Thu Aug 25 13:04:04 2022

Number of Points = 9925

Depth (nm)	Load (N)	Time (s)
1.404726	103.623058	0.000000
1.516902	115.988509	0.005005
1.659916	123.230126	0.010010
1.846935	110.365306	0.015014
1.978044	117.210149	0.020019
1.665862	106.255381	0.025024
1.480956	92.657901	0.030029
1.490549	85.272098	0.035034
1.086029	79.703916	0.040038
0.890273	73.669588	0.045043
0.483968	70.604239	0.050048
0.243768	56.850934	0.055053
0.445201	54.354759	0.060058
-0.458931	38.895814	0.065062
-0.322243	34.581125	0.070067
-0.829690	36.736036	0.075072
-0.907569	25.649693	0.080077
-1.128607	8.062096	0.085082
-1.778172	7.426682	0.090086
-2.052833	-0.588431	0.095091
-2.009437	0.891708	0.100096
-2.019659	-1.349833	0.105101
-2.539361	-4.236050	0.110106
-3.091456	-7.449386	0.115110
-3.600285	-9.584329	0.120115
-4.276695	-3.853204	0.125120
-4.452257	-7.638066	0.130125
-4.609641	-10.723420	0.135130
-4.650523	-15.263376	0.140134
-4.238550	-11.949057	0.145139
-4.992455	-0.947612	0.150144
-4.684823	-11.078765	0.155149
-5.413179	-5.975419	0.160154
-6.128962	-5.021738	0.165158
-5.985818	-24.400106	0.170163
-5.937291	-3.840112	0.175168
-6.302237	-8.841824	0.180173
-6.919257	-10.703550	0.185178
-7.337252	-1.064535	0.190182
-7.403042	-15.762602	0.195187
-7.489126	-5.508040	0.200192
-7.399259	-7.866503	0.205197
-7.816533	-7.380375	0.210202
-8.676023	-10.086800	0.215206
-8.643241	-11.373293	0.220211
-8.564813	-5.633889	0.225216
-9.088127	-16.039806	0.230221
-8.798265	-14.205979	0.235226
-9.763816	-11.906529	0.240230
-9.980196	-16.725872	0.245235
-10.409098	-14.605420	0.250240
-10.048923	-13.959530	0.255245
-10.296500	-15.072380	0.260250
-10.502013	-12.066274	0.265254
-10.534310	-13.209692	0.270259
-11.283986	-7.403813	0.275264
-11.809246	-10.260683	0.280269
-12.039773	-13.983148	0.285274
-12.178341	-9.279097	0.290278
-11.941157	-10.050285	0.295283
-12.765168	-9.139759	0.300288
-13.075366	-2.380842	0.305293
-13.527105	-8.549039	0.310298
-13.793016	-1.471193	0.315302
-13.499748	-13.102883	0.320307
-13.712057	-13.632799	0.325312
-13.553450	-12.540874	0.330317
-13.562823	-8.768230	0.335322
-14.370419	-8.116540	0.340326
-14.374981	-9.039676	0.345331
-14.889887	-5.172004	0.350336
-15.512775	-8.519780	0.355341
-15.681511	-5.804174	0.360346
-16.341552	-4.239128	0.365350
-16.011977	-2.174240	0.370355
-16.051830	-1.269518	0.375360
-16.147252	-8.743232	0.380365
-16.662413	-6.283395	0.385370
-17.312594	-3.226597	0.390374
-17.407034	-7.951153	0.395379
-17.725293	-2.617830	0.400384
-17.752916	-0.683637	0.405389
-17.731931	-13.933641	0.410394
-18.375099	-6.689119	0.415398
-18.554340	-10.160190	0.420403
-19.098411	-3.842358	0.425408
-19.263805	-10.802068	0.430413
-19.124866	-12.576595	0.435418
-19.026797	0.347806	0.440422
-19.720738	-9.297385	0.445427
-20.441736	6.476194	0.450432
-20.938616	-1.472461	0.455437
-20.542183	-7.200912	0.460442
-20.818306	-3.883183	0.465446
-20.903116	-13.085973	0.470451
-20.745044	-1.512410	0.475456
-21.721202	-0.369235	0.480461
-22.051055	-7.600572	0.485466
-21.983999	-9.544171	0.490470
-22.076898	-21.415906	0.495475
-21.976161	-9.545463	0.500480
-23.158268	-12.856236	0.505485
-23.500792	-12.090753	0.510490
-23.834220	6.466323	0.515494
-24.023788	-2.682093	0.520499
-23.914072	1.720465	0.525504
-23.927340	0.004587	0.530509
-23.885166	-5.718977	0.535514
-23.705145	0.289249	0.540518
-24.349998	-7.905137	0.545523
-24.970013	-7.301820	0.550528
-24.864274	-10.149989	0.555533
-25.660705	-6.247697	0.560538
-26.529031	-2.258210	0.565542
-26.091101	-5.974680	0.570547
-26.382851	-4.584399	0.575552
-26.518473	-11.536118	0.580557
-26.593889	-2.254503	0.585562
-26.923532	-10.533078	0.590566
-27.576220	-9.032459	0.595571
-27.895489	-6.356542	0.600576
-27.960111	-10.737754	0.605581
-27.686442	-12.555537	0.610586
-28.180083	-10.880522	0.615590
-28.215964	-13.845706	0.620595
-28.702524	-1.702904	0.625600
-29.026548	2.561970	0.630605
-29.045243	-12.500982	0.635610
-29.846082	-10.239993	0.640614
-30.315620	-11.786302	0.645619
-30.476703	-7.429902	0.650624
-30.167069	-15.862423	0.655629
-30.554410	-13.675716	0.660634
-31.012140	-15.274495	0.665638
-30.809709	-13.192851	0.670643
-30.672173	-5.969413	0.675648
-31.295655	-9.741038	0.680653
-31.766267	-15.127988	0.685658
-32.222982	-5.043146	0.690662
-31.965849	-13.208014	0.695667
-33.003145	-11.536401	0.700672
-33.835718	-1.243969	0.705677
-33.037947	-6.143122	0.710682
-33.656455	-3.999286	0.715686
-33.520424	-8.117708	0.720691
-33.664982	-8.322881	0.725696
-33.938077	2.255216	0.730701
-34.135104	-10.375333	0.735706
-34.630563	-8.244450	0.740710
-34.834002	-11.474447	0.745715
-35.392601	-9.203957	0.750720
-35.530485	-10.976239	0.755725
-35.423916	-11.856676	0.760730
-35.740309	-10.408750	0.765734
-35.928193	-8.553852	0.770739
-36.528170	-11.971654	0.775744
-36.920625	-6.598233	0.780749
-36.872160	-15.059436	0.785754
-37.096669	-2.701429	0.790758
-36.710819	-10.674494	0.795763
-37.175700	-12.291135	0.800768
-38.108126	-6.567353	0.805773
-38.343051	-5.499188	0.810778
-38.683095	-5.142218	0.815782
-39.084591	-8.875859	0.820787
-38.760205	-18.357896	0.825792
-38.767448	-8.349810	0.830797
-39.026169	-14.083172	0.835802
-39.829838	-3.725667	0.840806
-39.945265	-9.285330	0.845811
-39.999021	-6.049900	0.850816
-40.051767	-11.685822	0.855821
-40.409856	-12.711754	0.860826
-41.185560	-5.373698	0.865830
-41.377517	-11.851515	0.870835
-41.229770	0.634828	0.875840
-41.458267	-5.362702	0.880845
-41.365647	-8.762474	0.885850
-42.329005	-5.381357	0.890854
-42.572186	-8.563998	0.895859
-43.000993	-4.134010	0.900864
-43.133681	-5.362939	0.905869
-42.896479	-10.743735	0.910874
-43.224221	-4.137095	0.915878
-42.874211	-6.412931	0.920883
-43.607874	-9.252963	0.925888
-44.221689	-6.790323	0.930893
-43.870798	-13.830925	0.935898
-44.757899	-7.462510	0.940902
-45.391701	-13.845785	0.945907
-45.712672	-1.282837	0.950912
-46.108520	-1.508748	0.955917
-45.511652	-6.455516	0.960922
-45.751967	-3.371189	0.965926
-45.515607	-6.217679	0.970931
-45.958360	4.061134	0.975936
-46.745490	-5.107544	0.980941
-46.931139	-4.701999	0.985946
-47.429240	3.848579	0.990950
-47.448156	-5.842266	0.995955
-47.647482	-2.495441	1.000960
-47.928902	-7.994293	1.005965
-47.890734	-2.931955	1.010970
-48.462538	0.125219	1.015974
-48.714532	-2.761811	1.020979
-49.018052	1.680185	1.025984
-49.083187	2.835642	1.030989
-48.870988	4.188090	1.035994
-49.634044	-1.709862	1.040998
-49.969295	-1.904138	1.046003
-50.489319	0.613410	1.051008
-50.899459	5.220810	1.056013
-50.345589	3.792556	1.061018
-50.454634	12.892785	1.066022
-50.929011	2.710150	1.071027
-51.294727	4.773249	1.076032
-51.940431	6.177863	1.081037
-51.738906	2.745206	1.086042
-52.008991	8.637297	1.091046
-52.000711	2.162902	1.096051
-52.543943	1.210273	1.101056
-53.350445	-1.498124	1.106061
-53.257271	-9.229176	1.111066
-53.482478	0.708662	1.116070
-53.461846	-7.343220	1.121075
-53.289949	-2.061390	1.126080
-54.340615	-1.042578	1.131085
-54.163807	-2.158649	1.136090
-54.799168	4.277895	1.141094
-55.101780	-9.354841	1.146099
-54.728536	-3.107974	1.151104
-55.518134	4.937784	1.156109
-56.072210	-2.574796	1.161114
-56.613793	-1.449089	1.166118
-56.476542	-8.253737	1.171123
-56.566471	8.018910	1.176128
-56.438631	2.047803	1.181133
-56.577925	0.130209	1.186138
-56.490216	-3.955331	1.191142
-57.071170	-9.312336	1.196147
-57.546082	-1.262105	1.201152
-57.912854	4.224353	1.206157
-57.899703	-2.785480	1.211162
-58.251778	4.571625	1.216166
-58.884715	-0.024261	1.221171
-59.221834	-7.371515	1.226176
-59.231846	1.108910	1.231181
-59.086376	-8.218546	1.236186
-59.838952	-5.658232	1.241190
-59.770339	-4.745196	1.246195
-60.409173	-3.319513	1.251200
-60.486867	-0.804833	1.256205
-60.106530	-10.479139	1.261210
-60.572417	-0.763019	1.266214
-61.118440	-7.005023	1.271219
-61.961192	-5.664448	1.276224
-62.077729	1.731680	1.281229
-62.268998	0.986495	1.286234
-62.320735	-8.155037	1.291238
-62.467194	-4.515938	1.296243
-62.282949	-1.675305	1.301248
-62.613644	-4.512038	1.306253
-63.017722	-3.626176	1.311258
-63.514982	-6.095123	1.316262
-64.020676	-7.967961	1.321267
-63.962918	-1.409068	1.326272
-63.902450	1.444632	1.331277
-63.616715	-1.482361	1.336282
-64.916186	-10.662504	1.341286
-65.134206	-2.225418	1.346291
-65.155442	-7.698598	1.351296
-65.492237	-2.182037	1.356301
-65.160194	-16.572272	1.361306
-66.175944	-10.095112	1.366310
-66.409812	-5.075572	1.371315
-66.623201	-9.537876	1.376320
-66.824037	-7.627164	1.381325
-66.726922	-4.624182	1.386330
-66.913745	-6.970928	1.391334
-67.026055	-13.806073	1.396339
-67.568355	-18.036503	1.401344
-68.156015	-7.772958	1.406349
-68.402881	-11.442239	1.411354
-68.461575	-10.306775	1.416358
-68.322162	-16.956734	1.421363
-69.231702	-12.163519	1.426368
-69.957120	-13.733007	1.431373
-69.729446	-14.471069	1.436378
-69.820819	-5.576101	1.441382
-69.684617	-9.874883	1.446387
-69.662370	-16.661507	1.451392
-70.198497	-6.456656	1.456397
-70.714490	-7.182597	1.461402
-71.111499	-9.692561	1.466406
-70.876463	-10.811428	1.471411
-70.903197	-10.854728	1.476416
-71.734806	-6.016775	1.481421
-72.022967	-10.809049	1.486426
-72.427430	-20.461618	1.491430
-72.299143	-18.567676	1.496435
-72.573965	-2.073079	1.501440
-72.665655	-3.248320	1.506445
-72.859739	-11.617732	1.511450
-73.834359	-9.164995	1.516454
-74.029237	-16.158044	1.521459
-73.565161	-15.000089	1.526464
-74.090437	-5.062694	1.531469
-74.277473	-20.459925	1.536474
-75.325897	-14.271876	1.541478
-75.501013	-10.897209	1.546483
-75.465654	-15.218153	1.551488
-75.511336	-5.843125	1.556493
-75.275980	-11.464077	1.561498
-75.536528	-5.095758	1.566502
-75.843539	-17.569856	1.571507
-76.591370	-10.878413	1.576512
-76.800505	-17.185854	1.581517
-76.931337	-15.444300	1.586522
-77.031911	-7.411598	1.591526
-77.201398	-16.360667	1.596531
-77.982928	-12.277211	1.601536
-78.534927	-7.967126	1.606541
-78.332158	-11.159529	1.611546
-78.613275	-10.748516	1.616550
-78.658441	-12.895994	1.621555
-78.571481	-7.366739	1.626560
-78.787904	-13.011814	1.631565
-79.176629	-16.639882	1.636570
-79.871042	-2.205588	1.641574
-79.891591	-7.337188	1.646579
-80.152154	-15.699345	1.651584
-80.365912	-10.828491	1.656589
-80.788189	-15.220097	1.661594
-81.228407	-11.563444	1.666598
-81.606886	-8.694751	1.671603
-81.752025	-7.665964	1.676608
-81.809818	-3.398515	1.681613
-81.668018	-13.984570	1.686618
-81.754290	-3.932464	1.691622
-82.285503	-10.983546	1.696627
-82.766503	-10.329240	1.701632
-83.039289	-7.942181	1.706637
-82.655984	-12.934580	1.711642
-83.117916	-2.026342	1.716646
-84.164063	-9.502940	1.721651
-83.955476	-11.282053	1.726656
-84.506394	-3.106018	1.731661
-84.371677	-17.085680	1.736666
-84.621854	-17.517912	1.741670
-84.671127	-7.806965	1.746675
-84.928211	-2.559159	1.751680
-85.670683	-6.941723	1.756685
-85.534188	-5.210418	1.761690
-85.773159	-12.421186	1.766694
-86.273023	-22.409982	1.771699
-86.750650	-9.642162	1.776704
-87.191949	-3.580879	1.781709
-87.290436	-10.203054	1.786714
-87.101908	-10.197825	1.791718
-87.238338	-10.091058	1.796723
-87.835474	-10.089273	1.801728
-87.796780	-10.164971	1.806733
-88.137230	-14.601035	1.811738
-88.134112	-5.616470	1.816742
-88.672887	-7.569544	1.821747
-88.691341	-10.037583	1.826752
-89.109677	-11.569765	1.831757
-89.555810	-14.027737	1.836762
-90.571330	-5.184117	1.841766
-90.332284	-10.514581	1.846771
-90.184745	0.380416	1.851776
-90.282461	3.780924	1.856781
-89.989977	-6.297234	1.861786
-91.011019	-2.891255	1.866790
-91.027765	-8.773263	1.871795
-91.319465	-5.788452	1.876800
-91.983450	2.044633	1.881805
-91.853535	-2.768859	1.886810
-92.621844	6.466303	1.891814
-93.057845	-9.603770	1.896819
-93.279773	-12.770755	1.901824
-93.159836	-0.843211	1.906829
-92.894195	-4.776297	1.911834
-93.615946	-9.431026	1.916838
-93.253666	-8.813943	1.921843
-93.432208	-14.610485	1.926848
-94.322957	-1.344492	1.931853
-94.373774	-11.343543	1.936858
-94.667615	-4.280307	1.941862
-94.926332	-3.768399	1.946867
-95.050570	-1.486873	1.951872
-95.804246	6.768393	1.956877
-96.178908	-7.681953	1.961882
-96.442051	3.293215	1.966886
-96.443184	6.219843	1.971891
-96.093486	2.659564	1.976896
-96.394463	-4.044779	1.981901
-96.848133	2.394933	1.986906
-97.380500	8.334448	1.991910
-97.679673	3.056678	1.996915
-97.769991	4.406450	2.006912
-97.885556	-1.622865	2.016909
-96.840586	-2.806705	2.026906
-96.873030	4.028124	2.036902
-96.251715	0.503128	2.046899
-95.771243	-1.837210	2.056896
-94.517134	-1.853219	2.066893
-94.343505	-3.499243	2.076890
-94.209750	-5.037648	2.086886
-93.485118	-1.983442	2.096883
-92.957444	3.863961	2.106880
-92.959702	-6.370959	2.116877
-91.332812	-3.629193	2.126874
-90.945569	-3.959199	2.136870
-91.135694	-4.616887	2.146867
-91.340646	-6.061038	2.156864
-90.200537	-4.402417	2.166861
-89.172093	-7.072539	2.176858
-88.665074	-6.410780	2.186854
-88.460239	-3.785144	2.196851
-88.242256	-8.162437	2.206848
-87.685186	-7.483179	2.216845
-87.051579	-8.089374	2.226842
-86.404533	-5.342961	2.236838
-85.604625	-8.180013	2.246835
-85.313984	-11.656360	2.256832
-85.075985	-7.822648	2.266829
-84.614617	-11.452459	2.276826
-84.004673	-6.948431	2.286822
-83.734572	-7.500836	2.296819
-82.805402	-7.073119	2.306816
-82.724563	-14.780468	2.316813
-81.870185	-15.044286	2.326810
-81.142695	-6.570399	2.336806
-81.177353	-3.460575	2.346803
-80.617494	-5.100593	2.356800
-79.819625	-8.311127	2.366797
-79.604765	-12.212758	2.376794
-79.123360	-5.936787	2.386790
-78.624876	-4.443723	2.396787
-77.851622	-6.218548	2.406784
-77.261500	-4.476914	2.416781
-76.998454	-4.622733	2.426778
-76.855398	-9.409605	2.436774
-75.918910	-0.395089	2.446771
-75.443026	-10.286777	2.456768
-74.750158	-11.418610	2.466765
-74.161413	-4.972557	2.476762
-74.121348	-0.803718	2.486758
-73.872841	-6.380062	2.496755
-73.204816	-6.909286	2.506752
-72.388700	-5.389964	2.516749
-71.429627	-4.624807	2.526746
-71.466825	-3.513475	2.536742
-71.238254	-7.588317	2.546739
-70.618190	-5.870382	2.556736
-69.977258	-7.722675	2.566733
-69.284379	-2.617083	2.576730
-68.785912	-11.330714	2.586726
-68.574088	-6.776974	2.596723
-68.182407	-10.528914	2.606720
-67.781058	-6.600419	2.616717
-66.734958	-11.322881	2.626714
-66.169643	-4.065362	2.636710
-66.103007	-1.576461	2.646707
-65.380115	-1.582089	2.656704
-64.635639	-3.368243	2.666701
-64.499298	3.576357	2.676698
-64.258583	-3.756905	2.686694
-63.539520	2.836628	2.696691
-63.023011	1.808455	2.706688
-62.176721	-8.689305	2.716685
-61.778565	-9.714771	2.726682
-61.692541	-2.046363	2.736678
-60.903838	-3.063332	2.746675
-60.342311	-9.420487	2.756672
-60.105940	1.376340	2.766669
-59.249059	-8.622564	2.776666
-58.762078	2.686196	2.786662
-58.743654	-0.028405	2.796659
-57.776288	-1.133557	2.806656
-57.234550	-0.271329	2.816653
-57.114891	-4.335442	2.826650
-56.251017	-3.634562	2.836646
-55.779729	-2.308297	2.846643
-55.524405	0.828952	2.856640
-55.046781	1.279907	2.866637
-54.390155	-0.549502	2.876634
-53.840475	6.317663	2.886630
-53.046361	7.837268	2.896627
-52.966925	-0.256343	2.906624
-52.885446	-9.218252	2.916621
-51.767182	-2.864668	2.926618
-51.389069	-5.356860	2.936614
-51.012977	-2.305058	2.946611
-50.045067	7.803776	2.956608
-49.786194	3.857231	2.966605
-49.844745	-3.365783	2.976602
-49.050009	-6.487126	2.986598
-48.607598	6.098916	2.996595
-47.348515	-7.748551	3.006592
-46.824461	-4.266935	3.016589
-47.038401	-0.482783	3.026586
-46.682252	-1.913484	3.036582
-45.910232	-0.748380	3.046579
-45.323625	3.290475	3.056576
-45.141424	0.886000	3.066573
-44.306419	-5.754760	3.076570
-44.164216	-3.426587	3.086566
-43.349376	1.108700	3.096563
-42.486168	-6.170043	3.106560
-42.452089	-7.170140	3.116557
-42.017195	-4.178237	3.126554
-41.203617	-5.892853	3.136550
-40.931834	0.175215	3.146547
-40.319628	-2.135077	3.156544
-39.552374	-5.752628	3.166541
-39.423510	-8.905853	3.176538
-39.067680	-10.957394	3.186534
-38.178505	-1.726381	3.196531
-38.310049	-2.355237	3.206528
-37.274976	-1.639997	3.216525
-36.602112	-4.729572	3.226522
-36.496674	-8.202244	3.236518
-35.810638	-5.037447	3.246515
-35.407086	-2.376420	3.256512
-35.065439	-9.928235	3.266509
-34.026433	-9.324485	3.276506
-33.667711	-5.775782	3.286502
-33.449168	-2.141758	3.296499
-32.738475	-0.232110	3.306496
-32.213275	-0.035698	3.316493
-32.084425	-6.581652	3.326490
-31.283716	-8.420964	3.336486
-30.569749	-1.677742	3.346483
-30.521573	2.157207	3.356480
-30.002053	-4.285234	3.366477
-29.441951	-0.964487	3.376474
-29.029852	-1.646846	3.386470
-28.088231	4.005825	3.396467
-28.100458	-4.095598	3.406464
-27.398970	1.252573	3.416461
-26.802995	-4.108951	3.426458
-26.605411	-9.366869	3.436454
-25.793832	-1.590394	3.446451
-25.327011	-5.975000	3.456448
-24.874791	-4.531704	3.466445
-23.984353	-2.840288	3.476442
-24.166487	-6.746242	3.486438
-23.347733	-2.791278	3.496435
-22.367393	-2.678849	3.506432
-22.370579	-2.269766	3.516429
-22.110211	-9.346345	3.526426
-20.980078	-1.705313	3.536422
-20.700830	-4.289720	3.546419
-20.672905	-6.913943	3.556416
-19.752124	-0.675129	3.566413
-19.524304	-7.413988	3.576410
-18.960373	-8.044108	3.586406
-18.220848	-4.501216	3.596403
-18.080932	4.156616	3.606400
-17.067437	1.064355	3.616397
-16.623634	3.082346	3.626394
-16.408372	-2.124492	3.636390
-16.033403	0.737420	3.646387
-15.171558	2.221073	3.656384
-15.044921	1.196969	3.666381
-13.857581	-2.122103	3.676378
-13.459495	-3.876154	3.686374
-13.397850	-1.877481	3.696371
-13.163060	-2.810825	3.706368
-12.089002	-9.451025	3.716365
-11.739725	-5.371815	3.726362
-11.476382	-7.003384	3.736358
-10.934317	-1.598554	3.746355
-10.437541	-0.409328	3.756352
-9.296610	-6.077983	3.766349
-9.147038	-4.064576	3.776346
-9.203290	-9.906783	3.786342
-8.166247	-11.960520	3.796339
-7.682187	-9.559196	3.806336
-7.752266	-1.688927	3.816333
-6.602277	-7.210114	3.826330
-6.088877	-7.075207	3.836326
-5.725215	-4.506131	3.846323
-5.248010	-1.036177	3.856320
-4.669760	-2.340117	3.866317
-4.569830	-1.624072	3.876314
-4.124197	8.157955	3.886310
-3.769137	15.283706	3.896307
-3.275430	30.155237	3.906304
-2.576698	41.842671	3.916301
-2.179227	50.586886	3.926298
-1.609165	64.607008	3.936294
-1.586942	76.609538	3.946291
-0.853216	97.462399	3.956288
-0.506267	110.741397	3.966285
0.000000	118.681209	3.971290
0.217999	138.746575	3.976294
0.562549	148.832512	3.981299
0.890061	155.725692	3.986304
0.861181	160.596101	3.991309
0.596374	159.856102	3.996314
0.976125	160.805821	4.001318
0.795855	160.641042	4.006323
1.312135	153.292883	4.011328
1.016271	167.111207	4.016333
0.950971	156.355011	4.021338
0.816608	164.839183	4.026342
0.750167	160.436066	4.031347
1.002012	154.366382	4.036352
0.922999	162.038277	4.041357
0.846884	165.201312	4.046362
0.949485	178.080841	4.051366
1.088519	189.211417	4.056371
1.373825	187.980258	4.061376
1.394914	195.731397	4.066381
1.546992	187.415215	4.071386
1.080059	167.651329	4.076390
1.217335	172.229949	4.081395
1.398774	165.598645	4.086400
0.895553	162.504171	4.091405
1.083259	173.326551	4.096410
1.132426	169.689940	4.101414
1.403741	171.593133	4.106419
1.548957	178.714204	4.111424
1.349229	185.977910	4.116429
1.597826	173.125543	4.121434
1.412970	167.994322	4.126438
1.428379	164.185829	4.131443
1.347138	158.320194	4.136448
1.284251	165.015115	4.141453
1.303511	168.286595	4.146458
1.235388	166.816579	4.151462
1.055545	158.729590	4.156467
1.308752	170.500335	4.161472
1.378268	186.359023	4.166477
1.744848	180.451690	4.171482
1.691011	173.116918	4.176486
1.282769	169.422259	4.181491
1.510211	162.249067	4.186496
1.028718	169.465164	4.191501
1.324592	183.513494	4.196506
1.468525	181.418622	4.201510
1.225444	189.704702	4.206515
1.531886	182.832340	4.211520
1.558890	187.535811	4.216525
1.544531	184.570384	4.221530
1.647072	189.644840	4.226534
1.270538	185.511769	4.231539
1.669389	185.107554	4.236544
1.759610	183.976565	4.241549
1.633782	181.389277	4.246554
1.828371	187.869856	4.251558
1.449974	182.534834	4.256563
1.739680	183.644197	4.261568
1.543250	193.520688	4.266573
1.422454	190.723800	4.271578
1.790245	186.249476	4.276582
1.606405	187.012250	4.281587
1.767907	178.912898	4.286592
1.592065	187.027088	4.291597
1.594204	193.050597	4.296602
1.716201	187.488472	4.301606
1.605924	194.497717	4.306611
1.492209	190.389906	4.311616
1.697967	189.743859	4.316621
1.717109	198.390659	4.321626
1.866353	192.742005	4.326630
1.626571	197.215192	4.331635
1.508594	191.133836	4.336640
1.632097	203.981635	4.341645
1.749319	213.324931	4.346650
1.957751	216.326330	4.351654
2.092633	216.055224	4.356659
2.195892	217.124199	4.361664
1.828143	208.699626	4.366669
1.747965	211.417209	4.371674
2.008533	209.326206	4.376678
1.693737	221.806086	4.381683
1.944643	222.329899	4.386688
1.851337	217.459570	4.391693
2.024785	220.384193	4.396698
2.017216	226.545278	4.401702
1.738587	224.956377	4.406707
2.103491	223.687434	4.411712
1.728101	226.046306	4.416717
1.805619	220.760063	4.421722
1.637263	223.757223	4.426726
1.712766	225.286135	4.431731
1.807738	221.936571	4.436736
2.262446	220.137856	4.441741
1.804630	224.335159	4.446746
2.185172	223.709182	4.451750
1.924040	241.960943	4.456755
2.485531	240.591592	4.461760
2.202894	232.235933	4.466765
2.135407	223.495384	4.471770
2.310439	219.826387	4.476774
1.842857	229.846625	4.481779
2.562896	229.907785	4.486784
2.337858	229.737365	4.491789
2.134125	217.376625	4.496794
2.110136	227.887351	4.501798
2.270392	241.558336	4.506803
2.759772	230.825920	4.511808
2.648114	224.528424	4.516813
2.028571	216.516629	4.521818
2.240619	224.282154	4.526822
2.003841	231.314398	4.531827
2.501505	219.862506	4.536832
2.291044	216.671532	4.541837
2.702861	219.043106	4.546842
2.523263	221.175144	4.551846
2.285202	223.702328	4.556851
2.560682	213.851336	4.561856
2.378309	215.961662	4.566861
2.271286	218.177243	4.571866
2.351951	219.879355	4.576870
2.243555	233.405762	4.581875
2.024783	233.129954	4.586880
2.116365	239.345112	4.591885
2.637692	240.759879	4.596890
3.016877	252.061679	4.601894
2.942343	250.988138	4.606899
2.528506	234.487239	4.611904
2.276883	230.935709	4.616909
2.310018	236.017889	4.621914
3.056754	236.454524	4.626918
3.036716	239.491724	4.631923
2.868976	230.115135	4.636928
2.530093	232.287951	4.641933
2.359672	220.991356	4.646938
2.534629	221.112611	4.651942
2.209274	229.003468	4.656947
2.305726	229.548318	4.661952
2.395226	245.498842	4.666957
2.819879	255.401444	4.671962
2.606303	243.874310	4.676966
2.364138	252.252025	4.681971
2.535967	254.132849	4.686976
2.801374	257.144311	4.691981
2.695163	261.590259	4.696986
2.852277	250.916218	4.701990
2.811617	253.855410	4.706995
3.053746	248.587661	4.712000
2.549707	254.617732	4.717005
2.726808	260.303796	4.722010
2.673555	256.512369	4.727014
2.292611	251.769358	4.732019
2.473137	254.461918	4.737024
2.758721	249.465776	4.742029
2.240088	244.415304	4.747034
2.899717	268.904232	4.752038
2.901750	286.279558	4.757043
3.138252	277.057911	4.762048
2.950869	282.332846	4.767053
2.848447	262.919873	4.772058
3.162823	262.889567	4.777062
3.050442	272.819373	4.782067
2.997942	260.881005	4.787072
2.830583	267.880240	4.792077
2.841971	258.833082	4.797082
3.167010	260.183691	4.802086
2.888395	275.698364	4.807091
3.057392	271.891094	4.812096
3.147193	281.453862	4.817101
2.874965	269.844151	4.822106
3.032453	266.560714	4.827110
3.136002	285.258427	4.832115
3.167441	277.024383	4.837120
3.014413	277.636797	4.842125
2.756984	282.055821	4.847130
3.305871	272.911784	4.852134
2.707918	279.763350	4.857139
3.469944	268.260516	4.862144
3.137552	280.581839	4.867149
2.961156	281.662996	4.872154
3.022055	280.270835	4.877158
2.921165	284.570418	4.882163
3.119422	271.295589	4.887168
2.838097	278.306357	4.892173
3.089536	287.622336	4.897178
3.313385	277.143471	4.902182
2.813768	277.756405	4.907187
3.001676	275.752710	4.912192
3.303377	286.079562	4.917197
3.181899	293.425966	4.922202
3.275109	309.451897	4.927206
3.590487	300.350760	4.932211
3.541350	290.041213	4.937216
3.327644	287.341126	4.942221
3.364289	280.688173	4.947226
3.313831	281.161128	4.952230
3.080671	291.448396	4.957235
3.298275	296.460561	4.962240
3.394995	301.611892	4.967245
3.357538	300.500900	4.972250
3.419275	301.288478	4.977254
3.412742	308.376428	4.982259
3.543664	296.532686	4.987264
3.572025	308.164742	4.992269
3.395246	308.723929	4.997274
3.673619	297.803067	5.002278
3.233657	307.844331	5.007283
3.344690	311.145751	5.012288
3.326307	307.231788	5.017293
3.213053	303.911670	5.022298
3.379461	310.852299	5.027302
3.539597	308.270808	5.032307
3.746143	305.625098	5.037312
3.896264	312.792911	5.042317
3.673804	310.249220	5.047322
3.080833	307.991376	5.052326
3.030772	313.238476	5.057331
3.067366	313.757905	5.062336
3.386050	319.466099	5.067341
3.582752	328.793839	5.072346
3.708649	331.286158	5.077350
3.475698	339.013887	5.082355
3.899855	327.851860	5.087360
4.091542	331.358951	5.092365
3.925599	334.880946	5.097370
4.194891	321.560148	5.102374
3.706090	335.237986	5.107379
3.746981	322.022578	5.112384
3.787327	326.176653	5.117389
3.894601	331.427582	5.122394
4.128188	330.821462	5.127398
3.658119	322.245185	5.132403
3.877062	309.156916	5.137408
3.696725	312.548282	5.142413
3.712348	324.163361	5.147418
4.239081	333.626060	5.152422
3.676176	322.216885	5.157427
4.032999	326.191657	5.162432
3.986259	331.438243	5.167437
3.935149	330.000351	5.172442
3.788111	321.844870	5.177446
3.924972	334.969087	5.182451
3.969808	333.142830	5.187456
3.983122	339.737290	5.192461
4.039392	330.679899	5.197466
4.067887	333.902504	5.202470
3.799719	336.447076	5.207475
3.919109	326.892568	5.212480
3.970057	336.189364	5.217485
4.042483	335.092791	5.222490
3.943009	328.204878	5.227494
3.601683	335.902128	5.232499
4.036378	333.008691	5.237504
3.801799	341.635202	5.242509
3.803063	339.556337	5.247514
4.212792	338.185448	5.252518
4.058722	335.526631	5.257523
4.333440	339.843309	5.262528
3.893319	342.914707	5.267533
4.061584	339.499852	5.272538
4.133229	330.753271	5.277542
4.148896	344.209702	5.282547
4.211006	337.824827	5.287552
4.288313	339.818549	5.292557
4.156939	345.533990	5.297562
4.511283	343.972457	5.302566
4.113667	343.433597	5.307571
4.473424	346.256281	5.312576
4.083285	347.041893	5.317581
3.773143	348.280054	5.322586
4.112661	359.660905	5.327590
4.140817	371.489191	5.332595
4.567166	360.013582	5.337600
4.642469	366.658452	5.342605
4.258299	367.930360	5.347610
4.640948	368.667659	5.352614
4.360938	367.047324	5.357619
4.831797	361.449468	5.362624
4.531876	354.880859	5.367629
4.521965	347.089869	5.372634
4.443425	339.246359	5.377638
4.517316	342.718123	5.382643
4.662999	344.840341	5.387648
4.427625	336.632254	5.392653
4.112577	336.969492	5.397658
4.248805	337.008229	5.402662
4.182637	355.403569	5.407667
4.950618	358.136983	5.412672
5.082003	361.008106	5.417677
4.607563	350.027989	5.422682
4.633451	349.039950	5.427686
3.988498	350.919042	5.432691
4.891027	348.676818	5.437696
4.861325	347.906302	5.442701
4.366980	349.318860	5.447706
4.423219	343.966311	5.452710
4.485934	357.149619	5.457715
4.732414	359.249717	5.462720
4.661777	365.376438	5.467725
4.442328	372.874269	5.472730
4.783146	362.807310	5.477734
4.603239	371.763799	5.482739
4.796228	357.461486	5.487744
4.943785	370.403715	5.492749
4.831971	368.915218	5.497754
4.953319	358.442875	5.502758
4.715438	363.602356	5.507763
4.416358	356.638136	5.512768
4.758495	361.285949	5.517773
4.363295	364.052913	5.522778
4.647913	365.065007	5.527782
4.459735	371.713195	5.532787
4.343984	366.745099	5.537792
4.537232	364.348243	5.542797
4.497034	373.646684	5.547802
4.688684	374.660689	5.552806
4.981222	393.249808	5.557811
5.190480	394.178796	5.562816
5.152855	377.552378	5.567821
4.766534	366.416072	5.572826
4.921195	360.649454	5.577830
4.520528	363.853883	5.582835
4.758601	381.483391	5.587840
4.963871	394.030607	5.592845
5.250343	390.907277	5.597850
5.184199	390.832185	5.602854
5.118592	403.393374	5.607859
5.319674	388.542424	5.612864
4.649902	388.429028	5.617869
4.839834	390.310194	5.622874
5.089432	390.672862	5.627878
4.947778	394.026544	5.632883
5.262784	391.458743	5.637888
4.988961	393.314492	5.642893
5.015249	392.168196	5.647898
5.294198	388.027291	5.652902
5.070819	381.747243	5.657907
5.114184	384.363236	5.662912
5.116170	391.978245	5.667917
4.922708	393.340500	5.672922
4.998976	390.129879	5.677926
4.850803	393.883226	5.682931
4.744973	394.137064	5.687936
5.228416	394.861736	5.692941
5.085855	391.675910	5.697946
5.205631	384.775769	5.702950
4.808461	394.481338	5.707955
5.227629	402.727031	5.712960
5.161348	406.353651	5.717965
4.901624	412.785268	5.722970
5.496010	404.978667	5.727974
5.259975	404.303753	5.732979
5.405896	411.307745	5.737984
5.277442	410.967161	5.742989
5.349873	406.004373	5.747994
5.532954	410.234182	5.752998
5.375113	417.257295	5.758003
5.258469	409.147634	5.763008
5.394566	412.878592	5.768013
5.475498	412.976614	5.773018
5.596856	405.484579	5.778022
5.344075	417.094315	5.783027
5.265123	415.217840	5.788032
5.565903	412.184017	5.793037
5.749380	410.266425	5.798042
5.781408	413.706796	5.803046
5.456906	415.810940	5.808051
5.462435	416.768685	5.813056
5.492492	417.510610	5.818061
5.639809	418.079135	5.823066
5.624453	418.606706	5.828070
5.530681	418.950406	5.833075
5.573846	412.539998	5.838080
5.495466	413.159704	5.843085
5.132863	409.423041	5.848090
5.725419	407.422372	5.853094
5.732972	404.545227	5.858099
5.455913	406.445778	5.863104
5.716069	408.828485	5.868109
5.628317	412.768527	5.873114
5.867483	406.365377	5.878118
5.587183	411.961801	5.883123
5.778125	407.967561	5.888128
5.951331	410.098129	5.893133
5.997834	408.151378	5.898138
6.152118	407.855082	5.903142
5.630212	410.401454	5.908147
5.895302	408.917176	5.913152
5.633076	404.712359	5.918157
5.842423	403.752521	5.923162
6.052320	403.618359	5.928166
5.645287	408.196900	5.933171
5.665083	411.468340	5.938176
5.635011	411.438217	5.943181
5.670691	413.786492	5.948186
5.796640	411.893732	5.953190
5.351570	411.574282	5.958195
5.736179	417.180427	5.963200
5.765406	420.652877	5.968205
5.976445	432.588594	5.973210
6.156250	433.088752	5.978214
5.773594	418.901894	5.983219
5.860316	418.774376	5.988224
6.347877	424.551058	5.993229
5.833663	414.924930	5.998234
5.891206	413.390911	6.003238
5.784115	413.167206	6.008243
5.708657	403.443864	6.013248
6.298858	417.936659	6.018253
5.754868	415.168076	6.023258
6.164608	403.502047	6.028262
5.835262	409.723102	6.033267
5.991204	408.895022	6.038272
6.084814	408.272866	6.043277
6.012898	401.747612	6.048282
6.167861	397.736864	6.053286
5.813693	407.331296	6.058291
5.672734	406.938886	6.063296
5.722195	408.500369	6.068301
5.557588	418.131546	6.073306
5.808943	421.622978	6.078310
5.996121	434.154073	6.083315
5.989840	424.457847	6.088320
5.896099	429.449226	6.093325
6.333442	430.269711	6.098330
6.216851	420.767946	6.103334
5.831204	413.206645	6.108339
5.810903	420.625836	6.113344
5.932380	405.398193	6.118349
5.556309	423.241029	6.123354
6.259096	412.636424	6.128358
5.893252	414.307271	6.133363
5.882469	409.759327	6.138368
5.947623	405.642424	6.143373
5.789205	417.246866	6.148378
5.903111	412.233283	6.153382
5.877392	418.492193	6.158387
6.132748	423.837010	6.163392
6.312053	411.843238	6.168397
5.909932	415.164966	6.173402
6.099925	404.071220	6.178406
5.697086	403.261086	6.183411
5.807178	400.950022	6.188416
5.829747	402.743513	6.193421
5.726401	408.097070	6.198426
6.000853	408.879798	6.203430
5.664624	426.941028	6.208435
5.752005	426.351486	6.213440
6.084373	433.405369	6.218445
5.699547	435.126650	6.223450
6.130241	434.034051	6.228454
6.102633	430.789078	6.233459
6.208954	423.381651	6.238464
6.068397	412.330199	6.243469
5.767044	412.690604	6.248474
6.053953	402.698509	6.253478
6.189509	413.725364	6.258483
5.820775	406.395540	6.263488
6.060787	397.230231	6.268493
5.896852	404.659265	6.273498
6.118637	404.741545	6.278502
6.027749	407.884790	6.283507
6.120246	409.059869	6.288512
6.126051	410.109322	6.293517
5.699451	411.191723	6.298522
6.072433	403.422976	6.303526
5.980927	411.872076	6.308531
5.910117	408.061220	6.313536
6.037222	405.997433	6.318541
5.771249	403.504840	6.323546
6.061340	409.426356	6.328550
5.836276	409.942491	6.333555
5.676454	405.718464	6.338560
5.687641	399.214992	6.343565
5.720040	405.341402	6.348570
6.266305	406.170130	6.353574
6.166265	408.979442	6.358579
5.964293	407.653768	6.363584
5.893641	403.741646	6.368589
5.709668	408.190322	6.373594
5.876345	405.598301	6.378598
5.550304	407.781781	6.383603
5.981625	401.791463	6.388608
6.003298	392.097203	6.393613
5.786635	404.302400	6.398618
6.391030	398.547564	6.403622
5.683140	406.757871	6.408627
5.393014	402.231550	6.413632
5.657510	403.006347	6.418637
5.820069	419.575183	6.423642
5.962919	432.935822	6.428646
6.213033	435.054343	6.433651
6.367081	423.020228	6.438656
6.292512	414.945102	6.443661
5.935004	419.224812	6.448666
5.931301	410.369771	6.453670
5.372430	406.303183	6.458675
6.093126	397.366287	6.463680
5.744801	408.557541	6.468685
5.841597	406.919294	6.473690
6.228759	405.064704	6.478694
6.055438	413.485494	6.483699
5.645994	407.247246	6.488704
6.089377	405.839440	6.493709
5.884146	405.890547	6.498714
6.207523	406.934536	6.503718
6.002464	405.141098	6.508723
5.912158	402.836122	6.513728
5.755275	397.017063	6.518733
5.882507	406.482282	6.523738
6.199732	404.192549	6.528742
5.926077	403.779801	6.533747
6.265844	402.676139	6.538752
6.425527	398.651997	6.543757
6.194619	406.999547	6.548762
6.091383	401.634001	6.553766
5.987267	405.741125	6.558771
5.768202	412.039818	6.563776
6.023440	403.482740	6.568781
6.069286	401.779708	6.573786
6.096247	406.356689	6.578790
5.830260	409.460928	6.583795
6.059509	401.898205	6.588800
5.944354	402.378136	6.593805
5.674882	410.953199	6.598810
6.156854	402.629523	6.603814
6.000493	407.333307	6.608819
6.004556	412.293538	6.613824
6.104892	407.003665	6.618829
6.145609	411.917024	6.623834
6.412185	403.604949	6.628838
6.179076	397.076478	6.633843
5.894801	392.628338	6.638848
6.388652	382.825299	6.643853
5.537807	388.830656	6.648858
5.995234	375.828363	6.653862
6.077910	378.438195	6.658867
5.970215	391.417268	6.663872
5.842958	383.755383	6.668877
5.908023	390.740396	6.673882
5.763759	389.674608	6.678886
5.708165	386.921258	6.683891
5.944033	385.827549	6.688896
5.809374	387.614036	6.693901
5.680918	393.917508	6.698906
5.676594	389.090140	6.703910
5.768416	393.115940	6.708915
6.006244	397.957281	6.713920
6.197630	407.855386	6.718925
5.990271	396.953619	6.723930
6.027349	396.292864	6.728934
5.746690	384.826771	6.733939
5.656317	388.011061	6.738944
6.135237	393.716320	6.743949
6.042716	401.624558	6.748954
6.275953	397.013073	6.753958
5.707257	391.815374	6.758963
5.843914	383.286377	6.763968
5.828174	381.156387	6.768973
5.554129	391.165373	6.773978
6.183688	389.491111	6.778982
6.031510	408.108794	6.783987
6.069503	392.549384	6.788992
6.073278	391.659722	6.793997
5.505962	385.417743	6.799002
5.974333	396.370294	6.804006
6.088904	393.884519	6.809011
5.887655	385.541345	6.814016
5.918695	386.460290	6.819021
5.548431	394.617691	6.824026
5.918507	384.947942	6.829030
5.823383	407.059051	6.834035
5.589456	405.165729	6.839040
5.899890	411.530160	6.844045
5.934767	413.555848	6.849050
5.871852	399.739698	6.854054
5.761808	394.495447	6.859059
5.498674	412.244646	6.864064
5.732841	407.484312	6.869069
5.475426	406.085065	6.874074
6.119005	401.004315	6.879078
5.986170	409.640228	6.884083
6.159512	411.713826	6.889088
5.938478	402.883349	6.894093
5.882416	414.348363	6.899098
6.059573	407.290522	6.904102
5.814941	409.670060	6.909107
5.935361	415.836468	6.914112
5.791728	405.367649	6.919117
5.795538	416.832774	6.924122
6.087049	409.418485	6.929126
5.821481	408.042662	6.934131
5.413258	412.216418	6.939136
5.973762	402.773094	6.944141
5.678565	402.604173	6.949146
6.127575	407.722485	6.954150
5.341876	414.321937	6.959155
6.003269	421.811495	6.964160
6.206307	422.972418	6.969165
6.043824	413.357622	6.974170
6.102991	408.362108	6.979174
5.967145	408.452965	6.984179
5.746196	399.881911	6.989184
5.702288	399.676782	6.994189
5.830726	421.509265	6.999194
5.899940	421.482569	7.004198
6.010338	424.986596	7.009203
6.294926	426.492257	7.014208
5.806661	410.167376	7.019213
5.666108	410.246315	7.024218
5.984501	410.762724	7.029222
6.119506	428.459049	7.034227
5.771766	426.055196	7.039232
6.046674	423.999888	7.044237
6.037987	422.969804	7.049242
5.812095	412.931496	7.054246
6.029191	411.897676	7.059251
5.901382	424.617326	7.064256
5.811746	412.618235	7.069261
5.713586	433.518101	7.074266
6.023218	429.919724	7.079270
6.270488	433.443436	7.084275
6.161654	420.852545	7.089280
6.320083	412.266337	7.094285
5.984418	407.775624	7.099290
6.079321	403.711009	7.104294
6.137154	417.233657	7.109299
5.988710	410.388187	7.114304
6.149612	403.282273	7.119309
5.988951	411.017689	7.124314
5.885194	404.981490	7.129318
6.168736	407.721210	7.134323
5.886416	406.218295	7.139328
6.250266	415.643282	7.144333
5.864983	418.490960	7.149338
6.602474	404.457646	7.154342
6.158677	405.017544	7.159347
5.888790	398.140485	7.164352
5.562342	391.712064	7.169357
6.041742	402.242100	7.174362
6.202293	397.765394	7.179366
6.204072	391.013455	7.184371
6.015970	393.649897	7.189376
6.090681	389.268901	7.194381
6.036042	385.034727	7.199386
5.844325	382.049599	7.204390
5.821070	379.310166	7.209395
5.888615	381.764178	7.214400
6.019054	382.458735	7.219405
5.652182	388.116173	7.224410
5.822550	381.356807	7.229414
5.856223	383.433302	7.234419
5.735437	389.820995	7.239424
6.226571	383.308771	7.244429
6.089302	391.600512	7.249434
6.135609	383.835500	7.254438
6.005810	380.612875	7.259443
5.719275	381.328470	7.264448
6.185242	384.450903	7.269453
5.661338	387.994192	7.274458
5.572878	379.639677	7.279462
5.731775	387.040269	7.284467
5.962638	397.027098	7.289472
6.216476	404.767172	7.294477
5.932758	397.275331	7.299482
5.905848	391.992745	7.304486
5.817543	387.184863	7.309491
5.601887	382.381116	7.314496
5.903912	394.853060	7.319501
5.768354	395.010312	7.324506
5.856189	398.869055	7.329510
5.947808	409.298498	7.334515
5.745983	410.250766	7.339520
5.525916	400.986692	7.344525
5.868933	401.736531	7.349530
6.120165	406.974418	7.354534
5.842939	409.207198	7.359539
5.725445	410.937213	7.364544
6.147822	392.419499	7.369549
5.886077	407.817746	7.374554
6.235094	400.853206	7.379558
6.182852	404.461807	7.384563
5.877087	413.004591	7.389568
5.799081	408.805711	7.394573
5.816800	413.017137	7.399578
5.568675	407.386381	7.404582
5.716650	401.927690	7.409587
5.484516	402.017814	7.414592
6.306286	394.865307	7.419597
6.120858	405.436235	7.424602
5.964076	406.482688	7.429606
6.039047	406.081757	7.434611
5.713936	405.974472	7.439616
6.375958	407.496927	7.444621
5.758872	414.250299	7.449626
6.016190	411.172663	7.454630
5.990913	408.193091	7.459635
5.754234	407.948561	7.464640
5.931012	399.935303	7.469645
5.927096	406.288872	7.474650
6.075523	410.422869	7.479654
5.907449	408.563522	7.484659
5.994279	403.506727	7.489664
6.238329	402.117498	7.494669
6.054899	402.051291	7.499674
6.274285	407.360608	7.504678
6.316457	408.293629	7.509683
5.643663	407.791554	7.514688
5.871734	389.946547	7.519693
5.759979	406.333719	7.524698
6.173871	410.141377	7.529702
5.965662	412.290576	7.534707
5.611799	416.351409	7.539712
5.984932	406.136989	7.544717
5.608348	412.580588	7.549722
5.836206	405.872318	7.554726
5.915090	413.497435	7.559731
5.659692	409.560472	7.564736
5.714117	403.980393	7.569741
6.005321	408.104674	7.574746
5.991483	408.166923	7.579750
5.852328	409.520670	7.584755
6.057515	414.095040	7.589760
5.697534	416.894459	7.594765
5.981468	411.139209	7.599770
6.062043	411.525196	7.604774
5.971258	409.533514	7.609779
5.930649	408.941879	7.614784
6.057074	406.954131	7.619789
5.568195	409.852842	7.624794
5.917177	413.025247	7.629798
5.969446	412.184936	7.634803
5.888268	416.256829	7.639808
6.260079	406.975949	7.644813
5.964903	415.118431	7.649818
5.915961	415.768327	7.654822
6.014308	411.671532	7.659827
5.910890	413.525895	7.664832
5.906347	403.566809	7.669837
5.797752	417.273725	7.674842
5.447990	420.416403	7.679846
5.690366	415.303594	7.684851
5.617447	416.567868	7.689856
5.773612	410.152411	7.694861
5.370097	413.050403	7.699866
5.744746	431.506471	7.704870
5.899504	435.617335	7.709875
5.824325	444.829542	7.714880
5.976711	444.043147	7.719885
5.479030	439.698037	7.724890
5.699826	443.899799	7.729894
6.068389	429.332631	7.734899
5.700393	433.379864	7.739904
6.118848	443.270886	7.744909
6.040032	445.191001	7.749914
6.114985	437.541704	7.754918
6.125694	437.992424	7.759923
5.517776	438.837472	7.764928
5.692455	439.949055	7.769933
6.049863	445.977099	7.774938
5.495433	436.240197	7.779942
6.131513	443.376216	7.784947
6.101916	441.109180	7.789952
5.716198	438.616360	7.794957
6.192340	448.593262	7.799962
6.392677	446.375624	7.804966
6.256139	441.850539	7.809971
5.891980	443.366096	7.814976
6.266150	438.577491	7.819981
5.952637	440.123079	7.824986
5.871781	437.338877	7.829990
5.575932	424.764629	7.834995
5.738736	441.915595	7.840000
5.958928	440.900271	7.845005
5.623714	450.074128	7.850010
5.825167	447.979704	7.855014
6.360893	442.896858	7.860019
6.192226	442.008901	7.865024
6.149610	442.645152	7.870029
6.226633	444.566161	7.875034
5.887732	428.768370	7.880038
5.715065	418.101606	7.885043
6.139535	421.531112	7.890048
5.914041	419.051157	7.895053
5.680529	427.680706	7.900058
