Thu Aug 25 13:07:03 2022

Number of Points = 9926

Depth (nm)	Load (N)	Time (s)
1.170764	98.519273	0.000000
1.705673	93.695991	0.005005
1.544702	102.181050	0.010010
1.286783	87.354717	0.015014
1.152255	78.086808	0.020019
0.848208	79.899714	0.025024
0.497545	61.414784	0.030029
0.174852	62.607345	0.035034
0.356533	49.629416	0.040038
-0.073749	40.224368	0.045043
-0.331543	33.291679	0.050048
-0.368272	30.212632	0.055053
-0.729551	33.606896	0.060058
-1.389198	19.602868	0.065062
-1.669074	18.710121	0.070067
-1.989925	7.228330	0.075072
-1.798735	2.218480	0.080077
-2.036696	10.674430	0.085082
-2.429617	9.242572	0.090086
-2.719110	13.233028	0.095091
-3.024583	11.914019	0.100096
-3.541439	1.949913	0.105101
-4.402136	10.281970	0.110106
-4.328403	0.484760	0.115110
-4.947903	-7.890865	0.120115
-4.791070	-2.242927	0.125120
-4.399658	-7.568884	0.130125
-4.564728	3.128242	0.135130
-4.844084	-3.294850	0.140134
-5.638144	0.296930	0.145139
-6.013446	6.265529	0.150144
-6.081857	-4.774914	0.155149
-6.099666	-1.567350	0.160154
-6.091523	-14.704704	0.165158
-7.028390	-0.308435	0.170163
-7.252982	-2.940423	0.175168
-7.187817	-5.241323	0.180173
-7.561364	4.077429	0.185178
-7.460066	-2.373668	0.190182
-8.276861	-2.128754	0.195187
-8.584917	2.377138	0.200192
-8.798902	4.669474	0.205197
-9.136513	9.382480	0.210202
-8.764663	4.606916	0.215206
-9.004259	4.141295	0.220211
-9.336036	1.042044	0.225216
-9.882990	2.472221	0.230221
-10.378072	6.618274	0.235226
-10.149114	-1.760577	0.240230
-10.284594	7.169697	0.245235
-11.040999	9.180024	0.250240
-11.724172	2.032423	0.255245
-11.884694	2.146037	0.260250
-11.825452	0.763557	0.265254
-11.949181	-0.096707	0.270259
-11.891568	0.064987	0.275264
-11.755169	-3.338573	0.280269
-12.288285	4.486573	0.285274
-12.851585	5.210627	0.290278
-13.029218	-3.291180	0.295283
-13.103727	5.363784	0.300288
-13.241223	-7.371103	0.305293
-14.391072	-9.038703	0.310298
-14.266993	2.983028	0.315302
-14.881448	4.287740	0.320307
-14.782096	6.432904	0.325312
-14.869160	-1.782536	0.330317
-15.172660	9.268478	0.335322
-14.961798	2.157968	0.340326
-15.068117	-7.171262	0.345331
-16.121065	0.004501	0.350336
-16.232755	-9.504221	0.355341
-16.488780	1.700702	0.360346
-16.597390	-9.042372	0.365350
-16.548571	-4.146307	0.370355
-16.706317	-4.222954	0.375360
-17.247698	5.808633	0.380365
-18.006897	2.751041	0.385370
-17.747114	0.603146	0.390374
-17.954043	5.295675	0.395379
-18.207696	3.193425	0.400384
-18.603661	-2.151534	0.405389
-19.444787	1.014187	0.410394
-19.299394	-0.897485	0.415398
-19.443024	-4.782355	0.420403
-19.442521	-1.783306	0.425408
-19.328377	-3.525566	0.430413
-19.784232	3.176992	0.435418
-20.409320	-5.488823	0.440422
-20.700524	4.762993	0.445427
-20.962390	-3.608555	0.450432
-20.915132	4.192094	0.455437
-21.514678	0.353348	0.460442
-21.939706	-5.540715	0.465446
-22.249662	0.025336	0.470451
-22.778924	6.625501	0.475456
-22.116532	-5.057795	0.480461
-22.536137	1.123389	0.485466
-22.130811	-7.900028	0.490470
-22.684375	1.253938	0.495475
-23.463108	4.109326	0.500480
-23.738383	-4.209501	0.505485
-24.050721	5.270504	0.510490
-23.888292	0.549901	0.515494
-24.080750	-4.624462	0.520499
-24.893757	5.962213	0.525504
-25.092022	9.833970	0.530509
-25.320378	4.491222	0.535514
-25.278381	0.966410	0.540518
-25.329157	5.001719	0.545523
-25.663353	2.298319	0.550528
-26.289555	-6.455906	0.555533
-26.777503	5.351672	0.560538
-26.561781	-6.578013	0.565542
-26.839246	3.200248	0.570547
-26.977566	0.270003	0.575552
-26.812460	-1.239795	0.580557
-28.000283	-1.974460	0.585562
-28.174774	-5.807037	0.590566
-28.361690	-2.996923	0.595571
-28.339269	-2.282383	0.600576
-28.646895	-5.426545	0.605581
-29.090271	-3.933503	0.610586
-28.912344	-3.676765	0.615590
-29.222273	-2.210959	0.620595
-29.728309	2.952379	0.625600
-29.663356	-1.297368	0.630605
-29.914468	-7.807140	0.635610
-29.914169	-9.753025	0.640614
-30.725520	0.782768	0.645619
-30.825502	-1.283447	0.650624
-30.882267	-17.609193	0.655629
-31.265233	-3.280732	0.660634
-31.941346	-6.841722	0.665638
-32.572272	-16.389306	0.670643
-32.610764	-6.506124	0.675648
-32.508773	-17.582748	0.680653
-32.643214	-9.842221	0.685658
-32.567217	-8.981052	0.690662
-32.678163	-9.678802	0.695667
-33.262075	-16.228175	0.700672
-33.561165	-3.017009	0.705677
-33.664468	-0.580664	0.710682
-33.740614	-5.127843	0.715686
-34.532174	-16.149882	0.720691
-35.252878	1.816046	0.725696
-35.290974	-15.221311	0.730701
-35.455670	0.990195	0.735706
-35.766323	-4.858513	0.740710
-35.328618	-7.160836	0.745715
-35.531060	-9.907024	0.750720
-35.412273	-13.029412	0.755725
-36.572138	-11.319702	0.760730
-36.705836	-3.775443	0.765734
-36.947443	-8.929448	0.770739
-37.210835	-5.851086	0.775744
-36.830426	-4.509265	0.780749
-38.008111	0.734001	0.785754
-38.192159	-3.457748	0.790758
-38.408073	-7.736252	0.795763
-38.413470	-4.717297	0.800768
-38.288706	-11.017042	0.805773
-38.697813	1.866515	0.810778
-39.323188	-2.246593	0.815782
-39.586140	-12.035333	0.820787
-39.750789	-5.549250	0.825792
-39.931324	-12.051095	0.830797
-40.255996	-6.764316	0.835802
-40.107700	-9.587606	0.840806
-40.406328	-6.060796	0.845811
-41.145957	-0.101554	0.850816
-41.373918	-6.194172	0.855821
-41.438872	-10.417235	0.860826
-41.584197	-10.451535	0.865830
-41.602372	-10.572196	0.870835
-42.104449	-8.766235	0.875840
-42.513754	-11.103522	0.880845
-42.889202	-6.840174	0.885850
-43.077582	-9.639185	0.890854
-43.216575	-7.773055	0.895859
-43.602845	1.218656	0.900864
-42.996762	-10.209039	0.905869
-44.014620	-2.020041	0.910874
-44.314206	-6.845421	0.915878
-44.460417	-11.742288	0.920883
-44.753139	-1.167535	0.925888
-44.614716	-1.597473	0.930893
-45.416825	-2.996851	0.935898
-45.923817	-6.543209	0.940902
-45.720064	-7.214338	0.945907
-45.931080	-5.852615	0.950912
-45.887959	-1.999701	0.955917
-46.142696	1.140581	0.960922
-46.383127	5.436561	0.965926
-47.080125	-1.863892	0.970931
-47.434612	0.327071	0.975936
-47.299325	-5.613655	0.980941
-47.750874	-5.891039	0.985946
-47.832548	-8.149948	0.990950
-47.728969	-15.351208	0.995955
-48.434275	-5.812801	1.000960
-48.676939	-15.889455	1.005965
-48.912219	-4.757391	1.010970
-49.013742	-3.938010	1.015974
-49.545432	-9.467342	1.020979
-50.740996	1.065377	1.025984
-50.142010	-5.422569	1.030989
-50.423187	2.423211	1.035994
-50.468511	-9.573135	1.040998
-50.548888	-14.423369	1.046003
-50.850028	-1.129624	1.051008
-50.264278	-10.485030	1.056013
-51.588191	-8.366799	1.061018
-52.239688	-0.197239	1.066022
-52.084536	-12.253469	1.071027
-52.372979	-7.643085	1.076032
-52.299766	-15.364771	1.081037
-52.684792	-3.899195	1.086042
-52.757597	-2.049762	1.091046
-53.276210	-10.583556	1.096051
-53.873205	-0.907093	1.101056
-53.544009	-6.207483	1.106061
-53.928519	-2.407787	1.111066
-53.261163	-8.814696	1.116070
-54.041137	-4.513273	1.121075
-54.672493	-0.633770	1.126080
-54.716156	-7.811962	1.131085
-55.085126	-5.963580	1.136090
-56.077808	-1.315615	1.141094
-56.177589	2.667259	1.146099
-56.140895	5.236693	1.151104
-56.488917	-1.400264	1.156109
-56.578711	6.592702	1.161114
-56.362279	-3.397705	1.166118
-56.671931	-7.538134	1.171123
-57.045669	-3.642049	1.176128
-57.410371	-4.967593	1.181133
-58.127844	-0.147613	1.186138
-58.304303	-2.132241	1.191142
-58.050827	-2.266993	1.196147
-58.185617	-9.427742	1.201152
-58.099358	-1.914784	1.206157
-59.201550	-10.559618	1.211162
-59.249914	-8.976608	1.216166
-59.770375	-10.995920	1.221171
-59.881907	3.429220	1.226176
-59.912580	-5.744181	1.231181
-60.063691	6.893308	1.236186
-60.212651	-5.330411	1.241190
-60.468067	-0.794803	1.246195
-60.959657	7.760995	1.251200
-61.082875	0.588938	1.256205
-61.236216	11.692353	1.261210
-61.843177	3.874753	1.266214
-62.229618	6.858502	1.271219
-62.655308	5.254611	1.276224
-62.397597	-5.931838	1.281229
-62.545664	-1.950890	1.286234
-62.655915	-3.575731	1.291238
-63.527530	-0.718444	1.296243
-63.961906	-1.219982	1.301248
-63.912868	-11.990915	1.306253
-64.030394	-2.705957	1.311258
-63.995914	-8.131011	1.316262
-64.155928	-2.737152	1.321267
-64.524928	4.559239	1.326272
-64.734768	-7.740361	1.331277
-65.262231	-3.434210	1.336282
-65.731140	0.897568	1.341286
-65.373703	2.246152	1.346291
-66.082581	-0.642147	1.351296
-66.383069	-8.090146	1.356301
-66.640009	-0.918883	1.361306
-67.178923	-3.466816	1.366310
-67.071506	-2.730793	1.371315
-67.224025	-7.610853	1.376320
-66.784716	-12.624773	1.381325
-67.447259	5.534524	1.386330
-67.959748	-3.392538	1.391334
-68.242650	4.744580	1.396339
-68.587538	-5.547016	1.401344
-68.735679	-1.834976	1.406349
-68.968083	2.523020	1.411354
-69.491755	-0.729658	1.416358
-69.705460	-1.221480	1.421363
-70.080208	0.036184	1.426368
-70.287008	-11.694411	1.431373
-70.299628	2.133095	1.436378
-69.949329	-10.099246	1.441382
-70.309592	-5.692744	1.446387
-71.155604	-11.574620	1.451392
-71.385514	0.436130	1.456397
-71.817466	3.044194	1.461402
-71.598155	8.891149	1.466406
-71.821469	-1.498592	1.471411
-72.322779	3.214752	1.476416
-72.565642	-1.050037	1.481421
-73.021981	-2.120775	1.486426
-72.937673	-4.424673	1.491430
-72.875984	-6.456107	1.496435
-73.158140	8.337456	1.501440
-73.632746	-11.013818	1.506445
-74.002910	-4.565137	1.511450
-74.044001	0.253266	1.516454
-74.314058	-2.722774	1.521459
-74.573025	2.740375	1.526464
-75.370965	2.248348	1.531469
-75.592092	2.482191	1.536474
-75.659998	3.973351	1.541478
-76.025906	4.274172	1.546483
-76.058152	2.966140	1.551488
-75.963489	-10.842829	1.556493
-75.897801	-2.459778	1.561498
-76.818191	4.065630	1.566502
-77.036977	-4.875813	1.571507
-77.202709	-1.512195	1.576512
-77.199219	-6.416699	1.581517
-77.531843	3.550537	1.586522
-77.997367	2.671064	1.591526
-77.926460	-7.094056	1.596531
-78.470703	-0.203643	1.601536
-78.597201	-3.790637	1.606541
-79.598037	0.921884	1.611546
-80.008000	-2.725098	1.616550
-79.185088	-6.308994	1.621555
-79.627584	2.650398	1.626560
-79.537321	-1.290101	1.631565
-80.005841	-4.946889	1.636570
-80.273515	1.887534	1.641574
-80.916733	-0.954104	1.646579
-81.301268	-0.422573	1.651584
-81.310133	-1.813363	1.656589
-81.619240	-1.825163	1.661594
-81.873304	-1.864570	1.666598
-81.721387	-2.787005	1.671603
-82.456082	5.825866	1.676608
-82.918327	-8.224874	1.681613
-82.986196	-4.446319	1.686618
-83.363977	-7.778801	1.691622
-83.301463	-15.963883	1.696627
-83.241994	-4.571121	1.701632
-83.367378	-10.806357	1.706637
-84.254621	-6.054690	1.711642
-84.824436	-4.083088	1.716646
-84.641423	-8.534829	1.721651
-85.163065	-15.976643	1.726656
-84.827707	-17.649159	1.731661
-85.104476	-18.089970	1.736666
-85.106892	-15.463791	1.741670
-85.351561	-15.014287	1.746675
-86.231394	-8.362360	1.751680
-86.056237	-10.591907	1.756685
-86.499324	-9.200149	1.761690
-86.944378	-5.795928	1.766694
-87.154599	-9.790582	1.771699
-87.762882	0.618479	1.776704
-87.683079	-13.457078	1.781709
-87.616362	-16.346678	1.786714
-88.060259	-5.191420	1.791718
-87.971089	-8.024428	1.796723
-88.272337	-3.820162	1.801728
-88.625446	-7.871521	1.806733
-89.162211	8.316027	1.811738
-89.572105	5.643474	1.816742
-89.057002	-19.595610	1.821747
-89.541296	-8.785202	1.826752
-89.999650	-19.878421	1.831757
-90.548435	-7.476027	1.836762
-90.558783	-9.540465	1.841766
-90.381960	-7.831388	1.846771
-90.988109	-5.525061	1.851776
-91.454737	-3.272234	1.856781
-91.627270	-7.908709	1.861786
-91.909404	-6.807927	1.866790
-91.690939	-17.301681	1.871795
-92.065547	-1.680554	1.876800
-92.232278	-5.716824	1.881805
-93.094273	-10.697685	1.886810
-93.602040	-8.160000	1.891814
-93.546686	-6.741939	1.896819
-93.888770	-9.488390	1.901824
-93.414065	-16.472552	1.906829
-93.738782	-11.131984	1.911834
-94.146146	-8.996011	1.916838
-94.598682	-9.434590	1.921843
-95.295154	0.121418	1.926848
-94.816541	-5.480795	1.931853
-94.922405	-8.134546	1.936858
-95.487616	-10.384125	1.941862
-95.996075	-16.299906	1.946867
-96.388260	-10.040766	1.951872
-96.434685	-12.960094	1.956877
-96.512295	-8.746579	1.961882
-96.810872	-4.931874	1.966886
-96.654937	-18.196777	1.971891
-97.614060	-13.221875	1.976896
-97.766383	-16.089809	1.981901
-97.819516	-10.301412	1.986906
-98.229199	-4.795667	1.991910
-98.343543	-14.250179	1.996915
-98.096330	-12.730288	2.006912
-98.291719	-4.625159	2.016909
-98.328015	-9.973322	2.026906
-97.584259	-4.812530	2.036902
-96.818698	-13.241908	2.046899
-95.843465	-5.719351	2.056896
-95.513912	-5.524145	2.066893
-95.428376	-6.716219	2.076890
-95.433077	-0.009463	2.086886
-94.665836	-7.387393	2.096883
-93.519212	-3.905311	2.106880
-93.072767	-8.743071	2.116877
-92.830587	-2.508990	2.126874
-92.655627	-2.466957	2.136870
-91.693524	-4.658029	2.146867
-91.607592	-1.494420	2.156864
-90.779614	-0.613869	2.166861
-90.197151	-0.920792	2.176858
-89.773181	-4.098264	2.186854
-89.303626	-0.684319	2.196851
-89.060231	-6.732047	2.206848
-88.127957	-7.112790	2.216845
-87.285587	0.817063	2.226842
-87.395215	-10.300873	2.236838
-86.996484	-7.151432	2.246835
-86.582615	-0.617967	2.256832
-85.972582	-6.514069	2.266829
-84.890008	-3.889930	2.276826
-84.565785	-8.217528	2.286822
-84.528596	-1.463482	2.296819
-84.245441	-5.765639	2.306816
-83.339360	-9.883465	2.316813
-82.825543	-8.776290	2.326810
-81.872479	-7.367306	2.336806
-81.412454	-1.791418	2.346803
-81.389106	-5.302093	2.356800
-81.245593	-3.661722	2.366797
-80.651899	-5.361075	2.376794
-79.538591	-7.328748	2.386790
-78.881809	-3.769910	2.396787
-78.810066	0.127689	2.406784
-78.954153	-0.182600	2.416781
-77.917460	1.023213	2.426778
-77.273048	-2.182465	2.436774
-76.478487	-0.593421	2.446771
-76.370758	-4.133157	2.456768
-75.894110	-0.045578	2.466765
-75.002787	0.562121	2.476762
-74.937380	-5.378524	2.486758
-74.317214	-8.311136	2.496755
-73.780611	-6.203334	2.506752
-73.255112	-8.468543	2.516749
-72.948527	-2.352258	2.526746
-72.223428	-9.096355	2.536742
-71.886067	-3.209808	2.546739
-70.999091	-5.233882	2.556736
-70.737750	-0.814792	2.566733
-70.630261	-0.866725	2.576730
-69.449126	2.280502	2.586726
-69.164838	4.117396	2.596723
-68.902308	8.735875	2.606720
-68.168762	-0.721201	2.616717
-67.539557	3.396329	2.626714
-67.681092	2.683328	2.636710
-66.713378	5.604235	2.646707
-66.619808	2.519714	2.656704
-65.683514	-0.104470	2.666701
-64.835436	-2.961921	2.676698
-65.009784	-0.020456	2.686694
-64.059768	-2.627783	2.696691
-63.509598	3.067032	2.706688
-63.471567	0.856028	2.716685
-62.736259	1.209406	2.726682
-62.184728	-0.100035	2.736678
-62.095689	-1.622112	2.746675
-61.117013	5.377227	2.756672
-60.684305	2.435972	2.766669
-60.309307	-0.654631	2.776666
-59.508687	6.112847	2.786662
-59.415691	-0.319967	2.796659
-58.766225	6.433181	2.806656
-57.838735	6.484014	2.816653
-57.699314	6.908586	2.826650
-57.461320	2.093982	2.836646
-56.497461	1.679784	2.846643
-55.973065	0.000793	2.856640
-56.025624	-1.999612	2.866637
-55.567496	-1.080113	2.876634
-54.915903	-0.270123	2.886630
-53.650303	0.104703	2.896627
-53.331134	6.206350	2.906624
-53.407642	5.144203	2.916621
-53.020600	0.508985	2.926618
-52.197673	-2.325517	2.936614
-51.530311	-3.440862	2.946611
-51.415066	-5.043072	2.956608
-50.699448	-9.603058	2.966605
-50.387912	-1.735745	2.976602
-49.287402	-4.772131	2.986598
-48.835459	-8.175732	2.996595
-48.656192	-1.013122	3.006592
-48.564943	6.781005	3.016589
-48.039161	-0.844196	3.026586
-47.415637	-2.598907	3.036582
-46.399038	-11.682176	3.046579
-45.897052	-9.229991	3.056576
-45.932549	-8.904724	3.066573
-45.046536	-0.826480	3.076570
-44.277841	-2.559587	3.086566
-44.662913	-0.639988	3.096563
-44.004529	-0.901783	3.106560
-43.183291	-2.209133	3.116557
-42.788678	-2.001943	3.126554
-41.662567	-9.404422	3.136550
-41.288866	-2.535207	3.146547
-41.233888	-5.822756	3.156544
-41.298086	1.295639	3.166541
-40.092940	3.960769	3.176538
-39.919421	-1.809917	3.186534
-38.915440	-2.518671	3.196531
-38.340376	-0.790693	3.206528
-38.490975	-0.361861	3.216525
-37.579474	3.774797	3.226522
-37.093750	-3.232738	3.236518
-36.815321	2.057996	3.246515
-35.945291	2.729223	3.256512
-35.541961	1.829479	3.266509
-35.347745	2.280312	3.276506
-34.812547	2.272237	3.286502
-34.445897	-2.891978	3.296499
-33.957026	-5.024734	3.306496
-33.202123	-2.244709	3.316493
-32.393018	-2.568133	3.326490
-31.641731	2.309555	3.336486
-31.465089	-4.332769	3.346483
-31.440080	-0.643258	3.356480
-30.886193	-2.836886	3.366477
-30.489411	-1.128491	3.376474
-29.666355	0.478268	3.386470
-28.673760	-2.870661	3.396467
-28.435799	-2.185928	3.406464
-28.487135	-0.426326	3.416461
-27.886986	-3.127719	3.426458
-26.723066	-3.193122	3.436454
-26.993684	-6.147720	3.446451
-26.114390	-8.259286	3.456448
-25.916376	-6.592607	3.466445
-24.817347	-2.738757	3.476442
-24.236207	-2.354884	3.486438
-24.285236	-8.214243	3.496435
-23.932705	-6.331020	3.506432
-22.899066	-6.781491	3.516429
-22.740850	-7.436921	3.526426
-22.447349	-12.089157	3.536422
-21.577874	-7.388379	3.546419
-21.179138	-7.403582	3.556416
-20.516097	-6.950179	3.566413
-20.025518	-10.068393	3.576410
-19.603672	-10.400830	3.586406
-19.066827	-4.821134	3.596403
-18.587481	-6.698972	3.606400
-18.187902	-7.743847	3.616397
-17.754507	-4.359077	3.626394
-17.038977	-7.845158	3.636390
-16.510965	-9.249113	3.646387
-16.398589	-1.426618	3.656384
-15.428353	-4.955776	3.666381
-15.193986	-1.340249	3.676378
-14.733070	-3.870937	3.686374
-13.789195	-5.704350	3.696371
-13.544607	-9.015272	3.706368
-13.055981	-5.404737	3.716365
-12.713587	-9.155471	3.726362
-12.308283	-4.898318	3.736358
-11.249403	-9.379037	3.746355
-10.685132	-5.628299	3.756352
-10.622313	-5.920322	3.766349
-10.651532	-5.725920	3.776346
-9.995035	-6.481596	3.786342
-9.138141	-5.672092	3.796339
-8.483515	-5.249047	3.806336
-8.362401	-0.950533	3.816333
-7.426036	0.071436	3.826330
-7.089325	-3.231747	3.836326
-6.645307	-4.099851	3.846323
-6.341975	2.736046	3.856320
-5.467190	2.969373	3.866317
-5.504215	3.117482	3.876314
-4.712575	12.008816	3.886310
-3.870656	17.290463	3.896307
-3.735689	18.767451	3.906304
-3.367552	24.690374	3.916301
-2.774172	42.980042	3.926298
-2.354751	42.853893	3.936294
-1.871314	57.973970	3.946291
-1.705400	62.547417	3.956288
-1.391215	83.082512	3.966285
-0.779766	100.634471	3.976282
0.000000	109.896814	3.981286
-0.142488	129.616764	3.986291
-0.016582	114.442366	3.991296
0.299852	128.639205	3.996301
0.761431	144.518599	4.001306
0.675610	144.512940	4.006310
0.544496	156.691821	4.011315
0.380956	157.036866	4.016320
0.825703	154.312636	4.021325
0.898157	154.788386	4.026330
1.122464	148.030056	4.031334
0.656148	154.990576	4.036339
0.729302	145.069989	4.041344
1.048099	143.833495	4.046349
0.993179	144.791115	4.051354
1.236500	139.203577	4.056358
0.804117	138.062632	4.061363
0.737698	130.527274	4.066368
-0.014611	133.463962	4.071373
0.191538	138.598011	4.076378
1.145254	150.648045	4.081382
0.438683	156.143407	4.086387
0.956678	152.373140	4.091392
1.176822	147.940852	4.096397
1.014122	154.100818	4.101402
1.054568	144.049313	4.106406
0.944370	152.311303	4.111411
0.846930	148.124929	4.116416
1.215343	148.336005	4.121421
0.810307	147.981724	4.126426
0.758343	147.739803	4.131430
0.648585	148.481386	4.136435
0.847247	149.525827	4.141440
0.786477	151.686606	4.146445
0.811634	152.720267	4.151450
0.700885	148.374624	4.156454
1.097951	163.254893	4.161459
1.516101	162.531185	4.166464
0.978474	145.454876	4.171469
0.658342	150.089249	4.176474
0.929947	156.481729	4.181478
1.133890	171.385935	4.186483
1.211028	172.133038	4.191488
1.408179	162.278436	4.196493
1.371326	169.728502	4.201498
1.571158	163.293544	4.206502
1.360003	165.041284	4.211507
1.102760	155.286355	4.216512
1.061775	156.649922	4.221517
0.752155	157.824622	4.226522
1.311376	159.859787	4.231526
1.240425	182.381202	4.236531
1.577033	166.945952	4.241536
1.598615	163.775487	4.246541
1.658063	152.563051	4.251546
1.557722	151.822503	4.256550
1.151429	146.697417	4.261555
1.246038	149.349549	4.266560
1.278617	146.677244	4.271565
1.013484	152.274285	4.276570
1.119814	145.407889	4.281574
1.243917	155.904773	4.286579
1.290945	170.175495	4.291584
1.540990	170.848050	4.296589
1.254702	173.556701	4.301594
1.190280	169.096226	4.306598
1.291216	177.730112	4.311603
1.476198	177.004971	4.316608
1.721537	181.307141	4.321613
1.178454	182.423508	4.326618
1.838497	178.178556	4.331622
1.543509	175.364578	4.336627
1.918615	172.046972	4.341632
1.603364	163.275577	4.346637
1.303963	166.505144	4.351642
1.898845	166.623789	4.356646
1.518223	165.851225	4.361651
1.225028	160.952027	4.366656
1.508306	168.633511	4.371661
1.269271	169.803480	4.376666
1.262388	172.151974	4.381670
1.619224	174.098626	4.386675
1.422804	182.791761	4.391680
1.649914	180.709076	4.396685
1.499526	184.095636	4.401690
1.592767	176.630157	4.406694
1.322514	174.258399	4.411699
1.460760	173.179908	4.416704
1.728305	172.698098	4.421709
1.416128	177.059145	4.426714
1.626996	174.899911	4.431718
1.662644	182.797373	4.436723
1.987893	186.011332	4.441728
1.848411	179.151799	4.446733
1.989045	172.868485	4.451738
1.846745	175.500791	4.456742
1.651030	177.429613	4.461747
1.429085	168.839751	4.466752
2.080418	174.732974	4.471757
1.925099	188.193844	4.476762
1.861913	177.190435	4.481766
1.676499	170.512111	4.486771
1.890269	194.254449	4.491776
2.466972	186.178534	4.496781
1.536016	186.520431	4.501786
1.748079	177.473417	4.506790
2.048048	201.686321	4.511795
2.128405	201.996316	4.516800
2.102960	185.773041	4.521805
1.799728	189.591679	4.526810
1.957865	190.503265	4.531814
2.100116	204.120006	4.536819
2.262007	199.022942	4.541824
1.837270	191.796804	4.546829
1.793729	193.771388	4.551834
2.321646	194.371933	4.556838
2.163740	189.442038	4.561843
1.817087	192.704324	4.566848
2.078441	187.898568	4.571853
2.303570	205.203972	4.576858
2.081727	198.335189	4.581862
1.980741	191.814475	4.586867
2.066774	195.553141	4.591872
2.226207	199.226523	4.596877
2.220501	202.435391	4.601882
2.526984	192.199805	4.606886
1.872451	191.504958	4.611891
2.010360	195.384195	4.616896
2.145007	200.646526	4.621901
1.871976	203.400561	4.626906
2.069625	192.979544	4.631910
2.248190	202.945895	4.636915
2.091002	198.509439	4.641920
2.162140	206.116609	4.646925
2.414768	204.839857	4.651930
2.644265	196.486139	4.656934
2.291657	202.232944	4.661939
2.294259	196.749544	4.666944
2.238923	204.107606	4.671949
2.185155	205.115670	4.676954
2.616262	192.620584	4.681958
2.158085	205.360115	4.686963
2.399780	203.455479	4.691968
2.310136	204.241370	4.696973
2.320579	201.926871	4.701978
2.592767	200.732478	4.706982
2.027438	201.994703	4.711987
2.547384	200.970301	4.716992
2.020469	199.951733	4.721997
2.049217	198.301929	4.727002
