Thu Aug 25 12:46:25 2022

Number of Points = 9925

Depth (nm)	Load (N)	Time (s)
2.075774	115.368425	0.000000
2.549402	97.750951	0.005005
2.372316	103.853060	0.010010
2.048150	85.759479	0.015014
1.974965	77.943665	0.020019
1.672398	74.710140	0.025024
1.548798	60.179210	0.030029
1.165477	68.490296	0.035034
0.859273	45.540712	0.040038
0.694228	46.417530	0.045043
0.681682	40.509477	0.050048
0.491356	33.246713	0.055053
-0.086761	19.609610	0.060058
-0.124391	23.595429	0.065062
-0.663934	12.723748	0.070067
-1.057899	10.197419	0.075072
-1.281768	3.398670	0.080077
-1.829420	-0.245696	0.085082
-2.162906	-5.255560	0.090086
-2.253634	-1.546166	0.095091
-2.814817	0.667713	0.100096
-2.784955	1.422242	0.105101
-3.791908	3.981213	0.110106
-3.607200	0.105041	0.115110
-3.920691	-1.399343	0.120115
-4.096123	12.760580	0.125120
-3.849015	-1.515169	0.130125
-3.866915	-2.926662	0.135130
-4.235706	-2.229895	0.140134
-4.800453	-2.945101	0.145139
-5.413130	2.870882	0.150144
-5.321400	-8.071221	0.155149
-5.448722	6.701257	0.160154
-5.812519	3.414064	0.165158
-5.597107	0.254419	0.170163
-6.581226	10.516742	0.175168
-6.732306	8.967927	0.180173
-6.841388	9.329773	0.185178
-7.205589	2.999102	0.190182
-7.292360	0.298093	0.195187
-7.592467	4.385144	0.200192
-8.282543	1.133254	0.205197
-8.577317	0.556083	0.210202
-8.677784	7.895841	0.215206
-8.454837	0.799294	0.220211
-8.957942	8.145190	0.225216
-8.793099	-0.995535	0.230221
-8.730057	6.875426	0.235226
-9.297515	3.253146	0.240230
-9.367114	1.985795	0.245235
-10.015037	-5.439373	0.250240
-10.683658	-3.382667	0.255245
-10.969828	-8.735302	0.260250
-11.302238	-1.299095	0.265254
-11.006216	-5.452135	0.270259
-11.077363	-1.695189	0.275264
-11.148026	2.593194	0.280269
-11.510423	3.168737	0.285274
-12.446935	-0.746896	0.290278
-12.404788	-5.072130	0.295283
-12.640141	-3.228842	0.300288
-12.875247	-4.451278	0.305293
-12.686926	0.283746	0.310298
-13.672428	-5.895790	0.315302
-13.281394	-5.783147	0.320307
-13.998762	-0.896727	0.325312
-14.155822	-4.611781	0.330317
-13.972045	-1.717355	0.335322
-15.081504	2.249733	0.340326
-15.089387	-5.054254	0.345331
-15.102200	5.856311	0.350336
-15.360732	1.151078	0.355341
-15.582890	-5.394834	0.360346
-15.610576	-5.868320	0.365350
-15.988837	-12.750439	0.370355
-16.751599	-2.098863	0.375360
-16.828292	-11.878783	0.380365
-16.999438	-8.197919	0.385370
-17.036406	-2.317118	0.390374
-16.963007	-5.097005	0.395379
-17.108971	1.560178	0.400384
-17.843196	-11.862612	0.405389
-18.102309	-11.970806	0.410394
-18.474856	-10.134496	0.415398
-18.369667	-19.300666	0.420403
-19.392536	-4.669457	0.425408
-19.547776	-11.801656	0.430413
-19.837233	-9.054547	0.435418
-20.167333	-2.564667	0.440422
-19.827457	-7.268745	0.445427
-20.195300	7.658477	0.450432
-20.403885	-2.246316	0.455437
-20.259329	-1.465465	0.460442
-20.523130	-2.471433	0.465446
-20.629896	-2.872416	0.470451
-21.378708	-3.375283	0.475456
-21.163473	-4.073492	0.480461
-22.092771	0.811333	0.485466
-22.339083	1.675572	0.490470
-22.424865	-8.988778	0.495475
-22.730087	-1.050630	0.500480
-23.217045	-1.933047	0.505485
-23.072717	-3.056745	0.510490
-23.006306	-0.004725	0.515494
-23.565660	-4.327463	0.520499
-23.941479	-4.923572	0.525504
-24.343584	-4.354463	0.530509
-24.225238	4.070980	0.535514
-24.636807	11.788514	0.540518
-24.554554	0.718178	0.545523
-25.429453	4.585241	0.550528
-25.478177	4.418773	0.555533
-25.889080	4.596955	0.560538
-25.869807	5.315177	0.565542
-25.712113	3.161161	0.570547
-26.289443	1.176096	0.575552
-26.934648	-6.214694	0.580557
-27.236800	2.450640	0.585562
-27.382264	5.339705	0.590566
-27.035645	14.969581	0.595571
-27.599809	6.797293	0.600576
-27.299416	1.561559	0.605581
-28.003637	7.249518	0.610586
-28.556770	10.863686	0.615590
-28.315020	-3.037896	0.620595
-29.101442	1.694829	0.625600
-29.471824	0.743526	0.630605
-29.925083	2.111592	0.635610
-29.981776	7.176072	0.640614
-30.046045	0.833211	0.645619
-30.251129	5.797555	0.650624
-30.373682	5.493957	0.655629
-30.323738	3.132197	0.660634
-30.408437	8.732578	0.665638
-30.579015	13.229607	0.670643
-31.442857	14.741100	0.675648
-31.745977	3.509681	0.680653
-31.444651	-2.960064	0.685658
-32.328123	7.403546	0.690662
-32.896130	0.307544	0.695667
-33.347114	8.066054	0.700672
-33.667265	6.698755	0.705677
-33.547600	11.188273	0.710682
-33.552346	10.464419	0.715686
-33.225798	1.738120	0.720691
-33.337894	5.586905	0.725696
-33.389624	-0.558603	0.730701
-34.034779	7.635292	0.735706
-34.059367	8.252819	0.740710
-34.664689	5.541310	0.745715
-35.583422	7.203772	0.750720
-35.897760	6.427186	0.755725
-35.990723	5.426089	0.760730
-35.924246	12.834602	0.765734
-35.822284	9.461778	0.770739
-35.796424	8.783748	0.775744
-36.439327	8.419313	0.780749
-36.916060	16.928509	0.785754
-37.291408	11.801815	0.790758
-37.352227	3.060280	0.795763
-37.989543	11.452266	0.800768
-38.348049	4.560719	0.805773
-38.819966	4.517506	0.810778
-38.699031	7.747646	0.815782
-38.784536	10.253994	0.820787
-39.074788	2.867697	0.825792
-39.218029	0.257796	0.830797
-38.911809	1.753636	0.835802
-39.179453	20.477500	0.840806
-39.775517	4.207812	0.845811
-40.298975	17.723075	0.850816
-40.703620	5.447703	0.855821
-40.560714	-0.354977	0.860826
-41.000509	3.697013	0.865830
-41.124603	9.059957	0.870835
-41.828775	12.178934	0.875840
-42.047505	8.049598	0.880845
-41.984508	10.203645	0.885850
-42.106168	19.694922	0.890854
-41.955035	8.360689	0.895859
-42.481580	11.568894	0.900864
-43.182050	12.864964	0.905869
-43.341781	5.543638	0.910874
-43.963363	10.136642	0.915878
-43.716321	12.812348	0.920883
-43.754593	11.457830	0.925888
-43.752977	15.358403	0.930893
-44.561627	12.412996	0.935898
-44.858702	12.693567	0.940902
-44.916915	-2.752387	0.945907
-45.574503	10.464346	0.950912
-45.521236	9.585870	0.955917
-45.157916	9.095411	0.960922
-45.546907	1.942887	0.965926
-45.966508	8.465776	0.970931
-46.410938	20.525982	0.975936
-46.899248	4.688666	0.980941
-46.658554	5.704390	0.985946
-47.800269	14.159590	0.990950
-47.814760	0.370923	0.995955
-48.213685	4.530406	1.000960
-48.048275	-4.309847	1.005965
-48.057251	7.495459	1.010970
-48.283579	7.651049	1.015974
-48.377225	-7.178743	1.020979
-48.992434	2.905550	1.025984
-49.459830	-1.200640	1.030989
-49.348784	4.017891	1.035994
-49.939240	13.006813	1.040998
-49.467415	2.384804	1.046003
-49.961241	10.874529	1.051008
-50.508101	7.638168	1.056013
-50.747236	2.145285	1.061018
-51.029667	11.494068	1.066022
-50.964245	8.364251	1.071027
-51.677733	11.984563	1.076032
-51.395144	4.372469	1.081037
-52.004509	1.076300	1.086042
-52.742124	10.335052	1.091046
-52.080871	0.578708	1.096051
-52.731738	8.754516	1.101056
-52.737370	4.019150	1.106061
-53.143622	3.364535	1.111066
-53.801210	-4.138207	1.116070
-53.837712	5.962980	1.121075
-53.847187	2.917666	1.126080
-54.218063	2.406205	1.131085
-54.167194	2.894849	1.136090
-54.931769	8.051262	1.141094
-55.272297	10.670335	1.146099
-55.675768	12.818378	1.151104
-55.487393	3.009576	1.156109
-55.440365	6.466431	1.161114
-55.690001	14.490788	1.166118
-55.741112	7.978185	1.171123
-56.582468	10.792790	1.176128
-56.929071	14.646683	1.181133
-56.886228	8.052919	1.186138
-57.166612	8.400478	1.191142
-57.472781	12.988355	1.196147
-58.065892	0.350212	1.201152
-57.935758	7.859480	1.206157
-58.232788	-1.974503	1.211162
-58.709303	7.920382	1.216166
-58.334136	1.030940	1.221171
-58.802033	16.818568	1.226176
-59.348638	9.697065	1.231181
-59.724208	5.959302	1.236186
-59.816075	16.923385	1.241190
-60.095199	6.194411	1.246195
-60.321857	4.682750	1.251200
-60.607051	0.525866	1.256205
-60.440165	-1.436600	1.261210
-61.481434	1.181537	1.266214
-61.227945	2.698293	1.271219
-61.682935	10.890867	1.276224
-61.708112	8.196026	1.281229
-61.655720	0.920560	1.286234
-62.123715	7.498488	1.291238
-62.449767	2.822821	1.296243
-62.798457	12.371812	1.301248
-63.145127	7.386161	1.306253
-63.265645	0.912910	1.311258
-63.158194	7.736031	1.316262
-63.502154	2.044438	1.321267
-64.253565	5.787751	1.326272
-64.848119	16.425637	1.331277
-64.800167	4.965206	1.336282
-65.197954	8.634128	1.341286
-64.771928	10.509829	1.346291
-64.893408	12.173925	1.351296
-65.078963	16.916912	1.356301
-65.346121	5.613422	1.361306
-65.975779	0.801829	1.366310
-66.308248	7.687553	1.371315
-66.153447	7.397446	1.376320
-66.861826	7.122366	1.381325
-66.813100	4.393800	1.386330
-67.671877	9.808584	1.391334
-67.762948	8.266187	1.396339
-68.011829	7.102859	1.401344
-67.769592	1.980642	1.406349
-67.635284	5.411166	1.411354
-68.874710	15.511016	1.416358
-68.840119	13.211772	1.421363
-69.077430	9.898435	1.426368
-69.124506	5.387863	1.431373
-69.028459	3.316273	1.436378
-69.621464	5.101707	1.441382
-70.216407	-2.724061	1.446387
-70.499300	0.325742	1.451392
-70.580801	0.632646	1.456397
-70.325338	0.532411	1.461402
-70.843809	7.665579	1.466406
-71.544380	-3.266272	1.471411
-72.044056	9.327766	1.476416
-72.288242	8.207995	1.481421
-72.251997	-3.184157	1.486426
-72.499930	7.260207	1.491430
-72.395589	2.517102	1.496435
-72.437814	3.940988	1.501440
-72.829566	11.845242	1.506445
-73.538106	5.087639	1.511450
-73.719138	14.293984	1.516454
-73.563544	4.053720	1.521459
-73.984907	4.584720	1.526464
-73.928211	2.829345	1.531469
-74.166484	-3.900700	1.536474
-75.031900	0.939318	1.541478
-74.943943	4.975054	1.546483
-74.969169	0.669869	1.551488
-75.774741	6.392692	1.556493
-75.990800	10.276749	1.561498
-76.328272	5.359261	1.566502
-76.509535	1.755570	1.571507
-76.763627	6.325794	1.576512
-76.778038	3.303400	1.581517
-76.967843	4.364432	1.586522
-77.317523	8.234624	1.591526
-77.263824	6.261418	1.596531
-77.811471	3.041002	1.601536
-78.090152	6.469798	1.606541
-78.124864	6.788354	1.611546
-78.443311	9.014824	1.616550
-78.542802	2.908439	1.621555
-79.145340	6.258265	1.626560
-79.812687	12.671278	1.631565
-79.688011	7.295398	1.636570
-79.954288	8.406377	1.641574
-79.719535	13.510612	1.646579
-79.698205	9.460721	1.651584
-80.365666	7.967510	1.656589
-80.769008	11.244997	1.661594
-80.973509	4.443219	1.666598
-80.827897	-0.404428	1.671603
-81.149481	10.459602	1.676608
-81.785018	4.661837	1.681613
-81.870206	1.859342	1.686618
-82.548858	4.990140	1.691622
-82.227922	-2.526719	1.696627
-83.249957	3.188892	1.701632
-83.704543	-1.314772	1.706637
-83.513616	3.204704	1.711642
-83.358405	0.997293	1.716646
-83.528171	6.319935	1.721651
-83.831578	16.387016	1.726656
-83.942327	0.038133	1.731661
-84.275526	-3.544914	1.736666
-85.304332	3.529011	1.741670
-85.299787	0.285349	1.746675
-85.608109	4.126914	1.751680
-85.667283	5.619894	1.756685
-85.427679	6.148568	1.761690
-85.834744	16.466010	1.766694
-86.230769	8.773585	1.771699
-86.701026	7.572179	1.776704
-86.968215	10.097502	1.781709
-86.919336	3.626183	1.786714
-87.179789	13.237277	1.791718
-87.138917	4.577889	1.796723
-87.888965	3.853758	1.801728
-88.616977	7.030257	1.806733
-88.799709	2.746587	1.811738
-88.758205	4.173172	1.816742
-88.278833	-2.245377	1.821747
-88.719608	-1.584784	1.826752
-89.359891	-0.412038	1.831757
-89.763636	-1.000605	1.836762
-89.835894	0.965825	1.841766
-89.942077	-3.092555	1.846771
-90.110245	6.538877	1.851776
-90.615027	-0.538551	1.856781
-91.076360	-4.576084	1.861786
-91.573355	3.613577	1.866790
-91.868851	2.593595	1.871795
-91.899465	3.072861	1.876800
-91.834527	1.097895	1.881805
-91.606058	3.108953	1.886810
-91.823354	8.217579	1.891814
-91.913858	1.496017	1.896819
-92.694596	16.364550	1.901824
-93.269621	5.890754	1.906829
-92.931988	-3.792732	1.911834
-93.641492	2.019441	1.916838
-94.125657	-3.874805	1.921843
-94.172736	2.339773	1.926848
-94.711869	7.669671	1.931853
-94.414721	9.144784	1.936858
-94.472593	4.825731	1.941862
-95.104790	0.144253	1.946867
-95.426380	6.357554	1.951872
-96.098632	12.201859	1.956877
-95.823383	3.724046	1.961882
-95.970637	9.223494	1.966886
-95.734367	-0.950313	1.971891
-96.243297	7.149470	1.976896
-97.267657	0.963380	1.981901
-97.316000	-4.638487	1.986906
-97.443374	9.067804	1.991910
-97.480649	15.590899	1.996915
-97.653953	3.224594	2.006912
-97.884104	-1.155463	2.016909
-97.389615	2.885018	2.026906
-96.540456	-0.248146	2.036902
-96.131123	-7.699810	2.046899
-95.449102	4.208638	2.056896
-95.194083	-2.278009	2.066893
-95.010282	-5.474810	2.076890
-94.060094	-4.603853	2.086886
-93.532406	-2.833559	2.096883
-92.874181	0.725101	2.106880
-92.610263	-3.184341	2.116877
-92.561774	-0.328429	2.126874
-91.603692	-0.855712	2.136870
-91.195780	-0.298929	2.146867
-90.389333	-2.430707	2.156864
-89.839125	-4.085177	2.166861
-89.364804	-8.122621	2.176858
-89.395881	2.066569	2.186854
-88.541083	-0.696845	2.196851
-88.125803	3.362384	2.206848
-87.603157	0.454611	2.216845
-86.977584	6.536800	2.226842
-86.422978	7.469743	2.236838
-86.190801	8.526067	2.246835
-85.612855	8.454324	2.256832
-85.328005	4.940745	2.266829
-84.697767	3.638033	2.276826
-83.885574	1.004840	2.286822
-83.809030	-0.999898	2.296819
-82.657187	5.563699	2.306816
-82.533806	0.371139	2.316813
-82.658530	6.805310	2.326810
-81.824542	0.481369	2.336806
-81.002391	4.543370	2.346803
-80.416077	2.132471	2.356800
-80.044750	3.648499	2.366797
-79.609856	-1.462991	2.376794
-78.870121	-0.869502	2.386790
-78.493400	-1.774527	2.396787
-78.203079	-5.057711	2.406784
-77.450766	1.910612	2.416781
-77.196990	2.675281	2.426778
-76.722568	-5.147713	2.436774
-76.139828	3.690847	2.446771
-75.383257	1.516199	2.456768
-74.545023	5.205047	2.466765
-74.428418	4.353451	2.476762
-74.024867	5.772564	2.486758
-73.900177	3.117215	2.496755
-73.077811	4.461201	2.506752
-72.951666	8.546730	2.516749
-71.895084	3.128750	2.526746
-71.870787	-2.228850	2.536742
-70.877068	0.155839	2.546739
-70.238283	3.511641	2.556736
-70.056183	0.761766	2.566733
-69.783977	4.786394	2.576730
-68.693753	3.741061	2.586726
-68.860311	8.053019	2.596723
-67.730468	6.047966	2.606720
-67.040352	1.115063	2.616717
-67.075174	5.491910	2.626714
-67.057414	5.916590	2.636710
-66.317909	5.353866	2.646707
-65.377028	6.254796	2.656704
-64.491977	7.316529	2.666701
-64.500725	8.008292	2.676698
-64.321742	7.428857	2.686694
-63.734596	11.391468	2.696691
-63.019206	2.900318	2.706688
-62.660493	10.842650	2.716685
-61.727970	3.619448	2.726682
-61.357589	9.675103	2.736678
-61.232634	7.149592	2.746675
-60.306711	6.921957	2.756672
-60.046032	2.718415	2.766669
-59.688077	-1.322971	2.776666
-58.915413	4.549272	2.786662
-58.680466	-0.296472	2.796659
-57.745795	-1.482156	2.806656
-57.420986	5.020963	2.816653
-57.034326	4.697259	2.826650
-56.904400	4.458131	2.836646
-55.766867	2.442372	2.846643
-55.617965	6.498993	2.856640
-54.923413	3.504097	2.866637
-54.109268	2.581219	2.876634
-54.180673	9.352330	2.886630
-53.752900	8.090846	2.896627
-52.958047	9.949164	2.906624
-52.848548	6.393368	2.916621
-51.529814	4.875074	2.926618
-51.150535	1.536768	2.936614
-51.172659	10.105811	2.946611
-50.642143	9.461792	2.956608
-49.870547	-2.186969	2.966605
-49.593578	0.731347	2.976602
-49.129952	-0.374195	2.986598
-48.469404	-0.937217	2.996595
-48.375915	1.797604	3.006592
-47.134930	3.788759	3.016589
-46.964340	2.871683	3.026586
-46.738231	3.723052	3.036582
-45.709194	1.787650	3.046579
-45.383084	4.657086	3.056576
-45.057994	5.708356	3.066573
-43.908839	1.390945	3.076570
-43.943063	4.136275	3.086566
-43.721106	4.075964	3.096563
-43.045063	8.588519	3.106560
-42.645559	1.078202	3.116557
-41.770142	0.601890	3.126554
-40.893778	0.172946	3.136550
-40.779314	4.073405	3.146547
-40.915946	3.388200	3.156544
-40.038765	1.546284	3.166541
-39.547881	8.165936	3.176538
-38.942256	0.629659	3.186534
-38.297038	2.058426	3.196531
-38.151388	-0.647724	3.206528
-37.569860	0.556604	3.216525
-36.710570	2.141897	3.226522
-36.720513	5.434622	3.236518
-36.095914	5.865591	3.246515
-35.584865	2.202529	3.256512
-34.663332	-1.005327	3.266509
-33.892365	-0.758851	3.276506
-33.563538	4.226259	3.286502
-33.850013	1.027113	3.296499
-33.178370	1.327166	3.306496
-32.448960	-0.447246	3.316493
-32.166677	2.403715	3.326490
-31.310199	2.155285	3.336486
-30.901812	0.519871	3.346483
-30.777938	4.273137	3.356480
-29.789267	1.095943	3.366477
-29.783421	-3.381284	3.376474
-28.689295	4.955839	3.386470
-27.833363	1.112028	3.396467
-27.945845	-1.994003	3.406464
-27.847200	0.961759	3.416461
-26.583922	-2.331321	3.426458
-26.317257	0.886385	3.436454
-26.178066	-0.466096	3.446451
-25.370716	-0.637135	3.456448
-24.988864	0.421082	3.466445
-24.527732	-1.152904	3.476442
-23.771724	-3.508025	3.486438
-23.382417	3.235248	3.496435
-22.956727	1.774521	3.506432
-21.979094	0.163957	3.516429
-22.175559	0.938985	3.526426
-21.581666	-2.756063	3.536422
-20.727644	2.431862	3.546419
-20.488431	1.158743	3.556416
-19.818463	3.616340	3.566413
-18.845201	-6.594151	3.576410
-18.729054	-9.463570	3.586406
-18.765754	-3.705264	3.596403
-18.198569	-3.724632	3.606400
-17.435046	-1.969109	3.616397
-17.013722	-1.965622	3.626394
-16.249175	1.611234	3.636390
-16.096717	7.200522	3.646387
-15.305675	3.053264	3.656384
-14.919900	7.243836	3.666381
-14.425763	7.916994	3.676378
-13.975464	4.466191	3.686374
-13.358542	5.170796	3.696371
-12.987976	3.965796	3.706368
-12.171579	1.255921	3.716365
-11.978054	-0.209611	3.726362
-11.635495	4.627629	3.736358
-10.657377	3.450981	3.746355
-10.560046	5.833575	3.756352
-9.669484	-7.262507	3.766349
-9.124147	0.647417	3.776346
-8.937023	0.193420	3.786342
-8.834084	2.514947	3.796339
-8.127185	9.699475	3.806336
-7.108726	2.738412	3.816333
-6.527097	6.290077	3.826330
-6.133392	1.090005	3.836326
-6.225962	6.828558	3.846323
-5.543876	5.099576	3.856320
-4.937483	4.608398	3.866317
-4.497205	6.870735	3.876314
-3.627409	7.906355	3.886310
-3.204782	13.516672	3.896307
-3.205625	19.199675	3.906304
-2.585134	34.716442	3.916301
-2.353903	38.728496	3.926298
-1.961227	46.114328	3.936294
-1.415108	63.229851	3.946291
-1.088693	81.517065	3.956288
-0.448750	107.266103	3.966285
0.000000	107.230604	3.971290
0.358649	117.969142	3.976294
0.279696	125.546025	3.981299
0.705970	137.074416	3.986304
0.947305	135.644442	3.991309
0.893454	125.152178	3.996314
0.587027	133.498704	4.001318
0.958885	133.032217	4.006323
0.983885	128.086370	4.011328
0.656063	140.871879	4.016333
0.893510	135.649133	4.021338
0.512298	140.599981	4.026342
1.023348	130.186886	4.031347
0.836432	131.741021	4.036352
0.991241	148.684063	4.041357
1.288028	139.826316	4.046362
0.942490	141.769141	4.051366
0.889814	140.711102	4.056371
1.133524	145.456470	4.061376
0.995177	144.993991	4.066381
1.224438	148.001539	4.071386
0.930668	153.954267	4.076390
1.122256	157.325228	4.081395
1.198408	156.981003	4.086400
1.251087	151.306305	4.091405
1.189393	149.218283	4.096410
1.206471	152.831723	4.101414
1.029581	151.258465	4.106419
0.851719	147.559293	4.111424
0.851202	157.227820	4.116429
1.129716	155.994502	4.121434
1.406842	164.391981	4.126438
1.385923	151.448931	4.131443
1.705537	157.353011	4.136448
1.134333	159.660230	4.141453
1.571046	160.597795	4.146458
1.476570	162.371570	4.151462
0.982642	145.737724	4.156467
1.304179	151.435855	4.161472
1.267248	155.522835	4.166477
1.693642	150.963350	4.171482
1.369952	155.911517	4.176486
1.101082	151.698250	4.181491
1.068158	155.911154	4.186496
1.093485	163.379965	4.191501
1.574720	155.398155	4.196506
1.221744	164.289832	4.201510
1.126208	169.040903	4.206515
1.395024	160.424813	4.211520
1.140581	165.491848	4.216525
1.219263	170.155510	4.221530
1.323156	164.029853	4.226534
1.411315	165.806651	4.231539
1.577042	155.988655	4.236544
1.145239	169.568769	4.241549
1.371320	162.655166	4.246554
1.586365	171.600220	4.251558
1.409692	175.376901	4.256563
1.769376	182.122608	4.261568
1.568872	179.572271	4.266573
1.632647	170.561190	4.271578
1.413021	169.836195	4.276582
1.597859	185.208489	4.281587
1.812448	175.784629	4.286592
1.439821	184.986283	4.291597
1.662351	189.674869	4.296602
1.830421	191.878917	4.301606
1.859519	185.594127	4.306611
1.931091	167.201173	4.311616
1.582354	173.396640	4.316621
1.559611	162.817222	4.321626
1.573986	166.054597	4.326630
1.794324	178.982040	4.331635
1.862921	180.679646	4.336640
1.549090	182.620671	4.341645
1.896910	187.814815	4.346650
2.059122	190.380453	4.351654
1.584123	183.662111	4.356659
2.057133	170.065848	4.361664
2.003194	177.104153	4.366669
1.804480	160.047548	4.371674
1.907730	162.492704	4.376678
1.494620	167.394773	4.381683
1.960061	172.364838	4.386688
1.803710	183.699804	4.391693
2.061076	179.774244	4.396698
2.123091	184.136797	4.401702
1.481258	180.946917	4.406707
1.783184	181.092507	4.411712
1.991418	184.593744	4.416717
2.070276	194.477648	4.421722
2.208527	187.122211	4.426726
2.119177	181.428628	4.431731
2.196027	165.762040	4.436736
1.827320	167.765446	4.441741
2.047871	170.198553	4.446746
1.805330	182.309497	4.451750
1.943475	178.595608	4.456755
2.103694	174.435330	4.461760
2.294203	185.108503	4.466765
2.250578	183.729500	4.471770
2.074737	183.269731	4.476774
1.973373	191.321559	4.481779
1.902362	189.013527	4.486784
2.240726	186.983043	4.491789
2.271280	186.354893	4.496794
2.027237	187.329518	4.501798
2.126922	188.765986	4.506803
2.467256	189.009963	4.511808
2.222345	186.150203	4.516813
2.197051	183.885629	4.521818
1.935255	191.658870	4.526822
1.899938	194.445285	4.531827
2.250485	186.259308	4.536832
2.144204	202.645352	4.541837
2.070370	195.484494	4.546842
2.322480	193.717465	4.551846
1.819914	193.283576	4.556851
2.138849	198.191181	4.561856
2.126774	195.411999	4.566861
2.295654	193.427052	4.571866
2.070759	197.024629	4.576870
2.072746	196.758463	4.581875
2.737850	194.246509	4.586880
2.260792	211.136749	4.591885
2.313106	199.767254	4.596890
2.345647	205.020294	4.601894
2.494842	206.841317	4.606899
2.406478	213.957797	4.611904
2.394590	216.161570	4.616909
2.515899	201.772489	4.621914
2.691069	212.274072	4.626918
2.528308	211.574968	4.631923
2.594385	196.675681	4.636928
2.381875	209.566560	4.641933
2.569485	197.973384	4.646938
2.578707	206.802006	4.651942
2.578820	207.713067	4.656947
2.677370	214.632581	4.661952
2.474356	209.602213	4.666957
2.582034	208.120407	4.671962
2.440003	211.167157	4.676966
2.415256	211.237379	4.681971
2.457863	209.427242	4.686976
2.723801	216.424935	4.691981
2.517843	218.140251	4.696986
2.782405	211.821723	4.701990
2.755715	216.634786	4.706995
2.610325	213.544290	4.712000
2.318586	215.646375	4.717005
2.996779	216.523962	4.722010
2.912722	210.740954	4.727014
2.766375	214.278770	4.732019
3.030733	215.009222	4.737024
2.518547	219.673724	4.742029
2.811720	210.762724	4.747034
2.777749	218.354745	4.752038
2.695033	216.317466	4.757043
2.940805	212.659475	4.762048
2.582754	223.339524	4.767053
2.696793	220.277983	4.772058
2.712836	209.679805	4.777062
2.407056	206.870708	4.782067
2.508901	213.840325	4.787072
2.175997	214.506167	4.792077
2.861726	218.305925	4.797082
3.099031	223.226326	4.802086
2.688200	227.634501	4.807091
2.951933	233.901708	4.812096
3.019309	237.826829	4.817101
3.074818	235.277501	4.822106
2.991484	231.478078	4.827110
2.837386	230.806090	4.832115
3.485090	236.535403	4.837120
3.201846	230.856364	4.842125
2.981514	228.967198	4.847130
2.651515	211.608405	4.852134
2.880807	230.412825	4.857139
3.528971	226.438679	4.862144
3.053683	246.426039	4.867149
3.098325	237.117360	4.872154
2.797963	233.968883	4.877158
2.980338	239.059248	4.882163
3.094099	241.907736	4.887168
3.044280	247.774816	4.892173
2.910155	238.437197	4.897178
3.049801	247.789578	4.902182
3.260605	246.367543	4.907187
3.590975	245.762018	4.912192
3.313922	246.982268	4.917197
3.485749	242.320274	4.922202
3.109039	245.970122	4.927206
2.854738	244.962650	4.932211
3.389567	239.063682	4.937216
2.748363	247.889828	4.942221
2.994480	240.112501	4.947226
3.106115	244.214189	4.952230
3.131326	248.702749	4.957235
3.030705	237.914021	4.962240
2.991940	246.952665	4.967245
3.256151	246.050617	4.972250
3.345233	254.126419	4.977254
3.546405	268.755895	4.982259
3.832718	249.361086	4.987264
3.468565	248.889690	4.992269
3.605514	246.498446	4.997274
3.430306	240.055819	5.002278
3.184220	245.757493	5.007283
3.423880	239.540934	5.012288
3.340110	246.466879	5.017293
3.271816	241.080031	5.022298
3.266913	243.238419	5.027302
3.397055	259.173013	5.032307
3.831944	248.986921	5.037312
3.233299	251.102295	5.042317
3.674442	256.474830	5.047322
3.745523	261.130215	5.052326
3.245877	263.847021	5.057331
3.709420	268.124536	5.062336
3.601826	267.423113	5.067341
3.597241	262.304692	5.072346
3.664314	269.406332	5.077350
3.843423	272.247750	5.082355
3.291555	252.149018	5.087360
3.437210	261.054368	5.092365
3.966608	267.305273	5.097370
3.856669	259.726096	5.102374
3.586397	254.453149	5.107379
3.963661	248.544064	5.112384
3.626855	243.724477	5.117389
3.703187	244.092078	5.122394
3.531128	243.350136	5.127398
3.577115	253.204421	5.132403
3.960704	256.067583	5.137408
3.385894	263.427982	5.142413
3.850117	254.990041	5.147418
3.750667	264.996836	5.152422
3.643685	270.142039	5.157427
3.952179	263.373675	5.162432
3.677874	260.167326	5.167437
3.639886	258.654554	5.172442
3.886178	269.382313	5.177446
3.706582	261.434392	5.182451
3.974133	265.423070	5.187456
3.829388	267.682467	5.192461
3.913592	264.733163	5.197466
3.606922	264.341346	5.202470
3.580314	274.988479	5.207475
3.757507	269.664401	5.212480
3.454653	267.212346	5.217485
3.568039	260.743478	5.222490
3.694419	266.633577	5.227494
4.225688	289.927650	5.232499
4.496392	287.613522	5.237504
4.010990	289.473870	5.242509
4.128458	278.913544	5.247514
4.208864	285.915023	5.252518
3.972737	279.409159	5.257523
3.930052	269.291555	5.262528
3.904139	274.050727	5.267533
4.297395	284.575132	5.272538
3.917919	281.970562	5.277542
3.944992	300.515669	5.282547
4.138360	289.193620	5.287552
3.793283	291.275596	5.292557
4.085104	293.428629	5.297562
4.270315	283.208870	5.302566
3.875770	294.888117	5.307571
3.996775	289.677243	5.312576
3.616776	292.403781	5.317581
3.879666	288.148295	5.322586
4.242751	291.315238	5.327590
3.877296	296.016882	5.332595
4.371031	296.043834	5.337600
4.243505	310.354678	5.342605
3.902199	308.750218	5.347610
4.407973	307.835630	5.352614
4.568136	313.435708	5.357619
4.636811	301.908557	5.362624
4.030696	295.606193	5.367629
4.461055	288.056247	5.372634
4.434043	295.441563	5.377638
4.425365	307.506458	5.382643
4.396532	290.682544	5.387648
4.233932	301.227610	5.392653
4.293358	306.701098	5.397658
4.735524	316.885658	5.402662
4.552011	310.127925	5.407667
4.289250	296.472837	5.412672
4.186183	296.359173	5.417677
4.505895	308.717473	5.422682
4.714939	312.534991	5.427686
4.433596	306.906251	5.432691
4.828936	299.766756	5.437696
4.366518	291.008904	5.442701
4.075280	300.457298	5.447706
4.501385	311.485947	5.452710
4.686524	321.549426	5.457715
4.502364	312.229099	5.462720
4.823773	320.553274	5.467725
4.564923	321.141076	5.472730
4.599171	314.839614	5.477734
4.609236	325.411426	5.482739
4.814106	311.224304	5.487744
4.624283	322.656354	5.492749
4.552688	317.655986	5.497754
4.905621	316.493256	5.502758
4.348838	329.355902	5.507763
4.920488	310.884449	5.512768
4.809038	321.108295	5.517773
4.550060	314.454135	5.522778
4.811213	312.603417	5.527782
5.056750	320.774961	5.532787
5.004526	315.382409	5.537792
4.472626	309.115868	5.542797
4.798350	313.522558	5.547802
4.958954	309.241963	5.552806
4.764068	301.875398	5.557811
4.952199	301.029562	5.562816
4.617383	300.582042	5.567821
4.555539	308.216435	5.572826
4.758188	314.110419	5.577830
4.908303	315.811085	5.582835
4.711701	311.662389	5.587840
4.492934	320.567917	5.592845
4.719584	324.521887	5.597850
4.847970	321.046785	5.602854
4.634002	319.710280	5.607859
4.651942	317.530666	5.612864
4.654891	326.480554	5.617869
4.927792	318.914136	5.622874
4.725064	321.448386	5.627878
4.881819	334.936409	5.632883
5.210960	331.439342	5.637888
4.954461	339.322550	5.642893
5.201820	333.351531	5.647898
5.011118	332.615669	5.652902
4.786782	334.659750	5.657907
5.032329	329.100313	5.662912
5.061377	339.197750	5.667917
5.071677	342.445287	5.672922
5.128975	345.960714	5.677926
4.975587	338.938816	5.682931
5.336863	343.156441	5.687936
5.035590	353.606204	5.692941
5.146972	355.002887	5.697946
5.470101	353.462002	5.702950
5.294627	354.403745	5.707955
5.241779	344.047240	5.712960
4.707616	348.731037	5.717965
4.872363	347.518695	5.722970
5.466981	349.099097	5.727974
4.985811	358.988579	5.732979
5.079774	347.232805	5.737984
4.977310	344.841093	5.742989
4.905548	342.533158	5.747994
5.219420	346.435501	5.752998
5.038213	350.276206	5.758003
5.195626	346.806042	5.763008
4.963620	357.763822	5.768013
5.335187	372.895045	5.773018
5.597471	365.570722	5.778022
5.283442	373.893239	5.783027
5.461423	374.064579	5.788032
5.508430	379.524216	5.793037
5.611736	372.221635	5.798042
5.445685	356.460058	5.803046
5.242811	346.430785	5.808051
5.163661	344.971912	5.813056
5.539049	360.602410	5.818061
5.506524	371.086008	5.823066
5.770578	368.576754	5.828070
5.267366	366.630652	5.833075
5.398259	365.426776	5.838080
5.148885	376.412600	5.843085
5.486993	373.837957	5.848090
5.689416	367.760070	5.853094
5.487094	370.765672	5.858099
5.598115	376.313357	5.863104
5.578778	366.846952	5.868109
5.134448	372.899274	5.873114
5.921070	374.180670	5.878118
5.448720	371.568492	5.883123
5.239114	370.076272	5.888128
5.139029	372.565972	5.893133
4.845300	374.782284	5.898138
5.531850	377.604326	5.903142
5.258252	385.404810	5.908147
5.916877	383.235539	5.913152
5.888581	391.687307	5.918157
5.641124	393.481910	5.923162
5.660841	392.463135	5.928166
5.569800	400.431180	5.933171
6.028910	396.445489	5.938176
5.778227	400.407824	5.943181
5.706682	398.520638	5.948186
6.280265	396.757005	5.953190
5.945883	404.649281	5.958195
6.096397	387.129606	5.963200
5.714123	384.541279	5.968205
5.549746	388.142067	5.973210
5.908336	383.808288	5.978214
5.575715	394.607844	5.983219
6.391353	393.777583	5.988224
5.850428	392.270832	5.993229
5.582703	383.397006	5.998234
5.782442	393.828407	6.003238
5.551017	405.336632	6.008243
5.932752	397.348158	6.013248
6.105485	403.303808	6.018253
6.062571	398.143896	6.023258
6.223253	385.140585	6.028262
5.724607	380.915807	6.033267
5.651594	367.395454	6.038272
5.608808	382.762453	6.043277
6.108514	395.064137	6.048282
5.897920	388.263160	6.053286
5.920460	385.238074	6.058291
6.045005	374.021670	6.063296
5.993886	375.203364	6.068301
5.737620	371.690440	6.073306
6.073179	370.359583	6.078310
5.478505	376.941674	6.083315
5.785203	372.701451	6.088320
5.603768	366.281901	6.093325
5.878250	380.197613	6.098330
5.994757	386.984663	6.103334
5.932673	382.030244	6.108339
5.999916	371.654907	6.113344
6.239637	370.680758	6.118349
5.913053	378.188977	6.123354
5.982960	371.483266	6.128358
5.820550	372.220478	6.133363
5.701677	366.224570	6.138368
5.432243	369.553907	6.143373
5.731279	376.135179	6.148378
5.906425	375.981089	6.153382
5.775624	374.558781	6.158387
5.538541	370.387939	6.163392
5.647437	379.542723	6.168397
5.828081	383.601993	6.173402
5.943838	383.748280	6.178406
5.790326	391.969724	6.183411
6.219520	391.472101	6.188416
6.182988	386.187802	6.193421
5.907859	374.983397	6.198426
5.868000	367.782345	6.203430
5.517677	374.136321	6.208435
5.781608	373.588660	6.213440
5.725992	379.478837	6.218445
5.532086	383.005156	6.223450
6.166669	385.645511	6.228454
5.904046	391.204286	6.233459
5.642797	378.162681	6.238464
5.814367	387.301321	6.243469
6.025371	390.201038	6.248474
6.013613	377.787912	6.253478
5.452083	368.431768	6.258483
5.876132	380.365636	6.263488
6.220175	392.058941	6.268493
5.807494	387.083520	6.273498
5.905244	377.181139	6.278502
5.905130	373.618589	6.283507
6.042074	369.955470	6.288512
5.738821	367.221884	6.293517
5.906778	362.804080	6.298522
6.053038	368.789177	6.303526
5.776969	370.604080	6.308531
6.018576	371.641831	6.313536
5.867384	366.438780	6.318541
6.011745	368.937637	6.323546
5.949291	365.365873	6.328550
5.518684	371.390733	6.333555
5.869537	366.036254	6.338560
5.527320	364.960290	6.343565
5.642763	374.734156	6.348570
5.868969	366.937747	6.353574
5.556461	377.145669	6.358579
6.041353	374.943507	6.363584
5.736649	375.968776	6.368589
5.560092	380.362429	6.373594
6.146254	387.933291	6.378598
5.657957	385.507112	6.383603
6.049575	388.388020	6.388608
5.979351	388.788079	6.393613
5.755728	380.834347	6.398618
5.924331	378.124907	6.403622
5.669364	377.585779	6.408627
5.910047	369.973766	6.413632
6.134911	375.361242	6.418637
5.939236	368.285845	6.423642
6.066010	369.749722	6.428646
5.877639	373.990196	6.433651
5.802956	367.452677	6.438656
5.628908	372.184464	6.443661
5.494748	370.196357	6.448666
6.078114	369.649269	6.453670
5.827101	369.770761	6.458675
5.895926	364.371883	6.463680
5.627812	359.917998	6.468685
5.709617	372.481300	6.473690
6.032638	378.441869	6.478694
5.692374	367.889932	6.483699
5.733778	374.701399	6.488704
5.750316	373.183239	6.493709
5.821673	394.429742	6.498714
5.745824	392.581197	6.503718
5.725246	398.022954	6.508723
5.785900	403.825318	6.513728
5.906347	398.019699	6.518733
5.944507	399.535428	6.523738
6.516401	388.511522	6.528742
5.947710	392.615432	6.533747
5.648594	382.465173	6.538752
5.958901	374.006999	6.543757
6.047461	382.699888	6.548762
5.814857	374.282483	6.553766
5.709548	374.795608	6.558771
5.754616	375.775566	6.563776
5.917521	381.248683	6.568781
5.760593	381.735094	6.573786
5.867543	381.284797	6.578790
5.717045	383.263528	6.583795
5.632922	371.611573	6.588800
5.689986	375.595289	6.593805
5.792968	392.293576	6.598810
6.252768	391.430481	6.603814
6.263450	389.840468	6.608819
5.956753	381.140433	6.613824
5.733173	381.456949	6.618829
5.887272	376.905268	6.623834
5.923287	364.712462	6.628838
6.005534	375.320452	6.633843
5.734269	376.954265	6.638848
5.513080	377.200801	6.643853
5.425751	378.818450	6.648858
5.578529	377.120751	6.653862
5.867075	395.257985	6.658867
5.754215	394.804161	6.663872
5.511549	399.442300	6.668877
5.830775	404.422684	6.673882
6.064508	395.286781	6.678886
5.623456	405.704690	6.683891
5.888570	399.790980	6.688896
5.657252	403.800903	6.693901
5.592220	404.741164	6.698906
5.888017	404.305571	6.703910
5.936216	409.524579	6.708915
6.111580	400.147876	6.713920
6.584036	409.109667	6.718925
5.940252	401.003453	6.723930
6.147609	378.419075	6.728934
5.892367	384.856236	6.733939
5.937345	376.591496	6.738944
5.657555	374.493326	6.743949
5.474323	375.097756	6.748954
5.800106	374.249331	6.753958
5.861787	385.281339	6.758963
5.597260	388.651040	6.763968
5.861052	395.022701	6.768973
5.695980	397.655467	6.773978
6.240550	391.359445	6.778982
5.821151	394.250363	6.783987
5.952689	380.188574	6.788992
5.970067	370.349411	6.793997
5.492539	374.451688	6.799002
5.663715	386.520096	6.804006
5.453824	397.164379	6.809011
5.804980	399.130954	6.814016
6.229299	392.958178	6.819021
5.786463	398.159203	6.824026
6.180473	396.259187	6.829030
5.823349	399.931307	6.834035
5.735726	396.993084	6.839040
5.538798	386.640145	6.844045
5.464948	392.362337	6.849050
5.950226	396.671280	6.854054
5.951834	398.233866	6.859059
6.096065	398.850267	6.864064
5.915962	393.623263	6.869069
5.818993	392.236783	6.874074
6.008897	389.131688	6.879078
6.290947	395.623879	6.884083
5.856042	390.319737	6.889088
5.917588	378.056481	6.894093
5.421762	385.331786	6.899098
5.576937	382.054959	6.904102
5.878795	396.706731	6.909107
5.819746	391.894206	6.914112
6.155730	395.283718	6.919117
5.960932	391.808617	6.924122
5.842677	380.076581	6.929126
5.974443	385.484973	6.934131
6.185590	387.454500	6.939136
6.156230	376.825370	6.944141
5.810155	377.037689	6.949146
5.919521	366.614626	6.954150
5.682124	366.499862	6.959155
5.821959	379.762774	6.964160
5.943716	374.978874	6.969165
6.093279	365.574594	6.974170
5.915379	361.726683	6.979174
5.786635	369.472826	6.984179
5.504281	369.077198	6.989184
5.715208	371.913647	6.994189
5.658210	376.497378	6.999194
6.217564	364.415569	7.004198
5.839881	371.713488	7.009203
5.819757	368.106617	7.014208
5.931223	364.194385	7.019213
5.759878	377.873056	7.024218
6.109244	356.639558	7.029222
6.130171	370.553859	7.034227
5.518651	371.408896	7.039232
5.934748	370.751970	7.044237
5.950570	373.451305	7.049242
5.945455	375.391438	7.054246
5.835450	378.224387	7.059251
5.788807	367.882715	7.064256
6.064364	378.362340	7.069261
5.896811	381.672552	7.074266
5.819869	370.655402	7.079270
5.824251	375.239008	7.084275
6.231667	366.237263	7.089280
6.012632	369.245484	7.094285
6.036930	374.490373	7.099290
6.204023	361.732853	7.104294
5.757290	374.299873	7.109299
5.977936	375.268140	7.114304
5.957580	364.197835	7.119309
5.795033	370.993799	7.124314
6.188520	362.854799	7.129318
5.384625	357.038991	7.134323
5.742750	356.849904	7.139328
5.849418	371.105121	7.144333
5.871016	362.037275	7.149338
6.276851	358.341520	7.154342
5.723361	356.039456	7.159347
5.753593	357.556424	7.164352
6.033640	355.199694	7.169357
5.933553	346.552727	7.174362
5.799202	346.231989	7.179366
5.837231	349.937101	7.184371
5.940444	347.320170	7.189376
5.713165	331.682105	7.194381
5.601904	354.380894	7.199386
5.875281	351.651877	7.204390
5.582011	366.017210	7.209395
6.075560	365.354477	7.214400
6.308026	362.394582	7.219405
5.854672	366.992955	7.224410
5.965743	349.302323	7.229414
5.849861	345.678822	7.234419
5.580364	341.848431	7.239424
5.713522	346.614337	7.244429
5.280183	348.248230	7.249434
5.911503	350.772030	7.254438
6.038252	371.354916	7.259443
6.018919	363.381839	7.264448
6.121471	361.657209	7.269453
5.765234	354.129237	7.274458
5.976116	351.058828	7.279462
5.527376	347.288158	7.284467
5.789207	352.869156	7.289472
6.075884	359.746595	7.294477
6.241819	366.658773	7.299482
5.866610	353.796397	7.304486
5.745932	344.554695	7.309491
5.621747	339.113297	7.314496
5.948449	338.141341	7.319501
5.620964	342.308690	7.324506
5.828898	338.922363	7.329510
5.732846	352.627184	7.334515
5.965713	360.860844	7.339520
6.279012	353.702543	7.344525
5.563078	359.854364	7.349530
5.965445	335.455088	7.354534
5.796266	355.299693	7.359539
5.807610	347.888141	7.364544
6.079252	341.774107	7.369549
6.029490	343.025190	7.374554
5.827262	342.414524	7.379558
5.996078	350.420928	7.384563
5.592935	336.866899	7.389568
5.643945	340.320034	7.394573
5.684610	348.821089	7.399578
5.872466	341.884932	7.404582
5.901464	350.368834	7.409587
5.514856	348.094409	7.414592
5.964065	347.843593	7.419597
5.885677	358.356516	7.424602
5.958903	348.015058	7.429606
6.413488	339.584915	7.434611
5.807740	336.177376	7.439616
5.828957	337.727393	7.444621
5.675582	341.389725	7.449626
6.097901	340.931146	7.454630
6.061755	340.231181	7.459635
6.170624	333.373844	7.464640
5.686363	333.370527	7.469645
5.589338	338.953961	7.474650
5.615375	334.077499	7.479654
5.597246	334.194141	7.484659
5.720883	340.432715	7.489664
5.973636	336.533155	7.494669
5.953475	344.354025	7.499674
5.944012	337.850591	7.504678
5.492620	332.314927	7.509683
5.499255	342.675311	7.514688
6.086907	349.195534	7.519693
5.873799	357.062460	7.524698
6.107415	345.588534	7.529702
5.640092	342.345971	7.534707
5.466034	346.884760	7.539712
5.864616	356.405441	7.544717
6.173556	364.820177	7.549722
5.757247	356.175294	7.554726
5.692642	341.264723	7.559731
5.834026	350.787733	7.564736
6.043772	366.700459	7.569741
5.446560	365.933374	7.574746
5.769906	366.104085	7.579750
6.090238	367.588256	7.584755
5.959526	360.202120	7.589760
6.058102	341.580125	7.594765
5.614499	354.314322	7.599770
5.753576	355.168816	7.604774
5.924832	363.864558	7.609779
5.785222	362.706229	7.614784
5.886165	362.272692	7.619789
5.860822	370.818902	7.624794
6.078820	352.659086	7.629798
5.746024	343.668923	7.634803
5.757589	344.812319	7.639808
5.657625	352.202761	7.644813
5.529188	369.832649	7.649818
5.916789	373.679152	7.654822
5.884912	363.369972	7.659827
5.838379	370.590694	7.664832
6.358358	367.630045	7.669837
5.827165	360.154793	7.674842
5.873662	348.852555	7.679846
6.090283	346.945535	7.684851
5.793723	343.252264	7.689856
5.867129	338.975833	7.694861
5.636844	341.346720	7.699866
5.829223	338.219100	7.704870
5.740210	347.702275	7.709875
5.772837	349.785192	7.714880
5.969468	359.147686	7.719885
5.938337	364.701821	7.724890
5.443727	353.690009	7.729894
5.856890	352.261570	7.734899
5.633301	353.666443	7.739904
6.438066	358.732095	7.744909
5.982208	367.693778	7.749914
6.110063	346.643697	7.754918
5.912823	348.269073	7.759923
5.673762	343.554370	7.764928
6.119298	335.869145	7.769933
5.709680	346.832600	7.774938
5.680565	335.070807	7.779942
5.570422	338.824444	7.784947
6.176422	342.070397	7.789952
5.933178	344.221847	7.794957
5.591911	343.174211	7.799962
6.077203	342.743731	7.804966
5.709557	343.677617	7.809971
5.660984	338.695783	7.814976
5.906722	334.471448	7.819981
6.023178	331.292448	7.824986
6.251027	336.065662	7.829990
5.805228	338.195063	7.834995
5.743389	341.532998	7.840000
5.928174	336.239349	7.845005
5.764924	341.013730	7.850010
5.938199	330.245309	7.855014
6.012244	336.902948	7.860019
5.494112	346.371098	7.865024
6.041083	336.344570	7.870029
5.782302	339.789293	7.875034
5.926794	329.813174	7.880038
6.026897	334.274202	7.885043
5.836171	336.581941	7.890048
5.843718	332.265210	7.895053
5.442744	333.014488	7.900058
6.111221	334.494730	7.905062
6.229932	340.946053	7.910067
5.959254	335.834499	7.915072
6.330541	333.533081	7.920077
5.973188	348.588661	7.925082
6.113018	340.438794	7.930086
6.265702	343.429899	7.935091
5.813022	340.896903	7.940096
5.904270	329.859754	7.945101
5.818200	335.169381	7.950106
5.760238	338.680719	7.955110
