Thu Aug 25 12:55:14 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
0.420614	103.397573	0.000000
0.088991	92.028156	0.005005
0.110567	100.427657	0.010010
0.191171	88.449483	0.015014
0.074594	75.834655	0.020019
-0.339831	73.485502	0.025024
-0.686756	55.452428	0.030029
-0.631114	63.194836	0.035034
-1.039913	51.309187	0.040038
-1.058427	34.499679	0.045043
-1.919774	36.615034	0.050048
-1.694095	25.591778	0.055053
-1.721360	23.498348	0.060058
-2.528440	16.050619	0.065062
-2.255293	4.981972	0.070067
-3.081492	4.930965	0.075072
-3.664735	6.287732	0.080077
-3.879952	5.027350	0.085082
-3.920351	-2.284232	0.090086
-4.595308	2.788509	0.095091
-5.442812	-6.041769	0.100096
-5.550818	1.264343	0.105101
-5.412817	8.152261	0.110106
-5.202815	4.911176	0.115110
-5.448757	-3.010444	0.120115
-5.868422	4.287553	0.125120
-5.771902	0.529573	0.130125
-6.305406	0.527619	0.135130
-6.776796	2.895084	0.140134
-6.828151	-8.208132	0.145139
-7.340250	-3.246331	0.150144
-7.030008	3.801260	0.155149
-7.686937	-1.240215	0.160154
-8.178770	0.035790	0.165158
-8.309325	-7.960854	0.170163
-9.026790	6.119456	0.175168
-9.108983	3.357589	0.180173
-8.872783	1.264010	0.185178
-8.956507	-0.792097	0.190182
-8.908177	-0.277771	0.195187
-9.604078	7.091982	0.200192
-9.683357	1.716389	0.205197
-9.813596	-1.983915	0.210202
-10.582119	1.983514	0.215206
-10.949969	8.273644	0.220211
-11.309840	5.248399	0.225216
-11.376605	2.047515	0.230221
-11.328564	-5.429782	0.235226
-11.556779	-1.024990	0.240230
-11.769047	-11.805597	0.245235
-12.246816	4.201852	0.250240
-12.928897	-2.977549	0.255245
-12.877879	0.725429	0.260250
-13.191722	6.535696	0.265254
-12.796269	2.287951	0.270259
-12.952486	11.566318	0.275264
-13.296263	7.845686	0.280269
-13.726240	9.026579	0.285274
-14.044111	9.186993	0.290278
-14.163549	2.526875	0.295283
-15.023567	6.385254	0.300288
-15.353629	-10.407032	0.305293
-15.640978	-2.101547	0.310298
-16.025447	-1.108120	0.315302
-15.586183	-0.243758	0.320307
-16.074371	8.346301	0.325312
-16.106037	-2.503737	0.330317
-15.872516	2.670270	0.335322
-16.333714	4.833658	0.340326
-16.885858	-6.020249	0.345331
-17.403557	9.123426	0.350336
-17.416728	-1.447936	0.355341
-17.346915	-7.065187	0.360346
-18.332556	2.608890	0.365350
-18.377177	0.106893	0.370355
-18.980165	1.634433	0.375360
-18.695930	-1.668902	0.380365
-18.399554	5.017028	0.385370
-18.980958	-0.210286	0.390374
-19.236350	-0.334909	0.395379
-20.108172	2.974824	0.400384
-20.027132	-3.036494	0.405389
-20.022157	-4.919836	0.410394
-20.336983	4.807324	0.415398
-20.821331	1.671869	0.420403
-21.471633	7.674060	0.425408
-21.262499	4.635592	0.430413
-21.421448	-3.742584	0.435418
-21.564900	-2.204788	0.440422
-21.286461	2.006725	0.445427
-22.048861	5.387899	0.450432
-22.642813	-7.920864	0.455437
-23.071574	6.721653	0.460442
-23.618205	2.014075	0.465446
-23.686274	-3.281015	0.470451
-23.437436	4.010314	0.475456
-23.560838	-3.278769	0.480461
-23.745160	3.539426	0.485466
-24.197651	2.461755	0.490470
-24.308600	-11.096692	0.495475
-24.809159	6.002662	0.500480
-24.882616	6.131108	0.505485
-24.883123	-4.065747	0.510490
-25.637233	9.748223	0.515494
-25.554145	5.419706	0.520499
-26.014227	1.113020	0.525504
-26.234414	-3.864004	0.530509
-25.833760	-5.929566	0.535514
-26.911232	3.730426	0.540518
-27.495352	-1.581883	0.545523
-27.658549	3.258813	0.550528
-27.207291	1.713670	0.555533
-27.534917	6.649733	0.560538
-27.884975	4.407566	0.565542
-28.529156	-0.714998	0.570547
-28.675697	2.727868	0.575552
-28.779967	1.516542	0.580557
-29.259818	2.281305	0.585562
-29.393560	0.046374	0.590566
-29.223991	-0.125851	0.595571
-29.767015	7.906486	0.600576
-29.994539	-5.946912	0.605581
-30.080477	-2.485068	0.610586
-30.573163	9.392847	0.615590
-30.511043	-3.550478	0.620595
-30.738312	3.505401	0.625600
-31.065560	-5.153289	0.630605
-31.896005	0.108331	0.635610
-32.512278	10.088370	0.640614
-31.896735	-3.289683	0.645619
-32.188738	3.450471	0.650624
-32.020754	-8.762789	0.655629
-32.231178	-1.981636	0.660634
-32.867407	4.647938	0.665638
-33.131322	5.543383	0.670643
-33.624649	12.508074	0.675648
-33.564329	-3.690483	0.680653
-34.217115	2.438645	0.685658
-34.733259	-0.214097	0.690662
-34.818223	-1.694204	0.695667
-35.199742	-11.236568	0.700672
-35.102533	-1.624593	0.705677
-35.472382	1.261639	0.710682
-35.352641	8.642799	0.715686
-35.198252	-1.442285	0.720691
-35.677423	4.846304	0.725696
-36.123694	3.593652	0.730701
-36.681386	3.949831	0.735706
-36.502002	0.624959	0.740710
-36.602611	-3.187554	0.745715
-37.700739	-5.423239	0.750720
-38.012530	-0.211248	0.755725
-38.049468	-4.577904	0.760730
-38.404500	8.945745	0.765734
-38.066484	-9.242034	0.770739
-38.180976	7.644969	0.775744
-38.287322	3.314497	0.780749
-38.970577	7.876011	0.785754
-39.270768	0.386837	0.790758
-39.149051	-6.896357	0.795763
-39.626218	3.115665	0.800768
-40.127360	7.537913	0.805773
-40.373545	3.406522	0.810778
-41.364998	4.593134	0.815782
-41.139405	-1.421850	0.820787
-41.411894	9.149729	0.825792
-40.981633	-1.437326	0.830797
-41.021647	-1.364741	0.835802
-41.556185	-6.384258	0.840806
-41.985571	-2.403528	0.845811
-42.346672	1.430462	0.850816
-42.663326	-2.462094	0.855821
-42.687882	2.673254	0.860826
-42.762143	9.777927	0.865830
-42.984654	5.418199	0.870835
-43.285986	3.864426	0.875840
-43.677850	-0.800960	0.880845
-43.864753	0.721498	0.885850
-44.657058	4.983723	0.890854
-44.806956	5.313972	0.895859
-45.159907	14.271986	0.900864
-45.207428	8.587695	0.905869
-45.319200	1.625821	0.910874
-45.517796	-0.231951	0.915878
-45.173289	-1.016884	0.920883
-45.717135	0.181851	0.925888
-46.385340	-3.886576	0.930893
-46.495684	-0.212099	0.935898
-46.955292	1.916239	0.940902
-46.811463	-4.199829	0.945907
-47.486498	0.044020	0.950912
-47.851515	-0.047607	0.955917
-47.679708	-12.865741	0.960922
-48.585087	-3.647169	0.965926
-48.420062	-5.900439	0.970931
-48.428367	-4.355344	0.975936
-48.970098	-5.010905	0.980941
-48.661827	1.132153	0.985946
-49.064516	-0.279187	0.990950
-49.543781	0.485485	0.995955
-49.870829	3.485234	1.000960
-49.705591	8.726888	1.005965
-49.600144	4.417014	1.010970
-50.685904	2.862765	1.015974
-51.107810	-0.579865	1.020979
-51.016858	3.325664	1.025984
-51.248720	5.266457	1.030989
-51.264861	1.285684	1.035994
-52.312565	10.368375	1.040998
-52.298254	-1.409520	1.046003
-52.968096	-0.017035	1.051008
-52.944549	2.927779	1.056013
-52.591099	1.148024	1.061018
-53.243256	3.790588	1.066022
-52.991346	-3.063753	1.071027
-53.210022	-0.720065	1.076032
-53.324859	1.240356	1.081037
-53.707541	6.305269	1.086042
-54.330101	5.440910	1.091046
-54.086638	-1.010310	1.096051
-55.357601	6.626720	1.101056
-55.551918	7.368891	1.106061
-55.602458	6.870485	1.111066
-55.981188	5.325676	1.116070
-55.774071	1.107440	1.121075
-56.152978	5.912333	1.126080
-56.292205	0.122191	1.131085
-55.897841	3.445503	1.136090
-56.872655	7.919824	1.141094
-56.944071	7.630333	1.146099
-57.411472	8.905677	1.151104
-57.570911	6.921545	1.156109
-57.475531	4.321682	1.161114
-58.015487	13.657012	1.166118
-58.383032	5.811394	1.171123
-58.816174	7.957733	1.176128
-59.186588	4.782282	1.181133
-58.987556	5.592534	1.186138
-58.845053	4.893037	1.191142
-59.387651	1.959702	1.196147
-59.969745	10.782776	1.201152
-60.326488	8.965602	1.206157
-60.536702	-1.530589	1.211162
-60.272407	0.446357	1.216166
-60.389220	-3.053567	1.221171
-61.083683	12.516438	1.226176
-61.776739	4.294717	1.231181
-61.386654	1.161458	1.236186
-61.877929	8.448530	1.241190
-61.472136	2.168027	1.246195
-62.384511	9.875423	1.251200
-62.989784	5.328897	1.256205
-63.173688	5.389228	1.261210
-63.436342	6.417354	1.266214
-63.362071	-0.652763	1.271219
-63.466663	4.384395	1.276224
-63.703198	-2.928087	1.281229
-63.860399	-4.450659	1.286234
-64.501891	-3.575145	1.291238
-64.713908	-1.675427	1.296243
-64.837968	8.037659	1.301248
-64.941810	2.583660	1.306253
-64.843952	1.872175	1.311258
-65.843928	6.011916	1.316262
-66.284888	3.056329	1.321267
-66.354224	4.822959	1.326272
-66.319149	-5.442743	1.331277
-66.189530	-3.080863	1.336282
-66.416943	4.345197	1.341286
-66.829067	-2.531647	1.346291
-67.268008	-2.883773	1.351296
-67.582090	3.151157	1.356301
-67.386386	5.888662	1.361306
-68.222615	9.325701	1.366310
-68.719347	-3.700897	1.371315
-69.166281	4.876369	1.376320
-69.292043	2.152968	1.381325
-69.072899	5.971971	1.386330
-69.733042	9.068207	1.391334
-69.400034	1.002091	1.396339
-69.446740	-8.656007	1.401344
-69.545304	-3.676744	1.406349
-70.511055	-5.841417	1.411354
-70.842633	7.147041	1.416358
-70.592504	3.807919	1.421363
-71.032575	9.375373	1.426368
-71.145936	8.190782	1.431373
-71.969781	-2.829354	1.436378
-72.177312	3.176225	1.441382
-72.149956	-1.289091	1.446387
-72.447134	-0.780739	1.451392
-72.382333	-4.122458	1.456397
-72.405011	-1.021705	1.461402
-73.203230	3.311050	1.466406
-73.241388	-1.599581	1.471411
-73.410242	10.347814	1.476416
-73.928641	7.277810	1.481421
-74.000530	7.947014	1.486426
-74.401029	4.618090	1.491430
-74.845628	4.481987	1.496435
-74.848435	1.457746	1.501440
-74.841969	4.727941	1.506445
-74.885001	-0.071196	1.511450
-75.947702	14.639019	1.516454
-76.192813	4.382414	1.521459
-76.345767	5.519902	1.526464
-76.752136	-4.474148	1.531469
-76.546659	-0.317647	1.536474
-76.750803	4.703471	1.541478
-76.461379	9.694710	1.546483
-77.149098	12.535839	1.551488
-77.779446	6.629661	1.556493
-77.850292	1.575454	1.561498
-78.269325	7.709088	1.566502
-78.040447	0.817226	1.571507
-78.889644	10.156716	1.576512
-79.389151	2.306470	1.581517
-79.075745	5.576026	1.586522
-79.776717	4.537293	1.591526
-79.542883	-4.348513	1.596531
-79.777160	5.704545	1.601536
-79.587901	0.321680	1.606541
-80.016268	-1.632966	1.611546
-80.692104	7.657212	1.616550
-80.965062	-0.636657	1.621555
-81.225776	0.198176	1.626560
-81.305175	7.113825	1.631565
-81.482090	-1.843663	1.636570
-82.225139	-2.644848	1.641574
-82.520650	-4.155238	1.646579
-82.711201	2.170383	1.651584
-82.784636	12.362758	1.656589
-82.654443	9.055084	1.661594
-82.713643	9.190787	1.666598
-82.857688	4.511882	1.671603
-83.700008	-0.503698	1.676608
-84.186902	-4.220880	1.681613
-83.622249	-5.432615	1.686618
-84.302423	5.066799	1.691622
-84.786732	1.962981	1.696627
-85.447676	10.836375	1.701632
-85.538136	-5.727691	1.706637
-85.276015	-1.184596	1.711642
-85.687943	4.473359	1.716646
-85.432326	2.110981	1.721651
-85.872965	4.385045	1.726656
-86.296138	4.916303	1.731661
-86.441828	-0.107193	1.736666
-87.033690	9.998734	1.741670
-86.875707	10.843891	1.746675
-87.625469	2.314685	1.751680
-88.372209	-0.479092	1.756685
-87.939459	3.018537	1.761690
-88.674871	8.404476	1.766694
-88.318475	2.742320	1.771699
-88.890434	4.100488	1.776704
-88.796392	0.934521	1.781709
-88.416234	8.553283	1.786714
-89.308501	9.702212	1.791718
-89.426245	1.032845	1.796723
-89.868713	6.126108	1.801728
-90.505324	9.405320	1.806733
-90.185178	8.149638	1.811738
-90.495632	8.286746	1.816742
-90.907049	3.311214	1.821747
-91.267120	6.338285	1.826752
-91.432812	1.501421	1.831757
-91.662341	-1.980840	1.836762
-91.960247	-0.814312	1.841766
-91.906251	2.454762	1.846771
-92.819031	5.052745	1.851776
-92.938805	2.160727	1.856781
-92.868532	3.921300	1.861786
-93.268976	16.404861	1.866790
-93.097413	-3.496906	1.871795
-93.219884	3.716556	1.876800
-93.650473	-2.942255	1.881805
-94.390872	-10.447863	1.886810
-94.767891	-0.916609	1.891814
-94.699054	-7.419557	1.896819
-94.666959	-4.669073	1.901824
-94.934870	-3.105447	1.906829
-95.414132	-1.904175	1.911834
-95.999587	6.150629	1.916838
-96.159160	-5.134940	1.921843
-96.046922	-10.230486	1.926848
-96.133493	-12.510770	1.931853
-96.434431	-5.051047	1.936858
-97.228648	3.574306	1.941862
-97.003913	0.321422	1.946867
-97.358121	0.101554	1.951872
-97.397444	-1.721062	1.956877
-97.805509	-5.020322	1.961882
-98.476950	3.633249	1.966886
-98.943980	5.009777	1.971891
-98.990784	0.809183	1.976896
-99.142651	-0.511742	1.981901
-99.046960	-4.633422	1.986906
-98.970807	13.517684	1.991910
-99.393901	-6.499708	1.996915
-100.167309	1.046530	2.006912
-99.447490	3.233325	2.016909
-99.170726	-1.001305	2.026906
-99.282241	0.016952	2.036902
-98.120294	1.919057	2.046899
-97.785769	3.824102	2.056896
-97.074015	5.331082	2.066893
-96.569138	-4.400601	2.076890
-96.349007	-1.581141	2.086886
-95.412994	-4.395352	2.096883
-95.339157	5.143788	2.106880
-94.977471	2.150306	2.116877
-94.266854	-3.910442	2.126874
-93.729410	-1.476490	2.136870
-92.857271	-1.499353	2.146867
-92.420635	4.900658	2.156864
-92.619397	-6.535926	2.166861
-91.610089	-2.620517	2.176858
-91.143738	-6.124577	2.186854
-91.007058	2.501889	2.196851
-90.174551	-3.128128	2.206848
-89.810096	-2.634282	2.216845
-88.745808	-4.888882	2.226842
-88.417538	-0.410594	2.236838
-88.229093	-4.625048	2.246835
-87.742105	-6.079599	2.256832
-86.969367	2.165266	2.266829
-86.425147	-2.266494	2.276826
-86.706359	-3.173021	2.286822
-85.869942	-2.433178	2.296819
-85.409625	-0.272244	2.306816
-84.487203	-2.808725	2.316813
-84.206900	-2.501265	2.326810
-83.627794	-1.223757	2.336806
-82.645773	1.618874	2.346803
-82.514657	-0.483170	2.356800
-82.604241	-6.256973	2.366797
-81.830514	-5.950800	2.376794
-81.111648	-7.185092	2.386790
-80.600743	-1.981481	2.396787
-79.844142	-1.279816	2.406784
-79.863546	-4.204081	2.416781
-79.432740	3.625528	2.426778
-78.490223	-6.884319	2.436774
-78.333120	-0.066706	2.446771
-77.653627	2.218277	2.456768
-76.849587	-1.459074	2.466765
-76.863285	-1.859486	2.476762
-75.939349	-2.625395	2.486758
-75.554005	0.738385	2.496755
-75.337605	6.029327	2.506752
-74.758534	-4.575628	2.516749
-74.172936	0.499072	2.526746
-73.838255	12.360535	2.536742
-73.138077	4.609808	2.546739
-72.795209	7.606444	2.556736
-71.847400	4.587645	2.566733
-71.372234	1.560542	2.576730
-71.379442	-3.887213	2.586726
-70.750283	5.637776	2.596723
-70.267191	-2.300680	2.606720
-69.428577	9.624373	2.616717
-69.027787	3.349242	2.626714
-68.916510	4.709559	2.636710
-67.930997	2.007971	2.646707
-67.469011	6.921476	2.656704
-67.324593	5.682160	2.666701
-66.547400	2.826312	2.676698
-65.879058	2.410898	2.686694
-65.600037	-1.307732	2.696691
-65.389173	-2.715849	2.706688
-64.570840	1.787025	2.716685
-64.397317	-2.770384	2.726682
-63.002435	-0.606998	2.736678
-62.812068	-6.472184	2.746675
-62.942016	-5.511228	2.756672
-62.166405	-2.595071	2.766669
-61.284258	-3.474808	2.776666
-61.221273	-9.725515	2.786662
-60.869791	-3.331167	2.796659
-59.963793	-5.374061	2.806656
-59.750389	9.161033	2.816653
-59.072282	-2.587184	2.826650
-58.366825	-7.278624	2.836646
-58.316982	-7.185310	2.846643
-57.374859	-4.691220	2.856640
-56.827747	-2.087719	2.866637
-57.013305	-3.984921	2.876634
-56.096692	-11.782225	2.886630
-55.503697	-9.163739	2.896627
-55.139728	-3.493609	2.906624
-54.344123	1.526013	2.916621
-54.004026	-0.589770	2.926618
-53.748315	-0.322804	2.936614
-53.246058	-6.623334	2.946611
-52.718727	-6.459117	2.956608
-51.929580	-7.802621	2.966605
-51.252342	-4.462401	2.976602
-51.111996	-10.614356	2.986598
-51.044900	-9.000027	2.996595
-50.057903	-8.480179	3.006592
-49.664293	-7.176772	3.016589
-48.595748	-6.346585	3.026586
-48.310615	-12.803160	3.036582
-48.103880	-14.707976	3.046579
-48.077048	-17.905580	3.056576
-47.306168	-13.553663	3.066573
-46.521493	-12.340041	3.076570
-45.908182	-14.485960	3.086566
-45.727758	-15.654888	3.096563
-45.120782	-15.633030	3.106560
-44.389337	-5.937169	3.116557
-44.215037	-7.722862	3.126554
-43.508277	-5.689239	3.136550
-43.055998	-2.256749	3.146547
-42.642326	-6.094678	3.156544
-41.970275	-7.540211	3.166541
-41.142450	-11.525394	3.176538
-41.261949	-8.545011	3.186534
-40.717205	-11.621027	3.196531
-40.018119	-12.224989	3.206528
-39.862346	-4.612045	3.216525
-38.739260	-4.246567	3.226522
-38.167942	-7.272894	3.236518
-38.418675	-4.303626	3.246515
-37.696760	-4.017842	3.256512
-36.738886	-7.088898	3.266509
-36.658769	-6.629693	3.276506
-35.885472	-1.872671	3.286502
-35.421717	0.518979	3.296499
-35.201410	-2.769131	3.306496
-34.260765	-4.380293	3.316493
-34.105999	-5.250595	3.326490
-33.648517	-8.962340	3.336486
-33.156877	-2.285840	3.346483
-32.410303	-6.673277	3.356480
-32.451823	-2.257420	3.366477
-31.500132	1.299560	3.376474
-30.821429	-6.080330	3.386470
-30.019747	-6.792234	3.396467
-29.723397	-8.606553	3.406464
-29.401389	-7.481994	3.416461
-29.002880	-16.104111	3.426458
-28.929412	-8.988290	3.436454
-28.228482	-5.262139	3.446451
-27.817341	-10.192566	3.456448
-26.852563	-10.030365	3.466445
-26.681325	-12.522000	3.476442
-25.890286	-9.069729	3.486438
-25.510287	-8.537134	3.496435
-25.218076	-13.426751	3.506432
-24.110472	-10.233157	3.516429
-24.017219	-9.227979	3.526426
-23.856096	-9.069737	3.536422
-22.918623	-10.873637	3.546419
-22.573601	-11.789587	3.556416
-21.958406	-7.254882	3.566413
-21.001892	-11.950811	3.576410
-20.750001	-10.390779	3.586406
-20.696425	-7.019362	3.596403
-20.391754	-6.788578	3.606400
-19.238176	-6.484896	3.616397
-19.158627	-7.020295	3.626394
-18.178860	-9.296490	3.636390
-17.851246	-7.764161	3.646387
-17.685156	-2.731432	3.656384
-16.989973	-4.155245	3.666381
-16.506156	-9.410673	3.676378
-16.172275	-12.900310	3.686374
-15.294929	-11.045468	3.696371
-15.215317	-11.916665	3.706368
-14.388472	-5.989604	3.716365
-13.367214	-9.700984	3.726362
-13.265227	-9.210360	3.736358
-13.314706	-1.324499	3.746355
-12.609753	-7.457215	3.756352
-11.801364	-10.707586	3.766349
-11.935547	-1.987990	3.776346
-11.138201	-15.101203	3.786342
-10.604663	-11.032043	3.796339
-9.718027	-10.119496	3.806336
-8.983297	-7.364822	3.816333
-8.788697	-8.935116	3.826330
-8.840905	-10.606124	3.836326
-8.088424	-14.820253	3.846323
-7.647583	-1.854017	3.856320
-6.910690	-1.263298	3.866317
-5.817481	-3.383038	3.876314
-6.052800	-11.807645	3.886310
-6.034822	-7.366265	3.896307
-5.369318	-4.895351	3.906304
-4.802932	9.647802	3.916301
-4.317776	14.215561	3.926298
-3.697393	26.295209	3.936294
-3.197944	30.591468	3.946291
-2.680470	44.740000	3.956288
-2.424596	62.407805	3.966285
-1.988757	73.179577	3.976282
-1.414811	83.562248	3.986278
-1.076277	99.775776	3.996275
-0.419245	126.944482	4.006272
0.000000	137.223601	4.011277
0.192193	138.768932	4.016282
0.229590	153.870049	4.021286
0.342768	165.855624	4.026291
0.726296	168.595366	4.031296
0.201156	166.608402	4.036301
0.136259	168.874232	4.041306
0.443367	161.653670	4.046310
0.741042	181.440738	4.051315
0.656779	187.310006	4.056320
0.490205	187.718801	4.061325
0.460799	189.264055	4.066330
1.010347	189.418276	4.071334
0.990017	199.159512	4.076339
1.128445	192.563325	4.081344
1.061427	200.786926	4.086349
1.219777	194.833031	4.091354
1.088497	191.484031	4.096358
0.891779	205.482907	4.101363
1.186173	202.057718	4.106368
1.136547	201.628766	4.111373
0.799689	203.725238	4.116378
0.902299	199.573950	4.121382
0.844175	198.791984	4.126387
1.233391	204.296003	4.131392
0.831274	198.743138	4.136397
1.088653	197.373893	4.141402
1.252142	191.852635	4.146406
1.354376	203.450802	4.151411
1.280777	197.201050	4.156416
1.248305	196.952910	4.161421
1.165014	206.444583	4.166426
1.252418	191.579889	4.171430
1.090398	205.585983	4.176435
0.915844	190.676910	4.181440
0.757314	204.343930	4.186445
0.916866	199.199779	4.191450
0.865213	206.465507	4.196454
1.077527	203.331594	4.201459
1.113603	201.152287	4.206464
1.046166	198.859483	4.211469
0.717344	202.020896	4.216474
1.434907	211.668671	4.221478
1.392673	228.800834	4.226483
1.241374	212.154335	4.231488
1.140836	208.800516	4.236493
1.469081	215.003799	4.241498
1.240861	213.175954	4.246502
1.426170	225.279983	4.251507
1.358485	212.129043	4.256512
1.477288	223.148815	4.261517
1.019587	222.514877	4.266522
1.191570	228.922985	4.271526
1.014970	221.107461	4.276531
1.110799	226.663783	4.281536
1.083245	232.217291	4.286541
0.788319	230.134136	4.291546
1.464273	229.177040	4.296550
1.055619	230.484321	4.301555
1.615753	239.460740	4.306560
1.663187	252.912025	4.311565
1.422498	235.105737	4.316570
1.817768	239.643857	4.321574
1.429982	243.769986	4.326579
1.409951	240.704108	4.331584
1.527513	248.421075	4.336589
1.676542	248.043255	4.341594
1.841109	249.149991	4.346598
1.506293	244.159217	4.351603
1.972080	221.838230	4.356608
1.393575	236.175363	4.361613
1.117336	231.634166	4.366618
1.764829	240.688649	4.371622
1.704242	250.401418	4.376627
1.872268	254.013349	4.381632
1.876422	269.410843	4.386637
1.334557	247.956399	4.391642
1.758343	236.161642	4.396646
1.965764	253.738775	4.401651
1.829284	253.934045	4.406656
1.546673	244.784174	4.411661
1.455700	260.645826	4.416666
1.922888	253.514042	4.421670
1.766407	257.297043	4.426675
1.832408	257.390984	4.431680
1.645782	260.201092	4.436685
1.560265	252.510490	4.441690
1.664034	259.324774	4.446694
1.672940	267.144197	4.451699
1.639968	258.255766	4.456704
1.650745	262.977524	4.461709
1.722527	258.577948	4.466714
2.110448	251.037799	4.471718
1.645515	255.226638	4.476723
1.835760	247.818704	4.481728
1.885186	261.139967	4.486733
1.448013	258.648818	4.491738
2.126553	263.022336	4.496742
1.872506	268.288635	4.501747
1.869058	274.040863	4.506752
1.970859	286.290898	4.511757
2.223759	285.956915	4.516762
2.007112	286.471636	4.521766
1.684141	276.856663	4.526771
2.175207	280.022508	4.531776
1.948033	283.383148	4.536781
1.843044	288.287570	4.541786
2.354305	280.411701	4.546790
2.276861	293.205526	4.551795
2.232388	280.114175	4.556800
2.377272	278.816335	4.561805
2.077533	272.646281	4.566810
2.388319	264.931547	4.571814
1.941826	263.299250	4.576819
1.957684	267.283045	4.581824
1.995265	281.159846	4.586829
2.069139	285.428790	4.591834
2.496428	276.914334	4.596838
2.525378	284.063059	4.601843
2.494726	282.530124	4.606848
2.390055	272.874622	4.611853
2.391740	267.290106	4.616858
2.203429	259.973118	4.621862
2.485071	267.917490	4.626867
2.239892	260.375290	4.631872
2.265436	262.554194	4.636877
2.055519	260.533648	4.641882
2.472318	268.713113	4.646886
2.184590	273.864465	4.651891
2.253270	270.743553	4.656896
2.419725	275.358663	4.661901
2.323700	284.827062	4.666906
2.388304	278.289867	4.671910
2.159682	288.402315	4.676915
2.384756	296.165735	4.681920
2.338204	288.089354	4.686925
2.608995	285.177223	4.691930
2.853505	275.919434	4.696934
2.374200	284.641114	4.701939
2.733402	283.559634	4.706944
2.476094	286.564321	4.711949
2.786191	272.946012	4.716954
2.485740	271.626197	4.721958
2.162457	270.344762	4.726963
2.452175	277.133081	4.731968
2.616594	286.462596	4.736973
2.460500	285.613717	4.741978
2.837394	284.279524	4.746982
2.609576	284.213854	4.751987
2.331931	282.052054	4.756992
2.301021	279.750353	4.761997
2.359403	285.442276	4.767002
3.118694	275.698863	4.772006
2.557088	285.363599	4.777011
2.516086	282.038403	4.782016
2.950400	279.610025	4.787021
2.827017	279.746295	4.792026
2.953799	280.593193	4.797030
2.707307	287.028924	4.802035
3.021977	280.759438	4.807040
2.767750	278.888204	4.812045
2.823164	274.234920	4.817050
2.962889	275.760009	4.822054
2.642352	277.123091	4.827059
2.583960	292.084307	4.832064
2.673261	276.425126	4.837069
2.258722	291.853439	4.842074
2.450583	269.005826	4.847078
2.317167	273.142727	4.852083
2.511910	276.446750	4.857088
2.758737	288.474743	4.862093
3.003294	294.760771	4.867098
3.003198	286.955529	4.872102
2.730172	297.403976	4.877107
2.855051	303.341756	4.882112
2.830643	303.674494	4.887117
2.826128	305.775854	4.892122
2.873026	303.591675	4.897126
2.727110	311.947914	4.902131
3.120201	309.067238	4.907136
3.443335	305.365438	4.912141
3.063613	305.352043	4.917146
3.464386	294.392937	4.922150
3.011838	294.580781	4.927155
2.657180	289.213445	4.932160
3.007682	291.610362	4.937165
2.828644	300.019242	4.942170
3.202951	307.072736	4.947174
3.034679	305.732208	4.952179
3.257497	312.654413	4.957184
3.096283	304.478929	4.962189
3.095745	312.337817	4.967194
3.110915	303.774022	4.972198
2.871490	304.216382	4.977203
3.274213	313.132078	4.982208
2.928864	318.064676	4.987213
3.054692	309.894837	4.992218
3.291415	308.500345	4.997222
3.062485	314.942827	5.002227
3.403085	312.295005	5.007232
3.290227	314.299444	5.012237
3.020605	315.154667	5.017242
3.403973	302.160784	5.022246
3.002210	313.885447	5.027251
2.887683	311.087469	5.032256
2.856434	317.818524	5.037261
3.320571	327.294093	5.042266
3.390072	324.888067	5.047270
3.374158	324.510778	5.052275
3.692888	328.760351	5.057280
3.613796	321.714133	5.062285
3.398527	331.036721	5.067290
3.099980	314.552405	5.072294
3.278163	322.917982	5.077299
3.271659	308.434907	5.082304
3.518284	331.577461	5.087309
3.539860	341.049611	5.092314
3.624547	337.619288	5.097318
3.481081	326.935265	5.102323
3.125456	329.069493	5.107328
3.920941	328.985862	5.112333
3.652210	337.911861	5.117338
3.382579	316.506430	5.122342
3.180244	326.523030	5.127347
3.576523	330.978757	5.132352
3.902380	340.254531	5.137357
3.786238	336.830364	5.142362
3.535519	325.799306	5.147366
3.290201	318.959471	5.152371
3.507252	321.563967	5.157376
3.533054	335.009212	5.162381
3.095518	343.088447	5.167386
3.443960	332.469719	5.172390
3.456937	338.361767	5.177395
3.614829	340.396555	5.182400
3.861125	342.135912	5.187405
3.506816	333.066832	5.192410
3.480821	336.573135	5.197414
3.607654	337.961042	5.202419
3.910956	335.581658	5.207424
3.642443	335.073101	5.212429
3.592476	340.680776	5.217434
3.646116	342.576871	5.222438
3.333809	343.116074	5.227443
3.736628	361.697269	5.232448
4.028564	364.267892	5.237453
3.882512	357.257461	5.242458
3.704133	355.779305	5.247462
3.535842	372.039157	5.252467
3.871501	361.283207	5.257472
3.867074	370.278544	5.262477
3.929611	371.303195	5.267482
4.067016	369.756577	5.272486
3.829985	368.192694	5.277491
4.189662	360.596811	5.282496
4.075202	361.307500	5.287501
4.064258	362.343664	5.292506
4.152022	368.182874	5.297510
3.755290	359.987317	5.302515
3.900708	361.264743	5.307520
3.753363	357.696761	5.312525
3.917684	367.867913	5.317530
3.866806	361.374092	5.322534
3.779271	368.857485	5.327539
4.043125	368.256023	5.332544
3.984218	365.822653	5.337549
3.495405	365.921265	5.342554
4.185075	363.044732	5.347558
3.735558	369.591399	5.352563
3.936173	371.224018	5.357568
3.760597	364.781372	5.362573
4.251136	376.296665	5.367578
4.104774	375.047614	5.372582
4.318701	377.690574	5.377587
4.076197	371.647563	5.382592
4.358677	379.636148	5.387597
4.044515	380.884341	5.392602
4.218807	367.901021	5.397606
4.216792	378.284906	5.402611
4.469312	380.001145	5.407616
4.361930	364.840951	5.412621
3.953567	368.767846	5.417626
4.398928	380.669880	5.422630
4.188775	392.184234	5.427635
4.484790	381.886912	5.432640
4.148038	376.045333	5.437645
4.222270	387.739758	5.442650
4.668435	389.039669	5.447654
4.358068	392.764550	5.452659
4.316590	387.819526	5.457664
4.654910	389.522321	5.462669
4.498949	385.835458	5.467674
4.205818	377.152250	5.472678
4.430154	376.971441	5.477683
4.407540	372.428436	5.482688
4.319890	376.070960	5.487693
4.428493	389.500109	5.492698
4.620389	388.650486	5.497702
4.542600	383.496012	5.502707
4.408504	377.635335	5.507712
4.729808	382.096494	5.512717
3.992577	384.192440	5.517722
4.507477	388.544172	5.522726
4.800269	383.837848	5.527731
4.791915	372.411274	5.532736
4.655105	384.401361	5.537741
4.717261	393.686843	5.542746
4.498354	369.796118	5.547750
4.324859	378.685069	5.552755
4.226919	380.199948	5.557760
4.142188	385.715005	5.562765
4.274881	392.736785	5.567770
4.542677	390.894482	5.572774
4.722603	396.633838	5.577779
4.512813	386.855535	5.582784
4.489422	385.580888	5.587789
4.398721	386.540962	5.592794
4.398811	385.860601	5.597798
4.576426	393.008224	5.602803
4.638488	412.978001	5.607808
5.247226	405.099461	5.612813
4.910358	399.915970	5.617818
5.069378	388.988358	5.622822
4.672075	386.642807	5.627827
4.671346	388.028557	5.632832
4.612635	392.485983	5.637837
4.846323	396.951382	5.642842
4.869046	404.559887	5.647846
4.756819	410.227961	5.652851
4.782531	410.141549	5.657856
4.863762	412.552198	5.662861
4.485089	414.291404	5.667866
4.754786	415.501904	5.672870
4.871990	422.440699	5.677875
4.748699	423.247689	5.682880
4.843942	417.983834	5.687885
4.662564	417.787497	5.692890
4.947321	412.013047	5.697894
4.748025	417.236008	5.702899
4.898553	410.008241	5.707904
4.662988	412.579260	5.712909
4.613164	413.830332	5.717914
5.067607	430.065434	5.722918
5.164187	443.550293	5.727923
4.987443	431.729273	5.732928
5.318246	432.616980	5.737933
4.882792	436.953107	5.742938
4.989972	424.739584	5.747942
4.878860	441.243647	5.752947
4.928586	443.257428	5.757952
5.066572	447.405631	5.762957
4.921076	455.132266	5.767962
5.173718	440.757181	5.772966
4.965058	441.998339	5.777971
4.938539	440.126212	5.782976
5.012842	441.610945	5.787981
5.128584	450.619133	5.792986
5.382888	436.345035	5.797990
4.875417	446.975839	5.802995
5.401926	451.464977	5.808000
5.588157	444.380302	5.813005
5.380005	443.963527	5.818010
5.471035	445.841119	5.823014
5.356283	450.133329	5.828019
4.949985	437.715503	5.833024
5.260353	444.984720	5.838029
4.943741	449.200986	5.843034
5.561788	444.127300	5.848038
5.313721	443.852824	5.853043
5.359427	451.549500	5.858048
5.151774	446.279309	5.863053
5.185748	442.951827	5.868058
5.408029	446.669195	5.873062
5.373767	450.641901	5.878067
5.615305	448.835344	5.883072
5.299891	446.584526	5.888077
5.411067	455.726314	5.893082
5.596990	455.042144	5.898086
5.422738	447.020502	5.903091
5.275839	446.840909	5.908096
5.690968	460.734628	5.913101
5.161666	463.826254	5.918106
5.400658	461.969474	5.923110
5.695066	470.313745	5.928115
5.714248	468.295245	5.933120
5.645488	472.286016	5.938125
5.287730	472.677315	5.943130
5.636159	477.301932	5.948134
5.226877	469.994169	5.953139
5.338162	478.060242	5.958144
5.755709	480.905439	5.963149
5.545986	479.131617	5.968154
5.909941	470.699762	5.973158
5.515379	475.934351	5.978163
5.503313	476.002559	5.983168
5.661101	480.606425	5.988173
5.447361	483.009515	5.993178
5.549816	475.105862	5.998182
5.415353	484.757565	6.003187
5.442154	481.209731	6.008192
5.635004	488.307547	6.013197
5.915941	488.677870	6.018202
5.677546	477.198685	6.023206
5.816191	492.024789	6.028211
6.036078	496.033616	6.033216
5.970804	479.772034	6.038221
5.532212	482.669112	6.043226
5.798137	482.858285	6.048230
5.572091	489.952130	6.053235
5.585697	480.660809	6.058240
5.560970	481.844677	6.063245
5.839692	489.213785	6.068250
5.960787	493.728488	6.073254
5.475824	489.757783	6.078259
5.861746	502.083676	6.083264
5.650723	510.405914	6.088269
5.992571	503.774576	6.093274
6.040481	490.355375	6.098278
5.537063	495.230527	6.103283
5.684127	485.295016	6.108288
5.677404	480.673561	6.113293
5.469446	501.717159	6.118298
6.027759	501.512496	6.123302
5.619288	500.718969	6.128307
5.965916	505.305909	6.133312
5.876366	493.037739	6.138317
5.841061	489.243362	6.143322
5.422383	488.299569	6.148326
5.544407	499.739799	6.153331
6.073912	493.313188	6.158336
6.080574	497.266837	6.163341
5.463830	485.875400	6.168346
5.721505	485.426767	6.173350
5.770966	492.040835	6.178355
5.779353	479.906030	6.183360
5.738392	483.139452	6.188365
5.844467	491.772677	6.193370
5.741467	479.199731	6.198374
5.775215	488.964290	6.203379
5.462803	485.849265	6.208384
5.883678	487.178457	6.213389
5.795611	508.791756	6.218394
5.978157	501.796224	6.223398
5.824213	492.999399	6.228403
5.651116	482.237665	6.233408
5.521988	483.361958	6.238413
5.573467	492.794701	6.243418
6.180275	497.565507	6.248422
5.562384	491.894493	6.253427
5.660517	490.062943	6.258432
5.898391	507.796912	6.263437
6.141339	496.103087	6.268442
5.408595	489.640123	6.273446
5.536252	488.528470	6.278451
6.054383	495.853742	6.283456
5.923638	487.572157	6.288461
5.473767	484.108499	6.293466
5.806338	495.386020	6.298470
5.763286	489.090250	6.303475
5.953363	494.239571	6.308480
6.045528	482.493447	6.313485
5.471729	480.966500	6.318490
5.674680	471.291166	6.323494
5.143397	479.201647	6.328499
5.807639	497.204170	6.333504
6.089426	493.945422	6.338509
5.984609	494.860255	6.343514
6.193459	477.030749	6.348518
5.974637	479.314408	6.353523
5.960802	474.137232	6.358528
5.928818	468.197249	6.363533
5.560386	471.086496	6.368538
5.616481	467.644809	6.373542
5.569650	472.976780	6.378547
5.770504	484.632446	6.383552
5.503481	478.140811	6.388557
5.566168	479.295162	6.393562
5.808231	476.011003	6.398566
5.798088	486.370914	6.403571
5.741309	479.466674	6.408576
5.838457	473.392558	6.413581
5.806401	487.305741	6.418586
6.086509	472.410620	6.423590
5.169623	477.565692	6.428595
5.298866	479.921370	6.433600
5.967182	492.990809	6.438605
5.893870	508.868897	6.443610
5.854775	503.442562	6.448614
5.521915	490.026071	6.453619
6.065568	502.646800	6.458624
5.854585	493.751341	6.463629
5.688586	486.573137	6.468634
5.900480	482.575509	6.473638
5.550985	486.148347	6.478643
5.483203	472.544799	6.483648
5.968595	489.009231	6.488653
5.821903	490.987352	6.493658
5.837985	487.026731	6.498662
5.695388	487.241945	6.503667
5.623604	485.285154	6.508672
5.671739	482.768556	6.513677
5.759753	500.747467	6.518682
6.350332	497.706100	6.523686
6.134734	495.683253	6.528691
5.987633	493.766737	6.533696
5.951967	482.122902	6.538701
5.727569	480.351379	6.543706
6.176150	486.251157	6.548710
5.785672	481.389264	6.553715
5.612460	480.925883	6.558720
5.770450	484.055364	6.563725
5.667928	484.878086	6.568730
5.751081	476.591467	6.573734
5.748180	485.320860	6.578739
5.908461	485.153251	6.583744
5.562590	475.693623	6.588749
5.679177	480.012870	6.593754
5.738980	472.796129	6.598758
5.985073	480.518369	6.603763
5.970768	483.348969	6.608768
5.521072	479.106978	6.613773
5.364616	483.048215	6.618778
5.886676	484.013529	6.623782
5.440264	483.912502	6.628787
5.597425	480.774526	6.633792
5.709503	479.329946	6.638797
5.752486	480.047610	6.643802
5.975163	482.546841	6.648806
5.567032	490.286167	6.653811
5.334576	479.353395	6.658816
5.898986	476.591387	6.663821
5.967640	481.664813	6.668826
5.855234	481.691794	6.673830
5.796890	493.340620	6.678835
6.008739	484.935753	6.683840
6.323645	483.133517	6.688845
5.808388	485.121927	6.693850
6.195090	480.040185	6.698854
5.923408	484.148176	6.703859
5.759275	480.092403	6.708864
5.709975	480.723283	6.713869
5.611509	482.646389	6.718874
5.766396	485.554887	6.723878
5.817825	476.450638	6.728883
6.169045	472.282482	6.733888
5.959772	476.247812	6.738893
5.699208	475.045121	6.743898
5.846980	460.907921	6.748902
5.632924	471.869265	6.753907
5.567022	470.145679	6.758912
5.567850	476.985666	6.763917
5.363922	484.613898	6.768922
5.642764	483.174828	6.773926
5.674986	486.564468	6.778931
5.863654	485.962127	6.783936
6.018847	489.971598	6.788941
5.914022	485.118732	6.793946
5.938055	485.393262	6.798950
5.965959	489.707424	6.803955
5.848210	484.568673	6.808960
5.665295	476.304759	6.813965
5.636294	487.107399	6.818970
5.960719	473.977090	6.823974
5.947074	476.345664	6.828979
5.666984	464.281379	6.833984
5.531686	454.396453	6.838989
5.366333	474.417750	6.843994
5.930279	474.943054	6.848998
5.698898	477.924727	6.854003
5.861330	479.667746	6.859008
6.039325	487.770829	6.864013
5.848093	486.073206	6.869018
5.992598	471.186677	6.874022
5.569488	467.111370	6.879027
5.612746	459.568186	6.884032
5.902007	471.782649	6.889037
5.154700	470.026617	6.894042
5.747861	473.385315	6.899046
5.588837	480.747074	6.904051
5.808860	488.555663	6.909056
5.871986	483.904280	6.914061
5.790676	481.290901	6.919066
5.885080	479.421971	6.924070
5.636552	478.138298	6.929075
5.603754	481.753266	6.934080
5.674656	477.831516	6.939085
5.386067	481.483398	6.944090
5.681663	482.310183	6.949094
5.718499	485.683280	6.954099
5.713234	482.216402	6.959104
5.950253	487.307744	6.964109
5.941609	477.744656	6.969114
5.937445	477.431965	6.974118
5.673784	478.352702	6.979123
5.334928	489.352594	6.984128
5.905100	484.922332	6.989133
5.456505	485.119049	6.994138
5.776728	484.891578	6.999142
5.920591	480.499637	7.004147
5.642497	490.578820	7.009152
5.824597	479.334315	7.014157
5.598302	478.999477	7.019162
5.629816	476.735428	7.024166
5.578970	485.814029	7.029171
5.964856	483.646321	7.034176
6.014231	480.794160	7.039181
5.821565	490.961202	7.044186
5.514609	475.433538	7.049190
5.633811	486.946971	7.054195
5.918309	491.977090	7.059200
5.947204	488.311863	7.064205
5.765424	487.631519	7.069210
5.768730	483.302730	7.074214
5.692060	485.548298	7.079219
5.366396	492.442611	7.084224
5.791460	493.106738	7.089229
5.771957	479.986017	7.094234
5.724659	483.040092	7.099238
5.657944	475.229386	7.104243
5.677315	479.899233	7.109248
5.788602	484.535697	7.114253
6.007599	474.259880	7.119258
5.948405	482.466565	7.124262
5.512585	487.745589	7.129267
5.365567	496.159035	7.134272
5.563469	483.301651	7.139277
5.387119	492.754271	7.144282
5.673205	483.040595	7.149286
5.853706	494.702621	7.154291
5.628130	492.500998	7.159296
5.905353	485.946233	7.164301
5.495859	501.551111	7.169306
5.999324	492.581679	7.174310
5.754891	484.820960	7.179315
5.856853	491.613469	7.184320
5.923908	481.247556	7.189325
5.819385	489.929597	7.194330
5.757473	494.362239	7.199334
5.401052	490.365066	7.204339
5.712188	485.820361	7.209344
5.763369	493.706028	7.214349
5.868870	494.277852	7.219354
5.650723	483.216282	7.224358
5.784432	496.562481	7.229363
5.613132	493.558227	7.234368
5.797158	497.313238	7.239373
5.881820	499.932175	7.244378
5.740856	484.669570	7.249382
5.591889	501.480186	7.254387
5.974787	509.788465	7.259392
6.030579	494.099541	7.264397
5.730843	495.193616	7.269402
5.641120	485.200289	7.274406
5.856659	487.409565	7.279411
5.750451	488.321453	7.284416
5.684698	480.728899	7.289421
5.678699	485.798204	7.294426
5.527683	482.287721	7.299430
6.034832	491.440254	7.304435
6.048688	494.073449	7.309440
5.798560	481.210331	7.314445
5.408431	484.435184	7.319450
5.700173	481.402676	7.324454
5.743945	491.254254	7.329459
5.731283	485.659262	7.334464
6.193033	483.429045	7.339469
5.591470	484.731766	7.344474
5.981654	478.039079	7.349478
5.930204	481.897422	7.354483
5.797480	483.572788	7.359488
5.913426	477.821603	7.364493
6.015918	479.055142	7.369498
5.844125	475.323282	7.374502
6.163189	486.197941	7.379507
6.017091	479.060916	7.384512
6.085467	481.476752	7.389517
5.807084	487.635970	7.394522
6.175956	478.368083	7.399526
5.962967	469.627979	7.404531
5.732205	469.015423	7.409536
5.905622	454.143361	7.414541
5.588932	452.516020	7.419546
6.303251	459.696640	7.424550
5.802786	460.591203	7.429555
5.726533	461.789469	7.434560
5.795964	461.879711	7.439565
5.554797	455.301772	7.444570
5.784724	454.224718	7.449574
5.644896	462.611712	7.454579
5.600987	461.457337	7.459584
5.847162	460.017059	7.464589
5.782749	458.527365	7.469594
5.904330	453.714967	7.474598
5.574113	460.502410	7.479603
5.464185	459.431147	7.484608
5.593571	449.289611	7.489613
5.316231	468.787431	7.494618
5.973161	474.638741	7.499622
6.003941	488.409198	7.504627
5.778093	475.827027	7.509632
5.962641	473.396628	7.514637
5.839372	464.731056	7.519642
5.657290	466.581838	7.524646
5.756009	462.937315	7.529651
5.559669	463.743097	7.534656
5.847494	467.260369	7.539661
5.324929	467.373760	7.544666
6.013984	476.238349	7.549670
5.975382	487.820801	7.554675
5.428625	472.694555	7.559680
6.092301	479.193399	7.564685
5.677561	471.228409	7.569690
5.804990	462.431808	7.574694
5.750312	458.396856	7.579699
5.455117	466.045708	7.584704
5.859249	461.875592	7.589709
5.573520	471.800932	7.594714
5.837728	482.709495	7.599718
5.942820	487.954389	7.604723
6.004207	486.138089	7.609728
5.986303	470.033614	7.614733
5.654540	467.703094	7.619738
5.559185	464.690110	7.624742
5.593367	474.441938	7.629747
5.763691	474.111399	7.634752
5.746004	471.924664	7.639757
5.651481	478.172133	7.644762
6.039451	480.193035	7.649766
5.925993	469.684563	7.654771
5.259437	467.944354	7.659776
5.383156	465.710153	7.664781
5.470620	480.291159	7.669786
5.789886	483.262489	7.674790
5.951545	493.620797	7.679795
5.792211	485.321545	7.684800
6.117547	485.795647	7.689805
6.112062	484.910505	7.694810
5.974992	476.212289	7.699814
5.857410	473.737475	7.704819
5.533214	461.844623	7.709824
5.730075	462.421114	7.714829
5.662742	463.773012	7.719834
5.342391	455.755274	7.724838
5.826615	464.060311	7.729843
5.905464	482.160866	7.734848
5.704396	480.211676	7.739853
5.705632	480.451812	7.744858
5.782388	482.388594	7.749862
5.872739	488.195800	7.754867
5.753301	493.504350	7.759872
5.922398	481.059618	7.764877
5.539699	474.994244	7.769882
5.755928	482.676871	7.774886
5.980064	486.757799	7.779891
5.730602	476.416170	7.784896
5.848566	470.269190	7.789901
5.514557	476.930679	7.794906
5.737351	475.339035	7.799910
5.978781	473.750798	7.804915
5.790693	469.192565	7.809920
5.985919	465.327270	7.814925
5.737061	462.562970	7.819930
5.590172	459.792185	7.824934
5.519870	457.442848	7.829939
5.585788	464.560543	7.834944
5.363108	466.420849	7.839949
5.702931	484.831704	7.844954
5.670928	483.213540	7.849958
5.759327	480.073683	7.854963
5.655391	495.292149	7.859968
5.850390	486.526079	7.864973
5.740374	484.344317	7.869978
5.989002	486.352250	7.874982
6.210053	479.037473	7.879987
5.906188	480.034114	7.884992
5.895969	475.337276	7.889997
5.491856	477.823978	7.895002
5.833435	478.583445	7.900006
5.345806	474.160731	7.905011
5.600296	487.152632	7.910016
5.919288	486.602640	7.915021
6.017790	488.532852	7.920026
5.841277	480.530532	7.925030
5.925108	489.524757	7.930035
5.817485	474.630271	7.935040
5.758349	463.442556	7.940045
5.493459	466.394676	7.945050
5.533351	476.721430	7.950054
5.528290	487.200771	7.955059
5.619310	485.243783	7.960064
5.784607	484.898212	7.965069
5.635140	489.426831	7.970074
5.971357	484.631416	7.975078