2.496191	204.625820	4.732006
2.693348	226.035917	4.737011
2.539230	216.957670	4.742016
2.504738	204.905692	4.747021
2.216987	217.605874	4.752026
2.797366	210.750601	4.757030
2.729300	215.076573	4.762035
2.526536	201.753802	4.767040
2.587187	209.343633	4.772045
2.461673	215.247854	4.777050
2.838502	215.770830	4.782054
2.676603	212.401311	4.787059
2.730082	210.342663	4.792064
2.801532	211.115970	4.797069
2.502185	198.165844	4.802074
2.636235	199.267868	4.807078
2.681869	205.831815	4.812083
2.618277	211.492211	4.817088
2.398308	210.302161	4.822093
2.615543	231.399065	4.827098
3.099639	224.533563	4.832102
2.771062	232.769693	4.837107
2.620952	229.812782	4.842112
2.714756	227.222623	4.847117
2.556416	229.800502	4.852122
2.539723	219.422544	4.857126
2.749252	232.155555	4.862131
2.621808	223.924190	4.867136
2.756030	229.395407	4.872141
2.617011	230.606658	4.877146
2.635009	219.179208	4.882150
3.001501	227.524734	4.887155
2.796911	225.993746	4.892160
3.156759	225.563913	4.897165
2.727962	230.737361	4.902170
3.102076	220.839181	4.907174
2.956303	219.703945	4.912179
3.199789	220.219339	4.917184
3.119939	221.551035	4.922189
2.927292	233.619385	4.927194
3.105536	215.525996	4.932198
2.948136	223.507508	4.937203
2.775068	230.694198	4.942208
2.994218	228.897498	4.947213
2.825841	229.698890	4.952218
2.956325	227.438347	4.957222
2.784791	232.840411	4.962227
2.676537	228.431082	4.967232
3.024829	231.404153	4.972237
3.076151	248.227458	4.977242
3.109131	240.897947	4.982246
2.784295	255.575019	4.987251
3.339831	259.423639	4.992256
3.497248	251.280509	4.997261
3.279270	248.460781	5.002266
3.066494	250.876347	5.007270
2.917961	249.906059	5.012275
3.028882	247.569484	5.017280
3.269412	252.710835	5.022285
3.066066	258.972120	5.027290
3.124174	251.512114	5.032294
3.127500	248.439410	5.037299
3.122396	242.087155	5.042304
3.305137	237.920137	5.047309
3.220632	250.275280	5.052314
3.465514	246.285189	5.057318
3.241542	252.669928	5.062323
3.438292	247.475638	5.067328
3.455560	251.864180	5.072333
3.305342	257.905166	5.077338
3.533676	251.665031	5.082342
3.487884	253.643138	5.087347
3.339580	254.571103	5.092352
3.413962	247.766622	5.097357
3.900187	249.930296	5.102362
3.716708	244.732305	5.107366
3.309077	257.267796	5.112371
3.296592	249.828344	5.117376
3.482264	249.438455	5.122381
3.500868	249.868860	5.127386
3.208154	246.358476	5.132390
3.149163	260.168146	5.137395
3.185943	250.806866	5.142400
3.720314	254.358238	5.147405
3.254599	253.462958	5.152410
3.620820	252.712581	5.157414
3.436098	254.500480	5.162419
2.990565	254.801123	5.167424
3.387767	247.354429	5.172429
3.432657	257.335428	5.177434
3.695752	261.046366	5.182438
3.565773	265.812330	5.187443
3.729620	271.585809	5.192448
3.609331	267.681403	5.197453
3.385551	267.254425	5.202458
3.651632	269.493724	5.207462
3.819623	270.191794	5.212467
3.413232	272.321316	5.217472
3.681789	264.682796	5.222477
3.672657	275.599267	5.227482
3.809689	266.883510	5.232486
3.894411	276.886753	5.237491
3.702813	266.934812	5.242496
4.067173	265.624731	5.247501
3.719211	272.997032	5.252506
4.137797	272.912342	5.257510
4.065271	276.947957	5.262515
3.615351	263.524656	5.267520
4.054521	261.260037	5.272525
3.695400	264.388245	5.277530
3.804020	264.725451	5.282534
4.122163	266.523150	5.287539
3.802606	266.997047	5.292544
3.937685	261.973770	5.297549
3.859666	269.496767	5.302554
4.035012	267.909410	5.307558
3.968310	278.290727	5.312563
3.566757	268.387500	5.317568
4.081549	271.897650	5.322573
3.833714	275.666497	5.327578
3.894297	274.182544	5.332582
3.995389	273.081394	5.337587
4.035865	273.252103	5.342592
4.242736	263.671174	5.347597
3.972029	272.695537	5.352602
3.938732	276.889524	5.357606
3.640650	279.827834	5.362611
3.725904	286.410913	5.367616
3.976659	274.532499	5.372621
3.912981	277.579617	5.377626
3.890894	272.634747	5.382630
3.913600	275.570252	5.387635
3.689501	273.210232	5.392640
4.146899	281.402333	5.397645
4.040242	286.863852	5.402650
3.923839	293.823386	5.407654
4.188815	296.132465	5.412659
4.117599	303.543677	5.417664
4.394626	286.462981	5.422669
4.310568	294.496309	5.427674
4.303491	288.878353	5.432678
4.073445	287.057113	5.437683
4.352875	294.732927	5.442688
4.409347	290.332576	5.447693
3.918450	304.880680	5.452698
4.311354	298.750789	5.457702
4.199042	298.600581	5.462707
4.551529	296.830440	5.467712
4.731358	298.491622	5.472717
4.425557	301.655776	5.477722
4.532955	291.799346	5.482726
4.652415	296.807816	5.487731
4.179942	301.497735	5.492736
4.177908	297.574793	5.497741
4.021362	297.849140	5.502746
4.209854	292.678278	5.507750
4.152033	297.293736	5.512755
3.744798	294.468852	5.517760
4.421384	288.003446	5.522765
4.244391	298.965214	5.527770
4.021382	300.850868	5.532774
4.629081	316.486054	5.537779
4.581540	322.817865	5.542784
4.675448	318.307234	5.547789
4.397230	319.002451	5.552794
4.760559	313.544755	5.557798
4.896310	308.249271	5.562803
4.348576	311.796190	5.567808
4.834871	311.251628	5.572813
4.536042	310.327033	5.577818
4.461753	304.820845	5.582822
4.827560	310.901222	5.587827
4.485933	310.742650	5.592832
4.790191	312.248293	5.597837
4.644822	308.803397	5.602842
4.705888	311.710751	5.607846
4.638952	308.633226	5.612851
4.787570	314.877350	5.617856
4.981464	313.685725	5.622861
4.414238	308.231459	5.627866
4.595247	314.385085	5.632870
4.916539	321.883506	5.637875
4.666431	322.697708	5.642880
4.798800	328.235686	5.647885
4.828205	329.556599	5.652890
4.910006	319.482697	5.657894
4.472505	325.132109	5.662899
4.482069	318.578208	5.667904
5.106442	308.365516	5.672909
4.273765	319.480651	5.677914
4.525663	321.383649	5.682918
4.739923	315.661401	5.687923
4.661847	318.157113	5.692928
4.864723	321.921793	5.697933
5.021557	330.584962	5.702938
5.084071	326.952464	5.707942
4.953724	325.381360	5.712947
4.957036	326.405798	5.717952
5.097125	321.859457	5.722957
4.528358	331.053938	5.727962
4.493366	312.930584	5.732966
4.928987	331.905268	5.737971
5.245532	346.542037	5.742976
5.040372	336.291618	5.747981
4.840544	346.652703	5.752986
4.967824	344.588805	5.757990
5.370244	342.997502	5.762995
5.018377	347.035770	5.768000
5.128336	341.269743	5.773005
5.236268	349.412224	5.778010
5.400684	347.196971	5.783014
5.204772	330.016322	5.788019
4.939821	328.384049	5.793024
4.879947	323.179324	5.798029
5.172712	351.743820	5.803034
5.511007	346.872181	5.808038
5.022552	331.252842	5.813043
4.930073	340.274624	5.818048
5.600007	344.766578	5.823053
5.103459	355.829071	5.828058
5.385171	357.015540	5.833062
5.000553	352.652645	5.838067
5.062133	360.527140	5.843072
5.214572	355.488461	5.848077
4.903403	349.038586	5.853082
5.277751	351.963302	5.858086
5.268279	357.346339	5.863091
5.200664	356.056476	5.868096
5.299564	349.273426	5.873101
5.215891	356.749888	5.878106
5.520812	350.507211	5.883110
5.345562	353.483236	5.888115
5.274647	355.794329	5.893120
5.382619	354.217521	5.898125
5.508845	350.192213	5.903130
5.531110	344.585461	5.908134
5.519831	353.369896	5.913139
5.428205	351.046059	5.918144
5.960623	355.088151	5.923149
5.626585	357.741035	5.928154
5.882843	350.499884	5.933158
5.683154	353.084260	5.938163
5.420670	350.584708	5.943168
5.527667	349.672457	5.948173
5.408883	358.821760	5.953178
5.267145	347.042759	5.958182
5.565384	353.734865	5.963187
5.391016	356.875272	5.968192
5.617871	349.958275	5.973197
5.329845	348.630179	5.978202
5.239400	349.729421	5.983206
5.507401	349.418382	5.988211
5.326576	355.619224	5.993216
5.828024	349.839313	5.998221
5.692800	353.308951	6.003226
5.243044	352.401673	6.008230
5.670379	344.254176	6.013235
5.316034	348.748425	6.018240
5.703187	354.556547	6.023245
5.449451	357.269617	6.028250
5.701356	351.449708	6.033254
5.981521	360.444753	6.038259
5.777640	353.202928	6.043264
5.732247	347.527680	6.048269
5.715729	351.579847	6.053274
5.219217	355.286431	6.058278
5.202279	352.039709	6.063283
5.750177	367.535610	6.068288
5.676883	356.182488	6.073293
5.520787	360.908276	6.078298
5.687277	356.686828	6.083302
5.554291	363.177576	6.088307
5.688520	363.498116	6.093312
5.856484	363.183768	6.098317
5.209575	353.214530	6.103322
5.490832	363.022510	6.108326
5.956310	371.773385	6.113331
5.389449	372.437896	6.118336
5.682420	362.245460	6.123341
5.609102	382.429426	6.128346
5.651784	374.547832	6.133350
5.730323	363.930237	6.138355
5.536097	367.798274	6.143360
5.610836	374.205859	6.148365
5.724868	373.362109	6.153370
5.809827	357.402961	6.158374
6.011551	356.191124	6.163379
5.602524	356.084241	6.168384
5.810580	353.561586	6.173389
5.581022	349.905241	6.178394
5.729673	348.587822	6.183398
5.580963	349.038116	6.188403
5.504959	352.957232	6.193408
5.395837	338.926807	6.198413
5.617351	346.118161	6.203418
5.491726	355.240059	6.208422
5.643459	357.396042	6.213427
5.531008	357.305968	6.218432
5.619668	352.796152	6.223437
5.620925	359.000104	6.228442
5.876066	347.136773	6.233446
6.020902	351.521172	6.238451
5.461087	359.515174	6.243456
5.618434	351.944662	6.248461
5.320237	348.466756	6.253466
5.524393	351.601639	6.258470
5.610074	348.120535	6.263475
5.179970	356.967429	6.268480
5.811219	349.287866	6.273485
5.666283	364.468364	6.278490
5.565732	355.574648	6.283494
5.731943	353.624874	6.288499
5.202669	358.589469	6.293504
5.702543	359.599384	6.298509
5.486386	380.767534	6.303514
5.858234	381.411521	6.308518
5.737098	383.480543	6.313523
5.692058	371.958466	6.318528
5.696567	359.447844	6.323533
5.285165	359.809580	6.328538
5.547631	372.069314	6.333542
5.943566	374.237659	6.338547
5.571951	371.714073	6.343552
5.756770	351.828787	6.348557
5.446398	356.205413	6.353562
5.677709	352.372453	6.358566
5.645041	354.664898	6.363571
5.477012	354.336753	6.368576
5.666094	355.487114	6.373581
5.403367	358.188937	6.378586
5.773364	367.460983	6.383590
5.817499	361.815997	6.388595
5.853484	361.544474	6.393600
5.917020	356.725373	6.398605
5.444183	350.139473	6.403610
5.484613	347.190655	6.408614
5.462333	347.773004	6.413619
5.557310	349.906240	6.418624
5.575623	339.136740	6.423629
5.711348	349.318699	6.428634
5.482351	355.678952	6.433638
5.905614	353.318735	6.438643
5.362357	345.975059	6.443648
5.575080	346.542735	6.448653
5.431050	355.199270	6.453658
5.849998	366.181605	6.458662
5.680261	361.130127	6.463667
5.543201	355.633758	6.468672
5.630158	344.246045	6.473677
5.573496	342.685541	6.478682
5.655066	353.853610	6.483686
5.528962	349.579929	6.488691
5.312982	359.468977	6.493696
5.675029	366.432672	6.498701
5.825094	372.569019	6.503706
5.843161	376.429107	6.508710
5.654506	359.731360	6.513715
5.094016	363.720060	6.518720
5.656812	363.558990	6.523725
5.984979	371.448670	6.528730
5.736756	380.058265	6.533734
5.771484	365.163702	6.538739
5.489118	355.086724	6.543744
5.468096	354.007865	6.548749
5.672906	362.261726	6.553754
5.525962	358.965768	6.558758
5.687034	359.155549	6.563763
5.586429	359.579324	6.568768
5.601215	350.936464	6.573773
5.313730	358.596724	6.578778
5.365968	373.803286	6.583782
5.864812	375.588503	6.588787
5.581399	375.531543	6.593792
5.903675	377.850638	6.598797
5.389671	376.266873	6.603802
5.741658	382.786049	6.608806
5.926441	374.540497	6.613811
5.506572	365.057712	6.618816
5.843881	354.450199	6.623821
5.619354	357.867390	6.628826
5.376185	360.866713	6.633830
5.673744	364.635550	6.638835
5.370364	366.597080	6.643840
5.956141	369.532965	6.648845
5.448654	366.695302	6.653850
5.408992	362.196097	6.658854
5.626105	366.622961	6.663859
5.535479	377.723110	6.668864
5.863935	365.326247	6.673869
5.813251	371.946476	6.678874
5.699236	374.555397	6.683878
5.407644	366.650249	6.688883
5.542530	383.008160	6.693888
6.034510	371.101378	6.698893
5.964744	369.185412	6.703898
5.608758	357.253307	6.708902
5.597305	347.320554	6.713907
5.661562	355.197790	6.718912
5.533581	343.967143	6.723917
5.740059	355.311800	6.728922
5.847082	351.134472	6.733926
5.762100	346.019098	6.738931
5.566219	356.838325	6.743936
5.661593	346.825558	6.748941
5.534797	353.789907	6.753946
5.511246	351.771787	6.758950
5.650690	348.516383	6.763955
5.192553	355.162480	6.768960
5.390324	350.929804	6.773965
5.234755	351.817782	6.778970
5.672839	365.442080	6.783974
5.897339	366.877965	6.788979
5.349887	355.070776	6.793984
5.625290	359.665679	6.798989
5.807959	368.286852	6.803994
5.580071	354.648356	6.808998
5.537408	351.440466	6.814003
5.793777	368.396277	6.819008
5.574631	354.626694	6.824013
5.501127	362.114220	6.829018
5.836222	360.647362	6.834022
5.554984	355.597537	6.839027
5.079689	358.212439	6.844032
5.447037	372.569180	6.849037
5.566615	383.127020	6.854042
5.474865	388.333127	6.859046
5.664742	377.182374	6.864051
5.583270	382.399525	6.869056
5.668565	376.048878	6.874061
5.914056	384.986091	6.879066
5.794828	383.669510	6.884070
5.996527	377.367065	6.889075
5.448217	371.773770	6.894080
6.016826	363.202323	6.899085
5.407685	371.093324	6.904090
5.738535	353.051818	6.909094
5.762704	358.847210	6.914099
5.277409	354.041333	6.919104
5.609471	355.640702	6.924109
5.412619	376.112942	6.929114
5.821750	370.527828	6.934118
5.933897	379.666269	6.939123
5.663998	364.363843	6.944128
5.440481	362.763040	6.949133
5.442135	366.888296	6.954138
5.500102	367.638411	6.959142
5.789368	371.927417	6.964147
5.613861	370.489938	6.969152
5.581131	367.122298	6.974157
5.642122	369.536115	6.979162
5.350463	373.545973	6.984166
5.430764	367.759274	6.989171
5.484992	381.127344	6.994176
5.997617	382.771193	6.999181
5.693343	393.161325	7.004186
5.808297	379.763329	7.009190
5.924034	373.366783	7.014195
5.247883	370.251818	7.019200
5.579073	362.454743	7.024205
5.420486	379.662246	7.029210
5.625110	385.502141	7.034214
5.658771	375.739478	7.039219
5.453796	379.685134	7.044224
5.987594	379.898776	7.049229
5.643269	378.918029	7.054234
5.150671	379.080510	7.059238
5.496949	379.880368	7.064243
5.262116	383.773754	7.069248
5.501407	387.330257	7.074253
5.840896	382.429947	7.079258
5.825903	376.791056	7.084262
5.731129	368.124224	7.089267
5.635922	376.817414	7.094272
5.923374	388.377201	7.099277
5.665221	385.570073	7.104282
5.713990	383.508980	7.109286
5.756434	375.890022	7.114291
5.550532	373.334144	7.119296
5.575751	366.530993	7.124301
5.647893	383.060090	7.129306
5.450802	374.235276	7.134310
5.899607	373.275797	7.139315
5.388996	375.829795	7.144320
5.339268	383.107956	7.149325
5.677122	381.691285	7.154330
5.560196	379.197398	7.159334
5.564470	381.939651	7.164339
5.449743	386.829810	7.169344
5.414514	379.463471	7.174349
5.055859	388.508000	7.179354
5.360836	379.367230	7.184358
5.517515	377.846065	7.189363
5.352891	394.700179	7.194368
5.256868	382.534332	7.199373
5.125225	394.052216	7.204378
5.717841	406.013466	7.209382
6.148360	404.139337	7.214387
5.651884	393.845942	7.219392
5.584561	387.044627	7.224397
5.338543	383.102946	7.229402
5.324918	385.655010	7.234406
5.837539	396.087998	7.239411
5.926859	402.040880	7.244416
5.814884	386.216969	7.249421
5.743886	382.693966	7.254426
5.924965	385.069987	7.259430
5.747116	376.963510	7.264435
5.599631	389.315962	7.269440
5.986446	369.667933	7.274445
5.606610	385.511692	7.279450
5.686094	381.572797	7.284454
5.907756	378.187443	7.289459
5.438545	383.414724	7.294464
5.516234	375.353634	7.299469
5.605776	379.575856	7.304474
5.612251	373.417898	7.309478
5.835320	382.213086	7.314483
5.668727	379.227095	7.319488
5.598525	371.328387	7.324493
5.558659	383.518436	7.329498
5.692869	383.234688	7.334502
5.723758	382.229953	7.339507
5.464215	387.772406	7.344512
5.845247	375.405265	7.349517
5.860215	386.321192	7.354522
5.626978	388.306536	7.359526
5.804766	376.271803	7.364531
5.495153	384.270908	7.369536
5.438484	367.729649	7.374541
5.613606	379.876520	7.379546
5.792743	377.140088	7.384550
5.996705	373.165871	7.389555
5.704464	384.338743	7.394560
6.129380	379.744597	7.399565
5.586933	356.426595	7.404570
5.598575	360.284522	7.409574
5.587124	343.919702	7.414579
5.099207	353.142657	7.419584
5.422517	361.321002	7.424589
5.847252	371.011590	7.429594
5.893330	366.834317	7.434598
5.947353	357.906888	7.439603
5.560044	352.282047	7.444608
5.361736	348.032334	7.449613
5.280980	355.030600	7.454618
5.416427	370.695533	7.459622
5.688783	373.243917	7.464627
5.520520	383.024260	7.469632
5.725163	374.259891	7.474637
5.787122	377.309488	7.479642
5.474519	367.724471	7.484646
5.556974	363.199805	7.489651
5.490897	380.041629	7.494656
6.106549	364.571979	7.499661
5.737613	371.896985	7.504666
5.837407	352.186375	7.509670
5.560669	349.062619	7.514675
5.496194	359.057646	7.519680
5.370952	350.917629	7.524685
5.593448	363.000117	7.529690
5.861722	366.001567	7.534694
5.754960	356.033120	7.539699
5.402265	351.870873	7.544704
5.422803	356.360171	7.549709
5.747553	370.011722	7.554714
5.811599	371.029811	7.559718
5.526770	358.808138	7.564723
5.496399	366.146536	7.569728
5.589592	365.423114	7.574733
5.439553	377.314038	7.579738
5.353369	376.103015	7.584742
6.023109	367.705550	7.589747
5.659355	368.309764	7.594752
5.772867	371.076029	7.599757
5.754472	366.886710	7.604762
5.479889	355.166484	7.609766
5.420290	359.908791	7.614771
5.494035	376.659099	7.619776
5.875918	371.587631	7.624781
6.180936	375.007279	7.629786
5.649700	361.400487	7.634790
5.753207	356.328345	7.639795
5.306902	357.730123	7.644800
5.283931	350.697241	7.649805
5.567699	357.198622	7.654810
5.385837	374.254739	7.659814
5.730257	370.631848	7.664819
5.473788	369.599370	7.669824
5.688248	371.618974	7.674829
5.739594	378.327625	7.679834
5.604181	381.104420	7.684838
5.860050	365.001425	7.689843
5.369951	368.090060	7.694848
5.764449	369.062700	7.699853
5.693962	370.089212	7.704858
5.508053	364.606822	7.709862
6.026566	357.473278	7.714867
5.425288	359.706114	7.719872
5.621597	348.971996	7.724877
5.414796	352.285167	7.729882
5.386320	360.543939	7.734886
5.967845	370.700356	7.739891
5.774102	365.459644	7.744896
5.787962	356.740994	7.749901
5.428225	352.526065	7.754906
5.506829	353.345714	7.759910
5.673511	353.025239	7.764915
5.205079	361.621871	7.769920
5.537594	367.884659	7.774925
5.433638	375.225098	7.779930
5.651443	376.339321	7.784934
5.414945	366.641139	7.789939
5.735402	374.098583	7.794944
5.793275	376.535036	7.799949
5.819896	372.284878	7.804954
5.769533	376.978284	7.809958
5.984230	368.028840	7.814963
5.673364	370.608491	7.819968
5.318899	357.989595	7.824973
5.289237	361.553430	7.829978
5.535502	371.512433	7.834982
5.467131	370.662460	7.839987
5.437121	374.064996	7.844992
5.562573	373.089740	7.849997
5.440247	374.111719	7.855002
5.638364	372.615701	7.860006
6.123087	369.442239	7.865011
5.496864	381.075572	7.870016
5.551236	373.378813	7.875021
5.510003	369.449342	7.880026
5.289714	376.175243	7.885030
5.768748	377.520626	7.890035
5.585800	380.469388	7.895040
6.036827	378.278829	7.900045
5.834735	378.598279	7.905050
5.620771	382.953479	7.910054
5.931504	365.089123	7.915059
5.501129	375.546460	7.920064
5.595050	364.796736	7.925069
6.081083	370.785529	7.930074
5.290992	371.905806	7.935078
5.720328	359.970880	7.940083
5.479973	364.839587	7.945088
5.707936	362.775731	7.950093
5.745800	362.601993	7.955098
5.203645	358.624456	7.960102
5.448086	365.805898	7.965107
5.227621	384.234848	7.970112
5.626833	375.351406	7.975117
5.651852	376.233237	7.980122
5.743954	371.027002	7.985139
5.937431	371.813908	7.990157
5.564001	376.094705	7.995174
5.745159	373.102937	8.000192
6.082534	380.532268	8.005210
5.743504	369.644235	8.010227
5.595538	357.391386	8.015245
5.826629	356.237917	8.020262
5.657382	357.914774	8.025280
5.711415	344.860279	8.030298
5.402353	349.250903	8.035315
5.659372	352.864879	8.040333
5.753785	365.031197	8.045350
5.932887	360.809006	8.050368
5.742090	356.654240	8.055386
5.630233	352.095792	8.060403
5.477138	346.253102	8.065421
5.477371	355.758087	8.070438
5.583552	361.055628	8.075456
6.058951	361.662663	8.080474
5.754157	368.413132	8.085491
5.753451	353.940803	8.090509
5.696770	356.975934	8.095526
5.799001	347.738666	8.100544
5.735443	357.903734	8.105562
5.552986	356.941290	8.110579
6.060305	367.853195	8.115597
5.407595	362.114025	8.120614
5.774579	368.443663	8.125632
5.786351	372.178118	8.130650
5.821054	372.999368	8.135667
5.949032	371.880988	8.140685
5.825876	377.526887	8.145702
5.902893	366.794572	8.150720
5.592202	352.219336	8.155738
5.529736	363.832730	8.160755
5.965636	367.585937	8.165773
5.993003	368.547189	8.170790
6.072410	365.214764	8.175808
5.923149	357.900884	8.180826
5.580079	351.459961	8.185843
5.866874	344.882484	8.190861
5.907232	351.913378	8.195878
5.526546	342.928499	8.200896
6.070831	353.411731	8.205914
5.753199	367.460328	8.210931
6.042739	357.957025	8.215949
5.892424	351.040939	8.220966
5.624986	339.273874	8.225984
6.175729	350.516630	8.231002
5.719757	358.559397	8.236019
5.834931	336.681293	8.241037
5.470313	356.458629	8.246054
5.695902	363.318497	8.251072
5.882408	359.458059	8.256090
5.886345	369.461082	8.261107
5.781235	369.142917	8.266125
5.723619	374.690184	8.271142
5.558164	366.432109	8.276160
5.812905	363.277337	8.281178
6.017865	365.457290	8.286195
6.028948	365.868835	8.291213
5.867403	366.029721	8.296230
5.804787	364.269027	8.301248
5.561422	363.543341	8.306266
5.315085	370.900025	8.311283
5.505425	375.610035	8.316301
5.695057	387.076648	8.321318
5.995905	383.375013	8.326336
6.578747	395.165027	8.331354
6.176618	395.944269	8.336371
6.473529	385.802332	8.341389
6.389045	376.067291	8.346406
6.125364	376.442993	8.351424
6.332201	370.168364	8.356442
6.332419	377.994499	8.361459
6.251592	373.980287	8.366477
6.019721	376.547415	8.371494
5.794721	371.356603	8.376512
6.268219	372.134348	8.381530
5.727628	375.914323	8.386547
6.033756	370.624514	8.391565
5.965447	365.721573	8.396582
5.957105	375.496153	8.401600
6.085194	372.231837	8.406618
5.971425	377.693230	8.411635
6.298143	369.260212	8.416653
6.180825	367.075749	8.421670
5.814670	368.344808	8.426688
6.215259	372.207688	8.431706
5.881457	378.640818	8.436723
5.836489	369.574924	8.441741
6.099822	371.673148	8.446758
5.953494	371.954725	8.451776
6.020992	366.159515	8.456794
5.867322	376.423918	8.461811
6.138563	377.021916	8.466829
6.360009	371.657014	8.471846
6.060194	373.149206	8.476864
6.223906	367.869088	8.481882
6.041714	371.930575	8.486899
6.319157	368.674417	8.491917
6.267184	373.403457	8.496934
6.257218	371.041230	8.501952
6.322069	365.839719	8.506970
6.335150	363.107813	8.511987
6.179978	371.248621	8.517005
6.000664	373.400421	8.522022
6.105746	375.981027	8.527040
6.308981	367.295961	8.532058
6.067866	367.838538	8.537075
5.956228	377.585122	8.542093
6.027649	376.548186	8.547110
5.793983	375.013104	8.552128
6.433411	377.901303	8.557146