5.376055	334.985359	7.960115
5.371738	338.542077	7.965120
5.870033	340.169209	7.970125
5.638483	345.683561	7.975142
5.906558	332.292632	7.980160
5.896457	345.286350	7.985178
5.508582	338.969250	7.990195
6.084063	335.612785	7.995213
5.813976	332.843232	8.000230
5.736013	333.044697	8.005248
5.617607	338.696169	8.010266
5.393093	338.810144	8.015283
5.614656	340.441570	8.020301
5.958856	341.482591	8.025318
5.639513	337.004026	8.030336
6.043519	347.932117	8.035354
6.035584	360.868703	8.040371
6.023916	342.592307	8.045389
5.686141	346.769702	8.050406
6.090867	347.709724	8.055424
6.234215	336.739862	8.060442
5.807955	337.526064	8.065459
6.340922	338.420746	8.070477
5.820061	342.068259	8.075494
5.550607	335.041497	8.080512
5.907259	340.669030	8.085530
5.465663	350.972231	8.090547
6.190542	353.121236	8.095565
6.143926	363.283665	8.100582
6.066091	355.535762	8.105600
6.113634	354.108127	8.110618
5.682496	353.112093	8.115635
6.160736	347.849007	8.120653
5.828900	352.543017	8.125670
5.962034	366.060253	8.130688
6.198088	363.072539	8.135706
5.830784	366.686530	8.140723
6.288632	365.667972	8.145741
5.987328	364.642127	8.150758
5.957360	356.255572	8.155776
6.088089	347.872245	8.160794
5.858653	362.528709	8.165811
6.278242	365.583915	8.170829
5.828245	358.926253	8.175846
5.838441	359.107593	8.180864
5.996996	369.865875	8.185882
5.699460	370.707648	8.190899
5.853897	365.981277	8.195917
5.795023	368.391936	8.200934
5.993997	366.909017	8.205952
5.809593	366.723222	8.210970
5.775101	367.596364	8.215987
5.899625	372.263057	8.221005
5.735153	369.183465	8.226022
6.035257	375.501513	8.231040
6.328288	392.761692	8.236058
6.094361	385.202332	8.241075
6.192878	367.943735	8.246093
6.260839	366.067939	8.251110
6.190723	365.747474	8.256128
5.669390	369.909455	8.261146
6.135758	385.615082	8.266163
6.169439	381.993209	8.271181
6.254484	389.755581	8.276198
6.459869	391.051881	8.281216
6.337934	388.587306	8.286234
5.930481	375.908093	8.291251
6.024063	371.939169	8.296269
6.469687	383.829579	8.301286
5.892823	372.546511	8.306304
6.045529	380.042662	8.311322
6.112282	390.199966	8.316339
6.545612	385.007021	8.321357
6.335167	388.179879	8.326374
6.454065	382.089472	8.331392
6.162385	368.868269	8.336410
6.047992	369.485690	8.341427
6.228694	369.712898	8.346445
6.177925	371.513227	8.351462
6.163956	383.911140	8.356480
6.523240	385.984890	8.361498
6.341283	377.912468	8.366515
6.213742	369.566441	8.371533
6.102986	368.037377	8.376550
6.191762	372.400407	8.381568
6.461121	375.674810	8.386586
6.010506	376.875078	8.391603
6.416612	377.193200	8.396621
6.541992	387.628492	8.401638
6.231828	371.415366	8.406656
6.393916	371.045896	8.411674
6.112140	375.627929	8.416691
6.949300	371.618240	8.421709
6.216224	357.339598	8.426726
5.836209	366.074216	8.431744
6.606919	367.812106	8.436762
6.095437	375.989823	8.441779
6.364614	370.440755	8.446797
6.219698	372.694485	8.451814
6.508157	384.142468	8.456832
6.425228	375.682152	8.461850
5.951168	374.623414	8.466867
6.198833	381.536651	8.471885
6.270227	384.974615	8.476902
6.256859	397.665929	8.481920
6.450937	392.084440	8.486938
6.515407	396.763705	8.491955
6.839445	395.819758	8.496973
6.603892	404.544383	8.501990
6.011134	395.558032	8.507008
6.430633	392.598375	8.512026
6.277231	403.490760	8.517043
6.388835	388.054125	8.522061
6.642906	395.834198	8.527078
6.187960	400.781036	8.532096
6.279521	400.640364	8.537114
6.376451	404.935853	8.542131
6.498177	399.813816	8.547149
6.514191	392.205825	8.552166
6.213853	400.359939	8.557184
6.695307	395.512896	8.562202
6.616333	402.862322	8.567219
6.607800	398.189878	8.572237
6.613933	401.795858	8.577255
6.328634	410.645044	8.582272
6.331003	398.700012	8.587290
6.496368	396.480752	8.592307
6.229747	394.685777	8.597325
6.381323	398.246878	8.602343
6.144138	400.193181	8.607360
6.579960	396.640838	8.612378
6.033068	397.000981	8.617395
6.482255	394.071386	8.622413
6.639794	396.605930	8.627431
6.191820	391.027209	8.632448
5.918312	401.297792	8.637466
6.137226	420.409420	8.642483
6.514119	424.449614	8.647501
6.795698	421.663039	8.652519
6.550461	435.223831	8.657536
6.773694	424.758946	8.662554
6.709504	434.166784	8.667571
6.659695	419.089924	8.672589
6.733871	429.359695	8.677607
7.146313	427.480412	8.682624
7.193151	406.307257	8.687642
6.668194	408.737299	8.692659
6.268180	404.255578	8.697677
6.719011	397.185364	8.702695
6.315335	403.020406	8.707712
7.043134	386.515252	8.712730
6.793110	397.255516	8.717747
6.779193	393.521179	8.722765
6.992771	397.236665	8.727783
6.620108	401.735116	8.732800
7.067692	397.313096	8.737818
6.552786	398.662292	8.742835
6.545405	406.644277	8.747853
6.475085	400.533018	8.752871
6.341971	401.194399	8.757888
6.259176	395.886660	8.762906
6.441528	401.576234	8.767923
6.389061	401.429727	8.772941
6.719624	414.575244	8.777959
6.206025	427.843567	8.782976
7.045404	423.028798	8.787994
6.549738	429.490481	8.793011
6.780463	428.188772	8.798029
7.112772	425.662488	8.803047
6.889257	432.321370	8.808064
7.038214	416.758938	8.813082
6.779854	402.715146	8.818099
6.605528	400.321893	8.823117
6.930831	410.738497	8.828135
6.479986	411.755769	8.833152
6.968478	410.782899	8.838170
6.432921	420.097328	8.843187
6.980503	422.324614	8.848205
6.975110	418.850864	8.853223
6.325034	425.343049	8.858240
7.124491	423.229561	8.863258
6.896706	419.623400	8.868275
6.798790	412.929488	8.873293
6.860556	412.758771	8.878311
6.711219	420.649397	8.883328
6.663285	417.633588	8.888346
6.733300	427.036174	8.893363
6.723752	428.454513	8.898381
6.928022	420.656070	8.903399
6.604187	422.805297	8.908416
6.681155	418.943107	8.913434
6.931449	417.609931	8.918451
6.525912	420.327374	8.923469
6.694671	415.380998	8.928487
6.666568	419.074395	8.933504
6.846573	423.476793	8.938522
6.810655	419.294622	8.943539
6.375005	422.190351	8.948557
7.192761	418.098486	8.953575
6.800875	433.689322	8.958592
6.978773	423.285189	8.963610
6.960356	428.551798	8.968627
6.971875	422.026927	8.973645
6.806737	421.986434	8.978663
7.236918	441.046049	8.983680
6.995228	431.913156	8.988698
6.653544	434.500677	8.993715
6.832347	434.895439	8.998733
7.001659	434.398606	9.003751
6.915832	450.326507	9.008768
6.724280	441.996786	9.013786
7.324986	448.671700	9.018803
7.054922	448.631868	9.023821
7.110117	446.859048	9.028839
7.159884	449.104375	9.033856
7.024815	444.486459	9.038874
7.083113	444.840142	9.043891
6.978552	441.605985	9.048909
7.272341	441.540924	9.053927
7.231282	445.930627	9.058944
6.994199	423.309257	9.063962
7.039042	419.161769	9.068979
6.943851	420.265327	9.073997
7.085127	425.409086	9.079015
7.125391	437.684932	9.084032
7.275557	443.212308	9.089050
7.291060	431.069538	9.094067
7.053329	423.633832	9.099085
7.100666	415.566493	9.104103
7.338806	417.173239	9.109120
7.042997	412.419572	9.114138
7.326442	416.588012	9.119155
7.279443	427.088204	9.124173
7.183734	424.527998	9.129191
7.120156	419.463391	9.134208
6.862352	413.709702	9.139226
7.182683	410.778203	9.144243
7.097004	414.442752	9.149261
7.051390	414.481360	9.154279
6.879285	422.176741	9.159296
7.188057	431.251591	9.164314
7.563957	427.023829	9.169331
6.996789	429.249052	9.174349
7.222409	426.404973	9.179367
7.201264	427.509553	9.184384
7.147775	427.697716	9.189402
7.313414	427.494945	9.194419
7.406371	438.882077	9.199437
7.111662	421.457824	9.204455
7.124581	419.827329	9.209472
7.228425	433.159858	9.214490
7.106526	437.890425	9.219507
7.261134	445.219049	9.224525
7.092498	435.718106	9.229543
7.234083	450.073516	9.234560
7.116877	449.050380	9.239578
7.201090	452.281222	9.244595
7.320149	445.228258	9.249613
7.289217	445.179361	9.254631
7.332561	446.807163	9.259648
7.242754	443.980944	9.264666
7.417204	448.169626	9.269683
7.199025	448.856959	9.274701
6.946085	452.393088	9.279719
7.454678	456.097077	9.284736
7.192191	461.417716	9.289754
7.684716	450.673940	9.294771
7.345106	453.813399	9.299789
7.296480	447.907006	9.304807
7.231180	445.218957	9.309824
7.388791	452.739616	9.314842
7.304779	450.291181	9.319859
7.226142	441.580856	9.324877
7.370916	450.198577	9.329895
7.107104	450.261906	9.334912
7.072310	453.022250	9.339930
7.334103	443.864113	9.344947
7.449085	447.957972	9.349965
7.145677	449.640103	9.354983
7.579480	461.459834	9.360000
7.418789	472.397584	9.365018
7.680787	469.667718	9.370035
7.177519	466.114177	9.375053
7.562927	467.445392	9.380071
7.683271	475.132844	9.385088
7.491488	467.263891	9.390106
7.722855	442.028702	9.395123
7.731288	464.114534	9.400141
7.527065	458.898384	9.405159
7.577514	450.590703	9.410176
7.403790	458.317911	9.415194
7.329119	441.461915	9.420211
7.373397	444.427618	9.425229
7.480090	448.002072	9.430247
7.664355	453.075989	9.435264
7.435126	455.775280	9.440282
7.585779	450.071190	9.445299
7.480529	450.993292	9.450317
7.395851	452.653776	9.455335
7.633585	466.186257	9.460352
7.616491	466.239332	9.465370
7.698521	461.016200	9.470387
7.398157	459.816635	9.475405
7.616065	461.284546	9.480423
7.793179	469.546919	9.485440
7.589789	461.383144	9.490458
7.733350	449.564277	9.495475
7.619538	460.128605	9.500493
7.790575	458.107262	9.505511
7.479189	445.185732	9.510528
7.525987	457.643603	9.515546
7.418989	457.145880	9.520563
7.797759	472.395099	9.525581
7.598793	472.694418	9.530599
7.671545	471.067167	9.535616
7.707480	481.103120	9.540634
7.720338	466.130010	9.545651
7.736878	474.565865	9.550669
7.697645	468.465491	9.555687
7.924153	466.624803	9.560704
7.661248	481.542226	9.565722
7.856529	471.207924	9.570739
7.820832	468.934952	9.575757
7.345863	463.060639	9.580775
7.695259	462.264193	9.585792
7.781907	472.165965	9.590810
7.922957	469.000618	9.595827
7.686381	475.708898	9.600845
7.416880	474.753802	9.605863
7.774654	473.870837	9.610880
7.716410	492.757727	9.615898
7.840611	469.865099	9.620915
7.651410	476.064189	9.625933
7.344418	475.083409	9.630951
8.034318	474.549190	9.635968
7.564392	480.385170	9.640986
8.036592	470.973149	9.646003
7.759839	472.982463	9.651021
8.072177	477.278933	9.656039
8.016599	479.080026	9.661056
7.616479	473.096154	9.666074
7.632403	465.241995	9.671091
7.689804	472.945620	9.676109
7.804539	470.481821	9.681127
7.826906	468.546887	9.686144
7.912958	483.059346	9.691162
7.806838	472.043282	9.696179
7.458630	479.984028	9.701197
7.468907	470.174171	9.706215
8.154606	485.094447	9.711232
7.981569	485.462286	9.716250
7.846166	479.159228	9.721267
7.975894	478.551832	9.726285
7.933929	482.831233	9.731303
8.088180	473.137670	9.736320
8.035577	480.741769	9.741338
7.917150	480.236370	9.746355
7.862319	472.421695	9.751373
7.600872	485.918795	9.756391
7.837231	490.874108	9.761408
7.830130	503.211068	9.766426
8.219269	504.778385	9.771443
8.119851	508.565025	9.776461
8.211845	503.715858	9.781479
8.604560	498.772239	9.786496
7.868257	490.505757	9.791514
7.848927	481.997557	9.796531
8.047209	495.791859	9.801549
8.001920	505.436613	9.806567
7.875117	498.816622	9.811584
7.937402	512.354536	9.816602
8.111868	503.049107	9.821619
7.917752	501.552027	9.826637
8.002784	501.437624	9.831655
8.275516	499.040584	9.836672
7.696104	510.362695	9.841690
7.945592	503.377635	9.846707
7.932555	502.584325	9.851725
7.666393	497.731316	9.856743
8.093469	502.704087	9.861760
7.982592	506.331577	9.866778
8.121598	511.955396	9.871795
8.331926	513.411875	9.876813
7.736974	506.663260	9.881831
8.016955	500.238308	9.886848
7.807225	513.730481	9.891866
7.804888	527.439477	9.896883
7.530785	531.414436	9.901901
7.892372	535.513858	9.906919
8.329888	535.208528	9.911936
8.228179	548.279862	9.916954
8.416359	533.342341	9.921971
8.519588	540.215154	9.926989
8.228758	532.980225	9.932007
8.398296	534.812325	9.937024
8.460625	535.439932	9.942042
8.806005	521.951543	9.947059
8.419315	530.561056	9.952077
8.492297	542.364791	9.957095
8.500186	532.842449	9.962112
8.159221	524.798030	9.967130
8.107044	525.566654	9.972147
8.388319	526.813204	9.977165
8.621092	536.165100	9.982183
7.993969	522.166368	9.987200
8.220082	527.741830	9.992218
8.481581	531.569756	9.997235
8.139110	537.436277	10.002253
8.345043	540.203099	10.007271
8.727136	529.792157	10.012288
8.514998	539.336839	10.017306
8.420491	522.190387	10.022323
8.263928	522.946964	10.027341
8.167407	520.727696	10.032359
8.483253	527.412557	10.037376
8.623262	533.168769	10.042394
8.409558	527.894124	10.047411
8.409359	504.418188	10.052429
8.267317	519.726958	10.057447
8.537336	515.275926	10.062464
8.619721	527.081334	10.067482
8.433203	517.867169	10.072499
8.411968	511.672442	10.077517
8.212358	518.172977	10.082535
8.581576	518.339092	10.087552
8.486754	531.100068	10.092570
8.457846	525.506138	10.097587
8.476788	521.444735	10.102605
8.340315	536.301370	10.107623
8.800576	529.400039	10.112640
8.481499	533.568237	10.117658
8.542071	528.092829	10.122675
8.509003	520.561901	10.127693
8.370214	531.502566	10.132711
8.756843	521.422276	10.137728
8.538248	526.357363	10.142746
8.463167	528.912594	10.147763
8.386886	531.089319	10.152781
8.404209	528.984755	10.157799
8.514301	529.182004	10.162816
8.619734	523.526001	10.167834
8.672121	520.317732	10.172851
8.949074	522.514850	10.177869
8.893248	525.881256	10.182887
9.026647	522.205860	10.187904
8.801029	511.053862	10.192922
8.602154	506.253424	10.197939
8.415381	498.405763	10.202957
8.555365	500.365564	10.207975
8.544778	515.186678	10.212992
8.948241	526.361115	10.218010
8.659879	518.248497	10.223027
8.622951	507.537149	10.228045
8.487320	511.947997	10.233063
8.746225	519.683186	10.238080
8.837370	533.841440	10.243098
8.752230	525.526566	10.248115
8.972618	523.535353	10.253133
8.255954	521.504766	10.258151
8.562173	521.371486	10.263168
8.794035	528.271477	10.268186
8.636733	530.293639	10.273203
8.727336	532.712459	10.278221
8.514438	531.811607	10.283239
8.531257	524.515856	10.288256
8.762382	530.112624	10.293274
8.650131	529.647280	10.298291
8.968948	529.751866	10.303309
8.710357	525.137503	10.308327
8.937948	522.416175	10.313344
8.825381	525.362285	10.318362
8.681599	530.686436	10.323379
8.849405	530.641113	10.328397
8.538737	522.692934	10.333415
8.960634	523.283138	10.338432
9.081400	528.846705	10.343450
9.040434	532.409598	10.348467
8.835725	516.836220	10.353485
8.868366	537.520338	10.358503
9.055848	534.881032	10.363520
8.916288	527.060674	10.368538
8.834187	524.207989	10.373555
8.851227	524.378792	10.378573
8.641150	521.893295	10.383591
9.053648	521.194256	10.388608
9.111910	526.966429	10.393626
8.816138	524.270298	10.398643
8.993986	520.382812	10.403661
8.513577	524.099762	10.408679
8.475968	531.420669	10.413696
8.682749	542.108383	10.418714
8.784821	552.364386	10.423731
9.258160	547.518575	10.428749
8.766302	550.839694	10.433767
9.100047	572.161481	10.438784
9.016112	557.377028	10.443802
8.840181	561.822605	10.448819
9.081071	550.666917	10.453837
9.167859	560.076413	10.458855
9.196188	556.688871	10.463872
8.850262	551.510675	10.468890
8.804782	558.119617	10.473907
9.111825	549.288851	10.478925
9.061741	558.050763	10.483943
9.216920	554.839006	10.488960
9.245647	551.296769	10.493978
8.852866	557.982217	10.498995
9.033097	553.602048	10.504013
9.561491	554.472212	10.509031
8.385221	553.170037	10.514048
8.844319	556.717701	10.519066
9.179768	562.238173	10.524083
9.103761	570.063727	10.529101
9.124597	560.719223	10.534119
9.305498	559.059240	10.539136
9.262911	559.024791	10.544154
9.101498	565.206934	10.549171
8.919800	555.969904	10.554189
9.504917	561.997211	10.559207
9.158858	559.864372	10.564224
9.333229	559.082722	10.569242
9.664718	563.549781	10.574259
9.470929	548.148234	10.579277
9.273041	565.946243	10.584295
9.710157	563.883200	10.589312
9.286911	551.146376	10.594330
8.666918	561.136823	10.599347
9.268519	562.617208	10.604365
9.305690	563.128838	10.609383
9.130204	561.127064	10.614400
9.398753	554.277851	10.619418
9.130886	562.016698	10.624435
9.251679	550.431705	10.629453
9.460503	570.927312	10.634471
9.384908	573.227010	10.639488
9.333702	566.068132	10.644506
9.458599	578.756846	10.649523
9.501479	567.209296	10.654541
9.506817	558.302720	10.659559
9.516616	557.994978	10.664576
9.686888	553.875144	10.669594
9.191653	557.749057	10.674611
9.660201	562.062098	10.679629
9.256370	551.951006	10.684647
9.443483	551.331461	10.689664
9.493943	556.252803	10.694682
9.047209	552.879734	10.699699
9.611660	561.135110	10.704717
9.343210	559.996809	10.709735
9.397008	573.413024	10.714752
9.696188	575.395228	10.719770
9.599805	588.071282	10.724787
9.759687	572.033635	10.729805
9.422666	561.438700	10.734823
9.477296	557.378010	10.739840
9.715523	548.558026	10.744858
9.454838	558.388034	10.749875
9.512663	560.546906	10.754893
9.691699	548.084947	10.759911
9.251524	551.896583	10.764928
9.499118	569.861483	10.769946
9.056653	586.586994	10.774963
9.389286	586.200267	10.779981
9.273199	584.858212	10.784999
9.325180	582.035002	10.790016
9.642793	576.001757	10.795034
9.574368	586.398102	10.800051
9.703122	582.398375	10.805069
9.621456	575.042295	10.810087
9.471152	575.245629	10.815104
9.678907	574.158947	10.820122
9.659808	577.156692	10.825139
9.599842	578.756512	10.830157
9.981755	572.129371	10.835175
9.385034	581.301989	10.840192
9.633467	574.083537	10.845210
9.773063	586.650034	10.850227
9.197219	583.347681	10.855245
9.741200	593.436641	10.860263
9.976953	606.019643	10.865280
10.086938	591.902210	10.870298
9.482466	588.367657	10.875315
9.998130	585.853649	10.880333
9.978444	581.902426	10.885351
9.656053	586.282593	10.890368
10.032917	573.300472	10.895386
9.662008	584.107125	10.900403
9.860193	579.080355	10.905421
10.007786	572.448902	10.910439
10.054362	580.864323	10.915456
9.890012	577.317618	10.920474
9.520773	575.169474	10.925491
9.909888	578.926923	10.930509
9.991048	576.301113	10.935527
9.798237	576.678364	10.940544
10.303501	568.466625	10.945562
9.968900	577.604483	10.950579
9.896232	578.537264	10.955597
9.856735	573.819134	10.960615
9.601706	587.510963	10.965632
9.805546	576.944886	10.970650
9.838054	581.225266	10.975667
10.049831	598.807644	10.980685
10.281941	603.293440	10.985703
9.895124	598.901119	10.990720
9.803642	579.122203	10.995738
9.723184	586.446691	11.000755
10.076122	601.226698	11.005773
10.231852	593.495745	11.010791
10.280790	603.810596	11.015808
9.796495	589.221389	11.020826
9.760095	595.406046	11.025843
9.733768	594.693709	11.030861
10.092205	599.759313	11.035879
10.327899	607.760108	11.040896
10.196697	598.180629	11.045914
10.345789	601.161493	11.050931
10.527639	605.513154	11.055949
10.326208	589.579438	11.060967
10.096055	577.664406	11.065984
9.879122	576.066754	11.071002
10.279478	579.569978	11.076019
9.888758	581.060675	11.081037
10.111918	573.527448	11.086055
9.718474	595.638538	11.091072
10.416059	596.422236	11.096090
10.062975	604.701471	11.101107
10.224162	599.945578	11.106125
10.120301	599.794498	11.111143
10.211438	604.352875	11.116160
10.552109	601.143604	11.121178
10.380445	606.882400	11.126195
10.326435	604.050548	11.131213
10.152959	598.454000	11.136231
10.001543	602.163600	11.141248
10.245348	591.165220	11.146266
10.365060	598.411013	11.151283
10.279038	596.347880	11.156301
10.632007	597.819887	11.161319
10.491648	604.844499	11.166336
10.229017	596.339651	11.171354
10.065514	588.106452	11.176371
9.988633	599.602347	11.181389
10.165403	599.154834	11.186407
10.079582	606.092007	11.191424
10.321842	603.100126	11.196442
10.619588	596.628175	11.201459
10.597802	605.638140	11.206477
10.696604	607.904207	11.211495
10.395338	607.001418	11.216512
10.545598	611.705167	11.221530
10.731530	603.407745	11.226547
10.093694	612.530016	11.231565
10.294257	598.688719	11.236583
10.339228	608.603408	11.241600
10.387079	598.655050	11.246618
10.430976	599.818877	11.251635
10.076794	612.216604	11.256653
10.414028	594.724728	11.261671
10.333127	602.506881	11.266688
10.479647	602.083043	11.271706
10.554174	593.276062	11.276723
10.589993	587.088149	11.281741
11.037280	591.830562	11.286759
10.818071	599.056873	11.291776
10.625187	598.724081	11.296794
10.902563	603.287992	11.301811
10.804826	612.259368	11.306829
10.952460	594.008248	11.311847
10.225011	602.633315	11.316864
10.320161	602.798192	11.321882
10.564416	595.817071	11.326899
10.645825	600.386438	11.331917
10.774192	601.006857	11.336935
10.438057	597.184107	11.341952
10.145656	606.334302	11.346970
10.531507	606.579864	11.351987
10.527446	601.083003	11.357005
11.002647	591.026666	11.362023
10.809632	605.273680	11.367040
10.864083	607.341569	11.372058
10.949879	596.513110	11.377075
10.943952	597.952986	11.382093
11.139790	597.625562	11.387111
10.662632	606.369205	11.392128
10.558834	599.893894	11.397146
10.493031	590.089579	11.402163
10.697285	597.716600	11.407181
10.576934	601.055260	11.412199
10.103167	608.147891	11.417216
10.307282	597.032650	11.422234
10.671539	595.590087	11.427251
11.001803	608.921987	11.432269
11.219550	605.378526	11.437287
10.412211	603.248527	11.442304
10.417378	602.162027	11.447322
11.170943	611.732167	11.452339
10.836720	618.402151	11.457357
11.296917	617.411614	11.462375
10.643531	617.883119	11.467392
10.794266	605.182557	11.472410
11.003046	615.298802	11.477427
11.040694	625.968884	11.482445
10.923962	617.794616	11.487463
11.297749	625.076351	11.492480
10.914821	615.037687	11.497498
11.078081	607.419157	11.502515
10.549965	615.716353	11.507533
11.000544	616.866956	11.512551
11.159917	630.913612	11.517568
10.784659	613.015798	11.522586
10.981380	614.553313	11.527603
10.659660	627.845368	11.532621
10.798983	620.445178	11.537639
11.123438	621.034874	11.542656
11.210465	624.625069	11.547674
11.575620	619.038796	11.552691
11.154732	624.870295	11.557709
10.996118	621.603549	11.562727
10.995052	626.785447	11.567744
10.731628	628.199399	11.572762
11.363518	626.815887	11.577779
10.988391	623.400027	11.582797
11.143900	621.027650	11.587815
11.189952	635.619083	11.592832
11.369819	625.987696	11.597850
11.034035	621.675736	11.602867
11.115374	637.284122	11.607885
11.084613	623.854591	11.612903
11.071737	630.004016	11.617920
11.010397	625.163062	11.622938
11.178472	623.514550	11.627955
11.130199	623.099140	11.632973
11.148030	622.329390	11.637991
11.184066	619.982043	11.643008
10.598654	625.548986	11.648026
10.975007	610.386259	11.653043
11.214298	629.788409	11.658061
11.270441	637.022087	11.663079
11.579116	651.007496	11.668096
11.510347	635.378002	11.673114
11.312244	620.052808	11.678131
11.099872	628.991661	11.683149
11.219981	629.673334	11.688167
11.749201	641.942139	11.693184
11.275287	636.288510	11.698202
11.566500	625.361576	11.703219
11.300121	625.204401	11.708237
11.753014	630.917933	11.713255
11.421736	618.658956	11.718272
11.254045	618.587304	11.723290
11.312576	624.463609	11.728307
11.088996	622.478830	11.733325
11.400695	633.194341	11.738343
11.546762	640.944106	11.743360
11.653009	641.997181	11.748378
11.738322	636.622006	11.753395
11.488582	627.121045	11.758413
11.432594	631.235421	11.763431
11.574784	639.686382	11.768448
11.522252	634.326493	11.773466
11.612926	628.271982	11.778483
11.505845	627.509180	11.783501
11.592498	632.061955	11.788519
11.753306	628.707291	11.793536
11.533018	620.353587	11.798554
11.655922	611.813573	11.803571
11.650138	620.874687	11.808589
11.265760	618.438577	11.813607
11.817468	622.274701	11.818624
11.301977	636.089428	11.823642
11.499202	632.773238	11.828659
11.683636	635.379342	11.833677
12.091920	640.131035	11.838695
11.760170	637.150189	11.843712
11.469692	646.082353	11.848730
11.444468	646.155637	11.853747
11.411888	640.852580	11.858765
11.666645	642.358914	11.863783
11.770414	638.965848	11.868800
11.743456	637.164855	11.873818
11.949030	633.392922	11.878835
11.615204	648.028106	11.883853
11.682040	646.909850	11.888871
11.810256	641.423810	11.893888
11.832653	644.131042	11.898906
11.939687	641.472767	11.903923
11.767389	640.142670	11.908941
11.761095	637.189727	11.913959
11.947281	643.557277	11.918976
11.624089	644.403082	11.923994
11.857349	635.053658	11.929011
11.702034	641.001342	11.934029
11.623574	644.541730	11.939047
11.921408	639.821222	11.944064
11.645558	638.302223	11.949082
12.163660	648.874951	11.954099
11.936455	646.445769	11.959117
11.732723	644.085493	11.964135
11.952490	646.121173	11.969152
11.749368	642.754099	11.974170
11.844946	641.211618	11.979187
12.108905	654.875833	11.984205
11.954058	650.699619	11.989223
12.123878	643.853218	11.994240
12.043277	643.767921	11.999258
12.295833	645.192549	12.004275
12.001316	647.668568	12.009293
12.286343	642.918508	12.014311
11.982482	639.721853	12.019328
11.934488	636.396747	12.024346
11.806819	635.776025	12.029363
11.886777	651.368861	12.034381
12.089689	661.684868	12.039399
12.297230	663.596233	12.044416
12.237359	666.073361	12.049434
12.638647	665.372918	12.054451
11.967021	651.024450	12.059469
12.103939	646.300750	12.064487
12.308466	642.273359	12.069504
12.243229	644.154877	12.074522
12.298779	641.675081	12.079539
12.067788	643.184938	12.084557
12.088427	635.945348	12.089575
12.420926	643.530205	12.094592
11.930446	642.155286	12.099610
12.173021	657.129357	12.104627
12.074813	661.483885	12.109645
12.456207	663.812980	12.114663
12.343182	655.915825	12.119680
12.192117	662.124782	12.124698
12.580660	650.797575	12.129715
12.772569	661.749623	12.134733
12.108287	642.757816	12.139751
12.431647	651.098346	12.144768
12.258983	655.840079	12.149786
12.335890	655.524976	12.154803
12.675301	666.169894	12.159821
12.529549	657.050255	12.164839
12.493950	640.475129	12.169856
12.164919	635.474142	12.174874
12.768105	639.791354	12.179891
12.546738	637.866187	12.184909
12.259814	639.902359	12.189927
12.216787	640.533854	12.194944
12.606787	654.929403	12.199962
12.668916	664.080885	12.204979
12.480941	643.240886	12.209997
12.251619	644.403343	12.215015
12.450647	646.032017	12.220032
12.520954	655.923828	12.225050
12.369187	654.562112	12.230067
12.685765	658.302540	12.235085
12.540235	661.774544	12.240103
12.705802	657.238857	12.245120
12.404029	660.978339	12.250138
12.444937	661.495698	12.255155
12.600832	652.369826	12.260173
12.786438	656.051879	12.265191
12.662513	656.705517	12.270208
12.642854	658.043409	12.275226
12.743133	668.255579	12.280243
12.836178	660.026333	12.285261
12.540529	664.765247	12.290279
12.701891	662.227845	12.295296
12.809431	663.902413	12.300314
12.891623	660.711540	12.305331
13.001670	658.440955	12.310349
12.562978	660.336806	12.315367
12.650010	670.330146	12.320384
12.439290	669.978057	12.325402
12.611103	663.421671	12.330419
12.654244	658.191952	12.335437
12.169574	661.436226	12.340455
12.428799	661.490189	12.345472
12.681164	663.296702	12.350490
12.392246	671.884651	12.355507
13.157923	677.334596	12.360525
12.906454	683.041739	12.365543
12.998167	680.467910	12.370560
13.209014	686.456069	12.375578
13.216629	674.702535	12.380595
12.895848	667.945616	12.385613
12.636937	665.029092	12.390631
12.654466	663.366294	12.395648
12.526835	678.057558	12.400666
12.565645	692.602836	12.405683
13.055515	680.360327	12.410701
12.585533	691.409786	12.415719
13.040026	684.528235	12.420736
13.154895	687.785876	12.425754
13.134911	680.798785	12.430771
13.211237	677.583582	12.435789
12.845267	684.697222	12.440807
12.715113	684.559728	12.445824
12.761019	684.697607	12.450842
12.972554	680.975223	12.455859
13.254915	678.996374	12.460877
13.020509	687.547388	12.465895
13.548052	681.168790	12.470912
13.133841	687.526284	12.475930
12.985682	684.504041	12.480947
13.147427	679.063229	12.485965
13.060659	678.275152	12.490983
13.118121	682.229753	12.496000
12.874633	682.233093	12.501018
13.163776	687.631472	12.506035
13.592893	691.755063	12.511053
13.319610	687.663669	12.516071
13.364186	674.433735	12.521088
12.789875	688.772115	12.526106
13.190619	694.503306	12.531123
13.544450	702.384648	12.536141
13.396100	703.802666	12.541159
13.437765	689.130969	12.546176
13.409324	678.967300	12.551194
13.172382	680.623260	12.556211
13.554848	678.461469	12.561229
13.354634	687.228032	12.566247
13.315719	678.994206	12.571264
13.229047	676.303159	12.576282
13.286601	697.169751	12.581299
13.728781	699.530353	12.586317
13.271059	700.804339	12.591335
13.298853	696.776223	12.596352
13.579457	698.098631	12.601370
13.584635	707.034995	12.606387
13.860055	690.303794	12.611405
13.262114	693.341758	12.616423
13.692082	682.086936	12.621440
13.817273	682.439611	12.626458
13.639240	679.968006	12.631475
13.596174	682.600294	12.636493
13.481578	682.116378	12.641511
13.632320	676.459540	12.646528
13.726889	677.577563	12.651546
13.562307	678.976032	12.656563
13.469518	672.492659	12.661581
13.358226	681.431480	12.666599
13.261753	671.843364	12.671616
13.856440	692.098773	12.676634
13.718919	694.297736	12.681651
13.998536	698.877099	12.686669
13.764990	681.556618	12.691687
13.537299	673.257697	12.696704
13.860822	677.003353	12.701722
13.643760	674.585201	12.706739
13.699507	677.268278	12.711757
13.512538	693.736107	12.716775
13.736826	695.496529	12.721792
13.886174	697.969283	12.726810
14.020180	702.918601	12.731827
14.080251	685.413256	12.736845
13.826036	675.666817	12.741863
13.532642	680.594731	12.746880
13.837145	684.125617	12.751898
13.995583	691.286485	12.756915
13.647929	685.698264	12.761933
13.887954	697.015181	12.766951
13.994533	696.338821	12.771968
13.961733	694.040119	12.776986
13.759716	697.435774	12.782003
13.937262	703.350262	12.787021
13.931069	694.637929	12.792039
14.080070	695.668530	12.797056
13.971184	690.604633	12.802074
13.911401	699.529081	12.807091
13.978539	687.551617	12.812109
13.970957	700.636717	12.817127
13.973759	698.512318	12.822144
14.051499	700.803787	12.827162
14.028063	700.933596	12.832179
13.989644	695.767138	12.837197
13.888150	698.998720	12.842215
14.002422	694.691967	12.847232
13.686159	687.442025	12.852250
13.931439	700.216107	12.857267
13.902594	693.426060	12.862285
13.922650	695.259506	12.867303
13.763517	694.949827	12.872320
14.272602	694.289298	12.877338
13.901855	703.899944	12.882355
14.349878	693.295540	12.887373
14.281846	699.485190	12.892391
14.291989	702.339518	12.897408
14.328189	706.717179	12.902426
14.204369	698.610257	12.907443
13.870582	698.413149	12.912461
14.259135	709.085107	12.917479
14.189908	725.143196	12.922496
14.290958	723.344229	12.927514
14.398203	731.380984	12.932531
14.259279	728.691804	12.937549
14.384755	725.270075	12.942567
14.641584	718.795023	12.947584
14.521293	721.581428	12.952602
14.471434	722.198217	12.957619
14.354006	716.908432	12.962637
14.336766	719.176915	12.967655
14.264266	717.632359	12.972672
14.620755	713.789427	12.977690
14.625570	726.658008	12.982707
14.822007	718.728118	12.987725
14.234193	705.780280	12.992743
14.100610	708.650817	12.997760
14.560308	712.738064	13.002778
14.532314	727.966026	13.007795
14.692198	717.277365	13.012813
14.659220	723.881255	13.017831
14.232545	720.113689	13.022848
14.616569	713.132714	13.027866
14.596183	725.112146	13.032883
14.433813	723.796267	13.037901
14.820369	723.931266	13.042919
14.565829	724.876772	13.047936
14.691143	722.206153	13.052954
14.340306	719.991992	13.057971
14.430047	718.371524	13.062989
14.751028	721.006739	13.068007
14.495174	725.433320	13.073024
14.671694	714.596886	13.078042
14.789391	726.946006	13.083059
14.811830	724.654424	13.088077
14.439155	724.015283	13.093095
14.204245	716.260274	13.098112
14.471817	711.165791	13.103130
14.353379	730.333764	13.108147
14.433830	743.020091	13.113165
14.876189	746.311640	13.118183
14.726131	745.587124	13.123200
15.387170	745.130005	13.128218
15.038920	750.132805	13.133235
14.860498	748.863620	13.138253
15.049550	742.026792	13.143271
14.939425	746.490506	13.148288
15.246479	742.147225	13.153306
15.167785	742.093187	13.158323
14.714315	728.442626	13.163341
14.821317	733.759103	13.168359
14.882719	740.092590	13.173376
15.432039	733.981962	13.178394
15.113636	735.496055	13.183411
14.968521	723.816911	13.188429
15.154399	714.566389	13.193447
14.837994	720.204822	13.198464
15.177438	724.383497	13.203482
14.878195	730.104451	13.208499
15.290611	736.436589	13.213517
15.690659	739.725298	13.218535
15.255959	728.069432	13.223552
15.110167	711.760814	13.228570
15.008216	721.247304	13.233587
15.248795	717.996890	13.238605
15.204485	720.339043	13.243623
14.498650	720.749340	13.248640
15.475021	724.335913	13.253658
15.036355	746.258614	13.258675
15.207690	743.012734	13.263693
15.186791	733.580003	13.268711
15.037052	749.742248	13.273728
15.523949	741.107271	13.278746
15.359262	743.354678	13.283763
15.151902	741.190618	13.288781
15.398870	742.259521	13.293799
15.109307	744.220379	13.298816
15.542845	737.588245	13.303834
15.572253	742.942128	13.308851
15.394871	746.431763	13.313869
15.481104	736.228004	13.318887
15.537605	748.943335	13.323904
15.606302	735.558097	13.328922
15.458263	747.036833	13.333939
14.984941	758.557074	13.338957
15.591892	747.457520	13.343975
14.933590	746.402379	13.348992
15.416485	741.498214	13.354010
15.494265	745.850435	13.359027
15.689372	754.258445	13.364045
15.898425	743.751414	13.369063
15.456076	745.682561	13.374080
15.470964	749.517614	13.379098
15.938524	753.701469	13.384115
15.473645	748.548164	13.389133
15.579520	744.365793	13.394151
15.539384	759.942825	13.399168
15.569681	748.561232	13.404186
15.532100	747.487733	13.409203
16.022819	753.438377	13.414221
15.988896	750.817950	13.419239
15.672007	744.174001	13.424256
15.538427	748.530936	13.429274
15.626042	745.181407	13.434291
15.143755	747.276602	13.439309
15.643439	749.612422	13.444327
15.620621	742.736205	13.449344
15.537884	739.438614	13.454362
15.715484	756.789816	13.459379
16.066965	769.380049	13.464397
15.864008	744.304002	13.469415
15.731462	752.365714	13.474432
15.924177	752.095581	13.479450
16.131893	755.802593	13.484467
15.633783	757.698296	13.489485
15.936815	749.006917	13.494503
15.858991	766.016293	13.499520
15.925065	763.433845	13.504538
15.992096	766.632723	13.509555
15.861500	765.876756	13.514573
16.192219	763.145546	13.519591
16.058626	766.246468	13.524608
15.981194	761.742516	13.529626
16.359576	759.641316	13.534643
15.731603	759.897402	13.539661
16.300666	755.550936	13.544679
16.068201	758.288650	13.549696
16.523958	756.162704	13.554714
16.236412	750.025399	13.559731
15.690498	745.591696	13.564749
16.175755	747.506896	13.569767
15.903898	760.428317	13.574784
15.838020	759.744261	13.579802
16.097861	755.370504	13.584819
16.187275	764.236895	13.589837
16.201562	763.931601	13.594855
16.458845	767.239527	13.599872
15.885825	763.374960	13.604890
16.041210	760.617572	13.609907
15.827140	763.964635	13.614925
15.944231	767.483876	13.619943
16.205474	768.212871	13.624960
16.162969	764.807985	13.629978
16.509436	768.834090	13.634995
16.501242	777.374950	13.640013
16.497534	762.195902	13.645031
16.263541	768.843927	13.650048
16.221715	758.950555	13.655066
16.131063	762.294059	13.660083
16.003769	777.802712	13.665101
16.710666	774.542343	13.670119
16.507377	785.603723	13.675136
16.487278	785.041883	13.680154
16.684281	786.882328	13.685171
16.727136	789.280262	13.690189
16.463722	778.689444	13.695207
16.957794	779.647050	13.700224
16.793192	776.166617	13.705242
16.503969	763.124617	13.710259
16.663015	768.858987	13.715277
16.490226	770.426008	13.720295
16.632194	774.200130	13.725312
16.771008	779.795661	13.730330
16.977931	785.304783	13.735347
16.733541	769.361858	13.740365
16.648373	754.258696	13.745383
16.800170	765.087704	13.750400
16.592728	765.650289	13.755418
16.798303	760.817971	13.760435
16.741253	770.259581	13.765453
17.064842	764.054922	13.770471
16.538127	765.027295	13.775488
16.899688	764.512955	13.780506
17.112948	768.247504	13.785523
16.814906	762.585213	13.790541
16.735488	747.307586	13.795559
16.830208	752.827966	13.800576
16.823992	757.625699	13.805594
17.100750	767.292720	13.810611
16.431907	764.440407	13.815629
16.770492	778.250816	13.820647
16.762404	776.746657	13.825664
16.712863	788.907426	13.830682
16.749378	783.896461	13.835699
17.142554	792.813103	13.840717
17.092524	785.650797	13.845735
16.910058	782.207876	13.850752
16.990490	785.316294	13.855770
17.046118	783.966255	13.860787
16.696181	789.344873	13.865805
17.010825	777.091883	13.870823
17.186267	780.384232	13.875840
17.004015	783.991403	13.880858
16.794171	772.473849	13.885875
17.001799	772.939843	13.890893
17.075310	770.229996	13.895911
16.773882	787.369101	13.900928
16.825219	793.745210	13.905946
17.321779	795.071659	13.910963
17.305564	811.960971	13.915981
17.512566	803.208871	13.920999
17.485728	807.362903	13.926016
17.486605	810.796218	13.931034
17.695658	796.659945	13.936051
17.565245	797.459773	13.941069
17.278764	784.060719	13.946087
17.431203	780.571638	13.951104
17.305077	781.560143	13.956122
17.242726	778.950477	13.961139
17.508198	788.963264	13.966157
17.530160	796.603153	13.971175
17.668915	794.836141	13.976192
17.448494	785.879616	13.981210
17.362564	779.776984	13.986227
17.135069	780.052375	13.991245
17.476779	792.741986	13.996263
17.537651	793.300403	14.001280
17.137653	798.781543	14.006298
17.515626	797.930113	14.011315
17.074095	805.910871	14.016333
17.324558	807.474697	14.021351
17.502783	808.191454	14.026368
17.159129	806.130792	14.031386
17.645079	794.059235	14.036403
17.463572	805.151929	14.041421
17.957695	824.820481	14.046439
17.803023	802.545483	14.051456
17.846333	795.911351	14.056474
17.778464	798.995671	14.061491
17.903615	800.288793	14.066509
17.538441	798.524996	14.071527
17.574023	788.755180	14.076544
17.415619	808.563821	14.081562
17.839205	818.214177	14.086579
17.922486	817.762371	14.091597
18.085958	817.427391	14.096615
18.017998	813.212278	14.101632
17.911545	819.092405	14.106650
17.898372	806.600420	14.111667
17.926285	811.954559	14.116685
18.111588	809.201944	14.121703
18.137046	800.232134	14.126720
17.746793	793.274610	14.131738
18.028151	795.240697	14.136755
17.997702	812.813900	14.141773
18.114192	809.204212	14.146791
18.316810	803.450843	14.151808
17.708385	795.587062	14.156826
18.139626	799.972281	14.161843
17.859128	805.807088	14.166861
17.726552	809.864077	14.171879
17.974636	812.125715	14.176896
18.014128	818.257533	14.181914
18.344563	810.331855	14.186931
18.326527	814.620209	14.191949
18.667033	814.762425	14.196967
18.458110	817.641628	14.201984
17.883726	814.354781	14.207002
18.334007	805.665549	14.212019
18.515704	812.690277	14.217037
18.290845	807.262661	14.222055
18.152667	806.280659	14.227072
17.946726	819.011913	14.232090
18.492195	808.865549	14.237107
18.555635	812.194387	14.242125
18.378566	812.913162	14.247143
18.454690	806.475859	14.252160
18.269399	810.815664	14.257178
18.346618	807.956907	14.262195
18.495776	813.168972	14.267213
18.148522	815.741640	14.272231
18.555296	814.352361	14.277248
18.664332	816.033021	14.282266
18.755084	810.259306	14.287283
18.393140	811.862278	14.292301
18.365429	814.769893	14.297319
18.159894	807.026022	14.302336
18.457997	808.626565	14.307354
18.667922	809.205811	14.312371
18.065666	815.286696	14.317389
18.165044	818.117594	14.322407
18.430579	820.527980	14.327424
18.541021	834.358398	14.332442
18.603652	835.030151	14.337459
19.000215	833.121756	14.342477
18.900583	837.539667	14.347495
19.017631	834.737781	14.352512
18.649926	830.765290	14.357530
18.690640	833.384473	14.362547
18.812772	837.297418	14.367565
18.820964	839.994282	14.372583
18.967496	836.995271	14.377600
18.997885	846.158131	14.382618
18.727328	840.229574	14.387635
18.875046	841.269852	14.392653
18.583925	834.583962	14.397671
18.813375	835.220110	14.402688
19.128100	846.964080	14.407706
18.839042	834.013522	14.412723
19.231979	837.861947	14.417741
19.181963	838.576596	14.422759
19.281537	832.681569	14.427776
19.013187	829.605549	14.432794
19.185361	834.520522	14.437811
19.272575	834.326878	14.442829
19.083424	834.845574	14.447847
19.177839	826.445621	14.452864
19.126916	829.189616	14.457882
19.125071	819.472984	14.462899
19.141331	821.206051	14.467917
19.120711	827.669186	14.472935
19.405309	828.501823	14.477952
19.032876	823.084700	14.482970
18.934488	828.647983	14.487987
19.445175	839.345065	14.493005
18.876639	836.966180	14.498023
18.824354	836.661847	14.503040
19.005567	835.254258	14.508058
19.110820	827.404878	14.513075
19.409551	826.256590	14.518093
18.751912	832.611249	14.523111
19.466861	821.175988	14.528128
19.106083	835.190692	14.533146
19.321664	839.417203	14.538163
19.666332	847.483085	14.543181
19.280565	842.446746	14.548199
19.630056	844.926033	14.553216
19.622714	856.676289	14.558234
19.599381	846.552750	14.563251
19.312831	835.422719	14.568269
19.498610	846.681957	14.573287
19.837761	857.446952	14.578304
19.504198	842.676127	14.583322
19.896277	842.046550	14.588339
19.917888	846.754739	14.593357
19.240912	827.237698	14.598375
19.723808	830.901611	14.603392
19.600417	843.512650	14.608410
19.914507	853.536791	14.613427
19.749550	852.041424	14.618445
19.758728	849.559398	14.623463
19.633640	837.141731	14.628480
19.896694	842.809335	14.633498
19.810004	847.414571	14.638515
19.987372	852.202501	14.643533
19.914077	842.841039	14.648551
19.902816	844.477433	14.653568
19.722903	842.545748	14.658586
19.931716	850.266839	14.663603
20.265674	855.390001	14.668621
19.694739	834.082754	14.673639
19.940171	835.884059	14.678656
20.056005	846.198037	14.683674
19.845961	842.980334	14.688691
20.125914	844.340724	14.693709
20.005159	859.375047	14.698727
