Thu Aug 25 13:01:14 2022

Number of Points = 9924

Depth (nm)	Load (N)	Time (s)
3.192515	101.741038	0.000000
2.698609	97.974293	0.005005
2.637199	89.273888	0.010010
2.361733	91.401846	0.015014
2.904400	81.622861	0.020019
2.836855	75.979635	0.025024
2.320131	73.510456	0.030029
2.104374	60.113891	0.035034
2.048825	63.896846	0.040038
1.703892	53.943733	0.045043
1.511240	45.105723	0.050048
1.079496	31.198852	0.055053
0.757589	22.751267	0.060058
0.404305	28.219697	0.065062
0.161869	29.200352	0.070067
-0.278308	12.029806	0.075072
-0.262623	17.721998	0.080077
-0.187798	12.879066	0.085082
-0.772118	5.741275	0.090086
-1.363882	-2.784239	0.095091
-1.282854	2.673083	0.100096
-1.692744	1.405226	0.105101
-2.078457	1.054236	0.110106
-2.150445	0.872392	0.115110
-2.509115	3.415175	0.120115
-2.793058	-5.547710	0.125120
-3.420824	4.392990	0.130125
-3.765749	4.510175	0.135130
-3.954210	6.795336	0.140134
-4.079516	16.647825	0.145139
-3.865633	10.008232	0.150144
-4.093394	-0.785789	0.155149
-4.790837	-7.636929	0.160154
-4.948299	3.552537	0.165158
-5.482515	-1.163328	0.170163
-5.492387	-4.762280	0.175168
-5.812453	3.051616	0.180173
-5.719919	-2.727398	0.185178
-5.537599	5.346306	0.190182
-6.329036	2.281100	0.195187
-6.529942	-3.097594	0.200192
-6.698647	-3.049149	0.205197
-6.992600	-3.974501	0.210202
-7.836389	1.074063	0.215206
-8.213190	0.699532	0.220211
-7.884973	-9.707031	0.225216
-8.373869	7.194342	0.230221
-8.104080	-6.309887	0.235226
-8.440915	0.136725	0.240230
-8.889528	5.234105	0.245235
-9.473758	-6.102011	0.250240
-9.762371	2.649758	0.255245
-9.909543	-1.376937	0.260250
-10.093896	5.340015	0.265254
-9.876924	3.005827	0.270259
-9.904962	-4.317194	0.275264
-10.854016	2.873914	0.280269
-10.855076	1.570475	0.285274
-11.157569	1.459548	0.290278
-11.755169	13.021703	0.295283
-11.086113	-3.718345	0.300288
-11.997715	6.760377	0.305293
-12.482892	-1.962171	0.310298
-12.776401	-4.399872	0.315302
-12.501052	-6.974161	0.320307
-12.393322	-6.738073	0.325312
-13.485077	-3.279995	0.330317
-13.601496	-5.622057	0.335322
-14.003060	-5.495997	0.340326
-14.082612	-1.462522	0.345331
-13.840315	0.375493	0.350336
-14.330951	9.864439	0.355341
-14.516994	-2.090891	0.360346
-15.122456	-1.556396	0.365350
-15.630476	-0.132331	0.370355
-15.396337	5.595231	0.375360
-15.526290	4.622036	0.380365
-15.476686	-2.051925	0.385370
-16.091382	-1.035090	0.390374
-16.683676	1.661358	0.395379
-16.849802	-2.359203	0.400384
-17.238225	5.981098	0.405389
-17.203633	-0.870846	0.410394
-17.129470	1.809765	0.415398
-17.731658	5.023457	0.420403
-18.109605	0.128084	0.425408
-18.511399	0.731909	0.430413
-18.689542	-9.452945	0.435418
-18.203220	-5.185430	0.440422
-18.769212	-3.249244	0.445427
-18.807216	-2.629652	0.450432
-20.060645	5.754431	0.455437
-19.963586	2.265275	0.460442
-20.307019	-2.682962	0.465446
-20.043671	4.802240	0.470451
-20.232579	-0.983296	0.475456
-20.262951	2.789373	0.480461
-20.843599	1.924760	0.485466
-21.322611	-5.159920	0.490470
-21.867353	-3.723774	0.495475
-21.582726	-14.170960	0.500480
-21.791614	8.441425	0.505485
-22.240408	-0.603199	0.510490
-22.744405	3.091819	0.515494
-22.892711	3.494574	0.520499
-23.030188	-7.908374	0.525504
-23.226820	-5.523859	0.530509
-23.063573	-0.674209	0.535514
-23.520830	-7.993252	0.540518
-24.164290	2.196680	0.545523
-24.221729	-2.005426	0.550528
-24.361324	-4.030643	0.555533
-24.885505	-4.932577	0.560538
-24.286911	-5.921846	0.565542
-24.995423	-3.124931	0.570547
-25.113417	-9.155694	0.575552
-25.336647	1.025341	0.580557
-26.393365	-3.975649	0.585562
-26.806072	-9.140820	0.590566
-27.111835	-7.159986	0.595571
-27.003829	-4.706143	0.600576
-27.417599	-1.531465	0.605581
-27.272907	-9.482663	0.610586
-27.190593	2.801858	0.615590
-27.718519	5.978606	0.620595
-27.225514	-6.807619	0.625600
-27.797958	-4.977989	0.630605
-28.527871	-7.113193	0.635610
-28.544841	-3.798207	0.640614
-28.837551	-1.145536	0.645619
-29.472968	-9.575617	0.650624
-29.646248	-5.261701	0.655629
-30.229533	-4.009341	0.660634
-30.085952	-16.383304	0.665638
-30.264777	-6.762889	0.670643
-30.006634	-8.812460	0.675648
-30.610608	-3.447129	0.680653
-30.954600	-11.093966	0.685658
-31.307537	-2.347940	0.690662
-31.838062	-7.444031	0.695667
-31.556834	-3.625273	0.700672
-31.873244	-2.395746	0.705677
-31.980243	-6.207270	0.710682
-32.553733	-3.969350	0.715686
-33.138081	-6.355152	0.720691
-32.841516	-10.299510	0.725696
-32.988015	0.638296	0.730701
-33.456902	-10.143245	0.735706
-34.260380	4.893337	0.740710
-34.441713	8.613730	0.745715
-34.462003	-0.061434	0.750720
-34.729447	6.475547	0.755725
-34.836035	-1.366679	0.760730
-34.909299	-8.821816	0.765734
-35.156091	-3.110653	0.770739
-34.661152	-5.668728	0.775744
-35.152967	0.928717	0.780749
-35.991632	-0.812958	0.785754
-36.211659	-4.938967	0.790758
-36.450526	-5.221214	0.795763
-37.105911	-9.857976	0.800768
-37.326641	1.559698	0.805773
-37.884372	3.791986	0.810778
-37.485165	-4.132654	0.815782
-37.993969	-5.521052	0.820787
-37.778274	-6.434508	0.825792
-37.906604	-2.273168	0.830797
-38.134938	-8.625164	0.835802
-38.389331	-11.046846	0.840806
-39.133806	-6.681397	0.845811
-39.234338	5.922841	0.850816
-39.074046	-0.265423	0.855821
-40.308994	6.758512	0.860826
-40.430079	-12.132469	0.865830
-40.771411	-3.647691	0.870835
-40.281043	-8.014723	0.875840
-40.733297	-4.055729	0.880845
-40.769830	-2.945985	0.885850
-40.625661	-8.372417	0.890854
-41.654112	8.002888	0.895859
-42.071466	-6.219415	0.900864
-42.391436	4.520947	0.905869
-42.174445	-1.565469	0.910874
-42.172291	-8.867907	0.915878
-42.599757	3.990036	0.920883
-43.605400	-2.316099	0.925888
-43.534153	-1.106183	0.930893
-44.063370	-0.827242	0.935898
-44.059488	-17.153002	0.940902
-44.153293	1.059528	0.945907
-43.914643	-5.087228	0.950912
-44.110514	-1.611332	0.955917
-44.304141	-3.479386	0.960922
-45.061620	-3.468401	0.965926
-45.630795	-1.860746	0.970931
-45.348903	-10.118178	0.975936
-45.386075	-0.874298	0.980941
-46.417600	-6.784068	0.985946
-46.553664	-11.771120	0.990950
-46.783663	-3.851118	0.995955
-46.980998	-9.220876	1.000960
-47.287927	0.938471	1.005965
-47.177480	-2.799556	1.010970
-47.003005	-3.102275	1.015974
-47.886445	-3.849839	1.020979
-48.425734	-8.672470	1.025984
-48.521178	1.902995	1.030989
-48.701436	-9.562849	1.035994
-48.555354	1.730911	1.040998
-48.747370	2.861854	1.046003
-48.854330	-4.436144	1.051008
-49.661028	3.890599	1.056013
-49.670170	-5.232399	1.061018
-50.049579	-1.939718	1.066022
-50.293501	-1.072726	1.071027
-49.698631	-4.408927	1.076032
-50.565723	-0.138158	1.081037
-51.178344	1.878103	1.086042
-51.298257	-0.925320	1.091046
-51.520873	-3.048260	1.096051
-52.194423	-13.225087	1.101056
-52.751489	-5.810660	1.106061
-52.358900	3.720225	1.111066
-52.559218	3.257931	1.116070
-52.785500	9.968798	1.121075
-52.736338	-3.121208	1.126080
-53.037551	6.973972	1.131085
-53.347974	5.722170	1.136090
-53.905881	2.190106	1.141094
-54.410163	6.622328	1.146099
-54.489375	3.154464	1.151104
-54.868150	6.269876	1.156109
-54.886087	7.455801	1.161114
-54.599586	0.659301	1.166118
-55.368053	9.236322	1.171123
-55.884152	6.899937	1.176128
-55.799533	15.833676	1.181133
-55.925112	13.448756	1.186138
-55.814428	10.295986	1.191142
-56.063127	9.382527	1.196147
-56.550830	2.511182	1.201152
-57.016786	12.322128	1.206157
-57.288720	-0.366389	1.211162
-57.779386	1.690876	1.216166
-58.492167	8.133120	1.221171
-58.482188	2.313259	1.226176
-58.167259	3.535612	1.231181
-58.742718	5.584017	1.236186
-58.774181	5.769147	1.241190
-59.035466	7.977133	1.246195
-58.934214	5.056797	1.251200
-59.248577	-0.073162	1.256205
-60.117354	7.225595	1.261210
-60.342141	0.898351	1.266214
-60.778518	2.535820	1.271219
-60.611940	-4.055225	1.276224
-60.653422	0.108326	1.281229
-60.569081	4.027536	1.286234
-60.807258	-2.072981	1.291238
-61.635019	10.790740	1.296243
-61.712379	-7.082033	1.301248
-61.637476	-2.490628	1.306253
-62.264008	-3.417651	1.311258
-62.688687	-4.183312	1.316262
-62.992892	-0.279152	1.321267
-62.623543	-5.339069	1.326272
-63.148827	-2.327252	1.331277
-64.027217	-3.603954	1.336282
-64.078409	1.779168	1.341286
-64.765407	1.883516	1.346291
-64.552171	-0.168512	1.351296
-64.621533	0.013066	1.356301
-64.665086	3.180357	1.361306
-64.550092	-3.674690	1.366310
-65.127927	1.237293	1.371315
-65.600870	-1.703803	1.376320
-65.988842	0.362681	1.381325
-66.247298	-4.352093	1.386330
-66.228809	2.570355	1.391334
-66.443181	5.834015	1.396339
-66.598110	-11.713385	1.401344
-66.931751	-2.030747	1.406349
-67.781945	5.644749	1.411354
-67.731403	4.776152	1.416358
-68.057416	1.992368	1.421363
-68.075050	-0.425283	1.426368
-67.752874	0.833900	1.431373
-68.778995	-0.653772	1.436378
-68.908762	-9.637643	1.441382
-69.353684	-8.644243	1.446387
-69.527403	-1.884670	1.451392
-69.276827	-3.467983	1.456397
-69.855345	-1.017301	1.461402
-70.290139	-10.855049	1.466406
-70.522438	-8.556694	1.471411
-70.966610	-7.772220	1.476416
-71.088175	-1.894017	1.481421
-70.936536	-3.461828	1.486426
-70.607280	-4.168452	1.491430
-71.164367	-2.173547	1.496435
-71.654123	-4.434962	1.501440
-71.785947	10.186332	1.506445
-72.355976	0.812696	1.511450
-72.530040	-10.359885	1.516454
-73.065782	1.844303	1.521459
-73.442642	-4.149061	1.526464
-73.299471	-3.988130	1.531469
-73.678969	6.214227	1.536474
-73.519977	-4.282878	1.541478
-74.188949	-9.113660	1.546483
-74.970016	-10.298042	1.551488
-75.296596	2.420703	1.556493
-74.771407	-2.173250	1.561498
-74.808445	-5.179483	1.566502
-75.272646	-4.572205	1.571507
-75.039657	-0.331438	1.576512
-75.650622	4.737597	1.581517
-76.496033	-5.855227	1.586522
-76.331639	-2.964131	1.591526
-76.579517	4.809978	1.596531
-76.995307	-0.180701	1.601536
-76.830153	-5.233932	1.606541
-77.614617	-5.383232	1.611546
-78.040246	-5.038262	1.616550
-78.078316	-8.762507	1.621555
-78.194258	1.297310	1.626560
-78.049426	-2.085435	1.631565
-78.596761	-6.704322	1.636570
-78.355279	-9.823798	1.641574
-79.516269	5.667435	1.646579
-79.192458	-4.520136	1.651584
-79.519171	-3.725593	1.656589
-79.641603	-1.026835	1.661594
-79.741731	-0.112771	1.666598
-80.828385	8.681785	1.671603
-81.122721	-1.956260	1.676608
-81.262862	-0.665766	1.681613
-81.132777	3.600617	1.686618
-81.061420	-4.430839	1.691622
-81.335044	0.461951	1.696627
-81.545296	-7.477921	1.701632
-81.776361	-5.053209	1.706637
-82.671725	0.167957	1.711642
-82.593885	-0.489782	1.716646
-83.058510	-6.491538	1.721651
-82.924955	-3.813909	1.726656
-83.752669	2.295165	1.731661
-83.924458	4.792849	1.736666
-83.959730	-7.094345	1.741670
-84.392854	3.986448	1.746675
-84.130067	-7.283058	1.751680
-84.023891	8.183630	1.756685
-84.592467	-0.810580	1.761690
-84.928856	-3.339635	1.766694
-85.285574	3.954817	1.771699
-85.486764	-2.616567	1.776704
-85.602196	-2.560648	1.781709
-86.537682	-8.058352	1.786714
-86.589800	-4.237986	1.791718
-86.615281	-0.377500	1.796723
-86.956465	-7.227503	1.801728
-86.960745	4.760532	1.806733
-87.335468	-2.669514	1.811738
-87.387822	-0.516413	1.816742
-88.156575	-4.382431	1.821747
-88.644122	-1.553697	1.826752
-88.391250	-1.783279	1.831757
-88.675513	-7.493756	1.836762
-88.441250	-5.192577	1.841766
-88.858756	-3.915570	1.846771
-89.543015	-0.546646	1.851776
-89.795836	1.302508	1.856781
-89.879403	1.650827	1.861786
-89.696029	-5.822374	1.866790
-90.480631	-0.666021	1.871795
-91.010810	-3.984125	1.876800
-91.269032	-2.890264	1.881805
-91.224785	-5.953526	1.886810
-91.432761	-10.287063	1.891814
-91.887469	-3.749218	1.896819
-91.960316	-6.642272	1.901824
-91.620423	-9.637963	1.906829
-92.326327	-8.350567	1.911834
-92.768807	-8.066232	1.916838
-93.271666	3.999926	1.921843
-93.256235	7.398421	1.926848
-93.433580	3.468206	1.931853
-93.840062	-0.796264	1.936858
-93.738146	-5.722527	1.941862
-94.131315	7.920983	1.946867
-94.780461	1.049629	1.951872
-94.817906	0.150526	1.956877
-94.762681	8.101769	1.961882
-94.930233	1.502967	1.966886
-95.006821	2.884744	1.971891
-95.834517	-9.352844	1.976896
-96.238601	-5.771558	1.981901
-96.664977	7.070394	1.986906
-96.654257	-3.555337	1.991910
-96.565374	-0.617608	1.996915
-96.434680	-11.572774	2.006912
-96.873125	1.299961	2.016909
-96.358391	-3.662563	2.026906
-95.712236	-6.925556	2.036902
-95.285903	-6.257695	2.046899
-94.354174	-5.488459	2.056896
-93.994871	-8.063439	2.066893
-93.890504	-7.551035	2.076890
-93.433062	-7.889077	2.086886
-92.415477	-9.239890	2.096883
-92.461782	-6.654302	2.106880
-91.577362	-12.428690	2.116877
-91.056119	-8.085199	2.126874
-90.752829	-9.026313	2.136870
-90.204352	-9.194886	2.146867
-89.820134	-9.058953	2.156864
-89.271041	-5.736692	2.166861
-88.631172	-7.098012	2.176858
-88.347880	-6.626316	2.186854
-87.049911	-8.290326	2.196851
-86.894417	-8.406825	2.206848
-86.842937	-6.733051	2.216845
-86.669345	-8.955813	2.226842
-85.709920	-9.043058	2.236838
-85.326108	-16.867774	2.246835
-84.462081	-9.229616	2.256832
-84.529491	-11.389273	2.266829
-83.060760	-5.287220	2.276826
-82.974728	-1.965260	2.286822
-83.088131	-2.825243	2.296819
-82.223083	-8.359010	2.306816
-81.458706	-0.347271	2.316813
-81.474013	-5.952171	2.326810
-80.452409	-5.136828	2.336806
-80.217445	-2.959611	2.346803
-79.672993	2.409787	2.356800
-78.952847	-2.290316	2.366797
-78.748161	-2.154762	2.376794
-78.437316	-2.086527	2.386790
-77.350844	-4.268597	2.396787
-77.497289	-0.583925	2.406784
-76.461522	-6.828690	2.416781
-75.778207	-0.660587	2.426778
-75.664536	-2.012316	2.436774
-75.297085	-5.805013	2.446771
-74.653283	-2.931580	2.456768
-74.513843	-8.009528	2.466765
-73.365984	0.436304	2.476762
-73.272272	-1.517350	2.486758
-72.482369	-0.104998	2.496755
-71.683005	-4.101587	2.506752
-71.826566	-2.118483	2.516749
-71.641833	3.633566	2.526746
-70.717720	1.426251	2.536742
-70.121061	3.635495	2.546739
-69.187212	0.197543	2.556736
-68.990814	2.564538	2.566733
-68.828431	3.280095	2.576730
-68.127566	2.061274	2.586726
-67.277015	2.073453	2.596723
-67.369708	-2.062128	2.606720
-67.024752	5.720728	2.616717
-66.328211	-0.987240	2.626714
-65.407893	-2.199265	2.636710
-64.799975	4.969014	2.646707
-64.497236	4.357439	2.656704
-64.058246	0.971684	2.666701
-63.323170	-0.667482	2.676698
-63.171905	4.712842	2.686694
-62.808073	2.203677	2.696691
-62.169976	2.420208	2.706688
-61.735557	1.325499	2.716685
-61.094232	1.098031	2.726682
-60.350620	4.925178	2.736678
-59.992183	2.923708	2.746675
-59.921482	-1.665130	2.756672
-58.914804	0.071220	2.766669
-58.536662	2.621982	2.776666
-58.015692	2.334176	2.786662
-57.452021	0.056628	2.796659
-57.162666	3.077467	2.806656
-56.787910	1.472585	2.816653
-55.964135	5.607122	2.826650
-55.708993	3.083309	2.836646
-55.001544	4.017572	2.846643
-54.423874	-2.225108	2.856640
-54.559517	-3.024586	2.866637
-53.335291	1.094722	2.876634
-52.944784	6.168296	2.886630
-52.791391	-0.194806	2.896627
-51.909748	-3.048034	2.906624
-51.758582	-9.030646	2.916621
-51.196598	-4.253207	2.926618
-50.194591	-1.873057	2.936614
-50.023000	-1.957231	2.946611
-49.509522	-6.083254	2.956608
-48.764160	-6.095773	2.966605
-48.491487	0.082824	2.976602
-48.388535	-4.244972	2.986598
-47.842962	-2.648614	2.996595
-47.055569	-5.439556	3.006592
-46.450469	2.980452	3.016589
-45.848931	-1.628206	3.026586
-45.752467	1.879023	3.036582
-44.933838	1.177112	3.046579
-44.193125	-2.366792	3.056576
-44.197434	-1.666297	3.066573
-43.663047	-1.690108	3.076570
-42.784104	-1.204034	3.086566
-42.702354	-3.862237	3.096563
-42.273499	-11.323379	3.106560
-41.347760	-6.634613	3.116557
-41.212148	-12.370866	3.126554
-40.785102	5.022951	3.136550
-39.964480	3.807542	3.146547
-39.507300	-0.461716	3.156544
-38.407694	-6.380693	3.166541
-38.129927	-10.362076	3.176538
-38.071371	3.136045	3.186534
-37.746651	-5.113409	3.196531
-37.571040	1.580912	3.206528
-36.753962	4.908708	3.216525
-35.609944	-4.881965	3.226522
-35.218173	-8.266655	3.236518
-35.172357	-0.167662	3.246515
-34.605514	0.351474	3.256512
-33.831572	-3.089930	3.266509
-33.440799	-2.755449	3.276506
-33.253540	-3.266565	3.286502
-32.514144	-3.012051	3.296499
-32.170895	-7.127240	3.306496
-30.925456	-6.974190	3.316493
-31.176766	-0.998595	3.326490
-31.030326	-6.932951	3.336486
-29.983251	-2.906260	3.346483
-29.472072	-1.684650	3.356480
-29.085696	-5.404284	3.366477
-28.621331	1.526730	3.376474
-28.352922	-6.226056	3.386470
-27.011090	-5.587595	3.396467
-26.766147	-5.863827	3.406464
-26.478568	-2.627297	3.416461
-26.618982	-5.504115	3.426458
-25.662005	-2.876153	3.436454
-24.562779	-7.017925	3.446451
-24.090525	-5.761705	3.456448
-23.711186	0.751808	3.466445
-24.008024	-3.887149	3.476442
-23.231735	-4.861191	3.486438
-22.481559	-0.353989	3.496435
-22.066450	-3.393876	3.506432
-21.200952	-3.482237	3.516429
-20.955703	-1.354145	3.526426
-20.685399	-0.436917	3.536422
-19.681351	-0.315735	3.546419
-19.470562	-2.823094	3.556416
-19.224762	2.070415	3.566413
-18.141201	1.238297	3.576410
-17.939670	-3.979262	3.586406
-17.841391	2.787366	3.596403
-17.148516	-8.668580	3.606400
-16.469252	-1.048975	3.616397
-15.996704	-3.986989	3.626394
-15.371314	-3.993378	3.636390
-15.011672	2.060722	3.646387
-14.621621	-2.087143	3.656384
-13.634868	2.446350	3.666381
-13.702108	-2.032179	3.676378
-12.972763	-0.825743	3.686374
-12.332604	-3.112106	3.696371
-12.139181	3.392526	3.706368
-11.250018	-3.614885	3.716365
-10.777082	-1.085309	3.726362
-10.434091	4.616606	3.736358
-10.230020	0.124078	3.746355
-9.271666	0.379133	3.756352
-9.057075	2.730609	3.766349
-8.460120	-0.841454	3.776346
-7.824971	3.062882	3.786342
-7.381885	6.116658	3.796339
-7.116397	0.188989	3.806336
-6.362646	1.961808	3.816333
-6.224669	3.770921	3.826330
-5.360089	6.948726	3.836326
-4.930563	6.247595	3.846323
-4.642288	2.796756	3.856320
-3.940667	7.831093	3.866317
-3.922620	10.359085	3.876314
-3.304267	28.581436	3.886310
-2.692912	33.351155	3.896307
-1.850064	40.346431	3.906304
-1.909463	41.410355	3.916301
-1.389103	59.169751	3.926298
-1.126063	72.309603	3.936294
-0.515853	87.321113	3.946291
-0.080574	106.449718	3.956288
0.000000	117.625111	3.961293
0.310518	130.221984	3.966298
0.913341	144.070222	3.971302
0.997226	146.600633	3.976307
1.110397	148.395620	3.981312
0.913712	142.911815	3.986317
1.050035	148.097922	3.991322
1.275834	165.836603	3.996326
1.571537	165.011844	4.001331
1.429479	157.804697	4.006336
1.213903	156.471581	4.011341
1.404025	159.238453	4.016346
1.283846	171.681372	4.021350
1.555499	165.187696	4.026355
1.688361	172.585846	4.031360
1.006154	158.778230	4.036365
1.293040	159.948043	4.041370
1.470926	172.192399	4.046374
2.008712	166.818138	4.051379
1.693042	163.672030	4.056384
1.806041	159.598207	4.061389
1.630722	142.870096	4.066394
1.590309	147.441645	4.071398
1.318046	141.450820	4.076403
1.349614	146.865314	4.081408
1.271252	142.293124	4.086413
1.542711	147.543481	4.091418
1.669797	168.205155	4.096422
1.885160	166.760225	4.101427
1.483547	166.060542	4.106432
1.658802	167.928062	4.111437
1.847543	164.462474	4.116442
1.607988	155.176173	4.121446
1.718553	148.046509	4.126451
1.610637	152.884903	4.131456
1.773501	161.970978	4.136461
1.890541	156.456995	4.141466
1.491119	165.510947	4.146470
1.688706	165.774088	4.151475
1.795371	172.654317	4.156480
1.552417	174.451320	4.161485
1.862680	167.214429	4.166490
1.767930	177.422892	4.171494
1.694990	174.858856	4.176499
1.634125	176.421683	4.181504
1.627571	174.967229	4.186509
1.941624	170.216487	4.191514
1.684041	178.349704	4.196518
1.955873	173.001291	4.201523
2.001089	173.183901	4.206528
1.717773	178.372491	4.211533
1.829956	176.146449	4.216538
1.816712	175.433372	4.221542
1.673332	163.161193	4.226547
1.636480	174.746325	4.231552
1.770583	171.308280	4.236557
1.995395	175.600996	4.241562
1.606858	173.595779	4.246566
2.165724	168.047369	4.251571
1.844089	169.973760	4.256576
1.358275	180.230843	4.261581
1.927687	181.008373	4.266586
2.142469	197.862948	4.271590
2.284962	206.135976	4.276595
2.348883	188.402215	4.281600
1.589081	186.901262	4.286605
2.185588	188.114316	4.291610
2.400928	198.498836	4.296614
2.180894	181.230358	4.301619
2.068940	175.293498	4.306624
2.203130	177.249712	4.311629
1.894307	177.544741	4.316634
1.955315	187.273219	4.321638
2.338653	190.044624	4.326643
2.388894	197.101384	4.331648
1.877164	186.570044	4.336653
2.378253	195.470262	4.341658
2.275452	195.432450	4.346662
2.449569	196.151692	4.351667
2.169556	184.024294	4.356672
2.038045	175.860021	4.361677
2.451752	181.730351	4.366682
2.162915	191.320654	4.371686
2.438687	194.371508	4.376691
2.461953	202.467059	4.381696
2.499768	183.392777	4.386701
2.521102	175.859462	4.391706
1.989702	183.459772	4.396710
2.167619	175.721587	4.401715
2.051905	188.872509	4.406720
2.218586	189.469528	4.411725
2.771904	191.809334	4.416730
2.612511	208.130914	4.421734
2.645154	196.830894	4.426739
2.417592	189.475777	4.431744
2.396471	199.805597	4.436749
2.516192	196.426748	4.441754
2.138885	199.165471	4.446758
2.271969	194.550646	4.451763
2.568146	193.852364	4.456768
2.310860	205.459399	4.461773
2.653350	193.107909	4.466778
2.429021	203.491716	4.471782
2.490480	203.535737	4.476787
2.570061	201.609034	4.481792
2.379066	211.731356	4.486797
2.584339	199.622826	4.491802
2.251019	205.853822	4.496806
2.421711	203.783127	4.501811
2.475721	207.156636	4.506816
2.348662	208.723509	4.511821
2.628774	199.453840	4.516826
2.427382	211.735503	4.521830
2.589801	206.932578	4.526835
2.642144	202.928361	4.531840
2.354035	209.348430	4.536845
2.757185	213.629032	4.541850
2.765234	226.238563	4.546854
2.949358	233.078205	4.551859
3.204044	226.036662	4.556864
2.650537	209.301304	4.561869
2.441224	209.147301	4.566874
2.528217	212.746600	4.571878
2.700628	219.875978	4.576883
3.104071	217.787797	4.581888
3.016438	220.617180	4.586893
3.275863	215.235897	4.591898
2.478712	206.381788	4.596902
2.555039	205.822357	4.601907
2.711042	215.779580	4.606912
2.564022	233.491318	4.611917
3.061670	231.926223	4.616922
2.705037	231.013842	4.621926
2.873694	225.089948	4.626931
2.693934	228.806976	4.631936
2.807541	229.089604	4.636941
3.009550	226.722930	4.641946
2.862400	234.838869	4.646950
3.103088	229.017585	4.651955
3.115601	223.488321	4.656960
3.063185	233.000474	4.661965
2.812910	226.942898	4.666970
3.479514	234.918683	4.671974
3.328200	231.227947	4.676979
3.435317	237.636723	4.681984
3.060822	238.815253	4.686989
3.323354	237.075021	4.691994
2.772453	226.049913	4.696998
2.773100	229.257777	4.702003
2.890675	228.888039	4.707008
2.918522	224.609239	4.712013
3.008901	218.650155	4.717018
2.797734	231.202286	4.722022
2.804516	236.279000	4.727027
3.124259	231.505204	4.732032
2.937554	236.261052	4.737037
2.945334	231.200771	4.742042
3.097520	253.291816	4.747046
3.515745	256.342508	4.752051
3.738837	252.510846	4.757056
3.281014	244.476763	4.762061
3.154154	236.862236	4.767066
2.915102	236.633797	4.772070
3.460574	247.387407	4.777075
3.846394	249.914819	4.782080
3.186346	245.753286	4.787085
3.038110	231.621500	4.792090
3.425242	233.237528	4.797094
3.484004	239.960770	4.802099
3.281296	231.949997	4.807104
3.252679	240.563068	4.812109
3.541211	245.301405	4.817114
3.395836	244.298975	4.822118
3.282470	251.466813	4.827123
3.160885	249.154002	4.832128
3.371652	257.761212	4.837133
3.594209	255.214141	4.842138
3.590900	256.480050	4.847142
3.503361	253.551287	4.852147
3.587063	253.237477	4.857152
3.092393	255.918665	4.862157
3.398186	253.127595	4.867162
3.433938	258.743952	4.872166
3.005028	267.217270	4.877171
3.417880	254.664883	4.882176
3.156649	255.525106	4.887181
3.348148	246.759687	4.892186
3.668045	260.101843	4.897190
3.431300	258.686613	4.902195
3.645307	260.601856	4.907200
3.562051	261.744247	4.912205
3.908238	264.281035	4.917210
3.773275	253.592544	4.922214
3.914189	257.313120	4.927219
3.827430	257.965670	4.932224
3.568357	261.790047	4.937229
3.492898	253.338540	4.942234
3.360744	257.168341	4.947238
3.808750	276.704163	4.952243
3.745626	273.141973	4.957248
3.586621	271.980322	4.962253
3.931928	275.846050	4.967258
3.909623	270.119744	4.972262
3.852584	268.527657	4.977267
3.725425	261.080848	4.982272
3.772781	273.478606	4.987277
4.307165	277.064769	4.992282
3.578053	270.718364	4.997286
3.778283	265.485549	5.002291
4.281809	265.238840	5.007296
3.786223	269.748857	5.012301
3.600769	263.646311	5.017306
3.819499	269.610496	5.022310
3.765197	271.539305	5.027315
4.383052	283.195937	5.032320
3.872043	276.353441	5.037325
4.102426	277.434037	5.042330
3.913142	269.351540	5.047334
4.062074	271.817993	5.052339
4.305030	265.531260	5.057344
3.658391	262.611001	5.062349
3.850434	268.611006	5.067354
4.077754	274.959831	5.072358
4.026761	276.483154	5.077363
4.286419	288.635684	5.082368
4.031910	287.615548	5.087373
4.138143	283.153607	5.092378
4.194263	290.234793	5.097382
3.928537	281.015803	5.102387
4.053901	279.635586	5.107392
3.991307	279.085264	5.112397
4.269665	276.326963	5.117402
4.385910	286.973839	5.122406
4.324109	280.551350	5.127411
4.056726	288.357115	5.132416
4.143649	288.242119	5.137421
4.162505	285.021430	5.142426
4.162517	287.786469	5.147430
4.218690	282.550910	5.152435
4.346735	281.163945	5.157440
4.282137	287.833766	5.162445
4.730665	280.195507	5.167450
3.974701	286.850263	5.172454
4.118589	289.551631	5.177459
4.564400	293.986923	5.182464
4.333617	290.498455	5.187469
4.114878	287.343466	5.192474
4.363555	294.252112	5.197478
4.125110	293.235787	5.202483
4.492559	287.309199	5.207488
4.018385	285.839417	5.212493
4.460383	280.549733	5.217498
4.333551	291.301138	5.222502
4.289700	293.535202	5.227507
4.294216	286.219615	5.232512
4.199402	292.486039	5.237517
4.699583	291.433080	5.242522
4.193185	291.002915	5.247526
4.273836	289.294338	5.252531
4.248928	289.415168	5.257536
4.097271	282.766307	5.262541
4.174804	284.294803	5.267546
4.544268	306.041816	5.272550
4.788225	305.468773	5.277555
4.651522	313.896330	5.282560
4.434889	315.739844	5.287565
4.951121	311.077613	5.292570
4.772397	303.936265	5.297574
4.570609	292.584327	5.302579
4.845591	291.867216	5.307584
4.559425	294.822631	5.312589
4.616141	290.216584	5.317594
4.447669	293.419319	5.322598
4.393600	307.949587	5.327603
4.661967	313.393470	5.332608
4.672191	312.442588	5.337613
4.943493	303.449498	5.342618
4.600688	316.003331	5.347622
4.763388	311.928013	5.352627
5.127049	308.438155	5.357632
4.602778	318.261570	5.362637
4.821885	306.764582	5.367642
4.670027	321.509503	5.372646
4.784352	319.716552	5.377651
5.000590	310.102486	5.382656
4.754198	313.839464	5.387661
4.900505	314.917416	5.392666
5.015099	320.296808	5.397670
4.631316	317.338519	5.402675
5.179376	301.718154	5.407680
4.542360	309.107270	5.412685
4.883426	303.466391	5.417690
4.864063	302.994718	5.422694
4.834667	318.732872	5.427699
5.192081	312.529432	5.432704
4.771576	319.179096	5.437709
4.939516	307.408544	5.442714
4.576901	317.810921	5.447718
5.263679	317.155841	5.452723
4.997072	319.551363	5.457728
4.865073	321.568283	5.462733
5.136241	309.202576	5.467738
4.967182	317.647859	5.472742
4.931325	309.465373	5.477747
5.050822	306.538966	5.482752
4.994692	310.410651	5.487757
4.639726	310.440823	5.492762
4.699345	312.022750	5.497766
4.609125	324.094078	5.502771
4.702232	318.466734	5.507776
5.203145	330.733356	5.512781
5.191359	329.460047	5.517786
5.230522	335.325836	5.522790
5.056496	340.851698	5.527795
5.292308	338.574628	5.532800
5.134124	347.976861	5.537805
5.025682	335.442818	5.542810
5.095535	333.694799	5.547814
5.121570	336.895541	5.552819
5.302475	339.467728	5.557824
4.905949	341.858298	5.562829
5.318454	336.222035	5.567834
5.234231	341.654731	5.572838
5.200807	349.597876	5.577843
4.811758	332.963187	5.582848
5.010531	343.499087	5.587853
5.272286	343.318733	5.592858
5.006073	347.068315	5.597862
5.245604	358.132525	5.602867
5.372807	352.433388	5.607872
5.341459	358.794298	5.612877
5.438221	360.209054	5.617882
5.452350	363.016187	5.622886
5.214120	370.564314	5.627891
5.375672	364.929395	5.632896
5.348945	367.619541	5.637901
5.563808	361.612430	5.642906
5.550263	366.214628	5.647910
5.565829	374.501294	5.652915
5.523284	368.983775	5.657920
5.538005	366.320553	5.662925
5.808116	366.781147	5.667930
5.889779	358.978868	5.672934
5.495858	365.583255	5.677939
5.407335	357.766511	5.682944
5.298347	364.101622	5.687949
5.540101	367.078740	5.692954
5.486042	368.093175	5.697958
5.411802	373.695163	5.702963
5.446794	362.195348	5.707968
5.406780	366.823840	5.712973
5.441150	365.780585	5.717978
5.223181	364.938221	5.722982
5.397445	366.011796	5.727987
5.716343	364.651871	5.732992
5.233622	373.200111	5.737997
5.658040	370.944107	5.743002
5.847413	385.502735	5.748006
5.897362	379.863151	5.753011
5.918301	380.831033	5.758016
5.337469	375.885083	5.763021
5.755105	382.052264	5.768026
5.991631	391.202846	5.773030
5.965747	389.849482	5.778035
5.924789	386.296452	5.783040
6.002096	377.994961	5.788045
5.684116	368.100725	5.793050
5.842833	371.350288	5.798054
5.682031	384.701413	5.803059
6.138438	383.592031	5.808064
5.632084	381.352143	5.813069
5.873448	383.395995	5.818074
6.127058	392.654635	5.823078
5.864762	385.994595	5.828083
6.245468	381.410530	5.833088
6.079310	386.194836	5.838093
5.773624	375.488727	5.843098
5.887778	383.677691	5.848102
6.075808	385.498939	5.853107
6.052591	382.237366	5.858112
5.805500	388.227119	5.863117
5.738924	385.355163	5.868122
5.837285	386.143231	5.873126
5.957501	384.994773	5.878131
5.948560	378.674701	5.883136
5.858107	389.711536	5.888141
5.927177	385.673019	5.893146
5.872831	385.548519	5.898150
6.075562	384.099223	5.903155
5.911612	380.612922	5.908160
5.552857	390.359822	5.913165
6.034802	386.585654	5.918170
6.181894	400.875666	5.923174
6.375200	406.495858	5.928179
6.218071	404.147465	5.933184
6.137881	413.724179	5.938189
6.126072	407.784206	5.943194
6.040955	406.006676	5.948198
5.954311	414.138527	5.953203
6.287868	402.740607	5.958208
6.475887	417.865801	5.963213
6.318309	420.911824	5.968218
6.101003	408.888346	5.973222
6.014536	414.523901	5.978227
6.400439	414.969518	5.983232
6.928189	418.129631	5.988237
6.596499	406.304415	5.993242
6.005198	403.438739	5.998246
6.178321	399.298491	6.003251
6.536953	395.591099	6.008256
6.217144	405.205352	6.013261
6.147467	394.610955	6.018266
6.238164	394.663051	6.023270
6.119257	386.559983	6.028275
6.431824	400.865198	6.033280
6.252637	405.999572	6.038285
5.924586	409.176710	6.043290
6.692881	412.802184	6.048294
6.330853	409.811996	6.053299
6.622240	400.499327	6.058304
6.096452	404.134563	6.063309
6.067224	388.905137	6.068314
5.805882	398.117910	6.073318
6.315585	419.374841	6.078323
6.799336	408.352029	6.083328
6.369385	411.178127	6.088333
6.609744	394.669396	6.093338
6.219971	393.616662	6.098342
6.328027	382.513521	6.103347
6.567258	387.326062	6.108352
6.219735	394.100364	6.113357
6.560909	386.750971	6.118362
6.213770	381.189422	6.123366
5.908773	393.310268	6.128371
6.141386	384.367493	6.133376
6.048858	387.558346	6.138381
6.095098	384.839561	6.143386
6.237500	389.872923	6.148390
5.795598	393.254562	6.153395
6.519487	396.361793	6.158400
6.315830	393.884647	6.163405
6.108127	392.002935	6.168410
6.376919	388.034368	6.173414
6.107335	402.592152	6.178419
6.561410	396.721560	6.183424
6.394969	387.290800	6.188429
6.085375	383.972854	6.193434
6.467094	381.432467	6.198438
6.169650	388.088186	6.203443
6.541945	379.332341	6.208448
6.446144	389.711938	6.213453
6.395732	392.643086	6.218458
6.493939	380.671434	6.223462
6.300163	393.992930	6.228467
6.236438	381.777724	6.233472
6.375029	388.434729	6.238477
6.205753	388.315581	6.243482
6.376664	388.386748	6.248486
6.161222	393.412901	6.253491
6.289019	388.884279	6.258496
5.926851	391.959188	6.263501
6.341994	387.907577	6.268506
6.542058	386.439716	6.273510
6.226013	396.448854	6.278515
6.240091	390.789576	6.283520
6.396232	382.912341	6.288525
6.269411	379.714459	6.293530
6.094588	382.763177	6.298534
5.730565	379.051953	6.303539
6.319070	381.088871	6.308544
5.724742	382.779593	6.313549
5.863188	392.296728	6.318554
6.096896	398.087763	6.323558
6.074411	409.215204	6.328563
6.436223	406.431152	6.333568
6.517162	408.003420	6.338573
6.453299	402.919513	6.343578
6.502364	403.117341	6.348582
6.348890	398.386007	6.353587
6.073136	392.936659	6.358592
5.865066	400.571824	6.363597
6.179325	402.708663	6.368602
6.470653	415.147389	6.373606
6.289102	418.371179	6.378611
6.427209	413.572009	6.383616
6.193275	423.878353	6.388621
6.286943	417.130890	6.393626
6.433281	418.148731	6.398630
6.288755	409.015091	6.403635
5.871164	392.264593	6.408640
6.495173	408.767341	6.413645
6.202088	414.843404	6.418650
6.287154	412.017289	6.423654
6.300975	410.727307	6.428659
6.776153	415.566164	6.433664
6.140806	401.823784	6.438669
5.984433	401.604536	6.443674
6.161386	402.443568	6.448678
6.052034	411.648353	6.453683
6.457040	405.377311	6.458688
6.270230	420.618185	6.463693
6.429005	408.330133	6.468698
6.463058	409.419352	6.473702
5.995573	407.413822	6.478707
6.398751	403.727924	6.483712
5.908485	402.513760	6.488717
6.453455	413.859186	6.493722
6.671041	408.623610	6.498726
6.096452	396.111940	6.503731
6.200728	404.565059	6.508736
5.808484	409.096885	6.513741
6.258474	417.394601	6.518746
6.548655	413.277139	6.523750
6.237399	422.706559	6.528755
6.530755	419.952214	6.533760
6.291454	418.714547	6.538765
6.022650	418.857772	6.543770
6.274913	412.816309	6.548774
6.424408	417.158851	6.553779
6.330856	401.404804	6.558784
5.979179	408.347446	6.563789
6.305280	415.933725	6.568794
6.697221	416.087323	6.573798
6.134463	411.831411	6.578803
6.212578	395.487309	6.583808
5.999054	401.819829	6.588813
6.015721	408.976848	6.593818
5.937997	414.047870	6.598822
6.278720	415.098531	6.603827
6.365933	413.547107	6.608832
6.051383	432.993765	6.613837
6.321112	426.721765	6.618842
6.195630	419.774514	6.623846
6.056838	418.024376	6.628851
6.152954	425.017089	6.633856
6.347598	419.392788	6.638861
6.394440	424.681584	6.643866
6.267927	415.295175	6.648870
6.292354	417.429969	6.653875
6.573566	420.540123	6.658880
6.418305	426.021941	6.663885
6.668469	424.821482	6.668890
6.780066	423.772450	6.673894
5.833114	410.515497	6.678899
6.175589	399.492678	6.683904
6.473805	421.076984	6.688909
6.224128	403.746494	6.693914
6.123308	406.596955	6.698918
6.077838	412.925294	6.703923
6.337226	408.913902	6.708928
5.773816	419.246555	6.713933
6.239203	411.744808	6.718938
6.408341	414.505516	6.723942
6.213077	421.376198	6.728947
6.219826	420.520770	6.733952
6.480309	419.461067	6.738957
6.408921	416.143758	6.743962
6.731707	417.295309	6.748966
6.059113	411.427229	6.753971
6.330952	403.506546	6.758976
6.233646	408.969787	6.763981
6.247142	412.827422	6.768986
6.457197	416.012001	6.773990
6.062670	414.184870	6.778995
6.415216	407.226002	6.784000
6.294336	415.280959	6.789005
6.336529	406.731849	6.794010
6.239284	402.646618	6.799014
6.148526	401.439463	6.804019
6.401004	407.607220	6.809024
6.007128	412.189924	6.814029
6.134948	404.187399	6.819034
6.812249	407.719559	6.824038
6.395286	398.065447	6.829043
6.405564	391.650607	6.834048
6.150377	395.623104	6.839053
6.032550	388.573423	6.844058
6.032951	389.917856	6.849062
5.759882	408.231663	6.854067
6.255317	408.112774	6.859072
6.195263	415.547579	6.864077
6.230194	415.953271	6.869082
6.483201	412.493386	6.874086
5.931821	419.970372	6.879091
6.411719	415.152451	6.884096
6.299847	418.472894	6.889101
6.297605	417.818196	6.894106
6.661324	415.935539	6.899110
6.452114	415.993495	6.904115
6.688703	404.455739	6.909120
6.260191	398.407048	6.914125
5.940793	391.132677	6.919130
6.072726	390.112100	6.924134
6.114235	403.709958	6.929139
6.470921	421.032906	6.934144
6.443817	423.188430	6.939149
6.378067	400.672065	6.944154
6.314756	395.983554	6.949158
6.076311	396.675694	6.954163
6.380208	396.615289	6.959168
5.860808	400.113479	6.964173
6.539471	407.131973	6.969178
6.304032	406.738446	6.974182
6.155851	407.058930	6.979187
6.338387	399.731223	6.984192
6.412924	416.035324	6.989197
6.225794	409.423612	6.994202
6.550000	397.451342	6.999206
5.980290	394.889176	7.004211
6.428993	388.196831	7.009216
6.177270	391.880876	7.014221
6.112536	381.684354	7.019226
6.153619	394.633686	7.024230
6.450918	410.554858	7.029235
6.662821	396.977135	7.034240
6.398573	391.649374	7.039245
6.271889	387.318816	7.044250
6.295611	388.292590	7.049254
5.871485	392.323194	7.054259
5.899485	387.525463	7.059264
6.713193	395.437142	7.064269
6.466624	394.811235	7.069274
6.385478	385.518976	7.074278
6.275083	399.808201	7.079283
6.554924	394.521745	7.084288
6.304048	388.799574	7.089293
6.440967	389.591093	7.094298
6.763261	388.297075	7.099302
6.475510	399.342682	7.104307
6.373527	388.240809	7.109312
6.309809	396.789850	7.114317
6.384863	386.141142	7.119322
6.160119	389.634293	7.124326
6.275717	392.795701	7.129331
6.369003	390.452368	7.134336
6.183960	385.450730	7.139341
5.957680	392.873604	7.144346
6.309632	393.957307	7.149350
6.190771	397.117485	7.154355
6.487209	402.335529	7.159360
6.427926	390.233519	7.164365
6.213997	392.019669	7.169370
6.538039	386.587080	7.174374
6.385674	395.703682	7.179379
6.219952	398.330187	7.184384
6.227562	389.324584	7.189389
6.300586	403.942587	7.194394
6.368220	377.501177	7.199398
6.170767	389.393194	7.204403
6.410189	388.896791	7.209408
6.377370	395.200995	7.214413
6.133005	395.093612	7.219418
6.162403	379.358287	7.224422
6.131816	394.479746	7.229427
6.104628	403.016739	7.234432
6.339636	398.281486	7.239437
6.204366	395.913850	7.244442
6.135063	391.428764	7.249446
6.074102	385.468026	7.254451
6.131760	384.117392	7.259456
6.588513	389.174269	7.264461
6.243774	398.305194	7.269466
6.352348	393.877661	7.274470
5.959278	399.418878	7.279475
6.264379	385.168483	7.284480
6.028789	389.362540	7.289485
6.026526	386.395084	7.294490
6.420668	382.786537	7.299494
6.328927	383.332302	7.304499
6.477889	390.671071	7.309504
6.398542	391.705288	7.314509
6.105664	391.798500	7.319514
6.169686	392.930479	7.324518
5.959948	392.333604	7.329523
5.966855	390.946628	7.334528
6.170140	393.746276	7.339533
5.907704	395.508388	7.344538
5.974839	383.772562	7.349542
6.109374	389.332353	7.354547
6.013781	404.435532	7.359552
6.407357	406.031583	7.364557
6.449477	407.695356	7.369562
6.214897	407.083390	7.374566
6.366139	415.215935	7.379571
6.381814	400.150312	7.384576
6.314425	383.053879	7.389581
6.203268	393.938934	7.394586
6.172924	390.580397	7.399590
6.164899	402.993250	7.404595
6.481504	397.868716	7.409600
6.157473	389.576316	7.414605
6.048793	390.795468	7.419610
6.346549	400.876120	7.424614
6.268334	410.357608	7.429619
6.584834	409.298620	7.434624
6.329344	397.167234	7.439629
6.259912	397.437413	7.444634
6.553080	395.486716	7.449638
5.912171	386.228376	7.454643
5.708373	387.247290	7.459648
6.390703	405.354452	7.464653
6.425373	409.708655	7.469658
6.478574	402.277822	7.474662
6.310838	401.649054	7.479667
6.192264	391.808985	7.484672
6.522805	387.517523	7.489677
5.810325	396.085953	7.494682
6.394011	396.408829	7.499686
6.279609	407.999936	7.504691
6.206482	393.381678	7.509696
6.279254	402.077019	7.514701
6.026891	404.043203	7.519706
5.982079	402.629527	7.524710
6.288717	410.582695	7.529715
6.565749	411.769889	7.534720
6.465400	413.250335	7.539725
6.270132	411.774808	7.544730
6.340267	399.611385	7.549734
6.193089	396.638158	7.554739
6.185212	403.612354	7.559744
6.572057	411.173295	7.564749
6.232597	400.962858	7.569754
6.410679	389.690549	7.574758
6.018413	394.266669	7.579763
6.251417	389.898737	7.584768
6.433255	383.966397	7.589773
6.323219	394.538057	7.594778
6.217055	385.800225	7.599782
6.406853	390.724919	7.604787
6.380616	392.219062	7.609792
6.373506	395.304782	7.614797
6.506815	389.819817	7.619802
6.413025	387.179921	7.624806
6.321748	395.793392	7.629811
6.406956	388.613821	7.634816
6.001551	391.619573	7.639821
5.980921	396.251363	7.644826
6.186487	393.419026	7.649830
5.901986	395.396571	7.654835
6.608407	387.385658	7.659840
6.443580	389.078690	7.664845
6.087902	396.525004	7.669850
6.537768	390.291233	7.674854
6.273272	390.174349	7.679859
6.205742	387.925817	7.684864
6.272025	381.964126	7.689869
6.048461	387.168725	7.694874
6.692989	381.056321	7.699878
6.285919	385.248771	7.704883
6.279722	382.009842	7.709888
5.972854	382.234963	7.714893
6.070630	379.909911	7.719898
6.297305	394.624058	7.724902
6.005602	389.155063	7.729907
6.249030	394.356100	7.734912
6.014681	391.355402	7.739917
6.127353	390.726994	7.744922
6.180018	395.935773	7.749926
6.579480	404.611569	7.754931
6.468539	392.144318	7.759936
6.317283	388.545292	7.764941
6.113906	388.934537	7.769946
6.287414	383.168022	7.774950
6.176704	397.017521	7.779955
6.345775	395.412143	7.784960
6.311756	393.405139	7.789965
6.323656	392.102804	7.794970
6.345833	385.024861	7.799974
6.246490	391.564120	7.804979
6.180411	391.982474	7.809984
6.295114	388.148783	7.814989
6.145523	389.361689	7.819994
6.427539	384.008454	7.824998
6.413749	393.812041	7.830003
6.082914	385.631444	7.835008
6.419787	389.669367	7.840013
6.098990	393.117455	7.845018
6.253280	387.442537	7.850022
6.094219	391.314548	7.855027
6.575278	379.463250	7.860032
6.496072	389.425785	7.865037
6.187405	395.605526	7.870042
6.484381	386.896281	7.875046
5.939233	386.620884	7.880051
6.022617	385.446558	7.885056
6.651813	386.648177	7.890061
6.176366	392.854049	7.895066
6.333154	379.825990	7.900070
6.035140	394.046527	7.905075
6.429370	385.337864	7.910080
6.139329	390.252315	7.915085
5.937696	391.011456	7.920090
6.307766	390.776164	7.925094
6.284950	397.638801	7.930099
