667.665837	26.720820
212.735049	8668.717966	26.725837
212.537501	8678.185779	26.730855
212.995253	8694.152643	26.735872
213.095030	8698.531840	26.740890
213.275940	8716.486928	26.745908
213.599212	8717.332936	26.750925
214.075169	8733.903165	26.755943
213.778504	8752.712935	26.760960
214.265579	8742.340977	26.765978
214.082069	8764.375484	26.770996
214.412216	8775.434002	26.776013
214.208694	8782.942174	26.781031
214.700076	8798.828086	26.786048
214.751386	8807.088809	26.791066
214.782146	8830.990474	26.796084
215.196576	8856.173886	26.801101
215.756185	8864.178200	26.806119
215.937280	8882.411256	26.811136
216.331320	8898.107283	26.816154
216.458523	8908.177886	26.821172
216.440677	8919.338363	26.826189
216.472652	8934.608084	26.831207
216.492150	8942.315018	26.836224
217.243978	8952.022584	26.841242
217.114328	8982.279848	26.846260
217.987248	8988.119777	26.851277
217.810779	9010.185045	26.856295
217.800721	9022.026330	26.861312
218.172196	9023.174213	26.866330
218.352136	9045.647805	26.871348
218.718873	9053.922369	26.876365
219.048746	9053.135055	26.881383
219.042859	9087.654348	26.886400
219.296736	9090.610828	26.891418
219.557990	9117.532988	26.896436
219.847994	9119.047254	26.901453
219.873836	9144.017250	26.906471
219.868315	9155.984202	26.911488
220.283103	9179.617774	26.916506
220.490030	9189.622365	26.921524
221.110023	9196.692281	26.926541
221.129198	9218.095688	26.931559
221.618345	9227.579339	26.936576
221.803465	9239.270210	26.941594
222.122563	9257.478857	26.946612
222.634726	9259.015164	26.951629
222.626038	9278.598090	26.956647
222.344113	9290.791551	26.961664
222.654508	9301.376725	26.966682
223.338694	9311.641291	26.971700
223.374821	9323.317668	26.976717
223.617485	9332.666334	26.981735
223.525086	9351.735179	26.986752
223.858055	9370.232237	26.991770
224.203064	9379.624882	26.996788
224.553414	9389.891273	27.001805
224.722615	9403.261277	27.006823
224.728559	9419.681581	27.011840
225.078425	9433.910512	27.016858
225.229239	9433.568002	27.021876
225.582213	9453.564896	27.026893
225.730606	9470.045019	27.031911
226.109670	9490.277823	27.036928
226.128840	9497.145187	27.041946
225.792273	9508.864279	27.046964
226.560558	9526.380826	27.051981
226.930273	9538.358702	27.056999
226.918849	9550.364719	27.062016
227.392483	9556.459980	27.067034
227.426936	9570.842621	27.072052
227.302837	9596.616577	27.077069
227.435470	9610.175585	27.082087
227.834486	9622.174183	27.087104
228.299449	9641.765381	27.092122
228.284017	9667.348757	27.097140
228.550592	9684.085247	27.102157
229.071059	9688.089352	27.107175
228.741895	9704.672912	27.112192
229.545460	9722.038879	27.117210
229.342610	9730.526112	27.122228
230.136751	9747.063189	27.127245
230.258463	9763.001525	27.132263
230.393969	9780.446943	27.137280
230.457571	9786.808587	27.142298
230.687955	9806.401975	27.147316
230.939991	9815.853610	27.152333
231.340232	9832.048324	27.157351
231.637404	9844.293510	27.162368
231.877070	9868.217455	27.167386
232.061015	9869.656835	27.172404
231.911454	9887.942675	27.177421
232.470648	9895.167625	27.182439
232.682649	9912.809572	27.187456
232.899689	9923.583383	27.192474
233.302623	9949.802551	27.197492
233.841128	9958.833649	27.202509
234.029221	9960.111359	27.207527
233.789440	9981.047865	27.212544
234.302612	9982.770365	27.217562
234.363202	9993.019333	27.222580
234.492793	10004.331022	27.227597
234.910044	10027.810572	27.232615
235.166070	10044.056480	27.237632
235.283360	10062.426985	27.242650
235.508965	10070.196821	27.247668
235.294063	10091.862078	27.252685
235.938777	10100.292481	27.257703
236.111408	10125.865969	27.262720
236.315872	10135.697797	27.267738
236.608063	10161.985132	27.272756
236.772103	10168.372218	27.277773
237.196280	10186.997885	27.282791
237.140336	10216.370988	27.287808
237.427058	10214.873647	27.292826
237.618751	10248.540039	27.297844
237.739008	10257.128452	27.302861
238.068809	10276.451005	27.307879
238.577143	10298.353681	27.312896
238.768545	10307.786647	27.317914
239.514924	10334.776655	27.322932
238.900180	10343.325533	27.327949
239.764495	10363.369599	27.332967
239.719825	10378.538840	27.337984
240.009494	10391.909626	27.343002
240.539545	10406.120547	27.348020
240.744058	10428.058341	27.353037
241.198268	10425.574867	27.358055
240.999647	10453.606656	27.363072
241.142408	10460.196099	27.368090
241.810184	10470.681748	27.373108
241.984244	10480.572199	27.378125
242.253454	10494.644071	27.383143
242.311670	10506.867134	27.388160
242.769643	10516.548937	27.393178
243.248267	10537.777684	27.398196
243.245621	10538.002288	27.403213
243.583322	10549.461683	27.408231
243.787912	10569.754566	27.413248
243.659111	10573.248018	27.418266
244.095522	10587.975793	27.423284
244.376009	10607.315886	27.428301
244.327970	10616.382355	27.433319
244.490584	10635.049444	27.438336
244.748996	10657.032741	27.443354
245.113756	10659.735289	27.448372
245.280850	10683.349579	27.453389
245.517980	10687.136214	27.458407
245.799651	10709.889526	27.463424
245.675996	10715.924019	27.468442
246.375420	10736.319545	27.473460
246.579846	10747.749419	27.478477
246.844849	10770.249655	27.483495
247.041328	10776.818164	27.488512
247.179035	10792.028635	27.493530
247.441202	10805.868186	27.498548
247.813628	10827.698048	27.503565
247.929002	10830.660717	27.508583
247.822070	10862.726748	27.513600
248.135778	10869.340077	27.518618
248.416518	10886.261722	27.523636
248.385041	10917.188773	27.528653
248.807643	10927.893070	27.533671
249.333987	10945.928811	27.538688
249.237709	10964.175778	27.543706
249.589118	10984.828179	27.548724
249.626514	11009.167339	27.553741
250.171845	11027.320172	27.558759
250.279547	11052.905097	27.563776
250.607821	11072.118196	27.568794
251.019068	11091.419360	27.573812
251.037272	11117.128910	27.578829
251.187892	11127.913820	27.583847
251.819184	11149.176183	27.588864
251.929746	11178.673117	27.593882
252.540919	11196.102178	27.598900
252.307382	11220.979801	27.603917
252.566609	11238.574552	27.608935
253.184671	11262.128398	27.613952
253.493251	11273.665425	27.618970
253.615783	11294.628736	27.623988
254.293521	11313.095814	27.629005
254.537573	11326.382843	27.634023
255.195544	11334.751738	27.639040
255.072132	11361.898432	27.644058
255.487594	11361.021838	27.649076
255.582935	11373.463842	27.654093
256.062829	11381.734348	27.659111
255.783337	11396.666480	27.664128
255.901023	11425.398533	27.669146
256.700095	11429.305695	27.674164
256.509493	11445.761723	27.679181
256.562261	11461.184975	27.684199
257.117246	11484.464792	27.689216
257.521172	11504.528527	27.694234
257.572686	11525.459013	27.699252
257.696369	11534.710588	27.704269
258.003387	11555.591609	27.709287
258.406622	11575.759733	27.714304
258.733990	11597.026008	27.719322
258.934591	11604.364638	27.724340
259.444569	11627.803252	27.729357
259.639167	11641.369813	27.734375
259.840751	11650.167164	27.739392
260.133364	11669.910640	27.744410
260.717375	11675.386188	27.749428
260.870722	11690.575991	27.754445
260.954694	11705.861932	27.759463
261.211250	11720.265110	27.764480
261.207928	11739.174016	27.769498
261.933422	11745.420008	27.774516
261.939366	11761.630797	27.779533
262.229804	11776.316063	27.784551
262.341212	11794.502880	27.789568
262.464937	11807.101769	27.794586
262.940240	11817.529914	27.799604
263.140914	11833.931302	27.804621
263.400779	11852.205439	27.809639
263.309818	11854.670095	27.814656
263.719602	11872.889190	27.819674
264.214086	11886.686831	27.824692
264.298679	11907.580983	27.829709
264.091734	11920.118069	27.834727
264.675472	11947.988475	27.839744
264.758031	11973.164926	27.844762
264.818724	11971.889165	27.849780
265.255836	12008.640128	27.854797
265.778082	12023.627154	27.859815
266.022597	12042.437543	27.864832
266.322231	12073.409357	27.869850
266.866505	12087.354076	27.874868
266.860648	12110.690949	27.879885
267.078998	12123.420484	27.884903
267.328227	12145.002766	27.889920
267.501273	12160.180389	27.894938
267.923616	12181.331397	27.899956
268.131055	12212.459982	27.904973
268.376615	12225.122168	27.909991
268.840458	12242.237398	27.915008
268.588325	12266.822479	27.920026
269.312548	12278.449746	27.925044
269.459665	12307.399579	27.930061
269.981262	12323.492179	27.935079
270.548222	12342.375510	27.940096
270.467531	12359.812985	27.945114
270.694751	12382.627378	27.950132
271.096583	12395.170463	27.955149
271.078361	12421.411696	27.960167
271.684583	12436.243794	27.965184
271.618034	12451.718126	27.970202
272.001530	12470.766113	27.975220
272.365193	12496.312902	27.980237
272.691648	12521.808714	27.985255
273.258415	12533.176598	27.990272
273.221679	12553.863107	27.995290
273.399493	12574.493923	28.000308
273.761034	12591.237080	28.005325
273.877022	12607.769247	28.010343
274.137362	12627.051419	28.015360
274.011050	12652.059391	28.020378
274.782434	12669.553145	28.025396
275.269487	12700.840836	28.030413
275.484453	12715.434447	28.035431
275.977684	12734.797088	28.040448
276.094921	12755.895484	28.045466
276.677579	12771.666272	28.050484
276.674921	12787.108764	28.055501
276.587209	12802.536171	28.060519
277.220099	12813.713868	28.065536
277.371468	12831.390161	28.070554
277.867962	12854.080836	28.075572
278.020157	12872.461250	28.080589
278.308377	12887.779311	28.085607
278.567404	12903.923013	28.090624
278.595624	12925.016594	28.095642
279.038325	12937.815746	28.100660
279.119379	12967.301151	28.105677
279.116729	12992.356516	28.110695
279.727734	13004.523027	28.115712
279.923400	13035.045331	28.120730
280.417484	13053.366048	28.125748
280.476838	13060.771584	28.130765
280.399599	13086.492450	28.135783
281.240208	13106.612646	28.140800
281.373655	13121.835139	28.145818
281.622331	13152.696702	28.150836
281.990565	13168.498254	28.155853
281.972259	13189.128883	28.160871
282.011132	13207.536848	28.165888
282.433986	13225.805731	28.170906
282.803891	13253.035759	28.175924
282.952520	13270.851842	28.180941
283.475132	13297.189571	28.185959
283.772015	13314.676148	28.190976
284.034325	13330.901807	28.195994
284.728420	13355.182173	28.201012
285.309987	13374.901116	28.206029
285.503492	13398.843101	28.211047
285.501085	13411.642824	28.216064
285.666649	13423.415158	28.221082
285.664976	13444.378206	28.226100
286.209396	13459.429220	28.231117
286.592838	13491.271309	28.236135
286.783165	13513.012806	28.241152
286.729594	13534.192511	28.246170
287.286577	13559.650451	28.251188
287.789602	13571.471071	28.256205
287.581280	13602.120732	28.261223
288.477775	13619.892625	28.266240
288.660663	13645.813509	28.271258
288.945405	13648.649035	28.276276
289.289949	13674.623587	28.281293
289.452606	13705.483734	28.286311
289.915806	13717.784390	28.291328
290.129294	13747.780813	28.296346
290.205952	13759.747292	28.301364
290.650250	13785.886378	28.306381
290.646112	13806.215442	28.311399
291.381360	13818.435651	28.316416
291.555667	13835.844010	28.321434
291.995151	13857.707933	28.326452
291.955578	13880.209060	28.331469
292.577011	13907.558530	28.336487
292.663867	13920.530938	28.341504
293.117569	13943.283310	28.346522
293.333761	13966.167656	28.351540
293.639794	13983.577623	28.356557
293.525635	14006.084267	28.361575
293.973132	14031.619994	28.366592
294.303979	14056.330817	28.371610
294.871991	14076.254733	28.376628
295.261825	14097.703523	28.381645
295.571549	14113.729780	28.386663
295.722793	14132.970569	28.391680
296.266379	14154.243749	28.396698
296.178656	14171.816629	28.401716
296.703105	14193.913962	28.406733
297.083038	14214.199087	28.411751
297.313075	14232.518094	28.416768
297.210488	14254.991638	28.421786
297.598483	14279.914868	28.426804
298.218471	14286.648804	28.431821
298.188522	14322.217324	28.436839
298.519364	14325.765788	28.441856
298.787123	14349.113081	28.446874
298.957028	14384.757788	28.451892
299.506764	14399.101290	28.456909
299.621115	14419.582987	28.461927
299.974321	14444.325551	28.466944
300.280808	14467.054237	28.471962
300.371215	14490.909527	28.476980
300.618161	14492.967875	28.481997
301.029996	14513.030408	28.487015
301.286837	14540.030496	28.492032
301.518747	14557.180995	28.497050
301.904066	14585.762220	28.502068
302.418078	14606.080449	28.507085
302.617080	14633.190791	28.512103
302.974650	14655.636938	28.517120
303.559378	14674.927223	28.522138
303.512569	14694.562797	28.527156
303.765042	14716.608595	28.532173
304.043638	14733.707725	28.537191
304.510682	14757.226425	28.542208
305.065445	14772.677956	28.547226
305.216259	14802.000523	28.552244
305.733108	14810.456244	28.557261
305.395077	14839.160634	28.562279
305.842367	14861.103443	28.567296
306.572827	14880.879584	28.572314
306.495175	14912.758381	28.577332
306.852513	14926.267062	28.582349
306.768369	14957.003666	28.587367
307.490118	14968.525603	28.592384
308.025306	14997.889323	28.597402
307.701927	15026.819093	28.602420
308.593485	15051.020164	28.607437
308.802044	15074.440783	28.612455
309.361670	15098.169638	28.617472
309.777312	15122.000035	28.622490
310.005533	15143.554275	28.627508
310.479957	15164.116172	28.632525
310.405472	15178.744383	28.637543
310.614290	15200.579657	28.642560
311.399617	15222.169891	28.647578
311.271468	15250.592514	28.652596
311.751365	15256.148590	28.657613
312.098598	15294.597050	28.662631
312.341939	15309.459822	28.667648
312.569104	15332.062999	28.672666
312.903796	15360.065868	28.677684
313.400885	15374.051988	28.682701
313.636371	15399.278502	28.687719
313.989369	15415.501207	28.692736
314.499483	15432.125689	28.697754
314.695150	15462.936130	28.702772
315.101018	15471.880123	28.707789
315.185245	15505.544273	28.712807
315.653263	15513.688965	28.717824
316.063490	15542.599345	28.722842
316.170738	15559.972406	28.727860
316.476558	15587.942231	28.732877
316.919868	15608.266286	28.737895
317.111722	15633.439935	28.742912
317.410702	15651.762137	28.747930
317.310071	15676.940600	28.752948
317.879594	15696.764907	28.757965
318.287796	15721.816347	28.762983
318.441097	15748.114249	28.768000
318.628807	15761.242661	28.773018
318.795647	15799.631958	28.778036
319.372139	15815.589431	28.783053
319.625573	15849.884624	28.788071
319.907779	15875.865620	28.793088
320.311240	15894.354874	28.798106
320.642447	15933.208242	28.803124
320.910627	15951.286041	28.808141
321.252630	15975.185886	28.813159
321.901675	15995.241243	28.818176
322.342602	16014.577518	28.823194
321.964827	16041.805470	28.828212
322.781293	16067.352450	28.833229
323.156362	16081.636144	28.838247
323.154305	16107.008185	28.843264
323.637969	16122.216114	28.848282
323.573179	16155.115134	28.853300
323.957093	16167.123425	28.858317
324.436993	16196.068095	28.863335
324.569174	16225.661067	28.868352
325.240764	16254.803206	28.873370
325.201039	16271.817759	28.878388
325.702138	16299.685386	28.883405
325.819428	16320.746655	28.888423
325.569442	16354.376206	28.893440
326.670579	16381.053966	28.898458
326.923923	16415.549166	28.903476
327.066692	16435.526365	28.908493
327.660080	16469.115603	28.913511
327.742002	16510.400169	28.918528
328.101205	16530.962630	28.923546
328.398454	16553.211988	28.928564
328.385904	16584.802252	28.933581
328.873682	16624.557935	28.938599
329.288851	16661.839312	28.943616
330.186826	16675.555124	28.948634
330.209374	16719.145689	28.953652
330.687741	16731.070050	28.958669
330.948712	16765.520462	28.963687
331.515968	16794.032261	28.968704
331.988152	16815.547004	28.973722
332.196394	16839.655230	28.978740
332.550052	16856.984546	28.983757
332.843813	16882.800846	28.988775
333.013022	16907.916537	28.993792
333.643662	16928.260024	28.998810
333.893460	16962.162946	29.003828
334.268009	16986.734885	29.008845
334.523073	17008.394404	29.013863
334.248780	17040.528628	29.018880
335.473705	17063.331308	29.023898
335.630298	17098.272453	29.028916
335.815258	17119.507192	29.033933
336.103293	17153.145453	29.038951
336.124012	17182.416222	29.043968
336.778736	17201.063208	29.048986
337.430859	17233.052634	29.054004
337.556502	17252.407954	29.059021
338.301666	17275.349211	29.064039
338.408668	17302.660930	29.069056
338.985569	17310.429249	29.074074
339.265102	17341.390648	29.079092
339.514964	17363.619936	29.084109
339.566860	17385.766548	29.089127
339.584220	17416.617519	29.094144
340.195724	17435.675811	29.099162
340.489555	17458.808013	29.104180
341.023413	17498.517215	29.109197
341.484262	17524.339786	29.114215
341.537510	17547.636127	29.119232
341.937588	17574.270586	29.124250
342.259334	17594.025110	29.129268
342.715849	17630.663827	29.134285
343.103977	17650.376423	29.139303
343.089513	17686.438331	29.144320
343.781686	17698.952064	29.149338
343.861464	17732.339672	29.154356
344.079602	17756.166366	29.159373
344.833022	17775.063779	29.164391
344.740043	17802.464385	29.169408
345.272831	17812.015015	29.174426
345.633752	17841.839963	29.179444
346.095997	17865.110523	29.184461
346.186858	17891.105253	29.189479
346.684522	17919.961282	29.194496
346.934232	17941.660590	29.199514
347.109864	17970.870377	29.204532
347.506425	18001.353323	29.209549
348.108694	18028.657978	29.214567
348.056109	18060.683350	29.219584
348.257830	18084.171873	29.224602
348.621811	18113.883044	29.229620
349.095570	18150.747474	29.234637
349.577841	18182.575550	29.239655
349.569180	18204.675724	29.244672
350.212179	18242.158208	29.249690
350.538279	18276.354720	29.254708
350.697203	18303.666033	29.259725
351.177070	18333.460468	29.264743
351.767842	18373.295217	29.269760
352.029333	18395.422784	29.274778
352.579963	18422.635001	29.279796
352.653978	18459.423645	29.284813
353.044139	18484.746839	29.289831
353.307554	18519.301068	29.294848
353.583421	18551.857023	29.299866
354.490232	18586.241095	29.304884
354.546101	18611.155626	29.309901
354.847955	18639.481123	29.314919
355.689006	18675.878365	29.319936
356.017623	18698.210564	29.324954
356.150974	18721.015616	29.329972
356.645989	18751.800203	29.334989
357.480120	18779.575015	29.340007
357.467021	18804.342653	29.345024
357.575998	18818.736390	29.350042
358.285051	18844.698737	29.355060
358.363496	18874.986490	29.360077
358.581673	18900.697279	29.365095
358.854910	18932.748860	29.370112
359.325699	18964.472612	29.375130
359.075827	18999.506117	29.380148
359.768593	19025.938775	29.385165
360.509930	19052.218551	29.390183
360.837133	19092.380360	29.395200
361.259189	19115.178557	29.400218
361.571754	19159.999058	29.405236
361.845502	19190.610508	29.410253
362.486688	19221.316081	29.415271
362.670898	19249.458719	29.420288
363.120952	19281.994926	29.425306
363.670042	19306.788862	29.430324
364.316158	19328.503438	29.435341
364.558596	19348.524885	29.440359
364.806076	19375.590064	29.445376
365.583216	19402.452274	29.450394
365.688453	19425.622676	29.455412
365.892726	19449.826374	29.460429
366.144164	19470.478333	29.465447
366.149910	19495.022765	29.470464
366.472918	19520.686359	29.475482
367.213224	19557.644378	29.480500
367.523879	19587.467238	29.485517
368.183332	19608.440830	29.490535
368.258348	19637.675193	29.495552
368.875512	19662.515780	29.500570
369.336654	19677.404656	29.505588
369.469887	19706.674229	29.510605
369.639390	19719.928220	29.515623
369.747315	19752.499849	29.520640
369.925958	19769.309510	29.525658
370.670122	19797.295726	29.530676
370.860760	19835.294399	29.535693
370.882037	19863.033812	29.540711
371.231789	19892.819422	29.545728
371.771317	19929.291508	29.550746
372.037500	19957.081145	29.555764
372.175459	19993.388800	29.560781
372.723788	20022.543280	29.565799
372.970071	20067.439422	29.570816
373.349752	20090.902485	29.575834
373.763656	20136.056846	29.580852
374.438837	20174.005549	29.585869
374.711235	20207.999037	29.590887
375.351781	20254.849360	29.595904
375.693020	20273.630542	29.600922
376.140293	20314.148826	29.605940
375.997331	20344.928446	29.610957
376.862631	20383.978743	29.615975
377.073618	20419.403825	29.620992
377.254426	20453.096171	29.626010
377.669004	20484.502643	29.631028
378.210846	20515.743910	29.636045
378.706401	20554.561820	29.641063
379.228802	20601.993807	29.646080
379.242359	20623.979502	29.651098
379.914533	20658.776762	29.656116
380.394056	20700.548143	29.661133
380.573967	20730.260533	29.666151
381.410220	20764.071887	29.671168
381.892799	20789.889062	29.676186
382.288231	20824.281358	29.681204
382.409587	20857.200225	29.686221
383.088623	20871.872646	29.691239
383.525217	20901.026978	29.696256
383.270990	20935.717102	29.701274
384.105988	20951.079137	29.706292
384.587179	20993.817601	29.711309
385.029588	21025.909290	29.716327
385.135515	21047.723027	29.721344
385.560213	21077.125904	29.726362
386.191943	21111.494325	29.731380
385.898989	21143.764578	29.736397
386.317997	21172.132252	29.741415
386.827086	21208.763127	29.746432
387.050660	21246.873101	29.751450
387.522055	21279.030166	29.756468
388.030210	21319.035499	29.761485
388.289949	21353.980733	29.766503
388.856024	21396.984793	29.771520
389.331873	21423.884332	29.776538
389.992510	21447.140722	29.781556
389.801191	21490.465817	29.786573
390.759311	21518.515756	29.791591
391.054212	21555.945379	29.796608
390.722468	21592.980375	29.801626
391.434653	21616.146747	29.806644
391.969449	21662.631547	29.811661