19.829371	853.895547	14.703744
19.799286	854.925814	14.708762
20.169635	845.397009	14.713779
20.459879	850.113604	14.718797
20.037925	852.480228	14.723815
20.286878	854.079009	14.728832
20.058123	850.242536	14.733850
19.961361	852.766495	14.738867
19.997848	856.787538	14.743885
20.012882	853.704984	14.748903
20.060537	850.137631	14.753920
20.142014	847.098317	14.758938
19.851923	841.766119	14.763955
20.264777	851.519161	14.768973
19.859979	855.691396	14.773991
20.023461	860.894919	14.779008
20.347133	869.923477	14.784026
20.501145	872.695330	14.789043
20.507554	863.570681	14.794061
20.391774	874.422743	14.799079
20.529118	865.438526	14.804096
20.419230	877.116499	14.809114
20.442284	872.956541	14.814131
20.708815	867.609708	14.819149
20.744092	876.617182	14.824167
20.564975	858.988195	14.829184
20.652748	847.417650	14.834202
20.237034	846.065715	14.839219
20.866439	858.479921	14.844237
20.679132	848.896475	14.849255
20.326059	848.778126	14.854272
20.680578	861.721403	14.859290
20.673305	865.212811	14.864307
20.808362	865.292542	14.869325
20.691364	870.246519	14.874343
21.106737	865.135147	14.879360
20.697270	860.689504	14.884378
20.296160	856.412968	14.889395
20.499830	864.803909	14.894413
20.666897	867.327561	14.899431
20.779586	860.849794	14.904448
20.708860	866.440313	14.909466
20.384352	866.895009	14.914483
20.573666	861.254160	14.919501
20.800557	872.999286	14.924519
20.813641	865.483071	14.929536
21.017453	875.300437	14.934554
20.645354	871.988197	14.939571
20.615751	875.259041	14.944589
20.760015	890.475932	14.949607
20.827572	890.916538	14.954624
20.756662	892.385555	14.959642
20.744504	895.814617	14.964659
21.384533	890.406103	14.969677
21.128856	892.109199	14.974695
21.070719	893.036564	14.979712
21.324928	892.248703	14.984730
21.447941	890.342136	14.989747
21.245412	884.488113	14.994765
21.170979	888.728517	14.999783
21.395991	890.340520	15.004800
21.400458	880.395645	15.009818
21.337970	890.453562	15.014835
21.385632	889.862166	15.019853
21.413343	888.996182	15.024871
21.326362	882.000574	15.029888
21.462001	889.679498	15.034906
21.163091	901.554361	15.039923
21.639235	887.956846	15.044941
21.776228	886.729752	15.049959
21.509509	892.350987	15.054976
21.944161	887.795173	15.059994
21.888053	890.221248	15.065011
21.444861	873.933831	15.070029
21.115941	878.722196	15.075047
21.585641	879.510055	15.080064
21.713875	881.266610	15.085082
21.675433	879.991263	15.090099
22.003997	879.024492	15.095117
21.717640	877.333546	15.100135
21.780888	871.216978	15.105152
21.605207	865.519703	15.110170
21.419520	866.372376	15.115187
21.662207	875.164313	15.120205
21.787128	875.854711	15.125223
22.062131	884.985577	15.130240
22.247759	878.385922	15.135258
21.610189	870.226869	15.140275
21.745568	864.319910	15.145293
21.659340	860.521065	15.150311
21.625284	864.363811	15.155328
21.690666	878.769377	15.160346
21.686863	874.253860	15.165363
21.739765	873.014695	15.170381
21.653489	877.859718	15.175399
21.974188	885.143566	15.180416
21.892657	881.994085	15.185434
21.950632	877.875992	15.190451
21.765726	877.166399	15.195469
21.892791	879.551150	15.200487
22.265308	877.876895	15.205504
22.148064	876.695947	15.210522
21.656785	879.430047	15.215539
22.215889	876.659882	15.220557
22.337629	879.651390	15.225575
21.928538	885.989216	15.230592
22.003213	882.663779	15.235610
22.146085	904.729093	15.240627
22.471438	884.969737	15.245645
22.270636	885.487103	15.250663
22.033879	885.896492	15.255680
22.483272	883.490658	15.260698
22.171984	892.975323	15.265715
22.500352	905.654482	15.270733
22.779882	912.357803	15.275751
22.183976	886.693016	15.280768
22.531360	889.336744	15.285786
22.501494	901.040064	15.290803
22.623978	882.028875	15.295821
22.235671	884.838362	15.300839
22.583505	900.045458	15.305856
22.807333	899.114031	15.310874
22.398552	896.280911	15.315891
22.561722	895.273781	15.320909
22.863824	896.586524	15.325927
22.413168	886.245888	15.330944
22.435429	883.884885	15.335962
22.467314	899.034184	15.340979
22.577228	910.078128	15.345997
22.623501	904.999327	15.351015
22.322851	898.125555	15.356032
22.886316	901.808418	15.361050
22.741961	899.924805	15.366067
22.557887	904.172923	15.371085
22.790492	901.075207	15.376103
22.688861	902.220830	15.381120
22.664235	897.247815	15.386138
22.345728	898.515780	15.391155
22.624009	902.375872	15.396173
22.842181	913.611143	15.401191
23.059925	925.061086	15.406208
23.069199	917.258264	15.411226
22.786689	914.493721	15.416243
22.767254	911.107284	15.421261
22.697653	902.903409	15.426279
22.721771	917.343873	15.431296
23.074360	917.487353	15.436314
22.923037	915.219817	15.441331
22.991368	910.907587	15.446349
23.398445	910.430294	15.451367
23.401969	912.203236	15.456384
23.616143	914.766851	15.461402
23.151828	916.565755	15.466419
23.035350	912.784261	15.471437
23.576056	921.384359	15.476455
23.212092	911.834868	15.481472
23.261477	906.944930	15.486490
23.312273	914.621378	15.491507
23.267944	917.209716	15.496525
23.248161	913.876982	15.501543
23.437454	917.261863	15.506560
23.354893	915.529515	15.511578
23.283339	914.010041	15.516595
23.125145	903.898131	15.521613
23.229049	907.728740	15.526631
23.292262	912.796507	15.531648
23.703398	923.010613	15.536666
23.403018	927.131790	15.541683
23.599095	925.283200	15.546701
23.669963	924.445167	15.551719
23.508055	933.300524	15.556736
23.967940	922.956063	15.561754
23.690247	916.110245	15.566771
23.381224	917.215777	15.571789
24.048011	923.918389	15.576807
23.648657	931.504424	15.581824
23.920614	919.803987	15.586842
23.796020	921.139404	15.591859
23.869106	923.987062	15.596877
24.001441	909.853253	15.601895
23.574130	918.428288	15.606912
23.725219	913.374089	15.611930
23.742292	923.741456	15.616947
23.883688	932.303135	15.621965
23.761064	933.117528	15.626983
23.763263	937.327001	15.632000
23.834368	935.160314	15.637018
24.123077	931.845516	15.642035
23.968683	934.009281	15.647053
23.944972	929.982871	15.652071
23.782875	932.163622	15.657088
24.160752	933.455028	15.662106
24.073419	926.734018	15.667123
23.835141	933.171332	15.672141
24.005696	925.946005	15.677159
24.024785	932.279878	15.682176
24.221705	939.646259	15.687194
24.293787	952.835829	15.692211
24.604284	944.843786	15.697229
24.224218	926.675006	15.702247
24.295436	927.061389	15.707264
24.333544	926.345255	15.712282
24.188637	928.769469	15.717299
24.279520	943.682341	15.722317
24.624384	946.244419	15.727335
24.650613	951.333772	15.732352
24.531241	945.217388	15.737370
24.366938	950.099902	15.742387
24.547969	954.622193	15.747405
24.809810	946.700890	15.752423
24.480436	935.501765	15.757440
24.693838	931.917894	15.762458
24.596081	932.365467	15.767475
24.511838	937.629917	15.772493
24.776435	930.607608	15.777511
24.485298	942.314021	15.782528
24.741887	943.185767	15.787546
24.757170	942.599442	15.792563
24.562784	946.309534	15.797581
25.002170	949.396456	15.802599
24.611652	952.771199	15.807616
24.733013	943.060443	15.812634
24.692616	955.096815	15.817651
24.635293	958.668667	15.822669
24.981078	949.345632	15.827687
24.818829	960.590042	15.832704
24.879494	962.634908	15.837722
25.120004	958.693328	15.842739
24.401527	963.795219	15.847757
24.928728	943.846380	15.852775
24.647196	950.874311	15.857792
24.886889	951.770795	15.862810
24.999493	951.453250	15.867827
24.918401	950.629556	15.872845
25.213162	957.226365	15.877863
25.028956	973.918085	15.882880
25.367082	971.365568	15.887898
25.324516	974.916177	15.892915
24.893835	971.202834	15.897933
25.393580	967.700328	15.902951
25.451165	967.997328	15.907968
25.508465	977.840862	15.912986
25.175036	963.208774	15.918003
25.149027	969.975767	15.923021
25.417812	969.327633	15.928039
25.406743	981.264751	15.933056
25.940172	971.306378	15.938074
25.457007	956.937601	15.943091
25.128001	956.970118	15.948109
25.740257	960.329763	15.953127
25.660325	967.231439	15.958144
25.883959	963.488166	15.963162
25.853275	946.479631	15.968179
25.136178	942.404063	15.973197
25.345058	948.294789	15.978215
25.484215	964.755953	15.983232
25.460393	965.655854	15.988250
25.702569	968.000491	15.993267
25.585698	973.121738	15.998285
25.860429	969.556654	16.003303
25.826323	978.199502	16.008320
25.843535	970.335452	16.013338
25.810474	969.194957	16.018355
25.643176	973.225864	16.023373
26.164537	972.232038	16.028391
25.966625	975.724934	16.033408
25.741028	970.900153	16.038426
25.768057	974.818562	16.043443
25.628536	965.827179	16.048461
26.040721	958.778580	16.053479
25.817711	968.227362	16.058496
26.097224	967.710094	16.063514
26.597749	972.056097	16.068531
26.047990	967.556667	16.073549
26.231567	967.631952	16.078567
26.234294	968.647617	16.083584
26.090207	966.221146	16.088602
26.034284	969.985290	16.093619
26.000259	967.566822	16.098637
26.199854	961.892772	16.103655
26.158196	965.550535	16.108672
26.031772	966.908333	16.113690
26.369278	982.057156	16.118707
26.179722	994.697603	16.123725
26.283649	991.645280	16.128743
26.189784	994.566444	16.133760
25.869212	998.671866	16.138778
26.656191	994.543671	16.143795
25.992373	992.473188	16.148813
26.462071	994.144696	16.153831
26.240386	998.379793	16.158848
26.350278	991.305959	16.163866
26.974652	986.467926	16.168883
26.689206	995.547801	16.173901
26.703365	989.514624	16.178919
26.810530	990.674876	16.183936
26.593393	991.368377	16.188954
26.541003	989.132668	16.193971
26.624556	982.375395	16.198989
26.685193	983.195791	16.204007
26.543874	989.766260	16.209024
26.315874	989.745081	16.214042
27.015795	1007.140926	16.219059
26.997189	1012.568687	16.224077
27.180781	1007.698721	16.229095
27.295530	1006.086932	16.234112
26.629559	998.273103	16.239130
27.187930	989.090312	16.244147
26.791217	1000.570302	16.249165
27.007374	1000.031401	16.254183
26.887255	1006.090459	16.259200
26.981471	1012.630344	16.264218
27.419033	1009.544680	16.269235
26.919965	1012.014927	16.274253
27.035453	1009.137518	16.279271
27.139869	1011.734123	16.284288
26.739399	1004.655037	16.289306
27.313234	1001.945663	16.294323
27.146885	1007.709001	16.299341
27.311876	1010.763185	16.304359
26.902135	1011.966555	16.309376
27.086376	1016.273760	16.314394
27.169959	1016.935925	16.319411
27.269614	1019.224002	16.324429
26.950041	1013.205235	16.329447
27.376777	1026.216214	16.334464
27.696628	1032.225283	16.339482
28.025262	1032.637611	16.344499
27.349594	1026.901854	16.349517
27.726383	1025.466763	16.354535
27.782908	1032.160888	16.359552
27.420762	1034.133148	16.364570
27.942280	1024.498511	16.369587
27.770104	1021.612521	16.374605
27.614990	1008.110663	16.379623
27.972930	1006.760579	16.384640
27.618717	999.065165	16.389658
27.895852	997.964432	16.394675
27.629344	1000.155239	16.399693
27.986739	1022.120814	16.404711
27.912630	1022.930765	16.409728
27.870579	1021.602323	16.414746
28.039709	1012.319557	16.419763
27.487383	1016.578060	16.424781
28.369325	1024.932236	16.429799
28.307171	1022.776950	16.434816
27.924959	1025.768544	16.439834
28.273550	1001.227427	16.444851
28.118026	997.306862	16.449869
27.740968	998.113784	16.454887
28.373013	1014.062259	16.459904
28.230239	1016.700750	16.464922
28.361956	1004.877061	16.469939
28.096065	1014.809123	16.474957
28.183689	1017.862805	16.479975
28.380723	1022.445724	16.484992
28.343229	1022.262150	16.490010
28.349368	1016.454288	16.495027
28.032073	1033.018589	16.500045
27.787290	1032.365709	16.505063
28.123157	1019.168778	16.510080
27.912218	1030.117897	16.515098
28.118807	1015.161310	16.520115
28.258103	1018.314197	16.525133
28.255573	1011.892299	16.530151
28.425250	1030.368499	16.535168
28.317088	1053.546326	16.540186
28.541897	1047.461190	16.545203
28.910595	1052.809346	16.550221
28.686958	1055.384771	16.555239
28.901370	1046.158010	16.560256
28.689212	1042.019085	16.565274
28.570887	1039.998832	16.570291
28.673010	1047.825089	16.575309
28.497009	1041.045343	16.580327
28.944393	1039.697022	16.585344
29.136915	1045.183235	16.590362
29.288440	1042.899790	16.595379
29.163761	1037.771995	16.600397
29.139073	1042.111941	16.605415
28.785810	1026.526677	16.610432
28.770237	1050.892382	16.615450
28.996744	1050.175128	16.620467
28.982013	1040.798074	16.625485
29.341281	1050.262970	16.630503
29.176153	1042.679926	16.635520
29.161355	1046.260913	16.640538
29.454617	1034.497102	16.645555
29.015182	1042.932082	16.650573
29.043537	1048.260975	16.655591
29.211811	1037.056401	16.660608
28.691734	1042.209281	16.665626
29.196116	1037.147032	16.670643
29.025374	1040.793477	16.675661
28.985352	1034.765618	16.680679
29.454794	1036.108959	16.685696
29.073353	1045.888725	16.690714
29.497396	1033.305988	16.695731
29.319281	1035.028503	16.700749
29.339439	1048.201032	16.705767
29.491045	1059.008158	16.710784
29.567487	1056.644955	16.715802
29.798489	1052.281957	16.720819
29.623340	1058.756763	16.725837
29.560679	1058.681276	16.730855
29.726599	1059.027578	16.735872
29.607613	1064.098688	16.740890
29.920603	1060.328772	16.745907
29.970873	1061.579996	16.750925
29.737982	1065.349795	16.755943
29.843590	1055.092323	16.760960
29.576849	1063.727479	16.765978
29.781624	1060.312197	16.770995
29.603807	1063.574738	16.776013
29.942940	1056.032605	16.781031
30.214600	1051.568561	16.786048
29.781324	1066.276474	16.791066
29.900098	1057.471799	16.796083
30.035379	1061.389045	16.801101
29.875259	1057.469187	16.806119
29.727318	1049.495275	16.811136
29.917814	1065.232104	16.816154
29.983274	1073.505940	16.821171
30.336985	1080.623747	16.826189
30.417633	1085.663585	16.831207
30.601824	1078.963093	16.836224
30.338952	1067.033923	16.841242
30.411842	1052.540077	16.846259
30.270050	1044.663035	16.851277
29.843103	1053.976553	16.856295
30.445838	1055.040230	16.861312
30.139399	1070.829676	16.866330
30.108940	1068.757782	16.871347
30.141076	1071.441462	16.876365
30.118870	1072.953357	16.881383
30.597388	1077.949791	16.886400
30.271108	1070.373049	16.891418
30.657827	1074.736909	16.896435
30.804706	1075.124065	16.901453
30.440180	1077.784685	16.906471
30.934192	1070.174099	16.911488
30.488367	1076.849114	16.916506
30.453768	1083.910994	16.921523
30.860443	1085.554515	16.926541
30.800501	1098.846931	16.931559
31.131740	1094.701753	16.936576
31.153562	1089.374260	16.941594
30.962026	1076.685963	16.946611
30.748716	1075.914538	16.951629
30.398468	1079.084174	16.956647
30.627565	1090.074842	16.961664
30.918182	1103.268155	16.966682
30.930595	1103.079917	16.971699
31.089101	1093.249648	16.976717
30.991779	1098.591936	16.981735
31.074089	1095.394655	16.986752
31.268612	1099.233198	16.991770
30.727918	1090.468713	16.996787
31.179807	1091.234126	17.001805
31.213396	1094.217391	17.006823
31.206868	1093.012770	17.011840
31.522880	1109.490541	17.016858
31.232416	1109.785269	17.021875
31.316906	1104.362744	17.026893
31.409298	1110.495842	17.031911
31.599834	1108.417722	17.036928
31.482851	1111.405646	17.041946
31.531511	1115.450087	17.046963
31.844041	1112.604908	17.051981
31.769297	1111.688691	17.056999
31.971186	1106.995717	17.062016
32.070506	1091.579334	17.067034
31.833437	1086.387081	17.072051
31.753962	1078.048969	17.077069
31.452762	1077.158768	17.082087
31.800208	1080.995438	17.087104
31.554664	1080.573055	17.092122
31.555926	1095.632642	17.097139
31.986450	1100.876449	17.102157
32.267244	1106.150029	17.107175
32.262665	1099.122490	17.112192
31.890830	1097.160886	17.117210
31.882509	1076.885537	17.122227
31.851960	1083.328229	17.127245
32.213097	1113.217756	17.132263
32.225384	1105.373353	17.137280
32.155109	1105.134952	17.142298
31.803878	1108.557218	17.147315
32.494896	1103.834948	17.152333
32.386009	1108.153387	17.157351
32.560554	1100.229914	17.162368
32.537667	1093.700720	17.167386
32.422786	1080.299803	17.172403
32.261466	1075.783668	17.177421
32.009113	1075.084633	17.182439
32.176711	1083.405589	17.187456
32.306891	1092.186858	17.192474
32.229523	1107.416569	17.197491
32.503684	1103.302424	17.202509
32.568555	1104.633416	17.207527
32.026969	1092.728962	17.212544
32.569845	1105.163211	17.217562
32.292781	1097.676579	17.222579
32.587261	1089.257781	17.227597
32.571851	1101.968852	17.232615
32.510377	1095.884371	17.237632
32.677388	1100.680302	17.242650
32.110787	1108.668166	17.247667
32.698399	1120.113935	17.252685
32.498959	1125.153485	17.257703
32.898285	1133.595953	17.262720
33.212351	1128.538249	17.267738
32.969313	1125.877945	17.272755
33.139635	1130.461921	17.277773
32.947383	1141.001070	17.282791
32.978602	1131.626236	17.287808
32.872689	1129.998515	17.292826
32.947070	1135.392809	17.297843
33.037514	1127.255276	17.302861
32.889845	1126.211625	17.307879
32.997005	1125.036528	17.312896
33.075706	1125.210299	17.317914
32.933097	1126.870454	17.322931
33.224202	1131.615393	17.327949
33.362043	1154.142564	17.332967
33.320646	1143.169595	17.337984
33.535833	1156.125449	17.343002
33.007603	1148.921151	17.348019
33.230063	1152.247230	17.353037
33.528920	1160.724386	17.358055
33.636701	1149.118953	17.363072
33.991719	1147.223347	17.368090
33.553166	1151.520862	17.373107
33.780662	1141.569301	17.378125
33.544969	1141.744993	17.383143
33.663618	1138.324254	17.388160
33.693374	1132.089764	17.393178
33.739175	1151.683749	17.398195
33.947483	1143.562457	17.403213
33.731634	1144.441960	17.408231
33.948338	1141.542360	17.413248
33.940040	1139.817290	17.418266
33.850318	1145.344598	17.423283
33.848879	1140.159594	17.428301
34.012462	1144.331208	17.433319
33.844014	1144.022979	17.438336
33.834020	1140.773878	17.443354
33.872229	1146.486276	17.448371
34.125592	1139.516140	17.453389
34.201792	1145.762244	17.458407
34.153104	1145.094415	17.463424
34.309383	1138.868502	17.468442
34.195698	1143.165610	17.473459
34.784802	1146.724585	17.478477
34.297589	1137.841241	17.483495
34.373465	1136.185037	17.488512
34.275724	1146.636796	17.493530
34.184201	1150.636935	17.498547
34.632437	1147.398092	17.503565
34.461045	1167.082930	17.508583
34.315260	1164.192781	17.513600
34.287643	1157.717955	17.518618
34.033958	1170.150817	17.523635
34.431926	1163.574594	17.528653
34.721822	1168.603763	17.533671
34.352425	1163.252333	17.538688
34.876571	1162.718823	17.543706
34.783834	1175.344228	17.548723
34.641136	1166.921303	17.553741
34.575993	1160.051557	17.558759
34.615344	1163.482068	17.563776
35.170495	1161.425713	17.568794
34.502065	1165.099665	17.573811
35.334648	1169.649320	17.578829
34.947563	1175.090680	17.583847
34.869800	1169.737739	17.588864
35.143103	1183.804852	17.593882
34.945137	1186.960115	17.598899
34.887685	1177.744322	17.603917
34.963604	1175.576852	17.608935
35.303042	1177.489700	17.613952
35.354961	1177.156412	17.618970
34.851176	1184.313932	17.623987
35.634413	1183.045530	17.629005
35.536745	1184.799638	17.634023
35.131461	1192.014315	17.639040
35.477385	1176.682302	17.644058
35.259429	1178.780313	17.649075
35.653700	1173.618510	17.654093
35.308391	1185.488208	17.659111
35.257945	1181.497489	17.664128
35.633361	1179.421953	17.669146
35.416161	1183.855214	17.674163
35.733803	1176.142824	17.679181
35.654465	1184.410995	17.684199
35.406668	1172.880192	17.689216
35.937831	1181.617616	17.694234
35.876477	1191.107462	17.699251
36.467388	1183.797237	17.704269
35.846199	1180.609173	17.709287
35.675231	1177.855516	17.714304
35.504377	1179.576907	17.719322
35.493200	1199.211431	17.724339
35.483660	1197.189895	17.729357
35.633706	1205.570465	17.734375
35.925382	1203.624815	17.739392
36.004879	1198.149394	17.744410
35.789989	1198.388100	17.749427
36.391942	1207.679353	17.754445
36.021555	1209.002806	17.759463
35.854621	1222.545614	17.764480
36.339789	1215.340309	17.769498
36.411642	1221.091642	17.774515
36.598878	1212.373999	17.779533
36.389709	1207.581294	17.784551
36.592357	1215.060505	17.789568
36.608912	1219.412968	17.794586
36.521808	1219.060433	17.799603
36.302182	1208.894858	17.804621
36.492139	1211.190903	17.809639
36.708514	1218.999334	17.814656
36.887148	1217.440636	17.819674
36.965325	1226.788715	17.824691
36.687213	1213.047188	17.829709
36.987814	1217.194195	17.834727
36.660570	1218.788609	17.839744
37.087504	1214.991341	17.844762
36.931410	1216.044527	17.849779
36.850627	1218.225196	17.854797
36.869501	1209.177315	17.859815
36.759405	1214.840384	17.864832
37.029540	1211.310688	17.869850
36.585827	1221.425364	17.874867
36.804781	1217.237789	17.879885
37.069972	1218.038771	17.884903
36.459960	1222.842864	17.889920
37.016679	1229.846871	17.894938
37.224476	1234.721658	17.899955
36.910157	1239.107030	17.904973
37.601225	1236.887356	17.909991
37.508784	1241.651389	17.915008
37.692221	1236.898154	17.920026
37.778854	1234.463902	17.925043
37.648407	1217.136213	17.930061
37.529355	1207.156859	17.935079
37.120432	1213.731465	17.940096
37.414192	1222.370402	17.945114
37.412667	1223.127963	17.950131
37.678422	1234.131912	17.955149
37.678363	1236.445107	17.960167
37.682961	1235.642690	17.965184
37.539121	1235.911291	17.970202
37.787741	1236.301447	17.975219
37.804814	1230.640129	17.980237
37.580527	1235.349076	17.985255
37.491612	1239.260461	17.990272
37.696838	1231.325811	17.995290
37.574915	1226.232245	18.000307
37.676396	1241.976865	18.005325
37.729709	1247.191451	18.010343
37.690010	1256.545390	18.015360
37.811884	1260.572082	18.020378
38.090852	1260.966951	18.025395
37.662105	1252.472034	18.030413
38.049348	1244.278479	18.035431
38.344190	1261.655988	18.040448
38.654720	1255.781421	18.045466
38.069552	1258.975271	18.050483
38.499722	1258.759450	18.055501
38.674821	1259.997442	18.060519
38.476346	1260.530232	18.065536
38.601354	1247.391417	18.070554
38.496875	1258.276657	18.075571
38.433143	1257.131482	18.080589
38.813665	1273.709755	18.085607
38.829988	1275.534378	18.090624
38.941207	1265.392676	18.095642
38.847504	1265.198971	18.100659
38.439677	1252.692764	18.105677
38.783766	1263.056431	18.110695
38.827788	1275.953981	18.115712
39.210087	1273.164119	18.120730
38.977971	1268.734768	18.125747
39.239990	1265.200021	18.130765
39.249107	1253.651005	18.135783
38.695421	1257.998142	18.140800
39.099107	1245.989666	18.145818
38.795224	1263.694520	18.150835
38.585852	1268.707263	18.155853
39.017831	1276.844871	18.160871
38.930582	1279.985960	18.165888
38.919861	1272.205051	18.170906
38.965775	1280.037061	18.175923
39.069635	1279.484186	18.180941
39.346722	1284.499615	18.185959
39.518167	1301.811286	18.190976
39.533524	1297.658747	18.195994
39.445414	1294.614368	18.201011
39.814559	1292.060103	18.206029
40.051071	1289.097413	18.211047
39.833161	1286.392120	18.216064
39.668723	1279.761955	18.221082
39.406585	1267.195041	18.226099
39.686210	1274.829480	18.231117
39.791856	1267.071368	18.236135
39.274015	1270.257827	18.241152
39.693254	1288.916110	18.246170
40.048983	1292.249738	18.251187
40.115010	1296.831162	18.256205
39.890143	1297.778359	18.261223
39.779450	1299.932165	18.266240
39.667410	1303.922929	18.271258
40.187094	1293.322724	18.276275
40.303569	1294.472070	18.281293
40.326104	1285.581373	18.286311
39.911150	1294.590168	18.291328
40.209786	1294.981956	18.296346
40.188057	1295.537551	18.301363
40.089349	1296.162013	18.306381
40.236238	1287.993472	18.311399
40.028654	1299.687027	18.316416
39.935548	1294.238619	18.321434
40.326818	1295.098749	18.326451
40.363410	1308.748596	18.331469
40.825259	1312.299140	18.336487
40.120590	1317.234857	18.341504
40.627264	1315.773083	18.346522
40.769277	1316.501847	18.351539
40.467281	1315.678031	18.356557
41.088402	1310.389126	18.361575
40.755907	1321.190203	18.366592
40.678101	1321.473707	18.371610
40.777600	1310.623733	18.376627
40.576095	1309.730522	18.381645
40.915982	1316.108948	18.386663
40.606786	1314.724506	18.391680
40.637242	1311.579493	18.396698
41.532905	1327.884596	18.401715
41.233697	1328.963367	18.406733
40.987589	1310.407118	18.411751
40.971002	1316.282796	18.416768
41.454574	1332.601973	18.421786
41.696179	1331.427889	18.426803
41.269574	1344.923108	18.431821
41.161248	1330.583665	18.436839
41.554425	1335.757652	18.441856
41.401385	1339.243588	18.446874
41.803778	1338.170550	18.451891
41.460679	1338.757561	18.456909
41.467806	1335.890765	18.461927
41.732591	1343.287709	18.466944
41.506436	1330.349024	18.471962
41.577945	1335.295687	18.476979
41.259055	1337.052910	18.481997
41.897132	1330.984984	18.487015
41.925877	1333.615584	18.492032
41.721446	1329.595307	18.497050
41.666885	1328.486561	18.502067
41.671901	1335.185713	18.507085
41.763669	1327.827396	18.512103
41.731419	1329.975228	18.517120
41.671436	1336.933883	18.522138
41.946334	1346.973911	18.527155
41.740998	1363.360024	18.532173
42.101216	1350.026485	18.537191
42.216419	1362.486894	18.542208
42.123088	1356.202180	18.547226
42.194366	1355.840609	18.552243
42.047557	1354.986165	18.557261
42.333359	1351.128926	18.562279
41.840529	1353.866495	18.567296
42.340052	1359.235274	18.572314
42.113122	1369.006787	18.577331
42.100788	1379.839792	18.582349
42.594360	1378.515771	18.587367
42.700539	1382.519702	18.592384
42.493248	1372.247954	18.597402
43.019730	1375.640055	18.602419
42.298177	1385.047241	18.607437
42.785773	1370.668051	18.612455
42.909712	1371.854103	18.617472
43.035344	1374.570520	18.622490
43.032779	1371.424359	18.627507
42.772161	1374.188667	18.632525
42.814329	1377.972243	18.637543
43.115811	1374.390264	18.642560
42.990300	1370.480694	18.647578
43.256962	1368.785110	18.652595
43.067474	1376.982261	18.657613
43.167703	1380.703090	18.662631
43.511604	1379.705488	18.667648
43.162305	1390.761715	18.672666
43.580457	1383.184974	18.677683
43.636193	1392.962708	18.682701
43.480223	1383.497145	18.687719
43.320121	1371.393873	18.692736
43.435163	1383.109521	18.697754
43.714988	1390.141194	18.702771
43.809996	1399.818101	18.707789
43.587126	1390.350392	18.712807
43.513442	1395.427121	18.717824
43.738769	1401.593143	18.722842
43.967193	1391.306769	18.727859
43.805376	1399.733135	18.732877
43.924671	1395.034091	18.737895
43.922728	1394.276874	18.742912
43.726407	1396.687115	18.747930
44.087776	1397.305772	18.752947
44.157613	1403.461441	18.757965
44.259083	1398.288641	18.762983
43.884527	1400.865669	18.768000
44.049715	1391.801083	18.773018
43.934836	1392.273441	18.778035
43.883674	1385.436133	18.783053
43.949799	1392.602279	18.788071
44.345693	1395.345785	18.793088
44.433263	1417.761240	18.798106
44.321236	1413.600228	18.803123
44.366026	1418.125048	18.808141
44.209223	1405.835035	18.813159
44.383472	1406.647119	18.818176
44.391207	1412.395936	18.823194
44.828246	1415.357071	18.828211
44.525601	1416.673081	18.833229
44.206922	1416.716603	18.838247
44.422393	1409.679713	18.843264
44.362470	1420.791610	18.848282
44.882348	1433.554756	18.853299
44.751209	1440.041739	18.858317
44.863025	1439.187799	18.863335
45.391149	1434.819184	18.868352
44.982990	1441.971292	18.873370
45.379737	1433.394293	18.878387
45.147094	1438.767351	18.883405
45.131943	1433.006872	18.888423
45.445314	1433.014486	18.893440
45.309584	1432.013129	18.898458
45.201729	1432.970403	18.903475
45.213358	1427.726461	18.908493
45.399489	1428.287364	18.913511
45.482175	1430.335146	18.918528
45.416995	1437.638652	18.923546
45.664643	1436.359469	18.928563
45.418700	1433.705885	18.933581
45.125566	1431.173308	18.938599
45.543920	1429.400301	18.943616
45.173471	1433.374773	18.948634
45.399752	1447.256949	18.953651
45.845960	1459.883326	18.958669
45.706136	1455.739284	18.963687
45.848593	1460.078391	18.968704
45.725842	1455.773876	18.973722
45.988230	1457.077105	18.978739
46.004549	1458.482006	18.983757
45.603825	1448.410941	18.988775
45.943236	1445.286931	18.993792
46.045010	1455.540346	18.998810
46.222183	1452.003076	19.003827
46.284273	1458.693333	19.008845
46.210657	1465.556339	19.013863
46.474504	1471.422846	19.018880
46.656556	1482.282265	19.023898
46.561765	1466.302653	19.028915
46.716300	1460.805927	19.033933
46.709238	1454.469790	19.038951
46.284187	1449.231140	19.043968
46.368138	1457.940934	19.048986
46.651268	1466.493288	19.054003
46.772182	1467.108594	19.059021
46.844152	1470.925392	19.064039
46.963642	1470.969694	19.069056
46.958642	1479.103271	19.074074
47.129378	1467.497236	19.079091
47.032493	1474.941431	19.084109
46.726364	1461.204101	19.089127
46.795236	1465.444281	19.094144
46.692629	1468.303773	19.099162
46.941743	1467.728135	19.104179
46.844365	1465.471011	19.109197
46.568277	1473.729114	19.114215
47.048171	1485.037355	19.119232
46.991874	1501.504390	19.124250
47.313313	1495.214606	19.129267
47.500633	1500.029555	19.134285
47.300313	1502.522491	19.139303
47.823729	1489.844967	19.144320
47.605548	1493.647266	19.149338
47.720622	1488.630107	19.154355
47.747791	1491.207326	19.159373
47.730636	1481.117175	19.164391
48.063438	1483.097371	19.169408
47.723834	1492.059744	19.174426
47.373740	1482.248984	19.179443
47.430456	1483.442421	19.184461
47.352473	1493.481012	19.189479
47.850699	1504.464486	19.194496
47.857375	1513.827074	19.199514
48.037743	1501.553600	19.204531
47.922884	1515.662855	19.209549
47.987963	1511.887503	19.214567
48.277607	1509.127903	19.219584
48.329189	1498.787119	19.224602
48.133394	1502.062023	19.229619
48.107400	1502.596201	19.234637
48.144323	1508.536145	19.239655
48.587302	1500.488384	19.244672
48.300692	1515.464033	19.249690
48.753604	1523.888823	19.254707
48.391018	1527.300323	19.259725
48.385002	1537.895737	19.264743
48.617612	1520.744413	19.269760
48.654190	1529.726765	19.274778
48.693453	1533.551856	19.279795
48.724012	1534.263376	19.284813
48.305095	1533.634602	19.289831
48.362308	1532.337910	19.294848
48.611695	1541.482596	19.299866
48.865341	1547.666323	19.304883
49.086607	1554.486318	19.309901
48.805564	1556.190294	19.314919
49.232442	1553.200891	19.319936
49.133072	1568.178808	19.324954
49.400497	1562.623336	19.329971
49.059130	1557.153780	19.334989
49.125850	1560.356006	19.340007
49.361114	1555.638751	19.345024
49.212432	1563.649704	19.350042
49.254587	1559.552869	19.355059
49.286900	1561.034171	19.360077
49.350684	1578.445033	19.365095
49.601046	1583.076549	19.370112
49.268557	1585.927893	19.375130
49.670054	1587.319796	19.380147
49.846252	1583.176707	19.385165
49.850650	1588.332781	19.390183
49.867034	1579.777434	19.395200
50.039553	1576.793164	19.400218
49.740012	1581.075312	19.405235
50.097871	1582.111115	19.410253
49.929660	1581.297885	19.415271
50.278752	1571.226044	19.420288
50.029128	1585.539515	19.425306
50.076411	1597.265919	19.430323
50.468354	1598.959138	19.435341
50.829951	1607.483486	19.440359
50.793316	1604.503577	19.445376
50.534192	1589.509018	19.450394
50.571776	1580.448549	19.455411
50.606993	1577.403736	19.460429
50.180961	1575.819816	19.465447
50.647097	1580.676315	19.470464
50.766843	1594.319663	19.475482
50.781403	1605.656703	19.480499
51.039562	1591.278568	19.485517
50.527753	1591.743689	19.490535
51.134215	1587.624710	19.495552
51.252198	1592.396896	19.500570
51.055436	1591.187330	19.505587
51.382706	1582.867312	19.510605
51.265148	1593.606474	19.515623
50.969261	1596.777150	19.520640
51.070095	1596.518246	19.525658
50.947227	1591.585677	19.530675
50.977080	1588.368124	19.535693
50.547564	1591.398781	19.540711
51.214440	1590.852366	19.545728
51.266697	1608.662717	19.550746
51.286455	1613.664904	19.555763
51.171507	1609.138211	19.560781
51.297654	1614.682339	19.565799
51.354667	1617.636773	19.570816
51.363979	1619.377318	19.575834
51.700014	1617.894916	19.580851
51.694105	1622.077417	19.585869
52.094142	1639.438812	19.590887
52.144841	1639.418150	19.595904
52.130935	1626.461776	19.600922
51.669875	1623.321130	19.605939
52.221394	1622.218400	19.610957
52.392757	1635.017358	19.615975
52.225959	1624.322531	19.620992
51.767986	1625.694451	19.626010
52.189296	1637.273914	19.631027
52.332965	1642.619634	19.636045
52.148246	1641.474454	19.641063
51.948593	1643.907341	19.646080
52.164033	1640.155744	19.651098
52.033345	1639.320853	19.656115
52.434424	1639.210578	19.661133
52.019416	1650.839024	19.666151
52.352645	1654.971555	19.671168
52.541131	1660.884648	19.676186
52.806045	1663.566662	19.681203
53.029691	1659.864271	19.686221
52.701847	1653.199605	19.691239
52.927377	1660.479747	19.696256
52.758845	1662.655282	19.701274
52.700202	1664.788352	19.706291
53.030788	1667.797769	19.711309
52.919183	1683.516200	19.716327
53.339006	1681.616698	19.721344
53.487788	1685.715014	19.726362
52.883202	1680.842114	19.731379
53.460020	1683.655156	19.736397
53.284506	1687.611766	19.741415
53.331886	1675.204366	19.746432
53.339636	1677.503771	19.751450
53.545865	1679.996155	19.756467
53.537578	1682.307542	19.761485
53.296010	1677.295711	19.766503
53.475994	1674.777342	19.771520
53.664953	1701.548311	19.776538
53.994344	1704.813556	19.781555
54.212545	1696.188663	19.786573
53.739284	1708.675234	19.791591
53.937899	1707.372155	19.796608
54.228351	1708.784622	19.801626
54.021163	1709.397690	19.806643
54.326419	1698.518400	19.811661
53.771921	1708.461346	19.816679
53.788931	1709.342263	19.821696
53.969360	1704.226437	19.826714
54.213632	1716.774175	19.831731
54.597082	1720.936725	19.836749
54.539357	1722.728811	19.841767
54.649287	1722.238092	19.846784
55.208759	1717.217520	19.851802
54.611865	1713.836192	19.856819
54.723981	1716.668394	19.861837
54.814127	1719.194751	19.866855
54.847927	1724.756537	19.871872
55.008608	1715.105479	19.876890
54.726512	1719.110354	19.881907
55.279236	1715.189126	19.886925
54.952969	1720.324457	19.891943
54.919326	1714.137569	19.896960
55.062450	1716.087546	19.901978
54.961110	1726.448683	19.906995
55.331414	1710.736832	19.912013
55.473081	1717.310569	19.917031
55.118705	1716.674832	19.922048
55.214621	1716.637617	19.927066
55.431251	1714.362824	19.932083
55.847718	1713.416956	19.937101
55.348080	1713.028053	19.942119
55.423886	1713.451608	19.947136
55.708289	1710.509750	19.952154
55.503067	1720.653616	19.957171
55.877041	1709.785645	19.962189
55.615916	1718.445483	19.967207
55.476289	1738.476286	19.972224
55.814904	1741.468678	19.977242
55.705969	1754.406316	19.982259
55.729371	1758.748369	19.987277
56.081673	1743.345442	19.992295
55.700660	1737.200346	19.997312
55.627864	1748.399675	20.002330
56.228100	1757.833507	20.007347
56.369985	1758.843195	20.012365
56.541068	1771.781158	20.017383
56.115701	1768.199365	20.022400
56.385422	1761.706139	20.027418
56.344690	1764.994669	20.032435
56.381699	1765.635755	20.037453
56.454122	1760.429531	20.042471
56.474119	1769.231553	20.047488
56.760924	1770.464704	20.052506
56.515352	1792.049140	20.057523
56.667359	1789.917015	20.062541
56.702656	1787.995692	20.067559
56.532907	1790.676395	20.072576
57.129013	1790.848009	20.077594
56.583455	1787.382879	20.082611
56.730573	1797.806122	20.087629
57.239021	1813.834646	20.092647
57.483286	1804.388210	20.097664
57.748272	1801.597712	20.102682
57.584648	1811.690928	20.107699
57.914373	1804.254106	20.112717
57.665638	1808.222214	20.117735
57.273486	1810.666347	20.122752
57.664518	1810.365130	20.127770
57.673907	1801.264783	20.132787
58.041522	1799.064161	20.137805
57.715125	1804.878078	20.142823
57.705773	1805.043560	20.147840
57.877423	1799.108519	20.152858
57.574114	1804.278149	20.157875
57.574518	1801.604849	20.162893
57.987243	1807.082044	20.167911
58.166825	1819.485345	20.172928
58.399204	1822.914145	20.177946
58.304752	1826.548796	20.182963
58.560308	1825.732281	20.187981
58.482324	1824.649266	20.192999
57.915350	1827.884547	20.198016
58.587268	1825.001886	20.203034
58.742189	1833.931134	20.208051
59.127207	1831.983418	20.213069
58.939443	1832.426178	20.218087
58.798376	1835.452711	20.223104
58.790117	1823.385307	20.228122
58.665198	1830.240710	20.233139
58.840400	1825.113045	20.238157
58.816623	1816.721678	20.243175
58.735103	1820.572066	20.248192
58.808327	1821.248509	20.253210
58.598785	1821.641029	20.258227
59.178904	1827.720051	20.263245
59.436867	1831.283709	20.268263
59.069213	1844.577549	20.273280
59.613908	1844.769843	20.278298
59.796872	1853.618962	20.283315
59.147063	1833.342268	20.288333
59.707870	1840.427934	20.293351
59.713362	1847.884648	20.298368
59.735370	1838.984290	20.303386
59.656438	1848.773904	20.308403
59.671187	1844.984275	20.313421
60.007402	1844.669554	20.318439
59.794920	1839.182874	20.323456
59.706446	1833.427442	20.328474
60.033634	1837.699826	20.333491
59.703049	1840.124849	20.338509
59.668581	1843.283015	20.343527
59.730372	1843.740329	20.348544
59.850542	1845.005904	20.353562
60.047362	1869.109057	20.358579
60.060706	1867.702441	20.363597
60.332175	1862.212520	20.368615
59.908434	1873.744641	20.373632
60.248220	1861.584810	20.378650
60.440235	1874.778362	20.383667
60.335189	1883.353861	20.388685
60.811850	1883.455823	20.393703
60.703062	1896.952157	20.398720
60.695381	1889.287277	20.403738
60.528522	1884.468825	20.408755
60.846158	1884.333751	20.413773
60.858744	1876.321694	20.418791
60.687286	1895.451881	20.423808
61.099227	1902.939619	20.428826
61.198367	1908.216650	20.433843
61.186342	1910.736949	20.438861
61.648610	1906.924534	20.443879
61.534953	1906.427812	20.448896
61.697616	1910.994254	20.453914
61.703696	1906.587389	20.458931
61.610297	1901.489160	20.463949
61.656984	1900.730615	20.468967
61.499358	1906.518123	20.473984
61.725130	1898.371662	20.479002
61.647972	1905.465782	20.484019
61.468175	1906.428040	20.489037
61.935240	1909.482392	20.494055
61.705034	1925.759297	20.499072
62.082297	1926.937259	20.504090
62.452791	1923.909290	20.509107
62.121407	1925.788456	20.514125
61.943530	1923.338744	20.519143
62.098253	1924.759870	20.524160
62.403291	1924.816131	20.529178
62.240567	1922.199932	20.534195
62.233595	1925.729372	20.539213
62.662800	1935.246903	20.544231
62.619687	1926.836421	20.549248
62.711018	1935.336994	20.554266
62.854257	1942.412378	20.559283
62.583365	1947.927289	20.564301
62.854170	1954.247335	20.569319
62.922213	1957.165381	20.574336
62.550357	1945.931246	20.579354
62.870562	1954.986148	20.584371
62.684285	1953.945340	20.589389
62.731450	1953.514946	20.594407
62.988322	1966.752057	20.599424
63.427488	1965.973047	20.604442
63.518932	1963.345424	20.609459
63.170769	1973.552855	20.614477
63.942699	1970.338900	20.619495
63.348074	1967.493692	20.624512
63.569194	1978.489314	20.629530
63.469628	1970.330672	20.634547
63.582245	1974.949156	20.639565
63.818448	1967.536388	20.644583
63.329375	1966.495678	20.649600
63.950909	1957.750659	20.654618
63.965364	1967.377372	20.659635
63.847809	1975.102744	20.664653
64.166885	1984.069469	20.669671
64.076997	1991.825229	20.674688
64.086311	1986.938119	20.679706
64.586895	1993.294768	20.684723
64.716121	1983.295017	20.689741
65.050384	1979.205974	20.694759
64.746883	1991.148553	20.699776
64.983865	1979.187800	20.704794
64.878986	1964.553797	20.709811
64.666817	1959.284797	20.714829
64.468074	1957.090832	20.719847
64.223693	1970.075096	20.724864
64.356393	1970.657013	20.729882
64.211807	1982.849264	20.734899
64.471203	1991.042644	20.739917
64.931081	1989.247298	20.744935
65.026820	2009.456139	20.749952
64.795620	2012.749307	20.754970
65.319394	2015.056278	20.759987
65.035375	2014.968126	20.765005
64.843897	2010.428073	20.770023
65.074902	2030.088685	20.775040
65.200713	2031.621655	20.780058
65.596561	2032.623129	20.785075
65.339467	2029.986982	20.790093
65.533113	2027.958767	20.795111
65.687890	2041.035191	20.800128
65.735591	2050.435816	20.805146
66.119775	2051.682135	20.810163
65.955273	2057.959957	20.815181
66.345988	2044.220308	20.820199
66.155339	2055.763367	20.825216
66.198113	2049.794782	20.830234
66.676909	2053.137679	20.835251
66.359709	2057.201781	20.840269
66.534830	2047.119060	20.845287
66.433609	2058.300943	20.850304
66.344563	2051.971128	20.855322
66.446888	2035.922252	20.860339
66.335366	2049.321292	20.865357
66.374367	2047.692874	20.870375
66.593570	2044.786426	20.875392
66.884698	2065.624334	20.880410
66.777810	2067.616676	20.885427
66.656764	2073.982377	20.890445
67.274490	2065.181094	20.895463
67.156814	2068.014637	20.900480
67.131498	2064.622590	20.905498
67.278283	2064.612122	20.910515
67.164009	2074.536794	20.915533
67.149109	2068.482557	20.920551
67.234253	2073.329451	20.925568
67.278533	2076.320673	20.930586
67.764388	2082.010576	20.935603
67.856537	2098.928311	20.940621
68.037740	2091.006515	20.945639
67.815892	2086.704749	20.950656
67.923110	2091.011658	20.955674
67.796797	2082.046048	20.960691
67.922084	2093.823678	20.965709
68.239672	2088.679942	20.970727
68.209842	2091.108375	20.975744
67.833383	2093.976154	20.980762
68.016353	2092.353581	20.985779
67.816439	2091.428520	20.990797
68.267246	2093.895268	20.995815
68.330640	2089.656118	21.000832
68.158082	2090.449980	21.005850
68.460822	2098.756549	21.010867
68.495174	2110.488471	21.015885
68.820873	2110.929693	21.020903
68.854705	2122.204076	21.025920
68.595338	2112.776418	21.030938
69.085927	2120.122527	21.035955
68.749953	2118.972608	21.040973
69.109554	2114.885876	21.045991
69.255790	2118.328229	21.051008
68.761237	2119.882655	21.056026
69.177058	2117.721784	21.061043
69.200007	2131.737342	21.066061
69.252626	2132.161384	21.071079
69.805215	2132.870042	21.076096
69.629987	2131.947423	21.081114
69.754053	2138.047507	21.086131
69.636167	2143.434355	21.091149
69.605372	2138.600829	21.096167
69.644157	2134.412865	21.101184
69.784054	2146.046217	21.106202
69.641385	2143.281663	21.111219
69.719506	2138.020784	21.116237
70.171118	2150.002966	21.121255
