Thu Aug 25 12:52:15 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
0.659125	101.000746	0.000000
0.429081	106.143100	0.005005
0.742386	110.124636	0.010010
0.380047	97.551560	0.015014
0.032921	97.821052	0.020019
0.357634	84.982146	0.025024
0.490825	81.205840	0.030029
-0.309705	79.246307	0.035034
-0.115992	59.379051	0.040038
-0.649830	71.516643	0.045043
-0.595842	59.289653	0.050048
-0.961763	51.744407	0.055053
-1.398093	49.433583	0.060058
-1.568595	41.095254	0.065062
-1.963771	34.016510	0.070067
-1.871411	27.721925	0.075072
-2.233887	26.785263	0.080077
-2.580522	9.802660	0.085082
-2.685430	2.861947	0.090086
-3.147832	1.513835	0.095091
-3.219182	-6.359115	0.100096
-4.074285	-2.593168	0.105101
-4.246389	3.201305	0.110106
-4.909995	-1.405595	0.115110
-5.453277	-1.839362	0.120115
-5.235998	-0.092241	0.125120
-5.316618	-3.986889	0.130125
-5.565478	2.819359	0.135130
-5.478078	-8.979383	0.140134
-5.445106	8.185158	0.145139
-6.042271	-8.065308	0.150144
-6.392389	-5.859125	0.155149
-7.078982	-4.100096	0.160154
-6.635744	-9.411931	0.165158
-7.272563	-1.178153	0.170163
-7.668791	-2.701148	0.175168
-8.226221	-7.593602	0.180173
-8.531250	8.965837	0.185178
-8.116577	3.161763	0.190182
-8.381215	3.405676	0.195187
-8.078158	0.653141	0.200192
-8.842705	-3.162821	0.205197
-9.544828	-0.097888	0.210202
-9.608271	-4.501429	0.215206
-9.770266	-0.923175	0.220211
-9.600506	-8.457414	0.225216
-10.228581	5.226159	0.230221
-10.636266	0.284930	0.235226
-11.398488	-12.658846	0.240230
-11.455169	-0.172123	0.245235
-11.434391	1.969620	0.250240
-10.837945	5.495478	0.255245
-11.476380	4.782391	0.260250
-11.873158	0.092554	0.265254
-12.062196	-2.424688	0.270259
-12.299862	-8.566310	0.275264
-12.388064	-0.073641	0.280269
-13.107919	2.927632	0.285274
-13.367549	-2.546159	0.290278
-14.010715	-1.920233	0.295283
-13.836447	-4.769648	0.300288
-13.758546	-4.003602	0.305293
-14.123152	2.577172	0.310298
-14.359597	-0.002246	0.315302
-15.147668	-6.408805	0.320307
-15.292948	0.371721	0.325312
-15.518439	-0.981873	0.330317
-15.293990	-3.105157	0.335322
-15.707051	-1.126393	0.340326
-15.885616	0.689078	0.345331
-16.833113	2.381420	0.350336
-16.774143	3.311785	0.355341
-16.452479	-1.772195	0.360346
-16.399015	-7.605091	0.365350
-17.764344	-3.594683	0.370355
-18.173720	2.161036	0.375360
-17.984013	7.832380	0.380365
-18.199578	-5.870935	0.385370
-18.362101	-1.223247	0.390374
-18.762399	5.869323	0.395379
-18.566317	5.215305	0.400384
-18.690210	1.994990	0.405389
-19.264768	3.154334	0.410394
-19.479278	-0.020144	0.415398
-19.737054	-1.688219	0.420403
-19.834265	3.838254	0.425408
-20.071564	-1.730785	0.430413
-20.785862	2.421227	0.435418
-20.850601	3.187477	0.440422
-21.450764	1.383223	0.445427
-21.470883	5.217659	0.450432
-21.702082	2.229294	0.455437
-21.550845	8.805175	0.460442
-21.861377	-6.208877	0.465446
-22.407658	2.665616	0.470451
-22.839629	5.441448	0.475456
-22.881784	3.018250	0.480461
-22.899305	8.079819	0.485466
-22.631798	0.780199	0.490470
-23.340569	1.821366	0.495475
-24.085937	-2.323466	0.500480
-24.229992	6.304507	0.505485
-24.241997	-0.521045	0.510490
-24.544044	9.052339	0.515494
-24.609715	9.328352	0.520499
-25.205315	7.846087	0.525504
-25.788149	2.679201	0.530509
-26.066016	4.801298	0.535514
-26.115685	0.917619	0.540518
-25.936804	8.950826	0.545523
-25.672984	-0.834934	0.550528
-26.422754	-1.511593	0.555533
-27.024988	-3.207953	0.560538
-27.239800	-2.975011	0.565542
-27.196535	2.374426	0.570547
-27.111215	-4.640381	0.575552
-27.471565	6.754972	0.580557
-28.392333	8.430473	0.585562
-28.603558	6.843689	0.590566
-28.832739	9.904124	0.595571
-28.821582	9.010161	0.600576
-28.971515	-0.796192	0.605581
-29.054576	7.920302	0.610586
-29.275837	1.779271	0.615590
-29.953355	12.964897	0.620595
-29.924905	5.326243	0.625600
-30.019767	1.025701	0.630605
-30.872926	4.139612	0.635610
-31.441347	-3.263146	0.640614
-31.303550	5.548454	0.645619
-31.954569	-1.556624	0.650624
-31.763510	-0.757688	0.655629
-31.808280	7.193502	0.660634
-31.814576	5.868838	0.665638
-31.786555	1.014366	0.670643
-32.103772	2.617444	0.675648
-32.842330	5.052172	0.680653
-33.253298	3.990233	0.685658
-33.080881	0.524174	0.690662
-33.305835	11.417424	0.695667
-33.984914	-1.659607	0.700672
-34.762920	9.443685	0.705677
-34.759458	8.734426	0.710682
-34.611897	4.009920	0.715686
-34.864603	9.589232	0.720691
-34.810186	2.054080	0.725696
-34.837082	7.022205	0.730701
-35.719080	6.609875	0.735706
-36.197475	5.925497	0.740710
-36.563313	15.695542	0.745715
-36.315039	4.206946	0.750720
-36.382324	2.581790	0.755725
-36.564448	10.912008	0.760730
-36.696846	5.022810	0.765734
-37.671526	5.820905	0.770739
-37.882193	0.570397	0.775744
-37.929933	6.538373	0.780749
-38.226597	4.531541	0.785754
-38.090186	3.257284	0.790758
-38.653226	11.476344	0.795763
-39.142289	8.800467	0.800768
-39.076361	8.650898	0.805773
-39.474911	11.045007	0.810778
-39.279477	6.078880	0.815782
-39.473918	16.135282	0.820787
-39.887155	10.002184	0.825792
-40.612815	14.753931	0.830797
-40.737739	10.840913	0.835802
-40.560193	7.383541	0.840806
-40.803021	20.206328	0.845811
-40.885387	10.411530	0.850816
-41.715331	7.023434	0.855821
-42.432620	14.962944	0.860826
-41.893987	10.572630	0.865830
-42.271910	11.770768	0.870835
-42.636946	5.829436	0.875840
-43.031868	13.832330	0.880845
-43.428709	10.256148	0.885850
-43.592970	6.001281	0.890854
-43.853657	13.005538	0.895859
-43.884583	9.118921	0.900864
-43.834912	11.499747	0.905869
-44.064704	20.100030	0.910874
-44.444160	7.668912	0.915878
-45.125585	22.920591	0.920883
-45.299561	14.114586	0.925888
-45.201243	8.711257	0.930893
-45.511217	12.790429	0.935898
-45.770819	-1.216035	0.940902
-46.466022	7.552080	0.945907
-46.841444	3.766900	0.950912
-46.694986	8.938817	0.955917
-46.784297	5.972513	0.960922
-46.677715	8.024881	0.965926
-47.006999	14.751984	0.970931
-47.450118	11.455138	0.975936
-47.688157	10.432542	0.980941
-48.109710	17.541101	0.985946
-47.996230	9.006433	0.990950
-49.149518	18.089940	0.995955
-49.715776	11.395523	1.000960
-49.676090	13.828533	1.005965
-50.097636	20.718793	1.010970
-49.242874	21.945247	1.015974
-49.467120	18.395804	1.020979
-49.735061	0.521362	1.025984
-49.908160	25.301741	1.030989
-50.426500	19.352789	1.035994
-50.818409	10.868837	1.040998
-50.853337	15.844549	1.046003
-51.305032	17.940102	1.051008
-51.839112	7.931346	1.056013
-52.391390	19.331469	1.061018
-52.793434	14.639294	1.066022
-52.822179	14.745005	1.071027
-53.054487	12.766055	1.076032
-52.885525	6.111463	1.081037
-52.942345	15.257282	1.086042
-53.130279	11.471196	1.091046
-53.436575	21.279370	1.096051
-53.967549	11.067646	1.101056
-54.093423	9.714262	1.106061
-54.231428	12.709791	1.111066
-54.108620	5.641650	1.116070
-55.021065	12.551878	1.121075
-55.451057	13.229826	1.126080
-55.454939	14.359865	1.131085
-55.673512	20.465345	1.136090
-55.649262	7.727361	1.141094
-55.675006	5.687571	1.146099
-56.421495	6.392965	1.151104
-56.754106	2.677008	1.156109
-57.176253	15.939177	1.161114
-56.869253	6.216251	1.166118
-57.108147	12.065483	1.171123
-57.602891	10.782553	1.176128
-57.801776	3.426298	1.181133
-58.223534	10.345060	1.186138
-58.286571	-0.832160	1.191142
-58.485161	10.920664	1.196147
-58.907642	11.581617	1.201152
-59.516918	8.972034	1.206157
-59.659025	14.182840	1.211162
-59.398194	9.855037	1.216166
-59.735056	15.292512	1.221171
-59.360671	11.260129	1.226176
-60.446978	2.359803	1.231181
-60.779569	3.756482	1.236186
-60.685260	0.147638	1.241190
-61.014321	9.260181	1.246195
-61.570850	5.661567	1.251200
-62.156537	5.566644	1.256205
-62.721151	13.861882	1.261210
-62.127377	6.352949	1.266214
-62.433853	13.981314	1.271219
-62.853729	11.161719	1.276224
-62.492651	14.031590	1.281229
-62.587241	10.502963	1.286234
-63.279492	0.427248	1.291238
-63.965553	10.522712	1.296243
-64.516397	2.424338	1.301248
-64.323271	2.235855	1.306253
-64.346754	7.880490	1.311258
-63.982242	-0.620740	1.316262
-65.073532	1.995810	1.321267
-65.558882	2.093973	1.326272
-65.574383	0.982725	1.331277
-66.380541	5.478164	1.336282
-65.846501	-1.850562	1.341286
-66.191753	8.185171	1.346291
-65.928674	9.194285	1.351296
-65.698817	3.631142	1.356301
-67.087321	13.156465	1.361306
-67.320869	3.413837	1.366310
-67.418269	13.005775	1.371315
-67.299528	7.846021	1.376320
-68.097884	11.527153	1.381325
-68.888004	10.306325	1.386330
-68.677029	0.962282	1.391334
-68.647053	11.458079	1.396339
-69.256976	-1.572833	1.401344
-69.021386	0.019555	1.406349
-69.076787	9.335991	1.411354
-68.899286	1.847994	1.416358
-69.976301	2.734894	1.421363
-70.096533	6.392026	1.426368
-69.886800	12.376606	1.431373
-70.795103	2.802982	1.436378
-71.082824	-5.425202	1.441382
-71.571410	9.739301	1.446387
-71.543845	6.428816	1.451392
-71.568861	-1.774095	1.456397
-71.734466	4.414828	1.461402
-72.128062	-0.177425	1.466406
-73.026390	8.217557	1.471411
-73.459581	8.952956	1.476416
-73.521602	6.244969	1.481421
-73.393578	6.705767	1.486426
-73.059556	5.622009	1.491430
-73.234954	4.421919	1.496435
-73.708381	2.983790	1.501440
-73.734246	1.402765	1.506445
-74.844659	6.834897	1.511450
-74.696263	3.806038	1.516454
-74.942874	5.008911	1.521459
-75.148744	0.523285	1.526464
-74.988894	-8.499530	1.531469
-75.731565	5.274762	1.536474
-76.141775	-5.041294	1.541478
-76.417379	-2.160249	1.546483
-76.730300	-2.149215	1.551488
-76.388402	-4.009328	1.556493
-76.751105	-3.781686	1.561498
-77.324460	-4.682135	1.566502
-77.825066	4.365535	1.571507
-77.910059	0.715184	1.576512
-77.883829	6.067289	1.581517
-77.872583	-1.432621	1.586522
-78.145348	4.339658	1.591526
-78.935346	1.672974	1.596531
-79.184756	1.417792	1.601536
-79.635162	-2.570771	1.606541
-79.504190	13.610298	1.611546
-79.435717	-1.292292	1.616550
-79.510288	3.974366	1.621555
-80.335182	6.023992	1.626560
-80.559592	4.803108	1.631565
-80.988535	6.496461	1.636570
-80.929109	0.694269	1.641574
-81.290267	3.414714	1.646579
-81.224005	4.280659	1.651584
-81.611663	4.123070	1.656589
-82.339990	5.319167	1.661594
-82.362227	-0.944793	1.666598
-82.348546	16.229095	1.671603
-82.410970	4.485465	1.676608
-82.556017	0.407925	1.681613
-83.261488	5.570962	1.686618
-83.595890	3.174575	1.691622
-83.832461	12.902215	1.696627
-83.487918	13.756194	1.701632
-83.905835	13.641311	1.706637
-84.915386	14.330980	1.711642
-85.065350	1.465278	1.716646
-85.268217	8.125114	1.721651
-85.257703	6.797817	1.726656
-85.263576	9.234801	1.731661
-85.374229	18.588371	1.736666
-85.895325	5.176542	1.741670
-86.487024	9.654198	1.746675
-86.836251	14.119172	1.751680
-86.706102	12.453589	1.756685
-86.625320	17.781330	1.761690
-86.841648	14.540699	1.766694
-87.654527	20.135022	1.771699
-88.125551	10.749143	1.776704
-88.080394	7.148000	1.781709
-88.381929	17.072483	1.786714
-88.293602	20.260339	1.791718
-88.582312	11.602031	1.796723
-88.792468	15.077102	1.801728
-89.381890	17.374571	1.806733
-90.105826	20.765634	1.811738
-89.814443	12.627035	1.816742
-90.146665	21.417375	1.821747
-90.093094	15.223789	1.826752
-90.020495	11.972686	1.831757
-90.506040	22.754911	1.836762
-90.729585	8.375801	1.841766
-91.088503	11.791923	1.846771
-91.435694	15.626990	1.851776
-91.683230	12.619040	1.856781
-92.453501	8.718562	1.861786
-92.563772	13.354901	1.866790
-92.836799	6.848662	1.871795
-92.950354	9.489180	1.876800
-92.567632	13.165580	1.881805
-92.964930	14.670477	1.886810
-93.217669	17.687148	1.891814
-93.997292	15.695884	1.896819
-94.334105	19.659039	1.901824
-94.210198	9.379507	1.906829
-94.413421	12.274523	1.911834
-94.021698	2.437084	1.916838
-94.956528	10.932701	1.921843
-95.341028	11.578213	1.926848
-95.508595	8.567225	1.931853
-96.136746	11.506678	1.936858
-95.532408	3.107074	1.941862
-96.232652	1.657031	1.946867
-96.767935	9.507908	1.951872
-96.683159	6.090383	1.956877
-97.307868	13.392125	1.961882
-97.469166	-0.655045	1.966886
-97.656709	3.427086	1.971891
-97.416711	5.230756	1.976896
-97.546022	1.818304	1.981901
-98.930044	15.364069	1.986906
-98.530576	9.714237	1.991910
-99.137493	7.778169	1.996915
-98.928186	9.779718	2.006912
-98.826319	13.232445	2.016909
-97.788703	11.381344	2.026906
-97.670185	9.290957	2.036902
-97.410884	5.588268	2.046899
-97.146016	7.257317	2.056896
-96.070787	7.259829	2.066893
-96.092006	7.050845	2.076890
-95.334369	8.921447	2.086886
-94.853921	8.158681	2.096883
-94.298229	3.104411	2.106880
-93.724428	11.567527	2.116877
-93.340033	14.171360	2.126874
-92.567282	10.274174	2.136870
-91.938338	10.071018	2.146867
-91.718523	16.543197	2.156864
-91.585421	20.450365	2.166861
-90.637444	13.278711	2.176858
-90.686810	17.806851	2.186854
-89.732810	10.390333	2.196851
-89.352107	9.354926	2.206848
-88.595485	10.094779	2.216845
-88.072935	13.481588	2.226842
-87.944288	12.688417	2.236838
-87.363083	10.348131	2.246835
-86.599870	8.533694	2.256832
-86.269745	8.019399	2.266829
-85.775429	8.505747	2.276826
-84.749735	4.058910	2.286822
-84.958614	11.304684	2.296819
-84.385622	9.222279	2.306816
-83.686880	1.209031	2.316813
-83.467446	6.426814	2.326810
-82.896847	9.783919	2.336806
-82.321913	8.547016	2.346803
-81.828292	4.227901	2.356800
-81.037648	4.189477	2.366797
-81.186668	13.687691	2.376794
-79.804322	3.970748	2.386790
-79.321302	2.000644	2.396787
-79.365816	13.218444	2.406784
-78.944376	10.070058	2.416781
-78.256168	15.125691	2.426778
-78.181112	16.805477	2.436774
-76.714326	8.684551	2.446771
-76.588121	12.257010	2.456768
-76.270535	9.520874	2.466765
-76.016667	17.169314	2.476762
-75.459573	12.637511	2.486758
-74.635646	11.044812	2.496755
-73.607552	13.386224	2.506752
-73.528965	16.582840	2.516749
-73.652882	17.026677	2.526746
-72.537689	13.474979	2.536742
-72.203007	10.219810	2.546739
-72.017072	16.538909	2.556736
-71.480478	18.083020	2.566733
-70.942589	8.466717	2.576730
-69.973745	12.078203	2.586726
-69.251840	9.833082	2.596723
-69.234154	11.775282	2.606720
-68.964535	13.240848	2.616717
-68.147251	13.841317	2.626714
-67.840032	14.502703	2.636710
-67.055129	9.124245	2.646707
-66.501291	9.870532	2.656704
-66.473709	5.526239	2.666701
-65.703554	8.861581	2.676698
-64.647879	10.593620	2.686694
-64.652838	7.230112	2.696691
-64.641062	8.558682	2.706688
-63.776091	6.655442	2.716685
-63.398035	0.726181	2.726682
-62.467287	4.923346	2.736678
-62.152134	0.670210	2.746675
-62.059697	5.977585	2.756672
-61.149279	3.037686	2.766669
-60.761904	5.922988	2.776666
-60.289042	6.998744	2.786662
-59.640566	9.539025	2.796659
-59.379190	6.504419	2.806656
-58.746526	10.871838	2.816653
-57.912073	12.385116	2.826650
-57.871171	10.563483	2.836646
-56.777773	7.905358	2.846643
-56.842038	10.804408	2.856640
-56.241262	12.284609	2.866637
-55.763212	13.083954	2.876634
-55.342546	16.733820	2.886630
-54.554380	15.010510	2.896627
-53.973677	16.557213	2.906624
-53.842459	11.420565	2.916621
-52.806104	17.191430	2.926618
-52.532520	14.202428	2.936614
-52.222251	15.031230	2.946611
-52.055411	9.407493	2.956608
-51.257368	5.753437	2.966605
-50.806708	6.040720	2.976602
-49.889982	11.390002	2.986598
-49.335657	3.969589	2.996595
-49.314042	8.778045	3.006592
-48.671528	8.522080	3.016589
-47.928143	12.580713	3.026586
-48.027124	12.862252	3.036582
-46.796568	12.596511	3.046579
-46.422586	15.525096	3.056576
-46.050749	14.598785	3.066573
-46.035414	14.171829	3.076570
-45.291766	12.363628	3.086566
-44.613615	6.257462	3.096563
-43.450926	5.828126	3.106560
-43.710394	7.167519	3.116557
-43.354242	7.814902	3.126554
-42.916171	6.086260	3.136550
-41.976525	15.417064	3.146547
-41.720052	8.299912	3.156544
-40.980007	19.949156	3.166541
-40.471697	17.126114	3.176538
-40.414297	21.770576	3.186534
-39.522143	11.607750	3.196531
-39.063802	7.737657	3.206528
-38.721583	3.676685	3.216525
-38.104134	8.379110	3.226522
-37.835069	10.395964	3.236518
-36.974443	7.134414	3.246515
-36.219654	0.696293	3.256512
-36.269708	10.755544	3.266509
-36.010174	3.964199	3.276506
-35.063066	7.446047	3.286502
-34.589161	0.773170	3.296499
-33.970707	1.990842	3.306496
-33.385279	4.933812	3.316493
-33.119425	7.381991	3.326490
-32.914598	3.656160	3.336486
-31.769046	0.546372	3.346483
-31.510373	0.420244	3.356480
-31.392000	4.279034	3.366477
-30.842798	4.424165	3.376474
-30.216444	6.163289	3.386470
-29.305635	0.600381	3.396467
-28.975247	4.796585	3.406464
-28.604321	7.475391	3.416461
-28.335133	5.842904	3.426458
-27.517607	13.384022	3.436454
-27.318799	10.555624	3.446451
-26.611166	9.301099	3.456448
-25.974135	7.297362	3.466445
-25.944225	7.745607	3.476442
-24.716806	11.893127	3.486438
-24.518202	7.335134	3.496435
-24.203345	7.871779	3.506432
-23.163770	12.241969	3.516429
-23.264987	14.399206	3.526426
-22.847198	12.581875	3.536422
-21.745476	4.825435	3.546419
-21.189785	2.771087	3.556416
-21.015582	3.491330	3.566413
-21.105442	6.305691	3.576410
-20.045046	2.521831	3.586406
-19.788001	7.185694	3.596403
-18.610084	1.048742	3.606400
-18.137230	5.780160	3.616397
-18.412351	6.190667	3.626394
-17.913268	3.283543	3.636390
-16.899332	6.675728	3.646387
-16.306528	2.049635	3.656384
-16.196515	5.060762	3.666381
-15.332898	0.515782	3.676378
-14.941587	1.078462	3.686374
-14.999644	5.044092	3.696371
-14.235663	2.700516	3.706368
-13.784734	7.340335	3.716365
-12.872143	6.303956	3.726362
-12.337822	14.016163	3.736358
-12.429469	11.173086	3.746355
-11.602668	-0.341653	3.756352
-11.258632	13.507914	3.766349
-10.347105	3.471939	3.776346
-9.598797	11.492740	3.786342
-9.474317	8.527102	3.796339
-9.277539	2.290454	3.806336
-8.330944	5.775554	3.816333
-7.781924	2.987319	3.826330
-7.848162	4.223575	3.836326
-7.026449	3.138079	3.846323
-6.275811	-0.765139	3.856320
-6.001922	-1.872505	3.866317
-5.892086	6.438403	3.876314
-5.140271	4.907694	3.886310
-4.865289	6.765231	3.896307
-3.983990	17.784127	3.906304
-3.879656	23.805574	3.916301
-3.415426	30.201455	3.926298
-2.923879	40.945645	3.936294
-2.490832	50.735990	3.946291
-1.904381	65.124161	3.956288
-1.649253	73.029028	3.966285
-1.198639	94.230328	3.976282
-0.484356	114.826466	3.986278
0.000000	125.391188	3.991283
-0.352303	141.584831	3.996288
0.124073	131.287960	4.001293
-0.174591	142.158039	4.006298
0.035401	153.777340	4.011302
0.694194	164.411992	4.016307
0.635061	158.020873	4.021312
0.846314	155.339647	4.026317
0.687608	159.819098	4.031322
0.646027	167.159250	4.036326
0.628631	165.542081	4.041331
0.458485	163.771673	4.046336
0.851640	162.058539	4.051341
0.275496	169.697587	4.056346
1.165929	181.855706	4.061350
0.932688	177.541999	4.066355
0.603877	184.446266	4.071360
1.092326	176.140670	4.076365
0.805124	187.002652	4.081370
0.932462	184.008699	4.086374
0.772513	192.686711	4.091379
0.945965	198.136034	4.096384
1.373249	184.929803	4.101389
0.882743	188.575387	4.106394
0.864357	169.231629	4.111398
1.168064	162.853261	4.116403
0.832277	169.783925	4.121408
0.648191	178.541643	4.126413
0.928588	188.580692	4.131418
0.957971	191.293757	4.136422
1.089340	198.230331	4.141427
0.998865	197.975551	4.146432
1.022218	197.326444	4.151437
1.304983	203.913428	4.156442
1.374972	195.455086	4.161446
1.342492	186.522416	4.166451
1.109112	183.556507	4.171456
0.884640	169.844959	4.176461
1.026015	185.901178	4.181466
1.244570	192.178675	4.186470
1.193539	188.004098	4.191475
1.376342	188.674622	4.196480
1.579421	183.922386	4.201485
1.283499	174.524791	4.206490
0.925384	171.708144	4.211494
1.237382	168.024027	4.216499
0.879568	172.743489	4.221504
1.178831	180.821190	4.226509
1.157013	189.547161	4.231514
1.209908	189.573641	4.236518
1.415830	184.703899	4.241523
1.414408	194.192315	4.246528
1.580820	190.591117	4.251533
1.288418	188.719637	4.256538
1.360440	195.257379	4.261542
1.443641	189.293208	4.266547
1.457283	184.289075	4.271552
1.333292	178.025172	4.276557
1.343260	179.940836	4.281562
1.235094	187.652102	4.286566
1.680696	187.076043	4.291571
1.030719	195.008248	4.296576
1.026021	190.057608	4.301581
1.424482	199.369475	4.306586
1.490507	184.489250	4.311590
1.458102	188.471186	4.316595
1.528707	198.916441	4.321600
1.232402	196.710209	4.326605
1.440402	192.181829	4.331610
1.212075	186.608160	4.336614
1.333513	188.775283	4.341619
1.390633	199.842755	4.346624
1.471618	190.598071	4.351629
1.495110	191.812419	4.356634
1.716453	188.446227	4.361638
1.635461	184.004259	4.366643
1.698893	197.655562	4.371648
1.632412	199.105473	4.376653
1.328843	197.077553	4.381658
1.356184	196.804313	4.386662
1.939099	197.915189	4.391667
1.587172	195.357000	4.396672
1.651865	204.559812	4.401677
1.300579	206.288469	4.406682
1.673795	215.541024	4.411686
1.493121	215.332014	4.416691
1.538341	228.995686	4.421696
1.832080	221.777288	4.426701
1.800578	224.167697	4.431706
2.043715	223.692964	4.436710
2.089440	218.997011	4.441715
1.900441	222.585868	4.446720
1.872715	215.496936	4.451725
1.998005	209.959603	4.456730
1.554134	197.870636	4.461734
1.733703	211.437314	4.466739
1.822433	224.186154	4.471744
1.853225	217.227259	4.476749
1.836751	216.549589	4.481754
1.663384	216.076839	4.486758
2.149596	212.036382	4.491763
1.574565	217.868746	4.496768
1.954185	214.101257	4.501773
2.074301	221.055422	4.506778
1.885899	219.164481	4.511782
2.101769	214.963898	4.516787
1.742519	221.480636	4.521792
1.974290	215.894980	4.526797
1.604720	219.489982	4.531802
1.647702	219.638241	4.536806
2.165467	215.036010	4.541811
1.836591	223.563331	4.546816
1.839111	213.388117	4.551821
1.429875	223.060670	4.556826
1.812541	240.831880	4.561830
1.911135	234.710254	4.566835
2.163730	244.880244	4.571840
2.363765	243.004370	4.576845
2.272466	244.398061	4.581850
2.376883	238.196427	4.586854
2.196319	243.549370	4.591859
2.456317	243.625661	4.596864
2.147234	236.343518	4.601869
2.348831	228.987691	4.606874
2.055135	223.702666	4.611878
2.076812	223.193028	4.616883
2.388174	237.707199	4.621888
2.421176	235.107675	4.626893
2.142763	235.243015	4.631898
2.108411	244.189278	4.636902
2.380196	239.755298	4.641907
2.442029	255.536138	4.646912
2.561945	242.969656	4.651917
2.263723	229.386677	4.656922
2.017352	232.696620	4.661926
2.471083	234.286492	4.666931
2.483834	246.487259	4.671936
2.651102	228.965175	4.676941
2.394687	230.299313	4.681946
2.062992	220.688997	4.686950
2.653969	224.101861	4.691955
2.433027	230.100215	4.696960
2.400189	220.810073	4.701965
2.314690	221.956077	4.706970
2.501272	235.847546	4.711974
2.594185	241.303174	4.716979
2.432935	238.658154	4.721984
2.751197	240.443262	4.726989
2.389805	237.747342	4.731994
2.388540	219.505015	4.736998
2.524511	231.591552	4.742003
2.382752	242.870549	4.747008
2.212395	239.803005	4.752013
1.983544	239.345276	4.757018
2.260018	248.236513	4.762022
2.451604	245.267284	4.767027
2.068011	253.132466	4.772032
2.095441	247.113738	4.777037
2.423255	257.638951	4.782042
2.424955	264.953378	4.787046
2.812303	265.009715	4.792051
2.860531	274.158194	4.797056
3.239676	273.915254	4.802061
3.265601	261.695686	4.807066
2.654029	256.637631	4.812070
2.772478	251.506325	4.817075
2.541683	253.861525	4.822080
2.794863	247.440423	4.827085
3.079822	252.432522	4.832090
2.424584	249.456769	4.837094
2.768207	249.143464	4.842099
2.574531	251.160648	4.847104
2.855461	260.782032	4.852109
2.905976	254.430647	4.857114
2.591165	256.245345	4.862118
2.907662	258.992529	4.867123
3.054081	270.960394	4.872128
3.233451	263.079679	4.877133
2.928368	250.364644	4.882138
2.481467	249.042557	4.887142
2.695821	253.229457	4.892147
2.586649	265.091830	4.897152
3.133336	269.910047	4.902157
3.112200	275.987843	4.907162
2.852035	270.466593	4.912166
3.069256	270.635009	4.917171
3.039897	276.451497	4.922176
3.048725	261.798473	4.927181
3.290824	268.758855	4.932186
2.835661	273.677097	4.937190
3.306076	266.965682	4.942195
2.762191	276.257557	4.947200
3.235502	264.822118	4.952205
3.381975	271.971494	4.957210
2.908434	254.527642	4.962214
3.218741	266.441352	4.967219
3.122619	268.911496	4.972224
2.836540	259.743273	4.977229
2.851981	266.134879	4.982234
2.557179	272.271372	4.987238
3.242548	267.256883	4.992243
3.018739	273.847333	4.997248
3.248756	268.344194	5.002253
3.237984	267.187894	5.007258
3.222244	274.682232	5.012262
3.307544	270.302774	5.017267
2.835000	275.926106	5.022272
3.029853	273.706184	5.027277
2.888322	269.321138	5.032282
3.064929	266.537754	5.037286
3.211697	264.954966	5.042291
2.971667	267.574211	5.047296
3.481523	284.366901	5.052301
3.355030	290.388443	5.057306
4.071331	295.056701	5.062310
3.478435	281.345844	5.067315
3.195670	280.969328	5.072320
3.476738	271.680597	5.077325
3.414973	268.839648	5.082330
3.330656	272.544993	5.087334
3.660571	275.017989	5.092339
3.453123	273.304036	5.097344
3.083529	264.303921	5.102349
3.644030	271.913618	5.107354
3.377862	282.253498	5.112358
3.560891	268.126841	5.117363
3.087791	272.076604	5.122368
3.119176	274.425528	5.127373
3.592364	294.299199	5.132378
3.531596	301.028632	5.137382
3.416556	298.066308	5.142387
3.235657	299.160825	5.147392
3.535125	301.480405	5.152397
3.473951	304.524057	5.157402
3.335312	305.064612	5.162406
3.359139	294.898668	5.167411
3.794851	307.900092	5.172416
3.769168	294.796391	5.177421
3.936408	297.684028	5.182426
3.667400	305.135802	5.187430
3.575592	298.120153	5.192435
3.676173	301.948397	5.197440
3.818712	301.543209	5.202445
3.551413	302.151380	5.207450
3.543807	309.441974	5.212454
3.591607	303.166929	5.217459
3.538363	305.772732	5.222464
3.258259	303.715811	5.227469
3.391033	307.418788	5.232474
3.364243	313.450025	5.237478
3.778775	310.765400	5.242483
3.823919	323.296510	5.247488
4.183431	321.626599	5.252493
3.815448	321.611454	5.257498
3.605767	328.433834	5.262502
3.883915	317.917974	5.267507
3.968730	325.646519	5.272512
3.992365	325.933855	5.277517
3.916203	319.969298	5.282522
3.696457	321.645718	5.287526
4.111629	321.751480	5.292531
3.720507	319.819523	5.297536
4.068908	321.093705	5.302541
4.045925	314.370993	5.307546
4.361665	331.915494	5.312550
4.524641	309.917195	5.317555
3.572156	308.740761	5.322560
3.766705	298.990999	5.327565
3.862351	301.124211	5.332570
3.697543	312.659968	5.337574
4.260197	321.534877	5.342579
3.786151	320.090485	5.347584
4.110286	321.058415	5.352589
4.106395	324.561341	5.357594
4.061556	319.781473	5.362598
4.272678	319.941354	5.367603
4.073274	320.130755	5.372608
4.239250	322.974301	5.377613
4.081523	326.346303	5.382618
3.505733	333.042546	5.387622
4.029868	325.778514	5.392627
4.090395	325.965155	5.397632
4.049648	317.713935	5.402637
4.140470	323.283814	5.407642
4.212865	326.078746	5.412646
4.213465	318.672116	5.417651
4.003474	329.110790	5.422656
4.169567	325.294475	5.427661
4.143849	316.117066	5.432666
4.161158	319.844464	5.437670
4.355833	314.985940	5.442675
3.979151	325.514007	5.447680
4.175317	334.807020	5.452685
4.370247	347.216598	5.457690
4.310831	348.456602	5.462694
4.624558	344.326080	5.467699
4.538208	357.880749	5.472704
4.512550	335.301356	5.477709
4.134049	335.544129	5.482714
4.218333	349.049909	5.487718
4.505304	347.663451	5.492723
4.152523	353.657192	5.497728
4.380641	350.884708	5.502733
4.666868	352.057900	5.507738
4.551411	348.428067	5.512742
4.734189	340.160797	5.517747
4.669081	349.143571	5.522752
4.762803	341.203473	5.527757
4.596245	327.321374	5.532762
4.381378	327.377153	5.537766
4.853050	323.512960	5.542771
4.350909	333.703176	5.547776
4.156558	327.212958	5.552781
4.601973	333.663772	5.557786
4.341253	346.815474	5.562790
4.604401	339.741029	5.567795
4.381462	350.156434	5.572800
4.418201	349.938668	5.577805
4.591638	363.566535	5.582810
4.281162	348.779966	5.587814
4.426822	339.563038	5.592819
4.362051	356.869783	5.597824
4.279834	343.952079	5.602829
4.637008	349.100574	5.607834
4.526666	359.017440	5.612838
4.980451	363.938826	5.617843
4.501433	360.011605	5.622848
4.988850	362.785810	5.627853
4.731704	361.076471	5.632858
4.729626	348.529029	5.637862
5.077265	349.189551	5.642867
4.928281	359.492132	5.647872
4.804616	351.500667	5.652877
4.746657	344.685345	5.657882
4.880122	351.292613	5.662886
5.042159	349.378388	5.667891
4.626866	352.303522	5.672896
4.581560	358.097225	5.677901
5.023792	359.135241	5.682906
4.811069	367.324885	5.687910
5.004151	370.793793	5.692915
4.841136	372.315793	5.697920
5.173338	379.860064	5.702925
5.408711	366.433827	5.707930
5.072473	366.328285	5.712934
4.904686	354.474371	5.717939
4.918747	351.419043	5.722944
4.816351	346.085025	5.727949
4.928851	352.423490	5.732954
4.888968	351.654568	5.737958
4.805161	365.477769	5.742963
4.714815	375.673093	5.747968
4.712243	371.180825	5.752973
4.782827	379.313430	5.757978
5.062824	377.099138	5.762982
4.873392	378.976463	5.767987
4.967834	383.732689	5.772992
4.954764	388.243163	5.777997
4.940332	374.913008	5.783002
4.719244	380.557087	5.788006
5.146646	392.193100	5.793011
5.076534	406.257802	5.798016
5.060212	408.702807	5.803021
5.269289	405.028440	5.808026
5.212346	408.179017	5.813030
5.699872	404.527463	5.818035
5.385720	406.085802	5.823040
5.219691	390.074310	5.828045
5.068571	392.224050	5.833050
5.261387	395.582271	5.838054
5.519350	409.377267	5.843059
5.743348	402.637970	5.848064
5.209236	383.801904	5.853069
5.298940	383.468268	5.858074
5.084310	378.335328	5.863078
5.324048	389.165492	5.868083
5.384028	399.444846	5.873088
5.317562	402.789908	5.878093
5.742451	404.460247	5.883098
5.352498	393.973091	5.888102
5.416831	386.546955	5.893107
5.146645	388.639418	5.898112
5.660788	404.368503	5.903117
5.855264	409.333694	5.908122
5.140054	392.623616	5.913126
5.529344	380.669745	5.918131
5.269862	400.550760	5.923136
5.104286	405.053496	5.928141
5.234258	408.364617	5.933146
5.231283	412.819730	5.938150
5.252620	405.707215	5.943155
5.157556	399.631696	5.948160
5.079661	403.772671	5.953165
5.615299	405.213681	5.958170
5.689001	412.251125	5.963174
5.754428	402.211483	5.968179
5.452828	405.226382	5.973184
5.908042	408.366317	5.978189
5.727357	404.101270	5.983194
5.764413	412.245471	5.988198
5.285549	399.652472	5.993203
5.419355	412.432350	5.998208
5.718521	416.004872	6.003213
5.608897	417.202126	6.008218
5.571131	424.408905	6.013222
5.663999	432.955669	6.018227
5.657747	443.321357	6.023232
5.638646	430.548729	6.028237
6.029383	430.481146	6.033242
5.529968	421.931575	6.038246
5.800016	422.480867	6.043251
5.386374	422.956944	6.048256
5.658806	430.304952	6.053261
6.051805	425.285607	6.058266
5.867132	420.856661	6.063270
6.120466	411.565876	6.068275
5.715783	415.327774	6.073280
5.687775	409.444230	6.078285
5.900902	407.740299	6.083290
5.558403	413.941262	6.088294
5.529623	396.750296	6.093299
5.385305	405.859406	6.098304
5.337064	403.598462	6.103309
5.631339	409.244060	6.108314
5.292158	415.235691	6.113318
5.564667	423.928316	6.118323
5.942330	432.231136	6.123328
5.795123	425.268410	6.128333
5.669465	414.622770	6.133338
5.280217	418.790385	6.138342
5.052615	425.463745	6.143347
5.694864	425.097320	6.148352
5.516904	432.519062	6.153357
5.866886	430.423516	6.158362
5.971293	440.955368	6.163366
6.037485	427.242372	6.168371
5.895756	425.388389	6.173376
5.910099	425.196278	6.178381
5.528914	405.311144	6.183386
5.441464	406.283454	6.188390
5.571623	410.078613	6.193395
5.747300	429.508655	6.198400
5.743766	422.659465	6.203405
5.481929	421.118538	6.208410
5.735382	433.009629	6.213414
5.661290	434.470243	6.218419
5.822808	432.524452	6.223424
5.534020	417.841999	6.228429
5.830259	428.982882	6.233434
5.621201	426.414929	6.238438
5.460437	430.287313	6.243443
5.663717	422.358488	6.248448
5.493084	430.975012	6.253453
5.945810	432.666303	6.258458
5.689069	436.354404	6.263462
6.000295	424.377933	6.268467
5.894601	425.425871	6.273472
5.555996	414.199811	6.278477
5.721779	404.796194	6.283482
5.686780	404.111928	6.288486
5.855980	401.152510	6.293491
5.537085	403.844244	6.298496
5.853675	404.699463	6.303501
6.002632	412.025680	6.308506
5.873060	419.275316	6.313510
5.755794	411.978866	6.318515
5.736209	396.960013	6.323520
5.544838	409.996489	6.328525
5.733102	413.035879	6.333530
5.391893	403.591473	6.338534
5.718396	407.754511	6.343539
5.618307	407.659425	6.348544
5.621669	412.293885	6.353549
5.597005	407.862018	6.358554
5.734967	415.114028	6.363558
5.353035	415.572480	6.368563
5.453888	412.433938	6.373568
5.158849	403.184784	6.378573
5.721593	410.819501	6.383578
5.871235	423.843685	6.388582
5.668835	412.884194	6.393587
5.753554	420.166694	6.398592
5.655674	411.582689	6.403597
5.504244	412.210675	6.408602
5.825543	413.932048	6.413606
5.816746	412.038255	6.418611
5.836394	414.085309	6.423616
5.690004	412.130815	6.428621
5.737995	417.897264	6.433626
5.671768	414.981059	6.438630
5.609252	399.073566	6.443635
5.420034	408.234006	6.448640
5.331106	414.733770	6.453645
5.818518	414.524487	6.458650
5.785045	417.427773	6.463654
5.856512	410.943332	6.468659
5.635694	425.468272	6.473664
5.638688	416.700775	6.478669
5.662812	414.080469	6.483674
5.642775	414.959958	6.488678
5.463323	407.372689	6.493683
5.480985	418.535067	6.498688
5.786102	429.484728	6.503693
5.873405	413.819511	6.508698
5.664533	416.019432	6.513702
5.811931	415.537548	6.518707
5.528124	420.666269	6.523712
5.331380	411.249845	6.528717
5.579761	428.786012	6.533722
5.644641	438.688124	6.538726
5.925170	431.984253	6.543731
5.954627	433.479264	6.548736
5.904230	419.464994	6.553741
5.694900	409.300715	6.558746
5.657944	416.387137	6.563750
5.848894	415.338430	6.568755
5.333343	412.502118	6.573760
5.442277	406.052938	6.578765
5.344042	404.391464	6.583770
5.432977	418.019957	6.588774
5.913146	430.369082	6.593779
5.937010	437.695928	6.598784
5.760544	431.202869	6.603789
5.731923	411.338419	6.608794
5.824567	414.335842	6.613798
5.871658	413.334986	6.618803
5.630631	406.159172	6.623808
5.626853	417.147734	6.628813
5.769322	404.675684	6.633818
5.602559	408.337026	6.638822
5.472554	403.814095	6.643827
5.689952	417.343363	6.648832
5.413508	408.603835	6.653837
5.531439	410.078654	6.658842
5.644354	425.443505	6.663846
5.964626	423.861993	6.668851
5.868294	425.677277	6.673856
5.667706	411.094909	6.678861
5.866038	405.349913	6.683866
5.654585	407.999503	6.688870
5.469165	412.347158	6.693875
5.326045	419.061064	6.698880
5.469457	416.485344	6.703885
6.017296	417.516308	6.708890
5.616786	427.712801	6.713894
5.603579	418.359368	6.718899
5.588253	417.099365	6.723904
5.771997	421.895394	6.728909
5.848977	408.883094	6.733914
5.559483	405.679161	6.738918
6.001069	412.086310	6.743923
5.872073	414.969760	6.748928
5.612514	413.156388	6.753933
5.910602	407.534970	6.758938
5.701869	413.525145	6.763942
5.698997	413.275618	6.768947
5.759613	418.641447	6.773952
5.577567	414.098192	6.778957
5.932173	413.678757	6.783962
5.618311	418.726763	6.788966
6.034839	413.131080	6.793971
5.920724	416.239995	6.798976
5.782626	413.765333	6.803981
5.716716	412.143087	6.808986
5.579211	421.548539	6.813990
5.564887	407.576084	6.818995
5.507191	415.228918	6.824000
5.788647	409.670219	6.829005
5.831919	415.450062	6.834010
5.382412	404.333136	6.839014
5.627075	416.453389	6.844019
5.857511	416.758945	6.849024
5.635354	408.042549	6.854029
5.761369	408.772601	6.859034
5.809251	412.830594	6.864038
5.992757	406.322273	6.869043
5.922086	412.721097	6.874048
5.559066	414.340878	6.879053
5.886253	411.995799	6.884058
5.578505	411.670652	6.889062
5.683204	417.333301	6.894067
5.882852	412.170243	6.899072
5.483043	413.039631	6.904077
5.663392	407.490447	6.909082
5.657723	417.761114	6.914086
5.557078	411.066353	6.919091
5.530903	417.154479	6.924096
5.488169	413.519565	6.929101
6.005270	417.336358	6.934106
5.436058	414.290148	6.939110
6.031076	407.287068	6.944115
5.973609	409.555017	6.949120
5.678270	396.835186	6.954125
5.379772	391.076289	6.959130
5.372385	405.640540	6.964134
5.497544	406.582702	6.969139
5.615409	407.121037	6.974144
5.524661	404.623137	6.979149
5.468156	409.466298	6.984154
5.446069	413.373898	6.989158
5.580445	417.089302	6.994163
5.332584	413.515003	6.999168
5.437364	410.018333	7.004173
5.932666	408.380923	7.009178
5.659337	419.329460	7.014182
5.626058	408.349801	7.019187
5.736914	409.838384	7.024192
5.848805	413.541491	7.029197
6.225776	402.238122	7.034202
5.783747	403.794349	7.039206
6.117079	399.442438	7.044211
5.527906	404.188718	7.049216
5.656007	413.169726	7.054221
5.897141	408.572823	7.059226
5.555713	416.273278	7.064230
5.408094	407.779327	7.069235
5.471655	408.111029	7.074240
5.787426	411.247503	7.079245
5.899161	407.123304	7.084250
5.600192	413.659141	7.089254
5.922600	405.237083	7.094259
5.596681	408.480426	7.099264
5.687940	405.251637	7.104269
5.945167	411.308011	7.109274
6.106872	414.772353	7.114278
5.610363	395.484281	7.119283
5.540325	389.265635	7.124288
5.750953	387.631701	7.129293
5.809160	378.320885	7.134298
5.450389	382.366655	7.139302
5.653726	378.392630	7.144307
5.666705	390.353009	7.149312
5.436946	387.418137	7.154317
5.918930	391.423928	7.159322
5.697732	400.282484	7.164326
5.565797	389.337277	7.169331
5.456491	399.108467	7.174336
5.778877	420.932682	7.179341
5.883689	408.805060	7.184346
5.756241	412.020470	7.189350
5.727636	398.762122	7.194355
5.557032	392.970531	7.199360
5.325068	391.659049	7.204365
5.606210	398.081841	7.209370
5.700789	402.135679	7.214374
5.766747	403.884403	7.219379
5.611443	399.194591	7.224384
5.734000	413.051935	7.229389
5.568707	416.130903	7.234394
5.752127	420.718170	7.239398
5.851643	418.111361	7.244403
5.785210	402.112728	7.249408
5.423728	400.226738	7.254413
5.493902	395.042842	7.259418
5.371747	411.235471	7.264422
5.886283	410.756175	7.269427
5.594931	413.623934	7.274432
5.678998	409.143392	7.279437
5.916686	409.938206	7.284442
5.903969	410.958920	7.289446
5.659681	395.310871	7.294451
5.333647	396.001016	7.299456
5.557693	400.303495	7.304461
5.871020	408.328475	7.309466
5.826070	421.977948	7.314470
5.801040	400.926508	7.319475
5.502593	400.849847	7.324480
5.161682	400.662777	7.329485
5.788384	395.407502	7.334490
5.571280	410.001451	7.339494
5.900184	406.150118	7.344499
5.658601	405.014154	7.349504
5.400558	423.730678	7.354509
5.667669	416.231629	7.359514
5.374070	415.455000	7.364518
5.920451	405.906325	7.369523
5.587629	408.391428	7.374528
5.350971	420.966760	7.379533
5.888749	417.272527	7.384538
5.398802	412.277630	7.389542
5.710269	409.672416	7.394547
5.722385	416.074089	7.399552
5.691566	410.456748	7.404557
5.755904	411.376801	7.409562
6.060532	405.741705	7.414566
5.982159	417.479128	7.419571
5.735280	419.007943	7.424576
5.701586	408.645297	7.429581
5.743902	403.699887	7.434586
5.577771	408.667794	7.439590
5.431322	411.971605	7.444595
5.483862	424.492135	7.449600
5.221436	416.417976	7.454605
5.603011	406.186424	7.459610
5.192768	419.570419	7.464614
5.955380	406.602559	7.469619
5.763761	407.284299	7.474624
5.706765	407.324834	7.479629
5.637309	409.366866	7.484634
5.514563	418.387180	7.489638
5.663808	413.355409	7.494643
5.514119	410.930020	7.499648
5.606647	408.374929	7.504653
5.652492	409.652230	7.509658
5.690357	411.680610	7.514662
5.711895	410.164889	7.519667
5.487729	409.108455	7.524672
5.245075	413.113892	7.529677
5.574368	405.484878	7.534682
5.424125	415.949044	7.539686
5.859626	409.891633	7.544691
5.718065	404.918084	7.549696
5.692465	401.501957	7.554701
5.729180	405.830624	7.559706
5.693101	418.444131	7.564710
5.848101	400.189791	7.569715
5.958263	404.994181	7.574720
5.879629	402.472236	7.579725
5.672244	412.837783	7.584730
5.474175	413.779969	7.589734
5.703011	409.574145	7.594739
5.524288	410.165277	7.599744
5.447248	412.597650	7.604749
5.679557	410.226306	7.609754
5.611657	411.942220	7.614758
5.647565	412.101080	7.619763
5.808297	404.444691	7.624768
5.407158	415.685342	7.629773
6.026495	408.880936	7.634778
5.378449	416.778133	7.639782
5.708969	405.624413	7.644787
5.740088	413.434178	7.649792
5.817486	418.006417	7.654797
5.747174	402.055849	7.659802
5.563158	411.092087	7.664806
5.752727	420.088777	7.669811
5.721836	414.401841	7.674816
5.625087	413.195726	7.679821
5.587449	408.364085	7.684826
5.782605	410.472227	7.689830
5.877220	405.458509	7.694835
5.629732	413.988988	7.699840
5.475414	405.828291	7.704845
5.650217	411.369220	7.709850
5.485900	415.280123	7.714854
5.549919	409.341030	7.719859
5.753488	408.116335	7.724864
5.860361	412.215707	7.729869
6.137907	403.769041	7.734874
5.738139	402.199105	7.739878
5.741484	409.007121	7.744883
6.154322	411.005224	7.749888
5.921240	413.430407	7.754893
5.870111	405.164955	7.759898
5.437697	416.837624	7.764902
6.086862	403.928670	7.769907
5.484247	417.779415	7.774912
5.590543	413.608609	7.779917
5.755648	418.841003	7.784922
5.244649	420.822501	7.789926
5.996306	416.484137	7.794931
5.923166	412.613536	7.799936
5.454517	412.361057	7.804941
5.372630	410.348999	7.809946
5.520611	411.271767	7.814950
5.330847	410.599095	7.819955
5.886526	415.871535	7.824960
5.614787	418.710910	7.829965
5.832694	415.158548	7.834970
5.632950	418.378959	7.839974
5.728724	410.618848	7.844979
5.508410	407.856503	7.849984
5.582215	414.261165	7.854989
5.869013	410.656880	7.859994
5.397531	418.640312	7.864998
5.743655	412.479842	7.870003
5.623274	407.987040	7.875008
5.664693	419.401967	7.880013
5.940248	408.937081	7.885018
5.761914	412.821706	7.890022
5.800781	413.916598	7.895027
5.793667	398.161781	7.900032
5.761699	401.697595	7.905037
5.732843	403.720610	7.910042
5.794081	405.270752	7.915046
5.720057	406.595308	7.920051
5.676543	404.093172	7.925056
5.550777	406.514195	7.930061
5.775164	398.781395	7.935066
5.537800	405.057634	7.940070
5.967283	412.108938	7.945075
6.058592	407.709522	7.950080
5.705920	395.485905	7.955085
5.439059	397.138076	7.960090
5.438335	380.812783	7.965094