5.612425	490.581785	7.980083
5.627098	485.583642	7.985088
5.705776	480.249596	7.990093
5.987547	489.019812	7.995098
5.793329	485.367397	8.000102
5.550309	486.993603	8.005107
5.792528	478.685225	8.010112
5.512436	477.868661	8.015130
5.403340	480.602756	8.020147
5.956440	483.479249	8.025165
5.703592	489.962844	8.030182
5.829948	480.753293	8.035200
5.970558	484.275079	8.040218
5.953253	480.986189	8.045235
5.972435	472.026962	8.050253
6.018984	473.076731	8.055270
5.852456	477.855300	8.060288
5.908366	482.191924	8.065306
5.707969	488.257050	8.070323
5.544115	483.201794	8.075341
5.933493	484.472401	8.080358
5.521803	480.443736	8.085376
6.070056	482.547822	8.090394
5.970530	481.095855	8.095411
5.911450	477.810356	8.100429
5.905823	480.010692	8.105446
5.787123	485.498131	8.110464
5.914746	485.506414	8.115482
5.849530	482.101955	8.120499
6.000667	482.516805	8.125517
5.722732	485.757033	8.130534
5.471689	485.212424	8.135552
5.861870	478.252634	8.140570
5.635157	480.755851	8.145587
5.762764	475.026931	8.150605
5.836140	471.995232	8.155622
6.111026	483.666287	8.160640
6.070757	488.270444	8.165658
5.699428	489.414090	8.170675
5.369129	477.729375	8.175693
5.604900	478.102562	8.180710
5.588582	480.957819	8.185728
6.153868	482.967718	8.190746
6.015002	486.908831	8.195763
5.814395	481.641585	8.200781
5.812879	483.525699	8.205798
5.896087	501.639344	8.210816
5.793224	501.308201	8.215834
6.103467	510.853049	8.220851
6.046441	505.168827	8.225869
6.026415	506.680306	8.230886
5.762376	515.033888	8.235904
5.896571	504.248360	8.240922
5.960630	513.440465	8.245939
6.044087	513.108531	8.250957
6.351667	507.468166	8.255974
5.999240	517.173650	8.260992
6.318900	510.663550	8.266010
5.883544	497.341652	8.271027
5.860676	509.450694	8.276045
6.276529	505.421751	8.281062
5.943008	499.537857	8.286080
5.989013	497.614965	8.291098
6.042742	507.168445	8.296115
6.079604	500.241914	8.301133
6.159721	504.880861	8.306150
5.995019	516.049617	8.311168
6.046854	512.084018	8.316186
6.073820	504.010331	8.321203
5.917086	512.277671	8.326221
5.982289	515.120161	8.331238
5.868896	516.832461	8.336256
6.480208	507.133504	8.341274
6.009850	516.166349	8.346291
5.882441	512.790563	8.351309
6.375025	506.793011	8.356326
6.175419	513.839470	8.361344
6.239308	501.790022	8.366362
6.250127	508.061900	8.371379
6.153956	510.371099	8.376397
6.070574	503.125738	8.381414
6.283007	511.931680	8.386432
6.593637	504.892826	8.391450
6.533803	497.347134	8.396467
6.036829	493.802040	8.401485
6.102943	492.257848	8.406502
5.905611	484.288741	8.411520
5.890359	488.857420	8.416538
5.689245	496.784571	8.421555
5.903262	509.042689	8.426573
6.213379	511.149376	8.431590
5.985742	519.986404	8.436608
6.469171	505.589586	8.441626
6.490899	504.787645	8.446643
6.189323	520.051965	8.451661
6.392351	510.915592	8.456678
6.385013	511.194327	8.461696
6.276757	503.485807	8.466714
6.039466	505.350061	8.471731
6.027878	511.350898	8.476749
6.465325	511.143380	8.481766
6.241438	516.966045	8.486784
6.357665	509.853507	8.491802
6.100981	518.452089	8.496819
6.251444	518.292692	8.501837
6.444621	509.628075	8.506854
5.920773	519.019593	8.511872
6.233259	509.124461	8.516890
6.202575	516.567329	8.521907
6.175094	515.252393	8.526925
6.076461	518.426665	8.531942
5.890309	516.726337	8.536960
6.441415	499.024282	8.541978
6.226723	508.039155	8.546995
6.130719	501.679391	8.552013
6.487536	503.548389	8.557030
6.022215	509.557201	8.562048
6.329214	512.131433	8.567066
6.269227	513.437736	8.572083
6.440004	514.531158	8.577101
6.316189	509.094083	8.582119
6.064798	513.731326	8.587136
6.332104	504.026310	8.592154
6.166086	510.562580	8.597171
6.144184	519.884921	8.602189
6.569818	530.696105	8.607207
6.332362	530.752121	8.612224
6.356167	527.504119	8.617242
6.465153	532.952743	8.622259
6.393953	540.872182	8.627277
6.500575	534.168236	8.632295
6.119525	534.025846	8.637312
6.495148	533.108495	8.642330
6.754329	539.442456	8.647347
6.862511	530.472410	8.652365
6.334106	524.830480	8.657383
6.558467	520.676903	8.662400
6.622112	516.807282	8.667418
6.365333	518.971234	8.672435
6.245711	514.978850	8.677453
6.230198	505.327614	8.682471
6.360370	513.272294	8.687488
6.368806	521.747288	8.692506
6.888232	526.169087	8.697523
6.434538	530.288924	8.702541
6.055700	516.749874	8.707559
6.353030	533.318381	8.712576
6.406153	539.170233	8.717594
6.835545	530.074122	8.722611
6.653969	546.357917	8.727629
6.699017	540.152764	8.732647
6.714783	538.455511	8.737664
6.512402	521.351171	8.742682
6.632658	513.871929	8.747699
5.957846	512.166116	8.752717
6.368785	529.076578	8.757735
6.359507	536.440361	8.762752
6.542485	532.362693	8.767770
6.777309	540.186846	8.772787
6.401323	550.214773	8.777805
6.382055	542.732134	8.782823
6.372341	543.916954	8.787840
6.680292	540.100567	8.792858
6.581083	544.638235	8.797875
6.401400	545.171191	8.802893
6.786566	545.041291	8.807911
6.659214	543.688353	8.812928
6.495284	537.500165	8.817946
6.568349	537.867288	8.822963
6.423293	548.417607	8.827981
6.281041	540.326236	8.832999
5.869258	548.447363	8.838016
6.093126	554.894159	8.843034
6.719950	557.547674	8.848051
6.450732	560.871757	8.853069
6.875039	567.501746	8.858087
6.791496	574.466928	8.863104
6.569401	566.236577	8.868122
6.878334	573.490558	8.873139
6.983291	569.901630	8.878157
6.955336	565.904339	8.883175
6.898995	570.387959	8.888192
6.914435	553.315732	8.893210
6.851652	546.325901	8.898227
6.764332	545.462149	8.903245
6.381273	539.507109	8.908263
6.782280	549.788835	8.913280
6.557073	557.609335	8.918298
7.008294	555.282122	8.923315
6.522480	553.344722	8.928333
6.736063	564.978099	8.933351
7.103173	562.073931	8.938368
6.867761	546.716740	8.943386
6.939178	545.039169	8.948403
6.690511	543.370725	8.953421
6.399245	538.013526	8.958439
6.714169	553.585221	8.963456
6.584771	564.868396	8.968474
6.874955	564.750223	8.973491
6.683982	578.034359	8.978509
6.786576	562.078243	8.983527
7.137983	570.067179	8.988544
6.822749	566.279001	8.993562
7.216654	565.125256	8.998579
6.930245	567.789316	9.003597
6.910173	554.007834	9.008615
6.845144	548.517355	9.013632
6.653486	543.084588	9.018650
6.408276	548.178460	9.023667
6.803436	557.334490	9.028685
7.096892	556.868667	9.033703
6.931134	563.310241	9.038720
7.039328	569.702583	9.043738
6.859512	559.389098	9.048755
6.657387	561.856916	9.053773
6.657796	564.589645	9.058791
6.924583	563.831356	9.063808
6.736300	562.973955	9.068826
6.908173	561.447901	9.073843
6.854229	563.062528	9.078861
6.951655	575.604045	9.083879
7.001551	570.174448	9.088896
6.833618	574.770228	9.093914
7.062486	565.875930	9.098931
6.853364	566.527107	9.103949
7.173481	571.712290	9.108967
6.659045	569.113500	9.113984
6.909209	573.183025	9.119002
6.552694	567.129142	9.124019
6.844620	572.501779	9.129037
6.964605	568.557047	9.134055
6.698860	567.711783	9.139072
6.736605	575.686751	9.144090
7.122007	584.702312	9.149107
6.840839	592.481103	9.154125
6.683310	591.012969	9.159143
6.855987	596.426387	9.164160
7.126861	605.014935	9.169178
7.088023	602.483634	9.174195
7.117331	601.478529	9.179213
7.392475	597.253862	9.184231
6.998091	608.603828	9.189248
7.260139	614.120014	9.194266
7.228913	600.851483	9.199283
7.187749	596.988799	9.204301
7.599001	596.185783	9.209319
7.391868	584.951914	9.214336
7.092441	573.906082	9.219354
6.940120	570.994935	9.224371
7.026931	583.828454	9.229389
7.300032	580.269984	9.234407
7.089123	571.460366	9.239424
6.940558	572.575425	9.244442
7.205136	580.293949	9.249459
7.031964	593.871953	9.254477
7.255135	588.039661	9.259495
7.337171	597.175344	9.264512
7.164155	582.448974	9.269530
7.422537	573.288116	9.274547
7.532287	579.131110	9.279565
7.147900	570.702123	9.284583
7.453919	564.768496	9.289600
7.165747	566.896347	9.294618
7.185800	563.248140	9.299635
6.773399	569.823035	9.304653
6.791942	563.211774	9.309671
6.938330	583.382647	9.314688
7.268968	589.323578	9.319706
7.369756	585.953050	9.324723
7.526021	588.295291	9.329741
7.399230	589.877153	9.334759
7.337366	593.654746	9.339776
7.467586	603.644416	9.344794
7.508923	583.494352	9.349811
6.995247	575.101400	9.354829
7.085068	582.553816	9.359847
7.232525	593.323417	9.364864
7.077142	590.766196	9.369882
7.304664	593.327647	9.374899
7.048154	593.241481	9.379917
7.179048	596.326155	9.384935
7.648460	594.371628	9.389952
7.000912	600.519474	9.394970
7.406654	591.505932	9.399987
7.435432	598.825909	9.405005
6.967160	595.774914	9.410023
7.592176	595.427554	9.415040
7.284340	598.849212	9.420058
7.427180	594.067763	9.425075
7.133551	605.827975	9.430093
7.416735	591.506644	9.435111
7.200782	598.767136	9.440128
7.085314	595.651396	9.445146
7.440418	596.889512	9.450163
7.328928	591.374742	9.455181
7.489073	588.733370	9.460199
7.824271	590.255470	9.465216
7.518428	592.682739	9.470234
7.548860	592.848260	9.475251
7.406425	590.462579	9.480269
7.103952	586.792318	9.485287
7.508100	580.111166	9.490304
7.581245	588.225759	9.495322
7.477264	589.059279	9.500339
7.662838	594.533792	9.505357
7.441115	599.018086	9.510375
7.434857	594.146389	9.515392
7.306789	603.409668	9.520410
7.312473	597.090743	9.525427
7.112836	599.709654	9.530445
7.230564	615.451156	9.535463
7.374358	614.103066	9.540480
7.216953	625.845102	9.545498
7.503348	616.641964	9.550515
7.601462	630.373150	9.555533
7.276452	622.203079	9.560551
7.372467	618.337832	9.565568
6.981042	623.770215	9.570586
7.547030	623.318494	9.575603
7.488050	627.310237	9.580621
7.268891	628.376399	9.585639
7.631724	629.755318	9.590656
7.350421	651.261912	9.595674
7.942827	646.268000	9.600691
7.792025	644.590524	9.605709
7.638844	630.577374	9.610727
7.884284	622.087550	9.615744
7.663280	632.611948	9.620762
7.604522	620.988736	9.625779
7.401449	630.266937	9.630797
7.146374	635.643246	9.635815
7.772278	633.307589	9.640832
7.902292	644.562792	9.645850
7.838279	643.237791	9.650867
7.880034	650.243331	9.655885
7.884259	647.695808	9.660903
7.979809	627.025961	9.665920
7.589378	627.049141	9.670938
7.674406	609.902840	9.675955
7.696766	622.153195	9.680973
7.778547	620.259399	9.685991
7.866881	614.877415	9.691008
7.255422	621.066951	9.696026
7.543901	634.616835	9.701043
7.726382	644.140747	9.706061
7.847808	643.727123	9.711079
8.220997	644.053536	9.716096
8.017032	642.933500	9.721114
7.924494	637.974324	9.726131
7.784412	626.395408	9.731149
7.837295	626.102976	9.736167
7.786289	613.291971	9.741184
7.515245	614.495650	9.746202
7.683716	629.818960	9.751219
7.969440	643.965730	9.756237
7.967502	636.224716	9.761255
7.684396	620.098606	9.766272
7.688449	637.552605	9.771290
7.873876	634.774721	9.776307
8.317367	637.232912	9.781325
7.775999	630.797715	9.786343
7.743046	623.762155	9.791360
7.982275	639.661366	9.796378
8.331150	639.685476	9.801395
8.197768	625.176922	9.806413
7.829075	620.611313	9.811431
8.136286	615.075114	9.816448
7.797098	615.386911	9.821466
7.966537	623.006751	9.826483
7.998333	618.734999	9.831501
7.722286	620.327626	9.836519
7.933170	620.054620	9.841536
7.782947	623.202279	9.846554
8.045700	621.327465	9.851571
7.802196	613.816814	9.856589
7.884485	620.951691	9.861607
8.171746	631.598425	9.866624
7.678671	632.423482	9.871642
8.061040	640.243497	9.876659
8.113268	642.971275	9.881677
7.892740	646.773739	9.886695
8.196143	646.075981	9.891712
8.093671	653.719503	9.896730
8.257379	649.723722	9.901747
7.848851	638.291000	9.906765
7.917910	632.142013	9.911783
8.040426	642.155002	9.916800
8.047313	650.734442	9.921818
7.999882	651.287705	9.926835
8.310728	645.747771	9.931853
8.292681	649.281825	9.936871
8.429812	643.740707	9.941888
7.779905	626.182521	9.946906
8.300143	635.186450	9.951923
8.416663	628.771252	9.956941
7.934972	628.196505	9.961959
7.962385	623.717156	9.966976
8.300792	636.129440	9.971994
7.476557	641.165738	9.977011
8.141432	643.794370	9.982029
7.839617	644.573683	9.987047
8.063939	644.134469	9.992064
7.919319	645.264693	9.997082
8.149496	653.200078	10.002099
8.155802	639.865677	10.007117
8.101901	648.015983	10.012135
8.070790	652.467268	10.017152
7.805450	643.543067	10.022170
8.143119	646.961426	10.027187
8.229964	648.617118	10.032205
7.853367	647.038136	10.037223
8.422921	661.042618	10.042240
8.591456	663.417661	10.047258
8.350938	656.345181	10.052275
7.919975	644.269029	10.057293
7.919760	660.644433	10.062311
8.485880	661.644364	10.067328
8.503308	673.501050	10.072346
8.506275	669.625124	10.077363
8.611798	648.881105	10.082381
8.080781	658.709321	10.087399
8.226075	643.251372	10.092416
8.411134	649.117303	10.097434
8.267448	648.590581	10.102451
8.113184	652.982268	10.107469
8.194653	662.610379	10.112487
8.758793	666.504499	10.117504
8.656871	665.781885	10.122522
8.353455	650.744529	10.127539
8.385985	656.331403	10.132557
8.110221	649.665236	10.137575
7.948364	657.277038	10.142592
8.620010	664.316435	10.147610
8.583574	678.135011	10.152627
8.613511	669.675775	10.157645
8.385906	674.596510	10.162663
8.574684	672.168391	10.167680
8.462241	657.019057	10.172698
8.213161	663.865043	10.177715
8.505533	666.214371	10.182733
8.440577	668.483986	10.187751
8.623406	678.168808	10.192768
8.518957	682.928238	10.197786
8.744675	676.066724	10.202803
8.549591	661.242760	10.207821
7.975127	656.469540	10.212839
8.257858	667.202212	10.217856
8.607978	668.371686	10.222874
8.511801	675.389380	10.227891
8.701840	671.723984	10.232909
8.735674	674.274768	10.237927
8.634515	686.342548	10.242944
8.646264	670.457374	10.247962
8.730648	672.545800	10.252979
8.600533	669.236681	10.257997
7.994066	678.685408	10.263015
8.586597	673.871350	10.268032
8.919802	676.605603	10.273050
8.491299	673.283274	10.278067
8.779934	673.704987	10.283085
8.414674	677.441771	10.288103
8.660163	677.832375	10.293120
8.873944	671.553402	10.298138
8.538134	681.559329	10.303155
8.625215	674.195672	10.308173
8.381372	683.814804	10.313191
8.720701	676.010836	10.318208
8.327019	667.362352	10.323226
8.072736	682.262793	10.328243
8.523402	681.482001	10.333261
8.563923	674.504336	10.338279
8.705081	668.388223	10.343296
9.018497	678.222998	10.348314
8.660597	677.067118	10.353331
8.637293	672.100241	10.358349
8.325573	675.380510	10.363367
8.941789	681.317753	10.368384
8.898932	681.482135	10.373402
8.485256	684.828874	10.378419
8.787521	693.033849	10.383437
9.142506	699.217156	10.388455
8.735862	686.575430	10.393472
9.066025	681.079796	10.398490
8.737226	679.414426	10.403507
8.838636	674.374359	10.408525
8.939019	668.826368	10.413543
9.020054	677.400514	10.418560
9.201702	675.560493	10.423578
8.779979	680.685215	10.428595
9.044541	675.193549	10.433613
8.777339	675.333122	10.438631
8.722402	670.598419	10.443648
8.686414	675.186174	10.448666
8.770397	671.669940	10.453683
8.753296	680.363606	10.458701
8.236600	682.700846	10.463719
8.946134	697.087369	10.468736
9.052342	702.325041	10.473754
8.632336	703.160744	10.478771
9.322021	708.316465	10.483789
9.001332	706.028126	10.488807
9.029825	709.643262	10.493824
8.914824	711.362144	10.498842
9.104916	723.829286	10.503859
9.043582	715.649417	10.508877
9.085942	710.549164	10.513895
8.984330	705.146420	10.518912
9.117195	705.573605	10.523930
9.252046	706.944069	10.528947
9.082694	682.964183	10.533965
9.140018	678.063566	10.538983
9.169307	676.455701	10.544000
8.903895	679.851792	10.549018
8.688035	681.154127	10.554035
8.820349	687.810976	10.559053
8.763240	704.084880	10.564071
9.011939	703.184252	10.569088
9.065756	705.084966	10.574106
8.795074	712.183665	10.579123
8.955261	707.112288	10.584141
9.265728	709.812239	10.589159
9.076232	701.759755	10.594176
8.998362	699.300827	10.599194
9.031893	705.449295	10.604211
9.372378	701.103911	10.609229
9.231949	700.472536	10.614247
9.237986	704.558251	10.619264
9.430305	699.964682	10.624282
9.374734	699.275830	10.629299
9.110003	700.027243	10.634317
9.220967	700.880740	10.639335
9.123330	709.536545	10.644352
8.889029	703.703309	10.649370
9.076547	701.019762	10.654387
8.936450	692.886958	10.659405
9.218293	703.263184	10.664423
9.016068	706.993364	10.669440
9.334804	695.932653	10.674458
9.307164	705.833504	10.679475
9.379001	702.890370	10.684493
9.488441	698.672706	10.689511
9.241554	696.855645	10.694528
9.650553	699.713726	10.699546
9.277823	702.788963	10.704563
9.571363	696.181904	10.709581
9.525237	705.233580	10.714599
9.283802	701.487459	10.719616
9.255263	687.972289	10.724634
9.276673	698.490303	10.729651
9.174444	703.937359	10.734669
9.338862	702.582875	10.739687
9.110834	697.237810	10.744704
9.333558	704.057226	10.749722
9.168748	708.384306	10.754739
9.008361	697.670063	10.759757
9.489903	719.328616	10.764775
9.669210	727.085811	10.769792
9.577096	729.182963	10.774810
9.084329	726.820595	10.779827
9.197721	724.741954	10.784845
9.256132	730.914935	10.789863
9.637892	730.132313	10.794880
9.653187	726.598428	10.799898
9.758358	724.723047	10.804915
9.682763	721.560011	10.809933
9.409514	724.174695	10.814951
9.566882	726.879701	10.819968
9.779096	720.531529	10.824986
9.455781	713.664504	10.830003
9.044493	715.224680	10.835021
9.229676	718.067339	10.840039
9.445784	728.930407	10.845056
9.618442	724.772260	10.850074
9.633936	732.378397	10.855091
9.708704	726.566157	10.860109
9.724331	723.221570	10.865127
9.858045	730.285317	10.870144
9.757758	722.660661	10.875162
9.740293	723.322841	10.880179
9.886080	730.384696	10.885197
9.797733	717.469013	10.890215
9.393545	722.562597	10.895232
9.748542	710.347476	10.900250
9.797585	724.575575	10.905267
9.843290	715.350138	10.910285
9.500890	704.557111	10.915303
9.168609	706.221673	10.920320
9.640312	712.304646	10.925338
9.570870	733.374199	10.930355
9.865983	716.355827	10.935373
10.120974	722.318123	10.940391
9.508359	723.752053	10.945408
9.684049	721.436431	10.950426
9.788542	732.455846	10.955443
9.579472	723.806813	10.960461
9.997322	727.127417	10.965479
9.957660	717.694446	10.970496
9.905732	718.052755	10.975514
9.886320	727.523137	10.980531
9.985804	727.832476	10.985549
10.046449	715.436252	10.990567
9.725586	716.272201	10.995584
9.482762	714.233594	11.000602
9.679682	719.457058	11.005619
9.655760	728.331697	11.010637
10.272066	724.271298	11.015655
9.359127	730.628028	11.020672
9.739365	727.119015	11.025690
10.013441	728.672795	11.030707
9.952173	722.922896	11.035725
9.736658	728.233074	11.040743
9.865470	728.433676	11.045760
9.793810	723.168245	11.050778
9.650241	719.416254	11.055795
9.682432	726.107740	11.060813
9.848280	723.389716	11.065831
9.594462	727.099581	11.070848
9.952488	721.864659	11.075866
9.963822	720.054474	11.080883
9.898693	734.420390	11.085901
10.360046	739.839115	11.090919
10.095898	732.158078	11.095936
9.926709	725.156446	11.100954
9.946811	720.769737	11.105971
9.775869	718.770360	11.110989
10.013391	729.541711	11.116007
9.741905	740.597949	11.121024
10.256676	741.956226	11.126042
10.409870	737.838996	11.131059
9.824599	746.334535	11.136077
9.839832	750.617636	11.141095
10.005518	763.823938	11.146112
10.075269	740.693300	11.151130
10.198361	739.941739	11.156147
10.318268	744.492463	11.161165
10.710430	734.234426	11.166183
9.930264	741.921050	11.171200
10.460360	740.837475	11.176218
10.077169	732.566015	11.181235
9.766850	744.363646	11.186253
9.959101	743.967325	11.191271
10.002140	750.758107	11.196288
10.010222	740.282532	11.201306
9.863591	749.062798	11.206323
9.966314	753.152310	11.211341
10.055023	745.097243	11.216359
9.663816	746.449146	11.221376
10.002652	748.611324	11.226394
10.192679	754.586965	11.231411
10.206480	771.348440	11.236429
10.650029	771.992039	11.241447
10.491494	771.246732	11.246464
10.194260	758.155464	11.251482
10.168740	759.756188	11.256499
10.074759	778.620560	11.261517
10.560831	764.942650	11.266535
10.349571	770.716081	11.271552
10.344081	772.212681	11.276570
10.616483	770.920169	11.281587
10.349085	775.720934	11.286605
10.699125	768.082506	11.291623
10.299357	755.783638	11.296640
10.347886	749.457946	11.301658
10.415523	759.829897	11.306675
10.558865	767.510692	11.311693
10.390239	757.245832	11.316711
10.352213	762.704938	11.321728
10.685041	759.575734	11.326746
10.768768	754.008236	11.331763
10.496470	755.145848	11.336781
10.620482	746.144812	11.341799
10.537258	746.059898	11.346816
10.152487	748.212373	11.351834
10.715576	748.237634	11.356851
10.176134	742.638389	11.361869
10.466915	756.509900	11.366887
10.539180	775.146248	11.371904
10.777543	764.580929	11.376922
10.794698	754.122860	11.381939
10.266848	752.261451	11.386957
10.553813	756.883834	11.391975
10.371471	767.853537	11.396992
10.660288	768.773845	11.402010
10.790709	766.613635	11.407027
10.720161	772.585928	11.412045
10.747721	762.684805	11.417063
10.316840	746.799486	11.422080
10.542280	761.224040	11.427098
10.597560	765.541896	11.432115
10.551820	766.984841	11.437133
10.427765	772.277546	11.442151
10.371684	779.232194	11.447168
10.818515	775.662244	11.452186
10.782853	773.187225	11.457203
10.879427	776.113204	11.462221
10.901027	772.363726	11.467239
10.826441	777.437241	11.472256
10.959006	776.330741	11.477274
11.002876	778.681150	11.482291
10.619389	767.793535	11.487309
10.665819	770.367606	11.492327
10.448993	784.921434	11.497344
11.014040	778.041429	11.502362
11.289416	771.654939	11.507379
10.761774	775.571821	11.512397
10.914254	774.165553	11.517415
10.770974	772.395367	11.522432
10.805127	772.386737	11.527450
10.884831	771.657752	11.532467
10.682603	779.452658	11.537485
10.758121	776.199663	11.542503
10.620743	779.720881	11.547520
10.866814	779.379243	11.552538
11.026024	771.350988	11.557555
11.006530	781.411552	11.562573
10.819660	775.368888	11.567591
10.998352	774.744315	11.572608
10.895834	785.467991	11.577626
11.221946	779.319704	11.582643
11.102426	783.876393	11.587661
11.102744	772.903395	11.592679
11.054175	778.294728	11.597696
10.965593	769.907663	11.602714
11.060881	767.926528	11.607731
10.865764	779.018161	11.612749
11.009725	771.572968	11.617767
10.973589	773.251096	11.622784
11.037829	766.487432	11.627802
11.022229	770.469254	11.632819
10.687395	777.019447	11.637837
10.942248	769.159245	11.642855
10.711191	771.789416	11.647872
10.749510	776.053128	11.652890
10.947521	776.107187	11.657907
10.702596	783.182943	11.662925
11.323556	795.248108	11.667943
11.308430	795.932015	11.672960
11.132659	787.561758	11.677978
11.153384	775.733485	11.682995
10.796975	779.920187	11.688013
11.224363	786.606581	11.693031
11.205517	796.654429	11.698048
11.155985	802.475114	11.703066
11.845777	798.674587	11.708083
11.032257	789.725747	11.713101
11.691126	781.745434	11.718119
11.328288	776.992672	11.723136
11.043887	779.899448	11.728154
11.252055	776.306931	11.733171
11.156270	773.778216	11.738189
10.946028	777.298226	11.743207
10.939915	788.376031	11.748224
11.198466	801.110214	11.753242
11.292139	791.889845	11.758259
10.937475	799.424618	11.763277
11.167594	789.750522	11.768295
11.473497	802.654014	11.773312
11.595131	802.470729	11.778330
11.768205	794.279344	11.783347
11.306853	800.656863	11.788365
11.724872	792.108361	11.793383
11.193952	797.023004	11.798400
11.254166	791.686398	11.803418
11.277215	794.011669	11.808435
11.114237	802.576770	11.813453
11.495860	804.855328	11.818471
11.356903	800.635533	11.823488
11.345991	801.438702	11.828506
11.227317	793.192041	11.833523
11.015564	806.571122	11.838541
11.456520	801.720818	11.843559
11.425884	811.631665	11.848576
11.457313	813.223470	11.853594
12.006459	814.645797	11.858611
11.397208	814.255132	11.863629
11.464972	803.006457	11.868647
11.759573	806.463153	11.873664
11.378395	800.570847	11.878682
11.715606	805.346317	11.883699
11.693447	802.575686	11.888717
11.574938	791.005906	11.893735
11.523825	802.766119	11.898752
11.768756	809.623122	11.903770
11.742749	808.352115	11.908787
11.654677	803.430063	11.913805
11.422054	811.327576	11.918823
11.706738	802.995621	11.923840
11.998370	816.450475	11.928858
11.631369	806.989848	11.933875
11.870980	818.717144	11.938893
11.614309	813.812038	11.943911
11.718041	815.244191	11.948928
11.484735	810.190257	11.953946
11.952552	814.869526	11.958963
11.941231	820.122491	11.963981
11.870562	816.507382	11.968999
11.758156	802.134255	11.974016
11.725661	803.581440	11.979034
12.018924	811.424959	11.984051
11.864400	815.475895	11.989069
11.702720	803.922338	11.994087
11.998454	811.311029	11.999104
11.849198	808.030130	12.004122
11.899754	801.069779	12.009139
11.680155	807.491474	12.014157
12.001293	806.380674	12.019175
12.317385	807.243062	12.024192
12.066489	808.093299	12.029210
12.032724	797.337066	12.034227
11.846120	796.315287	12.039245
11.474670	794.470394	12.044263
11.873985	803.887834	12.049280
11.755741	815.507094	12.054298
11.791099	820.992589	12.059315
12.086210	818.516231	12.064333
12.174272	813.254152	12.069351
12.291122	815.160781	12.074368
12.027433	817.666682	12.079386
11.996077	817.049772	12.084403
11.791248	823.204068	12.089421
11.923756	822.425781	12.094439
12.191856	811.792659	12.099456
12.038917	823.998034	12.104474
12.231718	826.568114	12.109491
11.959228	826.162555	12.114509
11.759077	831.508227	12.119527
12.172082	821.452005	12.124544
12.085775	823.683959	12.129562
12.010961	821.306587	12.134579
11.931863	820.018651	12.139597
11.981097	826.814803	12.144615
11.906515	822.477618	12.149632
11.840185	829.200358	12.154650
12.237803	813.380832	12.159667
11.954832	828.595162	12.164685
11.962198	838.995537	12.169703
12.262022	840.769357	12.174720
12.518065	852.541439	12.179738
12.473562	841.253525	12.184755
12.223530	827.555200	12.189773
12.188808	832.814991	12.194791
12.346071	835.305432	12.199808
12.089575	841.587752	12.204826
12.462048	843.151373	12.209843
12.590621	850.244375	12.214861
12.154438	839.614285	12.219879
12.295106	840.466290	12.224896
12.500113	848.752848	12.229914
12.727626	847.284325	12.234931
11.902613	834.603901	12.239949
11.883603	840.277803	12.244967
12.320558	848.348136	12.249984
12.093788	852.230517	12.255002
12.434855	847.588358	12.260019
12.608041	857.978542	12.265037
12.276130	859.958644	12.270055
12.337646	849.455699	12.275072
12.402423	855.078608	12.280090
12.818457	847.515014	12.285107
12.341266	847.315099	12.290125
12.311815	849.512901	12.295143
12.489451	841.172455	12.300160
12.050709	845.488838	12.305178
12.065295	843.586612	12.310195
12.366458	861.915784	12.315213
12.716855	877.930335	12.320231
12.815600	867.115429	12.325248
12.740863	878.472289	12.330266
12.832301	867.955177	12.335283
12.478391	861.367447	12.340301
12.566517	864.525141	12.345319
12.218331	875.978493	12.350336
12.491791	872.789143	12.355354
12.611382	865.581262	12.360371
12.807032	872.070464	12.365389
12.689505	874.133744	12.370407
12.658498	873.245374	12.375424
12.644604	879.798969	12.380442
12.781687	873.506696	12.385459
13.077553	873.368697	12.390477
12.649292	884.070884	12.395495
12.751001	869.465337	12.400512
13.065843	869.838767	12.405530
12.911596	866.495523	12.410547
13.141636	870.230594	12.415565
12.450764	869.609716	12.420583
12.903821	864.495563	12.425600
13.016324	872.960730	12.430618
13.098706	871.152022	12.435635
13.360905	872.537260	12.440653
12.786533	861.995081	12.445671
12.974449	852.327564	12.450688
12.837531	847.873906	12.455706
12.910461	845.953070	12.460723
12.771333	854.252524	12.465741
12.918831	858.110980	12.470759
13.304586	865.166849	12.475776
12.739314	858.646951	12.480794
12.879569	862.462361	12.485811
13.154997	865.167825	12.490829
12.826341	862.558817	12.495847
13.221070	866.836136	12.500864
12.744322	856.348094	12.505882
12.788129	865.878073	12.510899
12.979295	867.659453	12.515917
13.105084	872.414418	12.520935
13.265542	871.508673	12.525952
12.901294	880.042229	12.530970
13.093982	872.368450	12.535987
12.985432	872.505256	12.541005
12.808489	880.151075	12.546023
13.131016	871.352406	12.551040
12.829800	866.429017	12.556058
13.220155	878.385202	12.561075
13.401899	878.713213	12.566093
13.601565	873.966968	12.571111
13.249166	866.918246	12.576128
13.026718	880.744032	12.581146
12.920415	880.018940	12.586163
12.961620	872.955883	12.591181
13.002676	874.953290	12.596199
13.039713	870.030553	12.601216
13.192113	865.796651	12.606234
12.832897	873.881286	12.611251
13.443047	897.110452	12.616269
13.306799	898.794811	12.621287
13.450519	895.253394	12.626304
13.318399	897.016001	12.631322
13.164548	896.938996	12.636339
13.259695	897.807603	12.641357
13.118145	907.104710	12.646375
13.672782	893.924053	12.651392
13.475745	895.816754	12.656410
13.533596	903.754003	12.661427
13.718575	894.194223	12.666445
13.664573	890.576487	12.671463
13.520561	871.891052	12.676480
13.362907	879.846277	12.681498
13.199872	884.463459	12.686515
13.698321	888.573052	12.691533
13.421585	899.645989	12.696551
13.930978	897.252814	12.701568
13.874416	887.857115	12.706586
13.813969	872.342840	12.711603
13.393420	869.328501	12.716621
13.535760	863.205824	12.721639
13.667987	854.872486	12.726656
13.468567	857.898504	12.731674
13.326004	871.998949	12.736691
13.309122	869.997508	12.741709
13.361655	889.211431	12.746727
13.523181	894.292167	12.751744
13.216127	895.059687	12.756762
13.395001	892.579440	12.761779
13.869202	893.688463	12.766797
13.363159	896.914011	12.771815
13.924026	896.702933	12.776832
14.056126	891.616970	12.781850
13.695510	897.155062	12.786867
14.003491	886.039114	12.791885
13.510695	901.232731	12.796903
13.821305	889.131743	12.801920
13.895839	905.157982	12.806938
13.695111	907.594070	12.811955
13.745972	897.032804	12.816973
13.582306	901.413401	12.821991
13.318876	903.183959	12.827008
13.461270	898.235239	12.832026
13.503223	910.618423	12.837043
13.603206	917.627568	12.842061
13.803970	924.573588	12.847079
14.060704	928.986154	12.852096
14.223572	926.467385	12.857114
13.902719	928.761347	12.862131
13.939722	930.746773	12.867149
13.634669	927.083156	12.872167
13.908701	926.386835	12.877184
13.781533	927.217691	12.882202
13.616932	926.631121	12.887219
14.116735	925.470229	12.892237
14.084494	931.111519	12.897255
14.167747	927.989832	12.902272
13.737802	917.907837	12.907290
14.017160	922.799703	12.912307
14.391884	918.587760	12.917325
14.316167	914.809317	12.922343
13.951944	913.029553	12.927360
14.374979	908.993083	12.932378
14.364733	909.960256	12.937395
14.016827	906.530580	12.942413
14.130600	919.293843	12.947431
14.449098	921.762191	12.952448
14.358390	908.007282	12.957466
14.332146	914.474461	12.962483
14.121234	916.123182	12.967501
14.246099	922.301596	12.972519
14.461756	911.856515	12.977536
14.654786	916.537839	12.982554
14.245562	919.287466	12.987571
14.606274	912.543569	12.992589
14.307560	912.012726	12.997607
14.246679	908.478117	13.002624
14.205196	905.464341	13.007642
14.048062	911.525986	13.012659
14.391861	908.691688	13.017677
13.920838	917.516551	13.022695
14.262465	911.974869	13.027712
14.286897	913.886521	13.032730
14.285491	919.396742	13.037747
14.567564	915.868359	13.042765
14.569018	920.358791	13.047783
14.478730	912.814539	13.052800
14.612433	906.447044	13.057818
14.549410	913.604805	13.062835
14.470423	914.658490	13.067853
14.348483	908.450970	13.072871
14.542002	916.641528	13.077888
14.440333	913.056503	13.082906
14.279927	913.053109	13.087923
14.124911	900.135117	13.092941
14.138161	915.650252	13.097959
14.132084	918.535533	13.102976
14.134711	928.157206	13.107994
14.437903	934.528594	13.113011
14.522199	935.304228	13.118029
14.485099	937.840916	13.123047
14.441510	935.193545	13.128064
14.546253	936.101677	13.133082
14.419890	942.802307	13.138099
14.606349	930.282078	13.143117
14.581801	943.612995	13.148135
14.746419	942.510930	13.153152
14.575850	929.712120	13.158170
14.307372	950.336580	13.163187
14.757296	954.277063	13.168205
14.583257	957.393797	13.173223
14.835287	967.582340	13.178240
15.082256	958.407296	13.183258
14.912043	967.118778	13.188275
15.152483	960.317966	13.193293
15.057903	964.135477	13.198311
14.683906	945.362921	13.203328
14.920780	944.410484	13.208346
15.033803	949.486212	13.213363
14.862777	952.772890	13.218381
14.827902	942.313395	13.223399
15.120761	946.486772	13.228416
14.950868	938.320654	13.233434
14.611941	939.153131	13.238451
15.125736	947.836331	13.243469
15.172638	957.372186	13.248487
14.936265	960.795338	13.253504
15.226370	958.297655	13.258522
14.976511	954.076265	13.263539
15.480540	944.684223	13.268557
14.900868	938.314877	13.273575
14.690169	934.835295	13.278592
15.199516	939.167258	13.283610
14.637163	965.044948	13.288627
15.098568	960.768921	13.293645
14.829963	959.207704	13.298663
14.951021	947.360442	13.303680
15.069383	952.441645	13.308698
15.101967	957.495264	13.313715
15.157729	957.432754	13.318733
15.325524	951.258721	13.323751
15.315471	961.027567	13.328768
15.113437	958.165172	13.333786
15.079323	967.978818	13.338803
15.331912	956.751582	13.343821
15.363722	955.231661	13.348839
15.312581	958.499556	13.353856
14.927609	949.922155	13.358874
15.065926	965.310439	13.363891
15.183129	954.975435	13.368909
15.339503	960.318933	13.373927
15.435331	975.426699	13.378944
15.456534	966.915041	13.383962
15.414009	970.686527	13.388979
15.495377	969.625908	13.393997
15.470631	970.746838	13.399015
15.162332	961.605141	13.404032
15.561697	967.090454	13.409050
15.647850	983.812390	13.414067
15.662807	985.444663	13.419085
15.640699	969.106927	13.424103
15.808334	961.544334	13.429120
15.235715	949.401805	13.434138
15.210708	963.865763	13.439155
15.434883	967.156797	13.444173
15.392172	980.487431	13.449191
15.858252	982.891638	13.454208
15.613817	980.427210	13.459226
15.776372	992.640073	13.464243
15.300060	981.265089	13.469261
15.794965	989.269601	13.474279
15.725869	989.769463	13.479296
15.791967	983.352572	13.484314
15.866966	990.116346	13.489331
16.088139	975.908569	13.494349
15.838240	970.481640	13.499367
15.413312	963.393749	13.504384
15.494069	967.616143	13.509402
15.650737	978.996771	13.514419
15.637366	981.725411	13.519437
15.903272	984.893143	13.524455
15.336806	988.863491	13.529472
15.685439	987.265524	13.534490
15.704323	993.435321	13.539507
15.576865	986.938299	13.544525
15.778322	984.811115	13.549543
15.587596	982.196258	13.554560
16.021999	985.773099	13.559578
15.636924	994.066970	13.564595
15.576274	976.605465	13.569613
15.970447	998.675687	13.574631
16.184833	1006.803055	13.579648
15.991028	998.167276	13.584666
15.882214	990.493348	13.589683
15.716314	1002.757680	13.594701
16.022742	1008.431141	13.599719
15.912714	1017.717054	13.604736
16.059408	1016.778744	13.609754
15.936868	1021.171861	13.614771
16.098021	1018.669127	13.619789
16.441445	1011.037945	13.624807
15.974400	1022.579441	13.629824
16.320616	1017.911185	13.634842
16.611974	1012.058605	13.639859
16.406962	1005.106659	13.644877
16.403822	993.143123	13.649895
16.192935	986.188948	13.654912
16.408794	983.466205	13.659930
16.392631	986.009087	13.664947
16.217290	984.676257	13.669965
16.181425	974.485147	13.674983
16.352243	980.643758	13.680000
15.828451	988.154615	13.685018
16.271592	990.710743	13.690035
16.345774	1011.076453	13.695053
16.569769	1002.551939	13.700071
16.262252	1000.176289	13.705088
16.440795	1008.192507	13.710106
16.166016	1001.668067	13.715123
16.104282	1013.086092	13.720141
16.728268	1005.035406	13.725159
16.779325	1011.818719	13.730176
16.469344	1008.600835	13.735194
16.412474	1001.316404	13.740211
16.085129	1005.476513	13.745229
16.216130	1006.651939	13.750247
16.198819	1011.703923	13.755264
16.658751	1004.398480	13.760282
16.392699	1011.190451	13.765299
16.263411	1007.710722	13.770317
16.467487	1011.244759	13.775335
16.550447	1012.131061	13.780352
16.785525	992.552954	13.785370
16.387370	1007.343660	13.790387
16.433048	1006.294942	13.795405
16.349576	1005.203342	13.800423
16.568412	1013.834956	13.805440
16.827385	1023.605868	13.810458
16.678858	1023.774186	13.815475
16.756243	1015.723928	13.820493
16.992022	1010.129370	13.825511
16.305777	1005.777521	13.830528
16.728967	1018.751157	13.835546
16.835308	1026.081248	13.840563
16.931556	1030.522141	13.845581
16.782743	1025.918820	13.850599
16.727299	1029.458808	13.855616
16.800873	1026.464854	13.860634
16.855323	1033.515894	13.865651
16.879886	1027.045532	13.870669
17.030113	1028.019128	13.875687
16.701585	1028.345039	13.880704
17.261157	1020.702078	13.885722
16.809536	1025.538085	13.890739
17.014340	1023.558698	13.895757
16.820342	1026.416634	13.900775
16.230175	1035.900864	13.905792
16.802332	1034.069052	13.910810
16.935279	1030.497737	13.915827
16.968248	1036.277170	13.920845
17.009970	1027.755956	13.925863
16.978394	1023.730727	13.930880
16.780089	1024.519084	13.935898
17.021138	1027.188934	13.940915
16.890781	1026.701139	13.945933
17.168406	1030.794870	13.950951
16.971572	1050.862253	13.955968
17.157784	1051.662950	13.960986
17.134865	1056.393926	13.966003
17.604057	1057.712033	13.971021
17.293153	1055.482076	13.976039
17.632241	1049.902879	13.981056
17.109590	1027.558980	13.986074
17.174632	1015.348057	13.991091
17.205616	1025.738528	13.996109
17.376957	1033.203607	14.001127
17.197642	1054.562159	14.006144
17.493240	1055.402524	14.011162
17.572595	1052.814769	14.016179
17.315016	1043.084402	14.021197
17.415610	1038.833330	14.026215
17.244473	1045.970213	14.031232
17.573957	1042.933005	14.036250
17.374111	1047.442385	14.041267
17.482113	1054.658615	14.046285
17.671338	1045.587250	14.051303
17.504699	1056.548358	14.056320
17.596668	1044.118595	14.061338
17.738754	1039.365549	14.066355
17.466561	1038.776897	14.071373
17.608115	1025.256913	14.076391
17.175061	1027.789379	14.081408
17.562405	1051.770041	14.086426
17.730578	1045.914659	14.091443
17.444202	1048.048597	14.096461
17.794723	1044.818740	14.101479
17.162846	1056.304031	14.106496
17.663599	1048.562974	14.111514
17.654742	1052.092512	14.116531
17.579274	1044.394400	14.121549
17.905787	1044.093805	14.126567
17.822813	1043.074709	14.131584
17.976065	1046.118088	14.136602
17.907154	1053.298919	14.141619
17.937602	1050.444266	14.146637
17.813901	1040.490948	14.151655
17.317633	1061.750842	14.156672
17.791912	1042.640143	14.161690
17.828820	1047.806721	14.166707
17.827837	1050.546055	14.171725
18.419343	1051.267471	14.176743
17.998789	1057.856444	14.181760
17.817071	1041.067112	14.186778
18.449996	1044.423509	14.191795
18.202795	1047.911492	14.196813
18.221827	1040.965454	14.201831
18.219636	1047.189066	14.206848
17.900785	1032.431523	14.211866
18.027803	1033.882137	14.216883
17.725522	1040.689263	14.221901
18.152335	1042.575755	14.226919
17.830647	1045.030813	14.231936
18.061977	1042.567574	14.236954
18.166756	1049.604423	14.241971
17.710491	1056.246328	14.246989
17.792132	1048.659302	14.252007
17.807815	1050.121049	14.257024
17.901819	1050.715282	14.262042
17.983805	1048.849812	14.267059
17.645193	1059.298211	14.272077
17.884607	1063.530483	14.277095
18.121565	1075.024828	14.282112
18.230824	1081.650722	14.287130
18.635770	1066.801838	14.292147
18.152556	1074.344243	14.297165
18.369565	1070.393668	14.302183
18.205525	1075.301397	14.307200
18.752994	1068.367230	14.312218
18.629562	1069.626708	14.317235
18.369911	1083.054526	14.322253
18.507193	1069.961222	14.327271
18.354506	1071.821745	14.332288
18.697032	1073.260688	14.337306
18.763074	1072.085696	14.342323
18.853409	1076.600112	14.347341
18.760414	1056.303301	14.352359
18.487345	1051.908795	14.357376
18.265758	1050.750467	14.362394
18.642698	1067.338556	14.367411
18.374674	1070.375359	14.372429
18.803102	1068.181045	14.377447
18.838224	1078.201660	14.382464
18.748520	1068.205129	14.387482
18.867116	1054.660317	14.392499
18.543697	1052.242969	14.397517
18.807291	1042.519309	14.402535
18.357860	1039.121293	14.407552
18.602041	1056.686404	14.412570
18.704300	1051.242145	14.417587
18.684481	1068.791825	14.422605
18.726590	1063.555807	14.427623
18.888662	1062.637176	14.432640
18.401425	1065.831404	14.437658
18.970332	1072.435771	14.442675
19.010082	1068.074302	14.447693
18.705537	1059.746184	14.452711
18.630509	1070.184850	14.457728
18.599494	1062.473454	14.462746
18.872212	1061.427031	14.467763
18.939817	1062.896423	14.472781
18.757763	1063.016344	14.477799
18.987196	1056.015244	14.482816
18.763207	1073.764180	14.487834
18.964147	1063.703179	14.492851
18.549948	1065.699352	14.497869
19.435862	1084.476790	14.502887
19.352776	1074.491843	14.507904
19.254309	1079.240973	14.512922
19.286383	1062.238239	14.517939
19.211442	1072.288719	14.522957
19.130082	1059.491617	14.527975
19.131645	1062.483024	14.532992
19.078610	1068.039251	14.538010
19.116607	1057.353671	14.543027
18.973822	1068.683443	14.548045
19.259797	1066.126430	14.553063
19.135098	1078.040368	14.558080
19.117369	1086.065282	14.563098
19.261013	1077.556478	14.568115
19.419805	1086.405824	14.573133
19.534847	1084.244829	14.578151
19.545356	1087.720845	14.583168
19.330177	1071.820375	14.588186
19.343253	1077.640808	14.593203
19.326875	1081.682783	14.598221
19.718657	1084.619366	14.603239
19.800958	1073.791132	14.608256
19.466313	1063.690966	14.613274
19.433045	1053.647730	14.618291
19.516101	1060.968860	14.623309
19.368416	1059.234050	14.628327
19.626527	1055.564223	14.633344
18.882326	1058.981752	14.638362
19.285991	1058.877356	14.643379
19.785002	1071.510940	14.648397
19.642545	1079.407067	14.653415
19.753530	1081.087420	14.658432
19.589091	1080.166295	14.663450
19.776124	1079.543561	14.668467
19.708882	1079.752794	14.673485
19.691377	1078.783401	14.678503
19.546394	1079.550782	14.683520
19.670780	1078.574937	14.688538
19.764033	1073.621244	14.693555
19.377609	1080.750846	14.698573
19.608052	1081.134349	14.703591
19.551930	1082.821950	14.708608