392.257750	21692.922364	29.816679
392.582281	21722.487222	29.821696
393.270859	21765.687732	29.826714
393.358115	21786.096137	29.831732
393.773035	21817.536274	29.836749
394.255444	21855.322535	29.841767
394.753115	21876.292301	29.846784
394.997127	21912.732210	29.851802
395.472113	21946.741195	29.856820
395.655372	21977.497534	29.861837
396.191175	22005.506898	29.866855
396.526306	22031.443577	29.871872
396.509202	22081.352129	29.876890
397.085071	22099.466421	29.881908
397.532476	22135.761143	29.886925
397.728162	22173.359126	29.891943
398.202169	22211.482281	29.896960
398.472225	22250.446270	29.901978
399.128753	22293.551851	29.906996
399.392987	22334.741161	29.912013
399.741545	22376.662978	29.917031
400.047066	22407.445066	29.922048
400.431108	22443.712362	29.927066
400.859973	22485.836674	29.932084
401.287294	22525.913979	29.937101
401.667241	22569.948135	29.942119
401.885565	22605.748806	29.947136
402.477232	22649.263414	29.952154
403.092171	22701.911750	29.957172
403.236887	22734.394067	29.962189
403.569905	22773.791551	29.967207
404.319650	22823.866208	29.972224
404.671471	22859.924464	29.977242
405.359222	22890.950744	29.982260
405.600756	22940.941003	29.987277
406.427806	22982.252028	29.992295
406.719236	23014.041997	29.997312
406.828765	23051.377095	30.002330
407.525759	23081.921973	30.007348
407.673151	23124.906895	30.012365
408.170924	23158.806963	30.017383
408.720286	23186.967531	30.022400
408.930140	23234.372635	30.027418
409.428739	23268.342271	30.032436
410.060217	23309.160115	30.037453
410.527425	23341.675059	30.042471
410.743043	23376.700277	30.047488
411.230613	23414.747786	30.052506
411.876893	23444.391195	30.057524
412.505964	23489.399442	30.062541
412.753680	23521.051725	30.067559
413.131575	23551.678902	30.072576
413.223780	23579.342898	30.077594
414.058414	23613.905055	30.082612
414.275677	23656.785389	30.087629
414.534983	23689.459850	30.092647
414.981473	23724.885549	30.097664
415.482994	23759.253682	30.102682
415.807625	23792.986048	30.107700
416.277193	23829.590037	30.112717
416.882188	23866.672110	30.117735
417.134529	23900.434940	30.122752
417.413463	23938.193837	30.127770
417.958221	23972.618758	30.132788
418.070814	24013.051682	30.137805
418.413467	24052.936779	30.142823
418.846115	24088.226263	30.147840
419.325431	24125.050446	30.152858
419.945312	24167.932006	30.157876
420.219775	24199.435825	30.162893
420.430442	24246.527227	30.167911
421.033576	24272.582835	30.172928
421.498786	24310.433327	30.177946
422.249092	24340.687406	30.182964
422.274461	24379.965622	30.187981
422.638237	24410.387782	30.192999
423.132853	24442.116600	30.198016
423.329799	24494.601314	30.203034
423.597250	24521.935822	30.208052
424.343683	24560.595881	30.213069
424.489684	24605.322089	30.218087
425.261580	24631.825701	30.223104
425.502877	24673.781783	30.228122
425.919910	24710.781109	30.233140
426.478915	24752.314732	30.238157
426.999922	24789.323196	30.243175
427.367434	24820.857654	30.248192
427.445022	24868.135670	30.253210
427.901860	24910.342871	30.258228
428.488380	24946.330210	30.263245
428.651681	24997.797713	30.268263
429.280274	25030.599790	30.273280
429.185664	25086.677090	30.278298
429.892111	25127.183553	30.283316
430.603331	25170.571171	30.288333
430.853375	25216.679112	30.293351
431.169332	25255.180424	30.298368
431.817136	25306.117800	30.303386
432.599248	25346.732931	30.308404
433.248147	25380.284458	30.313421
433.406291	25429.225933	30.318439
433.547782	25470.137570	30.323456
434.001500	25518.830730	30.328474
434.352156	25552.195423	30.333492
434.950868	25592.112986	30.338509
435.146531	25644.834735	30.343527
436.156398	25693.226327	30.348544
436.145061	25728.177438	30.353562
437.046928	25768.338585	30.358580
437.451225	25813.728533	30.363597
438.028400	25858.402625	30.368615
438.355161	25886.671377	30.373632
438.666943	25935.691134	30.378650
439.213946	25968.324238	30.383668
439.766977	26006.682410	30.388685
440.121044	26062.161256	30.393703
440.609192	26085.292078	30.398720
441.021624	26130.062096	30.403738
441.462989	26173.942868	30.408756
441.812740	26214.286183	30.413773
442.221515	26253.956721	30.418791
442.908591	26289.184934	30.423808
443.338386	26339.293208	30.428826
443.580419	26367.620144	30.433844
444.268716	26412.410779	30.438861
444.716152	26454.445718	30.443879
445.314052	26488.771820	30.448896
445.645569	26530.900917	30.453914
445.931891	26570.894626	30.458932
446.074151	26609.861820	30.463949
446.209409	26648.912348	30.468967
447.400909	26692.708351	30.473984
447.505844	26738.216784	30.479002
447.973241	26787.896819	30.484020
448.902988	26815.680564	30.489037
448.873382	26856.539638	30.494055
449.958062	26893.609039	30.499072
450.321581	26940.935599	30.504090
450.021445	26981.812016	30.509108
450.779179	27009.009896	30.514125
451.018776	27064.932878	30.519143
451.582635	27088.988405	30.524160
452.216121	27132.297606	30.529178
452.235474	27171.626429	30.534196
452.413574	27199.111284	30.539213
453.366316	27247.351213	30.544231
453.907509	27280.341286	30.549248
453.884747	27329.359926	30.554266
454.130458	27362.996857	30.559284
454.686304	27408.025332	30.564301
455.154560	27459.021532	30.569319
455.896530	27501.082030	30.574336
456.637832	27545.127364	30.579354
456.651717	27593.679501	30.584372
457.468253	27625.849581	30.589389
457.256501	27683.785364	30.594407
457.594357	27723.779589	30.599424
458.034319	27782.327799	30.604442
458.618688	27837.807023	30.609460
459.362609	27882.206630	30.614477
459.633462	27931.762224	30.619495
460.279197	27989.185327	30.624512
460.808209	28025.800253	30.629530
461.504242	28077.527123	30.634548
462.025907	28118.776431	30.639565
462.318484	28167.090336	30.644583
462.993410	28214.775604	30.649600
463.478234	28257.314069	30.654618
463.837349	28305.150144	30.659636
464.575804	28346.814731	30.664653
464.653717	28397.552054	30.669671
465.514732	28436.157328	30.674688
465.847569	28479.794598	30.679706
466.160505	28515.464520	30.684724
466.999537	28559.920232	30.689741
467.232091	28604.913492	30.694759
467.567399	28651.325593	30.699776
468.267894	28691.182739	30.704794
468.622338	28734.241966	30.709812
469.236600	28788.056693	30.714829
469.703507	28830.902560	30.719847
469.926741	28876.763842	30.724864
470.713543	28909.825536	30.729882
470.908059	28962.783607	30.734900
471.744467	29005.034683	30.739917
471.846809	29049.549956	30.744935
472.725145	29087.856661	30.749952
473.249374	29127.040632	30.754970
473.581454	29175.647815	30.759988
474.203108	29209.570234	30.765005
474.344311	29261.197365	30.770023
474.774742	29302.046156	30.775040
475.660192	29348.430555	30.780058
475.952887	29391.627253	30.785076
476.212568	29427.591551	30.790093
476.769957	29478.667316	30.795111
477.172975	29524.868509	30.800128
477.565572	29563.207934	30.805146
478.377852	29611.146745	30.810164
478.749300	29654.300054	30.815181
479.373444	29705.770482	30.820199
479.813547	29748.293759	30.825216
480.273773	29787.849322	30.830234
480.531200	29829.832470	30.835252
481.010171	29878.816542	30.840269
481.721005	29925.090523	30.845287
482.028539	29964.765161	30.850304
482.686998	29999.043431	30.855322
482.956807	30053.332623	30.860340
483.483261	30080.627712	30.865357
483.940548	30138.933399	30.870375
484.228599	30168.737581	30.875392
484.678889	30208.048974	30.880410
485.059600	30251.771003	30.885428
485.519505	30283.210949	30.890445
486.237993	30337.778289	30.895463
486.536253	30377.164387	30.900480
486.878188	30442.745958	30.905498
487.354099	30474.746295	30.910516
487.995607	30520.254934	30.915533
488.362308	30583.013710	30.920551
489.038776	30619.667057	30.925568
489.486260	30669.113080	30.930586
489.579803	30719.468059	30.935604
490.407778	30761.616595	30.940621
490.517938	30814.086907	30.945639
491.004957	30866.738545	30.950656
491.767264	30908.480444	30.955674
492.000625	30974.207132	30.960692
492.851748	31025.784372	30.965709
493.178614	31079.536303	30.970727
493.343613	31126.239832	30.975744
494.124113	31185.389190	30.980762
494.747826	31241.257046	30.985780
495.510405	31282.057729	30.990797
496.034531	31327.365267	30.995815
496.373850	31382.361403	31.000832
497.362565	31419.744829	31.005850
497.502690	31484.495226	31.010868
498.248274	31526.316849	31.015885
498.487166	31580.785568	31.020903
499.233091	31619.787822	31.025920
499.772969	31663.393070	31.030938
500.127042	31718.463644	31.035956
500.465607	31763.415566	31.040973
501.319760	31819.937963	31.045991
501.762733	31860.043863	31.051008
502.315388	31902.320023	31.056026
502.548607	31954.862443	31.061044
503.286714	31995.181574	31.066061
503.736232	32050.914519	31.071079
504.096372	32103.936865	31.076096
504.619015	32143.904394	31.081114
504.665363	32204.682576	31.086132
505.288842	32249.306433	31.091149
505.879722	32296.786703	31.096167
506.189668	32368.574891	31.101184
507.305777	32418.666344	31.106202
507.568900	32470.977786	31.111220
508.145672	32515.192272	31.116237
508.760622	32562.972835	31.121255
509.231243	32617.237268	31.126272
510.188203	32664.490340	31.131290
510.266162	32718.399278	31.136308
511.168542	32762.765598	31.141325
511.682426	32812.149410	31.146343
512.051869	32850.884182	31.151360
512.608648	32901.260384	31.156378
512.904452	32955.932404	31.161396
513.508896	32984.262254	31.166413
513.853270	33035.430708	31.171431
513.936283	33085.021735	31.176448
515.087765	33131.739619	31.181466
515.770713	33190.985809	31.186484
515.970690	33234.843563	31.191501
516.629430	33274.159710	31.196519
516.674561	33325.167103	31.201536
517.440680	33370.213570	31.206554
517.804898	33421.778162	31.211572
518.181089	33462.896519	31.216589
518.555843	33508.820160	31.221607
519.296355	33560.313511	31.226624
519.635851	33606.261854	31.231642
519.742557	33666.326710	31.236660
520.383593	33706.367191	31.241677
520.953031	33764.260815	31.246695
521.391268	33830.647211	31.251712
522.063517	33877.271109	31.256730
522.624566	33936.310883	31.261748
522.786996	33989.710374	31.266765
523.516697	34049.362621	31.271783
523.979905	34112.104231	31.276800
525.010407	34159.418701	31.281818
524.880719	34214.230179	31.286836
525.389602	34277.553124	31.291853
525.785712	34331.150814	31.296871
526.526869	34398.983684	31.301888
527.239217	34450.515235	31.306906
527.625539	34512.340650	31.311924
528.329969	34571.144774	31.316941
528.625302	34627.028832	31.321959
529.111022	34691.058460	31.326976
530.053673	34751.494966	31.331994
530.782118	34823.358757	31.337012
531.382453	34875.237669	31.342029
532.296324	34927.687234	31.347047
532.531100	34978.700530	31.352064
532.896794	35034.018237	31.357082
533.561499	35086.172110	31.362100
534.174718	35145.516909	31.367117
534.840217	35202.090601	31.372135
535.365904	35253.507917	31.377152
535.992896	35301.817606	31.382170
536.330936	35357.387079	31.387188
536.656813	35409.854054	31.392205
537.762849	35459.676123	31.397223
537.877080	35512.859376	31.402240
538.460624	35569.010600	31.407258
538.830776	35633.010588	31.412276
539.208904	35687.487093	31.417293
540.254050	35743.617065	31.422311
540.430666	35808.324453	31.427328
541.532718	35847.304070	31.432346
541.898325	35907.119743	31.437364
542.226232	35961.547908	31.442381
543.013635	36006.242569	31.447399
543.390543	36072.177682	31.452416
543.784763	36119.779559	31.457434
544.408731	36171.411334	31.462452
545.128241	36234.903148	31.467469
545.715932	36288.165937	31.472487
545.910192	36349.957224	31.477504
546.612577	36418.137747	31.482522
547.279538	36456.238143	31.487540
547.779024	36507.624652	31.492557
548.382926	36565.128484	31.497575
548.554493	36630.737056	31.502592
549.033052	36674.267421	31.507610
549.825341	36740.537907	31.512628
550.494204	36800.359172	31.517645
551.063631	36855.681316	31.522663
551.189510	36918.591538	31.527680
552.067461	36977.286610	31.532698
552.627265	37028.076849	31.537716
553.238098	37083.323539	31.542733
554.117863	37127.481240	31.547751
554.512739	37180.675277	31.552768
554.771338	37219.037016	31.557786
555.113869	37278.341616	31.562804
555.518369	37331.793781	31.567821
556.008301	37381.546103	31.572839
557.004311	37436.056762	31.577856
556.929103	37495.244005	31.582874
557.736588	37560.553471	31.587892
557.986749	37620.942162	31.592909
558.786916	37676.679257	31.597927
559.303976	37738.417664	31.602944
560.039501	37793.147087	31.607962
560.750464	37858.643314	31.612980
561.030500	37923.372508	31.617997
561.710431	37976.144449	31.623015
561.976643	38039.377449	31.628032
563.084711	38103.016299	31.633050
563.383714	38157.252205	31.638068
563.770211	38227.460951	31.643085
564.711835	38278.523180	31.648103
564.896115	38337.387524	31.653120
565.627366	38409.281903	31.658138
566.562553	38480.739859	31.663156
566.652113	38543.230495	31.668173
567.593383	38602.103479	31.673191
567.867855	38663.838261	31.678208
568.304666	38726.028409	31.683226
569.297394	38795.808888	31.688244
569.572303	38854.318954	31.693261
570.415540	38911.677745	31.698279
570.844217	38972.358454	31.703296
571.352680	39026.070466	31.708314
571.816295	39096.181417	31.713332
572.440444	39168.651606	31.718349
573.435426	39226.898125	31.723367
574.238561	39297.196866	31.728384
574.491859	39359.506109	31.733402
575.315558	39413.979192	31.738420
575.885803	39472.324512	31.743437
576.528751	39524.157409	31.748455
577.283377	39593.977751	31.753472
577.752654	39647.653170	31.758490
578.438738	39708.605506	31.763508
578.527788	39776.633423	31.768525
579.645516	39831.871002	31.773543
579.834922	39888.019341	31.778560
580.290397	39951.949240	31.783578
580.949306	40010.256820	31.788596
581.605002	40071.139040	31.793613
582.547293	40128.340076	31.798631
582.723320	40190.461423	31.803648
583.391621	40261.726721	31.808666
584.197514	40317.811238	31.813684
584.450358	40376.771559	31.818701
585.290276	40434.691437	31.823719
585.870966	40508.007712	31.828736
586.293535	40568.118306	31.833754
586.903912	40617.005402	31.838772
587.434202	40688.243112	31.843789
588.039259	40746.706557	31.848807
588.321293	40808.174285	31.853824
588.566676	40876.282333	31.858842
589.492084	40934.525347	31.863860
589.957845	41015.444429	31.868877
590.382279	41074.632738	31.873895
591.276454	41138.130575	31.878912
591.289017	41198.598044	31.883930
592.256616	41252.869773	31.888948
592.964836	41322.393005	31.893965
593.819269	41380.085427	31.898983
594.153310	41449.667665	31.904000
594.505416	41507.983016	31.909018
594.848621	41568.026562	31.914036
595.609405	41635.335230	31.919053
596.030628	41697.112534	31.924071
596.394811	41772.870349	31.929088
597.448606	41846.439567	31.934106
597.823960	41902.861213	31.939124
598.451739	41983.688913	31.944141
599.523266	42048.186229	31.949159
600.006864	42125.210498	31.954176
600.075014	42190.908978	31.959194
601.289043	42255.093637	31.964212
601.486235	42330.019333	31.969229
602.236729	42393.739374	31.974247
602.798257	42460.689624	31.979264
603.428456	42534.567830	31.984282
603.970606	42606.625821	31.989300
604.797099	42678.715415	31.994317
605.553943	42746.483496	31.999335
606.135447	42819.592300	32.004352
606.454778	42890.130144	32.009370
607.615279	42951.270196	32.014388
608.206713	43030.899326	32.019405
608.993785	43092.262705	32.024423
609.511965	43150.341331	32.029440
609.996833	43230.670986	32.034458
610.606194	43292.897676	32.039476
611.092625	43361.317208	32.044493
611.493549	43432.470195	32.049511
612.368000	43507.755549	32.054528
612.810483	43567.611870	32.059546
613.600055	43635.592604	32.064564
614.251537	43712.216582	32.069581
614.699497	43782.351272	32.074599
615.140896	43851.462501	32.079616
615.743549	43941.934809	32.084634
616.916136	44009.464527	32.089652
617.121020	44084.907300	32.094669
617.989860	44156.248663	32.099687
618.688192	44218.527264	32.104704
619.011319	44288.594540	32.109722
619.727008	44350.896095	32.114740
620.103178	44431.936586	32.119757
620.759131	44500.952972	32.124775
621.188138	44583.301450	32.129792
622.005783	44656.309728	32.134810
622.810967	44730.237409	32.139828
623.325326	44807.829141	32.144845
623.816798	44878.030040	32.149863
624.701407	44948.555456	32.154880
625.248282	45028.660478	32.159898
626.248015	45099.636441	32.164916
626.683115	45180.120075	32.169933
627.348907	45242.583745	32.174951
627.980007	45318.052486	32.179968
628.692694	45383.855540	32.184986
629.571645	45446.450867	32.190004
630.033234	45517.278376	32.195021
630.729483	45591.320846	32.200039
631.253898	45660.424662	32.205056
632.030883	45735.517709	32.210074
632.611817	45796.218634	32.215092
633.325069	45865.217594	32.220109
633.966658	45920.823311	32.225127
634.451793	45982.317832	32.230144
634.843625	46048.394489	32.235162
635.689312	46107.251886	32.240180
636.033612	46174.487688	32.245197
636.465440	46236.693439	32.250215
636.956989	46308.100739	32.255232
637.369702	46383.455427	32.260250
638.032807	46454.589606	32.265268
639.017308	46535.801784	32.270285
639.405380	46604.702106	32.275303
640.019742	46676.426621	32.280320
640.740704	46757.294972	32.285338
641.245254	46830.169557	32.290356
641.976916	46909.588077	32.295373
642.469846	46985.982362	32.300391
643.310825	47056.900791	32.305408
644.052838	47144.795706	32.310426
644.869368	47212.523677	32.315444
645.411612	47296.869779	32.320461
646.172460	47368.339469	32.325479
647.017688	47442.801195	32.330496
647.362977	47534.479654	32.335514
647.937124	47600.064134	32.340532
648.749530	47678.220070	32.345549
649.375899	47754.083600	32.350567
650.160449	47820.635346	32.355584
650.289769	47910.280384	32.360602
651.323423	47983.809683	32.365620
652.006116	48060.899086	32.370637
652.181003	48142.180540	32.375655
653.199834	48220.717237	32.380672
653.977464	48299.000954	32.385690
654.902887	48377.609759	32.390708
655.372751	48462.901529	32.395725
655.882907	48534.939252	32.400743
656.862492	48614.173056	32.405760
657.377455	48688.399547	32.410778
658.282714	48771.991991	32.415796
658.787329	48839.691401	32.420813
659.377177	48921.764752	32.425831
660.406252	49002.624460	32.430848
661.024071	49085.592423	32.435866
661.484667	49154.286640	32.440884
662.267717	49224.588202	32.445901
662.747840	49305.484333	32.450919
663.508934	49373.607016	32.455936
664.060400	49459.996923	32.460954
665.054422	49533.176778	32.465972
666.032055	49606.979474	32.470989
666.278020	49693.025829	32.476007
667.238382	49759.568337	32.481024
667.614771	49840.596481	32.486042
668.583713	49914.009248	32.491060
669.003286	49993.594927	32.496077
669.776647	50056.535839	32.501095
670.420952	50132.486689	32.506112
670.865219	50200.863905	32.511130
671.786568	50282.649766	32.516148
672.521246	50363.579347	32.521165
673.089883	50440.131486	32.526183
673.765530	50510.466450	32.531200
674.484193	50584.414068	32.536218
675.211822	50663.808286	32.541236
675.683579	50720.977168	32.546253
676.198686	50805.321443	32.551271
676.838437	50881.636124	32.556288
677.458410	50960.839418	32.561306
678.314730	51023.491569	32.566324
679.037124	51098.161563	32.571341
679.605307	51171.590467	32.576359
680.110659	51236.436817	32.581376
680.706760	51314.942716	32.586394
681.226880	51378.781088	32.591412
682.124882	51461.258133	32.596429
683.047116	51536.670193	32.601447
683.603033	51605.489647	32.606464
684.073585	51690.204782	32.611482
684.861227	51765.461490	32.616500
685.494795	51837.047266	32.621517
685.798705	51914.923896	32.626535
686.472356	51999.639987	32.631552
687.374173	52097.488481	32.636570
687.828150	52172.267233	32.641588
688.682709	52245.831853	32.646605
689.414961	52331.324603	32.651623
690.442838	52412.348286	32.656640
690.749297	52505.305472	32.661658
691.521550	52575.580931	32.666676
692.290703	52672.440165	32.671693
692.707159	52752.156003	32.676711
693.880176	52829.038989	32.681728
694.605340	52910.307965	32.686746
695.265611	52995.257561	32.691764
696.077547	53078.000584	32.696781
696.952928	53165.119220	32.701799
697.669444	53248.909242	32.706816
698.471428	53330.775128	32.711834
699.380400	53401.993507	32.716852
700.025990	53474.088646	32.721869
700.250546	53553.514527	32.726887
701.085741	53637.186098	32.731904
701.631447	53712.170548	32.736922
702.276819	53797.802481	32.741940
702.944390	53878.077653	32.746957
703.515376	53968.360370	32.751975
704.639623	54052.842451	32.756992
705.260140	54136.302613	32.762010
705.874340	54219.529916	32.767028
706.769050	54304.979093	32.772045
706.916918	54395.810649	32.777063
707.974828	54478.741561	32.782080
708.959299	54565.285072	32.787098
709.650627	54650.001619	32.792116
710.420037	54722.910193	32.797133
710.808086	54812.769138	32.802151
712.031603	54894.631391	32.807168
712.415109	54980.928798	32.812186
713.255308	55066.503170	32.817204
713.995943	55139.936464	32.822221
714.560600	55232.655120	32.827239
715.479307	55317.597910	32.832256
716.014712	55396.759795	32.837274
716.490385	55480.633411	32.842292
717.218171	55554.911696	32.847309
717.889385	55655.253898	32.852327
718.792497	55739.675363	32.857344
719.596315	55832.219670	32.862362
720.150750	55920.322692	32.867380
720.849645	55997.929432	32.872397
721.208096	56079.893261	32.877415
722.410215	56166.940129	32.882432
723.187316	56255.034830	32.887450
723.727365	56344.477035	32.892468