70.157831	2157.611086	21.126272
70.062133	2164.796582	21.131290
70.270283	2154.503481	21.136307
69.984846	2166.856791	21.141325
69.820208	2165.061435	21.146343
70.140604	2159.652129	21.151360
69.883757	2176.605678	21.156378
70.297821	2177.964100	21.161395
70.782385	2179.412472	21.166413
70.599872	2179.803919	21.171431
70.610152	2183.030880	21.176448
70.715286	2193.006456	21.181466
70.986296	2190.388540	21.186483
70.939770	2199.488398	21.191501
70.921086	2196.726503	21.196519
71.204974	2199.137360	21.201536
71.321652	2205.904558	21.206554
71.251234	2204.214367	21.211571
71.358812	2202.461572	21.216589
71.182185	2208.182719	21.221607
71.680218	2206.425560	21.226624
71.740499	2216.322962	21.231642
71.999731	2213.536460	21.236659
71.615377	2222.130631	21.241677
71.633409	2224.390623	21.246695
72.043684	2216.019435	21.251712
72.332453	2211.022204	21.256730
72.234341	2214.054694	21.261747
72.347813	2217.830432	21.266765
72.150972	2218.230438	21.271783
72.421102	2213.315028	21.276800
71.860564	2217.919108	21.281818
72.229005	2218.823893	21.286835
72.502626	2215.050438	21.291853
72.052145	2205.400187	21.296871
72.057286	2214.845439	21.301888
72.340664	2235.167160	21.306906
72.536942	2236.225163	21.311923
72.649122	2243.867316	21.316941
72.657380	2236.174541	21.321959
72.655416	2242.086104	21.326976
72.587409	2254.812545	21.331994
72.998848	2261.217974	21.337011
72.687785	2260.897350	21.342029
72.832849	2262.840772	21.347047
73.152289	2258.712959	21.352064
73.521358	2289.578443	21.357082
73.492152	2285.413720	21.362099
73.611524	2285.300239	21.367117
73.694968	2289.276375	21.372135
73.578859	2288.325549	21.377152
73.786003	2293.734109	21.382170
73.870819	2285.562217	21.387187
73.921962	2284.449475	21.392205
73.501902	2284.925483	21.397223
73.859950	2286.526241	21.402240
73.861938	2303.773904	21.407258
74.270798	2299.950838	21.412275
74.253017	2310.346561	21.417293
74.260977	2308.382124	21.422311
74.251183	2306.865479	21.427328
74.111753	2310.655611	21.432346
74.129911	2303.472545	21.437363
74.503622	2318.430622	21.442381
74.534639	2325.719417	21.447399
74.824893	2333.150655	21.452416
74.681563	2340.037541	21.457434
74.740333	2333.933801	21.462451
74.761759	2330.689030	21.467469
74.921362	2347.811045	21.472487
75.159037	2346.675388	21.477504
75.260949	2366.732171	21.482522
75.504220	2354.404075	21.487539
75.575016	2350.971667	21.492557
75.482396	2356.698636	21.497575
75.868860	2344.872026	21.502592
75.844699	2349.429977	21.507610
76.229744	2349.208594	21.512627
76.025263	2347.350027	21.517645
76.135610	2342.844661	21.522663
76.047032	2345.616879	21.527680
75.517567	2341.495802	21.532698
75.793477	2338.712980	21.537715
75.791539	2345.426224	21.542733
75.654201	2354.865467	21.547751
76.071823	2358.539930	21.552768
76.076686	2365.974864	21.557786
76.122483	2362.729425	21.562803
76.162965	2387.002949	21.567821
76.287933	2394.299146	21.572839
76.728364	2391.692531	21.577856
76.711489	2397.925249	21.582874
76.910593	2395.050300	21.587891
77.379216	2398.271768	21.592909
76.879920	2399.435601	21.597927
77.170593	2402.618671	21.602944
76.859264	2399.820535	21.607962
76.790567	2395.968118	21.612979
77.267507	2412.911077	21.617997
77.573677	2424.221884	21.623015
77.586500	2420.012672	21.628032
77.552574	2425.500071	21.633050
77.529785	2421.113384	21.638067
77.501975	2415.010555	21.643085
77.577573	2428.696173	21.648103
77.646570	2423.518699	21.653120
77.700457	2418.630800	21.658138
77.811863	2416.924727	21.663155
77.827630	2432.907907	21.668173
77.703637	2438.955430	21.673191
78.177241	2433.503103	21.678208
78.370296	2446.791597	21.683226
77.965219	2443.361137	21.688243
78.046583	2442.950622	21.693261
78.369950	2462.411026	21.698279
78.995284	2461.558644	21.703296
78.899510	2467.604912	21.708314
79.121940	2461.052566	21.713331
79.150358	2464.990020	21.718349
79.037092	2464.972952	21.723367
79.322897	2456.946236	21.728384
79.388442	2463.377524	21.733402
79.223279	2455.134255	21.738419
79.100505	2448.481347	21.743437
79.115242	2459.257109	21.748455
79.242421	2460.853024	21.753472
79.270360	2459.118994	21.758490
79.159986	2467.215874	21.763507
79.562000	2469.412581	21.768525
79.682143	2468.620411	21.773543
79.541999	2473.404869	21.778560
79.750328	2480.946843	21.783578
79.618468	2485.837315	21.788595
80.033731	2486.337107	21.793613
79.850709	2493.287081	21.798631
79.981021	2483.700336	21.803648
80.117072	2497.269226	21.808666
79.841608	2508.245133	21.813683
80.164224	2507.837850	21.818701
80.371157	2516.462612	21.823719
79.940799	2513.560017	21.828736
80.411164	2525.927718	21.833754
80.442464	2532.651605	21.838771
80.758912	2534.959566	21.843789
80.629272	2538.189575	21.848807
81.299006	2529.146366	21.853824
81.069225	2522.721657	21.858842
81.161677	2525.149927	21.863859
81.328463	2539.462038	21.868877
81.379655	2546.167033	21.873895
81.688931	2547.216819	21.878912
81.824686	2551.759235	21.883930
81.868788	2548.485623	21.888947
81.833734	2548.532049	21.893965
81.978889	2554.799403	21.898983
81.677184	2543.213038	21.904000
81.746380	2550.467538	21.909018
81.621649	2557.345281	21.914035
81.919432	2542.685595	21.919053
81.971359	2549.844960	21.924071
82.154320	2546.559062	21.929088
82.273841	2558.344212	21.934106
82.423182	2568.212074	21.939123
82.466826	2562.861788	21.944141
82.255135	2569.210303	21.949159
82.211504	2563.750601	21.954176
82.614179	2575.327280	21.959194
82.518966	2562.502904	21.964211
82.829735	2569.123053	21.969229
82.999436	2590.435079	21.974247
82.968551	2588.555601	21.979264
82.769260	2591.480917	21.984282
83.035440	2595.993442	21.989299
83.237791	2594.762306	21.994317
83.276433	2600.058489	21.999335
83.332798	2597.272150	22.004352
83.318823	2600.054812	22.009370
83.128030	2603.515343	22.014387
83.455164	2613.535276	22.019405
83.647414	2618.611716	22.024423
83.704808	2622.961277	22.029440
83.996711	2616.861945	22.034458
83.797492	2629.691268	22.039475
84.029349	2620.116947	22.044493
83.910524	2628.432998	22.049511
84.332386	2645.043942	22.054528
84.600487	2644.433734	22.059546
84.598043	2645.746983	22.064563
84.571670	2635.272576	22.069581
84.648699	2646.316432	22.074599
84.975791	2641.461418	22.079616
84.730309	2634.360554	22.084634
84.511191	2643.800137	22.089651
84.932001	2640.710513	22.094669
84.588379	2648.171756	22.099687
84.696352	2642.009704	22.104704
85.373183	2647.237476	22.109722
85.199160	2658.626819	22.114739
85.286625	2665.048433	22.119757
85.218356	2657.979763	22.124775
85.431121	2655.165756	22.129792
85.795796	2654.035432	22.134810
85.222880	2668.135295	22.139827
85.544891	2669.170469	22.144845
85.598284	2681.521545	22.149863
85.530258	2679.954025	22.154880
86.052191	2677.293571	22.159898
86.234898	2683.716051	22.164915
86.472483	2687.706000	22.169933
86.014909	2695.380797	22.174951
86.306770	2705.620927	22.179968
86.379394	2700.250279	22.184986
86.109739	2703.439130	22.190003
86.481634	2698.132061	22.195021
86.539608	2704.959143	22.200039
86.849551	2720.511438	22.205056
87.072370	2729.234811	22.210074
87.126080	2731.120004	22.215091
87.143589	2726.518621	22.220109
87.246829	2728.329775	22.225127
87.152229	2726.460265	22.230144
87.533881	2713.188642	22.235162
87.552363	2719.684206	22.240179
87.516703	2723.505509	22.245197
87.787757	2714.862380	22.250215
87.689354	2722.736567	22.255232
87.673560	2714.832737	22.260250
87.815248	2732.532349	22.265267
88.060722	2729.725831	22.270285
88.055178	2746.432236	22.275303
87.556848	2745.392927	22.280320
88.227917	2745.915774	22.285338
87.950817	2744.321036	22.290355
88.050282	2748.765034	22.295373
88.327378	2768.873724	22.300391
88.427726	2769.413394	22.305408
88.809195	2770.622318	22.310426
88.410368	2778.379476	22.315443
88.656264	2772.164209	22.320461
88.771640	2777.069679	22.325479
88.477228	2773.965840	22.330496
88.844724	2793.927835	22.335514
88.663918	2796.645136	22.340531
89.043209	2797.507222	22.345549
89.120705	2800.995195	22.350567
89.204765	2798.409638	22.355584
89.596233	2811.907188	22.360602
89.515479	2822.963247	22.365619
89.614646	2819.668334	22.370637
89.919767	2823.281614	22.375655
89.650844	2832.479759	22.380672
89.999259	2827.968536	22.385690
90.001365	2822.103909	22.390707
90.174819	2810.054717	22.395725
90.331269	2814.054249	22.400743
90.150400	2823.948736	22.405760
90.316256	2839.069217	22.410778
90.145237	2838.669828	22.415795
90.608321	2835.504113	22.420813
91.125531	2840.393988	22.425831
91.014215	2836.892178	22.430848
90.694427	2838.353001	22.435866
91.015799	2835.764978	22.440883
91.193290	2842.368234	22.445901
91.110310	2841.841430	22.450919
91.124524	2849.817965	22.455936
90.867743	2856.962693	22.460954
90.669913	2871.701468	22.465971
91.512045	2862.571117	22.470989
91.332505	2868.094089	22.476007
91.268843	2886.656105	22.481024
91.870500	2880.650184	22.486042
91.799795	2879.304000	22.491059
91.602175	2882.503690	22.496077
91.867805	2880.445166	22.501095
91.813037	2888.060093	22.506112
91.727873	2902.162626	22.511130
91.704623	2911.735784	22.516147
92.272929	2910.005425	22.521165
92.534332	2915.333081	22.526183
92.559117	2928.891322	22.531200
92.798811	2930.176125	22.536218
92.860296	2931.479379	22.541235
93.159014	2928.670801	22.546253
92.922307	2921.956662	22.551271
92.788927	2925.379854	22.556288
93.087349	2929.148860	22.561306
93.348876	2924.821660	22.566323
93.535021	2937.852792	22.571341
93.606638	2947.969755	22.576359
93.563857	2946.148916	22.581376
93.693041	2947.387909	22.586394
93.694829	2943.871514	22.591411
93.608297	2956.434073	22.596429
94.045666	2939.293507	22.601447
93.793710	2946.188175	22.606464
93.931297	2947.940314	22.611482
94.103941	2955.049365	22.616499
94.340562	2962.268332	22.621517
94.632076	2963.393520	22.626535
94.441469	2979.501049	22.631552
94.525667	2974.292629	22.636570
94.026023	2973.067295	22.641587
94.583334	2967.472290	22.646605
94.790707	2975.036716	22.651623
94.342273	2986.627069	22.656640
94.573189	2988.793835	22.661658
95.166255	2995.073231	22.666675
95.500523	2988.730421	22.671693
95.508544	2988.997347	22.676711
95.433492	2991.852762	22.681728
95.630693	2993.251538	22.686746
95.613208	2991.294170	22.691763
95.397164	2989.642501	22.696781
95.457823	2997.946383	22.701799
95.219714	3011.350189	22.706816
95.726342	3015.619995	22.711834
95.726383	3013.887126	22.716851
95.821595	3030.694790	22.721869
96.042742	3034.229738	22.726887
96.386934	3047.595998	22.731904
96.241444	3042.950634	22.736922
96.481495	3040.536290	22.741939
96.464137	3041.103879	22.746957
96.622514	3044.254135	22.751975
96.231162	3054.771940	22.756992
96.583524	3063.557242	22.762010
96.852681	3063.436071	22.767027
96.629357	3062.019097	22.772045
97.137264	3073.361833	22.777063
97.393874	3085.722379	22.782080
97.517610	3086.532987	22.787098
97.297873	3077.938171	22.792115
97.714973	3087.243590	22.797133
97.750536	3077.964905	22.802151
97.731691	3085.782599	22.807168
97.683087	3091.755403	22.812186
98.053970	3108.188545	22.817203
98.301445	3099.697270	22.822221
98.196882	3106.199626	22.827239
97.892025	3116.899602	22.832256
98.391343	3112.929634	22.837274
98.305596	3107.454271	22.842291
98.381643	3123.681119	22.847309
98.393232	3131.563502	22.852327
98.568387	3135.582269	22.857344
98.837270	3125.541069	22.862362
98.927424	3125.100756	22.867379
99.064476	3129.639960	22.872397
99.564716	3137.515226	22.877415
99.298867	3158.069225	22.882432
99.598988	3145.630684	22.887450
99.509251	3142.362152	22.892467
99.721903	3152.633884	22.897485
100.055234	3143.264326	22.902503
99.814121	3147.484031	22.907520
99.947949	3141.582883	22.912538
99.889907	3153.819178	22.917555
99.817841	3149.844033	22.922573
100.061001	3151.696433	22.927591
99.708237	3170.973159	22.932608
99.968431	3170.187424	22.937626
100.441781	3174.547701	22.942643
100.252447	3176.338456	22.947661
100.606043	3189.940067	22.952679
100.546172	3201.984151	22.957696
100.690515	3197.075557	22.962714
101.087653	3199.282590	22.967731
101.014092	3195.945232	22.972749
101.219025	3187.236488	22.977767
101.244777	3199.292405	22.982784
101.335539	3214.314496	22.987802
101.420139	3213.865582	22.992819
101.269392	3227.637768	22.997837
101.696985	3214.049268	23.002855
101.329953	3221.874227	23.007872
101.736289	3219.585308	23.012890
101.858124	3214.582393	23.017907
102.103367	3249.262746	23.022925
102.421179	3235.233771	23.027943
102.315869	3239.590034	23.032960
102.585622	3227.389758	23.037978
102.534751	3236.184663	23.042995
102.633683	3243.633628	23.048013
102.741890	3235.741705	23.053031
102.311268	3240.963250	23.058048
102.482867	3235.425436	23.063066
102.944194	3242.675593	23.068083
102.955594	3255.213548	23.073101
103.238105	3254.916691	23.078119
103.246610	3261.057355	23.083136
103.011118	3264.288295	23.088154
103.489970	3254.024752	23.093171
103.311772	3276.941822	23.098189
103.585114	3280.443392	23.103207
103.521021	3285.108836	23.108224
103.727356	3282.794431	23.113242
103.851984	3286.319301	23.118259
103.757216	3292.681313	23.123277
104.435400	3298.117381	23.128295
104.033834	3310.218226	23.133312
103.788813	3314.760522	23.138330
104.254425	3324.566624	23.143347
103.818831	3330.745326	23.148365
104.358950	3334.574395	23.153383
104.461874	3341.312613	23.158400
104.398638	3346.186252	23.163418
104.947423	3361.553337	23.168435
104.963083	3362.791208	23.173453
105.069776	3358.996325	23.178471
105.252149	3372.539680	23.183488
105.454214	3377.059291	23.188506
105.421086	3378.162773	23.193523
105.612609	3379.606657	23.198541
106.066297	3380.128865	23.203559
105.862566	3378.844516	23.208576
106.225034	3379.428359	23.213594
106.106712	3386.712574	23.218611
106.231105	3392.847752	23.223629
106.374988	3397.420672	23.228647
106.612655	3402.152496	23.233664
106.365407	3405.369521	23.238682
106.978538	3390.621869	23.243699
106.671217	3402.802699	23.248717
106.830698	3395.423461	23.253735
106.928566	3402.654875	23.258752
106.954100	3415.361166	23.263770
107.255267	3425.657062	23.268787
106.957737	3428.089739	23.273805
106.873797	3424.125862	23.278823
107.346424	3432.958786	23.283840
107.312226	3441.975276	23.288858
107.751983	3450.696575	23.293875
107.588606	3459.143083	23.298893
107.785212	3449.356063	23.303911
108.034167	3450.544764	23.308928
108.088590	3464.486990	23.313946
108.137885	3473.503039	23.318963
108.363211	3479.830750	23.323981
108.148623	3474.596403	23.328999
108.391383	3472.140546	23.334016
108.457309	3479.111865	23.339034
108.637452	3484.720707	23.344051
108.479609	3503.692649	23.349069
108.938521	3496.774625	23.354087
108.493562	3498.996841	23.359104
108.656703	3509.958297	23.364122
109.092630	3522.070108	23.369139
108.964593	3527.613617	23.374157
109.251695	3527.773702	23.379175
109.307713	3534.036424	23.384192
109.132724	3551.379289	23.389210
109.630808	3548.653010	23.394227
109.772866	3553.459822	23.399245
110.045318	3555.553869	23.404263
110.005458	3557.078207	23.409280
110.427066	3578.377186	23.414298
110.599510	3578.006035	23.419315
110.672494	3581.980939	23.424333
110.935220	3583.858726	23.429351
111.335194	3573.809366	23.434368
110.949817	3578.304277	23.439386
111.541936	3570.330083	23.444403
111.255990	3580.156224	23.449421
111.344426	3576.749227	23.454439
111.149761	3580.841815	23.459456
110.969757	3575.283231	23.464474
111.435977	3569.156271	23.469491
110.989247	3599.069192	23.474509
111.304097	3600.828344	23.479527
111.560285	3600.390415	23.484544
111.839122	3617.943156	23.489562
111.655969	3620.392658	23.494579
111.851479	3626.062263	23.499597
111.948773	3621.403964	23.504615
112.116606	3631.326326	23.509632
111.930529	3645.394746	23.514650
112.107443	3639.720255	23.519667
112.289469	3657.392361	23.524685
112.498110	3668.447787	23.529703
112.581531	3664.807990	23.534720
112.562347	3679.715127	23.539738
113.242891	3688.193656	23.544755
113.269396	3699.176633	23.549773
113.497940	3690.312444	23.554791
113.811163	3695.546992	23.559808
113.349267	3700.404275	23.564826
113.713171	3705.413098	23.569843
113.794059	3719.670164	23.574861
113.837341	3717.409657	23.579879
114.104580	3720.962771	23.584896
114.013371	3710.573651	23.589914
114.133466	3717.833272	23.594931
114.387752	3735.317378	23.599949
114.699339	3733.993301	23.604967
114.758765	3725.531196	23.609984
114.672219	3735.323025	23.615002
115.192430	3734.985765	23.620019
115.162161	3738.920066	23.625037
114.520138	3743.095401	23.630055
114.828205	3758.860363	23.635072
115.095977	3767.122682	23.640090
115.721643	3758.792795	23.645107
115.598814	3769.732926	23.650125
115.653654	3775.150014	23.655143
115.899264	3789.678026	23.660160
115.794270	3788.895821	23.665178
116.081449	3789.564070	23.670195
116.096524	3794.113082	23.675213
115.806964	3794.262511	23.680231
115.951119	3802.796722	23.685248
116.194849	3808.256822	23.690266
116.274223	3806.085340	23.695283
116.449192	3816.710554	23.700301
116.403924	3823.487950	23.705319
116.485069	3831.246112	23.710336
116.602972	3840.968091	23.715354
116.906365	3841.498079	23.720371
116.924096	3865.966537	23.725389
117.107823	3860.789616	23.730407
117.472110	3861.840334	23.735424
117.121355	3872.118678	23.740442
117.623879	3875.735966	23.745459
117.807352	3891.593159	23.750477
117.781732	3898.418007	23.755495
118.005329	3884.062404	23.760512
118.090915	3897.693912	23.765530
118.468202	3910.809430	23.770547
118.323773	3914.272416	23.775565
117.940413	3924.325481	23.780583
118.431761	3921.862183	23.785600
118.351092	3938.284759	23.790618
118.957923	3942.845260	23.795635
119.031539	3942.997763	23.800653
119.418580	3952.646073	23.805671
119.612444	3940.883320	23.810688
119.254863	3950.907110	23.815706
119.551785	3960.111867	23.820723
119.772146	3964.849708	23.825741
119.682339	3962.341727	23.830759
120.150579	3965.475164	23.835776
119.902118	3975.573408	23.840794
119.924572	3961.729027	23.845811
120.252461	3981.275587	23.850829
120.179059	3986.157303	23.855847
120.423755	3987.558187	23.860864
120.200041	3991.140925	23.865882
120.537696	3994.149632	23.870899
120.595386	4006.696637	23.875917
120.678637	4012.172472	23.880935
120.837210	4010.695590	23.885952
120.984855	4035.778360	23.890970
121.087626	4036.639643	23.895987
121.598542	4039.744313	23.901005
121.418523	4032.058176	23.906023
121.514322	4036.812393	23.911040
121.653904	4056.641048	23.916058
121.924449	4054.458524	23.921075
122.220697	4060.529129	23.926093
121.926833	4054.940889	23.931111
122.326269	4065.256476	23.936128
122.413812	4073.910158	23.941146
122.642270	4080.635297	23.946163
122.729717	4084.989972	23.951181
123.001046	4077.179445	23.956199
123.052949	4079.494335	23.961216
122.948170	4085.331073	23.966234
123.279578	4098.917908	23.971251
123.415719	4094.625858	23.976269
123.362536	4109.317726	23.981287
123.831980	4099.156188	23.986304
123.669805	4104.957735	23.991322
123.501019	4103.238585	23.996339
123.866246	4111.416354	24.001357
123.637341	4124.945796	24.006375
124.140484	4112.178084	24.011392
124.073102	4132.815724	24.016410
123.945103	4127.785414	24.021427
124.325159	4145.436440	24.026445
124.284996	4154.829833	24.031463
124.335297	4145.166365	24.036480
124.641049	4155.329390	24.041498
124.831023	4174.878827	24.046515
125.307830	4176.514814	24.051533
125.405442	4184.917615	24.056551
125.026055	4174.595470	24.061568
125.244367	4173.393295	24.066586
125.450309	4183.246861	24.071603
125.664184	4196.908999	24.076621
125.650717	4209.359973	24.081639
125.936608	4197.453223	24.086656
125.837226	4208.317348	24.091674
126.026850	4212.318307	24.096691
126.214425	4216.995065	24.101709
126.143279	4239.814512	24.106727
126.166195	4226.329690	24.111744
126.451332	4248.007516	24.116762
126.439343	4251.730739	24.121779
126.925814	4256.284926	24.126797
126.691783	4273.214766	24.131815
126.910205	4278.641097	24.136832
127.043620	4288.357730	24.141850
127.324787	4299.803048	24.146867
127.463809	4297.237076	24.151885
127.634219	4307.165718	24.156903
127.741146	4307.420325	24.161920
128.047779	4318.400824	24.166938
128.192004	4322.323696	24.171955
128.462741	4324.907352	24.176973
127.941821	4325.639095	24.181991
128.520281	4324.134285	24.187008
128.593572	4335.422805	24.192026
128.722534	4355.332362	24.197043
128.851925	4348.295193	24.202061
128.816335	4352.391440	24.207079
129.507821	4351.506524	24.212096
129.040949	4360.891118	24.217114
129.562231	4370.253479	24.222131
129.748586	4373.099722	24.227149
129.560927	4387.948610	24.232167
129.951132	4372.922601	24.237184
130.071181	4376.445246	24.242202
130.189628	4391.085201	24.247219
130.257250	4394.253069	24.252237
130.335891	4394.843538	24.257255
130.383818	4390.571552	24.262272
130.102530	4392.095905	24.267290
130.648654	4414.219137	24.272307
130.924231	4416.540062	24.277325
130.688848	4429.322662	24.282343
130.464630	4419.774654	24.287360
131.124710	4439.803109	24.292378
131.308661	4448.530248	24.297395
131.634332	4438.340543	24.302413
131.586324	4457.005878	24.307431
132.002246	4461.334435	24.312448
131.952215	4472.071039	24.317466
131.646126	4480.638229	24.322483
132.173556	4471.729992	24.327501
132.400725	4483.196512	24.332519
132.681316	4496.876832	24.337536
132.647389	4494.865060	24.342554
132.564699	4502.276712	24.347571
132.784035	4499.470862	24.352589
133.045811	4504.808401	24.357607
133.109130	4495.628806	24.362624
132.952801	4504.904849	24.367642
132.947996	4527.404928	24.372659
133.085570	4525.820818	24.377677
133.087096	4540.362421	24.382695
133.444026	4543.573373	24.387712
133.384520	4550.378522	24.392730
133.571486	4556.930419	24.397747
133.750707	4560.582715	24.402765
133.853068	4576.390085	24.407783
133.827326	4572.549411	24.412800
134.383010	4595.675133	24.417818
134.073701	4610.675834	24.422835
135.016827	4605.875301	24.427853
135.229563	4619.484276	24.432871
135.541528	4624.315259	24.437888
135.552440	4625.430856	24.442906
135.078993	4623.772012	24.447923
135.236047	4623.860946	24.452941
135.262091	4632.777050	24.457959
135.833094	4645.591294	24.462976
135.868625	4651.999655	24.467994
135.899869	4655.220616	24.473011
135.956065	4659.435125	24.478029
136.035606	4666.568906	24.483047
136.084388	4669.572480	24.488064
136.655763	4667.317503	24.493082
136.420891	4679.705634	24.498099
136.566014	4690.828453	24.503117
136.719096	4698.433672	24.508135
137.136944	4707.916578	24.513152
137.237295	4704.441218	24.518170
137.254668	4724.498078	24.523187
137.578989	4718.096254	24.528205
137.580852	4721.915255	24.533223
137.869111	4726.263876	24.538240
137.948466	4738.691201	24.543258
137.949965	4746.231806	24.548275
138.119853	4748.455697	24.553293
138.017482	4759.083878	24.558311
138.450409	4771.774643	24.563328
138.903174	4776.226921	24.568346
138.805295	4785.569707	24.573363
138.896174	4778.371110	24.578381
139.002849	4786.412925	24.583399
139.444760	4794.825199	24.588416
139.237273	4804.188322	24.593434
139.226819	4809.331860	24.598451
139.254621	4803.614080	24.603469
139.414965	4824.500916	24.608487
139.365742	4833.618302	24.613504
139.647271	4839.884025	24.618522
139.469860	4857.313740	24.623539
139.847401	4854.397825	24.628557
140.010958	4874.633967	24.633575
139.993387	4889.734392	24.638592
140.481992	4886.668498	24.643610
140.613508	4910.255641	24.648627
141.072063	4907.841544	24.653645
141.394288	4913.557989	24.658663
141.521702	4913.272782	24.663680
141.498583	4911.666466	24.668698
141.380029	4930.065561	24.673715
141.928432	4931.658838	24.678733
142.047841	4931.557964	24.683751
142.136454	4939.586894	24.688768
142.167016	4940.753093	24.693786
141.815873	4944.018228	24.698803
142.198416	4945.650117	24.703821
142.780632	4954.899070	24.708839
142.703474	4959.791105	24.713856
142.743809	4955.097197	24.718874
142.927974	4955.080875	24.723891
143.465094	4970.053432	24.728909
143.293620	4980.948250	24.733927
143.588718	4984.468842	24.738944
143.822158	4985.559069	24.743962
143.520069	4979.671956	24.748979
143.811604	4984.973409	24.753997
143.543691	4992.212257	24.759015
143.622884	5011.170732	24.764032
143.797328	5013.917933	24.769050
143.790886	5022.583635	24.774067
144.045484	5031.615643	24.779085
144.224838	5038.658176	24.784103
144.577536	5049.947559	24.789120
144.440539	5054.972101	24.794138
144.841626	5070.209109	24.799155
144.995978	5078.069971	24.804173
145.200177	5076.484847	24.809191
145.420144	5100.247774	24.814208
145.787924	5107.469148	24.819226
145.546443	5112.522701	24.824243
145.725401	5114.158091	24.829261
146.188328	5122.914450	24.834279
146.013391	5138.377490	24.839296
146.364774	5131.772418	24.844314
146.412726	5147.775047	24.849331
146.859209	5158.200681	24.854349
146.531643	5160.486773	24.859367
146.786390	5160.674042	24.864384
147.135692	5174.060015	24.869402
147.254110	5187.924093	24.874419
147.464957	5189.087317	24.879437
147.700993	5182.001554	24.884455
147.459985	5191.022900	24.889472
147.495233	5215.752427	24.894490
147.804415	5211.006866	24.899507
147.698336	5221.556982	24.904525
148.563288	5227.175875	24.909543
148.393363	5233.035811	24.914560
148.664038	5231.954787	24.919578
148.636508	5246.441529	24.924595
148.879651	5259.790534	24.929613
149.366961	5260.001346	24.934631
149.013488	5259.987181	24.939648
149.156943	5267.193257	24.944666
149.627073	5281.235895	24.949683
149.442337	5275.443939	24.954701
149.863101	5295.832808	24.959719
149.929233	5306.914716	24.964736
150.479408	5300.521500	24.969754
150.627788	5309.857540	24.974771
150.404785	5302.752103	24.979789
150.886478	5312.708287	24.984807
150.570505	5331.145027	24.989824
150.849615	5331.805133	24.994842
151.104152	5337.769064	24.999859
151.233469	5334.333239	25.004877
151.362967	5347.428642	25.009895
151.236342	5358.433454	25.014912
151.607386	5353.801272	25.019930
151.210398	5362.319982	25.024947
151.134566	5373.323159	25.029965
151.274457	5378.465399	25.034983
152.007590	5404.376912	25.040000
152.203450	5411.571679	25.045018
152.143574	5418.891742	25.050035
152.498998	5438.233532	25.055053
152.532578	5434.863193	25.060071
152.792645	5449.020943	25.065088
152.958052	5456.384643	25.070106
153.596005	5463.724823	25.075123
153.579139	5459.450111	25.080141
153.811048	5464.268609	25.085159
153.727479	5470.853749	25.090176
153.807307	5468.663059	25.095194
153.884096	5483.455624	25.100211
154.062315	5494.497990	25.105229
154.271095	5479.278531	25.110247
154.161886	5494.583212	25.115264
154.747875	5515.394687	25.120282
155.083637	5524.452106	25.125299
154.730697	5525.274370	25.130317
154.905513	5523.876898	25.135335
155.149325	5539.539834	25.140352
155.445354	5545.513116	25.145370
155.754057	5552.444040	25.150387
155.562769	5558.247451	25.155405
155.909482	5559.948144	25.160423
155.798462	5569.678502	25.165440
156.234066	5570.039470	25.170458
156.337960	5588.369655	25.175475
155.989970	5585.276876	25.180493
156.557834	5599.575923	25.185511
156.489076	5622.731332	25.190528
156.766851	5616.882593	25.195546
156.798273	5622.108186	25.200563
156.972249	5636.936157	25.205581
157.380668	5633.715399	25.210599
157.462324	5654.817541	25.215616
157.789225	5662.787362	25.220634
157.969541	5664.510976	25.225651
157.792637	5668.272951	25.230669
158.342620	5678.351219	25.235687
158.090410	5691.143649	25.240704
158.713595	5699.610019	25.245722
159.128389	5704.819769	25.250739
158.870122	5713.042277	25.255757
159.124037	5715.354137	25.260775
159.346084	5722.589118	25.265792
159.468785	5719.776126	25.270810
159.548926	5734.287425	25.275827
159.660814	5744.974157	25.280845
159.796200	5734.756722	25.285863
159.863135	5750.870547	25.290880
160.304590	5761.578262	25.295898
160.472711	5772.297238	25.300915
160.464304	5771.206240	25.305933
160.734056	5776.280899	25.310951
160.685859	5789.966350	25.315968
161.173523	5795.947574	25.320986
161.251157	5801.999348	25.326003
160.954437	5803.497822	25.331021
161.386597	5813.979742	25.336039
161.268219	5832.644881	25.341056
161.441051	5842.498220	25.346074
162.205820	5848.423423	25.351091
161.813464	5856.831150	25.356109
162.160441	5855.460345	25.361127
161.837818	5872.831702	25.366144
162.140518	5870.830175	25.371162
162.480067	5886.244813	25.376179
162.381652	5904.976346	25.381197
162.923335	5899.171405	25.386215
162.951604	5913.700442	25.391232
163.238466	5927.980635	25.396250
163.416358	5937.555441	25.401267
163.589140	5944.091120	25.406285
163.416144	5956.495674	25.411303
163.547795	5952.686874	25.416320
164.180292	5958.178265	25.421338
164.523230	5972.809575	25.426355
164.297867	5983.435638	25.431373
164.522630	5991.238513	25.436391
164.476557	5998.749207	25.441408
164.964951	6011.845682	25.446426
165.306136	6014.800512	25.451443
164.406468	6018.050752	25.456461
165.395542	6024.960501	25.461479
165.329114	6039.602332	25.466496
165.744424	6050.225925	25.471514
165.792474	6059.199256	25.476531
165.973320	6070.358358	25.481549
166.349457	6075.918358	25.486567
166.610975	6088.709502	25.491584
166.280004	6087.043981	25.496602
166.792333	6095.483710	25.501619
166.793468	6110.383337	25.506637
167.307572	6111.426508	25.511655
167.245526	6114.734947	25.516672
167.393436	6136.373384	25.521690
167.727885	6138.906283	25.526707
167.375948	6152.005080	25.531725
167.951133	6155.368378	25.536743
167.670000	6162.672892	25.541760
167.995386	6175.204707	25.546778
168.527842	6187.246358	25.551795
168.396478	6202.144720	25.556813
168.800075	6207.548932	25.561831
169.092077	6229.104927	25.566848
168.836944	6225.899631	25.571866
169.652755	6235.671393	25.576883
169.617022	6255.438359	25.581901
169.936711	6251.994637	25.586919
169.358353	6258.506047	25.591936
169.895543	6271.995977	25.596954
169.975355	6274.126837	25.601971
170.171778	6275.099828	25.606989
170.687809	6295.834765	25.612007
170.562352	6306.189663	25.617024
170.566871	6312.183611	25.622042
171.122811	6323.041032	25.627059
170.998773	6338.898023	25.632077
171.510956	6337.390815	25.637095
171.718115	6356.677886	25.642112
171.282932	6375.412148	25.647130
171.718674	6367.442306	25.652147
171.684499	6381.312253	25.657165
172.033254	6397.382496	25.662183
171.894000	6409.876774	25.667200
172.175844	6426.948764	25.672218
172.592920	6423.376108	25.677236
172.847627	6442.750525	25.682253
173.120823	6432.204903	25.687271
173.289726	6449.297764	25.692288
173.382359	6465.787010	25.697306
174.138197	6463.790195	25.702324
173.839612	6471.972005	25.707341
174.361888	6474.248236	25.712359
174.430369	6475.089754	25.717376
174.367862	6494.930621	25.722394
174.499237	6485.912992	25.727412
174.621858	6501.459995	25.732429
174.762252	6491.301335	25.737447
175.336027	6505.016155	25.742464
175.175023	6523.575028	25.747482
175.302312	6522.087064	25.752500
175.286675	6526.471100	25.757517
175.144193	6537.930529	25.762535
175.405003	6544.891433	25.767552
175.555244	6565.302003	25.772570
176.215992	6569.343323	25.777588
176.106736	6585.147702	25.782605
176.183154	6595.783664	25.787623
176.666717	6608.764522	25.792640
176.658422	6618.570891	25.797658
177.272292	6628.251385	25.802676
177.118171	6639.456997	25.807693
176.988371	6648.436380	25.812711
177.262022	6653.889495	25.817728
177.399079	6663.669961	25.822746
177.835530	6678.909087	25.827764
177.956190	6691.110289	25.832781
178.041399	6696.785507	25.837799
178.295333	6713.442274	25.842816
178.353251	6723.863385	25.847834
178.841949	6726.586870	25.852852
178.879295	6739.435685	25.857869
179.365262	6749.549831	25.862887
179.200304	6765.101070	25.867904
179.277762	6766.600982	25.872922
179.923022	6775.976734	25.877940
180.217270	6790.938328	25.882957
180.241675	6800.152492	25.887975
180.332823	6792.883612	25.892992
180.463378	6817.811881	25.898010
180.508221	6820.159794	25.903028
180.764650	6823.064897	25.908045
180.960989	6831.286136	25.913063
180.991049	6848.015980	25.918080
181.008962	6859.305265	25.923098
181.353478	6874.694703	25.928116
181.676120	6885.061806	25.933133
181.767453	6884.482319	25.938151
182.115216	6891.240319	25.943168
182.060002	6908.255069	25.948186
182.577297	6909.843933	25.953204
182.686821	6927.641059	25.958221
182.895136	6933.732717	25.963239
183.336076	6942.799619	25.968256
183.365557	6959.403379	25.973274
183.614845	6956.491445	25.978292
183.506833	6957.821543	25.983309
183.680055	6974.636409	25.988327
184.219439	6984.676022	25.993344
183.959468	6997.735755	25.998362
184.236320	6995.952830	26.003380
184.230614	7013.414517	26.008397
184.258197	7022.691432	26.013415
184.720787	7028.250808	26.018432
184.605575	7046.544166	26.023450
185.205312	7061.657010	26.028468
185.351910	7071.404628	26.033485
185.313515	7066.971911	26.038503
185.727062	7073.937501	26.043520
185.840703	7097.195629	26.048538
186.145689	7108.452722	26.053556
186.247269	7117.970648	26.058573
186.411424	7116.991442	26.063591
186.748022	7132.833779	26.068608
186.510667	7140.441200	26.073626
186.626556	7131.823455	26.078644
187.134520	7159.158629	26.083661
187.249345	7172.990046	26.088679
187.442738	7180.700478	26.093696
187.496914	7189.629205	26.098714
187.911309	7200.897628	26.103732
188.097463	7209.183770	26.108749
188.433022	7225.187354	26.113767
188.334090	7221.613303	26.118784
188.612912	7244.564771	26.123802
188.735187	7251.626570	26.128820
189.182377	7253.355883	26.133837
189.375818	7274.237173	26.138855
189.854709	7279.945606	26.143872
189.658545	7284.522265	26.148890
189.432670	7285.419405	26.153908
189.759207	7298.507433	26.158925
189.803220	7310.863117	26.163943
190.063664	7323.090195	26.168960
190.300430	7337.751857	26.173978
190.452306	7351.284005	26.178996
190.569687	7359.151641	26.184013
190.917186	7367.968206	26.189031
191.297356	7381.818194	26.194048
191.626300	7402.078575	26.199066
192.032699	7414.383872	26.204084
191.895680	7423.450002	26.209101
192.334982	7431.343004	26.214119
192.651059	7439.264785	26.219136
192.425389	7439.315827	26.224154
193.049223	7445.430956	26.229172
193.327053	7459.900021	26.234189
193.269764	7469.294638	26.239207
193.230431	7465.878523	26.244224
193.093740	7493.109980	26.249242
193.739444	7496.560352	26.254260
193.905169	7504.218428	26.259277
194.125381	7519.912011	26.264295
194.106454	7525.954225	26.269312
194.033279	7552.787508	26.274330
194.182925	7558.806482	26.279348
194.822174	7574.102980	26.284365
194.607242	7591.392785	26.289383
195.499517	7593.494387	26.294400
195.236961	7607.202143	26.299418
195.673451	7619.237674	26.304436
195.837760	7627.379047	26.309453
196.037142	7633.611245	26.314471
196.230166	7647.427611	26.319488
196.446474	7654.676884	26.324506
196.574415	7666.675542	26.329524
196.928304	7682.414619	26.334541
197.065889	7687.103258	26.339559
197.319320	7693.696383	26.344576
197.884284	7709.768632	26.349594
197.814913	7715.730414	26.354612
198.009931	7712.940519	26.359629
198.076649	7737.861092	26.364647
198.644649	7744.445996	26.369664
198.376371	7746.486335	26.374682
198.499278	7754.435356	26.379700
198.705412	7763.428953	26.384717
198.688200	7779.087338	26.389735
199.208096	7790.541647	26.394752
198.933524	7802.385614	26.399770
199.553218	7808.908774	26.404788
199.781933	7824.939088	26.409805
199.954714	7837.319151	26.414823
200.155991	7834.638754	26.419840
200.146381	7848.142895	26.424858
200.293214	7857.016388	26.429876
200.489047	7873.137136	26.434893
200.753410	7881.834376	26.439911
200.971540	7894.864043	26.444928
201.029736	7907.738820	26.449946
200.977114	7911.001905	26.454964
201.578712	7927.633722	26.459981
201.752800	7938.902359	26.464999
202.010312	7958.094823	26.470016
202.093690	7969.166164	26.475034
202.156875	7984.685846	26.480052
202.886239	7989.660706	26.485069
202.964502	8003.261692	26.490087
203.130680	8016.447966	26.495104
203.145251	8022.450367	26.500122
203.470007	8041.288261	26.505140
203.940791	8044.245221	26.510157
203.873936	8060.571453	26.515175
204.314086	8062.333520	26.520192
204.495090	8073.465400	26.525210
204.686323	8099.651893	26.530228
204.551064	8099.404633	26.535245
204.729160	8116.567058	26.540263
205.207768	8122.493640	26.545280
205.056275	8130.324798	26.550298
205.404450	8139.769893	26.555316
205.712162	8156.122773	26.560333
205.969285	8176.319486	26.565351
206.173468	8178.320585	26.570368
206.248607	8199.884449	26.575386
206.273707	8206.434599	26.580404
206.786726	8218.420648	26.585421
206.662954	8238.194058	26.590439
206.811189	8250.051003	26.595456
207.378154	8268.598615	26.600474
207.817134	8282.342197	26.605492
207.728504	8294.725633	26.610509
207.837837	8305.234297	26.615527
208.568397	8321.767339	26.620544
208.763990	8327.476281	26.625562
209.166615	8346.551701	26.630580
209.094600	8347.522658	26.635597
209.490510	8355.426014	26.640615
209.797791	8369.660708	26.645632
209.879370	8367.223143	26.650650
209.664644	8378.076229	26.655668
210.104950	8389.180308	26.660685
210.363068	8406.971369	26.665703
210.257956	8416.162428	26.670720
210.629835	8440.471011	26.675738
210.811354	8435.397340	26.680756
211.254409	8458.763435	26.685773
211.396256	8465.434303	26.690791
211.443013	8474.023839	26.695808
211.717443	8483.155475	26.700826
211.636609	8497.485796	26.705844
212.121171	8512.078001	26.710861
211.918602	8530.487541	26.715879
212.150118	8538.164155	26.720896
212.400505	8554.523211	26.725914
212.636686	8574.051159	26.730932
212.933241	8587.283717	26.735949
213.292450	8608.705683	26.740967
213.482623	8595.314583	26.745984
213.738449	8617.270532	26.751002
213.654048	8635.096527	26.756020
214.335585	8635.908407	26.761037
214.170718	8646.084514	26.766055
214.482769	8657.426692	26.771072
215.011964	8670.266101	26.776090
214.638402	8677.024101	26.781108
215.028922	8680.754625	26.786125
215.357192	8703.731733	26.791143
215.873367	8707.316289	26.796160
216.069213	8724.302851	26.801178
216.370706	8745.642458	26.806196
215.952077	8743.261105	26.811213
216.349165	8768.519647	26.816231
216.152675	8773.908126	26.821248
217.042212	8791.104958	26.826266
217.089662	8810.293327	26.831284
217.171970	8820.096142	26.836301
217.547129	8835.305614	26.841319
217.988546	8850.214254	26.846336
218.099302	8857.890975	26.851354
217.970805	8874.691693	26.856372
218.208021	8884.249268	26.861389
218.457365	8901.426518	26.866407
218.769320	8910.192561	26.871424
218.649187	8926.739436	26.876442
219.270307	8941.237972	26.881460
219.737567	8954.103068	26.886477
219.731415	8972.030788	26.891495
219.808630	8984.319243	26.896512
220.505893	8992.661881	26.901530
220.295441	9005.213264	26.906548
220.710370	9012.138331	26.911565
220.800793	9042.083296	26.916583
221.129035	9054.013590	26.921600
221.524646	9053.793656	26.926618
221.735591	9081.885435	26.931636
222.275475	9084.298163	26.936653
221.977889	9096.108671	26.941671
222.142413	9105.150484	26.946688
222.540849	9114.903932	26.951706
222.579539	9133.430979	26.956724
223.037764	9139.351612	26.961741
223.038632	9156.931110	26.966759
223.329296	9165.934249	26.971776
223.647046	9181.099324	26.976794
223.756631	9196.900064	26.981812
224.109511	9202.780389	26.986829
224.107081	9220.751968	26.991847
224.452578	9234.766644	26.996864
224.896871	9244.171989	27.001882
225.311244	9264.424186	27.006900
225.535700	9271.278156	27.011917
225.816656	9281.520533	27.016935
225.655525	9288.270733	27.021952
225.938906	9298.155964	27.026970
226.114362	9314.650564	27.031988
226.538412	9320.475576	27.037005
226.772525	9326.633445	27.042023
227.103772	9338.778148	27.047040
227.050504	9349.309719	27.052058
227.328370	9368.090005	27.057076
227.840346	9376.502889	27.062093
228.042514	9384.506498	27.067111
227.850098	9391.350041	27.072128
228.283178	9399.661631	27.077146
227.957282	9407.526961	27.082164
228.584672	9421.314494	27.087181
228.510295	9444.968117	27.092199
228.728605	9453.423883	27.097216
229.147142	9464.509918	27.102234
229.366700	9482.453288	27.107252
229.590198	9502.145225	27.112269
229.956032	9521.934864	27.117287
230.062056	9539.517194	27.122304
230.274381	9538.337720	27.127322
230.122600	9552.910453	27.132340
230.778693	9567.716580	27.137357
230.533146	9572.771980	27.142375
230.645139	9601.950388	27.147392
231.223946	9615.575179	27.152410
231.389585	9632.030553	27.157428
231.778699	9649.556010	27.162445
232.059731	9662.873859	27.167463
232.006700	9687.051725	27.172480
232.303123	9694.194527	27.177498
232.548816	9712.295051	27.182516
232.808989	9723.472354	27.187533
233.214592	9743.328618	27.192551
233.189160	9763.441869	27.197568
234.067232	9779.769981	27.202586
233.705916	9794.694624	27.207604
234.376366	9814.831529	27.212621
234.444445	9822.512177	27.217639
234.866969	9830.999271	27.222656
235.099573	9846.613949	27.227674
235.116935	9871.642997	27.232692
235.521612	9877.101803	27.237709
235.866285	9894.306083	27.242727
235.669929	9910.082734	27.247744
236.517408	9922.361654	27.252762
236.165999	9932.441387	27.257780
236.374804	9952.650760	27.262797
236.891279	9964.523734	27.267815
237.251551	9985.410361	27.272832
237.591865	9991.441305	27.277850
237.645369	10014.368354	27.282868
238.038623	10019.787946	27.287885
238.446126	10021.959471	27.292903
238.781440	10038.208650	27.297920
238.796066	10046.459786	27.302938
239.081451	10068.425450	27.307956
239.279921	10080.212545	27.312973
239.535292	10088.817509	27.317991
239.701401	10098.143726	27.323008
240.033769	10105.527336	27.328026
240.160225	10127.189592	27.333044
239.959428	10133.011706	27.338061
240.492171	10147.888138	27.343079
240.705225	10171.377671	27.348096
240.766357	10178.835375	27.353114