5.663319	389.879841	7.970099
5.670420	398.601383	7.975104
5.848441	398.563965	7.980109
6.106866	396.014521	7.985114
5.498871	392.566258	7.990118
5.249135	385.376240	7.995136
5.769696	398.208019	8.000154
5.233305	404.007117	8.005171
5.659033	401.611425	8.010189
5.707675	411.796889	8.015206
5.917879	408.444056	8.020224
5.561625	405.640719	8.025242
5.474260	404.322642	8.030259
5.774606	403.571814	8.035277
5.620439	407.878308	8.040294
5.830617	404.790564	8.045312
5.506834	407.552063	8.050330
5.806585	410.768124	8.055347
5.817148	403.318832	8.060365
5.330392	409.195360	8.065382
5.107291	404.376717	8.070400
5.556841	406.682537	8.075418
5.355310	405.940918	8.080435
5.624511	401.247110	8.085453
5.318873	410.023808	8.090470
5.956873	415.092955	8.095488
5.887999	428.922816	8.100506
5.682471	428.270184	8.105523
5.934793	425.074848	8.110541
5.713466	416.920278	8.115558
5.714062	418.722094	8.120576
5.896342	423.143132	8.125594
5.499300	432.906139	8.130611
5.842208	428.434302	8.135629
5.664365	433.303082	8.140646
5.926496	428.648244	8.145664
5.939097	437.633866	8.150682
6.101004	435.371024	8.155699
6.103791	424.243315	8.160717
5.815784	421.684900	8.165734
5.905961	413.964356	8.170752
5.967967	406.181959	8.175770
5.721187	400.436077	8.180787
5.883197	406.299315	8.185805
5.468675	407.437190	8.190822
5.647935	420.890500	8.195840
6.089264	429.597507	8.200858
5.935741	442.017390	8.205875
6.144221	432.924476	8.210893
6.014182	425.295236	8.215910
5.922454	415.397312	8.220928
5.751316	416.468652	8.225946
5.724576	425.084895	8.230963
6.013547	431.916004	8.235981
5.648679	439.502804	8.240998
5.835011	439.240049	8.246016
6.198625	426.045578	8.251034
5.982929	436.755306	8.256051
6.017102	436.992912	8.261069
5.711682	442.553864	8.266086
6.116838	440.069873	8.271104
6.294200	432.323039	8.276122
6.093302	434.159582	8.281139
6.205303	420.395476	8.286157
6.024061	419.669612	8.291174
6.042278	418.704215	8.296192
6.218446	414.413140	8.301210
5.351335	419.320486	8.306227
5.831861	419.071595	8.311245
6.315652	429.173110	8.316262
6.127737	428.120091	8.321280
6.141172	411.079970	8.326298
5.544734	411.981264	8.331315
5.872613	416.202764	8.336333
5.787978	430.148703	8.341350
6.179107	426.234194	8.346368
6.291202	430.016142	8.351386
6.338748	424.019011	8.356403
6.087492	410.343387	8.361421
6.213178	407.025886	8.366438
5.884691	406.588178	8.371456
6.178321	392.565264	8.376474
6.148742	412.198714	8.381491
6.551424	400.563400	8.386509
5.945697	408.077474	8.391526
5.686589	408.824930	8.396544
6.118746	410.451830	8.401562
5.756111	408.873930	8.406579
5.924627	411.981167	8.411597
5.850949	424.095041	8.416614
6.261338	427.170696	8.421632
6.595017	435.389650	8.426650
6.396873	422.958534	8.431667
6.165203	406.433342	8.436685
5.869116	409.562882	8.441702
5.688280	418.067568	8.446720
6.514291	424.218089	8.451738
6.263704	425.443887	8.456755
6.037860	414.143726	8.461773
5.928150	423.972160	8.466790
6.091794	434.685566	8.471808
6.389392	433.237742	8.476826
6.387792	428.321273	8.481843
5.968872	408.341450	8.486861
6.247043	423.312966	8.491878
6.202311	432.657858	8.496896
6.181958	427.002721	8.501914
6.352033	429.557458	8.506931
6.191823	422.232745	8.511949
6.229865	422.851593	8.516966
6.199040	416.989819	8.521984
6.240535	414.976217	8.527002
6.257237	424.945789	8.532019
6.155662	427.691410	8.537037
6.304744	437.403564	8.542054
5.978241	433.424771	8.547072
6.111660	432.375053	8.552090
6.146098	431.230391	8.557107
6.221883	441.184403	8.562125
6.484641	434.850596	8.567143
6.429271	427.228590	8.572160
6.671985	424.662757	8.577178
6.586458	417.102285	8.582195
6.220014	406.259654	8.587213
6.233995	406.288988	8.592231
6.025992	412.936028	8.597248
6.105990	416.814519	8.602266
6.222270	422.908987	8.607283
6.428079	426.849818	8.612301
6.604991	420.217045	8.617319
5.921339	425.048311	8.622336
6.420913	422.600022	8.627354
6.415520	428.473717	8.632371
6.525530	428.734154	8.637389
6.187722	430.699445	8.642407
6.360637	436.119176	8.647424
6.273127	425.475824	8.652442
6.683969	428.286324	8.657459
6.585830	435.055012	8.662477
6.576652	428.202087	8.667495
6.106548	421.493967	8.672512
6.368684	421.746348	8.677530
6.169292	425.485582	8.682547
6.307767	429.064583	8.687565
6.384253	430.781927	8.692583
6.206112	439.876330	8.697600
6.374388	428.722689	8.702618
6.585721	441.060159	8.707635
6.375775	438.129752	8.712653
6.396992	435.652271	8.717671
6.369223	427.309581	8.722688
6.661741	432.817868	8.727706
6.522649	432.183228	8.732723
6.543499	423.387958	8.737741
6.630839	425.829427	8.742759
6.506067	429.673734	8.747776
6.363411	428.263334	8.752794
6.305437	435.461225	8.757811
6.494572	426.175689	8.762829
6.406304	430.080547	8.767847
6.276712	427.752927	8.772864
6.381595	431.217273	8.777882
6.429740	428.937543	8.782899
6.188792	430.111338	8.787917
6.423261	427.155482	8.792935
6.353557	438.587098	8.797952
6.482020	426.511900	8.802970
6.636049	429.110176	8.807987
6.628593	429.707751	8.813005
6.688305	428.224618	8.818023
6.490745	430.862204	8.823040
6.568854	416.939310	8.828058
6.667431	430.452606	8.833075
6.308480	431.543906	8.838093
6.710720	431.263100	8.843111
6.567180	437.814843	8.848128
6.713028	434.768731	8.853146
6.590446	436.583537	8.858163
6.387727	429.454827	8.863181
6.649000	437.416887	8.868199
6.336410	438.084361	8.873216
6.543642	435.763926	8.878234
6.533903	441.783471	8.883251
6.440496	454.042466	8.888269
6.902826	456.220060	8.893287
6.474033	460.897796	8.898304
6.913693	453.078297	8.903322
6.753354	454.129012	8.908339
6.801515	460.363552	8.913357
7.005718	436.966190	8.918375
6.655966	438.033959	8.923392
6.468615	436.065679	8.928410
6.733711	441.079652	8.933427
6.750632	432.237658	8.938445
6.498657	431.109470	8.943463
7.135107	448.902932	8.948480
6.944082	432.699547	8.953498
6.738034	437.358156	8.958515
6.591915	433.685611	8.963533
6.817634	424.088234	8.968551
6.320191	421.209188	8.973568
6.383601	428.138752	8.978586
6.730243	442.481025	8.983603
6.835469	447.823003	8.988621
6.673472	448.558401	8.993639
6.725413	461.119672	8.998656
6.492485	452.663949	9.003674
6.794521	454.734115	9.008691
6.643596	450.418542	9.013709
6.808810	448.593833	9.018727
6.904112	455.407958	9.023744
6.882170	450.794468	9.028762
6.933385	448.785651	9.033779
6.480465	451.292838	9.038797
6.558432	447.484195	9.043815
6.689851	452.998795	9.048832
6.880108	452.577636	9.053850
6.717760	448.248074	9.058867
6.565048	449.641573	9.063885
6.855527	451.110797	9.068903
6.503810	453.971354	9.073920
6.736029	452.953490	9.078938
6.875146	452.685509	9.083955
6.945025	462.488982	9.088973
6.886067	452.428114	9.093991
7.340836	462.250175	9.099008
6.861964	458.973741	9.104026
6.698625	452.353243	9.109043
7.220724	452.075747	9.114061
6.979604	449.106043	9.119079
7.177984	454.875236	9.124096
7.136195	454.701871	9.129114
6.852669	448.945952	9.134131
6.690367	447.087354	9.139149
6.684763	443.768327	9.144167
6.700355	454.249324	9.149184
7.000958	464.098697	9.154202
7.177117	459.400517	9.159219
6.630797	460.691588	9.164237
6.875622	465.869690	9.169255
6.845062	475.714153	9.174272
7.269957	479.693252	9.179290
7.380922	484.239086	9.184307
7.126225	468.683112	9.189325
6.959963	462.779429	9.194343
7.006717	461.358283	9.199360
6.814703	465.724369	9.204378
6.889132	464.930042	9.209395
7.187944	478.150070	9.214413
7.337429	485.135597	9.219431
6.922369	477.087093	9.224448
7.336477	470.805297	9.229466
7.447905	455.198281	9.234483
7.206779	452.881821	9.239501
6.988658	446.430853	9.244519
7.033166	460.186169	9.249536
7.010645	447.755921	9.254554
7.070389	453.045068	9.259571
7.154781	460.100743	9.264589
6.939622	446.018652	9.269607
6.982619	459.161985	9.274624
7.043414	455.510664	9.279642
7.242078	468.190960	9.284659
7.058414	475.298109	9.289677
7.227123	475.028647	9.294695
7.163691	474.770311	9.299712
7.447476	474.031543	9.304730
7.300729	462.640064	9.309747
7.074723	461.703464	9.314765
7.072199	458.207229	9.319783
6.740470	468.095719	9.324800
7.034188	470.564819	9.329818
7.428594	476.126581	9.334835
7.410282	488.181331	9.339853
7.233474	486.918288	9.344871
7.485097	481.491916	9.349888
7.590124	475.694044	9.354906
7.450132	464.039576	9.359923
7.123401	455.598549	9.364941
7.392786	451.397000	9.369959
7.087195	455.159192	9.374976
6.825522	460.391405	9.379994
7.079679	449.470445	9.385011
7.172727	468.270554	9.390029
7.154394	484.427813	9.395047
7.445590	477.199605	9.400064
7.423676	474.239731	9.405082
7.542866	472.163457	9.410099
7.304011	475.347157	9.415117
7.283102	465.889385	9.420135
6.992232	466.916372	9.425152
7.098473	478.345691	9.430170
7.462554	485.161896	9.435187
7.075964	489.397529	9.440205
7.461779	486.288563	9.445223
7.500927	478.714842	9.450240
7.448839	485.252273	9.455258
7.658026	470.690268	9.460275
7.437000	490.558925	9.465293
7.587246	479.786771	9.470311
7.256658	466.025704	9.475328
7.449839	475.570025	9.480346
7.369189	478.126184	9.485363
7.449572	482.304429	9.490381
7.171241	476.411988	9.495399
7.392027	481.597017	9.500416
7.107128	480.294105	9.505434
7.309106	478.867572	9.510451
7.295170	485.802965	9.515469
7.317821	480.671244	9.520487
7.379557	486.676450	9.525504
7.154185	487.036774	9.530522
7.800179	473.993682	9.535539
7.293724	491.909457	9.540557
7.087696	485.204118	9.545575
7.324394	484.841952	9.550592
7.595881	492.461612	9.555610
7.463357	482.323893	9.560627
7.366872	487.492362	9.565645
7.607547	487.937453	9.570663
7.327062	480.584224	9.575680
7.244806	488.489679	9.580698
7.267258	476.491018	9.585715
7.383659	502.214434	9.590733
7.449024	512.498319	9.595751
7.549106	505.909111	9.600768
7.552138	511.598477	9.605786
7.667160	508.244760	9.610803
7.605700	511.946622	9.615821
7.596056	517.776831	9.620839
7.685002	510.384641	9.625856
7.918989	519.720622	9.630874
8.173736	519.371408	9.635891
7.636678	499.141751	9.640909
7.596225	495.228577	9.645927
7.479357	481.765369	9.650944
7.007268	489.921252	9.655962
7.853401	504.980570	9.660979
7.945292	508.150323	9.665997
7.494142	501.985152	9.671015
7.802172	500.188553	9.676032
7.516342	503.739377	9.681050
7.743865	501.646126	9.686067
7.872538	504.750155	9.691085
7.613612	499.785622	9.696103
7.541553	503.962510	9.701120
7.647286	505.940364	9.706138
7.914372	496.510035	9.711155
7.809914	514.419650	9.716173
7.686096	508.020155	9.721191
7.540156	493.946115	9.726208
7.499005	505.531089	9.731226
7.769005	500.953893	9.736243
8.275344	516.394662	9.741261
7.924505	509.588927	9.746279
7.672793	489.769006	9.751296
7.582744	480.571365	9.756314
7.930501	494.825144	9.761331
8.317635	499.122586	9.766349
7.655661	491.138009	9.771367
7.737955	482.948460	9.776384
7.442958	484.108637	9.781402
7.923517	496.410273	9.786419
8.097475	500.816855	9.791437
7.675757	488.559578	9.796455
7.965869	486.491235	9.801472
7.670019	491.921315	9.806490
7.676690	490.332880	9.811507
7.805474	503.895146	9.816525
7.804678	507.839964	9.821543
8.036932	510.173533	9.826560
7.446727	508.852184	9.831578
7.915567	508.911235	9.836595
8.058911	510.447698	9.841613
7.803909	509.174814	9.846631
7.568503	501.397950	9.851648
7.661728	515.786299	9.856666
7.853752	503.076246	9.861683
7.568041	509.378894	9.866701
7.639011	513.795304	9.871719
7.886326	507.798403	9.876736
7.776591	511.905457	9.881754
7.860321	506.612681	9.886771
7.792023	513.307296	9.891789
7.982372	525.739630	9.896807
8.054473	523.834828	9.901824
8.044241	535.326614	9.906842
7.928441	523.147613	9.911859
8.135817	529.515020	9.916877
7.982016	522.829885	9.921895
8.015796	532.187775	9.926912
8.066608	533.760829	9.931930
8.278305	530.631800	9.936947
8.208154	524.154463	9.941965
7.860202	520.548238	9.946983
8.007613	510.104711	9.952000
7.941040	526.383174	9.957018
8.082476	529.172785	9.962035
8.399910	523.524652	9.967053
8.203477	522.409847	9.972071
8.219988	513.318569	9.977088
8.111287	506.597972	9.982106
8.066011	509.552533	9.987123
8.330571	511.584397	9.992141
8.035773	515.976067	9.997159
8.051710	502.479411	10.002176
7.969193	498.512867	10.007194
7.817711	511.333263	10.012211
8.082753	525.006739	10.017229
8.114473	531.862413	10.022247
8.359005	523.101475	10.027264
8.115493	538.157982	10.032282
8.604876	528.115297	10.037299
8.273542	520.542801	10.042317
7.675198	514.561634	10.047335
8.457304	511.112863	10.052352
8.105499	537.859581	10.057370
8.665011	528.143577	10.062387
8.196089	519.917302	10.067405
7.800539	524.763414	10.072423
8.315913	524.483816	10.077440
8.188323	533.958508	10.082458
8.492650	532.093059	10.087475
8.347245	544.082554	10.092493
8.254370	540.108156	10.097511
8.296675	525.793159	10.102528
8.454926	533.837675	10.107546
8.108355	522.341768	10.112563
8.192902	521.823562	10.117581
7.976183	528.377336	10.122599
8.286213	526.428944	10.127616
8.179439	529.740280	10.132634
8.151693	530.110666	10.137651
8.009589	532.080017	10.142669
8.391858	532.862684	10.147687
8.724783	530.206964	10.152704
8.101404	536.474166	10.157722
8.764438	531.450375	10.162739
8.674036	534.064874	10.167757
8.363506	525.693859	10.172775
8.199803	525.779435	10.177792
8.090716	529.444582	10.182810
8.489722	531.578458	10.187827
8.208654	534.790873	10.192845
8.198225	527.019772	10.197863
8.512084	532.370112	10.202880
8.049429	525.496685	10.207898
8.397646	529.645598	10.212915
8.576303	531.277516	10.217933
8.333208	533.322651	10.222951
8.670551	530.590500	10.227968
8.387448	534.238732	10.232986
8.479340	532.706367	10.238003
8.526580	534.374655	10.243021
8.170310	545.908043	10.248039
8.567576	531.225001	10.253056
8.554024	538.460155	10.258074
8.684772	545.107816	10.263091
8.659695	539.712158	10.268109
8.206863	533.916467	10.273127
8.293123	543.647990	10.278144
8.811716	552.103112	10.283162
8.853141	550.016923	10.288179
8.371105	536.396295	10.293197
8.363638	556.673375	10.298215
8.942647	550.056447	10.303232
8.502112	554.063864	10.308250
8.500989	557.380742	10.313267
8.582850	556.253889	10.318285
8.612458	560.496911	10.323303
8.706239	557.323237	10.328320
8.921953	554.278781	10.333338
9.059203	554.118388	10.338355
8.989930	539.899756	10.343373
8.874002	541.435821	10.348391
8.820908	534.813797	10.353408
8.531661	525.325454	10.358426
8.653203	535.426983	10.363443
8.962467	531.380112	10.368461
8.931826	535.616789	10.373479
8.844892	524.032864	10.378496
8.665008	534.901139	10.383514
8.444188	538.331332	10.388531
8.969539	531.347279	10.393549
8.230163	538.216477	10.398567
8.403654	529.883230	10.403584
8.273364	541.554777	10.408602
8.507113	556.495495	10.413619
8.888559	557.858957	10.418637
8.803174	564.755083	10.423655
8.646446	562.213948	10.428672
9.096640	565.598969	10.433690
8.797648	557.437569	10.438707
9.219075	557.466179	10.443725
8.869152	560.790372	10.448743
8.920286	546.764307	10.453760
8.674444	548.961353	10.458778
8.830991	564.261311	10.463795
8.992893	558.807949	10.468813
8.733027	568.754663	10.473831
9.081332	564.184117	10.478848
9.026567	551.503229	10.483866
8.757204	545.618828	10.488883
8.839802	543.018107	10.493901
8.767227	557.839565	10.498919
9.019747	560.024799	10.503936
9.019980	565.970241	10.508954
8.841064	565.714219	10.513971
9.220633	550.961351	10.518989
8.907471	563.876544	10.524007
9.066013	561.724666	10.529024
8.749916	561.067263	10.534042
9.079769	565.196971	10.539059
9.274965	557.895410	10.544077
8.989985	554.828419	10.549095
8.800520	537.425494	10.554112
9.090619	556.324208	10.559130
8.783532	560.294938	10.564147
8.969325	556.841761	10.569165
8.732922	559.816810	10.574183
8.871840	559.952800	10.579200
9.286913	565.422990	10.584218
8.625717	563.140776	10.589235
9.226911	565.997212	10.594253
9.033079	556.686406	10.599271
8.939726	560.929759	10.604288
9.248185	552.297645	10.609306
8.975969	558.954800	10.614323
8.909778	558.444432	10.619341
8.866708	561.900427	10.624359
9.200672	554.605528	10.629376
9.051898	561.581012	10.634394
8.732557	555.231070	10.639411
8.777419	556.101317	10.644429
9.276053	562.170637	10.649447
9.222427	560.459100	10.654464
9.404952	572.517153	10.659482
8.922663	561.323351	10.664499
9.069745	561.366544	10.669517
8.890258	570.158269	10.674535
9.614546	578.518058	10.679552
9.550227	575.757315	10.684570
9.055988	569.873427	10.689587
9.506429	571.484855	10.694605
9.069613	569.120146	10.699623
9.186491	563.553917	10.704640
9.368564	574.807316	10.709658
9.126475	577.616001	10.714675
9.186794	580.901166	10.719693
9.564132	581.507883	10.724711
9.383611	583.820930	10.729728
9.456876	568.478570	10.734746
8.878613	571.680752	10.739763
9.317567	568.276269	10.744781
9.148786	577.233577	10.749799
9.404220	580.857399	10.754816
9.339542	572.618253	10.759834
9.229645	584.952505	10.764851
9.136467	574.745452	10.769869
9.459286	594.655246	10.774887
9.042885	594.619470	10.779904
9.701182	592.666996	10.784922
9.202755	593.660238	10.789939
9.790492	581.771751	10.794957
9.483871	589.721872	10.799975
9.473744	587.757365	10.804992
9.784434	576.587629	10.810010
9.392412	588.259190	10.815027
9.328630	582.929543	10.820045
9.701860	586.197240	10.825063
9.364446	585.013002	10.830080
9.364499	586.190072	10.835098
9.174212	589.659671	10.840115
9.201863	585.637977	10.845133
9.465991	594.947184	10.850151
9.166282	598.689549	10.855168
9.567098	589.730523	10.860186
9.373799	585.336350	10.865203
9.437971	589.889543	10.870221
9.056631	590.239592	10.875239
9.266757	596.877991	10.880256
9.551408	610.223413	10.885274
9.442879	615.763035	10.890291
9.535131	611.589202	10.895309
9.392402	609.036399	10.900327
9.605627	614.178470	10.905344
9.866987	609.369072	10.910362
9.850331	613.625667	10.915379
9.626919	621.597479	10.920397
9.362608	616.075180	10.925415
9.834003	620.220594	10.930432
9.519784	612.386602	10.935450
9.406657	612.590486	10.940467
9.736667	613.204620	10.945485
9.731734	613.457823	10.950503
9.719179	620.408832	10.955520
9.604716	617.946273	10.960538
9.646090	613.824592	10.965555
9.918336	619.291931	10.970573
9.952321	619.482233	10.975591
9.794503	622.536497	10.980608
9.907954	615.279279	10.985626
9.720759	620.468311	10.990643
9.800351	618.751674	10.995661
9.803649	610.662806	11.000679
9.793777	618.657963	11.005696
9.561633	616.744018	11.010714
9.582092	619.842932	11.015731
9.411564	615.842815	11.020749
9.121154	613.590860	11.025767
9.484772	614.076652	11.030784
9.826459	614.625840	11.035802
9.502115	628.322314	11.040819
10.072460	635.835250	11.045837
9.974284	636.478604	11.050855
10.097226	634.594227	11.055872
10.100636	628.632346	11.060890
10.117969	633.921880	11.065907
9.880976	621.408350	11.070925
9.887170	613.082342	11.075943
9.530861	614.432015	11.080960
9.804602	621.609565	11.085978
9.807487	633.575885	11.090995
10.080213	637.443162	11.096013
10.110520	631.953592	11.101031
9.887993	638.369462	11.106048
10.324904	638.840615	11.111066
10.075218	644.235105	11.116083
10.163258	642.930553	11.121101
10.112105	633.922399	11.126119
9.813255	626.969618	11.131136
9.926899	626.803456	11.136154
9.847446	640.423699	11.141171
10.057438	644.767866	11.146189
10.116218	639.166535	11.151207
9.992012	634.395451	11.156224
9.954753	630.715277	11.161242
9.965534	639.922192	11.166259
10.034853	630.121992	11.171277
10.187587	629.974951	11.176295
9.809529	637.645953	11.181312
10.001772	627.491979	11.186330
9.914137	646.793956	11.191347
10.239301	631.888600	11.196365
10.439939	625.457161	11.201383
10.165768	646.918532	11.206400
10.365885	642.809842	11.211418
10.033026	637.213070	11.216435
9.998310	633.576678	11.221453
9.868705	632.123191	11.226471
10.002435	637.722692	11.231488
10.103030	633.954646	11.236506
10.041720	639.919222	11.241523
9.926733	640.211761	11.246541
10.149322	650.770893	11.251559
10.545691	659.469279	11.256576
10.459206	652.754613	11.261594
10.158991	651.308921	11.266611
10.336353	654.465308	11.271629
10.328596	653.743811	11.276647
10.369885	654.494702	11.281664
10.486407	650.708377	11.286682
10.086954	644.336242	11.291699
10.358097	656.497231	11.296717
10.477437	642.801231	11.301735
9.987061	649.697729	11.306752
10.720732	652.120012	11.311770
10.383659	659.008272	11.316787
10.195794	653.145780	11.321805
10.414917	657.816724	11.326823
10.170834	661.834409	11.331840
10.525297	654.993849	11.336858
10.160930	663.057192	11.341875
10.334700	668.483172	11.346893
10.598969	661.918673	11.351911
10.628277	670.393709	11.356928
10.379789	659.930075	11.361946
10.391364	664.557800	11.366963
10.533666	670.105476	11.371981
10.490970	658.284157	11.376999
10.751670	659.925323	11.382016
10.489518	662.046042	11.387034
10.488207	666.379141	11.392051
10.719008	660.728760	11.397069
10.836832	669.297224	11.402087
10.408332	662.472041	11.407104
10.726461	666.127083	11.412122
10.671417	668.960124	11.417139
10.655259	659.400519	11.422157
10.464347	654.930216	11.427175
10.477667	663.546609	11.432192
10.887465	655.217304	11.437210
10.681824	654.138647	11.442227
10.546681	664.188948	11.447245
10.794217	653.057463	11.452263
10.584824	662.261017	11.457280
10.564956	657.984820	11.462298
10.461377	661.740649	11.467315
10.762110	656.600021	11.472333
10.801409	658.553587	11.477351
10.515712	655.846453	11.482368
10.706245	660.651265	11.487386
10.240176	662.731351	11.492403
10.530434	663.370650	11.497421
10.684049	656.548936	11.502439
10.612759	666.661817	11.507456
10.544535	656.968360	11.512474
10.856417	655.597177	11.517491
10.437642	658.594504	11.522509
10.730394	656.383717	11.527527
10.720692	669.166232	11.532544
10.834315	659.854536	11.537562
10.872867	662.234254	11.542579
10.644455	662.042791	11.547597
10.813624	674.535351	11.552615
10.841387	686.740807	11.557632
10.980234	680.183330	11.562650
11.061070	685.169439	11.567667
10.979587	678.491849	11.572685
10.665533	672.245179	11.577703
10.924142	684.477579	11.582720
10.827988	678.083156	11.587738
10.870287	680.661105	11.592755
10.707840	693.186702	11.597773
11.462133	689.410896	11.602791
10.988873	687.708291	11.607808
10.868489	686.401678	11.612826
11.092264	687.966580	11.617843
10.867867	683.804474	11.622861
11.139125	689.969425	11.627879
10.790061	690.071421	11.632896
11.028659	684.852157	11.637914
11.344353	694.661424	11.642931
10.634931	688.820678	11.647949
11.081529	687.229569	11.652967
11.007866	695.465129	11.657984
11.035435	687.975184	11.663002
11.412420	690.579591	11.668019
11.234089	695.129782	11.673037
11.097961	690.912818	11.678055
11.283802	702.538093	11.683072
11.459988	684.547557	11.688090
11.349694	682.074868	11.693107
10.885119	672.191039	11.698125
10.885546	663.433565	11.703143
11.323037	683.476970	11.708160
10.889633	690.945226	11.713178
11.289134	695.521646	11.718195
10.838661	687.131455	11.723213
11.229599	690.244918	11.728231
11.250685	688.669985	11.733248
11.457358	693.885689	11.738266
11.260801	676.133445	11.743283
11.140185	688.324280	11.748301
11.454559	679.407155	11.753319
11.078728	682.404069	11.758336
11.454581	683.853625	11.763354
11.236197	684.755657	11.768371
11.086657	683.646117	11.773389
11.248427	675.043240	11.778407
11.084460	681.206952	11.783424
11.290084	688.306838	11.788442
11.394644	678.747244	11.793459
10.913148	689.031708	11.798477
11.193735	683.802710	11.803495
11.186856	686.666077	11.808512
11.209810	686.482566	11.813530
11.199330	677.960324	11.818547
10.773437	695.191491	11.823565
11.054508	696.687456	11.828583
11.152215	720.703664	11.833600
11.442541	718.218694	11.838618
11.552479	718.416031	11.843635
11.504313	722.021178	11.848653
11.309524	722.951074	11.853671
11.554570	719.580100	11.858688
11.449192	711.549240	11.863706
11.503516	718.922155	11.868723
11.365141	718.770233	11.873741
11.886898	718.776812	11.878759
11.370002	721.016348	11.883776
11.498786	720.910929	11.888794
11.723859	720.096143	11.893811
11.362914	718.319133	11.898829
11.723510	710.328873	11.903847
11.007633	723.165266	11.908864
11.320476	716.454281	11.913882
11.625434	715.046309	11.918899
11.825187	724.062712	11.923917
11.671930	722.906414	11.928935
11.520021	720.550694	11.933952
11.389616	713.432631	11.938970
12.104812	729.099638	11.943987
11.994894	728.012289	11.949005
11.850519	715.714556	11.954023
11.946013	721.724020	11.959040
11.799650	721.522856	11.964058
11.692703	719.620841	11.969075
11.648748	712.239922	11.974093
11.809378	711.687700	11.979111
11.716601	723.110489	11.984128
11.779255	715.744424	11.989146
11.795158	714.921386	11.994163
11.801084	718.454941	11.999181
11.211202	714.113406	12.004199
11.615408	720.819273	12.009216
11.541124	736.278622	12.014234
12.102702	731.639904	12.019251
11.892826	750.992705	12.024269
11.965528	740.197830	12.029287
11.943666	748.242261	12.034304
11.771964	738.252546	12.039322
12.359226	736.516316	12.044339
11.997169	742.303985	12.049357
11.820277	725.388059	12.054375
11.983092	730.721100	12.059392
12.115361	734.329537	12.064410
12.033829	724.543454	12.069427
11.968890	722.167795	12.074445
11.937727	712.705187	12.079463
11.837609	727.057729	12.084480
11.897745	735.625796	12.089498
12.159489	734.754771	12.094515
11.599523	748.778590	12.099533
11.620596	747.017461	12.104551
11.849486	748.395373	12.109568
12.004036	755.089877	12.114586
11.956084	743.736388	12.119603
11.948880	745.968651	12.124621
12.171159	738.990979	12.129639
12.401156	750.764002	12.134656
12.068149	750.156577	12.139674
11.844409	746.385676	12.144691
12.060579	754.402281	12.149709
12.162200	740.039949	12.154727
12.213548	743.108798	12.159744
12.069577	749.446126	12.164762
12.408178	743.355949	12.169779
12.317695	747.412703	12.174797
12.328346	742.137619	12.179815
12.330903	743.863421	12.184832
12.043207	743.438246	12.189850
11.876147	740.617836	12.194867
12.049662	754.889656	12.199885
11.878600	750.457244	12.204903
12.067741	751.213376	12.209920
12.180747	760.016170	12.214938
12.677826	767.720523	12.219955
12.179448	768.174120	12.224973
12.521772	767.031690	12.229991
12.370546	762.454155	12.235008
11.713438	756.030830	12.240026
12.092503	766.227840	12.245043
12.311500	770.302382	12.250061
12.328114	777.886359	12.255079
12.483546	776.618575	12.260096
12.273143	770.958393	12.265114
12.346171	761.220656	12.270131
12.137418	778.326362	12.275149
12.482759	780.124692	12.280167
12.392283	767.499739	12.285184
12.454754	777.809478	12.290202
12.464967	762.511545	12.295219
12.420504	774.094055	12.300237
12.579292	770.389446	12.305255
12.638126	766.391228	12.310272
12.212792	767.969478	12.315290
12.533753	761.907305	12.320307
12.749067	765.228180	12.325325
12.580454	765.939380	12.330343
12.730284	758.357666	12.335360
12.258837	765.841381	12.340378
12.601696	760.211282	12.345395
12.531874	761.617064	12.350413
12.527397	766.300979	12.355431
12.654559	764.740978	12.360448
12.375222	764.904633	12.365466
12.605501	779.959692	12.370483
12.705267	791.314487	12.375501
12.959944	791.119914	12.380519
13.003282	779.013635	12.385536
12.533978	779.860311	12.390554
12.900718	771.764919	12.395571
12.777379	766.750665	12.400589
12.946889	777.283475	12.405607
13.184070	774.264021	12.410624
12.820256	769.672455	12.415642
13.104210	757.503244	12.420659
12.990785	766.631854	12.425677
12.683459	774.272896	12.430695
13.043128	776.472927	12.435712
13.026445	765.398550	12.440730
12.737668	762.221663	12.445747
12.988189	766.493238	12.450765
12.664241	766.780648	12.455783
12.794850	769.650889	12.460800
12.691621	768.003909	12.465818
12.602117	765.827755	12.470835
12.485666	771.397069	12.475853
12.273423	770.057505	12.480871
12.680011	780.761456	12.485888
12.574971	792.994103	12.490906
12.559134	784.501053	12.495923
12.658267	787.934810	12.500941
12.504616	801.879229	12.505959
13.110985	790.994396	12.510976
12.981031	800.917728	12.515994
12.821482	789.269268	12.521011
13.135365	798.005892	12.526029
13.076960	798.371619	12.531047
13.300958	795.010241	12.536064
12.798229	804.161998	12.541082
13.185367	803.132466	12.546099
13.301235	796.597482	12.551117
12.982084	797.972903	12.556135
13.278399	793.558770	12.561152
13.054483	803.171775	12.566170
13.390667	795.081159	12.571187
13.218524	800.501417	12.576205
13.137847	803.745598	12.581223
13.103446	792.853862	12.586240
13.038450	794.224177	12.591258
13.018103	798.383563	12.596275
13.081996	800.932900	12.601293
13.000659	817.892446	12.606311
13.333343	821.930252	12.611328
13.130381	830.870950	12.616346
13.345191	822.168173	12.621363
13.645381	830.089596	12.626381
13.496540	832.918425	12.631399
13.197848	810.681823	12.636416
13.345982	825.295351	12.641434
13.648580	823.057754	12.646451
13.375429	804.651501	12.651469
13.364000	808.708506	12.656487
13.773689	800.183490	12.661504
13.235978	805.370690	12.666522
13.368384	805.075354	12.671539
13.507058	797.583734	12.676557
13.291393	799.454186	12.681575
13.375654	793.744672	12.686592
13.225590	804.576881	12.691610
13.589477	813.513963	12.696627
13.543446	813.489584	12.701645
13.501157	821.578274	12.706663
13.234114	819.799164	12.711680
13.400499	821.414096	12.716698
13.709358	821.397229	12.721715
13.540678	816.898154	12.726733
13.761471	815.459179	12.731751
13.932353	822.397304	12.736768
13.428705	805.179046	12.741786
13.373919	815.614477	12.746803
13.894997	819.341895	12.751821
13.498671	824.005170	12.756839
13.814218	815.100417	12.761856
13.432135	821.831688	12.766874
13.570807	820.329840	12.771891
13.661685	824.247741	12.776909
13.778906	826.334285	12.781927
13.903097	825.162913	12.786944
13.693225	832.110205	12.791962
13.586873	821.538998	12.796979
13.778697	820.776755	12.801997
13.832953	823.371786	12.807015
13.872662	826.429850	12.812032
13.755312	832.084531	12.817050
13.751589	823.722109	12.822067
13.633336	819.858924	12.827085
13.809137	822.725249	12.832103
14.005589	829.160747	12.837120
13.604960	829.397056	12.842138
13.455069	822.575495	12.847155
13.536828	834.475943	12.852173
13.982748	827.845052	12.857191
13.624170	821.539032	12.862208
13.617711	827.621311	12.867226
13.289342	826.921637	12.872243
13.959065	835.264852	12.877261
14.078400	841.453659	12.882279
13.764926	831.688079	12.887296
13.837713	837.388711	12.892314
13.830221	839.554758	12.897331
14.214407	842.082319	12.902349
13.802711	842.231998	12.907367
14.227930	847.517648	12.912384
14.041672	849.329849	12.917402
14.208326	848.057146	12.922419
14.446352	849.758688	12.927437
14.128328	839.261661	12.932455
14.088896	827.748992	12.937472
13.811348	838.219339	12.942490
14.094330	842.097677	12.947507
14.473288	834.142355	12.952525
14.105075	841.764563	12.957543
14.640130	836.770209	12.962560
14.075295	835.306002	12.967578
13.985418	824.473432	12.972595
14.351088	825.788895	12.977613
14.005360	833.095148	12.982631
13.936304	837.883876	12.987648
13.811961	846.200031	12.992666
14.304531	847.760703	12.997683
14.482133	838.479916	13.002701
14.494734	854.089858	13.007719
14.349705	842.028828	13.012736
14.255856	849.611208	13.017754
14.002774	859.863137	13.022771
14.349798	849.968812	13.027789
13.957273	858.566836	13.032807
14.173315	855.307680	13.037824
13.859758	854.466828	13.042842
14.004287	846.377816	13.047859
14.472206	854.080464	13.052877
14.307938	877.506761	13.057895
14.569875	867.070329	13.062912
14.619872	869.423034	13.067930
14.676282	876.256038	13.072947
14.497372	854.183653	13.077965
14.458878	849.768315	13.082983
14.683988	849.953920	13.088000
14.451382	851.943799	13.093018
14.530820	840.712302	13.098035
14.703068	848.549637	13.103053
14.348428	849.536143	13.108071
14.463377	855.097629	13.113088
14.480408	861.419238	13.118106
14.487491	865.631148	13.123123
14.794035	868.325515	13.128141
14.796793	867.940036	13.133159
14.745705	860.080486	13.138176
14.375604	863.568844	13.143194
14.672264	864.664745	13.148211
14.491101	859.918304	13.153229
14.323831	872.040833	13.158247
14.671863	872.951959	13.163264
14.501484	870.567554	13.168282
14.596199	869.164109	13.173299
14.870244	869.764930	13.178317
14.413020	875.715877	13.183335
14.408617	868.925152	13.188352
14.426078	872.251801	13.193370
14.585619	869.607418	13.198387
15.095942	877.331835	13.203405
14.637615	886.981612	13.208423
14.922199	881.035553	13.213440
14.999404	887.944199	13.218458
14.841625	893.475844	13.223475
15.269798	866.792304	13.228493
14.862853	873.458061	13.233511
14.718099	868.753251	13.238528
14.613707	874.771994	13.243546
14.486419	896.882845	13.248563
14.931356	890.299423	13.253581
14.783208	892.809412	13.258599
14.832250	884.037901	13.263616
14.446618	889.744103	13.268634
14.623086	900.468403	13.273651
15.158355	890.348898	13.278669
15.286717	898.571834	13.283687
15.114014	899.551927	13.288704
15.245630	890.369838	13.293722
15.058184	900.109726	13.298739
15.118746	891.803473	13.303757
14.974173	882.888727	13.308775
14.782777	883.010201	13.313792
14.688432	902.051569	13.318810
14.797210	911.621972	13.323827
15.095387	909.258824	13.328845
15.218035	920.789999	13.333863
15.096389	919.224786	13.338880
15.396561	913.724405	13.343898
15.340287	906.623052	13.348915
15.616232	914.964885	13.353933
15.649248	922.650496	13.358951
15.588712	915.524561	13.363968
15.336382	908.671679	13.368986
15.728993	915.082786	13.374003
15.738706	900.144581	13.379021
15.380376	897.395139	13.384039
15.287534	891.637603	13.389056
15.519684	888.855607	13.394074
15.189049	898.021473	13.399091
15.565115	883.464544	13.404109
15.511124	885.256024	13.409127
15.365210	873.895710	13.414144
15.661066	884.080580	13.419162
15.178888	879.040465	13.424179
15.174879	888.555943	13.429197
15.098001	906.209161	13.434215
15.384354	909.118139	13.439232
15.910603	918.326485	13.444250
15.510240	910.543729	13.449267
15.685544	915.262632	13.454285
15.639307	923.342520	13.459303
15.642621	915.647994	13.464320
15.827912	916.417360	13.469338
15.490085	921.377611	13.474355
15.612341	911.259690	13.479373
15.924695	912.592980	13.484391
15.559706	912.691160	13.489408
15.528737	907.113275	13.494426
15.521555	920.839175	13.499443
16.007073	907.025638	13.504461
16.150742	907.283965	13.509479
16.103813	904.567785	13.514496
15.529244	891.579930	13.519514
15.766597	895.058324	13.524531
15.525039	889.737506	13.529549
15.792872	904.688955	13.534567
15.582049	902.853689	13.539584
16.010769	914.179112	13.544602
15.991889	908.993814	13.549619
16.172606	909.940624	13.554637
15.627225	905.453211	13.559655
16.135194	900.583006	13.564672
15.930585	903.196517	13.569690
15.524669	908.230551	13.574707
15.656411	906.275339	13.579725
15.873745	906.632579	13.584743
15.638886	919.106562	13.589760
15.908920	917.050784	13.594778
15.791609	917.283729	13.599795
15.995165	911.864760	13.604813
15.994581	915.172153	13.609831
15.901913	911.629992	13.614848
16.013494	912.177374	13.619866
16.021860	925.361190	13.624883
15.923428	915.397766	13.629901
15.522389	915.163918	13.634919
16.012055	930.875907	13.639936
16.025911	942.906988	13.644954
16.213899	941.062882	13.649971
16.202448	945.590144	13.654989
15.948519	944.070903	13.660007
16.378069	950.106999	13.665024
16.429957	945.686944	13.670042
16.593951	943.969675	13.675059
16.443571	934.061718	13.680077
16.300611	930.038276	13.685095
16.050533	928.935005	13.690112
16.323493	935.131333	13.695130
16.258294	937.757721	13.700147
16.424927	941.446024	13.705165
16.380403	936.697089	13.710183
16.060750	933.083189	13.715200
16.514022	940.605130	13.720218
16.230430	942.644033	13.725235
16.575743	946.222289	13.730253
16.494144	945.111555	13.735271
16.196288	945.338074	13.740288
16.682028	936.854727	13.745306
16.568478	943.667048	13.750323
16.717004	937.843276	13.755341
16.656342	941.011761	13.760359
16.484648	940.612588	13.765376
16.642576	935.216540	13.770394
16.606996	945.055736	13.775411
16.533288	937.780374	13.780429
16.830064	943.351270	13.785447
16.663814	941.464834	13.790464
16.481498	918.720705	13.795482
16.465475	929.828638	13.800499
16.804221	938.637177	13.805517
16.696769	932.610512	13.810535
16.621573	946.044125	13.815552
16.984656	942.929176	13.820570
16.619775	945.798184	13.825587
16.705121	937.923534	13.830605
16.423308	932.129320	13.835623
16.471985	939.474808	13.840640
16.809784	943.123669	13.845658
16.675710	945.259069	13.850675
16.641711	945.526299	13.855693
17.068866	948.236494	13.860711
16.379616	941.537266	13.865728
16.750909	940.163065	13.870746
16.607079	948.990414	13.875763
16.728166	942.918470	13.880781
16.822951	943.301224	13.885799
16.477972	939.486160	13.890816
16.844707	938.040088	13.895834
16.665002	944.260006	13.900851
16.827394	956.002731	13.905869
16.917761	964.152753	13.910887
16.694998	964.399066	13.915904
16.968181	967.373234	13.920922
17.276178	963.108711	13.925939
16.850986	958.826520	13.930957
17.284832	971.445079	13.935975
17.118626	956.651156	13.940992
17.330783	958.176877	13.946010
17.270806	964.248652	13.951027
17.339008	966.516466	13.956045
17.422210	965.493520	13.961063
16.951327	964.560545	13.966080
17.370314	957.113303	13.971098
17.511356	956.431596	13.976115
17.119117	950.982887	13.981133
17.205248	949.871119	13.986151
16.797413	954.889687	13.991168
17.052066	954.114439	13.996186
17.202322	954.873516	14.001203
17.390748	960.915838	14.006221
17.183569	958.410953	14.011239
17.273872	964.124660	14.016256
17.356238	953.022024	14.021274
17.108767	948.838224	14.026291
16.943935	969.329780	14.031309
17.219217	957.849769	14.036327
17.069109	964.702540	14.041344
17.649927	954.522214	14.046362
17.616404	959.179172	14.051379
17.348539	957.109837	14.056397
17.587618	955.431297	14.061415
17.375558	963.543495	14.066432
17.728007	956.485382	14.071450
17.352038	956.957674	14.076467
17.224412	955.809969	14.081485
17.402943	968.821986	14.086503
17.627939	987.832345	14.091520
17.828535	979.791294	14.096538
17.827048	979.775715	14.101555
17.719572	986.830102	14.106573
17.939309	975.762734	14.111591
17.568977	971.156357	14.116608
17.619703	960.942316	14.121626
17.422291	970.952051	14.126643
17.600662	981.294242	14.131661
17.739776	978.911825	14.136679
17.558041	985.987314	14.141696
17.786329	980.678060	14.146714
17.857626	985.091380	14.151731
17.746250	987.125396	14.156749
17.952519	983.549006	14.161767
17.820142	985.920834	14.166784
18.107660	982.877679	14.171802
18.108199	980.090932	14.176819
17.663803	976.180982	14.181837
17.591382	977.868060	14.186855
17.793002	990.854384	14.191872
17.795445	975.286081	14.196890
18.072534	989.680719	14.201907
17.890176	981.762787	14.206925
18.075097	968.747397	14.211943
18.162617	976.610688	14.216960
18.107101	981.665581	14.221978
18.015556	983.352500	14.226995
17.757174	985.819812	14.232013
18.288867	972.828983	14.237031
18.273023	978.237428	14.242048
18.156578	983.999315	14.247066
18.054144	979.688639	14.252083
17.938203	991.708532	14.257101
18.074985	983.093642	14.262119
17.962178	985.427689	14.267136
17.926337	979.121540	14.272154
18.143278	983.903367	14.277171
17.818759	989.161360	14.282189
18.066060	1006.082216	14.287207
18.424823	1009.689937	14.292224
18.626706	1005.271612	14.297242
18.333277	1002.193243	14.302259
18.153656	1005.250988	14.307277
18.062106	1007.591175	14.312295
18.240541	1011.179812	14.317312
18.363779	1013.202318	14.322330
18.771256	1010.405456	14.327347
18.671623	1004.765714	14.332365
18.449815	1004.380703	14.337383
18.303004	1011.046779	14.342400
18.213873	1010.470563	14.347418
18.234843	1010.839637	14.352435
18.465860	1014.177034	14.357453
18.466373	1012.084578	14.362471
18.469224	1014.930693	14.367488
18.589650	1007.407131	14.372506
18.681601	1005.126776	14.377523
18.450842	1008.754278	14.382541
18.662765	997.505081	14.387559
18.567776	1013.558061	14.392576
18.630889	1008.056924	14.397594
18.656264	1006.452888	14.402611
18.546113	1008.814925	14.407629
18.706326	1006.757409	14.412647
18.627146	1012.131606	14.417664
18.791713	1004.572725	14.422682
18.771708	1007.832684	14.427699
18.390344	1001.568041	14.432717
18.625348	993.941323	14.437735
18.813458	1010.448571	14.442752
18.884384	1020.302680	14.447770
18.828168	1018.209644	14.452787
18.933409	1013.920071	14.457805
19.346035	1024.973525	14.462823
19.100889	1006.307050	14.467840
18.762202	1005.709973	14.472858
18.925517	995.525609	14.477875
18.712467	1001.981150	14.482893
19.089252	1006.084673	14.487911
19.034659	1020.831112	14.492928
18.730502	1008.864332	14.497946
18.784239	1018.484442	14.502963
19.275848	1022.847696	14.507981
18.827493	1020.225952	14.512999
18.626454	1021.248362	14.518016
18.661653	1021.362736	14.523034
18.872713	1020.600627	14.528051
18.745049	1027.860170	14.533069
18.945135	1027.465861	14.538087
18.765048	1039.360133	14.543104
19.150745	1041.237376	14.548122
18.952300	1047.327719	14.553139
19.269682	1059.557480	14.558157
19.377711	1050.334823	14.563175
19.599343	1060.051729	14.568192
19.468447	1044.715701	14.573210
19.594924	1047.100630	14.578227
19.386375	1050.961351	14.583245
19.697070	1039.601975	14.588263
19.364701	1024.657302	14.593280
19.474654	1015.645805	14.598298
19.824103	1014.596920	14.603315
19.660241	1017.115699	14.608333
19.552764	1020.111649	14.613351
19.450113	1020.506404	14.618368
19.410486	1018.994605	14.623386
19.409996	1022.967892	14.628403
18.988602	1015.567089	14.633421
19.352467	1013.032686	14.638439
19.254641	1026.854922	14.643456
19.635876	1040.434847	14.648474
19.813644	1037.030174	14.653491
19.592112	1044.850397	14.658509
19.842502	1033.377394	14.663527
19.829986	1038.324578	14.668544
19.484946	1052.782028	14.673562
20.073034	1040.470297	14.678579
19.614016	1036.306998	14.683597
19.447918	1032.829968	14.688615
19.886749	1035.276410	14.693632
19.955131	1035.691706	14.698650
19.684541	1036.074903	14.703667
19.454911	1043.423013	14.708685
19.741484	1038.855709	14.713703
