Thu Aug 25 12:58:15 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.362470	96.685923	0.000000
0.242711	109.476781	0.005005
0.438399	123.774807	0.010010
0.657169	108.617520	0.015014
0.474881	110.218376	0.020019
0.415139	103.447637	0.025024
0.224173	94.340443	0.030029
-0.005682	77.535539	0.035034
-0.256374	63.201662	0.040038
-0.347110	65.933457	0.045043
-0.827627	46.592541	0.050048
-1.192455	51.876153	0.055053
-1.450271	34.012643	0.060058
-1.627644	29.857820	0.065062
-1.909937	28.386497	0.070067
-2.592639	15.180210	0.075072
-2.533999	17.578545	0.080077
-3.271572	13.005296	0.085082
-3.701720	2.410687	0.090086
-4.144202	10.914514	0.095091
-4.139549	5.820012	0.100096
-4.443117	13.273851	0.105101
-4.527679	13.729921	0.110106
-4.497161	3.819275	0.115110
-5.040253	10.250779	0.120115
-5.771501	5.258924	0.125120
-5.528722	0.766194	0.130125
-5.570795	6.862932	0.135130
-5.650681	3.537567	0.140134
-6.560309	-0.723981	0.145139
-7.104631	-4.887740	0.150144
-6.887210	-0.438856	0.155149
-7.086094	5.448332	0.160154
-7.250195	3.464945	0.165158
-7.260970	6.089290	0.170163
-7.840735	-3.874429	0.175168
-8.187654	3.747550	0.180173
-8.513023	2.118463	0.185178
-8.373194	-8.340816	0.190182
-8.440015	-3.733502	0.195187
-9.185658	-6.258524	0.200192
-9.446339	-11.944201	0.205197
-9.995907	-3.885512	0.210202
-10.338697	-5.369500	0.215206
-10.415471	-7.202053	0.220211
-10.566141	-1.980485	0.225216
-10.004909	-0.742908	0.230221
-10.644428	4.064871	0.235226
-10.981981	-7.246595	0.240230
-11.483708	-1.251848	0.245235
-11.635339	3.536436	0.250240
-11.396093	-13.825936	0.255245
-11.931024	-3.111978	0.260250
-11.976192	-9.461012	0.265254
-12.513651	3.097820	0.270259
-12.651802	-3.220828	0.275264
-12.838629	-8.797854	0.280269
-14.012048	4.338351	0.285274
-13.798212	0.944820	0.290278
-14.014288	-3.539289	0.295283
-14.235312	-0.698505	0.300288
-14.425566	-0.918740	0.305293
-14.311050	-1.246838	0.310298
-14.658462	-7.823763	0.315302
-15.314772	-8.173456	0.320307
-15.235079	0.093526	0.325312
-15.435356	-7.496713	0.330317
-15.537826	3.937268	0.335322
-15.979634	1.722145	0.340326
-16.941166	3.688696	0.345331
-16.534069	-4.512402	0.350336
-16.849849	-9.654770	0.355341
-17.119406	4.573685	0.360346
-17.268179	2.584733	0.365350
-17.865309	10.059255	0.370355
-18.654893	1.666001	0.375360
-18.261919	-3.144490	0.380365
-18.625835	6.808685	0.385370
-18.524926	4.771120	0.390374
-18.985905	3.425874	0.395379
-18.679849	1.299219	0.400384
-18.932202	-6.450540	0.405389
-19.868137	9.682511	0.410394
-20.038465	2.609598	0.415398
-20.225441	11.269545	0.420403
-20.306537	9.735062	0.425408
-20.116831	7.035012	0.430413
-21.185628	13.223019	0.435418
-21.394538	3.634628	0.440422
-21.406382	14.181215	0.445427
-21.543471	9.178524	0.450432
-21.408660	0.596141	0.455437
-21.872634	2.041806	0.460442
-22.509103	0.401352	0.465446
-23.303322	9.241864	0.470451
-23.277154	6.741445	0.475456
-23.278255	3.514469	0.480461
-23.411144	16.674312	0.485466
-23.184892	4.708187	0.490470
-23.304231	6.191603	0.495475
-24.056828	2.481258	0.500480
-24.175408	-1.622657	0.505485
-24.769984	4.215797	0.510490
-24.988816	2.696568	0.515494
-25.925631	4.583317	0.520499
-25.610393	10.203289	0.525504
-25.455954	3.914725	0.530509
-26.087462	15.937807	0.535514
-26.319537	6.634619	0.540518
-26.310329	21.774866	0.545523
-26.475940	14.489238	0.550528
-26.620911	4.694674	0.555533
-27.444070	17.045179	0.560538
-27.318796	9.106532	0.565542
-27.792702	10.525280	0.570547
-27.671803	7.696805	0.575552
-27.811026	3.542340	0.580557
-28.469846	10.444396	0.585562
-28.903788	2.409874	0.590566
-29.124216	-1.475601	0.595571
-29.407070	5.753525	0.600576
-29.261153	-1.919432	0.605581
-29.670706	17.952980	0.610586
-29.242876	11.501354	0.615590
-29.822656	11.123852	0.620595
-30.583081	7.699473	0.625600
-30.640181	0.377866	0.630605
-30.706423	13.910079	0.635610
-31.279290	0.145596	0.640614
-31.806034	12.158587	0.645619
-32.324007	0.419805	0.650624
-32.213720	12.810713	0.655629
-32.445962	0.432373	0.660634
-32.150016	8.630672	0.665638
-32.204505	12.366022	0.670643
-32.642355	0.383731	0.675648
-33.006758	6.651195	0.680653
-33.351088	3.617203	0.685658
-33.352530	-7.066714	0.690662
-33.847139	0.872634	0.695667
-34.410928	0.457826	0.700672
-35.071969	2.421589	0.705677
-35.256335	8.031254	0.710682
-35.216480	-0.428681	0.715686
-35.278643	9.018468	0.720691
-35.123465	4.877987	0.725696
-34.863912	-0.465260	0.730701
-35.634730	11.152537	0.735706
-35.716886	4.682744	0.740710
-36.096962	13.607066	0.745715
-36.725590	5.802365	0.750720
-37.014347	5.796882	0.755725
-37.471750	15.166757	0.760730
-37.413622	3.144718	0.765734
-37.584678	5.484127	0.770739
-37.970487	5.746952	0.775744
-37.660957	5.821734	0.780749
-38.526670	3.135192	0.785754
-39.012051	-1.784449	0.790758
-39.170030	3.318042	0.795763
-39.695844	9.443117	0.800768
-39.503445	4.104064	0.805773
-39.534882	11.644976	0.810778
-39.477962	-5.030770	0.815782
-40.509544	-6.875069	0.820787
-40.626774	2.406697	0.825792
-40.710420	-6.647654	0.830797
-41.122891	6.900837	0.835802
-40.848474	-1.842624	0.840806
-40.894314	6.447192	0.845811
-41.880262	2.877816	0.850816
-41.918429	4.601615	0.855821
-42.445215	9.689127	0.860826
-42.372616	2.562334	0.865830
-42.424084	5.616999	0.870835
-42.704457	0.639926	0.875840
-43.223636	-5.201401	0.880845
-43.828755	10.060400	0.885850
-43.861315	5.927188	0.890854
-43.873247	6.798987	0.895859
-43.946175	9.939273	0.900864
-44.525788	-5.032706	0.905869
-45.047784	-1.372805	0.910874
-45.075123	2.684156	0.915878
-45.566949	1.691759	0.920883
-45.450157	11.338660	0.925888
-45.200163	-4.041719	0.930893
-45.702424	7.698512	0.935898
-46.199291	-6.340464	0.940902
-46.823863	-5.483406	0.945907
-46.897585	2.029326	0.950912
-46.815518	-1.118931	0.955917
-47.107655	5.023313	0.960922
-47.207669	0.011654	0.965926
-47.670050	-2.032563	0.970931
-48.245206	-1.265505	0.975936
-48.313656	-3.864992	0.980941
-48.589608	2.037432	0.985946
-48.406701	-1.898583	0.990950
-48.560921	2.554746	0.995955
-49.286528	2.889796	1.000960
-49.625396	-3.514460	1.005965
-50.188277	-2.869548	1.010970
-49.881367	-1.234620	1.015974
-50.104176	-5.236779	1.020979
-50.158425	6.594606	1.025984
-50.691871	-2.582259	1.030989
-51.464864	0.876525	1.035994
-51.461736	0.970841	1.040998
-51.293502	0.033210	1.046003
-51.889183	-1.389005	1.051008
-51.508118	-1.578533	1.056013
-51.991847	2.255707	1.061018
-52.581717	2.066450	1.066022
-53.231808	3.886129	1.071027
-53.202031	3.368827	1.076032
-52.932866	-0.258000	1.081037
-53.167701	5.663293	1.086042
-52.987448	-0.040853	1.091046
-53.839980	1.889640	1.096051
-54.179869	-2.885116	1.101056
-54.183199	-3.795865	1.106061
-55.384876	7.250359	1.111066
-55.740862	7.476875	1.116070
-55.316396	-3.286431	1.121075
-55.440912	12.444234	1.126080
-55.696580	7.140585	1.131085
-55.778565	3.986395	1.136090
-55.842926	4.777823	1.141094
-56.128665	-0.777377	1.146099
-56.983644	7.572781	1.151104
-57.196677	2.452279	1.156109
-57.544092	4.604184	1.161114
-57.401675	7.745529	1.166118
-57.632615	16.595864	1.171123
-57.646979	1.775761	1.176128
-58.303023	2.900344	1.181133
-58.405622	7.139941	1.186138
-58.803819	-2.431439	1.191142
-58.918019	4.878828	1.196147
-59.457608	5.681443	1.201152
-59.138633	0.075785	1.206157
-60.207251	11.692787	1.211162
-60.689134	2.242085	1.216166
-60.493321	9.307625	1.221171
-60.735156	10.186973	1.226176
-60.636680	7.618276	1.231181
-60.587261	7.433256	1.236186
-60.469383	10.818892	1.241190
-61.363198	5.219763	1.246195
-61.858775	3.247187	1.251200
-61.828285	-0.842118	1.256205
-61.986127	7.879700	1.261210
-62.567085	3.417963	1.266214
-63.257458	0.849484	1.271219
-63.798262	6.249241	1.276224
-63.514386	-4.343338	1.281229
-63.738491	2.202698	1.286234
-63.514984	2.056839	1.291238
-63.447921	4.703787	1.296243
-63.750376	9.686547	1.301248
-64.596620	4.703227	1.306253
-64.698368	7.034940	1.311258
-65.253298	2.145181	1.316262
-65.359154	12.263566	1.321267
-65.393348	18.042694	1.326272
-65.622865	-1.416579	1.331277
-66.081174	18.893740	1.336282
-66.387126	7.536192	1.341286
-66.303076	3.618829	1.346291
-66.423005	7.190423	1.351296
-66.554724	0.506936	1.356301
-67.793702	16.067376	1.361306
-67.816655	8.145630	1.366310
-67.912537	0.459941	1.371315
-68.251700	6.492495	1.376320
-68.066772	2.546670	1.381325
-68.324080	8.692949	1.386330
-68.273664	6.081163	1.391334
-69.243346	11.165307	1.396339
-69.438013	10.028272	1.401344
-69.424246	5.549280	1.406349
-69.662832	13.872461	1.411354
-69.741618	7.974784	1.416358
-70.370243	5.526344	1.421363
-71.049365	7.065834	1.426368
-70.873129	10.647971	1.431373
-71.208585	-1.432614	1.436378
-70.965823	2.082149	1.441382
-71.213827	3.978032	1.446387
-71.256009	3.892786	1.451392
-72.028223	3.602387	1.456397
-72.534476	3.763863	1.461402
-72.288521	2.602081	1.466406
-72.292563	3.330274	1.471411
-73.360568	4.873750	1.476416
-73.481315	7.521653	1.481421
-74.119201	6.273732	1.486426
-74.183144	7.954113	1.491430
-73.665684	10.062253	1.496435
-74.034312	8.016002	1.501440
-74.132427	6.088716	1.506445
-74.848947	7.501189	1.511450
-75.186927	-2.085952	1.516454
-75.292177	-8.802056	1.521459
-75.559553	-3.486274	1.526464
-75.873375	-2.497570	1.531469
-75.913830	-0.681664	1.536474
-76.279795	-9.543078	1.541478
-76.683517	4.431146	1.546483
-76.858828	8.710610	1.551488
-76.851663	-3.765345	1.556493
-77.197599	5.776884	1.561498
-77.375554	-0.285587	1.566502
-78.178805	7.369929	1.571507
-78.253118	3.882342	1.576512
-78.504002	2.776263	1.581517
-78.836923	7.494876	1.586522
-78.770935	-3.993709	1.591526
-78.806463	-0.251843	1.596531
-78.678177	1.996369	1.601536
-79.098310	-7.517785	1.606541
-79.373601	5.287869	1.611546
-79.472988	-11.221004	1.616550
-80.481382	-5.048791	1.621555
-81.356739	-3.693689	1.626560
-81.384258	-3.335142	1.631565
-81.103583	-1.367074	1.636570
-81.566395	-3.670649	1.641574
-81.352141	-9.332662	1.646579
-81.495492	-1.938738	1.651584
-81.575969	-10.012814	1.656589
-82.384140	-10.256448	1.661594
-82.477401	-12.247767	1.666598
-82.594806	-4.066968	1.671603
-83.051541	-5.026896	1.676608
-82.766295	-8.564492	1.681613
-83.621875	-1.773979	1.686618
-83.779673	-10.664845	1.691622
-83.935538	-3.294271	1.696627
-83.992109	-1.789053	1.701632
-84.522044	0.616079	1.706637
-85.193487	0.604122	1.711642
-85.113272	-0.158366	1.716646
-85.198346	-9.313728	1.721651
-85.493626	3.444436	1.726656
-85.267000	-6.629804	1.731661
-86.047795	-1.208263	1.736666
-86.469254	-7.178792	1.741670
-86.651452	-9.877514	1.746675
-86.852664	-6.239402	1.751680
-86.742254	-9.790732	1.756685
-87.797968	3.731993	1.761690
-88.040597	-8.290364	1.766694
-88.374100	-4.944736	1.771699
-88.583536	-3.054897	1.776704
-88.073007	-1.723960	1.781709
-88.450481	-3.794133	1.786714
-88.788834	-0.596441	1.791718
-88.808605	-6.095234	1.796723
-89.245029	-6.321187	1.801728
-89.633167	-1.192127	1.806733
-90.122110	2.984618	1.811738
-90.388787	-0.336784	1.816742
-90.067893	-2.389834	1.821747
-90.563493	1.825919	1.826752
-90.219722	-0.800194	1.831757
-90.829359	3.234111	1.836762
-90.833328	5.958628	1.841766
-91.105879	8.605007	1.846771
-91.878956	4.847259	1.851776
-92.114727	-0.753733	1.856781
-92.757610	2.763760	1.861786
-92.713805	3.724902	1.866790
-92.622430	-2.019099	1.871795
-93.019903	-4.329748	1.876800
-92.609917	-2.568604	1.881805
-93.936522	-0.063950	1.886810
-93.928193	-7.373656	1.891814
-94.209529	-2.137944	1.896819
-94.497314	-0.916036	1.901824
-94.116530	-0.498080	1.906829
-95.114876	-1.850870	1.911834
-95.667118	0.908936	1.916838
-95.762301	7.270256	1.921843
-95.868649	9.839973	1.926848
-95.815269	-2.567292	1.931853
-95.812632	3.860957	1.936858
-95.693735	1.953453	1.941862
-96.223179	-3.196560	1.946867
-96.849086	0.226524	1.951872
-97.195847	-4.996406	1.956877
-97.432614	-3.453461	1.961882
-97.611426	-10.120071	1.966886
-97.362788	-3.221006	1.971891
-98.209643	-4.758884	1.976896
-98.528870	-2.307673	1.981901
-99.126073	4.103834	1.986906
-98.991830	-3.019958	1.991910
-99.079221	-0.462705	1.996915
-98.959250	1.577951	2.006912
-99.070038	3.045958	2.016909
-98.788322	0.318463	2.026906
-98.112018	-3.909048	2.036902
-97.605768	-5.049804	2.046899
-97.262233	0.012175	2.056896
-96.238566	0.849423	2.066893
-96.101524	1.904794	2.076890
-96.178489	-5.530891	2.086886
-95.370981	-2.654545	2.096883
-94.646993	-4.032159	2.106880
-94.208264	-3.252142	2.116877
-93.721425	-3.068878	2.126874
-92.665805	3.151818	2.136870
-92.706819	4.637402	2.146867
-92.298250	-6.720090	2.156864
-91.359427	4.346656	2.166861
-90.977021	0.941311	2.176858
-90.632657	-0.563720	2.186854
-90.059000	-0.761525	2.196851
-89.542783	2.220653	2.206848
-89.390896	6.827988	2.216845
-88.367152	-5.696620	2.226842
-88.157855	7.375625	2.236838
-87.810354	6.253408	2.246835
-86.883567	8.632726	2.256832
-86.640753	0.342306	2.266829
-86.035424	0.288425	2.276826
-85.247947	-1.498281	2.286822
-85.033738	0.254590	2.296819
-85.230790	-2.863555	2.306816
-84.226512	3.219468	2.316813
-83.762727	-4.896498	2.326810
-82.924103	-5.398749	2.336806
-82.699602	-0.210413	2.346803
-81.446569	2.393386	2.356800
-81.228719	1.804670	2.366797
-81.280484	2.059658	2.376794
-80.939476	1.730413	2.386790
-79.990391	1.176008	2.396787
-79.739727	-2.215030	2.406784
-79.440259	2.065070	2.416781
-78.387448	2.270527	2.426778
-78.017496	-0.835092	2.436774
-76.799094	-3.525622	2.446771
-77.119522	6.807103	2.456768
-76.986791	8.363666	2.466765
-76.188691	0.417061	2.476762
-75.722131	11.231528	2.486758
-74.927372	8.262086	2.496755
-74.171961	4.443498	2.506752
-74.074120	6.100562	2.516749
-73.576186	0.063666	2.526746
-73.208195	5.831407	2.536742
-72.828006	-1.216579	2.546739
-72.080160	3.465270	2.556736
-71.457436	3.022191	2.566733
-71.365863	9.067663	2.576730
-70.190014	7.942367	2.586726
-69.662639	0.725598	2.596723
-69.821181	11.470119	2.606720
-69.078300	2.090808	2.616717
-68.650530	7.966393	2.626714
-68.004792	5.904122	2.636710
-66.815923	1.938422	2.646707
-66.977542	3.179974	2.656704
-66.794273	8.102343	2.666701
-66.434689	6.908542	2.676698
-65.493631	0.681836	2.686694
-65.085799	-3.297699	2.696691
-64.184333	4.914370	2.706688
-64.046907	1.604431	2.716685
-63.818096	13.013690	2.726682
-62.950851	12.484781	2.736678
-62.504182	9.969025	2.746675
-62.152472	8.244264	2.756672
-61.394914	7.523466	2.766669
-61.050520	6.281359	2.776666
-60.303524	7.180971	2.786662
-59.528634	4.407880	2.796659
-59.729357	6.004019	2.806656
-59.483792	10.292568	2.816653
-58.568630	4.890384	2.826650
-58.120328	9.207355	2.836646
-57.142518	8.255642	2.846643
-56.800428	13.568112	2.856640
-56.500603	3.909762	2.866637
-56.339188	3.241191	2.876634
-55.359276	7.969045	2.886630
-55.131286	6.460074	2.896627
-54.244418	9.438033	2.906624
-54.003256	5.604988	2.916621
-53.772593	8.188418	2.926618
-52.562525	9.180200	2.936614
-52.403679	10.438064	2.946611
-52.172042	4.214810	2.956608
-51.718947	-1.238517	2.966605
-50.849626	-4.951405	2.976602
-50.598675	-0.045977	2.986598
-50.078851	6.873236	2.996595
-49.128165	0.423276	3.006592
-49.201919	5.610832	3.016589
-48.782091	6.016843	3.026586
-48.162521	3.454990	3.036582
-47.367347	3.529757	3.046579
-46.652217	2.647714	3.056576
-46.406575	4.671262	3.066573
-46.247486	3.093891	3.076570
-45.254290	-1.056558	3.086566
-44.787451	0.989352	3.096563
-44.789414	-2.301915	3.106560
-43.984245	-1.173831	3.116557
-43.574636	5.968560	3.126554
-42.535068	-0.184880	3.136550
-42.011565	-2.937587	3.146547
-41.753148	0.997320	3.156544
-41.857929	10.117832	3.166541
-41.146783	-1.413788	3.176538
-40.331374	-0.787823	3.186534
-40.189157	4.796717	3.196531
-39.301722	1.632191	3.206528
-38.760111	0.425709	3.216525
-38.737066	1.803053	3.226522
-38.068261	-4.371487	3.236518
-37.867639	1.929330	3.246515
-36.529667	6.170261	3.256512
-36.369758	2.755428	3.266509
-36.347660	6.027276	3.276506
-35.281758	1.330074	3.286502
-34.997767	0.030909	3.296499
-34.456973	2.198280	3.306496
-33.531005	2.018137	3.316493
-33.767893	7.906000	3.326490
-33.332718	1.704707	3.336486
-31.950508	3.318922	3.346483
-31.986863	5.757289	3.356480
-31.657184	1.023387	3.366477
-31.242410	-6.185240	3.376474
-30.046084	7.993152	3.386470
-29.822907	8.448983	3.396467
-29.250339	6.721296	3.406464
-29.315535	4.428295	3.416461
-28.222176	3.018154	3.426458
-27.899259	7.959826	3.436454
-27.649943	3.327213	3.446451
-27.028030	8.656029	3.456448
-26.725237	6.881913	3.466445
-25.393776	6.071197	3.476442
-25.099851	4.235113	3.486438
-24.923930	4.204169	3.496435
-24.745920	-0.005454	3.506432
-23.937271	4.413450	3.516429
-23.425350	11.200858	3.526426
-23.177047	6.460697	3.536422
-22.251441	-0.178568	3.546419
-21.941016	0.599381	3.556416
-21.308492	0.186448	3.566413
-20.578608	7.953406	3.576410
-20.352619	1.306548	3.586406
-20.248151	2.848534	3.596403
-19.103851	2.824252	3.606400
-18.875831	-0.588581	3.616397
-18.691172	3.791875	3.626394
-17.792271	4.921115	3.636390
-17.113037	9.563038	3.646387
-17.300541	10.371488	3.656384
-16.314671	4.014218	3.666381
-15.663529	9.943509	3.676378
-15.599352	6.492990	3.686374
-14.625619	5.982247	3.696371
-14.340319	2.769515	3.706368
-14.200879	4.296517	3.716365
-13.375775	6.137408	3.726362
-13.129172	11.043522	3.736358
-12.152148	5.048770	3.746355
-11.934344	3.639598	3.756352
-11.601331	-0.401074	3.766349
-10.331120	2.884293	3.776346
-10.420942	8.435501	3.786342
-9.952757	6.888896	3.796339
-9.754813	7.240975	3.806336
-9.068990	7.126971	3.816333
-8.155224	2.425098	3.826330
-7.372041	3.863909	3.836326
-7.347311	1.879935	3.846323
-7.169208	0.948989	3.856320
-6.359805	7.227286	3.866317
-5.767057	3.459532	3.876314
-5.870009	6.953714	3.886310
-4.888624	8.611729	3.896307
-4.341511	14.398932	3.906304
-4.154337	17.426339	3.916301
-3.884030	23.209398	3.926298
-3.099644	36.435492	3.936294
-2.644654	39.652193	3.946291
-2.021255	50.752569	3.956288
-1.932769	58.753095	3.966285
-1.396068	74.441415	3.976282
-1.133363	89.862230	3.986278
-0.287462	103.417695	3.996275
0.000000	116.915304	4.001280
0.149069	132.119157	4.006285
0.352736	136.671472	4.011290
0.634819	137.566815	4.016294
0.595041	137.784915	4.021299
0.508231	135.020601	4.026304
0.625284	146.559486	4.031309
0.739407	154.321266	4.036314
1.174245	156.268366	4.041318
0.732576	163.335775	4.046323
1.099501	162.503049	4.051328
1.210362	165.219092	4.056333
1.189852	166.104898	4.061338
1.404756	167.039242	4.066342
1.298373	152.005631	4.071347
0.795572	148.727519	4.076352
0.753084	135.727721	4.081357
0.758613	149.017838	4.086362
1.392048	152.667580	4.091366
1.181314	159.527960	4.096371
1.384361	147.970338	4.101376
1.117074	139.827380	4.106381
0.710031	148.980624	4.111386
1.328613	156.628565	4.116390
1.087696	164.300444	4.121395
1.021544	157.280749	4.126400
0.982450	163.199901	4.131405
1.072731	175.369430	4.136410
1.371678	166.533457	4.141414
1.244463	176.452803	4.146419
1.027990	167.798827	4.151424
1.244349	168.821529	4.156429
1.222212	172.102585	4.161434
1.387433	171.715918	4.166438
1.317637	169.841124	4.171443
1.434184	171.040819	4.176448
1.172349	171.916980	4.181453
1.574084	173.875596	4.186458
1.298235	165.718148	4.191462
1.396993	165.648783	4.196467
1.170625	158.359958	4.201472
1.066645	161.872137	4.206477
0.829196	172.890771	4.211482
1.444289	160.309952	4.216486
1.205447	164.899969	4.221491
1.260676	176.480197	4.226496
1.702074	167.023946	4.231501
1.331534	162.083099	4.236506
1.601036	164.362992	4.241510
1.496117	175.107760	4.246515
1.630498	170.201695	4.251520
1.772723	161.178305	4.256525
1.160768	167.763025	4.261530
1.959698	167.552319	4.266534
1.715385	173.658655	4.271539
1.624967	160.758098	4.276544
1.635509	159.095348	4.281549
1.266492	167.603557	4.286554
1.568092	166.527962	4.291558
1.689702	180.097312	4.296563
1.540410	161.545944	4.301568
1.612935	164.454658	4.306573
1.576650	166.684385	4.311578
1.135066	157.084907	4.316582
1.177364	165.389464	4.321587
1.493226	167.497577	4.326592
1.245729	150.837739	4.331597
1.689743	163.999053	4.336602
1.674824	158.844298	4.341606
1.907162	169.469780	4.346611
2.194033	163.793169	4.351616
1.698037	159.327566	4.356621
1.502502	165.995739	4.361626
1.733991	158.609866	4.366630
1.488779	172.084821	4.371635
1.554473	164.876784	4.376640
1.765653	162.331536	4.381645
1.413486	165.632662	4.386650
1.505115	165.896613	4.391654
1.816639	183.106213	4.396659
1.921465	182.469578	4.401664
2.210882	186.268141	4.406669
1.480316	184.778454	4.411674
2.076461	178.819260	4.416678
1.813601	184.099589	4.421683
1.775999	178.894598	4.426688
2.267067	179.358560	4.431693
1.948272	180.610646	4.436698
1.665695	172.840232	4.441702
1.856838	177.378702	4.446707
2.036817	177.467456	4.451712
2.219994	187.657721	4.456717
1.974414	187.512591	4.461722
2.390629	178.939816	4.466726
1.806671	178.369971	4.471731
1.688982	175.237161	4.476736
2.198112	178.137581	4.481741
1.789392	189.784183	4.486746
1.758583	187.058544	4.491750
1.690329	185.743499	4.496755
1.823374	181.369160	4.501760
1.933623	182.525549	4.506765
1.541337	192.154237	4.511770
2.035601	187.296187	4.516774
1.718170	196.960606	4.521779
1.870539	194.212593	4.526784
2.158194	201.963024	4.531789
1.966601	209.529116	4.536794
2.257994	201.450458	4.541798
2.234281	208.955444	4.546803
2.381590	215.256702	4.551808
2.334362	204.238138	4.556813
2.226984	209.402364	4.561818
2.363076	204.505514	4.566822
2.539022	208.375645	4.571827
2.336012	208.783839	4.576832
2.568591	200.078472	4.581837
2.224131	198.458684	4.586842
2.084800	191.048639	4.591846
2.273581	198.384284	4.596851
2.511240	202.656040	4.601856
2.834786	192.398815	4.606861
2.151223	186.659107	4.611866
2.280514	188.293410	4.616870
2.436034	186.743985	4.621875
2.357334	181.896613	4.626880
2.230432	188.620482	4.631885
2.371843	197.077205	4.636890
2.481424	209.424071	4.641894
2.688260	207.645137	4.646899
2.429336	199.481858	4.651904
2.374629	196.994084	4.656909
2.231873	209.073597	4.661914
2.872441	195.681991	4.666918
2.496233	204.428630	4.671923
2.285630	200.313775	4.676928
2.515417	204.903145	4.681933
2.467453	212.709330	4.686938
2.691256	204.201492	4.691942
2.627097	212.905570	4.696947
2.469843	210.921087	4.701952
2.517434	212.283451	4.706957
2.474376	215.203955	4.711962
2.607606	208.317519	4.716966
2.837420	207.927059	4.721971
2.707740	211.205988	4.726976
2.938893	210.922888	4.731981
2.951233	212.091456	4.736986
2.930605	203.571294	4.741990
2.253092	194.945247	4.746995
2.395638	206.274529	4.752000
2.710894	207.882861	4.757005
2.498676	211.924545	4.762010
2.436437	219.786754	4.767014
2.687373	216.786009	4.772019
2.390156	215.582767	4.777024
2.502612	210.398549	4.782029
2.476809	215.442426	4.787034
2.828922	214.463319	4.792038
2.596208	217.935566	4.797043
2.799540	218.450940	4.802048
2.856281	212.009928	4.807053
2.508366	217.727544	4.812058
2.843796	234.047582	4.817062
3.097214	236.579946	4.822067
2.876300	241.515193	4.827072
3.337489	232.761336	4.832077
2.652873	228.053180	4.837082
3.241413	224.888805	4.842086
3.216669	226.743402	4.847091
2.872056	217.714002	4.852096
2.811986	211.813320	4.857101
3.061529	222.094448	4.862106
2.751883	211.901619	4.867110
2.721942	232.505745	4.872115
2.965373	232.302980	4.877120
2.903673	229.019017	4.882125
2.757911	241.753931	4.887130
3.273924	229.824513	4.892134
2.913683	249.480647	4.897139
2.940885	244.062999	4.902144
3.367603	239.981159	4.907149
3.813216	260.665835	4.912154
3.086300	238.152046	4.917158
3.268719	241.290331	4.922163
3.498240	239.131347	4.927168
3.081810	222.488419	4.932173
2.936812	223.627854	4.937178
3.196718	230.749885	4.942182
3.253794	237.565170	4.947187
3.081627	238.626604	4.952192
2.926629	236.413970	4.957197
3.183320	246.538965	4.962202
3.056449	245.486205	4.967206
3.441084	237.522638	4.972211
3.260250	244.992144	4.977216
3.364414	248.465400	4.982221
3.030670	254.117531	4.987226
2.884741	236.122390	4.992230
3.009992	247.337347	4.997235
3.123329	241.890384	5.002240
3.434870	239.364203	5.007245
3.053345	246.317815	5.012250
3.176121	240.416950	5.017254
3.329613	248.065033	5.022259
3.041007	242.921497	5.027264
3.361661	255.374531	5.032269
3.928520	264.511287	5.037274
3.833832	262.289200	5.042278
3.708822	246.802838	5.047283
3.705660	241.911977	5.052288
3.152393	239.508639	5.057293
3.105769	243.347210	5.062298
3.245663	238.345349	5.067302
3.626754	247.751652	5.072307
3.753937	256.175832	5.077312
3.667729	247.491915	5.082317
3.601873	249.947752	5.087322
3.305551	238.382891	5.092326
3.481458	256.474366	5.097331
3.341443	242.717801	5.102336
3.445917	250.500118	5.107341
3.577097	261.426248	5.112346
3.257862	257.768171	5.117350
3.752106	261.743470	5.122355
3.494236	269.465507	5.127360
3.359300	268.474122	5.132365
3.462170	265.110582	5.137370
3.786261	261.693400	5.142374
3.704268	264.502951	5.147379
3.592475	265.213235	5.152384
4.051798	269.621123	5.157389
3.522236	273.576498	5.162394
3.705084	260.860848	5.167398
3.806364	271.816980	5.172403
3.601605	278.505623	5.177408
4.019862	271.210665	5.182413
3.526743	272.762159	5.187418
3.825724	269.864611	5.192422
3.522915	266.131190	5.197427
3.686630	265.975717	5.202432
3.738552	261.247065	5.207437
3.505328	279.446960	5.212442
4.181209	283.273581	5.217446
4.122388	274.015873	5.222451
3.928498	275.033255	5.227456
3.765009	270.518690	5.232461
3.667563	272.957333	5.237466
4.149280	280.136381	5.242470
3.867193	274.162894	5.247475
4.056299	271.428097	5.252480
4.031566	270.046114	5.257485
3.809978	277.828910	5.262490
4.194127	275.123665	5.267494
3.964275	277.367915	5.272499
3.992657	273.873673	5.277504
4.134744	286.766003	5.282509
4.116644	284.759709	5.287514
3.894451	276.182507	5.292518
3.684435	279.031102	5.297523
4.045976	288.120944	5.302528
4.611122	297.903405	5.307533
4.337888	296.503407	5.312538
4.130225	282.004421	5.317542
4.118210	270.398157	5.322547
3.551838	274.277040	5.327552
4.187401	283.545413	5.332557
3.961349	290.829031	5.337562
4.506490	290.917522	5.342566
4.269260	293.134456	5.347571
4.131808	289.248569	5.352576
4.602405	283.321667	5.357581
4.263547	299.196909	5.362586
4.456975	297.673173	5.367590
4.430214	293.921806	5.372595
4.017873	291.376155	5.377600
4.196828	284.520491	5.382605
4.445864	289.179635	5.387610
4.112999	283.429240	5.392614
4.380395	301.712076	5.397619
4.166852	289.976020	5.402624
4.269703	293.933555	5.407629
4.359970	297.567189	5.412634
4.600049	296.573993	5.417638
4.069905	295.691985	5.422643
4.255542	289.183292	5.427648
4.392922	298.422159	5.432653
4.023124	298.198412	5.437658
3.983934	292.310251	5.442662
4.019511	293.921282	5.447667
4.251556	297.643436	5.452672
4.490699	296.808578	5.457677
4.586903	289.209725	5.462682
4.626019	291.883243	5.467686
4.564444	297.774324	5.472691
4.296870	298.338171	5.477696
4.351102	296.915340	5.482701
4.162663	304.382900	5.487706
4.583737	312.451004	5.492710
4.632798	312.803886	5.497715
4.068084	317.862625	5.502720
4.554202	320.099108	5.507725
4.527546	324.276262	5.512730
4.868934	325.475541	5.517734
4.874516	327.948671	5.522739
4.392251	325.568998	5.527744
4.591126	316.577783	5.532749
4.674194	326.040313	5.537754
4.626364	320.722985	5.542758
4.828286	314.850824	5.547763
4.761140	323.099834	5.552768
4.727787	317.106344	5.557773
4.683930	326.550795	5.562778
4.788271	323.459103	5.567782
4.719881	326.911953	5.572787
4.479157	325.832733	5.577792
4.788163	317.241887	5.582797
4.611906	325.621891	5.587802
4.909110	315.140929	5.592806
4.870470	315.437948	5.597811
4.449190	323.055894	5.602816
4.489800	319.528089	5.607821
4.677386	335.045627	5.612826
4.975374	332.208337	5.617830
5.182124	336.174913	5.622835
4.696317	327.167579	5.627840
4.841366	332.425171	5.632845
4.912500	350.542649	5.637850
4.817076	339.724547	5.642854
5.240065	337.538403	5.647859
5.168324	341.267033	5.652864
4.935808	323.984576	5.657869
4.841291	322.705274	5.662874
5.141351	323.651595	5.667878
4.797105	334.019494	5.672883
4.914411	341.847299	5.677888
4.982141	336.995925	5.682893
4.963415	346.737013	5.687898
4.839278	345.997038	5.692902
4.960355	350.138395	5.697907
4.862295	347.590952	5.702912
5.296599	344.412755	5.707917
5.205983	354.399235	5.712922
5.271721	351.174378	5.717926
5.246906	349.529804	5.722931
4.799722	353.681102	5.727936
5.741053	341.852654	5.732941
5.167471	347.931542	5.737946
5.275401	347.088766	5.742950
5.237002	348.616477	5.747955
5.326281	345.226578	5.752960
5.302562	345.030866	5.757965
5.242264	346.868900	5.762970
5.548410	339.714870	5.767974
5.329719	338.271521	5.772979
5.223311	348.561035	5.777984
5.285906	344.982322	5.782989
5.164929	349.063526	5.787994
5.296650	351.197349	5.792998
5.244144	348.804123	5.798003
4.976780	353.658091	5.803008
5.475031	347.271244	5.808013
5.255372	352.263273	5.813018
5.361982	349.133256	5.818022
5.378021	348.902840	5.823027
5.122012	353.755029	5.828032
5.682100	345.165961	5.833037
5.104399	350.913294	5.838042
4.764875	347.552613	5.843046
5.364197	344.259974	5.848051
5.443342	349.999307	5.853056
5.710168	343.506349	5.858061
5.366579	344.417473	5.863066
5.307607	348.099811	5.868070
5.517395	347.279041	5.873075
5.131094	349.848376	5.878080
5.510754	346.273772	5.883085
5.199007	370.908635	5.888090
5.676964	374.690354	5.893094
5.998498	384.536343	5.898099
5.862462	373.101308	5.903104
5.671094	353.645149	5.908109
5.463970	351.348916	5.913114
5.387587	352.790828	5.918118
5.536943	363.786941	5.923123
5.448068	375.861288	5.928128
5.881810	368.026014	5.933133
5.840483	374.768182	5.938138
5.855578	367.855900	5.943142
5.817831	368.080013	5.948147
5.497832	359.730072	5.953152
5.706911	365.468034	5.958157
5.696928	375.505168	5.963162
6.042936	372.179446	5.968166
5.960770	365.693702	5.973171
5.437836	367.521964	5.978176
5.780588	371.350177	5.983181
5.931874	376.989629	5.988186
6.047067	372.975552	5.993190
5.699769	368.878912	5.998195
5.657712	369.581438	6.003200
5.821516	371.178713	6.008205
5.483940	381.700623	6.013210
5.760549	377.705548	6.018214
5.995861	380.680543	6.023219
5.689592	375.292957	6.028224
6.024683	368.735508	6.033229
5.638862	379.128931	6.038234
6.051907	373.055989	6.043238
6.018659	375.421311	6.048243
6.092787	376.412525	6.053248
5.857866	370.365176	6.058253
5.874824	375.794713	6.063258
5.844591	377.915948	6.068262
5.778846	369.864696	6.073267
5.746763	377.826656	6.078272
5.429768	363.898405	6.083277
5.550853	377.879286	6.088282
5.902587	365.244671	6.093286
6.025319	376.358861	6.098291
5.943240	370.341349	6.103296
6.241426	370.753279	6.108301
5.865284	376.570282	6.113306
5.793434	382.013736	6.118310
6.125456	372.384684	6.123315
5.691908	369.399408	6.128320
5.724170	362.430653	6.133325
5.902607	368.825167	6.138330
6.015559	371.648485	6.143334
5.840205	369.223883	6.148339
5.599259	367.515092	6.153344
5.937684	359.432158	6.158349
5.607751	373.306526	6.163354
5.843062	362.572635	6.168358
5.867833	367.801625	6.173363
5.609998	373.517831	6.178368
5.870788	368.813375	6.183373
5.764825	375.641603	6.188378
5.790529	368.079073	6.193382
5.887322	367.443689	6.198387
5.865252	374.233462	6.203392
6.018977	371.137188	6.208397
5.685861	378.738180	6.213402
5.903678	377.283385	6.218406
5.718536	379.011265	6.223411
5.781105	366.700373	6.228416
5.751131	365.945643	6.233421
5.912369	370.318001	6.238426
5.850928	375.082761	6.243430
5.989488	371.681972	6.248435
6.021196	372.034410	6.253440
6.185031	367.142660	6.258445
6.058545	381.383801	6.263450
5.839377	364.181473	6.268454
5.527630	351.967205	6.273459
5.572577	371.901682	6.278464
5.827738	366.884889	6.283469
5.672896	382.351713	6.288474
6.097362	362.435214	6.293478
6.033624	367.722365	6.298483
5.895212	374.751834	6.303488
6.063081	362.433938	6.308493
5.870162	374.572044	6.313498
5.625459	360.667270	6.318502
5.808139	366.074003	6.323507
5.591016	367.920791	6.328512
5.565339	371.854187	6.333517
5.479615	375.268633	6.338522
5.804432	374.907578	6.343526
5.727738	373.543221	6.348531
5.601898	384.136364	6.353536
6.296955	378.547595	6.358541
5.980378	378.992569	6.363546
5.801013	374.948711	6.368550
6.002929	372.518783	6.373555
5.948363	379.816699	6.378560
6.099645	379.248710	6.383565
5.635185	377.673017	6.388570
5.550762	378.271447	6.393574
5.727213	380.711485	6.398579
5.890442	380.030890	6.403584
5.940955	372.122777	6.408589
5.647026	374.402390	6.413594
6.132820	375.582211	6.418598
6.045069	377.693475	6.423603
5.743479	375.586051	6.428608
5.790999	376.663694	6.433613
5.670964	382.073568	6.438618
5.954836	385.404796	6.443622
5.855457	382.066595	6.448627
5.834152	380.899208	6.453632
5.869940	373.733739	6.458637
5.765310	380.681985	6.463642
5.976072	376.627624	6.468646
5.754367	371.356506	6.473651
5.767921	385.521924	6.478656
6.036739	375.472491	6.483661
5.795566	374.858422	6.488666
5.389691	374.371401	6.493670
5.933747	381.354056	6.498675
5.579556	381.187976	6.503680
5.906586	373.828175	6.508685
6.004243	374.252540	6.513690
5.679831	374.084958	6.518694
5.435719	377.207837	6.523699
5.694088	382.270513	6.528704
5.541559	371.901112	6.533709
5.682058	376.618414	6.538714
5.917505	371.826176	6.543718
5.644129	374.134207	6.548723
5.556831	388.195202	6.553728
6.127187	391.209456	6.558733
5.756751	396.965458	6.563738
5.890679	390.616695	6.568742
6.388519	388.058140	6.573747
5.492699	385.619865	6.578752
6.204847	382.698694	6.583757
6.006743	378.426811	6.588762
5.934058	374.616182	6.593766
6.215612	383.228212	6.598771
6.214077	376.584294	6.603776
6.051051	371.354604	6.608781
5.613934	380.433582	6.613786
5.996307	376.576965	6.618790
5.973226	375.533246	6.623795
5.960657	379.388658	6.628800
6.288361	377.109868	6.633805
6.032445	372.774277	6.638810
6.025277	379.109288	6.643814
6.089302	367.101896	6.648819
5.567510	364.930896	6.653824
5.822471	353.675063	6.658829
5.748955	358.808716	6.663834
5.546808	356.840741	6.668838
5.884280	368.873594	6.673843
5.769953	373.149919	6.678848
6.043362	371.914210	6.683853
5.968811	380.404858	6.688858
5.627558	369.786609	6.693862
6.102562	374.549579	6.698867
5.942813	366.623791	6.703872
5.609905	355.811250	6.708877
5.816626	372.050338	6.713882
6.000524	371.594301	6.718886
5.669000	371.940375	6.723891
6.160658	373.388203	6.728896
6.184321	362.193915	6.733901
5.713687	359.467557	6.738906
5.467136	360.828561	6.743910
5.754118	356.654692	6.748915
5.827703	370.086175	6.753920
6.051508	378.080811	6.758925
5.631040	371.214625	6.763930
5.495102	379.294100	6.768934
6.278071	379.127025	6.773939
6.164479	376.148565	6.778944
6.423496	354.638115	6.783949
5.793807	358.308632	6.788954
5.605810	364.032877	6.793958
5.725991	354.541432	6.798963
5.483727	355.253179	6.803968
5.323080	349.124595	6.808973
5.769087	376.317340	6.813978
5.737537	379.356294	6.818982
5.856624	373.554041	6.823987
5.808473	386.444611	6.828992
6.148527	382.604115	6.833997
6.115359	382.023896	6.839002
5.719927	383.999865	6.844006
5.853844	378.315513	6.849011
6.032405	386.820292	6.854016
5.987492	367.954955	6.859021
5.110872	363.969724	6.864026
5.478146	368.240195	6.869030
5.903812	377.845232	6.874035
5.390474	382.975035	6.879040
5.659234	378.183904	6.884045
5.454058	380.987463	6.889050
5.531700	379.235083	6.894054
5.651576	372.069095	6.899059
5.363658	386.965136	6.904064
5.813584	391.323905	6.909069
5.862089	399.643418	6.914074
6.205065	406.882221	6.919078
6.141678	390.044612	6.924083
5.892684	383.863417	6.929088
5.969239	375.074841	6.934093
5.762698	380.178720	6.939098
5.644526	379.934531	6.944102
5.822530	373.483953	6.949107
5.571174	381.454960	6.954112
5.629651	383.540149	6.959117
5.884165	399.743301	6.964122
6.031497	403.434456	6.969126
6.183715	394.355597	6.974131
5.646772	387.994885	6.979136
6.198394	372.348614	6.984141
6.050171	379.503011	6.989146
5.723506	377.842453	6.994150
5.557460	377.153336	6.999155
5.697038	388.211109	7.004160
5.862832	375.545507	7.009165
5.561848	380.797066	7.014170
5.844621	394.252740	7.019174
5.840944	401.748340	7.024179
5.659158	401.688128	7.029184
5.814397	401.135338	7.034189
6.057637	402.394294	7.039194
6.150065	400.421291	7.044198
6.153691	376.600098	7.049203
5.685772	375.300201	7.054208
6.190579	381.086749	7.059213
6.155067	377.697413	7.064218
5.665780	382.070455	7.069222
5.994648	373.821328	7.074227
5.761891	370.086401	7.079232
6.028448	371.629611	7.084237
6.105232	384.234843	7.089242
6.256444	379.952523	7.094246
6.203068	384.867887	7.099251
6.213487	378.952941	7.104256
6.253513	376.165554	7.109261
5.682713	361.679106	7.114266
5.390730	359.639783	7.119270
6.034135	367.805958	7.124275
5.930717	369.116063	7.129280
6.112207	370.476443	7.134285
5.953269	363.926796	7.139290
5.954928	362.891857	7.144294
5.660492	352.259956	7.149299
5.792974	346.661262	7.154304
5.520247	348.741392	7.159309
6.034978	356.101964	7.164314
5.925906	365.936314	7.169318
5.941118	358.147636	7.174323
5.441595	361.569963	7.179328
5.758421	369.477253	7.184333
5.880465	374.684676	7.189338
5.789961	381.874325	7.194342
6.174765	383.440138	7.199347
5.793536	382.076037	7.204352
5.900256	371.871666	7.209357
5.834425	380.487501	7.214362
5.712959	368.192787	7.219366
6.015204	369.698766	7.224371
6.093508	367.696341	7.229376
5.928708	360.872360	7.234381
5.931361	361.276809	7.239386
5.735020	348.338927	7.244390
5.508705	347.788971	7.249395
5.658981	362.730234	7.254400
5.967813	373.986112	7.259405
6.059821	380.780160	7.264410
5.796894	364.331352	7.269414
5.621497	354.709044	7.274419
5.482140	373.909917	7.279424
5.614091	369.159207	7.284429
5.729258	379.122949	7.289434
5.647811	379.553230	7.294438
5.825378	376.760112	7.299443
5.694652	375.486479	7.304448
6.064253	376.608574	7.309453
5.870815	386.785192	7.314458
5.884044	379.104386	7.319462
5.890115	378.457907	7.324467
6.068483	380.492673	7.329472
6.188292	376.031772	7.334477
5.935038	377.941171	7.339482
5.863259	385.172181	7.344486
6.081789	381.221008	7.349491
5.841005	373.402829	7.354496
6.068693	351.565089	7.359501
5.782636	356.738369	7.364506
5.632761	351.130129	7.369510
5.695011	349.955980	7.374515
5.818507	374.968755	7.379520
5.948298	372.822217	7.384525
5.915756	373.991500	7.389530
5.637403	369.969480	7.394534
6.406014	374.097976	7.399539
5.947462	368.414703	7.404544
6.208525	353.095555	7.409549
5.756766	353.324422	7.414554
5.773643	349.490274	7.419558
5.992366	347.295003	7.424563
5.697349	358.392376	7.429568
5.705895	353.224396	7.434573
5.779502	352.045304	7.439578
5.645726	354.514961	7.444582
5.575053	352.035994	7.449587
5.553173	355.231620	7.454592
6.080473	363.162878	7.459597
6.054240	379.992144	7.464602
5.459467	365.677132	7.469606
5.633867	366.864612	7.474611
5.427144	371.047842	7.479616
5.791725	363.568264	7.484621
5.820895	377.566709	7.489626
5.845606	370.488400	7.494630
6.021309	370.568335	7.499635
5.699659	382.229893	7.504640
5.942453	372.599002	7.509645
5.810362	382.838775	7.514650
5.572068	382.679846	7.519654
6.129596	371.718291	7.524659
5.726301	385.778173	7.529664
6.158361	375.310849	7.534669
6.028814	379.605379	7.539674
6.053848	380.452422	7.544678
6.348481	375.331363	7.549683
5.955078	368.321728	7.554688
5.863320	366.023238	7.559693
5.727772	358.539762	7.564698
5.370469	354.099835	7.569702
5.991908	356.495459	7.574707
5.773503	381.042944	7.579712
5.877494	372.439900	7.584717
5.882569	373.356510	7.589722
5.657910	374.850130	7.594726
6.301096	381.741322	7.599731
5.889463	367.701342	7.604736
5.975637	352.529821	7.609741
5.659040	353.870161	7.614746
5.430318	352.991544	7.619750
5.903682	354.179639	7.624755
5.696255	374.767445	7.629760
6.153376	374.806451	7.634765
6.157270	378.728888	7.639770
5.676817	363.076647	7.644774
6.108268	350.185938	7.649779
5.613788	350.592345	7.654784
5.689790	344.407701	7.659789
5.686414	350.229568	7.664794
6.008460	366.763802	7.669798
5.939665	351.531139	7.674803
5.771889	351.089073	7.679808
5.637750	344.858258	7.684813
5.584624	359.986416	7.689818
5.741263	370.342298	7.694822
5.713303	374.772774	7.699827
5.785030	373.926178	7.704832
6.189294	383.702255	7.709837
5.392197	375.987056	7.714842
5.476899	374.897975	7.719846
5.601858	371.062708	7.724851
5.602189	369.898259	7.729856
5.564708	369.160525	7.734861
5.839812	376.960457	7.739866
5.516661	372.344328	7.744870
5.936147	366.457045	7.749875
5.885501	379.411278	7.754880
5.576369	373.748886	7.759885
5.684542	383.346722	7.764890
5.744299	374.304508	7.769894
5.925627	376.202765	7.774899
5.768244	376.398164	7.779904
6.009706	374.142378	7.784909
5.966903	389.835270	7.789914
6.137956	383.575607	7.794918
6.284529	378.503056	7.799923
5.813396	379.987836	7.804928
5.817841	371.881292	7.809933
5.872616	368.946059	7.814938
5.738532	376.958802	7.819942
5.883780	367.466587	7.824947
5.791648	371.913445	7.829952
5.790375	367.743607	7.834957
5.580130	368.902766	7.839962
5.801991	383.355091	7.844966
5.801993	373.850828	7.849971
5.600720	382.772630	7.854976
5.645777	383.635518	7.859981
5.877307	378.321860	7.864986
5.572149	382.064924	7.869990
6.038135	388.797216	7.874995
5.833668	403.465055	7.880000
5.902843	394.010056	7.885005
5.873998	395.283167	7.890010
5.602652	388.602423	7.895014
5.048289	403.372541	7.900019
5.297080	408.525314	7.905024
6.144127	404.671817	7.910029
5.709745	405.065645	7.915034
6.178439	405.953911	7.920038
6.306606	410.271346	7.925043
5.891976	413.794281	7.930048
5.889455	412.978299	7.935053
6.204057	413.552177	7.940058
6.276909	403.384732	7.945062
5.816517	387.030119	7.950067
5.751340	384.056728	7.955072
5.952326	382.629880	7.960077
5.922911	382.257886	7.965082