6.099054	394.984860	7.935104
6.621078	400.601004	7.940109
6.357872	400.901544	7.945114
6.413124	389.797181	7.950118
6.089790	393.606343	7.955123
6.139899	390.646500	7.960128
6.378628	386.383466	7.965146
6.007946	396.991131	7.970163
6.275803	396.728125	7.975181
6.410561	404.122926	7.980198
6.081774	397.607158	7.985216
6.272090	408.414106	7.990234
6.421615	410.419703	7.995251
6.304111	400.557273	8.000269
6.362900	415.875489	8.005286
6.143625	405.501989	8.010304
5.936513	406.269599	8.015322
6.669644	424.366537	8.020339
6.688970	407.931288	8.025357
6.217472	394.962247	8.030374
6.118099	399.051776	8.035392
6.397412	405.789620	8.040410
6.305873	417.073075	8.045427
6.451161	417.936947	8.050445
6.817191	413.846391	8.055462
6.150894	413.347901	8.060480
6.237623	394.582614	8.065498
6.251063	409.791166	8.070515
6.708604	410.066479	8.075533
6.643891	399.959096	8.080550
6.316862	405.952509	8.085568
6.476539	397.697118	8.090586
6.171867	398.076075	8.095603
6.224839	398.749287	8.100621
6.318468	398.447308	8.105638
6.326025	410.677741	8.110656
6.648300	404.568039	8.115674
6.206226	408.177940	8.120691
6.503466	414.745723	8.125709
6.173821	409.732230	8.130726
5.901566	423.909441	8.135744
6.803860	422.048040	8.140762
6.798345	414.484392	8.145779
6.882933	419.229903	8.150797
6.650968	399.406869	8.155814
6.698285	404.123503	8.160832
6.589549	388.049159	8.165850
6.113636	399.083562	8.170867
6.226361	396.698942	8.175885
6.218443	398.640844	8.180902
6.248397	408.384179	8.185920
6.924004	414.397223	8.190938
6.720381	407.331671	8.195955
6.522878	394.010437	8.200973
6.397576	398.675221	8.205990
6.224006	401.586652	8.211008
6.447196	406.685980	8.216026
6.317976	412.137168	8.221043
6.533577	410.405450	8.226061
6.829837	417.440441	8.231078
6.268533	421.908460	8.236096
6.507717	417.667365	8.241114
6.459535	422.149661	8.246131
6.589812	413.507554	8.251149
6.368509	418.938458	8.256166
6.271830	421.698991	8.261184
6.638700	411.653367	8.266202
5.967573	422.525869	8.271219
5.945359	419.941484	8.276237
6.139054	425.272654	8.281254
6.263368	435.392535	8.286272
7.347178	446.349844	8.291290
6.826277	434.537217	8.296307
6.691824	416.052712	8.301325
6.768572	419.171075	8.306342
6.590791	415.762164	8.311360
7.134477	418.958844	8.316378
6.690723	420.798624	8.321395
6.863709	417.334753	8.326413
6.828986	415.623321	8.331430
6.670486	417.882305	8.336448
6.792952	415.461443	8.341466
6.900740	416.328035	8.346483
6.854406	410.061494	8.351501
7.069631	415.708020	8.356518
6.683767	409.671400	8.361536
6.754379	410.105165	8.366554
6.585533	416.389374	8.371571
6.906188	411.384443	8.376589
6.888444	412.040333	8.381606
6.525754	398.543007	8.386624
6.865950	404.883153	8.391642
6.603269	405.678404	8.396659
6.943700	391.035826	8.401677
6.714513	397.278991	8.406694
6.235746	396.498658	8.411712
6.796316	403.530100	8.416730
6.706811	410.530858	8.421747
6.633595	411.662493	8.426765
7.018497	412.990590	8.431782
6.798432	412.311731	8.436800
6.923281	415.596125	8.441818
6.978326	419.601504	8.446835
6.685531	406.266789	8.451853
6.685392	398.206850	8.456870
6.693395	415.316030	8.461888
6.800735	416.223718	8.466906
6.530267	415.287672	8.471923
6.395375	420.755530	8.476941
6.625667	413.789245	8.481958
6.268607	415.101051	8.486976
6.450775	415.921276	8.491994
6.536782	417.403501	8.497011
6.755550	418.953286	8.502029
6.803435	424.673371	8.507046
6.481253	420.542321	8.512064
6.970985	433.571370	8.517082
7.183844	438.823803	8.522099
6.784358	433.534071	8.527117
7.231735	423.371687	8.532134
6.530892	414.613650	8.537152
6.762475	420.235524	8.542170
6.575720	422.808201	8.547187
6.768724	429.521708	8.552205
7.313800	433.144202	8.557223
7.067347	433.321536	8.562240
6.833712	424.954190	8.567258
6.738499	423.072356	8.572275
7.077911	433.332101	8.577293
7.172638	425.279377	8.582311
6.868969	426.642778	8.587328
7.188729	421.931471	8.592346
6.806241	414.483690	8.597363
6.828546	417.089882	8.602381
7.215178	417.950654	8.607399
6.751669	422.119332	8.612416
6.738277	411.719882	8.617434
6.707531	431.968827	8.622451
6.956841	439.743322	8.627469
6.895365	441.324395	8.632487
7.009534	443.105163	8.637504
7.082574	436.119327	8.642522
7.369843	443.616480	8.647539
7.010974	433.586725	8.652557
7.117574	426.573544	8.657575
6.791037	428.802053	8.662592
7.210485	422.361543	8.667610
6.887303	423.863700	8.672627
6.815171	427.740686	8.677645
7.318307	434.689622	8.682663
7.191299	437.637944	8.687680
6.587727	428.990891	8.692698
6.701559	440.633498	8.697715
7.039361	453.042589	8.702733
7.332628	445.126004	8.707751
6.929960	451.541533	8.712768
7.221431	450.419612	8.717786
7.254261	449.069974	8.722803
7.019457	444.537068	8.727821
7.125708	437.580741	8.732839
7.362918	442.633702	8.737856
7.144073	439.515240	8.742874
7.139850	433.854312	8.747891
7.109483	438.602061	8.752909
7.393014	440.113299	8.757927
6.759163	444.589534	8.762944
7.042898	432.657149	8.767962
7.046147	443.247278	8.772979
7.029638	438.869517	8.777997
7.296615	442.077999	8.783015
7.464226	442.102095	8.788032
7.314028	434.378073	8.793050
7.000816	431.750918	8.798067
7.358469	438.646912	8.803085
7.457145	439.363457	8.808103
7.064121	435.038378	8.813120
6.921721	418.985060	8.818138
7.245797	429.146221	8.823155
7.091947	435.352348	8.828173
7.233892	440.126748	8.833191
7.094833	457.987995	8.838208
7.235519	442.417316	8.843226
7.125981	440.338911	8.848243
7.212707	448.075768	8.853261
7.139489	442.586592	8.858279
7.158945	444.694622	8.863296
7.311612	446.399931	8.868314
7.596959	431.674434	8.873331
7.470702	440.170486	8.878349
7.133160	436.202784	8.883367
7.140959	441.326402	8.888384
7.212156	442.299714	8.893402
7.326029	438.690468	8.898419
7.022872	443.730266	8.903437
7.311506	439.522443	8.908455
6.861745	441.407347	8.913472
6.964132	445.812410	8.918490
7.217468	446.391114	8.923507
7.243438	444.872140	8.928525
7.514406	444.801148	8.933543
7.033823	450.424163	8.938560
7.159689	438.854176	8.943578
7.013185	439.340895	8.948595
7.097056	452.146373	8.953613
7.378327	455.614547	8.958631
7.332572	466.565814	8.963648
7.286706	456.370240	8.968666
7.788427	458.888700	8.973683
7.336461	458.344003	8.978701
7.330778	449.833633	8.983719
7.079830	459.854536	8.988736
7.300669	469.659514	8.993754
7.431393	462.260690	8.998771
7.173029	477.710701	9.003789
7.349951	465.309039	9.008807
7.203770	468.140450	9.013824
7.278891	471.524163	9.018842
7.296345	461.823590	9.023859
7.418232	471.887068	9.028877
7.666543	469.266601	9.033895
7.773751	470.868584	9.038912
7.586731	465.422477	9.043930
7.612928	466.655303	9.048947
7.452680	476.040315	9.053965
7.691099	475.258061	9.058983
7.536330	469.838458	9.064000
7.774274	462.526976	9.069018
7.929010	462.874979	9.074035
7.634153	457.294294	9.079053
7.467121	447.770955	9.084071
7.385747	438.934782	9.089088
7.435177	444.342209	9.094106
7.451416	440.278050	9.099123
7.416346	461.909936	9.104141
7.641346	463.818507	9.109159
7.661112	460.179821	9.114176
7.872417	462.342999	9.119194
7.587477	443.553844	9.124211
7.367752	440.056826	9.129229
7.594228	453.117669	9.134247
7.582164	456.300447	9.139264
7.559107	460.744102	9.144282
7.570461	461.108259	9.149299
7.597107	463.152049	9.154317
8.040635	457.272638	9.159335
7.486189	448.870339	9.164352
7.321641	440.788804	9.169370
7.862487	449.884076	9.174387
7.392690	454.659654	9.179405
7.449864	457.613835	9.184423
7.669375	464.944890	9.189440
7.415845	462.822772	9.194458
7.365787	461.653376	9.199475
7.474621	475.385914	9.204493
7.525277	465.519191	9.209511
7.802139	467.978210	9.214528
7.539918	461.227928	9.219546
7.510977	458.209095	9.224563
7.448668	462.311765	9.229581
8.028753	466.859735	9.234599
7.654809	476.079415	9.239616
7.787383	473.956760	9.244634
7.679524	467.024502	9.249651
7.639965	469.854987	9.254669
7.441054	469.175968	9.259687
7.671883	469.897054	9.264704
7.317753	475.815842	9.269722
7.957232	472.256780	9.274739
7.981525	477.724960	9.279757
7.783339	466.193105	9.284775
7.820535	472.991000	9.289792
7.434033	467.585616	9.294810
7.738260	474.714055	9.299827
7.454992	487.835856	9.304845
7.804717	492.000207	9.309863
7.653393	500.203571	9.314880
7.607520	491.734191	9.319898
8.157488	488.997031	9.324915
8.262110	495.342561	9.329933
8.251120	498.301117	9.334951
8.125248	490.642686	9.339968
7.669039	470.378185	9.344986
7.700193	471.739621	9.350003
7.502867	474.086746	9.355021
7.766105	486.270858	9.360039
7.820332	487.638148	9.365056
7.552234	489.223197	9.370074
7.670433	494.054980	9.375091
8.028670	491.455156	9.380109
8.049411	494.837927	9.385127
7.555356	489.155899	9.390144
7.660618	494.008644	9.395162
8.176115	483.933381	9.400179
7.859876	491.629253	9.405197
7.702022	497.937015	9.410215
7.969048	495.708085	9.415232
8.017523	491.272793	9.420250
8.180206	489.615630	9.425267
7.491871	482.329350	9.430285
7.830487	493.327707	9.435303
8.048913	499.197819	9.440320
8.048585	492.157185	9.445338
7.871544	491.967041	9.450355
7.423339	502.063054	9.455373
7.520582	498.806694	9.460391
7.704784	505.818252	9.465408
8.347533	515.809613	9.470426
8.493475	518.147141	9.475443
8.209210	500.569642	9.480461
8.136138	508.890136	9.485479
8.192813	490.833197	9.490496
7.727465	490.555682	9.495514
7.924708	496.271323	9.500531
8.018354	497.433623	9.505549
7.977029	497.600908	9.510567
7.975826	510.899437	9.515584
7.910838	520.572502	9.520602
8.043607	518.913712	9.525619
8.274150	528.543634	9.530637
8.110233	531.803866	9.535655
8.611595	520.515819	9.540672
7.846067	516.331135	9.545690
8.405583	513.090705	9.550707
8.075804	506.840137	9.555725
7.953799	499.995289	9.560743
8.313375	514.587968	9.565760
8.266297	525.406936	9.570778
8.114022	506.666356	9.575795
8.280942	513.626977	9.580813
8.266729	508.074887	9.585831
7.884038	492.693464	9.590848
7.734811	515.933815	9.595866
7.929476	509.926123	9.600883
8.077404	528.376787	9.605901
8.229057	522.710342	9.610919
8.551758	522.807969	9.615936
8.441096	524.472495	9.620954
8.246919	516.032652	9.625971
8.421020	516.323974	9.630989
8.561713	528.732442	9.636007
8.394986	520.947856	9.641024
8.222104	511.368595	9.646042
8.122341	497.858401	9.651059
8.116620	516.134312	9.656077
8.217008	516.203655	9.661095
8.521827	520.015288	9.666112
8.155148	523.891108	9.671130
8.475538	523.054984	9.676147
8.092128	518.725223	9.681165
8.334309	527.513881	9.686183
8.426076	516.835963	9.691200
8.833715	523.765184	9.696218
8.419072	513.955559	9.701235
8.163007	498.522734	9.706253
7.936391	491.927807	9.711271
8.176319	507.145137	9.716288
8.324229	517.299236	9.721306
8.470329	510.560699	9.726323
8.692522	514.880735	9.731341
8.410147	527.282906	9.736359
8.662678	512.594042	9.741376
8.096913	502.467277	9.746394
8.425797	511.778826	9.751411
8.175261	517.981196	9.756429
8.238014	520.246552	9.761447
8.769896	526.550396	9.766464
8.292329	528.698440	9.771482
8.498217	523.963923	9.776499
8.336700	513.237330	9.781517
8.636312	523.187784	9.786535
8.666837	525.167858	9.791552
8.483692	526.925791	9.796570
8.617272	521.082299	9.801587
8.492049	520.458004	9.806605
8.213559	528.081706	9.811623
8.631863	517.526194	9.816640
8.790785	523.393014	9.821658
8.417790	520.027291	9.826675
8.525258	525.810656	9.831693
8.600955	526.331990	9.836711
8.647106	517.999658	9.841728
9.086804	520.212265	9.846746
8.392160	508.442590	9.851763
8.394207	499.429215	9.856781
7.972983	504.705278	9.861799
8.509587	510.323571	9.866816
8.641785	517.927102	9.871834
8.827538	522.694660	9.876851
8.395282	515.630174	9.881869
8.356069	524.822680	9.886887
8.471901	516.867592	9.891904
8.644493	527.443861	9.896922
8.416588	523.853435	9.901939
8.647984	522.374851	9.906957
8.218765	523.767397	9.911975
8.593364	520.495979	9.916992
8.383942	520.749562	9.922010
8.430088	514.348574	9.927027
8.505091	525.874246	9.932045
8.517296	516.843492	9.937063
8.612084	527.687571	9.942080
8.473941	541.152744	9.947098
8.580707	550.903056	9.952115
8.877581	555.220869	9.957133
8.829898	553.574570	9.962151
8.842788	554.497063	9.967168
8.864500	548.888840	9.972186
8.721967	549.337070	9.977203
9.249855	543.759992	9.982221
8.405591	535.933234	9.987239
8.231884	533.347323	9.992256
8.568767	535.850595	9.997274
8.943666	548.004632	10.002291
9.177544	540.709533	10.007309
8.563721	550.414958	10.012327
9.188564	546.223861	10.017344
8.820565	544.403689	10.022362
8.641058	545.936992	10.027379
9.035579	540.857337	10.032397
8.603477	544.595089	10.037415
8.925863	546.819769	10.042432
8.964817	541.126795	10.047450
8.605859	549.858174	10.052467
8.902105	535.560071	10.057485
8.724725	546.516232	10.062503
9.193084	546.748827	10.067520
8.893783	544.068983	10.072538
9.399427	541.102076	10.077555
9.104416	526.849282	10.082573
8.443316	524.699497	10.087591
8.576898	513.724697	10.092608
8.892075	538.485986	10.097626
8.931220	535.191385	10.102643
9.478118	537.535521	10.107661
8.749775	541.237637	10.112679
8.945567	534.686964	10.117696
9.145099	534.974301	10.122714
8.787199	524.493065	10.127731
9.111209	528.812931	10.132749
8.996313	542.788857	10.137767
9.199803	524.049320	10.142784
8.752624	519.480243	10.147802
8.889773	535.344858	10.152819
8.954035	541.857674	10.157837
9.042413	553.128804	10.162855
8.865553	549.580867	10.167872
8.661062	544.033333	10.172890
8.890181	550.315195	10.177907
8.828754	543.893182	10.182925
8.796630	549.587973	10.187943
8.993041	540.304285	10.192960
8.893458	542.459379	10.197978
8.619241	546.235510	10.202995
8.903825	542.441707	10.208013
8.693371	548.606250	10.213031
9.009112	561.769951	10.218048
9.356153	571.523654	10.223066
9.093449	587.529859	10.228083
9.469161	567.078098	10.233101
9.190980	564.678964	10.238119
9.109974	553.396935	10.243136
9.157391	550.009518	10.248154
9.337665	549.709740	10.253171
9.135399	551.675797	10.258189
8.975396	543.902771	10.263207
9.136866	561.978964	10.268224
9.179001	565.311059	10.273242
9.357102	569.571746	10.278259
9.528013	565.562219	10.283277
9.299232	553.893091	10.288295
9.066617	550.745208	10.293312
9.136415	547.253299	10.298330
8.862608	557.688090	10.303347
8.940373	566.041782	10.308365
9.201765	571.239314	10.313383
9.151894	579.524648	10.318400
9.187791	575.031346	10.323418
9.155791	578.984127	10.328435
9.449466	566.838657	10.333453
9.317979	571.476053	10.338471
9.195553	573.375955	10.343488
9.201690	569.004082	10.348506
9.017916	577.575482	10.353523
9.235343	566.858911	10.358541
9.434788	565.823985	10.363559
9.044855	561.075514	10.368576
9.304690	567.892211	10.373594
9.205177	577.599119	10.378611
9.309334	570.131830	10.383629
9.359705	571.307227	10.388647
9.414637	572.122149	10.393664
9.451615	566.322180	10.398682
9.443362	577.267639	10.403699
9.420060	558.696144	10.408717
9.287095	563.299056	10.413735
9.200775	565.423673	10.418752
9.375018	568.851834	10.423770
9.765121	586.286318	10.428787
9.484520	576.973207	10.433805
9.315013	572.395324	10.438823
9.196470	572.726187	10.443840
9.631338	587.594308	10.448858
9.432361	589.818629	10.453875
9.261141	595.718265	10.458893
9.119581	597.640103	10.463911
9.254060	597.050854	10.468928
9.948846	596.780914	10.473946
9.674525	602.898678	10.478963
9.811992	598.045474	10.483981
9.648280	600.892276	10.488999
9.686665	589.073967	10.494016
9.839774	580.500786	10.499034
9.330713	590.076209	10.504051
9.550096	583.139970	10.509069
9.580046	582.421933	10.514087
9.697494	583.204969	10.519104
9.707631	587.498289	10.524122
9.801786	586.789126	10.529139
9.203414	573.278102	10.534157
9.225855	578.819187	10.539175
9.222547	591.199768	10.544192
9.428837	589.936550	10.549210
9.534146	603.884333	10.554227
9.715207	583.636620	10.559245
9.771154	589.043070	10.564263
9.431753	591.989982	10.569280
9.642838	599.300322	10.574298
9.296843	596.204909	10.579315
9.523371	588.226134	10.584333
9.782093	585.304219	10.589351
9.713608	593.636658	10.594368
9.734227	587.649897	10.599386
9.561052	597.030686	10.604403
9.791598	586.144791	10.609421
10.033399	592.494109	10.614439
10.015779	600.165330	10.619456
10.025938	593.302894	10.624474
9.718702	596.020704	10.629491
9.701177	596.878538	10.634509
9.881545	592.545632	10.639527
9.574449	592.420045	10.644544
9.796426	592.902682	10.649562
9.638781	596.865686	10.654579
9.564071	601.194393	10.659597
9.898435	601.261791	10.664615
9.924963	606.107968	10.669632
10.109485	594.749596	10.674650
9.665676	596.895515	10.679667
9.964405	593.446623	10.684685
9.806861	595.497196	10.689703
9.728875	593.132963	10.694720
10.407798	603.226003	10.699738
9.784607	607.085227	10.704755
9.531651	601.882939	10.709773
10.203786	600.979076	10.714791
9.759034	604.797718	10.719808
9.830566	602.539445	10.724826
9.857811	619.626871	10.729843
10.144838	615.223600	10.734861
10.123689	630.806989	10.739879
10.110200	624.661459	10.744896
9.926534	603.312688	10.749914
9.959589	598.737774	10.754931
9.850526	617.500195	10.759949
10.025408	614.951173	10.764967
10.267033	621.224789	10.769984
10.120967	619.549717	10.775002
9.915287	607.188969	10.780019
10.064107	605.483475	10.785037
10.262459	598.089778	10.790055
9.860030	597.388993	10.795072
10.186093	596.110164	10.800090
9.974171	603.925440	10.805107
10.142844	617.427805	10.810125
10.240674	608.942166	10.815143
9.941025	599.903427	10.820160
10.540231	601.911173	10.825178
10.150528	606.099886	10.830195
9.850227	603.921963	10.835213
10.120819	611.235608	10.840231
10.067034	621.364564	10.845248
10.330001	613.799790	10.850266
10.534291	610.769635	10.855283
10.300982	598.750892	10.860301
10.192759	601.945606	10.865319
10.017271	595.011270	10.870336
10.191625	591.383051	10.875354
9.988850	599.493536	10.880371
10.219559	612.642195	10.885389
10.068187	620.296512	10.890407
10.105412	626.823062	10.895424
10.375544	625.227947	10.900442
10.087917	625.692601	10.905459
10.336954	623.125647	10.910477
10.704948	623.456019	10.915495
10.359127	640.949057	10.920512
10.451275	620.323912	10.925530
10.240695	614.556404	10.930547
9.874284	618.100842	10.935565
10.271019	616.290232	10.940583
9.872070	622.519047	10.945600
10.335584	620.697973	10.950618
10.140241	628.901982	10.955635
10.310761	626.530366	10.960653
10.410246	627.556060	10.965671
10.554119	631.897864	10.970688
10.478123	616.364140	10.975706
10.242617	628.184681	10.980723
10.458403	628.444227	10.985741
10.524906	629.620256	10.990759
9.854477	632.656909	10.995776
10.177617	636.797057	11.000794
10.517292	631.587114	11.005811
10.582269	631.327490	11.010829
10.731269	630.117427	11.015847
10.219914	629.320098	11.020864
10.483598	615.834920	11.025882
10.434446	622.040487	11.030899
10.209019	631.009758	11.035917
10.618274	624.245726	11.040935
10.296437	633.940161	11.045952
10.151707	627.670025	11.050970
10.918167	646.667684	11.055987
10.650127	645.990022	11.061005
10.668050	636.421824	11.066023
10.508229	628.494097	11.071040
10.672555	624.624445	11.076058
10.908422	623.612211	11.081075
10.686149	624.776681	11.086093
10.697433	626.775559	11.091111
10.740973	630.931112	11.096128
10.663299	627.298191	11.101146
10.898364	629.173645	11.106163
10.713914	621.145639	11.111181
10.753277	613.994597	11.116199
10.451732	621.994335	11.121216
10.666659	616.494673	11.126234
10.623916	623.983648	11.131251
10.442557	631.355490	11.136269
10.618639	626.622460	11.141287
10.632367	616.256512	11.146304
10.509774	617.847176	11.151322
10.477851	626.773504	11.156339
10.676634	636.039230	11.161357
10.879370	636.332380	11.166375
10.807962	638.331592	11.171392
10.454420	623.403082	11.176410
11.157585	638.222896	11.181427
10.858332	653.603726	11.186445
11.080231	633.305376	11.191463
10.576310	628.748316	11.196480
10.652883	621.108603	11.201498
10.828624	632.871024	11.206515
10.804910	639.053676	11.211533
10.962841	640.496248	11.216551
10.938940	644.488800	11.221568
10.173454	645.328127	11.226586
11.012156	643.132686	11.231603
10.776453	647.653886	11.236621
11.172084	651.258815	11.241639
11.288807	663.109399	11.246656
10.778722	656.347385	11.251674
10.846857	650.842309	11.256691
10.845731	652.448659	11.261709
10.566659	645.842958	11.266727
10.435708	659.023071	11.271744
10.917448	648.744722	11.276762
10.844398	642.488596	11.281779
10.807662	649.503270	11.286797
11.021090	648.497706	11.291815
10.689017	653.021384	11.296832
10.834279	643.688851	11.301850
10.811856	648.145077	11.306867
10.592695	652.916152	11.311885
10.862191	659.646163	11.316903
10.772294	674.476656	11.321920
11.042069	671.035441	11.326938
11.324920	676.696702	11.331955
11.155911	683.940397	11.336973
11.177469	667.741245	11.341991
10.905844	674.660187	11.347008
11.343399	677.539027	11.352026
11.651392	675.653953	11.357043
11.253348	673.443998	11.362061
10.913751	658.614259	11.367079
11.050836	656.661289	11.372096
11.361430	663.889793	11.377114
11.343839	660.818654	11.382131
10.962594	650.224236	11.387149
11.100656	652.515679	11.392167
10.991757	666.247764	11.397184
11.306004	666.810621	11.402202
11.323725	668.543407	11.407219
11.405429	665.601877	11.412237
11.578498	662.194751	11.417255
11.251184	658.695612	11.422272
10.929051	657.013409	11.427290
11.210403	648.366454	11.432307
11.128178	659.392981	11.437325
11.283611	665.402407	11.442343
11.592016	667.607202	11.447360
11.014462	667.151603	11.452378
11.471526	656.653053	11.457395
11.115516	661.401390	11.462413
11.615837	668.451846	11.467431
11.515387	676.609450	11.472448
11.384583	656.161208	11.477466
11.242914	653.380911	11.482483
11.242090	661.649131	11.487501
11.155231	666.557271	11.492519
11.254072	664.597669	11.497536
11.141039	676.768283	11.502554
11.369707	669.215172	11.507571
11.178201	673.802038	11.512589
11.203821	674.908736	11.517607
11.441270	677.572776	11.522624
11.322295	680.687137	11.527642
11.422332	665.223619	11.532659
10.965675	674.898175	11.537677
10.996375	667.978842	11.542695
11.273686	684.295002	11.547712
11.232838	697.609348	11.552730
11.565289	693.602885	11.557747
11.585611	695.903314	11.562765
11.392166	696.034475	11.567783
11.489747	697.448637	11.572800
11.535485	705.968360	11.577818
11.848916	701.541995	11.582835
11.685284	701.447578	11.587853
11.813393	690.527176	11.592871
11.621704	695.691591	11.597888
11.456788	698.806842	11.602906
11.794205	690.640233	11.607923
11.488887	696.993260	11.612941
11.830196	697.280477	11.617959
12.039925	697.266418	11.622976
11.702194	698.572059	11.627994
11.816346	691.633331	11.633011
11.804519	689.425978	11.638029
11.733996	685.167073	11.643047
11.676386	673.032389	11.648064
11.423226	677.635227	11.653082
11.711228	693.081870	11.658099
11.838622	687.649550	11.663117
11.927382	698.374755	11.668135
11.795816	692.055197	11.673152
11.419194	697.425313	11.678170
11.703499	688.856771	11.683187
11.689907	689.325827	11.688205
11.755522	691.852689	11.693223
11.805152	697.503160	11.698240
11.749736	700.209933	11.703258
12.071803	686.204312	11.708275
11.601288	694.530360	11.713293
11.890474	697.353554	11.718311
11.880685	694.063435	11.723328
11.402768	698.177628	11.728346
11.754150	693.489699	11.733363
11.782149	694.965256	11.738381
11.780103	692.642761	11.743399
11.898337	696.341655	11.748416
11.604708	697.479439	11.753434
11.945924	687.911053	11.758451
11.610071	688.452692	11.763469
11.782369	684.666985	11.768487
11.698618	694.898508	11.773504
12.008642	717.798921	11.778522
12.470124	711.932394	11.783539
12.002787	700.865438	11.788557
11.758858	694.699183	11.793575
12.093032	703.915330	11.798592
11.876640	710.409064	11.803610
12.190009	708.456871	11.808627
12.062241	717.404573	11.813645
12.471053	710.467007	11.818663
12.610506	706.345613	11.823680
12.229105	698.408391	11.828698
12.138155	691.413435	11.833715
11.875580	694.973178	11.838733
11.578464	693.040898	11.843751
11.907076	692.440164	11.848768
12.291312	712.646499	11.853786
12.309475	702.383948	11.858803
12.160182	708.441132	11.863821
12.185631	698.351012	11.868839
12.248955	692.852988	11.873856
11.902136	702.933229	11.878874
12.108474	707.776507	11.883891
12.282966	718.620836	11.888909
12.534043	714.971103	11.893927
12.440963	713.944132	11.898944
12.114083	711.069767	11.903962
12.512472	710.874669	11.908979
12.559496	702.507400	11.913997
12.033621	694.198338	11.919015
12.410381	680.423994	11.924032
12.099642	689.712776	11.929050
12.412789	692.052532	11.934067
12.369754	693.286753	11.939085
12.244284	688.449475	11.944103
12.215569	692.670011	11.949120
12.465015	707.239079	11.954138
12.627329	698.635996	11.959155
12.064361	699.128013	11.964173
12.128040	704.886739	11.969191
12.484202	705.812261	11.974208
12.267743	716.285496	11.979226
12.858025	707.523836	11.984243
12.452942	712.974156	11.989261
12.208394	718.727531	11.994279
12.703476	708.055735	11.999296
12.515589	718.650728	12.004314
12.485630	714.887237	12.009331
12.717419	707.507191	12.014349
12.441062	715.979554	12.019367
12.659925	715.219289	12.024384
12.606259	718.698967	12.029402
12.461750	714.546322	12.034419
12.386966	712.825359	12.039437
12.527774	707.703357	12.044455
12.574228	716.286089	12.049472
12.630800	719.379264	12.054490
12.460247	717.098946	12.059507
12.533019	720.057038	12.064525
12.377936	716.966406	12.069543
12.750906	710.772918	12.074560
12.445665	722.740148	12.079578
12.717036	713.545611	12.084595
12.388166	713.366629	12.089613
12.534286	707.022492	12.094631
12.770232	707.140025	12.099648
12.385789	710.841942	12.104666
12.388168	711.633546	12.109683
12.632490	701.837336	12.114701
12.289351	710.752507	12.119719
12.735274	709.723136	12.124736
12.794816	733.798911	12.129754
12.831069	728.595454	12.134771
12.809492	722.599480	12.139789
12.802965	721.972360	12.144807
12.764149	714.770410	12.149824
12.784906	730.517735	12.154842
12.542981	736.150782	12.159859
13.155705	731.866867	12.164877
12.893797	744.133436	12.169895
13.087035	745.478966	12.174912
13.042553	726.102723	12.179930
12.421020	715.728952	12.184947
12.968538	729.462380	12.189965
12.858485	732.894091	12.194983
13.334570	742.271061	12.200000
13.288177	733.555494	12.205018
12.839386	722.144789	12.210035
12.654449	715.514847	12.215053
12.366489	732.235198	12.220071
13.106219	739.753104	12.225088
13.184020	735.644518	12.230106
12.898111	741.852508	12.235123
13.058800	738.422061	12.240141
12.911525	743.219766	12.245159
13.317901	736.885335	12.250176
13.158352	744.862880	12.255194
13.060566	738.288702	12.260211
12.999368	739.525772	12.265229
12.966960	738.094815	12.270247
13.532245	731.255803	12.275264
13.393726	736.276198	12.280282
13.275184	726.129727	12.285299
13.163185	724.692306	12.290317
13.101291	729.028503	12.295335
13.018858	709.484654	12.300352
12.814334	729.205739	12.305370
13.048079	725.820653	12.310387
13.634831	736.518350	12.315405
13.007521	742.609415	12.320423
13.340578	733.979564	12.325440
13.668170	731.791609	12.330458
13.286545	727.717139	12.335475
13.163352	719.606906	12.340493
13.143646	726.107699	12.345511
13.387889	727.580936	12.350528
13.118206	733.174150	12.355546
13.343628	731.049541	12.360563
13.334489	740.562495	12.365581
13.048406	739.423750	12.370599
13.138536	734.161357	12.375616
13.430698	738.303226	12.380634
13.202666	739.014167	12.385651
13.171779	732.618859	12.390669
12.913094	741.429293	12.395687
13.085825	738.703865	12.400704
13.186633	731.315929	12.405722
13.528995	733.777345	12.410739
13.434752	735.502434	12.415757
13.455286	721.995312	12.420775
13.504957	729.700228	12.425792
13.440370	735.791487	12.430810
13.301623	731.009926	12.435827
13.544569	737.857737	12.440845
13.353602	731.531692	12.445863
13.742791	737.349881	12.450880
13.483553	733.590751	12.455898
13.330891	733.775483	12.460915
13.678453	732.035682	12.465933
13.565568	750.530596	12.470951
13.669275	751.022301	12.475968
13.568439	738.581918	12.480986
13.637242	746.915009	12.486003
13.776094	744.425263	12.491021
13.458890	744.414867	12.496039
13.559111	755.936736	12.501056
13.910561	755.395539	12.506074
13.490387	752.346435	12.511091
13.973513	747.218124	12.516109
13.967470	745.625244	12.521127
13.398318	740.100070	12.526144
13.916549	732.069215	12.531162
13.422183	736.804536	12.536179
13.711229	738.633674	12.541197
14.007018	753.044038	12.546215
14.111590	752.872884	12.551232
13.617508	734.816784	12.556250
13.474221	744.032020	12.561267
13.760540	742.980316	12.566285
13.955673	760.836841	12.571303
13.681280	746.145137	12.576320
13.833644	749.324295	12.581338
13.723509	753.986795	12.586355
14.087927	748.451047	12.591373
14.061036	748.593982	12.596391
14.048322	749.870794	12.601408
13.884951	749.678505	12.606426
13.964968	753.746319	12.611443
13.972501	757.478350	12.616461
14.135193	753.889794	12.621479
14.049844	749.794144	12.626496
14.436803	743.194508	12.631514
13.678433	736.610221	12.636531
14.036687	733.571701	12.641549
13.811708	735.866387	12.646567
14.123322	736.148790	12.651584
13.733786	743.408127	12.656602
13.804034	746.499164	12.661619
14.343518	753.871724	12.666637
13.882304	755.764766	12.671655
13.930689	747.880104	12.676672
14.291339	749.666467	12.681690
14.056970	755.995774	12.686707
14.090029	750.985317	12.691725
13.894093	758.230106	12.696743
14.194229	752.836972	12.701760
14.232578	753.913279	12.706778
14.473250	760.180782	12.711795
14.501987	747.789519	12.716813
14.307262	757.098029	12.721831
14.693470	757.343499	12.726848
14.406463	749.075881	12.731866
13.998761	737.321056	12.736883
14.247897	739.481497	12.741901
14.126491	742.324849	12.746919
14.204188	747.614330	12.751936
14.621888	753.039891	12.756954
13.822901	757.813477	12.761971
14.107847	752.883475	12.766989
14.217259	752.863042	12.772007
14.377564	748.280776	12.777024
14.543412	752.698062	12.782042
14.529596	759.598734	12.787059
14.441088	750.280682	12.792077
14.185121	764.550286	12.797095
14.191156	758.884491	12.802112
14.180636	743.807460	12.807130
14.040389	759.548478	12.812147
14.219410	752.362876	12.817165
14.173556	761.373505	12.822183
14.090275	761.900820	12.827200
14.183757	761.046588	12.832218
14.015151	770.682374	12.837235
14.358897	767.816537	12.842253
14.310407	778.676905	12.847271
14.564382	775.648404	12.852288
14.824849	771.388113	12.857306
14.275130	778.489523	12.862323
14.391674	778.947660	12.867341
14.617202	771.060480	12.872359
14.235412	775.857068	12.877376
14.272280	770.281114	12.882394
14.128215	778.057431	12.887411
14.616769	785.794593	12.892429
14.879785	796.524114	12.897447
15.065594	796.277114	12.902464
15.159692	788.423142	12.907482
14.394998	781.871387	12.912499
14.648385	777.669009	12.917517
14.799481	775.691741	12.922535
14.351511	782.717250	12.927552
14.968332	795.253277	12.932570
15.218773	798.653765	12.937587
14.900950	782.782241	12.942605
14.551444	778.781621	12.947623
14.922447	774.822750	12.952640
14.514968	777.789825	12.957658
14.712450	790.524096	12.962675
14.872410	803.298970	12.967693
14.762604	798.541259	12.972711
15.060861	803.319668	12.977728
15.433229	800.051705	12.982746
15.110328	791.130122	12.987763
15.037124	770.221440	12.992781
14.662215	773.221282	12.997799
14.763657	780.807654	13.002816
14.857306	793.722299	13.007834
14.988701	801.019961	13.012851
15.336268	801.624940	13.017869
15.216974	794.476593	13.022887
14.765228	782.769664	13.027904
15.217748	784.156624	13.032922
15.033185	788.098641	13.037939
15.001361	784.004065	13.042957
15.139415	788.454117	13.047975
15.196077	795.855006	13.052992
15.125226	779.856425	13.058010
15.132281	784.330157	13.063027
15.003446	790.494618	13.068045
15.347747	793.571127	13.073063
15.247486	798.998960	13.078080
15.045268	780.127059	13.083098
14.832125	780.330735	13.088115
15.281297	785.208572	13.093133
15.433542	799.953892	13.098151
15.130082	801.083756	13.103168
15.210809	799.884379	13.108186
14.970382	801.449339	13.113203
15.223987	794.245722	13.118221
15.364551	802.438206	13.123239
15.182967	804.265349	13.128256
15.596232	804.891593	13.133274
15.310331	805.090890	13.138291
15.075580	810.258928	13.143309
15.080558	799.872154	13.148327
15.134866	805.569263	13.153344
15.347788	795.970428	13.158362
15.256926	800.977063	13.163379
15.368804	808.631240	13.168397
15.458208	797.559045	13.173415
14.937464	796.706373	13.178432
15.483136	796.838496	13.183450
15.462052	803.958076	13.188467
15.247894	807.472385	13.193485
15.349912	803.009692	13.198503
15.532503	816.891884	13.203520
15.964528	821.453677	13.208538
15.740564	816.799055	13.213555
15.654741	806.382321	13.218573
15.722180	797.358551	13.223591
15.638534	799.896191	13.228608
15.465926	799.800024	13.233626
15.601531	803.379452	13.238643
15.527117	798.351106	13.243661
15.324066	800.377274	13.248679
15.508702	812.094239	13.253696
15.887614	814.329031	13.258714
15.788869	822.707344	13.263731
15.625897	818.081035	13.268749
15.874970	814.602012	13.273767
15.731150	811.844117	13.278784
16.311133	816.439532	13.283802
15.867423	802.544334	13.288819
15.263868	805.128720	13.293837
15.540599	806.805159	13.298855
15.623405	814.697426	13.303872
15.929398	816.612281	13.308890
15.817477	820.785923	13.313907
15.718357	827.135091	13.318925
16.245993	820.393463	13.323943
15.957744	819.731584	13.328960
15.936865	811.056163	13.333978
15.712825	821.511713	13.338995
15.638940	823.546048	13.344013
15.927227	818.779608	13.349031
15.895167	812.807338	13.354048
15.757916	814.431874	13.359066
15.712550	808.789897	13.364083
15.426773	817.074433	13.369101
15.733926	818.165432	13.374119
15.657070	817.167471	13.379136
16.200844	821.314119	13.384154
16.019891	829.358173	13.389171
15.956405	824.056705	13.394189
16.333698	832.524540	13.399207
16.236141	830.617783	13.404224
16.079846	827.382152	13.409242
16.011408	818.307076	13.414259
16.002453	834.930160	13.419277
16.350298	830.924411	13.424295
16.128567	831.845809	13.429312
16.494264	827.180849	13.434330
16.220531	823.982554	13.439347
15.913333	828.953664	13.444365
16.102196	828.583108	13.449383
16.245342	841.228097	13.454400
16.440628	838.057302	13.459418
16.394631	842.649815	13.464435
16.448784	842.675910	13.469453
16.257965	827.074785	13.474471
16.317629	819.923635	13.479488
16.326222	824.529681	13.484506
16.304087	832.040762	13.489523
16.166344	838.282375	13.494541
16.627543	831.936165	13.499559
16.305640	843.022450	13.504576
16.507303	836.928343	13.509594
16.523197	849.580654	13.514611
16.379615	841.858573	13.519629
16.637774	829.185152	13.524647
16.774681	841.487133	13.529664
16.324555	825.891923	13.534682
16.472977	822.854706	13.539699
16.169562	833.934932	13.544717
16.336454	835.199389	13.549735
16.522925	843.034400	13.554752
16.449736	835.556917	13.559770
16.480048	847.793551	13.564787
16.760225	840.017701	13.569805
16.838262	833.087732	13.574823
16.737874	847.314090	13.579840
16.675612	830.162235	13.584858
16.799003	833.383817	13.589875
16.749152	835.856207	13.594893
16.789669	835.802387	13.599911
16.703966	836.042901	13.604928
16.793471	831.822005	13.609946
16.839266	836.810394	13.614963
16.649165	841.567498	13.619981
16.512816	835.832469	13.624999
16.882614	836.642252	13.630016
16.591832	830.145616	13.635034
16.929162	839.052066	13.640051
16.577384	845.570216	13.645069
17.027907	831.945147	13.650087
16.559758	834.016011	13.655104
16.795460	829.503963	13.660122
16.976169	834.761550	13.665139
16.708837	832.862459	13.670157
16.968443	842.724685	13.675175
16.846913	836.198373	13.680192
16.896865	840.993605	13.685210
17.002741	839.929142	13.690227
16.476274	838.332586	13.695245
17.026531	825.458766	13.700263
16.845001	845.340480	13.705280
16.547014	851.544088	13.710298
17.204868	856.818442	13.715315
17.076093	859.868098	13.720333
17.270920	862.743973	13.725351
17.422399	872.828288	13.730368
17.206652	867.976702	13.735386
17.112561	847.812827	13.740403
16.820446	845.049759	13.745421
17.247899	854.914097	13.750439
17.390399	865.006125	13.755456
17.425468	858.540477	13.760474
17.481977	839.965652	13.765491
17.351111	843.564748	13.770509
17.051484	841.080573	13.775527
17.250561	828.832980	13.780544
16.984235	838.597724	13.785562
17.236338	846.586558	13.790579
17.167663	856.790565	13.795597
17.347094	865.671274	13.800615
17.588982	858.191753	13.805632
17.351018	857.600889	13.810650
17.626822	859.854998	13.815667
17.111897	847.779223	13.820685
17.440085	852.963216	13.825703
17.644922	858.258057	13.830720
17.123656	856.300917	13.835738
17.528949	855.782840	13.840755
17.190396	861.917067	13.845773
17.448271	864.558999	13.850791
17.412748	861.023570	13.855808
17.536796	864.002055	13.860826
17.612643	861.241294	13.865843
17.593454	871.835192	13.870861
17.459375	870.104569	13.875879
17.623210	851.844280	13.880896
17.537430	860.144838	13.885914
17.883711	860.768956	13.890931
17.480151	861.441130	13.895949
17.230987	860.173514	13.900967
17.614761	857.178312	13.905984
17.404205	866.091722	13.911002
17.367760	860.981669	13.916019
17.425340	860.565409	13.921037
17.749714	853.716758	13.926055
17.699331	859.603860	13.931072
17.400340	864.393810	13.936090
17.852422	877.997138	13.941107
17.722170	884.212346	13.946125
17.868396	887.067438	13.951143
17.924435	890.586766	13.956160
17.497753	887.715386	13.961178
17.989050	888.275757	13.966195
18.102953	892.098449	13.971213
18.228645	885.378747	13.976231
18.012104	869.503900	13.981248
17.709959	873.338125	13.986266
18.014080	869.175114	13.991283
17.919315	880.702367	13.996301
18.121314	881.844560	14.001319
17.972867	881.498450	14.006336
17.738277	884.201765	14.011354
17.962088	876.336899	14.016371
18.006544	883.790230	14.021389
18.004160	885.134862	14.026407
18.149017	876.411351	14.031424
18.214536	874.220259	14.036442
18.230155	888.491591	14.041459
18.057995	889.629290	14.046477
18.231523	867.583600	14.051495
18.376395	879.130111	14.056512
17.910387	883.750572	14.061530
17.940353	872.533006	14.066547
17.884716	884.013105	14.071565
17.785701	882.242273	14.076583
17.919860	888.930459	14.081600
17.795771	884.102378	14.086618
18.218372	892.777741	14.091635
18.539754	910.721935	14.096653
18.278703	903.308572	14.101671
18.165337	898.614509	14.106688
17.952149	904.883745	14.111706
18.467040	896.935394	14.116723
18.316921	902.282705	14.121741
18.519246	902.134104	14.126759
18.904843	896.781188	14.131776
18.702858	902.010392	14.136794
18.942047	899.930944	14.141811
18.530457	882.896888	14.146829
18.377488	871.294569	14.151847
18.322320	869.015088	14.156864
18.204869	879.756933	14.161882
18.581641	886.069429	14.166899
18.422813	892.383794	14.171917
18.757701	898.273661	14.176935
18.599750	906.036430	14.181952
18.442620	909.166276	14.186970
19.022396	896.884236	14.191987
18.759830	895.918523	14.197005
18.732894	883.330759	14.202023
18.484519	876.420357	14.207040
18.641584	895.848284	14.212058
18.895941	892.494651	14.217075
18.579697	893.964199	14.222093
18.734598	892.718480	14.227111
18.699471	889.246100	14.232128
18.438439	910.642529	14.237146
18.630942	901.930475	14.242163
18.677219	905.530233	14.247181
18.566503	902.161213	14.252199
18.722058	902.171421	14.257216
18.600701	905.125246	14.262234
18.739481	903.427608	14.267251
18.607133	906.569351	14.272269
18.893675	901.026822	14.277287
18.893867	899.142613	14.282304
18.860820	918.862287	14.287322
19.448750	918.268255	14.292339
19.215396	912.299087	14.297357
19.170492	904.447908	14.302375
19.380514	897.453053	14.307392
19.343660	895.511531	14.312410
19.197486	892.968591	14.317427
19.002311	897.824336	14.322445
19.270026	901.304189	14.327463
19.281796	890.152581	14.332480
18.922317	895.611590	14.337498
19.080886	894.295867	14.342515
19.053634	902.637768	14.347533
19.411983	903.704972	14.352551
19.136386	902.302637	14.357568
19.069231	907.542276	14.362586
19.089378	904.638754	14.367603
18.889525	904.534231	14.372621
19.175421	906.483803	14.377639
19.649516	922.652582	14.382656
19.494028	911.811194	14.387674
19.089152	906.348592	14.392691
19.267506	913.970308	14.397709
19.219572	918.162350	14.402727
19.509096	917.769709	14.407744
19.391574	924.165977	14.412762
19.635182	926.497724	14.417779
19.922263	925.224981	14.422797
19.661767	912.850517	14.427815
19.388626	904.186173	14.432832
19.238307	906.727963	14.437850
19.249049	911.308448	14.442867
19.490850	914.691377	14.447885
19.370697	927.204109	14.452903
19.667709	920.596410	14.457920
19.351889	933.183985	14.462938
19.286204	927.362114	14.467955
19.359207	934.564837	14.472973
19.372336	934.799335	14.477991
19.520952	931.165612	14.483008
19.731835	928.219578	14.488026
19.728751	927.973770	14.493043
19.725102	930.565168	14.498061
19.232705	936.032391	14.503079
19.510377	928.572481	14.508096
19.775009	936.082857	14.513114
20.005039	930.956279	14.518131
20.087194	938.659351	14.523149
19.820007	932.616581	14.528167
19.942031	916.994763	14.533184
19.694426	921.574703	14.538202
19.282096	922.472319	14.543219
20.048466	941.088449	14.548237
19.911154	939.197377	14.553255
20.203202	937.819711	14.558272
19.881679	946.425494	14.563290
20.061270	941.956923	14.568307
20.011306	938.029259	14.573325
19.868347	938.029432	14.578343
20.061494	932.520462	14.583360
20.324634	944.512397	14.588378
20.524134	939.119196	14.593395
20.400551	936.051993	14.598413
19.843772	931.597812	14.603431
20.048855	933.840920	14.608448
19.951141	946.561593	14.613466
20.183450	943.501745	14.618483
20.171435	941.884536	14.623501
19.961324	937.293985	14.628519
19.996467	939.014600	14.633536
20.046143	939.663102	14.638554
20.192182	938.835342	14.643571
20.354000	937.433899	14.648589
20.099506	941.475270	14.653607
20.400542	944.347142	14.658624
20.112808	940.718667	14.663642
19.841807	940.593732	14.668659
20.462907	936.488341	14.673677