19.576321	1085.030280	14.713626
19.712390	1079.277750	14.718643
19.750971	1091.999269	14.723661
19.738600	1093.582183	14.728679
20.027422	1096.657979	14.733696
19.907244	1101.451544	14.738714
19.956721	1098.789566	14.743731
19.752903	1110.384554	14.748749
19.499246	1107.760602	14.753767
19.970387	1096.432762	14.758784
19.933774	1106.540374	14.763802
20.263566	1097.765703	14.768819
20.156036	1107.392108	14.773837
20.097537	1106.141950	14.778855
20.230603	1104.473604	14.783872
20.206910	1101.775752	14.788890
20.218354	1099.536311	14.793907
19.984497	1100.690012	14.798925
20.130155	1106.319264	14.803943
20.466911	1111.612455	14.808960
20.010796	1108.751974	14.813978
19.969332	1108.262872	14.818995
20.268034	1102.904587	14.824013
20.022503	1100.910541	14.829031
20.034278	1100.785493	14.834048
20.218486	1097.480696	14.839066
20.333873	1092.280527	14.844083
19.987250	1100.577890	14.849101
20.391692	1119.866316	14.854119
20.609978	1125.973357	14.859136
20.697000	1137.544885	14.864154
20.687137	1111.033655	14.869171
20.264702	1110.474852	14.874189
20.169730	1112.080178	14.879207
20.307358	1122.229928	14.884224
20.346436	1131.606151	14.889242
20.369948	1127.452344	14.894259
20.527094	1125.278436	14.899277
20.750218	1132.609208	14.904295
20.811591	1126.028899	14.909312
20.720497	1122.442175	14.914330
21.016834	1121.388892	14.919347
21.191343	1122.740552	14.924365
21.040344	1107.972426	14.929383
21.264685	1104.109060	14.934400
20.670300	1101.273399	14.939418
21.112510	1096.526965	14.944435
20.884538	1102.148482	14.949453
20.566344	1099.102286	14.954471
20.647283	1094.418768	14.959488
20.797011	1091.053101	14.964506
20.760283	1088.997938	14.969523
20.730817	1093.572155	14.974541
20.681929	1095.536341	14.979559
20.805371	1088.756968	14.984576
20.761258	1093.778460	14.989594
20.841345	1088.018919	14.994611
20.746578	1098.829933	14.999629
21.154899	1117.843186	15.004647
21.141000	1112.009998	15.009664
21.030912	1127.607760	15.014682
21.163342	1109.049182	15.019699
21.134666	1111.190089	15.024717
20.853165	1105.913241	15.029735
21.180048	1109.159806	15.034752
21.092795	1117.334486	15.039770
21.619943	1108.964401	15.044787
21.106783	1107.147990	15.049805
21.008155	1100.466523	15.054823
21.500794	1103.630311	15.059840
21.069547	1108.084441	15.064858
21.163919	1115.425911	15.069875
21.382290	1115.596706	15.074893
21.122270	1122.703364	15.079911
21.430493	1126.514604	15.084928
21.343301	1127.730537	15.089946
21.154689	1119.166471	15.094963
21.180729	1126.625952	15.099981
21.126640	1129.588219	15.104999
21.687207	1127.035514	15.110016
21.472806	1120.899214	15.115034
21.127354	1125.355685	15.120051
21.608489	1125.030862	15.125069
20.990997	1125.029654	15.130087
21.662462	1128.042348	15.135104
21.227227	1135.343725	15.140122
21.397983	1121.550842	15.145139
21.367164	1121.779616	15.150157
21.397584	1127.957119	15.155175
21.580390	1130.664513	15.160192
21.522632	1143.956600	15.165210
21.650365	1148.897532	15.170227
21.620470	1144.714218	15.175245
21.727369	1153.713743	15.180263
21.847359	1142.728079	15.185280
21.356416	1153.531769	15.190298
21.776441	1145.932710	15.195315
21.827178	1148.016997	15.200333
21.710579	1153.769407	15.205351
22.081048	1141.431645	15.210368
22.103591	1144.773239	15.215386
22.123907	1141.241641	15.220403
22.347250	1145.574284	15.225421
21.829415	1127.461563	15.230439
21.523771	1119.398684	15.235456
21.880921	1128.996477	15.240474
21.932945	1133.422233	15.245491
22.296935	1137.676032	15.250509
22.159191	1144.476353	15.255527
22.058048	1137.694278	15.260544
21.775683	1139.486761	15.265562
22.028305	1141.245918	15.270579
22.245768	1139.816817	15.275597
21.961376	1145.447187	15.280615
21.945766	1136.414181	15.285632
22.068338	1141.633638	15.290650
21.980776	1136.963886	15.295667
21.990297	1132.799646	15.300685
21.864598	1137.947545	15.305703
21.662320	1141.756721	15.310720
21.769055	1136.766184	15.315738
21.944552	1153.878235	15.320755
22.227959	1150.696746	15.325773
22.042170	1156.144408	15.330791
22.434343	1156.600406	15.335808
22.395284	1158.992262	15.340826
22.095542	1148.312206	15.345843
22.594808	1154.895957	15.350861
22.271440	1160.696545	15.355879
22.468632	1159.422101	15.360896
22.276300	1156.371956	15.365914
22.209814	1154.425592	15.370931
22.129875	1163.785765	15.375949
22.373176	1180.555849	15.380967
22.502281	1178.907052	15.385984
22.402187	1189.472795	15.391002
22.527102	1175.475607	15.396019
22.747051	1187.023184	15.401037
22.673287	1181.256160	15.406055
22.738600	1174.703618	15.411072
22.838544	1177.954194	15.416090
22.800508	1180.222812	15.421107
22.853902	1183.619541	15.426125
22.841469	1183.189007	15.431143
22.821926	1182.021106	15.436160
22.864696	1180.168078	15.441178
22.827995	1190.237880	15.446195
23.252846	1178.762602	15.451213
22.788953	1178.838317	15.456231
23.210977	1180.069147	15.461248
23.235981	1172.292120	15.466266
22.974255	1171.480910	15.471283
23.330919	1181.201888	15.476301
23.053949	1173.481642	15.481319
23.188940	1172.456792	15.486336
23.413765	1171.048626	15.491354
23.197836	1166.256963	15.496371
22.960116	1151.836914	15.501389
22.738339	1166.647455	15.506407
22.860809	1162.029998	15.511424
22.958622	1163.131737	15.516442
22.531133	1176.731093	15.521459
22.985548	1177.928445	15.526477
22.906717	1181.652014	15.531495
23.293685	1180.982171	15.536512
23.003837	1175.940147	15.541530
22.898450	1174.012500	15.546547
23.467776	1193.268860	15.551565
23.200171	1200.155823	15.556583
23.251361	1192.147460	15.561600
23.432976	1207.497609	15.566618
23.336595	1199.095785	15.571635
23.846168	1202.594619	15.576653
23.560351	1195.046168	15.581671
23.540257	1201.389407	15.586688
23.744937	1204.159659	15.591706
23.907980	1184.213920	15.596723
23.699849	1168.097658	15.601741
23.167523	1176.821795	15.606759
23.705459	1164.410441	15.611776
23.625245	1163.633910	15.616794
23.342198	1173.410931	15.621811
23.523554	1171.968549	15.626829
23.629909	1192.102200	15.631847
23.629607	1190.489457	15.636864
23.642998	1193.330705	15.641882
23.405639	1192.717654	15.646899
23.788207	1185.465286	15.651917
23.861939	1197.976238	15.656935
23.899907	1195.682134	15.661952
24.046503	1190.893627	15.666970
23.946849	1188.182416	15.671987
23.836131	1197.771498	15.677005
23.699947	1200.165953	15.682023
23.769329	1191.245839	15.687040
23.605226	1194.348434	15.692058
23.448133	1200.097735	15.697075
23.943993	1197.473105	15.702093
23.896871	1210.220759	15.707111
24.282887	1212.527086	15.712128
24.199666	1214.774384	15.717146
24.127867	1203.578883	15.722163
23.922253	1196.958326	15.727181
24.001776	1210.708650	15.732199
24.371184	1208.836002	15.737216
24.202668	1211.573206	15.742234
24.244351	1218.519018	15.747251
24.357504	1208.389636	15.752269
23.987976	1221.882112	15.757287
24.019385	1215.824034	15.762304
24.154723	1214.534030	15.767322
24.050935	1222.013893	15.772339
24.483912	1214.807265	15.777357
24.363627	1219.168518	15.782375
24.258636	1217.941416	15.787392
24.599485	1210.790251	15.792410
24.244609	1214.850577	15.797427
24.846511	1211.060580	15.802445
24.339720	1217.003537	15.807463
24.634235	1219.179029	15.812480
24.486109	1218.533061	15.817498
24.190132	1218.692924	15.822515
24.431693	1211.383740	15.827533
24.281491	1210.615017	15.832551
24.476674	1224.473467	15.837568
24.901333	1231.554946	15.842586
24.426183	1242.810666	15.847603
24.775598	1239.255889	15.852621
24.802382	1237.960801	15.857639
24.858251	1237.263935	15.862656
24.860174	1234.618856	15.867674
24.877713	1231.728326	15.872691
24.824362	1230.007122	15.877709
24.910884	1237.239415	15.882727
24.772084	1242.515634	15.887744
25.464159	1233.400103	15.892762
25.365899	1231.105247	15.897779
24.918409	1214.603554	15.902797
24.696528	1220.429287	15.907815
25.023559	1221.255267	15.912832
25.443742	1220.409801	15.917850
24.952425	1210.144744	15.922867
24.855380	1211.617855	15.927885
25.115522	1219.716061	15.932903
25.377782	1226.570510	15.937920
24.902470	1222.759932	15.942938
25.060743	1226.888188	15.947955
25.364271	1227.708384	15.952973
25.273144	1230.165213	15.957991
25.625833	1234.597537	15.963008
25.425031	1222.409188	15.968026
25.160084	1222.264378	15.973043
25.460954	1222.845140	15.978061
25.722103	1215.255166	15.983079
25.045270	1210.179087	15.988096
25.145137	1217.860576	15.993114
25.275199	1229.687361	15.998131
25.590538	1234.239149	16.003149
25.684310	1234.236957	16.008167
25.184074	1237.108192	16.013184
25.487749	1232.080461	16.018202
25.409029	1235.579953	16.023219
25.670387	1230.991212	16.028237
25.700342	1224.851305	16.033255
25.569194	1222.728867	16.038272
25.869029	1234.996129	16.043290
25.505036	1232.711349	16.048307
25.631004	1226.228184	16.053325
25.631645	1226.789712	16.058343
25.524820	1232.007267	16.063360
25.457622	1223.790213	16.068378
25.446766	1240.934701	16.073395
25.742046	1230.685250	16.078413
25.543622	1228.273540	16.083431
25.820943	1248.601382	16.088448
26.102683	1244.277696	16.093466
25.647650	1265.938485	16.098483
26.083555	1253.098071	16.103501
25.808524	1252.604534	16.108519
25.811135	1257.558788	16.113536
26.290987	1251.064351	16.118554
25.683184	1256.868508	16.123571
25.804076	1251.348682	16.128589
26.087400	1252.190980	16.133607
26.046942	1242.634776	16.138624
26.278767	1247.963384	16.143642
25.847306	1258.379107	16.148659
26.176029	1261.167804	16.153677
25.918461	1256.732947	16.158695
26.056118	1258.926708	16.163712
26.264129	1275.128034	16.168730
26.179108	1283.965183	16.173747
26.362887	1284.094062	16.178765
26.638289	1269.584055	16.183783
26.613015	1280.731441	16.188800
26.570330	1269.430347	16.193818
26.309799	1272.844720	16.198835
26.058329	1267.967076	16.203853
26.345696	1277.392840	16.208871
26.577644	1281.834626	16.213888
26.451187	1280.585635	16.218906
26.552367	1280.086803	16.223923
26.916126	1287.171535	16.228941
26.691476	1284.426243	16.233959
26.715291	1281.806130	16.238976
26.829116	1276.745013	16.243994
26.727114	1286.421143	16.249011
26.694202	1283.355465	16.254029
26.557020	1284.323611	16.259047
26.312062	1276.891805	16.264064
26.538507	1278.875991	16.269082
26.276738	1275.363315	16.274099
26.146699	1278.927664	16.279117
26.614869	1285.756186	16.284135
26.736775	1304.921815	16.289152
27.118442	1299.484199	16.294170
27.236818	1303.700778	16.299187
26.910113	1302.909210	16.304205
27.077025	1291.041913	16.309223
26.715925	1293.436904	16.314240
27.391558	1291.150181	16.319258
27.385018	1305.217032	16.324275
27.417716	1293.165626	16.329293
27.399797	1291.312628	16.334311
27.171581	1285.014327	16.339328
27.466393	1272.928179	16.344346
27.045401	1277.573255	16.349363
27.124387	1275.304274	16.354381
27.273139	1282.877143	16.359399
27.484827	1294.504982	16.364416
27.521870	1279.319074	16.369434
27.304392	1274.836904	16.374451
27.456703	1282.342941	16.379469
27.281319	1270.816476	16.384487
27.490619	1286.367491	16.389504
27.486540	1297.435825	16.394522
27.816527	1302.831123	16.399539
27.480727	1289.669764	16.404557
27.155694	1281.259542	16.409575
27.309447	1289.087260	16.414592
27.678169	1286.248999	16.419610
27.852644	1295.373712	16.424627
27.693392	1297.099583	16.429645
27.478198	1291.039089	16.434663
27.585542	1295.096443	16.439680
28.127159	1288.169421	16.444698
27.629830	1296.752428	16.449715
27.491176	1292.971142	16.454733
27.898431	1288.501544	16.459751
27.320142	1306.214699	16.464768
27.698456	1290.817516	16.469786
27.258364	1288.143850	16.474803
27.384573	1299.346412	16.479821
28.026446	1308.808170	16.484839
27.953425	1323.986869	16.489856
27.930144	1315.122239	16.494874
28.219870	1323.894381	16.499891
28.284349	1330.981838	16.504909
28.183601	1325.326296	16.509927
27.896874	1333.472366	16.514944
28.104104	1317.047884	16.519962
28.111338	1321.733179	16.524979
28.350808	1316.904839	16.529997
28.268585	1322.708724	16.535015
27.986618	1322.402470	16.540032
28.131806	1319.368845	16.545050
28.243325	1308.665284	16.550067
28.450912	1318.453877	16.555085
28.555863	1321.312359	16.560103
28.200240	1321.295368	16.565120
28.245290	1316.380720	16.570138
28.046050	1321.578065	16.575155
27.900635	1325.548790	16.580173
28.581422	1328.134009	16.585191
28.767593	1336.733027	16.590208
28.413685	1330.934104	16.595226
28.426554	1335.675326	16.600243
28.663285	1336.966758	16.605261
28.747602	1338.354657	16.610279
28.717800	1344.882512	16.615296
28.892374	1346.972666	16.620314
28.626131	1336.801665	16.625331
28.815822	1346.268017	16.630349
28.820297	1337.238075	16.635367
28.414279	1344.623324	16.640384
29.269069	1336.208112	16.645402
28.831614	1335.519105	16.650419
28.684343	1346.190166	16.655437
28.864189	1342.437865	16.660455
28.731330	1343.304348	16.665472
29.038711	1341.987380	16.670490
28.864722	1333.225252	16.675507
29.097509	1335.568226	16.680525
28.964429	1327.045854	16.685543
28.781449	1333.272643	16.690560
28.713207	1335.047377	16.695578
28.659938	1338.075824	16.700595
28.905735	1341.111066	16.705613
29.230148	1352.102718	16.710631
29.158883	1365.479140	16.715648
29.258697	1366.646854	16.720666
29.442189	1366.501211	16.725683
29.305453	1362.299871	16.730701
29.436454	1348.320530	16.735719
29.147972	1373.010295	16.740736
29.487318	1363.539692	16.745754
29.433213	1362.468716	16.750771
29.396522	1361.404479	16.755789
29.548532	1371.012453	16.760807
29.596647	1364.027018	16.765824
29.674868	1357.093675	16.770842
29.719527	1367.280223	16.775859
29.489015	1357.233005	16.780877
29.894054	1358.700049	16.785895
29.563895	1361.175411	16.790912
29.555406	1366.746843	16.795930
29.711745	1358.507327	16.800947
29.285880	1351.731864	16.805965
29.548960	1350.122023	16.810983
29.077066	1359.969760	16.816000
29.627942	1375.991221	16.821018
30.146037	1375.303983	16.826035
29.737580	1378.372308	16.831053
29.648835	1384.824202	16.836071
29.946796	1387.605115	16.841088
30.138494	1386.650267	16.846106
29.986594	1379.437377	16.851123
29.573269	1376.216682	16.856141
30.232720	1385.369602	16.861159
30.194362	1385.716330	16.866176
30.362518	1378.633183	16.871194
30.314867	1375.339415	16.876211
30.130964	1385.119952	16.881229
30.096368	1376.872472	16.886247
29.891240	1378.242605	16.891264
30.238162	1377.771543	16.896282
30.491970	1371.198865	16.901299
30.152941	1378.804016	16.906317
30.591426	1378.132407	16.911335
30.524603	1381.128270	16.916352
30.499078	1378.033016	16.921370
30.556320	1373.308954	16.926387
30.494013	1379.453734	16.931405
30.422051	1374.349112	16.936423
29.990947	1378.689671	16.941440
30.425421	1372.363253	16.946458
30.498607	1375.501287	16.951475
30.328264	1393.422023	16.956493
30.966305	1384.709374	16.961511
30.924357	1396.935621	16.966528
30.725787	1395.874654	16.971546
30.867276	1389.130210	16.976563
30.518933	1401.041532	16.981581
30.778389	1385.953236	16.986599
30.750711	1392.291419	16.991616
30.860413	1395.695146	16.996634
30.943012	1404.796439	17.001651
30.553335	1394.663680	17.006669
30.746857	1391.130143	17.011687
30.790247	1397.229965	17.016704
30.689505	1396.901628	17.021722
30.900273	1390.502951	17.026739
30.752845	1401.486507	17.031757
31.412261	1406.445198	17.036775
31.756179	1400.660000	17.041792
31.506261	1397.577808	17.046810
31.333973	1392.460496	17.051827
31.369652	1393.038631	17.056845
31.564936	1399.019977	17.061863
31.556431	1395.006830	17.066880
30.873611	1392.244940	17.071898
31.317046	1391.080229	17.076915
31.073050	1400.090672	17.081933
31.470651	1389.301213	17.086951
31.401182	1389.681219	17.091968
31.659733	1380.677721	17.096986
31.453551	1388.640775	17.102003
31.198610	1396.674590	17.107021
31.310166	1395.303090	17.112039
31.604562	1412.699731	17.117056
31.703680	1421.886811	17.122074
32.064190	1413.905628	17.127091
31.907385	1419.279397	17.132109
32.099413	1410.614525	17.137127
31.810481	1401.362265	17.142144
31.481437	1398.822668	17.147162
31.823523	1396.061151	17.152179
31.562722	1407.479057	17.157197
31.698976	1410.136981	17.162215
31.642713	1411.673149	17.167232
31.464933	1408.989925	17.172250
31.784660	1410.129498	17.177267
31.337238	1421.456727	17.182285
31.936432	1431.890958	17.187303
32.202731	1447.783493	17.192320
31.876368	1444.795324	17.197338
32.330793	1444.522022	17.202355
32.401854	1445.287128	17.207373
32.637032	1440.932820	17.212391
32.367946	1434.085422	17.217408
32.070409	1442.255326	17.222426
32.354276	1431.988613	17.227443
32.340281	1440.237172	17.232461
32.168582	1439.923108	17.237479
32.311203	1440.105776	17.242496
32.375730	1445.391224	17.247514
32.643410	1440.356450	17.252531
32.812775	1445.821142	17.257549
32.709004	1434.879825	17.262567
32.944960	1431.535300	17.267584
32.834409	1425.392090	17.272602
32.873789	1398.481381	17.277619
32.327461	1404.597859	17.282637
32.346911	1410.067093	17.287655
32.930444	1420.418560	17.292672
32.958988	1429.711380	17.297690
32.775932	1414.285275	17.302707
32.674744	1416.768953	17.307725
32.856776	1434.296835	17.312743
33.112813	1436.522566	17.317760
32.963242	1432.768208	17.322778
32.977526	1426.346652	17.327795
32.844457	1441.945132	17.332813
33.118328	1438.421089	17.337831
32.885144	1432.641089	17.342848
32.799439	1439.635349	17.347866
33.036854	1438.288310	17.352883
32.962776	1433.139819	17.357901
32.937153	1429.811030	17.362919
33.214160	1434.974818	17.367936
32.732801	1436.381923	17.372954
33.342104	1425.325733	17.377971
33.198450	1429.826404	17.382989
33.227491	1433.422665	17.388007
33.242193	1431.507735	17.393024
33.151618	1442.255180	17.398042
33.509261	1448.135362	17.403059
33.710633	1455.621161	17.408077
33.553227	1450.652986	17.413095
33.634482	1448.980102	17.418112
33.237956	1450.825217	17.423130
33.253533	1454.852802	17.428147
33.461493	1461.128842	17.433165
33.402446	1459.468472	17.438183
33.541797	1459.140388	17.443200
33.549976	1465.356208	17.448218
33.815808	1463.594441	17.453235
33.524284	1464.435293	17.458253
33.598764	1457.294205	17.463271
33.730449	1449.860122	17.468288
33.672016	1475.609099	17.473306
34.022841	1476.746959	17.478323
33.847618	1479.845034	17.483341
34.167457	1471.794454	17.488359
33.988956	1476.745586	17.493376
33.807781	1470.591335	17.498394
34.012063	1467.769342	17.503411
33.737477	1470.636818	17.508429
33.970361	1475.577147	17.513447
34.082553	1478.279878	17.518464
34.054133	1476.911367	17.523482
34.054538	1477.731728	17.528499
34.155471	1478.375385	17.533517
34.374435	1484.229968	17.538535
34.329185	1488.525879	17.543552
34.372084	1496.036524	17.548570
34.201762	1506.856466	17.553587
34.517872	1507.119255	17.558605
34.560549	1500.327132	17.563623
34.829352	1503.526063	17.568640
34.600002	1496.271610	17.573658
34.743970	1500.389547	17.578675
34.430330	1504.213091	17.583693
34.614278	1496.543571	17.588711
34.636643	1497.038585	17.593728
35.021406	1501.895161	17.598746
35.045806	1500.884463	17.603763
34.914640	1494.510919	17.608781
34.900573	1493.714543	17.613799
35.065191	1494.572295	17.618816
34.919892	1500.862670	17.623834
34.878461	1493.032794	17.628851
34.610658	1496.650329	17.633869
35.064610	1499.473095	17.638887
35.084476	1485.305923	17.643904
34.796099	1497.586628	17.648922
35.212916	1498.174482	17.653939
34.937972	1501.966715	17.658957
34.871815	1502.986863	17.663975
35.254910	1492.587798	17.668992
35.189389	1504.088785	17.674010
35.329070	1484.512463	17.679027
35.690546	1490.855984	17.684045
35.111734	1496.744041	17.689063
35.526628	1491.989160	17.694080
35.425113	1494.696973	17.699098
35.549425	1490.259033	17.704115
35.265627	1492.525168	17.709133
35.516987	1481.673355	17.714151
35.620952	1489.931860	17.719168
35.773542	1497.109724	17.724186
35.436909	1489.430248	17.729203
35.613228	1489.112151	17.734221
35.420741	1491.259833	17.739239
35.671489	1500.438976	17.744256
35.504632	1510.523039	17.749274
35.620778	1511.517781	17.754291
35.883345	1519.710423	17.759309
35.639404	1524.324665	17.764327
35.753865	1518.644812	17.769344
35.688653	1515.423201	17.774362
35.715023	1522.226356	17.779379
35.911663	1512.894804	17.784397
36.043447	1512.318584	17.789415
36.168572	1509.673097	17.794432
35.820125	1511.516997	17.799450
35.891873	1526.723681	17.804467
36.276301	1525.631326	17.809485
36.153080	1542.260351	17.814503
36.611709	1538.300220	17.819520
36.380191	1545.421514	17.824538
36.500441	1534.148377	17.829555
36.394098	1534.329025	17.834573
36.488661	1537.672032	17.839591
36.364961	1535.810335	17.844608
36.144971	1547.657460	17.849626
36.293589	1535.852830	17.854643
36.300151	1537.180340	17.859661
36.458896	1537.818097	17.864679
36.580974	1535.283542	17.869696
36.497759	1540.500644	17.874714
36.548990	1529.850580	17.879731
36.251846	1536.581345	17.884749
36.415775	1555.488182	17.889767
36.909220	1558.405762	17.894784
36.709890	1566.329949	17.899802
37.071183	1564.281802	17.904819
37.177371	1556.558164	17.909837
36.612705	1563.207771	17.914855
37.148847	1553.393794	17.919872
36.905927	1559.380731	17.924890
36.945787	1559.721519	17.929907
37.330969	1558.408127	17.934925
37.329630	1560.150308	17.939943
37.236913	1555.519125	17.944960
36.961743	1569.161188	17.949978
37.014767	1568.818224	17.954995
37.172366	1556.362043	17.960013
37.332078	1559.555985	17.965031
37.362890	1551.279241	17.970048
37.214996	1562.755299	17.975066
37.233127	1560.180220	17.980083
37.267911	1551.009714	17.985101
36.969254	1559.908875	17.990119
37.274178	1571.440231	17.995136
37.591893	1584.531798	18.000154
37.650601	1588.849317	18.005171
37.814769	1579.497570	18.010189
37.682797	1585.416638	18.015207
37.808916	1588.050928	18.020224
37.584207	1587.962929	18.025242
37.451048	1588.135155	18.030259
37.550986	1580.087421	18.035277
37.624817	1584.932773	18.040295
37.857223	1578.656878	18.045312
37.848343	1583.085976	18.050330
37.784345	1579.144601	18.055347
37.952477	1577.467561	18.060365
37.829355	1591.758041	18.065383
38.133630	1595.188129	18.070400
38.166579	1608.494753	18.075418
38.291356	1602.273584	18.080435
38.799992	1599.182968	18.085453
38.188757	1600.869223	18.090471
38.332172	1597.337184	18.095488
38.362580	1593.500942	18.100506
38.417857	1596.985823	18.105523
38.336013	1593.902510	18.110541
38.283397	1601.175687	18.115559
38.365301	1601.200603	18.120576
38.646674	1600.001307	18.125594
38.494827	1601.643991	18.130611
38.450440	1605.709408	18.135629
38.592809	1609.183802	18.140647
39.035651	1600.908754	18.145664
39.006676	1600.222012	18.150682
38.816883	1602.318789	18.155699
38.962133	1603.450996	18.160717
38.496836	1605.827637	18.165735
38.580970	1599.470818	18.170752
38.904185	1601.566118	18.175770
38.650373	1604.329369	18.180787
38.764047	1605.570671	18.185805
38.605641	1602.379425	18.190823
38.831297	1599.989588	18.195840
38.880388	1615.635423	18.200858
38.894946	1624.479230	18.205875
38.999803	1635.660100	18.210893
39.483193	1635.407506	18.215911
39.248812	1629.226820	18.220928
39.219484	1626.040594	18.225946
39.230310	1615.633509	18.230963
39.367713	1621.990092	18.235981
38.776867	1624.140240	18.240999
39.376394	1626.694052	18.246016
39.384365	1623.921729	18.251034
39.378785	1618.118632	18.256051
39.550353	1621.111901	18.261069
39.146410	1624.514093	18.266087
39.520027	1641.425148	18.271104
39.666474	1648.285281	18.276122
39.457081	1650.044288	18.281139
39.822658	1654.398955	18.286157
39.446732	1650.279206	18.291175
39.549177	1647.905511	18.296192
39.711150	1648.719502	18.301210
39.579584	1652.969012	18.306227
39.598677	1639.919057	18.311245
39.783380	1638.441399	18.316263
39.611205	1640.349217	18.321280
39.778706	1651.690706	18.326298
40.042192	1670.452671	18.331315
40.489340	1659.983510	18.336333
40.295427	1668.392915	18.341351
40.485564	1662.246697	18.346368
40.344241	1662.287652	18.351386
40.001447	1660.715903	18.356403
40.360058	1653.359797	18.361421
40.426540	1657.303708	18.366439
40.666087	1655.773271	18.371456
40.582727	1658.282594	18.376474
40.286770	1657.284208	18.381491
40.572534	1653.931839	18.386509
40.094553	1657.519217	18.391527
40.550478	1652.577974	18.396544
40.628996	1661.301319	18.401562
40.250903	1663.222466	18.406579
40.626839	1660.966875	18.411597
40.491842	1656.474841	18.416615
40.516536	1673.898213	18.421632
40.662483	1677.059617	18.426650
40.777897	1675.678023	18.431667
40.999315	1678.562499	18.436685
40.828170	1685.459782	18.441703
41.373058	1686.813419	18.446720
41.405927	1681.903736	18.451738
41.001187	1682.831767	18.456755
41.545961	1676.936112	18.461773
41.419210	1687.582068	18.466791
41.173590	1681.434685	18.471808
41.090446	1680.305120	18.476826
41.380905	1673.979068	18.481843
41.758839	1676.495019	18.486861
41.133281	1679.026174	18.491879
41.216515	1671.050448	18.496896
41.240345	1665.839210	18.501914
41.297754	1673.612760	18.506931
41.418495	1670.765953	18.511949
41.511866	1683.763347	18.516967
41.516304	1667.755349	18.521984
41.893028	1677.820614	18.527002
41.567843	1676.716348	18.532019
41.475449	1674.426828	18.537037
41.477635	1684.932654	18.542055
41.629181	1697.201377	18.547072
41.756056	1706.450530	18.552090
41.745232	1706.433166	18.557107
42.066473	1699.237540	18.562125
42.076525	1696.578495	18.567143
41.894995	1710.351170	18.572160
42.156700	1703.190118	18.577178
42.038464	1703.429439	18.582195
42.246869	1697.936794	18.587213
42.198095	1696.883898	18.592231
42.410501	1697.920377	18.597248
42.395387	1699.431187	18.602266
41.936312	1697.467374	18.607283
41.992996	1696.218064	18.612301
41.912097	1697.439361	18.617319
42.190809	1709.265265	18.622336
42.316288	1716.605265	18.627354
42.345306	1724.954521	18.632371
42.599112	1725.684695	18.637389
42.408544	1733.383507	18.642407
42.498203	1726.665994	18.647424
42.820334	1722.395831	18.652442
42.686507	1718.979793	18.657459
43.123752	1725.336775	18.662477
42.862976	1726.415833	18.667495
42.861446	1727.473209	18.672512
42.734927	1718.419414	18.677530
42.796442	1714.133277	18.682547
42.611356	1711.937174	18.687565
42.773072	1732.930660	18.692583
42.806719	1734.370712	18.697600
43.024700	1740.503261	18.702618
43.288962	1746.824233	18.707635
43.686041	1739.910218	18.712653
43.256351	1749.268686	18.717671
43.178214	1749.451228	18.722688
43.377512	1745.503281	18.727706
43.305497	1748.402182	18.732723
43.751303	1744.693341	18.737741
43.452476	1740.447875	18.742759
43.340117	1742.608280	18.747776
43.547395	1746.426003	18.752794
43.220361	1751.362610	18.757811
43.554020	1740.709200	18.762829
43.276325	1747.200296	18.767847
43.323478	1746.208112	18.772864
43.528591	1750.935104	18.777882
43.456999	1766.451646	18.782899
43.696133	1764.258504	18.787917
43.676599	1773.540099	18.792935
43.762950	1768.309567	18.797952
43.880054	1766.542669	18.802970
43.614056	1774.003992	18.807987
43.805392	1773.800311	18.813005
44.173071	1779.738994	18.818023
44.150565	1802.017515	18.823040
44.377596	1792.188719	18.828058
44.137290	1797.203274	18.833075
44.776079	1795.853287	18.838093
44.650100	1793.411214	18.843111
44.566870	1771.720260	18.848128
44.427617	1765.477283	18.853146
44.515174	1770.017557	18.858163
44.393856	1768.938152	18.863181
44.786786	1774.386853	18.868199
44.689587	1779.139125	18.873216
44.907276	1772.821284	18.878234
44.468658	1764.980931	18.883251
44.480087	1779.657604	18.888269
44.880379	1789.189030	18.893287
44.773865	1787.138409	18.898304
44.898707	1782.078580	18.903322
44.983202	1782.914184	18.908339
44.769549	1786.554853	18.913357
44.926250	1776.121663	18.918375
44.992598	1783.543543	18.923392
44.551316	1777.824439	18.928410
44.460857	1781.278537	18.933427
44.865145	1787.306168	18.938445
45.039750	1792.997378	18.943463
45.052349	1799.777548	18.948480
44.932811	1792.572045	18.953498
45.048356	1806.534949	18.958515
44.767528	1804.969258	18.963533
45.022745	1799.892153	18.968551
45.129272	1825.265469	18.973568
45.109980	1830.002393	18.978586
45.394305	1828.689004	18.983603
45.547985	1826.436655	18.988621
46.041229	1827.454389	18.993639
45.428274	1830.182419	18.998656
45.575972	1831.986489	19.003674
45.529786	1828.746060	19.008691
45.852019	1830.052538	19.013709
45.786758	1826.067122	19.018727
45.514389	1827.242682	19.023744
45.639130	1833.071114	19.028762
45.775876	1848.444624	19.033779
45.842163	1851.927830	19.038797
46.331856	1847.868086	19.043815
46.050370	1852.103259	19.048832
46.399965	1836.514436	19.053850
46.377098	1846.263681	19.058867
46.413887	1845.910631	19.063885
46.391957	1849.511806	19.068903
46.402480	1848.689469	19.073920
46.477894	1845.458390	19.078938
46.563527	1842.736985	19.083955
46.552821	1836.284481	19.088973
46.316989	1855.642459	19.093991
46.405084	1848.423338	19.099008
46.754670	1837.341312	19.104026
46.289000	1850.255990	19.109043
46.754763	1856.229829	19.114061
46.852456	1866.146401	19.119079
47.186082	1876.729807	19.124096
46.982948	1869.373257	19.129114
46.900721	1856.361112	19.134131
47.193815	1865.937779	19.139149
47.619604	1862.957936	19.144167
47.360353	1853.281040	19.149184
47.252460	1840.948315	19.154202
47.259409	1838.725266	19.159219
46.965424	1843.805053	19.164237
47.230120	1840.506446	19.169255
47.136537	1843.582323	19.174272
47.321113	1859.043030	19.179290
47.432004	1867.142823	19.184307
47.180677	1868.760088	19.189325
47.424511	1859.099048	19.194343
47.021808	1871.315863	19.199360
47.637257	1865.159748	19.204378
47.259573	1867.516384	19.209395
47.266403	1865.744661	19.214413
47.716064	1875.716555	19.219431
47.341569	1885.157970	19.224448
47.855913	1893.140910	19.229466
48.120125	1899.790171	19.234483
48.047169	1896.446620	19.239501
48.269878	1894.202384	19.244519
48.130587	1892.731282	19.249536
48.370957	1885.942757	19.254554
48.214859	1890.514925	19.259571
48.022788	1888.171562	19.264589
48.201682	1897.046564	19.269607
48.043527	1891.201008	19.274624
48.376253	1890.763719	19.279642
48.045288	1890.083251	19.284659
48.112377	1897.520842	19.289677
48.022034	1887.489237	19.294695
47.947683	1886.295161	19.299712
48.401968	1894.287511	19.304730
48.533968	1907.402100	19.309747
48.611429	1913.544101	19.314765
48.693727	1905.738843	19.319783
48.642815	1912.377517	19.324800
48.792709	1915.137529	19.329818
48.654855	1915.067479	19.334835
48.888851	1917.606016	19.339853
48.706463	1918.764328	19.344871
48.808334	1907.503303	19.349888
49.136319	1914.413997	19.354906
49.118810	1904.257354	19.359923
48.798661	1912.503601	19.364941
49.005611	1906.730234	19.369959
48.885850	1907.231747	19.374976
49.175077	1916.215714	19.379994
49.394538	1931.371194	19.385011
49.451019	1929.036224	19.390029
49.693995	1933.921446	19.395047
49.336014	1934.264609	19.400064
49.070955	1934.062999	19.405082
49.148534	1931.207133	19.410099
49.152486	1930.275360	19.415117
49.667916	1928.401854	19.420135
49.744214	1928.964175	19.425152
49.778678	1927.920317	19.430170
49.662257	1934.992171	19.435187
49.404852	1950.042486	19.440205
49.554929	1953.077050	19.445223
49.752152	1955.431992	19.450240
50.159677	1952.871593	19.455258
50.229079	1957.395823	19.460275
50.122105	1954.549933	19.465293
50.214741	1958.126868	19.470311
50.063381	1951.084088	19.475328
50.111626	1950.262148	19.480346
50.105511	1949.161526	19.485363
49.593952	1957.235796	19.490381
49.830559	1963.958839	19.495399
50.209808	1974.352105	19.500416
50.745870	1987.002628	19.505434
50.430626	1973.250519	19.510451
50.073163	1984.096912	19.515469
50.630561	1987.840896	19.520487
50.616259	1987.726239	19.525504
50.746222	1989.744559	19.530522
50.960309	1994.706913	19.535539
50.857225	2000.321766	19.540557
51.012441	2004.409653	19.545575
50.835500	2003.645084	19.550592
50.871263	1994.660405	19.555610
51.230400	1999.972448	19.560627
51.172548	1994.628735	19.565645
51.569505	1993.761626	19.570663
51.190776	1999.687930	19.575680
51.465240	1989.476025	19.580698
51.613134	1997.737350	19.585715
51.464502	2000.196981	19.590733
51.838648	1992.377521	19.595751
51.638057	1984.411408	19.600768
51.442681	1972.000774	19.605786
51.651121	1974.581196	19.610803
51.324508	1977.579989	19.615821
51.616826	1984.663568	19.620839
51.575324	2000.478578	19.625856
51.567597	1987.000195	19.630874
51.521360	1985.782770	19.635891
51.635077	1994.005263	19.640909
51.602076	1986.192787	19.645927
52.002587	1990.614653	19.650944
51.874620	1985.512318	19.655962
51.828269	1994.141772	19.660979
51.666735	2002.741935	19.665997
51.992316	2009.555204	19.671015
51.889041	2014.056007	19.676032
52.138290	2012.599766	19.681050
51.916163	2018.425795	19.686067
51.773747	2024.482353	19.691085
52.120410	2024.181744	19.696103
52.285157	2029.940851	19.701120
52.415097	2040.770879	19.706138
52.616579	2038.460518	19.711155
52.212204	2039.464254	19.716173
52.656041	2033.325502	19.721191
52.781817	2031.749738	19.726208
52.695403	2034.373209	19.731226
52.830373	2028.090332	19.736243
52.546779	2033.957557	19.741261
52.972470	2028.418144	19.746279
53.118707	2031.017787	19.751296
53.084559	2042.170194	19.756314
53.272111	2047.629064	19.761331
52.999173	2060.822990	19.766349
53.631456	2052.669547	19.771367
53.487251	2058.025752	19.776384
53.424386	2046.036153	19.781402
53.518619	2036.379521	19.786419
53.520550	2045.900910	19.791437
53.633518	2040.022294	19.796455
53.727387	2037.504714	19.801472
53.361121	2044.571571	19.806490
53.421925	2040.433802	19.811507
53.341667	2047.200209	19.816525
53.714594	2049.092099	19.821543
53.814921	2063.152269	19.826560
53.651340	2059.172738	19.831578
53.960191	2055.854550	19.836595
53.515217	2072.010571	19.841613
53.827287	2054.985118	19.846631
54.125485	2051.599167	19.851648
53.758283	2075.497436	19.856666
54.205368	2072.485818	19.861683
53.789786	2086.708894	19.866701
53.883845	2077.399434	19.871719
54.079766	2079.801937	19.876736
53.731028	2082.160377	19.881754
54.577265	2081.251278	19.886771
54.746461	2104.191316	19.891789
54.899962	2100.174721	19.896807
54.817339	2088.374398	19.901824
54.777788	2082.759525	19.906842
54.646617	2077.222130	19.911859
54.920225	2084.974609	19.916877
54.775608	2086.666700	19.921895
54.781946	2091.222938	19.926912
54.497985	2096.534773	19.931930
54.889470	2096.366008	19.936947
54.918571	2106.905736	19.941965
55.083476	2101.880569	19.946983
55.016432	2104.873431	19.952000
55.093992	2113.603459	19.957018
55.251119	2100.411612	19.962035
54.984972	2101.939694	19.967053
55.152367	2094.499749	19.972071
55.402776	2109.540070	19.977088
55.534014	2122.266739	19.982106
55.614189	2116.147063	19.987123
55.676102	2126.889963	19.992141
55.760426	2126.794571	19.997159
55.911617	2129.109407	20.002176
55.695578	2119.971596	20.007194
55.830350	2119.003537	20.012211
55.712694	2129.392688	20.017229
55.672021	2121.107945	20.022247
56.073998	2121.761269	20.027264
55.631279	2128.480345	20.032282
56.160040	2120.926963	20.037299
55.778160	2123.091768	20.042317
55.780594	2111.517965	20.047335
55.894534	2120.583151	20.052352
56.023847	2130.106719	20.057370
56.309455	2130.320646	20.062387
56.603434	2143.930781	20.067405
56.812010	2137.699455	20.072423
56.698607	2138.941654	20.077440
56.454946	2147.002441	20.082458
56.802194	2139.139791	20.087475
56.707807	2142.102226	20.092493
56.341326	2125.435505	20.097511
56.391170	2130.180612	20.102528
56.871336	2133.261329	20.107546
56.924845	2136.020696	20.112563
56.667019	2135.221452	20.117581
56.760994	2141.471406	20.122599
57.108249	2140.861408	20.127616
56.858333	2158.653351	20.132634
57.409979	2167.959278	20.137651
57.299693	2164.034495	20.142669
57.474661	2160.901380	20.147687
57.380147	2159.416930	20.152704
57.167975	2152.800200	20.157722
57.255563	2157.078614	20.162739
57.155535	2149.948812	20.167757
57.378221	2159.741813	20.172775
57.374727	2161.733720	20.177792
57.587631	2169.505216	20.182810
57.747758	2175.965743	20.187827
58.003749	2186.261669	20.192845
58.099086	2192.994307	20.197863
57.989738	2188.261415	20.202880
57.875571	2182.692919	20.207898
58.046714	2173.961518	20.212915
57.981338	2180.028151	20.217933
57.657750	2182.726675	20.222951
57.991135	2170.106818	20.227968
57.872839	2186.047641	20.232986
58.033576	2194.707867	20.238003
58.376361	2206.034869	20.243021
58.226762	2206.143398	20.248039
58.551490	2202.503932	20.253056
58.490088	2210.024906	20.258074
58.571687	2203.627242	20.263091
58.266738	2208.585762	20.268109
58.431902	2207.322576	20.273127
58.447702	2212.404428	20.278144
58.585454	2233.907228	20.283162
58.463993	2220.913589	20.288179
58.745682	2231.966132	20.293197
58.737370	2223.717300	20.298215
59.041335	2222.918405	20.303232
58.802896	2229.293060	20.308250
59.356304	2233.375423	20.313267
59.683078	2250.013502	20.318285
59.376254	2229.436409	20.323303
59.608571	2223.393855	20.328320
59.260883	2222.135274	20.333338
59.145335	2226.593867	20.338355
59.644267	2239.818483	20.343373
59.512533	2237.108982	20.348391
60.067174	2245.142578	20.353408
59.875490	2249.909778	20.358426
60.388912	2240.143175	20.363443
59.757849	2237.742300	20.368461
59.407858	2246.646686	20.373479
59.870297	2243.519015	20.378496
59.939264	2239.301019	20.383514
60.017438	2236.975235	20.388531
59.801228	2240.139826	20.393549
60.026348	2239.299630	20.398567
60.043172	2237.845069	20.403584
59.895214	2253.263533	20.408602
60.539718	2263.246146	20.413619
60.812631	2269.202998	20.418637
60.825082	2273.288066	20.423655
61.069609	2274.246957	20.428672
60.860101	2267.424622	20.433690
60.559897	2249.633300	20.438707
60.427277	2251.686477	20.443725
60.775261	2268.441181	20.448743
60.966854	2260.492403	20.453760
60.798102	2270.261578	20.458778
60.891809	2264.868790	20.463795
61.046893	2274.154846	20.468813
60.675274	2271.808002	20.473831
60.867051	2269.047810	20.478848
61.276303	2278.470788	20.483866
61.369500	2274.312110	20.488883
61.681361	2291.501724	20.493901
61.212110	2294.191526	20.498919
61.350565	2288.857997	20.503936
61.464144	2293.309113	20.508954
61.813430	2297.417160	20.513971
61.387958	2291.632290	20.518989
61.334698	2305.953421	20.524007
61.753443	2292.758318	20.529024
61.787954	2297.395408	20.534042
61.748060	2291.180865	20.539059
61.839674	2295.105199	20.544077
61.739270	2295.136587	20.549095
61.914027	2310.602378	20.554112
61.260779	2322.211750	20.559130
61.828049	2317.180293	20.564147
62.025512	2325.493969	20.569165
61.836369	2335.219033	20.574183
62.467273	2336.508749	20.579200
62.228822	2345.676601	20.584218
62.199078	2344.598593	20.589235
62.412068	2343.444681	20.594253
61.988714	2344.533465	20.599271
62.813624	2356.002797	20.604288
62.868737	2365.175163	20.609306
62.891643	2362.245736	20.614323
63.194169	2369.040663	20.619341
63.103252	2376.386432	20.624359
63.370755	2361.321308	20.629376
63.222121	2365.690435	20.634394
62.828112	2364.085617	20.639411
63.633066	2360.115235	20.644429
63.189284	2361.017854	20.649447
63.591385	2356.968565	20.654464
63.271888	2367.282169	20.659482
63.381972	2353.289543	20.664499
63.581122	2358.658321	20.669517
63.095200	2350.225460	20.674535
63.472680	2348.821693	20.679552
63.567785	2347.048717	20.684570
63.487210	2354.440198	20.689587
63.368589	2362.049103	20.694605
63.405647	2369.286448	20.699623
63.695327	2376.342192	20.704640
63.816176	2388.057565	20.709658
63.836872	2383.774508	20.714675
64.044120	2381.927149	20.719693
64.070492	2387.452406	20.724711
64.296097	2387.363282	20.729728
64.543250	2399.964680	20.734746
64.274075	2403.888753	20.739763
64.690458	2396.927278	20.744781
63.888401	2405.407058	20.749799
64.526476	2398.780114	20.754816
64.344454	2405.802464	20.759834
64.261296	2400.405784	20.764851
64.631366	2410.194768	20.769869
64.693379	2412.406837	20.774887
64.871928	2419.012903	20.779904
64.696480	2425.709151	20.784922
65.172569	2423.519835	20.789939
65.430377	2414.171921	20.794957
64.965131	2423.369033	20.799975
65.389981	2420.209349	20.804992
65.158147	2426.822904	20.810010
65.252376	2420.177007	20.815027
65.394454	2417.222588	20.820045
65.283877	2424.129600	20.825063
65.171526	2428.385750	20.830080
65.457345	2442.742236	20.835098
65.566865	2447.620103	20.840115
65.771255	2435.888205	20.845133
65.676999	2445.421719	20.850151
65.854469	2441.574880	20.855168
65.906206	2442.112660	20.860186
66.009347	2440.300542	20.865203
65.779879	2449.018870	20.870221
65.995171	2463.575790	20.875239
66.218323	2469.893991	20.880256
66.302834	2471.143078	20.885274
66.239037	2463.571929	20.890291
66.681740	2468.315542	20.895309
66.616737	2472.990362	20.900327
66.492499	2465.965223	20.905344
66.571763	2457.617347	20.910362
66.405658	2464.435235	20.915379
66.806119	2461.967400	20.920397
66.432635	2467.176593	20.925415
66.730200	2471.936634	20.930432
66.920895	2481.826351	20.935450
66.610089	2485.005805	20.940467
66.917285	2480.977670	20.945485
67.106296	2483.333969	20.950503
67.204939	2480.686177	20.955520
67.167537	2479.959691	20.960538
66.991538	2480.274350	20.965555
67.337570	2489.202364	20.970573
67.402011	2499.812533	20.975591
67.562619	2503.618794	20.980608
67.870747	2507.988985	20.985626
67.614018	2506.889719	20.990643
67.779071	2503.088998	20.995661
67.948044	2503.630505	21.000679
68.012854	2503.244648	21.005696
67.881209	2512.313791	21.010714
67.498451	2499.089462	21.015731
67.911291	2501.792587	21.020749
68.271450	2502.348326	21.025767
67.341601	2496.639256	21.030784
67.619173	2508.472180	21.035802
68.127032	2525.902739	21.040819
68.295677	2523.468060	21.045837
68.381077	2526.361360	21.050855
68.215307	2530.367100	21.055872
68.269485	2535.001171	21.060890
68.385693	2541.683328	21.065907
68.682157	2545.231602	21.070925
68.623174	2552.184234	21.075943
68.975718	2546.384696	21.080960
68.833300	2552.204721	21.085978
68.635421	2549.253044	21.090995
68.729915	2550.844593	21.096013
69.188330	2568.633272	21.101031
69.525514	2568.974839	21.106048