6.144011	376.809818	7.970086
5.951970	377.978780	7.975091
5.711723	378.297897	7.980096
5.885101	377.672661	7.985101
5.716156	372.070566	7.990106
5.760434	380.273669	7.995110
5.941601	375.853777	8.000115
5.596966	374.004799	8.005133
5.681259	381.631587	8.010150
5.847533	376.373173	8.015168
5.665287	377.941633	8.020186
6.151685	378.417576	8.025203
5.605859	383.596391	8.030221
5.480023	389.018669	8.035238
5.427825	404.439502	8.040256
5.846107	399.255204	8.045274
5.674269	396.034738	8.050291
5.828194	402.227374	8.055309
5.969676	392.917680	8.060326
6.262689	399.583978	8.065344
5.919675	407.495475	8.070362
5.935244	402.989649	8.075379
6.126145	412.584724	8.080397
5.978042	396.724845	8.085414
6.584731	405.566814	8.090432
6.473084	394.791478	8.095450
6.060758	385.761060	8.100467
5.750620	385.191016	8.105485
5.780488	375.378117	8.110502
5.887833	379.211222	8.115520
5.772934	382.631030	8.120538
5.888829	380.261722	8.125555
5.746454	395.898645	8.130573
6.317031	396.402424	8.135590
6.327975	389.391648	8.140608
5.831426	382.132189	8.145626
5.979082	377.356368	8.150643
5.740171	381.351021	8.155661
6.054167	386.436145	8.160678
5.845865	382.208394	8.165696
6.037365	394.665643	8.170714
6.133312	401.848806	8.175731
5.987268	400.246362	8.180749
6.323693	395.308418	8.185766
6.048444	387.783912	8.190784
5.904859	385.751900	8.195802
6.152061	387.881072	8.200819
5.872488	381.524879	8.205837
5.730524	389.714133	8.210854
5.828338	396.369989	8.215872
5.601000	403.928849	8.220890
5.910527	403.422659	8.225907
6.025227	408.785165	8.230925
6.255335	411.339891	8.235942
6.273455	411.131820	8.240960
6.306806	406.746282	8.245978
6.174819	401.392583	8.250995
6.192361	410.247968	8.256013
6.345629	405.146216	8.261030
6.397744	407.252308	8.266048
5.978475	416.169824	8.271066
5.964692	409.251275	8.276083
6.117095	414.213405	8.281101
6.452652	399.685216	8.286118
6.481845	397.632443	8.291136
6.164010	389.376159	8.296154
6.121022	386.163908	8.301171
5.914085	388.392636	8.306189
5.989233	390.375199	8.311206
6.070131	398.595810	8.316224
6.286426	406.337624	8.321242
6.423041	394.582971	8.326259
5.885472	394.572418	8.331277
6.010435	399.068633	8.336294
6.485889	397.286763	8.341312
6.223217	408.199429	8.346330
6.440271	391.133642	8.351347
6.181342	379.601918	8.356365
5.714724	378.510444	8.361382
6.343976	393.938106	8.366400
5.966195	393.602719	8.371418
6.534354	392.961335	8.376435
6.246717	405.083413	8.381453
6.415561	401.310956	8.386470
6.528847	392.621054	8.391488
6.566892	393.378682	8.396506
6.282083	381.254572	8.401523
6.377571	379.525924	8.406541
6.287276	379.255946	8.411558
6.121938	385.044169	8.416576
6.172365	391.593840	8.421594
6.396863	368.613005	8.426611
6.251035	381.965687	8.431629
6.061924	383.800307	8.436646
5.920095	384.668166	8.441664
6.116632	402.009755	8.446682
6.452521	397.289643	8.451699
6.028499	406.523475	8.456717
6.464498	410.570177	8.461734
6.281067	406.600452	8.466752
6.234259	409.103892	8.471770
6.338057	407.850461	8.476787
6.101509	407.972622	8.481805
6.172627	400.920855	8.486822
6.346976	403.020419	8.491840
5.962580	401.168144	8.496858
6.442714	409.045344	8.501875
6.461870	408.048169	8.506893
6.023466	404.377167	8.511910
6.475308	403.877081	8.516928
6.155055	411.141237	8.521946
6.186998	404.442742	8.526963
6.319714	399.416794	8.531981
6.325374	410.880704	8.536998
6.358049	399.940743	8.542016
6.522553	408.268178	8.547034
6.233303	400.966765	8.552051
6.168597	402.510499	8.557069
6.423834	404.382797	8.562087
6.571009	415.101866	8.567104
6.210052	412.955587	8.572122
6.305580	418.627210	8.577139
6.725590	423.881925	8.582157
6.596638	431.901903	8.587175
6.807118	414.521546	8.592192
6.338647	413.499788	8.597210
6.359282	409.116241	8.602227
6.455253	405.781230	8.607245
6.574923	414.241923	8.612263
6.682224	402.135256	8.617280
6.325665	405.510883	8.622298
6.661803	402.002545	8.627315
6.242638	399.597147	8.632333
6.453071	399.406281	8.637351
6.636987	403.527192	8.642368
6.459899	410.589038	8.647386
6.478360	416.967004	8.652403
6.670460	412.626018	8.657421
6.315837	421.530252	8.662439
6.473414	421.701114	8.667456
6.734786	423.698683	8.672474
6.567642	424.336984	8.677491
6.447748	425.567478	8.682509
6.350594	433.885430	8.687527
6.960346	424.423456	8.692544
6.881789	430.807161	8.697562
6.510581	422.022743	8.702579
6.409629	414.644485	8.707597
6.436874	426.531052	8.712615
6.682454	431.263994	8.717632
6.661605	433.990586	8.722650
7.161131	427.446037	8.727667
7.047387	414.026481	8.732685
6.392890	420.500420	8.737703
6.383242	403.388091	8.742720
6.253006	401.155172	8.747738
6.104678	418.440358	8.752755
6.876355	425.536592	8.757773
6.189744	427.218794	8.762791
6.505952	431.729234	8.767808
6.648696	436.137466	8.772826
6.472838	432.620980	8.777843
6.650583	427.928794	8.782861
6.585615	428.715186	8.787879
6.888865	428.159487	8.792896
6.760332	430.426428	8.797914
6.893875	432.936327	8.802931
6.676260	430.234262	8.807949
6.642883	428.314364	8.812967
6.925923	429.500661	8.817984
6.496038	433.575739	8.823002
6.507315	435.514666	8.828019
6.576514	440.423568	8.833037
6.559754	435.184348	8.838055
6.884339	432.558274	8.843072
6.898693	436.251329	8.848090
6.619206	431.217374	8.853107
7.013429	431.420585	8.858125
6.747241	437.824222	8.863143
6.858772	427.944852	8.868160
6.689063	433.285656	8.873178
6.594471	428.999052	8.878195
6.652561	421.507510	8.883213
6.381498	438.089274	8.888231
6.687421	432.827899	8.893248
6.514362	447.860611	8.898266
6.549840	459.307257	8.903283
6.958104	459.849093	8.908301
6.754773	470.676761	8.913319
6.938902	458.772612	8.918336
7.540005	467.041136	8.923354
6.815965	457.674515	8.928371
7.024640	443.475437	8.933389
6.781063	445.473230	8.938407
6.734060	444.947161	8.943424
6.787834	446.087331	8.948442
6.913705	451.334492	8.953459
7.024944	444.816060	8.958477
6.574258	450.106218	8.963495
6.673093	449.162828	8.968512
7.079238	462.703639	8.973530
6.701284	458.436179	8.978547
7.098378	456.316289	8.983565
6.971591	463.853109	8.988583
7.076303	455.644198	8.993600
7.257333	456.136431	8.998618
7.070377	449.172417	9.003635
7.020887	439.517083	9.008653
6.665557	442.141449	9.013671
6.866871	449.289188	9.018688
6.859227	453.171883	9.023706
6.869201	460.068741	9.028723
7.051208	457.963616	9.033741
6.884668	466.368193	9.038759
7.095848	462.333472	9.043776
7.071692	447.953121	9.048794
7.019811	460.603183	9.053811
7.330444	456.395092	9.058829
7.112654	458.956886	9.063847
7.066678	441.847056	9.068864
7.085814	437.470049	9.073882
6.354463	444.224278	9.078899
7.142459	447.105006	9.083917
7.034100	457.958811	9.088935
6.927358	459.808935	9.093952
7.373167	451.720151	9.098970
6.987481	457.359886	9.103987
7.075702	451.148012	9.109005
7.290022	460.919324	9.114023
7.029503	450.214616	9.119040
7.186894	454.393343	9.124058
7.195999	460.889554	9.129075
7.184047	456.719382	9.134093
7.233235	460.406984	9.139111
7.046218	446.727488	9.144128
6.907851	448.361661	9.149146
6.924730	457.261354	9.154163
7.271465	454.997877	9.159181
7.369448	449.349358	9.164199
7.561975	448.217721	9.169216
7.043325	445.190438	9.174234
6.898130	437.617132	9.179251
6.815537	442.455144	9.184269
6.886577	452.226809	9.189287
7.297600	457.082159	9.194304
7.202825	458.289785	9.199322
6.835806	448.179273	9.204339
7.354092	448.779608	9.209357
6.929226	455.208113	9.214375
6.898603	456.967416	9.219392
6.951798	453.067903	9.224410
7.002558	458.740241	9.229427
7.368668	450.850135	9.234445
7.184068	453.062748	9.239463
7.012189	456.759740	9.244480
7.325483	459.623328	9.249498
7.283738	456.701201	9.254515
7.008920	462.841114	9.259533
7.139545	469.479233	9.264551
7.325078	471.009012	9.269568
7.216971	471.527612	9.274586
7.106461	485.187259	9.279603
7.315878	483.611164	9.284621
7.129076	491.296253	9.289639
7.186024	490.147986	9.294656
7.510849	489.396402	9.299674
7.214326	487.659737	9.304691
7.428261	482.816700	9.309709
7.494688	483.011311	9.314727
7.137381	480.185959	9.319744
7.511920	486.637547	9.324762
7.618203	484.263419	9.329779
7.508566	479.934979	9.334797
7.550402	485.719176	9.339815
7.184115	485.467192	9.344832
7.441721	481.750239	9.349850
7.662660	472.942446	9.354867
7.241290	455.496947	9.359885
7.284766	456.291596	9.364903
7.410298	476.961104	9.369920
7.680240	478.490282	9.374938
7.293131	472.655830	9.379955
7.426566	462.346979	9.384973
7.713971	460.790224	9.389991
7.080780	458.623477	9.395008
7.450773	461.771670	9.400026
7.345051	469.702819	9.405043
7.874190	471.251345	9.410061
7.409750	471.989876	9.415079
7.316134	461.691353	9.420096
7.252689	465.415537	9.425114
7.294500	475.308559	9.430131
7.391483	477.858906	9.435149
7.412620	476.959246	9.440167
7.290419	486.862192	9.445184
7.667352	481.902099	9.450202
7.502663	488.526535	9.455219
7.303727	476.458332	9.460237
7.277765	474.452061	9.465255
7.782759	481.552233	9.470272
7.769836	471.843815	9.475290
7.491165	484.194914	9.480307
7.477582	482.218261	9.485325
7.466114	482.421921	9.490343
7.595877	482.878006	9.495360
7.642282	470.547306	9.500378
7.390541	480.536817	9.505395
7.428327	472.625560	9.510413
7.498995	482.501441	9.515431
7.190921	472.883448	9.520448
7.862840	463.891393	9.525466
7.341645	477.706897	9.530483
7.674026	476.373466	9.535501
7.542472	484.895645	9.540519
7.451936	476.770965	9.545536
7.777969	470.824779	9.550554
7.931889	477.885281	9.555571
8.170847	471.078587	9.560589
7.647247	475.812137	9.565607
7.667039	479.741032	9.570624
7.870520	471.658649	9.575642
7.648994	478.058458	9.580659
7.717652	483.409266	9.585677
7.635606	478.817730	9.590695
7.142159	482.653471	9.595712
7.689884	480.364812	9.600730
7.478035	489.849464	9.605747
8.040791	479.296613	9.610765
7.754551	478.363062	9.615783
7.179813	482.375641	9.620800
7.806973	486.827908	9.625818
7.677510	501.424648	9.630835
7.827771	506.614355	9.635853
7.791054	509.876772	9.640871
8.025376	512.768522	9.645888
8.488029	496.853885	9.650906
8.090152	494.602928	9.655923
7.817950	495.936186	9.660941
7.817280	482.236932	9.665959
7.832924	482.922335	9.670976
8.197572	482.874563	9.675994
7.646573	486.204930	9.681011
7.645748	479.868143	9.686029
7.777796	475.539707	9.691047
7.441274	487.344455	9.696064
7.639361	479.793085	9.701082
7.723915	483.692899	9.706099
8.001625	484.857945	9.711117
8.011859	487.816358	9.716135
7.473883	483.479291	9.721152
7.851045	494.515821	9.726170
8.152378	514.252119	9.731187
7.917905	493.978117	9.736205
7.993496	485.675926	9.741223
7.807937	500.915767	9.746240
8.070604	489.002448	9.751258
8.010861	500.921629	9.756275
7.784009	485.279135	9.761293
7.809553	484.113698	9.766311
8.135958	502.214515	9.771328
8.553883	494.338362	9.776346
8.091285	496.733392	9.781363
7.698035	490.571695	9.786381
8.096777	483.238192	9.791399
7.858085	485.932651	9.796416
7.835550	487.116338	9.801434
7.736051	487.728263	9.806451
7.952222	497.859064	9.811469
7.867660	504.070167	9.816487
8.203408	504.979970	9.821504
8.499237	502.389950	9.826522
8.066298	503.805196	9.831539
7.754214	482.331546	9.836557
7.988176	493.636663	9.841575
7.896024	506.905289	9.846592
7.997972	515.125811	9.851610
8.265931	511.217882	9.856627
8.535277	500.477462	9.861645
8.277071	492.836633	9.866663
8.010548	492.215571	9.871680
8.159575	481.708607	9.876698
7.929410	489.574057	9.881715
8.059180	496.426913	9.886733
8.410690	489.533150	9.891751
7.874804	488.708141	9.896768
8.387554	492.477751	9.901786
7.915779	492.927100	9.906803
7.736300	496.650536	9.911821
8.124302	499.470868	9.916839
8.058255	505.833705	9.921856
8.065875	510.171609	9.926874
8.129080	504.844101	9.931891
8.384630	505.242609	9.936909
8.702222	508.916569	9.941927
8.255728	518.848252	9.946944
8.622062	511.156900	9.951962
8.569752	497.096499	9.956979
8.180498	484.010390	9.961997
7.993780	475.926026	9.967015
7.993490	482.837124	9.972032
8.253007	494.958741	9.977050
8.530815	500.204202	9.982067
8.026703	498.654694	9.987085
8.205761	498.389849	9.992103
8.381346	503.578743	9.997120
8.347017	498.859806	10.002138
8.642108	507.147892	10.007155
8.260247	498.507117	10.012173
8.151709	485.143496	10.017191
7.979697	496.796244	10.022208
8.107370	500.149666	10.027226
8.109287	502.219454	10.032243
8.207266	511.109622	10.037261
8.697037	509.555871	10.042279
8.407682	505.659523	10.047296
8.502722	505.685551	10.052314
8.376282	510.388441	10.057331
8.115824	508.106484	10.062349
8.351941	503.562921	10.067367
8.567264	511.333336	10.072384
8.460209	500.986403	10.077402
8.412170	502.530690	10.082419
8.244128	498.552222	10.087437
8.631648	509.817511	10.092455
8.281490	511.920372	10.097472
8.601077	500.278993	10.102490
8.629368	500.672082	10.107507
8.362629	503.686517	10.112525
8.628375	499.718978	10.117543
8.481510	511.935836	10.122560
8.229109	510.848660	10.127578
8.533370	512.337749	10.132595
8.356475	508.540546	10.137613
8.261922	506.311490	10.142631
8.342387	512.834409	10.147648
8.282798	502.221264	10.152666
8.294522	502.626416	10.157683
8.444956	510.249208	10.162701
8.332826	515.394823	10.167719
8.042626	512.334890	10.172736
8.270477	519.409072	10.177754
8.634896	519.607487	10.182771
8.392322	529.210582	10.187789
8.785992	532.023720	10.192807
8.712673	534.338828	10.197824
8.930519	536.207530	10.202842
8.810841	531.659746	10.207859
8.298353	523.355004	10.212877
8.823276	523.723930	10.217895
8.488818	524.344268	10.222912
8.354281	533.274034	10.227930
8.626599	527.276286	10.232947
8.592398	522.087109	10.237965
8.696255	524.352365	10.242983
8.536049	522.221956	10.248000
8.642842	536.137928	10.253018
8.931752	539.267280	10.258035
8.640754	535.664673	10.263053
8.859644	527.538825	10.268071
8.525767	526.783148	10.273088
8.571010	532.806666	10.278106
8.560789	532.012902	10.283123
8.636097	540.729913	10.288141
8.781396	529.775383	10.293159
8.571481	522.139598	10.298176
8.499575	524.407146	10.303194
8.783664	528.203124	10.308211
8.661955	527.717160	10.313229
8.722028	520.319940	10.318247
8.705755	530.774356	10.323264
8.973104	525.739902	10.328282
8.584824	518.823183	10.333299
8.566733	531.632102	10.338317
9.030613	533.780991	10.343335
8.918489	537.203549	10.348352
8.826262	530.963116	10.353370
8.892222	521.194976	10.358387
8.556200	527.720039	10.363405
8.716810	525.249032	10.368423
8.744059	531.572013	10.373440
8.844678	523.859172	10.378458
8.809869	528.648695	10.383475
8.833411	552.215506	10.388493
9.202564	545.300022	10.393511
9.035857	537.793160	10.398528
8.813790	524.115940	10.403546
9.100224	533.907551	10.408563
9.084385	529.605428	10.413581
9.195259	528.521293	10.418599
8.995315	526.371863	10.423616
8.732246	527.388113	10.428634
9.034465	524.626676	10.433651
8.508775	527.337706	10.438669
8.750269	527.214556	10.443687
8.959624	548.842997	10.448704
8.995312	560.299142	10.453722
9.256338	552.311848	10.458739
9.093018	548.929074	10.463757
9.174412	540.774270	10.468775
8.935922	531.950070	10.473792
9.001392	535.770835	10.478810
9.200767	528.638962	10.483827
9.278215	532.435759	10.488845
8.916455	526.969701	10.493863
8.942857	523.020722	10.498880
8.945069	527.062834	10.503898
9.086770	539.332328	10.508915
9.037660	547.933138	10.513933
9.244791	548.796823	10.518951
9.050816	552.446803	10.523968
9.396136	545.970553	10.528986
9.008833	546.072154	10.534003
9.237969	542.031446	10.539021
9.241421	529.489686	10.544039
8.696198	531.948159	10.549056
8.973915	544.641312	10.554074
9.131713	543.947454	10.559091
9.085039	551.951439	10.564109
9.261477	552.015206	10.569127
9.245863	551.323271	10.574144
9.363335	542.597927	10.579162
9.709850	550.616046	10.584179
9.103272	553.333442	10.589197
9.043226	548.549093	10.594215
9.364354	544.298312	10.599232
9.341959	549.688652	10.604250
9.597980	541.026808	10.609267
9.071822	532.705268	10.614285
9.558627	533.026519	10.619303
9.454583	531.827734	10.624320
9.253518	534.913935	10.629338
9.409620	523.295000	10.634355
9.104097	522.670579	10.639373
9.123491	523.977086	10.644391
9.089878	530.006647	10.649408
9.340692	545.433775	10.654426
9.396166	541.893645	10.659443
9.424818	553.104736	10.664461
9.861844	546.352187	10.669479
9.626071	543.845452	10.674496
9.369916	528.680880	10.679514
9.305496	515.120977	10.684531
8.907582	520.418667	10.689549
9.212347	529.876045	10.694567
9.476235	539.456598	10.699584
9.809972	537.343470	10.704602
9.746435	534.838153	10.709619
9.241173	523.401734	10.714637
9.071773	521.922858	10.719655
9.148649	537.762238	10.724672
9.246647	544.907268	10.729690
9.590114	543.206023	10.734707
9.814112	548.160129	10.739725
9.613539	546.626174	10.744743
9.579016	544.431889	10.749760
9.541049	543.784482	10.754778
9.602024	536.292440	10.759795
9.496364	549.010951	10.764813
9.547294	552.635182	10.769831
9.589202	538.616791	10.774848
9.516841	533.458837	10.779866
9.691436	538.064075	10.784883
9.281989	549.331182	10.789901
9.571276	547.862488	10.794919
9.850228	540.992696	10.799936
9.594196	540.325807	10.804954
9.660167	535.023103	10.809971
9.502498	544.912703	10.814989
9.211446	538.425710	10.820007
9.535602	546.712416	10.825024
9.774713	546.655911	10.830042
9.679803	536.165044	10.835059
9.575968	543.095545	10.840077
9.431973	550.426815	10.845095
9.459616	531.601236	10.850112
9.383165	544.454022	10.855130
9.650906	551.029663	10.860147
9.511931	547.466350	10.865165
9.411509	544.152616	10.870183
9.498442	539.878570	10.875200
9.321853	547.006663	10.880218
9.690480	552.682876	10.885235
9.890426	555.308620	10.890253
9.730807	555.636479	10.895271
9.781407	546.457709	10.900288
9.553275	545.123731	10.905306
9.752309	561.325843	10.910323
10.032906	573.605157	10.915341
10.009932	571.604718	10.920359
9.859290	551.200752	10.925376
9.418237	549.603490	10.930394
9.863732	558.395053	10.935411
9.979953	569.270543	10.940429
9.840512	572.192461	10.945447
10.417388	562.691385	10.950464
10.287090	561.645035	10.955482
10.170945	548.320428	10.960499
9.837000	543.635800	10.965517
9.462199	544.161474	10.970535
9.908345	550.156898	10.975552
9.625159	551.441388	10.980570
9.619632	544.038657	10.985587
9.915305	544.755926	10.990605
9.988383	560.712686	10.995623
9.881389	545.755101	11.000640
10.085643	566.904683	11.005658
10.004864	552.511029	11.010675
9.874288	559.502531	11.015693
10.028896	564.334969	11.020711
10.025498	555.877864	11.025728
10.175542	554.453076	11.030746
9.997994	551.104088	11.035763
9.702757	559.396329	11.040781
9.962549	566.913648	11.045799
10.505779	565.297868	11.050816
10.091911	561.256915	11.055834
10.084588	553.384249	11.060851
9.814219	545.489684	11.065869
10.068206	561.626382	11.070887
10.340714	555.679087	11.075904
10.324431	564.871206	11.080922
10.267922	558.353768	11.085939
9.963725	554.649084	11.090957
10.056015	550.986420	11.095975
10.114328	553.094714	11.100992
9.542459	555.200759	11.106010
10.115103	551.809971	11.111027
10.125098	565.930479	11.116045
10.011011	572.209348	11.121063
10.196880	571.577362	11.126080
10.118169	564.160843	11.131098
10.231352	569.359534	11.136115
10.138061	576.783856	11.141133
10.047643	566.497395	11.146151
10.230923	567.197561	11.151168
10.445678	575.252114	11.156186
10.156029	570.229179	11.161203
10.218937	568.704433	11.166221
9.852526	574.457949	11.171239
10.328022	566.844143	11.176256
10.396716	571.481762	11.181274
10.058196	581.074671	11.186291
9.950587	579.740743	11.191309
10.228941	575.566084	11.196327
10.484883	568.346438	11.201344
10.184783	578.028000	11.206362
10.202050	577.390872	11.211379
10.093018	574.201558	11.216397
10.237652	574.409163	11.221415
10.530225	572.352974	11.226432
10.444138	570.072090	11.231450
10.248066	561.673573	11.236467
9.928292	573.949123	11.241485
9.962029	585.673833	11.246503
10.624554	594.636537	11.251520
10.278626	608.573004	11.256538
10.392361	597.067956	11.261555
10.387645	591.675324	11.266573
10.923891	597.833374	11.271591
10.942601	593.667833	11.276608
10.382391	581.640385	11.281626
10.326449	568.217968	11.286643
10.563385	568.881325	11.291661
10.359789	587.923646	11.296679
10.733120	586.119889	11.301696
10.607432	573.929691	11.306714
10.495236	572.366108	11.311731
10.711009	572.830810	11.316749
10.506262	565.112147	11.321767
10.541851	578.262982	11.326784
10.516983	566.801760	11.331802
10.635419	568.547187	11.336819
10.491542	566.663522	11.341837
10.391703	583.979141	11.346855
10.873290	576.582127	11.351872
10.678989	578.742626	11.356890
10.124357	576.074407	11.361907
10.382533	584.901644	11.366925
11.065611	592.081255	11.371943
11.054231	583.562272	11.376960
10.678108	577.536716	11.381978
10.697908	575.681053	11.386995
10.716613	569.177074	11.392013
10.496606	581.721020	11.397031
10.805804	580.179775	11.402048
10.942787	594.835831	11.407066
10.694885	600.343569	11.412083
10.764720	571.927169	11.417101
10.759644	576.443804	11.422119
10.717494	572.193130	11.427136
10.747630	566.545738	11.432154
10.542995	575.912540	11.437171
11.080887	578.993422	11.442189
10.708551	592.107195	11.447207
10.921475	568.566185	11.452224
10.568611	569.022150	11.457242
10.783929	585.354276	11.462259
10.856723	580.296641	11.467277
10.571500	587.577471	11.472295
10.839808	579.775216	11.477312
10.987329	585.748013	11.482330
10.918541	588.188650	11.487347
10.915476	590.177178	11.492365
10.535424	586.455969	11.497383
11.114852	590.019494	11.502400
10.934457	582.319098	11.507418
10.827788	590.001141	11.512435
11.184708	581.061537	11.517453
10.899278	592.173541	11.522471
11.280137	592.625001	11.527488
11.063778	581.417835	11.532506
10.968286	587.046856	11.537523
10.982530	587.328540	11.542541
10.884539	590.903529	11.547559
11.063891	588.776714	11.552576
10.830967	586.124360	11.557594
10.934739	593.691383	11.562611
11.177896	582.339636	11.567629
11.122693	581.117417	11.572647
11.299433	575.024174	11.577664
11.243322	588.653287	11.582682
10.750114	584.511151	11.587699
11.282084	591.957434	11.592717
10.911113	588.023364	11.597735
11.188552	589.100097	11.602752
11.024585	591.495687	11.607770
10.999486	594.387070	11.612787
10.933844	586.902222	11.617805
10.884906	588.320425	11.622823
11.190254	580.805856	11.627840
11.098252	581.804773	11.632858
10.744683	585.378779	11.637875
10.983335	587.739688	11.642893
10.866430	591.320797	11.647911
10.753886	579.980601	11.652928
11.263213	586.127085	11.657946
10.928423	603.643636	11.662963
11.456830	601.121303	11.667981
11.321092	602.833974	11.672999
11.488700	607.099499	11.678016
11.460308	585.161554	11.683034
11.109599	593.058559	11.688051
11.034255	578.266402	11.693069
10.919892	598.771667	11.698087
11.397025	601.139394	11.703104
11.227813	611.674623	11.708122
11.404572	605.117465	11.713139
11.525499	606.581639	11.718157
11.361938	608.806754	11.723175
11.030689	603.853443	11.728192
11.463609	593.355582	11.733210
11.343312	600.727341	11.738227
11.497825	602.119980	11.743245
11.050761	603.988726	11.748263
11.072579	601.943397	11.753280
11.483809	609.822015	11.758298
11.133283	612.650780	11.763315
11.534523	610.167306	11.768333
11.290276	611.139585	11.773351
11.147874	610.581122	11.778368
11.618830	601.368021	11.783386
11.676795	605.455064	11.788403
11.410847	606.878868	11.793421
11.586991	611.808930	11.798439
11.379261	606.208261	11.803456
11.309010	604.735934	11.808474
11.451782	613.155232	11.813491
11.792710	603.934100	11.818509
11.640236	609.199672	11.823527
11.862133	607.249226	11.828544
12.145755	609.637806	11.833562
11.510438	618.529311	11.838579
11.778548	610.698671	11.843597
11.657802	599.309256	11.848615
11.466754	603.937086	11.853632
11.584779	599.667622	11.858650
11.388063	613.495508	11.863667
11.661017	599.822721	11.868685
11.407085	607.130213	11.873703
11.553303	603.957706	11.878720
11.771141	600.934923	11.883738
11.246002	611.503829	11.888755
11.667364	614.719740	11.893773
11.550156	634.717407	11.898791
11.769157	632.789503	11.903808
11.975773	631.482077	11.908826
11.631084	632.892973	11.913843
12.073105	630.908036	11.918861
11.934448	636.745808	11.923879
11.795649	627.697657	11.928896
12.121272	627.930554	11.933914
11.569521	615.431542	11.938931
12.256777	612.341521	11.943949
12.006261	608.969241	11.948967
11.909615	611.136535	11.953984
12.073444	611.420028	11.959002
11.837100	611.759909	11.964019
12.253299	597.951071	11.969037
11.844434	601.205541	11.974055
11.956379	603.965000	11.979072
12.031801	606.048530	11.984090
11.853961	607.553203	11.989107
12.121885	606.078383	11.994125
11.971167	603.558314	11.999143
11.957473	604.794271	12.004160
12.029571	599.421160	12.009178
11.638671	599.226679	12.014195
11.953482	592.875113	12.019213
11.818433	603.038912	12.024231
11.676824	602.600245	12.029248
11.870534	604.027769	12.034266
11.785967	617.509883	12.039283
12.289665	632.143227	12.044301
12.149245	620.138342	12.049319
12.165272	627.750685	12.054336
12.233681	629.541826	12.059354
12.090370	631.012688	12.064371
12.126084	622.117078	12.069389
12.179643	623.689639	12.074407
11.913278	626.372676	12.079424
12.294491	631.889152	12.084442
12.101884	632.796538	12.089459
12.481120	627.097585	12.094477
12.279445	613.445503	12.099495
11.917984	607.155709	12.104512
12.303414	603.383989	12.109530
12.220050	614.246596	12.114547
12.297783	611.921106	12.119565
12.198631	603.286477	12.124583
12.108429	610.088635	12.129600
12.440848	613.611972	12.134618
12.292938	620.861833	12.139635
12.166036	613.020499	12.144653
12.049162	608.844640	12.149671
11.872868	621.788864	12.154688
12.254498	621.984584	12.159706
12.365968	629.970138	12.164723
12.735959	625.238311	12.169741
12.702582	619.468309	12.174759
12.477364	625.761452	12.179776
12.681149	624.135735	12.184794
12.240989	615.822772	12.189811
12.533969	606.978380	12.194829
12.518619	608.747928	12.199847
11.817137	605.724016	12.204864
12.296127	615.921004	12.209882
12.091293	629.100078	12.214899
12.288409	631.196101	12.219917
12.584168	628.116924	12.224935
12.380823	635.968769	12.229952
12.451340	623.927676	12.234970
12.213299	626.590496	12.239987
12.480696	630.445916	12.245005
12.490478	627.042316	12.250023
12.391597	628.335804	12.255040
12.618991	632.702421	12.260058
12.808612	630.555058	12.265075
12.460097	633.629664	12.270093
12.481389	628.576929	12.275111
12.481746	623.508541	12.280128
12.309703	630.727473	12.285146
12.332494	632.718266	12.290163
12.153292	624.979795	12.295181
12.358028	637.264727	12.300199
12.492817	652.463973	12.305216
12.453213	647.395528	12.310234
12.774683	653.158057	12.315251
12.922126	650.742744	12.320269
12.761220	654.280266	12.325287
12.949152	652.732769	12.330304
13.180773	647.577647	12.335322
13.164988	655.346464	12.340339
12.985135	645.061347	12.345357
12.718006	645.851021	12.350375
12.356594	636.468514	12.355392
12.671930	645.097476	12.360410
12.764118	643.564981	12.365427
13.030265	652.485676	12.370445
13.098838	641.341127	12.375463
12.570799	645.093959	12.380480
13.053335	646.280573	12.385498
12.926423	639.739423	12.390515
12.320151	634.772389	12.395533
12.737721	640.876464	12.400551
12.799360	655.566465	12.405568
13.041515	649.216795	12.410586
12.899784	658.210867	12.415603
12.986347	657.029547	12.420621
13.148576	649.404828	12.425639
12.839916	657.607699	12.430656
13.128584	657.174199	12.435674
12.695240	650.185594	12.440691
12.835896	648.096393	12.445709
12.979127	652.823341	12.450727
12.976439	655.127397	12.455744
13.003888	656.350601	12.460762
13.043317	658.190466	12.465779
13.044777	647.709681	12.470797
13.226033	652.676824	12.475815
13.096198	650.273397	12.480832
13.155764	651.586242	12.485850
12.815541	653.248905	12.490867
12.952798	649.194166	12.495885
13.167099	647.052402	12.500903
12.733190	658.291852	12.505920
12.760500	649.536401	12.510938
12.785555	649.349331	12.515955
12.816523	658.067035	12.520973
13.429458	671.348388	12.525991
13.179515	679.008736	12.531008
13.279007	677.613949	12.536026
13.223740	680.150310	12.541043
13.469746	674.219752	12.546061
13.328438	657.793684	12.551079
13.203626	650.258120	12.556096
13.329491	651.251308	12.561114
12.960919	656.613868	12.566131
13.301715	663.689346	12.571149
13.452518	669.727930	12.576167
13.301657	668.773158	12.581184
13.335848	678.096283	12.586202
13.546054	675.383954	12.591219
13.554760	671.996294	12.596237
13.366539	656.006769	12.601255
13.346810	650.294579	12.606272
13.494746	657.580153	12.611290
13.362865	654.138784	12.616307
13.419873	663.773908	12.621325
13.930407	652.348666	12.626343
13.506811	651.932089	12.631360
13.716687	646.887671	12.636378
13.462792	647.706830	12.641395
13.261885	650.679416	12.646413
13.253856	636.312166	12.651431
13.250464	648.784350	12.656448
13.709288	658.504838	12.661466
13.808631	660.401589	12.666483
13.556941	658.304432	12.671501
13.728333	643.252655	12.676519
13.383243	653.578780	12.681536
13.077369	651.935083	12.686554
13.480368	658.549532	12.691571
13.510649	671.846435	12.696589
13.674950	663.924739	12.701607
13.526629	670.925376	12.706624
13.466412	667.974550	12.711642
13.808472	668.034459	12.716659
13.690581	668.242172	12.721677
13.880802	659.126675	12.726695
13.574134	669.112273	12.731712
13.506670	666.765344	12.736730
13.495125	662.636086	12.741747
13.557583	671.626574	12.746765
13.709272	667.560103	12.751783
13.624256	675.314530	12.756800
13.921491	671.212630	12.761818
13.860304	669.988187	12.766835
13.907338	667.730615	12.771853
13.777181	659.773006	12.776871
13.830144	666.170901	12.781888
13.708549	659.893999	12.786906
13.743609	665.556239	12.791923
13.739742	668.081389	12.796941
14.037157	658.491505	12.801959
13.932733	671.724306	12.806976
13.872878	669.117407	12.811994
13.754050	664.146577	12.817011
13.620527	668.904267	12.822029
13.954205	675.472779	12.827047
13.888881	685.941282	12.832064
14.206642	687.800658	12.837082
14.468162	674.779704	12.842099
14.025247	671.970890	12.847117
13.910989	659.352807	12.852135
13.915908	664.820953	12.857152
13.729635	660.110001	12.862170
14.176839	680.464257	12.867187
14.219221	690.287880	12.872205
13.908840	677.994004	12.877223
13.869134	684.027728	12.882240
14.164518	694.098892	12.887258
14.361856	697.463528	12.892275
14.336096	692.913611	12.897293
14.252472	688.694654	12.902311
13.904518	686.795613	12.907328
14.226005	695.950658	12.912346
14.553744	687.899202	12.917363
14.240287	681.756494	12.922381
14.066102	664.622357	12.927399
14.101457	673.541353	12.932416
13.986466	688.675624	12.937434
14.511510	689.050847	12.942451
14.177844	693.407555	12.947469
14.306765	694.274034	12.952487
14.400446	682.065170	12.957504
14.555613	697.542129	12.962522
14.424443	686.693936	12.967539
13.853185	682.421994	12.972557
14.417145	688.307489	12.977575
14.061049	693.074811	12.982592
14.431316	688.866790	12.987610
14.396687	693.078815	12.992627
13.960293	690.262664	12.997645
14.238590	683.863138	13.002663
13.908767	688.654745	13.007680
14.260096	684.926221	13.012698
14.559004	691.796834	13.017715
14.470750	694.701284	13.022733
14.407415	694.995124	13.027751
14.318392	685.118632	13.032768
14.301563	691.770470	13.037786
14.826601	707.331499	13.042803
14.299966	694.588653	13.047821
14.980233	698.231076	13.052839
14.744123	699.590251	13.057856
14.172150	683.711320	13.062874
14.682878	690.495096	13.067891
14.656703	704.510927	13.072909
14.623645	710.070245	13.077927
14.806408	700.700274	13.082944
14.973393	695.747770	13.087962
14.928850	684.955433	13.092979
15.020317	684.013185	13.097997
14.982873	679.752281	13.103015
15.066837	693.387929	13.108032
14.747343	683.717962	13.113050
14.929168	681.780098	13.118067
14.662247	692.191828	13.123085
14.884625	684.797513	13.128103
14.791893	685.118049	13.133120
14.784317	683.948321	13.138138
15.045038	693.254897	13.143155
14.520836	692.099841	13.148173
14.740502	685.643228	13.153191
14.926797	686.945688	13.158208
14.735832	685.845719	13.163226
15.028677	677.919655	13.168243
14.902289	691.698713	13.173261
15.012455	689.260833	13.178279
14.737837	683.651685	13.183296
15.006780	691.688333	13.188314
14.899690	688.454513	13.193331
14.906124	688.541761	13.198349
14.621042	686.765414	13.203367
14.785423	690.867361	13.208384
14.510879	685.324473	13.213402
15.076991	680.498787	13.218419
14.523429	695.537676	13.223437
15.266513	700.271638	13.228455
15.279384	704.580365	13.233472
15.042419	702.092729	13.238490
15.095819	706.549742	13.243507
15.028551	702.101000	13.248525
15.220239	701.594331	13.253543
15.368793	703.158327	13.258560
15.279749	708.710637	13.263578
15.171072	696.470352	13.268595
14.775485	703.711715	13.273613
15.261463	705.932903	13.278631
15.082784	709.965528	13.283648
14.987160	712.221037	13.288666
15.350817	710.551328	13.293683
15.124260	709.046677	13.298701
15.485238	704.827485	13.303719
15.424568	712.398232	13.308736
15.381341	709.659333	13.313754
15.399549	712.269394	13.318771
15.381966	705.897283	13.323789
15.279451	705.480891	13.328807
15.213510	715.472979	13.333824
15.052365	714.996344	13.338842
15.183529	715.224997	13.343859
15.416039	714.068144	13.348877
15.316491	711.136097	13.353895
15.476837	713.051698	13.358912
15.129832	719.079931	13.363930
15.333999	710.498713	13.368947
15.224491	718.512618	13.373965
15.248420	713.099682	13.378983
15.384902	699.700667	13.384000
15.165765	723.529790	13.389018
15.986838	722.949756	13.394035
15.280622	718.039383	13.399053
15.563708	715.101034	13.404071
15.855051	733.901861	13.409088
15.557282	725.654900	13.414106
15.522586	713.974216	13.419123
15.786579	723.791538	13.424141
15.513889	717.743417	13.429159
16.006312	714.986865	13.434176
16.113786	721.780185	13.439194
15.633163	703.554770	13.444211
15.449400	700.443414	13.449229
15.469965	703.255077	13.454247
15.513264	697.141675	13.459264
15.210528	715.499073	13.464282
15.747080	712.738763	13.469299
15.804146	728.884375	13.474317
15.808331	727.485582	13.479335
15.725793	733.488163	13.484352
15.733095	731.624975	13.489370
15.732818	722.267893	13.494387
16.120698	732.419262	13.499405
15.860259	724.308465	13.504423
15.904011	729.896780	13.509440
15.795508	731.198094	13.514458
16.130096	732.748724	13.519475
15.978213	731.696277	13.524493
15.512913	731.977358	13.529511
15.550077	732.791943	13.534528
15.708144	729.219923	13.539546
15.795819	726.245916	13.544563
15.726353	725.338348	13.549581
15.593065	728.126783	13.554599
16.151521	733.277847	13.559616
15.830421	747.756490	13.564634
15.972986	751.896585	13.569651
16.349726	752.061515	13.574669
16.487624	741.174287	13.579687
16.184429	728.390096	13.584704
16.190699	730.516033	13.589722
16.593118	723.131363	13.594739
16.410556	723.172483	13.599757
16.164089	725.154980	13.604775
16.299256	725.285175	13.609792
16.329325	724.475622	13.614810
16.546032	719.026169	13.619827
16.174494	715.347780	13.624845
15.869423	727.261368	13.629863
15.903366	725.327734	13.634880
15.843164	730.253834	13.639898
16.023027	714.717829	13.644915
16.033873	720.513270	13.649933
16.136875	748.217798	13.654951
16.691985	742.112554	13.659968
16.522021	747.516608	13.664986
16.274966	745.544947	13.670003
16.496187	735.127509	13.675021
16.558606	746.977220	13.680039
16.645802	734.277028	13.685056
16.118433	727.479849	13.690074
16.194265	735.584644	13.695091
16.586183	738.303415	13.700109
16.539649	740.895221	13.705127
16.882036	729.414224	13.710144
16.386832	728.166259	13.715162
16.309986	728.553735	13.720179
16.432206	733.422853	13.725197
16.140547	746.505163	13.730215
16.639259	742.712510	13.735232
16.722631	734.882358	13.740250
16.838837	736.180024	13.745267
16.809820	746.264175	13.750285
16.290485	742.201835	13.755303
16.565863	743.783833	13.760320
16.438520	744.299144	13.765338
16.498844	743.671043	13.770355
16.657855	745.479559	13.775373
16.663078	746.706250	13.780391
16.775545	746.079448	13.785408
16.400113	742.496338	13.790426
16.770059	746.846960	13.795443
16.743891	742.470665	13.800461
16.749652	749.459814	13.805479
16.738180	743.045706	13.810496
16.520248	743.092368	13.815514
16.388498	743.018229	13.820531
16.615409	749.215330	13.825549
16.975801	756.218347	13.830567
17.207292	768.429750	13.835584
17.083287	759.275071	13.840602
16.808763	749.841021	13.845619
16.704156	740.143667	13.850637
17.278786	761.462669	13.855655
17.450377	744.523590	13.860672
16.995370	744.298125	13.865690
16.842165	735.630875	13.870707
16.867539	745.921100	13.875725
16.638666	753.104805	13.880743
16.795433	750.211488	13.885760
16.784925	760.463161	13.890778
17.130411	767.146623	13.895795
17.161637	758.040208	13.900813
17.118708	768.167577	13.905831
17.114551	771.484901	13.910848
17.484913	768.381389	13.915866
17.388915	764.331612	13.920883
17.377318	761.802346	13.925901
17.068961	767.673060	13.930919
17.162800	761.135148	13.935936
17.088913	763.510335	13.940954
17.558735	768.564844	13.945971
17.674979	758.034451	13.950989
17.492425	748.440824	13.956007
17.503969	736.598244	13.961024
17.366043	728.357796	13.966042
17.281075	736.655044	13.971059
17.360338	732.555724	13.976077
17.254155	731.565546	13.981095
17.307055	728.477066	13.986112
17.048302	736.435466	13.991130
17.290551	739.954020	13.996147
17.124484	754.657689	14.001165
17.410200	758.219930	14.006183
17.573836	747.574820	14.011200
17.422615	760.155451	14.016218
17.547458	752.299859	14.021235
17.868632	750.125559	14.026253
17.567453	749.973823	14.031271
17.371026	748.893640	14.036288
17.592439	765.234444	14.041306
17.339433	758.066061	14.046323
17.974549	750.951036	14.051341
17.620959	756.462758	14.056359
17.723085	749.166153	14.061376
17.680543	759.586948	14.066394
17.572479	749.322081	14.071411
17.921748	745.025818	14.076429
17.762557	745.763870	14.081447
17.080920	755.792487	14.086464
17.413806	754.127595	14.091482
17.565970	751.253934	14.096499
17.788581	754.299038	14.101517
17.619673	753.956163	14.106535
17.264085	754.917493	14.111552
17.664325	749.546573	14.116570
17.680138	744.766065	14.121587
17.910081	751.098392	14.126605
17.795496	774.179050	14.131623
18.092157	775.726158	14.136640
17.996913	768.671910	14.141658
17.720157	761.346299	14.146675
17.941377	758.199883	14.151693
17.953394	779.818498	14.156711
18.125389	782.587512	14.161728
17.928192	766.163789	14.166746
17.820727	777.781360	14.171763
17.943876	775.451889	14.176781
18.075039	782.951583	14.181799
18.367478	777.130482	14.186816
18.250891	774.721806	14.191834
17.713530	770.804296	14.196851
18.116404	775.124519	14.201869
18.085417	779.531655	14.206887
18.464867	778.556905	14.211904
18.221952	773.857952	14.216922
17.847329	771.855782	14.221939
17.991318	769.305294	14.226957
17.857183	788.529451	14.231975
17.779867	780.667650	14.236992
17.931073	781.846226	14.242010
18.025543	783.876298	14.247027
18.271753	778.621022	14.252045
17.987944	781.126932	14.257063
18.208626	776.705641	14.262080
18.408024	784.507072	14.267098
18.315239	783.647337	14.272115
18.406028	784.491392	14.277133
18.105307	787.268199	14.282151
18.345213	804.237308	14.287168
18.727009	799.213250	14.292186
18.358025	799.608629	14.297203
18.563441	800.289557	14.302221
18.662487	813.042455	14.307239
18.647697	786.766008	14.312256
18.689438	778.213362	14.317274
18.270118	774.353097	14.322291
18.670053	780.280101	14.327309
18.433864	783.924118	14.332327
18.815449	787.442942	14.337344
18.580995	780.565136	14.342362
18.571804	777.710440	14.347379
18.566171	779.494261	14.352397
18.599718	794.381284	14.357415
18.754430	796.029531	14.362432
18.734423	781.682975	14.367450
18.690525	795.670097	14.372467
18.844905	805.463613	14.377485
18.660067	805.776491	14.382503
18.475790	798.344856	14.387520
18.651045	797.588293	14.392538
18.770934	797.506285	14.397555
18.975871	799.146663	14.402573
18.874972	798.698457	14.407591
19.313083	794.953158	14.412608
19.396026	791.828401	14.417626
19.178230	782.622133	14.422643
18.632718	764.438380	14.427661
18.737184	767.208505	14.432679
18.799206	767.246018	14.437696
19.276291	785.563359	14.442714
18.689962	778.279933	14.447731
18.896715	789.535852	14.452749
18.626330	795.110290	14.457767
19.124973	783.989788	14.462784
19.087482	792.001909	14.467802
19.100810	801.167420	14.472819
19.112543	787.024172	14.477837
19.140416	795.736117	14.482855
19.230783	800.417737	14.487872
19.492360	796.700097	14.492890
19.382034	793.308972	14.497907
19.519599	775.185445	14.502925
18.929915	772.472193	14.507943
18.508947	786.650932	14.512960
19.013787	785.574484	14.517978
19.138633	795.666114	14.522995
19.109829	794.212524	14.528013
19.141927	798.963234	14.533031
18.976481	794.043853	14.538048
18.853373	788.221582	14.543066
18.916353	792.326818	14.548083
19.096557	795.990805	14.553101
19.431659	811.698451	14.558119
19.264783	816.906379	14.563136
19.834310	819.171297	14.568154
19.755838	822.594949	14.573171
19.368422	798.942566	14.578189
19.455977	798.991858	14.583207
19.486890	813.377531	14.588224
19.777553	806.196532	14.593242
19.491246	801.725278	14.598259
19.327979	786.252440	14.603277
19.485895	798.162963	14.608295
19.797815	814.502255	14.613312
19.720783	802.010784	14.618330
19.703051	807.687652	14.623347
19.673528	797.199010	14.628365
19.467290	787.100983	14.633383
19.359360	798.150589	14.638400
19.846388	799.790951	14.643418
19.826748	819.757760	14.648435
19.991795	811.637064	14.653453
19.919574	813.671166	14.658471
19.643494	798.149720	14.663488
19.593492	796.134556	14.668506
19.708850	805.116824	14.673523
19.938565	809.132822	14.678541
19.835471	815.211236	14.683559
19.854428	798.374916	14.688576
20.038842	807.510469	14.693594
19.765973	810.784694	14.698611
20.058331	809.403861	14.703629
20.187870	804.340428	14.708647