6.012083	432.934490	7.905062
6.098187	435.970913	7.910067
5.510424	431.851896	7.915072
5.938598	431.942970	7.920077
5.661478	443.173710	7.925082
5.992948	442.811686	7.930086
5.882523	444.970879	7.935091
5.285386	442.890845	7.940096
5.540527	445.024399	7.945101
5.855959	444.604775	7.950106
5.893110	442.941067	7.955110
6.097551	452.862463	7.960115
5.955686	452.353132	7.965120
5.863413	450.554674	7.970125
6.073453	447.087692	7.975142
5.710800	443.597390	7.980160
5.893840	439.911137	7.985178
5.748484	441.338199	7.990195
6.282054	439.553604	7.995213
6.350484	451.209749	8.000230
5.960111	443.545544	8.005248
5.805497	436.993105	8.010266
5.916210	449.974360	8.015283
6.281912	438.215418	8.020301
5.730560	439.702936	8.025318
5.761821	437.880280	8.030336
6.045147	444.510318	8.035354
5.846413	449.278242	8.040371
5.899795	442.314518	8.045389
5.711289	446.282428	8.050406
5.814120	443.192560	8.055424
5.408888	446.661101	8.060442
5.461942	466.846570	8.065459
6.218618	465.197429	8.070477
6.505456	466.727188	8.075494
6.176651	470.322613	8.080512
6.199040	462.953486	8.085530
6.042872	460.576376	8.090547
6.306908	437.201172	8.095565
5.930100	453.259956	8.100582
6.211271	438.775045	8.105600
6.390766	438.122046	8.110618
6.309321	445.052231	8.115635
6.254274	439.569777	8.120653
6.166175	442.717232	8.125670
6.029845	445.105391	8.130688
5.786711	443.164783	8.135706
6.061958	443.733845	8.140723
6.180953	442.929381	8.145741
5.772861	451.261419	8.150758
5.997054	443.257929	8.155776
6.136617	434.008548	8.160794
6.193598	442.280337	8.165811
5.880319	442.174757	8.170829
6.032971	451.403539	8.175846
6.139350	456.603337	8.180864
6.535622	462.761254	8.185882
6.006109	450.268417	8.190899
5.967866	449.210880	8.195917
5.928121	449.662040	8.200934
6.002555	462.983501	8.205952
6.216480	469.321467	8.210970
6.295368	471.385577	8.215987
5.961875	463.204371	8.221005
6.140832	480.290091	8.226022
6.220980	477.910665	8.231040
6.872038	470.417789	8.236058
6.416922	461.687599	8.241075
6.319158	447.839560	8.246093
6.066175	447.008172	8.251110
6.231578	442.914431	8.256128
6.141120	438.598850	8.261146
6.034922	446.321858	8.266163
5.998588	454.693479	8.271181
6.139579	467.373360	8.276198
6.119914	467.193374	8.281216
6.241532	462.213404	8.286234
6.476644	471.258864	8.291251
6.725895	472.542050	8.296269
5.973087	462.425780	8.301286
6.033230	466.938554	8.306304
6.411723	471.262596	8.311322
6.108523	474.500563	8.316339
6.228376	478.177170	8.321357
6.283163	483.359813	8.326374
6.019688	482.785685	8.331392
6.398730	471.267627	8.336410
6.453805	479.293581	8.341427
6.275323	479.024870	8.346445
5.973765	477.910760	8.351462
6.191009	472.694899	8.356480
6.128326	471.161512	8.361498
5.683559	476.349841	8.366515
6.278657	483.341296	8.371533
6.052040	479.561431	8.376550
5.937946	475.726068	8.381568
6.598794	473.435538	8.386586
6.200120	496.901247	8.391603
6.204316	496.433501	8.396621
6.674300	508.152998	8.401638
6.272226	496.965591	8.406656
6.718655	489.987603	8.411674
6.252461	490.593942	8.416691
6.287837	495.710203	8.421709
6.302274	489.715077	8.426726
6.232775	502.882396	8.431744
6.497535	513.314933	8.436762
6.169122	509.074488	8.441779
6.536654	510.534804	8.446797
6.418463	512.970622	8.451814
6.799865	512.759354	8.456832
6.883764	503.947846	8.461850
6.557646	489.346607	8.466867
6.388671	485.661850	8.471885
6.209598	489.353739	8.476902
6.270524	494.008407	8.481920
6.592706	492.370537	8.486938
6.545137	505.051586	8.491955
6.661430	489.355400	8.496973
6.565228	477.937045	8.501990
6.430546	487.286604	8.507008
6.609560	482.894078	8.512026
6.351378	485.408630	8.517043
6.374153	486.241312	8.522061
6.210485	484.120992	8.527078
6.485978	505.350931	8.532096
6.380401	499.652314	8.537114
6.560150	510.669367	8.542131
6.520334	505.919804	8.547149
6.806147	505.442648	8.552166
6.548356	510.592224	8.557184
6.434738	511.572508	8.562202
6.363005	516.386823	8.567219
6.611077	508.275421	8.572237
6.376838	509.694324	8.577255
6.087198	520.854354	8.582272
6.512068	517.464709	8.587290
6.566808	509.920081	8.592307
6.182877	511.378217	8.597325
6.405928	515.275347	8.602343
5.941533	513.994245	8.607360
6.440940	514.727002	8.612378
6.519248	530.130726	8.617395
6.728252	533.705014	8.622413
7.106366	528.318766	8.627431
6.947738	529.151470	8.632448
6.614805	514.292504	8.637466
6.444575	519.100161	8.642483
6.374451	516.636979	8.647501
6.399859	508.999118	8.652519
6.771224	522.239386	8.657536
6.917508	536.300722	8.662554
6.605284	513.141941	8.667571
6.505933	515.928256	8.672589
6.760173	523.471747	8.677607
6.375470	531.386749	8.682624
6.879666	537.502536	8.687642
6.922220	535.315185	8.692659
6.713369	519.076627	8.697677
6.766079	507.900008	8.702695
6.501424	518.232462	8.707712
6.803219	524.891194	8.712730
6.716089	525.031045	8.717747
6.492001	526.233765	8.722765
6.956059	532.927036	8.727783
6.633106	537.850145	8.732800
7.070313	530.728420	8.737818
6.973663	526.830352	8.742835
6.854090	527.328735	8.747853
6.971951	525.161144	8.752871
6.948332	520.068215	8.757888
6.690371	517.864835	8.762906
6.517579	523.310364	8.767923
6.759111	518.021257	8.772941
6.850220	517.438909	8.777959
6.528128	525.126349	8.782976
6.633345	513.420794	8.787994
6.797882	527.940008	8.793011
6.715422	542.882941	8.798029
7.098429	541.601607	8.803047
6.529842	539.948665	8.808064
6.953914	542.214319	8.813082
6.854434	535.003112	8.818099
6.723892	543.765075	8.823117
6.976034	551.444606	8.828135
6.877784	547.755066	8.833152
6.852514	543.186251	8.838170
7.093201	540.017962	8.843187
6.750780	545.843524	8.848205
6.918601	542.042871	8.853223
6.873018	542.204614	8.858240
6.742119	542.919366	8.863258
6.642956	545.544711	8.868275
6.614028	537.609240	8.873293
6.703936	535.793164	8.878311
6.618555	545.469543	8.883328
6.848002	542.984666	8.888346
6.936254	534.440703	8.893363
6.887077	545.850250	8.898381
7.036384	543.822897	8.903399
6.690079	541.178922	8.908416
7.106038	531.681059	8.913434
6.627007	542.362695	8.918451
6.659989	538.378042	8.923469
6.970330	533.074994	8.928487
6.707339	540.933061	8.933504
6.815878	550.358153	8.938522
6.918702	560.317475	8.943539
6.542532	571.465849	8.948557
7.225265	566.006615	8.953575
6.598447	569.494118	8.958592
7.145660	569.061210	8.963610
6.949995	562.988526	8.968627
6.751487	579.480232	8.973645
7.109278	569.016322	8.978663
6.769304	566.103109	8.983680
6.836968	564.334697	8.988698
7.155929	567.431018	8.993715
6.726764	577.091851	8.998733
7.384437	567.057481	9.003751
6.899543	571.513668	9.008768
6.943445	565.561237	9.013786
6.951750	565.635643	9.018803
6.882902	564.892162	9.023821
6.690510	564.666655	9.028839
6.733781	586.898749	9.033856
7.343524	596.870185	9.038874
7.471816	589.440232	9.043891
7.442964	598.445064	9.048909
7.179979	580.435061	9.053927
7.140190	575.846421	9.058944
6.991485	579.909109	9.063962
7.101260	576.606692	9.068979
7.042726	578.739683	9.073997
7.178935	573.422881	9.079015
7.154938	592.803214	9.084032
7.025755	596.922808	9.089050
7.295253	596.599684	9.094067
7.057562	604.494840	9.099085
7.554739	598.584988	9.104103
7.239282	597.914859	9.109120
7.464614	586.569133	9.114138
7.293948	570.879966	9.119155
6.954812	570.134654	9.124173
7.092283	571.908731	9.129191
7.167046	578.805026	9.134208
7.178958	597.731614	9.139226
7.242531	606.494751	9.144243
7.394165	609.431105	9.149261
7.365108	593.419930	9.154279
7.298454	587.219726	9.159296
6.821692	592.078587	9.164314
7.076754	590.287122	9.169331
6.983608	605.234936	9.174349
7.254054	594.254521	9.179367
7.411760	606.199736	9.184384
7.526149	597.089916	9.189402
7.298389	600.505433	9.194419
7.433447	608.389525	9.199437
7.464451	594.259265	9.204455
7.023570	595.303454	9.209472
6.923287	596.534117	9.214490
7.495722	597.365889	9.219507
7.384397	599.314650	9.224525
7.537228	598.574305	9.229543
7.539578	600.088690	9.234560
7.322019	603.401624	9.239578
7.602055	593.113983	9.244595
7.577082	607.394712	9.249613
7.539359	601.877936	9.254631
7.441232	605.636060	9.259648
7.062067	618.283938	9.264666
7.343582	599.481702	9.269683
7.039503	607.251562	9.274701
7.530292	603.646445	9.279719
7.373218	604.576739	9.284736
7.388775	606.597139	9.289754
7.430776	606.584214	9.294771
7.089959	611.765762	9.299789
7.071083	600.392018	9.304807
7.402684	601.072177	9.309824
7.234957	604.503535	9.314842
7.283900	606.632313	9.319859
6.943752	607.269399	9.324877
7.193694	614.008872	9.329895
7.643407	622.686270	9.334912
7.645685	634.813647	9.339930
7.847762	627.671919	9.344947
7.466761	620.489008	9.349965
7.596288	612.938931	9.354983
7.361704	605.004095	9.360000
7.290167	608.783300	9.365018
8.054587	616.660305	9.370035
7.632431	617.000972	9.375053
7.554301	606.617963	9.380071
7.325147	605.558771	9.385088
6.988275	609.900257	9.390106
7.388720	617.117923	9.395123
7.595973	628.683005	9.400141
7.587272	626.017680	9.405159
7.887420	621.445194	9.410176
7.806786	621.410459	9.415194
7.886383	617.784558	9.420211
7.625425	614.095252	9.425229
7.548103	612.138113	9.430247
7.551415	607.454350	9.435264
7.349245	624.218070	9.440282
7.743634	623.679718	9.445299
7.730352	628.680564	9.450317
7.630295	622.195248	9.455335
7.986596	625.184743	9.460352
7.003216	624.723406	9.465370
7.370650	630.444086	9.470387
7.453170	630.800354	9.475405
7.700937	626.078284	9.480423
7.523336	627.677670	9.485440
7.773911	633.366168	9.490458
7.728273	634.705038	9.495475
7.398074	641.510172	9.500493
7.664306	641.736670	9.505511
7.707033	635.143770	9.510528
7.622254	631.436325	9.515546
7.440444	632.692388	9.520563
7.800376	641.453290	9.525581
7.731888	636.357890	9.530599
8.012704	628.998697	9.535616
7.340368	632.707939	9.540634
7.757926	629.631844	9.545651
7.690354	638.301935	9.550669
7.876761	628.953596	9.555687
8.000448	628.811108	9.560704
7.557777	632.364446	9.565722
7.874429	618.927870	9.570739
7.886068	628.999347	9.575757
8.088580	625.903297	9.580775
8.175927	636.262718	9.585792
7.835641	629.054489	9.590810
7.814708	633.545294	9.595827
7.567943	635.657291	9.600845
7.780360	634.544691	9.605863
8.030621	634.877833	9.610880
7.521374	637.826220	9.615898
7.760401	625.370635	9.620915
7.970907	642.609357	9.625933
7.511355	639.541298	9.630951
7.853621	640.686847	9.635968
7.984505	658.840621	9.640986
7.882074	657.531196	9.646003
8.234368	663.194299	9.651021
8.109914	656.785376	9.656039
8.162508	637.081693	9.661056
7.940577	632.045050	9.666074
8.091361	637.963779	9.671091
8.089086	640.179481	9.676109
7.952363	636.088852	9.681127
8.002666	628.232446	9.686144
7.821832	636.724623	9.691162
7.915826	632.935517	9.696179
7.989606	635.388611	9.701197
7.927691	627.401464	9.706215
8.088510	630.771883	9.711232
8.087097	638.529048	9.716250
8.303613	639.047358	9.721267
8.036711	638.057195	9.726285
7.809799	639.563323	9.731303
8.077953	641.929158	9.736320
7.962681	636.601247	9.741338
8.142083	634.641752	9.746355
7.825116	638.058630	9.751373
7.475254	641.670011	9.756391
8.275353	646.991546	9.761408
8.059621	663.956244	9.766426
8.289988	658.138669	9.771443
8.115105	651.737650	9.776461
8.056480	652.769286	9.781479
8.411447	645.395313	9.786496
7.915714	646.953028	9.791514
7.780923	643.483789	9.796531
7.991389	656.743055	9.801549
8.144392	659.291037	9.806567
8.029792	651.551976	9.811584
8.012988	653.981396	9.816602
8.115361	658.219358	9.821619
8.224506	660.240880	9.826637
8.220042	666.193410	9.831655
8.325721	661.897537	9.836672
8.277152	668.245144	9.841690
8.124422	660.698246	9.846707
8.119598	671.217296	9.851725
8.082346	668.177740	9.856743
8.134682	661.169914	9.861760
8.033048	674.717936	9.866778
8.012699	667.358577	9.871795
8.102415	661.013927	9.876813
8.006888	667.050154	9.881831
8.552816	650.819450	9.886848
8.442412	656.693901	9.891866
8.297632	654.400188	9.896883
8.435338	657.414471	9.901901
8.140924	654.184835	9.906919
8.642721	651.433209	9.911936
8.223680	664.557583	9.916954
8.123720	666.637115	9.921971
8.203941	657.062401	9.926989
8.300283	663.750220	9.932007
8.285864	658.630563	9.937024
8.179617	660.679521	9.942042
8.167187	660.343764	9.947059
8.058238	662.241667	9.952077
8.188486	659.232673	9.957095
8.508382	647.430278	9.962112
7.978387	667.726262	9.967130
8.394558	671.915061	9.972147
8.159821	664.283180	9.977165
8.392472	683.172117	9.982183
8.749343	684.170213	9.987200
8.666840	678.259641	9.992218
8.355083	669.330162	9.997235
8.600112	670.087003	10.002253
7.988991	663.965769	10.007271
8.382689	672.074454	10.012288
8.488694	686.571410	10.017306
8.401252	685.196519	10.022323
8.528754	687.253037	10.027341
8.362675	683.968575	10.032359
8.660954	684.205832	10.037376
8.457311	692.802595	10.042394
8.348554	685.980946	10.047411
8.427437	690.408790	10.052429
8.550686	690.929092	10.057447
8.696507	690.963017	10.062464
8.479836	684.164589	10.067482
8.900200	676.335386	10.072499
8.681697	663.585386	10.077517
8.480728	661.278385	10.082535
8.560602	661.158540	10.087552
8.264692	657.073913	10.092570
8.173903	672.649421	10.097587
8.574174	678.510139	10.102605
8.856835	689.899344	10.107623
8.706121	684.728450	10.112640
8.698054	681.864201	10.117658
8.798601	683.773463	10.122675
9.038810	668.531077	10.127693
8.429069	670.756754	10.132711
8.586899	663.012873	10.137728
8.143722	673.341829	10.142746
8.050177	680.327650	10.147763
8.366902	679.353339	10.152781
8.449580	684.736798	10.157799
8.470206	690.508680	10.162816
8.247616	686.788101	10.167834
8.607454	687.621630	10.172851
8.645380	691.484687	10.177869
8.851441	693.042902	10.182887
8.641757	684.876909	10.187904
8.784850	687.161359	10.192922
8.847335	682.291579	10.197939
8.932597	692.335778	10.202957
8.746664	689.442590	10.207975
8.768662	681.789412	10.212992
8.732029	693.749355	10.218010
8.802988	680.692057	10.223027
8.898616	680.471913	10.228045
8.775800	681.043392	10.233063
8.744283	691.531922	10.238080
8.698961	682.838403	10.243098
8.827958	677.418559	10.248115
9.033031	677.749314	10.253133
9.037762	683.687787	10.258151
9.061073	681.954715	10.263168
9.209087	680.167391	10.268186
9.016921	691.236515	10.273203
9.060673	684.943240	10.278221
8.653671	691.937152	10.283239
8.957491	684.937251	10.288256
9.091527	681.192355	10.293274
8.730292	684.682450	10.298291
8.734680	683.189029	10.303309
8.686382	686.002085	10.308327
8.730547	679.951745	10.313344
8.844314	680.634479	10.318362
9.004184	688.467382	10.323379
8.713925	691.668645	10.328397
8.779486	702.012583	10.333415
8.920036	684.384219	10.338432
9.153052	682.031308	10.343450
8.649423	683.779612	10.348467
8.823410	686.453699	10.353485
8.739696	691.083744	10.358503
9.002262	688.391686	10.363520
8.977210	682.958107	10.368538
8.641830	687.943164	10.373555
9.201504	695.075953	10.378573
9.378940	710.726234	10.383591
9.035612	694.852571	10.388608
8.865061	691.751846	10.393626
8.614242	690.001763	10.398643
9.037286	690.702312	10.403661
9.267072	707.631961	10.408679
9.105575	712.488795	10.413696
9.190225	712.860510	10.418714
8.815696	716.870249	10.423731
9.047099	705.779118	10.428749
9.098329	711.666133	10.433767
9.185993	717.762037	10.438784
9.441140	710.037602	10.443802
9.253407	698.564019	10.448819
9.336202	698.585728	10.453837
9.198309	685.507501	10.458855
9.051500	689.620410	10.463872
9.037427	684.879389	10.468890
9.196321	698.509686	10.473907
9.278650	701.813521	10.478925
9.381798	689.335000	10.483943
8.993720	683.690055	10.488960
8.898304	681.382291	10.493978
9.064299	696.194905	10.498995
9.372863	706.633316	10.504013
9.127331	701.786544	10.509031
9.138052	700.446765	10.514048
9.249617	705.961405	10.519066
9.192403	715.494606	10.524083
9.325990	711.793955	10.529101
9.512999	717.697568	10.534119
9.430365	716.321921	10.539136
9.515437	709.652932	10.544154
9.165532	703.301407	10.549171
9.423446	700.297650	10.554189
9.545551	713.151079	10.559207
9.070571	697.553663	10.564224
9.620501	701.529007	10.569242
8.888356	701.558481	10.574259
9.314009	708.794325	10.579277
9.313056	709.864266	10.584295
9.118927	712.678085	10.589312
9.473883	707.254386	10.594330
9.237052	713.423221	10.599347
9.656204	714.004460	10.604365
9.206424	712.749454	10.609383
9.472096	715.383933	10.614400
9.205614	711.840640	10.619418
9.092329	712.151849	10.624435
9.241554	705.378135	10.629453
9.278704	709.086683	10.634471
9.459542	719.639789	10.639488
9.248455	723.251533	10.644506
9.252474	711.384979	10.649523
9.722825	709.354643	10.654541
9.243984	711.307349	10.659559
9.467421	716.362650	10.664576
9.357997	708.950958	10.669594
9.542481	719.052209	10.674611
9.744639	704.273349	10.679629
9.831222	711.035298	10.684647
9.617015	710.204133	10.689664
9.593123	708.434273	10.694682
9.608532	716.949389	10.699699
9.509761	701.479219	10.704717
9.487256	709.328082	10.709735
9.574662	710.384179	10.714752
9.722914	707.694249	10.719770
9.742226	714.599285	10.724787
9.460780	710.001136	10.729805
9.450251	712.700981	10.734823
9.776927	710.633195	10.739840
9.444408	717.798485	10.744858
9.387252	715.036596	10.749875
9.787630	712.569096	10.754893
9.848871	704.632046	10.759911
9.633792	711.526468	10.764928
9.492014	705.577836	10.769946
9.320076	707.599222	10.774963
9.495372	705.305845	10.779981
9.321260	727.701562	10.784999
9.391763	726.453401	10.790016
9.870203	730.465199	10.795034
9.730430	730.761623	10.800051
10.108380	730.418349	10.805069
9.676165	730.568089	10.810087
9.736984	737.577083	10.815104
9.706804	733.640153	10.820122
9.332777	734.721212	10.825139
9.550021	727.589691	10.830157
9.407045	739.206563	10.835175
10.040886	735.616877	10.840192
10.140097	729.728309	10.845210
9.851159	732.635881	10.850227
9.766529	726.488939	10.855245
9.779694	738.210735	10.860263
10.010610	739.206478	10.865280
9.995528	731.353959	10.870298
9.986869	739.074433	10.875315
10.113148	738.451853	10.880333
9.835852	733.243973	10.885351
9.866254	727.157903	10.890368
10.003558	728.414467	10.895386
9.846835	732.270162	10.900403
9.972634	727.693409	10.905421
9.874676	736.450360	10.910439
9.912047	742.279596	10.915456
10.274577	736.879948	10.920474
10.217627	734.348399	10.925491
10.138192	726.357641	10.930509
9.762648	707.822343	10.935527
9.762565	724.245224	10.940544
10.216424	719.516085	10.945562
9.938631	726.199431	10.950579
10.017423	722.475805	10.955597
10.008231	730.407799	10.960615
9.747032	732.108656	10.965632
9.946130	731.783937	10.970650
9.955127	737.952134	10.975667
10.443030	731.374656	10.980685
10.080321	738.020818	10.985703
9.883874	735.429074	10.990720
10.173445	739.410505	10.995738
10.083317	730.799723	11.000755
9.953958	732.274794	11.005773
10.009271	728.289757	11.010791
9.799176	736.966448	11.015808
10.113165	723.094707	11.020826
9.667662	728.668234	11.025843
9.880920	730.152740	11.030861
10.180633	727.738880	11.035879
9.886239	738.779869	11.040896
10.128313	731.133213	11.045914
10.006703	736.984201	11.050931
10.075349	737.525682	11.055949
10.357263	735.029403	11.060967
9.815106	734.341139	11.065984
10.279269	737.635648	11.071002
10.176477	743.669883	11.076019
10.025456	750.863554	11.081037
10.339706	756.983930	11.086055
10.565934	759.236429	11.091072
10.338688	746.661310	11.096090
10.236956	743.309950	11.101107
10.384597	739.064289	11.106125
10.005012	742.926502	11.111143
10.324359	747.824771	11.116160
10.296326	751.773917	11.121178
10.485377	752.741506	11.126195
10.629921	756.827716	11.131213
10.209475	746.899051	11.136231
10.322984	742.756567	11.141248
10.410101	734.562984	11.146266
10.252101	734.347865	11.151283
10.376415	733.381607	11.156301
10.466553	725.556786	11.161319
10.173761	745.784135	11.166336
10.566075	740.218872	11.171354
10.664218	743.091045	11.176371
10.281473	735.750568	11.181389
10.727244	739.934746	11.186407
10.258815	737.085813	11.191424
10.688870	741.291388	11.196442
10.374707	737.383173	11.201459
10.239048	739.278957	11.206477
10.200437	740.878667	11.211495
10.103866	758.613741	11.216512
10.714930	756.138471	11.221530
11.001161	763.598156	11.226547
10.642102	747.345056	11.231565
10.503168	740.193597	11.236583
10.399432	733.797180	11.241600
10.550487	747.725390	11.246618
10.523096	749.320187	11.251635
10.593046	758.581021	11.256653
11.007643	758.449757	11.261671
10.620679	754.417244	11.266688
10.693974	743.312992	11.271706
10.988579	733.597349	11.276723
10.467264	738.015102	11.281741
10.636926	726.053156	11.286759
10.628715	733.732532	11.291776
10.463406	730.826639	11.296794
10.284620	735.430566	11.301811
10.495898	743.012440	11.306829
10.370753	751.230856	11.311847
10.738072	759.971724	11.316864
10.987735	754.245770	11.321882
10.979732	754.029240	11.326899
10.481062	750.336124	11.331917
10.574808	753.884335	11.336935
10.600074	765.762044	11.341952
10.583515	755.735378	11.346970
10.561215	753.132125	11.351987
10.380131	761.690672	11.357005
10.673634	756.743650	11.362023
10.311073	756.469062	11.367040
10.657250	757.068048	11.372058
10.614482	759.075513	11.377075
10.626280	751.736329	11.382093
10.626392	762.854267	11.387111
10.771268	766.918337	11.392128
10.891653	771.674216	11.397146
11.141433	775.115931	11.402163
10.636169	772.430555	11.407181
10.815122	768.167358	11.412199
10.916191	784.634406	11.417216
10.693261	788.210149	11.422234
10.903533	780.284430	11.427251
10.881225	787.098183	11.432269
11.073107	786.465323	11.437287
11.117105	784.381858	11.442304
11.197267	781.765703	11.447322
11.145544	770.059323	11.452339
10.623678	765.536699	11.457357
10.802988	756.713273	11.462375
11.018420	771.373035	11.467392
10.791757	777.502430	11.472410
11.076155	777.517799	11.477427
11.018909	777.498334	11.482445
11.094219	776.467168	11.487463
11.091971	787.604426	11.492480
10.872119	779.897579	11.497498
10.865527	776.644916	11.502515
10.994661	785.271635	11.507533
10.939510	778.498357	11.512551
10.689763	781.863704	11.517568
11.104119	783.285148	11.522586
11.154695	777.874405	11.527603
11.386619	774.079437	11.532621
11.211933	774.542280	11.537639
11.286543	777.689547	11.542656
11.492039	775.041132	11.547674
11.293689	773.260730	11.552691
10.857276	782.443121	11.557709
11.039304	780.363277	11.562727
11.428591	779.147216	11.567744
11.076626	782.462306	11.572762
11.136424	781.900634	11.577779
10.972006	774.860452	11.582797
11.305297	773.242907	11.587815
11.155152	780.606867	11.592832
11.119270	787.432215	11.597850
11.419294	775.427721	11.602867
11.104178	784.960341	11.607885
11.154777	779.290815	11.612903
11.238268	776.854022	11.617920
10.999373	773.899690	11.622938
11.095630	778.836078	11.627955
11.132916	777.141833	11.632973
11.456262	780.458414	11.637991
11.586291	782.808040	11.643008
11.413741	777.930877	11.648026
11.426771	769.408056	11.653043
11.230399	774.996212	11.658061
11.298758	769.917203	11.663079
11.450510	782.879647	11.668096
11.183802	783.202272	11.673114
11.371849	775.068596	11.678131
11.142868	777.285121	11.683149
11.427053	781.573522	11.688167
11.615004	796.496389	11.693184
11.707996	792.792615	11.698202
11.624281	784.815124	11.703219
11.697436	776.128244	11.708237
11.541779	768.446057	11.713255
11.571879	774.929700	11.718272
11.217644	777.228967	11.723290
11.422778	777.657546	11.728307
11.232107	780.388782	11.733325
11.437079	768.960923	11.738343
11.432564	794.249295	11.743360
11.870988	802.448863	11.748378
11.869665	782.037092	11.753395
11.469379	777.293443	11.758413
11.330232	774.626443	11.763431
11.735570	786.820160	11.768448
11.299390	790.618666	11.773466
11.774882	789.641565	11.778483
12.039766	797.918814	11.783501
11.751925	780.461619	11.788519
11.494646	780.514521	11.793536
11.489762	773.632382	11.798554
11.786689	771.455640	11.803571
11.556083	779.700061	11.808589
11.457227	795.166485	11.813607
11.808499	794.767430	11.818624
11.398024	798.438832	11.823642
11.859546	805.101046	11.828659
11.814207	800.071401	11.833677
11.903047	797.406546	11.838695
12.016266	800.898065	11.843712
12.115889	798.035859	11.848730
11.831036	782.080373	11.853747
11.612678	784.418312	11.858765
11.578572	785.768009	11.863783
11.637867	788.135030	11.868800
11.797675	801.011018	11.873818
12.213210	801.144697	11.878835
11.934620	805.997811	11.883853
11.835321	793.077561	11.888871
11.876529	796.788648	11.893888
11.747543	799.226196	11.898906
11.878881	797.889602	11.903923
11.777226	807.628633	11.908941
12.062398	792.211837	11.913959
12.039486	798.309315	11.918976
12.276543	803.482428	11.923994
12.009099	787.110795	11.929011
11.752376	785.623562	11.934029
11.938796	795.487866	11.939047
12.281539	797.832568	11.944064
11.768618	794.643454	11.949082
11.873103	791.458592	11.954099
11.711690	797.852328	11.959117
11.771575	792.200277	11.964135
12.059012	801.954082	11.969152
11.756052	805.760121	11.974170
11.919690	795.806186	11.979187
12.027382	809.924277	11.984205
11.846930	798.840813	11.989223
12.067077	800.441012	11.994240
11.703314	801.283778	11.999258
12.178850	793.808802	12.004275
11.854174	801.304259	12.009293
11.846559	805.439567	12.014311
12.313249	809.033498	12.019328
12.164020	819.477430	12.024346
12.438987	812.718688	12.029363
12.053924	807.227867	12.034381
12.044656	806.124744	12.039399
12.163425	818.174032	12.044416
12.157033	826.702084	12.049434
12.303372	828.484266	12.054451
12.363317	825.489415	12.059469
12.154235	824.016805	12.064487
12.004453	823.601579	12.069504
12.119966	822.078112	12.074522
12.262225	815.138189	12.079539
12.525813	822.377381	12.084557
12.121448	819.594137	12.089575
12.448929	827.463957	12.094592
12.201631	817.381889	12.099610
12.550341	816.554040	12.104627
12.735819	819.545086	12.109645
12.590284	818.113014	12.114663
12.583533	815.179108	12.119680
12.623924	800.226697	12.124698
12.487071	787.198725	12.129715
12.132285	793.162004	12.134733
11.994686	795.518850	12.139751
12.787212	802.564707	12.144768
12.468233	812.766985	12.149786
12.689974	806.051299	12.154803
12.292503	801.442903	12.159821
12.221954	803.457882	12.164839
12.495217	813.781964	12.169856
12.218664	825.243094	12.174874
12.431843	819.626978	12.179891
12.697291	823.785780	12.184909
12.360589	832.255133	12.189927
12.850079	828.927890	12.194944
12.247140	831.199858	12.199962
12.707517	827.763566	12.204979
12.754683	822.122966	12.209997
12.769209	818.942726	12.215015
12.914061	819.854128	12.220032
12.525447	823.171812	12.225050
12.748649	821.012927	12.230067
12.726914	814.928685	12.235085
12.579157	825.205129	12.240103
12.295035	814.197860	12.245120
12.262611	825.005350	12.250138
12.494163	814.479024	12.255155
12.735308	820.449929	12.260173
12.726713	823.982630	12.265191
12.919777	818.211874	12.270208
12.917089	816.126253	12.275226
12.811695	816.890668	12.280243
12.590685	818.118171	12.285261
12.367903	824.815025	12.290279
12.863418	812.000384	12.295296
12.280541	824.576181	12.300314
12.605406	818.661697	12.305331
12.633465	819.184294	12.310349
12.539925	820.385514	12.315367
13.093047	825.477554	12.320384
12.890217	833.935400	12.325402
12.870818	829.160462	12.330419
13.004056	828.511541	12.335437
12.785045	826.169475	12.340455
13.032103	831.000198	12.345472
12.632038	822.819789	12.350490
13.199467	834.126598	12.355507
13.165245	840.194304	12.360525
12.759890	830.200110	12.365543
13.337577	830.178994	12.370560
12.900582	825.772446	12.375578
12.880231	821.833957	12.380595
12.822705	819.169941	12.385613
12.981573	836.918720	12.390631
13.372267	833.322929	12.395648
13.023581	838.193347	12.400666
12.733729	835.654093	12.405683
13.029663	836.535512	12.410701
13.036806	842.565178	12.415719
13.265551	844.706839	12.420736
13.106153	842.153457	12.425754
13.060433	841.516796	12.430771
13.209164	835.525760	12.435789
12.987971	831.991125	12.440807
13.058977	834.012331	12.445824
13.075027	846.374382	12.450842
13.382481	844.729320	12.455859
13.200153	836.113998	12.460877
12.964625	839.881076	12.465895
13.283219	840.313970	12.470912
13.100591	834.434813	12.475930
12.900643	842.043290	12.480947
13.072706	843.660494	12.485965
12.731798	852.420854	12.490983
13.339139	844.372932	12.496000
13.218621	845.471082	12.501018
12.980646	843.236127	12.506035
13.067535	839.773143	12.511053
12.929998	845.636129	12.516071
13.269804	850.439702	12.521088
13.522315	865.090576	12.526106
13.500763	865.264336	12.531123
13.798532	864.400285	12.536141
13.596160	848.008932	12.541159
13.584688	836.782203	12.546176
13.658909	838.357931	12.551194
13.560099	837.278303	12.556211
13.530732	824.662657	12.561229
13.239979	835.034097	12.566247
13.308966	838.314800	12.571264
13.297837	840.292071	12.576282
13.299675	839.411270	12.581299
13.434219	840.210677	12.586317
13.157639	839.117876	12.591335
13.572869	849.912048	12.596352
13.506001	861.015294	12.601370
13.574543	865.829815	12.606387
14.064114	856.575871	12.611405
13.639638	861.101559	12.616423
13.781074	844.271328	12.621440
13.529629	840.769835	12.626458
13.473159	839.197572	12.631475
13.614303	832.996284	12.636493
13.573223	849.147989	12.641511
13.719316	853.773628	12.646528
13.821577	859.952502	12.651546
13.747349	853.724990	12.656563
13.922680	840.474494	12.661581
13.295763	842.617675	12.666599
13.646304	849.243644	12.671616
13.917498	863.282511	12.676634
13.566045	862.147790	12.681651
14.095923	853.903715	12.686669
13.812693	854.784359	12.691687
13.404066	842.783552	12.696704
13.885532	855.293597	12.701722
13.869609	857.457815	12.706739
14.216840	861.089409	12.711757
13.639753	855.666529	12.716775
13.861079	853.416415	12.721792
14.150127	856.107214	12.726810
13.970578	851.546713	12.731827
14.017444	836.037828	12.736845
13.653281	836.817541	12.741863
13.757109	838.151942	12.746880
13.647869	846.607754	12.751898
13.651000	856.175757	12.756915
14.036980	857.737355	12.761933
14.112032	858.505058	12.766951
13.727023	859.095532	12.771968
13.913136	859.751159	12.776986
13.903973	854.804194	12.782003
14.218119	851.529666	12.787021
14.128984	863.576845	12.792039
14.063491	858.042250	12.797056
14.088077	858.887288	12.802074
13.837546	865.522232	12.807091
13.889737	863.936099	12.812109
14.110410	865.129116	12.817127
14.125538	861.387034	12.822144
13.989745	853.928920	12.827162
14.005228	861.229092	12.832179
14.136787	861.590305	12.837197
14.186635	864.476376	12.842215
13.913253	851.854761	12.847232
14.578613	847.651037	12.852250
14.180055	863.798803	12.857267
14.602693	859.140793	12.862285
14.115320	860.612007	12.867303
14.231897	859.527033	12.872320
14.085833	863.425268	12.877338
14.301172	858.405257	12.882355
14.518874	858.276440	12.887373
14.014650	860.116372	12.892391
14.347353	862.462657	12.897408
14.385344	858.294109	12.902426
14.014547	858.023965	12.907443
14.332255	856.386763	12.912461
14.170051	861.581424	12.917479
14.182079	854.851240	12.922496
14.339374	853.526354	12.927514
14.068103	855.487580	12.932531
14.288505	859.145356	12.937549
14.414351	877.129726	12.942567
14.278069	876.633487	12.947584
14.631029	880.134798	12.952602
14.518201	884.012050	12.957619
14.393439	874.365194	12.962637
14.313412	874.608077	12.967655
14.675371	878.486679	12.972672
14.594352	878.575081	12.977690
14.787351	874.221295	12.982707
14.910641	870.822030	12.987725
14.592611	855.187261	12.992743
14.290668	855.670044	12.997760
14.613047	861.359989	13.002778
14.769806	875.637704	13.007795
14.655324	865.515864	13.012813
14.215560	865.357513	13.017831
14.625656	876.808923	13.022848
14.680843	879.059833	13.027866
14.465322	878.493957	13.032883
14.777736	875.907672	13.037901
14.600091	876.086954	13.042919
14.606692	884.269010	13.047936
14.903021	879.450902	13.052954
14.784096	880.138543	13.057971
15.020261	878.769740	13.062989
14.782978	884.332781	13.068007
14.873637	883.374945	13.073024
14.811258	888.064815	13.078042
14.752789	884.933871	13.083059
14.766407	871.819144	13.088077
14.817787	876.554305	13.093095
14.975074	878.666140	13.098112
15.243517	874.707638	13.103130
15.337089	879.035395	13.108147
14.891472	860.665554	13.113165
14.576816	859.651301	13.118183
14.762623	874.593505	13.123200
14.976102	883.980240	13.128218
14.520604	876.613234	13.133235
14.879031	880.078973	13.138253
14.804006	879.718306	13.143271
15.073840	871.694850	13.148288
15.207181	873.835683	13.153306
14.629849	877.230283	13.158323
14.774186	873.830876	13.163341
14.920418	885.017516	13.168359
15.083682	884.363889	13.173376
15.090948	881.601348	13.178394
14.956921	890.483949	13.183411
15.064781	878.414818	13.188429
15.054537	876.055814	13.193447
14.764682	882.917835	13.198464
14.949184	881.026943	13.203482
15.192163	904.064442	13.208499
15.340379	906.370209	13.213517
15.257470	901.690410	13.218535
15.021460	894.879151	13.223552
15.196628	896.271808	13.228570
15.471967	903.736415	13.233587
15.435964	888.792742	13.238605
15.214843	879.766904	13.243623
15.077082	882.227930	13.248640
15.296264	886.406619	13.253658
15.018339	895.261274	13.258675
15.560178	893.017742	13.263693
15.695926	892.482037	13.268711
15.312369	895.505447	13.273728
15.502297	887.251504	13.278746
15.241446	889.949570	13.283763
15.427953	888.323454	13.288781
15.608207	898.135132	13.293799
15.346621	897.816317	13.298816
15.198288	890.009853	13.303834
15.261025	902.588693	13.308851
15.279089	893.402295	13.313869
15.171450	903.353757	13.318887
15.069131	902.880599	13.323904
15.576495	898.859410	13.328922
15.524097	912.220014	13.333939
15.491517	899.406000	13.338957
15.609566	897.942090	13.343975
15.768625	910.827742	13.348992
15.836025	904.679009	13.354010
15.660314	903.977505	13.359027
15.968260	894.733063	13.364045
15.669340	896.859574	13.369063
15.594160	904.713621	13.374080
15.661884	901.976318	13.379098
15.637059	901.431057	13.384115
15.253427	896.056751	13.389133
15.762862	897.725244	13.394151
15.818171	899.303941	13.399168
15.593938	894.150817	13.404186
15.565460	899.201458	13.409203
15.280582	900.167570	13.414221
15.553019	898.477496	13.419239
15.603960	914.135152	13.424256
15.882576	913.763257	13.429274
15.603155	915.353374	13.434291
15.597156	920.744488	13.439309
16.134775	919.467307	13.444327
15.911896	925.280573	13.449344
15.998482	920.930824	13.454362
15.811303	925.217373	13.459379
16.005935	919.948120	13.464397
16.246594	916.003430	13.469415
15.845521	914.311581	13.474432
16.183064	907.628208	13.479450
15.791281	908.295484	13.484467
16.140119	909.364281	13.489485
16.397032	901.544811	13.494503
15.873089	900.717985	13.499520
16.176469	899.537467	13.504538
15.744227	893.302918	13.509555
15.600816	890.822763	13.514573
16.019715	906.470098	13.519591
15.839209	920.488263	13.524608
16.323836	918.569278	13.529626
16.249473	914.961128	13.534643
16.314606	923.815697	13.539661
16.212397	917.993341	13.544679
16.032005	919.602657	13.549696
15.885144	914.835043	13.554714
16.289485	916.863993	13.559731
16.110930	923.986306	13.564749
16.325637	916.817238	13.569767
16.133677	920.621688	13.574784
16.388376	917.870868	13.579802
16.255027	922.830647	13.584819
16.316769	926.289230	13.589837
16.379719	915.792417	13.594855
16.234251	917.853861	13.599872
16.175613	914.419976	13.604890
16.314152	917.490978	13.609907
16.321383	922.277250	13.614925
16.375228	928.495292	13.619943
15.946428	926.915086	13.624960
16.412002	923.572637	13.629978
16.168006	922.900766	13.634995
16.044092	923.308319	13.640013
16.271899	920.280840	13.645031
16.603900	943.484326	13.650048
16.586421	939.570608	13.655066
16.809553	934.997486	13.660083
16.859659	928.608454	13.665101
16.697268	918.787585	13.670119
16.567107	919.934588	13.675136
16.765791	911.051246	13.680154
16.729690	919.382022	13.685171
16.596618	920.794573	13.690189
16.394253	903.955036	13.695207
16.279844	923.387763	13.700224
16.606001	916.185454	13.705242
16.837500	917.099064	13.710259
16.706620	919.899849	13.715277
16.627146	920.101620	13.720295
16.339629	926.341587	13.725312
16.265490	927.628139	13.730330
16.787157	929.196886	13.735347
16.712710	936.653194	13.740365
16.812428	930.186959	13.745383
16.482502	937.910517	13.750400
16.803401	944.001514	13.755418
16.738076	940.265709	13.760435
16.766821	945.187474	13.765453
17.099452	944.056020	13.770471
17.094494	938.818034	13.775488
16.999625	941.603712	13.780506
17.238273	944.034173	13.785523
17.257722	944.898956	13.790541
16.944444	924.453847	13.795559
16.798775	937.172665	13.800576
17.223606	940.959377	13.805594
16.797888	936.844530	13.810611
17.093397	940.083449	13.815629
17.200080	935.926212	13.820647
17.126993	940.876554	13.825664
16.956815	935.730728	13.830682
16.893819	927.336510	13.835699
17.020253	934.960162	13.840717
17.264105	938.308163	13.845735
16.895607	937.703136	13.850752
17.026979	937.587845	13.855770
17.051816	936.009146	13.860787
17.087676	942.299440	13.865805
17.105541	934.791970	13.870823
16.901313	938.771918	13.875840
17.261637	929.904267	13.880858
17.517691	927.011219	13.885875
17.209072	935.495156	13.890893
17.352508	944.586780	13.895911
16.931177	945.157700	13.900928
16.935114	934.310354	13.905946
17.154752	940.571852	13.910963
16.940976	942.066479	13.915981
17.372157	943.198117	13.920999
17.090080	952.659377	13.926016
17.441064	952.001582	13.931034
17.534022	959.911362	13.936051
17.372761	964.067624	13.941069
17.560000	958.417659	13.946087
17.879927	957.909900	13.951104
17.535036	953.252200	13.956122
17.835364	943.223117	13.961139
17.646653	940.099945	13.966157
17.354739	934.190540	13.971175
17.206102	937.031980	13.976192
17.341129	931.958259	13.981210
17.383588	944.281525	13.986227
17.599109	953.008402	13.991245
17.573321	959.302049	13.996263
17.563161	953.143361	14.001280
17.493678	955.798830	14.006298
17.701452	965.918663	14.011315
17.847388	952.915692	14.016333
17.916397	953.807424	14.021351
17.945062	958.460957	14.026368
17.800773	949.615554	14.031386
17.968381	934.295952	14.036403
17.540726	936.613054	14.041421
17.821702	946.699316	14.046439
17.884358	942.561599	14.051456
17.691117	942.301504	14.056474
17.935843	943.474980	14.061491
17.803802	947.740271	14.066509
17.754970	948.410622	14.071527
17.861097	954.128166	14.076544
17.890770	954.202382	14.081562
18.031154	950.806735	14.086579
17.732357	953.962045	14.091597
18.059339	964.132629	14.096615
18.196993	953.163333	14.101632
18.355719	945.993556	14.106650
18.047174	936.164019	14.111667
17.643249	939.313706	14.116685
17.697476	947.545134	14.121703
17.919535	947.898481	14.126720
17.901344	947.118645	14.131738
18.436576	941.224810	14.136755
18.132967	952.507220	14.141773
17.910084	962.170653	14.146791
18.351519	953.268191	14.151808
18.021743	950.858254	14.156826
18.095233	948.770149	14.161843
17.951507	956.960013	14.166861
18.307128	953.871476	14.171879
18.141340	957.037505	14.176896
18.109451	955.234159	14.181914
17.736104	954.920230	14.186931
17.841425	953.915911	14.191949
17.864400	957.342704	14.196967
17.729541	953.355854	14.201984
17.903899	969.622238	14.207002
18.493353	970.031633	14.212019
18.263388	976.335185	14.217037
18.647981	977.912791	14.222055
18.302979	983.088789	14.227072
18.242706	980.784948	14.232090
18.423380	971.812877	14.237107
18.455418	972.928159	14.242125
18.159497	975.243560	14.247143
18.652638	975.967853	14.252160
18.844300	978.569786	14.257178
18.789493	974.949092	14.262195
18.620090	973.807931	14.267213
18.578346	977.396350	14.272231
18.963609	972.718920	14.277248
18.446599	970.619188	14.282266
18.704453	976.950453	14.287283
18.693990	972.038374	14.292301
18.907351	971.840807	14.297319
18.621963	960.353953	14.302336
18.338501	951.640809	14.307354
18.622185	964.645832	14.312371
18.791249	971.202449	14.317389
18.687728	968.854892	14.322407
18.761792	975.237044	14.327424
18.429302	977.397226	14.332442
19.197240	972.988049	14.337459
18.698984	971.200965	14.342477
18.952137	972.830723	14.347495
18.956405	965.808218	14.352512
18.734597	979.302714	14.357530
19.282683	969.929089	14.362547
18.838355	969.263357	14.367565
18.814721	977.658480	14.372583
18.918301	968.597502	14.377600
18.742513	971.891335	14.382618
19.119525	965.555213	14.387635
19.086507	970.922172	14.392653
18.859322	968.032247	14.397671
18.666027	973.433786	14.402688
18.498911	973.273742	14.407706
19.253621	968.825612	14.412723
18.734120	979.611679	14.417741
18.745021	971.717113	14.422759
18.865366	972.717570	14.427776
18.892795	976.424541	14.432794
19.302731	964.711974	14.437811
18.803904	975.390656	14.442829
18.611339	983.392520	14.447847
19.634273	987.170740	14.452864
19.063419	999.164096	14.457882
19.329726	989.872480	14.462899
19.347313	992.110360	14.467917
19.247640	1000.015624	14.472935
19.439768	998.265539	14.477952
19.003047	997.769031	14.482970
18.944682	992.078640	14.487987
19.398300	992.149549	14.493005
19.133630	989.653665	14.498023
19.540784	990.558693	14.503040
19.384336	998.974635	14.508058
19.565133	996.598307	14.513075
19.432900	998.039136	14.518093
19.572468	992.219900	14.523111
19.393267	984.389828	14.528128
19.532529	989.650903	14.533146
19.881669	988.204428	14.538163
19.876873	993.541726	14.543181
19.578322	997.694259	14.548199
19.643841	986.761492	14.553216
19.258845	1000.552977	14.558234
19.797468	990.022619	14.563251
19.675173	995.734939	14.568269
19.478587	987.415273	14.573287
19.624893	993.975465	14.578304
19.431382	995.107151	14.583322
19.619069	990.915118	14.588339
19.532353	992.778013	14.593357
19.670023	990.967032	14.598375
19.680750	976.154823	14.603392
19.687502	990.661266	14.608410
19.803262	989.506983	14.613427
19.831352	987.407052	14.618445
19.810484	992.835231	14.623463
19.956028	983.609877	14.628480
19.714009	999.916279	14.633498
20.354243	993.652518	14.638515
20.068287	987.997786	14.643533
19.662897	995.565932	14.648551
19.873374	987.889403	14.653568
19.802065	989.923456	14.658586
19.886163	987.347681	14.663603