69.491178	2570.665477	21.111066
69.660431	2577.276215	21.116083
69.665663	2573.358492	21.121101
69.258275	2566.636480	21.126119
69.427489	2571.186258	21.131136
69.621117	2570.941180	21.136154
69.347319	2563.150398	21.141171
69.778223	2571.200372	21.146189
69.526166	2567.165154	21.151207
69.945881	2560.831167	21.156224
70.135921	2578.450441	21.161242
70.016643	2589.288285	21.166259
70.454370	2584.122399	21.171277
70.157407	2589.101864	21.176295
70.549404	2592.890828	21.181312
70.778640	2594.319244	21.186330
70.675031	2589.850463	21.191347
70.687507	2588.115659	21.196365
70.423782	2587.535092	21.201383
70.585443	2587.957814	21.206400
70.656557	2585.866646	21.211418
71.124538	2592.443211	21.216435
71.043032	2586.301365	21.221453
70.722874	2587.866353	21.226471
70.995239	2591.954958	21.231488
71.169723	2584.258053	21.236506
71.098304	2592.999030	21.241523
70.901106	2591.884120	21.246541
71.124617	2597.924569	21.251559
70.898309	2591.120523	21.256576
70.869390	2610.617325	21.261594
70.998945	2615.618346	21.266611
71.224322	2617.284079	21.271629
71.423849	2616.785584	21.276647
71.676663	2636.894756	21.281664
71.623915	2632.872483	21.286682
71.696853	2639.103813	21.291699
71.682188	2642.704008	21.296717
71.716176	2646.467015	21.301735
71.657437	2642.884384	21.306752
72.085123	2640.708939	21.311770
71.476868	2658.876289	21.316787
72.118673	2660.230603	21.321805
71.826256	2672.358088	21.326823
72.379789	2675.200161	21.331840
72.513198	2677.195926	21.336858
72.177161	2673.322181	21.341875
72.297328	2665.463319	21.346893
72.450456	2681.245278	21.351911
72.832281	2697.266006	21.356928
72.658714	2691.637222	21.361946
72.840892	2706.818136	21.366963
72.987616	2694.154566	21.371981
73.025628	2693.930711	21.376999
72.828040	2691.670167	21.382016
73.388660	2695.947190	21.387034
73.212457	2694.519679	21.392051
73.467200	2682.773419	21.397069
73.232663	2686.225014	21.402087
73.240952	2696.926157	21.407104
73.607451	2704.913690	21.412122
73.548902	2712.705857	21.417139
73.833705	2715.227080	21.422157
73.592771	2716.078997	21.427175
73.821429	2716.106173	21.432192
74.095161	2717.256196	21.437210
73.671257	2711.912808	21.442227
73.964817	2709.957208	21.447245
73.822786	2709.439631	21.452263
74.112037	2720.163049	21.457280
74.331029	2727.981176	21.462298
74.207736	2729.742577	21.467315
74.447853	2739.129174	21.472333
74.584506	2733.786328	21.477351
74.054724	2736.491989	21.482368
74.567420	2732.529444	21.487386
74.205613	2734.659613	21.492403
74.789953	2747.079024	21.497421
75.069151	2751.195000	21.502439
74.955431	2751.979645	21.507456
75.164048	2754.257160	21.512474
75.253904	2763.421129	21.517491
75.441520	2758.966647	21.522509
75.406681	2756.103014	21.527527
75.105709	2765.451308	21.532544
75.409244	2751.885711	21.537562
75.397717	2759.042452	21.542579
75.492412	2754.040729	21.547597
75.573217	2750.739207	21.552615
75.737741	2751.429760	21.557632
75.792131	2757.354731	21.562650
75.744701	2779.243845	21.567667
75.873496	2774.441925	21.572685
75.982306	2773.058127	21.577703
75.941726	2784.884268	21.582720
75.793204	2775.969102	21.587738
76.028261	2773.249397	21.592755
76.333867	2778.844648	21.597773
76.525660	2786.559751	21.602791
76.349196	2803.816895	21.607808
76.596711	2796.701821	21.612826
76.554260	2801.366881	21.617843
76.967324	2804.518196	21.622861
76.770001	2798.085117	21.627879
76.847861	2800.462028	21.632896
76.824867	2792.290984	21.637914
76.756645	2809.594299	21.642931
76.940049	2792.619872	21.647949
76.891374	2794.555804	21.652967
76.619627	2802.949526	21.657984
77.419568	2815.322581	21.663002
77.235109	2821.635332	21.668019
77.053807	2821.849829	21.673037
77.152407	2825.710060	21.678055
77.127787	2821.645463	21.683072
77.403929	2835.299949	21.688090
77.178549	2844.794250	21.693107
77.369043	2834.159470	21.698125
77.573465	2835.642292	21.703143
77.395247	2840.161354	21.708160
77.983961	2853.473356	21.713178
78.262447	2863.510495	21.718195
78.247420	2856.932054	21.723213
78.272259	2858.689197	21.728231
78.347471	2861.659897	21.733248
78.199829	2865.517685	21.738266
78.139057	2865.356649	21.743283
78.660869	2860.710909	21.748301
78.590849	2870.067259	21.753319
78.637708	2885.926015	21.758336
78.670731	2880.719298	21.763354
78.796136	2881.419141	21.768371
78.913159	2890.332735	21.773389
78.906925	2885.832843	21.778407
78.745050	2889.512963	21.783424
79.072920	2893.340445	21.788442
79.090453	2903.510021	21.793459
79.091341	2906.785900	21.798477
79.403677	2901.068297	21.803495
79.084268	2912.862458	21.808512
79.434268	2898.935975	21.813530
79.658137	2911.762315	21.818547
79.523731	2928.261811	21.823565
79.841623	2928.107728	21.828583
79.851328	2923.794702	21.833600
79.843819	2924.411216	21.838618
80.057217	2923.765355	21.843635
80.012170	2923.788070	21.848653
80.067750	2937.167881	21.853671
80.410903	2953.611517	21.858688
80.641204	2954.645268	21.863706
80.590968	2951.364240	21.868723
80.447360	2950.783780	21.873741
80.727207	2955.969658	21.878759
80.438446	2951.993759	21.883776
80.644536	2950.146524	21.888794
80.573315	2953.566270	21.893811
81.021674	2964.381686	21.898829
81.231396	2971.301849	21.903847
81.294689	2980.372248	21.908864
81.676237	2965.989433	21.913882
81.756664	2972.642638	21.918899
81.540978	2977.060293	21.923917
81.955496	2979.463389	21.928935
82.017567	2977.083220	21.933952
82.070146	2961.195933	21.938970
81.869792	2946.705459	21.943987
81.500615	2941.744798	21.949005
81.675772	2958.157947	21.954023
81.704270	2968.202749	21.959040
81.975572	2968.677740	21.964058
81.813815	2974.680834	21.969075
81.927517	2970.360973	21.974093
81.982796	2976.648842	21.979111
81.832928	2997.351751	21.984128
82.293818	2988.240003	21.989146
82.330020	2993.991153	21.994163
82.481937	2997.890412	21.999181
82.328696	3000.114183	22.004199
82.207671	3019.133488	22.009216
82.723384	3021.792170	22.014234
83.132054	3017.940549	22.019251
82.842917	3017.275575	22.024269
82.850516	3018.243222	22.029287
82.666585	3017.504952	22.034304
82.916237	3029.004878	22.039322
83.250961	3034.529367	22.044339
83.190819	3038.234609	22.049357
83.244429	3030.546984	22.054375
83.426644	3043.323131	22.059392
83.773340	3033.455975	22.064410
83.666544	3034.277422	22.069427
83.745852	3054.925553	22.074445
84.250714	3058.987308	22.079463
83.882037	3068.835581	22.084480
83.846467	3063.368122	22.089498
84.122516	3067.181666	22.094515
84.108175	3068.209566	22.099533
84.524516	3055.434064	22.104551
84.333764	3066.838888	22.109568
84.466786	3062.998882	22.114586
84.599477	3062.173130	22.119603
84.341354	3067.664262	22.124621
84.412616	3072.128514	22.129639
84.592065	3087.660519	22.134656
84.825760	3085.335510	22.139674
84.736342	3083.891215	22.144691
84.981381	3096.714370	22.149709
85.198681	3102.168901	22.154727
84.965726	3105.418328	22.159744
85.223798	3115.263120	22.164762
85.437145	3113.020201	22.169779
85.345692	3104.957585	22.174797
85.468052	3110.259713	22.179815
85.322089	3129.131541	22.184832
85.537767	3134.198118	22.189850
85.875792	3138.901499	22.194867
85.743133	3135.440820	22.199885
85.915395	3133.497867	22.204903
86.039441	3145.689826	22.209920
86.081317	3151.209732	22.214938
86.434074	3164.502121	22.219955
86.289136	3164.862424	22.224973
86.692434	3163.006365	22.229991
86.519882	3161.732900	22.235008
86.895461	3160.805965	22.240026
86.969017	3158.332443	22.245043
86.997413	3163.024370	22.250061
86.987125	3164.067421	22.255079
86.963491	3163.588095	22.260096
86.967458	3160.061818	22.265114
86.607365	3159.357455	22.270131
86.923296	3169.347867	22.275149
87.008084	3175.833183	22.280167
87.617097	3183.880778	22.285184
87.992000	3183.241168	22.290202
87.992978	3181.845827	22.295219
87.553700	3183.672559	22.300237
87.570711	3178.641858	22.305255
87.388008	3189.546811	22.310272
87.645266	3194.398579	22.315290
88.397911	3197.998607	22.320307
88.166295	3202.194718	22.325325
88.072854	3203.449643	22.330343
88.084474	3214.974355	22.335360
88.084290	3201.367631	22.340378
88.401015	3203.574610	22.345395
88.257880	3212.724811	22.350413
88.698904	3218.579891	22.355431
88.620469	3234.925710	22.360448
88.480030	3221.583976	22.365466
88.699056	3231.289761	22.370483
88.551977	3232.938156	22.375501
88.672717	3233.146367	22.380519
89.200186	3246.531382	22.385536
89.181247	3255.472771	22.390554
89.421250	3249.734829	22.395571
89.133474	3255.517883	22.400589
89.651252	3256.011080	22.405607
89.427515	3258.555241	22.410624
89.622038	3250.147911	22.415642
89.716505	3247.753163	22.420659
89.561374	3270.846502	22.425677
89.761299	3277.073939	22.430695
89.553016	3272.652950	22.435712
89.561555	3275.589976	22.440730
89.750745	3284.262051	22.445747
90.211982	3303.139930	22.450765
90.115146	3299.638888	22.455783
90.268881	3301.195972	22.460800
90.326117	3308.919756	22.465818
90.165084	3310.254716	22.470835
90.321527	3322.429094	22.475853
90.594815	3314.896307	22.480871
90.701400	3323.111057	22.485888
90.692185	3336.756974	22.490906
90.931487	3348.457571	22.495923
91.260241	3347.780997	22.500941
91.013255	3346.800090	22.505959
91.366339	3348.767826	22.510976
91.204164	3371.196420	22.515994
91.732252	3375.235672	22.521011
91.679316	3376.067633	22.526029
92.019846	3374.928395	22.531047
91.803086	3378.904435	22.536064
91.825035	3374.046503	22.541082
92.147163	3364.820586	22.546099
92.095252	3374.076515	22.551117
92.107346	3369.475787	22.556135
92.276166	3387.897718	22.561152
92.519766	3393.143059	22.566170
92.486625	3386.665109	22.571187
92.599371	3400.301435	22.576205
92.857246	3396.665894	22.581223
93.115318	3384.940751	22.586240
92.976970	3395.198152	22.591258
92.830296	3393.677582	22.596275
92.961957	3400.909988	22.601293
92.969206	3397.020178	22.606311
92.967332	3402.398669	22.611328
93.060066	3411.167980	22.616346
93.288562	3409.642288	22.621363
93.265212	3425.051698	22.626381
92.967670	3430.261892	22.631399
93.710093	3437.887851	22.636416
93.549305	3445.566943	22.641434
93.784662	3436.733341	22.646451
93.844426	3435.770652	22.651469
93.959779	3442.484841	22.656487
94.475740	3462.241233	22.661504
94.214698	3459.649651	22.666522
94.240480	3466.365257	22.671539
94.228906	3468.055570	22.676557
94.363137	3467.371592	22.681575
94.388139	3463.033947	22.686592
94.502527	3474.246032	22.691610
94.702227	3478.582947	22.696627
94.759905	3490.340498	22.701645
95.297513	3484.552701	22.706663
95.163114	3489.260749	22.711680
95.231538	3486.368197	22.716698
95.555270	3487.201121	22.721715
95.207404	3492.791661	22.726733
95.254294	3492.137148	22.731751
95.593585	3484.082629	22.736768
95.957128	3504.484739	22.741786
95.775221	3502.452045	22.746803
95.759429	3519.634198	22.751821
95.720711	3519.176162	22.756839
96.073457	3513.714011	22.761856
96.022242	3511.957533	22.766874
96.200564	3510.739543	22.771891
95.811252	3517.987335	22.776909
95.980169	3534.938560	22.781927
96.505610	3532.968639	22.786944
96.034519	3540.020935	22.791962
96.319145	3537.833081	22.796979
96.653851	3559.903150	22.801997
96.674326	3563.337051	22.807015
97.294961	3559.534173	22.812032
96.704608	3568.884028	22.817050
97.236143	3566.916305	22.822067
97.106623	3569.559377	22.827085
97.336104	3584.885123	22.832103
97.504330	3580.348257	22.837120
97.274464	3589.575362	22.842138
97.638677	3582.561639	22.847155
97.704372	3587.696031	22.852173
97.849731	3593.834281	22.857191
98.136268	3607.497193	22.862208
97.826134	3602.602849	22.867226
97.992284	3612.478096	22.872243
98.405901	3608.631890	22.877261
98.296553	3611.761038	22.882279
98.487806	3615.256570	22.887296
98.408085	3626.259279	22.892314
98.595065	3628.038439	22.897331
98.613251	3630.494249	22.902349
98.545919	3635.529556	22.907367
98.792641	3628.777259	22.912384
98.992924	3650.341392	22.917402
99.398147	3657.303786	22.922419
99.206468	3660.698348	22.927437
99.474254	3662.913052	22.932455
99.400527	3661.068553	22.937472
99.447198	3667.910371	22.942490
99.271892	3656.729558	22.947507
99.604633	3676.540141	22.952525
99.779295	3676.023421	22.957543
99.854383	3680.544038	22.962560
99.863108	3688.666970	22.967578
100.594069	3688.700675	22.972595
99.985162	3687.893235	22.977613
100.433982	3693.175952	22.982631
100.699592	3710.648771	22.987648
100.717825	3718.782853	22.992666
100.997867	3706.751052	22.997683
100.537513	3715.821795	23.002701
100.888125	3709.517175	23.007719
100.858204	3699.800197	23.012736
100.902776	3708.914927	23.017754
100.977892	3710.601149	23.022771
100.828865	3727.668650	23.027789
101.706348	3727.332202	23.032807
101.604842	3727.600489	23.037824
101.611539	3738.498193	23.042842
101.625178	3725.889471	23.047859
101.765112	3726.422942	23.052877
101.534855	3736.849596	23.057895
101.751077	3733.810751	23.062912
101.618596	3741.943205	23.067930
101.814319	3748.903737	23.072947
101.522205	3751.569152	23.077965
101.631808	3769.151691	23.082983
102.235670	3773.059220	23.088000
101.963870	3783.836453	23.093018
102.412331	3777.020932	23.098035
101.878005	3792.078287	23.103053
102.117362	3808.403242	23.108071
102.726214	3807.676457	23.113088
103.144299	3826.129223	23.118106
103.376442	3822.677542	23.123123
103.035658	3842.937872	23.128141
103.207636	3839.883847	23.133159
103.260997	3834.844113	23.138176
103.434095	3846.227143	23.143194
103.493762	3857.006146	23.148211
103.457220	3859.890359	23.153229
103.657482	3862.481805	23.158247
104.251480	3857.054352	23.163264
104.150410	3858.585121	23.168282
104.356274	3857.883595	23.173299
104.240958	3875.722421	23.178317
104.266219	3881.986901	23.183335
104.664081	3872.265937	23.188352
104.600288	3878.556994	23.193370
104.519141	3872.951236	23.198387
104.972601	3877.100142	23.203405
104.515525	3884.298725	23.208423
105.019169	3899.676477	23.213440
105.038421	3906.841475	23.218458
105.462508	3904.748514	23.223475
105.362282	3908.867387	23.228493
105.262449	3910.060234	23.233511
105.507552	3910.839213	23.238528
105.622864	3931.975101	23.243546
105.735458	3941.656909	23.248563
105.796824	3931.723496	23.253581
105.633498	3936.975934	23.258599
106.048395	3937.232761	23.263616
106.173894	3949.538665	23.268634
106.282770	3951.478444	23.273651
106.136144	3949.200286	23.278669
106.411673	3956.470347	23.283687
106.667677	3953.835564	23.288704
106.802594	3962.699538	23.293722
106.778865	3964.754786	23.298739
106.887647	3972.657004	23.303757
107.080687	3976.871985	23.308775
107.270365	3975.412299	23.313792
106.949481	3983.435496	23.318810
107.337016	3987.967211	23.323827
107.338081	4008.631845	23.328845
107.369714	4003.437649	23.333863
107.629917	4000.316116	23.338880
107.598697	4002.388324	23.343898
107.617255	4015.219207	23.348915
107.525654	4015.340752	23.353933
107.973693	4022.220826	23.358951
108.369296	4022.594308	23.363968
108.092628	4038.173338	23.368986
108.325016	4040.658773	23.374003
108.337566	4044.340206	23.379021
108.152210	4047.257232	23.384039
108.418689	4046.552515	23.389056
108.418988	4054.639055	23.394074
108.944911	4059.685696	23.399091
109.133218	4070.163751	23.404109
108.613049	4076.324366	23.409127
109.347401	4070.713884	23.414144
109.309001	4085.434960	23.419162
109.137130	4100.075953	23.424179
109.693514	4094.657479	23.429197
109.796049	4107.147004	23.434215
109.783140	4092.907164	23.439232
109.700605	4104.822806	23.444250
110.067694	4103.224841	23.449267
110.011573	4120.464384	23.454285
109.979706	4125.326980	23.459303
110.135246	4119.459959	23.464320
110.202056	4129.426806	23.469338
110.475080	4138.086157	23.474355
110.801322	4136.942800	23.479373
110.839387	4141.118970	23.484391
111.202540	4148.252280	23.489408
111.345723	4150.852711	23.494426
111.248828	4147.660843	23.499443
111.412003	4150.898896	23.504461
110.986739	4156.656429	23.509479
111.032109	4165.891208	23.514496
111.155821	4171.515392	23.519514
111.137735	4178.105564	23.524531
111.387768	4189.135863	23.529549
111.783346	4207.103297	23.534567
111.688847	4195.698010	23.539584
112.038586	4202.937605	23.544602
111.997654	4217.163625	23.549619
112.242273	4222.134438	23.554637
112.462690	4222.061905	23.559655
112.167263	4232.388578	23.564672
112.376867	4246.673218	23.569690
112.644338	4251.479482	23.574707
113.245607	4252.092201	23.579725
113.081565	4256.413693	23.584743
112.992011	4257.993195	23.589760
113.197935	4270.233057	23.594778
113.399483	4271.981591	23.599795
113.408318	4269.840015	23.604813
113.495603	4269.860938	23.609831
113.469462	4276.951126	23.614848
113.918007	4290.974260	23.619866
114.099469	4300.828545	23.624883
114.312635	4296.663234	23.629901
114.243194	4305.477325	23.634919
114.258053	4296.204384	23.639936
114.272329	4303.490264	23.644954
114.348136	4321.978221	23.649971
114.908685	4320.233140	23.654989
114.954861	4327.002686	23.660007
114.748586	4321.716257	23.665024
114.939389	4318.021600	23.670042
114.982480	4329.892456	23.675059
115.177642	4341.212368	23.680077
115.317126	4352.285337	23.685095
115.522403	4340.810898	23.690112
115.531208	4344.928570	23.695130
115.746851	4347.142059	23.700147
115.917414	4346.730126	23.705165
116.109657	4365.171478	23.710183
115.894643	4366.884277	23.715200
115.866181	4364.934764	23.720218
115.868937	4375.164298	23.725235
116.240365	4363.199814	23.730253
116.242595	4366.999719	23.735271
116.164268	4380.328977	23.740288
116.301754	4392.620678	23.745306
116.490258	4393.528492	23.750323
117.012195	4398.253894	23.755341
117.054824	4411.690484	23.760359
116.957415	4409.521345	23.765376
116.838465	4418.576826	23.770394
116.749633	4419.136689	23.775411
117.203614	4438.124212	23.780429
117.023713	4450.639282	23.785447
117.361018	4451.552195	23.790464
117.418604	4467.145511	23.795482
117.710277	4472.948646	23.800499
118.084879	4466.832553	23.805517
117.638436	4481.993498	23.810535
118.096141	4494.819048	23.815552
118.264981	4497.002011	23.820570
118.001747	4498.940174	23.825587
118.611438	4517.379409	23.830605
118.744793	4522.970626	23.835623
118.704393	4534.633743	23.840640
119.053079	4526.047004	23.845658
119.119001	4551.481017	23.850675
119.029415	4552.476598	23.855693
119.290166	4546.583488	23.860711
119.636382	4549.994951	23.865728
119.577122	4566.237956	23.870746
119.654605	4568.122747	23.875763
120.232372	4571.526347	23.880781
119.902367	4571.666306	23.885799
120.020579	4578.468851	23.890816
119.961001	4583.373789	23.895834
120.366055	4601.668406	23.900851
120.792075	4591.503896	23.905869
120.520397	4602.411008	23.910887
120.308922	4604.091710	23.915904
121.018991	4609.936660	23.920922
120.858711	4619.333305	23.925939
121.538893	4617.181205	23.930957
121.626887	4620.068122	23.935975
121.406966	4623.457817	23.940992
121.609907	4624.578024	23.946010
121.641292	4621.378601	23.951027
121.988693	4618.366407	23.956045
121.500546	4625.194523	23.961063
121.770099	4642.967491	23.966080
121.978135	4652.072868	23.971098
121.908127	4657.525536	23.976115
122.567287	4655.733411	23.981133
122.746089	4669.641273	23.986151
122.330151	4685.346840	23.991168
122.426144	4686.559562	23.996186
122.748884	4682.414875	24.001203
122.925501	4677.175677	24.006221
122.827403	4694.337113	24.011239
122.805312	4706.796071	24.016256
123.123405	4702.323830	24.021274
123.053710	4716.131772	24.026291
123.366822	4720.981515	24.031309
123.723188	4737.033297	24.036327
123.804093	4728.870354	24.041344
123.910847	4731.867985	24.046362
124.156293	4735.431002	24.051379
124.229495	4755.075096	24.056397
124.205299	4763.405684	24.061415
124.366700	4763.159318	24.066432
124.541807	4754.741709	24.071450
124.191098	4763.347565	24.076467
124.798323	4764.309746	24.081485
124.891318	4774.301253	24.086503
124.545061	4773.787201	24.091520
125.258113	4779.470757	24.096538
125.074852	4775.812516	24.101555
125.196407	4776.150037	24.106573
125.165706	4791.075652	24.111591
125.625777	4799.421928	24.116608
125.678633	4802.244936	24.121626
125.676822	4800.013425	24.126643
125.932131	4806.305314	24.131661
125.831591	4823.858666	24.136679
125.946886	4837.786076	24.141696
126.157866	4821.768178	24.146714
126.238189	4849.195285	24.151731
126.635018	4848.261785	24.156749
126.535029	4860.862470	24.161767
126.578270	4854.693996	24.166784
127.145888	4867.963448	24.171802
126.986061	4877.940959	24.176819
126.868986	4881.311432	24.181837
126.697020	4885.634314	24.186855
126.745643	4905.048835	24.191872
127.354184	4909.167373	24.196890
127.484306	4925.728250	24.201907
127.889874	4931.911415	24.206925
127.907411	4943.581499	24.211943
128.033364	4946.885501	24.216960
128.366454	4947.076249	24.221978
128.153171	4964.969368	24.226995
128.452237	4961.153454	24.232013
128.762010	4962.222223	24.237031
128.412297	4972.668297	24.242048
128.717253	4979.309160	24.247066
128.837060	4988.065523	24.252083
128.932165	4987.854793	24.257101
129.541759	5006.559693	24.262119
129.309549	5006.927389	24.267136
129.585491	5003.392868	24.272154
129.343090	5008.746385	24.277171
129.816507	5027.838804	24.282189
130.059628	5025.376343	24.287207
129.909413	5033.872000	24.292224
130.432845	5032.902875	24.297242
130.212127	5043.211987	24.302259
130.629182	5070.905486	24.307277
130.746236	5064.643306	24.312295
130.604002	5062.307500	24.317312
130.688872	5057.338249	24.322330
130.645522	5082.379768	24.327347
130.831514	5084.064532	24.332365
131.178828	5088.956364	24.337383
130.988505	5099.197614	24.342400
131.186916	5105.763674	24.347418
131.718173	5114.594527	24.352435
131.670980	5110.974876	24.357453
132.221433	5119.477596	24.362471
132.135951	5142.401413	24.367488
132.493762	5137.424102	24.372506
132.429425	5142.004806	24.377523
132.660879	5145.349135	24.382541
132.709143	5136.834429	24.387559
132.687647	5141.474709	24.392576
132.813971	5137.414355	24.397594
133.095974	5157.689055	24.402611
133.203142	5155.165804	24.407629
133.236185	5159.775449	24.412647
133.213126	5163.904611	24.417664
133.189038	5157.692921	24.422682
133.301538	5173.799078	24.427699
133.587349	5183.678530	24.432717
134.059603	5180.315242	24.437735
133.943353	5185.876323	24.442752
134.034164	5189.981339	24.447770
133.752515	5206.897389	24.452787
133.821102	5209.907392	24.457805
134.113429	5222.153299	24.462823
133.964104	5243.401616	24.467840
134.515623	5227.121676	24.472858
134.194726	5256.247376	24.477875
134.613506	5263.403979	24.482893
134.987925	5276.107397	24.487911
134.917377	5291.399518	24.492928
135.488962	5284.169573	24.497946
135.709583	5291.013159	24.502963
135.538747	5308.028738	24.507981
135.739868	5320.945578	24.512999
135.788904	5319.226881	24.518016
136.311684	5318.311507	24.523034
136.101084	5338.092233	24.528051
136.261738	5349.834854	24.533069
136.344515	5349.913305	24.538087
136.527796	5359.168120	24.543104
136.781292	5356.713459	24.548122
136.784182	5364.538174	24.553139
136.850768	5364.069907	24.558157
137.270161	5384.979916	24.563175
137.130797	5401.697083	24.568192
137.839134	5398.091588	24.573210
137.641270	5400.306857	24.578227
137.896449	5422.928281	24.583245
138.199494	5418.025765	24.588263
137.940916	5433.476885	24.593280
138.062205	5431.797365	24.598298
138.318406	5437.833645	24.603315
138.704442	5451.482359	24.608333
138.898588	5454.621095	24.613351
138.705938	5453.034949	24.618368
138.729711	5450.098575	24.623386
138.932632	5463.056270	24.628403
139.271117	5478.581192	24.633421
139.240506	5469.163258	24.638439
139.148418	5483.483509	24.643456
139.450954	5496.709721	24.648474
139.526184	5503.973905	24.653491
139.757334	5512.220637	24.658509
140.122455	5519.379435	24.663527
139.885254	5532.696544	24.668544
140.213610	5533.415204	24.673562
140.470947	5540.180529	24.678579
140.314166	5559.441683	24.683597
140.786596	5545.282506	24.688615
140.644415	5562.069708	24.693632
140.832766	5558.627720	24.698650
140.962843	5576.581285	24.703667
141.255440	5579.969778	24.708685
141.532277	5580.668101	24.713703
141.366655	5592.376765	24.718720
141.599681	5601.153565	24.723738
141.693507	5606.293591	24.728755
141.642189	5603.861398	24.733773
142.373258	5612.986329	24.738791
141.960882	5633.026266	24.743808
142.361197	5633.099164	24.748826
142.248302	5633.650206	24.753843
142.843716	5646.805390	24.758861
142.882730	5658.718788	24.763879
142.892786	5669.961199	24.768896
142.997668	5664.322588	24.773914
143.468172	5663.011333	24.778931
143.197645	5666.207120	24.783949
143.420468	5678.716758	24.788967
143.115623	5693.029467	24.793984
143.443802	5692.403412	24.799002
143.542659	5710.361999	24.804019
143.706948	5710.572890	24.809037
144.290233	5722.549425	24.814055
143.961400	5736.938531	24.819072
144.441218	5742.662091	24.824090
144.366935	5753.655760	24.829107
144.559124	5764.784466	24.834125
144.755497	5759.418752	24.839143
144.913225	5767.194128	24.844160
145.524691	5779.267301	24.849178
145.329449	5796.110380	24.854195
145.235686	5806.504202	24.859213
145.529423	5807.199887	24.864231
145.851974	5820.189602	24.869248
145.773658	5829.627691	24.874266
146.051723	5827.882536	24.879283
146.050330	5849.619768	24.884301
146.448189	5849.917179	24.889319
146.250795	5856.094109	24.894336
146.512582	5868.089541	24.899354
146.654339	5878.515954	24.904371
146.643529	5877.390575	24.909389
147.094502	5892.064851	24.914407
146.833891	5909.417037	24.919424
147.242285	5913.238864	24.924442
147.727742	5927.803595	24.929459
147.810851	5939.628192	24.934477
148.038326	5933.007490	24.939495
148.158068	5937.215470	24.944512
148.073081	5952.721906	24.949530
148.240245	5955.745000	24.954547
148.175259	5965.891336	24.959565
148.820891	5965.891080	24.964583
149.053317	5982.515807	24.969600
148.953700	5987.509469	24.974618
149.395155	5982.098981	24.979635
149.386283	5982.229674	24.984653
149.433484	5998.728753	24.989671
149.486310	6010.820151	24.994688
149.636914	6008.687728	24.999706
149.757525	6017.788544	25.004723
149.835013	6027.173915	25.009741
150.321127	6029.316828	25.014759
150.060168	6027.684512	25.019776
150.459222	6045.924700	25.024794
150.660145	6060.123735	25.029811
150.537929	6070.111787	25.034829
150.448671	6060.159775	25.039847
150.504660	6080.893915	25.044864
151.131816	6083.008425	25.049882
151.196598	6093.001917	25.054899
151.469096	6112.669913	25.059917
151.726403	6110.546016	25.064935
151.520993	6117.775491	25.069952
151.811454	6142.362098	25.074970
151.965647	6147.596993	25.079987
151.868763	6156.529919	25.085005
152.135708	6154.590756	25.090023
152.115728	6156.408905	25.095040
152.434925	6165.437646	25.100058
152.551852	6176.136445	25.105075
152.656655	6185.849078	25.110093
152.799608	6194.106780	25.115111
153.166768	6210.069780	25.120128
153.377445	6220.592922	25.125146
153.663154	6228.815648	25.130163
153.607745	6233.489929	25.135181
153.627512	6231.084398	25.140199
153.778217	6244.795829	25.145216
153.814496	6257.909623	25.150234
154.083122	6261.380919	25.155251
154.189586	6276.968123	25.160269
154.704647	6278.977104	25.165287
154.547122	6286.445372	25.170304
154.656370	6304.377660	25.175322
154.858515	6311.653849	25.180339
155.197176	6335.011484	25.185357
155.422830	6331.623487	25.190375
155.619062	6332.763794	25.195392
155.814888	6350.540507	25.200410
155.878569	6362.311599	25.205427
155.787118	6364.863874	25.210445
156.338913	6358.422656	25.215463
156.160102	6385.791647	25.220480
156.359008	6385.435211	25.225498
156.815111	6395.029783	25.230515
156.842233	6416.621163	25.235533
157.037445	6414.885778	25.240551
157.152296	6418.621113	25.245568
157.218346	6421.805339	25.250586
157.398754	6432.358599	25.255603
157.809485	6439.892588	25.260621
157.691844	6435.589211	25.265639
157.912397	6453.100134	25.270656
157.876181	6461.086128	25.275674
158.024153	6466.584105	25.280691
157.875336	6487.423396	25.285709
158.259282	6486.302429	25.290727
158.540479	6510.834159	25.295744
158.535782	6516.513910	25.300762
158.740090	6523.534141	25.305779
158.988303	6547.316605	25.310797
159.542201	6543.744559	25.315815
159.162338	6563.269007	25.320832
159.980190	6574.748458	25.325850
159.970713	6575.232816	25.330867
159.666584	6576.299998	25.335885
159.836024	6593.396046	25.340903
160.118661	6602.007713	25.345920
160.162196	6613.229673	25.350938
160.727802	6617.683645	25.355955
160.895363	6634.262302	25.360973
160.872845	6634.098393	25.365991
161.094290	6647.054026	25.371008
161.213995	6653.276250	25.376026
161.194726	6662.866515	25.381043
161.001101	6677.298310	25.386061
161.264287	6689.319316	25.391079
161.725678	6702.688829	25.396096
161.732838	6720.580693	25.401114
162.372993	6729.704646	25.406131
162.277225	6747.088621	25.411149
162.271090	6741.100876	25.416167
162.801450	6744.635438	25.421184
162.544627	6762.069913	25.426202
162.795434	6762.497715	25.431219
163.021366	6779.528262	25.436237
163.524389	6786.842739	25.441255
163.344802	6801.209294	25.446272
163.660202	6805.898237	25.451290
164.011428	6797.957203	25.456307
163.868616	6825.595856	25.461325
164.022346	6821.511896	25.466343
164.368132	6827.660878	25.471360
164.342835	6842.890378	25.476378
165.002606	6846.161606	25.481395
164.753191	6857.113921	25.486413
164.969270	6855.362598	25.491431
165.052232	6870.493082	25.496448
165.448577	6879.888917	25.501466
165.677175	6879.404702	25.506483
166.003685	6891.605335	25.511501
166.150681	6897.785484	25.516519
166.494107	6904.812479	25.521536
166.159953	6907.740639	25.526554
166.219956	6896.719857	25.531571
166.355899	6913.458407	25.536589
166.367034	6933.881690	25.541607
166.633109	6923.886170	25.546624
166.519485	6948.319337	25.551642
166.858658	6950.381205	25.556659
166.992338	6975.924779	25.561677
166.912327	6995.791008	25.566695
167.256812	7002.413790	25.571712
167.289285	7015.446641	25.576730
167.561893	7021.686075	25.581747
168.021452	7046.023262	25.586765
168.211020	7047.685550	25.591783
168.504996	7068.077299	25.596800
168.632024	7067.362751	25.601818
168.927572	7076.272527	25.606835
168.719565	7094.646747	25.611853
168.972968	7110.214795	25.616871
169.586508	7114.235194	25.621888
169.057171	7121.717852	25.626906
169.535430	7130.475910	25.631923
169.727525	7145.052843	25.636941
169.762086	7156.263913	25.641959
170.035173	7158.771816	25.646976
170.510765	7184.416805	25.651994
170.356043	7177.697685	25.657011
171.036075	7201.012414	25.662029
170.696814	7209.860700	25.667047
171.313559	7205.985088	25.672064
171.147220	7205.818449	25.677082
171.333896	7226.959596	25.682100
171.459319	7243.359143	25.687117
171.714163	7251.776582	25.692135
172.271676	7260.939005	25.697152
172.161050	7265.685337	25.702170
172.504424	7257.653785	25.707188
172.682245	7269.347594	25.712205
172.789637	7290.801146	25.717223
172.957679	7286.339163	25.722240
172.892419	7293.594495	25.727258
173.199009	7295.617310	25.732276
173.180065	7322.946861	25.737293
173.343676	7313.658560	25.742311
173.720101	7326.786125	25.747328
173.575551	7347.837237	25.752346
173.806873	7345.562580	25.757364
173.915420	7353.800939	25.762381
173.949886	7367.127325	25.767399
174.346587	7373.922009	25.772416
174.152304	7381.090251	25.777434
174.482802	7400.529553	25.782452
174.581736	7413.025057	25.787469
174.841681	7422.584604	25.792487
175.305375	7429.277261	25.797504
175.033903	7448.602557	25.802522
175.630192	7450.807308	25.807540
175.619055	7462.950722	25.812557
175.841989	7482.375391	25.817575
175.930109	7485.060695	25.822592
176.070426	7497.985439	25.827610
176.394161	7511.497074	25.832628
176.414455	7526.647385	25.837645
177.011316	7546.326085	25.842663
177.036360	7545.135004	25.847680
177.102796	7554.832273	25.852698
177.652361	7560.034045	25.857716
177.310177	7568.074765	25.862733
177.426828	7584.917973	25.867751
177.428491	7597.981318	25.872768
178.034202	7617.715535	25.877786
178.366914	7625.896798	25.882804
178.240763	7636.448263	25.887821
178.352385	7654.368867	25.892839
178.759324	7659.100515	25.897856
178.680452	7671.977637	25.902874
179.140949	7688.719717	25.907892
179.216194	7701.332780	25.912909
179.450259	7710.694481	25.917927
179.645567	7714.802635	25.922944
179.699491	7730.920213	25.927962
179.949189	7744.519386	25.932980
180.061552	7753.903331	25.937997
180.380182	7767.157076	25.943015
180.594153	7767.306540	25.948032
180.250924	7790.043572	25.953050
180.647600	7801.195148	25.958068
181.128707	7817.577369	25.963085
181.068314	7827.926061	25.968103
182.036087	7832.547795	25.973120
181.603891	7841.584579	25.978138
181.892785	7857.428678	25.983156
182.253758	7868.986834	25.988173
182.390523	7883.036319	25.993191
182.729902	7881.107732	25.998208
182.930462	7895.251415	26.003226
182.892448	7906.395383	26.008244
182.982921	7897.111934	26.013261
183.074530	7921.271141	26.018279
183.358363	7938.899848	26.023296
183.682979	7945.541869	26.028314
183.939797	7949.403659	26.033332
184.051574	7965.310325	26.038349
184.149501	7964.429821	26.043367
184.630260	7977.036372	26.048384
184.763506	7992.352481	26.053402
184.798895	7985.871636	26.058420
184.772404	8004.341449	26.063437
184.798642	8014.023157	26.068455
184.965083	8026.685297	26.073472
185.203276	8043.847691	26.078490
185.351081	8052.503262	26.083508
185.827572	8068.946415	26.088525
185.962705	8084.341232	26.093543
186.548845	8091.302246	26.098560
186.294858	8098.082323	26.103578
186.437637	8097.756750	26.108596
186.624307	8107.820640	26.113613
186.600086	8129.662009	26.118631
187.010857	8129.547020	26.123648
187.040714	8152.311290	26.128666
187.124019	8162.713429	26.133684
187.451504	8167.479756	26.138701
187.897065	8178.848058	26.143719
187.836731	8189.932551	26.148736
187.820179	8204.135740	26.153754
187.852852	8214.637396	26.158772
188.317751	8221.765838	26.163789
188.290898	8237.321915	26.168807
188.787006	8241.282036	26.173824
188.673032	8267.674419	26.178842
188.892605	8281.449192	26.183860
189.041261	8301.028429	26.188877
189.708972	8311.051799	26.193895
189.871616	8330.676234	26.198912
189.945686	8343.296234	26.203930
190.307175	8354.709386	26.208948
190.409380	8360.038299	26.213965
190.116607	8369.094540	26.218983
190.761696	8383.304714	26.224000
190.918292	8391.927495	26.229018
190.990040	8404.914131	26.234036
191.564207	8416.818091	26.239053
191.523700	8439.789481	26.244071
191.669509	8439.403442	26.249088
192.064633	8446.435558	26.254106
192.155188	8483.407428	26.259124
192.619698	8484.063841	26.264141
192.301176	8491.567691	26.269159
192.650733	8509.742308	26.274176
192.891038	8520.988274	26.279194
193.435540	8531.062638	26.284212
193.462460	8531.042511	26.289229
193.511182	8545.595654	26.294247
194.216313	8553.747402	26.299264
193.933864	8567.809409	26.304282
193.878979	8576.973713	26.309300
193.898126	8588.437484	26.314317
193.783535	8600.231617	26.319335
194.212589	8610.851360	26.324352
194.516088	8630.889739	26.329370
194.954724	8650.367088	26.334388
195.260109	8665.994608	26.339405
195.311287	8687.401756	26.344423
195.689564	8697.129702	26.349440
196.319148	8704.958689	26.354458
196.278537	8709.956469	26.359476
196.205472	8715.483432	26.364493
196.453751	8736.029413	26.369511
196.626266	8739.560441	26.374528
196.771209	8755.670966	26.379546
197.254991	8768.924815	26.384564
197.334666	8782.961826	26.389581
197.697389	8792.149216	26.394599
197.475388	8791.394566	26.399616
197.770104	8809.331806	26.404634
197.832234	8819.958636	26.409652
198.303592	8837.533564	26.414669
198.549691	8847.901113	26.419687
198.551182	8858.316458	26.424704
198.512468	8870.856612	26.429722
198.485101	8887.224723	26.434740
199.225061	8896.340439	26.439757
199.421468	8907.918713	26.444775
199.559875	8921.062601	26.449792
200.106219	8932.412421	26.454810
199.793474	8935.394372	26.459828
199.841900	8945.837143	26.464845
200.112039	8965.025496	26.469863
200.366759	8968.209020	26.474880
200.388290	8990.732515	26.479898
200.576843	9005.829261	26.484916
200.934390	9014.474525	26.489933
200.716967	9034.714923	26.494951
201.329501	9043.737013	26.499968
201.797893	9056.781943	26.504986
201.808911	9085.574371	26.510004
201.861879	9092.281464	26.515021
202.129996	9109.317024	26.520039
202.464208	9117.366110	26.525056
202.916363	9133.801394	26.530074
202.940570	9146.268730	26.535092
202.927782	9158.075684	26.540109
203.513177	9175.191049	26.545127
203.945857	9183.950913	26.550144
203.589849	9188.527796	26.555162
204.015542	9202.706670	26.560180
204.209507	9215.327424	26.565197
204.640999	9228.179346	26.570215
204.540480	9239.624377	26.575232
205.387141	9246.933366	26.580250
205.065669	9256.442868	26.585268
205.649745	9272.784991	26.590285
205.403086	9284.751798	26.595303
205.464860	9288.180301	26.600320
205.898638	9302.452703	26.605338
206.058231	9314.520066	26.610356
206.733771	9324.410156	26.615373
206.549145	9340.219199	26.620391
206.673177	9344.477804	26.625408
206.802177	9358.482265	26.630426
206.956970	9369.454827	26.635444
207.022936	9386.961177	26.640461
207.443854	9404.074104	26.645479
207.600070	9420.758073	26.650496
207.750432	9431.181991	26.655514
207.983361	9445.669093	26.660532
208.180865	9455.072136	26.665549
208.241292	9473.817110	26.670567
208.878416	9485.475097	26.675584
208.876445	9494.258998	26.680602
208.813433	9517.743576	26.685620
209.139495	9527.786401	26.690637
209.534642	9546.611620	26.695655
209.857389	9566.922683	26.700672
210.631192	9576.892236	26.705690
210.393487	9582.915693	26.710708
210.526677	9596.244001	26.715725
210.786708	9604.235458	26.720743
210.666850	9611.572868	26.725760
210.889004	9619.380823	26.730778
210.982930	9651.773159	26.735796
211.344153	9657.813321	26.740813
211.237302	9674.642922	26.745831
211.617461	9692.864423	26.750848
211.995959	9697.083245	26.755866
212.465273	9732.081736	26.760884
212.573555	9736.832293	26.765901
212.881004	9752.883493	26.770919
213.092602	9758.280921	26.775936
213.330059	9762.442919	26.780954
213.245087	9778.508256	26.785972
213.537410	9792.512716	26.790989
213.686334	9805.608220	26.796007
213.653694	9817.333452	26.801024
213.951728	9837.670784	26.806042
213.927391	9849.903076	26.811060
214.241890	9863.623107	26.816077
214.323796	9882.624033	26.821095
214.925681	9897.849355	26.826112
215.466797	9915.038645	26.831130
215.448002	9927.093304	26.836148
215.555193	9937.025397	26.841165
215.741641	9949.733077	26.846183
216.278572	9965.884280	26.851200
216.393243	9971.338000	26.856218
216.464519	9997.271247	26.861236
216.448979	10007.307854	26.866253
216.813852	10024.250159	26.871271
217.091379	10035.772224	26.876288
217.383489	10056.846404	26.881306
217.166625	10066.093649	26.886324
217.802345	10072.491940	26.891341
218.145689	10094.420117	26.896359
218.045700	10120.408781	26.901376
218.721845	10127.678527	26.906394
218.916526	10149.380620	26.911412
219.206935	10147.980456	26.916429
219.852165	10171.951664	26.921447
219.820534	10176.307467	26.926464
219.830741	10174.853316	26.931482
220.148402	10195.746834	26.936500
220.424710	10203.941234	26.941517
220.401082	10207.266459	26.946535
220.604610	10224.969910	26.951552
220.931167	10234.062643	26.956570
220.736383	10253.476715	26.961588
221.168323	10261.015266	26.966605
221.356191	10282.017622	26.971623
221.447378	10304.285508	26.976640
221.873354	10317.552678	26.981658
221.786370	10326.937579	26.986676
222.191174	10339.339775	26.991693
222.377670	10368.864488	26.996711
222.407126	10386.241723	27.001728
222.779234	10401.572918	27.006746
223.069255	10419.143019	27.011764
223.155808	10432.068756	27.016781
223.604856	10450.112858	27.021799
223.550121	10472.653246	27.026816
223.896184	10478.683422	27.031834
223.940175	10509.563149	27.036852
224.229719	10515.469575	27.041869
224.726827	10534.305080	27.046887
224.928480	10561.759552	27.051904
225.400543	10564.587237	27.056922
225.286760	10578.580126	27.061940
225.712572	10592.191688	27.066957
226.199402	10612.553966	27.071975
226.103978	10625.767263	27.076992
226.640435	10631.376128	27.082010
226.682271	10646.670852	27.087028
226.843273	10661.091229	27.092045
227.088341	10675.308994	27.097063
227.338403	10689.166029	27.102080
227.621591	10699.879287	27.107098
227.311115	10717.486904	27.112116
227.991289	10737.301192	27.117133
228.137516	10746.403480	27.122151
228.272111	10767.645228	27.127168
228.371175	10776.091832	27.132186
228.487636	10796.379714	27.137204
228.426398	10808.391068	27.142221
228.802837	10825.995377	27.147239
229.055780	10851.850827	27.152256
229.545440	10867.211352	27.157274
229.974076	10889.957543	27.162292
230.303014	10897.316719	27.167309
230.433447	10910.627452	27.172327
230.336674	10925.252607	27.177344
230.894460	10937.643866	27.182362
231.295337	10955.159213	27.187380
231.186347	10970.683072	27.192397
231.837367	10982.305092	27.197415
231.898775	10996.965518	27.202432
232.141415	11008.780990	27.207450
231.759224	11021.976336	27.212468
232.446415	11033.567460	27.217485
232.229300	11049.698793	27.222503
232.450737	11071.830355	27.227520
232.956188	11087.930626	27.232538
233.057298	11115.395344	27.237556
233.128828	11135.270668	27.242573
233.587273	11149.117503	27.247591
233.693704	11177.705590	27.252608
233.811940	11191.242624	27.257626
234.326911	11214.837716	27.262644
234.814651	11235.563658	27.267661
234.973834	11244.436809	27.272679
234.829236	11268.703667	27.277696
235.155938	11281.838666	27.282714
235.648162	11299.589479	27.287732
235.642371	11311.093561	27.292749
236.333474	11330.720466	27.297767
236.625873	11361.976333	27.302784
236.667614	11368.054471	27.307802
236.814712	11393.185199	27.312820
237.344816	11407.712526	27.317837
237.341570	11420.116210	27.322855
237.511246	11439.670188	27.327872
238.023566	11458.532660	27.332890
238.306885	11465.807634	27.337908
238.615163	11492.482608	27.342925
238.842798	11501.165169	27.347943
238.803322	11523.129729	27.352960