20.083598	1036.880144	14.718720
20.204103	1040.310602	14.723738
19.961106	1040.632671	14.728755
20.044364	1043.131670	14.733773
20.147940	1038.542544	14.738791
19.713906	1039.538343	14.743808
20.098304	1039.957775	14.748826
20.297296	1032.778506	14.753843
19.809097	1052.576036	14.758861
20.049458	1038.725069	14.763879
20.149830	1045.245129	14.768896
19.799090	1037.981573	14.773914
19.777116	1042.188609	14.778931
20.040480	1040.023407	14.783949
19.969914	1027.527698	14.788967
20.231511	1032.744364	14.793984
20.073237	1043.745265	14.799002
20.575803	1038.594996	14.804019
20.430578	1042.941267	14.809037
20.193521	1038.433914	14.814055
20.317071	1042.611838	14.819072
20.275342	1041.886180	14.824090
20.534880	1030.493798	14.829107
20.173115	1030.537823	14.834125
20.301352	1037.735183	14.839143
20.221451	1031.303372	14.844160
20.290384	1037.452806	14.849178
20.497951	1033.850956	14.854195
20.248948	1035.928632	14.859213
20.462212	1030.334533	14.864231
20.232079	1039.330087	14.869248
20.450653	1040.637054	14.874266
20.356935	1039.401978	14.879283
20.299667	1041.550602	14.884301
20.708347	1041.697979	14.889319
20.687554	1036.705453	14.894336
20.394995	1044.486310	14.899354
20.300220	1036.179081	14.904371
20.046742	1035.455041	14.909389
20.554541	1030.736309	14.914407
20.520107	1038.710256	14.919424
20.537318	1040.399075	14.924442
20.841867	1051.163359	14.929459
20.426236	1055.735042	14.934477
20.435849	1060.227474	14.939495
20.628449	1057.072944	14.944512
20.472107	1073.397528	14.949530
20.813202	1072.394132	14.954547
20.499786	1069.110594	14.959565
20.543711	1068.655543	14.964583
20.866307	1061.914499	14.969600
20.851554	1071.551681	14.974618
21.108687	1068.390193	14.979635
20.636780	1069.701204	14.984653
20.628641	1061.408792	14.989671
20.722859	1064.638241	14.994688
20.930787	1063.946050	14.999706
20.723292	1062.921308	15.004723
20.894482	1081.220657	15.009741
20.901086	1089.595305	15.014759
21.117068	1087.967709	15.019776
21.366818	1083.118978	15.024794
21.339995	1087.838038	15.029811
21.386684	1080.357556	15.034829
20.830764	1063.585906	15.039847
21.069881	1063.763007	15.044864
21.354469	1075.991606	15.049882
21.628444	1065.856138	15.054899
21.612488	1059.095554	15.059917
21.461820	1058.513198	15.064935
21.343327	1054.694182	15.069952
21.286912	1060.904290	15.074970
21.632017	1059.360610	15.079987
21.134273	1049.951993	15.085005
21.248576	1060.872326	15.090023
21.269716	1051.713776	15.095040
20.924210	1059.834303	15.100058
21.320369	1058.102739	15.105075
21.374630	1057.059075	15.110093
21.160587	1061.864268	15.115111
21.429671	1069.844323	15.120128
21.333812	1078.446464	15.125146
21.456594	1080.743611	15.130163
21.546127	1078.173284	15.135181
21.611669	1081.063238	15.140199
21.715202	1077.203118	15.145216
21.403296	1082.007870	15.150234
21.164668	1080.000213	15.155251
21.486054	1088.502269	15.160269
21.091694	1081.296024	15.165287
21.644301	1087.606384	15.170304
21.556109	1092.840003	15.175322
21.408750	1087.564327	15.180339
21.523439	1087.672559	15.185357
21.335848	1089.144157	15.190375
21.573834	1095.005185	15.195392
21.669236	1114.670318	15.200410
22.102423	1110.894243	15.205427
22.167910	1105.133921	15.210445
21.938708	1098.801220	15.215463
21.808110	1092.481474	15.220480
22.024509	1087.672682	15.225498
21.703701	1085.280259	15.230515
21.636315	1095.269691	15.235533
22.076454	1107.290899	15.240551
22.007650	1104.732753	15.245568
22.185492	1111.865565	15.250586
22.212420	1111.217512	15.255603
22.201562	1104.516073	15.260621
21.893193	1092.631950	15.265639
22.020844	1096.730347	15.270656
21.951755	1100.723867	15.275674
21.982052	1100.813763	15.280691
21.741448	1108.311945	15.285709
22.254439	1106.038194	15.290727
22.339865	1099.930758	15.295744
22.326714	1112.559492	15.300762
22.342295	1096.569292	15.305779
22.374504	1091.981866	15.310797
22.198070	1102.976181	15.315815
22.469518	1100.674002	15.320832
21.723818	1106.837486	15.325850
22.040044	1097.241348	15.330867
22.087782	1100.698998	15.335885
22.343332	1099.424973	15.340903
21.994768	1107.246192	15.345920
22.168230	1111.602509	15.350938
22.512838	1118.535621	15.355955
22.833554	1131.373996	15.360973
22.314409	1126.298576	15.365991
22.525812	1119.514970	15.371008
22.723635	1132.842829	15.376026
22.517859	1129.870627	15.381043
22.710165	1139.273426	15.386061
22.681389	1132.511667	15.391079
22.907554	1140.864562	15.396096
22.717885	1126.616988	15.401114
22.675951	1113.693844	15.406131
22.983899	1108.479371	15.411149
22.591072	1109.310923	15.416167
22.683708	1099.894987	15.421184
22.825429	1114.743292	15.426202
23.059590	1111.591708	15.431219
22.899926	1110.411142	15.436237
22.071796	1105.362048	15.441255
22.681855	1115.791318	15.446272
22.527555	1137.215559	15.451290
22.737495	1133.786892	15.456307
23.085883	1126.966040	15.461325
22.859551	1134.976408	15.466343
23.124504	1130.923722	15.471360
22.774087	1133.900949	15.476378
23.018651	1133.446019	15.481395
23.116194	1133.446482	15.486413
22.901006	1131.775983	15.491431
23.006560	1122.591547	15.496448
23.143261	1131.883131	15.501466
23.417969	1136.526556	15.506483
23.078650	1124.356918	15.511501
22.746055	1132.929904	15.516519
22.968209	1131.784189	15.521536
23.114983	1119.860294	15.526554
23.060975	1119.332221	15.531571
23.395173	1118.241537	15.536589
23.186180	1125.548577	15.541607
23.213388	1121.987592	15.546624
22.849603	1134.393560	15.551642
23.481992	1145.892352	15.556659
23.525746	1141.079037	15.561677
23.490187	1149.378266	15.566695
23.484517	1145.121819	15.571712
23.283712	1148.018800	15.576730
23.450591	1143.533341	15.581747
23.497515	1146.268428	15.586765
23.547765	1147.267252	15.591783
23.818784	1153.306165	15.596800
23.796307	1143.561094	15.601818
23.748231	1137.364106	15.606835
23.558384	1119.626148	15.611853
23.730074	1121.760999	15.616871
23.435209	1120.469068	15.621888
23.232974	1129.002691	15.626906
23.565601	1146.440502	15.631923
23.797141	1134.856776	15.636941
23.798387	1143.049246	15.641959
23.705544	1143.909539	15.646976
23.902501	1147.432184	15.651994
23.889485	1145.474379	15.657011
23.876169	1143.475595	15.662029
23.155343	1143.683179	15.667047
23.597777	1138.513900	15.672064
24.076236	1142.065023	15.677082
23.768352	1144.161405	15.682099
24.254797	1139.647968	15.687117
24.189398	1147.585788	15.692135
24.038801	1137.456839	15.697152
23.818365	1133.032067	15.702170
23.953101	1140.058032	15.707187
24.332168	1131.925832	15.712205
24.044069	1144.878542	15.717223
24.257845	1136.557637	15.722240
24.390328	1140.611105	15.727258
24.187968	1142.769850	15.732275
24.615656	1139.960334	15.737293
24.495225	1152.618529	15.742311
24.285005	1140.154090	15.747328
24.431206	1143.268108	15.752346
24.211651	1149.046203	15.757363
24.147637	1146.307415	15.762381
24.420594	1145.052751	15.767399
24.473773	1142.330317	15.772416
24.267357	1145.976124	15.777434
23.969408	1144.867716	15.782451
24.488731	1142.548786	15.787469
24.224790	1136.029004	15.792487
24.279615	1138.134829	15.797504
24.204523	1144.729756	15.802522
24.129628	1145.590393	15.807539
24.432116	1153.224415	15.812557
24.382325	1162.851356	15.817575
24.482216	1167.986097	15.822592
24.277214	1169.444650	15.827610
24.670661	1173.151115	15.832627
24.821142	1172.834005	15.837645
24.487848	1171.686951	15.842663
24.577545	1170.928072	15.847680
24.677475	1166.582488	15.852698
24.365420	1172.318278	15.857715
24.218359	1166.654356	15.862733
24.230678	1175.993854	15.867751
24.813065	1185.796321	15.872768
24.722620	1191.901350	15.877786
24.655436	1191.656215	15.882803
25.120559	1191.971482	15.887821
24.932446	1202.172400	15.892839
25.296656	1191.918577	15.897856
25.178392	1191.482624	15.902874
24.814698	1203.270068	15.907891
25.256219	1187.970467	15.912909
25.187781	1201.983900	15.917927
25.260196	1182.371208	15.922944
24.790993	1168.637628	15.927962
24.625447	1178.576213	15.932979
24.902967	1180.804946	15.937997
24.915640	1181.743385	15.943015
25.201968	1186.656411	15.948032
25.098312	1177.088147	15.953050
25.064052	1181.934633	15.958067
25.153453	1178.991917	15.963085
25.081060	1190.017322	15.968103
24.753939	1186.994694	15.973120
25.047804	1190.508475	15.978138
25.209941	1199.998087	15.983155
25.480612	1198.832142	15.988173
25.648391	1205.799306	15.993191
25.712818	1204.940240	15.998208
25.432208	1207.824487	16.003226
25.846553	1201.580272	16.008243
25.745519	1192.964672	16.013261
25.467683	1189.659758	16.018279
25.672573	1188.646137	16.023296
25.405221	1178.690097	16.028314
25.637386	1185.091726	16.033331
25.762977	1194.811130	16.038349
25.802697	1195.928374	16.043367
25.634699	1194.957398	16.048384
25.431841	1194.048689	16.053402
25.721787	1205.402353	16.058419
25.762198	1192.532523	16.063437
25.956324	1203.430969	16.068455
25.860679	1206.260989	16.073472
25.922755	1198.137399	16.078490
25.679912	1204.547185	16.083507
26.003467	1198.042632	16.088525
25.738917	1191.242051	16.093543
25.563778	1193.443875	16.098560
25.715903	1193.470501	16.103578
25.558625	1193.283665	16.108595
26.146687	1196.445230	16.113613
26.307910	1203.277716	16.118631
25.894971	1191.542458	16.123648
26.306429	1198.124290	16.128666
25.573343	1198.472653	16.133683
25.998923	1197.534911	16.138701
26.055674	1209.250172	16.143719
25.724033	1222.528506	16.148736
26.292788	1216.013932	16.153754
26.190846	1228.445214	16.158771
26.370151	1221.123782	16.163789
26.194413	1216.187041	16.168807
26.228166	1222.402013	16.173824
26.658920	1215.180047	16.178842
26.567276	1218.126210	16.183859
26.645711	1216.387606	16.188877
26.761094	1215.968695	16.193895
26.277416	1219.212975	16.198912
26.572678	1217.159523	16.203930
26.500401	1215.132098	16.208947
26.526736	1211.183055	16.213965
26.668820	1218.472996	16.218983
26.540179	1221.907811	16.224000
26.608145	1216.320640	16.229018
26.763358	1220.645128	16.234035
26.609585	1210.453517	16.239053
26.597576	1207.977979	16.244071
26.480246	1209.302874	16.249088
26.611165	1216.916467	16.254106
26.489188	1218.775439	16.259123
26.604139	1211.953259	16.264141
26.783161	1217.163982	16.269159
26.782823	1209.296327	16.274176
26.870896	1209.222532	16.279194
26.790163	1214.492888	16.284211
26.691406	1206.236698	16.289229
26.832260	1207.653688	16.294247
26.688137	1215.341933	16.299264
27.150433	1218.756744	16.304282
26.805995	1216.812988	16.309299
26.984166	1229.708483	16.314317
27.204026	1239.356335	16.319335
27.277859	1236.567532	16.324352
27.486120	1229.241560	16.329370
27.303254	1227.449219	16.334387
27.170322	1217.241715	16.339405
27.335973	1204.964499	16.344423
27.192298	1215.174242	16.349440
27.429434	1204.801462	16.354458
26.929357	1215.411039	16.359475
27.246986	1222.045452	16.364493
27.173597	1228.438164	16.369511
27.159264	1237.661946	16.374528
27.178610	1230.810556	16.379546
27.062053	1246.614652	16.384563
27.239994	1231.766580	16.389581
27.560506	1229.857498	16.394599
27.614042	1236.678466	16.399616
27.753517	1232.307735	16.404634
27.822609	1230.027778	16.409651
27.638764	1224.634697	16.414669
27.582450	1224.441509	16.419687
27.664038	1237.980169	16.424704
27.645195	1228.231326	16.429722
27.785639	1242.010084	16.434739
28.105521	1239.012310	16.439757
28.018244	1238.565189	16.444775
27.652367	1240.392947	16.449792
27.742793	1233.476769	16.454810
27.868007	1231.345813	16.459827
27.670385	1232.995725	16.464845
27.818396	1234.843956	16.469863
27.624795	1235.076235	16.474880
27.929316	1235.022177	16.479898
27.634373	1231.095065	16.484915
27.731694	1230.903052	16.489933
28.041686	1242.556566	16.494951
27.737542	1254.041214	16.499968
28.168081	1245.118232	16.504986
28.138804	1252.390853	16.510003
28.094750	1255.455803	16.515021
28.219600	1249.140160	16.520039
28.115097	1255.152736	16.525056
28.148490	1251.404557	16.530074
28.159241	1250.203593	16.535091
28.018372	1253.091200	16.540109
28.232891	1246.073520	16.545127
28.414351	1250.898850	16.550144
28.499098	1247.436125	16.555162
27.900686	1251.929194	16.560179
28.114850	1261.003574	16.565197
28.235187	1250.892073	16.570215
28.065310	1258.376080	16.575232
28.735620	1262.446298	16.580250
28.345176	1267.250781	16.585267
28.442805	1272.426934	16.590285
28.452636	1279.690282	16.595303
28.992976	1276.815757	16.600320
28.803424	1273.433876	16.605338
28.751395	1281.978752	16.610355
28.642349	1269.940199	16.615373
28.959722	1269.398117	16.620391
28.267093	1272.788758	16.625408
29.081939	1274.333691	16.630426
28.715188	1278.118259	16.635443
28.897137	1272.137657	16.640461
28.941726	1270.997663	16.645479
28.818461	1279.275979	16.650496
28.756464	1274.636993	16.655514
28.852319	1274.599850	16.660531
29.070113	1261.888377	16.665549
29.288151	1267.919851	16.670567
29.298524	1270.253571	16.675584
29.093362	1263.901264	16.680602
29.395326	1265.548646	16.685619
29.265795	1269.475931	16.690637
28.998226	1273.620513	16.695655
29.267357	1267.638877	16.700672
29.269675	1269.415261	16.705690
29.242179	1267.570169	16.710707
29.333131	1264.519894	16.715725
29.424816	1266.840873	16.720743
29.163442	1267.566626	16.725760
29.272481	1261.676349	16.730778
29.307448	1262.687042	16.735795
29.395894	1265.074803	16.740813
29.610852	1262.737271	16.745831
29.168376	1262.623522	16.750848
29.348918	1263.731331	16.755866
29.417423	1266.043318	16.760883
29.340046	1269.085088	16.765901
29.584606	1256.691328	16.770919
29.162233	1264.236991	16.775936
29.466543	1266.745570	16.780954
29.430337	1281.038047	16.785971
29.372394	1288.804341	16.790989
30.004891	1283.677829	16.796007
29.988490	1290.841147	16.801024
29.723729	1291.075107	16.806042
29.986791	1291.892268	16.811059
30.106785	1287.597162	16.816077
29.847991	1288.076349	16.821095
30.195222	1286.800571	16.826112
29.876456	1269.186809	16.831130
29.939918	1274.961628	16.836147
29.602067	1293.808028	16.841165
30.245722	1284.744334	16.846183
30.010473	1291.553763	16.851200
30.269566	1298.386731	16.856218
29.919424	1302.282315	16.861235
29.832269	1289.410311	16.866253
29.966632	1292.062290	16.871271
29.985257	1297.976691	16.876288
30.028536	1297.748962	16.881306
30.114920	1298.278212	16.886323
29.980523	1299.331223	16.891341
29.669594	1297.028744	16.896359
30.438086	1306.461280	16.901376
30.390402	1317.640689	16.906394
30.211453	1314.418091	16.911411
30.075928	1321.145632	16.916429
30.386295	1323.937304	16.921447
30.682848	1321.025226	16.926464
30.814407	1314.755848	16.931482
31.020894	1312.268153	16.936499
30.752299	1321.235159	16.941517
30.916770	1298.076436	16.946535
30.704118	1291.315024	16.951552
30.547745	1289.736283	16.956570
30.671075	1292.446798	16.961587
30.312556	1300.061369	16.966605
30.727857	1294.274580	16.971623
30.631393	1310.703613	16.976640
30.851804	1314.983194	16.981658
30.854615	1321.758492	16.986675
30.450148	1316.349456	16.991693
31.012318	1310.640641	16.996711
30.732892	1320.543496	17.001728
30.800890	1314.896327	17.006746
31.097924	1312.517526	17.011763
30.683281	1316.562080	17.016781
31.111859	1313.925974	17.021799
31.069607	1314.027239	17.026816
30.939319	1308.998141	17.031834
30.977729	1317.225896	17.036851
31.029789	1330.418944	17.041869
31.120642	1335.047046	17.046887
30.763490	1324.754686	17.051904
31.275256	1325.621247	17.056922
31.396461	1321.897166	17.061939
31.204632	1338.022417	17.066957
31.464678	1328.848385	17.071975
31.094873	1333.816915	17.076992
31.361239	1335.722355	17.082010
31.764909	1315.808298	17.087027
31.445610	1323.615557	17.092045
31.509792	1317.479816	17.097063
31.771729	1331.877105	17.102080
31.748724	1323.400701	17.107098
31.449820	1331.015412	17.112115
31.482267	1333.434047	17.117133
31.624530	1326.058414	17.122151
31.415766	1330.537791	17.127168
31.730089	1329.696372	17.132186
31.346439	1325.385490	17.137203
31.893327	1339.776010	17.142221
31.698422	1348.589467	17.147239
31.663730	1346.818080	17.152256
32.079647	1343.439155	17.157274
32.114323	1341.186667	17.162291
32.120756	1348.409549	17.167309
32.125645	1341.838104	17.172327
32.019901	1344.559270	17.177344
31.724151	1346.934651	17.182362
32.236928	1348.561634	17.187379
31.895425	1340.943042	17.192397
32.083527	1345.738953	17.197415
32.046063	1349.512971	17.202432
31.802272	1345.622001	17.207450
32.302461	1346.783879	17.212467
32.129580	1349.799599	17.217485
32.344434	1336.350046	17.222503
32.331490	1344.718408	17.227520
32.191028	1341.016386	17.232538
32.327881	1338.050429	17.237555
32.113665	1346.595500	17.242573
32.198514	1362.163007	17.247591
32.104479	1370.099100	17.252608
32.275425	1367.967275	17.257626
32.514618	1360.544881	17.262643
32.412709	1370.552500	17.267661
32.825522	1364.409459	17.272679
32.362272	1370.358356	17.277696
32.633495	1378.578065	17.282714
33.149443	1363.825254	17.287731
32.895481	1375.362080	17.292749
33.063862	1362.762423	17.297767
32.933955	1362.950008	17.302784
32.705131	1356.049087	17.307802
33.037654	1358.771019	17.312819
33.231240	1367.772935	17.317837
33.284175	1367.253346	17.322855
33.227078	1357.510426	17.327872
33.154742	1360.939601	17.332890
33.375697	1358.582183	17.337907
32.978806	1363.652799	17.342925
32.980548	1361.452808	17.347943
33.421055	1367.664063	17.352960
33.316808	1368.030672	17.357978
33.163181	1368.433421	17.362995
33.105761	1368.312991	17.368013
33.119089	1362.813233	17.373031
33.113944	1354.087853	17.378048
32.976858	1362.223200	17.383066
33.172913	1363.297026	17.388083
33.304874	1370.970483	17.393101
33.356323	1364.019334	17.398119
33.588294	1364.633078	17.403136
33.332728	1365.698765	17.408154
33.676949	1354.643219	17.413171
33.558034	1365.325713	17.418189
33.427896	1363.626086	17.423207
33.710510	1375.779458	17.428224
33.733876	1385.675936	17.433242
33.617697	1388.963656	17.438259
33.707054	1392.313852	17.443277
33.695457	1391.577147	17.448295
33.715475	1385.732336	17.453312
33.630735	1381.059014	17.458330
33.658595	1380.259320	17.463347
33.630074	1391.574634	17.468365
33.633482	1388.392881	17.473383
33.931644	1382.485557	17.478400
33.860282	1389.947872	17.483418
33.898618	1393.624812	17.488435
33.528247	1399.502360	17.493453
33.787904	1404.362818	17.498471
34.402528	1407.659122	17.503488
34.362693	1414.251780	17.508506
34.531330	1411.186152	17.513523
34.147032	1415.424798	17.518541
34.179070	1406.696722	17.523559
34.390432	1412.842906	17.528576
34.492174	1418.561279	17.533594
34.573449	1407.944547	17.538611
34.481806	1410.666669	17.543629
34.552243	1416.812843	17.548647
34.658306	1405.340124	17.553664
34.276165	1405.052811	17.558682
34.851677	1404.094723	17.563699
34.840476	1402.351210	17.568717
34.428523	1400.572652	17.573735
34.874280	1400.777345	17.578752
34.470288	1405.726004	17.583770
34.734625	1403.364938	17.588787
34.548712	1404.233514	17.593805
34.773653	1401.600898	17.598823
34.848152	1396.416608	17.603840
34.765907	1404.275126	17.608858
34.658339	1394.186629	17.613875
34.326340	1402.380936	17.618893
34.570211	1401.206555	17.623911
34.447980	1393.948077	17.628928
34.439222	1415.526580	17.633946
34.811379	1418.264403	17.638963
34.556383	1429.085026	17.643981
34.748659	1417.418902	17.648999
35.128342	1423.055858	17.654016
34.831074	1432.516582	17.659034
35.001184	1436.122390	17.664051
35.579734	1456.658984	17.669069
35.570535	1440.868027	17.674087
35.364910	1439.274899	17.679104
35.267202	1439.381697	17.684122
35.183125	1442.998928	17.689139
35.380294	1442.917507	17.694157
35.282343	1448.424169	17.699175
35.805374	1448.796644	17.704192
35.439238	1451.110480	17.709210
35.655463	1444.543756	17.714227
35.565779	1448.474306	17.719245
35.455863	1453.339031	17.724263
35.819279	1441.936425	17.729280
35.446884	1452.068524	17.734298
35.406716	1444.367959	17.739315
35.799816	1439.200013	17.744333
35.935682	1439.708891	17.749351
35.658216	1437.344344	17.754368
35.432895	1438.174912	17.759386
35.769291	1447.050347	17.764403
36.100950	1458.135693	17.769421
36.306729	1469.041943	17.774439
36.485578	1456.667809	17.779456
35.769933	1453.466156	17.784474
36.256644	1450.192889	17.789491
36.040700	1449.150511	17.794509
36.340363	1456.488447	17.799527
36.427808	1458.961601	17.804544
36.053803	1449.233569	17.809562
36.125159	1450.336405	17.814579
36.528830	1460.356383	17.819597
36.394326	1467.383635	17.824615
36.965898	1456.368147	17.829632
36.283868	1461.152092	17.834650
36.344448	1456.241377	17.839667
36.322109	1454.124045	17.844685
36.574050	1468.226352	17.849703
36.818957	1460.496894	17.854720
36.465787	1455.253355	17.859738
36.591232	1459.083926	17.864755
36.547013	1467.817025	17.869773
36.340679	1458.450899	17.874791
36.893646	1460.071596	17.879808
37.202923	1467.843551	17.884826
37.081834	1453.168386	17.889843
36.953880	1455.214520	17.894861
36.821023	1457.665383	17.899879
36.991882	1445.885827	17.904896
36.916277	1453.071110	17.909914
37.024320	1460.293897	17.914931
36.817747	1463.371721	17.919949
36.995389	1454.693396	17.924967
36.889393	1448.937740	17.929984
36.263554	1459.724963	17.935002
36.510405	1458.578514	17.940019
37.022033	1487.744531	17.945037
37.146238	1484.865742	17.950055
37.203465	1486.021290	17.955072
37.081633	1487.362690	17.960090
37.123641	1478.781347	17.965107
37.321848	1491.585526	17.970125
37.279214	1487.959668	17.975143
37.527384	1477.127389	17.980160
37.150221	1490.804392	17.985178
37.548541	1494.863629	17.990195
37.659619	1495.161787	17.995213
37.645757	1509.425698	18.000231
37.734444	1504.715703	18.005248
37.567042	1515.352232	18.010266
38.079806	1506.353119	18.015283
37.924352	1512.541030	18.020301
37.967723	1517.473278	18.025319
38.115179	1505.063002	18.030336
38.085517	1494.084885	18.035354
38.049623	1483.817842	18.040371
37.702423	1480.732033	18.045389
37.992689	1495.759363	18.050407
38.138221	1504.292327	18.055424
38.055567	1510.828610	18.060442
38.054726	1499.691333	18.065459
38.021823	1497.118038	18.070477
38.098274	1508.975583	18.075495
38.453683	1506.758033	18.080512
37.922314	1506.598245	18.085530
38.368205	1502.491880	18.090547
38.085409	1495.394224	18.095565
38.235185	1501.209244	18.100583
37.961902	1505.856571	18.105600
38.204861	1500.958296	18.110618
38.134813	1508.568785	18.115635
38.583759	1517.584419	18.120653
38.611566	1526.719692	18.125671
38.604579	1526.805964	18.130688
38.987935	1526.180950	18.135706
39.085954	1533.793520	18.140723
38.987349	1530.135395	18.145741
38.720863	1515.416684	18.150759
39.033548	1499.284895	18.155776
38.897019	1506.085250	18.160794
38.847816	1499.569562	18.165811
38.758492	1510.900789	18.170829
39.020345	1518.219427	18.175847
38.948959	1522.948740	18.180864
38.748313	1522.288988	18.185882
38.889195	1531.788419	18.190899
38.687459	1524.760106	18.195917
38.497078	1528.573900	18.200935
38.934835	1520.009431	18.205952
38.988149	1531.555020	18.210970
38.992486	1538.696252	18.215987
39.418863	1547.336721	18.221005
39.146902	1555.319709	18.226023
39.252308	1558.203495	18.231040
39.691304	1553.788914	18.236058
39.684172	1552.455024	18.241075
39.687605	1550.718671	18.246093
39.431653	1553.182522	18.251111
39.344306	1547.521748	18.256128
39.469274	1549.531420	18.261146
39.660356	1538.338801	18.266163
39.809417	1541.954239	18.271181
39.999485	1552.238122	18.276199
39.756407	1546.046297	18.281216
39.455789	1542.107380	18.286234
39.447075	1542.228639	18.291251
39.865187	1539.407939	18.296269
39.627343	1537.494786	18.301287
39.560319	1539.910098	18.306304
39.927779	1550.352387	18.311322
39.908190	1560.470297	18.316339
39.877472	1570.621516	18.321357
39.898637	1577.015318	18.326375
40.156472	1565.663892	18.331392
40.150659	1572.162910	18.336410
40.014771	1571.268937	18.341427
39.890563	1569.451590	18.346445
39.683404	1563.866389	18.351463
40.137551	1576.378051	18.356480
40.407154	1589.997979	18.361498
40.700600	1591.621478	18.366515
41.142797	1592.991286	18.371533
40.704545	1586.299823	18.376551
40.590895	1566.144633	18.381568
40.757477	1564.635194	18.386586
40.450612	1559.296003	18.391603
40.506903	1562.537797	18.396621
40.631967	1580.384113	18.401639
40.800672	1583.390536	18.406656
40.757805	1590.059477	18.411674
40.909472	1589.104668	18.416691
41.129201	1584.730746	18.421709
40.829667	1582.678922	18.426727
40.877776	1585.830479	18.431744
40.794637	1583.078840	18.436762
40.687258	1589.486475	18.441779
41.148848	1583.057992	18.446797
40.819217	1597.178933	18.451815
40.846073	1579.368694	18.456832
41.302710	1578.571242	18.461850
41.245488	1582.537762	18.466867
41.288846	1581.088656	18.471885
41.200770	1587.354403	18.476903
41.500736	1606.284244	18.481920
41.770991	1593.816795	18.486938
41.210007	1583.846571	18.491955
41.579370	1591.344065	18.496973
41.452470	1609.226731	18.501991
41.523140	1600.378894	18.507008
41.852800	1600.952093	18.512026
41.140870	1610.367420	18.517043
41.668527	1599.595425	18.522061
41.996085	1607.579184	18.527079
41.929965	1608.397440	18.532096
41.665479	1609.117381	18.537114
41.765162	1603.361009	18.542131
42.024289	1597.551254	18.547149
41.913765	1598.922450	18.552167
41.998283	1598.492586	18.557184
41.885313	1598.346142	18.562202
41.839138	1602.869544	18.567219
41.809838	1601.422352	18.572237
41.829568	1601.498127	18.577255
42.068914	1600.630572	18.582272
42.291814	1619.193785	18.587290
42.135929	1619.398066	18.592307
42.459391	1620.186843	18.597325
42.342095	1628.691616	18.602343
42.363432	1619.570616	18.607360
42.642441	1615.881713	18.612378
42.486890	1622.041273	18.617395
42.691101	1623.704005	18.622413
42.866400	1619.936671	18.627431
42.520039	1617.721757	18.632448
42.975209	1622.857772	18.637466
42.595413	1625.325257	18.642483
42.885617	1621.899702	18.647501
42.779891	1620.726429	18.652519
42.807380	1620.456987	18.657536
42.986089	1615.852786	18.662554
42.619860	1618.968275	18.667571
42.753774	1616.551873	18.672589
42.796048	1621.758892	18.677607
42.537741	1628.922375	18.682624
42.528610	1611.714223	18.687642
42.498042	1616.007952	18.692659
42.674283	1623.393698	18.697677
42.697946	1631.630220	18.702695
42.590705	1636.904853	18.707712
42.908142	1636.498458	18.712730
43.051932	1657.283292	18.717747
43.237774	1657.434033	18.722765
43.058092	1669.543266	18.727783
43.363537	1660.425072	18.732800
43.511312	1664.908633	18.737818
43.689714	1662.415823	18.742835
43.673895	1660.505741	18.747853
43.437793	1652.962024	18.752871
43.746029	1658.136851	18.757888
44.018553	1647.335369	18.762906
43.756268	1655.613548	18.767923
43.822110	1661.981445	18.772941
43.873298	1651.710129	18.777959
43.808608	1651.164778	18.782976
43.812023	1658.012696	18.787994
43.803916	1665.039157	18.793011
44.220814	1669.796152	18.798029
44.387004	1668.649705	18.803047
44.142297	1667.842207	18.808064
43.940794	1654.994168	18.813082
44.018666	1676.622533	18.818099
44.426846	1682.573861	18.823117
44.677397	1679.605814	18.828135
44.345113	1683.419781	18.833152
44.704085	1676.451889	18.838170
44.466824	1679.771258	18.843187
44.499440	1667.110603	18.848205
44.690874	1665.483647	18.853223
44.704677	1669.934549	18.858240
44.746739	1655.050608	18.863258
44.687079	1651.067602	18.868275
44.799095	1645.438680	18.873293
44.830727	1658.253297	18.878311
44.539494	1654.331821	18.883328
44.591745	1667.152682	18.888346
44.969340	1681.920319	18.893363
45.182368	1665.100210	18.898381
45.186233	1670.622548	18.903399
45.122451	1683.644648	18.908416
45.144142	1673.816624	18.913434
44.890754	1676.478917	18.918451
45.222121	1671.724543	18.923469
44.918870	1678.162899	18.928487
44.741383	1685.664056	18.933504
45.109498	1677.508079	18.938522
44.968240	1684.141975	18.943539
45.088818	1675.491420	18.948557
45.036558	1681.284502	18.953575
44.885300	1683.129173	18.958592
45.066515	1690.185945	18.963610
45.451941	1694.850043	18.968627
45.395395	1692.974742	18.973645
45.445969	1703.593010	18.978663
45.143405	1702.030826	18.983680
45.412464	1700.514788	18.988698
45.284711	1707.916639	18.993715
45.710725	1714.108195	18.998733
45.972637	1727.312841	19.003751
45.935031	1733.715907	19.008768
46.199429	1728.915204	19.013786
45.884442	1728.475343	19.018803
46.049057	1723.216875	19.023821
46.033054	1725.094011	19.028839
45.728997	1732.072187	19.033856
46.199184	1715.098124	19.038874
46.143846	1718.070241	19.043891
45.822772	1724.464065	19.048909
46.227770	1712.852789	19.053927
45.958654	1714.485542	19.058944
46.271914	1724.579798	19.063962
46.491554	1747.322195	19.068979
46.335922	1749.363230	19.073997
46.573776	1742.729889	19.079015
46.280300	1745.641485	19.084032
46.457778	1741.583433	19.089050
46.239243	1745.912955	19.094067
46.261107	1735.737710	19.099085
46.710992	1744.623916	19.104103
46.463649	1750.150921	19.109120
47.368381	1759.499234	19.114138
47.091728	1763.380246	19.119155
47.289977	1751.974918	19.124173
47.275553	1740.221043	19.129191
46.883424	1735.068737	19.134208
47.176795	1730.238246	19.139226
46.821373	1747.838100	19.144243
46.989472	1753.991179	19.149261
47.279022	1764.707750	19.154279
47.585203	1773.364005	19.159296
47.699556	1747.463674	19.164314
47.590487	1762.373903	19.169331
47.537183	1755.508448	19.174349
47.382568	1752.521813	19.179367
47.258172	1755.558408	19.184384
47.481255	1750.262367	19.189402
47.818743	1760.201360	19.194419
47.860088	1763.849500	19.199437
47.934882	1759.794908	19.204455
47.369224	1761.272143	19.209472
47.749661	1753.912669	19.214490
47.885451	1766.985617	19.219507
47.700233	1754.469491	19.224525
47.908038	1754.083427	19.229543
47.350499	1759.838928	19.234560
47.901255	1755.473064	19.239578
48.049419	1766.451644	19.244595
47.799635	1769.804551	19.249613
47.845120	1775.216252	19.254631
48.030967	1784.983345	19.259648
48.280262	1787.740475	19.264666
48.089768	1784.494352	19.269683
47.973391	1781.321829	19.274701
48.219607	1778.057781	19.279719
48.216416	1790.852701	19.284736
48.450467	1784.563945	19.289754
47.827205	1795.035363	19.294771
48.629914	1811.194577	19.299789
48.775158	1805.146961	19.304807
48.729183	1809.481022	19.309824
49.117157	1806.712344	19.314842
48.516942	1817.887110	19.319859
48.758923	1821.169290	19.324877
48.616580	1812.657700	19.329895
48.876576	1813.462742	19.334912
48.722821	1800.632365	19.339930
48.946305	1809.708720	19.344947
48.746803	1805.671846	19.349965
49.416697	1798.112358	19.354983
49.004009	1804.151311	19.360000
49.225434	1801.746422	19.365018
49.296944	1806.611221	19.370035
48.910524	1816.745722	19.375053
49.519135	1822.337469	19.380071
49.025701	1827.025682	19.385088
49.213935	1830.739191	19.390106
49.211267	1833.299104	19.395123
49.636287	1828.245975	19.400141
49.782014	1814.822675	19.405159
49.446480	1823.623682	19.410176
49.356518	1821.687327	19.415194
49.596894	1830.319204	19.420211
49.712309	1848.243044	19.425229
50.382227	1850.688112	19.430247
50.024594	1852.183257	19.435264
50.082970	1835.017965	19.440282
50.081623	1847.973594	19.445299
50.099181	1851.540267	19.450317
50.342474	1855.620720	19.455335
50.237639	1850.947268	19.460352
50.311103	1840.151610	19.465370
50.079937	1846.654476	19.470387
50.270585	1852.807213	19.475405
50.176977	1844.483645	19.480423
50.726013	1843.577025	19.485440
50.371078	1840.101019	19.490458
50.561196	1844.322354	19.495475
50.403595	1850.936780	19.500493
50.586780	1839.319147	19.505511
50.882212	1856.662488	19.510528
50.756082	1848.416602	19.515546
50.784590	1845.256084	19.520563
50.687822	1845.391141	19.525581
50.794568	1841.760742	19.530599
51.072597	1847.322236	19.535616
51.089199	1851.091044	19.540634
51.150632	1845.552041	19.545651
50.923729	1840.534774	19.550669
51.236130	1846.166626	19.555687
51.105934	1843.488596	19.560704
51.356364	1842.060678	19.565722
51.275108	1842.158588	19.570739
50.920121	1843.059986	19.575757
51.488463	1850.772584	19.580775
51.446130	1864.488935	19.585792
51.313912	1868.634537	19.590810
51.482965	1873.528256	19.595827
51.526636	1872.312624	19.600845
51.450900	1865.002486	19.605863
51.258001	1867.841535	19.610880
51.515124	1871.620003	19.615898
51.454513	1867.826459	19.620915
51.208765	1857.115521	19.625933
51.554916	1879.235465	19.630951
51.698219	1886.478147	19.635968
51.574676	1884.382934	19.640986
51.847077	1890.945782	19.646003
51.439944	1896.336911	19.651021
51.736630	1888.094193	19.656039
51.875775	1903.224444	19.661056
52.128870	1913.994156	19.666074
52.106384	1911.097254	19.671091
52.323838	1914.291769	19.676109
52.312332	1912.087473	19.681127
52.412616	1910.055025	19.686144
52.258656	1911.521419	19.691162
52.361517	1909.677929	19.696179
52.388192	1905.056446	19.701197
52.513297	1909.587805	19.706215
52.424090	1925.157824	19.711232
52.481253	1939.272083	19.716250
52.854652	1926.775619	19.721267
52.910027	1933.353550	19.726285
53.367580	1928.645616	19.731303
52.978914	1920.816398	19.736320
52.916070	1924.051675	19.741338
53.173854	1927.795335	19.746355
53.158207	1931.736482	19.751373
53.490933	1916.816252	19.756391
53.103314	1932.537181	19.761408
53.196195	1922.230773	19.766426
53.103031	1925.413993	19.771443
53.187772	1926.685187	19.776461
53.616910	1930.512462	19.781479
53.637493	1930.594417	19.786496
53.497560	1917.894343	19.791514
53.809100	1919.701245	19.796531
53.472306	1937.418294	19.801549
53.663333	1927.219592	19.806567
53.646341	1934.919786	19.811584
53.910083	1944.273945	19.816602
54.382253	1948.378525	19.821619
53.921441	1945.285186	19.826637
54.009069	1942.494112	19.831655
53.686134	1955.572793	19.836672
53.788965	1950.585890	19.841690
53.909216	1945.167039	19.846707
54.117740	1945.279512	19.851725
53.813481	1945.797399	19.856743
54.152731	1945.185594	19.861760
54.126329	1950.548647	19.866778
53.893580	1962.770541	19.871795
54.148701	1965.646716	19.876813
54.307354	1972.325254	19.881831
53.992083	1971.787593	19.886848
54.247013	1976.112422	19.891866
54.321717	1982.501136	19.896883
54.507377	1993.082631	19.901901
54.614976	1983.689135	19.906919
54.990031	1986.909467	19.911936
54.859703	1990.474090	19.916954
54.784933	1989.564207	19.921971
54.823487	1994.307979	19.926989
54.715213	1986.677816	19.932007
54.728134	1991.611810	19.937024
55.394969	2007.309616	19.942042
55.612744	2008.159156	19.947059
55.293045	1994.672933	19.952077
55.443641	1981.778961	19.957095
55.291651	1984.002503	19.962112
55.352870	1991.930326	19.967130
55.508742	2009.301993	19.972147
55.646548	2016.431972	19.977165
55.820079	2006.179157	19.982183
55.965115	2001.201408	19.987200
55.339158	2001.198455	19.992218
55.875350	2005.491848	19.997235
55.787972	2016.119291	20.002253
56.270112	2019.313383	20.007271
56.360289	2014.846037	20.012288
56.016220	1997.737332	20.017306
56.213336	1988.402397	20.022323
55.927546	1981.254520	20.027341
56.304421	1990.029202	20.032359
56.263514	1995.763798	20.037376
56.357892	2002.982633	20.042394
56.143740	1994.889337	20.047411
56.254163	2001.221965	20.052429
56.134818	2008.890886	20.057447
56.426955	1995.655967	20.062464
56.101907	2008.681364	20.067482
56.281686	1996.619162	20.072499
56.102146	2005.641988	20.077517
56.000150	2019.219470	20.082535
56.479670	2025.090304	20.087552
56.136924	2027.561505	20.092570
56.373724	2024.128461	20.097587
56.772168	2038.921531	20.102605
57.010624	2044.145277	20.107623
56.817678	2041.937832	20.112640
57.100028	2054.905971	20.117658
57.175739	2053.511723	20.122675
57.164084	2058.017206	20.127693
57.478630	2046.984822	20.132711
57.425365	2050.720433	20.137728
57.058285	2049.496555	20.142746
57.577565	2048.086464	20.147763
57.693132	2056.955773	20.152781
57.403149	2049.852710	20.157799
57.644417	2047.533048	20.162816
57.885882	2056.786607	20.167834
57.846363	2059.102998	20.172851
57.638676	2061.799216	20.177869
57.961653	2067.672497	20.182887
57.680852	2062.082898	20.187904
57.578237	2072.835848	20.192922
57.869893	2063.558652	20.197939
57.779960	2073.952981	20.202957
58.162643	2066.630902	20.207975
58.158184	2067.430050	20.212992
58.154662	2071.697558	20.218010
57.833567	2069.115681	20.223027
58.134048	2080.872227	20.228045
58.187226	2089.495687	20.233063
58.329400	2088.321416	20.238080
58.329144	2101.018259	20.243098
58.975436	2094.781582	20.248115
58.687984	2092.017691	20.253133
58.699714	2092.495541	20.258151
58.579862	2087.499305	20.263168
58.854593	2097.757612	20.268186
58.976655	2097.482813	20.273203
59.221779	2095.790598	20.278221
58.928182	2101.896205	20.283239
58.815993	2091.404062	20.288256
59.124063	2107.432744	20.293274
59.516990	2117.028707	20.298291
59.394576	2116.514478	20.303309
58.840065	2104.390510	20.308327
59.671453	2105.601545	20.313344
59.490701	2118.323524	20.318362
59.667161	2117.822433	20.323379
59.834716	2120.598735	20.328397
59.555463	2113.402439	20.333415
59.473860	2110.552640	20.338432
59.754220	2122.593257	20.343450
59.872116	2114.195396	20.348467
60.007114	2103.225825	20.353485
59.530892	2110.407861	20.358503
60.062022	2112.666412	20.363520
60.025999	2112.694115	20.368538
60.004418	2119.097964	20.373555
60.269455	2119.255237	20.378573
59.989155	2108.167679	20.383591
60.180476	2109.362223	20.388608
60.066903	2113.602798	20.393626
60.349251	2113.975128	20.398643
60.177975	2114.582646	20.403661
60.352822	2111.967245	20.408679
60.634503	2131.197177	20.413696
60.456879	2134.456788	20.418714
60.470781	2140.422703	20.423731
60.698554	2140.308082	20.428749
60.359424	2141.516304	20.433767
60.492012	2130.878480	20.438784
60.131278	2138.964005	20.443802
60.383070	2147.445911	20.448819
60.938738	2159.620158	20.453837
60.694646	2157.111418	20.458855
60.953829	2158.721403	20.463872
60.799870	2167.437318	20.468890
61.040381	2175.829480	20.473907
61.490391	2182.613939	20.478925
61.375212	2177.885212	20.483943
61.744075	2171.717224	20.488960
61.521461	2178.398765	20.493978
61.537869	2178.923225	20.498995
61.655277	2174.924985	20.504013
61.496265	2186.052943	20.509031
61.723492	2179.553663	20.514048
61.633246	2181.164743	20.519066
61.546252	2179.480371	20.524083
61.831946	2183.421701	20.529101
61.750509	2200.969602	20.534119
62.426245	2208.106903	20.539136
62.096026	2212.217329	20.544154
61.993338	2204.305307	20.549171
61.997087	2205.784888	20.554189
61.977545	2207.470108	20.559207
62.355727	2195.275693	20.564224
62.083997	2208.289724	20.569242
62.155326	2212.031097	20.574259
62.691208	2227.026872	20.579277
62.797925	2241.206195	20.584295
62.650436	2224.798685	20.589312
62.722385	2237.130831	20.594330
62.909252	2223.088500	20.599347
62.732588	2222.286095	20.604365
62.983257	2225.327126	20.609383
63.238482	2228.446346	20.614400
62.586960	2226.522184	20.619418
62.961506	2207.069337	20.624435
63.343105	2225.232740	20.629453
63.179390	2218.406499	20.634471
63.294811	2217.955998	20.639488
63.034562	2222.323731	20.644506
63.342072	2235.641540	20.649523
63.449033	2241.640250	20.654541
63.444893	2247.997227	20.659559
63.818429	2245.101346	20.664576
63.707111	2254.659611	20.669594
63.848657	2251.970505	20.674611
64.109203	2233.337137	20.679629
63.644633	2243.695578	20.684647
63.944810	2242.616474	20.689664
63.908939	2234.428858	20.694682
63.602661	2239.166756	20.699699
63.786701	2238.045882	20.704717
63.625958	2240.236109	20.709735
64.050359	2253.797573	20.714752
64.087444	2270.247589	20.719770
64.466979	2268.392275	20.724787
64.673582	2269.593904	20.729805
64.447714	2281.493015	20.734823
64.664992	2269.251169	20.739840
64.538158	2271.799038	20.744858
64.568101	2270.689681	20.749875
64.585211	2266.606139	20.754893
64.514530	2278.241071	20.759911
64.817457	2284.701443	20.764928
64.797345	2296.502048	20.769946
64.815109	2290.256473	20.774963
65.060808	2296.403894	20.779981
64.754626	2294.106852	20.784999
65.018397	2288.902118	20.790016
65.019981	2299.200180	20.795034
65.346937	2302.699531	20.800051
65.860620	2300.987313	20.805069
65.902508	2308.473296	20.810087
65.637177	2297.992401	20.815104
65.659651	2293.226296	20.820122
65.523465	2302.081517	20.825139
65.735484	2307.199018	20.830157
65.136718	2312.591888	20.835175
65.785068	2301.005230	20.840192
65.453970	2306.220449	20.845210
65.724308	2310.110559	20.850227
66.140099	2317.818857	20.855245
66.148002	2329.372075	20.860263
66.370585	2331.530660	20.865280
66.116229	2337.567075	20.870298
66.249615	2329.188781	20.875315
66.619856	2323.061555	20.880333
66.420041	2324.099624	20.885351
66.499827	2325.463151	20.890368
66.400803	2340.138734	20.895386
66.735459	2326.745417	20.900403
66.932568	2325.568837	20.905421
66.924656	2324.724208	20.910439
66.799548	2324.885800	20.915456
66.779197	2325.409712	20.920474
66.452258	2328.929459	20.925491
66.886879	2332.964266	20.930509
66.653253	2347.124405	20.935527
67.107232	2349.843242	20.940544
67.216800	2351.060080	20.945562
67.180842	2352.662671	20.950579
67.391935	2348.308854	20.955597
67.039690	2357.343134	20.960615
67.371939	2367.573648	20.965632
67.366417	2380.972171	20.970650
67.265171	2376.793527	20.975667
68.021641	2374.033309	20.980685
67.741933	2380.973202	20.985703
67.824436	2375.834718	20.990720
68.008169	2376.405559	20.995738
67.865833	2373.618887	21.000755
68.100606	2378.117403	21.005773
67.693027	2372.146743	21.010791
68.095842	2376.536871	21.015808
68.279284	2387.519772	21.020826
68.452603	2388.616160	21.025843
68.340971	2387.683627	21.030861
68.113829	2398.917074	21.035879
68.718929	2386.223029	21.040896
68.886882	2398.265662	21.045914
68.858098	2399.198036	21.050931
68.584176	2395.844940	21.055949
68.547476	2404.915020	21.060967
69.101221	2396.833788	21.065984
68.899487	2399.140920	21.071002
68.907874	2400.749192	21.076019
69.137038	2398.728058	21.081037
68.957077	2392.538674	21.086055
68.742170	2389.132147	21.091072
68.986798	2404.486159	21.096090
68.708608	2419.713793	21.101107