20.278297	810.612584	14.713664
20.294360	797.213428	14.718682
19.678841	794.662013	14.723699
19.855099	800.661939	14.728717
20.053715	802.552618	14.733735
19.730627	801.119889	14.738752
19.864089	800.391964	14.743770
20.010034	812.525281	14.748787
19.996215	808.667748	14.753805
20.074304	799.866397	14.758823
20.023466	812.346129	14.763840
20.290925	798.790817	14.768858
19.873397	808.008058	14.773875
20.088857	802.066464	14.778893
20.379519	802.156518	14.783911
19.987517	794.085237	14.788928
20.060450	793.672912	14.793946
19.971527	806.243815	14.798963
20.245493	823.056125	14.803981
20.602213	816.047811	14.808999
20.044632	823.491330	14.814016
20.468804	832.242188	14.819034
20.444485	827.373271	14.824051
20.449347	829.322713	14.829069
20.579488	832.032020	14.834087
20.395144	837.551963	14.839104
20.563436	821.446471	14.844122
20.299702	820.338959	14.849139
20.733340	827.254789	14.854157
20.508745	827.368767	14.859175
20.494246	822.305806	14.864192
20.754502	815.464086	14.869210
20.412672	822.236321	14.874227
20.345911	825.102711	14.879245
20.702241	825.927255	14.884263
20.426612	824.887880	14.889280
20.346843	822.356663	14.894298
20.389833	832.035100	14.899315
20.744274	830.868603	14.904333
20.474758	829.998685	14.909351
20.590953	824.697494	14.914368
20.544940	827.099880	14.919386
20.675115	827.391806	14.924403
20.416121	829.410991	14.929421
20.815677	833.968437	14.934439
20.380923	857.547496	14.939456
21.105368	849.386475	14.944474
21.391249	856.047751	14.949491
21.192245	848.574221	14.954509
20.981601	832.108362	14.959527
20.738924	826.285878	14.964544
21.116108	831.137165	14.969562
20.847564	839.860859	14.974579
20.643006	843.282180	14.979597
20.767769	844.139850	14.984615
20.818512	853.059682	14.989632
21.325050	850.736404	14.994650
21.428101	850.780113	14.999667
21.286077	843.464917	15.004685
21.356536	853.984829	15.009703
21.303986	848.517562	15.014720
21.287239	842.823778	15.019738
21.416587	840.496483	15.024755
21.137656	840.287611	15.029773
21.200969	843.300883	15.034791
21.104805	847.058676	15.039808
21.450121	845.552777	15.044826
21.238195	843.619783	15.049843
21.006906	839.808939	15.054861
21.293843	836.238798	15.059879
20.726025	842.781358	15.064896
21.363374	843.618678	15.069914
21.138553	848.883032	15.074931
21.387920	837.962501	15.079949
21.413125	834.272420	15.084967
21.066912	839.764076	15.089984
20.977220	835.921581	15.095002
21.021560	849.525686	15.100019
21.629119	865.708250	15.105037
22.028722	858.421797	15.110055
21.812248	863.018964	15.115072
21.793461	851.786983	15.120090
21.691283	854.965044	15.125107
21.391998	843.319419	15.130125
21.618406	854.808989	15.135143
21.528297	866.117781	15.140160
21.623144	861.413222	15.145178
21.431611	859.726343	15.150195
21.697006	867.397549	15.155213
22.188126	865.568998	15.160231
21.967875	869.813303	15.165248
21.988764	868.560207	15.170266
22.253191	865.347042	15.175283
21.782618	859.045850	15.180301
21.967397	839.245416	15.185319
21.506167	842.041068	15.190336
21.934964	847.105183	15.195354
22.129376	864.030983	15.200371
21.841990	865.559152	15.205389
21.789841	854.802618	15.210407
21.797646	860.696412	15.215424
21.968036	863.049119	15.220442
22.207519	866.984704	15.225459
22.129922	871.219282	15.230477
22.051194	855.919332	15.235495
22.039788	865.401181	15.240512
22.487350	852.597105	15.245530
22.400501	867.001272	15.250547
22.004923	852.397918	15.255565
22.354804	850.954420	15.260583
22.075854	850.780265	15.265600
22.018196	854.033403	15.270618
22.345495	868.902866	15.275635
22.132312	867.131015	15.280653
22.703583	858.659469	15.285671
22.418162	848.346591	15.290688
22.173240	840.384791	15.295706
22.353904	854.889048	15.300723
22.208985	860.200848	15.305741
22.161196	854.612910	15.310759
22.194940	857.141662	15.315776
22.091268	859.673009	15.320794
22.017809	858.838645	15.325811
22.343050	857.092890	15.330829
22.464964	850.187624	15.335847
22.650317	862.579892	15.340864
22.481932	848.360673	15.345882
22.442520	859.999193	15.350899
22.641310	854.281103	15.355917
22.540445	855.044735	15.360935
22.431026	857.955684	15.365952
22.497973	847.720145	15.370970
22.613464	867.123029	15.375987
22.541069	879.546225	15.381005
22.567849	873.135545	15.386023
22.490044	881.633712	15.391040
22.692694	873.324057	15.396058
22.701036	878.144783	15.401075
22.854659	882.832294	15.406093
22.519909	874.155550	15.411111
22.581336	871.965126	15.416128
22.879274	879.094744	15.421146
22.932319	878.710780	15.426163
22.752588	875.642943	15.431181
22.675133	878.952836	15.436199
22.509090	881.847414	15.441216
22.667266	887.260058	15.446234
22.956966	888.426409	15.451251
22.725497	899.075706	15.456269
23.358060	892.188248	15.461287
23.182131	901.389774	15.466304
23.185005	898.981300	15.471322
23.077808	898.089102	15.476339
23.196081	904.237006	15.481357
23.155845	897.862064	15.486375
23.458093	895.091099	15.491392
23.319079	896.072153	15.496410
23.329671	897.247520	15.501427
23.238603	890.596518	15.506445
23.308079	894.322057	15.511463
23.309527	892.627029	15.516480
23.207239	894.526994	15.521498
23.476159	893.017281	15.526515
23.461142	890.059337	15.531533
23.178126	890.750522	15.536551
23.682341	896.077394	15.541568
23.599530	897.917502	15.546586
23.315790	895.566557	15.551603
23.404823	897.578559	15.556621
23.673954	897.997040	15.561639
23.638941	901.480172	15.566656
23.598598	895.960484	15.571674
23.617686	894.246914	15.576691
23.639604	893.072551	15.581709
23.529626	891.117267	15.586727
23.678506	900.378357	15.591744
23.458703	897.739680	15.596762
23.626382	893.336131	15.601779
23.616437	897.118296	15.606797
23.586418	889.757130	15.611815
23.625303	901.023642	15.616832
23.683986	900.048649	15.621850
23.712313	894.818009	15.626867
23.208387	893.240033	15.631885
23.740686	892.408589	15.636903
23.893047	891.500972	15.641920
23.613996	899.005026	15.646938
23.790652	894.174030	15.651955
23.894013	902.577550	15.656973
23.993604	911.682264	15.661991
24.611960	919.326594	15.667008
23.772109	904.865390	15.672026
23.852971	896.290778	15.677043
24.096019	909.343081	15.682061
24.345968	907.949950	15.687079
24.060365	903.339703	15.692096
23.800090	904.494393	15.697114
24.352782	905.408098	15.702131
23.984514	921.232354	15.707149
24.333517	925.611549	15.712167
24.617449	923.146412	15.717184
24.183158	913.724683	15.722202
24.230767	892.156311	15.727219
24.334524	901.904162	15.732237
24.589016	896.556034	15.737255
24.159807	899.409794	15.742272
24.152424	905.334385	15.747290
24.434355	902.809604	15.752307
24.468479	916.118710	15.757325
24.605965	912.265851	15.762343
24.897050	911.522694	15.767360
24.180349	901.226864	15.772378
24.669075	904.627938	15.777395
24.164396	906.900223	15.782413
24.296715	905.045832	15.787431
24.433895	904.582413	15.792448
24.455038	910.300561	15.797466
24.659804	906.525526	15.802483
24.287719	923.142502	15.807501
24.407548	916.562591	15.812519
24.619500	916.794368	15.817536
24.262149	912.065970	15.822554
24.715813	906.516217	15.827571
24.401306	915.048330	15.832589
24.643531	925.471944	15.837607
24.852797	925.947143	15.842624
24.642875	928.545640	15.847642
24.849478	933.063915	15.852659
24.966865	941.840803	15.857677
24.863509	938.394909	15.862695
25.314913	931.598937	15.867712
24.440957	937.896000	15.872730
25.024855	934.746380	15.877747
24.875866	944.133059	15.882765
25.081920	941.844227	15.887783
25.212625	937.661059	15.892800
25.268646	934.745627	15.897818
25.294708	926.353159	15.902835
24.755449	928.324747	15.907853
24.884315	931.453998	15.912871
25.493909	933.548549	15.917888
25.228523	925.258551	15.922906
25.639498	926.872971	15.927923
25.163862	936.878880	15.932941
25.205270	928.995256	15.937959
25.420459	937.071997	15.942976
25.104592	940.412943	15.947994
25.385273	935.262676	15.953011
25.121495	925.681679	15.958029
25.118022	938.103584	15.963047
25.292072	929.511201	15.968064
25.292783	931.855787	15.973082
25.111074	932.310191	15.978099
25.280811	942.388559	15.983117
24.952426	928.449970	15.988135
25.295803	945.153689	15.993152
25.475970	952.753077	15.998170
25.438740	952.332761	16.003187
25.621820	953.462172	16.008205
25.517567	951.382906	16.013223
25.576171	959.329552	16.018240
25.692817	956.978985	16.023258
25.666595	948.862948	16.028275
25.518508	957.084979	16.033293
25.272162	949.397912	16.038311
25.666121	955.767733	16.043328
25.545607	957.998769	16.048346
26.318642	967.247312	16.053363
25.832300	970.450869	16.058381
25.966700	962.085593	16.063399
25.919432	954.171670	16.068416
25.474565	956.920593	16.073434
26.026560	967.788012	16.078451
25.964298	975.971358	16.083469
25.905648	970.091591	16.088487
26.288716	974.951464	16.093504
26.373979	978.519909	16.098522
26.331319	971.864448	16.103539
26.249540	968.004905	16.108557
26.281737	973.200624	16.113575
26.433478	951.098303	16.118592
26.139583	950.882306	16.123610
26.258403	942.049257	16.128627
26.284833	949.161481	16.133645
26.064360	951.275632	16.138663
26.317319	959.469543	16.143680
26.267472	961.629547	16.148698
26.394355	963.812355	16.153715
26.457720	968.435133	16.158733
26.582689	968.248186	16.163751
26.482941	968.055420	16.168768
26.418703	968.223171	16.173786
26.707323	963.440888	16.178803
26.558897	960.585886	16.183821
26.471251	953.498815	16.188839
26.564845	956.649377	16.193856
26.509086	970.206140	16.198874
26.498810	970.374904	16.203891
26.617197	972.025703	16.208909
26.447313	971.481001	16.213927
26.951570	969.476810	16.218944
26.512853	973.382975	16.223962
26.586778	954.107878	16.228979
26.519316	960.082926	16.233997
26.667580	971.221890	16.239015
26.491281	960.853980	16.244032
26.558793	971.715257	16.249050
26.301781	967.192034	16.254067
26.640216	970.490433	16.259085
26.677684	986.301671	16.264103
27.014924	990.496529	16.269120
26.693517	997.644335	16.274138
27.015257	994.157074	16.279155
27.255404	992.288936	16.284173
27.081101	992.246710	16.289191
27.594156	986.327858	16.294208
27.531070	987.824050	16.299226
27.073565	968.821552	16.304243
27.125925	961.901893	16.309261
27.204179	959.828746	16.314279
27.409874	952.705182	16.319296
27.032688	967.975445	16.324314
27.135434	954.316432	16.329331
26.929874	974.902691	16.334349
27.275966	987.465525	16.339367
27.779035	982.498156	16.344384
27.522003	985.492215	16.349402
27.377688	979.114615	16.354419
27.417721	984.454279	16.359437
27.214301	992.423059	16.364455
27.417447	979.499393	16.369472
27.315380	986.934728	16.374490
27.567218	985.194150	16.379507
27.119461	994.567704	16.384525
27.157084	989.767934	16.389543
27.498756	981.038808	16.394560
27.679972	987.397790	16.399578
27.563634	991.960365	16.404595
27.595584	989.528387	16.409613
27.917780	982.140401	16.414631
27.884482	974.710284	16.419648
27.631521	978.962895	16.424666
27.615145	982.569357	16.429683
27.415208	982.931943	16.434701
27.531595	999.481925	16.439719
28.115343	1007.122248	16.444736
28.024991	1011.431442	16.449754
28.093757	1010.382278	16.454771
28.100949	1001.475169	16.459789
28.344784	1013.176710	16.464807
28.463503	1001.127811	16.469824
28.168120	979.732996	16.474842
27.875357	976.181068	16.479859
27.931712	973.240330	16.484877
27.713526	976.973085	16.489895
28.201199	992.969418	16.494912
28.119403	1004.314865	16.499930
28.184516	1006.299069	16.504947
28.384147	997.200861	16.509965
28.390085	1007.257592	16.514983
28.492554	997.574991	16.520000
28.182174	998.693355	16.525018
28.234788	1000.670048	16.530035
28.339441	1000.296931	16.535053
28.364817	996.054512	16.540071
28.492478	989.416541	16.545088
28.180037	1002.780011	16.550106
28.035523	997.655318	16.555123
28.219304	988.625871	16.560141
28.069516	996.400053	16.565159
28.424550	997.710813	16.570176
28.453896	995.572739	16.575194
28.418466	1008.220611	16.580211
28.471651	1013.331000	16.585229
28.431150	1026.503555	16.590247
29.027690	1020.962940	16.595264
28.900654	1022.983563	16.600282
28.786668	1013.435855	16.605299
29.083108	1016.743999	16.610317
28.523794	1011.999878	16.615335
28.893729	1015.353312	16.620352
29.016274	1017.451598	16.625370
29.016818	1019.275503	16.630387
29.044892	1019.681261	16.635405
28.921626	1022.070531	16.640423
29.063368	1024.244707	16.645440
29.314763	1025.316081	16.650458
29.062942	1014.890543	16.655475
28.963331	1008.436499	16.660493
29.131824	1019.941562	16.665511
29.322944	1016.967078	16.670528
29.240650	1002.380790	16.675546
29.110417	1007.589344	16.680563
29.472732	999.683813	16.685581
28.893614	1007.190744	16.690599
29.461938	1008.928845	16.695616
29.427965	1003.490178	16.700634
29.145194	1007.946287	16.705651
29.064882	1008.201765	16.710669
29.249901	1020.209179	16.715687
29.340382	1017.834301	16.720704
28.959502	1013.339941	16.725722
28.504918	1013.707709	16.730739
29.118972	1013.103298	16.735757
29.270550	1029.587833	16.740775
29.547479	1040.501550	16.745792
29.616122	1041.409049	16.750810
29.660399	1044.245454	16.755827
29.952478	1042.599553	16.760845
29.654708	1046.278519	16.765863
29.694690	1038.896856	16.770880
29.910744	1028.158158	16.775898
29.915008	1033.014279	16.780915
30.273310	1031.001390	16.785933
30.023090	1025.063255	16.790951
29.950127	1009.124783	16.795968
29.863604	1009.835681	16.800986
29.605731	1009.374193	16.806003
29.717534	1015.005585	16.811021
29.870533	1032.922668	16.816039
30.129211	1033.109256	16.821056
29.804995	1033.043179	16.826074
30.159374	1030.753187	16.831091
29.958999	1029.206535	16.836109
29.912186	1029.358933	16.841127
30.275475	1032.116951	16.846144
30.322560	1021.003934	16.851162
30.129071	1029.406685	16.856179
30.175809	1033.091633	16.861197
30.259334	1036.294281	16.866215
30.326290	1033.096246	16.871232
30.246045	1037.066184	16.876250
29.866452	1036.620610	16.881267
29.967019	1032.880809	16.886285
29.999623	1038.332109	16.891303
30.003191	1051.633481	16.896320
30.316263	1055.232523	16.901338
30.665846	1061.896520	16.906355
30.372832	1062.043310	16.911373
30.344826	1058.774940	16.916391
30.697349	1058.063177	16.921408
30.420380	1063.307361	16.926426
30.466448	1057.218649	16.931443
30.888346	1053.254926	16.936461
30.276079	1065.500898	16.941479
30.603665	1059.308116	16.946496
30.804496	1048.028979	16.951514
30.346020	1055.318207	16.956531
30.698862	1051.188574	16.961549
30.753938	1063.203752	16.966567
30.628695	1059.284725	16.971584
30.981687	1068.747459	16.976602
31.031086	1081.644031	16.981619
31.500278	1084.824133	16.986637
31.109828	1064.412968	16.991655
31.022360	1056.966057	16.996672
30.830225	1055.822065	17.001690
30.825881	1056.734689	17.006707
31.172995	1064.064965	17.011725
31.245183	1074.127133	17.016743
31.293936	1073.355663	17.021760
31.130883	1074.100645	17.026778
31.146690	1075.104789	17.031795
31.381261	1075.635990	17.036813
31.186164	1078.064924	17.041831
31.462030	1084.058808	17.046848
31.378775	1084.428361	17.051866
31.408878	1088.683986	17.056883
31.309000	1081.267412	17.061901
31.604853	1078.276510	17.066919
31.542145	1084.784200	17.071936
31.640624	1081.161484	17.076954
31.427652	1081.724934	17.081971
31.520557	1083.266124	17.086989
31.414264	1079.915339	17.092007
31.868579	1077.587593	17.097024
31.994900	1074.702150	17.102042
31.785330	1075.514382	17.107059
31.861848	1068.581429	17.112077
31.398752	1072.494591	17.117095
31.531789	1072.634591	17.122112
31.550212	1064.988044	17.127130
31.882578	1075.527014	17.132147
31.992610	1080.644296	17.137165
31.607236	1072.303599	17.142183
31.441630	1072.171644	17.147200
31.963305	1087.291710	17.152218
32.140071	1094.011199	17.157235
32.280067	1096.261398	17.162253
32.061085	1099.012822	17.167271
32.103385	1088.064620	17.172288
32.429758	1094.565004	17.177306
32.169344	1104.736106	17.182323
32.631811	1098.717843	17.187341
32.232949	1084.010668	17.192359
31.992645	1078.111988	17.197376
32.047843	1091.380053	17.202394
32.364628	1096.111486	17.207411
32.524993	1098.658304	17.212429
32.351064	1092.730284	17.217447
32.374670	1095.876056	17.222464
32.475847	1097.756787	17.227482
32.407960	1091.540747	17.232499
32.363850	1092.055649	17.237517
32.407289	1092.294896	17.242535
32.470758	1086.881964	17.247552
32.645496	1094.879905	17.252570
31.972181	1093.284267	17.257587
32.507063	1091.398344	17.262605
32.648278	1088.434824	17.267623
32.547160	1089.905424	17.272640
32.855023	1085.126406	17.277658
32.661900	1083.389260	17.282675
32.501801	1093.184868	17.287693
32.581996	1106.256518	17.292711
33.021942	1115.573106	17.297728
33.090700	1113.690782	17.302746
33.113270	1112.068166	17.307763
33.009670	1118.077332	17.312781
33.098794	1116.709383	17.317799
33.154493	1110.382452	17.322816
33.163376	1106.641222	17.327834
32.858674	1107.288474	17.332851
32.945981	1108.486551	17.337869
33.339090	1108.465880	17.342887
33.118642	1119.703732	17.347904
33.287146	1116.874791	17.352922
33.470344	1117.357236	17.357939
33.391039	1109.397769	17.362957
33.183607	1109.777310	17.367975
33.088211	1115.191882	17.372992
33.252429	1110.249166	17.378010
32.934845	1115.928930	17.383027
33.099178	1116.313342	17.388045
33.694409	1121.966859	17.393063
33.408040	1127.408200	17.398080
33.666017	1129.220185	17.403098
33.452906	1134.331304	17.408115
33.875998	1139.961303	17.413133
33.910505	1135.411298	17.418151
33.700798	1136.491805	17.423168
34.035041	1131.957957	17.428186
33.942697	1131.268554	17.433203
33.798587	1127.036879	17.438221
33.793118	1128.063295	17.443239
33.746334	1123.238843	17.448256
34.056680	1129.097948	17.453274
33.812424	1134.305468	17.458291
33.888653	1135.647297	17.463309
34.117964	1136.659021	17.468327
34.068426	1138.411887	17.473344
34.209848	1131.617068	17.478362
34.326878	1132.356041	17.483379
33.791200	1135.665188	17.488397
34.260714	1130.519994	17.493415
34.093705	1130.624951	17.498432
34.105328	1127.814276	17.503450
33.847898	1130.518079	17.508467
33.932095	1123.189415	17.513485
34.273928	1131.047581	17.518503
34.137216	1137.024070	17.523520
34.364166	1146.607582	17.528538
34.546181	1149.671739	17.533555
34.600998	1154.939708	17.538573
34.659305	1156.006628	17.543591
34.830747	1158.419172	17.548608
34.697307	1139.043816	17.553626
34.308640	1138.347189	17.558643
34.805904	1148.020898	17.563661
34.852210	1149.793463	17.568679
34.607965	1138.946930	17.573696
34.788818	1150.320749	17.578714
34.641602	1157.428703	17.583731
34.707656	1158.175663	17.588749
34.884831	1149.762571	17.593767
34.943132	1155.970453	17.598784
35.057653	1150.830378	17.603802
35.169657	1159.699738	17.608819
35.352531	1158.269759	17.613837
35.369600	1143.500524	17.618855
34.545009	1138.387665	17.623872
34.847880	1141.246687	17.628890
34.889536	1150.609917	17.633907
34.725853	1151.541199	17.638925
35.076658	1156.204199	17.643943
34.966015	1165.610234	17.648960
35.009758	1153.487770	17.653978
34.816060	1161.019587	17.658995
35.071528	1153.320084	17.664013
35.381323	1165.629948	17.669031
35.328158	1179.123345	17.674048
35.749546	1171.498827	17.679066
35.325098	1175.677364	17.684083
35.506084	1177.810695	17.689101
35.835551	1167.448633	17.694119
35.661339	1181.099857	17.699136
35.420221	1168.485509	17.704154
35.866301	1167.901100	17.709171
35.344991	1175.802999	17.714189
35.479986	1167.544834	17.719207
35.599790	1176.630738	17.724224
35.330901	1163.563139	17.729242
35.428860	1169.960478	17.734259
35.588172	1163.506838	17.739277
36.237381	1174.494857	17.744295
36.002930	1167.566405	17.749312
35.774980	1169.650194	17.754330
36.160125	1185.356641	17.759347
36.213257	1187.797193	17.764365
36.322447	1167.888314	17.769383
36.074409	1163.341543	17.774400
35.799504	1164.441735	17.779418
35.984290	1188.896180	17.784435
36.043212	1198.351407	17.789453
36.307463	1189.760546	17.794471
36.114607	1187.695133	17.799488
36.569564	1192.013611	17.804506
36.245188	1198.016368	17.809523
36.245027	1194.623686	17.814541
36.198242	1188.517918	17.819559
36.352857	1186.117189	17.824576
36.235953	1187.953201	17.829594
36.413006	1190.046123	17.834611
35.845904	1182.027346	17.839629
36.522451	1200.534777	17.844647
36.796133	1216.896210	17.849664
36.939934	1207.270138	17.854682
36.659465	1213.512181	17.859699
36.666920	1207.498898	17.864717
37.081211	1201.036854	17.869735
36.678210	1210.832712	17.874752
36.973809	1207.725059	17.879770
36.794358	1205.992071	17.884787
36.930725	1215.936963	17.889805
37.060374	1208.326579	17.894823
37.128768	1215.508076	17.899840
36.949607	1199.090595	17.904858
37.174270	1206.200266	17.909875
37.276278	1209.418985	17.914893
37.358673	1201.850722	17.919911
37.107185	1203.559493	17.924928
37.190501	1202.697393	17.929946
37.501855	1200.783363	17.934963
36.768171	1202.555059	17.939981
37.179911	1201.622567	17.944999
37.043442	1204.758724	17.950016
37.366782	1207.725007	17.955034
37.032392	1202.333348	17.960051
37.003663	1204.783572	17.965069
37.687980	1214.172381	17.970087
37.579081	1221.798239	17.975104
37.930042	1218.252707	17.980122
37.781139	1203.083378	17.985139
37.331101	1198.804940	17.990157
37.793073	1204.914878	17.995175
37.723525	1221.465795	18.000192
37.351441	1229.053992	18.005210
37.711010	1225.175739	18.010227
37.519570	1233.742372	18.015245
37.696556	1224.215237	18.020263
37.644682	1228.714121	18.025280
37.915013	1215.233787	18.030298
37.839304	1227.222228	18.035315
37.762561	1226.104328	18.040333
37.962530	1218.915282	18.045351
37.867598	1234.939995	18.050368
38.159256	1243.778093	18.055386
38.766722	1245.727845	18.060403
38.286799	1234.103953	18.065421
38.116561	1229.330374	18.070439
38.291696	1239.537457	18.075456
38.338218	1242.162095	18.080474
38.686628	1244.149278	18.085491
38.494698	1244.289700	18.090509
38.522850	1235.779990	18.095527
38.490770	1238.947136	18.100544
38.054268	1241.574866	18.105562
38.406781	1242.409498	18.110579
38.629953	1238.827176	18.115597
38.779036	1244.500139	18.120615
38.775955	1252.718522	18.125632
38.734960	1253.412829	18.130650
39.111767	1244.558145	18.135667
38.879865	1252.187508	18.140685
38.921914	1254.140637	18.145703
38.626378	1238.574516	18.150720
38.464238	1241.755728	18.155738
39.004788	1242.677667	18.160755
39.056719	1240.895799	18.165773
39.091035	1237.371471	18.170791
38.995436	1240.835757	18.175808
38.580601	1240.095887	18.180826
39.153662	1235.625585	18.185843
39.117418	1239.639169	18.190861
38.993463	1236.553063	18.195879
39.345623	1258.399842	18.200896
39.291532	1263.056879	18.205914
39.566703	1260.419494	18.210931
39.143862	1260.299437	18.215949
39.373049	1253.452950	18.220967
39.612553	1262.731590	18.225984
39.438209	1260.398172	18.231002
39.173925	1258.413372	18.236019
39.275376	1261.679526	18.241037
39.596793	1255.033191	18.246055
39.409634	1261.658277	18.251072
39.511017	1268.051959	18.256090
39.914115	1256.845146	18.261107
39.713486	1261.342098	18.266125
39.562447	1256.852691	18.271143
39.661275	1257.670263	18.276160
39.589440	1257.634072	18.281178
39.937926	1259.902123	18.286195
39.755643	1262.972881	18.291213
39.772716	1268.713873	18.296231
40.058254	1276.975414	18.301248
39.823041	1279.896672	18.306266
39.949960	1278.604843	18.311283
39.994150	1283.117094	18.316301
40.290001	1283.149533	18.321319
40.194055	1277.262884	18.326336
40.157967	1281.819271	18.331354
40.329552	1274.337993	18.336371
40.231687	1286.822269	18.341389
40.092133	1280.734160	18.346407
40.502982	1278.179661	18.351424
40.357176	1274.124948	18.356442
40.500091	1273.329249	18.361459
40.177761	1275.866509	18.366477
40.770484	1278.888432	18.371495
40.695955	1269.277598	18.376512
40.314681	1274.718073	18.381530
40.389864	1278.796261	18.386547
40.793690	1294.562997	18.391565
40.786230	1290.382459	18.396583
40.976569	1295.619769	18.401600
40.880644	1289.688930	18.406618
41.033016	1286.010390	18.411635
41.060413	1302.520946	18.416653
41.276061	1299.886569	18.421671
41.014608	1298.220070	18.426688
41.210855	1300.190073	18.431706
41.375748	1283.866938	18.436723
41.085246	1293.490575	18.441741
41.059831	1297.433044	18.446759
41.203555	1299.079904	18.451776
41.309288	1311.096780	18.456794
41.116335	1304.300634	18.461811
41.089055	1301.499183	18.466829
41.231211	1290.468937	18.471847
40.975404	1291.187432	18.476864
40.856662	1298.189991	18.481882
41.145057	1302.237936	18.486899
41.283447	1312.630706	18.491917
41.334771	1314.629729	18.496935
41.620545	1315.799881	18.501952
41.539386	1308.976750	18.506970
41.523396	1308.174386	18.511987
41.618993	1310.112821	18.517005
41.575973	1317.848323	18.522023
41.797106	1321.556502	18.527040
42.091182	1329.848289	18.532058
42.182979	1322.073367	18.537075
41.935093	1320.199605	18.542093
41.877805	1320.991144	18.547111
42.189125	1316.593391	18.552128
41.972531	1329.721172	18.557146
42.294494	1346.785244	18.562163
42.167017	1343.683891	18.567181
42.085079	1333.502960	18.572199
42.418385	1330.231582	18.577216
42.191285	1335.944577	18.582234
42.357748	1327.166992	18.587251
42.334030	1333.914827	18.592269
42.325248	1340.284767	18.597287
42.441063	1335.343260	18.602304
42.580752	1344.208375	18.607322
42.822560	1333.500174	18.612339
42.552779	1338.011135	18.617357
42.731940	1339.747125	18.622375
42.518592	1336.763373	18.627392
42.282352	1335.320147	18.632410
42.593186	1334.889473	18.637427
42.725743	1338.355903	18.642445
42.905018	1333.022586	18.647463
42.999430	1333.272785	18.652480
42.816479	1332.543919	18.657498
43.027368	1324.684062	18.662515
42.918576	1330.807727	18.667533
42.922231	1332.179877	18.672551
43.354585	1327.450721	18.677568
43.168252	1335.622111	18.682586
42.785658	1327.874173	18.687603
42.792204	1336.930564	18.692621
42.927230	1345.291461	18.697639
43.261743	1352.219871	18.702656
43.203500	1358.338781	18.707674
43.355011	1352.324970	18.712691
43.381932	1357.606838	18.717709
43.072807	1354.669648	18.722727
43.639890	1353.633913	18.727744
43.221377	1353.601542	18.732762
43.315461	1357.500055	18.737779
43.639454	1356.401416	18.742797
43.544699	1355.822839	18.747815
43.669108	1365.968512	18.752832
43.759216	1380.168636	18.757850
43.908877	1378.283076	18.762867
43.995300	1376.344306	18.767885
43.625029	1390.326221	18.772903
44.036450	1377.240244	18.777920
43.928992	1381.334448	18.782938
43.929346	1370.714550	18.787955
43.746662	1375.647394	18.792973
43.973604	1378.003933	18.797991
44.359296	1382.819325	18.803008
44.660782	1379.717033	18.808026
44.219007	1373.199696	18.813043
44.105247	1368.098481	18.818061
43.831013	1379.373326	18.823079
43.977401	1372.492428	18.828096
43.871055	1383.554772	18.833114
44.144562	1391.524748	18.838131
44.525414	1390.631803	18.843149
44.601383	1393.785203	18.848167
44.694285	1389.147086	18.853184
44.458132	1397.783922	18.858202
44.813937	1383.721999	18.863219
44.907524	1387.118802	18.868237
44.790884	1390.980906	18.873255
45.033163	1391.091170	18.878272
44.663892	1391.956840	18.883290
44.948107	1392.833739	18.888307
44.870939	1384.223690	18.893325
44.924294	1389.002787	18.898343
44.975529	1392.466189	18.903360
44.950603	1387.521471	18.908378
45.226896	1384.580922	18.913395
45.106036	1384.486137	18.918413
45.090146	1394.170949	18.923431
45.328457	1403.074292	18.928448
45.236967	1410.069469	18.933466
44.815096	1406.701791	18.938483
45.221230	1416.162696	18.943501
45.012419	1418.631696	18.948519
45.619655	1409.756608	18.953536
45.473480	1412.203170	18.958554
45.272662	1410.653397	18.963571
45.647359	1403.695690	18.968589
45.261767	1417.964062	18.973607
45.513718	1418.394717	18.978624
45.780351	1431.784549	18.983642
45.658205	1443.452192	18.988659
45.931425	1436.825965	18.993677
45.840684	1432.920386	18.998695
46.066335	1433.374098	19.003712
45.983813	1439.105501	19.008730
45.983882	1432.474733	19.013747
45.940191	1429.366550	19.018765
45.786866	1431.362933	19.023783
46.202956	1426.686795	19.028800
46.175797	1437.108731	19.033818
46.237616	1427.312341	19.038835
45.972618	1417.330463	19.043853
46.289435	1434.228160	19.048871
46.459791	1429.000359	19.053888
46.446319	1428.506879	19.058906
46.612914	1426.741744	19.063923
46.219719	1430.135922	19.068941
46.180284	1428.775468	19.073959
46.610141	1448.931343	19.078976
46.819221	1451.966065	19.083994
46.986766	1455.354449	19.089011
46.918364	1445.881422	19.094029
46.938202	1462.125053	19.099047
46.909229	1456.723337	19.104064
47.073752	1453.118602	19.109082
47.260514	1449.920658	19.114099
47.225776	1428.692760	19.119117
47.212400	1429.928725	19.124135
46.996007	1422.337751	19.129152
47.059617	1419.645123	19.134170
47.209223	1425.141328	19.139187
47.304808	1434.590936	19.144205
47.222653	1446.425892	19.149223
46.967551	1449.994108	19.154240
47.362999	1451.124994	19.159258
47.129286	1448.677770	19.164275
47.606358	1443.231488	19.169293
47.088448	1449.400356	19.174311
47.380387	1456.853054	19.179328
47.271222	1449.822808	19.184346
47.476982	1457.361595	19.189363
47.511296	1445.079456	19.194381
47.426064	1469.481913	19.199399
47.823830	1463.628308	19.204416
47.483926	1461.961461	19.209434
47.557792	1466.330246	19.214451
47.861681	1459.929591	19.219469
47.708303	1471.005669	19.224487
47.961249	1471.164757	19.229504
47.950531	1466.230415	19.234522
47.953789	1459.419248	19.239539
48.330160	1471.138198	19.244557
48.119970	1477.214679	19.249575
48.162486	1481.017152	19.254592
48.458258	1492.347936	19.259610
48.037736	1492.893421	19.264627
48.512293	1492.910486	19.269645
48.518517	1492.565404	19.274663
48.867411	1484.431379	19.279680
48.478664	1493.240498	19.284698
48.461526	1488.963595	19.289715
48.773779	1483.577840	19.294733
48.545045	1492.541778	19.299751
48.646179	1481.704044	19.304768
48.377596	1495.130440	19.309786
48.403960	1491.481068	19.314803
48.604931	1482.524423	19.319821
48.810558	1486.698992	19.324839
48.792065	1484.489456	19.329856
49.119192	1492.959186	19.334874
48.851829	1494.541077	19.339891
48.948037	1502.317964	19.344909
48.866471	1516.179001	19.349927
48.944470	1518.268546	19.354944
49.212722	1513.252612	19.359962
48.873011	1509.913069	19.364979
49.298763	1510.505854	19.369997
49.210823	1516.383306	19.375015
49.387636	1508.292010	19.380032
49.602781	1509.889829	19.385050
49.557858	1516.937715	19.390067
49.199286	1510.066447	19.395085
49.469704	1531.071102	19.400103
49.712491	1531.888223	19.405120
49.799225	1536.813616	19.410138
49.740795	1537.958812	19.415155
50.165352	1530.046454	19.420173
50.289183	1539.220279	19.425191
50.244124	1537.564036	19.430208
50.427894	1536.720898	19.435226
50.056569	1532.269091	19.440243
50.111095	1524.234820	19.445261
50.427695	1536.237746	19.450279
50.331298	1524.402088	19.455296
50.355324	1517.306764	19.460314
50.383218	1520.859059	19.465331
50.736597	1514.876686	19.470349
50.543151	1519.946962	19.475367
50.707762	1501.638571	19.480384
50.565039	1500.376349	19.485402
50.250152	1502.315998	19.490419
50.276099	1502.065661	19.495437
50.188042	1529.978072	19.500455
50.511078	1540.436725	19.505472
50.777528	1532.830018	19.510490
50.455925	1528.108477	19.515507
50.750586	1528.844884	19.520525
50.637441	1535.329080	19.525543
50.490230	1535.989542	19.530560
51.037846	1542.726841	19.535578
50.897651	1561.416264	19.540595
51.169635	1559.416842	19.545613
50.819333	1556.091573	19.550631
50.814767	1557.020037	19.555648
51.286475	1556.122317	19.560666
50.730481	1562.347685	19.565683
51.229676	1556.064727	19.570701
51.594683	1563.165177	19.575719
51.200827	1557.814286	19.580736
51.375590	1563.874668	19.585754
51.247133	1571.699408	19.590771
51.527007	1582.347895	19.595789
51.508074	1582.300259	19.600807
51.407022	1579.986874	19.605824
51.604880	1577.049116	19.610842
51.676956	1586.925388	19.615859
52.163608	1571.747694	19.620877
51.416451	1588.594473	19.625895
51.339528	1577.992871	19.630912
51.978120	1592.586938	19.635930
51.798385	1604.216368	19.640947
52.511747	1588.968425	19.645965
52.456491	1598.299733	19.650983
52.589511	1606.626350	19.656000
52.195256	1585.612392	19.661018
51.880860	1583.783737	19.666035
52.051753	1586.897052	19.671053
52.015472	1602.095507	19.676071
52.200660	1606.544721	19.681088
52.392351	1594.566045	19.686106
52.343785	1597.786333	19.691123
52.205374	1590.463952	19.696141
52.402061	1612.739489	19.701159
52.281096	1619.471107	19.706176
52.965885	1608.791174	19.711194
52.784920	1623.523138	19.716211
52.768677	1622.155880	19.721229
52.700159	1614.835162	19.726247
52.646371	1615.888112	19.731264
52.753546	1616.483474	19.736282
52.554622	1628.658755	19.741299
53.150344	1632.387211	19.746317
53.084371	1637.929882	19.751335
52.968866	1646.992928	19.756352
53.604214	1640.511874	19.761370
53.499981	1644.132234	19.766387
53.722968	1634.970081	19.771405
53.685500	1630.740513	19.776423
53.459202	1635.677105	19.781440
53.822704	1624.848674	19.786458
53.819815	1638.454468	19.791475
53.625644	1631.718351	19.796493
53.767541	1636.183823	19.801511
53.513057	1629.094218	19.806528
53.869616	1618.901231	19.811546
53.963329	1632.741208	19.816563
53.579405	1626.968994	19.821581
53.921246	1627.401351	19.826599
53.526561	1631.821495	19.831616
53.493898	1628.455915	19.836634
53.916272	1645.444577	19.841651
53.874997	1641.562762	19.846669
54.325591	1651.487069	19.851687
54.314549	1656.819157	19.856704
53.955644	1644.396506	19.861722
53.871405	1655.692253	19.866739
54.094492	1666.210823	19.871757
54.233673	1673.330918	19.876775
54.092513	1679.627040	19.881792
54.646487	1666.827805	19.886810
54.210556	1677.430697	19.891827
54.600248	1694.380342	19.896845
54.837590	1701.399857	19.901863
55.297307	1697.572089	19.906880
55.737078	1702.218140	19.911898
55.146767	1684.712691	19.916915
55.125028	1676.384169	19.921933
55.449902	1670.999536	19.926951
55.165588	1671.624677	19.931968
55.415848	1667.343709	19.936986
55.014492	1670.991690	19.942003
55.342871	1670.567728	19.947021
55.327137	1664.763063	19.952039
54.905677	1670.361440	19.957056
55.436705	1675.671725	19.962074
55.613529	1686.380602	19.967091
55.626659	1694.240021	19.972109
55.884379	1693.423162	19.977127
55.673783	1703.927645	19.982144
55.952562	1682.792345	19.987162
55.588758	1691.704956	19.992179
55.776651	1688.184881	19.997197
55.783692	1689.625961	20.002215
55.619326	1687.183619	20.007232
55.819068	1690.532287	20.012250
55.877497	1690.728166	20.017267
55.634716	1687.370247	20.022285
56.069957	1681.201414	20.027303
55.825503	1698.502897	20.032320
56.186990	1698.553458	20.037338
56.083416	1716.669225	20.042355
56.349019	1709.491793	20.047373
56.310553	1707.897622	20.052391
56.277490	1719.437870	20.057408
56.659110	1705.731436	20.062426
56.455524	1709.480991	20.067443
56.137443	1710.092487	20.072461
56.471032	1718.488725	20.077479
56.677382	1722.303452	20.082496
56.682217	1732.859412	20.087514
56.537872	1728.848550	20.092531
56.980467	1733.838171	20.097549
57.287755	1728.150145	20.102567
57.164894	1731.186425	20.107584
57.496631	1732.605041	20.112602
56.971452	1734.233657	20.117619
56.974209	1724.790361	20.122637
56.923928	1728.657922	20.127655
57.173201	1726.355908	20.132672
57.294710	1723.297535	20.137690
57.087191	1741.110856	20.142707
56.957359	1746.546794	20.147725
57.458746	1744.464070	20.152743
57.467094	1754.833288	20.157760
57.531707	1750.783371	20.162778
57.478797	1751.145026	20.167795
57.634447	1758.249951	20.172813
58.053713	1757.963236	20.177831
57.864705	1780.861180	20.182848
58.463069	1765.874117	20.187866
58.427340	1769.064021	20.192883
57.805114	1757.872361	20.197901
58.245502	1762.366844	20.202919
58.060427	1766.924604	20.207936
58.557092	1759.540526	20.212954
58.606762	1767.637265	20.217971
58.678373	1767.761647	20.222989
58.725613	1762.761334	20.228007
58.578414	1757.403298	20.233024
58.574119	1756.292950	20.238042
58.984282	1747.710522	20.243059
58.810890	1757.757900	20.248077
58.985586	1746.438235	20.253095
58.452459	1745.786306	20.258112
58.449313	1744.944039	20.263130
58.703989	1749.366622	20.268147
58.616623	1769.263046	20.273165
59.084031	1771.234802	20.278183
59.017072	1778.532412	20.283200
58.638776	1762.764190	20.288218
59.100193	1760.258510	20.293235
58.805439	1763.369067	20.298253
59.160695	1779.099657	20.303271
59.292593	1782.411633	20.308288
59.341636	1782.571111	20.313306
59.353767	1792.643093	20.318323
59.329031	1789.879039	20.323341
59.595556	1791.768654	20.328359
59.504322	1792.467696	20.333376
59.438057	1783.413905	20.338394
59.492611	1782.597313	20.343411
59.200664	1790.567691	20.348429
59.427245	1800.950085	20.353447
59.411173	1818.051789	20.358464
59.927529	1815.326041	20.363482
59.625600	1809.913330	20.368499
59.760516	1816.595464	20.373517
60.065170	1830.932757	20.378535
60.219539	1843.169604	20.383552
60.430214	1832.144071	20.388570
60.193480	1838.483626	20.393587
60.304251	1834.246565	20.398605
60.578169	1830.757169	20.403623
60.513733	1836.855120	20.408640
60.690976	1834.125691	20.413658
60.814972	1830.372586	20.418675
60.782505	1835.802764	20.423693
60.913322	1830.590509	20.428711
60.538682	1837.428229	20.433728
60.648841	1828.431988	20.438746
60.937162	1827.130613	20.443763
60.857938	1851.475839	20.448781
60.939617	1858.825939	20.453799
61.085264	1856.660073	20.458816
60.788659	1862.396748	20.463834
61.185810	1861.892575	20.468851
61.068473	1854.945506	20.473869
61.077311	1845.526443	20.478887
61.287872	1857.814461	20.483904
61.527173	1865.206144	20.488922
61.902261	1876.982371	20.493939
61.915675	1881.067218	20.498957
61.892054	1878.426061	20.503975
61.897949	1884.509853	20.508992
61.809970	1871.858391	20.514010
62.365614	1874.573782	20.519027
61.923351	1872.582080	20.524045
61.981033	1866.153579	20.529063
62.133511	1862.295012	20.534080
61.753251	1864.551076	20.539098
61.877157	1863.758330	20.544115
62.187652	1877.536128	20.549133
62.138057	1863.357454	20.554151
62.181367	1868.144564	20.559168
62.235608	1870.092695	20.564186
62.305034	1869.459974	20.569203
62.175209	1896.464252	20.574221
62.612000	1894.278015	20.579239
62.299288	1903.368931	20.584256
62.614889	1899.241785	20.589274
62.923208	1897.710039	20.594291
62.350726	1891.310826	20.599309
62.844354	1886.818095	20.604327
62.595573	1903.994213	20.609344
62.612525	1911.692170	20.614362
63.011067	1923.802448	20.619379
63.000480	1924.589853	20.624397
63.454688	1923.698015	20.629415
62.881515	1923.595191	20.634432
63.243350	1923.405841	20.639450
63.412258	1917.685783	20.644467
63.222459	1931.040196	20.649485
63.542541	1930.993097	20.654503
63.446625	1941.694362	20.659520
63.415557	1943.684272	20.664538
63.786096	1941.480005	20.669555
63.818268	1942.251243	20.674573
64.030528	1933.406222	20.679591
64.295125	1934.248351	20.684608
64.198694	1941.276069	20.689626
64.258227	1936.917614	20.694643
64.137998	1937.245636	20.699661
64.429926	1936.865252	20.704679
64.117170	1936.204037	20.709696
64.375286	1931.625109	20.714714
64.293810	1939.950771	20.719731
64.269174	1935.917951	20.724749
64.505806	1930.487102	20.729767
64.499429	1944.014774	20.734784
64.600543	1941.997897	20.739802
64.904561	1941.378916	20.744819
64.563582	1937.951120	20.749837
64.796042	1940.865489	20.754855
64.571093	1931.533506	20.759872
64.794878	1952.009434	20.764890
64.965209	1959.692851	20.769907
64.945866	1966.235095	20.774925
65.029578	1962.469338	20.779943
65.124231	1961.188828	20.784960
64.860072	1961.233264	20.789978
65.206981	1963.968748	20.794995
65.313335	1966.006562	20.800013
65.151590	1971.131963	20.805031
65.326462	1982.557746	20.810048
65.576077	1987.716540	20.815066
65.736750	1986.286819	20.820083
65.401360	1990.274850	20.825101
65.841763	1989.858579	20.830119
65.727293	1987.430470	20.835136
65.746421	1983.296101	20.840154
66.289586	1984.274483	20.845171
66.047435	1987.326339	20.850189
66.138540	1979.677483	20.855207
65.959867	1987.661762	20.860224
66.006990	1998.290154	20.865242
66.158683	2003.278087	20.870259
66.130996	2006.842342	20.875277
65.963277	1999.546477	20.880295
66.503820	2004.060046	20.885312
66.508970	2008.215651	20.890330
66.496240	2008.157574	20.895347
66.603341	2023.879918	20.900365
66.598528	2019.531524	20.905383
66.688346	2024.503909	20.910400
66.571202	2023.789951	20.915418
66.969276	2024.241914	20.920435
66.705052	2028.045220	20.925453
66.633353	2022.586906	20.930471
67.283296	2029.545063	20.935488
66.976929	2033.626393	20.940506
67.370620	2036.218848	20.945523
67.257907	2041.178784	20.950541
67.529803	2040.470151	20.955559
67.325210	2040.012910	20.960576
67.403499	2044.744090	20.965594
67.660159	2037.741512	20.970611
67.495091	2039.032845	20.975629
67.670115	2038.402510	20.980647
67.853873	2041.040481	20.985664
67.878612	2051.975393	20.990682
68.195620	2065.146352	20.995699
68.139076	2063.365618	21.000717
67.953289	2069.757238	21.005735
68.195511	2066.834542	21.010752
68.171363	2058.831294	21.015770
68.311336	2057.335377	21.020787
68.197723	2060.247177	21.025805
68.477805	2062.620731	21.030823
68.485674	2050.010936	21.035840
68.526803	2059.374724	21.040858
68.370475	2051.736198	21.045875
68.533034	2055.516829	21.050893
68.594370	2058.028804	21.055911
68.806131	2062.590743	21.060928
68.682667	2072.163377	21.065946
68.738032	2083.197659	21.070963
68.645712	2086.273399	21.075981
69.280489	2082.964123	21.080999
69.333770	2087.478308	21.086016
69.242370	2085.081288	21.091034
69.320495	2082.231640	21.096051
69.481316	2090.986508	21.101069
69.696561	2095.421667	21.106087
69.560710	2082.739684	21.111104
69.209918	2095.074785	21.116122
69.473297	2089.175756	21.121139
69.608186	2104.903286	21.126157
69.829594	2104.281463	21.131175
70.136193	2105.145424	21.136192
69.887054	2116.817619	21.141210
70.001519	2114.183197	21.146227