724.497871	56433.332879	32.897485
725.232173	56513.948260	32.902503
725.807677	56599.417691	32.907520
726.789725	56669.767383	32.912538
727.237254	56757.434548	32.917556
728.349919	56828.909781	32.922573
728.471233	56913.476805	32.927591
729.438421	57005.208946	32.932608
730.375684	57073.142845	32.937626
730.653527	57158.698854	32.942644
731.585115	57236.064307	32.947661
732.420865	57328.356231	32.952679
733.077154	57410.828590	32.957696
733.871624	57496.456793	32.962714
734.520769	57587.006787	32.967732
735.331379	57668.683710	32.972749
735.950534	57752.295967	32.977767
736.598644	57841.714160	32.982784
737.417272	57926.036294	32.987802
737.913020	58014.928348	32.992820
739.017415	58101.358278	32.997837
739.554724	58200.023185	33.002855
740.484601	58288.841932	33.007872
740.715904	58371.833503	33.012890
741.702038	58478.151020	33.017908
742.720085	58555.405893	33.022925
743.343342	58652.103408	33.027943
744.086140	58734.547746	33.032960
744.484297	58830.091290	33.037978
745.585944	58931.107627	33.042996
746.473346	59027.277902	33.048013
746.741916	59121.779531	33.053031
747.884774	59214.416654	33.058048
748.925726	59311.576731	33.063066
749.254490	59412.703439	33.068084
750.097504	59500.717373	33.073101
750.807267	59588.360053	33.078119
751.536469	59692.482424	33.083136
752.598814	59778.222313	33.088154
753.303979	59872.721777	33.093172
754.330076	59959.322488	33.098189
755.093224	60060.586404	33.103207
755.679753	60147.800976	33.108224
756.589752	60243.288887	33.113242
757.449414	60333.904761	33.118260
758.174010	60417.041254	33.123277
758.524102	60506.015842	33.128295
759.371733	60606.123075	33.133312
759.989343	60695.138744	33.138330
760.629422	60798.007454	33.143348
761.765360	60896.076789	33.148365
762.376243	60988.696324	33.153383
763.059290	61077.734780	33.158400
763.828833	61174.007904	33.163418
764.398755	61273.040921	33.168436
765.268662	61373.280717	33.173453
766.103398	61476.071133	33.178471
766.623549	61571.675889	33.183488
768.094010	61674.475193	33.188506
768.877689	61768.697448	33.193524
769.543593	61870.186602	33.198541
770.451437	61959.826056	33.203559
770.771324	62041.891961	33.208576
771.863808	62140.314878	33.213594
772.538847	62237.290611	33.218612
773.300110	62330.467681	33.223629
773.953363	62413.951249	33.228647
774.887971	62514.907195	33.233664
775.912585	62602.789833	33.238682
776.427867	62701.754821	33.243700
777.052021	62783.383040	33.248717
777.858457	62869.933410	33.253735
778.534562	62958.384646	33.258752
779.756889	63039.679477	33.263770
780.205253	63134.750736	33.268788
780.874837	63221.671937	33.273805
781.622421	63311.809823	33.278823
782.277787	63411.300119	33.283840
783.068723	63497.570216	33.288858
783.676382	63601.506509	33.293876
784.220641	63677.325960	33.298893
784.980910	63776.453093	33.303911
785.990436	63874.028543	33.308928
786.736160	63979.945295	33.313946
787.231931	64078.944112	33.318964
788.026161	64174.978083	33.323981
789.019266	64280.110329	33.328999
789.799785	64384.269698	33.334016
790.663286	64486.840116	33.339034
791.383637	64592.472201	33.344052
792.208884	64696.891758	33.349069
793.064063	64800.680296	33.354087
793.384086	64913.460756	33.359104
794.390226	65015.327241	33.364122
795.475991	65119.752070	33.369140
795.962887	65232.691424	33.374157
796.746876	65338.557246	33.379175
797.807401	65448.856309	33.384192
798.773557	65544.476043	33.389210
799.877288	65658.086771	33.394228
800.858445	65768.361666	33.399245
801.716292	65866.468743	33.404263
802.436080	65972.461228	33.409280
803.070076	66070.211607	33.414298
803.642427	66174.518577	33.419316
804.429226	66283.844793	33.424333
805.653555	66379.940083	33.429351
806.353638	66498.765165	33.434368
806.933368	66594.772262	33.439386
808.042437	66698.668100	33.444404
808.525994	66811.918900	33.449421
809.785516	66903.781240	33.454439
810.083329	67014.694050	33.459456
811.100370	67113.401486	33.464474
811.968577	67226.942125	33.469492
812.524768	67340.449814	33.474509
813.764880	67441.143360	33.479527
814.203048	67535.327322	33.484544
815.313475	67648.186070	33.489562
816.271878	67762.075858	33.494580
816.411480	67864.944209	33.499597
817.667195	67970.968697	33.504615
818.290907	68091.117460	33.509632
819.155920	68184.933036	33.514650
819.907556	68305.062765	33.519668
820.945501	68406.716196	33.524685
822.175636	68506.446704	33.529703
822.790677	68625.940800	33.534720
823.998177	68729.759793	33.539738
824.395832	68820.035328	33.544756
825.080669	68935.163540	33.549773
826.333160	69037.026471	33.554791
826.850839	69145.666162	33.559808
827.733076	69245.466659	33.564826
828.654153	69352.587676	33.569844
829.678687	69454.551264	33.574861
830.249531	69565.482941	33.579879
830.760671	69672.200888	33.584896
831.820248	69755.613281	33.589914
832.419561	69856.410254	33.594932
833.077287	69958.002662	33.599949
834.137920	70058.645861	33.604967
834.795314	70174.220782	33.609984
835.439085	70262.531438	33.615002
836.273385	70362.565355	33.620020
837.005485	70478.129922	33.625037
838.177426	70578.137122	33.630055
838.755355	70694.701973	33.635072
839.927734	70800.295137	33.640090
840.648129	70912.684573	33.645108
841.284179	71009.611105	33.650125
842.238746	71120.723596	33.655143
842.908326	71233.882265	33.660160
843.915182	71337.882382	33.665178
844.784290	71457.242009	33.670196
845.141299	71564.941691	33.675213
846.083209	71671.359689	33.680231
846.797768	71804.917547	33.685248
847.734096	71913.072546	33.690266
848.866487	72045.097006	33.695284
849.462260	72162.108849	33.700301
850.208460	72273.195498	33.705319
851.386559	72392.827610	33.710336
852.317027	72504.165017	33.715354
852.754231	72630.956337	33.720372
853.751882	72760.776291	33.725389
854.824930	72866.456611	33.730407
855.689343	72984.582609	33.735424
856.588516	73104.033616	33.740442
857.386384	73220.891820	33.745460
858.495178	73338.841798	33.750477
859.121672	73460.591663	33.755495
860.012035	73575.372357	33.760512
861.281325	73700.366538	33.765530
861.934790	73826.154379	33.770548
862.734885	73946.333983	33.775565
864.368794	74052.665832	33.780583
864.922645	74178.496259	33.785600
865.496718	74290.504922	33.790618
866.800791	74399.245768	33.795636
867.175471	74520.216552	33.800653
867.996482	74641.117992	33.805671
868.960820	74761.313527	33.810688
870.453635	74877.740809	33.815706
870.932093	74994.682097	33.820724
871.772953	75116.279239	33.825741
872.686322	75231.975433	33.830759
873.644523	75354.619300	33.835776
874.410483	75474.481732	33.840794
875.256202	75591.976119	33.845812
876.314364	75702.356790	33.850829
877.179456	75825.346717	33.855847
877.856289	75943.591106	33.860864
878.890005	76064.680953	33.865882
880.102768	76172.898548	33.870900
880.602196	76290.032157	33.875917
881.475622	76398.113770	33.880935
882.248221	76525.377634	33.885952
883.402234	76653.671787	33.890970
884.224556	76760.939445	33.895988
884.851613	76881.754576	33.901005
885.983499	76995.511239	33.906023
886.765472	77120.382197	33.911040
887.539902	77237.160114	33.916058
888.481795	77350.073916	33.921076
889.490424	77470.793896	33.926093
890.377658	77575.394303	33.931111
891.535542	77691.759409	33.936128
892.017584	77796.500112	33.941146
892.907084	77905.180569	33.946164
893.687517	78024.177832	33.951181
894.556269	78131.430917	33.956199
895.473382	78246.746597	33.961216
896.314597	78352.839366	33.966234
897.234458	78468.687617	33.971252
897.746527	78592.416688	33.976269
898.571520	78708.648188	33.981287
899.146451	78831.190305	33.986304
900.041117	78954.088299	33.991322
900.987085	79090.331669	33.996340
901.792660	79222.670359	34.001357
903.213357	79347.324708	34.006375
903.814647	79476.009950	34.011392
904.923507	79611.584258	34.016410
905.707759	79731.639789	34.021428
906.642650	79866.051685	34.026445
907.507253	79992.037569	34.031463
908.519083	80119.027176	34.036480
909.536476	80253.795429	34.041498
910.476658	80377.237360	34.046516
911.054316	80512.012364	34.051533
912.003892	80643.309026	34.056551
913.205153	80772.831172	34.061568
913.881066	80909.087702	34.066586
915.375735	81044.025747	34.071604
915.836747	81183.662042	34.076621
916.753679	81311.584130	34.081639
917.701624	81433.319071	34.086656
918.395697	81575.809535	34.091674
919.408622	81706.315709	34.096692
920.545484	81842.770649	34.101709
921.457457	81974.218777	34.106727
922.584652	82117.150955	34.111744
923.672222	82257.746074	34.116762
924.488045	82386.119644	34.121780
925.396669	82527.314279	34.126797
926.197937	82650.027695	34.131815
927.265088	82795.430741	34.136832
927.969824	82931.274376	34.141850
929.184644	83059.233737	34.146868
930.099523	83197.845929	34.151885
930.920477	83334.915008	34.156903
932.003906	83465.000092	34.161920
933.277653	83601.429370	34.166938
934.118771	83726.117817	34.171956
935.002108	83866.017940	34.176973
935.847923	83997.219673	34.181991
936.861576	84135.491494	34.187008
937.926806	84275.846633	34.192026
939.028641	84395.834210	34.197044
939.778579	84532.856778	34.202061
940.826396	84662.116565	34.207079
941.822713	84782.717824	34.212096
942.924954	84924.704927	34.217114
943.779098	85044.049730	34.222132
945.071848	85178.291359	34.227149
945.502784	85305.230359	34.232167
946.745459	85435.274072	34.237184
947.126396	85569.014027	34.242202
948.471181	85696.305847	34.247220
949.262464	85828.892981	34.252237
949.954300	85958.074901	34.257255
951.054534	86076.257626	34.262272
952.000714	86219.504672	34.267290
952.870167	86351.701788	34.272308
953.340558	86479.666163	34.277325
954.558159	86598.973113	34.282343
955.756942	86722.858141	34.287360
956.780292	86844.971710	34.292378
957.578814	86968.312181	34.297396
958.610679	87105.632209	34.302413
958.897169	87232.019280	34.307431
960.070598	87367.582252	34.312448
960.983026	87498.105051	34.317466
962.113734	87626.782079	34.322484
963.164867	87772.871601	34.327501
963.833060	87908.642896	34.332519
964.920463	88040.205201	34.337536
965.842843	88175.785852	34.342554
967.474191	88303.703115	34.347572
967.891386	88444.496589	34.352589
968.662578	88577.492137	34.357607
969.779609	88719.875517	34.362624
970.625430	88868.587884	34.367642
971.621651	88994.871361	34.372660
972.800303	89142.493788	34.377677
973.405327	89291.271314	34.382695
974.786188	89434.440564	34.387712
975.269915	89574.519259	34.392730
976.447752	89716.517679	34.397748
977.517190	89864.832468	34.402765
978.578378	90020.639354	34.407783
979.617052	90160.912718	34.412800
980.177504	90318.548509	34.417818
981.186736	90456.293126	34.422836
982.197304	90604.696829	34.427853
983.296152	90762.567491	34.432871
984.285704	90910.925296	34.437888
985.113194	91066.368618	34.442906
986.409685	91210.484745	34.447924
987.376010	91366.237395	34.452941
988.213989	91513.620631	34.457959
989.770243	91670.118973	34.462976
990.667259	91818.026763	34.467994
991.844493	91960.149909	34.473012
992.805116	92106.743683	34.478029
993.693148	92259.331887	34.483047
994.848762	92404.350274	34.488064
995.656750	92558.942412	34.493082
996.638429	92692.683646	34.498100
997.672313	92845.758928	34.503117
998.709430	93000.114623	34.508135
999.624039	93141.714018	34.513152
1000.932952	93294.279507	34.518170
1002.092515	93447.819761	34.523188
1002.711422	93592.243348	34.528205
1004.195945	93732.628154	34.533223
1005.122226	93883.165077	34.538240
1005.993168	94035.688733	34.543258
1007.079697	94168.228494	34.548276
1007.799617	94321.195486	34.553293
1008.795285	94468.340076	34.558311
1010.268093	94610.771442	34.563328
1011.061933	94760.293975	34.568346
1012.369816	94911.219788	34.573364
1013.262386	95045.910486	34.578381
1014.003577	95201.502334	34.583399
1015.227717	95341.643650	34.588416
1016.076795	95491.592017	34.593434
1016.929876	95633.972979	34.598452
1018.250049	95792.202431	34.603469
1019.135687	95941.247235	34.608487
1020.124596	96072.821652	34.613504
1021.057657	96209.539186	34.618522
1021.849643	96349.118862	34.623540
1023.168894	96488.210966	34.628557
1023.882293	96632.012704	34.633575
1024.806421	96766.439647	34.638592
1025.721005	96917.816986	34.643610
1026.957987	97054.351158	34.648628
1027.614867	97201.219356	34.653645
1028.521165	97358.025639	34.658663
1029.794235	97509.222911	34.663680
1030.528866	97658.743143	34.668698
1032.185022	97808.259244	34.673716
1032.755863	97954.928890	34.678733
1034.020826	98111.657379	34.683751
1035.065544	98267.571767	34.688768
1035.683709	98428.763940	34.693786
1036.914942	98578.223406	34.698804
1038.012067	98731.634470	34.703821
1038.826019	98891.036196	34.708839
1040.143655	99049.941505	34.713856
1040.974573	99222.704028	34.718874
1042.457077	99369.478279	34.723892
1043.079650	99536.950613	34.728909
1044.044562	99697.448307	34.733927
1045.242878	99846.677944	34.738944
1046.123459	100014.708202	34.743962
1047.517680	100177.410354	34.748980
1048.593933	100344.334080	34.753997
1049.619132	100509.808710	34.759015
1050.631834	100671.495453	34.764032
1051.465071	100838.003355	34.769050
1052.656436	101009.400456	34.774068
1053.973037	101160.696797	34.779085
1054.957406	101332.685835	34.784103
1056.050045	101492.715969	34.789120
1056.948768	101660.244734	34.794138
1058.212141	101827.806011	34.799156
1059.148926	101986.709225	34.804173
1060.212800	102149.739158	34.809191
1061.279424	102316.737838	34.814208
1062.769661	102494.371755	34.819226
1063.978650	102659.042376	34.824244
1064.993271	102820.067423	34.829261
1065.770198	102980.712066	34.834279
1066.997410	103137.774956	34.839296
1068.057146	103312.615243	34.844314
1069.187297	103475.577926	34.849332
1069.981450	103643.500787	34.854349
1071.199556	103817.114418	34.859367
1071.947029	103981.280597	34.864384
1073.637871	104151.588771	34.869402
1074.597104	104310.892636	34.874420
1075.692540	104478.468211	34.879437
1076.832394	104638.886491	34.884455
1078.141921	104807.698126	34.889472
1079.198094	104977.336402	34.894490
1079.940943	105140.076175	34.899508
1081.302510	105296.405407	34.904525
1082.325110	105478.211221	34.909543
1083.336993	105634.609439	34.914560
1084.562719	105797.466966	34.919578
1085.368120	105953.353746	34.924596
1086.796726	106108.509674	34.929613
1087.835111	106289.328318	34.934631
1089.167118	106433.545327	34.939648
1090.253332	106598.685574	34.944666
1090.690498	106760.783547	34.949684
1092.162030	106917.432688	34.954701
1092.839995	107070.351975	34.959719
1094.367369	107233.562208	34.964736
1095.070952	107373.950648	34.969754
1096.166712	107523.940770	34.974772
1097.404288	107686.057275	34.979789
1098.437116	107855.764222	34.984807
1099.323866	107991.371278	34.989824
1100.413923	108154.540205	34.994842
1101.434661	108314.930988	34.999860
1102.259258	108485.459822	35.004877
1103.400013	108664.626393	35.009895
1104.585761	108811.425096	35.014912
1105.769999	108993.072010	35.019930
1106.790670	109163.548100	35.024948
1108.193345	109329.640955	35.029965
1109.060876	109504.213317	35.034983
1109.911784	109665.182179	35.040000
1111.123724	109845.662500	35.045018
1111.974187	110019.149498	35.050036
1113.214839	110204.572895	35.055053
1114.292942	110382.794260	35.060071
1115.646302	110552.197793	35.065088
1116.770738	110722.906137	35.070106
1117.891140	110911.585875	35.075124
1119.438919	111084.715292	35.080141
1120.386375	111274.527344	35.085159
1121.322499	111443.163445	35.090176
1122.611214	111621.155138	35.095194
1123.748301	111795.886817	35.100212
1125.092362	111967.264247	35.105229
1125.786818	112154.964628	35.110247
1127.120060	112340.701702	35.115264
1128.378162	112509.926523	35.120282
1129.445239	112696.201707	35.125300
1130.494951	112879.386070	35.130317
1131.716152	113058.828558	35.135335
1132.846847	113240.442129	35.140352
1134.463330	113420.458650	35.145370
1134.967527	113608.678301	35.150388
1136.891736	113782.953938	35.155405
1137.509608	113967.847465	35.160423
1139.091367	114142.153066	35.165440
1140.384442	114320.715408	35.170458
1141.540483	114511.944970	35.175476
1142.784134	114666.419142	35.180493
1143.913268	114859.899619	35.185511
1145.086850	115031.571854	35.190528
1146.197651	115200.261486	35.195546
1147.024784	115377.760417	35.200564
1148.297173	115555.672460	35.205581
1149.692062	115725.524926	35.210599
1150.331574	115909.803328	35.215616
1151.590227	116081.695416	35.220634
1153.054349	116264.058106	35.225652
1154.329375	116444.523383	35.230669
1155.114814	116621.641588	35.235687
1155.853265	116805.452311	35.240704
1157.555165	116989.201893	35.245722
1158.399562	117163.243947	35.250740
1159.859812	117344.432908	35.255757
1161.019526	117534.168052	35.260775
1161.990742	117710.031955	35.265792
1163.095361	117890.010806	35.270810
1164.547354	118077.901782	35.275828
1165.547297	118247.954341	35.280845
1166.667386	118433.590510	35.285863
1167.754833	118607.119153	35.290880
1169.375532	118775.465981	35.295898
1170.181053	118947.391336	35.300916
1171.472478	119108.637152	35.305933
1172.225035	119288.893366	35.310951
1173.202261	119456.735067	35.315968
1174.466456	119621.310671	35.320986
1175.727071	119805.536181	35.326004
1176.962919	119982.117520	35.331021
1177.743329	120161.333304	35.336039
1178.899540	120339.387500	35.341056
1180.407467	120514.584077	35.346074
1181.202041	120701.626764	35.351092
1182.691821	120880.899726	35.356109
1183.654845	121066.941046	35.361127
1184.937485	121250.256639	35.366144
1186.441303	121430.760395	35.371162
1186.663260	121627.715553	35.376180
1188.195940	121813.316053	35.381197
1189.827586	121997.125974	35.386215
1190.745937	122195.180071	35.391232
1192.335929	122391.379409	35.396250
1193.565585	122579.288985	35.401268
1194.677634	122768.892376	35.406285
1195.609872	122959.438195	35.411303
1196.567085	123156.387352	35.416320
1198.556339	123342.101152	35.421338
1199.434396	123544.709833	35.426356
1200.799231	123728.163595	35.431373
1202.292002	123925.438656	35.436391
1203.206539	124114.051786	35.441408
1204.425599	124308.250791	35.446426
1205.264803	124509.487629	35.451444
1206.897591	124693.474730	35.456461
1208.374729	124887.280903	35.461479
1209.246251	125079.406712	35.466496
1210.714411	125278.303414	35.471514
1211.660928	125476.166333	35.476532
1213.299241	125662.986064	35.481549
1214.324746	125864.200449	35.486567
1215.271993	126060.645179	35.491584
1216.917572	126254.076256	35.496602
1217.930563	126452.834252	35.501620
1219.458411	126637.024165	35.506637
1220.492646	126836.338908	35.511655
1221.812695	127036.992756	35.516672
1223.257711	127214.854700	35.521690
1224.163977	127424.963640	35.526708
1225.432277	127622.063331	35.531725
1226.610373	127823.225312	35.536743
1228.000295	128016.285964	35.541760
1229.163956	128209.357552	35.546778
1230.385459	128412.799302	35.551796
1231.405682	128610.158169	35.556813
1233.127694	128809.323923	35.561831
1234.139649	129007.764389	35.566848
1235.914253	129194.718239	35.571866
1236.823950	129399.393512	35.576884
1237.758787	129590.363015	35.581901
1239.245689	129787.096053	35.586919
1240.384702	129980.572915	35.591936
1241.975962	130181.148560	35.596954
1243.139042	130387.615981	35.601972
1244.036641	130568.381821	35.606989
1245.319647	130766.470842	35.612007
1246.155872	130961.598234	35.617024
1247.640445	131166.572611	35.622042
1248.810905	131378.144306	35.627060
1250.027644	131574.610613	35.632077
1251.342698	131766.342320	35.637095
1252.633637	131952.115055	35.642112
1254.018765	132125.489819	35.647130
1255.363694	132320.772080	35.652148
1256.533703	132504.954644	35.657165
1257.666498	132692.163720	35.662183
1258.776343	132880.113133	35.667200
1260.180840	133058.297594	35.672218
1261.135881	133262.895216	35.677236
1262.504200	133461.845963	35.682253
1263.923232	133651.031836	35.687271
1265.182857	133844.976480	35.692288
1266.306583	134039.679209	35.697306
1267.527618	134242.856595	35.702324
1268.531786	134439.635425	35.707341
1270.046678	134635.117002	35.712359
1271.288081	134848.813344	35.717376
1272.477305	135049.423430	35.722394
1273.743799	135255.567595	35.727412
1274.892390	135454.434699	35.732429
1275.884943	135664.633488	35.737447
1277.527366	135889.591051	35.742464
1279.171398	136082.101991	35.747482
1280.279723	136297.031511	35.752500
1281.075088	136510.970467	35.757517
1282.957400	136725.260557	35.762535
1283.531514	136940.251334	35.767552
1285.508553	137160.061418	35.772570
1286.402507	137373.087960	35.777588
1287.696573	137581.091029	35.782605
1289.053784	137796.217001	35.787623
1290.124345	138018.812602	35.792640
1291.424589	138231.297249	35.797658
1292.878404	138458.098876	35.802676
1294.116926	138680.036816	35.807693
1295.831432	138894.134749	35.812711
1297.056008	139119.046504	35.817728
1298.444624	139341.649350	35.822746
1299.494178	139555.600559	35.827764
1300.813577	139776.820316	35.832781
1302.158754	140004.166687	35.837799
1303.263327	140223.455080	35.842816
1304.778048	140447.845449	35.847834
1306.331098	140672.205486	35.852852
1307.239337	140900.779378	35.857869
1308.264020	141121.543834	35.862887
1309.305240	141348.411119	35.867904
1311.235704	141579.315653	35.872922
1312.605033	141808.012014	35.877940
1313.883476	142042.485507	35.882957
1315.529264	142267.016080	35.887975
1316.679801	142499.557318	35.892992
1318.354976	142719.592611	35.898010