20.336470	946.395330	14.678695
20.458020	943.475915	14.683712
20.548429	956.466926	14.688730
20.232287	946.616382	14.693747
20.681954	953.523407	14.698765
20.445823	965.072864	14.703783
20.769903	961.600995	14.708800
20.378030	941.878152	14.713818
20.343232	961.894799	14.718835
20.790431	960.704266	14.723853
20.749684	962.701867	14.728871
21.179875	947.877511	14.733888
21.063922	941.088350	14.738906
20.712585	936.879694	14.743923
20.939079	934.552918	14.748941
20.699822	930.342483	14.753959
20.752296	934.155874	14.758976
20.685217	932.405279	14.763994
20.639393	935.795407	14.769011
20.778770	925.428527	14.774029
20.656798	928.969442	14.779047
20.701011	931.569121	14.784064
20.331477	938.967416	14.789082
20.966710	950.620184	14.794099
21.205499	940.799463	14.799117
20.729738	930.936066	14.804135
20.787795	934.909531	14.809152
20.825037	951.878942	14.814170
20.882536	958.676997	14.819187
21.340252	956.970411	14.824205
20.939601	950.740258	14.829223
20.785165	958.736033	14.834240
20.951829	954.910125	14.839258
20.924218	962.687211	14.844275
20.884685	957.555523	14.849293
21.102011	957.540273	14.854311
21.234727	959.854685	14.859328
21.139890	958.272542	14.864346
20.775578	957.789835	14.869363
21.150443	951.046848	14.874381
21.101399	952.543965	14.879399
21.200033	949.725971	14.884416
21.359314	957.246550	14.889434
20.920870	960.575119	14.894451
21.269262	947.158472	14.899469
21.102780	950.397090	14.904487
21.230892	950.594638	14.909504
21.258416	951.527483	14.914522
21.489907	955.022490	14.919539
21.453927	946.630241	14.924557
21.433751	956.634199	14.929575
21.573702	952.171837	14.934592
21.264466	951.797268	14.939610
21.419714	952.000032	14.944627
21.491738	949.621715	14.949645
21.301129	951.538651	14.954663
20.953730	957.828934	14.959680
21.616501	973.816717	14.964698
21.750156	977.885646	14.969715
21.705524	976.541793	14.974733
21.649438	981.864928	14.979751
21.553911	979.525483	14.984768
21.743712	976.437575	14.989786
21.694364	975.978104	14.994803
21.940829	962.773079	14.999821
21.679204	960.557493	15.004839
21.593772	962.817720	15.009856
21.951980	956.269848	15.014874
21.253000	958.411606	15.019891
22.149432	962.878582	15.024909
22.001709	970.052785	15.029927
21.484823	972.131300	15.034944
22.063072	966.555670	15.039962
22.214727	975.226187	15.044979
22.203058	956.463103	15.049997
22.127814	954.158354	15.055015
22.007862	958.999174	15.060032
21.910640	949.366797	15.065050
21.710810	953.270216	15.070067
21.755278	944.461413	15.075085
21.705038	958.607418	15.080103
21.568251	963.570800	15.085120
21.494312	972.118868	15.090138
21.480280	982.014578	15.095155
21.961013	970.603246	15.100173
21.895334	982.930754	15.105191
21.601758	982.648407	15.110208
22.434252	990.625266	15.115226
22.602618	1003.058132	15.120243
22.397180	982.703262	15.125261
22.450518	980.517222	15.130279
22.148041	977.093024	15.135296
22.371601	969.954006	15.140314
22.038086	971.337902	15.145331
22.319469	975.484673	15.150349
22.614053	978.871967	15.155367
22.130740	968.078752	15.160384
22.456202	970.823722	15.165402
22.379178	970.157144	15.170419
22.524305	970.301533	15.175437
22.306210	973.765996	15.180455
22.227116	975.529761	15.185472
22.535715	974.177902	15.190490
22.303243	983.318871	15.195507
22.691784	987.265814	15.200525
22.685856	989.500965	15.205543
22.386100	981.276263	15.210560
22.622761	979.989325	15.215578
22.268479	987.006546	15.220595
22.587927	990.241621	15.225613
22.770306	1000.718806	15.230631
22.347222	1005.585042	15.235648
22.820384	996.926801	15.240666
22.545089	1004.739557	15.245683
22.687596	1001.150959	15.250701
22.917218	998.129393	15.255719
22.644604	992.459845	15.260736
22.638069	1001.893634	15.265754
22.730653	1001.989449	15.270771
22.614604	991.971827	15.275789
22.723462	992.428017	15.280807
22.860282	992.520058	15.285824
23.121332	995.237253	15.290842
22.851941	991.028369	15.295859
23.164365	985.876243	15.300877
23.256444	997.027151	15.305895
23.061867	992.986429	15.310912
22.961376	993.308159	15.315930
23.093786	995.808820	15.320947
22.856380	998.361112	15.325965
23.072940	995.180643	15.330983
23.271741	989.696017	15.336000
23.048364	987.054704	15.341018
22.902770	996.595486	15.346035
22.959680	990.896400	15.351053
22.594467	988.147918	15.356071
22.785471	1005.307888	15.361088
23.496600	1011.564888	15.366106
23.128140	1010.606292	15.371123
23.052214	1011.160864	15.376141
23.267138	1013.604417	15.381159
23.301204	1010.641891	15.386176
23.405732	1011.638415	15.391194
23.331465	1017.636610	15.396211
23.490968	1006.553303	15.401229
23.770747	1009.639959	15.406247
23.399214	1006.491669	15.411264
23.822096	1004.373961	15.416282
23.620309	1011.761783	15.421299
23.639729	1006.466206	15.426317
23.459236	1014.002175	15.431335
23.674257	1015.824005	15.436352
23.651961	1007.416961	15.441370
23.597460	1011.064087	15.446387
23.872796	1003.803332	15.451405
23.642958	996.987811	15.456423
23.478438	990.313540	15.461440
23.568573	992.745083	15.466458
24.007329	1006.319038	15.471475
23.879069	1004.694789	15.476493
23.760662	987.639944	15.481511
23.757801	981.177038	15.486528
23.617671	978.718347	15.491546
23.595850	991.370355	15.496563
23.201318	998.535901	15.501581
23.409741	1005.648006	15.506599
23.424139	1008.473278	15.511616
23.998192	1001.257241	15.516634
23.865010	1003.067353	15.521651
23.941804	1011.452965	15.526669
23.670595	996.987778	15.531687
23.885495	1001.189153	15.536704
24.146635	996.250191	15.541722
24.230962	1004.741919	15.546739
23.788572	993.509921	15.551757
24.138610	997.541797	15.556775
23.738496	1007.321282	15.561792
24.114421	1016.205995	15.566810
24.329807	1033.968101	15.571827
24.310322	1029.552791	15.576845
24.478487	1017.603409	15.581863
23.976595	1011.903505	15.586880
24.353278	1015.214826	15.591898
24.305966	1020.937394	15.596915
24.289585	1022.710272	15.601933
24.545026	1019.981310	15.606951
24.097778	1016.327317	15.611968
24.218288	1017.842057	15.616986
24.234644	1025.725893	15.622003
24.306299	1026.440384	15.627021
24.520060	1029.288073	15.632039
24.338533	1037.610027	15.637056
24.364144	1026.127953	15.642074
24.337146	1021.783252	15.647091
24.423587	1031.174086	15.652109
24.409172	1026.663306	15.657127
24.156678	1037.805109	15.662144
24.589557	1029.374076	15.667162
24.596864	1028.003147	15.672179
24.293258	1028.754341	15.677197
24.603473	1030.804261	15.682215
24.300406	1035.604363	15.687232
24.872359	1040.286304	15.692250
24.763076	1058.831467	15.697267
24.619992	1058.434018	15.702285
24.955351	1050.157114	15.707303
24.704276	1049.697688	15.712320
24.984994	1050.695012	15.717338
24.631756	1045.145379	15.722355
24.842773	1061.175618	15.727373
24.926232	1052.811944	15.732391
24.721166	1057.350538	15.737408
25.011372	1050.055876	15.742426
25.060036	1048.457553	15.747443
25.002108	1050.410517	15.752461
25.392248	1043.908105	15.757479
25.350592	1047.935088	15.762496
25.465549	1047.522458	15.767514
25.341866	1037.597526	15.772531
25.116633	1023.917238	15.777549
24.913418	1018.344108	15.782567
25.090074	1031.722458	15.787584
25.309633	1034.730190	15.792602
25.586103	1035.892284	15.797619
25.137399	1021.682109	15.802637
25.371073	1016.760068	15.807655
24.855958	1018.910895	15.812672
25.428126	1031.286826	15.817690
25.719943	1030.388883	15.822707
25.330919	1029.947916	15.827725
25.282305	1029.087532	15.832743
25.157950	1028.627189	15.837760
25.622681	1042.399078	15.842778
25.477658	1041.178249	15.847795
25.637093	1048.399035	15.852813
25.406510	1037.512529	15.857831
25.055077	1046.725819	15.862848
24.996828	1045.261015	15.867866
25.231004	1047.455397	15.872883
25.053289	1048.792798	15.877901
25.430271	1034.200775	15.882919
25.443595	1043.874477	15.887936
25.647696	1048.522534	15.892954
25.767439	1051.359711	15.897971
25.552091	1049.537659	15.902989
25.812803	1060.204583	15.908007
25.492478	1064.685496	15.913024
25.281740	1064.753095	15.918042
25.581084	1072.093984	15.923059
25.438996	1061.155728	15.928077
25.580255	1060.707417	15.933095
25.437456	1071.491219	15.938112
25.665387	1070.363437	15.943130
25.897210	1073.205148	15.948147
25.956168	1083.714343	15.953165
25.883516	1081.993010	15.958183
25.854313	1087.611774	15.963200
26.170905	1080.972545	15.968218
26.258842	1085.878660	15.973235
26.133685	1097.918912	15.978253
26.123882	1074.781350	15.983271
26.378620	1083.293754	15.988288
26.423540	1076.577169	15.993306
26.336198	1076.240416	15.998323
26.457654	1081.636752	16.003341
26.097945	1058.462512	16.008359
26.150195	1064.437745	16.013376
25.776532	1065.755353	16.018394
26.083546	1075.493514	16.023411
25.834266	1086.827353	16.028429
26.077591	1078.845729	16.033447
26.355468	1074.844577	16.038464
26.303178	1080.264979	16.043482
26.661119	1078.545611	16.048499
26.028848	1074.595539	16.053517
26.284274	1074.037820	16.058535
26.331231	1093.164469	16.063552
26.380766	1090.038556	16.068570
26.656340	1097.054967	16.073587
26.716458	1096.695110	16.078605
26.774795	1094.984812	16.083623
26.547993	1096.620248	16.088640
26.705716	1100.855852	16.093658
27.167075	1101.294687	16.098675
26.770322	1105.620323	16.103693
27.083410	1085.692192	16.108711
26.528680	1082.440043	16.113728
26.907709	1091.112863	16.118746
27.096861	1084.847059	16.123763
26.686720	1081.117810	16.128781
27.017722	1085.193714	16.133799
26.957978	1084.795831	16.138816
26.692178	1084.932019	16.143834
27.283067	1086.590822	16.148851
27.036211	1080.891963	16.153869
27.027208	1076.456064	16.158887
26.888233	1073.179804	16.163904
26.570213	1086.935509	16.168922
27.143938	1090.654641	16.173939
26.953101	1094.297899	16.178957
26.757187	1097.197163	16.183975
26.788443	1097.078519	16.188992
26.580407	1098.793069	16.194010
27.391747	1090.570961	16.199027
27.085792	1097.504911	16.204045
27.076523	1097.020222	16.209063
27.324299	1098.303584	16.214080
27.537601	1106.992910	16.219098
27.552121	1093.546411	16.224115
27.286104	1099.031865	16.229133
27.487471	1095.475052	16.234151
27.166817	1104.027124	16.239168
27.156092	1105.811748	16.244186
27.354316	1108.756561	16.249203
27.554820	1113.335770	16.254221
27.422583	1126.500648	16.259239
27.622789	1126.762644	16.264256
27.728698	1125.429908	16.269274
27.752857	1124.119449	16.274291
27.493766	1128.360404	16.279309
27.714282	1118.987430	16.284327
27.711870	1129.149651	16.289344
27.757090	1129.098250	16.294362
27.759908	1112.772238	16.299379
27.720639	1120.784756	16.304397
28.052896	1116.800322	16.309415
27.831975	1115.004383	16.314432
28.050558	1118.261598	16.319450
27.826631	1120.341566	16.324467
27.455958	1122.296200	16.329485
27.672676	1116.032378	16.334503
28.040293	1113.983279	16.339520
27.637666	1128.130978	16.344538
27.984955	1121.007229	16.349555
28.141541	1119.612904	16.354573
28.167401	1123.449440	16.359591
28.472263	1130.448652	16.364608
27.963334	1127.902552	16.369626
28.018405	1117.551926	16.374643
27.950632	1118.464996	16.379661
27.999847	1124.525933	16.384679
28.167713	1124.720411	16.389696
28.218179	1119.946970	16.394714
28.505082	1116.490364	16.399731
28.074903	1112.656947	16.404749
28.113054	1119.050985	16.409767
28.402530	1124.553557	16.414784
28.147961	1123.807490	16.419802
28.394523	1128.376330	16.424819
28.280216	1135.169812	16.429837
28.419817	1144.025342	16.434855
28.544039	1139.404448	16.439872
28.379093	1137.419851	16.444890
28.640906	1130.293711	16.449907
28.513300	1137.613156	16.454925
28.713554	1134.362632	16.459943
28.806255	1137.222995	16.464960
28.728179	1138.440646	16.469978
28.829579	1136.723596	16.474995
28.606107	1133.618359	16.480013
28.593870	1136.930676	16.485031
28.941128	1135.856780	16.490048
28.740686	1138.191855	16.495066
28.581454	1127.985256	16.500083
28.932360	1132.007558	16.505101
28.750046	1141.254361	16.510119
28.996905	1135.613833	16.515136
28.853498	1134.146585	16.520154
29.088999	1143.744504	16.525171
29.191286	1143.674694	16.530189
29.013505	1132.527385	16.535207
28.861334	1128.498924	16.540224
28.712631	1138.478938	16.545242
29.250618	1135.686754	16.550259
29.111310	1136.276508	16.555277
28.981889	1133.762466	16.560295
28.900906	1126.475436	16.565312
28.755863	1137.256473	16.570330
28.886057	1136.932974	16.575347
29.232177	1148.391323	16.580365
29.058849	1151.205003	16.585383
29.894606	1154.646402	16.590400
29.456585	1157.088132	16.595418
29.410374	1160.178552	16.600435
29.134750	1141.491345	16.605453
29.150257	1154.708837	16.610471
28.969780	1158.782843	16.615488
29.340245	1158.522687	16.620506
29.276937	1155.420755	16.625523
29.386885	1165.458092	16.630541
29.366258	1162.472552	16.635559
29.593176	1159.533436	16.640576
29.373226	1161.562292	16.645594
29.358951	1155.274686	16.650611
29.346067	1177.191148	16.655629
29.613482	1181.728332	16.660647
29.942812	1181.253707	16.665664
29.976563	1184.268485	16.670682
30.024572	1179.921461	16.675699
29.957177	1183.068855	16.680717
30.237729	1185.054010	16.685735
30.186400	1171.456819	16.690752
29.816796	1163.997236	16.695770
30.272579	1154.448523	16.700787
29.985212	1147.275873	16.705805
29.529659	1158.067702	16.710823
30.040332	1169.519218	16.715840
30.136027	1170.880064	16.720858
30.240839	1174.950401	16.725875
30.453540	1177.154477	16.730893
30.126899	1176.728978	16.735911
30.203680	1169.332003	16.740928
30.378217	1179.479152	16.745946
30.151840	1165.937794	16.750963
30.166623	1165.645001	16.755981
30.287939	1172.606714	16.760999
30.476233	1171.270535	16.766016
30.432897	1165.618658	16.771034
30.436270	1170.408654	16.776051
30.357427	1166.747403	16.781069
30.520243	1172.557022	16.786087
30.495551	1164.024043	16.791104
29.946831	1167.963236	16.796122
30.131843	1171.907395	16.801139
30.401048	1156.839838	16.806157
30.138839	1169.659028	16.811175
30.590369	1169.897427	16.816192
30.497896	1173.408521	16.821210
30.731112	1174.545842	16.826227
30.819351	1159.620249	16.831245
30.293511	1161.179464	16.836263
30.587957	1177.477611	16.841280
30.716731	1190.465938	16.846298
30.963716	1193.769211	16.851315
31.126170	1193.680506	16.856333
30.850515	1203.257555	16.861351
31.078781	1191.642635	16.866368
31.249877	1190.511127	16.871386
31.006808	1176.801957	16.876403
30.766470	1165.108991	16.881421
30.769189	1184.883317	16.886439
31.199869	1171.690303	16.891456
31.302417	1190.120359	16.896474
30.968934	1190.125136	16.901491
31.061251	1193.114959	16.906509
30.890536	1190.484300	16.911527
31.360092	1185.660959	16.916544
31.498289	1192.200299	16.921562
31.424447	1182.810294	16.926579
31.158316	1186.588447	16.931597
31.170862	1191.623172	16.936615
31.272911	1183.269148	16.941632
31.395262	1190.514737	16.946650
31.127646	1181.022544	16.951667
31.162528	1178.141917	16.956685
31.527876	1186.627573	16.961703
31.394619	1187.295277	16.966720
31.336157	1187.534684	16.971738
31.243383	1178.182361	16.976755
31.394205	1178.919169	16.981773
31.448238	1196.504740	16.986791
31.531855	1201.080193	16.991808
31.664047	1204.884307	16.996826
31.839678	1203.872012	17.001843
31.818920	1204.995478	17.006861
31.735493	1206.011993	17.011879
32.145822	1207.882141	17.016896
32.055308	1207.047249	17.021914
31.857640	1214.084203	17.026931
31.996528	1217.533809	17.031949
32.181944	1217.040706	17.036967
32.301901	1199.796827	17.041984
32.156812	1199.765775	17.047002
31.976746	1187.413233	17.052019
31.957471	1182.789563	17.057037
31.973664	1208.311862	17.062055
32.183149	1200.070390	17.067072
32.540637	1205.903169	17.072090
31.908410	1199.687119	17.077107
32.436729	1197.657015	17.082125
32.457497	1203.558329	17.087143
31.942646	1194.884374	17.092160
32.256963	1201.149963	17.097178
32.238649	1205.930743	17.102195
32.099472	1195.358034	17.107213
32.061445	1197.680293	17.112231
32.311152	1193.405808	17.117248
32.304424	1202.369504	17.122266
32.431033	1198.107993	17.127283
32.464931	1201.469901	17.132301
32.666837	1198.556789	17.137319
32.601519	1187.290837	17.142336
32.832305	1190.940641	17.147354
32.482658	1200.829093	17.152371
32.597424	1194.824222	17.157389
32.220275	1203.514584	17.162407
32.680905	1214.415374	17.167424
32.857524	1220.617335	17.172442
32.632771	1220.276861	17.177459
33.283647	1218.682003	17.182477
32.717600	1225.631506	17.187495
32.404988	1215.089115	17.192512
32.802825	1221.003942	17.197530
32.640510	1226.144972	17.202547
32.800446	1223.402539	17.207565
32.735796	1228.963783	17.212583
33.018359	1215.610900	17.217600
33.078272	1216.093701	17.222618
32.964637	1218.544577	17.227635
33.084697	1228.665575	17.232653
33.441544	1248.605402	17.237671
33.107283	1239.259324	17.242688
33.509363	1227.288933	17.247706
33.305154	1232.231394	17.252723
33.323056	1226.342678	17.257741
33.421718	1232.029819	17.262759
33.279456	1231.471286	17.267776
33.516461	1227.173537	17.272794
33.537034	1232.181768	17.277811
33.792840	1229.178153	17.282829
33.360515	1221.917727	17.287847
33.408150	1224.731514	17.292864
33.634585	1230.676356	17.297882
33.319020	1244.842066	17.302899
33.931910	1240.154050	17.307917
33.745304	1238.740900	17.312935
33.973747	1245.370265	17.317952
33.670089	1239.995846	17.322970
33.913091	1242.725376	17.327987
33.892519	1237.918851	17.333005
33.629134	1241.327344	17.338023
33.551349	1242.813209	17.343040
33.969966	1231.534525	17.348058
33.788362	1241.273590	17.353075
34.062031	1243.786869	17.358093
33.752090	1237.728601	17.363111
33.589155	1250.093623	17.368128
33.984125	1249.993734	17.373146
33.697152	1245.869598	17.378163
33.871914	1240.615887	17.383181
34.020290	1260.566299	17.388199
33.753399	1274.191056	17.393216
34.249526	1273.513565	17.398234
34.334100	1279.382816	17.403251
34.771778	1274.009004	17.408269
34.315497	1280.464787	17.413287
34.319458	1268.903896	17.418304
34.522126	1269.171820	17.423322
34.075050	1271.110037	17.428339
34.248204	1267.576547	17.433357
34.444377	1275.918332	17.438375
34.399850	1267.732406	17.443392
34.478821	1260.874712	17.448410
34.640976	1262.884739	17.453427
34.788302	1263.779894	17.458445
34.590177	1270.229940	17.463463
34.575055	1262.216142	17.468480
34.795431	1264.895569	17.473498
34.402599	1272.887808	17.478515
34.468149	1277.485047	17.483533
34.829602	1290.995590	17.488551
34.795567	1296.659360	17.493568
35.644678	1280.071208	17.498586
35.018522	1287.550879	17.503603
35.121925	1294.657463	17.508621
35.233692	1290.593923	17.513639
35.067798	1267.414293	17.518656
35.306236	1270.513785	17.523674
34.700134	1267.806156	17.528691
35.003089	1270.519985	17.533709
34.988143	1285.020493	17.538727
34.896987	1287.388959	17.543744
35.136190	1281.478176	17.548762
34.856746	1283.876142	17.553779
35.211309	1282.532840	17.558797
35.589176	1286.727685	17.563815
35.331902	1293.508912	17.568832
35.309045	1279.380138	17.573850
35.220901	1277.007937	17.578867
35.432127	1277.684791	17.583885
35.175114	1279.883575	17.588903
35.357149	1279.747618	17.593920
35.637437	1283.134056	17.598938
35.716495	1298.541376	17.603955
35.724950	1294.235236	17.608973
35.564538	1303.472379	17.613991
35.578129	1308.983518	17.619008
35.835503	1308.403395	17.624026
35.748225	1305.794361	17.629043
35.980584	1295.194941	17.634061
36.170696	1301.344320	17.639079
36.057627	1305.224754	17.644096
35.929904	1300.586485	17.649114
35.993346	1298.929018	17.654131
36.191847	1296.849588	17.659149
35.810450	1304.619135	17.664167
35.968247	1301.242685	17.669184
36.092801	1300.456146	17.674202
36.159197	1294.386234	17.679219
36.162604	1305.519669	17.684237
36.146415	1300.494682	17.689255
36.398884	1295.194065	17.694272
36.562043	1285.583829	17.699290
36.704590	1292.406558	17.704307
36.611703	1298.022742	17.709325
36.474417	1298.192446	17.714343
36.448355	1303.296369	17.719360
36.529848	1294.172313	17.724378
35.978493	1294.157574	17.729395
36.022875	1287.879666	17.734413
36.297221	1296.098756	17.739431
36.425764	1291.395091	17.744448
36.412066	1291.431818	17.749466
36.391409	1305.172659	17.754483
36.527184	1307.161577	17.759501
36.948593	1314.246747	17.764519
36.556472	1319.313351	17.769536
36.897280	1305.310623	17.774554
37.161398	1321.165512	17.779571
36.974254	1319.111786	17.784589
37.079396	1324.879996	17.789607
36.837436	1321.758687	17.794624
37.396525	1321.901339	17.799642
37.313556	1319.007594	17.804659
37.064811	1308.726550	17.809677
37.136864	1289.419803	17.814695
36.585474	1297.165485	17.819712
37.180236	1304.816805	17.824730
37.197541	1317.431355	17.829747
37.107125	1319.386283	17.834765
37.080526	1311.674073	17.839783
36.917287	1317.373872	17.844800
37.096061	1318.847950	17.849818
37.066633	1323.845105	17.854835
37.017243	1312.990005	17.859853
37.274824	1331.234964	17.864871
36.976325	1346.733040	17.869888
37.359809	1340.127418	17.874906
37.332471	1340.731194	17.879923
37.335229	1344.827028	17.884941
37.444213	1341.628638	17.889959
37.723063	1347.256026	17.894976
37.817948	1345.543133	17.899994
37.661286	1341.935066	17.905011
37.699601	1334.755496	17.910029
37.930773	1339.784412	17.915047
37.530236	1334.750204	17.920064
37.675960	1341.206365	17.925082
38.171781	1349.068874	17.930099
37.764015	1361.911007	17.935117
38.142626	1358.215915	17.940135
37.754598	1364.279165	17.945152
38.098593	1362.498838	17.950170
38.221043	1363.145421	17.955187
38.142368	1357.218143	17.960205
38.533265	1357.163076	17.965223
38.584114	1362.526377	17.970240
38.549204	1351.987733	17.975258
38.312684	1356.790117	17.980275
38.453617	1358.509978	17.985293
38.429687	1351.015093	17.990311
38.189584	1346.953019	17.995328
38.395362	1352.550830	18.000346
38.748474	1359.037624	18.005363
38.571754	1355.581025	18.010381
38.471983	1354.233159	18.015399
38.539189	1357.444705	18.020416
38.803724	1360.076201	18.025434
38.667041	1350.273057	18.030451
38.561738	1358.065644	18.035469
38.752542	1352.793608	18.040487
38.250030	1354.238725	18.045504
38.267188	1347.914567	18.050522
38.338900	1357.074341	18.055539
38.272551	1369.449560	18.060557
38.720981	1375.501686	18.065575
38.787954	1375.118658	18.070592
38.813323	1378.229460	18.075610
38.811882	1378.115937	18.080627
38.949637	1383.626581	18.085645
39.152709	1372.839191	18.090663
38.716309	1373.917331	18.095680
38.797075	1384.416975	18.100698
39.174131	1383.837034	18.105715
39.200392	1388.797079	18.110733
39.544608	1398.974576	18.115751
39.554137	1394.444172	18.120768
39.499187	1394.279071	18.125786
39.737124	1391.552795	18.130803
39.724330	1392.346807	18.135821
39.928916	1389.644692	18.140839
39.735948	1390.473245	18.145856
39.533161	1389.138360	18.150874
39.706190	1389.499297	18.155891
39.854508	1388.418685	18.160909
40.106813	1391.579144	18.165927
39.888579	1379.892041	18.170944
39.609101	1356.698531	18.175962
39.973664	1374.270339	18.180979
39.952727	1387.288577	18.185997
39.908194	1366.715546	18.191015
40.198425	1372.669376	18.196032
39.964839	1370.957449	18.201050
40.034406	1375.004952	18.206067
39.737234	1369.888263	18.211085
39.884342	1378.493415	18.216103
39.753041	1389.341881	18.221120
40.375524	1392.649479	18.226138
40.371092	1388.900781	18.231155
40.140037	1395.374967	18.236173
40.562632	1391.130156	18.241191
40.634233	1388.972764	18.246208
40.040127	1393.225242	18.251226
40.041417	1393.205970	18.256243
40.034464	1394.712309	18.261261
39.904748	1388.925567	18.266279
40.052242	1399.537847	18.271296
40.276230	1405.050766	18.276314
40.643816	1414.012728	18.281331
40.565360	1420.895380	18.286349
40.720022	1415.461722	18.291367
40.740661	1413.930877	18.296384
40.537976	1421.366347	18.301402
40.456338	1418.371387	18.306419
40.434648	1418.576632	18.311437
40.574803	1410.528970	18.316455
40.724208	1419.244239	18.321472
40.706752	1430.857569	18.326490
41.001265	1427.393400	18.331507
41.138758	1440.484689	18.336525
41.268527	1425.429286	18.341543
41.237044	1426.627032	18.346560
41.075390	1434.920809	18.351578
41.153241	1426.889213	18.356595
41.414097	1433.466231	18.361613
41.904560	1422.785269	18.366631
41.854841	1424.979996	18.371648
41.457172	1414.621234	18.376666
41.364710	1398.865335	18.381683
41.115814	1404.262988	18.386701
41.505622	1411.526726	18.391719
41.582772	1420.925533	18.396736
41.626035	1432.488323	18.401754
41.699138	1425.189652	18.406771
41.604379	1434.116761	18.411789
41.697208	1427.758627	18.416807
41.639483	1438.485137	18.421824
41.512982	1440.584593	18.426842
41.741667	1426.447852	18.431859
41.359441	1429.013426	18.436877
41.631759	1434.039078	18.441895
41.985563	1424.408366	18.446912
41.874492	1432.621630	18.451930
42.054583	1418.861754	18.456947
41.299551	1424.603811	18.461965
41.934549	1448.413657	18.466983
42.229523	1457.923529	18.472000
42.243648	1453.603839	18.477018
42.466412	1442.336774	18.482035
42.245574	1455.941829	18.487053
42.189787	1442.061095	18.492071
41.986435	1451.043097	18.497088
42.157500	1444.436003	18.502106
42.235758	1445.635493	18.507123
41.976797	1451.498661	18.512141
42.402984	1447.770850	18.517159
42.327800	1448.748216	18.522176
42.539762	1466.564941	18.527194
42.878044	1466.609640	18.532211
42.978001	1478.482328	18.537229
42.838010	1468.023200	18.542247
42.770789	1451.578458	18.547264
42.713140	1466.641251	18.552282
42.894183	1460.382899	18.557299
42.806796	1471.874662	18.562317
42.922596	1463.600408	18.567335
43.067722	1473.184261	18.572352
43.113464	1468.035910	18.577370
42.809173	1460.477602	18.582387
42.661684	1462.236350	18.587405
42.694370	1459.905157	18.592423
42.727328	1462.159521	18.597440
42.984073	1463.712918	18.602458
43.204214	1460.683293	18.607475
42.940573	1469.706310	18.612493
42.961222	1480.335355	18.617511
43.345726	1485.393940	18.622528
43.068492	1492.964202	18.627546
43.541098	1483.598881	18.632563
43.498438	1487.916469	18.637581
43.417992	1495.784120	18.642599
43.568105	1490.906602	18.647616
43.569196	1485.727369	18.652634
43.914783	1488.478736	18.657651
43.939848	1490.917386	18.662669
43.944410	1495.252825	18.667687
43.884325	1481.420072	18.672704
43.900896	1476.910636	18.677722
44.333767	1483.760538	18.682739
43.921755	1478.996342	18.687757
44.123564	1480.788732	18.692775
44.383882	1480.116621	18.697792
44.186589	1492.360954	18.702810
44.146955	1484.644400	18.707827
43.924652	1496.472912	18.712845
44.215388	1479.416613	18.717863
44.398105	1471.523209	18.722880
44.063937	1485.032429	18.727898
44.336701	1476.137100	18.732915
44.219583	1484.471261	18.737933
44.149324	1484.147603	18.742951
43.908187	1483.421508	18.747968
44.036875	1492.329416	18.752986
44.206014	1498.769343	18.758003
44.506398	1509.433476	18.763021
44.515703	1503.000035	18.768039
44.615758	1506.771378	18.773056
44.817205	1514.418137	18.778074
44.725748	1509.900370	18.783091
44.414841	1509.371407	18.788109
44.746376	1502.401462	18.793127
44.651272	1506.244409	18.798144
44.612816	1520.534186	18.803162
44.797217	1521.240500	18.808179
44.894747	1528.351253	18.813197
44.820933	1534.494724	18.818215
45.064751	1523.653521	18.823232
45.039601	1536.549446	18.828250
44.833050	1526.488895	18.833267
45.011953	1526.224033	18.838285
44.744609	1536.024031	18.843303
45.314070	1535.773721	18.848320
45.299127	1547.487723	18.853338
45.452040	1541.287402	18.858355
45.729654	1545.564292	18.863373
45.830737	1549.843594	18.868391
45.888622	1546.697357	18.873408
45.639489	1551.700595	18.878426
45.890592	1549.587647	18.883443
45.848892	1543.222147	18.888461
45.649001	1523.900947	18.893479
45.931629	1522.852935	18.898496
45.777942	1533.796519	18.903514
45.936033	1526.430840	18.908531
45.569885	1531.872149	18.913549
45.611505	1539.670199	18.918567
45.854224	1537.012584	18.923584
45.986312	1547.886154	18.928602
45.986505	1548.349917	18.933619
45.792830	1539.679124	18.938637
46.289876	1542.785485	18.943655
46.397198	1540.357377	18.948672
45.901679	1541.454256	18.953690
45.790740	1539.139244	18.958707
46.153080	1543.869942	18.963725
46.150400	1559.482807	18.968743
46.079656	1559.913501	18.973760
46.321556	1566.802824	18.978778
46.449130	1568.752028	18.983795
46.410635	1568.798953	18.988813
46.722058	1562.523294	18.993831
46.470960	1564.402432	18.998848
46.139326	1574.973113	19.003866
46.526378	1573.025065	19.008883
46.787886	1572.116066	19.013901
47.144832	1588.278558	19.018919
47.353527	1577.802606	19.023936
46.882287	1576.714905	19.028954
47.237806	1568.803853	19.033971
47.081665	1563.068534	19.038989
46.825201	1568.199164	19.044007
47.002902	1578.677422	19.049024
46.822391	1587.914704	19.054042
47.412785	1577.868125	19.059059
47.252075	1578.492805	19.064077
47.204906	1576.653816	19.069095
47.098588	1579.627487	19.074112
47.257329	1588.275101	19.079130
47.434275	1586.157988	19.084147
47.394939	1574.423792	19.089165
47.206045	1574.992924	19.094183
47.801839	1583.430042	19.099200
47.370910	1582.714742	19.104218
47.649015	1588.152964	19.109235
47.700187	1595.656036	19.114253
47.381115	1600.547162	19.119271
47.888591	1607.379111	19.124288
47.693613	1611.995163	19.129306
47.946150	1613.003248	19.134323
48.017685	1592.175073	19.139341
47.943464	1604.261338	19.144359
48.181626	1598.113916	19.149376
47.809433	1600.248728	19.154394
48.003067	1604.936444	19.159411
48.147318	1598.967846	19.164429
48.160363	1600.228059	19.169447
48.413505	1616.911797	19.174464
48.667320	1626.049491	19.179482
48.592133	1612.496729	19.184499
48.697691	1605.265488	19.189517
48.338537	1597.135018	19.194535
48.489914	1595.293323	19.199552
48.611078	1602.586606	19.204570
48.701905	1611.352175	19.209587
49.263076	1619.797890	19.214605
48.644890	1611.458674	19.219623
48.742618	1596.165137	19.224640
48.849586	1590.173979	19.229658
48.749436	1592.992043	19.234675
48.579825	1593.678082	19.239693
48.525468	1612.196277	19.244711
49.169681	1622.541506	19.249728
49.030552	1629.370624	19.254746
48.670062	1623.058197	19.259763
48.912041	1629.796045	19.264781
48.549001	1624.307729	19.269799
49.049913	1619.056460	19.274816
49.126550	1633.334607	19.279834
49.134216	1632.102438	19.284851
49.441259	1647.846745	19.289869
49.563427	1653.344135	19.294887
49.697977	1651.606063	19.299904
49.794093	1648.939841	19.304922
49.403147	1644.762469	19.309939
49.594462	1650.242712	19.314957
49.369576	1643.290459	19.319975
49.862376	1642.938544	19.324992
49.664705	1648.662779	19.330010
49.590356	1641.554389	19.335027
49.702157	1643.209411	19.340045
49.525796	1637.089049	19.345063
49.429855	1634.907382	19.350080
49.973610	1645.063225	19.355098
50.085196	1656.126277	19.360115
50.280405	1655.530636	19.365133
49.961739	1655.327950	19.370151
50.018814	1655.299938	19.375168
49.919342	1660.607980	19.380186
50.128628	1661.139978	19.385203
50.354894	1657.418199	19.390221
49.908954	1658.930219	19.395239
50.288427	1663.178555	19.400256
50.212815	1676.120358	19.405274
50.475477	1679.111979	19.410291
50.762880	1680.067265	19.415309
50.903644	1685.990966	19.420327
50.874839	1683.113924	19.425344
50.929165	1677.257225	19.430362
50.860518	1677.122670	19.435379
51.027085	1678.459827	19.440397
50.672767	1686.083275	19.445415
50.768150	1674.839178	19.450432
50.804140	1675.092196	19.455450
50.838720	1679.233616	19.460467
51.175588	1682.352475	19.465485
50.951852	1686.559617	19.470503
50.822188	1675.524358	19.475520
51.516412	1682.680548	19.480538
51.436262	1698.498188	19.485555
51.659770	1699.441394	19.490573
51.089990	1696.649107	19.495591
51.288782	1702.996093	19.500608
51.405093	1703.968719	19.505626
51.436796	1705.958207	19.510643
51.823610	1699.377181	19.515661
51.569898	1710.317608	19.520679
51.803250	1705.464862	19.525696
51.868498	1697.214201	19.530714
52.149327	1701.490625	19.535731
52.099756	1693.766069	19.540749
51.966187	1703.576759	19.545767
52.035986	1700.756853	19.550784
51.833359	1694.590091	19.555802
51.932647	1695.839955	19.560819
51.893734	1686.248540	19.565837
52.080838	1698.448568	19.570855
51.868827	1685.829271	19.575872
52.225926	1686.530626	19.580890
51.746824	1694.729083	19.585907
52.377699	1714.462386	19.590925
52.364028	1721.281350	19.595943
52.422467	1726.435275	19.600960
52.615997	1720.013921	19.605978
52.535957	1728.130934	19.610995
52.555320	1726.802246	19.616013
52.267159	1724.568627	19.621031
52.380197	1720.119760	19.626048
52.590718	1721.393226	19.631066
52.524785	1725.660865	19.636083
52.964505	1736.379048	19.641101
53.041910	1739.292400	19.646119
53.090614	1751.735069	19.651136
53.269550	1746.717257	19.656154
52.998217	1742.458001	19.661171
53.346819	1742.419030	19.666189
53.304884	1747.206811	19.671207
53.219859	1744.562643	19.676224
53.074598	1740.567676	19.681242
53.021465	1742.103371	19.686259
53.198906	1738.367134	19.691277
53.184321	1742.740348	19.696295
53.085742	1741.770986	19.701312
53.373629	1733.431773	19.706330
53.223161	1744.766326	19.711347
53.715682	1744.565941	19.716365
53.713540	1758.462030	19.721383
54.025832	1757.952191	19.726400
54.081805	1761.840954	19.731418
53.972945	1766.686566	19.736435
53.990935	1756.776909	19.741453
54.105220	1763.086661	19.746471
53.843471	1761.028792	19.751488
54.058786	1763.188348	19.756506
53.463065	1763.319420	19.761523
54.344033	1761.836801	19.766541
53.899221	1757.655218	19.771559
53.832778	1763.583005	19.776576
54.168439	1759.294921	19.781594
54.271381	1776.750315	19.786611
54.070467	1780.830819	19.791629
54.256853	1779.296066	19.796647
54.453201	1784.340032	19.801664
54.490835	1775.535047	19.806682
54.305851	1778.530544	19.811699
54.372628	1789.452366	19.816717
54.183368	1805.274571	19.821735
54.761262	1802.962061	19.826752
54.977112	1803.414135	19.831770
55.125200	1804.100902	19.836787
55.306313	1798.151711	19.841805
55.126253	1797.709542	19.846823
55.328528	1804.153855	19.851840
55.200531	1798.754900	19.856858
54.956256	1805.344921	19.861875
55.142331	1794.604126	19.866893
55.159169	1802.598689	19.871911
55.092897	1801.131924	19.876928
55.513021	1815.148103	19.881946
55.619905	1822.156515	19.886963
55.528570	1824.222102	19.891981
55.673619	1825.430088	19.896999
55.605409	1814.587100	19.902016
55.714267	1817.006355	19.907034
55.615391	1824.536187	19.912051
55.464772	1820.352681	19.917069
55.585472	1826.443685	19.922087
55.492531	1820.821466	19.927104
55.891245	1819.739469	19.932122
55.894638	1823.207266	19.937139
55.855986	1825.488676	19.942157
56.244171	1835.634286	19.947175
56.149075	1836.030929	19.952192
56.457530	1837.005018	19.957210
56.311251	1839.101307	19.962227
56.413549	1835.619836	19.967245
56.464360	1840.001764	19.972263
56.207106	1839.205589	19.977280
56.251949	1842.060940	19.982298
56.193116	1837.468546	19.987315
56.519230	1839.459263	19.992333
56.196411	1835.785603	19.997351
56.415908	1842.410281	20.002368
56.529196	1851.787872	20.007386
56.242819	1864.567160	20.012403
56.611287	1854.731935	20.017421
57.075150	1859.500464	20.022439
56.730994	1870.928563	20.027456
56.922517	1862.118361	20.032474
57.343800	1876.601498	20.037491
57.191142	1882.050492	20.042509
57.589496	1885.541633	20.047527
57.521548	1879.943883	20.052544
57.721985	1865.918527	20.057562
57.533101	1861.958772	20.062579
57.444899	1856.474664	20.067597
57.697855	1852.609798	20.072615
57.259052	1853.918730	20.077632
57.512747	1861.185041	20.082650
57.769140	1877.376174	20.087667
58.062808	1884.207013	20.092685
58.282365	1877.891985	20.097703
58.352674	1878.972821	20.102720
58.429454	1858.777876	20.107738
58.067818	1858.566139	20.112755
58.182594	1847.441980	20.117773
58.144647	1850.878387	20.122791
57.697111	1854.476803	20.127808
57.813912	1858.965169	20.132826
58.130325	1872.454806	20.137843
58.060320	1885.717797	20.142861
58.177168	1864.465611	20.147879
58.628113	1874.774993	20.152896
58.305346	1879.111312	20.157914
58.665048	1881.686948	20.162931
58.457084	1881.261772	20.167949
58.629976	1880.221465	20.172967
58.402652	1891.372478	20.177984
58.887050	1891.201770	20.183002
58.889921	1901.698141	20.188019
58.600585	1909.917460	20.193037
58.862843	1895.787714	20.198055
58.916483	1899.001483	20.203072
58.752768	1900.488241	20.208090
58.995933	1900.178590	20.213107
58.983871	1899.290345	20.218125
58.714284	1912.253241	20.223143
58.653438	1923.015247	20.228160
58.884357	1928.602988	20.233178
59.032517	1917.823874	20.238195
59.581177	1938.958962	20.243213
60.022309	1950.519715	20.248231
59.724161	1935.748694	20.253248
59.554905	1927.582008	20.258266
59.527699	1933.686754	20.263283
59.807992	1938.417788	20.268301
59.883857	1937.578886	20.273319
59.850087	1945.268995	20.278336
60.563730	1948.492984	20.283354
60.250820	1937.170670	20.288371
59.783944	1923.653792	20.293389
60.347246	1933.677341	20.298407
59.993939	1945.441460	20.303424
60.294321	1942.055175	20.308442
60.013030	1946.577530	20.313459
60.005824	1946.237673	20.318477
60.178814	1944.575608	20.323495
59.973967	1938.768897	20.328512
60.490280	1944.880016	20.333530
60.517860	1949.133057	20.338547
60.282249	1956.122593	20.343565
60.555389	1958.064814	20.348583
60.771908	1958.687214	20.353600
61.064028	1965.202722	20.358618
60.812653	1967.596379	20.363635
60.941659	1969.693737	20.368653
60.954071	1960.040482	20.373671
60.956310	1965.818709	20.378688
60.848812	1965.365167	20.383706
60.983094	1963.109516	20.388723
61.475729	1973.409267	20.393741
61.295409	1975.397287	20.398759
61.477316	1982.195177	20.403776
61.677554	1980.756074	20.408794
61.619299	1976.075185	20.413811
61.585539	1986.309081	20.418829
61.971741	1982.063523	20.423847
61.501269	1976.800228	20.428864
61.427818	1979.639418	20.433882
61.817312	1987.405252	20.438899
61.525461	1980.980950	20.443917
61.815056	1976.305527	20.448935
61.968201	1977.575377	20.453952
61.952874	1975.737670	20.458970
62.050399	1982.662398	20.463987
62.004319	1980.561245	20.469005
62.287898	1985.140287	20.474023
62.580936	1994.739119	20.479040
62.423249	2008.741829	20.484058
62.932991	2008.986905	20.489075
62.589566	1997.129648	20.494093
62.686206	1980.390484	20.499111
62.344711	1989.681599	20.504128
62.862258	1999.324160	20.509146
62.574744	1997.046220	20.514163
62.755370	2000.637773	20.519181
63.234131	1994.449365	20.524199
63.154701	2009.888441	20.529216
63.117885	1999.731597	20.534234
63.096566	2000.473318	20.539251
62.477451	1996.038098	20.544269
62.463090	1994.190770	20.549287
62.755956	2009.479991	20.554304
63.158680	2014.943004	20.559322
62.958758	2020.011250	20.564339
62.928017	2027.413719	20.569357
63.154057	2023.534098	20.574375
62.810118	2012.917240	20.579392
63.435187	2030.871791	20.584410
63.269282	2035.660136	20.589427
63.183083	2049.247702	20.594445
63.566199	2046.265035	20.599463
63.455789	2049.068997	20.604480
63.554741	2055.065648	20.609498
63.880134	2063.226598	20.614515
63.899896	2077.987419	20.619533
64.078080	2071.502066	20.624551
63.895794	2074.853823	20.629568
64.176747	2076.996822	20.634586
64.169808	2070.351110	20.639603
64.158060	2078.454425	20.644621
64.386508	2060.356366	20.649639
64.387091	2066.453647	20.654656
64.323262	2068.855806	20.659674
64.614752	2066.597605	20.664691
64.389963	2094.680615	20.669709
65.126896	2087.908883	20.674727
65.124544	2093.034566	20.679744
64.911866	2098.177422	20.684762
65.008971	2091.196638	20.689779
64.783248	2083.742530	20.694797
65.288945	2090.808494	20.699815
65.327516	2086.118718	20.704832
65.084242	2084.269373	20.709850
65.534200	2082.907912	20.714867
65.524071	2090.764807	20.719885
65.438792	2083.487527	20.724903
65.378142	2086.798137	20.729920
65.104857	2085.338533	20.734938
65.648921	2082.144436	20.739955
65.231308	2089.768503	20.744973
65.205173	2071.072794	20.749991
64.914587	2085.620291	20.755008
65.519936	2104.982455	20.760026
65.602779	2097.031835	20.765043
65.722103	2113.370900	20.770061
65.708607	2101.884796	20.775079
66.068032	2118.293553	20.780096
66.139070	2121.343676	20.785114
66.267010	2130.068968	20.790131
66.255824	2135.978752	20.795149
66.313450	2123.316901	20.800167
66.361981	2123.716296	20.805184
66.275110	2136.079478	20.810202
66.486272	2131.826592	20.815219
66.311845	2131.639173	20.820237
66.460424	2127.301411	20.825255
66.701126	2133.219071	20.830272
66.484822	2142.190823	20.835290
66.838285	2151.717151	20.840307
67.025350	2156.330295	20.845325
67.047596	2147.956765	20.850343
66.906573	2148.928703	20.855360
67.157091	2151.035450	20.860378
67.441967	2151.325227	20.865395
67.126711	2153.861472	20.870413
67.320820	2155.503646	20.875431
67.708105	2155.528049	20.880448
67.313700	2151.994938	20.885466
67.393301	2147.750036	20.890483
66.995895	2151.716229	20.895501
67.885771	2166.104093	20.900519
68.154874	2165.452674	20.905536
68.099031	2182.447305	20.910554
67.964669	2171.806986	20.915571
67.916431	2175.513333	20.920589
68.064531	2170.853716	20.925607
67.687991	2170.489661	20.930624
67.751277	2168.952070	20.935642
68.019086	2166.615509	20.940659
67.712210	2174.190700	20.945677
67.778773	2174.650393	20.950695
68.558307	2190.213845	20.955712
68.352245	2200.926178	20.960730
68.550619	2201.519868	20.965747
68.495681	2205.590221	20.970765
68.637746	2201.243994	20.975783
68.407804	2187.257412	20.980800
68.404829	2202.179701	20.985818
68.547827	2190.624837	20.990835
68.694776	2199.596515	20.995853
68.715569	2207.379182	21.000871
68.862670	2217.329231	21.005888
68.395310	2225.898506	21.010906
68.985595	2219.626271	21.015923
68.957614	2218.513265	21.020941
68.803212	2228.715704	21.025959
69.354446	2240.912706	21.030976
69.272383	2249.216480	21.035994
69.611908	2242.383867	21.041011
69.476727	2247.486219	21.046029
69.500855	2244.326213	21.051047
69.898912	2249.745845	21.056064
69.770704	2240.474265	21.061082
70.212787	2234.578726	21.066099
70.023416	2241.614781	21.071117
69.817283	2239.639668	21.076135
69.844419	2249.059371	21.081152