239.345438	11530.758897	27.357978
239.661521	11546.961855	27.362996
239.657786	11554.139736	27.368013
240.082960	11564.389170	27.373031
240.085575	11589.245971	27.378048
240.050869	11603.596684	27.383066
240.460693	11622.724836	27.388084
240.307411	11639.964499	27.393101
241.051942	11652.680641	27.398119
241.390514	11672.262084	27.403136
241.630576	11690.542214	27.408154
241.371629	11698.536926	27.413172
242.132942	11716.849104	27.418189
241.969860	11745.556059	27.423207
242.020657	11763.262785	27.428224
242.726070	11781.274326	27.433242
242.896781	11797.484484	27.438260
242.926538	11820.474280	27.443277
243.750370	11826.723717	27.448295
243.620773	11845.579774	27.453312
243.870716	11862.715424	27.458330
244.088648	11877.124659	27.463348
244.417870	11890.171272	27.468365
244.604830	11907.904169	27.473383
244.745045	11929.057932	27.478400
245.189134	11943.220220	27.483418
245.135945	11954.956321	27.488436
245.285924	11973.055056	27.493453
245.657459	11986.417199	27.498471
245.984535	12003.761937	27.503488
246.320802	12021.553654	27.508506
246.660990	12025.940057	27.513524
246.575989	12054.445784	27.518541
247.422191	12059.419215	27.523559
246.957986	12089.386449	27.528576
247.513434	12089.867712	27.533594
247.722897	12115.873812	27.538612
247.628501	12138.990809	27.543629
248.002032	12147.300300	27.548647
248.251164	12178.693771	27.553664
248.380792	12201.343132	27.558682
248.706783	12214.450475	27.563700
249.076805	12237.270637	27.568717
248.900821	12251.119778	27.573735
249.238340	12279.682811	27.578752
249.754054	12303.591778	27.583770
250.241227	12326.816842	27.588788
250.394924	12344.978509	27.593805
250.458238	12359.478647	27.598823
250.984094	12384.933461	27.603840
251.367507	12405.585460	27.608858
251.473917	12418.619977	27.613876
251.669407	12450.331769	27.618893
252.353280	12457.793850	27.623911
252.317524	12477.450559	27.628928
252.807167	12493.611354	27.633946
253.014302	12517.654194	27.638964
253.027642	12516.142530	27.643981
253.853004	12530.119219	27.648999
254.061572	12551.938752	27.654016
254.018481	12567.437812	27.659034
254.310859	12579.966471	27.664052
254.684970	12604.687467	27.669069
255.044500	12613.640404	27.674087
254.577272	12620.733404	27.679104
254.960717	12646.043512	27.684122
255.573976	12649.269398	27.689140
255.491716	12679.774570	27.694157
255.561042	12693.595080	27.699175
256.397770	12721.234268	27.704192
256.471054	12732.060516	27.709210
256.814031	12755.299223	27.714228
257.063470	12775.833668	27.719245
257.381436	12790.471088	27.724263
257.321214	12810.062500	27.729280
257.637367	12828.754973	27.734298
258.321506	12843.218229	27.739316
258.258299	12861.291212	27.744333
258.703080	12873.278296	27.749351
258.865936	12899.024353	27.754368
258.932402	12911.080198	27.759386
259.644640	12926.909652	27.764404
259.648580	12948.051167	27.769421
259.906114	12956.041290	27.774439
260.197011	12969.195708	27.779456
260.227217	12990.011047	27.784474
260.279149	13010.166155	27.789492
260.301711	13030.651153	27.794509
260.788109	13044.144477	27.799527
260.930433	13073.727720	27.804544
261.442326	13088.442362	27.809562
261.822813	13108.141890	27.814580
261.974063	13128.221565	27.819597
262.518192	13141.159589	27.824615
262.094422	13160.151459	27.829632
262.599430	13179.013645	27.834650
263.133543	13198.935522	27.839668
262.933600	13218.527138	27.844685
263.656762	13232.652995	27.849703
263.708273	13257.719071	27.854720
263.813813	13282.350390	27.859738
264.079528	13289.609880	27.864756
264.213431	13315.288404	27.869773
264.737182	13338.183711	27.874791
264.958768	13354.750404	27.879808
265.075136	13389.608887	27.884826
265.799357	13403.987346	27.889844
265.610710	13424.518487	27.894861
266.292130	13430.358130	27.899879
266.810990	13457.271322	27.904896
266.740606	13483.272612	27.909914
267.131749	13503.296156	27.914932
267.370457	13510.228371	27.919949
267.884501	13534.369693	27.924967
267.621058	13549.146148	27.929984
267.858626	13575.478285	27.935002
268.572112	13596.158830	27.940020
268.353223	13618.324459	27.945037
268.850128	13627.107930	27.950055
268.914430	13655.482144	27.955072
269.483386	13680.003488	27.960090
269.708210	13702.087075	27.965108
269.862349	13728.385122	27.970125
270.310438	13742.156537	27.975143
270.559406	13773.514780	27.980160
270.549799	13781.736583	27.985178
270.626040	13804.206741	27.990196
271.146299	13838.832242	27.995213
271.445946	13846.506654	28.000231
271.947284	13887.523981	28.005248
271.998158	13915.152222	28.010266
272.458289	13921.326702	28.015284
272.674015	13953.697877	28.020301
272.855128	13960.288731	28.025319
273.436285	13976.910174	28.030336
273.521660	14004.223646	28.035354
274.025106	14020.067776	28.040372
274.321735	14038.707655	28.045389
274.722246	14062.280026	28.050407
274.963122	14074.741949	28.055424
274.680023	14095.215972	28.060442
275.277711	14117.301635	28.065460
275.644233	14147.871501	28.070477
276.242485	14148.721939	28.075495
276.664107	14169.455147	28.080512
276.512632	14197.788175	28.085530
276.863708	14202.552358	28.090548
277.141794	14231.111851	28.095565
277.633756	14253.252133	28.100583
277.724486	14261.730025	28.105600
277.935049	14276.407524	28.110618
278.143025	14292.408702	28.115636
278.171972	14314.893186	28.120653
278.236454	14333.285486	28.125671
278.766934	14358.211660	28.130688
278.783582	14371.485808	28.135706
279.453849	14397.587076	28.140724
280.013188	14416.372503	28.145741
280.422622	14438.172214	28.150759
280.674633	14445.497458	28.155776
280.609535	14456.640075	28.160794
280.798758	14468.425024	28.165812
280.841653	14494.043599	28.170829
281.358873	14497.357493	28.175847
281.639428	14522.064061	28.180864
281.723940	14541.056636	28.185882
282.125906	14566.672749	28.190900
282.000557	14595.602330	28.195917
282.539698	14606.009268	28.200935
282.778507	14635.251373	28.205952
282.753882	14671.369143	28.210970
283.076459	14685.647268	28.215988
283.209936	14720.982395	28.221005
283.869584	14742.247419	28.226023
284.435328	14761.089031	28.231040
284.600434	14789.445983	28.236058
284.926905	14812.421344	28.241076
285.146097	14841.313116	28.246093
285.192685	14853.771243	28.251111
285.785417	14883.697314	28.256128
285.558577	14907.391112	28.261146
286.175525	14927.835572	28.266164
286.407856	14949.925745	28.271181
286.754586	14968.340766	28.276199
287.328540	14988.327762	28.281216
287.348074	15027.502796	28.286234
287.665216	15044.965571	28.291252
287.950571	15068.651975	28.296269
288.387730	15086.396023	28.301287
288.788309	15114.817636	28.306304
288.775394	15133.292311	28.311322
289.220335	15162.013398	28.316340
289.673873	15184.457660	28.321357
289.556701	15203.015058	28.326375
290.259460	15224.987641	28.331392
290.375603	15252.414935	28.336410
290.869320	15281.602306	28.341428
290.816549	15298.899020	28.346445
291.703222	15317.918308	28.351463
292.018771	15343.290018	28.356480
292.040142	15368.521504	28.361498
292.788201	15386.153963	28.366516
292.832285	15395.918786	28.371533
292.861676	15416.452650	28.376551
293.113999	15427.896683	28.381568
293.191473	15466.539255	28.386586
293.651100	15480.676490	28.391604
293.877366	15508.497484	28.396621
294.392536	15521.549053	28.401639
294.756352	15541.130536	28.406656
295.158517	15568.762988	28.411674
295.266702	15582.794275	28.416692
295.572098	15612.005333	28.421709
295.555119	15632.189798	28.426727
296.282773	15649.358259	28.431744
296.645185	15693.799631	28.436762
296.629367	15688.334842	28.441780
296.637630	15722.020651	28.446797
297.105121	15749.336767	28.451815
297.546562	15772.901682	28.456832
297.972744	15796.380580	28.461850
298.511795	15809.415972	28.466868
298.700916	15834.924999	28.471885
298.643345	15860.321099	28.476903
299.110535	15870.702100	28.481920
298.747137	15906.177255	28.486938
299.658803	15921.513685	28.491956
300.118637	15948.322780	28.496973
300.085574	15952.095826	28.501991
300.564129	15968.858258	28.507008
300.539220	16004.258462	28.512026
301.343817	16015.246798	28.517044
301.412722	16043.431169	28.522061
301.658611	16070.333959	28.527079
302.040182	16078.618650	28.532096
302.009760	16103.429666	28.537114
302.260986	16126.295211	28.542132
302.538089	16148.341851	28.547149
302.778797	16179.402122	28.552167
303.197324	16207.945724	28.557184
303.555940	16236.037617	28.562202
303.866156	16255.637702	28.567220
304.251372	16285.320526	28.572237
304.562930	16317.004773	28.577255
305.246609	16329.739918	28.582272
305.252880	16357.782953	28.587290
305.592006	16381.418336	28.592308
306.181151	16398.748141	28.597325
306.124242	16422.388759	28.602343
306.124354	16443.916915	28.607360
306.511363	16472.803806	28.612378
306.737958	16494.009117	28.617396
307.419148	16523.936528	28.622413
307.568469	16562.506876	28.627431
307.716268	16578.652048	28.632448
308.427803	16605.255230	28.637466
308.784535	16627.934284	28.642484
309.228624	16653.533955	28.647501
309.375864	16671.871313	28.652519
309.726773	16706.841229	28.657536
310.059045	16741.204529	28.662554
310.357980	16754.925680	28.667572
310.689970	16777.441382	28.672589
311.024476	16810.338888	28.677607
311.353931	16830.223973	28.682624
311.315559	16850.173013	28.687642
311.803238	16869.935438	28.692660
312.085333	16898.292970	28.697677
312.409380	16933.491763	28.702695
312.758242	16946.671430	28.707712
313.136812	16975.557238	28.712730
313.458124	16992.474698	28.717748
313.896103	17011.698619	28.722765
314.103262	17038.191892	28.727783
314.445328	17063.684904	28.732800
315.117102	17095.595120	28.737818
315.057743	17109.363173	28.742836
315.497482	17133.849176	28.747853
315.831029	17156.481946	28.752871
316.363324	17172.431565	28.757888
316.301872	17198.518611	28.762906
316.668923	17216.212440	28.767924
317.232087	17239.561091	28.772941
317.277393	17268.726963	28.777959
317.464362	17297.081029	28.782976
317.767556	17314.506991	28.787994
317.871119	17340.593649	28.793012
318.618171	17365.372940	28.798029
318.444753	17396.651656	28.803047
319.387408	17421.476187	28.808064
319.373969	17446.779017	28.813082
319.754680	17465.418532	28.818100
320.027343	17492.116956	28.823117
320.213710	17518.045584	28.828135
320.473686	17531.593345	28.833152
320.881418	17558.693965	28.838170
320.841243	17581.392091	28.843188
321.704741	17612.805645	28.848205
321.757351	17636.354781	28.853223
322.222518	17653.894659	28.858240
322.015291	17693.499150	28.863258
322.261256	17715.811471	28.868276
322.713483	17741.041741	28.873293
322.929910	17786.474207	28.878311
323.342457	17808.236194	28.883328
324.004107	17849.972859	28.888346
324.225241	17869.301093	28.893364
324.440695	17898.277005	28.898381
324.997685	17926.744602	28.903399
325.376197	17952.801649	28.908416
325.423368	17985.733528	28.913434
325.616249	18006.563570	28.918452
326.411753	18038.525454	28.923469
326.726652	18065.319131	28.928487
327.269868	18091.167356	28.933504
327.539179	18113.678639	28.938522
327.826277	18143.850344	28.943540
328.265453	18162.462420	28.948557
328.513470	18193.531099	28.953575
328.615636	18217.717569	28.958592
329.120386	18244.096382	28.963610
329.246037	18270.755730	28.968628
329.625221	18301.481838	28.973645
329.986443	18339.021190	28.978663
330.251487	18359.158005	28.983680
330.762389	18391.436709	28.988698
331.108313	18419.552717	28.993716
331.938674	18441.136249	28.998733
331.702732	18470.727040	29.003751
332.058421	18494.299234	29.008768
332.449651	18518.282856	29.013786
332.687112	18543.933190	29.018804
333.027706	18561.524992	29.023821
333.500156	18599.875041	29.028839
333.825180	18621.853817	29.033856
334.090316	18651.663324	29.038874
334.340092	18678.802886	29.043892
334.607186	18702.344987	29.048909
334.732740	18739.909392	29.053927
335.449162	18761.871241	29.058944
335.782069	18787.570122	29.063962
335.964648	18824.317086	29.068980
336.900437	18853.421660	29.073997
336.681289	18886.870612	29.079015
337.297254	18905.986402	29.084032
337.780703	18926.639241	29.089050
338.046037	18963.771525	29.094068
338.568108	18978.037380	29.099085
338.703526	19005.726008	29.104103
339.221393	19030.543331	29.109120
339.323105	19052.867147	29.114138
339.479072	19085.480585	29.119156
339.753378	19104.460554	29.124173
340.152071	19132.386106	29.129191
340.448976	19161.610173	29.134208
341.131042	19192.820945	29.139226
341.114823	19222.612217	29.144244
341.956384	19243.721047	29.149261
341.769307	19273.166403	29.154279
342.085703	19289.101043	29.159296
342.865769	19327.890818	29.164314
342.755640	19354.778119	29.169332
343.033298	19373.271342	29.174349
343.099508	19397.250096	29.179367
343.579135	19425.150755	29.184384
343.929952	19449.735742	29.189402
344.051528	19490.347475	29.194420
344.939171	19512.434983	29.199437
344.947390	19548.149197	29.204455
345.455650	19566.530666	29.209472
345.928014	19593.984124	29.214490
346.277013	19628.210915	29.219508
346.776835	19649.986564	29.224525
346.804498	19685.558987	29.229543
346.874972	19714.926755	29.234560
347.205448	19738.466495	29.239578
347.764801	19770.695667	29.244596
347.982803	19804.052436	29.249613
348.534896	19833.894615	29.254631
348.702143	19876.288014	29.259648
349.324339	19908.494933	29.264666
349.398283	19936.491459	29.269684
350.441339	19964.835354	29.274701
350.604574	19996.204498	29.279719
350.627665	20027.222874	29.284736
351.173186	20051.386393	29.289754
350.757110	20090.131274	29.294772
351.654946	20115.231639	29.299789
352.001704	20147.538960	29.304807
352.382550	20181.243636	29.309824
352.828570	20208.335628	29.314842
352.905547	20235.832965	29.319860
353.519129	20274.808654	29.324877
353.783894	20307.988362	29.329895
354.190001	20341.057531	29.334912
354.489103	20375.994770	29.339930
354.872348	20409.194000	29.344948
354.896374	20442.411645	29.349965
355.494918	20476.581872	29.354983
355.748470	20518.280762	29.360000
356.146555	20544.710985	29.365018
356.578997	20581.207282	29.370036
357.272430	20613.353654	29.375053
357.706341	20646.918132	29.380071
358.064737	20670.315613	29.385088
358.524183	20704.406932	29.390106
358.922404	20739.569388	29.395124
359.401125	20755.877854	29.400141
359.629158	20790.182484	29.405159
360.276336	20816.814155	29.410176
360.724553	20835.269405	29.415194
360.987810	20867.205566	29.420212
361.378559	20885.638273	29.425229
361.560971	20915.710602	29.430247
361.677225	20945.584831	29.435264
362.363950	20964.426179	29.440282
362.595954	21002.142523	29.445300
362.886437	21019.024081	29.450317
362.887730	21060.675174	29.455335
363.040415	21083.410335	29.460352
363.766030	21105.190145	29.465370
364.045805	21143.063557	29.470388
364.185868	21171.992941	29.475405
364.734651	21204.485183	29.480423
364.780883	21244.461532	29.485440
365.142780	21277.583430	29.490458
365.462906	21320.391973	29.495476
365.916125	21351.774721	29.500493
365.733315	21392.551794	29.505511
366.768421	21423.066323	29.510528
367.561542	21456.512729	29.515546
367.524579	21491.182336	29.520564
368.072384	21519.871440	29.525581
368.416817	21551.113580	29.530599
368.447408	21577.842862	29.535616
369.024706	21600.859634	29.540634
369.329047	21637.358997	29.545652
369.814903	21664.073951	29.550669
370.177495	21692.830230	29.555687
370.212741	21720.525735	29.560704
370.713493	21754.277508	29.565722
371.024718	21795.211818	29.570740
371.515562	21831.012540	29.575757
371.628645	21871.952769	29.580775
372.073530	21902.478349	29.585792
372.550693	21940.385557	29.590810
372.529126	21981.088034	29.595828
373.152797	22006.012605	29.600845
373.568750	22054.159740	29.605863
373.936227	22090.075036	29.610880
374.596330	22123.928856	29.615898
374.766427	22163.887659	29.620916
375.479634	22200.728421	29.625933
375.841314	22224.051405	29.630951
376.099086	22255.870610	29.635968
376.371199	22295.832655	29.640986
376.731981	22339.155181	29.646004
377.340673	22363.665502	29.651021
377.447301	22408.317045	29.656039
377.729188	22443.721919	29.661056
378.480093	22482.907943	29.666074
378.478520	22519.374701	29.671092
379.326576	22547.746550	29.676109
379.285845	22579.461376	29.681127
380.146326	22622.598826	29.686144
380.438103	22659.000934	29.691162
381.089311	22692.920309	29.696180
381.376458	22724.027935	29.701197
381.940399	22766.346442	29.706215
382.135528	22795.863559	29.711232
382.413440	22812.470580	29.716250
382.562409	22860.231794	29.721268
383.304186	22886.453339	29.726285
383.891572	22922.146123	29.731303
383.938411	22954.068996	29.736320
384.333156	22989.659375	29.741338
384.732645	23013.836762	29.746356
384.830718	23050.345756	29.751373
385.556314	23093.960335	29.756391
385.685380	23125.864284	29.761408
386.152189	23154.789613	29.766426
386.426659	23198.847915	29.771444
386.783939	23228.447701	29.776461
387.366874	23269.209785	29.781479
387.474404	23298.798242	29.786496
388.007533	23331.694535	29.791514
388.460698	23371.649339	29.796532
388.880125	23419.559106	29.801549
389.120805	23452.627792	29.806567
389.342864	23479.260127	29.811584
390.005937	23519.491992	29.816602
390.073134	23557.807742	29.821620
390.209889	23608.169884	29.826637
390.817679	23642.710651	29.831655
391.585538	23679.570874	29.836672
391.861705	23723.036050	29.841690
391.803151	23763.627894	29.846708
392.565045	23795.939337	29.851725
393.270642	23827.798337	29.856743
393.151710	23864.102673	29.861760
393.757817	23890.681721	29.866778
394.048350	23928.331259	29.871796
394.394865	23976.493919	29.876813
395.280898	23999.503033	29.881831
395.419983	24037.719970	29.886848
395.777436	24064.869029	29.891866
396.063775	24098.708923	29.896884
396.667086	24139.033550	29.901901
397.150973	24169.834557	29.906919
397.321354	24212.268333	29.911936
397.981761	24242.473048	29.916954
398.107624	24279.302228	29.921972
397.990077	24322.040436	29.926989
398.904405	24353.159793	29.932007
399.163088	24393.715860	29.937024
399.408567	24428.990929	29.942042
400.272669	24463.151712	29.947060
400.161929	24508.758334	29.952077
401.013121	24542.194522	29.957095
401.302415	24587.271013	29.962112
401.725627	24623.175823	29.967130
402.360854	24662.232580	29.972148
402.600456	24702.419402	29.977165
403.212568	24731.823506	29.982183
403.455098	24773.008515	29.987200
403.603915	24807.408317	29.992218
404.247857	24847.677448	29.997236
404.362878	24897.635453	30.002253
405.192769	24920.180444	30.007271
405.294874	24966.209783	30.012288
405.825047	25006.408577	30.017306
406.275793	25046.152230	30.022324
406.613236	25090.451298	30.027341
407.173343	25134.386958	30.032359
407.148859	25166.147572	30.037376
407.936810	25207.500831	30.042394
408.171620	25249.364242	30.047412
408.487900	25297.237774	30.052429
409.177111	25328.374949	30.057447
409.491627	25386.632465	30.062464
409.975122	25409.933769	30.067482
410.617575	25447.657431	30.072500
410.747499	25483.666595	30.077517
411.220173	25516.196753	30.082535
411.440214	25568.977605	30.087552
411.908429	25602.292269	30.092570
412.502876	25650.173628	30.097588
412.732984	25691.817497	30.102605
413.000100	25724.114749	30.107623
413.553671	25767.673617	30.112640
413.582081	25811.207396	30.117658
414.573886	25853.699249	30.122676
414.574967	25900.283742	30.127693
415.166269	25937.769852	30.132711
415.811492	25994.618517	30.137728
416.509517	26030.666073	30.142746
416.579124	26068.897747	30.147764
416.475647	26103.604718	30.152781
417.345370	26142.103051	30.157799
417.230015	26188.573723	30.162816
417.870051	26241.890956	30.167834
418.549504	26291.757679	30.172852
419.028358	26331.455221	30.177869
419.464813	26369.440397	30.182887
419.725837	26409.873749	30.187904
420.642062	26447.695442	30.192922
420.490968	26484.906998	30.197940
421.223011	26525.766101	30.202957
421.994192	26553.883909	30.207975
422.000854	26584.169258	30.212992
422.043938	26618.917357	30.218010
422.715426	26655.621169	30.223028
423.290959	26696.644176	30.228045
423.939562	26732.656483	30.233063
423.433592	26775.707210	30.238080
424.001420	26827.861721	30.243098
424.356932	26869.286117	30.248116
424.916182	26919.116330	30.253133
425.324714	26957.081699	30.258151
425.960570	27010.249919	30.263168
426.365125	27060.243756	30.268186
426.902716	27087.444516	30.273204
427.326015	27134.218522	30.278221
427.824905	27171.797236	30.283239
428.178453	27218.664528	30.288256
428.546461	27268.949021	30.293274
429.617131	27309.137259	30.298292
429.197055	27346.127061	30.303309
429.818282	27393.888258	30.308327
430.315138	27441.972431	30.313344
430.360463	27478.883257	30.318362
431.203346	27525.150006	30.323380
431.468282	27577.284356	30.328397
432.442744	27613.967727	30.333415
432.976469	27660.074629	30.338432
433.219159	27705.734216	30.343450
433.736042	27740.340490	30.348468
433.984577	27787.592132	30.353485
434.171637	27822.016343	30.358503
434.639100	27873.658323	30.363520
434.943174	27917.343052	30.368538
435.526984	27964.808057	30.373556
435.811265	28008.034673	30.378573
436.522310	28048.179569	30.383591
436.489857	28101.657577	30.388608
437.157610	28159.431591	30.393626
438.008470	28195.161979	30.398644
438.288500	28244.969641	30.403661
438.790969	28279.522200	30.408679
439.105474	28327.630701	30.413696
439.617664	28379.368085	30.418714
440.063443	28421.078572	30.423732
440.015187	28472.752276	30.428749
440.608380	28510.906522	30.433767
440.939605	28569.916400	30.438784
441.820300	28619.257960	30.443802
442.199882	28664.872962	30.448820
442.457072	28713.471731	30.453837
442.746471	28762.760871	30.458855
443.325253	28802.769942	30.463872
443.674818	28856.594622	30.468890
444.230467	28900.469598	30.473908
444.608034	28960.617432	30.478925
445.310879	29006.523892	30.483943
445.447370	29053.871856	30.488960
446.065632	29102.535091	30.493978
446.503815	29143.192628	30.498996
447.004580	29193.833999	30.504013
447.611914	29241.020151	30.509031
447.923369	29296.975827	30.514048
448.518762	29340.636923	30.519066
449.042837	29388.361103	30.524084
449.605045	29430.289286	30.529101
450.280943	29470.158025	30.534119
450.638887	29516.890825	30.539136
450.721183	29545.841272	30.544154
451.331616	29587.281815	30.549172
451.702256	29634.114030	30.554189
452.362611	29670.173926	30.559207
452.709200	29712.850751	30.564224
452.904034	29758.541364	30.569242
453.250337	29796.009730	30.574260
453.626104	29836.880693	30.579277
454.063707	29882.590448	30.584295
454.671799	29916.528701	30.589312
454.765584	29975.194202	30.594330
455.719404	30009.931830	30.599348
455.898073	30063.754826	30.604365
456.423999	30113.819279	30.609383
457.134643	30160.283369	30.614400
457.284564	30215.489313	30.619418
457.702978	30256.758994	30.624436
458.176915	30311.427699	30.629453
458.697906	30351.455155	30.634471
458.881872	30406.043100	30.639488
459.144819	30452.603254	30.644506
459.694088	30513.620045	30.649524
460.455876	30573.484831	30.654541
461.083352	30619.033724	30.659559
461.597031	30673.488552	30.664576
461.797911	30725.742061	30.669594
462.415874	30769.548040	30.674612
462.814681	30834.420182	30.679629
463.311583	30870.817532	30.684647
463.997458	30923.178899	30.689664
464.310378	30971.123135	30.694682
465.063923	31020.098425	30.699700
465.178361	31071.102024	30.704717
465.642493	31115.647170	30.709735
466.253718	31167.173748	30.714752
466.604517	31226.548488	30.719770
467.324507	31268.537869	30.724788
467.599372	31316.564723	30.729805
467.897661	31365.296049	30.734823
468.379213	31416.571723	30.739840
468.665195	31481.994582	30.744858
469.383965	31531.368472	30.749876
469.871180	31590.602771	30.754893
470.458245	31639.068246	30.759911
471.235498	31682.876491	30.764928
471.869959	31743.662290	30.769946
472.139850	31791.798489	30.774964
472.327344	31841.502879	30.779981
472.989239	31882.130759	30.784999
473.504922	31928.148886	30.790016
474.129072	31980.225456	30.795034
474.275559	32024.765403	30.800052
474.848007	32086.857905	30.805069
475.235579	32132.485623	30.810087
476.063339	32175.142723	30.815104
476.109678	32224.623578	30.820122
476.992985	32275.724644	30.825140
477.042340	32337.596367	30.830157
477.424912	32375.240723	30.835175
477.838873	32432.579640	30.840192
478.207252	32495.185791	30.845210
478.718265	32541.149102	30.850228
479.478464	32605.641407	30.855245
479.708687	32658.375641	30.860263
480.601265	32703.394453	30.865280
480.961217	32765.300978	30.870298
481.736888	32807.651423	30.875316
481.899458	32854.529807	30.880333
482.550272	32898.752382	30.885351
483.173101	32943.466241	30.890368
483.200592	32997.017030	30.895386
483.858157	33036.528806	30.900404
484.338727	33093.068823	30.905421
484.748935	33145.093291	30.910439
484.851545	33187.436123	30.915456
485.258983	33244.361014	30.920474
486.291578	33293.885908	30.925492
486.489142	33335.480781	30.930509
486.890528	33394.449128	30.935527
487.366645	33441.488348	30.940544
487.678774	33500.312914	30.945562
488.475665	33552.979607	30.950580
488.874974	33616.323974	30.955597
489.385519	33669.282381	30.960615
489.764376	33722.337415	30.965632
490.087747	33782.678387	30.970650
491.066230	33837.441687	30.975668
491.536310	33890.577694	30.980685
491.970373	33953.411834	30.985703
492.457347	34000.829953	30.990720
492.687469	34057.873331	30.995738
493.405095	34104.800337	31.000756
494.046764	34169.537297	31.005773
494.204331	34226.447075	31.010791
494.953446	34290.743967	31.015808
495.248798	34345.874809	31.020826
495.948220	34394.310089	31.025844
496.097401	34456.425309	31.030861
496.877044	34510.671433	31.035879
497.613982	34566.138336	31.040896
497.937350	34621.802936	31.045914
498.219578	34678.340335	31.050932
498.791813	34744.013043	31.055949
499.372225	34811.973504	31.060967
499.850347	34860.640518	31.065984
500.362586	34919.058327	31.071002
501.068665	34982.927792	31.076020
501.647504	35033.912538	31.081037
502.054211	35090.450508	31.086055
502.822387	35152.470818	31.091072
503.338397	35212.147089	31.096090
503.722296	35250.251622	31.101108
504.368247	35308.213283	31.106125
504.561607	35374.756614	31.111143
504.869482	35417.299386	31.116160
505.757347	35486.560635	31.121178
506.013547	35533.904519	31.126196
506.731220	35600.556126	31.131213
506.977247	35651.752555	31.136231
507.951662	35712.047638	31.141248
508.209437	35765.246892	31.146266
508.565581	35813.890934	31.151284
509.495406	35875.755254	31.156301
509.817819	35932.732311	31.161319
510.487663	35981.947264	31.166336
510.757345	36046.691308	31.171354
511.227891	36096.645929	31.176372
511.770192	36142.997890	31.181389
512.327329	36210.245630	31.186407
513.338928	36256.650798	31.191424
513.502184	36314.861527	31.196442
513.809559	36371.077004	31.201460
514.719352	36425.497332	31.206477
515.415317	36476.068827	31.211495
515.913323	36517.622886	31.216512
516.154148	36573.463600	31.221530
516.465208	36618.676685	31.226548
517.194890	36655.395364	31.231565
517.583228	36717.890739	31.236583
518.093231	36759.671028	31.241600
518.422606	36824.825418	31.246618
518.644950	36879.070021	31.251636
519.457204	36917.142061	31.256653
519.857090	36980.976946	31.261671
520.568660	37034.019757	31.266688
520.845586	37083.450550	31.271706
521.321315	37143.448379	31.276724
521.555562	37198.962936	31.281741
522.574522	37262.461409	31.286759
522.744578	37312.231963	31.291776
523.405210	37373.112055	31.296794
523.857381	37434.170410	31.301812
524.451934	37490.299580	31.306829
524.627800	37555.024934	31.311847
525.548613	37612.583035	31.316864
526.068333	37675.686654	31.321882
526.634879	37738.991804	31.326900
527.181851	37798.809568	31.331917
527.385487	37858.352442	31.336935
528.191703	37918.863478	31.341952
528.507836	37981.614137	31.346970
529.217210	38040.616678	31.351988
529.917767	38101.189041	31.357005
530.473002	38166.571394	31.362023
530.968300	38224.551905	31.367040
531.291579	38288.661942	31.372058
531.835733	38353.502754	31.377076
532.335114	38419.394200	31.382093
532.927495	38488.711439	31.387111
533.298969	38548.577740	31.392128
533.985854	38606.099248	31.397146
534.567200	38677.568932	31.402164
535.511576	38734.171434	31.407181
535.702377	38795.622393	31.412199
536.281869	38855.811103	31.417216
536.937456	38916.810176	31.422234
537.256561	38982.219331	31.427252
538.181855	39041.873778	31.432269
538.711683	39112.265241	31.437287
539.374276	39163.126537	31.442304
540.047931	39226.153660	31.447322
540.050333	39283.417377	31.452340
540.721694	39338.394669	31.457357
541.436392	39405.918624	31.462375
542.109593	39466.227158	31.467392
542.473558	39527.653069	31.472410
542.873526	39587.144652	31.477428
543.440442	39641.247365	31.482445
543.671934	39702.764084	31.487463
544.517940	39764.627425	31.492480
545.168888	39829.392684	31.497498
545.268000	39888.027847	31.502516
546.154253	39962.628771	31.507533
546.592779	40026.238926	31.512551
547.056086	40090.433543	31.517568
547.648390	40160.002779	31.522586
548.475807	40227.581198	31.527604
548.992423	40284.172522	31.532621
548.916694	40353.480189	31.537639
549.831605	40414.088685	31.542656
550.339132	40476.652147	31.547674
550.877715	40543.106765	31.552692
551.173596	40608.303088	31.557709
551.808529	40667.216916	31.562727
552.437959	40720.427093	31.567744
552.994443	40799.098562	31.572762
553.340419	40862.902733	31.577780
554.120640	40922.705224	31.582797
554.715335	40983.896712	31.587815
555.196289	41045.201053	31.592832
555.980958	41101.480555	31.597850
556.461213	41175.333337	31.602868
557.113588	41228.117406	31.607885
557.452445	41294.605586	31.612903
557.948943	41358.052418	31.617920
558.629708	41428.003960	31.622938
558.859129	41489.633547	31.627956
559.763471	41554.553972	31.632973
560.100255	41623.054727	31.637991
560.103712	41683.999229	31.643008
560.858964	41756.723039	31.648026
560.984431	41823.960938	31.653044
561.878697	41905.195605	31.658061
562.435288	41981.999152	31.663079
563.138493	42054.466454	31.668096
564.164274	42133.081851	31.673114
564.475257	42208.197961	31.678132
565.090359	42269.364532	31.683149
565.982202	42340.057554	31.688167
566.128518	42411.683482	31.693184
567.195243	42477.238991	31.698202
567.557404	42549.881509	31.703220
568.513561	42617.130874	31.708237
569.095900	42699.701298	31.713255
569.604757	42756.072504	31.718272
569.977903	42821.541584	31.723290
570.304338	42890.421072	31.728308
571.362177	42963.512602	31.733325
571.922970	43032.400103	31.738343
572.180573	43105.857786	31.743360
573.035619	43164.914606	31.748378
573.475979	43240.640149	31.753396
574.311325	43306.101525	31.758413
574.801281	43377.373145	31.763431
575.169723	43440.485478	31.768448
576.248554	43508.085202	31.773466
576.162717	43581.522343	31.778484
577.098241	43635.045834	31.783501
577.191548	43713.907767	31.788519
578.241936	43777.976910	31.793536
579.132455	43868.808597	31.798554
579.328429	43932.664104	31.803572
579.850064	43998.043816	31.808589
580.445492	44062.444374	31.813607
581.068143	44133.273830	31.818624
581.670727	44197.730587	31.823642
582.204849	44266.657717	31.828660
583.124315	44336.928970	31.833677
583.691722	44411.525311	31.838695
583.792564	44473.398398	31.843712
584.632828	44542.196200	31.848730
585.086507	44612.990386	31.853748
586.052755	44686.607972	31.858765
586.319724	44756.381803	31.863783
587.041239	44826.072013	31.868800
587.774031	44885.645945	31.873818
587.883628	44973.308761	31.878836
588.740321	45033.078755	31.883853
589.133497	45101.227167	31.888871
589.530635	45175.169541	31.893888
590.446890	45242.293925	31.898906
591.113381	45313.822413	31.903924
591.601192	45376.402808	31.908941
592.143525	45438.399189	31.913959
592.626754	45496.647454	31.918976
593.348460	45559.147446	31.923994
593.843436	45632.702779	31.929012
594.412879	45704.582981	31.934029
595.117525	45776.568757	31.939047
595.420598	45843.613845	31.944064
596.352595	45908.036584	31.949082
596.388916	45984.290164	31.954100
597.400309	46041.476598	31.959117
598.044617	46123.556550	31.964135
598.653234	46200.714415	31.969152
599.196546	46257.582492	31.974170
599.588323	46336.077945	31.979188
600.112068	46408.935438	31.984205
601.058195	46482.872041	31.989223
601.412533	46552.441649	31.994240
602.309844	46624.564437	31.999258
602.529071	46704.562184	32.004276
603.329640	46774.043610	32.009293
603.708125	46857.920214	32.014311
604.345641	46924.479624	32.019328
605.231895	47006.739983	32.024346
605.659814	47081.360694	32.029364
606.185405	47148.849275	32.034381
606.712118	47227.813810	32.039399
606.924617	47312.920091	32.044416
608.029330	47391.516316	32.049434
608.407616	47470.239232	32.054452
609.342750	47552.531873	32.059469
609.834067	47635.640837	32.064487
610.415654	47718.495563	32.069504
611.187228	47791.160523	32.074522
611.934523	47881.733491	32.079540
612.376549	47949.825901	32.084557
613.264471	48027.117054	32.089575
613.475580	48109.018974	32.094592
614.115517	48183.882139	32.099610
615.009296	48272.415540	32.104628
615.274261	48341.574411	32.109645
616.069063	48428.706755	32.114663
616.785209	48510.878987	32.119680
617.634951	48591.474227	32.124698
618.645338	48677.922109	32.129716
619.169177	48747.490862	32.134733
619.615371	48819.501460	32.139751
620.222038	48905.855261	32.144768
621.072793	48970.951077	32.149786
621.245709	49046.080008	32.154804
621.957866	49127.268094	32.159821
622.615430	49207.243933	32.164839
623.210412	49282.687149	32.169856
623.909780	49354.096683	32.174874
624.218991	49435.766541	32.179892
625.051863	49514.798591	32.184909
625.942699	49594.321667	32.189927
626.230367	49673.850901	32.194944
627.275356	49735.356372	32.199962
627.346040	49827.377996	32.204980
627.932941	49902.508160	32.209997
628.771881	49993.663540	32.215015
629.517018	50066.409457	32.220032
630.241225	50142.860245	32.225050
630.908646	50220.762767	32.230068
631.250559	50299.013906	32.235085
632.189799	50375.906327	32.240103
632.573872	50451.955849	32.245120
633.382891	50519.814918	32.250138
633.385267	50591.312131	32.255156
633.994969	50661.828636	32.260173
634.696335	50737.475079	32.265191
635.347799	50828.030383	32.270208
636.439472	50892.106840	32.275226
637.085696	50971.071872	32.280244
637.249788	51050.593557	32.285261
638.077002	51126.272180	32.290279
638.288709	51210.260417	32.295296
639.522425	51288.944703	32.300314
640.050970	51370.454167	32.305332
640.820908	51453.938250	32.310349
641.652299	51520.651473	32.315367
641.723473	51602.492805	32.320384
642.270841	51682.817170	32.325402
642.835430	51773.940261	32.330420
643.286865	51852.318690	32.335437
643.996256	51931.283417	32.340455
644.598504	52032.006926	32.345472
645.520858	52115.368268	32.350490
646.387015	52206.933053	32.355508
646.922522	52290.855491	32.360525
647.652036	52373.773378	32.365543
648.079728	52468.356573	32.370560
648.947337	52543.963870	32.375578
649.517073	52639.848017	32.380596
650.169523	52724.253591	32.385613
651.117168	52807.480556	32.390631
651.886652	52899.474500	32.395648
652.512325	52978.487514	32.400666
653.228187	53060.239310	32.405684
653.899457	53153.989808	32.410701
654.741248	53233.045768	32.415719
654.920222	53319.293131	32.420736
655.751979	53397.414675	32.425754
656.395101	53482.083882	32.430772
656.854100	53568.560409	32.435789
657.592532	53652.380001	32.440807
658.574618	53739.920620	32.445824
658.879373	53822.271005	32.450842
659.768950	53910.440572	32.455860
660.252163	53999.541065	32.460877
661.355119	54079.951165	32.465895
661.805552	54167.291861	32.470912
662.601987	54247.718894	32.475930
663.314409	54342.435893	32.480948
664.100593	54424.080156	32.485965
664.855437	54496.148568	32.490983
665.449512	54591.707777	32.496000
665.935597	54656.655110	32.501018
666.452018	54754.853397	32.506036
666.939524	54840.766889	32.511053
667.932634	54911.938592	32.516071
668.563961	55011.923543	32.521088
669.436748	55096.246143	32.526106
670.390302	55175.791050	32.531124
670.769678	55254.761651	32.536141
671.840488	55325.397161	32.541159
672.392584	55414.682040	32.546176
672.974029	55486.875544	32.551194
673.436074	55575.497972	32.556212
674.009682	55658.869502	32.561229
674.901862	55725.901557	32.566247
675.472783	55816.798792	32.571264
676.465436	55894.124951	32.576282
677.301834	55979.677811	32.581300
677.690957	56057.839472	32.586317
678.421242	56124.030966	32.591335
678.836057	56195.632493	32.596352
679.446094	56274.374154	32.601370
679.938899	56339.040227	32.606388
680.260498	56428.314362	32.611405
681.060436	56498.470475	32.616423
681.421966	56592.377996	32.621440
682.126441	56675.264241	32.626458
682.997856	56759.890390	32.631476
683.888811	56852.836305	32.636493
684.676137	56939.242024	32.641511
685.012612	57022.801005	32.646528
685.736712	57103.780637	32.651546
686.280472	57190.098821	32.656564
687.223458	57283.025593	32.661581
688.122236	57361.655984	32.666599
688.510036	57454.094416	32.671616
688.715753	57545.270580	32.676634
689.730933	57640.738054	32.681652
690.248161	57744.973813	32.686669
691.288904	57824.077153	32.691687
691.827905	57921.449440	32.696704
692.169978	58016.144049	32.701722
693.172013	58109.634388	32.706740
693.820263	58206.199556	32.711757
694.936903	58295.039636	32.716775
695.442477	58398.596471	32.721792
696.294986	58480.415070	32.726810
696.794392	58575.941690	32.731828
697.648095	58671.470166	32.736845
698.240091	58767.767886	32.741863
698.745711	58861.813571	32.746880
699.857840	58959.309144	32.751898
700.630636	59057.332960	32.756916
701.265023	59145.004763	32.761933
701.877279	59226.971102	32.766951
702.450054	59336.002786	32.771968
703.177506	59431.224879	32.776986
703.915072	59524.458260	32.782004
704.613700	59623.723913	32.787021
705.479526	59713.741462	32.792039
706.030754	59801.333701	32.797056
706.869529	59895.280562	32.802074
707.478534	59990.010674	32.807092
707.990967	60097.510749	32.812109
709.148522	60193.706539	32.817127
709.756612	60287.279593	32.822144
710.275845	60387.627186	32.827162
711.357641	60481.373661	32.832180
711.714865	60565.796102	32.837197
712.783009	60664.558685	32.842215
713.532131	60769.505332	32.847232
714.568584	60856.816466	32.852250
715.361707	60948.204544	32.857268
715.775733	61040.867689	32.862285
716.383631	61118.568283	32.867303
716.683825	61231.062962	32.872320
717.820689	61317.277564	32.877338
718.746229	61420.338314	32.882356
719.331934	61511.773622	32.887373
720.067898	61595.690840	32.892391
720.563954	61695.053553	32.897408
721.550368	61783.857066	32.902426
722.196737	61872.169749	32.907444
722.522165	61966.179583	32.912461
723.939377	62053.536609	32.917479
724.449480	62150.138951	32.922496
725.075024	62237.867481	32.927514
725.695962	62327.091002	32.932532
726.126326	62410.938560	32.937549
726.649460	62495.006098	32.942567
727.512619	62587.357811	32.947584
728.012684	62693.548068	32.952602
729.014282	62776.946571	32.957620
729.325382	62875.399733	32.962637
730.131209	62965.109356	32.967655
731.052464	63060.137856	32.972672
731.607519	63164.479325	32.977690
732.479876	63250.279938	32.982708
733.155216	63364.605709	32.987725
734.117161	63455.508122	32.992743
734.896669	63554.352743	32.997760
735.555668	63662.123883	33.002778
736.544794	63746.312582	33.007796
737.262203	63849.251391	33.012813
737.812463	63945.632820	33.017831
738.372139	64049.356839	33.022848
739.021408	64153.231856	33.027866
739.961919	64241.804414	33.032884
740.758182	64340.655841	33.037901
741.957122	64450.181756	33.042919
742.266924	64551.281677	33.047936
742.794567	64642.731219	33.052954
744.004029	64749.047010	33.057972
744.459753	64857.779425	33.062989
745.115759	64962.600041	33.068007
746.171543	65058.165838	33.073024
746.647724	65161.179441	33.078042
747.644582	65263.921994	33.083060
748.379041	65369.105544	33.088077
749.114932	65460.278521	33.093095
750.010787	65574.554472	33.098112
750.550911	65670.051383	33.103130
751.640323	65768.577589	33.108148
752.182265	65881.903685	33.113165
752.846438	65973.665880	33.118183
754.049138	66083.559164	33.123200
754.690175	66190.071321	33.128218
755.655542	66279.299250	33.133236
756.375398	66385.438995	33.138253
757.423614	66486.190409	33.143271
758.070328	66588.239717	33.148288
758.735647	66690.413149	33.153306
759.529781	66784.253617	33.158324
760.016127	66876.236852	33.163341
760.885967	66979.151852	33.168359
761.425305	67086.589080	33.173376
762.178684	67184.299631	33.178394
763.328211	67274.084702	33.183412
763.982367	67381.460866	33.188429
764.559909	67484.594622	33.193447
765.017513	67592.040435	33.198464
765.756503	67685.949826	33.203482
767.310156	67790.958097	33.208500
767.904509	67900.827825	33.213517
768.615339	67998.731758	33.218535
769.536457	68099.154841	33.223552
769.932322	68210.386644	33.228570
770.676475	68299.162370	33.233588
771.275281	68394.571613	33.238605
772.415444	68501.483770	33.243623
773.165348	68609.673207	33.248640
774.135804	68714.884212	33.253658
774.636439	68813.989228	33.258676
775.574884	68918.870482	33.263693
776.290776	69005.854778	33.268711
777.091632	69093.275636	33.273728
777.513055	69198.485932	33.278746
778.236342	69290.864931	33.283764
779.208073	69385.427920	33.288781
779.979623	69488.146706	33.293799
780.494491	69580.705012	33.298816
781.102349	69682.538370	33.303834
782.143976	69776.806890	33.308852
782.915641	69884.042072	33.313869
783.522697	69996.077980	33.318887
784.360722	70093.336685	33.323904
785.148440	70196.809273	33.328922
785.945360	70301.192683	33.333940
786.798455	70409.962359	33.338957
787.399195	70506.335236	33.343975
788.498021	70612.445675	33.348992
789.064051	70729.329096	33.354010
789.669340	70831.211661	33.359028
790.435505	70936.210333	33.364045
791.308963	71040.344070	33.369063
792.091271	71154.269905	33.374080