70.095403	2112.950139	21.151245
70.015281	2113.647452	21.156263
70.270756	2106.455668	21.161280
69.896318	2109.859658	21.166298
70.444378	2108.340830	21.171315
70.370687	2114.131031	21.176333
70.223857	2120.200958	21.181351
70.624667	2117.761535	21.186368
70.427037	2136.075513	21.191386
70.593182	2115.800022	21.196403
70.699476	2122.881264	21.201421
70.498340	2118.068102	21.206439
70.696295	2117.967547	21.211456
70.950961	2139.758090	21.216474
70.986773	2138.597250	21.221491
70.945960	2144.470679	21.226509
71.110691	2146.903345	21.231527
71.054717	2150.393159	21.236544
70.949255	2144.053241	21.241562
71.187612	2144.167281	21.246579
71.182409	2160.904660	21.251597
71.200879	2170.272056	21.256615
71.959876	2159.024705	21.261632
71.705995	2169.703513	21.266650
72.080953	2168.098182	21.271667
72.039534	2176.038948	21.276685
71.613316	2162.218871	21.281703
71.737990	2159.690150	21.286720
71.858969	2163.480474	21.291738
71.987205	2161.096375	21.296755
72.129256	2177.040615	21.301773
72.330391	2182.339616	21.306791
72.534897	2190.945665	21.311808
72.491505	2192.571428	21.316826
72.512612	2189.610765	21.321843
72.846363	2193.254141	21.326861
72.901688	2194.110133	21.331879
72.984790	2184.729754	21.336896
72.656236	2192.762855	21.341914
72.556208	2199.068494	21.346931
72.649411	2193.855715	21.351949
72.756704	2183.120743	21.356967
72.916031	2184.822051	21.361984
72.809416	2184.848116	21.367002
72.861159	2181.324028	21.372019
73.019353	2200.469183	21.377037
73.122027	2217.145528	21.382055
73.164069	2214.853828	21.387072
73.451487	2219.672221	21.392090
73.548910	2209.655212	21.397107
73.296184	2203.268910	21.402125
73.243078	2216.412753	21.407143
73.562715	2232.038860	21.412160
73.717284	2234.706682	21.417178
73.691043	2237.087222	21.422195
74.129523	2239.486481	21.427213
74.575848	2237.099877	21.432231
74.456618	2235.846546	21.437248
74.178315	2232.727639	21.442266
73.927104	2231.861092	21.447283
74.194524	2232.642828	21.452301
74.036999	2231.663764	21.457319
74.597528	2240.715877	21.462336
74.751769	2254.089218	21.467354
74.999578	2262.884195	21.472371
74.677784	2252.475207	21.477389
74.768475	2263.403071	21.482407
75.045002	2252.815129	21.487424
75.110084	2263.444020	21.492442
75.125997	2250.990628	21.497459
75.218922	2252.535073	21.502477
75.075225	2257.462050	21.507495
74.825678	2254.546936	21.512512
75.001291	2264.722970	21.517530
75.022127	2268.289143	21.522547
75.619772	2276.224513	21.527565
75.482388	2282.419258	21.532583
75.727583	2273.142838	21.537600
75.663391	2284.943971	21.542618
75.527559	2284.826277	21.547635
75.843241	2272.673075	21.552653
75.649649	2282.259963	21.557671
75.862624	2288.043180	21.562688
76.241055	2302.811147	21.567706
76.309529	2301.739862	21.572723
76.197132	2302.208687	21.577741
75.887634	2316.156549	21.582759
76.026688	2301.973221	21.587776
76.085756	2306.035232	21.592794
76.432638	2316.563195	21.597811
76.695499	2319.842128	21.602829
76.283634	2330.523690	21.607847
76.603959	2324.906025	21.612864
76.411903	2330.563346	21.617882
76.768615	2331.908664	21.622899
77.208995	2340.354743	21.627917
76.989296	2348.067871	21.632935
77.276692	2350.591811	21.637952
77.210993	2350.655652	21.642970
77.280340	2348.694204	21.647987
77.532155	2346.918784	21.653005
77.408689	2345.795509	21.658023
77.727771	2350.577416	21.663040
77.348015	2355.181606	21.668058
77.438863	2339.292033	21.673075
77.644237	2342.538947	21.678093
77.280890	2352.805783	21.683111
78.032931	2365.994022	21.688128
77.915829	2365.182204	21.693146
77.759134	2373.440948	21.698163
78.102909	2365.818620	21.703181
77.957739	2371.976743	21.708199
78.199017	2370.755292	21.713216
78.527778	2370.075611	21.718234
78.339476	2369.505344	21.723251
78.629902	2361.269622	21.728269
78.461899	2378.247325	21.733287
78.331067	2388.433567	21.738304
78.800978	2390.414471	21.743322
78.904404	2382.290096	21.748339
78.926209	2381.996210	21.753357
78.825920	2393.519019	21.758375
78.861809	2396.909273	21.763392
78.668574	2390.384183	21.768410
79.089270	2404.646946	21.773427
79.491065	2402.627095	21.778445
79.275198	2408.016744	21.783463
79.474699	2404.841885	21.788480
79.591374	2411.908990	21.793498
79.515679	2408.660470	21.798515
79.853608	2404.400311	21.803533
79.464095	2405.635306	21.808551
79.827524	2402.535761	21.813568
79.804173	2413.030258	21.818586
80.100866	2431.813099	21.823603
80.504634	2425.210244	21.828621
80.077953	2431.731260	21.833639
80.140156	2427.173433	21.838656
80.457499	2429.241367	21.843674
80.174408	2429.910525	21.848691
80.729557	2412.347989	21.853709
80.343034	2423.634767	21.858727
80.143687	2431.682448	21.863744
80.362081	2438.395921	21.868762
80.510045	2450.438507	21.873779
81.139472	2441.875053	21.878797
80.827984	2447.816237	21.883815
80.948476	2449.599402	21.888832
81.133866	2447.288369	21.893850
81.359971	2461.029341	21.898867
81.677330	2464.994111	21.903885
81.663476	2467.824069	21.908903
81.579128	2461.572257	21.913920
81.855031	2468.923739	21.918938
81.557826	2474.941597	21.923955
82.238923	2467.155914	21.928973
81.855061	2473.755452	21.933991
81.953733	2468.301871	21.939008
82.002990	2463.556695	21.944026
81.898404	2468.064148	21.949043
81.983870	2469.142673	21.954061
81.725124	2469.429282	21.959079
82.093126	2462.535340	21.964096
81.824760	2476.931365	21.969114
82.085522	2481.217463	21.974131
82.128111	2487.671291	21.979149
82.526682	2495.745257	21.984167
82.259513	2496.203618	21.989184
82.613391	2510.719955	21.994202
82.672843	2519.146895	21.999219
82.823275	2518.772889	22.004237
82.803614	2514.404608	22.009255
82.677100	2516.377973	22.014272
82.969907	2509.593635	22.019290
83.094627	2538.840885	22.024307
83.551901	2531.273297	22.029325
83.414212	2533.147418	22.034343
83.509361	2538.377914	22.039360
83.783271	2534.329748	22.044378
83.696387	2544.048395	22.049395
83.628277	2539.308962	22.054413
83.440584	2545.205534	22.059431
83.539990	2538.928063	22.064448
83.962862	2543.087782	22.069466
83.940598	2562.738173	22.074483
83.891065	2555.903299	22.079501
84.064356	2564.328206	22.084519
84.242096	2558.297259	22.089536
84.434856	2561.132735	22.094554
84.428758	2555.932253	22.099571
84.259932	2559.796471	22.104589
84.385773	2572.050910	22.109607
84.681233	2578.136913	22.114624
85.096074	2587.246745	22.119642
84.870739	2587.401875	22.124659
85.079566	2585.898285	22.129677
85.014644	2584.828945	22.134695
84.866995	2579.899969	22.139712
85.596211	2588.988954	22.144730
85.279360	2605.639858	22.149747
85.712672	2598.120183	22.154765
85.710654	2598.656939	22.159783
85.856887	2605.829955	22.164800
85.806159	2600.958380	22.169818
85.871620	2604.852181	22.174835
85.878663	2594.533502	22.179853
85.925160	2597.019472	22.184871
85.752066	2597.444159	22.189888
85.974220	2598.147788	22.194906
85.793226	2600.047637	22.199923
86.087798	2604.281125	22.204941
86.195142	2619.969236	22.209959
86.211802	2612.009847	22.214976
86.147644	2619.244235	22.219994
86.217616	2630.791020	22.225011
86.632076	2642.381681	22.230029
86.601730	2642.919720	22.235047
86.439182	2653.249952	22.240064
86.823153	2647.360255	22.245082
86.874100	2649.283738	22.250099
87.362063	2666.723895	22.255117
87.342944	2675.380993	22.260135
87.194861	2677.730182	22.265152
87.633351	2673.331115	22.270170
87.255152	2674.567511	22.275187
87.780964	2663.558377	22.280205
87.782175	2671.319093	22.285223
87.335333	2668.958745	22.290240
87.280487	2675.099664	22.295258
87.951707	2683.260402	22.300275
88.293951	2682.799530	22.305293
88.102991	2695.649703	22.310311
87.986614	2696.153880	22.315328
88.307253	2691.656494	22.320346
88.386362	2699.682761	22.325363
88.607399	2692.792820	22.330381
87.926615	2694.830949	22.335399
87.951449	2703.017217	22.340416
88.707826	2712.537561	22.345434
88.493661	2722.411962	22.350451
88.659535	2713.185617	22.355469
88.949379	2713.200068	22.360487
88.991663	2732.237702	22.365504
89.445481	2729.685740	22.370522
89.366786	2741.195920	22.375539
89.710884	2738.313967	22.380557
89.693403	2740.058809	22.385575
89.378829	2733.117052	22.390592
89.956183	2727.638897	22.395610
89.518367	2737.358973	22.400627
89.574141	2729.204034	22.405645
89.639744	2740.511703	22.410663
89.628895	2735.406600	22.415680
90.188272	2735.527163	22.420698
90.075827	2745.054240	22.425715
90.062073	2752.173475	22.430733
90.411125	2752.427988	22.435751
90.292648	2759.696193	22.440768
90.468327	2755.660211	22.445786
90.310029	2755.773278	22.450803
90.240383	2750.251297	22.455821
90.528393	2760.993897	22.460839
90.812291	2780.176787	22.465856
90.733521	2776.654093	22.470874
90.874168	2786.671780	22.475891
90.850907	2783.515974	22.480909
91.453391	2790.639676	22.485927
91.146058	2800.636026	22.490944
91.475391	2802.064576	22.495962
91.475290	2809.667748	22.500979
91.836325	2797.507089	22.505997
91.528241	2807.721337	22.511015
91.809119	2804.085481	22.516032
91.946835	2799.869222	22.521050
91.660999	2804.282063	22.526067
92.043196	2797.044903	22.531085
92.027366	2810.880858	22.536103
91.962737	2823.544052	22.541120
92.051529	2814.986220	22.546138
92.042064	2822.720269	22.551155
91.940995	2830.658044	22.556173
92.716774	2832.619484	22.561191
92.486188	2842.404993	22.566208
92.580749	2838.984535	22.571226
92.522957	2855.503553	22.576243
92.572570	2851.547269	22.581261
92.768211	2861.468008	22.586279
93.117977	2862.656646	22.591296
93.252882	2861.284550	22.596314
93.082723	2862.668268	22.601331
93.043279	2878.193385	22.606349
93.152469	2879.508089	22.611367
93.160658	2887.637081	22.616384
93.546583	2892.831593	22.621402
93.659021	2901.547094	22.626419
94.023263	2900.296876	22.631437
93.957873	2914.055456	22.636455
94.023153	2919.385429	22.641472
94.120039	2918.798869	22.646490
94.216687	2906.291345	22.651507
94.430280	2905.323538	22.656525
94.434241	2907.582655	22.661543
94.501575	2913.508828	22.666560
94.859151	2910.201805	22.671578
94.932165	2908.615311	22.676595
94.838207	2906.392173	22.681613
95.001295	2927.118595	22.686631
94.920672	2931.789688	22.691648
94.873562	2934.640710	22.696666
94.843810	2929.500638	22.701683
95.092048	2931.077621	22.706701
95.541193	2935.337471	22.711719
95.272281	2928.552606	22.716736
95.577283	2936.969678	22.721754
95.658587	2942.107774	22.726771
95.689971	2954.086900	22.731789
96.022088	2955.735962	22.736807
95.911307	2950.384487	22.741824
95.865680	2950.268436	22.746842
96.067361	2950.467136	22.751859
95.761808	2962.019310	22.756877
96.410152	2968.744528	22.761895
96.119155	2978.549043	22.766912
96.484741	2979.110280	22.771930
96.629931	2989.244148	22.776947
96.443582	2981.310088	22.781965
96.667222	2977.998787	22.786983
96.886937	2985.744343	22.792000
96.806329	2997.438046	22.797018
97.339077	3002.114061	22.802035
97.314848	3001.533848	22.807053
97.219852	2999.029957	22.812071
97.122135	2999.190346	22.817088
97.531763	2996.547428	22.822106
97.688509	3008.156609	22.827123
97.338370	3016.303923	22.832141
97.926993	3012.922809	22.837159
97.706462	3016.053511	22.842176
98.017804	3026.549585	22.847194
98.031450	3021.412157	22.852211
97.905144	3021.665399	22.857229
98.102053	3015.164176	22.862247
97.840433	3044.245526	22.867264
98.149129	3048.701000	22.872282
98.341257	3040.003779	22.877299
98.334053	3056.041620	22.882317
98.488419	3071.344008	22.887335
98.719268	3065.377167	22.892352
98.526409	3067.253673	22.897370
99.085668	3077.496312	22.902387
98.933845	3080.464761	22.907405
99.286902	3077.874882	22.912423
99.161538	3090.566716	22.917440
99.159431	3081.445407	22.922458
99.354757	3089.444172	22.927475
99.628174	3096.903614	22.932493
99.900437	3113.301721	22.937511
99.766586	3112.394648	22.942528
99.630807	3109.998131	22.947546
99.962755	3112.641451	22.952563
99.790664	3112.958680	22.957581
100.764107	3128.224324	22.962599
100.727564	3135.808093	22.967616
100.751580	3134.090381	22.972634
100.874853	3141.456583	22.977651
100.674389	3140.149633	22.982669
101.206291	3135.208727	22.987687
100.875068	3145.275290	22.992704
101.215220	3126.596872	22.997722
101.137625	3138.889881	23.002739
100.838458	3143.854081	23.007757
101.499447	3134.733015	23.012775
101.366126	3136.398201	23.017792
101.452924	3128.629595	23.022810
101.306561	3128.371513	23.027827
101.175670	3136.935875	23.032845
101.661189	3139.031202	23.037863
101.488389	3156.796294	23.042880
101.823495	3152.274435	23.047898
101.789495	3154.773093	23.052915
101.852374	3171.323994	23.057933
102.173090	3170.355172	23.062951
102.140735	3182.817873	23.067968
102.013740	3178.245310	23.072986
102.450165	3170.349318	23.078003
102.256892	3177.320095	23.083021
102.467394	3193.671138	23.088039
102.488116	3201.962434	23.093056
102.643493	3205.842278	23.098074
102.964864	3203.778129	23.103091
103.009083	3222.588726	23.108109
103.279916	3214.062155	23.113127
103.189922	3234.901175	23.118144
103.468942	3226.464847	23.123162
103.699241	3224.175087	23.128179
103.667866	3227.623380	23.133197
104.041804	3222.413666	23.138215
104.056256	3222.720609	23.143232
104.002562	3241.085751	23.148250
104.280265	3238.277248	23.153267
104.527070	3257.712647	23.158285
104.612054	3241.602259	23.163303
104.405301	3241.962795	23.168320
104.505126	3241.069607	23.173338
104.574774	3242.374752	23.178355
104.990112	3256.566438	23.183373
104.722868	3248.130462	23.188391
104.718697	3246.770658	23.193408
104.695523	3258.616501	23.198426
105.083324	3259.679270	23.203443
105.031531	3264.409058	23.208461
105.045011	3267.301140	23.213479
105.332084	3265.425421	23.218496
105.220465	3288.679282	23.223514
105.794534	3290.722879	23.228531
105.472275	3294.604978	23.233549
105.759794	3291.198393	23.238567
105.656756	3310.758096	23.243584
105.877655	3314.233164	23.248602
105.992777	3316.954672	23.253619
105.761617	3324.007192	23.258637
106.104441	3334.637390	23.263655
106.614248	3345.481311	23.268672
106.216765	3348.434634	23.273690
106.959715	3335.995998	23.278707
106.994184	3341.810678	23.283725
106.978588	3340.209622	23.288743
107.046522	3352.429477	23.293760
106.988382	3363.864237	23.298778
107.018443	3368.660136	23.303795
107.122354	3370.928903	23.308813
107.444808	3369.707294	23.313831
107.549367	3368.756545	23.318848
107.358175	3385.025505	23.323866
108.050428	3387.397790	23.328883
107.854313	3399.400228	23.333901
108.286478	3390.002412	23.338919
108.221948	3402.457681	23.343936
108.345640	3394.885184	23.348954
108.286999	3387.865200	23.353971
108.129689	3400.937855	23.358989
108.307903	3402.557414	23.364007
108.631864	3422.059810	23.369024
108.268854	3414.001734	23.374042
108.681215	3408.293566	23.379059
108.863707	3415.893637	23.384077
108.853763	3429.501890	23.389095
108.944866	3439.855957	23.394112
108.902585	3441.380655	23.399130
109.499634	3432.338898	23.404147
109.358245	3448.631675	23.409165
109.578153	3450.677120	23.414183
109.437501	3459.082192	23.419200
109.378500	3471.811240	23.424218
109.886139	3463.061230	23.429235
110.037980	3469.536169	23.434253
109.929209	3469.982361	23.439271
110.093016	3483.099456	23.444288
110.271663	3484.068754	23.449306
110.420207	3474.046192	23.454323
110.363317	3479.344969	23.459341
110.726810	3487.140811	23.464359
110.644187	3497.080245	23.469376
110.902138	3512.843383	23.474394
110.845831	3506.498439	23.479411
111.224607	3502.117998	23.484429
111.374560	3508.094549	23.489447
111.329283	3508.982147	23.494464
111.606765	3528.018492	23.499482
111.684464	3524.559515	23.504499
111.681724	3534.663208	23.509517
112.196320	3533.607179	23.514535
111.957792	3533.571846	23.519552
112.179760	3530.005045	23.524570
112.037386	3519.614557	23.529587
112.288487	3531.761648	23.534605
112.690937	3537.982719	23.539623
112.527779	3551.198433	23.544640
112.100685	3548.137325	23.549658
112.422042	3541.859453	23.554675
112.700380	3541.654768	23.559693
112.910318	3566.427299	23.564711
112.965616	3571.209828	23.569728
113.197406	3575.156689	23.574746
113.301164	3570.895070	23.579763
113.197422	3568.550286	23.584781
113.021234	3571.049184	23.589799
113.624084	3595.330938	23.594816
113.193414	3602.411666	23.599834
113.453479	3590.433581	23.604851
114.052667	3611.351286	23.609869
113.885821	3617.828860	23.614887
114.079221	3609.184825	23.619904
114.354108	3619.093566	23.624922
114.286999	3620.240253	23.629939
114.285320	3628.863512	23.634957
114.567038	3641.788652	23.639975
114.862604	3638.778440	23.644992
114.707399	3648.700921	23.650010
115.283217	3635.117264	23.655027
114.883866	3651.393824	23.660045
115.355589	3656.347861	23.665063
115.827450	3677.490752	23.670080
115.119290	3675.499467	23.675098
115.323100	3671.695601	23.680115
115.425093	3669.684708	23.685133
115.592465	3680.812893	23.690151
116.054403	3686.952100	23.695168
115.945361	3700.762307	23.700186
116.312091	3694.622466	23.705203
116.105103	3701.201050	23.710221
116.026717	3705.442729	23.715239
116.396546	3701.016298	23.720256
116.460558	3714.884624	23.725274
117.006896	3710.452632	23.730291
116.791484	3724.042795	23.735309
116.939986	3720.528500	23.740327
116.831237	3718.998819	23.745344
116.681514	3720.518278	23.750362
117.072280	3714.418855	23.755379
117.422350	3729.842646	23.760397
117.210780	3737.457244	23.765415
117.826695	3733.497268	23.770432
117.545157	3735.223605	23.775450
117.420788	3736.710687	23.780467
117.826945	3762.478560	23.785485
117.423148	3765.186743	23.790503
117.897736	3765.920311	23.795520
118.238486	3791.647971	23.800538
118.439237	3790.975672	23.805555
118.599033	3801.009861	23.810573
118.388695	3793.757820	23.815591
118.560221	3787.815817	23.820608
118.735524	3812.808744	23.825626
118.655539	3807.417470	23.830643
118.886499	3813.466653	23.835661
119.307191	3826.209177	23.840679
119.432689	3820.810958	23.845696
119.788414	3838.190904	23.850714
119.677376	3835.036041	23.855731
119.386428	3833.979943	23.860749
119.667077	3832.809044	23.865767
119.932390	3847.343493	23.870784
120.143906	3857.644214	23.875802
120.317051	3857.235060	23.880819
120.412621	3866.363999	23.885837
120.203505	3860.939281	23.890855
120.536802	3873.572432	23.895872
120.511640	3884.260606	23.900890
121.017112	3879.475149	23.905907
120.739716	3882.529685	23.910925
120.946154	3885.669397	23.915943
121.273997	3894.032837	23.920960
121.487557	3905.166549	23.925978
121.642722	3911.426492	23.930995
121.360636	3904.829549	23.936013
121.956760	3914.606060	23.941031
121.662871	3903.390021	23.946048
121.971423	3916.339560	23.951066
121.954749	3914.113659	23.956083
122.185660	3926.254709	23.961101
121.645783	3930.619243	23.966119
122.040976	3933.858803	23.971136
122.120626	3945.322846	23.976154
122.512680	3949.926462	23.981171
122.419280	3945.275844	23.986189
122.748003	3962.360282	23.991207
123.118122	3969.782842	23.996224
123.204175	3980.201137	24.001242
123.147301	3974.556838	24.006259
123.517412	3972.800607	24.011277
123.521996	3988.998404	24.016295
124.045871	3996.390573	24.021312
123.854771	4006.243119	24.026330
124.042783	3993.426986	24.031347
124.168249	3992.589716	24.036365
124.204594	3997.864569	24.041383
124.519678	3991.985232	24.046400
124.199625	4000.159835	24.051418
124.763769	3992.874759	24.056435
124.670228	3989.786568	24.061453
125.006675	4007.254920	24.066471
124.878741	4009.446460	24.071488
124.960804	4017.797960	24.076506
124.849404	4015.359625	24.081523
125.060422	4009.348235	24.086541
125.127693	4010.505458	24.091559
125.739592	4028.956507	24.096576
125.347565	4036.100789	24.101594
125.482150	4038.838296	24.106611
125.859241	4038.100485	24.111629
125.546566	4041.990709	24.116647
126.046295	4059.626072	24.121664
126.237170	4067.600717	24.126682
126.425341	4069.654362	24.131699
126.450149	4068.069007	24.136717
126.192884	4066.126979	24.141735
126.484940	4080.436476	24.146752
126.788892	4093.835074	24.151770
127.003195	4087.245521	24.156787
126.741229	4092.137864	24.161805
126.878519	4115.981917	24.166823
127.275109	4116.449957	24.171840
127.025873	4120.472298	24.176858
127.342016	4137.075941	24.181875
127.658957	4137.114560	24.186893
127.528407	4144.748199	24.191911
127.951988	4153.033632	24.196928
128.348715	4167.775013	24.201946
128.110784	4170.993861	24.206963
128.631702	4166.363732	24.211981
128.405954	4178.361857	24.216999
128.733799	4171.350462	24.222016
128.498477	4181.538299	24.227034
128.760282	4190.284681	24.232051
128.780671	4190.268754	24.237069
128.868686	4194.418193	24.242087
129.418881	4196.456169	24.247104
129.165201	4217.486096	24.252122
129.289847	4220.007394	24.257139
129.463346	4222.113857	24.262157
129.891620	4244.331117	24.267175
130.007356	4246.497136	24.272192
130.114858	4237.758941	24.277210
130.164715	4242.529874	24.282227
130.144105	4247.532799	24.287245
130.346017	4267.443471	24.292263
130.841007	4262.504891	24.297280
130.657382	4268.300377	24.302298
130.424027	4268.990213	24.307315
130.607248	4274.535685	24.312333
130.398085	4288.854430	24.317351
130.708839	4294.007468	24.322368
131.192226	4299.663745	24.327386
131.297764	4308.541985	24.332403
131.584258	4317.312968	24.337421
131.535824	4338.617057	24.342439
131.541079	4336.154090	24.347456
131.928678	4340.083022	24.352474
132.151389	4341.708322	24.357491
132.303623	4349.143077	24.362509
132.271144	4369.545111	24.367527
132.354617	4364.604689	24.372544
132.573247	4360.492182	24.377562
132.803357	4370.414664	24.382579
132.995214	4380.289484	24.387597
132.805914	4398.285641	24.392615
133.294638	4390.283079	24.397632
133.548038	4386.771160	24.402650
133.048028	4384.254773	24.407667
133.395142	4393.675997	24.412685
133.818951	4407.734691	24.417703
133.915810	4419.218432	24.422720
134.261777	4414.688249	24.427738
134.157741	4409.057515	24.432755
134.206296	4412.799688	24.437773
133.775109	4426.806112	24.442791
133.936490	4428.567287	24.447808
134.591845	4443.561927	24.452826
134.286917	4455.878818	24.457843
134.801009	4452.319732	24.462861
134.767632	4465.534717	24.467879
135.088294	4470.130713	24.472896
135.217459	4485.646574	24.477914
135.237116	4489.661591	24.482931
135.717290	4486.584442	24.487949
135.602032	4496.980913	24.492967
135.811941	4502.194000	24.497984
135.936581	4510.507491	24.503002
135.878801	4508.805620	24.508019
136.051706	4510.830142	24.513037
135.960488	4531.525644	24.518055
136.550199	4526.423800	24.523072
136.978562	4524.544759	24.528090
136.743599	4540.196625	24.533107
136.969837	4552.313575	24.538125
136.979385	4558.583929	24.543143
137.304749	4555.496300	24.548160
137.726870	4556.695817	24.553178
137.619351	4560.380403	24.558195
137.789649	4570.403903	24.563213
137.750985	4590.769276	24.568231
138.164631	4581.550514	24.573248
137.975276	4578.903361	24.578266
138.240626	4581.229058	24.583283
138.599608	4587.248975	24.588301
137.980487	4599.463673	24.593319
138.291183	4603.688796	24.598336
138.504306	4615.949887	24.603354
138.303360	4620.018432	24.608371
138.831382	4624.332618	24.613389
138.761939	4640.179594	24.618407
139.269219	4648.130178	24.623424
139.553517	4658.110614	24.628442
139.615938	4666.411829	24.633459
139.738261	4666.108473	24.638477
139.987992	4686.845432	24.643495
140.080422	4688.803669	24.648512
140.261966	4689.169686	24.653530
140.464761	4684.453535	24.658547
140.455767	4686.538139	24.663565
140.588079	4699.616858	24.668583
140.765051	4706.132494	24.673600
141.051661	4702.940435	24.678618
141.214650	4715.184194	24.683635
141.270542	4707.890077	24.688653
140.990082	4720.863026	24.693671
141.298182	4743.762595	24.698688
141.519757	4733.566915	24.703706
141.642254	4748.099209	24.708723
141.886303	4752.618896	24.713741
141.902088	4766.946966	24.718759
141.938566	4754.643300	24.723776
141.882245	4760.497911	24.728794
141.832629	4781.382884	24.733811
142.414513	4775.291046	24.738829
142.506007	4791.526447	24.743847
142.943455	4792.676231	24.748864
142.687323	4798.903063	24.753882
142.516670	4809.952324	24.758899
143.044345	4811.346810	24.763917
143.328300	4827.372168	24.768935
143.343326	4837.442237	24.773952
143.652640	4834.612757	24.778970
143.423091	4843.698425	24.783987
143.744540	4843.543793	24.789005
144.158626	4867.686375	24.794023
144.178057	4869.589780	24.799040
144.686307	4864.080785	24.804058
144.718440	4867.951886	24.809075
144.636246	4861.395878	24.814093
144.660753	4876.884278	24.819111
144.784634	4893.146261	24.824128
145.025320	4891.782695	24.829146
144.770958	4895.531388	24.834163
145.322434	4911.568571	24.839181
145.309279	4922.615321	24.844199
145.551358	4912.479461	24.849216
146.025171	4930.517459	24.854234
145.750000	4938.243530	24.859251
145.967306	4942.799021	24.864269
146.300201	4951.196881	24.869287
146.181257	4962.752653	24.874304
147.080635	4960.471496	24.879322
146.333907	4972.507569	24.884339
146.610057	4973.998291	24.889357
147.129983	4982.789846	24.894375
147.009531	4983.458863	24.899392
147.276758	4993.603144	24.904410
147.608195	5004.065655	24.909427
147.530039	5013.598019	24.914445
147.570698	5020.305578	24.919463
147.933971	5019.705628	24.924480
148.129663	5026.862388	24.929498
148.011137	5045.492037	24.934515
148.335124	5044.124880	24.939533
148.157381	5035.127959	24.944551
148.618328	5048.543703	24.949568
149.119819	5068.338875	24.954586
148.829284	5067.008013	24.959603
149.012648	5074.229855	24.964621
149.326725	5071.516386	24.969639
149.309198	5092.589240	24.974656
149.423241	5097.523955	24.979674
149.388804	5100.452245	24.984691
149.511808	5108.848338	24.989709
149.981500	5114.191359	24.994727
149.645682	5121.945949	24.999744
150.355017	5123.826526	25.004762
150.268671	5137.545882	25.009779
150.650078	5136.614802	25.014797
150.588932	5149.121243	25.019815
150.656193	5157.159925	25.024832
151.227686	5161.641044	25.029850
150.952135	5173.319338	25.034867
151.184279	5175.798675	25.039885
151.414237	5183.931832	25.044903
151.481249	5196.746514	25.049920
151.806372	5194.618426	25.054938
151.805029	5194.230267	25.059955
151.951262	5217.335717	25.064973
152.207091	5221.421221	25.069991
152.207030	5223.173043	25.075008
152.593231	5215.871169	25.080026
152.454705	5222.527959	25.085043
152.800471	5231.940362	25.090061
152.672183	5229.668652	25.095079
152.927204	5238.792240	25.100096
153.140699	5249.061877	25.105114
153.221394	5268.942129	25.110131
153.002975	5266.652969	25.115149
153.529779	5271.987090	25.120167
153.404904	5289.835141	25.125184
153.852765	5295.232142	25.130202
153.673870	5312.479450	25.135219
154.313406	5317.120405	25.140237
154.260160	5325.799897	25.145255
154.250922	5330.081627	25.150272
154.761782	5343.145697	25.155290
154.705082	5361.298800	25.160307
155.257617	5355.388142	25.165325
154.953671	5370.593814	25.170343
155.004242	5379.938900	25.175360
155.527796	5385.582915	25.180378
155.660592	5402.206969	25.185395
155.633113	5397.419385	25.190413
155.983704	5413.018143	25.195431
156.067893	5420.138863	25.200448
156.438831	5428.407876	25.205466
156.035406	5434.910530	25.210483
156.425633	5442.027508	25.215501
156.787372	5443.460668	25.220519
156.985371	5456.071926	25.225536
157.682177	5451.843227	25.230554
157.608724	5474.629875	25.235571
157.637563	5483.811116	25.240589
158.137581	5485.642453	25.245607
157.648555	5489.042917	25.250624
158.055543	5474.193276	25.255642
158.156168	5492.072487	25.260659
158.275076	5505.466394	25.265677
158.446961	5504.653351	25.270695
158.106347	5510.208664	25.275712
158.772558	5517.774874	25.280730
158.831640	5521.648206	25.285747
158.669515	5527.374431	25.290765
158.830363	5533.665610	25.295783
158.800570	5541.205131	25.300800
159.310870	5564.181381	25.305818
159.457934	5574.303775	25.310835
159.359088	5583.501913	25.315853
160.137975	5587.931708	25.320871
160.173437	5599.479476	25.325888
160.395763	5600.230552	25.330906
160.380643	5598.739706	25.335923
160.614429	5624.903401	25.340941
160.768748	5628.645039	25.345959
160.996711	5636.728204	25.350976
161.186997	5636.972918	25.355994
160.963053	5660.471530	25.361011
161.392858	5657.531505	25.366029
161.362381	5654.032252	25.371047
161.173023	5674.656037	25.376064
161.623637	5683.351463	25.381082
161.672463	5704.316770	25.386099
162.119640	5706.200601	25.391117
162.419402	5708.849350	25.396135
162.288991	5727.279527	25.401152
162.717410	5744.441569	25.406170
162.746348	5740.380569	25.411187
162.791001	5746.806823	25.416205
163.327761	5753.244372	25.421223
163.301047	5760.183727	25.426240
163.146737	5762.250182	25.431258
163.180218	5775.196791	25.436275
163.629128	5787.096591	25.441293
163.906667	5792.277358	25.446311
163.734121	5800.871593	25.451328
164.039468	5803.263788	25.456346
164.278246	5812.822678	25.461363
164.306314	5828.039849	25.466381
164.668776	5834.902479	25.471399
164.509386	5842.206732	25.476416
164.659606	5853.724056	25.481434
165.053374	5865.986099	25.486451
164.965373	5877.013584	25.491469
165.400339	5888.792523	25.496487
165.665852	5904.771211	25.501504
165.961120	5910.002898	25.506522
166.220362	5927.188459	25.511539
166.081664	5926.471405	25.516557
166.672607	5932.139758	25.521575
166.550682	5939.154074	25.526592
166.800207	5942.839824	25.531610
166.547990	5952.077958	25.536627
166.924443	5970.103829	25.541645
167.478085	5962.478695	25.546663
167.328786	5970.343318	25.551680
167.400023	5985.200301	25.556698
167.457384	5995.087598	25.561715
167.625804	6008.707717	25.566733
168.294416	6015.389870	25.571751
168.504495	6016.057651	25.576768
168.736353	6021.719151	25.581786
168.887905	6049.828268	25.586803
168.681243	6047.085751	25.591821
169.082525	6046.047342	25.596839
169.237404	6054.028499	25.601856
169.464699	6067.746768	25.606874
169.857167	6078.992682	25.611891
169.736894	6082.698512	25.616909
170.079527	6072.988204	25.621927
170.067433	6092.820754	25.626944
170.242103	6101.644843	25.631962
170.742313	6110.430564	25.636979
170.385421	6107.859940	25.641997
170.876447	6123.680377	25.647015
171.051534	6132.315010	25.652032
171.279516	6130.760782	25.657050
171.385449	6130.128510	25.662067
170.991520	6150.084075	25.667085
171.658050	6150.260502	25.672103
171.896983	6155.895682	25.677120
171.986948	6161.532104	25.682138
172.282509	6177.105412	25.687156
172.179438	6196.024234	25.692173
172.284608	6191.143056	25.697191
172.548413	6210.556853	25.702208
172.549351	6213.306156	25.707226
172.657506	6217.212986	25.712244
172.979822	6236.598704	25.717261
172.832868	6236.129161	25.722279
173.005195	6251.140990	25.727296
173.292912	6261.017597	25.732314
173.688280	6270.757387	25.737332
173.448602	6289.763998	25.742349
174.032585	6299.774151	25.747367
174.324351	6310.966535	25.752384
174.671456	6326.550837	25.757402
174.723082	6331.015830	25.762420
174.574100	6337.166416	25.767437
175.005861	6328.878357	25.772455
174.993248	6336.914288	25.777472
174.992791	6348.872226	25.782490
175.524255	6352.924275	25.787508
175.440978	6358.344823	25.792525
176.039137	6370.174271	25.797543
176.068801	6369.370845	25.802560
176.174845	6385.630637	25.807578
176.295722	6382.918834	25.812596
176.412487	6398.911786	25.817613
176.701189	6386.296024	25.822631
177.083112	6397.275458	25.827648
176.977156	6416.396994	25.832666
177.444189	6418.211499	25.837684
177.364718	6431.204678	25.842701
177.792915	6441.393998	25.847719
177.581606	6460.118541	25.852736
177.612882	6463.576570	25.857754
177.863372	6467.287530	25.862772
177.902755	6479.128823	25.867789
177.821186	6494.821463	25.872807
178.462841	6498.382758	25.877824
178.477161	6520.355119	25.882842
178.989494	6511.997532	25.887860
179.129601	6533.498777	25.892877
179.494120	6543.148840	25.897895
179.508208	6554.034465	25.902912
179.496064	6565.195694	25.907930
179.754941	6571.386639	25.912948
179.776807	6585.967728	25.917965
179.820497	6597.751600	25.922983
180.207982	6616.013143	25.928000
180.527090	6629.007157	25.933018
180.836493	6642.163701	25.938036
180.991986	6646.798754	25.943053
181.191165	6652.825451	25.948071
181.192223	6666.030317	25.953088
181.540025	6670.407955	25.958106
181.690373	6685.120524	25.963124
182.031509	6700.264119	25.968141
182.259664	6695.183600	25.973159
182.295947	6707.666369	25.978176
182.554868	6719.767013	25.983194
182.996598	6717.244818	25.988212
182.761925	6733.277333	25.993229
183.230874	6740.271997	25.998247
183.316166	6749.277714	26.003264
183.198489	6748.415275	26.008282
183.424620	6762.358384	26.013300
183.934067	6780.547318	26.018317
183.713619	6780.745905	26.023335
183.975801	6789.108339	26.028352
184.180462	6797.012570	26.033370
184.407716	6799.085659	26.038388
184.836336	6818.515320	26.043405
184.788976	6814.336603	26.048423
184.892394	6835.218885	26.053440
184.994453	6853.471712	26.058458
185.068320	6859.019320	26.063476
185.357744	6874.717303	26.068493
185.361655	6868.099732	26.073511
186.272315	6894.108692	26.078528
185.861794	6910.825544	26.083546
186.156006	6909.677588	26.088564
186.368127	6928.973967	26.093581
186.445642	6929.580470	26.098599
186.741521	6927.668281	26.103616
186.985124	6954.160655	26.108634
187.252319	6950.794465	26.113652
187.193647	6961.966381	26.118669
187.651110	6974.203406	26.123687
187.589018	6985.369557	26.128704
187.544422	6994.057953	26.133722
188.205079	7002.462239	26.138740
188.520943	7006.784980	26.143757
188.540781	7019.008512	26.148775
188.204891	7019.711351	26.153792
188.619165	7037.691309	26.158810
189.271268	7056.366434	26.163828
189.338754	7077.033634	26.168845
189.411502	7070.278930	26.173863
189.805153	7081.809400	26.178880
189.506278	7098.316359	26.183898
190.029596	7093.290513	26.188916
190.002209	7110.979842	26.193933
190.176709	7118.898407	26.198951
190.703532	7131.250949	26.203968
190.641733	7148.888880	26.208986
191.080055	7153.435557	26.214004
191.588159	7167.508433	26.219021
191.765528	7172.686343	26.224039
191.669886	7172.663336	26.229056
191.783921	7177.668067	26.234074
191.928306	7191.488560	26.239092
192.033598	7208.203799	26.244109
191.983503	7219.330329	26.249127
192.287795	7217.293672	26.254144
192.174398	7237.806286	26.259162
192.600065	7248.845675	26.264180
192.806930	7277.601495	26.269197
192.908752	7282.219862	26.274215
193.063954	7291.091771	26.279232
193.574633	7307.513134	26.284250
193.625607	7313.080250	26.289268
194.001701	7330.438239	26.294285
194.342865	7334.877060	26.299303
194.646632	7354.645702	26.304320
194.282853	7362.977024	26.309338
194.949865	7367.061736	26.314356
195.160601	7394.282841	26.319373
195.522453	7398.847873	26.324391
195.610236	7397.536493	26.329408
195.831842	7413.501276	26.334426
196.053965	7420.089733	26.339444
196.174030	7422.451187	26.344461
196.142249	7439.516436	26.349479
196.543486	7446.812422	26.354496
196.695246	7451.880771	26.359514
196.805760	7461.151231	26.364532
196.669173	7467.931650	26.369549
197.575992	7497.670483	26.374567
197.526815	7501.397029	26.379584
197.306019	7514.239475	26.384602
197.613424	7524.603015	26.389620
197.428130	7536.388632	26.394637
198.021560	7547.761819	26.399655
198.418024	7555.200661	26.404672
198.328931	7578.437505	26.409690
198.693730	7589.527675	26.414708
198.973946	7598.872644	26.419725
198.705147	7611.457488	26.424743
199.340522	7615.528270	26.429760
199.408706	7625.610484	26.434778
199.741374	7634.653650	26.439796
199.806703	7657.291823	26.444813
200.074018	7657.786534	26.449831
200.675663	7667.722061	26.454848
200.501906	7670.972503	26.459866
200.513550	7668.782749	26.464884
200.916592	7695.162815	26.469901
201.433068	7703.242738	26.474919
201.234460	7709.988763	26.479936
201.336739	7718.622920	26.484954
201.692782	7720.925346	26.489972
202.052303	7750.712441	26.494989
202.096750	7751.583030	26.500007
202.385851	7752.794138	26.505024
202.298082	7768.671941	26.510042
202.586422	7769.693746	26.515060
202.889093	7798.526925	26.520077
203.248928	7806.729301	26.525095
203.646674	7810.556377	26.530112
203.240473	7829.470692	26.535130
203.526462	7836.052450	26.540148
203.771968	7854.934151	26.545165
203.929456	7871.875437	26.550183
204.709468	7872.286680	26.555200
204.402661	7889.638523	26.560218
204.459825	7892.669719	26.565236
204.879754	7910.109786	26.570253
204.995805	7925.857925	26.575271
205.380606	7932.692589	26.580288
205.321710	7948.796491	26.585306
205.615603	7957.545968	26.590324
206.079971	7975.528467	26.595341
206.189800	7990.886157	26.600359
206.433373	7993.319892	26.605376
206.534561	8009.275641	26.610394
206.578385	8027.437727	26.615412
207.079758	8031.955804	26.620429
206.708604	8059.480571	26.625447
207.275945	8068.544016	26.630464
207.393575	8089.693845	26.635482
207.566385	8094.181324	26.640500
208.133765	8104.668634	26.645517
208.085362	8114.756751	26.650535
208.725077	8127.540588	26.655552
208.820582	8147.377434	26.660570
208.707350	8152.995785	26.665588
209.350078	8169.384604	26.670605
209.320329	8170.617276	26.675623
209.411489	8185.453971	26.680640
209.980672	8200.474678	26.685658
210.233191	8214.332668	26.690676
210.510910	8225.711534	26.695693
210.214334	8236.700490	26.700711
210.830787	8245.109117	26.705728
210.932950	8261.472201	26.710746
211.118940	8262.923653	26.715764
211.490719	8276.362051	26.720781
211.518668	8284.989174	26.725799
211.713303	8284.769149	26.730816
211.869504	8307.507538	26.735834
211.856913	8318.489940	26.740852
212.020083	8329.643715	26.745869
212.149056	8346.940346	26.750887
212.739167	8359.056486	26.755904
212.838709	8377.882659	26.760922
213.032445	8391.014374	26.765940
213.352603	8390.471597	26.770957
213.455190	8416.899762	26.775975
214.122711	8410.048237	26.780992
214.222905	8423.936562	26.786010
214.144905	8434.386247	26.791028
214.306359	8455.608558	26.796045
214.677999	8456.289009	26.801063
214.751428	8470.225761	26.806080
214.882465	8483.610466	26.811098
214.847096	8491.802444	26.816116
215.197167	8499.255252	26.821133
215.149883	8515.660915	26.826151
215.374591	8530.603253	26.831168
215.750730	8549.029508	26.836186
215.914856	8568.761341	26.841204
216.373448	8581.876958	26.846221
216.524179	8591.387945	26.851239
216.805737	8603.877772	26.856256
216.878782	8620.510939	26.861274
217.014448	8638.974955	26.866292
217.557466	8651.606974	26.871309
217.437514	8668.942901	26.876327
218.063021	8678.117508	26.881344
218.332646	8698.006598	26.886362
218.181934	8713.538305	26.891380
218.926514	8730.378934	26.896397
218.808086	8732.901049	26.901415
219.265343	8747.415638	26.906432
219.518902	8760.718205	26.911450
219.104444	8763.987601	26.916468
220.074645	8786.343326	26.921485
219.856032	8800.543925	26.926503
220.030162	8808.617978	26.931520
220.168374	8823.706706	26.936538
220.779445	8838.453006	26.941556
220.728350	8852.422182	26.946573
221.118146	8873.937553	26.951591
221.238064	8881.117161	26.956608
222.031949	8895.216049	26.961626
222.183314	8909.245111	26.966644
222.055689	8911.759219	26.971661
222.171897	8922.080881	26.976679
222.520215	8937.559858	26.981696
222.645462	8956.332076	26.986714
222.468885	8973.954995	26.991732
223.002316	8989.534465	26.996749
223.092969	9004.542387	27.001767
223.426125	9006.706486	27.006784
223.695968	9025.531896	27.011802
223.741613	9042.415999	27.016820
224.169664	9055.464119	27.021837
224.249913	9080.586462	27.026855
224.657199	9093.022194	27.031872
224.900530	9108.183090	27.036890
225.138462	9124.727732	27.041908
225.619602	9129.590237	27.046925
225.415266	9149.667721	27.051943
225.842731	9151.274010	27.056960
226.378504	9165.612449	27.061978
226.521868	9182.601348	27.066996
226.583852	9188.416730	27.072013
226.854053	9209.316610	27.077031
226.905413	9219.051867	27.082048
226.865513	9224.962153	27.087066
226.997789	9239.310184	27.092084
227.511766	9261.305404	27.097101
227.688238	9273.695326	27.102119
228.310938	9292.402584	27.107136
228.263601	9300.350523	27.112154
228.600709	9329.288038	27.117172
228.983411	9334.001838	27.122189
229.053918	9333.684427	27.127207
229.210198	9345.597648	27.132224
229.285941	9354.918705	27.137242
229.512352	9368.415400	27.142260
229.975834	9376.097067	27.147277
230.372748	9393.469521	27.152295
230.227024	9409.278871	27.157312
230.413533	9426.630642	27.162330
230.644780	9431.743915	27.167348
231.075744	9440.924121	27.172365
231.010899	9457.143925	27.177383
231.159993	9470.810673	27.182400
231.551371	9488.777662	27.187418
231.484991	9501.433108	27.192436
232.104114	9521.546175	27.197453
232.072537	9536.696811	27.202471
232.590973	9543.166989	27.207488
232.894043	9568.738160	27.212506
232.750872	9582.858073	27.217524
233.280281	9595.628636	27.222541
232.984892	9618.508835	27.227559
233.239291	9628.029373	27.232576
233.876394	9650.703544	27.237594
234.324891	9673.186272	27.242612
234.539195	9680.742917	27.247629
234.959856	9706.055895	27.252647
235.052399	9707.026393	27.257664
235.158126	9726.989620	27.262682
235.451571	9738.654274	27.267700
235.873818	9748.603242	27.272717
235.695525	9772.630361	27.277735
236.700382	9782.759616	27.282752
236.460611	9797.731533	27.287770
236.526026	9814.449054	27.292788
236.660418	9818.374639	27.297805
236.953911	9840.433501	27.302823
237.153432	9854.455732	27.307840
237.703208	9868.025272	27.312858
237.814424	9886.854302	27.317876
238.187495	9900.170538	27.322893
238.618205	9912.890475	27.327911
238.809696	9935.701106	27.332928
238.949892	9935.296990	27.337946
239.106219	9954.194799	27.342964
239.343361	9963.800304	27.347981
239.202537	9980.919701	27.352999
239.612374	9984.682190	27.358016
240.208001	9999.207658	27.363034
240.185475	10021.928781	27.368052
240.384736	10041.827173	27.373069
240.688200	10055.722763	27.378087
240.928083	10074.184507	27.383104
