Thu Aug 25 12:43:26 2022

Number of Points = 9925

Depth (nm)	Load (N)	Time (s)
2.100720	105.963910	0.000000
2.035575	111.602430	0.005005
2.002220	105.710324	0.010010
2.195812	94.249217	0.015014
1.764081	82.924061	0.020019
1.796702	75.743464	0.025024
1.501465	83.604193	0.030029
1.092123	71.414990	0.035034
1.268020	63.212197	0.040038
0.770697	67.621272	0.045043
0.839285	47.197839	0.050048
0.482537	40.138375	0.055053
0.068029	39.785656	0.060058
0.048742	34.033740	0.065062
-0.615084	29.806508	0.070067
-1.124979	19.316219	0.075072
-1.390921	11.005509	0.080077
-1.710217	19.439456	0.085082
-1.425533	17.923652	0.090086
-1.382502	11.342564	0.095091
-2.209671	13.373540	0.100096
-2.241260	8.664437	0.105101
-2.451846	13.879623	0.110106
-2.831821	9.804075	0.115110
-3.425710	6.663716	0.120115
-3.798513	3.241944	0.125120
-4.266995	4.400468	0.130125
-4.210068	6.868723	0.135130
-4.022212	4.510713	0.140134
-4.436142	9.447710	0.145139
-4.837757	9.247996	0.150144
-5.383023	12.544599	0.155149
-5.786870	9.959759	0.160154
-5.070994	5.820076	0.165158
-5.535116	10.473872	0.170163
-5.883274	10.246799	0.175168
-6.347953	14.948141	0.180173
-6.779256	19.514539	0.185178
-6.970397	8.980641	0.190182
-7.151602	20.129604	0.195187
-7.577789	13.824516	0.200192
-7.732592	15.221795	0.205197
-7.874864	16.620274	0.210202
-7.998845	8.850471	0.215206
-8.342951	14.665546	0.220211
-8.700285	7.527095	0.225216
-9.223954	9.845875	0.230221
-9.643908	15.286856	0.235226
-9.569611	5.287174	0.240230
-9.691218	12.905531	0.245235
-9.740604	5.453073	0.250240
-9.884698	5.570514	0.255245
-10.035854	9.960138	0.260250
-10.259141	1.826247	0.265254
-11.091321	21.666817	0.270259
-11.073461	11.448184	0.275264
-11.125155	9.254257	0.280269
-11.977528	14.228316	0.285274
-12.343188	13.260502	0.290278
-12.492814	17.377804	0.295283
-12.710002	13.972777	0.300288
-12.884743	10.276361	0.305293
-12.855593	1.036730	0.310298
-12.863403	4.676228	0.315302
-13.248225	13.762682	0.320307
-13.276186	15.079975	0.325312
-13.906426	21.310045	0.330317
-14.180303	20.979585	0.335322
-14.056017	12.307174	0.340326
-14.423133	11.902738	0.345331
-14.893713	14.096142	0.350336
-15.321817	4.377661	0.355341
-15.656378	9.976104	0.360346
-15.478618	8.084747	0.365350
-15.872146	9.962357	0.370355
-15.800507	13.197101	0.375360
-16.319018	8.880668	0.380365
-17.132515	15.395715	0.385370
-16.742264	6.814512	0.390374
-17.019048	8.879474	0.395379
-17.217283	9.986164	0.400384
-18.048818	7.392408	0.405389
-18.414165	7.535025	0.410394
-18.758688	13.793092	0.415398
-18.733582	20.350750	0.420403
-18.724054	15.657349	0.425408
-18.846594	15.088041	0.430413
-18.910274	13.525580	0.435418
-18.878421	21.796940	0.440422
-19.440325	16.898845	0.445427
-19.612216	18.653142	0.450432
-20.012218	19.573148	0.455437
-20.205452	19.037062	0.460442
-20.863819	16.027029	0.465446
-21.709791	16.425289	0.470451
-21.838882	13.541134	0.475456
-21.203207	17.190539	0.480461
-21.561393	14.158782	0.485466
-21.637521	12.436921	0.490470
-21.696139	18.314833	0.495475
-22.064864	5.521363	0.500480
-22.778814	12.387808	0.505485
-23.387099	17.390062	0.510490
-23.260859	8.866045	0.515494
-23.042391	6.072966	0.520499
-23.279447	10.944285	0.525504
-24.236152	10.303199	0.530509
-24.778107	14.156106	0.535514
-24.587021	12.794173	0.540518
-24.713404	16.063108	0.545523
-24.594630	11.975853	0.550528
-24.657813	12.422302	0.555533
-25.598059	19.355845	0.560538
-25.731222	6.845006	0.565542
-25.931146	11.131539	0.570547
-26.121157	3.732755	0.575552
-26.010169	3.864012	0.580557
-27.236946	12.468620	0.585562
-27.303913	13.203565	0.590566
-27.458619	14.439476	0.595571
-27.242597	15.671083	0.600576
-27.688555	14.731670	0.605581
-27.704675	21.498268	0.610586
-27.652744	12.954255	0.615590
-28.269055	17.976749	0.620595
-28.434559	15.110955	0.625600
-28.655490	10.874447	0.630605
-28.972893	20.323664	0.635610
-29.490826	6.999916	0.640614
-30.023631	13.141950	0.645619
-30.085094	12.721260	0.650624
-30.232210	8.634538	0.655629
-30.837693	19.859470	0.660634
-30.320111	15.700234	0.665638
-30.715009	20.377988	0.670643
-31.127901	16.927695	0.675648
-31.369175	18.904836	0.680653
-31.862572	20.984758	0.685658
-31.578904	10.487195	0.690662
-32.288027	18.264049	0.695667
-32.770721	11.363540	0.700672
-32.936495	11.186985	0.705677
-33.299096	18.957000	0.710682
-33.017727	10.699741	0.715686
-33.409328	10.080843	0.720691
-33.309003	7.328422	0.725696
-33.827508	10.592358	0.730701
-34.537782	15.974425	0.735706
-34.819121	12.639563	0.740710
-35.081425	18.992316	0.745715
-35.086582	19.252503	0.750720
-34.944737	4.775009	0.755725
-35.270216	15.835842	0.760730
-35.687251	5.058933	0.765734
-36.499476	9.621741	0.770739
-36.548248	8.879522	0.775744
-36.287255	7.955890	0.780749
-36.628309	13.549023	0.785754
-36.368463	1.852970	0.790758
-36.956074	14.207723	0.795763
-37.521179	11.964529	0.800768
-37.612074	9.162975	0.805773
-38.183996	9.420219	0.810778
-38.022681	18.104725	0.815782
-38.614120	16.495245	0.820787
-38.775805	15.217061	0.825792
-39.030417	8.552899	0.830797
-39.153912	7.347825	0.835802
-39.448330	4.271278	0.840806
-39.529410	12.895686	0.845811
-40.038520	15.604494	0.850816
-40.331026	18.557773	0.855821
-40.954055	17.823277	0.860826
-40.646001	14.636508	0.865830
-41.023084	16.065452	0.870835
-41.378659	8.958365	0.875840
-40.980844	12.774751	0.880845
-41.849838	12.708384	0.885850
-41.953538	8.538929	0.890854
-42.343827	17.967928	0.895859
-42.643803	7.599784	0.900864
-42.533271	13.334130	0.905869
-42.663357	10.326746	0.910874
-43.122805	12.667103	0.915878
-43.969568	10.774927	0.920883
-44.201938	12.320401	0.925888
-43.984186	11.125132	0.930893
-44.258250	20.251182	0.935898
-44.086572	18.262700	0.940902
-44.622348	14.581727	0.945907
-45.103949	13.695356	0.950912
-45.215980	11.843079	0.955917
-45.572751	20.206967	0.960922
-45.174165	8.973226	0.965926
-45.730121	21.674202	0.970931
-46.437200	18.826828	0.975936
-46.559844	12.290685	0.980941
-47.210189	14.404689	0.985946
-47.360861	13.172236	0.990950
-47.323233	14.808282	0.995955
-47.117823	19.018650	1.000960
-47.423530	12.631414	1.005965
-48.168816	13.187906	1.010970
-48.344683	11.595568	1.015974
-48.326861	12.582983	1.020979
-48.719370	21.550422	1.025984
-48.348497	6.198645	1.030989
-49.345268	10.347444	1.035994
-49.734562	7.108593	1.040998
-49.872484	15.713434	1.046003
-50.179946	15.201575	1.051008
-50.050872	10.827968	1.056013
-50.151154	17.389451	1.061018
-50.566693	10.753670	1.066022
-50.968670	10.398990	1.071027
-51.249816	10.794171	1.076032
-51.271917	13.252662	1.081037
-51.712792	26.027357	1.086042
-52.201447	2.239635	1.091046
-52.524462	20.206568	1.096051
-52.628537	15.084880	1.101056
-52.737405	12.482296	1.106061
-52.905635	13.612759	1.111066
-52.670889	9.675012	1.116070
-53.332696	18.267029	1.121075
-53.713647	20.626725	1.126080
-54.146467	4.670053	1.131085
-54.411816	12.453299	1.136090
-54.162021	9.250350	1.141094
-55.313540	10.528558	1.146099
-55.504934	13.235039	1.151104
-55.586685	13.576830	1.156109
-55.681866	13.797339	1.161114
-55.551646	6.481257	1.166118
-55.833512	7.901609	1.171123
-56.194514	13.203638	1.176128
-55.961007	9.164844	1.181133
-57.104040	12.979058	1.186138
-57.304198	8.805736	1.191142
-57.279794	17.185825	1.196147
-57.332613	10.202143	1.201152
-57.373598	2.675607	1.206157
-58.116817	14.592834	1.211162
-58.482402	8.512376	1.216166
-58.478110	16.642516	1.221171
-58.740104	13.874100	1.226176
-59.131420	2.083927	1.231181
-59.248761	16.649227	1.236186
-59.238313	8.614755	1.241190
-59.823929	8.551443	1.246195
-60.158271	16.222115	1.251200
-60.048777	11.165040	1.256205
-60.319582	14.459768	1.261210
-60.574853	15.167271	1.266214
-61.162893	13.323142	1.271219
-61.728932	11.377489	1.276224
-61.620375	4.979129	1.281229
-62.168248	18.096450	1.286234
-61.492320	10.134874	1.291238
-61.537103	13.419496	1.296243
-62.635520	10.722030	1.301248
-62.573415	7.722497	1.306253
-62.998870	10.693444	1.311258
-62.977651	6.596166	1.316262
-63.771603	10.817590	1.321267
-64.063210	10.331722	1.326272
-63.998046	9.565324	1.331277
-64.448581	11.524634	1.336282
-64.766249	13.700407	1.341286
-64.765346	25.611774	1.346291
-64.940327	18.849712	1.351296
-65.485361	11.531868	1.356301
-65.958991	8.084769	1.361306
-65.988005	1.461193	1.366310
-66.340346	6.821975	1.371315
-66.473554	12.660950	1.376320
-66.574663	5.476030	1.381325
-66.993274	22.613219	1.386330
-66.504876	11.105977	1.391334
-66.599629	14.335154	1.396339
-67.552079	3.689603	1.401344
-67.758289	8.217565	1.406349
-68.010786	15.173057	1.411354
-68.212736	2.400921	1.416358
-68.676762	6.526355	1.421363
-69.093287	16.930737	1.426368
-69.421032	9.297272	1.431373
-69.647448	9.702860	1.436378
-69.147209	3.619614	1.441382
-69.286963	-0.999769	1.446387
-70.044149	2.972284	1.451392
-70.364760	7.195468	1.456397
-70.691885	8.819065	1.461402
-71.000398	8.120710	1.466406
-71.102652	-1.477975	1.471411
-71.403804	11.366564	1.476416
-71.121067	8.183763	1.481421
-72.066705	15.222555	1.486426
-72.195307	-2.275070	1.491430
-72.570974	9.720602	1.496435
-72.397066	20.136872	1.501440
-72.813839	12.852714	1.506445
-72.980027	21.923895	1.511450
-72.718102	12.612987	1.516454
-73.403494	19.051017	1.521459
-73.878898	20.476386	1.526464
-73.588757	16.181944	1.531469
-74.471872	23.027444	1.536474
-74.770639	24.260620	1.541478
-75.103993	26.154114	1.546483
-75.248036	20.485030	1.551488
-75.154809	14.971758	1.556493
-75.203946	23.543707	1.561498
-75.286877	21.981099	1.566502
-76.288028	23.821045	1.571507
-76.676890	25.824477	1.576512
-76.373103	19.493597	1.581517
-76.630524	24.330145	1.586522
-76.939701	24.122277	1.591526
-77.660473	19.774266	1.596531
-78.205177	9.298940	1.601536
-77.881294	11.377350	1.606541
-78.444804	19.460419	1.611546
-78.321529	13.584934	1.616550
-78.428133	12.478455	1.621555
-78.486238	12.867161	1.626560
-78.543870	11.667587	1.631565
-79.294232	18.122124	1.636570
-79.516032	14.243259	1.641574
-79.739870	15.512150	1.646579
-79.987599	24.096234	1.651584
-79.994940	17.807780	1.656589
-81.015939	14.860903	1.661594
-81.114255	5.745653	1.666598
-81.349142	5.564110	1.671603
-81.418892	22.393533	1.676608
-81.257996	12.570108	1.681613
-81.475038	13.524722	1.686618
-82.126377	13.797577	1.691622
-82.307181	16.144894	1.696627
-82.942189	21.015296	1.701632
-82.802268	7.107584	1.706637
-82.694879	13.943408	1.711642
-82.913397	9.931152	1.716646
-83.605784	16.300675	1.721651
-84.427943	13.303659	1.726656
-84.293430	7.426416	1.731661
-84.187130	17.508427	1.736666
-84.258086	18.123775	1.741670
-84.634552	16.347735	1.746675
-85.257335	17.979696	1.751680
-85.441611	1.800588	1.756685
-85.645543	17.866420	1.761690
-85.722199	13.183364	1.766694
-85.439656	12.487308	1.771699
-86.356832	8.989489	1.776704
-86.802695	7.920351	1.781709
-86.909491	15.985638	1.786714
-87.168128	12.362483	1.791718
-86.978231	5.119310	1.796723
-87.928842	2.132933	1.801728
-88.083749	0.442401	1.806733
-88.692651	10.304282	1.811738
-88.440995	9.926277	1.816742
-88.592859	6.219954	1.821747
-88.574125	15.224189	1.826752
-88.684510	6.705617	1.831757
-89.140575	5.283737	1.836762
-89.682957	9.285408	1.841766
-89.924228	12.259132	1.846771
-90.421306	16.756744	1.851776
-90.065615	3.669440	1.856781
-90.005915	2.571704	1.861786
-90.839185	2.154894	1.866790
-91.334896	10.882233	1.871795
-91.421192	8.570344	1.876800
-91.407844	2.440005	1.881805
-91.992964	5.543538	1.886810
-91.955149	4.110709	1.891814
-92.529304	-0.690541	1.896819
-92.883552	8.688511	1.901824
-93.057651	5.998074	1.906829
-92.968669	3.497369	1.911834
-92.920133	5.992246	1.916838
-93.259462	2.448176	1.921843
-94.539811	4.088261	1.926848
-94.290262	-4.401284	1.931853
-94.774577	10.240493	1.936858
-95.147431	1.924402	1.941862
-94.824676	5.986663	1.946867
-95.181881	16.685468	1.951872
-94.807819	2.699943	1.956877
-95.164547	9.447138	1.961882
-95.912426	7.533146	1.966886
-96.018570	5.847627	1.971891
-96.165168	3.823599	1.976896
-96.437222	-2.379076	1.981901
-97.413726	11.191382	1.986906
-97.946905	7.646050	1.991910
-97.157293	3.605540	1.996915
-97.670856	5.348333	2.006912
-97.100027	3.389782	2.016909
-96.435573	6.361507	2.026906
-96.542542	5.855482	2.036902
-96.258944	-0.423300	2.046899
-95.296419	2.568242	2.056896
-95.138451	16.142794	2.066893
-93.979523	9.628645	2.076890
-93.698586	7.607812	2.086886
-93.705021	12.575847	2.096883
-93.480289	11.707400	2.106880
-92.517021	9.060128	2.116877
-91.435344	11.842933	2.126874
-90.652326	11.929215	2.136870
-90.833275	12.961666	2.146867
-91.118115	14.156116	2.156864
-90.025551	16.189613	2.166861
-89.613055	10.989859	2.176858
-88.422551	10.419909	2.186854
-88.303758	18.108478	2.196851
-88.099608	18.649764	2.206848
-87.432454	15.428000	2.216845
-86.973786	18.438310	2.226842
-86.378718	20.907727	2.236838
-85.407396	13.694378	2.246835
-85.605236	15.375709	2.256832
-84.967431	18.133034	2.266829
-84.151544	13.310396	2.276826
-84.051250	11.051773	2.286822
-83.506906	17.016896	2.296819
-82.718551	12.388640	2.306816
-82.516226	12.733808	2.316813
-81.417578	10.524656	2.326810
-81.069628	11.182793	2.336806
-81.128013	9.858196	2.346803
-80.636844	7.493976	2.356800
-79.964212	15.878209	2.366797
-79.311054	5.974562	2.376794
-78.467735	10.438812	2.386790
-78.358423	10.088965	2.396787
-78.157455	8.869447	2.406784
-77.295962	13.226312	2.416781
-76.765664	16.877967	2.426778
-76.275217	13.408294	2.436774
-75.742947	2.833009	2.446771
-75.244465	4.737850	2.456768
-75.100040	14.776083	2.466765
-74.037048	6.138698	2.476762
-73.923374	13.793222	2.486758
-73.373439	7.133748	2.496755
-72.581818	11.922880	2.506752
-72.432813	10.017754	2.516749
-72.301698	11.090005	2.526746
-71.359049	10.124905	2.536742
-70.759805	8.842981	2.546739
-69.848775	11.744396	2.556736
-69.657288	21.572519	2.566733
-69.588132	12.783581	2.576730
-69.248285	16.613966	2.586726
-68.324401	13.329802	2.596723
-67.495704	6.613976	2.606720
-66.917813	7.327950	2.616717
-66.612324	13.846853	2.626714
-66.644253	14.700731	2.636710
-66.011866	17.056595	2.646707
-65.538362	11.939148	2.656704
-64.609369	13.481927	2.666701
-64.120988	12.489805	2.676698
-63.821554	12.262223	2.686694
-63.665082	12.804644	2.696691
-62.665156	8.859165	2.706688
-62.209942	7.748696	2.716685
-61.744590	2.014807	2.726682
-60.868213	4.623877	2.736678
-60.745163	4.477785	2.746675
-60.520329	2.947251	2.756672
-60.231293	11.090650	2.766669
-59.432006	12.235602	2.776666
-58.551624	3.211849	2.786662
-57.980352	8.855972	2.796659
-57.982436	8.764334	2.806656
-57.585276	9.931114	2.816653
-56.391212	0.069427	2.826650
-56.361853	6.131082	2.836646
-55.835574	1.857509	2.846643
-55.261903	2.505621	2.856640
-55.056947	6.008682	2.866637
-53.932862	3.843065	2.876634
-53.485507	-1.020024	2.886630
-53.360826	4.370958	2.896627
-53.391868	7.733602	2.906624
-52.528327	2.216086	2.916621
-51.589291	8.027499	2.926618
-51.178786	0.328658	2.936614
-51.175890	3.571942	2.946611
-50.067989	-1.559375	2.956608
-49.881580	6.457553	2.966605
-49.101808	0.189722	2.976602
-48.249006	1.608224	2.986598
-47.874475	4.546187	2.996595
-48.270694	7.947043	3.006592
-47.797719	6.333279	3.016589
-47.016165	2.307977	3.026586
-45.924323	5.969847	3.036582
-45.553364	11.559828	3.046579
-45.356656	4.347483	3.056576
-44.872089	10.870005	3.066573
-44.101706	11.842090	3.076570
-43.804695	14.164975	3.086566
-42.900200	1.659190	3.096563
-42.661250	8.606670	3.106560
-42.384044	7.014077	3.116557
-41.876792	8.277649	3.126554
-41.253027	7.029898	3.136550
-40.990258	3.652923	3.146547
-40.127654	2.478622	3.156544
-39.771839	7.500770	3.166541
-39.505012	15.096454	3.176538
-38.480603	8.970854	3.186534
-38.154606	16.595281	3.196531
-37.980676	10.995749	3.206528
-36.946236	6.268751	3.216525
-36.138838	10.257128	3.226522
-36.531269	8.177079	3.236518
-35.950515	4.639406	3.246515
-35.106699	4.418392	3.256512
-34.761541	9.758991	3.266509
-34.324174	-0.772913	3.276506
-33.791146	4.522409	3.286502
-33.245354	8.307855	3.296499
-32.363998	4.010324	3.306496
-32.111462	6.327506	3.316493
-31.924667	0.957212	3.326490
-31.306594	-0.422694	3.336486
-30.881761	1.693262	3.346483
-30.315364	3.958098	3.356480
-29.778770	5.359624	3.366477
-29.301270	6.795752	3.376474
-28.439559	2.580495	3.386470
-27.959781	1.611899	3.396467
-27.916195	-2.541691	3.406464
-27.482849	0.361715	3.416461
-26.661355	0.470484	3.426458
-26.223412	7.909474	3.436454
-25.300167	5.034062	3.446451
-25.097921	2.870338	3.456448
-24.907588	6.736823	3.466445
-24.216873	4.654953	3.476442
-23.425260	5.794774	3.486438
-23.399678	1.624998	3.496435
-22.663086	8.804951	3.506432
-21.868113	4.739534	3.516429
-22.065927	-1.052003	3.526426
-20.943407	8.234262	3.536422
-20.507203	6.524890	3.546419
-20.298436	0.767848	3.556416
-20.074298	1.366192	3.566413
-18.791842	2.834585	3.576410
-18.524837	8.203270	3.586406
-18.615907	6.586018	3.596403
-17.661630	8.843933	3.606400
-17.496149	4.953177	3.616397
-16.351939	14.448291	3.626394
-16.243297	2.212924	3.636390
-15.719216	11.349037	3.646387
-14.895504	7.551549	3.656384
-14.480636	9.941500	3.666381
-14.324888	8.580181	3.676378
-13.579752	0.673685	3.686374
-13.410297	8.788308	3.696371
-12.858028	7.456726	3.706368
-11.946672	5.970679	3.716365
-11.692941	3.377570	3.726362
-11.518631	4.788345	3.736358
-10.502694	5.395673	3.746355
-10.240869	9.352328	3.756352
-9.195758	6.315271	3.766349
-8.887939	11.794772	3.776346
-8.543150	17.753157	3.786342
-8.134150	13.890767	3.796339
-8.013750	10.532930	3.806336
-6.862845	12.113805	3.816333
-6.912020	15.913282	3.826330
-6.232952	13.449931	3.836326
-5.952198	7.871676	3.846323
-5.414634	7.898222	3.856320
-4.910362	14.246601	3.866317
-4.081838	20.436472	3.876314
-4.130193	34.604080	3.886310
-3.543349	38.813927	3.896307
-2.887179	43.136456	3.906304
-2.168271	62.683200	3.916301
-1.719382	63.357206	3.926298
-1.542128	70.048283	3.936294
-1.110437	87.105800	3.946291
-0.670918	91.512973	3.956288
-0.262929	116.943629	3.966285
0.000000	123.195964	3.971290
0.204648	142.099086	3.976294
0.741664	142.081334	3.981299
0.393218	144.119574	3.986304
0.752568	158.211669	3.991309
1.039381	160.371840	3.996314
1.023247	163.734261	4.001318
1.207947	163.844478	4.006323
1.085003	170.697476	4.011328
1.315308	178.131049	4.016333
1.304684	163.405226	4.021338
1.237758	175.390603	4.026342
1.654212	167.384191	4.031347
1.622469	171.764636	4.036352
1.035844	150.640143	4.041357
0.837178	142.932604	4.046362
0.841747	164.008981	4.051366
1.341456	159.140661	4.056371
1.404035	170.656486	4.061376
1.486390	173.250496	4.066381
1.497437	165.949855	4.071386
1.707395	172.092624	4.076390
1.729472	157.083269	4.081395
1.462825	156.172699	4.086400
1.193356	146.552670	4.091405
1.183956	149.515397	4.096410
0.967283	148.261636	4.101414
1.328166	159.933197	4.106419
1.501621	180.391503	4.111424
1.531381	166.722384	4.116429
1.449571	164.991906	4.121434
1.255728	172.270469	4.126438
1.394829	174.257631	4.131443
1.488316	170.867170	4.136448
1.601612	169.413009	4.141453
1.711751	168.705997	4.146458
1.410711	168.250073	4.151462
1.424022	158.133309	4.156467
1.212651	174.121362	4.161472
1.637538	169.812098	4.166477
1.987724	166.466840	4.171482
1.726510	172.895409	4.176486
1.591866	152.168337	4.181491
1.620947	152.923040	4.186496
1.377231	159.272931	4.191501
1.529424	161.422557	4.196506
1.365901	170.392158	4.201510
1.596411	171.630999	4.206515
1.522210	170.747223	4.211520
1.151493	174.699884	4.216525
1.698733	175.231030	4.221530
1.476953	172.835940	4.226534
1.846229	169.437069	4.231539
1.441598	172.028287	4.236544
1.524329	168.516124	4.241549
1.728816	175.963233	4.246554
1.638654	174.658010	4.251558
1.797951	178.021421	4.256563
1.547828	180.262560	4.261568
1.474619	178.252319	4.266573
1.557503	180.001514	4.271578
1.675130	190.663995	4.276582
1.789838	195.385335	4.281587
1.723558	199.008723	4.286592
1.930633	206.205499	4.291597
2.151087	205.281882	4.296602
2.230638	198.062244	4.301606
2.310287	194.718240	4.306611
1.769666	190.610872	4.311616
1.832243	181.995504	4.316621
1.900943	171.629606	4.321626
1.855194	177.030986	4.326630
2.111805	171.909683	4.331635
1.911085	177.945957	4.336640
1.621915	180.525412	4.341645
1.927699	182.872441	4.346650
2.018566	195.861341	4.351654
2.281407	191.988755	4.356659
2.166876	197.650858	4.361664
1.932222	188.230998	4.366669
2.359864	185.484212	4.371674
2.051088	181.005158	4.376678
1.916042	173.505939	4.381683
1.596537	178.276326	4.386688
1.979894	191.485152	4.391693
1.880536	190.791981	4.396698
2.207564	201.203357	4.401702
2.130855	193.340644	4.406707
2.037711	195.427473	4.411712
2.166278	195.350331	4.416717
2.419469	196.212292	4.421722
2.493335	195.650169	4.426726
2.593013	201.085719	4.431731
2.303084	200.681838	4.436736
2.264637	190.193510	4.441741
2.095061	189.419591	4.446746
1.874666	201.175929	4.451750
2.263965	199.289373	4.456755
1.981427	197.384696	4.461760
2.138006	196.331880	4.466765
2.133710	194.013444	4.471770
1.850819	205.023429	4.476774
2.225987	196.055352	4.481779
2.036352	198.555939	4.486784
2.008721	196.424658	4.491789
2.514651	193.472613	4.496794
2.030260	203.068316	4.501798
2.705339	202.399337	4.506803
2.683004	213.665900	4.511808
2.286583	193.837185	4.516813
2.457214	197.024814	4.521818
2.178914	204.209054	4.526822
2.739765	203.228938	4.531827
2.205488	203.138593	4.536832
2.077245	207.521511	4.541837
2.706279	215.832272	4.546842
2.335718	221.610430	4.551846
2.630098	222.348878	4.556851
2.888416	220.454368	4.561856
2.424171	219.318488	4.566861
2.635180	213.081171	4.571866
2.786221	220.963785	4.576870
2.875523	221.873573	4.581875
2.526800	204.967049	4.586880
2.375840	199.305314	4.591885
2.737643	196.075291	4.596890
2.278674	213.946666	4.601894
2.585457	205.087377	4.606899
2.580295	221.637957	4.611904
2.903986	226.731526	4.616909
2.898324	216.219063	4.621914
2.759726	214.535443	4.626918
2.951997	212.360214	4.631923
2.562733	209.273179	4.636928
2.345625	207.171585	4.641933
2.943289	209.036281	4.646938
2.561039	225.339059	4.651942
2.720090	224.912287	4.656947
2.709093	223.572510	4.661952
2.881384	222.583671	4.666957
2.790530	225.660414	4.671962
2.677662	224.782694	4.676966
3.154332	226.587254	4.681971
2.855044	219.838260	4.686976
2.670579	214.140640	4.691981
2.783198	220.469523	4.696986
2.655360	232.610018	4.701990
2.970683	229.804892	4.706995
2.775149	225.896550	4.712000
2.799861	228.322427	4.717005
2.897233	221.448005	4.722010
2.574658	223.143673	4.727014
2.915337	221.252078	4.732019
2.977072	220.533665	4.737024
2.908089	219.709182	4.742029
2.880168	212.373498	4.747034
2.723534	222.129831	4.752038
2.972163	217.765914	4.757043
2.739149	222.842305	4.762048
3.012130	226.323955	4.767053
3.048203	227.447730	4.772058
3.062735	224.958658	4.777062
2.893701	228.882894	4.782067
3.325634	236.623426	4.787072
3.108431	235.781036	4.792077
3.121560	224.958735	4.797082
2.904922	233.269129	4.802086
3.472674	238.625022	4.807091
3.298198	237.367807	4.812096
3.033503	236.830256	4.817101
3.126698	230.813876	4.822106
2.908499	236.460596	4.827110
3.085312	239.710541	4.832115
3.096330	247.248105	4.837120
3.218117	251.091977	4.842125
3.402882	257.931596	4.847130
3.293836	253.051064	4.852134
3.744469	252.524820	4.857139
3.303152	240.656891	4.862144
3.018783	246.908777	4.867149
3.414020	252.000636	4.872154
3.169623	253.279091	4.877158
3.580136	250.310349	4.882163
3.282465	242.254442	4.887168
3.161300	244.260245	4.892173
3.382635	245.861201	4.897178
2.996193	251.695642	4.902182
3.255957	249.911636	4.907187
3.330861	253.057326	4.912192
2.857326	249.505754	4.917197
2.941112	248.382082	4.922202
2.983580	255.781842	4.927206
3.035515	256.026760	4.932211
3.209852	261.659441	4.937216
3.711213	269.136005	4.942221
4.089898	272.632740	4.947226
3.588104	261.976520	4.952230
3.450331	259.713790	4.957235
3.003099	265.459682	4.962240
3.175297	273.655385	4.967245
3.576814	264.474334	4.972250
3.697365	278.072421	4.977254
3.664110	271.980925	4.982259
3.584839	279.308020	4.987264
3.590999	287.564547	4.992269
3.912975	275.099264	4.997274
3.564269	278.504324	5.002278
3.836022	284.229318	5.007283
3.648781	280.012775	5.012288
3.834014	273.064455	5.017293
3.939602	276.104100	5.022298
3.794460	277.439772	5.027302
3.800885	267.817579	5.032307
3.697884	261.341539	5.037312
3.590486	258.305245	5.042317
4.004632	261.780603	5.047322
3.602153	257.917334	5.052326
3.641972	260.546495	5.057331
3.849386	272.640816	5.062336
3.621642	275.527041	5.067341
3.968463	276.991278	5.072346
3.695547	276.616368	5.077350
3.846800	272.723283	5.082355
3.841621	273.027771	5.087360
3.738651	281.269756	5.092365
3.876035	271.484670	5.097370
3.999075	281.178232	5.102374
4.168474	277.408855	5.107379
4.221152	276.384970	5.112384
3.869022	271.425459	5.117389
3.725684	252.446054	5.122394
3.722890	268.543882	5.127398
3.948224	266.002792	5.132403
3.922477	271.885130	5.137408
3.941857	277.478819	5.142413
3.987736	271.416054	5.147418
3.938426	280.725325	5.152422
3.959374	275.900350	5.157427
3.931494	266.982734	5.162432
3.864266	280.426744	5.167437
4.067589	270.286472	5.172442
4.090843	276.056727	5.177446
4.096064	267.769849	5.182451
4.101120	274.593339	5.187456
4.137312	281.263254	5.192461
4.181977	270.559372	5.197466
4.427131	279.148615	5.202470
3.873750	276.343551	5.207475
4.095807	283.999927	5.212480
4.047456	284.108695	5.217485
4.392942	272.392717	5.222490
4.054761	282.591988	5.227494
4.276773	278.985213	5.232499
4.216332	276.498389	5.237504
4.182720	279.474422	5.242509
4.749299	277.332287	5.247514
4.321454	284.568465	5.252518
4.314160	280.962816	5.257523
4.472673	283.541745	5.262528
4.062802	276.038086	5.267533
4.347560	271.393244	5.272538
3.906454	275.594241	5.277542
4.108051	273.189749	5.282547
4.057170	274.289186	5.287552
3.724658	282.361490	5.292557
4.151790	275.932097	5.297562
4.186855	293.637558	5.302566
4.208850	308.567256	5.307571
4.363004	309.799087	5.312576
4.073919	311.555956	5.317581
4.451658	300.882128	5.322586
4.439780	313.940997	5.327590
4.797377	312.704815	5.332595
4.523937	318.303268	5.337600
4.579130	303.250636	5.342605
4.770627	302.840925	5.347610
4.233328	301.071068	5.352614
4.421226	304.430021	5.357619
4.727704	315.467955	5.362624
4.518156	311.735799	5.367629
4.848534	301.534472	5.372634
4.790025	297.753344	5.377638
4.565644	306.979326	5.382643
4.663066	304.075451	5.387648
4.544767	294.564536	5.392653
4.759376	295.913446	5.397658
4.644329	301.104255	5.402662
4.468640	287.489381	5.407667
4.603245	296.118099	5.412672
4.325824	305.178382	5.417677
4.951893	299.084813	5.422682
4.339140	311.345633	5.427686
4.361571	305.052408	5.432691
4.516371	302.636261	5.437696
3.922245	306.563843	5.442701
4.199858	302.499090	5.447706
4.450509	318.085844	5.452710
5.158292	328.712888	5.457715
5.076996	329.592463	5.462720
4.577062	334.704379	5.467725
4.864865	313.474322	5.472730
4.881746	327.920774	5.477734
4.681126	321.969382	5.482739
4.734220	315.614400	5.487744
4.433994	329.585345	5.492749
5.104027	327.246658	5.497754
4.872331	336.321938	5.502758
5.014478	333.721105	5.507763
4.955282	327.029366	5.512768
4.659815	334.051829	5.517773
5.189451	334.468677	5.522778
5.080521	328.496589	5.527782
4.933104	323.884646	5.532787
4.988002	335.341669	5.537792
5.021656	327.809624	5.542797
5.314827	326.691106	5.547802
5.425384	330.935396	5.552806
5.101153	314.300182	5.557811
5.333361	302.086232	5.562816
4.418228	307.978218	5.567821
4.684239	303.342632	5.572826
4.963227	316.235704	5.577830
5.123959	326.590950	5.582835
5.178514	332.520838	5.587840
5.168257	338.267889	5.592845
5.473497	332.291019	5.597850
5.278492	337.171657	5.602854
4.986576	330.880218	5.607859
5.178076	336.247637	5.612864
5.007260	332.164553	5.617869
5.401245	321.345795	5.622874
5.101982	326.106722	5.627878
5.036064	327.290777	5.632883
5.144455	328.368425	5.637888
4.893673	337.487826	5.642893
5.132330	329.082085	5.647898
4.896522	332.244835	5.652902
5.025631	326.159519	5.657907
5.334487	323.874258	5.662912
5.235258	328.701922	5.667917
5.031637	315.043945	5.672922
4.879218	329.431502	5.677926
4.991079	334.279877	5.682931
5.452645	345.527652	5.687936
5.306627	351.824338	5.692941
5.533599	348.583775	5.697946
5.522733	348.481022	5.702950
5.468075	349.634840	5.707955
5.732730	337.004485	5.712960
5.437270	339.512181	5.717965
5.605101	327.314627	5.722970
5.539479	324.692565	5.727974
5.341745	331.604799	5.732979
5.589165	337.162777	5.737984
4.951416	333.007317	5.742989
5.202767	328.560688	5.747994
5.322003	348.648025	5.752998
5.542684	362.701897	5.758003
5.479182	353.913207	5.763008
5.423674	362.764739	5.768013
5.715118	350.108030	5.773018
5.412979	364.474780	5.778022
5.529673	358.157275	5.783027
5.880979	356.014060	5.788032
5.662244	354.374621	5.793037
6.160500	353.293571	5.798042
5.805996	347.935770	5.803046
5.457695	333.170964	5.808051
5.413569	343.893683	5.813056
5.540968	356.010089	5.818061
5.442556	348.065285	5.823066
5.422989	356.151865	5.828070
5.480234	354.348959	5.833075
5.605838	361.270656	5.838080
5.740700	361.461452	5.843085
5.686766	352.171380	5.848090
5.535608	357.181198	5.853094
5.384998	360.453992	5.858099
5.375299	348.375992	5.863104
5.395078	363.454782	5.868109
5.640407	367.412203	5.873114
5.980308	383.794970	5.878118
5.795198	384.735106	5.883123
5.403674	377.589206	5.888128
5.673870	390.932973	5.893133
5.922809	377.602682	5.898138
6.119796	382.067565	5.903142
6.301518	386.857551	5.908147
6.312279	374.988303	5.913152
5.893960	391.869537	5.918157
5.821312	380.807475	5.923162
5.560124	392.314060	5.928166
5.358780	382.455433	5.933171
5.375985	384.044093	5.938176
5.723708	392.278789	5.943181
6.069587	380.641775	5.948186
5.619760	380.639438	5.953190
5.804230	390.431005	5.958195
6.169265	397.245596	5.963200
5.778767	397.040969	5.968205
6.226178	400.830690	5.973210
6.168064	404.399055	5.978214
6.077188	404.944768	5.983219
6.235686	406.701121	5.988224
6.054255	397.070326	5.993229
6.057062	386.328640	5.998234
5.980926	396.167371	6.003238
6.135348	393.222912	6.008243
6.247226	381.758605	6.013248
5.967020	387.601755	6.018253
5.990752	386.205903	6.023258
6.119945	390.023334	6.028262
6.308845	395.024174	6.033267
6.072679	382.617794	6.038272
6.105488	385.988407	6.043277
5.751280	378.108980	6.048282
6.054235	380.130604	6.053286
5.994912	389.330767	6.058291
6.173576	385.028393	6.063296
5.930225	385.066473	6.068301
6.377191	393.386863	6.073306
5.927997	386.762535	6.078310
5.489788	382.806758	6.083315
6.246815	390.490093	6.088320
6.286486	410.124883	6.093325
6.064865	397.118250	6.098330
6.099398	399.181934	6.103334
5.977771	396.967278	6.108339
5.853782	390.908941	6.113344
6.084061	397.763630	6.118349
6.314963	404.229072	6.123354
6.211083	401.223841	6.128358
6.201840	396.802206	6.133363
5.840968	382.330403	6.138368
5.818411	396.612243	6.143373
6.329686	395.842370	6.148378
6.093367	396.594373	6.153382
6.143069	395.953771	6.158387
6.226709	378.631316	6.163392
6.185226	387.281341	6.168397
6.009963	379.880088	6.173402
5.941410	386.974587	6.178406
5.827827	384.524550	6.183411
6.245461	382.962574	6.188416
6.117242	384.507579	6.193421
5.961220	378.682061	6.198426
5.933104	379.876015	6.203430
5.932533	382.315365	6.208435
6.236684	386.659052	6.213440
6.160899	393.223165	6.218445
6.106883	380.671184	6.223450
5.879644	390.682287	6.228454
6.045960	391.583180	6.233459
6.085348	384.366596	6.238464
6.130411	400.071058	6.243469
5.904577	392.063939	6.248474
6.004189	395.493692	6.253478
6.136645	403.066080	6.258483
6.155701	396.668945	6.263488
6.059103	397.519282	6.268493
6.423835	398.515640	6.273498
5.991040	385.656000	6.278502
5.946222	389.620921	6.283507
6.091970	383.890491	6.288512
5.857661	388.764646	6.293517
5.929247	389.338689	6.298522
6.259462	388.679445	6.303526
6.081996	399.821732	6.308531
6.215347	398.320116	6.313536
5.823903	387.371277	6.318541
5.906762	388.104909	6.323546
6.044450	396.138393	6.328550
6.157813	400.125989	6.333555
6.222977	394.692926	6.338560
5.984771	394.935849	6.343565
6.058938	385.208063	6.348570
6.009535	387.205802	6.353574
5.964936	396.944676	6.358579
6.166493	402.550991	6.363584
5.973913	404.507888	6.368589
5.995648	407.962500	6.373594
6.191137	406.210697	6.378598
5.975287	408.440167	6.383603
6.240183	401.754568	6.388608
6.014418	407.105128	6.393613
5.983277	406.208266	6.398618
6.294529	397.420950	6.403622
6.078505	393.569566	6.408627
6.026932	385.342154	6.413632
5.826033	389.799777	6.418637
6.151137	404.501724	6.423642
6.338659	403.263710	6.428646
5.977383	388.314226	6.433651
6.197671	372.308667	6.438656
6.102113	384.146807	6.443661
6.063103	378.211204	6.448666
5.991320	389.409694	6.453670
5.898199	388.234636	6.458675
5.944835	381.086522	6.463680
5.865509	386.164188	6.468685
6.066184	392.248375	6.473690
6.196164	410.771168	6.478694
6.242072	397.583408	6.483699
6.486358	387.563204	6.488704
5.761915	388.850444	6.493709
6.375969	386.662892	6.498714
6.047019	381.389663	6.503718
5.942663	379.763939	6.508723
6.253488	375.472498	6.513728
5.983983	384.974516	6.518733
6.021554	382.889946	6.523738
6.391838	379.209298	6.528742
5.844494	388.093611	6.533747
5.908177	385.410149	6.538752
5.687474	376.994100	6.543757
5.888152	379.860673	6.548762
6.103497	387.236564	6.553766
6.074949	405.787354	6.558771
5.965985	400.954226	6.563776
6.165109	412.069153	6.568781
6.281797	404.479773	6.573786
6.070010	396.438813	6.578790
5.815729	399.272267	6.583795
6.219223	399.215324	6.588800
6.226746	394.892306	6.593805
5.857161	396.133436	6.598810
6.006033	395.720910	6.603814
5.920393	408.500334	6.608819
6.331419	413.086716	6.613824
6.123836	413.774104	6.618829
6.131693	395.931984	6.623834
5.910864	390.768364	6.628838
5.788345	400.190411	6.633843
6.662393	401.752389	6.638848
5.904283	403.753602	6.643853
5.743387	391.183559	6.648858
6.325229	400.080782	6.653862
6.151245	399.975113	6.658867
5.878332	398.515005	6.663872
5.493292	390.396788	6.668877
6.191283	406.049573	6.673882
6.206000	411.330816	6.678886
6.063613	413.150133	6.683891
6.017738	411.733547	6.688896
6.034468	418.985544	6.693901
6.200474	413.865714	6.698906
6.017881	411.486598	6.703910
6.266831	408.846873	6.708915
6.175069	402.381676	6.713920
6.051392	396.342271	6.718925
5.764567	394.216776	6.723930
6.320658	394.423832	6.728934
6.041570	401.244434	6.733939
6.018708	391.288233	6.738944
5.880212	391.537679	6.743949
6.137634	403.871032	6.748954
6.371274	407.216510	6.753958
6.077519	390.674529	6.758963
6.086473	392.916231	6.763968
5.816697	393.322292	6.768973
6.029210	386.869538	6.773978
6.292382	399.483568	6.778982
5.790252	400.198124	6.783987
6.238829	405.082348	6.788992
6.196167	395.524726	6.793997
6.035472	386.406392	6.799002
5.861808	394.444365	6.804006
5.785969	403.045996	6.809011
6.343271	408.327647	6.814016
6.202758	407.042952	6.819021
6.131318	397.205093	6.824026
5.995670	384.048954	6.829030
5.880111	402.471001	6.834035
6.201513	404.872561	6.839040
5.830189	405.307189	6.844045
5.762856	402.036797	6.849050
5.980567	414.961688	6.854054
5.945036	411.708459	6.859059
6.141300	414.831999	6.864064
5.890560	417.652246	6.869069
5.839315	411.981147	6.874074
5.961703	416.125524	6.879078
6.027437	414.909755	6.884083
6.294869	405.078909	6.889088
6.450313	411.660584	6.894093
6.508623	415.438505	6.899098
6.624998	399.692818	6.904102
6.013350	407.590609	6.909107
6.333112	393.135541	6.914112
5.992024	392.217640	6.919117
6.024120	390.801494	6.924122
6.106825	393.129719	6.929126
5.853683	396.254066	6.934131
5.652610	384.993820	6.939136
5.730342	400.908303	6.944141
6.318900	415.439264	6.949146
5.896602	411.360762	6.954150
5.741640	413.909730	6.959155
6.233433	413.332740	6.964160
6.081907	419.506923	6.969165
6.235872	413.193050	6.974170
6.469940	409.043345	6.979174
6.038029	401.698114	6.984179
5.776151	402.802144	6.989184
5.936793	413.980050	6.994189
6.232864	410.064245	6.999194
6.424177	415.165956	7.004198
5.801088	409.318695	7.009203
5.873671	397.186639	7.014208
5.854863	402.685109	7.019213
6.400355	416.166098	7.024218
6.149317	406.941683	7.029222
6.260931	394.936395	7.034227
5.898506	392.351334	7.039232
5.919703	395.597216	7.044237
5.707417	393.055072	7.049242
5.768386	398.797311	7.054246
5.875981	411.748945	7.059251
6.143657	410.213626	7.064256
6.169859	419.729443	7.069261
6.321906	411.254974	7.074266
6.291036	404.675829	7.079270
6.356394	418.991369	7.084275
6.597748	410.123248	7.089280
6.217065	403.997556	7.094285
5.802238	395.257566	7.099290
6.276423	388.554999	7.104294
6.393862	397.458545	7.109299
6.286563	387.151736	7.114304
5.964363	383.158799	7.119309
6.086690	389.783621	7.124314
6.056738	385.438001	7.129318
5.800071	392.400623	7.134323
5.950178	376.238373	7.139328
6.035532	385.691118	7.144333
5.752007	385.748148	7.149338
6.197428	373.810797	7.154342
5.973912	388.586036	7.159347
5.801463	384.553816	7.164352
6.117800	389.800449	7.169357
6.071389	385.172664	7.174362
5.928070	383.929540	7.179366
5.762306	382.379878	7.184371
6.117608	393.451340	7.189376
6.091430	408.119743	7.194381
6.230568	401.684809	7.199386
5.984823	393.228382	7.204390
5.648830	398.188076	7.209395
6.086627	399.356488	7.214400
6.107100	407.262807	7.219405
6.035215	410.311299	7.224410
6.228233	417.143358	7.229414
6.303841	423.383197	7.234419
6.475744	397.903188	7.239424
5.903105	401.469911	7.244429
6.053030	394.454308	7.249434
6.136652	387.021980	7.254438
5.858686	394.168277	7.259443
5.973817	384.766276	7.264448
6.006876	386.137311	7.269453
6.146075	388.149793	7.274458
6.260006	380.934186	7.279462
5.898626	398.537348	7.284467
6.323828	390.194101	7.289472
6.102180	385.596937	7.294477
6.286838	389.870760	7.299482
6.128042	385.523182	7.304486
6.002580	388.836335	7.309491
6.038431	381.408330	7.314496
5.610292	392.441189	7.319501
5.819759	384.796150	7.324506
6.088777	392.144651	7.329510
5.955967	394.089019	7.334515
6.072273	402.685853	7.339520
6.070386	422.539145	7.344525
6.154421	405.713325	7.349530
6.168972	392.261556	7.354534
6.271607	396.927892	7.359539
6.292048	382.405834	7.364544
6.126248	395.064927	7.369549
6.048083	393.536340	7.374554
6.088284	387.477589	7.379558
5.887513	385.038048	7.384563
5.933833	393.946408	7.389568
6.060205	387.766585	7.394573
6.012784	390.513841	7.399578
6.340279	386.725998	7.404582
6.220000	383.742322	7.409587
6.215180	383.328567	7.414592
6.590411	381.105667	7.419597
6.113168	388.808381	7.424602
6.518580	387.700747	7.429606
5.944999	388.654294	7.434611
6.294721	387.109286	7.439616
6.295189	397.325165	7.444621
6.205278	390.157312	7.449626
6.002728	388.705164	7.454630
6.028658	390.839800	7.459635
5.835049	389.927265	7.464640
6.085638	387.651126	7.469645
5.737799	389.097662	7.474650
6.216788	387.352062	7.479654
6.148311	390.868263	7.484659
6.283798	385.310287	7.489664
6.282675	388.638760	7.494669
6.070295	390.567120	7.499674
6.010196	379.898571	7.504678
6.012100	391.955569	7.509683
6.060352	378.147345	7.514688
6.212005	383.742490	7.519693
6.314728	380.091109	7.524698
6.280231	368.985111	7.529702
6.163033	367.981509	7.534707
6.378679	366.615702	7.539712
5.989972	367.113164	7.544717
5.898524	366.447221	7.549722
5.751501	353.334017	7.554726
5.933821	368.494914	7.559731
6.008558	358.270333	7.564736
5.845595	369.109765	7.569741
5.837147	377.450882	7.574746
6.091384	389.512636	7.579750
5.849444	389.512528	7.584755
6.078028	381.978393	7.589760
6.373107	385.614804	7.594765
6.473984	392.084796	7.599770
6.165133	366.534622	7.604774
6.136514	374.518222	7.609779
6.162036	358.188844	7.614784
6.102620	356.862971	7.619789
5.851312	363.176158	7.624794
6.086339	350.253036	7.629798
5.973098	359.755868	7.634803
6.121064	359.014447	7.639808
6.123605	358.014231	7.644813
5.794112	360.255173	7.649818
6.237169	353.475238	7.654822
6.093812	367.516548	7.659827
6.006265	356.906099	7.664832
5.885723	359.804015	7.669837
6.094664	368.636261	7.674842
6.251500	362.578226	7.679846
6.196359	362.343202	7.684851
6.006442	353.618614	7.689856
5.851562	359.859742	7.694861
5.722016	367.700961	7.699866
6.227634	373.746854	7.704870
6.419760	392.003620	7.709875
6.346559	377.119743	7.714880
6.021896	363.702162	7.719885
6.317674	364.013281	7.724890
5.990628	356.433334	7.729894
5.830943	362.216462	7.734899
5.903145	362.844192	7.739904
5.888563	361.175929	7.744909
5.703098	360.898048	7.749914
5.869856	368.199286	7.754918
5.893497	387.333514	7.759923
6.224834	389.357021	7.764928
6.426084	389.151428	7.769933
6.342308	386.636607	7.774938
6.478128	367.559555	7.779942
6.124590	364.552318	7.784947
5.905754	358.186143	7.789952
5.879241	364.527385	7.794957
5.752284	368.261557	7.799962
6.068148	361.387650	7.804966
6.058942	377.242966	7.809971
6.035996	370.665756	7.814976
6.244385	368.820184	7.819981
5.998096	374.518807	7.824986
6.136625	360.949558	7.829990
5.925052	360.191703	7.834995
5.889961	358.843036	7.840000
5.897294	365.824395	7.845005
6.000870	376.106366	7.850010
6.509896	370.410771	7.855014
6.067220	376.453383	7.860019
5.886748	365.120317	7.865024
5.939621	371.844601	7.870029
5.869865	384.346266	7.875034
6.174248	381.156845	7.880038
6.035050	384.095654	7.885043
6.160759	378.172208	7.890048
5.972031	387.417956	7.895053
6.006554	385.647082	7.900058
5.953967	389.300002	7.905062
6.002607	383.499363	7.910067
6.099219	387.786981	7.915072
6.150773	375.515863	7.920077
6.003953	381.274834	7.925082
6.038808	382.481069	7.930086
6.219644	391.399990	7.935091
6.415341	381.950564	7.940096
6.510735	381.391390	7.945101
6.191439	361.737069	7.950106