6.432386	374.751890	8.562163
6.235175	367.398182	8.567181
6.433014	369.932696	8.572199
5.982367	373.307264	8.577216
6.099542	368.794977	8.582234
6.045005	384.850455	8.587251
6.434718	391.236500	8.592269
6.247569	392.392308	8.597287
6.346222	392.446155	8.602304
6.416240	385.883693	8.607322
6.147025	390.703579	8.612339
6.256125	385.889600	8.617357
6.395161	395.988233	8.622375
6.337970	394.274023	8.627392
6.224150	392.145812	8.632410
5.839823	389.160592	8.637427
6.328317	393.066508	8.642445
6.506713	400.725882	8.647463
6.368070	397.815774	8.652480
6.465622	396.654823	8.657498
6.294519	402.895215	8.662515
6.481227	396.282908	8.667533
6.716564	397.110593	8.672551
6.432819	397.016073	8.677568
6.344213	381.850602	8.682586
6.342775	374.825975	8.687603
5.960205	383.497872	8.692621
6.424332	378.659826	8.697639
6.252694	392.808643	8.702656
6.912143	391.127314	8.707674
6.591172	381.296782	8.712691
5.993158	374.495013	8.717709
6.241487	389.294385	8.722727
6.407050	402.535164	8.727744
6.656881	394.461315	8.732762
6.254700	399.191585	8.737779
6.201013	398.161626	8.742797
6.561774	395.574054	8.747815
6.319854	401.143895	8.752832
6.978269	395.120393	8.757850
6.516626	393.346477	8.762867
6.148223	393.126368	8.767885
6.449768	391.665216	8.772903
5.991364	394.100585	8.777920
6.306129	391.624361	8.782938
6.297237	396.302477	8.787955
5.994835	395.702802	8.792973
6.363882	396.626300	8.797991
6.207137	398.724075	8.803008
6.339037	388.907788	8.808026
6.169892	393.585766	8.813043
6.052601	408.868467	8.818061
6.452274	407.300422	8.823079
6.502924	425.797800	8.828096
6.690468	422.855515	8.833114
6.641733	423.033440	8.838131
6.727215	419.302426	8.843149
6.887510	412.097811	8.848167
6.614986	428.875440	8.853184
6.547438	412.406465	8.858202
6.682905	424.515899	8.863219
6.500353	415.193830	8.868237
6.839138	400.576754	8.873255
6.171168	415.311432	8.878272
6.819967	415.484207	8.883290
6.536000	417.756550	8.888307
6.199825	426.796736	8.893325
6.543745	432.249550	8.898343
6.602309	433.638259	8.903360
6.888457	419.168269	8.908378
6.751508	422.272792	8.913395
6.741856	425.906474	8.918413
6.858425	423.890484	8.923431
6.702030	422.936576	8.928448
6.513493	427.721741	8.933466
6.702796	422.756332	8.938483
6.898038	430.485661	8.943501
6.692328	414.489607	8.948519
6.643303	409.476336	8.953536
6.584382	402.889890	8.958554
6.416327	409.659975	8.963571
6.351693	421.762890	8.968589
6.704906	415.253874	8.973607
6.942736	427.978427	8.978624
6.411872	425.331737	8.983642
6.722239	423.320096	8.988659
6.666157	418.961173	8.993677
6.860895	416.588957	8.998695
6.772619	426.189898	9.003712
6.577031	422.001153	9.008730
7.184873	415.417529	9.013747
6.613734	420.884325	9.018765
7.083357	419.803931	9.023783
7.054700	423.626781	9.028800
6.848592	421.459379	9.033818
7.075758	423.673729	9.038835
6.615644	413.713502	9.043853
6.685454	415.472828	9.048871
6.686989	426.006428	9.053888
6.988877	425.782282	9.058906
6.776938	418.184712	9.063923
6.936943	431.218102	9.068941
6.862293	428.310586	9.073959
6.761650	430.595232	9.078976
6.736338	434.780475	9.083994
6.777908	429.131317	9.089011
6.548494	432.553283	9.094029
6.893166	427.743407	9.099047
6.870018	425.462132	9.104064
6.689714	420.406312	9.109082
6.778679	425.094349	9.114099
6.475357	419.281484	9.119117
6.745785	418.730911	9.124135
6.841024	424.759168	9.129152
6.893834	428.039085	9.134170
7.435435	426.805403	9.139187
7.052105	424.810933	9.144205
7.174937	419.884341	9.149223
6.931397	422.923514	9.154240
6.911526	424.987224	9.159258
7.094572	425.700027	9.164275
6.928676	432.851632	9.169293
7.022060	426.992387	9.174311
7.081908	427.093339	9.179328
6.670857	420.287505	9.184346
7.025086	418.587725	9.189363
6.954697	429.167309	9.194381
6.916340	422.902678	9.199399
6.988110	426.725572	9.204416
6.723463	433.946297	9.209434
7.408736	432.756376	9.214451
6.856353	437.248260	9.219469
6.932395	425.048629	9.224487
6.868197	424.313802	9.229504
6.948770	421.640740	9.234522
7.064763	431.888170	9.239539
6.893460	439.170010	9.244557
7.090835	430.454274	9.249575
7.003722	431.319859	9.254592
6.789597	427.878779	9.259610
7.045127	425.074164	9.264627
6.597169	439.518773	9.269645
7.084488	420.567621	9.274663
7.152339	433.937341	9.279680
7.444306	438.599887	9.284698
7.347224	428.207235	9.289715
6.772691	427.214701	9.294733
6.847132	422.062163	9.299751
7.018152	429.517579	9.304768
7.207548	442.316002	9.309786
7.272132	447.048890	9.314803
7.060333	457.546507	9.319821
7.214597	460.693770	9.324839
7.522927	450.152379	9.329856
7.368752	434.716272	9.334874
7.146198	430.184616	9.339891
7.035214	423.237093	9.344909
7.098298	421.996336	9.349927
6.844158	425.936565	9.354944
7.494690	436.964927	9.359962
7.347870	428.612387	9.364979
6.875844	429.655043	9.369997
7.452254	436.365299	9.375015
7.600564	430.910854	9.380032
7.187134	426.724682	9.385050
7.100927	422.357855	9.390067
7.013254	421.566747	9.395085
7.080664	429.407623	9.400103
7.093293	441.470043	9.405120
7.570309	450.818327	9.410138
7.631503	439.040730	9.415155
7.062642	434.181484	9.420173
7.351511	427.518445	9.425191
7.268967	423.305677	9.430208
6.797709	430.290532	9.435226
7.222473	444.355412	9.440243
7.112236	452.366141	9.445261
7.479882	451.396396	9.450279
7.231228	452.056921	9.455296
7.424790	452.891153	9.460314
7.957473	451.119229	9.465331
7.877964	443.614506	9.470349
7.249379	435.126009	9.475367
7.452867	434.910968	9.480384
7.120484	427.603661	9.485402
7.485675	424.706126	9.490419
7.240452	434.315882	9.495437
7.146496	434.551385	9.500455
7.132916	443.689356	9.505472
7.418436	444.152577	9.510490
7.583074	441.299085	9.515507
7.566870	443.292795	9.520525
7.697464	446.775121	9.525543
7.160278	438.392221	9.530560
7.295710	446.512777	9.535578
7.460948	448.654783	9.540595
7.305569	444.813180	9.545613
7.389125	449.208584	9.550631
7.597002	450.472915	9.555648
7.270182	449.772924	9.560666
7.828705	445.466019	9.565683
7.426083	451.714300	9.570701
7.594474	448.191194	9.575719
7.741196	452.535677	9.580736
7.385856	458.448351	9.585754
7.582381	452.288917	9.590771
7.533039	453.252726	9.595789
7.347453	449.141302	9.600807
7.594986	451.434514	9.605824
7.422044	457.293364	9.610842
7.749557	458.813503	9.615859
7.486404	459.410028	9.620877
7.306480	456.796710	9.625895
7.747786	449.532273	9.630912
7.509730	455.918871	9.635930
7.581649	459.230514	9.640947
7.690015	457.168468	9.645965
7.794763	459.136918	9.650983
7.789481	459.585743	9.656000
7.468387	450.424216	9.661018
7.728588	444.049683	9.666035
7.664681	454.271664	9.671053
7.420623	449.156398	9.676071
7.595926	445.483887	9.681088
7.597806	454.900306	9.686106
7.591105	440.880122	9.691123
7.535277	451.182885	9.696141
7.728974	455.166562	9.701159
7.767680	453.109120	9.706176
7.475576	450.712193	9.711194
7.605523	441.385328	9.716211
7.213146	453.211415	9.721229
7.478659	452.235581	9.726247
7.210967	450.159875	9.731264
7.381771	462.749788	9.736282
7.562503	455.911179	9.741299
7.573088	458.815869	9.746317
7.568555	455.629121	9.751335
7.951568	468.586573	9.756352
7.694163	475.421175	9.761370
7.931006	466.831780	9.766387
8.066525	454.266207	9.771405
7.658026	453.676842	9.776423
7.791355	455.322079	9.781440
7.631949	461.456518	9.786458
7.792052	450.363999	9.791475
7.722917	454.802263	9.796493
7.491549	455.078230	9.801511
7.779847	467.933758	9.806528
7.968800	476.064877	9.811546
8.219539	465.538812	9.816563
7.709514	465.650158	9.821581
7.439886	472.360442	9.826599
7.986518	475.597710	9.831616
8.235269	475.243035	9.836634
7.728835	466.463986	9.841651
7.378940	474.521742	9.846669
7.819880	479.741622	9.851687
8.015374	475.217037	9.856704
7.384509	480.901490	9.861722
7.946881	475.950197	9.866739
7.895436	475.563662	9.871757
8.216610	480.149059	9.876775
8.002793	480.362317	9.881792
7.771367	482.033149	9.886810
7.877163	472.719519	9.891827
8.134204	483.348819	9.896845
7.881185	480.983634	9.901863
8.112542	479.946879	9.906880
8.157236	479.589462	9.911898
7.895108	473.861642	9.916915
7.982008	476.056950	9.921933
8.081820	479.992226	9.926951
7.820599	470.742414	9.931968
8.244286	481.197280	9.936986
8.363998	478.880992	9.942003
7.799177	480.465206	9.947021
8.025562	483.389737	9.952039
8.094621	471.266906	9.957056
8.007222	482.745429	9.962074
8.036090	476.861563	9.967091
8.051330	484.770596	9.972109
7.873555	487.045244	9.977127
8.227340	483.672963	9.982144
7.682429	495.437770	9.987162
7.978725	485.889160	9.992179
8.058693	482.717570	9.997197
7.932835	483.936364	10.002215
8.124825	483.215044	10.007232
7.862906	491.599848	10.012250
7.878369	488.166966	10.017267
7.991839	484.870207	10.022285
7.625428	482.797341	10.027303
7.608043	485.444487	10.032320
8.052269	496.060245	10.037338
8.058613	501.461832	10.042355
8.248243	506.102560	10.047373
8.359155	510.701975	10.052391
8.270242	495.508053	10.057408
8.379689	505.813355	10.062426
8.000885	503.950710	10.067443
7.968334	504.025114	10.072461
7.946841	513.391577	10.077479
8.440196	507.160372	10.082496
8.377093	515.561373	10.087514
8.120826	509.434994	10.092531
8.275415	506.807127	10.097549
8.314987	508.574356	10.102567
8.442211	498.070780	10.107584
8.300973	502.911670	10.112602
8.061277	509.156534	10.117619
8.279847	498.010644	10.122637
8.118563	508.970589	10.127655
8.507912	503.487822	10.132672
8.197543	502.362376	10.137690
8.468978	500.656626	10.142707
8.393026	505.907007	10.147725
8.146905	502.139569	10.152743
8.470005	500.523553	10.157760
8.188915	510.069543	10.162778
8.461470	510.399099	10.167795
8.126959	515.462778	10.172813
8.090836	514.559448	10.177831
8.324761	509.883666	10.182848
8.273096	505.022260	10.187866
7.964140	502.353413	10.192883
8.020296	517.104106	10.197901
7.919360	519.546599	10.202919
8.500342	531.437980	10.207936
8.523309	533.081582	10.212954
8.629171	545.429265	10.217971
8.542976	530.995433	10.222989
8.301978	521.897059	10.228007
8.460851	523.093334	10.233024
8.616424	535.594167	10.238042
8.274313	529.361311	10.243059
8.621364	523.219294	10.248077
8.176670	531.127828	10.253095
8.610496	533.271942	10.258112
8.558858	534.125662	10.263130
8.323096	539.341132	10.268147
8.429358	535.931884	10.273165
8.681095	537.299803	10.278183
8.827547	535.989171	10.283200
8.754815	539.074184	10.288218
8.389315	529.619774	10.293235
8.648348	529.001556	10.298253
8.143034	532.296357	10.303271
8.700853	533.890871	10.308288
8.404174	539.570320	10.313306
8.629676	539.348674	10.318323
8.658156	535.522425	10.323341
8.709311	548.951651	10.328359
8.504799	536.963158	10.333376
8.468103	528.018962	10.338394
8.413672	531.467179	10.343411
8.569945	530.388537	10.348429
8.449077	540.000957	10.353447
8.418613	538.036393	10.358464
8.779655	543.016346	10.363482
8.484365	535.662158	10.368499
8.766589	540.585032	10.373517
8.667204	531.590697	10.378535
8.789671	530.602558	10.383552
8.713037	530.166320	10.388570
8.733045	529.822237	10.393587
8.953716	528.364278	10.398605
9.058085	538.357971	10.403623
9.035166	529.209646	10.408640
8.774314	532.892176	10.413658
9.012525	527.338408	10.418675
9.078536	533.065170	10.423693
8.661360	532.944218	10.428711
8.632330	531.957726	10.433728
8.925481	531.053297	10.438746
8.398360	538.002765	10.443763
8.881905	532.164406	10.448781
8.838707	529.813676	10.453799
8.731583	542.494528	10.458816
8.639364	529.850975	10.463834
8.295038	533.817981	10.468851
8.753824	525.146448	10.473869
8.750322	536.138491	10.478887
8.994162	527.017798	10.483904
8.838877	531.961883	10.488922
8.884735	532.907623	10.493939
9.086402	533.775304	10.498957
8.817139	536.332535	10.503975
8.896753	532.801231	10.508992
8.724371	541.383468	10.514010
8.750233	536.169081	10.519027
8.814316	535.067014	10.524045
9.060342	539.310752	10.529063
8.986559	529.753832	10.534080
9.002607	538.183468	10.539098
8.734070	536.937856	10.544115
9.261257	536.337584	10.549133
8.956598	541.096792	10.554151
8.776458	538.057464	10.559168
9.022734	542.869207	10.564186
8.730646	543.426087	10.569203
8.871782	537.578259	10.574221
9.038621	539.511742	10.579239
8.872274	535.166912	10.584256
8.798700	533.313244	10.589274
8.988730	555.957719	10.594291
9.130261	551.883381	10.599309
9.149343	564.929481	10.604327
9.330673	554.120750	10.609344
9.087254	542.595939	10.614362
8.518008	544.051464	10.619379
9.266491	546.799529	10.624397
9.474186	552.491474	10.629415
9.321583	548.437976	10.634432
8.833512	541.173950	10.639450
8.883180	545.397963	10.644467
9.164734	542.901675	10.649485
9.012120	563.015250	10.654503
9.230661	556.416832	10.659520
9.227399	556.032213	10.664538
9.083196	554.407359	10.669555
9.354673	556.255022	10.674573
9.303786	565.007582	10.679591
9.418515	559.410037	10.684608
9.156106	551.463712	10.689626
8.730898	554.799613	10.694643
9.134211	555.793491	10.699661
8.902972	556.874166	10.704679
9.088239	564.046542	10.709696
9.151533	562.600615	10.714714
8.783487	562.935867	10.719731
9.355663	560.820075	10.724749
9.322853	568.676714	10.729767
9.090061	563.461820	10.734784
9.230022	558.680828	10.739802
8.919618	571.724909	10.744819
9.519986	563.226833	10.749837
8.810886	569.813507	10.754855
8.996316	576.231626	10.759872
9.300270	577.654482	10.764890
9.224986	587.979307	10.769907
9.534781	581.353959	10.774925
9.508866	590.803206	10.779943
9.631229	595.792169	10.784960
9.529375	575.068086	10.789978
9.267296	580.991435	10.794995
9.405101	552.532837	10.800013
9.319416	554.171373	10.805031
9.362538	567.002271	10.810048
9.716250	571.901330	10.815066
9.130660	570.143660	10.820083
9.281478	570.145153	10.825101
9.559300	580.455675	10.830119
9.406981	577.755963	10.835136
9.708208	585.487690	10.840154
9.464458	583.597564	10.845171
9.682281	582.070619	10.850189
9.099062	573.432936	10.855207
9.539196	578.564609	10.860224
9.931554	577.114460	10.865242
9.297730	567.121404	10.870259
9.227325	564.055410	10.875277
9.669814	579.222149	10.880295
9.730657	582.036934	10.885312
9.631610	586.681888	10.890330
9.718117	575.562954	10.895347
9.860638	574.852537	10.900365
9.603233	561.382777	10.905383
9.346278	558.125108	10.910400
9.297654	567.694666	10.915418
9.310502	582.739376	10.920435
9.510869	574.881478	10.925453
9.658800	585.146082	10.930471
9.436748	585.373254	10.935488
9.588489	589.726452	10.940506
9.354715	588.825684	10.945523
9.416723	581.617466	10.950541
9.566866	587.883328	10.955559
9.324193	586.832476	10.960576
9.825254	584.428023	10.965594
9.435862	582.153618	10.970611
9.449920	576.830615	10.975629
9.733095	586.692179	10.980647
9.502815	596.110333	10.985664
10.066305	600.686198	10.990682
9.755774	600.520135	10.995699
9.912584	580.418238	11.000717
9.755964	592.516746	11.005735
9.269041	584.236354	11.010752
9.663439	595.585813	11.015770
9.987160	601.707719	11.020787
10.102652	608.259884	11.025805
10.091670	583.355893	11.030823
9.842308	589.270940	11.035840
9.926118	587.818641	11.040858
9.866295	585.170708	11.045875
10.031885	583.834983	11.050893
10.069261	575.677575	11.055911
9.640938	583.529918	11.060928
10.198274	572.210985	11.065946
9.673601	569.768430	11.070963
9.579459	575.075330	11.075981
9.995153	581.653032	11.080999
9.835698	587.882196	11.086016
9.811181	585.774684	11.091034
9.820300	580.714385	11.096051
9.876104	581.428197	11.101069
9.717493	586.609502	11.106087
10.045907	597.663188	11.111104
9.965035	602.283208	11.116122
10.095759	609.139099	11.121139
9.907205	604.977612	11.126157
9.931253	597.620701	11.131175
9.866843	602.651552	11.136192
10.375290	604.067616	11.141210
10.003177	604.627569	11.146227
9.899240	599.821664	11.151245
10.190393	598.002362	11.156263
10.074885	600.526044	11.161280
10.159944	602.131521	11.166298
10.188153	607.394014	11.171315
10.294642	603.748033	11.176333
9.675517	581.448193	11.181351
9.945299	592.242819	11.186368
10.251950	594.043949	11.191386
10.034162	612.451036	11.196403
9.889353	609.687026	11.201421
10.255487	603.207477	11.206439
9.630745	609.449588	11.211456
10.026173	599.295251	11.216474
10.378587	604.655270	11.221491
10.217102	603.620098	11.226509
10.274558	599.107643	11.231527
10.298910	605.674086	11.236544
10.474218	596.441020	11.241562
10.173568	610.272551	11.246579
10.203230	606.644918	11.251597
10.340119	597.755541	11.256615
10.165329	610.080969	11.261632
10.466928	603.182342	11.266650
10.449585	601.685930	11.271667
10.525217	597.145381	11.276685
10.369524	610.594439	11.281703
10.239933	606.881304	11.286720
10.446972	592.521399	11.291738
10.550108	601.776863	11.296755
10.372595	589.206592	11.301773
10.325332	575.754390	11.306791
10.220521	578.891774	11.311808
10.162387	584.830506	11.316826
10.508295	595.726816	11.321843
10.524823	598.283459	11.326861
10.694651	589.754998	11.331879
9.806267	584.387196	11.336896
10.211285	581.761105	11.341914
10.049325	593.642701	11.346931
10.419032	607.366042	11.351949
10.556201	598.344078	11.356967
10.064168	598.783964	11.361984
10.474391	596.434766	11.367002
10.336150	601.688624	11.372019
10.334609	602.348305	11.377037
10.294597	603.238076	11.382055
10.208808	608.291213	11.387072
10.282208	604.369549	11.392090
10.216383	599.620789	11.397107
10.323798	605.019194	11.402125
10.739529	611.527475	11.407143
10.651087	615.261903	11.412160
10.639734	600.715303	11.417178
10.482642	608.200112	11.422195
10.375803	604.070003	11.427213
10.621144	605.413682	11.432231
10.377233	616.023720	11.437248
10.861698	611.561122	11.442266
10.568735	610.016376	11.447283
10.394891	609.551185	11.452301
11.029658	614.317858	11.457319
10.701581	616.332049	11.462336
10.734603	606.840404	11.467354
10.685682	611.660547	11.472371
10.901326	597.826309	11.477389
10.804686	599.794769	11.482407
10.649950	607.695775	11.487424
10.632446	594.554476	11.492442
10.523237	598.367894	11.497459
10.824103	596.998351	11.502477
11.118048	591.306444	11.507495
10.940356	606.444144	11.512512
10.865146	603.372585	11.517530
10.644837	603.315461	11.522547
10.505703	600.099284	11.527565
10.552787	601.158446	11.532583
10.340156	612.669296	11.537600
10.928329	624.083087	11.542618
10.908580	620.346428	11.547635
11.124498	621.350735	11.552653
10.981747	606.562785	11.557671
10.723362	609.793664	11.562688
10.802312	597.549278	11.567706
10.793414	600.529627	11.572723
10.825493	607.454622	11.577741
10.622055	601.007509	11.582759
10.584997	620.563402	11.587776
10.827821	631.643142	11.592794
10.875774	633.102957	11.597811
10.870232	630.866234	11.602829
10.750488	635.877362	11.607847
10.718519	635.853846	11.612864
10.720705	630.983968	11.617882
11.037297	627.863641	11.622899
10.649619	636.258749	11.627917
10.980464	622.365416	11.632935
10.712710	627.241942	11.637952
10.924123	634.902555	11.642970
11.159313	634.329095	11.647987
10.877410	636.945125	11.653005
10.697317	633.807943	11.658023
11.141983	636.294355	11.663040
10.953263	641.221617	11.668058
10.995982	644.174951	11.673075
10.963741	660.293454	11.678093
10.695681	650.609118	11.683111
10.984373	663.117585	11.688128
11.220285	663.235135	11.693146
11.154655	649.123034	11.698163
11.057395	662.585066	11.703181
11.086047	652.431361	11.708199
11.217058	659.145215	11.713216
10.954506	658.315224	11.718234
11.444585	651.601643	11.723251
11.306868	656.448334	11.728269
11.531286	652.417791	11.733287
11.200743	651.671037	11.738304
11.504638	657.919146	11.743322
11.707538	653.977181	11.748339
11.009569	651.107330	11.753357
11.056898	636.933358	11.758375
10.852972	650.478366	11.763392
11.254427	644.299382	11.768410
11.140989	653.153304	11.773427
11.038414	654.810275	11.778445
11.507872	650.236410	11.783463
11.214110	657.124114	11.788480
11.224573	657.494738	11.793498
11.571958	647.489912	11.798515
11.367537	654.332059	11.803533
11.571127	647.300448	11.808551
11.196993	656.169971	11.813568
11.335730	659.395442	11.818586
11.412380	654.744265	11.823603
11.239500	656.623691	11.828621
11.478871	645.338751	11.833639
11.490253	650.067406	11.838656
11.437960	656.715305	11.843674
11.792416	656.075820	11.848691
11.392059	657.561697	11.853709
11.641488	652.441636	11.858727
11.572776	653.253855	11.863744
11.626007	649.284848	11.868762
11.757966	650.469570	11.873779
11.296863	645.454526	11.878797
11.851912	645.342191	11.883815
11.885237	649.347883	11.888832
11.316012	645.615259	11.893850
11.311924	640.686401	11.898867
11.169346	646.278622	11.903885
11.420106	644.052234	11.908903
11.466650	646.619960	11.913920
11.891814	656.916908	11.918938
11.707513	650.656128	11.923955
11.404743	658.678181	11.928973
11.639205	654.005434	11.933991
11.328802	652.722193	11.939008
11.152958	654.333839	11.944026
11.150681	654.756951	11.949043
11.417838	650.719713	11.954061
11.653073	647.277613	11.959079
11.883635	646.559711	11.964096
11.413897	657.530204	11.969114
11.890898	656.675859	11.974131
11.865966	663.732885	11.979149
11.662115	663.878311	11.984167
11.800708	667.394141	11.989184
11.600694	665.632854	11.994202
11.949960	648.451413	11.999219
11.715004	670.421004	12.004237
12.084719	672.171237	12.009255
11.738782	664.600867	12.014272
11.736324	658.548279	12.019290
12.033853	658.940197	12.024307
11.817065	665.301447	12.029325
11.667852	659.375994	12.034343
11.788430	657.469803	12.039360
11.920240	669.636781	12.044378
12.159856	666.623182	12.049395
12.057696	664.029208	12.054413
11.828035	661.306887	12.059431
11.908040	653.789706	12.064448
11.966021	657.845185	12.069466
11.841284	654.891831	12.074483
12.138458	666.679447	12.079501
11.806846	661.871328	12.084519
12.058907	661.531910	12.089536
11.857271	660.663972	12.094554
12.248188	661.678733	12.099571
12.102912	667.110437	12.104589
12.018038	653.023439	12.109607
11.791907	659.692264	12.114624
11.678369	661.480342	12.119642
12.343678	665.642639	12.124659
12.080019	667.236487	12.129677
12.407476	669.100638	12.134695
12.018183	671.960717	12.139712
11.773927	674.495114	12.144730
12.087879	667.897485	12.149747
11.738988	666.449859	12.154765
12.291859	668.133524	12.159783
12.345418	663.722649	12.164800
12.013509	668.483004	12.169818
12.316395	661.795593	12.174835
12.458956	671.265823	12.179853
12.486705	673.388372	12.184871
12.428738	666.170515	12.189888
11.977413	660.399695	12.194906
12.254627	662.319054	12.199923
12.255400	669.463574	12.204941
12.490755	673.904677	12.209959
12.280286	662.068512	12.214976
12.155167	663.299825	12.219994
12.464462	661.528168	12.225011
11.900142	656.529292	12.230029
12.302413	662.828261	12.235047
12.145510	662.666528	12.240064
12.449156	671.767537	12.245082
12.298573	663.453345	12.250099
12.173929	668.862882	12.255117
12.197306	666.268173	12.260135
12.142528	674.039938	12.265152
12.105149	677.999909	12.270170
12.358370	675.126189	12.275187
11.934084	678.099049	12.280205