68.826086	2411.524163	21.106125
69.173284	2422.639236	21.111143
69.487643	2430.827424	21.116160
69.839929	2433.480148	21.121178
69.572203	2435.257927	21.126195
69.865876	2427.968585	21.131213
69.513576	2442.661840	21.136231
69.599793	2434.799023	21.141248
69.918619	2435.550692	21.146266
69.734290	2438.309584	21.151283
70.439249	2452.032390	21.156301
70.151781	2459.522695	21.161319
70.322916	2461.143347	21.166336
70.486237	2459.369231	21.171354
70.400196	2453.417602	21.176371
70.723601	2453.136502	21.181389
70.456795	2460.980212	21.186407
70.599472	2457.536585	21.191424
70.507280	2455.979245	21.196442
70.355082	2457.524310	21.201459
70.889427	2457.904508	21.206477
70.356367	2465.859371	21.211495
70.783911	2477.012387	21.216512
71.197348	2483.253525	21.221530
70.922072	2484.098278	21.226547
70.989068	2485.397542	21.231565
71.080875	2487.942747	21.236583
71.106517	2488.598327	21.241600
71.452066	2482.074088	21.246618
71.068794	2486.678931	21.251635
71.487130	2497.442042	21.256653
71.320742	2514.542763	21.261671
71.513644	2510.460029	21.266688
71.770012	2512.600718	21.271706
71.447518	2511.486598	21.276723
71.761329	2503.253542	21.281741
71.803441	2510.935254	21.286759
71.878999	2514.562406	21.291776
72.461335	2519.419957	21.296794
72.156198	2532.748757	21.301811
72.245472	2527.325116	21.306829
72.245050	2523.468349	21.311847
72.255427	2531.997730	21.316864
72.187317	2536.562677	21.321882
72.525031	2522.843654	21.326899
72.655883	2519.114659	21.331917
72.421529	2525.741357	21.336935
72.739250	2523.368627	21.341952
72.561239	2528.020225	21.346970
72.599986	2523.197856	21.351987
72.715134	2536.555495	21.357005
72.843338	2545.388348	21.362023
72.770598	2543.184101	21.367040
72.880944	2547.979894	21.372058
72.796925	2546.531731	21.377075
73.513008	2553.631289	21.382093
73.367225	2564.997276	21.387111
73.458851	2571.326738	21.392128
73.843530	2568.839360	21.397146
73.590881	2580.206318	21.402163
73.888700	2569.125737	21.407181
73.825927	2575.839192	21.412199
73.653799	2574.493204	21.417216
73.996872	2574.641413	21.422234
73.595350	2577.904620	21.427251
74.085732	2570.047857	21.432269
73.934868	2569.134085	21.437287
73.852942	2582.093399	21.442304
74.125906	2571.351263	21.447322
74.079062	2584.892126	21.452339
74.288932	2589.198915	21.457357
74.361116	2593.805018	21.462375
74.498482	2596.071671	21.467392
74.466669	2596.007187	21.472410
74.640200	2592.842753	21.477427
74.754577	2587.869646	21.482445
74.708111	2614.331748	21.487463
74.719103	2620.989476	21.492480
74.950292	2618.352551	21.497498
75.049271	2612.116232	21.502515
75.129286	2611.747017	21.507533
75.119064	2614.453408	21.512551
75.346158	2618.296707	21.517568
75.440280	2613.651851	21.522586
74.956223	2621.892626	21.527603
75.876987	2634.931594	21.532621
75.999995	2642.405006	21.537639
75.849187	2650.994415	21.542656
76.098185	2639.672103	21.547674
75.900958	2645.346181	21.552691
75.712229	2640.010248	21.557709
75.850039	2640.963876	21.562727
75.868105	2641.595400	21.567744
75.957787	2631.083938	21.572762
75.592097	2640.900036	21.577779
76.143004	2652.428353	21.582797
76.406689	2656.190180	21.587815
76.484256	2657.939131	21.592832
76.869703	2657.133854	21.597850
76.505225	2658.538606	21.602867
76.587259	2657.124385	21.607885
76.487149	2662.849532	21.612903
76.583352	2655.111300	21.617920
76.883618	2653.467206	21.622938
76.541883	2660.041341	21.627955
76.678677	2680.768490	21.632973
76.980500	2683.063043	21.637991
76.881574	2690.905800	21.643008
77.198752	2685.146569	21.648026
77.306892	2680.894019	21.653043
77.210937	2681.941085	21.658061
77.098289	2691.367231	21.663079
77.627614	2706.099317	21.668096
77.727953	2699.922722	21.673114
77.372966	2707.562580	21.678131
77.633003	2710.075146	21.683149
77.572342	2713.417533	21.688167
77.922339	2703.578538	21.693184
78.000018	2699.974615	21.698202
77.725705	2726.232710	21.703219
78.033245	2720.516008	21.708237
78.257588	2731.792548	21.713255
78.102891	2736.828757	21.718272
78.391400	2726.642736	21.723290
78.603518	2735.866526	21.728307
78.597499	2726.105391	21.733325
78.339526	2727.162063	21.738343
78.484372	2742.260566	21.743360
78.915154	2743.127268	21.748378
79.001762	2749.880507	21.753395
78.784900	2742.453250	21.758413
79.005552	2745.511699	21.763431
79.031319	2749.336070	21.768448
79.411512	2740.454959	21.773466
78.957807	2739.910555	21.778483
79.091577	2745.100409	21.783501
79.486979	2753.250798	21.788519
79.250299	2767.077191	21.793536
79.574983	2757.213727	21.798554
79.883095	2767.031636	21.803571
79.716301	2771.037678	21.808589
79.843680	2759.301950	21.813607
79.688685	2761.724896	21.818624
79.885630	2766.030597	21.823642
80.156830	2782.772644	21.828659
79.817234	2789.759951	21.833677
80.217461	2788.049685	21.838695
80.024639	2793.025601	21.843712
80.404142	2787.878341	21.848730
80.306349	2791.529553	21.853747
80.535487	2789.161200	21.858765
80.712567	2800.069603	21.863783
80.730164	2811.473270	21.868800
81.025241	2814.876719	21.873818
80.948310	2816.558363	21.878835
81.126208	2818.992285	21.883853
81.361600	2808.606231	21.888871
80.968903	2811.928065	21.893888
81.055896	2818.125780	21.898906
81.266896	2806.509480	21.903923
81.265913	2802.706396	21.908941
81.549372	2805.193213	21.913959
81.147606	2814.469037	21.918976
81.464852	2819.276674	21.923994
81.360732	2835.793516	21.929011
81.339113	2837.567494	21.934029
81.886035	2837.649050	21.939047
81.613588	2837.720108	21.944064
81.774839	2850.152305	21.949082
82.073543	2856.136961	21.954099
82.259786	2858.127713	21.959117
82.511195	2849.266726	21.964135
82.597160	2863.721224	21.969152
82.660557	2849.571502	21.974170
82.471429	2844.592221	21.979187
82.478602	2852.689858	21.984205
82.525603	2855.728189	21.989223
82.288726	2857.971448	21.994240
82.424996	2871.206092	21.999258
82.844270	2884.207033	22.004275
82.824777	2880.018621	22.009293
82.863871	2880.918292	22.014311
82.917895	2882.093369	22.019328
82.896827	2882.125042	22.024346
83.272386	2889.792548	22.029363
83.109768	2903.395975	22.034381
83.750491	2897.352427	22.039399
83.437076	2907.536067	22.044416
83.477714	2907.270858	22.049434
83.731391	2898.794548	22.054451
83.614202	2901.691332	22.059469
83.686269	2907.607359	22.064487
83.832187	2919.287673	22.069504
84.270515	2927.317793	22.074522
84.374214	2929.176300	22.079539
84.449712	2929.085533	22.084557
84.534006	2926.149644	22.089575
84.757180	2921.399272	22.094592
84.463894	2919.750306	22.099610
84.471150	2919.989008	22.104627
84.123051	2918.317067	22.109645
84.761123	2915.231294	22.114663
84.238796	2923.658105	22.119680
84.724385	2936.345699	22.124698
84.890458	2947.259072	22.129715
84.766033	2951.375295	22.134733
85.108548	2942.421083	22.139751
85.034952	2948.543005	22.144768
85.337627	2958.352402	22.149786
85.543250	2967.971855	22.154803
85.475363	2966.950376	22.159821
85.805106	2968.151698	22.164839
85.724097	2970.077023	22.169856
85.495831	2966.846070	22.174874
85.792247	2966.089448	22.179891
86.120335	2970.175810	22.184909
86.251161	2960.531982	22.189927
85.869313	2960.945270	22.194944
85.858079	2980.850091	22.199962
86.307811	2989.165667	22.204979
86.297051	2994.655985	22.209997
86.704657	2988.046092	22.215015
86.659333	2986.998983	22.220032
86.618064	2987.889156	22.225050
86.952428	2999.943995	22.230067
86.615518	2990.206153	22.235085
87.030873	2983.276270	22.240103
87.178814	2991.345602	22.245120
86.873997	2994.581107	22.250138
87.469337	3010.076375	22.255155
87.433777	3016.646856	22.260173
87.733085	3009.899268	22.265191
87.516459	3008.819028	22.270208
87.273532	3008.828649	22.275226
87.642532	3007.615626	22.280243
87.354096	3012.076338	22.285261
87.693563	3003.453977	22.290279
87.517256	3016.213767	22.295296
87.958336	3019.610161	22.300314
87.747013	3024.169262	22.305331
87.677499	3038.155889	22.310349
87.813652	3024.272379	22.315367
87.799188	3036.104146	22.320384
88.057936	3048.489643	22.325402
88.020665	3049.290819	22.330419
88.235027	3060.676442	22.335437
88.419075	3050.181513	22.340455
88.548772	3071.014379	22.345472
88.758977	3078.957214	22.350490
89.081991	3085.506261	22.355507
88.740959	3090.631729	22.360525
89.039808	3078.177713	22.365543
89.662129	3087.605696	22.370560
89.223282	3085.294617	22.375578
89.062058	3084.770658	22.380595
89.228469	3084.331086	22.385613
89.262618	3081.014812	22.390631
89.189259	3092.003659	22.395648
89.338144	3106.309619	22.400666
89.523209	3110.456296	22.405683
89.609922	3109.741992	22.410701
89.717811	3100.663494	22.415719
89.826719	3119.896304	22.420736
89.991627	3126.312324	22.425754
89.891127	3137.289670	22.430771
89.882187	3139.781314	22.435789
90.338611	3132.380972	22.440807
90.833685	3150.495972	22.445824
90.584170	3153.413528	22.450842
90.980247	3152.354066	22.455859
90.780973	3159.524686	22.460877
90.888087	3151.355283	22.465895
90.951825	3143.795522	22.470912
90.952994	3149.154612	22.475930
91.156723	3148.254692	22.480947
91.193244	3155.584055	22.485965
91.196331	3144.495643	22.490983
91.027363	3154.540009	22.496000
90.981466	3170.669287	22.501018
91.558483	3177.093352	22.506035
91.394336	3173.432535	22.511053
91.308646	3172.745239	22.516071
91.548108	3187.374791	22.521088
91.737586	3189.327199	22.526106
91.958064	3197.252696	22.531123
91.862690	3194.556383	22.536141
91.775093	3204.736372	22.541159
92.007320	3218.233987	22.546176
92.295514	3218.551771	22.551194
92.550492	3216.046752	22.556211
92.740126	3215.123787	22.561229
92.870943	3215.125352	22.566247
92.492326	3224.012694	22.571264
92.516040	3231.094749	22.576282
93.431412	3231.361616	22.581299
93.027069	3237.406048	22.586317
93.413761	3242.300762	22.591335
93.365436	3236.563903	22.596352
93.617699	3234.362307	22.601370
93.660551	3237.155165	22.606387
93.044390	3241.891372	22.611405
93.633781	3230.420674	22.616423
93.919710	3252.586464	22.621440
93.765924	3263.256609	22.626458
94.114535	3263.517584	22.631475
94.057668	3272.726980	22.636493
94.312401	3260.030406	22.641511
94.112398	3268.653065	22.646528
94.406942	3267.820975	22.651546
94.338464	3260.493350	22.656563
94.372717	3259.964010	22.661581
94.292485	3257.549378	22.666599
94.514011	3265.522085	22.671616
94.473944	3277.897744	22.676634
94.623620	3281.866941	22.681651
94.852936	3293.711183	22.686669
94.675341	3281.031829	22.691687
95.112573	3285.745042	22.696704
94.785601	3290.729488	22.701722
94.829863	3293.695728	22.706739
95.455201	3301.614653	22.711757
95.574285	3304.566016	22.716775
95.597349	3307.390391	22.721792
95.628402	3317.536073	22.726810
95.490225	3310.238286	22.731827
95.275408	3322.622415	22.736845
95.397556	3329.919496	22.741863
95.737858	3333.978778	22.746880
95.447396	3333.487684	22.751898
96.051632	3348.132812	22.756915
96.382147	3364.499978	22.761933
96.369277	3355.613868	22.766951
96.378756	3360.170022	22.771968
96.673783	3363.081204	22.776986
96.884430	3364.815687	22.782003
96.897816	3367.758370	22.787021
96.922988	3373.849180	22.792039
97.003205	3367.536633	22.797056
96.809931	3371.032481	22.802074
97.260570	3368.821884	22.807091
96.941435	3374.370100	22.812109
96.894864	3381.157066	22.817127
97.719001	3392.074921	22.822144
97.549992	3393.427009	22.827162
97.634931	3395.411599	22.832179
97.669763	3399.496660	22.837197
98.005913	3403.745986	22.842215
98.315627	3387.975950	22.847232
98.199274	3392.602327	22.852250
98.476781	3406.831561	22.857267
98.460068	3415.037350	22.862285
98.187865	3420.130033	22.867303
98.658324	3428.306846	22.872320
98.511956	3425.627956	22.877338
98.434484	3414.697189	22.882355
98.445365	3416.024251	22.887373
98.770701	3411.977379	22.892391
98.778942	3432.905442	22.897408
98.667046	3443.367127	22.902426
98.819244	3440.802429	22.907443
99.149048	3450.263807	22.912461
99.105462	3463.691192	22.917479
99.384396	3455.617828	22.922496
99.475879	3473.588069	22.927514
99.494412	3462.389728	22.932531
99.515791	3473.288213	22.937549
99.694421	3486.049538	22.942567
100.314871	3477.698561	22.947584
100.150796	3494.613624	22.952602
100.149528	3489.456384	22.957619
100.362843	3486.077247	22.962637
100.399806	3491.244608	22.967655
100.034135	3486.823067	22.972672
100.396329	3502.052282	22.977690
100.721265	3506.079291	22.982707
100.834390	3508.769647	22.987725
100.784858	3506.940402	22.992743
100.915900	3501.159575	22.997760
100.994962	3506.992638	23.002778
101.218485	3506.499920	23.007795
101.483774	3518.881560	23.012813
101.500501	3533.738825	23.017831
101.380124	3534.439415	23.022848
101.537558	3537.653095	23.027866
101.735602	3525.271379	23.032883
101.845411	3534.382199	23.037901
102.041706	3532.981572	23.042919
102.155075	3527.705359	23.047936
102.305788	3531.109470	23.052954
102.254297	3533.838246	23.057971
102.356756	3534.989996	23.062989
102.104925	3527.331169	23.068007
102.266349	3527.482599	23.073024
102.324284	3547.355113	23.078042
102.224589	3556.069508	23.083059
102.712344	3548.698809	23.088077
102.231388	3556.371383	23.093095
102.294759	3571.997826	23.098112
102.889540	3577.592297	23.103130
103.090974	3582.377252	23.108147
103.150995	3578.839047	23.113165
103.136742	3597.514055	23.118183
103.426236	3607.448968	23.123200
103.255874	3605.083130	23.128218
103.324312	3606.088712	23.133235
103.125855	3619.723542	23.138253
103.647261	3632.484925	23.143271
104.094745	3634.052920	23.148288
104.159047	3638.840436	23.153306
104.123238	3635.001601	23.158323
104.244799	3641.560319	23.163341
104.312337	3657.618600	23.168359
104.348026	3647.594770	23.173376
104.635701	3664.164613	23.178394
105.183101	3660.218619	23.183411
105.030655	3657.717401	23.188429
104.673008	3653.474473	23.193447
105.132260	3662.934621	23.198464
105.408362	3685.765313	23.203482
105.098302	3679.122417	23.208499
105.344980	3673.585395	23.213517
104.996035	3679.299346	23.218535
105.228300	3677.792070	23.223552
105.235164	3706.390569	23.228570
105.361006	3708.450851	23.233587
105.503952	3712.856774	23.238605
105.915733	3724.915751	23.243623
106.246729	3724.538756	23.248640
106.407057	3729.238656	23.253658
106.461385	3733.882568	23.258675
106.926036	3731.698141	23.263693
106.843945	3725.723377	23.268711
106.770531	3720.776225	23.273728
106.409054	3727.180238	23.278746
106.955085	3733.464168	23.283763
107.412347	3740.929856	23.288781
107.431890	3745.026860	23.293799
107.601638	3740.297270	23.298816
107.653995	3750.165255	23.303834
107.584425	3742.875482	23.308851
107.791759	3743.565770	23.313869
107.501609	3741.771042	23.318887
107.899227	3739.196259	23.323904
107.821370	3737.791223	23.328922
108.041057	3728.739084	23.333939
108.065553	3737.254197	23.338957
107.906388	3734.930777	23.343975
108.453323	3743.263039	23.348992
108.394033	3749.401928	23.354010
108.211000	3752.274443	23.359027
108.395219	3754.303489	23.364045
108.563623	3767.012958	23.369063
108.416512	3754.047579	23.374080
108.408114	3768.066226	23.379098
108.840418	3786.763001	23.384115
109.150546	3781.528484	23.389133
108.914673	3791.744659	23.394151
109.071607	3781.007361	23.399168
108.973233	3794.127938	23.404186
109.238603	3811.285338	23.409203
109.494383	3809.786992	23.414221
109.353789	3818.845652	23.419239
109.734882	3831.158861	23.424256
109.377771	3841.217302	23.429274
109.681840	3843.186549	23.434291
109.897700	3846.495290	23.439309
109.693602	3867.125703	23.444327
110.089031	3867.868593	23.449344
110.074295	3872.330822	23.454362
110.216860	3882.850741	23.459379
110.792532	3881.182330	23.464397
110.413299	3882.251751	23.469415
111.008605	3888.771056	23.474432
111.260251	3908.373733	23.479450
111.142203	3906.968667	23.484467
111.575463	3913.718534	23.489485
111.364797	3919.047912	23.494503
111.660992	3922.233608	23.499520
111.836978	3917.007444	23.504538
111.698261	3915.040624	23.509555
112.063621	3909.658537	23.514573
111.910584	3919.015895	23.519591
111.937173	3923.560042	23.524608
111.962196	3928.884061	23.529626
112.053281	3929.065453	23.534643
112.013251	3933.878862	23.539661
112.165667	3956.767152	23.544679
112.230660	3958.682332	23.549696
112.735364	3954.660899	23.554714
112.668126	3958.096080	23.559731
113.020291	3978.039756	23.564749
112.814855	3994.283140	23.569767
113.212669	3985.995221	23.574784
112.991554	3989.558677	23.579802
113.623025	4000.084133	23.584819
113.517943	4014.645236	23.589837
113.813174	4013.781442	23.594855
114.283058	4000.738160	23.599872
114.199900	4001.379278	23.604890
114.224636	4012.195495	23.609907
114.128809	4008.886789	23.614925
114.268449	4009.016385	23.619943
114.257091	4007.149545	23.624960
114.282330	4011.615015	23.629978
114.439436	4028.546540	23.634995
114.519629	4028.281431	23.640013
114.620720	4034.748806	23.645031
114.624397	4037.658398	23.650048
115.131331	4058.906761	23.655066
114.925689	4065.295946	23.660083
115.364372	4057.156256	23.665101
115.116980	4051.699681	23.670119
115.493160	4056.760400	23.675136
115.974839	4072.085007	23.680154
116.042469	4092.458469	23.685171
115.885244	4077.048225	23.690189
115.639623	4080.662884	23.695207
115.659963	4087.657424	23.700224
116.251621	4089.748931	23.705242
116.058748	4082.143760	23.710259
116.199725	4085.802013	23.715277
116.101359	4098.471442	23.720295
116.388059	4108.691147	23.725312
116.727409	4101.690682	23.730330
116.363964	4109.641779	23.735347
117.088937	4117.892663	23.740365
116.739975	4126.163453	23.745383
116.726345	4127.342899	23.750400
117.213899	4119.167116	23.755418
116.890087	4136.994756	23.760435
117.148643	4151.985087	23.765453
117.115637	4158.782845	23.770471
117.611673	4168.275373	23.775488
117.612687	4171.595739	23.780506
117.895949	4182.709292	23.785523
118.429538	4180.596079	23.790541
118.062004	4182.392818	23.795559
118.333363	4194.227909	23.800576
118.573453	4211.522219	23.805594
118.444342	4208.717407	23.810611
118.642923	4204.062091	23.815629
118.580137	4216.972230	23.820647
119.249804	4226.822671	23.825664
118.998896	4217.487340	23.830682
119.031586	4222.444098	23.835699
119.672073	4215.405880	23.840717
119.294919	4222.970933	23.845735
119.415885	4227.961209	23.850752
120.006259	4241.409791	23.855770
119.569898	4251.730232	23.860787
119.818046	4258.042077	23.865805
119.893037	4259.207647	23.870823
120.201167	4268.909585	23.875840
120.281901	4270.345710	23.880858
120.058370	4279.581728	23.885875
120.308731	4279.542470	23.890893
120.406802	4285.429623	23.895911
120.765032	4299.047188	23.900928
121.159798	4303.085532	23.905946
121.094713	4301.994095	23.910963
121.025780	4294.274724	23.915981
121.419236	4296.018535	23.920999
121.022286	4309.391431	23.926016
121.362952	4323.933450	23.931034
121.317866	4325.171497	23.936051
121.689123	4327.060829	23.941069
121.385572	4333.001450	23.946087
121.945806	4342.607114	23.951104
122.071677	4334.582594	23.956122
121.912920	4351.942681	23.961139
122.541869	4353.678012	23.966157
122.580715	4366.206185	23.971175
122.575346	4370.105220	23.976192
123.191775	4369.090081	23.981210
122.744069	4366.597145	23.986227
123.129656	4365.914880	23.991245
122.804061	4374.677685	23.996263
122.961297	4386.874835	24.001280
123.452204	4389.768123	24.006298
123.818203	4397.478805	24.011315
123.455725	4389.357164	24.016333
123.640818	4391.805956	24.021351
123.705240	4407.912737	24.026368
124.258434	4412.585986	24.031386
124.185051	4414.832228	24.036403
124.247540	4413.853369	24.041421
124.491647	4413.508915	24.046439
124.460329	4417.355209	24.051456
124.687124	4406.950651	24.056474
124.580096	4414.489245	24.061491
124.769740	4412.540368	24.066509
124.864428	4429.901857	24.071527
125.090250	4443.679161	24.076544
125.319224	4434.050739	24.081562
124.922579	4443.162450	24.086579
125.130826	4437.574401	24.091597
125.303354	4450.618289	24.096615
125.259712	4458.803517	24.101632
125.548327	4453.250219	24.106650
125.448870	4465.954796	24.111667
125.743860	4479.506650	24.116685
125.482179	4491.911544	24.121703
126.360385	4508.468555	24.126720
126.446972	4507.397535	24.131738
126.370610	4514.319008	24.136755
126.341085	4508.165300	24.141773
126.637993	4520.021853	24.146791
126.667048	4535.884926	24.151808
127.142995	4532.802193	24.156826
127.087651	4540.443219	24.161843
127.157094	4534.324501	24.166861
127.553659	4546.765191	24.171879
127.239756	4549.232208	24.176896
127.908735	4555.389844	24.181914
127.594816	4560.451501	24.186931
127.981031	4571.359774	24.191949
128.265857	4589.641732	24.196967
128.130033	4593.409741	24.201984
128.435010	4588.920735	24.207002
128.500058	4588.171890	24.212019
128.368650	4590.162099	24.217037
128.511397	4599.703891	24.222055
128.727159	4615.866059	24.227072
129.088299	4613.861885	24.232090
129.553499	4617.317938	24.237107
129.428540	4612.179758	24.242125
129.383041	4623.862755	24.247143
129.370184	4637.819642	24.252160
129.623347	4634.983283	24.257178
129.367607	4635.496791	24.262195
129.676778	4646.139407	24.267213
130.163887	4665.002112	24.272231
130.097445	4667.259924	24.277248
130.152587	4666.013899	24.282266
130.279216	4677.010252	24.287283
130.446742	4685.957940	24.292301
130.335393	4686.524585	24.297319
130.544607	4683.717199	24.302336
131.020221	4694.573662	24.307354
131.157176	4710.574652	24.312371
131.240123	4716.574792	24.317389
131.656849	4718.643278	24.322407
131.347446	4714.660843	24.327424
131.754986	4712.652546	24.332442
131.504143	4720.684118	24.337459
131.494450	4739.643673	24.342477
131.786755	4735.709008	24.347495
131.683330	4749.503405	24.352512
132.187850	4750.443887	24.357530
132.498751	4761.913310	24.362547
132.668252	4773.114492	24.367565
132.700740	4764.157454	24.372583
132.448047	4758.995053	24.377600
132.879630	4771.976491	24.382618
133.162647	4782.986285	24.387635
133.357838	4785.569279	24.392653
133.329114	4785.507459	24.397671
133.517561	4787.681161	24.402688
133.814339	4784.856885	24.407706
133.536088	4784.625826	24.412723
133.800614	4794.565304	24.417741
133.882861	4806.029543	24.422759
133.668761	4812.619176	24.427776
133.646318	4811.113835	24.432794
133.887099	4821.293788	24.437811
134.113537	4834.288470	24.442829
134.131817	4839.850553	24.447847
134.179002	4856.443383	24.452864
134.771108	4860.536163	24.457882
134.822089	4862.270555	24.462899
134.460629	4876.017090	24.467917
135.277833	4885.096677	24.472935
135.249107	4889.315137	24.477952
135.660050	4896.766467	24.482970
135.815116	4900.498436	24.487987
135.867233	4904.877844	24.493005
135.793248	4902.973375	24.498023
135.545322	4915.209103	24.503040
135.983711	4918.868279	24.508058
136.062854	4931.841916	24.513075
136.099141	4933.244021	24.518093
136.549099	4946.481543	24.523111
137.017921	4956.840491	24.528128
137.151862	4965.623125	24.533146
137.226272	4959.626592	24.538163
137.287196	4954.730657	24.543181
137.410703	4969.414540	24.548199
137.394337	4979.057217	24.553216
137.584574	4982.363869	24.558234
137.628476	4989.490797	24.563251
137.822961	4998.626966	24.568269
138.144908	5003.204024	24.573287
138.120263	5015.079711	24.578304
138.221681	5012.153431	24.583322
137.977147	5019.521266	24.588339
138.452213	5028.092658	24.593357
139.176509	5032.950754	24.598375
138.779877	5038.129668	24.603392
138.893515	5037.489986	24.608410
139.262010	5046.254850	24.613427
139.043474	5051.869883	24.618445
139.003958	5058.852078	24.623463
139.285955	5067.431639	24.628480
139.812308	5079.694533	24.633498
139.654232	5084.119541	24.638515
139.579032	5091.700777	24.643533
140.283388	5096.038022	24.648551
140.438922	5103.115939	24.653568
140.541032	5108.642875	24.658586
140.725351	5108.825456	24.663603
140.376241	5113.457169	24.668621
140.807219	5122.767841	24.673639
140.569349	5138.824774	24.678656
141.057893	5138.625095	24.683674
141.440885	5142.352970	24.688691
141.397003	5154.430628	24.693709
141.719315	5159.998839	24.698727
141.782908	5175.213112	24.703744
141.798168	5163.723829	24.708762
141.810037	5165.644304	24.713779
141.877990	5174.061740	24.718797
142.708088	5179.013783	24.723815
142.110808	5183.728586	24.728832
142.410871	5182.696683	24.733850
142.499086	5193.566790	24.738867
142.404983	5191.911657	24.743885
143.007643	5205.523176	24.748903
142.842659	5206.013011	24.753920
142.925378	5208.844119	24.758938
142.632309	5223.258869	24.763955
142.823772	5239.516940	24.768973
143.662754	5236.544517	24.773991
143.650702	5259.794815	24.779008
144.099836	5266.163909	24.784026
144.146465	5258.006194	24.789043
144.120719	5267.164375	24.794061
144.242022	5263.388966	24.799079
144.443490	5283.373470	24.804096
144.606729	5293.651065	24.809114
144.376863	5297.111976	24.814131
144.289172	5312.564715	24.819149
144.527526	5316.293190	24.824167
144.747813	5321.306087	24.829184
144.950467	5338.919841	24.834202
145.153179	5340.384291	24.839219
145.152715	5354.784869	24.844237
145.489529	5362.794103	24.849255
145.949110	5369.871839	24.854272
146.318772	5376.973136	24.859290
146.544745	5390.501760	24.864307
146.294453	5401.882736	24.869325
146.981116	5395.045175	24.874343
146.653160	5398.824509	24.879360
146.787419	5400.997305	24.884378
147.091188	5410.744731	24.889395
147.211437	5414.640092	24.894413
147.185826	5414.120069	24.899431
147.177872	5414.635814	24.904448
147.638815	5433.752792	24.909466
147.779171	5440.410228	24.914483
147.750958	5442.529567	24.919501
147.691927	5438.504590	24.924519
148.075509	5456.901371	24.929536
148.303094	5462.506612	24.934554
148.946480	5466.547305	24.939571
148.496653	5464.111365	24.944589
148.707908	5468.380748	24.949607
149.082315	5484.177915	24.954624
149.299796	5499.302060	24.959642
149.238168	5494.270504	24.964659
149.043557	5494.562962	24.969677
149.259168	5504.873508	24.974695
149.757172	5512.099957	24.979712
149.708760	5514.418181	24.984730
149.929434	5525.510796	24.989747
149.929354	5538.288937	24.994765
150.259171	5543.631968	24.999783
150.269191	5543.264192	25.004800
150.480271	5560.504354	25.009818
151.229971	5566.605500	25.014835
150.556371	5573.589374	25.019853
151.188790	5570.927048	25.024871
150.935034	5578.318649	25.029888
151.060504	5585.032134	25.034906
151.357327	5593.290798	25.039923
151.438330	5593.789455	25.044941
151.665552	5606.115352	25.049959
152.032923	5620.815217	25.054976
152.162602	5617.830750	25.059994
152.147901	5611.525983	25.065011
152.206973	5619.111655	25.070029
152.357591	5628.558054	25.075047
152.288166	5638.263055	25.080064
152.433962	5641.532597	25.085082
153.168608	5651.885021	25.090099
152.974791	5659.346181	25.095117
153.188714	5663.207980	25.100135
153.176102	5664.699877	25.105152
153.481837	5681.653849	25.110170
153.621386	5689.722542	25.115187
153.709089	5697.777264	25.120205
154.025262	5692.787480	25.125223
154.165446	5706.856946	25.130240
154.140901	5718.316392	25.135258
154.561468	5715.583065	25.140275
154.234970	5730.107622	25.145293
154.749732	5729.288276	25.150311
155.161912	5738.842119	25.155328
154.958025	5750.402286	25.160346
155.443267	5744.265372	25.165363
155.411889	5747.366975	25.170381
155.316006	5763.799955	25.175399
155.514731	5769.624468	25.180416
156.097352	5771.439806	25.185434
156.096914	5783.864624	25.190451
156.041996	5795.770815	25.195469
156.235538	5790.579247	25.200487
156.115865	5797.072365	25.205504
156.422938	5811.361989	25.210522
156.504258	5822.350349	25.215539
156.503428	5830.639969	25.220557
157.054461	5843.890721	25.225575
157.157530	5847.946702	25.230592
157.281344	5866.747615	25.235610
157.653276	5872.990124	25.240627
157.506196	5884.045870	25.245645
157.886686	5884.503929	25.250663
157.912791	5906.066538	25.255680
158.078142	5904.661112	25.260698
158.283081	5907.043866	25.265715
158.299245	5918.124565	25.270733
158.731369	5920.522237	25.275751
158.674129	5926.380588	25.280768
158.663146	5951.342544	25.285786
159.408651	5954.780198	25.290803
159.518628	5959.135011	25.295821
159.392873	5953.197923	25.300839
159.426646	5975.674865	25.305856
159.539890	5985.897548	25.310874
160.292542	5985.097745	25.315891
160.246936	5999.546941	25.320909
160.195138	6014.192837	25.325927
160.605004	6013.430952	25.330944
160.375588	6011.247669	25.335962
160.859760	6023.745095	25.340979
161.090527	6036.275916	25.345997
161.295598	6033.481601	25.351015
161.407477	6026.765425	25.356032
161.269921	6044.426845	25.361050
161.596255	6049.290745	25.366067
161.367840	6056.009337	25.371085
161.669431	6077.001811	25.376103
161.944296	6078.745439	25.381120
161.838810	6086.366555	25.386138
162.128924	6093.322757	25.391155
162.210715	6096.318300	25.396173
162.744382	6106.058493	25.401191
162.918766	6119.311631	25.406208
162.981791	6131.398438	25.411226
163.524145	6127.405364	25.416243
163.385059	6137.004743	25.421261
163.523278	6132.778245	25.426279
163.844128	6146.052652	25.431296
163.724413	6156.255104	25.436314
164.254827	6155.831043	25.441331
163.647150	6162.599620	25.446349
163.902017	6175.691822	25.451367
164.577884	6182.874891	25.456384
164.444228	6188.884195	25.461402
164.647888	6191.273501	25.466419
164.807053	6208.879124	25.471437
164.837157	6206.408932	25.476455
165.225282	6219.426624	25.481472
165.239787	6240.028625	25.486490
165.008914	6234.761368	25.491507
165.523344	6250.275249	25.496525
165.857110	6255.257998	25.501543
165.824302	6263.783269	25.506560
165.964858	6279.264201	25.511578
166.292465	6277.321927	25.516595
166.411526	6297.730833	25.521613
166.784117	6316.161770	25.526631
167.020638	6316.557164	25.531648
167.291957	6326.262812	25.536666
167.660756	6337.099111	25.541683
167.469714	6346.681484	25.546701
167.780778	6346.181296	25.551719
168.053575	6337.750907	25.556736
167.819689	6357.107137	25.561754
168.007093	6358.229978	25.566771
167.871655	6367.582674	25.571789
168.279900	6389.341685	25.576807
168.659703	6394.213085	25.581824
168.450870	6407.940011	25.586842
168.844438	6422.488048	25.591859
169.120351	6419.376366	25.596877
169.304649	6423.078814	25.601895
169.509158	6447.089052	25.606912
169.508681	6458.523092	25.611930
169.806243	6450.821155	25.616947
169.507781	6464.177032	25.621965
169.963769	6473.853827	25.626983
170.355413	6480.497530	25.632000
170.417848	6499.971642	25.637018
170.653137	6504.123858	25.642035
170.810799	6514.055762	25.647053
171.078990	6526.180138	25.652071
171.381227	6531.584604	25.657088
171.193030	6540.601559	25.662106
171.650276	6545.205164	25.667123
171.808725	6550.142853	25.672141
171.708153	6548.138201	25.677159
172.212482	6562.293334	25.682176
172.527058	6576.383500	25.687194
172.784932	6579.209478	25.692212
173.019334	6581.505628	25.697229
172.936132	6569.993006	25.702247
173.129727	6589.538214	25.707264
172.828948	6598.749618	25.712282
173.331529	6596.306372	25.717300
173.622726	6607.761104	25.722317
173.711695	6625.491771	25.727335
173.893145	6621.855033	25.732352
173.598796	6627.826518	25.737370
173.905309	6633.242972	25.742388
174.397598	6653.098177	25.747405
174.336295	6654.885057	25.752423
174.519803	6654.616353	25.757440
174.478056	6668.184709	25.762458
174.856242	6684.654733	25.767476
175.039563	6690.320955	25.772493
175.069658	6705.194493	25.777511
175.334031	6699.732710	25.782528
175.556788	6714.418230	25.787546
175.848482	6732.584456	25.792564
175.830037	6736.546024	25.797581
175.486902	6739.362007	25.802599
175.978176	6761.256825	25.807616
175.848421	6767.360413	25.812634
176.410728	6785.121256	25.817652
176.379447	6795.294424	25.822669
176.763075	6811.365943	25.827687
177.031738	6813.580990	25.832704
177.256670	6824.777904	25.837722
177.584695	6842.354524	25.842740
177.598136	6841.136984	25.847757
177.751084	6862.219939	25.852775
177.687382	6862.599242	25.857792
178.133780	6879.093480	25.862810
178.446155	6892.688603	25.867828
178.527982	6892.205373	25.872845
178.619561	6915.201611	25.877863
179.206050	6919.472530	25.882880
179.554949	6931.237272	25.887898
179.630178	6920.640366	25.892916
179.715077	6933.687130	25.897933
179.780686	6958.155449	25.902951
179.861130	6955.948764	25.907968
180.034093	6960.527559	25.912986
180.162174	6969.331015	25.918004
180.804631	6971.383344	25.923021
180.581547	6984.929831	25.928039
181.025050	6988.408685	25.933056
181.150025	7000.858876	25.938074
181.098284	6996.775589	25.943092
181.266518	7009.320030	25.948109
180.949729	7024.863768	25.953127
181.722458	7031.984647	25.958144
182.160835	7045.721146	25.963162
182.168797	7052.895547	25.968180
182.744633	7063.526213	25.973197
182.367900	7072.781321	25.978215
182.811509	7080.761952	25.983232
183.040046	7087.541922	25.988250
183.259113	7098.506309	25.993268
183.438338	7106.821966	25.998285
183.304573	7115.376076	26.003303
183.435895	7117.060213	26.008320
183.230669	7128.245778	26.013338
183.742610	7139.214819	26.018356
183.927101	7153.679385	26.023373
183.933533	7165.838878	26.028391
184.549683	7177.331453	26.033408
184.664613	7187.421950	26.038426
184.627820	7194.287724	26.043444
184.882360	7210.442955	26.048461
185.227545	7227.944646	26.053479
185.503036	7230.430172	26.058496
185.572106	7244.559314	26.063514
185.563583	7245.782357	26.068532
185.829750	7254.299133	26.073549
185.938291	7276.526024	26.078567
186.064254	7279.950501	26.083584
186.182151	7276.623503	26.088602
186.864306	7295.559397	26.093620
186.922667	7304.588610	26.098637
187.081579	7305.204545	26.103655
187.149318	7316.650530	26.108672
187.754841	7320.549198	26.113690
187.535736	7321.202256	26.118708
187.705327	7333.822472	26.123725
187.739103	7349.251581	26.128743
188.330513	7344.593914	26.133760
188.205726	7364.483422	26.138778
188.543657	7371.912482	26.143796
188.259037	7382.119348	26.148813
188.412819	7400.269956	26.153831
188.817357	7407.505490	26.158848
188.983793	7423.658926	26.163866
189.233366	7431.155520	26.168884
189.554299	7447.133238	26.173901
189.644621	7456.615282	26.178919
189.946769	7468.248784	26.183936
190.195060	7481.945935	26.188954
190.169922	7484.106068	26.193972
190.318906	7503.728690	26.198989
190.658601	7509.345411	26.204007
190.912650	7519.016513	26.209024
190.980487	7531.766458	26.214042
191.219868	7545.322987	26.219060
191.319498	7557.363957	26.224077
191.395552	7576.991768	26.229095
191.854583	7585.396401	26.234112
192.210153	7593.488916	26.239130
192.353192	7612.171795	26.244148
192.910866	7614.278523	26.249165
192.870473	7626.628763	26.254183
192.896043	7637.513289	26.259200
192.829703	7643.158934	26.264218
193.035232	7655.773741	26.269236
193.803544	7659.637509	26.274253
193.560316	7677.938984	26.279271
193.916276	7682.265142	26.284288
194.031474	7695.680228	26.289306
194.371457	7707.579460	26.294324
195.034187	7715.807017	26.299341
194.634714	7727.291723	26.304359
194.643552	7733.999011	26.309376
194.986341	7749.698905	26.314394
195.183560	7762.469782	26.319412
195.398492	7763.342149	26.324429
195.584103	7782.646782	26.329447
195.954615	7784.609214	26.334464
196.012739	7807.807543	26.339482
196.000551	7816.573396	26.344500
196.677568	7811.851690	26.349517
196.966636	7832.128325	26.354535
196.828974	7837.977783	26.359552
197.396650	7844.701746	26.364570
197.365963	7853.252676	26.369588
197.296921	7855.315548	26.374605
197.180534	7868.874380	26.379623
197.673346	7888.449861	26.384640
198.054318	7897.517221	26.389658
197.954874	7921.460189	26.394676
198.454660	7912.122173	26.399693
198.316829	7933.062483	26.404711
199.036434	7946.695615	26.409728
199.104257	7944.724413	26.414746
199.116347	7966.743094	26.419764
199.421130	7973.135754	26.424781
199.702824	7979.724615	26.429799
200.020814	7994.781402	26.434816
200.224969	7998.825180	26.439834
200.125647	8004.984392	26.444852
200.639901	8006.286599	26.449869
200.017742	8014.409345	26.454887
200.667533	8029.306839	26.459904
200.816222	8044.617500	26.464922
200.926894	8057.042230	26.469940
200.998123	8066.224497	26.474957
201.138922	8083.626423	26.479975
201.603476	8094.079381	26.484992
201.665427	8113.050137	26.490010
201.880585	8123.750551	26.495028
202.041429	8135.712852	26.500045
202.178168	8148.405072	26.505063
202.325779	8166.301674	26.510080
202.625874	8177.162454	26.515098
202.480021	8198.956742	26.520116
203.187727	8218.240024	26.525133
203.653455	8230.419821	26.530151
203.988984	8229.874713	26.535168
204.234542	8252.927423	26.540186
204.316740	8257.498662	26.545204
204.532292	8255.226457	26.550221
204.902557	8260.927019	26.555239
204.874384	8274.712270	26.560256
205.169103	8278.795594	26.565274
205.114079	8300.297944	26.570292
205.376743	8308.818914	26.575309
205.422239	8312.578218	26.580327
205.710458	8324.744843	26.585344
206.088450	8340.875411	26.590362
206.232420	8355.366211	26.595380
206.385699	8360.223111	26.600397
206.463591	8381.748933	26.605415
206.820253	8384.506045	26.610432
207.104186	8396.262960	26.615450
207.389311	8408.846869	26.620468
207.204796	8428.822649	26.625485
207.476430	8436.092039	26.630503
207.798867	8454.687679	26.635520
207.829690	8467.475639	26.640538
208.187117	8491.164654	26.645556
208.774871	8500.578777	26.650573
208.570308	8497.336807	26.655591
209.098799	8513.204003	26.660608
209.285755	8527.280928	26.665626
209.602615	8543.348635	26.670644
209.707884	8548.623539	26.675661
210.009977	8557.864598	26.680679
210.162938	8571.703780	26.685696
210.639777	8572.819303	26.690714
210.383997	8585.169195	26.695732
210.823336	8592.627062	26.700749
210.991839	8607.253132	26.705767
210.892769	8617.816785	26.710784
211.447404	8626.753112	26.715802
211.545455	8638.981308	26.720820
211.559132	8653.764272	26.725837
211.986740	8667.579443	26.730855
211.979178	8680.780842	26.735872
212.290529	8688.195655	26.740890
212.282173	8692.718043	26.745908
212.722112	8706.256634	26.750925
212.926265	8719.529082	26.755943
213.413434	8735.289284	26.760960
213.437246	8738.786865	26.765978
213.528857	8758.763943	26.770996
213.689025	8769.959557	26.776013
213.843045	8780.619414	26.781031
213.913917	8787.532056	26.786048
214.167797	8802.094389	26.791066
214.297008	8812.963370	26.796084
214.614023	8823.818723	26.801101
215.064690	8842.006325	26.806119
215.348075	8857.454418	26.811136
215.577383	8861.917515	26.816154
215.614887	8881.237025	26.821172
215.867599	8888.730564	26.826189
216.232559	8900.165696	26.831207
216.327061	8908.801690	26.836224
216.848607	8917.212926	26.841242
216.688405	8929.399682	26.846260
216.865918	8936.283044	26.851277
217.288907	8957.648126	26.856295
217.538962	8975.166378	26.861312
217.800988	8982.216481	26.866330
217.769068	8995.153553	26.871348
218.106650	8998.680960	26.876365
217.807583	9009.247751	26.881383
218.389017	9025.157610	26.886400
218.799305	9033.646317	26.891418
218.875523	9050.831945	26.896436
219.174183	9078.518541	26.901453
219.748410	9084.468404	26.906471
219.885305	9088.106200	26.911488
220.303622	9101.717928	26.916506
220.356951	9119.977522	26.921524
220.254575	9117.679244	26.926541
220.648376	9139.683720	26.931559
221.153983	9149.837220	26.936576
220.934093	9150.057914	26.941594
221.058466	9169.329385	26.946612
221.003224	9170.300977	26.951629
221.402752	9185.986888	26.956647
220.993508	9209.414895	26.961664
221.685156	9224.808808	26.966682
222.215701	9254.609456	26.971700
222.526103	9257.967520	26.976717
222.841891	9279.431856	26.981735
222.723220	9291.754421	26.986752
223.215688	9301.032332	26.991770
223.363949	9321.727321	26.996788
223.735500	9333.486891	27.001805
223.866776	9331.041478	27.006823
223.817597	9350.043537	27.011840
224.404702	9370.480393	27.016858
224.528618	9386.392775	27.021876
224.835918	9391.472089	27.026893
224.826620	9408.144172	27.031911
225.030137	9419.080801	27.036928
225.469494	9442.398261	27.041946
225.870046	9449.641539	27.046964
225.928556	9455.618639	27.051981
226.599039	9480.863801	27.056999
226.606164	9486.722667	27.062016
226.911802	9489.784730	27.067034
227.058359	9505.125347	27.072052
227.295060	9509.805299	27.077069
227.451768	9525.163285	27.082087
227.636645	9541.940835	27.087104
228.070750	9540.909805	27.092122
227.888125	9557.280811	27.097140
228.265490	9561.708253	27.102157
228.946913	9570.865136	27.107175
228.781100	9589.547874	27.112192
229.045166	9590.197933	27.117210
229.134950	9595.661845	27.122228
228.913729	9605.370606	27.127245
229.110993	9617.912269	27.132263
228.852829	9641.184539	27.137280
229.363396	9649.165271	27.142298
229.711992	9661.080199	27.147316
230.085779	9693.634073	27.152333
230.341283	9702.643043	27.157351
230.470778	9729.008909	27.162368
231.004979	9739.998117	27.167386
231.076354	9761.747574	27.172404
231.086845	9763.870816	27.177421
231.695762	9784.794106	27.182439
231.850089	9801.500898	27.187456
232.321854	9808.808939	27.192474
232.460982	9835.593380	27.197492
232.384797	9849.778836	27.202509
232.735089	9861.737831	27.207527
232.777507	9881.079710	27.212544
233.037264	9898.060553	27.217562
233.279578	9905.218290	27.222580
233.462731	9931.017175	27.227597
234.316561	9945.789531	27.232615
234.217992	9963.669598	27.237632
234.244676	9975.976158	27.242650
234.639344	9991.174112	27.247668
235.073037	10010.038050	27.252685
235.168404	10019.315381	27.257703
235.326528	10038.917151	27.262720
235.952917	10044.177150	27.267738
236.421641	10064.219691	27.272756
236.222342	10075.844981	27.277773
236.839961	10086.458221	27.282791
236.664917	10101.556068	27.287808
237.389877	10101.780311	27.292826
237.108349	10119.136636	27.297844
237.215616	10135.421687	27.302861
237.726492	10152.454989	27.307879
237.876834	10156.820258	27.312896
238.565245	10175.603414	27.317914
238.279673	10182.859741	27.322932
238.638316	10205.092008	27.327949
239.153627	10217.113789	27.332967
239.204342	10244.894638	27.337984
239.312172	10240.375168	27.343002
239.032370	10273.954423	27.348020