1319.267752	142946.538178	35.903028
1320.742385	143178.219628	35.908045
1322.459538	143392.273621	35.913063
1323.515503	143625.545686	35.918080
1324.844283	143847.734333	35.923098
1325.863265	144071.508167	35.928116
1327.355277	144305.984327	35.933133
1328.890620	144514.081033	35.938151
1330.138745	144752.189254	35.943168
1331.618285	144976.821530	35.948186
1333.029912	145200.005844	35.953204
1334.162741	145427.308949	35.958221
1335.474317	145645.764024	35.963239
1336.520559	145883.579145	35.968256
1338.107851	146097.690321	35.973274
1339.467128	146315.925014	35.978292
1340.672161	146528.892045	35.983309
1342.278147	146736.250593	35.988327
1343.287410	146949.110379	35.993344
1344.916680	147168.486806	35.998362
1346.298613	147376.377987	36.003380
1347.366222	147593.115206	36.008397
1348.742962	147801.960839	36.013415
1350.102616	148029.506409	36.018432
1351.391959	148233.264945	36.023450
1352.612242	148458.079838	36.028468
1353.664489	148676.778616	36.033485
1355.310510	148893.836807	36.038503
1356.830656	149128.508112	36.043520
1357.965070	149351.233174	36.048538
1359.284107	149581.381129	36.053556
1360.465511	149814.331418	36.058573
1362.071498	150037.975576	36.063591
1363.340610	150270.749091	36.068608
1364.685233	150499.310287	36.073626
1366.161830	150723.954911	36.078644
1367.316871	150972.273304	36.083661
1368.527195	151197.431209	36.088679
1369.995471	151442.224676	36.093696
1371.263497	151676.426017	36.098714
1373.095285	151902.403462	36.103732
1374.504146	152157.618203	36.108749
1375.338453	152398.757784	36.113767
1376.915116	152637.408459	36.118784
1378.027504	152874.317595	36.123802
1379.692873	153119.861910	36.128820
1381.060073	153365.085839	36.133837
1382.571831	153612.243086	36.138855
1384.329456	153867.525236	36.143872
1385.478820	154106.350545	36.148890
1387.047970	154346.862945	36.153908
1388.419648	154594.439888	36.158925
1389.529544	154839.926223	36.163943
1391.157680	155089.978624	36.168960
1392.272702	155335.580505	36.173978
1393.786105	155587.823753	36.178996
1395.382552	155840.194732	36.184013
1397.244773	156075.552521	36.189031
1398.285832	156329.662831	36.194048
1400.436298	156569.407907	36.199066
1401.597323	156811.390764	36.204084
1402.877474	157056.250374	36.209101
1404.691119	157291.176276	36.214119
1406.114719	157526.900455	36.219136
1407.503333	157771.047788	36.224154
1409.017021	158002.748123	36.229172
1410.167932	158243.545005	36.234189
1411.712083	158474.645706	36.239207
1413.103508	158717.996618	36.244224
1414.497019	158957.628477	36.249242
1415.994600	159202.716634	36.254260
1416.671153	159452.771185	36.259277
1418.400075	159688.202019	36.264295
1420.166161	159924.262698	36.269312
1421.749487	160172.781722	36.274330
1422.860114	160413.364861	36.279348
1424.283670	160661.529964	36.284365
1425.740405	160892.450230	36.289383
1427.154326	161134.956466	36.294400
1428.347005	161387.629420	36.299418
1430.215557	161623.071029	36.304436
1431.203645	161868.554031	36.309453
1432.591311	162101.647770	36.314471
1434.181582	162326.597973	36.319488
1435.408735	162563.819272	36.324506
1437.085633	162805.046450	36.329524
1438.611976	163044.672995	36.334541
1440.030872	163268.396370	36.339559
1441.357529	163492.731662	36.344576
1442.623056	163729.100538	36.349594
1444.084862	163957.936085	36.354612
1445.466679	164196.903842	36.359629
1446.580693	164428.436259	36.364647
1448.118619	164678.223930	36.369664
1449.504092	164920.710580	36.374682
1450.884054	165156.152450	36.379700
1452.180117	165401.359155	36.384717
1453.628098	165645.082866	36.389735
1455.160788	165894.698087	36.394752
1456.231776	166150.391975	36.399770
1458.149209	166411.401190	36.404788
1459.272622	166663.063930	36.409805
1460.778701	166922.933268	36.414823
1462.456822	167184.592286	36.419840
1463.732286	167435.421415	36.424858
1465.207193	167694.397014	36.429876
1466.893464	167960.945941	36.434893
1468.268874	168221.703911	36.439911
1469.599271	168480.336778	36.444928
1470.836236	168745.816225	36.449946
1472.577200	169003.015426	36.454964
1473.980800	169278.983963	36.459981
1475.537630	169548.733324	36.464999
1477.049974	169821.334828	36.470016
1478.484202	170084.363104	36.475034
1479.996185	170351.278233	36.480052
1481.460604	170640.980899	36.485069
1482.929269	170896.375525	36.490087
1484.560156	171171.515620	36.495104
1485.874516	171456.445271	36.500122
1487.248754	171728.465877	36.505140
1488.908516	171999.350770	36.510157
1490.585800	172279.160344	36.515175
1492.558943	172554.416939	36.520192
1493.750838	172815.168968	36.525210
1495.716280	173084.790846	36.530228
1496.807104	173355.172741	36.535245
1498.234534	173623.509313	36.540263
1500.112343	173896.182491	36.545280
1501.892466	174172.998739	36.550298
1503.277457	174439.706674	36.555316
1504.632761	174720.578487	36.560333
1506.174595	174987.695425	36.565351
1508.062300	175248.930660	36.570368
1509.482000	175523.865141	36.575386
1510.809064	175785.062855	36.580404
1512.078594	176063.552754	36.585421
1513.801130	176337.312405	36.590439
1515.918042	176595.671615	36.595456
1517.084062	176870.155032	36.600474
1518.435495	177136.584910	36.605492
1519.904446	177417.016355	36.610509
1521.504603	177690.113839	36.615527
1523.064206	177953.440649	36.620544
1524.573020	178227.900186	36.625562
1526.050557	178501.603569	36.630580
1527.584510	178778.829215	36.635597
1529.084936	179039.552650	36.640615
1530.967375	179303.620333	36.645632
1532.366713	179572.691545	36.650650
1534.337615	179842.588429	36.655668
1535.340634	180084.852485	36.660685
1536.942942	180346.173340	36.665703
1538.634564	180594.350267	36.670720
1540.053210	180853.796485	36.675738
1541.597874	181098.213485	36.680756
1542.578945	181351.710261	36.685773
1544.299598	181606.133302	36.690791
1546.224296	181860.982270	36.695808
1546.914680	182131.873646	36.700826
1548.262879	182384.985582	36.705844
1550.044859	182646.995947	36.710861
1551.750592	182923.648502	36.715879
1553.480706	183184.322331	36.720896
1554.332493	183468.577278	36.725914
1556.415083	183738.366341	36.730932
1557.736295	184014.142428	36.735949
1559.283110	184311.447610	36.740967
1561.233825	184640.413749	36.745984
1562.289205	184921.339142	36.751002
1563.856706	185195.022621	36.756020
1565.375509	185482.099814	36.761037
1566.581805	185761.606952	36.766055
1568.487302	186059.648503	36.771072
1569.664207	186344.546465	36.776090
1571.564827	186633.878436	36.781108
1573.186528	186928.614150	36.786125
1574.950243	187220.331304	36.791143
1576.644515	187507.462784	36.796160
1577.602769	187807.435477	36.801178
1579.734776	188100.037158	36.806196
1581.410077	188388.139123	36.811213
1582.972673	188690.508834	36.816231
1584.847696	188983.051472	36.821248
1586.089492	189277.598980	36.826266
1587.910265	189570.964435	36.831284
1589.434846	189863.284792	36.836301
1591.198209	190160.343767	36.841319
1592.917980	190456.699116	36.846336
1594.498089	190753.127873	36.851354
1596.072446	191045.570405	36.856372
1597.793079	191339.006783	36.861389
1599.242871	191643.586312	36.866407
1600.989482	191940.296759	36.871424
1602.805315	192240.832596	36.876442
1604.351152	192525.815360	36.881460
1605.978830	192820.412874	36.886477
1607.390190	193120.099706	36.891495
1609.665603	193406.773749	36.896512
1610.923143	193701.659847	36.901530
1612.316020	194001.326234	36.906548
1614.329959	194301.150123	36.911565
1615.538832	194597.747738	36.916583
1617.774543	194889.892506	36.921600
1619.285558	195183.573798	36.926618
1620.846584	195472.955076	36.931636
1622.676681	195771.667965	36.936653
1624.086850	196063.233212	36.941671
1625.678401	196351.138269	36.946688
1627.019049	196655.924399	36.951706
1628.568930	196949.196917	36.956724
1630.178116	197242.867178	36.961741
1632.212779	197546.911540	36.966759
1633.865640	197843.395759	36.971776
1635.434201	198144.694703	36.976794
1637.002302	198438.322965	36.981812
1638.854462	198738.079999	36.986829
1640.234923	199031.129121	36.991847
1642.305571	199322.495857	36.996864
1643.518072	199608.358182	37.001882
1645.177247	199894.582952	37.006900
1646.674433	200157.768454	37.011917
1648.716237	200441.013068	37.016935
1649.799673	200715.644392	37.021952
1651.501390	200999.248014	37.026970
1653.086685	201282.489300	37.031988
1654.954604	201573.053507	37.037005
1656.008586	201858.817522	37.042023
1658.105885	202146.400118	37.047040
1659.281316	202444.542464	37.052058
1660.743218	202732.835108	37.057076
1662.878289	203035.959560	37.062093
1664.218401	203336.363832	37.067111
1666.299011	203630.784697	37.072128
1667.780002	203942.675286	37.077146
1668.993794	204247.012790	37.082164
1670.529760	204543.425500	37.087181
1671.874730	204853.636858	37.092199
1673.990281	205165.023648	37.097216
1675.445299	205493.203973	37.102234
1677.425640	205807.762859	37.107252
1679.102919	206117.492280	37.112269
1680.239073	206450.499759	37.117287
1682.445005	206758.546986	37.122304
1684.220439	207084.215527	37.127322
1685.859618	207395.248280	37.132340
1687.770728	207715.688865	37.137357
1689.277357	208061.189904	37.142375
1691.103214	208369.374996	37.147392
1692.944986	208691.910817	37.152410
1694.323289	209013.859107	37.157428
1696.351585	209342.031511	37.162445
1697.874914	209674.982976	37.167463
1699.855209	209993.154808	37.172480
1701.790384	210326.144257	37.177498
1703.192742	210651.875906	37.182516
1705.222904	210977.382672	37.187533
1706.761777	211305.278410	37.192551
1708.607126	211624.438556	37.197568
1710.113879	211961.866365	37.202586
1711.796735	212287.809980	37.207604
1713.871499	212608.408658	37.212621
1715.589651	212943.619733	37.217639
1717.118871	213274.186444	37.222656
1718.829299	213598.170975	37.227674
1720.754365	213935.840209	37.232692
1722.360599	214262.991711	37.237709
1724.115155	214595.861535	37.242727
1725.735016	214927.736578	37.247744
1727.715340	215269.767809	37.252762
1729.753830	215587.377178	37.257780
1731.533381	215913.105722	37.262797
1733.196032	216257.448410	37.267815
1735.073764	216580.977351	37.272832
1736.867258	216911.708993	37.277850
1738.640995	217235.838941	37.282868
1740.544140	217550.066729	37.287885
1742.032711	217886.460988	37.292903
1743.916591	218207.373404	37.297920
1745.658220	218538.495243	37.302938
1747.178182	218881.210752	37.307956
1749.303990	219188.113654	37.312973
1750.865855	219507.908555	37.317991
1752.641100	219839.660896	37.323008
1754.532461	220165.247443	37.328026
1756.255584	220493.477065	37.333044
1758.074999	220804.289988	37.338061
1759.793868	221110.037946	37.343079
1760.802350	221420.825549	37.348096
1762.919462	221729.051778	37.353114
1764.718013	222034.279454	37.358132
1766.543722	222343.034120	37.363149
1768.096434	222652.111020	37.368167
1769.907444	222963.154483	37.373184
1771.370859	223265.386374	37.378202
1773.304973	223581.796340	37.383220
1775.171082	223893.618852	37.388237
1776.505200	224215.101986	37.393255
1778.496193	224533.484674	37.398272
1779.841323	224859.310230	37.403290
1781.854965	225180.788703	37.408308
1783.792324	225505.607052	37.413325
1785.213020	225844.757939	37.418343
1787.453442	226175.727440	37.423360
1789.080499	226516.827514	37.428378
1791.091887	226836.553388	37.433396
1792.929581	227170.634303	37.438413
1794.643119	227500.669944	37.443431
1796.148857	227841.204519	37.448448
1797.987769	228182.880877	37.453466
1799.511825	228522.218441	37.458484
1801.596997	228855.117098	37.463501
1803.394028	229209.908221	37.468519
1805.482237	229551.494372	37.473536
1807.013793	229897.968869	37.478554
1808.883825	230240.630470	37.483572
1810.984117	230584.500695	37.488589
1812.584982	230930.963913	37.493607
1814.372420	231280.573267	37.498624
1816.413963	231623.410629	37.503642
1818.429465	231982.993087	37.508660
1820.019545	232333.902951	37.513677
1822.348357	232684.011099	37.518695
1823.681183	233029.956215	37.523712
1825.893207	233378.557955	37.528730
1827.702841	233730.651943	37.533748
1829.503398	234069.003613	37.538765
1831.097042	234432.842052	37.543783
1833.285486	234778.728244	37.548800
1835.183915	235121.687297	37.553818
1837.103907	235493.196525	37.558836
1839.083557	235824.837603	37.563853
1841.336567	236182.906298	37.568871
1842.874258	236529.832747	37.573888
1844.874839	236870.233901	37.578906
1846.862847	237218.562631	37.583924
1848.455174	237561.186301	37.588941
1850.347087	237912.755612	37.593959
1852.165851	238260.474646	37.598976
1854.482657	238609.969822	37.603994
1855.943597	238962.596137	37.609012
1857.986945	239301.057376	37.614029
1859.972156	239649.231437	37.619047
1861.615143	239996.086837	37.624064
1863.758897	240342.329976	37.629082
1865.385798	240686.900716	37.634100
1867.412812	241030.620898	37.639117
1869.162247	241377.508664	37.644135
1870.677486	241736.600758	37.649152
1872.710339	242079.988364	37.654170
1874.757963	242440.926767	37.659188
1876.402871	242782.494241	37.664205
1877.963134	243131.517567	37.669223
1879.695969	243477.287170	37.674240
1882.122996	243832.803989	37.679258
1883.619349	244171.623686	37.684276
1885.744571	244505.822727	37.689293
1887.159775	244829.590139	37.694311
1889.114835	245176.135150	37.699328
1890.954210	245511.063189	37.704346
1892.757964	245845.615204	37.709364
1894.743015	246184.101114	37.714381
1896.415680	246528.808171	37.719399
1898.124370	246880.062854	37.724416
1900.331868	247223.592655	37.729434
1901.886575	247567.757420	37.734452
1903.866571	247925.623146	37.739469
1905.821715	248280.138928	37.744487
1907.692298	248638.909434	37.749504
1909.777427	248990.837806	37.754522
1911.212992	249351.122842	37.759540
1913.173666	249708.124268	37.764557
1914.847437	250067.811650	37.769575
1916.705518	250447.029042	37.774592
1918.810920	250813.455015	37.779610
1920.231260	251187.074501	37.784628
1922.500344	251563.405315	37.789645
1924.395769	251942.791107	37.794663
1926.176855	252336.317259	37.799680
1928.518748	252710.957343	37.804698
1930.260776	253095.038164	37.809716
1931.851594	253476.753890	37.814733
1933.830891	253866.485518	37.819751
1936.061239	254264.508486	37.824768
1937.434901	254655.348771	37.829786
1939.757653	255050.865708	37.834804
1942.037457	255446.845447	37.839821
1943.796225	255846.512523	37.844839
1945.546692	256247.703769	37.849856
1947.700251	256641.566029	37.854874
1949.350765	257044.980364	37.859892
1951.396146	257454.072248	37.864909
1953.274099	257843.122385	37.869927
1955.522139	258256.345688	37.874944
1957.569449	258657.406720	37.879962
1959.375326	259068.105619	37.884980
1961.803492	259466.691340	37.889997
1963.657936	259872.757007	37.895015
1965.919893	260279.570325	37.900032
1968.161417	260685.420215	37.905050
1970.171737	261089.501444	37.910068
1972.075076	261492.962981	37.915085
1974.199650	261888.870082	37.920103
1976.135337	262287.319915	37.925120
1978.326410	262675.136659	37.930138
1980.231239	263089.615645	37.935156
1982.298510	263487.176923	37.940173
1985.000104	263879.811577	37.945191
1986.408355	264276.990426	37.950208
1988.447766	264678.158297	37.955226
1990.619967	265074.224006	37.960244
1992.411271	265456.886274	37.965261
1994.416098	265856.531007	37.970279
1996.334041	266257.229101	37.975296
1998.194481	266654.200961	37.980314
2000.188439	267056.280865	37.985332
2002.389997	267452.662754	37.990349
2004.547460	267847.018043	37.995367
2006.166297	268245.773706	38.000384
2008.470510	268637.410544	38.005402
2010.269721	269040.045967	38.010420
2012.047482	269451.064358	38.015437
2014.323719	269832.287368	38.020455
2016.406612	270223.596575	38.025472
2018.403013	270587.945267	38.030490
2020.000828	270968.533123	38.035508
2021.839507	271343.443428	38.040525
2023.689593	271724.953684	38.045543
2025.662670	272120.995677	38.050560
2027.572556	272508.258342	38.055578
2029.843945	272903.462780	38.060596
2031.261519	273288.360847	38.065613
2033.945105	273684.792419	38.070631
2035.719141	274086.900912	38.075648
2037.575643	274465.807504	38.080666
2039.562079	274881.237527	38.085684
2041.728250	275285.005818	38.090701
2043.820239	275687.285344	38.095719
2045.410095	276112.345514	38.100736
2047.209316	276521.777579	38.105754
2049.508309	276940.475000	38.110772
2051.124170	277365.041898	38.115789
2053.481203	277787.001774	38.120807
2055.897821	278215.146510	38.125824
2057.864653	278635.207368	38.130842
2059.913607	279066.045988	38.135860
2061.854212	279501.063888	38.140877
2064.086295	279929.964311	38.145895
2065.944099	280358.285963	38.150912
2067.980484	280790.259404	38.155930
2070.329132	281235.919801	38.160948
2072.284791	281664.827996	38.165965
2074.661242	282105.552233	38.170983
2076.558227	282546.044053	38.176000
2079.004648	282975.273943	38.181018
2081.082288	283417.077963	38.186036
2082.799153	283865.360184	38.191053
2085.547629	284300.349805	38.196071
2087.449231	284746.540578	38.201088
2089.564955	285187.133897	38.206106
2091.760005	285625.121894	38.211124
2093.603635	286078.499166	38.216141
2096.083987	286512.069233	38.221159
2097.922108	286957.976030	38.226176
2099.902651	287406.015868	38.231194
2102.449479	287849.418900	38.236212
2104.254551	288301.923643	38.241229
2106.889253	288742.564523	38.246247
2108.836336	289195.929484	38.251264
2111.147264	289629.962371	38.256282
2113.262740	290062.550184	38.261300
2115.197382	290519.767065	38.266317
2117.456983	290963.269581	38.271335
2119.844517	291414.594577	38.276352
2121.742205	291849.920841	38.281370
2124.114486	292307.665417	38.286388
2125.821008	292752.866521	38.291405
2128.454224	293189.337630	38.296423
2130.396274	293635.104723	38.301440
2132.477693	294079.653382	38.306458
2134.971482	294529.795981	38.311476
2137.116640	294973.617047	38.316493
2139.182694	295412.318586	38.321511
2141.086225	295861.451570	38.326528
2143.456721	296299.083226	38.331546
2145.949429	296751.696860	38.336564
2147.661780	297197.777331	38.341581
2149.991929	297640.634941	38.346599
2151.832480	298079.808301	38.351616
2153.892939	298523.132738	38.356634
2156.053649	298962.249072	38.361652
2158.266537	299392.595241	38.366669
2160.460780	299812.735460	38.371687
2162.676934	300232.335907	38.376704
2164.828495	300646.739004	38.381722
2166.941100	301063.023604	38.386740
2168.964875	301491.884967	38.391757
2170.856894	301910.659946	38.396775
2172.825592	302350.768946	38.401792
2174.921827	302774.049189	38.406810
2177.329249	303213.955426	38.411828
2179.092090	303641.824778	38.416845
2181.636596	304073.985277	38.421863
2183.811492	304526.050724	38.426880
2185.544797	304977.242063	38.431898
2187.837900	305419.533558	38.436916
2189.927912	305878.530199	38.441933
2192.247730	306319.819693	38.446951
2194.462106	306789.602030	38.451968
2196.509453	307240.267155	38.456986
2198.435811	307693.866167	38.462004
2200.686965	308165.914221	38.467021
2203.211463	308623.573876	38.472039
2205.235638	309089.658281	38.477056
2207.680705	309559.302001	38.482074
2210.111574	310026.709788	38.487092
2212.158359	310504.376486	38.492109
2214.287417	310965.857683	38.497127
2216.270988	311437.306520	38.502144
2218.744344	311921.161366	38.507162
2221.170216	312390.653307	38.512180
2223.289686	312873.259292	38.517197
2225.658899	313355.871962	38.522215
2227.807932	313833.514241	38.527232
2230.069553	314314.357140	38.532250
2232.283161	314793.984299	38.537268
2234.559799	315293.772770	38.542285
2236.813254	315769.931856	38.547303
2239.104130	316261.687741	38.552320
2241.409531	316746.076314	38.557338
2243.979067	317232.017100	38.562356
2246.002625	317715.855503	38.567373
2248.773355	318208.656761	38.572391
2250.981327	318694.409592	38.577408
2252.919775	319192.938265	38.582426
2255.369170	319674.709000	38.587444
2257.412300	320158.161983	38.592461
2259.484643	320653.734589	38.597479
2262.385972	321137.905036	38.602496
2264.439277	321637.072506	38.607514
2266.860521	322114.480967	38.612532
2269.133083	322612.511472	38.617549
2271.550744	323088.564555	38.622567
2273.947493	323577.962214	38.627584
2276.007539	324076.896544	38.632602
2278.595606	324561.380873	38.637620
2281.070939	325054.706966	38.642637
2283.565862	325537.468937	38.647655
2285.913967	326015.909437	38.652672
2287.732728	326501.125350	38.657690
2290.617612	326993.145911	38.662708
2292.493378	327477.782919	38.667725
2295.032803	327958.377665	38.672743
2297.380623	328432.070278	38.677760
2299.417461	328920.444741	38.682778
2301.927940	329398.134228	38.687796
2304.093917	329880.539862	38.692813
2306.550859	330365.938371	38.697831
2308.750727	330844.698854	38.702848
2310.718931	331296.268568	38.707866
2312.854546	331758.715380	38.712884
2314.994191	332207.964338	38.717901
2317.665281	332681.985714	38.722919
2320.020631	333138.191553	38.727936
2322.126765	333604.451061	38.732954
2324.512073	334061.427425	38.737972
2326.379253	334521.142791	38.742989
2328.565927	334988.716903	38.748007
2330.633318	335459.981900	38.753024
2333.274891	335938.557940	38.758042
2335.740585	336422.405957	38.763060
2337.861173	336906.428392	38.768077
2339.683888	337391.759248	38.773095
2342.019987	337885.754113	38.778112
2344.183158	338377.359669	38.783130
2346.691927	338877.477463	38.788148
2348.774300	339379.785516	38.793165
2351.134717	339896.347863	38.798183
2353.333732	340403.898765	38.803200