12.166538	681.931537	12.285223
12.180948	672.909834	12.290240
12.166830	691.032624	12.295258
12.535022	687.282506	12.300275
12.349821	700.127182	12.305293
12.657543	697.443736	12.310311
12.631681	697.813740	12.315328
12.540020	700.930150	12.320346
12.912679	693.376567	12.325363
12.723901	687.946456	12.330381
12.654443	679.565897	12.335399
12.854157	677.297009	12.340416
12.304397	677.364088	12.345434
12.341749	670.323799	12.350451
12.528473	670.742547	12.355469
12.564057	680.914355	12.360487
12.720634	689.918494	12.365504
12.913670	692.456963	12.370522
12.721530	673.665650	12.375539
12.691363	673.029624	12.380557
12.651036	663.865022	12.385575
12.811555	666.907200	12.390592
12.301323	666.125483	12.395610
12.706322	671.669788	12.400627
12.943557	685.600139	12.405645
12.805306	679.332134	12.410663
12.892061	672.634400	12.415680
12.436653	672.033441	12.420698
12.799677	679.263219	12.425715
12.704126	678.836253	12.430733
13.042288	689.206812	12.435751
12.889325	685.225923	12.440768
12.857573	671.304157	12.445786
12.606709	659.916136	12.450803
12.535482	672.380016	12.455821
12.788675	686.232128	12.460839
12.645332	683.524682	12.465856
12.960824	693.081438	12.470874
12.780697	687.870879	12.475891
13.171895	690.463507	12.480909
13.031373	692.369425	12.485927
13.177491	684.254890	12.490944
13.129721	695.105644	12.495962
12.752441	687.183568	12.500979
12.604023	683.728988	12.505997
12.417699	687.705986	12.511015
12.993864	687.467267	12.516032
12.895287	683.048665	12.521050
12.791854	686.845418	12.526067
12.979906	689.312083	12.531085
12.933139	693.882602	12.536103
12.918854	688.191620	12.541120
13.368161	689.099404	12.546138
13.144564	690.911040	12.551155
13.134796	688.794893	12.556173
12.721103	696.859589	12.561191
12.991665	684.948041	12.566208
12.472624	691.312475	12.571226
12.890546	701.354963	12.576243
13.159217	704.550617	12.581261
13.343714	703.016260	12.586279
13.371113	706.480092	12.591296
13.583891	709.924347	12.596314
13.158913	701.239717	12.601331
13.117817	689.768318	12.606349
13.220133	689.127312	12.611367
13.414059	694.591086	12.616384
13.035473	692.056196	12.621402
13.035238	697.796546	12.626419
13.122366	695.052987	12.631437
12.839433	705.066431	12.636455
13.310359	701.625263	12.641472
13.362913	711.191668	12.646490
13.207894	705.765729	12.651507
13.403453	700.483680	12.656525
13.573793	712.518418	12.661543
13.644455	718.348653	12.666560
13.496551	715.998524	12.671578
13.135240	706.265651	12.676595
13.353151	708.844406	12.681613
12.938152	716.101425	12.686631
13.223574	706.096807	12.691648
12.980360	711.884698	12.696666
13.262188	705.008065	12.701683
13.144750	721.644904	12.706701
13.277933	727.222347	12.711719
13.548888	723.714675	12.716736
13.717810	725.338582	12.721754
13.810656	732.528662	12.726771
14.200086	718.575582	12.731789
13.940681	711.872109	12.736807
13.864376	709.917865	12.741824
13.652092	714.104065	12.746842
13.582764	697.982245	12.751859
13.795787	709.483272	12.756877
13.545014	711.371752	12.761895
14.039312	710.764005	12.766912
13.709785	705.198149	12.771930
13.784646	700.493592	12.776947
13.678834	705.202753	12.781965
13.334714	713.865629	12.786983
13.495762	705.808706	12.792000
13.662117	701.241293	12.797018
13.408783	707.396843	12.802035
13.259390	706.530186	12.807053
13.206449	706.781356	12.812071
13.394163	705.865036	12.817088
13.590848	724.185207	12.822106
13.895308	726.106617	12.827123
13.776655	733.847389	12.832141
13.974043	736.874336	12.837159
14.138665	724.234585	12.842176
14.142356	731.738436	12.847194
14.070397	724.939317	12.852211
13.827420	713.370144	12.857229
13.443353	710.258595	12.862247
13.947017	714.424140	12.867264
13.916280	712.576365	12.872282
13.825922	720.353725	12.877299
14.086020	719.116792	12.882317
13.965796	723.802970	12.887335
14.184848	714.698689	12.892352
13.927379	712.028055	12.897370
13.678455	705.089411	12.902387
13.882173	719.602556	12.907405
14.009311	737.270914	12.912423
14.215171	729.121752	12.917440
14.330663	734.399010	12.922458
14.064476	731.000743	12.927475
14.114156	715.119040	12.932493
13.905247	719.604515	12.937511
14.273397	721.288726	12.942528
14.020858	722.647305	12.947546
13.687078	727.297515	12.952563
14.003270	725.840354	12.957581
13.589886	737.344868	12.962599
14.071087	722.118233	12.967616
14.251020	726.508073	12.972634
13.953185	729.994464	12.977651
14.153113	727.299500	12.982669
13.778138	734.850059	12.987687
13.920277	730.422132	12.992704
14.048525	724.715119	12.997722
14.058761	737.292514	13.002739
14.313537	755.035566	13.007757
14.350584	756.938916	13.012775
14.256317	756.293994	13.017792
14.431831	753.280957	13.022810
14.576537	759.531952	13.027827
14.427332	751.236438	13.032845
14.381701	743.707346	13.037863
14.278084	739.750271	13.042880
14.276572	734.155104	13.047898
14.011115	756.435695	13.052915
14.583493	745.190036	13.057933
14.134362	756.813774	13.062951
14.408847	744.967843	13.067968
14.479100	750.548842	13.072986
14.481650	747.086375	13.078003
14.459605	754.351269	13.083021
14.600268	763.559912	13.088039
14.728498	746.353049	13.093056
14.643512	753.640427	13.098074
15.060552	756.055445	13.103091
14.603229	740.256313	13.108109
14.445782	740.965673	13.113127
14.513920	737.527646	13.118144
14.601822	739.221053	13.123162
14.592068	753.742425	13.128179
14.796586	760.460580	13.133197
14.494253	758.838392	13.138215
14.786485	745.689479	13.143232
14.613239	747.224986	13.148250
14.471963	753.628085	13.153267
14.815530	744.864044	13.158285
14.662317	747.147500	13.163303
14.957562	752.974116	13.168320
14.820591	747.346520	13.173338
14.672842	737.207781	13.178355
14.857377	739.018592	13.183373
14.520759	731.389929	13.188391
14.996677	742.761423	13.193408
14.792751	744.544736	13.198426
14.824191	750.826098	13.203443
14.690306	746.507687	13.208461
15.151143	742.528446	13.213479
14.786650	736.160167	13.218496
14.823453	743.254890	13.223514
14.668748	746.172900	13.228531
14.948353	736.907641	13.233549
14.879114	744.113653	13.238567
14.707663	746.548290	13.243584
14.408759	752.811982	13.248602
14.745646	746.081342	13.253619
14.821456	745.889459	13.258637
14.634076	757.746744	13.263655
14.885832	756.530051	13.268672
14.897165	747.467766	13.273690
14.680859	749.650654	13.278707
15.174973	754.761297	13.283725
14.932041	758.270650	13.288743
15.110225	760.177134	13.293760
15.435096	766.368345	13.298778
15.019461	754.374914	13.303795
15.095088	743.652058	13.308813
14.804568	757.721959	13.313831
15.371218	759.857914	13.318848
15.195838	760.961408	13.323866
15.240952	775.792941	13.328883
15.337042	773.290966	13.333901
15.405471	763.288757	13.338919
15.092472	752.014555	13.343936
14.799287	749.403159	13.348954
15.075574	769.853714	13.353971
15.579611	765.375388	13.358989
15.834804	773.527824	13.364007
15.337583	765.081701	13.369024
15.007241	744.046081	13.374042
15.197443	761.234363	13.379059
15.254232	762.118443	13.384077
15.232928	761.275895	13.389095
15.170419	774.467478	13.394112
15.302888	765.234724	13.399130
15.630545	768.421148	13.404147
15.528652	771.485524	13.409165
15.569676	775.695167	13.414183
15.237376	767.762852	13.419200
15.637053	771.783755	13.424218
15.289682	764.077866	13.429235
15.683236	769.876462	13.434253
15.841213	767.323766	13.439271
15.457242	768.071775	13.444288
15.883669	767.528309	13.449306
15.839190	753.419123	13.454323
15.844105	740.312074	13.459341
15.317097	743.575597	13.464359
15.110244	746.511246	13.469376
15.652922	747.233989	13.474394
15.686421	757.731218	13.479411
15.496513	757.331657	13.484429
15.631951	760.327288	13.489447
15.508836	767.159895	13.494464
15.603494	765.172546	13.499482
15.403288	772.121376	13.504499
15.265472	766.474971	13.509517
15.510581	758.467971	13.514535
15.671257	767.610363	13.519552
15.699862	765.245197	13.524570
15.841711	773.153456	13.529587
15.339540	774.822553	13.534605
15.708056	772.574543	13.539623
15.663467	767.232270	13.544640
16.034134	772.008807	13.549658
15.585736	764.852083	13.554675
15.903021	763.568318	13.559693
15.750612	771.721498	13.564711
15.645323	786.920591	13.569728
16.212502	782.877341	13.574746
15.709934	795.595084	13.579763
15.710663	795.989326	13.584781
16.164045	799.231797	13.589799
15.916165	795.540312	13.594816
16.190679	783.855299	13.599834
16.105614	785.102436	13.604851
16.313609	792.990873	13.609869
16.082919	770.730922	13.614887
15.967605	766.236026	13.619904
15.922319	778.099464	13.624922
16.058653	791.695409	13.629939
16.223107	795.421810	13.634957
16.359145	783.114703	13.639975
15.901252	784.688500	13.644992
16.328696	774.421749	13.650010
15.921362	784.710350	13.655027
15.714108	787.592419	13.660045
15.829207	787.886691	13.665063
15.901972	791.223509	13.670080
15.885539	786.836193	13.675098
16.164480	794.502074	13.680115
16.255995	785.553441	13.685133
16.046955	790.297733	13.690151
15.974733	790.432003	13.695168
16.094580	782.514047	13.700186
16.600884	802.568834	13.705203
16.466980	801.702901	13.710221
16.526554	794.027915	13.715239
16.280660	800.466357	13.720256
16.136120	791.172849	13.725274
16.270689	792.271964	13.730291
16.530554	811.595349	13.735309
16.651612	811.298545	13.740327
16.338555	803.767146	13.745344
16.462406	805.148811	13.750362
16.403449	804.823406	13.755379
16.406401	811.241798	13.760397
16.490745	812.572848	13.765415
16.213777	823.039864	13.770432
16.453147	814.759179	13.775450
16.474275	817.091068	13.780467
16.392310	816.627256	13.785485
16.704843	812.242041	13.790503
16.608047	815.583340	13.795520
16.839685	809.093231	13.800538
16.557365	811.456884	13.805555
16.893888	805.676187	13.810573
16.697876	802.525689	13.815591
16.727928	806.667630	13.820608
17.138740	814.495897	13.825626
16.799602	821.943046	13.830643
16.599043	807.801466	13.835661
16.752870	808.421033	13.840679
16.467552	814.004113	13.845696
16.856601	813.431788	13.850714
16.673073	811.809916	13.855731
16.648249	814.161628	13.860749
16.984158	806.831508	13.865767
16.803869	819.031709	13.870784
16.605869	810.242034	13.875802
16.645320	811.826274	13.880819
16.070126	821.923443	13.885837
16.371483	817.666212	13.890855
16.511451	828.055281	13.895872
16.936802	833.088358	13.900890
17.082431	833.011769	13.905907
17.619849	834.435937	13.910925
17.068033	825.764807	13.915943
17.081914	825.068224	13.920960
17.013515	807.513408	13.925978
16.972301	817.432237	13.930995
16.807984	822.475647	13.936013
17.147714	830.580148	13.941031
16.928210	834.881118	13.946048
16.973357	834.050246	13.951066
17.238521	844.485983	13.956083
17.173263	841.163512	13.961101
17.208217	837.639145	13.966119
17.216670	851.646498	13.971136
17.658081	839.733325	13.976154
17.334499	825.468994	13.981171
17.207681	823.465846	13.986189
17.381104	818.446010	13.991207
16.825718	821.401564	13.996224
16.947896	833.396592	14.001242
17.177314	835.620109	14.006259
17.052930	840.502631	14.011277
17.378430	837.324067	14.016295
17.190905	843.693418	14.021312
17.306069	841.724939	14.026330
17.476201	840.719848	14.031347
17.161021	838.714652	14.036365
17.121820	842.040620	14.041383
17.059121	841.078321	14.046400
17.039607	841.785009	14.051418
17.344569	837.587169	14.056435
17.299535	843.176792	14.061453
17.686882	848.364152	14.066471
17.368195	862.343872	14.071488
17.555196	860.083265	14.076506
17.640013	854.916354	14.081523
17.769139	865.408131	14.086541
17.738865	855.367685	14.091559
17.390795	840.504412	14.096576
17.678999	840.121458	14.101594
17.741488	849.052056	14.106611
17.560542	849.102374	14.111629
17.620405	839.139335	14.116647
17.762616	859.147089	14.121664
17.932632	844.486665	14.126682
18.097167	834.377839	14.131699
17.726595	840.583362	14.136717
17.730655	833.889057	14.141735
17.326551	839.635925	14.146752
17.285236	842.274250	14.151770
17.644079	850.192727	14.156787
17.685575	852.388884	14.161805
18.094303	849.645408	14.166823
18.089693	861.786554	14.171840
18.179832	863.924597	14.176858
17.890056	857.263698	14.181875
17.787191	852.441777	14.186893
17.883038	862.181364	14.191911
18.106138	855.247601	14.196928
17.937826	856.526721	14.201946
18.011788	849.562678	14.206963
18.216018	864.344108	14.211981
17.817591	852.751862	14.216999
17.914899	852.304142	14.222016
17.768211	855.848928	14.227034
17.637185	854.354527	14.232051
17.945618	861.592933	14.237069
17.872006	852.540748	14.242087
17.749600	850.047750	14.247104
17.876800	866.529628	14.252122
18.022361	856.546840	14.257139
17.970403	858.460990	14.262157
17.802134	859.014258	14.267175
18.060492	865.114938	14.272192
18.427840	881.455060	14.277210
18.454319	886.121451	14.282227
18.273429	883.066402	14.287245
18.192595	864.311098	14.292263
18.339628	870.615417	14.297280
18.636873	872.026725	14.302298
18.563212	866.490159	14.307315
18.057048	860.743644	14.312333
18.273128	858.020883	14.317351
18.608278	857.984028	14.322368
18.075296	861.213794	14.327386
18.607277	857.065588	14.332403
18.379748	872.498503	14.337421
18.652179	867.122309	14.342439
18.590215	860.416248	14.347456
18.297948	862.582648	14.352474
18.573618	860.986655	14.357491
18.426739	870.682224	14.362509
18.473537	877.661824	14.367527
18.456220	877.178413	14.372544
18.529378	882.295087	14.377562
18.507885	872.215386	14.382579
18.449685	882.553484	14.387597
18.690987	873.622364	14.392615
18.687571	875.894990	14.397632
18.354060	884.048193	14.402650
18.649129	883.613669	14.407667
18.711140	870.210397	14.412685
18.717155	879.904107	14.417703
18.777324	879.585283	14.422720
18.602729	867.787542	14.427738
18.930423	865.782606	14.432755
18.671574	873.551716	14.437773
18.669632	869.029564	14.442791
18.801319	871.410411	14.447808
18.918377	871.423506	14.452826
19.226067	875.878574	14.457843
18.928443	878.926297	14.462861
18.714180	868.895736	14.467879
19.152178	872.150099	14.472896
18.856918	879.445227	14.477914
18.894466	878.426193	14.482931
18.818495	864.902530	14.487949
18.937087	870.182498	14.492967
18.980971	870.595228	14.497984
18.809211	875.349481	14.503002
19.034184	875.143694	14.508019
18.833367	874.117824	14.513037
19.112691	869.062447	14.518055
18.808218	872.988569	14.523072
18.811505	884.077594	14.528090
19.226745	880.922832	14.533107
19.128702	898.080668	14.538125
19.418211	900.222194	14.543143
19.591090	895.009914	14.548160
19.276591	874.539711	14.553178
19.472545	868.478056	14.558195
19.150813	870.380826	14.563213
19.031528	874.464128	14.568231
18.948084	873.322038	14.573248
19.226732	887.782553	14.578266
19.606258	891.522615	14.583283
19.361886	896.834213	14.588301
19.418269	894.470988	14.593319
19.467191	890.792942	14.598336
18.915051	887.243784	14.603354
19.640720	895.748602	14.608371
19.555797	895.212666	14.613389
19.735364	896.711843	14.618407
19.599757	892.624044	14.623424
19.080621	882.259384	14.628442
19.254897	891.134618	14.633459
19.705450	902.402890	14.638477
19.056069	899.522228	14.643495
19.663808	898.360206	14.648512
19.558053	909.785074	14.653530
19.639212	901.036824	14.658547
19.867056	898.937073	14.663565
19.530778	893.602593	14.668583
19.652713	887.495724	14.673600
19.371292	900.447139	14.678618
19.874532	887.116736	14.683635
19.524117	891.252034	14.688653
19.600693	894.234820	14.693671
19.658760	891.069745	14.698688
19.595060	893.604286	14.703706
19.554290	899.426791	14.708723
19.564687	903.562367	14.713741
19.653827	904.495035	14.718759
19.519343	914.614726	14.723776
20.025103	921.033274	14.728794
19.994238	915.379533	14.733811
20.134038	915.638377	14.738829
20.121248	914.649319	14.743847
20.476152	912.933609	14.748864
19.897670	913.557462	14.753882
19.828161	890.741923	14.758899
19.706848	899.521460	14.763917
20.089754	907.830675	14.768935
20.055317	918.509060	14.773952
19.972663	919.632749	14.778970
20.329897	928.214244	14.783987
20.445803	917.071556	14.789005
20.042555	909.768841	14.794023
20.257982	910.066330	14.799040
20.260160	910.766467	14.804058
20.159876	893.942408	14.809075
20.003635	896.289474	14.814093
20.099518	902.967898	14.819111
20.446513	914.293430	14.824128
20.174766	924.990064	14.829146
20.434307	915.910896	14.834163
20.642765	914.334897	14.839181
19.997967	899.716884	14.844199
20.408439	891.358863	14.849216
20.167087	906.651960	14.854234
20.458062	913.344003	14.859251
20.215020	918.342969	14.864269
20.344534	913.746560	14.869287
20.332417	914.616196	14.874304
20.332655	917.487867	14.879322
20.758396	899.533642	14.884339
19.899725	906.225923	14.889357
20.216125	915.915204	14.894375
20.333410	910.989346	14.899392
20.110996	914.905776	14.904410
20.417857	910.979025	14.909427
20.255865	920.768509	14.914445
20.713853	930.849031	14.919463
20.691169	935.756671	14.924480
20.724250	940.040182	14.929498
20.915271	937.012061	14.934515
20.785040	939.478136	14.939533
21.092536	940.909935	14.944551
20.946835	923.884677	14.949568
20.835263	923.438124	14.954586
20.300368	914.240427	14.959603
20.675012	922.194331	14.964621
21.026094	935.176062	14.969639
20.752422	939.463452	14.974656
20.543445	938.943796	14.979674
20.854631	940.258249	14.984691
21.103220	942.614478	14.989709
20.994556	934.855335	14.994727
21.396108	929.597750	14.999744
21.213991	933.050270	15.004762
20.971089	921.313690	15.009779
20.960729	912.472474	15.014797
20.963905	923.785608	15.019815
21.233630	930.881781	15.024832
21.214247	913.802027	15.029850
20.975484	913.018791	15.034867
21.228700	909.113069	15.039885
20.876143	915.176937	15.044903
21.299488	913.557803	15.049920
21.194347	929.949908	15.054938
21.095612	936.737734	15.059955
21.524012	941.249647	15.064973
21.076496	930.592865	15.069991
21.438402	925.133206	15.075008
21.443858	931.459729	15.080026
20.786981	932.231568	15.085043
21.322554	930.317132	15.090061
20.880222	937.925667	15.095079
21.104405	930.543574	15.100096
21.097366	931.942600	15.105114
21.357617	932.558121	15.110131
21.124049	932.496761	15.115149
21.182509	934.743920	15.120167
21.353185	928.171800	15.125184
21.531725	933.865280	15.130202
21.317820	936.145645	15.135219
21.939041	946.711851	15.140237
21.591504	951.493665	15.145255
21.615423	933.501374	15.150272
21.426473	934.165184	15.155290
21.511930	926.012707	15.160307
21.486399	939.179682	15.165325
21.656374	947.686382	15.170343
21.869339	950.133402	15.175360
21.990049	959.941731	15.180378
21.544397	945.339816	15.185395
21.899835	934.869657	15.190413
22.093047	932.163091	15.195431
21.891416	926.990545	15.200448
21.626099	926.104169	15.205466
21.472424	931.010240	15.210483
21.668845	934.277217	15.215501
21.951386	954.209442	15.220519
21.776920	955.820899	15.225536
21.800634	958.325974	15.230554
22.028868	965.280336	15.235571
21.960469	952.209865	15.240589
22.106940	960.713942	15.245607
22.159493	960.030230	15.250624
22.213102	960.441438	15.255642
22.090956	944.599076	15.260659
22.236202	941.448736	15.265677
21.909151	937.952665	15.270695
22.227401	940.316914	15.275712
21.838119	952.726679	15.280730
22.106308	949.222553	15.285747
22.164145	954.852899	15.290765
22.095557	954.554248	15.295783
22.522150	953.496345	15.300800
22.256524	956.431769	15.305818
22.193122	967.130500	15.310835
22.182354	946.495858	15.315853
21.931602	953.875564	15.320871
21.890549	956.845231	15.325888
22.098229	959.605510	15.330906
21.967938	956.634041	15.335923
22.115839	964.415202	15.340941
22.127341	962.068468	15.345959
22.379537	969.180027	15.350976
22.446462	976.721412	15.355994
22.654326	975.697778	15.361011
22.966678	976.611257	15.366029
22.296261	967.911301	15.371047
22.401606	972.764177	15.376064
22.598717	986.192956	15.381082
22.525368	981.953368	15.386099
22.851798	976.934761	15.391117
22.693610	980.607608	15.396135
22.933013	984.031966	15.401152
23.113819	971.948093	15.406170
22.618406	955.359458	15.411187
22.454952	950.117806	15.416205
22.548355	951.075055	15.421223
22.616848	959.755455	15.426240
22.613726	969.561100	15.431258
22.774105	976.532410	15.436275
23.118917	968.727450	15.441293
22.974749	982.184449	15.446311
23.167960	974.993386	15.451328
23.023848	971.456023	15.456346
22.722528	970.344907	15.461363
23.251212	982.434138	15.466381
23.065553	968.179641	15.471399
22.761112	955.146151	15.476416
23.108977	960.039923	15.481434
23.169529	968.147202	15.486451
22.635020	961.796012	15.491469
22.640034	969.646902	15.496487
22.896127	973.027616	15.501504
22.948259	977.459633	15.506522
22.540272	974.922997	15.511539
22.653664	977.145775	15.516557
22.635112	981.910766	15.521575
23.124032	989.117790	15.526592
23.052520	993.597586	15.531610
22.995214	992.956332	15.536627
23.130382	991.802073	15.541645
23.275994	997.324004	15.546663
23.243633	995.728924	15.551680
23.451138	990.722635	15.556698
23.280423	997.865751	15.561715
23.479787	992.261122	15.566733
23.222921	998.186947	15.571751
22.940962	990.622193	15.576768
23.153652	998.109190	15.581786
23.159695	996.422884	15.586803
23.356084	1000.185350	15.591821
23.989399	1009.228568	15.596839
23.732463	1007.602400	15.601856
23.626148	998.561576	15.606874
23.440298	991.739173	15.611891
23.701790	997.785758	15.616909
23.548934	1001.265266	15.621927
23.440118	994.020528	15.626944
23.695399	1006.506070	15.631962
23.045484	1017.700677	15.636979
23.481285	1012.762757	15.641997
23.653264	1021.966627	15.647015
23.515784	1016.061308	15.652032
23.920621	1012.579943	15.657050
23.692896	1012.577629	15.662067
24.069312	1012.086175	15.667085
24.184396	1011.995436	15.672103
23.866490	1013.279069	15.677120
24.066363	1007.298806	15.682138
23.979539	1010.348238	15.687155
24.170831	1011.271219	15.692173
23.907866	1011.870886	15.697191
23.962999	1010.517723	15.702208
23.910619	1008.357721	15.707226
23.958362	1020.288796	15.712243
24.196108	1008.438980	15.717261
23.723857	1008.560187	15.722279
24.162466	1011.044446	15.727296
24.085210	1010.769243	15.732314
23.553386	1013.787410	15.737331
24.279966	1016.873506	15.742349
24.441715	1035.641294	15.747367
24.759473	1032.586988	15.752384
24.725520	1018.576932	15.757402
24.726595	1014.003776	15.762419
24.329225	998.131902	15.767437
24.477018	1007.415296	15.772455
24.270382	999.210717	15.777472
24.484155	1010.093269	15.782490
24.262022	1000.616145	15.787507
24.407276	1005.573233	15.792525
24.460517	1002.661364	15.797543
24.327039	1003.710970	15.802560
24.538096	1001.433953	15.807578
24.170030	1003.243008	15.812595
24.335488	1009.677036	15.817613
24.513533	1033.034067	15.822631
24.680490	1030.700838	15.827648
24.618070	1032.809154	15.832666
24.487169	1032.977867	15.837683
24.848500	1029.752629	15.842701
25.267068	1036.636172	15.847719
24.521764	1018.278311	15.852736
24.993186	1020.959407	15.857754
24.739246	1013.122004	15.862771
25.049782	1009.128383	15.867789