5.935650	362.017548	7.955110
5.748198	367.855650	7.960115
5.399223	367.505310	7.965120
6.049980	376.948556	7.970125
5.956088	387.912133	7.975142
6.416099	393.050162	7.980160
6.163753	386.462561	7.985178
6.105731	381.583337	7.990195
6.492474	384.337625	7.995213
6.037093	371.239962	8.000230
6.241069	357.287929	8.005248
5.920647	356.946771	8.010266
5.716013	365.824357	8.015283
6.022814	377.831216	8.020301
6.231960	379.177462	8.025318
6.648122	379.285773	8.030336
5.799124	382.962661	8.035354
5.940033	375.707543	8.040371
6.274867	379.722798	8.045389
6.232164	380.527846	8.050406
6.144582	378.790075	8.055424
6.378680	381.300041	8.060442
6.098099	371.996609	8.065459
5.933162	368.784599	8.070477
6.537393	363.883665	8.075494
6.183876	358.795130	8.080512
5.852422	365.347864	8.085530
6.211868	366.929330	8.090547
5.877973	361.484276	8.095565
5.960883	385.619066	8.100582
6.499526	373.227175	8.105600
5.988823	371.208568	8.110618
5.940984	374.381236	8.115635
5.809670	378.917646	8.120653
6.260911	380.229115	8.125670
6.429224	377.138455	8.130688
6.263001	381.623532	8.135706
6.163217	379.079800	8.140723
6.471873	374.341938	8.145741
5.980421	389.159425	8.150758
6.388785	377.728359	8.155776
6.384764	386.634482	8.160794
6.334883	381.498366	8.165811
6.494208	378.863543	8.170829
6.118572	382.119130	8.175846
6.013222	373.185866	8.180864
6.078170	378.761326	8.185882
5.871150	377.026491	8.190899
6.251478	381.498514	8.195917
5.981106	384.469369	8.200934
6.480700	382.873123	8.205952
6.435841	385.426797	8.210970
6.322560	383.169197	8.215987
6.163021	385.396862	8.221005
5.966309	383.559427	8.226022
6.335891	383.671881	8.231040
6.270180	382.845852	8.236058
5.964296	383.982465	8.241075
6.260473	381.768005	8.246093
6.334103	403.524834	8.251110
6.791502	403.847587	8.256128
6.312979	397.932884	8.261146
6.302006	389.120523	8.266163
6.270006	383.050657	8.271181
5.945914	387.910760	8.276198
6.523890	395.778971	8.281216
6.262261	403.056069	8.286234
6.433365	403.783437	8.291251
6.647054	397.327936	8.296269
6.577833	399.251122	8.301286
6.403158	398.205484	8.306304
6.230693	392.100819	8.311322
6.320113	399.796276	8.316339
6.640825	403.640183	8.321357
6.125293	407.858110	8.326374
6.565942	408.776771	8.331392
6.378277	414.268747	8.336410
6.507822	407.308883	8.341427
6.792987	403.404658	8.346445
6.325435	399.905548	8.351462
6.134386	399.559897	8.356480
6.515232	407.058219	8.361498
6.396934	405.643990	8.366515
6.538771	407.859150	8.371533
6.059169	401.111495	8.376550
6.335795	400.395926	8.381568
6.579868	408.168139	8.386586
6.505346	412.787176	8.391603
6.808384	406.895177	8.396621
6.652348	410.450872	8.401638
6.720944	403.601543	8.406656
6.761939	403.453061	8.411674
6.508716	401.182672	8.416691
6.278062	386.677031	8.421709
6.642192	398.974718	8.426726
6.513277	407.045210	8.431744
6.528479	404.000626	8.436762
6.657402	420.077912	8.441779
6.665196	403.003976	8.446797
6.744902	391.668577	8.451814
6.451629	381.041711	8.456832
6.447237	385.775984	8.461850
6.510019	392.904419	8.466867
6.786917	398.269953	8.471885
6.660753	395.711418	8.476902
6.263249	391.421861	8.481920
6.445251	399.412075	8.486938
6.298263	401.751384	8.491955
6.769113	400.809726	8.496973
6.521231	412.000971	8.501990
6.651804	414.094823	8.507008
6.862170	411.934829	8.512026
6.821250	407.466323	8.517043
6.758054	410.584599	8.522061
6.824398	408.882667	8.527078
6.699053	400.410108	8.532096
6.656078	392.145551	8.537114
6.328690	402.528750	8.542131
6.846682	398.111527	8.547149
6.760805	412.193310	8.552166
6.649387	407.489700	8.557184
6.537407	396.645073	8.562202
6.892695	397.144769	8.567219
6.733698	399.356573	8.572237
6.706221	402.614416	8.577255
6.445154	403.639868	8.582272
7.026124	394.198278	8.587290
6.711229	405.447355	8.592307
6.745698	396.773035	8.597325
6.636415	397.840976	8.602343
6.365080	417.477554	8.607360
6.667997	413.109805	8.612378
6.600664	420.230237	8.617395
6.466419	408.833677	8.622413
6.514574	411.887170	8.627431
6.565689	412.437682	8.632448
6.555102	415.673946	8.637466
6.365073	417.988443	8.642483
6.672470	405.515999	8.647501
6.622442	405.160876	8.652519
6.657009	413.808505	8.657536
6.886582	415.113684	8.662554
6.420123	411.563907	8.667571
6.635693	417.797423	8.672589
6.720836	441.739438	8.677607
6.817540	444.696968	8.682624
7.154399	429.493309	8.687642
6.992695	430.922911	8.692659
7.144257	423.517784	8.697677
6.819748	418.525671	8.702695
6.548081	408.914714	8.707712
6.981571	419.879285	8.712730
6.815573	422.846416	8.717747
6.933872	412.738860	8.722765
6.984023	412.014595	8.727783
6.528556	413.827890	8.732800
6.890749	422.095991	8.737818
6.842381	430.813427	8.742835
7.247115	428.569329	8.747853
6.933570	419.599236	8.752871
6.810882	423.332743	8.757888
6.784808	421.007826	8.762906
6.433015	432.982215	8.767923
7.081057	422.722225	8.772941
7.058684	440.984933	8.777959
7.173122	442.017823	8.782976
7.342764	434.347930	8.787994
6.587980	426.500995	8.793011
6.888654	424.481482	8.798029
7.018822	430.378094	8.803047
6.755394	439.542636	8.808064
7.088107	427.930890	8.813082
6.667380	439.105053	8.818099
6.894920	429.946036	8.823117
7.147154	441.696403	8.828135
7.209952	434.264154	8.833152
7.447720	440.333256	8.838170
7.050450	433.222398	8.843187
6.701086	413.203281	8.848205
7.135710	414.208092	8.853223
6.963397	427.669122	8.858240
7.326456	419.464007	8.863258
7.020885	431.936076	8.868275
7.004536	421.057516	8.873293
7.069861	424.168280	8.878311
6.791974	433.833695	8.883328
7.307940	429.625062	8.888346
7.152530	440.899665	8.893363
7.108691	432.013538	8.898381
6.937327	429.900731	8.903399
7.117506	430.853893	8.908416
7.205685	436.545650	8.913434
6.928688	438.021719	8.918451
7.202434	435.804456	8.923469
6.944859	435.611237	8.928487
6.750327	443.086119	8.933504
7.219639	437.530971	8.938522
7.130540	436.478233	8.943539
7.147410	442.061245	8.948557
7.221553	432.023713	8.953575
6.776964	432.591934	8.958592
7.034774	433.829575	8.963610
6.922470	432.180878	8.968627
6.911783	440.958686	8.973645
7.196334	437.215494	8.978663
6.733072	443.293453	8.983680
6.986454	429.671289	8.988698
7.138298	429.391832	8.993715
7.000098	434.024007	8.998733
6.427031	440.712454	9.003751
6.688517	455.749689	9.008768
7.306278	445.159919	9.013786
7.477799	455.524938	9.018803
7.601471	455.398215	9.023821
7.771464	446.813088	9.028839
7.480909	451.683732	9.033856
7.407972	434.543521	9.038874
7.215191	428.473585	9.043891
7.098784	433.105502	9.048909
6.986474	434.887122	9.053927
7.455181	438.878259	9.058944
7.368651	440.589570	9.063962
7.141832	438.068889	9.068979
7.050785	445.612763	9.073997
7.594939	448.272971	9.079015
7.073748	455.044811	9.084032
7.561223	442.866015	9.089050
7.166710	443.915534	9.094067
7.338234	440.600301	9.099085
7.667507	450.612400	9.104103
7.470623	442.277261	9.109120
7.585136	429.487888	9.114138
7.372739	429.959769	9.119155
7.227241	437.007249	9.124173
7.005418	431.118585	9.129191
7.196952	436.497506	9.134208
7.207115	431.137376	9.139226
7.221469	440.472986	9.144243
7.303932	450.545847	9.149261
7.321520	450.419966	9.154279
7.276012	457.047849	9.159296
7.462416	460.723466	9.164314
7.591555	456.714290	9.169331
7.461883	451.767379	9.174349
7.633431	454.599577	9.179367
7.371109	459.200715	9.184384
7.616298	453.204157	9.189402
7.723794	466.413094	9.194419
7.267888	447.736055	9.199437
7.549690	441.800035	9.204455
7.265267	446.161639	9.209472
7.126005	440.525121	9.214490
7.672618	453.223438	9.219507
7.598179	455.753355	9.224525
7.289701	459.295075	9.229543
7.437130	462.077405	9.234560
7.343959	459.551560	9.239578
7.718277	457.675138	9.244595
7.384718	455.398394	9.249613
7.705104	452.205000	9.254631
7.646252	455.824371	9.259648
7.584374	454.596955	9.264666
7.306940	462.286804	9.269683
7.086886	457.559177	9.274701
7.451150	451.859540	9.279719
7.293982	461.095805	9.284736
7.517322	456.279771	9.289754
7.562615	458.645763	9.294771
7.317381	459.624557	9.299789
7.439510	454.250033	9.304807
7.698233	455.159332	9.309824
7.555708	452.202569	9.314842
7.706042	456.868436	9.319859
7.538414	464.162388	9.324877
7.706414	452.084134	9.329895
7.553964	454.875580	9.334912
7.605849	450.468260	9.339930
7.725350	461.033935	9.344947
7.488691	463.235824	9.349965
7.633333	453.004199	9.354983
7.173808	462.931616	9.360000
7.130740	452.716779	9.365018
7.263867	473.634404	9.370035
7.866282	482.202561	9.375053
8.178515	483.564220	9.380071
7.800673	481.395397	9.385088
7.861244	469.018386	9.390106
7.718320	470.063200	9.395123
7.861257	459.825527	9.400141
8.068513	455.128778	9.405159
7.494860	457.639085	9.410176
7.715818	456.304238	9.415194
7.446234	452.139789	9.420211
7.139218	459.809025	9.425229
7.619406	471.605746	9.430247
7.634715	475.396535	9.435264
7.822649	481.994162	9.440282
8.185213	484.398808	9.445299
7.898398	484.781366	9.450317
8.181972	470.816773	9.455335
7.660285	472.167083	9.460352
7.936655	462.779494	9.465370
7.874510	471.275049	9.470387
7.643838	466.631134	9.475405
7.954851	461.031354	9.480423
7.618134	469.342713	9.485440
7.853858	469.886392	9.490458
7.847705	480.279263	9.495475
7.654864	482.445887	9.500493
8.008818	482.627062	9.505511
7.617287	484.761702	9.510528
7.798954	484.449169	9.515546
8.057104	487.573913	9.520563
7.670526	484.074721	9.525581
7.947315	482.825798	9.530599
7.988998	482.156505	9.535616
7.754934	491.774059	9.540634
7.676484	484.805729	9.545651
7.735959	491.499226	9.550669
7.811965	479.659427	9.555687
7.617018	484.328909	9.560704
7.624416	483.857490	9.565722
8.044233	484.782575	9.570739
7.886685	493.069028	9.575757
8.318035	477.553881	9.580775
7.959133	484.937770	9.585792
8.089023	484.339863	9.590810
8.206266	478.483263	9.595827
7.970621	488.271475	9.600845
8.158792	485.849866	9.605863
8.344102	488.294908	9.610880
8.238553	486.594655	9.615898
8.066289	486.706803	9.620915
7.765025	488.211924	9.625933
7.853442	482.744844	9.630951
8.136544	486.389536	9.635968
8.006409	481.300680	9.640986
7.980011	489.449819	9.646003
8.128198	492.642285	9.651021
8.112515	485.986009	9.656039
7.930771	485.187623	9.661056
7.913792	485.824544	9.666074
7.879537	491.314598	9.671091
7.738061	489.036156	9.676109
8.274117	479.052453	9.681127
8.235020	480.765803	9.686144
8.101044	486.561811	9.691162
8.175205	476.063508	9.696179
8.094002	486.992001	9.701197
8.286231	490.556259	9.706215
8.165271	480.148485	9.711232
8.168148	480.387824	9.716250
8.329553	478.936076	9.721267
8.261810	482.174996	9.726285
8.449261	474.783159	9.731303
8.326019	477.702574	9.736320
8.178206	480.619528	9.741338
8.128266	484.145991	9.746355
8.112395	487.695518	9.751373
8.374196	481.595363	9.756391
8.346119	483.275428	9.761408
8.215106	485.495481	9.766426
8.134341	485.719523	9.771443
8.060791	484.121553	9.776461
8.281880	480.817481	9.781479
8.202981	483.505890	9.786496
8.084437	480.658972	9.791514
8.474010	478.830650	9.796531
8.289588	482.747409	9.801549
7.868817	485.672418	9.806567
8.301739	477.266984	9.811584
7.857867	487.292947	9.816602
7.961752	476.957242	9.821619
7.822189	482.391210	9.826637
7.961057	485.632472	9.831655
8.232893	493.005900	9.836672
8.335741	513.590648	9.841690
8.604752	510.591485	9.846707
8.258275	503.592560	9.851725
8.073652	497.442427	9.856743
8.574514	501.870350	9.861760
8.541108	514.634344	9.866778
8.640151	494.112536	9.871795
8.158955	489.047125	9.876813
8.049179	488.963291	9.881831
8.493839	498.534464	9.886848
8.393962	507.496691	9.891866
8.439240	506.047357	9.896883
8.641645	505.927232	9.901901
8.451891	501.276897	9.906919
8.288061	483.027424	9.911936
8.261920	498.141320	9.916954
8.600146	506.062924	9.921971
8.749285	507.778340	9.926989
8.406762	492.658985	9.932007
8.335982	481.031531	9.937024
8.314795	499.272023	9.942042
8.471620	514.032220	9.947059
8.292786	508.054744	9.952077
8.742866	498.668321	9.957095
8.697124	506.192499	9.962112
8.240810	507.769252	9.967130
8.418561	514.223321	9.972147
8.188124	512.952885	9.977165
8.629197	514.527887	9.982183
8.862060	514.813241	9.987200
8.455057	514.984259	9.992218
8.815857	508.313167	9.997235
8.558766	514.838524	10.002253
8.604802	513.584729	10.007271
8.543619	513.316557	10.012288
8.093289	517.454866	10.017306
8.350078	507.278221	10.022323
8.241556	514.086410	10.027341
8.348807	505.353297	10.032359
8.593492	505.494789	10.037376
8.498323	515.084282	10.042394
8.798205	512.518934	10.047411
8.435149	511.758423	10.052429
8.391749	521.008452	10.057447
8.259234	511.277807	10.062464
8.329384	524.183372	10.067482
8.840923	527.341004	10.072499
8.486145	530.747982	10.077517
8.357919	539.146626	10.082535
8.943287	540.793696	10.087552
8.682076	545.732351	10.092570
8.730189	543.528337	10.097587
8.807349	534.509592	10.102605
8.901316	542.728258	10.107623
8.873083	535.105104	10.112640
8.695789	528.183802	10.117658
8.149600	523.624022	10.122675
8.191522	538.929258	10.127693
8.537939	535.596072	10.132711
8.898734	539.405326	10.137728
8.919333	544.154659	10.142746
8.916180	543.419806	10.147763
8.906049	542.966911	10.152781
8.969983	542.451919	10.157799
8.922012	534.349023	10.162816
8.769740	534.432792	10.167834
8.610600	537.354686	10.172851
8.802783	536.096925	10.177869
8.944953	542.136859	10.182887
9.094714	533.633756	10.187904
9.078211	540.796764	10.192922
9.174531	532.131622	10.197939
9.250265	531.734701	10.202957
9.007181	527.338865	10.207975
9.062998	511.863593	10.212992
8.899543	515.938019	10.218010
8.865854	514.526303	10.223027
8.592700	514.076751	10.228045
8.706745	515.472621	10.233063
9.026911	521.055474	10.238080
8.785401	519.281847	10.243098
8.984857	533.180164	10.248115
8.831624	536.893233	10.253133
9.234029	536.110615	10.258151
9.136438	511.655934	10.263168
8.606536	515.756218	10.268186
9.195093	523.632295	10.273203
9.181281	517.079855	10.278221
9.114367	522.079578	10.283239
8.846902	514.740067	10.288256
8.754071	522.214826	10.293274
9.179889	530.801209	10.298291
9.055518	525.932341	10.303309
8.960012	536.408673	10.308327
9.273318	539.688885	10.313344
8.899493	536.746258	10.318362
9.105386	535.205484	10.323379
9.233774	529.921474	10.328397
8.829130	522.382549	10.333415
9.244377	522.197518	10.338432
9.036270	530.962121	10.343450
8.835540	530.958809	10.348467
8.864895	535.501643	10.353485
8.699284	544.742429	10.358503
8.821251	534.353366	10.363520
9.005619	534.838821	10.368538
8.959929	537.130717	10.373555
9.273027	537.406656	10.378573
9.233089	542.724048	10.383591
9.448533	534.046552	10.388608
9.292142	533.821700	10.393626
9.137268	528.850314	10.398643
9.169874	537.362611	10.403661
8.972310	531.025148	10.408679
9.244053	529.401474	10.413696
8.754151	532.984258	10.418714
9.267969	531.373148	10.423731
9.046267	531.007051	10.428749
9.013060	538.459851	10.433767
9.055299	536.465040	10.438784
9.106109	535.705954	10.443802
9.087621	528.248532	10.448819
9.535311	549.072778	10.453837
9.322810	548.250806	10.458855
9.268645	532.877954	10.463872
9.186869	532.133330	10.468890
9.034743	538.973607	10.473907
9.563933	551.062502	10.478925
9.481377	561.063451	10.483943
9.480305	535.227159	10.488960
9.161482	541.932611	10.493978
9.175416	542.492108	10.498995
9.399910	550.968035	10.504013
9.057075	548.863145	10.509031
9.507091	554.564517	10.514048
9.193652	561.398520	10.519066
9.415687	563.042560	10.524083
9.762039	557.279424	10.529101
9.275157	565.929935	10.534119
9.179481	564.139766	10.539136
9.698676	568.656350	10.544154
9.222163	573.234273	10.549171
9.788227	571.403535	10.554189
9.452880	567.353504	10.559207
9.782376	558.339391	10.564224
9.477621	546.735931	10.569242
9.348754	549.791938	10.574259
9.520715	546.460839	10.579277
9.458918	554.684981	10.584295
9.074244	557.414999	10.589312
9.001504	564.236535	10.594330
9.331628	575.545600	10.599347
9.408232	578.323266	10.604365
9.187623	575.770035	10.609383
9.546538	568.597445	10.614400
9.453710	569.015881	10.619418
9.114346	575.992806	10.624435
9.185322	565.883111	10.629453
9.145868	576.855610	10.634471
9.304179	589.286663	10.639488
10.029670	597.431651	10.644506
9.506483	604.547842	10.649523
10.228338	594.755869	10.654541
9.754431	587.922043	10.659559
9.668337	580.427856	10.664576
9.799314	574.240871	10.669594
9.467471	567.028190	10.674611
9.707114	569.780309	10.679629
9.637896	574.259703	10.684647
9.570087	566.731098	10.689664
9.571828	565.181284	10.694682
9.534210	561.371782	10.699699
9.493354	573.439557	10.704717
9.760668	587.298881	10.709735
10.043970	587.557399	10.714752
9.719386	576.723883	10.719770
9.621778	581.788392	10.724787
9.529830	566.345693	10.729805
9.560082	585.976228	10.734823
9.518351	592.742423	10.739840
9.686388	589.781158	10.744858
9.587723	597.386250	10.749875
10.012273	598.042357	10.754893
10.172779	596.896852	10.759911
10.073398	591.405516	10.764928
9.727580	581.373740	10.769946
9.776296	581.811024	10.774963
9.745588	599.434575	10.779981
9.826971	602.482894	10.784999
9.826028	597.755613	10.790016
9.692511	595.794645	10.795034
9.510613	595.943017	10.800051
9.904149	591.535780	10.805069
10.097815	588.810339	10.810087
9.809798	593.727961	10.815104
9.659135	594.010293	10.820122
9.882648	593.340908	10.825139
9.690907	593.516068	10.830157
9.683241	592.191787	10.835175
9.836602	601.063890	10.840192
9.730360	598.824094	10.845210
9.818957	596.632665	10.850227
9.759031	591.072031	10.855245
9.934055	595.932881	10.860263
9.980689	599.037137	10.865280
9.850871	594.806574	10.870298
9.680355	595.906212	10.875315
9.916586	603.774413	10.880333
10.028807	616.723945	10.885351
10.352053	614.871288	10.890368
9.824213	601.592305	10.895386
10.133461	608.290891	10.900403
9.910764	601.152613	10.905421
10.118770	618.035037	10.910439
9.911247	616.016235	10.915456
10.324476	612.820889	10.920474
10.156097	605.800330	10.925491
9.972157	601.912760	10.930509
10.204187	620.533421	10.935527
9.841661	609.731077	10.940544
10.078997	620.089035	10.945562
10.294037	625.470642	10.950579
10.099562	619.789069	10.955597
10.496763	617.669205	10.960615
10.311663	605.204361	10.965632
10.054193	598.169362	10.970650
9.784915	599.581119	10.975667
10.107010	606.224042	10.980685
10.102388	616.332732	10.985703
10.469833	623.514509	10.990720
10.308418	616.025797	10.995738
10.000103	622.010110	11.000755
9.873650	625.150958	11.005773
10.016845	634.911450	11.010791
9.956635	625.860535	11.015808
10.515586	613.474764	11.020826
10.150281	628.528303	11.025843
9.960234	628.734755	11.030861
10.433768	627.145728	11.035879
9.993287	632.731031	11.040896
10.422794	620.482302	11.045914
9.996102	628.189296	11.050931
10.353065	619.795697	11.055949
9.966520	628.187521	11.060967
10.112998	629.458398	11.065984
10.630026	620.578973	11.071002
9.838996	634.986011	11.076019
10.767519	637.907915	11.081037
10.272112	625.144539	11.086055
10.516809	631.891118	11.091072
10.607497	631.286724	11.096090
10.218655	629.741298	11.101107
10.139309	622.425917	11.106125
10.454682	631.190599	11.111143
10.571362	635.009721	11.116160
11.017596	622.856199	11.121178
10.483851	627.367364	11.126195
10.471518	622.130621	11.131213
10.318619	624.319406	11.136231
10.142945	618.000573	11.141248
10.369176	618.946529	11.146266
10.051851	634.402809	11.151283
10.561951	638.526361	11.156301
10.501867	650.161700	11.161319
10.372656	653.050521	11.166336
10.772253	648.061653	11.171354
10.617572	656.379290	11.176371
10.771138	648.175338	11.181389
10.871119	646.291388	11.186407
10.215045	640.129868	11.191424
10.836513	633.048658	11.196442
10.589631	632.399327	11.201459
10.533103	631.366721	11.206477
10.613306	643.399796	11.211495
10.641930	646.415364	11.216512
10.765574	642.075649	11.221530
10.388657	635.482228	11.226547
10.633137	641.809123	11.231565
10.537290	657.666221	11.236583
10.476559	651.578674	11.241600
10.214699	653.964416	11.246618
10.295576	659.521688	11.251635
10.304102	647.392550	11.256653
10.789214	647.221818	11.261671
10.208718	647.590433	11.266688
10.589391	648.827773	11.271706
10.619334	650.915330	11.276723
10.852367	650.651550	11.281741
10.476500	650.931299	11.286759
10.391657	661.873092	11.291776
10.845557	664.727355	11.296794
10.584140	669.217952	11.301811
10.947393	673.673790	11.306829
10.653273	679.255111	11.311847
11.049038	677.659329	11.316864
10.911158	668.399655	11.321882
11.097302	679.437855	11.326899
11.192389	672.814646	11.331917
11.120186	663.175455	11.336935
10.562799	656.853300	11.341952
10.955673	655.911224	11.346970
10.549673	656.416601	11.351987
10.849172	667.231905	11.357005
11.036950	663.251366	11.362023
10.711985	683.089142	11.367040
11.032396	678.361982	11.372058
10.957603	675.186286	11.377075
11.069711	664.432618	11.382093
11.332878	666.720319	11.387111
11.103077	668.230037	11.392128
10.935492	649.151005	11.397146
10.849066	652.361326	11.402163
10.947411	660.374233	11.407181
10.938586	666.923862	11.412199
10.757001	682.040178	11.417216
10.954677	667.666012	11.422234
11.231551	671.810336	11.427251
11.126388	674.891052	11.432269
11.191642	673.233447	11.437287
10.790251	675.416992	11.442304
11.052647	670.698923	11.447322
10.713295	674.867217	11.452339
10.593395	676.012577	11.457357
11.087030	680.163965	11.462375
10.753120	681.355481	11.467392
11.100437	664.265967	11.472410
11.354022	666.274303	11.477427
11.233177	681.059209	11.482445
11.221884	678.870798	11.487463
10.843368	679.532815	11.492480
11.017007	667.507181	11.497498
10.766144	670.333015	11.502515
10.703258	681.590116	11.507533
11.197920	683.686913	11.512551
10.960850	700.377220	11.517568
11.368599	704.513669	11.522586
11.216493	701.482625	11.527603
11.275705	706.355340	11.532621
11.525145	698.278354	11.537639
11.382592	705.839875	11.542656
11.262402	680.429137	11.547674
11.362301	699.222062	11.552691
11.460789	700.538334	11.557709
11.206959	674.040854	11.562727
11.166159	693.900390	11.567744
11.492534	691.775836	11.572762
11.772047	691.713057	11.577779
11.411361	683.207809	11.582797
11.147349	681.349330	11.587815
11.246595	673.456834	11.592832
11.086561	674.958777	11.597850
11.679438	688.953363	11.602867
11.266868	692.981654	11.607885
11.516259	702.523572	11.612903
11.581157	703.715718	11.617920
11.240897	682.561936	11.622938
12.020779	691.979704	11.627955
11.459345	681.353649	11.632973
11.263422	680.702643	11.637991
11.360728	681.820282	11.643008
11.675936	681.303785	11.648026
10.917322	681.933839	11.653043
11.164821	700.814092	11.658061
11.830829	700.166891	11.663079
11.811990	704.950849	11.668096
11.556121	707.742758	11.673114
11.948976	715.176212	11.678131
11.430894	703.738619	11.683149
11.045316	689.894480	11.688167
11.424211	709.006619	11.693184
11.637838	701.616898	11.698202
11.686685	698.374489	11.703219
11.527722	703.928328	11.708237
11.609479	704.306790	11.713255
11.605917	705.885205	11.718272
11.382498	702.751726	11.723290
11.745691	710.748404	11.728307
11.636975	708.755136	11.733325
11.756945	708.344968	11.738343
11.791398	707.395932	11.743360
11.714826	704.144770	11.748378
11.575360	698.053765	11.753395
11.197019	708.407255	11.758413
11.750359	699.986006	11.763431
11.703308	712.903759	11.768448
11.817106	702.190829	11.773466
11.991821	708.314083	11.778483
11.727482	705.824489	11.783501
11.724233	708.485299	11.788519
11.587636	702.639996	11.793536
11.434485	710.458801	11.798554
11.748087	708.241571	11.803571
11.510918	706.965864	11.808589
11.623833	698.446365	11.813607
11.589668	705.463883	11.818624
11.708948	725.449852	11.823642
12.030036	736.678383	11.828659
11.843508	730.913479	11.833677
11.950180	733.383500	11.838695
12.004283	740.352487	11.843712
11.857040	736.995627	11.848730
11.937946	733.094933	11.853747
11.981893	733.242633	11.858765
12.118126	723.810593	11.863783
11.841350	730.383293	11.868800
11.568546	730.082004	11.873818
11.791348	733.401679	11.878835
11.696216	746.544741	11.883853
11.970017	729.062739	11.888871
12.053689	732.448395	11.893888
11.622667	741.756115	11.898906
12.060477	735.344273	11.903923
11.693532	738.715327	11.908941
12.095515	740.713043	11.913959
11.936722	735.458189	11.918976
11.536265	740.898399	11.923994
11.922582	739.613363	11.929011
11.817101	756.147403	11.934029
12.171814	756.322151	11.939047
12.157799	765.558234	11.944064
12.420949	768.950489	11.949082
12.170500	766.244114	11.954099
12.152601	775.556551	11.959117
12.103469	762.937748	11.964135
12.222801	760.384876	11.969152
11.874560	758.612169	11.974170
12.161446	762.821218	11.979187
12.058028	769.672885	11.984205
12.402899	760.473225	11.989223
12.021379	759.447351	11.994240
12.108840	756.965745	11.999258
12.351283	753.910743	12.004275
12.037615	769.738953	12.009293
12.100416	767.005588	12.014311
12.507539	774.108626	12.019328
12.354422	771.175560	12.024346
12.307427	768.809694	12.029363
12.591581	771.220353	12.034381
12.436190	765.141288	12.039399
11.979708	770.239988	12.044416
12.416913	766.965120	12.049434
12.811089	755.734854	12.054451
12.246406	770.403182	12.059469
12.238698	768.734909	12.064487
12.234312	757.431390	12.069504
11.971387	764.506864	12.074522
12.221654	762.469966	12.079539
11.917904	759.743541	12.084557
12.243757	756.956339	12.089575
12.242058	771.261901	12.094592
12.134759	776.261711	12.099610
12.608340	774.805208	12.104627
12.206923	782.161166	12.109645
12.669686	780.119374	12.114663
12.700980	782.282474	12.119680
12.443554	789.041514	12.124698
12.665483	786.633510	12.129715
12.365981	791.647660	12.134733
12.497444	777.015536	12.139751
12.308137	794.752491	12.144768
12.413345	785.836524	12.149786
12.715052	780.490570	12.154803
12.775432	781.102757	12.159821
12.687564	780.144481	12.164839
12.745077	788.416309	12.169856
12.985543	782.906379	12.174874
12.885166	779.188715	12.179891
12.696327	787.871529	12.184909
12.736713	777.192148	12.189927
12.963309	778.911233	12.194944
12.439822	774.433038	12.199962
12.971917	767.271105	12.204979
12.420102	776.499939	12.209997
12.280656	779.343046	12.215015
12.613067	782.670803	12.220032
12.649734	786.909595	12.225050
12.802553	779.775525	12.230067
12.848856	789.526036	12.235085
12.951955	786.751640	12.240103
12.573833	783.200570	12.245120
12.623908	785.834102	12.250138
12.776951	779.321694	12.255155
12.967083	778.114731	12.260173
12.524867	777.969374	12.265191
12.830557	791.365249	12.270208
12.483041	787.285516	12.275226
12.702421	775.656588	12.280243
12.585737	769.085460	12.285261
12.753930	779.280774	12.290279
12.743988	791.268112	12.295296
12.957298	807.379862	12.300314
13.293980	803.237104	12.305331
13.176439	807.351739	12.310349
13.015286	794.422260	12.315367
13.319185	780.634123	12.320384
12.619601	783.486100	12.325402
12.756868	785.234962	12.330419
12.575168	802.074478	12.335437
13.295668	797.792688	12.340455
13.479489	807.928765	12.345472
13.416350	806.442745	12.350490
13.232663	792.854073	12.355507
13.305795	785.057138	12.360525
12.886879	783.607929	12.365543
12.888940	782.272642	12.370560
12.919748	790.750629	12.375578
12.948252	784.819470	12.380595
13.376848	797.482876	12.385613
13.232518	798.767772	12.390631
13.230672	778.539159	12.395648
13.034347	783.603412	12.400666
12.979027	797.888995	12.405683
13.110471	794.617847	12.410701
13.516330	803.185399	12.415719
13.428330	808.901723	12.420736
13.202476	798.879431	12.425754
13.414632	782.899743	12.430771
12.951779	796.463377	12.435789
12.700527	799.418681	12.440807
13.479192	808.505339	12.445824
13.240168	813.285955	12.450842
13.596885	811.595294	12.455859
13.404542	810.830112	12.460877
13.330398	813.407370	12.465895
13.648189	812.432870	12.470912
13.249782	807.354395	12.475930
13.714138	792.730060	12.480947
13.107875	789.915328	12.485965
13.159762	792.772641	12.490983
13.128441	795.169617	12.496000
12.926159	807.234439	12.501018
13.307791	802.718562	12.506035
13.238185	804.550333	12.511053
13.053962	809.555893	12.516071
13.603539	802.902451	12.521088
13.295128	809.921954	12.526106
13.098279	804.281720	12.531123
13.597257	814.213784	12.536141
13.401487	806.414792	12.541159
13.466676	806.385593	12.546176
13.510316	814.198856	12.551194
13.747320	818.179046	12.556211
13.420986	820.019485	12.561229
13.361270	829.209112	12.566247
13.803924	829.998093	12.571264
13.770078	843.428272	12.576282
13.740341	837.528312	12.581299
13.678752	816.488499	12.586317
13.299426	826.239447	12.591335
13.849477	828.255000	12.596352
13.433282	837.386875	12.601370
13.797767	840.671748	12.606387
13.947559	839.594179	12.611405
13.656483	839.933229	12.616423
13.899158	832.144424	12.621440
13.559580	832.696203	12.626458
13.630164	834.695361	12.631475
13.557776	838.032904	12.636493
13.585755	842.553940	12.641511
13.957975	832.718791	12.646528
13.857588	839.491114	12.651546
14.152962	836.345754	12.656563
14.221716	839.869468	12.661581
13.309547	827.086039	12.666599
13.795072	822.045790	12.671616
14.025703	838.558801	12.676634
14.119821	838.149526	12.681651
13.762204	838.240223	12.686669
13.542042	832.859255	12.691687
13.995519	835.719925	12.696704
13.623346	835.222761	12.701722
13.606703	824.075756	12.706739
13.834117	832.279958	12.711757
13.653672	833.573671	12.716775
14.073386	827.467592	12.721792
13.982558	833.711392	12.726810
13.860772	823.025834	12.731827
13.848262	820.919648	12.736845
13.754664	832.487772	12.741863
13.856687	835.498184	12.746880
13.629195	840.930258	12.751898
14.082492	853.555119	12.756915
14.239932	851.924080	12.761933
14.184573	857.098812	12.766951
14.322240	851.854280	12.771968
13.851909	852.805246	12.776986
14.444808	852.245235	12.782003
14.347251	845.879367	12.787021
14.068933	845.058226	12.792039
14.176091	838.439376	12.797056
13.940206	838.649857	12.802074
13.668932	855.793796	12.807091
14.214881	852.340925	12.812109
14.041550	861.412669	12.817127
14.367168	856.113440	12.822144
14.220210	859.661489	12.827162
14.243262	862.068889	12.832179
14.509185	855.649222	12.837197
14.099845	859.613927	12.842215
13.914794	850.247939	12.847232
13.865487	854.856828	12.852250
13.623093	861.462060	12.857267
13.911996	868.479516	12.862285
14.073656	875.504288	12.867303
14.530199	875.227576	12.872320
14.424257	885.415409	12.877338
14.433141	895.862972	12.882355
14.722568	886.236427	12.887373
14.461200	891.045812	12.892391
14.686084	881.022279	12.897408
14.689314	884.187035	12.902426
14.403369	873.407246	12.907443
14.721729	862.109897	12.912461
14.489744	872.680393	12.917479
14.344075	867.881042	12.922496
14.654144	862.697857	12.927514
14.384238	866.634404	12.932531
14.298818	864.624845	12.937549
14.580976	873.596825	12.942567
14.856631	875.917311	12.947584
14.690583	886.234485	12.952602
14.184902	881.601991	12.957619
14.579202	888.293669	12.962637
14.571479	885.801712	12.967655
15.016639	889.064486	12.972672
14.769868	892.454609	12.977690
14.530406	896.184419	12.982707
14.829708	883.047028	12.987725
14.441500	889.403714	12.992743
15.006955	889.463392	12.997760
14.966018	889.299341	13.002778
14.439019	879.226357	13.007795
14.729718	884.362655	13.012813
14.718654	885.775002	13.017831
14.961138	887.772479	13.022848
14.845370	885.777140	13.027866
14.941327	888.526575	13.032883
14.827541	876.583706	13.037901
14.654474	885.554434	13.042919
14.772725	887.091688	13.047936
14.641122	881.296038	13.052954
14.760886	893.054836	13.057971
14.770367	888.631961	13.062989
14.770397	886.444907	13.068007
14.947280	881.187909	13.073024
14.996833	885.080719	13.078042
14.627753	892.068733	13.083059
14.716896	881.523663	13.088077
14.812953	885.996174	13.093095
14.731675	877.412341	13.098112
15.094317	883.960652	13.103130
14.827815	889.420944	13.108147
15.216647	879.488491	13.113165
14.977350	882.246272	13.118183
14.923783	879.777279	13.123200
15.262350	879.348636	13.128218
14.936933	897.940163	13.133235
14.877813	883.713358	13.138253
15.242431	891.867688	13.143271
15.026266	891.308208	13.148288
15.596066	885.459464	13.153306
14.964181	887.723330	13.158323
15.223109	880.765100	13.163341
15.247794	883.967520	13.168359
14.986527	881.307005	13.173376
15.178063	884.991373	13.178394
14.873731	889.829580	13.183411
15.506106	896.648062	13.188429
15.210124	897.821025	13.193447
15.362789	904.033009	13.198464
15.294891	912.062609	13.203482
15.050456	907.789969	13.208499
15.206237	900.292464	13.213517
15.566825	900.908112	13.218535
15.085961	907.320348	13.223552
15.392141	906.925182	13.228570
15.098467	905.405846	13.233587
15.647963	903.839607	13.238605
15.545057	909.665598	13.243623
15.324655	909.034197	13.248640
15.525944	912.227887	13.253658
15.067387	905.650313	13.258675
15.232665	910.140386	13.263693
15.262063	915.882532	13.268711
15.115842	902.997972	13.273728
15.533254	905.349900	13.278746
15.360012	904.199864	13.283763
15.559364	905.285749	13.288781
15.513768	915.719769	13.293799
15.295981	915.627609	13.298816
15.330361	909.695488	13.303834
15.389297	914.694536	13.308851
15.694564	933.648037	13.313869
15.811890	932.550303	13.318887
15.636079	930.340301	13.323904
15.991920	923.786598	13.328922
15.506964	916.799740	13.333939
15.465734	912.731948	13.338957
15.312607	913.017827	13.343975
15.627893	930.095179	13.348992
15.771916	932.439453	13.354010
15.823812	939.980074	13.359027
15.919052	927.714081	13.364045
15.909005	932.004409	13.369063
15.882844	933.911438	13.374080
15.773946	937.403045	13.379098
15.766412	936.883460	13.384115
15.983804	932.658376	13.389133
16.113366	923.113666	13.394151
15.917676	926.473701	13.399168
15.645909	907.420185	13.404186
15.810290	921.611482	13.409203
16.254086	924.401098	13.414221
16.220218	918.217732	13.419239
15.706269	909.815286	13.424256
15.988214	903.405715	13.429274
15.680702	910.541882	13.434291
16.032642	922.046568	13.439309
16.286649	921.940447	13.444327
16.073920	923.056186	13.449344
15.887000	909.944464	13.454362
16.140275	910.876733	13.459379
15.520552	905.905490	13.464397
15.795403	916.888913	13.469415
16.095882	922.557029	13.474432
16.247732	914.589912	13.479450
16.312019	918.928551	13.484467
16.495341	924.299439	13.489485
16.431367	922.772513	13.494503
16.423079	926.324095	13.499520
15.960578	910.749806	13.504538
15.864824	906.756832	13.509555
16.243782	918.926322	13.514573
16.152635	927.300403	13.519591
16.243819	933.828149	13.524608
16.554494	925.302803	13.529626
15.947044	915.867262	13.534643
16.259458	928.861394	13.539661
16.565530	927.191281	13.544679
16.040003	925.275918	13.549696
16.129144	922.642546	13.554714
15.891474	936.461341	13.559731
16.253296	927.987942	13.564749
16.408766	936.926154	13.569767
16.179910	936.532767	13.574784
16.228373	928.076906	13.579802
16.258634	930.599953	13.584819
16.178811	925.086514	13.589837
15.987796	929.780742	13.594855
16.186728	927.433128	13.599872
16.136426	937.451325	13.604890
16.228183	956.081691	13.609907
16.431798	950.138820	13.614925
16.349668	960.777408	13.619943
16.287202	958.369759	13.624960
16.634606	952.240254	13.629978
15.984723	950.107683	13.634995
16.600682	964.338715	13.640013
16.881506	950.345777	13.645031
16.613229	959.135796	13.650048
16.501479	953.374882	13.655066
16.559970	956.701409	13.660083
16.584532	947.971569	13.665101
16.755841	952.154590	13.670119
16.727752	965.180008	13.675136
16.891320	954.932508	13.680154
16.886482	960.771552	13.685171
16.629982	949.639959	13.690189
16.575150	946.495802	13.695207
16.414736	959.857535	13.700224
16.979992	954.344002	13.705242
16.952980	954.745822	13.710259
16.835113	959.081453	13.715277
16.844971	945.572795	13.720295
16.650515	950.097151	13.725312
16.932114	955.493676	13.730330
16.802462	958.398394	13.735347
16.925505	946.295293	13.740365
17.441684	949.622691	13.745383
17.183452	954.775589	13.750400
17.208623	949.529719	13.755418
16.846094	957.081630	13.760435
16.703843	953.133801	13.765453
17.065590	948.232833	13.770471
16.606410	953.363566	13.775488
17.055012	945.905371	13.780506
16.976639	950.525150	13.785523
17.155600	958.636014	13.790541
17.086244	955.478351	13.795559
16.703491	964.163231	13.800576
17.302004	973.120409	13.805594
17.596458	966.910830	13.810611
17.377792	957.887730	13.815629
17.239333	955.331039	13.820647
16.942831	960.527806	13.825664
17.218232	951.613492	13.830682
16.929567	951.178981	13.835699
17.111721	951.835212	13.840717
17.177942	956.369221	13.845735
16.873048	965.742502	13.850752
17.245675	974.981230	13.855770
17.037317	973.975549	13.860787
17.166548	967.015516	13.865805
17.298746	972.072531	13.870823
17.217428	983.651452	13.875840
17.513005	968.785171	13.880858
17.145137	971.843982	13.885875
17.290165	977.094651	13.890893
17.570830	973.036372	13.895911
17.095448	978.731394	13.900928
17.375718	979.949776	13.905946
17.450886	982.399521	13.910963
16.788270	988.635132	13.915981
17.196536	988.132449	13.920999
17.355422	981.906236	13.926016
17.341605	994.591763	13.931034
17.289099	999.614608	13.936051
17.389776	1010.022608	13.941069
17.439078	1006.085781	13.946087
17.528756	1006.652360	13.951104
17.508912	1004.897602	13.956122
17.785319	1005.936706	13.961139
17.564692	1004.254435	13.966157
17.843017	1003.380784	13.971175
17.505627	1007.233260	13.976192
17.740281	1000.326125	13.981210
17.916878	1006.969905	13.986227
17.547527	1006.368151	13.991245
17.968203	1003.698600	13.996263
17.954728	1010.359539	14.001280
17.767235	1011.638589	14.006298
17.838820	1000.957342	14.011315
17.894853	1006.635382	14.016333
17.968060	1010.445616	14.021351
18.185405	1002.259912	14.026368
18.078459	1003.769343	14.031386
17.878355	1001.424280	14.036403
17.976853	999.095549	14.041421
17.952672	982.508916	14.046439
17.783739	987.265973	14.051456
17.913716	1001.895077	14.056474
18.051484	999.658025	14.061491
17.819106	1001.818282	14.066509
18.088595	999.601618	14.071527
17.647911	1006.622986	14.076544
17.744733	1001.662526	14.081562
17.802989	990.929723	14.086579
17.880582	998.788240	14.091597
17.631264	993.803119	14.096615
18.160091	1002.181084	14.101632
17.917707	1005.337006	14.106650
18.269833	1003.656514	14.111667
18.052031	1002.945806	14.116685
18.226215	993.690718	14.121703
18.020905	1002.398308	14.126720
17.998541	1002.477503	14.131738
17.976337	995.613772	14.136755
17.721279	1001.040746	14.141773
18.361133	1003.177951	14.146791
18.218166	1024.164726	14.151808
18.256937	1024.196473	14.156826
18.630553	1023.128006	14.161843
18.261521	1030.646253	14.166861
18.309092	1016.497302	14.171879
18.426794	1022.127814	14.176896
18.252681	1020.577111	14.181914
18.477010	1014.877130	14.186931
18.594092	1016.408267	14.191949
18.446026	1008.702699	14.196967
18.118920	1016.558360	14.201984
18.129689	1018.961395	14.207002
18.031075	1013.637069	14.212019
18.612639	1023.594182	14.217037
18.340039	1009.189283	14.222055
18.717501	1016.880900	14.227072
18.450050	1019.314904	14.232090
18.566961	1027.596471	14.237107
18.275164	1028.295406	14.242125
18.616831	1026.594460	14.247143
18.379891	1030.825685	14.252160
18.501872	1030.677133	14.257178
18.804673	1021.026330	14.262195
18.539723	1023.797620	14.267213
18.480803	1025.836026	14.272231
18.510087	1032.234648	14.277248
18.569498	1029.877322	14.282266
18.797586	1019.010594	14.287283
18.756917	1024.075773	14.292301
18.501262	1021.720476	14.297319
18.710230	1040.332565	14.302336
18.962705	1046.503714	14.307354
18.627768	1053.779938	14.312371
18.828602	1058.106684	14.317389
19.409544	1046.449333	14.322407
19.055267	1041.120875	14.327424
18.987612	1039.048550	14.332442
18.963309	1023.134100	14.337459
18.686441	1021.536379	14.342477
18.701635	1024.705597	14.347495
19.116358	1046.340336	14.352512
19.031176	1051.115846	14.357530
19.443891	1041.081729	14.362547
18.703543	1048.279457	14.367565
18.940181	1037.193622	14.372583
18.981291	1054.342455	14.377600
18.878839	1056.905249	14.382618
19.165877	1053.568649	14.387635
19.158700	1065.580984	14.392653
19.143651	1048.895028	14.397671
19.252374	1046.201763	14.402688
18.998109	1051.107909	14.407706
19.456368	1052.124835	14.412723
18.744949	1048.900494	14.417741
19.423833	1045.846490	14.422759
19.167306	1037.968551	14.427776
19.260107	1057.719194	14.432794
19.426684	1045.517684	14.437811
19.250191	1046.801325	14.442829
19.448528	1035.822480	14.447847
19.540696	1043.378926	14.452864
19.444539	1047.452394	14.457882
19.320088	1039.099315	14.462899
18.943359	1052.394023	14.467917
19.300977	1045.502319	14.472935
19.329913	1048.110799	14.477952
19.420675	1045.657039	14.482970
19.426301	1042.108907	14.487987
19.148211	1052.996009	14.493005
18.815678	1040.506623	14.498023
19.275989	1043.400971	14.503040
19.262475	1052.277354	14.508058
19.491011	1052.695943	14.513075
19.734700	1065.117106	14.518093
19.351812	1064.444885	14.523111
19.529637	1064.789367	14.528128
19.313782	1079.841958	14.533146
19.816720	1067.357353	14.538163
19.756924	1074.350628	14.543181
19.606264	1073.755632	14.548199
19.942879	1071.266504	14.553216
19.849774	1072.442405	14.558234
19.796181	1071.945813	14.563251
19.931031	1075.547582	14.568269
19.599090	1064.863249	14.573287
19.554770	1065.050028	14.578304
19.975054	1070.866682	14.583322
19.794801	1067.063640	14.588339
20.066031	1071.410918	14.593357
19.890173	1074.417571	14.598375
19.945646	1078.438886	14.603392
19.784144	1072.603676	14.608410
20.029884	1057.420074	14.613427
19.871121	1071.961930	14.618445
19.819107	1062.111072	14.623463
20.033662	1066.987949	14.628480
19.691281	1070.557191	14.633498
20.076923	1066.384611	14.638515
20.195734	1074.927841	14.643533
19.454060	1065.753096	14.648551
20.008506	1064.571086	14.653568
19.825802	1064.814263	14.658586
19.615868	1062.041533	14.663603
19.621428	1068.238753	14.668621
20.184815	1077.166772	14.673639
20.526009	1083.683803	14.678656
20.009861	1083.288087	14.683674
20.130405	1089.221140	14.688691