19.945624	983.832161	14.668621
19.825996	982.711603	14.673639
20.165447	985.473422	14.678656
20.087975	992.352702	14.683674
20.007675	984.163144	14.688691
19.990821	987.331090	14.693709
19.870514	981.587290	14.698727
19.885369	987.151884	14.703744
19.723696	1005.591696	14.708762
20.096027	1010.330255	14.713779
19.962166	1007.974823	14.718797
20.146150	1017.388342	14.723815
20.220883	1002.345171	14.728832
20.011920	1018.138316	14.733850
20.506396	1018.767726	14.738867
20.127281	1013.313779	14.743885
20.180388	1014.599335	14.748903
20.287612	1004.448991	14.753920
20.202217	1011.575678	14.758938
20.160550	1010.095757	14.763955
20.301497	1016.476912	14.768973
20.167839	1009.655885	14.773991
20.501943	999.179656	14.779008
20.137785	1013.387617	14.784026
20.079078	1022.053350	14.789043
20.567337	1032.552163	14.794061
20.524857	1037.185304	14.799079
20.650999	1036.423877	14.804096
21.010430	1041.751460	14.809114
20.870110	1025.602692	14.814131
20.863697	1013.018031	14.819149
20.430310	1004.350442	14.824167
20.653699	996.495157	14.829184
20.659970	1000.423204	14.834202
20.812095	1005.817971	14.839219
20.615886	1004.649449	14.844237
20.649000	1008.955152	14.849255
20.902246	1005.062119	14.854272
20.461479	1013.292237	14.859290
20.265565	1015.595131	14.864307
20.837213	1015.732756	14.869325
20.779142	1032.101888	14.874343
21.118827	1030.338148	14.879360
20.669706	1017.239010	14.884378
20.769480	1023.699203	14.889395
21.177346	1017.203592	14.894413
20.886396	1023.885953	14.899431
20.804134	1015.343230	14.904448
20.933693	1021.423206	14.909466
20.856651	1023.597020	14.914483
21.028758	1026.848979	14.919501
20.842876	1034.515295	14.924519
21.104666	1022.295715	14.929536
21.009842	1032.254709	14.934554
21.157161	1028.883209	14.939571
21.090658	1028.783140	14.944589
21.287079	1034.691696	14.949607
21.220259	1021.333836	14.954624
21.042270	1030.949246	14.959642
21.054450	1024.342054	14.964659
21.195708	1028.179527	14.969677
21.227774	1038.213320	14.974695
21.516885	1033.535160	14.979712
21.148968	1024.914110	14.984730
20.927186	1026.384750	14.989747
20.963425	1026.789304	14.994765
20.828290	1032.538363	14.999783
20.676946	1021.342900	15.004800
21.189996	1031.837828	15.009818
21.196660	1032.843477	15.014835
21.336161	1041.263564	15.019853
21.405463	1046.059080	15.024871
21.293484	1051.649878	15.029888
21.439575	1056.291350	15.034906
21.624547	1057.534158	15.039923
21.810655	1052.016887	15.044941
21.852954	1049.277234	15.049959
21.306671	1024.936289	15.054976
21.426063	1032.974507	15.059994
21.606674	1035.672856	15.065011
21.629568	1036.272009	15.070029
21.532173	1051.157745	15.075047
21.904585	1048.902870	15.080064
21.770760	1045.404998	15.085082
21.515090	1034.519369	15.090099
21.519880	1038.204653	15.095117
21.528814	1046.424289	15.100135
21.774500	1049.320732	15.105152
21.737833	1055.149047	15.110170
21.730626	1060.177465	15.115187
21.750674	1047.023732	15.120205
21.720095	1041.742391	15.125223
21.824328	1032.447743	15.130240
21.708955	1043.757524	15.135258
21.680426	1045.702828	15.140275
21.784574	1046.194575	15.145293
22.164127	1046.753627	15.150311
21.826387	1033.760105	15.155328
21.816679	1042.295092	15.160346
21.670220	1043.766556	15.165363
22.147491	1041.204912	15.170381
21.920364	1057.209225	15.175399
22.250411	1043.956429	15.180416
22.090746	1051.110548	15.185434
21.857009	1050.632729	15.190451
22.554868	1042.813540	15.195469
22.076551	1045.362660	15.200487
22.410737	1039.645464	15.205504
22.104927	1047.624073	15.210522
22.305681	1060.039385	15.215539
22.231515	1048.339495	15.220557
22.191762	1049.440782	15.225575
22.009439	1047.850349	15.230592
22.208877	1043.880530	15.235610
22.026757	1049.147795	15.240627
22.568191	1041.558247	15.245645
22.292338	1042.403029	15.250663
22.659615	1048.284819	15.255680
22.591677	1046.136809	15.260698
22.616548	1053.467149	15.265715
22.123315	1046.743471	15.270733
22.203070	1043.025940	15.275751
22.158522	1041.966200	15.280768
22.651151	1054.632431	15.285786
22.585492	1059.894075	15.290803
22.524651	1042.271665	15.295821
22.235959	1047.637679	15.300839
22.639665	1068.914475	15.305856
22.669656	1072.841976	15.310874
22.836291	1068.877291	15.315891
22.920288	1064.370119	15.320909
22.579755	1063.583977	15.325927
22.643620	1058.953725	15.330944
23.083395	1067.926396	15.335962
22.761088	1061.671407	15.340979
23.078068	1045.280554	15.345997
22.221621	1045.291630	15.351015
22.533945	1057.228701	15.356032
23.049328	1071.829091	15.361050
22.792214	1065.750083	15.366067
23.195688	1064.626458	15.371085
23.162749	1076.033799	15.376103
22.968032	1048.797441	15.381120
22.796226	1053.094235	15.386138
22.845237	1065.564885	15.391155
22.996903	1055.000440	15.396173
23.224291	1073.341493	15.401191
23.134215	1064.184573	15.406208
23.173387	1055.307216	15.411226
22.953056	1068.400751	15.416243
23.007011	1060.726623	15.421261
23.077462	1064.294325	15.426279
22.977082	1072.114523	15.431296
23.064553	1072.198618	15.436314
22.790091	1078.165186	15.441331
23.072043	1069.647426	15.446349
22.863528	1078.554414	15.451367
22.636095	1067.818979	15.456384
23.359969	1071.438942	15.461402
23.144185	1066.893530	15.466419
23.061591	1062.431395	15.471437
23.088787	1074.299540	15.476455
23.377179	1085.811180	15.481472
23.523153	1088.338234	15.486490
23.167692	1091.764384	15.491507
23.571360	1085.341991	15.496525
23.510973	1087.749895	15.501543
23.333097	1089.655486	15.506560
23.703257	1086.356360	15.511578
23.136424	1088.572208	15.516595
23.550524	1086.714751	15.521613
23.458150	1088.991963	15.526631
23.528522	1089.085050	15.531648
23.454573	1081.222664	15.536666
23.835882	1088.320442	15.541683
23.678788	1085.627804	15.546701
23.885895	1084.702206	15.551719
23.665776	1085.191110	15.556736
23.763534	1073.675710	15.561754
23.494516	1089.907528	15.566771
23.592844	1086.868749	15.571789
23.717224	1088.566032	15.576807
23.929345	1084.663647	15.581824
24.151955	1079.655058	15.586842
23.668826	1088.829146	15.591859
23.849769	1079.755990	15.596877
23.784047	1077.449835	15.601895
24.001416	1081.856078	15.606912
24.293253	1077.291092	15.611930
23.962272	1080.688157	15.616947
24.322573	1077.235939	15.621965
24.008678	1076.590793	15.626983
23.944535	1077.749553	15.632000
24.138901	1076.235802	15.637018
23.865861	1078.714893	15.642035
24.191225	1079.749509	15.647053
23.982124	1077.860303	15.652071
23.844510	1080.655857	15.657088
24.116297	1080.717386	15.662106
24.272106	1087.724259	15.667123
24.016616	1080.745563	15.672141
23.985872	1077.076896	15.677159
24.397584	1095.168179	15.682176
24.432367	1092.076238	15.687194
24.413649	1102.818631	15.692211
24.583668	1093.586230	15.697229
24.440742	1084.566971	15.702247
24.073237	1079.597192	15.707264
24.191965	1079.351333	15.712282
24.369587	1099.786252	15.717299
24.556625	1093.697607	15.722317
24.666098	1105.338281	15.727335
24.908299	1096.621602	15.732352
24.621711	1089.439487	15.737370
24.588561	1095.283043	15.742387
24.568633	1094.557123	15.747405
24.727916	1104.873986	15.752423
24.456477	1093.463758	15.757440
24.564570	1092.051887	15.762458
24.611506	1101.834071	15.767475
24.754882	1107.211304	15.772493
24.529750	1099.347351	15.777511
24.336787	1096.594057	15.782528
24.459089	1101.166683	15.787546
24.594151	1114.195101	15.792563
24.718595	1104.228200	15.797581
24.642209	1098.247100	15.802599
24.715079	1099.327589	15.807616
24.890362	1096.021124	15.812634
24.074838	1109.902239	15.817651
24.633408	1110.149215	15.822669
25.142570	1119.893703	15.827687
25.236443	1123.202119	15.832704
25.525098	1123.295720	15.837722
25.312351	1125.490809	15.842739
25.572573	1113.429206	15.847757
25.467073	1102.851375	15.852775
25.090735	1093.534159	15.857792
25.373661	1089.484975	15.862810
25.092631	1099.820330	15.867827
25.393567	1102.061168	15.872845
24.940404	1094.674769	15.877863
24.957523	1089.729933	15.882880
25.109937	1093.057574	15.887898
25.472268	1100.508634	15.892915
25.417726	1088.449027	15.897933
25.374357	1087.805677	15.902951
24.956909	1099.806623	15.907968
25.355181	1091.788192	15.912986
25.211563	1098.469589	15.918003
25.156442	1108.296169	15.923021
25.678806	1114.077942	15.928039
25.501535	1120.111349	15.933056
25.791100	1119.879750	15.938074
25.554838	1117.606621	15.943091
25.723305	1112.975746	15.948109
25.636476	1110.357304	15.953127
25.786849	1112.211468	15.958144
25.549509	1096.494414	15.963162
25.494690	1106.784862	15.968179
25.983514	1107.206872	15.973197
25.778297	1094.555470	15.978215
25.725507	1097.795340	15.983232
25.570850	1091.722361	15.988250
25.948764	1104.977818	15.993267
26.194143	1104.866754	15.998285
25.836426	1092.280273	16.003303
25.700870	1097.155238	16.008320
25.769315	1090.204682	16.013338
25.789279	1102.007705	16.018355
25.966867	1115.887863	16.023373
25.878988	1110.243085	16.028391
26.038030	1119.120908	16.033408
25.647859	1112.037066	16.038426
25.946933	1117.150060	16.043443
25.927474	1116.979502	16.048461
25.785539	1110.251254	16.053479
25.515901	1121.733581	16.058496
25.677064	1112.265865	16.063514
25.579328	1116.929776	16.068531
25.228225	1125.736049	16.073549
25.948084	1128.431976	16.078567
25.993504	1128.854030	16.083584
26.113919	1130.365740	16.088602
26.125916	1131.818696	16.093619
25.903739	1140.904586	16.098637
26.301324	1143.240743	16.103655
26.555149	1158.933100	16.108672
26.552336	1150.687142	16.113690
26.355145	1146.555375	16.118707
26.204250	1153.686070	16.123725
26.366873	1149.204428	16.128743
26.260517	1160.853707	16.133760
26.364370	1158.091770	16.138778
26.567177	1151.880710	16.143795
26.461057	1157.072980	16.148813
26.641579	1142.439164	16.153831
26.604692	1148.703057	16.158848
26.702623	1148.384715	16.163866
26.627235	1148.955089	16.168883
26.632237	1154.568618	16.173901
26.904394	1151.761376	16.178919
26.647601	1139.474640	16.183936
26.869442	1135.368743	16.188954
26.998446	1144.065087	16.193971
26.670524	1147.316514	16.198989
26.988720	1135.558247	16.204007
26.912629	1144.157334	16.209024
26.757209	1143.455796	16.214042
26.710490	1144.810652	16.219059
26.976790	1140.470564	16.224077
27.119899	1140.400771	16.229095
26.764745	1144.694755	16.234112
26.839326	1139.576795	16.239130
27.090193	1151.785499	16.244147
27.018834	1145.790971	16.249165
26.977638	1137.169170	16.254183
26.954630	1148.158423	16.259200
27.177654	1149.808698	16.264218
27.269598	1158.472984	16.269235
27.162597	1162.219992	16.274253
27.172391	1172.781230	16.279271
27.150644	1163.724009	16.284288
27.446957	1172.226890	16.289306
27.240685	1170.655978	16.294323
27.311214	1163.171719	16.299341
27.794914	1161.672591	16.304359
27.426027	1171.418974	16.309376
27.554897	1163.288083	16.314394
27.604922	1164.116526	16.319411
27.549034	1153.038572	16.324429
27.583472	1148.286672	16.329447
27.377608	1144.831626	16.334464
27.606766	1152.379315	16.339482
27.728728	1154.430444	16.344499
27.506097	1151.173691	16.349517
27.787143	1145.120793	16.354535
27.859909	1165.859403	16.359552
27.956070	1156.259833	16.364570
27.553022	1140.518209	16.369587
27.491593	1141.376738	16.374605
27.535189	1151.645481	16.379623
27.685149	1155.611010	16.384640
27.626486	1154.783856	16.389658
28.103668	1155.422293	16.394675
27.886271	1153.449170	16.399693
27.830225	1157.216596	16.404711
28.029871	1166.520439	16.409728
28.019121	1151.282247	16.414746
28.031305	1157.491117	16.419763
27.656764	1164.013052	16.424781
27.921824	1155.744058	16.429799
27.676095	1162.996915	16.434816
27.618105	1158.044893	16.439834
27.927038	1160.540113	16.444851
27.920069	1182.831315	16.449869
28.202162	1180.028824	16.454887
28.095072	1188.654880	16.459904
27.947580	1181.498273	16.464922
28.192279	1186.812316	16.469939
27.950401	1190.208065	16.474957
28.134173	1179.973042	16.479975
28.240375	1183.415242	16.484992
28.295140	1174.765764	16.490010
28.353173	1178.811976	16.495027
28.283511	1177.115514	16.500045
28.350454	1180.223026	16.505063
28.302604	1180.208400	16.510080
28.636647	1190.396943	16.515098
28.461369	1180.259203	16.520115
28.380870	1194.040999	16.525133
28.784466	1193.125637	16.530151
28.333731	1203.304598	16.535168
28.648769	1206.414270	16.540186
28.816802	1198.595973	16.545203
28.845907	1217.974976	16.550221
28.909751	1204.416620	16.555239
28.911586	1202.046214	16.560256
28.691688	1193.745883	16.565274
29.009339	1196.119818	16.570291
28.820750	1189.095883	16.575309
29.165512	1199.005032	16.580327
28.836061	1184.580475	16.585344
28.657083	1183.336655	16.590362
28.779532	1183.989646	16.595379
29.000743	1195.253098	16.600397
29.091420	1186.793654	16.605415
28.931561	1205.223919	16.610432
28.728906	1194.920040	16.615450
28.977167	1194.821148	16.620467
28.946977	1207.566247	16.625485
28.871332	1200.313166	16.630503
28.901371	1208.848316	16.635520
28.989022	1196.397116	16.640538
29.000332	1199.011559	16.645555
29.176208	1206.280431	16.650573
29.317348	1214.211178	16.655591
29.634649	1216.859735	16.660608
29.258211	1212.424666	16.665626
29.582150	1212.481181	16.670643
29.387011	1207.231886	16.675661
29.490608	1203.062446	16.680679
29.488289	1209.642848	16.685696
29.668567	1219.861812	16.690714
29.590604	1203.141360	16.695731
29.453808	1210.702228	16.700749
29.876505	1209.840679	16.705767
29.743122	1205.020380	16.710784
29.624435	1189.612869	16.715802
29.633180	1193.723612	16.720819
29.587604	1199.203064	16.725837
29.783910	1201.940007	16.730855
29.695052	1213.419315	16.735872
29.642266	1214.727788	16.740890
29.948918	1210.681172	16.745907
29.833983	1218.112382	16.750925
29.663282	1210.785823	16.755943
29.978205	1211.566454	16.760960
29.984708	1217.381746	16.765978
30.280602	1203.865931	16.770995
30.081396	1211.663802	16.776013
29.985194	1214.752700	16.781031
30.019889	1205.857034	16.786048
30.039564	1216.741808	16.791066
30.363443	1216.492209	16.796083
30.425765	1219.442657	16.801101
30.298205	1213.873493	16.806119
29.984643	1211.259001	16.811136
29.901476	1211.997858	16.816154
29.981354	1207.614376	16.821171
29.737115	1214.232683	16.826189
30.196657	1211.695885	16.831207
30.117720	1209.959847	16.836224
30.121808	1212.913106	16.841242
30.435267	1209.998395	16.846259
30.090049	1214.922020	16.851277
30.395615	1221.596203	16.856295
30.444213	1237.888848	16.861312
30.398084	1235.071500	16.866330
30.705532	1232.425981	16.871347
30.811390	1228.010020	16.876365
30.743528	1229.125190	16.881383
31.008502	1230.652131	16.886400
30.554282	1224.925853	16.891418
30.730604	1209.936021	16.896435
30.355843	1208.341010	16.901453
30.723026	1219.357537	16.906471
30.900333	1228.254645	16.911488
30.554830	1234.175588	16.916506
30.984277	1233.922072	16.921523
30.699551	1223.425901	16.926541
30.626242	1224.961661	16.931559
31.013624	1227.207906	16.936576
30.651981	1225.446730	16.941594
30.957942	1218.083357	16.946611
31.010801	1223.077163	16.951629
30.888356	1221.168053	16.956647
31.204474	1227.682790	16.961664
31.119304	1230.930913	16.966682
31.297727	1222.637590	16.971699
31.415815	1223.894045	16.976717
30.976187	1228.942923	16.981735
31.390114	1223.191083	16.986752
31.171377	1225.172520	16.991770
31.170821	1222.455335	16.996787
31.152775	1224.373769	17.001805
31.284106	1233.975539	17.006823
31.624262	1221.478448	17.011840
31.426102	1228.035889	17.016858
31.254656	1227.538838	17.021875
31.529291	1221.284941	17.026893
31.387767	1224.623946	17.031911
31.490232	1244.944570	17.036928
31.466465	1261.510516	17.041946
32.023402	1250.109259	17.046963
31.461394	1260.362492	17.051981
31.493403	1251.281025	17.056999
31.490973	1252.954010	17.062016
31.312766	1247.171856	17.067034
31.558241	1250.301903	17.072051
31.603764	1251.803267	17.077069
31.534926	1255.938805	17.082087
31.912262	1238.746183	17.087104
31.504097	1253.522982	17.092122
31.728850	1254.718544	17.097139
31.691362	1269.449902	17.102157
32.276465	1280.356582	17.107175
32.441947	1280.425301	17.112192
32.182793	1270.281715	17.117210
32.291327	1262.652599	17.122227
32.104992	1258.380245	17.127245
31.571406	1251.321973	17.132263
32.101840	1264.932362	17.137280
32.332207	1269.645895	17.142298
31.952654	1270.150316	17.147315
32.143306	1272.660929	17.152333
32.373661	1277.185111	17.157351
32.740872	1284.307268	17.162368
32.354321	1275.297680	17.167386
32.813274	1275.235208	17.172403
32.669640	1276.807237	17.177421
32.583890	1274.163355	17.182439
32.768803	1271.697980	17.187456
32.440456	1253.984725	17.192474
32.376668	1243.744270	17.197491
32.683592	1251.342935	17.202509
32.498949	1264.200639	17.207527
32.691496	1258.221532	17.212544
32.397745	1261.066824	17.217562
32.751685	1269.087335	17.222579
32.601507	1270.714040	17.227597
32.448401	1281.827904	17.232615
32.898742	1268.859063	17.237632
32.531950	1279.526706	17.242650
32.936871	1275.764492	17.247667
32.748821	1272.997777	17.252685
32.531749	1280.407143	17.257703
33.092794	1271.268026	17.262720
32.889854	1277.551669	17.267738
33.082126	1268.918472	17.272755
33.234397	1267.629059	17.277773
33.054774	1277.711933	17.282791
33.112663	1270.936536	17.287808
32.958399	1279.879307	17.292826
32.900446	1268.867879	17.297843
33.107227	1259.424498	17.302861
32.926269	1279.227813	17.307879
33.154836	1285.835187	17.312896
33.154165	1289.758072	17.317914
33.249430	1290.718295	17.322931
33.489853	1281.948154	17.327949
33.243281	1292.581189	17.332967
33.461992	1288.980696	17.337984
33.500990	1286.866397	17.343002
33.664776	1291.397857	17.348019
33.130789	1291.756054	17.353037
33.353756	1289.048020	17.358055
33.395030	1278.961504	17.363072
33.169856	1289.537534	17.368090
33.521763	1299.489803	17.373107
33.653660	1306.894999	17.378125
33.523714	1313.359731	17.383143
33.822059	1310.125468	17.388160
33.798273	1306.641863	17.393178
34.041049	1308.765603	17.398195
34.064607	1303.551445	17.403213
34.035221	1305.070862	17.408231
34.420754	1302.267925	17.413248
34.022602	1300.853301	17.418266
33.972134	1316.754425	17.423283
34.125504	1304.936663	17.428301
33.965091	1314.208631	17.433319
34.177063	1306.137240	17.438336
33.987173	1309.398629	17.443354
34.129913	1318.840861	17.448371
34.135095	1313.408664	17.453389
33.943199	1309.569530	17.458407
34.182823	1310.305157	17.463424
33.991740	1312.105538	17.468442
34.461976	1305.940891	17.473459
34.362989	1309.894965	17.478477
34.607925	1313.470094	17.483495
34.633499	1300.804477	17.488512
34.349034	1313.494813	17.493530
34.351148	1309.499045	17.498547
34.732548	1303.209457	17.503565
34.579235	1305.117533	17.508583
34.600348	1300.733768	17.513600
34.713285	1313.579599	17.518618
34.417451	1309.687320	17.523635
34.556772	1308.014909	17.528653
34.312260	1310.678918	17.533671
34.702995	1319.697272	17.538688
35.152800	1324.906636	17.543706
34.863401	1319.896147	17.548723
35.106010	1315.092651	17.553741
34.662291	1313.558928	17.558759
34.883076	1320.132818	17.563776
34.881953	1328.594010	17.568794
35.100237	1332.905495	17.573811
35.186617	1330.480798	17.578829
34.909785	1333.459155	17.583847
34.941566	1324.835297	17.588864
35.109387	1330.275042	17.593882
34.909334	1327.361871	17.598899
35.106163	1335.476458	17.603917
35.446602	1336.530819	17.608935
35.411535	1335.734674	17.613952
35.285044	1328.019273	17.618970
35.329952	1336.309148	17.623987
35.430933	1335.456973	17.629005
34.905102	1335.094340	17.634023
35.152128	1324.448521	17.639040
35.021320	1329.215503	17.644058
35.449656	1334.623901	17.649075
35.544626	1348.356232	17.654093
35.519542	1351.314085	17.659111
35.816328	1344.580129	17.664128
35.402507	1346.503778	17.669146
35.641662	1353.737549	17.674163
35.653273	1346.133052	17.679181
35.703375	1354.933383	17.684199
35.556778	1347.681890	17.689216
35.897143	1352.520228	17.694234
35.722024	1364.060487	17.699251
35.590378	1351.911793	17.704269
35.676714	1353.848602	17.709287
35.830228	1344.309376	17.714304
35.806318	1357.100936	17.719322
35.964580	1368.623680	17.724339
36.121986	1381.645637	17.729357
36.199016	1378.689044	17.734375
36.178452	1378.376640	17.739392
35.938037	1375.192062	17.744410
36.364237	1374.620304	17.749427
36.378900	1370.101827	17.754445
36.184929	1374.468445	17.759463
36.293896	1370.039338	17.764480
36.187078	1369.778319	17.769498
36.523542	1379.641530	17.774515
36.730351	1371.217454	17.779533
36.525049	1372.388882	17.784551
36.499564	1376.148410	17.789568
36.749815	1368.885226	17.794586
36.221735	1371.303327	17.799603
36.578782	1361.157822	17.804621
36.543492	1370.422839	17.809639
36.610034	1372.416402	17.814656
36.677797	1370.897214	17.819674
36.363688	1382.392987	17.824691
36.901822	1364.603826	17.829709
36.851317	1372.242764	17.834727
36.943991	1374.756119	17.839744
37.297652	1370.743129	17.844762
36.728638	1365.486091	17.849779
36.888849	1360.717584	17.854797
36.931478	1367.369900	17.859815
37.038868	1378.275745	17.864832
37.283966	1389.440900	17.869850
36.939554	1388.453369	17.874867
37.170525	1388.978906	17.879885
37.119553	1389.861056	17.884903
37.190922	1390.320077	17.889920
37.336525	1384.424026	17.894938
37.245463	1394.963326	17.899955
37.656455	1389.978787	17.904973
37.491586	1389.777359	17.909991
37.169461	1392.939555	17.915008
37.524812	1385.334836	17.920026
37.393299	1383.600706	17.925043
37.890687	1386.618722	17.930061
37.499521	1381.901883	17.935079
37.262528	1386.616086	17.940096
37.600801	1384.745232	17.945114
37.375702	1379.349095	17.950131
37.768048	1386.653556	17.955149
37.608545	1382.560012	17.960167
37.803148	1385.941061	17.965184
37.669046	1379.129430	17.970202
37.360024	1396.046319	17.975219
37.594055	1385.323601	17.980237
37.762255	1394.285337	17.985255
37.510483	1407.399826	17.990272
37.937070	1404.991246	17.995290
37.848588	1415.498594	18.000307
38.157598	1407.831696	18.005325
38.341802	1411.069206	18.010343
38.028461	1412.260719	18.015360
38.094794	1407.194471	18.020378
37.774471	1403.971912	18.025395
38.191388	1402.953463	18.030413
38.018010	1412.931289	18.035431
38.345205	1415.269043	18.040448
38.622823	1423.156409	18.045466
38.580084	1420.821360	18.050483
38.391810	1411.225191	18.055501
38.342068	1414.559319	18.060519
38.477446	1420.139880	18.065536
38.753168	1421.564164	18.070554
38.392590	1425.335177	18.075571
38.808747	1416.651051	18.080589
38.531617	1426.840809	18.085607
38.657952	1434.051261	18.090624
39.003859	1425.463348	18.095642
38.877336	1428.708518	18.100659
38.850509	1413.567300	18.105677
38.984508	1414.426782	18.110695
38.638405	1422.370843	18.115712
38.745172	1425.121849	18.120730
38.955298	1424.814327	18.125747
39.476568	1419.184469	18.130765
38.866990	1423.237501	18.135783
38.892917	1423.116637	18.140800
39.217933	1417.205089	18.145818
38.626710	1428.573888	18.150835
38.984404	1422.698245	18.155853
39.117631	1437.068465	18.160871
39.304895	1442.738739	18.165888
39.149171	1441.768981	18.170906
39.125705	1452.815299	18.175923
39.170814	1451.728864	18.180941
39.156644	1443.544514	18.185959
39.357321	1446.962495	18.190976
39.867174	1432.112733	18.195994
39.126203	1442.289962	18.201011
39.327218	1444.391858	18.206029
39.610536	1438.960229	18.211047
39.592934	1444.264952	18.216064
39.691330	1457.561310	18.221082
39.401447	1472.524893	18.226099
39.991984	1470.261040	18.231117
40.099470	1466.447553	18.236135
39.613472	1468.669715	18.241152
39.862107	1463.151990	18.246170
39.819035	1470.455274	18.251187
40.052667	1464.384451	18.256205
40.311315	1468.973681	18.261223
40.123189	1465.275941	18.266240
40.388913	1459.985924	18.271258
40.117286	1465.362012	18.276275
40.144233	1466.408691	18.281293
40.186367	1458.237604	18.286311
40.273103	1473.483024	18.291328
40.570676	1456.214324	18.296346
40.410524	1461.320470	18.301363
40.362728	1468.242623	18.306381
40.501111	1459.267467	18.311399
40.358742	1460.220747	18.316416
40.289169	1469.879369	18.321434
40.236122	1463.582050	18.326451
40.439490	1460.766603	18.331469
40.341177	1456.313144	18.336487
40.230926	1461.632388	18.341504
40.690842	1466.947512	18.346522
40.827551	1465.808852	18.351539
40.789952	1471.997228	18.356557
40.799508	1476.410881	18.361575
40.474194	1483.161916	18.366592
40.945908	1487.534722	18.371610
41.169623	1490.188516	18.376627
41.003052	1482.485639	18.381645
40.990289	1487.941103	18.386663
40.982687	1494.828565	18.391680
41.043237	1483.804749	18.396698
40.855733	1479.715570	18.401715
40.773012	1476.989128	18.406733
41.032941	1482.651185	18.411751
41.116200	1492.244847	18.416768
41.189765	1480.407912	18.421786
41.486706	1492.827392	18.426803
41.418474	1512.840534	18.431821
41.682475	1506.086406	18.436839
41.236344	1503.789301	18.441856
41.508373	1508.120812	18.446874
41.285569	1513.082146	18.451891
41.538879	1505.913107	18.456909
41.690376	1502.338882	18.461927
41.816761	1507.103486	18.466944
41.895287	1505.860325	18.471962
41.856189	1503.079705	18.476979
41.672323	1504.108920	18.481997
41.967423	1498.413482	18.487015
41.386729	1510.077343	18.492032
41.974733	1499.857703	18.497050
42.090421	1508.278586	18.502067
41.650332	1499.880061	18.507085
41.696425	1493.194795	18.512103
41.881416	1495.507502	18.517120
42.126995	1511.065754	18.522138
42.189522	1511.690274	18.527155
41.926854	1526.924208	18.532173
42.228094	1525.406298	18.537191
42.453869	1534.841947	18.542208
42.263861	1526.782943	18.547226
42.550353	1528.688411	18.552243
42.379770	1522.169633	18.557261
42.489998	1525.270425	18.562279
42.249326	1531.345463	18.567296
42.622593	1531.523646	18.572314
42.803564	1523.927254	18.577331
42.559345	1522.564237	18.582349
42.930891	1516.140412	18.587367
42.284336	1521.679407	18.592384
42.406606	1515.654418	18.597402
42.325919	1521.467690	18.602419
42.315586	1517.360211	18.607437
42.995096	1522.669350	18.612455
42.741411	1535.534910	18.617472
42.987046	1541.155043	18.622490
43.194447	1545.237899	18.627507
42.798243	1543.523132	18.632525
42.938733	1539.313119	18.637543
42.968125	1541.454540	18.642560
43.074376	1541.822889	18.647578
43.346436	1539.684668	18.652595
43.378598	1544.407238	18.657613
43.348537	1536.159059	18.662631
42.944675	1542.922423	18.667648
42.978493	1537.065928	18.672666
43.399530	1538.514793	18.677683
42.613730	1539.805586	18.682701
43.488703	1538.437638	18.687719
43.655497	1556.204828	18.692736
43.774028	1564.925110	18.697754
43.551954	1568.210523	18.702771
43.207375	1570.738761	18.707789
43.731482	1563.732410	18.712807
43.625966	1566.415706	18.717824
43.638382	1565.536369	18.722842
43.813370	1564.350678	18.727859
43.646524	1568.735185	18.732877
44.255052	1564.496019	18.737895
43.761751	1561.641377	18.742912
44.204526	1554.240652	18.747930
44.053455	1561.908051	18.752947
43.814040	1567.389582	18.757965
44.286858	1569.145934	18.762983
43.883989	1578.620137	18.768000
44.248950	1572.336187	18.773018
44.442787	1583.247548	18.778035
44.384978	1583.266042	18.783053
44.689933	1577.531163	18.788071
44.713053	1587.086958	18.793088
44.508255	1592.790303	18.798106
44.512837	1581.932995	18.803123
44.534833	1588.607561	18.808141
44.536840	1572.003631	18.813159
44.082742	1581.993973	18.818176
44.586402	1583.401493	18.823194
44.793255	1574.052614	18.828211
44.469760	1585.486868	18.833229
44.705011	1578.752998	18.838247
44.552861	1580.244333	18.843264
44.737712	1577.071988	18.848282
44.869787	1589.908707	18.853299
45.067727	1603.514643	18.858317
45.079091	1599.823491	18.863335
44.800774	1604.462170	18.868352
44.950990	1603.883150	18.873370
45.150280	1603.249102	18.878387
44.898904	1608.928190	18.883405
45.074840	1609.269842	18.888423
45.045922	1605.360926	18.893440
45.205362	1595.309370	18.898458
44.963186	1591.992477	18.903475
45.177809	1616.471309	18.908493
45.652302	1627.919426	18.913511
45.492320	1630.112621	18.918528
45.686070	1625.386129	18.923546
45.820872	1619.305490	18.928563
45.686332	1619.768375	18.933581
46.010903	1622.037137	18.938599
45.885067	1621.760158	18.943616
45.806334	1606.352339	18.948634
45.955516	1599.720313	18.953651
46.228989	1599.039927	18.958669
45.953376	1586.512820	18.963687
45.839825	1598.210850	18.968704
45.870770	1600.664476	18.973722
46.163078	1614.672225	18.978739
46.165443	1622.997302	18.983757
46.229547	1627.522374	18.988775
46.185262	1628.059485	18.993792
46.417279	1626.303091	18.998810
46.439424	1617.292415	19.003827
46.487583	1624.641432	19.008845
46.534489	1625.094825	19.013863
46.249569	1625.836905	19.018880
46.259842	1625.611189	19.023898
46.339123	1617.948634	19.028915
46.007069	1625.549736	19.033933
46.310153	1612.663684	19.038951
46.016976	1622.868691	19.043968
46.217298	1630.645175	19.048986
46.715417	1640.154981	19.054003
46.722943	1647.131655	19.059021
46.962090	1643.938168	19.064039
46.849678	1654.212706	19.069056
46.679803	1657.597261	19.074074
46.908451	1648.901375	19.079091
46.626026	1653.629077	19.084109
47.183223	1645.001644	19.089127
47.209159	1650.208083	19.094144
47.237659	1643.661225	19.099162
47.130054	1644.747931	19.104179
46.973548	1639.347281	19.109197
47.320114	1655.757733	19.114215
47.087118	1672.116985	19.119232
47.231110	1679.927564	19.124250
47.419432	1671.316885	19.129267
47.186551	1673.338458	19.134285
47.306536	1660.989173	19.139303
47.790984	1669.421788	19.144320
47.422421	1665.408274	19.149338
47.689122	1668.017488	19.154355
47.518180	1666.482023	19.159373
47.819269	1668.274760	19.164391
48.031398	1669.323997	19.169408
47.692949	1674.966252	19.174426
47.758918	1664.007752	19.179443
47.693827	1678.374522	19.184461
47.793762	1682.830874	19.189479
48.300249	1699.762297	19.194496
48.286125	1699.177463	19.199514
48.477369	1688.783180	19.204531
48.519529	1699.582669	19.209549
48.450100	1698.476293	19.214567
48.605188	1689.226988	19.219584
48.435037	1677.986719	19.224602
48.714121	1659.893851	19.229619
47.998093	1662.218352	19.234637
47.956428	1678.459265	19.239655
48.585274	1678.493259	19.244672
48.527786	1679.363820	19.249690
48.464720	1683.268164	19.254707
48.597020	1688.606280	19.259725
48.337382	1692.636105	19.264743
48.541524	1686.364688	19.269760
48.706527	1685.070094	19.274778
49.074363	1687.373114	19.279795
48.353833	1696.348005	19.284813
48.374780	1692.513313	19.289831
48.906449	1710.589584	19.294848
48.730503	1714.356976	19.299866
49.499506	1713.621040	19.304883
49.182391	1720.187830	19.309901
48.872598	1715.956800	19.314919
49.616032	1702.673467	19.319936
49.033321	1716.613250	19.324954
49.225472	1707.613766	19.329971
49.078183	1710.701284	19.334989
49.208485	1712.770108	19.340007
49.347909	1709.633261	19.345024
49.186712	1714.891130	19.350042
49.372324	1717.472028	19.355059
49.470303	1735.461629	19.360077
49.674597	1739.576576	19.365095
49.876435	1737.916423	19.370112
49.422643	1742.570006	19.375130
49.844482	1739.666635	19.380147
49.775986	1740.538923	19.385165
49.756574	1748.605523	19.390183
49.880555	1738.313274	19.395200
49.658659	1731.824551	19.400218
49.947304	1737.141342	19.405235
49.930159	1742.597570	19.410253
50.172708	1749.919338	19.415271
50.448893	1747.458535	19.420288
50.259991	1750.849244	19.425306
50.554202	1749.950995	19.430323
50.365525	1759.088756	19.435341
50.218179	1750.963003	19.440359
50.716231	1744.383569	19.445376
50.172046	1755.211838	19.450394
50.566698	1743.854632	19.455411
50.717635	1746.545115	19.460429
50.482228	1752.755111	19.465447
50.685202	1749.040220	19.470464
50.869591	1755.140261	19.475482
50.682410	1748.248436	19.480499
50.336518	1749.104222	19.485517
50.641096	1762.093930	19.490535
51.119811	1769.400797	19.495552
50.878313	1774.971085	19.500570
50.912148	1768.013065	19.505587
51.106674	1764.738179	19.510605
51.267809	1769.046100	19.515623
51.199457	1760.866937	19.520640
51.194165	1770.613486	19.525658
51.428008	1772.697654	19.530675
51.347513	1767.433388	19.535693
51.643163	1769.217519	19.540711
51.430118	1763.828844	19.545728
51.471518	1763.541441	19.550746
51.615038	1762.045068	19.555763
51.355361	1770.417581	19.560781
51.109672	1776.032710	19.565799
51.496603	1779.266930	19.570816
51.383262	1788.828432	19.575834
52.125376	1785.470905	19.580851
52.361266	1792.866322	19.585869
52.145029	1786.805910	19.590887
52.352983	1782.537930	19.595904
52.026513	1788.355080	19.600922
52.025597	1784.435426	19.605939
52.153266	1781.303565	19.610957
52.331474	1787.799086	19.615975
52.587334	1781.541625	19.620992
52.478314	1794.428889	19.626010
52.244803	1782.097033	19.631027
52.491719	1781.758494	19.636045
52.141002	1788.838692	19.641063
52.385947	1778.123498	19.646080
52.265487	1778.413756	19.651098
52.605159	1777.218030	19.656115
52.751847	1776.440729	19.661133
52.584953	1784.751372	19.666151
52.318981	1779.424638	19.671168
52.125680	1781.137045	19.676186
52.549413	1802.241154	19.681203
53.016591	1808.694564	19.686221
52.665507	1815.651745	19.691239
52.747601	1811.769575	19.696256
52.590494	1809.698564	19.701274
52.805441	1806.404691	19.706291
52.983028	1818.846254	19.711309
53.192615	1832.043413	19.716327
53.152097	1839.791446	19.721344
53.103841	1837.583448	19.726362
53.393952	1833.353080	19.731379
53.222038	1832.682503	19.736397
53.177603	1830.739013	19.741415
53.318373	1828.334131	19.746432
53.360284	1835.788362	19.751450
53.610919	1845.112975	19.756467
54.178711	1849.319330	19.761485
53.801387	1849.337387	19.766503
53.608889	1846.448194	19.771520
53.788007	1850.485055	19.776538
53.911317	1859.065867	19.781555
54.141462	1851.026101	19.786573
53.909191	1862.496734	19.791591
54.169532	1851.343554	19.796608
53.799074	1853.658120	19.801626
54.139452	1847.422110	19.806643
53.714188	1849.069874	19.811661
54.131594	1853.129366	19.816679
54.168142	1851.005917	19.821696
54.347032	1866.827409	19.826714
54.480978	1879.995426	19.831731
54.857332	1876.398522	19.836749
54.389023	1882.064343	19.841767
54.621420	1877.429568	19.846784
54.529671	1871.160261	19.851802
54.558360	1869.795487	19.856819
54.832692	1865.498152	19.861837
54.218537	1874.759442	19.866855
54.804496	1870.631047	19.871872
54.666933	1869.860405	19.876890
54.933469	1876.881801	19.881907
55.031033	1886.303006	19.886925
55.083738	1892.045002	19.891943
55.595051	1892.097413	19.896960
55.226379	1902.588980	19.901978
55.144682	1885.619150	19.906995
55.425055	1896.169982	19.912013
55.297627	1889.874698	19.917031
55.601808	1890.426654	19.922048
55.374650	1904.064705	19.927066
55.416776	1895.915512	19.932083
55.747861	1894.591727	19.937101
55.723385	1895.902126	19.942119
55.591501	1889.541264	19.947136
55.434419	1893.611873	19.952154
55.504578	1887.743258	19.957171
55.645223	1887.516048	19.962189
55.810862	1899.280993	19.967207
56.114075	1888.304122	19.972224
55.671799	1885.924306	19.977242
55.549200	1891.343448	19.982259
55.929450	1903.040054	19.987277
55.998375	1909.470686	19.992295
56.154977	1911.311333	19.997312
56.081292	1909.735361	20.002330
55.953267	1924.295237	20.007347
56.398391	1914.391261	20.012365
56.086802	1920.995131	20.017383
56.326043	1935.803610	20.022400
56.618156	1939.548212	20.027418
56.250690	1936.083615	20.032435
56.715656	1938.002194	20.037453
57.082410	1946.989908	20.042471
56.746510	1931.470610	20.047488
56.569454	1929.964485	20.052506
56.449696	1942.951375	20.057523
56.836651	1943.165291	20.062541
56.621611	1949.236454	20.067559
56.656491	1950.449189	20.072576
56.848230	1964.087931	20.077594
57.185239	1964.814640	20.082611
57.339361	1959.008592	20.087629
57.324279	1959.055107	20.092647
57.339901	1958.604470	20.097664
57.356862	1952.696827	20.102682
57.385203	1958.654116	20.107699
57.508282	1948.680649	20.112717
57.182980	1970.524051	20.117735
57.784019	1972.588585	20.122752
57.877094	1982.013701	20.127770
57.875250	1978.239327	20.132787
58.183870	1987.873691	20.137805
57.948630	1983.258503	20.142823
58.026772	1982.157392	20.147840
57.993431	1982.601274	20.152858
58.387614	1985.250527	20.157875
58.250189	1987.190902	20.162893
58.139060	1994.031655	20.167911
58.280163	1992.036986	20.172928
58.511552	1980.878793	20.177946
58.247127	1983.340877	20.182963
58.059131	1976.354410	20.187981
57.963295	1977.401420	20.192999
58.055679	1989.278895	20.198016
57.699230	1984.291347	20.203034
58.182557	2002.072507	20.208051
58.452761	2008.818803	20.213069
58.471063	2009.207254	20.218087
58.739761	2000.801592	20.223104
58.498096	2013.523588	20.228122
58.345773	2026.237908	20.233139
59.236453	2031.432059	20.238157
59.161941	2029.155562	20.243175
59.592606	2028.093898	20.248192
59.537003	2021.553768	20.253210
59.455949	2043.687221	20.258227
59.472470	2026.907012	20.263245
59.648685	2020.731380	20.268263
59.573456	2010.271355	20.273280
59.480250	2003.920173	20.278298
59.279208	2001.650879	20.283315
59.845258	1998.901612	20.288333
59.715744	2015.364893	20.293351
59.432175	2005.672872	20.298368
59.574928	2008.074321	20.303386
59.432102	2009.273873	20.308403
59.558544	2016.939015	20.313421
59.780015	2015.360975	20.318439
59.972687	2017.309600	20.323456
59.756112	2020.029300	20.328474
59.886025	2020.327675	20.333491
60.208724	2010.572226	20.338509
60.000412	2029.894623	20.343527
60.189534	2037.019737	20.348544
60.092528	2037.625085	20.353562
60.177192	2042.289063	20.358579
60.465039	2038.762803	20.363597
60.203526	2044.156415	20.368615
60.303961	2041.429594	20.373632
60.519422	2038.195564	20.378650
60.339443	2044.024562	20.383667
60.681986	2045.236440	20.388685
60.882451	2066.224351	20.393703
61.092132	2067.068852	20.398720
61.032082	2065.575943	20.403738
60.971563	2067.157111	20.408755
60.992571	2069.826971	20.413773
60.914952	2070.558682	20.418791
60.851058	2069.056907	20.423808
61.309130	2058.926743	20.428826
61.178090	2067.115125	20.433843
61.099838	2065.476733	20.438861
60.961620	2072.204986	20.443879
60.943384	2068.726675	20.448896
61.359358	2079.101723	20.453914
61.166338	2087.287200	20.458931
61.228590	2078.427813	20.463949
61.561888	2082.532097	20.468967
61.440131	2104.425829	20.473984
61.733667	2111.111700	20.479002
61.761876	2110.921040	20.484019
62.367059	2108.361302	20.489037
62.344311	2113.906890	20.494055
62.284360	2107.297975	20.499072
62.415384	2111.361367	20.504090
62.122965	2109.955358	20.509107
62.422241	2098.111058	20.514125
62.381635	2099.831132	20.519143
62.306933	2103.276605	20.524160
62.627485	2100.815115	20.529178
62.160479	2090.372240	20.534195
62.342367	2095.939414	20.539213
62.443780	2107.288490	20.544231
62.342434	2101.610791	20.549248
62.765609	2111.482915	20.554266
62.517901	2124.953924	20.559283
62.283523	2125.015862	20.564301
62.445648	2124.157226	20.569319
62.297875	2133.108872	20.574336
62.728416	2136.797112	20.579354
63.060393	2142.479653	20.584371
63.813249	2139.745282	20.589389
63.423936	2147.030499	20.594407
63.427960	2151.397844	20.599424
63.596939	2142.389149	20.604442
63.684098	2151.042042	20.609459
63.803328	2141.933835	20.614477
63.718956	2144.841142	20.619495
63.775885	2145.346630	20.624512
63.864384	2131.657468	20.629530
63.943841	2141.608709	20.634547
64.062245	2132.229213	20.639565
64.054216	2141.465108	20.644583
63.814727	2134.006925	20.649600
64.147047	2138.793086	20.654618
63.904505	2137.868452	20.659635
63.969030	2134.509717	20.664653
64.369104	2129.678179	20.669671
64.189267	2133.932303	20.674688
64.422587	2131.108904	20.679706
64.100200	2132.993059	20.684723
64.468215	2127.304937	20.689741
64.100203	2131.313964	20.694759
64.021102	2139.920311	20.699776
64.781726	2145.381048	20.704794
64.127464	2155.712362	20.709811
64.373115	2159.218116	20.714829
64.907391	2160.841814	20.719847
64.668621	2164.341408	20.724864
64.721710	2165.901629	20.729882
64.879594	2173.101125	20.734899
64.730390	2176.147993	20.739917
64.738856	2190.866597	20.744935
64.572534	2186.470952	20.749952
65.146660	2189.189882	20.754970
65.184046	2184.538240	20.759987
65.141659	2192.813784	20.765005
65.222514	2202.322988	20.770023
65.314927	2199.827795	20.775040
65.503342	2207.735796	20.780058
65.177231	2208.515913	20.785075
65.477786	2207.373630	20.790093
65.768582	2215.278218	20.795111
65.770692	2223.044987	20.800128
66.090877	2228.382233	20.805146
66.281795	2242.614660	20.810163
66.132778	2231.818897	20.815181
66.352991	2228.498874	20.820199
66.554593	2228.202145	20.825216
66.471500	2223.417877	20.830234
66.400251	2228.715456	20.835251
66.505020	2225.877466	20.840269
66.864920	2222.961631	20.845287
66.623189	2235.368185	20.850304
66.861872	2228.879710	20.855322
66.517885	2217.101398	20.860339
66.768109	2220.230874	20.865357
66.800575	2220.932719	20.870375
66.983679	2223.223723	20.875392
66.878347	2218.458721	20.880410
66.749084	2220.306316	20.885427
66.671518	2217.291749	20.890445
67.124749	2215.589010	20.895463
66.750044	2219.936807	20.900480
67.099523	2232.092927	20.905498
67.159459	2250.524546	20.910515
67.092545	2250.358256	20.915533
67.238269	2247.043588	20.920551
66.936537	2256.982026	20.925568
67.308156	2255.850699	20.930586
67.168441	2262.358330	20.935603
67.444830	2264.028755	20.940621
67.318690	2275.874378	20.945639
67.038280	2284.846880	20.950656
67.428077	2289.251658	20.955674
68.018818	2298.939827	20.960691
68.082292	2305.380922	20.965709
68.077771	2296.273089	20.970727
67.819200	2312.220324	20.975744
67.977189	2301.903488	20.980762
68.065368	2310.231220	20.985779
68.458224	2300.401500	20.990797
68.337482	2298.242675	20.995815
68.227381	2312.632784	21.000832
68.672134	2320.841532	21.005850
68.541372	2325.043827	21.010867
68.815546	2330.079014	21.015885
69.020086	2321.345552	21.020903
69.031776	2328.975152	21.025920
69.171047	2313.775590	21.030938
69.616256	2319.579315	21.035955
69.319068	2322.131792	21.040973
69.574986	2316.660008	21.045991
69.481735	2323.425495	21.051008
69.313963	2302.258511	21.056026