70.073060	2268.849994	21.086170
70.258383	2264.556941	21.091187
70.025276	2264.590172	21.096205
70.317553	2259.494495	21.101223
70.627788	2255.030381	21.106240
70.278114	2253.933057	21.111258
70.763488	2265.764819	21.116275
70.497477	2259.147003	21.121293
70.596777	2258.683146	21.126311
70.389178	2275.884694	21.131328
70.649209	2285.690844	21.136346
71.350109	2283.276946	21.141363
70.959795	2289.287209	21.146381
71.250540	2275.073800	21.151399
71.348023	2283.160094	21.156416
71.215806	2287.889573	21.161434
71.369570	2291.785223	21.166451
71.195380	2291.114882	21.171469
71.449134	2280.773486	21.176487
71.510864	2284.487876	21.181504
71.269938	2284.339278	21.186522
71.720353	2292.780575	21.191539
71.667386	2299.530169	21.196557
71.627477	2305.602314	21.201575
72.113544	2313.277414	21.206592
71.890615	2311.974019	21.211610
72.023204	2309.485039	21.216627
71.835222	2308.397096	21.221645
71.887244	2309.938458	21.226663
72.256923	2300.948637	21.231680
71.804420	2301.161422	21.236698
72.179158	2308.983362	21.241715
71.886579	2322.366761	21.246733
72.060874	2327.521644	21.251751
72.637104	2325.442884	21.256768
72.245229	2326.018591	21.261786
71.898612	2320.511705	21.266803
72.181164	2331.235934	21.271821
72.300808	2343.951948	21.276839
72.717917	2344.410378	21.281856
72.549496	2356.780176	21.286874
72.928214	2361.776797	21.291891
73.447408	2377.374889	21.296909
73.164409	2374.799518	21.301927
73.238376	2369.643330	21.306944
73.374576	2376.180261	21.311962
73.277425	2369.554884	21.316979
73.358951	2369.374703	21.321997
73.446153	2365.964929	21.327015
73.889059	2366.990575	21.332032
73.818852	2368.036645	21.337050
74.037015	2369.463611	21.342067
73.743600	2362.922640	21.347085
73.544809	2361.217789	21.352103
74.012490	2363.779736	21.357120
73.383755	2380.009003	21.362138
74.060499	2378.047046	21.367155
73.607281	2386.948729	21.372173
73.842655	2396.275917	21.377191
74.323152	2392.659338	21.382208
74.481433	2389.661343	21.387226
74.592094	2403.887431	21.392243
74.882906	2403.658680	21.397261
74.477838	2412.442367	21.402279
75.069894	2411.431043	21.407296
74.909993	2418.513047	21.412314
75.122673	2414.875301	21.417331
75.096132	2420.074301	21.422349
74.800041	2415.462121	21.427367
75.239507	2410.763105	21.432384
74.810201	2419.074020	21.437402
74.982762	2415.947538	21.442419
75.203987	2409.114460	21.447437
75.005534	2413.144223	21.452455
75.337629	2418.201818	21.457472
75.547931	2431.291894	21.462490
75.509265	2440.860875	21.467507
75.737002	2436.397017	21.472525
75.492416	2444.410732	21.477543
75.661995	2440.195850	21.482560
75.808423	2437.180768	21.487578
75.634130	2440.341973	21.492595
76.115892	2443.823314	21.497613
75.921486	2451.298940	21.502631
76.155987	2455.109386	21.507648
76.107035	2457.676541	21.512666
76.380551	2461.903796	21.517683
76.311838	2459.746167	21.522701
76.402134	2469.389643	21.527719
76.479845	2465.940307	21.532736
76.481044	2483.630102	21.537754
76.615191	2494.705918	21.542771
77.163894	2487.430143	21.547789
76.757843	2493.468188	21.552807
76.787654	2488.991141	21.557824
76.686215	2499.488423	21.562842
76.528684	2492.421134	21.567859
77.165529	2492.261257	21.572877
77.037014	2506.891010	21.577895
77.304225	2508.556481	21.582912
77.384139	2510.535349	21.587930
77.273198	2512.462060	21.592947
77.633726	2509.609103	21.597965
77.289768	2509.451396	21.602983
77.529347	2511.446279	21.608000
77.472686	2533.491190	21.613018
77.340555	2546.161578	21.618035
77.909723	2527.886578	21.623053
77.795960	2534.816217	21.628071
78.217549	2534.248205	21.633088
78.127927	2531.797165	21.638106
78.189632	2535.994500	21.643123
78.374525	2530.227533	21.648141
78.112939	2548.507731	21.653159
78.617069	2550.016154	21.658176
78.641112	2563.915076	21.663194
78.421303	2557.637086	21.668211
78.725702	2555.042251	21.673229
78.735330	2558.439778	21.678247
78.683700	2549.900891	21.683264
78.626480	2561.095101	21.688282
78.619797	2559.707310	21.693299
79.040710	2571.823959	21.698317
79.424913	2579.770781	21.703335
79.448660	2572.245823	21.708352
79.340761	2579.414427	21.713370
79.027783	2585.905031	21.718387
79.242793	2569.067871	21.723405
79.478403	2573.020194	21.728423
79.261478	2578.716178	21.733440
79.757390	2587.260951	21.738458
79.820896	2601.324151	21.743475
79.979233	2593.948529	21.748493
79.835979	2600.220022	21.753511
80.241234	2599.411543	21.758528
80.051486	2589.868526	21.763546
80.233800	2590.758269	21.768563
80.821690	2603.243298	21.773581
80.358920	2598.726619	21.778599
80.461498	2594.496950	21.783616
80.217278	2597.492393	21.788634
80.488414	2600.508092	21.793651
80.675328	2610.366905	21.798669
80.661698	2626.080254	21.803687
80.816818	2626.425087	21.808704
80.677620	2620.519497	21.813722
80.941604	2611.334619	21.818739
80.956458	2616.678686	21.823757
80.904855	2623.475530	21.828775
81.105563	2642.302002	21.833792
81.475754	2635.742179	21.838810
81.210820	2649.598068	21.843827
81.500650	2641.520095	21.848845
81.379703	2643.145396	21.853863
81.540725	2637.031800	21.858880
81.722051	2644.174054	21.863898
81.524093	2649.551472	21.868915
82.048849	2653.218644	21.873933
81.918235	2671.614162	21.878951
82.056773	2668.997955	21.883968
82.507704	2654.014296	21.888986
82.374143	2665.050099	21.894003
82.407698	2665.483415	21.899021
82.439474	2662.634598	21.904039
82.256914	2665.216402	21.909056
82.662980	2659.162249	21.914074
81.947901	2656.496724	21.919091
82.495710	2665.147025	21.924109
82.565306	2685.843597	21.929127
82.513870	2681.189861	21.934144
82.780566	2684.970062	21.939162
82.816258	2680.274270	21.944179
83.209608	2683.409707	21.949197
83.217992	2699.555222	21.954215
83.146524	2709.101080	21.959232
83.263349	2712.077850	21.964250
83.007220	2713.235129	21.969267
83.487587	2703.296696	21.974285
83.351646	2712.464448	21.979303
83.275477	2710.677228	21.984320
83.724618	2708.043914	21.989338
83.177566	2728.644620	21.994355
83.858970	2729.617141	21.999373
83.849954	2736.530446	22.004391
83.685500	2733.677643	22.009408
84.110346	2728.974525	22.014426
84.260538	2736.402593	22.019443
84.402729	2741.234382	22.024461
84.379997	2756.766213	22.029479
84.379553	2758.719824	22.034496
84.402769	2758.028005	22.039514
83.901603	2759.744447	22.044531
84.288455	2756.426525	22.049549
84.577720	2776.422831	22.054567
84.792531	2786.930700	22.059584
84.812177	2779.911287	22.064602
84.890750	2787.356909	22.069619
85.189988	2782.064312	22.074637
85.177772	2779.345461	22.079655
85.458900	2801.082126	22.084672
86.024390	2800.898710	22.089690
85.322801	2807.137814	22.094707
85.580621	2803.025802	22.099725
85.806929	2796.100253	22.104743
85.738798	2800.251712	22.109760
85.682981	2798.587542	22.114778
86.075082	2795.896873	22.119795
86.424747	2791.505354	22.124813
86.146342	2795.733943	22.129831
85.960012	2796.230117	22.134848
86.274116	2800.754088	22.139866
86.226108	2810.406790	22.144883
86.271121	2808.231301	22.149901
86.388631	2826.944753	22.154919
86.212023	2827.660338	22.159936
86.593393	2821.423785	22.164954
86.401426	2825.496809	22.169971
86.607320	2840.803521	22.174989
86.577248	2851.564416	22.180007
86.860978	2845.655615	22.185024
86.972041	2841.563431	22.190042
87.135181	2856.232991	22.195059
87.400344	2859.884065	22.200077
87.714844	2872.172244	22.205095
87.200657	2877.681334	22.210112
87.902579	2872.918988	22.215130
87.343797	2870.355190	22.220147
88.006821	2872.634111	22.225165
88.122625	2866.117216	22.230183
87.604970	2862.953610	22.235200
88.330869	2872.447222	22.240218
87.798124	2868.468523	22.245235
87.935320	2877.524129	22.250253
87.719972	2886.458225	22.255271
87.900446	2896.173019	22.260288
88.214290	2896.521396	22.265306
88.366236	2906.433193	22.270323
88.682318	2918.979965	22.275341
88.608826	2920.386389	22.280359
88.329939	2928.137414	22.285376
88.576094	2914.230329	22.290394
88.308526	2925.637625	22.295411
88.680990	2934.441777	22.300429
89.007274	2941.122725	22.305447
89.047457	2955.022575	22.310464
89.372816	2941.109373	22.315482
89.446889	2942.382213	22.320499
89.383590	2939.220002	22.325517
89.684271	2947.943877	22.330535
89.825260	2970.150884	22.335552
90.043129	2970.706829	22.340570
89.924835	2967.657384	22.345587
90.116778	2963.631407	22.350605
90.159366	2955.835058	22.355623
89.917572	2960.367258	22.360640
90.114193	2962.804480	22.365658
89.840055	2967.894087	22.370675
90.031466	2966.642508	22.375693
90.126653	2966.087747	22.380711
90.323120	2990.637471	22.385728
90.547751	2980.663204	22.390746
90.510924	2995.099083	22.395763
90.523806	2989.639822	22.400781
91.090550	2989.759206	22.405799
90.729185	2994.651020	22.410816
91.239513	2993.665096	22.415834
90.962315	3010.215441	22.420851
91.462378	3008.170633	22.425869
91.708038	3018.134090	22.430887
91.665045	3020.533112	22.435904
91.981209	3015.184139	22.440922
91.625584	3010.303384	22.445939
92.013516	3007.423963	22.450957
91.877396	3005.608232	22.455975
91.713225	3005.169854	22.460992
91.581700	3004.211896	22.466010
91.825539	3016.107247	22.471027
91.854982	3032.249760	22.476045
91.926758	3033.841745	22.481063
91.840421	3041.054498	22.486080
92.411636	3039.935940	22.491098
92.268428	3048.659971	22.496115
92.197786	3047.998627	22.501133
92.341052	3053.471048	22.506151
92.533564	3059.213503	22.511168
92.840302	3074.002773	22.516186
92.884379	3080.544925	22.521203
92.917219	3086.047281	22.526221
93.086208	3078.126920	22.531239
92.730543	3083.582830	22.536256
93.638627	3088.521970	22.541274
93.418817	3101.664138	22.546291
93.200585	3105.024873	22.551309
93.586913	3108.139392	22.556327
93.650229	3108.482837	22.561344
93.649062	3108.034699	22.566362
93.768869	3129.216286	22.571379
93.630474	3135.796515	22.576397
93.921716	3127.497167	22.581415
93.681374	3133.818774	22.586432
94.167993	3139.221646	22.591450
94.357806	3143.099209	22.596467
94.604465	3144.231398	22.601485
94.704720	3149.151930	22.606503
94.597228	3149.932449	22.611520
94.577337	3153.369431	22.616538
94.277101	3164.254902	22.621555
94.579711	3167.852829	22.626573
95.007648	3167.492118	22.631591
94.682746	3173.836455	22.636608
94.796672	3176.214069	22.641626
95.272061	3186.340471	22.646643
95.537538	3195.799077	22.651661
96.049967	3196.409881	22.656679
96.000324	3199.920971	22.661696
95.900240	3202.130117	22.666714
95.939043	3205.112880	22.671731
95.722172	3201.684307	22.676749
96.315449	3200.073064	22.681767
95.918646	3205.276642	22.686784
95.909844	3200.644499	22.691802
96.650568	3188.676569	22.696819
96.239031	3197.265960	22.701837
96.672278	3190.355183	22.706855
96.541175	3193.247783	22.711872
96.212764	3204.895193	22.716890
96.280203	3211.316951	22.721907
96.007240	3226.010948	22.726925
96.539329	3222.149405	22.731943
96.419090	3242.649106	22.736960
96.788161	3249.721155	22.741978
96.829380	3249.367373	22.746995
96.774806	3269.152968	22.752013
97.272845	3266.698135	22.757031
97.337261	3275.746406	22.762048
97.461123	3275.142956	22.767066
97.460242	3283.955271	22.772083
97.474793	3298.888347	22.777101
97.935639	3296.641338	22.782119
97.912537	3304.788015	22.787136
97.814189	3306.302521	22.792154
97.945545	3303.324376	22.797171
98.138723	3326.558904	22.802189
98.239344	3327.546703	22.807207
98.471372	3331.657570	22.812224
98.751003	3319.872263	22.817242
98.788783	3324.048280	22.822259
98.659808	3325.034174	22.827277
99.132666	3328.696993	22.832295
99.057239	3344.654214	22.837312
99.546609	3345.439075	22.842330
99.383210	3354.131698	22.847347
99.286238	3351.609103	22.852365
99.394582	3343.350937	22.857383
99.593613	3347.615323	22.862400
99.812055	3339.778632	22.867418
100.138430	3341.400195	22.872435
99.717188	3346.724425	22.877453
100.129834	3345.116219	22.882471
99.733223	3343.720018	22.887488
99.833415	3351.124611	22.892506
100.111246	3359.192602	22.897523
100.092108	3369.030457	22.902541
100.117321	3369.266250	22.907559
100.181861	3371.869411	22.912576
100.673416	3370.643376	22.917594
100.625027	3393.448706	22.922611
100.712918	3401.726383	22.927629
100.901240	3397.909193	22.932647
100.790362	3406.309546	22.937664
100.636475	3396.618449	22.942682
100.806423	3396.626409	22.947699
100.993923	3420.108138	22.952717
101.446073	3415.387941	22.957735
101.008969	3423.571126	22.962752
101.404884	3430.418100	22.967770
101.607467	3428.224163	22.972787
101.671371	3443.430537	22.977805
101.881170	3445.616413	22.982823
101.998279	3449.761093	22.987840
101.682623	3443.788189	22.992858
102.008866	3449.314127	22.997875
101.791156	3449.900454	23.002893
102.313889	3457.302017	23.007911
102.204304	3470.168366	23.012928
102.490007	3467.629990	23.017946
102.428588	3468.823093	23.022963
102.332940	3466.215054	23.027981
102.700665	3488.188329	23.032999
102.922630	3490.416493	23.038016
102.821412	3495.526500	23.043034
103.201047	3492.398955	23.048051
102.711536	3502.130665	23.053069
102.921017	3509.445606	23.058087
103.530268	3520.400273	23.063104
103.479800	3517.220168	23.068122
103.896835	3513.692222	23.073139
103.485355	3523.418031	23.078157
103.646684	3531.264472	23.083175
103.953645	3542.225480	23.088192
103.907565	3552.073967	23.093210
103.966557	3552.307627	23.098227
103.989221	3552.297630	23.103245
103.838473	3547.438287	23.108263
104.197867	3560.426917	23.113280
104.059997	3569.147206	23.118298
104.668434	3571.690435	23.123315
104.778511	3585.838639	23.128333
105.083670	3585.869603	23.133351
105.114433	3589.971030	23.138368
104.929189	3595.526646	23.143386
104.978449	3585.936187	23.148403
105.267772	3594.766314	23.153421
105.787365	3606.113840	23.158439
105.679004	3609.902496	23.163456
105.965711	3616.482581	23.168474
106.304907	3611.937847	23.173491
105.944093	3610.753804	23.178509
106.225079	3613.597690	23.183527
106.430117	3611.848389	23.188544
106.628364	3614.916712	23.193562
106.570098	3610.869821	23.198579
106.319580	3618.269498	23.203597
106.435707	3613.908059	23.208615
106.452558	3617.399343	23.213632
106.569494	3612.273946	23.218650
106.896674	3618.509963	23.223667
106.908571	3641.744891	23.228685
106.981121	3640.732832	23.233703
107.244405	3643.708906	23.238720
106.888842	3642.281000	23.243738
107.324498	3636.158762	23.248755
107.125229	3660.566234	23.253773
107.238536	3659.920236	23.258791
107.523290	3653.951043	23.263808
107.314406	3668.941525	23.268826
107.686018	3675.890246	23.273843
107.932945	3690.206473	23.278861
107.885036	3697.511312	23.283879
108.148131	3693.814912	23.288896
108.123165	3698.206009	23.293914
108.337707	3705.671740	23.298931
108.386306	3715.578079	23.303949
108.253036	3716.589917	23.308967
108.471237	3718.449407	23.313984
108.718360	3726.601283	23.319002
108.738108	3733.280049	23.324019
108.934790	3740.123635	23.329037
108.863070	3742.672445	23.334055
109.228480	3734.026628	23.339072
108.988907	3740.910155	23.344090
109.029208	3750.735748	23.349107
109.355007	3766.583135	23.354125
109.493011	3772.773091	23.359143
109.457829	3766.595164	23.364160
109.849318	3790.241110	23.369178
109.661552	3786.293378	23.374195
109.492757	3802.767491	23.379213
110.197869	3800.772539	23.384231
110.377780	3813.155042	23.389248
110.347860	3822.107892	23.394266
110.818426	3824.429718	23.399283
110.757764	3825.600631	23.404301
110.963407	3820.726412	23.409319
110.898776	3817.220211	23.414336
110.772671	3826.345951	23.419354
110.814535	3819.363687	23.424371
110.771786	3832.169320	23.429389
110.892823	3839.371996	23.434407
111.194758	3843.304741	23.439424
111.220604	3860.878393	23.444442
111.425399	3862.405422	23.449459
111.477234	3876.957525	23.454477
111.724610	3870.716356	23.459495
112.147320	3884.307637	23.464512
111.605005	3891.636355	23.469530
112.019335	3885.002885	23.474547
111.859632	3888.632355	23.479565
112.080797	3909.372865	23.484583
112.353545	3909.257403	23.489600
111.973683	3925.408023	23.494618
112.442438	3924.731580	23.499635
112.846634	3932.811596	23.504653
112.721022	3930.899432	23.509671
113.063805	3936.094665	23.514688
113.126702	3954.180250	23.519706
113.483210	3948.603738	23.524723
113.542243	3958.167684	23.529741
113.420193	3963.883957	23.534759
113.974776	3960.457475	23.539776
113.850953	3958.387210	23.544794
113.420414	3956.589100	23.549811
114.278511	3976.614405	23.554829
113.991170	3984.521866	23.559847
114.388519	3983.853452	23.564864
114.219268	3986.480703	23.569882
114.750709	3995.348849	23.574899
114.482595	3989.816523	23.579917
114.331171	4000.830686	23.584935
115.174145	3989.963579	23.589952
114.604679	4002.189008	23.594970
115.119035	4008.885079	23.599987
114.883053	4009.426940	23.605005
115.156556	4027.050332	23.610023
115.703775	4027.456864	23.615040
115.583290	4035.385553	23.620058
115.422747	4037.269692	23.625075
115.845570	4040.391284	23.630093
115.540798	4042.749386	23.635111
116.105272	4044.781921	23.640128
115.812416	4057.727902	23.645146
115.548369	4057.955363	23.650163
115.933775	4074.765856	23.655181
116.052135	4089.680163	23.660199
116.561524	4088.145118	23.665216
116.467522	4088.216526	23.670234
116.512670	4085.573714	23.675251
116.895451	4094.809247	23.680269
116.802313	4114.961639	23.685287
117.108252	4123.091853	23.690304
117.088807	4115.371010	23.695322
117.384665	4107.745966	23.700339
117.398267	4114.318518	23.705357
117.365427	4133.814418	23.710375
117.651960	4135.221347	23.715392
117.473617	4147.473976	23.720410
117.838658	4147.937462	23.725427
117.901483	4143.508493	23.730445
117.735151	4163.808131	23.735463
118.471694	4164.434364	23.740480
118.096857	4180.773809	23.745498
118.385395	4162.992504	23.750515
118.621178	4168.835852	23.755533
118.739074	4194.731532	23.760551
118.848028	4189.765045	23.765568
118.799653	4192.010398	23.770586
118.926584	4191.497975	23.775603
119.481044	4190.060022	23.780621
119.451150	4192.330889	23.785639
119.523195	4200.463062	23.790656
119.506724	4207.318124	23.795674
119.605360	4215.932229	23.800691
119.811797	4216.117547	23.805709
119.383580	4217.772187	23.810727
120.012518	4223.456110	23.815744
119.706422	4229.946219	23.820762
120.085132	4234.722416	23.825779
120.235864	4243.694519	23.830797
120.375207	4254.063558	23.835815
120.593659	4258.656544	23.840832
120.754841	4261.696063	23.845850
120.822136	4262.225138	23.850867
120.988829	4264.076972	23.855885
121.024341	4276.646550	23.860903
121.360545	4277.070367	23.865920
121.421756	4293.616209	23.870938
121.295846	4280.744869	23.875955
121.722175	4277.521496	23.880973
122.033463	4302.979851	23.885991
122.032578	4297.263525	23.891008
122.444780	4304.979461	23.896026
122.150238	4300.540156	23.901043
122.332103	4307.970222	23.906061
122.162664	4307.324309	23.911079
122.362735	4305.708292	23.916096
122.528669	4315.921691	23.921114
122.472134	4328.714051	23.926131
122.600875	4327.794158	23.931149
122.550961	4335.254235	23.936167
122.790311	4344.878516	23.941184
123.041680	4356.123340	23.946202
123.229557	4360.509659	23.951219
123.615779	4354.341267	23.956237
123.057964	4362.670041	23.961255
123.604938	4380.932730	23.966272
123.749350	4393.141272	23.971290
123.874100	4384.169858	23.976307
124.510822	4397.620678	23.981325
124.179727	4405.986551	23.986343
124.449161	4406.761730	23.991360
124.617217	4408.887979	23.996378
124.348711	4414.160180	24.001395
124.470980	4403.948652	24.006413
124.666391	4404.602857	24.011431
124.487829	4411.508643	24.016448
124.721141	4425.944373	24.021466
124.789020	4437.281124	24.026483
124.966780	4426.628453	24.031501
125.139612	4444.432160	24.036519
125.215265	4450.698403	24.041536
125.105473	4464.383016	24.046554
125.565371	4464.809555	24.051571
125.674823	4482.159226	24.056589
125.534267	4488.096359	24.061607
125.767737	4477.419148	24.066624
125.968297	4495.572087	24.071642
125.937774	4503.376408	24.076659
126.288590	4504.741731	24.081677
126.596809	4519.462510	24.086695
126.511693	4524.844897	24.091712
126.867052	4535.300201	24.096730
126.750218	4546.602828	24.101747
127.411591	4537.496764	24.106765
127.453880	4554.689732	24.111783
127.385232	4561.985543	24.116800
127.538831	4557.750580	24.121818
127.557441	4558.372516	24.126835
127.735354	4558.322414	24.131853
127.645112	4575.450939	24.136871
127.946838	4583.278998	24.141888
128.374829	4585.528682	24.146906
128.096013	4584.896738	24.151923
128.813957	4589.449433	24.156941
128.418189	4598.646216	24.161959
128.798715	4596.405323	24.166976
128.992725	4608.637806	24.171994
128.678748	4615.678517	24.177011
129.025416	4615.087466	24.182029
128.792444	4624.113558	24.187047
128.580465	4623.224934	24.192064
128.876806	4631.776697	24.197082
128.760270	4653.385343	24.202099
129.078213	4653.584763	24.207117
129.308705	4678.803781	24.212135
129.709905	4686.534231	24.217152
129.890538	4683.399785	24.222170
129.994943	4704.863401	24.227187
130.348322	4712.449840	24.232205
130.292645	4719.459595	24.237223
130.334034	4714.292062	24.242240
131.138870	4738.793036	24.247258
130.954558	4737.300332	24.252275
131.129980	4729.624455	24.257293
130.764225	4738.011692	24.262311
131.195934	4736.902270	24.267328
131.618417	4741.201422	24.272346
131.507647	4756.407853	24.277363
131.587073	4762.187507	24.282381
131.793008	4759.342642	24.287399
131.784043	4755.458224	24.292416
131.957933	4780.140172	24.297434
132.122427	4788.548526	24.302451
132.381459	4785.133475	24.307469
132.188644	4787.388904	24.312487
132.623616	4794.725856	24.317504
132.699275	4802.696749	24.322522
132.843964	4813.298854	24.327539
133.159611	4809.979094	24.332557
133.403351	4805.935128	24.337575
133.018459	4814.956705	24.342592
133.626404	4819.312047	24.347610
133.335795	4830.064428	24.352627
133.661862	4831.777717	24.357645
133.639060	4839.104334	24.362663
133.730431	4848.152323	24.367680
133.897787	4839.293960	24.372698
133.915578	4851.390073	24.377715
134.159454	4857.551188	24.382733
134.174935	4871.273298	24.387751
134.175586	4870.610186	24.392768
134.582095	4880.356922	24.397786
134.408707	4884.165500	24.402803
134.442299	4883.689777	24.407821
134.568746	4896.352859	24.412839
134.664828	4907.313011	24.417856
135.216152	4907.321199	24.422874
135.273055	4931.639737	24.427891
135.745159	4933.791015	24.432909
135.958972	4937.434776	24.437927
135.834305	4951.134710	24.442944
136.046234	4937.165155	24.447962
135.998365	4945.019731	24.452979
136.164347	4958.156460	24.457997
136.291886	4971.204524	24.463015
136.521821	4972.541473	24.468032
136.616204	4982.624411	24.473050
136.597441	4989.142374	24.478067
136.833063	4994.285257	24.483085
137.000897	4994.527137	24.488103
137.077908	5009.846406	24.493120
137.502847	5014.820746	24.498138
137.619899	5027.677943	24.503155
137.795191	5027.543023	24.508173
137.613597	5026.589643	24.513191
137.841441	5035.745764	24.518208
138.068455	5046.347734	24.523226
138.012673	5041.375257	24.528243
138.230700	5039.162927	24.533261
138.535939	5052.827152	24.538279
138.535234	5063.641575	24.543296
138.892756	5062.761562	24.548314
138.516876	5067.207965	24.553331
138.970465	5076.256139	24.558349
138.866456	5090.546379	24.563367
139.148151	5093.784964	24.568384
139.636575	5098.809356	24.573402
139.392557	5123.273148	24.578419
139.631772	5122.948287	24.583437
139.734486	5129.415703	24.588455
139.797163	5130.854626	24.593472
140.199462	5144.131236	24.598490
140.082309	5153.489826	24.603507
140.522104	5144.803281	24.608525
140.679539	5150.239394	24.613543
140.697171	5169.068766	24.618560
141.118352	5178.582933	24.623578
140.665584	5184.338772	24.628595
140.842679	5174.402319	24.633613
141.295588	5191.878785	24.638631
141.560780	5209.312075	24.643648
141.567088	5199.901108	24.648666
141.789442	5198.663472	24.653683
141.656787	5201.818630	24.658701
142.077703	5221.276172	24.663719
141.721207	5222.436701	24.668736
141.917374	5221.613525	24.673754
142.241842	5244.302787	24.678771
142.599072	5259.202728	24.683789
142.742020	5261.755998	24.688807
142.336037	5257.968395	24.693824
142.803469	5270.994991	24.698842
142.692595	5271.214250	24.703859
143.074363	5278.736505	24.708877
143.005668	5278.418844	24.713895
143.089646	5292.853406	24.718912
143.419275	5301.804318	24.723930
143.159703	5309.253446	24.728947
143.322345	5329.938457	24.733965
143.818838	5333.389651	24.738983
143.809865	5345.130429	24.744000
143.909223	5352.968428	24.749018
144.307560	5367.770475	24.754035
144.234744	5365.430056	24.759053
144.788679	5385.078428	24.764071
144.316987	5391.244503	24.769088
144.847030	5392.603914	24.774106
144.956028	5405.967701	24.779123
145.369969	5407.743039	24.784141
145.655292	5416.145380	24.789159
145.343504	5425.597734	24.794176
146.126993	5430.269799	24.799194
145.833490	5438.005236	24.804211
145.957284	5443.803409	24.809229
146.431214	5449.625646	24.814247
145.963403	5466.839413	24.819264
146.523751	5456.564979	24.824282
146.620175	5469.419406	24.829299
146.587848	5480.826167	24.834317
146.771959	5477.823621	24.839335
146.580706	5478.636300	24.844352
147.020596	5496.519150	24.849370
147.401191	5507.687622	24.854387
147.588279	5510.496015	24.859405
147.953189	5510.697558	24.864423
147.699638	5539.879449	24.869440
147.913514	5534.230103	24.874458
148.060821	5536.413399	24.879475
147.935213	5545.779827	24.884493
148.222861	5553.174891	24.889511
148.250425	5569.035852	24.894528
148.780034	5573.211095	24.899546
148.975960	5584.859950	24.904563
148.972394	5581.296491	24.909581
149.296379	5580.172332	24.914599
148.996035	5592.385067	24.919616
149.540294	5606.608873	24.924634
149.877790	5612.891315	24.929651
149.462781	5616.646354	24.934669
149.623119	5625.699708	24.939687
149.718705	5637.667357	24.944704
149.962516	5634.806953	24.949722
149.840946	5651.278493	24.954739
150.484811	5666.872526	24.959757
150.476048	5683.111767	24.964775
150.565726	5686.367913	24.969792
151.016225	5690.751292	24.974810
150.921454	5701.520852	24.979827
150.737611	5723.002414	24.984845
151.127532	5721.309181	24.989863
151.363811	5733.302202	24.994880
151.628376	5740.044365	24.999898
151.639397	5757.344379	25.004915
151.865585	5746.752801	25.009933
152.230520	5764.028943	25.014951
152.408680	5778.073486	25.019968
152.469537	5767.978146	25.024986
152.634133	5780.711627	25.030003
152.419120	5780.704140	25.035021
153.122722	5792.529286	25.040039
152.919246	5805.800267	25.045056
153.213980	5799.039637	25.050074
153.494639	5813.589007	25.055091
153.383166	5821.621229	25.060109
153.659328	5829.340189	25.065127
153.892921	5837.517232	25.070144
153.962104	5835.148192	25.075162
154.071975	5845.494345	25.080179
154.168985	5852.909927	25.085197
154.600552	5857.536222	25.090215
154.631489	5857.243980	25.095232
154.706783	5869.814737	25.100250
154.636821	5875.656029	25.105267
154.819632	5885.321551	25.110285
154.820140	5884.087058	25.115303
155.252637	5904.392675	25.120320
155.224088	5903.964541	25.125338
155.430465	5910.122419	25.130355
155.357445	5926.570815	25.135373
155.859092	5932.821339	25.140391
155.656635	5933.784158	25.145408
156.271723	5949.449233	25.150426
156.568657	5959.684070	25.155443
156.389813	5961.318733	25.160461
156.891661	5985.136493	25.165479
156.732467	5984.892975	25.170496
156.899533	5983.711301	25.175514
157.231460	5995.171804	25.180531
157.365056	6014.526838	25.185549
157.636578	6009.297633	25.190567
157.517957	6016.011541	25.195584
157.816821	6029.447055	25.200602
157.923887	6041.987699	25.205619
157.890970	6043.451140	25.210637
158.271019	6052.975366	25.215655
158.133836	6061.744088	25.220672
158.534306	6070.630615	25.225690
158.818438	6088.727854	25.230707
158.978238	6089.892783	25.235725
159.016649	6099.246424	25.240743
159.015032	6121.722695	25.245760
159.274517	6121.539854	25.250778
159.405768	6129.549969	25.255795
159.702312	6143.781436	25.260813
159.893117	6151.368694	25.265831
159.726005	6150.706564	25.270848
160.066527	6163.378026	25.275866
160.312142	6175.325679	25.280883
160.617902	6178.614354	25.285901
160.419849	6191.928960	25.290919
160.671832	6203.118007	25.295936
161.032800	6204.627085	25.300954
161.247645	6216.102913	25.305971
161.461049	6229.176305	25.310989
161.463762	6224.816229	25.316007
161.390511	6235.308091	25.321024
161.460355	6241.888382	25.326042
161.605772	6250.009974	25.331059
161.994384	6269.798845	25.336077
162.451714	6275.756535	25.341095
162.760634	6287.274491	25.346112
162.529709	6288.273356	25.351130
163.032267	6300.439695	25.356147
163.067506	6310.150659	25.361165
163.196823	6304.713203	25.366183
163.005651	6313.670440	25.371200
163.334591	6322.786116	25.376218
163.772924	6325.043873	25.381235
163.568323	6332.203847	25.386253
163.813341	6329.744061	25.391271
163.939413	6344.696887	25.396288
163.658667	6354.021739	25.401306
164.319177	6352.248178	25.406323
164.631552	6373.968442	25.411341
164.557952	6397.131884	25.416359
164.690033	6382.744411	25.421376
164.807261	6394.857535	25.426394
164.906198	6402.064688	25.431411
165.195684	6412.894426	25.436429
165.244861	6420.822822	25.441447
165.549704	6436.439059	25.446464
165.819049	6437.511085	25.451482
165.801279	6450.592441	25.456499
166.136060	6466.857476	25.461517
166.235621	6469.395615	25.466535
166.256328	6476.094176	25.471552
166.536063	6484.191673	25.476570
167.066815	6485.967761	25.481587
166.543898	6508.718740	25.486605
167.125060	6514.464541	25.491623
166.670530	6522.550814	25.496640
166.988323	6541.786000	25.501658
167.365133	6552.908354	25.506675
167.558759	6565.776734	25.511693
167.722580	6576.449473	25.516711
168.201064	6588.247268	25.521728
168.387748	6597.249623	25.526746
168.445950	6601.457918	25.531763
168.555477	6609.730508	25.536781
168.931198	6620.041763	25.541799
168.924516	6627.628589	25.546816
169.392157	6643.153204	25.551834
169.641749	6653.162238	25.556851
169.763516	6659.624054	25.561869
169.572101	6654.085212	25.566887
170.079759	6669.347875	25.571904
169.973421	6673.935532	25.576922
170.309816	6671.802327	25.581939
170.081253	6686.880441	25.586957
170.497986	6696.654961	25.591975
170.669065	6710.568740	25.596992
171.320070	6726.143622	25.602010
171.337831	6726.759451	25.607027
171.312143	6739.637056	25.612045
171.423383	6740.424497	25.617063
171.456743	6740.210783	25.622080
171.202343	6754.778430	25.627098
171.897300	6757.731590	25.632115
171.854231	6776.714183	25.637133
172.092866	6789.181059	25.642151
172.386448	6796.547286	25.647168
172.343947	6810.971289	25.652186
172.760574	6807.281784	25.657203
172.720791	6832.950198	25.662221
172.959567	6836.584117	25.667239
173.212015	6844.739716	25.672256
173.147355	6865.200049	25.677274
173.567202	6868.120562	25.682292
173.814210	6888.011207	25.687309
173.769212	6887.326762	25.692327
173.979681	6893.042364	25.697344
174.107846	6916.869369	25.702362
174.768230	6921.835762	25.707380
174.721451	6927.493812	25.712397
174.925155	6928.348855	25.717415
175.147612	6927.840335	25.722432
175.205427	6949.935793	25.727450
175.436279	6947.822248	25.732468
175.360324	6947.884524	25.737485
175.481685	6967.570799	25.742503
176.074098	6975.038657	25.747520
175.996771	6980.625743	25.752538
176.311980	6987.950777	25.757556
176.439254	7006.720662	25.762573
176.525803	7009.630274	25.767591
176.751079	7014.181850	25.772608
176.365382	7026.134253	25.777626
176.754363	7031.559908	25.782644
176.998730	7057.812348	25.787661
177.058574	7062.377224	25.792679
177.965188	7071.292283	25.797696
177.777750	7091.999401	25.802714
178.016847	7093.934892	25.807732
178.286652	7094.978474	25.812749
178.434923	7106.831493	25.817767
178.811598	7111.640341	25.822784
178.491315	7131.771656	25.827802
178.753661	7120.999992	25.832820
178.950413	7138.976208	25.837837
179.050704	7150.334818	25.842855
179.373625	7154.864818	25.847872
179.485238	7171.809456	25.852890
179.847019	7167.272940	25.857908
179.887569	7179.417536	25.862925
179.648638	7187.404025	25.867943
179.861990	7206.400557	25.872960
179.956340	7218.520965	25.877978
180.272397	7228.440978	25.882996
180.712459	7253.412885	25.888013
180.534335	7255.060175	25.893031
181.120539	7271.343361	25.898048
181.289249	7286.378669	25.903066
181.465685	7294.091773	25.908084
181.566230	7300.667633	25.913101
181.927458	7329.752895	25.918119
182.268348	7327.442122	25.923136
182.196925	7333.618743	25.928154
182.227763	7352.142060	25.933172
182.366507	7369.581432	25.938189
182.332184	7374.489463	25.943207
183.366580	7383.469895	25.948224
183.207913	7401.378925	25.953242
183.359229	7405.651742	25.958260
183.413830	7412.578951	25.963277
183.621797	7419.898859	25.968295
184.126802	7441.186114	25.973312
184.260519	7439.596007	25.978330
184.349164	7443.026263	25.983348
184.618786	7455.362457	25.988365
184.696460	7468.117041	25.993383
185.282220	7462.427789	25.998400
185.008236	7483.830816	26.003418
185.039863	7494.575310	26.008436
185.395041	7507.115968	26.013453
185.194296	7524.053038	26.018471
185.852997	7514.286121	26.023488
186.102789	7539.979609	26.028506
186.223650	7552.768526	26.033524
186.136088	7556.359002	26.038541
186.751559	7574.456311	26.043559
187.237889	7583.064935	26.048576
187.037433	7582.524785	26.053594
187.274487	7576.804887	26.058612
187.512529	7581.730288	26.063629
187.311754	7592.520718	26.068647
187.564756	7601.532118	26.073664
187.751029	7600.918754	26.078682
187.767210	7613.894592	26.083700
188.045391	7622.384307	26.088717
187.939988	7635.562315	26.093735
188.563882	7640.462012	26.098752
188.188971	7653.893774	26.103770
188.244021	7679.816858	26.108788
188.578600	7691.221181	26.113805
188.918213	7704.105372	26.118823
189.230367	7712.880254	26.123840
189.340245	7732.452334	26.128858
189.309247	7748.674782	26.133876
189.710801	7764.299097	26.138893
189.823964	7772.596896	26.143911
190.352741	7789.792454	26.148928
190.524657	7802.497778	26.153946
190.689790	7816.792171	26.158964
191.103952	7820.253585	26.163981
191.235266	7831.178395	26.168999
191.501574	7842.034708	26.174016
191.574422	7858.458821	26.179034
191.638117	7856.829135	26.184052
191.737708	7869.173301	26.189069
192.187268	7881.194299	26.194087
192.411154	7889.632659	26.199104
192.494290	7907.939974	26.204122
192.675690	7922.427639	26.209140
192.967232	7920.465489	26.214157
193.161862	7939.721432	26.219175
193.698432	7931.940289	26.224192
193.840849	7957.878490	26.229210
194.013129	7963.445712	26.234228
193.944921	7968.318167	26.239245
193.779439	7980.590279	26.244263
194.312824	7988.165670	26.249280
194.220990	8001.149230	26.254298
194.796053	8020.550871	26.259316
194.786542	8027.804064	26.264333
194.950896	8040.671748	26.269351
195.247106	8047.987553	26.274368
195.268012	8058.573042	26.279386
195.596235	8073.088338	26.284404
195.910811	8080.249738	26.289421
196.115276	8101.445927	26.294439
196.234670	8103.921200	26.299456
196.595970	8114.955376	26.304474
196.447033	8121.295944	26.309492
196.939951	8132.606279	26.314509
196.913107	8150.785837	26.319527
197.023658	8154.904201	26.324544
197.280182	8170.374783	26.329562
197.450613	8176.223342	26.334580
197.612188	8188.450669	26.339597
197.836855	8218.654246	26.344615
198.291351	8217.837830	26.349632
198.220772	8224.241929	26.354650
198.152283	8241.651446	26.359668
198.478119	8255.390606	26.364685
198.457822	8264.966072	26.369703
198.761020	8279.280237	26.374720
199.237600	8283.707516	26.379738
199.037303	8312.768638	26.384756
199.611949	8319.346361	26.389773
199.732997	8335.842276	26.394791
200.038386	8351.766297	26.399808
200.223783	8359.345843	26.404826
200.689240	8377.899972	26.409844
200.927173	8375.163200	26.414861
200.793590	8388.219871	26.419879
201.000825	8399.609854	26.424896
201.472647	8413.566205	26.429914
201.477032	8419.336668	26.434932
201.583562	8434.499467	26.439949
201.958292	8446.500985	26.444967
202.395348	8453.419185	26.449984
202.137146	8461.604984	26.455002
202.403949	8462.519674	26.460020
202.885478	8468.193303	26.465037
203.092322	8489.351678	26.470055
203.245975	8498.394866	26.475072
203.085334	8513.801643	26.480090
203.496347	8523.830609	26.485108
203.728014	8530.209564	26.490125
203.639424	8554.022123	26.495143
203.834574	8560.498368	26.500160
204.200063	8576.874116	26.505178
204.386868	8584.213588	26.510196
204.850801	8599.847782	26.515213
204.816254	8612.469190	26.520231
205.013533	8629.234414	26.525248
205.216470	8644.735887	26.530266
205.503146	8654.042461	26.535284
206.060450	8655.555720	26.540301
205.686501	8675.766574	26.545319
206.148823	8686.286428	26.550336
206.144586	8693.687444	26.555354
206.238138	8727.540019	26.560372
206.664341	8727.094251	26.565389
206.883169	8752.529069	26.570407
206.914255	8758.374385	26.575424
207.474103	8780.049246	26.580442
207.061405	8793.260430	26.585460
207.757847	8802.067188	26.590477
208.231555	8821.485550	26.595495
208.468182	8832.501799	26.600512
208.784738	8833.822311	26.605530
208.803094	8855.073775	26.610548
209.416857	8870.321644	26.615565
209.486066	8860.027558	26.620583
209.614966	8874.738885	26.625600
209.630667	8893.386090	26.630618
209.721935	8901.649939	26.635636
210.163621	8912.179469	26.640653
210.224987	8930.620651	26.645671
210.279631	8932.559977	26.650688
210.748639	8954.331362	26.655706
210.893001	8955.445222	26.660724
210.925830	8960.800954	26.665741
210.860804	8971.918216	26.670759
211.294874	8995.759965	26.675776
211.404205	8995.493280	26.680794
211.512239	9021.776182	26.685812
211.870309	9036.123381	26.690829
212.131497	9055.995197	26.695847
212.337563	9058.198125	26.700864
212.825056	9069.105755	26.705882
212.802235	9089.931393	26.710900
213.075585	9088.906525	26.715917
213.315555	9113.571308	26.720935
213.486972	9114.485189	26.725952
213.671109	9130.173135	26.730970
213.840448	9141.231682	26.735988
213.866973	9161.336123	26.741005
214.173293	9178.867768	26.746023
214.209612	9185.157575	26.751040
214.609271	9193.771061	26.756058
214.324708	9220.848238	26.761076
214.697514	9217.499801	26.766093
214.866777	9255.878509	26.771111
214.958380	9260.053762	26.776128
215.953020	9280.458165	26.781146
215.811943	9297.573784	26.786164
216.325151	9309.478394	26.791181
216.324036	9326.038528	26.796199
216.435997	9334.419306	26.801216
216.699161	9344.364531	26.806234
216.885733	9368.880152	26.811252
217.453109	9375.560428	26.816269
217.332368	9396.496468	26.821287
217.512263	9402.707025	26.826304
218.199624	9415.635810	26.831322
218.374000	9440.589148	26.836340
218.649298	9437.180172	26.841357
218.774920	9449.903349	26.846375
218.982093	9456.324350	26.851392
219.197762	9476.983608	26.856410
219.630184	9491.540526	26.861428
219.794587	9496.225389	26.866445
219.908453	9505.079546	26.871463
220.062675	9515.367135	26.876480
220.181165	9521.391596	26.881498
220.353322	9541.587298	26.886516
220.220251	9551.670483	26.891533
220.836117	9569.419221	26.896551
220.913291	9579.141119	26.901568
221.282766	9593.174384	26.906586
221.113102	9620.609867	26.911604
221.452095	9631.859986	26.916621
221.664484	9652.883050	26.921639
222.207079	9671.505326	26.926656
222.605846	9687.927361	26.931674
222.578068	9701.552491	26.936692
222.887401	9712.017962	26.941709
223.190070	9722.977033	26.946727
223.365940	9733.826522	26.951744
223.489578	9737.261194	26.956762
223.813267	9758.380608	26.961780
224.214626	9774.972813	26.966797
224.344299	9783.452055	26.971815
224.581421	9803.148468	26.976832
224.966705	9806.542165	26.981850
224.884643	9823.484836	26.986868
225.244577	9828.379114	26.991885
225.485640	9843.190460	26.996903
225.807992	9861.427495	27.001920
225.849913	9866.573675	27.006938
225.872914	9887.955043	27.011956
226.251543	9895.252354	27.016973
226.450040	9908.346475	27.021991
226.614438	9922.036383	27.027008
226.933477	9935.351603	27.032026
227.092105	9958.445226	27.037044
227.252050	9965.855759	27.042061
227.973665	9978.590127	27.047079
227.440768	9993.371281	27.052096
228.131925	9999.852420	27.057114
228.471272	10016.625056	27.062132
228.553090	10032.468719	27.067149
228.662026	10034.080754	27.072167
228.602432	10059.567289	27.077184
229.114728	10058.820682	27.082202
229.145379	10076.882604	27.087220
229.260519	10089.832038	27.092237
229.432321	10108.617034	27.097255
229.627733	10118.045993	27.102272
230.432006	10146.036943	27.107290
230.597059	10156.288457	27.112308
230.583275	10167.379458	27.117325
230.996968	10179.230753	27.122343
231.137715	10206.217470	27.127360
231.375025	10205.873886	27.132378
231.687853	10219.648114	27.137396
231.634636	10233.874378	27.142413
232.209002	10241.854750	27.147431
232.078451	10273.834974	27.152448
232.907264	10278.226503	27.157466
232.938523	10295.928588	27.162484
233.214615	10299.105829	27.167501
233.737696	10309.973883	27.172519
233.910245	10323.634392	27.177536
234.247512	10323.837179	27.182554
234.135503	10346.114844	27.187572
234.234880	10346.957977	27.192589
234.764649	10358.788046	27.197607
234.568344	10384.927938	27.202624
234.999074	10390.104921	27.207642
235.385526	10404.470833	27.212660
235.474212	10420.705278	27.217677
235.659086	10428.333114	27.222695
235.966066	10449.111761	27.227712
236.380768	10456.400485	27.232730
236.214671	10466.192529	27.237748
236.560943	10491.395047	27.242765
236.506746	10496.670129	27.247783
236.656470	10518.976462	27.252800
237.038515	10532.534839	27.257818
236.954219	10555.863022	27.262836
237.379707	10578.381986	27.267853
237.685605	10596.407604	27.272871
238.067995	10615.700058	27.277888
238.130993	10628.118096	27.282906
238.337333	10658.710565	27.287924
238.839753	10671.565001	27.292941
239.268021	10684.680508	27.297959
239.418131	10713.279993	27.302976
239.740393	10730.248557	27.307994
239.828531	10746.300233	27.313012
240.142983	10759.209435	27.318029