2355.720498	340925.869629	38.808218
2358.270936	341436.876078	38.813236
2361.098480	341948.922279	38.818253
2363.161659	342470.058452	38.823271
2365.484413	342979.251897	38.828288
2367.885098	343507.902600	38.833306
2370.598004	344030.562051	38.838324
2372.565680	344557.717352	38.843341
2374.899281	345087.875758	38.848359
2377.473879	345624.251870	38.853376
2379.802049	346151.123172	38.858394
2382.134855	346680.901698	38.863412
2384.649735	347213.153793	38.868429
2387.064010	347744.145260	38.873447
2389.461068	348284.538385	38.878464
2391.987263	348833.320867	38.883482
2394.711816	349366.316988	38.888500
2397.014247	349910.501650	38.893517
2399.445905	350449.484534	38.898535
2402.074587	350990.506761	38.903552
2404.709357	351529.820235	38.908570
2406.928462	352062.166619	38.913588
2409.285770	352612.052626	38.918605
2411.703597	353147.874021	38.923623
2414.385904	353687.625403	38.928640
2416.706099	354231.429896	38.933658
2419.326114	354769.093653	38.938676
2421.812627	355313.259061	38.943693
2423.920656	355864.749945	38.948711
2426.798293	356398.162465	38.953728
2429.190780	356947.054581	38.958746
2431.966346	357486.522981	38.963764
2433.985185	358020.979731	38.968781
2436.217304	358572.200050	38.973799
2439.307705	359105.583007	38.978816
2441.344312	359647.967845	38.983834
2443.639384	360184.295184	38.988852
2446.233024	360740.007414	38.993869
2448.678565	361285.492522	38.998887
2451.372732	361823.857229	39.003904
2453.923834	362370.497239	39.008922
2456.514660	362913.091076	39.013940
2458.707838	363457.916780	39.018957
2461.319040	364004.060933	39.023975
2464.055641	364537.604798	39.028992
2466.201730	365085.879673	39.034010
2468.217180	365625.320008	39.039028
2471.115631	366160.101243	39.044045
2473.329471	366676.961586	39.049063
2475.928604	367187.923839	39.054080
2478.084369	367706.751332	39.059098
2480.798185	368215.371241	39.064116
2483.420304	368742.063828	39.069133
2485.643354	369264.197236	39.074151
2488.265483	369763.301335	39.079168
2490.182650	370291.114162	39.084186
2493.016693	370815.124935	39.089204
2495.206315	371348.930990	39.094221
2497.276871	371879.299560	39.099239
2500.097135	372413.771938	39.104256
2502.191838	372955.720283	39.109274
2505.088175	373482.837850	39.114292
2507.311606	374036.804504	39.119309
2509.477216	374590.414271	39.124327
2512.131696	375132.915935	39.129344
2514.662665	375699.923698	39.134362
2516.867887	376258.509234	39.139380
2519.624676	376807.953155	39.144397
2522.150984	377375.838269	39.149415
2524.838768	377942.191479	39.154432
2527.009060	378523.254868	39.159450
2530.032052	379092.368159	39.164468
2532.484765	379661.355728	39.169485
2535.103835	380249.377938	39.174503
2537.607181	380813.393380	39.179520
2540.148257	381396.437537	39.184538
2542.652371	381976.384422	39.189556
2545.515405	382557.553856	39.194573
2547.746235	383139.340931	39.199591
2550.526479	383721.662048	39.204608
2553.167363	384319.440167	39.209626
2555.993007	384891.698681	39.214644
2558.486217	385489.573715	39.219661
2560.931865	386082.149440	39.224679
2563.653573	386667.602954	39.229696
2566.144362	387264.474012	39.234714
2569.003722	387845.953515	39.239732
2571.498306	388441.453807	39.244749
2574.223054	389029.814066	39.249767
2577.120341	389625.805306	39.254784
2579.498783	390219.888383	39.259802
2582.108651	390808.654604	39.264820
2585.471511	391392.174629	39.269837
2587.538794	391982.364619	39.274855
2590.180915	392570.981994	39.279872
2592.521180	393169.860063	39.284890
2595.266286	393760.609571	39.289908
2598.483095	394355.979389	39.294925
2600.789306	394952.135008	39.299943
2603.186909	395519.808742	39.304960
2606.159003	396125.703248	39.309978
2608.908010	396718.606522	39.314996
2611.458312	397306.058624	39.320013
2614.541732	397899.284903	39.325031
2617.311290	398479.940574	39.330048
2620.016476	399072.436973	39.335066
2622.335515	399652.172166	39.340084
2625.269378	400219.041122	39.345101
2627.895795	400806.393236	39.350119
2630.254414	401391.241532	39.355136
2632.924823	401973.090595	39.360154
2635.754292	402553.229798	39.365172
2638.416567	403128.977245	39.370189
2640.825009	403718.465080	39.375207
2643.309497	404290.263347	39.380224
2646.078182	404864.026994	39.385242
2648.596940	405434.171494	39.390260
2651.286481	405979.174898	39.395277
2653.717361	406532.808079	39.400295
2656.409074	407082.287959	39.405312
2658.900008	407651.165827	39.410330
2661.003139	408216.497190	39.415348
2663.703454	408774.130955	39.420365
2666.015252	409342.639147	39.425383
2668.762030	409912.380092	39.430400
2671.060024	410496.494620	39.435418
2673.416474	411075.575675	39.440436
2676.337582	411663.558333	39.445453
2678.776530	412256.355951	39.450471
2681.261027	412847.410177	39.455488
2683.646451	413462.442158	39.460506
2686.368246	414066.224422	39.465524
2688.863555	414674.881207	39.470541
2691.949320	415297.288069	39.475559
2694.324488	415916.651795	39.480576
2697.356916	416532.354029	39.485594
2699.696148	417158.717681	39.490612
2702.363327	417789.866828	39.495629
2704.561892	418418.541512	39.500647
2707.621258	419052.676411	39.505664
2710.326599	419699.642247	39.510682
2713.016808	420344.011194	39.515700
2716.168274	420987.579987	39.520717
2718.699276	421649.682992	39.525735
2721.505319	422298.473347	39.530752
2724.141409	422946.511285	39.535770
2726.631862	423604.107848	39.540788
2729.882567	424262.979999	39.545805
2732.455756	424920.015451	39.550823
2735.429527	425584.095596	39.555840
2738.420811	426249.667816	39.560858
2741.031678	426907.037073	39.565876
2744.178154	427566.778084	39.570893
2746.844122	428235.520015	39.575911
2749.622297	428899.318604	39.580928
2752.528128	429555.037883	39.585946
2755.178130	430216.942053	39.590964
2758.211178	430877.702639	39.595981
2760.931300	431543.493660	39.600999
2763.912157	432205.632830	39.606016
2766.803559	432882.874782	39.611034
2769.393247	433549.628495	39.616052
2772.503067	434198.691421	39.621069
2775.330209	434871.174071	39.626087
2778.739003	435534.800152	39.631104
2781.553258	436202.033398	39.636122
2784.077966	436863.882049	39.641140
2787.081081	437513.506382	39.646157
2789.783537	438176.494240	39.651175
2792.390016	438833.764727	39.656192
2795.185602	439487.597792	39.661210
2798.145944	440149.415081	39.666228
2801.118694	440810.802937	39.671245
2803.808101	441477.768534	39.676263
2806.817162	442131.779017	39.681280
2809.610309	442786.608458	39.686298
2812.651518	443446.780661	39.691316
2815.338745	444097.640382	39.696333
2818.222677	444754.204207	39.701351
2820.938319	445411.730477	39.706368
2823.656707	446062.111629	39.711386
2826.518194	446716.992419	39.716404
2830.185018	447369.653172	39.721421
2832.499809	448012.907135	39.726439
2835.188608	448632.598705	39.731456
2838.058843	449247.797031	39.736474
2840.555825	449867.829546	39.741492
2843.291743	450475.079355	39.746509
2846.166110	451088.345679	39.751527
2848.891457	451712.570145	39.756544
2851.399036	452358.566373	39.761562
2853.836208	452982.336878	39.766580
2857.226908	453617.446325	39.771597
2859.574662	454256.229642	39.776615
2862.036833	454892.700292	39.781632
2865.149661	455536.365276	39.786650
2867.659515	456201.704283	39.791668
2870.352554	456851.292011	39.796685
2873.091095	457513.213852	39.801703
2875.871646	458187.519338	39.806720
2879.194196	458858.231473	39.811738
2882.053631	459532.017831	39.816756
2884.694637	460209.748062	39.821773
2887.601485	460892.153276	39.826791
2890.089315	461581.358304	39.831808
2893.313491	462265.374517	39.836826
2896.222322	462963.186794	39.841844
2898.852918	463663.031921	39.846861
2901.894708	464373.681164	39.851879
2904.821275	465077.961791	39.856896
2907.575285	465781.180416	39.861914
2910.368781	466503.582745	39.866932
2913.515639	467208.445333	39.871949
2916.470246	467927.330518	39.876967
2919.526897	468657.466697	39.881984
2922.564056	469382.429144	39.887002
2924.868308	470098.698769	39.892020
2928.399289	470828.260962	39.897037
2931.499956	471560.177636	39.902055
2934.030417	472287.763457	39.907072
2937.464749	473019.158926	39.912090
2939.898273	473768.930816	39.917108
2943.053107	474492.739990	39.922125
2946.627020	475240.450012	39.927143
2949.352381	475977.973124	39.932160
2952.864087	476711.457469	39.937178
2955.345014	477447.589820	39.942196
2958.723900	478182.186664	39.947213
2961.608165	478920.002413	39.952231
2964.266132	479661.700219	39.957248
2967.865378	480389.103520	39.962266
2970.706608	481129.947460	39.967284
2973.618695	481868.074267	39.972301
2976.976774	482597.227045	39.977319
2979.782139	483340.642669	39.982336
2982.794341	484076.784651	39.987354
2986.166642	484817.773275	39.992372
2989.430278	485553.956765	39.997389
2992.484637	486279.910138	40.002407
2995.317438	487012.362843	40.007424
2998.721946	487738.897671	40.012442
3001.374640	488473.172494	40.017460
3004.601268	489200.572189	40.022477
3007.906044	489923.744045	40.027495
3011.056887	490668.362140	40.032512
3014.195309	491379.754573	40.037530
3016.799357	492105.852586	40.042548
3019.680366	492826.030311	40.047565
3022.907615	493543.299160	40.052583
3025.818184	494260.129829	40.057600
3029.261010	494978.051208	40.062618
3032.052639	495684.609986	40.067636
3035.779832	496369.842301	40.072653
3038.521961	497040.999138	40.077671
3041.630706	497725.862310	40.082688
3044.397646	498395.342405	40.087706
3047.575767	499071.926128	40.092724
3050.657083	499723.375412	40.097741
3053.683065	500406.565498	40.102759
3056.382869	501080.412622	40.107776
3059.344052	501744.876467	40.112794
3062.088459	502436.520666	40.117812
3065.505956	503126.567003	40.122829
3068.495793	503813.929651	40.127847
3071.437356	504507.607286	40.132864
3074.344572	505197.985980	40.137882
3077.427339	505920.405148	40.142900
3080.675872	506607.592925	40.147917
3083.766330	507314.846071	40.152935
3086.506355	508030.771657	40.157952
3089.518479	508730.721861	40.162970
3092.596180	509446.422159	40.167988
3095.423707	510178.724225	40.173005
3098.490705	510903.003525	40.178023
3101.341790	511643.977007	40.183040
3104.437193	512375.065863	40.188058
3107.553086	513115.668103	40.193076
3110.504222	513860.983506	40.198093
3113.730952	514616.423338	40.203111
3116.576460	515382.943300	40.208128
3119.827903	516132.614236	40.213146
3122.756193	516904.918873	40.218164
3125.429111	517668.522565	40.223181
3128.715517	518452.849716	40.228199
3131.557264	519231.721999	40.233216
3135.167132	520014.902968	40.238234
3138.127278	520805.679365	40.243252
3141.139314	521597.909020	40.248269
3144.416158	522400.202198	40.253287
3147.060006	523200.887995	40.258304
3150.721553	524005.587671	40.263322
3154.038592	524810.393113	40.268340
3157.024751	525614.950337	40.273357
3160.485325	526414.460990	40.278375
3163.067550	527234.607656	40.283392
3166.427268	528038.808207	40.288410
3169.485916	528863.048808	40.293428
3173.123612	529682.475839	40.298445
3176.481449	530492.553431	40.303463
3179.308112	531318.784845	40.308480
3182.401376	532132.467879	40.313498
3185.805117	532947.557731	40.318516
3189.107563	533779.382827	40.323533
3192.891707	534607.413659	40.328551
3195.912453	535431.895673	40.333568
3199.023077	536247.073345	40.338586
3202.539967	537065.950621	40.343604
3205.516848	537883.755380	40.348621
3209.176600	538697.033971	40.353639
3212.424472	539523.273630	40.358656
3215.755718	540334.992604	40.363674
3218.996532	541142.558419	40.368692
3222.118416	541966.449524	40.373709
3225.681068	542768.591506	40.378727
3228.957794	543598.572834	40.383744
3232.412368	544399.824093	40.388762
3235.153724	545208.108378	40.393780
3238.500750	546025.625829	40.398797
3242.030887	546831.724420	40.403815
3244.998782	547627.977322	40.408832
3248.248866	548402.418035	40.413850
3251.479221	549179.922270	40.418868
3254.608812	549937.384061	40.423885
3258.127934	550704.415783	40.428903
3261.048876	551470.790722	40.433920
3263.928790	552228.901098	40.438938
3267.062193	553013.947033	40.443956
3270.070868	553787.732022	40.448973
3273.478655	554579.801997	40.453991
3276.517231	555363.556779	40.459008
3279.669347	556155.963751	40.464026
3282.471321	556961.002774	40.469044
3285.576109	557763.935549	40.474061
3289.156026	558576.661933	40.479079
3291.854277	559385.111110	40.484096
3295.213559	560208.934154	40.489114
3298.552138	561047.332445	40.494132
3301.342052	561871.879844	40.499149
3305.072242	562714.256165	40.504167
3308.123212	563574.309850	40.509184
3311.620878	564422.860753	40.514202
3314.856361	565276.749714	40.519220
3317.853628	566132.365947	40.524237
3321.148358	566991.477946	40.529255
3324.278877	567873.885166	40.534272
3328.266620	568746.527868	40.539290
3331.385729	569611.129740	40.544308
3334.661598	570492.812569	40.549325
3338.005565	571374.967382	40.554343
3341.448062	572258.490063	40.559360
3344.592424	573145.243861	40.564378
3348.038115	574049.597001	40.569396
3351.173803	574944.368536	40.574413
3354.882521	575843.933122	40.579431
3357.978730	576743.971801	40.584448
3362.056954	577651.989418	40.589466
3365.356567	578549.950081	40.594484
3368.802958	579456.318990	40.599501
3372.332731	580366.552302	40.604519
3375.239491	581267.706091	40.609536
3379.000323	582184.955627	40.614554
3383.215211	583096.357452	40.619572
3386.022113	584006.203883	40.624589
3389.744579	584897.983258	40.629607
3393.161438	585808.684573	40.634624
3396.914525	586723.906156	40.639642
3400.474876	587623.686052	40.644660
3403.808033	588533.422699	40.649677
3406.997973	589433.909895	40.654695
3410.764900	590335.081287	40.659712
3414.643758	591234.410916	40.664730
3418.076749	592134.684205	40.669748
3421.161580	593037.084451	40.674765
3424.882549	593927.220153	40.679783
3428.199756	594833.228637	40.684800
3431.665962	595730.246273	40.689818
3435.367371	596619.909719	40.694836
3438.458468	597531.266389	40.699853
3442.112910	598428.125514	40.704871
3445.454040	599316.519191	40.709888
3449.298966	600213.845083	40.714906
3452.697794	601108.068688	40.719924
3456.160877	602010.541536	40.724941
3459.488685	602911.310192	40.729959
3463.223204	603810.739330	40.734976
3466.333250	604689.528199	40.739994
3470.067961	605574.930842	40.745012
3473.050021	606459.461751	40.750016
3476.715521	607295.520182	40.755021
3479.647352	608094.764942	40.760026
3482.948141	608843.779455	40.765031
3486.135752	609519.096780	40.770036
3488.907118	610164.882229	40.775040
3491.942918	610729.534097	40.780045
3494.644206	611255.608176	40.785050
3497.338107	611720.611084	40.790055
3499.956207	612135.710567	40.795060
3501.785180	612512.972389	40.800064
3504.059710	612808.116081	40.805069
3506.192820	613075.479192	40.810074
3507.866037	613285.270732	40.815079
3509.650688	613459.849373	40.820084
3511.117706	613604.732575	40.825088
3512.453719	613687.001498	40.830093
3513.691833	613765.236190	40.835098
3514.834163	613788.950867	40.840103
3515.773420	613776.357565	40.845108
3516.758656	613748.611309	40.850112
3518.440415	613692.763807	40.855117
3518.995424	613613.498454	40.860122
3519.831216	613509.394964	40.865127
3520.351593	613364.999543	40.870132
3521.080413	613227.867809	40.875136
3521.803851	613056.992242	40.880141
3522.175483	612882.819433	40.885146
3522.156820	612670.611298	40.890151
3522.692160	612462.261500	40.895156
3523.674344	612251.287896	40.900160
3523.736000	612007.607386	40.905165
3524.077951	611755.777866	40.910170
3523.862874	611509.628844	40.915175
3524.345460	611233.115766	40.920180
3524.104409	610973.458203	40.925184
3524.141364	610693.650116	40.930189
3524.394001	610417.100771	40.935194
3524.319995	610135.794604	40.940199
3524.950118	609839.118983	40.945204
3524.580112	609540.640811	40.950208
3524.386541	609243.626563	40.955213
3524.459557	608934.459644	40.960218
3524.418881	608640.604572	40.965223
3524.259364	608333.956393	40.970228
3524.120994	608030.396594	40.975232
3524.187700	607718.143027	40.980237
3524.147519	607413.699337	40.985242
3523.641913	607111.520189	40.990247
3523.802465	606803.575731	40.995252
3523.427638	606511.262456	41.000256
3523.137992	606191.715015	41.005261
3522.845406	605890.267024	41.010266
3522.729254	605588.532499	41.015271
3522.734750	605286.119768	41.020276
3522.185435	605005.047201	41.025280
3522.233070	604710.865792	41.030285
3522.208559	604421.340238	41.035290
3521.941363	604127.591705	41.040295
3521.881059	603818.892191	41.045300
3521.534101	603539.799586	41.050304
3521.457823	603237.740042	41.055309
3521.025787	602953.391030	41.060314
3520.629870	602680.587853	41.065319
3520.979186	602392.198208	41.070324
3520.727871	602119.057448	41.075328
3520.628471	601847.537229	41.080333
3520.160095	601566.058530	41.085338
3519.710789	601277.862977	41.090343
3519.305006	601008.220532	41.095348
3519.174194	600762.001291	41.100352
3518.953981	600486.010144	41.105357
3519.091254	600224.621042	41.110362
3518.688659	599966.062733	41.115367
3518.910087	599710.904294	41.120372
3518.316932	599448.608933	41.125376
3518.029824	599205.180634	41.130381
3518.347384	598959.349501	41.135386
3517.458325	598717.255443	41.140391
3517.421666	598476.474297	41.145396
3517.293685	598240.307564	41.150400
3516.673717	598001.108571	41.155405
3516.866145	597776.896345	41.160410
3516.448062	597544.964712	41.165415
3516.410799	597320.227976	41.170420
3515.990556	597099.601735	41.175424
3515.893616	596874.664579	41.180429
3515.843295	596662.082357	41.185434
3515.337900	596438.101006	41.190439
3514.970414	596227.161863	41.195444
3514.640347	596027.779266	41.200448
3514.792984	595815.949475	41.205453
3514.579977	595612.835383	41.210458
3514.612909	595422.247708	41.215463
3514.374181	595220.832674	41.220468
3513.703036	595027.293362	41.225472
3513.742934	594834.991459	41.230477
3513.430807	594650.353018	41.235482
3513.068256	594462.714503	41.240487
3513.903111	594286.203584	41.245492
3513.100856	594098.326905	41.250496
3512.881642	593926.832664	41.255501
3512.847485	593743.887913	41.260506
3512.469908	593579.324233	41.265511
3512.605235	593403.859658	41.270516
3512.538839	593239.141920	41.275520
3512.210105	593073.761453	41.280525
3512.325914	592913.768359	41.285530
3511.700540	592744.772862	41.290535
3512.026464	592579.933550	41.295540
3511.390773	592421.102419	41.300544
3511.398033	592267.027100	41.305549
3511.381483	592111.701033	41.310554
3511.075361	591970.042714	41.315559
3511.164216	591813.343393	41.320564
3510.698246	591668.500215	41.325568
3510.745451	591522.673184	41.330573
3510.441108	591379.203438	41.335578
3510.058119	591248.167451	41.340583
3510.237689	591103.766775	41.345588
3509.877684	590971.271066	41.350592
3510.108508	590843.039725	41.355597
3509.958706	590715.116844	41.360602
3509.862923	590588.236042	41.365607
3510.102838	590460.149013	41.370612
3509.928315	590321.454261	41.375616
3509.495350	590181.295149	41.380621
3509.225459	590062.300945	41.385626
3509.534764	589947.273008	41.390631
3509.581933	589816.352747	41.395636
3509.336576	589688.432617	41.400640
3509.162805	589566.562132	41.405645
3509.193257	589451.622611	41.410650
3508.618120	589334.020865	41.415655
3508.877270	589204.112210	41.420660
3508.505089	589096.847626	41.425664
3508.933667	588989.356587	41.430669
3508.645542	588881.525575	41.435674
3508.488170	588765.255279	41.440679
3508.674096	588643.919433	41.445684
3507.849594	588548.595321	41.450688
3507.787073	588443.330227	41.455693
3507.920006	588335.478060	41.460698
3508.090927	588238.041397	41.465703
3507.957111	588131.381390	41.470708
3507.909739	588036.833241	41.475712
3507.666377	587934.598028	41.480717
3507.565478	587822.317557	41.485722
3507.602161	587737.675466	41.490727
3507.469638	587644.139419	41.495732
3507.454334	587554.392707	41.500736
3507.139134	587454.469326	41.505741
3507.193060	587365.010899	41.510746
3507.176858	587270.952332	41.515751
3506.775593	587179.108013	41.520756
3506.496831	587097.066014	41.525760
3506.931075	587003.536080	41.530765
3506.920990	586926.913212	41.535770
3506.700832	586851.575511	41.540775
3506.415497	586756.502163	41.545780
3506.721379	586684.087971	41.550784
3506.821044	586596.520461	41.555789
3506.695225	586511.393075	41.560794
3506.293188	586435.930583	41.565799
3506.612630	586355.593675	41.570804
3505.956291	586280.871500	41.575808
3506.219689	586197.434919	41.580813
3506.338679	586134.919466	41.585818
3505.995162	586065.459407	41.590823
3506.172573	585988.199211	41.595828
3505.854871	585905.502783	41.600832
3505.965341	585825.996551	41.605837
3506.188682	585758.099857	41.610842
3505.712052	585690.462528	41.615847
3505.816662	585620.929585	41.620852
3505.548155	585558.521530	41.625856
3505.534015	585490.008729	41.630861
3505.450554	585428.372936	41.635866
3504.810978	585368.126890	41.640871
3504.788866	585302.471081	41.645876
3505.102988	585240.621711	41.650880
3505.411999	585174.161538	41.655885
3505.361426	585117.430838	41.660890
3505.162229	585068.241501	41.665895
3505.316469	584999.799553	41.670900
3505.199066	584941.474449	41.675904
3505.229689	584885.531827	41.680909
3505.275487	584823.671927	41.685914
3504.945582	584767.133451	41.690919
3505.282478	584712.094424	41.695924
3505.132984	584659.487018	41.700928
3505.369878	584587.169972	41.705933
3504.983415	584533.797008	41.710938