69.461593	2306.249911	21.061043
69.398499	2310.410040	21.066061
69.792144	2314.397615	21.071079
69.532256	2310.960274	21.076096
69.472763	2307.491537	21.081114
69.678203	2312.777352	21.086131
69.838529	2316.384877	21.091149
69.926582	2303.806602	21.096167
69.585388	2323.408934	21.101184
69.775216	2318.026406	21.106202
69.993149	2313.075019	21.111219
69.639565	2312.571754	21.116237
69.917192	2313.055294	21.121255
69.742951	2331.542622	21.126272
69.983779	2335.519427	21.131290
70.171236	2334.237051	21.136307
69.875013	2345.759040	21.141325
70.328297	2343.538680	21.146343
70.330711	2348.774255	21.151360
70.240060	2349.697385	21.156378
70.519448	2353.500879	21.161395
70.738238	2355.814715	21.166413
70.628931	2353.439476	21.171431
70.964573	2379.178615	21.176448
71.146758	2387.800954	21.181466
71.095554	2380.792897	21.186483
71.234930	2385.050722	21.191501
71.286290	2380.027575	21.196519
71.322389	2389.922624	21.201536
71.433626	2382.702906	21.206554
71.158218	2382.941702	21.211571
71.518043	2386.820972	21.216589
71.612365	2379.872175	21.221607
71.633863	2386.269378	21.226624
71.323504	2381.599577	21.231642
71.874163	2382.987178	21.236659
71.915941	2405.464785	21.241677
71.682543	2400.337909	21.246695
71.962816	2401.307080	21.251712
71.993872	2405.471416	21.256730
72.348186	2408.193258	21.261747
72.107977	2416.260033	21.266765
72.385957	2404.930160	21.271783
72.548808	2411.399909	21.276800
72.405687	2402.269552	21.281818
72.538407	2402.955697	21.286835
72.299706	2405.868288	21.291853
72.540151	2395.014564	21.296871
72.305193	2409.250725	21.301888
72.435637	2416.625048	21.306906
72.469127	2412.930263	21.311923
72.436089	2431.146236	21.316941
73.003276	2422.781985	21.321959
72.906254	2427.682832	21.326976
72.848067	2424.592603	21.331994
73.230338	2436.166154	21.337011
72.843554	2447.333129	21.342029
73.232217	2445.268063	21.347047
73.177117	2443.698601	21.352064
73.440293	2447.659305	21.357082
73.243735	2436.391136	21.362099
73.250846	2447.408027	21.367117
73.796119	2462.784439	21.372135
73.620907	2473.375429	21.377152
73.952324	2461.405922	21.382170
73.652294	2466.209185	21.387187
73.826278	2469.653639	21.392205
73.474894	2466.445219	21.397223
73.809622	2481.412777	21.402240
73.941626	2490.585882	21.407258
74.079408	2491.836185	21.412275
73.887747	2495.782946	21.417293
74.631646	2487.321543	21.422311
74.535109	2498.089589	21.427328
74.467028	2489.351416	21.432346
74.722062	2496.561070	21.437363
74.771022	2514.079398	21.442381
75.162888	2510.318977	21.447399
74.985537	2518.559005	21.452416
74.857124	2510.786584	21.457434
75.248083	2506.275144	21.462451
75.179311	2510.887536	21.467469
75.453832	2502.638536	21.472487
75.528062	2507.023374	21.477504
75.114611	2520.429118	21.482522
75.417844	2509.473960	21.487539
75.615225	2510.585526	21.492557
75.687353	2496.305297	21.497575
75.341565	2507.762563	21.502592
75.534773	2511.020957	21.507610
75.845551	2516.183019	21.512627
75.524897	2528.883036	21.517645
76.030012	2530.328283	21.522663
75.996657	2529.298262	21.527680
75.874122	2536.914263	21.532698
75.870359	2527.787257	21.537715
76.179753	2532.084758	21.542733
76.126193	2543.890781	21.547751
76.191758	2556.842766	21.552768
75.943263	2565.229676	21.557786
76.226648	2558.276438	21.562803
76.208408	2560.573783	21.567821
76.437940	2565.357227	21.572839
76.682388	2576.217079	21.577856
76.718481	2578.859402	21.582874
77.040539	2567.879166	21.587891
76.693223	2575.760799	21.592909
77.130245	2577.027349	21.597927
77.038773	2573.386827	21.602944
77.061079	2569.191934	21.607962
77.381679	2587.204321	21.612979
77.451954	2598.646957	21.617997
77.408981	2599.325919	21.623015
77.797657	2606.871324	21.628032
77.783107	2604.781041	21.633050
77.761745	2596.650946	21.638067
77.577162	2599.258411	21.643085
77.944566	2595.271405	21.648103
78.188953	2598.348208	21.653120
78.009636	2591.704162	21.658138
78.141155	2594.372566	21.663155
78.166349	2605.134229	21.668173
78.225524	2595.599652	21.673191
78.074408	2592.189401	21.678208
77.951023	2593.168171	21.683226
78.222986	2602.224721	21.688243
78.312025	2613.973730	21.693261
77.975908	2615.910584	21.698279
78.352920	2620.282729	21.703296
78.323462	2615.947596	21.708314
78.647982	2624.200571	21.713331
78.544235	2645.751275	21.718349
79.053854	2643.547303	21.723367
78.912540	2648.319435	21.728384
78.860847	2653.399455	21.733402
78.819433	2633.430564	21.738419
78.939817	2650.675874	21.743437
79.237112	2654.599718	21.748455
79.447085	2666.872675	21.753472
79.537437	2670.866818	21.758490
79.629351	2671.950732	21.763507
80.004826	2664.225546	21.768525
80.110817	2658.316348	21.773543
80.189844	2653.967365	21.778560
79.768485	2666.282423	21.783578
79.890866	2657.091402	21.788595
79.595263	2675.680157	21.793613
80.083892	2677.200591	21.798631
80.285506	2679.902213	21.803648
80.440725	2686.259635	21.808666
80.388798	2687.530206	21.813683
80.416039	2680.304592	21.818701
80.504634	2682.897675	21.823719
80.840923	2690.492354	21.828736
80.838530	2699.143760	21.833754
81.121557	2695.059487	21.838771
80.976640	2713.233306	21.843789
80.756389	2714.921617	21.848807
81.053082	2707.230849	21.853824
81.268764	2711.296894	21.858842
81.711657	2701.055128	21.863859
81.256302	2703.764997	21.868877
81.437042	2706.962257	21.873895
81.483425	2708.264769	21.878912
81.130878	2702.866105	21.883930
81.311273	2698.845253	21.888947
81.479608	2720.441791	21.893965
81.441258	2730.468627	21.898983
82.063086	2728.089255	21.904000
82.028203	2725.623402	21.909018
82.224651	2728.401589	21.914035
81.983799	2736.020430	21.919053
82.056636	2734.004813	21.924071
82.411451	2728.921401	21.929088
81.866531	2746.596125	21.934106
82.306635	2750.914231	21.939123
82.370385	2751.469167	21.944141
82.377631	2753.027153	21.949159
82.483718	2753.767984	21.954176
82.645045	2754.967274	21.959194
82.573551	2759.674842	21.964211
82.658839	2771.875876	21.969229
82.980021	2771.216380	21.974247
82.989302	2768.917192	21.979264
82.815005	2776.591902	21.984282
82.808543	2768.159558	21.989299
83.254829	2778.498702	21.994317
83.274106	2787.629652	21.999335
83.616356	2795.283409	22.004352
83.252675	2805.304445	22.009370
83.772970	2792.247805	22.014387
83.822222	2791.447853	22.019405
83.321174	2786.564795	22.024423
83.935009	2787.358637	22.029440
83.797162	2795.876659	22.034458
83.786249	2807.887637	22.039475
84.188521	2812.208529	22.044493
84.160759	2820.510476	22.049511
84.242625	2814.333574	22.054528
84.338680	2819.109592	22.059546
84.505569	2826.289002	22.064563
84.209697	2825.735648	22.069581
84.302910	2830.423741	22.074599
84.852339	2838.408020	22.079616
84.729969	2841.835852	22.084634
85.059450	2836.342918	22.089651
85.118248	2840.177920	22.094669
84.915512	2840.386398	22.099687
85.251787	2841.185854	22.104704
85.099312	2843.261238	22.109722
85.702577	2851.738924	22.114739
86.032009	2861.951238	22.119757
85.275309	2856.413850	22.124775
85.576820	2851.714343	22.129792
85.644845	2865.524651	22.134810
85.776967	2858.020569	22.139827
85.953780	2861.600371	22.144845
85.961456	2860.800618	22.149863
85.898172	2866.400131	22.154880
85.917227	2861.012636	22.159898
85.990564	2865.053675	22.164915
85.934519	2879.902885	22.169933
85.882652	2887.678396	22.174951
86.786920	2892.248905	22.179968
86.560779	2889.885587	22.184986
86.861153	2885.539744	22.190003
86.709795	2885.806453	22.195021
86.499511	2884.434856	22.200039
86.858800	2894.573075	22.205056
86.926926	2905.618561	22.210074
86.668656	2907.233940	22.215091
87.124143	2903.252005	22.220109
87.004291	2911.259113	22.225127
87.262364	2903.662686	22.230144
87.191357	2928.339555	22.235162
87.519053	2930.914151	22.240179
87.597289	2931.359512	22.245197
87.605846	2938.844676	22.250215
87.578738	2924.888964	22.255232
87.590326	2937.429904	22.260250
87.908810	2935.984928	22.265267
87.955323	2939.380006	22.270285
87.896205	2948.618007	22.275303
88.238829	2953.402774	22.280320
88.197648	2967.163988	22.285338
88.439466	2960.229734	22.290355
88.452714	2949.783707	22.295373
88.286246	2959.960147	22.300391
88.884450	2943.952754	22.305408
88.572454	2954.256146	22.310426
88.308178	2973.436823	22.315443
88.827514	2965.319693	22.320461
88.673901	2970.305303	22.325479
89.186968	2974.514190	22.330496
88.995755	2976.892343	22.335514
89.296864	2982.838799	22.340531
89.530239	2975.905861	22.345549
89.284132	2982.900697	22.350567
89.683098	2990.438341	22.355584
89.719936	3001.643443	22.360602
89.663674	3006.875778	22.365619
89.695525	3005.396798	22.370637
89.757056	3003.127269	22.375655
89.779976	2995.567646	22.380672
89.904586	3008.438112	22.385690
89.962862	3000.494200	22.390707
90.165116	2992.530891	22.395725
90.218058	3010.860228	22.400743
90.324918	3013.485215	22.405760
90.426145	3018.825441	22.410778
90.546415	3025.197928	22.415795
90.657728	3015.282526	22.420813
90.323544	3017.585241	22.425831
90.587227	3024.427630	22.430848
90.354656	3037.268858	22.435866
90.671554	3043.279141	22.440883
90.535025	3042.738690	22.445901
90.735710	3058.223258	22.450919
91.280994	3071.116235	22.455936
91.055010	3082.536157	22.460954
91.124619	3081.212224	22.465971
91.757066	3072.622827	22.470989
91.674525	3096.209675	22.476007
91.885173	3100.320785	22.481024
91.916030	3096.982928	22.486042
92.045101	3092.809061	22.491059
92.531454	3096.381446	22.496077
92.293599	3093.918936	22.501095
92.501230	3093.804312	22.506112
92.650345	3094.434259	22.511130
92.253922	3099.148635	22.516147
92.976397	3085.368891	22.521165
92.720737	3095.215351	22.526183
92.710765	3094.014354	22.531200
93.033457	3090.583432	22.536218
92.508068	3091.581022	22.541235
92.668737	3087.487425	22.546253
92.615247	3103.422164	22.551271
93.165319	3106.747850	22.556288
92.961830	3110.582972	22.561306
92.879298	3121.967819	22.566323
92.986024	3123.368220	22.571341
93.223359	3134.601961	22.576359
93.602396	3136.054388	22.581376
93.446218	3138.682729	22.586394
93.600695	3137.140339	22.591411
93.730509	3144.309904	22.596429
93.837465	3155.510429	22.601447
93.898233	3168.236354	22.606464
94.101563	3160.910366	22.611482
93.924153	3164.529944	22.616499
94.030890	3160.350092	22.621517
94.230559	3173.171041	22.626535
94.545163	3186.134962	22.631552
94.571648	3189.189193	22.636570
94.662396	3190.481634	22.641587
94.945299	3184.121609	22.646605
94.818899	3188.970453	22.651623
94.805576	3182.499026	22.656640
95.127485	3194.537025	22.661658
95.157653	3207.968462	22.666675
95.614011	3214.042172	22.671693
95.485119	3217.032376	22.676711
95.321078	3210.373082	22.681728
95.555495	3208.423630	22.686746
95.448871	3207.922676	22.691763
96.046645	3203.508070	22.696781
95.654599	3205.867217	22.701799
95.833370	3206.189522	22.706816
95.907580	3203.577105	22.711834
95.628777	3219.941780	22.716851
96.095752	3221.885438	22.721869
96.149506	3225.768657	22.726887
96.228176	3219.153397	22.731904
96.243582	3236.242121	22.736922
96.408889	3244.255200	22.741939
96.313944	3250.964486	22.746957
96.435688	3255.465156	22.751975
96.736073	3253.265488	22.756992
96.839545	3260.963166	22.762010
96.970317	3265.793833	22.767027
96.915475	3277.161814	22.772045
97.057376	3279.828695	22.777063
97.214874	3279.305296	22.782080
97.067694	3279.107384	22.787098
97.048653	3306.734056	22.792115
96.849150	3303.870974	22.797133
97.449234	3318.358933	22.802151
97.555249	3320.330748	22.807168
97.904646	3325.499620	22.812186
98.298091	3335.777926	22.817203
98.567868	3331.951245	22.822221
98.271216	3329.706229	22.827239
98.446995	3322.551775	22.832256
98.400586	3326.245549	22.837274
98.496061	3327.278444	22.842291
98.574510	3347.400051	22.847309
98.731449	3352.914712	22.852327
98.866289	3350.680999	22.857344
99.463552	3345.171208	22.862362
99.032089	3352.599230	22.867379
99.137529	3357.219263	22.872397
99.261964	3357.411207	22.877415
99.335358	3350.661006	22.882432
99.527973	3351.950124	22.887450
99.521644	3371.037152	22.892467
99.587943	3365.225475	22.897485
99.927301	3368.887227	22.902503
99.672771	3377.950903	22.907520
99.880758	3366.666115	22.912538
99.645657	3370.222178	22.917555
100.260323	3383.994584	22.922573
100.146387	3395.974750	22.927591
99.838998	3392.538329	22.932608
100.161746	3396.717165	22.937626
100.008096	3403.041168	22.942643
100.824793	3406.312513	22.947661
100.698354	3419.140540	22.952679
100.499276	3426.964597	22.957696
100.634297	3422.874943	22.962714
100.781466	3422.065936	22.967731
101.177843	3432.905659	22.972749
101.172090	3446.993100	22.977767
101.006792	3451.816545	22.982784
101.555424	3446.955072	22.987802
101.575257	3449.634790	22.992819
101.623900	3439.586941	22.997837
101.639865	3442.734397	23.002855
101.914100	3441.971763	23.007872
102.161753	3458.247860	23.012890
102.127066	3472.485044	23.017907
102.164112	3468.101411	23.022925
102.520793	3473.897289	23.027943
102.472815	3479.017992	23.032960
102.401927	3469.029885	23.037978
102.387980	3467.226631	23.042995
102.624946	3473.025484	23.048013
102.468780	3466.636305	23.053031
102.445019	3473.129360	23.058048
102.781570	3487.548273	23.063066
102.716972	3499.186209	23.068083
102.916559	3492.094240	23.073101
103.043059	3493.292725	23.078119
103.284180	3500.400804	23.083136
103.802311	3506.960478	23.088154
103.556593	3523.402306	23.093171
103.611116	3518.482506	23.098189
103.559112	3521.820534	23.103207
103.714221	3520.312732	23.108224
103.719346	3518.418108	23.113242
103.444618	3534.731927	23.118259
103.653599	3535.791240	23.123277
103.933160	3538.493406	23.128295
103.867101	3559.464844	23.133312
104.239877	3559.157060	23.138330
104.588800	3573.637229	23.143347
104.706959	3571.851144	23.148365
104.626487	3569.487007	23.153383
105.000119	3587.779313	23.158400
105.156460	3595.569853	23.163418
104.889076	3601.040597	23.168435
105.518867	3586.309161	23.173453
105.591428	3589.353085	23.178471
104.908270	3597.123646	23.183488
105.290621	3588.573190	23.188506
105.616452	3603.492575	23.193523
105.826406	3620.566963	23.198541
105.910796	3618.337964	23.203559
105.850793	3622.494754	23.208576
105.813510	3612.207764	23.213594
105.725591	3626.232465	23.218611
106.224415	3638.495550	23.223629
106.747591	3645.669969	23.228647
106.302902	3638.899826	23.233664
106.465289	3644.432661	23.238682
106.696316	3648.651176	23.243699
107.036361	3645.195338	23.248717
107.194432	3649.740917	23.253735
107.155196	3661.532800	23.258752
107.323132	3665.161499	23.263770
106.917786	3669.918451	23.268787
107.082972	3667.503189	23.273805
107.373911	3660.286371	23.278823
107.404269	3674.838626	23.283840
107.410194	3676.261176	23.288858
107.581239	3684.576561	23.293875
107.501716	3687.792676	23.298893
107.697020	3681.367294	23.303911
107.901233	3694.964362	23.308928
108.178150	3698.263516	23.313946
108.099538	3711.630305	23.318963
108.257395	3713.827610	23.323981
108.348138	3715.356816	23.328999
108.358793	3719.931821	23.334016
108.759265	3723.041179	23.339034
108.781458	3741.953688	23.344051
108.955637	3735.878794	23.349069
109.068270	3728.904517	23.354087
109.070307	3741.308630	23.359104
109.042909	3723.649945	23.364122
109.295336	3740.231714	23.369139
109.087058	3756.175497	23.374157
109.304061	3757.448199	23.379175
109.460459	3759.147034	23.384192
109.583970	3758.635260	23.389210
109.914511	3768.851073	23.394227
109.771365	3782.373217	23.399245
110.396365	3773.835160	23.404263
110.561758	3782.129381	23.409280
110.294890	3778.642348	23.414298
109.880673	3792.790895	23.419315
110.218236	3798.157452	23.424333
110.436977	3797.454001	23.429351
110.514742	3804.631982	23.434368
110.798487	3803.476456	23.439386
110.911489	3814.363962	23.444403
110.929698	3823.713392	23.449421
111.076905	3820.492897	23.454439
110.826793	3823.896738	23.459456
111.206953	3830.228792	23.464474
111.665643	3847.965140	23.469491
111.561486	3861.538049	23.474509
111.955778	3855.002521	23.479527
111.746975	3864.722114	23.484544
112.002736	3858.179881	23.489562
112.292605	3857.821954	23.494579
112.048867	3874.557333	23.499597
112.401530	3880.303471	23.504615
112.799256	3876.522915	23.509632
112.468691	3878.992457	23.514650
112.638191	3879.717088	23.519667
112.891874	3882.893660	23.524685
113.000938	3873.653607	23.529703
113.027098	3888.052028	23.534720
112.971379	3886.627729	23.539738
113.328354	3891.877644	23.544755
113.259189	3889.552727	23.549773
113.283312	3884.722812	23.554791
113.209276	3899.837656	23.559808
113.532298	3904.581560	23.564826
113.878239	3917.149706	23.569843
113.646614	3920.771615	23.574861
114.108142	3922.583637	23.579879
114.033283	3944.046139	23.584896
114.358947	3945.005130	23.589914
114.566952	3951.888159	23.594931
114.570333	3945.357027	23.599949
114.686460	3934.392448	23.604967
114.192796	3938.307925	23.609984
114.481238	3941.239177	23.615002
114.752048	3957.840360	23.620019
114.696751	3970.749167	23.625037
114.910795	3972.183324	23.630055
114.921761	3981.694947	23.635072
115.371557	3995.004410	23.640090
115.060076	3990.511122	23.645107
115.441994	3996.978685	23.650125
115.736221	4008.437631	23.655143
115.370128	4009.691230	23.660160
115.834785	4015.088443	23.665178
116.281843	4015.277196	23.670195
116.194976	4041.084902	23.675213
116.653787	4037.010666	23.680231
116.338602	4037.356716	23.685248
116.288205	4041.319555	23.690266
116.772938	4030.085690	23.695283
116.912248	4040.101199	23.700301
116.882826	4032.473590	23.705319
117.074654	4036.228033	23.710336
117.142101	4024.709186	23.715354
116.989696	4034.075986	23.720371
117.068084	4052.841133	23.725389
117.709398	4048.495259	23.730407
117.478359	4052.647379	23.735424
117.615645	4056.666040	23.740442
117.673791	4067.170898	23.745459
117.621563	4079.498521	23.750477
118.022171	4072.327488	23.755495
118.159683	4084.660109	23.760512
117.765864	4086.198977	23.765530
117.905223	4096.760570	23.770547
118.103788	4106.710017	23.775565
118.019891	4117.811625	23.780583
118.527725	4127.513776	23.785600
118.971849	4130.591116	23.790618
118.965836	4139.215371	23.795635
118.766418	4142.122082	23.800653
118.924331	4147.431666	23.805671
119.175439	4159.408804	23.810688
119.420249	4163.672628	23.815706
119.951012	4163.014972	23.820723
119.458676	4169.379677	23.825741
119.852005	4180.835832	23.830759
120.209531	4189.071730	23.835776
120.084751	4186.585041	23.840794
120.615754	4195.926923	23.845811
120.188134	4196.214835	23.850829
120.495084	4186.306021	23.855847
120.621447	4190.793576	23.860864
120.538121	4207.592510	23.865882
120.844752	4215.855333	23.870899
120.790219	4213.335539	23.875917
121.412568	4205.684656	23.880935
121.096908	4211.665019	23.885952
121.344912	4213.608374	23.890970
121.386956	4227.243875	23.895987
121.400802	4232.279349	23.901005
121.616431	4232.696906	23.906023
121.653701	4229.796580	23.911040
121.558230	4235.821365	23.916058
121.991718	4243.508793	23.921075
122.001543	4269.415307	23.926093
122.025657	4264.818869	23.931111
122.206206	4266.340365	23.936128
122.356243	4269.662659	23.941146
122.856953	4277.816193	23.946163
122.494971	4279.801461	23.951181
122.640909	4274.646183	23.956199
123.160922	4284.176063	23.961216
122.895959	4306.347412	23.966234
123.013179	4301.332353	23.971251
123.289147	4303.580669	23.976269
123.410169	4300.367348	23.981287
123.565554	4316.728115	23.986304
123.536284	4332.098291	23.991322
123.847749	4336.689454	23.996339
124.035455	4324.968501	24.001357
123.933528	4328.080920	24.006375
123.991016	4341.830876	24.011392
124.029118	4349.668675	24.016410
124.371816	4346.098658	24.021427
124.241861	4350.749511	24.026445
124.426784	4349.511583	24.031463
124.726860	4374.103876	24.036480
124.580372	4374.189923	24.041498
125.430985	4381.038727	24.046515
125.137496	4386.494856	24.051533
124.901729	4379.773769	24.056551
125.100786	4384.051126	24.061568
125.309747	4396.101309	24.066586
125.702880	4395.361046	24.071603
125.717287	4405.904517	24.076621
125.842053	4417.014651	24.081639
126.265301	4416.124471	24.086656
126.102828	4423.163572	24.091674
126.197498	4424.767979	24.096691
126.371723	4429.964614	24.101709
126.494661	4429.980043	24.106727
126.558376	4443.890081	24.111744
126.589852	4457.069721	24.116762
126.613816	4441.444532	24.121779
126.503705	4458.999135	24.126797
127.280495	4467.055843	24.131815
127.285573	4470.814382	24.136832
127.078812	4474.492478	24.141850
127.285122	4481.372819	24.146867
127.608835	4506.163602	24.151885
127.880850	4502.008053	24.156903
127.806339	4495.397389	24.161920
127.932866	4513.038074	24.166938
128.699874	4521.642411	24.171955
128.314711	4530.411476	24.176973
128.257848	4526.777763	24.181991
128.751780	4526.709818	24.187008
128.590592	4527.969226	24.192026
128.678598	4539.268271	24.197043
129.020971	4545.559151	24.202061
129.180207	4550.379389	24.207079
129.577388	4541.772504	24.212096
129.171249	4547.590388	24.217114
129.593405	4560.873034	24.222131
129.543821	4563.418593	24.227149
129.955266	4575.673911	24.232167
129.966366	4566.534079	24.237184
129.929491	4576.586956	24.242202
130.241010	4577.027377	24.247219
130.176359	4592.816817	24.252237
130.119025	4595.253117	24.257255
130.376545	4592.084647	24.262272
130.471224	4610.993018	24.267290
130.604182	4619.409494	24.272307
130.922037	4619.154492	24.277325
130.932996	4613.502598	24.282343
131.048152	4624.383940	24.287360
130.708176	4640.907831	24.292378
131.241518	4646.060893	24.297395
131.321228	4655.139126	24.302413
131.165710	4670.497801	24.307431
131.755547	4665.077165	24.312448
131.693682	4672.084818	24.317466
132.008961	4683.398850	24.322483
132.116146	4691.409051	24.327501
132.459436	4689.249839	24.332519
132.730612	4688.067820	24.337536
132.738530	4700.686310	24.342554
132.446897	4711.388383	24.347571
132.797890	4714.991771	24.352589
132.801326	4722.462691	24.357607
133.109191	4711.833762	24.362624
132.940695	4736.679878	24.367642
133.685768	4746.004290	24.372659
133.833016	4747.868793	24.377677
133.973182	4750.640330	24.382695
134.110954	4745.157919	24.387712
133.748567	4750.902725	24.392730
133.848511	4740.255849	24.397747
134.067160	4744.495500	24.402765
134.238243	4764.758837	24.407783
134.238173	4767.909034	24.412800
134.346299	4775.748672	24.417818
134.568020	4784.110284	24.422835
134.726175	4798.798088	24.427853
134.831476	4799.460214	24.432871
135.338896	4795.971627	24.437888
135.129947	4810.208750	24.442906
135.173099	4821.634946	24.447923
135.420898	4822.741917	24.452941
135.590958	4821.960829	24.457959
135.429256	4830.650837	24.462976
135.446991	4844.161191	24.467994
135.681881	4852.056759	24.473011
136.213654	4867.645675	24.478029
136.007153	4872.068755	24.483047
136.354390	4876.354580	24.488064
136.610152	4878.003233	24.493082
136.951921	4889.594177	24.498099
136.685112	4899.598029	24.503117
137.002451	4903.601297	24.508135
137.235307	4900.174644	24.513152
137.163850	4912.464809	24.518170
137.361944	4916.770852	24.523187
137.471803	4927.135529	24.528205
137.561700	4926.537450	24.533223
137.917192	4938.268321	24.538240
137.885152	4954.469631	24.543258
138.152487	4952.006632	24.548275
138.248533	4951.511756	24.553293
138.376366	4965.484748	24.558311
138.878493	4971.318299	24.563328
138.674303	4980.305439	24.568346
138.875587	4972.676014	24.573363
138.965953	4972.421925	24.578381
138.701157	4984.167933	24.583399
139.088542	4992.200656	24.588416
139.351438	5003.106428	24.593434
139.473903	5007.291765	24.598451
139.410848	5021.379933	24.603469
139.902012	5026.265090	24.608487
140.248563	5028.518223	24.613504
140.289406	5034.515603	24.618522
140.266652	5034.926334	24.623539
140.432396	5043.855550	24.628557
140.391207	5048.634719	24.633575
140.626315	5049.478540	24.638592
140.946256	5055.561621	24.643610
141.161669	5058.592882	24.648627
141.177010	5063.423175	24.653645
141.272497	5074.525672	24.658663
141.397898	5076.904998	24.663680
140.853908	5078.271764	24.668698
141.127469	5092.228337	24.673715
142.032585	5100.981771	24.678733
141.836805	5103.619754	24.683751
141.903764	5109.344757	24.688768
141.904405	5122.406602	24.693786
141.967279	5127.747146	24.698803
142.375129	5118.810034	24.703821
142.150247	5135.392099	24.708839
142.802841	5150.779248	24.713856
142.635622	5154.025144	24.718874
142.755359	5155.332125	24.723891
142.952112	5161.904874	24.728909
142.743430	5179.440891	24.733927
143.139268	5175.499380	24.738944
143.295149	5188.978877	24.743962
143.170557	5197.417030	24.748979
143.490269	5199.049382	24.753997
143.653460	5216.511391	24.759015
144.071591	5227.645506	24.764032
143.851856	5230.508223	24.769050
144.019511	5252.511932	24.774067
144.489450	5254.329090	24.779085
144.504124	5264.128054	24.784103
144.951779	5273.309939	24.789120
145.183948	5286.244087	24.794138
144.912812	5280.288953	24.799155
145.497417	5272.804530	24.804173
145.349902	5286.672545	24.809191
145.361548	5293.119668	24.814208
145.685999	5302.601809	24.819226
145.603808	5304.922145	24.824243
146.304522	5320.314526	24.829261
146.149018	5327.494932	24.834279
146.367984	5333.909589	24.839296
146.744252	5334.699742	24.844314
146.528446	5341.457142	24.849331
147.002246	5342.834933	24.854349
146.881227	5362.724865	24.859367
147.212548	5363.604134	24.864384
147.318836	5363.161304	24.869402
147.127591	5372.541188	24.874419
147.676742	5380.596091	24.879437
147.285711	5386.699125	24.884455
147.614612	5385.362814	24.889472
147.763615	5404.692800	24.894490
147.650550	5417.015075	24.899507
148.199689	5411.196548	24.904525
148.587987	5429.415812	24.909543
148.412048	5431.488851	24.914560
148.659251	5441.734448	24.919578
148.346501	5450.360028	24.924595
148.744785	5466.996284	24.929613
149.071603	5478.170112	24.934631
149.419117	5472.544142	24.939648
149.134977	5482.535243	24.944666
149.289708	5495.544805	24.949683
149.631327	5490.803617	24.954701
149.892038	5507.180521	24.959719
150.053543	5512.628835	24.964736
150.054433	5511.081900	24.969754
150.181432	5526.526457	24.974771
150.297315	5529.990070	24.979789
150.536930	5540.663061	24.984807
150.321822	5539.601366	24.989824
150.775122	5561.043004	24.994842
150.631359	5564.834558	24.999859
151.075852	5569.891322	25.004877
151.203756	5580.960638	25.009895
151.874109	5584.416312	25.014912
152.102642	5587.748648	25.019930
151.670883	5594.461056	25.024947
152.145988	5603.089546	25.029965
151.791654	5615.967449	25.034983
152.120790	5619.094628	25.040000
152.315227	5627.965972	25.045018
152.423471	5644.786723	25.050035
152.873736	5645.363271	25.055053
152.930222	5651.086927	25.060071
152.547791	5655.578794	25.065088
153.005970	5659.146640	25.070106
153.109770	5665.396369	25.075123
153.422688	5672.951774	25.080141
153.206450	5686.546757	25.085159
153.392719	5697.430225	25.090176
153.503975	5702.454002	25.095194
153.504823	5716.598985	25.100211
153.584227	5719.039266	25.105229
153.657379	5738.261534	25.110247
154.428615	5756.582124	25.115264
154.826785	5762.567957	25.120282
154.632929	5773.520493	25.125299
154.881095	5780.360045	25.130317
155.015525	5780.951354	25.135335
155.366013	5800.831027	25.140352
155.574011	5801.833811	25.145370
155.342043	5809.462010	25.150387
155.969524	5811.017791	25.155405
155.927101	5824.459376	25.160423
156.267372	5831.420257	25.165440
156.651191	5823.133695	25.170458
156.315476	5833.398231	25.175475
156.758131	5837.454679	25.180493
157.060119	5861.107980	25.185511
156.949335	5860.089899	25.190528
157.305204	5858.310546	25.195546
157.127714	5857.909006	25.200563
157.280748	5866.414459	25.205581
156.999758	5875.000539	25.210599
157.587653	5892.014695	25.215616
157.849760	5894.716795	25.220634
157.901225	5910.486026	25.225651
158.145613	5903.506061	25.230669
157.897011	5916.383393	25.235687
158.167609	5933.965002	25.240704
158.884273	5941.930777	25.245722
158.874785	5944.246118	25.250739
158.936637	5956.134134	25.255757
159.277822	5971.327697	25.260775
159.009399	5971.451792	25.265792
159.470891	5971.846658	25.270810
159.578097	5993.747088	25.275827
159.930100	5982.387615	25.280845
159.774482	5985.284598	25.285863
159.834720	6011.734960	25.290880
160.086973	6016.187460	25.295898
160.425557	6022.473134	25.300915
160.572280	6028.637344	25.305933
160.627935	6038.165135	25.310951
160.729948	6036.450789	25.315968
160.983933	6040.650484	25.320986
161.196520	6058.575916	25.326003
160.961916	6060.127880	25.331021
161.362279	6084.637323	25.336039
161.296910	6096.068690	25.341056
161.837755	6093.660552	25.346074
161.902687	6115.643512	25.351091
161.813422	6120.550450	25.356109
161.832263	6127.366081	25.361127
162.244451	6147.473223	25.366144
162.597262	6150.334775	25.371162
162.457981	6156.262881	25.376179
163.087997	6173.324367	25.381197
162.884623	6168.441099	25.386215
163.067098	6183.082012	25.391232
163.605769	6187.170849	25.396250
163.626397	6203.241900	25.401267
163.652556	6203.976456	25.406285
163.987028	6204.384914	25.411303
163.911729	6207.019963	25.416320
164.152858	6210.637707	25.421338
164.215329	6230.057884	25.426355
164.581064	6231.455833	25.431373
164.663696	6237.715387	25.436391
164.870672	6245.912671	25.441408
165.287557	6256.214220	25.446426
164.839686	6259.163344	25.451443
165.393239	6261.084309	25.456461
165.546366	6277.756555	25.461479
165.607138	6285.395912	25.466496
165.730891	6289.177272	25.471514
165.808094	6306.723244	25.476531
165.562977	6304.697067	25.481549
165.923414	6328.673280	25.486567
166.246728	6334.083863	25.491584
166.651637	6339.901520	25.496602
166.725484	6362.233785	25.501619
166.634313	6356.407944	25.506637
167.180666	6363.971261	25.511655
167.192498	6383.522650	25.516672
167.252995	6384.011916	25.521690
167.436950	6406.822605	25.526707
167.875307	6412.897061	25.531725
167.884195	6418.022306	25.536743
167.865137	6436.694682	25.541760
168.306499	6446.171730	25.546778
168.618504	6453.680250	25.551795
168.648175	6458.082495	25.556813
168.789125	6465.542054	25.561831
168.598306	6474.240559	25.566848
169.414020	6480.716817	25.571866
169.552586	6496.580238	25.576883
169.559029	6495.900478	25.581901
169.842119	6515.693627	25.586919
169.847043	6515.699137	25.591936
170.132675	6516.936031	25.596954
170.292061	6538.207041	25.601971
170.270121	6546.178305	25.606989
170.396009	6551.042180	25.612007
170.389196	6560.624226	25.617024
170.963463	6569.051387	25.622042
171.037081	6581.796626	25.627059
171.565928	6592.746919	25.632077
171.426487	6601.762590	25.637095
171.486107	6604.010365	25.642112
172.002213	6608.153342	25.647130
171.914636	6626.997645	25.652147
172.108503	6624.220780	25.657165
172.194965	6627.102036	25.662183
172.477689	6647.848754	25.667200
172.483798	6656.178709	25.672218
172.864815	6661.261508	25.677236
172.881520	6662.941464	25.682253
173.411268	6677.020114	25.687271
173.353036	6679.087478	25.692288
173.689387	6687.321516	25.697306
174.141707	6695.654193	25.702324
173.936680	6710.091058	25.707341
174.101806	6701.497423	25.712359
174.110309	6716.159703	25.717376
174.436293	6716.260131	25.722394
174.462679	6727.020888	25.727412
174.436754	6734.194170	25.732429
174.478499	6739.686867	25.737447
174.379956	6751.376389	25.742464
175.211966	6754.608083	25.747482
175.296526	6774.770399	25.752500
175.431384	6779.238320	25.757517
175.628314	6787.450049	25.762535
175.399169	6804.567800	25.767552
175.865461	6812.980421	25.772570
176.524099	6827.424135	25.777588
176.365993	6838.261212	25.782605
176.513256	6834.816043	25.787623
176.708523	6840.796136	25.792640
176.901339	6848.471865	25.797658
177.056779	6861.179225	25.802676
176.861290	6872.359966	25.807693
177.555445	6874.587289	25.812711
177.626450	6898.978947	25.817728
177.871994	6895.512056	25.822746
177.586065	6913.488010	25.827764
177.446823	6924.236946	25.832781
178.351777	6943.929978	25.837799
178.185636	6958.430397	25.842816
178.925292	6972.321701	25.847834
178.987445	6974.853246	25.852852
178.858895	6975.763602	25.857869
179.178633	6986.446984	25.862887
178.919482	7010.530624	25.867904
179.306021	7003.954158	25.872922
179.582893	7028.086438	25.877940
179.770577	7039.614495	25.882957
180.150295	7049.035219	25.887975
179.882472	7065.224822	25.892992
180.394823	7065.804322	25.898010
180.479260	7089.212323	25.903028
180.809818	7097.936778	25.908045
181.176423	7113.057854	25.913063
181.099180	7116.785636	25.918080
181.650114	7126.394249	25.923098
181.566304	7142.400401	25.928116
181.616107	7154.878272	25.933133
182.127760	7159.214648	25.938151
182.487493	7169.692984	25.943168
183.038797	7167.447233	25.948186
182.446767	7172.262739	25.953204
182.947426	7183.621892	25.958221
183.158797	7188.204205	25.963239
182.945027	7211.981088	25.968256
182.911211	7207.986495	25.973274
183.153943	7221.277093	25.978292
183.333115	7229.520214	25.983309
183.936280	7232.415327	25.988327
183.586228	7249.871285	25.993344
183.873513	7263.669518	25.998362
184.237610	7278.257596	26.003380
184.477610	7277.342330	26.008397
184.828264	7294.865347	26.013415
184.948504	7300.137555	26.018432
185.254625	7305.570063	26.023450
185.579672	7316.565346	26.028468
185.660464	7323.100215	26.033485
185.761975	7331.399746	26.038503
185.942765	7337.694810	26.043520
186.014315	7353.089609	26.048538
185.978872	7353.202467	26.053556
186.097150	7376.731811	26.058573
186.912559	7380.547106	26.063591
186.673362	7394.431073	26.068608
186.835426	7390.914028	26.073626
187.041611	7398.818352	26.078644
187.056826	7418.026199	26.083661
187.462418	7426.417042	26.088679
187.555186	7438.730525	26.093696
187.617364	7439.721518	26.098714
188.134585	7450.491042	26.103732
187.969857	7465.572524	26.108749
188.352253	7469.458831	26.113767
188.242877	7480.771672	26.118784
188.259170	7496.323626	26.123802
188.590650	7509.221689	26.128820
188.754434	7524.725305	26.133837
189.209467	7538.396441	26.138855
189.553469	7543.150642	26.143872
189.665836	7555.192786	26.148890
190.220165	7563.835052	26.153908
190.027017	7577.579347	26.158925
190.604628	7584.573170	26.163943
190.313515	7591.491570	26.168960
190.440799	7610.915679	26.173978
190.369576	7617.569178	26.178996
190.481783	7629.933412	26.184013
190.813311	7647.020935	26.189031
191.035959	7653.448459	26.194048
191.151051	7670.522555	26.199066
191.769663	7684.067148	26.204084
191.912745	7689.007558	26.209101
192.261453	7702.966978	26.214119
192.230185	7718.040386	26.219136
192.415402	7731.747621	26.224154
192.802323	7743.282791	26.229172
192.704939	7760.551266	26.234189
193.030345	7771.281573	26.239207
193.646339	7780.021620	26.244224
193.610258	7797.021647	26.249242
193.730700	7807.891425	26.254260
193.982647	7804.278137	26.259277
194.235094	7823.193519	26.264295
194.472272	7842.704839	26.269312
194.341896	7839.546071	26.274330
194.692755	7856.270855	26.279348
194.535108	7866.802228	26.284365
195.148183	7870.270479	26.289383
195.208254	7888.313144	26.294400
195.547059	7895.568649	26.299418
195.956872	7911.381325	26.304436
195.699110	7917.028635	26.309453
196.207393	7930.322343	26.314471
196.270015	7943.477510	26.319488
196.262020	7950.503229	26.324506
196.825229	7970.298259	26.329524
196.695183	7979.095291	26.334541
197.298773	7994.274678	26.339559
197.071669	8001.271601	26.344576
197.382287	8011.436089	26.349594
197.648326	8016.650934	26.354612
197.710746	8033.421065	26.359629
197.992790	8041.275896	26.364647
198.206059	8050.439072	26.369664
198.263551	8064.659070	26.374682
198.641154	8064.697753	26.379700
198.686701	8076.927503	26.384717
198.760129	8099.700776	26.389735
199.347341	8103.160495	26.394752
199.388858	8115.965495	26.399770
200.061611	8129.508249	26.404788
200.123497	8143.497151	26.409805
200.259477	8135.491482	26.414823
200.347799	8147.941890	26.419840
200.202688	8162.481000	26.424858
200.681241	8160.612757	26.429876
200.606868	8167.355346	26.434893
200.484480	8190.775045	26.439911
200.811619	8201.063334	26.444928
200.758156	8222.237033	26.449946
201.386175	8236.923439	26.454964
201.517951	8249.518650	26.459981
201.760456	8262.459593	26.464999
202.022455	8274.055709	26.470016
202.120927	8289.734370	26.475034
202.508855	8298.870307	26.480052
202.271268	8315.911850	26.485069
202.727666	8327.562788	26.490087
203.371288	8341.855348	26.495104
203.508226	8353.114349	26.500122
203.250787	8361.303246	26.505140
203.396642	8375.260225	26.510157
203.795265	8391.030866	26.515175
204.151819	8402.817465	26.520192
204.658004	8418.640736	26.525210
204.637437	8424.715143	26.530228
204.683134	8437.503925	26.535245
204.689496	8452.603607	26.540263
205.365515	8472.059472	26.545280
205.770971	8478.663862	26.550298
206.130788	8483.930449	26.555316
206.094479	8505.019697	26.560333
206.155048	8504.962819	26.565351
206.502516	8510.973284	26.570368
206.866368	8528.280719	26.575386
206.722081	8525.761763	26.580404
207.086988	8544.167745	26.585421
207.190844	8552.934720	26.590439
207.284779	8549.459701	26.595456
207.419324	8578.557294	26.600474
207.686484	8587.548120	26.605492
207.723886	8595.968764	26.610509
207.921253	8614.925156	26.615527
207.970819	8628.749023	26.620544
208.465858	8644.425846	26.625562
208.797227	8648.847651	26.630580
208.889703	8665.405271	26.635597
209.211735	8685.721902	26.640615
209.632771	8691.342037	26.645632
209.710784	8694.044980	26.650650
209.824975	8710.807614	26.655668
209.904674	8725.753956	26.660685
209.961949	8738.919997	26.665703
210.545616	8747.400365	26.670720
210.554275	8770.954969	26.675738
210.729027	8767.770342	26.680756
210.569330	8802.269023	26.685773
210.647300	8811.049647	26.690791
211.437712	8821.650889	26.695808
211.215163	8851.802535	26.700826
211.841956	8863.022993	26.705844
212.183843	8875.724632	26.710861
212.321272	8889.222362	26.715879
212.500603	8897.418845	26.720896
212.837546	8911.883024	26.725914
213.045961	8920.520132	26.730932
213.363769	8936.038689	26.735949
213.405938	8953.321141	26.740967
213.800742	8952.602553	26.745984
213.625930	8960.428314	26.751002
214.118301	8971.846702	26.756020
214.529258	8972.833656	26.761037
214.504912	8985.393836	26.766055
214.961190	9001.623240	26.771072
214.946201	9006.165693	26.776090
214.907475	9005.773913	26.781108
214.892221	9034.374740	26.786125
215.259102	9040.524414	26.791143
215.468154	9053.881595	26.796160
215.404006	9071.607044	26.801178
215.781227	9092.158585	26.806196
216.339152	9104.886526	26.811213
216.359767	9119.289917	26.816231
216.770119	9133.262862	26.821248
216.941290	9150.086427	26.826266
217.154347	9151.587457	26.831284
217.437467	9176.387751	26.836301
217.522038	9190.152877	26.841319
217.685706	9205.086450	26.846336
217.711156	9217.733705	26.851354
217.964822	9226.363867	26.856372
218.122342	9251.881700	26.861389
218.433871	9269.921046	26.866407
219.002561	9285.520571	26.871424
218.999641	9297.155672	26.876442
219.719299	9308.797562	26.881460
220.370995	9316.045656	26.886477
219.939244	9325.424173	26.891495
220.392988	9333.915693	26.896512
220.212982	9350.620801	26.901530
220.326752	9368.880663	26.906548
220.637230	9383.680874	26.911565
220.703342	9400.356942	26.916583
221.220861	9403.872031	26.921600
221.461600	9426.598620	26.926618
221.349428	9430.632284	26.931636
221.758231	9459.063140	26.936653
222.111709	9466.588497	26.941671
222.182729	9477.725898	26.946688
222.319961	9488.852933	26.951706
222.526382	9510.697788	26.956724
223.270704	9522.026529	26.961741
223.065974	9543.039144	26.966759
223.632876	9549.621784	26.971776
223.237938	9565.792431	26.976794
223.726328	9578.165338	26.981812
224.236332	9596.726447	26.986829
224.201041	9611.922002	26.991847
224.512020	9619.103612	26.996864
224.654031	9638.429659	27.001882
225.241046	9649.719975	27.006900
225.338294	9662.312081	27.011917
225.475183	9674.771691	27.016935
225.625529	9688.552141	27.021952
225.984553	9692.275243	27.026970
226.322408	9710.954998	27.031988
226.432320	9724.104018	27.037005
226.489503	9739.815630	27.042023
227.114637	9744.403224	27.047040
227.320405	9763.501554	27.052058
227.358763	9778.786744	27.057076
227.513771	9784.745683	27.062093
227.890607	9798.200253	27.067111
228.373533	9803.343739	27.072128
228.136539	9823.414506	27.077146
228.429206	9832.790301	27.082164
228.827264	9840.814010	27.087181
228.513688	9866.229669	27.092199
229.515055	9867.083137	27.097216
229.189940	9877.926047	27.102234
229.487089	9884.118501	27.107252
229.636821	9889.721513	27.112269
229.750568	9912.746440	27.117287
230.166180	9919.895989	27.122304
230.337541	9936.578150	27.127322
230.452837	9951.156797	27.132340
231.112971	9961.498095	27.137357
231.355267	9983.063188	27.142375
231.128076	9981.810517	27.147392
231.324629	9998.810845	27.152410
231.661141	10002.439657	27.157428
232.007253	10030.297082	27.162445
231.727992	10035.847359	27.167463
231.944865	10057.561763	27.172480
232.407129	10082.227846	27.177498
232.625761	10109.836978	27.182516
233.068859	10127.487124	27.187533
233.250138	10139.955878	27.192551
233.642820	10150.408643	27.197568
234.117133	10170.238897	27.202586
233.996971	10189.597114	27.207604
234.332965	10197.482300	27.212621
234.493862	10216.060827	27.217639
234.737379	10223.426899	27.222656
235.209301	10241.413644	27.227674
235.082067	10245.819267	27.232692
235.322862	10268.259543	27.237709
235.464184	10291.334295	27.242727
236.017724	10299.687483	27.247744
236.131874	10317.209364	27.252762
236.169061	10332.059457	27.257780
236.786218	10345.606233	27.262797
237.149740	10367.544308	27.267815
237.289480	10375.602400	27.272832
237.957485	10379.662452	27.277850
237.970513	10407.320020	27.282868
238.196941	10411.221914	27.287885
238.049304	10423.271917	27.292903
238.319689	10433.175650	27.297920
238.681940	10447.605484	27.302938