241.044965	10201.736863	27.358132
241.329437	10208.417589	27.363149
241.535185	10232.827164	27.368167
241.763646	10248.401781	27.373184
242.278202	10261.361414	27.378202
242.390765	10274.652415	27.383220
242.518035	10301.537200	27.388237
242.941945	10320.983899	27.393255
242.834061	10340.390782	27.398272
243.411045	10336.126111	27.403290
243.519469	10365.400996	27.408308
243.917515	10376.452895	27.413325
244.019903	10395.119619	27.418343
244.442622	10418.024057	27.423360
244.745322	10422.494916	27.428378
245.136383	10430.191526	27.433396
245.023682	10437.190309	27.438413
245.546919	10448.213168	27.443431
245.543396	10461.310934	27.448448
246.018746	10469.467981	27.453466
246.183551	10469.432596	27.458484
246.308001	10477.571993	27.463501
246.559106	10491.946572	27.468519
246.568858	10515.724143	27.473536
246.884683	10519.627776	27.478554
247.234506	10542.837435	27.483572
247.545927	10546.350232	27.488589
247.799652	10565.116561	27.493607
247.875136	10582.177351	27.498624
248.014329	10598.704028	27.503642
248.163023	10619.981310	27.508660
248.217816	10632.419609	27.513677
248.506342	10657.334607	27.518695
248.884280	10677.597207	27.523712
249.615574	10704.113243	27.528730
249.822136	10715.574246	27.533748
249.801582	10730.209434	27.538765
250.090771	10741.818544	27.543783
250.437221	10768.363382	27.548800
250.603088	10785.040765	27.553818
250.962700	10795.319018	27.558836
251.408350	10809.840189	27.563853
251.485214	10815.369570	27.568871
251.933910	10839.849237	27.573888
252.084048	10852.894787	27.578906
252.552079	10868.021908	27.583924
252.344342	10885.771485	27.588941
253.304492	10891.759303	27.593959
253.101493	10910.944859	27.598976
253.063932	10918.083614	27.603994
253.656376	10930.463149	27.609012
253.781990	10951.905460	27.614029
254.601513	10959.917237	27.619047
254.310727	10974.077104	27.624064
254.804623	10994.830255	27.629082
255.154718	11001.905158	27.634100
255.065273	11016.090353	27.639117
255.444882	11026.836083	27.644135
255.471617	11048.319254	27.649152
255.868454	11064.837558	27.654170
256.039858	11085.429769	27.659188
256.167106	11099.540032	27.664205
256.795960	11105.241954	27.669223
256.761493	11127.802075	27.674240
257.042930	11145.307915	27.679258
257.647104	11158.863555	27.684276
257.180224	11182.186156	27.689293
258.031685	11191.831837	27.694311
258.054983	11220.830891	27.699328
258.509706	11238.638066	27.704346
259.000728	11255.107050	27.709364
259.149784	11251.925970	27.714381
259.526057	11263.581757	27.719399
259.494254	11286.804756	27.724416
260.114376	11301.646318	27.729434
260.215450	11307.124688	27.734452
260.259997	11323.158449	27.739469
260.612078	11333.558169	27.744487
260.775901	11357.123212	27.749504
260.830836	11376.347778	27.754522
261.287506	11392.200206	27.759540
261.483780	11402.864353	27.764557
261.736824	11413.617501	27.769575
261.944025	11432.174108	27.774592
262.419920	11448.955084	27.779610
262.686949	11456.134744	27.784628
262.800084	11475.798683	27.789645
263.047920	11471.721102	27.794663
262.736275	11498.041667	27.799680
263.225332	11520.602349	27.804698
263.753495	11535.354300	27.809716
263.852049	11556.792067	27.814733
264.544155	11569.999517	27.819751
264.329313	11588.025588	27.824768
264.714171	11608.638615	27.829786
264.888138	11619.628465	27.834804
265.082183	11644.174335	27.839821
265.427170	11669.208140	27.844839
265.506719	11689.922764	27.849856
265.456584	11701.446685	27.854874
265.785475	11719.940306	27.859892
266.568351	11753.204098	27.864909
266.882122	11764.920512	27.869927
267.315208	11793.518379	27.874944
267.541943	11803.833790	27.879962
267.947356	11826.793186	27.884980
268.246749	11844.372650	27.889997
268.617929	11858.975772	27.895015
268.842324	11861.776172	27.900032
268.818919	11881.682965	27.905050
269.578954	11894.744221	27.910068
269.689991	11922.679083	27.915085
270.069206	11929.563470	27.920103
270.206124	11943.186559	27.925120
270.671059	11950.900645	27.930138
270.975938	11968.217272	27.935156
270.943409	11983.259504	27.940173
271.222736	11990.263766	27.945191
271.388512	12008.233773	27.950208
271.646367	12029.293454	27.955226
271.830386	12037.525245	27.960244
272.036494	12065.994879	27.965261
272.549235	12073.123654	27.970279
272.188424	12098.022286	27.975296
272.913831	12117.448884	27.980314
273.461214	12148.388247	27.985332
273.213710	12162.810635	27.990349
273.877482	12179.041799	27.995367
273.955094	12209.202247	28.000384
274.102831	12210.609490	28.005402
274.442948	12235.145879	28.010420
274.481816	12264.257780	28.015437
275.185526	12287.720468	28.020455
275.089824	12304.557013	28.025472
275.493885	12325.117293	28.030490
276.159330	12339.087337	28.035508
276.069689	12358.354499	28.040525
276.785657	12379.999636	28.045543
276.549020	12398.358308	28.050560
276.826139	12418.998574	28.055578
277.382470	12442.124549	28.060596
277.386150	12462.217181	28.065613
277.897083	12476.413634	28.070631
278.435365	12502.258252	28.075648
278.250471	12521.351030	28.080666
278.816197	12530.401125	28.085684
279.015709	12560.309358	28.090701
279.406013	12571.376399	28.095719
279.406376	12596.819101	28.100736
279.447567	12610.801875	28.105754
280.406524	12627.372444	28.110772
280.343094	12645.789485	28.115789
280.572485	12657.033361	28.120807
280.993622	12679.631336	28.125824
281.199742	12700.823029	28.130842
281.509402	12713.320673	28.135860
281.676049	12729.352292	28.140877
281.666939	12746.564085	28.145895
282.270097	12764.235770	28.150912
282.527358	12782.021657	28.155930
282.843280	12795.911004	28.160948
283.150745	12822.006954	28.165965
283.465682	12831.450165	28.170983
283.814482	12851.280726	28.176000
283.890734	12874.112960	28.181018
284.314199	12882.654982	28.186036
284.799620	12916.668482	28.191053
285.154364	12924.618126	28.196071
285.233105	12937.338409	28.201088
285.414256	12962.677492	28.206106
285.520256	12978.235661	28.211124
285.919802	13000.379503	28.216141
286.472281	13012.858257	28.221159
286.398897	13040.053125	28.226176
286.629684	13060.717140	28.231194
286.958844	13079.392055	28.236212
287.058910	13107.033539	28.241229
287.618158	13130.807281	28.246247
288.049168	13151.455820	28.251264
288.543673	13173.957629	28.256282
288.878330	13190.418066	28.261300
289.346651	13215.210387	28.266317
289.697900	13228.027128	28.271335
290.093024	13235.920051	28.276352
290.352362	13262.627319	28.281370
290.596987	13260.548855	28.286388
290.885570	13280.133504	28.291405
291.167636	13291.350559	28.296423
291.586851	13306.285181	28.301440
291.286492	13327.279011	28.306458
291.806355	13342.955812	28.311476
291.995715	13348.894643	28.316493
292.275665	13375.049352	28.321511
292.785029	13389.897285	28.326528
292.696320	13414.136052	28.331546
292.723708	13424.483577	28.336564
293.334864	13452.771844	28.341581
293.450462	13475.895491	28.346599
294.139899	13488.668907	28.351616
294.176014	13522.014902	28.356634
294.603404	13536.664205	28.361652
294.494883	13554.081783	28.366669
294.685620	13575.677932	28.371687
295.112347	13597.862428	28.376704
295.624368	13632.883616	28.381722
296.272950	13644.340321	28.386740
296.221864	13669.735677	28.391757
296.504571	13693.171321	28.396775
296.920652	13704.553952	28.401792
296.987639	13729.662458	28.406810
297.252307	13746.374354	28.411828
297.528868	13776.540870	28.416845
297.814422	13792.788459	28.421863
298.317435	13813.306435	28.426880
298.455676	13835.883786	28.431898
299.034031	13855.973141	28.436916
299.454487	13893.289278	28.441933
299.293037	13902.479208	28.446951
299.771844	13917.054431	28.451968
300.275082	13930.713153	28.456986
300.483348	13954.078670	28.462004
300.839659	13974.790337	28.467021
301.113115	13993.200125	28.472039
301.239539	14002.174472	28.477056
301.970800	14021.892661	28.482074
301.828711	14043.513055	28.487092
302.487775	14072.360042	28.492109
302.510626	14083.223407	28.497127
302.795244	14098.577660	28.502144
303.032856	14113.339247	28.507162
303.605903	14132.084372	28.512180
303.784072	14154.008432	28.517197
303.828069	14169.668875	28.522215
304.093241	14180.039567	28.527232
304.401648	14212.245092	28.532250
305.044232	14227.410734	28.537268
305.057946	14250.983946	28.542285
305.384595	14273.462825	28.547303
306.297463	14294.081342	28.552320
306.208657	14315.504208	28.557338
306.459998	14331.498649	28.562356
307.018385	14363.106279	28.567373
307.119923	14373.486919	28.572391
307.572611	14393.252290	28.577408
307.544998	14412.366541	28.582426
307.940445	14432.317776	28.587444
308.406152	14459.224944	28.592461
308.166436	14481.097988	28.597479
308.867697	14497.729522	28.602496
309.029662	14520.607153	28.607514
309.576291	14550.059899	28.612532
310.038816	14570.070251	28.617549
310.389013	14591.917337	28.622567
310.898935	14610.887579	28.627584
310.860224	14635.072693	28.632602
311.156860	14649.961253	28.637620
311.559053	14682.336056	28.642637
311.495145	14709.825536	28.647655
312.272515	14724.095638	28.652672
312.556479	14736.077537	28.657690
312.635882	14758.200940	28.662708
312.605011	14786.399112	28.667725
312.716497	14815.418273	28.672743
313.605772	14828.069703	28.677760
314.317359	14862.619741	28.682778
314.742113	14876.427242	28.687796
315.005294	14894.451047	28.692813
315.098076	14921.069878	28.697831
315.637216	14931.075924	28.702848
315.989254	14962.533693	28.707866
315.860169	14981.670724	28.712884
316.272784	15006.493059	28.717901
316.441596	15022.968429	28.722919
316.553231	15042.064655	28.727936
316.871447	15060.260017	28.732954
317.263819	15084.261316	28.737972
317.743871	15114.205419	28.742989
317.784838	15134.863521	28.748007
318.517603	15157.911483	28.753024
318.525160	15182.885928	28.758042
319.002765	15211.096666	28.763060
319.622011	15222.950553	28.768077
319.401158	15249.025208	28.773095
320.286249	15264.971692	28.778112
320.565536	15274.345905	28.783130
320.565295	15303.143276	28.788148
320.956702	15321.169506	28.793165
321.159122	15341.505659	28.798183
321.763797	15352.976595	28.803200
321.872639	15377.237440	28.808218
322.170324	15399.908523	28.813236
322.553834	15411.474146	28.818253
322.600673	15433.448672	28.823271
323.272939	15459.800613	28.828288
323.416824	15479.479673	28.833306
323.464929	15504.486086	28.838324
324.023351	15523.497014	28.843341
324.300677	15554.143131	28.848359
324.481475	15576.845366	28.853376
324.940631	15593.392606	28.858394
325.262779	15618.094097	28.863412
325.637076	15648.099819	28.868429
325.839307	15669.251207	28.873447
326.291995	15684.397224	28.878464
326.776722	15707.607879	28.883482
326.732718	15740.663934	28.888500
327.472445	15766.557240	28.893517
327.494716	15792.929338	28.898535
328.075409	15810.664233	28.903552
328.175194	15837.848591	28.908570
328.611294	15871.840353	28.913588
329.191459	15889.139544	28.918605
329.006605	15906.343813	28.923623
329.592332	15925.366656	28.928640
329.870965	15959.623279	28.933658
330.095971	15985.325884	28.938676
330.671075	16007.189892	28.943693
330.836641	16038.748123	28.948711
331.217950	16062.458647	28.953728
331.971666	16078.176874	28.958746
332.017477	16112.915579	28.963764
332.392502	16131.216764	28.968781
332.722043	16155.715648	28.973799
333.221432	16176.824207	28.978816
333.354202	16200.766499	28.983834
333.279298	16225.189852	28.988852
333.811146	16252.881957	28.993869
334.038131	16279.345835	28.998887
334.394333	16296.342520	29.003904
334.560016	16333.665426	29.008922
334.941534	16366.178969	29.013940
335.483086	16387.530675	29.018957
335.435450	16431.914818	29.023975
336.010776	16449.730108	29.028992
336.790715	16483.684885	29.034010
336.890600	16506.612512	29.039028
337.311026	16533.889760	29.044045
337.503242	16568.249440	29.049063
338.026686	16589.225185	29.054080
338.722249	16617.050096	29.059098
338.858222	16636.949519	29.064116
339.259419	16655.812480	29.069133
339.525374	16680.347260	29.074151
340.097385	16699.679398	29.079168
340.152507	16723.081757	29.084186
340.622019	16746.182344	29.089204
340.967313	16765.322646	29.094221
341.076564	16793.287031	29.099239
341.597980	16810.204595	29.104256
341.955536	16843.145944	29.109274
342.232776	16873.377245	29.114292
342.574279	16884.264930	29.119309
342.577869	16919.318081	29.124327
343.069293	16948.274631	29.129344
343.660418	16973.930682	29.134362
343.729956	16988.196488	29.139380
344.198759	17008.666400	29.144397
344.123266	17032.335964	29.149415
344.485367	17056.625585	29.154432
344.976917	17091.975329	29.159450
345.246746	17108.566167	29.164468
345.618381	17131.774147	29.169485
345.779318	17164.055106	29.174503
346.311153	17185.210227	29.179520
346.732265	17217.153612	29.184538
346.694698	17246.534602	29.189556
347.399190	17263.632357	29.194573
347.867672	17297.394142	29.199591
348.261052	17323.580697	29.204608
348.483225	17342.150191	29.209626
348.746541	17374.345975	29.214644
349.231925	17394.864238	29.219661
349.348577	17429.230969	29.224679
350.088055	17455.161336	29.229696
350.158990	17477.128099	29.234714
350.627056	17513.448843	29.239732
350.898082	17535.156906	29.244749
351.366540	17565.773124	29.249767
351.593995	17589.629657	29.254784
351.892547	17620.727426	29.259802
352.386020	17649.703659	29.264820
352.824296	17674.323264	29.269837
353.534957	17703.322413	29.274855
353.701604	17731.048577	29.279872
353.959531	17751.558627	29.284890
354.042555	17778.040791	29.289908
354.853811	17791.906723	29.294925
354.875228	17832.416993	29.299943
355.507451	17862.230983	29.304960
355.895285	17885.412060	29.309978
356.038889	17911.272123	29.314996
356.353859	17935.241722	29.320013
356.706259	17972.345860	29.325031
356.993334	17998.366773	29.330048
357.360026	18013.098505	29.335066
357.689371	18043.434029	29.340084
358.488840	18071.699624	29.345101
358.601635	18107.584365	29.350119
359.173949	18124.286632	29.355136
359.360125	18163.066049	29.360154
359.884046	18187.281202	29.365172
360.210696	18208.671745	29.370189
360.264093	18223.547475	29.375207
360.323325	18255.441858	29.380224
360.852093	18290.307824	29.385242
361.293985	18315.016122	29.390260
361.853088	18346.169006	29.395277
362.165351	18373.431045	29.400295
362.672593	18405.969390	29.405312
362.823817	18441.008482	29.410330
363.170307	18477.324804	29.415348
363.673107	18493.703443	29.420365
363.892327	18525.497395	29.425383
364.300351	18557.792511	29.430400
364.262249	18579.461715	29.435418
364.776812	18609.788064	29.440436
365.293734	18650.386682	29.445453
365.751936	18684.462060	29.450471
366.383067	18709.469739	29.455488
366.355575	18729.829679	29.460506
366.708109	18765.848660	29.465524
367.540436	18784.999961	29.470541
367.958745	18804.664692	29.475559
367.449900	18834.305116	29.480576
368.031690	18853.735803	29.485594
368.562148	18879.486015	29.490612
369.194909	18917.312492	29.495629
369.468342	18946.678924	29.500647
369.723907	18968.959614	29.505664
369.978553	18991.581635	29.510682
370.667713	19015.967790	29.515700
370.402338	19046.827647	29.520717
371.225245	19075.432196	29.525735
371.310127	19106.565811	29.530752
372.004271	19130.843927	29.535770
372.274725	19168.531789	29.540788
373.027763	19200.072643	29.545805
373.389937	19217.693272	29.550823
373.713076	19249.579531	29.555840
374.034345	19260.155828	29.560858
374.420278	19291.071998	29.565876
374.695848	19310.184668	29.570893
375.265963	19351.085992	29.575911
375.634754	19376.464154	29.580928
375.897984	19390.499209	29.585946
376.012743	19427.832882	29.590964
376.405039	19452.240813	29.595981
376.864071	19480.643918	29.600999
377.248547	19520.696476	29.606016
377.477592	19540.581136	29.611034
377.520857	19577.231313	29.616052
377.765425	19605.257521	29.621069
378.437767	19642.352632	29.626087
378.710091	19678.676490	29.631104
379.382445	19719.183488	29.636122
379.601513	19751.105821	29.641140
380.160890	19781.395383	29.646157
380.507584	19814.586715	29.651175
380.915796	19851.079151	29.656192
381.623044	19877.270527	29.661210
381.953940	19913.585646	29.666228
382.329201	19942.754400	29.671245
382.663584	19975.739436	29.676263
382.972297	19997.753930	29.681280
383.269780	20030.239386	29.686298
383.686303	20073.674586	29.691316
383.862934	20098.622558	29.696333
384.384315	20125.917471	29.701351
384.676260	20166.270161	29.706368
385.000903	20209.107188	29.711386
385.481340	20240.780877	29.716404
386.180510	20274.814966	29.721421
386.711308	20301.274642	29.726439
386.962247	20332.213601	29.731456
387.219482	20355.487574	29.736474
387.280786	20389.470136	29.741492
388.307032	20423.965032	29.746509
388.428009	20453.806204	29.751527
388.449335	20493.228938	29.756544
388.794991	20522.106230	29.761562
389.380246	20553.372270	29.766580
390.057046	20584.421835	29.771597
390.369493	20619.123656	29.776615
390.723987	20665.021397	29.781632
391.058210	20677.586715	29.786650
391.581962	20713.456094	29.791668
391.757299	20736.509566	29.796685
392.188009	20777.094510	29.801703
392.540843	20811.543927	29.806720
392.893415	20835.170002	29.811738
393.306291	20876.522472	29.816756
393.870558	20909.321425	29.821773
394.189589	20934.722036	29.826791
394.521247	20973.414729	29.831808
394.696592	20987.679523	29.836826
394.943849	21024.294126	29.841844
395.636569	21062.519739	29.846861
396.060688	21086.109634	29.851879
396.054133	21129.259600	29.856896
396.456447	21154.919145	29.861914
397.649603	21193.186678	29.866932
397.668683	21223.613643	29.871949
398.110929	21250.789826	29.876967
398.078451	21288.611348	29.881984
398.517598	21320.059457	29.887002
399.105256	21348.937967	29.892020
399.485714	21389.626823	29.897037
399.645375	21428.631687	29.902055
400.108560	21465.333340	29.907072
400.747816	21499.385253	29.912090
401.389523	21537.746151	29.917108
401.262841	21569.529712	29.922125
401.694532	21604.770631	29.927143
402.188585	21652.986716	29.932160
402.957893	21684.996603	29.937178
403.293182	21716.246776	29.942196
403.622767	21753.551210	29.947213
403.931633	21792.893588	29.952231
404.633736	21831.909063	29.957248
404.796816	21867.938135	29.962266
404.913869	21898.799423	29.967284
405.259385	21937.656122	29.972301
406.060866	21977.945348	29.977319
406.418852	22009.426223	29.982336
406.569734	22048.869680	29.987354
407.529228	22082.809251	29.992372
407.811473	22122.510306	29.997389
408.184155	22160.585973	30.002407
408.373145	22201.982604	30.007424
409.228193	22225.323117	30.012442
409.772162	22262.196842	30.017460
409.960489	22295.714146	30.022477
410.313696	22331.202451	30.027495
411.031922	22371.000006	30.032512
411.243641	22399.711457	30.037530
411.629666	22433.817282	30.042548
411.646763	22472.284146	30.047565
412.820543	22507.309333	30.052583
412.693378	22531.480181	30.057600
412.944163	22564.514235	30.062618
413.568857	22606.576464	30.067636
413.825054	22652.134033	30.072653
414.140398	22684.766397	30.077671
414.771486	22721.545183	30.082688
415.005848	22760.661027	30.087706
415.415036	22797.499987	30.092724
415.921280	22839.827706	30.097741
416.381677	22877.265422	30.102759
416.645594	22913.173172	30.107776
416.958587	22941.951691	30.112794
417.271653	22988.145668	30.117812
417.665648	23024.968471	30.122829
418.485876	23064.492357	30.127847
418.473083	23112.627080	30.132864
418.852717	23152.049533	30.137882
419.682424	23192.760189	30.142900
419.744480	23230.406303	30.147917
420.335100	23268.702723	30.152935
420.615807	23307.667041	30.157952
421.534679	23346.537797	30.162970
421.937633	23386.664814	30.167988
422.156703	23413.980028	30.173005
423.133740	23439.982220	30.178023
423.331758	23478.991421	30.183040
423.595412	23508.378815	30.188058
424.102641	23535.718573	30.193076
424.299721	23575.322120	30.198093
424.911796	23607.789452	30.203111
425.110346	23648.524068	30.208128
425.492792	23682.992794	30.213146
425.979631	23713.855850	30.218164
426.293959	23754.989624	30.223181
426.974839	23786.290030	30.228199
427.214942	23820.812887	30.233216
427.851731	23861.700473	30.238234
427.945203	23893.920892	30.243252
428.288528	23943.676475	30.248269
429.298112	23972.758134	30.253287
429.393972	24013.699160	30.258304
429.582133	24049.089988	30.263322
430.294141	24080.701952	30.268340
430.904352	24121.436246	30.273357
431.596201	24159.964981	30.278375
431.689215	24201.886354	30.283392
431.913510	24243.193220	30.288410
432.816561	24272.481589	30.293428
432.838123	24311.665399	30.298445
433.717305	24345.653015	30.303463
433.587406	24387.900391	30.308480
434.267770	24434.210808	30.313498
434.782452	24466.195545	30.318516
434.908994	24510.463190	30.323533
435.404427	24546.678870	30.328551
435.729137	24584.002007	30.333568
436.136044	24627.853141	30.338586
436.741753	24671.205580	30.343604
436.971518	24725.145524	30.348621
437.819970	24755.517492	30.353639
437.941236	24804.772821	30.358656
438.366889	24843.483597	30.363674
438.999608	24892.589516	30.368692
439.131775	24935.252012	30.373709
439.678443	24983.613265	30.378727
440.073688	25033.458214	30.383744
440.472539	25060.027062	30.388762
440.897264	25109.602151	30.393780
441.255046	25157.911252	30.398797
442.033369	25201.136681	30.403815
442.729324	25238.390246	30.408832
443.064580	25284.421728	30.413850
443.682846	25327.552422	30.418868
443.910504	25380.799272	30.423885
444.519166	25411.228750	30.428903
444.892859	25450.650338	30.433920
445.442040	25488.022152	30.438938
445.863983	25527.764967	30.443956
445.884658	25580.722448	30.448973
446.565862	25614.951782	30.453991
447.146796	25650.732623	30.459008
447.432356	25696.355714	30.464026
448.263236	25740.762221	30.469044
448.580689	25783.435410	30.474061
448.540825	25815.458592	30.479079
449.090189	25851.845134	30.484096
449.895321	25901.925069	30.489114
450.325988	25931.093929	30.494132
450.574615	25978.619449	30.499149
451.028146	26013.472883	30.504167
451.390579	26049.737379	30.509184
451.637743	26093.338640	30.514202
452.362518	26128.718595	30.519220
452.762374	26172.182349	30.524237
453.252491	26199.850742	30.529255
453.773721	26251.834124	30.534272
454.449646	26281.470686	30.539290
454.632335	26323.578349	30.544308
455.057925	26364.421944	30.549325
455.641193	26401.802752	30.554343
456.166566	26439.729912	30.559360
456.308880	26480.763475	30.564378
456.934728	26514.819719	30.569396
457.144937	26565.512737	30.574413
457.720500	26606.535577	30.579431
458.297556	26648.430461	30.584448
458.453004	26693.829689	30.589466
459.152295	26732.463307	30.594484
459.169208	26783.528439	30.599501
459.718796	26817.603457	30.604519
460.220129	26868.934227	30.609536
460.721204	26918.640841	30.614554
461.366332	26956.581813	30.619572
461.216033	27011.320545	30.624589
462.127058	27053.227160	30.629607
462.417800	27097.746528	30.634624
463.021234	27154.181541	30.639642
463.351627	27202.518773	30.644660
464.075400	27263.131999	30.649677
464.446482	27302.930507	30.654695
464.913209	27349.805672	30.659712
465.005818	27412.287930	30.664730
466.162881	27441.370473	30.669748
466.436383	27494.034206	30.674765
466.975650	27545.796857	30.679783
467.647604	27590.327120	30.684800
467.617696	27635.637390	30.689818
468.586364	27679.931759	30.694836
469.215480	27735.814472	30.699853
469.603051	27782.285872	30.704871
469.869449	27820.034950	30.709888
470.510708	27857.851797	30.714906
471.030557	27901.989404	30.719924
471.640619	27939.868175	30.724941
472.065370	27994.468911	30.729959
472.612419	28028.988803	30.734976
472.355046	28077.635072	30.739994
473.140409	28126.111816	30.745012
473.619910	28172.765648	30.750029
474.215626	28221.360811	30.755047
474.998357	28271.690289	30.760064
475.272279	28313.901551	30.765082
475.878655	28347.186461	30.770100
476.251814	28395.090006	30.775117
476.565644	28439.754064	30.780135
477.251474	28478.241405	30.785152
477.434435	28536.136677	30.790170
478.276564	28571.173822	30.795188
478.844696	28620.766627	30.800205
478.753522	28660.279892	30.805223
479.692554	28698.835446	30.810240
480.037987	28745.220820	30.815258
480.275848	28796.370153	30.820276
480.845039	28845.356528	30.825293
481.226510	28891.869329	30.830311
481.704260	28936.711065	30.835328
482.098594	28973.784853	30.840346
482.481532	29018.654260	30.845364
482.917291	29065.645667	30.850381
483.635778	29110.209880	30.855399
484.176463	29147.457010	30.860416
484.665610	29202.942143	30.865434
485.147203	29242.904107	30.870452
485.571025	29278.646406	30.875469
486.242541	29332.333428	30.880487
486.427546	29363.663242	30.885504
486.629815	29420.028276	30.890522
487.327597	29471.966925	30.895540
487.806523	29516.847670	30.900557
488.167328	29565.514417	30.905575
488.846770	29605.939147	30.910592
489.280849	29654.607270	30.915610
489.837752	29704.444656	30.920628
490.351557	29758.852823	30.925645
490.340615	29809.936182	30.930663
491.430899	29856.769991	30.935680
491.751259	29915.640058	30.940698
492.170241	29961.308674	30.945716
492.756154	30007.134562	30.950733
493.054320	30066.691235	30.955751
493.939565	30102.198339	30.960768
494.309230	30163.166387	30.965786
494.888726	30208.127704	30.970804
495.463760	30255.163225	30.975821
495.904284	30311.329021	30.980839
496.545898	30349.049263	30.985856
496.770121	30404.168232	30.990874
497.819762	30446.445693	30.995892
498.094077	30502.941470	31.000909
498.188652	30554.465284	31.005927
499.080666	30603.266206	31.010944
499.691520	30647.679923	31.015962
499.999249	30689.631578	31.020980
500.259898	30746.041657	31.025997
500.793718	30793.476790	31.031015
501.347898	30845.188524	31.036032
501.970280	30899.772335	31.041050
502.549455	30951.638459	31.046068
503.267702	31004.551279	31.051085
503.705211	31062.287337	31.056103
504.218191	31088.428932	31.061120
504.178305	31145.550936	31.066138
505.008113	31197.119232	31.071156
505.590921	31241.740907	31.076173
506.264419	31298.896999	31.081191
506.659388	31347.878671	31.086208
507.351443	31397.926548	31.091226
507.687057	31441.133375	31.096244
508.229784	31486.868155	31.101261
508.515547	31547.499395	31.106279
509.205716	31582.906839	31.111296
509.597095	31648.294763	31.116314
510.278411	31694.988171	31.121332
510.646697	31741.857147	31.126349
511.033002	31795.329715	31.131367
511.563760	31841.452781	31.136384
512.299288	31894.801368	31.141402
512.887877	31947.193216	31.146420
513.520343	31994.116211	31.151437
513.688153	32042.540837	31.156455
514.480600	32093.706285	31.161472
515.218801	32138.090599	31.166490
515.201669	32191.703233	31.171508
516.110580	32240.303055	31.176525
516.181954	32280.183400	31.181543
517.036794	32321.439425	31.186560
517.338083	32365.405859	31.191578
517.544778	32409.994115	31.196596
518.449977	32452.329898	31.201613
518.892954	32505.845986	31.206631
518.870280	32547.827845	31.211648
519.566424	32596.221582	31.216666
519.852430	32647.834386	31.221684
520.252119	32707.363751	31.226701
520.784864	32751.282101	31.231719
521.669718	32819.125247	31.236736
522.287072	32865.262299	31.241754
522.790387	32919.623485	31.246772
523.153274	32962.342380	31.251789
523.776037	33018.885234	31.256807
524.364578	33073.163926	31.261824
525.079550	33129.800115	31.266842
525.480857	33189.975464	31.271860
525.803199	33238.366006	31.276877
526.211661	33296.877786	31.281895
526.998784	33338.443570	31.286912
527.542857	33396.390670	31.291930
527.974005	33448.968994	31.296948
528.652943	33507.198748	31.301965
529.408793	33563.545200	31.306983
529.687447	33608.466139	31.312000
530.345084	33672.238087	31.317018
530.508834	33720.673545	31.322036
531.305996	33781.844431	31.327053
531.644183	33833.926159	31.332071
532.458681	33894.506670	31.337088
532.410882	33950.094879	31.342106
533.162079	34020.706795	31.347124
533.895228	34062.276142	31.352141
534.696862	34128.891018	31.357159
535.133015	34183.493600	31.362176
535.823455	34235.919472	31.367194
536.321659	34282.792746	31.372212
536.582894	34341.785711	31.377229
536.990238	34411.371625	31.382247
537.940029	34460.937550	31.387264
538.367110	34519.772262	31.392282
538.757546	34578.176613	31.397300
539.476837	34629.505122	31.402317
539.887075	34686.458777	31.407335
540.561113	34741.936013	31.412352
541.132957	34794.571527	31.417370
541.784138	34850.552123	31.422388
542.170775	34912.498729	31.427405
542.818571	34967.114447	31.432423
543.308846	35023.240834	31.437440
543.988554	35078.977300	31.442458
544.575483	35131.895816	31.447476
545.196472	35182.065015	31.452493
545.503522	35241.824697	31.457511
546.098443	35290.556623	31.462528
546.604394	35339.353178	31.467546
547.264678	35407.815211	31.472564
547.822123	35453.929373	31.477581
548.079197	35511.421388	31.482599
548.963507	35570.117851	31.487616
549.562626	35624.622749	31.492634
549.803185	35680.859536	31.497652
550.448189	35736.185846	31.502669
551.010893	35793.662371	31.507687
551.540933	35843.600778	31.512704
552.187856	35896.815309	31.517722
552.371601	35948.167655	31.522740
553.049960	35992.955173	31.527757
553.848874	36046.961953	31.532775
554.163935	36102.517935	31.537792
554.786340	36158.493839	31.542810
555.460286	36212.982201	31.547828
555.843789	36255.325129	31.552845
556.295463	36313.497024	31.557863
556.844363	36368.827381	31.562880
557.763727	36420.514600	31.567898
557.643008	36477.265339	31.572916
558.623560	36526.179980	31.577933
559.149234	36586.396083	31.582951
559.375873	36634.278213	31.587968
560.158832	36701.605970	31.592986
560.258347	36764.121438	31.598004
561.197946	36819.524562	31.603021
561.701483	36889.950841	31.608039
562.097548	36950.706782	31.613056
562.725934	37006.563827	31.618074
563.160414	37067.010558	31.623092
563.651883	37130.079078	31.628109
564.341071	37204.302984	31.633127
564.747366	37269.901984	31.638144
565.253806	37336.686961	31.643162
565.948488	37406.579121	31.648180
566.810831	37463.304975	31.653197
567.189719	37532.930829	31.658215
568.105734	37596.136580	31.663232
568.166096	37657.661659	31.668250
568.905413	37727.686992	31.673268
570.053790	37794.948304	31.678285
570.484706	37857.415051	31.683303
570.645713	37916.990076	31.688320
571.468985	37979.882650	31.693338
571.815403	38052.525336	31.698356
572.706245	38108.679298	31.703373
573.236336	38174.078278	31.708391
573.601936	38238.801282	31.713408
574.336326	38305.863430	31.718426
574.901097	38370.290037	31.723444
575.352774	38430.484953	31.728461
576.060336	38504.704142	31.733479
576.474800	38569.882124	31.738496
577.902078	38635.673193	31.743514
577.988140	38700.681667	31.748532
578.679255	38753.586494	31.753549
579.197796	38813.613907	31.758567
579.587134	38883.830607	31.763584
580.468735	38940.108333	31.768602
580.736683	39012.393421	31.773620
581.522215	39074.118835	31.778637
581.917988	39134.906273	31.783655
582.455117	39206.005202	31.788672
583.331086	39266.287770	31.793690
583.929329	39333.279564	31.798708
584.653570	39386.427387	31.803725
585.015861	39455.031206	31.808743
585.842341	39514.424192	31.813760
586.012659	39569.986491	31.818778
586.508798	39634.345393	31.823796
587.330977	39707.070897	31.828813
587.931871	39767.929168	31.833831
588.434362	39834.602322	31.838848
588.984592	39894.330523	31.843866
589.311164	39963.219805	31.848884
590.013725	40013.899777	31.853901
590.724475	40093.436283	31.858919
591.055405	40155.975908	31.863936
591.749621	40212.640442	31.868954
592.048365	40282.749361	31.873972
593.159290	40338.387660	31.878989
593.881995	40407.545172	31.884007
593.926490	40466.531976	31.889024
594.843917	40520.752759	31.894042
595.391256	40597.451737	31.899060
596.032967	40649.616309	31.904077
596.218969	40711.130363	31.909095
596.766484	40780.196326	31.914112
597.866097	40848.012334	31.919130
597.981154	40908.007522	31.924148
598.971844	40978.883089	31.929165
599.356457	41050.922655	31.934183
599.840745	41119.550546	31.939200
600.854390	41182.909576	31.944218
601.019214	41250.563324	31.949236
601.860256	41319.996120	31.954253
602.350485	41396.909228	31.959271
602.800523	41456.878753	31.964288
603.395004	41531.954500	31.969306
604.186398	41604.020720	31.974324
604.805654	41670.074008	31.979341
605.253051	41745.628901	31.984359
605.974644	41816.037011	31.989376
606.888819	41885.460140	31.994394
607.199038	41965.901046	31.999412
607.710346	42028.771954	32.004429
608.155699	42098.781491	32.009447
609.018220	42176.562450	32.014464
609.875887	42258.272212	32.019482
610.544937	42322.320986	32.024500
611.145871	42383.471138	32.029517
611.776170	42465.432324	32.034535
612.248587	42535.363108	32.039552
612.526647	42589.670159	32.044570
613.490443	42673.116862	32.049588
613.859447	42753.285778	32.054605
614.583801	42829.389236	32.059623
615.361081	42894.624483	32.064640
616.272959	42968.308167	32.069658
616.633076	43046.537727	32.074676
617.217483	43109.052378	32.079693
618.098962	43180.306344	32.084711
618.407468	43261.644080	32.089728
619.334514	43325.819810	32.094746
619.806420	43410.105350	32.099764
620.409484	43479.278599	32.104781
621.106071	43545.578392	32.109799
621.379502	43619.250370	32.114816
622.090793	43683.808816	32.119834
623.023560	43761.021389	32.124852
623.434641	43838.549968	32.129869
624.218394	43911.712869	32.134887
625.040432	43989.784852	32.139904
625.621825	44052.163470	32.144922
626.738434	44116.571139	32.149940
627.026739	44185.599790	32.154957
627.421363	44254.466517	32.159975
627.717135	44325.929740	32.164992
628.505532	44388.770270	32.170010
629.071502	44468.939826	32.175028
629.831463	44538.490302	32.180045
630.902995	44609.054898	32.185063
631.444957	44696.946238	32.190080
632.050252	44751.017551	32.195098
632.535139	44814.128206	32.200116
633.251160	44872.743256	32.205133
633.946757	44933.404850	32.210151
634.418535	44997.656696	32.215168
635.083632	45059.506312	32.220186
635.518235	45129.501773	32.225204
636.244136	45185.320124	32.230221
637.151532	45256.817050	32.235239
637.631556	45332.682664	32.240256
638.599030	45386.527995	32.245274
638.767685	45449.601402	32.250292
639.364214	45512.462484	32.255309
639.800183	45576.531821	32.260327
640.360869	45657.908369	32.265344
640.792540	45718.569138	32.270362
641.623789	45797.670781	32.275380
641.907477	45871.696491	32.280397
642.552585	45953.636547	32.285415
642.834279	46028.865017	32.290432
643.626928	46105.633175	32.295450
644.597416	46193.184915	32.300468
645.108982	46277.841949	32.305485
646.167828	46349.084565	32.310503
646.667321	46436.881816	32.315520
647.749194	46506.261452	32.320538
648.079441	46583.255476	32.325556
648.923253	46657.240326	32.330573
649.646033	46725.841820	32.335591
649.908048	46814.936637	32.340608
650.910777	46891.465802	32.345626
651.686942	46967.821941	32.350644
652.268169	47043.361147	32.355661
652.972070	47119.514022	32.360679
653.757494	47193.237737	32.365696
654.323734	47265.098121	32.370714
654.809503	47337.932938	32.375732
655.403607	47421.189525	32.380749
656.230462	47487.341375	32.385767
656.973318	47575.680626	32.390784
657.683789	47652.239149	32.395802
658.276288	47729.721087	32.400820
659.069596	47797.802336	32.405837
659.823849	47877.524322	32.410855
660.248439	47960.164126	32.415872
661.283382	48030.068225	32.420890
661.940374	48099.962134	32.425908
662.300494	48174.736253	32.430925
662.957526	48248.635334	32.435943
663.379585	48322.413287	32.440960
664.345346	48414.485219	32.445978
665.055247	48480.664598	32.450996
665.902010	48554.054129	32.456013
666.653461	48633.861444	32.461031
666.870358	48714.170315	32.466048
667.544540	48782.323771	32.471066
668.468973	48860.807806	32.476084
668.616008	48945.095308	32.481101
669.493675	49015.900151	32.486119
669.922482	49098.948325	32.491136
670.944445	49179.480725	32.496154
671.499870	49263.003158	32.501172
672.281257	49340.030746	32.506189
673.037922	49411.823777	32.511207
673.460561	49491.356570	32.516224
674.275024	49574.523223	32.521242
674.950143	49652.011386	32.526260
675.363876	49731.135149	32.531277
676.723098	49802.259279	32.536295
676.797240	49882.442740	32.541312
677.408654	49958.252588	32.546330
678.363504	50028.118386	32.551348
678.946524	50097.245410	32.556365
679.922795	50161.818800	32.561383
680.345519	50244.644283	32.566400
680.982494	50307.961498	32.571418
681.635517	50370.498129	32.576436
682.284125	50453.238369	32.581453
683.086413	50536.385090	32.586471
683.783411	50611.361142	32.591488
684.298632	50686.581030	32.596506
685.058203	50758.668854	32.601524
685.390752	50847.717686	32.606541
686.185356	50928.247512	32.611559
686.955781	51001.163271	32.616576
687.268545	51083.034561	32.621594
688.196648	51162.962178	32.626612
688.605242	51248.995127	32.631629
689.482795	51336.524161	32.636647
689.820786	51426.289360	32.641664
690.490390	51521.147225	32.646682
691.681166	51604.667208	32.651700
691.998997	51685.217374	32.656717
692.805422	51777.125206	32.661735
693.739445	51860.711626	32.666752
694.167362	51959.386692	32.671770
695.099355	52044.688873	32.676788
695.752455	52132.698984	32.681805
696.670500	52214.384549	32.686823
697.162536	52302.376228	32.691840
697.848640	52394.102846	32.696858
698.638381	52483.611536	32.701876
699.440830	52573.662767	32.706893
700.175652	52662.775765	32.711911
700.501458	52752.933967	32.716928
701.540723	52836.532709	32.721946
702.261625	52921.972392	32.726964
703.190754	53010.512087	32.731981
703.811704	53091.456251	32.736999
704.462017	53182.103156	32.742016
705.263901	53275.055367	32.747034
705.954526	53359.090246	32.752052
706.397339	53449.916222	32.757069
707.315382	53533.644007	32.762087
708.061693	53624.942029	32.767104
708.577702	53713.099772	32.772122
709.369780	53808.112252	32.777140
709.812552	53887.454403	32.782157
711.011865	53979.467548	32.787175
711.799840	54068.121921	32.792192
712.523147	54158.273882	32.797210
713.267295	54239.354575	32.802228
713.783133	54331.317916	32.807245
714.395884	54415.223203	32.812263
714.991072	54508.301238	32.817280
716.137721	54604.894097	32.822298
717.063012	54683.878585	32.827316
717.294784	54759.890026	32.832333
717.974495	54857.265812	32.837351
718.759317	54938.988026	32.842368
719.455714	55036.039183	32.847386
720.167777	55116.564671	32.852404
720.934319	55209.125002	32.857421
721.391491	55293.620994	32.862439
722.248089	55376.402990	32.867456
723.188490	55475.215031	32.872474
723.817749	55554.913272	32.877492
724.128573	55657.109189	32.882509
725.003936	55738.857944	32.887527
725.959550	55831.511330	32.892544
726.982501	55913.497047	32.897562
727.681494	55993.622511	32.902580
727.976854	56069.697789	32.907597
728.986596	56145.731056	32.912615
729.806047	56230.800179	32.917632
730.183577	56321.027145	32.922650
731.032949	56393.890281	32.927668
731.575072	56483.161750	32.932685
732.064961	56571.144318	32.937703
733.048540	56657.714507	32.942720
733.439361	56751.194049	32.947738
734.314794	56838.256492	32.952756
734.737337	56941.668205	32.957773
735.102560	57023.494906	32.962791
736.434042	57134.688976	32.967808
737.315286	57237.618746	32.972826
737.827484	57320.917091	32.977844
738.566928	57424.490111	32.982861
739.230927	57512.910881	32.987879
739.828099	57613.563965	32.992896
740.616634	57720.447026	32.997914
741.475511	57819.667575	33.002932
742.168269	57921.604455	33.007949
743.409751	58015.955706	33.012967
743.945340	58116.228115	33.017984
744.421801	58212.041730	33.023002
745.186987	58316.108224	33.028020
746.199016	58417.794659	33.033037
746.913852	58516.160843	33.038055
747.806015	58617.740301	33.043072
748.719382	58712.962139	33.048090
749.667961	58802.134231	33.053108
750.516177	58903.240728	33.058125
751.226076	58999.932340	33.063143
751.698926	59084.129039	33.068160
752.730201	59189.448825	33.073178
753.461614	59282.606313	33.078196
753.864193	59379.056394	33.083213
754.688013	59485.656874	33.088231
755.683578	59571.032993	33.093248
756.432480	59680.728585	33.098266
757.141915	59773.245762	33.103284
758.157406	59870.291740	33.108301
759.002750	59963.490952	33.113319
759.664534	60051.775726	33.118336
760.250085	60151.352418	33.123354
761.157369	60245.138002	33.128372
761.987802	60350.165093	33.133389
762.321679	60449.744427	33.138407
763.242421	60542.383337	33.143424
763.751530	60637.378479	33.148442
765.008610	60734.947081	33.153460
765.383560	60832.211108	33.158477
765.969455	60933.284784	33.163495
766.853318	61032.343584	33.168512
767.764256	61139.057880	33.173530
768.622094	61227.961843	33.178548
769.500503	61328.086135	33.183565
770.144954	61437.812261	33.188583
770.956960	61540.726731	33.193600
771.414490	61632.929536	33.198618
772.713341	61732.033773	33.203636
773.288536	61836.961576	33.208653
773.986990	61933.552591	33.213671
775.058979	62032.807502	33.218688
775.636913	62123.689246	33.223706
776.351952	62215.024626	33.228724
777.055550	62304.785882	33.233741
777.532787	62400.520780	33.238759
778.694159	62477.265405	33.243776
779.277693	62572.420916	33.248794
779.999335	62670.321559	33.253812
780.738593	62771.619279	33.258829
781.223837	62871.963303	33.263847
782.362034	62959.911658	33.268864
782.830115	63057.682605	33.273882
783.743573	63154.371305	33.278900
784.408959	63254.093586	33.283917
785.049541	63360.081109	33.288935
786.372665	63457.618440	33.293952
786.905276	63565.402645	33.298970
787.728443	63664.177579	33.303988
788.916514	63761.901842	33.309005
789.537012	63872.041286	33.314023
790.045434	63959.553664	33.319040
790.783433	64069.036167	33.324058
791.807543	64171.972609	33.329076
792.622287	64280.342456	33.334093
793.130195	64381.347385	33.339111
794.346150	64487.756043	33.344128
794.999343	64592.632562	33.349146
795.698508	64700.851383	33.354164