3504.959298	584486.983701	41.715943
3505.208924	584423.235035	41.720948
3505.299118	584375.551245	41.725952
3504.940506	584317.962293	41.730957
3505.146378	584257.076696	41.735962
3504.790536	584203.546957	41.740967
3505.050792	584146.461878	41.745972
3504.891572	584104.580507	41.750976
3504.773436	584032.014541	41.755981
3504.650502	583983.008920	41.760986
3504.637440	583933.284113	41.765991
3504.814112	583868.841841	41.770996
3504.782899	583818.768454	41.776000
3504.851840	583770.834719	41.781005
3505.034675	583723.735161	41.786010
3505.119152	583665.672486	41.791015
3505.106569	583604.516650	41.796020
3504.857258	583560.441590	41.801024
3504.510189	583499.838758	41.806029
3504.804226	583449.361933	41.811034
3504.688699	583390.777641	41.816039
3504.612785	583339.355537	41.821044
3504.451124	583292.759165	41.826048
3504.320385	583234.928385	41.831053
3504.548783	583194.436752	41.836058
3504.397629	583144.278782	41.841063
3504.363584	583095.505967	41.846068
3504.243631	583046.646101	41.851072
3504.455639	583009.264536	41.856077
3504.493826	582956.519369	41.861082
3504.199226	582926.235259	41.866087
3504.061578	582870.007884	41.871092
3504.136967	582830.992689	41.876096
3503.997842	582786.446104	41.881101
3504.408765	582750.887496	41.886106
3504.444999	582715.136680	41.891111
3504.369888	582657.745375	41.896116
3504.077714	582611.266790	41.901120
3504.309121	582569.117968	41.906125
3504.220892	582526.617879	41.911130
3504.101212	582478.958679	41.916135
3504.496983	582431.820311	41.921140
3504.538583	582389.700477	41.926144
3504.102638	582340.184988	41.931149
3504.105208	582292.355465	41.936154
3504.120560	582266.082057	41.941159
3504.130044	582201.806578	41.946164
3504.419501	582171.830176	41.951168
3504.054519	582117.389263	41.956173
3504.269793	582080.455269	41.961178
3503.849262	582038.506612	41.966183
3504.099191	581988.982598	41.971188
3504.312023	581960.421433	41.976192
3504.369477	581911.027433	41.981197
3504.416099	581870.208400	41.986202
3503.736789	581812.656467	41.991207
3503.820551	581784.816953	41.996212
3503.819136	581744.957584	42.001216
3503.888217	581701.978488	42.006221
3504.190502	581658.561660	42.011226
3504.034530	581634.619897	42.016231
3503.805604	581596.901376	42.021236
3503.534528	581554.476269	42.026240
3503.798573	581526.457505	42.031245
3504.194665	581480.418090	42.036250
3503.918107	581441.102031	42.041255
3503.764251	581396.351583	42.046260
3504.204720	581361.034587	42.051264
3503.883963	581323.730608	42.056269
3504.053176	581276.823297	42.061274
3503.780948	581241.065794	42.066279
3504.152570	581189.864553	42.071284
3504.140299	581162.991157	42.076288
3503.742631	581113.714887	42.081293
3504.354043	581074.208568	42.086298
3504.210289	581041.539077	42.091303
3503.825340	580991.257450	42.096308
3504.051609	580955.019963	42.101312
3503.984970	580914.716528	42.106317
3503.933668	580860.320669	42.111322
3503.298216	580831.989491	42.116327
3503.702448	580794.971529	42.121332
3503.613679	580764.900022	42.126336
3503.944216	580725.185659	42.131341
3503.901668	580692.549460	42.136346
3503.108954	580653.261149	42.141351
3503.584119	580613.122633	42.146356
3503.619037	580580.875139	42.151360
3503.366522	580553.686821	42.156365
3503.641365	580516.287010	42.161370
3503.683441	580492.412103	42.166375
3503.646188	580447.439019	42.171380
3503.496909	580416.222718	42.176384
3503.628649	580386.667298	42.181389
3503.401937	580338.413879	42.186394
3503.503461	580321.298791	42.191399
3503.380496	580273.229447	42.196404
3503.657572	580257.541010	42.201408
3502.955693	580222.449121	42.206413
3503.220450	580193.875290	42.211418
3503.616433	580164.628985	42.216423
3503.430056	580128.202583	42.221428
3503.383316	580096.969355	42.226432
3503.357143	580070.847668	42.231437
3503.403613	580036.440530	42.236442
3503.354461	580003.051151	42.241447
3503.452322	579967.081244	42.246452
3503.202016	579948.566349	42.251456
3502.962115	579913.601846	42.256461
3503.249978	579874.593163	42.261466
3502.762422	579855.011980	42.266471
3502.901605	579821.041000	42.271476
3503.139114	579804.204737	42.276480
3502.921608	579781.171230	42.281485
3502.895933	579751.438142	42.286490
3502.620340	579743.357420	42.291495
3503.232548	579712.722157	42.296500
3503.142556	579687.712784	42.301504
3503.264522	579662.870808	42.306509
3503.089095	579638.576742	42.311514
3503.056107	579606.888660	42.316519
3502.994057	579585.334873	42.321524
3503.468780	579551.310615	42.326528
3502.923433	579530.383901	42.331533
3503.342120	579500.229640	42.336538
3503.061206	579482.721715	42.341543
3503.380314	579446.665390	42.346548
3503.339263	579410.163768	42.351552
3502.912939	579387.663574	42.356557
3502.948451	579353.356334	42.361562
3503.130235	579336.277333	42.366567
3502.788837	579300.123195	42.371572
3503.152100	579282.213357	42.376576
3503.179578	579263.102254	42.381581
3503.636046	579230.684646	42.386586
3503.193107	579198.658295	42.391591
3503.052963	579169.242444	42.396596
3502.860514	579146.705200	42.401600
3502.873553	579124.185937	42.406605
3502.867123	579096.103033	42.411610
3502.793733	579077.157830	42.416615
3502.952201	579043.883566	42.421620
3503.125168	579027.858623	42.426624
3502.947680	579009.431080	42.431629
3503.199598	578980.354642	42.436634
3502.715881	578961.824441	42.441639
3502.943836	578933.554035	42.446644
3503.374245	578902.644069	42.451648
3502.917630	578879.646074	42.456653
3503.309180	578844.429044	42.461658
3503.018205	578835.698101	42.466663
3503.142148	578804.284110	42.471668
3502.785384	578775.302292	42.476672
3502.723209	578749.634495	42.481677
3503.041379	578723.305361	42.486682
3503.000233	578693.973083	42.491687
3502.981034	578671.357642	42.496692
3503.100804	578647.416480	42.501696
3503.039968	578619.942706	42.506701
3503.609487	578595.279147	42.511706
3503.119440	578566.718840	42.516711
3503.150229	578540.985878	42.521716
3503.028006	578514.123269	42.526720
3503.082522	578491.546093	42.531725
3503.411767	578468.374242	42.536730
3503.188615	578445.288700	42.541735
3503.175631	578398.899266	42.546740
3503.241728	578376.721272	42.551744
3503.340865	578353.033471	42.556749
3503.619045	578326.408735	42.561754
3503.305563	578293.757703	42.566759
3503.214735	578269.547733	42.571764
3503.283190	578242.654662	42.576768
3502.978776	578199.720415	42.581773
3503.014606	578168.268256	42.586778
3503.086616	578153.461541	42.591783
3503.209716	578128.967053	42.596788
3503.147150	578109.316354	42.601792
3503.156350	578070.044002	42.606797
3503.273628	578037.124260	42.611802
3503.312582	578011.639576	42.616807
3503.042895	577975.169002	42.621812
3503.369637	577959.620039	42.626816
3503.416631	577938.998968	42.631821
3503.477634	577893.849750	42.636826
3502.786034	577872.240603	42.641831
3503.143134	577847.458141	42.646836
3503.573392	577821.209674	42.651840
3503.006614	577784.684610	42.656845
3503.377250	577760.752489	42.661850
3502.869241	577741.070466	42.666855
3503.178320	577707.618212	42.671860
3503.154206	577694.832163	42.676864
3502.546810	577667.993210	42.681869
3502.997956	577643.596845	42.686874
3503.256600	577629.863703	42.691879
3503.038366	577596.944961	42.696884
3502.762456	577565.941097	42.701888
3502.581456	577530.107243	42.706893
3502.908236	577522.331992	42.711898
3502.795899	577504.493662	42.716903
3503.090569	577478.917633	42.721908
3502.892846	577457.330787	42.726912
3502.960193	577434.398371	42.731917
3502.990612	577398.932306	42.736922
3503.020213	577379.065286	42.741927
3503.044127	577351.374515	42.746932
3503.040001	577329.155265	42.751936
3502.923291	577306.100886	42.756941
3503.337826	577280.756456	42.761946
3502.884811	577251.434622	42.766951
3503.011373	577228.743319	42.771956
3503.024986	577206.822003	42.776960
3503.057160	577185.299011	42.781965
3502.861956	577155.184244	42.786970
3502.747504	577131.978678	42.791975
3502.785606	577108.197468	42.796980
3503.289569	577085.497035	42.801985
3502.619582	577061.675944	42.806989
3502.936650	577037.550020	42.811994
3502.376895	577017.523697	42.816999
3502.726653	576992.590018	42.822004
3503.181178	576980.631197	42.827009
3502.997826	576956.483010	42.832013
3503.420602	576922.509046	42.837018
3502.576230	576900.169502	42.842023
3502.705320	576869.802633	42.847028
3502.880870	576861.699449	42.852033
3502.748483	576841.204720	42.857037
3503.116296	576810.700052	42.862042
3503.243444	576796.434686	42.867047
3502.966096	576767.435244	42.872052
3502.968019	576735.733562	42.877057
3503.214206	576714.627655	42.882061
3503.243368	576683.423174	42.887066
3502.820389	576669.945899	42.892071
3502.958177	576632.654838	42.897076
3502.488467	576613.165484	42.902081
3502.641851	576592.675788	42.907085
3502.870218	576573.177557	42.912090
3502.832420	576546.748479	42.917095
3502.359370	576531.322572	42.922100
3502.771608	576507.080309	42.927105
3502.517129	576489.061937	42.932109
3502.763081	576454.462102	42.937114
3502.763046	576448.492863	42.942119
3502.748283	576423.113289	42.947124
3502.902308	576409.194364	42.952129
3502.654815	576393.783169	42.957133
3502.708631	576368.242264	42.962138
3502.458074	576356.342845	42.967143
3502.783445	576344.403541	42.972148
3503.176591	576309.479275	42.977153
3502.702138	576283.769951	42.982157
3502.799382	576260.379000	42.987162
3502.985725	576249.013118	42.992167
3502.482575	576218.743327	42.997172
3502.918318	576205.081086	43.002177
3502.627293	576189.475764	43.007181
3502.612716	576164.597207	43.012186
3502.452024	576142.249594	43.017191
3502.916129	576119.854426	43.022196
3502.611965	576095.622946	43.027201
3502.475199	576089.123095	43.032205
3502.701507	576053.672320	43.037210
3502.959678	576047.863158	43.042215
3502.864912	576024.551897	43.047220
3503.108831	576011.471210	43.052225
3503.111025	575985.335542	43.057229
3502.771124	575947.063444	43.062234
3502.368636	575927.512224	43.067239
3502.723358	575905.735700	43.072244
3502.427595	575886.518875	43.077249
3502.207956	575882.590237	43.082253
3502.484517	575846.980463	43.087258
3502.723823	575825.673308	43.092263
3502.819363	575821.394390	43.097268
3502.777719	575797.422214	43.102273
3502.616415	575779.789456	43.107277
3502.625943	575748.585449	43.112282
3502.323483	575734.034744	43.117287
3502.495169	575709.226391	43.122292
3502.613001	575712.719531	43.127297
3502.566543	575685.286480	43.132301
3502.373907	575672.725133	43.137306
3502.723588	575661.032133	43.142311
3502.695651	575634.950526	43.147316
3502.809263	575619.832975	43.152321
3502.299103	575600.097355	43.157325
3502.450716	575579.656258	43.162330
3502.521524	575562.889855	43.167335
3502.816814	575546.539826	43.172340
3502.635184	575522.438452	43.177345
3502.392341	575511.690747	43.182349
3502.701886	575489.519155	43.187354
3502.898182	575459.990797	43.192359
3502.568025	575436.263621	43.197364
3502.865642	575425.732341	43.202369
3502.533017	575406.068959	43.207373
3502.841413	575384.449172	43.212378
3502.938199	575372.444243	43.217383
3503.144210	575346.174895	43.222388
3502.944882	575316.457177	43.227393
3502.583951	575299.306374	43.232397
3502.858951	575272.925737	43.237402
3502.730495	575243.698418	43.242407
3502.492899	575225.073373	43.247412
3502.769477	575208.625446	43.252417
3502.819052	575184.587540	43.257421
3502.547087	575161.402528	43.262426
3502.880227	575148.758402	43.267431
3502.675210	575133.037831	43.272436
3502.741742	575103.880001	43.277441
3502.817780	575093.232549	43.282445
3502.896920	575062.417103	43.287450
3502.500908	575041.257954	43.292455
3502.658970	575032.353502	43.297460
3502.769763	575022.001558	43.302465
3502.192441	574991.740056	43.307469
3502.411780	574977.207135	43.312474
3502.382150	574971.091235	43.317479
3502.615429	574943.512311	43.322484
3502.744775	574928.341205	43.327489
3502.591312	574902.879551	43.332493
3502.588687	574879.401010	43.337498
3502.733949	574873.408222	43.342503
3502.446393	574853.485985	43.347508
3502.590778	574816.087543	43.352513
3502.465989	574806.574934	43.357517
3502.354035	574794.953207	43.362522
3502.892646	574778.865045	43.367527
3502.607802	574760.497465	43.372532
3502.548194	574741.041087	43.377537
3502.858550	574726.844801	43.382541
3502.748876	574699.318895	43.387546
3502.430162	574688.481925	43.392551
3502.260533	574654.342891	43.397556
3502.531173	574639.299818	43.402561
3502.027729	574625.330966	43.407565
3502.879697	574609.043067	43.412570
3502.591442	574597.498867	43.417575
3502.702302	574577.413518	43.422580
3502.666681	574561.464988	43.427585
3502.566596	574537.449100	43.432589
3502.429204	574527.837885	43.437594
3502.352364	574505.323405	43.442599
3502.169743	574479.714843	43.447604
3502.437213	574465.775788	43.452609
3502.436283	574451.126114	43.457613
3502.197863	574425.425811	43.462618
3502.430491	574439.286747	43.467623
3502.264002	574421.552331	43.472628
3502.328578	574396.306303	43.477633
3502.151962	574388.356741	43.482637
3502.478015	574373.304653	43.487642
3502.165928	574360.559832	43.492647
3502.543289	574363.310424	43.497652
3502.535170	574330.750637	43.502657
3502.374439	574318.082449	43.507661
3502.406219	574295.600742	43.512666
3502.283241	574289.448894	43.517671
3502.447980	574269.806118	43.522676
3502.607490	574244.043195	43.527681
3502.626915	574234.056014	43.532685
3502.027863	574213.228080	43.537690
3502.424767	574196.960561	43.542695
3502.063208	574189.792348	43.547700
3502.453959	574171.870084	43.552705
3502.206071	574164.232537	43.557709
3502.799695	574144.572669	43.562714
3502.585004	574129.002727	43.567719
3503.019042	574114.384963	43.572724
3502.830043	574083.207389	43.577729
3502.281399	574060.163711	43.582733
3502.616164	574046.012930	43.587738
3502.545819	574027.961832	43.592743
3502.473957	574016.433381	43.597748
3502.567663	573984.408578	43.602753
3502.377222	573988.402000	43.607757
3502.406272	573958.293794	43.612762
3502.609939	573940.199720	43.617767
3502.497729	573930.834925	43.622772
3502.882836	573904.132848	43.627777
3501.868270	573889.741254	43.632781
3502.385536	573865.727776	43.637786
3502.520056	573858.531973	43.642791
3502.610626	573852.848236	43.647796
3502.567536	573825.661007	43.652801
3502.444076	573817.853254	43.657805
3502.371602	573790.971576	43.662810
3502.442524	573781.828897	43.667815
3502.140870	573765.669965	43.672820
3502.616213	573745.225118	43.677825
3502.167650	573742.786557	43.682829
3502.704298	573728.001734	43.687834
3502.623861	573716.173275	43.692839
3502.593047	573694.101550	43.697844
3502.429770	573669.943177	43.702849
3502.224702	573667.416360	43.707853
3502.516621	573636.864812	43.712858
3502.372768	573616.616881	43.717863
3502.227353	573605.601254	43.722868
3502.465770	573589.558339	43.727873
3502.343033	573582.051357	43.732877
3502.169937	573576.659573	43.737882
3502.150048	573549.317530	43.742887
3501.882733	573539.525087	43.747892
3502.448981	573543.199673	43.752897
3502.328524	573524.152112	43.757901
3502.167827	573496.581080	43.762906
3502.240105	573496.068037	43.767911
3502.108471	573471.452720	43.772916
3502.187547	573446.001607	43.777921
3502.447991	573450.476657	43.782925
3502.434430	573424.437876	43.787930
3502.297009	573416.632028	43.792935
3502.373262	573404.678397	43.797940
3502.652305	573381.554118	43.802945
3502.475219	573372.801108	43.807949
3502.280073	573342.575789	43.812954
3502.416481	573325.494761	43.817959
3502.356356	573328.012948	43.822964
3502.156294	573303.257435	43.827969
3502.190489	573278.565599	43.832973
3502.456182	573270.796984	43.837978
3502.358215	573263.486622	43.842983
3502.098847	573243.908370	43.847988
3502.452782	573238.534386	43.852993
3502.319465	573226.011217	43.857997
3502.726598	573199.755626	43.863002
3502.497843	573193.117954	43.868007
3502.141665	573176.063531	43.873012
3502.820761	573163.463465	43.878017
3502.515363	573140.831473	43.883021
3502.523331	573123.218278	43.888026
3502.363694	573107.487793	43.893031
3502.625714	573090.487129	43.898036
3502.720669	573082.142956	43.903041
3503.262064	573060.482312	43.908045
3502.338890	573034.333952	43.913050
3502.490455	573013.988584	43.918055
3502.365432	573004.073079	43.923060
3502.547313	572972.834469	43.928065
3502.015238	572966.394614	43.933069
3502.327407	572958.166925	43.938074
3502.775849	572953.129274	43.943079
3502.681597	572934.026448	43.948084
3502.811191	572895.670610	43.953089
3502.156786	572884.332431	43.958093
3502.243574	572864.398343	43.963098
3502.527718	572840.670034	43.968103
3502.177838	572826.725123	43.973108
3502.616616	572822.692483	43.978113
3502.565831	572804.786913	43.983117
3502.451378	572783.328627	43.988122
3502.613113	572767.948855	43.993127
3502.706869	572760.256949	43.998132
3502.597053	572731.271115	44.003137
3502.706096	572722.673585	44.008141
3502.744516	572706.108729	44.013146
3502.597338	572689.020899	44.018151
3502.172215	572658.026852	44.023156
3502.206650	572636.344298	44.028161
3502.450003	572636.607332	44.033165
3502.317082	572609.330875	44.038170
3502.606491	572588.160336	44.043175
3502.288088	572586.303318	44.048180
3502.763419	572558.028429	44.053185
3502.925638	572551.279081	44.058189
3502.762890	572526.064428	44.063194
3502.863400	572507.482408	44.068199
3502.176101	572479.037821	44.073204
3502.469760	572465.945270	44.078209
3502.173035	572445.167172	44.083213
3502.372738	572434.999686	44.088218
3502.865705	572431.660953	44.093223
3502.348110	572407.605461	44.098228
3502.527678	572394.079046	44.103233
3502.272853	572381.122322	44.108237
3502.480065	572349.827861	44.113242
3502.633831	572351.259047	44.118247
3502.531773	572325.081041	44.123252
3502.657417	572313.821064	44.128257
3502.573604	572289.546968	44.133261
3502.423234	572264.881783	44.138266
3502.938949	572250.951386	44.143271
3502.405632	572239.142005	44.148276
3502.680808	572216.768670	44.153281
3502.463925	572197.733957	44.158285
3502.006881	572185.210067	44.163290
3502.180690	572159.640903	44.168295
3502.447638	572149.362289	44.173300
3502.518128	572142.827763	44.178305
3502.349851	572127.799803	44.183309
3502.107749	572100.739917	44.188314
3502.448584	572094.514368	44.193319
3502.261225	572078.385342	44.198324
3502.541042	572051.093203	44.203329
3502.592964	572050.282191	44.208333
3502.231844	572027.405782	44.213338
3502.125955	572018.490051	44.218343
3502.489903	572004.432536	44.223348
3502.719647	571979.556765	44.228353
3502.661342	571970.583376	44.233357
3502.818402	571943.611261	44.238362
3502.655655	571918.395260	44.243367
3502.481173	571906.178161	44.248372
3503.026009	571884.615113	44.253377
3503.036339	571869.257798	44.258381
3502.655503	571836.949853	44.263386
3502.579593	571816.939002	44.268391
3502.467135	571803.708451	44.273396
3502.626699	571784.814927	44.278401
3502.212813	571768.871422	44.283405
3502.408203	571758.603643	44.288410
3502.591331	571735.340469	44.293415
3502.222431	571732.387184	44.298420
3502.242347	571697.858339	44.303425
3502.346211	571698.745399	44.308429
3502.186126	571679.550391	44.313434
3502.040161	571653.929717	44.318439
3501.561220	571647.681532	44.323444
3502.232873	571642.106584	44.328449
3502.083685	571637.763983	44.333453
3502.293426	571623.228276	44.338458
3502.223671	571600.506191	44.343463
3502.335842	571596.122717	44.348468
3502.675415	571571.479803	44.353473
3502.347019	571564.304736	44.358477
3502.436962	571548.533076	44.363482
3502.239502	571533.408526	44.368487
3502.463525	571519.974493	44.373492
3502.875303	571507.113296	44.378497
3502.708174	571480.190765	44.383501
3502.522201	571459.544104	44.388506
3502.671346	571436.185265	44.393511
3502.160536	571435.211261	44.398516
3502.414980	571397.583621	44.403521
3502.202049	571394.204390	44.408525
3502.402143	571386.745856	44.413530
3502.045236	571368.534593	44.418535
3502.050995	571359.701261	44.423540
3502.336499	571347.210915	44.428545
3502.105006	571320.749729	44.433549
3502.522426	571305.328015	44.438554
3502.805885	571293.440145	44.443559
3502.828270	571270.552446	44.448564
3502.737883	571259.425570	44.453569
3502.612976	571237.062677	44.458573
3502.089384	571218.024088	44.463578
3502.194948	571190.205098	44.468583
3502.092604	571183.797413	44.473588
3502.543934	571179.962979	44.478593
3502.214791	571161.195008	44.483597
3501.883706	571134.096550	44.488602
3502.425445	571129.194075	44.493607
3502.394180	571112.386869	44.498612
3502.279712	571084.852947	44.503617
3502.338334	571097.691276	44.508621
3502.044014	571073.848983	44.513626
3502.491499	571063.741914	44.518631
3502.047363	571057.688703	44.523636
3502.168800	571044.370520	44.528641
3502.092573	571030.230064	44.533645
3502.182232	571021.132425	44.538650
3502.574452	571003.756998	44.543655
3502.011193	570992.503043	44.548660
3502.585717	570983.981993	44.553665
3502.298603	570975.394892	44.558669
3502.158387	570949.621180	44.563674
3502.148750	570941.040862	44.568679
3502.262320	570935.603006	44.573684
3502.397481	570914.905156	44.578689
3502.193648	570901.185979	44.583693
3501.582849	570891.645690	44.588698
3502.366346	570883.142084	44.593703
3501.706954	570861.715180	44.598708
3502.076141	570850.265127	44.603713
3501.989232	570851.382823	44.608717
3502.248771	570841.957366	44.613722