239.524951	10473.904862	27.307956
239.589737	10464.794748	27.312973
239.679301	10484.641404	27.317991
239.525238	10498.201751	27.323008
239.766379	10518.675144	27.328026
240.064428	10528.451451	27.333044
240.643476	10541.439144	27.338061
240.818788	10558.582240	27.343079
240.745162	10575.353871	27.348096
241.225426	10590.592601	27.353114
241.341520	10605.515803	27.358132
241.486630	10614.820382	27.363149
241.743611	10631.432916	27.368167
241.948132	10644.072030	27.373184
242.038739	10658.411965	27.378202
242.090714	10680.702336	27.383220
242.245388	10701.258941	27.388237
242.834602	10729.227730	27.393255
242.978495	10734.121462	27.398272
243.384684	10752.046373	27.403290
243.485602	10781.493688	27.408308
243.883276	10795.697213	27.413325
244.074465	10812.329687	27.418343
243.946379	10819.069017	27.423360
244.285218	10836.916148	27.428378
244.460064	10855.641531	27.433396
244.790396	10865.476108	27.438413
245.026002	10880.990219	27.443431
245.263571	10900.065784	27.448448
245.377852	10907.922852	27.453466
245.650982	10939.743198	27.458484
245.770738	10958.900430	27.463501
246.317773	10974.548972	27.468519
246.484216	11001.526604	27.473536
246.853695	11009.662654	27.478554
246.712755	11029.486001	27.483572
247.463628	11039.456877	27.488589
247.832706	11061.022298	27.493607
248.019497	11077.687273	27.498624
248.204296	11097.908044	27.503642
248.447092	11118.306052	27.508660
248.999737	11130.452051	27.513677
248.840110	11149.350112	27.518695
249.387698	11155.352192	27.523712
249.771701	11179.166795	27.528730
249.749123	11190.537755	27.533748
249.988492	11205.385286	27.538765
250.226534	11227.808198	27.543783
250.568586	11238.825249	27.548800
250.942875	11250.623508	27.553818
251.087293	11267.317392	27.558836
251.312787	11283.603885	27.563853
251.576335	11293.098651	27.568871
251.770871	11324.875124	27.573888
252.283649	11323.923253	27.578906
252.231312	11345.176099	27.583924
252.499764	11359.416084	27.588941
252.870994	11377.981760	27.593959
253.085622	11403.165185	27.598976
253.415793	11416.988207	27.603994
253.664674	11434.644752	27.609012
253.909274	11446.100319	27.614029
253.971945	11456.204489	27.619047
254.309048	11473.711471	27.624064
254.617689	11497.222516	27.629082
255.062930	11514.971525	27.634100
255.149673	11529.350623	27.639117
255.252958	11543.809241	27.644135
255.180575	11564.714972	27.649152
255.798451	11578.875124	27.654170
255.985556	11609.904870	27.659188
255.980813	11620.692279	27.664205
256.272780	11646.107057	27.669223
256.658901	11660.366730	27.674240
257.229250	11676.520599	27.679258
257.014135	11707.534571	27.684276
257.722295	11723.212181	27.689293
258.010526	11740.913373	27.694311
258.279182	11758.399765	27.699328
258.897140	11754.444192	27.704346
258.540796	11776.294591	27.709364
258.782024	11792.582218	27.714381
259.128976	11820.574798	27.719399
259.238209	11833.198063	27.724416
260.159416	11845.570988	27.729434
259.867128	11873.670101	27.734452
260.178450	11881.139884	27.739469
260.758254	11898.091372	27.744487
261.087395	11912.075965	27.749504
261.204962	11928.572547	27.754522
261.429458	11946.236550	27.759540
261.964269	11968.882265	27.764557
262.096846	11974.614900	27.769575
261.916466	11982.793302	27.774592
262.689470	11995.268487	27.779610
262.631794	12014.141970	27.784628
262.731324	12027.988942	27.789645
263.029391	12038.871254	27.794663
262.963876	12060.588005	27.799680
263.458679	12081.310724	27.804698
263.570982	12107.910017	27.809716
264.015592	12116.909485	27.814733
263.976787	12136.768521	27.819751
264.246275	12161.593853	27.824768
265.048536	12182.543247	27.829786
264.921924	12192.513259	27.834804
265.246129	12220.449999	27.839821
265.510042	12238.029156	27.844839
265.607972	12248.017705	27.849856
266.206031	12272.782239	27.854874
266.617821	12291.588773	27.859892
266.876094	12310.394111	27.864909
267.115308	12331.586607	27.869927
267.137739	12347.937410	27.874944
267.705123	12355.323060	27.879962
267.837038	12380.789165	27.884980
268.180279	12392.918263	27.889997
268.165076	12417.564323	27.895015
268.654422	12434.037843	27.900032
268.779759	12453.833605	27.905050
268.706367	12481.030923	27.910068
269.261057	12497.765837	27.915085
269.328008	12518.792900	27.920103
269.532706	12547.402519	27.925120
270.148498	12560.047970	27.930138
270.503371	12579.732118	27.935156
270.137503	12606.467017	27.940173
270.658713	12636.037706	27.945191
270.951396	12654.291685	27.950208
271.578591	12668.748041	27.955226
271.996059	12695.050884	27.960244
271.825223	12718.783826	27.965261
272.494988	12728.130421	27.970279
272.977829	12750.791534	27.975296
273.230794	12760.973962	27.980314
273.401769	12783.860811	27.985332
273.640865	12804.880172	27.990349
274.077767	12817.787503	27.995367
274.185779	12841.644286	28.000384
274.619087	12838.847948	28.005402
274.399377	12861.682407	28.010420
274.618201	12891.367180	28.015437
275.492711	12910.414479	28.020455
275.695253	12935.004997	28.025472
275.962686	12947.285276	28.030490
276.215640	12979.538547	28.035508
276.032491	12984.667257	28.040525
276.629665	13000.571744	28.045543
276.845589	13022.794990	28.050560
276.955518	13041.321133	28.055578
277.364640	13069.792149	28.060596
277.576037	13079.886523	28.065613
278.073463	13096.084615	28.070631
278.274201	13126.429442	28.075648
278.735195	13142.958550	28.080666
279.147023	13155.753197	28.085684
279.117614	13180.996171	28.090701
279.815324	13190.565993	28.095719
279.419349	13208.366268	28.100736
280.138270	13228.369862	28.105754
280.284252	13241.342004	28.110772
280.596993	13246.257310	28.115789
280.589001	13264.612665	28.120807
281.046862	13293.837455	28.125824
281.274352	13303.424151	28.130842
281.410103	13321.239134	28.135860
281.579245	13342.674273	28.140877
282.096217	13359.602182	28.145895
282.248709	13382.025266	28.150912
282.473541	13395.004109	28.155930
283.010181	13424.813622	28.160948
282.712928	13440.305941	28.165965
283.568712	13465.641162	28.170983
283.286167	13485.309257	28.176000
284.031041	13497.303516	28.181018
284.540102	13524.717417	28.186036
284.177053	13543.836056	28.191053
284.851924	13566.597545	28.196071
284.833350	13599.270208	28.201088
285.347664	13598.636955	28.206106
285.710719	13633.899483	28.211124
285.680847	13661.135887	28.216141
286.256521	13676.876936	28.221159
286.504677	13705.487812	28.226176
286.636749	13717.401354	28.231194
286.952879	13742.309879	28.236212
287.411811	13767.284492	28.241229
287.810110	13789.416906	28.246247
287.951062	13815.028792	28.251264
288.214056	13834.510732	28.256282
288.613675	13864.705578	28.261300
289.071054	13882.309643	28.266317
289.315026	13900.253489	28.271335
289.778239	13922.884341	28.276352
290.017887	13942.199512	28.281370
290.265587	13952.901332	28.286388
290.287519	13981.813341	28.291405
290.601852	13998.129313	28.296423
290.775095	14025.501800	28.301440
291.702635	14043.711357	28.306458
291.957647	14069.539418	28.311476
291.441887	14094.891370	28.316493
292.502621	14103.511045	28.321511
292.506809	14128.750013	28.326528
292.977817	14145.865838	28.331546
293.080302	14166.889159	28.336564
292.972192	14188.179194	28.341581
293.767633	14206.756995	28.346599
294.044453	14225.567646	28.351616
294.321587	14239.255769	28.356634
294.479887	14260.570473	28.361652
294.776241	14295.099356	28.366669
295.357510	14307.195553	28.371687
295.598518	14339.642493	28.376704
296.058726	14353.122006	28.381722
296.170376	14372.726107	28.386740
296.439962	14383.756348	28.391757
296.789806	14398.405910	28.396775
296.998976	14432.901326	28.401792
297.341201	14444.817144	28.406810
297.467240	14464.106426	28.411828
297.664985	14497.912110	28.416845
298.103422	14509.149679	28.421863
298.263499	14541.041167	28.426880
298.401361	14561.295100	28.431898
299.190557	14576.570777	28.436916
299.054003	14608.306718	28.441933
299.457074	14627.792792	28.446951
299.775443	14648.694397	28.451968
299.932287	14666.084136	28.456986
300.232245	14677.157163	28.462004
300.499312	14703.723215	28.467021
301.030336	14721.329155	28.472039
301.209659	14741.485196	28.477056
301.379011	14767.671867	28.482074
302.020317	14791.990771	28.487092
301.991390	14808.345417	28.492109
302.486274	14833.397912	28.497127
302.701020	14857.183654	28.502144
302.866750	14877.992565	28.507162
303.507923	14901.945274	28.512180
303.317063	14925.867277	28.517197
304.115730	14951.990361	28.522215
304.264124	14977.940576	28.527232
304.246401	14995.856965	28.532250
304.800310	15015.866187	28.537268
305.104192	15050.139435	28.542285
305.232125	15067.363521	28.547303
305.315703	15093.687247	28.552320
305.717930	15115.744789	28.557338
306.052757	15131.575306	28.562356
306.501053	15165.933521	28.567373
306.797281	15186.842341	28.572391
307.010165	15218.856177	28.577408
307.234364	15254.778272	28.582426
308.261513	15264.404924	28.587444
308.475152	15298.335865	28.592461
308.779597	15327.215128	28.597479
308.917828	15345.890677	28.602496
309.282611	15373.513023	28.607514
309.483386	15393.584274	28.612532
309.702262	15414.047502	28.617549
310.170496	15434.231658	28.622567
310.391196	15464.532863	28.627584
310.417829	15488.115139	28.632602
311.180150	15504.169566	28.637620
311.634247	15540.220417	28.642637
311.710209	15551.821742	28.647655
311.733703	15585.533467	28.652672
312.049559	15609.793850	28.657690
312.731105	15630.538571	28.662708
313.196351	15666.985868	28.667725
313.455875	15671.865925	28.672743
313.531864	15700.535184	28.677760
313.755471	15722.889868	28.682778
314.272139	15749.168761	28.687796
314.617805	15786.152991	28.692813
315.301869	15806.161603	28.697831
315.458854	15828.646865	28.702848
315.608140	15846.196780	28.707866
316.294969	15868.172707	28.712884
316.040049	15893.277717	28.717901
316.538556	15916.938205	28.722919
317.028848	15936.058209	28.727936
317.152098	15954.534558	28.732954
317.700037	15986.133970	28.737972
317.661416	16013.741469	28.742989
317.956792	16033.394292	28.748007
318.533093	16055.144548	28.753024
318.659384	16083.376951	28.758042
319.447315	16099.431026	28.763060
318.883224	16130.980622	28.768077
319.688681	16156.501026	28.773095
320.006621	16170.626324	28.778112
320.410416	16194.965267	28.783130
320.870871	16212.567844	28.788148
321.049365	16241.484005	28.793165
321.211293	16261.369582	28.798183
321.222362	16278.843630	28.803200
321.815972	16289.539953	28.808218
322.209160	16323.327715	28.813236
322.401240	16349.260306	28.818253
322.593394	16369.052822	28.823271
323.373608	16396.933732	28.828288
323.542669	16412.832334	28.833306
324.064410	16430.943503	28.838324
323.881620	16447.677398	28.843341
324.111111	16473.057875	28.848359
324.696942	16498.474163	28.853376
324.856893	16531.310213	28.858394
325.538083	16545.584190	28.863412
325.389428	16567.028504	28.868429
325.583254	16592.686358	28.873447
326.407528	16624.505691	28.878464
326.431906	16663.092772	28.883482
327.055318	16681.425142	28.888500
327.164924	16701.303577	28.893517
327.490935	16724.783618	28.898535
327.521832	16762.747644	28.903552
328.015036	16788.943195	28.908570
328.513630	16817.203635	28.913588
329.164347	16847.717612	28.918605
329.246903	16870.117833	28.923623
329.910082	16887.057559	28.928640
330.262042	16914.298783	28.933658
330.560212	16938.250914	28.938676
330.720301	16961.188688	28.943693
331.083561	16984.239960	28.948711
331.722086	17015.397306	28.953728
331.586962	17042.519176	28.958746
332.013232	17055.775335	28.963764
331.889262	17090.766754	28.968781
332.299155	17122.010623	28.973799
332.911598	17151.403453	28.978816
333.323354	17186.203734	28.983834
333.613857	17195.747768	28.988852
334.009628	17227.632062	28.993869
334.468534	17248.830347	28.998887
334.751024	17278.470890	29.003904
335.179868	17304.146572	29.008922
335.344730	17331.247125	29.013940
335.300890	17370.358003	29.018957
335.404757	17396.375308	29.023975
335.799280	17420.489828	29.028992
336.319292	17451.975991	29.034010
337.005734	17479.374089	29.039028
337.214211	17510.643819	29.044045
337.926042	17545.277712	29.049063
338.281391	17565.772388	29.054080
338.538809	17587.564851	29.059098
338.603998	17621.163045	29.064116
339.175055	17644.327854	29.069133
339.608069	17673.882251	29.074151
340.433795	17691.795372	29.079168
340.122618	17714.409864	29.084186
340.749870	17732.644713	29.089204
340.875756	17755.727771	29.094221
341.625874	17781.669633	29.099239
341.989545	17799.661549	29.104256
341.985198	17831.919068	29.109274
342.818330	17845.314197	29.114292
343.060327	17863.925390	29.119309
342.791497	17900.728803	29.124327
343.201122	17907.727541	29.129344
343.476243	17932.227816	29.134362
343.903430	17955.693503	29.139380
344.269393	17987.090953	29.144397
344.432388	18009.808402	29.149415
344.824417	18030.601064	29.154432
345.051420	18059.941937	29.159450
345.614005	18078.256735	29.164468
345.655322	18104.809144	29.169485
345.614031	18128.544267	29.174503
346.464806	18154.205525	29.179520
346.796613	18186.284625	29.184538
347.024888	18208.164480	29.189556
347.503493	18242.899329	29.194573
347.513072	18257.794663	29.199591
347.554914	18291.858858	29.204608
348.205529	18329.776259	29.209626
348.661121	18357.887746	29.214644
349.132648	18381.315415	29.219661
349.396268	18417.278284	29.224679
350.062583	18451.421833	29.229696
350.365925	18479.007709	29.234714
350.531329	18510.405832	29.239732
350.847895	18541.085382	29.244749
351.099823	18568.755250	29.249767
351.720230	18592.621044	29.254784
351.940181	18627.093847	29.259802
352.333452	18649.504311	29.264820
352.549047	18683.485114	29.269837
352.892934	18719.897162	29.274855
353.168250	18730.549937	29.279872
353.530702	18769.650528	29.284890
354.228739	18797.320338	29.289908
354.444711	18831.408741	29.294925
354.774420	18861.290698	29.299943
355.459896	18886.479713	29.304960
355.636437	18928.149496	29.309978
356.410786	18948.775852	29.314996
356.569100	18968.247798	29.320013
356.681444	19002.169515	29.325031
357.230959	19035.991224	29.330048
357.388133	19059.885928	29.335066
357.737596	19084.950934	29.340084
358.473583	19114.245257	29.345101
358.572705	19153.849071	29.350119
358.974958	19174.805621	29.355136
359.302862	19210.027007	29.360154
359.887674	19233.210513	29.365172
360.158375	19250.119021	29.370189
360.258263	19285.837468	29.375207
360.818406	19317.693128	29.380224
361.264286	19341.100698	29.385242
361.229727	19371.918689	29.390260
362.100367	19408.514866	29.395277
361.859334	19442.334751	29.400295
362.359196	19468.886686	29.405312
362.047010	19498.800667	29.410330
362.994003	19538.758935	29.415348
363.689636	19575.376519	29.420365
363.796831	19603.335882	29.425383
364.580283	19628.302015	29.430400
364.949435	19665.394217	29.435418
365.452052	19689.450394	29.440436
365.703848	19717.854805	29.445453
365.828297	19740.637171	29.450471
366.189552	19753.924314	29.455488
366.392657	19786.158885	29.460506
366.549334	19814.275068	29.465524
367.379523	19845.767066	29.470541
367.447143	19881.592744	29.475559
368.119825	19905.275051	29.480576
368.150590	19927.895402	29.485594
368.483374	19965.379274	29.490612
368.936745	19993.967328	29.495629
369.035168	20027.703458	29.500647
369.248850	20055.918467	29.505664
369.633187	20087.278510	29.510682
370.126660	20123.012650	29.515700
370.463109	20162.379145	29.520717
371.009258	20191.243592	29.525735
371.366205	20216.378376	29.530752
371.875242	20246.682953	29.535770
371.984849	20281.175955	29.540788
372.742237	20312.098829	29.545805
372.865655	20344.018249	29.550823
373.575620	20372.598254	29.555840
374.038806	20405.987258	29.560858
374.046039	20438.638997	29.565876
374.820282	20453.422544	29.570893
374.884229	20497.672211	29.575911
375.026598	20528.514849	29.580928
375.406201	20559.092917	29.585946
375.663808	20606.945535	29.590964
376.372375	20640.056403	29.595981
376.778554	20674.648962	29.600999
377.093150	20698.230360	29.606016
377.851556	20733.582920	29.611034
378.017574	20776.648324	29.616052
378.675637	20793.465897	29.621069
378.601392	20826.579648	29.626087
378.988078	20861.630515	29.631104
379.362322	20891.167397	29.636122
379.741626	20926.857699	29.641140
380.630679	20960.844375	29.646157
380.461159	20984.546176	29.651175
381.099942	21015.532967	29.656192
381.184850	21047.838668	29.661210
381.528077	21087.180678	29.666228
382.248379	21115.279940	29.671245
382.518299	21163.789106	29.676263
382.756175	21181.544785	29.681280
383.290307	21228.521552	29.686298
383.412529	21266.059840	29.691316
384.180691	21291.801354	29.696333
384.647771	21318.740043	29.701351
385.090078	21355.192118	29.706368
385.744978	21392.514519	29.711386
385.554886	21430.158906	29.716404
385.961094	21454.030152	29.721421
386.242597	21484.953590	29.726439
386.789404	21524.157167	29.731456
387.232122	21553.159868	29.736474
387.465482	21594.731626	29.741492
388.098326	21621.802731	29.746509
388.298615	21669.357288	29.751527
388.428888	21700.222609	29.756544
388.988522	21727.273732	29.761562
389.337267	21766.957442	29.766580
389.832927	21793.285705	29.771597
390.157393	21830.787067	29.776615
390.962439	21864.175544	29.781632
391.196112	21898.923645	29.786650
391.585415	21929.224292	29.791668
392.518751	21949.911056	29.796685
392.344119	21997.303970	29.801703
392.929476	22024.534716	29.806720
393.069216	22048.675896	29.811738
393.236466	22085.027067	29.816756
393.744142	22112.611319	29.821773
394.198254	22141.126548	29.826791
394.372106	22180.762656	29.831808
395.303593	22195.541845	29.836826
395.311932	22231.981365	29.841844
395.532919	22263.421008	29.846861
395.856595	22299.741752	29.851879
396.630077	22330.147127	29.856896
397.154703	22363.030627	29.861914
396.757136	22402.371228	29.866932
397.343133	22436.698588	29.871949
397.815570	22462.841812	29.876967
397.998872	22499.001659	29.881984
398.681196	22539.380301	29.887002
398.941701	22587.502654	29.892020
399.709879	22613.125829	29.897037
400.006709	22653.691465	29.902055
400.149567	22695.804184	29.907072
400.804282	22730.393006	29.912090
400.681544	22779.757510	29.917108
401.767473	22803.252196	29.922125
402.090988	22845.911968	29.927143
402.419756	22882.776420	29.932160
402.793972	22925.099828	29.937178
403.291712	22947.770550	29.942196
403.592881	22979.028150	29.947213
403.917686	23022.111478	29.952231
404.302601	23059.959564	29.957248
404.855527	23093.029413	29.962266
405.196685	23129.961892	29.967284
405.720026	23175.529475	29.972301
406.350957	23208.694724	29.977319
406.409513	23250.050879	29.982336
407.052692	23278.424383	29.987354
407.350030	23314.359315	29.992372
407.926289	23353.884175	29.997389
408.066503	23391.234085	30.002407
408.425867	23437.162870	30.007424
409.140928	23458.612116	30.012442
409.430814	23506.460358	30.017460
410.006928	23529.587093	30.022477
410.493964	23573.063272	30.027495
410.669398	23617.492014	30.032512
411.055004	23649.274580	30.037530
410.699255	23683.720005	30.042548
411.440662	23721.443995	30.047565
411.821269	23777.361108	30.052583
412.175858	23820.435174	30.057600
413.020361	23852.190420	30.062618
413.363871	23904.151449	30.067636
413.587967	23938.841417	30.072653
414.272386	23984.568879	30.077671
415.062771	24019.012301	30.082688
415.396956	24053.015364	30.087706
415.642534	24084.574097	30.092724
416.381770	24132.675745	30.097741
416.563714	24165.382077	30.102759
416.956200	24197.777426	30.107776
417.447820	24230.410080	30.112794
417.382276	24275.434142	30.117812
418.029215	24300.433892	30.122829
418.782198	24346.543253	30.127847
419.194174	24389.647472	30.132864
419.443744	24419.657819	30.137882
420.122969	24460.615918	30.142900
420.479679	24497.125076	30.147917
420.966961	24517.037564	30.152935
421.092224	24563.113034	30.157952
421.758875	24588.116376	30.162970
422.043416	24625.281671	30.167988
422.164615	24655.502065	30.173005
422.508754	24688.038492	30.178023
423.022737	24728.011878	30.183040
423.458366	24757.879833	30.188058
423.629205	24800.605607	30.193076
424.111618	24838.625059	30.198093
424.522531	24884.308939	30.203111
424.924383	24908.500997	30.208128
425.598997	24945.871215	30.213146
426.042142	24991.771482	30.218164
426.236774	25034.026365	30.223181
427.080727	25067.439401	30.228199
426.796646	25106.893927	30.233216
427.555376	25144.365095	30.238234
427.813410	25182.527778	30.243252
428.153234	25223.287803	30.248269
428.821143	25271.738305	30.253287
429.209922	25319.095074	30.258304
429.797189	25359.658621	30.263322
429.824028	25407.078608	30.268340
430.172518	25439.723007	30.273357
431.148978	25483.341543	30.278375
431.241458	25538.891578	30.283392
431.957553	25573.652663	30.288410
432.212833	25627.616422	30.293428
432.959793	25659.547810	30.298445
433.451736	25695.690364	30.303463
434.038001	25744.496069	30.308480
434.396466	25779.692724	30.313498
434.795876	25813.309349	30.318516
435.223562	25863.404179	30.323533
435.614314	25905.345767	30.328551
435.830634	25953.931842	30.333568
436.298538	25984.201043	30.338586
436.578036	26027.430640	30.343604
437.450591	26073.550513	30.348621
437.778064	26114.421713	30.353639
438.333958	26172.599581	30.358656
438.771787	26189.146536	30.363674
439.316121	26228.688377	30.368692
439.516070	26269.978034	30.373709
440.206663	26308.694466	30.378727
440.561380	26356.766859	30.383744
441.098160	26391.298313	30.388762
441.741172	26428.600388	30.393780
442.139371	26472.596046	30.398797
442.561338	26507.821944	30.403815
442.507488	26551.717932	30.408832
443.219335	26575.149250	30.413850
443.575640	26622.627923	30.418868
444.195892	26672.271135	30.423885
444.575999	26704.274277	30.428903
444.975847	26751.196567	30.433920
445.330934	26792.121692	30.438938
446.103021	26819.740536	30.443956
446.162679	26874.559898	30.448973
446.937825	26907.203041	30.453991
447.300909	26954.630866	30.459008
447.664472	26991.465799	30.464026
447.781029	27034.862112	30.469044
448.091626	27078.898087	30.474061
448.827192	27117.899759	30.479079
449.584437	27159.382033	30.484096
449.680416	27199.817648	30.489114
449.906527	27244.707831	30.494132
450.586899	27293.237068	30.499149
451.151400	27324.213674	30.504167
451.608678	27359.536645	30.509184
451.652575	27400.480134	30.514202
452.627955	27433.636323	30.519220
453.008757	27478.850421	30.524237
453.122265	27515.074455	30.529255
453.546588	27563.202005	30.534272
454.138948	27601.019812	30.539290
454.649609	27626.613883	30.544308
455.202045	27680.460710	30.549325
455.608714	27713.573701	30.554343
455.911108	27754.768159	30.559360
456.274325	27804.321662	30.564378
456.751507	27852.978868	30.569396
457.334386	27896.929719	30.574413
457.924503	27929.192644	30.579431
458.160151	27976.446867	30.584448
459.028669	28016.067824	30.589466
459.348370	28057.999702	30.594484
459.385586	28096.246697	30.599501
459.854357	28140.323396	30.604519
460.099104	28186.521119	30.609536
460.737976	28239.521546	30.614554
461.534562	28296.662791	30.619572
461.579136	28348.467147	30.624589
462.213065	28383.947527	30.629607
462.362410	28433.757282	30.634624
463.341634	28477.116353	30.639642
463.531488	28527.943965	30.644660
464.338708	28577.334985	30.649677
464.816088	28623.927076	30.654695
464.987884	28674.890619	30.659712
465.578148	28721.686482	30.664730
466.101696	28770.193227	30.669748
466.556772	28815.777901	30.674765
467.387829	28854.578312	30.679783
467.761529	28907.204818	30.684800
468.441378	28938.064671	30.689818
468.824325	28983.338647	30.694836
468.976843	29026.385900	30.699853
469.736238	29066.948850	30.704871
470.169699	29114.016688	30.709888
470.383521	29162.332672	30.714906
470.887450	29203.195067	30.719924
471.489964	29254.661479	30.724941
471.842111	29291.293751	30.729959
472.399287	29350.118908	30.734976
473.127132	29387.836624	30.739994
473.567737	29434.126580	30.745012
473.740445	29481.571119	30.750029
474.623527	29515.345655	30.755047
474.845810	29569.457755	30.760064
475.254389	29606.979354	30.765082
475.720893	29649.890235	30.770100
476.270821	29702.244647	30.775117
476.876428	29749.489253	30.780135
477.257727	29797.881636	30.785152
477.773496	29840.380640	30.790170
478.197556	29883.368189	30.795188
478.115008	29922.958481	30.800205
479.063532	29969.410294	30.805223
479.241269	30018.587309	30.810240
479.537844	30062.075616	30.815258
480.651638	30111.093598	30.820276
481.220175	30174.458039	30.825293
481.596560	30199.924644	30.830311
481.765578	30248.553615	30.835328
482.351307	30294.677381	30.840346
482.966749	30334.930345	30.845364
482.937163	30384.267130	30.850381
483.707744	30429.135891	30.855399
484.418169	30460.442061	30.860416
484.561078	30509.455020	30.865434
485.281887	30554.060026	30.870452
485.636024	30604.759563	30.875469
486.101719	30640.346044	30.880487
486.568172	30685.130244	30.885504
487.202786	30731.411686	30.890522
487.726903	30777.192173	30.895540
487.829722	30822.204304	30.900557
488.211271	30868.645798	30.905575
488.834535	30915.789161	30.910592
489.347266	30967.855490	30.915610
489.752546	31020.823804	30.920628
490.277364	31071.858081	30.925645
490.724831	31119.718497	30.930663
491.232027	31179.226782	30.935680
491.702611	31227.343013	30.940698
492.655765	31268.746014	30.945716
492.686241	31324.561664	30.950733
493.501413	31372.877129	30.955751
493.999760	31418.821110	30.960768
494.135906	31482.446923	30.965786
494.818945	31526.832354	30.970804
495.402525	31577.125345	30.975821
495.838106	31622.434787	30.980839
496.285287	31679.248180	30.985856
496.739324	31741.206612	30.990874
497.250172	31783.375316	30.995892
498.182682	31834.417150	31.000909
498.416518	31888.621997	31.005927
498.677336	31943.062991	31.010944
498.939743	31989.614154	31.015962
499.653854	32040.874035	31.020980
500.088470	32100.130799	31.025997
500.646924	32157.648767	31.031015
501.386122	32211.876453	31.036032
501.668883	32271.498873	31.041050
502.776722	32315.345303	31.046068
503.054825	32377.219383	31.051085
503.476819	32426.174175	31.056103
504.148021	32467.952470	31.061120
504.713987	32517.542419	31.066138
505.180523	32568.899271	31.071156
505.588481	32624.083963	31.076173
506.213638	32669.916007	31.081191
506.458973	32725.354031	31.086208
506.590595	32780.057679	31.091226
507.435727	32828.991395	31.096244
507.876395	32888.394853	31.101261
508.413597	32940.689873	31.106279
509.282154	32992.066986	31.111296
509.589674	33048.046154	31.116314
509.892242	33090.363916	31.121332
510.503048	33155.715986	31.126349
511.100937	33206.845195	31.131367
511.599446	33261.132264	31.136384
511.736089	33324.226203	31.141402
512.518352	33358.617086	31.146420
512.876420	33422.776722	31.151437
513.464727	33481.943777	31.156455
513.997242	33540.007001	31.161472
514.477026	33606.051162	31.166490
515.000584	33649.682105	31.171508
515.453980	33709.161758	31.176525
515.993396	33760.933714	31.181543
516.562867	33812.157359	31.186560
517.182905	33864.662990	31.191578
517.793460	33916.000580	31.196596
518.278278	33947.145006	31.201613
518.561094	34006.285511	31.206631
519.226716	34044.982441	31.211648
519.347195	34099.925197	31.216666
520.445042	34149.827693	31.221684
520.855702	34197.321558	31.226701
521.144457	34255.734737	31.231719
521.659995	34305.589708	31.236736
521.853290	34364.024460	31.241754
522.961803	34415.765794	31.246772
523.405837	34479.440984	31.251789
523.669884	34543.998114	31.256807
524.525462	34588.483138	31.261824
524.760847	34644.591652	31.266842
525.288483	34697.910487	31.271860
525.648486	34753.753187	31.276877
526.409297	34806.100012	31.281895
526.898284	34865.804966	31.286912
527.487178	34924.533380	31.291930
528.115922	34988.415114	31.296948
528.514192	35047.869233	31.301965
529.191348	35099.780966	31.306983
529.891768	35148.451889	31.312000
529.951050	35211.816492	31.317018
530.789222	35265.676145	31.322036
531.695151	35316.016119	31.327053
531.774032	35374.895210	31.332071
532.548541	35426.893663	31.337088
532.757436	35491.222042	31.342106
533.548796	35558.380598	31.347124
533.778270	35602.124859	31.352141
534.311414	35665.049862	31.357159
535.201203	35719.851033	31.362176
535.912564	35780.111770	31.367194
536.474487	35836.703424	31.372212
537.030251	35893.188702	31.377229
537.244630	35935.418476	31.382247
538.116572	35983.944311	31.387264
538.351861	36051.640455	31.392282
539.070227	36113.557693	31.397300
539.414382	36172.656688	31.402317
539.746842	36228.362142	31.407335
540.722715	36284.181958	31.412352
540.829308	36346.145101	31.417370
541.795784	36396.345363	31.422388
542.757935	36453.489322	31.427405
542.581723	36513.442194	31.432423
543.453975	36568.899589	31.437440
543.419996	36630.019283	31.442458
544.557875	36683.715443	31.447476
544.868874	36747.007241	31.452493
545.254162	36802.503570	31.457511
546.058513	36870.574783	31.462528
546.442671	36932.622618	31.467546
547.188852	36977.762115	31.472564
547.567985	37034.436158	31.477581
547.748162	37104.382746	31.482599
548.813399	37157.060754	31.487616
549.059493	37216.892539	31.492634
549.463775	37279.633806	31.497652
550.400572	37337.852765	31.502669
550.780063	37414.611162	31.507687
551.394678	37459.557279	31.512704
551.809767	37521.696826	31.517722
552.490851	37578.356631	31.522740
552.848844	37637.476470	31.527757
553.111169	37690.357422	31.532775
553.931280	37747.552375	31.537792
554.208446	37812.541015	31.542810
554.977051	37872.469850	31.547828
555.910323	37940.581178	31.552845
555.938478	37989.079297	31.557863
556.491913	38041.131381	31.562880
556.649572	38106.417866	31.567898
557.287323	38174.993584	31.572916
558.147434	38233.872001	31.577933
558.586787	38309.017976	31.582951
559.119675	38362.534844	31.587968
560.028109	38441.364144	31.592986
560.437964	38493.439806	31.598004
561.013339	38554.785720	31.603021
561.372175	38632.184069	31.608039
561.898032	38684.134517	31.613056
562.287699	38756.880431	31.618074
562.965085	38818.015073	31.623092
563.772740	38883.069300	31.628109
564.233528	38958.448159	31.633127
564.895877	39022.671828	31.638144
565.571318	39097.789890	31.643162
566.499468	39155.041217	31.648180
566.981089	39219.413930	31.653197
567.660787	39286.677527	31.658215
568.361412	39332.878888	31.663232
568.683106	39416.015461	31.668250
569.287534	39471.813190	31.673268
570.120898	39534.152301	31.678285
570.751149	39608.393830	31.683303
571.329497	39650.573886	31.688320
571.658643	39724.603679	31.693338
572.601963	39780.507230	31.698356
572.960206	39834.282756	31.703373
573.561547	39906.569324	31.708391
574.038423	39951.327171	31.713408
574.834877	40023.450760	31.718426
575.403804	40081.924457	31.723444
575.908178	40136.847837	31.728461
576.139758	40207.782994	31.733479
576.886755	40264.180210	31.738496
577.494939	40335.240205	31.743514
578.108779	40395.206582	31.748532
578.673261	40454.877282	31.753549
578.978311	40529.976080	31.758567
580.016401	40577.518605	31.763584
580.441263	40644.895877	31.768602
581.026012	40703.267569	31.773620
581.377106	40766.659706	31.778637
582.012341	40844.730977	31.783655
582.635647	40904.014220	31.788672
583.194525	40969.347654	31.793690
583.443491	41033.395336	31.798708
584.315115	41105.934471	31.803725
584.910806	41169.668941	31.808743
585.604308	41229.821192	31.813760
586.537674	41300.422293	31.818778
586.628356	41366.197064	31.823796
587.553296	41424.511074	31.828813
587.962139	41504.245591	31.833831
588.546253	41562.436255	31.838848
589.313135	41628.890174	31.843866
589.913530	41686.250076	31.848884
590.551354	41739.486842	31.853901
591.177934	41808.999167	31.858919
591.839968	41860.334998	31.863936
592.193920	41917.196490	31.868954
592.484291	41974.978863	31.873972
593.335435	42042.698452	31.878989
593.912495	42105.173582	31.884007
594.506209	42152.776472	31.889024
595.043209	42218.218243	31.894042
595.281266	42281.828524	31.899060
596.484356	42331.784109	31.904077
596.402035	42401.276502	31.909095
596.833642	42461.460487	31.914112
597.797598	42527.582654	31.919130
598.361854	42600.263406	31.924148
598.854798	42658.028490	31.929165
599.117951	42737.689083	31.934183
599.907834	42799.171438	31.939200
600.384273	42867.021816	31.944218
601.038233	42942.074200	31.949236
601.729221	43001.592846	31.954253
602.286285	43089.753923	31.959271
602.981748	43153.193870	31.964288
603.376703	43229.053135	31.969306
603.832547	43298.457731	31.974324
604.900023	43375.394985	31.979341
605.442577	43461.086643	31.984359
605.826841	43524.045066	31.989376
606.561821	43589.074041	31.994394
606.623276	43672.602705	31.999412
607.719214	43749.454569	32.004429
608.310495	43821.951656	32.009447
609.154988	43903.979626	32.014464
609.859495	43975.320911	32.019482
610.092030	44043.801344	32.024500
611.043137	44113.257426	32.029517
611.511922	44190.259636	32.034535
612.344255	44260.196536	32.039552
612.857174	44340.468953	32.044570
613.486558	44420.394491	32.049588
614.422027	44484.078970	32.054605
615.263811	44566.008592	32.059623
615.571458	44623.402965	32.064640
616.571599	44687.666176	32.069658
617.261101	44757.993891	32.074676
617.902367	44820.833492	32.079693
618.146633	44895.241824	32.084711
619.019974	44959.968473	32.089728
619.722888	45026.214865	32.094746
619.960160	45093.824824	32.099764
621.305772	45163.892917	32.104781
621.524207	45228.235823	32.109799
621.989749	45299.776904	32.114816
623.068030	45362.821593	32.119834
623.712810	45426.819964	32.124852
624.244754	45481.543543	32.129869
624.688479	45552.570128	32.134887
625.098408	45625.594879	32.139904
625.787889	45689.169489	32.144922
626.231159	45755.756013	32.149940
627.274422	45826.075955	32.154957
627.536718	45901.326144	32.159975
627.986149	45971.891363	32.164992
628.724189	46035.914818	32.170010
629.524094	46101.839219	32.175028
630.036235	46167.903769	32.180045
630.468260	46251.643372	32.185063
631.057693	46326.059314	32.190080
631.968005	46390.929795	32.195098
632.646594	46467.552697	32.200116
632.965689	46517.763658	32.205133
633.772918	46596.302643	32.210151
634.499814	46667.010040	32.215168
635.483397	46721.507745	32.220186
635.554395	46787.485040	32.225204
635.889227	46849.752004	32.230221
636.669475	46925.253448	32.235239
637.002921	46987.938541	32.240256
638.003444	47058.964906	32.245274
638.456648	47130.614944	32.250292
639.302706	47200.792917	32.255309
639.796903	47278.364755	32.260327
640.317557	47346.544408	32.265344
641.264227	47422.192256	32.270362
641.580141	47496.161422	32.275380
642.260607	47562.886931	32.280397
642.959412	47640.105314	32.285415
643.580262	47716.304955	32.290432
644.463128	47790.527917	32.295450
645.114628	47881.761346	32.300468
645.771332	47947.156813	32.305485
645.956025	48027.164772	32.310503
646.801594	48109.328096	32.315520
647.579005	48175.806137	32.320538
648.273289	48259.322275	32.325556
648.966560	48330.078075	32.330573
649.587243	48398.504603	32.335591
650.369586	48475.940494	32.340608
650.741957	48556.452354	32.345626
651.280517	48642.056778	32.350644
651.951369	48721.010390	32.355661
652.850352	48801.674730	32.360679
653.340196	48884.383710	32.365696
654.394692	48962.139252	32.370714
654.919443	49041.724222	32.375732
655.440964	49110.832725	32.380749
656.045847	49201.686457	32.385767
656.969729	49281.266693	32.390784
657.740820	49346.964593	32.395802
658.302996	49439.198891	32.400820
659.130286	49520.085775	32.405837
659.582632	49588.845914	32.410855
660.133697	49658.501884	32.415872
660.907685	49727.224719	32.420890
661.642904	49811.739770	32.425908
662.293738	49888.353202	32.430925
663.204534	49972.512339	32.435943
663.861454	50050.473024	32.440960
664.547569	50118.723602	32.445978
665.038257	50201.310642	32.450996
665.555416	50276.845376	32.456013
666.478903	50347.236000	32.461031
667.132110	50429.216303	32.466048
668.068146	50499.396627	32.471066
668.245272	50582.584604	32.476084
668.947750	50655.022839	32.481101
669.939075	50734.293823	32.486119
670.607616	50813.508064	32.491136
671.307497	50884.080867	32.496154
671.718717	50961.608552	32.501172
672.613267	51034.182405	32.506189
673.279276	51105.830513	32.511207
673.961252	51183.715163	32.516224
674.642125	51257.379854	32.521242
675.216836	51346.955955	32.526260
675.988163	51411.052519	32.531277
676.813625	51490.826624	32.536295
677.244009	51562.645918	32.541312
677.979380	51630.481949	32.546330
678.519751	51700.626632	32.551348
679.366770	51779.341650	32.556365
679.953106	51836.476394	32.561383
680.372565	51912.791063	32.566400
681.070493	51981.988089	32.571418
681.739086	52059.251331	32.576436
682.125380	52122.777387	32.581453
683.088593	52202.019816	32.586471
683.720835	52272.442904	32.591488
684.527311	52350.375236	32.596506
684.708906	52430.240732	32.601524
685.492779	52510.499420	32.606541
685.978230	52580.092175	32.611559
686.673467	52678.089450	32.616576
687.403995	52767.697225	32.621594
687.749133	52851.158066	32.626612
688.722418	52934.976442	32.631629
689.504763	53019.185709	32.636647
690.197354	53123.146144	32.641664
690.965081	53194.999885	32.646682
691.435151	53278.657831	32.651700
692.225711	53366.834698	32.656717
693.184922	53450.328061	32.661735
693.445815	53543.606657	32.666752
694.329584	53627.239024	32.671770
695.303500	53716.945193	32.676788
695.836704	53810.536574	32.681805
696.591594	53895.462027	32.686823
697.024288	53988.278835	32.691840
698.128980	54067.163685	32.696858
698.788007	54157.041075	32.701876
699.350608	54246.332726	32.706893
700.351904	54329.158147	32.711911
700.965938	54420.252281	32.716928
701.778557	54502.569953	32.721946
702.752132	54588.963459	32.726964
703.190000	54674.466607	32.731981
704.149486	54757.958225	32.736999
704.426588	54855.314925	32.742016
705.378305	54934.840479	32.747034
705.788492	55022.532519	32.752052
706.912759	55115.131529	32.757069
707.590940	55192.289637	32.762087
708.287692	55288.285053	32.767104
709.086543	55366.677875	32.772122
709.519194	55465.221462	32.777140
710.285812	55539.246866	32.782157
711.161151	55622.318027	32.787175
711.613498	55721.802551	32.792192
712.453621	55804.114097	32.797210
712.988346	55900.776547	32.802228
713.692277	55987.818586	32.807245
714.691572	56072.447748	32.812263
714.819392	56153.340494	32.817280
715.870496	56255.113079	32.822298
716.766458	56344.607222	32.827316
717.618664	56438.190636	32.832333
718.321819	56519.102110	32.837351
718.941543	56598.299144	32.842368
719.822700	56693.840968	32.847386
720.652036	56784.935739	32.852404
720.994296	56864.423929	32.857421
722.023263	56956.279203	32.862439
722.451548	57042.387252	32.867456
723.590675	57129.498195	32.872474
724.099215	57211.037402	32.877492
724.484761	57296.197370	32.882509
725.708530	57373.201124	32.887527
725.885829	57454.033538	32.892544
726.676061	57540.814533	32.897562
727.401537	57617.264188	32.902580
728.218854	57708.016234	32.907597
729.169038	57788.285694	32.912615
729.493752	57869.653381	32.917632
730.250201	57952.390465	32.922650
731.076787	58042.003055	32.927668
731.611501	58128.294518	32.932685
732.506964	58208.434700	32.937703
732.764666	58302.219725	32.942720
733.730426	58386.134410	32.947738
734.531786	58480.974269	32.952756
735.240677	58571.569311	32.957773
736.246348	58660.630807	32.962791
736.676453	58761.403581	32.967808
737.256158	58852.342700	32.972826
738.083921	58939.236760	32.977844
738.564529	59037.470980	32.982861
740.191983	59123.487260	32.987879
740.179966	59228.622615	32.992896
740.998155	59317.962731	32.997914
741.607091	59407.956242	33.002932
742.826601	59511.083368	33.007949
743.435464	59604.881717	33.012967
743.996071	59702.530091	33.017984
744.802574	59800.260612	33.023002
745.798168	59890.062427	33.028020
746.318223	59989.674179	33.033037
747.399119	60086.077936	33.038055
747.848618	60184.802703	33.043072
748.894912	60282.643185	33.048090
749.770618	60373.725181	33.053108
750.776754	60468.027982	33.058125
751.318663	60562.789963	33.063143
751.740802	60669.275078	33.068160
752.491552	60758.238557	33.073178
753.341291	60848.946585	33.078196
754.177455	60957.374710	33.083213
755.111970	61042.658035	33.088231
755.671377	61140.850369	33.093248
756.522491	61239.567119	33.098266
757.262736	61331.129637	33.103284
758.175960	61438.433716	33.108301
759.122022	61536.060664	33.113319
759.627984	61626.825388	33.118336
760.207313	61715.452013	33.123354
761.337286	61807.189482	33.128372
761.594458	61906.419698	33.133389
762.787736	62001.357403	33.138407
763.752960	62107.478812	33.143424
763.992661	62199.179897	33.148442
764.973979	62297.798186	33.153460
765.442713	62400.839760	33.158477
766.255356	62495.281889	33.163495
767.330444	62590.670823	33.168512
767.934206	62690.983040	33.173530
769.098629	62777.850602	33.178548
769.691003	62889.794452	33.183565
770.556694	62976.867750	33.188583
771.406971	63079.333283	33.193600
771.809788	63170.930105	33.198618
772.571371	63268.004008	33.203636
773.290253	63374.967050	33.208653
774.162288	63463.978219	33.213671
774.724046	63556.089666	33.218688
775.183972	63665.645753	33.223706
776.312996	63752.604550	33.228724
777.076422	63851.180803	33.233741
778.025238	63938.997791	33.238759
778.777466	64039.387132	33.243776
779.230900	64134.056305	33.248794
780.113088	64223.416775	33.253812
780.626293	64317.843040	33.258829
781.858288	64410.048924	33.263847
782.556831	64511.423509	33.268864
782.893837	64598.667533	33.273882
783.973418	64691.493421	33.278900
784.876832	64804.960855	33.283917
785.596502	64887.707950	33.288935
786.305107	64986.582130	33.293952
786.599075	65087.826124	33.298970
787.759575	65192.651164	33.303988
788.463634	65307.500589	33.309005
789.436922	65410.861712	33.314023
790.501130	65508.764237	33.319040