241.053184	10085.146382	27.388122
241.524298	10108.431240	27.393140
241.576052	10108.827179	27.398157
241.616400	10138.668108	27.403175
242.080638	10156.024412	27.408192
242.447966	10168.006136	27.413210
242.484265	10188.830089	27.418228
242.972024	10194.879045	27.423245
243.115683	10213.659117	27.428263
243.784991	10232.969413	27.433280
244.106867	10240.007397	27.438298
243.838066	10251.615206	27.443316
244.080768	10263.805964	27.448333
244.398022	10288.431815	27.453351
244.462370	10285.680940	27.458368
244.955985	10298.643885	27.463386
244.995033	10303.058130	27.468404
245.336822	10317.560462	27.473421
245.408216	10340.728251	27.478439
245.554809	10347.651648	27.483456
246.067083	10368.448600	27.488474
246.121271	10387.943826	27.493492
246.165922	10390.352207	27.498509
246.315691	10410.612384	27.503527
246.970617	10422.978640	27.508544
247.156563	10448.553577	27.513562
247.127512	10466.350558	27.518580
247.653542	10484.250052	27.523597
247.671096	10495.279534	27.528615
248.013706	10520.987904	27.533632
248.090908	10537.249543	27.538650
248.347561	10562.415712	27.543668
248.918221	10568.732823	27.548685
249.038821	10586.781180	27.553703
249.122242	10606.224691	27.558720
249.656327	10620.649772	27.563738
249.812820	10646.081189	27.568756
250.020305	10662.818261	27.573773
250.299358	10686.841217	27.578791
250.538174	10700.188528	27.583808
251.046279	10710.092987	27.588826
251.454628	10734.001022	27.593844
251.416170	10744.935227	27.598861
251.596948	10763.738455	27.603879
252.202359	10780.596435	27.608896
252.776255	10786.455268	27.613914
252.619334	10807.935374	27.618932
253.085416	10816.523453	27.623949
252.866476	10834.726280	27.628967
253.315213	10851.258377	27.633984
253.760158	10863.181026	27.639002
253.349880	10879.124629	27.644020
253.800634	10898.258293	27.649037
254.165601	10916.720221	27.654055
254.264921	10933.471322	27.659072
254.747720	10946.935311	27.664090
254.809669	10974.023928	27.669108
254.749733	10988.757064	27.674125
255.506146	10995.919877	27.679143
255.624461	11024.752203	27.684160
256.127043	11037.600584	27.689178
256.136922	11069.973850	27.694196
256.253860	11078.452548	27.699213
256.808062	11099.117442	27.704231
257.204120	11129.873613	27.709248
257.577631	11134.257764	27.714266
257.748779	11163.132548	27.719284
258.120668	11172.259712	27.724301
258.318460	11180.798416	27.729319
258.347581	11195.230419	27.734336
258.708565	11206.699111	27.739354
258.898034	11226.537145	27.744372
259.089113	11239.516560	27.749389
259.426010	11266.208873	27.754407
259.737503	11279.516794	27.759424
259.864678	11285.928884	27.764442
260.338363	11309.732691	27.769460
260.223716	11318.762472	27.774477
260.623227	11328.504285	27.779495
260.922626	11351.239742	27.784512
261.378162	11371.974073	27.789530
261.522086	11392.394110	27.794548
261.628730	11402.210258	27.799565
262.008808	11425.788893	27.804583
261.972398	11437.758894	27.809600
262.291622	11449.095339	27.814618
262.361016	11470.499698	27.819636
262.904077	11489.303740	27.824653
263.209798	11504.965195	27.829671
263.031905	11526.004173	27.834688
263.546273	11538.216358	27.839706
263.870657	11561.706000	27.844724
264.223325	11576.987553	27.849741
264.562337	11597.115164	27.854759
264.862021	11620.150882	27.859776
264.528014	11638.214625	27.864794
265.050631	11658.973500	27.869812
265.666744	11675.915869	27.874829
265.629456	11696.273049	27.879847
265.966770	11710.815055	27.884864
265.931196	11738.017938	27.889882
266.354190	11759.023043	27.894900
266.787229	11781.125487	27.899917
267.486953	11800.120024	27.904935
267.761858	11816.872827	27.909952
267.849101	11823.982899	27.914970
268.098349	11836.839937	27.919988
268.244439	11864.279795	27.925005
268.650654	11872.419867	27.930023
268.745093	11900.660462	27.935040
269.410077	11912.542997	27.940058
269.627664	11938.225527	27.945076
270.015406	11943.084461	27.950093
270.350316	11961.166880	27.955111
270.417306	11970.910592	27.960128
270.543113	11990.986763	27.965146
271.118801	12000.436076	27.970164
271.123634	12028.353019	27.975181
271.219587	12043.940419	27.980199
271.415660	12064.078289	27.985216
271.681035	12077.005594	27.990234
271.798531	12107.926998	27.995252
271.783321	12117.724714	28.000269
272.468887	12142.604767	28.005287
272.996852	12167.051662	28.010304
273.394560	12184.521319	28.015322
273.454781	12206.947919	28.020340
273.513594	12236.685079	28.025357
274.154081	12251.587368	28.030375
274.196997	12281.661816	28.035392
274.405101	12294.863498	28.040410
274.740406	12308.534724	28.045428
274.713772	12334.117107	28.050445
275.315913	12356.597938	28.055463
275.533973	12373.859076	28.060480
275.501641	12384.730116	28.065498
275.818886	12410.129262	28.070516
276.062169	12434.510575	28.075533
276.492448	12451.479598	28.080551
276.809894	12484.182895	28.085568
277.502333	12505.411883	28.090586
277.526376	12522.302503	28.095604
277.755762	12540.670425	28.100621
278.277458	12556.071558	28.105639
278.297188	12583.942777	28.110656
278.977612	12600.108547	28.115674
279.120612	12623.476349	28.120692
279.437143	12634.479198	28.125709
279.687787	12651.852327	28.130727
279.484760	12670.698635	28.135744
280.051465	12687.254923	28.140762
280.578218	12710.316404	28.145780
280.917819	12719.054644	28.150797
280.922443	12735.408498	28.155815
281.108415	12759.079209	28.160832
281.342488	12764.871901	28.165850
281.781918	12781.966104	28.170868
281.775420	12804.514390	28.175885
282.334488	12817.099354	28.180903
282.314460	12849.372989	28.185920
282.802059	12868.149203	28.190938
283.185521	12880.553296	28.195956
283.548015	12904.935488	28.200973
284.030916	12925.196715	28.205991
283.980175	12933.506724	28.211008
284.199044	12952.808281	28.216026
284.348137	12977.053467	28.221044
284.400331	12996.068542	28.226061
285.189513	13020.327201	28.231079
284.990076	13045.893403	28.236096
285.336940	13060.453902	28.241114
285.996085	13085.629870	28.246132
286.109729	13123.633650	28.251149
286.641506	13137.110487	28.256167
286.385578	13159.663530	28.261184
286.658526	13177.175756	28.266202
287.374097	13197.157665	28.271220
287.535332	13237.355318	28.276237
288.153364	13248.683936	28.281255
288.049522	13273.095441	28.286272
288.245939	13283.593259	28.291290
288.950213	13316.338454	28.296308
289.436609	13333.274216	28.301325
289.783527	13355.875167	28.306343
289.897731	13375.645142	28.311360
289.993284	13387.772553	28.316378
290.500156	13411.488550	28.321396
290.441678	13426.494945	28.326413
290.795782	13447.569566	28.331431
291.173978	13473.750094	28.336448
291.538952	13491.706106	28.341466
291.930549	13507.567360	28.346484
291.952050	13538.964049	28.351501
292.327109	13560.509216	28.356519
292.249398	13581.023180	28.361536
292.971465	13601.752952	28.366554
293.267998	13620.269305	28.371572
293.529997	13642.792317	28.376589
293.747020	13668.805721	28.381607
294.248646	13695.545142	28.386624
294.376272	13719.936752	28.391642
294.886387	13731.412045	28.396660
294.958889	13754.549114	28.401677
295.561936	13778.345247	28.406695
295.736979	13789.661473	28.411712
295.865674	13815.341527	28.416730
296.138486	13833.795485	28.421748
296.191530	13860.535929	28.426765
296.570960	13873.784510	28.431783
297.079414	13904.218104	28.436800
297.299755	13927.884889	28.441818
297.653487	13949.301198	28.446836
297.869417	13975.157288	28.451853
298.350639	13994.570396	28.456871
298.750398	14013.184653	28.461888
299.058028	14031.784937	28.466906
299.519840	14056.421491	28.471924
299.276947	14077.482953	28.476941
299.947400	14092.344107	28.481959
300.384403	14109.032493	28.486976
300.547743	14130.065117	28.491994
301.198808	14140.476400	28.497012
300.976894	14167.089807	28.502029
301.537248	14177.859556	28.507047
301.765499	14197.489354	28.512064
301.846121	14215.307422	28.517082
302.276682	14229.691487	28.522100
302.372632	14256.877379	28.527117
302.648441	14268.288641	28.532135
302.873177	14278.684671	28.537152
303.026656	14316.874083	28.542170
303.310179	14324.630192	28.547188
303.440918	14361.645266	28.552205
303.947798	14375.360589	28.557223
304.352258	14408.568353	28.562240
304.866275	14439.690411	28.567258
305.191024	14459.816986	28.572276
304.918894	14484.973310	28.577293
305.350610	14501.985002	28.582311
306.041219	14537.576806	28.587328
306.253002	14567.037838	28.592346
306.529817	14583.511711	28.597364
306.733722	14614.388920	28.602381
307.008325	14634.431947	28.607399
307.835290	14656.305500	28.612416
308.041611	14687.491953	28.617434
308.084249	14695.241733	28.622452
308.232696	14730.236650	28.627469
308.696330	14751.491368	28.632487
309.171095	14780.879953	28.637504
309.395216	14804.935696	28.642522
309.891033	14828.181460	28.647540
309.964348	14846.923466	28.652557
310.476322	14864.185044	28.657575
310.737576	14888.462469	28.662592
310.883296	14923.350786	28.667610
311.409958	14933.715671	28.672628
311.891466	14973.175159	28.677645
312.212099	14995.779018	28.682663
312.035741	15016.442623	28.687680
312.460121	15040.669423	28.692698
312.991702	15060.682118	28.697716
312.836268	15089.367693	28.702733
313.296620	15109.505295	28.707751
313.763667	15135.731039	28.712768
313.766631	15165.683655	28.717786
314.586435	15185.458676	28.722804
314.523714	15221.138177	28.727821
315.257869	15243.980750	28.732839
315.562982	15267.241129	28.737856
315.802017	15286.529260	28.742874
316.525435	15312.446632	28.747892
316.747200	15340.805041	28.752909
317.090817	15343.786252	28.757927
317.388741	15361.953506	28.762944
317.522172	15389.324636	28.767962
318.030174	15409.006607	28.772980
318.353599	15431.613702	28.777997
318.806948	15458.934819	28.783015
319.320948	15470.265272	28.788032
318.827513	15492.990920	28.793050
319.579735	15508.415193	28.798068
319.579916	15537.512914	28.803085
319.829204	15560.706594	28.808103
320.244294	15579.575806	28.813120
320.439087	15607.733542	28.818138
320.834859	15623.930692	28.823156
320.731198	15648.162015	28.828173
320.769192	15675.482177	28.833191
321.291990	15698.124682	28.838208
321.734473	15736.919123	28.843226
321.968986	15745.574152	28.848244
322.753963	15785.843701	28.853261
322.735504	15798.066303	28.858279
323.300732	15823.409053	28.863296
323.293690	15860.104339	28.868314
323.882235	15872.421410	28.873332
324.342696	15902.669886	28.878349
324.660541	15933.676661	28.883367
324.674542	15943.484401	28.888384
324.700962	15972.120698	28.893402
325.298387	15999.009421	28.898420
325.368562	16034.104255	28.903437
325.812601	16055.464563	28.908455
326.504520	16089.874638	28.913472
326.439941	16117.492596	28.918490
326.936828	16147.896834	28.923508
327.361069	16179.105271	28.928525
327.554277	16205.953372	28.933543
328.383636	16231.356357	28.938560
328.489488	16256.964304	28.943578
328.738663	16275.699108	28.948596
328.860183	16307.217325	28.953613
329.517885	16343.942063	28.958631
330.139662	16367.324730	28.963648
330.580280	16394.478615	28.968666
330.802198	16413.148336	28.973684
330.824101	16437.120938	28.978701
331.310598	16453.863632	28.983719
331.812108	16485.107840	28.988736
332.129401	16508.254109	28.993754
332.536976	16525.299811	28.998772
332.625296	16557.720655	29.003789
332.892498	16586.007455	29.008807
333.144871	16596.646782	29.013824
333.445903	16637.976224	29.018842
334.025932	16657.973524	29.023860
334.451029	16681.081004	29.028877
334.276465	16707.750523	29.033895
335.040588	16732.677975	29.038912
335.163418	16758.801930	29.043930
335.894667	16785.051715	29.048948
335.916922	16813.674121	29.053965
336.213854	16843.734911	29.058983
336.866552	16867.400774	29.064000
337.232657	16887.987730	29.069018
337.157385	16912.794214	29.074036
337.530038	16941.908358	29.079053
337.509515	16970.673516	29.084071
338.435150	17001.842651	29.089088
338.491972	17030.475757	29.094106
339.110912	17059.166150	29.099124
339.347746	17083.987137	29.104141
339.648473	17107.326236	29.109159
340.286392	17133.385806	29.114176
340.321677	17160.354731	29.119194
340.683343	17181.056406	29.124212
341.140741	17211.307419	29.129229
341.209656	17236.950878	29.134247
341.806584	17253.168431	29.139264
342.213551	17281.532274	29.144282
342.522327	17298.843669	29.149300
342.832667	17329.939148	29.154317
342.847979	17347.403948	29.159335
343.540181	17381.592025	29.164352
343.369982	17403.369066	29.169370
344.047994	17421.841975	29.174388
344.219604	17448.038186	29.179405
344.589196	17489.080747	29.184423
345.175098	17511.743930	29.189440
345.152427	17546.303287	29.194458
345.814955	17555.511189	29.199476
346.053906	17588.962008	29.204493
345.936856	17612.973625	29.209511
346.269881	17630.395231	29.214528
346.810910	17670.027814	29.219546
347.520317	17698.736574	29.224564
347.705803	17732.297094	29.229581
347.924866	17753.508160	29.234599
349.030120	17767.858691	29.239616
348.646823	17796.865106	29.244634
349.132730	17830.296610	29.249652
349.566248	17855.473142	29.254669
349.704579	17890.007891	29.259687
350.106078	17917.356411	29.264704
350.470315	17938.949259	29.269722
350.541717	17976.110084	29.274740
350.946539	18005.593521	29.279757
351.380670	18043.253597	29.284775
352.072433	18071.106491	29.289792
352.188654	18101.267033	29.294810
352.584325	18129.791827	29.299828
353.139979	18163.977404	29.304845
353.649674	18194.171220	29.309863
353.739747	18219.256717	29.314880
354.006508	18240.783041	29.319898
354.346004	18273.764425	29.324916
354.985818	18296.994985	29.329933
354.983463	18338.236590	29.334951
355.693420	18350.065572	29.339968
356.079614	18375.509214	29.344986
356.206227	18408.012443	29.350004
356.710778	18445.302163	29.355021
356.757517	18474.633920	29.360039
357.151647	18503.904988	29.365056
357.603267	18542.157153	29.370074
357.835764	18567.568262	29.375092
358.707807	18603.145486	29.380109
358.622452	18637.615517	29.385127
359.263534	18658.982588	29.390144
359.631351	18687.367256	29.395162
359.524382	18726.313780	29.400180
360.460114	18753.352357	29.405197
360.819449	18783.077855	29.410215
361.126400	18793.611917	29.415232
361.518227	18833.289198	29.420250
361.581327	18853.666678	29.425268
362.245053	18873.867966	29.430285
362.208145	18922.128964	29.435303
363.026512	18947.562520	29.440320
363.440678	18973.400584	29.445338
363.688613	19004.773868	29.450356
363.890004	19028.396187	29.455373
363.768226	19056.706454	29.460391
364.570579	19089.774664	29.465408
364.901130	19120.989884	29.470426
365.163663	19149.935053	29.475444
365.884315	19186.269932	29.480461
366.171045	19218.635710	29.485479
366.586334	19251.448929	29.490496
366.853397	19283.969525	29.495514
366.906850	19310.584780	29.500532
367.340087	19321.851180	29.505549
367.829236	19364.313141	29.510567
368.052304	19378.847283	29.515584
368.417800	19416.407043	29.520602
368.735102	19445.659970	29.525620
369.422516	19478.058184	29.530637
369.134102	19502.206374	29.535655
369.851775	19530.828096	29.540672
370.117972	19570.229607	29.545690
370.534085	19597.344432	29.550708
371.055972	19624.878669	29.555725
371.065145	19660.194947	29.560743
371.628792	19692.638177	29.565760
371.830800	19725.750958	29.570778
371.960556	19762.912362	29.575796
372.902439	19789.123747	29.580813
373.021822	19829.692350	29.585831
373.678363	19847.646532	29.590848
374.118229	19886.794025	29.595866
374.072157	19918.695004	29.600884
374.828814	19950.963112	29.605901
375.045477	19991.813764	29.610919
375.357399	20019.646809	29.615936
376.063345	20057.211334	29.620954
376.236104	20088.452813	29.625972
376.755667	20133.085131	29.630989
377.400847	20158.585304	29.636007
377.565607	20185.272767	29.641024
377.989372	20212.962202	29.646042
378.372585	20252.169845	29.651060
378.880505	20280.490653	29.656077
379.167440	20309.920220	29.661095
379.776802	20337.700807	29.666112
380.044407	20368.106501	29.671130
379.867775	20394.980407	29.676148
380.484604	20427.315430	29.681165
380.952054	20471.495446	29.686183
381.728390	20495.939313	29.691200
382.098717	20518.538674	29.696218
382.673589	20548.940747	29.701236
382.364604	20582.716299	29.706253
382.681639	20610.840024	29.711271
383.329176	20647.726130	29.716288
383.780544	20681.262704	29.721306
383.637187	20715.878158	29.726324
384.372569	20742.811872	29.731341
384.697750	20783.129063	29.736359
385.205189	20817.156240	29.741376
385.747259	20852.372233	29.746394
385.674337	20893.004743	29.751412
386.421340	20908.917512	29.756429
386.652127	20948.529525	29.761447
387.280021	20980.408797	29.766464
387.357770	21004.267690	29.771482
387.823251	21044.500255	29.776500
388.567987	21078.882462	29.781517
388.654583	21105.393860	29.786535
389.002305	21146.681315	29.791552
389.206766	21177.711045	29.796570
389.618705	21212.834333	29.801588
390.053858	21237.717997	29.806605
390.310032	21283.310371	29.811623
391.363459	21312.741430	29.816640
391.514137	21347.918518	29.821658
391.764276	21379.889200	29.826676
392.437465	21412.646680	29.831693
392.483358	21452.686737	29.836711
393.589439	21471.267043	29.841728
393.528724	21491.976265	29.846746
393.681523	21525.700053	29.851764
394.453991	21555.845260	29.856781
394.355130	21593.317629	29.861799
394.883774	21620.108005	29.866816
395.219196	21648.761099	29.871834
395.475338	21671.518679	29.876852
395.810049	21706.092578	29.881869
396.406891	21744.890607	29.886887
396.548934	21786.426451	29.891904
396.947785	21814.140998	29.896922
397.476632	21854.030395	29.901940
398.197950	21886.932774	29.906957
398.163654	21919.258498	29.911975
398.344047	21945.339292	29.916992
398.870818	21986.391936	29.922010
399.034910	22026.661072	29.927028
399.660858	22056.735212	29.932045
400.370162	22106.403647	29.937063
400.556673	22138.884708	29.942080
401.208234	22185.838968	29.947098
401.558760	22213.858630	29.952116
402.033783	22247.286739	29.957133
402.166600	22294.006565	29.962151
402.527804	22328.514211	29.967168
403.326432	22368.943727	29.972186
403.245894	22405.308950	29.977204
403.750527	22440.129228	29.982221
404.461939	22478.973939	29.987239
404.749397	22513.221744	29.992256
405.072906	22545.821029	29.997274
405.035297	22594.621920	30.002292
406.016524	22630.284133	30.007309
406.230401	22673.788426	30.012327
406.890761	22710.253003	30.017344
407.691512	22742.405037	30.022362
407.470565	22783.336325	30.027380
408.210747	22819.706452	30.032397
408.363238	22858.569943	30.037415
408.830153	22889.832966	30.042432
409.498820	22926.833761	30.047450
409.566581	22967.480079	30.052468
410.462686	23005.538601	30.057485
410.694524	23045.040895	30.062503
410.862005	23084.123647	30.067520
411.888397	23113.251989	30.072538
411.908026	23146.727665	30.077556
412.283052	23175.901251	30.082573
412.785697	23214.533654	30.087591
413.024672	23248.120484	30.092608
413.477566	23285.604406	30.097626
413.836941	23326.597571	30.102644
414.153816	23366.074543	30.107661
414.617087	23408.296490	30.112679
414.943062	23445.851146	30.117696
415.798455	23478.653016	30.122714
415.978582	23526.290933	30.127732
416.610855	23556.467464	30.132749
416.808743	23594.712307	30.137767
416.897749	23636.348789	30.142784
417.786518	23665.809144	30.147802
418.002628	23700.594669	30.152820
418.729984	23739.572051	30.157837
419.046121	23786.753251	30.162855
419.735445	23816.782214	30.167872
419.875834	23844.748615	30.172890
420.121818	23884.894932	30.177908
420.414669	23912.262482	30.182925
421.197943	23957.216002	30.187943
421.761238	23991.530571	30.192960
422.067889	24014.004867	30.197978
422.056122	24046.027178	30.202996
422.502636	24077.042480	30.208013
423.357261	24113.807810	30.213031
423.822715	24148.283321	30.218048
424.217431	24170.465942	30.223066
424.091396	24208.718459	30.228084
424.505635	24238.759546	30.233101
425.169134	24281.286909	30.238119
425.662437	24319.613256	30.243136
426.051759	24360.730241	30.248154
426.343873	24399.657013	30.253172
426.890914	24428.388395	30.258189
427.179095	24465.976165	30.263207
427.333670	24516.982454	30.268224
428.080740	24546.377829	30.273242
428.730625	24589.388268	30.278260
428.740341	24628.347076	30.283277
429.217406	24665.115680	30.288295
429.672786	24709.060548	30.293312
429.935420	24744.422005	30.298330
430.506049	24779.115955	30.303348
430.790639	24829.464385	30.308365
430.837843	24887.256815	30.313383
431.292947	24927.265028	30.318400
432.098066	24960.532226	30.323418
432.324513	25022.227839	30.328436
432.835105	25062.853285	30.333453
433.305262	25104.249840	30.338471
433.635601	25161.632163	30.343488
434.419014	25197.424749	30.348506
434.709156	25246.964419	30.353524
435.544468	25292.696440	30.358541
435.773219	25338.011664	30.363559
436.544655	25385.997447	30.368576
437.176929	25415.886067	30.373594
437.353535	25450.693451	30.378612
437.849588	25503.506798	30.383629
438.257975	25529.891512	30.388647
438.562149	25570.013122	30.393664
439.487615	25607.465287	30.398682
439.712617	25652.364688	30.403700
439.926312	25678.539934	30.408717
440.662512	25723.138226	30.413735
440.576319	25766.721511	30.418752
441.382819	25799.022923	30.423770
441.559703	25851.489012	30.428788
442.122525	25891.159948	30.433805
442.645364	25929.408896	30.438823
442.885823	25971.032809	30.443840
443.445787	26006.577431	30.448858
443.421753	26057.994796	30.453876
443.921644	26096.095973	30.458893
444.633531	26147.158135	30.463911
445.227644	26197.948147	30.468928
445.809342	26226.878914	30.473946
446.129470	26273.243703	30.478964
446.941070	26318.741600	30.483981
447.334575	26352.871909	30.488999
447.382256	26394.729132	30.494016
448.073002	26426.841114	30.499034
448.217680	26474.763329	30.504052
448.722840	26512.422051	30.509069
449.382799	26554.708282	30.514087
449.542629	26604.246407	30.519104
450.029683	26644.708078	30.524122
450.630973	26678.610462	30.529140
451.033694	26726.025154	30.534157
451.677702	26751.180026	30.539175
451.675458	26784.507167	30.544192
452.276441	26830.171929	30.549210
452.665695	26864.689304	30.554228
453.133870	26906.298431	30.559245
453.652277	26947.476312	30.564263
454.207209	26986.082491	30.569280
454.577241	27026.063942	30.574298
454.945396	27065.944640	30.579316
455.335689	27111.029955	30.584333
455.969198	27153.144606	30.589351
456.066863	27191.860718	30.594368
457.099083	27244.537743	30.599386
457.371321	27281.336871	30.604404
457.515696	27324.312223	30.609421
458.384186	27358.736415	30.614439
458.581333	27407.986231	30.619456
459.098258	27455.801890	30.624474
459.842665	27504.492186	30.629492
459.965085	27543.401025	30.634509
460.276817	27583.689768	30.639527
460.870821	27633.731245	30.644544
461.328578	27672.442434	30.649562
461.743422	27716.867906	30.654580
462.406904	27769.768381	30.659597
462.967541	27816.939660	30.664615
463.092232	27855.166110	30.669632
463.519986	27896.056719	30.674650
464.252840	27944.111490	30.679668
464.448701	27992.092466	30.684685
465.030509	28038.489819	30.689703
465.283832	28090.437736	30.694720
466.081870	28140.094538	30.699738
466.868383	28188.173083	30.704756
467.181303	28230.397060	30.709773
467.369908	28274.043803	30.714791
467.950698	28315.429584	30.719808
468.509778	28361.249718	30.724826
468.981168	28409.365499	30.729844
469.155055	28459.531687	30.734861
469.997259	28495.011172	30.739879
470.173324	28547.250465	30.744896
471.107830	28600.786972	30.749914
471.343684	28639.490503	30.754932
471.503703	28686.549551	30.759949
472.045040	28728.890480	30.764967
472.446878	28786.739583	30.769984
472.732221	28832.293921	30.775002
473.234296	28884.185927	30.780020
474.183488	28943.087511	30.785037
474.900610	28984.345835	30.790055
475.064421	29026.828682	30.795072
475.654593	29068.991998	30.800090
476.265002	29110.962600	30.805108
476.571893	29157.778488	30.810125
477.140248	29206.525696	30.815143
477.487588	29257.924556	30.820160
478.039536	29304.999486	30.825178
478.604378	29342.571910	30.830196
478.879374	29382.920514	30.835213
479.800778	29425.260242	30.840231
479.837911	29482.883976	30.845248
480.314565	29523.744889	30.850266
481.286279	29571.310944	30.855284
481.525609	29617.443132	30.860301
482.175019	29650.862507	30.865319
482.815811	29693.594404	30.870336
483.032635	29733.112086	30.875354
483.565147	29762.965829	30.880372
483.796532	29806.141355	30.885389
484.222862	29853.407888	30.890407
484.486597	29890.585986	30.895424
484.953372	29932.378481	30.900442
485.647686	29977.346633	30.905460
485.746619	30025.562460	30.910477
486.674739	30070.393055	30.915495
487.003735	30121.455590	30.920512
487.411052	30165.843292	30.925530
487.976275	30207.639889	30.930548
488.389646	30256.635103	30.935565
488.773085	30298.011538	30.940583
488.977195	30352.046286	30.945600
489.460136	30409.090746	30.950618
490.362180	30465.620900	30.955636
490.772247	30514.806887	30.960653
491.270884	30553.965928	30.965671
491.692907	30607.954571	30.970688
491.506618	30653.947125	30.975706
492.640550	30712.919659	30.980724
493.186374	30767.622622	30.985741
493.574308	30806.028253	30.990759
494.188255	30877.036720	30.995776
494.523913	30933.441928	31.000794
495.360310	30979.698572	31.005812
495.425275	31041.229026	31.010829
496.017531	31084.287481	31.015847
496.753809	31143.968329	31.020864
496.916559	31191.614247	31.025882
497.688580	31250.948435	31.030900
498.010803	31303.171807	31.035917
498.698210	31355.628912	31.040935
498.939296	31411.152547	31.045952
499.713152	31463.621672	31.050970
500.371699	31515.103831	31.055988
500.624184	31571.403683	31.061005
501.326211	31626.135017	31.066023
502.002086	31685.611940	31.071040
502.277986	31735.795389	31.076058
503.258900	31780.836361	31.081076
503.535730	31830.235985	31.086093
504.091320	31875.116189	31.091111
504.865873	31928.591553	31.096128
505.111359	31974.690087	31.101146
505.723601	32022.621531	31.106164
506.009074	32079.808977	31.111181
506.663275	32122.676544	31.116199
507.166363	32170.163921	31.121216
507.855542	32222.572357	31.126234
508.106374	32269.132208	31.131252
508.741700	32325.551149	31.136269
509.341211	32368.756530	31.141287
509.848126	32425.530919	31.146304
510.136033	32468.652548	31.151322
511.151836	32501.209915	31.156340
511.143379	32565.398979	31.161357
511.860961	32595.746224	31.166375
512.219602	32655.964704	31.171392
512.362690	32713.397457	31.176410
512.951817	32765.822925	31.181428
513.231742	32827.704303	31.186445
514.159402	32870.094345	31.191463
514.838841	32931.110542	31.196480
514.843622	32981.680841	31.201498
516.016018	33025.727216	31.206516
516.055739	33075.628437	31.211533
516.647395	33127.093435	31.216551
517.110040	33174.526203	31.221568
517.423329	33218.334524	31.226586
518.085445	33261.095706	31.231604
518.404252	33323.010387	31.236621
518.851735	33372.494401	31.241639
519.240256	33432.122454	31.246656
519.860941	33480.403641	31.251674
520.527386	33531.238327	31.256692
521.121811	33588.337243	31.261709
521.643523	33645.156873	31.266727
522.256058	33697.113144	31.271744
522.670598	33746.717000	31.276762
522.940208	33792.619758	31.281780
523.514758	33853.269392	31.286797
524.184133	33904.913796	31.291815
524.768159	33979.193557	31.296832
525.095982	34029.317459	31.301850
525.804541	34083.175363	31.306868
526.142468	34152.309809	31.311885
526.723744	34199.315341	31.316903
527.186218	34265.357888	31.321920
527.547199	34319.245542	31.326938
528.626909	34379.754346	31.331956
529.122857	34439.716166	31.336973
529.325824	34487.780567	31.341991
530.051365	34548.851136	31.347008
530.755397	34606.232807	31.352026
531.697952	34656.938446	31.357044
532.066749	34710.857487	31.362061
532.477155	34759.560222	31.367079
532.836164	34805.843188	31.372096
533.661637	34875.586495	31.377114
534.555318	34918.852208	31.382132
534.902442	34976.056837	31.387149
535.271357	35026.752041	31.392167
535.602932	35077.339404	31.397184
536.009059	35138.904299	31.402202
536.971326	35185.599440	31.407220
537.632099	35253.049298	31.412237
538.231202	35296.191201	31.417255
538.448319	35353.050480	31.422272
539.152895	35404.908013	31.427290
539.755988	35451.223711	31.432308
540.044106	35518.239587	31.437325
540.434225	35570.051929	31.442343
541.386133	35628.725368	31.447360
541.672708	35690.260001	31.452378
542.681956	35731.131825	31.457396
543.016259	35791.723470	31.462413
543.728215	35841.500636	31.467431
544.157742	35895.090697	31.472448
544.271699	35949.767300	31.477466
545.073962	35991.886074	31.482484
545.405519	36057.550024	31.487501
546.171471	36105.650050	31.492519
546.865620	36164.491799	31.497536
546.953135	36215.050536	31.502554
547.476149	36261.703020	31.507572
548.045340	36329.802950	31.512589
548.995222	36392.822846	31.517607
549.618631	36442.077810	31.522624
550.024930	36501.863470	31.527642
550.716661	36546.283341	31.532660
551.170770	36608.180100	31.537677
551.599210	36658.623258	31.542695
552.129715	36716.252793	31.547712
552.618227	36758.428543	31.552730
553.046338	36814.038269	31.557748
553.460692	36867.803876	31.562765
553.971114	36927.460597	31.567783
554.699945	36974.651506	31.572800
554.786760	37030.049664	31.577818
555.605296	37080.862712	31.582836
556.011107	37138.652027	31.587853
556.801511	37190.873543	31.592871
557.408735	37256.479028	31.597888
557.602500	37305.012834	31.602906
558.229464	37356.861973	31.607924
558.667051	37427.837902	31.612941
559.332257	37491.512675	31.617959
560.045701	37550.658743	31.622976
560.340993	37623.327020	31.627994
561.081703	37675.102201	31.633012
561.373489	37742.997123	31.638029
561.962552	37801.233790	31.643047
562.364044	37860.189269	31.648064
562.733820	37937.355696	31.653082
564.009844	37998.729349	31.658100
564.296762	38071.014703	31.663117
564.990888	38141.832657	31.668135
565.689029	38194.336658	31.673152
565.685028	38262.488224	31.678170
566.793916	38328.106940	31.683188
567.072873	38385.887852	31.688205
567.825791	38458.525214	31.693223
568.262802	38521.486236	31.698240
568.753495	38585.324374	31.703258
569.760759	38662.184865	31.708276
570.375542	38722.405688	31.713293
571.187923	38783.955373	31.718311
571.942117	38843.357886	31.723328
572.288114	38905.967493	31.728346
572.970338	38956.496445	31.733364
573.584881	39024.294253	31.738381
573.813632	39078.126063	31.743399
574.576790	39143.200622	31.748416
574.742814	39213.820214	31.753434
575.425600	39273.962356	31.758452
576.544301	39342.365198	31.763469
577.007588	39403.617169	31.768487
577.635554	39463.028502	31.773504
578.057906	39524.919636	31.778522
579.038058	39582.802618	31.783540
579.510056	39639.291809	31.788557
579.758370	39704.815484	31.793575
580.489682	39761.182165	31.798592
580.797030	39838.535895	31.803610
581.509947	39898.478996	31.808628
582.378437	39959.586857	31.813645
582.582371	40023.423541	31.818663
583.301014	40080.716377	31.823680
583.880546	40151.729600	31.828698
584.542208	40208.102022	31.833716
584.864869	40260.631888	31.838733
585.456093	40332.706358	31.843751
586.505175	40391.282700	31.848768
586.713378	40459.237160	31.853786
587.455891	40517.267360	31.858804
588.518240	40582.343637	31.863821
588.736540	40650.474194	31.868839
589.409819	40686.006967	31.873856
590.101913	40755.081887	31.878874
590.379326	40822.672465	31.883892
591.089615	40871.443257	31.888909
591.424464	40932.846128	31.893927
592.312621	40978.509255	31.898944
592.867921	41043.811781	31.903962
593.229910	41097.456945	31.908980
593.729222	41154.913440	31.913997
594.042467	41212.588965	31.919015
594.742904	41274.017756	31.924032
595.323069	41342.340451	31.929050
596.078185	41401.174252	31.934068
596.536996	41470.408130	31.939085
596.778959	41523.175026	31.944103
597.773835	41589.327415	31.949120
598.285273	41660.071582	31.954138
598.687040	41728.505639	31.959156
599.534602	41784.258478	31.964173
599.607349	41863.989945	31.969191
600.711542	41923.548426	31.974208
600.889915	41999.538523	31.979226
601.471631	42071.873192	31.984244
602.213964	42133.386371	31.989261
602.757775	42218.301321	31.994279
603.596765	42287.807123	31.999296
604.248200	42354.489968	32.004314
604.887607	42419.296385	32.009332
605.508434	42486.964793	32.014349
606.049278	42557.896985	32.019367
606.716040	42631.674920	32.024384
607.491412	42700.255881	32.029402
608.348524	42774.080380	32.034420
609.268887	42831.386757	32.039437
609.294345	42906.663886	32.044455
609.771315	42959.802218	32.049472
610.403171	43038.248586	32.054490
611.134972	43111.252591	32.059508
611.782124	43178.197922	32.064525
612.208871	43253.116097	32.069543
613.045297	43328.482708	32.074560
613.766629	43385.144889	32.079578
614.189520	43461.569778	32.084596
614.935917	43525.565694	32.089613
615.132265	43598.225040	32.094631
616.292987	43664.971228	32.099648
616.739282	43743.695836	32.104666
617.511381	43808.618367	32.109684
617.965664	43878.233687	32.114701
618.369495	43962.570004	32.119719
619.348133	44025.202653	32.124736
619.642447	44104.970731	32.129754
620.219847	44175.984599	32.134772
620.965019	44244.410598	32.139789
621.505874	44320.345547	32.144807
622.352741	44381.563946	32.149824
623.215562	44451.186654	32.154842
623.229817	44537.730512	32.159860
624.381638	44604.588447	32.164877
624.684332	44681.763783	32.169895
625.698853	44749.668402	32.174912
626.409939	44820.277519	32.179930
627.040587	44884.320766	32.184948
628.075078	44954.120578	32.189965
628.262915	45011.888880	32.194983
628.979314	45076.393674	32.200000
629.562346	45149.712313	32.205018
629.979429	45222.608052	32.210036
630.617540	45286.973894	32.215053
630.810901	45359.215603	32.220071
631.560358	45422.375147	32.225088
632.380625	45500.009937	32.230106
632.974670	45560.973842	32.235124
633.691465	45629.655228	32.240141
634.085646	45690.701391	32.245159
634.513779	45771.106009	32.250176
635.439386	45840.919306	32.255194
636.127707	45909.536421	32.260212
636.730604	45963.756569	32.265229
637.143795	46045.758650	32.270247
637.844926	46105.492670	32.275264
638.634158	46181.787233	32.280282
638.961070	46249.816728	32.285300
639.834277	46327.344864	32.290317
640.208952	46395.911361	32.295335
640.908387	46468.709980	32.300352
641.621531	46545.188493	32.305370
641.890086	46629.809058	32.310388
642.444175	46703.421963	32.315405
643.215067	46782.131699	32.320423
643.765067	46863.931863	32.325440
644.541485	46936.745237	32.330458
645.244025	47019.236939	32.335476
646.141348	47092.765726	32.340493
646.435643	47183.387968	32.345511
647.333026	47254.234916	32.350528
648.164747	47335.910422	32.355546
648.847421	47411.846240	32.360564
649.316368	47499.899192	32.365581
650.151942	47573.243088	32.370599
650.734755	47649.499007	32.375616
651.927759	47726.545326	32.380634
651.893926	47810.002965	32.385652
652.756022	47876.643945	32.390669
653.131704	47956.330659	32.395687
653.985134	48028.736902	32.400704
654.790998	48114.797221	32.405722
655.265884	48198.511920	32.410740
656.409963	48276.326952	32.415757
656.845842	48353.576208	32.420775
657.562806	48436.482020	32.425792
658.089209	48513.028033	32.430810
658.890986	48586.285583	32.435828
659.232738	48670.174699	32.440845
660.068480	48750.994213	32.445863
660.933924	48826.672031	32.450880
661.777649	48907.838821	32.455898
662.238182	48978.481164	32.460916
663.197159	49051.532107	32.465933
663.544017	49129.727965	32.470951
664.412460	49208.019560	32.475968
664.848226	49292.611166	32.480986
665.325584	49364.789497	32.486004
666.271473	49441.317205	32.491021
666.833233	49528.477663	32.496039
667.470421	49612.754191	32.501056
668.184576	49680.562450	32.506074
668.819662	49758.544480	32.511092
669.815526	49837.666086	32.516109
670.233288	49915.619411	32.521127
671.108378	49994.406154	32.526144
671.627138	50075.811445	32.531162
672.070293	50160.031781	32.536180
673.107320	50235.997398	32.541197
673.545617	50312.569530	32.546215
674.384643	50390.173764	32.551232
674.913482	50454.659910	32.556250
675.257333	50543.636274	32.561268
675.954803	50620.643381	32.566285
677.040451	50705.138394	32.571303
677.715998	50785.471303	32.576320
678.399263	50847.802062	32.581338
679.133777	50921.944423	32.586356
679.688000	50987.162048	32.591373
680.764715	51063.402573	32.596391
680.836920	51121.368963	32.601408
681.739932	51196.529834	32.606426
681.945705	51285.891331	32.611444
682.564010	51366.437694	32.616461
683.256885	51446.257653	32.621479
683.870571	51526.615469	32.626496
684.800380	51594.749908	32.631514
685.307011	51680.123760	32.636532
686.499381	51759.322403	32.641549
686.991513	51842.604697	32.646567
687.518869	51913.777061	32.651584
688.363075	52002.598395	32.656602
688.874563	52092.218834	32.661620
689.674023	52168.670921	32.666637
690.352526	52248.337686	32.671655
690.883930	52333.096260	32.676672
691.983496	52418.247076	32.681690
692.059286	52497.793933	32.686708
692.853124	52587.663132	32.691725
693.938517	52664.508680	32.696743
694.263695	52770.106975	32.701760
695.377498	52844.626349	32.706778
696.007758	52933.959314	32.711796
696.665634	53009.885795	32.716813
697.130295	53104.200088	32.721831
697.882626	53188.977784	32.726848
698.944796	53274.795676	32.731866
699.510038	53368.715600	32.736884
700.196251	53444.620065	32.741901
701.014449	53531.957858	32.746919
701.383587	53617.227412	32.751936
702.471555	53706.611869	32.756954
702.847177	53795.007126	32.761972
703.833413	53878.320523	32.766989
704.581175	53960.924836	32.772007
705.076157	54053.624501	32.777024
706.088534	54140.662029	32.782042
706.665665	54232.944529	32.787060
707.198037	54312.008350	32.792077
708.081862	54402.857597	32.797095
708.691717	54491.908562	32.802112
709.833486	54572.447241	32.807130
710.205073	54670.231301	32.812148
711.001161	54747.185909	32.817165
711.423952	54835.444770	32.822183
712.340685	54923.797476	32.827200
713.057855	55017.035674	32.832218
713.773097	55106.629346	32.837236
714.504968	55192.999551	32.842253
715.047263	55287.228124	32.847271
715.687954	55365.708928	32.852288
716.512684	55456.425907	32.857306
716.997874	55553.765469	32.862324
717.930036	55629.764995	32.867341
718.837214	55727.640402	32.872359
719.224835	55819.996714	32.877376
720.432644	55909.092250	32.882394
720.958857	56003.345156	32.887412
722.050222	56079.738880	32.892429
722.645045	56173.855141	32.897447
722.910822	56252.720338	32.902464
723.833554	56347.640316	32.907482
724.843398	56430.515952	32.912500
725.581441	56516.219126	32.917517
725.993762	56601.036943	32.922535
726.556370	56678.736851	32.927552
727.644612	56749.861249	32.932570
727.978839	56828.274597	32.937588
728.592266	56906.030572	32.942605
729.405270	57000.799437	32.947623
729.983639	57084.327164	32.952640
731.257626	57177.644820	32.957658
731.473402	57264.938755	32.962676
732.019851	57347.320510	32.967693
732.792187	57435.502582	32.972711
733.565075	57518.298827	32.977728
734.464368	57613.012285	32.982746
735.198253	57708.827974	32.987764
735.600816	57794.974316	32.992781
736.484901	57890.305174	32.997799
737.782707	57985.204527	33.002816
738.396531	58071.888404	33.007834
739.104513	58161.190821	33.012852
739.578638	58255.903758	33.017869
740.337411	58337.597394	33.022887
741.353586	58449.188768	33.027904
741.989059	58534.003752	33.032922
742.793398	58626.489124	33.037940
743.625350	58719.964242	33.042957
744.430573	58812.627408	33.047975
744.828680	58910.089117	33.052992
745.658244	59003.211249	33.058010
746.437360	59091.683118	33.063028
747.399882	59193.083143	33.068045
748.134437	59282.303238	33.073063
748.615993	59379.798065	33.078080
749.342447	59477.077703	33.083098
750.183026	59580.821404	33.088116
750.969671	59671.439944	33.093133
752.112458	59767.212380	33.098151
752.450422	59858.844998	33.103168
753.490321	59948.443803	33.108186
754.024305	60044.521541	33.113204
754.619703	60148.647851	33.118221
755.822117	60244.931862	33.123239
756.334398	60343.666361	33.128256
757.008508	60439.711045	33.133274
757.796990	60538.732229	33.138292
758.894824	60631.381792	33.143309
759.762050	60724.833738	33.148327
760.170328	60830.777282	33.153344
761.074035	60917.362573	33.158362
761.973046	61018.925695	33.163380
762.542449	61111.590185	33.168397
763.578990	61202.871552	33.173415
764.395689	61306.449045	33.178432
765.217076	61391.219499	33.183450
765.717540	61486.181358	33.188468
766.313162	61588.224780	33.193485
767.660766	61680.510009	33.198503
767.908865	61780.715922	33.203520
768.543068	61868.264631	33.208538
769.385247	61960.838948	33.213556
770.202525	62061.596223	33.218573
770.991384	62150.539692	33.223591
771.465913	62263.505629	33.228608
772.781784	62356.678263	33.233626
773.204613	62454.181796	33.238644
773.937704	62550.409030	33.243661
775.058193	62645.582096	33.248679
775.435985	62746.056463	33.253696
776.143245	62838.174063	33.258714
777.186284	62929.061953	33.263732
777.711812	63025.893270	33.268749
778.706989	63117.681945	33.273767
779.456480	63203.039594	33.278784
780.345187	63297.504439	33.283802
780.866778	63386.779053	33.288820
781.276372	63479.895224	33.293837
782.094399	63581.411875	33.298855
782.841978	63681.350967	33.303872
783.241653	63779.293786	33.308890
784.604811	63877.630559	33.313908
785.146954	63986.339450	33.318925
786.404526	64083.009580	33.323943
786.845923	64185.505616	33.328960
787.569465	64287.210851	33.333978
788.497086	64390.619196	33.338996
789.335606	64491.560211	33.344013
790.190753	64591.441764	33.349031
790.627094	64695.915915	33.354048
791.595930	64810.487309	33.359066
792.202113	64908.326214	33.364084
793.218021	65015.895425	33.369101
794.190936	65122.769080	33.374119
795.041209	65233.733271	33.379136
795.688747	65341.589469	33.384154