796.952440	64799.582320	33.359181
797.382266	64908.274712	33.364199
798.615286	65005.933464	33.369216
799.147963	65114.522004	33.374234
799.816324	65220.430715	33.379252
800.752606	65325.297604	33.384269
801.459050	65432.739696	33.389287
802.335889	65547.917546	33.394304
802.994669	65647.688332	33.399322
803.889760	65754.279194	33.404340
804.888725	65851.857570	33.409357
805.733150	65967.086717	33.414375
806.664801	66063.251914	33.419392
807.129119	66175.977362	33.424410
808.104051	66277.879086	33.429428
808.689742	66377.075366	33.434445
809.698888	66486.538536	33.439463
810.457266	66594.059712	33.444480
811.269533	66711.848822	33.449498
812.003980	66818.311008	33.454516
813.083448	66925.384419	33.459533
813.787293	67036.835189	33.464551
814.839653	67128.179880	33.469568
815.401452	67235.284996	33.474586
815.925244	67339.857542	33.479604
816.700863	67467.894055	33.484621
817.566029	67581.246746	33.489639
818.531411	67684.763812	33.494656
819.224067	67792.452271	33.499674
820.282441	67898.874554	33.504692
820.887043	68013.561625	33.509709
822.373820	68140.603685	33.514727
822.971715	68239.957226	33.519744
823.601102	68347.588263	33.524762
824.649915	68444.852130	33.529780
825.458416	68547.124524	33.534797
825.930529	68663.684141	33.539815
827.101432	68771.783028	33.544832
828.027850	68881.212372	33.549850
828.580740	68986.477226	33.554868
829.289871	69090.059053	33.559885
830.081916	69209.832021	33.564903
831.208980	69304.782001	33.569920
831.971450	69400.872208	33.574938
832.699175	69502.065567	33.579956
833.340239	69596.288535	33.584973
833.900045	69712.224911	33.589991
835.127872	69812.612970	33.595008
836.197535	69912.101678	33.600026
836.606452	70014.733707	33.605044
837.483351	70120.699621	33.610061
838.287539	70235.580563	33.615079
839.461528	70331.229825	33.620096
840.324869	70439.010199	33.625114
841.246602	70548.504279	33.630132
842.029199	70651.650209	33.635149
842.228753	70769.059810	33.640167
843.143960	70874.452861	33.645184
844.410630	70978.423487	33.650202
845.471356	71089.025242	33.655220
845.982430	71198.611669	33.660237
846.743756	71310.426423	33.665255
847.691518	71418.159605	33.670272
848.637809	71524.550945	33.675290
849.538374	71633.964210	33.680308
850.256142	71736.757257	33.685325
851.130398	71862.311211	33.690343
852.101075	71967.623963	33.695360
853.084099	72086.461940	33.700378
853.784878	72196.643418	33.705396
854.376410	72307.222427	33.710413
855.275863	72427.075601	33.715431
856.320980	72545.842589	33.720448
857.055157	72658.376578	33.725466
857.999496	72780.364834	33.730484
858.869811	72897.134233	33.735501
859.328544	73011.448072	33.740519
860.561308	73127.211784	33.745536
861.885476	73239.225206	33.750554
862.419590	73362.939617	33.755572
863.591934	73473.356536	33.760589
864.512865	73596.289490	33.765607
865.239672	73701.735967	33.770624
866.122904	73813.782845	33.775642
866.736850	73935.435464	33.780660
868.136214	74050.429779	33.785677
868.624068	74160.652722	33.790695
869.502775	74277.059515	33.795712
870.426458	74394.979760	33.800730
871.173696	74518.438140	33.805748
872.282027	74626.893844	33.810765
872.870683	74745.070751	33.815783
874.075046	74868.446494	33.820800
875.280847	74985.096472	33.825818
875.610648	75088.140519	33.830836
876.945631	75201.072467	33.835853
877.221589	75319.490858	33.840871
878.004383	75425.568681	33.845888
879.125872	75546.870436	33.850906
879.929162	75668.653243	33.855924
880.574035	75781.797012	33.860941
881.625453	75907.582888	33.865959
882.610162	76017.368265	33.870976
883.395586	76149.150562	33.875994
884.177197	76282.555531	33.881012
885.494067	76394.912591	33.886029
885.855076	76511.587413	33.891047
887.087018	76627.214296	33.896064
887.777795	76741.355612	33.901082
888.555062	76869.747735	33.906100
889.777147	76975.496802	33.911117
890.646274	77091.093786	33.916135
891.281857	77203.573520	33.921152
892.548585	77309.392896	33.926170
893.860465	77423.693169	33.931188
894.479504	77520.329135	33.936205
895.319797	77631.803135	33.941223
896.119151	77746.577715	33.946240
897.234574	77853.182971	33.951258
897.379217	77950.021411	33.956276
898.710020	78065.195501	33.961293
899.584273	78188.663315	33.966311
900.541005	78301.350626	33.971328
901.139241	78417.312318	33.976346
901.946721	78541.222893	33.981364
903.072526	78651.617498	33.986381
903.890621	78778.795965	33.991399
904.391684	78898.879524	33.996416
905.471597	79014.768300	34.001434
906.182334	79144.537008	34.006452
907.384000	79263.017528	34.011469
908.199544	79406.934819	34.016487
909.067776	79527.939114	34.021504
909.794044	79645.570868	34.026522
910.451297	79777.555313	34.031540
911.825956	79901.839244	34.036557
912.573205	80040.664843	34.041575
913.820788	80162.740056	34.046592
914.411704	80293.863151	34.051610
915.107583	80434.953888	34.056628
916.349679	80559.020782	34.061645
917.341433	80697.621317	34.066663
918.170567	80826.049010	34.071680
919.014973	80957.008821	34.076698
920.011952	81087.337209	34.081716
921.278005	81216.813209	34.086733
921.970024	81350.218628	34.091751
922.878864	81489.786284	34.096768
924.112355	81607.549573	34.101786
925.348249	81741.568531	34.106804
926.119902	81872.075198	34.111821
926.999630	82003.338420	34.116839
927.805618	82127.467841	34.121856
928.920050	82255.350568	34.126874
929.485664	82386.930823	34.131892
930.978405	82523.599360	34.136909
931.754761	82659.354424	34.141927
932.809741	82784.207953	34.146944
934.218190	82912.985218	34.151962
934.643148	83040.713353	34.156980
935.673827	83160.085993	34.161997
936.499826	83288.943482	34.167015
937.422182	83418.381989	34.172032
938.715604	83536.321285	34.177050
939.231183	83673.541130	34.182068
940.521557	83806.192840	34.187085
941.611676	83928.308961	34.192103
942.199251	84059.006519	34.197120
943.189318	84184.091734	34.202138
943.848685	84311.674794	34.207156
944.731178	84444.456672	34.212173
946.018454	84579.089139	34.217191
946.729404	84699.747357	34.222208
947.864032	84831.287769	34.227226
948.484504	84965.392874	34.232244
949.225188	85093.612901	34.237261
950.484613	85229.887379	34.242279
951.410687	85357.192541	34.247296
952.058365	85479.866026	34.252314
953.099455	85612.983244	34.257332
954.312113	85727.294715	34.262349
955.210553	85854.492339	34.267367
955.927674	85982.213110	34.272384
956.746376	86104.380923	34.277402
958.042583	86244.950173	34.282420
959.122426	86358.195130	34.287437
959.854581	86488.957045	34.292455
960.733826	86618.518008	34.297472
961.907139	86739.023597	34.302490
962.830435	86877.588716	34.307508
963.758460	87008.423661	34.312525
964.809946	87136.350568	34.317543
965.636840	87269.280772	34.322560
966.599230	87399.719236	34.327578
966.990266	87540.043578	34.332596
968.293978	87670.049624	34.337613
969.421959	87809.575547	34.342631
970.122094	87955.061915	34.347648
971.282854	88085.332954	34.352666
972.074431	88231.820185	34.357684
973.515941	88370.704048	34.362701
974.295415	88500.174855	34.367719
975.085838	88650.288789	34.372736
976.379036	88788.551508	34.377754
976.983447	88935.654477	34.382772
977.912280	89076.193374	34.387789
979.284421	89218.577182	34.392807
979.903124	89355.161213	34.397824
980.943496	89506.368248	34.402842
982.064899	89655.776412	34.407860
983.185078	89791.320741	34.412877
984.363617	89930.455827	34.417895
985.317997	90082.705793	34.422912
986.132411	90221.886567	34.427930
986.921131	90369.500023	34.432948
988.026588	90507.483244	34.437965
989.355203	90646.420716	34.442983
989.931211	90796.287486	34.448000
991.201341	90947.389761	34.453018
992.279738	91095.721854	34.458036
993.514384	91234.043043	34.463053
994.399348	91373.129365	34.468071
995.376043	91515.231093	34.473088
996.619028	91664.845646	34.478106
997.885073	91806.168327	34.483124
998.480326	91945.961695	34.488141
999.594444	92084.812607	34.493159
1000.713469	92222.028376	34.498176
1001.882280	92369.249854	34.503194
1002.732764	92506.914534	34.508212
1003.734959	92638.928533	34.513229
1005.163484	92783.665137	34.518247
1006.021173	92931.014079	34.523264
1007.246033	93060.738926	34.528282
1007.548412	93201.116228	34.533300
1008.957683	93335.439696	34.538317
1009.645556	93481.284197	34.543335
1011.024945	93619.542835	34.548352
1011.810839	93757.996415	34.553370
1012.677385	93902.306593	34.558388
1013.761334	94033.350467	34.563405
1015.346398	94182.289994	34.568423
1015.510673	94324.329137	34.573440
1016.662366	94456.137391	34.578458
1017.526899	94601.084911	34.583476
1018.453816	94755.339847	34.588493
1019.889982	94882.453455	34.593511
1020.964632	95018.002774	34.598528
1021.986033	95140.175499	34.603546
1022.639818	95279.100197	34.608564
1023.678178	95413.351314	34.613581
1024.959693	95551.621210	34.618599
1025.625502	95691.014861	34.623616
1026.477210	95817.868860	34.628634
1027.362168	95959.878670	34.633652
1028.742297	96100.797511	34.638669
1029.758791	96240.607714	34.643687
1030.474650	96391.671350	34.648704
1031.329665	96532.585606	34.653722
1032.801162	96682.923874	34.658740
1033.732867	96831.205065	34.663757
1034.560828	96967.384538	34.668775
1035.792438	97112.793255	34.673792
1036.626826	97264.501683	34.678810
1037.570949	97418.069792	34.683828
1038.488188	97572.986578	34.688845
1039.823089	97717.722709	34.693863
1040.788946	97879.859106	34.698880
1041.702565	98036.033713	34.703898
1043.091959	98194.315023	34.708916
1043.926924	98341.502837	34.713933
1045.016334	98493.380021	34.718951
1046.126030	98653.266666	34.723968
1047.668472	98809.371953	34.728986
1048.685940	98967.651929	34.734004
1049.360532	99111.584989	34.739021
1050.274933	99271.872928	34.744039
1051.240034	99430.049280	34.749056
1052.305227	99582.746755	34.754074
1053.575365	99742.892597	34.759092
1054.330928	99903.715640	34.764109
1055.662413	100059.390938	34.769127
1056.402539	100230.905270	34.774144
1057.554785	100387.066598	34.779162
1058.641478	100550.135676	34.784180
1059.888466	100715.411785	34.789197
1060.953003	100879.842517	34.794215
1061.919175	101044.593749	34.799232
1063.443530	101209.638765	34.804250
1064.297257	101375.803859	34.809268
1065.137337	101535.315870	34.814285
1066.421521	101699.361340	34.819303
1067.577179	101860.435664	34.824320
1068.396626	102021.702875	34.829338
1069.840183	102177.814460	34.834356
1070.687888	102345.341988	34.839373
1072.304501	102506.550158	34.844391
1073.358932	102679.308625	34.849408
1074.637882	102825.141299	34.854426
1075.909206	102983.236172	34.859444
1076.644120	103134.404388	34.864461
1077.686059	103280.187414	34.869479
1078.548716	103441.099760	34.874496
1079.915457	103603.569556	34.879514
1081.162123	103761.621269	34.884532
1082.095275	103912.685901	34.889549
1082.542072	104069.292083	34.894567
1084.452259	104226.456003	34.899584
1085.451868	104392.943030	34.904602
1086.180779	104546.312085	34.909620
1087.543018	104717.042246	34.914637
1088.964565	104859.450709	34.919655
1089.752917	105018.201383	34.924672
1091.148209	105175.754658	34.929690
1092.329359	105310.670981	34.934708
1092.894993	105451.478827	34.939725
1094.347170	105588.167021	34.944743
1095.189154	105731.696950	34.949760
1096.268649	105874.809905	34.954778
1097.343661	106021.740816	34.959796
1097.996730	106172.136649	34.964813
1099.345385	106321.206965	34.969831
1100.190415	106478.040904	34.974848
1101.633142	106625.576211	34.979866
1102.744381	106773.633217	34.984884
1103.539925	106936.183086	34.989901
1104.490755	107094.689755	34.994919
1105.951729	107253.091929	34.999936
1106.659256	107401.684018	35.004954
1107.734278	107557.751416	35.009972
1108.534872	107732.173178	35.014989
1109.522965	107889.295488	35.020007
1110.755822	108063.346912	35.025024
1111.416588	108231.985339	35.030042
1112.832784	108409.978865	35.035060
1114.118308	108579.345421	35.040077
1115.418250	108749.129013	35.045095
1116.381125	108919.790464	35.050112
1117.818014	109099.901998	35.055130
1118.890338	109264.080666	35.060148
1119.783810	109434.286292	35.065165
1121.069757	109607.208487	35.070183
1122.344903	109781.972010	35.075200
1123.208765	109962.418626	35.080218
1124.416365	110125.692447	35.085236
1125.388443	110305.565895	35.090253
1127.026116	110482.825113	35.095271
1128.093317	110654.784848	35.100288
1129.378092	110829.311096	35.105306
1130.432523	110994.591242	35.110324
1131.549093	111174.915702	35.115341
1132.651510	111337.983301	35.120359
1133.849070	111507.707430	35.125376
1135.081043	111692.036600	35.130394
1136.006174	111862.730846	35.135412
1137.434082	112038.762446	35.140429
1138.503090	112214.115532	35.145447
1139.700702	112395.853856	35.150464
1140.897793	112571.340817	35.155482
1142.159269	112733.743065	35.160500
1143.207908	112914.632245	35.165517
1144.298533	113085.521979	35.170535
1145.831907	113257.154887	35.175552
1146.999031	113432.029272	35.180570
1147.981955	113602.075884	35.185588
1149.047465	113771.653784	35.190605
1150.043891	113944.819825	35.195623
1151.380946	114115.726551	35.200640
1152.549916	114289.564768	35.205658
1153.640410	114453.092188	35.210676
1154.967136	114639.552253	35.215693
1156.025344	114804.037515	35.220711
1157.198151	114981.442346	35.225728
1158.346067	115154.463548	35.230746
1159.609487	115327.416747	35.235764
1161.029408	115501.310185	35.240781
1162.353592	115666.303032	35.245799
1163.241217	115835.753414	35.250816
1164.206435	116010.861931	35.255834
1166.029803	116182.120656	35.260852
1166.859234	116355.324154	35.265869
1167.786863	116517.490999	35.270887
1169.057113	116673.047443	35.275904
1170.075107	116827.819580	35.280922
1171.384024	116988.216469	35.285940
1172.511659	117144.355281	35.290957
1173.770890	117301.374699	35.295975
1174.591265	117471.261585	35.300992
1175.496521	117630.950685	35.306010
1176.839768	117797.598867	35.311028
1178.004686	117957.083802	35.316045
1179.130064	118119.112433	35.321063
1180.494461	118292.114253	35.326080
1181.144508	118462.958201	35.331098
1182.435007	118642.721226	35.336116
1183.599875	118808.830975	35.341133
1185.038696	118969.393503	35.346151
1186.385487	119162.215157	35.351168
1187.548524	119335.050275	35.356186
1188.855337	119509.373135	35.361204
1189.843326	119677.074547	35.366221
1190.873317	119857.125061	35.371239
1192.099307	120035.725033	35.376256
1193.369910	120217.160257	35.381274
1194.563586	120391.606294	35.386292
1195.463967	120579.748074	35.391309
1196.665926	120766.473570	35.396327
1198.000624	120941.077588	35.401344
1199.045384	121119.216198	35.406362
1200.450092	121309.540512	35.411380
1201.439654	121491.431600	35.416397
1202.502481	121688.534477	35.421415
1204.252617	121862.075430	35.426432
1205.237444	122056.921678	35.431450
1206.366077	122235.585016	35.436468
1207.811602	122433.862211	35.441485
1209.017826	122627.712512	35.446503
1210.076894	122805.755032	35.451520
1211.262749	123000.802802	35.456538
1212.519168	123190.664663	35.461556
1213.787106	123387.617038	35.466573
1215.139306	123576.514300	35.471591
1216.527588	123756.069902	35.476608
1217.765606	123957.000485	35.481626
1219.140680	124141.076121	35.486644
1220.511625	124325.686066	35.491661
1221.774202	124518.420333	35.496679
1223.008699	124710.119638	35.501696
1224.138084	124889.657394	35.506714
1225.059723	125073.021706	35.511732
1226.053429	125268.415035	35.516749
1227.400696	125456.611431	35.521767
1228.888080	125644.215866	35.526784
1229.922918	125845.149565	35.531802
1230.884760	126029.476071	35.536820
1232.486272	126222.051171	35.541837
1233.686920	126414.486936	35.546855
1235.121658	126611.124380	35.551872
1236.081411	126811.300657	35.556890
1237.278523	127002.255344	35.561908
1238.605050	127199.407321	35.566925
1240.245456	127384.026958	35.571943
1241.420591	127582.853782	35.576960
1242.004965	127781.406103	35.581978
1243.674358	127968.776929	35.586996
1244.903616	128160.937196	35.592013
1245.675820	128361.594345	35.597031
1247.468173	128550.496392	35.602048
1248.712579	128756.727441	35.607066
1249.977829	128940.220041	35.612084
1251.045499	129122.640540	35.617101
1252.045132	129306.912195	35.622119
1253.564366	129484.150415	35.627136
1254.676757	129674.838715	35.632154
1255.710578	129855.313736	35.637172
1257.397285	130038.427913	35.642189
1258.007294	130232.293203	35.647207
1259.560274	130408.832145	35.652224
1260.519898	130607.389730	35.657242
1261.696436	130795.509987	35.662260
1263.062485	130988.422921	35.667277
1264.338991	131194.787614	35.672295
1265.542721	131381.929173	35.677312
1266.702684	131590.788221	35.682330
1267.983044	131797.243997	35.687348
1269.488476	131992.030158	35.692365
1270.446382	132194.135378	35.697383
1271.513059	132389.981703	35.702400
1272.874331	132598.192317	35.707418
1273.742420	132808.714339	35.712436
1275.488213	133018.148313	35.717453
1276.407453	133229.235332	35.722471
1278.410589	133441.257625	35.727488
1279.373890	133647.733662	35.732506
1280.994777	133872.138855	35.737524
1281.755622	134083.800360	35.742541
1283.245378	134301.997892	35.747559
1284.485494	134514.309695	35.752576
1285.788386	134726.739569	35.757594
1287.313742	134939.643197	35.762612
1288.811544	135157.336052	35.767629
1290.028978	135368.183461	35.772647
1291.331474	135579.767219	35.777664
1292.563881	135805.461069	35.782682
1293.802292	136009.696897	35.787700
1295.501819	136228.568830	35.792717
1296.782045	136443.890863	35.797735
1298.530470	136659.698970	35.802752
1299.520459	136862.086704	35.807770
1301.092575	137070.792624	35.812788
1302.447979	137282.591702	35.817805
1303.677700	137489.284639	35.822823
1305.161328	137692.994646	35.827840
1306.501612	137903.250732	35.832858
1307.738585	138112.280295	35.837876
1309.355663	138323.307120	35.842893
1310.200997	138536.676510	35.847911
1311.720447	138734.700181	35.852928
1312.964567	138941.130791	35.857946
1314.197354	139156.472813	35.862964
1315.820228	139363.772390	35.867981
1316.969317	139588.165159	35.872999
1318.551559	139790.701287	35.878016
1319.913520	140004.288314	35.883034
1321.112802	140202.380927	35.888052
1322.195206	140422.917371	35.893069
1323.480318	140636.608084	35.898087
1325.152873	140840.264008	35.903104
1326.184423	141058.400044	35.908122
1327.365137	141265.307502	35.913140
1329.017200	141473.436557	35.918157
1330.133883	141700.407866	35.923175
1331.469230	141898.536903	35.928192
1333.024795	142124.553101	35.933210
1334.224638	142337.198579	35.938228
1335.534056	142543.774030	35.943245
1336.650087	142752.766611	35.948263
1338.086754	142957.115562	35.953280
1339.552040	143157.196516	35.958298
1340.869732	143364.091391	35.963316
1342.247362	143552.714447	35.968333
1343.269163	143762.144856	35.973351
1344.514289	143957.542173	35.978368
1345.748035	144163.235092	35.983386
1346.954044	144361.571915	35.988404
1348.250791	144572.155703	35.993421
1349.475865	144787.066858	35.998439
1350.685083	144990.228597	36.003456
1351.904945	145213.874487	36.008474
1352.957637	145430.084555	36.013492
1354.458558	145645.235389	36.018509
1355.667264	145880.486602	36.023527
1356.894786	146106.534033	36.028544
1358.773830	146336.503951	36.033562
1359.984913	146550.701249	36.038580
1361.412891	146787.876913	36.043597
1362.249501	147019.218819	36.048615
1363.940164	147240.769021	36.053632
1365.428412	147481.022705	36.058650
1366.803875	147713.539912	36.063668
1368.105200	147940.662644	36.068685
1369.499399	148189.133800	36.073703
1370.828127	148411.431006	36.078720
1372.376439	148659.537540	36.083738
1373.745506	148893.761791	36.088756
1375.092045	149126.137416	36.093773
1376.491716	149375.400226	36.098791
1378.037607	149606.490114	36.103808
1379.314928	149837.876897	36.108826
1380.897822	150084.994549	36.113844
1382.298870	150315.234308	36.118861
1383.380462	150561.848706	36.123879
1384.892771	150791.768424	36.128896
1386.358585	151041.942472	36.133914
1387.939222	151283.798120	36.138932
1389.461652	151533.165850	36.143949
1390.650664	151772.990500	36.148967
1392.030355	152012.519773	36.153984
1393.536840	152258.973714	36.159002
1394.790855	152498.448585	36.164020
1396.632601	152733.630819	36.169037
1397.772456	152973.696812	36.174055
1399.446122	153210.113269	36.179072
1401.078067	153460.678385	36.184090
1402.540716	153701.522054	36.189108
1404.140880	153935.185729	36.194125
1405.196747	154175.828496	36.199143
1406.958800	154414.736876	36.204160
1408.447423	154644.638021	36.209178
1409.944336	154884.681560	36.214196
1411.508862	155121.719636	36.219213
1412.787518	155359.539701	36.224231
1414.543535	155585.695948	36.229248
1415.915826	155813.703062	36.234266
1417.100260	156049.268357	36.239284
1418.375436	156274.321924	36.244301
1419.935007	156499.890402	36.249319
1421.353689	156735.536021	36.254336
1422.920226	156971.768783	36.259354
1424.258974	157212.735224	36.264372
1425.761333	157433.542933	36.269389
1427.197844	157675.828896	36.274407
1428.802395	157899.872226	36.279424
1429.800216	158133.748441	36.284442
1431.258092	158362.653247	36.289460
1433.049765	158589.780130	36.294477
1434.417893	158813.482978	36.299495
1435.570158	159022.341632	36.304512
1436.928730	159239.357148	36.309530
1437.944919	159456.401625	36.314548
1439.527849	159677.801531	36.319565
1440.672647	159897.353797	36.324583
1442.081581	160124.406586	36.329600
1443.743110	160360.523330	36.334618
1444.554268	160588.039531	36.339636
1446.474917	160821.921122	36.344653
1447.816883	161058.966497	36.349671
1448.838175	161287.467973	36.354688
1450.786193	161528.292421	36.359706
1452.080072	161774.577777	36.364724
1453.693840	162023.276998	36.369741
1454.775002	162267.350374	36.374759
1456.185304	162507.399332	36.379776
1457.864727	162745.464573	36.384794
1459.279546	162995.049292	36.389812
1460.653535	163235.868376	36.394829
1462.387247	163486.471523	36.399847
1463.638810	163738.738105	36.404864
1464.950224	163981.156724	36.409882
1466.498857	164237.174868	36.414900
1468.189036	164491.826033	36.419917
1469.093602	164735.212503	36.424935
1470.714819	164989.139958	36.429952
1472.459836	165248.775084	36.434970
1473.681063	165528.261621	36.439988
1475.299536	165768.378636	36.445005
1476.962406	166039.050223	36.450023
1478.306261	166301.646958	36.455040
1480.091461	166553.865907	36.460058
1481.485882	166810.578094	36.465076
1483.186385	167073.731371	36.470093
1484.411953	167337.797962	36.475111
1486.033223	167593.195133	36.480128
1487.347223	167862.658714	36.485146
1489.091561	168123.548997	36.490164
1490.592308	168384.008571	36.495181
1492.133281	168642.875663	36.500199
1493.602238	168906.224337	36.505216
1495.337286	169159.971371	36.510234
1496.632075	169427.932871	36.515252
1498.344841	169690.116177	36.520269
1500.066873	169958.355575	36.525287
1501.205803	170219.310063	36.530304
1502.981256	170468.217617	36.535322
1504.405425	170742.486938	36.540340
1506.193098	170987.699365	36.545357
1507.622290	171257.576464	36.550375
1509.124984	171529.538119	36.555392
1510.692935	171776.996874	36.560410
1512.003413	172047.847684	36.565428
1513.632507	172303.183807	36.570445
1515.472024	172556.481604	36.575463
1516.944029	172825.329024	36.580480
1518.932310	173078.452871	36.585498
1520.104090	173337.724109	36.590516
1521.346191	173587.347499	36.595533
1523.338486	173852.790169	36.600551
1524.369321	174113.952613	36.605568
1526.295833	174357.211208	36.610586
1527.527840	174618.064458	36.615604
1529.001521	174875.147488	36.620621
1530.843746	175128.084856	36.625639
1532.137072	175392.613464	36.630656
1533.843736	175639.681684	36.635674
1535.047200	175890.511894	36.640692
1536.575701	176127.704826	36.645709
1538.102253	176363.222562	36.650727
1539.518570	176617.577188	36.655744
1541.245588	176858.118893	36.660762
1542.595596	177107.253639	36.665780
1544.082753	177357.459722	36.670797
1545.927154	177601.616932	36.675815
1547.021801	177847.466802	36.680832
1548.493922	178099.379014	36.685850
1549.927120	178361.507742	36.690868
1551.404953	178616.265054	36.695885
1552.710067	178877.780448	36.700903
1554.157989	179139.833014	36.705920
1555.988771	179404.112216	36.710938
1557.700480	179671.712530	36.715956
1559.020804	179941.254329	36.720973
1560.582708	180202.555646	36.725991
1561.827544	180471.856866	36.731008
1563.608334	180747.500677	36.736026
1565.386609	181020.453523	36.741044
1566.987054	181294.857302	36.746061
1568.243022	181581.202138	36.751079
1570.194348	181857.228939	36.756096
1571.464567	182125.464277	36.761114
1573.124663	182408.243421	36.766132
1574.794327	182696.482576	36.771149
1576.660343	182973.897494	36.776167
1578.128549	183251.807247	36.781184
1579.819664	183533.873689	36.786202
1580.927357	183813.974955	36.791220
1582.777101	184098.202487	36.796237
1584.612426	184381.569529	36.801255
1585.696675	184698.708549	36.806272
1587.642019	185025.009856	36.811290
1588.900829	185318.045206	36.816308
1590.644820	185603.614298	36.821325
1592.373241	185881.566842	36.826343
1593.828419	186186.232196	36.831360
1595.732065	186468.527572	36.836378
1597.054444	186755.232587	36.841396
1598.859386	187050.955892	36.846413
1600.577932	187344.940965	36.851431
1602.288218	187635.651575	36.856448
1603.773291	187916.898705	36.861466
1605.387187	188206.051141	36.866484
1606.750185	188507.359346	36.871501
1608.854719	188797.655739	36.876519
1610.142041	189094.329184	36.881536
1612.065856	189388.795591	36.886554
1613.396872	189681.755326	36.891572
1614.444057	189975.115831	36.896589
1616.610044	190272.442233	36.901607
1618.220521	190573.412380	36.906624
1620.238269	190862.965577	36.911642
1621.755056	191155.671339	36.916660
1623.200312	191452.224493	36.921677
1625.149624	191750.731538	36.926695
1626.735391	192047.822972	36.931712
1628.345386	192335.716275	36.936730
1629.893117	192630.046387	36.941748
1631.564686	192926.339076	36.946765
1633.438034	193218.308133	36.951783
1634.655157	193516.502188	36.956800
1636.376614	193801.917502	36.961818
1638.168811	194101.089751	36.966836
1639.841369	194398.147714	36.971853
1641.555841	194679.959078	36.976871
1642.884372	194964.549368	36.981888
1645.020278	195227.448219	36.986906
1646.615341	195506.308052	36.991924
1648.284618	195770.424036	36.996941
1650.082349	196036.349325	37.001959
1651.137028	196323.373029	37.006976
1653.057210	196600.990310	37.011994
1654.471530	196872.413108	37.017012
1656.189335	197140.943943	37.022029
1657.793230	197427.350478	37.027047
1659.215946	197714.827399	37.032064
1660.565540	197994.644985	37.037082
1662.113367	198297.979561	37.042100
1663.835829	198592.701583	37.047117
1665.864595	198888.417717	37.052135
1667.217612	199186.069110	37.057152
1669.060989	199484.406391	37.062170
1670.217086	199785.290389	37.067188
1671.431638	200082.253879	37.072205
1673.890852	200388.701353	37.077223
1675.199906	200706.709585	37.082240
1676.768143	201007.861571	37.087258
1678.613064	201324.008959	37.092276
1680.309970	201644.295279	37.097293
1681.959790	201954.860443	37.102311
1683.100790	202274.904690	37.107328
1685.184551	202595.614857	37.112346
1686.984260	202917.843396	37.117364
1688.436612	203244.851742	37.122381
1690.604898	203569.995845	37.127399
1692.123142	203890.339524	37.132416
1694.083322	204207.439243	37.137434
1695.771528	204537.664459	37.142452
1697.498623	204857.850041	37.147469
1699.212043	205165.743305	37.152487
1700.668101	205507.971187	37.157504
1702.362200	205826.969526	37.162522
1704.096887	206158.841294	37.167540
1705.990641	206491.755611	37.172557
1707.862693	206811.616678	37.177575
1709.382741	207143.752167	37.182592
1711.368237	207466.670192	37.187610
1713.219666	207789.508041	37.192628
1714.803241	208122.778150	37.197645
1716.863907	208453.763986	37.202663
1718.418151	208780.206135	37.207680
1720.343957	209103.237337	37.212698
1721.982414	209437.288148	37.217716
1723.473258	209762.953987	37.222733
1725.677895	210090.871042	37.227751
1727.421351	210419.038491	37.232768
1729.032207	210749.767426	37.237786
1731.019180	211069.743035	37.242804
1732.806854	211396.710745	37.247821
1734.548602	211709.460037	37.252839
1736.363766	212040.183873	37.257856
1737.967533	212373.176660	37.262874
1739.881540	212689.177050	37.267892
1741.783348	213006.322820	37.272909
1743.389873	213329.586572	37.277927
1745.120562	213659.918824	37.282944
1747.043157	213980.466338	37.287962
1748.751415	214302.673515	37.292980
1750.784315	214616.650167	37.297997
1752.532844	214939.486680	37.303015
1754.118334	215252.822555	37.308032
1755.969909	215566.777532	37.313050
1757.724700	215880.646273	37.318068
1758.983563	216186.870083	37.323085
1760.986618	216481.825357	37.328103
1762.294967	216787.482941	37.333120
1764.002143	217085.838204	37.338138
1766.036613	217399.181534	37.343156
1767.184489	217708.776994	37.348173
1769.454049	218014.920000	37.353191
1771.555888	218327.389596	37.358208
1772.867043	218637.950771	37.363226
1774.393169	218939.663289	37.368244
1776.118483	219259.356197	37.373261
1777.941822	219575.883822	37.378279
1779.786698	219901.579060	37.383296
1781.234280	220228.047921	37.388314
1782.794824	220545.201366	37.393332
1784.226143	220884.832310	37.398349
1786.640815	221206.653695	37.403367
1788.402430	221555.810511	37.408384
1789.894642	221882.044332	37.413402
1791.604152	222209.489038	37.418420
1793.353964	222557.326982	37.423437
1795.542322	222899.253446	37.428455
1797.202030	223237.096435	37.433472
1798.896591	223579.913226	37.438490
1801.032152	223929.189907	37.443508
1802.652661	224285.990622	37.448525
1804.314859	224629.777953	37.453543
1806.612568	224970.315750	37.458560
1808.094077	225319.135988	37.463578
1810.047831	225665.037070	37.468596
1811.645808	226020.469538	37.473613
1813.953840	226366.010300	37.478631
1815.595540	226723.823854	37.483648
1817.255671	227085.800748	37.488666
1819.145277	227429.018874	37.493684
1821.156752	227784.437225	37.498701
1822.703348	228140.131475	37.503719
1824.673586	228492.660051	37.508736
1826.714000	228855.491592	37.513754
1828.687993	229198.873917	37.518772
1830.329906	229566.035457	37.523789
1832.468154	229927.530306	37.528807
1834.146503	230278.859155	37.533824
1836.068288	230636.195912	37.538842
1838.095889	230987.800047	37.543860
1839.711200	231346.200576	37.548877
1842.031945	231702.864678	37.553895
1843.978253	232062.254584	37.558912
1845.525789	232423.383334	37.563930
1847.711581	232760.938769	37.568948
1849.655871	233119.744038	37.573965
1851.189458	233475.641072	37.578983
1853.539694	233823.687292	37.584000
1855.114053	234187.884490	37.589018
1857.115915	234532.275735	37.594036
1858.892664	234889.708683	37.599053
1860.864605	235238.778347	37.604071
1862.813320	235594.634153	37.609088
1864.810695	235955.511964	37.614106
1867.183358	236288.412034	37.619124
1868.556686	236641.841934	37.624141
1870.619239	236980.404112	37.629159
1872.392370	237330.239657	37.634176
1873.977075	237684.448342	37.639194
1876.152386	238028.555221	37.644212
1878.067715	238379.002491	37.649229
1879.337006	238725.282664	37.654247
1881.407101	239060.234196	37.659264
1883.399817	239400.201940	37.664282
1885.001303	239724.073914	37.669300
1886.738689	240057.196498	37.674317
1888.734487	240398.026276	37.679335
1890.655417	240734.955223	37.684352
1892.186052	241067.270602	37.689370
1893.771782	241405.114849	37.694388
1895.614229	241753.638644	37.699405
1897.052805	242102.656999	37.704423
1899.312869	242455.687030	37.709440
1900.863184	242806.211069	37.714458
1903.207168	243173.249421	37.719476
1904.788146	243532.455415	37.724493
1906.246241	243893.102630	37.729511
1908.475120	244246.134770	37.734528
1909.925232	244620.220197	37.739546
1911.993384	245000.355754	37.744564
1913.852010	245372.597713	37.749581
1915.981268	245749.343744	37.754599
1917.648099	246117.549891	37.759616
1919.734057	246516.655642	37.764634
1921.791760	246891.581679	37.769652
1923.464425	247284.501442	37.774669
1925.541920	247667.424641	37.779687
1927.433447	248046.260933	37.784704
1929.212545	248445.334344	37.789722
1931.576161	248833.011342	37.794740
1933.295814	249229.298005	37.799757
1934.652653	249617.206971	37.804775
1937.465545	250008.062488	37.809792
1939.430791	250412.436628	37.814810
1941.138967	250802.472419	37.819828
1943.360796	251200.707941	37.824845
1945.110646	251606.789297	37.829863
1947.492805	251991.915721	37.834880
1949.021983	252405.878675	37.839898
1951.476533	252795.310038	37.844916
1953.281009	253195.078966	37.849933
1955.131042	253588.413069	37.854951
1957.701356	253997.382346	37.859968
1959.224150	254391.908513	37.864986
1961.658202	254786.773616	37.870004
1963.419015	255188.575883	37.875021
1965.431167	255578.754679	37.880039
1967.734848	255982.755764	37.885056
1969.365749	256385.819444	37.890074
1971.737164	256779.266047	37.895092
1973.752146	257176.069346	37.900109
1975.781837	257572.869112	37.905127
1977.852571	257963.209418	37.910144
1979.203889	258366.336008	37.915162
1981.384337	258762.778198	37.920180
1983.846382	259169.208244	37.925197
1986.101143	259561.394308	37.930215
1988.099613	259949.656726	37.935232
1990.029924	260345.142203	37.940250
1991.984292	260727.973284	37.945268
1994.449025	261117.657466	37.950285
1996.200575	261508.417100	37.955303
1998.302785	261901.076309	37.960320
2000.218245	262296.684333	37.965338
2002.469202	262675.728617	37.970356
2004.454295	263066.928815	37.975373
2006.455142	263464.246425	37.980391
2008.132272	263839.083883	37.985408
2009.910928	264231.201103	37.990426
2012.156588	264617.630548	37.995444
2014.401653	265002.280705	38.000461
2016.264231	265377.870993	38.005479
2018.229542	265735.080347	38.010496
2020.239032	266103.330050	38.015514
2022.390538	266468.813104	38.020532
2024.169771	266837.604092	38.025549
2025.918310	267205.179363	38.030567
2027.835132	267577.933616	38.035584
2029.421636	267959.475168	38.040602
2031.926376	268336.274436	38.045620
2033.678302	268709.761230	38.050637
2035.712429	269103.393892	38.055655
2037.862787	269488.828546	38.060672
2039.668340	269872.690072	38.065690
2041.247689	270254.502760	38.070708
2043.555876	270651.895582	38.075725
2044.935628	271052.784389	38.080743
2047.169730	271460.623615	38.085760
2049.251044	271865.614965	38.090778
2051.305786	272275.408675	38.095796
2053.357045	272683.143831	38.100813
2055.274146	273108.650533	38.105831
2057.517701	273523.335774	38.110848
2059.625607	273942.789392	38.115866
2061.716622	274356.757891	38.120884
2063.345513	274782.479006	38.125901
2065.478028	275216.372939	38.130919
2067.748420	275629.062564	38.135936
2069.705502	276074.306076	38.140954
2072.053660	276492.312292	38.145972
2074.338625	276925.284326	38.150989
2076.202539	277358.243676	38.156007
2078.385269	277789.246091	38.161024
2080.769642	278232.277369	38.166042
2082.739988	278661.225735	38.171060
2084.779631	279090.770334	38.176077
2086.703126	279527.085726	38.181095
2089.043253	279962.901693	38.186112
2091.299318	280403.553248	38.191130
2093.432045	280828.629259	38.196148
2095.766910	281258.292956	38.201165
2097.509680	281701.073975	38.206183
2099.893478	282131.943766	38.211200
2101.843555	282573.341107	38.216218
2104.172860	283012.619490	38.221236
2106.364920	283451.154808	38.226253
2108.163292	283893.583380	38.231271
2110.976305	284325.921642	38.236288
2112.960067	284755.517514	38.241306
2115.001932	285198.610644	38.246324
2117.135957	285631.173868	38.251341
2119.329880	286072.358438	38.256359
2121.612460	286504.410353	38.261376
2123.638941	286937.413656	38.266394
2125.783796	287371.436681	38.271412
2128.156544	287812.632494	38.276429
2130.463480	288251.093308	38.281447
2132.624409	288675.176968	38.286464
2134.982269	289125.151660	38.291482
2136.880917	289549.169006	38.296500
2139.301024	289984.121664	38.301517
2141.550667	290419.021817	38.306535
2143.655800	290830.912173	38.311552
2145.980161	291265.617002	38.316570
2148.060949	291693.450699	38.321588
2150.647883	292112.772686	38.326605
2152.235883	292540.702948	38.331623
2154.237152	292950.919595	38.336640
2156.286408	293378.898712	38.341658
2158.658259	293781.637928	38.346676
2161.146903	294176.510846	38.351693
2162.768920	294570.323418	38.356711
2164.753834	294978.472137	38.361728
2166.736562	295373.746225	38.366746
2168.792007	295778.400047	38.371764
2170.785646	296193.012981	38.376781
2172.803629	296615.184819	38.381799
2175.046761	297028.508654	38.386816
2176.913216	297451.637362	38.391834
2178.834562	297871.809341	38.396852
2181.136679	298298.316261	38.401869
2183.159226	298733.216085	38.406887
2185.193406	299165.648132	38.411904
2187.688449	299599.045556	38.416922
2189.659789	300036.202557	38.421940
2192.057574	300474.000164	38.426957
2193.990147	300932.150662	38.431975
2196.284346	301372.724300	38.436992
2198.648501	301814.400350	38.442010
2200.614215	302267.380916	38.447028
2203.241915	302707.002846	38.452045
2205.334938	303165.337506	38.457063
2207.649157	303629.294404	38.462080
2209.815395	304087.457202	38.467098
2211.703461	304544.212542	38.472116
2213.743836	304989.999354	38.477133
2215.559833	305460.389191	38.482151
2218.395776	305934.981139	38.487168
2220.897667	306401.447364	38.492186
2223.160276	306868.276675	38.497204
2225.735272	307331.372198	38.502221
2227.714149	307805.775905	38.507239
2230.081572	308279.378175	38.512256
2232.512714	308748.422457	38.517274
2234.471009	309215.708688	38.522292
2236.810779	309682.956128	38.527309
2239.036714	310156.511511	38.532327
2241.059804	310626.261361	38.537344
2243.789729	311103.078889	38.542362
2245.950050	311583.483303	38.547380
2248.386171	312052.088436	38.552397
2250.488822	312541.552995	38.557415
2252.603938	313005.275010	38.562432
2255.166748	313481.485407	38.567450
2257.514606	313975.490257	38.572468
2259.251162	314443.495451	38.577485
2261.735647	314922.571032	38.582503
2264.460003	315395.589257	38.587520
2266.694689	315879.160479	38.592538
2269.069947	316367.983193	38.597556
2271.386728	316836.710331	38.602573
2273.689717	317319.671602	38.607591
2275.710046	317784.070140	38.612608
2278.330925	318277.604362	38.617626
2280.699559	318757.062925	38.622644
2282.951045	319227.779601	38.627661
2285.130863	319716.443459	38.632679
2287.151172	320180.283566	38.637696
2289.752852	320654.152658	38.642714
2291.730358	321131.463700	38.647732
2294.259757	321611.169819	38.652749
2296.362105	322095.428663	38.657767
2298.717698	322578.525834	38.662784
2301.070902	323057.811651	38.667802
2303.596700	323535.035029	38.672820
2305.674408	324009.963248	38.677837
2308.411135	324488.563556	38.682855
2310.473019	324934.253337	38.687872
2312.640694	325390.781315	38.692890
2314.980772	325841.745968	38.697908
2317.920998	326287.867088	38.702925
2319.910605	326741.616734	38.707943
2322.020774	327184.457898	38.712960
2324.099803	327643.333810	38.717978
2326.357369	328091.317626	38.722996
2328.649650	328558.623578	38.728013
2330.777557	329022.879860	38.733031
2333.128319	329483.670798	38.738048
2335.450568	329951.361402	38.743066
2337.375561	330427.429784	38.748084
2339.682852	330894.426382	38.753101
2342.116858	331380.652623	38.758119
2344.435320	331858.747410	38.763136
2346.834019	332348.214083	38.768154
2348.683372	332839.079529	38.773172
2351.210040	333328.894052	38.778189
2353.987888	333819.677611	38.783207
2355.978774	334308.472379	38.788224
2358.600067	334807.435675	38.793242
2360.985869	335305.338351	38.798260
2363.060877	335800.010718	38.803277
2365.481347	336306.595029	38.808295
2367.712975	336803.613763	38.813312
2370.222176	337311.159529	38.818330
2372.407662	337835.667078	38.823348
2375.249380	338341.751338	38.828365
2377.763981	338856.021479	38.833383
2379.565921	339367.073085	38.838400
2382.380651	339881.484433	38.843418
2384.543664	340406.668030	38.848436
2387.290700	340925.919100	38.853453
2389.484234	341452.071490	38.858471
2391.840379	341975.933347	38.863488
2394.796326	342489.193917	38.868506
2396.550489	343019.119503	38.873524
2399.311263	343538.101268	38.878541
2401.941397	344064.374008	38.883559
2404.076983	344596.853087	38.888576
2406.604590	345115.365581	38.893594
2409.338192	345636.627423	38.898612
2411.635395	346173.722542	38.903629
2414.297489	346694.446683	38.908647
2416.436164	347233.603657	38.913664
2419.452451	347753.393730	38.918682
2421.877115	348283.436364	38.923700
2424.012647	348797.033936	38.928717
2426.471667	349330.350736	38.933735
2429.350526	349859.536261	38.938752
2431.844068	350379.366631	38.943770
2434.137212	350910.452284	38.948788
2436.502199	351431.249392	38.953805
2438.913588	351959.738484	38.958823
2441.408637	352487.216994	38.963840
2444.226319	353010.224855	38.968858
2446.882677	353542.528511	38.973876
2449.076131	354056.920734	38.978893
2451.592526	354582.687839	38.983911
2453.596997	355106.295280	38.988928
2456.409777	355624.773345	38.993946
2459.179748	356158.814860	38.998964
2461.490681	356673.221776	39.003981
2463.576082	357198.860079	39.008999
2466.290879	357731.767667	39.014016
2469.142747	358249.536526	39.019034
2471.466274	358759.800014	39.024052
2473.888745	359260.153671	39.029069
2476.553244	359740.689933	39.034087
2478.711327	360221.779363	39.039104
2481.090421	360709.492796	39.044122
2483.549527	361203.522429	39.049140
2486.474132	361695.874277	39.054157
2488.529162	362184.121257	39.059175
2490.491766	362678.863064	39.064192
2493.295178	363173.059561	39.069210
2495.795976	363674.112758	39.074228
2497.825825	364178.297691	39.079245
2500.515989	364688.757233	39.084263
2502.590594	365196.212249	39.089280