240.686682	10764.394087	27.323047
240.429103	10789.628451	27.328064
240.687454	10797.715404	27.333082
240.857762	10810.738792	27.338100
241.069653	10829.808728	27.343117
241.490542	10844.213790	27.348135
241.466531	10865.704681	27.353152
241.857596	10884.563466	27.358170
242.209977	10907.198478	27.363188
242.364591	10922.728363	27.368205
242.756719	10937.968446	27.373223
242.776786	10958.590519	27.378240
243.310616	10973.688445	27.383258
243.557501	10989.311289	27.388276
243.812154	11006.729600	27.393293
244.145920	11016.964630	27.398311
244.320573	11038.206723	27.403328
244.734890	11047.800789	27.408346
245.000408	11061.889337	27.413364
245.272875	11059.516207	27.418381
245.221161	11076.935213	27.423399
245.351973	11092.153207	27.428416
245.999873	11102.269606	27.433434
246.207327	11118.672349	27.438452
246.203711	11130.608568	27.443469
246.716932	11140.515579	27.448487
246.874942	11155.252562	27.453504
246.757818	11160.575579	27.458522
247.514343	11173.390556	27.463540
246.909994	11188.477497	27.468557
247.355625	11197.498361	27.473575
247.719647	11222.973797	27.478592
247.673478	11237.644943	27.483610
248.125502	11252.926423	27.488628
248.110578	11275.284710	27.493645
248.416189	11295.205631	27.498663
248.640805	11324.144874	27.503680
249.146579	11340.614754	27.508698
249.284302	11357.420179	27.513716
249.645010	11373.271809	27.518733
250.023205	11392.445729	27.523751
250.261338	11420.884093	27.528768
250.897840	11440.137589	27.533786
250.993819	11440.946571	27.538804
250.950848	11467.622856	27.543821
251.589606	11468.034202	27.548839
251.388220	11501.094904	27.553856
251.615462	11508.956528	27.558874
252.082688	11530.011250	27.563892
252.311507	11546.060517	27.568909
252.676095	11553.306998	27.573927
253.053267	11583.526868	27.578944
253.122117	11601.366392	27.583962
253.711303	11612.145909	27.588980
253.751207	11618.773847	27.593997
254.169869	11643.897105	27.599015
254.130892	11661.298867	27.604032
254.289823	11670.784848	27.609050
254.628274	11690.303173	27.614068
254.547780	11712.858555	27.619085
255.104144	11724.249560	27.624103
255.305484	11750.546940	27.629120
255.669082	11764.064892	27.634138
255.971178	11783.980567	27.639156
255.881838	11795.772750	27.644173
256.705713	11811.747974	27.649191
256.597046	11837.374076	27.654208
256.763729	11849.546164	27.659226
257.246462	11868.925237	27.664244
257.648760	11884.856043	27.669261
258.133961	11903.369543	27.674279
258.196717	11915.643213	27.679296
258.339117	11935.306184	27.684314
258.536273	11945.588383	27.689332
258.450651	11958.927384	27.694349
258.678095	11977.528702	27.699367
259.236834	12009.227063	27.704384
259.573028	12028.783986	27.709402
259.898264	12041.161878	27.714420
259.973235	12063.882793	27.719437
260.514832	12081.945546	27.724455
260.821279	12100.237777	27.729472
261.041956	12109.057488	27.734490
261.313113	12124.326960	27.739508
261.382946	12145.558304	27.744525
261.641036	12163.425556	27.749543
261.932956	12164.772277	27.754560
262.106288	12184.411715	27.759578
262.526895	12199.907302	27.764596
262.465103	12214.793229	27.769613
263.280119	12229.289190	27.774631
262.974977	12240.041803	27.779648
263.202183	12248.219523	27.784666
263.467303	12262.732180	27.789684
263.595052	12300.362593	27.794701
264.180502	12311.834660	27.799719
264.648386	12327.142951	27.804736
264.590679	12352.689139	27.809754
265.154447	12356.178501	27.814772
265.083436	12380.302633	27.819789
265.366016	12396.274731	27.824807
265.632322	12406.066360	27.829824
265.734607	12431.723378	27.834842
266.165378	12446.377593	27.839860
266.241079	12472.566190	27.844877
266.506472	12482.263266	27.849895
266.645725	12512.938732	27.854912
267.146919	12536.957638	27.859930
267.766590	12557.253850	27.864948
267.877451	12570.682502	27.869965
268.334302	12590.956889	27.874983
268.433889	12605.751527	27.880000
269.034812	12634.665413	27.885018
268.961695	12628.976782	27.890036
269.468593	12652.726523	27.895053
269.542400	12670.724174	27.900071
269.727629	12677.711822	27.905088
269.819613	12701.507673	27.910106
270.291975	12720.513460	27.915124
270.550231	12742.783323	27.920141
270.627833	12763.249935	27.925159
271.274645	12791.338979	27.930176
271.279633	12810.888597	27.935194
271.801541	12817.469871	27.940212
271.889285	12852.101330	27.945229
272.006481	12871.481853	27.950247
272.908004	12892.359541	27.955264
272.889595	12904.567620	27.960282
273.275457	12919.845031	27.965300
273.151863	12939.146501	27.970317
273.549850	12955.852579	27.975335
274.024012	12981.761565	27.980352
274.143677	13004.552399	27.985370
274.847974	13019.334739	27.990388
274.826132	13031.562386	27.995405
274.923345	13052.610457	28.000423
275.178454	13074.552778	28.005440
275.676261	13094.265492	28.010458
275.978905	13110.585583	28.015476
276.277127	13128.046401	28.020493
276.495206	13141.029181	28.025511
276.779296	13159.152254	28.030528
276.953434	13177.636785	28.035546
277.101965	13200.259118	28.040564
277.323256	13217.520487	28.045581
277.734257	13238.386975	28.050599
277.899441	13262.797342	28.055616
277.966381	13282.981968	28.060634
278.404821	13301.614696	28.065652
278.824887	13321.260876	28.070669
278.862202	13341.210198	28.075687
279.385938	13364.077117	28.080704
279.260427	13391.271164	28.085722
280.023886	13408.242507	28.090740
280.566192	13426.716978	28.095757
280.736154	13444.359237	28.100775
280.999270	13459.293142	28.105792
280.920666	13480.189222	28.110810
280.866106	13480.816605	28.115828
281.492787	13512.648957	28.120845
281.537665	13536.731141	28.125863
281.931103	13553.368983	28.130880
281.867511	13566.282489	28.135898
282.529296	13592.109232	28.140916
282.756381	13621.547419	28.145933
282.722334	13635.501652	28.150951
283.315136	13656.996993	28.155968
283.404151	13686.962195	28.160986
283.607482	13706.990111	28.166004
283.935074	13735.282148	28.171021
284.601650	13752.183709	28.176039
285.260691	13773.675123	28.181056
285.102269	13802.700270	28.186074
285.468611	13816.197157	28.191092
285.855916	13828.212795	28.196109
286.172136	13863.422973	28.201127
286.520289	13877.778591	28.206144
286.865981	13903.907921	28.211162
287.176533	13909.796329	28.216180
287.216781	13929.660541	28.221197
287.471360	13956.979024	28.226215
287.754648	13969.465810	28.231232
288.120602	13998.086987	28.236250
288.639781	14009.365195	28.241268
288.710511	14035.032482	28.246285
288.793861	14056.001725	28.251303
289.547521	14074.674262	28.256320
289.569545	14098.460716	28.261338
289.979781	14111.284576	28.266356
290.303263	14140.758996	28.271373
290.212642	14160.643948	28.276391
290.748919	14175.829332	28.281408
290.905498	14203.994108	28.286426
291.812097	14219.399432	28.291444
291.555601	14246.185711	28.296461
291.773589	14267.093040	28.301479
292.529020	14279.250260	28.306496
292.639936	14306.724392	28.311514
293.196957	14324.947940	28.316532
293.415539	14333.971139	28.321549
293.228202	14365.815584	28.326567
293.805017	14382.760192	28.331584
294.102250	14404.612180	28.336602
294.109382	14421.589216	28.341620
294.580649	14450.614612	28.346637
294.793973	14466.090839	28.351655
295.242322	14479.322698	28.356672
295.324638	14515.208671	28.361690
295.722404	14535.020667	28.366708
296.264202	14557.813558	28.371725
296.263427	14582.046332	28.376743
296.888800	14600.335234	28.381760
297.065200	14620.542030	28.386778
297.458149	14641.649753	28.391796
297.629309	14656.071583	28.396813
297.652146	14673.741187	28.401831
298.270468	14687.950875	28.406848
298.358881	14716.139718	28.411866
298.454591	14736.368750	28.416884
299.362315	14755.589461	28.421901
298.763272	14777.497003	28.426919
299.611115	14805.412262	28.431936
299.668578	14826.591692	28.436954
300.159238	14851.316307	28.441972
300.668231	14871.692346	28.446989
300.700660	14886.442431	28.452007
301.204173	14900.660788	28.457024
301.133375	14923.051074	28.462042
301.441004	14952.598713	28.467060
301.762597	14967.271981	28.472077
301.767086	14978.410312	28.477095
302.542579	15004.028510	28.482112
302.752222	15034.374873	28.487130
302.939026	15048.551362	28.492148
303.675791	15078.016181	28.497165
303.645505	15099.636025	28.502183
304.004093	15111.593808	28.507200
304.199713	15135.319618	28.512218
304.421058	15154.250308	28.517236
304.717491	15172.815526	28.522253
304.980640	15205.301414	28.527271
305.673906	15230.825416	28.532288
305.508631	15261.540381	28.537306
306.048507	15266.193133	28.542324
306.266869	15298.799895	28.547341
306.439941	15323.325364	28.552359
307.175599	15354.177282	28.557376
307.430752	15376.766546	28.562394
307.339398	15399.388007	28.567412
308.145085	15430.156437	28.572429
308.507672	15446.118568	28.577447
308.785138	15467.103168	28.582464
309.140317	15487.611341	28.587482
309.199381	15510.518888	28.592500
309.903202	15538.934692	28.597517
310.264859	15562.328662	28.602535
310.469586	15582.194092	28.607552
310.762158	15603.577586	28.612570
310.593698	15616.256234	28.617588
311.111997	15630.062232	28.622605
311.402093	15659.184170	28.627623
311.980089	15673.880985	28.632640
312.136795	15703.968238	28.637658
312.241083	15729.743085	28.642676
312.689637	15752.709928	28.647693
312.956130	15785.809003	28.652711
313.369667	15806.261001	28.657728
313.482862	15836.481614	28.662746
313.909643	15858.911908	28.667764
314.389105	15881.495055	28.672781
314.405972	15912.394142	28.677799
315.012893	15932.825457	28.682816
314.966745	15959.413780	28.687834
315.394303	15982.864267	28.692852
315.854801	16004.645133	28.697869
315.930977	16035.711999	28.702887
316.675258	16056.668338	28.707904
316.891334	16087.024833	28.712922
317.281434	16111.991079	28.717940
317.678328	16128.077901	28.722957
317.984240	16157.905609	28.727975
318.224154	16167.558023	28.732992
318.616174	16184.836392	28.738010
318.592007	16212.407059	28.743028
319.442590	16228.606088	28.748045
319.460004	16258.839209	28.753063
319.961388	16275.705720	28.758080
320.188681	16297.548716	28.763098
320.184043	16316.882335	28.768116
320.545433	16342.349259	28.773133
320.556710	16374.371223	28.778151
321.124259	16394.180658	28.783168
321.189456	16417.031471	28.788186
321.312406	16445.517499	28.793204
321.915233	16468.189402	28.798221
322.459004	16496.180029	28.803239
322.509259	16517.239270	28.808256
323.157000	16543.195393	28.813274
323.180671	16565.626487	28.818292
323.804769	16588.361528	28.823309
324.075550	16615.485438	28.828327
324.317215	16634.493367	28.833344
324.778338	16656.139057	28.838362
324.921946	16695.752889	28.843380
325.488166	16710.970345	28.848397
325.579129	16737.727776	28.853415
325.897668	16753.672627	28.858432
326.087874	16776.289502	28.863450
326.618197	16804.661711	28.868468
327.191158	16832.092349	28.873485
327.272655	16873.289239	28.878503
327.693161	16888.428587	28.883520
328.269715	16906.967395	28.888538
328.402803	16941.943437	28.893556
328.647432	16962.953765	28.898573
328.837603	16985.217130	28.903591
329.097236	17013.679427	28.908608
329.468153	17040.033345	28.913626
329.599066	17071.655534	28.918644
330.214181	17097.630150	28.923661
330.022728	17131.861404	28.928679
330.885992	17156.407439	28.933696
331.439178	17179.536479	28.938714
331.567676	17206.787741	28.943732
332.199308	17226.069982	28.948749
332.401568	17255.842977	28.953767
332.798211	17278.061702	28.958784
333.362582	17309.654286	28.963802
333.258321	17324.035979	28.968820
333.727325	17352.440710	28.973837
333.867483	17386.342508	28.978855
334.220404	17414.247494	28.983872
334.510136	17434.752202	28.988890
335.021455	17465.437340	28.993908
335.408805	17485.705705	28.998925
335.676704	17515.847858	29.003943
335.746490	17542.161187	29.008960
336.264488	17575.119701	29.013978
336.467630	17599.712848	29.018996
336.972219	17625.673900	29.024013
337.247142	17660.395279	29.029031
337.321036	17679.777974	29.034048
337.814783	17710.302000	29.039066
338.209113	17750.444126	29.044084
338.813298	17772.864654	29.049101
339.093379	17806.479937	29.054119
339.580890	17832.791402	29.059136
339.863326	17846.929703	29.064154
340.076261	17885.337952	29.069172
340.463737	17895.530372	29.074189
340.948623	17929.025342	29.079207
341.197158	17959.809284	29.084224
341.793705	17979.546315	29.089242
341.920110	18007.146493	29.094260
342.334432	18029.154833	29.099277
342.593642	18057.858797	29.104295
342.973551	18085.122452	29.109312
342.993419	18104.678290	29.114330
343.550962	18126.872785	29.119348
344.106039	18144.797029	29.124365
344.368702	18168.313908	29.129383
344.662037	18188.281857	29.134400
345.274688	18213.721366	29.139418
345.419723	18237.244118	29.144436
345.576711	18250.991722	29.149453
345.898811	18278.934368	29.154471
346.259593	18300.155386	29.159488
346.381584	18322.462555	29.164506
346.628966	18351.288840	29.169524
347.343107	18368.341814	29.174541
347.738912	18402.792881	29.179559
347.513428	18427.561617	29.184576
347.917316	18446.918656	29.189594
347.939414	18485.989751	29.194612
348.840452	18512.433210	29.199629
348.937624	18543.924095	29.204647
349.702609	18580.895262	29.209664
349.912482	18603.403788	29.214682
350.265914	18642.979254	29.219700
350.567673	18665.170208	29.224717
350.522337	18689.481453	29.229735
350.872174	18720.623477	29.234752
351.483046	18757.796017	29.239770
351.866363	18790.910365	29.244788
352.006058	18825.983532	29.249805
352.665768	18853.040174	29.254823
353.084007	18881.821527	29.259840
353.349708	18903.140228	29.264858
353.593576	18945.007876	29.269876
354.143681	18964.374117	29.274893
354.406960	18998.676416	29.279911
354.597033	19027.828570	29.284928
355.124009	19057.281794	29.289946
355.242895	19098.013181	29.294964
356.010351	19126.455891	29.299981
356.190213	19153.771333	29.304999
356.847662	19179.603116	29.310016
357.534107	19212.095769	29.315034
357.305103	19241.743504	29.320052
358.106483	19260.584201	29.325069
358.184098	19292.452113	29.330087
358.683045	19319.540904	29.335104
358.986351	19340.380348	29.340122
359.201690	19379.808355	29.345140
359.464574	19412.986848	29.350157
359.918221	19433.708073	29.355175
360.439021	19460.130249	29.360192
360.595453	19496.636178	29.365210
360.859250	19540.410012	29.370228
361.457157	19562.479783	29.375245
362.115044	19592.823103	29.380263
362.295673	19624.182614	29.385280
362.497912	19648.715310	29.390298
362.620396	19676.267919	29.395316
363.172171	19703.696460	29.400333
364.085851	19738.826934	29.405351
364.384008	19767.413588	29.410368
364.267650	19784.547351	29.415386
365.038212	19821.627406	29.420404
365.240642	19844.928290	29.425421
365.648910	19860.311964	29.430439
365.742168	19897.510891	29.435456
365.873082	19927.261237	29.440474
366.085353	19964.921827	29.445492
366.210913	19990.180911	29.450509
366.935238	20028.336367	29.455527
367.265808	20063.179672	29.460544
367.856245	20081.605616	29.465562
367.903899	20113.460602	29.470580
368.740148	20148.932487	29.475597
368.863046	20183.587398	29.480615
369.438098	20204.960154	29.485632
369.679684	20219.965854	29.490650
369.583848	20258.351318	29.495668
370.057939	20289.185739	29.500685
371.043062	20325.582361	29.505703
371.178926	20351.863854	29.510720
371.295361	20371.830155	29.515738
371.645521	20415.895692	29.520756
372.213377	20452.320000	29.525773
371.994390	20481.810078	29.530791
372.857684	20512.684979	29.535808
373.137821	20542.014828	29.540826
373.667025	20565.834032	29.545844
373.798592	20605.852593	29.550861
374.443732	20633.305722	29.555879
375.079833	20685.477750	29.560896
375.113837	20713.810196	29.565914
375.586599	20740.696548	29.570932
375.785839	20770.614383	29.575949
376.355839	20813.483790	29.580967
376.432694	20843.035481	29.585984
376.954017	20874.931236	29.591002
377.372708	20908.485914	29.596020
377.632744	20937.996418	29.601037
378.183140	20976.193597	29.606055
378.424175	21013.093474	29.611072
379.114178	21046.340513	29.616090
379.381971	21079.824341	29.621108
380.194731	21115.276379	29.626125
380.580039	21137.040026	29.631143
380.713387	21176.718268	29.636160
381.380088	21204.345736	29.641178
381.645790	21227.031768	29.646196
382.089106	21257.607150	29.651213
382.640052	21285.524561	29.656231
382.803162	21309.572611	29.661248
383.166618	21335.655484	29.666266
383.827717	21376.647867	29.671284
383.383081	21412.076243	29.676301
383.959623	21432.274842	29.681319
384.324279	21472.233376	29.686336
384.956481	21508.080883	29.691354
385.247459	21542.743450	29.696372
385.758815	21578.350949	29.701389
386.030088	21607.892288	29.706407
385.859031	21636.340320	29.711424
386.406260	21671.929732	29.716442
387.027911	21714.761415	29.721460
387.062556	21747.600475	29.726477
387.574288	21785.034395	29.731495
388.142971	21819.262187	29.736512
388.087694	21862.800501	29.741530
388.986067	21897.962512	29.746548
389.459434	21928.635326	29.751565
389.970777	21967.718851	29.756583
389.974986	22002.976875	29.761600
390.551731	22028.806097	29.766618
390.919433	22064.841377	29.771636
391.596333	22114.325298	29.776653
391.598139	22131.695340	29.781671
392.265612	22173.276029	29.786688
392.643623	22207.970359	29.791706
392.969689	22244.852896	29.796724
393.168954	22277.332148	29.801741
393.537957	22305.209992	29.806759
394.008943	22335.315109	29.811776
394.148290	22367.942911	29.816794
394.840614	22398.379950	29.821812
394.840001	22429.367901	29.826829
395.465398	22458.343206	29.831847
395.782052	22505.066285	29.836864
396.530530	22535.406275	29.841882
397.139442	22566.103077	29.846900
396.996074	22602.105644	29.851917
397.932609	22639.183965	29.856935
397.895602	22666.304443	29.861952
398.683826	22695.538946	29.866970
399.040812	22735.267425	29.871988
399.264306	22768.122826	29.877005
399.902000	22787.093658	29.882023
399.784290	22824.021505	29.887040
400.380312	22855.466423	29.892058
400.658957	22898.360710	29.897076
400.855498	22926.241163	29.902093
401.717778	22959.628732	29.907111
401.816328	23002.987471	29.912128
402.214829	23037.427277	29.917146
402.565436	23077.296458	29.922164
402.928407	23115.350188	29.927181
403.579031	23157.093556	29.932199
403.928922	23198.827244	29.937216
403.989287	23227.127556	29.942234
404.697816	23276.192352	29.947252
404.919036	23312.966908	29.952269
405.623151	23356.092540	29.957287
405.866029	23393.021832	29.962304
406.287119	23424.912119	29.967322
406.743440	23459.147701	29.972340
407.101685	23504.741784	29.977357
407.751688	23538.763906	29.982375
408.303040	23575.449320	29.987392
408.553965	23617.919785	29.992410
409.023643	23650.504265	29.997428
409.534050	23688.359054	30.002445
409.854790	23724.392058	30.007463
409.683814	23783.902703	30.012480
410.341456	23814.656993	30.017498
410.889168	23847.716163	30.022516
411.086976	23883.793987	30.027533
411.689081	23926.058434	30.032551
411.994552	23958.378444	30.037568
412.294956	24004.899042	30.042586
412.872538	24045.682519	30.047604
413.262194	24095.292191	30.052621
413.786495	24129.151744	30.057639
413.933520	24165.301224	30.062656
414.293542	24203.945201	30.067674
415.222538	24244.288550	30.072692
415.390231	24288.997940	30.077709
416.476518	24335.124470	30.082727
416.497494	24364.051873	30.087744
417.080321	24397.157008	30.092762
417.489572	24431.793440	30.097780
417.737720	24468.066657	30.102797
418.588102	24500.782478	30.107815
418.513946	24532.170702	30.112832
418.963572	24571.079414	30.117850
419.630871	24607.641128	30.122868
420.142142	24635.474667	30.127885
420.571983	24663.851850	30.132903
421.092841	24713.846958	30.137920
420.853932	24749.880990	30.142938
421.096755	24779.039667	30.147956
421.480247	24812.960350	30.152973
422.445135	24848.407865	30.157991
422.939372	24889.123957	30.163008
423.335537	24924.262546	30.168026
423.761890	24949.562978	30.173044
424.217325	24979.876752	30.178061
424.062548	25002.683505	30.183079
424.758417	25045.959426	30.188096
424.871417	25080.150438	30.193114
425.443097	25110.977063	30.198132
425.796166	25158.218858	30.203149
426.137742	25193.758295	30.208167
426.401669	25239.187821	30.213184
426.817506	25285.320435	30.218202
427.375060	25321.281295	30.223220
427.771952	25365.691745	30.228237
428.220700	25409.613861	30.233255
428.781290	25448.077139	30.238272
429.163546	25490.499395	30.243290
429.655728	25536.007596	30.248308
430.104315	25582.830951	30.253325
430.163999	25616.797387	30.258343
430.791494	25652.526686	30.263360
431.022028	25705.862422	30.268378
431.596052	25743.173926	30.273396
431.899960	25795.392411	30.278413
432.551693	25839.624948	30.283431
432.733783	25888.342514	30.288448
433.332274	25928.342855	30.293466
433.953533	25974.425909	30.298484
434.397521	26027.469938	30.303501
434.864470	26061.152128	30.308519
435.435391	26098.483736	30.313536
435.773550	26149.888801	30.318554
436.441328	26177.263872	30.323572
436.710271	26232.611095	30.328589
437.135891	26275.717101	30.333607
437.952633	26313.358210	30.338624
437.831247	26362.737504	30.343642
438.603690	26401.390622	30.348660
438.758206	26446.587191	30.353677
439.298656	26491.344200	30.358695
439.984358	26529.157921	30.363712
440.215710	26576.813950	30.368730
441.098856	26618.742983	30.373748
441.347445	26655.272872	30.378765
441.419589	26703.093180	30.383783
442.251244	26743.286142	30.388800
442.738966	26783.008469	30.393818
443.202148	26822.981210	30.398836
443.322875	26861.876332	30.403853
443.761711	26907.282207	30.408871
444.343175	26938.577795	30.413888
444.850737	26987.461914	30.418906
445.416932	27027.241952	30.423924
445.940455	27070.340633	30.428941
446.057580	27113.016388	30.433959
447.065687	27149.238590	30.438976
447.296781	27191.220375	30.443994
447.749888	27220.311714	30.449012
447.962464	27256.279485	30.454029
448.529478	27305.578527	30.459047
449.033002	27336.861655	30.464064
449.492709	27386.816068	30.469082
449.762998	27418.951196	30.474100
450.090447	27455.419606	30.479117
450.823598	27501.223144	30.484135
450.812276	27535.861246	30.489152
451.002133	27578.937420	30.494170
451.724724	27610.957763	30.499188
452.096861	27655.724738	30.504205
452.699385	27698.926146	30.509223
452.945123	27733.909876	30.514240
453.144614	27785.138538	30.519258
453.698430	27814.815410	30.524276
453.844209	27857.595686	30.529293
454.108650	27915.147769	30.534311
454.914703	27964.252947	30.539328
455.250034	28021.174801	30.544346
455.954697	28057.812751	30.549364
456.272575	28109.592544	30.554381
457.022895	28167.372629	30.559399
457.648610	28205.135656	30.564416
458.099806	28256.522016	30.569434
458.456204	28298.739283	30.574452
458.889768	28338.270862	30.579469
459.040097	28386.740230	30.584487
459.756951	28426.657422	30.589504
459.912472	28482.521544	30.594522
460.913588	28529.024955	30.599540
461.238910	28578.143696	30.604557
461.256190	28631.615312	30.609575
462.543248	28671.077062	30.614592
462.524436	28727.120857	30.619610
463.229632	28766.604396	30.624628
463.612093	28811.979092	30.629645
464.306310	28856.078797	30.634663
464.673382	28895.394312	30.639680
464.756801	28949.178764	30.644698
465.789954	28988.636649	30.649716
465.949888	29038.256469	30.654733
466.391614	29092.775300	30.659751
466.774016	29135.495896	30.664768
467.248447	29176.444920	30.669786
467.918681	29232.767753	30.674804
468.669671	29287.162808	30.679821
468.823149	29326.354575	30.684839
469.259505	29380.274507	30.689856
469.479315	29434.601443	30.694874
469.951025	29477.150733	30.699892
470.873876	29528.851994	30.704909
470.986806	29582.955858	30.709927
471.557924	29617.550495	30.714944
472.102391	29672.250726	30.719962
472.833680	29717.459002	30.724980
473.305125	29767.625981	30.729997
473.679492	29814.451715	30.735015
474.293175	29844.476140	30.740032
474.513927	29898.646119	30.745050
474.865348	29949.812135	30.750068
475.412800	30000.062593	30.755085
475.805767	30042.258749	30.760103
476.400154	30086.041700	30.765120
477.026245	30143.322133	30.770138
477.224021	30182.401125	30.775156
477.843896	30233.696473	30.780173
477.949360	30280.464238	30.785191
478.699367	30331.341200	30.790208
479.202789	30385.917001	30.795226
479.877944	30443.841687	30.800244
480.131473	30485.384195	30.805261
480.737848	30531.353428	30.810279
481.612145	30567.596321	30.815296
481.750638	30615.358460	30.820314
482.208295	30661.231166	30.825332
483.087339	30705.558743	30.830349
483.053500	30735.319236	30.835367
483.750008	30772.203522	30.840384
484.025399	30825.513964	30.845402
484.563336	30865.501841	30.850420
484.780120	30911.141000	30.855437
485.384997	30961.852597	30.860455
486.003086	31003.282149	30.865472
486.575859	31046.659615	30.870490
486.921026	31094.959431	30.875508
487.633485	31136.387112	30.880525
487.557692	31189.216153	30.885543
488.424058	31234.103152	30.890560
488.984391	31276.667552	30.895578
489.153666	31324.578221	30.900596
489.789846	31375.052021	30.905613
489.870947	31427.073201	30.910631
490.155345	31464.105447	30.915648
490.800650	31531.039992	30.920666
491.327347	31592.050865	30.925684
491.950915	31644.841064	30.930701
492.657134	31699.647750	30.935719
493.150082	31736.047244	30.940736
493.833361	31804.822692	30.945754
494.032736	31840.313752	30.950772
494.632402	31895.725575	30.955789
494.788438	31957.699599	30.960807
495.551851	32000.328501	30.965824
495.968997	32063.880349	30.970842
496.274031	32116.430824	30.975860
496.875128	32173.493184	30.980877
497.699949	32228.933847	30.985895
497.959001	32283.262093	30.990912
498.689891	32339.760889	30.995930
499.227743	32386.434054	31.000948
499.923919	32433.746339	31.005965
500.114280	32498.422417	31.010983
500.961540	32538.150111	31.016000
501.508235	32585.574661	31.021018
501.756702	32638.375546	31.026036
502.467510	32695.864695	31.031053
502.784616	32742.503686	31.036071
503.221764	32792.866681	31.041088
503.728126	32857.557596	31.046106
504.288651	32911.404026	31.051124
504.962404	32955.825450	31.056141
505.304201	33005.154408	31.061159
505.609264	33058.965362	31.066176
505.948117	33118.682446	31.071194
506.339954	33170.558137	31.076212
507.450468	33229.946045	31.081229
508.095319	33282.275520	31.086247
508.758003	33329.367473	31.091264
508.989050	33390.676467	31.096282
509.352027	33426.157235	31.101300
509.966104	33487.128337	31.106317
510.558958	33544.916470	31.111335
511.119200	33591.873319	31.116352
511.716062	33638.653833	31.121370
512.008958	33688.542101	31.126388
512.854792	33742.586228	31.131405
513.071512	33791.854430	31.136423
513.497486	33838.263839	31.141440
514.112341	33898.135904	31.146458
514.808283	33947.746696	31.151476
515.186521	33994.720305	31.156493
515.846117	34047.397112	31.161511
516.253669	34092.526497	31.166528
516.659503	34141.949250	31.171546
516.971158	34184.760835	31.176564
517.967094	34231.537065	31.181581
518.393915	34279.490019	31.186599
518.688033	34320.527981	31.191616
519.289843	34371.602387	31.196634
519.509286	34427.010897	31.201652
520.094249	34465.506152	31.206669
520.465888	34523.344260	31.211687
521.284991	34576.509540	31.216704
522.089622	34621.343925	31.221722
522.052621	34676.489764	31.226740
522.737121	34732.332051	31.231757
522.903344	34771.203260	31.236775
523.693079	34822.489586	31.241792
524.176334	34882.087883	31.246810
524.483889	34947.910188	31.251828
525.354197	34997.477169	31.256845
525.393499	35054.932506	31.261863
526.052820	35106.948101	31.266880
526.699241	35162.057715	31.271898
527.061853	35218.052863	31.276916
527.571624	35276.276053	31.281933
528.445453	35335.972526	31.286951
529.023923	35398.225621	31.291968
529.465657	35454.974073	31.296986
529.821580	35511.287188	31.302004
530.626726	35564.166277	31.307021
531.091690	35625.887719	31.312039
531.800248	35682.323100	31.317056
533.008469	35732.597635	31.322074
533.080328	35773.584697	31.327092
533.705231	35826.138579	31.332109
533.904915	35884.677569	31.337127
534.385943	35936.786352	31.342144
535.104485	35994.921905	31.347162
535.518749	36044.714511	31.352180
536.006972	36103.442865	31.357197
536.798984	36166.575293	31.362215
537.295594	36220.749997	31.367232
537.964887	36273.051425	31.372250
538.420320	36331.374537	31.377268
539.015372	36377.029531	31.382285
539.130473	36429.677392	31.387303
539.904779	36484.536442	31.392320
540.688197	36547.747222	31.397338
540.963518	36605.454319	31.402356
541.477214	36648.194960	31.407373
541.970074	36710.326184	31.412391
542.549038	36765.463158	31.417408
543.307837	36826.079734	31.422426
543.710682	36887.605883	31.427444
544.419595	36931.859415	31.432461
544.968924	36989.069348	31.437479
545.456837	37042.254724	31.442496
546.341183	37099.089987	31.447514
546.488458	37159.189910	31.452532
547.263973	37207.834692	31.457549
547.819383	37275.187249	31.462567
548.093554	37323.645227	31.467584
548.657260	37366.695644	31.472602
549.025421	37432.041855	31.477620
549.813289	37484.504732	31.482637
550.313279	37537.777974	31.487655
550.752018	37591.623737	31.492672
551.595711	37650.528310	31.497690
551.955145	37700.124674	31.502708
552.561098	37762.424616	31.507725
552.987232	37818.347066	31.512743
553.792827	37860.247629	31.517760
554.359668	37908.850798	31.522778
554.146012	37964.355289	31.527796
555.182787	38006.365375	31.532813
555.894257	38065.095758	31.537831
556.120160	38114.966939	31.542848
556.837864	38162.522611	31.547866
557.248763	38224.076618	31.552884
558.065597	38273.754436	31.557901
558.452940	38335.280831	31.562919
558.786053	38389.328521	31.567936
559.618101	38444.594585	31.572954
559.845645	38505.767064	31.577972
560.825846	38555.122724	31.582989
561.482006	38622.722994	31.588007
561.597735	38676.508225	31.593024
562.509339	38721.631688	31.598042
563.017820	38778.783212	31.603060
563.359556	38840.248624	31.608077
563.793377	38896.710196	31.613095
564.486615	38953.181879	31.618112
565.119487	39004.591335	31.623130
565.983232	39078.389632	31.628148
566.462903	39131.031266	31.633165
567.172194	39193.780805	31.638183
567.828768	39246.666947	31.643200
568.096081	39306.121641	31.648218
568.906446	39370.335692	31.653236
569.567822	39420.704522	31.658253
570.203859	39474.821311	31.663271
570.317161	39537.330007	31.668288
571.110417	39595.918931	31.673306
571.350771	39661.721939	31.678324
571.956801	39719.284382	31.683341
572.282643	39778.712229	31.688359
573.187664	39841.825087	31.693376
573.684767	39898.646159	31.698394
574.419413	39960.894329	31.703412
575.076286	40024.811816	31.708429
575.497069	40086.616208	31.713447
575.768903	40155.483057	31.718464
576.614611	40214.021161	31.723482
577.156931	40278.589765	31.728500
577.566968	40341.534944	31.733517
578.276852	40407.045314	31.738535
578.770879	40474.120190	31.743552
579.643829	40534.356151	31.748570
580.106620	40600.683703	31.753588
580.730152	40663.166310	31.758605
581.607662	40722.232051	31.763623
581.705312	40801.702736	31.768640
582.720575	40855.972271	31.773658
583.303335	40911.283654	31.778676
583.990428	40977.197747	31.783693
584.344311	41034.170693	31.788711
585.001303	41094.707652	31.793728
585.734366	41149.926528	31.798746
586.460140	41213.514147	31.803764
586.456637	41266.173361	31.808781
587.488502	41336.588272	31.813799
587.870097	41397.738416	31.818816
588.718266	41461.111520	31.823834
589.179648	41526.234079	31.828852
589.768106	41574.051469	31.833869
590.509793	41633.710164	31.838887
590.936093	41696.985576	31.843904
591.476516	41752.362633	31.848922
592.181320	41812.280580	31.853940
592.829083	41861.752727	31.858957
593.509795	41905.135354	31.863975
593.691007	41958.323878	31.868992
594.064658	42015.454393	31.874010
594.725525	42079.029384	31.879028
595.493510	42138.862427	31.884045
595.822209	42191.807045	31.889063
596.100981	42256.511295	31.894080
596.788823	42318.881018	31.899098
597.240212	42386.670482	31.904116
597.684127	42452.260235	31.909133
598.658501	42516.464159	31.914151
598.962544	42594.941270	31.919168
599.762805	42654.561931	31.924186
600.290647	42730.651564	31.929204
600.666220	42806.474352	31.934221
601.453495	42869.791469	31.939239
601.956917	42937.498571	31.944256
602.736756	43005.194215	31.949274
603.328774	43083.280074	31.954292
603.801282	43148.304473	31.959309
604.390921	43219.578979	31.964327
605.725214	43291.331663	31.969344
606.199234	43363.421715	31.974362
606.825162	43433.729792	31.979380
607.238838	43491.895192	31.984397
608.056874	43559.554920	31.989415
608.351711	43620.680526	31.994432
609.360093	43687.722582	31.999450
609.578884	43769.968115	32.004468
610.197291	43836.477111	32.009485
611.424067	43904.269963	32.014503
611.748318	43972.387803	32.019520
612.867187	44036.073793	32.024538
612.894537	44102.062583	32.029556
613.595459	44168.414162	32.034573
614.070398	44238.065277	32.039591
614.659399	44308.755104	32.044608
615.292956	44367.938389	32.049626
616.160884	44449.717887	32.054644
616.729731	44519.785310	32.059661
617.795118	44585.669890	32.064679
618.474964	44645.333730	32.069696
618.938106	44707.093817	32.074714
619.501300	44764.688793	32.079732
619.800660	44831.813703	32.084749
620.714520	44895.945423	32.089767
620.825342	44968.211405	32.094784
621.604417	45038.456276	32.099802
622.419608	45103.363127	32.104820
623.143615	45166.494262	32.109837
623.779091	45242.265656	32.114855
624.495721	45313.944466	32.119872
625.256415	45374.249143	32.124890
625.578147	45435.881564	32.129908
625.843022	45514.115724	32.134925
626.857421	45576.822986	32.139943
627.303590	45649.848351	32.144960
628.016368	45717.898002	32.149978
628.774641	45772.782837	32.154996
628.815596	45844.588134	32.160013
629.846341	45910.437754	32.165031
630.514009	45986.617802	32.170048
630.732475	46055.637849	32.175066
631.471321	46132.250060	32.180084
632.258410	46201.782474	32.185101
632.926943	46261.243622	32.190119
633.622172	46336.136347	32.195136
634.052044	46396.982681	32.200154
634.980834	46455.840562	32.205172
635.457601	46519.166039	32.210189
635.975971	46588.476031	32.215207
636.362690	46660.172836	32.220224
637.164238	46725.915231	32.225242
637.641201	46788.431681	32.230260
638.238596	46862.215408	32.235277
639.135874	46924.109701	32.240295
639.780302	46994.312171	32.245312
640.108341	47061.825133	32.250330
640.694959	47134.238632	32.255348
641.403858	47212.940546	32.260365
642.115284	47274.801640	32.265383
642.431439	47358.158479	32.270400
643.152632	47429.223310	32.275418
643.750133	47503.047063	32.280436
644.366347	47588.116491	32.285453
645.147238	47657.508839	32.290471
645.800914	47739.061793	32.295488
646.497736	47819.874411	32.300506
647.392872	47883.992253	32.305524
647.846511	47973.915703	32.310541
648.388105	48052.381009	32.315559
649.205574	48134.846058	32.320576
649.524534	48197.182350	32.325594
650.535440	48277.858831	32.330612
651.161045	48353.629535	32.335629
651.566848	48428.182235	32.340647
652.258910	48511.484421	32.345664
652.875403	48594.343224	32.350682
653.712131	48676.066988	32.355700
654.736182	48766.094026	32.360717
655.318350	48834.211440	32.365735
655.786546	48918.435913	32.370752
656.605158	48999.752429	32.375770
657.056606	49068.378174	32.380788
657.780049	49155.859822	32.385805
658.515795	49237.183830	32.390823
659.144772	49321.277046	32.395840
659.691449	49402.511037	32.400858
660.695995	49463.433736	32.405876
661.428376	49547.220547	32.410893
661.883463	49619.529658	32.415911
662.629179	49707.319940	32.420928
663.277297	49781.035559	32.425946
664.257659	49858.843596	32.430964
664.739744	49942.569810	32.435981
665.387212	50030.895531	32.440999
666.382968	50104.956351	32.446016
666.647107	50177.505911	32.451034
667.473110	50251.859526	32.456052
668.053301	50332.806826	32.461069
668.992792	50399.348068	32.466087
669.729177	50480.986400	32.471104
670.123672	50552.510695	32.476122
670.821356	50630.719929	32.481140
670.860439	50711.234458	32.486157
671.826203	50776.292088	32.491175
672.446717	50863.897573	32.496192
672.945473	50947.137610	32.501210
673.884448	51029.771180	32.506228
674.337767	51109.969128	32.511245
675.221280	51185.386064	32.516263
676.138419	51269.042618	32.521280
676.859388	51354.767634	32.526298
677.718007	51420.811952	32.531316
677.856634	51507.463954	32.536333
678.774376	51559.705476	32.541351
679.129663	51644.925680	32.546368
680.138935	51714.193262	32.551386
680.986559	51782.746040	32.556404
681.265120	51860.379640	32.561421
681.552667	51937.626105	32.566439
682.753984	52017.627783	32.571456
683.253474	52085.305808	32.576474
684.211300	52152.861631	32.581492
684.545388	52243.832866	32.586509
685.074461	52314.329073	32.591527
685.920281	52400.044709	32.596544
686.620031	52483.897863	32.601562
687.625669	52563.735896	32.606580
687.798990	52644.710665	32.611597
688.330994	52720.731808	32.616615
689.455298	52811.594155	32.621632
689.400182	52894.592504	32.626650
690.624773	52977.473003	32.631668
691.230918	53070.790459	32.636685
691.974425	53149.950157	32.641703
692.539525	53235.080016	32.646720
693.270077	53320.861366	32.651738
694.346775	53411.347484	32.656756
694.816670	53502.251706	32.661773
695.472197	53588.836787	32.666791
696.053983	53675.788106	32.671808
696.665090	53773.372696	32.676826
697.419977	53850.837038	32.681844
698.377643	53936.021860	32.686861
698.975357	54026.952385	32.691879
699.739960	54109.883598	32.696896
700.055763	54208.535071	32.701914
701.043798	54297.779161	32.706932
701.864338	54388.739465	32.711949
702.667342	54475.532520	32.716967
703.602377	54561.640744	32.721984
704.200077	54657.997064	32.727002
705.047207	54744.493091	32.732020
705.354999	54838.383182	32.737037
706.117571	54918.995029	32.742055
707.206436	55008.466487	32.747072
707.464032	55111.605035	32.752090
708.215685	55197.345591	32.757108
708.942000	55284.438396	32.762125
709.730554	55368.882777	32.767143
710.269595	55458.631887	32.772160
710.790123	55555.383643	32.777178
711.964766	55652.875061	32.782196
712.646001	55734.071982	32.787213
713.552006	55829.656976	32.792231
714.007014	55916.338914	32.797248
714.756101	56013.487085	32.802266
715.709814	56103.331900	32.807284
716.437391	56187.105224	32.812301
717.240258	56276.879383	32.817319
718.052626	56357.095912	32.822336
718.843010	56453.188822	32.827354
719.251579	56535.399473	32.832372
720.297660	56632.952997	32.837389
720.861718	56711.127401	32.842407
721.480684	56790.382033	32.847424
722.200965	56884.076334	32.852442
722.910990	56967.829820	32.857460
723.467248	57052.398799	32.862477
724.495771	57140.716834	32.867495
724.986927	57236.454681	32.872512
725.351958	57316.326753	32.877530
726.058088	57391.595077	32.882548
727.317533	57480.985786	32.887565
728.036329	57568.474150	32.892583
728.503844	57638.369222	32.897600
729.304523	57732.199804	32.902618
730.117598	57801.889336	32.907636
730.842854	57888.491765	32.912653
731.357270	57982.577010	32.917671
732.235907	58073.029564	32.922688
732.812665	58158.700499	32.927706
733.450722	58245.330518	32.932724
734.221904	58333.205863	32.937741
734.728019	58415.597528	32.942759
735.541666	58495.561477	32.947776
736.221226	58597.022261	32.952794
737.105714	58692.337174	32.957812
737.706356	58782.183978	32.962829
738.064636	58873.683077	32.967847
739.205601	58966.598017	32.972864
739.768744	59076.756746	32.977882
740.412835	59169.389488	32.982900
740.933928	59275.492143	32.987917
741.988171	59374.353014	32.992935
743.107636	59478.141167	32.997952
743.797622	59579.401865	33.002970
744.533651	59664.736683	33.007988
745.581081	59765.467454	33.013005
746.021643	59852.039175	33.018023
746.904564	59946.295847	33.023040
747.329306	60048.638100	33.028058
748.264482	60133.645869	33.033076
748.991835	60229.504107	33.038093
749.975785	60335.184411	33.043111
750.914642	60425.085573	33.048128
751.381208	60538.620833	33.053146
752.006795	60624.799174	33.058164
753.195368	60724.790178	33.063181
753.769128	60820.029120	33.068199
754.804961	60909.309193	33.073216
755.122624	61008.317324	33.078234
756.001533	61105.541516	33.083252
756.533158	61198.826212	33.088269
757.409755	61303.261476	33.093287
758.110056	61400.097013	33.098304
758.992609	61508.083399	33.103322
759.926112	61596.343843	33.108340
761.092516	61695.297782	33.113357
761.552850	61791.533082	33.118375
762.125653	61881.876693	33.123392
763.063715	61986.153291	33.128410
763.853247	62077.919637	33.133428
764.529629	62169.438169	33.138445
765.299162	62266.032031	33.143463
766.611788	62362.028466	33.148480
766.659784	62464.275142	33.153498
767.286705	62563.772814	33.158516
768.372255	62661.261956	33.163533
768.767839	62754.877672	33.168551
770.090294	62850.146451	33.173568
770.509019	62956.274646	33.178586
771.239805	63056.182164	33.183604
772.593689	63151.706727	33.188621
773.108870	63244.298994	33.193639
773.664146	63344.671959	33.198656
774.311181	63439.605615	33.203674
775.161213	63533.197399	33.208692
776.190823	63631.952562	33.213709
776.844706	63723.936132	33.218727
778.016495	63809.122050	33.223744
778.454334	63905.812186	33.228762
779.523158	63990.115878	33.233780
779.781601	64074.850630	33.238797
780.832926	64164.557806	33.243815
781.584832	64261.788896	33.248832
782.053900	64348.821334	33.253850
782.954764	64443.383506	33.258868
783.931683	64534.749682	33.263885
784.620597	64628.396104	33.268903
785.495851	64717.987215	33.273920
786.189703	64812.925061	33.278938
786.726901	64905.766914	33.283956
787.738905	65005.536859	33.288973
788.025491	65108.250768	33.293991
788.960666	65207.204174	33.299008
789.497183	65306.574935	33.304026
790.684254	65408.566595	33.309044
791.459419	65513.434193	33.314061
792.187188	65623.412570	33.319079
792.758315	65721.817201	33.324096