791.053388	65623.417275	33.324058
792.127307	65710.068570	33.329076
792.564615	65824.189701	33.334093
793.371079	65923.514393	33.339111
794.340790	66030.221499	33.344128
795.143483	66136.676629	33.349146
796.110952	66230.291803	33.354164
796.969503	66338.771386	33.359181
797.288575	66438.339024	33.364199
798.493233	66541.674850	33.369216
798.864688	66650.206706	33.374234
799.936429	66754.184686	33.379252
800.759448	66864.242267	33.384269
801.606575	66969.433951	33.389287
802.129845	67076.474934	33.394304
803.021640	67185.472093	33.399322
803.861500	67295.351607	33.404340
804.942640	67402.477549	33.409357
805.351952	67511.716269	33.414375
806.442889	67617.290321	33.419392
807.295108	67728.664029	33.424410
808.029181	67831.280957	33.429428
809.011158	67946.662262	33.434445
809.476487	68059.763234	33.439463
810.597149	68153.576734	33.444480
811.449191	68274.786113	33.449498
812.277051	68371.406932	33.454516
812.886994	68480.700659	33.459533
813.904279	68589.038264	33.464551
814.665183	68699.423691	33.469568
815.544407	68804.934452	33.474586
816.454985	68897.960400	33.479604
817.074850	69018.342140	33.484621
817.620566	69132.087411	33.489639
818.566466	69239.470115	33.494656
819.446806	69361.243705	33.499674
820.359000	69468.246375	33.504692
821.290458	69572.352679	33.509709
822.181570	69672.609428	33.514727
823.175924	69790.004310	33.519744
823.554625	69894.458078	33.524762
824.628351	70000.772760	33.529780
825.270605	70124.505872	33.534797
826.152755	70217.832279	33.539815
827.560261	70329.617801	33.544832
828.147441	70442.912708	33.549850
828.713045	70541.849646	33.554868
829.258807	70662.446888	33.559885
830.338467	70760.822896	33.564903
831.352383	70862.363130	33.569920
831.763976	70965.454544	33.574938
832.428326	71064.365327	33.579956
833.650941	71163.163734	33.584973
834.493734	71271.761455	33.589991
835.412260	71367.112676	33.595008
835.705869	71471.402407	33.600026
836.919237	71575.003922	33.605044
837.354325	71682.210672	33.610061
838.290137	71789.808069	33.615079
838.830787	71906.954173	33.620096
839.491491	72019.649083	33.625114
840.581666	72128.882866	33.630132
841.432533	72245.867906	33.635149
842.104998	72364.249286	33.640167
843.091191	72479.732290	33.645184
843.631707	72599.325955	33.650202
844.583212	72714.663424	33.655220
845.407444	72839.026746	33.660237
846.487822	72961.488651	33.665255
847.294590	73072.721249	33.670272
847.966428	73197.984063	33.675290
849.099257	73321.174040	33.680308
850.044389	73440.302812	33.685325
850.856279	73555.488460	33.690343
851.778824	73675.597116	33.695360
852.933255	73794.694696	33.700378
853.354324	73915.858260	33.705396
854.038285	74037.525863	33.710413
855.129166	74169.136824	33.715431
855.960514	74282.802576	33.720448
856.449475	74397.839747	33.725466
857.475805	74520.355258	33.730484
858.621002	74643.828052	33.735501
859.378201	74780.902945	33.740519
860.635594	74897.658612	33.745536
861.401924	75015.201023	33.750554
862.287234	75142.491529	33.755572
862.911701	75269.886813	33.760589
863.803663	75395.049410	33.765607
864.834602	75511.007164	33.770624
865.685448	75639.002095	33.775642
866.701174	75748.059636	33.780660
867.673138	75876.822094	33.785677
868.434064	76000.513267	33.790695
869.508029	76118.480991	33.795712
870.200744	76244.236073	33.800730
871.236509	76357.485853	33.805748
872.268378	76482.403545	33.810765
872.948997	76605.755353	33.815783
873.795532	76724.420031	33.820800
874.693491	76851.868584	33.825818
875.849549	76962.429150	33.830836
876.431618	77081.554828	33.835853
877.118958	77208.670656	33.840871
878.313511	77326.422037	33.845888
879.113445	77449.898318	33.850906
880.313270	77564.001506	33.855924
880.802699	77690.694507	33.860941
881.669425	77821.433507	33.865959
882.727257	77935.763165	33.870976
883.387567	78060.746238	33.875994
884.522498	78184.908128	33.881012
885.090853	78301.038841	33.886029
885.974586	78423.138181	33.891047
886.847385	78537.917369	33.896064
887.680245	78670.756005	33.901082
888.477306	78788.474534	33.906100
889.635807	78905.490866	33.911117
890.280087	79032.102434	33.916135
891.415344	79136.809368	33.921152
892.235103	79258.111605	33.926170
892.883326	79372.992762	33.931188
893.781967	79490.685697	33.936205
894.628881	79609.654130	33.941223
895.489277	79718.840448	33.946240
896.317302	79855.422882	33.951258
897.410644	79965.029777	33.956276
898.426576	80081.338573	33.961293
898.969478	80211.113344	33.966311
899.782231	80335.335303	33.971328
900.994376	80461.573057	33.976346
901.756506	80580.571572	33.981364
902.391927	80709.966754	33.986381
903.368133	80845.669295	33.991399
904.692701	80969.104428	33.996416
905.652538	81104.506711	34.001434
906.444948	81224.820862	34.006452
907.210708	81350.777757	34.011469
907.942793	81480.972218	34.016487
909.071230	81608.558567	34.021504
910.277549	81747.434911	34.026522
910.650437	81872.505402	34.031540
911.503433	82006.953154	34.036557
912.381727	82141.486274	34.041575
913.656577	82271.307975	34.046592
914.440886	82415.625842	34.051610
915.612451	82548.505849	34.056628
916.442877	82677.043268	34.061645
917.301993	82816.486029	34.066663
918.185657	82943.343816	34.071680
919.527118	83081.305923	34.076698
920.081454	83220.557642	34.081716
921.456421	83350.799396	34.086733
921.933652	83480.232002	34.091751
923.249733	83606.315467	34.096768
924.171591	83736.718620	34.101786
925.301148	83869.573346	34.106804
926.318719	84003.966738	34.111821
926.892621	84139.773356	34.116839
928.071977	84256.377814	34.121856
928.841466	84393.536155	34.126874
929.586299	84539.644881	34.131892
930.835921	84657.899892	34.136909
931.471978	84799.123187	34.141927
932.775972	84930.625009	34.146944
933.619326	85064.391714	34.151962
934.627369	85197.322276	34.156980
935.688349	85324.454259	34.161997
936.247096	85457.139572	34.167015
937.145169	85587.580162	34.172032
938.425924	85717.112415	34.177050
939.170379	85859.337640	34.182068
940.267462	85979.598732	34.187085
940.892770	86128.217860	34.192103
942.006021	86251.810254	34.197120
942.711844	86391.877221	34.202138
943.671638	86523.490837	34.207156
945.086558	86658.366554	34.212173
945.581920	86804.500385	34.217191
946.587614	86930.241417	34.222208
947.501955	87062.612234	34.227226
948.421749	87199.544846	34.232244
949.747302	87338.429481	34.237261
950.785915	87476.117795	34.242279
952.099167	87606.565748	34.247296
952.475128	87727.403135	34.252314
953.443888	87853.217259	34.257332
954.599099	87969.498202	34.262349
955.024622	88096.881126	34.267367
956.229014	88224.345412	34.272384
957.223587	88344.961737	34.277402
957.972093	88469.368262	34.282420
959.091358	88601.764591	34.287437
959.876234	88724.747119	34.292455
960.953858	88855.833106	34.297472
961.669160	88987.838173	34.302490
962.414882	89122.145583	34.307508
963.177050	89253.206671	34.312525
964.271203	89401.958980	34.317543
965.136171	89536.617109	34.322560
966.296302	89671.559140	34.327578
966.881554	89823.168702	34.332596
968.188171	89959.394464	34.337613
969.179167	90104.909317	34.342631
970.643408	90245.496766	34.347648
971.511064	90376.558928	34.352666
972.259111	90528.640837	34.357684
973.133054	90659.601856	34.362701
974.149334	90813.024650	34.367719
975.086968	90946.346961	34.372736
976.435929	91087.349282	34.377754
977.395067	91228.806191	34.382772
978.212234	91375.000768	34.387789
979.166744	91528.310120	34.392807
979.817819	91669.931389	34.397824
980.946669	91812.644549	34.402842
982.431559	91961.956683	34.407860
983.178334	92102.931264	34.412877
984.377224	92257.245332	34.417895
984.953691	92399.490049	34.422912
986.231862	92541.752310	34.427930
986.720869	92693.543405	34.432948
987.884102	92838.030434	34.437965
988.946678	92999.125226	34.442983
990.008202	93146.874386	34.448000
991.031980	93291.512133	34.453018
991.770140	93452.799520	34.458036
993.206986	93601.721576	34.463053
994.398214	93747.868931	34.468071
995.368288	93896.434538	34.473088
996.303954	94043.802099	34.478106
996.828561	94202.211531	34.483124
998.001951	94347.996932	34.488141
999.323490	94499.083502	34.493159
1000.756140	94641.914345	34.498176
1001.786105	94791.057936	34.503194
1001.980857	94948.039777	34.508212
1003.286944	95095.290954	34.513229
1004.697352	95250.017849	34.518247
1005.711666	95389.267008	34.523264
1006.860837	95527.329496	34.528282
1007.357394	95674.025651	34.533300
1008.570773	95827.189087	34.538317
1009.673125	95970.850960	34.543335
1010.693182	96116.288351	34.548352
1011.721528	96261.053280	34.553370
1012.831404	96414.197755	34.558388
1013.794729	96555.412206	34.563405
1014.552213	96697.584888	34.568423
1015.605260	96844.123312	34.573440
1017.086610	96989.061509	34.578458
1017.593413	97139.388341	34.583476
1018.719151	97285.372338	34.588493
1019.725409	97420.702011	34.593511
1020.858552	97559.637919	34.598528
1021.749466	97688.940027	34.603546
1022.543650	97827.816085	34.608564
1023.661251	97963.498261	34.613581
1024.612225	98111.059981	34.618599
1025.449670	98245.506854	34.623616
1026.391796	98387.582125	34.628634
1027.398743	98525.489808	34.633652
1028.331293	98675.136049	34.638669
1029.703619	98827.363661	34.643687
1030.836359	98975.395314	34.648704
1031.874283	99121.008456	34.653722
1032.805736	99271.177412	34.658740
1033.707138	99414.429916	34.663757
1034.683996	99558.888277	34.668775
1035.565461	99718.828779	34.673792
1036.542881	99857.887769	34.678810
1037.595613	100018.639657	34.683828
1038.795517	100177.683167	34.688845
1039.810602	100331.254248	34.693863
1040.595099	100490.960184	34.698880
1041.746259	100626.356731	34.703898
1042.438308	100805.970261	34.708916
1043.490616	100964.203978	34.713933
1044.981890	101128.860902	34.718951
1045.762344	101297.560161	34.723968
1046.919156	101456.527907	34.728986
1047.987212	101627.580013	34.734004
1049.132215	101780.972748	34.739021
1050.323455	101951.056378	34.744039
1051.266542	102105.230261	34.749056
1052.462831	102280.715816	34.754074
1052.852461	102444.727705	34.759092
1054.321892	102605.528479	34.764109
1055.306685	102776.891188	34.769127
1056.525657	102941.016585	34.774144
1057.776344	103109.195050	34.779162
1058.979960	103269.685653	34.784180
1059.689619	103437.430646	34.789197
1060.912539	103604.462175	34.794215
1062.091897	103770.537751	34.799232
1063.554970	103937.330481	34.804250
1064.381268	104102.182385	34.809268
1065.539497	104261.569089	34.814285
1066.756595	104426.145854	34.819303
1067.692988	104597.753711	34.824320
1069.144064	104748.665087	34.829338
1069.919884	104914.822180	34.834356
1071.178292	105078.064314	34.839373
1072.207179	105237.932351	34.844391
1073.149174	105401.834207	34.849408
1074.367780	105575.101922	34.854426
1075.031279	105727.421623	34.859444
1076.188697	105894.157765	34.864461
1077.478274	106048.016587	34.869479
1078.584733	106224.728748	34.874496
1079.643822	106382.302360	34.879514
1080.490570	106551.968727	34.884532
1081.755788	106711.198038	34.889549
1082.986493	106876.291759	34.894567
1083.693189	107045.006114	34.899584
1084.922404	107204.940768	34.904602
1085.808241	107379.005184	34.909620
1087.065171	107541.993045	34.914637
1088.165459	107703.662062	34.919655
1089.070934	107876.736831	34.924672
1090.044420	108040.164515	34.929690
1091.189300	108195.640687	34.934708
1092.049103	108362.524161	34.939725
1093.221892	108518.086173	34.944743
1094.452403	108682.009231	34.949760
1095.619601	108841.048125	34.954778
1096.581193	108991.801193	34.959796
1097.667559	109158.653007	34.964813
1098.477289	109320.438432	34.969831
1099.752086	109492.575728	34.974848
1100.979668	109648.692166	34.979866
1101.840009	109824.484766	34.984884
1102.765197	109990.084953	34.989901
1104.101223	110155.025571	34.994919
1104.953655	110328.184184	34.999936
1106.258807	110506.332706	35.004954
1107.474818	110675.796493	35.009972
1108.467532	110846.538852	35.014989
1110.023332	111010.903739	35.020007
1110.899766	111186.840083	35.025024
1111.959602	111356.635929	35.030042
1113.197167	111532.504759	35.035060
1114.432223	111700.943209	35.040077
1115.642464	111879.481239	35.045095
1116.223563	112052.487799	35.050112
1117.871825	112226.799254	35.055130
1119.037209	112407.832637	35.060148
1119.889547	112575.307844	35.065165
1121.146166	112750.152391	35.070183
1122.187616	112937.929479	35.075200
1123.032969	113118.978481	35.080218
1124.226832	113294.710573	35.085236
1125.316765	113475.837209	35.090253
1126.790749	113668.280970	35.095271
1127.648344	113849.826320	35.100288
1129.154638	114015.950206	35.105306
1130.018321	114200.388019	35.110324
1131.188110	114374.924217	35.115341
1132.544140	114563.053602	35.120359
1133.572544	114749.548397	35.125376
1134.748901	114926.901824	35.130394
1135.973102	115110.476047	35.135412
1137.279264	115296.524265	35.140429
1138.375809	115471.470307	35.145447
1139.495260	115660.809191	35.150464
1140.464584	115833.988508	35.155482
1141.576832	116019.702894	35.160500
1142.707328	116205.910008	35.165517
1143.884885	116380.987167	35.170535
1145.129926	116571.592065	35.175552
1145.863752	116763.102408	35.180570
1147.191048	116948.305763	35.185588
1148.268902	117136.681994	35.190605
1150.060675	117325.530863	35.195623
1150.621642	117524.860073	35.200640
1151.807634	117700.373319	35.205658
1152.919690	117878.448459	35.210676
1153.719322	118070.843031	35.215693
1155.542171	118263.433551	35.220711
1156.739112	118449.793571	35.225728
1157.900577	118641.766543	35.230746
1159.049229	118826.702634	35.235764
1159.908691	119009.997857	35.240781
1161.356800	119200.165617	35.245799
1162.689144	119390.555397	35.250816
1163.768495	119573.552512	35.255834
1164.863626	119746.933007	35.260852
1165.807979	119940.671592	35.265869
1167.529306	120118.116334	35.270887
1168.437926	120302.082311	35.275904
1169.593266	120473.782234	35.280922
1170.722450	120641.478546	35.285940
1171.566008	120823.161189	35.290957
1172.987985	120990.102804	35.295975
1173.687665	121177.479874	35.300992
1175.376449	121352.652015	35.306010
1176.402837	121533.370632	35.311028
1177.460883	121709.695991	35.316045
1179.000904	121876.293087	35.321063
1180.273933	122058.726097	35.326080
1181.215104	122250.827537	35.331098
1182.299431	122422.813522	35.336116
1183.275164	122601.718245	35.341133
1184.822043	122786.522018	35.346151
1185.664117	122971.741445	35.351168
1186.862798	123157.184996	35.356186
1188.215297	123345.066392	35.361204
1189.522096	123542.660575	35.366221
1190.573262	123726.886643	35.371239
1191.453137	123914.400691	35.376256
1192.708410	124109.303602	35.381274
1193.992165	124291.986203	35.386292
1195.246845	124492.840884	35.391309
1196.562799	124683.842398	35.396327
1197.530361	124879.250777	35.401344
1198.786384	125077.900725	35.406362
1200.004599	125272.624751	35.411380
1201.367157	125472.414419	35.416397
1202.480416	125659.900020	35.421415
1203.979381	125860.444118	35.426432
1204.768868	126066.733175	35.431450
1206.249181	126248.708715	35.436468
1207.371147	126462.280677	35.441485
1208.777434	126650.854065	35.446503
1209.713347	126849.486600	35.451520
1211.313697	127053.826738	35.456538
1212.483831	127245.104084	35.461556
1213.806667	127450.986700	35.466573
1214.632174	127637.371807	35.471591
1216.201457	127846.732159	35.476608
1217.479787	128044.048070	35.481626
1218.760762	128242.975797	35.486644
1219.833265	128450.260078	35.491661
1220.913416	128648.713666	35.496679
1222.071441	128857.889695	35.501696
1223.248027	129048.882457	35.506714
1225.152306	129247.780794	35.511732
1225.847855	129465.368045	35.516749
1226.986553	129661.216224	35.521767
1228.456969	129854.754933	35.526784
1229.810778	130069.476266	35.531802
1230.895614	130280.193307	35.536820
1232.158351	130473.640448	35.541837
1233.756983	130674.940582	35.546855
1234.892247	130878.192045	35.551872
1236.023379	131069.505476	35.556890
1237.494724	131278.542806	35.561908
1238.279869	131473.617169	35.566925
1239.508313	131674.675389	35.571943
1241.056966	131881.432294	35.576960
1241.920536	132080.570104	35.581978
1243.494010	132273.862447	35.586996
1244.352828	132490.272044	35.592013
1245.877070	132687.862686	35.597031
1247.060390	132891.522063	35.602048
1248.261977	133107.271977	35.607066
1249.713295	133298.062868	35.612084
1250.923527	133497.850717	35.617101
1252.347176	133678.636002	35.622119
1252.871422	133867.379269	35.627136
1254.446917	134066.287706	35.632154
1255.792526	134256.084129	35.637172
1256.931263	134444.505239	35.642189
1258.100364	134641.474955	35.647207
1259.481675	134842.092220	35.652224
1260.515852	135037.485936	35.657242
1261.872661	135234.657272	35.662260
1262.955308	135432.519549	35.667277
1264.037435	135635.306316	35.672295
1265.470560	135835.209261	35.677312
1266.992030	136039.997464	35.682330
1268.178703	136245.841482	35.687348
1269.191283	136455.279507	35.692365
1270.601511	136664.491272	35.697383
1271.763110	136868.045149	35.702400
1272.996821	137073.669788	35.707418
1274.677883	137286.813939	35.712436
1275.623401	137497.079357	35.717453
1276.968439	137707.701961	35.722471
1278.125476	137917.022480	35.727488
1279.520477	138136.611160	35.732506
1280.648841	138345.658904	35.737524
1281.882927	138570.452449	35.742541
1282.987832	138782.132713	35.747559
1284.594581	139001.248130	35.752576
1285.897595	139222.912143	35.757594
1287.586318	139436.470985	35.762612
1288.625464	139662.708901	35.767629
1289.784140	139880.096449	35.772647
1291.505580	140094.985650	35.777664
1292.320210	140320.665365	35.782682
1294.083867	140542.390320	35.787700
1295.209315	140760.903866	35.792717
1296.413232	140976.106460	35.797735
1297.938838	141194.242054	35.802752
1299.135939	141436.454328	35.807770
1300.412845	141644.287618	35.812788
1301.537842	141859.912604	35.817805
1302.891579	142086.671064	35.822823
1304.686318	142320.456003	35.827840
1305.610048	142546.662026	35.832858
1307.123071	142757.420177	35.837876
1308.521326	142989.036659	35.842893
1309.921043	143224.207636	35.847911
1311.473919	143437.094628	35.852928
1312.370324	143653.905488	35.857946
1314.083947	143862.923556	35.862964
1315.219737	144096.731181	35.867981
1316.300147	144319.532033	35.872999
1317.820752	144543.711843	35.878016
1319.424325	144766.800846	35.883034
1320.824037	144974.184638	35.888052
1321.440338	145196.592399	35.893069
1322.916537	145424.895292	35.898087
1324.708136	145649.443718	35.903104
1325.527018	145879.425364	35.908122
1327.059817	146101.757064	35.913140
1328.384345	146336.548140	35.918157
1329.466985	146568.395430	35.923175
1330.793712	146786.345376	35.928192
1332.238502	147016.081801	35.933210
1333.816961	147238.017767	35.938228
1334.805912	147456.328012	35.943245
1335.941155	147686.344307	35.948263
1337.598724	147906.785680	35.953280
1338.904351	148128.755430	35.958298
1340.544102	148340.557616	35.963316
1341.714360	148554.845789	35.968333
1342.746129	148765.945189	35.973351
1344.481588	148983.954504	35.978368
1345.755628	149196.033123	35.983386
1346.920492	149398.800247	35.988404
1348.134385	149623.176886	35.993421
1349.456678	149840.378528	35.998439
1350.868766	150053.619388	36.003456
1351.898982	150276.542381	36.008474
1353.176790	150502.283538	36.013492
1354.808410	150726.307411	36.018509
1356.060307	150964.316365	36.023527
1357.164280	151183.118834	36.028544
1358.476458	151411.650932	36.033562
1359.966226	151648.305480	36.038580
1361.444467	151888.669396	36.043597
1362.695791	152120.603157	36.048615
1364.131696	152347.545724	36.053632
1365.394406	152594.623349	36.058650
1366.817533	152816.174938	36.063668
1368.209958	153058.689891	36.068685
1369.274803	153293.920035	36.073703
1371.163356	153535.991253	36.078720
1372.395590	153776.972989	36.083738
1373.615258	154014.695313	36.088756
1374.809084	154258.490500	36.093773
1376.122124	154520.433548	36.098791
1378.000888	154753.815884	36.103808
1378.975398	155003.246744	36.108826
1380.701326	155252.649919	36.113844
1382.056681	155500.652304	36.118861
1383.610809	155751.480897	36.123879
1385.040022	155983.110517	36.128896
1386.419323	156230.642542	36.133914
1387.734140	156480.597688	36.138932
1389.372965	156732.610500	36.143949
1390.473321	156978.018508	36.148967
1392.256848	157222.660459	36.153984
1393.106788	157471.702329	36.159002
1394.789526	157728.980850	36.164020
1396.249974	157978.830598	36.169037
1397.546240	158224.708133	36.174055
1399.393580	158472.315806	36.179072
1400.382900	158728.107516	36.184090
1402.087559	158973.543290	36.189108
1403.692617	159217.154820	36.194125
1404.889821	159470.111424	36.199143
1406.534646	159716.473581	36.204160
1407.982338	159973.950667	36.209178
1409.076630	160213.215354	36.214196
1410.929795	160462.328151	36.219213
1412.367692	160706.746098	36.224231
1413.860523	160957.999328	36.229248
1415.128762	161195.183826	36.234266
1416.494505	161443.615041	36.239284
1418.202724	161676.644445	36.244301
1419.320730	161940.947978	36.249319
1420.999977	162175.570703	36.254336
1422.518491	162424.261107	36.259354
1424.002144	162683.711395	36.264372
1425.392101	162916.579255	36.269389
1426.625842	163165.659855	36.274407
1428.373743	163407.360668	36.279424
1429.288951	163641.206830	36.284442
1430.799163	163904.492019	36.289460
1432.061630	164137.968174	36.294477
1433.842249	164373.331968	36.299495
1435.118410	164591.089571	36.304512
1436.275874	164830.526455	36.309530
1437.788366	165053.631822	36.314548
1439.456611	165283.912434	36.319565
1440.556609	165530.254959	36.324583
1442.405507	165754.109851	36.329600
1443.318050	165999.467683	36.334618
1444.658933	166238.639572	36.339636
1446.344823	166467.347018	36.344653
1447.224727	166711.709451	36.349671
1449.079106	166968.236074	36.354688
1450.449014	167211.457033	36.359706
1451.483072	167463.212897	36.364724
1453.414879	167713.115063	36.369741
1454.610863	167961.888981	36.374759
1455.952779	168216.392662	36.379776
1457.165901	168458.918715	36.384794
1458.538919	168721.456540	36.389812
1460.226223	168982.485961	36.394829
1461.926765	169245.495008	36.399847
1463.083784	169508.577379	36.404864
1464.621360	169774.140583	36.409882
1465.822113	170043.249225	36.414900
1467.579456	170299.142673	36.419917
1468.968841	170580.794118	36.424935
1470.438126	170843.502237	36.429952
1472.060168	171108.231662	36.434970
1473.338692	171377.383735	36.439988
1474.791472	171652.071028	36.445005
1476.741925	171919.888192	36.450023
1478.134077	172187.539725	36.455040
1479.857380	172457.489436	36.460058
1481.521980	172732.033168	36.465076
1482.707416	172996.266069	36.470093
1483.853502	173272.022964	36.475111
1485.871015	173539.873331	36.480128
1487.316907	173811.318704	36.485146
1488.605669	174086.497408	36.490164
1490.410613	174361.355009	36.495181
1491.480487	174635.008004	36.500199
1493.045532	174907.301919	36.505216
1494.524303	175189.781466	36.510234
1495.580507	175474.029688	36.515252
1497.711384	175745.006118	36.520269
1499.282643	176026.521708	36.525287
1500.849330	176306.007240	36.530304
1502.473854	176583.998949	36.535322
1503.761564	176861.079217	36.540340
1505.576930	177129.620649	36.545357
1506.787904	177417.203664	36.550375
1508.716599	177688.751365	36.555392
1509.839831	177970.940404	36.560410
1511.105057	178243.990541	36.565428
1512.962223	178523.425202	36.570445
1514.356012	178814.666871	36.575463
1516.050188	179089.735104	36.580480
1517.990644	179368.118123	36.585498
1519.246945	179651.815604	36.590516
1520.870407	179918.059097	36.595533
1522.328617	180209.396844	36.600551
1523.991729	180476.956465	36.605568
1525.488568	180752.695630	36.610586
1526.876123	181029.036884	36.615604
1528.395044	181296.850048	36.620621
1529.611829	181583.480509	36.625639
1531.179489	181871.047464	36.630656
1532.850410	182141.252092	36.635674
1534.302958	182416.114176	36.640692
1535.965074	182676.416339	36.645709
1537.477811	182933.923354	36.650727
1538.739998	183199.674014	36.655744
1540.338416	183466.820501	36.660762
1541.586245	183739.356323	36.665780
1543.373701	183988.670143	36.670797
1544.766606	184263.648393	36.675815
1546.191951	184587.083497	36.680832
1547.714044	184886.375431	36.685850
1549.014070	185164.926551	36.690868
1550.782336	185437.690339	36.695885
1552.113722	185721.216302	36.700903
1553.469768	186004.129602	36.705920
1555.201769	186287.035631	36.710938
1556.612643	186580.990639	36.715956
1558.290775	186872.593283	36.720973
1559.792070	187161.989241	36.725991
1561.417663	187450.147344	36.731008
1562.944343	187729.330201	36.736026
1564.347466	188040.638430	36.741044
1566.005723	188330.343141	36.746061
1567.754245	188626.562262	36.751079
1569.169702	188924.053497	36.756096
1570.732953	189228.050203	36.761114
1572.335004	189531.609850	36.766132
1573.865654	189826.316815	36.771149
1575.698818	190138.274759	36.776167
1577.054001	190427.168658	36.781184
1579.084512	190731.477209	36.786202
1580.644042	191040.940345	36.791220
1582.100222	191344.679943	36.796237
1584.024469	191645.730793	36.801255
1585.293842	191954.251067	36.806272
1587.032892	192252.131919	36.811290
1588.591567	192562.157882	36.816308
1590.032007	192864.328864	36.821325
1591.372926	193177.667135	36.826343
1593.509773	193485.547413	36.831360
1594.814398	193789.646920	36.836378
1596.341146	194111.950344	36.841396
1598.268610	194417.223893	36.846413
1599.888965	194730.369776	36.851431
1601.825535	195044.228942	36.856448
1603.516253	195346.010891	36.861466
1604.820051	195664.415750	36.866484
1606.881609	195965.455188	36.871501
1608.515459	196262.116957	36.876519
1610.009389	196571.425808	36.881536
1611.809370	196881.551088	36.886554
1613.219467	197189.197892	36.891572
1615.235904	197484.989470	36.896589
1616.748063	197790.284611	36.901607
1618.265646	198098.983370	36.906624
1619.861038	198403.809507	36.911642
1621.796177	198703.731322	36.916660
1623.302524	199007.835944	36.921677
1625.019390	199305.583119	36.926695
1626.649736	199609.161465	36.931712
1628.461866	199906.539235	36.936730
1629.937088	200214.816992	36.941748
1631.637982	200509.723868	36.946765
1633.044798	200823.398738	36.951783
1634.388248	201130.200097	36.956800
1636.562447	201429.505327	36.961818
1637.899088	201738.772874	36.966836
1639.608051	202043.562685	36.971853
1641.642581	202331.790478	36.976871
1642.821112	202620.686154	36.981888
1644.685365	202906.833115	36.986906
1646.072231	203200.269565	36.991924
1647.458968	203465.535005	36.996941
1649.316896	203760.549789	37.001959
1651.085300	204051.006558	37.006976
1652.619762	204333.015866	37.011994
1654.307422	204625.518351	37.017012
1655.956539	204913.658020	37.022029
1657.468312	205204.918742	37.027047
1658.894597	205505.084266	37.032064
1660.840390	205806.540682	37.037082
1662.351151	206099.479417	37.042100
1663.959916	206403.809156	37.047117
1665.658541	206692.273778	37.052135
1666.829281	207000.966009	37.057152
1668.792123	207309.890350	37.062170
1670.031710	207615.448069	37.067188
1672.004364	207924.651137	37.072205
1673.975147	208236.776270	37.077223
1675.328408	208549.176272	37.082240
1676.936643	208855.236765	37.087258
1678.340229	209192.499490	37.092276
1680.385110	209503.166644	37.097293
1681.777162	209820.007735	37.102311
1683.702274	210143.929537	37.107328
1685.348237	210469.546635	37.112346
1686.824228	210797.959692	37.117364
1688.879899	211124.326347	37.122381
1690.517555	211447.253107	37.127399
1691.972975	211781.538709	37.132416
1694.235342	212103.834941	37.137434
1695.889646	212432.374331	37.142452
1697.554177	212760.328177	37.147469
1699.191821	213089.048670	37.152487
1700.808574	213422.497833	37.157504
1702.417038	213751.858625	37.162522
1704.138826	214074.952678	37.167540
1706.144018	214409.967820	37.172557
1707.905598	214744.970576	37.177575
1709.264180	215083.491600	37.182592
1711.465228	215415.022049	37.187610
1713.353733	215746.398443	37.192628
1714.786242	216071.698727	37.197645
1716.567011	216407.309518	37.202663
1718.243410	216752.031469	37.207680
1720.361541	217073.236761	37.212698
1721.767629	217407.077808	37.217716
1723.560047	217748.428979	37.222733
1725.947592	218079.932124	37.227751
1727.316314	218417.869674	37.232768
1729.422751	218744.133169	37.237786
1730.836304	219085.188759	37.242804
1732.691605	219414.387948	37.247821
1734.703536	219737.008552	37.252839
1735.945400	220082.105327	37.257856
1737.900276	220412.813619	37.262874
1739.517723	220742.584089	37.267892
1741.125327	221071.365462	37.272909
1742.994918	221404.551655	37.277927
1744.855865	221735.656175	37.282944
1746.741796	222070.313447	37.287962
1748.320185	222402.453124	37.292980
1750.367140	222733.020714	37.297997
1752.177169	223053.540031	37.303015
1753.525814	223393.235470	37.308032
1755.347142	223715.810856	37.313050
1757.309236	224047.611340	37.318068
1758.807625	224359.211960	37.323085
1760.494133	224669.436748	37.328103
1762.238433	224987.476965	37.333120
1763.989230	225289.537001	37.338138
1765.535872	225612.155488	37.343156
1767.217064	225924.946933	37.348173
1769.568353	226245.584980	37.353191
1771.005494	226568.169744	37.358208
1772.748624	226874.092324	37.363226
1774.360018	227194.185552	37.368244
1775.488366	227527.920096	37.373261
1777.677792	227850.691808	37.378279
1779.382767	228184.310585	37.383296
1780.943260	228513.582394	37.388314
1782.721370	228844.649155	37.393332
1783.913833	229195.216151	37.398349
1786.054452	229530.392240	37.403367
1787.572951	229887.258981	37.408384
1788.901658	230238.490183	37.413402
1790.773716	230591.922570	37.418420
1792.918442	230950.113479	37.423437
1794.645104	231304.940094	37.428455
1796.417039	231679.269679	37.433472
1798.397793	232031.617360	37.438490
1800.132866	232399.067810	37.443508
1801.802718	232764.114859	37.448525
1803.957313	233123.547761	37.453543
1806.037521	233498.488420	37.458560
1807.557584	233851.719938	37.463578
1809.641739	234211.518730	37.468596
1811.342052	234578.820621	37.473613
1813.713308	234948.278153	37.478631
1815.406539	235319.467301	37.483648
1816.918508	235684.739996	37.488666
1818.987227	236047.156224	37.493684
1821.066997	236413.406336	37.498701
1823.007009	236771.853619	37.503719
1824.546674	237141.413774	37.508736
1826.504390	237505.522547	37.513754
1828.451240	237865.949103	37.518772
1830.630208	238241.581075	37.523789
1832.210512	238598.609277	37.528807
1833.695655	238976.838475	37.533824
1835.740282	239335.622201	37.538842
1837.675886	239701.916558	37.543860
1839.767607	240073.622341	37.548877
1841.767406	240440.642383	37.553895
1843.628923	240810.249300	37.558912
1845.427300	241179.738560	37.563930
1847.560790	241539.292982	37.568948
1848.978443	241907.341965	37.573965
1850.944928	242269.563397	37.578983
1853.165665	242635.148520	37.584000
1854.795377	243003.391270	37.589018
1856.799872	243362.226457	37.594036
1858.619384	243729.854064	37.599053
1860.617714	244093.769647	37.604071
1862.537056	244463.793684	37.609088
1864.527400	244813.559859	37.614106
1866.394446	245181.660199	37.619124
1867.878919	245550.607230	37.624141
1870.272206	245904.703178	37.629159
1871.968339	246272.929879	37.634176
1873.688562	246628.831819	37.639194
1875.805906	246993.307848	37.644212
1877.387569	247364.420854	37.649229
1879.543593	247719.388851	37.654247
1881.294922	248070.634510	37.659264
1882.929228	248416.410869	37.664282
1885.090275	248762.332750	37.669300
1886.516951	249106.489081	37.674317
1888.672660	249444.180079	37.679335
1890.341952	249792.640847	37.684352
1892.258000	250136.235863	37.689370
1893.865637	250476.423731	37.694388
1895.556840	250835.547743	37.699405
1897.528418	251183.882032	37.704423
1899.226122	251537.846831	37.709440
1900.938849	251898.057336	37.714458
1903.008912	252263.215242	37.719476
1904.986424	252632.654243	37.724493
1906.798958	252999.704982	37.729511
1908.494543	253371.040580	37.734528
1910.124321	253736.314551	37.739546
1912.551197	254105.958935	37.744564
1913.862146	254489.925562	37.749581
1915.938346	254852.612059	37.754599
1917.784694	255246.373951	37.759616
1919.495599	255639.089047	37.764634
1921.819860	256027.719044	37.769652
1923.684470	256420.052177	37.774669
1925.846005	256809.594369	37.779687
1927.640118	257199.675496	37.784704
1929.235832	257592.428164	37.789722
1931.522090	257985.223967	37.794740
1932.878706	258388.679874	37.799757
1935.192442	258781.875265	37.804775
1937.347633	259184.822589	37.809792
1939.446959	259591.612770	37.814810
1940.899092	259992.406744	37.819828
1943.381563	260395.476561	37.824845
1945.073694	260793.004407	37.829863
1947.347729	261197.704249	37.834880
1949.028458	261604.730682	37.839898
1951.122405	262002.267625	37.844916
1953.140113	262411.143386	37.849933
1955.159483	262815.877214	37.854951
1957.281143	263227.654621	37.859968
1959.225348	263640.753593	37.864986
1961.378608	264043.404491	37.870004
1963.340871	264451.569986	37.875021
1965.223814	264857.790554	37.880039
1967.665063	265264.099959	37.885056
1969.600701	265669.521694	37.890074
1972.007158	266060.466954	37.895092
1973.333392	266467.047578	37.900109
1975.325670	266869.433131	37.905127
1977.669219	267273.209793	37.910144
1979.295105	267679.535321	37.915162
1981.750450	268079.201967	37.920180
1983.352866	268494.975908	37.925197
1985.769093	268887.051187	37.930215
1987.622437	269298.972585	37.935232
1989.639414	269709.723643	37.940250
1991.687651	270106.803939	37.945268
1993.793204	270517.994668	37.950285
1995.654373	270917.894427	37.955303
1997.916570	271326.847352	37.960320
1999.975056	271725.214159	37.965338
2001.741601	272121.872427	37.970356
2003.551335	272533.684225	37.975373
2006.076363	272927.680419	37.980391
2007.558506	273325.317348	37.985408
2009.968280	273733.550117	37.990426
2012.170522	274130.613449	37.995444
2013.856945	274530.117478	38.000461
2015.900731	274902.110134	38.005479
2017.660683	275278.158132	38.010496
2019.444299	275661.337026	38.015514
2021.996911	276046.400078	38.020532
2023.652924	276423.551051	38.025549
2025.562171	276812.596659	38.030567
2027.377011	277193.096775	38.035584
2029.119418	277593.668887	38.040602
2031.482862	277987.158028	38.045620
2033.570578	278393.512941	38.050637
2035.631071	278773.154234	38.055655
2037.662992	279170.676226	38.060672
2039.265117	279566.917444	38.065690
2041.196531	279976.335736	38.070708
2043.216209	280377.306950	38.075725
2045.234720	280785.843737	38.080743
2047.509370	281197.512473	38.085760
2049.327867	281609.174072	38.090778
2051.466519	282017.761345	38.095796
2053.565670	282436.281502	38.100813
2055.391607	282857.381329	38.105831
2057.570321	283284.060842	38.110848
2059.280754	283703.396140	38.115866
2061.494250	284134.483496	38.120884
2063.674152	284568.011170	38.125901
2065.660950	285004.156409	38.130919
2067.945816	285419.684035	38.135936
2069.727992	285861.645359	38.140954
2072.251045	286289.547384	38.145972
2074.003313	286727.470276	38.150989
2076.308611	287164.135715	38.156007
2078.628625	287589.572691	38.161024
2080.482433	288033.666669	38.166042
2082.866219	288467.340288	38.171060
2084.624962	288913.271309	38.176077
2087.311916	289360.323571	38.181095
2089.034873	289791.933354	38.186112
2091.114673	290234.935687	38.191130
2093.685871	290663.512220	38.196148
2095.624665	291109.069504	38.201165
2097.593618	291554.415743	38.206183
2099.827964	291993.166555	38.211200
2102.140234	292442.489680	38.216218
2104.337246	292879.970443	38.221236
2106.496034	293325.680271	38.226253
2108.262180	293770.254908	38.231271
2110.667023	294214.421629	38.236288
2112.713304	294664.912222	38.241306
2115.066855	295102.885331	38.246324
2116.748020	295546.038096	38.251341
2119.031427	295990.007244	38.256359
2121.617984	296434.484088	38.261376
2123.416383	296880.553304	38.266394
2126.025975	297322.303105	38.271412
2128.148343	297777.860450	38.276429
2130.436294	298205.690397	38.281447
2132.473831	298650.362668	38.286464
2134.435675	299087.858664	38.291482
2136.776886	299528.617531	38.296500
2138.961674	299969.803520	38.301517
2141.098607	300416.426146	38.306535
2143.295183	300851.002651	38.311552
2145.389492	301293.943685	38.316570
2147.552250	301736.184932	38.321588
2150.200155	302164.689108	38.326605
2151.743248	302612.376394	38.331623
2153.798591	303032.309792	38.336640
2155.635410	303467.048125	38.341658
2157.974197	303888.148787	38.346676
2160.334847	304312.263383	38.351693
2162.224877	304734.950435	38.356711
2163.931008	305148.118300	38.361728
2166.213894	305572.310796	38.366746
2168.126511	305996.633826	38.371764
2170.306459	306414.134044	38.376781
2172.631435	306845.518203	38.381799
2174.780284	307269.565071	38.386816
2176.729675	307710.443040	38.391834
2178.732184	308146.714494	38.396852
2181.195571	308577.731948	38.401869
2182.834642	309019.484353	38.406887
2185.117715	309474.914444	38.411904
2187.088784	309927.140191	38.416922
2188.893728	310375.758118	38.421940
2191.254495	310832.889154	38.426957
2193.608472	311295.879891	38.431975
2196.004212	311751.930605	38.436992
2198.059122	312223.486994	38.442010
2200.126602	312687.244916	38.447028
2202.123360	313157.608105	38.452045
2204.250146	313636.879870	38.457063
2206.751186	314104.413518	38.462080
2208.814832	314587.289151	38.467098
2211.305442	315071.057280	38.472116
2213.420406	315536.580949	38.477133
2215.731453	316012.956508	38.482151
2218.292964	316504.717774	38.487168
2220.437370	316989.788351	38.492186
2222.339378	317468.953183	38.497204
2224.705103	317957.277638	38.502221
2227.254157	318442.649622	38.507239
2229.483741	318923.193850	38.512256
2231.837203	319418.939300	38.517274
2234.114492	319906.672100	38.522292
2236.398720	320394.855054	38.527309
2238.442753	320882.638633	38.532327
2241.107888	321383.159392	38.537344
2243.144825	321863.193344	38.542362
2245.417669	322360.109895	38.547380
2247.928118	322849.777043	38.552397
2250.039468	323351.959594	38.557415
2252.639618	323834.470987	38.562432
2254.903194	324328.548996	38.567450
2257.470661	324817.321263	38.572468
2259.800059	325302.268243	38.577485
2261.748070	325794.957022	38.582503
2264.520035	326276.702296	38.587520
2266.517139	326774.674271	38.592538
2268.881863	327264.894926	38.597556
2271.233751	327738.899236	38.602573
2273.507059	328225.240544	38.607591
2276.072827	328708.434883	38.612608
2278.104076	329208.451424	38.617626
2280.644399	329693.362815	38.622644
2283.031548	330178.038436	38.627661
2285.109390	330652.938382	38.632679
2287.755462	331141.087808	38.637696
2290.068391	331633.824182	38.642714
2292.242331	332100.091168	38.647732
2294.734180	332582.005672	38.652749
2297.036963	333071.858422	38.657767
2299.461803	333549.940524	38.662784
2301.983933	334016.915821	38.667802
2303.920913	334495.417331	38.672820
2306.236361	334975.755990	38.677837
2308.438736	335445.249336	38.682855
2310.854694	335902.908115	38.687872
2312.867350	336354.409695	38.692890
2315.085340	336807.978916	38.697908
2317.163878	337254.132349	38.702925
2319.495246	337711.198326	38.707943
2321.548889	338165.714803	38.712960
2323.640410	338632.343665	38.717978
2326.048491	339098.384302	38.722996
2328.396959	339569.069695	38.728013
2330.671898	340032.430431	38.733031
2332.742335	340511.161574	38.738048
2335.257083	340988.650051	38.743066
2337.223685	341472.685116	38.748084
2339.424878	341958.299943	38.753101
2341.691630	342452.596696	38.758119
2344.250807	342945.319008	38.763136
2346.248010	343447.099867	38.768154
2348.436321	343945.293083	38.773172
2350.799403	344438.836218	38.778189
2353.249516	344951.352881	38.783207
2355.627340	345463.568813	38.788224
2357.880777	345966.743377	38.793242
2360.267078	346489.390226	38.798260
2362.997979	346996.608100	38.803277
2364.955461	347516.389828	38.808295
2367.234704	348038.724895	38.813312
2369.836263	348555.600312	38.818330
2372.338179	349079.278725	38.823348
2375.078978	349596.496358	38.828365
2377.284768	350141.807401	38.833383
2379.614749	350657.322948	38.838400
2382.089230	351182.924241	38.843418
2384.652614	351723.791727	38.848436
2386.956508	352244.940018	38.853453
2389.332141	352785.387960	38.858471
2391.501053	353314.805147	38.863488
2394.446085	353851.723244	38.868506
2396.684037	354392.925935	38.873524
2399.391016	354924.006659	38.878541
2401.897387	355465.148891	38.883559
2404.522416	355987.173960	38.888576
2406.788632	356514.088330	38.893594
2408.729738	357059.398010	38.898612
2411.688639	357587.326480	38.903629
2413.795769	358133.529094	38.908647
2416.508765	358667.814696	38.913664
2419.182796	359206.532964	38.918682
2421.494455	359740.330179	38.923700
2423.822273	360276.498088	38.928717
2426.431632	360812.333590	38.933735
2429.003570	361350.370505	38.938752
2431.548647	361882.470965	38.943770
2433.872225	362418.727872	38.948788
2436.473298	362954.982354	38.953805
2438.910583	363489.047728	38.958823
2441.176606	364034.991243	38.963840
2443.868351	364558.074022	38.968858
2446.196374	365106.547528	38.973876
2448.355773	365639.096472	38.978893
2451.123905	366180.182113	38.983911
2453.767414	366716.056678	38.988928
2456.272804	367255.515969	38.993946
2458.221804	367795.254841	38.998964
2460.717636	368321.923688	39.003981
2463.197156	368868.299750	39.008999
2465.588954	369404.897968	39.014016
2468.414284	369944.686872	39.019034
2470.814976	370471.431842	39.024052
2473.693843	370984.840336	39.029069
2475.810615	371500.284220	39.034087
2478.183132	372004.783605	39.039104
2480.550849	372500.761447	39.044122
2482.572035	373014.443847	39.049140
2485.084158	373523.074068	39.054157
2487.448017	374051.200770	39.059175
2489.846888	374561.324153	39.064192
2492.405640	375089.476237	39.069210
2494.659582	375615.943007	39.074228