19.952675	1095.541764	14.693709
20.180035	1094.041763	14.698727
20.346714	1089.114515	14.703744
20.399891	1102.430265	14.708762
20.407641	1100.402925	14.713779
20.209443	1100.437085	14.718797
20.449953	1094.431580	14.723815
20.546220	1089.729964	14.728832
20.437196	1084.066413	14.733850
20.449027	1090.328931	14.738867
20.378932	1092.706775	14.743885
20.218142	1099.977823	14.748903
20.347401	1091.900555	14.753920
20.298076	1090.986717	14.758938
20.528969	1093.958045	14.763955
20.236490	1093.877587	14.768973
20.357954	1098.825864	14.773991
20.562524	1095.896662	14.779008
20.550913	1099.041690	14.784026
20.559203	1089.951404	14.789043
20.321828	1103.382109	14.794061
20.514420	1091.501547	14.799079
20.708008	1091.733104	14.804096
20.262346	1095.236481	14.809114
20.656771	1100.208263	14.814131
20.467490	1111.895704	14.819149
20.628087	1122.553163	14.824167
20.779558	1118.130076	14.829184
20.893049	1128.981117	14.834202
20.993172	1110.585502	14.839219
20.931078	1112.558142	14.844237
20.825640	1104.852165	14.849255
20.911668	1106.953078	14.854272
20.507130	1108.550172	14.859290
20.965163	1108.532007	14.864307
21.073101	1120.873491	14.869325
20.809508	1119.216875	14.874343
21.051265	1114.350442	14.879360
20.890611	1120.065625	14.884378
20.810443	1115.240165	14.889395
20.773364	1115.687749	14.894413
20.606920	1119.522932	14.899431
21.162084	1110.286988	14.904448
20.946119	1120.640520	14.909466
21.269727	1126.434468	14.914483
20.878661	1120.531067	14.919501
20.774359	1118.032119	14.924519
21.257081	1106.456393	14.929536
21.119825	1114.948242	14.934554
21.168436	1113.037577	14.939571
21.509912	1110.661294	14.944589
21.306372	1110.693136	14.949607
21.197166	1116.504401	14.954624
21.195348	1120.578885	14.959642
21.250016	1116.167809	14.964659
21.226021	1122.073026	14.969677
21.422811	1111.842322	14.974695
21.650388	1118.459220	14.979712
21.281135	1114.228178	14.984730
21.238401	1118.293293	14.989747
21.453962	1119.026349	14.994765
21.029914	1116.691111	14.999783
21.275907	1108.696535	15.004800
21.166692	1122.006185	15.009818
21.635535	1129.431063	15.014835
21.636116	1132.978140	15.019853
21.659736	1139.810045	15.024871
21.861576	1134.009406	15.029888
21.537356	1123.686754	15.034906
21.420638	1119.308843	15.039923
21.889834	1119.831742	15.044941
21.731705	1125.410828	15.049959
21.847076	1115.196035	15.054976
21.444945	1119.667764	15.059994
21.412845	1126.183337	15.065011
21.606140	1136.832526	15.070029
21.851975	1141.335283	15.075047
21.942541	1132.011172	15.080064
21.954075	1142.073445	15.085082
21.860602	1137.145918	15.090099
21.939904	1140.305112	15.095117
21.689390	1149.455369	15.100135
21.986793	1142.061809	15.105152
21.695316	1146.169059	15.110170
22.067416	1143.873182	15.115187
22.143160	1132.569494	15.120205
21.672385	1138.427950	15.125223
21.793559	1136.692112	15.130240
21.927457	1141.988756	15.135258
21.838846	1139.730350	15.140275
22.043540	1133.563181	15.145293
21.966527	1138.665646	15.150311
21.972618	1135.682328	15.155328
22.063603	1137.271214	15.160346
21.819182	1133.806425	15.165363
22.371884	1126.511730	15.170381
21.804066	1137.775646	15.175399
22.091404	1133.419632	15.180416
21.956094	1145.925481	15.185434
21.873919	1142.119680	15.190451
22.121197	1132.411243	15.195469
22.188556	1141.297090	15.200487
22.450003	1138.936498	15.205504
22.571563	1152.882217	15.210522
22.139183	1143.703154	15.215539
22.461528	1138.779906	15.220557
22.074898	1136.820665	15.225575
22.521106	1137.167280	15.230592
22.133755	1150.539466	15.235610
22.791095	1155.340678	15.240627
22.500794	1153.461020	15.245645
22.132484	1163.794264	15.250663
22.406236	1154.772808	15.255680
22.320176	1156.171679	15.260698
22.426946	1154.611670	15.265715
22.296058	1162.761707	15.270733
22.723667	1165.048956	15.275751
22.858999	1157.649224	15.280768
22.728496	1155.624604	15.285786
22.454905	1166.694112	15.290803
22.616977	1148.336090	15.295821
22.556987	1158.280186	15.300839
22.537284	1159.447749	15.305856
22.526583	1152.440139	15.310874
22.293145	1155.642025	15.315891
22.743872	1158.490555	15.320909
22.917991	1164.970676	15.325927
22.970265	1158.085745	15.330944
22.900010	1155.654043	15.335962
22.538089	1157.907201	15.340979
22.924586	1164.000586	15.345997
23.005435	1182.658144	15.351015
22.859573	1184.429316	15.356032
22.885740	1182.105582	15.361050
22.985351	1183.753083	15.366067
23.149783	1176.061598	15.371085
23.070964	1178.150478	15.376103
23.056863	1173.027463	15.381120
23.249221	1178.501156	15.386138
23.111456	1177.967255	15.391155
23.395703	1180.863964	15.396173
23.170250	1180.059771	15.401191
23.266874	1172.082257	15.406208
23.161134	1161.558089	15.411226
23.034793	1162.108025	15.416243
23.240244	1168.532744	15.421261
22.936831	1177.918528	15.426279
23.281360	1173.503049	15.431296
23.184871	1175.032947	15.436314
23.113989	1174.068832	15.441331
23.279173	1180.256860	15.446349
22.953177	1182.027852	15.451367
23.224785	1174.732998	15.456384
22.941253	1165.511666	15.461402
22.948655	1169.947644	15.466419
23.710071	1171.952212	15.471437
23.408489	1188.144980	15.476455
23.592499	1183.391721	15.481472
23.620429	1170.277705	15.486490
23.476403	1174.999349	15.491507
23.733614	1173.422079	15.496525
23.231891	1178.774142	15.501543
23.330905	1180.974018	15.506560
23.616420	1192.662860	15.511578
23.417701	1200.782516	15.516595
23.617957	1199.438236	15.521613
23.791108	1210.848042	15.526631
24.070819	1198.887485	15.531648
24.093793	1201.881941	15.536666
23.675509	1205.103330	15.541683
23.937866	1190.882717	15.546701
23.920200	1205.926453	15.551719
24.015873	1192.587205	15.556736
23.646378	1183.701234	15.561754
23.640435	1202.435530	15.566771
23.998142	1191.964967	15.571789
23.890946	1195.036623	15.576807
23.847322	1191.480399	15.581824
24.257987	1195.184149	15.586842
23.794927	1192.867637	15.591859
24.046790	1189.807930	15.596877
24.196397	1197.664720	15.601895
24.076847	1197.023819	15.606912
24.127201	1200.815583	15.611930
24.088920	1192.341630	15.616947
24.286369	1186.781510	15.621965
24.300554	1197.099026	15.626983
23.933702	1194.464474	15.632000
24.374131	1190.993359	15.637018
24.295699	1194.871574	15.642035
24.313354	1190.128599	15.647053
24.075686	1195.161575	15.652071
24.445343	1192.417937	15.657088
24.683570	1184.364581	15.662106
23.911019	1191.823039	15.667123
24.570983	1184.123339	15.672141
24.520543	1191.421316	15.677159
24.388268	1191.015946	15.682176
24.610517	1186.285098	15.687194
24.090999	1189.187820	15.692211
24.312461	1183.466144	15.697229
24.048472	1194.130209	15.702247
24.136939	1193.494587	15.707264
24.406754	1186.796473	15.712282
23.946217	1193.536994	15.717299
24.230305	1201.883970	15.722317
24.391291	1205.573192	15.727335
24.531172	1214.504519	15.732352
24.789409	1208.313155	15.737370
24.580733	1213.269009	15.742387
24.892840	1212.803478	15.747405
24.839298	1213.269424	15.752423
24.991770	1212.406015	15.757440
24.909520	1212.166380	15.762458
24.741239	1212.615588	15.767475
25.159316	1202.997121	15.772493
25.034692	1211.647987	15.777511
24.805371	1212.163565	15.782528
24.991949	1200.997108	15.787546
24.835721	1218.580973	15.792563
24.884203	1207.313068	15.797581
24.956642	1212.022898	15.802599
24.953921	1212.345177	15.807616
25.032862	1210.890512	15.812634
24.789739	1219.992307	15.817651
25.293194	1210.136390	15.822669
25.120633	1204.400702	15.827687
25.117916	1213.903497	15.832704
25.143390	1206.129627	15.837722
25.184913	1211.131487	15.842739
25.021614	1207.600323	15.847757
25.182796	1215.385876	15.852775
24.699305	1213.113590	15.857792
25.011637	1212.625933	15.862810
24.931465	1222.118777	15.867827
25.354322	1220.461899	15.872845
25.110568	1222.065369	15.877863
25.261238	1241.687224	15.882880
25.587216	1240.834500	15.887898
25.451571	1246.312267	15.892915
25.630325	1237.330902	15.897933
25.457191	1243.212187	15.902951
25.653214	1239.438518	15.907968
25.853936	1236.737122	15.912986
25.302178	1237.230635	15.918003
25.946785	1228.416132	15.923021
25.643119	1219.494582	15.928039
25.251797	1221.136953	15.933056
25.414787	1222.528367	15.938074
25.455478	1234.536472	15.943091
25.491051	1238.617747	15.948109
25.468493	1237.160048	15.953127
25.386616	1235.746357	15.958144
25.759734	1237.199526	15.963162
25.919332	1233.624076	15.968179
25.557514	1230.745725	15.973197
25.655811	1239.083957	15.978215
25.426149	1239.640616	15.983232
25.805192	1238.003224	15.988250
25.742421	1242.396565	15.993267
25.921471	1259.748052	15.998285
25.797012	1257.810838	16.003303
25.996983	1258.536876	16.008320
26.507112	1246.237218	16.013338
26.233526	1261.557792	16.018355
26.339077	1247.055580	16.023373
25.925642	1238.002892	16.028391
25.864157	1240.893819	16.033408
25.833730	1245.130609	16.038426
25.848428	1255.063057	16.043443
25.902620	1254.170862	16.048461
26.307405	1251.055626	16.053479
26.269107	1251.162567	16.058496
26.295690	1257.195607	16.063514
26.231970	1260.067952	16.068531
26.183966	1255.653993	16.073549
26.394376	1253.452867	16.078567
25.927371	1254.100364	16.083584
26.296445	1248.257707	16.088602
26.257864	1252.776652	16.093619
26.461628	1247.625792	16.098637
26.394755	1255.093633	16.103655
26.622090	1263.702003	16.108672
26.845307	1257.894819	16.113690
26.372746	1250.849079	16.118707
26.397579	1245.211843	16.123725
26.697389	1254.389540	16.128743
26.687079	1267.753231	16.133760
26.570824	1259.663861	16.138778
26.503876	1277.539919	16.143795
26.443203	1275.813624	16.148813
26.921821	1279.314234	16.153831
26.628352	1282.475053	16.158848
26.953956	1273.186628	16.163866
27.081385	1287.794275	16.168883
26.692505	1284.118552	16.173901
26.954827	1272.327935	16.178919
26.941224	1285.013634	16.183936
27.113513	1277.213574	16.188954
26.940632	1265.061945	16.193971
26.641766	1264.701610	16.198989
26.896164	1267.902822	16.204007
26.977110	1282.953264	16.209024
26.834644	1275.145714	16.214042
27.016793	1278.181517	16.219059
26.652737	1275.716934	16.224077
27.399403	1271.137435	16.229095
26.872373	1268.748882	16.234112
27.387880	1273.048468	16.239130
27.321754	1273.039844	16.244147
26.952985	1275.297245	16.249165
27.565643	1268.851508	16.254183
27.201674	1273.901139	16.259200
27.365722	1268.907980	16.264218
27.406769	1275.289066	16.269235
27.050735	1276.222145	16.274253
27.422801	1273.373972	16.279271
27.114388	1273.728369	16.284288
27.622550	1270.710545	16.289306
27.342259	1271.445557	16.294323
27.204114	1265.682366	16.299341
27.591512	1266.574703	16.304359
27.076070	1276.265168	16.309376
27.444512	1286.435708	16.314394
27.661328	1294.714370	16.319411
27.694284	1295.696959	16.324429
27.871000	1292.077789	16.329447
27.587369	1280.688298	16.334464
27.888513	1284.851055	16.339482
27.718903	1287.099345	16.344499
27.541757	1281.339103	16.349517
27.490674	1281.160858	16.354535
28.096249	1296.791854	16.359552
27.807974	1289.774031	16.364570
27.922846	1285.265116	16.369587
27.665206	1296.041860	16.374605
28.078428	1294.863027	16.379623
27.912690	1290.861997	16.384640
27.852687	1282.239921	16.389658
27.863110	1293.883566	16.394675
28.048557	1297.805669	16.399693
28.076033	1286.241193	16.404711
27.951082	1292.124413	16.409728
28.046691	1295.584047	16.414746
28.305965	1287.113922	16.419763
28.104350	1291.188190	16.424781
28.245468	1292.737677	16.429799
28.318499	1293.275314	16.434816
27.828736	1291.136548	16.439834
28.541057	1290.295875	16.444851
28.084229	1295.795578	16.449869
28.353890	1287.279643	16.454887
27.967793	1297.691493	16.459904
28.402871	1291.052656	16.464922
28.549183	1290.976032	16.469939
28.031599	1291.483127	16.474957
28.389883	1286.500557	16.479975
28.010817	1307.638270	16.484992
28.344435	1311.600278	16.490010
28.214423	1321.621711	16.495027
28.173743	1323.714099	16.500045
28.265242	1316.589424	16.505063
28.508975	1316.980391	16.510080
28.354463	1318.733995	16.515098
28.276976	1318.367376	16.520115
28.268457	1322.379837	16.525133
28.490247	1333.321336	16.530151
28.348778	1343.177312	16.535168
28.607369	1351.247475	16.540186
28.566644	1335.906542	16.545203
28.733921	1344.117247	16.550221
28.897457	1345.278202	16.555239
28.909712	1348.343793	16.560256
28.712610	1339.544347	16.565274
28.801406	1339.962746	16.570291
28.906337	1338.882709	16.575309
28.956048	1336.485837	16.580327
28.734229	1342.501019	16.585344
29.187797	1358.717640	16.590362
29.453532	1355.920830	16.595379
29.095822	1338.190029	16.600397
29.325769	1339.230122	16.605415
29.159112	1341.765144	16.610432
29.106038	1329.326447	16.615450
29.234041	1335.952716	16.620467
29.206517	1336.733337	16.625485
29.656876	1353.385974	16.630503
29.446321	1340.934072	16.635520
29.177360	1335.885657	16.640538
29.389611	1330.862837	16.645555
28.991340	1341.472287	16.650573
29.822040	1348.127322	16.655591
29.581193	1353.520616	16.660608
29.142565	1356.590578	16.665626
29.815860	1355.175326	16.670643
29.692992	1362.232247	16.675661
29.916760	1351.697366	16.680679
29.440771	1343.800027	16.685696
29.706346	1337.048871	16.690714
29.957268	1330.972225	16.695731
29.484333	1331.068367	16.700749
29.663842	1322.080528	16.705767
29.421899	1348.258903	16.710784
29.675690	1355.032735	16.715802
29.720215	1352.750286	16.720819
29.794604	1359.760520	16.725837
29.787479	1356.924408	16.730855
29.737983	1359.980740	16.735872
29.660330	1363.151941	16.740890
29.950818	1352.518240	16.745907
29.963576	1360.775254	16.750925
30.107588	1349.059930	16.755943
29.832263	1354.815247	16.760960
30.033820	1357.077976	16.765978
29.866492	1354.330084	16.770995
29.629429	1354.506038	16.776013
29.888536	1357.700217	16.781031
30.222703	1367.623701	16.786048
30.410750	1377.033575	16.791066
30.489523	1373.994646	16.796083
30.429769	1373.420112	16.801101
30.628466	1372.429527	16.806119
30.048365	1366.328435	16.811136
30.505846	1368.099769	16.816154
30.617620	1361.243309	16.821171
30.159385	1361.851564	16.826189
30.271976	1361.480410	16.831207
30.619973	1363.619206	16.836224
30.449960	1381.410526	16.841242
30.498676	1371.815125	16.846259
30.720806	1375.671535	16.851277
30.916236	1371.598118	16.856295
30.859005	1371.105243	16.861312
30.897603	1366.788146	16.866330
30.715849	1347.161457	16.871347
30.538604	1343.944887	16.876365
30.716602	1344.393493	16.881383
30.730094	1348.617114	16.886400
30.695438	1350.626508	16.891418
30.735497	1350.225691	16.896435
30.446293	1366.640752	16.901453
30.620625	1361.813221	16.906471
30.650252	1368.811536	16.911488
30.727817	1374.599933	16.916506
30.911317	1368.104632	16.921523
30.652053	1371.222236	16.926541
30.951753	1373.583204	16.931559
30.875983	1369.353456	16.936576
30.781926	1380.969345	16.941594
30.891075	1380.857516	16.946611
31.162142	1399.242491	16.951629
31.301951	1401.704257	16.956647
31.255443	1395.790960	16.961664
31.284485	1401.823664	16.966682
31.383099	1398.851053	16.971699
31.339706	1408.076290	16.976717
31.068523	1396.997213	16.981735
31.520631	1396.058445	16.986752
31.418539	1387.629113	16.991770
31.830794	1390.751963	16.996787
31.538731	1397.923774	17.001805
31.320185	1392.687556	17.006823
31.929602	1394.248888	17.011840
31.626843	1393.750299	17.016858
31.712803	1393.219208	17.021875
31.462927	1397.862817	17.026893
31.370226	1395.440911	17.031911
31.575606	1389.633323	17.036928
31.378741	1389.114986	17.041946
31.514150	1390.334003	17.046963
31.712806	1395.623732	17.051981
31.859320	1396.645341	17.056999
32.173037	1386.358289	17.062016
31.861168	1395.745511	17.067034
32.092119	1386.878974	17.072051
32.022123	1390.118411	17.077069
31.998949	1397.156570	17.082087
32.272685	1388.194962	17.087104
31.927582	1392.250707	17.092122
32.220954	1380.130093	17.097139
31.585575	1396.321699	17.102157
31.798451	1386.848898	17.107175
32.145229	1390.575323	17.112192
31.993852	1390.753632	17.117210
32.301501	1387.047653	17.122227
32.013806	1391.252200	17.127245
32.347528	1399.935489	17.132263
32.398112	1398.359015	17.137280
32.153005	1393.887538	17.142298
32.013084	1407.053882	17.147315
32.144613	1415.178699	17.152333
32.344369	1411.432813	17.157351
32.447771	1418.542670	17.162368
32.532544	1416.541097	17.167386
32.589049	1407.821807	17.172403
32.508494	1417.434741	17.177421
32.498249	1416.565257	17.182439
32.574111	1406.315462	17.187456
32.445505	1415.228993	17.192474
32.523932	1406.471554	17.197491
32.706800	1407.440128	17.202509
32.555193	1404.872809	17.207527
32.553289	1408.903189	17.212544
32.600585	1410.268562	17.217562
32.418499	1411.603600	17.222579
32.810271	1419.368893	17.227597
32.869977	1436.300575	17.232615
33.105893	1428.405269	17.237632
33.177518	1437.953343	17.242650
33.425396	1433.272066	17.247667
33.034489	1427.213896	17.252685
32.801937	1411.095033	17.257703
33.350854	1427.031679	17.262720
33.277984	1423.625164	17.267738
33.033459	1409.439614	17.272755
33.173528	1419.933203	17.277773
32.992739	1428.716056	17.282791
33.415581	1429.262008	17.287808
33.094776	1440.490566	17.292826
33.502703	1433.044855	17.297843
33.486329	1422.635925	17.302861
33.461493	1431.930854	17.307879
33.433331	1426.292396	17.312896
33.630011	1440.453797	17.317914
33.053622	1435.030627	17.322931
33.299168	1440.142602	17.327949
33.214298	1434.664511	17.332967
33.437642	1418.149150	17.337984
33.334753	1432.682544	17.343002
33.345346	1429.455463	17.348019
33.419016	1436.838241	17.353037
33.279076	1442.988957	17.358055
33.698122	1443.223066	17.363072
33.818271	1452.526849	17.368090
33.841946	1450.916715	17.373107
33.882959	1453.097309	17.378125
33.971065	1451.054183	17.383143
33.976789	1446.881078	17.388160
34.022300	1452.030711	17.393178
33.915066	1447.259896	17.398195
34.440244	1447.430037	17.403213
33.768376	1450.252524	17.408231
34.197236	1445.817454	17.413248
33.984239	1447.854801	17.418266
34.360205	1445.782353	17.423283
34.133784	1448.595010	17.428301
34.276307	1447.130363	17.433319
34.283430	1442.723501	17.438336
34.233957	1446.373162	17.443354
34.238336	1448.736228	17.448371
34.268227	1438.970164	17.453389
34.245289	1452.373843	17.458407
34.747885	1444.285261	17.463424
34.566536	1440.081507	17.468442
34.486046	1441.441656	17.473459
34.721546	1445.920863	17.478477
34.425753	1444.944633	17.483495
34.622313	1438.406232	17.488512
34.137182	1448.552807	17.493530
34.228260	1443.132357	17.498547
34.236560	1439.362812	17.503565
34.426488	1442.883440	17.508583
34.429792	1455.304667	17.513600
34.674366	1459.798236	17.518618
34.816244	1459.195262	17.523635
35.173672	1458.728938	17.528653
35.217317	1463.979857	17.533671
35.223294	1452.248221	17.538688
34.898455	1465.342591	17.543706
34.955026	1462.903599	17.548723
34.879617	1453.674756	17.553741
34.983816	1465.177583	17.558759
35.024968	1461.308207	17.563776
34.461848	1463.529807	17.568794
34.803294	1475.793923	17.573811
34.964489	1463.697118	17.578829
34.704242	1464.283823	17.583847
34.731455	1446.621998	17.588864
34.690061	1464.885576	17.593882
35.004076	1474.954294	17.598899
35.001268	1492.760554	17.603917
34.690637	1486.200614	17.608935
35.392526	1479.993297	17.613952
35.119922	1483.709484	17.618970
35.229509	1501.103649	17.623987
35.582205	1507.966189	17.629005
35.392694	1515.383923	17.634023
35.763409	1513.987665	17.639040
35.751294	1504.250238	17.644058
35.836812	1512.300253	17.649075
36.167110	1504.339631	17.654093
36.101173	1505.441872	17.659111
36.014344	1495.545735	17.664128
35.884053	1471.710274	17.669146
35.799548	1479.603868	17.674163
35.699611	1472.417602	17.679181
35.779235	1476.656140	17.684199
36.161257	1488.762421	17.689216
36.025143	1494.950427	17.694234
35.785532	1494.435629	17.699251
36.361207	1489.999637	17.704269
36.145582	1497.074300	17.709287
36.392654	1497.644638	17.714304
36.255299	1485.585128	17.719322
36.141099	1483.204449	17.724339
35.984954	1483.080535	17.729357
36.355498	1490.792379	17.734375
36.340872	1486.931737	17.739392
36.349844	1499.983298	17.744410
35.996641	1502.699057	17.749427
36.098478	1497.131731	17.754445
36.115800	1503.100030	17.759463
36.179598	1494.755114	17.764480
36.561214	1489.939254	17.769498
36.415044	1492.944480	17.774515
36.947975	1495.145840	17.779533
36.538724	1492.423207	17.784551
36.715269	1494.292223	17.789568
36.352067	1490.508287	17.794586
36.525992	1490.777647	17.799603
36.766365	1497.054995	17.804621
36.844889	1525.506199	17.809639
36.685194	1514.744112	17.814656
36.745898	1511.947843	17.819674
36.897492	1519.056501	17.824691
37.081080	1513.252288	17.829709
36.897953	1514.735827	17.834727
37.138241	1516.910454	17.839744
37.169270	1508.712683	17.844762
36.902668	1519.011260	17.849779
36.992086	1516.059005	17.854797
36.951283	1521.597740	17.859815
37.091094	1516.586218	17.864832
36.889071	1513.550233	17.869850
37.181252	1514.299705	17.874867
37.167910	1513.638995	17.879885
37.106655	1514.566927	17.884903
37.525290	1512.004925	17.889920
37.338867	1512.387551	17.894938
36.927695	1523.977476	17.899955
37.532790	1520.969672	17.904973
37.250953	1532.675044	17.909991
37.346218	1540.464755	17.915008
37.538677	1530.168217	17.920026
37.212336	1546.043280	17.925043
37.513670	1533.189132	17.930061
37.619508	1543.767056	17.935079
37.472530	1539.198113	17.940096
37.890314	1532.785972	17.945114
37.854277	1542.041686	17.950131
37.928570	1535.146848	17.955149
37.975913	1540.267815	17.960167
37.953168	1531.702900	17.965184
37.923421	1525.174678	17.970202
37.791736	1538.314581	17.975219
38.044308	1533.446341	17.980237
38.037593	1534.491966	17.985255
37.753249	1532.617644	17.990272
38.063319	1548.023749	17.995290
38.005205	1562.969976	18.000307
38.639091	1559.657838	18.005325
38.605307	1559.492660	18.010343
38.521778	1550.473333	18.015360
38.442300	1544.464162	18.020378
38.276928	1550.183377	18.025395
38.516018	1544.073798	18.030413
38.293203	1540.520332	18.035431
38.417387	1549.239681	18.040448
38.548527	1551.955303	18.045466
38.436138	1549.154589	18.050483
38.621558	1548.450112	18.055501
38.730480	1550.298170	18.060519
38.826777	1554.530958	18.065536
38.972778	1549.963448	18.070554
38.653402	1554.895712	18.075571
38.840491	1554.699083	18.080589
38.911828	1555.426352	18.085607
38.675731	1542.321870	18.090624
39.000392	1548.636526	18.095642
38.978781	1551.906283	18.100659
38.738070	1551.663068	18.105677
38.970678	1552.106280	18.110695
38.970160	1550.373688	18.115712
39.147974	1546.931029	18.120730
38.782118	1556.992701	18.125747
38.805979	1541.549949	18.130765
38.977624	1548.093717	18.135783
38.951201	1557.783455	18.140800
39.277526	1568.462555	18.145818
39.072596	1571.022542	18.150835
39.350782	1570.278282	18.155853
39.369773	1575.047077	18.160871
39.070280	1580.386508	18.165888
39.239149	1568.121164	18.170906
38.943256	1568.186411	18.175923
39.767457	1566.132087	18.180941
39.670660	1568.047095	18.185959
39.535583	1567.882007	18.190976
39.827261	1576.054392	18.195994
39.867459	1572.387124	18.201011
39.667121	1568.113727	18.206029
39.629890	1563.944170	18.211047
39.594402	1569.324288	18.216064
40.117398	1568.759433	18.221082
39.539265	1584.307889	18.226099
40.065345	1584.200165	18.231117
40.295481	1594.291561	18.236135
40.167965	1585.414815	18.241152
40.200741	1572.870975	18.246170
39.908683	1573.595217	18.251187
40.140111	1563.579747	18.256205
39.966851	1576.309603	18.261223
40.088724	1588.800714	18.266240
40.330286	1591.211848	18.271258
40.321937	1592.320852	18.276275
40.398375	1597.165863	18.281293
40.498167	1596.118176	18.286311
40.177491	1596.379820	18.291328
40.324417	1593.383827	18.296346
39.989934	1606.729132	18.301363
39.986662	1600.247231	18.306381
40.204888	1593.127837	18.311399
40.052230	1595.641766	18.316416
39.819671	1607.083832	18.321434
40.245967	1622.550690	18.326451
40.245672	1614.603945	18.331469
40.613044	1625.469162	18.336487
40.406164	1618.889760	18.341504
41.072878	1627.726126	18.346522
41.062233	1634.708763	18.351539
41.277037	1630.162012	18.356557
41.209217	1621.563089	18.361575
41.122903	1627.086895	18.366592
41.360524	1616.013173	18.371610
40.764414	1613.228275	18.376627
40.893756	1613.987485	18.381645
40.925450	1623.908008	18.386663
41.145352	1625.407308	18.391680
41.646370	1632.691650	18.396698
41.502811	1638.375916	18.401715
41.586601	1633.003890	18.406733
41.399502	1624.044936	18.411751
41.127989	1619.792147	18.416768
41.384944	1624.545763	18.421786
41.275642	1624.543903	18.426803
41.100123	1625.120493	18.431821
41.164549	1634.117504	18.436839
41.099736	1629.333682	18.441856
41.438220	1630.451466	18.446874
41.505588	1635.913324	18.451891
41.878312	1651.252894	18.456909
41.995548	1652.932393	18.461927
41.883723	1652.845717	18.466944
41.842155	1652.861648	18.471962
41.745644	1658.049372	18.476979
42.553282	1657.089603	18.481997
42.119108	1640.932691	18.487015
41.923373	1634.499868	18.492032
42.002282	1629.702995	18.497050
42.048768	1643.165372	18.502067
42.000187	1645.880764	18.507085
42.186633	1648.685571	18.512103
42.137739	1651.814446	18.517120
42.500813	1658.034755	18.522138
42.559511	1660.749120	18.527155
42.273214	1652.724085	18.532173
42.326018	1648.205868	18.537191
42.261739	1651.330841	18.542208
42.192302	1646.607703	18.547226
41.890425	1649.227074	18.552243
42.137365	1654.566123	18.557261
42.390774	1648.034520	18.562279
42.341698	1653.236902	18.567296
42.922340	1660.915902	18.572314
42.457593	1676.841169	18.577331
42.677834	1672.962624	18.582349
42.684546	1670.660812	18.587367
42.375484	1687.650510	18.592384
42.977299	1671.577419	18.597402
43.044128	1668.073226	18.602419
43.014741	1670.227005	18.607437
43.449082	1667.268023	18.612455
42.946628	1673.762811	18.617472
43.155244	1667.705305	18.622490
42.947449	1681.330634	18.627507
42.411479	1671.088181	18.632525
42.860358	1671.106168	18.637543
43.159755	1686.719204	18.642560
43.251736	1695.954940	18.647578
43.128824	1693.465138	18.652595
43.707723	1696.943809	18.657613
43.923000	1694.448360	18.662631
43.342843	1690.086112	18.667648
43.473422	1689.229267	18.672666
43.387581	1687.393259	18.677683
43.139846	1696.057336	18.682701
43.695763	1686.944064	18.687719
43.629906	1702.412358	18.692736
43.293905	1695.061006	18.697754
43.498416	1697.856679	18.702771
43.622970	1695.157681	18.707789
43.912016	1687.238157	18.712807
43.691319	1698.242897	18.717824
44.039258	1693.706830	18.722842
43.782117	1708.359295	18.727859
43.749114	1716.888746	18.732877
44.302508	1714.106775	18.737895
44.430387	1727.840502	18.742912
44.305429	1726.878517	18.747930
44.435597	1723.638961	18.752947
44.305304	1723.728757	18.757965
44.369916	1718.463858	18.762983
44.542846	1730.568349	18.768000
44.191366	1714.849721	18.773018
44.095741	1727.239298	18.778035
44.346055	1721.134212	18.783053
44.516987	1717.361219	18.788071
44.538686	1721.627826	18.793088
44.863131	1723.053947	18.798106
44.982160	1719.440574	18.803123
44.553636	1721.035165	18.808141
44.751009	1721.654326	18.813159
44.647106	1706.575453	18.818176
44.805519	1711.385559	18.823194
45.273881	1716.472172	18.828211
45.078763	1718.200617	18.833229
45.094063	1714.966435	18.838247
44.668962	1718.905391	18.843264
44.784140	1714.872875	18.848282
45.203399	1710.884241	18.853299
44.843441	1720.667353	18.858317
44.871098	1717.292371	18.863335
44.922980	1719.537571	18.868352
44.984409	1736.024272	18.873370
45.380902	1742.308807	18.878387
45.121514	1739.010355	18.883405
45.733180	1735.521776	18.888423
45.458556	1732.778011	18.893440
45.375000	1731.285644	18.898458
45.606938	1730.305613	18.903475
45.640049	1739.105600	18.908493
45.328845	1736.859901	18.913511
45.327355	1742.414636	18.918528
45.485722	1733.641357	18.923546
45.899597	1742.561579	18.928563
45.550441	1744.415153	18.933581
45.662226	1733.279019	18.938599
45.764774	1738.479761	18.943616
45.756199	1739.825509	18.948634
45.775854	1748.823280	18.953651
45.811266	1770.328968	18.958669
46.150904	1763.171549	18.963687
46.170028	1769.811883	18.968704
46.149310	1770.439968	18.973722
45.882701	1755.724238	18.978739
45.989364	1762.524434	18.983757
46.173008	1772.440167	18.988775
46.299804	1753.294896	18.993792
46.230191	1760.031186	18.998810
46.251678	1756.818119	19.003827
45.967479	1755.483427	19.008845
46.346837	1765.052892	19.013863
46.141606	1784.440753	19.018880
46.232998	1784.814573	19.023898
46.444677	1773.066279	19.028915
46.094190	1779.502578	19.033933
46.452454	1787.664628	19.038951
46.275435	1799.139142	19.043968
46.577600	1800.253159	19.048986
47.338163	1804.795367	19.054003
46.986284	1808.028548	19.059021
46.933909	1802.942910	19.064039
46.770304	1804.899970	19.069056
47.135760	1791.628467	19.074074
47.109951	1800.087398	19.079091
46.878415	1806.476666	19.084109
47.032774	1795.248611	19.089127
47.417507	1792.578267	19.094144
47.387218	1793.327780	19.099162
47.812509	1783.483797	19.104179
47.349646	1793.693352	19.109197
47.316372	1795.712047	19.114215
47.480839	1788.417951	19.119232
47.507095	1796.395323	19.124250
47.777434	1801.112173	19.129267
47.428095	1796.057285	19.134285
47.551042	1791.878358	19.139303
47.599266	1802.295039	19.144320
47.629414	1811.890839	19.149338
47.781520	1805.599127	19.154355
47.928716	1821.734776	19.159373
47.950452	1818.663680	19.164391
47.757463	1819.334538	19.169408
47.926674	1817.941425	19.174426
48.093607	1809.564423	19.179443
47.556525	1817.759464	19.184461
47.871178	1826.597438	19.189479
48.198968	1808.948126	19.194496
47.825534	1817.461531	19.199514
48.273039	1824.527104	19.204531
48.236320	1836.427813	19.209549
48.302681	1837.496723	19.214567
48.631747	1836.959090	19.219584
48.638738	1846.495416	19.224602
49.005933	1839.156913	19.229619
48.480277	1846.292912	19.234637
48.739942	1839.662423	19.239655
48.617750	1841.281617	19.244672
48.490394	1844.040941	19.249690
48.606420	1842.804491	19.254707
48.354977	1841.773949	19.259725
48.505144	1840.857220	19.264743
48.784977	1835.776331	19.269760
48.655400	1844.687072	19.274778
48.785592	1837.559283	19.279795
48.910029	1846.001008	19.284813
48.938156	1852.800918	19.289831
49.303725	1852.775152	19.294848
48.864090	1865.461736	19.299866
48.998598	1856.326037	19.304883
48.886224	1857.972098	19.309901
49.056986	1859.248729	19.314919
49.343166	1859.642527	19.319936
49.262866	1858.686162	19.324954
49.170938	1858.334418	19.329971
49.114211	1857.677337	19.334989
49.617211	1873.864591	19.340007
49.753403	1879.956413	19.345024
49.688489	1873.446198	19.350042
49.959974	1882.287807	19.355059
49.954003	1885.264821	19.360077
49.715537	1875.799358	19.365095
50.085127	1876.924909	19.370112
49.666726	1884.325004	19.375130
50.165996	1875.703384	19.380147
50.327295	1870.691553	19.385165
50.046298	1878.969583	19.390183
50.435508	1872.697507	19.395200
50.213848	1876.850792	19.400218
50.495525	1874.714169	19.405235
50.299134	1883.038910	19.410253
49.843020	1885.079680	19.415271
50.335204	1875.032650	19.420288
50.201760	1869.874482	19.425306
50.207401	1872.707653	19.430323
50.232833	1867.587713	19.435341
50.468415	1880.064367	19.440359
50.555203	1877.039877	19.445376
50.281839	1891.209006	19.450394
50.620738	1896.016133	19.455411
50.729558	1890.602236	19.460429
50.365741	1897.182686	19.465447
51.065816	1893.863275	19.470464
50.649676	1894.812112	19.475482
51.039493	1882.843318	19.480499
50.848004	1894.184451	19.485517
50.604868	1903.248722	19.490535
50.767112	1898.056842	19.495552
50.785980	1910.980911	19.500570
50.919713	1917.716960	19.505587
51.009809	1923.036480	19.510605
51.081780	1925.925543	19.515623
51.739492	1914.372379	19.520640
51.467399	1921.295099	19.525658
51.732003	1914.196716	19.530675
51.792912	1921.685843	19.535693
51.461866	1917.429684	19.540711
51.428712	1918.353233	19.545728
51.280400	1923.482873	19.550746
51.742742	1917.133047	19.555763
51.890214	1918.833082	19.560781
51.701965	1913.008099	19.565799
52.016072	1924.446772	19.570816
51.724317	1936.712578	19.575834
52.251643	1930.333629	19.580851
52.287733	1941.938958	19.585869
51.670904	1923.247712	19.590887
52.248566	1924.763573	19.595904
51.977161	1938.642078	19.600922
52.143112	1942.280179	19.605939
52.250851	1942.664065	19.610957
52.109853	1951.115867	19.615975
52.047085	1934.969930	19.620992
52.131992	1939.343459	19.626010
52.251379	1930.320552	19.631027
52.051759	1940.612031	19.636045
52.320969	1948.027504	19.641063
52.686812	1959.647456	19.646080
52.580853	1964.486428	19.651098
52.928978	1960.467856	19.656115
52.943925	1959.007377	19.661133
52.591412	1962.205968	19.666151
52.621794	1961.077610	19.671168
52.902315	1961.260844	19.676186
53.074113	1956.626068	19.681203
52.424441	1951.040637	19.686221
52.944941	1956.608335	19.691239
52.976775	1955.782730	19.696256
52.963853	1977.788581	19.701274
53.292526	1986.387735	19.706291
53.374183	1988.072841	19.711309
53.334150	1991.424465	19.716327
53.428635	1976.642510	19.721344
53.103260	1991.814018	19.726362
53.534982	1974.905708	19.731379
53.499987	1981.005449	19.736397
53.652236	1984.266981	19.741415
53.694948	1981.132606	19.746432
53.843279	1980.048888	19.751450
53.936506	1992.787783	19.756467
53.901939	1983.713226	19.761485
53.544336	1984.905379	19.766503
53.768380	1988.408146	19.771520
53.790580	1992.958783	19.776538
53.944100	1995.816145	19.781555
54.056519	2006.074551	19.786573
54.272699	2009.064120	19.791591
54.418796	2004.969886	19.796608
54.529109	2006.618943	19.801626
54.326515	2003.832290	19.806643
54.795518	2003.837659	19.811661
54.411634	2003.519031	19.816679
54.526968	2000.467955	19.821696
54.619188	2008.169979	19.826714
54.579812	1999.948298	19.831731
54.594166	2005.232369	19.836749
54.679592	2010.278071	19.841767
54.555897	2004.853229	19.846784
54.619956	1998.562621	19.851802
54.510476	1993.558465	19.856819
54.906712	1998.899475	19.861837
54.638401	2005.941563	19.866855
54.838224	2010.016217	19.871872
55.157807	2026.115573	19.876890
55.222756	2028.945789	19.881907
55.318833	2023.164591	19.886925
55.002695	2023.703261	19.891943
55.054002	2025.819191	19.896960
55.639696	2026.680502	19.901978
55.418410	2025.799870	19.906995
54.991493	2023.278752	19.912013
55.072665	2019.308305	19.917031
55.456955	2019.907659	19.922048
55.319211	2023.129420	19.927066
55.198687	2046.622932	19.932083
55.728472	2049.238299	19.937101
55.793946	2049.095437	19.942119
56.042847	2043.069365	19.947136
55.932633	2050.430710	19.952154
55.957540	2053.200926	19.957171
56.044008	2056.163485	19.962189
56.028704	2057.289387	19.967207
56.471868	2052.558417	19.972224
56.154705	2051.083688	19.977242
56.009109	2050.560454	19.982259
56.081023	2042.024648	19.987277
56.159269	2046.260381	19.992295
56.266855	2051.867555	19.997312
56.011751	2048.950257	20.002330
56.186311	2046.063477	20.007347
56.587918	2057.980870	20.012365
56.309269	2070.093223	20.017383
56.438452	2063.924942	20.022400
56.462791	2074.029917	20.027418
56.630315	2078.803979	20.032435
56.733077	2075.682272	20.037453
56.331431	2079.462984	20.042471
56.388123	2073.801558	20.047488
56.504476	2077.693630	20.052506
56.509837	2103.954290	20.057523
57.080261	2105.016829	20.062541
56.927453	2094.979207	20.067559
57.172310	2095.546757	20.072576
57.352683	2094.928264	20.077594
57.130065	2104.399708	20.082611
57.417529	2107.166669	20.087629
57.717120	2115.385402	20.092647
57.407363	2113.625462	20.097664
57.644279	2115.115826	20.102682
57.657043	2112.895066	20.107699
57.952916	2113.590335	20.112717
57.759829	2106.528870	20.117735
58.053135	2109.367505	20.122752
57.986474	2111.902748	20.127770
57.882748	2111.413980	20.132787
57.905474	2110.425679	20.137805
57.812079	2115.351094	20.142823
57.960124	2105.228456	20.147840
58.223647	2104.798923	20.152858
57.789649	2111.513534	20.157875
57.920015	2106.399178	20.162893
57.833853	2118.017463	20.167911
58.002531	2127.752686	20.172928
58.163118	2133.152750	20.177946
58.284524	2139.335347	20.182963
58.463548	2132.013582	20.187981
58.329544	2134.376328	20.192999
58.313197	2138.440695	20.198016
58.492774	2140.271433	20.203034
58.441927	2153.923026	20.208051
58.897722	2154.290257	20.213069
59.068579	2156.677831	20.218087
59.175182	2158.699899	20.223104
59.503009	2154.693933	20.228122
58.899950	2160.560819	20.233139
59.247647	2140.963924	20.238157
59.297301	2150.023474	20.243175
59.498674	2150.578902	20.248192
59.341799	2151.023188	20.253210
59.227912	2146.493090	20.258227
59.311315	2155.162314	20.263245
58.877013	2147.946107	20.268263
59.675374	2156.497002	20.273280
59.651743	2149.696172	20.278298
59.570939	2150.810251	20.283315
59.722258	2147.393721	20.288333
59.581772	2155.665643	20.293351
59.978388	2149.796288	20.298368
59.928351	2143.018535	20.303386
59.640447	2152.260372	20.308403
59.790288	2148.806201	20.313421
59.909410	2157.848559	20.318439
59.979952	2178.348758	20.323456
60.105998	2168.841810	20.328474
59.759049	2167.510605	20.333491
60.319072	2170.159125	20.338509
60.423397	2174.387646	20.343527
60.127530	2168.989730	20.348544
60.454529	2180.107784	20.353562
60.320590	2181.911901	20.358579
60.817580	2173.631353	20.363597
60.496532	2177.775030	20.368615
60.421513	2177.360664	20.373632
60.582075	2181.533035	20.378650
60.608578	2190.731944	20.383667
61.029628	2196.267958	20.388685
60.657525	2194.375754	20.393703
60.928214	2189.454003	20.398720
60.788553	2187.739994	20.403738
60.357848	2193.198002	20.408755
60.817257	2211.992998	20.413773
61.020786	2226.409592	20.418791
60.678316	2225.093461	20.423808
61.027632	2217.653455	20.428826
61.405541	2225.266625	20.433843
61.307398	2225.149397	20.438861
61.750835	2226.951427	20.443879
61.647617	2243.183500	20.448896
61.925330	2238.535214	20.453914
61.753437	2241.440444	20.458931
61.862876	2231.380593	20.463949
62.125478	2240.072280	20.468967
61.628873	2237.549425	20.473984
61.820608	2226.397303	20.479002
61.654493	2238.905584	20.484019
61.739454	2238.690234	20.489037
61.558437	2241.464338	20.494055
61.962437	2247.978269	20.499072
62.424283	2251.434362	20.504090
62.052001	2263.359524	20.509107
62.477359	2254.730368	20.514125
62.367054	2261.624713	20.519143
62.313752	2268.642685	20.524160
62.590860	2257.085814	20.529178
62.562390	2270.008090	20.534195
62.912860	2256.419828	20.539213
62.717277	2260.752168	20.544231
62.728287	2256.054137	20.549248
62.761060	2262.329564	20.554266
62.776197	2276.734686	20.559283
63.057975	2274.219271	20.564301
63.249629	2283.748990	20.569319
63.145586	2288.805519	20.574336
63.381178	2280.562721	20.579354
63.187234	2286.958893	20.584371
63.413745	2280.207194	20.589389
63.513314	2275.785643	20.594407
63.595065	2278.357622	20.599424
63.609320	2274.224019	20.604442
63.464788	2280.751315	20.609459
63.620313	2279.186726	20.614477
63.425502	2282.401694	20.619495
63.217717	2287.840584	20.624512
63.537602	2288.191239	20.629530
63.717661	2295.693414	20.634547
63.759859	2309.835523	20.639565
63.837585	2305.284831	20.644583
64.030734	2303.490263	20.649600
64.000664	2296.103354	20.654618
64.194265	2306.658510	20.659635
64.176311	2308.592804	20.664653
64.297417	2289.949672	20.669671
64.026688	2304.579502	20.674688
64.269450	2294.823806	20.679706
64.450955	2313.113290	20.684723
64.639967	2327.289220	20.689741
64.864378	2333.932316	20.694759
64.585210	2328.676915	20.699776
65.051685	2323.743388	20.704794
64.809743	2324.185226	20.709811
65.062338	2320.411938	20.714829
65.000257	2316.347094	20.719847
64.892750	2327.687966	20.724864
65.046873	2322.090100	20.729882
64.973208	2319.179046	20.734899
65.129483	2322.102307	20.739917
65.310121	2320.754707	20.744935
65.210711	2324.024169	20.749952
65.307152	2314.316636	20.754970
65.360235	2339.604398	20.759987
65.480849	2341.182438	20.765005
65.473397	2345.624190	20.770023
65.044263	2359.461453	20.775040
65.410567	2344.349402	20.780058
65.278854	2345.966976	20.785075
65.722252	2361.971490	20.790093
65.681105	2365.837803	20.795111
65.693289	2379.309263	20.800128
65.959135	2369.767680	20.805146
66.076616	2370.131113	20.810163
65.490233	2370.175595	20.815181
66.059033	2375.824229	20.820199
66.909657	2393.614446	20.825216
66.514451	2380.411191	20.830234
66.761855	2385.100229	20.835251
66.693828	2395.276666	20.840269
66.866354	2390.067253	20.845287
66.542542	2391.594997	20.850304
66.534891	2389.595173	20.855322
66.551138	2384.467057	20.860339
66.437856	2390.045820	20.865357
66.696320	2381.591090	20.870375
66.745144	2385.474872	20.875392
66.878554	2400.574843	20.880410
67.145170	2406.595912	20.885427
67.108841	2411.938541	20.890445
67.401703	2407.357273	20.895463
67.260176	2414.922508	20.900480
67.344399	2415.335338	20.905498
67.693054	2410.309784	20.910515
67.500939	2409.405625	20.915533
67.870665	2398.787298	20.920551
67.654943	2405.770804	20.925568
67.785703	2405.440969	20.930586
67.601261	2404.579794	20.935603
67.309547	2401.753387	20.940621
67.608728	2400.993182	20.945639
67.676075	2422.333686	20.950656
67.780444	2438.451352	20.955674
67.891907	2426.487937	20.960691
67.764090	2428.859220	20.965709
68.210609	2429.016452	20.970727
68.204064	2434.209240	20.975744
68.622074	2424.700598	20.980762
68.551166	2431.661426	20.985779
68.518520	2435.195030	20.990797
68.692633	2431.516074	20.995815
68.743137	2441.658185	21.000832
68.896469	2446.412476	21.005850
68.690963	2438.519611	21.010867
68.511973	2442.783116	21.015885
68.919799	2446.162496	21.020903
69.115742	2450.761774	21.025920
69.106493	2452.170803	21.030938
69.212835	2450.879020	21.035955
69.119147	2449.110441	21.040973
69.038835	2440.254281	21.045991
68.998773	2446.437032	21.051008
68.819191	2449.747484	21.056026
69.088250	2466.489532	21.061043
69.308031	2470.646380	21.066061
69.784042	2463.334761	21.071079
69.589898	2467.982537	21.076096
69.846225	2475.993598	21.081114