793.556466	65838.236975	33.329114
794.649143	65939.815030	33.334132
795.339793	66038.227496	33.339149
795.920870	66142.501289	33.344167
796.708695	66252.567954	33.349184
797.325551	66360.395242	33.354202
798.306774	66478.074541	33.359220
799.435374	66587.259879	33.364237
800.266754	66697.365963	33.369255
801.255576	66785.287756	33.374272
801.941908	66885.521297	33.379290
802.868056	66991.517341	33.384308
803.693098	67100.169907	33.389325
804.374529	67209.795156	33.394343
805.196739	67313.396482	33.399360
806.180075	67428.224278	33.404378
806.465170	67524.546894	33.409396
807.348316	67626.037836	33.414413
808.058804	67746.247374	33.419431
809.316448	67853.689354	33.424448
810.258050	67967.481361	33.429466
811.486739	68068.058823	33.434484
812.104452	68171.701963	33.439501
812.883818	68279.518208	33.444519
813.412900	68376.312350	33.449536
814.426665	68485.739034	33.454554
815.099293	68590.736611	33.459572
816.087689	68692.120294	33.464589
816.632358	68804.971373	33.469607
817.678631	68902.212051	33.474624
818.583165	69014.260518	33.479642
819.206272	69115.323138	33.484660
820.269779	69220.186076	33.489677
820.695800	69339.447106	33.494695
821.799430	69441.341239	33.499712
822.399911	69546.474294	33.504730
823.235201	69650.697168	33.509748
824.110836	69761.366640	33.514765
825.111430	69875.797348	33.519783
825.836127	69973.744611	33.524800
826.795183	70078.557711	33.529818
827.410823	70180.879427	33.534836
828.377495	70280.778290	33.539853
828.958144	70398.151917	33.544871
830.040441	70502.896764	33.549888
830.798255	70608.478056	33.554906
831.442664	70705.655416	33.559924
832.315267	70796.718264	33.564941
833.263195	70913.555423	33.569959
833.976285	71006.455062	33.574976
834.648164	71108.809590	33.579994
835.360456	71218.339288	33.585012
836.644941	71315.836628	33.590029
837.235615	71417.508492	33.595047
838.393963	71513.189865	33.600064
838.767466	71625.117371	33.605082
839.577029	71728.579959	33.610100
840.540988	71831.461501	33.615117
841.478006	71944.024047	33.620135
842.063501	72041.063579	33.625152
842.978355	72145.169917	33.630170
843.364036	72266.673370	33.635188
844.129956	72370.322622	33.640205
845.305248	72497.884324	33.645223
845.884610	72604.210832	33.650240
847.154591	72724.855970	33.655258
847.709376	72838.280113	33.660276
848.763010	72956.363678	33.665293
848.991555	73079.225374	33.670311
849.882912	73196.056149	33.675328
851.134154	73318.606818	33.680346
851.745713	73433.126554	33.685364
852.592057	73565.317358	33.690381
853.791600	73694.286946	33.695399
854.565652	73813.102061	33.700416
855.416194	73930.056437	33.705434
856.379243	74057.253514	33.710452
857.176021	74173.571383	33.715469
857.891543	74299.149057	33.720487
858.526850	74422.459889	33.725504
859.438915	74544.765285	33.730522
860.384857	74675.742638	33.735540
861.601181	74804.740272	33.740557
862.625515	74923.204441	33.745575
863.593463	75050.988129	33.750592
864.696901	75177.408509	33.755610
865.552862	75294.355303	33.760628
866.277249	75400.125519	33.765645
867.150336	75524.050177	33.770663
868.003790	75644.317663	33.775680
868.871324	75759.187237	33.780698
869.780270	75877.965004	33.785716
870.671851	75995.846630	33.790733
871.179655	76120.527915	33.795751
872.529341	76249.992922	33.800768
873.709370	76365.880199	33.805786
874.519354	76491.149242	33.810804
875.307510	76610.278480	33.815821
876.043305	76721.651148	33.820839
876.758949	76836.409711	33.825856
878.077344	76945.247195	33.830874
878.693405	77072.424103	33.835892
880.254403	77183.821460	33.840909
880.581628	77300.479633	33.845927
881.864095	77417.685470	33.850944
882.764638	77527.642144	33.855962
883.464131	77641.697200	33.860980
884.398210	77748.571159	33.865997
884.804357	77864.547959	33.871015
885.455694	77988.201828	33.876032
886.408083	78094.972919	33.881050
887.087258	78235.953798	33.886068
888.353346	78349.086955	33.891085
889.238557	78466.587499	33.896103
889.824174	78581.741099	33.901120
890.784566	78697.887990	33.906138
891.522860	78816.844577	33.911156
892.872949	78924.342061	33.916173
893.637344	79035.339563	33.921191
894.345791	79144.027879	33.926208
895.570997	79263.885643	33.931226
896.210522	79380.757086	33.936244
897.220407	79487.727254	33.941261
897.794263	79608.423290	33.946279
898.631919	79716.789559	33.951296
899.651339	79836.491977	33.956314
900.121287	79953.329030	33.961332
901.328641	80081.060659	33.966349
902.357775	80204.981987	33.971367
902.989553	80328.383292	33.976384
904.195129	80441.673815	33.981402
904.788645	80571.619585	33.986420
905.625126	80699.576812	33.991437
906.912774	80832.544472	33.996455
907.463778	80958.216379	34.001472
908.673942	81083.861655	34.006490
909.227002	81223.040296	34.011508
910.428300	81347.117090	34.016525
911.156813	81478.933715	34.021543
911.934023	81605.688039	34.026560
912.708588	81733.444272	34.031578
913.914147	81873.524882	34.036596
914.961965	82012.186495	34.041613
916.078090	82144.794431	34.046631
916.639324	82280.125273	34.051648
917.884925	82403.730972	34.056666
918.490368	82543.845509	34.061684
919.859627	82678.253501	34.066701
920.611473	82803.420684	34.071719
921.559751	82940.265202	34.076736
922.662923	83061.070539	34.081754
923.633889	83199.800663	34.086772
924.682817	83318.322201	34.091789
925.903226	83454.632421	34.096807
926.325429	83579.499841	34.101824
927.272713	83708.086843	34.106842
928.157897	83844.502091	34.111860
929.255096	83973.041467	34.116877
930.257213	84101.507610	34.121895
930.934027	84227.377007	34.126912
932.292965	84363.720543	34.131930
932.955074	84495.396793	34.136948
934.171054	84634.665698	34.141965
934.937263	84765.161125	34.146983
936.132724	84895.247805	34.152000
937.158255	85010.890920	34.157018
937.660009	85150.654285	34.162036
939.004289	85272.609619	34.167053
940.126092	85404.471466	34.172071
940.694859	85532.631681	34.177088
941.960045	85655.196576	34.182106
942.425636	85788.290692	34.187124
943.469300	85915.415186	34.192141
944.579375	86042.871977	34.197159
945.302016	86178.563376	34.202176
946.428074	86315.738224	34.207194
947.115676	86440.348345	34.212212
948.000848	86571.834352	34.217229
949.081800	86690.592805	34.222247
949.580548	86834.723938	34.227264
950.747770	86969.943889	34.232282
951.653223	87110.299724	34.237300
952.971285	87229.922973	34.242317
954.182909	87354.556311	34.247335
954.725523	87482.716497	34.252352
955.925036	87595.085787	34.257370
956.539731	87723.413149	34.262388
957.039168	87847.311018	34.267405
958.731080	87974.418980	34.272423
959.305812	88097.647129	34.277440
960.124557	88219.937817	34.282458
961.338126	88354.092349	34.287476
962.188739	88483.539302	34.292493
963.190069	88619.109612	34.297511
963.554960	88755.705320	34.302528
964.871648	88887.273493	34.307546
965.736185	89030.141448	34.312564
966.282724	89158.257574	34.317581
967.529195	89301.434552	34.322599
968.163677	89445.683883	34.327616
969.460733	89580.502561	34.332634
970.303849	89736.190039	34.337652
971.484152	89880.317986	34.342669
972.367044	90025.202911	34.347687
973.480719	90163.436768	34.352704
974.703720	90309.410441	34.357722
975.347989	90464.638557	34.362740
975.988435	90605.610028	34.367757
976.956840	90754.350590	34.372775
978.056902	90900.536484	34.377792
978.918085	91042.083781	34.382810
980.146941	91200.481369	34.387828
981.085436	91355.820087	34.392845
982.149452	91499.403648	34.397863
983.240173	91651.450106	34.402880
984.410778	91803.117262	34.407898
985.573235	91950.477163	34.412916
986.193153	92098.214233	34.417933
987.354515	92237.476730	34.422951
988.316615	92395.516729	34.427968
989.152550	92544.274125	34.432986
990.366613	92698.461180	34.438004
991.133249	92850.513658	34.443021
992.268275	92998.694094	34.448039
993.325434	93163.859092	34.453056
994.667581	93299.080178	34.458074
995.343845	93454.914252	34.463092
996.658416	93609.660522	34.468109
997.500933	93750.919097	34.473127
998.208960	93901.249452	34.478144
999.298069	94053.282731	34.483162
1000.574947	94207.429486	34.488180
1001.393720	94363.993675	34.493197
1002.439676	94514.730413	34.498215
1003.422584	94669.559262	34.503232
1004.425733	94826.451829	34.508250
1005.487780	94973.398280	34.513268
1006.680610	95120.439028	34.518285
1008.124918	95273.233910	34.523303
1008.860514	95416.633650	34.528320
1010.016422	95570.539906	34.533338
1010.965469	95726.152528	34.538356
1011.869894	95863.177244	34.543373
1013.290519	96013.152704	34.548391
1013.951298	96154.564720	34.553408
1015.129591	96305.872479	34.558426
1016.122535	96450.656382	34.563444
1016.776739	96604.811046	34.568461
1018.242107	96739.279880	34.573479
1019.318691	96894.269846	34.578496
1020.050029	97020.932058	34.583514
1020.815643	97165.412564	34.588532
1022.054748	97306.903988	34.593549
1022.914623	97433.889992	34.598567
1023.874001	97584.021188	34.603584
1025.088658	97713.437390	34.608602
1026.036655	97862.291332	34.613620
1026.947687	98004.306265	34.618637
1027.832641	98143.917304	34.623655
1028.819353	98296.582954	34.628672
1029.930350	98431.431357	34.633690
1031.226447	98590.553274	34.638708
1031.810401	98731.494386	34.643725
1032.944687	98877.382793	34.648743
1033.841441	99029.977280	34.653760
1034.728100	99187.733731	34.658778
1035.856095	99326.475163	34.663796
1036.617385	99490.058952	34.668813
1037.800579	99646.478124	34.673831
1038.688638	99802.335738	34.678848
1039.531061	99956.654579	34.683866
1040.923174	100118.976444	34.688884
1041.857090	100288.001310	34.693901
1042.840794	100443.834354	34.698919
1043.883093	100616.989599	34.703936
1045.250660	100783.350184	34.708954
1046.308570	100949.379758	34.713972
1047.325722	101102.827252	34.718989
1048.521052	101261.762547	34.724007
1049.730410	101428.328678	34.729024
1050.612584	101588.772577	34.734042
1051.812254	101746.378326	34.739060
1052.428995	101906.979439	34.744077
1053.649619	102075.131879	34.749095
1054.685145	102249.932326	34.754112
1055.761148	102407.395778	34.759130
1057.390960	102572.887587	34.764148
1058.279297	102744.290466	34.769165
1059.362495	102905.026258	34.774183
1060.526850	103072.786858	34.779200
1061.381847	103228.818071	34.784218
1062.549031	103390.519333	34.789236
1063.568981	103557.899260	34.794253
1064.862357	103711.353659	34.799271
1065.951510	103880.030307	34.804288
1066.793684	104047.148897	34.809306
1067.918132	104215.314541	34.814324
1068.978937	104387.003158	34.819341
1070.316022	104544.232960	34.824359
1071.487710	104702.630540	34.829376
1072.725851	104865.240727	34.834394
1073.668018	105026.706159	34.839412
1074.522397	105179.804889	34.844429
1075.996543	105344.941717	34.849447
1077.001477	105509.417385	34.854464
1077.993389	105673.731051	34.859482
1079.179903	105829.227914	34.864500
1080.046934	105993.182280	34.869517
1081.301048	106151.903408	34.874535
1082.239685	106302.470693	34.879552
1083.143973	106471.886614	34.884570
1084.614833	106635.572010	34.889588
1085.213220	106800.028791	34.894605
1086.601491	106953.559114	34.899623
1087.457990	107124.469332	34.904640
1088.480774	107276.587401	34.909658
1089.933438	107441.078349	34.914676
1090.900424	107617.996927	34.919693
1092.282174	107756.289889	34.924711
1093.003806	107912.439603	34.929728
1093.874670	108063.278818	34.934746
1095.369307	108219.562509	34.939764
1096.076230	108370.771107	34.944781
1097.188910	108524.592493	34.949799
1097.989488	108676.776863	34.954816
1098.892426	108841.322477	34.959834
1100.482419	109001.272226	34.964852
1101.014259	109168.261506	34.969869
1102.161877	109331.794679	34.974887
1103.362523	109495.459807	34.979904
1104.244255	109666.797054	34.984922
1105.752708	109834.308715	34.989940
1106.278587	110011.967921	34.994957
1107.699319	110170.973034	34.999975
1108.534755	110346.822743	35.004992
1109.734302	110524.810231	35.010010
1111.473102	110699.429651	35.015028
1112.583303	110873.450850	35.020045
1113.369357	111041.930999	35.025063
1114.763367	111223.112706	35.030080
1115.478163	111396.995458	35.035098
1116.906663	111571.135098	35.040116
1117.569191	111751.558950	35.045133
1119.001436	111922.541899	35.050151
1120.140607	112109.652468	35.055168
1121.124606	112283.408601	35.060186
1122.265718	112458.497977	35.065204
1123.727757	112647.780190	35.070221
1124.462321	112821.755521	35.075239
1126.027805	112998.074679	35.080256
1126.988900	113186.753287	35.085274
1128.266927	113355.065800	35.090292
1129.057293	113543.012034	35.095309
1130.640238	113730.492725	35.100327
1131.390935	113907.945789	35.105344
1132.657664	114092.040819	35.110362
1133.730413	114271.588625	35.115380
1134.903479	114449.143068	35.120397
1135.978554	114638.255240	35.125415
1137.245346	114826.590071	35.130432
1138.347113	115006.631567	35.135450
1140.025311	115195.525350	35.140468
1140.993652	115378.037402	35.145485
1142.055794	115558.696589	35.150503
1142.832384	115738.209122	35.155520
1143.843890	115925.143608	35.160538
1145.933207	116097.210122	35.165556
1146.803566	116288.290667	35.170573
1147.547803	116470.640231	35.175591
1149.067194	116651.841954	35.180608
1150.238245	116842.231388	35.185626
1151.669631	117016.751633	35.190644
1152.357695	117208.727911	35.195661
1153.630956	117395.539978	35.200679
1155.252504	117569.030984	35.205696
1155.939274	117751.586019	35.210714
1157.208859	117930.752824	35.215732
1158.241414	118121.766555	35.220749
1159.393253	118309.426616	35.225767
1160.875572	118484.567195	35.230784
1161.893833	118668.952022	35.235802
1163.150341	118850.281550	35.240820
1164.252372	119037.432931	35.245837
1165.431300	119218.294337	35.250855
1166.758558	119397.065785	35.255872
1167.842913	119582.205739	35.260890
1168.947616	119743.001415	35.265908
1170.049193	119914.795949	35.270925
1170.908104	120081.720207	35.275943
1172.566277	120249.357265	35.280960
1173.461303	120421.909426	35.285978
1174.263734	120598.193555	35.290996
1175.438578	120774.889529	35.296013
1176.775364	120951.954192	35.301031
1178.169565	121126.448267	35.306048
1178.650483	121309.788160	35.311066
1180.093730	121481.257056	35.316084
1181.458739	121666.883108	35.321101
1182.545145	121853.695339	35.326119
1183.891135	122030.522416	35.331136
1184.878111	122222.273921	35.336154
1185.951542	122403.255447	35.341172
1187.073418	122599.173905	35.346189
1187.791738	122780.390345	35.351207
1189.615316	122970.606394	35.356224
1190.493528	123171.373724	35.361242
1191.878550	123357.562755	35.366260
1192.949725	123556.475048	35.371277
1194.004273	123754.249191	35.376295
1195.650318	123948.722137	35.381312
1196.891930	124148.283047	35.386330
1198.061567	124337.846805	35.391348
1199.419564	124526.164086	35.396365
1200.314272	124721.138969	35.401383
1201.739825	124919.317462	35.406400
1202.423936	125119.617450	35.411418
1203.879992	125318.757287	35.416436
1205.162343	125510.934995	35.421453
1206.636200	125715.376968	35.426471
1207.576981	125913.331709	35.431488
1209.107600	126111.385372	35.436506
1210.056117	126314.111055	35.441524
1211.348872	126506.647037	35.446541
1212.340273	126715.242002	35.451559
1213.872879	126905.534773	35.456576
1214.910681	127113.401325	35.461594
1216.363082	127314.467156	35.466612
1217.840776	127507.981130	35.471629
1218.906906	127713.867052	35.476647
1220.356905	127917.219874	35.481664
1221.448898	128117.863884	35.486682
1222.981985	128320.254105	35.491700
1224.035010	128509.829971	35.496717
1225.079924	128700.156526	35.501735
1226.828429	128900.193998	35.506752
1227.767726	129111.663798	35.511770
1229.188727	129306.057700	35.516788
1230.694552	129501.593802	35.521805
1231.780094	129700.216301	35.526823
1232.848116	129887.436052	35.531840
1234.012252	130097.517955	35.536858
1235.382691	130282.154504	35.541876
1236.766497	130479.224061	35.546893
1237.579631	130669.976353	35.551911
1239.068117	130867.640334	35.556928
1240.068322	131073.146861	35.561946
1241.249426	131258.426274	35.566964
1242.937880	131467.037073	35.571981
1244.498152	131670.492067	35.576999
1245.448402	131847.778367	35.582016
1246.769663	132047.491375	35.587034
1248.024800	132247.405975	35.592052
1249.334513	132439.281036	35.597069
1250.686999	132626.074762	35.602087
1252.139924	132803.451199	35.607104
1253.237969	132983.789639	35.612122
1254.346530	133159.026252	35.617140
1255.563849	133337.888249	35.622157
1256.497902	133519.726459	35.627175
1258.016862	133707.095081	35.632192
1259.041770	133886.649238	35.637210
1260.321573	134063.220346	35.642228
1261.536860	134256.983371	35.647245
1262.164311	134443.327240	35.652263
1263.343809	134633.836371	35.657280
1264.574970	134833.753699	35.662298
1266.003281	135034.770408	35.667316
1267.232058	135233.471702	35.672333
1268.326617	135442.054615	35.677351
1269.588215	135642.694060	35.682368
1271.035221	135841.681099	35.687386
1272.159736	136051.924461	35.692404
1273.352728	136259.036401	35.697421
1274.715426	136477.835380	35.702439
1276.251474	136671.355488	35.707456
1277.194993	136883.965931	35.712474
1278.675136	137105.008313	35.717492
1280.169701	137302.395313	35.722509
1281.272054	137517.927893	35.727527
1282.659658	137725.333212	35.732544
1283.643444	137937.510726	35.737562
1285.278454	138154.422246	35.742580
1286.538399	138362.916364	35.747597
1287.523934	138579.385838	35.752615
1289.142640	138790.681028	35.757632
1290.526811	139011.531734	35.762650
1291.761882	139216.492889	35.767668
1293.008393	139428.280674	35.772685
1294.325336	139653.269338	35.777703
1295.842768	139863.278036	35.782720
1297.159372	140082.532585	35.787738
1298.571917	140303.131039	35.792756
1299.989760	140507.992997	35.797773
1301.029507	140726.354704	35.802791
1302.486239	140936.098405	35.807808
1303.537871	141160.412288	35.812826
1304.742894	141377.888079	35.817844
1306.134913	141591.896269	35.822861
1307.444850	141816.464645	35.827879
1308.809619	142034.667145	35.832896
1310.074559	142258.470429	35.837914
1311.432624	142478.503506	35.842932
1313.097265	142696.915840	35.847949
1314.010270	142926.209187	35.852967
1315.435885	143139.876200	35.857984
1316.945356	143361.006366	35.863002
1318.293991	143581.071207	35.868020
1319.693505	143795.367015	35.873037
1320.714639	144021.069417	35.878055
1322.195085	144240.088493	35.883072
1323.495796	144473.453110	35.888090
1324.954696	144686.550387	35.893108
1326.207341	144907.207205	35.898125
1327.445601	145136.421681	35.903143
1328.846155	145350.076640	35.908160
1329.932281	145576.740414	35.913178
1331.602405	145800.458028	35.918196
1333.124583	146018.830944	35.923213
1334.254139	146239.170095	35.928231
1335.667204	146460.620817	35.933248
1337.065474	146677.251676	35.938266
1338.135439	146899.329140	35.943284
1339.496556	147099.061178	35.948301
1340.544998	147313.858260	35.953319
1342.193550	147509.904104	35.958336
1343.769562	147720.215928	35.963354
1344.861404	147933.054081	35.968372
1346.206932	148130.926660	35.973389
1346.900873	148351.939479	35.978407
1348.572423	148576.138428	35.983424
1349.882075	148786.851594	35.988442
1351.256793	149007.773272	35.993460
1352.392871	149221.333170	35.998477
1353.441620	149451.599018	36.003495
1354.759659	149665.411449	36.008512
1356.621397	149899.359904	36.013530
1357.441695	150131.174906	36.018548
1359.435373	150347.943357	36.023565
1360.162779	150577.896195	36.028583
1361.756569	150817.970674	36.033600
1363.145702	151048.989710	36.038618
1364.403269	151278.862507	36.043636
1365.925525	151510.560789	36.048653
1366.798067	151754.204906	36.053671
1368.325055	151984.660456	36.058688
1369.643298	152217.662997	36.063706
1370.864820	152464.619443	36.068724
1372.365090	152712.421917	36.073741
1373.757992	152960.178821	36.078759
1375.254101	153203.871283	36.083776
1376.719793	153458.054821	36.088794
1378.214126	153702.333630	36.093812
1379.723808	153940.048218	36.098829
1381.105660	154184.194369	36.103847
1382.260996	154431.956790	36.108864
1383.530104	154672.606358	36.113882
1385.044002	154925.227468	36.118900
1386.717016	155168.316664	36.123917
1387.755698	155426.891849	36.128935
1389.028505	155686.053564	36.133952
1391.157038	155929.582413	36.138970
1392.472784	156180.411955	36.143988
1394.140722	156410.545896	36.149005
1395.473154	156671.530648	36.154023
1396.762124	156921.301162	36.159040
1398.371747	157160.942834	36.164058
1399.366802	157413.059173	36.169076
1401.294593	157660.930109	36.174093
1402.388916	157904.413106	36.179111
1403.718246	158148.050724	36.184128
1405.317805	158403.643884	36.189146
1406.892499	158643.982444	36.194164
1408.225020	158878.723189	36.199181
1409.400861	159133.636704	36.204199
1410.865403	159388.975810	36.209216
1412.390636	159631.890421	36.214234
1413.653384	159886.564918	36.219252
1415.320515	160126.463137	36.224269
1416.487380	160385.217217	36.229287
1418.097269	160638.469324	36.234304
1419.284395	160893.337483	36.239322
1420.266585	161145.166397	36.244340
1422.285280	161398.560688	36.249357
1423.802675	161646.156317	36.254375
1425.389259	161900.508935	36.259392
1426.997250	162154.275199	36.264410
1428.137549	162417.662981	36.269428
1429.770373	162664.444612	36.274445
1431.491970	162914.133364	36.279463
1432.620307	163143.805391	36.284480
1433.849845	163379.074052	36.289498
1435.159895	163617.403417	36.294516
1436.810972	163847.618189	36.299533
1438.001580	164085.447389	36.304551
1439.220129	164316.505953	36.309568
1440.872173	164546.583330	36.314586
1441.911466	164786.089225	36.319604
1443.417927	165030.055465	36.324621
1444.837199	165275.737555	36.329639
1445.964123	165517.454200	36.334656
1447.481287	165763.770250	36.339674
1449.100475	166017.511416	36.344692
1450.423956	166276.149916	36.349709
1451.856667	166521.770886	36.354727
1453.066738	166775.147181	36.359744
1454.467362	167028.139063	36.364762
1456.020510	167295.658539	36.369780
1457.400888	167559.473195	36.374797
1458.297879	167831.414338	36.379815
1459.859103	168088.879596	36.384832
1461.634174	168352.800484	36.389850
1463.320651	168625.979668	36.394868
1465.002241	168883.124213	36.399885
1466.216068	169158.893418	36.404903
1467.626731	169435.089960	36.409920
1469.344481	169700.535705	36.414938
1470.800835	169980.155407	36.419956
1472.384105	170240.697601	36.424973
1473.639841	170521.480813	36.429991
1475.310659	170787.445702	36.435008
1477.037263	171058.164358	36.440026
1478.162753	171334.615771	36.445044
1479.968730	171611.609264	36.450061
1481.196200	171883.996195	36.455079
1483.052074	172161.618759	36.460096
1484.452869	172440.596022	36.465114
1485.984231	172718.626921	36.470132
1487.379630	172989.924869	36.475149
1489.003508	173260.438827	36.480167
1490.502014	173541.804636	36.485184
1492.132948	173821.525388	36.490202
1493.562402	174097.608946	36.495220
1495.357994	174361.230193	36.500237
1496.722315	174638.405145	36.505255
1498.308773	174926.212690	36.510272
1499.793175	175193.732893	36.515290
1501.113326	175467.565285	36.520308
1502.963907	175748.439281	36.525325
1504.370014	176024.012430	36.530343
1505.831888	176295.768274	36.535360
1507.827521	176567.936700	36.540378
1508.812594	176847.349882	36.545396
1510.419524	177115.542829	36.550413
1512.097441	177383.090591	36.555431
1513.262039	177664.941876	36.560448
1515.136144	177937.794049	36.565466
1516.645950	178218.983591	36.570484
1518.451835	178486.184596	36.575501
1519.825659	178769.276600	36.580519
1521.150459	179036.706966	36.585536
1522.784324	179306.400946	36.590554
1523.975473	179591.733762	36.595572
1525.467562	179872.753580	36.600589
1527.190309	180157.776419	36.605607
1528.044276	180429.932437	36.610624
1530.020523	180715.526902	36.615642
1531.741563	181001.898743	36.620660
1533.215233	181277.668397	36.625677
1534.720028	181541.192094	36.630695
1536.100971	181803.415213	36.635712
1537.685987	182065.099159	36.640730
1538.779981	182329.095734	36.645748
1540.628452	182597.749866	36.650765
1542.247508	182861.233965	36.655783
1543.432602	183136.978018	36.660800
1545.282467	183402.510155	36.665818
1546.427223	183671.506001	36.670836
1548.093169	183951.190096	36.675853
1549.300312	184231.607160	36.680871
1550.789798	184514.393724	36.685888
1552.493151	184791.305845	36.690906
1553.647465	185079.200856	36.695924
1555.170088	185366.886644	36.700941
1556.950501	185684.097580	36.705959
1557.937818	186011.745731	36.710976
1559.748073	186314.146138	36.715994
1561.134334	186610.949701	36.721012
1562.915970	186918.512413	36.726029
1564.680226	187209.594402	36.731047
1566.200372	187520.095324	36.736064
1567.663643	187808.635275	36.741082
1569.372806	188127.261664	36.746100
1570.675892	188423.372046	36.751117
1572.367474	188733.697182	36.756135
1574.199969	189035.441325	36.761152
1575.900574	189342.871134	36.766170
1577.676574	189653.820596	36.771188
1578.914329	189960.918107	36.776205
1580.499998	190266.895172	36.781223
1581.886515	190572.142198	36.786240
1583.852227	190879.585406	36.791258
1585.348243	191197.745721	36.796276
1587.292343	191503.669893	36.801293
1588.788565	191796.913831	36.806311
1590.228187	192115.466397	36.811328
1592.115581	192426.735901	36.816346
1594.179158	192744.684422	36.821364
1595.512227	193046.720133	36.826381
1597.478961	193342.510371	36.831399
1598.643173	193654.327903	36.836416
1600.808411	193957.454776	36.841434
1602.279208	194270.749871	36.846452
1603.777539	194572.534678	36.851469
1606.096505	194873.912325	36.856487
1607.213792	195184.877185	36.861504
1608.786625	195483.426418	36.866522
1610.779393	195779.167231	36.871540
1612.314984	196090.627512	36.876557
1614.065985	196395.424984	36.881575
1615.862763	196694.907025	36.886592
1617.056922	196989.327480	36.891610
1618.981644	197289.451181	36.896628
1620.426454	197585.205307	36.901645
1622.296783	197883.840036	36.906663
1623.890421	198191.485505	36.911680
1625.164095	198498.114798	36.916698
1626.946538	198804.512674	36.921716
1628.470959	199104.550245	36.926733
1630.311035	199398.340903	36.931751
1631.966676	199700.238827	36.936768
1633.421988	199998.053532	36.941786
1635.440853	200299.921141	36.946804
1636.885519	200610.033275	36.951821
1638.300345	200909.583326	36.956839
1640.104530	201211.994242	36.961856
1641.655187	201495.139601	36.966874
1642.945026	201780.917287	36.971892
1644.488701	202072.041030	36.976909
1646.438544	202360.027993	36.981927
1647.551584	202636.918477	36.986944
1649.504340	202938.978898	36.991962
1651.189256	203218.905284	36.996980
1652.593880	203513.660281	37.001997
1654.162672	203804.732067	37.007015
1655.651194	204111.947571	37.012032
1657.355842	204400.382524	37.017050
1658.791560	204710.223721	37.022068
1660.683889	205007.063911	37.027085
1662.314921	205308.746570	37.032103
1663.791577	205618.709771	37.037120
1665.430302	205930.502486	37.042138
1667.171970	206239.078778	37.047156
1668.764871	206547.729601	37.052173
1670.471461	206865.304938	37.057191
1672.144395	207184.689614	37.062208
1673.913906	207489.020991	37.067226
1675.457895	207807.664628	37.072244
1676.758481	208129.801622	37.077261
1678.553033	208454.427474	37.082279
1680.269076	208789.506778	37.087296
1681.973012	209109.168642	37.092314
1683.985279	209433.533077	37.097332
1685.330998	209766.004284	37.102349
1687.223520	210096.662910	37.107367
1688.640375	210417.565264	37.112384
1690.321750	210756.209000	37.117402
1692.236411	211098.322314	37.122420
1694.036299	211435.881367	37.127437
1695.569841	211765.429572	37.132455
1697.436210	212107.653229	37.137472
1698.773751	212440.738522	37.142490
1700.738001	212779.162461	37.147508
1702.262433	213124.895612	37.152525
1704.414518	213454.704420	37.157543
1706.150479	213803.504403	37.162560
1707.797570	214144.646717	37.167578
1709.736717	214480.866129	37.172596
1711.457889	214814.071502	37.177613
1713.581242	215158.010823	37.182631
1715.304351	215495.611317	37.187648
1716.886755	215824.418980	37.192666
1718.515339	216165.261083	37.197684
1720.298166	216507.298692	37.202701
1722.058115	216846.825149	37.207719
1723.830835	217180.252914	37.212736
1725.372171	217519.331371	37.217754
1727.464928	217863.125094	37.222772
1728.847667	218210.231038	37.227789
1731.212810	218552.331302	37.232807
1732.695654	218889.057168	37.237824
1734.222714	219219.323683	37.242842
1736.283903	219557.026355	37.247860
1737.841494	219904.359897	37.252877
1739.790529	220236.567764	37.257895
1741.797126	220577.480339	37.262912
1743.275345	220909.838362	37.267930
1745.146125	221238.654719	37.272948
1746.648882	221573.320896	37.277965
1748.388888	221910.998535	37.282983
1750.454999	222250.835390	37.288000
1752.273191	222578.440963	37.293018
1754.211679	222906.612076	37.298036
1755.550281	223250.983309	37.303053
1757.711282	223562.962727	37.308071
1759.325751	223878.025392	37.313088
1761.062356	224194.720245	37.318106
1762.928423	224510.480317	37.323124
1764.505253	224810.331904	37.328141
1766.052410	225124.693878	37.333159
1767.776023	225445.506285	37.338176
1769.376957	225761.942979	37.343194
1771.347549	226082.792933	37.348212
1772.944670	226402.608935	37.353229
1774.589252	226715.964844	37.358247
1776.171791	227047.748385	37.363264
1778.064225	227380.118486	37.368282
1779.757775	227713.408794	37.373300
1781.325857	228044.864173	37.378317
1783.264242	228381.647192	37.383335
1784.682092	228727.606230	37.388352
1786.389727	229065.212698	37.393370
1788.149303	229406.824769	37.398388
1790.168388	229758.379896	37.403405
1791.424981	230102.534616	37.408423
1793.344702	230455.299001	37.413440
1795.259403	230814.262588	37.418458
1797.130381	231174.426829	37.423476
1798.769043	231530.715025	37.428493
1800.410383	231890.736989	37.433511
1802.444705	232259.995088	37.438528
1804.293664	232622.067247	37.443546
1805.989019	232984.620477	37.448564
1807.800102	233361.254506	37.453581
1809.773036	233726.609015	37.458599
1811.414267	234087.493268	37.463616
1813.122915	234454.666839	37.468634
1814.930470	234830.741365	37.473652
1816.757121	235203.179832	37.478669
1818.243930	235574.883623	37.483687
1820.551033	235945.696595	37.488704
1822.528673	236330.405782	37.493722
1824.573391	236710.455199	37.498740
1826.426668	237091.550314	37.503757
1828.410244	237465.384587	37.508775
1829.953460	237838.830084	37.513792
1831.607036	238225.467738	37.518810
1833.589922	238603.822644	37.523828
1835.815063	238981.453279	37.528845
1837.437258	239360.193923	37.533863
1839.887776	239745.028299	37.538880
1841.125606	240124.005900	37.543898
1843.400873	240489.179035	37.548916
1845.248959	240874.156906	37.553933
1847.334441	241249.596233	37.558951
1849.543639	241619.325320	37.563968
1851.339609	241993.868921	37.568986
1852.897608	242371.827809	37.574004
1854.750956	242739.146774	37.579021
1856.366166	243106.756457	37.584039
1858.613395	243484.808921	37.589056
1860.512945	243869.037278	37.594074
1862.235062	244234.850172	37.599092
1864.099363	244611.106201	37.604109
1865.903740	244985.110080	37.609127
1868.016958	245356.499272	37.614144
1870.059105	245736.281826	37.619162
1872.036088	246107.894172	37.624180
1873.683935	246489.540572	37.629197
1875.362133	246852.815358	37.634215
1877.376009	247219.821908	37.639232
1879.256433	247600.845414	37.644250
1881.535103	247973.143565	37.649268
1883.114746	248320.884561	37.654285
1885.099478	248667.367576	37.659303
1886.728694	249021.780256	37.664320
1888.425839	249378.493184	37.669338
1890.045972	249728.257201	37.674356
1891.901682	250081.285907	37.679373
1893.626266	250438.906754	37.684391
1895.457749	250802.047736	37.689408
1896.873333	251172.111510	37.694426
1898.959390	251543.314201	37.699444
1900.911669	251912.758806	37.704461
1902.667526	252290.031613	37.709479
1904.609243	252668.595288	37.714496
1906.580946	253060.184375	37.719514
1908.555189	253432.060364	37.724532
1910.335264	253816.742763	37.729549
1911.935070	254206.710442	37.734567
1914.355170	254585.372069	37.739584
1915.812285	254977.163432	37.744602
1917.710087	255369.164138	37.749620
1919.469800	255770.583761	37.754637
1921.235843	256173.195042	37.759655
1923.548386	256568.200879	37.764672
1925.145892	256978.126161	37.769690
1927.485954	257390.728049	37.774708
1929.551250	257788.639127	37.779725
1931.183943	258196.522912	37.784743
1933.430290	258592.929855	37.789760
1935.029430	259008.410993	37.794778
1937.111073	259423.891411	37.799796
1939.180575	259841.683718	37.804813
1941.058575	260253.078239	37.809831
1943.349997	260665.803634	37.814848
1945.239270	261075.034461	37.819866
1946.815386	261488.427620	37.824884
1949.073891	261904.963681	37.829901
1951.031978	262323.500977	37.834919
1953.074066	262744.639710	37.839936
1954.755892	263163.953613	37.844954
1957.142783	263584.298544	37.849972
1959.094767	264007.021211	37.854989
1960.912152	264425.648554	37.860007
1963.180154	264836.939533	37.865024
1965.105066	265257.375438	37.870042
1966.982686	265673.118194	37.875060
1969.053726	266094.162747	37.880077
1971.118809	266527.169292	37.885095
1973.451970	266938.390722	37.890112
1975.376277	267365.446915	37.895130
1977.628010	267778.988810	37.900148
1979.861518	268183.261373	37.905165
1981.539823	268612.306186	37.910183
1983.515568	269027.790700	37.915200
1985.082570	269451.058314	37.920218
1987.347898	269863.573007	37.925236
1989.530343	270282.981609	37.930253
1991.637321	270708.266941	37.935271
1993.899380	271106.756975	37.940288
1995.873379	271528.605144	37.945306
1997.665978	271938.847709	37.950324
1999.869795	272343.411230	37.955341
2001.846253	272757.887898	37.960359
2003.997707	273162.328788	37.965376
2005.839788	273573.114578	37.970394
2007.938800	273985.356577	37.975412
2010.075048	274392.714578	37.980429
2012.107085	274814.613660	37.985447
2014.021138	275209.481950	37.990464
2015.957624	275602.719465	37.995482
2018.378625	275984.578006	38.000500
2020.020789	276359.674284	38.005517
2021.905823	276749.257227	38.010535
2023.805173	277138.328101	38.015552
2025.492424	277530.045982	38.020570
2027.974944	277918.716993	38.025588
2029.865036	278310.450000	38.030605
2031.468913	278714.821816	38.035623
2033.915690	279110.349103	38.040640
2035.454843	279512.923753	38.045658
2037.420476	279917.029397	38.050676
2039.596066	280315.106863	38.055693
2041.336665	280727.014083	38.060711
2043.661172	281143.144685	38.065728
2045.508183	281552.262631	38.070746
2047.574200	281975.285360	38.075764
2049.740459	282385.796099	38.080781
2051.345495	282809.825604	38.085799
2053.441549	283232.099771	38.090816
2055.314220	283660.526185	38.095834
2057.162695	284095.479844	38.100852
2059.307667	284535.843917	38.105869
2061.457479	284967.443830	38.110887
2063.630751	285395.812455	38.115904
2065.909821	285849.402149	38.120922
2067.968307	286282.785469	38.125940
2069.810993	286721.379782	38.130957
2071.868114	287172.709912	38.135975
2074.403108	287613.272155	38.140992
2076.057815	288055.518057	38.146010
2078.008571	288495.480166	38.151028
2080.653292	288947.061566	38.156045
2082.936271	289404.079334	38.161063
2084.800115	289848.641572	38.166080
2087.198192	290292.482325	38.171098
2089.223565	290739.018888	38.176116
2091.418106	291184.738676	38.181133
2093.860489	291637.805082	38.186151
2095.875925	292078.442964	38.191168
2098.033787	292531.141033	38.196186
2100.332072	292973.124634	38.201204
2102.809470	293416.041777	38.206221
2104.455964	293866.626306	38.211239
2106.735960	294313.376087	38.216256
2108.728801	294749.808673	38.221274
2110.928889	295195.294812	38.226292
2113.134397	295640.370480	38.231309
2114.902472	296092.594556	38.236327
2117.633004	296545.223048	38.241344
2119.650996	296983.462834	38.246362
2121.621630	297433.918230	38.251380
2123.985408	297880.373436	38.256397
2126.168767	298324.263796	38.261415
2128.101236	298764.331009	38.266432
2129.924192	299215.582183	38.271450
2132.419747	299670.557856	38.276468
2134.618608	300105.698408	38.281485
2136.552775	300556.388026	38.286503
2139.265833	301007.459763	38.291520
2141.253744	301458.387307	38.296538
2143.416832	301909.537504	38.301556
2145.991378	302353.003821	38.306573
2147.903677	302790.629843	38.311591
2150.115833	303218.152777	38.316608
2152.271482	303664.948256	38.321626
2154.348111	304105.583763	38.326644
2156.455398	304533.366139	38.331661
2158.233995	304961.120226	38.336679
2160.415470	305389.315390	38.341696
2162.358862	305810.030561	38.346714
2164.349737	306226.597262	38.351732
2166.379800	306644.372793	38.356749
2168.174513	307082.462898	38.361767
2170.369350	307501.906160	38.366784
2172.775306	307938.801618	38.371802
2174.741783	308371.548446	38.376820
2177.117577	308807.933248	38.381837
2179.290226	309251.655988	38.386855
2181.039061	309697.903021	38.391872
2183.292805	310144.676100	38.396890
2185.253088	310587.455281	38.401908
2187.696667	311033.378165	38.406925
2189.438549	311502.782508	38.411943
2191.834341	311951.013900	38.416960
2193.892113	312405.664397	38.421978
2195.765643	312884.704308	38.426996
2198.315760	313345.258352	38.432013
2200.088694	313818.492348	38.437031
2202.222623	314297.426137	38.442048
2204.945703	314777.582463	38.447066
2206.798988	315251.525070	38.452084
2208.792142	315727.242720	38.457101
2211.403904	316225.724475	38.462119
2213.420730	316709.980520	38.467136
2215.844616	317196.070957	38.472154
2218.312370	317686.158848	38.477172
2220.614311	318164.187663	38.482189
2222.658337	318662.578563	38.487207
2224.604762	319150.828371	38.492224
2227.246998	319648.936752	38.497242
2229.327187	320139.590613	38.502260
2231.995449	320629.461723	38.507277
2234.155377	321132.855756	38.512295
2236.383242	321624.103850	38.517312
2238.908801	322122.404640	38.522330
2240.926639	322623.874655	38.527348
2243.398402	323113.570095	38.532365
2245.845767	323623.588166	38.537383
2247.761313	324117.038012	38.542400
2250.109866	324594.302107	38.547418
2253.001240	325100.883145	38.552436
2255.494923	325587.729339	38.557453
2257.531090	326088.393146	38.562471
2259.934865	326583.487484	38.567488
2262.360003	327064.034313	38.572506
2264.561753	327555.038018	38.577524
2266.915374	328052.887512	38.582541
2269.207897	328547.137639	38.587559
2271.286996	329041.846257	38.592576
2273.881751	329524.290242	38.597594
2276.109115	330021.449573	38.602612
2278.772835	330501.917175	38.607629
2280.810292	330987.576012	38.612647
2283.097412	331477.426291	38.617664
2285.307764	331970.783195	38.622682
2287.425354	332461.560660	38.627700
2290.005084	332949.874897	38.632717
2292.558461	333443.818573	38.637735
2294.799929	333930.549495	38.642752
2296.999235	334407.362181	38.647770
2298.837971	334900.713530	38.652788
2301.532096	335375.559269	38.657805
2303.756887	335872.946631	38.662823
2305.793263	336367.845542	38.667840
2308.397895	336848.850127	38.672858
2310.111763	337323.976201	38.677876
2312.734923	337785.789544	38.682893
2315.056261	338250.865478	38.687911
2317.236190	338712.000736	38.692928
2319.409188	339180.993902	38.697946
2321.395599	339647.702031	38.702964
2323.964622	340121.211648	38.707981
2326.096717	340600.363078	38.712999
2328.113473	341080.515174	38.718016
2330.483267	341568.493067	38.723034
2332.307929	342060.429759	38.728052
2334.690249	342550.294092	38.733069
2337.383316	343042.182492	38.738087
2339.388641	343544.594659	38.743104
2342.006911	344040.411398	38.748122
2343.944758	344543.326706	38.753140
2346.368678	345046.792549	38.758157
2348.945589	345544.622642	38.763175
2351.241934	346055.447586	38.768192
2353.147006	346568.735024	38.773210
2355.181862	347096.828680	38.778228
2358.010665	347613.835348	38.783245
2360.602103	348148.291435	38.788263
2362.616137	348664.115970	38.793280
2365.429978	349182.723297	38.798298
2367.678015	349702.754795	38.803316
2370.155314	350232.098333	38.808333
2372.336397	350767.590168	38.813351
2374.878524	351311.079455	38.818368
2377.222073	351835.498916	38.823386
2379.842507	352370.084092	38.828404
2382.451981	352908.490407	38.833421
2384.753989	353448.685069	38.838439
2387.182939	353980.433637	38.843456
2389.826583	354516.931215	38.848474
2392.015558	355062.237083	38.853492
2394.644349	355590.935664	38.858509
2397.141069	356125.045661	38.863527
2399.381625	356679.466819	38.868544
2401.984694	357207.026497	38.873562
2404.165962	357755.936666	38.878580
2406.954363	358286.921693	38.883597
2409.580853	358831.484298	38.888615
2412.012107	359370.567156	38.893632
2414.635248	359904.667614	38.898650
2416.946827	360459.465326	38.903668
2419.676121	360978.347162	38.908685
2421.433835	361522.109977	38.913703
2423.901286	362056.652705	38.918720
2426.696887	362599.827948	38.923738
2429.372555	363145.749227	38.928756
2431.512822	363685.585437	38.933773
2434.035484	364228.595933	38.938791
2436.441694	364770.828908	38.943808
2439.165033	365304.816379	38.948826
2441.547101	365850.454295	38.953844
2444.209716	366390.031948	38.958861
2446.603683	366931.922250	38.963879
2448.481212	367470.386013	38.968896
2451.093466	368013.057954	38.973914
2453.545045	368553.337357	38.978932
2456.064097	369101.603246	38.983949
2458.790393	369637.207152	38.988967
2461.050622	370182.021031	38.993984
2463.502712	370730.214965	38.999002
2466.071737	371265.406930	39.004020
2468.743400	371811.872943	39.009037
2470.905022	372337.682505	39.014055
2473.270813	372861.321870	39.019072
2476.279772	373371.600048	39.024090
2478.062499	373888.166334	39.029108
2480.645691	374396.313154	39.034125
2483.092303	374906.650604	39.039143
2485.430048	375430.422436	39.044160
2487.659591	375951.566369	39.049178
2490.304292	376473.800595	39.054196
2492.539805	376995.252690	39.059213
2495.318782	377527.071688	39.064231
2497.426462	378060.099651	39.069248