2505.411703	365714.286933	39.094298
2507.460700	366247.957203	39.099316
2510.181242	366762.911701	39.104333
2512.576735	367289.691506	39.109351
2514.877460	367824.180043	39.114368
2517.599393	368345.238301	39.119386
2520.059322	368881.937344	39.124404
2522.430208	369419.222934	39.129421
2525.210422	369962.540929	39.134439
2527.291180	370508.516986	39.139456
2530.113420	371051.959303	39.144474
2532.482948	371613.020655	39.149492
2534.902082	372168.488783	39.154509
2537.658937	372725.995844	39.159527
2539.843317	373283.327795	39.164544
2542.734515	373839.119087	39.169562
2544.800232	374411.267817	39.174580
2547.237760	374976.202093	39.179597
2550.206670	375552.669686	39.184615
2552.662661	376118.945236	39.189632
2555.620940	376697.796654	39.194650
2558.248894	377274.635327	39.199668
2560.801397	377842.176639	39.204685
2563.541961	378414.008037	39.209703
2565.972402	379000.567289	39.214720
2568.713286	379563.254802	39.219738
2571.068570	380154.714122	39.224756
2573.726192	380736.791795	39.229773
2576.649087	381310.861918	39.234791
2578.833768	381885.034822	39.239808
2581.613747	382467.839754	39.244826
2584.342657	383061.023395	39.249844
2587.216833	383640.165363	39.254861
2589.793886	384224.431108	39.259879
2592.601634	384813.560405	39.264896
2594.797100	385393.427168	39.269914
2597.212530	385975.348115	39.274932
2599.822570	386562.391109	39.279949
2603.400393	387151.548051	39.284967
2605.458412	387737.079904	39.289984
2608.164618	388321.812967	39.295002
2611.057233	388908.174288	39.300020
2613.529302	389479.522045	39.305037
2616.270115	390068.082448	39.310055
2619.095303	390650.032656	39.315072
2621.842678	391227.373283	39.320090
2624.488156	391803.197134	39.325108
2626.478129	392400.528139	39.330125
2629.451949	392975.007003	39.335143
2632.303187	393559.010144	39.340160
2634.545686	394136.816141	39.345178
2637.167683	394727.915001	39.350196
2639.580296	395311.437791	39.355213
2642.588115	395891.157443	39.360231
2645.283059	396466.608697	39.365248
2648.189351	397020.750668	39.370266
2650.889464	397573.899397	39.375284
2653.402333	398119.369847	39.380301
2656.059911	398651.997890	39.385319
2658.665547	399198.441085	39.390336
2661.191266	399750.502604	39.395354
2663.405687	400308.926834	39.400372
2665.656793	400856.449398	39.405389
2668.632002	401417.309261	39.410407
2671.502509	401981.360467	39.415424
2674.057749	402542.359735	39.420442
2676.593353	403111.496678	39.425460
2679.086635	403690.798578	39.430477
2681.533681	404263.817463	39.435495
2684.195871	404847.871159	39.440512
2686.998425	405436.492902	39.445530
2689.944495	406032.060200	39.450548
2692.504931	406615.274177	39.455565
2695.207555	407205.484336	39.460583
2697.776950	407806.477577	39.465600
2700.746219	408405.418618	39.470618
2703.202288	408995.670265	39.475636
2705.573871	409607.574564	39.480653
2708.620216	410201.749218	39.485671
2711.432928	410812.437783	39.490688
2714.401393	411417.772702	39.495706
2716.937689	412030.898728	39.500724
2719.617041	412652.787563	39.505741
2722.779087	413263.150131	39.510759
2725.512028	413866.480382	39.515776
2727.959496	414483.293911	39.520794
2730.847354	415093.444903	39.525812
2733.425897	415724.871258	39.530829
2736.334735	416343.531455	39.535847
2739.008792	416961.856223	39.540864
2742.049750	417589.614067	39.545882
2744.849388	418221.436981	39.550900
2747.536789	418834.141206	39.555917
2750.434836	419465.304251	39.560935
2753.090651	420093.654027	39.565952
2755.825407	420726.372009	39.570970
2758.729443	421353.633328	39.575988
2761.356554	421991.942439	39.581005
2764.091038	422614.185711	39.586023
2767.049473	423247.397950	39.591040
2769.829535	423883.601598	39.596058
2772.884350	424525.455722	39.601076
2775.374800	425146.092430	39.606093
2778.317703	425786.457843	39.611111
2781.100858	426421.165620	39.616128
2784.039256	427061.187798	39.621146
2786.803685	427683.219969	39.626164
2789.360856	428328.670289	39.631181
2792.578622	428965.352401	39.636199
2795.191176	429608.629361	39.641216
2798.083633	430249.920847	39.646234
2800.985630	430889.572530	39.651252
2803.344952	431526.912719	39.656269
2806.298509	432169.446042	39.661287
2809.420800	432805.108972	39.666304
2812.108869	433449.663144	39.671322
2814.965879	434088.661017	39.676340
2817.567138	434736.976094	39.681357
2820.441124	435376.029729	39.686375
2823.024498	436019.503743	39.691392
2825.932687	436664.067503	39.696410
2829.038598	437303.677376	39.701428
2831.558073	437945.934269	39.706445
2834.769840	438552.744638	39.711463
2837.412311	439158.260437	39.716480
2840.342397	439766.439947	39.721498
2843.419883	440367.958667	39.726516
2845.494689	440978.556540	39.731533
2848.476237	441592.528801	39.736551
2851.138254	442207.945201	39.741568
2854.095438	442821.375567	39.746586
2856.960627	443440.154185	39.751604
2859.212929	444057.038043	39.756621
2862.631422	444686.951907	39.761639
2865.172749	445321.173324	39.766656
2868.218578	445959.081695	39.771674
2870.728880	446590.435689	39.776692
2873.322521	447233.066912	39.781709
2876.325683	447878.489774	39.786727
2879.200587	448541.028175	39.791744
2881.880699	449190.595427	39.796762
2884.663946	449842.243809	39.801780
2887.318036	450511.914186	39.806797
2890.323338	451186.503023	39.811815
2893.248528	451852.193010	39.816832
2895.941833	452529.607021	39.821850
2898.944675	453205.937041	39.826868
2901.472109	453895.895130	39.831885
2904.319188	454583.656035	39.836903
2907.070633	455277.916591	39.841920
2910.317251	455979.996877	39.846938
2913.386533	456667.136355	39.851956
2916.205010	457376.899289	39.856973
2919.369240	458077.444056	39.861991
2922.214406	458785.227192	39.867008
2925.133088	459497.965843	39.872026
2928.224997	460195.912456	39.877044
2931.126557	460923.128029	39.882061
2934.176050	461635.807651	39.887079
2937.248745	462349.059267	39.892096
2940.305718	463073.030263	39.897114
2943.291314	463783.611388	39.902132
2946.552380	464511.928592	39.907149
2949.533642	465209.686112	39.912167
2952.660434	465928.125318	39.917184
2955.771259	466662.980936	39.922202
2958.821294	467371.079313	39.927220
2962.041760	468082.197654	39.932237
2965.270861	468786.575844	39.937255
2967.516617	469497.483037	39.942272
2970.642785	470222.141453	39.947290
2973.917787	470936.607891	39.952308
2976.769281	471663.010550	39.957325
2980.395834	472367.424852	39.962343
2983.517306	473079.350414	39.967360
2986.210965	473800.488440	39.972378
2989.640312	474504.638917	39.977396
2992.559001	475215.241515	39.982413
2995.968143	475919.232345	39.987431
2998.774252	476620.765828	39.992448
3001.882037	477316.424008	39.997466
3004.704897	478033.268117	40.002484
3007.854955	478732.285509	40.007501
3010.715475	479435.652078	40.012519
3013.956883	480138.877328	40.017536
3016.731475	480833.676928	40.022554
3019.756034	481532.287299	40.027572
3023.115358	482247.495038	40.032589
3025.700380	482953.518703	40.037607
3028.925904	483647.366736	40.042624
3031.839065	484336.445639	40.047642
3034.765566	485002.414735	40.052660
3037.795903	485670.102293	40.057677
3040.797766	486329.704172	40.062695
3044.065925	486999.614336	40.067712
3046.689294	487672.114880	40.072730
3049.701670	488335.306236	40.077748
3052.696284	489002.853957	40.082765
3055.313135	489672.144011	40.087783
3058.071293	490352.463550	40.092800
3061.019685	491046.724611	40.097818
3064.176968	491729.790501	40.102836
3067.059342	492430.343912	40.107853
3069.969363	493133.025699	40.112871
3072.880920	493841.414913	40.117888
3075.833672	494563.057660	40.122906
3078.781140	495269.308721	40.127924
3081.605355	495998.051796	40.132941
3084.754902	496727.715006	40.137959
3087.931673	497459.502648	40.142976
3090.837557	498192.856806	40.147994
3093.848377	498933.608143	40.153012
3097.212640	499679.048694	40.158029
3100.278918	500418.558195	40.163047
3103.201435	501172.044852	40.168064
3105.941297	501926.930100	40.173082
3109.378307	502695.003497	40.178100
3112.428704	503451.924425	40.183117
3115.289462	504225.944402	40.188135
3118.712716	505007.986218	40.193152
3121.919587	505785.037754	40.198170
3125.174291	506554.291167	40.203188
3128.083928	507335.228871	40.208205
3131.360334	508123.863829	40.213223
3134.767148	508901.166046	40.218240
3137.582602	509691.797528	40.223258
3141.046860	510485.653069	40.228276
3144.373814	511270.984950	40.233293
3147.584174	512065.444267	40.238311
3150.974860	512853.895722	40.243328
3154.419473	513640.634427	40.248346
3157.470888	514418.791131	40.253364
3160.471980	515219.488444	40.258381
3163.429856	516012.000683	40.263399
3166.911099	516817.205719	40.268416
3170.175514	517606.913080	40.273434
3173.474213	518399.434747	40.278452
3176.835464	519191.246956	40.283469
3180.006498	519999.479124	40.288487
3183.632650	520784.923904	40.293504
3186.694939	521585.790177	40.298522
3189.828745	522379.310507	40.303540
3193.056667	523168.095658	40.308557
3196.422048	523964.551205	40.313575
3199.866472	524744.717151	40.318592
3202.760521	525544.518371	40.323610
3206.357419	526331.149136	40.328628
3209.537321	527127.041998	40.333645
3212.264528	527921.852426	40.338663
3215.741421	528700.272806	40.343680
3219.096166	529498.857936	40.348698
3222.326513	530281.241131	40.353716
3225.397982	531072.039594	40.358733
3228.547364	531868.804110	40.363751
3231.972913	532655.784745	40.368768
3235.011271	533454.025788	40.373786
3238.697447	534245.940298	40.378804
3242.133702	535033.627724	40.383821
3244.908163	535810.576387	40.388839
3248.131738	536566.574238	40.393856
3251.526782	537325.763363	40.398874
3254.261763	538068.947968	40.403892
3257.706788	538820.560922	40.408909
3261.063723	539569.382626	40.413927
3263.976058	540322.445087	40.418944
3266.768534	541087.525239	40.423962
3270.557785	541841.513898	40.428980
3273.356063	542606.500555	40.433997
3276.810957	543372.140540	40.439015
3279.839196	544149.540209	40.444032
3282.904285	544926.383860	40.449050
3285.865694	545711.572566	40.454068
3289.269967	546505.019163	40.459085
3292.401176	547302.118986	40.464103
3295.707822	548088.456787	40.469120
3298.920418	548896.925948	40.474138
3301.947416	549704.518234	40.479156
3305.227812	550510.663598	40.484173
3308.722437	551336.327482	40.489191
3311.769522	552152.779799	40.494208
3315.067698	552981.120063	40.499226
3318.587695	553824.257857	40.504244
3321.647015	554653.974445	40.509261
3325.261878	555497.230840	40.514279
3328.317562	556334.450720	40.519296
3331.626604	557182.548036	40.524314
3334.592982	558028.132912	40.529332
3338.047560	558897.634151	40.534349
3341.828955	559759.003521	40.539367
3345.319693	560617.349414	40.544384
3348.195801	561486.500207	40.549402
3352.088149	562351.670748	40.554420
3355.700761	563214.567062	40.559437
3358.937316	564086.875026	40.564455
3362.815274	564949.100814	40.569472
3366.131125	565824.872274	40.574490
3369.222039	566680.031273	40.579508
3373.000566	567541.478981	40.584525
3376.456125	568427.897378	40.589543
3380.289590	569292.860578	40.594560
3383.760696	570164.122977	40.599578
3386.909129	571022.304409	40.604596
3390.529963	571883.200545	40.609613
3393.957603	572765.233001	40.614631
3397.444687	573626.818790	40.619648
3401.284481	574496.540886	40.624666
3404.890052	575359.827654	40.629684
3408.382686	576222.915794	40.634701
3411.995159	577091.822531	40.639719
3415.461420	577942.674967	40.644736
3418.995873	578799.104584	40.649754
3422.119731	579649.380175	40.654772
3425.900691	580511.641806	40.659789
3429.009346	581369.940531	40.664807
3432.725709	582218.976206	40.669824
3436.192390	583074.136045	40.674842
3439.450850	583940.361982	40.679860
3442.983838	584788.478005	40.684877
3446.198406	585658.324724	40.689895
3449.873838	586495.937590	40.694912
3453.127835	587356.794689	40.699930
3456.638135	588223.841031	40.704948
3459.819107	589077.825603	40.709965
3463.269781	589942.544565	40.714983
3466.753317	590813.035327	40.720000
3470.086728	591672.337003	40.725018
3473.487403	592511.006757	40.730023
3476.819829	593320.233085	40.735028
3479.737031	594091.802176	40.740032
3482.766749	594803.355092	40.745037
3485.753959	595471.753015	40.750042
3488.185762	596088.722250	40.755047
3491.255312	596663.297862	40.760052
3493.726670	597174.251517	40.765056
3496.066935	597630.681151	40.770061
3498.631320	598042.100180	40.775066
3500.914124	598408.492786	40.780071
3503.031204	598713.676494	40.785076
3504.663143	598979.481716	40.790080
3506.587747	599200.183500	40.795085
3508.259758	599385.030146	40.800090
3509.702915	599530.165593	40.805095
3511.110767	599623.748335	40.810100
3512.683830	599694.129269	40.815104
3513.614399	599730.823645	40.820109
3515.235091	599736.526640	40.825114
3516.257345	599723.402705	40.830119
3517.136110	599664.751692	40.835124
3517.628850	599583.085421	40.840128
3518.274285	599473.563875	40.845133
3519.394291	599360.963645	40.850138
3519.914828	599226.330935	40.855143
3520.703005	599060.869422	40.860148
3521.079205	598886.759586	40.865152
3521.682888	598693.188385	40.870157
3521.893908	598489.863234	40.875162
3522.743312	598275.270739	40.880167
3523.103882	598036.420069	40.885172
3522.869693	597793.151259	40.890176
3522.540332	597549.090680	40.895181
3522.805895	597291.664028	40.900186
3523.209032	597040.117501	40.905191
3523.309184	596765.280564	40.910196
3523.215369	596492.619800	40.915200
3523.476940	596216.992344	40.920205
3523.611555	595929.961106	40.925210
3523.417060	595646.578843	40.930215
3523.596403	595349.510188	40.935220
3523.163721	595060.741421	40.940224
3523.284293	594758.157022	40.945229
3522.857573	594467.067620	40.950234
3522.671098	594180.740425	40.955239
3522.891570	593884.325552	40.960244
3522.530247	593588.995058	40.965248
3522.359518	593298.234380	40.970253
3522.556175	593001.448124	40.975258
3522.361891	592715.032743	40.980263
3522.259378	592407.407818	40.985268
3521.596212	592122.302095	40.990272
3521.799574	591828.688049	40.995277
3521.639158	591543.488342	41.000282
3521.107985	591248.370280	41.005287
3521.475342	590962.772086	41.010292
3521.043873	590681.198744	41.015296
3520.685913	590387.883572	41.020301
3520.526855	590106.954002	41.025306
3520.712095	589821.654621	41.030311
3520.625022	589542.502731	41.035316
3519.936443	589274.209886	41.040320
3519.694298	588982.291397	41.045325
3519.647431	588721.350116	41.050330
3519.327374	588447.367285	41.055335
3519.395284	588182.035744	41.060340
3518.820563	587925.166479	41.065344
3518.696356	587653.087236	41.070349
3518.528910	587402.906909	41.075354
3518.427754	587140.583068	41.080359
3518.131490	586885.349534	41.085364
3517.456036	586637.085240	41.090368
3517.730172	586381.700617	41.095373
3517.516538	586140.118559	41.100378
3517.194848	585886.870326	41.105383
3517.208668	585650.303886	41.110388
3516.744569	585422.678478	41.115392
3516.319545	585182.361306	41.120397
3516.694604	584945.923646	41.125402
3516.115000	584726.772648	41.130407
3516.234149	584491.618296	41.135412
3515.440798	584276.702240	41.140416
3515.246509	584053.166670	41.145421
3515.400157	583830.173697	41.150426
3514.870576	583617.459273	41.155431
3514.826619	583404.815206	41.160436
3514.357503	583201.206993	41.165440
3514.432644	582993.850278	41.170445
3514.192232	582786.639257	41.175450
3514.168080	582589.367213	41.180455
3513.973836	582389.310673	41.185460
3513.830959	582204.333361	41.190464
3513.737116	582002.449224	41.195469
3513.529936	581802.083244	41.200474
3512.936195	581626.943577	41.205479
3512.752161	581440.505896	41.210484
3512.838161	581253.320898	41.215488
3512.733283	581083.110208	41.220493
3512.620068	580906.881206	41.225498
3512.452277	580723.738269	41.230503
3512.247863	580543.155342	41.235508
3511.910152	580382.196656	41.240512
3512.062988	580204.460724	41.245517
3511.660786	580033.728816	41.250522
3511.157944	579876.649827	41.255527
3511.273634	579711.247807	41.260532
3511.042838	579560.741239	41.265536
3510.413645	579398.058690	41.270541
3510.781466	579244.144459	41.275546
3510.307199	579099.737769	41.280551
3510.146480	578953.073567	41.285556
3509.822825	578818.118121	41.290560
3510.209424	578678.135140	41.295565
3510.066765	578534.622172	41.300570
3509.906040	578400.187875	41.305575
3510.073357	578256.321955	41.310580
3509.777735	578121.153083	41.315584
3509.422889	577974.406062	41.320589
3509.665866	577842.409690	41.325594
3509.220743	577713.027133	41.330599
3509.428345	577578.475219	41.335604
3509.069696	577450.681124	41.340608
3508.791742	577313.342968	41.345613
3509.047702	577193.776061	41.350618
3508.571522	577075.024559	41.355623
3509.084880	576950.298608	41.360628
3508.836234	576845.102310	41.365632
3508.633113	576716.924415	41.370637
3508.158658	576593.853742	41.375642
3508.030368	576479.204914	41.380647
3508.298409	576360.780962	41.385652
3508.059843	576254.624475	41.390656
3507.690952	576141.213712	41.395661
3507.937330	576033.825578	41.400666
3508.034719	575923.349540	41.405671
3508.222545	575813.510419	41.410676
3507.863426	575710.227018	41.415680
3507.757310	575590.498996	41.420685
3507.707484	575488.218683	41.425690
3507.488215	575380.997450	41.430695
3507.527373	575277.898654	41.435700
3507.279836	575176.599592	41.440704
3507.417737	575081.961854	41.445709
3507.384425	574982.433600	41.450714
3507.260927	574877.400009	41.455719
3507.143031	574783.853303	41.460724
3506.893656	574680.994835	41.465728
3506.506917	574585.832918	41.470733
3507.125874	574509.076026	41.475738
3506.206173	574419.564933	41.480743
3506.459371	574326.458133	41.485748
3506.193214	574237.094282	41.490752
3506.418098	574152.619983	41.495757
3506.387958	574065.074238	41.500762
3506.003663	573987.718062	41.505767
3506.252989	573901.482025	41.510772
3505.942360	573817.289632	41.515776
3505.522227	573730.454520	41.520781
3505.726500	573659.275814	41.525786
3505.652551	573592.154108	41.530791
3505.680116	573511.368606	41.535796
3505.412069	573442.369715	41.540800
3505.712339	573364.199812	41.545805
3505.465640	573290.028586	41.550810
3505.420869	573217.782175	41.555815
3505.410130	573142.920811	41.560820
3505.557060	573078.220179	41.565824
3505.363268	572997.716506	41.570829
3505.467496	572929.408953	41.575834
3505.138426	572863.777964	41.580839
3505.423427	572792.581202	41.585844
3505.372253	572723.544036	41.590848
3505.085917	572655.346070	41.595853
3505.071914	572584.395462	41.600858
3504.706571	572524.990363	41.605863
3505.032574	572459.053912	41.610868
3504.823762	572402.483929	41.615872
3504.953725	572337.681374	41.620877
3505.175014	572268.247590	41.625882
3504.617366	572204.254292	41.630887
3504.575275	572141.484739	41.635892
3504.566296	572083.175780	41.640896
3504.376307	572016.012720	41.645901
3504.592468	571955.961747	41.650906
3504.718243	571910.878787	41.655911
3504.828831	571850.793582	41.660916
3504.723920	571791.494486	41.665920
3504.710810	571730.976346	41.670925
3504.837885	571669.331947	41.675930
3504.622611	571610.852089	41.680935
3504.900232	571540.451586	41.685940
3505.127487	571485.264197	41.690944
3504.414305	571419.935842	41.695949
3505.032757	571357.259445	41.700954
3504.529925	571303.188995	41.705959
3504.649035	571245.257203	41.710964
3504.718612	571187.784526	41.715968
3504.204796	571122.523670	41.720973
3504.370855	571069.301065	41.725978
3504.538140	571026.717399	41.730983
3504.589201	570966.134986	41.735988
3503.901355	570905.115715	41.740992
3503.777993	570850.431747	41.745997
3504.089416	570806.670439	41.751002
3503.711305	570765.827224	41.756007
3504.024431	570695.968022	41.761012
3503.960406	570663.105284	41.766016
3503.978850	570607.544802	41.771021
3504.197894	570570.522165	41.776026
3503.947350	570524.990686	41.781031
3503.900271	570456.491219	41.786036
3504.079528	570417.015083	41.791040
3504.000341	570369.097339	41.796045
3503.714539	570324.273213	41.801050
3503.677477	570281.116453	41.806055
3504.007720	570219.783797	41.811060
3503.783351	570180.369943	41.816064
3503.834791	570130.373013	41.821069
3503.514226	570087.008892	41.826074
3503.666719	570039.103740	41.831079
3503.626842	569998.957759	41.836084
3504.022086	569965.569510	41.841088
3503.302324	569914.286867	41.846093
3503.617278	569869.567807	41.851098
3503.493040	569832.345498	41.856103
3503.813826	569776.834102	41.861108
3503.934449	569745.545985	41.866112
3503.575335	569691.144289	41.871117
3503.607843	569639.742815	41.876122
3503.642711	569594.966088	41.881127
3503.517519	569548.306904	41.886132
3503.930010	569517.072921	41.891136
3503.559178	569470.401629	41.896141
3503.583807	569430.394151	41.901146
3503.588056	569397.115568	41.906151
3503.581671	569340.599160	41.911156
3503.360336	569308.208866	41.916160
3503.850509	569273.448549	41.921165
3503.838547	569218.488408	41.926170
3503.291950	569188.256757	41.931175
3503.335184	569143.326379	41.936180
3503.343658	569106.833879	41.941184
3503.427797	569065.611169	41.946189
3503.967890	569019.146998	41.951194
3503.369383	568976.675434	41.956199
3503.320156	568933.415116	41.961204
3503.354600	568896.466134	41.966208
3503.078930	568861.924688	41.971213
3503.292393	568812.499032	41.976218
3503.234019	568779.680208	41.981223
3503.565073	568737.664790	41.986228
3503.461032	568704.551717	41.991232
3503.198647	568660.018600	41.996237
3503.634408	568623.256984	42.001242
3503.203951	568594.611891	42.006247
3503.262865	568551.483821	42.011252
3503.448060	568514.961816	42.016256
3503.120864	568472.646760	42.021261
3503.273126	568431.310735	42.026266
3502.881767	568409.987842	42.031271
3502.731108	568367.142829	42.036276
3503.166019	568323.352757	42.041280
3503.246089	568298.994304	42.046285
3503.432234	568262.320758	42.051290
3503.085088	568228.491352	42.056295
3503.105675	568182.607003	42.061300
3503.152015	568148.916643	42.066304
3502.898156	568109.148900	42.071309
3503.578324	568079.224534	42.076314
3503.076876	568037.236310	42.081319
3503.487058	567999.271934	42.086324
3503.457117	567968.052720	42.091328
3503.297017	567930.127069	42.096333
3503.294557	567886.704910	42.101338
3503.187369	567852.033694	42.106343
3503.197659	567817.143210	42.111348
3502.893472	567773.315995	42.116352
3503.110468	567745.621771	42.121357
3502.955591	567704.230755	42.126362
3502.790892	567677.248640	42.131367
3502.998256	567644.385041	42.136372
3502.932965	567614.927414	42.141376
3502.587783	567579.790579	42.146381
3502.893172	567540.234652	42.151386
3503.099090	567529.459355	42.156391
3502.838896	567483.164310	42.161396
3502.939032	567453.580009	42.166400
3502.801316	567418.008637	42.171405
3502.617190	567377.524649	42.176410
3502.704339	567361.697392	42.181415
3503.226073	567328.382136	42.186420
3503.165500	567305.198216	42.191424
3502.977849	567270.889247	42.196429
3502.703398	567223.440740	42.201434
3502.714398	567203.709389	42.206439
3502.998810	567170.330373	42.211444
3502.972567	567148.295431	42.216448
3502.736714	567111.784607	42.221453
3502.685363	567082.373647	42.226458
3503.031907	567057.368483	42.231463
3503.117589	567018.296946	42.236468
3503.129137	566987.871848	42.241472
3502.925497	566944.527801	42.246477
3503.203187	566904.522199	42.251482
3502.979528	566886.383306	42.256487
3502.962186	566838.692211	42.261492
3502.906122	566805.616390	42.266496
3502.773213	566768.285122	42.271501
3502.897022	566739.347951	42.276506
3502.824993	566708.533548	42.281511
3502.960155	566684.815740	42.286516
3503.177243	566644.718306	42.291520
3502.999668	566613.819742	42.296525
3503.300707	566589.071707	42.301530
3502.981433	566561.458485	42.306535
3502.549082	566512.174150	42.311540
3502.789586	566493.309407	42.316544
3502.671060	566461.246478	42.321549
3502.958713	566435.345478	42.326554
3502.813874	566405.294737	42.331559
3503.050994	566366.147120	42.336564
3502.811116	566336.813944	42.341568
3502.774358	566313.122251	42.346573
3503.068464	566262.970196	42.351578
3502.831206	566240.615068	42.356583
3502.929621	566197.020176	42.361588
3503.053770	566170.893113	42.366592
3502.746888	566147.293516	42.371597
3502.995578	566100.712557	42.376602
3502.551278	566075.326836	42.381607
3502.488406	566057.613373	42.386612
3502.770236	566032.013628	42.391616
3502.709522	566003.003051	42.396621
3503.326876	565963.443182	42.401626
3503.032226	565950.284489	42.406631
3503.216209	565908.331996	42.411636
3502.981319	565868.151912	42.416640
3502.708806	565830.789239	42.421645
3503.160782	565795.622781	42.426650
3502.727641	565762.753557	42.431655
3502.986906	565722.947598	42.436660
3502.928770	565701.868859	42.441664
3502.439584	565674.631546	42.446669
3502.224448	565640.322042	42.451674
3502.592442	565616.917118	42.456679
3502.498228	565592.078122	42.461684
3502.928638	565563.391344	42.466688
3503.052686	565523.505422	42.471693
3502.502890	565502.302342	42.476698
3502.476410	565484.230846	42.481703
3502.695946	565447.091277	42.486708
3502.395111	565420.125181	42.491712
3502.759266	565393.055067	42.496717
3503.247093	565366.467660	42.501722
3502.744733	565345.507929	42.506727
3502.789413	565309.901570	42.511732
3502.757879	565282.742425	42.516736
3502.747202	565240.918375	42.521741
3502.784937	565213.095497	42.526746
3502.386445	565198.194797	42.531751
3502.677651	565161.695857	42.536756
3502.695097	565135.181456	42.541760
3502.754125	565111.020435	42.546765
3502.801939	565077.873239	42.551770
3502.529678	565051.353725	42.556775
3502.494907	565026.303380	42.561780
3502.579222	565004.799413	42.566784
3502.623935	564974.363851	42.571789
3502.298195	564946.597157	42.576794
3502.453665	564923.274276	42.581799
3502.323020	564888.397009	42.586804
3502.710965	564867.849572	42.591808
3502.503770	564848.198537	42.596813
3502.338705	564813.226000	42.601818
3502.457202	564795.783537	42.606823
3502.795522	564762.790881	42.611828
3502.692882	564730.369198	42.616832
3502.569526	564711.458024	42.621837
3502.421337	564677.637344	42.626842
3502.181587	564666.376719	42.631847
3502.531300	564644.629745	42.636852
3502.477392	564608.986441	42.641856
3502.245857	564590.895401	42.646861
3502.791503	564554.254356	42.651866
3502.421762	564528.100385	42.656871
3502.668359	564503.155571	42.661876
3502.768842	564467.638342	42.666880
3502.617823	564444.713918	42.671885
3502.225191	564405.005365	42.676890
3502.299691	564398.767021	42.681895
3502.489083	564372.173789	42.686900
3502.483071	564341.091713	42.691904
3502.373675	564333.526282	42.696909
3502.544288	564293.879944	42.701914
3502.319584	564276.088636	42.706919
3502.123798	564252.819327	42.711924
3502.532324	564218.157056	42.716928
3502.392956	564204.218878	42.721933
3502.655569	564183.890693	42.726938
3502.218318	564154.884155	42.731943
3502.442935	564126.778390	42.736948
3502.294808	564107.669245	42.741952
3502.335803	564089.032663	42.746957
3502.476741	564053.758930	42.751962
3502.351674	564035.650382	42.756967
3502.289494	564013.062734	42.761972
3502.528636	563991.683344	42.766976
3502.295187	563965.205505	42.771981
3502.757121	563941.531456	42.776986
3502.677312	563926.278005	42.781991
3502.528283	563897.627501	42.786996
3502.659331	563863.811026	42.792001
3502.674456	563845.429183	42.797005
3502.774152	563803.632940	42.802010
3502.240863	563779.963494	42.807015
3502.183678	563758.730438	42.812020
3502.283814	563733.505574	42.817025
3502.473423	563712.585374	42.822029
3502.536976	563681.992844	42.827034
3502.666436	563667.057863	42.832039
3502.349928	563638.282252	42.837044
3502.373531	563602.071361	42.842049
3502.187519	563596.777237	42.847053
3502.770961	563561.332407	42.852058
3502.017583	563547.640086	42.857063
3502.113569	563511.518035	42.862068
3502.070388	563503.288875	42.867073
3502.429756	563472.699771	42.872077
3502.527404	563442.854564	42.877082
3502.065855	563435.393820	42.882087
3502.430711	563411.281908	42.887092
3502.196776	563384.903266	42.892097
3502.106247	563365.783902	42.897101
3502.083866	563349.114588	42.902106
3502.187434	563330.115480	42.907111
3501.950310	563310.114998	42.912116
3502.653140	563287.205477	42.917121
3501.801065	563272.825189	42.922125
3502.252040	563242.271383	42.927130
3502.147950	563236.311435	42.932135
3502.297827	563201.485711	42.937140
3502.330190	563184.405847	42.942145
3501.782039	563158.176254	42.947149
3501.966258	563141.926326	42.952154
3502.061391	563114.491232	42.957159
3501.860214	563100.260077	42.962164
3502.324703	563087.180348	42.967169
3502.364042	563071.856935	42.972173
3502.584889	563041.690124	42.977178
3501.995605	563016.571492	42.982183
3502.107162	562984.211916	42.987188
3502.036621	562964.385683	42.992193
3502.003884	562946.612559	42.997197
3502.193393	562925.891854	43.002202
3502.003803	562910.302693	43.007207
3502.239027	562882.794936	43.012212
3502.273494	562870.234179	43.017217
3501.892007	562856.231800	43.022221
3502.103932	562831.690614	43.027226
3502.406756	562817.330104	43.032231
3502.302541	562804.640294	43.037236
3502.077767	562775.647333	43.042241
3502.088551	562761.583516	43.047245
3502.243018	562733.284488	43.052250
3502.032527	562712.374829	43.057255
3502.316019	562693.045231	43.062260
3502.531744	562666.142677	43.067265
3501.875779	562650.475411	43.072269
3501.960852	562637.052719	43.077274
3502.062380	562623.878550	43.082279
3502.378479	562603.037041	43.087284
3502.733419	562566.469817	43.092289
3502.257974	562551.025310	43.097293
3502.457321	562519.353843	43.102298
3502.717082	562498.621402	43.107303
3502.322580	562470.508005	43.112308
3502.572773	562440.987959	43.117313
3502.305890	562431.637889	43.122317
3502.331413	562392.459801	43.127322
3502.478956	562376.264771	43.132327
3502.650839	562351.527949	43.137332
3502.444391	562329.512061	43.142337
3502.368935	562289.847183	43.147341
3502.698143	562270.710639	43.152346
3502.186686	562250.500113	43.157351
3502.073739	562225.606658	43.162356
3502.388651	562201.901863	43.167361
3502.207923	562186.913041	43.172365
3502.622293	562153.650029	43.177370
3502.054706	562124.407703	43.182375
3501.717037	562108.288156	43.187380
3502.170903	562088.529135	43.192385
3501.836750	562065.377553	43.197389
3502.069921	562054.191148	43.202394
3501.799954	562032.686879	43.207399
3502.207082	562020.016731	43.212404
3502.213243	562005.601158	43.217409
3502.060042	561994.023074	43.222413
3501.927109	561948.891517	43.227418
3502.199168	561933.228887	43.232423
3502.106663	561923.298674	43.237428
3502.349814	561906.987601	43.242433
3502.349726	561886.746731	43.247437
3502.275340	561865.010678	43.252442
3502.274376	561835.176797	43.257447
3502.385158	561827.926902	43.262452
3502.378848	561804.422200	43.267457
3501.836887	561773.668223	43.272461
3501.969808	561746.575606	43.277466
3502.240200	561740.355450	43.282471
3502.244318	561722.172903	43.287476
3502.537181	561693.699058	43.292481
3502.059023	561674.085046	43.297485
3502.283089	561640.096939	43.302490
3502.029760	561623.712409	43.307495
3502.175258	561603.749651	43.312500
3501.968207	561580.326109	43.317505
3501.788063	561569.404764	43.322509
3502.373588	561543.747726	43.327514
3502.021988	561532.802924	43.332519
3501.964083	561504.283003	43.337524
3502.098350	561487.586556	43.342529
3501.596637	561473.199499	43.347533
3501.935469	561454.009897	43.352538
3501.742408	561440.127048	43.357543
3502.124683	561422.186284	43.362548
3502.036108	561407.885243	43.367553
3502.029337	561391.411618	43.372557
3502.580667	561372.188664	43.377562
3502.118043	561338.959996	43.382567
3502.234109	561328.996674	43.387572
3501.898783	561306.446511	43.392577
3502.168117	561292.742340	43.397581
3502.007366	561259.616940	43.402586
3502.024012	561241.682832	43.407591
3501.813470	561225.240829	43.412596
3502.474067	561203.890938	43.417601
3501.677913	561185.882896	43.422605
3501.764025	561171.252889	43.427610
3502.173436	561167.974175	43.432615
3501.930160	561136.719780	43.437620
3502.265671	561125.918326	43.442625
3502.124827	561110.570295	43.447629
3502.211383	561087.200329	43.452634
3502.234481	561060.726049	43.457639
3502.063345	561037.898558	43.462644
3502.610923	561025.305846	43.467649
3502.305340	561006.969694	43.472653
3502.594353	560978.344037	43.477658
3502.205357	560955.801591	43.482663
3502.130053	560929.794464	43.487668
3502.145212	560902.617858	43.492673
3501.773701	560892.228095	43.497677
3501.665995	560869.942888	43.502682
3502.393870	560846.673108	43.507687
3501.885631	560827.012152	43.512692
3501.959986	560802.739392	43.517697
3501.972444	560791.435606	43.522701
3501.999746	560771.389456	43.527706
3501.811586	560757.304114	43.532711
3501.950850	560744.574015	43.537716
3501.924061	560723.632097	43.542721
3502.095941	560717.225884	43.547725
3502.125968	560688.238169	43.552730
3501.859848	560668.639559	43.557735
3501.529689	560665.426092	43.562740
3501.990596	560639.434961	43.567745
3501.983752	560632.705027	43.572749
3501.976508	560605.832624	43.577754
3502.040166	560591.607256	43.582759
3501.986676	560576.948106	43.587764
3502.269769	560561.030777	43.592769
3501.859959	560540.851645	43.597773
3502.147890	560521.367101	43.602778
3501.903622	560502.568497	43.607783
3501.997539	560488.036886	43.612788
3502.142334	560476.460953	43.617793
3501.749907	560445.077347	43.622797
3502.174054	560428.032696	43.627802
3501.998479	560412.337564	43.632807
3502.060248	560396.655540	43.637812
3502.207352	560377.845786	43.642817
3501.849656	560346.808111	43.647821
3502.137731	560328.779952	43.652826
3501.997217	560315.389880	43.657831
3501.877309	560299.183576	43.662836
3501.950634	560276.969413	43.667841
3502.124153	560258.557197	43.672845
3502.201059	560242.269814	43.677850
3502.347638	560227.126863	43.682855
3502.306846	560207.140634	43.687860
3502.087410	560175.327406	43.692865
3502.216975	560162.799128	43.697869
3502.001054	560137.917356	43.702874
3501.944360	560109.594804	43.707879
3501.711810	560101.392865	43.712884
3501.747749	560091.993589	43.717889
3501.852318	560072.737903	43.722893
3502.008195	560051.213673	43.727898
3501.882029	560051.886332	43.732903
3502.164768	560034.059491	43.737908
3502.179565	560011.100480	43.742913
3502.318107	559998.068291	43.747917
3502.280041	559969.139690	43.752922
3502.055143	559937.778778	43.757927
3501.768527	559935.613209	43.762932
3501.985563	559901.721666	43.767937
3501.749090	559889.149852	43.772941
3501.640331	559878.567415	43.777946
3501.591545	559852.754705	43.782951
3501.851539	559846.384481	43.787956
3502.038628	559836.609736	43.792961
3501.760447	559812.339820	43.797965
3501.582907	559802.320643	43.802970
3501.794055	559786.313053	43.807975
3501.691560	559771.057752	43.812980
3501.876057	559747.267951	43.817985
3501.981290	559744.136869	43.822989
3501.356310	559725.848654	43.827994
3501.906271	559722.447105	43.832999
3501.522271	559715.223029	43.838004
3501.675228	559677.723972	43.843009
3501.539309	559676.087379	43.848013
3501.705251	559657.122831	43.853018
3501.694441	559637.382126	43.858023
3501.228043	559624.795739	43.863028
3501.413600	559611.102721	43.868033
3501.573592	559623.234481	43.873037
3502.053319	559595.379424	43.878042
3501.758539	559585.981213	43.883047
3501.545310	559581.895170	43.888052
3502.003307	559557.358940	43.893057
3501.410110	559551.423348	43.898061
3502.046336	559536.052262	43.903066
3501.791579	559508.562999	43.908071
3501.894057	559511.812187	43.913076
3501.746587	559481.794317	43.918081
3502.014125	559475.171538	43.923085
3501.672677	559460.505784	43.928090
3501.926943	559425.451639	43.933095
3502.014313	559424.885291	43.938100
3502.157596	559394.520333	43.943105
3501.654657	559392.187536	43.948109
3501.858477	559382.108386	43.953114
3501.945866	559359.689359	43.958119
3502.183053	559344.832532	43.963124
3502.188653	559314.087003	43.968129
3501.796188	559300.232805	43.973133
3501.857270	559285.051779	43.978138
3502.019995	559255.939337	43.983143
3501.882554	559251.238494	43.988148
3501.843294	559218.590741	43.993153
3501.617686	559227.919696	43.998157
3501.731082	559208.460279	44.003162
3501.717431	559191.783715	44.008167
3501.817335	559173.130138	44.013172
3501.952966	559151.959099	44.018177
3502.093877	559149.023231	44.023181
3501.951512	559137.591356	44.028186
3502.025407	559106.382479	44.033191
3501.902068	559097.911583	44.038196
3502.676689	559065.789260	44.043201
3501.873010	559054.109026	44.048205
3501.691007	559027.712495	44.053210
3501.800272	559006.042943	44.058215
3501.883017	559012.108657	44.063220
3501.967568	558971.804759	44.068225
3502.113066	558965.803628	44.073229
3502.135931	558945.905794	44.078234
3502.056304	558932.906541	44.083239
3501.790290	558915.716423	44.088244
3502.073907	558886.533939	44.093249
3501.652879	558880.068709	44.098253
3501.742927	558856.693793	44.103258
3501.842599	558856.828830	44.108263
3502.022932	558830.023548	44.113268
3501.846077	558800.309976	44.118273
3501.952746	558806.522772	44.123277
3501.853094	558781.218063	44.128282
3501.757938	558770.481793	44.133287
3501.968254	558760.501578	44.138292
3502.081629	558736.720870	44.143297
3502.019300	558735.374073	44.148301
3501.859171	558707.114576	44.153306
3501.829038	558687.626504	44.158311
3502.261385	558664.649849	44.163316
3502.132572	558653.165149	44.168321
3501.788374	558623.929448	44.173325
3501.628300	558607.777345	44.178330
3502.087195	558599.767705	44.183335
3501.482967	558580.118008	44.188340
3501.462695	558553.996576	44.193345
3501.764063	558561.736487	44.198349
3501.152159	558534.752951	44.203354
3501.960169	558521.363287	44.208359
3501.398486	558519.592132	44.213364
3501.215263	558522.685297	44.218369
3501.514583	558504.853570	44.223373
3501.584414	558487.007452	44.228378
3501.369802	558483.071964	44.233383
3501.205187	558474.255396	44.238388
3501.605224	558463.541915	44.243393
3501.726202	558456.841003	44.248397
3501.478152	558436.884187	44.253402
3501.532113	558432.454537	44.258407
3501.443690	558424.831781	44.263412
3501.823870	558410.202634	44.268417
3501.609075	558391.797987	44.273421
3501.469433	558392.372364	44.278426
3501.847925	558368.901155	44.283431
3501.465889	558360.369693	44.288436
3501.827608	558345.140468	44.293441
3501.724711	558337.670641	44.298445
3501.685943	558310.144833	44.303450
3501.757394	558316.112188	44.308455
3501.342635	558293.618928	44.313460
3501.821361	558263.399601	44.318465
3501.617389	558260.869116	44.323469
3501.656079	558256.441787	44.328474
3501.641073	558235.493628	44.333479
3501.820502	558227.075260	44.338484
3501.671557	558221.823156	44.343489
3501.642548	558201.831703	44.348493
3501.859978	558182.856754	44.353498
3501.845811	558177.684043	44.358503
3501.527209	558158.340682	44.363508
3501.614336	558132.955152	44.368513
3501.534391	558145.025453	44.373517
3501.650997	558120.891320	44.378522
3501.342092	558105.716385	44.383527
3501.358600	558098.529189	44.388532
3501.783110	558084.244402	44.393537
3501.370237	558084.158126	44.398541
3500.842175	558070.122719	44.403546
3501.120693	558060.734154	44.408551
3501.424009	558054.104994	44.413556
3501.364422	558049.893918	44.418561
3501.282421	558052.117273	44.423565
3501.563523	558041.924424	44.428570
3501.933159	558023.076151	44.433575
3501.576600	558015.947226	44.438580
3501.746413	558008.434559	44.443585
3501.380812	557995.830678	44.448589
3501.512496	557979.933563	44.453594
3501.723829	557964.425910	44.458599
3501.299131	557953.087272	44.463604
3501.478097	557935.122782	44.468609
3501.248195	557929.481267	44.473613
3501.921414	557929.124718	44.478618
3501.604052	557908.173007	44.483623
3501.387080	557901.976794	44.488628
3501.578627	557886.773587	44.493633
3501.561199	557893.357957	44.498637
3501.575947	557870.495296	44.503642
3501.794470	557852.825952	44.508647
3501.468329	557845.943382	44.513652
3501.318269	557842.047831	44.518657
3501.428064	557828.917273	44.523661
3501.513730	557810.816453	44.528666
3501.563981	557805.080841	44.533671
3501.277609	557801.558285	44.538676
3501.482587	557791.779064	44.543681
3501.369097	557780.190639	44.548685
3501.412588	557778.375005	44.553690
3501.198465	557767.354970	44.558695
3501.151669	557766.357334	44.563700
3501.590356	557748.150989	44.568705
3501.525718	557727.862852	44.573709
3501.376840	557721.605657	44.578714
3501.483363	557709.781797	44.583719
3501.727223	557713.863509	44.588724
3501.629967	557691.620931	44.593729
3501.365014	557684.527729	44.598733
3501.965398	557675.390004	44.603738
3501.693092	557657.696615	44.608743
3501.014489	557638.458929	44.613748
3501.298641	557632.636425	44.618753
3501.324924	557632.079544	44.623757
3501.235600	557628.877835	44.628762
3501.740698	557606.993125	44.633767
3501.491562	557590.954050	44.638772
3502.115167	557576.386314	44.643777
3501.474047	557574.677674	44.648781
3501.440868	557563.026239	44.653786
3501.590988	557547.778833	44.658791
3501.588480	557555.064469	44.663796
3501.637115	557535.110003	44.668801
3501.597246	557522.002503	44.673805
3501.856945	557514.475474	44.678810
3501.690934	557492.745712	44.683815
3501.518219	557480.060886	44.688820
3501.830326	557469.812459	44.693825
3501.643725	557459.591740	44.698829
3501.720173	557436.366893	44.703834
3501.376337	557430.843441	44.708839
3501.320426	557427.134012	44.713844
3501.933931	557416.185246	44.718849
3501.972777	557400.100894	44.723853
3501.831277	557387.813045	44.728858
3501.658985	557362.064473	44.733863
3501.462066	557354.156525	44.738868
3501.561802	557350.673963	44.743873
3501.352374	557327.644328	44.748877