239.412466	10285.372251	27.353037
239.572039	10303.152211	27.358055
239.965983	10320.889156	27.363072
240.526565	10334.362676	27.368090
241.367737	10348.202722	27.373108
240.744056	10364.877181	27.378125
241.387559	10372.739518	27.383143
241.623276	10395.682758	27.388160
242.014040	10407.380007	27.393178
242.173366	10426.514687	27.398196
242.087982	10439.195905	27.403213
242.460453	10441.489858	27.408231
242.712677	10472.494858	27.413248
243.108730	10483.032522	27.418266
243.654931	10494.266582	27.423284
243.698887	10503.050164	27.428301
244.037914	10508.061665	27.433319
244.008427	10527.674393	27.438336
244.457891	10540.925499	27.443354
244.617671	10549.744636	27.448372
244.548330	10567.775419	27.453389
245.101049	10564.913340	27.458407
245.258451	10573.994935	27.463424
245.609490	10583.867156	27.468442
246.135753	10595.628550	27.473460
246.320694	10600.550543	27.478477
246.534301	10603.548271	27.483495
246.115673	10627.667861	27.488512
246.617026	10643.045401	27.493530
246.923103	10652.567901	27.498548
246.930289	10664.296982	27.503565
247.449965	10681.755657	27.508583
247.440334	10692.461191	27.513600
247.521317	10705.706988	27.518618
247.802761	10724.279745	27.523636
247.959533	10755.379105	27.528653
248.440947	10768.499065	27.533671
248.548698	10788.535783	27.538688
248.419983	10812.142874	27.543706
249.221999	10817.511357	27.548724
249.335815	10842.747686	27.553741
249.402019	10855.601208	27.558759
249.808510	10881.233800	27.563776
249.622754	10902.541756	27.568794
250.174494	10920.065097	27.573812
250.533578	10935.045207	27.578829
251.405738	10955.672810	27.583847
251.441467	10975.566288	27.588864
251.582756	10995.064339	27.593882
251.671728	11001.321346	27.598900
251.914667	11025.034678	27.603917
252.478574	11036.209455	27.608935
252.634249	11047.902885	27.613952
252.747447	11059.618764	27.618970
253.066815	11075.953504	27.623988
253.422225	11093.371988	27.629005
253.750985	11099.484104	27.634023
253.873533	11126.730844	27.639040
254.291102	11148.408734	27.644058
254.525654	11153.392569	27.649076
254.697449	11171.143020	27.654093
254.818219	11186.331175	27.659111
254.988626	11202.793563	27.664128
254.958018	11221.226239	27.669146
255.465495	11240.019866	27.674164
255.773646	11263.394891	27.679181
256.414818	11263.401775	27.684199
256.097482	11296.695078	27.689216
256.458774	11308.779583	27.694234
257.258324	11332.197705	27.699252
257.173355	11353.023050	27.704269
257.781697	11361.361806	27.709287
258.061567	11378.195591	27.714304
258.103950	11402.755495	27.719322
258.311487	11401.017814	27.724340
258.215066	11427.629868	27.729357
258.721896	11438.109669	27.734375
258.920137	11453.254327	27.739392
259.501110	11481.683362	27.744410
259.704675	11483.615513	27.749428
259.603816	11495.996731	27.754445
259.865496	11513.057682	27.759463
260.263043	11531.164660	27.764480
260.464807	11555.740845	27.769498
261.154038	11570.268719	27.774516
260.937655	11580.284036	27.779533
261.591059	11591.590380	27.784551
261.889673	11601.755545	27.789568
262.091338	11624.178288	27.794586
262.409520	11622.593770	27.799604
262.548872	11641.704400	27.804621
263.033798	11646.380740	27.809639
263.147348	11657.190677	27.814656
263.151898	11675.479351	27.819674
263.425282	11689.895630	27.824692
263.460113	11713.730849	27.829709
263.968747	11715.068950	27.834727
263.903399	11730.662468	27.839744
264.220393	11751.785265	27.844762
264.487513	11759.050348	27.849780
264.607831	11783.071200	27.854797
265.003682	11806.515263	27.859815
265.472363	11821.655746	27.864832
265.873565	11852.159713	27.869850
266.055450	11865.801026	27.874868
265.962258	11881.026418	27.879885
266.363168	11887.298008	27.884903
266.528439	11911.274088	27.889920
266.718506	11935.296838	27.894938
267.521356	11948.995666	27.899956
267.376681	11974.545574	27.904973
267.527342	11987.948720	27.909991
267.984602	12012.251803	27.915008
268.192475	12023.770302	27.920026
268.662545	12044.708402	27.925044
268.639006	12074.672975	27.930061
269.114472	12097.444955	27.935079
269.790865	12121.240185	27.940096
269.480258	12131.403180	27.945114
269.914052	12147.875660	27.950132
270.151199	12173.596542	27.955149
270.397143	12188.570115	27.960167
270.690183	12206.059399	27.965184
270.777138	12230.701816	27.970202
271.325391	12249.335336	27.975220
271.607050	12265.200190	27.980237
271.805926	12281.668535	27.985255
272.320267	12313.573381	27.990272
272.787049	12332.336585	27.995290
273.366211	12342.439255	28.000308
272.861102	12363.318899	28.005325
273.542279	12375.432927	28.010343
273.690249	12386.098946	28.015360
273.789927	12408.405971	28.020378
274.571318	12410.951896	28.025396
274.479822	12445.244454	28.030413
274.863904	12458.036643	28.035431
275.479193	12469.286333	28.040448
275.702345	12485.353166	28.045466
275.728411	12500.408798	28.050484
275.875065	12511.141408	28.055501
276.168077	12531.059382	28.060519
276.535205	12547.811072	28.065536
276.902846	12566.747932	28.070554
277.213940	12575.964312	28.075572
276.901665	12607.200208	28.080589
277.433734	12620.793527	28.085607
277.689582	12636.091163	28.090624
277.827848	12664.032394	28.095642
278.412770	12683.614276	28.100660
278.704484	12698.217928	28.105677
278.711650	12717.268250	28.110695
279.114005	12734.611427	28.115712
279.308615	12763.696606	28.120730
279.980627	12771.293389	28.125748
280.049005	12792.446825	28.130765
280.450380	12802.984963	28.135783
280.598095	12812.246000	28.140800
280.661373	12834.827650	28.145818
281.066184	12837.852628	28.150836
281.403821	12860.757648	28.155853
281.545438	12876.224953	28.160871
282.002653	12890.202825	28.165888
282.139197	12907.685696	28.170906
282.222286	12917.607438	28.175924
282.629092	12944.679643	28.180941
282.640703	12958.477895	28.185959
283.074012	12976.624873	28.190976
283.491464	13011.722948	28.195994
283.948085	13019.195677	28.201012
284.135202	13047.657196	28.206029
284.340303	13062.830494	28.211047
284.694859	13082.720461	28.216064
284.972967	13100.591866	28.221082
285.262632	13110.115027	28.226100
285.382185	13130.774501	28.231117
285.644947	13161.580170	28.236135
286.115916	13175.672944	28.241152
286.299486	13207.166896	28.246170
286.673482	13217.927454	28.251188
286.620128	13243.970042	28.256205
287.303471	13270.683597	28.261223
287.689853	13285.133922	28.266240
287.622349	13313.585199	28.271258
288.325800	13334.112372	28.276276
288.275162	13350.229146	28.281293
288.702281	13370.938598	28.286311
289.121157	13382.674353	28.291328
289.187785	13409.475239	28.296346
289.970136	13419.429814	28.301364
289.869008	13442.161104	28.306381
290.038028	13466.173306	28.311399
290.309867	13480.764886	28.316416
290.188714	13516.586185	28.321434
290.622254	13533.022018	28.326452
291.299240	13563.921354	28.331469
291.708445	13583.026412	28.336487
291.968426	13602.508564	28.341504
292.412853	13622.643977	28.346522
292.429845	13640.872599	28.351540
292.898893	13666.761297	28.356557
293.095940	13685.009126	28.361575
293.417567	13697.609824	28.366592
293.505357	13731.734509	28.371610
293.786923	13748.279603	28.376628
294.340940	13775.209928	28.381645
294.483341	13798.115084	28.386663
294.885512	13822.744932	28.391680
294.807540	13839.816978	28.396698
295.442812	13860.450146	28.401716
295.917837	13879.320969	28.406733
295.795212	13897.963308	28.411751
296.283381	13926.925332	28.416768
296.300055	13947.077568	28.421786
296.761116	13964.349514	28.426804
297.260072	13992.071978	28.431821
297.407073	14010.918522	28.436839
297.492659	14037.044648	28.441856
297.699352	14060.192696	28.446874
298.242723	14078.692987	28.451892
298.604758	14110.855263	28.456909
298.681956	14135.782755	28.461927
299.654695	14153.858993	28.466944
299.916034	14178.779804	28.471962
300.100497	14195.463665	28.476980
300.313916	14198.746231	28.481997
300.867969	14220.933679	28.487015
301.066942	14234.706665	28.492032
301.151037	14254.403367	28.497050
301.360347	14277.459683	28.502068
301.776977	14285.826617	28.507085
302.110541	14313.957594	28.512103
302.679228	14319.300486	28.517120
302.670570	14344.964917	28.522138
302.755637	14365.928001	28.527156
303.111478	14385.459102	28.532173
303.278474	14417.396638	28.537191
303.658626	14425.971470	28.542208
303.749639	14452.163636	28.547226
304.561644	14474.620473	28.552244
304.925803	14490.575329	28.557261
305.085963	14520.353917	28.562279
305.548331	14541.476004	28.567296
305.870982	14561.915726	28.572314
305.684760	14582.555195	28.577332
305.813972	14596.762568	28.582349
306.046425	14630.897783	28.587367
306.546106	14662.998372	28.592384
306.738134	14681.472174	28.597402
307.123944	14713.410668	28.602420
307.830712	14740.934284	28.607437
307.779142	14764.897407	28.612455
308.276967	14783.386570	28.617472
308.710511	14799.899296	28.622490
309.007305	14823.274181	28.627508
309.304224	14843.187653	28.632525
309.479530	14873.709761	28.637543
309.878666	14895.060064	28.642560
310.469614	14911.996701	28.647578
310.518881	14940.580550	28.652596
310.910124	14967.234869	28.657613
311.296373	14992.964638	28.662631
311.400908	15003.891593	28.667648
311.598201	15040.521755	28.672666
311.940129	15052.602216	28.677684
312.592329	15083.795306	28.682701
312.852121	15099.435403	28.687719
312.996170	15115.011528	28.692736
313.413698	15155.233113	28.697754
313.552140	15179.883920	28.702772
314.031558	15197.552055	28.707789
314.541712	15221.377223	28.712807
315.356298	15239.409789	28.717824
315.265970	15269.408804	28.722842
315.447735	15291.520010	28.727860
315.968165	15299.722691	28.732877
315.778160	15328.549890	28.737895
316.523995	15331.935592	28.742912
316.936061	15359.130426	28.747930
316.861503	15392.042289	28.752948
317.312518	15403.616345	28.757965
317.383549	15429.980370	28.762983
317.995154	15447.596447	28.768000
318.508561	15467.719848	28.773018
318.480384	15500.321432	28.778036
318.875783	15514.844682	28.783053
318.926440	15540.441415	28.788071
319.356024	15560.003225	28.793088
319.747704	15576.191555	28.798106
319.728861	15604.891288	28.803124
320.098417	15637.721370	28.808141
320.536485	15655.942803	28.813159
320.890043	15679.467761	28.818176
321.180239	15701.309785	28.823194
321.390755	15722.431571	28.828212
321.967991	15742.895844	28.833229
322.060705	15769.130603	28.838247
322.789418	15790.758751	28.843264
322.904150	15805.060882	28.848282
323.424233	15830.050700	28.853300
323.543365	15849.677229	28.858317
323.685755	15878.645845	28.863335
324.078715	15902.566022	28.868352
324.481707	15925.256035	28.873370
324.778297	15947.590049	28.878388
325.095879	15969.248058	28.883405
324.891018	15990.744732	28.888423
325.376500	16017.960584	28.893440
325.849134	16051.612210	28.898458
326.307671	16083.926927	28.903476
326.520206	16110.010727	28.908493
326.663249	16126.765930	28.913511
327.386629	16161.663957	28.918528
327.475977	16186.077387	28.923546
327.569500	16219.902398	28.928564
328.493261	16246.133967	28.933581
328.811399	16272.469914	28.938599
329.186461	16298.177921	28.943616
329.512040	16318.195824	28.948634
329.828894	16342.823335	28.953652
330.669748	16362.387869	28.958669
330.441004	16387.123011	28.963687
331.022902	16396.823135	28.968704
331.369162	16422.570563	28.973722
331.486201	16449.819474	28.978740
332.109135	16468.413850	28.983757
332.614750	16491.571708	28.988775
332.541431	16515.575163	28.993792
332.911879	16537.683515	28.998810
332.800140	16556.342523	29.003828
333.449639	16590.731748	29.008845
333.514239	16620.342211	29.013863
334.366569	16641.816140	29.018880
334.575480	16660.399752	29.023898
334.681704	16700.720716	29.028916
334.889026	16717.561120	29.033933
335.467528	16747.350278	29.038951
335.849955	16764.346489	29.043968
336.294501	16795.372746	29.048986
336.221835	16814.856583	29.054004
336.658215	16830.325135	29.059021
337.223967	16864.222598	29.064039
337.685120	16881.730903	29.069056
338.007297	16915.003310	29.074074
338.041212	16953.121968	29.079092
338.879740	16963.072769	29.084109
339.101421	16990.801950	29.089127
339.095968	17010.057512	29.094144
339.425530	17037.555077	29.099162
339.770311	17063.938470	29.104180
340.666653	17084.985907	29.109197
340.806439	17114.269490	29.114215
341.345156	17130.774069	29.119232
341.629451	17157.849326	29.124250
341.173719	17182.778971	29.129268
341.696970	17209.242000	29.134285
342.395978	17231.148067	29.139303
342.571836	17260.419903	29.144320
343.278931	17285.635008	29.149338
343.245797	17308.028567	29.154356
343.422930	17325.550178	29.159373
344.132849	17355.825074	29.164391
344.488528	17373.274539	29.169408
344.902010	17394.979144	29.174426
344.740865	17414.834371	29.179444
345.110278	17430.929834	29.184461
345.668050	17463.288175	29.189479
345.894363	17488.616760	29.194496
346.147058	17507.845015	29.199514
346.436021	17546.145996	29.204532
346.984723	17576.105353	29.209549
347.309385	17598.234728	29.214567
347.595372	17622.158003	29.219584
348.051672	17644.715344	29.224602
348.405823	17672.513194	29.229620
348.687653	17692.766803	29.234637
349.069433	17714.539907	29.239655
348.802183	17746.250914	29.244672
349.624906	17772.712026	29.249690
349.907096	17811.728462	29.254708
350.257103	17838.402696	29.259725
350.633159	17869.488787	29.264743
350.632701	17896.736030	29.269760
351.188840	17925.330190	29.274778
351.366836	17962.758613	29.279796
352.179208	17986.612518	29.284813
352.308364	18025.830245	29.289831
352.800540	18060.139333	29.294848
353.167458	18082.755408	29.299866
353.539239	18117.051868	29.304884
354.042342	18143.854162	29.309901
354.459076	18169.374923	29.314919
354.542947	18205.624539	29.319936
355.088401	18235.920257	29.324954
355.336978	18264.266169	29.329972
356.045275	18281.395880	29.334989
356.224381	18311.907042	29.340007
356.693295	18339.675236	29.345024
356.967753	18354.364879	29.350042
357.171084	18390.368693	29.355060
357.738265	18423.889607	29.360077
358.369581	18444.733656	29.365095
358.400964	18469.304351	29.370112
358.851902	18504.353531	29.375130
359.083949	18525.740352	29.380148
359.552270	18554.709303	29.385165
359.761703	18589.859644	29.390183
360.016678	18608.418957	29.395200
360.196952	18635.961127	29.400218
360.874519	18673.059954	29.405236
361.100901	18704.714150	29.410253
361.838600	18735.650213	29.415271
362.019798	18760.703227	29.420288
362.424348	18778.733853	29.425306
362.622227	18810.670667	29.430324
363.028642	18835.461059	29.435341
363.384505	18861.605088	29.440359
363.466078	18906.101068	29.445376
364.118688	18929.564186	29.450394
364.124200	18963.066608	29.455412
364.915735	18989.534268	29.460429
365.334686	19012.168545	29.465447
365.494922	19047.472727	29.470464
365.997322	19073.391915	29.475482
366.401646	19102.807639	29.480500
366.642172	19129.519747	29.485517
367.468616	19163.254038	29.490535
367.691261	19184.630419	29.495552
368.018668	19200.702341	29.500570
367.866497	19230.401281	29.505588
368.535722	19255.985004	29.510605
368.729168	19279.248798	29.515623
368.954443	19313.563996	29.520640
369.303960	19329.089219	29.525658
369.873567	19366.825436	29.530676
369.783546	19391.883836	29.535693
370.659250	19435.018309	29.540711
370.703079	19456.751532	29.545728
371.360793	19485.471072	29.550746
371.359093	19522.696872	29.555764
371.686174	19543.501303	29.560781
372.479914	19573.330587	29.565799
372.441120	19606.822097	29.570816
373.252924	19637.135136	29.575834
373.211887	19687.742680	29.580852
373.768969	19711.164841	29.585869
374.115506	19741.873143	29.590887
374.724562	19781.019226	29.595904
375.072380	19805.959027	29.600922
375.463591	19836.167669	29.605940
375.980858	19862.805839	29.610957
376.054421	19889.298732	29.615975
376.357785	19925.870973	29.620992
377.007032	19953.796445	29.626010
377.164570	19981.672616	29.631028
377.349264	20024.171089	29.636045
378.342599	20057.969240	29.641063
378.461429	20091.120978	29.646080
378.871876	20118.193227	29.651098
379.495820	20161.634104	29.656116
379.682556	20185.923574	29.661133
380.481455	20212.568651	29.666151
380.380299	20250.468504	29.671168
380.783870	20275.033712	29.676186
381.266649	20310.093781	29.681204
381.746147	20342.298576	29.686221
382.023759	20371.950877	29.691239
382.411488	20408.081160	29.696256
382.798069	20428.100063	29.701274
383.044008	20465.225676	29.706292
383.218351	20497.611209	29.711309
384.071179	20524.968551	29.716327
384.646506	20561.846885	29.721344
384.991811	20581.360625	29.726362
385.336215	20614.667463	29.731380
385.404388	20643.171449	29.736397
386.117181	20680.868814	29.741415
386.117735	20713.376699	29.746432
386.900715	20744.296215	29.751450
387.001527	20772.605724	29.756468
387.505772	20795.809997	29.761485
387.824181	20828.236692	29.766503
388.201893	20874.150302	29.771520
388.534173	20903.030311	29.776538
388.859769	20937.143081	29.781556
388.914017	20970.590747	29.786573
389.959612	20996.977103	29.791591
389.828973	21037.315696	29.796608
390.598530	21053.793767	29.801626
390.830411	21096.362987	29.806644
391.309278	21138.015338	29.811661
391.531055	21160.973636	29.816679
391.402192	21200.326595	29.821696
392.182851	21230.368963	29.826714
392.463404	21270.871092	29.831732
393.188221	21303.203316	29.836749
393.763257	21329.373173	29.841767
393.728482	21363.814828	29.846784
394.455312	21385.708578	29.851802
394.902458	21420.384455	29.856820
395.191510	21442.827055	29.861837
395.718432	21473.604586	29.866855
396.287634	21504.179666	29.871872
396.372845	21529.017460	29.876890
396.883991	21558.811889	29.881908
396.796886	21595.145099	29.886925
397.011009	21611.799102	29.891943
397.177808	21659.301967	29.896960
397.772266	21699.964322	29.901978
398.046587	21738.174700	29.906996
398.704299	21780.154240	29.912013
399.462874	21812.033382	29.917031
399.739346	21851.513706	29.922048
400.435708	21880.009542	29.927066
400.481661	21914.426871	29.932084
400.872661	21952.019105	29.937101
401.329235	21988.211006	29.942119
401.473379	22018.941925	29.947136
402.242408	22057.340819	29.952154
402.823150	22096.565451	29.957172
403.104602	22128.665173	29.962189
403.537678	22160.052443	29.967207
404.036187	22208.736840	29.972224
404.541865	22234.735515	29.977242
405.086802	22253.303406	29.982260
405.077446	22298.781764	29.987277
405.581721	22329.305102	29.992295
405.723170	22368.858157	29.997312
406.470250	22398.092426	30.002330
407.127970	22428.983654	30.007348
407.263983	22468.278683	30.012365
407.934406	22492.608969	30.017383
407.966308	22536.507992	30.022400
408.322843	22568.122742	30.027418
409.123213	22605.348782	30.032436
409.379457	22632.429680	30.037453
409.852052	22668.525529	30.042471
410.444749	22711.724156	30.047488
410.741420	22743.171629	30.052506
411.192167	22774.367533	30.057524
411.341818	22811.657972	30.062541
411.943933	22840.953515	30.067559
411.793770	22886.057171	30.072576
412.573223	22917.612552	30.077594
413.197017	22948.737391	30.082612
413.334006	22987.376107	30.087629
413.837815	23014.380833	30.092647
413.994137	23053.749666	30.097664
414.613239	23086.347811	30.102682
415.120078	23120.145272	30.107700
415.538800	23166.380048	30.112717
416.066515	23200.187014	30.117735
416.021059	23240.996996	30.122752
416.490502	23268.228622	30.127770
417.172289	23311.869579	30.132788
417.475012	23342.798877	30.137805
418.516796	23379.912724	30.142823
418.206306	23415.051999	30.147840
418.914189	23453.406300	30.152858
419.147862	23488.612131	30.157876
419.314861	23511.992482	30.162893
420.145901	23550.928010	30.167911
420.696163	23598.122671	30.172928
420.747088	23630.747510	30.177946
421.395377	23653.622927	30.182964
421.483924	23696.011635	30.187981
422.351735	23729.090059	30.192999
422.324460	23764.798562	30.198016
422.381750	23797.542743	30.203034
423.280684	23829.409463	30.208052
423.658767	23870.236540	30.213069
424.337762	23896.602043	30.218087
424.428696	23938.719157	30.223104
424.723736	23974.118452	30.228122
425.045107	24006.107517	30.233140
425.464904	24053.235217	30.238157
426.196824	24088.111284	30.243175
426.636383	24127.197728	30.248192
426.965747	24174.472587	30.253210
427.451216	24198.404207	30.258228
427.842387	24246.263585	30.263245
427.920892	24284.332575	30.268263
428.448952	24325.017018	30.273280
428.969828	24360.583847	30.278298
429.538147	24398.272994	30.283316
430.291034	24442.853218	30.288333
430.598777	24475.780463	30.293351
430.926464	24527.707620	30.298368
431.072811	24565.646445	30.303386
432.013285	24590.537359	30.308404
432.084317	24642.915789	30.313421
432.828729	24680.483090	30.318439
433.330556	24728.263090	30.323456
433.888733	24759.710695	30.328474
434.315665	24797.321624	30.333492
434.702710	24835.690913	30.338509
434.754144	24870.946677	30.343527
435.261801	24915.857069	30.348544
435.982677	24954.698832	30.353562
436.278842	24989.170743	30.358580
436.714227	25036.013922	30.363597
437.146284	25074.951714	30.368615
437.813921	25108.714711	30.373632
437.803964	25149.832684	30.378650
438.487910	25185.887336	30.383668
438.721797	25223.504020	30.388685
439.773074	25261.574168	30.393703
440.001380	25305.644412	30.398720
440.301303	25341.822693	30.403738
440.701026	25377.776851	30.408756
440.918299	25418.644906	30.413773
441.664474	25453.615914	30.418791
442.403153	25500.159872	30.423808
442.620901	25531.946402	30.428826
442.932807	25567.510181	30.433844
443.467441	25619.331901	30.438861
443.707468	25665.025315	30.443879
444.053102	25704.022100	30.448896
444.130252	25741.822299	30.453914
444.929206	25768.487475	30.458932
445.717063	25825.705240	30.463949
445.371967	25858.231402	30.468967
446.477310	25911.171601	30.473984
446.781096	25945.429073	30.479002
447.489355	25987.321059	30.484020
447.766592	26024.780766	30.489037
448.459695	26076.863241	30.494055
448.775836	26119.183484	30.499072
449.066785	26160.490225	30.504090
449.751086	26193.778423	30.509108
450.015083	26242.307115	30.514125
450.628563	26266.903722	30.519143
450.941553	26294.972939	30.524160
451.619734	26332.591620	30.529178
451.977319	26370.633475	30.534196
452.264620	26409.824043	30.539213
452.806071	26438.003038	30.544231
453.050117	26474.185778	30.549248
452.883639	26518.023451	30.554266
453.817148	26560.709292	30.559284
454.113232	26604.183969	30.564301
454.747395	26647.194969	30.569319
455.305105	26694.054435	30.574336
455.904491	26734.024701	30.579354
456.722095	26770.396224	30.584372
457.077286	26797.397720	30.589389
457.301537	26839.986671	30.594407
457.894351	26882.404218	30.599424
457.813674	26927.468118	30.604442
458.518041	26957.954523	30.609460
458.758595	27005.635466	30.614477
459.549459	27047.965455	30.619495
459.817631	27096.527138	30.624512
460.429197	27135.510307	30.629530
460.948446	27188.653096	30.634548
460.988237	27238.432806	30.639565
461.410893	27273.590366	30.644583
461.820492	27318.584659	30.649600
462.191379	27368.186418	30.654618
463.242668	27404.787937	30.659636
463.401343	27450.466513	30.664653
463.936672	27506.375991	30.669671
464.318781	27551.962913	30.674688
464.772450	27604.352275	30.679706
465.444988	27646.721006	30.684724
465.970310	27696.741814	30.689741
466.499534	27740.460508	30.694759
467.147507	27789.135009	30.699776
467.282243	27829.369825	30.704794
467.667016	27879.065461	30.709812
468.411324	27921.202299	30.714829
468.798780	27963.824923	30.719847
469.338482	28002.024605	30.724864
470.041245	28046.089692	30.729882
470.379986	28094.478360	30.734900
470.611803	28139.104105	30.739917
471.008604	28177.396025	30.744935
471.307963	28228.515410	30.749952
472.433660	28283.898418	30.754970
472.816946	28321.813480	30.759988
473.565514	28369.607664	30.765005
473.719866	28416.243513	30.770023
474.244991	28452.783952	30.775040
474.023692	28485.857463	30.780058
474.974313	28532.874525	30.785076
475.595411	28583.527228	30.790093
476.128282	28624.933813	30.795111
476.736788	28659.438886	30.800128
476.564375	28719.394117	30.805146
477.431519	28767.606799	30.810164
477.990050	28815.109423	30.815181
478.308827	28867.472581	30.820199
479.149376	28893.067113	30.825216
479.267263	28951.169761	30.830234
480.097294	28986.885918	30.835252
480.346327	29021.523755	30.840269
480.868468	29060.429792	30.845287
481.476096	29105.719372	30.850304
481.640516	29152.797789	30.855322
482.273159	29190.043298	30.860340
482.404794	29230.508906	30.865357
482.854625	29274.388696	30.870375
483.581939	29314.223879	30.875392
483.732622	29355.792938	30.880410
484.055034	29399.623420	30.885428
484.658445	29451.652714	30.890445
485.233350	29497.940699	30.895463
485.923667	29541.530546	30.900480
486.261581	29587.135241	30.905498
487.021012	29635.164555	30.910516
487.025089	29682.920378	30.915533
487.877576	29720.062881	30.920551
488.190376	29766.209207	30.925568
488.329664	29821.365274	30.930586
489.127294	29864.129880	30.935604
489.526714	29915.686598	30.940621
489.730214	29972.659855	30.945639
490.443933	30014.249515	30.950656
491.226900	30078.218466	30.955674
492.253590	30118.722624	30.960692
492.333379	30157.718984	30.965709
492.756350	30212.528239	30.970727
493.323835	30253.142513	30.975744
493.721232	30310.908109	30.980762
494.096144	30352.380841	30.985780
494.184618	30403.355338	30.990797
494.842504	30457.894558	30.995815
495.547368	30508.880237	31.000832
495.943928	30576.040361	31.005850
496.533801	30625.666261	31.010868
497.158751	30663.408714	31.015885
497.240412	30722.230026	31.020903
498.276970	30771.558739	31.025920
498.758691	30824.571423	31.030938
499.225996	30869.577100	31.035956
499.946657	30918.778638	31.040973
500.349072	30983.246180	31.045991
500.775375	31029.289043	31.051008
501.214960	31073.616771	31.056026
501.229840	31127.405047	31.061044
502.519115	31177.118693	31.066061
502.633184	31228.540045	31.071079
503.552530	31272.211463	31.076096
503.714326	31332.722481	31.081114
504.394026	31375.407537	31.086132
504.791997	31427.790066	31.091149
505.371928	31486.434352	31.096167
505.691049	31526.426239	31.101184
506.217200	31587.664828	31.106202
506.787908	31639.913365	31.111220
507.614604	31685.977155	31.116237
508.005882	31739.550014	31.121255
508.621931	31788.959652	31.126272
508.859512	31837.372939	31.131290
509.379806	31877.567900	31.136308
510.367894	31927.355805	31.141325
510.676518	31985.146283	31.146343
511.314979	32035.596108	31.151360
511.549072	32077.069051	31.156378
512.110721	32129.901852	31.161396
512.724025	32182.473819	31.166413
513.000486	32237.545274	31.171431
513.744921	32295.439046	31.176448
514.172549	32335.681014	31.181466
514.572460	32382.299981	31.186484
515.137958	32433.881191	31.191501
515.051896	32483.680611	31.196519
515.875849	32530.163951	31.201536
516.508340	32587.235231	31.206554
516.994002	32625.609979	31.211572
517.007010	32671.367165	31.216589
517.679120	32732.118415	31.221607
518.437418	32775.179677	31.226624
519.084054	32833.115543	31.231642
519.379302	32875.914463	31.236660
519.849773	32934.617893	31.241677
520.267980	32987.519582	31.246695
521.110555	33028.298499	31.251712
521.209298	33083.406336	31.256730
521.996262	33139.007137	31.261748
522.602808	33193.808129	31.266765
522.593345	33237.161291	31.271783
523.667110	33300.418118	31.276800
524.464448	33355.644855	31.281818
524.671369	33409.718714	31.286836
525.257686	33456.576412	31.291853
525.433564	33520.246391	31.296871
526.005755	33569.009579	31.301888
526.813700	33628.325940	31.306906
527.623934	33683.071017	31.311924
528.033285	33737.866379	31.316941
528.672509	33789.483632	31.321959
528.934855	33842.841810	31.326976
529.534349	33898.081991	31.331994
529.965349	33956.509946	31.337012
530.983435	34005.659527	31.342029
531.305861	34059.489353	31.347047
532.012269	34110.458298	31.352064
532.124604	34160.679512	31.357082
532.838919	34214.479968	31.362100
533.317227	34267.223719	31.367117
533.793728	34329.584543	31.372135
534.778339	34372.879184	31.377152
535.057888	34436.415561	31.382170
535.596225	34492.311785	31.387188
536.273027	34549.817714	31.392205
536.171024	34604.916708	31.397223
536.864320	34653.650792	31.402240
537.718444	34715.409859	31.407258
537.945974	34770.078308	31.412276
538.708825	34811.916420	31.417293
538.750217	34882.332635	31.422311
539.381778	34938.854035	31.427328
540.054071	34998.979519	31.432346
540.609821	35058.219265	31.437364
541.519045	35120.160567	31.442381
541.644369	35185.341988	31.447399
542.074710	35247.719068	31.452416
542.603673	35301.835848	31.457434
543.514424	35358.814148	31.462452
544.029502	35414.356041	31.467469
544.760217	35481.947428	31.472487
545.060543	35541.032515	31.477504
545.629331	35601.011519	31.482522
546.024536	35655.257638	31.487540
546.536056	35720.285367	31.492557
547.433316	35777.500855	31.497575
548.173607	35833.040183	31.502592
548.682550	35882.235930	31.507610
549.212800	35952.888953	31.512628
549.958842	35998.013713	31.517645
550.392930	36048.650585	31.522663
550.741655	36109.310444	31.527680
551.448167	36158.937474	31.532698
552.014582	36219.633106	31.537716
552.521531	36272.408970	31.542733
552.767842	36320.628831	31.547751
553.676189	36363.231287	31.552768
554.185078	36418.138125	31.557786
554.106855	36475.375479	31.562804
554.971746	36524.763565	31.567821
555.196467	36580.170598	31.572839
555.846022	36632.962958	31.577856
556.377473	36696.757502	31.582874
556.765938	36754.459990	31.587892
557.945561	36806.973738	31.592909
558.318759	36880.860354	31.597927
558.965859	36933.015181	31.602944
559.491390	36981.882048	31.607962
559.613025	37048.473525	31.612980
560.436995	37104.755541	31.617997
561.030518	37165.076528	31.623015
561.601202	37224.794212	31.628032
561.911504	37278.773194	31.633050
562.357249	37352.656396	31.638068
563.113649	37414.672564	31.643085
563.639207	37487.082999	31.648103
564.086862	37546.441434	31.653120
564.856237	37605.237437	31.658138
565.614424	37669.486278	31.663156
566.365590	37729.354157	31.668173
566.810421	37790.515933	31.673191
567.341278	37853.422380	31.678208
567.968674	37914.404148	31.683226
568.519436	37970.509895	31.688244
569.359889	38025.621865	31.693261
569.564551	38090.540434	31.698279
570.312408	38158.346273	31.703296
570.701477	38211.259196	31.708314
571.324704	38288.532632	31.713332
572.033400	38341.667737	31.718349
572.803724	38404.848153	31.723367
573.424005	38468.956559	31.728384
574.131799	38521.339714	31.733402
574.398992	38599.005184	31.738420
575.256012	38638.825059	31.743437
575.351098	38712.894319	31.748455
575.877769	38771.364730	31.753472
576.669733	38819.371934	31.758490
576.940114	38890.669768	31.763508
577.742529	38954.858596	31.768525
578.184680	39024.011442	31.773543
578.893812	39073.543613	31.778560
579.986790	39140.400475	31.783578
580.075523	39211.323077	31.788596
580.713284	39276.310176	31.793613
581.556572	39335.510380	31.798631
581.654171	39401.132645	31.803648
582.744924	39457.473883	31.808666
583.195729	39520.486254	31.813684
583.634784	39580.857158	31.818701
583.997432	39650.454492	31.823719
584.835251	39703.262833	31.828736
585.534657	39771.656814	31.833754
586.013355	39836.335318	31.838772
586.734267	39897.086678	31.843789
587.120652	39957.372013	31.848807
587.761983	40020.842960	31.853824
588.491300	40086.444244	31.858842
588.790981	40155.547111	31.863860
589.596109	40215.059254	31.868877
590.219170	40280.152844	31.873895
590.696815	40333.676855	31.878912
591.220012	40392.114225	31.883930
591.704713	40453.606136	31.888948
592.501442	40506.365942	31.893965
592.969205	40571.307639	31.898983
593.724122	40625.402409	31.904000
594.302771	40692.546979	31.909018
594.845821	40753.094574	31.914036
595.179523	40801.329715	31.919053
595.632985	40871.953938	31.924071
596.259060	40929.775804	31.929088
596.937739	40984.844732	31.934106
597.511338	41058.467549	31.939124
597.777435	41115.682205	31.944141
598.586984	41182.937581	31.949159
598.914625	41248.023397	31.954176
599.486796	41317.871511	31.959194
599.860878	41397.889302	31.964212
600.488670	41463.023617	31.969229
601.216823	41546.705412	31.974247
601.958432	41620.841402	31.979264
602.877274	41691.597768	31.984282
603.217807	41766.069026	31.989300
603.971234	41833.088518	31.994317
604.826804	41914.240815	31.999335
605.246013	41983.545766	32.004352
605.979928	42052.099589	32.009370
606.488819	42127.450155	32.014388
607.411224	42190.914993	32.019405
607.918413	42266.892466	32.024423
608.324823	42327.731447	32.029440
609.372595	42391.474501	32.034458
609.654280	42461.491911	32.039476
610.011783	42533.129515	32.044493
610.957791	42606.009761	32.049511
611.349178	42673.974009	32.054528
612.337510	42737.885498	32.059546
612.813893	42806.912102	32.064564
613.666866	42893.128459	32.069581
614.136451	42950.252756	32.074599
614.746163	43020.353388	32.079616
615.676227	43078.443220	32.084634
615.941496	43162.665371	32.089652
616.865642	43222.957667	32.094669
617.502831	43291.068744	32.099687
618.213952	43362.653650	32.104704
618.657643	43427.645488	32.109722
618.960027	43491.451522	32.114740
619.573249	43553.064788	32.119757
620.434712	43635.013137	32.124775
620.802524	43703.654715	32.129792
621.555049	43774.342593	32.134810
622.006933	43852.548033	32.139828
622.559741	43913.469643	32.144845
623.555319	43980.375485	32.149863
623.603719	44068.784493	32.154880
624.509293	44140.575490	32.159898
625.175138	44212.094315	32.164916
625.858455	44279.328279	32.169933
626.490675	44362.586631	32.174951
627.209586	44431.953502	32.179968
628.348225	44490.817704	32.184986
628.605320	44574.281081	32.190004
629.625846	44634.872064	32.195021
629.981155	44705.194961	32.200039
630.416145	44767.712432	32.205056
631.047546	44827.561524	32.210074
631.415396	44909.465349	32.215092
632.251464	44973.932143	32.220109
633.257269	45045.786261	32.225127
633.376480	45104.912946	32.230144
634.314020	45165.606924	32.235162
634.600689	45230.027656	32.240180
635.371850	45288.641549	32.245197
635.998641	45358.601365	32.250215
636.730669	45427.108959	32.255232
637.193455	45491.306759	32.260250
637.298011	45560.241971	32.265268
638.138716	45636.286245	32.270285
638.974864	45716.949389	32.275303
639.635674	45785.140282	32.280320
640.655782	45845.405659	32.285338
641.246304	45927.271995	32.290356
641.453583	45987.139994	32.295373
642.421124	46052.443302	32.300391
642.794154	46128.752262	32.305408
643.542776	46191.566181	32.310426
643.921630	46275.314130	32.315444
644.737085	46350.251385	32.320461
645.588846	46422.905812	32.325479
646.002532	46501.955189	32.330496
646.906975	46564.657178	32.335514
647.340034	46648.701675	32.340532
647.888536	46720.752959	32.345549
648.593232	46800.928148	32.350567
648.655476	46881.185255	32.355584
649.791419	46958.788284	32.360602
650.589965	47041.872349	32.365620
651.255162	47120.669404	32.370637
651.908953	47185.411474	32.375655
652.848186	47267.993536	32.380672
653.559012	47346.025069	32.385690
653.905970	47426.075029	32.390708
654.626176	47502.935254	32.395725
655.189875	47577.441519	32.400743
655.448554	47659.536903	32.405760
656.138332	47730.588671	32.410778
656.974081	47825.297800	32.415796
657.732943	47901.198018	32.420813
658.835902	47974.988482	32.425831
659.244341	48066.096150	32.430848
660.395721	48137.614655	32.435866
661.009213	48210.767635	32.440884
661.728348	48292.400939	32.445901
662.291773	48369.642932	32.450919
662.793387	48437.366932	32.455936
663.787576	48504.919092	32.460954
664.371578	48581.329785	32.465972
664.947371	48652.933720	32.470989
665.762573	48731.573668	32.476007
666.227420	48808.098680	32.481024
666.865604	48882.508966	32.486042
667.458811	48961.968992	32.491060
667.932129	49033.140962	32.496077
668.771436	49107.552116	32.501095
669.447806	49187.512372	32.506112
670.409340	49258.697160	32.511130
671.125976	49341.973259	32.516148
671.545145	49418.115191	32.521165
672.308277	49499.106886	32.526183
672.579122	49576.651845	32.531200
673.487080	49642.240524	32.536218
673.988834	49721.540344	32.541236
674.680224	49813.097822	32.546253
675.665493	49880.611145	32.551271
676.274338	49961.875386	32.556288
676.907328	50028.735680	32.561306
677.657065	50095.394399	32.566324
678.026195	50168.079393	32.571341
678.577618	50232.763867	32.576359
679.301849	50313.568377	32.581376
680.030528	50389.557485	32.586394
680.712770	50458.075360	32.591412
681.446974	50531.602788	32.596429
682.037157	50603.058686	32.601447
682.830325	50699.760446	32.606464
683.571874	50762.689283	32.611482
684.253759	50847.387245	32.616500
684.670135	50917.384415	32.621517
685.312975	50992.908070	32.626535
685.813162	51070.694200	32.631552
686.675640	51152.966923	32.636570
687.241189	51238.557712	32.641588
687.990702	51325.480406	32.646605
688.790637	51405.701073	32.651623
689.225008	51487.763617	32.656640
690.189902	51568.522159	32.661658
690.902790	51645.517602	32.666676
691.169329	51734.738424	32.671693
692.158909	51820.828102	32.676711
692.419507	51900.919800	32.681728
693.302965	51988.260598	32.686746
694.464027	52070.439185	32.691764
694.513066	52164.074437	32.696781
695.636370	52247.803513	32.701799
696.256817	52346.962675	32.706816
697.037075	52433.802428	32.711834
697.971833	52509.297941	32.716852
698.321675	52610.354631	32.721869
699.148372	52697.618380	32.726887
700.038545	52780.386078	32.731904
700.984753	52871.611968	32.736922
701.665704	52945.446440	32.741940
701.993373	53041.541076	32.746957
702.779365	53123.826398	32.751975
703.528686	53213.407548	32.756992
704.420899	53298.359898	32.762010
705.256986	53382.125354	32.767028
706.121077	53469.082372	32.772045
706.785037	53540.909067	32.777063
707.214837	53630.276065	32.782080
708.086319	53713.834661	32.787098
708.681951	53793.013404	32.792116
709.286602	53886.543199	32.797133
710.186571	53970.408321	32.802151
710.725922	54063.942716	32.807168
711.465866	54148.327129	32.812186
712.497771	54232.558541	32.817204
713.137105	54325.375881	32.822221
713.793405	54412.362589	32.827239
714.587958	54497.359866	32.832256
715.175451	54580.852093	32.837274
716.124047	54655.023378	32.842292
716.290752	54748.403671	32.847309
717.451197	54825.466018	32.852327
717.747560	54917.966014	32.857344
718.774440	55016.180456	32.862362
719.109183	55088.759536	32.867380
720.383766	55182.075623	32.872397
721.161141	55263.528061	32.877415
721.535629	55347.347451	32.882432
722.403273	55440.867509	32.887450
723.149805	55521.180191	32.892468
723.377749	55619.496924	32.897485
724.376246	55706.124681	32.902503
725.195071	55780.205886	32.907520
725.701448	55868.575730	32.912538
726.495699	55947.635630	32.917556
726.804424	56027.670501	32.922573
727.646147	56101.875693	32.927591
728.262785	56200.089645	32.932608
729.080690	56296.209301	32.937626
730.011665	56375.742851	32.942644
730.584540	56467.984046	32.947661
731.256988	56547.470048	32.952679
732.186760	56646.162086	32.957696
732.770038	56731.554835	32.962714
733.516635	56819.333628	32.967732
734.031384	56913.743797	32.972749
734.812796	57008.903699	32.977767
735.181736	57101.521027	32.982784
736.105605	57195.545457	32.987802
737.176648	57296.376236	32.992820
737.260448	57386.165930	32.997837
738.164035	57476.378210	33.002855
739.038222	57577.994156	33.007872
739.618818	57674.802058	33.012890
740.521396	57769.629534	33.017908
741.346706	57880.438019	33.022925
742.320880	57983.951430	33.027943
742.860839	58067.463262	33.032960
743.612954	58173.676868	33.037978
744.576981	58268.553641	33.042996
745.310008	58371.131762	33.048013
746.251226	58469.816814	33.053031
747.040641	58552.512745	33.058048
748.042869	58659.828601	33.063066
748.763433	58755.827733	33.068084
749.442340	58853.852859	33.073101
750.191418	58944.746742	33.078119
751.171027	59036.630242	33.083136
751.912993	59121.171091	33.088154
752.567314	59214.979739	33.093172
753.112794	59318.401407	33.098189
753.946103	59412.043533	33.103207
754.866322	59504.767275	33.108224
755.612894	59598.790819	33.113242
756.463003	59688.671573	33.118260
757.033399	59782.400600	33.123277
758.072460	59876.227496	33.128295
758.792383	59969.516063	33.133312
759.349396	60072.008644	33.138330
760.307089	60161.918599	33.143348
761.278895	60257.719722	33.148365
761.893927	60346.943428	33.153383
762.645526	60431.829113	33.158400
763.542720	60537.872056	33.163418
764.644341	60620.779300	33.168436
764.759296	60720.805525	33.173453
765.694626	60811.094827	33.178471
766.663764	60902.423610	33.183488
767.210784	61001.997190	33.188506
768.060380	61085.078396	33.193524
768.593886	61178.438728	33.198541
769.262012	61269.860321	33.203559
770.556109	61369.052532	33.208576
770.977405	61454.727759	33.213594
771.615029	61558.688826	33.218612
772.283646	61661.809894	33.223629
773.171584	61751.280808	33.228647
774.225108	61840.181717	33.233664
774.858362	61945.183246	33.238682
775.615830	62034.960476	33.243700
776.173750	62131.669291	33.248717
776.744525	62215.760163	33.253735
777.362340	62309.396422	33.258752
777.985839	62408.830749	33.263770
779.101297	62494.489494	33.268788
780.009521	62595.589185	33.273805
780.642158	62686.635409	33.278823
781.865889	62785.768347	33.283840
782.353873	62876.932875	33.288858
783.236121	62965.225256	33.293876
783.915696	63058.962282	33.298893
784.697098	63147.720568	33.303911
785.557125	63249.153316	33.308928
785.811618	63346.047303	33.313946
786.547384	63445.854353	33.318964
787.028800	63545.030582	33.323981
787.911501	63647.911115	33.328999
789.010148	63748.865376	33.334016
789.190826	63864.670062	33.339034
790.256309	63966.744602	33.344052
791.123955	64085.177615	33.349069
792.157215	64193.791491	33.354087
793.185960	64301.577204	33.359104