69.648137	2467.581954	21.086131
69.685849	2475.097038	21.091149
69.701631	2469.189409	21.096167
69.626534	2485.382576	21.101184
69.893415	2487.676247	21.106202
70.249890	2494.592231	21.111219
70.071441	2484.091301	21.116237
70.126712	2483.205189	21.121255
70.641705	2488.770762	21.126272
70.430386	2495.277038	21.131290
70.345747	2489.303076	21.136307
70.628780	2488.362342	21.141325
70.432487	2497.091334	21.146343
70.561289	2504.740498	21.151360
70.803648	2513.760570	21.156378
71.018289	2513.881542	21.161395
70.806465	2512.421831	21.166413
70.758931	2507.470948	21.171431
70.781146	2506.653136	21.176448
71.402825	2505.747715	21.181466
71.481917	2504.242425	21.186483
71.146768	2508.549348	21.191501
71.316205	2512.303796	21.196519
71.414527	2528.977970	21.201536
71.771442	2530.317011	21.206554
71.500019	2529.002350	21.211571
71.401334	2536.586172	21.216589
72.003615	2533.228316	21.221607
71.914360	2535.416828	21.226624
71.733219	2527.090872	21.231642
71.873612	2523.316184	21.236659
71.801756	2529.178864	21.241677
71.782923	2524.962014	21.246695
71.694042	2525.121073	21.251712
72.014585	2531.663965	21.256730
72.249151	2537.677475	21.261747
72.044242	2543.330608	21.266765
72.551430	2542.288472	21.271783
72.170052	2548.641512	21.276800
72.424822	2544.170330	21.281818
72.717451	2547.340536	21.286835
72.697210	2553.848458	21.291853
72.409421	2552.346990	21.296871
72.461665	2561.791391	21.301888
72.629374	2576.056071	21.306906
72.836942	2573.871012	21.311923
72.818732	2579.094074	21.316941
73.077496	2580.745175	21.321959
73.576180	2570.213852	21.326976
73.166792	2576.369297	21.331994
73.423450	2576.887673	21.337011
73.342441	2574.337528	21.342029
73.475304	2567.458367	21.347047
73.487163	2574.955451	21.352064
73.418875	2594.840337	21.357082
73.753199	2590.072627	21.362099
73.688107	2601.214501	21.367117
74.097623	2596.536004	21.372135
73.754313	2599.203032	21.377152
73.750464	2604.988802	21.382170
73.930895	2602.148357	21.387187
73.867279	2609.054456	21.392205
73.927178	2599.128408	21.397223
74.090374	2616.865589	21.402240
74.112440	2615.492314	21.407258
74.391791	2613.374907	21.412275
74.314244	2623.991669	21.417293
74.351100	2621.038001	21.422311
74.164457	2617.084133	21.427328
74.069192	2645.397066	21.432346
74.345289	2643.804087	21.437363
74.423976	2640.973264	21.442381
74.655549	2656.613553	21.447399
74.729178	2670.523778	21.452416
74.815140	2673.448644	21.457434
75.214868	2663.983771	21.462451
75.297568	2665.952832	21.467469
75.476814	2665.912074	21.472487
75.598282	2668.361109	21.477504
75.765620	2664.992471	21.482522
75.626666	2659.490917	21.487539
75.639067	2671.034149	21.492557
75.727831	2663.013020	21.497575
75.709845	2670.139237	21.502592
75.675816	2678.360001	21.507610
75.923228	2678.570525	21.512627
76.169125	2687.580663	21.517645
76.261656	2684.207960	21.522663
76.026714	2681.520954	21.527680
76.061438	2684.542222	21.532698
76.489298	2681.230604	21.537715
75.930623	2685.642026	21.542733
76.061785	2680.243329	21.547751
76.426320	2685.169743	21.552768
76.875280	2700.577173	21.557786
77.115760	2699.905058	21.562803
76.896075	2709.237488	21.567821
77.106553	2700.171519	21.572839
77.294074	2706.028336	21.577856
76.734964	2702.539951	21.582874
76.842948	2699.041734	21.587891
76.940700	2707.030402	21.592909
77.138923	2696.612360	21.597927
77.492792	2701.714039	21.602944
77.227649	2703.425142	21.607962
77.386047	2696.137943	21.612979
77.063356	2709.494840	21.617997
77.369195	2716.611370	21.623015
77.504717	2729.000139	21.628032
77.349686	2727.862909	21.633050
78.078745	2726.195799	21.638067
77.935393	2723.289285	21.643085
77.867772	2721.532376	21.648103
77.687271	2719.395476	21.653120
77.743781	2732.920223	21.658138
78.069075	2742.807988	21.663155
78.189228	2748.744810	21.668173
78.332291	2743.700877	21.673191
78.538234	2752.045042	21.678208
78.595565	2757.303663	21.683226
78.639405	2744.656274	21.688243
78.805235	2755.638973	21.693261
78.575993	2756.934153	21.698279
78.633940	2750.060348	21.703296
78.502190	2760.710933	21.708314
78.832172	2767.852106	21.713331
78.619933	2775.539037	21.718349
78.824868	2779.060735	21.723367
78.827412	2770.134619	21.728384
79.100959	2786.907825	21.733402
79.118274	2795.250001	21.738419
78.974555	2795.853206	21.743437
79.347832	2801.261179	21.748455
79.463350	2798.086850	21.753472
79.295904	2800.189802	21.758490
79.288435	2801.030467	21.763507
79.670998	2809.028212	21.768525
79.724979	2815.429914	21.773543
79.871385	2815.886666	21.778560
79.694303	2824.221439	21.783578
80.082714	2836.343416	21.788595
80.380175	2841.201478	21.793613
80.267058	2839.379093	21.798631
80.696012	2837.746368	21.803648
80.229667	2841.935052	21.808666
80.561777	2836.274423	21.813683
80.638932	2837.581572	21.818701
80.113376	2838.143605	21.823719
80.548017	2851.640759	21.828736
80.856665	2857.424992	21.833754
80.844653	2856.451562	21.838771
81.127959	2858.629084	21.843789
81.439091	2856.453015	21.848807
81.225922	2854.453777	21.853824
81.462607	2850.480875	21.858842
81.324307	2847.510426	21.863859
81.645115	2851.206511	21.868877
81.320533	2854.864842	21.873895
81.656745	2856.822610	21.878912
81.726963	2873.927592	21.883930
81.613311	2879.159382	21.888947
81.928350	2874.943797	21.893965
82.103344	2872.091537	21.898983
82.194584	2877.931933	21.904000
82.358815	2887.415770	21.909018
82.128677	2875.960070	21.914035
82.080295	2882.961729	21.919053
82.299633	2874.569710	21.924071
82.501696	2872.940968	21.929088
82.358037	2881.968050	21.934106
82.346342	2883.781490	21.939123
82.521953	2895.299295	21.944141
82.192975	2904.967726	21.949159
82.264301	2904.681912	21.954176
82.393929	2911.125451	21.959194
82.867759	2915.296254	21.964211
82.829745	2932.765432	21.969229
83.229753	2934.104066	21.974247
83.452235	2934.602558	21.979264
83.357049	2932.183988	21.984282
83.153430	2931.171137	21.989299
83.382898	2933.729535	21.994317
83.511447	2932.926607	21.999335
83.665719	2924.923503	22.004352
83.448887	2936.657475	22.009370
83.706063	2948.566529	22.014387
83.811688	2952.144851	22.019405
83.925002	2962.574099	22.024423
83.845918	2949.538674	22.029440
84.005460	2957.501991	22.034458
84.259170	2951.976702	22.039475
84.286065	2951.208637	22.044493
83.853895	2959.703374	22.049511
84.325086	2967.235966	22.054528
84.175258	2971.712805	22.059546
84.510257	2971.189994	22.064563
84.405345	2976.679252	22.069581
84.508290	2989.038586	22.074599
85.148046	2995.247577	22.079616
85.124657	2999.925547	22.084634
85.218746	2992.165404	22.089651
84.978483	2998.600646	22.094669
84.958144	3005.515897	22.099687
85.084963	2995.777988	22.104704
85.334236	2999.343283	22.109722
85.480747	3002.804742	22.114739
85.795932	3011.990403	22.119757
85.874788	3027.427694	22.124775
86.137621	3029.311761	22.129792
85.550076	3028.990300	22.134810
85.843682	3023.619705	22.139827
86.372311	3023.590489	22.144845
85.771544	3022.778729	22.149863
86.147627	3018.755545	22.154880
86.231776	3031.941626	22.159898
86.093048	3031.316286	22.164915
86.104607	3027.018808	22.169933
86.434724	3054.864897	22.174951
86.430349	3041.180143	22.179968
86.363496	3043.652422	22.184986
86.525997	3049.121899	22.190003
86.388872	3050.633072	22.195021
86.522559	3075.041276	22.200039
86.778350	3069.850185	22.205056
86.971332	3072.714162	22.210074
87.024520	3079.422235	22.215091
87.442832	3079.012618	22.220109
87.295839	3092.137114	22.225127
87.413853	3094.239563	22.230144
87.483038	3092.256029	22.235162
87.489381	3099.031418	22.240179
88.011831	3088.710695	22.245197
87.825392	3090.093880	22.250215
88.134831	3094.318888	22.255232
88.225184	3095.955392	22.260250
88.072371	3100.625260	22.265267
88.266362	3094.206601	22.270285
88.060044	3093.879066	22.275303
88.188101	3099.410767	22.280320
88.311229	3109.027410	22.285338
88.160730	3113.772669	22.290355
88.458647	3114.966345	22.295373
88.227262	3120.096713	22.300391
88.338026	3112.759997	22.305408
88.745588	3129.581964	22.310426
88.951549	3138.980490	22.315443
88.991172	3139.261450	22.320461
88.584459	3142.351957	22.325479
89.276071	3140.425555	22.330496
88.947017	3139.107251	22.335514
89.298450	3142.928005	22.340531
89.421738	3150.303715	22.345549
89.520294	3157.124646	22.350567
89.548744	3159.872384	22.355584
89.822562	3160.959370	22.360602
89.897334	3161.695636	22.365619
90.076435	3154.278759	22.370637
89.549202	3151.729007	22.375655
89.335528	3154.142242	22.380672
89.324341	3169.470668	22.385690
89.858247	3175.153432	22.390707
90.178186	3168.645576	22.395725
90.484650	3186.951090	22.400743
90.709050	3196.031132	22.405760
90.508047	3197.678575	22.410778
90.473129	3202.756092	22.415795
90.782842	3209.436648	22.420813
90.882166	3201.470438	22.425831
90.798389	3201.234170	22.430848
91.121779	3199.157141	22.435866
91.425724	3215.023296	22.440883
91.623677	3218.855487	22.445901
91.204230	3224.529819	22.450919
91.488538	3220.672470	22.455936
91.560293	3217.826862	22.460954
91.523594	3221.762099	22.465971
91.466443	3204.613610	22.470989
91.373442	3218.764990	22.476007
91.849925	3221.950699	22.481024
91.796485	3231.579290	22.486042
91.613912	3244.248657	22.491059
92.199924	3241.707538	22.496077
92.010171	3246.077074	22.501095
92.061014	3238.882258	22.506112
92.053425	3258.774146	22.511130
92.069274	3266.845332	22.516147
92.610042	3261.382288	22.521165
92.796335	3257.969539	22.526183
92.674667	3263.616166	22.531200
92.914510	3270.456036	22.536218
93.075094	3281.054814	22.541235
93.151999	3284.154793	22.546253
93.241989	3292.934004	22.551271
93.167609	3293.996645	22.556288
93.791750	3289.811443	22.561306
93.457718	3282.828410	22.566323
93.654427	3278.678615	22.571341
93.460141	3283.134089	22.576359
93.507910	3286.576354	22.581376
93.844484	3308.589044	22.586394
93.710496	3318.779492	22.591411
94.276613	3307.091451	22.596429
93.913837	3315.698576	22.601447
94.008860	3315.481638	22.606464
94.075255	3311.386972	22.611482
94.257719	3332.095045	22.616499
94.159241	3330.475474	22.621517
93.846825	3338.617060	22.626535
94.310447	3344.023668	22.631552
94.478249	3350.874856	22.636570
94.324011	3367.150652	22.641587
94.743667	3365.153210	22.646605
94.415476	3364.655387	22.651623
94.845044	3380.243191	22.656640
94.866307	3383.471843	22.661658
95.201726	3393.904419	22.666675
95.593461	3384.692927	22.671693
95.665215	3391.256175	22.676711
95.814830	3387.243141	22.681728
95.887188	3386.613124	22.686746
96.058757	3379.522432	22.691763
95.611566	3384.017554	22.696781
95.699874	3387.399831	22.701799
95.937866	3404.365404	22.706816
96.140483	3401.657078	22.711834
96.269940	3411.026701	22.716851
96.447058	3405.450148	22.721869
96.498488	3409.696717	22.726887
96.400420	3405.331105	22.731904
96.553613	3404.637921	22.736922
96.624478	3411.270754	22.741939
97.002489	3418.609821	22.746957
96.763819	3431.663707	22.751975
97.077611	3432.343598	22.756992
97.282953	3431.244551	22.762010
97.380863	3433.167125	22.767027
97.581660	3431.323904	22.772045
97.391346	3433.597795	22.777063
97.766751	3431.616748	22.782080
97.628541	3422.242075	22.787098
97.511959	3427.329293	22.792115
97.654156	3438.795868	22.797133
97.786825	3450.721605	22.802151
97.776336	3455.678583	22.807168
97.774274	3447.841775	22.812186
97.893726	3464.611349	22.817203
98.236194	3468.865990	22.822221
98.183971	3484.822904	22.827239
98.292337	3484.859534	22.832256
98.717430	3488.892919	22.837274
98.528629	3480.229997	22.842291
98.734696	3483.454965	22.847309
98.895028	3508.673906	22.852327
99.071222	3510.293843	22.857344
99.308957	3498.281528	22.862362
98.562786	3510.512280	22.867379
99.172365	3509.406708	22.872397
99.276189	3506.985288	22.877415
98.962098	3508.413753	22.882432
99.500782	3525.114544	22.887450
99.342785	3519.186453	22.892467
99.515906	3520.753215	22.897485
99.543736	3527.736871	22.902503
99.704893	3539.124787	22.907520
100.022987	3552.587071	22.912538
99.796993	3550.757048	22.917555
100.039382	3547.606899	22.922573
100.077316	3563.669697	22.927591
100.321270	3578.554488	22.932608
100.691965	3575.958682	22.937626
100.728625	3577.682550	22.942643
100.711741	3574.478328	22.947661
101.133495	3581.138313	22.952679
101.137758	3576.684032	22.957696
101.211367	3572.701804	22.962714
101.104453	3596.927467	22.967731
101.126048	3595.645724	22.972749
101.409342	3596.197835	22.977767
101.195998	3605.192006	22.982784
101.708394	3594.531690	22.987802
101.530010	3600.086306	22.992819
101.418074	3606.138681	22.997837
101.819230	3609.320480	23.002855
101.745483	3620.439088	23.007872
101.755381	3619.679970	23.012890
101.920391	3622.722015	23.017907
101.652982	3623.126839	23.022925
102.300111	3635.442389	23.027943
102.252551	3638.864937	23.032960
102.388861	3649.928558	23.037978
102.418132	3652.748838	23.042995
102.456088	3645.252872	23.048013
102.733136	3660.653340	23.053031
102.874393	3663.961090	23.058048
103.341109	3664.506560	23.063066
103.418243	3676.349613	23.068083
103.190117	3683.262959	23.073101
103.101781	3668.192628	23.078119
102.643510	3674.933710	23.083136
103.437354	3684.129944	23.088154
103.597911	3692.876198	23.093171
103.497273	3686.588712	23.098189
103.598998	3693.286253	23.103207
103.636320	3711.643935	23.108224
104.089823	3725.151416	23.113242
104.165362	3725.647703	23.118259
104.416860	3715.836216	23.123277
104.634056	3714.773170	23.128295
104.296151	3718.275942	23.133312
104.458182	3729.206172	23.138330
104.758375	3735.519124	23.143347
105.046750	3738.532392	23.148365
105.131706	3734.519944	23.153383
105.287135	3738.775546	23.158400
105.290143	3738.541456	23.163418
105.146182	3733.602188	23.168435
105.492938	3736.789377	23.173453
105.455542	3737.413830	23.178471
105.391472	3750.980325	23.183488
105.536628	3760.388702	23.188506
105.572576	3759.477148	23.193523
105.685875	3767.186091	23.198541
105.839851	3762.376892	23.203559
105.708651	3782.793739	23.208576
106.169173	3785.265559	23.213594
105.858118	3789.149212	23.218611
106.209709	3789.296085	23.223629
106.652267	3793.923355	23.228647
106.477433	3808.615127	23.233664
107.094138	3805.494667	23.238682
106.607870	3813.057682	23.243699
106.710736	3813.628599	23.248717
107.269681	3806.956816	23.253735
106.833188	3815.013895	23.258752
107.224918	3828.521662	23.263770
107.477867	3830.779813	23.268787
107.286985	3827.542836	23.273805
107.541079	3830.290044	23.278823
107.321101	3836.289982	23.283840
107.759100	3839.993164	23.288858
108.202446	3858.015935	23.293875
107.883235	3863.453815	23.298893
108.018236	3851.062817	23.303911
108.174701	3863.297578	23.308928
108.515228	3859.074618	23.313946
108.522552	3862.179285	23.318963
108.498624	3860.876249	23.323981
108.982396	3875.010373	23.328999
108.890005	3891.987133	23.334016
109.120648	3887.983390	23.339034
109.066066	3884.923899	23.344051
109.087369	3885.510753	23.349069
109.299265	3872.397510	23.354087
108.935120	3877.271131	23.359104
109.259031	3878.063085	23.364122
109.411968	3880.680956	23.369139
109.565876	3889.482005	23.374157
109.596410	3894.909288	23.379175
109.736143	3901.275845	23.384192
109.443315	3904.395982	23.389210
109.855026	3902.750086	23.394227
109.685887	3906.472649	23.399245
109.897571	3918.370534	23.404263
110.357890	3922.979273	23.409280
110.285338	3926.143811	23.414298
110.224583	3929.016115	23.419315
110.349887	3943.932422	23.424333
110.672133	3942.073280	23.429351
110.441717	3945.426687	23.434368
110.884726	3949.170139	23.439386
110.928969	3977.204475	23.444403
111.031066	3978.892879	23.449421
111.631789	3964.367718	23.454439
111.780161	3976.547009	23.459456
111.600497	3959.416999	23.464474
111.804004	3966.720503	23.469491
111.692226	3972.444710	23.474509
111.862319	3990.137971	23.479527
111.954387	4000.766844	23.484544
112.268080	3992.930833	23.489562
112.181624	4002.523973	23.494579
112.063395	3995.708862	23.499597
112.188561	4004.489219	23.504615
112.597379	4015.696597	23.509632
112.752437	4019.636685	23.514650
112.682140	4017.861130	23.519667
112.611337	4025.223416	23.524685
112.919271	4035.534414	23.529703
113.463675	4044.511089	23.534720
113.464084	4047.124474	23.539738
113.177040	4040.159035	23.544755
113.157949	4051.414538	23.549773
113.578963	4051.916680	23.554791
113.413194	4066.638804	23.559808
113.303785	4078.523972	23.564826
113.648262	4074.114116	23.569843
113.945491	4089.590698	23.574861
113.922582	4090.310742	23.579879
114.092317	4093.973940	23.584896
114.472098	4102.121050	23.589914
114.359805	4097.754342	23.594931
114.065962	4112.509195	23.599949
114.725601	4115.069810	23.604967
115.113527	4118.900838	23.609984
115.025649	4126.205869	23.615002
115.285742	4124.031335	23.620019
114.864533	4128.206926	23.625037
115.494886	4135.257395	23.630055
115.512370	4143.912653	23.635072
115.650926	4146.655916	23.640090
115.854959	4140.730873	23.645107
115.548136	4144.670754	23.650125
115.783412	4143.601695	23.655143
116.006145	4155.860993	23.660160
115.878513	4158.655431	23.665178
116.390716	4159.364239	23.670195
116.553093	4165.133935	23.675213
116.313049	4165.281968	23.680231
116.745532	4166.161087	23.685248
116.614146	4167.482067	23.690266
117.076428	4170.764866	23.695283
116.184742	4190.619530	23.700301
116.577855	4182.158649	23.705319
116.858370	4187.246995	23.710336
117.253964	4189.220860	23.715354
117.252977	4201.679374	23.720371
117.228433	4218.068183	23.725389
117.435776	4218.995203	23.730407
117.178657	4214.808979	23.735424
117.223039	4229.100601	23.740442
117.900402	4235.787068	23.745459
117.777975	4252.323813	23.750477
117.721770	4249.513874	23.755495
118.064673	4254.680844	23.760512
118.055014	4273.368412	23.765530
118.125939	4267.925022	23.770547
118.243858	4278.168078	23.775565
118.727540	4280.345947	23.780583
118.729682	4282.059509	23.785600
118.935916	4286.275717	23.790618
119.099399	4298.819005	23.795635
119.068029	4308.763511	23.800653
119.291336	4309.621749	23.805671
119.403618	4314.035757	23.810688
119.419112	4310.636945	23.815706
120.066148	4323.903072	23.820723
119.638253	4335.873027	23.825741
119.853907	4326.597110	23.830759
120.034129	4333.882316	23.835776
119.916286	4336.760471	23.840794
120.275905	4355.753261	23.845811
120.325910	4360.296982	23.850829
120.520694	4357.274099	23.855847
120.711211	4354.873705	23.860864
120.669212	4362.345247	23.865882
121.051409	4381.934253	23.870899
121.284341	4388.775631	23.875917
121.058887	4386.026907	23.880935
121.299944	4386.664573	23.885952
120.734143	4392.450576	23.890970
121.260409	4397.128016	23.895987
121.571196	4408.818153	23.901005
121.846698	4415.394042	23.906023
121.960015	4406.626526	23.911040
121.891463	4418.243529	23.916058
122.211169	4429.840744	23.921075
122.176069	4439.334531	23.926093
122.116639	4435.486590	23.931111
122.500917	4435.741983	23.936128
122.038410	4446.372777	23.941146
122.826816	4457.413640	23.946163
122.667551	4466.595464	23.951181
122.725506	4469.351405	23.956199
123.301872	4474.964802	23.961216
123.243706	4482.271633	23.966234
123.432753	4488.804277	23.971251
123.547645	4487.577297	23.976269
123.604764	4480.674558	23.981287
123.571333	4482.125411	23.986304
123.335545	4506.454546	23.991322
124.014820	4512.780979	23.996339
124.171488	4510.739394	24.001357
123.873334	4519.122320	24.006375
124.341823	4523.281714	24.011392
124.353796	4542.105055	24.016410
124.704748	4540.178226	24.021427
124.547413	4542.930029	24.026445
124.585472	4537.160276	24.031463
124.908396	4537.201172	24.036480
124.850638	4558.229211	24.041498
125.046772	4557.646048	24.046515
125.303600	4563.953458	24.051533
124.992296	4561.644284	24.056551
125.306553	4572.393350	24.061568
125.308594	4589.700023	24.066586
125.382398	4590.692176	24.071603
125.491663	4598.796667	24.076621
125.899250	4609.957259	24.081639
126.090727	4615.911930	24.086656
125.930574	4620.021480	24.091674
126.153936	4628.054448	24.096691
126.338624	4640.960804	24.101709
126.372523	4651.207764	24.106727
126.789354	4647.948029	24.111744
126.798122	4653.085393	24.116762
127.243121	4663.403684	24.121779
127.164813	4663.314895	24.126797
127.289265	4665.634318	24.131815
127.589308	4659.921334	24.136832
127.200992	4675.224892	24.141850
127.604291	4685.136225	24.146867
127.908168	4686.720483	24.151885
128.162372	4684.385825	24.156903
128.249498	4678.832452	24.161920
128.093248	4688.815669	24.166938
128.317417	4694.812592	24.171955
128.270852	4709.062022	24.176973
128.362829	4710.269134	24.181991
128.964762	4707.971533	24.187008
128.941579	4730.402158	24.192026
129.246955	4725.357499	24.197043
129.532740	4734.482359	24.202061
129.263938	4733.744763	24.207079
129.844673	4721.254931	24.212096
129.615558	4737.780424	24.217114
129.577808	4730.977679	24.222131
129.490489	4734.157297	24.227149
129.825459	4746.468854	24.232167
130.376485	4742.941869	24.237184
129.913543	4748.203667	24.242202
130.356437	4746.069865	24.247219
130.214724	4762.468052	24.252237
130.377953	4771.047114	24.257255
130.811595	4775.234121	24.262272
130.196777	4772.950375	24.267290
130.843695	4784.174588	24.272307
131.150817	4798.094059	24.277325
131.190210	4799.281006	24.282343
131.302780	4788.168122	24.287360
130.985731	4814.221237	24.292378
131.341466	4817.505066	24.297395
131.551553	4827.942324	24.302413
131.246647	4831.418040	24.307431
131.849933	4834.770411	24.312448
131.496095	4862.347652	24.317466
131.845540	4871.800357	24.322483
132.007005	4886.048899	24.327501
131.970286	4892.149891	24.332519
132.476249	4896.660190	24.337536
132.457362	4908.146619	24.342554
132.867011	4907.517368	24.347571
133.160614	4911.281274	24.352589
132.867866	4916.090322	24.357607
133.413590	4924.041351	24.362624
133.669121	4929.973464	24.367642
133.249136	4937.820115	24.372659
133.710270	4932.362741	24.377677
133.646643	4939.894726	24.382695
133.746385	4934.557101	24.387712
133.983398	4949.516708	24.392730
134.180388	4956.862668	24.397747
134.480171	4964.946944	24.402765
134.474364	4962.671926	24.407783
134.379227	4958.819998	24.412800
134.873536	4970.188185	24.417818
135.018741	4979.546683	24.422835
135.302214	4987.327338	24.427853
135.163424	4983.119240	24.432871
135.392976	4973.449404	24.437888
135.511201	4978.399258	24.442906
135.442496	4989.457937	24.447923
135.698501	5009.199967	24.452941
135.913680	5007.966711	24.457959
136.289128	4993.438149	24.462976
136.404614	4998.735660	24.467994
136.045472	5006.115107	24.473011
136.304359	5005.982957	24.478029
136.038101	5029.430569	24.483047
136.482539	5025.733992	24.488064
136.425551	5041.582539	24.493082
136.548487	5057.421851	24.498099
136.637190	5058.130760	24.503117
137.046985	5072.836125	24.508135
137.349629	5063.874490	24.513152
137.480717	5073.462521	24.518170
137.386551	5081.775867	24.523187
137.741350	5077.335745	24.528205
137.691507	5102.198413	24.533223
138.094885	5098.097899	24.538240
137.732256	5104.107975	24.543258
138.153227	5118.060360	24.548275
138.515833	5121.529407	24.553293
138.169488	5124.045755	24.558311
138.541870	5129.555583	24.563328
138.824887	5140.609756	24.568346
138.754838	5146.659236	24.573363
138.995055	5153.727037	24.578381
138.883669	5159.489434	24.583399
139.394926	5169.058990	24.588416
139.587777	5172.718785	24.593434
139.647456	5175.244131	24.598451
139.703514	5177.530144	24.603469
139.582664	5194.736695	24.608487
140.366636	5200.040014	24.613504
140.341925	5200.937154	24.618522
140.280449	5206.514977	24.623539
140.799170	5212.923631	24.628557
140.717060	5229.407597	24.633575
140.626527	5234.516491	24.638592
141.273437	5232.145493	24.643610
140.729368	5241.599486	24.648627
141.207966	5243.371070	24.653645
141.183525	5266.818979	24.658663
141.127085	5258.049241	24.663680
141.334823	5275.131787	24.668698
141.590635	5285.439036	24.673715
141.854723	5285.397612	24.678733
142.032187	5288.621072	24.683751
142.123541	5294.294930	24.688768
142.020717	5307.092129	24.693786
142.185485	5315.822724	24.698803
142.447231	5310.844716	24.703821
142.819407	5326.619961	24.708839
142.632701	5334.843752	24.713856
142.770449	5331.974849	24.718874
142.875910	5342.362505	24.723891
142.980645	5342.443902	24.728909
143.477682	5375.984053	24.733927
143.419314	5362.728997	24.738944
143.804851	5366.967872	24.743962
143.703322	5364.556283	24.748979
143.613204	5375.886864	24.753997
144.122663	5386.725782	24.759015
144.547594	5389.367549	24.764032
144.543801	5387.341537	24.769050
144.359844	5411.660601	24.774067
144.429138	5411.637069	24.779085
145.022569	5416.610448	24.784103
144.702448	5419.896104	24.789120
145.101366	5427.526282	24.794138
145.021177	5438.669105	24.799155
145.111104	5442.281947	24.804173
145.399741	5462.429719	24.809191
145.628144	5465.774652	24.814208
145.826202	5471.649656	24.819226
145.832814	5476.396167	24.824243
146.492007	5487.555762	24.829261
146.209141	5494.800345	24.834279
146.406436	5503.484898	24.839296
146.329965	5505.908510	24.844314
146.214492	5517.056909	24.849331
146.372336	5516.763815	24.854349
146.748146	5542.819901	24.859367
147.029742	5544.126785	24.864384
147.328142	5544.755510	24.869402
147.213621	5565.118077	24.874419
147.671330	5575.343353	24.879437
147.655465	5571.804013	24.884455
147.684713	5585.590847	24.889472
148.195928	5589.731169	24.894490
147.971540	5597.402251	24.899507
148.165464	5596.582653	24.904525
148.406812	5623.651115	24.909543
148.472872	5617.696703	24.914560
148.354915	5634.451811	24.919578
149.074398	5643.935333	24.924595
149.227052	5651.462137	24.929613
149.103025	5654.483518	24.934631
149.318941	5658.221871	24.939648
150.041455	5673.197555	24.944666
149.696291	5678.226510	24.949683
150.072009	5678.609533	24.954701
150.069740	5677.811199	24.959719
150.174825	5694.948100	24.964736
150.181846	5699.732485	24.969754
150.528711	5700.517772	24.974771
150.888097	5700.208883	24.979789
150.698847	5715.643113	24.984807
150.740063	5720.248528	24.989824
151.266630	5728.341808	24.994842
150.798807	5736.208921	24.999859
151.373823	5757.098168	25.004877
151.476614	5752.523748	25.009895
151.383798	5766.462423	25.014912
151.628933	5767.790819	25.019930
151.901621	5785.002561	25.024947
152.275455	5778.254898	25.029965
152.302414	5790.419703	25.034983
152.169081	5791.737946	25.040000
152.580012	5804.455004	25.045018
152.713209	5818.184691	25.050035
152.800215	5808.189511	25.055053
153.125724	5815.771376	25.060071
153.303890	5830.014883	25.065088
153.500353	5834.820131	25.070106
153.352403	5840.351718	25.075123
153.344411	5840.094070	25.080141
153.878496	5849.846656	25.085159
153.692103	5863.837946	25.090176
153.876793	5868.455645	25.095194
153.942858	5870.620221	25.100211
154.155985	5880.161100	25.105229
154.308202	5895.412559	25.110247
154.348022	5896.608981	25.115264
154.327724	5906.211697	25.120282
154.497453	5908.249552	25.125299
154.661006	5921.570500	25.130317
155.029922	5931.513156	25.135335
154.777825	5943.908028	25.140352
155.361684	5958.896199	25.145370
155.784595	5968.836730	25.150387
155.665974	5970.020098	25.155405
155.834829	5987.065208	25.160423
155.885162	5988.408355	25.165440
156.221655	5992.209963	25.170458
156.438083	6012.259168	25.175475
156.988848	6012.617933	25.180493
156.885714	6009.982380	25.185511
156.692567	6032.343373	25.190528
157.253661	6033.429727	25.195546
157.402485	6047.131884	25.200563
157.437518	6041.441049	25.205581
157.494850	6057.866034	25.210599
157.900621	6069.807526	25.215616
157.827808	6061.270410	25.220634
158.126324	6079.021344	25.225651
158.512049	6087.648244	25.230669
158.469526	6096.578996	25.235687
158.442261	6099.585291	25.240704
158.523533	6098.069894	25.245722
158.633617	6106.714732	25.250739
159.054918	6122.883879	25.255757
159.098452	6142.957158	25.260775
159.036967	6145.548972	25.265792
158.942793	6148.297432	25.270810
159.212898	6176.899550	25.275827
159.699370	6171.999748	25.280845
159.966665	6196.173394	25.285863
159.633825	6198.116394	25.290880
160.372330	6203.856457	25.295898
160.595616	6225.382192	25.300915
160.856369	6226.291481	25.305933
160.957786	6224.046859	25.310951
161.068848	6232.448532	25.315968
161.615525	6237.590460	25.320986
162.100417	6251.685225	25.326003
161.584731	6255.146878	25.331021
162.008063	6245.884807	25.336039
161.991996	6257.071747	25.341056
162.332765	6253.413267	25.346074
162.415017	6263.839808	25.351091
162.716331	6272.587350	25.356109
162.766552	6272.232186	25.361127
162.788752	6280.875092	25.366144
162.892188	6270.959162	25.371162
162.912082	6270.741334	25.376179
162.761234	6289.538318	25.381197
163.224069	6295.577299	25.386215
163.177821	6299.981900	25.391232
163.235079	6301.592313	25.396250
163.414662	6331.411591	25.401267
163.337965	6323.793588	25.406285
163.918543	6340.907110	25.411303
163.682559	6351.632944	25.416320
163.986399	6341.647698	25.421338
164.021710	6372.395645	25.426355
164.280453	6376.692505	25.431373
164.610898	6384.920979	25.436391
164.657079	6411.465584	25.441408
164.935390	6411.055744	25.446426
165.176460	6428.888623	25.451443
165.153178	6441.247982	25.456461
165.419800	6437.272774	25.461479
165.153830	6454.077073	25.466496
165.758380	6458.970079	25.471514
165.988517	6480.495040	25.476531
166.499022	6482.949939	25.481549
166.908001	6481.455777	25.486567
166.496618	6504.672307	25.491584
166.498250	6507.191148	25.496602
166.559953	6511.032757	25.501619
167.259271	6537.891923	25.506637
167.417889	6535.016407	25.511655
167.372554	6545.077962	25.516672
167.348713	6548.503653	25.521690
167.932846	6561.740236	25.526707
168.275788	6561.882183	25.531725
168.474083	6563.912480	25.536743
168.217872	6586.852257	25.541760
168.721395	6596.439563	25.546778
168.684676	6596.751480	25.551795
168.862171	6599.751032	25.556813
169.021216	6617.836866	25.561831
168.932018	6620.676166	25.566848
169.357661	6629.704302	25.571866
169.288454	6649.016056	25.576883
169.315463	6641.198577	25.581901
170.042583	6657.809597	25.586919
169.975564	6680.871380	25.591936
170.104957	6672.939985	25.596954
170.324510	6680.785045	25.601971
170.555253	6700.040391	25.606989
170.797316	6708.203935	25.612007
170.685169	6714.595154	25.617024
170.907863	6722.149309	25.622042
171.363487	6722.122075	25.627059
171.277138	6727.385414	25.632077
171.624898	6750.196048	25.637095
171.652851	6757.812295	25.642112
171.781559	6757.454297	25.647130
172.078813	6776.705617	25.652147
172.367464	6786.860197	25.657165
172.297670	6783.392209	25.662183
172.263499	6797.426655	25.667200
172.985941	6806.736696	25.672218
172.820940	6807.419127	25.677236
172.844015	6828.427638	25.682253
172.960719	6825.561801	25.687271
173.008452	6842.377288	25.692288
173.076397	6857.904772	25.697306
173.570093	6868.352433	25.702324
173.745667	6882.688715	25.707341
174.185743	6882.332444	25.712359
174.249924	6901.752999	25.717376
174.414452	6910.594885	25.722394
174.880954	6909.356858	25.727412
174.716997	6915.219591	25.732429
174.926465	6925.497144	25.737447
174.889325	6934.989388	25.742464
175.523520	6937.541777	25.747482
175.739964	6941.993771	25.752500
175.608787	6952.012174	25.757517
175.818066	6964.379647	25.762535
175.680087	6974.099221	25.767552
176.001123	6980.870948	25.772570
176.367951	6988.658341	25.777588
176.271200	7002.106092	25.782605
176.478373	7014.196121	25.787623
176.819152	7031.313131	25.792640
177.004897	7028.947866	25.797658
177.229613	7044.021607	25.802676
177.233520	7051.187146	25.807693
177.296505	7056.749189	25.812711
177.650644	7072.383550	25.817728
177.832173	7075.672986	25.822746
178.199380	7087.627499	25.827764
177.902038	7101.488736	25.832781
178.269189	7101.579543	25.837799
178.806886	7117.510349	25.842816
179.119152	7133.918456	25.847834
178.873617	7128.422772	25.852852
178.790885	7150.398464	25.857869
179.217042	7156.733915	25.862887
179.677572	7171.313061	25.867904
179.717492	7180.449252	25.872922
180.155025	7183.070370	25.877940
180.255635	7194.009144	25.882957
180.675887	7206.173254	25.887975
180.472807	7210.286948	25.892992
180.902677	7209.632362	25.898010
181.195640	7224.875505	25.903028
180.916931	7228.407546	25.908045
181.383907	7238.016700	25.913063
181.508871	7236.390186	25.918080
181.289371	7249.604792	25.923098
181.548294	7250.167157	25.928116
181.608199	7278.573465	25.933133
181.767992	7278.933530	25.938151
182.026505	7302.772216	25.943168
182.203963	7309.291902	25.948186
182.603610	7318.191859	25.953204
182.440065	7336.688832	25.958221
183.359610	7339.177634	25.963239
183.220256	7354.630676	25.968256
183.115486	7371.277963	25.973274
183.399890	7375.845695	25.978292
183.403002	7394.225064	25.983309
183.689434	7392.386979	25.988327
184.490126	7413.807863	25.993344
184.314631	7420.275547	25.998362
184.833953	7424.014085	26.003380
184.559067	7437.212246	26.008397
185.074306	7444.414640	26.013415
184.989991	7447.095452	26.018432
185.117625	7457.884928	26.023450
185.938263	7469.582392	26.028468
185.555337	7488.199124	26.033485
185.575257	7486.866861	26.038503
185.997735	7495.457099	26.043520
186.193901	7504.347983	26.048538
186.466440	7510.840218	26.053556
186.577566	7530.055189	26.058573
186.410569	7538.340014	26.063591
186.886239	7541.283538	26.068608
186.952364	7565.594684	26.073626
187.291993	7565.588782	26.078644
187.734125	7571.236805	26.083661
187.771972	7566.343781	26.088679
187.854209	7577.465611	26.093696
187.851217	7593.083753	26.098714
188.029743	7603.467557	26.103732
187.825849	7615.395075	26.108749
188.125553	7617.823173	26.113767
187.720677	7628.361529	26.118784
188.601282	7644.832591	26.123802
189.108385	7660.629753	26.128820
189.001283	7675.519218	26.133837
189.114230	7682.753161	26.138855
189.222285	7686.938184	26.143872
189.532137	7707.571283	26.148890
189.918787	7715.119103	26.153908
189.839142	7738.613543	26.158925
190.081012	7760.472810	26.163943
190.373350	7767.372448	26.168960
190.650872	7781.876568	26.173978
191.169580	7778.110988	26.178996
191.066466	7804.911455	26.184013
191.490183	7808.055741	26.189031
191.421674	7815.264493	26.194048
191.635862	7835.388652	26.199066
191.796975	7840.184180	26.204084
191.611121	7850.243205	26.209101
192.263211	7861.604265	26.214119
192.329872	7876.293031	26.219136
192.624566	7889.181288	26.224154
193.175112	7896.820318	26.229172
193.084006	7916.926095	26.234189
193.165735	7916.663834	26.239207
193.252979	7929.540419	26.244224
193.665334	7938.950132	26.249242
194.191497	7948.521973	26.254260
194.097553	7962.541413	26.259277
194.553305	7969.854360	26.264295
194.262705	7980.659150	26.269312
194.713362	8000.945339	26.274330
195.000876	8002.964977	26.279348
195.126629	8009.189933	26.284365
195.457022	8030.893583	26.289383
195.612165	8042.073727	26.294400
195.478692	8040.187707	26.299418
195.507617	8044.587262	26.304436
196.126915	8061.030180	26.309453
195.733851	8079.563852	26.314471
196.156032	8077.887545	26.319488
196.357757	8105.411021	26.324506
196.612060	8105.203806	26.329524
197.066790	8133.180194	26.334541
197.212544	8139.616743	26.339559
197.489274	8143.106140	26.344576
197.668562	8170.806869	26.349594
198.008436	8169.064521	26.354612
197.966213	8190.855148	26.359629
197.991371	8197.228525	26.364647
198.307725	8208.093059	26.369664
198.312613	8221.213219	26.374682
198.941373	8220.249617	26.379700
199.170148	8242.657687	26.384717
199.305665	8259.517541	26.389735
199.842008	8260.096463	26.394752
199.556383	8259.866491	26.399770
200.016063	8276.249365	26.404788
199.816744	8286.061322	26.409805
199.942029	8289.378730	26.414823
200.491882	8293.100038	26.419840
200.295343	8317.241793	26.424858
200.300147	8310.424741	26.429876
200.708167	8341.796366	26.434893
200.871292	8347.715653	26.439911
201.105948	8357.298647	26.444928
201.316697	8371.276977	26.449946
201.502208	8387.178815	26.454964
201.796666	8395.435930	26.459981
201.705585	8414.844514	26.464999
202.333113	8416.365774	26.470016
202.295777	8433.941125	26.475034
202.789454	8449.289594	26.480052
202.976432	8459.479970	26.485069
203.083975	8473.689232	26.490087
203.503433	8482.198320	26.495104
203.588223	8492.505752	26.500122
203.749513	8506.592961	26.505140
204.287648	8505.539357	26.510157
203.912478	8507.716541	26.515175
204.563069	8521.304047	26.520192
204.545541	8531.561229	26.525210
204.395505	8551.878986	26.530228
204.782097	8556.825651	26.535245
205.055287	8580.038565	26.540263
205.365480	8585.284510	26.545280
205.300562	8600.272296	26.550298
205.603705	8611.704272	26.555316
205.773334	8633.500116	26.560333
205.794174	8641.667605	26.565351
206.699276	8660.007956	26.570368
206.387048	8678.955781	26.575386
206.772491	8691.341016	26.580404
207.230769	8700.295602	26.585421
207.369140	8716.593444	26.590439
207.554051	8721.732766	26.595456
207.468192	8734.753846	26.600474
207.787502	8741.024499	26.605492
208.115012	8764.260706	26.610509
208.002593	8778.855112	26.615527
208.702737	8784.911414	26.620544
208.715793	8800.518589	26.625562
208.767555	8819.138014	26.630580
208.921178	8820.761966	26.635597
209.370839	8843.966508	26.640615
209.413164	8852.585365	26.645632
209.503467	8866.844987	26.650650
210.101555	8876.608107	26.655668
210.172232	8895.897135	26.660685
210.843295	8900.028963	26.665703
210.913672	8904.305411	26.670720
210.615238	8922.600934	26.675738
210.767271	8934.252532	26.680756
211.023946	8936.826465	26.685773
211.272274	8957.590573	26.690791
211.770662	8967.198869	26.695808
211.694341	8982.318196	26.700826
211.872946	8999.434024	26.705844
211.990091	9012.846568	26.710861
212.207219	9025.214194	26.715879
212.538471	9045.476034	26.720896
212.557035	9057.767441	26.725914
213.074644	9063.593537	26.730932
213.231244	9083.440764	26.735949
213.488976	9103.584738	26.740967
213.780529	9099.295647	26.745984
213.939839	9116.076778	26.751002
214.203654	9133.469850	26.756020
214.254989	9133.266007	26.761037
214.490737	9153.318761	26.766055
214.689675	9161.433320	26.771072
214.712085	9179.508338	26.776090
214.975929	9188.503093	26.781108
215.466722	9204.338863	26.786125
215.440397	9222.560478	26.791143
215.967118	9231.141512	26.796160
215.951304	9257.646243	26.801178
215.903684	9252.150492	26.806196
216.477455	9277.432577	26.811213
216.400545	9288.378298	26.816231
217.118824	9300.579193	26.821248
217.019264	9308.911073	26.826266
216.887602	9333.959601	26.831284
217.582097	9344.964474	26.836301
217.241454	9358.887850	26.841319
217.532167	9369.766556	26.846336
217.879130	9389.641119	26.851354
218.258043	9406.151311	26.856372
218.210190	9412.883848	26.861389
218.182580	9434.105325	26.866407
218.938689	9447.023417	26.871424
219.098694	9472.477937	26.876442
219.343243	9489.486008	26.881460
219.871797	9503.405932	26.886477
219.941202	9512.415519	26.891495
220.324857	9535.066103	26.896512
220.493864	9535.674203	26.901530
220.781596	9552.309315	26.906548
220.723825	9555.134667	26.911565
220.886985	9587.970721	26.916583
221.316670	9591.935294	26.921600
221.872766	9610.675415	26.926618
221.973590	9620.592607	26.931636
222.204156	9626.429119	26.936653
222.102321	9647.861381	26.941671
222.389513	9654.674127	26.946688
222.726065	9674.212787	26.951706
222.395144	9683.433567	26.956724
223.008677	9697.469776	26.961741
223.442238	9715.509320	26.966759
223.871189	9730.793216	26.971776
224.035553	9736.201259	26.976794
224.007872	9759.273339	26.981812
224.341028	9759.940980	26.986829
224.097621	9787.931356	26.991847
224.857319	9801.420620	26.996864
225.173652	9818.411432	27.001882
225.463570	9817.854468	27.006900
225.742983	9832.107306	27.011917
225.626079	9841.746143	27.016935
225.633459	9861.222901	27.021952
226.355833	9876.214673	27.026970
226.049842	9885.191684	27.031988
226.335218	9893.937131	27.037005
226.429523	9906.842399	27.042023
226.901367	9924.484630	27.047040
227.095792	9947.212721	27.052058
227.300623	9952.980747	27.057076
227.453141	9964.973915	27.062093
227.500033	9980.081063	27.067111
228.032792	9998.045350	27.072128
228.135950	10016.563198	27.077146
228.069428	10032.821670	27.082164
228.766570	10056.156301	27.087181
228.807825	10071.415962	27.092199
228.860365	10079.721200	27.097216
229.386170	10089.995161	27.102234
229.175403	10112.588012	27.107252
229.891151	10125.029813	27.112269
229.667260	10140.713119	27.117287
229.987954	10140.656515	27.122304
230.119995	10164.300830	27.127322
230.557097	10185.560871	27.132340
231.016153	10204.629382	27.137357
231.051358	10215.090779	27.142375
231.392583	10225.529502	27.147392
231.427077	10238.267550	27.152410
231.661936	10255.009455	27.157428
232.276121	10266.305316	27.162445
232.250051	10290.432392	27.167463
232.349693	10301.654165	27.172480
232.660308	10314.276387	27.177498
233.261391	10332.315545	27.182516
233.571170	10342.547709	27.187533
233.598987	10349.818130	27.192551
233.659704	10359.741998	27.197568
233.891430	10379.117844	27.202586
234.365238	10392.229223	27.207604
234.815305	10403.838209	27.212621
234.993166	10422.701553	27.217639
235.497445	10430.497287	27.222656
235.476111	10434.883179	27.227674
235.404542	10446.684423	27.232692
235.718556	10459.792465	27.237709
235.697160	10476.710485	27.242727
235.948248	10484.536434	27.247744
236.190497	10507.901846	27.252762
236.205113	10527.239234	27.257780
236.087142	10540.285549	27.262797
236.887532	10571.321608	27.267815
237.040045	10587.407317	27.272832
237.448063	10605.470670	27.277850
237.448537	10630.418138	27.282868
237.795769	10642.343348	27.287885
238.163239	10663.640103	27.292903
238.138278	10671.215725	27.297920
238.893863	10693.045328	27.302938
238.725262	10717.498406	27.307956
239.427216	10730.435351	27.312973
239.661731	10740.824771	27.317991
239.851480	10749.402463	27.323008