3502.042377	570822.015354	44.618727
3501.838005	570812.863143	44.623732
3501.877805	570797.901273	44.628737
3502.394957	570809.012080	44.633741
3502.433989	570785.117071	44.638746
3502.504932	570773.312072	44.643751
3502.219425	570761.512597	44.648756
3501.955876	570732.846832	44.653761
3502.203538	570726.233612	44.658765
3502.206352	570722.418957	44.663770
3502.342991	570707.492018	44.668775
3501.900731	570692.454809	44.673780
3502.362345	570676.774405	44.678785
3502.157006	570677.408758	44.683789
3501.964468	570648.079245	44.688794
3502.335206	570646.616045	44.693799
3502.540735	570643.120985	44.698804
3502.550862	570609.845068	44.703809
3502.405836	570610.269247	44.708813
3502.388227	570584.475544	44.713818
3502.071569	570575.641821	44.718823
3502.412434	570556.266234	44.723828
3502.310606	570552.317318	44.728833
3502.576281	570538.474119	44.733837
3502.366576	570520.790556	44.738842
3502.062092	570494.589805	44.743847
3501.994135	570483.107349	44.748852
3501.996219	570473.772025	44.753857
3502.086728	570471.700165	44.758861
3501.981309	570456.609986	44.763866
3502.466011	570444.489023	44.768871
3502.259145	570439.452345	44.773876
3502.152270	570427.273280	44.778881
3502.078374	570405.854365	44.783885
3502.185766	570398.811188	44.788890
3502.010666	570393.066883	44.793895
3502.078979	570377.798876	44.798900
3502.231544	570368.540319	44.803905
3501.831746	570356.708103	44.808909
3502.464381	570346.270327	44.813914
3501.956172	570316.537613	44.818919
3501.680362	570313.268268	44.823924
3501.619507	570298.923749	44.828929
3501.899797	570306.458469	44.833933
3501.993510	570292.742235	44.838938
3502.192488	570279.661986	44.843943
3501.799044	570269.083412	44.848948
3502.055202	570260.310464	44.853953
3502.215473	570269.670781	44.858957
3501.464122	570243.689881	44.863962
3502.268657	570221.029132	44.868967
3502.061139	570217.297379	44.873972
3502.520311	570212.608182	44.878977
3502.018810	570201.745303	44.883981
3502.221015	570181.336782	44.888986
3502.116584	570176.484731	44.893991
3502.020772	570177.955211	44.898996
3501.981425	570158.989718	44.904001
3502.329302	570149.148366	44.909005
3502.126764	570143.307845	44.914010
3502.549973	570126.779471	44.919015
3502.124318	570111.688710	44.924020
3502.151438	570101.144613	44.929025
3502.269335	570087.926252	44.934029
3502.069680	570062.360591	44.939034
3502.329800	570054.389907	44.944039
3501.988018	570054.794673	44.949044
3502.301551	570022.021708	44.954049
3502.006867	570022.469302	44.959053
3502.288996	570008.873844	44.964058
3502.087237	570001.477231	44.969063
3501.679708	569975.441970	44.974068
3501.893719	569977.667087	44.979073
3502.145217	569972.106832	44.984077
3502.069664	569965.342941	44.989082
3501.954258	569931.833727	44.994087
3502.020362	569932.325304	44.999092
3501.947544	569924.456769	45.004097
3501.717007	569918.771082	45.009101
3502.132353	569919.709969	45.014106
3502.043159	569902.709280	45.019111
3501.615598	569891.433019	45.024116
3502.031529	569873.751031	45.029121
3501.879316	569876.334564	45.034125
3502.092559	569869.625852	45.039130
3502.129027	569848.238831	45.044135
3501.768482	569853.013149	45.049140
3502.071024	569837.858378	45.054145
3502.137906	569836.793917	45.059149
3501.935824	569821.316484	45.064154
3501.957031	569800.785009	45.069159
3501.729039	569802.226008	45.074164
3501.920701	569784.578943	45.079169
3502.130671	569783.542299	45.084173
3502.096060	569772.555830	45.089178
3501.834757	569762.959955	45.094183
3501.790873	569751.322427	45.099188
3501.959939	569739.601407	45.104193
3501.692232	569751.538624	45.109197
3501.802354	569740.780455	45.114202
3501.797841	569724.569326	45.119207
3501.928185	569724.850103	45.124212
3502.238422	569716.118478	45.129217
3502.059805	569714.791235	45.134221
3501.621101	569691.771694	45.139226
3502.163505	569684.660075	45.144231
3501.557615	569673.160518	45.149236
3501.951023	569665.620454	45.154241
3501.586285	569671.800870	45.159245
3501.602226	569675.763529	45.164250
3501.588786	569671.298573	45.169255
3501.610091	569666.276074	45.174260
3501.969922	569660.447774	45.179265
3501.774942	569635.131388	45.184269
3501.726691	569632.227807	45.189274
3502.144080	569629.954118	45.194279
3501.666373	569628.221895	45.199284
3502.268930	569620.347953	45.204289
3501.760729	569600.200033	45.209293
3501.923306	569586.622765	45.214298
3501.918154	569586.523192	45.219303
3501.947256	569587.723258	45.224308
3502.122530	569575.800331	45.229313
3501.902996	569560.325274	45.234317
3501.625395	569548.422924	45.239322
3502.071658	569541.627400	45.244327
3501.782500	569544.985300	45.249332
3502.063685	569534.150003	45.254337
3502.176514	569526.703904	45.259341
3502.217373	569512.242114	45.264346
3502.551792	569508.375215	45.269351
3501.862940	569484.792054	45.274356
3501.849799	569461.404366	45.279361
3502.120443	569460.308016	45.284365
3501.985052	569461.533810	45.289370
3502.275301	569446.531024	45.294375
3501.795560	569430.544350	45.299380
3502.141633	569415.582989	45.304385
3502.237129	569420.988891	45.309389
3502.159320	569403.032017	45.314394
3502.207824	569383.750351	45.319399
3501.918143	569379.428852	45.324404
3501.901622	569379.381247	45.329409
3501.985575	569358.136469	45.334413
3502.476524	569349.225737	45.339418
3502.511036	569331.753123	45.344423
3501.632151	569314.774628	45.349428
3502.132960	569306.213674	45.354433
3502.081616	569299.897345	45.359437
3502.052801	569293.025365	45.364442
3502.457556	569281.116451	45.369447
3502.653207	569271.197761	45.374452
3502.236047	569251.336154	45.379457
3502.266932	569233.261636	45.384461
3502.262707	569224.327830	45.389466
3502.530425	569207.270314	45.394471
3502.200979	569190.858259	45.399476
3502.472559	569170.437097	45.404481
3502.429846	569155.586372	45.409485
3502.476145	569143.331802	45.414490
3502.723242	569123.014772	45.419495
3502.236198	569117.268397	45.424500
3502.354727	569105.404049	45.429505
3502.424852	569096.107161	45.434509
3502.305704	569067.464847	45.439514
3502.295498	569053.913962	45.444519
3502.075265	569053.797813	45.449524
3502.120418	569026.384572	45.454529
3501.988811	569021.787252	45.459533
3501.728240	569013.345108	45.464538
3502.330779	569010.741189	45.469543
3502.268429	569000.260263	45.474548
3502.011351	568976.106607	45.479553
3502.574186	568973.508886	45.484557
3501.903263	568953.335071	45.489562
3502.121672	568922.330661	45.494567
3502.412805	568926.501532	45.499572
3502.177495	568920.765900	45.504577
3502.504040	568903.849323	45.509581
3502.212251	568892.400265	45.514586
3502.508173	568877.395851	45.519591
3502.365801	568855.934551	45.524596
3502.096920	568845.786942	45.529601
3502.386512	568822.501214	45.534605
3502.231710	568816.301184	45.539610
3502.468352	568813.403054	45.544615
3502.262897	568785.476266	45.549620
3502.502105	568775.700927	45.554625
3502.647058	568765.086988	45.559629
3502.358279	568740.636618	45.564634
3502.207481	568729.918294	45.569639
3502.167062	568711.352144	45.574644
3502.468189	568686.809440	45.579649
3502.123178	568687.566125	45.584653
3502.113371	568670.601396	45.589658
3502.543108	568643.629082	45.594663
3502.171418	568641.026794	45.599668
3502.546054	568625.658374	45.604673
3502.357439	568609.424256	45.609677
3502.188599	568596.399595	45.614682
3502.242017	568580.378580	45.619687
3502.087928	568573.626146	45.624692
3502.446400	568556.553480	45.629697
3502.415226	568543.055467	45.634701
3502.339159	568533.831177	45.639706
3502.384409	568514.950137	45.644711
3502.205951	568488.875688	45.649716
3502.254691	568481.338539	45.654721
3502.345893	568477.007351	45.659725
3502.004185	568451.962278	45.664730
3502.419363	568435.784115	45.669735
3502.234602	568438.021677	45.674740
3502.551504	568419.449393	45.679745
3502.110060	568403.656086	45.684749
3502.184938	568408.413124	45.689754
3502.119125	568382.170233	45.694759
3501.971973	568373.760084	45.699764
3501.989941	568364.069180	45.704769
3502.133542	568358.776005	45.709773
3502.044950	568344.935354	45.714778
3502.099940	568324.897937	45.719783
3502.073590	568322.693367	45.724788
3502.034648	568309.899062	45.729793
3501.991674	568306.040565	45.734797
3501.755278	568285.898039	45.739802
3502.157624	568274.440246	45.744807
3501.949537	568277.083067	45.749812
3502.189671	568269.817046	45.754817
3502.198628	568248.481548	45.759821
3502.285264	568178.240885	45.764826
3502.417547	568061.207518	45.769831
3501.744154	567905.494822	45.774836
3501.249909	567703.869027	45.779841
3500.962305	567447.588388	45.784845
3500.909161	567156.926827	45.789850
3500.638687	566818.397272	45.794855
3499.666303	566432.623551	45.799860
3499.325897	566003.609863	45.804865
3498.297160	565528.997153	45.809869
3497.981871	565007.004132	45.814874
3497.152839	564434.903885	45.819879
3496.200945	563839.795401	45.824884
3494.973429	563186.043077	45.829889
3494.219196	562499.284379	45.834893
3493.151494	561777.225758	45.839898
3492.228673	561007.985306	45.844903
3490.378750	560199.608005	45.849908
3489.285490	559356.846322	45.854913
3487.906945	558466.944336	45.859917
3486.452042	557552.669663	45.864922
3485.149922	556581.520993	45.869927
3483.262339	555604.354708	45.874932
3481.708667	554573.634266	45.879937
3480.253617	553517.579254	45.884941
3478.414075	552421.782489	45.889946
3476.640846	551291.994349	45.894951
3474.584783	550131.176259	45.899956
3472.727019	548933.261276	45.904961
3470.602770	547712.642767	45.909965
3468.818297	546467.710979	45.914970
3466.628061	545182.028624	45.919975
3464.013206	543876.762919	45.924980
3461.985532	542532.181238	45.929985
3459.758175	541179.637782	45.934989
3457.135326	539797.273569	45.939994
3454.686124	538385.242122	45.944999
3451.573643	536959.971349	45.950004
3449.832112	535499.697459	45.955009
3447.158307	534039.050545	45.960013
3444.281220	532537.590923	45.965018
3441.828925	531022.295944	45.970023
3438.976081	529503.966419	45.975028
3436.309979	527952.443832	45.980033
3433.540745	526385.744416	45.985037
3430.482255	524801.071907	45.990042
3427.505108	523209.094103	45.995047
3424.481295	521591.085575	46.000052
3421.456641	519955.698478	46.005057
3418.531686	518319.896457	46.010061
3415.106880	516674.852564	46.015066
3412.433785	515007.413262	46.020071
3409.231851	513340.762219	46.025076
3405.893018	511648.921994	46.030081
3402.672661	509947.024086	46.035085
3399.357664	508249.675397	46.040090
3396.239830	506517.438188	46.045095
3392.793140	504807.339140	46.050100
3389.613935	503057.740433	46.055105
3386.297455	501320.363646	46.060109
3382.849745	499571.797314	46.065114
3379.609180	497798.005075	46.070119
3376.115372	496049.529661	46.075124
3372.971438	494270.249615	46.080129
3369.048231	492474.974139	46.085133
3365.360450	490691.212400	46.090138
3362.128382	488896.866016	46.095143
3358.251330	487114.480075	46.100148
3354.919484	485322.102531	46.105153
3351.228274	483520.630657	46.110157
3347.574495	481725.562757	46.115162
3344.293417	479918.456603	46.120167
3340.546720	478114.298712	46.125172
3337.060329	476298.826002	46.130177
3333.307219	474493.045873	46.135181
3329.609602	472685.436855	46.140186
3325.920652	470868.524287	46.145191
3321.994068	469063.329960	46.150196
3318.483833	467245.887349	46.155201
3315.065706	465429.192383	46.160205
3310.779679	463613.902794	46.165210
3307.122027	461795.486652	46.170215
3303.433056	459991.957658	46.175220
3299.976294	458173.933774	46.180225
3296.358035	456357.464326	46.185229
3292.178680	454554.759984	46.190234
3288.828713	452729.369359	46.195239
3284.601069	450921.695113	46.200244
3280.806407	449108.454472	46.205249
3277.078356	447299.881130	46.210253
3273.455543	445500.630358	46.215258
3269.929541	443688.325085	46.220263
3265.829768	441897.860584	46.225268
3261.743955	440090.152811	46.230273
3258.017870	438287.330760	46.235277
3254.322086	436493.805529	46.240282
3250.886912	434696.828645	46.245287
3246.633428	432908.121720	46.250292
3242.707094	431115.347866	46.255297
3239.107442	429325.501039	46.260301
3235.383305	427544.330462	46.265306
3231.627564	425762.955224	46.270311
3227.626014	423987.239684	46.275316
3223.816125	422206.522991	46.280321
3220.066932	420433.551438	46.285325
3216.488739	418662.885852	46.290330
3212.464715	416891.987849	46.295335
3208.917845	415132.226234	46.300340
3204.988314	413366.140880	46.305345
3201.341635	411600.779213	46.310349
3197.180499	409831.397874	46.315354
3193.568982	408071.882881	46.320359
3189.580944	406318.222690	46.325364
3185.675679	404574.305720	46.330369
3182.244646	402816.733517	46.335373
3178.134661	401080.241896	46.340378
3174.287593	399336.371926	46.345383
3170.353576	397606.341775	46.350388
3166.418064	395871.667219	46.355393
3163.060504	394149.211742	46.360397
3159.058422	392419.169645	46.365402
3155.210399	390697.356574	46.370407
3151.226070	388967.929769	46.375412
3147.281863	387260.361109	46.380417
3143.970699	385553.110131	46.385421
3139.781537	383849.918329	46.390426
3136.348053	382141.213366	46.395431
3132.455569	380445.925993	46.400436
3128.059287	378750.963000	46.405441
3124.408508	377055.952532	46.410445
3120.696835	375365.365088	46.415450
3117.204318	373683.324561	46.420455
3113.066663	372003.974061	46.425460
3109.368710	370326.561340	46.430465
3105.922571	368656.782599	46.435469
3102.226713	366981.634540	46.440474
3098.531246	365305.016484	46.445479
3094.725526	363645.368358	46.450484
3090.781391	361983.284855	46.455489
3087.011440	360316.913572	46.460493
3083.229119	358650.223210	46.465498
3079.241667	356989.192092	46.470503
3075.542293	355345.029946	46.475508
3071.791794	353693.621542	46.480513
3068.015295	352047.392749	46.485517
3064.472942	350416.167813	46.490522
3060.744519	348763.815729	46.495527
3057.122899	347132.185196	46.500532
3053.230322	345497.771479	46.505537
3049.346136	343858.090756	46.510541
3045.533354	342242.043242	46.515546
3041.769332	340610.478517	46.520551
3038.352604	338993.837782	46.525556
3034.521076	337369.712501	46.530561
3030.769517	335751.198573	46.535565
3026.821837	334148.284892	46.540570
3023.044794	332531.516472	46.545575
3019.411429	330938.259620	46.550580
3015.941766	329321.485425	46.555585
3012.309100	327723.696238	46.560589
3008.389349	326123.318532	46.565594
3004.727573	324525.813314	46.570599
3000.953537	322934.597815	46.575604
2996.875496	321332.913193	46.580609
2993.653230	319747.952606	46.585613
2989.429474	318159.655672	46.590618
2986.008085	316582.599633	46.595623
2982.210363	315004.020053	46.600628
2978.673084	313425.904631	46.605633
2975.165762	311841.114761	46.610637
2970.957674	310270.351223	46.615642
2967.892092	308694.191730	46.620647
2964.116201	307130.282099	46.625652
2960.291436	305570.351895	46.630657
2956.362759	303995.730960	46.635661
2952.215865	302445.401421	46.640666
2948.745509	300885.350910	46.645671
2944.881790	299338.857171	46.650676
2941.010046	297789.470518	46.655681
2937.413090	296246.539671	46.660685
2933.638898	294709.449494	46.665690
2930.043429	293167.378362	46.670695
2926.340592	291633.200996	46.675700
2922.853972	290109.490238	46.680705
2919.336122	288568.386076	46.685709
2915.832318	287043.713592	46.690714
2911.980218	285513.052322	46.695719
2907.980928	283991.697164	46.700724
2904.449687	282451.981479	46.705729
2900.980303	280941.781184	46.710733
2897.124607	279434.716253	46.715738
2893.252886	277907.713617	46.720743
2889.633854	276394.695751	46.725748
2885.837727	274876.024439	46.730753
2882.530509	273363.232119	46.735757
2878.622219	271859.673204	46.740762
2875.185665	270346.746244	46.745767
2871.056102	268840.904696	46.750772
2867.562352	267345.328575	46.755777
2864.091285	265847.153952	46.760781
2860.259620	264359.097217	46.765786
2856.517530	262863.365834	46.770791
2853.049571	261380.354345	46.775796
2849.373128	259893.663491	46.780801
2845.928885	258400.933109	46.785805
2842.290388	256918.681466	46.790810
2838.805751	255435.777490	46.795815
2834.541757	253953.844961	46.800820
2831.369405	252469.179552	46.805825
2827.463995	250991.159066	46.810829
2823.591395	249519.868444	46.815834
2820.445993	248047.839965	46.820839
2816.637554	246574.629657	46.825844
2813.024229	245096.462166	46.830849
2809.814733	243627.032779	46.835853
2805.579424	242156.251440	46.840858
2802.271625	240686.436644	46.845863
2798.376937	239224.091269	46.850868
2794.752234	237766.942828	46.855873
2791.266302	236296.649759	46.860877
2787.528665	234854.507678	46.865882
2784.069673	233391.509028	46.870887
2780.447043	231923.947246	46.875892
2776.615412	230467.824678	46.880897
2773.181258	229006.925416	46.885901
2769.162106	227564.682562	46.890906
2765.579814	226125.783004	46.895911
2761.721218	224683.487839	46.900916
2758.069437	223238.791941	46.905921
2754.788360	221803.666328	46.910925
2750.903251	220371.489394	46.915930
2747.677226	218933.455793	46.920935
2743.192407	217488.898424	46.925940
2740.093324	216064.936245	46.930945
2736.615283	214634.390502	46.935949
2733.081520	213199.019697	46.940954
2729.179924	211773.110319	46.945959
2725.607593	210350.925413	46.950964
2721.672622	208932.191819	46.955969
2718.219071	207508.246358	46.960973
2714.761080	206088.996437	46.965978
2711.213934	204673.590012	46.970983
2707.468908	203255.346732	46.975988
2703.857354	201843.129114	46.980993
2700.394906	200424.761958	46.985997
2696.493165	199009.480773	46.991002
2693.042866	197605.372601	46.996007
2689.129145	196188.362303	47.001012
2685.088732	194786.920423	47.006017
2681.657547	193395.482349	47.011021
2678.159301	191996.735698	47.016026
2674.494498	190598.591202	47.021031
2670.922271	189207.426172	47.026036
2667.461567	187820.946225	47.031041
2663.740119	186434.982976	47.036045
2659.996412	185058.106609	47.041050
2656.530502	183664.297488	47.046055
2652.629194	182272.944279	47.051060
2649.251103	180894.897600	47.056065
2645.627762	179512.479357	47.061069
2642.150444	178137.800121	47.066074
2638.384619	176752.366499	47.071079
2634.625494	175382.371411	47.076084
2630.959105	174011.188017	47.081089
2627.816498	172632.066214	47.086093
2623.887834	171268.215059	47.091098
2620.705352	169884.044110	47.096103
2616.915241	168526.522474	47.101108
2613.304667	167170.462172	47.106113
2609.426593	165801.677120	47.111117
2606.054917	164433.565626	47.116122
2602.422692	163070.957792	47.121127
2598.795946	161712.323085	47.126132
2595.011883	160342.910138	47.131137
2591.646280	158986.736503	47.136141
2587.629939	157639.450927	47.141146
2584.042657	156282.455623	47.146151
2580.262518	154936.301189	47.151156
2576.411882	153591.550689	47.156161
2573.166479	152243.212047	47.161165
2569.414306	150905.025911	47.166170
2565.966598	149563.147014	47.171175
2562.486520	148230.608729	47.176180
2558.724117	146890.831197	47.181185
2555.333933	145553.307578	47.186189
2551.824763	144134.478167	47.191194
2548.218234	142795.953948	47.196199
2544.705429	141474.997105	47.201204
2540.705723	140145.462210	47.206209
2537.321087	138810.664262	47.211213
2533.679772	137479.900884	47.216218
2530.381609	136161.678695	47.221223
2526.459082	134837.778203	47.226228
2522.758326	133510.981342	47.231233
2519.033427	132193.590518	47.236237
2515.816155	130875.205798	47.241242
2511.875656	129551.097611	47.246247
2508.743372	128242.244305	47.251252
2505.142137	126922.922441	47.256257
2501.688879	125612.840709	47.261261
2497.688915	124304.679735	47.266266
2494.263073	122980.013851	47.271271
2490.492417	121683.056334	47.276276
2486.837067	120376.063997	47.281281
2483.328321	119066.282187	47.286285
2479.645694	117764.291189	47.291290
2476.095458	116460.162415	47.296295
2472.450936	115163.430706	47.301300
2468.695172	113860.734773	47.306305
2465.218636	112565.009222	47.311309
2461.501315	111271.669031	47.316314
2458.363169	109969.690440	47.321319
2454.717071	108682.586774	47.326324
2450.638811	107390.703617	47.331329
2447.370495	106103.140536	47.336333
2443.602780	104828.161770	47.341338
2440.063542	103535.793287	47.346343
2436.744308	102250.761813	47.351348
2432.750785	100971.198660	47.356353
2429.408823	99692.905379	47.361357
2425.306620	98418.123991	47.366362
2421.721482	97133.386613	47.371367
2418.009421	95875.408815	47.376372
2414.372488	94607.862325	47.381377
2411.022912	93338.657763	47.386381
2406.680346	92081.096965	47.391386
2403.194340	90817.952049	47.396391
2399.778441	89562.192856	47.401396
2395.597913	88305.525900	47.406401
2392.386021	87056.637544	47.411405
2388.885931	85822.304690	47.416410
2385.127516	84584.443902	47.421415
2381.359248	83346.955224	47.426420
2377.781343	82112.221261	47.431425
2374.516759	80874.075082	47.436429
2370.466003	79650.992487	47.441434
2367.246514	78416.618480	47.446439
2363.507739	77186.470258	47.451444
2359.261947	75966.857624	47.456449
2356.109560	74742.683839	47.461453
2352.444279	73535.154059	47.466458
2348.858593	72322.942571	47.471463
2345.362002	71106.112460	47.476468
2341.372259	69898.176557	47.481473
2338.059384	68691.396721	47.486477
2334.233398	67493.570487	47.491482
2330.933403	66283.009842	47.496487
2327.171529	65078.678551	47.501492
2323.559183	63879.763320	47.506497
2320.067482	62680.296105	47.511501
2316.456349	61493.153683	47.516506