793.926536	64402.982680	33.364122
794.814793	64506.834485	33.369140
795.572810	64615.854145	33.374157
796.338802	64723.518207	33.379175
797.536165	64828.399194	33.384192
797.823375	64931.561828	33.389210
798.477583	65034.952309	33.394228
799.574431	65137.058339	33.399245
800.187283	65253.225910	33.404263
800.750682	65354.586981	33.409280
801.657726	65474.147285	33.414298
802.842326	65583.598149	33.419316
803.685959	65698.256462	33.424333
804.215925	65813.293634	33.429351
805.315779	65920.188749	33.434368
806.107936	66018.952501	33.439386
807.206959	66142.981092	33.444404
807.958076	66248.311384	33.449421
808.816591	66352.567960	33.454439
809.532297	66451.060450	33.459456
809.890371	66562.310107	33.464474
810.545102	66666.891122	33.469492
811.973142	66787.825915	33.474509
812.797603	66897.142550	33.479527
814.000947	66992.857229	33.484544
814.359828	67102.513570	33.489562
815.268559	67208.538606	33.494580
816.068410	67312.175128	33.499597
817.143562	67427.419126	33.504615
818.336305	67538.814586	33.509632
818.643178	67640.921394	33.514650
819.481207	67737.329226	33.519668
820.139445	67838.830943	33.524685
820.900548	67949.194054	33.529703
821.856473	68053.600596	33.534720
823.098791	68167.625033	33.539738
823.747242	68265.552501	33.544756
824.600285	68367.601993	33.549773
825.366714	68482.373517	33.554791
826.260649	68589.350012	33.559808
826.649729	68696.171723	33.564826
827.742816	68806.575162	33.569844
828.320689	68912.646361	33.574861
829.078359	69023.508495	33.579879
830.327409	69118.590725	33.584896
830.670451	69226.947851	33.589914
831.527566	69314.911624	33.594932
832.788521	69423.125835	33.599949
833.261985	69525.593926	33.604967
833.846781	69621.719168	33.609984
834.606468	69725.162701	33.615002
835.703307	69828.161256	33.620020
836.656990	69929.055007	33.625037
837.088119	70036.812814	33.630055
837.972692	70145.462567	33.635072
838.984769	70257.930184	33.640090
839.909429	70358.963121	33.645108
840.845168	70470.037827	33.650125
841.407739	70578.043242	33.655143
842.445174	70681.896673	33.660160
843.275248	70796.586118	33.665178
844.174916	70895.282037	33.670196
845.138176	71017.461890	33.675213
845.460215	71125.393237	33.680231
846.594366	71232.450622	33.685248
847.551821	71356.393405	33.690266
848.106318	71465.568927	33.695284
849.146653	71570.995905	33.700301
849.789819	71695.141478	33.705319
851.012002	71807.329529	33.710336
851.601520	71924.176672	33.715354
852.292207	72034.853072	33.720372
853.218891	72155.156774	33.725389
854.014305	72277.026778	33.730407
855.081303	72401.742582	33.735424
855.837218	72527.508275	33.740442
856.329486	72641.004732	33.745460
857.574809	72758.082172	33.750477
858.637609	72895.099457	33.755495
859.483732	72995.014867	33.760512
860.268867	73122.476034	33.765530
861.264551	73245.661718	33.770548
862.168431	73354.574989	33.775565
862.748019	73469.897890	33.780583
863.951502	73591.330037	33.785600
864.668332	73715.929507	33.790618
865.635928	73833.954469	33.795636
866.333107	73952.794943	33.800653
867.114262	74080.121973	33.805671
868.093779	74193.650069	33.810688
869.140652	74320.151310	33.815706
869.824847	74437.513979	33.820724
871.117405	74550.031904	33.825741
871.968806	74673.424085	33.830759
872.593931	74797.333600	33.835776
873.542437	74916.278318	33.840794
874.542913	75036.469446	33.845812
875.585847	75153.323055	33.850829
876.535265	75276.056633	33.855847
877.405759	75387.073435	33.860864
878.122195	75513.860029	33.865882
878.712480	75631.508609	33.870900
879.872862	75744.052212	33.875917
880.765911	75867.950018	33.880935
881.535470	75992.412422	33.885952
882.662147	76105.000804	33.890970
883.346919	76220.458351	33.895988
884.429803	76339.514957	33.901005
884.714950	76454.846060	33.906023
885.469895	76579.376775	33.911040
886.641031	76702.272101	33.916058
887.570650	76823.077621	33.921076
888.516429	76945.489952	33.926093
889.174214	77066.883829	33.931111
890.142388	77156.116566	33.936128
891.048437	77291.901278	33.941146
891.901808	77401.244144	33.946164
892.805119	77516.761629	33.951181
893.533452	77628.468567	33.956199
894.225470	77747.123788	33.961216
895.155125	77865.792985	33.966234
895.803070	77994.894776	33.971252
896.669138	78119.250403	33.976269
897.549165	78247.037536	33.981287
898.492594	78366.099452	33.986304
899.127504	78496.396464	33.991322
899.966227	78631.678924	33.996340
901.309884	78755.785279	34.001357
902.034890	78888.388386	34.006375
902.754745	79017.128972	34.011392
903.733334	79149.224879	34.016410
904.791051	79289.239724	34.021428
905.710430	79418.267651	34.026445
906.436590	79554.611089	34.031463
907.694434	79688.566180	34.036480
908.908382	79817.157094	34.041498
910.105358	79949.222606	34.046516
910.917904	80077.712873	34.051533
911.490826	80207.128101	34.056551
911.977292	80332.984714	34.061568
913.389068	80475.610640	34.066586
914.511368	80606.804095	34.071604
915.309018	80738.074337	34.076621
915.879966	80874.473856	34.081639
917.312502	81006.558153	34.086656
918.030895	81135.346745	34.091674
918.657948	81264.758375	34.096692
919.919883	81395.857634	34.101709
921.010711	81538.121107	34.106727
921.714689	81673.870175	34.111744
922.728088	81804.832871	34.116762
923.776553	81941.251474	34.121780
924.799612	82061.507657	34.126797
925.426248	82212.412197	34.131815
926.281346	82340.107912	34.136832
927.586873	82478.173990	34.141850
928.291019	82603.765918	34.146868
929.463379	82733.364959	34.151885
930.481119	82890.090927	34.156903
931.329937	83021.376429	34.161920
932.172161	83155.552463	34.166938
933.396916	83292.494786	34.171956
934.260389	83419.408451	34.176973
935.018117	83560.707884	34.181991
936.037753	83679.780389	34.187008
937.239356	83827.866556	34.192026
937.701879	83960.103814	34.197044
938.820203	84082.811773	34.202061
939.665796	84228.358195	34.207079
940.668699	84365.061618	34.212096
941.603105	84493.185353	34.217114
942.389110	84633.395915	34.222132
943.482432	84767.514828	34.227149
944.225897	84913.802966	34.232167
945.197302	85041.834645	34.237184
946.422705	85183.246218	34.242202
947.336677	85322.667126	34.247220
948.355137	85448.957236	34.252237
949.751503	85597.642905	34.257255
950.609171	85728.166400	34.262272
951.798571	85848.032263	34.267290
952.438549	85976.322709	34.272308
953.351273	86085.233725	34.277325
953.873660	86212.504528	34.282343
954.872952	86332.541544	34.287360
956.157349	86462.608682	34.292378
957.020480	86588.281782	34.297396
957.864842	86706.405761	34.302413
958.639571	86831.523500	34.307431
959.545706	86963.983779	34.312448
960.404686	87084.248603	34.317466
961.026570	87229.464914	34.322484
962.173334	87358.721204	34.327501
963.333354	87502.283223	34.332519
964.524811	87630.659309	34.337536
965.161004	87771.339281	34.342554
965.636247	87905.353958	34.347572
967.177819	88050.810496	34.352589
968.410353	88188.142192	34.357607
968.559767	88323.553095	34.362624
970.009033	88470.268086	34.367642
970.892832	88605.425889	34.372660
971.742557	88747.749897	34.377677
972.704865	88899.004156	34.382695
973.567996	89041.593606	34.387712
974.768091	89178.174573	34.392730
975.724512	89342.954319	34.397748
977.010531	89481.677679	34.402765
977.912014	89624.492030	34.407783
979.037405	89768.792819	34.412800
980.249314	89907.162227	34.417818
981.103850	90057.995656	34.422836
982.152366	90194.579651	34.427853
982.831801	90341.690526	34.432871
983.619779	90479.621999	34.437888
984.935718	90627.775251	34.442906
985.827884	90778.137468	34.447924
986.830523	90915.897916	34.452941
987.515069	91077.738698	34.457959
988.827655	91222.346673	34.462976
990.028903	91375.299672	34.467994
990.598281	91523.510835	34.473012
992.235623	91666.866036	34.478029
993.260296	91811.750038	34.483047
994.120780	91958.548918	34.488064
995.345677	92087.902133	34.493082
996.164795	92239.702569	34.498100
997.378737	92385.839791	34.503117
998.404168	92531.842457	34.508135
999.033783	92675.195415	34.513152
1000.440932	92809.554996	34.518170
1001.002089	92959.244689	34.523188
1002.261326	93112.374771	34.528205
1003.386994	93246.983138	34.533223
1004.324178	93395.995014	34.538240
1005.497057	93544.894659	34.543258
1006.726177	93688.297905	34.548276
1007.494871	93831.076773	34.553293
1008.347581	93965.642291	34.558311
1009.598020	94120.147682	34.563328
1010.598762	94243.498976	34.568346
1011.212672	94399.879967	34.573364
1012.362845	94543.160109	34.578381
1013.482446	94693.036956	34.583399
1014.278817	94843.674964	34.588416
1015.251587	94975.336037	34.593434
1016.499174	95128.769467	34.598452
1017.863264	95273.908156	34.603469
1018.413276	95416.791930	34.608487
1019.432613	95558.474725	34.613504
1020.466897	95681.446189	34.618522
1021.506158	95813.379254	34.623540
1022.775378	95950.702201	34.628557
1023.209210	96097.841055	34.633575
1024.158138	96236.470329	34.638592
1025.312059	96365.117320	34.643610
1025.985608	96519.192508	34.648628
1027.101417	96653.627008	34.653645
1028.529664	96798.648618	34.658663
1029.157437	96944.620187	34.663680
1030.392952	97074.702407	34.668698
1031.436750	97238.496683	34.673716
1032.227823	97384.001031	34.678733
1033.043259	97537.501191	34.683751
1034.372476	97681.743719	34.688768
1035.431941	97838.312916	34.693786
1036.128942	98006.576959	34.698804
1037.073854	98156.814564	34.703821
1038.207959	98304.208971	34.708839
1039.305838	98467.354575	34.713856
1040.347041	98620.976723	34.718874
1040.990022	98786.895391	34.723892
1042.730574	98949.042749	34.728909
1043.484324	99105.704041	34.733927
1044.643466	99274.434828	34.738944
1045.973437	99422.500958	34.743962
1046.727519	99589.268427	34.748980
1047.946514	99746.189603	34.753997
1048.927174	99899.827330	34.759015
1050.041066	100067.174807	34.764032
1051.128993	100229.747719	34.769050
1052.092874	100390.337778	34.774068
1053.402163	100554.525766	34.779085
1054.538669	100713.226750	34.784103
1055.008285	100875.341864	34.789120
1056.392909	101031.140331	34.794138
1057.415229	101197.379610	34.799156
1058.887221	101358.528786	34.804173
1059.360601	101521.305772	34.809191
1060.662413	101686.375413	34.814208
1062.118198	101845.615101	34.819226
1063.124094	102019.417399	34.824244
1064.296379	102175.013652	34.829261
1065.494965	102342.055224	34.834279
1066.193169	102504.725798	34.839296
1067.587752	102661.836328	34.844314
1068.777446	102813.616590	34.849332
1069.818920	102973.066045	34.854349
1071.064423	103141.321462	34.859367
1072.025947	103303.409536	34.864384
1073.109401	103461.878488	34.869402
1073.998706	103620.594132	34.874420
1075.349360	103784.030988	34.879437
1076.553000	103937.246924	34.884455
1077.640770	104101.322407	34.889472
1079.126401	104244.124023	34.894490
1079.960099	104403.663556	34.899508
1080.664338	104557.822706	34.904525
1082.022581	104720.793803	34.909543
1083.008793	104862.852074	34.914560
1084.517065	105016.760649	34.919578
1085.380187	105179.824160	34.924596
1086.124631	105335.704993	34.929613
1087.639598	105489.170882	34.934631
1088.691028	105650.850450	34.939648
1089.552074	105795.328707	34.944666
1090.641089	105955.786577	34.949684
1091.461648	106102.605576	34.954701
1093.031655	106249.231794	34.959719
1093.486760	106392.026295	34.964736
1094.199680	106541.400042	34.969754
1095.905775	106686.244296	34.974772
1096.578004	106834.928285	34.979789
1097.563318	106986.252117	34.984807
1098.906497	107156.401594	34.989824
1099.832424	107303.171202	34.994842
1100.864354	107455.859284	34.999860
1101.548616	107621.777509	35.004877
1102.874368	107781.712320	35.009895
1103.777423	107954.064971	35.014912
1104.958001	108113.390012	35.019930
1106.021382	108287.912980	35.024948
1107.077911	108453.371121	35.029965
1108.234046	108620.792670	35.034983
1109.299879	108795.609460	35.040000
1110.723178	108959.579641	35.045018
1111.403167	109128.967639	35.050036
1112.586480	109304.415316	35.055053
1114.063654	109480.185619	35.060071
1115.184958	109657.610353	35.065088
1116.272392	109818.111749	35.070106
1117.142024	109995.983392	35.075124
1118.553191	110179.186120	35.080141
1119.781598	110343.637125	35.085159
1120.505957	110520.646449	35.090176
1121.850544	110693.057584	35.095194
1123.614874	110869.829749	35.100212
1124.423956	111052.383035	35.105229
1125.533796	111214.611972	35.110247
1126.388146	111397.350166	35.115264
1127.743572	111570.955954	35.120282
1129.027696	111751.345929	35.125300
1130.256803	111925.721452	35.130317
1131.548550	112097.348680	35.135335
1132.559946	112274.714914	35.140352
1133.843398	112448.780097	35.145370
1135.055037	112626.776193	35.150388
1136.171785	112803.697339	35.155405
1137.144754	112975.429386	35.160423
1138.446635	113154.834386	35.165440
1139.795488	113314.689125	35.170458
1140.810915	113485.376973	35.175476
1141.765106	113677.952795	35.180493
1142.582977	113841.811922	35.185511
1143.491774	114025.455369	35.190528
1145.390125	114202.019987	35.195546
1146.436143	114376.512068	35.200564
1147.281997	114563.985625	35.205581
1148.673392	114735.622407	35.210599
1149.790585	114927.304152	35.215616
1151.106131	115089.886049	35.220634
1151.989407	115273.070453	35.225652
1153.454144	115446.855212	35.230669
1154.678739	115625.865864	35.235687
1155.439841	115794.612976	35.240704
1156.584628	115980.207830	35.245722
1158.109424	116152.185439	35.250740
1158.922697	116339.584308	35.255757
1159.980627	116515.352969	35.260775
1161.320960	116688.275150	35.265792
1162.527236	116872.647179	35.270810
1163.635010	117055.830573	35.275828
1164.843044	117241.447153	35.280845
1165.946177	117417.174912	35.285863
1166.963329	117600.628822	35.290880
1168.003494	117770.317814	35.295898
1169.448622	117943.597195	35.300916
1170.525158	118107.650256	35.305933
1171.737961	118272.646696	35.310951
1172.706985	118450.949778	35.315968
1173.891144	118619.947759	35.320986
1174.888473	118788.963053	35.326004
1176.292518	118962.393037	35.331021
1177.404959	119141.577489	35.336039
1178.122748	119323.196578	35.341056
1179.496978	119494.819745	35.346074
1180.413151	119672.274236	35.351092
1181.612130	119859.465215	35.356109
1182.731098	120051.033203	35.361127
1183.874401	120238.666020	35.366144
1185.197041	120424.546518	35.371162
1186.433444	120625.967849	35.376180
1187.694627	120814.396836	35.381197
1189.083573	121000.168228	35.386215
1189.965659	121196.447076	35.391232
1190.839593	121382.808320	35.396250
1192.044097	121578.873704	35.401268
1193.250323	121779.684129	35.406285
1194.596918	121969.399217	35.411303
1195.507934	122177.970637	35.416320
1197.108834	122382.033265	35.421338
1198.377163	122577.395922	35.426356
1199.510032	122774.924632	35.431373
1200.848212	122980.705985	35.436391
1202.138839	123187.003281	35.441408
1203.206988	123381.563965	35.446426
1204.684383	123571.304300	35.451444
1205.546593	123782.987155	35.456461
1206.551178	123977.852468	35.461479
1208.120484	124182.944153	35.466496
1209.471872	124382.653989	35.471514
1210.844769	124587.106111	35.476532
1211.745535	124788.829498	35.481549
1213.072503	124988.837938	35.486567
1214.028427	125192.089751	35.491584
1215.396939	125403.232440	35.496602
1216.840469	125598.544305	35.501620
1218.234596	125808.391051	35.506637
1219.230260	126004.904082	35.511655
1220.681539	126211.876752	35.516672
1221.756705	126423.172123	35.521690
1223.420926	126628.806813	35.526708
1224.192579	126837.284579	35.531725
1225.574065	127026.079158	35.536743
1226.794835	127241.276212	35.541760
1227.732472	127449.857946	35.546778
1229.267510	127641.282902	35.551796
1230.560936	127852.729017	35.556813
1231.593836	128058.355435	35.561831
1232.940050	128263.616630	35.566848
1234.031790	128471.595720	35.571866
1235.484159	128674.913813	35.576884
1236.562600	128885.865914	35.581901
1237.815637	129083.571205	35.586919
1239.296417	129301.960799	35.591936
1240.150505	129513.039961	35.596954
1241.791054	129714.747621	35.601972
1242.788249	129934.713334	35.606989
1244.001706	130137.682516	35.612007
1245.161078	130343.883885	35.617024
1246.246526	130552.127912	35.622042
1247.597708	130760.153715	35.627060
1249.179518	130977.533695	35.632077
1250.395519	131165.611378	35.637095
1251.702918	131358.459069	35.642112
1253.193928	131553.613537	35.647130
1254.159671	131739.398224	35.652148
1255.233847	131939.758493	35.657165
1256.567845	132128.519743	35.662183
1257.626686	132316.994978	35.667200
1259.023331	132525.897638	35.672218
1260.030874	132715.905257	35.677236
1261.092973	132921.994520	35.682253
1262.371852	133127.733592	35.687271
1263.794184	133335.240299	35.692288
1264.952240	133544.768825	35.697306
1266.408475	133750.762185	35.702324
1267.308183	133964.228659	35.707341
1268.899663	134169.504886	35.712359
1270.099320	134378.929312	35.717376
1271.200711	134599.485884	35.722394
1272.568915	134809.989903	35.727412
1273.966133	135034.334472	35.732429
1275.150484	135240.884822	35.737447
1276.307016	135460.497958	35.742464
1277.551583	135682.598219	35.747482
1279.065717	135888.300452	35.752500
1279.919678	136115.527128	35.757517
1281.867580	136343.878043	35.762535
1282.802244	136555.574721	35.767552
1284.412137	136788.409504	35.772570
1285.921610	136992.366228	35.777588
1286.927021	137220.082260	35.782605
1288.326902	137446.214858	35.787623
1289.566683	137651.815653	35.792640
1290.491109	137882.352127	35.797658
1292.064532	138098.346673	35.802676
1293.251007	138322.410358	35.807693
1294.652806	138546.530241	35.812711
1295.739361	138780.294488	35.817728
1297.265000	139015.793208	35.822746
1298.673496	139228.734989	35.827764
1300.000128	139457.414178	35.832781
1301.353118	139678.577480	35.837799
1302.719761	139903.864152	35.842816
1303.517160	140135.167583	35.847834
1305.591224	140362.998055	35.852852
1306.672813	140592.634783	35.857869
1308.075084	140810.864011	35.862887
1309.251260	141043.267399	35.867904
1310.373071	141271.251231	35.872922
1312.247878	141495.425147	35.877940
1313.387126	141726.010066	35.882957
1314.891782	141947.413872	35.887975
1316.141903	142177.894731	35.892992
1317.496141	142406.710499	35.898010
1318.903677	142621.038079	35.903028
1320.689139	142850.232608	35.908045
1321.623100	143074.954463	35.913063
1323.178707	143295.721783	35.918080
1324.212780	143509.159802	35.923098
1325.501841	143728.168552	35.928116
1327.204559	143943.965956	35.933133
1328.310152	144172.346503	35.938151
1329.763597	144397.018378	35.943168
1331.090696	144620.936826	35.948186
1332.261993	144841.898040	35.953204
1333.385635	145070.825584	35.958221
1334.544341	145290.318445	35.963239
1336.668719	145515.499481	35.968256
1337.817263	145734.703927	35.973274
1338.927698	145940.194947	35.978292
1339.958702	146149.633837	35.983309
1341.240456	146358.958175	35.988327
1342.924743	146575.340794	35.993344
1343.873410	146785.099769	35.998362
1344.977869	146995.304828	36.003380
1345.932178	147225.220409	36.008397
1347.334002	147438.947321	36.013415
1348.783461	147657.706641	36.018432
1350.471751	147886.025191	36.023450
1351.448030	148104.340036	36.028468
1352.954224	148342.259423	36.033485
1354.064893	148574.593454	36.038503
1355.736373	148789.717931	36.043520
1356.870243	149023.459206	36.048538
1358.470033	149246.009458	36.053556
1359.800550	149498.825078	36.058573
1361.036077	149721.269308	36.063591
1362.549936	149947.034591	36.068608
1363.717132	150195.994919	36.073626
1365.358408	150426.946501	36.078644
1366.697432	150660.700840	36.083661
1367.795970	150911.020682	36.088679
1369.553414	151130.951846	36.093696
1370.521321	151373.119634	36.098714
1372.254964	151611.868288	36.103732
1373.658104	151859.974160	36.108749
1375.052507	152101.469081	36.113767
1376.440856	152339.170560	36.118784
1377.755856	152576.808369	36.123802
1379.371109	152819.604677	36.128820
1380.497410	153058.898879	36.133837
1381.615894	153306.954170	36.138855
1383.269491	153553.200398	36.143872
1384.352439	153791.438182	36.148890
1386.018861	154043.079513	36.153908
1387.397474	154290.527137	36.158925
1389.132717	154541.474398	36.163943
1390.719094	154784.118582	36.168960
1391.920923	155025.757650	36.173978
1393.388267	155278.362229	36.178996
1394.652915	155532.586440	36.184013
1396.160008	155776.770517	36.189031
1397.477529	156011.819794	36.194048
1398.656898	156270.490962	36.199066
1400.464123	156511.152777	36.204084
1401.925191	156763.967842	36.209101
1403.347941	157011.648586	36.214119
1404.872225	157247.432088	36.219136
1406.322408	157489.372446	36.224154
1408.143603	157732.817185	36.229172
1409.693118	157975.048626	36.234189
1410.795162	158223.647821	36.239207
1412.739489	158454.266882	36.244224
1413.830898	158700.927340	36.249242
1414.702415	158937.479745	36.254260
1416.697140	159178.465626	36.259277
1417.903929	159425.187103	36.264295
1419.273216	159658.211237	36.269312
1420.643104	159904.693272	36.274330
1421.712568	160153.153012	36.279348
1423.413904	160405.425050	36.284365
1424.684785	160649.779976	36.289383
1426.490162	160892.084370	36.294400
1427.725827	161140.179210	36.299418
1429.048339	161370.462061	36.304436
1431.109339	161619.153239	36.309453
1432.283385	161854.920244	36.314471
1433.660419	162087.317336	36.319488
1435.106540	162308.151202	36.324506
1436.410480	162544.687541	36.329524
1438.033880	162774.852145	36.334541
1439.224016	163012.982299	36.339559
1440.962054	163230.942393	36.344576
1442.212551	163456.038554	36.349594
1443.644181	163686.617259	36.354612
1444.776811	163921.420613	36.359629
1445.831167	164156.909948	36.364647
1447.797021	164388.727881	36.369664
1448.910864	164631.878132	36.374682
1450.073103	164882.030084	36.379700
1451.400734	165110.166882	36.384717
1452.653976	165370.831726	36.389735
1454.189531	165609.475722	36.394752
1455.473523	165869.401261	36.399770
1456.902672	166127.121249	36.404788
1458.437306	166381.029391	36.409805
1459.551658	166641.390685	36.414823
1461.318567	166900.190691	36.419840
1462.581287	167164.441314	36.424858
1464.062913	167434.029433	36.429876
1465.816741	167694.967488	36.434893
1467.195145	167973.817158	36.439911
1468.883943	168224.914516	36.444928
1470.320893	168504.722069	36.449946
1471.703860	168757.722931	36.454964
1473.305279	169035.945066	36.459981
1474.862166	169303.776254	36.464999
1476.612214	169566.029509	36.470016
1477.826277	169829.624625	36.475034
1479.605126	170104.534470	36.480052
1480.768437	170361.574922	36.485069
1482.230778	170643.342088	36.490087
1483.798640	170909.196595	36.495104
1485.321279	171188.861299	36.500122
1486.997106	171452.034354	36.505140
1488.525346	171720.983429	36.510157
1490.139876	171998.274988	36.515175
1491.766560	172257.319091	36.520192
1493.040071	172533.599355	36.525210
1494.157675	172809.879613	36.530228
1496.483458	173080.968817	36.535245
1497.550260	173368.445775	36.540263
1499.590524	173634.350067	36.545280
1500.761264	173902.219853	36.550298
1501.803983	174171.583545	36.555316
1503.899419	174439.665954	36.560333
1504.918578	174726.469591	36.565351
1507.002931	174994.822245	36.570368
1508.454143	175274.741318	36.575386
1509.875799	175539.275760	36.580404
1511.580956	175820.071223	36.585421
1512.776986	176090.941082	36.590439
1514.554512	176360.590661	36.595456
1516.065337	176640.301866	36.600474
1517.585446	176899.745894	36.605492
1519.223420	177181.089790	36.610509
1520.759096	177458.133144	36.615527
1522.366051	177720.156582	36.620544
1523.932270	177993.895275	36.625562
1525.346778	178267.810964	36.630580
1526.979584	178541.972722	36.635597
1528.335908	178812.978545	36.640615
1529.880314	179081.771587	36.645632
1531.497028	179358.046401	36.650650
1532.828844	179614.810508	36.655668
1534.469099	179872.060430	36.660685
1535.539178	180138.391131	36.665703
1537.173410	180387.490789	36.670720
1538.640128	180652.414838	36.675738
1540.248855	180911.653683	36.680756
1541.730012	181182.215351	36.685773
1543.046299	181444.346044	36.690791
1544.574011	181704.996688	36.695808
1546.163025	181973.181745	36.700826
1547.590321	182256.784265	36.705844
1549.259859	182524.247130	36.710861
1550.564328	182797.634930	36.715879
1552.527000	183070.869696	36.720896
1553.989831	183342.964331	36.725914
1555.141260	183624.353588	36.730932
1556.942788	183900.282768	36.735949
1558.358777	184183.410133	36.740967
1559.799459	184449.491775	36.745984
1561.249356	184748.438957	36.751002
1562.806741	185032.359365	36.756020
1564.338113	185394.615561	36.761037
1565.777387	185683.432904	36.766055
1567.645506	185974.622270	36.771072
1569.070029	186262.833958	36.776090
1570.533703	186561.962065	36.781108
1571.821575	186858.959578	36.786125
1574.209313	187165.869413	36.791143
1575.210648	187456.868339	36.796160
1576.911224	187754.133941	36.801178
1578.472642	188057.848278	36.806196
1580.410822	188359.142305	36.811213
1581.910278	188662.309212	36.816231
1583.528345	188968.303179	36.821248
1585.106070	189272.272288	36.826266
1586.986475	189569.895611	36.831284
1588.775681	189874.138032	36.836301
1590.212361	190167.692120	36.841319
1591.958417	190468.234420	36.846336
1593.655627	190767.819920	36.851354
1595.218661	191060.416655	36.856372
1596.929492	191358.248883	36.861389
1598.727750	191671.740321	36.866407
1600.086761	191971.686569	36.871424
1601.798047	192266.980892	36.876442
1603.052175	192577.638726	36.881460
1605.142356	192854.739006	36.886477
1606.910605	193165.927457	36.891495
1608.599361	193466.333710	36.896512
1610.127818	193758.535831	36.901530
1611.513445	194063.182082	36.906548
1613.435992	194355.958895	36.911565
1614.784019	194660.866428	36.916583
1616.625101	194964.071815	36.921600
1618.029896	195257.211052	36.926618
1619.510635	195567.865961	36.931636
1621.367984	195867.946454	36.936653
1622.971911	196168.905505	36.941671
1624.691079	196472.590529	36.946688
1626.145020	196772.736093	36.951706
1627.641804	197081.613737	36.956724
1629.629513	197385.792106	36.961741
1630.873513	197692.119637	36.966759
1632.712623	197991.419983	36.971776
1634.528355	198294.839682	36.976794
1636.174695	198598.286501	36.981812
1637.393886	198897.863472	36.986829
1639.324351	199208.557381	36.991847
1640.625290	199496.412401	36.996864
1642.562741	199790.188621	37.001882
1643.821445	200077.213034	37.006900
1645.849121	200366.911848	37.011917
1647.078359	200651.706495	37.016935
1648.759306	200938.767946	37.021952
1650.027915	201230.644647	37.026970
1651.335880	201534.353178	37.031988
1652.988344	201829.320718	37.037005
1654.948572	202126.526812	37.042023
1656.561899	202438.622736	37.047040
1658.257994	202731.781384	37.052058
1659.585176	203055.811534	37.057076
1661.473618	203352.319618	37.062093
1663.211929	203667.624216	37.067111
1664.495132	203980.536504	37.072128
1666.538342	204290.942509	37.077146
1667.870686	204614.263249	37.082164
1669.724643	204916.977425	37.087181
1671.171863	205239.950967	37.092199
1672.998025	205565.558424	37.097216
1674.753562	205874.233699	37.102234
1676.211703	206212.956860	37.107252
1677.941668	206536.192995	37.112269
1679.953358	206857.353279	37.117287
1681.429174	207176.337019	37.122304
1683.249972	207508.146595	37.127322
1684.982688	207840.249870	37.132340
1687.079126	208156.343501	37.137357
1688.846531	208483.818875	37.142375
1690.030793	208806.584737	37.147392
1692.000371	209132.911596	37.152410
1693.510630	209455.652681	37.157428
1695.043564	209781.794670	37.162445
1697.060033	210125.262702	37.167463
1698.639019	210457.241086	37.172480
1700.507017	210796.770270	37.177498
1702.402281	211131.392727	37.182516
1704.640683	211464.082016	37.187533
1706.219430	211782.445710	37.192551
1707.723649	212121.398278	37.197568
1710.060343	212448.662312	37.202586
1711.261194	212783.827130	37.207604
1713.038361	213103.913963	37.212621
1714.904145	213435.672913	37.217639
1716.518846	213767.268245	37.222656
1718.855730	214094.381436	37.227674
1720.542609	214415.804593	37.232692
1722.085909	214734.202046	37.237709
1724.014466	215060.490848	37.242727
1725.632577	215388.022478	37.247744
1727.414899	215708.009144	37.252762
1728.676978	216039.991857	37.257780
1730.952058	216364.245949	37.262797
1732.289453	216690.120434	37.267815
1734.009976	217030.339185	37.272832
1736.287985	217343.695225	37.277850
1737.802656	217677.367019	37.282868
1739.736045	217996.493259	37.287885
1741.872271	218318.407776	37.292903
1743.469684	218638.933359	37.297920
1745.501232	218962.414245	37.302938
1747.053376	219284.700115	37.307956
1748.825754	219602.582189	37.312973
1750.653862	219928.508749	37.317991
1752.375733	220248.278900	37.323008
1754.442041	220553.337158	37.328026
1755.737937	220871.141886	37.333044
1757.337921	221180.312574	37.338061
1759.363727	221485.834751	37.343079
1760.602951	221782.487073	37.348096
1762.690189	222083.401668	37.353114
1764.144564	222391.477699	37.358132
1765.847077	222694.586578	37.363149
1767.371749	222990.661013	37.368167
1768.997797	223301.403189	37.373184
1770.788073	223614.126635	37.378202
1772.593831	223931.293413	37.383220
1774.042145	224245.188225	37.388237
1775.928742	224567.677270	37.393255
1777.623888	224884.886838	37.398272
1779.557899	225211.407742	37.403290
1781.415454	225545.079161	37.408308
1783.179732	225856.130128	37.413325
1784.999312	226187.749737	37.418343
1786.525842	226522.285841	37.423360
1788.324606	226839.098072	37.428378
1789.776962	227172.350101	37.433396
1791.765448	227507.525104	37.438413
1793.246914	227844.735501	37.443431
1795.068244	228185.576232	37.448448
1797.107743	228533.165623	37.453466
1798.757258	228879.926803	37.458484
1800.227169	229227.859165	37.463501
1802.308009	229571.834396	37.468519
1803.394263	229925.694880	37.473536
1805.952285	230281.763699	37.478554
1807.747387	230630.889436	37.483572
1809.490782	230980.785224	37.488589
1811.676357	231337.267490	37.493607
1813.653542	231698.558121	37.498624
1815.204925	232051.633492	37.503642
1817.256573	232405.163856	37.508660
1819.379309	232764.119316	37.513677
1820.844331	233120.459244	37.518695
1822.582146	233474.012623	37.523712
1824.467083	233822.868418	37.528730
1826.197845	234193.620792	37.533748
1827.977207	234562.993455	37.538765
1830.191062	234915.150255	37.543783
1832.236304	235284.429889	37.548800
1834.211709	235636.801217	37.553818
1836.309494	236000.762586	37.558836
1837.615061	236356.565965	37.563853
1839.714188	236705.843097	37.568871
1841.414429	237071.923316	37.573888
1843.597560	237425.454403	37.578906
1845.266836	237780.615147	37.583924
1847.398849	238137.227310	37.588941
1849.388512	238497.240020	37.593959
1850.724464	238862.384498	37.598976
1853.198147	239224.937172	37.603994
1855.179071	239574.940987	37.609012
1856.878354	239927.706611	37.614029
1859.181043	240284.594331	37.619047
1860.810969	240639.783218	37.624064
1862.668765	240985.485939	37.629082
1864.822443	241338.458048	37.634100
1866.749971	241682.446901	37.639117
1868.666907	242029.967983	37.644135
1870.100114	242383.025945	37.649152
1872.213670	242730.972509	37.654170
1874.221176	243081.754894	37.659188
1875.732581	243427.838595	37.664205
1877.748063	243776.129160	37.669223
1879.522596	244123.847207	37.674240
1881.552136	244474.319117	37.679258
1883.426157	244795.347420	37.684276
1885.214653	245132.519430	37.689293
1887.056631	245454.263007	37.694311
1888.516002	245787.675012	37.699328
1890.394730	246111.520216	37.704346
1892.153780	246452.479625	37.709364
1893.942112	246791.884289	37.714381
1896.247769	247123.078565	37.719399
1897.944057	247471.412720	37.724416
1900.038287	247799.107917	37.729434
1901.515109	248144.452231	37.734452
1903.149924	248491.955764	37.739469
1905.240008	248846.195206	37.744487
1906.974943	249202.445473	37.749504
1908.927480	249554.749001	37.754522
1910.980039	249901.727080	37.759540
1912.500503	250273.072144	37.764557
1914.680342	250616.802727	37.769575
1916.231705	250993.323336	37.774592
1918.346934	251351.541607	37.779610
1920.259601	251713.905866	37.784628
1922.498842	252087.953831	37.789645
1924.700745	252445.647967	37.794663
1926.310242	252825.228630	37.799680
1928.079243	253188.881922	37.804698
1930.270243	253561.181029	37.809716
1931.859846	253937.485114	37.814733
1934.020036	254320.557321	37.819751
1935.701039	254695.879832	37.824768
1938.033801	255075.392173	37.829786
1940.158793	255440.076236	37.834804
1941.802026	255827.162343	37.839821
1943.983053	256203.342306	37.844839
1945.747767	256587.155848	37.849856
1948.029040	256967.585309	37.854874
1949.709218	257347.853691	37.859892
1951.757114	257734.464406	37.864909
1954.074114	258116.129485	37.869927
1956.010710	258499.199149	37.874944
1957.702575	258881.289888	37.879962
1959.808072	259267.734392	37.884980
1961.593932	259645.413722	37.889997
1963.726808	260032.461078	37.895015
1965.887778	260420.798177	37.900032
1967.735465	260801.893148	37.905050
1970.092432	261185.218578	37.910068
1971.934208	261579.951723	37.915085
1974.157897	261955.319798	37.920103
1975.755526	262350.494824	37.925120
1978.042542	262730.574729	37.930138
1979.984720	263125.032658	37.935156
1982.036230	263515.484310	37.940173
1984.314577	263902.266921	37.945191
1986.082634	264282.371730	37.950208
1987.913839	264659.290371	37.955226
1989.983227	265052.171852	37.960244
1991.839765	265444.145367	37.965261
1994.525528	265822.602366	37.970279
1996.094175	266204.432989	37.975296
1998.172185	266588.900124	37.980314
1999.917105	266974.103645	37.985332
2002.097357	267364.926819	37.990349
2004.201645	267743.619830	37.995367
2005.967055	268133.311073	38.000384
2007.749799	268526.375980	38.005402
2009.711386	268909.886955	38.010420
2011.983024	269303.024509	38.015437
2013.640496	269679.417644	38.020455
2015.609938	270059.443116	38.025472
2017.660644	270438.082811	38.030490
2019.719870	270802.319122	38.035508
2021.209522	271179.341840	38.040525
2023.265692	271543.727991	38.045543
2024.821504	271925.410310	38.050560
2026.985341	272308.214899	38.055578
2028.912798	272694.762759	38.060596
2030.343766	273087.380253	38.065613
2032.500194	273486.866574	38.070631
2034.760105	273883.312606	38.075648
2036.609747	274284.849488	38.080666
2038.658720	274695.953123	38.085684
2040.211383	275109.697397	38.090701
2042.324128	275507.809452	38.095719
2044.172080	275919.370135	38.100736
2046.142487	276341.779039	38.105754
2048.338892	276762.347246	38.110772
2050.144482	277205.627339	38.115789
2052.219010	277618.210408	38.120807
2054.165214	278066.314182	38.125824
2056.548234	278502.208073	38.130842
2058.809353	278932.277676	38.135860
2060.668935	279371.473683	38.140877
2062.714655	279806.066940	38.145895
2064.617996	280250.279143	38.150912
2066.698228	280691.108934	38.155930
2069.277041	281126.296708	38.160948
2071.078970	281584.255096	38.165965
2072.916963	282021.965872	38.170983
2075.651382	282475.760446	38.176000
2077.482887	282926.544575	38.181018
2079.834053	283374.502021	38.186036
2081.652800	283834.043133	38.191053
2084.029023	284282.981185	38.196071
2086.148046	284726.192329	38.201088
2088.278283	285176.838986	38.206106
2090.643846	285621.351580	38.211124
2092.822981	286071.959251	38.216141
2094.963982	286526.302548	38.221159
2097.181951	286981.011589	38.226176
2099.291833	287435.048827	38.231194
2101.777161	287881.432007	38.236212
2103.416492	288334.724078	38.241229
2105.821518	288780.656588	38.246247
2108.172703	289231.494960	38.251264
2110.253288	289682.169353	38.256282
2112.671527	290125.627447	38.261300
2114.666361	290573.769789	38.266317
2116.796177	291021.202251	38.271335
2119.231862	291466.247710	38.276352
2121.167558	291918.299725	38.281370
2123.181264	292355.686113	38.286388
2125.528119	292806.143818	38.291405
2127.674047	293241.065699	38.296423
2129.680798	293691.214536	38.301440
2132.124932	294136.137509	38.306458
2133.885803	294577.711111	38.311476
2135.981473	295026.921878	38.316493
2138.004419	295475.125020	38.321511
2140.420741	295928.797870	38.326528
2142.909294	296369.888611	38.331546
2144.981620	296811.548841	38.336564
2147.410240	297255.079395	38.341581
2149.332765	297693.912751	38.346599
2151.441567	298133.652886	38.351616
2153.247700	298585.368987	38.356634
2155.592217	299011.051497	38.361652
2157.817873	299437.231679	38.366669
2159.488192	299860.753665	38.371687
2162.074448	300281.158843	38.376704
2163.980282	300693.619730	38.381722
2166.385574	301110.848099	38.386740
2167.583187	301540.701309	38.391757
2169.892279	301964.132271	38.396775
2172.381462	302390.527187	38.401792
2174.332269	302829.543272	38.406810
2176.121714	303265.407790	38.411828
2178.150630	303700.012731	38.416845
2180.220947	304151.716882	38.421863
2182.601570	304605.754685	38.426880
2184.412299	305049.368535	38.431898
2186.713943	305499.374673	38.436916
2188.709948	305965.898757	38.441933
2190.709135	306421.350783	38.446951
2193.358089	306885.428910	38.451968
2195.163105	307357.122781	38.456986
2197.684014	307817.176339	38.462004
2199.957088	308287.925101	38.467021
2202.005357	308755.277894	38.472039
2204.341068	309226.667775	38.477056
2206.383812	309707.337932	38.482074
2208.717477	310180.774779	38.487092
2211.326213	310669.189722	38.492109
2213.295940	311138.689149	38.497127
2215.442418	311620.491401	38.502144
2217.810666	312108.878390	38.507162
2219.891452	312585.554153	38.512180
2222.185238	313070.364125	38.517197
2224.345566	313559.276068	38.522215
2226.798158	314044.380933	38.527232
2229.000280	314537.159028	38.532250
2231.760214	315015.632278	38.537268
2233.584028	315509.347301	38.542285
2235.895104	315994.529664	38.547303
2238.318907	316487.810179	38.552320
2240.749830	316980.754220	38.557338
2242.856967	317471.002659	38.562356
2245.090328	317970.894691	38.567373
2247.285715	318458.580603	38.572391
2249.962020	318957.859168	38.577408
2251.990059	319453.883716	38.582426
2254.187486	319941.121284	38.587444
2256.469534	320452.903990	38.592461
2258.450307	320941.128386	38.597479
2261.059350	321436.886873	38.602496
2263.648995	321939.519225	38.607514
2266.007908	322431.448167	38.612532
2268.192421	322923.677738	38.617549
2270.547948	323420.771956	38.622567
2273.093216	323909.507922	38.627584
2275.213082	324404.495793	38.632602
2278.031582	324884.042982	38.637620
2280.270032	325394.985468	38.642637
2282.320493	325886.236439	38.647655
2284.472338	326372.416501	38.652672
2287.109930	326862.016043	38.657690
2289.417230	327351.838876	38.662708
2291.936786	327847.559388	38.667725
2293.815002	328337.995377	38.672743
2296.156119	328813.993029	38.677760
2298.646362	329306.680703	38.682778
2300.800473	329797.816440	38.687796
2303.139819	330288.790161	38.692813
2305.161742	330774.073820	38.697831
2307.268382	331254.340404	38.702848
2309.441340	331718.379923	38.707866
2311.993666	332179.411715	38.712884
2314.397211	332652.155952	38.717901
2316.439910	333115.184096	38.722919
2318.762419	333587.472698	38.727936
2321.057568	334060.469928	38.732954
2323.466353	334526.873361	38.737972
2326.089861	335005.134317	38.742989
2327.969030	335462.400775	38.748007
2330.282916	335936.664884	38.753024
2332.161343	336423.623096	38.758042
2334.530490	336905.145988	38.763060
2336.710777	337398.461413	38.768077
2339.113601	337889.325684	38.773095
2341.420095	338380.832462	38.778112
2343.745275	338878.721316	38.783130
2346.271273	339384.738908	38.788148
2348.531570	339873.645344	38.793165
2350.649020	340380.498945	38.798183
2353.500791	340889.766660	38.803200
2355.689799	341393.804632	38.808218
2358.100718	341903.608485	38.813236
2360.511996	342408.433998	38.818253
2362.873954	342932.787876	38.823271
2365.123901	343435.899110	38.828288
2367.224200	343945.873675	38.833306
2369.874028	344468.409276	38.838324
2372.541380	344993.622241	38.843341
2374.616936	345517.347396	38.848359
2377.152051	346028.516070	38.853376
2379.416326	346555.264006	38.858394
2381.702738	347085.829253	38.863412
2384.708884	347606.688342	38.868429
2386.750885	348140.698288	38.873447
2389.878836	348656.982906	38.878464
2391.756977	349191.686125	38.883482
2394.254043	349717.130341	38.888500
2396.596257	350245.100524	38.893517
2399.046082	350781.209641	38.898535
2401.519278	351310.460474	38.903552
2403.898285	351843.368369	38.908570
2406.352545	352368.649506	38.913588
2408.910676	352917.357661	38.918605
2411.397668	353449.588069	38.923623
2413.652508	353989.172742	38.928640
2416.306132	354519.356246	38.933658
2418.662797	355052.340596	38.938676
2421.035339	355581.333248	38.943693
2423.471058	356126.430160	38.948711
2426.559050	356653.796975	38.953728
2428.290874	357193.256050	38.958746
2430.880031	357733.788352	38.963764
2433.708040	358261.117618	38.968781
2436.028310	358802.433585	38.973799
2438.840926	359340.367652	38.978816
2440.997824	359875.707883	38.983834
2443.144754	360419.784981	38.988852
2445.829696	360947.520787	38.993869
2447.937997	361500.582442	38.998887
2450.746510	362027.189961	39.003904
2453.045955	362579.010426	39.008922
2455.140338	363119.396764	39.013940
2457.810708	363665.385606	39.018957
2460.217482	364209.656788	39.023975
2462.825856	364741.265223	39.028992
2465.170665	365287.528132	39.034010
2467.570274	365832.479712	39.039028
2470.359453	366376.726526	39.044045
2472.493119	366894.380833	39.049063
2475.186183	367408.491893	39.054080
2477.361350	367929.846138	39.059098
2479.553940	368438.923416	39.064116
2481.990947	368963.157219	39.069133
2484.444890	369482.158743	39.074151
2487.024204	370009.391563	39.079168
2489.350340	370532.169177	39.084186
2491.345674	371056.787750	39.089204
2493.512517	371596.926802	39.094221
2496.228510	372140.288583	39.099239
2499.153822	372679.882484	39.104256