240.439341	10766.335815	27.328026
240.262509	10789.277810	27.333044
240.798746	10790.946197	27.338061
240.928072	10800.142786	27.343079
240.857628	10819.531691	27.348096
241.582278	10824.741763	27.353114
241.614383	10840.338186	27.358132
242.046105	10848.025475	27.363149
242.072996	10867.418128	27.368167
242.300765	10873.763837	27.373184
242.374668	10887.058200	27.378202
242.583972	10908.301072	27.383220
242.991782	10916.538396	27.388237
243.279246	10930.572940	27.393255
243.128561	10946.996953	27.398272
243.847532	10963.584714	27.403290
243.530764	10984.644848	27.408308
244.009479	10992.271157	27.413325
244.255523	11018.551064	27.418343
244.304359	11037.267887	27.423360
244.883920	11045.585720	27.428378
244.802588	11070.916028	27.433396
245.282395	11087.702404	27.438413
245.384474	11083.155204	27.443431
245.118613	11107.437727	27.448448
245.765452	11121.119301	27.453466
245.930818	11138.040236	27.458484
245.923089	11154.363095	27.463501
246.293782	11171.599232	27.468519
246.083324	11208.086870	27.473536
247.172730	11214.414547	27.478554
247.297028	11234.319642	27.483572
247.412253	11250.547540	27.488589
248.101721	11272.902873	27.493607
248.145830	11286.101142	27.498624
248.511847	11297.509133	27.503642
248.410508	11316.852869	27.508660
248.612510	11330.250626	27.513677
248.765786	11344.401231	27.518695
249.303233	11366.376312	27.523712
249.700782	11381.044424	27.528730
249.289346	11408.719354	27.533748
249.807826	11424.132708	27.538765
250.154077	11436.996404	27.543783
250.291602	11455.908155	27.548800
250.891522	11477.459926	27.553818
251.105463	11505.065449	27.558836
251.500459	11526.772528	27.563853
251.674972	11525.838887	27.568871
251.687636	11553.150771	27.573888
251.962695	11562.713298	27.578906
252.397630	11587.556085	27.583924
252.570908	11608.562251	27.588941
253.089699	11624.013613	27.593959
253.297110	11638.155958	27.598976
253.493862	11652.009476	27.603994
253.522424	11671.273230	27.609012
254.116911	11697.720541	27.614029
254.280788	11706.081685	27.619047
254.407026	11724.682862	27.624064
254.571547	11736.678443	27.629082
254.822145	11756.232745	27.634100
254.942835	11781.437630	27.639117
255.447820	11799.269062	27.644135
255.643816	11815.279542	27.649152
256.182152	11823.964163	27.654170
256.127447	11842.672745	27.659188
256.309406	11863.652574	27.664205
256.498489	11891.354132	27.669223
256.774694	11908.264712	27.674240
257.014405	11922.642200	27.679258
257.287787	11937.927012	27.684276
257.727621	11971.611227	27.689293
257.957795	11995.864553	27.694311
258.044624	12007.496704	27.699328
258.487065	12029.550600	27.704346
258.748102	12042.358589	27.709364
259.322632	12064.893919	27.714381
259.528437	12077.129555	27.719399
259.338276	12092.035547	27.724416
260.096650	12114.238990	27.729434
260.258032	12126.961600	27.734452
260.344830	12149.996578	27.739469
260.505070	12164.787738	27.744487
260.896955	12182.274107	27.749504
261.265793	12189.801280	27.754522
261.413788	12216.246637	27.759540
261.361568	12230.837455	27.764557
261.805862	12249.203015	27.769575
261.755693	12260.762050	27.774592
262.226013	12285.057074	27.779610
262.263320	12317.216589	27.784628
262.521098	12323.074945	27.789645
263.189289	12344.664383	27.794663
263.121343	12365.674446	27.799680
263.601082	12381.195706	27.804698
263.776738	12403.244465	27.809716
264.186215	12424.287169	27.814733
264.432933	12437.508187	27.819751
264.508587	12467.429366	27.824768
264.925436	12474.159675	27.829786
265.417656	12486.979118	27.834804
265.403107	12511.381968	27.839821
266.010011	12533.398060	27.844839
266.171340	12542.170494	27.849856
265.846783	12552.847443	27.854874
266.531629	12580.734450	27.859892
266.923640	12607.836857	27.864909
266.861239	12611.121281	27.869927
267.207312	12645.159278	27.874944
267.713840	12661.469196	27.879962
268.119880	12672.928595	27.884980
268.150970	12700.409776	27.889997
268.890305	12708.343326	27.895015
268.839297	12730.349028	27.900032
269.088549	12739.155149	27.905050
269.215152	12761.755166	27.910068
269.492331	12780.823211	27.915085
269.935732	12804.223123	27.920103
270.165970	12825.171194	27.925120
270.245753	12843.632331	27.930138
270.769180	12864.458727	27.935156
270.825346	12884.152026	27.940173
271.153421	12899.855367	27.945191
271.494595	12925.523030	27.950208
271.939782	12941.508061	27.955226
271.941581	12951.401473	27.960244
272.208054	12979.907245	27.965261
272.871726	12990.492788	27.970279
272.946251	13011.342300	27.975296
273.136582	13026.312581	27.980314
272.981128	13049.661344	27.985332
273.371644	13082.136305	27.990349
273.259051	13096.149871	27.995367
273.821541	13115.896727	28.000384
274.153034	13150.878984	28.005402
274.920088	13177.026598	28.010420
274.726588	13190.023415	28.015437
275.376429	13205.180806	28.020455
275.449931	13228.932879	28.025472
275.989573	13252.024579	28.030490
276.158687	13269.850017	28.035508
276.484176	13292.027923	28.040525
276.738768	13306.865198	28.045543
276.697432	13324.287854	28.050560
277.303085	13343.532384	28.055578
277.690930	13364.677422	28.060596
277.960279	13388.945346	28.065613
278.020122	13397.010897	28.070631
278.653668	13426.808300	28.075648
278.521672	13444.529488	28.080666
278.957354	13469.504115	28.085684
279.376614	13486.027371	28.090701
279.357507	13494.509554	28.095719
279.500372	13518.409024	28.100736
279.745236	13543.508380	28.105754
280.083015	13560.164469	28.110772
279.864018	13584.344927	28.115789
280.852668	13595.937840	28.120807
281.125644	13629.224815	28.125824
280.939685	13644.459802	28.130842
281.258916	13663.765316	28.135860
281.760598	13698.402961	28.140877
282.164908	13699.261723	28.145895
282.598579	13732.981622	28.150912
282.720273	13737.816423	28.155930
283.274811	13761.755925	28.160948
283.113031	13785.119215	28.165965
283.617582	13800.975667	28.170983
283.928245	13814.317111	28.176000
284.208295	13847.587570	28.181018
284.382487	13853.990051	28.186036
284.634684	13874.708462	28.191053
285.272159	13894.769665	28.196071
285.239354	13925.938624	28.201088
285.314769	13945.661588	28.206106
285.883201	13957.235284	28.211124
285.688000	13986.664414	28.216141
286.353876	14005.991769	28.221159
286.424778	14031.744322	28.226176
286.754791	14057.108930	28.231194
287.239613	14071.146477	28.236212
287.247395	14094.966773	28.241229
287.982850	14125.361982	28.246247
288.372680	14142.796798	28.251264
288.414678	14171.367946	28.256282
288.883141	14182.824800	28.261300
289.155517	14203.426715	28.266317
289.396978	14216.529791	28.271335
289.515172	14242.711043	28.276352
290.028865	14267.068137	28.281370
290.477379	14283.764361	28.286388
290.638088	14311.581278	28.291405
291.095401	14319.670225	28.296423
291.209542	14346.041742	28.301440
291.143778	14363.740777	28.306458
292.013482	14379.243646	28.311476
292.225632	14407.324246	28.316493
292.458388	14424.790242	28.321511
292.693094	14444.564566	28.326528
292.944322	14471.953817	28.331546
293.340916	14492.786082	28.336564
293.195538	14509.648176	28.341581
293.603683	14521.717893	28.346599
293.929929	14560.847093	28.351616
294.004237	14577.870640	28.356634
294.254518	14601.164061	28.361652
294.587342	14631.421027	28.366669
295.168839	14655.013189	28.371687
295.721075	14677.640396	28.376704
295.837430	14697.878828	28.381722
296.321107	14714.895217	28.386740
296.321712	14742.797848	28.391757
296.897447	14748.180791	28.396775
297.361095	14775.729854	28.401792
297.214590	14799.546773	28.406810
297.362333	14816.502181	28.411828
297.691365	14845.793665	28.416845
298.079525	14859.976425	28.421863
298.577183	14897.620360	28.426880
298.548460	14919.767221	28.431898
299.387414	14947.835699	28.436916
299.433649	14959.807634	28.441933
299.936289	14972.728195	28.446951
300.140781	14996.882000	28.451968
299.946270	15022.551136	28.456986
300.553771	15029.691491	28.462004
300.603828	15052.849441	28.467021
301.264033	15081.700942	28.472039
301.622802	15101.822871	28.477056
301.647209	15127.918962	28.482074
302.121907	15130.825963	28.487092
302.136626	15155.325523	28.492109
302.586050	15175.398587	28.497127
302.693382	15192.291177	28.502144
302.881544	15216.157254	28.507162
303.370810	15239.151878	28.512180
303.515718	15268.848689	28.517197
304.011028	15288.320924	28.522215
304.392331	15314.531911	28.527232
304.553964	15341.168975	28.532250
304.945983	15366.494028	28.537268
305.399411	15388.843834	28.542285
305.624029	15406.144612	28.547303
305.780751	15434.472276	28.552320
305.789295	15459.339557	28.557338
306.250791	15487.815375	28.562356
306.502757	15512.695126	28.567373
306.934516	15543.080162	28.572391
307.264026	15568.671100	28.577408
307.608319	15595.939999	28.582426
308.101125	15623.008805	28.587444
308.261613	15642.312765	28.592461
308.378526	15663.164851	28.597479
308.862431	15693.488265	28.602496
309.033542	15725.787332	28.607514
309.582369	15746.328656	28.612532
309.757806	15784.530151	28.617549
309.883627	15807.898230	28.622567
310.348395	15827.066276	28.627584
310.921442	15857.815002	28.632602
311.420360	15882.094354	28.637620
311.506701	15919.580484	28.642637
311.493024	15938.169799	28.647655
312.217103	15966.046155	28.652672
312.218164	15988.546484	28.657690
312.337387	16010.775655	28.662708
312.777433	16039.381989	28.667725
313.105024	16077.819223	28.672743
313.661105	16091.367015	28.677760
313.584826	16135.432790	28.682778
314.020981	16166.904628	28.687796
314.650302	16193.845467	28.692813
314.720304	16216.287886	28.697831
315.465130	16236.723229	28.702848
315.668665	16263.898263	28.707866
316.086377	16288.392992	28.712884
316.229428	16305.988461	28.717901
316.667797	16327.909011	28.722919
316.890493	16355.501250	28.727936
317.129023	16386.739094	28.732954
317.829586	16405.618103	28.737972
317.886571	16435.478939	28.742989
318.379592	16450.189712	28.748007
318.957973	16477.808530	28.753024
319.125419	16500.337087	28.758042
319.489913	16519.780530	28.763060
319.625972	16546.871778	28.768077
319.860567	16563.085509	28.773095
320.217845	16579.201073	28.778112
320.485607	16614.262825	28.783130
320.782288	16630.012060	28.788148
320.766248	16658.463345	28.793165
321.025793	16685.563872	28.798183
321.407635	16697.500110	28.803200
321.476221	16723.850446	28.808218
322.275910	16745.048420	28.813236
322.478232	16771.027273	28.818253
322.712551	16800.428174	28.823271
322.767185	16822.794742	28.828288
323.489987	16853.527919	28.833306
323.622525	16877.180514	28.838324
323.663243	16896.772971	28.843341
324.061341	16931.211596	28.848359
324.696321	16955.679456	28.853376
324.755507	16992.056948	28.858394
325.255624	17021.934558	28.863412
325.688788	17046.175143	28.868429
325.853781	17070.198762	28.873447
326.368335	17098.387539	28.878464
326.434032	17136.514146	28.883482
326.715950	17154.840385	28.888500
327.144375	17185.784453	28.893517
327.504686	17208.703720	28.898535
328.057982	17234.542935	28.903552
328.236027	17267.566823	28.908570
328.486929	17293.781983	28.913588
328.962008	17331.377369	28.918605
329.109674	17359.668220	28.923623
329.741136	17383.713917	28.928640
329.728581	17416.540494	28.933658
330.226751	17436.854662	28.938676
330.538947	17462.270785	28.943693
330.936218	17494.755335	28.948711
331.283398	17526.616053	28.953728
331.677362	17555.658276	28.958746
331.988601	17580.638808	28.963764
332.664075	17611.071056	28.968781
332.547068	17632.347273	28.973799
332.861416	17664.169138	28.978816
333.112932	17697.087490	28.983834
333.709149	17721.233889	28.988852
334.360468	17748.833626	28.993869
334.641499	17771.955501	28.998887
334.907719	17786.816538	29.003904
335.351862	17827.671205	29.008922
335.773642	17849.899320	29.013940
336.158011	17870.541325	29.018957
336.092525	17890.653661	29.023975
336.577114	17925.108935	29.028992
336.528590	17947.682485	29.034010
337.113791	17975.476109	29.039028
337.507553	17999.597712	29.044045
337.569235	18024.358891	29.049063
338.162732	18056.971583	29.054080
338.356245	18092.470917	29.059098
338.837281	18118.846987	29.064116
339.219421	18145.030106	29.069133
339.218284	18180.705395	29.074151
339.802129	18205.448186	29.079168
340.393492	18233.140133	29.084186
340.687320	18255.300311	29.089204
340.762649	18277.387342	29.094221
341.476089	18306.437503	29.099239
341.648861	18334.624762	29.104256
342.053496	18358.637709	29.109274
342.301062	18384.501081	29.114292
342.695390	18404.087051	29.119309
342.962139	18432.468212	29.124327
342.942493	18464.280532	29.129344
343.310155	18484.331948	29.134362
343.227062	18515.465666	29.139380
343.475475	18549.485220	29.144397
343.996998	18584.814035	29.149415
344.837613	18612.328491	29.154432
345.457265	18647.048186	29.159450
345.689572	18675.182388	29.164468
345.666694	18691.839408	29.169485
345.936408	18724.573436	29.174503
346.490354	18748.367626	29.179520
346.867106	18772.303321	29.184538
347.232252	18795.261613	29.189556
347.612176	18824.200532	29.194573
348.102492	18857.323516	29.199591
348.348321	18883.465804	29.204608
348.538111	18906.742314	29.209626
348.876926	18933.779864	29.214644
349.222037	18958.504151	29.219661
349.656846	18991.983538	29.224679
350.007321	19017.111399	29.229696
350.111277	19047.237403	29.234714
350.252785	19091.307363	29.239732
350.937148	19120.148490	29.244749
351.075530	19153.775674	29.249767
351.607784	19182.027887	29.254784
352.288616	19214.729927	29.259802
352.515880	19255.324625	29.264820
353.189368	19283.030475	29.269837
353.251366	19306.959270	29.274855
353.418787	19333.240801	29.279872
354.065455	19357.867814	29.284890
354.276144	19386.878302	29.289908
354.416441	19413.897071	29.294925
354.856124	19459.488005	29.299943
355.578029	19495.267248	29.304960
355.908615	19515.458211	29.309978
355.963150	19547.677661	29.314996
356.596912	19569.021608	29.320013
356.930401	19609.739397	29.325031
357.047926	19640.565489	29.330048
357.556048	19668.525239	29.335066
357.528928	19700.940954	29.340084
358.194278	19728.048498	29.345101
358.584907	19763.665311	29.350119
358.936072	19794.726723	29.355136
358.936529	19817.155763	29.360154
359.664192	19859.644570	29.365172
359.652722	19878.316284	29.370189
359.958243	19921.250436	29.375207
360.711660	19949.273254	29.380224
360.840605	19993.441984	29.385242
361.372932	20019.035462	29.390260
362.029812	20059.899393	29.395277
362.090983	20092.554651	29.400295
362.684321	20127.356920	29.405312
362.946434	20160.574723	29.410330
363.296634	20184.806946	29.415348
363.728041	20218.737558	29.420365
364.021303	20254.522151	29.425383
364.200131	20279.204655	29.430400
364.695766	20315.052432	29.435418
364.977506	20349.695403	29.440436
365.742578	20373.502732	29.445453
365.908921	20414.810700	29.450471
366.254108	20438.803927	29.455488
366.528708	20465.683060	29.460506
366.512770	20501.851407	29.465524
367.395278	20524.351591	29.470541
367.590722	20569.755906	29.475559
367.809253	20588.682910	29.480576
368.181201	20618.244928	29.485594
368.539947	20656.661060	29.490612
369.005125	20675.094591	29.495629
369.367896	20718.735492	29.500647
369.725131	20743.693914	29.505664
369.748396	20767.820108	29.510682
370.227969	20803.924029	29.515700
370.877519	20834.251642	29.520717
371.238213	20867.069775	29.525735
371.397965	20897.164605	29.530752
371.775988	20923.156221	29.535770
372.228832	20961.994181	29.540788
372.601666	20992.801357	29.545805
372.653048	21030.697704	29.550823
373.143786	21058.403102	29.555840
373.674151	21099.339561	29.560858
374.260089	21134.460698	29.565876
374.648831	21170.282548	29.570893
375.011267	21204.983888	29.575911
375.111942	21231.000398	29.580928
375.616320	21263.765092	29.585946
375.916931	21304.801152	29.590964
376.533869	21339.380722	29.595981
376.732628	21377.962329	29.600999
376.939801	21406.995306	29.606016
377.651944	21430.786935	29.611034
377.801232	21468.548733	29.616052
378.486722	21501.980500	29.621069
378.717790	21542.528776	29.626087
379.117872	21575.171315	29.631104
379.620923	21602.692309	29.636122
379.834155	21651.085048	29.641140
380.398337	21680.517449	29.646157
380.557912	21721.475367	29.651175
380.870985	21745.955437	29.656192
381.598877	21778.742844	29.661210
381.816585	21818.188004	29.666228
382.292004	21856.885178	29.671245
382.554024	21889.063319	29.676263
382.509069	21926.104485	29.681280
383.643091	21961.476136	29.686298
383.640714	21997.499764	29.691316
384.290206	22037.029377	29.696333
384.703848	22066.985119	29.701351
385.100716	22099.016102	29.706368
385.529568	22121.462802	29.711386
385.627447	22161.647761	29.716404
386.658852	22194.192431	29.721421
386.784664	22232.250029	29.726439
386.887381	22262.760278	29.731456
387.105686	22292.462610	29.736474
387.170905	22335.452295	29.741492
387.846849	22361.285398	29.746509
388.251481	22403.495393	29.751527
388.283911	22445.909115	29.756544
389.117252	22471.464950	29.761562
389.455241	22515.082104	29.766580
389.858543	22541.975498	29.771597
390.992665	22584.090568	29.776615
390.864346	22620.002354	29.781632
391.324904	22649.073289	29.786650
391.419777	22683.288337	29.791668
391.983731	22710.251579	29.796685
392.469734	22747.103684	29.801703
392.789258	22787.198319	29.806720
392.981610	22814.011382	29.811738
393.373088	22866.707704	29.816756
393.856495	22882.638098	29.821773
394.404122	22916.150721	29.826791
394.623962	22953.506193	29.831808
395.150895	22982.377646	29.836826
395.345992	23014.624966	29.841844
395.804687	23046.161223	29.846861
396.240265	23077.043963	29.851879
396.262060	23123.391286	29.856896
396.850999	23141.308523	29.861914
397.230272	23173.685229	29.866932
397.230383	23210.942899	29.871949
397.704397	23256.170715	29.876967
398.098601	23303.009889	29.881984
398.818959	23339.655765	29.887002
399.187085	23383.630297	29.892020
399.205433	23418.029211	29.897037
399.789435	23461.256027	29.902055
399.909270	23508.720031	29.907072
400.839899	23539.999888	29.912090
401.334928	23572.978400	29.917108
401.507307	23623.910049	29.922125
402.302872	23655.552486	29.927143
402.198607	23691.304449	29.932160
403.004023	23720.164948	29.937178
403.089039	23761.473669	29.942196
403.653427	23798.561896	29.947213
403.897848	23843.947074	29.952231
404.175986	23889.346032	29.957248
404.864613	23918.629553	29.962266
404.918372	23958.862962	29.967284
405.611949	24004.374051	29.972301
406.039533	24042.514223	29.977319
406.348946	24083.181794	29.982336
407.118153	24117.691798	29.987354
407.605059	24163.096592	29.992372
407.729503	24201.568926	29.997389
408.670925	24231.040809	30.002407
408.783901	24276.390682	30.007424
409.155744	24309.117965	30.012442
409.673253	24354.139229	30.017460
409.808885	24386.296964	30.022477
410.448298	24420.050518	30.027495
410.748953	24457.908025	30.032512
411.486064	24499.046609	30.037530
411.719768	24534.841930	30.042548
411.800883	24570.686495	30.047565
412.391744	24607.772075	30.052583
412.699542	24648.908697	30.057600
412.845624	24692.503790	30.062618
413.326973	24726.358455	30.067636
414.019727	24772.079965	30.072653
414.365541	24813.419518	30.077671
414.711850	24859.979133	30.082688
414.905758	24894.435237	30.087706
415.469327	24944.797071	30.092724
415.759154	24986.341660	30.097741
416.450466	25028.329025	30.102759
416.767787	25073.560212	30.107776
417.735976	25108.476819	30.112794
418.084777	25141.714650	30.117812
418.162610	25182.205848	30.122829
418.639204	25216.175839	30.127847
418.938213	25251.785254	30.132864
419.616218	25295.999834	30.137882
419.641618	25338.572460	30.142900
419.967338	25385.433548	30.147917
420.551086	25425.877590	30.152935
420.575170	25461.018529	30.157952
421.208650	25496.007196	30.162970
421.652725	25530.791756	30.167988
422.069827	25572.412416	30.173005
422.432699	25614.787406	30.178023
422.881998	25660.112995	30.183040
423.442003	25698.810684	30.188058
423.970245	25730.156995	30.193076
424.113854	25774.437371	30.198093
424.526717	25808.702742	30.203111
425.223364	25858.502498	30.208128
425.460072	25885.970001	30.213146
425.591565	25925.575805	30.218164
426.199618	25972.052750	30.223181
426.864099	26015.316703	30.228199
427.125651	26063.339663	30.233216
427.238013	26102.449525	30.238234
428.133223	26149.810951	30.243252
428.273825	26191.330833	30.248269
428.734504	26229.773333	30.253287
429.312036	26289.559623	30.258304
429.901247	26320.423292	30.263322
430.441388	26362.272792	30.268340
430.618103	26408.021963	30.273357
431.097485	26443.763230	30.278375
431.135296	26502.421214	30.283392
431.926836	26545.584236	30.288410
432.612291	26589.130540	30.293428
432.807040	26632.008012	30.298445
433.313469	26677.270050	30.303463
433.633554	26717.890703	30.308480
434.205773	26769.703074	30.313498
434.516384	26807.860483	30.318516
435.256508	26850.020962	30.323533
435.796497	26895.847058	30.328551
435.956665	26938.509382	30.333568
436.941363	26975.518667	30.338586
436.904124	27010.817265	30.343604
437.290376	27060.460025	30.348621
437.971537	27104.924563	30.353639
438.101425	27146.903145	30.358656
438.335401	27190.578341	30.363674
438.710655	27241.019635	30.368692
439.064842	27286.268953	30.373709
440.102937	27326.595066	30.378727
440.525311	27378.103796	30.383744
440.746643	27413.236181	30.388762
441.094226	27454.998006	30.393780
441.625143	27515.364051	30.398797
442.390100	27554.602028	30.403815
442.644615	27606.896091	30.408832
443.455902	27640.217275	30.413850
443.203552	27690.479882	30.418868
443.893829	27734.748431	30.423885
444.601728	27774.830086	30.428903
444.874159	27826.635220	30.433920
445.591517	27867.082170	30.438938
446.265043	27907.605593	30.443956
446.405201	27953.471414	30.448973
447.130561	27979.853907	30.453991
447.327832	28025.432835	30.459008
447.994312	28069.351881	30.464026
448.538026	28106.735693	30.469044
448.618217	28156.460663	30.474061
449.289246	28197.718256	30.479079
449.190812	28243.824362	30.484096
449.436071	28275.029308	30.489114
450.158901	28317.631667	30.494132
450.423930	28366.481215	30.499149
451.013392	28409.831545	30.504167
451.580313	28443.223923	30.509184
451.548242	28493.883811	30.514202
452.375800	28530.509687	30.519220
452.593059	28572.319493	30.524237
453.084580	28608.315492	30.529255
453.660272	28664.872771	30.534272
453.914978	28706.108106	30.539290
454.854390	28747.356375	30.544308
454.884857	28797.590039	30.549325
455.508413	28839.817140	30.554343
455.554302	28890.048614	30.559360
456.182627	28938.589784	30.564378
456.439865	28977.126223	30.569396
457.010944	29040.790020	30.574413
457.713378	29067.917065	30.579431
457.999186	29121.708168	30.584448
458.435834	29170.456897	30.589466
458.876332	29217.934611	30.594484
459.221543	29266.868558	30.599501
459.994790	29317.733034	30.604519
460.485843	29371.625386	30.609536
460.869795	29420.187008	30.614554
461.376186	29458.615791	30.619572
461.759677	29516.457099	30.624589
462.312473	29571.313757	30.629607
463.215851	29609.111739	30.634624
463.342740	29655.843119	30.639642
463.790165	29702.341084	30.644660
464.645523	29750.304989	30.649677
465.022352	29791.498087	30.654695
465.485995	29838.126564	30.659712
465.971775	29887.602558	30.664730
466.471090	29925.217881	30.669748
466.787596	29972.261625	30.674765
467.407359	30012.304571	30.679783
467.778907	30059.788704	30.684800
468.146580	30114.808550	30.689818
469.119000	30157.230245	30.694836
468.800185	30192.142247	30.699853
469.649122	30237.358513	30.704871
470.040713	30295.099593	30.709888
470.358958	30332.895733	30.714906
471.117284	30393.348409	30.719924
471.418216	30441.141583	30.724941
471.839710	30489.421699	30.729959
472.474253	30528.211689	30.734976
473.214206	30580.234997	30.739994
473.148614	30625.753391	30.745012
473.509683	30673.227931	30.750029
474.352336	30725.058515	30.755047
474.672294	30776.579166	30.760064
475.086422	30820.328684	30.765082
475.624815	30865.519106	30.770100
476.027785	30916.167372	30.775117
476.707762	30967.790147	30.780135
477.519741	31021.023344	30.785152
477.664417	31069.689535	30.790170
478.458130	31107.627551	30.795188
478.837863	31154.853726	30.800205
479.264886	31201.535263	30.805223
479.816738	31241.894665	30.810240
479.644863	31298.196955	30.815258
480.147281	31348.318643	30.820276
480.715972	31390.350943	30.825293
481.561956	31444.155173	30.830311
481.804873	31484.203097	30.835328
482.114133	31543.009952	30.840346
482.747187	31583.565917	30.845364
483.264454	31624.999857	30.850381
483.502245	31670.593133	30.855399
483.992426	31725.933118	30.860416
484.519447	31765.001457	30.865434
485.106768	31813.713848	30.870452
485.261749	31867.273382	30.875469
486.250769	31919.090345	30.880487
486.803966	31955.518727	30.885504
487.012422	32008.596108	30.890522
487.431202	32050.596324	30.895540
488.167216	32112.119578	30.900557
488.615322	32151.169392	30.905575
489.506679	32207.269670	30.910592
489.635039	32259.671142	30.915610
490.309837	32301.834068	30.920628
490.346516	32350.374757	30.925645
490.748153	32392.188686	30.930663
491.364456	32440.815817	30.935680
491.761936	32508.942872	30.940698
492.843454	32545.921739	30.945716
492.660181	32595.009532	30.950733
493.441287	32645.438402	30.955751
493.993489	32710.248077	30.960768
494.302636	32766.542201	30.965786
494.870708	32806.472189	30.970804
495.299415	32868.500995	30.975821
495.925870	32919.991581	30.980839
496.804250	32968.484057	30.985856
496.938205	33024.060296	30.990874
497.654102	33071.269767	30.995892
497.704150	33125.639231	31.000909
498.481823	33173.123755	31.005927
499.140695	33224.711167	31.010944
499.337742	33280.714438	31.015962
499.735563	33330.844622	31.020980
500.300150	33394.061255	31.025997
501.097556	33445.374619	31.031015
501.318271	33496.677277	31.036032
501.713384	33555.659688	31.041050
502.747062	33608.529678	31.046068
503.206232	33663.658361	31.051085
503.396732	33712.841957	31.056103
504.389073	33767.425868	31.061120
504.552061	33823.005992	31.066138
505.341534	33859.160428	31.071156
505.739566	33923.890513	31.076173
506.257622	33970.519713	31.081191
506.982895	34020.473802	31.086208
507.556729	34072.525511	31.091226
508.117178	34121.146316	31.096244
508.248259	34163.208469	31.101261
509.091438	34207.884190	31.106279
509.420107	34254.322391	31.111296
509.597333	34314.858468	31.116314
510.585545	34363.842769	31.121332
510.514837	34421.288300	31.126349
511.225980	34476.828548	31.131367
511.673949	34532.549260	31.136384
512.110951	34594.139266	31.141402
513.127583	34636.657991	31.146420
513.643689	34689.371497	31.151437
513.781412	34735.726854	31.156455
514.518731	34793.571622	31.161472
514.852480	34847.224555	31.166490
515.279771	34898.472972	31.171508
515.840678	34941.082656	31.176525
516.085671	35006.643017	31.181543
516.820111	35043.054691	31.186560
517.138033	35105.018909	31.191578
517.706451	35147.830163	31.196596
518.164359	35193.346018	31.201613
518.550437	35252.050051	31.206631
519.251254	35303.452615	31.211648
519.617431	35361.040918	31.216666
520.174590	35404.745981	31.221684
520.727385	35457.398744	31.226701
521.217311	35512.811962	31.231719
521.846742	35569.885378	31.236736
521.936799	35622.459276	31.241754
522.721347	35679.755289	31.246772
523.374886	35743.900817	31.251789
523.817464	35796.540068	31.256807
524.143640	35856.804292	31.261824
524.809075	35908.953658	31.266842
525.148582	35968.912604	31.271860
525.609845	36022.542209	31.276877
526.452412	36080.601631	31.281895
527.487038	36138.498344	31.286912
527.563033	36205.277613	31.291930
527.950180	36256.314281	31.296948
528.854862	36311.221994	31.301965
529.436560	36368.899407	31.306983
529.838334	36422.400224	31.312000
530.528853	36485.701207	31.317018
531.019617	36539.491894	31.322036
531.830846	36593.428546	31.327053
531.921600	36640.977855	31.332071
532.836784	36699.988726	31.337088
533.165437	36757.049197	31.342106
533.815574	36814.577981	31.347124
534.584558	36867.750496	31.352141
534.740694	36922.954075	31.357159
535.392256	36978.073878	31.362176
535.678249	37032.612417	31.367194
536.642590	37089.340245	31.372212
536.861968	37142.340264	31.377229
537.268301	37205.827002	31.382247
537.731833	37255.412346	31.387264
538.353357	37314.059879	31.392282
538.867350	37374.577196	31.397300
539.512849	37441.207884	31.402317
539.999183	37503.051507	31.407335
540.855297	37553.221051	31.412352
541.272493	37608.929330	31.417370
541.462835	37674.158640	31.422388
541.993423	37732.359937	31.427405
542.484365	37792.072619	31.432423
543.413150	37844.988556	31.437440
543.783168	37910.854423	31.442458
544.325412	37977.041317	31.447476
545.067282	38039.105729	31.452493
545.590367	38094.760738	31.457511
546.272393	38153.742565	31.462528
546.468344	38218.909408	31.467546
547.183896	38273.415433	31.472564
547.821531	38326.264326	31.477581
548.616904	38382.490837	31.482599
549.093274	38432.386747	31.487616
549.671475	38508.118573	31.492634
550.015732	38559.534213	31.497652
550.634292	38612.197078	31.502669
550.897127	38676.033140	31.507687
551.621154	38717.695192	31.512704
552.160918	38780.318271	31.517722
552.762733	38847.200456	31.522740
553.346910	38894.076687	31.527757
553.741505	38944.473529	31.532775
554.503668	38997.317208	31.537792
554.786252	39046.738970	31.542810
555.169953	39102.431053	31.547828
555.749980	39156.979505	31.552845
556.243341	39226.289293	31.557863
556.658044	39274.628445	31.562880
557.498868	39339.033634	31.567898
558.004886	39398.040098	31.572916
558.472940	39448.116726	31.577933
558.941989	39508.849434	31.582951
559.840911	39570.444631	31.587968
560.104887	39638.027228	31.592986
560.411376	39702.447618	31.598004
561.113931	39761.841683	31.603021
561.570719	39832.752827	31.608039
562.472252	39899.009485	31.613056
563.043316	39961.245291	31.618074
563.494114	40024.859827	31.623092
563.889091	40082.038855	31.628109
564.660997	40149.771161	31.633127
565.531037	40211.967183	31.638144
565.850376	40277.494015	31.643162
566.433546	40345.541084	31.648180
566.923367	40415.133484	31.653197
567.515766	40473.730898	31.658215
567.991551	40538.399191	31.663232
568.485929	40609.174159	31.668250
569.286064	40668.062106	31.673268
570.097765	40729.756461	31.678285
570.601120	40803.161627	31.683303
570.682468	40860.783931	31.688320
571.416737	40934.197642	31.693338
572.247567	40997.300125	31.698356
573.017863	41062.322286	31.703373
573.629357	41137.419267	31.708391
574.367309	41207.133438	31.713408
574.572660	41266.856128	31.718426
575.406693	41322.938723	31.723444
575.940636	41381.490802	31.728461
576.309839	41447.626816	31.733479
576.690886	41507.436488	31.738496
577.484377	41571.969527	31.743514
578.131993	41642.578363	31.748532
578.928274	41716.117799	31.753549
578.990478	41781.177093	31.758567
579.937894	41837.711279	31.763584
580.536612	41912.262654	31.768602
580.775424	41968.731061	31.773620
581.388575	42028.138956	31.778637
581.967589	42096.242708	31.783655
582.958492	42179.423917	31.788672
583.758231	42237.089111	31.793690
584.177788	42299.424861	31.798708
585.038471	42353.304842	31.803725
585.597625	42416.359075	31.808743
585.750263	42484.018481	31.813760
586.626374	42535.992677	31.818778
587.124229	42602.276458	31.823796
587.873511	42661.443364	31.828813
588.376181	42734.178304	31.833831
588.833081	42793.650683	31.838848
589.232421	42858.723600	31.843866
589.844989	42925.142184	31.848884
590.202194	42980.184138	31.853901
590.481833	43053.619194	31.858919
591.312113	43107.923235	31.863936
592.189155	43167.090460	31.868954
592.528591	43228.745609	31.873972
593.371481	43290.214551	31.878989
593.827181	43357.898738	31.884007
594.338699	43420.046135	31.889024
594.981382	43482.211115	31.894042
595.321066	43543.380054	31.899060
596.152306	43602.454410	31.904077
596.249001	43677.425598	31.909095
597.172789	43741.957221	31.914112
597.598660	43807.376657	31.919130
598.078931	43880.384527	31.924148
598.848692	43946.269192	31.929165
599.074718	44021.290861	31.934183
599.650472	44096.030295	31.939200
600.579462	44172.700847	31.944218
600.974079	44239.771063	31.949236
601.805665	44303.350958	31.954253
602.415649	44380.597202	31.959271
603.064383	44456.439702	31.964288
603.694058	44526.250872	31.969306
604.014824	44606.857780	31.974324
605.025675	44681.467775	31.979341
605.322446	44762.483840	31.984359
606.029676	44831.531069	31.989376
606.861955	44895.485754	31.994394
607.159994	44972.903086	31.999412
608.106717	45048.694599	32.004429
608.762713	45123.987890	32.009447
609.339531	45199.451977	32.014464
610.164861	45272.404027	32.019482
610.444699	45348.509748	32.024500
611.077664	45409.435438	32.029517
611.685541	45490.316847	32.034535
612.318095	45561.933652	32.039552
612.810640	45634.053378	32.044570
613.473752	45714.870011	32.049588
613.951832	45789.775890	32.054605
614.965433	45869.500739	32.059623
615.247731	45945.418316	32.064640
616.553405	46004.348806	32.069658
617.156572	46084.613145	32.074676
617.470866	46156.566355	32.079693
618.358650	46226.658692	32.084711
618.745467	46290.332857	32.089728
619.555515	46364.783789	32.094746
620.130227	46437.456237	32.099764
620.737580	46510.446439	32.104781
621.729507	46583.863759	32.109799
622.027443	46657.465919	32.114816
622.882975	46720.081010	32.119834
623.248384	46788.434966	32.124852
623.639432	46865.749343	32.129869
624.402079	46941.367293	32.134887
624.858497	47011.852261	32.139904
625.876893	47085.754186	32.144922
626.286697	47160.510819	32.149940
627.090024	47231.536810	32.154957
627.742545	47302.346242	32.159975
627.864838	47369.898624	32.164992
628.925566	47446.420528	32.170010
629.293464	47521.184912	32.175028
630.188488	47591.919309	32.180045
630.853278	47666.726244	32.185063
631.184975	47737.796049	32.190080
632.160408	47815.161318	32.195098
632.575697	47872.762060	32.200116
633.718811	47938.492393	32.205133
634.244895	47998.106907	32.210151
634.902658	48054.411156	32.215168
635.569854	48114.579591	32.220186
635.794638	48191.329818	32.225204
636.530581	48248.640882	32.230221
637.079325	48315.262537	32.235239
637.675597	48390.379930	32.240256
638.525134	48445.408765	32.245274
639.079652	48518.502266	32.250292
639.521991	48577.562010	32.255309
640.171666	48658.226744	32.260327
640.698651	48720.367358	32.265344
641.584921	48783.641298	32.270362
642.155068	48860.871131	32.275380
642.381321	48927.412214	32.280397
643.343181	49005.030387	32.285415
643.809089	49083.219987	32.290432
644.297792	49149.910417	32.295450
644.969486	49230.738216	32.300468
645.703592	49309.164965	32.305485
646.463038	49383.228778	32.310503
646.581966	49461.828313	32.315520
647.444507	49531.884171	32.320538
648.367674	49619.836057	32.325556
648.695223	49703.560224	32.330573
649.585394	49781.192249	32.335591
650.126250	49864.959521	32.340608
650.870938	49934.699730	32.345626
651.637440	50023.639406	32.350644
652.343353	50095.474110	32.355661
652.669230	50175.910163	32.360679
653.748580	50265.864734	32.365696
654.300901	50326.512516	32.370714
654.849826	50421.827615	32.375732
655.672714	50513.164677	32.380749
656.607844	50578.992102	32.385767
656.982859	50652.506458	32.390784
658.077261	50738.139000	32.395802
658.305840	50815.296006	32.400820
659.240156	50889.210724	32.405837
659.813643	50972.097401	32.410855
660.373611	51039.573051	32.415872
661.347270	51122.302686	32.420890
661.832604	51200.331904	32.425908
662.429869	51276.205188	32.430925
663.152750	51353.856040	32.435943
663.976181	51434.534914	32.440960
664.929647	51514.592593	32.445978
665.277281	51582.868700	32.450996
666.126724	51652.926711	32.456013
666.863194	51734.733890	32.461031
667.300943	51799.896024	32.466048
668.124415	51878.387095	32.471066
668.507211	51961.262869	32.476084
669.461122	52042.195503	32.481101
670.273037	52112.944159	32.486119
670.341564	52189.251243	32.491136
671.323432	52265.105483	32.496154
671.755210	52334.300782	32.501172
672.566928	52417.471682	32.506189
673.107428	52499.090760	32.511207
673.379260	52576.626489	32.516224
674.208603	52658.226198	32.521242
675.094228	52738.988434	32.526260
675.797351	52825.379665	32.531277
676.123634	52901.452539	32.536295
676.837627	52986.697320	32.541312
677.724434	53057.829434	32.546330
678.352687	53137.450031	32.551348
678.870788	53204.077899	32.556365
679.944871	53269.929138	32.561383
680.318230	53350.931904	32.566400
681.004970	53432.822415	32.571418
681.810391	53497.577326	32.576436
682.435883	53575.029327	32.581453
683.433768	53663.155658	32.586471
683.690075	53734.464497	32.591488
684.178624	53807.262255	32.596506
685.009334	53897.807667	32.601524
685.628025	53973.015556	32.606541
686.480947	54047.244106	32.611559
686.991819	54133.094384	32.616576
687.954794	54213.678710	32.621594
688.482731	54296.932345	32.626612
689.079818	54378.916120	32.631629
690.093202	54454.348502	32.636647
690.610353	54546.103578	32.641664
691.282833	54628.715570	32.646682
691.792553	54711.967189	32.651700
692.275554	54791.616115	32.656717
693.301377	54881.236109	32.661735
693.836820	54967.737389	32.666752
694.974091	55057.505134	32.671770
695.294871	55135.649138	32.676788
696.271396	55219.462278	32.681805
696.920314	55303.776342	32.686823
697.654510	55402.398805	32.691840
698.170072	55480.222324	32.696858
699.102150	55567.821796	32.701876
699.297150	55651.777835	32.706893
700.360157	55742.812859	32.711911
701.400389	55841.022151	32.716928
702.019475	55920.058650	32.721946
702.995775	55996.457366	32.726964
703.535329	56085.734027	32.731981
703.879213	56173.035455	32.736999
704.947105	56261.002256	32.742016
705.732683	56347.216220	32.747034
706.702224	56431.597976	32.752052
707.314203	56510.517293	32.757069
707.747572	56585.072625	32.762087
707.906856	56672.069351	32.767104
708.912576	56757.250355	32.772122
709.796806	56844.362017	32.777140
710.401663	56940.333951	32.782157
710.933167	57037.178493	32.787175
711.601530	57117.027660	32.792192
712.316974	57203.306315	32.797210
713.295904	57288.284540	32.802228
713.903785	57382.093235	32.807245
714.648476	57463.513861	32.812263
715.326256	57570.881879	32.817280
716.610483	57655.693338	32.822298
717.339459	57741.971803	32.827316
717.343418	57827.148915	32.832333
718.559535	57915.231475	32.837351
719.056187	58012.768946	32.842368
719.779016	58085.410144	32.847386
720.573212	58176.825616	32.852404
720.811150	58272.119785	32.857421
721.699427	58353.400668	32.862439
722.640575	58450.560158	32.867456
723.510523	58532.698973	32.872474
723.915490	58624.031511	32.877492
724.484191	58706.192772	32.882509
725.302747	58789.897537	32.887527
726.007597	58879.671343	32.892544
726.742229	58969.086367	32.897562
727.327175	59045.587690	32.902580
727.960187	59136.848464	32.907597
728.784390	59218.300516	32.912615
729.245023	59312.006822	32.917632
729.858159	59410.645666	32.922650
730.833362	59504.987374	32.927668
731.783516	59593.668353	32.932685
732.502383	59684.632900	32.937703
732.789094	59771.430910	32.942720
733.424982	59863.845954	32.947738
734.549280	59957.969844	32.952756
734.892222	60058.008173	32.957773
735.763253	60143.677920	32.962791
736.352490	60253.268079	32.967808
737.724630	60349.380197	32.972826
737.905813	60444.552483	32.977844
738.499938	60542.451943	32.982861
739.163014	60642.094378	32.987879
740.103473	60745.105607	32.992896
741.065172	60840.828171	32.997914
741.799429	60933.478707	33.002932
742.647167	61048.855508	33.007949
743.579295	61136.177609	33.012967
744.219629	61242.301651	33.017984
745.037672	61343.087384	33.023002
746.053444	61434.322091	33.028020
746.550098	61531.588747	33.033037
747.620722	61620.391114	33.038055
748.014978	61728.758672	33.043072
748.755556	61818.265444	33.048090
749.921464	61919.885282	33.053108
750.407585	62016.573112	33.058125
751.467775	62108.487018	33.063143
752.192238	62209.658092	33.068160
752.708545	62311.843376	33.073178
753.689842	62404.543033	33.078196
754.059403	62502.694329	33.083213
755.085725	62593.741745	33.088231
755.640465	62704.886468	33.093248
756.479611	62792.532833	33.098266
757.313786	62897.209252	33.103284
758.028450	63003.867282	33.108301
759.076334	63092.380945	33.113319
759.692882	63191.059691	33.118336
760.497824	63280.435036	33.123354
761.122266	63383.500391	33.128372
761.936632	63486.219899	33.133389
762.714550	63582.254041	33.138407
763.498640	63677.964721	33.143424
764.329816	63777.333865	33.148442
765.397107	63870.228087	33.153460
766.259841	63967.427938	33.158477
766.553891	64060.906097	33.163495
767.156045	64163.541328	33.168512
767.456869	64259.994639	33.173530
768.975151	64354.776254	33.178548
769.809092	64470.550926	33.183565
770.749613	64552.312531	33.188583
771.658943	64658.491295	33.193600
772.180050	64752.911429	33.198618
773.191408	64840.626626	33.203636
773.764047	64950.632598	33.208653
774.221757	65038.200933	33.213671
775.500097	65129.186445	33.218688
775.858609	65222.931053	33.223706
776.673770	65307.462418	33.228724
777.278123	65408.988103	33.233741
778.031117	65489.997055	33.238759
779.051961	65575.111224	33.243776
779.686677	65678.146377	33.248794
780.841410	65758.536135	33.253812
780.870982	65857.956702	33.258829
781.809153	65944.104382	33.263847
782.578074	66044.790111	33.268864
783.092241	66137.924917	33.273882
783.777234	66243.847889	33.278900
784.703321	66342.180261	33.283917
785.560716	66441.878680	33.288935
786.562255	66547.664708	33.293952
787.304267	66650.288118	33.298970
788.219667	66747.287798	33.303988
788.945267	66850.566722	33.309005
789.723595	66953.527564	33.314023
790.450078	67052.906970	33.319040
791.010680	67146.766310	33.324058
791.890887	67257.975080	33.329076
792.448301	67365.942453	33.334093
793.312299	67469.246521	33.339111