24.789879	999.114366	15.872807
24.460614	999.181612	15.877824
24.824083	1006.424077	15.882842
24.263305	1028.454625	15.887859
24.624896	1014.448872	15.892877
25.194174	1026.137288	15.897895
24.937278	1030.409448	15.902912
24.929660	1024.632106	15.907930
24.748479	1030.053766	15.912947
25.104787	1027.684559	15.917965
25.118518	1029.853529	15.922983
24.761933	1022.802238	15.928000
24.883035	1020.933797	15.933018
24.747282	1031.659682	15.938035
25.038832	1025.248473	15.943053
25.093423	1036.733508	15.948071
24.980028	1043.132341	15.953088
24.989092	1052.712055	15.958106
25.184425	1052.394143	15.963123
25.234518	1043.597041	15.968141
25.364142	1052.037528	15.973159
25.274898	1050.094740	15.978176
25.493943	1050.861892	15.983194
25.238837	1051.981051	15.988211
25.424168	1051.794096	15.993229
25.204221	1047.558526	15.998247
25.136686	1043.870292	16.003264
25.432305	1043.852255	16.008282
25.068191	1047.371182	16.013299
25.364412	1059.184455	16.018317
25.761093	1066.680525	16.023335
25.551959	1067.101342	16.028352
26.101561	1062.587403	16.033370
25.616331	1054.464319	16.038387
25.520729	1049.212007	16.043405
26.024621	1049.783047	16.048423
25.662911	1063.662365	16.053440
25.715189	1050.497174	16.058458
25.629390	1063.033039	16.063475
25.960603	1065.127024	16.068493
25.959076	1068.109452	16.073511
25.797907	1070.902292	16.078528
25.969942	1058.841827	16.083546
25.895070	1068.115956	16.088563
26.051774	1063.426883	16.093581
26.188142	1064.150183	16.098599
25.959670	1052.815208	16.103616
25.991215	1041.366916	16.108634
25.972091	1052.831952	16.113651
26.190188	1056.991826	16.118669
25.976980	1048.892399	16.123687
25.824362	1065.140584	16.128704
26.336692	1056.744436	16.133722
26.340333	1069.051692	16.138739
26.380803	1063.901136	16.143757
26.249215	1051.765167	16.148775
25.975947	1059.716502	16.153792
26.235589	1051.735497	16.158810
26.111431	1067.477440	16.163827
26.320098	1063.360909	16.168845
26.066740	1059.698630	16.173863
26.005890	1063.794911	16.178880
26.007272	1054.547832	16.183898
26.001376	1066.054986	16.188915
26.123171	1060.235265	16.193933
26.154827	1063.524926	16.198951
25.989314	1076.928535	16.203968
26.844644	1086.233660	16.208986
26.766067	1095.438955	16.214003
26.399727	1080.537316	16.219021
26.809516	1084.260054	16.224039
26.813302	1087.727659	16.229056
26.947628	1073.088420	16.234074
26.453948	1066.475168	16.239091
25.947657	1063.931830	16.244109
26.702362	1073.612485	16.249127
26.365136	1078.484238	16.254144
26.427376	1086.209444	16.259162
26.385608	1077.997934	16.264179
26.683131	1088.709618	16.269197
26.707233	1082.103600	16.274215
26.467014	1089.560608	16.279232
27.175399	1093.157667	16.284250
27.182388	1093.853901	16.289267
27.345640	1088.037143	16.294285
26.968350	1084.135493	16.299303
26.778608	1092.998432	16.304320
26.954302	1084.307867	16.309338
27.013261	1074.448982	16.314355
26.958164	1090.757653	16.319373
27.507069	1106.877028	16.324391
27.065728	1096.020358	16.329408
27.353444	1082.540537	16.334426
27.506812	1086.660066	16.339443
27.413814	1085.172311	16.344461
26.816062	1083.261853	16.349479
27.057224	1093.436402	16.354496
27.304983	1099.608253	16.359514
27.639174	1108.360708	16.364531
27.727023	1109.744882	16.369549
27.699906	1090.608528	16.374567
27.559214	1086.635093	16.379584
27.293189	1082.447761	16.384602
27.008318	1079.623569	16.389619
27.575838	1089.500823	16.394637
27.608375	1096.157686	16.399655
27.843900	1097.947922	16.404672
27.774575	1079.244239	16.409690
27.716046	1082.115677	16.414707
27.547642	1083.988134	16.419725
28.041357	1074.152653	16.424743
27.602785	1078.484848	16.429760
27.686874	1074.782319	16.434778
27.707919	1070.657311	16.439795
27.396210	1080.265207	16.444813
27.916295	1091.841450	16.449831
27.760626	1097.306472	16.454848
27.774493	1091.939163	16.459866
27.807730	1103.392872	16.464883
27.918519	1097.792620	16.469901
27.910753	1103.209223	16.474919
27.807250	1103.496723	16.479936
27.709992	1109.460695	16.484954
27.962133	1107.508596	16.489971
28.158919	1106.000684	16.494989
28.400865	1102.216610	16.500007
28.045046	1106.015124	16.505024
27.879827	1114.766931	16.510042
27.863970	1110.294236	16.515059
28.127166	1112.304207	16.520077
28.420959	1107.186533	16.525095
28.169182	1114.462321	16.530112
28.387437	1105.490514	16.535130
28.477859	1099.808243	16.540147
28.061990	1098.478374	16.545165
28.399430	1102.231387	16.550183
28.155383	1112.639763	16.555200
28.155917	1107.438645	16.560218
28.232259	1108.117701	16.565235
27.964229	1101.314444	16.570253
28.283472	1111.328442	16.575271
28.030838	1121.173264	16.580288
28.173585	1118.544007	16.585306
28.699241	1120.052096	16.590323
28.443397	1132.680926	16.595341
28.594121	1127.989618	16.600359
28.347140	1129.732375	16.605376
28.693718	1123.331445	16.610394
29.057105	1127.762071	16.615411
29.093496	1126.497044	16.620429
29.150823	1120.330788	16.625447
28.779547	1128.755115	16.630464
28.997002	1118.606277	16.635482
29.053604	1126.711092	16.640499
28.353787	1129.967043	16.645517
28.424926	1122.034477	16.650535
28.788427	1131.366191	16.655552
28.875132	1131.620735	16.660570
28.718516	1132.781273	16.665587
28.769411	1138.409609	16.670605
28.664921	1131.908930	16.675623
29.123308	1148.285528	16.680640
29.088358	1149.729972	16.685658
29.574032	1151.711402	16.690675
29.193545	1151.843478	16.695693
29.488456	1140.861959	16.700711
29.105171	1142.742841	16.705728
29.365385	1139.609169	16.710746
29.220023	1131.723142	16.715763
28.731222	1130.300553	16.720781
29.081331	1142.480990	16.725799
29.337974	1135.163157	16.730816
29.399440	1146.148553	16.735834
29.458357	1147.486768	16.740851
29.309839	1150.829921	16.745869
29.522781	1147.356504	16.750887
29.543006	1150.856261	16.755904
29.785394	1142.559173	16.760922
29.845533	1136.111596	16.765939
29.720812	1141.650680	16.770957
29.640242	1136.888307	16.775975
29.394958	1150.194013	16.780992
28.986969	1145.280959	16.786010
29.849078	1146.187210	16.791027
29.614436	1146.968643	16.796045
29.889443	1142.671281	16.801063
29.760852	1145.051917	16.806080
29.665473	1143.195290	16.811098
29.655575	1140.268045	16.816115
29.873453	1142.095765	16.821133
29.690759	1142.200008	16.826151
29.718351	1156.823157	16.831168
29.661998	1167.950107	16.836186
29.865166	1162.016614	16.841203
30.184340	1169.184033	16.846221
30.264358	1155.247534	16.851239
30.163104	1162.790100	16.856256
30.167555	1159.586040	16.861274
29.923033	1155.764561	16.866291
29.848362	1160.147061	16.871309
30.061125	1154.682297	16.876327
29.818635	1162.398474	16.881344
29.583584	1162.930655	16.886362
30.082688	1165.194014	16.891379
30.384319	1186.079746	16.896397
30.697925	1179.810198	16.901415
30.691240	1173.019616	16.906432
30.015424	1168.650307	16.911450
30.601243	1174.642982	16.916467
30.496648	1176.044689	16.921485
30.594156	1174.997308	16.926503
30.833274	1189.057151	16.931520
30.382231	1169.166597	16.936538
30.553716	1171.250906	16.941555
30.554578	1171.806087	16.946573
30.843298	1178.978281	16.951591
30.963364	1183.677426	16.956608
30.773529	1164.295080	16.961626
30.616104	1157.026333	16.966643
30.590286	1172.689843	16.971661
31.062377	1174.916408	16.976679
30.963807	1181.363463	16.981696
30.826326	1173.100631	16.986714
31.092058	1184.577927	16.991731
30.933754	1181.844345	16.996749
31.195745	1182.642645	17.001767
30.842874	1163.651929	17.006784
30.886073	1170.354487	17.011802
31.031308	1176.643418	17.016819
31.054239	1181.572382	17.021837
31.171228	1181.096323	17.026855
31.231283	1184.435207	17.031872
31.013106	1186.476424	17.036890
31.315227	1187.792317	17.041907
31.284108	1187.557221	17.046925
31.219724	1180.340161	17.051943
31.432913	1180.224583	17.056960
31.297205	1181.022075	17.061978
31.445614	1177.331538	17.066995
31.388018	1186.454694	17.072013
31.184004	1179.830731	17.077031
31.578798	1182.362907	17.082048
31.493118	1180.766697	17.087066
31.597131	1177.395550	17.092083
31.487182	1172.192788	17.097101
31.444936	1176.260933	17.102119
31.496401	1176.691418	17.107136
31.590911	1181.855328	17.112154
31.691205	1171.816338	17.117171
31.210301	1177.237664	17.122189
31.429716	1178.774804	17.127207
31.550714	1181.182615	17.132224
31.680900	1199.191791	17.137242
31.767761	1201.488184	17.142259
31.688093	1206.673079	17.147277
31.642541	1201.968320	17.152295
31.900670	1202.584184	17.157312
31.847773	1211.498326	17.162330
32.072871	1201.029498	17.167347
31.995828	1207.375356	17.172365
31.780266	1203.972222	17.177383
32.227392	1193.093058	17.182400
32.156429	1207.794809	17.187418
32.177944	1201.021889	17.192435
32.175123	1204.241236	17.197453
32.175837	1204.878495	17.202471
31.826414	1188.819052	17.207488
32.017245	1213.332533	17.212506
32.148976	1202.610080	17.217523
32.346077	1206.464001	17.222541
31.888815	1212.680078	17.227559
32.263745	1215.407881	17.232576
32.303014	1228.476552	17.237594
32.551409	1212.020456	17.242611
32.417433	1216.191347	17.247629
32.426420	1220.156797	17.252647
32.468854	1230.741271	17.257664
32.335382	1237.963857	17.262682
32.540120	1228.255623	17.267699
32.415281	1219.495310	17.272717
32.683232	1222.694327	17.277735
32.576795	1216.664153	17.282752
32.722192	1222.845773	17.287770
32.442345	1217.010032	17.292787
32.196215	1227.298876	17.297805
32.764064	1241.676497	17.302823
33.059948	1243.719232	17.307840
33.087127	1243.569679	17.312858
33.160653	1248.175143	17.317875
33.254276	1250.199074	17.322893
33.182619	1242.140499	17.327911
33.027165	1228.146158	17.332928
32.894361	1223.562366	17.337946
33.189243	1238.080585	17.342963
33.043903	1240.829945	17.347981
32.767063	1241.586433	17.352999
32.992816	1240.067660	17.358016
32.968164	1237.584538	17.363034
33.316451	1237.185852	17.368051
32.990187	1243.829555	17.373069
32.986124	1242.053288	17.378087
33.455232	1233.162039	17.383104
32.809013	1234.544466	17.388122
33.316773	1245.157031	17.393139
33.668393	1264.166720	17.398157
33.590650	1271.055528	17.403175
33.661088	1262.176233	17.408192
33.668516	1261.139805	17.413210
34.056820	1258.071253	17.418227
33.379489	1238.755738	17.423245
33.433073	1235.802751	17.428263
33.586652	1244.428931	17.433280
33.529873	1251.491179	17.438298
33.997948	1247.447575	17.443315
33.795032	1262.555067	17.448333
33.637822	1255.920586	17.453351
33.962724	1245.874767	17.458368
33.639669	1253.363757	17.463386
33.855634	1250.694606	17.468403
33.938866	1258.113630	17.473421
34.062390	1247.351409	17.478439
33.889694	1250.531105	17.483456
33.802918	1256.468237	17.488474
33.884381	1249.259857	17.493491
34.208134	1253.908171	17.498509
33.910494	1249.034606	17.503527
34.165953	1254.782412	17.508544
34.018000	1262.969833	17.513562
33.788754	1274.748809	17.518579
34.535611	1273.476603	17.523597
34.407289	1275.525843	17.528615
35.090434	1281.367601	17.533632
34.745167	1274.936153	17.538650
34.563096	1253.267607	17.543667
34.621211	1253.435110	17.548685
34.719511	1253.586850	17.553703
34.644218	1249.164459	17.558720
34.279290	1255.770042	17.563738
34.447837	1244.505289	17.568755
34.598554	1248.596868	17.573773
34.295072	1262.457749	17.578791
34.579020	1259.099423	17.583808
34.554410	1274.696559	17.588826
34.572513	1277.953667	17.593843
34.703578	1271.558048	17.598861
34.473130	1283.173110	17.603879
35.140753	1265.777090	17.608896
34.979785	1281.401908	17.613914
35.093714	1280.213088	17.618931
35.284880	1270.939318	17.623949
35.120856	1267.458666	17.628967
35.039313	1270.620928	17.633984
34.978326	1270.497812	17.639002
34.878565	1269.490801	17.644019
34.952595	1276.295870	17.649037
35.073224	1270.684554	17.654055
34.884599	1271.099007	17.659072
34.638325	1277.821712	17.664090
34.877051	1287.974662	17.669107
35.005905	1290.703161	17.674125
35.101857	1287.642538	17.679143
35.336664	1289.391879	17.684160
35.338996	1303.463664	17.689178
35.066001	1301.224578	17.694195
35.138782	1294.500398	17.699213
35.067998	1299.866971	17.704231
35.461005	1310.690066	17.709248
35.691198	1323.378585	17.714266
35.575141	1311.154795	17.719283
35.673041	1311.893601	17.724301
36.284088	1325.380862	17.729319
36.141885	1317.576312	17.734336
35.815535	1303.652871	17.739354
35.843196	1305.106453	17.744371
36.261964	1303.519562	17.749389
35.969481	1293.453677	17.754407
36.179843	1295.156355	17.759424
35.991987	1296.596363	17.764442
35.633190	1289.011961	17.769459
36.151989	1295.299211	17.774477
36.001749	1302.502359	17.779495
36.120680	1297.080657	17.784512
36.109097	1315.260491	17.789530
35.959919	1321.620847	17.794547
36.197238	1315.997546	17.799565
36.346883	1318.176816	17.804583
36.310561	1312.959322	17.809600
36.124818	1319.363278	17.814618
36.379656	1316.956281	17.819635
36.494471	1313.570793	17.824653
36.624367	1321.695772	17.829671
36.531561	1310.838014	17.834688
36.098591	1313.114877	17.839706
36.075121	1312.540897	17.844723
36.376105	1303.966300	17.849741
36.326713	1312.920971	17.854759
36.462776	1303.583231	17.859776
36.227347	1316.609795	17.864794
36.521233	1327.360064	17.869811
36.570182	1331.328746	17.874829
36.882238	1331.813084	17.879847
36.963312	1332.011706	17.884864
36.880508	1331.068309	17.889882
36.547143	1332.881427	17.894899
37.074105	1324.773208	17.899917
36.758913	1324.645736	17.904935
36.929384	1334.541153	17.909952
37.004403	1329.539748	17.914970
37.144337	1330.199382	17.919987
37.152924	1328.553674	17.925005
36.969921	1327.550234	17.930023
37.096644	1331.765516	17.935040
37.128513	1330.359167	17.940058
37.166915	1332.981919	17.945075
37.471832	1332.145039	17.950093
37.172393	1332.567388	17.955111
37.280458	1325.799796	17.960128
36.886047	1334.088982	17.965146
36.870272	1347.829109	17.970163
37.465622	1343.992771	17.975181
37.329422	1354.955614	17.980199
37.480085	1357.238875	17.985216
37.766963	1353.586571	17.990234
37.522846	1361.972147	17.995251
37.851755	1350.978861	18.000269
37.603718	1365.923089	18.005287
37.487961	1362.497974	18.010304
37.721488	1353.564678	18.015322
37.388403	1360.585049	18.020339
37.603968	1358.723865	18.025357
37.595051	1371.143754	18.030375
37.725604	1374.963955	18.035392
38.163804	1385.385522	18.040410
37.702434	1386.540173	18.045427
38.235341	1375.950430	18.050445
38.226492	1373.701509	18.055463
38.294406	1375.003616	18.060480
38.350235	1374.189982	18.065498
37.963950	1379.899514	18.070515
38.515464	1375.479876	18.075533
38.586796	1375.074084	18.080551
38.436644	1377.609615	18.085568
38.584309	1380.332024	18.090586
38.186908	1375.789649	18.095603
38.552373	1371.613765	18.100621
38.818432	1368.996711	18.105639
38.485561	1374.303380	18.110656
38.588999	1370.379998	18.115674
38.526492	1373.081685	18.120691
38.733515	1368.431988	18.125709
38.496349	1375.307943	18.130727
38.699406	1375.597912	18.135744
38.828829	1365.866688	18.140762
38.746843	1373.545185	18.145779
38.608760	1362.199007	18.150797
38.590969	1368.646097	18.155815
38.454077	1373.082580	18.160832
38.949577	1372.985889	18.165850
38.792869	1383.074611	18.170867
39.009948	1374.128102	18.175885
38.475943	1375.653910	18.180903
38.817003	1388.659634	18.185920
38.670482	1390.771701	18.190938
38.758968	1393.670649	18.195955
38.953901	1399.311215	18.200973
38.953450	1400.355781	18.205991
39.153707	1399.194454	18.211008
39.592443	1399.788340	18.216026
39.172115	1400.062365	18.221043
39.645511	1393.739304	18.226061
39.462042	1393.878385	18.231079
39.157358	1396.236149	18.236096
39.324027	1382.109164	18.241114
39.008382	1395.703799	18.246131
39.333638	1408.263869	18.251149
39.562934	1423.398457	18.256167
39.398357	1416.954427	18.261184
39.510339	1417.315473	18.266202
39.300956	1426.967485	18.271219
39.967654	1416.583984	18.276237
39.987467	1415.567698	18.281255
39.952502	1411.268343	18.286272
39.972417	1418.384915	18.291290
39.670307	1423.071369	18.296307
40.043597	1420.989798	18.301325
40.094414	1426.782346	18.306343
39.742315	1420.317200	18.311360
40.065026	1415.103387	18.316378
40.150920	1421.265995	18.321395
40.078076	1421.558164	18.326413
40.207213	1410.476215	18.331431
40.144330	1416.491711	18.336448
40.223049	1416.274118	18.341466
40.181518	1421.901244	18.346483
40.343026	1428.143530	18.351501
40.428266	1444.802938	18.356519
40.460230	1438.719445	18.361536
40.755687	1435.655943	18.366554
40.657710	1444.327944	18.371571
40.711385	1437.991730	18.376589
40.729578	1432.948704	18.381607
40.607556	1444.616313	18.386624
40.937116	1435.323932	18.391642
40.584329	1437.070672	18.396659
40.714318	1426.638705	18.401677
41.062029	1431.693586	18.406695
40.655729	1435.534793	18.411712
41.022390	1429.190571	18.416730
40.830462	1438.123453	18.421747
40.487211	1431.483340	18.426765
40.637755	1434.864900	18.431783
40.603809	1439.853342	18.436800
40.991878	1428.093311	18.441818
40.515977	1432.008541	18.446835
40.897683	1437.247454	18.451853
40.796747	1453.333253	18.456871
40.920088	1460.042299	18.461888
41.222500	1459.953768	18.466906
41.231566	1463.976067	18.471923
41.138550	1461.869716	18.476941
41.327294	1454.032191	18.481959
41.309891	1460.984206	18.486976
41.531695	1465.033137	18.491994
41.300265	1469.620162	18.497011
41.528571	1483.748207	18.502029
41.660709	1480.129588	18.507047
41.385812	1483.388457	18.512064
41.812290	1481.153372	18.517082
41.407349	1483.340654	18.522099
42.135341	1480.322990	18.527117
42.235909	1474.664259	18.532135
42.031127	1480.878741	18.537152
41.856323	1470.734356	18.542170
41.707626	1473.130809	18.547187
41.598537	1475.814562	18.552205
41.407032	1468.513156	18.557223
41.654387	1477.452976	18.562240
41.961445	1477.051277	18.567258
42.411537	1482.516186	18.572275
42.286960	1478.133020	18.577293
42.459102	1474.438704	18.582311
42.141424	1482.043717	18.587328
42.161967	1477.644126	18.592346
41.968172	1487.315819	18.597363
42.333837	1497.717258	18.602381
42.419070	1507.768144	18.607399
42.147960	1506.226204	18.612416
42.607233	1502.733061	18.617434
42.361312	1505.526623	18.622451
42.335737	1505.953406	18.627469
42.337577	1499.637915	18.632487
42.462561	1498.788193	18.637504
42.567384	1498.724307	18.642522
42.633302	1508.509963	18.647539
42.575047	1524.929983	18.652557
43.245792	1522.079080	18.657575
43.009427	1520.288686	18.662592
43.251958	1517.511187	18.667610
43.115866	1509.014440	18.672627
42.962515	1510.247078	18.677645
43.440887	1511.301840	18.682663
43.154291	1503.330475	18.687680
43.168590	1493.254283	18.692698
42.944120	1496.527345	18.697715
42.933954	1511.443893	18.702733
43.248131	1513.692088	18.707751
43.013700	1527.482391	18.712768
43.407375	1516.702930	18.717786
43.596352	1513.106959	18.722803
43.450234	1522.310431	18.727821
43.598339	1518.392643	18.732839
43.624134	1524.646758	18.737856
43.745108	1516.220190	18.742874
43.658361	1516.959530	18.747891
43.594195	1516.776947	18.752909
43.655626	1515.874061	18.757927
43.169393	1517.146230	18.762944
43.892517	1514.902535	18.767962
43.744537	1511.375138	18.772979
43.571136	1517.442698	18.777997
44.150864	1530.360637	18.783015
44.194189	1541.093485	18.788032
44.153533	1538.770627	18.793050
44.214977	1533.354704	18.798067
44.322117	1537.636224	18.803085
43.923173	1524.184755	18.808103
43.910115	1532.063970	18.813120
44.294410	1531.498683	18.818138
44.317511	1539.507943	18.823155
44.319980	1540.697234	18.828173
44.412408	1541.061346	18.833191
44.075561	1536.989148	18.838208
44.345656	1535.933642	18.843226
44.175797	1535.130113	18.848243
44.132408	1538.914482	18.853261
44.327838	1530.747655	18.858279
44.264633	1543.176169	18.863296
44.658718	1544.190488	18.868314
44.632484	1557.689406	18.873331
44.766245	1558.097538	18.878349
44.908076	1562.241077	18.883367
44.796111	1557.849604	18.888384
45.036809	1555.321708	18.893402
45.180435	1554.166088	18.898419
45.293305	1550.619906	18.903437
45.079510	1543.009521	18.908455
45.009922	1551.105896	18.913472
45.201174	1541.465880	18.918490
44.699163	1542.014650	18.923507
45.018761	1557.147827	18.928525
44.990666	1550.862256	18.933543
44.940687	1552.223875	18.938560
45.126116	1555.085569	18.943578
45.257366	1560.089190	18.948595
45.316673	1582.670238	18.953613
45.675935	1573.619298	18.958631
45.358777	1581.669263	18.963648
45.718265	1581.568634	18.968666
45.992106	1587.559834	18.973683
45.434230	1581.647605	18.978701
45.739836	1583.733041	18.983719
46.039391	1582.107997	18.988736
45.915845	1582.070424	18.993754
45.933129	1580.985093	18.998771
45.886919	1589.768981	19.003789
46.041345	1575.776313	19.008807
45.846873	1578.246228	19.013824
45.915998	1580.977818	19.018842
45.675280	1578.698924	19.023859
45.552579	1584.023221	19.028877
45.855790	1566.964887	19.033895
45.704580	1581.862564	19.038912
45.947783	1590.784156	19.043930
45.984259	1598.545180	19.048947
46.057211	1603.027742	19.053965
46.095253	1597.826917	19.058983
46.563504	1597.769211	19.064000
46.484583	1595.891022	19.069018
46.433628	1602.624274	19.074035
46.300998	1607.931198	19.079053
46.306486	1594.103869	19.084071
46.291595	1610.349907	19.089088
46.815288	1619.306466	19.094106
47.058979	1612.722656	19.099123
46.971329	1618.256078	19.104141
47.476220	1606.474472	19.109159
46.938825	1611.526060	19.114176
47.092582	1609.772369	19.119194
47.051464	1598.754851	19.124211
47.080513	1607.479617	19.129229
47.295959	1604.810495	19.134247
47.202086	1607.403516	19.139264
47.111945	1615.569416	19.144282
47.610869	1612.944246	19.149299
47.238908	1618.178211	19.154317
47.328068	1609.908071	19.159335
47.469753	1604.302820	19.164352
47.410600	1605.631165	19.169370
47.825239	1605.730189	19.174387
47.068331	1614.243565	19.179405
47.353929	1608.906115	19.184423
47.536580	1611.986017	19.189440
47.116488	1607.264089	19.194458
47.231312	1601.950242	19.199475
47.335268	1611.745775	19.204493
47.524641	1613.136173	19.209511
47.650448	1632.020679	19.214528
47.713153	1630.925073	19.219546
47.879636	1630.008879	19.224563
47.711984	1641.027320	19.229581
47.731942	1631.174240	19.234599
47.536184	1634.502792	19.239616
47.796248	1639.628272	19.244634
48.028832	1653.121427	19.249651
48.034013	1661.496488	19.254669
48.279016	1657.847527	19.259687
48.268194	1654.200776	19.264704
48.339303	1654.249476	19.269722
48.372948	1653.354093	19.274739
48.547838	1661.914016	19.279757
48.321121	1653.210480	19.284775
48.519257	1656.313211	19.289792
48.249079	1652.249477	19.294810
48.583947	1647.327199	19.299827
48.560092	1654.999865	19.304845
48.620196	1651.840649	19.309863
48.569140	1657.706041	19.314880
48.560865	1669.482215	19.319898
48.959363	1676.435428	19.324915
48.511988	1679.680326	19.329933
48.884591	1678.154289	19.334951
48.850591	1682.180229	19.339968
48.823106	1676.809756	19.344986
49.122534	1680.789767	19.350003