2312.807451	60301.086019	47.521511
2309.234817	59113.563320	47.526516
2305.340277	57930.711093	47.531521
2301.352865	56740.056780	47.536525
2298.133781	55571.040455	47.541530
2294.303756	54388.853384	47.546535
2290.799521	53221.824166	47.551540
2286.837274	52051.340077	47.556545
2283.512992	50888.769536	47.561549
2279.646843	49728.397100	47.566554
2276.063623	48566.148506	47.571559
2272.682426	47403.464174	47.576564
2268.539326	46250.643025	47.581569
2265.540421	45093.293913	47.586573
2261.638353	43955.798378	47.591578
2257.713997	42808.902991	47.596583
2254.262696	41679.322759	47.601588
2250.647654	40547.638439	47.606593
2247.094833	39403.030468	47.611597
2243.142258	38282.954173	47.616602
2239.328143	37150.444013	47.621607
2235.638930	36031.299201	47.626612
2231.689759	34923.169388	47.631617
2228.253050	33808.862289	47.636621
2224.230000	32701.551075	47.641626
2220.648247	31607.754498	47.646631
2216.587929	30517.303262	47.651636
2212.959235	29430.219554	47.656641
2209.277929	28353.651038	47.661645
2205.173746	27280.018602	47.666650
2201.034824	26208.488350	47.671655
2197.331714	25148.344953	47.676660
2193.033128	24102.852759	47.681665
2189.557936	23065.002624	47.686669
2185.267543	22043.374244	47.691674
2181.307603	21022.886908	47.696679
2177.128910	20021.261587	47.701684
2173.025744	19029.043524	47.706689
2168.974631	18048.122675	47.711693
2164.218951	17095.386926	47.716698
2159.333162	16164.928670	47.721703
2154.026158	15272.955048	47.726708
2147.823933	14399.650815	47.731713
2142.632314	13558.627449	47.736717
2137.793456	12762.400834	47.741722
2132.431532	11987.592662	47.746727
2127.202639	11254.475755	47.751732
2122.217947	10544.195573	47.756737
2117.194769	9866.559488	47.761741
2111.940897	9238.817147	47.766746
2106.422949	8622.124058	47.771751
2101.603977	8063.404729	47.776756
2095.991400	7544.786124	47.781761
2091.218388	7041.442308	47.786765
2085.541742	6584.465210	47.791770
2080.631217	6152.331575	47.796775
2075.982110	5757.787418	47.801780
2071.607349	5393.122115	47.806785
2067.344458	5038.238153	47.811789
2063.350759	4703.999884	47.816794
2059.425477	4403.643419	47.821799
2055.322193	4105.800760	47.826804
2051.529647	3823.812743	47.831809
2048.241686	3547.819549	47.836813
2044.147317	3291.481042	47.841818
2040.964545	3054.236461	47.846823
2037.499379	2804.065504	47.851828
2034.485413	2570.914458	47.856833
2031.379482	2321.829948	47.861837
2027.787782	2091.784676	47.866842
2024.422809	1876.701758	47.871847
2021.425668	1648.388512	47.876852
2017.650660	1431.742403	47.881857
2014.975727	1204.485481	47.886861
2011.488758	994.943962	47.891866
2008.289272	779.206021	47.896871
2004.477840	559.310971	47.901876
2000.143771	370.057155	47.906881
1996.023146	179.477938	47.911885
1988.020085	112.954405	47.916890
1977.781574	128.654560	47.921895
1971.299084	129.469609	47.926900
1966.588486	132.639712	47.931905
1964.219339	131.963207	47.936909
1962.414033	132.910110	47.941914
1960.192383	135.004196	47.946919
1957.975923	134.984026	47.951924
1955.029845	125.403009	47.956929
1951.801654	123.320141	47.961933
1948.451557	131.956449	47.966938
1945.094065	124.341281	47.971943
1942.195960	123.870943	47.976948
1938.629646	129.605046	47.981953
1935.634211	133.193324	47.986957
1931.840330	133.565533	47.991962
1928.530227	123.415050	47.996967
1925.693052	131.752795	48.001972
1922.262607	137.538412	48.006977
1918.746083	136.076491	48.011981
1915.803950	126.630915	48.016986
1912.182869	135.521615	48.021991
1909.104931	132.716040	48.026996
1905.252811	136.333977	48.032001
1901.717249	133.726568	48.037005
1897.794975	142.544181	48.042010
1894.844960	133.447865	48.047015
1892.329747	125.925545	48.052020
1888.539761	139.540981	48.057025
1884.868624	127.953677	48.062029
1881.322480	138.117177	48.067034
1877.547768	135.854093	48.072039
1874.785677	133.799553	48.077044
1871.411685	135.169125	48.082049
1867.792602	131.220677	48.087053
1864.263194	127.087350	48.092058
1861.132611	126.330704	48.097063
1857.522378	127.525271	48.102068
1853.747927	123.439788	48.107073
1850.443711	129.506233	48.112077
1846.864353	136.346584	48.117082
1843.631671	128.424013	48.122087
1840.338167	131.979864	48.127092
1836.720742	132.713645	48.132097
1833.370492	125.448572	48.137101
1829.861543	132.151354	48.142106
1826.572800	130.511447	48.147111
1823.085826	135.002437	48.152116
1819.776936	130.201850	48.157121
1815.656198	125.683342	48.162125
1812.313666	137.817702	48.167130
1808.816910	134.679057	48.172135
1805.352425	129.804746	48.177140
1802.407133	135.498653	48.182145
1798.440940	134.284319	48.187149
1795.257038	131.900334	48.192154
1791.718554	130.650707	48.197159
1788.511962	130.190722	48.202164
1784.838866	130.803515	48.207169
1781.635703	124.992954	48.212173
1778.195655	125.752781	48.217178
1774.333319	126.971011	48.222183
1771.100983	120.177905	48.227188
1767.533962	129.708766	48.232193
1763.886129	125.923049	48.237197
1760.462411	128.325519	48.242202
1756.720823	119.520822	48.247207
1753.647761	121.495085	48.252212
1749.625886	123.722242	48.257217
1746.098195	130.535551	48.262221
1743.145818	124.413666	48.267226
1739.752468	126.839864	48.272231
1736.375976	121.594298	48.277236
1732.546903	121.804403	48.282241
1729.388042	120.625105	48.287245
1725.821218	117.364578	48.292250
1722.138872	127.457677	48.297255
1718.921772	118.612044	48.302260
1715.134905	119.324927	48.307265
1711.912955	122.989840	48.312269
1708.127740	128.432393	48.317274
1704.561158	124.121443	48.322279
1701.286501	121.609321	48.327284
1697.861501	123.888621	48.332289
1694.262995	128.469871	48.337293
1690.700137	128.423187	48.342298
1687.238684	120.995237	48.347303
1683.954354	120.231069	48.352308
1680.152128	122.692802	48.357313
1676.571956	121.465560	48.362317
1673.359460	118.655811	48.367322
1669.878707	120.165543	48.372327
1666.491402	118.085526	48.377332
1662.908842	124.698630	48.382337
1659.363345	125.573078	48.387341
1655.785854	127.480779	48.392346
1652.572500	118.824415	48.397351
1648.919072	113.429233	48.402356
1645.198673	123.733955	48.407361
1642.215369	121.865968	48.412365
1638.526213	117.444513	48.417370
1634.695682	124.188186	48.422375
1631.396146	123.537149	48.427380
1628.052634	117.207597	48.432385
1624.687642	115.067153	48.437389
1620.919033	122.883168	48.442394
1617.450038	123.375488	48.447399
1614.015574	120.144908	48.452404
1610.290211	129.972682	48.457409
1606.700256	122.226347	48.462413
1603.394063	121.098623	48.467418
1600.150460	117.559760	48.472423
1596.901155	119.912835	48.477428
1592.966565	117.779292	48.482433
1589.935291	113.593419	48.487437
1586.390495	119.890579	48.492442
1582.486726	127.775218	48.497447
1579.065855	117.525156	48.502452
1575.423409	114.361946	48.507457
1571.663793	111.172784	48.512461
1568.604659	111.945828	48.517466
1565.021967	109.263663	48.522471
1561.522471	113.478270	48.527476
1558.332366	119.558567	48.532481
1554.815204	110.968780	48.537485
1551.209503	121.537155	48.542490
1547.579578	129.293521	48.547495
1544.155343	119.161061	48.552500
1540.451419	126.198167	48.557505
1537.134299	120.554233	48.562509
1533.513255	126.588092	48.567514
1530.169536	113.918306	48.572519
1526.881661	120.494816	48.577524
1522.811798	119.148120	48.582529
1519.436895	120.410375	48.587533
1515.857857	107.815398	48.592538
1512.408358	117.321597	48.597543
1509.044565	110.950975	48.602548
1505.634839	109.782541	48.607553
1502.062740	115.739142	48.612557
1498.674549	115.766428	48.617562
1495.194542	116.931244	48.622567
1491.883554	110.846599	48.627572
1488.317638	113.116382	48.632577
1484.665203	113.289440	48.637581
1481.243273	115.324713	48.642586
1478.006922	117.106308	48.647591
1474.579467	116.601898	48.652596
1470.347250	118.308415	48.657601
1467.270466	122.004460	48.662605
1463.507004	111.472710	48.667610
1459.933312	113.016042	48.672615
1456.647023	118.665322	48.677620
1453.144958	116.169899	48.682625
1449.466597	118.090294	48.687629
1446.307310	116.509349	48.692634
1443.085013	114.159967	48.697639
1439.356188	110.769881	48.702644
1435.403220	123.373196	48.707649
1431.907377	116.064633	48.712653
1428.927356	127.196345	48.717658
1424.991223	115.593792	48.722663
1421.945572	113.621737	48.727668
1418.094795	116.271499	48.732673
1414.640825	116.429335	48.737677
1410.982575	111.009696	48.742682
1407.181802	112.015939	48.747687
1404.409437	111.143251	48.752692
1400.595895	111.610482	48.757697
1397.370333	106.876109	48.762701
1393.695024	115.050916	48.767706
1389.868326	112.027354	48.772711
1386.480288	115.028644	48.777716
1383.080418	121.958090	48.782721
1379.813943	122.374497	48.787725
1376.282314	115.628391	48.792730
1372.527952	113.115543	48.797735
1369.100610	109.013891	48.802740
1365.512751	121.914421	48.807745
1362.211910	109.655625	48.812749
1358.766008	107.214723	48.817754
1354.851239	118.144746	48.822759
1351.985103	117.286751	48.827764
1348.379000	121.980032	48.832769
1344.653445	108.604459	48.837773
1341.196254	114.239394	48.842778
1337.597539	117.909608	48.847783
1334.116886	110.747410	48.852788
1330.641586	114.565987	48.857793
1327.060555	106.963917	48.862797
1323.725856	111.048394	48.867802
1320.021696	114.447212	48.872807
1317.125957	103.039369	48.877812
1312.752311	111.187472	48.882817
1309.500741	101.300184	48.887821
1306.064569	108.785833	48.892826
1302.677079	108.297374	48.897831
1299.400397	102.808561	48.902836
1295.764323	107.202821	48.907841
1292.012917	103.901754	48.912845
1288.809755	104.811325	48.917850
1284.816413	106.955095	48.922855
1281.844021	107.980407	48.927860
1278.036447	108.427768	48.932865
1274.723191	93.655733	48.937869
1271.512465	102.476028	48.942874
1267.606086	104.289809	48.947879
1264.341212	106.069607	48.952884
1260.836707	109.449844	48.957889
1256.598207	102.833435	48.962893
1253.259294	111.186579	48.967898
1249.794164	110.362273	48.972903
1246.610396	100.980099	48.977908
1243.250834	112.585715	48.982913
1239.755492	105.267667	48.987917
1236.522076	112.284990	48.992922
1232.570585	104.351808	48.997927
1228.963439	101.566032	49.002932
1225.142895	108.381037	49.007937
1221.957786	103.747966	49.012941
1218.524615	99.998470	49.017946
1214.604068	108.907759	49.022951
1211.882571	98.624311	49.027956
1208.415924	113.888249	49.032961
1204.511250	110.408727	49.037965
1201.473385	114.548014	49.042970
1197.760780	122.912223	49.047975
1194.273812	115.934571	49.052980
1190.408037	112.360378	49.057985
1187.172574	110.389641	49.062989
1183.784569	107.142460	49.067994
1179.801772	111.293642	49.072999
1176.478492	97.374284	49.078004
1172.886928	111.971238	49.083009
1169.530868	109.101882	49.088013
1165.997033	102.014524	49.093018
1162.570663	112.852322	49.098023
1159.179451	113.395899	49.103028
1155.404344	115.575158	49.108033
1152.305892	117.382722	49.113037
1148.842818	115.469779	49.118042
1145.180236	121.820315	49.123047
1141.726692	115.312025	49.128052
1137.984668	115.755505	49.133057
1134.242370	111.285629	49.138061
1131.066345	108.584258	49.143066
1127.263555	122.366398	49.148071
1123.936282	109.545524	49.153076
1120.768304	113.483737	49.158081
1117.327707	109.494991	49.163085
1113.922869	102.184975	49.168090
1109.791195	109.108842	49.173095
1106.759536	104.973818	49.178100
1102.911895	106.829088	49.183105
1099.516947	107.800385	49.188109
1095.991038	106.700909	49.193114
1092.160841	107.253126	49.198119
1088.787634	104.310554	49.203124
1085.187099	103.342990	49.208129
1081.891841	105.431329	49.213133
1079.017774	104.887876	49.218138
1075.027228	99.805151	49.223143
1071.989589	98.338167	49.228148
1067.907698	105.633911	49.233153
1064.262361	92.062432	49.238157
1061.188009	97.147117	49.243162
1057.283384	110.464314	49.248167
1054.148924	97.705043	49.253172
1050.371730	102.390402	49.258177
1047.024455	95.504847	49.263181
1043.507486	99.038969	49.268186
1039.848746	105.838193	49.273191
1036.047603	100.811253	49.278196
1032.587863	104.409187	49.283201
1029.852037	97.121014	49.288205
1026.361819	102.884602	49.293210
1023.021724	108.279832	49.298215
1019.369665	105.475860	49.303220
1015.335090	101.671906	49.308225
1011.880951	107.701938	49.313229
1008.099292	98.786805	49.318234
1004.854998	104.828276	49.323239
1001.499657	96.213399	49.328244
997.930155	96.595120	49.333249
994.504643	97.644006	49.338253
991.014353	98.320216	49.343258
987.236153	100.500021	49.348263
984.168780	90.966855	49.353268
980.229663	93.152875	49.358273
976.883455	92.072765	49.363277
973.890904	94.249786	49.368282
969.742090	102.451399	49.373287
966.576957	93.926981	49.378292
962.409838	101.584125	49.383297
959.143814	96.590495	49.388301
955.830293	99.725789	49.393306
952.416423	100.026210	49.398311
949.005788	96.124592	49.403316
945.376977	91.282688	49.408321
941.784595	101.969358	49.413325
938.646312	94.873951	49.418330
935.210549	99.509053	49.423335
931.646504	97.365228	49.428340
928.427590	100.321200	49.433345
924.396657	101.933152	49.438349
921.093224	98.527295	49.443354
917.009180	102.919059	49.448359
913.731036	105.137653	49.453364
910.321211	98.783975	49.458369
906.936873	96.668969	49.463373
903.436954	93.398292	49.468378
899.746718	101.581910	49.473383
896.428658	95.963691	49.478388
892.769561	101.522807	49.483393
889.160634	107.159492	49.488397
885.875044	96.777832	49.493402
882.259374	101.947331	49.498407
878.665381	98.754670	49.503412
875.393620	95.059130	49.508417
871.882291	95.488737	49.513421
868.470500	99.231079	49.518426
864.966039	101.659136	49.523431
861.377885	101.613551	49.528436
857.615563	100.601806	49.533441
854.438957	97.492496	49.538445
850.756767	103.441226	49.543450
847.048881	99.813988	49.548455
843.762499	96.278940	49.553460
840.374204	97.451769	49.558465
836.968262	94.878258	49.563469
833.481726	102.580740	49.568474
829.743378	107.168347	49.573479
826.456941	100.010759	49.578484
822.901291	104.753258	49.583489
819.322717	90.073610	49.588493
815.693026	93.429305	49.593498
812.106043	104.001271	49.598503
808.632455	94.421053	49.603508
805.156387	100.248935	49.608513
801.964913	95.854305	49.613517
798.655991	89.415273	49.618522
794.613259	100.511034	49.623527
790.892069	94.180855	49.628532
787.899388	99.395200	49.633537
784.472104	92.047714	49.638541
781.015134	84.182855	49.643546
777.039944	98.131281	49.648551
774.235410	98.045276	49.653556
770.261147	92.131230	49.658561
766.774459	97.312207	49.663565
763.235608	93.171311	49.668570
759.644641	95.537021	49.673575
756.477904	84.852071	49.678580
752.813687	89.877352	49.683585
749.288714	93.317913	49.688589
745.630387	99.516045	49.693594
742.152861	104.869607	49.698599
739.140724	87.886638	49.703604
735.498299	95.341473	49.708609
731.617267	98.904240	49.713613
728.008136	91.651696	49.718618
724.467911	93.579196	49.723623
721.529194	86.829118	49.728628
717.835343	83.392733	49.733633
714.284695	96.853908	49.738637
710.654621	86.108658	49.743642
706.906467	101.381984	49.748647
703.955882	85.781466	49.753652
699.991496	89.591419	49.758657
696.760180	88.287773	49.763661
693.470738	90.688545	49.768666
689.818940	99.217391	49.773671
686.088452	89.405378	49.778676
682.343611	88.878193	49.783681
678.729928	90.377446	49.788685
675.846759	96.640870	49.793690
672.321256	100.439052	49.798695
669.031463	86.511536	49.803700
665.431327	91.498338	49.808705
661.523379	90.591740	49.813709
658.204248	96.151478	49.818714
654.518318	96.864778	49.823719
651.345411	89.635703	49.828724
647.458132	94.806689	49.833729
643.816003	93.001080	49.838733
640.949123	91.561284	49.843738
636.846619	89.353209	49.848743
633.729264	90.872826	49.853748
630.039085	80.579963	49.858753
626.344046	87.021166	49.863757
623.275521	82.335268	49.868762
619.579364	88.903201	49.873767
616.228046	82.448740	49.878772
612.610412	83.094413	49.883777
609.367615	94.719857	49.888781
606.115934	80.593416	49.893786
602.081578	86.227218	49.898791
598.831993	91.358461	49.903796
595.227641	89.287525	49.908801
591.102637	86.494530	49.913805
587.911960	84.833379	49.918810
584.191348	87.273241	49.923815
581.234690	81.908606	49.928820
577.647244	87.491407	49.933825
574.445751	84.692989	49.938829
570.786921	83.323467	49.943834
566.972234	86.996130	49.948839
563.560409	89.909665	49.953844
560.302136	90.483255	49.958849
556.656844	80.825649	49.963853
553.058953	80.911425	49.968858
549.207737	86.146401	49.973863
546.030150	82.433078	49.978868
542.594693	79.845325	49.983873
539.045920	93.056311	49.988877
535.612196	91.543977	49.993882
531.784568	90.242037	49.998887
528.586444	90.575262	50.003892
525.087049	94.894595	50.008897
521.359203	92.270385	50.013901
518.175645	93.667529	50.018906
514.362536	96.226313	50.023911
510.939584	92.719112	50.028916
507.508596	90.798232	50.033921
503.824101	102.442268	50.038925
500.516889	89.688163	50.043930
496.582897	98.017659	50.048935
493.446329	85.920212	50.053940
490.214908	88.163267	50.058945
486.547723	95.903641	50.063949
483.273392	86.909308	50.068954
479.668120	97.572821	50.073959
476.053071	80.032678	50.078964
472.682443	96.265674	50.083969
469.201716	87.360623	50.088973
465.762393	85.532815	50.093978
461.572906	91.096059	50.098983
458.214998	81.526366	50.103988
454.850632	90.358281	50.108993
451.343876	95.495051	50.113997
448.287557	90.114435	50.119002
444.192596	90.309749	50.124007
440.919993	94.308847	50.129012
437.369564	87.879321	50.134017
433.877879	89.264645	50.139021
430.678276	87.592294	50.144026
426.937494	93.177020	50.149031
423.544138	81.195761	50.154036
420.026488	92.927580	50.159041
416.303272	96.848571	50.164045
413.162877	90.044777	50.169050
409.192215	100.297306	50.174055
406.057422	86.595578	50.179060
402.806178	81.353084	50.184065
398.960751	87.779959	50.189069
395.378770	86.303558	50.194074
391.585564	84.104101	50.199079
388.339477	86.631064	50.204084
384.747490	82.375268	50.209089
381.203626	91.475770	50.214093
378.238768	83.309379	50.219098
374.350107	85.734518	50.224103
370.793654	85.190610	50.229108
367.280865	81.798785	50.234113
363.691313	83.107716	50.239117
360.283844	73.438267	50.244122
357.156124	80.863220	50.249127
353.835681	83.658109	50.254132
350.089089	87.067088	50.259137
345.982237	83.186190	50.264141
342.861824	76.882343	50.269146
339.008795	87.141773	50.274151
335.891692	85.386932	50.279156
332.526498	81.627148	50.284161
329.019747	83.419836	50.289165
325.302682	86.020598	50.294170
321.872387	90.519005	50.299175
318.399532	85.627637	50.304180
314.748849	90.410508	50.309185
311.197210	86.920386	50.314189
308.128617	91.814559	50.319194
304.328237	86.117117	50.324199
301.082564	76.346419	50.329204
297.474850	78.873113	50.334209
293.293596	80.983448	50.339213
290.157837	73.378549	50.344218
286.544573	80.974496	50.349223
283.148192	79.725336	50.354228
280.068340	89.142327	50.359233
276.144831	78.728005	50.364237
272.981912	81.378022	50.369242
269.362545	76.718439	50.374247
265.710860	86.418002	50.379252
262.378431	94.425554	50.384257
258.725729	87.759028	50.389261
255.151060	90.334348	50.394266
251.380379	93.168168	50.399271
248.505759	86.737265	50.404276
244.762788	80.524655	50.409281
241.546883	89.570661	50.414285
237.643593	83.177522	50.419290
234.223114	90.439568	50.424295
230.687415	86.757157	50.429300
227.242620	83.272481	50.434305
223.793344	86.299572	50.439309
220.603371	79.563741	50.444314
216.649234	83.916454	50.449319
213.200540	88.515858	50.454324
209.552907	90.507834	50.459329
206.027439	92.569260	50.464333
202.968601	82.348550	50.469338
199.343249	92.274969	50.474343
195.901853	81.177715	50.479348
192.483464	81.874599	50.484353
188.558198	85.599537	50.489357
185.093272	82.491359	50.494362
181.189274	82.150673	50.499367
178.000249	95.080776	50.504372
174.822648	84.625580	50.509377
171.159143	85.288106	50.514381
167.468691	82.734127	50.519386
164.048455	87.272142	50.524391
160.821378	91.966560	50.529396
157.837758	85.824854	50.534401
153.472617	89.969900	50.539405
150.623125	87.217739	50.544410
146.113157	88.275481	50.549415
142.821493	89.183488	50.554420
139.949749	93.733659	50.559425
136.356924	80.840984	50.564429
133.258435	77.529887	50.569434
129.352914	88.117156	50.574439
125.388926	88.462943	50.579444
122.301855	80.031065	50.584449
118.368690	81.612228	50.589453
115.178232	79.331118	50.594458
111.501772	86.304274	50.599463
108.153451	92.817896	50.604468
104.587312	83.040543	50.609473
101.208760	88.527510	50.614477
97.373951	82.658392	50.619482
94.181527	87.790332	50.624487
90.705889	83.348758	50.629492
87.300544	91.472192	50.634497
83.609829	95.011730	50.639501
80.225892	84.573086	50.644506
76.301642	95.973240	50.649511
72.912982	86.237698	50.654516
69.673426	83.578317	50.659521
66.009067	85.443257	50.664525
62.687760	84.511455	50.669530
58.829804	91.114431	50.674535
55.528791	80.485638	50.679540
51.690220	86.747054	50.684545
48.298107	86.500236	50.689549
45.578426	82.655254	50.694554
42.215579	83.444736	50.699559
38.491808	92.902570	50.704564
34.839619	85.970314	50.709569
30.830603	87.917743	50.714573
27.509113	78.285598	50.719578
24.167761	88.566212	50.724583
20.416982	79.466406	50.729588
16.748342	88.985211	50.734593
13.115146	89.886666	50.739597
9.867236	94.169945	50.744602
6.624354	91.719918	50.749607
2.871170	88.331113	50.754612