792.676378	71263.920980	33.379098
793.582882	71382.666422	33.384116
794.381116	71489.650712	33.389133
795.224865	71597.451552	33.394151
796.280192	71719.417514	33.399168
796.975545	71837.349493	33.404186
797.797084	71940.671672	33.409204
798.514253	72060.045087	33.414221
799.297994	72165.590522	33.419239
800.265437	72289.130736	33.424256
801.056446	72408.481494	33.429274
802.252431	72506.275690	33.434292
802.739308	72630.488034	33.439309
803.442170	72726.587055	33.444327
804.599863	72850.784047	33.449344
805.275552	72958.756071	33.454362
806.190554	73067.501681	33.459380
806.937100	73180.124580	33.464397
807.280553	73297.649511	33.469415
808.354991	73412.869258	33.474432
809.160051	73537.238665	33.479450
810.006241	73648.885310	33.484468
810.442505	73763.636520	33.489485
811.570062	73888.539712	33.494503
812.601670	74001.058104	33.499520
813.030410	74123.576538	33.504538
813.849731	74228.909248	33.509556
814.850912	74349.515100	33.514573
815.709633	74472.208460	33.519591
816.804205	74584.174774	33.524608
817.492845	74711.835863	33.529626
818.711865	74812.282248	33.534644
819.484886	74934.725134	33.539661
820.194946	75052.618354	33.544679
821.114161	75155.241001	33.549696
821.930581	75269.027089	33.554714
822.851591	75383.101288	33.559732
823.846404	75501.521895	33.564749
824.417503	75604.213425	33.569767
825.483776	75712.363374	33.574784
825.789670	75823.533621	33.579802
826.687824	75932.711487	33.584820
827.608552	76044.394395	33.589837
828.571851	76160.226007	33.594855
829.538278	76272.814751	33.599872
829.908657	76388.524831	33.604890
830.658292	76481.437735	33.609908
831.635545	76586.134191	33.614925
831.839626	76695.347795	33.619943
832.758910	76802.676366	33.624960
834.104152	76935.476875	33.629978
835.045917	77033.492022	33.634996
835.609543	77144.335940	33.640013
836.152221	77253.296067	33.645031
837.082053	77366.186416	33.650048
837.972553	77483.061147	33.655066
838.457484	77600.215240	33.660084
839.309744	77717.603681	33.665101
840.077214	77840.605240	33.670119
841.272238	77949.858699	33.675136
841.878890	78070.846882	33.680154
842.318777	78193.546600	33.685172
843.467216	78318.732940	33.690189
844.004677	78445.903118	33.695207
845.125476	78569.726730	33.700224
845.981970	78688.157462	33.705242
846.995889	78811.986226	33.710260
848.247061	78942.112741	33.715277
848.631971	79066.623896	33.720295
849.801286	79186.198638	33.725312
850.562036	79305.989897	33.730330
851.557543	79434.929878	33.735348
852.276468	79550.383300	33.740365
853.438597	79680.514551	33.745383
854.026529	79799.106098	33.750400
854.869280	79929.655925	33.755418
855.858197	80044.777730	33.760436
857.318643	80165.603353	33.765453
857.816625	80297.982583	33.770471
858.804780	80413.802840	33.775488
859.455654	80546.501377	33.780506
860.199296	80654.227146	33.785524
861.230135	80783.877316	33.790541
861.900642	80912.102164	33.795559
862.982737	81036.284882	33.800576
863.592733	81167.054297	33.805594
864.503156	81286.855946	33.810612
865.621873	81412.098848	33.815629
866.225332	81545.658403	33.820647
867.451127	81663.271062	33.825664
868.348655	81794.733221	33.830682
869.073135	81912.095994	33.835700
870.105995	82033.085293	33.840717
870.602835	82162.673378	33.845735
871.923644	82287.812498	33.850752
872.261520	82426.219801	33.855770
873.412454	82540.363504	33.860788
874.584073	82674.979750	33.865805
875.457750	82805.702779	33.870823
876.063327	82919.211181	33.875840
877.100063	83052.279191	33.880858
878.001165	83170.683834	33.885876
879.007483	83300.209997	33.890893
879.625099	83422.296549	33.895911
880.471262	83545.412181	33.900928
881.661638	83670.945255	33.905946
882.319401	83802.492245	33.910964
883.113241	83922.082514	33.915981
883.931613	84055.303421	33.920999
884.785331	84181.385611	33.926016
885.571597	84308.847396	33.931034
886.370510	84442.364577	33.936052
887.739401	84565.605473	33.941069
888.086666	84699.473331	33.946087
889.046309	84817.698206	33.951104
889.972477	84946.636120	33.956122
891.096382	85052.380272	33.961140
891.978169	85179.501489	33.966157
892.366254	85298.730171	33.971175
893.417239	85421.530307	33.976192
894.303337	85545.205781	33.981210
894.992675	85666.086802	33.986228
895.925352	85787.221675	33.991245
896.593229	85931.714634	33.996263
898.030631	86048.627885	34.001280
898.509315	86189.362859	34.006298
899.480980	86310.709227	34.011316
900.614071	86440.711163	34.016333
900.983011	86584.531856	34.021351
902.089215	86714.222416	34.026368
903.202024	86844.457421	34.031386
903.543821	86976.448450	34.036404
904.738611	87114.934136	34.041421
905.731863	87262.740889	34.046439
906.658442	87395.757408	34.051456
907.657044	87538.039522	34.056474
908.505700	87686.073801	34.061492
909.603920	87809.066657	34.066509
910.314332	87949.761114	34.071527
911.783848	88088.550525	34.076544
912.855613	88230.571068	34.081562
913.320475	88369.835924	34.086580
914.593253	88499.343517	34.091597
915.599213	88633.012168	34.096615
916.507309	88763.591853	34.101632
917.321178	88897.545232	34.106650
918.699433	89034.312995	34.111668
919.532056	89158.265503	34.116685
920.135925	89291.822647	34.121703
921.148536	89432.007898	34.126720
922.175558	89561.419186	34.131738
923.374865	89695.417185	34.136756
924.300314	89824.439967	34.141773
924.754306	89954.589025	34.146791
925.839731	90089.202273	34.151808
926.755691	90223.056892	34.156826
927.600654	90358.482090	34.161844
928.522731	90491.715936	34.166861
929.460184	90637.583761	34.171879
930.659871	90773.069346	34.176896
931.525709	90907.581224	34.181914
932.657403	91042.077423	34.186932
933.164034	91177.800079	34.191949
934.436380	91318.333679	34.196967
934.950897	91455.044922	34.201984
935.898642	91596.289691	34.207002
937.059960	91727.856551	34.212020
937.946532	91863.484762	34.217037
938.796222	92008.891308	34.222055
939.700850	92147.078183	34.227072
940.410101	92283.902079	34.232090
941.703348	92432.130982	34.237108
942.789928	92562.927327	34.242125
943.523097	92700.902736	34.247143
944.141608	92844.004639	34.252160
944.947684	92985.645589	34.257178
946.013585	93141.949347	34.262196
947.266184	93278.781338	34.267213
948.281441	93417.856545	34.272231
949.188083	93554.262280	34.277248
950.279364	93695.075990	34.282266
951.031363	93847.858106	34.287284
952.393242	93969.364474	34.292301
952.965698	94110.147234	34.297319
954.061579	94229.782310	34.302336
954.773044	94364.016675	34.307354
955.511160	94504.230246	34.312372
956.669680	94636.925447	34.317389
957.827124	94760.621759	34.322407
958.302843	94890.027907	34.327424
959.491840	95024.519922	34.332442
960.440602	95169.152655	34.337460
961.352483	95302.079443	34.342477
962.122594	95447.945636	34.347495
963.186248	95578.454109	34.352512
964.322427	95727.154382	34.357530
964.969040	95872.192600	34.362548
966.032953	96005.225330	34.367565
966.741453	96160.953762	34.372583
967.666244	96310.653279	34.377600
968.909829	96447.779500	34.382618
969.869465	96602.127115	34.387636
971.172446	96745.494732	34.392653
971.831972	96897.837216	34.397671
972.789658	97051.819717	34.402688
974.248884	97187.305477	34.407706
974.894421	97347.461041	34.412724
976.163608	97488.897801	34.417741
976.480052	97642.273677	34.422759
977.949268	97786.190425	34.427776
978.730116	97930.063480	34.432794
979.398005	98092.374347	34.437812
980.669575	98244.576749	34.442829
981.649856	98398.574907	34.447847
982.439373	98551.348646	34.452864
983.915739	98706.411547	34.457882
984.327366	98862.339147	34.462900
986.079758	99013.975514	34.467917
986.897124	99171.666608	34.472935
988.019807	99320.170302	34.477952
988.836214	99470.776373	34.482970
989.716742	99624.605861	34.487988
990.394144	99785.592656	34.493005
991.500763	99937.917641	34.498023
992.736534	100094.013739	34.503040
994.299931	100255.193767	34.508058
994.737883	100416.525447	34.513076
995.674085	100559.599901	34.518093
996.965655	100716.717158	34.523111
998.103861	100873.402778	34.528128
999.214018	101023.044566	34.533146
1000.186873	101183.941308	34.538164
1001.175132	101336.811170	34.543181
1002.167340	101485.662140	34.548199
1003.119451	101632.656360	34.553216
1004.033363	101784.741219	34.558234
1005.131811	101936.823245	34.563252
1006.197771	102095.465806	34.568269
1006.897769	102247.053797	34.573287
1008.169984	102406.527698	34.578304
1009.307554	102553.027880	34.583322
1010.055378	102713.396793	34.588340
1011.282876	102872.981371	34.593357
1012.365847	103017.869280	34.598375
1013.563132	103176.902184	34.603392
1014.635248	103317.748550	34.608410
1015.313571	103481.821609	34.613428
1016.847919	103635.757708	34.618445
1018.190237	103776.335485	34.623463
1018.707305	103914.912967	34.628480
1019.771487	104052.784084	34.633498
1020.834988	104190.313535	34.638516
1021.512782	104324.987706	34.643533
1022.595317	104463.998774	34.648551
1023.392773	104603.422752	34.653568
1024.958878	104739.100647	34.658586
1025.366468	104886.131095	34.663604
1026.291652	105025.359308	34.668621
1027.377448	105173.375264	34.673639
1028.053292	105321.456051	34.678656
1029.263962	105472.408122	34.683674
1030.091330	105631.992395	34.688692
1031.400429	105779.481527	34.693709
1032.493695	105930.238458	34.698727
1033.507290	106092.534589	34.703744
1034.649335	106241.155030	34.708762
1035.515841	106396.856683	34.713780
1036.554573	106555.321705	34.718797
1037.534957	106712.325696	34.723815
1038.449330	106868.148800	34.728832
1039.799344	107020.303207	34.733850
1040.571357	107200.889342	34.738868
1041.319980	107344.465984	34.743885
1042.430343	107507.134074	34.748903
1043.493803	107667.794073	34.753920
1044.739660	107832.382602	34.758938
1045.914311	108004.033497	34.763956
1046.965136	108166.371633	34.768973
1048.010150	108322.294975	34.773991
1048.847483	108492.213109	34.779008
1050.102966	108651.807777	34.784026
1051.393850	108823.127499	34.789044
1052.386416	108983.868090	34.794061
1053.099713	109150.499110	34.799079
1054.011029	109317.759339	34.804096
1055.572008	109487.860687	34.809114
1056.406998	109662.971480	34.814132
1057.611432	109817.329422	34.819149
1058.364866	109987.965422	34.824167
1059.410222	110163.109173	34.829184
1060.560129	110333.735499	34.834202
1061.642290	110505.349732	34.839220
1062.750369	110682.730871	34.844237
1063.782874	110847.100655	34.849255
1064.874506	111029.038817	34.854272
1066.282684	111194.632247	34.859290
1067.404602	111375.768487	34.864308
1068.072240	111533.705454	34.869325
1069.603230	111709.021753	34.874343
1070.451993	111876.494086	34.879360
1071.988268	112043.859564	34.884378
1073.150207	112213.795495	34.889396
1074.140480	112395.274553	34.894413
1075.302439	112557.463272	34.899431
1076.507970	112715.904611	34.904448
1077.634965	112876.273981	34.909466
1078.838660	113037.989076	34.914484
1079.873177	113202.394703	34.919501
1080.973462	113365.509841	34.924519
1081.640155	113528.883832	34.929536
1083.145057	113686.546955	34.934554
1083.810735	113853.258102	34.939572
1085.277297	114014.568588	34.944589
1085.970694	114178.727642	34.949607
1087.114427	114348.295939	34.954624
1088.165586	114503.585827	34.959642
1088.987140	114677.949510	34.964660
1090.225566	114843.002799	34.969677
1091.552265	114998.733597	34.974695
1092.295252	115151.880289	34.979712
1093.508410	115306.475993	34.984730
1094.609155	115466.264722	34.989748
1095.508880	115622.331344	34.994765
1096.778821	115777.744544	34.999783
1097.789909	115934.200912	35.004800
1099.010044	116101.139827	35.009818
1099.858069	116266.083011	35.014836
1100.672269	116423.028864	35.019853
1102.039092	116587.220015	35.024871
1102.918769	116761.964904	35.029888
1104.172531	116922.763307	35.034906
1105.065398	117094.793353	35.039924
1106.193768	117263.958811	35.044941
1107.276021	117426.929798	35.049959
1108.093316	117606.559013	35.054976
1109.735947	117773.794383	35.059994
1110.680393	117953.633655	35.065012
1111.542025	118127.588600	35.070029
1112.638339	118314.521632	35.075047
1113.613247	118495.804705	35.080064
1114.859150	118674.623503	35.085082
1116.102092	118855.942434	35.090100
1116.758532	119038.812759	35.095117
1118.127187	119211.196503	35.100135
1119.297487	119415.754855	35.105152
1120.558614	119591.290238	35.110170
1121.407432	119777.216336	35.115188
1122.773028	119970.406918	35.120205
1123.751702	120151.583064	35.125223
1124.886285	120350.266195	35.130240
1126.386961	120520.554801	35.135258
1127.323504	120726.272965	35.140276
1128.450395	120909.002387	35.145293
1130.335487	121089.977583	35.150311
1131.064513	121275.257298	35.155328
1132.429396	121460.565198	35.160346
1133.476634	121644.452204	35.165364
1134.719143	121831.201771	35.170381
1136.075430	122015.701773	35.175399
1137.182220	122196.182334	35.180416
1138.157484	122370.582553	35.185434
1139.432275	122552.167456	35.190452
1140.392920	122742.504752	35.195469
1141.881470	122922.687833	35.200487
1142.740082	123112.459331	35.205504
1144.065407	123295.803050	35.210522
1145.342725	123477.150752	35.215540
1146.180206	123651.172210	35.220557
1147.489657	123831.920250	35.225575
1148.782886	124023.201099	35.230592
1150.094826	124208.898023	35.235610
1151.192467	124386.357945	35.240628
1152.481359	124577.337638	35.245645
1153.537108	124754.336344	35.250663
1154.363700	124931.726916	35.255680
1155.516104	125114.091087	35.260698
1156.851055	125295.146163	35.265716
1157.897237	125478.860680	35.270733
1159.438810	125662.942503	35.275751
1160.401192	125844.870289	35.280768
1161.390175	126024.346182	35.285786
1162.949027	126205.319495	35.290804
1163.612282	126393.424255	35.295821
1165.214587	126579.124600	35.300839
1166.366153	126753.846017	35.305856
1167.557934	126934.156843	35.310874
1168.355998	127099.508622	35.315892
1169.125553	127287.055266	35.320909
1170.724287	127449.035196	35.325927
1171.849655	127628.065345	35.330944
1172.897263	127795.778711	35.335962
1174.118599	127965.660459	35.340980
1175.254577	128147.596570	35.345997
1176.659802	128316.981524	35.351015
1177.417986	128498.965615	35.356032
1178.501918	128673.223543	35.361050
1180.037310	128855.404693	35.366068
1180.959857	129047.134857	35.371085
1181.947634	129215.929020	35.376103
1183.265146	129411.189619	35.381120
1184.275425	129596.932608	35.386138
1185.018423	129782.692874	35.391156
1186.261975	129978.843119	35.396173
1187.711529	130155.219533	35.401191
1188.755603	130360.297022	35.406208
1190.120870	130557.775797	35.411226
1191.157602	130754.774009	35.416244
1192.017557	130962.573080	35.421261
1193.556801	131155.776814	35.426279
1194.483738	131359.519753	35.431296
1195.800211	131557.048805	35.436314
1196.920458	131760.408090	35.441332
1198.238084	131976.311729	35.446349
1199.393525	132172.536490	35.451367
1201.005844	132378.854192	35.456384
1201.973437	132576.201390	35.461402
1203.451236	132782.795825	35.466420
1204.648737	132991.313050	35.471437
1206.015561	133194.957612	35.476455
1206.824934	133405.580458	35.481472
1208.051580	133610.048275	35.486490
1209.373130	133810.961937	35.491508
1210.846552	134014.821979	35.496525
1212.169812	134214.937783	35.501543
1213.529560	134421.241102	35.506560
1214.443395	134617.857135	35.511578
1215.952930	134828.288265	35.516596
1217.303420	135034.240549	35.521613
1217.988568	135242.226721	35.526631
1219.426036	135448.459134	35.531648
1220.499932	135659.660257	35.536666
1221.906399	135868.576928	35.541684
1222.959190	136078.146338	35.546701
1224.654817	136283.022397	35.551719
1225.673969	136492.802010	35.556736
1227.036778	136706.957539	35.561754
1228.852810	136901.234188	35.566772
1229.876920	137106.307873	35.571789
1231.318257	137308.867984	35.576807
1232.229533	137508.212542	35.581824
1233.707744	137708.040263	35.586842
1234.649445	137901.620435	35.591860
1235.801911	138109.876385	35.596877
1237.369799	138312.801766	35.601895
1238.470259	138516.270742	35.606912
1239.425241	138717.326817	35.611930
1241.057708	138914.622851	35.616948
1241.976789	139126.853885	35.621965
1243.445585	139332.768756	35.626983
1244.349389	139539.445569	35.632000
1245.791972	139742.333266	35.637018
1247.108750	139948.629943	35.642036
1248.226159	140149.298636	35.647053
1249.430094	140338.685176	35.652071
1250.703386	140542.097712	35.657088
1251.703575	140731.606532	35.662106
1252.698021	140931.752035	35.667124
1254.021864	141135.209927	35.672141
1255.129641	141319.094775	35.677159
1256.256004	141526.912883	35.682176
1257.534153	141733.616677	35.687194
1259.188586	141929.474890	35.692212
1260.185110	142147.062839	35.697229
1261.097945	142336.718507	35.702247
1262.754907	142543.074522	35.707264
1263.687179	142758.847677	35.712282
1265.060788	142955.870793	35.717300
1266.405964	143188.270518	35.722317
1267.563079	143391.954254	35.727335
1269.034899	143599.993569	35.732352
1269.714573	143815.062049	35.737370
1271.461281	144043.874612	35.742388
1272.509222	144257.732394	35.747405
1273.838863	144467.536352	35.752423
1274.504263	144697.853804	35.757440
1276.167286	144927.191160	35.762458
1277.380571	145141.293333	35.767476
1278.691274	145382.593048	35.772493
1279.684838	145599.016121	35.777511
1281.151525	145818.818333	35.782528
1282.687585	146056.519437	35.787546
1284.232360	146280.690241	35.792564
1285.633075	146512.893472	35.797581
1286.887480	146731.374724	35.802599
1288.516953	146975.119732	35.807616
1289.509605	147199.076318	35.812634
1290.529099	147424.870093	35.817652
1292.384007	147648.972872	35.822669
1293.667202	147872.366460	35.827687
1294.843588	148095.104997	35.832704
1295.651089	148327.980328	35.837722
1297.490466	148562.599092	35.842740
1298.744110	148790.519853	35.847757
1300.214504	149020.870104	35.852775
1301.429587	149240.751464	35.857792
1302.698032	149480.007747	35.862810
1303.846657	149710.627112	35.867828
1305.212843	149941.632285	35.872845
1306.907419	150169.121777	35.877863
1308.163571	150397.328211	35.882880
1309.409143	150643.269908	35.887898
1310.968818	150865.655304	35.892916
1312.243442	151088.390866	35.897933
1313.543343	151323.854993	35.902951
1314.473840	151553.640446	35.907968
1315.908349	151791.903476	35.912986
1317.472583	152020.779274	35.918004
1318.716567	152249.376106	35.923021
1319.936714	152484.781484	35.928039
1321.008522	152714.765407	35.933056
1322.531223	152951.052034	35.938074
1323.844235	153187.562885	35.943092
1324.984383	153424.660321	35.948109
1326.052893	153658.291786	35.953127
1327.929152	153903.704858	35.958144
1329.048332	154140.618146	35.963162
1330.166198	154371.134730	35.968180
1331.429190	154607.951271	35.973197
1333.375728	154852.367247	35.978215
1334.511620	155089.929236	35.983232
1335.788338	155323.890322	35.988250
1336.819948	155546.668791	35.993268
1338.191446	155787.370365	35.998285
1339.339839	156010.754352	36.003303
1341.037794	156239.461077	36.008320
1342.277518	156470.893604	36.013338
1343.683723	156678.422191	36.018356
1345.304594	156905.569410	36.023373
1346.337878	157129.419952	36.028391
1347.301345	157366.370670	36.033408
1348.876595	157579.372809	36.038426
1350.137395	157820.417319	36.043444
1351.328054	158054.986616	36.048461
1352.659918	158286.944924	36.053479
1354.182594	158532.013693	36.058496
1355.101404	158774.004175	36.063514
1356.755461	159009.888384	36.068532
1358.107357	159251.368625	36.073549
1359.472886	159488.848653	36.078567
1361.206248	159735.374591	36.083584
1362.287294	159987.437248	36.088602
1363.823235	160225.515490	36.093620
1364.903898	160459.006648	36.098637
1366.082089	160711.399790	36.103655
1367.888054	160957.919174	36.108672
1368.783842	161211.666163	36.113690
1370.604261	161455.163648	36.118708
1371.707730	161717.602096	36.123725
1373.091960	161966.540109	36.128743
1374.688962	162218.721312	36.133760
1375.689426	162474.132763	36.138778
1377.193089	162727.498581	36.143796
1379.024604	162987.289032	36.148813
1380.513725	163250.854053	36.153831
1381.866119	163499.460123	36.158848
1383.116136	163767.724110	36.163866
1384.783215	164015.546486	36.168884
1386.011100	164268.275804	36.173901
1387.020424	164527.197994	36.178919
1388.884601	164783.435411	36.183936
1390.458523	165036.862544	36.188954
1391.660271	165294.157815	36.193972
1393.219495	165552.921686	36.198989
1394.090350	165807.731389	36.204007
1396.055535	166056.276387	36.209024
1397.103259	166327.210397	36.214042
1399.071740	166583.006559	36.219060
1400.400699	166836.580261	36.224077
1401.445972	167103.861024	36.229095
1403.354002	167345.893440	36.234112
1404.329358	167614.405984	36.239130
1405.840521	167868.767493	36.244148
1407.235716	168122.157702	36.249165
1408.592433	168386.220322	36.254183
1410.117856	168639.693557	36.259200
1411.736282	168908.694380	36.264218
1413.188320	169156.568799	36.269236
1414.765607	169410.163588	36.274253
1415.689780	169671.809955	36.279271
1417.718116	169927.583351	36.284288
1419.092326	170186.964481	36.289306
1420.674661	170440.904865	36.294324
1421.913448	170700.766094	36.299341
1423.080442	170945.770743	36.304359
1424.675378	171198.695935	36.309376
1425.978334	171467.209466	36.314394
1427.397939	171722.487504	36.319412
1428.872497	171965.199844	36.324429
1430.113853	172232.100418	36.329447
1431.926877	172478.735778	36.334464
1432.952455	172727.666492	36.339482
1434.214673	172967.113810	36.344500
1435.889940	173207.716205	36.349517
1437.290450	173459.142833	36.354535
1438.819998	173693.242820	36.359552
1440.036569	173941.385623	36.364570
1441.402503	174180.210897	36.369588
1443.004925	174430.986805	36.374605
1444.108098	174679.467102	36.379623
1445.487035	174927.232002	36.384640
1446.662797	175188.184736	36.389658
1448.381612	175446.577163	36.394676
1449.958526	175698.541918	36.399693
1451.197510	175969.201387	36.404711
1452.944894	176218.779174	36.409728
1454.373774	176480.496382	36.414746
1455.530078	176743.450720	36.419764
1456.998194	177008.998349	36.424781
1458.346625	177261.994069	36.429799
1460.093402	177535.753732	36.434816
1461.578710	177800.158278	36.439834
1463.047234	178073.607653	36.444852
1464.521761	178337.228222	36.449869
1465.925575	178598.016160	36.454887
1467.312515	178867.595014	36.459904
1468.701951	179145.987226	36.464922
1470.331057	179411.517041	36.469940
1471.938479	179684.695727	36.474957
1473.257099	179969.120836	36.479975
1475.006850	180240.247120	36.484992
1476.218190	180519.179434	36.490010
1478.036772	180794.842817	36.495028
1479.578383	181066.689882	36.500045
1480.897403	181339.664705	36.505063
1482.491913	181619.480113	36.510080
1483.440872	181892.616068	36.515098
1485.401492	182178.979386	36.520116
1486.947454	182447.426414	36.525133
1488.322954	182747.547358	36.530151
1490.017434	183017.090273	36.535168
1491.440807	183290.867144	36.540186
1492.947046	183572.530804	36.545204
1494.811383	183849.211871	36.550221
1495.922558	184140.946104	36.555239
1497.790690	184406.655847	36.560256
1499.347544	184694.893099	36.565274
1500.965479	184956.198641	36.570292
1502.537692	185299.500332	36.575309
1504.001574	185605.330917	36.580327
1505.930011	185875.530733	36.585344
1507.141464	186143.481334	36.590362
1508.618519	186420.890426	36.595380
1510.059296	186686.876173	36.600397
1511.705932	186966.800107	36.605415
1513.023924	187239.740528	36.610432
1514.826201	187516.034800	36.615450
1516.405227	187793.837904	36.620468
1518.312375	188068.974185	36.625485
1519.394190	188347.364511	36.630503
1520.887742	188615.683533	36.635520
1522.569567	188884.456335	36.640538
1523.736490	189163.724382	36.645556
1525.328311	189436.779796	36.650573
1526.557619	189722.719679	36.655591
1528.648110	189998.035202	36.660608
1530.130829	190266.639229	36.665626
1531.814491	190556.472506	36.670644
1533.047261	190813.178749	36.675661
1534.439570	191079.995358	36.680679
1535.985563	191338.050736	36.685696
1537.694543	191601.059670	36.690714
1539.120220	191856.366327	36.695732
1540.587519	192108.593523	36.700749
1542.161626	192376.451364	36.705767
1543.651308	192639.547650	36.710784
1545.074271	192893.053420	36.715802
1546.279585	193157.033525	36.720820
1548.501699	193429.389755	36.725837
1549.435090	193702.532482	36.730855
1550.927325	193969.263464	36.735872
1552.448407	194247.700380	36.740890
1553.926964	194517.279542	36.745908
1555.480339	194797.109626	36.750925
1556.992350	195084.287731	36.755943
1558.510035	195352.821001	36.760960
1559.728679	195636.007380	36.765978
1561.591423	195929.787528	36.770996
1563.080688	196213.008939	36.776013
1564.406137	196511.472065	36.781031
1566.341954	196790.204883	36.786048
1568.396789	197081.315605	36.791066
1569.473642	197373.291219	36.796084
1571.270076	197658.982180	36.801101
1572.398212	197958.749257	36.806119
1574.301294	198254.001139	36.811136
1575.900177	198546.176777	36.816154
1577.553669	198839.487514	36.821172
1579.087008	199132.233368	36.826189
1581.092149	199431.662867	36.831207
1582.570494	199721.116166	36.836224
1584.193169	200013.697261	36.841242
1585.733594	200313.074133	36.846260
1587.797849	200608.635450	36.851277
1588.745735	200902.797072	36.856295
1590.450412	201205.604558	36.861312
1592.125233	201501.787250	36.866330
1593.323189	201805.716601	36.871348
1594.655837	202107.491600	36.876365
1596.857130	202409.334391	36.881383
1598.551623	202705.947885	36.886400
1600.204285	203014.278986	36.891418
1602.014217	203321.874721	36.896436
1603.627222	203613.040881	36.901453
1604.743390	203922.956207	36.906471
1606.899874	204226.739589	36.911488
1608.622240	204538.059795	36.916506
1610.007202	204838.891141	36.921524
1611.907911	205131.945169	36.926541
1613.329000	205440.316400	36.931559
1615.160717	205739.097742	36.936576
1617.033709	206037.263381	36.941594
1618.528853	206337.698632	36.946612
1620.361752	206636.379442	36.951629
1621.859507	206928.203483	36.956647
1623.239036	207226.752821	36.961664
1624.912564	207529.168620	36.966682
1626.509157	207832.460565	36.971700
1628.059949	208127.377024	36.976717
1629.607913	208437.028150	36.981735
1631.310597	208731.261097	36.986752
1632.796141	209042.955018	36.991770
1634.313225	209348.496791	36.996788
1635.899480	209652.376888	37.001805
1637.557860	209957.744849	37.006823
1639.197537	210265.631023	37.011840
1640.641290	210564.911046	37.016858
1642.187484	210866.690301	37.021876
1644.414321	211147.507112	37.026893
1645.687780	211444.731633	37.031911
1647.351843	211737.627534	37.036928
1648.972857	212015.770999	37.041946
1650.471208	212311.640197	37.046964
1652.366024	212601.401573	37.051981
1654.013492	212901.744418	37.056999
1654.984593	213193.352922	37.062016
1657.032987	213501.127635	37.067034
1658.308531	213798.252411	37.072052
1660.298114	214099.558916	37.077069
1661.781087	214400.513089	37.082087
1663.395737	214712.776965	37.087104
1665.093071	215016.213049	37.092122
1666.673612	215344.588751	37.097140
1668.459863	215650.475563	37.102157
1669.972521	215964.204385	37.107175
1671.482003	216285.605886	37.112192
1673.449381	216593.675146	37.117210
1675.024837	216922.027422	37.122228
1676.844320	217234.921571	37.127245
1678.328648	217556.734325	37.132263
1680.021776	217891.724636	37.137280
1681.807103	218207.927216	37.142298
1683.358184	218533.439067	37.147316
1685.375503	218856.159908	37.152333
1687.432176	219195.082488	37.157351
1688.700535	219512.636834	37.162368
1691.004361	219835.541947	37.167386
1692.282957	220171.055604	37.172404
1693.884152	220485.357371	37.177421
1695.709188	220809.963664	37.182439
1697.489242	221146.948876	37.187456
1699.319059	221471.986517	37.192474
1700.569670	221810.985508	37.197492
1702.582505	222134.445053	37.202509
1704.126647	222472.483745	37.207527
1706.168288	222800.511672	37.212544
1708.179166	223128.442861	37.217562
1709.583854	223462.591354	37.222580
1711.157795	223796.789623	37.227597
1712.964983	224125.540361	37.232615
1714.377957	224457.426716	37.237632
1716.504541	224788.312277	37.242650
1718.084599	225137.574320	37.247668
1719.986782	225470.120877	37.252685
1721.872665	225812.450554	37.257703
1723.385394	226149.402136	37.262720
1725.297353	226479.330501	37.267738
1726.929388	226833.055454	37.272756
1729.030899	227171.693082	37.277773
1730.668556	227498.285504	37.282791
1731.848795	227848.676847	37.287808
1733.841993	228173.308197	37.292826
1735.638493	228522.180318	37.297844
1737.592126	228866.505833	37.302861
1739.329302	229196.511834	37.307879
1740.492643	229543.297978	37.312896
1742.680858	229876.205445	37.317914
1744.176004	230222.812390	37.322932
1745.922513	230566.204356	37.327949
1747.669585	230909.367445	37.332967
1749.586700	231252.808610	37.337984
1751.392835	231592.227739	37.343002
1752.897072	231929.432983	37.348020
1754.428660	232273.645247	37.353037
1756.388713	232612.023570	37.358055
1758.130002	232937.632354	37.363072
1760.202956	233256.914277	37.368090
1761.874390	233591.602773	37.373108
1763.802035	233900.923304	37.378125
1765.321477	234222.171104	37.383143
1766.789459	234559.227907	37.388160
1768.845435	234880.315065	37.393178
1770.496139	235198.823406	37.398196
1772.273455	235522.112999	37.403213
1774.033000	235843.880887	37.408231
1775.745541	236181.609398	37.413248
1777.266451	236518.681692	37.418266
1778.792260	236857.200916	37.423284
1780.932664	237196.512769	37.428301
1782.870335	237540.987542	37.433319
1784.109292	237875.638492	37.438336
1786.220493	238223.438670	37.443354
1788.072398	238572.168164	37.448372
1789.530233	238912.651980	37.453389
1791.075310	239261.606520	37.458407
1793.315053	239625.592396	37.463424
1794.820169	239963.933699	37.468442
1796.820679	240324.552049	37.473460
1798.561522	240685.083537	37.478477
1800.692136	241035.824072	37.483495
1802.027053	241406.198365	37.488512
1803.923010	241764.671816	37.493530
1805.619400	242133.997742	37.498548
1807.458020	242491.158136	37.503565
1809.205870	242863.345445	37.508583
1811.382603	243232.569094	37.513600
1813.042379	243594.150512	37.518618
1814.769358	243967.202986	37.523636
1816.775921	244340.338088	37.528653
1818.586694	244711.140707	37.533671
1820.757904	245092.072821	37.538688
1822.711390	245444.206097	37.543706
1824.423717	245821.296623	37.548724
1826.230370	246191.436729	37.553741
1828.268468	246567.788977	37.558759
1829.735449	246941.587980	37.563776
1831.844203	247307.029981	37.568794
1833.574888	247686.425604	37.573812
1835.393798	248061.157980	37.578829
1837.581852	248431.259374	37.583847
1839.388773	248802.435725	37.588864
1841.746287	249168.597078	37.593882
1843.373543	249550.494305	37.598900
1844.941549	249924.906287	37.603917
1847.067698	250301.668693	37.608935
1848.906023	250674.969780	37.613952
1850.775408	251037.545485	37.618970
1852.580732	251402.264151	37.623988
1854.372143	251788.372547	37.629005
1856.433289	252154.675137	37.634023
1858.031758	252530.981337	37.639040
1859.907108	252899.521146	37.644058
1861.872609	253278.130385	37.649076
1863.687713	253641.648232	37.654093
1865.839816	254014.002962	37.659111
1867.458012	254404.983319	37.664128
1869.101048	254779.981231	37.669146
1870.992832	255156.031461	37.674164
1872.898894	255534.643948	37.679181
1874.930388	255905.869406	37.684199
1876.968327	256292.739900	37.689216
1878.779808	256662.956219	37.694234
1880.400080	257024.996895	37.699252
1882.337813	257389.679372	37.704269
1884.432182	257741.991499	37.709287
1886.020247	258100.782849	37.714304
1887.696429	258463.801288	37.719322
1889.692730	258811.223405	37.724340
1891.081706	259174.183074	37.729357
1893.063545	259532.044998	37.734375
1895.070976	259906.970885	37.739392
1897.031593	260269.380568	37.744410
1898.827761	260636.107491	37.749428
1899.800422	261019.853183	37.754445
1902.310266	261395.076652	37.759463
1903.682307	261775.277498	37.764480
1905.744108	262166.900662	37.769498
1907.865793	262559.249663	37.774516
1909.986718	262938.922938	37.779533
1911.622566	263336.450495	37.784551
1913.690661	263725.603312	37.789568
1915.794959	264107.586407	37.794586
1917.604635	264501.221698	37.799604
1919.579529	264893.432691	37.804621
1921.723000	265289.171691	37.809639
1923.248039	265684.472542	37.814656
1925.191366	266081.662114	37.819674
1926.897022	266481.909756	37.824692
1928.946585	266883.879880	37.829709
1931.167273	267288.183652	37.834727
1933.041073	267687.739704	37.839744
1934.893608	268100.072813	37.844762
1936.896316	268505.269125	37.849780
1939.082743	268919.146524	37.854797
1941.112882	269315.344100	37.859815
1942.963832	269734.908734	37.864832
1944.973050	270144.541533	37.869850
1946.959038	270549.731523	37.874868
1949.148695	270965.605612	37.879885
1951.325856	271373.708092	37.884903
1953.195589	271777.945598	37.889920
1954.884506	272192.800187	37.894938
1957.178137	272601.716842	37.899956
1958.879161	273012.730644	37.904973
1961.220717	273417.013664	37.909991
1963.041041	273838.671504	37.915008
1964.860545	274239.121169	37.920026
1967.503147	274658.995438	37.925044
1969.207428	275067.586017	37.930061
1971.016483	275469.631328	37.935079
1973.074019	275893.400255	37.940096
1975.129698	276298.907526	37.945114
1977.148312	276715.541930	37.950132
1978.835878	277135.298827	37.955149
1981.047127	277553.270043	37.960167
1982.926283	277968.675250	37.965184
1985.232898	278386.906414	37.970202
1987.338309	278797.319672	37.975220
1988.961424	279219.640272	37.980237
1991.313663	279635.317945	37.985255
1993.249328	280047.198491	37.990272
1994.905404	280462.015492	37.995290
1997.402956	280866.667689	38.000308
1999.127424	281284.719851	38.005325
2001.259030	281700.090313	38.010343
2003.665806	282125.801499	38.015360
2005.315088	282530.221625	38.020378
2007.455003	282935.603837	38.025396
2009.351069	283356.638945	38.030413
2011.382728	283766.985066	38.035431
2013.020361	284165.480963	38.040448
2015.088057	284570.357144	38.045466
2017.269065	284949.083803	38.050484
2018.892442	285357.630663	38.055501
2020.995884	285749.467727	38.060519
2023.030629	286143.979483	38.065536
2024.760245	286546.205168	38.070554
2026.969424	286938.805900	38.075572
2028.522991	287346.767538	38.080589
2030.655033	287747.729527	38.085607
2032.729614	288172.515546	38.090624
2034.580628	288570.596379	38.095642
2036.462175	288976.338201	38.100660
2038.510761	289413.511147	38.105677
2040.773765	289826.678314	38.110695
2042.762710	290240.672779	38.115712
2044.595995	290663.626429	38.120730
2046.610477	291076.316441	38.125748
2048.800519	291506.444871	38.130765
2050.730745	291937.398045	38.135783
2052.736035	292370.342258	38.140800
2054.556540	292802.652162	38.145818
2056.936874	293232.154682	38.150836
2058.764553	293683.474044	38.155853
2060.935507	294121.838494	38.160871
2063.361497	294561.302312	38.165888
2065.130181	295014.524953	38.170906
2067.698439	295448.247351	38.175924
2069.834253	295903.538300	38.180941
2072.170780	296331.628686	38.185959
2073.761619	296778.213599	38.190976
2075.409221	297224.075272	38.195994
2078.051922	297678.587316	38.201012
2080.089211	298136.313083	38.206029
2082.313971	298579.077999	38.211047
2084.376781	299032.958925	38.216064
2086.448078	299478.558646	38.221082
2088.686305	299936.466603	38.226100
2090.621937	300380.836261	38.231117
2092.701065	300842.467927	38.236135
2095.029662	301301.721093	38.241152
2096.844549	301753.079523	38.246170
2099.510102	302210.495153	38.251188
2101.322835	302672.305017	38.256205
2103.126786	303121.470358	38.261223
2105.829924	303578.233601	38.266240
2107.842684	304045.051687	38.271258
2110.130894	304501.643258	38.276276
2112.108289	304962.366284	38.281293
2114.588129	305424.326528	38.286311
2116.521651	305874.361470	38.291328
2118.610559	306333.912354	38.296346
2121.112380	306786.236313	38.301364
2123.034524	307247.937121	38.306381
2125.185054	307702.389152	38.311399
2127.158935	308160.113632	38.316416
2129.335891	308620.594157	38.321434
2131.348700	309078.354743	38.326452
2133.870453	309540.879362	38.331469
2136.074426	310001.088771	38.336487
2138.388551	310460.616624	38.341504
2140.243513	310923.511464	38.346522
2142.150242	311371.088942	38.351540
2144.504716	311842.145513	38.356557
2146.229518	312284.108264	38.361575
2148.269903	312755.839323	38.366592
2150.537382	313220.804369	38.371610
2153.047861	313683.087236	38.376628
2155.505452	314137.100014	38.381645
2157.182461	314572.424365	38.386663
2159.719933	315008.142909	38.391680
2161.574383	315440.969427	38.396698
2163.791199	315865.385563	38.401716
2165.748552	316312.957936	38.406733
2167.392798	316742.251855	38.411751
2170.174464	317181.819357	38.416768
2171.580555	317621.927609	38.421786
2173.981802	318077.178303	38.426804
2175.872865	318534.788025	38.431821
2178.008561	318986.492649	38.436839
2179.942222	319445.025091	38.441856
2182.005389	319908.303147	38.446874
2184.605726	320363.397248	38.451892
2186.462449	320838.472013	38.456909
2188.277700	321311.797071	38.461927
2190.660089	321784.038494	38.466944
2192.738079	322265.482569	38.471962
2194.950519	322749.158426	38.476980
2197.102685	323232.381378	38.481997
2199.087602	323720.268313	38.487015
2201.488652	324210.824748	38.492032
2203.401942	324704.141218	38.497050
2205.610884	325198.978624	38.502068
2208.115825	325700.715842	38.507085
2210.253382	326194.892605	38.512103
2212.875977	326688.023297	38.517120
2214.699723	327193.781193	38.522138
2217.280926	327694.162302	38.527156
2219.453266	328208.073148	38.532173
2221.732785	328714.374683	38.537191
2224.126710	329214.182335	38.542208
2226.340366	329715.686242	38.547226
2228.897083	330228.191275	38.552244
2230.990111	330738.428084	38.557261
2233.368088	331249.628339	38.562279
2235.639831	331753.684405	38.567296
2238.026297	332263.170104	38.572314
2240.325488	332763.479365	38.577332
2242.153721	333272.100231	38.582349
2244.946244	333789.594202	38.587367
2247.067681	334300.920339	38.592384
2249.405804	334810.100136	38.597402
2252.105257	335308.968397	38.602420
2253.992601	335829.797162	38.607437
2256.214955	336341.054013	38.612455
2258.925500	336848.219634	38.617472
2261.192204	337374.699671	38.622490
2263.498714	337878.718146	38.627508
2266.278380	338382.376567	38.632525
2268.341522	338890.147527	38.637543
2270.585727	339380.559643	38.642560
2272.953067	339889.460907	38.647578
2275.013774	340392.315759	38.652596
2277.669181	340892.255190	38.657613
2279.888387	341403.491181	38.662631
2282.399447	341905.061948	38.667648
2284.260431	342417.429707	38.672666
2287.059714	342918.408194	38.677684
2289.446550	343417.313647	38.682701
2291.701574	343927.289578	38.687719
2293.918571	344419.080813	38.692736
2295.747045	344920.587732	38.697754
2298.271890	345426.187944	38.702772
2300.439343	345924.659973	38.707789
2302.812151	346426.034085	38.712807
2305.396077	346927.012671	38.717824
2307.502290	347420.958334	38.722842
2309.531466	347896.423252	38.727860
2311.885401	348376.952654	38.732877
2313.907626	348861.229014	38.737895
2316.367710	349331.610628	38.742912
2318.570132	349815.109405	38.747930
2320.628693	350295.225897	38.752948
2323.059741	350787.092498	38.757965
2324.977379	351269.676064	38.762983
2327.183808	351754.463773	38.768000
2329.160417	352261.971877	38.773018
2331.698596	352765.226117	38.778036
2333.868561	353271.192089	38.783053
2336.439811	353778.532334	38.788071
2338.692672	354293.190354	38.793088
2341.055093	354808.152405	38.798106
2343.522796	355307.320926	38.803124
2345.371380	355825.490211	38.808141
2347.566084	356352.849709	38.813159
2350.087019	356879.439403	38.818176
2352.588233	357407.899084	38.823194
2354.646563	357928.662072	38.828212
2356.836959	358479.586066	38.833229
2359.025235	359017.065785	38.838247
2362.123454	359545.648609	38.843264
2364.039893	360089.919745	38.848282
2366.798484	360634.987163	38.853300
2369.315106	361182.008874	38.858317
2371.235922	361722.016856	38.863335
2373.892786	362267.805455	38.868352
2376.223472	362823.823802	38.873370
2378.827475	363378.977899	38.878388
2381.415594	363937.849606	38.883405
2383.632253	364494.487819	38.888423
2386.563718	365034.581155	38.893440
2388.435819	365585.854284	38.898458
2391.229034	366135.579007	38.903476
2393.639611	366694.577530	38.908493
2395.830324	367253.650247	38.913511
2398.544390	367804.799853	38.918528
2401.060443	368363.394494	38.923546
2403.553373	368913.340866	38.928564
2406.064909	369475.056433	38.933581
2408.464773	370038.146561	38.938599
2410.998058	370578.146615	38.943616
2413.312637	371146.168777	38.948634
2415.952126	371693.782642	38.953652
2418.622380	372250.502142	38.958669
2420.595502	372806.914084	38.963687
2423.210089	373366.026714	38.968704
2425.416552	373915.564365	38.973722
2428.020504	374475.314706	38.978740
2430.730079	375035.138344	38.983757
2432.988300	375605.154510	38.988775
2435.671155	376152.773670	38.993792
2438.120779	376717.593724	38.998810
2440.531548	377269.285895	39.003828
2443.334694	377829.366056	39.008845
2445.633080	378389.513374	39.013863
2448.208875	378928.251795	39.018880
2450.570850	379486.896756	39.023898
2453.103373	380041.323811	39.028916
2455.768820	380590.601895	39.033933
2458.081378	381144.381429	39.038951
2460.550164	381689.690553	39.043968
2463.227784	382242.553755	39.048986
2465.405875	382790.975086	39.054004
2467.862995	383338.176085	39.059021
2470.290645	383884.635576	39.064039
2473.052476	384405.326022	39.069056
2475.136714	384936.469618	39.074074
2477.506286	385458.136883	39.079092
2480.248440	385978.570232	39.084109
2482.356337	386498.940111	39.089127
2485.017954	387027.315849	39.094144
2487.552590	387553.395999	39.099162
2489.695501	388081.855922	39.104180
2491.943999	388599.248159	39.109197
2494.322497	389138.156996	39.114215
2497.069052	389684.946972	39.119232
2499.499950	390230.913335	39.124250