48.933065	1680.727805	19.355021
48.994289	1674.046322	19.360039
49.052437	1677.789564	19.365056
49.049592	1693.667694	19.370074
49.383749	1695.085911	19.375091
49.549180	1702.047245	19.380109
49.765385	1709.193144	19.385127
49.738610	1698.555192	19.390144
49.290630	1701.724446	19.395162
49.890245	1699.484300	19.400179
49.491518	1697.757198	19.405197
49.605908	1696.091723	19.410215
49.424444	1687.071793	19.415232
49.266155	1698.596918	19.420250
49.927800	1691.338489	19.425267
49.796563	1687.868397	19.430285
50.018605	1697.875864	19.435303
49.885321	1701.920519	19.440320
50.096642	1711.995949	19.445338
50.184430	1706.471699	19.450355
50.320965	1716.085449	19.455373
50.394037	1716.698765	19.460391
50.316762	1712.806778	19.465408
50.528528	1717.292868	19.470426
50.425843	1709.081144	19.475443
50.422861	1716.895742	19.480461
50.672788	1717.724362	19.485479
50.937178	1716.985340	19.490496
50.796837	1708.855259	19.495514
50.853902	1704.080639	19.500531
50.712494	1697.654969	19.505549
50.453969	1694.643502	19.510567
50.683440	1689.579927	19.515584
50.244253	1701.234275	19.520602
51.072909	1713.674663	19.525619
50.590925	1718.162142	19.530637
50.619775	1706.556047	19.535655
50.795371	1707.509928	19.540672
50.656531	1706.420647	19.545690
51.000183	1714.076787	19.550707
50.896194	1734.547000	19.555725
50.856396	1736.061682	19.560743
50.949327	1734.143929	19.565760
50.908005	1739.562826	19.570778
51.337318	1745.592841	19.575795
51.144751	1738.685992	19.580813
51.409871	1753.584858	19.585831
51.658311	1759.100383	19.590848
51.393701	1770.607496	19.595866
51.717660	1765.289238	19.600883
51.723837	1771.028927	19.605901
51.762819	1749.631279	19.610919
51.988017	1760.383103	19.615936
51.722641	1761.238808	19.620954
51.783192	1761.033526	19.625971
51.515170	1767.608332	19.630989
51.891370	1758.472590	19.636007
52.087288	1751.056717	19.641024
51.682385	1760.603832	19.646042
51.833629	1749.780159	19.651059
52.122360	1760.203272	19.656077
52.095608	1758.282177	19.661095
51.842947	1763.415436	19.666112
52.148741	1779.466206	19.671130
52.149225	1782.700919	19.676147
52.449466	1779.724978	19.681165
52.494198	1772.900864	19.686183
52.312551	1777.063574	19.691200
52.263497	1784.266842	19.696218
52.307097	1780.775652	19.701235
52.523783	1791.241631	19.706253
52.611860	1804.375663	19.711271
53.158691	1800.433216	19.716288
53.121770	1805.169744	19.721306
53.108761	1799.484521	19.726323
53.017890	1796.923327	19.731341
53.323415	1799.838834	19.736359
53.427238	1793.665062	19.741376
53.238368	1793.038079	19.746394
53.144121	1776.281676	19.751411
53.193055	1782.428108	19.756429
53.121542	1790.307127	19.761447
53.637839	1795.499812	19.766464
53.258815	1797.736722	19.771482
53.335639	1802.815214	19.776499
52.953893	1799.598958	19.781517
53.128699	1801.922678	19.786535
53.493754	1800.123241	19.791552
53.408979	1806.741939	19.796570
53.613865	1807.681769	19.801587
53.633558	1816.739484	19.806605
53.668810	1820.969214	19.811623
53.943991	1824.088308	19.816640
53.739239	1824.659944	19.821658
53.943749	1822.506935	19.826675
53.709660	1825.756315	19.831693
54.148951	1828.300550	19.836711
54.214951	1818.695790	19.841728
53.923298	1824.008756	19.846746
54.294102	1822.041147	19.851763
54.089899	1822.584293	19.856781
54.434556	1840.210194	19.861799
54.611268	1849.625204	19.866816
54.440820	1844.636866	19.871834
54.167469	1846.260738	19.876851
54.437104	1850.857724	19.881869
54.356161	1844.895931	19.886887
54.462421	1842.183917	19.891904
54.535136	1848.856857	19.896922
54.458532	1853.025219	19.901939
55.074323	1851.593620	19.906957
54.750102	1864.334669	19.911975
55.100033	1867.782910	19.916992
55.200892	1869.676381	19.922010
55.072960	1863.008683	19.927027
55.014018	1861.348257	19.932045
54.663772	1864.158219	19.937063
54.966123	1866.158986	19.942080
55.144102	1874.964698	19.947098
55.034600	1874.397866	19.952115
55.383605	1868.371860	19.957133
55.139691	1868.397328	19.962151
55.609628	1868.434039	19.967168
55.269297	1869.150003	19.972186
55.260010	1867.134635	19.977203
55.481962	1877.975407	19.982221
55.452055	1894.972033	19.987239
55.835251	1892.592191	19.992256
55.788561	1898.911446	19.997274
55.681213	1892.325724	20.002291
55.751064	1889.553131	20.007309
55.572921	1889.053862	20.012327
55.850167	1880.567923	20.017344
55.748150	1898.800390	20.022362
56.179666	1902.371565	20.027379
56.232253	1909.120269	20.032397
55.977182	1906.666843	20.037415
56.477738	1902.106730	20.042432
56.434861	1910.631458	20.047450
56.449863	1915.394596	20.052467
56.622449	1917.677651	20.057485
56.291753	1913.014224	20.062503
56.644353	1916.045460	20.067520
56.559402	1921.730042	20.072538
56.262400	1916.149241	20.077555
56.403144	1923.123998	20.082573
56.452966	1939.678954	20.087591
56.960995	1930.434101	20.092608
57.005314	1937.903689	20.097626
56.966888	1945.222129	20.102643
57.097734	1932.454265	20.107661
57.244713	1937.007370	20.112679
57.486840	1932.509830	20.117696
57.298542	1935.218685	20.122714
57.434113	1926.893787	20.127731
57.852631	1921.630102	20.132749
57.601367	1926.520173	20.137767
57.806836	1928.652900	20.142784
57.676005	1941.887607	20.147802
57.411948	1934.531100	20.152819
57.882617	1929.909386	20.157837
57.797161	1928.480343	20.162855
57.732224	1928.121138	20.167872
57.488021	1937.696821	20.172890
57.852377	1934.319461	20.177907
58.045512	1923.504900	20.182925
57.976739	1931.456141	20.187943
57.835383	1925.345985	20.192960
57.593526	1934.290092	20.197978
57.588619	1935.909786	20.202995
58.328541	1940.363680	20.208013
58.187361	1950.999439	20.213031
58.462552	1947.913778	20.218048
58.123336	1943.400012	20.223066
58.391488	1946.911577	20.228083
58.811991	1944.308116	20.233101
58.436534	1946.872714	20.238119
58.447305	1953.258730	20.243136
58.594301	1941.106914	20.248154
58.756201	1950.019331	20.253171
58.670696	1948.473520	20.258189
58.504775	1951.952102	20.263207
58.853198	1955.649923	20.268224
58.940866	1966.189872	20.273242
58.974075	1966.812599	20.278259
59.426792	1965.400229	20.283277
59.085753	1966.665459	20.288295
59.296011	1964.568341	20.293312
59.108793	1971.525067	20.298330
58.947009	1970.145852	20.303347
59.227443	1963.631903	20.308365
59.072604	1971.659766	20.313383
59.218116	1972.097628	20.318400
59.062041	1968.277896	20.323418
59.512729	1979.900309	20.328435
59.743938	1986.128714	20.333453
59.437001	1991.216889	20.338471
59.533863	1992.347236	20.343488
59.761057	1989.294336	20.348506
59.454638	1996.765246	20.353523
59.794962	1991.018292	20.358541
59.535204	1987.883883	20.363559
59.669853	2007.054599	20.368576
59.776453	2015.852626	20.373594
59.914769	2009.095819	20.378611
60.308430	2016.154072	20.383629
59.935805	2019.459908	20.388647
60.189165	2016.440777	20.393664
60.198741	2030.559338	20.398682
60.401543	2035.681280	20.403699
60.977090	2030.351932	20.408717
60.579153	2041.959008	20.413735
60.801907	2033.894978	20.418752
60.643736	2040.676753	20.423770
60.923820	2037.858575	20.428787
60.923241	2030.183016	20.433805
60.572292	2027.110227	20.438823
61.061780	2037.016017	20.443840
61.142280	2032.398597	20.448858
60.992342	2028.486365	20.453875
61.347801	2030.945927	20.458893
61.298847	2037.518069	20.463911
61.009374	2028.619038	20.468928
61.461488	2026.711257	20.473946
61.308413	2024.582688	20.478963
61.568884	2033.848962	20.483981
61.204074	2044.601871	20.488999
61.415239	2046.680066	20.494016
61.402655	2055.960728	20.499034
61.658602	2051.833408	20.504051
61.529407	2055.164233	20.509069
61.424100	2053.466869	20.514087
61.428633	2054.374981	20.519104
61.753799	2074.888806	20.524122
61.471812	2077.091610	20.529139
61.865392	2079.403183	20.534157
61.926793	2067.031144	20.539175
61.791892	2076.858042	20.544192
61.797352	2089.591782	20.549210
61.963104	2099.567264	20.554227
62.845386	2106.599497	20.559245
62.735969	2110.129221	20.564263
62.532249	2101.349274	20.569280
62.291243	2101.740390	20.574298
62.440770	2107.404074	20.579315
62.767152	2096.423355	20.584333
62.501838	2101.397732	20.589351
62.678952	2106.391164	20.594368
62.762362	2111.131012	20.599386
62.673969	2127.114455	20.604403
63.036689	2121.259801	20.609421
62.951188	2122.481849	20.614439
63.078879	2121.590645	20.619456
63.135433	2125.965444	20.624474
63.042510	2128.993929	20.629491
63.126165	2126.190732	20.634509
63.258773	2124.443462	20.639527
63.181992	2119.339377	20.644544
63.186658	2118.486384	20.649562
63.526375	2140.042664	20.654579
63.819228	2151.664669	20.659597
63.467210	2151.359905	20.664615
63.663730	2156.015766	20.669632
63.887235	2148.380795	20.674650
63.732813	2148.300715	20.679667
63.895555	2141.644181	20.684685
64.146341	2146.989031	20.689703
64.028248	2159.533878	20.694720
64.110383	2147.587761	20.699738
64.053988	2145.955315	20.704755
64.228622	2148.430599	20.709773
64.314380	2142.063861	20.714791
64.214414	2144.856746	20.719808
64.596085	2166.081408	20.724826
64.226689	2177.232780	20.729843
64.478749	2166.992716	20.734861
64.430651	2167.148465	20.739879
64.487678	2171.434831	20.744896
64.550181	2180.372404	20.749914
64.591528	2171.560339	20.754931
64.993571	2161.659729	20.759949
64.679558	2184.943864	20.764967
64.984291	2187.130504	20.769984
65.381998	2187.614074	20.775002
65.389576	2199.318677	20.780019
65.072573	2197.802803	20.785037
64.904471	2193.874444	20.790055
65.163330	2192.268347	20.795072
65.607906	2193.700867	20.800090
65.513559	2189.956631	20.805107
65.911634	2190.989301	20.810125
65.516782	2200.039568	20.815143
65.444758	2192.261514	20.820160
65.862290	2190.715772	20.825178
66.006522	2205.479307	20.830195
66.110382	2199.245425	20.835213
65.848709	2200.349900	20.840231
65.998324	2209.905056	20.845248
66.194232	2200.614284	20.850266
66.222017	2209.307980	20.855283
66.206641	2209.423885	20.860301
66.366837	2220.473375	20.865319
66.197199	2214.272869	20.870336
66.541465	2207.076584	20.875354
65.979733	2210.677194	20.880371
66.351500	2204.480238	20.885389
66.385711	2209.515025	20.890407
66.750587	2220.093750	20.895424
66.923083	2222.361078	20.900442
66.641397	2238.908282	20.905459
66.902564	2240.385322	20.910477
66.389800	2241.163032	20.915495
66.656056	2238.659442	20.920512
66.401408	2234.687824	20.925530
66.745992	2243.530736	20.930547
66.661561	2254.366085	20.935565
67.303170	2263.149847	20.940583
67.021712	2273.470072	20.945600
67.398542	2260.357295	20.950618
67.054964	2264.318248	20.955635
67.030312	2265.887411	20.960653
67.078064	2279.962314	20.965671
67.533066	2293.468446	20.970688
67.713538	2293.039224	20.975706
67.611368	2288.693377	20.980723
67.841428	2288.477312	20.985741
68.162062	2293.713423	20.990759
67.887686	2299.269997	20.995776
67.757667	2288.423789	21.000794
67.886942	2296.126391	21.005811
68.304177	2299.889250	21.010829
68.126810	2310.423583	21.015847
68.267683	2315.236542	21.020864
68.362695	2302.975850	21.025882
67.756601	2305.516666	21.030899
68.472131	2300.484075	21.035917
68.419577	2310.190891	21.040935
68.715807	2326.616071	21.045952
68.916202	2327.168431	21.050970
69.070529	2329.867850	21.055987
69.200802	2328.095678	21.061005
69.245351	2319.936352	21.066023
68.868554	2330.053775	21.071040
69.625015	2328.451765	21.076058
68.982200	2321.066069	21.081075
69.751492	2321.589265	21.086093
69.217492	2322.073631	21.091111
69.291985	2326.486698	21.096128
69.327744	2316.883254	21.101146
69.248064	2320.777625	21.106163
69.240948	2318.266357	21.111181
69.512048	2324.892612	21.116199
69.342183	2324.483560	21.121216
69.856948	2332.614978	21.126234
69.940913	2350.146513	21.131251
69.960626	2346.343345	21.136269
70.287930	2351.284910	21.141287
69.900954	2357.174754	21.146304
70.252769	2344.087928	21.151322
70.255266	2345.861148	21.156339
70.214282	2349.099304	21.161357
70.213802	2342.935373	21.166375
69.914384	2349.837232	21.171392
70.087141	2349.024172	21.176410
70.109296	2361.285229	21.181427
70.315607	2366.892757	21.186445
70.421567	2370.997919	21.191463
70.385074	2384.063521	21.196480
70.387234	2373.688906	21.201498
70.759645	2386.311711	21.206515
71.024156	2404.411519	21.211533
71.052853	2391.618304	21.216551
71.086823	2396.280759	21.221568
71.231969	2395.973845	21.226586
71.364557	2392.781050	21.231603
71.643781	2390.218598	21.236621
71.428456	2391.164329	21.241639
71.458561	2394.151489	21.246656
71.782029	2385.396115	21.251674
71.681358	2389.805080	21.256691
71.502788	2387.989761	21.261709
71.722814	2386.263488	21.266727
71.614385	2399.135223	21.271744
71.771975	2406.214837	21.276762
71.657159	2409.417229	21.281779
71.513446	2418.257828	21.286797
72.041253	2407.586222	21.291815
71.481157	2424.126718	21.296832
72.160791	2425.721266	21.301850
72.019998	2435.132674	21.306867
72.106650	2441.519600	21.311885
72.341084	2435.132621	21.316903
72.304396	2440.036554	21.321920
72.576499	2435.903461	21.326938
72.637552	2431.500446	21.331955
72.600176	2431.155849	21.336973
73.008692	2450.666022	21.341991
72.630315	2463.930428	21.347008
72.969807	2462.030779	21.352026
72.818249	2463.048583	21.357043
73.017234	2455.313171	21.362061
73.075366	2457.607915	21.367079
72.275485	2467.435057	21.372096
72.844537	2468.327337	21.377114
73.223945	2476.372719	21.382131
73.022817	2488.249079	21.387149
73.290947	2476.459816	21.392167
73.242192	2492.033387	21.397184
73.563151	2492.361716	21.402202
73.656797	2504.854692	21.407219
73.796200	2495.730429	21.412237
73.742263	2511.405825	21.417255
73.958477	2516.238595	21.422272
73.843198	2506.257884	21.427290
74.156237	2508.320173	21.432307
74.062239	2510.067497	21.437325
74.741996	2521.054708	21.442343
74.599490	2524.056309	21.447360
74.406724	2498.259700	21.452378
74.615027	2508.657977	21.457395
74.545319	2522.315925	21.462413
74.875501	2514.891328	21.467431
74.702338	2535.815149	21.472448
74.862286	2515.742154	21.477466
74.783885	2523.486859	21.482483
75.000004	2517.399399	21.487501
75.076821	2523.794207	21.492519
74.482964	2526.825493	21.497536
74.566674	2526.487172	21.502554
75.215883	2540.433330	21.507571
75.334689	2550.274391	21.512589
75.312966	2551.540130	21.517607
75.048279	2555.652906	21.522624
75.371332	2552.442867	21.527642
75.534688	2557.189245	21.532659
75.439100	2568.099121	21.537677
75.940567	2568.875749	21.542695
75.717446	2573.647964	21.547712
75.869430	2578.481345	21.552730
75.739073	2585.827074	21.557747
76.119687	2586.982438	21.562765
76.206263	2578.349301	21.567783
75.755187	2581.812712	21.572800
76.653726	2599.213712	21.577818
76.660756	2602.182430	21.582835
76.616387	2602.567997	21.587853
76.793060	2600.775904	21.592871
76.698461	2600.089936	21.597888
76.771700	2597.395607	21.602906
76.809198	2599.065527	21.607923
76.886628	2597.181674	21.612941
76.780878	2598.918223	21.617959
76.503562	2593.659209	21.622976
76.913054	2594.134633	21.627994
77.120356	2604.189102	21.633011
77.201760	2608.465441	21.638029
77.239078	2612.846529	21.643047
77.308373	2627.233944	21.648064
77.399004	2639.134128	21.653082
77.638856	2627.907838	21.658099
77.605983	2629.670846	21.663117
77.611797	2628.230604	21.668135
77.702267	2631.262001	21.673152
77.760769	2628.118646	21.678170
78.117546	2620.311100	21.683187
78.088977	2628.856019	21.688205
77.742720	2624.886042	21.693223
77.597681	2626.963302	21.698240
78.367539	2641.389310	21.703258
78.566451	2642.790921	21.708275
78.296213	2645.386472	21.713293
78.119526	2651.549613	21.718311
78.398547	2650.268559	21.723328
78.545799	2655.165826	21.728346
78.249309	2646.778885	21.733363
78.248031	2660.378874	21.738381
78.562858	2671.492787	21.743399
78.704317	2672.584628	21.748416
78.599315	2670.044461	21.753434
78.942101	2681.886231	21.758451
78.604191	2683.236235	21.763469
79.055721	2688.139493	21.768487
79.018862	2702.575161	21.773504
79.284500	2694.718739	21.778522
79.654930	2687.612851	21.783539
79.279830	2696.006943	21.788557
79.548667	2703.126056	21.793575
79.874917	2712.133037	21.798592
79.796996	2706.303044	21.803610
79.897657	2719.735611	21.808627
79.764247	2724.632682	21.813645
79.814354	2716.690082	21.818663
80.254436	2718.631495	21.823680
80.079058	2712.554806	21.828698
79.975631	2714.770741	21.833715
80.020384	2725.447262	21.838733
80.663120	2734.420451	21.843751
80.712442	2734.674564	21.848768
80.744393	2743.806574	21.853786
80.850528	2740.949261	21.858803
80.841792	2739.751159	21.863821
81.114740	2730.959346	21.868839
81.188455	2736.082776	21.873856
80.860034	2734.262494	21.878874
80.756499	2734.130252	21.883891
80.376772	2738.305278	21.888909
80.718972	2749.187706	21.893927
81.045137	2757.942229	21.898944
81.171785	2761.725465	21.903962
81.381830	2752.195481	21.908979
81.442290	2781.049189	21.913997
81.680900	2780.440413	21.919015
82.061454	2785.162291	21.924032
81.866058	2782.778298	21.929050
81.886322	2778.517305	21.934067
81.929736	2777.976985	21.939085
82.159563	2774.630016	21.944103
81.989845	2777.964166	21.949120
82.131372	2786.192142	21.954138
81.974506	2773.869595	21.959155
82.309487	2799.410514	21.964173
82.353044	2799.012200	21.969191
82.630166	2795.771440	21.974208
82.631313	2804.094010	21.979226
82.663717	2805.906776	21.984243
82.579477	2811.215940	21.989261
82.645161	2801.194089	21.994279
82.943138	2804.338190	21.999296
82.685109	2801.528454	22.004314
83.144082	2809.309026	22.009331
82.810132	2824.952816	22.014349
83.309802	2834.920578	22.019367
83.519022	2827.044531	22.024384
83.199291	2838.832392	22.029402
83.489737	2827.329775	22.034419
83.434129	2825.394148	22.039437
83.403624	2824.982187	22.044455
83.314236	2825.624152	22.049472
83.427952	2840.740171	22.054490
83.715312	2848.449805	22.059507
83.757909	2850.185230	22.064525
83.508506	2846.793394	22.069543
84.000736	2864.163623	22.074560
83.850673	2866.661473	22.079578
84.306487	2869.007588	22.084595
84.002769	2870.999269	22.089613
84.668832	2882.724243	22.094631
84.528915	2884.595577	22.099648
84.732161	2895.083245	22.104666
84.845501	2895.990134	22.109683
84.944747	2891.524211	22.114701
85.175196	2896.130763	22.119719
85.392318	2894.900421	22.124736
85.106775	2890.248600	22.129754
85.298082	2884.000781	22.134771
85.177202	2895.467154	22.139789
85.042479	2892.934767	22.144807
85.267688	2902.036580	22.149824
85.481037	2914.122873	22.154842
86.031007	2912.644697	22.159859
85.524682	2905.783398	22.164877
85.649376	2915.405958	22.169895
85.814556	2909.468376	22.174912
85.791974	2915.869428	22.179930
85.879387	2918.610981	22.184947
86.120950	2922.796023	22.189965
86.048252	2934.516838	22.194983
86.572845	2937.622302	22.200000
86.619822	2938.722650	22.205018
86.670442	2932.963976	22.210035
86.286037	2931.294473	22.215053
86.294233	2937.917958	22.220071
86.478295	2936.755918	22.225088
86.636955	2953.907061	22.230106
87.021660	2949.705710	22.235123
87.006704	2963.513225	22.240141
86.916330	2958.000723	22.245159
87.095322	2956.293450	22.250176
86.989763	2962.338241	22.255194
87.243715	2973.171506	22.260211
87.315688	2985.630337	22.265229
87.600438	2995.792828	22.270247
87.703212	2982.776122	22.275264
87.721313	2992.677390	22.280282
87.670686	2984.624205	22.285299
87.334926	2994.681913	22.290317
88.075337	3004.167025	22.295335
87.944247	3008.899686	22.300352
87.720377	3012.576922	22.305370
87.754949	3015.399363	22.310387
88.161746	3014.688480	22.315405
88.485161	3012.721858	22.320423
88.800225	3021.471937	22.325440
88.485116	3028.701604	22.330458
88.675216	3027.011521	22.335475
88.519102	3030.488772	22.340493
88.540069	3034.017186	22.345511
88.970555	3029.111118	22.350528
88.587990	3027.599129	22.355546
88.862528	3023.130961	22.360563
88.691909	3033.172286	22.365581
89.036616	3041.210735	22.370599
89.049425	3045.021334	22.375616
88.895885	3049.763835	22.380634
89.427258	3062.838804	22.385651
89.773963	3069.876426	22.390669
89.628302	3073.181611	22.395687
90.030021	3071.303714	22.400704
89.994628	3085.584803	22.405722
89.834674	3080.064228	22.410739
89.962574	3075.158210	22.415757
89.625205	3070.896366	22.420775
89.823570	3084.957770	22.425792
89.673319	3094.876001	22.430810
90.404378	3094.439406	22.435827
90.322815	3094.815029	22.440845
90.247265	3117.368633	22.445863
90.680680	3124.569441	22.450880
90.581195	3119.531755	22.455898
90.450123	3127.647939	22.460915
90.935277	3117.093070	22.465933
90.919466	3127.053381	22.470951
91.211211	3137.773512	22.475968
91.406249	3146.094269	22.480986
91.946268	3134.410325	22.486003
91.679979	3141.468263	22.491021
91.721015	3149.109305	22.496039
91.966989	3141.281020	22.501056
91.778146	3150.353140	22.506074
91.810420	3146.872929	22.511091
91.753369	3140.550307	22.516109
91.754609	3152.108179	22.521127
92.209693	3140.134538	22.526144
92.008653	3151.155976	22.531162
92.441609	3162.062310	22.536179
92.539969	3173.485042	22.541197
92.599382	3167.245165	22.546215
93.088179	3168.869683	22.551232
92.699201	3169.479690	22.556250
92.412158	3160.538684	22.561267
92.789272	3164.273295	22.566285
92.315788	3163.520414	22.571303
92.926369	3180.026532	22.576320
92.985284	3188.677948	22.581338
93.430004	3185.467675	22.586355
93.250366	3195.794566	22.591373
93.186485	3198.856555	22.596391
93.621537	3182.489355	22.601408
92.938462	3199.021417	22.606426
92.957449	3202.449174	22.611443
93.507790	3212.030457	22.616461
93.317303	3225.884610	22.621479
93.901917	3223.570886	22.626496
94.009707	3243.712944	22.631514
93.901469	3247.198517	22.636531
93.798261	3246.397090	22.641549
94.074027	3249.749908	22.646567
94.525325	3247.498099	22.651584
94.724548	3272.252953	22.656602
94.700326	3264.189195	22.661619
94.994857	3262.293354	22.666637
94.693527	3269.520957	22.671655
94.726185	3272.113330	22.676672
95.109134	3268.249903	22.681690
95.199015	3263.072039	22.686707
94.863439	3269.954662	22.691725
94.696395	3272.833980	22.696743
95.014016	3274.355919	22.701760
95.069176	3283.891725	22.706778
95.293630	3276.357131	22.711795
95.166779	3289.276575	22.716813
95.297321	3296.196651	22.721831
95.421294	3306.419225	22.726848
95.716054	3309.412419	22.731866
95.692230	3321.501424	22.736883
96.175327	3322.785972	22.741901
95.919082	3319.148927	22.746919
96.177908	3327.099958	22.751936
96.226722	3346.336049	22.756954
96.122569	3346.996126	22.761971
96.478614	3346.280558	22.766989
96.652431	3341.686059	22.772007
97.148199	3341.147447	22.777024
96.955887	3347.101801	22.782042
97.011673	3360.945880	22.787059
97.122852	3360.843119	22.792077
97.212719	3372.797564	22.797095
97.358218	3369.258539	22.802112
96.939881	3377.047399	22.807130
97.032840	3376.401454	22.812147
97.701529	3372.922494	22.817165
97.461415	3387.472616	22.822183
97.982349	3398.387405	22.827200