2501.385833	373230.164675	39.109274
2504.171515	373774.674091	39.114292
2506.364086	374321.697581	39.119309
2508.836378	374883.486960	39.124327
2511.537402	375426.076512	39.129344
2514.068779	375994.547076	39.134362
2516.281428	376554.492997	39.139380
2519.052364	377114.238578	39.144397
2521.411863	377681.129682	39.149415
2523.853180	378246.400051	39.154432
2526.342633	378820.263277	39.159450
2528.527076	379397.961265	39.164468
2530.928457	379978.348239	39.169485
2533.433799	380574.334096	39.174503
2536.462192	381157.560338	39.179520
2539.273763	381744.935858	39.184538
2541.287193	382324.596777	39.189556
2544.135058	382920.956432	39.194573
2546.468814	383524.423331	39.199591
2549.516774	384111.404032	39.204608
2552.144488	384709.174737	39.209626
2554.657479	385301.732525	39.214644
2557.408105	385899.835833	39.219661
2560.052459	386498.346762	39.224679
2562.608848	387090.957054	39.229696
2565.231576	387690.430519	39.234714
2567.938419	388288.939542	39.239732
2570.649339	388892.371060	39.244749
2573.248714	389503.274753	39.249767
2575.491999	390090.089568	39.254784
2578.507603	390698.594445	39.259802
2581.162706	391293.570021	39.264820
2583.710982	391896.092453	39.269837
2586.227092	392505.845645	39.274855
2589.015005	393103.135975	39.279872
2591.796788	393704.108580	39.284890
2594.130154	394309.642391	39.289908
2596.627375	394908.958554	39.294925
2599.310981	395516.786593	39.299943
2602.179132	396113.432451	39.304960
2604.476526	396732.275703	39.309978
2607.184338	397341.318807	39.314996
2610.180222	397938.354208	39.320013
2612.749816	398551.943566	39.325031
2615.100056	399146.821804	39.330048
2617.975044	399753.700597	39.335066
2620.653526	400366.364609	39.340084
2623.616137	400956.747602	39.345101
2626.436222	401567.990946	39.350119
2628.756524	402159.860726	39.355136
2631.489511	402763.493837	39.360154
2634.237066	403364.072061	39.365172
2636.969151	403965.345362	39.370189
2639.405118	404564.472878	39.375207
2642.033222	405158.088941	39.380224
2644.880263	405753.274464	39.385242
2647.460336	406325.258769	39.390260
2650.125938	406887.448757	39.395277
2652.971447	407461.690136	39.400295
2655.440657	408023.376115	39.405312
2658.156891	408583.339449	39.410330
2660.553363	409139.847360	39.415348
2663.321992	409711.310052	39.420365
2665.471997	410285.080778	39.425383
2668.054028	410848.548990	39.430400
2670.507594	411432.411378	39.435418
2672.849317	412018.147428	39.440436
2675.967341	412601.925005	39.445453
2678.386282	413196.318440	39.450471
2681.076430	413784.886164	39.455488
2683.827037	414376.564567	39.460506
2686.261165	414973.739147	39.465524
2689.313444	415568.119449	39.470541
2691.718080	416181.956927	39.475559
2694.252673	416785.589805	39.480576
2697.210180	417396.422519	39.485594
2699.753493	418013.978383	39.490612
2702.637638	418627.821348	39.495629
2705.213915	419251.556284	39.500647
2707.841071	419872.432553	39.505664
2710.602477	420493.623255	39.510682
2713.280504	421127.349470	39.515700
2715.790153	421747.682170	39.520717
2718.659017	422393.475772	39.525735
2721.484153	423027.120425	39.530752
2724.322732	423666.911974	39.535770
2727.144439	424307.596155	39.540788
2729.884925	424935.683476	39.545805
2732.684147	425582.499122	39.550823
2735.132181	426227.781691	39.555840
2738.090236	426869.222727	39.560858
2740.663114	427523.341730	39.565876
2743.445772	428170.683153	39.570893
2745.972483	428823.654568	39.575911
2749.192168	429475.434599	39.580928
2751.904759	430134.854406	39.585946
2754.715337	430788.272538	39.590964
2757.633354	431448.879781	39.595981
2760.116827	432104.630176	39.600999
2763.347932	432765.295574	39.606016
2766.343857	433423.852709	39.611034
2768.952176	434077.293390	39.616052
2771.649741	434724.886547	39.621069
2774.413297	435394.934700	39.626087
2777.374232	436059.673374	39.631104
2780.297243	436717.977667	39.636122
2782.998646	437375.586509	39.641140
2785.648498	438033.180668	39.646157
2788.808186	438694.512104	39.651175
2791.576662	439362.196846	39.656192
2794.854283	440013.359143	39.661210
2797.733079	440675.675335	39.666228
2800.530449	441321.411267	39.671245
2803.147536	441981.751929	39.676263
2805.918713	442637.549359	39.681280
2809.263964	443296.213997	39.686298
2811.791221	443953.467786	39.691316
2814.688025	444602.003475	39.696333
2817.676455	445246.057389	39.701351
2820.557100	445899.347819	39.706368
2822.872227	446552.703311	39.711386
2825.892093	447203.551609	39.716404
2828.812782	447846.413229	39.721421
2831.449719	448486.115056	39.726439
2834.206823	449119.766450	39.731456
2837.220869	449729.724284	39.736474
2840.032456	450353.477352	39.741492
2842.502006	450962.216063	39.746509
2845.101148	451580.758996	39.751527
2847.753449	452205.835384	39.756544
2850.595827	452831.667777	39.761562
2853.432767	453470.200626	39.766580
2856.460092	454093.283778	39.771597
2859.376390	454738.118886	39.776615
2861.896376	455374.057711	39.781632
2864.591742	456008.936466	39.786650
2867.160224	456670.361241	39.791668
2869.886855	457319.219065	39.796685
2872.703095	457973.741711	39.801703
2875.048769	458644.614379	39.806720
2878.402012	459308.086705	39.811738
2880.938476	459982.763266	39.816756
2884.153733	460663.867200	39.821773
2886.507040	461343.211734	39.826791
2889.671783	462027.498557	39.831808
2892.790074	462708.485413	39.836826
2895.513776	463406.509607	39.841844
2898.586685	464095.167158	39.846861
2901.776691	464793.565497	39.851879
2904.590105	465485.990358	39.856896
2907.443055	466185.341883	39.861914
2910.308922	466883.249640	39.866932
2913.394223	467583.212329	39.871949
2916.252592	468286.762140	39.876967
2918.922975	469002.769380	39.881984
2921.850502	469704.432199	39.887002
2924.687569	470430.034779	39.892020
2928.117555	471138.870409	39.897037
2931.043550	471862.126162	39.902055
2933.553150	472592.928386	39.907072
2936.901846	473314.540629	39.912090
2939.490796	474043.903571	39.917108
2943.099324	474771.158172	39.922125
2946.114398	475499.884357	39.927143
2948.977777	476230.063169	39.932160
2952.093339	476954.170120	39.937178
2954.691905	477685.584073	39.942196
2958.190645	478403.011864	39.947213
2961.044568	479142.081550	39.952231
2963.745375	479870.656752	39.957248
2967.119161	480603.981894	39.962266
2969.866676	481341.755379	39.967284
2973.062298	482075.745116	39.972301
2976.048923	482808.573961	39.977319
2978.951567	483538.458733	39.982336
2981.646068	484274.993063	39.987354
2984.667905	485020.158015	39.992372
2987.787608	485765.019746	39.997389
2990.993738	486505.549445	40.002407
2993.554232	487245.690925	40.007424
2996.666934	487981.428207	40.012442
2999.713746	488735.325410	40.017460
3002.785714	489475.480153	40.022477
3006.182299	490222.851542	40.027495
3008.817247	490956.051231	40.032512
3012.034925	491701.161222	40.037530
3014.656106	492452.522042	40.042548
3018.102993	493203.061393	40.047565
3021.437394	493946.883151	40.052583
3023.773135	494678.990638	40.057600
3027.277857	495413.195437	40.062618
3030.410253	496148.932526	40.067636
3033.210767	496869.530435	40.072653
3036.505190	497574.912506	40.077671
3038.939840	498282.408814	40.082688
3041.948879	498970.903756	40.087706
3044.976889	499694.498695	40.092724
3047.469133	500395.591497	40.097741
3050.686845	501115.109661	40.102759
3053.835995	501840.743044	40.107776
3056.617160	502555.627489	40.112794
3059.366258	503298.260737	40.117812
3062.575171	504021.912918	40.122829
3065.676221	504757.320202	40.127847
3068.382312	505498.537850	40.132864
3071.326564	506242.044488	40.137882
3074.427320	506991.374227	40.142900
3077.307632	507750.056290	40.147917
3080.560511	508506.274978	40.152935
3083.642914	509268.314958	40.157952
3087.013008	510034.393302	40.162970
3089.965208	510807.788326	40.167988
3092.751191	511565.424119	40.173005
3096.096571	512345.663483	40.178023
3099.246404	513125.386716	40.183040
3102.638935	513899.295426	40.188058
3106.122225	514685.516462	40.193076
3108.679483	515473.748109	40.198093
3111.728794	516251.701403	40.203111
3114.720331	517041.937028	40.208128
3118.096722	517835.686388	40.213146
3121.453699	518625.823397	40.218164
3125.144088	519425.111363	40.223181
3128.035704	520218.445421	40.228199
3130.921737	521016.960870	40.233216
3134.442888	521811.962416	40.238234
3137.036091	522609.072180	40.243252
3140.734255	523420.383973	40.248269
3144.311672	524213.575850	40.253287
3147.220069	525014.814141	40.258304
3150.529526	525809.862033	40.263322
3153.736935	526624.069662	40.268340
3156.627494	527436.970485	40.273357
3160.333030	528244.770841	40.278375
3163.215507	529044.512882	40.283392
3167.005939	529847.881390	40.288410
3170.075851	530657.892477	40.293428
3173.150719	531461.574787	40.298445
3176.360430	532252.882895	40.303463
3179.478877	533073.030423	40.308480
3182.444164	533874.621746	40.313498
3185.750954	534678.921461	40.318516
3188.849010	535503.687199	40.323533
3192.047342	536313.976166	40.328551
3195.210887	537134.861325	40.333568
3198.912152	537936.284184	40.338586
3202.052836	538750.994934	40.343604
3205.043422	539560.105749	40.348621
3208.585437	540378.864802	40.353639
3211.812473	541199.376281	40.358656
3215.018248	542003.428811	40.363674
3217.997414	542821.915936	40.368692
3221.126136	543629.940267	40.373709
3224.530453	544435.310464	40.378727
3227.632216	545267.063314	40.383744
3230.941370	546074.398845	40.388762
3234.588696	546894.770640	40.393780
3237.400162	547705.989735	40.398797
3240.950992	548519.697832	40.403815
3244.242762	549311.878140	40.408832
3247.000006	550084.082177	40.413850
3250.445882	550860.341732	40.418868
3253.287722	551626.969112	40.423885
3256.848696	552400.154025	40.428903
3259.728348	553176.554519	40.433920
3262.734155	553952.835250	40.438938
3266.286979	554723.566664	40.443956
3268.939149	555517.095744	40.448973
3272.285775	556306.654535	40.453991
3275.515337	557102.694769	40.459008
3278.370295	557892.576381	40.464026
3281.472870	558702.862184	40.469044
3285.135458	559505.188336	40.474061
3288.408026	560321.750601	40.479079
3291.333439	561145.024119	40.484096
3294.655936	561968.027698	40.489114
3298.338863	562788.462658	40.494132
3301.257622	563611.464106	40.499149
3304.485422	564440.770320	40.504167
3307.749243	565286.839692	40.509184
3310.953634	566127.548364	40.514202
3314.011099	566972.675740	40.519220
3317.362593	567828.961513	40.524237
3321.290300	568686.845974	40.529255
3324.280679	569544.762887	40.534272
3327.896036	570395.459369	40.539290
3330.794569	571256.416226	40.544308
3334.350538	572133.973071	40.549325
3338.062465	572999.776383	40.554343
3340.885947	573882.467725	40.559360
3344.335236	574754.633812	40.564378
3348.298017	575634.858352	40.569396
3351.393233	576512.748051	40.574413
3354.944166	577392.499025	40.579431
3357.922043	578283.526219	40.584448
3361.379947	579166.954021	40.589466
3365.169893	580059.613117	40.594484
3368.496964	580957.974355	40.599501
3371.795723	581841.764348	40.604519
3375.213198	582735.266152	40.609536
3379.261941	583599.745856	40.614554
3383.662811	584477.751828	40.619572
3387.148191	585355.930524	40.624589
3391.102408	586227.316720	40.629607
3394.430692	587096.381762	40.634624
3398.065746	587955.732880	40.639642
3401.455600	588815.004237	40.644660
3404.424939	589689.015317	40.649677
3408.178102	590545.693446	40.654695
3411.405267	591412.328769	40.659712
3414.958487	592283.789343	40.664730
3418.660092	593150.060097	40.669748
3421.570905	594004.245471	40.674765
3425.447974	594865.254180	40.679783
3428.156063	595736.215110	40.684800
3432.084364	596615.104091	40.689818
3435.602768	597474.358736	40.694836
3438.961096	598339.810021	40.699853
3442.151354	599196.978067	40.704871
3445.341365	600061.714642	40.709888
3448.809593	600936.570035	40.714906
3452.075117	601807.140880	40.719924
3455.475454	602692.741323	40.724941
3458.865882	603560.001413	40.729959
3461.796288	604445.076537	40.734976
3465.473712	605336.396138	40.739994
3468.957267	606214.446699	40.745012
3472.422171	607084.408921	40.750016
3475.611645	607911.387044	40.755021
3478.881417	608692.175837	40.760026
3482.034698	609428.616766	40.765031
3485.091109	610120.716253	40.770036
3487.872584	610745.060730	40.775040
3490.892744	611326.631326	40.780045
3493.158194	611849.792107	40.785050
3495.742353	612321.933243	40.790055
3498.445250	612724.196506	40.795060
3500.654218	613103.975853	40.800064
3503.161194	613416.561167	40.805069
3504.575255	613676.022347	40.810074
3506.693799	613898.227760	40.815079
3508.450611	614083.046637	40.820084
3509.650833	614227.512489	40.825088
3511.545948	614323.384140	40.830093
3513.098959	614395.816493	40.835098
3514.161873	614417.042886	40.840103
3515.102234	614425.092997	40.845108
3516.177573	614384.838740	40.850112
3517.028204	614331.523900	40.855117
3517.783706	614264.278294	40.860122
3518.224786	614151.346184	40.865127
3519.280825	614030.169194	40.870132
3520.069378	613896.836182	40.875136
3520.735251	613727.880595	40.880141
3521.357380	613558.279188	40.885146
3521.699084	613361.375443	40.890151
3522.112511	613157.158271	40.895156
3522.047611	612933.115750	40.900160
3522.570193	612689.479873	40.905165
3522.902955	612452.866732	40.910170
3522.991548	612208.937177	40.915175
3523.442707	611942.347401	40.920180
3523.512299	611674.460362	40.925184
3523.372103	611402.049262	40.930189
3523.288585	611131.471944	40.935194
3522.945288	610845.527944	40.940199
3523.323843	610568.813360	40.945204
3523.074665	610285.738988	40.950208
3523.569903	609994.689667	40.955213
3523.429618	609696.280498	40.960218
3523.145007	609405.536282	40.965223
3523.596906	609099.065885	40.970228
3522.978847	608807.656634	40.975232
3523.194894	608489.452390	40.980237
3523.076455	608195.346956	40.985242
3523.001080	607894.524362	40.990247
3522.750353	607590.119176	40.995252
3522.572822	607296.397295	41.000256
3522.905711	606984.480279	41.005261
3522.184140	606682.822813	41.010266
3521.970938	606384.528541	41.015271
3521.998413	606079.584882	41.020276
3521.460510	605801.533982	41.025280
3521.415164	605487.779789	41.030285
3521.397036	605205.979633	41.035290
3521.160128	604902.743436	41.040295
3521.099397	604612.778971	41.045300
3520.689412	604330.215690	41.050304
3520.546281	604034.894471	41.055309
3520.051291	603753.929815	41.060314
3520.011810	603470.334482	41.065319
3520.137393	603180.350815	41.070324
3519.502959	602916.498122	41.075328
3519.560690	602634.816283	41.080333
3519.170676	602363.805626	41.085338
3519.232968	602094.818999	41.090343
3518.895497	601823.435756	41.095348
3518.341425	601557.684394	41.100352
3518.277657	601293.000684	41.105357
3518.470902	601043.084272	41.110362
3518.011590	600790.260949	41.115367
3517.904799	600524.363308	41.120372
3517.499063	600265.612973	41.125376
3517.377308	600019.174895	41.130381
3517.141646	599774.550770	41.135386
3517.333914	599529.203320	41.140391
3516.624579	599298.257119	41.145396
3516.441105	599057.462439	41.150400
3516.256009	598812.057107	41.155405
3516.043829	598578.063891	41.160410
3516.011083	598356.051999	41.165415
3516.041331	598116.253630	41.170420
3515.656662	597900.895321	41.175424
3515.353134	597663.742102	41.180429
3515.178064	597450.644772	41.185434
3514.726308	597230.727343	41.190439
3515.173213	597011.866458	41.195444
3514.349705	596809.471778	41.200448
3514.035903	596592.874063	41.205453
3513.982764	596398.562413	41.210458
3513.741567	596195.564249	41.215463
3513.601587	595997.803923	41.220468
3512.863179	595801.485424	41.225472
3513.297686	595608.284794	41.230477
3513.065834	595429.355938	41.235482
3512.651141	595233.927744	41.240487
3512.989494	595049.795650	41.245492
3512.617507	594880.644346	41.250496
3512.519684	594684.956210	41.255501
3512.290846	594506.111492	41.260506
3511.935406	594331.790739	41.265511
3511.940863	594162.518931	41.270516
3511.722655	593987.720368	41.275520
3511.373052	593826.161171	41.280525
3511.169917	593657.865518	41.285530
3511.322533	593497.925657	41.290535
3511.179672	593330.366674	41.295540
3510.993683	593178.388303	41.300544
3510.933255	593014.367522	41.305549
3510.469807	592864.982451	41.310554
3510.647552	592708.883525	41.315559
3510.475154	592557.645516	41.320564
3510.353948	592409.603050	41.325568
3510.388601	592252.618243	41.330573
3509.691484	592109.870972	41.335578
3509.729444	591962.849343	41.340583
3509.749163	591828.752162	41.345588
3509.765554	591705.674083	41.350592
3509.570634	591556.729705	41.355597
3509.395708	591414.041814	41.360602
3509.160666	591295.606935	41.365607
3509.137406	591151.489215	41.370612
3509.015701	591024.517537	41.375616
3508.609114	590887.068767	41.380621
3508.760295	590767.515677	41.385626
3508.730789	590651.596490	41.390631
3508.627827	590522.912665	41.395636
3508.316464	590404.429805	41.400640
3508.306856	590272.271621	41.405645
3508.071136	590154.325271	41.410650
3507.755809	590047.261733	41.415655
3507.830155	589938.282503	41.420660
3507.643403	589820.124441	41.425664
3507.893868	589715.774809	41.430669
3507.238490	589609.110791	41.435674
3507.653025	589495.965565	41.440679
3507.178052	589400.193584	41.445684
3507.100153	589303.406717	41.450688
3507.475854	589192.017995	41.455693
3507.406694	589089.966956	41.460698
3507.425718	588987.800960	41.465703
3506.928895	588872.035922	41.470708
3507.049202	588785.434896	41.475712
3506.717823	588680.815498	41.480717
3506.758272	588590.768077	41.485722
3506.890088	588488.128773	41.490727
3506.597038	588390.615772	41.495732
3506.471425	588303.748696	41.500736
3506.545092	588205.725731	41.505741
3506.504514	588121.549750	41.510746
3506.129031	588038.828526	41.515751
3506.334236	587945.593118	41.520756
3505.463269	587864.401197	41.525760
3505.984254	587775.674963	41.530765
3506.140160	587701.637395	41.535770
3506.063029	587614.657001	41.540775
3506.422420	587537.629953	41.545780
3505.936806	587450.060651	41.550784
3506.088320	587358.632624	41.555789
3505.529353	587279.041251	41.560794
3505.726928	587201.936897	41.565799
3505.827279	587122.090964	41.570804
3505.817120	587048.626157	41.575808
3505.896071	586962.718647	41.580813
3505.693767	586889.633603	41.585818
3505.265513	586801.649194	41.590823
3505.416574	586732.066000	41.595828
3505.283152	586665.182951	41.600832
3505.258239	586585.452897	41.605837
3505.532315	586514.145144	41.610842
3505.411008	586443.099200	41.615847
3505.159472	586358.541618	41.620852
3504.768419	586294.753697	41.625856
3504.895305	586227.275979	41.630861
3505.200791	586162.075339	41.635866
3504.736317	586098.548336	41.640871
3505.079941	586031.235995	41.645876
3504.875172	585972.679491	41.650880
3504.517928	585894.499896	41.655885
3504.723107	585828.360685	41.660890
3504.706405	585765.363172	41.665895
3504.899865	585699.976809	41.670900
3504.464421	585642.958193	41.675904
3504.387085	585580.821136	41.680909
3504.312410	585526.452013	41.685914
3504.488692	585470.990849	41.690919
3504.965588	585407.613386	41.695924
3504.170702	585355.761821	41.700928
3504.197108	585287.692550	41.705933
3504.234307	585225.084472	41.710938
3504.570779	585171.200651	41.715943
3504.338902	585103.170610	41.720948
3504.047461	585046.076243	41.725952
3504.459968	584993.683348	41.730957
3503.946657	584936.222108	41.735962
3503.779777	584886.525689	41.740967
3504.556946	584825.503849	41.745972
3504.203253	584777.740847	41.750976
3504.357157	584728.645177	41.755981
3504.236709	584675.080968	41.760986
3503.461982	584619.563664	41.765991
3503.889755	584568.920721	41.770996
3503.385826	584523.235221	41.776000
3503.856434	584466.319452	41.781005
3504.089221	584416.508295	41.786010
3503.892481	584374.182700	41.791015
3503.835671	584315.493941	41.796020
3503.526524	584275.491340	41.801024
3503.677023	584222.734713	41.806029
3503.624533	584175.473390	41.811034
3503.811591	584128.124289	41.816039
3504.234855	584071.665020	41.821044
3503.692511	584039.116851	41.826048
3503.806165	583980.650290	41.831053
3503.782296	583933.734346	41.836058
3503.693123	583885.675464	41.841063
3504.406772	583833.029442	41.846068
3503.565519	583791.905180	41.851072
3503.741008	583740.646188	41.856077
3503.636591	583692.538715	41.861082
3503.268866	583640.562113	41.866087
3503.285010	583589.527844	41.871092
3502.913678	583553.492562	41.876096
3503.368693	583514.671098	41.881101
3503.743757	583470.848993	41.886106
3503.000669	583435.823912	41.891111
3503.478215	583390.331169	41.896116
3502.923362	583356.629930	41.901120
3503.387779	583312.091397	41.906125
3503.489663	583273.675204	41.911130
3503.347634	583245.824537	41.916135
3503.164993	583195.370958	41.921140
3503.095564	583171.519256	41.926144
3503.683655	583116.082078	41.931149
3503.433219	583072.957754	41.936154
3503.474735	583029.637225	41.941159
3503.663003	582978.122025	41.946164
3503.075078	582936.403498	41.951168
3503.345528	582885.426474	41.956173
3502.930660	582852.704458	41.961178
3503.228211	582814.707273	41.966183
3503.700263	582781.946661	41.971188
3503.005022	582741.096434	41.976192
3503.343383	582694.770314	41.981197
3503.338237	582648.798503	41.986202
3503.116118	582617.098464	41.991207
3503.009723	582572.946986	41.996212
3503.246296	582543.481197	42.001216
3502.900106	582504.280088	42.006221
3503.415043	582460.783045	42.011226
3503.482567	582429.137455	42.016231
3503.378770	582374.556737	42.021236
3502.993445	582337.717499	42.026240
3503.339268	582288.681209	42.031245
3503.596918	582255.451200	42.036250
3503.026016	582211.972521	42.041255
3503.318092	582170.965830	42.046260
3503.226141	582128.464802	42.051264
3503.256642	582093.214233	42.056269
3503.238935	582050.550890	42.061274
3502.992826	582025.821872	42.066279
3503.031551	581978.486722	42.071284
3503.109512	581946.035927	42.076288
3503.186188	581904.811238	42.081293
3503.131017	581864.659891	42.086298
3503.289846	581830.140482	42.091303
3503.767183	581775.465955	42.096308
3502.992125	581740.691160	42.101312
3503.102065	581701.867133	42.106317
3503.421097	581668.024107	42.111322
3503.372480	581619.999141	42.116327
3503.212138	581575.551278	42.121332
3502.963317	581540.543168	42.126336
3502.908864	581502.446085	42.131341
3503.137975	581466.961916	42.136346
3502.921596	581442.979032	42.141351
3503.077411	581398.781869	42.146356
3502.815166	581363.574740	42.151360
3502.887917	581326.710655	42.156365
3502.996770	581289.188986	42.161370
3502.593625	581255.708298	42.166375
3503.112856	581219.325599	42.171380
3502.709024	581181.983994	42.176384
3503.004647	581143.479965	42.181389
3502.753560	581116.493362	42.186394
3502.453631	581078.132349	42.191399
3502.682050	581049.265548	42.196404
3502.624564	581030.321173	42.201408
3502.784492	580995.347721	42.206413
3503.091153	580963.560271	42.211418
3502.696875	580933.286271	42.216423
3502.706541	580891.717294	42.221428
3502.780532	580866.333940	42.226432
3502.430621	580835.451034	42.231437
3502.474704	580802.701332	42.236442
3502.382706	580769.020103	42.241447
3502.536236	580731.138564	42.246452
3502.377838	580714.215123	42.251456
3502.477284	580671.076864	42.256461
3502.602686	580652.805252	42.261466
3501.996939	580622.312746	42.266471
3502.745833	580588.148511	42.271476
3502.202379	580569.179033	42.276480
3502.560219	580537.984082	42.281485
3502.167478	580515.982351	42.286490
3502.710443	580492.329990	42.291495
3502.993208	580460.344262	42.296500
3502.453379	580428.888188	42.301504
3502.994825	580400.422060	42.306509
3502.759316	580371.074438	42.311514
3502.731819	580335.777199	42.316519
3502.785932	580300.416945	42.321524
3502.509368	580269.420706	42.326528
3502.814288	580227.151204	42.331533
3502.392326	580201.643282	42.336538
3502.524624	580178.305179	42.341543
3502.612657	580155.375107	42.346548
3502.545934	580127.855823	42.351552
3502.735636	580095.281851	42.356557
3502.418222	580056.117707	42.361562
3502.315284	580025.996265	42.366567
3502.635855	580003.029527	42.371572
3502.898150	579980.573310	42.376576
3502.423740	579944.793089	42.381581
3502.625006	579922.246003	42.386586
3502.839681	579887.711820	42.391591
3502.935487	579862.322761	42.396596
3503.063468	579836.276709	42.401600
3502.780571	579779.554900	42.406605
3502.652344	579744.171235	42.411610
3502.174841	579718.069121	42.416615
3502.730021	579690.050355	42.421620
3502.497187	579658.844987	42.426624
3502.825546	579645.604869	42.431629
3502.800226	579607.697314	42.436634
3502.438874	579577.013282	42.441639
3502.272245	579540.782463	42.446644
3502.439741	579522.953745	42.451648
3502.743163	579490.661113	42.456653
3502.710697	579458.320600	42.461658
3502.762950	579437.149830	42.466663
3502.815776	579390.403211	42.471668
3502.911758	579360.299017	42.476672
3502.473396	579330.077681	42.481677
3502.818976	579297.226261	42.486682
3502.632322	579275.741490	42.491687
3502.561530	579233.677398	42.496692
3502.272787	579220.934443	42.501696
3502.737613	579173.821611	42.506701
3502.679041	579151.815082	42.511706
3502.296233	579109.949750	42.516711
3502.434083	579085.103994	42.521716
3502.575452	579067.178332	42.526720
3502.644100	579036.776637	42.531725
3502.193818	579003.346668	42.536730
3502.056023	578992.335112	42.541735
3502.612408	578953.180934	42.546740
3502.500660	578922.355774	42.551744
3502.812913	578892.467261	42.556749
3503.388209	578866.098260	42.561754
3502.755350	578836.608101	42.566759
3502.578633	578797.868890	42.571764
3503.179118	578768.235892	42.576768
3502.633752	578726.043470	42.581773
3502.789295	578699.840000	42.586778
3502.594574	578666.569674	42.591783
3502.921876	578639.737390	42.596788
3502.468717	578605.955614	42.601792
3502.640753	578574.683914	42.606797
3502.215381	578535.932513	42.611802
3502.126582	578509.816947	42.616807
3502.716318	578489.463098	42.621812
3502.406815	578465.889561	42.626816
3502.818951	578436.034365	42.631821
3502.573262	578402.620762	42.636826
3502.311771	578367.654781	42.641831
3502.482213	578331.718408	42.646836
3502.339320	578308.218798	42.651840
3502.461038	578284.226390	42.656845
3502.643957	578248.638874	42.661850
3502.806294	578230.658439	42.666855
3502.541022	578197.146974	42.671860
3502.102929	578165.518125	42.676864
3502.196358	578151.861581	42.681869
3502.554490	578123.568772	42.686874
3502.581661	578103.703402	42.691879
3502.364361	578064.115366	42.696884
3502.138675	578040.427517	42.701888
3502.028008	578003.079550	42.706893
3502.201863	577993.472775	42.711898
3502.057185	577966.562198	42.716903
3502.131209	577935.003101	42.721908
3501.764308	577923.273978	42.726912
3502.025982	577900.312125	42.731917
3501.911758	577877.057902	42.736922
3501.952082	577860.550451	42.741927
3502.629983	577827.893540	42.746932
3501.922037	577811.603305	42.751936
3501.926291	577785.220720	42.756941
3501.819723	577778.065074	42.761946
3502.178291	577754.134814	42.766951
3502.373817	577721.252067	42.771956
3502.335531	577697.935444	42.776960
3502.077450	577677.963444	42.781965
3501.885124	577649.504709	42.786970
3502.003813	577625.461206	42.791975
3501.704277	577600.279276	42.796980
3501.465632	577600.767959	42.801985
3501.798604	577573.932235	42.806989
3501.675559	577562.214767	42.811994
3501.768241	577543.943178	42.816999
3502.520809	577523.361496	42.822004
3501.796842	577512.941685	42.827009
3502.151016	577495.180864	42.832013
3502.078831	577469.862783	42.837018
3502.198438	577447.473941	42.842023
3502.558086	577412.658656	42.847028
3502.507112	577401.631957	42.852033
3502.369752	577370.555732	42.857037
3502.002919	577340.367976	42.862042
3502.202494	577333.414975	42.867047
3502.267102	577295.385194	42.872052
3502.360353	577270.743012	42.877057
3502.321676	577249.080731	42.882061
3502.212750	577222.212932	42.887066
3502.124799	577196.144324	42.892071
3502.511722	577165.236361	42.897076
3502.255708	577142.002776	42.902081
3502.258936	577108.947661	42.907085
3502.139297	577087.799312	42.912090
3501.904069	577070.982663	42.917095
3502.424317	577044.768464	42.922100
3502.407684	577029.622987	42.927105
3502.455046	577002.529593	42.932109
3502.407013	576975.150090	42.937114
3502.407968	576947.512065	42.942119
3502.266868	576916.936761	42.947124
3502.167051	576903.258747	42.952129
3502.076874	576884.262275	42.957133
3502.213477	576855.800261	42.962138
3502.272165	576842.699313	42.967143
3502.586154	576811.952259	42.972148
3502.190808	576788.187962	42.977153
3501.592209	576751.263220	42.982157
3501.999335	576720.952800	42.987162
3502.080569	576709.001863	42.992167
3502.325725	576682.428541	42.997172
3502.069520	576673.539957	43.002177
3501.687762	576633.069676	43.007181
3502.202927	576622.254672	43.012186
3501.873975	576605.301492	43.017191
3502.294133	576581.208623	43.022196
3501.913185	576557.441585	43.027201
3502.146210	576535.936096	43.032205
3502.264881	576510.184722	43.037210
3502.019012	576491.964346	43.042215
3502.032094	576465.376630	43.047220
3502.411065	576454.733241	43.052225
3502.107951	576426.238557	43.057229
3501.899395	576390.104400	43.062234
3501.696547	576379.200762	43.067239
3502.026019	576355.874019	43.072244
3502.354327	576342.730338	43.077249
3502.027468	576318.101579	43.082253
3501.864896	576290.337013	43.087258
3501.861654	576270.222338	43.092263
3501.935303	576243.775116	43.097268
3502.105703	576230.605828	43.102273
3502.139428	576215.953008	43.107277
3501.753095	576192.487014	43.112282
3501.511506	576169.198995	43.117287
3501.982905	576166.516794	43.122292
3501.640852	576141.739534	43.127297
3501.940828	576119.821480	43.132301
3501.952641	576096.644186	43.137306
3502.255233	576083.454060	43.142311
3502.249973	576050.798464	43.147316
3502.017423	576039.096523	43.152321
3501.726925	576018.524668	43.157325
3501.797238	575998.749154	43.162330
3502.159030	575980.583443	43.167335
3501.706380	575950.154539	43.172340
3501.637831	575935.015703	43.177345
3501.881832	575919.476836	43.182349
3502.082728	575895.918421	43.187354
3501.767521	575884.630553	43.192359
3502.173191	575870.320451	43.197364
3502.028994	575858.153030	43.202369
3502.182328	575829.384818	43.207373
3502.126298	575804.913252	43.212378
3501.957789	575778.552959	43.217383
3502.341445	575755.918809	43.222388
3502.056968	575723.305914	43.227393
3502.019271	575699.684057	43.232397
3501.854006	575676.433251	43.237402
3501.529338	575661.384250	43.242407
3502.069236	575641.233706	43.247412
3501.782720	575623.168771	43.252417
3501.677463	575611.647146	43.257421
3501.895551	575583.369837	43.262426
3501.966330	575570.516345	43.267431
3501.750221	575546.871893	43.272436
3502.148541	575542.896663	43.277441
3501.940291	575517.495120	43.282445
3501.962825	575498.177689	43.287450
3501.868317	575477.373541	43.292455
3501.811573	575457.817604	43.297460
3501.701659	575440.778256	43.302465
3501.791686	575419.092326	43.307469
3501.470257	575408.908611	43.312474
3501.527818	575389.334686	43.317479
3502.130469	575371.933006	43.322484
3501.576761	575359.528065	43.327489
3501.791928	575340.581583	43.332493
3501.738588	575329.051552	43.337498
3501.780694	575313.342747	43.342503
3502.044633	575299.806581	43.347508
3501.370660	575275.781637	43.352513
3501.292991	575259.690146	43.357517
3501.299735	575255.374694	43.362522
3501.274367	575243.739869	43.367527
3502.087626	575214.315083	43.372532
3502.057945	575206.945107	43.377537
3501.249705	575185.348987	43.382541
3501.764242	575167.057755	43.387546
3501.806488	575170.261833	43.392551
3501.592583	575143.957318	43.397556
3501.665784	575129.748422	43.402561
3501.435258	575108.764186	43.407565
3501.820519	575087.282303	43.412570
3501.706336	575096.229982	43.417575
3501.837248	575054.720685	43.422580
3501.603823	575056.111677	43.427585
3501.462129	575029.344094	43.432589
3501.515603	575013.582927	43.437594
3501.196330	575007.813304	43.442599
3501.616589	574999.218985	43.447604
3501.638519	574989.834072	43.452609
3501.764647	574967.489444	43.457613
3501.887085	574941.182043	43.462618
3501.274470	574932.297628	43.467623
3501.971300	574916.736760	43.472628
3501.864615	574903.709577	43.477633
3502.136285	574877.328530	43.482637
3502.155841	574857.859963	43.487642
3502.086179	574844.074391	43.492647
3502.198643	574818.520797	43.497652
3502.135982	574802.075124	43.502657
3501.663043	574763.368285	43.507661
3501.897481	574748.632012	43.512666
3501.899954	574738.898746	43.517671
3502.185133	574713.418253	43.522676
3501.822881	574699.377229	43.527681
3501.963903	574677.782242	43.532685
3502.003112	574655.651265	43.537690
3501.937141	574641.463511	43.542695
3502.032344	574619.022689	43.547700
3501.558919	574596.118847	43.552705
3501.813600	574585.392793	43.557709
3501.922579	574562.448005	43.562714
3501.870091	574553.576064	43.567719
3502.224365	574519.906596	43.572724
3502.502892	574509.477764	43.577729
3502.172604	574489.962912	43.582733
3502.071611	574458.571932	43.587738
3502.078866	574438.402177	43.592743
3501.959169	574405.157658	43.597748
3501.858811	574377.729847	43.602753
3501.581799	574362.470975	43.607757
3501.741425	574358.632991	43.612762
3501.170720	574345.326507	43.617767
3501.729062	574322.310983	43.622772
3501.438047	574312.372375	43.627777
3501.488492	574300.925412	43.632781
3501.722455	574278.412051	43.637786
3501.423690	574263.909016	43.642791
3501.770895	574258.335845	43.647796
3501.352523	574233.516144	43.652801
3501.365914	574220.268714	43.657805
3502.032267	574212.438077	43.662810
3501.432441	574199.788204	43.667815
3501.646826	574184.151240	43.672820
3501.521704	574183.568706	43.677825
3501.801934	574158.388768	43.682829
3501.420555	574150.320504	43.687834
3501.699395	574127.047248	43.692839
3501.789388	574104.556048	43.697844
3501.858725	574102.437945	43.702849
3501.395497	574075.718367	43.707853
3501.696950	574063.930891	43.712858
3501.380726	574059.916334	43.717863
3501.254484	574031.036731	43.722868
3501.497344	574025.630276	43.727873
3501.965507	574020.690322	43.732877
3501.403758	573989.470414	43.737882
3501.202198	573974.249394	43.742887
3501.590635	573976.948136	43.747892
3501.377261	573972.265224	43.752897
3501.750642	573935.279631	43.757901
3501.798575	573921.875934	43.762906
3501.479009	573906.221713	43.767911
3501.527655	573887.900907	43.772916
3501.457861	573900.555400	43.777921
3501.718097	573875.227440	43.782925
3501.732540	573852.898071	43.787930
3501.375408	573844.324064	43.792935
3501.512231	573825.889027	43.797940
3501.507160	573809.432906	43.802945
3501.634927	573809.111859	43.807949
3501.502576	573784.597671	43.812954
3501.288662	573761.802086	43.817959
3501.786791	573760.620360	43.822964
3501.826692	573740.594778	43.827969
3501.712915	573719.940925	43.832973
3501.854877	573708.679752	43.837978
3501.643970	573688.592939	43.842983
3501.547506	573676.064483	43.847988
3501.801329	573664.434560	43.852993
3501.733415	573646.282107	43.857997
3502.046223	573630.980214	43.863002
3501.581354	573611.033314	43.868007
3501.789756	573595.145602	43.873012
3502.139751	573570.906768	43.878017
3501.589417	573552.628884	43.883021
3501.792483	573536.942623	43.888026
3501.387101	573528.024696	43.893031
3501.616667	573520.412393	43.898036
3501.583113	573504.211156	43.903041
3501.745818	573484.617497	43.908045
3501.957020	573477.961360	43.913050
3501.695386	573456.376817	43.918055
3501.558835	573443.754021	43.923060
3501.607309	573417.053241	43.928065
3501.717112	573405.545919	43.933069
3501.745616	573398.717595	43.938074
3501.381336	573380.008943	43.943079
3501.911668	573353.684264	43.948084
3501.558611	573349.173456	43.953089
3501.775826	573329.621184	43.958093
3502.000616	573314.984908	43.963098
3501.550114	573296.841530	43.968103
3501.760968	573282.157214	43.973108
3501.798138	573274.574824	43.978113
3501.970774	573248.205468	43.983117
3502.050253	573224.058360	43.988122
3501.912371	573218.460164	43.993127
3502.150262	573195.944041	43.998132
3501.655606	573163.155901	44.003137
3501.634531	573154.277952	44.008141
3501.593852	573136.622190	44.013146
3501.165852	573117.973243	44.018151
3501.433853	573116.375841	44.023156
3501.671539	573091.651777	44.028161
3501.393116	573073.982907	44.033165
3501.630747	573062.455253	44.038170
3501.274678	573056.991440	44.043175
3501.277502	573035.214222	44.048180
3501.518250	573031.413286	44.053185
3501.786462	573030.267432	44.058189
3501.816186	573004.421620	44.063194
3501.426424	572994.798351	44.068199
3502.038944	572974.230305	44.073204
3502.005662	572954.867081	44.078209
3501.803049	572937.386855	44.083213
3501.475019	572910.743743	44.088218
3501.607052	572913.231940	44.093223
3501.628529	572882.068332	44.098228
3501.605294	572870.531088	44.103233
3500.999847	572866.511140	44.108237
3501.529548	572861.510891	44.113242
3501.457967	572848.074432	44.118247
3501.471088	572822.280979	44.123252
3501.418611	572829.966353	44.128257
3501.463843	572795.788127	44.133261
3501.528980	572774.151201	44.138266
3501.783072	572783.795801	44.143271
3501.550972	572757.237688	44.148276
3501.767598	572742.351061	44.153281
3501.377242	572727.810195	44.158285
3501.348912	572715.119491	44.163290
3501.163647	572710.933443	44.168295
3501.440253	572696.488984	44.173300
3501.427274	572693.229385	44.178305
3501.323654	572669.711863	44.183309
3501.381585	572659.867786	44.188314
3501.017411	572659.272363	44.193319
3501.389689	572651.536813	44.198324
3501.569851	572630.182702	44.203329
3501.290152	572617.681721	44.208333
3501.647479	572604.077565	44.213338
3500.921895	572603.889889	44.218343
3500.949998	572570.817598	44.223348
3501.337706	572574.971983	44.228353
3501.206132	572568.971048	44.233357
3501.444915	572575.206051	44.238362
3501.415344	572557.146220	44.243367
3501.908221	572529.821913	44.248372
3501.652555	572525.094831	44.253377
3501.441430	572503.701295	44.258381
3501.532597	572484.970145	44.263386
3501.419139	572485.489641	44.268391
3501.728687	572467.978805	44.273396
3501.785278	572448.600668	44.278401
3501.591510	572436.989284	44.283405
3501.772240	572413.627498	44.288410
3501.439395	572403.593391	44.293415
3501.581017	572389.520903	44.298420
3501.405982	572370.981719	44.303425
3501.675759	572367.577464	44.308429
3501.677814	572352.573332	44.313434
3501.425937	572340.268416	44.318439
3501.686052	572322.162925	44.323444
3501.582110	572313.247093	44.328449
3501.386428	572284.524438	44.333453
3501.597105	572274.555788	44.338458
3501.261376	572270.292738	44.343463
3501.442684	572241.410679	44.348468
3501.552434	572238.733929	44.353473
3501.438138	572240.056453	44.358477
3501.316950	572222.010412	44.363482
3501.253441	572214.242333	44.368487
3501.161673	572199.302847	44.373492
3501.500458	572202.712310	44.378497
3501.278135	572198.481685	44.383501
3501.564739	572171.891295	44.388506
3501.517604	572161.912669	44.393511
3501.149913	572154.392825	44.398516
3501.382616	572140.506514	44.403521
3500.954331	572125.920624	44.408525
3501.221435	572120.007669	44.413530
3500.990298	572112.466449	44.418535
3501.596236	572118.142497	44.423540
3501.813874	572095.125555	44.428545
3501.484363	572075.807142	44.433549
3501.568794	572074.037571	44.438554
3501.548389	572058.584933	44.443559
3501.536305	572036.958677	44.448564
3501.685169	572034.576852	44.453569
3501.450804	572007.314802	44.458573
3501.408408	571996.582569	44.463578
3501.517185	571994.106639	44.468583
3501.782588	571955.826772	44.473588
3501.327545	571951.130619	44.478593
3501.323439	571944.958882	44.483597
3501.456540	571921.754078	44.488602
3501.517373	571916.575809	44.493607
3501.502557	571907.394817	44.498612
3501.759931	571896.515264	44.503617
3501.914992	571870.396372	44.508621
3501.748884	571862.794638	44.513626
3501.872335	571844.057387	44.518631
3501.868647	571820.472305	44.523636
3501.639954	571804.550061	44.528641
3501.407345	571789.481508	44.533645
3501.552778	571776.511681	44.538650
3501.674284	571769.517293	44.543655
3501.949203	571748.849272	44.548660
3501.212496	571727.285527	44.553665
3501.654654	571715.021982	44.558669
3501.898161	571694.358773	44.563674
3501.481343	571683.885511	44.568679
3501.540011	571662.096935	44.573684
3501.551602	571666.410821	44.578689
3501.378843	571649.425775	44.583693
3501.422939	571627.990693	44.588698
3501.245413	571620.541130	44.593703
3501.544370	571617.232458	44.598708
3501.479472	571595.663805	44.603713
3501.125121	571576.298243	44.608717
3501.481964	571565.402825	44.613722
3501.586986	571559.966570	44.618727
3501.806080	571545.379096	44.623732
3501.661510	571549.667255	44.628737
3501.492193	571528.415899	44.633741
3501.762444	571505.740828	44.638746
3501.488857	571500.213181	44.643751
3501.854847	571478.878048	44.648756
3501.505249	571457.855478	44.653761
3501.498981	571453.390063	44.658765
3501.555020	571435.114334	44.663770
3501.175323	571421.071966	44.668775
3501.733000	571414.209910	44.673780
3501.815137	571404.812620	44.678785
3501.369906	571384.858731	44.683789
3501.261977	571379.556050	44.688794
3501.148310	571363.916313	44.693799
3501.591917	571339.156256	44.698804
3501.235734	571334.795681	44.703809
3501.393076	571335.523816	44.708813
3501.311553	571309.691549	44.713818
3501.190777	571303.035858	44.718823
3501.269200	571289.724662	44.723828
3501.338582	571284.896063	44.728833
3500.974489	571275.417872	44.733837
3501.158439	571250.848771	44.738842
3501.269547	571248.071207	44.743847
3501.501744	571243.919724	44.748852
3501.339455	571253.982011	44.753857
3501.574724	571233.218887	44.758861
3502.008907	571212.474815	44.763866
3501.413286	571208.001068	44.768871
3501.697283	571182.261925	44.773876