797.205280	65443.669017	33.389172
797.308316	65547.825343	33.394189
798.536693	65648.121135	33.399207
799.016614	65752.174965	33.404224
799.858371	65865.625088	33.409242
801.017986	65957.980847	33.414260
801.536115	66065.892044	33.419277
802.262653	66167.306799	33.424295
803.302014	66281.734515	33.429312
804.008525	66384.159952	33.434330
804.539021	66489.247220	33.439348
805.301204	66588.499067	33.444365
806.663563	66703.359285	33.449383
807.302869	66813.603636	33.454400
808.195879	66909.613530	33.459418
809.193269	67012.337840	33.464436
809.946348	67116.531747	33.469453
810.911253	67213.854817	33.474471
811.532988	67327.079966	33.479488
812.548729	67423.186537	33.484506
813.514138	67527.684443	33.489524
813.869291	67637.128392	33.494541
814.963015	67737.827054	33.499559
815.635650	67843.714410	33.504576
816.575976	67951.624434	33.509594
817.291838	68056.486484	33.514612
818.072073	68160.952642	33.519629
819.138374	68259.460506	33.524647
819.848568	68365.806349	33.529664
820.780543	68462.993673	33.534682
821.178023	68565.507867	33.539700
822.246369	68671.551943	33.544717
823.329197	68777.834801	33.549735
823.909026	68883.101426	33.554752
824.452794	68978.508870	33.559770
825.108296	69089.545600	33.564788
825.980470	69193.494971	33.569805
827.147870	69296.372734	33.574823
827.738038	69421.339020	33.579840
828.597683	69531.484507	33.584858
829.430592	69631.579179	33.589876
830.329759	69735.672132	33.594893
831.026684	69832.160527	33.599911
831.764553	69935.196727	33.604928
832.334847	70032.978473	33.609946
833.422776	70148.067974	33.614964
834.442936	70244.171669	33.619981
835.145769	70353.775277	33.624999
835.966874	70447.061337	33.630016
836.813909	70550.310835	33.635034
837.494071	70656.765736	33.640052
838.158442	70766.047808	33.645069
839.169594	70869.488168	33.650087
840.245416	70984.836544	33.655104
840.918014	71083.695382	33.660122
841.685522	71189.353536	33.665140
842.416786	71295.815693	33.670157
843.251190	71404.643182	33.675175
843.944715	71524.347280	33.680192
844.843173	71640.308904	33.685210
845.688931	71750.491229	33.690228
846.389205	71868.739320	33.695245
847.739756	71980.363410	33.700263
848.441159	72096.370558	33.705280
849.253248	72206.952689	33.710298
849.916453	72317.368612	33.715316
850.567930	72435.791530	33.720333
851.636754	72557.974675	33.725351
852.736943	72673.681259	33.730368
853.543363	72804.228044	33.735386
854.340285	72909.128516	33.740404
855.265202	73035.820119	33.745421
856.197519	73144.284782	33.750439
857.175336	73259.645763	33.755456
858.052065	73373.693130	33.760474
859.121447	73489.268757	33.765492
859.876993	73617.724912	33.770509
860.433020	73728.340797	33.775527
861.740649	73838.434130	33.780544
862.273411	73954.805110	33.785562
863.363781	74070.962620	33.790580
864.051864	74197.848816	33.795597
864.917257	74313.168613	33.800615
865.661022	74426.595293	33.805632
866.543399	74548.322746	33.810650
867.960226	74665.521045	33.815668
868.557580	74792.284920	33.820685
869.718734	74909.068310	33.825703
870.349533	75026.061919	33.830720
871.214548	75138.763267	33.835738
872.735873	75244.116800	33.840756
873.102501	75369.513478	33.845773
874.225225	75474.765652	33.850791
874.953085	75590.885145	33.855808
875.586936	75709.540631	33.860826
876.570140	75820.782253	33.865844
877.640838	75938.673641	33.870861
878.657571	76051.152356	33.875879
879.281402	76168.836031	33.880896
880.286334	76289.906098	33.885914
881.488169	76400.621831	33.890932
881.852242	76523.440061	33.895949
882.645603	76624.555294	33.900967
883.436965	76738.693597	33.905984
884.357659	76871.560392	33.911002
885.384476	76983.699350	33.916020
886.198077	77102.763468	33.921037
887.165019	77210.149616	33.926055
887.993351	77331.974029	33.931072
888.632897	77460.377910	33.936090
889.697256	77576.491178	33.941108
890.331011	77692.013618	33.946125
890.893989	77788.925403	33.951143
892.282873	77901.847526	33.956160
892.935585	78019.838680	33.961178
893.874279	78128.829049	33.966196
894.674316	78250.623959	33.971213
895.695531	78363.352178	33.976231
896.376328	78485.318816	33.981248
897.227397	78599.974915	33.986266
898.298344	78718.904387	33.991284
899.064461	78845.027223	33.996301
900.057871	78967.035717	34.001319
900.976378	79088.993133	34.006336
901.787603	79212.526149	34.011354
902.677381	79322.821104	34.016372
903.085930	79459.847281	34.021389
904.020422	79586.795943	34.026407
905.204664	79713.262661	34.031424
905.988695	79851.714254	34.036442
907.353862	79972.794786	34.041460
908.121181	80109.476591	34.046477
909.080812	80235.588101	34.051495
910.125228	80352.755015	34.056512
910.401088	80490.225115	34.061530
911.872716	80612.748733	34.066548
912.647897	80749.635144	34.071565
913.714071	80880.445938	34.076583
914.691679	81003.732774	34.081600
915.717029	81148.361117	34.086618
916.971442	81261.761385	34.091636
917.619228	81395.376752	34.096653
918.776788	81517.408690	34.101671
919.680816	81639.316144	34.106688
920.538803	81773.432525	34.111706
921.727969	81899.718282	34.116724
922.226654	82025.783293	34.121741
923.347027	82147.950478	34.126759
924.560684	82267.810277	34.131776
925.195733	82399.899289	34.136794
926.474980	82523.893077	34.141812
927.180182	82654.413838	34.146829
928.182230	82769.772895	34.151847
929.189213	82895.458090	34.156864
929.882851	83031.950191	34.161882
931.124359	83154.178759	34.166900
931.762874	83285.397064	34.171917
932.378337	83403.454711	34.176935
934.060699	83534.371343	34.181952
934.633747	83668.123136	34.186970
935.718994	83792.406233	34.191988
936.638552	83920.365041	34.197005
937.564932	84055.735884	34.202023
938.538588	84176.452225	34.207040
939.343001	84301.503747	34.212058
940.268362	84430.350894	34.217076
941.001071	84564.816790	34.222093
941.865720	84698.274295	34.227111
943.235276	84817.993663	34.232128
943.861489	84953.719836	34.237146
944.711869	85074.940753	34.242164
945.554110	85220.606782	34.247181
946.406660	85344.375461	34.252199
947.859886	85478.517376	34.257216
948.727390	85613.207801	34.262234
949.610882	85733.970109	34.267252
950.564612	85876.631445	34.272269
951.314459	86013.420319	34.277287
952.769002	86137.706371	34.282304
953.442574	86258.681130	34.287322
954.407149	86369.384515	34.292340
955.395171	86482.175538	34.297357
955.900661	86617.598903	34.302375
956.927408	86744.450926	34.307392
958.006657	86872.841290	34.312410
959.401629	86995.239483	34.317428
959.944577	87116.770476	34.322445
960.521636	87249.549709	34.327463
961.825107	87374.143461	34.332480
962.538513	87503.151448	34.337498
963.575837	87637.279686	34.342516
964.618849	87764.767195	34.347533
965.544633	87905.922073	34.352551
966.788626	88042.148802	34.357568
967.368455	88171.155277	34.362586
968.081105	88300.863870	34.367604
969.443754	88444.246700	34.372621
969.942252	88586.865743	34.377639
971.412035	88723.072925	34.382656
972.141608	88864.934762	34.387674
973.211781	88995.338123	34.392692
974.357525	89133.993144	34.397709
975.109924	89276.195542	34.402727
976.180798	89418.120633	34.407744
977.085403	89564.812274	34.412762
978.319821	89707.460863	34.417780
979.130737	89841.355686	34.422797
979.977200	89993.520806	34.427815
981.085812	90134.353459	34.432832
982.112614	90291.890817	34.437850
982.843670	90429.590199	34.442868
984.158842	90569.771537	34.447885
985.156481	90719.508640	34.452903
985.857070	90856.733136	34.457920
986.818248	91006.375978	34.462938
987.987399	91143.933984	34.467956
989.452373	91295.210374	34.472973
990.209808	91452.821313	34.477991
991.482774	91583.863215	34.483008
992.079901	91736.443711	34.488026
993.018861	91875.600014	34.493044
994.162067	92022.164851	34.498061
995.244829	92164.177049	34.503079
996.144705	92314.938617	34.508096
997.256815	92467.023881	34.513114
998.429160	92612.509652	34.518132
999.700063	92758.107431	34.523149
1000.143604	92905.559208	34.528167
1001.482126	93037.965969	34.533184
1002.312425	93186.588001	34.538202
1003.618830	93335.567158	34.543220
1004.413896	93472.611186	34.548237
1005.679805	93629.570687	34.553255
1006.520946	93758.268576	34.558272
1007.106497	93913.485472	34.563290
1008.379781	94056.592013	34.568308
1009.820901	94208.647055	34.573325
1010.509058	94358.475788	34.578343
1011.857106	94492.611154	34.583360
1012.481202	94639.523251	34.588378
1013.954327	94793.807036	34.593396
1015.007999	94925.062307	34.598413
1015.662594	95070.298482	34.603431
1017.081400	95217.253665	34.608448
1018.210379	95346.179262	34.613466
1018.983306	95491.538304	34.618484
1019.824528	95610.749657	34.623501
1020.570770	95750.625424	34.628519
1021.655199	95886.189735	34.633536
1022.824129	96022.070979	34.638554
1023.685972	96157.227648	34.643572
1024.598164	96274.199417	34.648589
1025.185075	96425.106028	34.653607
1026.496109	96561.296935	34.658624
1027.415839	96697.169404	34.663642
1028.019898	96852.043058	34.668660
1029.246231	96998.250774	34.673677
1030.050388	97139.264517	34.678695
1031.436022	97290.912212	34.683712
1032.400240	97446.581714	34.688730
1033.484317	97593.739840	34.693748
1034.691639	97747.534637	34.698765
1035.607601	97907.359241	34.703783
1036.849138	98055.065303	34.708800
1037.822546	98199.720860	34.713818
1038.605380	98351.227120	34.718836
1039.932319	98502.217892	34.723853
1040.689715	98659.497644	34.728871
1042.167978	98802.682404	34.733888
1043.242479	98958.367361	34.738906
1044.053103	99117.948277	34.743924
1045.409738	99268.506976	34.748941
1045.774659	99417.877839	34.753959
1047.178001	99581.627858	34.758976
1048.353343	99743.271901	34.763994
1049.138837	99904.597460	34.769012
1050.461424	100052.845147	34.774029
1051.295610	100217.803123	34.779047
1052.308447	100374.873750	34.784064
1053.379806	100524.075720	34.789082
1054.470127	100695.537778	34.794100
1055.505123	100848.296736	34.799117
1056.557774	101021.630064	34.804135
1057.975620	101182.330476	34.809152
1059.172637	101338.159809	34.814170
1060.050274	101499.250626	34.819188
1061.612290	101660.919715	34.824205
1062.413836	101824.648442	34.829223
1063.651319	101975.250992	34.834240
1064.649238	102134.792006	34.839258
1065.297563	102288.226768	34.844276
1066.753693	102449.434521	34.849293
1067.891065	102620.658371	34.854311
1068.977882	102773.088512	34.859328
1069.986869	102932.048419	34.864346
1070.968757	103085.472687	34.869364
1072.168471	103243.389918	34.874381
1072.716712	103416.954265	34.879399
1074.194526	103573.599665	34.884416
1075.253079	103734.926617	34.889434
1076.515057	103892.596271	34.894452
1077.897335	104055.547731	34.899469
1078.561924	104215.239665	34.904487
1079.528603	104369.090623	34.909504
1080.487147	104543.091063	34.914522
1081.816407	104698.661876	34.919540
1083.102346	104860.085430	34.924557
1083.947987	105021.794241	34.929575
1084.915602	105168.243849	34.934592
1085.949570	105336.315198	34.939610
1087.273112	105508.564394	34.944628
1088.661536	105651.653483	34.949645
1089.447859	105822.010329	34.954663
1090.529348	105973.758441	34.959680
1091.624418	106124.579466	34.964698
1092.216527	106286.625630	34.969716
1094.098532	106432.189410	34.974733
1094.529879	106580.047779	34.979751
1095.290394	106728.996469	34.984768
1096.720807	106889.684270	34.989786
1097.376943	107044.508941	34.994804
1098.748340	107205.904877	34.999821
1100.076500	107377.706280	35.004839
1100.946924	107528.708136	35.009856
1101.996037	107695.482619	35.014874
1102.792437	107862.145303	35.019892
1104.605588	108013.229937	35.024909
1105.351375	108188.715170	35.029927
1106.527473	108335.006184	35.034944
1107.452353	108506.990456	35.039962
1108.444633	108689.921318	35.044980
1109.439903	108855.708013	35.049997
1110.394088	109028.869599	35.055015
1111.561544	109206.272179	35.060032
1113.038675	109379.543847	35.065050
1113.882291	109558.926445	35.070068
1115.045587	109728.786998	35.075085
1116.368288	109908.743123	35.080103
1117.601378	110079.634313	35.085120
1119.052026	110252.660801	35.090138
1119.875503	110429.819046	35.095156
1121.040101	110600.165489	35.100173
1122.093916	110786.153885	35.105191
1123.104334	110964.363475	35.110208
1124.419087	111140.129456	35.115226
1125.184664	111319.634651	35.120244
1126.580643	111493.779067	35.125261
1127.573166	111666.985618	35.130279
1129.206099	111848.374114	35.135296
1130.189233	112021.900903	35.140314
1131.396136	112205.374353	35.145332
1132.628517	112380.474486	35.150349
1134.188912	112549.233711	35.155367
1135.134071	112725.674079	35.160384
1136.370762	112897.795701	35.165402
1137.691597	113077.932965	35.170420
1138.803757	113248.908965	35.175437
1139.964897	113435.021106	35.180455
1140.734810	113599.546169	35.185472
1142.058677	113773.256308	35.190490
1143.257027	113946.910828	35.195508
1144.557055	114114.158113	35.200525
1145.830976	114297.517511	35.205543
1146.652864	114457.903682	35.210560
1147.956609	114634.106917	35.215578
1148.737758	114819.232903	35.220596
1150.219494	114995.092926	35.225613
1150.932788	115176.629323	35.230631
1152.159407	115345.466419	35.235648
1153.323872	115520.376635	35.240666
1154.628622	115699.400493	35.245684
1155.907334	115880.636207	35.250701
1157.090097	116057.271036	35.255719
1158.111418	116233.006077	35.260736
1159.094430	116409.686530	35.265754
1159.963667	116594.617331	35.270772
1161.446155	116785.071936	35.275789
1162.862729	116967.191889	35.280807
1163.677543	117138.448078	35.285824
1164.901808	117319.052411	35.290842
1166.149489	117503.154722	35.295860
1167.395398	117671.897841	35.300877
1169.027295	117853.937637	35.305895
1169.674242	118007.922949	35.310912
1170.930123	118172.252654	35.315930
1171.668745	118340.723009	35.320948
1173.112618	118501.092587	35.325965
1173.971224	118678.614937	35.330983
1174.988649	118848.578699	35.336000
1176.293722	119027.275850	35.341018
1177.010867	119205.203323	35.346036
1178.622505	119384.069783	35.351053
1179.591688	119568.428633	35.356071
1180.986958	119750.869693	35.361088
1182.264652	119935.384958	35.366106
1183.141985	120122.424640	35.371124
1184.433990	120297.273541	35.376141
1185.754884	120477.154638	35.381159
1186.900069	120668.708926	35.386176
1188.042540	120851.943167	35.391194
1188.980801	121038.470319	35.396212
1190.267767	121217.890801	35.401229
1191.587245	121418.326499	35.406247
1192.501395	121602.792418	35.411264
1194.131718	121788.009697	35.416282
1195.617555	121982.231766	35.421300
1196.237615	122169.981173	35.426317
1197.789408	122372.110596	35.431335
1198.781825	122560.970644	35.436352
1200.308290	122756.166951	35.441370
1201.181630	122951.377662	35.446388
1202.500388	123138.362621	35.451405
1203.505951	123336.256600	35.456423
1204.882411	123527.877385	35.461440
1206.049178	123714.800036	35.466458
1207.365651	123923.203002	35.471476
1208.830190	124115.941872	35.476493
1209.928361	124318.380523	35.481511
1211.196441	124509.642375	35.486528
1212.524740	124706.515743	35.491546
1213.505184	124914.329435	35.496564
1215.066852	125098.304189	35.501581
1216.417137	125290.838192	35.506599
1217.316335	125493.859385	35.511616
1218.990251	125691.711035	35.516634
1220.034871	125887.391240	35.521652
1221.210528	126070.073331	35.526669
1222.654765	126264.068875	35.531687
1223.801325	126464.112817	35.536704
1225.393769	126657.262369	35.541722
1226.475239	126858.041566	35.546740
1227.185130	127040.153836	35.551757
1228.560254	127236.537247	35.556775
1229.607326	127436.461908	35.561792
1231.464311	127628.039429	35.566810
1232.332114	127826.902928	35.571828
1233.614042	128025.207739	35.576845
1235.137263	128212.006313	35.581863
1236.075331	128415.352945	35.586880
1237.299017	128601.997144	35.591898
1238.475830	128806.259855	35.596916
1239.872767	129005.655108	35.601933
1240.793724	129201.116502	35.606951
1241.906148	129406.863965	35.611968
1243.508178	129603.108738	35.616986
1244.791242	129804.898195	35.622004
1246.174740	130002.016416	35.627021
1247.194896	130202.212164	35.632039
1248.691670	130390.940374	35.637056
1249.737380	130583.939784	35.642074
1250.990475	130777.783080	35.647092
1252.210510	130962.902932	35.652109
1253.249238	131140.223301	35.657127
1254.873711	131329.646178	35.662144
1255.989642	131508.338996	35.667162
1256.841136	131706.512613	35.672180
1258.205361	131890.738357	35.677197
1259.383881	132087.999701	35.682215
1260.379463	132278.984340	35.687232
1261.852726	132469.780839	35.692250
1262.616379	132664.280152	35.697268
1263.866497	132868.994764	35.702285
1265.524211	133075.600602	35.707303
1266.605629	133288.603995	35.712320
1267.921310	133485.735938	35.717338
1269.311862	133691.054131	35.722356
1270.330421	133889.985462	35.727373
1271.662569	134096.405927	35.732391
1272.716386	134311.766028	35.737408
1273.968242	134517.452344	35.742426
1275.073094	134729.735669	35.747444
1276.609362	134935.899641	35.752461
1278.203310	135158.830934	35.757479
1279.106969	135378.115296	35.762496
1280.786846	135596.619357	35.767514
1282.078994	135811.340215	35.772532
1283.092118	136029.468522	35.777549
1284.451508	136235.818369	35.782567
1285.750396	136455.617090	35.787584
1287.402804	136678.838543	35.792602
1288.349181	136894.544968	35.797620
1289.766877	137106.574677	35.802637
1291.453813	137334.400356	35.807655
1292.354368	137563.048207	35.812672
1294.072994	137764.551817	35.817690
1294.891564	137979.039665	35.822708
1295.917550	138192.252386	35.827725
1297.787073	138422.097941	35.832743
1299.167865	138651.285083	35.837760
1300.308831	138867.833137	35.842778
1301.868006	139093.606164	35.847796
1303.276376	139305.571171	35.852813
1304.417757	139525.218667	35.857831
1305.495797	139753.214865	35.862848
1307.681145	139970.467444	35.867866
1308.742048	140182.427295	35.872884
1309.780096	140403.529070	35.877901
1311.078265	140622.992092	35.882919
1312.451796	140851.848321	35.887936
1313.982443	141064.741120	35.892954
1315.016053	141285.746109	35.897972
1316.118343	141507.553586	35.902989
1317.699536	141721.418572	35.908007
1318.775077	141946.836536	35.913024
1320.505639	142178.346365	35.918042
1321.806585	142404.035742	35.923060
1323.151812	142624.249219	35.928077
1324.723066	142846.928522	35.933095
1325.979038	143061.484830	35.938112
1327.509909	143276.747841	35.943130
1328.946454	143499.057722	35.948148
1329.925855	143715.462360	35.953165
1331.131362	143935.043557	35.958183
1332.449649	144158.923280	35.963200
1333.742941	144367.818816	35.968218
1335.302623	144592.309968	35.973236
1336.752107	144817.276279	35.978253
1338.135997	145026.249202	35.983271
1338.985392	145237.629300	35.988288
1340.387700	145442.514200	35.993306
1341.685294	145643.354813	35.998324
1342.787832	145852.095934	36.003341
1344.312699	146054.692191	36.008359
1345.565161	146268.805760	36.013376
1346.906205	146480.532875	36.018394
1348.308902	146691.223118	36.023412
1349.598018	146906.552065	36.028429
1351.016184	147116.480064	36.033447
1352.125673	147339.847917	36.038464
1352.997449	147562.136980	36.043482
1354.992177	147779.529524	36.048500
1356.208398	148003.429284	36.053517
1357.892116	148223.461667	36.058535
1358.864626	148446.233712	36.063552
1360.569695	148668.384311	36.068570
1361.203584	148895.158741	36.073588
1362.545831	149127.966683	36.078605
1364.301022	149344.222685	36.083623
1365.590684	149593.135708	36.088640
1367.036285	149824.216918	36.093658
1368.440673	150052.081483	36.098676
1369.842991	150276.786698	36.103693
1371.364110	150507.579751	36.108711
1372.282285	150751.783543	36.113728
1373.724133	150974.124471	36.118746
1375.299048	151217.935595	36.123764
1376.738004	151457.300942	36.128781
1378.119822	151686.978339	36.133799
1379.302079	151923.593287	36.138816
1380.566034	152167.317640	36.143834
1382.443046	152416.253104	36.148852
1383.649607	152648.665679	36.153869
1385.112736	152887.182905	36.158887
1386.748778	153129.063360	36.163904
1388.078727	153376.958947	36.168922
1389.454581	153619.174186	36.173940
1390.871095	153853.285246	36.178957
1392.411795	154090.487899	36.183975
1393.871053	154330.865144	36.188992
1395.227086	154573.633380	36.194010
1396.564765	154806.199273	36.199028
1398.057862	155048.719556	36.204045
1399.452922	155284.972453	36.209063
1400.826558	155526.637512	36.214080
1402.433534	155769.676140	36.219098
1403.931896	156002.196269	36.224116
1405.300880	156248.498554	36.229133
1407.012444	156478.791020	36.234151
1407.904435	156721.932791	36.239168
1409.475725	156955.092683	36.244186
1411.158547	157199.458268	36.249204
1412.406674	157439.995558	36.254221
1413.909751	157669.715899	36.259239
1415.208929	157919.285911	36.264256
1416.565086	158149.221497	36.269274
1418.110761	158395.009848	36.274292
1419.398959	158636.891302	36.279309
1421.013501	158875.472662	36.284327
1422.437516	159116.192182	36.289344
1423.553178	159358.712856	36.294362
1425.328413	159596.370491	36.299380
1426.187296	159845.636400	36.304397
1428.101986	160077.027913	36.309415
1429.310722	160328.983208	36.314432
1430.633654	160572.618757	36.319450
1432.173517	160805.303090	36.324468
1433.882005	161036.235281	36.329485
1434.906687	161267.935517	36.334503
1436.750864	161484.641639	36.339520
1438.193032	161721.610380	36.344538
1439.671457	161950.258564	36.349556
1440.842710	162186.471586	36.354573
1442.085512	162405.357061	36.359591
1443.657845	162631.872743	36.364608
1444.835468	162859.707897	36.369626
1446.376745	163101.008203	36.374644
1447.774443	163337.494663	36.379661
1449.289425	163575.449063	36.384679
1450.444091	163815.250875	36.389696
1452.082477	164059.256470	36.394714
1453.593707	164297.036297	36.399732
1454.547995	164551.320473	36.404749
1456.280683	164790.273539	36.409767
1457.869674	165030.240262	36.414784
1459.005028	165284.232237	36.419802
1460.515437	165525.927035	36.424820
1462.232404	165786.533601	36.429837
1463.740150	166031.455524	36.434855
1465.507601	166281.606774	36.439872
1466.204480	166538.719217	36.444890
1467.942135	166792.089235	36.449908
1469.225001	167055.282480	36.454925
1470.824260	167311.989903	36.459943
1472.187193	167563.694594	36.464960
1473.710225	167826.459531	36.469978
1475.222577	168089.074748	36.474996
1476.723720	168364.656333	36.480013
1478.229013	168616.456740	36.485031
1479.669869	168877.841727	36.490048
1481.009952	169143.941375	36.495066
1482.795589	169416.219282	36.500084
1484.243539	169688.906580	36.505101
1485.513673	169952.823501	36.510119
1487.161226	170218.777355	36.515136
1488.732377	170491.105509	36.520154
1490.388978	170748.501810	36.525172
1491.676019	171025.650614	36.530189
1493.382739	171284.958230	36.535207
1495.168858	171558.247020	36.540224
1496.731528	171833.895429	36.545242
1498.202606	172089.420695	36.550260
1499.490591	172360.923770	36.555277
1501.020714	172623.768139	36.560295
1503.203753	172890.879248	36.565312
1504.343458	173149.266091	36.570330
1506.074469	173414.087943	36.575348
1507.534187	173682.153021	36.580365
1508.905822	173936.417424	36.585383
1510.509107	174215.521749	36.590400
1511.561845	174479.920004	36.595418
1513.623977	174739.653330	36.600436
1515.204660	175011.487962	36.605453
1516.709670	175270.980039	36.610471
1518.445703	175542.373092	36.615488
1519.483695	175823.006330	36.620506
1521.304595	176074.654788	36.625524
1522.902030	176333.373854	36.630541
1524.188500	176599.659823	36.635559
1525.819084	176849.435651	36.640576
1527.324205	177124.400165	36.645594
1528.923294	177391.553996	36.650612
1530.467439	177664.355408	36.655629
1532.025679	177923.644213	36.660647
1533.574661	178177.779616	36.665664
1534.886877	178426.771778	36.670682
1536.567329	178675.681622	36.675700
1538.215528	178925.359144	36.680717
1539.458453	179171.672144	36.685735
1540.719642	179412.928856	36.690752
1542.077115	179666.742978	36.695770
1543.944019	179919.487579	36.700788
1545.099044	180182.681197	36.705805
1546.695250	180435.672793	36.710823
1548.093248	180692.124832	36.715840
1549.293089	180959.682124	36.720858
1551.171146	181224.314863	36.725876
1552.712427	181497.636431	36.730893
1554.121447	181767.906317	36.735911
1556.111361	182033.438183	36.740928
1557.431918	182307.025239	36.745946
1558.802697	182575.855718	36.750964
1560.024038	182863.479830	36.755981
1561.915598	183134.516234	36.760999
1563.101867	183415.188271	36.766016
1564.725337	183704.047274	36.771034
1566.126134	183977.169327	36.776052
1567.704460	184273.199524	36.781069
1569.551263	184559.359193	36.786087
1571.280851	184849.424073	36.791104
1572.277090	185210.772816	36.796122
1574.316808	185500.791022	36.801140
1575.679496	185803.310839	36.806157
1577.321102	186097.075922	36.811175
1579.066737	186387.955421	36.816192
1580.462359	186676.833149	36.821210
1582.290179	186973.644877	36.826228
1583.413784	187268.738873	36.831245
1585.236611	187568.702584	36.836263
1587.208676	187873.215723	36.841280
1588.931017	188165.195889	36.846298
1590.648728	188463.883123	36.851316
1592.189317	188770.752265	36.856333
1593.958452	189059.323869	36.861351
1595.346528	189354.051868	36.866368
1597.047953	189659.577454	36.871386
1598.761313	189949.023652	36.876404
1600.379168	190243.311574	36.881421
1602.047646	190541.122964	36.886439
1603.686928	190840.031895	36.891456
1605.386146	191135.909545	36.896474
1607.146694	191431.575124	36.901492
1608.683030	191734.312482	36.906509
1610.018766	192019.733340	36.911527
1611.686087	192322.629460	36.916544
1613.152956	192626.014906	36.921562
1614.906268	192917.773477	36.926580
1616.484344	193225.537312	36.931597
1618.060612	193528.755402	36.936615
1620.052503	193829.699273	36.941632
1621.519422	194125.366373	36.946650
1623.560612	194426.507116	36.951668
1624.859565	194722.786070	36.956685
1626.316463	195025.645286	36.961703
1627.868788	195316.145216	36.966720
1629.581726	195628.592802	36.971738
1631.770064	195925.751250	36.976756
1633.586285	196221.393679	36.981773
1634.950791	196521.222469	36.986791
1636.889918	196818.574217	36.991808
1638.449850	197114.309417	36.996826
1640.028068	197396.350856	37.001844
1641.692734	197676.677394	37.006861
1643.032365	197954.388145	37.011879
1644.646578	198232.208851	37.016896
1646.205349	198511.435847	37.021914
1647.821088	198787.123574	37.026932
1649.724615	199071.454225	37.031949
1650.666789	199353.929085	37.036967
1653.057297	199621.495411	37.041984
1654.298292	199908.242843	37.047002
1655.919283	200194.702699	37.052020
1657.546052	200489.900504	37.057037
1659.110416	200767.657277	37.062055
1660.878804	201054.324182	37.067072
1662.036194	201353.178692	37.072090
1663.760249	201656.136433	37.077108
1665.407852	201950.342842	37.082125
1666.491963	202253.528784	37.087143
1668.376943	202554.227481	37.092160
1669.748693	202875.481437	37.097178
1671.643280	203179.024752	37.102196
1673.648981	203496.675031	37.107213
1674.897726	203809.617802	37.112231
1676.963102	204124.414701	37.117248
1678.148247	204443.439705	37.122266
1679.742477	204764.890681	37.127284
1681.521128	205087.075400	37.132301
1683.245165	205414.171932	37.137319
1685.152963	205731.688735	37.142336
1686.810653	206067.789309	37.147354
1688.385512	206380.278604	37.152372
1690.199327	206712.088055	37.157389
1691.944097	207041.012863	37.162407
1694.063569	207368.329927	37.167424
1695.725662	207696.658954	37.172442
1697.255192	208022.773711	37.177460
1699.193007	208348.698008	37.182477
1700.641835	208684.911368	37.187495
1702.374494	209011.529141	37.192512
1704.095282	209342.950420	37.197530
1706.089549	209680.756374	37.202548
1708.267509	210000.116578	37.207565
1709.617518	210334.010455	37.212583
1711.206723	210669.112076	37.217600
1713.427072	210998.272536	37.222618
1715.179866	211319.377427	37.227636
1717.095768	211639.923673	37.232653
1718.684723	211976.093794	37.237671
1720.536994	212292.865560	37.242688
1722.125012	212635.717679	37.247706
1724.105393	212963.749259	37.252724
1725.421698	213288.963665	37.257741
1727.292807	213619.527945	37.262759
1728.828846	213941.812562	37.267776
1730.853858	214270.448087	37.272794
1732.343542	214598.380160	37.277812
1734.463530	214929.516367	37.282829
1735.524287	215265.645326	37.287847
1737.254690	215590.568311	37.292864
1739.683945	215918.379836	37.297882
1741.526950	216248.087019	37.302900
1743.161286	216580.215060	37.307917
1744.705260	216917.107999	37.312935
1746.936890	217238.346382	37.317952
1748.682007	217566.418539	37.322970
1750.227059	217900.822379	37.327988
1752.233732	218221.766310	37.333005
1753.499852	218550.295065	37.338023
1755.098270	218875.113828	37.343040
1757.126365	219196.029518	37.348058
1758.665626	219515.853273	37.353076
1760.621011	219824.815357	37.358093
1762.098517	220127.577560	37.363111
1764.092081	220439.633204	37.368128
1765.183617	220758.587588	37.373146
1767.361546	221059.614661	37.378164
1769.053270	221382.717811	37.383181
1770.521610	221709.133139	37.388199
1772.163954	222026.655315	37.393216
1773.851688	222352.655424	37.398234
1775.574854	222679.869461	37.403252
1777.643374	222997.198147	37.408269
1778.779860	223337.307769	37.413287
1780.968151	223676.617754	37.418304
1782.528138	224006.753612	37.423322
1784.230290	224352.008093	37.428340
1786.215549	224691.959653	37.433357
1787.607296	225043.283518	37.438375
1789.811434	225379.161601	37.443392
1791.045341	225720.043685	37.448410
1792.777551	226070.501333	37.453428
1794.897590	226424.988326	37.458445
1796.873138	226785.035984	37.463463
1798.146056	227132.999585	37.468480
1800.375495	227491.889628	37.473498
1801.899553	227847.206391	37.478516
1803.999911	228213.229620	37.483533
1805.701974	228576.774672	37.488551
1807.676682	228930.979073	37.493568
1809.536812	229291.730128	37.498586
1811.192133	229659.118151	37.503604
1813.460407	230027.832739	37.508621
1815.134934	230388.383776	37.513639
1817.119238	230752.087079	37.518656
1818.826851	231116.875064	37.523674
1820.657501	231480.297196	37.528692
1822.894536	231840.098983	37.533709
1824.369269	232219.809512	37.538727
1826.774844	232573.614564	37.543744
1828.409503	232937.777798	37.548762
1830.301450	233296.616513	37.553780
1832.146069	233662.981927	37.558797
1833.959733	234032.603601	37.563815
1835.906248	234393.770122	37.568832
1837.825707	234757.303140	37.573850
1839.562126	235121.855240	37.578868
1841.678375	235482.460809	37.583885
1843.563167	235844.245439	37.588903
1845.725633	236206.595969	37.593920
1847.274442	236570.185336	37.598938
1849.151323	236931.944746	37.603956
1851.071119	237296.389852	37.608973
1852.830764	237661.367699	37.613991
1854.728350	238015.933493	37.619008
1856.534878	238382.605233	37.624026
1858.541260	238754.452991	37.629044
1860.481882	239110.255577	37.634061
1862.369432	239468.225332	37.639079
1864.444467	239829.797995	37.644096
1866.803304	240192.265709	37.649114
1868.525978	240538.701352	37.654132
1870.713931	240891.262154	37.659149
1872.230810	241250.100486	37.664167
1873.834586	241603.513824	37.669184
1875.925920	241962.972548	37.674202
1877.820138	242321.750298	37.679220
1879.671211	242669.306071	37.684237
1881.387106	243025.671957	37.689255
1882.992090	243358.277373	37.694272
1885.098789	243691.972334	37.699290
1886.822296	244033.652484	37.704308
1888.607215	244355.279559	37.709325
1890.605618	244701.945423	37.714343
1891.978488	245036.616826	37.719360
1893.957223	245379.093166	37.724378
1895.814764	245741.249647	37.729396
1897.644370	246075.568440	37.734413
1899.340254	246434.319577	37.739431
1901.441941	246778.425431	37.744448
1903.275856	247133.165444	37.749466
1905.326055	247504.357197	37.754484
1906.715488	247852.763937	37.759501
1908.561268	248215.832023	37.764519
1910.379042	248582.714109	37.769536
1912.646376	248954.122908	37.774554
1914.120736	249308.940278	37.779572
1916.144280	249694.839516	37.784589
1917.850927	250066.536829	37.789607
1919.954333	250429.661513	37.794624
1921.714151	250822.026110	37.799642
1923.220732	251204.522589	37.804660
1925.555300	251591.181512	37.809677
1927.536624	251984.499228	37.814695
1929.503849	252375.404966	37.819712
1931.490250	252746.569540	37.824730
1933.408434	253151.020051	37.829748
1935.722589	253539.480684	37.834765
1937.572593	253929.689398	37.839783
1939.574442	254318.069781	37.844800
1941.415039	254714.221745	37.849818
1943.361226	255118.154259	37.854836
1945.793139	255502.374421	37.859853
1947.634083	255895.373157	37.864871
1949.675652	256285.291211	37.869888
1951.623801	256679.871113	37.874906
1953.314600	257083.101003	37.879924
1955.699477	257467.525993	37.884941
1957.493317	257862.964631	37.889959
1959.770221	258269.553548	37.894976
1962.072101	258647.840930	37.899994
1963.766511	259046.212416	37.905012
1965.860493	259443.529452	37.910029
1968.030691	259835.727766	37.915047
1969.990305	260226.357509	37.920064
1972.429308	260607.055660	37.925082
1974.274404	261002.247347	37.930100
1975.985134	261394.994887	37.935117
1978.163272	261786.677333	37.940135
1979.940315	262173.849189	37.945152
1982.537707	262567.571473	37.950170
1983.924209	262946.419795	37.955188
1986.122901	263344.265599	37.960205
1988.388366	263723.507055	37.965223
1990.300588	264119.540627	37.970240
1992.224822	264504.979318	37.975258
1994.193366	264893.406755	37.980276
1996.378950	265275.829979	37.985293
1998.393380	265665.441069	37.990311
1999.948711	266048.544169	37.995328
2002.088657	266435.999126	38.000346
2003.713523	266841.210664	38.005364
2005.367178	267222.134954	38.010381
2007.747501	267622.246927	38.015399
2009.929918	268016.089398	38.020416
2012.346027	268399.175598	38.025434
2013.823659	268800.566791	38.030452
2015.716534	269170.626250	38.035469
2017.620689	269546.676396	38.040487
2019.458703	269914.227065	38.045504
2021.414527	270297.606040	38.050522
2023.310588	270671.392422	38.055540
2024.976537	271060.070831	38.060557
2027.222411	271439.310547	38.065575
2029.053636	271829.280395	38.070592
2031.166310	272217.121901	38.075610
2032.957973	272613.291361	38.080628
2035.237958	273000.112694	38.085645
2037.178988	273404.356776	38.090663
2038.986692	273807.451540	38.095680
2041.059324	274205.626766	38.100698
2042.985567	274607.607076	38.105716
2045.089463	275020.249517	38.110733
2046.959714	275430.183642	38.115751
2048.908666	275852.979226	38.120768
2050.879072	276257.966643	38.125786
2052.875219	276686.261390	38.130804
2055.571576	277098.038632	38.135821
2057.583463	277532.980010	38.140839
2059.442826	277948.540702	38.145856
2061.543285	278370.181715	38.150874
2063.689100	278813.500797	38.155892
2066.129264	279241.534233	38.160909
2068.091769	279655.368051	38.165927
2069.966519	280082.291610	38.170944
2072.180187	280506.772602	38.175962
2074.202700	280944.181443	38.180980
2076.738731	281367.870593	38.185997
2078.731571	281806.827959	38.191015
2080.832188	282238.122201	38.196032
2082.861066	282661.273647	38.201050
2084.957011	283100.283136	38.206068
2087.165119	283525.889954	38.211085
2089.269784	283959.229956	38.216103
2091.203864	284400.618200	38.221120
2093.565707	284832.211158	38.226138
2095.439603	285277.386753	38.231156
2097.956222	285702.043127	38.236173
2100.153694	286144.496163	38.241191
2101.947820	286581.245308	38.246208
2104.342680	287024.017128	38.251226
2105.897019	287458.131827	38.256244
2108.235834	287892.095531	38.261261
2110.544704	288344.952465	38.266279
2112.671062	288780.847843	38.271296
2115.062670	289226.093569	38.276314
2116.858424	289664.218310	38.281332
2119.163975	290106.652909	38.286349
2121.598462	290544.976300	38.291367
2123.593620	290991.134888	38.296384
2125.730429	291425.029900	38.301402
2127.711327	291878.623725	38.306420
2129.969640	292312.950482	38.311437
2132.445302	292757.827732	38.316455
2134.596761	293198.512341	38.321472
2136.625058	293627.102168	38.326490
2138.850694	294068.225779	38.331508
2140.485402	294509.083109	38.336525
2143.019303	294946.267394	38.341543
2145.097104	295398.372212	38.346560
2147.198509	295824.928893	38.351578
2148.992024	296271.663604	38.356596
2151.318655	296712.979912	38.361613
2153.587698	297158.440064	38.366631
2155.534680	297592.319482	38.371648
2157.818006	298001.973921	38.376666
2160.069679	298430.467800	38.381684
2161.912012	298845.973380	38.386701
2164.457883	299267.179415	38.391719
2166.019363	299682.062582	38.396736
2168.190225	300096.872660	38.401754
2170.377542	300523.786354	38.406772
2172.307536	300961.323015	38.411789
2174.850584	301379.822209	38.416807
2176.927553	301813.597181	38.421824
2178.887944	302240.634274	38.426842
2180.820693	302687.980607	38.431860
2182.845397	303122.235360	38.436877
2185.095261	303565.792975	38.441895
2187.301617	304014.278268	38.446912
2189.365012	304463.391271	38.451930
2191.424889	304917.857005	38.456948
2193.550504	305371.470743	38.461965
2196.195290	305823.171576	38.466983
2198.034630	306293.854448	38.472000
2200.512557	306738.262695	38.477018
2202.549081	307212.028269	38.482036
2204.697143	307672.902721	38.487053
2207.260878	308141.322667	38.492071
2209.266217	308607.566466	38.497088
2211.562416	309070.689067	38.502106
2213.685707	309554.952126	38.507124
2215.767381	310011.804567	38.512141
2218.277579	310496.378370	38.517159
2221.063483	310973.594335	38.522176
2222.827450	311446.802899	38.527194
2225.141511	311924.717630	38.532212
2227.469872	312399.173522	38.537229
2229.784140	312877.662260	38.542247
2231.869048	313356.105816	38.547264
2234.451019	313830.786610	38.552282
2236.607808	314310.452627	38.557300
2238.527061	314790.404569	38.562317
2241.169770	315271.811765	38.567335
2243.331176	315759.278488	38.572352
2245.736456	316245.153704	38.577370
2248.041775	316723.857293	38.582388
2250.453078	317210.786940	38.587405
2252.614765	317689.705614	38.592423
2254.813096	318181.454232	38.597440
2257.647493	318655.816129	38.602458
2259.291849	319139.773777	38.607476
2262.080991	319622.176620	38.612493
2264.474308	320106.970593	38.617511
2266.551994	320590.742685	38.622528
2268.789405	321069.130077	38.627546
2271.202625	321559.715451	38.632564
2273.423003	322038.982700	38.637581
2275.572066	322530.739980	38.642599
2277.597933	323019.364337	38.647616
2280.421567	323499.535474	38.652634
2282.671091	323994.279279	38.657652
2284.895559	324463.926713	38.662669
2287.163363	324946.882913	38.667687
2289.852863	325438.241976	38.672704
2292.527632	325919.778221	38.677722
2294.619538	326399.573108	38.682740
2296.463557	326890.260255	38.687757
2298.741733	327358.394194	38.692775
2301.169871	327841.595136	38.697792
2303.505826	328330.995150	38.702810
2305.840900	328804.481792	38.707828
2308.184953	329277.377808	38.712845
2310.631492	329727.063781	38.717863
2312.615334	330190.668877	38.722880
2314.697107	330643.623279	38.727898
2316.848327	331106.125710	38.732916
2319.063767	331561.813659	38.737933
2321.450120	332025.739623	38.742951
2323.600069	332487.489878	38.747968
2325.768828	332955.801888	38.752986
2327.910779	333433.219288	38.758004
2329.970902	333909.070655	38.763021
2332.270290	334387.998697	38.768039
2334.666464	334884.560673	38.773056
2336.582499	335356.255978	38.778074
2338.530468	335852.393135	38.783092
2341.053758	336351.046273	38.788109
2343.547515	336853.451315	38.793127
2345.646171	337360.781316	38.798144
2348.175122	337866.920875	38.803162
2350.520230	338377.343302	38.808180
2352.818602	338897.353354	38.813197
2355.353674	339403.140609	38.818215
2357.706837	339924.040236	38.823232
2360.064250	340445.590985	38.828250
2362.603878	340957.619980	38.833268
2364.820024	341485.315150	38.838285
2367.311025	342002.992233	38.843303
2369.547654	342536.146444	38.848320
2371.967315	343058.155756	38.853338
2374.730347	343586.342153	38.858356
2376.751373	344127.646246	38.863373
2379.393077	344645.031907	38.868391
2381.756598	345179.621500	38.873408
2383.932870	345720.039153	38.878426
2386.640747	346255.039712	38.883444
2388.680656	346799.975192	38.888461
2391.398216	347330.037613	38.893479
2394.013818	347875.829076	38.898496
2396.180034	348417.624751	38.903514
2398.812447	348952.010594	38.908532
2401.049438	349492.611124	38.913549
2403.978029	350042.476129	38.918567
2406.057823	350582.500029	38.923584
2408.320078	351129.027935	38.928602
2411.010929	351675.023176	38.933620
2413.566856	352227.774394	38.938637
2416.354930	352763.011206	38.943655
2418.059493	353322.696742	38.948672
2421.208245	353859.608047	38.953690
2423.731029	354406.216618	38.958708
2426.112918	354953.319419	38.963725
2428.447633	355490.076720	38.968743
2431.003777	356045.499087	38.973760
2432.981613	356591.394183	38.978778
2436.173468	357124.009178	38.983796
2438.335013	357668.842497	38.988813
2441.026569	358220.402140	38.993831
2443.128955	358752.069281	38.998848
2445.884149	359303.776818	39.003866
2448.324031	359845.460597	39.008884
2450.648692	360386.468304	39.013901
2453.292186	360939.278703	39.018919
2455.502826	361482.464309	39.023936
2457.779647	362021.498295	39.028954
2460.583915	362569.032090	39.033972
2463.134320	363116.950287	39.038989
2465.439369	363648.220018	39.044007
2468.184670	364197.025352	39.049024
2470.727294	364735.613302	39.054042
2473.062925	365243.153061	39.059060
2475.296453	365767.045912	39.064077
2477.866347	366275.544640	39.069095
2480.126381	366787.250571	39.074112
2482.475485	367307.929598	39.079130
2485.322590	367825.125578	39.084148
2487.812124	368337.882852	39.089165
2490.042990	368857.082312	39.094183
2492.274811	369383.088394	39.099200
2494.204631	369909.511976	39.104218
2496.803224	370440.838099	39.109236
2499.422464	370979.448233	39.114253
2501.882363	371518.959688	39.119271
2504.033876	372065.577911	39.124288