794.043775	67578.409533	33.344128
794.621582	67695.385028	33.349146
795.832726	67797.034142	33.354164
796.820005	67911.717744	33.359181
797.460057	68017.085236	33.364199
798.243614	68120.822416	33.369216
798.919733	68230.452751	33.374234
799.850659	68340.721157	33.379252
800.280529	68454.069796	33.384269
801.230984	68563.918195	33.389287
802.571011	68676.536422	33.394304
802.842525	68785.181372	33.399322
803.579322	68895.799143	33.404340
804.194377	69010.868846	33.409357
805.362735	69119.685027	33.414375
806.532125	69232.889613	33.419392
807.507882	69355.718113	33.424410
808.226818	69463.042087	33.429428
808.896486	69570.203252	33.434445
809.961837	69679.525485	33.439463
810.700558	69770.048420	33.444480
811.498447	69899.315506	33.449498
812.353066	70003.967267	33.454516
813.553809	70113.783033	33.459533
814.303449	70224.125825	33.464551
815.364381	70316.601205	33.469568
815.863934	70425.426260	33.474586
816.829030	70523.755797	33.479604
817.315712	70643.310796	33.484621
818.270955	70746.341347	33.489639
819.349407	70845.452226	33.494656
819.827983	70954.624715	33.499674
820.780739	71050.209870	33.504692
821.891269	71166.313346	33.509709
822.563543	71273.088465	33.514727
823.529345	71370.509181	33.519744
823.985437	71470.593769	33.524762
824.990470	71575.405566	33.529780
825.458354	71673.804604	33.534797
826.561324	71790.063999	33.539815
827.739871	71895.103204	33.544832
827.986696	72006.000836	33.549850
829.028024	72106.084851	33.554868
829.570256	72209.464443	33.559885
830.462649	72322.440784	33.564903
831.314161	72415.893596	33.569920
832.553413	72517.620039	33.574938
832.932886	72622.483282	33.579956
833.732436	72713.006828	33.584973
834.561745	72809.263639	33.589991
835.622400	72917.124506	33.595008
836.162944	73022.635398	33.600026
837.009019	73113.710324	33.605044
838.003196	73229.651090	33.610061
838.514023	73333.660611	33.615079
839.327781	73440.890961	33.620096
839.933273	73547.445047	33.625114
841.099540	73655.330366	33.630132
842.008999	73761.331059	33.635149
842.394725	73864.893586	33.640167
843.550104	73980.850371	33.645184
844.057982	74098.517686	33.650202
844.907999	74213.547979	33.655220
846.016259	74327.195675	33.660237
846.829744	74450.921954	33.665255
847.961997	74561.678902	33.670272
848.842869	74682.001031	33.675290
849.349071	74787.600258	33.680308
850.254595	74904.562832	33.685325
851.189966	75009.487719	33.690343
852.115111	75135.733034	33.695360
852.861643	75265.502994	33.700378
853.481572	75369.034638	33.705396
854.636105	75492.408287	33.710413
855.105292	75614.977779	33.715431
856.399297	75729.869021	33.720448
857.022639	75857.938373	33.725466
858.005087	75976.958304	33.730484
859.052518	76095.233875	33.735501
859.773915	76204.503808	33.740519
861.167919	76327.235722	33.745536
861.751371	76442.823949	33.750554
862.735149	76562.669627	33.755572
863.556491	76679.425028	33.760589
864.521021	76811.600430	33.765607
865.382471	76915.125483	33.770624
866.377111	77037.758452	33.775642
867.004870	77145.045304	33.780660
868.065680	77263.716555	33.785677
869.106338	77381.061340	33.790695
869.559063	77493.279466	33.795712
870.566423	77615.418978	33.800730
871.381636	77732.483866	33.805748
872.223790	77856.208498	33.810765
873.254659	77970.428295	33.815783
874.237059	78093.587301	33.820800
874.947443	78205.261256	33.825818
875.825890	78326.841370	33.830836
876.755846	78447.159778	33.835853
877.534724	78572.126373	33.840871
878.816179	78691.833394	33.845888
879.285268	78804.434355	33.850906
880.261955	78923.632681	33.855924
881.482854	79037.839810	33.860941
881.793761	79157.700817	33.865959
882.954201	79267.053546	33.870976
883.752644	79379.136523	33.875994
884.600688	79498.927565	33.881012
885.563038	79629.254495	33.886029
886.164138	79757.370841	33.891047
887.262576	79868.420628	33.896064
887.725439	79993.949871	33.901082
888.508215	80107.355824	33.906100
889.805131	80225.496053	33.911117
890.505988	80349.051228	33.916135
891.409638	80456.447084	33.921152
892.429720	80578.724359	33.926170
893.051732	80689.966037	33.931188
894.037948	80803.140244	33.936205
894.839516	80917.230691	33.941223
896.224561	81033.523442	33.946240
897.112626	81154.544266	33.951258
897.565479	81272.238268	33.956276
898.752513	81382.279278	33.961293
899.172519	81509.000301	33.966311
899.995759	81629.602542	33.971328
901.028730	81745.522586	33.976346
901.710253	81878.209874	33.981364
902.891179	82001.380387	33.986381
903.750958	82127.085066	33.991399
904.708767	82245.666985	33.996416
905.840364	82393.680480	34.001434
906.625419	82511.276940	34.006452
907.662541	82633.142336	34.011469
908.617534	82759.544448	34.016487
909.397999	82884.200585	34.021504
910.156111	83017.071260	34.026522
910.974154	83147.741162	34.031540
912.195537	83270.847493	34.036557
912.894495	83398.382202	34.041575
913.895543	83531.065183	34.046592
914.902471	83666.598790	34.051610
915.599801	83796.124842	34.056628
916.569741	83925.355376	34.061645
917.477202	84061.894758	34.066663
918.254028	84190.903305	34.071680
919.395543	84326.127520	34.076698
920.209255	84456.956123	34.081716
921.049778	84597.297202	34.086733
922.260083	84734.109135	34.091751
922.977228	84867.007465	34.096768
923.805624	85004.146575	34.101786
924.640135	85153.969503	34.106804
925.784721	85277.121798	34.111821
926.889320	85421.860562	34.116839
927.701133	85556.559269	34.121856
928.772065	85695.222285	34.126874
929.548276	85835.440048	34.131892
930.861862	85968.072631	34.136909
931.673035	86103.661001	34.141927
932.491702	86227.273856	34.146944
933.671683	86372.068905	34.151962
933.917709	86509.813185	34.156980
935.086608	86647.160170	34.161997
936.184128	86797.583982	34.167015
937.217787	86933.166709	34.172032
937.812733	87072.240273	34.177050
938.872995	87216.906178	34.182068
940.085654	87352.260056	34.187085
941.074186	87487.953789	34.192103
942.034525	87625.502751	34.197120
942.942354	87768.015559	34.202138
943.682977	87899.225888	34.207156
945.159166	88029.396521	34.212173
945.958464	88172.549237	34.217191
946.752932	88308.188418	34.222208
948.001077	88436.242168	34.227226
948.776529	88576.004237	34.232244
949.859287	88699.003171	34.237261
950.779255	88842.659821	34.242279
951.468505	88974.035029	34.247296
952.751137	89102.757929	34.252314
953.388463	89225.043046	34.257332
954.363113	89340.546346	34.262349
955.235903	89477.674043	34.267367
956.274332	89599.644425	34.272384
957.477672	89720.803733	34.277402
957.919419	89861.042299	34.282420
958.910654	89981.652893	34.287437
959.819639	90113.011376	34.292455
961.158840	90252.845110	34.297472
961.996011	90377.524311	34.302490
962.575900	90505.653551	34.307508
964.049841	90642.350257	34.312525
964.703614	90785.512935	34.317543
965.761224	90919.056920	34.322560
966.680637	91048.529438	34.327578
967.422513	91186.027624	34.332596
968.636403	91324.466459	34.337613
969.384383	91466.096717	34.342631
970.190957	91611.672817	34.347648
971.463584	91752.943435	34.352666
972.423969	91892.882097	34.357684
973.521149	92031.139639	34.362701
974.552139	92175.504582	34.367719
975.260749	92316.891477	34.372736
976.535606	92456.352556	34.377754
977.095646	92608.816288	34.382772
978.425284	92746.559039	34.387789
979.534111	92895.959725	34.392807
980.285194	93037.064454	34.397824
981.424979	93176.549962	34.402842
982.099353	93323.321006	34.407860
983.014502	93474.808170	34.412877
984.240706	93620.619656	34.417895
985.082731	93777.481304	34.422912
986.523217	93920.890414	34.427930
987.194319	94066.512066	34.432948
988.278627	94217.811614	34.437965
988.934275	94364.286331	34.442983
990.051670	94528.473050	34.448000
990.998990	94665.536389	34.453018
992.162260	94829.071065	34.458036
993.086327	94974.429211	34.463053
994.047968	95133.573272	34.468071
994.945400	95287.974800	34.473088
996.248549	95444.595210	34.478106
997.215513	95596.566300	34.483124
998.510238	95732.692625	34.488141
999.617160	95888.306555	34.493159
1000.547813	96043.340406	34.498176
1001.453713	96189.036617	34.503194
1002.484471	96346.223899	34.508212
1003.638093	96488.396768	34.513229
1004.744187	96639.717311	34.518247
1005.407226	96787.862807	34.523264
1006.595225	96933.923935	34.528282
1007.129019	97088.391241	34.533300
1008.449622	97233.913257	34.538317
1009.264383	97384.535062	34.543335
1010.146638	97545.389734	34.548352
1011.362591	97701.768804	34.553370
1012.078507	97855.057744	34.558388
1012.914125	98007.821607	34.563405
1014.513610	98165.359879	34.568423
1015.147347	98321.490870	34.573440
1016.195004	98477.697264	34.578458
1017.282219	98635.140578	34.583476
1018.863965	98782.264120	34.588493
1019.591794	98932.412430	34.593511
1020.303798	99070.824794	34.598528
1021.364786	99218.044542	34.603546
1022.122274	99363.892618	34.608564
1023.280423	99509.298301	34.613581
1024.534512	99663.918815	34.618599
1025.313372	99801.423746	34.623616
1026.277589	99948.040776	34.628634
1027.303360	100109.912714	34.633652
1028.369529	100259.747992	34.638669
1029.466296	100408.552270	34.643687
1030.025084	100567.317483	34.648704
1031.250716	100719.652800	34.653722
1032.386806	100884.376522	34.658740
1033.559428	101041.361770	34.663757
1034.439252	101202.171678	34.668775
1035.396843	101360.852953	34.673792
1036.606214	101516.566914	34.678810
1037.196364	101678.400732	34.683828
1038.261453	101831.374916	34.688845
1039.581325	102003.314805	34.693863
1040.145819	102166.207344	34.698880
1041.767751	102327.895490	34.703898
1042.472596	102503.585689	34.708916
1043.406543	102677.846300	34.713933
1044.708485	102842.325647	34.718951
1045.492129	103009.118420	34.723968
1046.959669	103177.174269	34.728986
1047.745123	103352.830984	34.734004
1048.700259	103508.835032	34.739021
1049.879682	103686.815469	34.744039
1050.933788	103864.917906	34.749056
1052.328730	104017.115138	34.754074
1053.020115	104200.905694	34.759092
1054.362534	104369.659132	34.764109
1055.148322	104545.575640	34.769127
1056.408285	104727.149924	34.774144
1057.532438	104896.307879	34.779162
1058.609775	105063.711556	34.784180
1059.801975	105238.617084	34.789197
1061.185470	105401.815591	34.794215
1061.937152	105581.546735	34.799232
1063.446027	105743.700199	34.804250
1064.693462	105917.357961	34.809268
1065.542753	106083.686548	34.814285
1066.534242	106251.413842	34.819303
1067.326658	106425.792112	34.824320
1068.610910	106575.723099	34.829338
1069.920438	106759.354666	34.834356
1071.057749	106921.711385	34.839373
1072.285949	107088.391301	34.844391
1073.263296	107265.141462	34.849408
1074.647620	107418.725089	34.854426
1075.524495	107590.154193	34.859444
1076.588287	107744.043062	34.864461
1077.950455	107906.749635	34.869479
1078.949331	108077.895764	34.874496
1079.978891	108238.398813	34.879514
1080.694007	108402.895553	34.884532
1082.060676	108576.433947	34.889549
1083.031246	108726.448752	34.894567
1083.982289	108912.088057	34.899584
1085.410832	109070.668376	34.904602
1086.600189	109234.435379	34.909620
1087.407651	109394.382510	34.914637
1088.667732	109559.851914	34.919655
1089.274323	109727.859209	34.924672
1090.315125	109887.061901	34.929690
1091.282733	110050.829384	34.934708
1092.440919	110206.527764	34.939725
1093.670365	110358.981898	34.944743
1094.459082	110528.118505	34.949760
1095.726745	110690.129965	34.954778
1096.690569	110846.051813	34.959796
1097.640819	111010.650763	34.964813
1098.590399	111165.853386	34.969831
1099.791317	111331.606661	34.974848
1101.093552	111505.359799	34.979866
1101.979323	111675.171486	34.984884
1103.009133	111839.317934	34.989901
1104.550210	112005.680546	34.994919
1105.337487	112183.385626	34.999936
1106.452355	112348.104464	35.004954
1107.419684	112513.468583	35.009972
1108.479445	112694.291405	35.014989
1109.897907	112862.680981	35.020007
1110.740498	113040.711368	35.025024
1111.816288	113219.175372	35.030042
1113.005792	113397.622452	35.035060
1113.895333	113578.501702	35.040077
1115.393801	113757.193876	35.045095
1116.226140	113941.596987	35.050112
1117.554564	114119.100013	35.055130
1118.396175	114303.034231	35.060148
1119.382118	114483.750678	35.065165
1121.010986	114671.698132	35.070183
1122.326847	114851.616441	35.075200
1123.611757	115022.522778	35.080218
1124.373413	115210.380455	35.085236
1125.409062	115395.786374	35.090253
1127.117236	115574.835063	35.095271
1127.697463	115764.043018	35.100288
1129.068774	115940.203668	35.105306
1130.634903	116122.257844	35.110324
1131.340894	116305.436887	35.115341
1132.916918	116487.085422	35.120359
1133.942975	116671.573300	35.125376
1135.024834	116844.206737	35.130394
1136.191814	117026.746374	35.135412
1137.513556	117201.576249	35.140429
1138.696816	117382.973519	35.145447
1139.792517	117572.693379	35.150464
1141.103354	117747.032818	35.155482
1142.347533	117928.740275	35.160500
1143.456496	118114.338443	35.165517
1144.373356	118274.002989	35.170535
1145.310754	118465.261525	35.175552
1146.701586	118647.368043	35.180570
1147.878213	118825.817806	35.185588
1148.994221	119012.015414	35.190605
1150.128398	119189.408024	35.195623
1151.432835	119366.812854	35.200640
1152.517118	119546.853321	35.205658
1153.662542	119727.595402	35.210676
1154.724236	119909.416959	35.215693
1156.084091	120095.581642	35.220711
1157.049369	120276.354496	35.225728
1158.330201	120452.486844	35.230746
1159.835613	120646.419941	35.235764
1160.242230	120823.629524	35.240781
1161.920113	121002.010885	35.245799
1162.795516	121196.628867	35.250816
1163.757949	121371.128089	35.255834
1165.318408	121549.225887	35.260852
1166.341477	121737.924782	35.265869
1167.411435	121911.115668	35.270887
1168.692621	122088.841016	35.275904
1169.554888	122255.621715	35.280922
1170.909385	122427.793541	35.285940
1171.966748	122603.869066	35.290957
1173.279445	122769.807594	35.295975
1173.979811	122951.268539	35.300992
1175.025925	123121.931312	35.306010
1176.227788	123309.201590	35.311028
1177.235282	123487.039482	35.316045
1178.505232	123666.308651	35.321063
1180.003450	123858.634870	35.326080
1180.925169	124049.821713	35.331098
1182.097854	124223.717012	35.336116
1183.245972	124416.658901	35.341133
1184.234376	124609.969246	35.346151
1185.684579	124794.784500	35.351168
1187.039593	124979.501322	35.356186
1188.120502	125171.036457	35.361204
1189.034038	125372.227754	35.366221
1190.340329	125559.403336	35.371239
1191.774702	125763.077712	35.376256
1192.915495	125951.448169	35.381274
1193.918745	126148.290398	35.386292
1195.115647	126351.763829	35.391309
1196.341888	126545.172985	35.396327
1197.377658	126734.641858	35.401344
1198.447713	126942.426245	35.406362
1200.155458	127139.645027	35.411380
1201.162532	127339.245430	35.416397
1202.411331	127536.220767	35.421415
1203.576224	127750.071507	35.426432
1204.817700	127956.996774	35.431450
1206.176150	128154.059361	35.436468
1207.236565	128362.309088	35.441485
1208.711259	128571.205493	35.446503
1210.181154	128766.071259	35.451520
1211.263095	128955.403428	35.456538
1212.607640	129168.332448	35.461556
1213.435437	129361.918527	35.466573
1215.037478	129563.529839	35.471591
1215.844047	129768.628915	35.476608
1217.288943	129976.192007	35.481626
1218.664218	130172.056014	35.486644
1219.837506	130377.938013	35.491661
1221.112772	130583.322890	35.496679
1222.152165	130800.253823	35.501696
1223.541898	131005.127956	35.506714
1225.177339	131193.025760	35.511732
1226.360920	131397.337676	35.516749
1227.267276	131603.838291	35.521767
1228.075756	131815.126065	35.526784
1229.710681	132011.884033	35.531802
1231.512232	132208.769068	35.536820
1232.826854	132420.348507	35.541837
1233.801402	132612.263994	35.546855
1234.873539	132821.929272	35.551872
1235.930963	133018.452259	35.556890
1237.794813	133206.145329	35.561908
1238.804578	133420.594224	35.566925
1239.969671	133617.762843	35.571943
1241.005125	133820.002863	35.576960
1242.320475	134025.968644	35.581978
1244.189238	134220.314315	35.586996
1244.583139	134429.852273	35.592013
1246.034725	134626.231839	35.597031
1247.591847	134831.376746	35.602048
1248.608083	135027.838908	35.607066
1250.093836	135229.938666	35.612084
1251.059417	135421.055533	35.617101
1252.183759	135607.402468	35.622119
1253.456420	135796.531349	35.627136
1254.542298	135986.705425	35.632154
1255.720791	136174.924275	35.637172
1256.890943	136373.385826	35.642189
1258.232322	136570.121001	35.647207
1259.643918	136764.967930	35.652224
1261.222073	136960.551006	35.657242
1262.200132	137148.348389	35.662260
1263.581069	137353.811411	35.667277
1264.589452	137555.412434	35.672295
1265.928318	137752.559127	35.677312
1266.963017	137949.310114	35.682330
1268.468624	138145.569438	35.687348
1269.881777	138349.508990	35.692365
1270.583739	138552.253655	35.697383
1272.103969	138763.640165	35.702400
1273.140758	138979.088104	35.707418
1274.626858	139187.791484	35.712436
1275.931778	139404.798397	35.717453
1277.405992	139608.924200	35.722471
1278.906886	139819.087467	35.727488
1279.852150	140033.095096	35.732506
1281.344671	140232.080958	35.737524
1282.440039	140446.219228	35.742541
1283.694454	140651.627599	35.747559
1284.986849	140871.016333	35.752576
1286.284929	141086.369433	35.757594
1287.384010	141304.330929	35.762612
1288.525008	141517.641892	35.767629
1289.923020	141731.535426	35.772647
1291.211722	141962.275592	35.777664
1292.139367	142182.399984	35.782682
1293.673150	142400.615617	35.787700
1294.817246	142621.583800	35.792717
1296.332096	142850.173274	35.797735
1297.864712	143076.819222	35.802752
1299.199582	143304.842471	35.807770
1300.589330	143526.829645	35.812788
1301.955765	143755.878043	35.817805
1303.408793	143976.994279	35.822823
1304.833772	144198.725090	35.827840
1306.061827	144411.565324	35.832858
1307.444201	144635.068897	35.837876
1308.423571	144846.160332	35.842893
1309.904038	145078.344513	35.847911
1311.332376	145305.511849	35.852928
1312.519984	145522.741856	35.857946
1314.028771	145742.676717	35.862964
1315.373348	145970.469349	35.867981
1316.858938	146200.271687	35.872999
1318.456098	146407.490562	35.878016
1319.701428	146624.703503	35.883034
1321.352226	146836.586511	35.888052
1322.518464	147048.063919	35.893069
1323.698555	147279.619668	35.898087
1325.165342	147489.071777	35.903104
1326.158256	147700.820120	35.908122
1327.901528	147914.647703	35.913140
1328.913945	148139.925212	35.918157
1330.388497	148361.475805	35.923175
1331.738546	148572.981354	35.928192
1332.894348	148795.573702	35.933210
1334.177739	149009.604625	35.938228
1335.923473	149227.701965	35.943245
1336.803361	149446.138817	35.948263
1338.366401	149662.997216	35.953280
1339.419408	149858.002487	35.958298
1341.201515	150060.269106	35.963316
1342.468225	150272.060963	35.968333
1343.660975	150469.534447	35.973351
1345.191727	150672.756613	35.978368
1346.248528	150877.475390	35.983386
1347.615090	151078.147999	35.988404
1348.559506	151286.440068	35.993421
1349.792110	151503.281361	35.998439
1351.229303	151718.555554	36.003456
1352.681678	151934.907169	36.008474
1353.631998	152146.083015	36.013492
1355.193267	152364.627964	36.018509
1356.083071	152584.954458	36.023527
1357.804663	152801.838517	36.028544
1358.632742	153031.150989	36.033562
1359.814549	153258.479541	36.038580
1361.047354	153495.740443	36.043597
1362.557112	153743.837811	36.048615
1364.148457	153966.954132	36.053632
1365.405382	154216.299073	36.058650
1367.062278	154440.079770	36.063668
1368.596719	154691.858713	36.068685
1369.773292	154914.726284	36.073703
1371.094763	155156.448589	36.078720
1372.530634	155391.933716	36.083738
1373.783130	155635.192139	36.088756
1375.551007	155871.769737	36.093773
1376.191967	156119.505511	36.098791
1377.742231	156356.588823	36.103808
1379.186781	156607.971174	36.108826
1380.796696	156858.820915	36.113844
1382.357131	157107.927575	36.118861
1383.244798	157347.454400	36.123879
1385.268801	157589.838396	36.128896
1386.407305	157842.149793	36.133914
1387.919465	158085.022138	36.138932
1389.350181	158330.663033	36.143949
1390.670858	158581.590619	36.148967
1392.617451	158826.568788	36.153984
1393.687656	159077.816908	36.159002
1394.925713	159329.166732	36.164020
1396.390284	159573.944030	36.169037
1397.518969	159830.543484	36.174055
1399.259161	160080.776736	36.179072
1400.805597	160325.493394	36.184090
1402.217310	160568.886369	36.189108
1403.228952	160811.670040	36.194125
1404.802907	161066.859123	36.199143
1406.608304	161316.414212	36.204160
1407.895871	161572.691198	36.209178
1409.335866	161826.368108	36.214196
1411.005514	162074.982527	36.219213
1412.346217	162318.050512	36.224231
1414.069012	162562.468851	36.229248
1415.277744	162815.931928	36.234266
1416.835126	163059.705138	36.239284
1418.523585	163309.159273	36.244301
1419.563929	163556.735207	36.249319
1421.238739	163803.831875	36.254336
1422.431059	164048.884718	36.259354
1424.283479	164283.551176	36.264372
1425.619908	164528.481655	36.269389
1427.052218	164776.292788	36.274407
1428.593254	165006.465223	36.279424
1429.773939	165257.237677	36.284442
1431.277716	165493.943570	36.289460
1432.694806	165728.797463	36.294477
1434.036707	165968.082338	36.299495
1435.745509	166187.084916	36.304512
1436.927729	166427.564469	36.309530
1438.233776	166644.320746	36.314548
1439.816312	166863.599163	36.319565
1440.761588	167092.297446	36.324583
1442.500487	167323.576678	36.329600
1443.915181	167564.696694	36.334618
1445.026828	167790.552504	36.339636
1446.592319	168033.707414	36.344653
1447.742862	168264.916754	36.349671
1448.944943	168508.041283	36.354688
1450.462711	168754.126429	36.359706
1451.907547	168993.659424	36.364724
1453.400177	169245.717823	36.369741
1454.638862	169501.410150	36.374759
1456.092031	169749.324482	36.379776
1457.420143	170007.074230	36.384794
1458.581587	170262.273406	36.389812
1460.382064	170512.434160	36.394829
1461.606225	170788.233170	36.399847
1463.522338	171050.935383	36.404864
1464.585512	171314.559262	36.409882
1466.225491	171580.925334	36.414900
1467.888465	171841.816077	36.419917
1469.241982	172108.800226	36.424935
1470.777274	172362.398888	36.429952
1472.186778	172637.185187	36.434970
1473.626349	172895.790791	36.439988
1475.284886	173173.447800	36.445005
1476.723152	173442.467631	36.450023
1477.884099	173710.554050	36.455040
1479.629031	173987.781381	36.460058
1481.158955	174264.357641	36.465076
1482.929336	174527.361117	36.470093
1484.654268	174804.200773	36.475111
1485.889534	175071.492845	36.480128
1487.445018	175339.700737	36.485146
1489.040935	175624.410848	36.490164
1490.844629	175889.864279	36.495181
1492.223990	176160.654768	36.500199
1493.626673	176422.299693	36.505216
1495.511678	176690.625480	36.510234
1496.800285	176960.366105	36.515252
1497.910905	177230.313230	36.520269
1499.663837	177505.722619	36.525287
1501.061201	177771.664652	36.530304
1502.921739	178041.700145	36.535322
1504.265597	178328.554123	36.540340
1505.957265	178583.176226	36.545357
1507.595277	178859.852393	36.550375
1509.236636	179125.557206	36.555392
1510.656765	179393.507029	36.560410
1511.875813	179669.057621	36.565428
1513.415544	179931.758436	36.570445
1514.740789	180210.773555	36.575463
1516.812703	180483.526391	36.580480
1518.435125	180761.861746	36.585498
1519.815866	181032.057620	36.590516
1521.293219	181296.448406	36.595533
1522.851309	181564.814817	36.600551
1524.429379	181836.760022	36.605568
1525.598427	182104.376128	36.610586
1527.252602	182376.234785	36.615604
1528.846932	182646.757470	36.620621
1530.463224	182918.191829	36.625639
1531.934060	183183.731852	36.630656
1533.310244	183453.782977	36.635674
1535.019196	183714.029663	36.640692
1536.655744	183961.004814	36.645709
1537.944923	184225.052171	36.650727
1539.417113	184479.826386	36.655744
1540.570235	184742.880455	36.660762
1542.278737	185003.308384	36.665780
1543.919114	185331.944257	36.670797
1545.212150	185594.419858	36.675815
1546.850830	185853.260738	36.680832
1548.162040	186111.315342	36.685850
1549.617064	186391.115342	36.690868
1551.339789	186657.742678	36.695885
1552.539157	186933.596422	36.700903
1554.402882	187219.455934	36.705920
1555.571421	187497.551123	36.710938
1556.640011	187774.773682	36.715956
1558.428097	188053.865521	36.720973
1559.902834	188337.934683	36.725991
1561.487275	188622.368404	36.731008
1563.230019	188918.563663	36.736026
1564.492619	189211.609047	36.741044
1566.147921	189500.047111	36.746061
1567.623474	189803.728738	36.751079
1569.485915	190098.511334	36.756096
1571.180838	190395.276721	36.761114
1572.574546	190694.249035	36.766132
1574.190580	190983.382748	36.771149
1575.719496	191289.498324	36.776167
1577.221856	191597.904887	36.781184
1578.825817	191897.482321	36.786202
1580.093618	192197.163902	36.791220
1581.800104	192503.762759	36.796237
1583.454909	192817.660491	36.801255
1585.390596	193117.976385	36.806272
1586.905727	193426.436305	36.811290
1588.416095	193744.448486	36.816308
1590.470134	194051.657118	36.821325
1591.442810	194360.839192	36.826343
1593.055886	194662.707833	36.831360
1594.964259	194974.335815	36.836378
1596.673522	195296.791228	36.841396
1598.651789	195601.881587	36.846413
1599.967580	195909.743453	36.851431
1601.833857	196216.503789	36.856448
1603.599817	196535.600230	36.861466
1604.973964	196839.314556	36.866484
1606.539812	197143.228137	36.871501
1608.370188	197454.696058	36.876519
1610.215647	197762.326619	36.881536
1611.838554	198063.845418	36.886554
1613.742899	198383.508491	36.891572
1615.176745	198677.894791	36.896589
1616.766122	198984.069215	36.901607
1618.787091	199292.564484	36.906624
1620.492016	199591.838080	36.911642
1621.851072	199892.385671	36.916660
1623.350282	200194.969461	36.921677
1624.927672	200505.009819	36.926695
1626.390017	200804.222018	36.931712
1628.265448	201108.755385	36.936730
1630.008947	201418.568230	36.941748
1631.532134	201712.996884	36.946765
1633.432998	202020.652388	36.951783
1635.041323	202321.165324	36.956800
1636.591084	202622.450008	36.961818
1638.281845	202930.139971	36.966836
1639.765428	203226.330108	36.971853
1641.430082	203525.515293	36.976871
1642.918600	203820.079837	36.981888
1644.961118	204098.147998	36.986906
1646.278118	204382.325149	36.991924
1647.850560	204655.691965	36.996941
1649.559729	204945.320956	37.001959
1651.126826	205231.162175	37.006976
1653.015751	205510.526503	37.011994
1654.089270	205815.777367	37.017012
1655.733142	206093.859880	37.022029
1657.686148	206393.029653	37.027047
1658.735951	206691.883936	37.032064
1660.492036	206988.341821	37.037082
1662.033902	207294.232765	37.042100
1664.106613	207587.796745	37.047117
1665.708577	207898.150040	37.052135
1667.051355	208205.241895	37.057152
1668.887759	208514.543182	37.062170
1670.622630	208822.590592	37.067188
1672.105451	209128.620164	37.072205
1674.088137	209438.636409	37.077223
1675.604947	209747.887627	37.082240
1677.380270	210062.687493	37.087258
1679.051128	210388.986412	37.092276
1680.585039	210696.457812	37.097293
1682.717073	211009.348494	37.102311
1684.533301	211329.147883	37.107328
1685.944906	211645.911716	37.112346
1687.674723	211965.268053	37.117364
1689.672671	212279.603665	37.122381
1691.336295	212584.389359	37.127399
1692.863276	212905.937704	37.132416
1694.857851	213213.339574	37.137434
1696.431194	213535.795802	37.142452
1698.451738	213853.431858	37.147469
1699.994307	214173.251505	37.152487
1701.824156	214493.331319	37.157504
1703.669295	214813.485222	37.162522
1705.389273	215124.843870	37.167540
1707.323339	215442.291569	37.172557
1709.155124	215751.753319	37.177575
1710.476659	216066.223487	37.182592
1712.376578	216392.136708	37.187610
1714.295213	216701.788764	37.192628
1716.027011	217017.745019	37.197645
1717.554349	217338.585615	37.202663
1719.276809	217649.564567	37.207680
1721.261663	217968.809719	37.212698
1722.666765	218290.127288	37.217716
1724.519206	218601.289663	37.222733
1726.545068	218917.124791	37.227751
1728.096821	219248.835540	37.232768
1729.729038	219561.963549	37.237786
1731.544630	219886.164545	37.242804
1733.386035	220203.197711	37.247821
1735.219302	220521.019802	37.252839
1736.813840	220842.359722	37.257856
1738.777490	221160.847549	37.262874
1740.197438	221481.656119	37.267892
1741.633516	221793.951905	37.272909
1743.497834	222114.970564	37.277927
1745.186944	222442.266120	37.282944
1747.114098	222762.335150	37.287962
1748.399887	223091.091187	37.292980
1750.486926	223414.514060	37.297997
1752.292569	223740.496022	37.303015
1753.674001	224077.747610	37.308032
1755.182127	224387.644610	37.313050
1757.285537	224730.245153	37.318068
1758.776940	225033.107876	37.323085
1760.961880	225339.113798	37.328103
1762.209911	225654.742059	37.333120
1764.141203	225963.886965	37.338138
1765.750791	226280.678019	37.343156
1767.561710	226598.580728	37.348173
1769.125448	226898.434381	37.353191
1770.846589	227227.300227	37.358208
1772.563406	227538.968143	37.363226
1774.213895	227869.013526	37.368244
1775.924688	228189.345052	37.373261
1777.614255	228513.338012	37.378279
1779.225936	228849.918082	37.383296
1781.349265	229187.332534	37.388314
1783.018960	229515.367565	37.393332
1784.369780	229856.535457	37.398349
1786.457261	230193.294664	37.403367
1788.369636	230545.120307	37.408384
1789.533373	230880.474137	37.413402
1791.372476	231231.370980	37.418420
1792.804987	231585.735401	37.423437
1795.140602	231944.124555	37.428455
1797.024825	232296.360173	37.433472
1798.936871	232650.801366	37.438490
1800.596715	232998.448148	37.443508
1802.155005	233367.170417	37.448525
1804.095079	233716.576543	37.453543
1805.804635	234081.387819	37.458560
1807.526433	234438.143880	37.463578
1809.903367	234809.201098	37.468596
1811.538474	235172.448098	37.473613
1813.532530	235538.788677	37.478631
1814.927978	235902.936256	37.483648
1816.988131	236268.325873	37.488666
1818.672750	236634.942466	37.493684
1820.925652	237003.679879	37.498701
1822.833104	237378.618639	37.503719
1824.542737	237736.313486	37.508736
1826.348635	238106.034177	37.513754
1828.665677	238476.563580	37.518772
1830.346233	238850.240560	37.523789
1832.548393	239209.431680	37.528807
1833.947690	239583.024735	37.533824
1836.278782	239952.406948	37.538842
1838.082523	240313.310250	37.543860
1839.766298	240677.712105	37.548877
1842.060995	241031.577100	37.553895
1843.658939	241403.307536	37.558912
1846.063669	241763.759157	37.563930
1847.729498	242129.685954	37.568948
1849.466869	242497.988904	37.573965
1851.676193	242841.169945	37.578983
1853.141251	243212.588166	37.584000
1855.101757	243576.205728	37.589018
1857.108631	243934.302990	37.594036
1859.142791	244305.630344	37.599053
1861.049430	244661.023975	37.604071
1862.715710	245029.359282	37.609088
1865.121466	245376.620884	37.614106
1866.598821	245731.876630	37.619124
1868.288769	246094.414469	37.624141
1870.411598	246449.212289	37.629159
1872.206280	246804.340234	37.634176
1874.239590	247169.515009	37.639194
1876.408054	247521.229971	37.644212
1878.413195	247875.941910	37.649229
1880.193844	248229.519768	37.654247
1881.754667	248574.342090	37.659264
1883.490046	248908.467432	37.664282
1885.544749	249243.634462	37.669300
1887.138938	249579.228524	37.674317
1889.307605	249907.543200	37.679335
1890.638677	250254.938298	37.684352
1892.543804	250582.530803	37.689370
1894.220441	250933.782302	37.694388
1895.994603	251281.232870	37.699405
1898.074338	251617.127780	37.704423
1899.334732	251981.270047	37.709440
1901.400425	252325.472023	37.714458
1903.376134	252676.164745	37.719476
1904.824697	253047.793919	37.724493
1907.010581	253399.518913	37.729511
1908.582603	253783.726110	37.734528
1910.517520	254146.233417	37.739546
1912.415241	254516.696265	37.744564
1914.347035	254902.800042	37.749581
1916.169262	255265.042664	37.754599
1918.057520	255655.850373	37.759616
1919.938372	256031.290409	37.764634
1922.254039	256415.653330	37.769652
1924.157958	256801.171796	37.774669
1926.546456	257172.515776	37.779687
1928.331755	257568.718898	37.784704
1929.944971	257942.163210	37.789722
1931.796634	258324.002130	37.794740
1933.864717	258709.082688	37.799757
1935.979835	259103.324267	37.804775
1937.650448	259499.843951	37.809792
1939.380016	259880.376262	37.814810
1941.547715	260280.117610	37.819828
1943.521546	260679.938724	37.824845
1945.475424	261070.922337	37.829863
1947.676715	261475.302511	37.834880
1949.705049	261872.037519	37.839898
1951.934677	262275.114982	37.844916
1953.465749	262671.670941	37.849933
1955.552257	263061.864838	37.854951
1957.183747	263474.403940	37.859968
1959.284500	263879.806975	37.864986
1961.959488	264280.165732	37.870004
1963.686616	264687.656066	37.875021
1965.821055	265086.292956	37.880039
1967.679743	265485.504825	37.885056
1969.740896	265888.315498	37.890074
1972.322816	266281.239113	37.895092
1973.868077	266685.625831	37.900109
1975.748396	267083.202424	37.905127
1978.059427	267481.751347	37.910144
1979.668646	267880.103658	37.915162
1982.045501	268274.499055	37.920180
1983.913286	268675.728399	37.925197
1985.666581	269077.964473	37.930215
1987.776159	269475.469831	37.935232
1990.009359	269879.709981	37.940250
1992.210476	270289.007529	37.945268
1993.859454	270681.093797	37.950285
1996.114989	271084.004409	37.955303
1997.764414	271484.773058	37.960320
1999.915580	271883.175626	37.965338
2002.086629	272278.144645	37.970356
2003.901526	272682.361348	37.975373
2006.220192	273084.516369	37.980391
2007.877148	273477.757139	37.985408
2009.993572	273880.244804	37.990426
2011.752645	274281.821381	37.995444
2013.487129	274678.625327	38.000461
2015.375552	275059.124196	38.005479
2017.612465	275440.658816	38.010496
2019.496186	275833.243442	38.015514
2021.724843	276210.229821	38.020532
2023.142637	276602.655029	38.025549
2025.214007	276988.500118	38.030567
2027.333758	277380.430711	38.035584
2029.004552	277783.121104	38.040602
2031.096807	278176.144012	38.045620
2032.997542	278573.867612	38.050637
2035.312906	278974.749456	38.055655
2037.235003	279393.771955	38.060672
2038.833198	279803.624473	38.065690
2041.109624	280207.807189	38.070708
2043.178214	280629.872612	38.075725
2045.247816	281035.708421	38.080743
2047.027476	281454.716191	38.085760
2049.129885	281867.601850	38.090778
2051.065346	282287.418433	38.095796
2053.173774	282722.492585	38.100813
2055.280291	283142.429736	38.105831
2057.407513	283569.826848	38.110848
2058.843218	284008.248697	38.115866
2061.335834	284439.366925	38.120884
2063.314728	284878.434683	38.125901
2065.689522	285311.597319	38.130919
2067.571282	285754.508964	38.135936
2069.907357	286199.124102	38.140954
2072.029750	286635.237877	38.145972
2073.990172	287080.388375	38.150989
2076.245230	287520.436756	38.156007
2078.424976	287972.047273	38.161024
2080.229565	288412.744137	38.166042
2082.582118	288846.344202	38.171060
2084.670959	289311.417097	38.176077
2086.577787	289756.024403	38.181095
2089.305517	290196.869239	38.186112
2091.141842	290650.368120	38.191130
2093.531614	291094.077897	38.196148
2095.388524	291541.930339	38.201165
2097.564187	291987.063677	38.206183
2099.812695	292435.635429	38.211200
2102.171815	292892.920685	38.216218
2104.233603	293328.312297	38.221236
2106.437016	293775.637051	38.226253
2108.791240	294220.421308	38.231271
2110.989998	294667.663902	38.236288
2112.901791	295115.455769	38.241306
2115.468362	295554.458814	38.246324
2117.341661	296012.786132	38.251341
2119.832121	296450.296363	38.256359
2121.777381	296891.417506	38.261376
2123.471186	297335.925785	38.266394
2126.006311	297765.954865	38.271412
2128.041632	298225.026060	38.276429
2130.458590	298668.953695	38.281447
2132.482711	299101.692736	38.286464
2134.415176	299551.401210	38.291482
2136.820886	299993.365169	38.296500
2138.852431	300440.359848	38.301517
2141.021458	300880.398869	38.306535
2143.218225	301317.307469	38.311552
2145.437276	301765.023423	38.316570
2147.945366	302201.774547	38.321588
2149.807074	302646.391159	38.326605
2151.906586	303082.234283	38.331623
2153.929428	303521.055831	38.336640
2155.888701	303958.690542	38.341658
2158.317553	304381.321926	38.346676
2160.579994	304794.507484	38.351693
2162.460355	305215.923212	38.356711
2164.828452	305624.516374	38.361728
2166.495641	306040.551826	38.366746
2168.812526	306458.741348	38.371764
2170.958074	306872.562865	38.376781
2172.828217	307293.023671	38.381799
2175.611173	307723.745130	38.386816
2177.227319	308150.431845	38.391834
2179.299408	308580.394024	38.396852
2181.467015	309010.439011	38.401869
2183.568039	309459.146438	38.406887
2185.710810	309894.010078	38.411904
2187.454866	310348.222188	38.416922
2189.892130	310778.234633	38.421940
2192.016020	311234.587077	38.426957
2193.833105	311682.074440	38.431975
2195.829240	312140.697029	38.436992
2198.260731	312600.642950	38.442010
2200.579096	313062.962390	38.447028
2202.867672	313536.068336	38.452045
2204.640536	314005.214757	38.457063
2207.074777	314463.796623	38.462080
2209.238625	314934.902708	38.467098
2211.630997	315410.333322	38.472116
2213.674492	315886.625630	38.477133
2216.265670	316365.796476	38.482151
2218.663026	316838.368847	38.487168
2220.568877	317313.830024	38.492186
2222.704025	317795.543841	38.497204
2225.424356	318273.506526	38.502221
2227.130408	318758.271428	38.507239
2229.833848	319237.723449	38.512256
2232.133538	319723.526670	38.517274
2234.139656	320203.711483	38.522292
2236.773531	320700.566115	38.527309
2238.914877	321172.877787	38.532327
2241.277739	321664.028714	38.537344
2243.254511	322160.309317	38.542362
2246.085190	322647.391743	38.547380
2248.206677	323128.946344	38.552397
2250.574000	323619.642316	38.557415
2253.313913	324101.672494	38.562432
2255.431204	324578.821246	38.567450
2257.997079	325067.870391	38.572468
2260.462291	325549.875779	38.577485
2262.580736	326029.646167	38.582503
2265.210619	326499.435684	38.587520
2267.179178	326972.469292	38.592538
2269.687769	327446.250097	38.597556
2272.083845	327931.485342	38.602573
2274.167625	328409.938704	38.607591
2276.783923	328875.237046	38.612608
2278.673945	329357.692414	38.617626
2280.951883	329835.514533	38.622644
2283.146523	330303.094427	38.627661
2285.284846	330786.913960	38.632679
2287.881260	331262.461529	38.637696
2289.918862	331738.927801	38.642714
2292.592802	332220.895037	38.647732
2294.889545	332694.771984	38.652749
2296.851915	333168.314795	38.657767
2299.597212	333638.837286	38.662784
2301.957903	334123.416771	38.667802
2304.033110	334601.997312	38.672820
2306.259730	335073.673668	38.677837
2308.422294	335545.912103	38.682855
2310.527946	335999.661617	38.687872
2312.860070	336468.564125	38.692890
2315.172105	336909.358989	38.697908
2317.761938	337364.766050	38.702925
2319.477451	337821.217302	38.707943
2321.874170	338276.237283	38.712960
2323.909920	338742.062343	38.717978
2326.057871	339211.084995	38.722996
2328.353244	339665.646658	38.728013
2330.589934	340148.948043	38.733031
2332.956933	340615.685963	38.738048
2334.978008	341099.008090	38.743066
2337.369480	341580.946804	38.748084
2339.975737	342065.584340	38.753101
2341.944878	342562.082448	38.758119
2344.408853	343051.927559	38.763136
2346.352066	343548.897431	38.768154
2348.855237	344041.816338	38.773172
2351.032397	344542.158866	38.778189
2353.100936	345052.553399	38.783207
2355.852043	345562.072718	38.788224
2357.823001	346076.068096	38.793242
2360.022888	346594.356090	38.798260
2362.635365	347111.354354	38.803277
2364.659309	347639.822203	38.808295
2367.216208	348157.776508	38.813312
2369.443044	348687.742711	38.818330
2371.911981	349217.763947	38.823348
2374.535140	349746.636839	38.828365
2377.043400	350304.170831	38.833383
2379.627845	350824.943893	38.838400
2381.179895	351363.339424	38.843418
2384.012988	351904.923048	38.848436
2386.717242	352454.149178	38.853453
2388.760292	352989.981324	38.858471
2391.261154	353525.504664	38.863488
2393.669768	354085.042190	38.868506
2396.396231	354631.260969	38.873524
2398.981903	355178.278176	38.878541
2401.152277	355719.849586	38.883559
2404.090262	356260.454940	38.888576
2406.485882	356810.413912	38.893594
2408.882428	357352.960807	38.898612
2411.442809	357899.857952	38.903629
2413.807463	358452.656902	38.908647
2415.970600	358997.822131	38.913664
2418.666694	359538.382271	38.918682
2421.199487	360097.892916	38.923700
2423.597256	360639.696694	38.928717
2426.094502	361202.056583	38.933735
2428.415698	361734.829143	38.938752
2431.161747	362285.799958	38.943770
2433.256047	362833.592951	38.948788
2436.249679	363385.163548	38.953805
2438.888427	363934.118164	38.958823
2441.335505	364476.046902	38.963840
2443.699189	365023.807587	38.968858
2446.233442	365568.135330	38.973876
2448.663142	366114.724664	38.978893
2450.894914	366657.254558	38.983911
2453.230275	367203.913995	38.988928
2456.405711	367746.655790	38.993946
2458.811018	368286.036070	38.998964
2461.081284	368824.565672	39.003981
2463.495156	369372.919616	39.008999
2466.086580	369902.180202	39.014016
2468.588676	370449.992572	39.019034
2470.855144	370984.249896	39.024052
2472.765340	371497.725250	39.029069
2475.412629	372020.298512	39.034087
2478.030799	372537.115051	39.039104
2480.500181	373049.384671	39.044122
2482.710555	373569.716652	39.049140
2485.107658	374084.663817	39.054157
2487.528273	374605.475231	39.059175
2489.951151	375134.813935	39.064192
2492.422936	375659.929251	39.069210
2494.561197	376194.029138	39.074228
2497.412529	376725.701609	39.079245
2499.212205	377276.349836	39.084263
2501.896798	377810.838688	39.089280