2497.049265	376143.771604	39.079245
2499.548401	376684.847054	39.084263
2501.771759	377221.572248	39.089280
2504.328816	377750.862941	39.094298
2506.894535	378307.068774	39.099316
2509.590619	378852.907653	39.104333
2511.868053	379397.787529	39.109351
2514.113018	379956.567140	39.114368
2516.525617	380510.977362	39.119386
2518.864910	381077.823572	39.124404
2521.556240	381637.865149	39.129421
2524.215541	382197.089165	39.134439
2526.560639	382777.650088	39.139456
2529.202118	383341.486888	39.144474
2531.506860	383933.602110	39.149492
2534.296688	384509.242406	39.154509
2536.677668	385090.201137	39.159527
2539.042795	385676.948228	39.164544
2541.855303	386271.563257	39.169562
2544.347638	386866.492872	39.174580
2546.479958	387446.980418	39.179597
2549.483986	388052.057305	39.184615
2552.048989	388654.326889	39.189632
2554.651167	389254.221248	39.194650
2557.007564	389847.657645	39.199668
2559.985069	390460.225105	39.204685
2562.412210	391061.318134	39.209703
2565.112290	391660.632080	39.214720
2567.611774	392267.051470	39.219738
2570.335138	392882.332121	39.224756
2573.443090	393477.891798	39.229773
2575.859227	394081.443326	39.234791
2578.581928	394697.437169	39.239808
2581.367276	395300.849597	39.244826
2584.046443	395899.251300	39.249844
2586.473810	396500.562953	39.254861
2589.605482	397110.760267	39.259879
2591.872712	397717.128399	39.264896
2594.947954	398315.609403	39.269914
2597.478128	398915.223374	39.274932
2600.372246	399519.168855	39.279949
2602.904748	400109.083488	39.284967
2605.323763	400716.362255	39.289984
2608.015134	401298.882309	39.295002
2610.993992	401908.724680	39.300020
2613.760616	402509.878685	39.305037
2616.606927	403099.920579	39.310055
2619.370951	403693.452118	39.315072
2622.117606	404276.747937	39.320090
2624.339948	404872.357636	39.325108
2627.038471	405448.950548	39.330125
2629.873748	406040.688620	39.335143
2632.372641	406633.678133	39.340160
2635.198481	407224.526075	39.345178
2637.844513	407815.437039	39.350196
2640.585438	408397.766155	39.355213
2643.019387	408977.952224	39.360231
2645.842419	409561.755695	39.365248
2648.163765	410123.765002	39.370266
2650.694573	410667.310943	39.375284
2652.994112	411219.328478	39.380301
2656.109705	411768.674806	39.385319
2658.260243	412333.689287	39.390336
2660.935660	412881.254982	39.395354
2663.273955	413445.300404	39.400372
2665.961071	414008.618845	39.405389
2668.728223	414580.964622	39.410407
2671.169552	415154.104766	39.415424
2673.991325	415717.913470	39.420442
2676.450171	416301.237512	39.425460
2678.896907	416874.178618	39.430477
2681.339137	417457.068711	39.435495
2683.672617	418052.957804	39.440512
2686.789975	418645.774014	39.445530
2689.512445	419251.784285	39.450548
2692.088829	419849.253091	39.455565
2694.631156	420462.032927	39.460583
2696.856222	421067.056600	39.465600
2699.563144	421677.600180	39.470618
2702.141699	422304.832522	39.475636
2704.954355	422925.132286	39.480653
2708.085344	423549.509600	39.485671
2710.474798	424190.213958	39.490688
2713.268158	424810.358201	39.495706
2716.118947	425453.579589	39.500724
2718.689527	426083.376219	39.505741
2721.486531	426719.032656	39.510759
2723.953159	427365.286270	39.515776
2727.132456	428003.824751	39.520794
2729.609286	428650.641742	39.525812
2732.249103	429303.629633	39.530829
2735.250088	429943.599491	39.535847
2737.915072	430600.179952	39.540864
2740.988059	431260.212716	39.545882
2743.882091	431919.290932	39.550900
2746.694333	432572.092720	39.555917
2749.411711	433221.349760	39.560935
2752.057787	433872.819838	39.565952
2755.093920	434534.212897	39.570970
2757.910410	435185.814158	39.575988
2760.353270	435850.286762	39.581005
2763.385444	436511.208130	39.586023
2766.386524	437174.587349	39.591040
2769.107338	437838.391481	39.596058
2772.131828	438496.769297	39.601076
2775.229792	439160.063922	39.606093
2778.260278	439808.391550	39.611111
2780.950907	440460.084224	39.616128
2783.744258	441115.425935	39.621146
2786.498428	441775.499246	39.626164
2789.393718	442429.212846	39.631181
2792.426599	443078.436833	39.636199
2795.139797	443734.860495	39.641216
2797.977779	444382.048724	39.646234
2800.893503	445039.505395	39.651252
2803.631418	445687.521864	39.656269
2806.715637	446339.501451	39.661287
2809.098804	446981.618569	39.666304
2812.206096	447637.083136	39.671322
2815.003284	448287.472201	39.676340
2817.804885	448946.471947	39.681357
2820.884142	449591.518280	39.686375
2823.519516	450243.124343	39.691392
2826.342321	450884.276342	39.696410
2829.339585	451540.928505	39.701428
2831.784200	452170.935362	39.706445
2834.587595	452782.638646	39.711463
2837.291744	453405.543583	39.716480
2839.963906	454016.164520	39.721498
2842.873007	454629.251194	39.726516
2845.650887	455257.631783	39.731533
2848.226347	455883.194788	39.736551
2851.036923	456512.282269	39.741568
2853.649819	457133.403256	39.746586
2856.543284	457757.385428	39.751604
2858.992450	458410.282741	39.756621
2861.778593	459044.328959	39.761639
2864.521814	459691.428964	39.766656
2867.162757	460343.617325	39.771674
2870.432179	460996.994525	39.776692
2872.685641	461670.336035	39.781709
2875.908232	462319.532153	39.786727
2878.191559	462985.349175	39.791744
2881.311721	463659.989801	39.796762
2884.336265	464334.214766	39.801780
2886.750332	465024.248297	39.806797
2889.767868	465710.072837	39.811815
2892.480185	466405.097947	39.816832
2895.389209	467102.484561	39.821850
2898.359910	467786.818525	39.826868
2901.227093	468496.057107	39.831885
2904.279379	469190.105329	39.836903
2906.929825	469912.127758	39.841920
2909.726355	470616.293046	39.846938
2913.007256	471337.649761	39.851956
2915.746211	472056.487511	39.856973
2919.257375	472780.971667	39.861991
2921.812839	473503.354274	39.867008
2924.865203	474225.727748	39.872026
2928.380528	474946.584727	39.877044
2931.173111	475681.891055	39.882061
2934.301069	476407.885419	39.887079
2937.297582	477131.296336	39.892096
2940.185165	477853.078321	39.897114
2943.123144	478568.770749	39.902132
2946.266872	479317.464271	39.907149
2949.089845	480045.507411	39.912167
2952.083836	480769.256511	39.917184
2955.763254	481498.912788	39.922202
2958.568483	482227.159859	39.927220
2961.583516	482946.470924	39.932237
2964.153641	483671.159722	39.937255
2967.633665	484402.525209	39.942272
2970.408048	485133.815279	39.947290
2973.699002	485862.470703	39.952308
2976.632536	486592.507768	39.957325
2980.109185	487322.425136	39.962343
2983.098625	488040.696471	39.967360
2985.639832	488766.560163	39.972378
2988.953201	489489.145398	39.977396
2991.933080	490217.288944	39.982413
2995.088123	490947.686884	39.987431
2998.263508	491666.160223	39.992448
3001.390255	492386.520563	39.997466
3004.471590	493106.651926	40.002484
3007.437622	493835.226612	40.007501
3010.264002	494546.264056	40.012519
3013.716230	495271.620725	40.017536
3016.494704	495975.346432	40.022554
3019.399569	496694.676925	40.027572
3022.074804	497422.717888	40.032589
3025.092441	498143.319237	40.037607
3028.321223	498868.080691	40.042624
3031.296532	499575.429041	40.047642
3034.409790	500266.614238	40.052660
3036.943326	500956.347227	40.057677
3039.919790	501638.227262	40.062695
3042.727907	502319.094899	40.067712
3045.978642	503012.744546	40.072730
3049.039902	503707.698768	40.077748
3051.893856	504408.337981	40.082765
3054.911473	505100.463827	40.087783
3057.694776	505794.957588	40.092800
3060.794041	506510.700921	40.097818
3063.559674	507209.455285	40.102836
3066.602075	507930.569398	40.107853
3068.954625	508642.749834	40.112871
3072.785935	509366.937019	40.117888
3075.433691	510107.267484	40.122906
3078.550820	510832.194893	40.127924
3081.212955	511575.211823	40.132941
3083.974063	512320.135073	40.137959
3087.385390	513067.582086	40.142976
3090.002640	513825.069785	40.147994
3093.849002	514588.659611	40.153012
3096.923813	515352.830574	40.158029
3099.996049	516102.278068	40.163047
3102.915493	516870.763064	40.168064
3105.934759	517645.573933	40.173082
3108.939287	518421.298201	40.178100
3112.151819	519205.038720	40.183117
3115.523418	519976.545063	40.188135
3118.433603	520770.144329	40.193152
3121.785293	521558.250182	40.198170
3125.225882	522338.958608	40.203188
3128.402737	523131.220914	40.208205
3131.138192	523922.852036	40.213223
3134.481953	524709.919332	40.218240
3137.493175	525514.929021	40.223258
3140.799242	526306.379237	40.228276
3143.577945	527115.296976	40.233293
3147.049694	527920.540308	40.238311
3150.605590	528731.397303	40.243328
3153.963701	529528.723639	40.248346
3157.592242	530337.058839	40.253364
3160.325396	531138.553252	40.258381
3163.556362	531939.418231	40.263399
3166.946825	532737.697998	40.268416
3170.351983	533545.818103	40.273434
3173.391133	534336.170541	40.278452
3176.678688	535139.037424	40.283469
3179.934038	535943.867209	40.288487
3183.664561	536736.122366	40.293504
3186.728575	537537.166819	40.298522
3190.101276	538330.131708	40.303540
3193.592528	539132.062845	40.308557
3196.451381	539917.931760	40.313575
3199.954822	540706.160178	40.318592
3202.938796	541507.066158	40.323610
3206.594276	542293.916666	40.328628
3209.639903	543082.117604	40.333645
3212.790125	543881.992653	40.338663
3216.295445	544673.181952	40.343680
3219.368335	545463.686129	40.348698
3222.807069	546250.972591	40.353716
3226.029532	547049.378005	40.358733
3229.125685	547840.629301	40.363751
3232.675056	548614.757044	40.368768
3235.871945	549404.688084	40.373786
3238.828218	550183.974704	40.378804
3242.335885	550974.959071	40.383821
3245.277854	551739.606912	40.388839
3248.407346	552481.365038	40.393856
3251.698986	553229.268929	40.398874
3254.507158	553977.552991	40.403892
3257.974939	554718.519215	40.408909
3261.145958	555467.205290	40.413927
3264.208915	556218.267314	40.418944
3267.263157	556979.908552	40.423962
3270.514209	557732.299376	40.428980
3273.516720	558486.335171	40.433997
3276.603610	559254.290140	40.439015
3279.986270	560021.146965	40.444032
3283.122228	560799.866726	40.449050
3286.377079	561575.660822	40.454068
3289.583882	562365.938848	40.459085
3292.601054	563148.679484	40.464103
3296.362951	563941.068653	40.469120
3299.056158	564746.793529	40.474138
3302.671353	565531.133982	40.479156
3305.585119	566342.873785	40.484173
3308.610222	567154.639438	40.489191
3312.099750	567962.870603	40.494208
3315.074634	568810.078044	40.499226
3318.486169	569626.715983	40.504244
3322.171475	570458.571372	40.509261
3325.306241	571296.809482	40.514279
3328.920569	572124.800320	40.519296
3332.240439	572963.537498	40.524314
3335.137984	573817.392429	40.529332
3338.499089	574658.249747	40.534349
3342.249419	575509.591614	40.539367
3345.496725	576359.146496	40.544384
3348.683002	577223.905892	40.549402
3351.927965	578078.383936	40.554420
3355.278733	578946.636336	40.559437
3358.970434	579818.519161	40.564455
3362.745371	580684.118711	40.569472
3366.028602	581557.379166	40.574490
3369.964357	582419.117040	40.579508
3373.020090	583288.375560	40.584525
3376.419766	584158.761564	40.589543
3379.406187	585018.994087	40.594560
3382.921126	585905.271673	40.599578
3386.495191	586773.472677	40.604596
3390.135403	587641.744005	40.609613
3393.075593	588522.699991	40.614631
3397.165326	589394.309130	40.619648
3400.285357	590276.843169	40.624666
3403.711550	591150.912560	40.629684
3407.110712	592034.807662	40.634701
3410.556585	592913.276957	40.639719
3414.070462	593792.462664	40.644736
3417.432092	594687.433896	40.649754
3420.912556	595571.073317	40.654772
3424.163639	596454.225466	40.659789
3427.687343	597343.004087	40.664807
3431.898997	598221.164138	40.669824
3435.032196	599111.652170	40.674842
3438.252631	599983.528751	40.679860
3441.750412	600869.017638	40.684877
3445.559402	601756.978438	40.689895
3448.991183	602625.955707	40.694912
3452.226182	603508.366304	40.699930
3455.962573	604385.333533	40.704948
3459.356039	605266.072338	40.709965
3462.596146	606143.865927	40.714983
3466.445686	607016.001263	40.720000
3469.806109	607894.474564	40.725018
3472.904047	608756.395742	40.730023
3476.602125	609583.007471	40.735028
3479.562298	610357.814856	40.740032
3483.121939	611082.020521	40.745037
3485.978546	611758.788530	40.750042
3488.812452	612364.125466	40.755047
3491.873915	612928.898788	40.760052
3494.219776	613447.714091	40.765056
3497.100485	613888.142579	40.770061
3499.339944	614305.759782	40.775066
3501.424700	614651.510845	40.780071
3503.621402	614940.955243	40.785076
3505.382151	615198.323209	40.790080
3507.538367	615416.990159	40.795085
3509.229510	615590.246341	40.800090
3510.792808	615704.198020	40.805095
3512.019499	615787.166151	40.810100
3513.481365	615850.956271	40.815104
3514.723938	615869.902548	40.820109
3515.842374	615870.977057	40.825114
3516.600681	615824.381355	40.830119
3517.664355	615757.847331	40.835124
3518.382277	615672.475902	40.840128
3519.571269	615563.890868	40.845133
3520.010723	615429.833393	40.850138
3520.619717	615282.203536	40.855143
3521.263536	615101.579900	40.860148
3521.562481	614925.655071	40.865152
3522.430757	614716.750693	40.870157
3523.084031	614496.279740	40.875162
3523.234446	614262.237137	40.880167
3522.963994	614022.556654	40.885172
3523.119586	613770.307434	40.890176
3523.607776	613514.350855	40.895181
3523.937932	613255.063272	40.900186
3523.911268	612980.727945	40.905191
3524.266055	612700.976495	40.910196
3523.948250	612416.373195	40.915200
3524.174738	612116.578643	40.920205
3524.127716	611823.617342	40.925210
3523.814599	611529.639232	40.930215
3524.101520	611219.809326	40.935220
3524.041548	610924.824143	40.940224
3524.009167	610623.525917	40.945229
3523.766794	610314.601161	40.950234
3523.714393	610008.837599	40.955239
3523.738993	609706.153177	40.960244
3523.405637	609402.915635	40.965248
3523.380062	609084.518302	40.970253
3523.501311	608783.141616	40.975258
3523.270698	608476.009677	40.980263
3522.809573	608162.152747	40.985268
3522.518927	607854.661441	40.990272
3522.612345	607551.352252	40.995277
3522.080505	607248.031799	41.000282
3522.060054	606943.822123	41.005287
3521.726697	606648.456005	41.010292
3521.670800	606359.290791	41.015296
3521.617386	606063.413904	41.020301
3521.243330	605771.780739	41.025306
3520.756532	605483.108499	41.030311
3521.003129	605184.107851	41.035316
3520.669817	604909.603465	41.040320
3520.114773	604614.313734	41.045325
3520.121121	604346.395353	41.050330
3519.479391	604057.807550	41.055335
3519.807848	603785.321295	41.060340
3519.198826	603528.185341	41.065344
3518.978516	603248.465524	41.070349
3519.102258	602990.100861	41.075354
3519.065621	602719.144833	41.080359
3519.074919	602461.035105	41.085364
3518.701005	602201.427570	41.090368
3518.546538	601944.481602	41.095373
3518.098696	601687.875425	41.100378
3517.650001	601422.505020	41.105383
3517.999806	601178.873662	41.110388
3517.554317	600930.656406	41.115392
3517.477831	600670.463770	41.120397
3517.176921	600427.166859	41.125402
3516.916275	600188.863185	41.130407
3516.749324	599949.037847	41.135412
3516.308609	599711.352092	41.140416
3516.449795	599480.928106	41.145421
3516.364546	599256.591278	41.150426
3515.578824	599027.403475	41.155431
3515.998771	598801.426167	41.160436
3515.278273	598584.032294	41.165440
3515.208753	598354.417491	41.170445
3515.063163	598143.432518	41.175450
3514.403854	597931.071810	41.180455
3514.818358	597726.449008	41.185460
3514.307225	597531.879724	41.190464
3514.023346	597316.494135	41.195469
3514.190610	597118.556916	41.200474
3513.793020	596912.443160	41.205479
3513.291945	596718.708462	41.210484
3513.331639	596534.198564	41.215488
3513.250254	596344.897643	41.220493
3512.884741	596161.896636	41.225498
3512.594680	595978.079519	41.230503
3512.741369	595788.132131	41.235508
3512.833821	595620.272297	41.240512
3512.409359	595443.477223	41.245517
3512.395770	595270.420691	41.250522
3512.045714	595093.157472	41.255527
3511.776887	594925.343130	41.260532
3511.306321	594759.610858	41.265536
3511.511449	594605.488718	41.270541
3511.866844	594437.919650	41.275546
3511.497665	594270.110658	41.280551
3511.432412	594108.762002	41.285556
3511.202976	593952.044064	41.290560
3511.064937	593782.688817	41.295565
3510.673456	593641.166549	41.300570
3510.518293	593487.735648	41.305575
3510.856276	593327.063384	41.310580
3510.437324	593184.637838	41.315584
3510.048940	593031.687609	41.320589
3510.299154	592896.466131	41.325594
3509.794173	592760.309175	41.330599
3509.571619	592615.140636	41.335604
3509.542494	592487.120194	41.340608
3509.667315	592344.398095	41.345613
3509.647407	592220.630590	41.350618
3509.303152	592084.139367	41.355623
3509.378890	591948.833020	41.360628
3509.258538	591821.770617	41.365632
3509.078518	591691.009227	41.370637
3508.922196	591577.424301	41.375642
3508.210868	591442.986003	41.380647
3508.582081	591332.772450	41.385652
3508.153232	591214.517479	41.390656
3508.432479	591099.757336	41.395661
3508.311432	590984.557593	41.400666
3508.031812	590864.522106	41.405671
3508.046119	590742.134893	41.410676
3507.588938	590650.880105	41.415680
3507.701368	590539.045680	41.420685
3507.594467	590432.204074	41.425690
3507.515950	590331.418876	41.430695
3507.298744	590231.405897	41.435700
3507.500677	590128.170212	41.440704
3507.695988	590020.726190	41.445709
3507.699165	589919.723973	41.450714
3507.287043	589812.523138	41.455719
3507.554202	589714.082968	41.460724
3507.434326	589618.357794	41.465728
3506.830009	589518.599130	41.470733
3506.675256	589416.715055	41.475738
3506.730202	589323.865893	41.480743
3506.967690	589231.538535	41.485748
3506.954777	589151.374670	41.490752
3506.802686	589052.893811	41.495757
3506.622245	588965.740156	41.500762
3506.522464	588882.180756	41.505767
3506.401046	588781.688429	41.510772
3506.040951	588701.324976	41.515776
3506.161836	588612.718405	41.520781
3506.023241	588532.619710	41.525786
3506.170009	588453.327634	41.530791
3506.265867	588372.890464	41.535796
3505.853433	588295.989598	41.540800
3505.833923	588213.314428	41.545805
3505.880992	588137.092223	41.550810
3505.885815	588065.085233	41.555815
3505.981184	587986.499302	41.560820
3505.702851	587909.274073	41.565824
3505.662230	587829.555744	41.570829
3505.731302	587753.828507	41.575834
3505.503197	587676.493548	41.580839
3505.649183	587606.616207	41.585844
3505.553107	587544.443285	41.590848
3505.079688	587464.739825	41.595853
3505.470944	587395.574459	41.600858
3505.251631	587342.540020	41.605863
3505.459809	587253.858597	41.610868
3505.239448	587186.341005	41.615872
3505.159097	587127.621031	41.620877
3505.262087	587048.626221	41.625882
3504.940526	586991.546854	41.630887
3505.250591	586932.063199	41.635892
3504.768525	586867.040126	41.640896
3505.145842	586803.937021	41.645901
3505.026295	586731.990756	41.650906
3505.067245	586671.495333	41.655911
3505.024385	586601.490713	41.660916
3504.801700	586547.350380	41.665920
3504.631689	586481.223786	41.670925
3504.228377	586414.882679	41.675930
3504.249016	586366.216217	41.680935
3503.990986	586313.834333	41.685940
3504.023600	586276.993192	41.690944
3504.076838	586218.097078	41.695949
3504.646443	586170.045566	41.700954
3504.346967	586111.554840	41.705959
3504.677861	586053.165728	41.710964
3504.252954	585998.603219	41.715968
3504.401765	585951.869489	41.720973
3504.379055	585890.427432	41.725978
3504.171321	585830.818243	41.730983
3504.484485	585783.456670	41.735988
3504.041965	585738.819246	41.740992
3503.823564	585677.857660	41.745997
3504.213583	585629.481009	41.751002
3504.134150	585588.996296	41.756007
3504.440173	585541.083467	41.761012
3504.029905	585495.638078	41.766016
3503.808405	585433.021628	41.771021
3503.963963	585390.243999	41.776026
3504.073445	585338.401434	41.781031
3504.060512	585276.603547	41.786036
3504.134046	585246.919935	41.791040
3504.269126	585197.979769	41.796045
3503.955400	585136.578968	41.801050
3503.813989	585081.315965	41.806055
3504.553421	585041.753789	41.811060
3504.029652	584991.211521	41.816064
3503.982612	584948.764577	41.821069
3504.121780	584900.373797	41.826074
3504.081329	584850.858040	41.831079
3504.327939	584803.101641	41.836084
3504.179941	584759.266277	41.841088
3504.372752	584696.079601	41.846093
3504.272616	584641.158794	41.851098
3503.907632	584598.509574	41.856103
3503.987859	584551.078837	41.861108
3503.527584	584504.434144	41.866112
3503.427464	584448.610116	41.871117
3503.530405	584405.485989	41.876122
3503.131590	584377.277382	41.881127
3503.720989	584334.127054	41.886132
3504.010040	584298.341933	41.891136
3503.417715	584247.055053	41.896141
3503.802099	584199.474995	41.901146
3503.674108	584156.636625	41.906151
3503.788641	584123.484811	41.911156
3503.666531	584072.374240	41.916160
3503.787523	584034.158298	41.921165
3503.633013	583992.877383	41.926170
3503.463283	583951.498437	41.931175
3503.884429	583908.924149	41.936180
3504.037571	583861.378778	41.941184
3503.819450	583819.054462	41.946189
3503.933891	583773.870795	41.951194
3503.909391	583727.355186	41.956199
3503.821525	583681.049802	41.961204
3503.484805	583638.592944	41.966208
3503.475530	583590.420112	41.971213
3503.439593	583555.435319	41.976218
3503.149761	583525.653466	41.981223
3503.198058	583471.405417	41.986228
3503.378569	583435.433937	41.991232
3503.329928	583396.189564	41.996237
3503.823929	583361.472222	42.001242
3503.473750	583322.374986	42.006247
3503.594005	583280.396742	42.011252
3503.470946	583239.910175	42.016256
3503.700659	583195.407946	42.021261
3503.304473	583159.325193	42.026266
3502.918353	583121.436012	42.031271
3503.273701	583079.570646	42.036276
3503.124892	583042.596599	42.041280
3503.183158	583008.547847	42.046285
3503.739370	582975.925112	42.051290
3503.685891	582937.632372	42.056295
3503.627648	582904.503895	42.061300
3503.655592	582858.678271	42.066304
3503.525121	582812.075093	42.071309
3503.511441	582770.968107	42.076314
3503.205120	582735.772312	42.081319
3503.180678	582691.758981	42.086324
3503.648149	582657.745442	42.091328
3503.511872	582619.264005	42.096333
3503.593413	582580.547846	42.101338
3503.077199	582538.465739	42.106343
3503.379170	582505.630691	42.111348
3503.167344	582474.279632	42.116352
3503.316622	582431.842410	42.121357
3503.520764	582388.744694	42.126362
3503.257864	582353.089675	42.131367
3503.168008	582320.365465	42.136372
3503.113919	582286.783265	42.141376
3503.261643	582251.815756	42.146381
3503.490395	582208.362541	42.151386
3503.218644	582177.320820	42.156391
3503.195964	582136.764371	42.161396
3502.882048	582112.397147	42.166400
3503.075149	582077.421992	42.171405
3503.118265	582036.152980	42.176410
3503.185740	582008.116076	42.181415
3502.882651	581968.204484	42.186420
3502.884435	581938.924254	42.191424
3502.894614	581907.687289	42.196429
3503.121099	581867.893095	42.201434
3502.969304	581842.998558	42.206439
3502.953610	581800.684976	42.211444
3502.884757	581768.707911	42.216448
3503.056068	581738.046929	42.221453
3503.105474	581703.393883	42.226458
3502.855757	581684.129749	42.231463
3503.398950	581644.385516	42.236468
3503.304526	581609.453831	42.241472
3503.194866	581570.964577	42.246477
3503.303048	581536.552513	42.251482
3503.152443	581518.877036	42.256487
3503.007322	581474.526748	42.261492
3502.610179	581439.491431	42.266496
3502.652765	581409.752169	42.271501
3503.113521	581369.969701	42.276506
3503.035814	581348.722651	42.281511
3503.226473	581322.118800	42.286516
3502.974544	581291.572886	42.291520
3503.115810	581248.580837	42.296525
3502.947676	581204.884886	42.301530
3502.929031	581188.542039	42.306535
3503.086405	581144.744823	42.311540
3503.145471	581115.202756	42.316544
3503.209948	581076.584280	42.321549
3503.089267	581047.922527	42.326554
3502.563371	581024.338154	42.331559
3502.772445	580979.228535	42.336564
3502.971650	580950.366098	42.341568
3502.702300	580922.379099	42.346573
3502.772459	580888.973798	42.351578
3502.556900	580860.727526	42.356583
3502.891004	580834.300646	42.361588
3502.925693	580815.993377	42.366592
3502.801757	580783.370229	42.371597
3503.120981	580755.290797	42.376602
3502.467434	580727.864791	42.381607
3502.383765	580708.071573	42.386612
3502.718304	580677.281855	42.391616
3502.766002	580639.065619	42.396621
3503.148335	580621.756681	42.401626
3502.837612	580589.262448	42.406631
3503.046019	580555.082383	42.411636
3502.922385	580513.131758	42.416640
3502.634155	580492.367267	42.421645
3502.842553	580448.609471	42.426650
3502.503511	580423.891445	42.431655
3503.024141	580392.620553	42.436660
3503.220203	580369.172638	42.441664
3502.933151	580346.050920	42.446669
3502.908518	580309.399324	42.451674
3502.625418	580277.501590	42.456679
3502.728442	580225.485553	42.461684
3502.223977	580214.883564	42.466688
3502.450258	580194.689964	42.471693
3502.904184	580163.328566	42.476698
3502.723762	580141.593810	42.481703
3502.913218	580113.031592	42.486708
3502.973966	580075.764136	42.491712
3502.918988	580044.832978	42.496717
3502.829938	580023.585162	42.501722
3502.596261	579997.545928	42.506727
3502.905049	579961.543101	42.511732
3502.779581	579933.731696	42.516736
3503.091093	579904.497965	42.521741
3502.750326	579864.033068	42.526746
3502.683052	579835.008808	42.531751
3502.971284	579807.834466	42.536756
3503.128224	579777.120167	42.541760
3502.712655	579744.038088	42.546765
3502.849615	579720.999222	42.551770
3502.886512	579702.639625	42.556775
3502.969837	579660.352543	42.561780
3503.106427	579631.947798	42.566784
3502.512064	579602.202971	42.571789
3503.117358	579572.621557	42.576794
3502.672361	579533.826623	42.581799
3502.268884	579500.992669	42.586804
3502.816615	579487.066172	42.591808
3502.536305	579465.295560	42.596813
3502.860204	579437.462814	42.601818
3502.126517	579410.647850	42.606823
3502.256351	579381.792187	42.611828
3502.640223	579366.637445	42.616832
3502.523401	579340.728849	42.621837
3502.829381	579319.066892	42.626842
3503.031988	579295.615694	42.631847
3502.510188	579249.008547	42.636852
3502.647836	579234.193011	42.641856
3502.393424	579205.998751	42.646861
3502.646411	579171.657021	42.651866
3502.361017	579153.948696	42.656871
3502.773159	579113.664264	42.661876
3502.580757	579087.967495	42.666880
3502.052198	579068.842704	42.671885
3502.524388	579041.086086	42.676890
3502.336069	579026.421533	42.681895
3502.472237	578997.112533	42.686900
3502.757119	578986.235517	42.691904
3502.536117	578953.170818	42.696909
3502.804104	578921.985449	42.701914
3502.138531	578908.147606	42.706919
3502.560342	578873.828717	42.711924
3502.464428	578851.476419	42.716928
3502.250823	578838.520700	42.721933
3502.925663	578812.938476	42.726938
3502.345064	578787.953664	42.731943
3502.434093	578752.583102	42.736948
3502.522143	578736.621179	42.741952
3502.703998	578711.918214	42.746957
3502.623390	578677.276053	42.751962
3502.686255	578658.459312	42.756967
3502.851406	578625.283122	42.761972
3502.632256	578590.261133	42.766976
3502.374444	578574.102287	42.771981
3502.528873	578541.429045	42.776986
3502.262226	578520.256274	42.781991
3502.333311	578495.469843	42.786996
3502.610645	578482.236351	42.792001
3502.278402	578457.011361	42.797005
3502.432736	578427.146346	42.802010
3502.418285	578413.757777	42.807015
3502.612818	578389.001964	42.812020
3502.528228	578364.941720	42.817025
3502.549625	578340.062405	42.822029
3502.934009	578324.755713	42.827034
3502.834646	578288.359914	42.832039
3502.451618	578263.493498	42.837044
3502.611353	578223.696699	42.842049
3502.565504	578205.046650	42.847053
3502.463620	578165.842235	42.852058
3502.745723	578154.413152	42.857063
3502.509061	578127.366930	42.862068
3502.513909	578105.047539	42.867073
3502.471340	578081.581966	42.872077
3502.498339	578055.096203	42.877082
3502.248427	578036.227001	42.882087
3502.241320	578009.896927	42.887092
3502.578121	577990.283917	42.892097
3502.311546	577961.988102	42.897101
3502.589915	577927.488116	42.902106
3502.339581	577912.079466	42.907111
3502.382990	577879.822887	42.912116
3502.512965	577862.900214	42.917121
3502.296735	577836.000558	42.922125
3502.488750	577815.406768	42.927130
3502.392346	577799.271721	42.932135
3502.589306	577771.404516	42.937140
3502.352645	577748.720923	42.942145
3502.014467	577720.536002	42.947149
3502.439311	577697.598424	42.952154
3502.170983	577692.875515	42.957159
3502.075553	577663.448756	42.962164
3502.254860	577653.439607	42.967169
3502.159880	577636.200664	42.972173
3502.113215	577606.966759	42.977178
3502.410529	577590.418766	42.982183
3502.082355	577564.037520	42.987188
3502.363877	577542.426104	42.992193
3502.127386	577529.873695	42.997197
3501.966450	577508.431696	43.002202
3502.149869	577494.559681	43.007207
3502.067077	577466.033252	43.012212
3502.359194	577457.260220	43.017217
3502.245485	577429.490888	43.022221
3502.213838	577418.210419	43.027226
3502.433758	577391.542455	43.032231
3502.164390	577363.596664	43.037236
3502.458060	577331.650486	43.042241
3502.515026	577326.374991	43.047245
3502.545015	577296.526399	43.052250
3502.100014	577278.689573	43.057255
3502.274673	577250.924876	43.062260
3502.639147	577231.807795	43.067265
3502.230008	577210.303710	43.072269
3502.916579	577176.088705	43.077274
3502.277913	577169.517450	43.082279
3502.091860	577135.488896	43.087284
3502.275973	577106.267765	43.092289
3502.074757	577090.348716	43.097293
3502.154077	577071.777528	43.102298
3502.412691	577053.228441	43.107303
3502.096067	577037.778788	43.112308
3501.977984	577017.884079	43.117313
3501.960250	576997.973646	43.122317
3502.169367	576978.077874	43.127322
3502.158091	576966.191855	43.132327
3502.084186	576938.214445	43.137332
3502.200958	576918.032047	43.142337
3502.186015	576915.225417	43.147341
3502.084457	576888.456035	43.152346
3502.288518	576870.818048	43.157351
3501.773786	576848.477058	43.162356
3501.920115	576836.365623	43.167361
3502.147846	576815.012016	43.172365
3502.161341	576794.594741	43.177370
3502.173234	576784.360189	43.182375
3502.050884	576761.656724	43.187380
3502.078668	576760.649144	43.192385
3502.013557	576722.938734	43.197389
3502.177258	576704.002624	43.202394
3502.206168	576685.037394	43.207399
3502.421783	576672.212703	43.212404
3502.576379	576642.694017	43.217409
3501.882423	576621.935576	43.222413
3502.232079	576588.824833	43.227418
3501.933645	576577.133775	43.232423
3502.279939	576559.473065	43.237428
3501.881422	576542.029085	43.242433
3502.195234	576527.383074	43.247437
3502.213881	576497.534131	43.252442
3502.193026	576491.718634	43.257447
3502.383564	576460.989977	43.262452
3502.589536	576446.511205	43.267457
3501.912467	576419.028086	43.272461
3502.336286	576405.117146	43.277466
3501.848499	576384.727328	43.282471
3502.258960	576365.250454	43.287476
3501.862897	576340.281474	43.292481
3502.055612	576340.100829	43.297485
3502.112782	576312.602990	43.302490
3501.867772	576297.893555	43.307495
3501.922433	576284.140500	43.312500
3502.018028	576259.194804	43.317505
3501.943147	576257.601279	43.322509
3502.188256	576236.394344	43.327514
3502.186817	576211.814850	43.332519
3501.917435	576193.497374	43.337524
3501.651750	576173.022287	43.342529
3501.588103	576170.774877	43.347533
3502.070632	576149.380174	43.352538
3501.921589	576128.585794	43.357543
3502.028357	576131.027060	43.362548
3501.776637	576117.522350	43.367553
3501.985935	576095.518139	43.372557
3502.325082	576083.425914	43.377562
3502.337405	576054.881028	43.382567
3502.077681	576041.678458	43.387572
3502.449233	576011.020602	43.392577
3502.025244	576003.512149	43.397581
3502.097231	575969.941358	43.402586
3502.221854	575962.848752	43.407591
3502.123847	575945.557520	43.412596
3502.475097	575925.838324	43.417601
3502.102711	575895.396780	43.422605
3502.109877	575873.674555	43.427610
3502.323578	575855.080350	43.432615
3502.079330	575839.718059	43.437620
3502.479575	575822.348746	43.442625
3502.093352	575800.386892	43.447629
3502.323989	575774.967531	43.452634
3502.548692	575757.926550	43.457639
3502.243772	575726.922191	43.462644
3502.221917	575710.020011	43.467649
3501.974078	575699.223095	43.472653
3501.913921	575672.544674	43.477658
3502.141057	575670.703191	43.482663
3502.116954	575634.738498	43.487668
3502.101171	575621.396968	43.492673
3502.006677	575592.717113	43.497677
3502.092620	575585.329323	43.502682
3501.977706	575577.421108	43.507687
3501.605532	575551.794488	43.512692
3502.012732	575534.473811	43.517697
3502.151634	575517.144885	43.522701
3502.061236	575498.597632	43.527706
3501.988688	575492.338207	43.532711
3501.759702	575476.120213	43.537716
3501.880510	575460.951165	43.542721
3501.962733	575447.042281	43.547725
3501.890738	575435.314633	43.552730
3501.990800	575421.503262	43.557735
3501.971213	575396.573661	43.562740
3502.176643	575379.685621	43.567745
3501.869036	575351.439798	43.572749
3502.152288	575335.091356	43.577754
3502.130951	575331.984331	43.582759
3501.872168	575309.048428	43.587764
3502.348199	575289.308614	43.592769
3502.137060	575274.040707	43.597773
3501.876797	575254.064767	43.602778
3501.650329	575238.046704	43.607783
3502.103068	575228.243490	43.612788
3502.015718	575211.451135	43.617793
3501.984006	575185.469453	43.622797
3502.256707	575166.664222	43.627802
3502.367449	575157.666921	43.632807
3502.138279	575136.582230	43.637812
3502.465122	575112.450691	43.642817
3502.078121	575096.407355	43.647821
3502.449398	575066.298820	43.652826
3501.485979	575053.104760	43.657831
3501.791605	575045.230764	43.662836
3501.798709	575015.781039	43.667841
3501.733549	575006.961621	43.672845
3501.922507	575003.821630	43.677850
3501.767056	574983.628153	43.682855
3501.835904	574973.784397	43.687860
3501.841525	574960.388570	43.692865
3501.904864	574938.003573	43.697869
3502.257666	574928.265891	43.702874
3502.067162	574904.014111	43.707879
3501.941829	574891.642045	43.712884
3502.088781	574871.300755	43.717889
3501.971122	574852.305183	43.722893
3502.080887	574840.899683	43.727898
3502.121855	574821.377572	43.732903
3501.881445	574807.066817	43.737908
3501.772798	574788.370741	43.742913
3501.660569	574775.093456	43.747917
3502.123129	574757.863276	43.752922
3501.397547	574747.140131	43.757927
3501.713761	574733.795819	43.762932
3501.943178	574716.050160	43.767937
3501.838218	574710.046214	43.772941
3501.710065	574686.737437	43.777946
3502.013809	574682.626193	43.782951
3501.784705	574660.537211	43.787956
3502.032639	574637.169538	43.792961
3501.551735	574641.408769	43.797965
3502.218098	574631.019778	43.802970
3501.684626	574607.774200	43.807975
3501.766033	574592.008108	43.812980
3501.838454	574571.527420	43.817985
3501.630335	574559.820142	43.822989
3502.124748	574545.193500	43.827994
3502.087012	574528.643223	43.832999
3502.184004	574515.734287	43.838004
3502.308461	574494.141580	43.843009
3502.203208	574478.253998	43.848013
3502.271160	574444.027082	43.853018
3502.109448	574432.864292	43.858023
3502.127381	574421.021190	43.863028
3502.067837	574393.988454	43.868033
3501.763340	574388.316555	43.873037
3501.582110	574364.714386	43.878042
3501.754589	574361.376111	43.883047
3501.887533	574348.110167	43.888052
3502.186522	574329.951658	43.893057
3502.233488	574309.775503	43.898061
3502.205079	574292.019314	43.903066
3501.710683	574270.021211	43.908071
3501.624571	574260.351572	43.913076
3501.845319	574236.385266	43.918081
3501.625907	574224.579062	43.923085
3501.978548	574214.288907	43.928090
3501.753369	574200.928261	43.933095
3501.379620	574185.433442	43.938100
3502.045711	574178.204898	43.943105
3501.833947	574164.189879	43.948109
3502.045559	574135.809670	43.953114
3502.047757	574132.748807	43.958119
3501.781759	574113.775182	43.963124
3501.968811	574094.379495	43.968129
3501.944360	574090.520033	43.973133
3501.975281	574063.171332	43.978138
3502.253642	574052.240404	43.983143
3502.017893	574030.351916	43.988148
3501.941820	574007.585493	43.993153
3501.660031	574003.615713	43.998157
3501.744488	573985.239328	44.003162
3502.153755	573980.358747	44.008167
3501.882531	573962.238618	44.013172
3502.234465	573935.040115	44.018177
3501.868392	573924.259980	44.023181
3501.650775	573896.648692	44.028186
3501.716825	573888.911694	44.033191
3501.934397	573887.874189	44.038196
3502.213928	573853.662585	44.043201
3501.858728	573857.782107	44.048205
3502.116036	573830.497799	44.053210
3502.194987	573810.917833	44.058215
3502.373866	573806.123368	44.063220
3502.074458	573771.951849	44.068225
3501.520679	573757.036494	44.073229
3501.735184	573732.468015	44.078234
3501.935614	573720.344782	44.083239
3501.363248	573713.811289	44.088244
3501.804005	573704.410027	44.093249
3501.445818	573687.457050	44.098253
3501.848432	573677.559989	44.103258
3501.762909	573678.928023	44.108263
3501.655674	573655.664024	44.113268
3501.725859	573637.038435	44.118273
3501.870659	573639.323776	44.123277
3501.792915	573620.771461	44.128282
3501.843809	573611.932810	44.133287
3501.448928	573597.694844	44.138292
3501.783056	573579.931037	44.143297
3501.673132	573575.131448	44.148301
3501.659743	573562.238681	44.153306
3501.711304	573555.557384	44.158311
3501.594604	573537.261894	44.163316
3501.830054	573519.663943	44.168321
3501.749788	573518.371918	44.173325
3501.991013	573491.841930	44.178330
3501.937304	573476.697505	44.183335
3501.835464	573474.054127	44.188340
3501.657065	573442.170737	44.193345
3501.798737	573440.241908	44.198349
3501.789277	573418.617912	44.203354
3502.136384	573400.199519	44.208359
3501.901461	573389.749596	44.213364
3501.496964	573365.076389	44.218369
3502.257542	573366.061314	44.223373
3502.024084	573353.553941	44.228378
3501.757961	573334.829904	44.233383
3502.003653	573315.072490	44.238388
3501.911641	573298.880129	44.243393
3501.592159	573282.171371	44.248397
3501.943498	573265.759127	44.253402
3501.918978	573260.293768	44.258407
3502.027016	573239.253171	44.263412
3501.907307	573222.613447	44.268417
3501.771408	573213.051048	44.273421
3501.888947	573183.478939	44.278426
3501.567682	573179.063454	44.283431
3501.629809	573173.935741	44.288436
3501.878161	573144.493609	44.293441
3501.737715	573145.769940	44.298445
3502.169957	573136.821128	44.303450
3501.841192	573122.973638	44.308455
3501.907796	573105.401441	44.313460
3501.933482	573093.756445	44.318465
3501.871049	573074.247487	44.323469
3501.815221	573055.490114	44.328474
3502.096001	573051.933819	44.333479
3501.769900	573035.376262	44.338484
3502.146180	573027.540002	44.343489
3502.127696	573013.493342	44.348493
3502.100731	572984.997020	44.353498
3501.324675	572956.567555	44.358503
3501.606145	572959.483972	44.363508
3502.032699	572935.733632	44.368513
3501.723585	572927.954273	44.373517
3501.587414	572910.212765	44.378522
3501.649252	572897.809256	44.383527
3501.764988	572894.529601	44.388532
3501.755319	572868.087556	44.393537
3501.689981	572868.348625	44.398541
3501.846334	572859.743791	44.403546
3501.610928	572840.662893	44.408551
3501.658691	572824.999958	44.413556
3501.792751	572821.717417	44.418561
3501.606202	572813.115975	44.423565
3501.679720	572785.205577	44.428570
3501.399636	572770.848267	44.433575
3501.228725	572771.978868	44.438580
3501.489201	572763.658752	44.443585
3501.297327	572767.452064	44.448589
3501.423549	572747.561806	44.453594
3501.992711	572738.741813	44.458599
3501.595565	572735.140864	44.463604
3501.933560	572716.622434	44.468609
3502.239065	572695.901208	44.473613
3502.050619	572687.601038	44.478618
3501.690396	572660.761707	44.483623
3501.864640	572659.128726	44.488628
3502.131007	572640.771905	44.493633
3501.784939	572619.650615	44.498637
3501.876030	572604.582746	44.503642
3501.733550	572587.243149	44.508647
3501.652427	572569.341966	44.513652
3502.007650	572558.247051	44.518657
3502.060757	572547.600787	44.523661
3501.780408	572530.282656	44.528666
3501.662611	572528.143341	44.533671
3501.372120	572517.149330	44.538676
3501.927892	572493.227330	44.543681
3501.607038	572488.861688	44.548685
3501.477027	572477.993089	44.553690
3502.022167	572457.886299	44.558695
3501.770514	572452.104803	44.563700
3501.555258	572435.478862	44.568705
3501.887901	572418.064731	44.573709
3501.760920	572391.539558	44.578714
3501.981534	572394.014019	44.583719
3501.696504	572382.567407	44.588724
3502.060354	572355.965420	44.593729
3501.882177	572368.136743	44.598733
3501.475976	572335.533161	44.603738
3501.461604	572321.986801	44.608743
3501.608648	572316.293448	44.613748
3501.707034	572308.449959	44.618753
3501.529844	572296.835862	44.623757
3501.502502	572273.456179	44.628762
3501.611526	572275.747391	44.633767
3501.750108	572261.675247	44.638772
3501.857035	572248.962901	44.643777
3501.703260	572251.596282	44.648781
3501.572296	572226.928016	44.653786
3501.655153	572214.369936	44.658791
3501.720445	572205.527941	44.663796
3501.663070	572195.099341	44.668801
3501.145066	572197.639132	44.673805
3501.116458	572180.281111	44.678810
3501.595767	572160.083727	44.683815
3501.521647	572150.862040	44.688820
3501.718996	572143.153508	44.693825
3501.757372	572139.283561	44.698829
3501.633699	572119.230549	44.703834
3501.932668	572115.068950	44.708839
3501.818426	572111.925384	44.713844
3501.811245	572087.488369	44.718849
3501.693274	572081.334519	44.723853
3501.714904	572067.330599	44.728858
3501.735725	572045.347988	44.733863
3501.583838	572026.754477	44.738868
3501.672351	572026.439521	44.743873