2506.498212	372616.266246	39.129306
2508.986179	373162.202048	39.134324
2511.193768	373708.576213	39.139341
2514.026339	374273.944261	39.144359
2516.576749	374834.657837	39.149376
2518.905155	375405.502773	39.154394
2521.712952	375958.299317	39.159412
2523.958313	376532.528067	39.164429
2526.313301	377104.979452	39.169447
2529.179836	377685.191402	39.174464
2531.677021	378263.573967	39.179482
2533.970039	378840.633327	39.184500
2536.621686	379431.606190	39.189517
2539.311144	380005.943711	39.194535
2541.987519	380590.934183	39.199552
2544.556307	381187.604758	39.204570
2547.368080	381772.243597	39.209588
2549.828349	382366.067350	39.214605
2552.156726	382946.525607	39.219623
2554.803181	383534.569489	39.224640
2557.470736	384132.473512	39.229658
2560.269953	384724.442237	39.234676
2562.477832	385320.921422	39.239693
2565.348870	385930.552454	39.244711
2568.269208	386531.779110	39.249728
2570.553974	387125.443404	39.254746
2573.378878	387721.034898	39.259764
2576.099830	388316.679075	39.264781
2578.944616	388916.872652	39.269799
2581.717197	389519.468380	39.274816
2584.386307	390107.279026	39.279834
2586.993561	390703.643057	39.284852
2589.531343	391295.192974	39.289869
2592.051531	391886.478131	39.294887
2594.815556	392479.736133	39.299904
2597.242994	393089.437248	39.304922
2600.031393	393671.371118	39.309940
2602.865485	394273.788999	39.314957
2605.794382	394864.329741	39.319975
2608.251190	395459.789974	39.324992
2610.979177	396049.370859	39.330010
2613.618242	396635.761609	39.335028
2616.451647	397231.320964	39.340045
2619.060781	397824.875429	39.345063
2621.942391	398406.526871	39.350080
2624.338402	398997.503270	39.355098
2626.868047	399571.739578	39.360116
2629.054759	400157.657366	39.365133
2632.117872	400749.294743	39.370151
2634.725195	401329.599863	39.375168
2636.965966	401928.067364	39.380186
2640.024062	402512.675459	39.385204
2642.173538	403108.393294	39.390221
2644.707581	403685.613446	39.395239
2647.747242	404248.417629	39.400256
2650.559387	404815.646213	39.405274
2653.053063	405373.295193	39.410292
2655.490317	405939.845586	39.415309
2657.935854	406508.100869	39.420327
2660.613968	407066.336690	39.425344
2662.846663	407639.150619	39.430362
2665.548709	408205.146613	39.435380
2668.119266	408784.557218	39.440397
2670.653551	409362.035583	39.445415
2673.544259	409945.362709	39.450432
2676.073520	410531.311129	39.455450
2678.731004	411110.545512	39.460468
2680.990095	411696.049538	39.465485
2683.491391	412295.665115	39.470503
2686.532534	412897.557302	39.475520
2688.909662	413495.995415	39.480538
2691.800002	414097.118815	39.485556
2694.310839	414720.440663	39.490573
2696.896391	415332.250296	39.495591
2699.903094	415939.322967	39.500608
2701.976523	416562.912138	39.505626
2704.837761	417187.118378	39.510644
2707.408648	417819.899037	39.515661
2709.963144	418455.191955	39.520679
2713.425150	419084.153633	39.525696
2715.908971	419717.042241	39.530714
2718.858515	420346.298778	39.535732
2721.176672	420994.193873	39.540749
2724.293707	421629.402905	39.545767
2727.169992	422276.260185	39.550784
2729.588622	422922.865242	39.555802
2732.183926	423570.837975	39.560820
2735.219439	424221.198753	39.565837
2738.464932	424872.264247	39.570855
2741.340807	425512.597720	39.575872
2743.822910	426174.863383	39.580890
2746.535722	426814.574265	39.585908
2749.287721	427467.048545	39.590925
2752.571230	428119.772239	39.595943
2755.803902	428768.489029	39.600960
2758.301312	429418.765484	39.605978
2761.022362	430064.992400	39.610996
2763.839412	430712.699458	39.616013
2766.471593	431370.320536	39.621031
2769.835465	432008.649864	39.626048
2772.059339	432666.948215	39.631066
2774.943203	433311.475782	39.636084
2778.050736	433973.634704	39.641101
2781.095415	434634.113123	39.646119
2784.080627	435281.793351	39.651136
2786.979757	435926.534380	39.656154
2789.822077	436566.159088	39.661172
2792.913772	437206.733917	39.666189
2795.367525	437854.309031	39.671207
2798.126179	438484.585503	39.676224
2800.669505	439142.257993	39.681242
2803.878525	439784.495567	39.686260
2806.811128	440425.390392	39.691277
2809.491131	441059.786024	39.696295
2812.488239	441703.708532	39.701312
2815.110329	442358.679486	39.706330
2818.198325	442994.511329	39.711348
2820.614960	443629.416101	39.716365
2823.420699	444269.541609	39.721383
2826.383616	444912.044603	39.726400
2828.840476	445550.008240	39.731418
2831.768963	446184.340619	39.736436
2834.706509	446807.589607	39.741453
2837.263084	447414.666260	39.746471
2840.558006	448022.617087	39.751488
2842.911203	448646.197231	39.756506
2845.884489	449258.196472	39.761524
2848.819458	449861.899964	39.766541
2851.262114	450479.444311	39.771559
2854.095939	451099.935542	39.776576
2856.509968	451720.218378	39.781594
2859.409901	452355.297033	39.786612
2862.034996	452981.359190	39.791629
2864.518652	453617.921679	39.796647
2867.759970	454254.241732	39.801664
2870.396569	454914.812719	39.806682
2873.110866	455562.374053	39.811700
2875.881227	456225.448962	39.816717
2878.488497	456875.502039	39.821735
2881.777716	457550.155090	39.826752
2884.448164	458221.547636	39.831770
2887.188464	458886.090053	39.836788
2890.330850	459555.338151	39.841805
2892.614139	460235.897373	39.846823
2895.645388	460920.198096	39.851840
2898.581530	461620.380935	39.856858
2901.377582	462305.772875	39.861876
2904.229911	463005.407140	39.866893
2907.093634	463709.248729	39.871911
2909.925961	464407.415322	39.876928
2913.143329	465124.511924	39.881946
2915.857829	465838.074745	39.886964
2919.264366	466552.860864	39.891981
2922.080782	467271.088207	39.896999
2925.336294	467980.035693	39.902016
2928.076603	468702.248127	39.907034
2930.953130	469412.504793	39.912052
2933.766164	470137.870804	39.917069
2936.896790	470870.467612	39.922087
2939.965395	471578.784875	39.927104
2942.715463	472317.528593	39.932122
2945.898334	473042.304281	39.937140
2949.232641	473767.275967	39.942157
2952.177401	474503.217173	39.947175
2955.379773	475220.581128	39.952192
2958.537794	475954.708327	39.957210
2961.742934	476694.541579	39.962228
2964.402696	477403.624755	39.967245
2967.335779	478137.384229	39.972263
2970.384428	478844.124310	39.977280
2973.310516	479577.314097	39.982298
2976.276734	480310.211505	39.987316
2979.597573	481042.414501	39.992333
2982.258568	481777.357502	39.997351
2985.747055	482501.805655	40.002368
2988.623596	483229.540911	40.007386
2991.660960	483956.108351	40.012404
2994.741334	484687.925674	40.017421
2997.635918	485418.074661	40.022439
3001.161376	486144.714736	40.027456
3003.873712	486870.540715	40.032474
3006.911964	487597.591153	40.037492
3010.199259	488313.787645	40.042509
3012.708112	489045.687855	40.047527
3015.692423	489769.771708	40.052544
3018.824741	490504.475868	40.057562
3021.720747	491233.439499	40.062580
3024.859848	491957.394190	40.067597
3027.666259	492683.380415	40.072615
3030.764015	493403.393909	40.077632
3033.931336	494107.701002	40.082650
3037.001797	494806.098502	40.087668
3040.025025	495484.430611	40.092685
3042.923847	496171.109058	40.097703
3045.766345	496867.179236	40.102720
3048.507504	497565.397164	40.107738
3051.239578	498260.160055	40.112756
3054.142985	498952.799272	40.117773
3056.927059	499680.962397	40.122791
3059.942741	500389.825055	40.127808
3062.452452	501117.103505	40.132826
3065.893357	501839.066219	40.137844
3068.902432	502572.736273	40.142861
3071.940850	503315.573773	40.147879
3075.280373	504053.041981	40.152896
3078.184253	504797.635372	40.157914
3081.121088	505545.908247	40.162932
3084.486744	506286.175465	40.167949
3087.261542	507039.929653	40.172967
3090.156199	507798.152793	40.177984
3093.096352	508555.825074	40.183002
3096.477610	509330.490760	40.188020
3099.786707	510097.579938	40.193037
3102.587797	510865.259820	40.198055
3105.600714	511639.402748	40.203072
3108.836373	512419.050262	40.208090
3112.380448	513204.891956	40.213108
3115.320870	513985.352512	40.218125
3118.194206	514768.897046	40.223143
3121.766484	515556.913552	40.228160
3124.912947	516354.805870	40.233178
3127.867989	517151.625860	40.238196
3131.083530	517948.861347	40.243213
3134.286659	518758.870683	40.248231
3137.374125	519544.872905	40.253248
3140.441656	520343.046543	40.258266
3143.626564	521157.690201	40.263284
3147.012979	521963.056024	40.268301
3150.063996	522768.526472	40.273319
3153.478594	523570.776043	40.278336
3156.723196	524392.500164	40.283354
3160.117242	525206.563219	40.288372
3163.967183	526006.638328	40.293389
3167.071606	526809.293555	40.298407
3170.361533	527603.431363	40.303424
3173.841953	528417.333351	40.308442
3176.923642	529217.132706	40.313460
3180.379816	530006.779333	40.318477
3183.387080	530807.045509	40.323495
3186.589330	531585.938557	40.328512
3189.943414	532388.061971	40.333530
3193.373538	533192.935780	40.338548
3196.618119	533985.737751	40.343565
3199.547849	534790.389203	40.348583
3203.171358	535573.042648	40.353600
3206.419102	536373.779631	40.358618
3209.424154	537161.101312	40.363636
3212.954713	537957.076373	40.368653
3215.900809	538752.139266	40.373671
3219.217809	539538.260963	40.378688
3222.318046	540332.096288	40.383706
3225.665438	541121.125758	40.388724
3229.020472	541916.728216	40.393741
3232.163319	542715.223578	40.398759
3235.244774	543502.739732	40.403776
3238.546830	544293.382542	40.408794
3241.868216	545088.085745	40.413812
3245.128020	545870.457511	40.418829
3248.828986	546628.683833	40.423847
3251.171850	547363.852855	40.428864
3254.392994	548111.730427	40.433882
3257.190687	548878.084442	40.438900
3261.015358	549631.091042	40.443917
3263.680192	550379.067570	40.448935
3266.677989	551137.626455	40.453952
3269.640907	551914.745078	40.458970
3273.123689	552685.164821	40.463988
3276.061603	553452.512443	40.469005
3279.262170	554237.215265	40.474023
3282.347082	555018.576676	40.479040
3285.268915	555819.260164	40.484058
3288.316107	556623.228524	40.489076
3291.520268	557424.662534	40.494093
3294.792020	558244.072634	40.499111
3298.172056	559063.559618	40.504128
3301.851863	559890.609238	40.509146
3304.765986	560726.488565	40.514164
3308.191531	561561.427092	40.519181
3311.288937	562379.675953	40.524199
3314.766773	563224.206500	40.529216
3317.797298	564060.782010	40.534234
3321.205430	564921.479282	40.539252
3324.748220	565763.461845	40.544269
3327.909437	566622.519184	40.549287
3331.155251	567477.744031	40.554304
3334.613256	568341.834756	40.559322
3337.920099	569209.188567	40.564340
3341.394818	570072.295452	40.569357
3345.193730	570942.094471	40.574375
3348.424398	571811.715830	40.579392
3351.919255	572691.489803	40.584410
3355.294167	573557.301419	40.589428
3359.089066	574434.841302	40.594445
3362.193312	575303.814286	40.599463
3365.491092	576196.406536	40.604480
3369.259997	577070.692978	40.609498
3372.421690	577944.305732	40.614516
3375.958544	578827.145860	40.619533
3379.189237	579714.365590	40.624551
3382.965679	580595.027235	40.629568
3386.462491	581473.112043	40.634586
3389.777005	582360.106888	40.639604
3393.627614	583237.295950	40.644621
3397.031510	584121.534746	40.649639
3400.217480	584999.786892	40.654656
3404.148461	585882.851168	40.659674
3407.017827	586762.910716	40.664692
3410.892754	587650.489260	40.669709
3414.274439	588532.824519	40.674727
3417.769024	589409.622937	40.679744
3421.205135	590286.908958	40.684762
3424.720367	591167.059168	40.689780
3428.259991	592049.032009	40.694797
3431.607692	592933.859822	40.699815
3434.737168	593816.700251	40.704832
3438.427011	594696.233075	40.709850
3441.631027	595578.166471	40.714868
3445.492053	596448.037604	40.719885
3449.152446	597351.226986	40.724903
3452.159049	598230.672875	40.729920
3455.807609	599102.105979	40.734938
3459.259403	599981.685206	40.739956
3462.484716	600844.402517	40.744973
3466.093722	601726.605917	40.749991
3469.442211	602613.017879	40.755008
3473.240194	603484.879929	40.760013
3476.346789	604306.704739	40.765018
3479.751749	605087.744610	40.770023
3483.060020	605816.214531	40.775028
3485.889998	606488.283516	40.780032
3489.120114	607093.171267	40.785037
3491.824256	607658.443069	40.790042
3494.248731	608158.310071	40.795047
3497.008580	608613.190274	40.800052
3499.466413	609022.039080	40.805056
3501.861607	609361.621136	40.810061
3503.544282	609672.399841	40.815066
3505.424822	609926.082897	40.820071
3507.847533	610135.721716	40.825076
3509.184795	610282.172323	40.830080
3510.645623	610413.650816	40.835085
3511.947470	610513.151336	40.840090
3513.490994	610570.911895	40.845095
3514.651634	610588.930897	40.850100
3515.912317	610577.933394	40.855104
3517.144490	610528.839074	40.860109
3517.937107	610462.562533	40.865114
3518.570157	610373.309375	40.870119
3519.677223	610255.029585	40.875124
3520.065110	610113.259090	40.880128
3520.692331	609957.997991	40.885133
3521.173679	609794.256425	40.890138
3521.604149	609599.616331	40.895143
3522.127027	609396.456839	40.900148
3522.567494	609179.203835	40.905152
3522.966675	608938.048126	40.910157
3523.267070	608704.203732	40.915162
3523.012485	608453.586743	40.920167
3523.587581	608199.232963	40.925172
3523.214211	607930.466931	40.930176
3523.879432	607663.432086	40.935181
3523.659817	607390.876679	40.940186
3523.978466	607101.323637	40.945191
3523.839305	606822.338178	40.950196
3523.745878	606522.579159	40.955200
3524.092288	606228.995489	40.960205
3524.073430	605931.958855	40.965210
3523.824939	605616.790224	40.970215
3523.856667	605318.077135	40.975220
3523.461608	605022.874092	40.980224
3523.554970	604713.477771	40.985229
3523.072909	604413.367955	40.990234
3522.752350	604113.174149	40.995239
3523.058707	603810.672116	41.000244
3522.819783	603507.796173	41.005248
3522.379811	603201.190006	41.010253
3522.290597	602913.084363	41.015258
3522.567691	602605.397770	41.020263
3522.013377	602309.291605	41.025268
3521.841834	602013.917865	41.030272
3521.969550	601707.379067	41.035277
3521.776733	601417.897019	41.040282
3521.585932	601119.147851	41.045287
3521.368420	600838.912374	41.050292
3521.010204	600538.120760	41.055296
3521.086127	600242.658203	41.060301
3520.595066	599963.192797	41.065306
3520.343961	599680.328783	41.070311
3520.300480	599395.022008	41.075316
3520.203376	599115.722702	41.080320
3520.196939	598833.998994	41.085325
3519.668891	598563.062046	41.090330
3519.394139	598282.116390	41.095335
3519.372452	598007.331399	41.100340
3518.905864	597741.770424	41.105344
3519.014864	597468.302667	41.110349
3518.428277	597208.854940	41.115354
3518.357194	596952.574623	41.120359
3518.086285	596695.368028	41.125364
3517.547862	596443.454316	41.130368
3517.604283	596196.598915	41.135373
3517.373165	595942.722553	41.140378
3517.230538	595695.135505	41.145383
3516.760364	595451.599834	41.150388
3516.554210	595220.235721	41.155392
3516.405010	594977.940969	41.160397
3515.931545	594757.575340	41.165402
3516.288911	594526.708970	41.170407
3515.805487	594295.718633	41.175412
3515.369914	594078.988853	41.180416
3515.545138	593854.596817	41.185421
3515.411981	593645.673806	41.190426
3515.054470	593422.057113	41.195431
3515.045888	593212.705482	41.200436
3514.537796	592998.769847	41.205440
3515.134623	592782.052682	41.210445
3514.519278	592571.430999	41.215450
3514.071100	592365.086682	41.220455
3514.087406	592160.068291	41.225460
3513.724914	591969.982151	41.230464
3514.123123	591774.363827	41.235469
3513.535364	591578.395146	41.240474
3513.656011	591378.505039	41.245479
3513.400402	591183.228624	41.250484
3513.005532	590997.688914	41.255488
3512.680297	590807.275791	41.260493
3512.705867	590636.091797	41.265498
3512.197555	590457.523976	41.270503
3512.240860	590279.668538	41.275508
3511.998069	590111.123279	41.280512
3511.989044	589935.825417	41.285517
3512.144299	589764.457005	41.290522
3511.497523	589588.802294	41.295527
3511.481887	589426.724066	41.300532
3510.930214	589269.436914	41.305536
3511.344046	589102.777395	41.310541
3510.659220	588950.867555	41.315546
3511.018018	588790.424817	41.320551
3510.753329	588645.610096	41.325556
3510.613499	588488.447629	41.330560
3510.679780	588338.816910	41.335565
3510.264638	588192.967398	41.340570
3510.236642	588047.756927	41.345575
3510.223827	587905.348277	41.350580
3509.685230	587766.427450	41.355584
3510.011055	587616.946642	41.360589
3509.614514	587484.514419	41.365594
3509.623629	587348.860099	41.370599
3509.410014	587206.624015	41.375604
3509.561828	587084.023523	41.380608
3509.492435	586949.178306	41.385613
3509.080379	586825.961458	41.390618
3508.825458	586691.292392	41.395623
3508.462263	586554.132795	41.400628
3508.696104	586436.774354	41.405632
3508.756116	586317.136446	41.410637
3508.581585	586198.836945	41.415642
3508.656516	586081.649877	41.420647
3508.217774	585958.577745	41.425652
3508.301917	585847.400948	41.430656
3508.211106	585730.085659	41.435661
3508.336729	585614.489481	41.440666
3507.814290	585493.881080	41.445671
3507.865752	585379.998119	41.450676
3507.464425	585293.801798	41.455680
3507.872775	585172.994227	41.460685
3507.412253	585082.144128	41.465690
3507.560741	584972.301684	41.470695
3507.711287	584862.708434	41.475700
3507.032085	584758.055712	41.480704
3507.277599	584652.254939	41.485709
3507.244974	584557.323628	41.490714
3506.950762	584460.226869	41.495719
3507.249096	584370.956503	41.500724
3507.171840	584265.803970	41.505728
3507.210151	584163.389337	41.510733
3506.800141	584067.510246	41.515738
3506.836364	583977.124727	41.520743
3506.787363	583871.312338	41.525748
3506.291684	583793.189581	41.530752
3506.392930	583701.037129	41.535757
3505.939698	583620.049156	41.540762
3506.051103	583533.758836	41.545767
3505.847515	583454.384895	41.550772
3506.042220	583375.148638	41.555776
3506.114137	583281.443213	41.560781
3506.067856	583213.823677	41.565786
3505.837364	583129.789405	41.570791
3505.768638	583054.702806	41.575796
3505.677462	582978.265634	41.580800
3506.124598	582893.321511	41.585805
3505.683329	582816.336354	41.590810
3505.537042	582737.549881	41.595815
3505.665696	582663.883626	41.600820
3505.522832	582596.576202	41.605824
3505.899316	582521.165699	41.610829
3505.733397	582455.465314	41.615834
3505.880518	582376.279449	41.620839
3505.848293	582303.237556	41.625844
3505.265468	582228.376101	41.630848
3505.879520	582151.672547	41.635853
3505.722027	582077.846570	41.640858
3505.502430	581996.459177	41.645863
3505.139779	581912.336011	41.650868
3504.886813	581852.311126	41.655872
3505.094234	581784.292203	41.660877
3504.990590	581714.466387	41.665882
3504.740198	581657.147487	41.670887
3504.905138	581586.827634	41.675892
3504.910845	581521.696525	41.680896
3504.833976	581458.533366	41.685901
3504.844248	581401.723922	41.690906
3505.097951	581342.369152	41.695911
3505.211071	581274.462117	41.700916
3504.896245	581214.242878	41.705920
3504.770890	581138.099152	41.710925
3504.389735	581084.006717	41.715930
3504.529881	581022.261226	41.720935
3504.767224	580972.935242	41.725940
3504.313989	580898.947062	41.730944
3504.787313	580835.794624	41.735949
3504.565769	580784.483721	41.740954
3504.415053	580723.283455	41.745959
3504.739798	580671.936774	41.750964
3504.355700	580614.131947	41.755968
3504.192738	580550.375353	41.760973
3504.512753	580509.358152	41.765978
3504.615856	580457.994986	41.770983
3504.652051	580400.825355	41.775988
3504.399372	580342.848138	41.780992
3504.305614	580279.430178	41.785997
3504.296746	580229.487503	41.791002
3504.194473	580175.246745	41.796007
3504.194788	580113.919219	41.801012
3504.062382	580064.095402	41.806016
3504.366293	580013.400825	41.811021
3503.754824	579954.825776	41.816026
3503.679371	579913.266448	41.821031
3504.214788	579856.818312	41.826036
3504.017804	579824.454425	41.831040
3504.140694	579768.421356	41.836045
3504.229539	579715.903615	41.841050
3504.109699	579662.766335	41.846055
3504.167924	579606.040496	41.851060
3503.912680	579565.410629	41.856064
3503.910665	579504.380991	41.861069
3504.114577	579475.664363	41.866074
3503.900350	579417.576010	41.871079
3504.267713	579373.488174	41.876084
3503.948346	579321.483723	41.881088
3504.046992	579259.835224	41.886093
3503.900410	579215.676661	41.891098
3503.661293	579173.337767	41.896103
3504.230705	579117.833413	41.901108
3503.850451	579078.525201	41.906112
3504.090676	579033.904250	41.911117
3504.113885	578980.891804	41.916122
3503.889207	578933.233810	41.921127
3504.385549	578878.140892	41.926132
3503.659356	578826.498632	41.931136
3504.092212	578777.082198	41.936141
3504.124023	578728.681116	41.941146
3504.227425	578669.736787	41.946151
3504.243377	578617.275416	41.951156
3503.363741	578582.807951	41.956160
3504.050717	578523.420557	41.961165
3503.205629	578466.980591	41.966170
3503.581995	578426.699204	41.971175
3503.685573	578384.855423	41.976180
3503.292482	578340.681777	41.981184
3503.368420	578294.779573	41.986189
3503.049218	578256.411830	41.991194
3503.134039	578208.451588	41.996199
3503.421364	578185.686896	42.001204
3503.268119	578153.110699	42.006208
3503.447397	578107.342033	42.011213
3503.214918	578063.944651	42.016218
3503.542875	578027.982674	42.021223
3503.323486	577988.946399	42.026228
3503.195194	577941.369410	42.031232
3503.362053	577909.093545	42.036237
3503.756375	577872.167747	42.041242
3503.484198	577838.355343	42.046247
3503.524944	577792.155646	42.051252
3503.025873	577752.259465	42.056256
3503.365736	577716.043846	42.061261
3503.100135	577680.424323	42.066266
3503.309331	577631.539354	42.071271
3503.367139	577591.354919	42.076276
3502.958562	577565.939148	42.081280
3503.258924	577527.572360	42.086285
3502.796703	577489.023713	42.091290
3502.894845	577447.578531	42.096295
3502.997286	577411.499359	42.101300
3502.974495	577384.167045	42.106304
3503.299960	577343.588776	42.111309
3503.030412	577314.990770	42.116314
3502.993609	577279.033255	42.121319
3503.355244	577249.884990	42.126324
3503.307075	577216.587426	42.131328
3503.185796	577180.291693	42.136333
3503.230470	577138.452460	42.141338
3503.109090	577106.720930	42.146343
3503.036051	577064.699189	42.151348
3502.895683	577033.421849	42.156352
3503.491060	576996.662375	42.161357
3503.180467	576961.147914	42.166362
3503.172824	576925.335183	42.171367
3503.376384	576877.250360	42.176372
3502.979956	576850.225953	42.181376
3503.126654	576814.639540	42.186381
3503.110034	576774.965413	42.191386
3502.753009	576745.928188	42.196391
3503.424465	576707.099301	42.201396
3502.981119	576669.196966	42.206400
3503.352080	576627.505463	42.211405
3503.190392	576596.982652	42.216410
3503.196456	576563.423866	42.221415
3503.667992	576529.140118	42.226420
3503.292103	576495.941809	42.231424
3503.401217	576450.879610	42.236429
3503.258224	576405.655994	42.241434
3503.164055	576367.497405	42.246439
3503.364551	576322.922027	42.251444
3502.772225	576293.268304	42.256448
3503.204325	576251.465526	42.261453
3503.229834	576223.520885	42.266458
3502.999427	576176.855297	42.271463
3503.243355	576145.766221	42.276468
3502.967079	576121.028769	42.281472
3503.239211	576071.926520	42.286477
3503.217140	576042.283314	42.291482
3503.144252	576004.320819	42.296487
3503.000542	575965.767302	42.301492
3502.583889	575936.436320	42.306496
3502.984486	575902.663394	42.311501
3502.762262	575875.408748	42.316506
3502.909608	575844.634925	42.321511
3503.339379	575810.104696	42.326516
3502.500576	575782.996379	42.331520
3503.046553	575731.592430	42.336525
3502.865646	575712.457627	42.341530
3503.047991	575671.895701	42.346535
3503.087414	575644.047775	42.351540
3502.716022	575608.839531	42.356544
3502.963070	575576.745091	42.361549
3503.018379	575539.814464	42.366554
3502.784580	575514.768043	42.371559
3502.685514	575472.443422	42.376564
3502.698443	575457.441659	42.381568
3503.036326	575429.546546	42.386573
3502.800342	575393.162638	42.391578
3503.040667	575350.082173	42.396583
3502.717660	575314.965778	42.401588
3502.867242	575291.062927	42.406592
3503.085076	575256.313302	42.411597
3502.666082	575230.793531	42.416602
3503.172615	575199.811296	42.421607
3503.214689	575157.062089	42.426612
3503.010166	575131.057058	42.431616
3502.904874	575098.564831	42.436621
3502.929874	575066.403316	42.441626
3502.881538	575036.059219	42.446631
3503.022556	574999.615104	42.451636
3503.064813	574974.825335	42.456640
3503.234666	574934.814562	42.461645
3503.088654	574903.482010	42.466650
3502.696146	574859.896582	42.471655
3502.910034	574823.440507	42.476660
3502.548030	574780.803213	42.481664
3502.962709	574752.894425	42.486669
3502.785719	574737.269194	42.491674
3503.079492	574705.967683	42.496679
3502.714085	574675.371167	42.501684
3502.760352	574639.944094	42.506688
3503.048046	574611.201923	42.511693
3502.999167	574587.178098	42.516698
3503.069609	574551.395779	42.521703
3503.359844	574507.100216	42.526708
3502.505593	574473.368674	42.531712
3502.716246	574434.654182	42.536717
3502.789821	574405.694110	42.541722
3502.876425	574380.344226	42.546727
3503.198596	574349.840024	42.551732
3503.040759	574316.852051	42.556736
3502.737717	574276.712190	42.561741
3502.674796	574250.231451	42.566746
3502.653761	574216.770257	42.571751
3502.610526	574190.185956	42.576756
3502.266817	574166.809388	42.581760
3502.702366	574130.316427	42.586765
3502.523890	574108.067860	42.591770
3502.750758	574070.955095	42.596775
3502.656605	574053.710458	42.601780
3502.464208	574017.415644	42.606784
3502.700512	573997.209260	42.611789
3502.615519	573968.624065	42.616794
3502.681856	573946.286736	42.621799
3503.046163	573908.299016	42.626804
3502.793042	573883.502857	42.631808
3503.082694	573846.479888	42.636813
3502.713425	573827.973412	42.641818
3502.656200	573790.101366	42.646823
3503.027582	573758.032501	42.651828
3502.702923	573726.222877	42.656832
3502.757884	573705.693107	42.661837
3502.642051	573660.253540	42.666842
3502.597786	573624.385874	42.671847
3502.874561	573599.155036	42.676852
3502.605164	573580.732891	42.681856
3502.988891	573544.045448	42.686861
3502.878665	573519.677725	42.691866
3502.829200	573480.248016	42.696871
3502.644101	573446.810195	42.701876
3502.888841	573428.056553	42.706880
3502.774345	573393.905089	42.711885
3503.045189	573359.592931	42.716890
3502.503974	573329.823061	42.721895
3502.611658	573289.364612	42.726900
3502.192558	573267.553414	42.731904
3502.714938	573239.774595	42.736909
3502.494832	573226.612633	42.741914
3502.274299	573198.598620	42.746919
3502.660372	573165.070678	42.751924
3502.211865	573150.589576	42.756928
3502.376099	573121.812755	42.761933
3502.242807	573102.565732	42.766938
3502.347485	573070.737326	42.771943
3502.252324	573052.889203	42.776948
3502.485921	573029.369857	42.781952
3502.067451	572997.572851	42.786957
3501.895708	572991.528181	42.791962
3501.978012	572958.197647	42.796967
3502.184297	572941.305767	42.801972
3502.373740	572928.430676	42.806977
3502.818393	572895.545086	42.811981
3502.137522	572863.236773	42.816986
3502.313241	572857.739844	42.821991
3502.337391	572827.278138	42.826996
3502.203139	572816.059209	42.832001
3502.274157	572772.142384	42.837005
3502.481630	572762.475674	42.842010
3502.304584	572741.729540	42.847015
3502.406195	572717.778580	42.852020
3502.061407	572705.287821	42.857025
3501.922525	572664.062837	42.862029
3502.515051	572649.568887	42.867034
3502.290466	572621.804974	42.872039
3502.052445	572597.354890	42.877044
3502.167321	572577.415858	42.882049
3502.612187	572551.955703	42.887053
3502.501318	572538.474792	42.892058
3502.176769	572520.410797	42.897063
3502.341083	572494.091149	42.902068
3502.347809	572466.190337	42.907073
3502.383062	572441.446300	42.912077
3502.472819	572413.281482	42.917082
3502.147302	572393.661871	42.922087
3502.236438	572360.629596	42.927092
3501.902572	572355.964784	42.932097
3502.326656	572322.328058	42.937101
3502.611534	572305.322589	42.942106
3502.174362	572278.644851	42.947111
3502.411727	572250.205653	42.952116
3502.029966	572236.616191	42.957121
3502.215098	572214.909230	42.962125
3502.507593	572186.160172	42.967130
3502.336117	572158.637728	42.972135
3502.451689	572143.414808	42.977140
3502.169975	572113.852079	42.982145
3502.294299	572098.577549	42.987149
3502.028576	572066.703876	42.992154
3502.261603	572053.921345	42.997159
3502.630918	572025.109691	43.002164
3501.971788	572006.043375	43.007169
3502.273728	571970.618179	43.012173
3502.078024	571956.648026	43.017178
3502.227607	571937.103899	43.022183
3502.287495	571916.319218	43.027188
3502.160964	571900.130185	43.032193
3502.330195	571872.704333	43.037197
3502.515956	571861.083160	43.042202
3501.986691	571838.834798	43.047207
3502.087094	571814.681399	43.052212
3502.110143	571797.766287	43.057217
3502.326809	571770.583685	43.062221
3502.181174	571755.953087	43.067226
3502.086024	571727.614750	43.072231
3502.206902	571713.996268	43.077236
3502.113512	571700.461449	43.082241
3502.630368	571665.403169	43.087245
3502.127340	571636.927638	43.092250
3501.782455	571620.270513	43.097255
3502.310465	571597.806214	43.102260
3501.813081	571582.477634	43.107265
3501.980750	571559.919042	43.112269
3502.086080	571546.854808	43.117274
3502.026014	571529.500641	43.122279
3501.977995	571499.397948	43.127284
3501.609043	571492.480003	43.132289
3502.255491	571468.742346	43.137293
3502.534849	571447.069378	43.142298
3502.517395	571425.643505	43.147303
3502.542146	571386.997878	43.152308
3502.217636	571376.710583	43.157313
3502.361597	571341.358315	43.162317
3502.171755	571319.156242	43.167322
3502.136657	571310.329174	43.172327
3502.281936	571280.195686	43.177332
3502.092102	571263.212692	43.182337
3502.261772	571242.760914	43.187341
3502.315606	571224.485153	43.192346
3502.139287	571211.012901	43.197351
3502.268113	571187.606505	43.202356
3502.491065	571171.411987	43.207361
3502.109276	571143.919970	43.212365
3502.259322	571119.958081	43.217370
3502.263775	571101.840399	43.222375
3502.695041	571072.163508	43.227380
3502.454664	571048.061761	43.232385
3502.340335	571021.430976	43.237389
3502.341116	571005.421512	43.242394
3501.949509	570972.259627	43.247399
3502.431771	570944.431309	43.252404
3502.262731	570939.087726	43.257409
3502.382145	570911.817912	43.262413
3502.227129	570891.516636	43.267418
3502.233352	570873.348129	43.272423
3502.550806	570840.928183	43.277428
3502.103927	570813.596103	43.282433
3501.967635	570789.879032	43.287437
3502.017146	570770.649674	43.292442
3502.002213	570756.398855	43.297447
3502.402988	570733.601445	43.302452
3502.105811	570702.682425	43.307457
3502.324801	570685.684847	43.312461
3502.286018	570664.160505	43.317466
3502.179360	570644.001791	43.322471
3502.562707	570609.814334	43.327476
3502.300221	570602.879202	43.332481
3502.385933	570573.204850	43.337485
3502.176503	570559.636630	43.342490
3502.226551	570540.206050	43.347495
3502.703264	570520.859302	43.352500
3502.225396	570492.678104	43.357505
3502.127470	570459.418630	43.362509
3502.085073	570445.121528	43.367514
3502.247486	570425.221494	43.372519
3502.704297	570407.282937	43.377524
3501.881296	570380.008617	43.382529
3501.997587	570362.474542	43.387533
3502.349239	570333.209691	43.392538
3501.867289	570318.429069	43.397543
3502.188521	570293.284348	43.402548
3501.907614	570289.162480	43.407553
3501.980631	570260.442891	43.412557
3501.900242	570247.958285	43.417562
3502.012253	570235.493778	43.422567
3502.271334	570211.613321	43.427572
3502.300085	570197.254598	43.432577
3502.113393	570165.262877	43.437581
3501.798577	570149.552499	43.442586
3501.826438	570129.120901	43.447591
3502.246908	570107.072011	43.452596
3501.918420	570089.908188	43.457601
3501.831630	570067.537003	43.462605
3501.714536	570063.891343	43.467610
3501.727109	570033.022469	43.472615
3502.171468	570021.660144	43.477620
3501.850425	570000.078298	43.482625
3502.125701	569987.437427	43.487629
3502.065920	569974.748541	43.492634
3501.501979	569952.050201	43.497639
3502.134414	569939.754967	43.502644
3501.691734	569917.991220	43.507649
3501.913588	569902.246796	43.512653
3501.644410	569902.589913	43.517658
3501.925278	569891.855305	43.522663
3502.317482	569866.999699	43.527668
3502.212828	569844.580680	43.532673
3501.960941	569826.049334	43.537677
3502.263747	569812.450341	43.542682
3502.351784	569788.595743	43.547687
3502.264690	569752.873162	43.552692
3501.884191	569739.380901	43.557697
3501.859561	569709.621180	43.562701
3501.687781	569700.161749	43.567706
3501.879068	569702.791885	43.572711
3501.999954	569660.361039	43.577716
3501.983707	569659.209066	43.582721
3502.144686	569628.215518	43.587725
3502.119554	569622.146136	43.592730
3501.996689	569598.625264	43.597735
3501.931053	569569.724853	43.602740
3501.623978	569562.093369	43.607745
3502.212949	569528.523043	43.612749
3502.152705	569520.250639	43.617754
3501.754563	569496.672207	43.622759
3501.992472	569477.611997	43.627764
3502.415437	569462.789189	43.632769
3501.963569	569452.419680	43.637773
3501.997460	569429.526459	43.642778
3501.752202	569404.719314	43.647783
3501.875174	569387.785018	43.652788
3501.721648	569369.739485	43.657793
3501.670858	569353.033074	43.662797
3501.367573	569349.165327	43.667802
3501.603837	569341.247985	43.672807
3502.098819	569323.753510	43.677812
3501.989188	569317.396017	43.682817
3501.601033	569278.205502	43.687821
3501.653353	569262.085159	43.692826
3501.603118	569269.571714	43.697831
3501.882493	569242.624278	43.702836
3501.681172	569235.528172	43.707841
3502.081814	569219.102348	43.712845
3502.149670	569194.597155	43.717850
3501.778207	569190.087495	43.722855
3502.080964	569160.877496	43.727860
3501.991724	569148.644046	43.732865
3501.876249	569133.904987	43.737869
3502.169485	569111.522723	43.742874
3502.313099	569095.187097	43.747879
3502.079084	569063.601253	43.752884
3502.021908	569047.447532	43.757889
3502.013749	569028.374851	43.762893
3502.049953	569014.816593	43.767898
3501.800778	568990.862472	43.772903
3501.953985	568969.304934	43.777908
3502.178992	568957.724879	43.782913
3501.904519	568934.627905	43.787917
3502.087355	568925.363370	43.792922
3502.092665	568901.168499	43.797927
3501.825430	568887.155578	43.802932
3501.706492	568867.999559	43.807937
3501.531074	568854.474195	43.812941
3502.196396	568861.046032	43.817946
3502.072899	568817.847157	43.822951
3502.458127	568806.944639	43.827956
3502.217613	568783.992639	43.832961
3501.732716	568760.275667	43.837965
3501.794284	568744.855891	43.842970
3502.162684	568725.723842	43.847975
3502.287449	568701.710659	43.852980
3502.068268	568685.832735	43.857985
3502.121343	568663.838516	43.862989
3502.258258	568645.194284	43.867994
3502.163724	568627.841108	43.872999
3502.124570	568598.331760	43.878004
3501.925646	568582.952489	43.883009
3502.078489	568565.610743	43.888013
3502.449469	568543.064632	43.893018
3502.139782	568522.331568	43.898023
3502.234786	568499.376745	43.903028
3502.288774	568499.117216	43.908033
3502.341265	568461.712307	43.913037
3502.414738	568439.061911	43.918042
3502.360108	568418.690363	43.923047
3502.244466	568398.177726	43.928052
3502.413429	568369.538805	43.933057
3502.259743	568343.962095	43.938061
3502.309249	568319.508105	43.943066
3501.798848	568298.806015	43.948071
3501.987102	568287.431824	43.953076
3501.537382	568269.280273	43.958081
3501.759281	568232.500707	43.963085
3501.901793	568225.350224	43.968090
3501.812171	568215.625735	43.973095
3501.906331	568206.575278	43.978100
3501.649772	568199.135780	43.983105
3502.043321	568175.079482	43.988109
3502.361101	568164.688883	43.993114
3502.002907	568144.113315	43.998119
3501.981225	568109.329166	44.003124
3501.718078	568107.211666	44.008129
3502.011382	568068.111287	44.013133
3502.034498	568061.531552	44.018138
3501.807593	568048.013288	44.023143
3502.097232	568027.587230	44.028148
3501.775715	568006.955483	44.033153
3501.973315	567982.126235	44.038157
3501.740088	567972.524387	44.043162
3501.612066	567967.173001	44.048167
3501.621040	567940.013796	44.053172
3501.808090	567949.371682	44.058177
3501.855569	567927.226334	44.063181
3501.800122	567904.996636	44.068186
3501.686116	567895.175289	44.073191
3501.413668	567878.501388	44.078196
3501.253059	567869.390095	44.083201
3501.694134	567862.845308	44.088205
3501.703083	567854.058893	44.093210
3501.492613	567832.104286	44.098215
3502.036909	567815.453212	44.103220
3501.696423	567808.327778	44.108225
3501.951911	567800.356177	44.113229
3501.813799	567774.173370	44.118234
3501.966291	567768.878439	44.123239
3502.036017	567748.486267	44.128244
3501.905067	567731.539032	44.133249
3501.616251	567710.951843	44.138253
3501.696925	567700.949296	44.143258
3501.840909	567689.983039	44.148263
3502.306523	567667.520827	44.153268
3501.685216	567662.698216	44.158273
3501.619156	567634.646416	44.163277
3501.677083	567619.526907	44.168282
3501.303271	567602.266045	44.173287
3501.486377	567605.550553	44.178292
3501.370531	567594.173019	44.183297
3501.576480	567570.094589	44.188301
3501.606306	567566.676170	44.193306
3501.936233	567566.022077	44.198311
3501.850467	567529.388770	44.203316
3501.856392	567530.140751	44.208321
3501.505810	567503.940344	44.213325
3501.918708	567490.923819	44.218330
3501.797222	567484.717769	44.223335
3501.588516	567464.469024	44.228340
3501.513792	567451.127073	44.233345
3501.619320	567435.046057	44.238349
3502.038729	567439.548705	44.243354
3501.523205	567408.152929	44.248359
3501.845395	567395.050074	44.253364
3501.816217	567387.474100	44.258369
3501.940571	567356.429966	44.263373
3501.763173	567360.825136	44.268378
3502.131031	567332.303155	44.273383
3501.918666	567317.627120	44.278388
3501.902571	567304.828055	44.283393
3501.899425	567274.857873	44.288397
3502.020848	567266.254237	44.293402
3501.731470	567238.939215	44.298407
3502.332038	567223.182134	44.303412
3502.339168	567203.200403	44.308417
3502.125859	567191.285482	44.313421
3501.936562	567171.485010	44.318426
3502.148535	567158.047699	44.323431
3502.578076	567123.089635	44.328436
3501.922296	567115.661641	44.333441
3501.973749	567090.803123	44.338445
3502.033933	567075.531941	44.343450
3501.990151	567058.770904	44.348455
3501.535628	567031.029380	44.353460
3501.839950	567033.592260	44.358465
3501.621438	566997.178829	44.363469
3501.850162	566985.144389	44.368474
3501.632413	566984.726494	44.373479
3501.654918	566960.173440	44.378484
3501.580028	566948.035815	44.383489
3501.757231	566930.838418	44.388493
3501.695734	566925.074520	44.393498
3501.397578	566909.206492	44.398503
3501.540274	566895.578893	44.403508
3501.503322	566890.463788	44.408513
3501.817692	566878.164830	44.413517
3501.499165	566869.880695	44.418522
3501.360815	566859.007991	44.423527
3502.039641	566845.547541	44.428532
3501.988125	566837.271844	44.433537
3501.657279	566822.212069	44.438541
3501.661627	566799.067223	44.443546
3501.576732	566778.145266	44.448551
3502.029355	566773.807046	44.453556
3501.642238	566757.852308	44.458561
3501.742172	566737.252813	44.463565
3502.073171	566729.218468	44.468570
3501.563113	566704.346491	44.473575
3501.662756	566692.181313	44.478580
3501.753254	566686.092307	44.483585
3501.456585	566658.526030	44.488589
3501.760207	566646.780759	44.493594
3501.618696	566637.866327	44.498599
3501.956668	566617.631046	44.503604
3501.291867	566602.070936	44.508609
3501.565712	566592.288258	44.513613
3501.517642	566593.701406	44.518618
3501.665532	566574.048018	44.523623
3501.462250	566561.277393	44.528628
3501.534175	566546.957576	44.533633
3501.344089	566543.573233	44.538637
3501.537041	566525.418875	44.543642
3501.289766	566519.482995	44.548647
3501.637966	566504.969321	44.553652
3501.799057	566511.269906	44.558657
3501.621372	566483.082145	44.563661
3501.514685	566480.437828	44.568666
3501.773432	566474.673848	44.573671
3501.800430	566441.132204	44.578676
3501.780492	566440.382131	44.583681
3501.869814	566420.938462	44.588685
3502.077509	566389.878709	44.593690
3501.711890	566386.772789	44.598695
3501.804217	566374.407599	44.603700
3501.671509	566365.340963	44.608705
3501.379708	566350.726322	44.613709
3501.699789	566348.818555	44.618714
3501.232641	566328.005747	44.623719
3501.851911	566318.470076	44.628724
3501.381680	566313.422450	44.633729
3501.283237	566295.162666	44.638733
3501.794276	566276.958193	44.643738
3501.543690	566273.281990	44.648743
3501.721688	566260.602047	44.653748
3501.573855	566241.647010	44.658753
3501.521041	566222.877913	44.663757
3501.759465	566217.619049	44.668762
3501.769492	566211.040308	44.673767
3502.082785	566189.552974	44.678772
3501.806919	566181.462501	44.683777
3501.750245	566168.668523	44.688781
3501.748607	566142.661513	44.693786
3501.256268	566139.073267	44.698791
3501.732900	566124.237799	44.703796
3501.868535	566101.171449	44.708801
3501.620942	566089.762822	44.713805
3501.597870	566079.574265	44.718810
3501.316304	566068.924037	44.723815
3502.135371	566057.700080	44.728820
3501.727379	566043.354252	44.733825
3501.646088	566025.693850	44.738829
3501.649549	566021.777022	44.743834
3501.567158	566015.915523	44.748839
3501.306121	565984.275262	44.753844
3501.638072	565985.679284	44.758849
3501.255867	565977.354253	44.763853
3501.778337	565973.808142	44.768858
3501.505000	565955.424541	44.773863
3502.006497	565935.363339	44.778868