2501.635236	390769.723270	39.129268
2504.183208	391312.912810	39.134285
2506.559504	391875.611700	39.139303
2509.004127	392426.438504	39.144320
2511.876237	392981.540363	39.149338
2514.070083	393540.381044	39.154356
2516.715669	394101.770892	39.159373
2518.919949	394673.646289	39.164391
2522.109008	395238.721690	39.169408
2524.218256	395816.305569	39.174426
2526.641056	396374.892328	39.179444
2529.224538	396949.995010	39.184461
2531.470362	397536.982338	39.189479
2534.042080	398111.501642	39.194496
2536.669297	398712.827193	39.199514
2539.089628	399301.818469	39.204532
2541.739193	399891.518256	39.209549
2544.193616	400485.232303	39.214567
2547.233516	401070.589182	39.219584
2550.076241	401667.502082	39.224602
2552.438878	402263.968416	39.229620
2555.177326	402852.161328	39.234637
2557.999233	403449.385263	39.239655
2560.461781	404043.764988	39.244672
2563.379523	404633.148969	39.249690
2565.678012	405244.779992	39.254708
2568.212297	405837.987897	39.259725
2570.739906	406440.289801	39.264743
2573.709083	407032.841366	39.269760
2576.722299	407624.054644	39.274778
2579.266880	408235.109895	39.279796
2581.668154	408832.205582	39.284813
2584.188142	409439.740064	39.289831
2586.524776	410025.024441	39.294848
2589.596686	410622.320750	39.299866
2591.926606	411228.975213	39.304884
2594.610720	411833.483119	39.309901
2597.179549	412429.493108	39.314919
2599.908407	413032.189890	39.319936
2602.493099	413626.090211	39.324954
2605.209752	414243.829869	39.329972
2607.327621	414838.275469	39.334989
2610.451293	415442.815492	39.340007
2613.317984	416044.090728	39.345024
2615.889200	416650.604839	39.350042
2618.223278	417249.653018	39.355060
2620.997493	417845.479544	39.360077
2623.808231	418452.410059	39.365095
2626.387983	419049.092556	39.370112
2629.065631	419655.452612	39.375130
2631.662612	420259.430755	39.380148
2634.448432	420850.668771	39.385165
2636.683781	421449.207216	39.390183
2639.406713	422054.579654	39.395200
2641.932173	422658.903254	39.400218
2644.579461	423251.054652	39.405236
2647.223608	423830.498209	39.410253
2649.937283	424406.172878	39.415271
2652.524891	424970.576154	39.420288
2655.006531	425538.974340	39.425306
2657.377817	426112.328314	39.430324
2659.650849	426701.100636	39.435341
2662.313327	427287.671502	39.440359
2665.152092	427871.063345	39.445376
2667.654671	428455.147843	39.450394
2670.271671	429056.636753	39.455412
2672.857684	429639.561247	39.460429
2675.760168	430246.681205	39.465447
2678.045158	430836.289491	39.470464
2680.266570	431460.360387	39.475482
2682.789788	432072.082620	39.480500
2685.594670	432692.687177	39.485517
2688.657733	433313.686399	39.490535
2691.145381	433926.568794	39.495552
2693.780497	434558.409856	39.500570
2696.062525	435186.495428	39.505588
2699.164541	435823.578463	39.510605
2701.662086	436462.048621	39.515623
2704.375043	437097.179408	39.520640
2707.243601	437752.374241	39.525658
2709.627615	438408.329581	39.530676
2712.524087	439043.417058	39.535693
2715.311466	439699.971785	39.540711
2718.079603	440357.820102	39.545728
2720.773018	441009.999022	39.550746
2723.587717	441675.472437	39.555764
2726.390817	442335.619899	39.560781
2729.080101	443001.520102	39.565799
2732.123678	443669.058299	39.570816
2735.196323	444332.325062	39.575834
2737.872126	445002.044345	39.580852
2740.995877	445649.143840	39.585869
2743.935991	446315.036375	39.590887
2746.542565	446980.401222	39.595904
2749.795427	447640.136174	39.600922
2752.578827	448300.627478	39.605940
2755.415707	448953.107902	39.610957
2758.402588	449607.459993	39.615975
2760.995637	450267.353472	39.620992
2764.189954	450923.291317	39.626010
2766.475160	451581.568710	39.631028
2769.308122	452235.394232	39.636045
2772.103007	452899.550983	39.641063
2775.109744	453551.180382	39.646080
2778.249243	454206.248121	39.651098
2780.809261	454867.742437	39.656116
2783.433969	455523.093926	39.661133
2786.384121	456186.799322	39.666151
2789.505890	456848.231764	39.671168
2792.265779	457504.093274	39.676186
2795.042121	458167.901568	39.681204
2797.769865	458808.426358	39.686221
2800.682547	459465.148383	39.691239
2803.520813	460135.482154	39.696256
2806.212104	460792.793511	39.701274
2808.989400	461457.736012	39.706292
2811.619011	462098.052155	39.711309
2814.435890	462762.937405	39.716327
2817.309069	463428.948171	39.721344
2820.090577	464085.815170	39.726362
2822.575559	464758.947816	39.731380
2825.602037	465411.840015	39.736397
2828.510396	466075.520666	39.741415
2831.139452	466739.218593	39.746432
2833.876352	467368.622999	39.751450
2836.430295	468003.126601	39.756468
2839.089008	468645.054353	39.761485
2841.592865	469276.641908	39.766503
2844.200798	469923.117523	39.771520
2846.905430	470561.937265	39.776538
2849.529168	471217.739765	39.781556
2852.257331	471868.658468	39.786573
2855.371492	472527.659843	39.791591
2857.761011	473191.437237	39.796608
2860.850959	473852.203822	39.801626
2863.229266	474539.424340	39.806644
2866.310735	475216.472408	39.811661
2869.123702	475897.869662	39.816679
2871.774246	476582.288127	39.821696
2874.876153	477272.555216	39.826714
2877.915635	477956.753019	39.831732
2880.561597	478651.467535	39.836749
2883.224396	479355.977868	39.841767
2885.899516	480058.489128	39.846784
2889.246392	480759.150373	39.851802
2891.897483	481472.589438	39.856820
2895.039674	482187.128676	39.861837
2897.705144	482914.509655	39.866855
2900.457022	483633.175859	39.871872
2903.922920	484344.541916	39.876890
2906.484335	485092.849101	39.881908
2909.835195	485818.424558	39.886925
2912.254767	486542.499192	39.891943
2914.814049	487284.906169	39.896960
2917.874290	488024.428045	39.901978
2920.511079	488771.687508	39.906996
2923.731962	489530.354011	39.912013
2927.131601	490273.591976	39.917031
2930.107815	491029.703089	39.922048
2932.589330	491776.284417	39.927066
2935.924987	492541.933218	39.932084
2938.975213	493297.012103	39.937101
2942.281737	494054.329121	39.942119
2944.705998	494810.738491	39.947136
2948.314175	495556.098643	39.952154
2951.204908	496311.150067	39.957172
2954.374609	497076.943680	39.962189
2957.543807	497843.855416	39.967207
2960.410576	498599.397291	39.972224
2963.592237	499342.467654	39.977242
2966.476852	500117.207841	39.982260
2969.249060	500875.515746	39.987277
2972.425189	501628.234818	39.992295
2975.420288	502394.128918	39.997312
2978.985387	503157.427274	40.002330
2981.721150	503915.228982	40.007348
2984.705079	504663.843936	40.012365
2987.786503	505425.939784	40.017383
2990.713181	506186.811541	40.022400
2994.202801	506934.976586	40.027418
2996.974636	507689.704265	40.032436
2999.594760	508441.447293	40.037453
3003.259669	509197.111784	40.042471
3005.998771	509959.419557	40.047488
3009.073958	510703.475610	40.052506
3012.333574	511464.312289	40.057524
3015.419688	512217.992973	40.062541
3018.233744	512960.158873	40.067559
3021.387924	513717.720433	40.072576
3024.673681	514453.647730	40.077594
3027.504673	515208.261528	40.082612
3030.655101	515944.130331	40.087629
3033.872784	516648.073669	40.092647
3036.348878	517365.067486	40.097664
3038.912678	518057.829292	40.102682
3041.873815	518774.069888	40.107700
3045.056620	519489.986707	40.112717
3048.036941	520214.090312	40.117735
3050.560777	520925.460192	40.122752
3053.840669	521654.214447	40.127770
3056.608111	522384.014418	40.132788
3059.228149	523118.621973	40.137805
3062.887916	523859.207345	40.142823
3065.014991	524611.497835	40.147840
3068.248197	525355.985935	40.152858
3071.485640	526114.700167	40.157876
3074.403487	526875.179207	40.162893
3077.679808	527626.716883	40.167911
3080.389772	528404.471477	40.172928
3083.392691	529171.435236	40.177946
3086.807403	529944.467571	40.182964
3089.596297	530730.559950	40.187981
3092.583344	531506.127962	40.192999
3095.299695	532301.979957	40.198016
3098.314101	533095.125281	40.203034
3101.817664	533895.175026	40.208052
3104.548968	534692.684973	40.213069
3107.962392	535500.381042	40.218087
3110.895923	536312.368385	40.223104
3114.377054	537130.844743	40.228122
3117.699598	537939.103580	40.233140
3120.612185	538759.421275	40.238157
3123.918646	539570.540023	40.243175
3126.674954	540397.802403	40.248192
3129.345691	541221.661611	40.253210
3132.830777	542057.282154	40.258228
3136.358908	542886.016295	40.263245
3139.968094	543722.208678	40.268263
3142.757111	544555.814199	40.273280
3145.778498	545394.845712	40.278298
3149.414607	546229.711298	40.283316
3152.517493	547068.466086	40.288333
3156.105755	547909.796294	40.293351
3158.420969	548748.710173	40.298368
3162.000385	549592.333703	40.303386
3165.809081	550431.149475	40.308404
3168.557077	551272.028875	40.313421
3172.393389	552104.557520	40.318439
3175.522312	552950.274924	40.323456
3178.827433	553781.768541	40.328474
3182.170260	554624.878724	40.333492
3185.110566	555460.574291	40.338509
3188.676523	556286.991769	40.343527
3191.777408	557119.839881	40.348544
3195.422910	557943.874950	40.353562
3198.514354	558786.280003	40.358580
3201.333102	559608.374541	40.363597
3205.462614	560439.977209	40.368615
3209.053455	561267.847971	40.373632
3212.381457	562086.984795	40.378650
3215.055022	562904.363425	40.383668
3218.311088	563727.654753	40.388685
3222.057730	564538.239755	40.393703
3225.510321	565359.031134	40.398720
3228.001925	566173.905293	40.403738
3231.416556	566983.920833	40.408756
3234.504651	567781.262448	40.413773
3237.898277	568599.630050	40.418791
3241.463141	569418.162963	40.423808
3244.470490	570206.087075	40.428826
3247.943682	570978.716523	40.433844
3250.522093	571760.593562	40.438861
3254.009266	572526.358562	40.443879
3256.883620	573294.670141	40.448896
3260.272562	574062.398787	40.453914
3263.511478	574834.702532	40.458932
3266.484155	575620.555209	40.463949
3269.829194	576388.632755	40.468967
3272.833521	577163.565222	40.473984
3276.077552	577953.915025	40.479002
3279.490015	578740.530863	40.484020
3281.915885	579539.750447	40.489037
3285.861691	580337.224495	40.494055
3288.643904	581136.073435	40.499072
3291.793510	581958.461618	40.504090
3294.869498	582756.897440	40.509108
3298.045927	583585.860776	40.514125
3301.553497	584405.710148	40.519143
3305.005098	585245.454617	40.524160
3307.532071	586073.631374	40.529178
3311.438920	586910.127199	40.534196
3314.823915	587762.584729	40.539213
3318.196252	588604.831575	40.544231
3321.307472	589450.252080	40.549248
3324.459528	590301.946297	40.554266
3327.721185	591155.454758	40.559284
3331.081096	592017.823398	40.564301
3334.410814	592879.827587	40.569319
3338.102176	593757.941016	40.574336
3341.558377	594615.988627	40.579354
3345.055506	595486.247472	40.584372
3348.451867	596358.997722	40.589389
3351.892753	597232.418079	40.594407
3355.320899	598107.965231	40.599424
3358.349343	598984.550564	40.604442
3362.293461	599857.424736	40.609460
3365.329470	600738.255741	40.614477
3369.146852	601610.903504	40.619495
3372.345962	602501.543624	40.624512
3375.761017	603375.354118	40.629530
3379.092508	604273.757002	40.634548
3382.399603	605159.311115	40.639565
3386.046734	606046.083227	40.644583
3388.920383	606935.793539	40.649600
3392.742889	607828.770506	40.654618
3396.634427	608711.731998	40.659636
3399.706248	609606.516679	40.664653
3403.204277	610495.520297	40.669671
3406.752553	611402.491222	40.674688
3409.987648	612284.297633	40.679706
3413.882537	613174.350525	40.684724
3416.865050	614074.339119	40.689741
3420.473648	614963.879703	40.694759
3423.878313	615863.791506	40.699776
3427.029528	616759.973576	40.704794
3430.826924	617669.978919	40.709812
3434.090996	618570.416239	40.714829
3437.800129	619460.586862	40.719847
3440.972421	620364.712535	40.724864
3444.051410	621266.727421	40.729882
3447.929830	622169.431488	40.734900
3451.172505	623081.964954	40.739917
3454.830319	623978.011901	40.744935
3458.222756	624883.679950	40.749952
3461.530526	625791.717283	40.754970
3465.081146	626695.449327	40.759988
3468.525219	627600.059902	40.765005
3472.421181	628492.997051	40.770010
3475.461664	629348.962070	40.775015
3478.561820	630160.727883	40.780020
3482.091752	630919.315770	40.785024
3484.987737	631611.732149	40.790029
3488.175740	632260.347733	40.795034
3490.937485	632859.296981	40.800039
3493.104558	633397.191650	40.805044
3496.172792	633878.098156	40.810048
3498.133324	634308.225078	40.815053
3500.650195	634685.124484	40.820058
3503.457445	635018.021690	40.825063
3504.987912	635300.482931	40.830068
3507.107607	635533.767128	40.835072
3508.667439	635731.373794	40.840077
3510.255890	635866.531211	40.845082
3512.258561	635975.289396	40.850087
3513.464739	636042.477973	40.855092
3514.503748	636080.966116	40.860096
3515.545868	636079.207187	40.865101
3516.606022	636058.843249	40.870106
3517.806365	636006.838467	40.875111
3518.500752	635934.315166	40.880116
3519.664698	635818.976732	40.885120
3519.949560	635698.886695	40.890125
3520.710639	635545.354668	40.895130
3521.253732	635380.083643	40.900135
3521.367729	635203.754401	40.905140
3522.497034	635000.628660	40.910144
3522.720662	634795.295876	40.915149
3523.197523	634573.109641	40.920154
3523.452606	634327.558752	40.925159
3524.082045	634076.007024	40.930164
3524.083884	633805.441336	40.935168
3524.100851	633536.910895	40.940173
3524.184604	633270.956554	40.945178
3524.050536	632981.581531	40.950183
3523.906195	632702.277024	40.955188
3524.425539	632407.344523	40.960192
3524.562668	632110.566773	40.965197
3524.199731	631808.519335	40.970202
3523.980826	631507.288088	40.975207
3524.166237	631209.077804	40.980212
3524.575073	630889.915726	40.985216
3524.048567	630585.110913	40.990221
3524.310021	630263.106743	40.995226
3524.087467	629949.102169	41.000231
3524.087409	629638.695671	41.005236
3523.943249	629311.033880	41.010240
3523.805038	628996.785480	41.015245
3523.669065	628680.679824	41.020250
3523.432886	628365.128528	41.025255
3522.949448	628051.003172	41.030260
3523.085803	627741.812167	41.035264
3522.622222	627436.848174	41.040269
3522.261154	627128.464120	41.045274
3522.517051	626810.588875	41.050279
3522.160667	626505.928316	41.055284
3521.970705	626202.679964	41.060288
3521.533488	625897.363980	41.065293
3521.639188	625594.499788	41.070298
3521.401809	625297.072015	41.075303
3520.905677	624999.625694	41.080308
3520.944959	624698.691319	41.085312
3520.931223	624409.539984	41.090317
3520.426547	624123.952207	41.095322
3520.393469	623835.086521	41.100327
3519.879562	623553.128802	41.105332
3519.774712	623265.555900	41.110336
3519.510407	622998.424745	41.115341
3519.374610	622723.874993	41.120346
3519.199982	622445.827683	41.125351
3518.600395	622179.026315	41.130356
3518.449162	621904.805709	41.135360
3518.362343	621649.247326	41.140365
3517.821057	621385.412112	41.145370
3517.937650	621129.708568	41.150375
3517.504738	620890.867559	41.155380
3517.747858	620627.339003	41.160384
3517.200352	620382.059864	41.165389
3516.992805	620135.822323	41.170394
3516.719990	619891.836840	41.175399
3516.603975	619648.420310	41.180404
3516.253866	619418.522945	41.185408
3515.964775	619177.419952	41.190413
3515.662604	618955.497759	41.195418
3515.469603	618736.900925	41.200423
3515.113319	618510.630642	41.205428
3515.537726	618288.579968	41.210432
3514.906936	618080.729269	41.215437
3514.874921	617847.348236	41.220442
3514.798816	617644.548157	41.225447
3514.651830	617433.410457	41.230452
3514.448484	617230.272067	41.235456
3513.868162	617015.745434	41.240461
3514.008326	616820.240316	41.245466
3513.753226	616612.400203	41.250471
3513.428558	616417.159750	41.255476
3513.444933	616224.011033	41.260480
3513.012691	616034.476910	41.265485
3512.840099	615850.995613	41.270490
3512.849991	615662.084978	41.275495
3512.743029	615481.735170	41.280500
3512.642334	615295.833557	41.285504
3512.429022	615118.742428	41.290509
3512.297992	614936.787252	41.295514
3511.818652	614757.682158	41.300519
3511.573745	614599.279640	41.305524
3511.497818	614425.803474	41.310528
3511.472944	614265.411978	41.315533
3510.911055	614095.205010	41.320538
3510.995477	613932.641803	41.325543
3510.903364	613788.048455	41.330548
3511.059275	613627.368603	41.335552
3510.577363	613475.233749	41.340557
3510.514431	613328.129876	41.345562
3510.488523	613164.571768	41.350567
3510.630070	613019.530960	41.355572
3510.678970	612856.456060	41.360576
3510.047121	612712.731515	41.365581
3510.130107	612570.492912	41.370586
3509.706195	612426.281858	41.375591
3509.614197	612289.315859	41.380596
3509.568310	612128.193758	41.385600
3509.330381	612002.095361	41.390605
3509.262280	611868.819530	41.395610
3509.303398	611752.723436	41.400615
3509.008409	611616.829982	41.405620
3509.676282	611478.534312	41.410624
3508.801869	611345.227651	41.415629
3509.031222	611220.046426	41.420634
3508.768177	611094.440643	41.425639
3508.586603	610962.970607	41.430644
3508.391517	610840.201034	41.435648
3508.122861	610726.691637	41.440653
3507.807604	610613.888275	41.445658
3507.801552	610497.885200	41.450663
3507.716178	610386.943457	41.455668
3507.826389	610277.520022	41.460672
3507.673892	610176.037043	41.465677
3507.608387	610068.989002	41.470682
3507.429515	609954.806897	41.475687
3507.499869	609855.286068	41.480692
3507.650118	609753.051473	41.485696
3507.530301	609642.056989	41.490701
3507.302779	609540.529398	41.495706
3507.575911	609435.121984	41.500711
3507.172465	609333.769857	41.505716
3507.357800	609221.572915	41.510720
3506.932324	609138.975365	41.515725
3506.795064	609032.327721	41.520730
3506.774233	608935.412645	41.525735
3506.566898	608844.126935	41.530740
3506.671020	608735.538074	41.535744
3506.653273	608662.124883	41.540749
3506.309406	608566.407058	41.545754
3506.385334	608470.572698	41.550759
3506.092698	608390.198857	41.555764
3506.378176	608301.982039	41.560768
3506.165045	608220.544168	41.565773
3505.967776	608137.052614	41.570778
3506.373465	608039.662262	41.575783
3506.187812	607959.118267	41.580788
3506.032467	607878.168782	41.585792
3506.137799	607796.827800	41.590797
3505.780825	607707.255851	41.595802
3505.768521	607623.831228	41.600807
3505.622214	607544.878338	41.605812
3505.744614	607463.432009	41.610816
3505.689344	607391.766163	41.615821
3505.702133	607319.238878	41.620826
3505.500103	607238.291636	41.625831
3505.457129	607164.721600	41.630836
3505.344479	607090.011499	41.635840
3505.391102	607027.480588	41.640845
3504.832394	606944.335932	41.645850
3505.335842	606877.431027	41.650855
3505.085471	606809.393030	41.655860
3505.215043	606744.146345	41.660864
3505.266664	606682.963105	41.665869
3505.059482	606614.066711	41.670874
3504.713005	606545.391716	41.675879
3504.480379	606475.898117	41.680884
3504.455338	606409.222850	41.685888
3504.933620	606347.270605	41.690893
3504.799695	606286.314099	41.695898
3504.537716	606221.425444	41.700903
3504.287427	606159.335850	41.705908
3504.127603	606102.184061	41.710912
3504.162398	606047.602766	41.715917
3504.708077	605993.091387	41.720922
3504.570729	605945.089598	41.725927
3504.054952	605893.895155	41.730932
3504.338744	605827.367937	41.735936
3504.425415	605765.023189	41.740941
3504.390584	605709.200358	41.745946
3504.255647	605658.995743	41.750951
3504.085744	605614.149113	41.755956
3504.497042	605536.944584	41.760960
3504.693413	605488.188130	41.765965
3504.261593	605427.022974	41.770970
3503.812687	605378.216795	41.775975
3503.774188	605340.202124	41.780980
3504.164749	605273.054315	41.785984
3503.935538	605230.766690	41.790989
3503.306855	605185.489639	41.795994
3503.882458	605128.717763	41.800999
3504.053541	605083.415295	41.806004
3504.136572	605021.366792	41.811008
3503.947488	604989.577927	41.816013
3503.677444	604927.734144	41.821018
3503.985394	604879.207518	41.826023
3503.793149	604829.308000	41.831028
3503.753798	604786.888816	41.836032
3503.843747	604733.692781	41.841037
3503.888536	604683.555384	41.846042
3504.105710	604623.734888	41.851047
3504.058516	604582.166612	41.856052
3503.933240	604542.311429	41.861056
3504.020405	604492.066416	41.866061
3504.136402	604436.513312	41.871066
3503.837740	604386.528228	41.876071
3503.866576	604349.099764	41.881076
3503.475211	604291.673950	41.886080
3503.818951	604245.740435	41.891085
3503.745375	604198.471039	41.896090
3503.660197	604149.101859	41.901095
3503.567047	604110.440779	41.906100
3503.590448	604057.701970	41.911104
3503.749124	604007.543493	41.916109
3503.796905	603966.258096	41.921114
3503.826526	603922.023367	41.926119
3503.340553	603878.419428	41.931124
3503.566358	603831.001484	41.936128
3503.508282	603797.237128	41.941133
3503.654555	603746.578981	41.946138
3503.863948	603710.170715	41.951143
3503.178218	603667.297603	41.956148
3503.408708	603614.874413	41.961152
3503.798608	603571.732684	41.966157
3503.664815	603534.076521	41.971162
3503.513476	603485.264915	41.976167
3503.720278	603440.950399	41.981172
3503.787299	603382.997558	41.986176
3503.765393	603347.574874	41.991181
3503.621185	603306.316863	41.996186
3503.501727	603255.697860	42.001191
3503.170120	603220.123007	42.006196
3503.601693	603172.169512	42.011200
3503.694389	603140.531066	42.016205
3503.415747	603094.139333	42.021210
3503.545664	603036.925298	42.026215
3503.388628	603009.979053	42.031220
3503.376065	602964.595953	42.036224
3503.304168	602921.823949	42.041229
3503.636948	602877.737531	42.046234
3503.665032	602829.595338	42.051239
3502.981758	602795.775340	42.056244
3503.168420	602748.108374	42.061248
3502.971980	602712.710809	42.066253
3503.114528	602675.608809	42.071258
3503.192991	602648.875012	42.076263
3503.373551	602611.666762	42.081268
3503.119509	602571.924212	42.086272
3503.432153	602528.840274	42.091277
3503.644422	602488.424019	42.096282
3503.593305	602440.742776	42.101287
3503.332818	602400.800415	42.106292
3503.553537	602354.827729	42.111296
3503.035719	602317.327270	42.116301
3503.059530	602282.093973	42.121306
3503.494752	602244.294139	42.126311
3503.109155	602193.661525	42.131316
3502.864662	602161.872644	42.136320
3502.880130	602128.491704	42.141325
3503.047640	602090.332820	42.146330
3503.267578	602049.413235	42.151335
3503.082249	602019.716478	42.156340
3503.168313	601981.269668	42.161344
3502.984835	601955.726037	42.166349
3503.155525	601923.421132	42.171354
3503.158472	601872.325865	42.176359
3503.347805	601844.621838	42.181364
3503.307408	601798.187076	42.186368
3503.002770	601755.796972	42.191373
3502.721382	601721.009844	42.196378
3502.933519	601692.200866	42.201383
3503.139933	601663.492792	42.206388
3503.063376	601621.316710	42.211392
3502.837405	601578.663362	42.216397
3503.039184	601548.754610	42.221402
3503.163082	601512.301974	42.226407
3503.024534	601473.688224	42.231412
3503.261792	601444.374177	42.236416
3502.985528	601402.828982	42.241421
3503.048507	601363.432627	42.246426
3502.891936	601336.431927	42.251431
3502.621546	601314.553702	42.256436
3502.605288	601266.961730	42.261440
3502.884007	601240.243061	42.266445
3502.579205	601206.909238	42.271450
3502.910944	601173.625941	42.276455
3502.696666	601152.088933	42.281460
3502.475898	601114.737891	42.286464
3503.089131	601077.806862	42.291469
3502.813293	601049.372681	42.296474
3502.737676	601018.404723	42.301479
3502.732114	600992.180294	42.306484
3503.014007	600940.786617	42.311488
3502.819168	600917.894781	42.316493
3502.870222	600889.258916	42.321498
3502.527903	600852.426423	42.326503
3502.719147	600829.624184	42.331508
3502.948842	600798.858092	42.336512
3502.890047	600758.677708	42.341517
3502.117527	600727.967982	42.346522
3502.766562	600698.837720	42.351527
3502.736170	600663.807630	42.356532
3502.939964	600636.848885	42.361536
3502.629325	600612.573088	42.366541
3502.139242	600593.780739	42.371546
3502.646369	600557.014612	42.376551
3502.659070	600531.787176	42.381556
3502.813753	600500.080976	42.386560
3502.470186	600477.962183	42.391565
3502.311508	600444.703183	42.396570
3502.413031	600414.606657	42.401575
3502.150303	600383.515917	42.406580
3502.786862	600352.284500	42.411584
3502.555845	600336.304104	42.416589
3502.471575	600306.937031	42.421594
3502.451438	600274.957170	42.426599
3502.785998	600253.482664	42.431604
3502.694536	600229.772334	42.436608
3502.458847	600199.577750	42.441613
3502.313543	600168.367909	42.446618
3502.587228	600133.388612	42.451623
3502.510398	600111.827972	42.456628
3502.852901	600083.194392	42.461632
3502.716189	600057.488646	42.466637
3502.562094	600027.280810	42.471642
3502.826813	599993.653872	42.476647
3502.630985	599967.506671	42.481652
3502.677508	599935.715565	42.486656
3502.690008	599904.780588	42.491661
3502.478737	599883.340601	42.496666
3502.549707	599858.502861	42.501671
3502.076667	599833.549892	42.506676
3502.162796	599795.845838	42.511680
3502.627165	599771.296770	42.516685
3502.489178	599754.249809	42.521690
3502.731093	599721.726752	42.526695
3502.518038	599701.237700	42.531700
3503.243063	599657.126430	42.536704
3503.027885	599625.175076	42.541709
3502.610498	599598.861372	42.546714
3502.629576	599570.477173	42.551719
3502.802333	599534.911000	42.556724
3502.309692	599498.547732	42.561728
3502.575890	599474.179116	42.566733
3502.156698	599441.007709	42.571738
3502.247945	599426.226932	42.576743
3502.375482	599405.183501	42.581748
3502.418472	599369.987445	42.586752
3502.608609	599352.888536	42.591757
3502.281423	599325.058363	42.596762
3502.150367	599302.002851	42.601767
3502.653170	599278.247524	42.606772
3502.608439	599245.717748	42.611776
3502.707418	599223.326893	42.616781
3502.360615	599192.846438	42.621786
3502.901007	599168.083852	42.626791
3502.518392	599141.162879	42.631796
3502.686038	599099.238795	42.636800
3502.256204	599076.880239	42.641805
3502.426287	599051.023949	42.646810
3502.709276	599014.888153	42.651815
3502.416144	599002.719804	42.656820
3502.609560	598972.955181	42.661824
3502.745298	598946.853716	42.666829
3502.611569	598913.435782	42.671834
3502.650161	598877.437835	42.676839
3502.542361	598864.589597	42.681844
3502.372649	598821.115277	42.686848
3502.603076	598805.460876	42.691853
3502.638911	598776.721503	42.696858
3503.093715	598728.543771	42.701863
3502.610061	598700.385989	42.706868
3502.658929	598669.141332	42.711872
3502.508010	598648.290094	42.716877
3502.631445	598621.488915	42.721882
3502.728800	598594.491507	42.726887
3502.492005	598563.891909	42.731892
3502.331175	598536.684415	42.736896
3502.471233	598507.177115	42.741901
3502.467681	598481.296510	42.746906
3502.562792	598441.333487	42.751911
3502.382751	598427.244500	42.756916
3502.566421	598402.135398	42.761920
3502.406282	598378.782043	42.766925
3502.380755	598344.494356	42.771930
3502.172952	598316.993272	42.776935
3502.193395	598292.860583	42.781940
3502.584428	598271.873816	42.786945
3502.689394	598241.870648	42.791949
3502.474617	598216.973577	42.796954
3502.482662	598176.622669	42.801959
3502.028124	598165.279565	42.806964
3502.148441	598139.478879	42.811969
3501.833901	598110.792461	42.816973
3501.646787	598105.615155	42.821978
3502.003967	598074.670968	42.826983
3501.944551	598068.021882	42.831988
3502.184709	598048.610181	42.836993
3502.178461	598024.631236	42.841997
3502.246493	598004.795802	42.847002
3502.384198	597973.885631	42.852007
3502.517209	597959.346577	42.857012
3502.396737	597930.829581	42.862017
3502.373182	597902.197230	42.867021
3502.159218	597894.871315	42.872026
3502.425610	597867.495178	42.877031
3502.462047	597831.443929	42.882036
3502.184710	597801.649462	42.887041
3502.382476	597778.889649	42.892045
3502.355781	597755.664240	42.897050
3502.249180	597729.948090	42.902055
3502.191416	597707.778770	42.907060
3502.396260	597680.461834	42.912065
3502.083288	597666.092224	42.917069
3502.336415	597645.175835	42.922074
3502.322856	597617.492366	42.927079
3501.915443	597593.925604	42.932084
3502.232914	597570.846244	42.937089
3502.323422	597552.308120	42.942093
3502.159758	597540.368158	42.947098
3502.253548	597507.410838	42.952103
3502.500652	597493.303890	42.957108
3502.816758	597455.505433	42.962113
3502.252469	597442.025909	42.967117
3502.173006	597398.681802	42.972122
3502.421941	597366.951421	42.977127
3501.900811	597366.632243	42.982132
3502.724586	597333.560263	42.987137
3502.483931	597320.280318	42.992141
3502.185329	597295.494303	42.997146
3502.299273	597252.770217	43.002151
3502.205570	597242.270892	43.007156
3502.024664	597212.459685	43.012161
3502.608113	597194.945328	43.017165
3501.999354	597163.949213	43.022170
3502.419972	597142.254651	43.027175
3502.103714	597119.623841	43.032180
3502.145667	597093.482383	43.037185
3502.219383	597080.603590	43.042189
3502.013563	597053.499432	43.047194
3502.479524	597030.996483	43.052199
3501.998122	597001.832461	43.057204
3501.948681	596988.321936	43.062209
3502.175067	596967.658724	43.067213
3501.982688	596945.959453	43.072218
3501.833886	596909.533474	43.077223
3501.761040	596904.437847	43.082228
3501.825050	596883.048840	43.087233
3501.998489	596856.585835	43.092237
3501.869514	596859.910349	43.097242
3502.000855	596826.894969	43.102247
3501.980502	596824.144290	43.107252
3502.121699	596799.338425	43.112257
3502.085721	596786.826900	43.117261
3502.010637	596754.794859	43.122266
3501.945070	596732.524574	43.127271
3501.908706	596713.804540	43.132276
3502.249600	596691.871177	43.137281
3502.412571	596681.982061	43.142285
3502.312641	596662.120294	43.147290
3502.485398	596628.296720	43.152295
3502.271185	596609.253822	43.157300
3502.221073	596583.125495	43.162305
3502.299378	596557.577859	43.167309
3502.283249	596537.652688	43.172314
3502.448889	596503.228996	43.177319
3502.143489	596492.912228	43.182324
3502.217360	596459.654339	43.187329
3502.052170	596438.550612	43.192333
3502.086027	596415.513070	43.197338
3502.385610	596380.216851	43.202343
3502.261585	596371.023221	43.207348
3502.188269	596340.692034	43.212353
3502.435849	596325.632122	43.217357
3502.388820	596297.700077	43.222362
3502.525419	596266.384522	43.227367
3502.084782	596249.929973	43.232372
3502.529525	596215.762139	43.237377
3502.494806	596197.241218	43.242381
3502.071512	596167.915593	43.247386
3502.407879	596147.183518	43.252391
3502.088400	596121.396587	43.257396
3502.370870	596096.767278	43.262401
3502.011513	596081.801902	43.267405
3502.236662	596050.521938	43.272410
3502.454500	596033.863970	43.277415
3502.057297	596011.694084	43.282420
3502.068540	595994.617706	43.287425
3502.114879	595964.066446	43.292429
3501.609620	595952.077944	43.297434
3501.903738	595918.984215	43.302439
3501.787922	595913.444178	43.307444
3502.246139	595897.699792	43.312449
3501.951754	595873.210214	43.317453
3502.029114	595858.276395	43.322458
3501.893654	595827.452727	43.327463
3501.890365	595820.242652	43.332468
3502.045630	595793.479398	43.337473
3501.684192	595778.313625	43.342477
3501.727008	595763.535292	43.347482
3501.684776	595737.353574	43.352487
3501.519776	595733.323323	43.357492
3501.783472	595707.844803	43.362497
3501.452413	595693.875918	43.367501
3501.652450	595694.495477	43.372506
3502.110228	595668.285496	43.377511
3501.569884	595658.405228	43.382516
3501.653629	595642.919300	43.387521
3501.416830	595611.459889	43.392525
3501.538925	595606.533457	43.397530
3501.480182	595600.283301	43.402535
3501.245854	595585.698266	43.407540
3501.858924	595572.633178	43.412545
3501.890119	595564.516207	43.417549
3501.789708	595549.109005	43.422554
3502.142155	595517.156608	43.427559
3501.897554	595502.172471	43.432564
3501.816524	595489.015491	43.437569
3501.714221	595472.156319	43.442573
3501.524981	595452.907137	43.447578
3502.082205	595444.207098	43.452583
3501.590123	595426.807893	43.457588
3501.900492	595402.222686	43.462593
3501.959051	595400.460795	43.467597
3501.839585	595376.042873	43.472602
3501.962739	595359.398650	43.477607
3501.957595	595339.319285	43.482612
3502.168306	595321.209141	43.487617
3502.373519	595314.967628	43.492621
3501.963721	595289.192790	43.497626
3502.116959	595260.375426	43.502631
3501.951574	595244.026507	43.507636
3501.962614	595216.883743	43.512641
3502.379916	595207.053647	43.517645
3502.022477	595187.379598	43.522650
3502.300921	595156.839806	43.527655
3501.875383	595134.622437	43.532660
3501.984829	595115.726558	43.537665
3502.264341	595092.647741	43.542669
3501.678158	595082.824175	43.547674
3502.100944	595055.917090	43.552679
3502.016950	595035.599096	43.557684
3501.884372	595015.589118	43.562689
3502.328209	594997.191596	43.567693
3501.860855	594976.582882	43.572698
3502.189526	594958.153220	43.577703
3502.136263	594942.687690	43.582708
3502.034198	594907.900059	43.587713
3502.152915	594891.406029	43.592717
3502.320747	594876.156224	43.597722
3502.223282	594835.658840	43.602727
3501.694631	594826.827588	43.607732
3501.999760	594810.103981	43.612737
3501.958791	594788.376619	43.617741
3501.792885	594771.325967	43.622746
3501.925443	594753.327230	43.627751
3501.714626	594738.837510	43.632756
3501.670442	594716.559648	43.637761
3501.719336	594693.115394	43.642765
3501.691240	594691.016386	43.647770
3501.939995	594663.133955	43.652775
3501.966833	594663.730575	43.657780
3501.794014	594643.926499	43.662785
3502.131525	594624.393157	43.667789
3501.551521	594605.704310	43.672794
3501.987948	594577.692160	43.677799
3501.659446	594575.189384	43.682804
3502.076040	594558.047328	43.687809
3501.964728	594545.244463	43.692813
3501.894374	594529.931241	43.697818
3502.030303	594498.209949	43.702823
3501.986816	594482.391669	43.707828
3501.640013	594457.155830	43.712833
3501.987523	594442.928979	43.717837
3501.808816	594430.537145	43.722842
3501.944232	594411.185243	43.727847
3501.910759	594393.662567	43.732852
3501.838905	594369.134729	43.737857
3501.957293	594342.824306	43.742861
3501.617505	594336.717500	43.747866
3501.721698	594320.475255	43.752871
3501.434748	594295.079436	43.757876
3501.740545	594286.618083	43.762881
3501.695648	594277.109788	43.767885
3501.897992	594271.368914	43.772890
3501.821721	594242.584674	43.777895
3501.970902	594227.987900	43.782900
3501.994461	594200.239623	43.787905
3502.046849	594181.150685	43.792909
3501.712338	594161.871793	43.797914
3502.156585	594149.632649	43.802919
3501.626651	594134.641106	43.807924
3501.827426	594122.439992	43.812929
3501.878860	594094.787245	43.817933
3501.909082	594070.292842	43.822938
3501.734145	594061.706140	43.827943
3502.012205	594035.420078	43.832948
3501.860757	594031.336979	43.837953
3502.085329	594025.642580	43.842957
3501.926507	593996.169443	43.847962
3501.912923	593976.389313	43.852967
3501.936296	593954.249539	43.857972
3501.673611	593937.913821	43.862977
3501.919039	593921.047910	43.867981
3501.514242	593913.198164	43.872986
3501.821549	593898.225648	43.877991
3501.686391	593879.015242	43.882996
3501.908201	593853.538836	43.888001
3501.612348	593840.713890	43.893005
3501.185653	593836.523498	43.898010
3501.585759	593816.578237	43.903015
3501.701671	593805.692164	43.908020
3501.585314	593785.527089	43.913025
3501.847511	593773.516304	43.918029
3501.688083	593759.217545	43.923034
3502.093740	593737.768797	43.928039
3501.646896	593723.264508	43.933044
3501.750474	593709.124896	43.938049
3501.592267	593700.234791	43.943053
3501.562468	593684.964097	43.948058
3502.063231	593664.401823	43.953063
3501.678602	593658.101304	43.958068
3501.719561	593632.201896	43.963073
3501.883473	593619.555224	43.968077
3501.686220	593605.863169	43.973082
3501.915627	593578.281427	43.978087
3501.836533	593563.869681	43.983092
3501.878229	593553.946537	43.988097
3501.920991	593530.550769	43.993101
3501.846609	593527.657431	43.998106
3501.933460	593505.957556	44.003111
3501.950929	593481.664130	44.008116
3501.912101	593456.528024	44.013121
3502.131274	593439.815710	44.018125
3501.747461	593431.010733	44.023130
3501.830263	593413.919025	44.028135
3502.020024	593393.204514	44.033140
3501.766225	593373.060145	44.038145
3502.003698	593356.394924	44.043149
3501.632514	593347.637988	44.048154
3501.873708	593328.768431	44.053159
3501.828230	593311.696614	44.058164
3501.669696	593292.989652	44.063169
3501.709973	593282.415377	44.068173
3501.647364	593266.448028	44.073178
3501.939275	593251.727439	44.078183
3501.782157	593235.424224	44.083188
3501.541381	593211.921828	44.088193
3502.015126	593198.274609	44.093197
3501.512456	593189.838607	44.098202
3501.868254	593171.251367	44.103207
3501.677455	593164.719913	44.108212
3502.010792	593133.464557	44.113217
3501.835773	593122.422927	44.118221
3501.952592	593101.869511	44.123226
3501.964359	593085.489580	44.128231
3501.585777	593067.968591	44.133236
3501.457787	593049.256427	44.138241
3501.497440	593033.823687	44.143245
3501.595264	593033.808271	44.148250
3501.697735	593007.046273	44.153255
3501.650253	593000.091626	44.158260
3501.754799	592987.503574	44.163265
3501.435460	592957.952489	44.168269
3501.743192	592948.237625	44.173274
3501.818254	592936.154984	44.178279
3501.613657	592917.955429	44.183284
3501.499428	592905.752086	44.188289
3501.774136	592907.111438	44.193293
3501.593867	592880.393323	44.198298
3501.480398	592863.181158	44.203303
3501.499528	592865.231596	44.208308
3501.373543	592842.511827	44.213313
3501.508978	592837.081166	44.218317
3501.490360	592833.477709	44.223322
3501.800493	592814.596469	44.228327
3501.834114	592792.903468	44.233332
3502.013253	592772.489937	44.238337
3501.826343	592760.798661	44.243341
3501.695699	592747.395614	44.248346
3501.795401	592727.044502	44.253351
3501.459178	592699.849443	44.258356
3501.567045	592696.326341	44.263361
3501.869409	592684.257969	44.268365
3501.864693	592679.900975	44.273370
3502.191051	592659.113602	44.278375
3502.034506	592643.410444	44.283380
3501.756481	592619.361604	44.288385
3501.842934	592592.350634	44.293389
3501.731587	592584.854734	44.298394
3501.756054	592570.124930	44.303399
3501.416918	592552.246311	44.308404
3501.382901	592544.537941	44.313409
3501.808437	592536.557372	44.318413
3501.621565	592519.556482	44.323418
3501.991582	592503.069567	44.328423
3501.607384	592494.163697	44.333428
3501.351356	592468.007366	44.338433
3501.747558	592460.231681	44.343437
3501.668446	592448.473122	44.348442
3501.733227	592418.559966	44.353447
3501.475536	592421.905981	44.358452
3501.687596	592402.838994	44.363457
3502.078501	592383.844192	44.368461
3501.953838	592366.332445	44.373466
3501.809572	592345.267413	44.378471
3501.560545	592343.503015	44.383476
3501.765836	592318.776873	44.388481
3501.763339	592292.530391	44.393485
3501.638203	592296.907597	44.398490
3501.647288	592281.528640	44.403495
3501.463619	592253.757615	44.408500
3501.512231	592250.944883	44.413505
3501.243799	592230.399930	44.418509
3501.259021	592219.327627	44.423514
3501.440207	592208.780354	44.428519
3501.379836	592211.895227	44.433524
3501.077222	592202.124835	44.438529
3500.948904	592185.815516	44.443533
3501.277096	592174.443792	44.448538
3501.617524	592160.415378	44.453543
3501.445339	592164.649723	44.458548
3501.269184	592171.589539	44.463553
3501.273372	592160.769350	44.468557
3501.223460	592131.624671	44.473562
3501.796267	592121.416811	44.478567
3501.527789	592126.267305	44.483572
3501.648726	592104.459080	44.488577
3501.912319	592087.036451	44.493581
3501.880857	592074.218138	44.498586
3502.040657	592061.069367	44.503591
3501.803855	592039.216753	44.508596
3501.683662	592024.108089	44.513601
3501.495956	592012.265847	44.518605
3501.431203	592007.567331	44.523610
3501.858803	591979.750128	44.528615
3501.637203	591966.761047	44.533620
3501.599455	591949.936302	44.538625
3501.776648	591919.453181	44.543629
3501.695031	591918.814634	44.548634
3501.811785	591915.840888	44.553639
3501.719023	591887.754157	44.558644
3501.848239	591881.672801	44.563649
3501.715610	591869.621426	44.568653
3501.570768	591855.818751	44.573658
3501.523848	591848.612810	44.578663
3501.669230	591838.120862	44.583668
3501.866232	591813.394853	44.588673
3501.715763	591790.776863	44.593677
3501.476365	591770.627222	44.598682
3501.742769	591750.198104	44.603687
3501.744919	591753.052878	44.608692
3501.537593	591740.311750	44.613697
3501.726039	591716.989428	44.618701
3501.755943	591712.326076	44.623706
3501.520485	591686.916002	44.628711
3501.858448	591676.944804	44.633716
3501.696414	591663.495213	44.638721
3501.703519	591631.134359	44.643725
3501.782751	591622.055128	44.648730
3501.991119	591609.499321	44.653735
3501.694245	591596.972391	44.658740
3501.399800	591585.697381	44.663745
3501.587418	591570.139217	44.668749
3501.528700	591559.478533	44.673754
3501.668126	591542.575360	44.678759
3501.577969	591525.858329	44.683764
3501.268000	591510.728516	44.688769
3501.873043	591496.257128	44.693773
3501.662079	591498.644355	44.698778
3501.668544	591478.906567	44.703783
3501.625675	591460.979809	44.708788
3501.589203	591447.710692	44.713793
3501.674357	591427.659949	44.718797
3501.220664	591417.261242	44.723802
3501.397464	591411.122088	44.728807
3501.441031	591417.527107	44.733812
3501.435110	591390.277085	44.738817
3501.686003	591371.202197	44.743821
3501.571626	591369.767241	44.748826
3501.444193	591348.196682	44.753831
3501.732215	591338.633728	44.758836
3501.799332	591323.244326	44.763841
3501.772994	591315.884529	44.768845
3501.298428	591307.091981	44.773850
3501.654341	591287.399400	44.778855
3501.511320	591273.445409	44.783860
3501.717663	591263.193841	44.788865
3501.624542	591255.894536	44.793869
3501.500861	591234.673821	44.798874