3501.833741	572025.209909	44.748877
3501.584593	572000.459265	44.753882
3501.738723	571981.466572	44.758887
3501.828858	571977.036482	44.763892
3501.676444	571959.496754	44.768897
3501.944028	571946.558230	44.773901
3501.805516	571939.604608	44.778906
3501.774731	571913.514917	44.783911
3501.944869	571905.258479	44.788916
3502.215339	571886.548531	44.793921
3501.804910	571870.253365	44.798925
3501.754772	571857.565137	44.803930
3501.671671	571846.236963	44.808935
3501.779730	571826.899940	44.813940
3501.745797	571810.596013	44.818945
3501.779830	571819.773998	44.823949
3502.100344	571787.356329	44.828954
3502.115729	571777.116700	44.833959
3501.537846	571754.574752	44.838964
3501.925191	571740.312529	44.843969
3501.824387	571729.488831	44.848973
3501.671132	571721.483548	44.853978
3501.797479	571705.706423	44.858983
3501.880981	571709.306487	44.863988
3502.282123	571691.880541	44.868993
3501.952029	571669.349870	44.873997
3501.756500	571658.641279	44.879002
3501.712979	571627.484454	44.884007
3501.817152	571618.535560	44.889012
3501.858036	571602.671287	44.894017
3501.602000	571583.842419	44.899021
3501.480699	571578.240831	44.904026
3501.872882	571567.390094	44.909031
3502.004968	571557.583674	44.914036
3501.861925	571533.517994	44.919041
3501.612352	571532.302392	44.924045
3501.494129	571515.308652	44.929050
3501.294129	571488.240770	44.934055
3501.475671	571492.076495	44.939060
3501.508426	571488.106838	44.944065
3501.636844	571483.018186	44.949069
3501.619262	571460.187328	44.954074
3501.367898	571450.340392	44.959079
3501.600455	571444.633237	44.964084
3501.439019	571441.647414	44.969089
3501.794621	571448.115685	44.974093
3501.469218	571424.931408	44.979098
3501.382957	571415.560470	44.984103
3501.569939	571410.261894	44.989108
3501.494771	571401.391051	44.994113
3501.569940	571387.628846	44.999117
3501.099972	571369.134171	45.004122
3501.580084	571358.670963	45.009127
3501.672563	571361.767893	45.014132
3501.801820	571355.876106	45.019137
3501.410079	571335.361778	45.024141
3501.741655	571327.932820	45.029146
3501.592867	571310.993738	45.034151
3501.770617	571304.090656	45.039156
3501.890027	571278.628429	45.044161
3501.937142	571282.585609	45.049165
3501.636927	571260.501118	45.054170
3502.254552	571252.475363	45.059175
3501.297521	571244.846320	45.064180
3501.596316	571220.961831	45.069185
3501.856891	571205.464141	45.074189
3501.623145	571190.043706	45.079194
3501.828138	571193.223462	45.084199
3501.721807	571172.513668	45.089204
3501.708961	571157.660877	45.094209
3501.741413	571158.659473	45.099213
3501.858158	571140.273445	45.104218
3501.671437	571111.947966	45.109223
3501.520525	571115.835790	45.114228
3502.000257	571103.515556	45.119233
3502.078039	571091.509072	45.124237
3501.568983	571075.278370	45.129242
3501.657757	571063.972734	45.134247
3501.925843	571061.371333	45.139252
3501.843694	571041.159376	45.144257
3501.960101	571026.938621	45.149261
3501.759420	571009.957018	45.154266
3501.964108	570995.421309	45.159271
3501.510538	570979.031238	45.164276
3501.449561	570960.973820	45.169281
3501.647605	570957.981858	45.174285
3501.489086	570947.417369	45.179290
3501.444991	570924.388841	45.184295
3501.291560	570921.100513	45.189300
3501.847073	570915.141863	45.194305
3501.605431	570909.408200	45.199309
3501.552066	570904.046591	45.204314
3501.876917	570887.384140	45.209319
3501.625662	570878.189113	45.214324
3501.730344	570877.821413	45.219329
3501.869198	570849.243640	45.224333
3501.462182	570830.487315	45.229338
3501.958428	570830.510079	45.234343
3501.661266	570812.790468	45.239348
3501.850109	570795.045040	45.244353
3501.691917	570795.170111	45.249357
3501.494232	570784.410848	45.254362
3502.202521	570759.959514	45.259367
3501.837646	570750.280279	45.264372
3501.724038	570732.782783	45.269377
3501.607310	570716.289488	45.274381
3501.499847	570706.569974	45.279386
3501.904688	570705.302165	45.284391
3501.975421	570687.324099	45.289396
3501.937653	570669.965212	45.294401
3501.711200	570666.136166	45.299405
3501.706177	570630.403565	45.304410
3501.358192	570632.314865	45.309415
3501.650718	570634.929033	45.314420
3501.961417	570615.156782	45.319425
3501.998058	570600.797405	45.324429
3501.747364	570584.375050	45.329434
3501.653577	570563.009752	45.334439
3501.618660	570550.418066	45.339444
3501.486138	570553.299452	45.344449
3501.498045	570550.888548	45.349453
3501.341388	570527.876817	45.354458
3501.526261	570504.109018	45.359463
3501.530991	570504.710502	45.364468
3501.661859	570493.849414	45.369473
3501.329670	570499.070673	45.374477
3501.425801	570475.668004	45.379482
3501.823850	570454.827872	45.384487
3501.429309	570452.129170	45.389492
3501.846682	570449.353730	45.394497
3501.869684	570431.734041	45.399501
3501.615061	570419.678440	45.404506
3501.814779	570408.103872	45.409511
3501.840484	570402.528913	45.414516
3501.642886	570388.105511	45.419521
3501.492688	570387.075002	45.424525
3501.296211	570380.882316	45.429530
3501.258827	570356.647072	45.434535
3501.682041	570343.933351	45.439540
3501.887946	570334.816984	45.444545
3501.463427	570331.871997	45.449549
3501.523527	570317.709351	45.454554
3501.841242	570298.738478	45.459559
3501.362853	570297.960022	45.464564
3501.395328	570291.932252	45.469569
3501.618228	570281.106764	45.474573
3501.207951	570257.531871	45.479578
3501.476332	570256.084591	45.484583
3501.396570	570260.764606	45.489588
3501.505573	570250.007083	45.494593
3501.445024	570253.780694	45.499597
3501.420455	570237.071545	45.504602
3501.811374	570212.166770	45.509607
3501.652234	570212.442562	45.514612
3501.733749	570206.055756	45.519617
3501.993932	570180.870215	45.524621
3501.745526	570173.832316	45.529626
3501.851765	570165.986130	45.534631
3501.811493	570151.889161	45.539636
3501.346948	570133.893526	45.544641
3501.217793	570132.658946	45.549645
3501.214903	570126.686807	45.554650
3501.432942	570108.132718	45.559655
3501.088055	570093.380641	45.564660
3501.306077	570080.096430	45.569665
3501.949966	570075.378278	45.574669
3501.492310	570081.121238	45.579674
3501.753960	570060.853802	45.584679
3501.700954	570048.665911	45.589684
3501.578251	570041.507899	45.594689
3501.856395	570031.878100	45.599693
3501.472611	570018.135806	45.604698
3501.538509	570003.720917	45.609703
3501.209235	570005.729774	45.614708
3501.225438	569997.345457	45.619713
3501.384177	570002.289434	45.624717
3501.186640	569988.618369	45.629722
3501.613653	569957.835146	45.634727
3501.413425	569962.634495	45.639732
3501.287623	569953.820633	45.644737
3500.845793	569954.090434	45.649741
3501.164209	569956.399570	45.654746
3501.199977	569953.382526	45.659751
3501.229205	569952.976402	45.664756
3501.276966	569946.042634	45.669761
3501.595634	569925.163760	45.674765
3501.191917	569912.026741	45.679770
3501.286983	569905.587459	45.684775
3501.419835	569909.079996	45.689780
3501.241051	569901.529140	45.694785
3501.591518	569903.431752	45.699789
3501.268828	569874.823319	45.704794
3501.252664	569868.351214	45.709799
3501.098366	569874.649141	45.714804
3501.158216	569860.987877	45.719809
3501.194075	569868.259896	45.724813
3501.407921	569862.454500	45.729818
3501.426234	569856.830240	45.734823
3501.601239	569831.858013	45.739828
3501.248199	569772.336448	45.744833
3501.153782	569663.235129	45.749837
3500.807707	569522.601246	45.754842
3500.781489	569327.707237	45.759847
3500.214765	569087.418625	45.764852
3500.321552	568797.527143	45.769857
3499.578134	568463.035958	45.774861
3498.903254	568078.727503	45.779866
3498.410241	567653.514762	45.784871
3498.120294	567185.130816	45.789876
3497.138457	566669.643777	45.794881
3496.398555	566116.139488	45.799885
3494.915916	565510.808209	45.804890
3494.302506	564874.479109	45.809895
3493.350013	564206.130924	45.814900
3492.251653	563477.053326	45.819905
3490.666772	562715.964924	45.824909
3489.364148	561936.551290	45.829914
3488.432082	561103.534696	45.834919
3486.730531	560226.023509	45.839924
3485.746772	559320.202693	45.844929
3484.065217	558373.978442	45.849933
3482.188568	557399.220857	45.854938
3480.312024	556370.215645	45.859943
3478.752965	555337.906314	45.864948
3476.707650	554249.597466	45.869953
3474.950565	553135.360732	45.874957
3473.047942	551994.704196	45.879962
3471.070834	550829.469738	45.884967
3469.054451	549629.439066	45.889972
3467.020358	548397.716479	45.894977
3464.812656	547139.044262	45.899981
3462.691011	545860.113223	45.904986
3460.034907	544543.209392	45.909991
3457.927057	543219.390040	45.914996
3455.638348	541846.508757	45.920001
3452.954657	540460.306409	45.925005
3450.009445	539060.808750	45.930010
3447.679107	537631.016211	45.935015
3445.312985	536178.671380	45.940020
3442.138613	534710.985598	45.945025
3439.583599	533237.145236	45.950029
3436.879349	531735.669917	45.955034
3433.889292	530214.578577	45.960039
3430.972666	528681.060942	45.965044
3428.041051	527130.544154	45.970049
3425.807166	525567.898596	45.975053
3422.401726	523985.856607	45.980058
3419.747653	522403.005564	45.985063
3416.621109	520782.349987	45.990068
3413.754772	519162.920416	45.995073
3410.505750	517514.527415	46.000077
3407.564671	515861.703222	46.005082
3404.143115	514193.277955	46.010087
3400.988197	512522.794247	46.015092
3397.496404	510844.295814	46.020097
3394.697259	509150.559522	46.025101
3391.073355	507451.452164	46.030106
3387.970679	505743.332408	46.035111
3384.454245	504031.036437	46.040116
3381.081490	502302.720527	46.045121
3377.664410	500576.021152	46.050125
3374.086965	498848.485436	46.055130
3370.985617	497099.219397	46.060135
3367.398543	495355.525674	46.065140
3363.974009	493594.688294	46.070145
3360.315545	491831.962867	46.075149
3356.674607	490058.776608	46.080154
3353.303009	488288.471593	46.085159
3349.678566	486522.748274	46.090164
3346.199337	484742.250332	46.095169
3342.774221	482958.305275	46.100173
3338.818542	481193.944347	46.105178
3335.255565	479397.537885	46.110183
3331.454106	477619.764746	46.115188
3327.961879	475842.603703	46.120193
3324.351766	474050.351555	46.125197
3320.614054	472264.189180	46.130202
3317.121217	470466.112558	46.135207
3313.362019	468679.712832	46.140212
3309.438515	466887.430729	46.145217
3306.212430	465086.298748	46.150221
3302.471583	463305.590448	46.155226
3299.156196	461502.975968	46.160231
3295.445326	459698.411033	46.165236
3291.418505	457906.304860	46.170241
3287.634978	456111.495284	46.175245
3283.402570	454311.813767	46.180250
3279.895170	452506.317540	46.185255
3276.424040	450725.182257	46.190260
3272.441665	448924.509318	46.195265
3268.891870	447134.625990	46.200269
3265.293977	445359.207204	46.205274
3261.569509	443556.543749	46.210279
3257.356998	441756.008947	46.215284
3253.536732	439985.020623	46.220289
3249.697204	438197.861513	46.225293
3245.747042	436409.993800	46.230298
3242.194158	434634.562578	46.235303
3238.213586	432859.997342	46.240308
3234.431179	431092.688035	46.245313
3231.091187	429310.200387	46.250317
3226.977332	427547.540527	46.255322
3223.402242	425779.977598	46.260327
3219.688935	424014.612941	46.265332
3215.944574	422246.210157	46.270337
3212.141348	420486.840739	46.275341
3208.122292	418726.392142	46.280346
3204.470595	416964.013667	46.285351
3200.468945	415210.975124	46.290356
3196.817337	413454.897336	46.295361
3193.359990	411713.760423	46.300365
3189.493033	409961.946341	46.305370
3185.620236	408196.752836	46.310375
3181.811861	406457.079173	46.315380
3177.827791	404708.418541	46.320385
3174.373980	402971.564950	46.325389
3170.015057	401238.830758	46.330394
3166.519121	399502.989217	46.335399
3162.460825	397781.671790	46.340404
3158.486496	396056.357582	46.345409
3155.294834	394334.297878	46.350413
3151.550539	392621.287417	46.355418
3147.184522	390903.176314	46.360423
3143.399994	389184.828239	46.365428
3139.581708	387486.294664	46.370433
3136.080326	385773.251577	46.375437
3131.954003	384079.918239	46.380442
3128.499896	382374.560253	46.385447
3124.567084	380665.533181	46.390452
3121.054378	378981.952281	46.395457
3117.007922	377294.258554	46.400461
3113.077379	375618.732794	46.405466
3109.462041	373931.141136	46.410471
3105.511407	372250.051177	46.415476
3101.690790	370577.272359	46.420481
3098.178069	368912.220644	46.425485
3094.129339	367241.616135	46.430490
3090.904364	365567.278985	46.435495
3087.098327	363914.838390	46.440500
3083.122443	362252.344847	46.445505
3079.628025	360577.688417	46.450509
3075.518456	358931.395932	46.455514
3071.888857	357274.163433	46.460519
3068.138098	355623.545049	46.465524
3064.340931	353979.760021	46.470529
3060.618626	352326.574503	46.475533
3056.794591	350691.647203	46.480538
3053.012953	349043.488050	46.485543
3049.142057	347413.894790	46.490548
3045.275893	345783.737957	46.495553
3041.790216	344156.926068	46.500557
3037.736321	342537.092406	46.505562
3034.214598	340917.455843	46.510567
3030.198133	339297.135488	46.515572
3026.689760	337690.317748	46.520577
3022.782293	336079.523879	46.525581
3018.864293	334478.681101	46.530586
3015.068938	332872.918108	46.535591
3011.873171	331268.112255	46.540596
3007.988913	329673.444673	46.545601
3004.365245	328079.866589	46.550605
3000.228546	326484.066119	46.555610
2996.546938	324888.410966	46.560615
2993.390290	323312.326641	46.565620
2989.376131	321725.224759	46.570625
2985.574092	320147.366834	46.575629
2981.943988	318576.445945	46.580634
2978.650869	316983.356934	46.585639
2974.613826	315418.442330	46.590644
2970.678409	313847.096477	46.595649
2967.223031	312275.418278	46.600653
2963.478416	310709.966858	46.605658
2959.663980	309136.459114	46.610663
2955.989650	307590.871129	46.615668
2952.011630	306039.581848	46.620673
2948.581816	304465.483660	46.625677
2944.547273	302927.596602	46.630682
2941.063271	301372.628027	46.635687
2937.672996	299826.075023	46.640692
2933.946681	298282.025124	46.645697
2930.272322	296732.528311	46.650701
2926.594925	295191.898667	46.655706
2923.164317	293646.658796	46.660711
2919.364976	292109.353038	46.665716
2915.487689	290572.453436	46.670721
2912.058714	289038.373333	46.675725
2908.114605	287501.562142	46.680730
2904.457523	285977.907891	46.685735
2901.249787	284445.365726	46.690740
2897.124299	282924.898532	46.695745
2893.946575	281389.178552	46.700749
2890.347750	279871.441038	46.705754
2886.586113	278336.894350	46.710759
2882.843470	276807.151549	46.715764
2878.993962	275282.640857	46.720769
2874.996665	273754.789251	46.725773
2871.514462	272254.252023	46.730778
2868.114669	270731.650800	46.735783
2864.472892	269225.408782	46.740788
2860.592696	267704.079753	46.745793
2857.107489	266197.179195	46.750797
2853.156055	264694.377523	46.755802
2849.851650	263195.705363	46.760807
2845.937993	261701.181935	46.765812
2842.269734	260199.418937	46.770817
2839.041437	258709.842161	46.775821
2834.957389	257213.276004	46.780826
2831.558393	255713.350916	46.785831
2827.717243	254220.786997	46.790836
2824.247165	252738.183050	46.795841
2820.669200	251242.032711	46.800845
2816.826319	249764.780663	46.805850
2812.980013	248274.578555	46.810855
2809.272203	246785.717452	46.815860
2805.809149	245321.204458	46.820865
2802.373875	243839.536574	46.825869
2798.329303	242362.436314	46.830874
2794.836006	240891.123802	46.835879
2791.011662	239425.024797	46.840884
2787.310300	237959.102780	46.845889
2783.820502	236487.385005	46.850893
2779.898832	235034.855779	46.855898
2776.433442	233576.366768	46.860903
2772.782158	232122.232140	46.865908
2769.193910	230669.943261	46.870913
2765.735635	229211.620499	46.875917
2761.891052	227766.599922	46.880922
2758.236480	226312.786915	46.885927
2754.365899	224867.131700	46.890932
2750.737614	223420.190731	46.895937
2747.332869	221974.692870	46.900941
2743.640417	220546.076614	46.905946
2740.201248	219105.452617	46.910951
2736.399555	217666.289156	46.915956
2732.501918	216235.880276	46.920961
2729.291571	214792.506637	46.925965
2725.915422	213375.931717	46.930970
2721.967154	211930.901825	46.935975
2718.493871	210493.470363	46.940980
2714.693337	209068.704261	46.945985
2711.410360	207636.708637	46.950989
2707.573647	206212.550641	46.955994
2704.046374	204786.469008	46.960999
2700.246807	203370.041356	46.966004
2696.588700	201954.926553	46.971009
2693.041953	200535.297987	46.976013
2689.423714	199113.757230	46.981018
2685.540133	197696.702036	46.986023
2682.261098	196289.370348	46.991028
2678.903006	194873.533807	46.996033
2675.041137	193461.356122	47.001037
2671.308016	192051.567516	47.006042
2667.802630	190638.117820	47.011047
2663.985308	189223.384117	47.016052
2660.411880	187835.189559	47.021057
2656.617904	186427.974235	47.026061
2652.946909	185038.990688	47.031066
2649.472760	183635.124467	47.036071
2645.701450	182235.220620	47.041076
2642.223152	180853.879466	47.046081
2638.533761	179454.615421	47.051085
2635.084956	178074.534100	47.056090
2631.493942	176679.449049	47.061095
2627.751348	175294.200661	47.066100
2624.103114	173908.833610	47.071105
2620.796329	172523.220793	47.076109
2617.127453	171144.741743	47.081114
2613.278955	169762.751561	47.086119
2610.061257	168386.111370	47.091124
2606.197342	167010.998793	47.096129
2602.594807	165622.952278	47.101133
2598.829846	164260.404028	47.106138
2595.148143	162886.923907	47.111143
2591.633592	161519.632307	47.116148
2588.211817	160154.468149	47.121153
2584.757931	158780.760204	47.126157
2581.172029	157422.096434	47.131162
2577.101625	156054.273719	47.136167
2573.677180	154681.214533	47.141172
2569.968065	153322.969688	47.146177
2566.178814	151953.303520	47.151181
2562.649633	150607.058644	47.156186
2559.062837	149245.139786	47.161191
2555.718824	147900.383783	47.166196
2551.976556	146551.156039	47.171201
2548.574640	145155.007305	47.176205
2544.842432	143763.440076	47.181210
2540.987619	142421.553738	47.186215
2537.606638	141077.326819	47.191220
2534.015221	139730.167363	47.196225
2530.675159	138382.955681	47.201229
2526.745567	137040.327655	47.206234
2523.277694	135692.183116	47.211239
2519.818547	134364.495382	47.216244
2515.861139	133027.282046	47.221249
2512.511909	131688.360234	47.226253
2508.489572	130359.455921	47.231258
2504.983693	129026.543175	47.236263
2501.469176	127692.846865	47.241268
2498.186492	126375.920881	47.246273
2494.556768	125035.205033	47.251277
2490.470561	123717.396287	47.256282
2486.837762	122398.809453	47.261287
2483.225995	121081.712961	47.266292
2479.607793	119771.147548	47.271297
2476.086851	118448.428622	47.276301
2472.213670	117146.258503	47.281306
2468.639992	115836.520495	47.286311
2465.251499	114528.757713	47.291316
2461.796552	113239.539391	47.296321
2458.131368	111928.517828	47.301325
2454.363972	110630.375832	47.306330
2451.148232	109331.673652	47.311335
2447.038149	108025.277159	47.316340
2443.444483	106738.032408	47.321345
2439.989296	105436.830737	47.326349
2436.100702	104146.462612	47.331354
2432.575167	102859.646319	47.336359
2429.400500	101580.336919	47.341364
2425.290295	100293.533835	47.346369
2421.629794	98996.123982	47.351373
2418.334593	97731.969205	47.356378
2414.439288	96456.101085	47.361383
2411.093906	95165.558560	47.366388
2407.458489	93909.285571	47.371393
2403.681386	92642.119359	47.376397
2399.811105	91367.662874	47.381402
2396.517117	90092.915532	47.386407
2392.508615	88831.191948	47.391412
2388.578735	87578.491885	47.396417
2385.182388	86320.768580	47.401421
2381.823241	85077.677589	47.406426
2378.262842	83811.474902	47.411431
2375.080162	82566.939904	47.416436
2370.955545	81320.028015	47.421441
2367.279060	80075.361951	47.426445
2363.613416	78830.863799	47.431450
2360.052370	77596.705226	47.436455
2356.616260	76343.900692	47.441460
2352.339214	75121.027269	47.446465
2348.985085	73881.035526	47.451469
2345.195477	72660.775297	47.456474
2341.596712	71438.306325	47.461479
2338.215766	70217.739011	47.466484
2334.494579	68995.529643	47.471489
2331.123005	67783.403588	47.476493
2327.115255	66567.707929	47.481498
2323.521332	65352.424197	47.486503
2319.922359	64142.638824	47.491508
2316.249307	62937.714898	47.496513
2312.783368	61736.979872	47.501517
2309.029466	60551.064650	47.506522
2305.345193	59345.688518	47.511527
2301.696404	58151.426453	47.516532
2297.672939	56960.841388	47.521537
2294.557151	55776.118274	47.526541
2290.760681	54600.366541	47.531546
2286.930818	53411.412330	47.536551
2283.565378	52229.817008	47.541556
2279.655031	51064.377794	47.546561
2276.163124	49890.336280	47.551565
2272.482984	48728.061253	47.556570
2268.812046	47562.285369	47.561575
2265.333217	46400.699573	47.566580
2261.545626	45245.849018	47.571585
2257.939223	44094.060680	47.576589
2254.014980	42941.201880	47.581594
2250.286214	41795.753265	47.586599
2246.756329	40646.978718	47.591604
2242.860422	39514.679734	47.596609
2239.222124	38376.839028	47.601613
2235.345039	37257.949727	47.606618
2231.548095	36140.120316	47.611623
2228.098732	35007.886231	47.616628
2224.321018	33900.459390	47.621633
2220.521370	32786.394289	47.626637
2216.911685	31693.711385	47.631642
2213.148413	30592.579050	47.636647
2209.371857	29505.195879	47.641652
2205.479662	28422.723187	47.646657
2201.900851	27341.304045	47.651661
2197.539134	26260.045611	47.656666
2193.758082	25189.309724	47.661671
2189.968051	24122.845222	47.666676
2186.064446	23088.803533	47.671681
2182.433138	22034.411856	47.676685
2178.392658	20998.162368	47.681690
2174.122569	19981.310313	47.686695
2170.315939	18957.179446	47.691700
2166.256499	17955.107091	47.696705
2161.859445	16956.350137	47.701709
2157.807690	15990.848855	47.706714
2152.855186	15034.253893	47.711719
2148.450876	14108.722766	47.716724
2142.860588	13218.372464	47.721729
2137.144962	12346.088173	47.726733
2131.913294	11522.043682	47.731738
2126.666631	10723.530686	47.736743
2121.591382	9959.605184	47.741748
2115.644327	9221.597934	47.746753
2110.034131	8539.330273	47.751757
2103.999607	7908.591597	47.756762
2098.054926	7315.442652	47.761767
2092.688242	6751.966961	47.766772
2086.831186	6236.213913	47.771777
2081.908391	5753.518686	47.776781
2076.435516	5310.696790	47.781786
2071.573934	4906.522469	47.786791
2067.433582	4520.576854	47.791796
2062.805909	4172.775719	47.796801
2058.812697	3833.565338	47.801805
2054.732631	3524.095294	47.806810
2050.596183	3215.895618	47.811815
2047.150779	2939.334525	47.816820
2043.452939	2674.806665	47.821825
2039.911634	2422.810762	47.826829
2036.904006	2183.391701	47.831834
2033.391415	1940.852699	47.836839
2030.009912	1701.118853	47.841844
2026.587596	1476.050620	47.846849
2023.095283	1240.061232	47.851853
2020.182589	1025.505798	47.856858
2016.462248	812.623323	47.861863
2013.215777	594.641755	47.866868
2009.567844	394.285258	47.871873
2006.016403	187.148425	47.876877
1998.877794	86.573042	47.881882
1986.808543	145.616369	47.886887
1980.106451	154.182359	47.891892
1975.720644	149.224297	47.896897
1973.316599	143.158849	47.901901
1971.692491	134.819947	47.906906
1969.249925	146.617279	47.911911
1967.167656	139.621934	47.916916
1964.349122	148.510411	47.921921
1961.440289	142.954238	47.926925
1958.314160	141.611510	47.931930
1955.181790	140.298235	47.936935
1952.134874	130.831016	47.941940
1948.500418	143.643782	47.946945
1945.529643	141.286465	47.951949
1942.103496	140.882894	47.956954
1938.386268	143.093915	47.961959
1934.824144	140.193202	47.966964
1931.663971	138.953889	47.971969
1928.858803	137.203432	47.976973
1925.544343	141.496519	47.981978
1921.851052	140.973401	47.986983
1918.066400	141.635204	47.991988
1915.179422	144.263658	47.996993
1911.769509	143.095070	48.001997
1908.790651	135.888855	48.007002
1904.668711	145.528648	48.012007
1901.650980	131.497779	48.017012
1897.692784	148.252748	48.022017
1894.403661	138.323560	48.027021
1890.977332	141.257889	48.032026
1887.963104	138.780836	48.037031
1884.569133	141.216544	48.042036
1881.246186	137.072999	48.047041
1878.210094	144.442088	48.052045
1874.515584	144.137483	48.057050
1870.730864	142.325187	48.062055
1867.625619	134.790742	48.067060
1863.753073	138.937054	48.072065
1860.618630	133.359272	48.077069
1857.454360	133.911359	48.082074
1853.190579	142.570425	48.087079
1850.048414	137.190012	48.092084
1846.995258	146.732176	48.097089
1843.505501	135.821977	48.102093
1840.304051	137.746666	48.107098
1836.252054	144.237003	48.112103
1832.678397	138.917793	48.117108
1829.100549	142.537095	48.122113
1825.491291	141.219392	48.127117
1822.506763	139.171157	48.132122
1819.062089	141.380695	48.137127
1815.982302	137.648387	48.142132
1812.158792	137.291223	48.147137
1808.798165	127.813039	48.152141
1805.330095	131.443642	48.157146
1801.681433	131.944995	48.162151
1798.138305	126.412211	48.167156
1794.845262	130.926613	48.172161
1791.280030	134.388923	48.177165
1788.146097	131.702838	48.182170
1784.517206	136.491270	48.187175
1780.795771	130.682667	48.192180
1777.197799	135.700387	48.197185
1773.703863	131.602624	48.202189
1770.422807	128.477649	48.207194
1766.513964	138.808651	48.212199
1763.825618	128.722225	48.217204
1760.363790	126.555712	48.222209
1756.656792	129.907337	48.227213
1753.498235	130.404775	48.232218
1749.393593	136.219988	48.237223
1746.017262	126.472198	48.242228
1742.610336	130.919012	48.247233
1739.155707	134.076120	48.252237
1735.568862	132.542965	48.257242
1732.114161	141.265281	48.262247
1728.884212	126.695044	48.267252
1725.148575	127.086646	48.272257
1721.501801	123.171015	48.277261
1718.304500	128.765141	48.282266
1714.646278	131.998412	48.287271
1711.358574	129.345910	48.292276
1707.602637	126.462960	48.297281
1704.336196	128.606672	48.302285
1701.298980	127.392483	48.307290
1697.264839	126.055899	48.312295
1694.130399	129.817824	48.317300
1690.321915	136.301735	48.322305
1686.934653	130.469345	48.327309
1683.649143	131.654243	48.332314
1679.628618	126.670795	48.337319
1676.432336	130.224098	48.342324
1673.035275	126.297879	48.347329
1669.549025	127.621768	48.352333
1666.246691	120.668755	48.357338
1662.452781	133.158515	48.362343
1659.078457	123.530674	48.367348
1654.995849	131.784950	48.372353
1651.720951	117.943144	48.377357
1648.305708	121.821796	48.382362
1644.435229	126.550001	48.387367
1641.612317	118.791120	48.392372
1637.879350	127.791128	48.397377
1634.655862	123.980130	48.402381
1631.066496	123.769891	48.407386
1627.387900	126.778583	48.412391
1624.013691	124.547784	48.417396
1620.660148	125.581993	48.422401
1617.202220	126.882483	48.427405
1613.654721	118.696002	48.432410
1610.109258	119.086355	48.437415
1606.399580	114.174518	48.442420
1603.065018	116.259317	48.447425
1599.466252	110.466399	48.452429
1595.815355	121.392999	48.457434
1592.213211	115.698689	48.462439
1589.133511	113.788815	48.467444
1585.456588	120.128772	48.472449
1582.391590	115.359658	48.477453
1578.607284	116.470792	48.482458
1575.124703	124.007904	48.487463
1571.894015	113.243955	48.492468
1568.213422	124.083461	48.497473
1564.742956	120.697131	48.502477
1561.198973	111.605269	48.507482
1557.180819	122.630492	48.512487
1554.225801	115.499774	48.517492
1550.845198	122.840592	48.522497
1546.781113	119.053624	48.527501
1543.666468	117.152396	48.532506
1539.909549	127.950074	48.537511
1536.853805	115.095937	48.542516
1533.463110	114.696446	48.547521
1530.203093	124.612737	48.552525
1526.447905	119.056305	48.557530
1522.312081	120.700217	48.562535
1518.819235	118.725313	48.567540
1515.511613	123.729303	48.572545
1511.917969	121.982154	48.577549
1508.523466	126.569464	48.582554
1505.004704	123.367890	48.587559
1502.128009	122.106491	48.592564
1498.147862	123.741866	48.597569
1494.562154	121.408173	48.602573
1490.993129	117.774701	48.607578
1487.639161	130.901178	48.612583
1484.041058	116.603824	48.617588
1480.534143	116.877454	48.622593
1477.271610	115.809337	48.627597
1474.115822	115.433210	48.632602
1470.172871	120.590441	48.637607
1466.663831	118.684531	48.642612
1463.188851	119.127180	48.647617
1459.270165	122.787291	48.652621
1456.196631	116.415495	48.657626
1452.906599	114.152599	48.662631
1448.709396	118.093595	48.667636
1445.589612	122.112727	48.672641
1442.285810	118.383973	48.677645
1438.954173	118.215721	48.682650
1435.125268	114.559673	48.687655
1432.261166	106.902232	48.692660
1428.681670	109.123503	48.697665
1424.557477	122.949531	48.702669
1421.287980	112.565051	48.707674
1417.397834	113.822528	48.712679
1414.062885	101.239953	48.717684
1410.851501	108.294882	48.722689
1407.300119	111.989266	48.727693
1403.693611	112.155123	48.732698
1399.985385	123.451427	48.737703
1396.555484	110.643265	48.742708
1392.941121	119.131218	48.747713
1389.358802	119.745721	48.752717
1386.423199	112.710104	48.757722
1382.818830	122.275362	48.762727
1379.396307	113.408179	48.767732
1375.543654	124.103824	48.772737
1371.986864	124.312531	48.777741
1368.639671	109.665908	48.782746
1365.377031	122.733817	48.787751
1361.810450	113.114054	48.792756
1358.342557	125.378846	48.797761
1354.428490	109.583909	48.802765
1351.255842	107.036914	48.807770
1347.443608	119.482160	48.812775
1344.275734	111.486313	48.817780
1341.111158	109.070938	48.822785
1337.269898	107.482843	48.827789
1333.787445	104.414863	48.832794
1329.716990	113.363378	48.837799
1326.456277	109.156514	48.842804
1323.331391	113.312521	48.847809
1319.598947	116.877086	48.852813
1316.167388	120.875455	48.857818
1312.682894	113.555620	48.862823
1309.090826	110.612377	48.867828
1305.942979	115.509154	48.872833
1301.990713	103.092867	48.877837
1298.689649	113.202298	48.882842
1295.151342	110.611321	48.887847
1291.876616	111.389684	48.892852
1288.302771	121.032448	48.897857
1284.833448	112.786414	48.902861
1281.343895	113.639540	48.907866
1277.434190	111.059251	48.912871
1274.013259	113.334849	48.917876
1270.822684	110.344588	48.922881
1267.389598	112.574633	48.927885
1264.072322	112.685772	48.932890
1260.052327	102.836478	48.937895
1256.476810	111.767648	48.942900
1252.814021	113.856483	48.947905
1249.490877	105.916621	48.952909
1246.231813	106.161025	48.957914
1242.466642	123.689523	48.962919
1239.231702	109.971370	48.967924
1235.544532	111.867871	48.972929
1232.080847	108.806481	48.977933
1228.661422	110.892028	48.982938
1225.235069	114.016395	48.987943
1221.488727	114.065001	48.992948
1217.981813	116.037696	48.997953
1214.460318	114.105355	49.002957
1211.201855	106.516058	49.007962
1207.559439	113.891626	49.012967
1204.048579	114.327327	49.017972
1200.430990	111.100214	49.022977
1196.885147	111.060493	49.027981
1193.778978	102.026808	49.032986
1190.380757	111.702213	49.037991
1186.763638	103.283206	49.042996
1183.518194	111.061715	49.048001
1179.905123	109.877731	49.053005
1176.304129	102.769190	49.058010
1172.620957	110.597247	49.063015
1169.034433	108.855442	49.068020
1165.447147	110.489553	49.073025
1161.771177	111.634502	49.078029
1158.568827	112.028247	49.083034
1154.658884	109.925785	49.088039
1151.500124	112.568511	49.093044
1148.126397	113.027055	49.098049
1144.573217	114.412220	49.103053
1141.520991	112.431751	49.108058
1137.459113	118.828953	49.113063
1133.755940	112.489412	49.118068
1130.675912	110.854991	49.123073
1126.818692	112.967983	49.128077
1123.639271	106.097189	49.133082
1119.978478	109.002023	49.138087
1116.774910	101.094118	49.143092
1113.232887	104.967470	49.148097
1109.511040	113.602049	49.153101
1105.982235	112.835179	49.158106
1102.747982	114.613361	49.163111
1099.118363	112.796071	49.168116
1095.580039	106.876839	49.173121
1091.986560	108.429686	49.178125
1088.933635	118.914783	49.183130
1084.683487	121.000723	49.188135
1081.115119	110.198101	49.193140
1077.926182	118.635359	49.198145
1074.674265	107.963533	49.203149
1071.165798	102.634435	49.208154
1067.623804	104.176066	49.213159
1064.129016	100.594420	49.218164
1060.798800	105.257219	49.223169
1057.080848	107.174423	49.228173
1053.408832	107.809419	49.233178
1050.392309	118.589388	49.238183
1046.508435	112.047219	49.243188
1042.822112	96.890698	49.248193
1039.297945	109.430129	49.253197
1036.248714	97.758465	49.258202
1032.438407	101.395433	49.263207
1028.898477	97.159632	49.268212
1025.680123	108.806447	49.273217
1022.097885	104.586763	49.278221
1018.857024	92.562292	49.283226
1014.732364	101.570016	49.288231
1011.312440	99.530101	49.293236
1008.186480	101.354634	49.298241
1004.813927	103.837885	49.303245
1001.176149	102.929927	49.308250
997.370280	96.869128	49.313255
993.830678	102.257607	49.318260
990.317647	96.824852	49.323265
986.754863	100.169976	49.328269
983.277061	95.573284	49.333274
980.083553	113.240120	49.338279
976.429336	99.176448	49.343284
973.046528	105.154163	49.348289
969.358466	108.234167	49.353293
965.823025	108.442843	49.358298
962.526097	112.214595	49.363303
959.084210	109.817463	49.368308
955.327693	106.099666	49.373313
951.505544	112.386630	49.378317
948.456792	96.836094	49.383322
945.064658	101.745909	49.388327
941.578197	106.876144	49.393332
938.000493	107.787488	49.398337
934.507081	111.567867	49.403341
931.024515	93.778848	49.408346
927.439264	108.871576	49.413351
923.828228	100.764954	49.418356
920.852213	102.429992	49.423361
916.939818	109.746682	49.428365
913.398580	102.309355	49.433370
910.100347	108.267520	49.438375
906.433937	106.085902	49.443380
903.180173	95.642242	49.448385
899.381445	109.158025	49.453389
895.863369	107.234764	49.458394
891.922549	109.974716	49.463399
888.731674	114.096888	49.468404
885.595733	111.737300	49.473409
881.536403	98.426822	49.478413
878.363416	105.833391	49.483418
874.857471	104.490381	49.488423
871.385575	102.303630	49.493428
867.697348	112.046680	49.498433
864.331013	109.409960	49.503437
861.201351	106.017997	49.508442
857.597964	107.388980	49.513447
853.988142	98.522886	49.518452
850.565840	105.016197	49.523457
846.316797	112.850707	49.528461
843.348030	102.761082	49.533466
839.898098	107.224394	49.538471
836.047383	101.056793	49.543476
832.755339	107.086779	49.548481
829.302403	107.598968	49.553485
826.165576	104.151192	49.558490
822.282592	112.285900	49.563495
819.029332	107.888232	49.568500
815.512432	105.161211	49.573505
811.566897	108.892206	49.578509
808.255492	98.960657	49.583514
805.010239	105.249084	49.588519
801.375291	109.829968	49.593524
797.714206	106.378874	49.598529
794.150820	108.335249	49.603533
791.262613	108.382526	49.608538
787.296607	112.509048	49.613543
783.681287	104.289262	49.618548
780.640086	114.696661	49.623553
776.813220	113.666537	49.628557
773.210320	110.668257	49.633562
769.246283	112.222302	49.638567
766.122998	111.113644	49.643572
763.092167	108.414932	49.648577
759.412068	106.985340	49.653581
756.018970	102.191974	49.658586
752.132121	114.775625	49.663591
748.658149	107.049420	49.668596
745.460746	111.185312	49.673601
741.832955	103.631898	49.678605
738.450211	101.522989	49.683610
734.854867	102.867448	49.688615
731.612012	102.672884	49.693620
727.718931	103.950074	49.698625
723.841267	108.084933	49.703629
720.900337	102.749363	49.708634
717.107787	97.528179	49.713639
713.724344	97.232249	49.718644
710.485382	103.918358	49.723649
706.388540	111.093162	49.728653
703.230755	106.582510	49.733658
699.373846	99.833802	49.738663
696.158611	102.099529	49.743668
692.893237	104.999541	49.748673
688.873390	111.754164	49.753677
685.553985	102.580071	49.758682
682.630532	109.643892	49.763687
679.065043	101.887759	49.768692
675.360729	100.424029	49.773697
671.593620	101.738463	49.778701
667.806388	96.586073	49.783706
664.317768	105.427877	49.788711
661.108707	102.504011	49.793716
658.019442	105.113859	49.798721
653.972856	102.931773	49.803725
651.275991	101.145760	49.808730
647.262666	97.408205	49.813735
643.768341	101.407127	49.818740
640.135179	93.930537	49.823745
636.554184	102.388176	49.828749
633.439681	92.416381	49.833754
629.747702	97.436532	49.838759
626.048384	96.212489	49.843764
623.181855	98.423628	49.848769
618.969340	100.744324	49.853773
615.600169	94.605818	49.858778
611.741315	107.852686	49.863783
608.619131	108.012595	49.868788
605.418179	108.517041	49.873793
601.378786	104.204613	49.878797
598.379560	101.576942	49.883802
594.327833	105.033583	49.888807
590.716071	108.791485	49.893812
587.899164	94.217226	49.898817
584.265231	103.448813	49.903821
580.392023	95.709283	49.908826
577.138211	106.387310	49.913831
573.764087	106.431662	49.918836
570.444589	102.610788	49.923841
566.679482	106.506612	49.928845
563.062255	95.784665	49.933850
559.653663	93.496374	49.938855
555.944152	94.241841	49.943860
552.778423	100.770990	49.948865
548.920159	100.043280	49.953869
546.054929	96.100648	49.958874
542.490577	92.305480	49.963879
538.684980	100.279465	49.968884
534.886333	96.647547	49.973889
531.043860	98.979929	49.978893
527.679524	91.556202	49.983898
524.463728	99.254314	49.988903
520.650311	101.873220	49.993908
517.595861	92.739967	49.998913
514.248047	103.635214	50.003917
510.898562	99.945612	50.008922
507.083386	98.878973	50.013927
503.307883	105.807368	50.018932
500.534971	104.115572	50.023937
496.134958	101.197965	50.028941
493.030668	94.796558	50.033946
489.313365	90.879835	50.038951
485.612082	106.601460	50.043956
482.570259	88.984103	50.048961
479.070141	97.748666	50.053965
476.124085	91.509148	50.058970
472.293978	95.889756	50.063975
468.685672	106.455654	50.068980
465.093209	94.486505	50.073985
461.275688	91.949088	50.078989
458.050949	102.530839	50.083994
454.296752	97.936529	50.088999
451.300245	93.723424	50.094004
447.485200	100.512497	50.099009
443.669952	105.064800	50.104013
440.302979	92.392784	50.109018
437.054024	93.056670	50.114023
433.731814	93.921858	50.119028
430.053937	96.703069	50.124033
426.196793	103.505072	50.129037
422.944563	91.438361	50.134042
419.559479	100.890453	50.139047
415.697764	95.354372	50.144052
412.306750	94.376361	50.149057
408.961413	93.824637	50.154061
405.724912	99.817578	50.159066
401.988892	101.234820	50.164071
397.899519	110.177136	50.169076
395.116265	102.535892	50.174081
391.170498	107.450350	50.179085
388.071999	100.959490	50.184090
385.093144	98.673558	50.189095
380.982475	100.905640	50.194100
377.532781	90.793469	50.199105
373.774150	104.388546	50.204109
370.585277	92.909892	50.209114
367.138314	94.658361	50.214119
363.158076	89.381321	50.219124
359.893957	97.188291	50.224129
356.366462	95.564121	50.229133
352.841683	92.927112	50.234138
349.558455	94.877734	50.239143
345.767349	91.023257	50.244148
342.407454	89.252615	50.249153
338.738161	93.114533	50.254157
335.197060	92.432149	50.259162
331.599717	89.993181	50.264167
328.180270	92.806716	50.269172
325.164675	85.154445	50.274177
321.533832	87.434777	50.279181
318.054849	82.439915	50.284186
314.071070	86.468165	50.289191
310.218928	90.640313	50.294196
307.503999	92.821470	50.299201
303.810718	98.990401	50.304205
300.650259	93.480569	50.309210
297.294170	86.944680	50.314215
293.571428	93.640253	50.319220
289.805722	85.150035	50.324225
286.448491	105.943159	50.329229
282.537814	96.779614	50.334234
279.393179	84.984025	50.339239
276.220407	93.311390	50.344244
272.517096	90.053806	50.349249
268.608287	94.661960	50.354253
264.918042	90.873979	50.359258
261.779628	93.808032	50.364263
258.273680	88.899676	50.369268
254.801995	82.514795	50.374273
251.079559	102.023686	50.379277
248.039265	91.047004	50.384282
244.505194	86.902370	50.389287
240.788649	87.089077	50.394292
237.656452	84.159662	50.399297
234.025943	95.906035	50.404301
229.963552	88.177339	50.409306
226.575151	88.236715	50.414311
222.847584	81.774873	50.419316
219.783908	93.571658	50.424321
216.305934	93.211631	50.429325
213.368184	89.467143	50.434330
209.330829	89.147294	50.439335
205.844091	92.107458	50.444340
202.607860	89.305086	50.449345
198.802287	89.249491	50.454349
195.063489	84.020135	50.459354
191.676793	88.537034	50.464359
188.150480	90.449863	50.469364
184.691173	78.548594	50.474369
181.017710	91.136949	50.479373
177.498067	80.526468	50.484378
174.276075	88.788804	50.489383
170.642148	94.951648	50.494388
167.448310	86.368736	50.499393
163.617931	89.714949	50.504397
160.215828	97.635347	50.509402
156.742072	96.553339	50.514407
152.997181	96.779325	50.519412
149.689825	86.648130	50.524417
146.422676	87.754738	50.529421
143.092729	90.877025	50.534426
139.536355	90.589424	50.539431
135.516277	89.668946	50.544436
132.086510	78.452781	50.549441
128.395165	89.579120	50.554445
124.678724	89.091974	50.559450
121.631055	89.129646	50.564455
118.262618	85.209058	50.569460
114.942148	88.997430	50.574465
111.059117	89.352645	50.579469
107.548275	88.342908	50.584474
104.374363	85.078391	50.589479
100.673253	97.503426	50.594484
97.077878	89.128987	50.599489
93.273413	94.233399	50.604493
89.971727	93.890096	50.609498
86.932427	91.360640	50.614503
82.965962	89.988858	50.619508
79.676933	91.257107	50.624513
76.717189	102.446021	50.629517
72.836250	90.731082	50.634522
69.243441	97.336778	50.639527
65.491407	98.104928	50.644532
62.037694	86.924182	50.649537
58.456545	98.469887	50.654541
55.162437	89.092805	50.659546
51.439995	85.436519	50.664551
47.876293	99.763624	50.669556
44.665131	89.835707	50.674561
40.971152	89.436827	50.679565
37.773165	94.955608	50.684570
34.538098	90.542754	50.689575
30.784592	93.468851	50.694580
27.205983	93.384098	50.699585
23.159641	95.698011	50.704589
19.854987	94.700298	50.709594
16.664016	85.819609	50.714599
12.801459	96.966489	50.719604
9.604558	84.543295	50.724609
5.729796	94.249403	50.729613
2.658615	91.528819	50.734618