2504.571529	378346.078278	39.094298
2506.525512	378896.567517	39.099316
2508.929570	379445.885693	39.104333
2511.341032	380019.431636	39.109351
2513.655356	380585.533503	39.114368
2516.388263	381161.537039	39.119386
2519.031608	381727.942566	39.124404
2521.362756	382290.914707	39.129421
2523.900998	382873.673056	39.134439
2526.866121	383454.122735	39.139456
2529.232234	384031.385962	39.144474
2531.509222	384613.740421	39.149492
2534.234269	385193.023190	39.154509
2536.573109	385776.531575	39.159527
2539.259033	386370.987832	39.164544
2542.004500	386966.838807	39.169562
2544.441998	387566.319531	39.174580
2547.234766	388160.412792	39.179597
2549.754616	388761.649726	39.184615
2552.280127	389358.566755	39.189632
2555.215369	389948.619611	39.194650
2557.721224	390552.954782	39.199668
2560.604430	391148.506508	39.204685
2563.039355	391757.987982	39.209703
2565.590812	392357.106574	39.214720
2568.356959	392953.999567	39.219738
2571.106018	393546.171731	39.224756
2573.634133	394156.692155	39.229773
2576.063419	394758.757416	39.234791
2578.752353	395357.931738	39.239808
2581.772961	395954.862163	39.244826
2584.058068	396563.080835	39.249844
2586.886196	397165.680905	39.254861
2589.268481	397766.816614	39.259879
2591.881361	398367.749005	39.264896
2594.674516	398976.433286	39.269914
2597.471284	399583.177592	39.274932
2600.518813	400178.022313	39.279949
2602.977212	400784.130095	39.284967
2605.641934	401382.293752	39.289984
2608.328678	401981.551903	39.295002
2610.593346	402583.694687	39.300020
2613.585219	403185.454801	39.305037
2616.341563	403785.262062	39.310055
2618.422570	404373.670993	39.315072
2621.205785	404971.013435	39.320090
2623.801659	405574.846860	39.325108
2626.509671	406176.318707	39.330125
2629.009998	406785.093686	39.335143
2631.788848	407388.900134	39.340160
2634.740965	407996.356886	39.345178
2637.499969	408608.836452	39.350196
2639.970247	409201.762998	39.355213
2642.756497	409800.645070	39.360231
2645.222770	410382.662216	39.365248
2647.968089	410950.909427	39.370266
2650.494127	411526.208400	39.375284
2653.365626	412081.454779	39.380301
2655.298874	412649.076295	39.385319
2657.935384	413214.245847	39.390336
2660.470037	413783.868117	39.395354
2663.018501	414366.675880	39.400372
2665.947248	414936.104696	39.405389
2668.371508	415515.258485	39.410407
2670.763924	416102.696795	39.415424
2673.474542	416686.528464	39.420442
2675.595674	417280.147244	39.425460
2678.524084	417875.797842	39.430477
2681.062262	418477.966232	39.435495
2683.801328	419082.361704	39.440512
2686.657080	419684.041061	39.445530
2689.212251	420291.464548	39.450548
2691.787559	420904.632019	39.455565
2694.754145	421529.350757	39.460583
2697.202566	422140.731435	39.465600
2699.773428	422765.626188	39.470618
2702.332265	423387.773306	39.475636
2705.346254	424009.931381	39.480653
2708.035679	424651.940842	39.485671
2710.666796	425278.013062	39.490688
2713.558114	425916.057794	39.495706
2716.020315	426559.356638	39.500724
2719.048933	427196.934781	39.505741
2721.826393	427838.424405	39.510759
2724.225946	428478.941472	39.515776
2727.265955	429127.829975	39.520794
2729.841851	429779.954286	39.525812
2732.937107	430432.986744	39.530829
2735.786052	431076.735937	39.535847
2738.056565	431726.013042	39.540864
2740.972322	432378.503362	39.545882
2743.712112	433025.793832	39.550900
2746.733271	433690.504640	39.555917
2749.435876	434352.513522	39.560935
2752.519770	435011.610168	39.565952
2755.482893	435661.758929	39.570970
2758.156716	436328.706978	39.575988
2761.116503	436982.247474	39.581005
2764.116591	437639.397183	39.586023
2766.565884	438299.540748	39.591040
2769.581383	438949.468067	39.596058
2772.345004	439620.227306	39.601076
2775.358822	440266.775016	39.606093
2778.241262	440929.890916	39.611111
2781.269828	441583.564408	39.616128
2783.980714	442231.809078	39.621146
2786.646771	442877.866091	39.626164
2789.804598	443552.564416	39.631181
2793.149428	444195.943673	39.636199
2795.492537	444846.376609	39.641216
2798.139791	445488.759042	39.646234
2801.398834	446136.629171	39.651252
2804.026502	446783.665987	39.656269
2806.985504	447427.294949	39.661287
2809.557569	448071.214065	39.666304
2812.717268	448724.764203	39.671322
2814.991099	449375.500477	39.676340
2818.053261	450025.685962	39.681357
2820.842542	450671.800738	39.686375
2823.662181	451325.814221	39.691392
2826.575418	451966.207917	39.696410
2829.265583	452615.650335	39.701428
2832.460112	453255.751521	39.706445
2834.884650	453877.978311	39.711463
2837.338305	454492.354116	39.716480
2840.259260	455102.142756	39.721498
2842.974593	455727.691054	39.726516
2845.624685	456335.459965	39.731533
2848.500947	456968.106033	39.736551
2850.939521	457598.273930	39.741568
2853.406071	458226.345271	39.746586
2856.355193	458858.406179	39.751604
2858.741904	459506.630402	39.756621
2861.708788	460141.517904	39.761639
2864.389806	460806.855105	39.766656
2867.174028	461458.475595	39.771674
2869.481209	462119.430015	39.776692
2872.595568	462788.557717	39.781709
2875.744767	463464.464800	39.786727
2878.262497	464147.052762	39.791744
2881.330504	464817.217205	39.796762
2884.325357	465505.376208	39.801780
2887.230038	466186.559480	39.806797
2889.877319	466874.161536	39.811815
2892.456867	467574.961456	39.816832
2895.766489	468266.538483	39.821850
2898.577754	468970.925155	39.826868
2901.241519	469674.497827	39.831885
2904.312463	470387.306808	39.836903
2906.984173	471093.389478	39.841920
2910.267156	471817.954192	39.846938
2913.803467	472535.841198	39.851956
2915.748595	473255.659698	39.856973
2918.959229	473969.903586	39.861991
2921.639842	474695.946517	39.867008
2924.783962	475426.270516	39.872026
2928.033170	476155.687773	39.877044
2931.115499	476884.845792	39.882061
2934.343532	477609.108278	39.887079
2937.364168	478345.568960	39.892096
2940.276875	479076.669289	39.897114
2943.223922	479813.829238	39.902132
2946.916245	480552.551789	39.907149
2949.463600	481265.614487	39.912167
2952.022585	481991.947568	39.917184
2955.720540	482728.449941	39.922202
2958.699204	483461.049002	39.927220
2961.321035	484206.921667	39.932237
2964.438247	484940.386540	39.937255
2967.613156	485669.676001	39.942272
2970.559367	486392.064308	39.947290
2973.522748	487125.348315	39.952308
2976.604157	487850.115332	39.957325
2979.853015	488593.410057	39.962343
2982.605759	489333.320709	39.967360
2985.998312	490060.301246	39.972378
2988.801711	490794.591880	39.977396
2991.849361	491534.449450	39.982413
2994.827187	492263.000308	39.987431
2997.773946	493005.168217	39.992448
3000.911858	493728.032765	39.997466
3003.799294	494454.476645	40.002484
3006.576728	495191.778418	40.007501
3010.152339	495924.286487	40.012519
3012.905835	496669.725466	40.017536
3016.150271	497399.745045	40.022554
3019.645627	498142.929245	40.027572
3022.139918	498867.002356	40.032589
3025.105397	499596.956102	40.037607
3028.177930	500323.031077	40.042624
3031.170409	501045.206683	40.047642
3034.404648	501738.972616	40.052660
3037.064823	502438.230414	40.057677
3040.061704	503131.060657	40.062695
3042.365055	503825.123390	40.067712
3045.928964	504535.561191	40.072730
3048.557229	505232.121607	40.077748
3051.567231	505936.437550	40.082765
3054.483524	506643.299246	40.087783
3057.099342	507355.455322	40.092800
3060.140695	508074.652760	40.097818
3062.870455	508815.292344	40.102836
3065.814375	509542.831097	40.107853
3069.013188	510280.905607	40.112871
3071.927229	511027.586588	40.117888
3075.150121	511764.623367	40.122906
3077.917804	512519.344805	40.127924
3081.394137	513274.316743	40.132941
3084.159532	514022.519725	40.137959
3087.013398	514800.587166	40.142976
3090.101827	515554.338605	40.147994
3093.379728	516330.543652	40.153012
3096.247607	517114.762584	40.158029
3099.551944	517886.099082	40.163047
3102.230088	518677.346251	40.168064
3105.444185	519464.341683	40.173082
3108.674509	520251.138060	40.178100
3111.786313	521050.974903	40.183117
3114.960671	521850.905242	40.188135
3118.193638	522655.351945	40.193152
3121.011758	523453.031227	40.198170
3124.790901	524257.346414	40.203188
3127.636947	525066.281011	40.208205
3131.263826	525873.938912	40.213223
3134.474160	526686.887812	40.218240
3138.031861	527508.071569	40.223258
3141.358323	528319.243864	40.228276
3143.912534	529118.984102	40.233293
3147.314391	529915.127526	40.238311
3150.855329	530736.463291	40.243328
3153.960672	531546.365020	40.248346
3156.952328	532349.153320	40.253364
3159.658656	533174.432552	40.258381
3163.015563	533986.351761	40.263399
3166.358285	534811.125463	40.268416
3169.660034	535639.768565	40.273434
3173.335067	536449.273260	40.278452
3176.587865	537263.109707	40.283469
3179.729164	538086.298073	40.288487
3182.794025	538896.495497	40.293504
3186.488906	539727.672033	40.298522
3189.660396	540529.065530	40.303540
3192.744583	541347.885109	40.308557
3196.181086	542140.904563	40.313575
3199.389428	542971.491157	40.318592
3202.582794	543779.999162	40.323610
3206.066134	544588.359184	40.328628
3208.715004	545401.462509	40.333645
3212.300370	546205.035806	40.338663
3215.562429	547031.329585	40.343680
3218.948908	547850.526671	40.348698
3222.478165	548665.032785	40.353716
3225.172695	549475.101839	40.358733
3228.191761	550277.644872	40.363751
3231.307402	551091.402097	40.368768
3234.603885	551902.569628	40.373786
3237.961340	552709.261403	40.378804
3241.366290	553534.090100	40.383821
3244.607820	554335.577868	40.388839
3247.888240	555110.690032	40.393856
3250.826763	555883.850804	40.398874
3254.079649	556648.191695	40.403892
3257.046338	557425.207854	40.408909
3260.385380	558186.980967	40.413927
3262.908515	558973.286427	40.418944
3266.124804	559755.623281	40.423962
3269.330899	560548.030808	40.428980
3272.314312	561349.487975	40.433997
3275.558453	562142.533797	40.439015
3278.717790	562951.418749	40.444032
3281.768542	563759.363176	40.449050
3285.364313	564573.727751	40.454068
3288.706139	565403.149885	40.459085
3291.816061	566214.821143	40.464103
3294.720117	567043.593494	40.469120
3297.743753	567878.496613	40.474138
3301.122637	568717.739777	40.479156
3304.603556	569563.464153	40.484173
3307.884345	570398.294273	40.489191
3310.976641	571260.674316	40.494208
3314.116104	572124.483384	40.499226
3317.495263	572985.536777	40.504244
3321.094661	573861.904401	40.509261
3324.153646	574729.631440	40.514279
3327.787421	575610.561977	40.519296
3330.824370	576490.416123	40.524314
3334.427938	577366.810751	40.529332
3337.890319	578246.560603	40.534349
3341.258491	579135.710014	40.539367
3344.601046	580019.690595	40.544384
3347.719285	580915.839290	40.549402
3350.873604	581806.908847	40.554420
3354.287554	582709.367278	40.559437
3358.151662	583611.831401	40.564455
3361.330896	584514.328447	40.569472
3365.105904	585430.906149	40.574490
3368.696548	586324.090775	40.579508
3372.025779	587239.236536	40.584525
3375.288298	588138.321753	40.589543
3378.837221	589044.034485	40.594560
3382.198653	589947.351919	40.599578
3385.707317	590851.220233	40.604596
3388.813734	591769.864847	40.609613
3392.427867	592675.311849	40.614631
3395.517724	593596.000628	40.619648
3399.431758	594507.389938	40.624666
3402.945290	595422.210104	40.629684
3406.475272	596338.197373	40.634701
3410.291665	597256.557478	40.639719
3413.670743	598166.666885	40.644736
3417.151753	599068.792740	40.649754
3420.837650	599977.149564	40.654772
3424.460326	600887.683899	40.659789
3427.963224	601786.477011	40.664807
3431.315178	602676.681097	40.669824
3434.651220	603587.523305	40.674842
3438.745869	604488.285880	40.679860
3441.541047	605388.274878	40.684877
3445.300319	606283.144860	40.689895
3448.644866	607185.335723	40.694912
3452.075934	608076.458670	40.699930
3455.643823	608974.266553	40.704948
3459.461442	609876.595005	40.709965
3462.645420	610765.426841	40.714983
3466.201771	611667.587239	40.720000
3469.335714	612561.007008	40.725018
3472.926235	613439.174633	40.730023
3476.219174	614283.565423	40.735028
3479.488328	615063.965332	40.740032
3482.732794	615809.225383	40.745037
3485.403535	616514.541838	40.750042
3488.525795	617146.683260	40.755047
3491.337164	617731.465320	40.760052
3494.044460	618246.130543	40.765056
3496.857517	618715.138026	40.770061
3499.037714	619136.711221	40.775066
3501.259520	619505.655082	40.780071
3502.963177	619826.309208	40.785076
3505.262377	620094.657704	40.790080
3507.094254	620312.519427	40.795085
3508.773340	620505.274275	40.800090
3510.221352	620654.953433	40.805095
3511.323412	620760.927457	40.810100
3512.847858	620834.566286	40.815104
3514.361372	620874.240069	40.820109
3515.561471	620879.297199	40.825114
3516.614754	620847.264114	40.830119
3517.638372	620796.903647	40.835124
3518.484054	620721.944855	40.840128
3519.536407	620610.638360	40.845133
3520.312964	620490.682032	40.850138
3520.614097	620339.827713	40.855143
3521.454814	620181.443619	40.860148
3522.146235	619992.657889	40.865152
3522.521999	619792.028426	40.870157
3522.534863	619582.409441	40.875162
3523.043232	619347.829470	40.880167
3523.129316	619120.054469	40.885172
3523.570638	618873.833274	40.890176
3523.949422	618617.423564	40.895181
3523.556576	618351.784777	40.900186
3524.002507	618081.510970	40.905191
3523.645057	617798.314337	40.910196
3524.267491	617525.849331	40.915200
3524.215705	617245.687179	40.920205
3524.395361	616954.687447	40.925210
3524.603231	616656.129119	40.930215
3524.194942	616364.654426	40.935220
3524.168937	616055.620384	40.940224
3524.169975	615750.970474	40.945229
3523.939202	615450.045883	40.950234
3524.265307	615134.931088	40.955239
3523.525744	614828.819583	40.960244
3523.720560	614524.951820	40.965248
3523.583843	614219.177338	40.970253
3523.138396	613913.891694	40.975258
3523.106322	613604.783163	40.980263
3523.221510	613303.090387	40.985268
3522.828416	612999.568437	40.990272
3522.971029	612688.404928	40.995277
3522.716904	612378.343711	41.000282
3522.736463	612083.778444	41.005287
3522.147031	611776.750865	41.010292
3522.298029	611474.997937	41.015296
3522.116401	611171.788067	41.020301
3521.717840	610880.953115	41.025306
3521.556448	610566.071927	41.030311
3521.226279	610286.809682	41.035316
3520.274020	609988.135233	41.040320
3520.891599	609712.259390	41.045325
3520.684180	609426.603597	41.050330
3520.538065	609143.130604	41.055335
3520.057306	608860.502215	41.060340
3519.771859	608581.686358	41.065344
3519.610041	608303.443724	41.070349
3519.614285	608037.771142	41.075354
3519.190088	607760.705094	41.080359
3519.223739	607501.666073	41.085364
3518.855649	607243.283530	41.090368
3518.606910	606978.323288	41.095373
3518.404253	606721.552387	41.100378
3518.102284	606466.191206	41.105383
3518.003457	606219.045731	41.110388
3517.769900	605957.758513	41.115392
3517.574698	605710.515848	41.120397
3517.323757	605471.780502	41.125402
3517.027996	605228.444074	41.130407
3516.768752	604986.246866	41.135412
3516.698901	604757.072243	41.140416
3516.336414	604521.534285	41.145421
3516.022742	604291.336795	41.150426
3516.116559	604066.424065	41.155431
3515.900215	603847.509048	41.160436
3515.584648	603614.995228	41.165440
3515.512671	603392.695646	41.170445
3515.047980	603189.667190	41.175450
3515.306960	602963.403733	41.180455
3514.760066	602754.625156	41.185460
3514.583956	602543.382460	41.190464
3514.525636	602338.272203	41.195469
3514.151719	602141.314168	41.200474
3514.215194	601928.219990	41.205479
3513.811603	601728.656513	41.210484
3513.619918	601546.822290	41.215488
3513.630112	601349.539012	41.220493
3513.347100	601167.111890	41.225498
3513.527555	600970.495496	41.230503
3513.176960	600797.581669	41.235508
3512.766715	600604.353976	41.240512
3513.082672	600422.070460	41.245517
3512.651637	600248.609568	41.250522
3512.379449	600064.609905	41.255527
3512.142462	599897.469550	41.260532
3512.225295	599717.212351	41.265536
3512.310789	599554.320785	41.270541
3511.721398	599388.679007	41.275546
3511.743783	599221.987897	41.280551
3511.496206	599048.979037	41.285556
3511.180112	598896.952475	41.290560
3511.232090	598733.903247	41.295565
3511.244625	598577.315373	41.300570
3511.024720	598422.263321	41.305575
3510.917804	598271.596712	41.310580
3510.471190	598120.580555	41.315584
3510.636434	597975.323913	41.320589
3510.410180	597831.227866	41.325594
3510.248141	597680.861806	41.330599
3510.160595	597547.303704	41.335604
3509.784706	597398.819446	41.340608
3510.080981	597257.637800	41.345613
3509.640622	597131.639499	41.350618
3509.572138	596980.898374	41.355623
3509.486356	596864.754794	41.360628
3509.702604	596733.542170	41.365632
3509.748196	596598.098717	41.370637
3509.448260	596467.864738	41.375642
3509.329547	596332.944276	41.380647
3509.119167	596205.096444	41.385652
3508.687708	596083.991227	41.390656
3509.058425	595961.457346	41.395661
3508.414193	595840.082170	41.400666
3509.055966	595723.411750	41.405671
3508.442829	595607.036375	41.410676
3508.234121	595493.300517	41.415680
3507.790587	595378.899100	41.420685
3507.786918	595268.684101	41.425690
3507.833422	595154.103504	41.430695
3507.763643	595062.675188	41.435700
3507.488620	594959.409947	41.440704
3507.571193	594855.587025	41.445709
3507.340289	594758.322221	41.450714
3507.721115	594649.593110	41.455719
3507.369516	594557.253015	41.460724
3507.208988	594441.395055	41.465728
3506.954300	594344.580901	41.470733
3506.912265	594263.107254	41.475738
3506.841625	594168.165770	41.480743
3506.924396	594077.907080	41.485748
3506.413423	593996.304377	41.490752
3506.614449	593894.657153	41.495757
3506.805232	593813.494246	41.500762
3506.718754	593722.307441	41.505767
3506.655642	593640.231336	41.510772
3506.608779	593556.198802	41.515776
3506.606138	593470.105254	41.520781
3506.480978	593384.731345	41.525786
3506.542514	593303.785106	41.530791
3506.600562	593210.618033	41.535796
3506.278692	593118.160654	41.540800
3506.461886	593037.343635	41.545805
3506.043358	592965.435264	41.550810
3505.980006	592886.458754	41.555815
3505.857846	592815.154166	41.560820
3506.083392	592732.525092	41.565824
3506.057198	592644.675519	41.570829
3506.141463	592568.879207	41.575834
3506.399816	592482.586641	41.580839
3506.284271	592398.054857	41.585844
3505.829374	592329.954657	41.590848
3506.002164	592258.600252	41.595853
3505.621895	592177.363933	41.600858
3505.756443	592110.071806	41.605863
3505.553651	592024.649089	41.610868
3505.757034	591953.187689	41.615872
3506.047534	591880.259545	41.620877
3505.471806	591812.124850	41.625882
3505.443684	591740.347582	41.630887
3505.566212	591663.937785	41.635892
3505.332794	591604.865067	41.640896
3505.666637	591527.269133	41.645901
3505.318807	591468.413922	41.650906
3505.047487	591401.381174	41.655911
3505.493795	591336.189483	41.660916
3505.138802	591264.610416	41.665920
3504.964328	591194.104732	41.670925
3504.862666	591140.268788	41.675930
3505.019602	591079.679407	41.680935
3505.049781	591015.202061	41.685940
3504.742353	590952.330072	41.690944
3504.717204	590884.203604	41.695949
3504.751024	590829.894062	41.700954
3504.775096	590775.886349	41.705959
3504.675456	590721.496931	41.710964
3504.509917	590663.660845	41.715968
3504.860669	590600.233033	41.720973
3504.404961	590552.962147	41.725978
3504.547999	590497.481611	41.730983
3504.225745	590437.214015	41.735988
3504.162790	590389.730719	41.740992
3504.406296	590337.490043	41.745997
3504.797393	590292.841053	41.751002
3504.693285	590236.045142	41.756007
3504.738717	590180.327737	41.761012
3504.195133	590114.231317	41.766016
3504.452726	590072.207465	41.771021
3503.969902	590021.581798	41.776026
3504.578841	589961.817270	41.781031
3504.638833	589921.477031	41.786036
3504.412733	589870.459819	41.791040
3504.837789	589805.011687	41.796045
3504.229958	589759.214027	41.801050
3504.716313	589707.283045	41.806055
3504.522622	589647.291543	41.811060
3503.974010	589589.509579	41.816064
3504.045503	589540.999489	41.821069
3503.780384	589501.710551	41.826074
3503.993629	589457.637041	41.831079
3503.886985	589409.404721	41.836084
3504.034881	589366.894246	41.841088
3503.861818	589318.872317	41.846093
3504.141880	589275.539169	41.851098
3504.019654	589237.529622	41.856103
3504.119911	589192.570830	41.861108
3503.873381	589137.043996	41.866112
3503.861452	589089.597108	41.871117
3503.779077	589042.561861	41.876122
3503.874821	588997.903593	41.881127
3503.900011	588957.364777	41.886132
3503.638926	588920.478132	41.891136
3503.888394	588872.889219	41.896141
3503.917235	588843.372575	41.901146
3503.637194	588784.191468	41.906151
3503.917974	588742.910412	41.911156
3503.788479	588695.881024	41.916160
3503.900858	588649.364790	41.921165
3503.708354	588614.921594	41.926170
3503.655877	588571.787936	41.931175
3503.702489	588524.179098	41.936180
3503.521664	588485.574786	41.941184
3503.826545	588442.334640	41.946189
3503.713306	588410.784628	41.951194
3503.480852	588370.734861	41.956199
3503.822462	588325.584417	41.961204
3503.764701	588286.910051	41.966208
3503.800654	588244.913753	41.971213
3503.803433	588218.656517	41.976218
3503.937826	588163.015029	41.981223
3503.681978	588111.292645	41.986228
3503.644082	588074.769097	41.991232
3503.818390	588034.403954	41.996237
3503.966765	587995.295449	42.001242
3503.957683	587936.919214	42.006247
3503.652243	587901.489212	42.011252
3504.089869	587850.158270	42.016256
3504.039371	587813.535594	42.021261
3503.851497	587773.326320	42.026266
3504.209159	587720.503955	42.031271
3504.031851	587681.846121	42.036276
3503.765773	587628.770043	42.041280
3503.791319	587581.410917	42.046285
3503.718432	587550.303096	42.051290
3503.704957	587504.202520	42.056295
3503.736401	587471.224031	42.061300
3503.566697	587433.065241	42.066304
3503.917902	587385.303567	42.071309
3503.803729	587348.639165	42.076314
3503.579855	587298.411280	42.081319
3503.481455	587260.741864	42.086324
3503.551456	587217.834242	42.091328
3503.826290	587177.099410	42.096333
3503.811413	587133.803820	42.101338
3503.711954	587095.632864	42.106343
3503.511849	587051.964997	42.111348
3503.296154	587015.916709	42.116352
3503.627985	586978.980882	42.121357
3503.162005	586947.030733	42.126362
3503.168944	586908.090772	42.131367
3503.713859	586863.804537	42.136372
3503.180191	586831.112910	42.141376
3502.891408	586791.166350	42.146381
3503.223539	586768.462399	42.151386
3503.315427	586727.153104	42.156391
3503.374034	586699.179551	42.161396
3503.348261	586656.735729	42.166400
3503.392456	586614.832077	42.171405
3503.417544	586586.713128	42.176410
3503.646524	586538.215111	42.181415
3503.875453	586500.291428	42.186420
3503.737221	586464.630135	42.191424
3503.863159	586416.298033	42.196429
3503.536621	586384.675249	42.201434
3503.667420	586341.453971	42.206439
3503.473845	586309.158660	42.211444
3502.888530	586277.676254	42.216448
3503.426420	586236.094906	42.221453
3503.414306	586204.723151	42.226458
3503.203152	586168.320523	42.231463
3502.987459	586127.909045	42.236468
3502.848784	586100.115151	42.241472
3503.139318	586071.602551	42.246477
3503.249250	586043.067991	42.251482
3503.545999	585997.764555	42.256487
3503.378554	585955.089557	42.261492
3503.250825	585921.980905	42.266496
3503.242156	585884.593416	42.271501
3503.337139	585861.523702	42.276506
3503.456992	585819.254332	42.281511
3503.369632	585779.573293	42.286516
3502.905521	585749.122922	42.291520
3503.377930	585706.747882	42.296525
3503.093517	585679.877860	42.301530
3503.142766	585646.189385	42.306535
3502.705808	585619.894384	42.311540
3502.978811	585593.287850	42.316544
3503.085998	585556.282090	42.321549
3502.908815	585533.955920	42.326554
3502.849476	585500.183729	42.331559
3502.661294	585470.190652	42.336564
3502.685521	585442.920949	42.341568
3502.649165	585405.937120	42.346573
3502.728946	585394.948027	42.351578
3502.946634	585365.542790	42.356583
3502.792536	585324.968346	42.361588
3503.001677	585308.295191	42.366592
3503.415337	585269.987508	42.371597
3503.029324	585235.162884	42.376602
3502.899980	585214.883590	42.381607
3503.080937	585178.666975	42.386612
3503.069622	585143.081769	42.391616
3503.125345	585103.426029	42.396621
3503.041761	585078.878898	42.401626
3502.844106	585044.274835	42.406631
3502.656367	585016.886838	42.411636
3502.500658	584991.749311	42.416640
3502.968458	584967.316225	42.421645
3502.698831	584944.903058	42.426650
3503.001348	584920.345336	42.431655
3502.879979	584882.370557	42.436660
3502.880709	584868.937232	42.441664
3503.119624	584831.106447	42.446669
3502.638749	584810.630739	42.451674
3502.830414	584779.172912	42.456679
3502.920347	584752.242086	42.461684
3502.650569	584721.407598	42.466688
3503.120694	584689.705486	42.471693
3503.195287	584665.533698	42.476698
3503.052001	584638.238054	42.481703
3503.114124	584601.486736	42.486708
3503.147437	584565.642052	42.491712
3503.183694	584529.145162	42.496717
3502.776573	584506.000710	42.501722
3502.876004	584474.907308	42.506727
3502.967978	584440.406434	42.511732
3502.667179	584421.004609	42.516736
3503.195454	584395.157275	42.521741
3502.966231	584362.611155	42.526746
3502.925810	584326.777218	42.531751
3502.759124	584300.035778	42.536756
3502.649350	584280.754221	42.541760
3502.360093	584243.505245	42.546765
3502.281774	584231.988309	42.551770
3502.713881	584203.899859	42.556775
3502.781403	584172.058685	42.561780
3502.413034	584155.173300	42.566784
3502.479636	584112.955798	42.571789
3502.584156	584099.605560	42.576794
3502.639973	584067.615531	42.581799
3502.670457	584054.878342	42.586804
3502.347308	584031.318738	42.591808
3502.712721	584003.992118	42.596813
3502.622521	583983.955063	42.601818
3502.814307	583953.998688	42.606823
3502.832489	583931.839221	42.611828
3503.065193	583900.322333	42.616832
3502.920978	583861.796181	42.621837
3502.724356	583846.938734	42.626842
3502.513363	583808.472963	42.631847
3502.571921	583795.430312	42.636852
3502.487723	583772.985758	42.641856
3502.693723	583746.886511	42.646861
3502.964837	583723.183215	42.651866
3502.713527	583699.912443	42.656871
3502.991199	583666.583208	42.661876
3502.206983	583642.894331	42.666880
3502.684696	583612.591551	42.671885
3502.652864	583595.351915	42.676890
3502.678924	583568.779080	42.681895
3502.608146	583543.925734	42.686900
3502.312499	583523.819697	42.691904
3502.787755	583498.429718	42.696909
3502.625761	583475.395157	42.701914
3502.382809	583440.642723	42.706919
3502.829192	583430.246046	42.711924
3502.548655	583409.586005	42.716928
3502.659807	583373.374349	42.721933
3502.413513	583357.521392	42.726938
3502.753121	583335.561128	42.731943
3502.814718	583314.697031	42.736948
3502.639407	583279.031156	42.741952
3502.728986	583250.191725	42.746957
3502.866876	583237.286405	42.751962
3502.702859	583201.718776	42.756967
3502.659983	583170.794326	42.761972
3502.556043	583152.061323	42.766976
3502.478183	583118.685747	42.771981
3502.493985	583110.010430	42.776986
3502.515060	583078.574406	42.781991
3502.256575	583058.311312	42.786996
3502.265208	583031.689773	42.792001
3502.554872	583007.530849	42.797005
3502.442045	582988.247501	42.802010
3502.441608	582969.297475	42.807015
3502.592353	582936.787994	42.812020
3502.681955	582931.459882	42.817025
3502.905873	582894.827964	42.822029
3502.603027	582882.141527	42.827034
3502.638551	582859.325462	42.832039
3502.950626	582826.990968	42.837044
3502.511568	582800.539124	42.842049
3502.460199	582776.132209	42.847053
3502.288917	582744.625037	42.852058
3502.327201	582733.740037	42.857063
3502.409119	582716.731909	42.862068
3502.310423	582690.126324	42.867073
3502.792971	582664.983957	42.872077
3502.543298	582649.782247	42.877082
3502.803525	582619.059535	42.882087
3502.687915	582600.979160	42.887092
3502.932802	582573.016093	42.892097
3503.124945	582531.875855	42.897101
3502.704925	582517.953954	42.902106
3502.478841	582487.858380	42.907111
3502.673890	582464.465079	42.912116
3502.590516	582446.479681	42.917121
3502.582014	582418.355295	42.922125
3502.776412	582400.627208	42.927130
3502.638148	582361.543388	42.932135
3502.850708	582330.175566	42.937140
3502.643441	582306.945097	42.942145
3502.745844	582279.504916	42.947149
3502.773551	582266.214601	42.952154
3502.736389	582238.695865	42.957159
3502.760574	582205.401843	42.962164
3502.606365	582185.120841	42.967169
3502.545839	582158.959231	42.972173
3502.524444	582132.189807	42.977178
3502.349554	582112.262857	42.982183
3502.419159	582084.977729	42.987188
3502.498244	582069.272595	42.992193
3502.253741	582037.624440	42.997197
3502.384680	582022.913867	43.002202
3502.443845	581998.187130	43.007207
3502.743415	581984.753703	43.012212
3502.645101	581946.915592	43.017217
3502.856429	581928.482182	43.022221
3502.862532	581902.560235	43.027226
3502.579108	581867.608616	43.032231
3502.582257	581850.210369	43.037236
3502.474521	581825.108236	43.042241
3502.828116	581794.368636	43.047245
3502.471947	581780.134992	43.052250
3502.261161	581758.708880	43.057255
3502.595002	581730.830053	43.062260
3502.626821	581704.953760	43.067265
3502.631650	581684.195731	43.072269
3502.443776	581657.952567	43.077274
3502.558717	581635.973912	43.082279
3502.503719	581612.718177	43.087284
3502.205810	581604.993215	43.092289
3502.493814	581572.809232	43.097293
3502.341387	581562.053170	43.102298
3502.572608	581539.604896	43.107303
3502.282677	581522.903758	43.112308
3502.336983	581497.424576	43.117313
3502.439373	581488.333336	43.122317
3501.941159	581465.898667	43.127322
3502.278631	581449.951704	43.132327
3502.473148	581420.639836	43.137332
3502.263908	581417.062455	43.142337
3502.621238	581374.488182	43.147341
3502.285742	581359.047411	43.152346
3501.912759	581331.328216	43.157351
3502.372334	581314.609872	43.162356
3502.152130	581291.078447	43.167361
3502.565307	581274.668137	43.172365
3502.478556	581266.057544	43.177370
3502.394290	581237.641158	43.182375
3502.928216	581218.805154	43.187380
3502.686970	581199.839598	43.192385
3502.784334	581160.664555	43.197389
3502.287919	581132.011485	43.202394
3502.063319	581125.127119	43.207399
3502.269887	581105.740409	43.212404
3501.916388	581078.318380	43.217409
3502.099251	581066.205752	43.222413
3502.036004	581055.084267	43.227418
3501.797773	581019.621490	43.232423
3502.247573	581011.979787	43.237428
3501.967708	580997.833488	43.242433
3502.231216	580979.741333	43.247437
3502.225154	580971.168038	43.252442
3501.813854	580952.028076	43.257447
3502.185427	580942.041900	43.262452
3502.143729	580936.683213	43.267457
3502.409534	580913.125149	43.272461
3502.277673	580885.667993	43.277466
3502.123621	580863.328723	43.282471
3502.343183	580846.747481	43.287476
3502.224266	580844.008208	43.292481
3502.210581	580815.780273	43.297485
3502.145599	580792.424091	43.302490
3501.708563	580780.257634	43.307495
3502.241360	580776.764611	43.312500
3502.404916	580755.278034	43.317505
3502.346313	580733.124149	43.322509
3502.410003	580713.307808	43.327514
3502.390927	580695.861079	43.332519
3502.074127	580663.969580	43.337524
3502.227378	580654.368277	43.342529
3502.673944	580631.383072	43.347533
3502.255668	580614.851054	43.352538
3502.078895	580582.987575	43.357543
3502.571001	580567.516605	43.362548
3502.272386	580562.950051	43.367553
3502.127527	580530.078564	43.372557
3502.150736	580511.822639	43.377562
3502.327567	580486.472411	43.382567
3502.647192	580465.211593	43.387572
3502.030934	580441.539702	43.392577
3502.202248	580427.221852	43.397581
3502.491989	580411.631870	43.402586
3502.398262	580392.541581	43.407591
3502.226779	580367.546398	43.412596
3501.674081	580358.105344	43.417601
3501.948771	580339.458812	43.422605
3502.104018	580329.355473	43.427610
3502.000071	580318.490334	43.432615
3502.683229	580301.334360	43.437620
3501.961198	580292.020011	43.442625
3502.221531	580268.060278	43.447629
3502.156138	580249.015458	43.452634
3502.057918	580231.931385	43.457639
3502.517272	580213.907658	43.462644
3501.944660	580189.325796	43.467649
3502.094415	580177.117086	43.472653
3502.061734	580157.214527	43.477658
3502.236404	580151.019313	43.482663
3502.273706	580113.304174	43.487668
3502.071597	580109.424380	43.492673
3501.999846	580090.881736	43.497677
3502.231589	580077.857772	43.502682
3502.440285	580060.324292	43.507687
3502.164187	580036.899232	43.512692
3501.895652	580032.377901	43.517697
3501.877981	580003.396338	43.522701
3502.159271	579995.980869	43.527706
3502.215896	579984.187674	43.532711
3502.344388	579949.065310	43.537716
3502.446412	579941.577538	43.542721
3502.235433	579914.431224	43.547725
3502.288392	579898.626808	43.552730
3501.832050	579877.085003	43.557735
3502.271324	579853.848602	43.562740
3501.922245	579846.381140	43.567745
3502.107175	579826.644557	43.572749
3502.161758	579822.423654	43.577754
3501.858059	579800.105636	43.582759
3502.284967	579772.809108	43.587764
3502.399011	579763.965370	43.592769
3502.095789	579745.057160	43.597773
3502.246893	579727.532159	43.602778
3502.199836	579704.973241	43.607783
3502.257463	579695.536502	43.612788
3502.034423	579675.061072	43.617793
3502.318643	579650.444361	43.622797
3502.430105	579633.677621	43.627802
3502.190752	579611.800494	43.632807
3502.440810	579589.194893	43.637812
3502.378643	579571.552545	43.642817
3502.272128	579556.223904	43.647821
3502.192048	579534.271577	43.652826
3501.677434	579520.210236	43.657831
3502.118654	579500.934491	43.662836
3502.037424	579492.622546	43.667841
3501.986395	579472.771780	43.672845
3502.353615	579463.637483	43.677850
3501.998308	579450.303374	43.682855
3502.112072	579435.040426	43.687860
3501.997429	579415.901581	43.692865
3502.373933	579395.181463	43.697869
3502.239095	579371.933512	43.702874
3501.771521	579355.407321	43.707879
3501.929696	579341.190427	43.712884
3502.048475	579324.622674	43.717889
3502.330087	579309.584060	43.722893
3502.614748	579287.574226	43.727898
3502.374236	579287.210584	43.732903
3502.071988	579250.648882	43.737908
3502.553918	579240.694083	43.742913
3502.569432	579207.292119	43.747917
3502.618595	579193.844321	43.752922
3502.222432	579169.734110	43.757927
3501.969665	579157.236161	43.762932
3501.806689	579135.296007	43.767937
3502.628924	579118.317077	43.772941
3502.611133	579096.554749	43.777946
3501.989227	579074.585920	43.782951
3502.165366	579055.852348	43.787956
3502.136914	579035.345320	43.792961
3502.358984	579022.472088	43.797965
3501.884741	579006.197170	43.802970
3501.698752	578989.275361	43.807975
3501.939617	578981.564637	43.812980
3501.732846	578969.560792	43.817985
3501.907792	578949.723917	43.822989
3501.912533	578938.740136	43.827994
3501.772806	578929.634505	43.832999
3501.973157	578909.592984	43.838004
3502.071033	578896.438117	43.843009
3502.228477	578885.430411	43.848013
3502.051003	578868.055728	43.853018
3501.872567	578856.097482	43.858023
3502.199152	578837.490478	43.863028
3501.841364	578824.757818	43.868033
3502.062836	578820.059085	43.873037
3502.163568	578789.852225	43.878042
3502.045710	578783.250622	43.883047
3502.095164	578759.621523	43.888052
3501.905635	578747.163379	43.893057
3501.909684	578734.073141	43.898061
3501.781306	578718.847068	43.903066
3501.578718	578708.948657	43.908071
3502.180658	578688.442745	43.913076
3502.233326	578687.180668	43.918081
3502.226589	578658.143743	43.923085
3501.852137	578649.074577	43.928090
3501.836809	578625.003953	43.933095
3502.246129	578605.831956	43.938100
3502.502772	578595.360131	43.943105
3502.127818	578574.204293	43.948109
3502.412799	578575.112587	43.953114
3502.360628	578545.330187	43.958119
3502.517547	578504.832518	43.963124
3501.912813	578493.893426	43.968129
3501.942543	578475.683296	43.973133
3501.900897	578470.223107	43.978138
3502.180046	578448.764163	43.983143
3502.150828	578426.300174	43.988148
3502.211233	578426.140223	43.993153
3502.311012	578397.838264	43.998157
3502.209739	578385.115152	44.003162
3502.041363	578368.741332	44.008167
3501.909857	578344.939032	44.013172
3502.256350	578334.503070	44.018177
3502.182469	578320.220848	44.023181
3501.952971	578313.536113	44.028186
3502.012977	578292.361896	44.033191
3501.862063	578272.474453	44.038196
3502.129281	578260.044669	44.043201
3502.351818	578245.364936	44.048205
3502.059866	578230.966229	44.053210
3501.675259	578216.030295	44.058215
3502.356429	578204.588968	44.063220
3501.720839	578190.795624	44.068225
3502.122622	578170.119440	44.073229
3502.128406	578156.175632	44.078234
3501.982448	578134.230847	44.083239
3502.214382	578119.950715	44.088244
3502.443524	578101.658648	44.093249
3502.228230	578076.163623	44.098253
3502.076622	578071.623211	44.103258
3501.863570	578051.243543	44.108263
3502.029188	578028.246748	44.113268
3502.209229	578018.287906	44.118273
3502.063254	578001.609116	44.123277
3502.416238	577984.300595	44.128282
3502.526709	577961.663369	44.133287
3502.375404	577939.067021	44.138292
3502.172982	577923.600662	44.143297
3502.507021	577892.702887	44.148301
3502.467949	577872.496316	44.153306
3501.850472	577862.611857	44.158311
3502.124416	577848.074034	44.163316
3502.204942	577834.720008	44.168321
3502.111563	577825.405607	44.173325
3502.353799	577805.355560	44.178330
3501.908543	577787.820434	44.183335
3502.362988	577764.777946	44.188340
3502.036303	577751.788416	44.193345
3502.218440	577736.763241	44.198349
3502.254536	577711.930270	44.203354
3501.942405	577696.881998	44.208359
3502.040124	577661.355997	44.213364
3502.026977	577659.100965	44.218369
3501.924346	577646.477537	44.223373
3502.044093	577631.461974	44.228378
3501.671699	577618.278809	44.233383
3502.103543	577616.004359	44.238388
3501.939165	577601.233799	44.243393
3501.884547	577577.217217	44.248397
3502.143541	577568.148456	44.253402
3501.754453	577547.343977	44.258407
3502.377797	577526.782442	44.263412
3502.344777	577517.157406	44.268417
3502.165751	577494.163236	44.273421
3502.047704	577484.451150	44.278426
3501.958895	577459.887933	44.283431
3502.098738	577440.455129	44.288436
3501.960035	577426.683472	44.293441
3501.650688	577410.430600	44.298445
3501.851720	577404.731322	44.303450
3501.703769	577394.622572	44.308455
3501.979529	577372.961469	44.313460
3501.930150	577369.006681	44.318465
3501.977228	577352.748162	44.323469
3502.003996	577333.483323	44.328474
3501.759265	577318.875426	44.333479
3502.064055	577301.974650	44.338484
3502.061631	577286.125037	44.343489
3501.915933	577273.257131	44.348493
3502.542987	577262.726157	44.353498
3502.226553	577244.066557	44.358503
3502.230664	577227.363149	44.363508
3502.114604	577211.932463	44.368513
3502.139270	577195.125477	44.373517
3501.931755	577178.505239	44.378522
3501.954100	577154.124608	44.383527
3501.947834	577143.341419	44.388532
3501.671344	577132.048717	44.393537
3501.363277	577113.237115	44.398541
3501.776166	577105.247417	44.403546
3501.945489	577098.399286	44.408551
3502.072127	577080.071419	44.413556
3501.525347	577073.636176	44.418561
3501.948597	577056.265080	44.423565
3502.038812	577046.219102	44.428570
3501.800204	577035.070857	44.433575
3502.209107	577021.965484	44.438580
3501.777416	577020.929417	44.443585
3501.664512	576996.569588	44.448589
3502.142680	576981.045688	44.453594
3501.689536	576980.163449	44.458599
3502.031852	576961.500715	44.463604
3502.059937	576960.543244	44.468609
3501.955853	576937.736854	44.473613
3501.903808	576920.790970	44.478618
3502.022867	576915.003939	44.483623
3501.877020	576893.708781	44.488628
3501.823887	576873.703245	44.493633
3501.993466	576864.597736	44.498637
3501.786468	576850.434767	44.503642
3501.730540	576839.508570	44.508647
3501.988773	576817.999617	44.513652
3501.739222	576814.778168	44.518657
3501.874966	576802.668286	44.523661
3501.870472	576787.470376	44.528666
3501.802473	576782.364604	44.533671
3501.891498	576773.823378	44.538676
3501.602605	576746.330414	44.543681
3501.731980	576738.234297	44.548685
3502.045314	576727.802029	44.553690
3501.744512	576722.381500	44.558695
3501.841865	576697.185582	44.563700
3501.898528	576697.527799	44.568705
3502.176350	576678.724196	44.573709
3502.117794	576666.945507	44.578714
3501.664290	576661.548821	44.583719
3502.416310	576638.407344	44.588724
3502.021075	576618.555157	44.593729
3502.009659	576608.474514	44.598733
3502.245702	576583.356981	44.603738
3501.980115	576569.453622	44.608743
3502.008994	576557.310021	44.613748
3501.811974	576545.001076	44.618753
3501.943162	576522.809160	44.623757
3501.939559	576518.044332	44.628762
3502.037956	576489.888256	44.633767
3501.964781	576485.535582	44.638772
3502.102768	576469.813351	44.643777
3502.064941	576446.243178	44.648781
3502.024082	576444.443690	44.653786
3502.160196	576417.635907	44.658791
3502.277797	576403.421629	44.663796
3502.001187	576390.623336	44.668801
3501.693658	576367.245646	44.673805
3502.298484	576361.031256	44.678810
3501.834049	576346.958059	44.683815
3501.858869	576316.756398	44.688820
3502.156855	576323.933149	44.693825
3502.039052	576304.137359	44.698829
3502.109391	576275.383182	44.703834
3501.720792	576283.269245	44.708839
3501.752588	576250.457862	44.713844
3501.640279	576239.740545	44.718849
3502.039195	576235.263810	44.723853
3501.581912	576222.593896	44.728858
3501.517535	576211.116616	44.733863
3502.062584	576177.873644	44.738868
3501.775378	576189.756963	44.743873
3501.463891	576176.913716	44.748877
3501.873357	576154.828060	44.753882
3501.875775	576158.088237	44.758887