2500.101977	378597.207695	39.074266
2502.526961	379128.822001	39.079284
2504.702327	379666.087860	39.084301
2507.469859	380209.050528	39.089319
2509.541686	380762.115625	39.094336
2512.418776	381311.294464	39.099354
2515.443035	381871.962790	39.104372
2517.358965	382413.087791	39.109389
2519.891006	382965.780666	39.114407
2522.401896	383527.936927	39.119424
2524.749766	384090.536888	39.124442
2527.358479	384665.062362	39.129460
2530.074995	385226.743856	39.134477
2532.694701	385787.237826	39.139495
2534.828821	386371.371264	39.144512
2537.414905	386936.884260	39.149530
2539.901695	387515.694136	39.154548
2542.508913	388097.991458	39.159565
2545.077520	388678.761943	39.164583
2548.003406	389274.427253	39.169600
2550.680400	389856.014061	39.174618
2552.999706	390440.985199	39.179636
2555.485007	391018.017056	39.184653
2558.502167	391610.801116	39.189671
2560.705802	392201.216896	39.194688
2563.538748	392791.823690	39.199706
2566.481044	393383.867288	39.204724
2568.865485	393969.806628	39.209741
2571.485629	394554.834105	39.214759
2573.977737	395146.499621	39.219776
2576.506146	395736.676595	39.224794
2579.297132	396325.937203	39.229812
2581.785068	396933.101019	39.234829
2584.877024	397522.740334	39.239847
2587.720294	398123.793706	39.244864
2590.188824	398715.424196	39.249882
2592.827602	399295.876791	39.254900
2595.594038	399884.495084	39.259917
2598.332479	400484.997776	39.264935
2600.708124	401072.938333	39.269952
2603.689093	401644.319560	39.274970
2606.177937	402246.030114	39.279988
2608.693350	402838.863644	39.285005
2611.427680	403426.333431	39.290023
2613.750545	404019.672420	39.295040
2616.048586	404602.928809	39.300058
2618.955680	405201.256791	39.305076
2621.836035	405798.560935	39.310093
2624.733935	406383.397903	39.315111
2627.232415	406976.833833	39.320128
2630.195189	407575.089631	39.325146
2632.714784	408166.314661	39.330164
2634.889006	408761.119787	39.335181
2637.578364	409354.411586	39.340199
2640.059412	409937.145468	39.345216
2642.681659	410534.817658	39.350234
2645.947686	411118.156207	39.355252
2648.189562	411684.589945	39.360269
2650.912432	412232.063506	39.365287
2653.352666	412796.261771	39.370304
2655.892162	413353.549831	39.375322
2658.274112	413914.844403	39.380340
2660.565746	414481.753335	39.385357
2663.625280	415044.480437	39.390375
2666.095359	415623.015951	39.395392
2668.586309	416188.482566	39.400410
2671.252340	416768.777085	39.405428
2673.459407	417354.336977	39.410445
2676.253347	417948.538562	39.415463
2678.953802	418539.096513	39.420480
2681.303005	419129.237553	39.425498
2684.085061	419724.047996	39.430516
2686.499451	420333.918481	39.435533
2689.377447	420932.927213	39.440551
2691.701841	421542.624420	39.445568
2694.477963	422164.368868	39.450586
2697.358304	422780.617164	39.455604
2699.833956	423405.303700	39.460621
2702.661458	424019.904825	39.465639
2705.344891	424659.183306	39.470656
2708.072050	425284.783932	39.475674
2710.498316	425926.186042	39.480692
2713.310255	426560.985739	39.485709
2715.925835	427201.913072	39.490727
2718.838218	427839.740308	39.495744
2721.704979	428493.477703	39.500762
2724.211031	429140.425888	39.505780
2726.889481	429787.730352	39.510797
2729.792017	430437.809094	39.515815
2732.596022	431106.431378	39.520832
2735.549465	431758.935072	39.525850
2738.511832	432425.769084	39.530868
2741.121992	433077.423176	39.535885
2743.979948	433737.355261	39.540903
2746.967287	434399.619768	39.545920
2749.975837	435041.240496	39.550938
2752.619893	435700.886187	39.555956
2755.406509	436360.790062	39.560973
2758.073462	437028.572293	39.565991
2761.090590	437697.640564	39.571008
2763.936761	438358.375382	39.576026
2766.858834	439020.894088	39.581044
2769.430228	439678.947965	39.586061
2772.442220	440338.728612	39.591079
2775.158531	441006.312009	39.596096
2778.188870	441663.416153	39.601114
2781.284541	442313.111818	39.606132
2783.788594	442979.647394	39.611149
2786.611203	443631.865162	39.616167
2789.604172	444302.519460	39.621184
2792.322451	444954.555188	39.626202
2795.455345	445604.886727	39.631220
2797.877135	446272.426982	39.636237
2801.256937	446933.076270	39.641255
2803.762633	447583.889787	39.646272
2806.556933	448239.583585	39.651290
2809.350020	448901.262796	39.656308
2811.750011	449566.816722	39.661325
2814.896418	450207.286038	39.666343
2817.792720	450877.056040	39.671360
2820.426130	451534.017910	39.676378
2823.440708	452193.824142	39.681396
2826.242405	452870.046689	39.686413
2829.119743	453513.922476	39.691431
2831.271353	454164.097416	39.696448
2834.267562	454800.284917	39.701466
2837.113232	455432.283239	39.706484
2839.625383	456072.084110	39.711501
2842.715234	456688.704634	39.716519
2845.438422	457328.224432	39.721536
2848.300722	457973.301058	39.726554
2851.024306	458600.055332	39.731572
2853.624121	459240.179763	39.736589
2856.107768	459884.537536	39.741607
2859.020451	460536.777077	39.746624
2861.779495	461190.983712	39.751642
2864.666687	461845.801153	39.756660
2867.211096	462515.582149	39.761677
2870.333574	463177.223971	39.766695
2872.933461	463844.673208	39.771712
2875.498514	464521.132125	39.776730
2878.694220	465191.058196	39.781748
2881.292027	465884.609537	39.786765
2884.124505	466570.528699	39.791783
2886.889425	467272.773506	39.796800
2890.051653	467956.263570	39.801818
2892.987604	468662.004027	39.806836
2895.702620	469358.468622	39.811853
2898.518038	470059.880988	39.816871
2901.572007	470774.590455	39.821888
2904.146482	471488.587225	39.826906
2907.179291	472203.287895	39.831924
2910.118558	472913.383089	39.836941
2913.519988	473636.535255	39.841959
2916.456908	474357.610026	39.846976
2919.585014	475089.563391	39.851994
2922.525318	475811.883313	39.857012
2925.445477	476535.534973	39.862029
2928.779843	477256.266021	39.867047
2931.724524	477980.554006	39.872064
2934.735477	478713.871801	39.877082
2937.941966	479436.388878	39.882100
2940.735639	480161.810340	39.887117
2943.367716	480884.149228	39.892135
2946.663632	481608.669331	39.897152
2949.542825	482342.140971	39.902170
2953.077027	483062.524729	39.907188
2955.909622	483801.730062	39.912205
2958.726957	484529.010951	39.917223
2961.743786	485258.443392	39.922240
2964.604842	485982.676181	39.927258
2967.952351	486720.250473	39.932276
2970.969395	487450.435289	39.937293
2974.002211	488180.431606	39.942311
2977.476749	488909.114896	39.947328
2979.764785	489643.489588	39.952346
2983.203893	490367.726030	39.957364
2985.725704	491087.890756	39.962381
2989.232343	491821.414961	39.967399
2992.486496	492546.935324	39.972416
2995.451353	493279.012444	39.977434
2998.480710	494000.267266	39.982452
3001.500377	494724.509914	39.987469
3004.439391	495446.061200	39.992487
3007.412782	496169.283821	39.997504
3010.343623	496896.958532	40.002522
3013.412789	497625.934944	40.007540
3016.656820	498357.817982	40.012557
3019.609698	499077.326494	40.017575
3022.488104	499802.599926	40.022592
3025.465399	500514.281839	40.027610
3028.631059	501240.092997	40.032628
3031.490340	501952.679070	40.037645
3034.552101	502650.301568	40.042663
3037.380330	503336.603782	40.047680
3040.356768	504032.260266	40.052698
3043.097568	504716.446944	40.057716
3045.972431	505407.020515	40.062733
3048.804594	506107.529635	40.067751
3052.278253	506800.910530	40.072768
3055.078223	507509.556418	40.077786
3057.721171	508214.468621	40.082804
3060.765843	508929.796482	40.087821
3063.105713	509642.632770	40.092839
3066.745192	510357.543431	40.097856
3069.667820	511097.527260	40.102874
3072.490374	511815.408305	40.107892
3075.594739	512559.510840	40.112909
3078.519182	513296.158859	40.117927
3081.646287	514034.948601	40.122944
3084.566961	514790.626384	40.127962
3087.958586	515543.473906	40.132980
3090.601787	516290.564926	40.137997
3093.729150	517056.191637	40.143015
3096.946430	517825.380993	40.148032
3100.091286	518592.728535	40.153050
3103.168773	519361.149137	40.158068
3106.249353	520133.044144	40.163085
3109.138781	520914.675574	40.168103
3112.478738	521697.950251	40.173120
3115.587278	522491.567996	40.178138
3119.124822	523276.930815	40.183156
3122.552924	524070.203942	40.188173
3125.310389	524848.712074	40.193191
3128.738708	525627.019463	40.198208
3131.214702	526432.610013	40.203226
3134.837562	527226.065937	40.208244
3137.942088	528022.418468	40.213261
3140.770550	528835.794236	40.218279
3144.494196	529629.641797	40.223296
3147.653397	530428.200295	40.228314
3150.906134	531225.741020	40.233332
3154.145320	532041.815845	40.238349
3157.482617	532850.341827	40.243367
3161.224150	533645.598363	40.248384
3164.217665	534452.872596	40.253402
3167.826554	535253.874760	40.258420
3170.633435	536049.680939	40.263437
3173.619573	536845.961755	40.268455
3177.066219	537656.376716	40.273472
3180.346409	538453.966683	40.278490
3183.439180	539258.913771	40.283508
3186.971279	540076.086973	40.288525
3190.371112	540865.927831	40.293543
3193.276369	541659.509792	40.298560
3196.705658	542464.550650	40.303578
3200.017801	543264.139180	40.308596
3202.978997	544057.409765	40.313613
3205.917149	544860.365976	40.318631
3209.550014	545661.155033	40.323648
3212.650637	546474.014239	40.328666
3215.618643	547269.736725	40.333684
3219.043969	548082.689887	40.338701
3222.039633	548890.240031	40.343719
3225.501320	549693.301168	40.348736
3228.880256	550488.148804	40.353754
3232.181563	551294.088177	40.358772
3235.449373	552116.725533	40.363789
3238.347270	552916.954562	40.368807
3241.652332	553701.826921	40.373824
3244.727568	554503.126239	40.378842
3247.986799	555265.145540	40.383860
3251.347876	556033.967221	40.388877
3254.249438	556798.701602	40.393895
3257.474690	557562.083494	40.398912
3260.796710	558332.868053	40.403930
3263.800893	559095.233951	40.408948
3267.153411	559866.114550	40.413965
3269.896359	560649.515710	40.418983
3273.399492	561413.257366	40.424000
3276.586513	562207.707673	40.429018
3279.494139	562999.392778	40.434036
3282.833628	563787.350394	40.439053
3285.490871	564597.449288	40.444071
3289.136684	565401.627907	40.449088
3292.107924	566207.358665	40.454106
3295.105773	567020.840968	40.459124
3298.432644	567851.138788	40.464141
3301.726827	568679.980003	40.469159
3304.923554	569502.118132	40.474176
3308.210112	570351.666639	40.479194
3311.227881	571186.727585	40.484212
3314.397323	572036.819809	40.489229
3318.068920	572891.474673	40.494247
3321.614976	573746.034742	40.499264
3324.471222	574612.397993	40.504282
3327.810085	575475.466907	40.509300
3331.275875	576350.057761	40.514317
3334.650519	577231.398862	40.519335
3338.471416	578102.245366	40.524352
3341.385934	578987.422064	40.529370
3344.437446	579860.502571	40.534388
3348.533568	580742.303761	40.539405
3351.966168	581620.587735	40.544423
3355.334089	582507.463149	40.549440
3358.849035	583400.494520	40.554458
3362.484831	584278.984877	40.559476
3365.841235	585158.848350	40.564493
3369.165436	586052.793342	40.569511
3372.601111	586937.900014	40.574528
3376.081161	587830.075172	40.579546
3379.406839	588725.799500	40.584564
3383.153944	589611.289033	40.589581
3386.308099	590495.399426	40.594599
3389.839071	591378.478893	40.599616
3393.010564	592289.920103	40.604634
3396.540485	593178.846784	40.609652
3400.301691	594063.816890	40.614669
3403.557075	594969.671225	40.619687
3407.117081	595864.962222	40.624704
3410.373828	596763.121509	40.629722
3413.586105	597664.207576	40.634740
3417.289984	598564.490625	40.639757
3421.089885	599461.685872	40.644775
3424.361799	600358.737091	40.649792
3427.853714	601256.176149	40.654810
3430.773937	602156.422582	40.659828
3434.768064	603062.512313	40.664845
3438.122860	603963.981567	40.669863
3441.442902	604857.642933	40.674880
3445.344931	605767.402531	40.679898
3448.609468	606659.219860	40.684916
3452.388234	607549.532348	40.689933
3455.193976	608458.526444	40.694951
3459.081139	609347.268739	40.699968
3462.644502	610246.757273	40.704986
3465.834198	611144.429253	40.710004
3469.507505	612031.424254	40.715021
3472.904590	612919.461970	40.720026
3476.374158	613758.016883	40.725031
3479.557589	614552.962528	40.730036
3482.718390	615298.170578	40.735040
3485.837949	615988.107705	40.740045
3488.125080	616617.911762	40.745050
3491.305607	617196.568483	40.750055
3493.986792	617731.249687	40.755060
3496.618608	618206.803073	40.760064
3498.909686	618616.937519	40.765069
3501.593092	618988.574747	40.770074
3503.418570	619312.522396	40.775079
3505.327656	619579.246098	40.780084
3507.150598	619805.362269	40.785088
3509.030318	619983.408104	40.790093
3510.774286	620142.389586	40.795098
3512.049037	620238.001250	40.800103
3513.415455	620309.120699	40.805108
3514.547313	620348.456398	40.810112
3516.182774	620340.557813	40.815117
3517.098506	620327.826395	40.820122
3517.849475	620256.275908	40.825127
3518.593324	620174.535467	40.830132
3519.289352	620072.370572	40.835136
3519.979886	619938.434218	40.840141
3520.339013	619809.293641	40.845146
3520.890569	619645.251811	40.850151
3521.813225	619476.453278	40.855156
3521.993286	619278.692320	40.860160
3522.693232	619076.199941	40.865165
3523.211070	618858.294172	40.870170
3523.629902	618625.460623	40.875175
3523.824504	618379.416557	40.880180
3523.545986	618118.750945	40.885184
3523.760565	617851.955610	40.890189
3523.654806	617588.750845	40.895194
3524.111554	617319.355093	40.900199
3524.439571	617036.880199	40.905204
3524.408415	616754.503434	40.910208
3524.313607	616465.032568	40.915213
3524.206135	616176.454830	40.920218
3524.453913	615878.168012	40.925223
3524.443998	615582.111573	40.930228
3524.231345	615280.480520	40.935232
3524.006054	614968.346620	40.940237
3524.215686	614668.680336	40.945242
3523.947277	614356.384214	40.950247
3523.657267	614054.128628	40.955252
3523.525135	613752.039226	40.960256
3523.627916	613444.405434	40.965261
3522.952569	613140.483098	40.970266
3523.004376	612844.036465	40.975271
3523.118065	612539.022856	40.980276
3523.203649	612239.603694	40.985280
3523.167987	611927.845898	40.990285
3522.595053	611625.061852	40.995290
3522.557456	611313.685428	41.000295
3522.322559	611019.030088	41.005300
3522.017245	610715.977063	41.010304
3521.556072	610414.839450	41.015309
3521.413794	610126.944070	41.020314
3521.328381	609833.531087	41.025319
3521.087969	609550.785287	41.030324
3520.984634	609267.910200	41.035328
3520.590578	608983.522426	41.040333
3520.444182	608704.739226	41.045338
3520.367422	608427.187835	41.050343
3520.190360	608150.394792	41.055348
3519.564534	607881.866838	41.060352
3519.769028	607601.198178	41.065357
3519.431945	607339.012915	41.070362
3518.801975	607066.562883	41.075367
3518.976444	606811.036683	41.080372
3518.507733	606559.906498	41.085376
3518.798136	606295.045403	41.090381
3518.214598	606048.422697	41.095386
3517.817490	605797.212672	41.100391
3517.925457	605542.915997	41.105396
3517.546519	605300.745753	41.110400
3517.576343	605063.108541	41.115405
3517.418871	604816.089571	41.120410
3516.953165	604576.417380	41.125415
3517.127135	604339.341358	41.130420
3516.535628	604113.036615	41.135424
3516.250919	603869.166995	41.140429
3515.905673	603653.871275	41.145434
3515.746989	603434.589048	41.150439
3515.470917	603220.574460	41.155444
3515.470584	603003.109741	41.160448
3515.521654	602780.578448	41.165453
3514.581891	602577.112594	41.170458
3514.950224	602362.329059	41.175463
3514.615100	602166.066694	41.180468
3514.343232	601966.337745	41.185472
3514.194358	601759.729660	41.190477
3514.143027	601569.216830	41.195482
3513.981061	601372.211804	41.200487
3513.718555	601185.178162	41.205492
3514.017384	600989.845535	41.210496
3513.472882	600810.056178	41.215501
3513.490917	600625.671303	41.220506
3512.832054	600434.632147	41.225511
3512.916684	600254.935093	41.230516
3512.526644	600077.761729	41.235520
3512.915680	599890.502967	41.240525
3512.372084	599720.254919	41.245530
3512.002529	599558.836621	41.250535
3512.555200	599385.508576	41.255540
3512.147134	599219.085495	41.260544
3511.996618	599052.419283	41.265549
3511.504268	598884.402236	41.270554
3511.108105	598729.082427	41.275559
3511.495483	598572.186105	41.280564
3510.981817	598424.989828	41.285568
3511.262627	598268.305877	41.290573
3510.947482	598119.372214	41.295578
3510.799853	597973.113631	41.300583
3510.839988	597823.068927	41.305588
3510.647497	597687.126399	41.310592
3510.402354	597534.318607	41.315597
3510.184214	597395.572714	41.320602
3510.132284	597251.642228	41.325607
3509.991891	597112.730266	41.330612
3510.268454	596988.971718	41.335616
3510.084811	596845.807300	41.340621
3510.024562	596705.425488	41.345626
3509.519001	596578.680158	41.350631
3509.797570	596450.909473	41.355636
3509.205032	596328.831225	41.360640
3509.507769	596204.208212	41.365645
3508.963951	596071.954996	41.370650
3509.243351	595946.881961	41.375655
3508.930361	595826.807178	41.380660
3508.814646	595714.461539	41.385664
3508.989214	595588.749718	41.390669
3508.550893	595470.643371	41.395674
3508.506157	595356.830693	41.400679
3508.411453	595243.475286	41.405684
3508.283238	595136.934230	41.410688
3508.229026	595018.512426	41.415693
3508.182875	594926.728976	41.420698
3508.214556	594804.936213	41.425703
3508.050591	594702.703054	41.430708
3507.881129	594600.119223	41.435712
3507.693342	594497.537267	41.440717
3507.517719	594396.805358	41.445722
3507.621590	594302.539181	41.450727
3507.707228	594199.360730	41.455732
3507.356581	594100.506350	41.460736
3507.534610	593998.413287	41.465741
3507.461416	593915.339479	41.470746
3507.167524	593814.670635	41.475751
3507.505525	593719.861885	41.480756
3507.230680	593631.708969	41.485760
3506.957744	593537.995768	41.490765
3507.029993	593447.633483	41.495770
3506.517159	593348.547066	41.500775
3506.792384	593262.358563	41.505780
3506.294012	593180.597619	41.510784
3506.564624	593094.909339	41.515789
3506.653410	593019.466313	41.520794
3506.385883	592939.370353	41.525799
3506.341803	592856.534186	41.530804
3506.150760	592782.285224	41.535808
3506.559060	592689.109210	41.540813
3506.167262	592615.842137	41.545818
3506.303818	592542.592141	41.550823
3506.402703	592451.315688	41.555828
3506.327341	592387.414216	41.560832
3506.188110	592308.144984	41.565837
3506.097210	592235.178889	41.570842
3506.468869	592148.966348	41.575847
3506.279026	592074.061117	41.580852
3505.751970	591994.699922	41.585856
3505.906467	591921.342695	41.590861
3506.159143	591852.327562	41.595866
3505.672122	591766.196088	41.600871
3505.899066	591702.393549	41.605876
3505.799344	591640.094376	41.610880
3505.900235	591561.383192	41.615885
3505.901192	591483.588728	41.620890
3505.510984	591415.873523	41.625895
3505.982640	591346.069504	41.630900
3505.675979	591280.544506	41.635904
3505.961499	591208.664747	41.640909
3505.795459	591134.149989	41.645914
3505.439165	591064.924429	41.650919
3505.656917	590998.564306	41.655924
3505.060912	590936.689302	41.660928
3505.289007	590872.330606	41.665933
3505.190055	590801.510147	41.670938
3505.414651	590740.657945	41.675943
3505.276371	590673.449738	41.680948
3504.957428	590621.148185	41.685952
3505.286214	590552.613783	41.690957
3505.062801	590495.988314	41.695962
3505.082096	590435.617361	41.700967
3505.230695	590381.037244	41.705972
3505.073289	590315.432933	41.710976
3505.385468	590253.061332	41.715981
3505.021319	590191.696881	41.720986
3505.140683	590137.120099	41.725991
3505.007751	590076.670735	41.730996
3504.787185	590013.479239	41.736000
3505.132920	589947.693835	41.741005
3505.263030	589898.675285	41.746010
3504.722282	589831.875448	41.751015
3504.784544	589779.810821	41.756020
3505.002969	589719.955843	41.761024
3505.239136	589654.285984	41.766029
3504.688002	589588.187682	41.771034
3504.393469	589537.680719	41.776039
3504.566983	589490.858024	41.781044
3504.470339	589442.474078	41.786048
3504.723103	589390.728512	41.791053
3504.664952	589343.891293	41.796058
3504.708432	589290.123741	41.801063
3504.507636	589229.279414	41.806068
3504.334484	589181.206879	41.811072
3504.067648	589132.898257	41.816077
3504.463632	589079.174757	41.821082
3504.330876	589045.425096	41.826087
3504.594783	588979.245756	41.831092
3504.183981	588937.021427	41.836096
3504.478723	588884.214675	41.841101
3504.635433	588837.842726	41.846106
3504.497299	588790.414349	41.851111
3504.634887	588733.422565	41.856116
3504.249110	588699.611166	41.861120
3504.363180	588639.916844	41.866125
3504.089316	588585.594125	41.871130
3504.127982	588538.838498	41.876135
3504.330163	588500.124318	41.881140
3503.996405	588463.498064	41.886144
3503.880183	588413.258614	41.891149
3504.110987	588374.890263	41.896154
3503.856406	588327.377847	41.901159
3503.931255	588273.700558	41.906164
3503.838477	588241.144728	41.911168
3504.020549	588192.912056	41.916173
3504.226785	588158.304902	41.921178
3504.268373	588104.832411	41.926183
3503.966310	588061.535383	41.931188
3503.882718	588024.567882	41.936192
3504.270219	587984.319619	41.941197
3504.144981	587946.005411	41.946202
3503.790580	587893.946740	41.951207
3504.167862	587847.085086	41.956212
3503.886123	587807.642327	41.961216
3504.269480	587764.337182	41.966221
3503.856653	587715.694287	41.971226
3503.708098	587684.749043	41.976231
3503.866931	587627.146797	41.981236
3503.601697	587598.324205	41.986240
3503.770622	587553.698744	41.991245
3503.886929	587517.449935	41.996250
3503.600952	587473.396373	42.001255
3504.169139	587439.131238	42.006260
3503.687072	587401.572456	42.011264
3503.973003	587358.531486	42.016269
3503.573403	587320.959533	42.021274
3503.568390	587278.665301	42.026279
3503.593684	587235.965266	42.031284
3503.649252	587211.250850	42.036288
3503.861605	587168.771873	42.041293
3503.855583	587136.349507	42.046298
3503.640322	587094.839126	42.051303
3503.816423	587047.203664	42.056308
3503.754718	587017.946805	42.061312
3503.954421	586969.355152	42.066317
3503.812718	586940.411274	42.071322
3503.888025	586898.904836	42.076327
3503.801653	586848.302680	42.081332
3504.092217	586812.575542	42.086336
3503.921453	586774.565009	42.091341
3503.831388	586734.837816	42.096346
3503.780107	586695.204646	42.101351
3503.618458	586646.818390	42.106356
3503.724935	586618.887284	42.111360
3503.949454	586572.144256	42.116365
3503.916096	586528.949459	42.121370
3503.954022	586490.654731	42.126375
3504.103747	586452.141925	42.131380
3503.582918	586407.469246	42.136384
3503.988240	586369.968641	42.141389
3504.068353	586326.705188	42.146394
3503.621824	586277.409605	42.151399
3503.491916	586243.199730	42.156404
3503.569727	586217.627590	42.161408
3503.560600	586176.582657	42.166413
3503.634178	586134.171461	42.171418
3503.868130	586099.102369	42.176423
3503.850327	586062.318387	42.181428
3503.585269	586024.420213	42.186432
3503.817328	585979.177016	42.191437
3504.025103	585933.636715	42.196442
3503.994114	585910.135729	42.201447
3504.009437	585853.348442	42.206452
3503.462474	585820.806250	42.211456
3504.018457	585776.914915	42.216461
3503.512314	585743.012886	42.221466
3503.382334	585698.476677	42.226471
3503.662341	585662.045749	42.231476
3503.472851	585635.311153	42.236480
3503.769343	585597.323710	42.241485
3503.677102	585566.313521	42.246490
3503.317152	585527.977374	42.251495
3503.584667	585477.263414	42.256500
3503.156335	585455.277068	42.261504
3503.219448	585415.471004	42.266509
3502.806572	585389.622786	42.271514
3503.305920	585359.521952	42.276519
3503.436792	585328.175480	42.281524
3503.331096	585298.770523	42.286528
3503.370828	585256.862429	42.291533
3503.115755	585229.535630	42.296538
3503.050578	585203.732861	42.301543
3503.255001	585167.512591	42.306548
3502.833039	585145.875481	42.311552
3502.923719	585114.634926	42.316557
3503.285022	585077.036526	42.321562
3503.500662	585051.540356	42.326567
3503.265429	585022.054659	42.331572
3503.366480	584991.012622	42.336576
3503.209709	584957.304149	42.341581
3503.352720	584917.383538	42.346586
3503.309510	584891.275857	42.351591
3503.066709	584857.730898	42.356596
3502.926236	584836.801025	42.361600
3503.217844	584802.470621	42.366605
3503.353712	584776.835912	42.371610
3503.264666	584740.309240	42.376615
3503.402008	584709.110358	42.381620
3503.082512	584690.213164	42.386624
3503.148050	584653.411414	42.391629
3503.019656	584623.156071	42.396634
3503.020609	584589.872934	42.401639
3503.148277	584558.825511	42.406644
3502.909129	584534.552111	42.411648
3502.857895	584507.041266	42.416653
3503.078860	584476.129400	42.421658
3503.174218	584458.219585	42.426663
3503.253819	584425.575284	42.431668
3502.850801	584401.828464	42.436672
3502.626598	584373.843067	42.441677
3502.859295	584347.390204	42.446682
3502.530947	584320.022463	42.451687
3503.217868	584288.235208	42.456692
3503.178615	584279.519242	42.461696
3503.005000	584247.214754	42.466701
3503.280160	584219.602037	42.471706
3503.186127	584193.049500	42.476711
3502.925763	584154.492464	42.481716
3502.829463	584127.238346	42.486720
3502.666290	584096.736352	42.491725
3502.727051	584070.359828	42.496730
3502.996447	584058.637929	42.501735
3503.305477	584036.583585	42.506740
3502.902225	583997.597188	42.511744
3502.865750	583961.510851	42.516749
3503.584662	583943.402462	42.521754
3502.822419	583912.993609	42.526759
3502.997718	583892.263209	42.531764
3502.852451	583865.216607	42.536768
3502.948413	583835.625813	42.541773
3503.355374	583810.548009	42.546778
3502.573779	583782.197082	42.551783
3502.699943	583754.155332	42.556788
3503.003267	583744.382814	42.561792
3503.210170	583713.671516	42.566797
3503.323656	583685.681703	42.571802
3503.087575	583662.258085	42.576807
3503.224174	583624.689842	42.581812
3502.910617	583595.663714	42.586816
3502.802105	583562.294314	42.591821
3503.221208	583546.086936	42.596826
3503.143967	583519.981313	42.601831
3503.149393	583474.261911	42.606836
3502.854749	583449.292965	42.611840
3502.821331	583426.288332	42.616845
3503.272896	583396.640767	42.621850
3502.947779	583368.919234	42.626855
3503.334618	583339.582417	42.631860
3502.968187	583312.468767	42.636864
3503.262215	583282.895654	42.641869
3503.094964	583243.969949	42.646874
3502.706714	583227.336874	42.651879
3502.896722	583198.130712	42.656884
3502.806032	583180.598819	42.661888
3503.430389	583143.052945	42.666893
3503.473648	583116.777133	42.671898
3502.964737	583099.761674	42.676903
3502.886150	583059.768692	42.681908
3502.969912	583033.636745	42.686912
3502.973469	582992.527774	42.691917
3503.223370	582975.293234	42.696922
3502.746506	582950.903096	42.701927
3502.969173	582922.693746	42.706932
3502.674891	582897.873887	42.711936
3502.857720	582882.153665	42.716941
3502.777249	582847.674797	42.721946
3502.687622	582828.888857	42.726951
3502.869591	582799.181566	42.731956
3502.596289	582779.521861	42.736960
3502.451505	582749.765251	42.741965
3502.979928	582732.185992	42.746970
3502.602581	582712.943500	42.751975
3503.177720	582684.828841	42.756980
3502.768666	582658.321843	42.761984
3502.535952	582639.507815	42.766989
3502.433267	582618.918744	42.771994
3502.221280	582592.681584	42.776999
3502.742306	582576.807790	42.782004
3502.386364	582553.149875	42.787009
3502.349033	582548.442967	42.792013
3502.705529	582514.345953	42.797018
3502.460800	582503.855865	42.802023
3502.714957	582471.128344	42.807028
3502.787488	582467.457051	42.812033
3502.955985	582427.172474	42.817037
3502.553508	582407.582433	42.822042
3502.787034	582383.832005	42.827047
3502.854939	582358.001746	42.832052
3502.972084	582346.251696	42.837057
3502.730362	582316.659477	42.842061
3502.798568	582294.589163	42.847066
3502.537859	582265.450992	42.852071
3503.069046	582249.324463	42.857076
3502.766315	582223.952915	42.862081
3502.739026	582193.925760	42.867085
3502.824575	582175.562543	42.872090
3502.729784	582154.018788	42.877095
3502.864320	582124.066417	42.882100
3502.596440	582104.906020	42.887105
3502.978505	582079.878314	42.892109
3502.769698	582053.388692	42.897114
3502.622525	582040.626773	42.902119
3503.096727	582006.710339	42.907124
3502.885504	581984.181721	42.912129
3502.885915	581963.324626	42.917133
3502.932359	581926.316195	42.922138
3502.298063	581910.521783	42.927143
3502.590562	581884.003524	42.932148
3502.516940	581866.366597	42.937153
3502.549303	581840.941784	42.942157
3502.794270	581831.828486	42.947162
3502.521204	581803.844188	42.952167
3502.539921	581776.917234	42.957172
3502.224603	581754.905798	42.962177
3502.550499	581737.507036	42.967181
3502.994567	581714.123360	42.972186
3502.529954	581705.371575	42.977191
3502.967993	581675.721509	42.982196
3502.496489	581657.193825	42.987201
3502.913324	581631.558011	42.992205
3502.430149	581613.683876	42.997210
3502.154468	581598.785584	43.002215
3502.418917	581576.883713	43.007220
3502.363390	581557.087505	43.012225
3502.110376	581531.756731	43.017229
3502.544104	581528.179079	43.022234
3502.478737	581505.375989	43.027239
3502.340931	581477.369719	43.032244
3502.162830	581464.511690	43.037249
3502.426914	581452.938278	43.042253
3502.444352	581424.205656	43.047258
3502.422613	581420.598893	43.052263
3502.754898	581396.530072	43.057268
3502.127413	581374.967794	43.062273
3502.404978	581357.375434	43.067277
3502.602159	581331.271869	43.072282
3502.184093	581319.303559	43.077287
3502.465880	581294.139336	43.082292
3502.678635	581289.242375	43.087297
3502.221991	581270.661578	43.092301
3502.310836	581246.580348	43.097306
3502.298054	581240.765963	43.102311
3502.444798	581214.319026	43.107316
3502.632025	581199.397970	43.112321
3502.546057	581179.405284	43.117325
3502.415473	581158.767711	43.122330
3502.486945	581137.145841	43.127335
3502.557324	581118.582681	43.132340
3502.575696	581103.687892	43.137345
3502.646737	581084.673305	43.142349
3502.680545	581059.848161	43.147354
3502.841739	581046.385054	43.152359
3502.838038	581016.300873	43.157364
3502.873322	580998.996526	43.162369
3502.212992	580962.847480	43.167373
3502.534571	580955.827425	43.172378
3502.915919	580928.741435	43.177383
3503.141266	580905.640956	43.182388
3502.500501	580885.333337	43.187393
3502.598970	580856.837285	43.192397
3502.470463	580838.154320	43.197402
3502.457736	580821.759757	43.202407
3502.481720	580801.749201	43.207412
3502.432102	580782.351821	43.212417
3502.438603	580764.149048	43.217421
3502.443510	580745.645640	43.222426
3502.935648	580726.464325	43.227431
3502.453092	580702.120242	43.232436
3502.385695	580687.739727	43.237441
3502.885797	580669.208922	43.242445
3502.502771	580636.024018	43.247450
3502.607896	580621.265448	43.252455
3502.886428	580587.776408	43.257460
3502.505850	580566.274237	43.262465
3502.345543	580551.857928	43.267469
3502.642888	580535.715328	43.272474
3502.336480	580515.956480	43.277479
3502.639752	580497.556445	43.282484
3502.675441	580468.968925	43.287489
3502.343466	580457.587945	43.292493
3502.389366	580424.285210	43.297498
3502.480549	580419.958455	43.302503
3502.679305	580383.723361	43.307508
3502.834186	580385.504198	43.312513
3502.812146	580351.961148	43.317517
3502.830653	580328.941948	43.322522
3502.180653	580304.422589	43.327527
3502.303160	580288.056240	43.332532
3502.373203	580264.928562	43.337537
3502.220489	580254.522239	43.342541
3502.613302	580228.937090	43.347546
3502.380146	580222.354307	43.352551
3502.238786	580199.710844	43.357556
3502.041422	580174.769423	43.362561
3502.228605	580166.917418	43.367565
3502.641688	580145.290358	43.372570
3502.450423	580132.583275	43.377575
3502.652967	580114.950532	43.382580
3502.314432	580100.110191	43.387585
3502.857670	580076.456840	43.392589
3502.757369	580051.098806	43.397594
3502.292076	580032.366842	43.402599
3502.328574	580013.506257	43.407604
3502.481352	580000.293928	43.412609
3502.332846	579983.217312	43.417613
3502.780650	579956.720316	43.422618
3502.454112	579940.574093	43.427623
3502.578023	579925.761516	43.432628
3502.394296	579897.106533	43.437633
3502.344533	579889.341520	43.442637
3502.657345	579870.186765	43.447642
3502.410056	579849.113682	43.452647
3502.730646	579825.745338	43.457652
3502.584387	579803.302418	43.462657
3502.769342	579780.707382	43.467661
3502.776286	579765.110530	43.472666
3502.438383	579738.535257	43.477671
3502.553012	579717.856669	43.482676
3502.547087	579703.565564	43.487681
3502.271101	579682.296062	43.492685
3502.302288	579663.586155	43.497690
3502.252235	579652.912483	43.502695
3502.178781	579629.705623	43.507700
3502.171586	579618.824628	43.512705
3502.269349	579589.121897	43.517709
3502.485002	579577.554107	43.522714
3502.377832	579565.936476	43.527719
3502.515660	579540.740641	43.532724
3502.271145	579526.336164	43.537729
3502.594152	579507.730819	43.542733
3502.326583	579490.571763	43.547738
3502.262733	579474.333647	43.552743
3502.356182	579453.256693	43.557748
3502.363231	579435.703585	43.562753
3502.252264	579435.169168	43.567757
3502.647028	579407.425453	43.572762
3502.378019	579387.909490	43.577767
3502.532052	579372.188796	43.582772
3502.153377	579361.716663	43.587777
3502.460677	579334.387628	43.592781
3502.570577	579310.950845	43.597786
3502.561301	579308.595167	43.602791
3502.453243	579280.428253	43.607796
3502.420558	579264.686449	43.612801
3502.407250	579246.835331	43.617805
3502.287131	579229.702970	43.622810
3501.864319	579213.269843	43.627815
3502.352153	579190.475814	43.632820
3502.138436	579182.535341	43.637825
3502.027465	579161.941138	43.642829
3502.411496	579142.573402	43.647834
3502.008935	579137.119747	43.652839
3502.755053	579119.550902	43.657844
3502.695215	579099.650685	43.662849
3502.472000	579087.148000	43.667853
3502.339529	579065.052484	43.672858
3502.298082	579048.509345	43.677863
3502.417801	579026.374328	43.682868
3502.314743	579015.256980	43.687873
3502.478119	578993.064922	43.692877
3502.398653	578962.686124	43.697882
3502.346343	578956.525670	43.702887
3502.157301	578925.411644	43.707892
3502.520855	578921.693686	43.712897
3502.039361	578910.936297	43.717901
3502.247236	578890.492350	43.722906
3502.081053	578882.594382	43.727911
3502.171349	578852.991158	43.732916
3502.173418	578850.633610	43.737921
3502.164956	578838.799185	43.742925
3502.474066	578814.828708	43.747930
3502.036314	578813.442627	43.752935
3502.359562	578793.481977	43.757940
3502.434210	578768.996391	43.762945
3502.190589	578756.295918	43.767949
3502.510492	578724.700560	43.772954
3502.604493	578728.697846	43.777959
3502.442518	578705.402595	43.782964
3502.387762	578678.830677	43.787969
3502.251534	578675.591982	43.792973
3502.252641	578648.108527	43.797978
3502.127135	578648.729835	43.802983
3501.918125	578617.417464	43.807988
3502.017889	578594.181367	43.812993
3502.408965	578599.987884	43.817997
3502.261124	578565.004706	43.823002
3501.913328	578559.090834	43.828007
3502.012029	578545.835084	43.833012
3502.514883	578536.628627	43.838017
3502.476727	578507.395634	43.843021
3502.577971	578494.289883	43.848026
3502.344219	578478.427943	43.853031
3502.538278	578455.076511	43.858036
3502.607692	578426.227710	43.863041
3502.620117	578424.971815	43.868045
3502.718512	578400.983238	43.873050
3502.640992	578392.017850	43.878055
3502.312220	578364.635421	43.883060
3502.460977	578345.503698	43.888065
3502.251324	578325.073836	43.893069
3502.845599	578309.282824	43.898074
3502.224851	578288.215013	43.903079
3502.447872	578272.381681	43.908084
3502.761361	578256.233262	43.913089
3502.468056	578232.957555	43.918093
3502.759253	578209.038733	43.923098
3502.228827	578190.564613	43.928103
3502.159126	578172.068591	43.933108
3502.288972	578148.877020	43.938113
3501.973740	578142.406140	43.943117
3502.439021	578124.578718	43.948122
3501.945698	578105.195881	43.953127
3502.030056	578094.449549	43.958132
3502.045911	578092.440766	43.963137
3501.897277	578073.003988	43.968141
3502.259838	578059.054406	43.973146
3502.116524	578053.409224	43.978151
3502.486655	578026.067168	43.983156
3502.271610	578016.420813	43.988161
3501.912712	577996.063834	43.993165
3502.322316	577975.285750	43.998170
3502.269925	577975.394116	44.003175
3502.253410	577946.507356	44.008180
3502.358450	577935.406554	44.013185
3502.581868	577911.798624	44.018189
3502.073040	577883.289593	44.023194
3501.902604	577884.770605	44.028199
3502.321428	577882.197236	44.033204
3502.201929	577849.865615	44.038209
3501.979521	577851.455066	44.043213
3502.464191	577823.643213	44.048218
3502.061697	577817.185784	44.053223
3502.356945	577806.105275	44.058228
3502.505467	577786.571390	44.063233
3502.431865	577759.298052	44.068237
3502.352955	577752.238287	44.073242
3502.070935	577732.570990	44.078247
3502.349653	577721.392669	44.083252
3502.242815	577703.001989	44.088257
3501.855859	577686.410533	44.093261
3502.219899	577678.228197	44.098266
3502.089229	577663.001013	44.103271
3501.909833	577642.264233	44.108276
3502.389606	577639.079406	44.113281
3501.972669	577626.605365	44.118285
3502.086111	577598.700519	44.123290
3501.800980	577598.343707	44.128295
3501.884123	577597.879167	44.133300
3501.908630	577587.292175	44.138305
3501.778137	577567.350117	44.143309
3502.151519	577561.423284	44.148314
3501.803343	577562.380400	44.153319
3502.020928	577538.220872	44.158324
3502.092654	577516.090368	44.163329
3502.367901	577519.708656	44.168333
3502.148334	577492.056230	44.173338
3501.762716	577486.749582	44.178343
3502.086269	577477.520133	44.183348
3501.968579	577461.638604	44.188353
3501.974791	577449.248685	44.193357
3502.159913	577438.536130	44.198362
3502.122503	577435.733040	44.203367
3502.206406	577410.189731	44.208372
3502.475149	577395.401317	44.213377
3502.027620	577387.395799	44.218381
3502.250015	577355.360403	44.223386
3502.062574	577353.333110	44.228391
3502.108391	577336.773794	44.233396
3502.203969	577313.184589	44.238401
3502.357720	577308.495745	44.243405
3502.252878	577302.693695	44.248410
3502.269594	577271.041316	44.253415
3502.170073	577257.213134	44.258420
3502.290585	577245.707966	44.263425
3502.187505	577221.547727	44.268429
3502.363022	577212.591994	44.273434
3501.916602	577200.623667	44.278439
3502.234809	577182.015209	44.283444
3502.275830	577185.519748	44.288449
3501.842887	577160.558251	44.293453
3501.817932	577140.699251	44.298458
3501.795156	577138.295067	44.303463
3501.969429	577128.336290	44.308468
3502.407724	577109.508305	44.313473
3501.967076	577097.338330	44.318477
3502.237013	577088.016627	44.323482
3502.322875	577074.259555	44.328487
3502.364300	577050.778581	44.333492
3502.476997	577051.412896	44.338497
3502.260611	577027.871859	44.343501
3502.109033	577017.813447	44.348506
3502.035807	577002.877339	44.353511
3501.975753	576972.941531	44.358516
3501.927470	576975.306433	44.363521
3502.084596	576971.720426	44.368525
3501.961597	576938.534011	44.373530
3501.712611	576936.566423	44.378535
3501.984067	576918.968027	44.383540
3502.015460	576915.552137	44.388545
3501.971843	576904.222756	44.393549
3501.977154	576880.546433	44.398554
3502.330646	576881.243434	44.403559
3502.083019	576870.447509	44.408564
3502.377892	576851.390714	44.413569
3501.815979	576841.797569	44.418573
3502.245734	576819.108122	44.423578
3502.015819	576821.752249	44.428583
3501.989414	576807.410481	44.433588
3502.247611	576788.409473	44.438593
3501.953305	576771.501213	44.443597
3502.249947	576756.757758	44.448602
3502.070210	576750.666168	44.453607
3502.080250	576734.111556	44.458612
3502.038448	576724.386842	44.463617
3501.935194	576729.368729	44.468621
3501.873410	576698.529573	44.473626
3501.999142	576687.925908	44.478631
3501.894170	576675.402034	44.483636
3501.801717	576662.274260	44.488641
3501.938021	576651.468265	44.493645
3501.877268	576634.272483	44.498650
3502.314963	576632.347975	44.503655
3501.864192	576612.504446	44.508660
3502.237710	576602.815022	44.513665
3502.014412	576589.607297	44.518669
3501.622716	576591.223388	44.523674
3501.620174	576571.911648	44.528679
3501.918962	576556.365017	44.533684
3502.033722	576546.766157	44.538689
3501.686790	576548.726384	44.543693
3501.652300	576540.956654	44.548698
3501.903720	576532.891417	44.553703
3501.824181	576515.748552	44.558708
3502.040842	576504.779370	44.563713
3501.633779	576509.206912	44.568717
3501.824829	576491.871225	44.573722
3501.967142	576476.900722	44.578727
3501.845541	576460.115478	44.583732
3502.073936	576460.581255	44.588737
3502.024848	576448.850978	44.593741
3502.135279	576440.055290	44.598746
3502.193007	576425.850367	44.603751
3502.590684	576416.708786	44.608756
3502.117319	576398.423425	44.613761
3501.978523	576399.448226	44.618765
3501.932696	576381.196324	44.623770
3501.828544	576353.071587	44.628775
3502.182598	576344.789522	44.633780
3502.345795	576329.063126	44.638785
3501.792939	576325.788554	44.643789
3501.944788	576298.727228	44.648794
3502.002800	576293.551306	44.653799
3502.292621	576292.452457	44.658804
3502.331845	576267.264669	44.663809
3502.171230	576261.320311	44.668813
3502.111762	576239.809750	44.673818
3502.169675	576230.470320	44.678823
3502.173766	576223.195965	44.683828
3502.150308	576195.108381	44.688833
3501.958039	576181.794999	44.693837
3501.932938	576169.207911	44.698842
3502.064391	576171.595046	44.703847
3501.846407	576140.778777	44.708852
3501.885663	576138.214192	44.713857
3501.885612	576132.244665	44.718861
3502.104554	576129.802477	44.723866
3502.019489	576105.386203	44.728871
3501.591595	576101.740886	44.733876