97.771318	3397.097857	22.832218
97.783760	3385.398563	22.837235
97.887962	3381.720816	22.842253
97.749973	3390.191706	22.847271
98.237255	3401.929250	22.852288
98.399058	3404.050058	22.857306
98.547188	3406.365543	22.862323
98.794212	3407.999556	22.867341
98.397338	3407.490321	22.872359
98.842706	3406.429346	22.877376
98.851712	3407.371545	22.882394
98.630905	3404.041405	22.887411
98.822146	3412.489131	22.892429
98.724625	3429.595642	22.897447
98.989825	3433.786570	22.902464
99.557972	3424.679887	22.907482
99.434406	3428.032175	22.912499
99.743729	3445.308528	22.917517
99.905710	3458.192309	22.922535
99.632736	3443.109947	22.927552
100.042367	3449.396129	22.932570
100.130744	3455.994616	22.937587
100.343104	3459.404752	22.942605
100.333186	3456.723324	22.947623
100.177277	3449.295594	22.952640
100.046040	3459.223670	22.957658
100.037470	3452.991189	22.962675
100.627001	3457.345937	22.967693
100.100320	3471.663269	22.972711
100.372753	3482.342443	22.977728
100.769726	3472.899578	22.982746
100.715780	3487.086046	22.987763
100.929662	3491.300808	22.992781
100.909889	3501.059941	22.997799
101.304858	3503.968029	23.002816
101.033334	3502.656388	23.007834
101.150508	3503.824681	23.012851
101.204319	3503.235366	23.017869
100.868334	3514.549609	23.022887
101.635908	3526.896678	23.027904
101.595617	3521.679164	23.032922
101.514458	3532.568424	23.037939
102.363923	3531.854454	23.042957
102.041781	3549.258243	23.047975
102.231509	3547.056848	23.052992
102.353450	3555.152522	23.058010
102.000435	3550.713104	23.063027
102.380909	3539.855602	23.068045
102.186760	3544.557249	23.073063
102.578561	3566.845658	23.078080
102.711946	3572.149356	23.083098
102.834692	3572.010063	23.088115
102.943692	3577.983568	23.093133
102.715001	3571.384679	23.098151
102.751212	3585.045773	23.103168
103.176848	3597.389648	23.108186
103.054094	3602.746110	23.113203
103.784566	3593.967422	23.118221
103.598438	3617.040828	23.123239
103.744136	3622.093262	23.128256
103.760948	3636.499173	23.133274
103.789706	3626.372178	23.138291
104.116190	3623.025693	23.143309
104.067870	3627.881270	23.148327
104.115657	3635.707684	23.153344
104.161865	3640.706271	23.158362
104.015505	3649.876144	23.163379
104.495004	3641.294569	23.168397
104.316681	3651.110187	23.173415
104.890262	3668.367446	23.178432
104.793826	3664.269719	23.183450
104.691652	3668.871767	23.188467
105.292234	3677.236549	23.193485
104.963078	3680.864132	23.198503
105.258320	3695.965053	23.203520
105.741204	3692.379421	23.208538
105.221829	3700.607198	23.213555
105.898013	3695.665615	23.218573
105.795975	3697.000831	23.223591
106.034118	3693.112657	23.228608
106.334322	3690.167976	23.233626
105.821362	3697.106958	23.238643
106.387598	3694.215288	23.243661
106.169703	3718.821472	23.248679
106.435408	3719.884444	23.253696
106.307558	3720.892289	23.258714
106.617162	3720.528026	23.263731
106.779630	3717.058872	23.268749
106.847880	3729.711337	23.273767
106.721676	3746.667980	23.278784
106.948142	3749.245839	23.283802
107.115517	3754.989312	23.288819
107.369076	3742.507112	23.293837
107.149589	3753.405551	23.298855
106.961046	3752.229238	23.303872
107.054374	3773.090645	23.308890
107.346227	3777.444764	23.313907
107.465014	3774.967226	23.318925
107.926000	3790.174827	23.323943
107.869369	3786.850457	23.328960
107.986269	3793.065836	23.333978
107.730717	3791.644354	23.338995
108.170318	3790.404349	23.344013
108.441350	3799.205895	23.349031
108.261562	3805.316254	23.354048
108.574376	3816.282841	23.359066
108.510071	3809.920089	23.364083
108.887157	3822.328539	23.369101
108.899282	3816.607178	23.374119
108.960882	3823.320468	23.379136
109.193461	3837.837928	23.384154
109.386782	3843.858282	23.389171
109.564615	3840.020558	23.394189
109.447985	3845.735958	23.399207
109.465949	3845.439479	23.404224
109.754087	3836.922513	23.409242
109.630726	3838.567247	23.414259
109.711291	3841.344735	23.419277
109.747579	3858.276025	23.424295
110.018786	3855.187511	23.429312
110.050955	3856.839445	23.434330
109.839606	3861.717469	23.439347
110.267349	3880.140387	23.444365
110.647356	3883.079289	23.449383
110.701160	3888.496553	23.454400
110.789464	3893.968384	23.459418
110.650777	3890.776794	23.464435
110.992250	3902.584854	23.469453
111.503761	3905.269585	23.474471
111.171890	3917.514566	23.479488
111.448132	3903.930279	23.484506
111.195240	3907.015686	23.489523
111.522548	3900.335881	23.494541
111.589354	3916.735329	23.499559
111.619130	3939.210326	23.504576
111.724568	3933.291239	23.509594
111.750586	3931.424772	23.514611
111.752170	3932.033583	23.519629
112.049722	3950.233928	23.524647
112.045154	3961.862667	23.529664
112.033548	3958.922605	23.534682
112.223485	3979.627076	23.539699
112.500326	3987.083179	23.544717
112.635968	3985.322630	23.549735
112.759990	3992.266090	23.554752
113.209801	3997.138416	23.559770
113.353957	4004.435398	23.564787
113.195476	4009.611350	23.569805
113.327701	4008.059657	23.574823
113.530399	4009.445002	23.579840
113.736937	4001.013341	23.584858
113.650856	4019.384332	23.589875
113.995742	4021.384995	23.594893
114.234287	4027.404638	23.599911
113.863387	4031.749020	23.604928
114.535465	4032.514772	23.609946
114.333329	4036.703303	23.614963
114.419417	4017.962749	23.619981
114.290549	4023.774814	23.624999
114.009490	4043.419999	23.630016
114.420942	4049.974401	23.635034
114.585758	4065.339108	23.640051
114.856412	4075.343440	23.645069
115.051451	4082.215836	23.650087
115.097333	4085.734239	23.655104
115.235796	4075.984358	23.660122
115.386521	4088.958733	23.665139
115.291192	4088.837819	23.670157
115.709026	4100.807648	23.675175
115.518325	4110.344531	23.680192
115.757289	4098.637696	23.685210
115.874894	4097.467056	23.690227
115.515917	4114.305846	23.695245
115.577684	4123.468602	23.700263
116.125061	4134.622740	23.705280
116.143414	4129.702036	23.710298
116.583040	4140.636328	23.715315
116.461917	4149.770935	23.720333
116.722461	4149.853094	23.725351
116.366939	4156.786521	23.730368
116.838180	4161.791261	23.735386
117.119969	4164.925514	23.740403
117.433313	4171.867789	23.745421
117.263614	4167.405811	23.750439
116.853305	4173.375649	23.755456
117.468214	4181.814177	23.760474
117.638869	4195.341036	23.765491
117.639566	4200.504730	23.770509
117.866567	4202.467066	23.775527
117.928059	4210.686136	23.780544
118.486143	4219.253528	23.785562
118.583444	4223.202647	23.790579
118.743614	4215.368405	23.795597
118.660457	4224.468694	23.800615
118.898618	4220.362611	23.805632
119.104783	4217.391546	23.810650
119.059623	4222.335166	23.815667
118.668911	4223.311622	23.820685
119.207008	4232.516596	23.825703
119.384424	4241.077352	23.830720
119.685927	4237.930369	23.835738
119.513231	4249.932841	23.840755
119.701431	4248.044089	23.845773
119.686345	4242.655127	23.850791
119.676260	4264.249812	23.855808
119.717572	4277.980072	23.860826
120.140242	4271.316756	23.865843
120.154593	4277.608340	23.870861
120.252917	4273.953430	23.875879
119.863370	4295.686513	23.880896
119.917404	4299.579298	23.885914
120.700561	4308.711197	23.890931
121.112333	4321.285005	23.895949
121.291129	4323.668403	23.900967
121.176743	4338.777220	23.905984
121.438279	4331.331074	23.911002
121.565841	4321.371287	23.916019
121.613564	4326.556057	23.921037
121.539359	4328.865459	23.926055
121.310841	4334.702705	23.931072
121.672033	4341.321904	23.936090
121.903434	4345.398394	23.941107
122.073758	4344.629820	23.946125
122.227309	4355.814230	23.951143
121.724386	4377.656710	23.956160
122.162784	4379.314491	23.961178
122.326697	4371.485909	23.966195
122.581484	4383.740300	23.971213
122.479769	4392.963525	23.976231
122.399476	4409.373837	23.981248
122.766567	4411.895040	23.986266
122.876369	4416.075821	23.991283
123.165718	4434.041202	23.996301
123.083810	4429.732698	24.001319
123.190054	4444.450356	24.006336
123.747400	4447.042765	24.011354
123.354350	4451.179232	24.016371
123.618519	4447.024833	24.021389
123.863180	4458.368639	24.026407
124.165086	4461.272525	24.031424
124.617136	4473.054165	24.036442
124.593070	4474.718122	24.041459
124.205721	4479.851150	24.046477
124.672574	4472.076071	24.051495
124.599000	4479.322131	24.056512
124.709119	4485.223162	24.061530
124.730349	4490.371095	24.066547
124.749247	4499.114632	24.071565
125.608396	4488.437250	24.076583
125.182866	4492.742952	24.081600
125.202253	4509.058825	24.086618
125.511271	4527.248484	24.091635
125.609713	4526.784717	24.096653
126.090237	4520.538374	24.101671
126.142437	4528.746417	24.106688
126.072419	4538.286713	24.111706
126.426508	4549.509268	24.116723
126.404513	4548.742406	24.121741
126.830545	4551.421689	24.126759
126.656104	4554.071943	24.131776
126.917830	4545.833400	24.136794
126.677667	4544.800851	24.141811
126.505916	4564.950295	24.146829
126.836490	4569.323792	24.151847
126.707376	4566.417823	24.156864
127.136735	4580.832451	24.161882
127.268765	4586.531222	24.166899
127.340959	4596.229189	24.171917
127.564059	4614.785924	24.176935
127.536690	4613.862076	24.181952
127.982835	4624.000200	24.186970
127.952992	4623.534433	24.191987
128.186716	4653.127853	24.197005
128.324446	4632.462572	24.202023
128.194440	4644.594346	24.207040
128.288923	4652.265527	24.212058
128.827567	4656.798995	24.217075
128.931250	4661.249095	24.222093
128.998014	4670.477632	24.227111
129.227731	4665.754095	24.232128
129.261502	4680.246560	24.237146
129.624564	4684.652873	24.242163
129.266495	4694.279413	24.247181
130.003387	4694.672044	24.252199
129.808233	4685.075112	24.257216
129.949605	4703.739438	24.262234
130.145660	4713.743184	24.267251
130.296274	4724.827274	24.272269
130.326302	4731.624759	24.277287
130.179637	4716.347938	24.282304
130.110577	4728.675393	24.287322
130.665724	4727.366722	24.292339
130.618938	4743.680547	24.297357
130.936043	4757.260639	24.302375
130.866568	4770.415198	24.307392
130.978503	4773.333115	24.312410
131.520198	4779.264481	24.317427
131.388595	4783.467384	24.322445
131.680059	4785.040902	24.327463
132.074743	4801.048874	24.332480
131.914869	4792.090293	24.337498
132.208005	4781.128945	24.342515
132.117646	4803.765877	24.347533
132.317908	4811.988731	24.352551
132.395809	4823.747145	24.357568
132.424299	4820.150415	24.362586
132.721431	4820.656136	24.367603
132.702039	4827.938038	24.372621
133.000515	4837.300811	24.377639
132.998041	4849.662108	24.382656
133.071069	4851.497124	24.387674
133.140618	4846.391439	24.392691
132.895221	4862.225125	24.397709
133.229513	4860.897385	24.402727
133.218642	4873.159004	24.407744
133.600464	4884.535249	24.412762
133.898960	4893.863326	24.417779
133.872813	4905.032035	24.422797
134.115714	4898.327213	24.427815
134.496139	4916.351404	24.432832
134.451627	4927.901791	24.437850
134.605224	4929.818890	24.442867
134.711171	4925.259879	24.447885
134.917820	4925.846067	24.452903
135.184220	4951.473371	24.457920
135.137785	4956.392137	24.462938
135.384559	4955.201207	24.467955
135.655239	4967.352493	24.472973
135.544516	4961.009235	24.477991
135.558893	4975.160907	24.483008
135.331281	4986.209713	24.488026
135.857619	4985.246448	24.493043
135.923085	4999.428014	24.498061
136.350974	4991.595689	24.503079
136.081744	5003.768452	24.508096
136.027187	5018.303432	24.513114
136.381700	5025.081758	24.518131
137.046753	5037.278629	24.523149
137.256363	5040.073963	24.528167
137.042005	5050.909241	24.533184
137.113296	5060.070977	24.538202
137.425106	5055.823750	24.543219
137.222720	5054.261260	24.548237
137.745436	5064.188770	24.553255
137.764387	5080.312672	24.558272
137.692916	5078.852776	24.563290
138.013675	5088.998179	24.568307
137.963410	5099.438457	24.573325
138.479225	5095.588556	24.578343
138.244970	5101.524799	24.583360
138.717786	5116.106657	24.588378
139.082446	5120.134036	24.593395
139.191024	5141.749050	24.598413
139.307911	5123.867441	24.603431
139.513388	5122.746102	24.608448
139.171308	5123.235181	24.613466
139.768722	5143.719312	24.618483
139.757279	5157.553198	24.623501
140.163122	5149.354938	24.628519
140.286263	5150.184648	24.633536
139.738534	5158.266001	24.638554
139.863655	5157.274043	24.643571
140.466030	5168.054039	24.648589
140.511820	5172.412324	24.653607
140.601574	5182.069972	24.658624
140.516763	5184.621046	24.663642
140.564992	5197.571234	24.668659
140.632214	5195.628736	24.673677
140.967951	5208.758009	24.678695
141.163352	5216.672460	24.683712
141.043917	5226.890058	24.688730
141.055137	5230.893918	24.693747
141.289446	5254.222349	24.698765
141.497554	5261.740251	24.703783
142.176410	5270.958428	24.708800
142.062984	5284.982001	24.713818
142.250304	5278.055314	24.718835
142.086698	5290.012852	24.723853
142.306213	5283.059024	24.728871
142.743445	5297.409855	24.733888
142.689964	5312.569913	24.738906
142.669748	5316.793368	24.743923
142.602593	5320.809526	24.748941
142.937981	5335.498319	24.753959
143.113931	5332.070940	24.758976
143.110985	5347.728171	24.763994
143.374773	5356.793610	24.769011
143.585497	5364.001794	24.774029
143.841106	5370.609502	24.779047
144.378624	5379.196453	24.784064
144.259078	5384.713923	24.789082
144.299498	5382.706159	24.794099
144.561279	5387.876636	24.799117
144.472640	5400.649542	24.804135
145.011174	5404.640275	24.809152
144.670932	5415.760648	24.814170
144.951185	5417.989404	24.819187
144.795737	5439.071624	24.824205
145.051528	5430.350647	24.829223
145.511542	5443.627922	24.834240
145.701558	5456.975915	24.839258
145.793466	5462.545511	24.844275
146.067160	5463.140154	24.849293
146.368018	5480.397676	24.854311
146.569880	5484.810500	24.859328
146.337291	5501.936961	24.864346
146.347215	5485.867895	24.869363
146.365240	5499.356503	24.874381
146.953753	5505.826877	24.879399
147.010671	5511.026327	24.884416
146.943538	5521.198016	24.889434
147.101172	5535.589682	24.894451
147.768622	5538.152376	24.899469
147.621429	5544.646479	24.904487
148.011065	5543.234261	24.909504
147.950467	5550.387169	24.914522
148.326479	5567.670880	24.919539
148.546990	5563.229499	24.924557
148.764552	5568.536379	24.929575
148.803049	5565.458784	24.934592
148.634133	5574.554241	24.939610
149.005436	5580.515723	24.944627
148.890857	5589.994101	24.949645
149.029200	5594.003379	24.954663
149.090666	5597.377583	24.959680
149.123486	5622.976134	24.964698
149.135927	5617.266785	24.969715
149.629809	5625.270390	24.974733
149.750362	5647.966869	24.979751
150.101483	5644.688764	24.984768
149.880448	5651.314427	24.989786
150.179228	5660.554466	24.994803
150.083748	5665.405346	24.999821
150.312767	5676.240980	25.004839
150.779824	5689.785650	25.009856
151.028607	5703.437129	25.014874
151.332309	5704.974088	25.019891
151.503473	5702.150319	25.024909
151.197359	5709.572191	25.029927
151.568021	5716.613408	25.034944
151.486717	5720.268851	25.039962
151.661082	5728.792906	25.044979
151.739199	5743.345558	25.049997
152.065366	5751.062979	25.055015
152.664811	5743.616987	25.060032
152.446076	5756.116949	25.065050
152.203832	5748.701802	25.070067
152.675203	5758.331537	25.075085
152.757928	5776.501076	25.080103
153.084129	5760.416943	25.085120
153.060874	5785.257427	25.090138
153.050430	5787.257137	25.095155
153.356113	5790.826714	25.100173
153.434846	5799.659358	25.105191
153.838523	5806.114603	25.110208
153.656345	5829.108114	25.115226
153.816650	5826.409139	25.120243
154.269929	5834.381316	25.125261
153.997655	5845.109338	25.130279
154.491108	5848.008695	25.135296
154.745440	5858.909920	25.140314
154.564688	5871.353502	25.145331
154.888886	5874.036312	25.150349
154.853397	5891.697312	25.155367
155.579408	5895.661941	25.160384
155.382575	5905.835223	25.165402
155.421460	5903.695059	25.170419
155.534408	5907.825184	25.175437
155.304752	5934.674318	25.180455
155.846173	5929.961604	25.185472
156.149047	5946.856227	25.190490
156.245425	5956.112341	25.195507
156.564495	5962.214715	25.200525
156.694279	5977.580211	25.205543
156.837449	5980.073582	25.210560
157.096443	5979.521492	25.215578
156.886054	5988.790958	25.220595
157.332830	5995.028016	25.225613
157.383350	6003.833611	25.230631
157.387265	6014.752063	25.235648
157.984128	6026.619355	25.240666
157.940829	6031.029682	25.245683
158.171305	6039.826043	25.250701
158.151172	6062.273595	25.255719
158.675920	6062.267026	25.260736
158.671618	6068.019188	25.265754
158.754881	6065.657394	25.270771
159.265085	6078.703140	25.275789
159.051721	6090.069211	25.280807
159.281163	6084.685591	25.285824
159.516544	6100.997459	25.290842
159.313206	6111.556998	25.295859
160.097267	6114.079412	25.300877
159.618511	6119.681788	25.305895
159.917060	6116.582301	25.310912
159.972129	6137.250376	25.315930
160.148465	6139.710162	25.320947
160.495001	6159.110930	25.325965
160.535524	6165.244382	25.330983
160.872052	6168.525092	25.336000
160.876431	6183.219073	25.341018
161.123675	6201.044425	25.346035
161.338055	6197.134192	25.351053
161.446838	6203.184357	25.356071
161.747922	6217.049002	25.361088
161.953022	6220.151433	25.366106
161.865046	6220.247169	25.371123
161.938390	6227.887600	25.376141
161.998983	6247.345885	25.381159
162.408511	6244.702509	25.386176
162.488925	6266.004429	25.391194
162.841555	6270.876814	25.396211
162.969742	6272.122483	25.401229
163.061899	6273.361169	25.406247
163.279706	6283.131924	25.411264
163.448616	6297.026806	25.416282
163.363988	6297.270387	25.421299
163.800396	6296.046508	25.426317
163.458017	6320.142199	25.431335
163.898978	6323.501280	25.436352
163.786873	6339.346926	25.441370
164.039459	6343.502625	25.446387
164.689433	6352.694311	25.451405
164.520200	6364.321966	25.456423
164.504899	6366.410890	25.461440
164.652471	6381.710803	25.466458
164.936919	6391.862620	25.471475
165.290369	6408.361458	25.476493
165.285950	6419.480335	25.481511
165.312025	6433.126211	25.486528
165.687090	6435.482297	25.491546
165.545859	6438.579043	25.496563
165.723969	6451.187774	25.501581
166.265410	6469.803857	25.506599
166.319723	6480.866217	25.511616
166.715241	6487.442943	25.516634
166.942781	6489.945264	25.521651
167.051124	6502.441844	25.526669
167.239305	6516.084484	25.531687
167.428685	6513.642872	25.536704
167.928446	6527.306157	25.541722
168.213870	6523.324746	25.546739
168.512836	6535.886191	25.551757
168.184507	6542.131220	25.556775
168.464179	6540.673020	25.561792
168.660908	6534.868221	25.566810
168.161998	6562.129804	25.571827
168.769840	6558.524048	25.576845
168.909098	6568.218869	25.581863
168.495171	6580.345894	25.586880
169.289504	6588.277600	25.591898
168.998342	6606.585457	25.596915
169.489355	6613.800735	25.601933
169.965790	6635.846040	25.606951
170.158805	6636.191345	25.611968
170.395084	6646.032008	25.616986
170.846002	6653.032603	25.622003
170.994370	6650.284869	25.627021
170.632331	6651.443207	25.632039
170.803571	6657.057562	25.637056
171.131440	6675.552626	25.642074
171.154683	6682.888566	25.647091
171.150513	6678.327431	25.652109
171.094963	6695.471465	25.657127
171.243929	6705.215347	25.662144
171.506141	6711.096429	25.667162
171.626428	6728.370790	25.672180
171.908986	6733.554180	25.677197
172.225531	6748.395435	25.682215
172.260668	6754.400496	25.687232
172.656430	6767.357330	25.692250
172.673485	6784.502700	25.697268
172.916286	6783.659535	25.702285
172.965851	6802.510858	25.707303
173.183062	6807.934959	25.712320
173.589288	6814.083945	25.717338
173.640422	6834.289359	25.722356
174.072438	6838.262374	25.727373
173.998246	6844.142532	25.732391
173.768442	6854.135245	25.737408
174.154997	6860.918708	25.742426
174.457393	6873.056823	25.747444
174.652430	6871.933860	25.752461
174.493315	6892.393258	25.757479
174.642314	6893.522061	25.762496
175.020428	6908.634764	25.767514
174.939729	6922.180925	25.772532
175.027286	6925.147202	25.777549
175.151471	6941.259412	25.782567
176.013595	6950.326615	25.787584
176.099548	6964.200272	25.792602
176.050859	6972.968207	25.797620
176.599851	6977.184951	25.802637
176.547644	6988.068576	25.807655
176.663241	6994.837712	25.812672
176.745271	7006.079148	25.817690
176.931293	7026.838200	25.822708
177.094936	7016.220972	25.827725
177.296297	7042.233911	25.832743
177.470783	7048.854937	25.837760
177.838791	7053.396803	25.842778
177.881457	7078.778014	25.847796
178.106866	7074.660668	25.852813
178.059974	7092.450885	25.857831
178.480851	7107.601250	25.862848
178.872875	7109.882159	25.867866
179.017401	7129.375583	25.872884
179.177606	7134.619295	25.877901
179.081973	7135.256071	25.882919
179.106968	7159.408955	25.887936
179.547471	7162.045324	25.892954
179.721545	7178.689764	25.897972
180.090145	7182.698045	25.902989
179.962396	7194.098738	25.908007
180.185615	7208.910789	25.913024
180.471340	7214.630501	25.918042
180.699785	7227.973765	25.923060
180.995966	7241.656850	25.928077
181.345212	7241.387341	25.933095
181.289159	7242.851357	25.938112
181.613265	7258.215895	25.943130
181.419901	7279.151474	25.948148
181.501679	7278.709193	25.953165
181.623093	7301.227635	25.958183
181.814537	7309.658198	25.963200
181.934760	7329.853331	25.968218
182.220974	7347.645279	25.973236
182.755015	7357.206059	25.978253
182.869452	7358.390818	25.983271
182.968893	7376.521437	25.988288
183.471766	7384.259222	25.993306
183.273145	7400.090921	25.998324
183.894614	7404.403749	26.003341
183.776448	7410.534064	26.008359
183.802410	7420.136589	26.013376
184.358378	7424.349188	26.018394
184.019989	7439.110498	26.023412
184.603295	7451.100808	26.028429
184.797676	7471.628591	26.033447
184.697374	7469.620546	26.038464
185.233495	7482.947365	26.043482
185.218939	7493.594928	26.048500
185.155191	7504.884762	26.053517
185.492959	7521.172382	26.058535
185.886472	7526.067112	26.063552
186.052066	7540.863201	26.068570
186.174124	7551.833511	26.073588
186.098685	7547.365407	26.078605
186.310890	7567.110723	26.083623
186.642784	7580.820036	26.088640
186.788719	7585.744096	26.093658
187.038101	7604.710159	26.098676
187.216756	7606.434195	26.103693
187.145944	7622.012441	26.108711
187.378367	7628.915046	26.113728
187.733333	7645.035916	26.118746
187.788292	7655.675840	26.123764
188.420302	7664.387977	26.128781
188.717239	7675.728750	26.133799
188.503896	7688.270217	26.138816
189.056807	7698.838471	26.143834
189.102710	7696.577033	26.148852
189.124938	7721.776065	26.153869
189.423084	7719.149933	26.158887
189.366791	7723.442733	26.163904
189.803641	7739.850777	26.168922
189.880437	7747.241892	26.173940
189.989769	7759.928594	26.178957
190.364000	7769.824017	26.183975
190.192979	7784.341545	26.188992
190.422580	7796.895778	26.194010
190.486453	7802.969291	26.199028
190.829189	7814.688135	26.204045
191.206217	7829.047230	26.209063