3501.418599	557310.902395	44.753882
3501.347238	557304.934330	44.758887
3501.372173	557307.945022	44.763892
3501.744106	557304.570629	44.768897
3501.667352	557284.082652	44.773901
3501.497394	557267.628804	44.778906
3501.827946	557258.884660	44.783911
3501.776625	557238.141404	44.788916
3501.882665	557229.030375	44.793921
3501.459942	557229.448079	44.798925
3501.411564	557205.438375	44.803930
3501.492491	557181.106937	44.808935
3501.465267	557183.723852	44.813940
3501.719483	557181.925430	44.818945
3501.284251	557157.624389	44.823949
3501.241738	557151.551247	44.828954
3501.546071	557146.378543	44.833959
3501.322680	557139.931708	44.838964
3501.409139	557126.351816	44.843969
3501.573157	557121.703492	44.848973
3501.561674	557105.928085	44.853978
3501.730614	557088.818063	44.858983
3501.832064	557096.740922	44.863988
3501.892319	557066.634232	44.868993
3501.534687	557059.906865	44.873997
3501.540380	557035.084433	44.879002
3502.022041	557019.935261	44.884007
3501.656354	557023.208074	44.889012
3501.333818	557003.009267	44.894017
3501.821057	556986.301554	44.899021
3501.633605	556980.401721	44.904026
3501.861351	556973.080332	44.909031
3501.834518	556945.248028	44.914036
3501.663959	556932.612528	44.919041
3502.271370	556918.147019	44.924045
3502.033837	556909.441182	44.929050
3501.922022	556893.630932	44.934055
3501.827981	556871.939034	44.939060
3501.628142	556855.037069	44.944065
3501.414148	556829.796333	44.949069
3501.602713	556818.812961	44.954074
3501.573489	556809.722759	44.959079
3501.732248	556807.738218	44.964084
3501.620453	556786.651902	44.969089
3501.426097	556773.617978	44.974093
3501.427447	556769.698405	44.979098
3501.960899	556756.550686	44.984103
3501.994830	556751.168849	44.989108
3502.181571	556737.723579	44.994113
3502.057458	556716.840055	44.999117
3502.101127	556698.090900	45.004122
3501.800961	556660.200947	45.009127
3501.633819	556657.312627	45.014132
3501.693159	556644.741377	45.019137
3501.728778	556631.621099	45.024141
3501.964313	556608.721506	45.029146
3501.748618	556594.736017	45.034151
3501.353998	556578.215843	45.039156
3501.612783	556581.240409	45.044161
3501.383254	556569.618699	45.049165
3501.618733	556567.772868	45.054170
3501.821259	556537.592358	45.059175
3501.685576	556536.357274	45.064180
3501.589837	556518.936078	45.069185
3501.419793	556499.164811	45.074189
3501.533552	556499.046436	45.079194
3501.429957	556488.610915	45.084199
3501.194898	556485.431682	45.089204
3501.665704	556465.811417	45.094209
3502.018484	556447.516029	45.099213
3501.735376	556434.847348	45.104218
3501.950093	556411.699391	45.109223
3501.699684	556415.657825	45.114228
3501.627651	556399.689957	45.119233
3501.630921	556376.223246	45.124237
3501.434313	556368.565838	45.129242
3501.629959	556357.379941	45.134247
3501.668037	556353.303744	45.139252
3501.592421	556319.196511	45.144257
3501.328310	556323.508860	45.149261
3501.590764	556319.196579	45.154266
3501.820087	556293.885408	45.159271
3501.543788	556284.180194	45.164276
3501.779938	556273.138634	45.169281
3501.750375	556251.636526	45.174285
3501.217125	556241.870948	45.179290
3501.403739	556235.661023	45.184295
3501.335787	556231.601360	45.189300
3501.679892	556215.819438	45.194305
3501.982328	556201.350494	45.199309
3501.679422	556202.101243	45.204314
3501.464796	556172.889515	45.209319
3501.881324	556156.241952	45.214324
3501.731153	556149.079639	45.219329
3501.327947	556138.389153	45.224333
3501.291231	556112.867940	45.229338
3501.596714	556116.739571	45.234343
3501.813031	556118.313651	45.239348
3501.736465	556091.341379	45.244353
3501.746089	556088.324787	45.249357
3501.835027	556078.512059	45.254362
3501.573026	556049.809936	45.259367
3501.267500	556038.350339	45.264372
3501.733861	556030.237322	45.269377
3501.768461	556032.241822	45.274381
3501.636838	556009.800483	45.279386
3501.801399	555993.594085	45.284391
3501.460868	555994.551729	45.289396
3501.660228	555970.701818	45.294401
3501.809785	555962.688531	45.299405
3501.782574	555952.190351	45.304410
3501.563154	555937.802671	45.309415
3501.429020	555922.999636	45.314420
3501.799470	555903.394142	45.319425
3501.421622	555902.196848	45.324429
3501.566379	555894.184266	45.329434
3501.745997	555862.699119	45.334439
3501.361664	555862.256598	45.339444
3501.230902	555845.945416	45.344449
3501.541774	555825.947102	45.349453
3501.379782	555819.741208	45.354458
3501.830373	555817.861636	45.359463
3501.672484	555811.303339	45.364468
3501.371569	555787.129261	45.369473
3501.650128	555767.186152	45.374477
3501.792695	555758.319551	45.379482
3501.645510	555739.950491	45.384487
3501.138258	555732.290985	45.389492
3501.688839	555732.003813	45.394497
3501.942973	555732.114743	45.399501
3501.574808	555712.423398	45.404506
3502.052882	555693.102245	45.409511
3501.764582	555672.493822	45.414516
3501.819747	555653.439725	45.419521
3501.788111	555649.173180	45.424525
3501.521923	555629.717016	45.429530
3502.179470	555616.196889	45.434535
3501.945509	555602.966872	45.439540
3501.945481	555587.840947	45.444545
3501.741066	555574.857540	45.449549
3501.733848	555561.893543	45.454554
3501.997499	555544.716259	45.459559
3501.515504	555537.153184	45.464564
3501.277582	555513.521480	45.469569
3501.752876	555500.632743	45.474573
3501.672555	555496.876278	45.479578
3501.754351	555493.496488	45.484583
3501.281667	555463.820848	45.489588
3501.152857	555442.734824	45.494593
3501.646832	555453.562311	45.499597
3501.290123	555453.718484	45.504602
3501.810843	555438.108942	45.509607
3501.598960	555425.227045	45.514612
3501.576958	555421.762956	45.519617
3501.669026	555411.798435	45.524621
3501.435902	555395.150872	45.529626
3501.426547	555374.247065	45.534631
3501.430359	555375.000166	45.539636
3501.687446	555365.713350	45.544641
3501.552376	555335.331326	45.549645
3501.345793	555338.026935	45.554650
3501.410695	555322.186983	45.559655
3501.512781	555320.110552	45.564660
3501.034472	555304.305241	45.569665
3501.636772	555282.602111	45.574669
3501.192611	555291.867792	45.579674
3501.844478	555280.107040	45.584679
3501.367585	555271.939959	45.589684
3501.382714	555250.931603	45.594689
3501.704354	555251.283253	45.599693
3501.395235	555256.608086	45.604698
3501.612261	555235.819407	45.609703
3501.174061	555219.203659	45.614708
3501.342789	555208.623944	45.619713
3501.482961	555206.290271	45.624717
3501.431191	555205.644973	45.629722
3501.567548	555187.381500	45.634727
3501.172985	555166.386789	45.639732
3501.201986	555156.029885	45.644737
3501.354714	555146.909976	45.649741
3501.507529	555160.303754	45.654746
3501.610076	555138.980013	45.659751
3501.796240	555126.688869	45.664756
3501.794293	555114.527627	45.669761
3501.287266	555103.802190	45.674765
3501.643417	555083.996580	45.679770
3501.526111	555073.059428	45.684775
3501.414405	555074.483911	45.689780
3501.929866	555071.136716	45.694785
3501.823667	555047.584010	45.699789
3501.733385	555041.064976	45.704794
3501.782082	555014.874769	45.709799
3501.664219	554999.816779	45.714804
3501.275386	554996.158640	45.719809
3501.312296	554990.926311	45.724813
3501.553773	554978.827387	45.729818
3501.733145	554953.068908	45.734823
3501.201787	554935.160708	45.739828
3501.165461	554873.955906	45.744833
3501.112627	554778.579778	45.749837
3501.079876	554629.074181	45.754842
3500.953118	554425.002623	45.759847
3500.390639	554186.619415	45.764852
3499.905269	553888.260506	45.769857
3499.724417	553554.161730	45.774861
3499.078503	553177.252972	45.779866
3498.462924	552736.191191	45.784871
3498.095305	552272.153391	45.789876
3497.223983	551757.959021	45.794881
3495.980796	551191.721119	45.799885
3495.253263	550594.156910	45.804890
3494.488409	549955.192680	45.809895
3493.448424	549277.523915	45.814900
3492.169761	548553.696954	45.819905
3490.911355	547790.250477	45.824909
3489.944522	546997.745467	45.829914
3488.952693	546149.672365	45.834919
3487.126462	545275.971090	45.839924
3485.697402	544355.720995	45.844929
3483.980468	543417.942735	45.849933
3482.641664	542421.076373	45.854938
3480.718954	541405.456270	45.859943
3479.020400	540356.008478	45.864948
3477.140039	539273.241192	45.869953
3475.488123	538156.780107	45.874957
3473.655638	537019.363193	45.879962
3471.621837	535827.467259	45.884967
3469.427220	534619.629338	45.889972
3467.392003	533380.088710	45.894977
3465.225437	532113.665140	45.899981
3463.038769	530828.188753	45.904986
3460.617352	529496.696792	45.909991
3458.046834	528154.667661	45.914996
3455.568456	526788.965592	45.920001
3453.451641	525396.368327	45.925005
3450.719191	523990.270272	45.930010
3448.232304	522557.232065	45.935015
3445.366149	521098.603249	45.940020
3442.304973	519634.102028	45.945025
3439.804959	518136.897289	45.950029
3437.187324	516658.700255	45.955034
3434.676000	515132.840072	45.960039
3431.740477	513584.088815	45.965044
3428.739455	512024.283294	45.970049
3426.059670	510456.234717	45.975053
3422.996083	508877.882941	45.980058
3420.101991	507253.730731	45.985063
3416.291988	505644.769851	45.990068
3413.829791	504010.947978	45.995073
3410.970438	502370.896784	46.000077
3407.681822	500723.459681	46.005082
3404.481085	499054.776713	46.010087
3401.311919	497377.166220	46.015092
3397.877280	495694.307356	46.020097
3394.875964	493995.235994	46.025101
3391.152134	492297.194567	46.030106
3387.931276	490587.520398	46.035111
3384.423397	488866.031362	46.040116
3380.675705	487135.141777	46.045121
3377.660540	485408.690140	46.050125
3373.950130	483671.595136	46.055130
3370.777058	481928.158566	46.060135
3366.979366	480185.484110	46.065140
3363.723689	478429.695612	46.070145
3360.415404	476673.771338	46.075149
3356.626357	474931.781273	46.080154
3352.995671	473156.617088	46.085159
3349.467718	471390.646158	46.090164
3345.761914	469619.607172	46.095169
3342.493886	467848.511197	46.100173
3338.416499	466081.701806	46.105178
3334.770514	464317.116313	46.110183
3331.125132	462534.944129	46.115188
3327.197113	460749.846197	46.120193
3324.017047	458977.144332	46.125197
3320.055454	457210.757837	46.130202
3316.255334	455421.494548	46.135207
3312.722932	453644.406130	46.140212
3308.646288	451871.627272	46.145217
3305.216466	450093.710706	46.150221
3301.218056	448319.149179	46.155226
3297.803211	446538.651276	46.160231
3293.887447	444772.640904	46.165236
3290.351724	442989.335072	46.170241
3286.355254	441216.919730	46.175245
3282.461606	439450.854006	46.180250
3278.940461	437675.547641	46.185255
3274.863438	435898.389088	46.190260
3270.866416	434135.745998	46.195265
3267.277653	432375.969087	46.200269
3263.582714	430612.604001	46.205274
3260.006308	428852.001567	46.210279
3255.734688	427097.332152	46.215284
3252.347360	425333.652293	46.220289
3248.610851	423575.753240	46.225293
3244.404588	421827.813827	46.230298
3240.465691	420068.174900	46.235303
3236.568464	418327.343866	46.240308
3232.719288	416582.100997	46.245313
3229.396574	414845.354364	46.250317
3225.374551	413107.257008	46.255322
3221.533358	411365.795603	46.260327
3217.549256	409648.108737	46.265332
3214.038151	407910.733324	46.270337
3210.314847	406189.337347	46.275341
3206.109068	404469.558671	46.280346
3202.474817	402745.551130	46.285351
3198.695353	401030.773071	46.290356
3194.358071	399319.405502	46.295361
3191.242288	397616.551973	46.300365
3187.300244	395913.044436	46.305370
3183.687174	394200.734070	46.310375
3179.544146	392497.166371	46.315380
3175.747780	390799.059812	46.320385
3172.156517	389103.798860	46.325389
3168.272383	387415.245844	46.330394
3164.352502	385715.641898	46.335399
3160.274240	384029.913065	46.340404
3156.774090	382346.521777	46.345409
3153.126418	380668.325678	46.350413
3149.085437	378994.857486	46.355418
3145.123159	377325.308959	46.360423
3141.351476	375652.730754	46.365428
3137.610994	373997.188958	46.370433
3133.902289	372326.173869	46.375437
3129.982689	370679.172633	46.380442
3126.540119	369017.900159	46.385447
3122.324283	367373.368014	46.390452
3118.804963	365729.242084	46.395457
3115.068381	364079.212605	46.400461
3110.944403	362443.151711	46.405466
3107.567714	360806.858160	46.410471
3103.213963	359178.861889	46.415476
3099.203132	357542.642864	46.420481
3096.246548	355921.650015	46.425485
3092.432571	354301.291362	46.430490
3088.665819	352675.478701	46.435495
3085.065432	351059.267471	46.440500
3081.181395	349447.265056	46.445505
3077.415712	347828.580435	46.450509
3073.275919	346218.341312	46.455514
3069.708399	344612.867941	46.460519
3066.086859	343006.793439	46.465524
3062.191985	341407.857400	46.470529
3058.540380	339803.953560	46.475533
3054.904561	338216.529234	46.480538
3051.238200	336619.859381	46.485543
3047.443553	335037.966332	46.490548
3043.534699	333449.665512	46.495553
3039.638426	331859.032070	46.500557
3035.694548	330282.862961	46.505562
3031.920702	328699.303135	46.510567
3028.340676	327129.512245	46.515572
3024.363809	325567.683723	46.520577
3020.776255	324001.994745	46.525581
3016.980210	322451.390010	46.530586
3013.586124	320892.473191	46.535591
3009.952260	319338.116247	46.540596
3005.928926	317778.803141	46.545601
3002.318332	316222.652424	46.550605
2998.741461	314680.156705	46.555610
2995.041784	313134.574562	46.560615
2991.177059	311592.961676	46.565620
2987.292026	310053.871700	46.570625
2983.816536	308513.803158	46.575629
2980.076885	306981.896322	46.580634
2976.038189	305447.037094	46.585639
2972.702477	303923.753885	46.590644
2968.822923	302385.953258	46.595649
2965.391730	300857.327435	46.600653
2961.447923	299350.092569	46.605658
2957.918541	297833.741367	46.610663
2954.272197	296324.418059	46.615668
2950.285986	294801.643038	46.620673
2946.681446	293283.019672	46.625677
2942.928328	291792.916348	46.630682
2939.251117	290270.359621	46.635687
2935.478909	288778.786719	46.640692
2931.795210	287281.742950	46.645697
2928.463039	285773.357837	46.650701
2924.564008	284284.579457	46.655706
2921.106061	282785.389218	46.660711
2917.410784	281306.979101	46.665716
2913.550650	279803.588693	46.670721
2910.160002	278308.598334	46.675725
2906.365933	276822.171316	46.680730
2902.867431	275333.607758	46.685735
2898.878711	273841.121612	46.690740
2894.955129	272362.933888	46.695745
2891.239330	270876.387618	46.700749
2887.432029	269406.050817	46.705754
2883.924129	267930.194608	46.710759
2880.356722	266470.901783	46.715764
2876.398109	264995.886309	46.720769
2872.956262	263532.788021	46.725773
2869.288191	262092.725181	46.730778
2865.843540	260626.863392	46.735783
2861.868537	259171.455784	46.740788
2858.092902	257713.147187	46.745793
2854.700261	256260.287870	46.750797
2850.766232	254822.624133	46.755802
2847.566547	253378.922291	46.760807
2844.022098	251924.105491	46.765812
2839.936005	250492.025207	46.770817
2836.987595	249040.068066	46.775821
2833.164236	247604.534621	46.780826
2829.364512	246167.127006	46.785831
2825.701179	244721.410371	46.790836
2821.958186	243283.922350	46.795841
2818.191767	241842.175628	46.800845
2814.511184	240408.022014	46.805850
2810.766658	238976.748649	46.810855
2806.840999	237561.949375	46.815860
2803.251061	236137.413408	46.820865
2799.795638	234721.306572	46.825869
2795.593658	233305.133506	46.830874
2792.178368	231893.417799	46.835879
2788.584612	230481.548423	46.840884
2785.105825	229084.150324	46.845889
2781.465960	227663.140257	46.850893
2777.828216	226270.220977	46.855898
2774.435395	224859.561853	46.860903
2770.882164	223458.733532	46.865908
2767.020581	222052.503865	46.870913
2763.524672	220654.699673	46.875917
2759.755677	219261.804898	46.880922
2756.606939	217865.224787	46.885927
2752.822573	216474.732726	46.890932
2748.929349	215080.543347	46.895937
2745.285363	213682.524936	46.900941
2741.425408	212295.166159	46.905946
2737.932001	210906.559081	46.910951
2734.355056	209518.353801	46.915956
2730.734141	208130.493844	46.920961
2727.092665	206762.204543	46.925965
2723.659083	205374.510108	46.930970
2719.900569	203996.477110	46.935975
2716.172895	202609.077073	46.940980
2712.697644	201243.524557	46.945985
2708.892027	199858.577764	46.950989
2705.289313	198488.509203	46.955994
2701.946939	197120.067488	46.960999
2698.388908	195753.047520	46.966004
2694.540007	194381.528041	46.971009
2691.065084	193018.036897	46.976013
2687.098525	191660.672595	46.981018
2683.798857	190293.618666	46.986023
2680.268936	188944.187516	46.991028
2676.674804	187573.061169	46.996033
2673.127000	186205.866361	47.001037
2669.041955	184862.276668	47.006042
2665.523914	183499.314623	47.011047
2662.161962	182145.717587	47.016052
2658.064226	180798.544254	47.021057
2654.616580	179447.291313	47.026061
2650.866664	178097.099090	47.031066
2647.110692	176760.932776	47.036071
2643.716339	175428.652092	47.041076
2640.090068	174080.949019	47.046081
2636.481259	172739.312784	47.051085
2632.757619	171419.944239	47.056090
2629.233331	170075.476943	47.061095
2625.825377	168752.083268	47.066100
2621.903364	167420.952896	47.071105
2618.624026	166088.143173	47.076109
2614.724577	164766.950279	47.081114
2611.283663	163434.573939	47.086119
2607.586973	162118.951286	47.091124
2603.857147	160787.284955	47.096129
2600.521732	159466.683532	47.101133
2596.755906	158156.995889	47.106138
2592.887233	156839.588838	47.111143
2589.514463	155529.922169	47.116148
2585.692389	154217.784226	47.121153
2581.725317	152904.108072	47.126157
2578.232186	151615.127884	47.131162
2574.622291	150304.587454	47.136167
2571.101998	149003.405016	47.141172
2567.316746	147702.728259	47.146177
2563.624216	146408.647859	47.151181
2559.818817	145119.109189	47.156186
2556.753513	143751.538763	47.161191
2552.943307	142457.195360	47.166196
2549.260149	141180.640833	47.171201
2545.931422	139887.231589	47.176205
2542.558758	138601.981360	47.181210
2538.797430	137332.093988	47.186215
2535.102365	136044.432649	47.191220
2531.097422	134769.119821	47.196225
2527.980443	133481.771420	47.201229
2524.146750	132206.288479	47.206234
2520.288556	130940.933966	47.211239
2516.654274	129671.879799	47.216244
2513.472576	128410.411797	47.221249
2509.911022	127129.872569	47.226253
2506.166990	125863.405116	47.231258
2502.773326	124598.028451	47.236263
2499.307664	123337.077663	47.241268
2495.338370	122078.623627	47.246273
2491.879949	120811.329165	47.251277
2488.154593	119552.625351	47.256282
2484.511100	118303.487341	47.261287
2480.922922	117035.001909	47.266292
2477.413334	115792.589030	47.271297
2473.910050	114538.162324	47.276301
2470.168060	113289.283144	47.281306
2466.520056	112043.496309	47.286311
2463.180123	110789.529173	47.291316
2459.282205	109551.077051	47.296321
2455.832001	108306.699479	47.301325
2451.932718	107063.529881	47.306330
2448.167655	105834.075302	47.311335
2444.976652	104597.532834	47.316340
2441.334920	103361.195122	47.321345
2437.999919	102123.609483	47.326349
2434.295344	100903.541286	47.331354
2430.575308	99660.350629	47.336359
2427.035818	98434.464307	47.341364
2422.742326	97209.085870	47.346369
2419.592328	95983.969738	47.351373
2415.845889	94769.554925	47.356378
2411.944470	93550.840227	47.361383
2408.700282	92341.499389	47.366388
2405.083326	91131.451392	47.371393
2401.013576	89923.796852	47.376397
2397.493753	88711.950081	47.381402
2393.848290	87501.315685	47.386407
2390.454581	86310.764595	47.391412
2386.648958	85117.658512	47.396417
2383.230431	83910.274953	47.401421
2379.712564	82726.102268	47.406426
2375.878711	81538.369867	47.411431
2372.314197	80339.848623	47.416436
2368.660564	79157.993100	47.421441
2365.122944	77962.376596	47.426445
2361.429340	76779.714284	47.431450
2357.911060	75603.844547	47.436455
2354.066272	74428.622852	47.441460
2350.286011	73272.375865	47.446465
2346.740697	72086.035163	47.451469
2342.971242	70919.793723	47.456474
2339.596517	69752.005877	47.461479
2335.719287	68593.560005	47.466484
2332.108754	67434.267209	47.471489
2328.673906	66281.848190	47.476493
2324.876461	65134.292004	47.481498
2321.498953	63981.949103	47.486503
2317.605963	62829.453982	47.491508
2313.742087	61690.442830	47.496513
2310.155530	60547.480586	47.501517
2306.345247	59412.170591	47.506522
2303.015271	58279.554023	47.511527
2299.196242	57152.974171	47.516532
2295.529963	56032.710857	47.521537
2291.748471	54905.526106	47.526541
2288.029401	53789.766720	47.531546
2284.667919	52674.124558	47.536551
2280.747433	51564.097472	47.541556
2277.643812	50468.280835	47.546561
2273.595396	49357.459223	47.551565
2269.707261	48254.772240	47.556570
2265.996643	47158.662428	47.561575
2262.462375	46068.406339	47.566580
2258.547290	44976.816422	47.571585
2255.033454	43889.357829	47.576589
2251.455184	42828.221653	47.581594
2247.710878	41751.360345	47.586599
2243.964646	40670.290922	47.591604
2240.033385	39605.440010	47.596609
2236.584439	38541.529320	47.601613
2232.489586	37495.719779	47.606618
2228.700864	36444.866857	47.611623
2225.169370	35395.324726	47.616628
2221.244157	34352.640393	47.621633
2217.642274	33319.857554	47.626637
2213.588628	32293.946198	47.631642
2209.557267	31285.181265	47.636647
2205.689946	30279.513208	47.641652
2201.521002	29288.098645	47.646657
2197.305168	28301.428438	47.651661
2192.472451	27353.980657	47.656666
2187.310722	26430.643359	47.661671
2181.915734	25529.687735	47.666676
2176.499814	24646.661675	47.671681
2171.580566	23782.014212	47.676685
2166.355993	22955.679198	47.681690
2162.209275	22163.387511	47.686695
2157.367977	21383.569983	47.691700
2152.711217	20638.157464	47.696705
2148.524089	19896.569924	47.701709
2144.556312	19192.873117	47.706714
2140.197600	18497.743854	47.711719
2136.199331	17820.754293	47.716724
2131.845422	17164.491048	47.721729
2128.203119	16520.786201	47.726733
2123.932459	15890.677841	47.731738
2120.406591	15266.451769	47.736743
2116.644887	14662.389037	47.741748
2112.457979	14069.268878	47.746753
2108.346615	13494.556879	47.751757
2104.841130	12921.103497	47.756762
2101.227051	12359.733999	47.761767
2097.796154	11800.616061	47.766772
2094.015555	11261.257238	47.771777
2090.530913	10717.245675	47.776781
2086.520910	10199.704502	47.781786
2083.090820	9678.924561	47.786791
2078.950121	9155.538566	47.791796
2075.158948	8653.253733	47.796801
2071.051647	8157.368727	47.801805
2067.227586	7677.025206	47.806810
2063.163135	7213.971912	47.811815
2058.928533	6760.227125	47.816820
2054.133423	6330.742218	47.821825
2049.469490	5917.052085	47.826829
2045.481421	5516.696865	47.831834
2041.231971	5122.002333	47.836839
2037.143926	4770.877792	47.841844
2032.557094	4420.227301	47.846849
2028.572438	4070.451361	47.851853
2024.286131	3746.317282	47.856858
2020.387486	3436.507463	47.861863
2016.839234	3126.350664	47.866868
2012.807975	2844.025807	47.871873
2009.119523	2547.947281	47.876877
2005.223699	2272.486125	47.881882
2001.690966	2004.553720	47.886887
1998.107494	1740.854187	47.891892
1994.421045	1488.929192	47.896897
1990.903403	1235.778986	47.901901
1987.077976	989.881762	47.906906
1983.587429	752.908479	47.911911
1979.718460	530.336393	47.916916
1974.854995	336.679155	47.921921
1970.179372	163.502677	47.926925
1960.407274	132.406128	47.931930
1950.998270	139.266351	47.936935
1945.245812	141.425599	47.941940
1941.116972	149.753389	47.946945
1938.871888	142.618949	47.951949
1937.544686	142.826533	47.956954
1935.363316	142.459076	47.961959
1933.086554	134.342480	47.966964
1929.750466	150.572889	47.971969
1926.141756	144.556692	47.976973
1923.232454	142.379528	47.981978
1919.956656	138.709434	47.986983
1917.368092	138.940388	47.991988
1913.833480	145.213617	47.996993
1910.479896	139.515020	48.001997
1906.941011	142.887678	48.007002
1903.547940	148.037746	48.012007
1900.289948	142.678543	48.017012
1896.758402	146.423389	48.022017
1893.568396	136.367903	48.027021
1890.492599	142.379511	48.032026
1887.260981	138.313361	48.037031
1884.065428	140.505973	48.042036
1880.104222	138.205520	48.047041
1876.819509	138.143612	48.052045
1873.419289	141.266785	48.057050
1869.931448	137.658363	48.062055
1866.675314	144.767576	48.067060
1863.147109	142.101969	48.072065
1859.837236	142.724229	48.077069
1856.692215	141.998209	48.082074
1852.754829	141.098783	48.087079
1849.296466	134.147907	48.092084
1845.262357	141.018189	48.097089
1842.568422	132.425886	48.102093
1839.455658	138.193346	48.107098
1836.254101	147.369505	48.112103
1832.554626	141.032182	48.117108
1829.045443	145.150046	48.122113
1825.635722	136.831115	48.127117
1822.573804	136.971647	48.132122
1818.084895	148.605085	48.137127
1815.381779	135.727223	48.142132
1811.824221	139.020571	48.147137
1808.020589	133.028601	48.152141
1804.831254	139.909068	48.157146
1800.863381	143.573524	48.162151
1797.905125	141.188918	48.167156
1794.029846	143.674594	48.172161
1791.215416	134.854383	48.177165
1787.683514	134.786894	48.182170
1784.206963	138.700341	48.187175
1780.710324	131.894691	48.192180
1777.004131	141.399775	48.197185
1773.864764	134.025675	48.202189
1770.767148	134.026272	48.207194
1766.510128	140.175307	48.212199
1763.007238	139.116168	48.217204
1759.221868	140.315923	48.222209
1756.034878	127.573927	48.227213
1752.679465	137.090561	48.232218
1749.092802	138.490182	48.237223
1746.089676	125.741564	48.242228
1742.533853	140.035316	48.247233
1739.443952	133.751338	48.252237
1735.699613	135.004793	48.257242
1732.017692	139.061130	48.262247
1728.292691	130.430904	48.267252
1724.716346	130.190053	48.272257
1721.104759	133.134371	48.277261
1717.862706	126.668566	48.282266
1714.555884	132.722697	48.287271
1711.156766	133.314677	48.292276
1707.923813	126.246322	48.297281
1703.944165	131.225643	48.302285
1700.634474	133.088148	48.307290
1697.328936	137.553839	48.312295
1693.537623	126.238422	48.317300
1690.217923	131.165086	48.322305
1686.541265	128.468993	48.327309
1683.215078	122.396029	48.332314
1679.807193	137.229803	48.337319
1676.552808	125.175449	48.342324
1672.493986	128.104353	48.347329
1669.693022	122.006144	48.352333
1665.711714	122.268464	48.357338
1662.059377	123.216473	48.362343
1659.013117	123.648839	48.367348
1655.161350	124.039590	48.372353
1651.678068	124.249282	48.377357
1647.896236	123.297118	48.382362
1644.452140	136.105385	48.387367
1641.245216	126.153895	48.392372
1638.136176	135.249172	48.397377
1635.105528	127.193705	48.402381
1631.293116	127.527684	48.407386
1627.472378	127.806018	48.412391
1623.785565	129.072656	48.417396
1620.243792	124.637518	48.422401
1617.244947	127.802353	48.427405
1613.960007	133.473426	48.432410
1609.806319	136.796862	48.437415
1606.553828	126.184948	48.442420
1602.637756	119.350105	48.447425
1599.349761	116.045876	48.452429
1595.884645	120.245495	48.457434
1592.181585	119.284187	48.462439
1588.931559	121.143714	48.467444
1584.796265	117.624081	48.472449
1581.637082	121.158876	48.477453
1578.533027	126.393512	48.482458
1574.871847	125.650287	48.487463
1571.616449	123.252147	48.492468
1568.225878	118.787038	48.497473
1564.191258	119.456384	48.502477
1561.019235	115.615149	48.507482
1557.488213	122.495366	48.512487
1553.972439	116.705233	48.517492
1550.584651	117.621366	48.522497
1547.141308	132.163312	48.527501
1543.600378	117.879076	48.532506
1540.146795	125.066724	48.537511
1536.645263	113.408634	48.542516
1533.138750	118.307629	48.547521
1529.469288	122.355751	48.552525
1525.728405	123.001284	48.557530
1522.387338	119.487084	48.562535
1518.910110	120.705134	48.567540
1515.497681	116.790809	48.572545
1512.413388	130.260975	48.577549
1508.859006	121.626292	48.582554
1505.141714	128.080089	48.587559
1501.362388	118.854181	48.592564
1497.722208	122.891403	48.597569
1494.659526	125.616998	48.602573
1491.206311	119.032468	48.607578
1487.612972	133.357455	48.612583
1483.914924	115.905539	48.617588
1480.436386	130.975038	48.622593
1476.976922	124.416800	48.627597
1473.924026	118.981363	48.632602
1469.675404	126.157430	48.637607
1466.488817	117.670847	48.642612
1463.023822	123.939630	48.647617
1459.805021	117.065316	48.652621
1456.367865	111.047778	48.657626
1452.523700	122.798707	48.662631
1448.984143	116.803525	48.667636
1445.109086	127.600657	48.672641
1442.115297	122.298350	48.677645
1438.876073	118.948577	48.682650
1434.771062	125.637095	48.687655
1431.794037	117.320208	48.692660
1428.097087	114.795077	48.697665
1424.523863	115.265704	48.702669
1421.272657	118.308736	48.707674
1417.601893	126.799108	48.712679
1414.488027	124.669939	48.717684
1410.530675	111.048917	48.722689
1406.585509	122.404372	48.727693
1403.536542	113.367916	48.732698
1400.132559	112.366193	48.737703
1396.794848	116.156780	48.742708
1393.275705	113.550045	48.747713
1389.558940	107.171333	48.752717
1386.277127	108.678385	48.757722
1382.479179	124.686931	48.762727
1379.083486	115.575040	48.767732
1375.312352	107.562821	48.772737
1372.185551	119.647579	48.777741
1368.634978	115.166462	48.782746
1365.059190	122.841534	48.787751
1361.608409	116.623679	48.792756
1357.938491	116.502012	48.797761
1354.561036	111.421151	48.802765
1351.403372	105.622503	48.807770
1347.598807	120.629160	48.812775
1343.926537	111.478321	48.817780
1340.481393	122.742869	48.822785
1336.968203	114.914917	48.827789
1333.670008	108.170144	48.832794
1330.209033	116.501145	48.837799
1326.651620	111.201687	48.842804
1323.002901	111.779082	48.847809
1319.488378	107.653019	48.852813
1316.151565	107.105893	48.857818
1312.654968	120.849444	48.862823
1309.011246	109.346598	48.867828
1305.695724	120.476964	48.872833
1301.999321	113.228213	48.877837
1298.389333	119.174884	48.882842
1295.170747	115.768147	48.887847
1291.606433	103.066450	48.892852
1288.139809	110.322647	48.897857
1284.774807	113.269636	48.902861
1281.359855	101.942971	48.907866
1277.455866	109.245489	48.912871
1274.055678	104.861097	48.917876
1270.639848	109.882019	48.922881
1266.960929	108.613329	48.927885
1263.662587	106.155581	48.932890
1259.722246	106.633115	48.937895
1256.426631	108.442931	48.942900
1252.592891	111.172238	48.947905
1248.895655	112.693745	48.952909
1246.065427	106.407270	48.957914
1242.870436	112.659157	48.962919
1239.957481	110.732720	48.967924
1236.193241	115.646842	48.972929
1232.169870	115.523604	48.977933
1228.535656	113.763866	48.982938
1224.519195	115.215131	48.987943
1221.576527	113.312333	48.992948
1218.380441	109.158606	48.997953
1214.715636	102.249807	49.002957
1211.050360	111.935297	49.007962
1207.072311	104.078937	49.012967
1203.752705	105.139538	49.017972
1200.413443	107.253604	49.022977
1196.729109	115.480400	49.027981
1193.786496	99.618851	49.032986
1190.040036	103.014735	49.037991
1186.983316	101.319634	49.042996
1183.497265	109.613469	49.048001
1179.312871	112.062333	49.053005
1176.081608	105.025566	49.058010
1172.417297	110.727673	49.063015
1168.981340	102.093591	49.068020
1165.388290	96.562497	49.073025
1162.117877	104.047442	49.078029
1158.558997	106.278163	49.083034
1154.866997	102.480513	49.088039
1151.465451	98.890500	49.093044
1148.266517	108.249892	49.098049
1144.034043	104.017996	49.103053
1141.055244	106.898240	49.108058
1137.598127	111.052454	49.113063
1134.049678	109.658984	49.118068
1130.504158	107.274783	49.123073
1126.876430	102.653983	49.128077
1123.799380	102.588284	49.133082
1119.699956	107.352436	49.138087
1116.356955	103.341973	49.143092
1113.043879	99.491346	49.148097
1109.159204	103.510022	49.153101
1106.343890	100.606543	49.158106
1102.397686	111.171292	49.163111
1099.334073	100.488907	49.168116
1095.369432	107.699740	49.173121
1091.856434	103.674772	49.178125
1088.735471	100.727400	49.183130
1084.818465	104.425275	49.188135
1081.479643	106.570949	49.193140
1077.745582	104.839558	49.198145
1074.383511	104.169918	49.203149
1071.295459	98.844542	49.208154
1067.309614	109.497766	49.213159
1064.203120	103.792457	49.218164
1060.375553	98.437332	49.223169
1056.996542	107.242799	49.228173
1053.678960	94.107117	49.233178
1049.944652	109.840009	49.238183
1046.411923	102.923261	49.243188
1042.656824	116.137859	49.248193
1039.203233	113.593764	49.253197
1035.985055	98.227855	49.258202
1032.231216	101.558511	49.263207
1028.993716	94.908768	49.268212
1025.557226	104.289564	49.273217
1021.659265	99.056210	49.278221
1018.482572	99.917323	49.283226
1015.058137	93.730296	49.288231
1011.733804	95.481411	49.293236
1007.976387	101.704357	49.298241
1004.261302	99.204384	49.303245
1001.071324	94.451824	49.308250
997.430850	98.024174	49.313255
993.846706	96.731262	49.318260
990.366695	99.180650	49.323265
986.779356	104.962516	49.328269
983.648461	95.856802	49.333274
980.008741	106.303997	49.338279
976.373551	103.946551	49.343284
973.027106	99.528552	49.348289
969.289834	104.802380	49.353293
966.090510	100.048131	49.358298
962.443024	101.688506	49.363303
958.380113	97.259305	49.368308
955.440703	99.617733	49.373313
951.513026	97.122594	49.378317
948.480717	96.464643	49.383322
944.771359	107.533367	49.388327
941.619455	101.718154	49.393332
937.994207	103.256979	49.398337
934.230088	94.215633	49.403341
930.708212	95.928102	49.408346
927.187324	103.107476	49.413351
923.810979	96.849679	49.418356
920.435524	101.408798	49.423361
916.802404	99.225062	49.428365
913.536126	106.076668	49.433370
909.784041	103.588854	49.438375
906.360582	101.318509	49.443380
903.118924	99.731556	49.448385
899.421470	102.876259	49.453389
895.816152	106.974661	49.458394
891.716904	101.307804	49.463399
888.658582	89.061766	49.468404
885.219096	98.908147	49.473409
881.932387	102.887061	49.478413
878.740326	96.299866	49.483418
875.047960	107.815210	49.488423
871.318025	97.335335	49.493428
867.853290	96.729303	49.498433
863.768921	100.757192	49.503437
860.826995	89.837557	49.508442
857.185118	101.740472	49.513447
853.737053	97.980685	49.518452
850.382739	91.887152	49.523457
846.715788	97.083569	49.528461
843.733772	89.818084	49.533466
839.576435	99.621858	49.538471
836.035702	94.187118	49.543476
833.192999	96.925914	49.548481
829.264750	101.669701	49.553485
825.851406	97.420426	49.558490
821.985939	103.824873	49.563495
818.647060	98.481920	49.568500
815.364496	102.817716	49.573505
811.821678	96.389878	49.578509
808.154012	85.935092	49.583514
804.721565	97.381276	49.588519
801.119901	95.012325	49.593524
797.794272	100.436890	49.598529
794.022244	94.434101	49.603533
790.990310	84.041128	49.608538
787.155364	97.439133	49.613543
783.731900	99.386185	49.618548
780.292551	92.783970	49.623553
776.936622	99.279487	49.628557
773.316640	93.252898	49.633562
769.822308	102.769375	49.638567
766.019648	98.008441	49.643572
762.474493	99.088692	49.648577
759.170299	93.262598	49.653581
755.657170	91.832107	49.658586
752.583350	99.495189	49.663591
748.980925	99.676403	49.668596
745.179509	99.676805	49.673601
741.491819	90.655223	49.678605
737.950473	89.510736	49.683610
734.242973	101.452437	49.688615
731.209088	96.571129	49.693620
728.066560	99.189226	49.698625
724.333164	96.628961	49.703629
721.047431	88.911205	49.708634
717.277601	103.577213	49.713639
713.833351	90.803219	49.718644
710.000425	92.384142	49.723649
706.259576	96.165306	49.728653
703.073255	89.327345	49.733658
699.719643	102.181759	49.738663
696.192879	90.135715	49.743668
693.057403	88.358201	49.748673
689.026113	90.150534	49.753677
686.185093	85.555423	49.758682
682.299938	90.972731	49.763687
678.243088	84.770991	49.768692
675.102628	90.736076	49.773697
671.631732	89.510978	49.778701
667.933224	90.245116	49.783706
664.018103	95.474134	49.788711
660.867416	96.761570	49.793716
657.901343	88.560339	49.798721
654.515332	95.943303	49.803725
650.743734	90.446721	49.808730
647.007759	97.036597	49.813735
643.438260	97.968843	49.818740
640.088305	87.040434	49.823745
636.637638	88.501409	49.828749
633.291273	86.959427	49.833754
629.372451	93.653874	49.838759
625.951022	97.192053	49.843764
622.420138	99.244572	49.848769
618.926844	102.325767	49.853773
615.392850	97.522825	49.858778
612.488775	98.866568	49.863783
608.767901	96.687212	49.868788
605.743565	93.965330	49.873793
601.860864	107.519575	49.878797
598.196307	95.615380	49.883802
593.913843	97.111727	49.888807
590.997519	88.988154	49.893812
587.764471	87.779624	49.898817
583.624888	95.138258	49.903821
580.734302	85.694521	49.908826
576.935857	98.251631	49.913831
573.529979	92.058720	49.918836
570.230650	83.245323	49.923841
566.595808	94.093673	49.928845
563.192262	94.123587	49.933850
559.277875	84.631393	49.938855
555.703985	90.215137	49.943860
552.652373	91.895222	49.948865
549.440335	95.903676	49.953869
545.695056	101.944545	49.958874
542.002724	92.898475	49.963879
538.513250	90.973976	49.968884
535.067357	96.107406	49.973889
531.086943	99.486391	49.978893
528.183678	92.240330	49.983898
524.452586	98.000571	49.988903
520.805957	98.451392	49.993908
517.488418	99.685914	49.998913
514.027691	91.619161	50.003917
510.837558	85.727851	50.008922
507.249360	92.471802	50.013927
503.344362	88.771071	50.018932
499.796635	94.107125	50.023937
496.309947	98.418044	50.028941
492.910575	92.534201	50.033946
489.161981	91.893677	50.038951
485.727823	85.167392	50.043956
482.748712	95.220193	50.048961
478.883575	104.048179	50.053965
475.551871	94.654587	50.058970
471.621892	89.774525	50.063975
467.975949	92.531664	50.068980
464.858081	87.495933	50.073985
460.843471	87.593121	50.078989
457.999516	86.428100	50.083994
454.683792	94.318977	50.088999
451.171630	88.047854	50.094004
447.874881	88.494524	50.099009
443.842391	91.119226	50.104013
440.326597	79.188657	50.109018
436.583317	89.471891	50.114023
433.539515	88.037621	50.119028
430.136017	88.289043	50.124033
426.305368	95.273480	50.129037
423.074936	85.234460	50.134042
419.636175	84.020247	50.139047
415.743566	87.157731	50.144052
412.262939	78.043770	50.149057
408.791084	88.221223	50.154061
405.611250	90.494085	50.159066
401.801567	94.074172	50.164071
398.183706	101.661213	50.169076
395.043129	89.738328	50.174081
391.647464	89.188099	50.179085
387.775668	85.517023	50.184090
384.027186	96.835653	50.189095
380.469573	98.354603	50.194100
377.426087	93.955830	50.199105
373.881305	92.378587	50.204109
370.613717	95.924395	50.209114
367.173155	104.021520	50.214119
362.739125	94.617147	50.219124
359.646692	98.088066	50.224129
356.084790	95.981994	50.229133
352.791142	88.496593	50.234138
349.709073	85.720572	50.239143
346.244301	91.034194	50.244148
342.984642	93.382857	50.249153
338.797899	96.357637	50.254157
335.087234	88.861635	50.259162
331.486945	94.035137	50.264167
328.228016	97.133509	50.269172
325.268306	79.610899	50.274177
320.990839	96.764174	50.279181
317.951737	88.030348	50.284186
314.106417	95.706831	50.289191
310.711585	92.660273	50.294196
307.411868	91.981150	50.299201
303.921508	97.188064	50.304205
300.589276	87.955991	50.309210
296.677237	94.576735	50.314215
293.058279	94.735408	50.319220
289.681995	90.300215	50.324225
286.130075	91.600009	50.329229
282.639936	98.844375	50.334234
279.736292	88.798520	50.339239
275.806852	88.363589	50.344244
272.109359	86.104786	50.349249
268.339959	91.782533	50.354253
265.472621	81.851225	50.359258
261.685991	88.781368	50.364263
258.480944	90.713376	50.369268
254.883002	81.367926	50.374273
250.965406	92.573881	50.379277
247.699189	86.343417	50.384282
244.151985	93.261372	50.389287
240.813736	83.742367	50.394292
237.912532	92.378302	50.399297
233.617286	85.647814	50.404301
230.210277	82.312131	50.409306
226.664650	88.429405	50.414311
222.807973	92.184606	50.419316
219.650212	91.340908	50.424321
216.177033	89.145067	50.429325
212.666678	82.282143	50.434330
209.145252	84.820556	50.439335
205.756973	89.065539	50.444340
202.273899	85.495008	50.449345
198.055113	95.134637	50.454349
195.500745	93.781966	50.459354
191.999654	92.087221	50.464359
188.289028	88.837084	50.469364
185.141824	78.943326	50.474369
180.998247	87.732773	50.479373
177.747788	80.867116	50.484378
173.784651	81.193654	50.489383
170.761206	82.856795	50.494388
167.694097	90.031760	50.499393
163.527756	90.203474	50.504397
160.025468	82.624295	50.509402
156.619415	94.762555	50.514407
152.807815	88.124021	50.519412
149.519958	83.890173	50.524417
145.675329	92.778337	50.529421
142.626896	83.549335	50.534426
139.294245	84.349759	50.539431
135.713218	85.268190	50.544436
132.293697	80.390584	50.549441
128.559287	92.912490	50.554445
125.171411	85.666581	50.559450
121.472880	87.590527	50.564455
117.902023	90.481572	50.569460
114.517973	84.747357	50.574465
110.781761	83.554559	50.579469
107.620229	78.048082	50.584474
104.176721	84.411993	50.589479
100.623316	87.335112	50.594484
97.101199	84.403500	50.599489
93.560361	91.605249	50.604493
90.056080	88.411415	50.609498
86.770408	86.233708	50.614503
83.310178	88.632867	50.619508
79.551380	84.526615	50.624513
76.054505	86.532882	50.629517
72.798485	85.967227	50.634522
68.978378	86.584618	50.639527
65.516528	89.863569	50.644532
62.214493	84.600586	50.649537
58.126584	83.763472	50.654541
54.892392	89.009431	50.659546
51.813598	85.941942	50.664551
47.929518	84.832450	50.669556
44.444107	88.418823	50.674561
40.769814	89.105130	50.679565
37.433240	87.343546	50.684570
33.969305	85.212772	50.689575
30.343283	91.538868	50.694580
27.239618	86.504249	50.699585
23.763345	94.205276	50.704589
20.181066	78.995006	50.709594
16.440192	81.143929	50.714599
12.893216	90.732156	50.719604
9.538752	82.867293	50.724609
5.962723	92.754307	50.729613
2.625895	83.067511	50.734618