3501.908226	576097.628034	44.738881
3501.930342	576086.588532	44.743885
3501.881085	576064.724897	44.748890
3502.049399	576063.193551	44.753895
3502.184832	576048.022900	44.758900
3502.192402	576048.623544	44.763905
3502.111681	576022.500853	44.768909
3502.216260	576011.448386	44.773914
3501.956403	575997.192243	44.778919
3501.719757	575979.270500	44.783924
3501.975515	575971.254347	44.788929
3501.879700	575964.848228	44.793933
3501.949363	575961.676884	44.798938
3501.879549	575944.280807	44.803943
3502.018691	575934.777942	44.808948
3502.206942	575923.912964	44.813953
3501.740916	575903.167612	44.818957
3501.888110	575881.925044	44.823962
3501.878534	575884.534944	44.828967
3501.894580	575881.271631	44.833972
3502.097881	575869.099979	44.838977
3502.112255	575849.985011	44.843981
3502.028623	575842.774289	44.848986
3501.779114	575848.832880	44.853991
3501.841102	575823.490047	44.858996
3501.470472	575813.514963	44.864001
3501.604352	575812.791597	44.869005
3502.270421	575795.631403	44.874010
3501.846119	575787.420445	44.879015
3501.979721	575771.547404	44.884020
3502.053553	575758.292249	44.889025
3502.065959	575755.330458	44.894029
3502.206913	575740.459518	44.899034
3502.446157	575731.442481	44.904039
3501.905409	575723.149350	44.909044
3502.157817	575718.344093	44.914049
3502.093374	575697.184427	44.919053
3502.429596	575687.048564	44.924058
3502.063541	575664.431035	44.929063
3502.033767	575647.228900	44.934068
3502.126134	575638.786568	44.939073
3501.855253	575634.364072	44.944077
3502.078160	575610.901885	44.949082
3502.060315	575606.489987	44.954087
3502.208258	575601.199358	44.959092
3501.920134	575577.164839	44.964097
3501.795267	575568.656082	44.969101
3502.018509	575554.123192	44.974106
3501.834548	575555.606620	44.979111
3502.133585	575528.219440	44.984116
3502.164141	575521.241489	44.989121
3501.797857	575520.897290	44.994125
3501.947714	575501.309059	44.999130
3501.918157	575478.437888	45.004135
3501.863261	575470.469944	45.009140
3502.058882	575471.041222	45.014145
3501.763490	575451.071014	45.019149
3501.988718	575435.183176	45.024154
3501.782897	575430.650096	45.029159
3501.795864	575427.437300	45.034164
3502.171332	575424.318331	45.039169
3502.430598	575406.669315	45.044173
3502.298265	575393.897458	45.049178
3502.172476	575381.124564	45.054183
3502.442670	575365.179431	45.059188
3502.285219	575339.819649	45.064193
3502.023327	575322.653305	45.069197
3502.281193	575306.057850	45.074202
3502.464673	575306.480534	45.079207
3502.176945	575279.033977	45.084212
3502.279491	575256.342372	45.089217
3502.344978	575244.944096	45.094221
3502.028676	575234.508500	45.099226
3502.143614	575235.895076	45.104231
3502.028810	575218.605245	45.109236
3502.090478	575192.157366	45.114241
3502.092047	575186.437921	45.119245
3502.262614	575177.782349	45.124250
3502.095232	575159.196297	45.129255
3501.922718	575147.383622	45.134260
3502.106903	575128.943230	45.139265
3502.118479	575111.934484	45.144269
3501.853226	575101.490784	45.149274
3501.828864	575108.367424	45.154279
3501.648222	575092.743224	45.159284
3501.942929	575079.252072	45.164289
3502.093018	575077.522772	45.169293
3502.301098	575068.008400	45.174298
3501.969193	575044.280594	45.179303
3501.838133	575035.070052	45.184308
3502.264876	575022.762222	45.189313
3501.790329	575012.953174	45.194317
3501.729547	574997.560945	45.199322
3501.693693	574996.011205	45.204327
3502.053780	574983.513080	45.209332
3502.222708	574972.901050	45.214337
3502.005916	574960.643587	45.219341
3501.866890	574943.808636	45.224346
3501.748839	574936.502377	45.229351
3501.913627	574934.168736	45.234356
3502.230888	574915.707192	45.239361
3501.960759	574909.779238	45.244365
3501.897594	574903.517915	45.249370
3501.513209	574891.386914	45.254375
3501.770228	574870.376116	45.259380
3501.924954	574856.756076	45.264385
3502.094400	574859.940251	45.269389
3502.400224	574851.263286	45.274394
3501.904447	574825.453549	45.279399
3501.804935	574825.569309	45.284404
3502.094541	574812.680664	45.289409
3501.581305	574792.994189	45.294413
3501.862576	574778.451230	45.299418
3501.812830	574778.509042	45.304423
3501.441046	574775.205700	45.309428
3502.081848	574757.094671	45.314433
3502.057992	574745.509182	45.319437
3501.825140	574742.685803	45.324442
3501.844786	574724.370811	45.329447
3501.870674	574731.089317	45.334452
3502.134121	574724.275143	45.339457
3502.015420	574709.543776	45.344461
3502.222435	574685.580458	45.349466
3502.237936	574677.299932	45.354471
3502.022412	574670.359924	45.359476
3501.915063	574645.141255	45.364481
3502.021284	574647.382151	45.369485
3502.053524	574623.947721	45.374490
3502.367360	574604.482810	45.379495
3502.042654	574615.219611	45.384500
3502.414764	574576.931850	45.389505
3502.056697	574568.007263	45.394509
3501.930411	574563.210550	45.399514
3501.964611	574542.836017	45.404519
3501.887684	574516.107200	45.409524
3501.841865	574507.434773	45.414529
3501.971732	574514.739197	45.419533
3501.854892	574498.903518	45.424538
3501.803078	574482.154585	45.429543
3501.712761	574471.733123	45.434548
3502.124415	574477.388066	45.439553
3501.925156	574467.585676	45.444557
3501.833704	574445.474644	45.449562
3501.814060	574434.189200	45.454567
3501.737748	574434.150826	45.459572
3501.924166	574435.676838	45.464577
3501.988114	574422.120637	45.469581
3501.943581	574404.768403	45.474586
3501.993192	574407.670416	45.479591
3501.864433	574408.693826	45.484596
3502.109222	574384.222257	45.489601
3501.988350	574370.343691	45.494605
3501.889096	574359.471985	45.499610
3502.152562	574354.363398	45.504615
3502.176901	574342.368593	45.509620
3501.909966	574323.947240	45.514625
3502.246042	574328.058768	45.519629
3502.172370	574300.927566	45.524634
3501.871689	574278.447546	45.529639
3502.123223	574278.006720	45.534644
3502.036420	574256.195619	45.539649
3502.114294	574246.199199	45.544653
3501.854035	574245.838380	45.549658
3502.135782	574234.706307	45.554663
3502.023678	574211.143072	45.559668
3502.107174	574201.246076	45.564673
3502.070401	574202.405639	45.569677
3501.917370	574175.186197	45.574682
3502.085928	574159.205083	45.579687
3501.852084	574154.876556	45.584692
3501.905737	574140.970425	45.589697
3502.045655	574138.640510	45.594701
3502.109262	574106.570531	45.599706
3502.368238	574106.078363	45.604711
3501.641344	574095.756070	45.609716
3502.065458	574066.890808	45.614721
3501.967784	574081.656571	45.619725
3502.211338	574061.398960	45.624730
3501.411057	574039.046737	45.629735
3501.553463	574038.723308	45.634740
3501.907305	574029.988036	45.639745
3502.168509	574026.786207	45.644749
3502.352095	574020.887200	45.649754
3501.872988	573998.384343	45.654759
3501.663026	573995.155817	45.659764
3502.442534	573982.340161	45.664769
3501.918355	573966.216206	45.669773
3501.995058	573948.091728	45.674778
3501.873608	573939.731726	45.679783
3501.765837	573938.042565	45.684788
3502.025719	573906.944793	45.689793
3501.941086	573908.713943	45.694797
3502.147452	573897.392632	45.699802
3501.849510	573876.416573	45.704807
3501.777343	573866.342928	45.709812
3502.046204	573866.150244	45.714817
3502.061406	573869.810371	45.719821
3502.281040	573845.040532	45.724826
3501.807309	573810.043321	45.729831
3502.003964	573746.593121	45.734836
3501.715035	573650.003281	45.739841
3501.276187	573498.996578	45.744845
3501.296680	573290.515226	45.749850
3501.109061	573048.895798	45.754855
3500.544870	572749.826179	45.759860
3499.804990	572415.600347	45.764865
3499.200778	572044.761462	45.769869
3498.566005	571612.892813	45.774874
3498.025727	571152.588297	45.779879
3497.099224	570623.619220	45.784884
3496.628056	570065.243639	45.789889
3495.402307	569478.650301	45.794893
3493.892904	568833.794765	45.799898
3493.139949	568165.442668	45.804903
3491.907405	567459.877516	45.809908
3491.053931	566702.047593	45.814913
3489.728050	565914.468632	45.819917
3488.263475	565087.592549	45.824922
3486.982701	564219.452509	45.829927
3485.358236	563325.037024	45.834932
3484.022745	562372.701222	45.839937
3482.244712	561390.271139	45.844941
3480.765032	560380.888707	45.849946
3479.149037	559332.709294	45.854951
3477.301397	558252.319339	45.859956
3474.689874	557148.586529	45.864961
3473.183545	556004.227972	45.869965
3471.127186	554831.954492	45.874970
3469.133639	553633.572404	45.879975
3466.867550	552411.539544	45.884980
3465.092084	551155.726125	45.889985
3462.418029	549874.785722	45.894989
3460.429767	548564.893305	45.899994
3457.790752	547235.853892	45.904999
3455.790936	545889.019274	45.910004
3453.185267	544495.205213	45.915009
3450.494642	543093.451139	45.920013
3448.243440	541672.152395	45.925018
3445.303296	540215.731019	45.930023
3442.447123	538744.132735	45.935028
3439.673215	537259.014161	45.940033
3437.189809	535759.080584	45.945037
3434.303206	534248.362562	45.950042
3431.923491	532702.599985	45.955047
3428.731191	531153.708356	45.960052
3426.000823	529584.669223	45.965057
3422.832936	527995.063013	45.970061
3419.987288	526390.808775	45.975066
3417.036946	524788.491975	45.980071
3413.483836	523162.145383	45.985076
3410.545489	521522.152277	45.990081
3407.624370	519882.712392	45.995085
3404.250291	518224.043296	46.000090
3401.321276	516547.460504	46.005095
3397.455437	514869.760207	46.010100
3394.314769	513180.751062	46.015105
3390.890976	511497.429502	46.020109
3387.732852	509777.351788	46.025114
3384.567172	508076.885857	46.030119
3380.929776	506361.711053	46.035124
3377.937102	504632.052396	46.040129
3374.480035	502906.192621	46.045133
3370.761656	501166.895634	46.050138
3367.389159	499421.330240	46.055143
3363.929795	497664.818834	46.060148
3360.450663	495904.415447	46.065153
3356.792348	494135.500454	46.070157
3353.316742	492370.133471	46.075162
3350.102790	490598.609518	46.080167
3345.673699	488831.309811	46.085172
3342.101518	487056.498366	46.090177
3338.075823	485295.342381	46.095181
3334.684411	483512.414937	46.100186
3331.425243	481751.089169	46.105191
3327.939044	479978.483528	46.110196
3324.241776	478187.113646	46.115201
3320.672888	476418.973245	46.120205
3317.118984	474629.758318	46.125210
3313.429051	472854.773659	46.130215
3309.482051	471064.163663	46.135220
3306.008496	469281.272652	46.140225
3301.915845	467499.094453	46.145229
3298.744967	465704.745848	46.150234
3294.870991	463921.391858	46.155239
3291.031562	462137.995386	46.160244
3287.673274	460345.077967	46.165249
3283.800781	458559.339044	46.170253
3279.826263	456766.953998	46.175258
3276.002089	454976.486104	46.180263
3272.304890	453194.571378	46.185268
3268.728083	451411.698761	46.190273
3264.813635	449637.660651	46.195277
3261.226937	447846.182446	46.200282
3257.583214	446067.852266	46.205287
3253.386467	444292.625415	46.210292
3250.092637	442508.476831	46.215297
3245.883353	440741.317387	46.220301
3241.929317	438969.240447	46.225306
3238.373455	437194.756566	46.230311
3234.600012	435433.921230	46.235316
3230.846306	433669.526629	46.240321
3226.956338	431899.925446	46.245325
3223.009301	430129.666088	46.250330
3219.261542	428384.455147	46.255335
3215.549574	426625.349902	46.260340
3211.836042	424872.173258	46.265345
3208.053994	423125.546925	46.270349
3203.908447	421383.086593	46.275354
3200.120973	419639.003242	46.280359
3196.462436	417893.333656	46.285364
3192.610741	416160.480139	46.290369
3188.760202	414429.868219	46.295373
3185.173813	412692.025024	46.300378
3181.435518	410956.804631	46.305383
3177.340704	409234.538451	46.310388
3173.723330	407504.351706	46.315393
3169.518586	405795.075250	46.320397
3165.905604	404068.680121	46.325402
3162.017452	402365.030261	46.330407
3158.419964	400657.655778	46.335412
3154.918969	398949.936936	46.340417
3150.773739	397248.081125	46.345421
3147.295421	395547.622261	46.350426
3143.396591	393843.655899	46.355431
3139.322381	392154.520761	46.360436
3135.354799	390450.884233	46.365441
3131.416702	388772.078739	46.370445
3127.798292	387090.621620	46.375450
3124.237197	385415.745350	46.380455
3120.077316	383744.863619	46.385460
3116.540323	382061.333194	46.390465
3112.887051	380393.734900	46.395469
3108.863611	378739.649303	46.400474
3105.248225	377065.434330	46.405479
3101.468170	375411.662313	46.410484
3098.006584	373754.945288	46.415489
3094.370582	372096.377001	46.420493
3090.177955	370440.387370	46.425498
3086.424891	368789.108628	46.430503
3082.503154	367145.432528	46.435508
3078.932566	365505.646924	46.440513
3075.174454	363865.899425	46.445517
3071.403718	362222.860429	46.450522
3067.586080	360598.085086	46.455527
3063.640874	358970.115923	46.460532
3060.139581	357333.654154	46.465537
3055.999945	355721.528165	46.470541
3052.334914	354103.042730	46.475546
3048.787992	352486.133408	46.480551
3045.061455	350876.999629	46.485556
3041.418898	349269.806388	46.490561
3037.708582	347659.926463	46.495565
3033.715787	346051.233018	46.500570
3030.156051	344447.785009	46.505575
3026.180670	342855.132633	46.510580
3022.830105	341252.290965	46.515585
3019.239197	339662.102279	46.520589
3015.211397	338062.603675	46.525594
3011.611485	336478.606922	46.530599
3007.794397	334889.692695	46.535604
3004.158573	333308.261008	46.540609
3000.628081	331727.789224	46.545613
2996.852479	330139.990667	46.550618
2993.175693	328556.613809	46.555623
2989.208706	326986.522112	46.560628
2985.764148	325410.639934	46.565633
2981.879750	323834.104036	46.570637
2978.237243	322279.475423	46.575642
2974.627741	320704.253503	46.580647
2970.576198	319148.505301	46.585652
2967.063549	317590.479850	46.590657
2963.488395	316041.924930	46.595661
2959.901796	314473.802658	46.600666
2956.129312	312934.001360	46.605671
2952.465114	311378.762778	46.610676
2948.822373	309828.635378	46.615681
2945.222555	308275.474015	46.620685
2941.311233	306735.723458	46.625690
2937.872783	305192.466801	46.630695
2933.708675	303644.594119	46.635700
2930.626219	302108.162554	46.640705
2926.439202	300570.841142	46.645709
2922.713949	299024.342897	46.650714
2919.262459	297502.804035	46.655719
2915.308535	295980.004570	46.660724
2911.712584	294456.370701	46.665729
2908.319649	292926.072880	46.670733
2904.258139	291412.895821	46.675738
2900.828297	289895.000721	46.680743
2897.103320	288381.391934	46.685748
2893.180835	286855.991864	46.690753
2889.663606	285349.892053	46.695757
2885.692228	283843.524311	46.700762
2882.293404	282338.358261	46.705767
2878.353698	280843.810705	46.710772
2875.134719	279336.670068	46.715777
2871.152138	277833.463223	46.720781
2867.587096	276336.196147	46.725786
2863.821726	274836.309773	46.730791
2859.849203	273353.564218	46.735796
2856.362265	271856.254202	46.740801
2852.570341	270383.945127	46.745805
2848.636182	268899.819406	46.750810
2845.326883	267412.898694	46.755815
2841.642589	265944.093091	46.760820
2838.021719	264473.804552	46.765825
2834.597332	263002.802384	46.770829
2830.743626	261532.560317	46.775834
2827.565679	260067.999381	46.780839
2823.778436	258592.972646	46.785844
2820.156130	257125.542055	46.790849
2816.513605	255658.734415	46.795853
2812.949298	254191.261804	46.800858
2809.475644	252723.454096	46.805863
2805.873172	251264.845545	46.810868
2801.816187	249797.559229	46.815873
2797.847027	248341.706499	46.820877
2794.386061	246883.979516	46.825882
2791.051137	245431.595205	46.830887
2787.471271	243979.926354	46.835892
2783.673568	242519.113324	46.840897
2779.858246	241085.035647	46.845901
2776.377116	239635.438348	46.850906
2772.725357	238182.243740	46.855911
2769.099388	236741.950950	46.860916
2765.609305	235301.198040	46.865921
2761.928835	233859.883952	46.870925
2757.872659	232422.826547	46.875930
2754.853688	230992.760011	46.880935
2750.823285	229554.927862	46.885940
2747.474024	228112.300637	46.890945
2743.904155	226685.267981	46.895949
2739.915937	225252.263806	46.900954
2736.466051	223828.038599	46.905959
2732.411932	222409.919226	46.910964
2728.967280	220988.598645	46.915969
2725.377618	219571.607038	46.920973
2721.515264	218156.290814	46.925978
2718.459112	216735.172358	46.930983
2714.241343	215315.156596	46.935988
2710.719567	213902.957571	46.940993
2707.242143	212491.699415	46.945997
2703.696444	211090.314378	46.951002
2699.933497	209677.942276	46.956007
2696.261620	208268.645113	46.961012
2692.586913	206874.739265	46.966017
2688.689808	205482.786962	46.971021
2685.068817	204075.622041	46.976026
2681.524472	202680.374110	46.981031
2678.177477	201288.416747	46.986036
2675.225670	199899.261181	46.991041
2671.357300	198500.226934	46.996045
2667.478707	197114.882606	47.001050
2663.812431	195708.966859	47.006055
2660.347162	194327.659621	47.011060
2656.463749	192932.527810	47.016065
2653.158569	191556.190861	47.021069
2649.231361	190163.032361	47.026074
2645.462206	188790.925255	47.031079
2641.787342	187411.053423	47.036084
2638.145142	186033.765946	47.041089
2634.861078	184668.968867	47.046093
2630.913288	183298.793897	47.051098
2627.647489	181919.492017	47.056103
2623.506904	180555.803041	47.061108
2620.235644	179189.477590	47.066113
2616.914900	177825.014133	47.071117
2612.938062	176464.354062	47.076122
2609.527011	175095.008905	47.081127
2605.526707	173741.717359	47.086132
2602.108365	172379.472141	47.091137
2598.447749	171020.929548	47.096141
2594.946978	169675.396194	47.101146
2591.278260	168309.088210	47.106151
2587.653418	166972.407594	47.111156
2584.344941	165615.221940	47.116161
2580.392823	164273.629244	47.121165
2576.686697	162921.192930	47.126170
2573.216603	161583.881438	47.131175
2569.687418	160246.848844	47.136180
2566.141768	158902.108784	47.141185
2562.449363	157569.792060	47.146189
2559.011547	156233.672195	47.151194
2555.215467	154887.698819	47.156199
2551.442798	153557.584782	47.161204
2547.893943	152224.437903	47.166209
2544.614958	150893.329428	47.171213
2540.673634	149557.330146	47.176218
2537.413321	148235.191616	47.181223
2533.721572	146865.180254	47.186228
2530.543580	145489.792891	47.191233
2526.342580	144170.920284	47.196237
2522.634630	142843.823541	47.201242
2519.179376	141531.787582	47.206247
2515.456128	140206.990999	47.211252
2512.143289	138898.566630	47.216257
2508.835153	137575.241380	47.221261
2504.691104	136265.112031	47.226266
2501.199069	134948.913367	47.231271
2497.764374	133646.190651	47.236276
2493.830874	132325.112959	47.241281
2490.342547	131018.481541	47.246285
2486.678301	129724.573789	47.251290
2483.250104	128408.637307	47.256295
2479.554969	127113.071359	47.261300
2476.074198	125811.496064	47.266305
2472.207221	124522.881118	47.271309
2468.785843	123223.884711	47.276314
2465.542547	121917.220996	47.281319
2461.617054	120624.264094	47.286324
2458.209366	119331.765030	47.291329
2454.444722	118044.108485	47.296333
2450.287009	116751.152603	47.301338
2447.032761	115463.707528	47.306343
2443.419163	114189.396512	47.311348
2440.059024	112897.594355	47.316353
2436.687097	111620.843067	47.321357
2433.215190	110340.351357	47.326362
2429.506394	109058.010454	47.331367
2425.561816	107779.440094	47.336372
2421.779372	106495.564904	47.341377
2418.110389	105226.949115	47.346381
2414.643411	103957.815233	47.351386
2411.410453	102689.595173	47.356391
2407.396320	101421.380449	47.361396
2403.809903	100152.664715	47.366401
2400.150306	98900.379940	47.371405
2396.313430	97639.872434	47.376410
2392.628151	96384.665103	47.381415
2389.140361	95136.618734	47.386420
2385.554456	93885.498683	47.391425
2381.802380	92638.648491	47.396429
2378.282138	91393.121456	47.401434
2374.658397	90143.163651	47.406439
2370.664343	88907.761902	47.411444
2367.213507	87677.840307	47.416449
2363.670387	86433.640854	47.421453
2359.719983	85210.773609	47.426458
2356.311933	83978.574055	47.431463
2353.028368	82757.675239	47.436468
2349.430203	81535.772742	47.441473
2345.842971	80317.312676	47.446477
2342.131403	79096.257702	47.451482
2338.526559	77870.006924	47.456487
2334.779707	76662.209986	47.461492
2331.026144	75446.771462	47.466497
2327.625968	74230.862230	47.471501
2323.621730	73034.670735	47.476506
2320.427270	71822.470315	47.481511
2316.635710	70626.061846	47.486516
2312.991536	69416.797627	47.491521
2309.186252	68223.053190	47.496525
2305.429447	67027.451923	47.501530
2302.205139	65834.527059	47.506535
2298.573158	64653.121356	47.511540
2295.051621	63464.657759	47.516545
2290.938232	62279.078406	47.521549
2287.342096	61105.373831	47.526554
2284.190247	59926.464443	47.531559
2280.043189	58746.377652	47.536564
2276.458936	57572.370537	47.541569
2272.653870	56412.877230	47.546573
2268.904577	55245.151245	47.551578
2265.509716	54089.792264	47.556583
2261.982194	52932.112276	47.561588
2258.415079	51773.613628	47.566593
2254.575838	50626.569833	47.571597
2251.045660	49476.857523	47.576602
2247.554742	48327.640375	47.581607
2243.861375	47185.730362	47.586612
2240.155061	46038.691708	47.591617
2236.353939	44900.338383	47.596621
2232.570967	43771.355692	47.601626
2229.281704	42642.486016	47.606631
2225.488736	41517.366920	47.611636
2221.730723	40391.399403	47.616641
2218.134559	39266.821254	47.621645
2214.396159	38152.657591	47.626650
2210.619826	37033.960976	47.631655
2206.981881	35931.497847	47.636660
2203.185868	34835.613757	47.641665
2199.560091	33729.078879	47.646669
2195.797397	32637.512108	47.651674
2192.224556	31541.523068	47.656679
2188.334179	30466.568215	47.661684
2184.718181	29385.326748	47.666689
2180.874687	28309.652662	47.671693
2177.043111	27235.446134	47.676698
2173.284141	26166.062359	47.681703
2169.526880	25096.899358	47.686708
2165.770482	24043.074483	47.691713
2162.298587	22990.787192	47.696717
2158.667370	21951.978805	47.701722
2154.971093	20913.963370	47.706727
2150.730440	19879.628500	47.711732
2147.150502	18849.203412	47.716737
2143.437537	17832.527832	47.721741
2139.269371	16814.893546	47.726746
2135.722839	15804.761263	47.731751
2131.501471	14815.109140	47.736756
2127.927642	13820.939261	47.741761
2123.993049	12835.742463	47.746765
2120.216588	11860.506482	47.751770
2116.255399	10897.259060	47.756775
2111.984838	9936.828532	47.761780
2108.329062	8986.170051	47.766785
2104.059194	8047.266123	47.771789
2099.822524	7125.305905	47.776794
2096.359826	6214.591435	47.781799
2092.051327	5321.514283	47.786804
2087.571157	4430.858802	47.791809
2083.313319	3555.945619	47.796813
2077.682058	2745.027938	47.801818
2069.078864	2017.205962	47.806823
2059.411924	1378.043753	47.811828
2049.846402	820.063030	47.816833
2040.073931	347.098015	47.821837
2024.933643	125.667783	47.826842
2005.382830	145.783110	47.831847
1994.699528	156.458947	47.836852
1990.897247	144.872958	47.841857
1990.713945	147.157330	47.846861
1991.895745	155.258393	47.851866
1993.011681	151.438890	47.856871
1993.149163	152.132273	47.861876
1991.872308	150.269106	47.866881
1989.811560	144.614919	47.871885
1986.491319	157.843498	47.876890
1983.577458	141.591031	47.881895
1980.596805	148.236290	47.886900
1977.176979	151.077722	47.891905
1973.909897	142.758511	47.896909
1970.611276	148.295559	47.901914
1967.860539	143.711154	47.906919
1964.874042	152.540387	47.911924
1961.731268	147.356084	47.916929
1958.618103	142.755626	47.921933
1955.369923	146.098566	47.926938
1952.211730	139.591030	47.931943
1948.619476	154.228959	47.936948
1945.613647	154.680191	47.941953
1942.336920	143.708034	47.946957
1938.816436	151.412239	47.951962
1935.941782	147.188929	47.956967
1932.221227	139.965782	47.961972
1928.768207	139.395468	47.966977
1925.590481	142.044002	47.971981
1921.663149	151.646906	47.976986
1918.944979	139.448372	47.981991
1915.566366	144.058289	47.986996
1911.865987	143.058439	47.992001
1908.471442	149.050288	47.997005
1905.197089	151.362761	48.002010
1902.381462	139.005473	48.007015
1898.668636	143.901817	48.012020
1894.877457	137.822393	48.017025
1891.600215	138.553400	48.022029
1887.801677	139.663383	48.027034
1884.625477	139.638241	48.032039
1880.789491	138.485612	48.037044
1877.723601	137.750329	48.042049
1874.730775	133.694234	48.047053
1871.405297	139.846130	48.052058
1868.456562	135.144041	48.057063
1864.602429	140.173241	48.062068
1861.180845	131.289782	48.067073
1857.897007	131.132792	48.072077
1853.453786	145.451470	48.077082
1850.091004	140.406043	48.082087
1847.076817	137.055672	48.087092
1843.427502	135.804241	48.092097
1840.011914	133.785388	48.097101
1836.513190	132.975478	48.102106
1832.975668	134.212318	48.107111
1829.655669	142.410373	48.112116
1825.785948	137.244964	48.117121
1823.167665	130.548580	48.122125
1819.331578	139.207060	48.127130
1816.405823	135.846024	48.132135
1812.326503	135.756584	48.137140
1808.817354	135.109671	48.142145
1805.853243	129.641197	48.147149
1801.622440	140.253428	48.152154
1798.450825	132.817880	48.157159
1794.631193	128.495722	48.162164
1791.393136	134.845933	48.167169
1788.339444	129.635099	48.172173
1784.952588	137.233005	48.177178
1781.227300	145.725458	48.182183
1777.779253	138.905831	48.187188
1774.198305	135.622032	48.192193
1770.536984	129.816578	48.197197
1767.709275	137.485176	48.202202
1764.189483	133.695087	48.207207
1760.608775	132.992948	48.212212
1756.906578	139.830269	48.217217
1753.509351	122.944861	48.222221
1749.425561	136.422682	48.227226
1746.253044	130.224357	48.232231
1742.939288	134.751402	48.237236
1739.501172	138.298137	48.242241
1736.470354	132.947695	48.247245
1732.261055	140.538282	48.252250
1728.939740	136.429235	48.257255
1725.421035	138.261131	48.262260
1722.027865	129.851021	48.267265
1718.650995	128.278580	48.272269
1714.755513	142.900729	48.277274
1711.970406	126.084060	48.282279
1708.567533	130.175796	48.287284
1704.300278	131.226317	48.292289
1700.980391	129.043835	48.297293
1697.488699	135.269246	48.302298
1694.341552	125.722795	48.307303
1690.653764	130.732344	48.312308
1686.980246	134.986669	48.317313
1684.015355	128.942540	48.322317
1680.018645	133.016487	48.327322
1676.425125	138.808576	48.332327
1673.386860	128.596505	48.337332
1669.677438	133.119053	48.342337
1666.601276	122.428852	48.347341
1662.778165	126.032698	48.352346
1659.253414	118.010218	48.357351
1655.638487	124.568143	48.362356
1652.037422	127.289335	48.367361
1648.727635	125.592521	48.372365
1645.409458	126.092722	48.377370
1642.177048	125.801198	48.382375
1638.536161	131.309637	48.387380
1634.490238	139.238527	48.392385
1631.431846	124.293363	48.397389
1627.835757	129.566997	48.402394
1624.378633	129.595393	48.407399
1620.221068	134.593067	48.412404
1617.170243	136.902277	48.417409
1614.544391	126.426362	48.422413
1610.436928	131.821167	48.427418
1607.204863	120.272682	48.432423
1603.025043	129.010329	48.437428
1599.796942	126.607867	48.442433
1596.309640	125.739304	48.447437
1592.711395	128.343011	48.452442
1589.203297	130.005608	48.457447
1586.022180	132.534541	48.462452
1582.747098	133.505756	48.467457
1579.092232	120.700974	48.472461
1575.512371	130.322353	48.477466
1572.052282	121.191937	48.482471
1568.386373	123.512006	48.487476
1564.615184	127.088777	48.492481
1561.435052	121.929451	48.497485
1558.030628	122.848149	48.502490
1554.349301	112.028085	48.507495
1551.075294	121.788262	48.512500
1547.618930	119.415218	48.517505
1544.161796	113.517790	48.522509
1540.358245	125.711579	48.527514
1537.006942	126.868749	48.532519
1533.858957	124.760662	48.537524
1529.942617	121.133974	48.542529
1526.258365	119.328130	48.547533
1522.863259	124.361525	48.552538
1519.273251	117.374398	48.557543
1515.817781	122.486847	48.562548
1512.534013	121.045441	48.567553
1509.187256	123.514898	48.572557
1505.249892	121.865741	48.577562
1502.034487	120.451605	48.582567
1498.765012	120.219713	48.587572
1494.811652	125.492359	48.592577
1491.460991	116.060107	48.597581
1487.918500	122.619399	48.602586
1484.806944	114.769606	48.607591
1481.007302	117.455494	48.612596
1477.494848	122.573710	48.617601
1474.108011	116.133782	48.622605
1470.492766	120.755549	48.627610
1467.042373	119.080806	48.632615
1463.293490	121.037402	48.637620
1459.761041	122.298883	48.642625
1456.533401	117.431777	48.647629
1452.997670	123.762226	48.652634
1449.674860	114.373090	48.657639
1446.042763	118.602023	48.662644
1442.491285	121.831225	48.667649
1439.430218	109.759331	48.672653
1435.381054	126.379820	48.677658
1431.935820	122.043502	48.682663
1428.619333	118.386240	48.687668
1424.818056	116.067230	48.692673
1421.383081	123.068467	48.697677
1417.785424	119.831715	48.702682
1414.328473	119.673491	48.707687
1411.296090	114.937194	48.712692
1407.664947	118.618648	48.717697
1404.256596	113.077480	48.722701
1400.782102	114.804482	48.727706
1396.951182	117.147275	48.732711
1393.456489	112.062562	48.737716
1389.566158	120.891008	48.742721
1386.494958	109.099139	48.747725
1382.770611	113.687389	48.752730
1379.616355	123.681968	48.757735
1376.582469	111.767199	48.762740
1372.596243	117.165255	48.767745
1369.153166	108.041760	48.772749
1365.568194	115.787842	48.777754
1361.890984	112.712266	48.782759
1358.526222	114.700522	48.787764
1354.437142	110.822534	48.792769
1351.496800	111.431368	48.797773
1347.942968	120.064781	48.802778
1344.255967	116.933795	48.807783
1341.062115	111.118624	48.812788
1337.850343	114.930611	48.817793
1334.268944	114.472349	48.822797
1330.620329	125.642174	48.827802
1326.887974	122.407559	48.832807
1323.844328	117.350345	48.837812
1320.016398	116.168198	48.842817
1316.199329	108.504844	48.847821
1313.002707	118.597819	48.852826
1309.147066	117.179564	48.857831
1306.193681	114.560190	48.862836
1302.360305	115.448043	48.867841
1299.026033	113.622304	48.872845
1295.456463	125.371398	48.877850
1292.028599	119.482142	48.882855
1288.811208	118.397426	48.887860
1285.214504	113.619796	48.892865
1281.847999	111.277078	48.897869
1277.852194	118.837558	48.902874
1274.587343	124.293570	48.907879
1270.790171	109.587616	48.912884
1266.919892	117.485960	48.917889
1263.878231	108.960910	48.922893
1260.405864	116.395160	48.927898
1256.586338	113.727891	48.932903
1253.835457	113.788228	48.937908
1250.123228	121.408732	48.942913
1246.305209	110.942411	48.947917
1242.652411	120.265240	48.952922
1239.261443	112.642785	48.957927
1235.940391	108.435806	48.962932
1232.213446	110.790855	48.967937
1229.170300	111.450622	48.972941
1225.538404	127.006077	48.977946
1222.194189	123.878425	48.982951
1218.658800	122.125327	48.987956
1214.700572	122.542367	48.992961
1211.305267	118.062274	48.997965
1207.901601	119.211930	49.002970
1204.273643	123.772497	49.007975
1200.798211	104.026869	49.012980
1197.499070	105.536659	49.017985
1194.198919	112.190977	49.022989
1190.505085	113.651825	49.027994
1186.864490	112.646053	49.032999
1183.257902	115.304988	49.038004
1179.857417	120.946779	49.043009
1176.749579	110.764789	49.048013
1173.076104	108.346779	49.053018
1169.461375	108.384188	49.058023
1166.040026	111.827230	49.063028
1162.550552	108.124383	49.068033
1159.240552	107.601550	49.073037
1155.241905	113.609081	49.078042
1151.714947	110.690404	49.083047
1148.736576	108.761543	49.088052
1144.538468	112.474898	49.093057
1141.336868	115.516543	49.098061
1138.113169	115.024499	49.103066
1134.124810	112.924726	49.108071
1131.120403	104.121809	49.113076
1127.478849	119.669302	49.118081
1123.964844	104.311643	49.123085
1120.355733	108.657308	49.128090
1116.813189	104.953296	49.133095
1113.476694	103.339948	49.138100
1109.802440	107.366779	49.143105
1106.297445	103.473391	49.148109
1103.173591	115.956358	49.153114
1099.291003	99.295980	49.158119
1096.428102	101.484164	49.163124
1092.587912	109.286101	49.168129
1088.959571	110.135608	49.173133
1085.003240	105.806681	49.178138
1081.556053	108.643178	49.183143
1078.320441	104.163450	49.188148
1074.868619	108.316823	49.193153
1071.460315	99.643607	49.198157
1067.845371	104.183195	49.203162
1064.445676	107.822200	49.208167
1060.834094	95.982200	49.213172
1057.405012	108.234544	49.218177
1054.116616	100.691026	49.223181
1050.573989	102.928697	49.228186
1046.831026	105.390727	49.233191
1043.505663	106.227617	49.238196
1040.018608	104.511315	49.243201
1036.660713	100.863849	49.248205
1032.533965	105.638608	49.253210
1029.344912	105.660043	49.258215
1025.611440	102.849683	49.263220
1021.564935	108.662269	49.268225
1018.545633	99.418797	49.273229
1015.506312	99.730010	49.278234
1012.238882	99.428359	49.283239
1008.932852	94.611666	49.288244
1004.685546	102.638726	49.293249
1001.443224	99.412948	49.298253
997.852361	104.382232	49.303258
994.188342	95.173276	49.308263
990.985136	102.758449	49.313268
986.880881	107.912525	49.318273
983.404748	98.807035	49.323277
980.233817	106.342865	49.328282
976.622139	102.032792	49.333287
973.390321	101.956536	49.338292
969.819650	109.308182	49.343297
966.678117	100.242058	49.348301
962.778993	105.576001	49.353306
959.153515	104.093379	49.358311
955.888762	94.676390	49.363316
952.112585	101.224970	49.368321
948.877536	95.055731	49.373325
945.402337	97.026612	49.378330
941.346100	104.871916	49.383335
938.299044	96.300387	49.388340
934.661399	105.402625	49.393345
931.184053	104.839635	49.398349
927.862350	93.150469	49.403354
924.434639	90.409338	49.408359
921.080174	93.674303	49.413364
917.581650	105.380723	49.418369
913.910174	101.541956	49.423373
910.046849	101.036247	49.428378
906.370252	100.830338	49.433383
903.604164	91.794044	49.438388
899.800474	95.081899	49.443393
896.421597	89.893837	49.448397
892.500725	96.268937	49.453402
889.051134	101.057945	49.458407
885.429335	97.901121	49.463412
882.173468	109.705602	49.468417
878.851330	101.379651	49.473421
875.206112	101.535842	49.478426
871.485829	107.787794	49.483431
868.107341	98.907514	49.488436
864.549293	108.006802	49.493441
861.406268	103.085545	49.498445
857.973582	102.676943	49.503450
854.108908	101.870907	49.508455
850.882777	99.974613	49.513460
847.098240	101.389680	49.518465
843.369084	107.073545	49.523469
839.879543	94.496359	49.528474
836.666488	103.481519	49.533479
833.565893	97.620306	49.538484
829.675201	98.596414	49.543489
826.420216	98.837053	49.548493
822.732664	102.540194	49.553498
819.231280	100.174477	49.558503
816.003527	95.339274	49.563508
812.277729	101.494029	49.568513
808.707139	96.797937	49.573517
805.342881	102.889753	49.578522
801.352816	100.230401	49.583527
797.790029	102.692785	49.588532
794.559881	99.901783	49.593537
791.195340	95.420210	49.598541
787.768225	102.208420	49.603546
784.144379	102.098704	49.608551
780.882882	103.732453	49.613556
776.923449	105.099004	49.618561
773.650813	92.902344	49.623565
770.225368	91.578302	49.628570
766.858386	100.976732	49.633575
763.186415	94.866495	49.638580
759.143461	102.905941	49.643585
755.868062	97.037331	49.648589
752.471530	90.757415	49.653594
749.232447	99.784638	49.658599
746.161601	93.064575	49.663604
742.193209	96.745283	49.668609
738.822863	98.984560	49.673613
734.880088	109.137570	49.678618
731.148271	97.901862	49.683623
728.286434	106.126523	49.688628
724.853651	102.123904	49.693633
721.034660	90.594969	49.698637
717.600472	90.727666	49.703642
714.219427	94.775157	49.708647
710.531575	100.234296	49.713652
706.653520	96.877229	49.718657
703.291839	92.240217	49.723661
700.001637	92.885055	49.728666
696.661607	98.273909	49.733671
693.213372	94.454061	49.738676
689.830528	103.791722	49.743681
685.993459	90.430630	49.748685
682.130789	92.737534	49.753690
679.218540	93.139689	49.758695
675.494805	95.140096	49.763700
671.703271	98.100262	49.768705
668.774407	85.179093	49.773709
665.046578	92.966736	49.778714
661.386530	88.281554	49.783719
658.387412	89.143416	49.788724
654.862958	93.798689	49.793729
650.860735	87.983838	49.798733
647.536799	95.512079	49.803738
643.893456	94.389892	49.808743
640.520794	89.131358	49.813748
637.070485	87.551830	49.818753
633.309627	93.389428	49.823757
629.992757	87.160367	49.828762
626.419902	93.136205	49.833767
622.942600	92.522705	49.838772
619.519960	97.896047	49.843777
615.987992	92.532755	49.848781
612.524373	101.667949	49.853786
608.836988	101.603055	49.858791
605.586724	90.842499	49.863796
602.020484	93.925599	49.868801
598.195329	90.883004	49.873805
594.878202	86.780070	49.878810
591.259763	90.222530	49.883815
588.330497	90.595740	49.888820
584.394141	94.549908	49.893825
581.202600	92.844452	49.898829
577.471511	91.334232	49.903834
573.356917	102.207075	49.908839
570.547304	91.330064	49.913844
567.061888	100.323150	49.918849
563.739026	88.972862	49.923853
560.303911	85.904001	49.928858
556.554341	84.766849	49.933863
552.638373	81.225965	49.938868
549.102953	91.397488	49.943873
546.005022	94.160485	49.948877
542.488718	93.619564	49.953882
538.987178	87.735843	49.958887
535.242098	91.321546	49.963892
531.765825	88.648288	49.968897
528.506492	92.132605	49.973901
524.621570	94.202609	49.978906
521.429047	93.822960	49.983911
518.048428	91.492235	49.988916
514.113495	96.702236	49.993921
511.137895	96.462623	49.998925
507.430662	95.863034	50.003930
503.770711	85.676066	50.008935
500.512388	92.361995	50.013940
496.533901	103.985514	50.018945
493.120963	82.964988	50.023949
490.043113	88.565945	50.028954
486.052231	100.276830	50.033959
483.209537	98.146606	50.038964
479.187332	99.551588	50.043969
476.238274	89.164700	50.048973
472.715277	86.685449	50.053978
469.166786	93.233336	50.058983
465.662193	97.360374	50.063988
461.357259	97.847852	50.068993
457.873191	92.771360	50.073997
454.848408	101.562616	50.079002
451.151337	95.222332	50.084007
447.880287	89.818247	50.089012
444.128183	93.537965	50.094017
440.680824	87.582524	50.099021
437.459837	91.257020	50.104026
433.648285	93.182690	50.109031
430.686647	97.303791	50.114036
427.082862	102.819468	50.119041
423.191586	101.008532	50.124045
419.742616	98.369008	50.129050
416.342632	99.850565	50.134055
412.887182	98.177016	50.139060
409.181897	95.039799	50.144065
405.756082	89.947878	50.149069
402.350952	93.192479	50.154074
398.513760	103.547365	50.159079
395.331360	96.477913	50.164084
391.883395	92.167760	50.169089
388.481368	87.758664	50.174093
385.141678	103.464697	50.179098
381.051514	107.664506	50.184103
377.695660	86.625608	50.189108
374.269991	98.444151	50.194113
370.952790	92.193102	50.199117
367.044086	103.865847	50.204122
363.449765	94.301422	50.209127
360.382565	85.255556	50.214132
356.699103	96.908838	50.219137
353.032057	93.037984	50.224141
349.589487	86.945790	50.229146
346.081301	92.032061	50.234151
343.053150	84.406957	50.239156
339.023112	89.432603	50.244161
335.553507	89.194501	50.249165
332.378155	90.900333	50.254170
328.675984	98.326565	50.259175
325.350090	94.063759	50.264180
321.913067	104.463556	50.269185
318.083851	84.005051	50.274189
314.655281	97.924822	50.279194
311.025193	101.109781	50.284199
307.851561	79.362171	50.289204
303.939491	88.494933	50.294209
300.725809	91.725399	50.299213
297.512126	90.988472	50.304218
293.670359	90.372082	50.309223
290.215731	81.320498	50.314228
286.884382	78.127927	50.319233
283.123055	83.956233	50.324237
279.607723	83.203291	50.329242
275.827819	83.564320	50.334247
272.955208	90.759378	50.339252
269.089392	96.309829	50.344257
265.637200	91.411927	50.349261
262.257327	90.226480	50.354266
258.581076	89.666435	50.359271
255.311282	78.991365	50.364276
251.184803	91.565134	50.369281
248.013736	92.602764	50.374285
244.662458	85.458593	50.379290
240.910040	96.553231	50.384295
237.907956	84.472634	50.389300
233.766815	82.925559	50.394305
230.890726	89.741518	50.399309
227.073710	83.654254	50.404314
223.365850	87.379781	50.409319
220.445074	91.016810	50.414324
216.749446	84.901043	50.419329
213.250420	90.827493	50.424333
209.549954	83.940524	50.429338
205.786783	82.944861	50.434343
202.777394	84.419091	50.439348
199.073263	87.837156	50.444353
196.072355	88.212226	50.449357
192.363640	87.973674	50.454362
188.320253	97.430778	50.459367
184.954364	82.980574	50.464372
181.548423	93.217348	50.469377
177.611720	84.658958	50.474381
175.050436	86.398358	50.479386
171.001647	91.300460	50.484391
167.755291	81.308300	50.489396
163.746539	96.062491	50.494401
160.090038	84.182529	50.499405
156.858884	100.108894	50.504410
153.118393	98.252313	50.509415
149.900869	95.513366	50.514420
146.654307	89.643657	50.519425
142.748630	95.061195	50.524429
139.417330	86.980624	50.529434
136.170748	99.084394	50.534439
132.539612	85.109209	50.539444
129.066273	90.294501	50.544449
125.746023	86.954721	50.549453
122.701336	86.707081	50.554458
118.522076	90.452718	50.559463
115.307932	94.752678	50.564468
111.195151	102.825457	50.569473
107.667827	94.791426	50.574477
104.457924	81.541212	50.579482
101.077466	83.940487	50.584487
97.666916	84.275364	50.589492
94.118634	81.145331	50.594497
90.250612	89.034232	50.599501
87.202998	88.473848	50.604506
83.245130	80.238368	50.609511
80.057406	93.952785	50.614516
76.463584	92.759801	50.619521
73.247493	87.356755	50.624525
69.412971	92.940346	50.629530
65.874677	89.520854	50.634535
62.356783	81.216453	50.639540
58.605934	85.958026	50.644545
55.572309	86.708432	50.649549
52.169551	90.642491	50.654554
48.343445	91.804966	50.659559
44.882759	85.646145	50.664564
41.403424	101.481706	50.669569
37.727145	91.598087	50.674573
34.916948	88.589722	50.679578
30.945530	90.325470	50.684583
27.587926	81.521404	50.689588
23.673158	91.521569	50.694593
20.333577	82.490053	50.699597
16.934187	81.576683	50.704602
13.561064	80.523157	50.709607
10.062353	88.471284	50.714612
6.192173	87.770888	50.719617
2.584124	88.446797	50.724621