3501.924514	576136.761222	44.763892
3501.664640	576121.903314	44.768897
3501.678664	576112.420208	44.773901
3501.589768	576108.972786	44.778906
3501.821804	576114.554755	44.783911
3501.913958	576085.796684	44.788916
3501.743624	576070.724057	44.793921
3501.941159	576071.144598	44.798925
3501.827653	576052.350962	44.803930
3502.094679	576025.471615	44.808935
3501.822485	576028.273122	44.813940
3501.806018	576023.058621	44.818945
3501.884077	575989.336297	44.823949
3502.003442	575981.191037	44.828954
3502.050876	575971.200951	44.833959
3502.190399	575946.297741	44.838964
3502.104403	575936.177991	44.843969
3502.327458	575915.224618	44.848973
3502.415086	575899.007821	44.853978
3502.127841	575883.050262	44.858983
3502.105185	575859.677145	44.863988
3502.047941	575863.598871	44.868993
3502.030478	575825.476518	44.873997
3502.556619	575808.237910	44.879002
3501.879218	575804.782067	44.884007
3501.986962	575781.488731	44.889012
3501.759651	575781.775042	44.894017
3501.691982	575758.559246	44.899021
3502.009797	575738.293039	44.904026
3501.910465	575735.649774	44.909031
3502.178867	575723.467828	44.914036
3501.906298	575698.227173	44.919041
3501.726047	575693.389280	44.924045
3502.025739	575692.790562	44.929050
3501.680000	575662.946068	44.934055
3501.853125	575651.982907	44.939060
3502.030687	575645.232937	44.944065
3502.041756	575624.211833	44.949069
3502.354799	575615.233383	44.954074
3501.979504	575601.747301	44.959079
3502.077183	575580.261084	44.964084
3502.174841	575565.798039	44.969089
3502.007689	575537.380099	44.974093
3502.252231	575525.803661	44.979098
3501.681755	575507.431715	44.984103
3502.031422	575494.133165	44.989108
3502.155938	575489.648868	44.994113
3502.060424	575477.623881	44.999117
3501.749473	575448.877035	45.004122
3502.124407	575447.865213	45.009127
3501.954643	575417.691559	45.014132
3501.688539	575414.422126	45.019137
3501.745872	575399.463507	45.024141
3502.090116	575398.757478	45.029146
3501.817255	575379.335465	45.034151
3502.073739	575359.579833	45.039156
3501.626097	575361.656431	45.044161
3501.864413	575335.482261	45.049165
3502.140985	575317.429085	45.054170
3502.029296	575320.306007	45.059175
3502.090929	575297.620883	45.064180
3502.095536	575286.031542	45.069185
3502.123260	575260.492124	45.074189
3501.914368	575242.263886	45.079194
3501.714521	575233.866986	45.084199
3502.302764	575220.681320	45.089204
3502.088602	575197.286600	45.094209
3502.121808	575188.702731	45.099213
3502.335020	575166.495322	45.104218
3502.235111	575165.005865	45.109223
3502.275273	575136.404002	45.114228
3501.854960	575120.466163	45.119233
3502.076660	575106.585150	45.124237
3502.004483	575081.913799	45.129242
3501.681932	575079.857122	45.134247
3502.165806	575065.132386	45.139252
3502.154972	575036.437905	45.144257
3501.928963	575027.141915	45.149261
3501.943648	575005.868252	45.154266
3501.539829	574993.589936	45.159271
3501.922363	574981.740527	45.164276
3502.024116	574977.410092	45.169281
3501.680367	574953.182260	45.174285
3501.862761	574955.963132	45.179290
3502.144983	574949.296723	45.184295
3501.955694	574932.870985	45.189300
3501.962258	574917.367809	45.194305
3501.636536	574900.712510	45.199309
3501.593201	574873.327082	45.204314
3501.369036	574872.559376	45.209319
3501.657487	574858.667624	45.214324
3501.750280	574869.640053	45.219329
3501.855721	574853.569475	45.224333
3502.104480	574840.536777	45.229338
3502.088234	574816.558468	45.234343
3501.810948	574809.477754	45.239348
3501.699223	574795.849161	45.244353
3501.552020	574774.650540	45.249357
3501.623682	574778.151136	45.254362
3501.682106	574773.225365	45.259367
3501.834978	574757.398082	45.264372
3501.642871	574741.373860	45.269377
3501.528587	574732.862871	45.274381
3502.081056	574726.655778	45.279386
3501.453605	574703.575490	45.284391
3501.853555	574690.920342	45.289396
3501.936698	574686.291686	45.294401
3501.782060	574679.091377	45.299405
3501.571835	574660.912576	45.304410
3501.535966	574657.857777	45.309415
3501.639675	574649.613665	45.314420
3501.377893	574651.661334	45.319425
3501.460032	574649.039612	45.324429
3501.773266	574618.738144	45.329434
3501.660556	574613.186847	45.334439
3501.642982	574607.570504	45.339444
3501.709788	574597.224982	45.344449
3501.462813	574583.617277	45.349453
3501.955504	574563.472137	45.354458
3501.826177	574570.215112	45.359463
3501.908079	574555.853577	45.364468
3501.906154	574536.387756	45.369473
3501.868436	574526.560213	45.374477
3501.843410	574520.142266	45.379482
3501.711578	574498.740042	45.384487
3501.946988	574485.357829	45.389492
3501.830259	574485.225516	45.394497
3501.802307	574469.827464	45.399501
3501.888497	574435.547348	45.404506
3501.814638	574443.034289	45.409511
3502.156680	574420.554421	45.414516
3501.677836	574407.384118	45.419521
3501.731893	574399.849979	45.424525
3502.120825	574390.908868	45.429530
3501.943778	574374.430232	45.434535
3502.168431	574360.748528	45.439540
3502.030373	574349.180528	45.444545
3501.926009	574337.406564	45.449549
3502.234462	574317.540646	45.454554
3501.832338	574305.361655	45.459559
3501.750261	574290.021990	45.464564
3502.019330	574279.995759	45.469569
3501.959106	574268.064308	45.474573
3501.930014	574242.732158	45.479578
3502.002889	574244.677410	45.484583
3501.736854	574231.674319	45.489588
3501.874204	574216.350423	45.494593
3501.422708	574199.964608	45.499597
3501.760422	574193.991487	45.504602
3501.673935	574185.726599	45.509607
3501.852942	574159.508808	45.514612
3501.920153	574155.333975	45.519617
3501.943590	574149.710993	45.524621
3501.701464	574140.366619	45.529626
3501.618850	574125.227502	45.534631
3502.005160	574113.677631	45.539636
3501.669982	574111.572575	45.544641
3501.432205	574083.061669	45.549645
3501.794638	574073.020659	45.554650
3501.493777	574071.211265	45.559655
3501.598602	574057.246893	45.564660
3501.659013	574050.965840	45.569665
3501.108404	574034.745797	45.574669
3501.647343	574025.931467	45.579674
3501.731642	574030.333427	45.584679
3501.758796	574019.893231	45.589684
3501.610348	574022.123984	45.594689
3501.326149	573993.971319	45.599693
3501.533827	573979.338526	45.604698
3501.324514	573984.639342	45.609703
3501.697576	573968.174460	45.614708
3501.540889	573970.306166	45.619713
3501.169343	573974.628892	45.624717
3501.853146	573960.523716	45.629722
3501.337347	573934.012639	45.634727
3501.718945	573930.139785	45.639732
3501.440250	573927.624480	45.644737
3501.641415	573926.890560	45.649741
3502.135222	573916.728529	45.654746
3501.691204	573892.363576	45.659751
3501.949906	573884.746929	45.664756
3501.655487	573871.798034	45.669761
3501.689584	573853.579738	45.674765
3501.922516	573843.408251	45.679770
3501.578543	573839.698969	45.684775
3501.677029	573823.577842	45.689780
3501.723467	573809.471773	45.694785
3501.647024	573802.057985	45.699789
3501.760893	573797.925899	45.704794
3501.691119	573794.625299	45.709799
3501.488274	573768.666993	45.714804
3501.350301	573762.165926	45.719809
3501.628090	573749.528827	45.724813
3501.927626	573746.622043	45.729818
3501.868097	573743.771391	45.734823
3501.580305	573708.845105	45.739828
3501.466125	573655.628163	45.744833
3501.060929	573547.515281	45.749837
3501.606838	573392.138073	45.754842
3501.044869	573197.092047	45.759847
3500.698958	572949.473313	45.764852
3500.381897	572665.967014	45.769857
3499.777878	572313.350438	45.774861
3499.675756	571932.392123	45.779866
3498.671444	571500.023512	45.784871
3498.392383	571027.978761	45.789876
3497.450754	570499.054675	45.794881
3496.819784	569943.858112	45.799885
3495.933834	569333.261294	45.804890
3494.507242	568690.691479	45.809895
3493.605549	568003.427031	45.814900
3492.689840	567278.773425	45.819905
3491.786368	566520.936881	45.824909
3490.632974	565707.207325	45.829914
3489.051660	564856.832437	45.834919
3487.789537	563970.089268	45.839924
3486.385353	563053.419833	45.844929
3484.604698	562087.969523	45.849933
3483.402481	561079.755399	45.854938
3481.372398	560057.519133	45.859943
3480.109195	558986.394259	45.864948
3478.312965	557884.758876	45.869953
3476.382968	556754.100091	45.874957
3474.909526	555587.985993	45.879962
3472.228483	554382.294474	45.884967
3470.348101	553145.596514	45.889972
3468.508801	551887.854317	45.894977
3466.317763	550610.480652	45.899981
3464.029822	549291.458495	45.904986
3461.479909	547968.714696	45.909991
3459.157192	546593.794046	45.914996
3456.857116	545200.711179	45.920001
3454.256770	543797.659883	45.925005
3451.671703	542365.019040	45.930010
3449.419013	540906.201241	45.935015
3447.307667	539432.549662	45.940020
3444.327241	537936.115789	45.945025
3441.521465	536404.499050	45.950029
3438.688738	534869.330363	45.955034
3435.312697	533322.836790	45.960039
3433.200651	531745.499656	45.965044
3429.906341	530159.645799	45.970049
3427.082450	528557.561382	45.975053
3424.064401	526939.244752	45.980058
3421.085692	525313.016460	45.985063
3418.559978	523666.970987	45.990068
3415.354051	522005.310211	45.995073
3411.888711	520348.977041	46.000077
3408.817810	518659.116513	46.005082
3405.244137	516965.999382	46.010087
3402.345736	515256.687706	46.015092
3399.004716	513543.300339	46.020097
3395.642039	511828.040302	46.025101
3392.266219	510101.728823	46.030106
3389.019948	508371.956609	46.035111
3386.000716	506615.505419	46.040116
3382.552147	504870.355726	46.045121
3379.026656	503097.860716	46.050125
3375.715933	501337.173723	46.055130
3371.925803	499572.915918	46.060135
3368.935706	497795.550010	46.065140
3365.310492	496013.928962	46.070145
3361.314813	494201.860276	46.075149
3358.219546	492401.648940	46.080154
3354.414333	490614.411049	46.085159
3350.304350	488815.343019	46.090164
3347.113494	487015.009167	46.095169
3343.579892	485217.750122	46.100173
3339.726070	483416.037399	46.105178
3335.787147	481617.362631	46.110183
3332.485081	479800.392020	46.115188
3328.930384	477998.968730	46.120193
3325.354066	476191.279172	46.125197
3321.294385	474376.889459	46.130202
3317.636867	472574.214108	46.135207
3313.956870	470759.157015	46.140212
3310.132917	468944.578424	46.145217
3306.298802	467151.395822	46.150221
3302.802139	465338.899308	46.155226
3298.982751	463535.817158	46.160231
3295.216589	461727.576378	46.165236
3291.803942	459921.010607	46.170241
3287.807477	458115.357702	46.175245
3284.044022	456299.662496	46.180250
3280.241967	454502.104581	46.185255
3276.085256	452696.016118	46.190260
3272.507115	450893.702477	46.195265
3268.176410	449107.524362	46.200269
3264.696564	447315.517279	46.205274
3261.088024	445518.796232	46.210279
3257.447211	443733.652149	46.215284
3253.124944	441941.047820	46.220289
3249.711865	440159.119489	46.225293
3246.196041	438378.101754	46.230298
3242.133932	436594.671537	46.235303
3237.863179	434809.688744	46.240308
3234.309161	433040.287518	46.245313
3230.451381	431263.526426	46.250317
3227.027672	429493.479144	46.255322
3222.856326	427730.941870	46.260327
3218.974267	425956.292352	46.265332
3215.335038	424204.918141	46.270337
3211.464038	422452.972875	46.275341
3207.527938	420683.346055	46.280346
3203.827243	418927.423792	46.285351
3199.843134	417179.308550	46.290356
3196.245141	415424.801011	46.295361
3192.161446	413678.542118	46.300365
3188.548122	411942.008785	46.305370
3184.702560	410213.742117	46.310375
3180.961798	408481.619364	46.315380
3176.979161	406754.421086	46.320385
3173.345402	405028.150680	46.325389
3169.123606	403305.036511	46.330394
3165.203121	401590.015897	46.335399
3161.654413	399876.230010	46.340404
3157.952045	398169.497462	46.345409
3154.159972	396467.324064	46.350413
3150.686759	394751.121285	46.355418
3145.858928	393058.814600	46.360423
3142.703418	391358.056084	46.365428
3138.676337	389674.754565	46.370433
3134.902632	387982.971797	46.375437
3130.862088	386283.474092	46.380442
3126.978917	384615.980503	46.385447
3123.416812	382934.311421	46.390452
3119.665252	381262.566903	46.395457
3115.699920	379598.036618	46.400461
3111.774664	377932.785171	46.405466
3108.432333	376278.945054	46.410471
3104.652869	374612.397241	46.415476
3100.812623	372956.171129	46.420481
3097.046751	371304.609255	46.425485
3093.489643	369648.343923	46.430490
3089.368313	368002.079024	46.435495
3085.646185	366363.710428	46.440500
3081.905543	364728.605381	46.445505
3077.876874	363094.368339	46.450509
3074.440432	361457.076628	46.455514
3070.475683	359832.051924	46.460519
3066.870840	358209.856918	46.465524
3063.231364	356577.898061	46.470529
3059.519948	354958.572683	46.475533
3055.966425	353334.360406	46.480538
3051.755607	351725.495545	46.485543
3048.143574	350119.456144	46.490548
3044.338628	348495.598001	46.495553
3040.539834	346897.920815	46.500557
3036.732367	345292.541431	46.505562
3033.190337	343697.773952	46.510567
3029.388099	342100.583040	46.515572
3026.068867	340506.116657	46.520577
3022.018924	338909.556528	46.525581
3018.153620	337318.974068	46.530586
3014.651457	335730.630240	46.535591
3010.460659	334144.029573	46.540596
3007.019128	332570.520478	46.545601
3003.033928	331001.227770	46.550605
2999.425865	329417.441245	46.555610
2995.298652	327854.147875	46.560615
2991.761134	326290.598960	46.565620
2988.334621	324727.938686	46.570625
2984.452209	323175.898179	46.575629
2981.447693	321618.701661	46.580634
2977.190359	320066.935425	46.585639
2973.475243	318508.845962	46.590644
2969.860655	316959.539301	46.595649
2966.109116	315409.411274	46.600653
2962.435677	313859.853975	46.605658
2958.624624	312326.474695	46.610663
2955.102450	310784.424622	46.615668
2951.374895	309248.820304	46.620673
2947.674890	307715.707857	46.625677
2944.238526	306173.039742	46.630682
2940.239292	304641.177490	46.635687
2936.250949	303116.444762	46.640692
2932.777898	301589.398265	46.645697
2929.017609	300075.129712	46.650701
2925.344130	298544.846915	46.655706
2921.421430	297035.712410	46.660711
2917.976747	295521.321411	46.665716
2914.348401	294005.672348	46.670721
2910.389732	292508.160116	46.675725
2907.056350	291003.869203	46.680730
2903.446906	289498.770375	46.685735
2899.760741	287994.233356	46.690740
2896.305402	286490.847359	46.695745
2892.394215	285001.042314	46.700749
2888.887752	283500.245231	46.705754
2885.252297	282003.687798	46.710759
2881.568066	280505.732008	46.715764
2877.999901	279002.762954	46.720769
2874.009397	277511.669317	46.725773
2870.698907	276023.216085	46.730778
2866.816300	274531.463829	46.735783
2863.106404	273047.474474	46.740788
2859.415282	271558.287511	46.745793
2855.608309	270084.498459	46.750797
2852.319011	268604.900809	46.755802
2848.442941	267125.346185	46.760807
2844.822604	265659.606936	46.765812
2841.116985	264182.044286	46.770817
2837.370848	262710.935150	46.775821
2833.781981	261241.895124	46.780826
2830.324765	259787.025106	46.785831
2826.551022	258326.456888	46.790836
2822.810112	256855.170529	46.795841
2818.650672	255404.051146	46.800845
2815.436931	253945.332062	46.805850
2811.997642	252492.821683	46.810855
2808.173246	251039.720748	46.815860
2804.324852	249598.299641	46.820865
2800.221288	248160.700661	46.825869
2797.157668	246714.548560	46.830874
2793.512104	245269.546093	46.835879
2789.947980	243840.871055	46.840884
2786.159029	242405.752943	46.845889
2782.487900	240975.905116	46.850893
2779.221705	239534.143233	46.855898
2775.337961	238110.120320	46.860903
2771.867190	236678.080175	46.865908
2768.132723	235248.724242	46.870913
2764.451287	233829.058593	46.875917
2761.055852	232388.484912	46.880922
2757.221700	230970.465263	46.885927
2753.668759	229535.894860	46.890932
2750.305320	228121.311275	46.895937
2746.205240	226707.401769	46.900941
2742.638412	225288.085070	46.905946
2739.361553	223875.472254	46.910951
2735.280221	222459.394751	46.915956
2731.902777	221051.918881	46.920961
2727.852231	219653.719104	46.925965
2724.744551	218239.609235	46.930970
2720.674240	216830.925358	46.935975
2717.188147	215425.948996	46.940980
2713.433400	214017.224518	46.945985
2709.980912	212625.292899	46.950989
2706.260310	211226.812823	46.955994
2702.788470	209834.820396	46.960999
2699.051194	208442.240043	46.966004
2695.689845	207046.756402	46.971009
2691.842188	205652.045082	46.976013
2688.257250	204261.937075	46.981018
2684.670118	202879.861557	46.986023
2681.261456	201490.179274	46.991028
2677.312144	200098.860971	46.996033
2673.521341	198731.188480	47.001037
2670.267803	197342.688728	47.006042
2666.518697	195981.426797	47.011047
2663.014970	194607.253840	47.016052
2659.172274	193228.564156	47.021057
2655.643019	191848.465155	47.026061
2652.318581	190480.089151	47.031066
2648.612986	189106.491929	47.036071
2644.714008	187742.949227	47.041076
2641.451494	186372.779653	47.046081
2637.210540	185008.408490	47.051085
2633.765438	183643.370937	47.056090
2630.578741	182287.020357	47.061095
2626.824475	180923.240815	47.066100
2623.035116	179556.023986	47.071105
2619.678165	178208.086193	47.076109
2615.903896	176855.320426	47.081114
2611.908483	175505.691714	47.086119
2608.257131	174150.569950	47.091124
2604.998202	172812.137301	47.096129
2601.165140	171469.145483	47.101133
2597.570731	170113.512069	47.106138
2593.459396	168793.512535	47.111143
2590.200960	167446.913872	47.116148
2586.673614	166122.607903	47.121153
2583.103976	164790.161974	47.126157
2579.769839	163462.593237	47.131162
2575.625709	162130.990198	47.136167
2571.987146	160810.167048	47.141172
2568.816578	159476.252180	47.146177
2565.070645	158167.376451	47.151181
2561.448871	156836.911247	47.156186
2557.659694	155509.849046	47.161191
2553.834191	154189.656804	47.166196
2550.189154	152873.259100	47.171201
2546.653259	151572.222683	47.176205
2543.061554	150258.423364	47.181210
2539.342009	148964.400219	47.186215
2535.997408	147651.427352	47.191220
2532.237550	146334.658374	47.196225
2528.690658	144964.013958	47.201229
2525.110539	143667.364577	47.206234
2521.769819	142366.779657	47.211239
2517.992490	141066.119226	47.216244
2514.695621	139777.938114	47.221249
2510.734685	138482.109236	47.226253
2507.092286	137178.518227	47.231258
2503.469353	135895.608820	47.236263
2500.071661	134607.522445	47.241268
2496.171821	133320.391067	47.246273
2492.765534	132043.307567	47.251277
2489.139538	130748.970154	47.256282
2485.886548	129476.657399	47.261287
2482.142098	128197.005656	47.266292
2478.486079	126908.551699	47.271297
2475.061975	125626.244797	47.276301
2471.228717	124356.417337	47.281306
2467.854899	123076.230631	47.286311
2464.202862	121800.007447	47.291316
2460.462074	120518.409095	47.296321
2456.910326	119252.757812	47.301325
2453.266142	117983.894448	47.306330
2449.327213	116712.207531	47.311335
2445.801848	115455.452719	47.316340
2442.676353	114185.021610	47.321345
2438.435399	112932.838687	47.326349
2435.225847	111670.353345	47.331354
2431.466121	110414.139344	47.336359
2427.849950	109163.299760	47.341364
2424.213775	107912.736709	47.346369
2420.516353	106670.783883	47.351373
2417.067734	105415.362111	47.356378
2413.649624	104171.930932	47.361383
2409.763194	102924.284431	47.366388
2405.970744	101680.101884	47.371393
2402.339424	100449.032689	47.376397
2398.771925	99203.663296	47.381402
2395.099310	97978.769507	47.386407
2391.464303	96756.013689	47.391412
2388.558190	95521.232490	47.396417
2384.220454	94296.394487	47.401421
2380.722894	93069.363905	47.406426
2377.135123	91845.585742	47.411431
2373.546158	90631.729660	47.416436
2369.936644	89393.670171	47.421441
2365.954985	88187.762770	47.426445
2362.537922	86965.731818	47.431450
2359.085539	85762.038534	47.436455
2355.225856	84554.622132	47.441460
2351.649479	83359.076606	47.446465
2347.785049	82158.913334	47.451469
2344.294970	80958.869207	47.456474
2340.727369	79765.340705	47.461479
2337.074166	78577.160195	47.466484
2333.390187	77393.048789	47.471489
2329.594436	76205.957892	47.476493
2326.388953	75020.515348	47.481498
2322.778157	73837.473945	47.486503
2318.814016	72653.498717	47.491508
2315.279638	71476.162498	47.496513
2311.466351	70300.306366	47.501517
2308.330791	69115.325270	47.506522
2304.758936	67957.508822	47.511527
2300.837185	66784.126561	47.516532
2297.414451	65618.768480	47.521537
2293.536265	64465.658044	47.526541
2290.009945	63297.611138	47.531546
2286.403264	62147.439605	47.536551
2282.487518	60999.781159	47.541556
2279.160478	59841.866952	47.546561
2275.334214	58696.294517	47.551565
2271.811295	57557.359385	47.556570
2268.194152	56406.405300	47.561575
2264.343772	55272.324687	47.566580
2261.061245	54135.347794	47.571585
2257.267182	52995.130390	47.576589
2253.858655	51868.248973	47.581594
2249.816877	50732.481408	47.586599
2245.805021	49609.857090	47.591604
2242.464367	48498.491779	47.596609
2238.676449	47378.491175	47.601613
2235.241457	46259.416388	47.606618
2231.465947	45159.996155	47.611623
2227.528447	44058.955431	47.616628
2224.170369	42954.618826	47.621633
2220.385499	41866.205742	47.626637
2216.444955	40764.859490	47.631642
2212.792026	39681.929703	47.636647
2209.186321	38596.548278	47.641652
2205.636095	37516.892925	47.646657
2201.557009	36457.280281	47.651661
2197.837725	35379.521083	47.656666
2194.487581	34313.846767	47.661671
2190.569877	33251.236884	47.666676
2186.861753	32192.811988	47.671681
2182.990403	31140.506081	47.676685
2179.256078	30095.849614	47.681690
2175.642732	29061.898779	47.686695
2171.766699	28026.418657	47.691700
2167.947216	26995.385925	47.696705
2163.713616	25974.703204	47.701709
2159.944453	24958.161908	47.706714
2156.487182	23948.959696	47.711719
2152.356860	22957.443368	47.716724
2149.284139	21964.113005	47.721729
2144.919220	20985.312871	47.726733
2141.212289	19994.555929	47.731738
2137.231273	19026.472703	47.736743
2133.565298	18065.861878	47.741748
2129.802736	17097.681706	47.746753
2125.799697	16164.660380	47.751757
2122.149708	15206.788383	47.756762
2118.223319	14281.458341	47.761767
2114.235751	13356.144638	47.766772
2110.347321	12435.792937	47.771777
2105.803518	11544.020521	47.776781
2102.110767	10651.764539	47.781786
2097.511203	9787.960763	47.786791
2092.902350	8937.780887	47.791796
2087.747224	8114.177030	47.796801
2081.878980	7340.982900	47.801805
2076.821098	6567.219573	47.806810
2071.913062	5834.269455	47.811815
2066.686126	5123.877429	47.816820
2061.595741	4441.067866	47.821825
2056.634570	3802.218258	47.826829
2051.976780	3181.852046	47.831834
2046.857286	2592.693561	47.836839
2042.179125	2026.542535	47.841844
2037.747642	1492.666412	47.846849
2032.803052	993.304284	47.851853
2027.801769	519.301483	47.856858
2020.129111	150.784304	47.861863
1999.763768	163.399189	47.866868
1985.415477	159.683643	47.871873
1977.906588	171.179029	47.876877
1975.152335	160.992104	47.881882
1974.923886	163.843622	47.886887
1975.126560	171.047569	47.891892
1975.103781	164.922719	47.896897
1974.129080	160.715415	47.901901
1972.426314	161.121022	47.906906
1969.931281	152.671621	47.911911
1966.799198	158.986311	47.916916
1963.466954	162.073566	47.921921
1959.772065	168.084012	47.926925
1956.797705	158.621255	47.931930
1953.660905	154.429571	47.936935
1950.541175	159.018038	47.941940
1947.307475	149.387058	47.946945
1944.067077	163.634632	47.951949
1940.887357	159.579384	47.956954
1937.872113	156.722807	47.961959
1934.532491	157.751565	47.966964
1931.084082	155.854975	47.971969
1927.657180	169.021234	47.976973
1924.379679	157.729767	47.981978
1921.627728	153.867023	47.986983
1918.272715	156.350397	47.991988
1915.236493	155.012589	47.996993
1911.007823	156.341832	48.001997
1907.931274	154.988190	48.007002
1904.731548	142.738583	48.012007
1900.701558	154.977292	48.017012
1898.120241	151.704802	48.022017
1895.030047	162.018374	48.027021
1891.483748	155.239493	48.032026
1887.308791	164.707228	48.037031
1884.204569	144.150259	48.042036
1880.855523	157.956086	48.047041
1877.140671	161.834087	48.052045
1873.649208	150.639405	48.057050
1870.961436	151.214990	48.062055
1866.877236	153.825143	48.067060
1863.711853	145.499664	48.072065
1860.292539	160.828807	48.077069
1857.123172	146.834354	48.082074
1853.150904	149.240330	48.087079
1849.572910	151.496020	48.092084
1846.648289	141.686998	48.097089
1843.162537	155.549026	48.102093
1839.182668	154.662642	48.107098
1836.234792	152.311260	48.112103
1833.092916	155.406728	48.117108
1829.952031	147.966464	48.122113
1826.229975	153.797694	48.127117
1822.181822	155.671377	48.132122
1819.452938	150.305395	48.137127
1815.139310	154.232826	48.142132
1812.041275	144.640784	48.147137
1808.517538	146.574776	48.152141
1805.402711	144.825349	48.157146
1801.760414	157.582397	48.162151
1797.960960	153.219213	48.167156
1794.869055	147.872084	48.172161
1791.164617	150.843624	48.177165
1787.640975	149.404960	48.182170
1784.334999	138.089546	48.187175
1780.770558	149.752378	48.192180
1777.207259	141.963781	48.197185
1773.923354	143.895053	48.202189
1770.174349	152.030624	48.207194
1767.270637	139.377237	48.212199
1763.483970	158.677549	48.217204
1759.937717	141.160663	48.222209
1756.605842	148.383049	48.227213
1753.291853	145.873849	48.232218
1749.804581	151.203274	48.237223
1745.686387	150.060157	48.242228
1742.709587	153.322809	48.247233
1738.964301	150.390717	48.252237
1735.619149	140.761448	48.257242
1732.234888	139.883136	48.262247
1728.686405	149.936257	48.267252
1725.195052	141.785237	48.272257
1721.450183	139.517493	48.277261
1718.295427	145.051157	48.282266
1714.490674	143.539452	48.287271
1711.361805	150.657311	48.292276
1708.526276	136.806841	48.297281
1704.843571	144.761205	48.302285
1700.980807	138.351482	48.307290
1697.589851	132.117865	48.312295
1693.423843	136.215229	48.317300
1690.151398	131.706339	48.322305
1686.730776	147.140115	48.327309
1683.360508	145.364265	48.332314
1679.819171	142.365476	48.337319
1676.519900	152.623223	48.342324
1672.962142	143.384766	48.347329
1669.250148	145.085669	48.352333
1666.051631	147.712307	48.357338
1662.716150	146.155651	48.362343
1659.106439	152.741324	48.367348
1655.371158	149.674818	48.372353
1652.126877	149.654170	48.377357
1648.293657	150.921625	48.382362
1644.874173	143.863565	48.387367
1641.531440	141.944211	48.392372
1638.789353	133.185569	48.397377
1635.176939	140.398106	48.402381
1630.793227	134.933674	48.407386
1627.631380	140.996829	48.412391
1623.858073	144.286094	48.417396
1620.523623	138.575184	48.422401
1617.121281	132.273777	48.427405
1613.207805	138.574800	48.432410
1610.354120	138.686025	48.437415
1606.595911	142.640500	48.442420
1603.481968	135.695994	48.447425
1599.652744	137.687358	48.452429
1596.306826	143.171876	48.457434
1592.444800	144.529283	48.462439
1588.829174	143.377176	48.467444
1585.615452	135.290333	48.472449
1582.378517	140.476217	48.477453
1578.961813	123.568764	48.482458
1575.413751	131.989315	48.487463
1572.031915	143.168023	48.492468
1568.093792	128.794148	48.497473
1564.409340	140.064513	48.502477
1561.304678	132.672472	48.507482
1557.619549	127.405628	48.512487
1553.657314	145.401477	48.517492
1550.870949	137.734986	48.522497
1547.066167	136.406853	48.527501
1543.516561	134.766692	48.532506
1540.339706	138.984544	48.537511
1536.851305	142.529809	48.542516
1533.131281	135.398613	48.547521
1529.852328	131.292604	48.552525
1526.599403	132.652776	48.557530
1522.912818	138.019790	48.562535
1518.937989	145.412478	48.567540
1515.591718	131.778076	48.572545
1512.407710	149.436988	48.577549
1508.414282	135.293263	48.582554
1505.227991	141.338129	48.587559
1501.936540	139.809439	48.592564
1498.468578	130.974634	48.597569
1494.984167	131.845854	48.602573
1491.283325	134.487892	48.607578
1487.763867	131.457279	48.612583
1483.780212	138.006616	48.617588
1480.836406	137.647918	48.622593
1477.236772	133.041618	48.627597
1473.606453	129.506332	48.632602
1470.694423	124.153316	48.637607
1466.757076	128.521862	48.642612
1463.399519	131.398084	48.647617
1459.636216	124.586917	48.652621
1456.417360	134.265795	48.657626
1453.149880	126.930920	48.662631
1449.346604	133.983555	48.667636
1445.658766	135.136577	48.672641
1442.164977	139.299660	48.677645
1438.590895	128.102297	48.682650
1435.132008	135.629389	48.687655
1431.742250	134.900739	48.692660
1429.085810	133.921260	48.697665
1424.964071	136.717792	48.702669
1421.598232	133.796037	48.707674
1417.644273	131.852213	48.712679
1413.277967	136.673912	48.717684
1410.496163	125.861922	48.722689
1407.173920	141.071538	48.727693
1404.330130	137.903552	48.732698
1400.710010	138.131645	48.737703
1396.630361	137.276877	48.742708
1393.352920	128.048455	48.747713
1389.757677	131.113769	48.752717
1386.273378	134.168045	48.757722
1382.755450	128.239173	48.762727
1379.007917	139.883302	48.767732
1376.112699	135.094007	48.772737
1372.512196	126.855820	48.777741
1368.931717	137.363300	48.782746
1365.235721	132.284901	48.787751
1361.578360	137.204456	48.792756
1358.116596	128.071342	48.797761
1354.927110	139.574337	48.802765
1351.084453	133.285012	48.807770
1347.722827	133.431530	48.812775
1343.993289	128.488108	48.817780
1340.626966	127.910850	48.822785
1337.040186	125.830487	48.827789
1333.738254	122.212214	48.832794
1330.914824	124.799215	48.837799
1327.054658	129.848606	48.842804
1323.782470	127.016634	48.847809
1319.598843	128.459288	48.852813
1316.243639	128.446621	48.857818
1312.859620	122.348117	48.862823
1309.164526	122.676567	48.867828
1305.899443	127.772016	48.872833
1302.277595	124.172197	48.877837
1298.668193	122.974932	48.882842
1295.482888	126.681635	48.887847
1291.354152	129.466658	48.892852
1288.191910	123.067685	48.897857
1284.645437	121.563175	48.902861
1281.144974	122.595173	48.907866
1278.078203	119.607672	48.912871
1274.137608	125.827628	48.917876
1271.163609	119.465634	48.922881
1267.121561	124.916847	48.927885
1263.302132	127.229509	48.932890
1260.326153	120.402747	48.937895
1256.425755	119.349132	48.942900
1253.428032	116.977266	48.947905
1249.510543	119.760873	48.952909
1246.563221	119.399633	48.957914
1242.944881	119.953378	48.962919
1239.181014	121.554983	48.967924
1235.993850	119.206452	48.972929
1232.153025	122.373541	48.977933
1228.681457	123.467473	48.982938
1224.897540	116.985512	48.987943
1221.485685	124.343943	48.992948
1218.030114	118.380068	48.997953
1214.933715	126.986280	49.002957
1211.235186	128.267613	49.007962
1208.054777	121.476038	49.012967
1204.442759	123.262695	49.017972
1201.098738	120.207892	49.022977
1197.519838	126.260516	49.027981
1193.345076	123.367409	49.032986
1189.976190	116.102304	49.037991
1186.610259	121.574249	49.042996
1183.443730	118.830193	49.048001
1179.946226	122.611116	49.053005
1175.843319	127.572009	49.058010
1172.526466	107.760577	49.063015
1168.880861	115.930748	49.068020
1165.636411	120.475666	49.073025
1162.054718	120.441563	49.078029
1158.648990	119.386474	49.083034
1155.520466	117.351500	49.088039
1151.763159	119.856961	49.093044
1148.542131	115.596493	49.098049
1145.157071	110.289176	49.103053
1141.093245	126.836168	49.108058
1137.736418	117.449441	49.113063
1134.121412	123.846265	49.118068
1130.808285	117.777866	49.123073
1127.315400	117.587500	49.128077
1123.894144	117.309989	49.133082
1120.080707	113.904759	49.138087
1116.358700	119.511568	49.143092
1113.179687	111.194859	49.148097
1109.783618	123.492721	49.153101
1106.128645	120.350592	49.158106
1102.673748	113.972202	49.163111
1099.320337	114.544634	49.168116
1095.761658	115.639596	49.173121
1092.261272	117.883387	49.178125
1088.758324	119.339792	49.183130
1085.180135	109.858033	49.188135
1081.286842	110.831379	49.193140
1077.968359	112.904323	49.198145
1074.594713	116.431766	49.203149
1071.084120	115.703182	49.208154
1067.984704	106.845674	49.213159
1064.228517	115.112286	49.218164
1060.556114	104.550614	49.223169
1057.150918	121.798112	49.228173
1053.566419	119.170164	49.233178
1050.335926	109.415680	49.238183
1046.423089	115.507978	49.243188
1043.154563	119.170835	49.248193
1039.789920	118.780085	49.253197
1036.190480	122.966164	49.258202
1032.665763	115.219314	49.263207
1028.990312	129.136519	49.268212
1025.558633	116.439560	49.273217
1022.257049	116.269901	49.278221
1018.669499	112.807200	49.283226
1015.099189	108.152211	49.288231
1011.397781	110.032028	49.293236
1008.233442	109.277728	49.298241
1004.833501	110.034651	49.303245
1001.279651	119.889473	49.308250
997.825461	112.688426	49.313255
994.078372	116.574929	49.318260
990.488813	107.373410	49.323265
987.024675	108.817446	49.328269
983.743817	113.671843	49.333274
980.200938	112.233327	49.338279
976.289654	116.661246	49.343284
972.986394	111.992934	49.348289
969.225597	116.669379	49.353293
965.622302	115.597839	49.358298
962.741905	112.385110	49.363303
959.118068	116.037188	49.368308
955.823506	108.317613	49.373313
952.346347	110.741315	49.378317
948.249381	114.388384	49.383322
945.280284	107.842245	49.388327
941.606400	102.880797	49.393332
938.027141	105.959580	49.398337
934.335218	109.793171	49.403341
930.807954	112.879634	49.408346
928.207143	105.475393	49.413351
924.242430	100.423450	49.418356
920.602026	102.018497	49.423361
916.540080	105.792973	49.428365
913.077273	108.856694	49.433370
909.789335	98.013431	49.438375
906.264680	113.533239	49.443380
903.419565	109.036830	49.448385
899.342146	107.875039	49.453389
896.101108	104.823211	49.458394
893.150661	99.539695	49.463399
888.647669	113.327076	49.468404
885.174273	113.143239	49.473409
882.113536	117.463318	49.478413
878.713544	114.433221	49.483418
875.266511	110.496153	49.488423
871.410554	115.522897	49.493428
868.236469	112.011334	49.498433
864.599564	105.209123	49.503437
860.806564	106.938821	49.508442
857.688968	106.104485	49.513447
853.657142	113.300668	49.518452
850.755444	103.855461	49.523457
847.267651	106.679504	49.528461
843.675171	112.044655	49.533466
840.007471	105.772469	49.538471
836.102501	113.385398	49.543476
832.382738	117.726432	49.548481
829.405466	109.469999	49.553485
826.384479	102.688419	49.558490
822.714002	108.632111	49.563495
818.921833	113.737471	49.568500
815.311746	107.585989	49.573505
811.891998	115.806327	49.578509
807.876932	119.295092	49.583514
805.304471	102.281153	49.588519
801.478993	108.853411	49.593524
798.087948	109.824153	49.598529
794.763201	107.146144	49.603533
790.713404	110.893458	49.608538
787.549503	105.289059	49.613543
784.034257	108.240812	49.618548
780.749744	108.150823	49.623553
777.026687	104.162107	49.628557
773.155912	112.952965	49.633562
769.967265	112.240518	49.638567
765.930949	106.592410	49.643572
762.667576	105.894832	49.648577
759.631861	106.085433	49.653581
756.207236	105.761128	49.658586
752.815756	109.149097	49.663591
748.872285	100.208764	49.668596
745.018810	94.418140	49.673601
742.039473	94.849859	49.678605
738.494238	104.564193	49.683610
735.269486	102.781722	49.688615
731.546494	101.232305	49.693620
727.983473	100.882226	49.698625
724.198589	110.083597	49.703629
720.579771	106.568969	49.708634
717.277825	103.026867	49.713639
713.830651	103.256609	49.718644
710.486712	95.997299	49.723649
706.961882	101.500598	49.728653
703.419184	103.311383	49.733658
700.063678	92.235188	49.738663
696.067907	104.870672	49.743668
692.827540	98.297511	49.748673
689.466148	105.803214	49.753677
685.799464	107.073431	49.758682
682.149698	96.353377	49.763687
678.531893	108.689228	49.768692
675.040966	101.263122	49.773697
672.042971	99.846965	49.778701
668.695181	99.554952	49.783706
664.892825	96.746146	49.788711
661.134226	105.010100	49.793716
657.553674	98.199161	49.798721
654.259268	102.530589	49.803725
651.011147	105.314001	49.808730
647.832651	102.205016	49.813735
643.679155	105.946483	49.818740
640.222822	97.831596	49.823745
636.916029	97.213631	49.828749
633.231493	103.045692	49.833754
629.734017	97.427161	49.838759
626.104002	101.716245	49.843764
622.553595	91.758956	49.848769
618.853906	91.686592	49.853773
615.847645	98.839300	49.858778
612.639920	95.801346	49.863783
608.736322	102.316301	49.868788
605.516804	89.143405	49.873793
602.045408	96.166481	49.878797
598.242821	92.952776	49.883802
594.897470	93.511469	49.888807
591.225244	102.075133	49.893812
587.801522	101.051551	49.898817
584.139910	99.609643	49.903821
580.861424	101.837842	49.908826
577.572199	96.651795	49.913831
573.382036	99.775767	49.918836
570.011551	100.746535	49.923841
566.537363	105.365580	49.928845
563.171289	106.341988	49.933850
559.678116	103.630337	49.938855
555.927510	113.449664	49.943860
552.566195	106.775276	49.948865
549.274804	103.215768	49.953869
545.511811	114.147530	49.958874
542.308241	97.359107	49.963879
539.018389	109.539228	49.968884
535.347061	107.222490	49.973889
531.603249	100.085997	49.978893
528.220023	105.633619	49.983898
524.745822	103.808036	49.988903
520.733687	104.936269	49.993908
517.592170	99.088025	49.998913
514.404551	107.582142	50.003917
510.578859	104.144300	50.008922
507.725341	106.138283	50.013927
503.595544	114.352865	50.018932
500.273819	99.228140	50.023937
496.871848	93.737080	50.028941
492.975339	105.271903	50.033946
489.334061	98.695181	50.038951
485.996109	101.907175	50.043956
482.453673	99.972074	50.048961
479.162618	109.690971	50.053965
475.709396	104.366133	50.058970
472.203783	97.869411	50.063975
468.795984	104.151736	50.068980
465.361824	100.791796	50.073985
461.541173	105.936549	50.078989
457.892808	108.045555	50.083994
454.674319	106.360284	50.088999
450.967162	105.004659	50.094004
447.599466	97.945337	50.099009
444.251162	99.453685	50.104013
440.806835	108.487911	50.109018
437.274555	93.244341	50.114023
433.129809	99.332057	50.119028
430.097669	96.943720	50.124033
426.581753	97.234959	50.129037
423.189076	110.282276	50.134042
419.883448	108.847951	50.139047
416.380324	100.449426	50.144052
412.546233	94.890044	50.149057
408.925699	104.129050	50.154061
405.620386	106.196996	50.159066
402.284717	99.971081	50.164071
398.267680	104.545501	50.169076
394.701959	97.627954	50.174081
391.640216	100.050061	50.179085
387.976510	103.256167	50.184090
384.748219	92.786622	50.189095
380.973627	106.618278	50.194100
377.401378	102.871875	50.199105
374.149396	98.284361	50.204109
370.373249	108.553842	50.209114
367.281106	105.795271	50.214119
363.464280	108.411598	50.219124
360.191643	100.318683	50.224129
356.527764	106.125462	50.229133
352.765738	111.795755	50.234138
349.586067	102.463896	50.239143
346.028870	106.460100	50.244148
342.599694	102.387577	50.249153
338.885323	103.624272	50.254157
335.524271	107.105696	50.259162
332.229984	98.193601	50.264167
328.554317	103.309367	50.269172
324.915466	105.524502	50.274177
321.576749	105.370405	50.279181
318.151535	103.249328	50.284186
314.479989	104.087015	50.289191
310.548754	108.024765	50.294196
307.383392	99.133615	50.299201
303.848773	103.926735	50.304205
300.669750	100.264301	50.309210
297.169069	103.071578	50.314215
293.375496	105.266670	50.319220
289.817879	94.352043	50.324225
286.382797	85.626548	50.329229
282.650257	103.896759	50.334234
279.624290	93.636015	50.339239
276.008475	107.597856	50.344244
272.684215	100.803892	50.349249
269.315151	94.712983	50.354253
265.576575	100.613752	50.359258
261.832451	100.811091	50.364263
258.452991	104.950328	50.369268
254.892759	100.335220	50.374273
251.465708	105.741101	50.379277
248.091929	111.749250	50.384282
244.832884	105.669586	50.389287
240.926859	107.047078	50.394292
237.135574	110.080238	50.399297
233.797217	108.151234	50.404301
230.021918	107.802972	50.409306
226.804414	95.810027	50.414311
223.125680	95.180882	50.419316
220.169146	98.671741	50.424321
216.411452	97.096343	50.429325
212.603310	106.070573	50.434330
209.345568	98.794813	50.439335
205.916027	96.424522	50.444340
202.853322	98.138154	50.449345
199.137254	90.962678	50.454349
194.773920	106.307162	50.459354
191.715907	114.857000	50.464359
188.133621	107.059444	50.469364
184.644814	99.832549	50.474369
181.619226	96.595383	50.479373
177.971151	108.834884	50.484378
174.625236	102.196216	50.489383
170.633618	114.438922	50.494388
166.966830	108.347239	50.499393
163.684112	106.042548	50.504397
160.267615	107.289598	50.509402
157.271242	102.339421	50.514407
153.749244	110.731003	50.519412
150.029449	107.754468	50.524417
146.305797	105.132882	50.529421
142.410392	111.757467	50.534426
139.220236	113.370866	50.539431
135.933167	99.490591	50.544436
132.705727	100.005672	50.549441
128.727044	107.402616	50.554445
125.120280	100.959863	50.559450
121.582136	99.090680	50.564455
118.224727	108.396129	50.569460
114.886464	102.673786	50.574465
111.253776	102.730342	50.579469
107.994001	97.802470	50.584474
104.308894	98.370284	50.589479
100.499243	98.277399	50.594484
97.115907	103.591061	50.599489
93.724632	105.400502	50.604493
90.350367	101.597897	50.609498
86.958790	96.962769	50.614503
83.174702	105.145496	50.619508
79.723936	112.424948	50.624513
76.490818	88.250810	50.629517
72.590911	103.915038	50.634522
69.388417	96.516788	50.639527
66.265284	101.283489	50.644532
62.297920	101.212166	50.649537
58.749151	100.619678	50.654541
55.210006	101.692993	50.659546
51.881698	104.603070	50.664551
48.402018	95.628405	50.669556
44.459558	99.836944	50.674561
41.187473	101.653039	50.679565
37.844204	106.261250	50.684570
34.486471	100.279400	50.689575
30.528591	110.833738	50.694580
27.075958	112.380733	50.699585
23.306531	98.525472	50.704589
19.666069	96.811570	50.709594
16.797568	97.779823	50.714599
13.339078	103.608331	50.719604
9.816463	96.646245	50.724609
6.306850	100.223828	50.729613
2.235775	98.204079	50.734618