3501.468758	565923.096165	44.783873
3501.577178	565903.849476	44.788877
3501.414489	565894.536118	44.793882
3501.304603	565890.436133	44.798887
3501.555862	565876.087454	44.803892
3501.732957	565865.214712	44.808897
3501.617213	565860.613551	44.813901
3501.787644	565848.235590	44.818906
3501.353232	565842.228200	44.823911
3501.496382	565816.348449	44.828916
3501.698817	565817.622114	44.833921
3501.752810	565808.626271	44.838925
3501.854603	565784.309374	44.843930
3501.629535	565762.754786	44.848935
3501.534680	565760.008037	44.853940
3501.505921	565739.376680	44.858945
3501.365102	565725.591194	44.863949
3501.810708	565713.471325	44.868954
3501.642753	565719.924198	44.873959
3501.756657	565697.563367	44.878964
3501.590238	565685.237892	44.883969
3501.519876	565676.261387	44.888973
3501.745421	565653.129884	44.893978
3501.368801	565648.469002	44.898983
3501.627805	565640.445162	44.903988
3501.533061	565633.982891	44.908993
3501.436482	565603.269856	44.913997
3501.488542	565598.140265	44.919002
3501.024022	565596.505661	44.924007
3501.657483	565589.126177	44.929012
3501.505567	565572.229266	44.934017
3501.459501	565567.014583	44.939021
3501.523530	565558.016978	44.944026
3501.260815	565557.656266	44.949031
3501.451589	565535.132477	44.954036
3501.424869	565520.023461	44.959041
3501.277121	565501.770136	44.964045
3501.809138	565502.691054	44.969050
3501.402257	565502.704345	44.974055
3501.630165	565470.484151	44.979060
3501.344843	565468.218996	44.984065
3501.553747	565469.642318	44.989069
3501.382799	565458.522346	44.994074
3501.455854	565434.962358	44.999079
3501.287920	565424.795873	45.004084
3501.320947	565418.464138	45.009089
3501.390031	565418.553652	45.014093
3501.453786	565412.719210	45.019098
3501.221312	565398.997875	45.024103
3501.690050	565366.789955	45.029108
3501.205541	565370.229680	45.034113
3501.067526	565363.924654	45.039117
3501.228453	565367.062638	45.044122
3501.105491	565366.429021	45.049127
3501.476950	565345.533558	45.054132
3500.999838	565333.306490	45.059137
3501.249481	565328.296524	45.064141
3501.234867	565330.859435	45.069146
3501.483590	565328.560976	45.074151
3501.857186	565317.355742	45.079156
3501.233924	565302.490331	45.084161
3501.484144	565296.325419	45.089165
3501.261829	565293.698905	45.094170
3500.994591	565285.807298	45.099175
3501.691329	565272.292026	45.104180
3501.376002	565258.483055	45.109185
3501.196108	565253.038098	45.114189
3501.702566	565247.485843	45.119194
3501.255426	565241.630761	45.124199
3501.253573	565216.927193	45.129204
3501.424240	565211.929524	45.134209
3501.422935	565201.837216	45.139213
3501.421813	565203.594670	45.144218
3501.100612	565208.515241	45.149223
3501.385900	565191.549428	45.154228
3501.339978	565173.831990	45.159233
3501.526912	565172.949072	45.164237
3501.691200	565166.747314	45.169242
3501.470483	565167.032768	45.174247
3501.402160	565138.272320	45.179252
3501.276400	565135.379620	45.184257
3501.294052	565126.639988	45.189261
3501.514232	565126.454827	45.194266
3501.181588	565127.209681	45.199271
3501.310757	565099.623336	45.204276
3501.243397	565095.114730	45.209281
3501.407894	565082.385403	45.214285
3501.188509	565080.009440	45.219290
3501.464501	565076.401170	45.224295
3501.514256	565067.154360	45.229300
3501.529345	565049.577830	45.234305
3501.299286	565040.625799	45.239309
3501.662039	565035.397179	45.244314
3501.096723	565024.187806	45.249319
3500.769152	565014.799094	45.254324
3500.997972	565006.930173	45.259329
3501.584821	565006.386419	45.264333
3501.510796	565000.372463	45.269338
3501.076152	565000.942422	45.274343
3501.270465	564996.643930	45.279348
3501.777984	564994.204526	45.284353
3501.433456	564974.223717	45.289357
3502.241302	564948.790458	45.294362
3501.780432	564940.728038	45.299367
3501.672189	564915.889827	45.304372
3501.704334	564908.704345	45.309377
3501.236088	564899.689016	45.314381
3501.341417	564884.006196	45.319386
3501.599387	564875.429656	45.324391
3501.663080	564866.230720	45.329396
3501.186676	564869.167198	45.334401
3501.624891	564845.649358	45.339405
3501.552843	564830.446108	45.344410
3501.493153	564839.393172	45.349415
3501.642036	564821.243043	45.354420
3501.584343	564804.380498	45.359425
3501.324959	564796.487330	45.364429
3501.841687	564791.334956	45.369434
3501.440004	564773.973802	45.374439
3501.625869	564750.796497	45.379444
3501.437832	564742.440222	45.384449
3501.647114	564750.089982	45.389453
3501.912124	564728.306223	45.394458
3501.581592	564713.494720	45.399463
3501.598063	564700.135346	45.404468
3501.585727	564685.926836	45.409473
3501.300577	564680.698917	45.414477
3501.440141	564664.608744	45.419482
3501.213212	564662.484941	45.424487
3501.314879	564656.744621	45.429492
3501.118577	564641.359695	45.434497
3501.350003	564630.025388	45.439501
3501.411423	564621.881096	45.444506
3501.387480	564625.650744	45.449511
3501.094251	564620.875983	45.454516
3501.309084	564620.038876	45.459521
3501.472314	564606.355172	45.464525
3501.488003	564584.961616	45.469530
3501.203325	564594.496389	45.474535
3501.240543	564584.146456	45.479540
3501.336819	564576.097111	45.484545
3501.303181	564557.372540	45.489549
3501.579596	564543.319572	45.494554
3501.109502	564531.893981	45.499559
3501.179630	564529.020720	45.504564
3501.821163	564541.272936	45.509569
3501.209463	564518.119423	45.514573
3501.483446	564511.548671	45.519578
3501.765226	564506.834614	45.524583
3501.322695	564495.254036	45.529588
3501.599297	564495.662616	45.534593
3501.838878	564476.744562	45.539597
3501.401514	564470.536062	45.544602
3501.364157	564463.612241	45.549607
3501.454282	564428.598711	45.554612
3501.563275	564416.931836	45.559617
3501.061097	564414.700373	45.564621
3501.307095	564421.340322	45.569626
3501.393135	564413.694180	45.574631
3501.179942	564398.060501	45.579636
3501.062705	564385.977031	45.584641
3501.703222	564378.445044	45.589645
3501.661960	564368.860406	45.594650
3501.522859	564366.471745	45.599655
3501.459302	564343.884985	45.604660
3501.782739	564341.373796	45.609665
3501.343159	564334.362133	45.614669
3501.697804	564327.025447	45.619674
3501.422494	564306.480308	45.624679
3501.740455	564286.997331	45.629684
3501.575623	564288.077506	45.634689
3501.851932	564275.982615	45.639693
3501.682183	564250.248729	45.644698
3501.437720	564250.035764	45.649703
3501.882260	564225.210095	45.654708
3501.827504	564220.799610	45.659713
3501.585337	564205.521708	45.664717
3501.694358	564189.435655	45.669722
3501.753323	564177.475070	45.674727
3501.936866	564162.431854	45.679732
3501.782512	564154.772908	45.684737
3501.661504	564126.671001	45.689741
3501.902373	564124.373537	45.694746
3501.619969	564107.545112	45.699751
3501.768953	564082.212970	45.704756
3501.837308	564076.778868	45.709761
3501.842249	564055.938397	45.714765
3501.660526	564042.810117	45.719770
3501.596446	564037.848645	45.724775
3501.619534	564014.745542	45.729780
3501.710616	564005.742510	45.734785
3501.771104	563996.844686	45.739789
3501.766641	563977.361382	45.744794
3501.302257	563976.329114	45.749799
3501.298896	563959.004905	45.754804
3501.541849	563959.519198	45.759809
3501.263454	563933.801599	45.764813
3501.708117	563906.112895	45.769818
3501.261426	563854.861166	45.774823
3501.029701	563753.258047	45.779828
3501.162253	563597.612978	45.784833
3500.820484	563401.965499	45.789837
3501.036003	563158.920686	45.794842
3500.181156	562864.662139	45.799847
3499.896776	562516.719693	45.804852
3499.139803	562126.200530	45.809857
3498.449004	561700.198510	45.814861
3498.004911	561226.677075	45.819866
3496.733891	560719.460991	45.824871
3496.287155	560158.747331	45.829876
3495.647801	559566.188160	45.834881
3494.230192	558924.638734	45.839885
3493.435196	558242.011153	45.844890
3491.833670	557516.361374	45.849895
3491.124580	556759.676280	45.854900
3489.655936	555966.379333	45.859905
3488.303402	555128.486881	45.864909
3487.058683	554247.750049	45.869914
3485.331001	553344.406755	45.874919
3483.805030	552393.664880	45.879924
3482.292205	551408.814067	45.884929
3480.773646	550392.714817	45.889933
3479.114320	549343.218758	45.894938
3477.002515	548263.433540	45.899943
3474.913940	547141.610584	45.904948
3472.993892	545994.261972	45.909953
3470.820780	544827.884834	45.914957
3469.109179	543620.582159	45.919962
3467.001561	542396.623508	45.924967
3464.843666	541131.952053	45.929972
3462.543562	539844.684260	45.934977
3459.835006	538524.690468	45.939981
3457.546087	537191.660342	45.944986
3455.601879	535834.025781	45.949991
3452.636012	534439.207507	45.954996
3450.329444	533034.418630	45.960001
3447.632163	531608.593094	45.965005
3445.342438	530155.456710	45.970010
3442.377589	528690.983449	45.975015
3440.275782	527194.531806	45.980020
3436.981234	525691.850742	45.985025
3434.293768	524168.400907	45.990029
3431.283330	522620.240528	45.995034
3428.228918	521072.059270	46.000039
3425.680531	519494.946455	46.005044
3422.739078	517912.973839	46.010049
3419.594575	516311.594033	46.015053
3416.100442	514698.789366	46.020058
3412.782715	513087.432159	46.025063
3410.257735	511445.761382	46.030068
3407.379711	509795.127301	46.035073
3403.966856	508128.495304	46.040077
3400.684948	506452.162966	46.045082
3397.524021	504783.433310	46.050087
3394.590534	503081.173739	46.055092
3390.879686	501387.614280	46.060097
3387.511594	499679.319435	46.065101
3384.290402	497959.041441	46.070106
3380.234275	496235.411166	46.075111
3377.387023	494518.357361	46.080116
3373.759717	492791.987613	46.085121
3369.993989	491047.918493	46.090125
3366.684550	489298.273498	46.095130
3362.975182	487536.014023	46.100135
3360.280227	485788.849480	46.105140
3356.292880	484037.950189	46.110145
3352.675762	482272.193618	46.115149
3349.018738	480507.961413	46.120154
3345.046017	478746.713639	46.125159
3341.769741	476984.200654	46.130164
3338.098999	475208.715615	46.135169
3334.222658	473446.209941	46.140173
3330.688501	471669.049767	46.145178
3327.517679	469904.633692	46.150183
3324.284853	468123.147787	46.155188
3320.530916	466347.569802	46.160193
3316.456926	464561.129863	46.165197
3312.771333	462772.162855	46.170202
3308.863522	460996.346688	46.175207
3305.691423	459204.950827	46.180212
3301.992834	457425.088762	46.185217
3297.959529	455645.450446	46.190221
3294.278538	453844.724019	46.195226
3290.315932	452067.039604	46.200231
3286.411869	450281.422964	46.205236
3282.714834	448505.518481	46.210241
3279.059197	446728.926399	46.215245
3275.483244	444954.376320	46.220250
3271.769141	443174.814627	46.225255
3268.008884	441388.403685	46.230260
3264.192410	439613.530701	46.235265
3260.225870	437831.371309	46.240269
3256.710904	436063.867933	46.245274
3252.826803	434303.706710	46.250279
3248.909082	432526.466682	46.255284
3245.411542	430762.123247	46.260289
3241.303850	428997.514008	46.265293
3237.922549	427233.698376	46.270298
3234.021960	425468.287708	46.275303
3230.004533	423711.966689	46.280308
3226.071865	421951.881442	46.285313
3221.995058	420198.867360	46.290317
3218.645480	418441.332126	46.295322
3214.654666	416697.948002	46.300327
3210.801440	414946.182912	46.305332
3207.421166	413214.841786	46.310337
3203.030287	411476.824161	46.315341
3199.574391	409736.796597	46.320346
3195.747025	408004.653543	46.325351
3192.006459	406273.325333	46.330356
3187.888734	404549.989211	46.335361
3183.924225	402827.055717	46.340365
3180.789022	401112.894900	46.345370
3176.346868	399386.631188	46.350375
3172.565929	397667.342754	46.355380
3168.706477	395959.817650	46.360385
3164.767001	394258.374853	46.365389
3161.130679	392551.789108	46.370394
3157.683093	390853.734712	46.375399
3153.737562	389167.596734	46.380404
3150.162010	387470.648864	46.385409
3146.210755	385771.968875	46.390413
3142.285969	384082.387155	46.395418
3138.281789	382397.657452	46.400423
3134.790561	380713.067681	46.405428
3131.108699	379040.690211	46.410433
3126.932043	377378.442781	46.415437
3123.432012	375687.616031	46.420442
3119.446947	374029.220212	46.425447
3115.561610	372369.234694	46.430452
3111.802912	370711.288749	46.435457
3108.066027	369056.924544	46.440461
3104.431678	367410.119952	46.445466
3100.726832	365752.992273	46.450471
3096.838325	364108.146991	46.455476
3092.724305	362467.894544	46.460481
3089.046869	360834.877723	46.465485
3085.510458	359190.746024	46.470490
3081.748338	357561.173769	46.475495
3078.145155	355921.222253	46.480500
3074.586098	354292.437108	46.485505
3070.129920	352663.047140	46.490509
3066.771119	351039.782672	46.495514
3062.875910	349428.366683	46.500519
3058.925452	347800.559017	46.505524
3055.130978	346203.943245	46.510529
3051.516410	344585.434674	46.515533
3048.105897	342983.750881	46.520538
3044.215803	341390.916390	46.525543
3040.315701	339773.905211	46.530548
3036.556031	338184.338299	46.535553
3033.106109	336597.755308	46.540557
3029.281803	334999.438090	46.545562
3025.374893	333425.530948	46.550567
3021.718799	331834.071313	46.555572
3017.698257	330246.748176	46.560577
3013.794270	328687.600797	46.565581
3010.705298	327103.336290	46.570586
3006.687177	325532.636229	46.575591
3003.010983	323964.009639	46.580596
2999.481178	322400.388407	46.585601
2995.839898	320826.677267	46.590605
2992.323081	319263.523050	46.595610
2988.478424	317704.485345	46.600615
2984.584848	316143.415529	46.605620
2981.038232	314576.868353	46.610625
2977.011589	313024.769719	46.615629
2973.683427	311480.194575	46.620634
2970.102665	309923.292248	46.625639
2966.541892	308368.346756	46.630644
2962.731976	306831.611839	46.635649
2958.712285	305279.618457	46.640653
2955.408085	303726.218824	46.645658
2951.471230	302195.980744	46.650663
2947.952103	300652.576604	46.655668
2944.334393	299120.342672	46.660673
2940.442983	297584.163804	46.665677
2936.981655	296048.333942	46.670682
2932.884562	294520.275092	46.675687
2929.374205	292993.255702	46.680692
2925.198872	291486.385797	46.685697
2921.842707	289961.862629	46.690701
2918.302338	288441.455320	46.695706
2914.289927	286923.326209	46.700711
2911.135755	285406.708207	46.705716
2907.209533	283897.483515	46.710721
2903.444070	282387.869929	46.715725
2899.772378	280876.147509	46.720730
2896.068641	279383.468355	46.725735
2892.229825	277873.263975	46.730740
2888.575631	276386.221579	46.735745
2884.771352	274872.542333	46.740749
2881.370109	273378.250429	46.745754
2877.286006	271894.987699	46.750759
2873.751342	270396.565411	46.755764
2870.253037	268924.721474	46.760769
2866.571266	267439.107256	46.765773
2863.176609	265962.032058	46.770778
2859.401285	264483.008371	46.775783
2855.933146	262995.843290	46.780788
2851.936520	261525.037910	46.785793
2848.025611	260051.678787	46.790797
2844.709283	258574.413745	46.795802
2841.101995	257114.085676	46.800807
2837.353800	255645.359113	46.805812
2834.098818	254176.284633	46.810817
2830.190114	252706.380240	46.815821
2826.647224	251235.308970	46.820826
2822.868370	249786.009730	46.825831
2819.299332	248324.109575	46.830836
2815.919398	246868.407267	46.835841
2812.056637	245417.939147	46.840845
2808.451570	243952.979943	46.845850
2804.815820	242500.877044	46.850855
2800.986219	241029.847097	46.855860
2797.488118	239590.515984	46.860865
2793.627095	238140.970472	46.865869
2790.128825	236694.494171	46.870874
2786.444573	235263.780709	46.875879
2782.811116	233822.917625	46.880884
2779.035302	232376.647505	46.885889
2775.487057	230945.619448	46.890893
2772.187768	229504.412869	46.895898
2768.131118	228074.554349	46.900903
2764.790556	226641.475127	46.905908
2761.572222	225202.212506	46.910913
2757.426422	223779.140395	46.915917
2753.978638	222345.466532	46.920922
2750.165851	220929.373819	46.925927
2745.999662	219500.756761	46.930932
2742.951968	218076.424629	46.935937
2739.087781	216667.224832	46.940941
2735.516668	215243.822669	46.945946
2731.599462	213835.022131	46.950951
2728.195418	212430.603806	46.955956
2724.585789	211011.757676	46.960961
2721.051217	209602.839390	46.965965
2717.394425	208194.380708	46.970970
2713.886848	206794.362279	46.975975
2710.436612	205384.080118	46.980980
2706.456877	203979.977142	46.985985
2702.958849	202578.737778	46.990989
2699.670277	201180.965493	46.995994
2695.612306	199779.250251	47.000999
2691.907940	198376.804276	47.006004
2688.855837	196980.890463	47.011009
2684.873482	195596.162483	47.016013
2681.212229	194193.138944	47.021018
2677.883691	192807.624199	47.026023
2674.229656	191413.084343	47.031028
2670.367168	190029.110263	47.036033
2667.165216	188639.319707	47.041037
2663.704163	187251.929654	47.046042
2659.947623	185862.439186	47.051047
2656.009887	184471.595086	47.056052
2652.721060	183094.622764	47.061057
2648.761229	181714.464671	47.066061
2645.637323	180336.258552	47.071066
2641.874993	178956.619892	47.076071
2637.833658	177573.277993	47.081076
2634.326763	176198.137063	47.086081
2630.262484	174832.412017	47.091085
2627.260088	173467.269471	47.096090
2623.544973	172106.119195	47.101095
2620.134784	170731.871630	47.106100
2616.707136	169360.567036	47.111105
2612.719231	167999.317439	47.116109
2609.285421	166619.829782	47.121114
2605.556674	165247.734654	47.126119
2602.281835	163893.607227	47.131124
2598.192373	162544.318766	47.136129
2594.308365	161185.467212	47.141133
2591.411926	159826.922845	47.146138
2587.521723	158473.858108	47.151143
2583.688622	157117.912490	47.156148
2580.425354	155776.315374	47.161153
2576.157470	154431.660639	47.166157
2572.909982	153075.321990	47.171162
2568.955344	151733.112444	47.176167
2565.619725	150390.138540	47.181172
2562.160887	149066.305207	47.186177
2557.954779	147724.958827	47.191181
2554.551572	146386.562227	47.196186
2550.842904	145048.998708	47.201191
2547.441585	143644.645606	47.206196
2543.979214	142327.830583	47.211201
2540.270285	141000.846881	47.216205
2536.737887	139671.645315	47.221210
2532.902440	138357.617400	47.226215
2529.264595	137025.262254	47.231220
2525.841427	135710.710050	47.236225
2521.906993	134397.306151	47.241229
2518.441699	133093.128374	47.246234
2515.347701	131763.387210	47.251239
2511.317456	130463.789908	47.256244
2507.864514	129149.271614	47.261249
2504.161033	127851.305305	47.266253
2500.891283	126539.548956	47.271258
2497.175927	125235.726090	47.276263
2493.417586	123933.007242	47.281268
2489.701004	122635.029711	47.286273
2486.013699	121331.608610	47.291277
2482.567959	120038.099782	47.296282
2478.861811	118742.767293	47.301287
2475.512553	117437.529366	47.306292
2471.793245	116153.235912	47.311297
2467.878121	114866.397789	47.316301
2464.285030	113571.670719	47.321306
2460.534246	112296.200689	47.326311
2456.542763	111006.903990	47.331316
2453.564678	109731.149944	47.336321
2449.575554	108460.914326	47.341325
2446.437027	107190.096074	47.346330
2442.756442	105917.362688	47.351335
2438.977865	104642.556453	47.356340
2435.565528	103370.664649	47.361345
2431.640121	102102.295304	47.366349
2428.324615	100840.920769	47.371354
2424.400062	99584.214834	47.376359
2420.683992	98323.203785	47.381364
2417.500477	97056.808498	47.386369
2413.764418	95806.613613	47.391373
2410.005241	94551.655706	47.396378
2406.406673	93303.521704	47.401383
2402.669966	92053.413978	47.406388
2399.049309	90815.105359	47.411393
2394.918522	89563.382705	47.416397
2392.178825	88314.150089	47.421402
2388.568861	87087.466590	47.426407
2384.478121	85845.092544	47.431412
2381.354787	84608.578103	47.436417
2377.397475	83375.498989	47.441421
2374.132726	82138.960250	47.446426
2370.250940	80914.753141	47.451431
2366.832651	79680.784621	47.456436
2363.274234	78451.464876	47.461441
2359.267813	77233.827152	47.466445
2355.955633	76005.771717	47.471450
2351.938961	74788.193667	47.476455
2348.448468	73580.645560	47.481460
2344.913633	72365.260555	47.486465
2341.211812	71152.788795	47.491469
2337.639411	69944.364778	47.496474
2333.860635	68747.855546	47.501479
2330.269625	67538.403331	47.506484
2326.837654	66341.360846	47.511489
2322.822179	65150.165581	47.516493
2319.520648	63947.020281	47.521498
2315.891204	62760.040927	47.526503
2312.056568	61575.726696	47.531508
2308.452655	60386.140275	47.536513
2304.605635	59208.312920	47.541517
2301.236460	58020.302099	47.546522
2297.240980	56861.051458	47.551527
2293.628744	55680.985462	47.556532
2289.923696	54510.312334	47.561537
2286.231712	53345.753592	47.566541
2282.907752	52178.619115	47.571546
2279.059416	51038.026922	47.576551
2275.284870	49875.715199	47.581556
2271.910602	48719.520264	47.586561
2267.930519	47575.136124	47.591565
2264.281909	46431.455188	47.596570
2261.014349	45287.651845	47.601575
2256.901887	44152.898132	47.606580
2253.127492	43032.930853	47.611585
2249.434945	41914.104185	47.616589
2246.057225	40788.018418	47.621594
2242.267775	39664.007655	47.626599
2238.492952	38542.550492	47.631604
2235.110859	37437.376729	47.636609
2231.446288	36336.652665	47.641613
2227.898282	35216.562870	47.646618
2223.748668	34126.595849	47.651623
2220.407799	33016.288022	47.656628
2216.413170	31931.259003	47.661633
2212.573047	30845.438148	47.666637
2208.554417	29752.908111	47.671642
2204.873899	28690.915163	47.676647
2201.299965	27623.421975	47.681652
2197.285173	26561.458457	47.686657
2192.992494	25506.620619	47.691661
2189.470752	24448.758316	47.696666
2185.526189	23414.978555	47.701671
2181.866504	22381.663722	47.706676
2177.810840	21359.506053	47.711681
2173.810651	20350.473191	47.716685
2170.206134	19341.613752	47.721690
2165.974118	18356.117982	47.726695
2161.727771	17371.776244	47.731700
2157.528855	16401.492405	47.736705
2153.665068	15443.709172	47.741709
2149.661835	14497.783570	47.746714
2144.915804	13576.457239	47.751719
2139.835178	12684.516455	47.756724
2134.630199	11818.980137	47.761729
2129.124111	10976.994857	47.766733
2124.092952	10168.882616	47.771738
2118.561117	9392.883054	47.776743
2113.722077	8648.406745	47.781748
2108.763098	7926.271481	47.786753
2103.874499	7241.599394	47.791757
2098.686381	6577.774387	47.796762
2094.385767	5942.938478	47.801767
2088.940784	5339.213714	47.806772
2084.602888	4762.076974	47.811777
2078.989703	4238.161251	47.816781
2073.517128	3735.526047	47.821786
2067.986988	3284.695938	47.826791
2062.576084	2877.519760	47.831796
2057.137234	2494.500435	47.836801
2052.314489	2137.057651	47.841805
2048.020266	1810.585804	47.846810
2043.564907	1511.368907	47.851815
2039.141557	1230.576188	47.856820
2034.835019	979.950928	47.861825
2030.490967	754.766915	47.866829
2026.439261	530.245552	47.871834
2022.202865	345.468943	47.876839
2017.672132	197.295485	47.881844
2011.055572	122.505825	47.886849
2001.488783	139.141661	47.891853
1995.638624	144.568595	47.896858
1991.975194	139.329731	47.901863
1989.153070	141.011442	47.906868
1987.833284	144.293108	47.911873
1985.788895	145.413349	47.916877
1984.184051	141.162205	47.921882
1981.387237	142.627980	47.926887
1978.524689	132.840748	47.931892
1974.932275	139.344468	47.936897
1971.365136	147.780512	47.941901
1968.273162	130.673239	47.946906
1965.151226	134.638707	47.951911
1961.885178	137.459268	47.956916
1958.844435	136.289767	47.961921
1955.437508	145.020293	47.966925
1952.047409	148.761965	47.971930
1948.503912	136.648296	47.976935
1945.820291	143.712194	47.981940
1942.829149	134.663288	47.986945
1938.969392	137.146475	47.991949
1936.224809	146.108731	47.996954
1932.441455	142.255436	48.001959
1928.668867	134.743055	48.006964
1925.039727	139.835135	48.011969
1921.549031	147.623296	48.016973
1918.511388	134.933761	48.021978
1914.993549	136.664243	48.026983
1911.975425	135.741161	48.031988
1909.263070	135.023340	48.036993
1904.850663	141.003643	48.041997
1901.887144	140.600380	48.047002
1898.311691	152.141478	48.052007
1894.778453	142.092215	48.057012
1891.907019	140.766522	48.062017
1888.260022	142.188184	48.067021
1885.047782	151.808943	48.072026
1881.186286	142.598851	48.077031
1877.969003	140.033270	48.082036
1874.102285	131.583326	48.087041
1870.269145	137.858982	48.092045
1867.481909	130.992888	48.097050
1864.571529	136.950137	48.102055
1860.533242	130.912585	48.107060
1857.515161	123.690305	48.112065
1853.669020	138.415458	48.117069
1849.978369	130.744753	48.122074
1846.274331	130.950948	48.127079
1843.288396	138.986013	48.132084
1839.700090	131.530257	48.137089
1836.305651	139.483714	48.142093
1832.835772	135.404230	48.147098
1829.640724	133.100949	48.152103
1826.178026	133.475034	48.157108
1822.879051	126.923162	48.162113
1819.064371	134.047017	48.167117
1815.469504	129.306875	48.172122
1811.913383	136.700327	48.177127
1808.240364	138.480438	48.182132
1805.156065	129.449328	48.187137
1801.583703	136.383404	48.192141
1798.240202	129.303819	48.197146
1794.730728	133.051560	48.202151
1791.479490	135.347817	48.207156
1788.012830	126.325930	48.212161
1783.983948	126.491231	48.217165
1780.865397	127.890343	48.222170
1777.495922	126.734376	48.227175
1774.158526	133.723440	48.232180
1770.806565	127.154568	48.237185
1767.024696	128.486643	48.242189
1763.159422	121.697542	48.247194
1760.094287	132.301398	48.252199
1756.347688	134.374623	48.257204
1752.659737	138.586918	48.262209
1749.352508	130.125405	48.267213
1746.008616	125.507369	48.272218
1743.064883	124.189872	48.277223
1739.283595	129.261521	48.282228
1735.887258	127.853500	48.287233
1732.263460	125.503453	48.292237
1728.784649	120.716709	48.297242
1724.752674	135.847469	48.302247
1721.206747	120.763448	48.307252
1718.386921	123.431983	48.312257
1714.803885	122.711267	48.317261
1711.702477	120.855292	48.322266
1708.063017	120.421826	48.327271
1703.994539	126.389503	48.332276
1700.596392	118.954671	48.337281
1697.117128	128.237589	48.342285
1693.915567	116.769741	48.347290
1690.231297	122.750061	48.352295
1686.779393	133.401807	48.357300
1683.591752	125.092453	48.362305
1679.728515	126.411982	48.367309
1676.235687	120.744741	48.372314
1672.886373	128.033095	48.377319
1669.499807	129.999381	48.382324
1666.170845	127.476661	48.387329
1662.223259	133.529841	48.392333
1658.552723	124.834152	48.397338
1655.309462	133.153144	48.402343
1651.755185	135.420938	48.407348
1648.864641	123.720925	48.412353
1645.102348	129.659687	48.417357
1641.330416	118.724063	48.422362
1638.021846	129.894402	48.427367
1634.039871	127.606775	48.432372
1630.936662	124.425460	48.437377
1627.427222	128.144772	48.442381
1624.154086	113.815395	48.447386
1620.616449	122.753116	48.452391
1616.977848	119.484754	48.457396
1613.321984	118.041462	48.462401
1609.855973	119.298847	48.467405
1606.669524	123.505464	48.472410
1603.291192	124.129016	48.477415
1599.176863	123.548442	48.482420
1596.319521	110.410046	48.487425
1592.381216	121.299291	48.492429
1589.142578	120.287430	48.497434
1585.534538	117.039607	48.502439
1581.729379	119.023977	48.507444
1578.852800	114.611283	48.512449
1575.218177	123.431316	48.517453
1571.531305	127.181578	48.522458
1567.787284	127.463734	48.527463
1564.452096	116.488266	48.532468
1561.147190	112.424198	48.537473
1557.465874	123.703513	48.542477
1553.746637	125.019532	48.547482
1550.506449	116.231228	48.552487
1546.989117	116.876554	48.557492
1544.007211	127.182680	48.562497
1540.252836	131.468715	48.567501
1536.710403	121.351453	48.572506
1532.878991	126.260167	48.577511
1529.614582	123.392025	48.582516
1526.135052	119.526146	48.587521
1522.583907	116.525713	48.592525
1518.962832	121.819134	48.597530
1515.519371	119.143542	48.602535
1512.029380	115.953203	48.607540
1508.815813	120.429853	48.612545
1504.819059	121.175543	48.617549
1501.625394	116.293635	48.622554
1498.280279	109.619398	48.627559
1494.627352	112.127313	48.632564
1491.317648	112.566150	48.637569
1487.374679	131.182231	48.642573
1483.949159	122.173016	48.647578
1480.529270	123.170118	48.652583
1477.070501	127.359283	48.657588
1473.881454	112.811163	48.662593
1469.981505	122.027103	48.667597
1466.590878	116.331295	48.672602
1463.042246	117.699738	48.677607
1459.505725	120.005944	48.682612
1456.170994	122.856383	48.687617
1452.503853	118.171992	48.692621
1449.317408	117.743643	48.697626
1446.071042	112.955429	48.702631
1442.002971	118.508669	48.707636
1438.705413	116.636027	48.712641
1434.827002	125.544881	48.717645
1431.526687	122.944992	48.722650
1428.214295	127.342219	48.727655
1424.663583	124.275314	48.732660
1421.308725	113.704793	48.737665
1417.667510	125.306907	48.742669
1414.233985	114.789832	48.747674
1410.393402	117.149976	48.752679
1406.985028	123.460529	48.757684
1403.846258	105.908432	48.762689
1400.113091	116.917484	48.767693
1396.503980	122.022405	48.772698
1393.003139	123.440341	48.777703
1389.524802	117.941793	48.782708
1386.390322	109.174977	48.787713
1382.653969	111.227744	48.792717
1379.149414	110.194301	48.797722
1375.582342	111.780800	48.802727
1372.097680	121.251310	48.807732
1368.799588	114.503320	48.812737
1364.820982	121.086647	48.817741
1361.438007	110.906542	48.822746
1357.848788	117.283382	48.827751
1354.600002	121.531465	48.832756
1351.681698	114.189345	48.837761
1347.798427	129.641780	48.842765
1343.815252	116.413951	48.847770
1340.580941	121.495022	48.852775
1336.670021	119.765886	48.857780
1333.711552	115.619196	48.862785
1330.328945	122.558502	48.867789
1326.929912	115.446670	48.872794
1323.237508	117.182524	48.877799
1319.293805	126.905246	48.882804
1315.922496	114.315661	48.887809
1312.504838	123.797847	48.892813
1308.910675	119.355197	48.897818
1305.992269	110.073687	48.902823
1302.306881	120.534275	48.907828
1298.996461	112.668249	48.912833
1294.936524	117.293269	48.917837
1291.560637	122.431318	48.922842
1287.999132	119.828074	48.927847
1284.311573	110.698615	48.932852
1280.971330	114.331434	48.937857
1277.467069	121.811830	48.942861
1274.257146	113.857313	48.947866
1270.940183	104.467364	48.952871
1267.317749	113.187494	48.957876
1263.272504	112.548789	48.962881
1260.077532	118.262815	48.967885
1256.751101	109.298304	48.972890
1253.121082	108.683189	48.977895
1249.528835	118.031364	48.982900
1246.239489	112.854474	48.987905
1242.359868	115.967453	48.992909
1239.223513	113.329311	48.997914
1235.554510	110.682804	49.002919
1231.769743	109.459158	49.007924
1228.649699	105.999038	49.012929
1224.963028	108.891987	49.017933
1221.637018	106.704331	49.022938
1217.856767	100.417873	49.027943
1214.283139	106.539207	49.032948
1211.021510	101.392797	49.037953
1207.620363	112.416363	49.042957
1204.177060	107.418620	49.047962
1200.614709	100.519078	49.052967
1196.859267	107.905934	49.057972
1193.116733	102.550073	49.062977
1190.316330	107.594892	49.067981
1186.702137	107.879013	49.072986
1182.980970	107.578757	49.077991
1179.435473	113.407792	49.082996
1176.140268	109.294891	49.088001
1172.466418	108.711978	49.093005
1169.066192	97.202698	49.098010
1165.681262	99.611821	49.103015
1161.937248	109.572247	49.108020
1158.753005	105.207859	49.113025
1155.007418	115.124243	49.118029
1151.167175	111.928762	49.123034
1148.081432	104.840729	49.128039
1144.515588	112.938254	49.133044
1140.970104	106.298692	49.138049
1137.109954	111.129778	49.143053
1133.934721	102.024590	49.148058
1130.344786	103.640064	49.153063
1126.734396	102.341704	49.158068
1123.748379	100.806386	49.163073
1120.397007	101.821355	49.168077
1116.696764	107.358254	49.173082
1113.147054	94.635351	49.178087
1109.087163	104.882530	49.183092
1105.966459	101.356117	49.188097
1102.673260	112.862693	49.193101
1099.089557	104.849709	49.198106
1095.595814	103.178750	49.203111
1091.925362	108.207947	49.208116
1088.302791	108.085283	49.213121
1084.783793	104.735132	49.218125
1081.452158	113.238942	49.223130
1078.057364	102.121163	49.228135
1074.406465	107.023914	49.233140
1071.036431	106.937651	49.238145
1067.606937	109.996040	49.243149
1064.120446	111.712404	49.248154
1060.535857	105.983850	49.253159
1056.839459	114.209412	49.258164
1053.457978	106.588738	49.263169
1049.898136	113.343894	49.268173
1046.226557	108.075063	49.273178
1042.920464	111.996845	49.278183
1039.305819	104.248164	49.283188
1036.023821	110.602312	49.288193
1032.475840	99.853394	49.293197
1029.030484	109.245071	49.298202
1025.349441	109.020852	49.303207
1021.787519	101.118391	49.308212
1018.471305	98.951422	49.313217
1014.774118	103.409015	49.318221
1011.236907	100.726147	49.323226
1008.122581	100.827664	49.328231
1004.629638	98.992097	49.333236
1001.251341	100.109401	49.338241
997.218620	109.618361	49.343245
993.669003	97.483969	49.348250
990.346806	92.277525	49.353255
986.671075	101.797030	49.358260
983.516894	99.690127	49.363265
979.832606	100.735124	49.368269
976.308417	93.048245	49.373274
973.189273	96.548461	49.378279
969.338662	97.771366	49.383284
966.241378	96.522446	49.388289
962.568267	98.669868	49.393293
959.039601	94.084233	49.398298
955.374312	105.823110	49.403303
951.655911	102.934512	49.408308
948.326637	85.719370	49.413313
944.923295	100.938552	49.418317
941.693842	101.295403	49.423322
938.083415	99.519386	49.428327
934.118476	101.712513	49.433332
930.360484	102.595059	49.438337
927.092616	110.079670	49.443341
923.628132	104.946148	49.448346
920.181291	109.418362	49.453351
916.878570	112.036164	49.458356
913.511796	104.688498	49.463361
909.956409	101.467504	49.468365
906.408535	100.134130	49.473370
902.781308	109.127205	49.478375
899.063060	115.204846	49.483380
895.834898	100.254993	49.488385
892.751332	97.947237	49.493389
889.073176	105.132262	49.498394
885.536420	105.546742	49.503399
881.803049	99.041120	49.508404
878.410938	96.636146	49.513409
874.572021	97.914206	49.518413
871.531024	98.064398	49.523418
867.914627	89.243545	49.528423
864.040460	110.642625	49.533428
860.686600	91.729241	49.538433
856.869353	105.864796	49.543437
853.487009	94.672406	49.548442
850.273771	90.942274	49.553447
846.769674	102.722379	49.558452
843.258480	93.960993	49.563457
839.627001	103.422994	49.568461
836.739030	98.509289	49.573466
833.052410	99.725552	49.578471
829.392761	105.227717	49.583476
826.081495	102.550670	49.588481
822.110984	102.261126	49.593485
818.492213	105.146752	49.598490
815.229551	97.700569	49.603495
811.478942	95.604863	49.608500
808.354829	97.834057	49.613505
804.474640	105.620232	49.618509
801.264054	97.738786	49.623514
798.140554	94.760262	49.628519
793.969837	110.523600	49.633524
790.812912	101.058177	49.638529
787.161536	102.749837	49.643533
783.896740	102.751603	49.648538
780.006712	91.161014	49.653543
776.446704	98.716721	49.658548
773.565709	96.956261	49.663553
769.740282	104.544044	49.668557
766.064022	99.136864	49.673562
762.673927	104.169727	49.678567
758.865302	101.156132	49.683572
755.854974	98.340237	49.688577
752.367418	100.142300	49.693581
748.837161	103.377928	49.698586
745.365829	100.504512	49.703591
741.688417	106.047455	49.708596
738.384304	98.006672	49.713601
734.485995	98.958725	49.718605
731.122090	105.158105	49.723610
727.396175	96.844853	49.728615
724.081816	105.687745	49.733620
721.048080	99.569351	49.738625
717.243910	98.918439	49.743629
713.744413	87.469214	49.748634
710.245733	96.011934	49.753639
706.590110	97.334124	49.758644
703.531871	93.022945	49.763649
699.636533	94.563015	49.768653
696.232008	96.969037	49.773658
692.652035	97.361883	49.778663
688.803874	98.495929	49.783668
685.405560	96.591883	49.788673
682.184608	98.247814	49.793677
678.695504	104.014393	49.798682
675.297967	91.229910	49.803687
671.527760	92.772541	49.808692
668.346883	92.764369	49.813697
664.416904	97.470517	49.818701
660.891407	95.178266	49.823706
657.710089	92.740367	49.828711
654.146760	95.202912	49.833716
650.673127	89.716596	49.838721
646.785198	93.565102	49.843725
643.631874	85.029344	49.848730
640.240479	91.688640	49.853735
636.659432	93.676231	49.858740
633.701033	91.522974	49.863745
629.389537	95.921883	49.868749
625.809338	94.887916	49.873754
622.635287	98.387346	49.878759
618.873018	94.876165	49.883764
615.566070	97.039140	49.888769
612.027547	101.054406	49.893773
608.200464	92.826661	49.898778
604.856768	86.323419	49.903783
601.902205	100.013883	49.908788
598.264942	87.963020	49.913793
594.871293	98.539469	49.918797
591.008239	96.521579	49.923802
587.544559	81.089913	49.928807
583.779657	86.760504	49.933812
580.672967	92.906988	49.938817
576.797396	96.712457	49.943821
572.854167	98.468890	49.948826
570.210378	96.627054	49.953831
566.699670	102.716597	49.958836
563.386087	99.919790	49.963841
559.639370	103.660793	49.968845
555.923988	95.576932	49.973850
552.562234	90.870413	49.978855
549.132780	102.442754	49.983860
545.539983	88.271534	49.988865
541.960238	97.538858	49.993869
538.822672	99.083700	49.998874
535.227614	91.316369	50.003879
531.387486	99.922115	50.008884
527.920192	86.731010	50.013889
524.478864	95.413503	50.018893
521.164337	92.060033	50.023898
517.662466	94.468709	50.028903
513.661358	102.441605	50.033908
510.294178	93.923575	50.038913
506.871442	96.968439	50.043917
503.395002	93.485309	50.048922
500.223172	93.909219	50.053927
496.301332	106.862182	50.058932
493.003703	95.150483	50.063937
489.226070	109.925357	50.068941
486.064154	106.443590	50.073946
482.515064	96.511370	50.078951
478.522925	110.313758	50.083956
475.058555	95.078400	50.088961
472.024985	96.936012	50.093965
468.571143	97.812233	50.098970
464.825308	100.825460	50.103975
461.051701	110.993224	50.108980
458.065333	104.345483	50.113985
454.413132	108.603241	50.118989
451.240024	94.271417	50.123994
447.566270	101.734314	50.128999
443.576072	98.474048	50.134004
440.553149	108.353393	50.139009
436.809337	106.889540	50.144013
433.222044	101.288238	50.149018
429.424949	100.819840	50.154023
425.957539	108.218789	50.159028
423.060868	104.888492	50.164033
419.751712	104.957447	50.169037
416.305408	104.193661	50.174042
412.482689	105.390277	50.179047
409.002727	104.144540	50.184052
405.569152	97.193543	50.189057
401.941554	94.347908	50.194061
398.338094	99.392163	50.199066
395.017084	99.317450	50.204071
391.294254	104.646165	50.209076
387.969527	98.076764	50.214081
384.411740	101.373783	50.219085
380.790415	100.292572	50.224090
377.261476	93.163535	50.229095
373.568738	98.440084	50.234100
370.183469	97.008687	50.239105
366.525915	93.788104	50.244109
363.178921	94.606499	50.249114
359.872173	95.538816	50.254119
356.424194	94.012842	50.259124
353.215557	88.466163	50.264129
349.709583	96.285630	50.269133
345.873216	98.626541	50.274138
342.433287	95.017535	50.279143
339.002475	93.469896	50.284148
335.318996	89.402329	50.289153
331.777904	104.149683	50.294157
328.155644	106.675366	50.299162
324.667730	97.945372	50.304167
321.007823	99.850523	50.309172
317.512962	97.332149	50.314177
314.555939	101.620269	50.319181
310.819214	94.890810	50.324186
307.442483	98.947281	50.329191
303.657385	99.546419	50.334196
300.262263	92.570465	50.339201
296.891361	91.127355	50.344205
293.408232	94.118479	50.349210
289.893766	90.176319	50.354215
285.794184	102.730078	50.359220
282.394967	98.345917	50.364225
278.578407	116.072446	50.369229
275.648064	106.587568	50.374234
272.499949	93.574381	50.379239
269.098396	96.258503	50.384244
265.777836	93.254097	50.389249
261.549680	103.537422	50.394253
257.904877	94.771926	50.399258
254.936710	85.191752	50.404263
251.444456	90.772300	50.409268
247.533829	90.201542	50.414273
244.150612	81.970891	50.419277
240.799455	91.034818	50.424282
237.090801	97.497168	50.429287
233.460108	98.537226	50.434292
230.052424	83.536739	50.439297
227.177466	88.935171	50.444301
223.165355	97.131364	50.449306
220.022079	94.377618	50.454311
216.230091	97.793646	50.459316
212.800202	93.493416	50.464321
209.428439	99.169002	50.469325
205.601361	94.899359	50.474330
202.017824	89.879714	50.479335
198.527998	91.008450	50.484340
195.057939	92.403014	50.489345
191.376940	95.055010	50.494349
187.922640	96.709702	50.499354
184.931258	97.105455	50.504359
181.283917	95.227964	50.509364
177.898450	90.810058	50.514369
174.044723	94.770455	50.519373
170.819460	83.901803	50.524378
167.329139	94.436569	50.529383
163.393098	94.698743	50.534388
159.990311	86.094704	50.539393
156.756408	95.336443	50.544397
152.620776	92.342714	50.549402
149.653471	88.128233	50.554407
146.359451	103.029921	50.559412
142.552562	95.182063	50.564417
138.943594	95.551197	50.569421
135.618421	94.872950	50.574426
132.290013	95.419598	50.579431
128.592727	95.517831	50.584436
124.802860	94.415675	50.589441
121.491007	100.597603	50.594445
117.881922	86.552550	50.599450
114.453490	93.546852	50.604455
111.044820	99.079556	50.609460
108.035694	92.758230	50.614465
104.146437	89.966375	50.619469
100.386196	90.159905	50.624474
97.127617	88.585381	50.629479
93.600549	103.684948	50.634484
90.167521	93.082998	50.639489
86.667627	97.168332	50.644493
83.086846	89.977952	50.649498
79.578120	92.694752	50.654503
76.103643	94.551967	50.659508
72.809546	97.326894	50.664513
69.116372	95.554711	50.669517
65.386839	87.346760	50.674522
62.356714	86.517912	50.679527
58.040368	92.192839	50.684532
54.638961	87.122581	50.689537
51.716757	77.367616	50.694541
48.108715	82.071024	50.699546
44.929200	80.781529	50.704551
41.242031	89.711497	50.709556
37.435959	89.956529	50.714561
33.547881	85.516192	50.719565
30.175564	85.914732	50.724570
27.016099	78.114203	50.729575
23.256382	88.415969	50.734580
20.095396	81.099739	50.739585
16.590507	82.724456	50.744589
12.843516	84.905968	50.749594
9.764740	77.197209	50.754599
6.033582	88.899226	50.759604
2.884191	87.241192	50.764609