3501.454853	591226.515530	44.803879
3501.577522	591216.076621	44.808884
3501.413114	591199.520972	44.813889
3501.334905	591175.487746	44.818893
3501.328609	591169.928118	44.823898
3501.541130	591156.920284	44.828903
3501.188033	591166.092569	44.833908
3501.358637	591154.894689	44.838913
3501.605860	591127.454143	44.843917
3501.561299	591134.724718	44.848922
3502.034613	591113.210057	44.853927
3501.329982	591102.950463	44.858932
3501.123444	591089.507110	44.863937
3501.506010	591074.969747	44.868941
3501.615288	591065.133924	44.873946
3501.646251	591050.501209	44.878951
3501.584151	591046.603378	44.883956
3501.818222	591024.524800	44.888961
3501.850316	591005.884231	44.893965
3501.733296	590994.029813	44.898970
3501.677951	590969.641885	44.903975
3501.155991	590959.654169	44.908980
3501.493096	590959.250678	44.913985
3501.601276	590949.865781	44.918989
3501.700389	590921.095284	44.923994
3501.546381	590919.516175	44.928999
3501.884917	590910.145328	44.934004
3501.559814	590889.506473	44.939009
3501.553326	590880.840783	44.944013
3501.469241	590869.431942	44.949018
3501.261339	590847.371997	44.954023
3501.427747	590839.330494	44.959028
3501.456245	590839.225724	44.964033
3501.553716	590818.971537	44.969037
3501.455675	590799.699704	44.974042
3501.597354	590784.398068	44.979047
3501.092843	590776.160823	44.984052
3501.141673	590776.403549	44.989057
3501.355513	590764.246673	44.994061
3500.889671	590757.205682	44.999066
3501.385861	590751.016223	45.004071
3501.245866	590749.334705	45.009076
3501.434474	590737.031454	45.014081
3501.519668	590716.027544	45.019085
3501.374395	590710.940274	45.024090
3501.301891	590699.930216	45.029095
3501.461622	590700.005316	45.034100
3501.680859	590688.398575	45.039105
3501.759836	590671.102709	45.044109
3501.690860	590665.252037	45.049114
3501.677612	590647.419486	45.054119
3501.491496	590633.271011	45.059124
3501.289482	590620.377431	45.064129
3501.543252	590597.292956	45.069133
3501.182695	590582.119644	45.074138
3501.074371	590567.708436	45.079143
3501.331136	590575.282964	45.084148
3501.091498	590573.065925	45.089153
3501.725202	590557.987634	45.094157
3501.634409	590552.140311	45.099162
3501.755253	590533.134368	45.104167
3501.676009	590525.131033	45.109172
3501.265461	590510.466409	45.114177
3501.624303	590501.492815	45.119181
3501.292114	590488.920012	45.124186
3501.261703	590469.637016	45.129191
3501.423996	590456.736386	45.134196
3501.548258	590452.709009	45.139201
3501.415977	590441.708032	45.144205
3501.149539	590432.882227	45.149210
3501.327064	590410.460546	45.154215
3501.840265	590412.133627	45.159220
3501.470337	590400.869170	45.164225
3501.516750	590373.658490	45.169229
3501.514707	590367.446505	45.174234
3501.401988	590360.951228	45.179239
3501.645170	590355.552571	45.184244
3501.367455	590329.143924	45.189249
3501.380168	590324.833348	45.194253
3501.727766	590326.131544	45.199258
3501.485240	590306.129937	45.204263
3501.713051	590290.463446	45.209268
3501.919102	590287.775885	45.214273
3501.437111	590261.549302	45.219277
3501.675421	590250.189602	45.224282
3501.934971	590239.978843	45.229287
3501.878147	590224.657346	45.234292
3502.092325	590206.588116	45.239297
3501.933839	590195.641082	45.244301
3501.497024	590175.920102	45.249306
3501.831302	590158.483306	45.254311
3501.775608	590134.794930	45.259316
3501.608590	590120.843194	45.264321
3501.561837	590106.321544	45.269325
3501.855614	590093.099328	45.274330
3501.813354	590076.572955	45.279335
3501.579203	590052.912297	45.284340
3501.646663	590040.326593	45.289345
3501.771856	590032.691730	45.294349
3501.528540	590004.673716	45.299354
3501.848662	590000.715753	45.304359
3501.644577	589998.943935	45.309364
3501.377779	589979.496616	45.314369
3501.961291	589965.327149	45.319373
3501.758953	589957.442836	45.324378
3501.534326	589923.459767	45.329383
3501.452202	589921.217968	45.334388
3501.602979	589917.386649	45.339393
3501.972928	589882.709300	45.344397
3501.652789	589877.448569	45.349402
3501.777074	589869.012125	45.354407
3501.584157	589852.759463	45.359412
3501.721571	589843.369034	45.364417
3501.705505	589815.465304	45.369421
3501.268334	589804.310934	45.374426
3501.637831	589791.477319	45.379431
3501.594970	589786.624106	45.384436
3501.596445	589763.777694	45.389441
3501.411156	589747.974592	45.394445
3501.297538	589747.641523	45.399450
3501.480711	589740.097592	45.404455
3501.847195	589715.841287	45.409460
3501.692081	589707.749002	45.414465
3501.626700	589689.472104	45.419469
3501.362359	589669.472726	45.424474
3501.673669	589664.814598	45.429479
3501.410209	589651.779158	45.434484
3501.295296	589640.073224	45.439489
3501.773246	589624.116155	45.444493
3501.299468	589620.733079	45.449498
3501.650608	589605.346925	45.454503
3501.428622	589598.367252	45.459508
3501.205448	589582.419523	45.464513
3501.665981	589567.266724	45.469517
3501.437651	589559.887202	45.474522
3501.308784	589544.676205	45.479527
3501.469417	589532.476160	45.484532
3501.353498	589534.999265	45.489537
3501.308637	589521.929494	45.494541
3501.218198	589509.267650	45.499546
3501.357362	589487.651686	45.504551
3501.234636	589500.296531	45.509556
3501.006584	589496.724694	45.514561
3501.399494	589488.546573	45.519565
3501.084820	589487.192777	45.524570
3501.220796	589458.863538	45.529575
3501.637919	589459.850359	45.534580
3501.446045	589455.471213	45.539585
3501.655326	589441.960797	45.544589
3501.349399	589410.894770	45.549594
3501.341929	589412.048177	45.554599
3501.293663	589410.151698	45.559604
3501.283783	589407.397470	45.564609
3501.578531	589379.143407	45.569613
3501.198493	589378.501255	45.574618
3501.277655	589367.816846	45.579623
3501.574505	589362.409306	45.584628
3501.174489	589344.134033	45.589633
3501.658107	589329.929251	45.594637
3501.429213	589328.912746	45.599642
3501.569049	589318.168700	45.604647
3501.391800	589302.864719	45.609652
3501.496722	589285.161752	45.614657
3501.570840	589288.056032	45.619661
3501.299834	589277.025448	45.624666
3501.428956	589252.805212	45.629671
3501.306333	589248.665673	45.634676
3501.261790	589248.923031	45.639681
3501.499093	589241.320188	45.644685
3500.915447	589228.183979	45.649690
3501.487334	589205.848459	45.654695
3501.264250	589199.319631	45.659700
3501.012908	589196.953823	45.664705
3501.512565	589195.172065	45.669709
3500.977739	589186.487400	45.674714
3501.143682	589159.305077	45.679719
3501.131406	589157.853862	45.684724
3501.097499	589156.907066	45.689729
3501.227451	589150.222811	45.694733
3501.056783	589156.662666	45.699738
3501.071464	589158.013052	45.704743
3501.476516	589160.454802	45.709748
3501.330393	589125.655287	45.714753
3501.249282	589111.789023	45.719757
3500.943548	589115.243771	45.724762
3501.127483	589117.519681	45.729767
3501.232291	589115.749532	45.734772
3501.214700	589095.259578	45.739777
3501.255502	589074.910770	45.744781
3501.151152	589076.981234	45.749786
3501.196729	589071.512622	45.754791
3501.426704	589073.330406	45.759796
3500.829560	589064.505072	45.764801
3501.260696	589044.445916	45.769805
3501.199741	589041.749685	45.774810
3501.402105	589016.765904	45.779815
3501.469865	588952.971947	45.784820
3501.052745	588858.087990	45.789825
3501.489716	588704.195331	45.794829
3500.998328	588500.439035	45.799834
3500.466683	588253.291711	45.804839
3500.415592	587951.644906	45.809844
3499.707900	587612.459057	45.814849
3499.517287	587225.123713	45.819853
3498.582089	586792.988216	45.824858
3497.892188	586307.422718	45.829863
3497.080989	585794.840247	45.834868
3496.183946	585227.965168	45.839873
3495.487686	584614.663993	45.844877
3494.160866	583980.724356	45.849882
3493.280601	583295.695387	45.854887
3492.231297	582572.698744	45.859892
3490.844743	581813.107062	45.864897
3489.769642	581005.630006	45.869901
3488.435748	580166.944403	45.874906
3487.416912	579276.643291	45.879911
3485.601954	578355.751925	45.884916
3483.874895	577403.071411	45.889921
3482.184607	576409.171436	45.894925
3480.440274	575403.001538	45.899930
3478.840646	574338.671365	45.904935
3477.199236	573245.396384	45.909940
3474.985455	572125.208578	45.914945
3473.394757	570982.078897	45.919949
3471.173047	569805.456058	45.924954
3469.136801	568584.259706	45.929959
3467.285915	567348.346250	45.934964
3464.656189	566072.808807	45.939969
3462.276996	564766.512226	45.944973
3460.060772	563454.519561	45.949978
3457.755254	562113.564892	45.954983
3455.763632	560750.306751	45.959988
3453.090687	559360.121267	45.964993
3450.934451	557932.814179	45.969997
3448.366696	556492.938678	45.975002
3446.097802	555027.665626	45.980007
3442.855661	553534.973999	45.985012
3440.147045	552029.950282	45.990017
3437.561778	550512.101962	45.995021
3434.307081	548987.331268	46.000026
3431.691023	547434.462931	46.005031
3428.865857	545855.078361	46.010036
3426.486789	544265.413062	46.015041
3423.435435	542660.658852	46.020045
3420.251340	541048.524934	46.025050
3417.001238	539405.450338	46.030055
3414.100119	537758.786227	46.035060
3410.880328	536106.824900	46.040065
3407.876116	534435.488118	46.045069
3404.663371	532758.378492	46.050074
3401.485816	531066.846956	46.055079
3398.263665	529365.232388	46.060084
3394.743050	527658.104615	46.065089
3391.661673	525927.264490	46.070093
3388.164389	524210.419101	46.075098
3384.971368	522470.329996	46.080103
3381.571757	520727.628573	46.085108
3378.249166	518980.154232	46.090113
3375.046810	517216.458306	46.095117
3371.166006	515463.529161	46.100122
3367.812280	513687.253902	46.105127
3364.152362	511914.933064	46.110132
3360.756955	510145.623119	46.115137
3357.227706	508350.338278	46.120141
3353.842939	506582.747032	46.125146
3350.064645	504781.096256	46.130151
3346.655218	502991.673382	46.135156
3343.065897	501193.427369	46.140161
3339.797786	499380.625830	46.145165
3335.960015	497573.997231	46.150170
3332.216085	495765.566894	46.155175
3328.621250	493955.529033	46.160180
3324.773861	492150.410349	46.165185
3321.432754	490343.227858	46.170189
3317.482468	488534.207306	46.175194
3313.709265	486716.407841	46.180199
3309.859614	484902.648003	46.185204
3306.238522	483098.288897	46.190209
3302.648830	481287.096409	46.195213
3298.638894	479477.225638	46.200218
3295.305860	477665.575783	46.205223
3291.324193	475847.502789	46.210228
3287.369341	474039.632567	46.215233
3284.290849	472231.877758	46.220237
3280.078588	470424.149781	46.225242
3276.183991	468612.278964	46.230247
3272.636361	466807.336340	46.235252
3268.462658	465010.287107	46.240257
3265.059348	463202.909234	46.245261
3261.410352	461413.891972	46.250266
3257.678706	459602.134663	46.255271
3253.313074	457806.375874	46.260276
3249.700129	456013.804703	46.265281
3246.052401	454216.044328	46.270285
3241.914303	452436.398189	46.275290
3238.499299	450642.337256	46.280295
3234.778803	448856.497097	46.285300
3230.686361	447080.259027	46.290305
3227.011825	445297.857585	46.295309
3222.936018	443517.522920	46.300314
3219.244768	441745.414157	46.305319
3215.808803	439965.600696	46.310324
3211.887271	438200.536217	46.315329
3208.228562	436442.307751	46.320333
3204.077911	434673.304324	46.325338
3200.271442	432907.834103	46.330343
3196.442459	431144.031245	46.335348
3192.301157	429387.466759	46.340353
3188.755557	427638.306075	46.345357
3185.090157	425897.221965	46.350362
3181.358262	424151.688955	46.355367
3177.626200	422400.581590	46.360372
3173.572947	420656.219233	46.365377
3170.020987	418922.431215	46.370381
3165.960593	417190.150607	46.375386
3162.285329	415461.217134	46.380391
3158.449256	413733.588239	46.385396
3154.806247	412011.064934	46.390401
3150.732549	410281.827135	46.395405
3146.762417	408573.843591	46.400410
3143.223989	406859.572550	46.405415
3139.511444	405147.987335	46.410420
3135.697752	403446.435661	46.415425
3131.932509	401730.033390	46.420429
3128.128582	400026.753779	46.425434
3124.413433	398334.195763	46.430439
3120.349980	396640.097915	46.435444
3116.298264	394938.415364	46.440449
3112.908886	393247.929354	46.445453
3108.690037	391571.821140	46.450458
3105.017587	389888.861495	46.455463
3101.375747	388211.036948	46.460468
3097.245505	386549.017584	46.465473
3093.903486	384875.263668	46.470477
3089.891781	383226.438256	46.475482
3085.971022	381558.727523	46.480487
3082.716045	379898.576180	46.485492
3078.810743	378243.856208	46.490497
3075.240543	376592.917208	46.495501
3071.213898	374943.624278	46.500506
3067.044655	373302.051295	46.505511
3063.676739	371644.911856	46.510516
3059.510586	370014.980069	46.515521
3056.054230	368381.870176	46.520525
3052.500944	366752.162132	46.525530
3048.448288	365113.445231	46.530535
3044.946011	363495.233016	46.535540
3041.143118	361870.905532	46.540545
3037.869049	360249.201965	46.545549
3033.868387	358632.607345	46.550554
3030.178578	357010.693711	46.555559
3026.423993	355394.931881	46.560564
3022.584959	353780.294287	46.565569
3018.893696	352172.287120	46.570573
3015.282658	350564.135846	46.575578
3011.636132	348967.960091	46.580583
3007.880705	347352.199387	46.585588
3003.853889	345765.995925	46.590593
3000.479271	344162.581246	46.595597
2996.741448	342573.081694	46.600602
2993.018560	340975.649928	46.605607
2989.168757	339391.210174	46.610612
2985.587665	337800.300599	46.615617
2981.453158	336222.707762	46.620621
2977.894621	334639.260285	46.625626
2974.568360	333056.904434	46.630631
2970.606066	331482.618811	46.635636
2966.910684	329907.158500	46.640641
2963.090372	328329.440991	46.645645
2959.385275	326777.257363	46.650650
2955.626498	325211.692619	46.655655
2952.337036	323647.215373	46.660660
2948.564336	322082.881753	46.665665
2945.063610	320521.958226	46.670669
2941.233006	318967.669552	46.675674
2937.448028	317398.001749	46.680679
2933.656217	315853.493699	46.685684
2929.870850	314304.987713	46.690689
2926.395939	312758.543590	46.695693
2922.194598	311218.650418	46.700698
2918.598405	309682.022435	46.705703
2914.971549	308146.011951	46.710708
2911.374198	306614.656798	46.715713
2908.145793	305070.065358	46.720717
2904.000776	303550.715036	46.725722
2900.623650	302013.410268	46.730727
2897.066098	300479.677841	46.735732
2892.949383	298967.801864	46.740737
2889.519805	297447.199495	46.745741
2886.019552	295927.229007	46.750746
2882.232349	294398.685292	46.755751
2878.582054	292881.738805	46.760756
2874.870357	291372.120341	46.765761
2871.483936	289853.860817	46.770765
2867.445515	288348.496852	46.775770
2864.093377	286835.047830	46.780775
2860.627715	285327.946396	46.785780
2856.465547	283825.451990	46.790785
2852.737466	282311.426217	46.795789
2849.000662	280805.465806	46.800794
2845.462034	279312.835404	46.805799
2841.702688	277816.670969	46.810804
2838.029291	276330.495813	46.815809
2834.267877	274826.662012	46.820813
2830.665542	273350.860210	46.825818
2827.026675	271869.182095	46.830823
2823.676326	270379.183833	46.835828
2820.037847	268898.805633	46.840833
2816.129003	267416.027207	46.845837
2812.332910	265938.301167	46.850842
2808.937505	264462.578721	46.855847
2805.188072	262986.636034	46.860852
2801.402256	261516.714046	46.865857
2797.943037	260050.032225	46.870861
2794.279802	258584.764535	46.875866
2790.849850	257119.850239	46.880871
2787.083714	255649.521965	46.885876
2783.534006	254191.520383	46.890881
2780.255723	252723.605627	46.895885
2776.420793	251263.632663	46.900890
2772.849998	249804.852651	46.905895
2768.731810	248342.529034	46.910900
2765.488028	246894.904119	46.915905
2761.600437	245434.100024	46.920909
2757.876834	243987.037844	46.925914
2754.044650	242537.461641	46.930919
2750.728212	241085.452747	46.935924
2746.734432	239655.291575	46.940929
2743.267728	238213.910953	46.945933
2739.737057	236772.024313	46.950938
2736.102199	235325.792891	46.955943
2732.626861	233888.267109	46.960948
2728.859324	232459.238272	46.965953
2725.404800	231032.550898	46.970957
2721.730965	229603.271577	46.975962
2718.241777	228170.650167	46.980967
2714.669015	226745.477264	46.985972
2710.957289	225316.046489	46.990977
2707.280465	223883.884973	46.995981
2703.344220	222467.733741	47.000986
2699.782106	221043.680845	47.005991
2696.198991	219625.312840	47.010996
2692.477720	218206.306958	47.016001
2689.251603	216781.394676	47.021005
2685.404272	215375.099491	47.026010
2681.545084	213957.961224	47.031015
2678.337932	212546.838919	47.036020
2674.402544	211143.477178	47.041025
2670.900392	209720.723957	47.046029
2667.398138	208322.657047	47.051034
2663.762873	206926.732824	47.056039
2660.494457	205519.044681	47.061044
2656.465480	204117.036955	47.066049
2652.947842	202710.451611	47.071053
2649.329022	201324.012105	47.076058
2645.381663	199920.011958	47.081063
2642.301954	198531.728647	47.086068
2638.228558	197143.078497	47.091073
2635.101595	195734.964544	47.096077
2631.263173	194348.291262	47.101082
2627.492814	192966.358462	47.106087
2624.214936	191568.753276	47.111092
2620.044947	190191.013774	47.116097
2616.686077	188807.230300	47.121101
2612.946796	187427.241181	47.126106
2608.927645	186053.195662	47.131111
2605.762423	184670.733380	47.136116
2601.770407	183304.435953	47.141121
2598.423232	181935.408595	47.146125
2594.929444	180568.028142	47.151130
2591.055374	179197.341051	47.156135
2587.889225	177839.193552	47.161140
2584.175716	176483.724648	47.166145
2580.474320	175106.811874	47.171149
2576.671816	173747.378804	47.176154
2573.141768	172385.800420	47.181159
2569.743399	171035.351372	47.186164
2565.947699	169676.727020	47.191169
2562.451172	168311.105166	47.196173
2558.596049	166964.913820	47.201178
2555.250631	165611.642142	47.206183
2551.444441	164266.895664	47.211188
2547.840487	162927.566848	47.216193
2544.491956	161572.315100	47.221197
2540.409008	160241.733616	47.226202
2536.782115	158894.982939	47.231207
2533.238066	157556.305182	47.236212
2529.519252	156225.791606	47.241217
2526.304420	154888.191130	47.246221
2522.204616	153559.286654	47.251226
2518.891128	152225.772328	47.256231
2514.898297	150901.138750	47.261236
2511.288567	149573.333927	47.266241
2508.129667	148250.479550	47.271245
2504.551081	146942.713841	47.276250
2501.297115	145537.357309	47.281255
2497.587503	144199.091390	47.286260
2494.075114	142892.627399	47.291265
2490.169924	141567.530031	47.296269
2486.646611	140252.880176	47.301274
2482.837062	138939.048984	47.306279
2479.235705	137624.203890	47.311284
2475.707070	136323.735197	47.316289
2472.003797	135004.387765	47.321293
2468.193007	133695.921618	47.326298
2464.639106	132400.073037	47.331303
2460.804114	131097.424682	47.336308
2457.293594	129807.116184	47.341313
2453.745896	128512.374989	47.346317
2450.076434	127224.052364	47.351322
2446.457883	125932.543679	47.356327
2443.131984	124646.676950	47.361332
2439.377989	123356.593691	47.366337
2435.823211	122067.729036	47.371341
2432.433667	120777.761395	47.376346
2428.272842	119506.841971	47.381351
2425.039813	118220.788119	47.386356
2421.264532	116948.557928	47.391361
2418.001670	115671.293226	47.396365
2413.799798	114403.425208	47.401370
2410.160225	113130.503228	47.406375
2407.190520	111861.526089	47.411380
2403.021215	110600.219124	47.416385
2399.425760	109334.099523	47.421389
2396.017848	108070.767640	47.426394
2392.446497	106816.609505	47.431399
2388.811036	105554.244146	47.436404
2385.374159	104307.250349	47.441409
2381.387287	103039.084604	47.446413
2378.014196	101795.796991	47.451418
2374.239393	100545.259774	47.456423
2370.610502	99295.751684	47.461428
2366.921462	98057.447387	47.466433
2363.711576	96803.153692	47.471437
2359.900320	95575.919994	47.476442
2356.348849	94337.421746	47.481447
2352.634045	93086.723068	47.486452
2348.605812	91856.544086	47.491457
2345.377609	90615.806829	47.496461
2341.871347	89393.765276	47.501466
2337.757916	88165.897077	47.506471
2334.757372	86945.414081	47.511476
2331.123583	85724.445562	47.516481
2327.699311	84499.455616	47.521485
2323.821913	83280.978158	47.526490
2320.076470	82063.192414	47.531495
2316.681183	80841.402953	47.536500
2312.893262	79641.295091	47.541505
2309.219724	78418.486181	47.546509
2305.158313	77229.562329	47.551514
2301.636788	76020.349216	47.556519
2298.265280	74819.420849	47.561524
2294.170615	73629.516401	47.566529
2290.702781	72431.300215	47.571533
2287.004739	71244.233634	47.576538
2283.284947	70054.900313	47.581543
2279.912671	68874.936633	47.586548
2275.976478	67700.980259	47.591553
2272.509849	66525.861310	47.596557
2268.552089	65357.271294	47.601562
2264.974228	64184.810260	47.606567
2261.276710	63029.095425	47.611572
2257.663609	61876.746306	47.616577
2253.860936	60707.662923	47.621581
2250.143935	59559.366209	47.626586
2246.485335	58419.230190	47.631591
2242.888873	57265.038678	47.636596
2239.226499	56135.816670	47.641601
2235.732578	54998.271863	47.646605
2232.028225	53867.552013	47.651610
2228.317817	52730.917363	47.656615
2224.759862	51605.815068	47.661620
2220.490659	50489.733728	47.666625
2217.050003	49373.417882	47.671629
2213.424172	48264.568144	47.676634
2209.596234	47168.913752	47.681639
2205.913366	46068.342465	47.686644
2201.906948	44983.019889	47.691649
2198.398759	43884.747540	47.696653
2194.159285	42805.014383	47.701658
2190.437444	41732.411752	47.706663
2186.658651	40657.365582	47.711668
2182.746027	39604.134231	47.716673
2178.617917	38555.856642	47.721677
2174.659615	37518.564647	47.726682
2170.806119	36488.406373	47.731687
2166.761557	35462.891689	47.736692
2162.597905	34459.206319	47.741697
2158.288609	33463.774343	47.746701
2153.177733	32502.690797	47.751706
2148.319926	31566.266520	47.756711
2143.499983	30647.921830	47.761716
2138.537101	29759.356414	47.766721
2133.372994	28872.533685	47.771725
2128.493843	28032.280942	47.776730
2123.700557	27218.447789	47.781735
2119.623239	26406.594414	47.786740
2115.221277	25636.300864	47.791745
2110.718549	24872.483378	47.796749
2106.498705	24136.724087	47.801754
2102.183267	23418.302570	47.806759
2097.936034	22714.777698	47.811764
2094.007545	22033.337070	47.816769
2089.979396	21366.093747	47.821773
2086.492145	20712.534401	47.826778
2082.480105	20070.987500	47.831783
2078.704471	19424.781557	47.836788
2074.939311	18814.927118	47.841793
2071.230422	18192.687631	47.846797
2067.305169	17598.585094	47.851802
2063.894790	16992.589332	47.856807
2060.511501	16402.238676	47.861812
2056.911877	15829.140428	47.866817
2052.975519	15247.910881	47.871821
2049.506331	14673.946376	47.876826
2045.866250	14115.974132	47.881831
2042.675408	13549.133353	47.886836
2038.788996	12994.579065	47.891841
2035.518002	12441.138240	47.896845
2031.906628	11893.832634	47.901850
2028.578405	11351.661955	47.906855
2024.994299	10811.984484	47.911860
2020.864948	10279.258168	47.916865
2017.481338	9743.533869	47.921869
2014.018831	9215.994531	47.926874
2010.626107	8685.771830	47.931879
2006.979274	8161.905981	47.936884
2003.664233	7654.005990	47.941889
2000.157979	7130.536601	47.946893
1996.433925	6617.433932	47.951898
1992.767761	6104.235218	47.956903
1989.393578	5590.084190	47.961908
1985.135474	5095.349468	47.966913
1981.674127	4593.547615	47.971917
1977.533164	4114.542982	47.976922
1973.140034	3652.428496	47.981927
1968.041534	3211.972924	47.986932
1962.888269	2797.816217	47.991937
1958.088239	2386.562801	47.996941
1952.608736	2025.782868	48.001946
1947.861771	1673.305758	48.006951
1944.040627	1340.029386	48.011956
1938.695582	1026.054421	48.016961
1934.487001	733.039129	48.021965
1929.661681	468.508482	48.026970
1924.775667	227.837244	48.031975
1916.054527	113.423946	48.036980
1903.238573	167.651685	48.041985
1895.859843	169.435817	48.046989
1891.714163	166.756058	48.051994
1890.388137	164.701287	48.056999
1888.805037	161.275669	48.062004
1886.990436	163.729901	48.067009
1885.769960	161.690252	48.072013
1883.255043	168.762556	48.077018
1879.834704	154.323182	48.082023
1876.317686	156.474327	48.087028
1873.337407	155.181477	48.092033
1870.199371	155.090265	48.097037
1867.052424	154.753669	48.102042
1863.558370	151.190486	48.107047
1860.770676	141.315637	48.112052
1857.245687	154.861032	48.117057
1853.756843	152.448676	48.122061
1850.716874	156.591166	48.127066
1847.534479	156.820123	48.132071
1844.114621	156.428162	48.137076
1840.317041	162.682435	48.142081
1837.281957	157.443366	48.147085
1834.153963	147.865393	48.152090
1830.484721	152.043085	48.157095
1827.374930	148.634923	48.162100
1824.043834	152.541396	48.167105
1820.793777	142.773718	48.172109
1817.214596	141.533479	48.177114
1813.660349	153.238942	48.182119
1810.273755	147.093086	48.187124
1806.399648	147.670755	48.192129
1803.507854	145.633232	48.197133
1800.499151	147.068920	48.202138
1796.557193	143.645461	48.207143
1793.508736	143.084661	48.212148
1789.598193	146.695833	48.217153
1785.836089	139.314744	48.222157
1782.943342	144.076468	48.227162
1779.138023	145.124286	48.232167
1776.302470	142.021248	48.237172
1772.945736	148.263496	48.242177
1769.085753	145.323942	48.247181
1765.816860	135.613023	48.252186
1762.336165	145.468793	48.257191
1758.981392	143.484756	48.262196
1755.159461	145.784898	48.267201
1751.701684	144.737660	48.272205
1748.794518	140.820075	48.277210
1745.236415	147.445030	48.282215
1741.563883	139.293784	48.287220
1737.741328	147.804645	48.292225
1734.644320	143.214403	48.297229
1731.287169	150.769721	48.302234
1727.854963	146.481881	48.307239
1724.363773	141.434462	48.312244
1720.884347	146.683497	48.317249
1717.523976	145.997523	48.322253
1713.831191	144.332162	48.327258
1710.471607	143.165164	48.332263
1707.280624	134.182415	48.337268
1703.349891	138.638356	48.342273
1699.880350	133.030725	48.347277
1696.453973	135.841636	48.352282
1693.016127	149.174103	48.357287
1689.562286	139.735773	48.362292
1685.887035	141.155584	48.367297
1682.867923	145.212590	48.372301
1679.729534	139.907488	48.377306
1675.577507	135.203965	48.382311
1672.251750	135.025131	48.387316
1668.655345	144.838920	48.392321
1665.471026	137.642710	48.397325
1661.918508	130.769892	48.402330
1658.059223	138.346862	48.407335
1654.702150	132.671026	48.412340
1650.904021	135.707816	48.417345
1648.065775	131.994620	48.422349
1644.999708	135.163618	48.427354
1640.842583	141.619754	48.432359
1637.807332	142.550264	48.437364
1633.945840	140.753146	48.442369
1630.106810	134.345971	48.447373
1626.653830	136.088527	48.452378
1623.259298	140.264418	48.457383
1620.185875	119.142664	48.462388
1616.658845	133.257905	48.467393
1613.038435	131.249053	48.472397
1609.892581	131.766601	48.477402
1606.490967	137.269250	48.482407
1602.479903	130.433421	48.487412
1598.731270	131.845764	48.492417
1595.355680	139.653942	48.497421
1591.475816	133.863794	48.502426
1588.195371	143.371882	48.507431
1585.255107	126.895951	48.512436
1581.502094	136.398904	48.517441
1578.291673	126.229650	48.522445
1574.820851	128.680549	48.527450
1570.847517	131.393603	48.532455
1568.058187	123.167482	48.537460
1564.059590	132.620288	48.542465
1560.790672	130.739945	48.547469
1556.923892	127.289002	48.552474
1553.720618	133.387060	48.557479
1550.523128	124.993868	48.562484
1546.416567	131.277601	48.567489
1543.265397	128.053189	48.572493
1540.078081	130.292043	48.577498
1535.977038	127.684552	48.582503
1532.940102	122.983739	48.587508
1529.264845	133.876112	48.592513
1525.857123	135.260432	48.597517
1521.966032	126.482254	48.602522
1518.436135	131.555742	48.607527
1514.862386	133.791812	48.612532
1511.585434	133.570590	48.617537
1508.678439	133.911573	48.622541
1505.175681	129.625372	48.627546
1501.457860	127.350228	48.632551
1498.086112	126.346563	48.637556
1494.287875	130.620481	48.642561
1490.681105	131.536083	48.647565
1487.271117	125.780007	48.652570
1483.691236	138.343787	48.657575
1480.250384	129.371765	48.662580
1476.849565	129.796380	48.667585
1473.586916	137.143975	48.672589
1470.001839	126.910018	48.677594
1466.130992	135.874614	48.682599
1462.884980	133.595239	48.687604
1459.079411	133.551691	48.692609
1455.472923	132.119700	48.697613
1452.103786	127.404471	48.702618
1448.839889	139.330328	48.707623
1445.412245	137.481195	48.712628
1441.567203	133.738988	48.717633
1438.456289	131.334069	48.722637
1435.253508	131.075951	48.727642
1431.353711	131.929870	48.732647
1428.071996	130.526149	48.737652
1424.396015	132.379609	48.742657
1421.247085	121.087130	48.747661
1417.489089	122.807893	48.752666
1413.434552	132.199898	48.757671
1410.216780	126.461223	48.762676
1406.465207	125.665743	48.767681
1403.322471	122.819719	48.772685
1400.004241	125.876391	48.777690
1396.664771	139.161879	48.782695
1393.405678	121.239453	48.787700
1389.301537	125.516995	48.792705
1385.810773	120.744900	48.797709
1382.215382	119.978768	48.802714
1378.612620	123.728568	48.807719
1375.747317	120.389863	48.812724
1372.140154	123.248156	48.817729
1368.411756	123.230528	48.822733
1364.857298	127.925084	48.827738
1361.067898	123.348445	48.832743
1357.938167	121.772258	48.837748
1354.067421	122.260983	48.842753
1350.769739	126.371171	48.847757
1347.355859	122.713376	48.852762
1343.884820	122.630161	48.857767
1340.797157	119.402207	48.862772
1337.036112	118.535469	48.867777
1333.444689	117.161280	48.872781
1329.822269	117.092275	48.877786
1326.280405	122.958649	48.882791
1323.256525	110.877833	48.887796
1319.278591	116.151230	48.892801
1315.536194	108.542642	48.897805
1312.303398	122.140476	48.902810
1308.906644	121.748245	48.907815
1305.430983	117.125682	48.912820
1301.712473	121.336562	48.917825
1298.271752	132.037254	48.922829
1295.041592	128.401340	48.927834
1291.580276	121.005026	48.932839
1287.813504	123.062576	48.937844
1284.148062	129.157122	48.942849
1280.510487	121.048070	48.947853
1277.272576	117.524112	48.952858
1274.081512	129.508204	48.957863
1270.669092	123.347626	48.962868
1266.751604	116.288497	48.967873
1263.225810	120.668542	48.972877
1260.253381	124.414622	48.977882
1256.100093	124.985581	48.982887
1253.159602	114.217379	48.987892
1249.444316	114.321133	48.992897
1245.875430	115.376426	48.997901
1242.543778	118.498523	49.002906
1238.635117	122.463940	49.007911
1235.506346	112.819902	49.012916
1231.409281	123.534770	49.017921
1228.432765	122.589551	49.022925
1225.280027	112.477860	49.027930
1221.038789	119.668658	49.032935
1218.136765	113.595886	49.037940
1214.005070	115.384717	49.042945
1210.910067	117.419388	49.047949
1207.697619	120.801251	49.052954
1203.667285	127.199724	49.057959
1200.639200	116.410452	49.062964
1197.203227	122.760172	49.067969
1193.366994	122.841751	49.072973
1189.775993	121.825061	49.077978
1186.138714	119.958222	49.082983
1183.047961	121.672691	49.087988
1179.376009	130.346804	49.092993
1175.691037	120.369073	49.097997
1172.577884	114.190161	49.103002
1168.841132	123.548311	49.108007
1165.559144	116.500472	49.113012
1162.152639	117.682237	49.118017
1158.174709	119.345776	49.123021
1154.837521	117.893887	49.128026
1150.912802	117.280641	49.133031
1147.698719	115.923379	49.138036
1144.451557	124.375968	49.143041
1140.971821	123.199505	49.148045
1137.686990	119.296957	49.153050
1134.161282	122.822800	49.158055
1130.413797	116.284459	49.163060
1126.729640	126.716415	49.168065
1123.126135	117.311263	49.173069
1120.037697	121.923445	49.178074
1116.133247	124.350632	49.183079
1112.646809	119.027465	49.188084
1109.068476	124.409224	49.193089
1105.763918	123.085123	49.198093
1102.698918	113.665278	49.203098
1098.771386	122.860325	49.208103
1095.560477	121.126089	49.213108
1091.401480	121.349992	49.218113
1088.323014	122.065964	49.223117
1085.007810	118.158699	49.228122
1081.209547	123.676143	49.233127
1078.132773	114.859275	49.238132
1074.334231	121.623308	49.243137
1070.460649	124.823979	49.248141
1067.206038	117.487149	49.253146
1063.794030	114.471426	49.258151
1060.735958	111.859045	49.263156
1056.842383	109.478718	49.268161
1053.141846	116.160971	49.273165
1049.848034	114.563120	49.278170
1046.133191	117.808550	49.283175
1042.806052	117.626981	49.288180
1039.323271	123.034932	49.293185
1035.457317	112.756571	49.298189
1032.365165	114.993334	49.303194
1028.633533	119.731556	49.308199
1025.442499	108.477482	49.313204
1021.798503	109.177613	49.318209
1017.980799	114.185582	49.323213
1014.610527	111.194983	49.328218
1011.183589	114.417494	49.333223
1008.000906	114.146880	49.338228
1004.479354	117.343078	49.343233
1000.566379	115.465694	49.348237
997.429106	104.807505	49.353242
993.571303	113.001392	49.358247
990.360177	109.890970	49.363252
986.691079	113.841116	49.368257
983.024833	122.985799	49.373261
979.890865	113.156015	49.378266
976.395187	115.538235	49.383271
973.178868	116.475148	49.388276
969.299787	117.781593	49.393281
965.937009	116.938067	49.398285
962.708667	112.979284	49.403290
958.707142	120.632530	49.408295
955.219774	117.464130	49.413300
951.539672	120.599749	49.418305
948.216462	125.596760	49.423309
944.880130	116.478894	49.428314
941.149029	113.076575	49.433319
937.550857	113.010249	49.438324
933.827142	119.215272	49.443329
930.659882	112.510240	49.448333
927.357749	112.204572	49.453338
924.054044	127.635950	49.458343
920.595706	114.104697	49.463348
916.463709	122.243469	49.468353
912.905327	112.783893	49.473357
909.327828	116.292610	49.478362
905.705647	127.942486	49.483367
902.406262	125.548279	49.488372
899.526853	130.352426	49.493377
895.767570	116.570907	49.498381
892.508561	104.337265	49.503386
888.580622	109.220169	49.508391
885.180713	110.897715	49.513396
881.289135	122.532828	49.518401
878.045426	118.044962	49.523405
874.860921	110.589667	49.528410
870.979636	120.976630	49.533415
867.620226	117.563598	49.538420
864.190118	124.839497	49.543425
860.586944	115.602097	49.548429
857.573693	106.145778	49.553434
853.634017	116.513414	49.558439
850.312377	121.193827	49.563444
846.139579	110.998411	49.568449
843.287808	117.225119	49.573453
839.733057	108.710990	49.578458
836.199838	118.790356	49.583463
832.864668	110.665796	49.588468
829.280499	105.857935	49.593473
825.279429	105.462429	49.598477
821.862280	110.217916	49.603482
818.086364	111.125447	49.608487
815.453166	99.619601	49.613492
812.030337	107.897295	49.618497
808.503869	104.165594	49.623501
805.040641	100.987150	49.628506
800.850331	116.101793	49.633511
797.619901	113.488018	49.638516
793.762160	112.484776	49.643521
790.000125	115.949664	49.648525
786.985409	104.895881	49.653530
783.870105	115.090154	49.658535
780.725782	102.335559	49.663540
777.027086	105.214720	49.668545
773.058026	110.002865	49.673549
769.923976	101.346960	49.678554
765.891221	102.408628	49.683559
762.422805	110.446701	49.688564
758.842373	95.112310	49.693569
755.630735	104.451624	49.698573
752.164228	107.095113	49.703578
748.638481	108.131177	49.708583
745.269365	100.954789	49.713588
741.026040	116.023968	49.718593
737.696238	112.834145	49.723597
734.576671	104.498694	49.728602
730.988815	106.094992	49.733607
727.776025	107.673686	49.738612
724.197850	103.700177	49.743617
720.471446	101.534267	49.748621
717.065916	107.512360	49.753626
713.288038	99.128150	49.758631
710.132440	107.724699	49.763636
706.681385	110.293018	49.768641
702.964643	109.672702	49.773645
699.826297	105.377219	49.778650
696.028569	98.008543	49.783655
692.657558	98.131367	49.788660
688.953713	114.593573	49.793665
685.229957	105.666215	49.798669
682.230759	106.107307	49.803674
678.573088	109.932385	49.808679
674.954549	102.051593	49.813684
671.178423	112.194355	49.818689
667.738010	107.519076	49.823693
664.555188	103.660850	49.828698
660.871616	112.007899	49.833703
657.509860	105.137283	49.838708
654.021328	114.640218	49.843713
650.762209	106.915122	49.848717
647.160698	101.676615	49.853722
643.069121	109.103625	49.858727
639.611581	103.984945	49.863732
636.230225	100.502677	49.868737
633.039404	104.846287	49.873741
630.011811	99.831124	49.878746
625.909260	104.988249	49.883751
622.508100	104.188826	49.888756
619.201809	109.543959	49.893761
615.234604	109.636794	49.898765
612.004690	105.814437	49.903770
608.074598	110.191577	49.908775
605.195093	110.607621	49.913780
601.251780	111.183945	49.918785
597.855937	107.049053	49.923789
595.054138	102.976153	49.928794
590.841790	99.699980	49.933799
587.617161	100.502280	49.938804
583.973477	106.071618	49.943809
580.249851	107.508901	49.948813
576.713329	100.773261	49.953818
573.441333	98.802006	49.958823
570.091340	106.407131	49.963828
566.498247	110.484731	49.968833
562.807491	106.782025	49.973837
559.430119	104.197682	49.978842
555.851566	103.859508	49.983847
552.073231	110.943261	49.988852
548.825753	111.882033	49.993857
545.546373	100.686306	49.998861
542.306886	97.029994	50.003866
538.243596	103.573076	50.008871
534.662641	109.025039	50.013876
531.274493	100.605187	50.018881
527.464435	102.483140	50.023885
524.261064	110.103282	50.028890
520.716142	112.733825	50.033895
517.460419	98.981221	50.038900
514.307629	106.713667	50.043905
510.197992	110.669707	50.048909
507.116792	103.033868	50.053914
502.975293	109.592379	50.058919
499.533583	106.515092	50.063924
496.434729	105.959439	50.068929
492.791752	108.766704	50.073933
489.375375	99.408481	50.078938
485.743748	105.978888	50.083943
482.585756	95.283044	50.088948
478.930524	98.202965	50.093953
474.977273	108.689911	50.098957
472.150636	100.463716	50.103962
468.244032	115.204995	50.108967
465.014787	102.849828	50.113972
460.964692	106.600407	50.118977
457.657592	107.621317	50.123981
454.459050	105.926506	50.128986
450.952458	99.692443	50.133991
447.316498	93.592543	50.138996
443.645716	103.165211	50.144001
440.304640	98.648479	50.149005
436.915566	101.143909	50.154010
433.111318	102.366085	50.159015
429.900022	107.231829	50.164020
426.460318	103.356982	50.169025
422.584452	102.666792	50.174029
419.709306	104.955179	50.179034
415.722099	97.508748	50.184039
412.145459	101.166204	50.189044
408.889547	103.643951	50.194049
405.197135	102.962999	50.199053
402.087056	102.725516	50.204058
397.895158	97.101864	50.209063
394.369725	102.032642	50.214068
390.645218	109.421236	50.219073
387.456084	101.837155	50.224077
384.325498	97.676623	50.229082
380.729994	104.579934	50.234087
377.555608	104.526541	50.239092
373.960538	106.734718	50.244097
370.270113	111.985584	50.249101
366.443847	110.047442	50.254106
362.837958	107.688799	50.259111
359.975894	104.887774	50.264116
356.278925	102.938876	50.269121
352.688930	119.386505	50.274125
349.418676	107.249788	50.279130
345.760198	114.773591	50.284135
342.287764	108.508912	50.289140
339.094828	109.037413	50.294145
335.247332	115.806208	50.299149
331.719944	104.377340	50.304154
328.370899	111.049073	50.309159
324.660645	98.032160	50.314164
320.748976	108.189939	50.319169
317.220258	106.600684	50.324173
314.223183	102.662876	50.329178
310.310040	105.246773	50.334183
307.146307	101.844444	50.339188
304.000665	101.840360	50.344193
300.263347	98.398170	50.349197
296.999135	91.389048	50.354202
293.404632	101.013090	50.359207
289.728359	102.465218	50.364212
286.089839	101.275995	50.369217
282.242552	102.213907	50.374221
279.090056	97.202625	50.379226
275.423594	107.461215	50.384231
272.144330	97.069202	50.389236
268.403788	104.302160	50.394241
264.874942	97.574952	50.399245
262.005638	101.839839	50.404250
258.061645	103.017540	50.409255
254.651868	98.552777	50.414260
251.094090	98.711350	50.419265
247.779172	99.749380	50.424269
244.739234	100.244455	50.429274
240.471333	106.057236	50.434279
237.304379	96.359499	50.439284
233.386103	101.370857	50.444289
229.525092	99.245230	50.449293
226.703947	98.313969	50.454298
223.047570	103.461477	50.459303
219.567360	93.977339	50.464308
216.033488	103.155307	50.469313
212.227843	100.359782	50.474317
209.086376	97.441228	50.479322
205.416761	107.643387	50.484327
202.256643	103.006655	50.489332
198.639476	109.356598	50.494337
195.026639	112.111799	50.499341
191.739262	100.942800	50.504346
187.839188	103.553175	50.509351
184.756038	97.793904	50.514356
181.148255	95.037000	50.519361
177.387793	96.303044	50.524365
173.889163	100.002152	50.529370
170.454060	106.703236	50.534375
166.739230	97.951911	50.539380
163.469741	105.996972	50.544385
159.998039	103.509826	50.549389
156.636461	99.578561	50.554394
152.935243	106.368798	50.559399
149.586613	99.297031	50.564404
146.017432	100.397078	50.569409
142.540782	102.431767	50.574413
139.180908	95.700292	50.579418
135.525074	103.283862	50.584423
131.652034	95.683651	50.589428
128.642551	98.724006	50.594433
124.864195	110.385915	50.599437
121.462123	95.422558	50.604442
118.010125	110.769771	50.609447
114.280196	98.012320	50.614452
111.305717	101.461653	50.619457
107.400867	97.368748	50.624461
104.102344	94.974719	50.629466
100.237489	103.559167	50.634471
97.174207	102.656393	50.639476
93.415186	103.242033	50.644481
89.520581	110.030954	50.649485
86.432425	95.353796	50.654490
82.973256	96.933346	50.659495
79.733659	98.820187	50.664500
75.981610	97.715281	50.669505
72.299642	95.672408	50.674509
69.067525	92.815568	50.679514
65.367813	99.311367	50.684519
61.873706	98.238821	50.689524
58.536053	92.307504	50.694529
54.755069	96.971554	50.699533
51.536060	90.559740	50.704538
48.093671	97.546744	50.709543
44.594939	95.209417	50.714548
40.652947	92.688437	50.719553
37.252683	94.233467	50.724557
33.960260	90.614127	50.729562
30.435597	90.305690	50.734567
26.696877	89.746053	50.739572
23.571638	95.338767	50.744577
19.888001	102.499623	50.749581
16.279641	91.213325	50.754586
12.827269	100.147632	50.759591
9.593536	94.383552	50.764596
6.059268	94.472103	50.769601
2.527136	96.202323	50.774605