3501.529778	571171.347733	44.778881
3501.336469	571157.075161	44.783885
3501.938020	571124.410877	44.788890
3501.681089	571125.705642	44.793895
3501.647932	571110.454454	44.798900
3501.407948	571094.432612	44.803905
3501.078131	571093.179318	44.808909
3501.847676	571097.073816	44.813914
3501.395789	571069.492228	44.818919
3501.554383	571049.393170	44.823924
3501.778374	571038.969691	44.828929
3501.285563	571023.438945	44.833933
3501.713542	571005.505868	44.838938
3501.647116	571005.315476	44.843943
3502.060896	570984.373437	44.848948
3501.894317	570964.626179	44.853953
3501.504168	570940.949137	44.858957
3501.649447	570925.669807	44.863962
3501.590409	570922.918763	44.868967
3501.569324	570894.867917	44.873972
3501.942514	570886.177496	44.878977
3501.368873	570869.153584	44.883981
3501.592740	570854.614670	44.888986
3501.532861	570850.057027	44.893991
3501.618401	570821.638027	44.898996
3501.077290	570805.863601	44.904001
3501.326843	570800.153457	44.909005
3501.801096	570796.114533	44.914010
3501.381240	570784.737554	44.919015
3501.596359	570777.226057	44.924020
3501.499860	570756.915429	44.929025
3501.359947	570744.039226	44.934029
3501.354494	570734.454331	44.939034
3501.214993	570717.261949	44.944039
3501.299603	570695.065976	44.949044
3501.188231	570698.395707	44.954049
3501.247819	570685.237314	44.959053
3501.359259	570668.708250	44.964058
3501.036125	570682.008171	44.969063
3501.795213	570666.682726	44.974068
3501.471554	570642.643359	44.979073
3501.110715	570632.762624	44.984077
3501.368249	570633.776267	44.989082
3501.244296	570623.005305	44.994087
3501.105149	570600.743754	44.999092
3501.398576	570591.915017	45.004097
3501.529481	570592.296020	45.009101
3501.723041	570564.210807	45.014106
3501.456949	570554.164629	45.019111
3501.715334	570546.495654	45.024116
3501.562659	570521.626297	45.029121
3501.552328	570509.582767	45.034125
3501.725063	570491.738978	45.039130
3501.374814	570483.362100	45.044135
3501.153658	570473.308825	45.049140
3501.363005	570465.998780	45.054145
3501.514107	570457.392942	45.059149
3501.735840	570440.143672	45.064154
3501.291409	570438.657279	45.069159
3501.553632	570427.675197	45.074164
3501.320762	570405.277352	45.079169
3501.110924	570395.272428	45.084173
3501.307951	570385.555210	45.089178
3501.222019	570385.116914	45.094183
3501.433625	570361.946860	45.099188
3501.184219	570345.574118	45.104193
3501.203498	570346.725412	45.109197
3501.235692	570343.859589	45.114202
3501.602496	570328.745587	45.119207
3501.503229	570320.078409	45.124212
3501.338634	570307.707460	45.129217
3501.321798	570287.734867	45.134221
3501.398574	570267.245715	45.139226
3501.289387	570261.842331	45.144231
3501.068222	570250.935648	45.149236
3501.013165	570262.036014	45.154241
3501.050845	570247.324680	45.159245
3501.207768	570231.440335	45.164250
3500.936655	570235.798956	45.169255
3501.118850	570221.717457	45.174260
3501.227547	570239.467415	45.179265
3501.361352	570226.196513	45.184269
3501.397084	570204.910637	45.189274
3501.270423	570195.193671	45.194279
3501.270692	570185.507043	45.199284
3501.270801	570175.268347	45.204289
3501.223520	570156.856159	45.209293
3501.373310	570145.640436	45.214298
3501.426937	570140.914197	45.219303
3501.080170	570131.683292	45.224308
3501.406864	570123.501460	45.229313
3501.219050	570102.601669	45.234317
3501.127437	570101.311024	45.239322
3501.302025	570099.828193	45.244327
3501.224908	570080.015231	45.249332
3501.370762	570067.946820	45.254337
3501.155816	570064.667853	45.259341
3501.381423	570063.227233	45.264346
3501.159112	570066.825439	45.269351
3501.337650	570035.629503	45.274356
3501.441796	570027.582774	45.279361
3501.377427	570016.300024	45.284365
3501.572072	570006.984380	45.289370
3501.072398	569990.349113	45.294375
3501.145741	569979.345940	45.299380
3501.277149	569974.356521	45.304385
3501.221112	569969.095261	45.309389
3501.079254	569956.619997	45.314394
3501.371567	569937.803035	45.319399
3501.429866	569926.350448	45.324404
3501.504100	569928.396622	45.329409
3501.722711	569916.517440	45.334413
3501.624265	569900.973702	45.339418
3501.548903	569893.356468	45.344423
3501.402624	569864.419235	45.349428
3501.380215	569848.612585	45.354433
3501.227295	569845.173286	45.359437
3501.603162	569837.234519	45.364442
3500.903947	569821.834783	45.369447
3501.100925	569807.850847	45.374452
3501.228063	569820.127744	45.379457
3501.068083	569795.910435	45.384461
3500.685481	569790.298616	45.389466
3500.833018	569800.163169	45.394471
3501.145440	569791.732378	45.399476
3501.243095	569767.876262	45.404481
3501.210969	569768.885076	45.409485
3501.377270	569751.693628	45.414490
3501.690013	569755.710200	45.419495
3501.409247	569727.897855	45.424500
3501.498635	569719.702644	45.429505
3501.190883	569717.943829	45.434509
3501.387188	569707.925002	45.439514
3500.902537	569694.398828	45.444519
3501.282506	569686.107975	45.449524
3501.317225	569677.318980	45.454529
3500.773050	569676.400185	45.459533
3501.143161	569674.736160	45.464538
3501.072600	569662.751346	45.469543
3501.263661	569640.536690	45.474548
3501.033778	569634.850728	45.479553
3501.076986	569637.002188	45.484557
3501.164561	569634.177722	45.489562
3501.431656	569627.410227	45.494567
3501.228961	569602.245541	45.499572
3501.481027	569605.468580	45.504577
3501.281921	569595.812622	45.509581
3501.205939	569583.326653	45.514586
3500.834787	569564.412031	45.519591
3501.598428	569566.149726	45.524596
3501.602758	569557.064238	45.529601
3501.273349	569553.250904	45.534605
3501.299457	569536.382203	45.539610
3501.314255	569524.685055	45.544615
3501.484855	569515.473156	45.549620
3501.641413	569508.170755	45.554625
3501.363236	569489.141089	45.559629
3501.382386	569476.589940	45.564634
3501.236133	569488.608776	45.569639
3501.158372	569463.976372	45.574644
3501.292469	569449.248942	45.579649
3501.196481	569433.152067	45.584653
3501.145043	569435.268169	45.589658
3501.253864	569434.448040	45.594663
3501.393302	569417.762220	45.599668
3501.446234	569408.317666	45.604673
3501.222112	569394.599830	45.609677
3501.378718	569391.563741	45.614682
3501.232183	569376.227582	45.619687
3501.554348	569357.906933	45.624692
3501.345999	569350.159548	45.629697
3501.362754	569345.890484	45.634701
3501.129513	569326.853524	45.639706
3501.106214	569316.316562	45.644711
3500.805998	569309.085443	45.649716
3500.983543	569317.389730	45.654721
3501.219358	569308.619210	45.659725
3501.351666	569299.212351	45.664730
3501.051471	569289.320971	45.669735
3501.161047	569271.284385	45.674740
3501.461999	569267.472798	45.679745
3500.955270	569262.331863	45.684749
3501.145230	569256.278918	45.689754
3501.279805	569236.230630	45.694759
3501.057524	569212.724538	45.699764
3501.242465	569223.688002	45.704769
3501.312909	569221.970373	45.709773
3501.285577	569224.735262	45.714778
3501.558873	569201.201867	45.719783
3501.520701	569180.277000	45.724788
3501.678534	569179.148029	45.729793
3501.277133	569163.148714	45.734797
3501.564164	569140.064792	45.739802
3501.331765	569141.155163	45.744807
3501.336429	569118.316116	45.749812
3501.690231	569110.882240	45.754817
3501.404285	569085.578853	45.759821
3501.624075	569016.376608	45.764826
3501.414930	568919.483227	45.769831
3501.308680	568757.268577	45.774836
3500.549340	568554.143232	45.779841
3500.402419	568304.887423	45.784845
3500.310312	568007.075390	45.789850
3499.559837	567661.467475	45.794855
3498.960663	567284.599908	45.799860
3498.679817	566854.755455	45.804865
3498.017516	566388.655817	45.809869
3496.960422	565849.295272	45.814874
3496.099033	565294.564812	45.819879
3495.620230	564695.309409	45.824884
3494.296002	564050.760126	45.829889
3493.839396	563370.484626	45.834893
3492.829692	562644.805139	45.839898
3491.254860	561875.121505	45.844903
3490.026076	561064.196008	45.849908
3488.673860	560227.967122	45.854913
3487.277689	559333.110651	45.859917
3485.437013	558415.648060	45.864922
3484.104579	557467.537039	45.869927
3482.294198	556475.608912	45.874932
3480.539571	555457.709739	45.879937
3478.920910	554408.694446	45.884941
3477.165760	553313.418846	45.889946
3475.335598	552192.872341	45.894951
3473.658141	551043.493732	45.899956
3471.900712	549862.194540	45.904961
3469.600042	548629.931663	45.909965
3468.083063	547384.800679	45.914970
3465.518597	546117.629799	45.919975
3463.310872	544819.190172	45.924980
3460.767503	543487.317253	45.929985
3458.284320	542135.471691	45.934989
3455.952203	540753.721882	45.939994
3453.787097	539369.479647	45.944999
3450.909587	537939.553589	45.950004
3448.623314	536507.360992	45.955009
3445.591046	535046.131296	45.960013
3443.087159	533559.180013	45.965018
3440.027804	532054.673761	45.970023
3437.428098	530535.419426	45.975028
3434.579541	529013.357878	45.980033
3431.450665	527465.981026	45.985037
3429.320649	525891.116474	45.990042
3426.300821	524310.763117	45.995047
3423.247996	522711.938489	46.000052
3420.555735	521090.645208	46.005057
3417.162073	519465.638027	46.010061
3414.197681	517819.402054	46.015066
3410.545210	516175.141486	46.020071
3407.578038	514509.453486	46.025076
3404.233409	512838.430161	46.030081
3401.237545	511155.401989	46.035085
3398.183190	509456.949817	46.040090
3394.642807	507770.675027	46.045095
3391.543663	506053.964913	46.050100
3388.075466	504337.862097	46.055105
3385.090418	502618.198440	46.060109
3381.457172	500864.571157	46.065114
3377.810992	499136.119177	46.070119
3374.286877	497379.935336	46.075124
3371.257952	495625.685379	46.080129
3367.968996	493868.541927	46.085133
3364.094293	492093.913709	46.090138
3360.678229	490318.448397	46.095143
3357.097049	488537.749900	46.100148
3353.379491	486759.743354	46.105153
3349.767226	484987.525337	46.110157
3346.771709	483205.004180	46.115162
3342.499011	481410.705511	46.120167
3339.228805	479622.613671	46.125172
3335.644873	477830.173446	46.130177
3331.976727	476037.240863	46.135181
3328.308466	474236.878805	46.140186
3324.401280	472440.397482	46.145191
3320.724557	470646.007235	46.150196
3317.331480	468846.673228	46.155201
3313.485692	467049.995145	46.160205
3309.635033	465246.700243	46.165210
3306.073625	463446.403237	46.170215
3302.135421	461641.673119	46.175220
3298.596811	459847.566655	46.180225
3294.445096	458051.951548	46.185229
3290.663006	456251.942535	46.190234
3287.232820	454462.016786	46.195239
3283.268841	452662.780246	46.200244
3279.569569	450878.960866	46.205249
3275.593636	449085.742170	46.210253
3271.889616	447298.732202	46.215258
3268.289780	445510.922323	46.220263
3264.287131	443731.660056	46.225268
3260.809916	441949.915674	46.230273
3256.858460	440153.183971	46.235277
3253.207689	438375.633648	46.240282
3249.144509	436599.753893	46.245287
3245.451874	434814.835543	46.250292
3242.027431	433046.936906	46.255297
3237.695122	431275.016166	46.260301
3234.008728	429488.644566	46.265306
3229.986128	427723.247693	46.270311
3226.100790	425960.562194	46.275316
3222.497792	424202.240295	46.280321
3218.888716	422459.735978	46.285325
3215.177080	420696.921232	46.290330
3211.049688	418951.361800	46.295335
3207.472863	417194.566690	46.300340
3203.946805	415438.327083	46.305345
3200.181403	413690.601569	46.310349
3196.131881	411939.937829	46.315354
3192.263809	410208.075127	46.320359
3188.570761	408457.329223	46.325364
3184.810039	406727.153879	46.330369
3181.027049	404993.803624	46.335373
3177.227154	403258.749661	46.340378
3173.020101	401529.158082	46.345383
3169.559172	399797.594182	46.350388
3165.563764	398084.914914	46.355393
3161.449382	396364.820356	46.360397
3158.137496	394647.470112	46.365402
3154.502915	392946.950902	46.370407
3150.118386	391241.809603	46.375412
3146.215150	389529.543936	46.380417
3142.425911	387823.716728	46.385421
3138.965826	386134.579130	46.390426
3135.096985	384449.886261	46.395431
3131.337745	382747.316156	46.400436
3127.878581	381064.698001	46.405441
3123.950429	379375.568763	46.410445
3119.945014	377697.517663	46.415450
3115.990888	376020.698851	46.420455
3112.295894	374342.084090	46.425460
3108.392426	372680.137797	46.430465
3104.909156	371017.212604	46.435469
3100.951617	369338.435486	46.440474
3097.066249	367696.588566	46.445479
3093.575172	366019.345738	46.450484
3090.088086	364380.422606	46.455489
3085.653986	362727.630877	46.460493
3082.421051	361078.675526	46.465498
3078.663478	359433.751962	46.470503
3074.559961	357784.574394	46.475508
3070.862293	356148.181173	46.480513
3067.123474	354517.681115	46.485517
3063.454806	352882.840712	46.490522
3059.741639	351256.235525	46.495527
3055.975672	349624.014878	46.500532
3052.047748	348006.940423	46.505537
3048.264603	346392.052482	46.510541
3044.915083	344761.230480	46.515546
3040.719661	343152.354100	46.520551
3037.580615	341531.693724	46.525556
3033.799450	339917.059701	46.530561
3029.652704	338311.513002	46.535565
3025.860688	336712.883381	46.540570
3022.372454	335119.476842	46.545575
3018.477974	333510.348038	46.550580
3015.111031	331909.638965	46.555585
3011.313199	330323.376977	46.560589
3007.276288	328723.860908	46.565594
3003.389577	327133.031961	46.570599
3000.021296	325550.478469	46.575604
2996.152988	323966.720426	46.580609
2992.573305	322395.779746	46.585613
2989.005012	320816.154076	46.590618
2985.328099	319239.921438	46.595623
2981.292245	317657.937615	46.600628
2977.692217	316082.291451	46.605633
2973.858992	314516.498729	46.610637
2970.204630	312954.186613	46.615642
2966.207113	311394.623766	46.620647
2962.819149	309844.431231	46.625652
2959.104981	308297.013592	46.630657
2955.037140	306738.634232	46.635661
2951.498811	305180.021697	46.640666
2947.608383	303647.324530	46.645671
2944.360634	302100.229326	46.650676
2940.468447	300560.977874	46.655681
2936.631874	299028.113306	46.660685
2933.408617	297489.052533	46.665690
2929.606584	295966.610472	46.670695
2926.351601	294419.123079	46.675700
2922.397147	292887.053655	46.680705
2918.482430	291362.677503	46.685709
2914.934666	289829.882152	46.690714
2910.850057	288303.904994	46.695719
2907.477744	286790.152626	46.700724
2903.854427	285262.021261	46.705729
2900.170562	283736.028944	46.710733
2896.540686	282223.106108	46.715738
2892.575751	280714.404483	46.720743
2889.103724	279205.263819	46.725748
2885.443426	277695.460477	46.730753
2881.395142	276181.869338	46.735757
2877.871406	274664.501090	46.740762
2873.742797	273165.888541	46.745767
2870.510724	271675.028154	46.750772
2867.274090	270176.046011	46.755777
2863.197194	268678.036253	46.760781
2859.915277	267185.607550	46.765786
2855.906966	265706.434380	46.770791
2852.217548	264213.005994	46.775796
2848.806097	262727.152203	46.780801
2845.120977	261252.423640	46.785805
2841.288842	259765.908401	46.790810
2837.794220	258290.424668	46.795815
2833.757162	256803.828559	46.800820
2830.417884	255330.934352	46.805825
2826.754737	253853.134268	46.810829
2823.068726	252388.208586	46.815834
2819.315244	250926.284250	46.820839
2815.531023	249454.750092	46.825844
2812.034360	247989.754140	46.830849
2808.252247	246523.924930	46.835853
2804.855087	245067.982188	46.840858
2801.142914	243615.592957	46.845863
2797.844653	242160.327956	46.850868
2794.048014	240704.266154	46.855873
2790.047662	239247.362209	46.860877
2786.609915	237788.249052	46.865882
2783.260831	236348.369752	46.870887
2779.529220	234896.803488	46.875892
2775.708039	233447.283707	46.880897
2771.750114	232009.012829	46.885901
2768.500295	230560.694825	46.890906
2764.896676	229129.315324	46.895911
2761.209876	227683.735103	46.900916
2757.721363	226243.190908	46.905921
2753.769499	224811.097936	46.910925
2750.484085	223373.934427	46.915930
2747.000643	221944.596299	46.920935
2743.333045	220505.788631	46.925940
2739.551269	219078.309375	46.930945
2735.740790	217646.737134	46.935949
2732.048627	216221.109842	46.940954
2728.450986	214796.007039	46.945959
2725.059353	213365.630613	46.950964
2721.287057	211951.364778	46.955969
2717.625506	210529.498488	46.960973
2714.068654	209104.286702	46.965978
2710.668130	207703.635158	46.970983
2706.685939	206272.062984	46.975988
2703.395043	204863.567823	46.980993
2699.503990	203458.563556	46.985997
2696.072690	202047.156464	46.991002
2692.124346	200638.973956	46.996007
2688.749024	199227.988739	47.001012
2685.279419	197829.407720	47.006017
2681.057051	196426.118870	47.011021
2677.966615	195025.162500	47.016026
2673.762826	193632.009048	47.021031
2670.502545	192231.465262	47.026036
2666.833321	190837.800488	47.031041
2663.297536	189454.469972	47.036045
2659.625972	188058.012104	47.041050
2656.146045	186672.720850	47.046055
2652.375593	185285.939785	47.051060
2648.743124	183887.366168	47.056065
2644.890043	182511.636545	47.061069
2641.603487	181128.428311	47.066074
2637.932662	179754.110860	47.071079
2634.383346	178379.209749	47.076084
2630.801022	177008.842179	47.081089
2626.999415	175629.173952	47.086093
2623.324206	174257.376469	47.091098
2619.916426	172883.129109	47.096103
2616.052026	171513.241893	47.101108
2612.634606	170153.391416	47.106113
2608.687052	168786.087375	47.111117
2605.390580	167418.210842	47.116122
2601.984729	166060.013781	47.121127
2598.010887	164701.550378	47.126132
2594.275658	163340.925832	47.131137
2590.746717	161984.599203	47.136141
2587.142105	160630.463899	47.141146
2583.563383	159288.088523	47.146151
2579.939542	157937.158200	47.151156
2576.666089	156588.735821	47.156161
2572.746134	155242.710484	47.161165
2569.032672	153884.911737	47.166170
2565.539108	152537.113661	47.171175
2561.811857	151206.373676	47.176180
2558.385508	149859.876997	47.181185
2554.580937	148531.364813	47.186189
2550.939164	147181.647602	47.191194
2547.393643	145827.063834	47.196199
2543.981665	144437.719070	47.201204
2540.280627	143110.703712	47.206209
2536.460528	141781.592072	47.211213
2533.369728	140449.425177	47.216218
2529.294038	139128.938050	47.221223
2525.483707	137804.260427	47.226228
2522.253703	136488.015362	47.231233
2518.515650	135170.551615	47.236237
2515.168564	133845.800992	47.241242
2511.489045	132538.735029	47.246247
2507.936358	131209.859141	47.251252
2504.505704	129899.996392	47.256257
2500.707824	128581.136351	47.261261
2497.455249	127265.106835	47.266266
2493.536148	125961.713413	47.271271
2489.877439	124655.268077	47.276276
2486.429909	123340.056093	47.281281
2482.487813	122042.426440	47.286285
2479.475969	120735.028528	47.291290
2475.416713	119434.794507	47.296295
2471.668842	118125.781117	47.301300
2468.357536	116826.523233	47.306305
2464.514498	115540.757716	47.311309
2461.193061	114235.615004	47.316314
2457.531267	112942.078898	47.321319
2453.893646	111644.173181	47.326324
2450.314623	110356.323865	47.331329
2446.748145	109070.006814	47.336333
2443.289494	107778.545833	47.341338
2439.311324	106487.582855	47.346343
2435.641049	105208.137454	47.351348
2432.024361	103932.710633	47.356353
2428.122332	102660.465690	47.361357
2424.829512	101375.997341	47.366362
2421.038313	100116.187731	47.371367
2417.341538	98838.999860	47.376372
2414.054625	97574.405989	47.381377
2409.864942	96312.049566	47.386381
2406.337264	95047.123833	47.391386
2403.251057	93803.490908	47.396391
2399.241932	92549.581615	47.401396
2395.778542	91293.579736	47.406401
2392.032723	90037.635835	47.411405
2388.633584	88773.990547	47.416410
2384.705608	87529.348463	47.421415
2381.250487	86294.746782	47.426420
2377.811829	85053.385271	47.431425
2373.597779	83812.630076	47.436429
2370.604239	82564.471459	47.441434
2366.419251	81336.204301	47.446439
2362.933388	80099.307498	47.451444
2359.186353	78880.313196	47.456449
2355.430038	77657.081032	47.461453
2351.870492	76428.893991	47.466458
2348.591333	75213.151090	47.471463
2344.580180	74005.082308	47.476468
2341.204104	72777.590841	47.481473
2337.573563	71564.175924	47.486477
2333.781603	70357.787297	47.491482
2330.205837	69159.558841	47.496487
2326.622057	67958.454032	47.501492
2322.655874	66750.399922	47.506497
2318.949835	65561.848593	47.511501
2315.859100	64369.384820	47.516506
2311.868769	63176.362847	47.521511
2308.268177	61993.681522	47.526516
2304.853964	60811.109791	47.531521
2301.154783	59623.981408	47.536525
2297.436604	58447.720044	47.541530
2293.665103	57268.205313	47.546535
2290.026232	56096.614230	47.551540
2286.624148	54924.814925	47.556545
2282.880777	53764.521113	47.561549
2279.156211	52587.590124	47.566554
2275.519173	51424.267280	47.571559
2272.093786	50263.741401	47.576564
2268.435203	49113.072135	47.581569
2264.570998	47957.431037	47.586573
2261.045756	46801.687502	47.591578
2257.250279	45661.456414	47.596583
2253.480698	44528.102674	47.601588
2249.702537	43394.756837	47.606593
2245.958775	42258.641459	47.611597
2242.656085	41125.641413	47.616602
2238.380903	40004.309164	47.621607
2234.786697	38888.019067	47.626612
2231.111933	37779.654008	47.631617
2227.178234	36672.096370	47.636621
2223.937735	35576.646028	47.641626
2219.832868	34476.062480	47.646631
2216.045578	33377.717520	47.651636
2212.392841	32291.996425	47.656641
2208.367982	31220.396526	47.661645
2204.677062	30147.715734	47.666650
2200.637443	29086.089425	47.671655
2196.651886	28039.109604	47.676660
2191.660567	27005.907277	47.681665
2187.064262	25978.132041	47.686669
2181.946942	25000.861401	47.691674
2176.550770	24048.042412	47.696679
2171.235122	23112.057486	47.701684
2166.382462	22200.529106	47.706689
2161.220768	21323.596573	47.711693
2156.449881	20474.678416	47.716698
2152.357681	19654.308888	47.721703
2147.332756	18850.188971	47.726708
2143.129157	18071.612701	47.731713
2138.778534	17317.531603	47.736717
2134.155894	16576.426423	47.741722
2129.989055	15862.637084	47.746727
2125.911688	15166.231103	47.751732
2121.827190	14486.436551	47.756737
2117.703258	13821.186112	47.761741
2114.110161	13167.701116	47.766746
2109.894769	12538.096561	47.771751
2106.185758	11907.654883	47.776756
2102.526007	11294.001910	47.781761
2098.795927	10697.344717	47.786765
2095.273710	10101.126622	47.791770
2091.399291	9519.863458	47.796775
2087.486100	8935.794606	47.801780
2083.986473	8367.993157	47.806785
2080.300690	7815.962778	47.811789
2076.513456	7251.855113	47.816794
2073.171593	6712.198304	47.821799
2069.856427	6159.956830	47.826804
2066.219133	5625.786890	47.831809
2062.254115	5100.576622	47.836813
2059.053156	4563.995837	47.841818
2055.079661	4050.852118	47.846823
2051.640750	3532.528648	47.851828
2048.244327	3013.320975	47.856833
2044.674763	2517.665723	47.861837
2041.017839	2003.419733	47.866842
2036.935298	1510.938472	47.871847
2033.127728	1021.325895	47.876852
2028.020113	563.600899	47.881857
2020.760255	196.242135	47.886861
2004.445121	97.302021	47.891866
1986.944208	141.663944	47.896871
1977.129518	144.256414	47.901876
1973.270790	135.685044	47.906881
1972.233794	150.356664	47.911885
1972.424129	146.084132	47.916890
1972.644670	145.862922	47.921895
1971.352330	140.392342	47.926900
1969.447820	141.867273	47.931905
1966.096244	136.791690	47.936909
1963.391400	147.013330	47.941914
1960.114206	146.943963	47.946919
1956.698993	143.121730	47.951924
1954.075018	138.928905	47.956929
1950.333238	148.211792	47.961933
1947.376113	143.871777	47.966938
1943.868792	148.625321	47.971943
1940.779753	145.296233	47.976948
1937.939084	142.330090	47.981953
1934.343426	142.402317	47.986957
1931.288281	137.745444	47.991962
1927.683594	131.450275	47.996967
1924.174122	141.598507	48.001972
1921.060380	133.758493	48.006977
1917.785165	132.787135	48.011981
1914.954593	138.364954	48.016986
1911.590916	137.179644	48.021991
1908.288645	135.690490	48.026996
1904.249896	133.762912	48.032001
1900.640081	136.925274	48.037005
1897.008210	136.753237	48.042010
1893.634203	145.130676	48.047015
1890.618887	140.714363	48.052020
1887.665862	135.487853	48.057025
1884.225435	139.487441	48.062029
1881.144898	133.458290	48.067034
1876.794517	138.761405	48.072039
1873.281647	140.114708	48.077044
1870.428461	125.966375	48.082049
1866.686440	139.153493	48.087053
1863.523237	141.148125	48.092058
1860.144795	134.396786	48.097063
1856.643655	141.389384	48.102068
1853.563604	144.285356	48.107073
1849.981513	141.745320	48.112077
1846.251872	132.204655	48.117082
1842.543689	142.140388	48.122087
1838.965687	135.692375	48.127092
1835.556196	128.714947	48.132097
1832.290225	134.421031	48.137101
1829.075067	130.257483	48.142106
1825.501342	134.743032	48.147111
1822.102955	134.531318	48.152116
1819.061645	134.890166	48.157121
1815.221713	144.719972	48.162125
1811.853925	134.657609	48.167130
1807.928777	135.784378	48.172135
1804.765005	127.297324	48.177140
1801.183621	128.484196	48.182145
1797.779861	130.734797	48.187149
1794.726306	133.816467	48.192154
1791.264572	130.330615	48.197159
1787.636290	129.819524	48.202164
1784.111721	123.863062	48.207169
1780.053934	133.704819	48.212173
1777.097006	129.478730	48.217178
1773.414407	127.014567	48.222183
1769.862958	132.945683	48.227188
1766.897204	131.103347	48.232193
1763.183386	135.686771	48.237197
1759.721444	122.431041	48.242202
1756.024032	126.439244	48.247207
1752.816787	130.851641	48.252212
1749.619816	127.779962	48.257217
1745.927319	130.961639	48.262221
1742.371390	125.617557	48.267226
1738.400792	126.061749	48.272231
1735.142864	123.053400	48.277236
1732.121950	119.305590	48.282241
1728.308353	124.183055	48.287245
1725.037459	114.583314	48.292250
1721.265920	127.215080	48.297255
1717.747484	128.534502	48.302260
1714.905562	126.381729	48.307265
1711.002882	125.989542	48.312269
1707.645708	127.033786	48.317274
1703.844435	135.386386	48.322279
1700.482411	135.561337	48.327284
1697.039894	127.032525	48.332289
1693.219123	128.108199	48.337293
1690.069815	126.168061	48.342298
1686.782652	132.602017	48.347303
1683.022544	125.923138	48.352308
1679.676829	122.669113	48.357313
1676.282032	129.126245	48.362317
1672.650020	132.754072	48.367322
1668.902016	127.867196	48.372327
1665.429134	129.714193	48.377332
1662.073184	130.653854	48.382337
1658.242841	132.294201	48.387341
1655.467850	131.826784	48.392346
1652.029850	130.450709	48.397351
1648.182614	129.100718	48.402356
1644.636150	119.417582	48.407361
1640.978812	135.071942	48.412365
1637.757101	120.146133	48.417370
1634.086548	110.640619	48.422375
1630.721836	113.710917	48.427380
1627.826870	114.651208	48.432385
1623.636698	121.118938	48.437389
1620.292657	116.444114	48.442394
1616.641381	119.970566	48.447399
1613.043745	123.020377	48.452404
1609.833419	119.023835	48.457409
1606.026476	127.627291	48.462413
1602.946534	119.604935	48.467418
1599.754087	118.598581	48.472423
1595.943608	126.873555	48.477428
1592.398061	119.746673	48.482433
1588.758422	116.532358	48.487437
1585.033884	111.379251	48.492442
1581.831163	117.657642	48.497447
1578.098245	119.153052	48.502452
1574.670416	112.105834	48.507457
1571.330449	119.440281	48.512461
1568.088442	117.495709	48.517466
1564.596859	113.505240	48.522471
1560.814964	119.883779	48.527476
1557.152512	117.647506	48.532481
1553.217754	114.840072	48.537485
1550.468519	110.591046	48.542490
1547.227458	111.731065	48.547495
1543.516669	108.214686	48.552500
1540.136511	111.891720	48.557505
1535.932212	116.504525	48.562509
1532.922301	119.465535	48.567514
1529.160513	111.401234	48.572519
1525.529246	112.244823	48.577524
1522.397251	109.295935	48.582529
1519.052934	120.120776	48.587533
1515.437569	113.691407	48.592538
1511.744958	108.640904	48.597543
1508.187805	106.049640	48.602548
1504.784867	105.512872	48.607553
1501.552527	117.845152	48.612557
1498.338097	106.113742	48.617562
1494.738984	110.214211	48.622567
1490.985998	111.412229	48.627572
1487.098702	109.881908	48.632577
1483.826675	119.274885	48.637581
1479.992524	113.151865	48.642586
1477.108081	114.552468	48.647591
1473.520017	111.542102	48.652596
1470.534915	109.873735	48.657601
1466.242626	111.624423	48.662605
1462.950880	108.039322	48.667610
1459.111505	116.166992	48.672615
1455.660406	105.693882	48.677620
1452.320738	112.844809	48.682625
1448.846818	112.426741	48.687629
1445.416773	110.249048	48.692634
1441.704893	111.307769	48.697639
1438.335393	124.639158	48.702644
1435.060618	107.858263	48.707649
1431.406717	114.586974	48.712653
1428.632523	114.764917	48.717658
1424.714210	118.089617	48.722663
1420.931264	107.560895	48.727668
1417.433558	110.044622	48.732673
1413.563579	118.955398	48.737677
1410.215324	113.591600	48.742682
1406.861787	121.057932	48.747687
1403.312761	112.761062	48.752692
1399.529531	106.614289	48.757697
1396.324590	122.257991	48.762701
1392.741311	106.041113	48.767706
1389.600104	112.205517	48.772711
1386.091939	114.678237	48.777716
1382.691464	112.843958	48.782721
1378.884301	116.072180	48.787725
1375.250646	118.396864	48.792730
1371.851135	115.860069	48.797735
1368.320585	121.436845	48.802740
1364.963784	116.533155	48.807745
1361.557860	117.243449	48.812749
1358.021981	112.699997	48.817754
1354.281587	116.594833	48.822759
1350.903222	120.774693	48.827764
1347.648002	106.085231	48.832769
1343.823398	115.311634	48.837773
1340.634526	110.052631	48.842778
1337.051210	120.456174	48.847783
1333.124849	116.654078	48.852788
1330.122919	113.067950	48.857793
1326.338941	120.623832	48.862797
1322.745214	111.811963	48.867802
1319.258925	112.509541	48.872807
1315.461055	120.222629	48.877812
1312.446471	110.984740	48.882817
1308.812774	108.430844	48.887821
1305.367975	102.522207	48.892826
1302.544103	114.929793	48.897831
1298.639517	115.050605	48.902836
1295.056496	105.211998	48.907841
1291.230983	109.607408	48.912845
1287.695031	108.949165	48.917850
1284.398666	115.621952	48.922855
1281.098398	112.098363	48.927860
1277.464326	114.866081	48.932865
1273.597455	107.353032	48.937869
1270.499773	115.510188	48.942874
1267.265049	112.422441	48.947879
1263.297081	121.668152	48.952884
1260.178001	107.833795	48.957889
1256.051615	125.070803	48.962893
1252.607638	118.016750	48.967898
1249.074346	118.126912	48.972903
1245.878354	121.461989	48.977908
1242.299457	112.568739	48.982913
1238.613889	122.722557	48.987917
1235.076053	119.906904	48.992922
1232.327604	117.053096	48.997927
1228.606566	113.155627	49.002932
1224.982919	116.782290	49.007937
1221.084821	117.256463	49.012941
1217.820231	118.150329	49.017946
1214.290988	116.114801	49.022951
1210.609027	120.503588	49.027956
1207.394359	111.543841	49.032961
1203.922217	118.943373	49.037965
1200.526517	122.708369	49.042970
1196.910533	124.511484	49.047975
1193.170779	113.232608	49.052980
1189.937339	104.443493	49.057985
1186.305642	119.091000	49.062989
1183.081684	107.503588	49.067994
1179.688290	109.942589	49.072999
1175.647957	111.767851	49.078004
1172.505330	109.811022	49.083009
1168.578478	120.689182	49.088013
1165.026856	116.866457	49.093018
1161.796017	107.656158	49.098023
1158.165743	119.604715	49.103028
1154.918623	105.686046	49.108033
1150.962416	123.817109	49.113037
1148.101945	110.730102	49.118042
1144.505302	112.786476	49.123047
1140.838883	123.101843	49.128052
1137.647069	112.018790	49.133057
1133.749620	114.565196	49.138061
1130.283506	111.143558	49.143066
1126.803954	117.484395	49.148071
1123.248255	118.980699	49.153076
1119.896915	109.979110	49.158081
1116.115481	112.105554	49.163085
1113.300413	102.694140	49.168090
1109.725641	111.792913	49.173095
1105.876266	116.201617	49.178100
1102.176676	112.408412	49.183105
1098.554688	107.774141	49.188109
1095.220861	107.647483	49.193114
1091.755584	105.171711	49.198119
1088.221211	110.053132	49.203124
1084.789741	96.634773	49.208129
1081.614313	104.959170	49.213133
1078.000735	103.196334	49.218138
1074.418419	103.652764	49.223143
1070.652260	99.335314	49.228148
1067.333336	92.726850	49.233153
1063.445194	103.067452	49.238157
1060.433668	109.018647	49.243162
1056.642601	109.817821	49.248167
1053.151559	112.395542	49.253172
1049.805373	104.899153	49.258177
1046.190519	112.431807	49.263181
1042.803969	101.913975	49.268186
1039.077929	107.262025	49.273191
1035.356931	112.137881	49.278196
1032.300037	108.462382	49.283201
1028.806892	115.229327	49.288205
1025.442179	101.243710	49.293210
1021.879063	104.791359	49.298215
1018.095917	101.539631	49.303220
1014.970679	109.337325	49.308225
1011.296665	115.012605	49.313229
1007.712011	117.355057	49.318234
1004.163539	103.009072	49.323239
1000.666482	112.551298	49.328244
997.569536	109.087730	49.333249
994.006471	101.036856	49.338253
990.253951	104.323101	49.343258
986.652066	108.297620	49.348263
982.787382	111.009799	49.353268
979.736416	104.400540	49.358273
975.852556	111.288789	49.363277
972.962215	111.273072	49.368282
969.279028	103.250507	49.373287
965.455029	105.769657	49.378292
962.203318	103.826817	49.383297
958.513954	108.985652	49.388301
955.316801	102.759967	49.393306
952.062894	108.983265	49.398311
948.187622	107.087445	49.403316
944.654676	100.822593	49.408321
940.941505	116.362455	49.413325
937.843457	107.482639	49.418330
934.496151	109.525357	49.423335
930.605227	117.661271	49.428340
927.563248	106.292254	49.433345
923.611242	110.751895	49.438349
919.931209	112.444914	49.443354
916.250752	110.388887	49.448359
913.066154	107.090937	49.453364
910.259717	106.780522	49.458369
906.002284	110.775459	49.463373
902.766206	111.778861	49.468378
898.892992	105.095899	49.473383
895.443314	102.310872	49.478388
892.251571	104.930368	49.483393
888.609978	115.248246	49.488397
885.217549	111.068508	49.493402
881.680363	109.059665	49.498407
877.730708	109.339567	49.503412
874.279007	108.320268	49.508417
871.256918	110.530386	49.513421
867.764789	101.949595	49.518426
864.233078	116.717569	49.523431
860.432996	113.718498	49.528436
857.167516	103.146989	49.533441
853.342281	115.442537	49.538445
849.778544	107.429796	49.543450
847.313283	104.629845	49.548455
843.125020	104.624417	49.553460
839.686264	108.171639	49.558465
835.742649	115.246468	49.563469
832.726982	104.060038	49.568474
829.069994	107.331384	49.573479
825.445780	101.545954	49.578484
822.553696	107.649354	49.583489
818.461430	114.582949	49.588493
814.994535	105.998229	49.593498
811.682615	112.800138	49.598503
807.688247	112.153748	49.603508
804.098191	99.054590	49.608513
801.211416	111.722058	49.613517
797.443465	106.012932	49.618522
794.417409	115.908576	49.623527
790.525378	113.873077	49.628532
787.167204	107.758094	49.633537
783.809839	113.042175	49.638541
779.886913	109.771307	49.643546
776.474678	100.096026	49.648551
772.845111	103.926255	49.653556
769.706791	102.120756	49.658561
765.988439	122.704582	49.663565
762.445600	112.802976	49.668570
759.083134	106.976584	49.673575
755.629532	118.394541	49.678580
752.373844	116.417597	49.683585
748.736753	122.631362	49.688589
745.194881	115.282802	49.693594
741.493216	103.624862	49.698599
737.750916	114.461600	49.703604
734.467345	101.972550	49.708609
730.945995	113.217620	49.713613
727.493472	102.172416	49.718618
723.981955	109.907290	49.723623
720.045753	107.394678	49.728628
717.126842	110.455566	49.733633
713.285576	108.171702	49.738637
710.361005	108.132953	49.743642
706.367315	105.910928	49.748647
702.800989	119.323930	49.753652
699.415772	107.284252	49.758657
695.984990	114.478139	49.763661
692.567491	105.113771	49.768666
689.362957	111.671105	49.773671
685.410448	114.346533	49.778676
682.281998	109.973674	49.783681
678.445703	116.943168	49.788685
674.926556	101.485427	49.793690
671.347993	115.571076	49.798695
667.856616	115.969125	49.803700
664.528771	111.820491	49.808705
660.602059	116.766663	49.813709
657.505193	108.472081	49.818714
654.226152	105.065631	49.823719
650.687857	107.492702	49.828724
646.908970	98.441223	49.833729
643.379965	113.711870	49.838733
640.098235	105.408283	49.843738
636.586913	103.822600	49.848743
633.012218	111.776210	49.853748
629.287491	104.892949	49.858753
625.608868	107.152179	49.863757
622.226497	106.470136	49.868762
618.574397	101.717400	49.873767
615.448649	109.534263	49.878772
611.913895	96.815690	49.883777
608.530451	100.683362	49.888781
605.215038	97.738215	49.893786
601.519251	95.906188	49.898791
597.438589	108.744858	49.903796
594.413741	98.268662	49.908801
590.589064	104.325190	49.913805
587.006127	104.649022	49.918810
584.164438	104.148073	49.923815
580.689469	103.822239	49.928820
577.126116	99.925666	49.933825
573.313678	96.998264	49.938829
569.729758	102.279927	49.943834
566.371899	98.746649	49.948839
562.554107	105.010920	49.953844
559.380606	97.332671	49.958849
555.911880	96.781240	49.963853
552.347508	90.021605	49.968858
548.583954	102.200009	49.973863
544.879185	110.151872	49.978868
542.249495	96.703115	49.983873
538.224237	108.799127	49.988877
534.611348	104.565476	49.993882
531.061385	100.476998	49.998887
527.809897	103.311616	50.003892
524.449825	100.914505	50.008897
520.749030	104.619938	50.013901
517.345595	95.550849	50.018906
514.114984	97.031261	50.023911
510.158175	97.299785	50.028916
506.744608	98.555751	50.033921
503.230425	103.158954	50.038925
499.589268	101.562025	50.043930
496.313367	104.229633	50.048935
492.837283	98.936849	50.053940
489.610133	95.591941	50.058945
485.874618	104.988164	50.063949
482.420610	98.214436	50.068954
478.952202	93.091303	50.073959
474.741755	109.914576	50.078964
471.571357	106.389939	50.083969
468.261910	94.851047	50.088973
464.944093	96.943092	50.093978
461.189711	100.783492	50.098983
457.751550	100.331716	50.103988
454.308005	101.750587	50.108993
450.863708	109.734451	50.113997
447.031305	100.121970	50.119002
443.607861	107.229362	50.124007
439.802813	107.167258	50.129012
436.863825	98.794258	50.134017
432.869510	105.067243	50.139021
429.447080	97.333127	50.144026
426.546662	103.580306	50.149031
423.264301	101.006545	50.154036
419.642469	86.919138	50.159041
415.820999	95.734050	50.164045
412.090276	95.356593	50.169050
408.601404	87.939785	50.174055
404.744009	98.418156	50.179060
401.837774	97.073152	50.184065
398.346472	100.033963	50.189069
394.940454	96.960721	50.194074
391.723539	92.478448	50.199079
387.922081	107.219185	50.204084
383.960503	92.299149	50.209089
380.454615	92.664779	50.214093
377.044058	90.924212	50.219098
374.038537	93.036974	50.224103
369.870246	101.096301	50.229108
366.684321	96.621837	50.234113
362.855564	97.620187	50.239117
359.413112	95.694795	50.244122
356.750293	98.782113	50.249127
352.791901	105.153907	50.254132
349.103024	101.175854	50.259137
345.513948	99.868228	50.264141
341.638450	97.548764	50.269146
338.622618	93.696245	50.274151
334.737776	97.250242	50.279156
331.765311	94.634302	50.284161
328.039594	102.697087	50.289165
324.673562	93.774091	50.294170
321.100241	98.332836	50.299175
317.710592	93.545453	50.304180
314.384789	85.191974	50.309185
310.735520	93.992603	50.314189
307.231868	91.665528	50.319194
303.314506	94.152107	50.324199
300.192908	100.933846	50.329204
296.417935	104.457993	50.334209
292.915431	99.922418	50.339213
290.025198	92.437195	50.344218
285.963767	96.306780	50.349223
282.323259	93.156422	50.354228
279.423569	91.171349	50.359233
275.416700	100.474106	50.364237
272.008530	92.070270	50.369242
268.582798	86.734899	50.374247
264.965769	110.634422	50.379252
261.801565	101.550118	50.384257
258.112847	104.785519	50.389261
254.853392	91.894289	50.394266
251.107686	96.128884	50.399271
247.408021	92.497422	50.404276
243.879396	85.570977	50.409281
240.336881	90.896889	50.414285
236.808754	97.815097	50.419290
233.261578	92.992315	50.424295
229.821689	99.972635	50.429300
226.596489	86.433807	50.434305
223.009618	91.681251	50.439309
219.440718	93.069227	50.444314
216.218752	101.714365	50.449319
212.474965	95.669533	50.454324
209.142490	92.695580	50.459329
205.533012	86.123509	50.464333
202.037594	87.000102	50.469338
198.584543	85.604790	50.474343
194.811079	92.213429	50.479348
191.649671	87.336561	50.484353
187.912740	90.187231	50.489357
184.063801	83.715961	50.494362
181.052361	84.557870	50.499367
177.192248	102.209046	50.504372
174.045156	92.647537	50.509377
170.455208	95.063896	50.514381
166.776996	92.131470	50.519386
163.534782	90.073548	50.524391
160.039976	99.179066	50.529396
156.985090	87.122715	50.534401
153.072107	100.216840	50.539405
149.330851	92.846017	50.544410
145.773035	90.866020	50.549415
142.104304	88.346576	50.554420
139.069798	89.258553	50.559425
135.736528	94.266980	50.564429
131.862568	94.693537	50.569434
128.373502	90.462818	50.574439
124.812850	96.857809	50.579444
121.732839	94.802965	50.584449
117.829476	87.514505	50.589453
114.664589	89.551077	50.594458
111.048504	84.084246	50.599463
107.077966	96.491369	50.604468
104.054644	92.855250	50.609473
100.312802	103.347264	50.614477
96.969159	100.011270	50.619482
93.761574	93.619894	50.624487
89.970904	95.877906	50.629492
86.610699	93.452518	50.634497
82.449987	88.640508	50.639501
79.018712	88.475708	50.644506
75.675849	88.819081	50.649511
71.810992	88.456457	50.654516
69.211413	85.677787	50.659521
65.418351	90.258398	50.664525
61.966861	87.850487	50.669530
58.604302	90.256574	50.674535
54.380919	98.014609	50.679540
51.221306	90.302767	50.684545
47.978553	89.146653	50.689549
44.738038	87.907931	50.694554
41.323162	88.427116	50.699559
37.189417	98.271865	50.704564
33.793285	92.207452	50.709569
30.295046	97.887175	50.714573
26.944871	92.698259	50.719578
23.238862	88.507906	50.724583
19.518052	94.140245	50.729588
16.413083	87.112726	50.734593
12.856820	97.654784	50.739597
9.164000	100.618841	50.744602
5.947966	94.140241	50.749607
2.141461	93.192697	50.754612