191.467226	7850.865706	26.214080
191.931196	7851.114918	26.219098
192.020207	7867.444972	26.224116
191.925663	7878.509392	26.229133
192.381665	7882.718816	26.234151
192.334727	7906.798705	26.239168
192.984342	7900.224818	26.244186
192.743558	7920.155131	26.249204
192.698190	7928.474694	26.254221
193.254853	7934.774131	26.259239
193.497347	7952.990247	26.264256
193.671918	7962.680271	26.269274
193.459754	7969.857862	26.274292
193.512600	7983.443864	26.279309
193.973807	7990.512817	26.284327
194.238437	8017.505388	26.289344
194.787504	8018.255879	26.294362
194.793224	8040.326097	26.299380
195.140830	8051.946459	26.304397
195.201750	8059.438056	26.309415
195.326701	8078.537755	26.314432
195.436406	8079.148709	26.319450
195.750347	8094.575523	26.324468
196.236406	8099.222283	26.329485
196.049048	8111.965177	26.334503
196.512447	8131.346563	26.339520
196.569873	8134.491397	26.344538
196.577252	8136.987393	26.349556
196.766060	8160.560272	26.354573
197.110677	8173.886021	26.359591
197.120805	8187.355738	26.364608
197.213366	8197.658585	26.369626
197.842458	8213.127684	26.374644
198.043412	8225.030013	26.379661
198.178241	8228.014353	26.384679
198.489926	8251.599669	26.389696
198.619948	8252.220075	26.394714
198.655294	8263.163348	26.399732
198.757967	8276.132433	26.404749
199.448716	8276.099870	26.409767
199.431346	8298.578126	26.414784
199.241507	8300.022141	26.419802
199.723917	8305.566154	26.424820
199.720320	8318.037302	26.429837
199.918318	8323.878446	26.434855
200.244951	8343.025752	26.439872
200.278869	8352.548586	26.444890
200.350813	8362.381182	26.449908
200.693084	8383.622427	26.454925
200.656746	8388.849929	26.459943
201.276863	8409.031073	26.464960
201.428703	8412.435837	26.469978
201.422300	8417.257699	26.474996
201.623768	8447.818911	26.480013
201.891304	8451.694918	26.485031
201.999283	8459.829681	26.490048
202.437428	8473.279910	26.495066
202.701877	8492.743357	26.500084
202.694266	8502.547448	26.505101
203.254153	8519.356816	26.510119
203.115009	8533.623676	26.515136
203.662348	8526.974035	26.520154
203.916124	8549.179644	26.525172
203.524377	8565.134150	26.530189
203.926717	8577.049358	26.535207
204.404210	8583.683455	26.540224
204.488186	8595.976897	26.545242
204.784609	8605.401908	26.550260
205.087023	8616.322495	26.555277
205.482204	8625.877277	26.560295
205.484916	8642.199432	26.565312
205.690932	8651.910149	26.570330
205.816282	8654.397205	26.575348
205.359114	8674.772661	26.580365
206.259005	8681.956276	26.585383
205.904776	8703.505904	26.590400
206.394912	8719.944359	26.595418
206.684048	8721.275485	26.600436
206.750531	8750.803834	26.605453
207.213089	8760.370231	26.610471
207.477195	8771.764179	26.615488
207.651331	8780.640137	26.620506
208.126422	8791.669537	26.625524
207.981117	8811.620578	26.630541
208.401994	8814.503371	26.635559
208.626491	8827.898926	26.640576
208.598890	8842.388499	26.645594
208.821788	8849.785582	26.650612
208.747798	8869.993878	26.655629
209.301726	8869.022953	26.660647
209.492858	8890.114808	26.665664
209.636710	8898.171527	26.670682
209.676296	8908.555685	26.675700
209.856713	8929.043072	26.680717
210.446627	8935.681785	26.685735
210.582571	8953.994510	26.690752
210.744506	8963.747025	26.695770
211.233400	8975.850996	26.700788
210.994553	8994.216159	26.705805
211.155446	8999.637100	26.710823
211.708590	9022.708826	26.715840
211.769431	9037.857193	26.720858
212.013648	9037.064226	26.725876
212.026713	9066.478312	26.730893
212.299154	9073.195224	26.735911
212.545850	9082.846121	26.740928
212.769393	9105.432847	26.745946
213.055755	9123.456963	26.750964
212.911525	9126.276784	26.755981
213.666455	9135.317667	26.760999
213.639801	9150.265137	26.766016
213.624687	9161.598876	26.771034
213.950593	9173.479084	26.776052
213.798551	9187.218041	26.781069
214.537302	9192.472740	26.786087
214.655755	9211.119973	26.791104
214.887254	9228.710764	26.796122
215.289684	9236.856572	26.801140
215.273076	9252.247729	26.806157
215.864782	9266.031255	26.811175
215.971307	9280.301247	26.816192
216.319712	9298.745207	26.821210
216.472469	9297.344568	26.826228
216.437960	9309.818066	26.831245
216.580629	9316.615386	26.836263
216.615456	9328.392898	26.841280
216.700737	9346.003550	26.846298
217.135937	9351.937310	26.851316
217.390672	9371.621057	26.856333
217.693781	9388.250427	26.861351
218.043871	9409.321127	26.866368
217.846692	9410.005461	26.871386
218.296701	9425.686755	26.876404
218.364881	9448.623442	26.881421
218.918071	9452.394922	26.886439
219.234864	9476.745071	26.891456
219.388666	9488.447215	26.896474
219.396501	9499.660743	26.901492
219.708827	9517.116009	26.906509
220.174140	9521.880047	26.911527
220.325065	9539.764759	26.916544
220.404029	9558.677429	26.921562
220.676574	9561.359406	26.926580
220.346674	9585.754173	26.931597
220.780631	9598.470213	26.936615
221.150838	9613.545326	26.941632
220.787944	9635.899356	26.946650
221.723191	9653.380304	26.951668
221.676084	9667.731492	26.956685
221.880242	9679.482700	26.961703
222.384765	9700.816859	26.966720
222.590059	9720.565552	26.971738
222.910830	9728.844350	26.976756
223.006249	9757.845638	26.981773
222.997615	9762.636623	26.986791
223.508004	9778.021435	26.991808
223.740786	9787.933784	26.996826
224.244529	9801.639924	27.001844
224.342410	9820.369924	27.006861
224.341461	9823.053738	27.011879
225.079686	9849.125442	27.016896
224.723722	9848.407519	27.021914
225.195014	9861.774630	27.026932
225.329180	9879.813849	27.031949
225.752925	9899.714798	27.036967
226.066211	9906.927643	27.041984
225.698679	9931.054060	27.047002
226.021806	9934.416485	27.052020
226.401930	9948.931453	27.057037
226.594640	9961.341376	27.062055
227.073764	9984.937395	27.067072
227.120331	10002.974669	27.072090
227.680660	10008.993235	27.077108
227.748618	10024.251798	27.082125
227.606853	10039.663211	27.087143
227.717262	10050.027438	27.092160
228.159362	10060.825956	27.097178
228.626493	10077.824928	27.102196
228.498357	10090.578840	27.107213
228.866517	10104.858996	27.112231
229.323969	10109.772818	27.117248
229.577546	10131.377276	27.122266
229.595641	10133.196167	27.127284
229.791414	10144.835314	27.132301
229.974413	10158.917181	27.137319
230.519399	10170.608992	27.142336
230.734623	10189.128375	27.147354
230.845810	10199.868301	27.152372
231.199866	10206.639147	27.157389
231.308520	10223.085018	27.162407
231.557068	10231.009088	27.167424
231.689985	10238.294522	27.172442
231.949332	10258.635236	27.177460
232.164878	10266.030878	27.182477
232.265303	10281.609785	27.187495
232.467416	10298.543121	27.192512
232.412650	10313.874824	27.197530
232.899028	10332.193997	27.202548
232.963183	10350.999278	27.207565
233.484880	10367.996282	27.212583
233.937076	10382.162447	27.217600
233.754975	10393.946197	27.222618
234.120213	10419.654026	27.227636
234.608919	10427.335320	27.232653
234.926409	10442.858255	27.237671
235.206590	10458.980659	27.242688
235.073739	10473.453253	27.247706
235.527283	10487.496143	27.252724
235.513199	10504.684560	27.257741
236.047919	10506.561487	27.262759
236.305256	10530.079269	27.267776
236.265759	10543.324807	27.272794
236.670925	10560.640206	27.277812
236.849835	10579.064624	27.282829
237.093302	10598.448308	27.287847
237.532719	10602.247321	27.292864
237.599064	10630.367252	27.297882
237.860432	10630.638781	27.302900
237.940213	10656.918962	27.307917
237.887013	10664.836808	27.312935
237.967671	10685.297547	27.317952
238.580821	10708.968213	27.322970
238.630622	10722.897706	27.327988
238.893704	10739.853466	27.333005
239.252984	10760.381155	27.338023
239.660642	10775.722891	27.343040
239.933317	10797.243030	27.348058
240.071099	10808.073866	27.353076
240.245404	10828.867424	27.358093
240.521582	10853.440446	27.363111
241.048639	10862.113705	27.368128
241.012174	10891.971011	27.373146
241.552252	10897.926730	27.378164
241.745331	10929.955285	27.383181
241.733930	10939.208672	27.388199
242.252147	10943.746917	27.393216
242.124427	10967.417139	27.398234
242.701843	10974.011183	27.403252
242.974240	10989.036421	27.408269
242.855017	11009.617238	27.413287
243.147459	11027.127554	27.418304
243.593842	11050.827935	27.423322
244.130234	11068.019047	27.428340
244.489244	11074.562085	27.433357
244.028450	11081.893490	27.438375
244.401666	11095.750492	27.443392
244.929368	11111.073699	27.448410
245.061578	11130.061714	27.453428
245.221053	11136.452890	27.458445
245.137166	11150.116299	27.463463
245.729159	11154.744083	27.468480
245.653704	11180.853543	27.473498
246.449336	11191.982567	27.478516
246.597613	11212.000692	27.483533
246.415676	11228.780313	27.488551
247.074520	11242.633729	27.493568
247.173741	11255.501225	27.498586
247.112301	11257.860011	27.503604
247.968534	11279.803983	27.508621
247.690939	11300.053114	27.513639
247.991182	11312.459719	27.518656
248.457692	11331.231371	27.523674
249.100803	11342.330697	27.528692
249.190612	11368.250330	27.533709
248.756229	11393.554272	27.538727
249.217818	11399.490872	27.543744
249.486174	11415.129671	27.548762
250.047245	11439.696725	27.553780
249.979743	11453.534617	27.558797
250.192026	11474.130322	27.563815
250.700798	11492.687109	27.568832
250.836095	11508.289992	27.573850
251.417842	11533.662296	27.578868
251.252680	11549.618576	27.583885
251.503268	11566.993856	27.588903
252.115576	11573.825790	27.593920
252.100691	11601.170475	27.598938
252.553232	11618.160505	27.603956
252.966060	11626.002593	27.608973
253.044891	11646.922533	27.613991
253.487988	11649.000237	27.619008
253.473812	11676.427021	27.624026
253.777886	11685.255588	27.629044
254.137233	11707.634722	27.634061
254.301565	11715.241054	27.639079
254.728424	11730.116381	27.644096
254.889960	11765.353228	27.649114
254.996167	11765.541719	27.654132
255.286908	11781.572033	27.659149
255.328377	11810.035502	27.664167
255.838034	11830.272398	27.669184
256.044053	11842.229926	27.674202
256.345289	11856.957673	27.679220
256.383362	11874.028649	27.684237
256.825407	11899.407543	27.689255
256.777185	11912.765932	27.694272
257.198748	11930.970516	27.699290
257.483877	11950.743789	27.704308
258.101445	11969.773457	27.709325
257.836481	11985.483645	27.714343
258.068179	12010.061991	27.719360
258.355283	12030.166604	27.724378
258.857992	12055.330950	27.729396
259.271583	12070.874915	27.734413
259.394408	12089.398018	27.739431
259.999007	12108.275127	27.744448
260.050404	12122.019097	27.749466
260.231992	12125.293571	27.754484
260.736078	12143.220179	27.759501
260.581249	12167.594025	27.764519
260.967641	12186.619075	27.769536
261.298459	12198.686750	27.774554
261.340291	12214.873263	27.779572
262.034720	12225.702978	27.784589
261.432699	12248.375455	27.789607
262.109062	12263.884732	27.794624
262.246460	12276.803786	27.799642
262.653048	12298.023621	27.804660
263.052965	12313.544667	27.809677
263.113508	12334.461918	27.814695
263.600675	12340.666384	27.819712
263.645425	12374.555326	27.824730
263.808612	12383.185244	27.829748
264.241037	12403.662219	27.834765
263.871740	12429.888910	27.839783
264.626957	12454.174250	27.844800
264.818322	12474.704853	27.849818
265.162937	12502.199788	27.854836
265.361558	12509.930542	27.859853
265.185906	12536.575460	27.864871
266.068061	12554.345342	27.869888
266.392749	12578.477234	27.874906
266.562296	12596.857728	27.879924
266.902355	12606.296874	27.884941
266.671885	12643.504117	27.889959
267.022450	12663.814200	27.894976
267.534283	12685.327456	27.899994
267.964385	12704.905127	27.905012
268.156340	12725.546436	27.910029
268.583380	12740.125692	27.915047
269.039439	12759.361460	27.920064
269.170826	12773.184951	27.925082
269.433508	12794.453151	27.930100
269.916282	12812.686893	27.935117
270.040223	12835.198979	27.940135
270.534448	12857.280454	27.945152
270.350978	12859.538554	27.950170
270.318194	12887.162642	27.955188
271.156257	12900.300786	27.960205
270.972094	12925.125467	27.965223
271.675809	12936.285721	27.970240
271.990719	12953.674309	27.975258
272.135044	12976.505478	27.980276
272.523194	12997.413195	27.985293
272.737971	13020.779703	27.990311
273.216426	13032.047933	27.995328
273.335187	13057.008494	28.000346
273.722153	13080.502842	28.005364
274.129467	13088.340091	28.010381
274.131310	13110.262147	28.015399
274.242138	13128.406035	28.020416
274.662867	13148.358272	28.025434
274.867002	13155.782105	28.030452
275.446096	13172.488445	28.035469
275.277776	13199.644736	28.040487
275.578369	13219.786397	28.045504
276.026055	13235.903891	28.050522
276.126082	13266.665696	28.055540
276.691092	13286.728113	28.060557
276.687307	13305.783832	28.065575
277.381686	13321.107997	28.070592
277.372530	13333.144388	28.075610
277.712450	13367.080449	28.080628
278.226873	13382.189688	28.085645
277.993046	13405.759579	28.090663
278.371287	13418.692213	28.095680
279.000881	13435.422455	28.100698
279.203608	13453.801741	28.105716
279.411092	13468.659119	28.110733
279.710681	13496.175183	28.115751
279.996020	13506.397065	28.120768
280.277732	13524.732467	28.125786
280.442858	13539.356527	28.130804
281.033465	13551.902287	28.135821
280.994838	13568.743639	28.140839
281.623880	13586.380454	28.145856
281.640193	13598.195120	28.150874
281.353284	13615.789121	28.155892
281.939159	13627.107197	28.160909
282.191910	13649.871664	28.165927
282.236580	13670.451807	28.170944
282.893199	13693.288856	28.175962
282.763330	13720.351440	28.180980
283.376936	13735.063300	28.185997
283.452408	13756.311377	28.191015
284.120499	13786.385006	28.196032
284.124187	13806.330630	28.201050
284.195433	13833.036590	28.206068
284.671098	13847.375387	28.211085
284.557043	13874.479926	28.216103
284.958594	13899.239392	28.221120
285.739019	13917.793910	28.226138
285.756846	13942.629333	28.231156
285.940965	13965.714421	28.236173
286.573420	13999.242605	28.241191
286.753896	14018.058581	28.246208
286.771997	14035.927316	28.251226
287.142186	14062.005678	28.256244
287.421033	14080.528393	28.261261
287.654815	14107.221909	28.266279
287.919683	14137.652963	28.271296
288.663777	14164.055026	28.276314
288.841185	14189.866897	28.281332
289.080001	14209.277126	28.286349
289.675597	14234.799323	28.291367
289.763237	14250.336137	28.296384
290.212460	14260.665395	28.301402
290.394512	14294.100431	28.306420
290.759227	14312.736247	28.311437
290.870643	14331.010674	28.316455
291.094996	14359.022969	28.321472
291.252169	14385.507804	28.326490
291.503528	14407.872309	28.331508
292.270094	14430.231930	28.336525
292.496525	14456.017533	28.341543
292.262813	14482.746908	28.346560
293.023170	14499.340754	28.351578
293.369755	14523.645391	28.356596
293.792342	14539.543693	28.361613
294.160221	14564.918830	28.366631
294.099481	14577.403076	28.371648
294.600471	14597.855892	28.376666
294.774520	14619.699020	28.381684
295.232568	14633.804306	28.386701
295.629979	14667.319956	28.391719
295.456388	14689.574498	28.396736
295.755521	14703.717362	28.401754
296.274819	14728.222595	28.406772
296.682142	14749.195561	28.411789
296.710890	14778.515033	28.416807
297.156694	14798.499817	28.421824
297.520685	14819.040653	28.426842
297.718535	14846.359846	28.431860
298.157988	14862.145237	28.436877
298.449776	14872.796365	28.441895
298.691264	14911.926956	28.446912
299.079821	14926.570772	28.451930
298.858095	14948.785781	28.456948
299.496129	14968.036340	28.461965
299.654571	14990.501355	28.466983
299.691571	15007.812185	28.472000
300.358693	15028.173115	28.477018
300.612472	15052.786681	28.482036
300.992243	15064.892730	28.487053
301.317955	15086.674736	28.492071
301.809999	15110.720464	28.497088
302.156317	15120.185150	28.502106
302.024495	15147.919617	28.507124
302.365649	15170.495187	28.512141
302.892493	15194.927197	28.517159
302.728698	15213.627732	28.522176
303.130200	15235.356977	28.527194
303.638206	15260.445790	28.532212
304.070810	15284.178900	28.537229
304.164625	15304.285676	28.542247
304.146148	15333.679719	28.547264
304.982462	15351.693130	28.552282
305.069904	15379.409376	28.557300
305.431731	15409.018737	28.562317
306.015949	15427.226466	28.567335
306.234261	15453.662145	28.572352
306.764791	15473.315371	28.577370
306.744634	15487.448823	28.582388
307.063322	15505.963522	28.587405
307.178933	15533.204984	28.592423
307.612020	15554.275865	28.597440
307.981626	15572.188882	28.602458
308.300578	15600.453479	28.607476
308.602745	15626.118253	28.612493
309.108307	15646.495676	28.617511
309.258775	15669.730220	28.622528
310.049946	15685.615958	28.627546
309.723872	15714.041771	28.632564
310.312111	15735.578097	28.637581
310.590388	15758.735877	28.642599
310.280005	15787.023529	28.647616
311.200222	15814.281481	28.652634
311.108104	15847.989582	28.657652
311.730146	15868.491123	28.662669
312.111324	15901.585092	28.667687
311.950505	15927.376487	28.672704
312.411618	15940.787408	28.677722
312.775643	15978.227019	28.682740
313.319606	15997.161717	28.687757
313.747588	16023.764318	28.692775
313.422861	16050.980738	28.697792
314.074119	16072.349649	28.702810
314.330684	16100.204681	28.707828
314.902554	16123.689608	28.712845
314.888844	16149.113985	28.717863
315.144088	16171.694716	28.722880
315.671189	16197.827214	28.727898
316.008100	16226.800572	28.732916
316.508977	16254.661777	28.737933
317.078103	16283.434605	28.742951
317.381326	16317.719612	28.747968
317.537273	16322.732834	28.752986
317.619315	16357.412625	28.758004
318.388851	16371.479878	28.763021
318.577409	16403.091967	28.768039
318.671866	16422.574431	28.773056
319.007601	16442.780317	28.778074
319.282917	16470.389744	28.783092
319.491078	16492.975068	28.788109
320.086899	16516.532528	28.793127
320.133162	16545.507675	28.798144
320.759501	16561.543144	28.803162
321.209643	16574.251878	28.808180
321.227263	16602.296675	28.813197
321.527050	16625.490032	28.818215
321.881103	16645.026812	28.823232
322.049902	16660.088560	28.828250
322.551436	16693.089233	28.833268
322.579545	16713.855275	28.838285
322.999364	16729.000939	28.843303
322.998666	16758.795509	28.848320
323.518629	16783.625440	28.853338
323.886550	16817.386357	28.858356
324.243301	16837.102947	28.863373
324.274124	16862.499177	28.868391
324.524904	16896.818697	28.873408
325.128996	16921.847253	28.878426
325.493730	16951.929162	28.883444
325.484287	16993.219546	28.888461
326.131918	17011.867367	28.893479
326.412181	17043.946248	28.898496
327.094544	17067.623487	28.903514
327.308216	17087.767046	28.908532
327.495266	17122.842381	28.913549
328.018678	17138.231147	28.918567
327.834113	17167.824569	28.923584
328.458943	17197.202809	28.928602
328.657472	17226.660505	28.933620
329.170304	17254.868732	28.938637
329.821466	17283.175361	28.943655
329.599031	17320.867375	28.948672
330.265327	17338.388113	28.953690
330.533614	17367.462376	28.958708
330.831123	17395.028586	28.963725
331.341924	17423.243695	28.968743
331.636091	17449.149051	28.973760
332.018895	17475.653339	28.978778
332.322637	17506.168926	28.983796
332.505361	17535.566395	28.988813
333.345775	17566.825586	28.993831
333.352680	17598.752367	28.998848
333.547366	17614.072974	29.003866
334.001323	17638.266814	29.008884
334.679038	17664.017617	29.013901
335.138808	17694.142651	29.018919
334.899108	17721.616588	29.023936
335.204464	17746.130757	29.028954
335.680842	17774.294914	29.033972
336.094849	17794.275161	29.038989
336.536244	17815.565168	29.044007
336.758144	17853.308646	29.049024
336.969663	17872.859519	29.054042
337.127954	17906.822586	29.059060
337.485728	17925.188187	29.064077
337.972956	17951.784167	29.069095
338.430252	17987.943248	29.074112
339.229421	18008.419325	29.079130
339.164810	18042.960852	29.084148
339.352287	18067.146429	29.089165
339.864228	18076.005417	29.094183
340.043499	18111.039536	29.099200
340.494436	18132.315761	29.104218
340.841983	18166.224367	29.109236
341.155139	18188.002370	29.114253
341.929771	18213.694501	29.119271
341.983528	18234.546600	29.124288
342.319632	18260.307484	29.129306
342.426980	18292.137542	29.134324
343.017196	18311.427374	29.139341
343.548731	18335.489897	29.144359
343.730532	18357.124408	29.149376
343.930406	18377.290422	29.154394
344.530678	18397.671714	29.159412
344.748653	18425.946787	29.164429
345.048205	18448.618002	29.169447
345.118709	18463.162708	29.174464
345.605894	18491.383072	29.179482
346.036485	18506.926457	29.184500
346.292155	18541.159674	29.189517
346.627029	18564.261410	29.194535
346.751661	18586.145203	29.199552
346.765070	18614.484181	29.204570
347.368618	18628.332698	29.209588
347.411183	18667.931665	29.214605
347.912143	18698.797298	29.219623
348.213351	18732.082376	29.224640
348.677976	18772.045050	29.229658
349.045289	18803.058138	29.234676
348.847885	18837.097498	29.239693
349.769532	18861.453361	29.244711
350.154089	18898.655329	29.249728
350.133044	18930.828749	29.254746
350.755894	18958.327263	29.259764
351.050858	19000.041744	29.264781
351.478379	19024.746879	29.269799
351.792629	19054.865228	29.274816
351.945728	19091.105599	29.279834
352.737915	19111.963008	29.284852
353.414310	19152.480852	29.289869
353.876839	19176.112974	29.294887
353.871045	19197.266053	29.299904
354.092918	19220.980150	29.304922
354.872666	19254.102709	29.309940
355.112934	19290.051807	29.314957
355.456925	19319.142402	29.319975
356.053592	19346.380212	29.324992
355.947256	19375.737287	29.330010
356.384291	19409.052787	29.335028
356.682187	19435.503550	29.340045
357.402021	19469.236066	29.345063
357.369654	19499.864290	29.350080
357.888627	19527.297744	29.355098
358.239942	19553.525488	29.360116
358.780038	19586.243889	29.365133
359.100250	19614.738437	29.370151
359.339776	19627.779117	29.375168
359.397269	19658.936865	29.380186
360.094148	19695.788164	29.385204
360.198123	19735.455490	29.390221
360.357485	19753.834942	29.395239
361.093669	19792.790503	29.400256
361.114533	19824.636605	29.405274
361.881533	19854.628405	29.410292
362.207746	19893.825292	29.415309
362.642514	19926.781896	29.420327
363.032822	19949.541728	29.425344
363.444315	19986.236096	29.430362
363.871999	20007.675967	29.435380
363.906938	20044.340972	29.440397
364.460706	20069.874288	29.445415
364.663660	20100.839362	29.450432
365.242778	20131.979336	29.455450
365.807124	20150.491587	29.460468
366.090642	20184.748593	29.465485
366.298602	20207.846881	29.470503
366.752167	20229.775762	29.475520
366.855403	20262.797498	29.480538
367.419713	20285.246144	29.485556
367.388773	20313.872531	29.490573
367.978651	20345.560847	29.495591
368.598668	20365.145004	29.500608
368.729147	20395.704890	29.505626
368.988125	20421.461751	29.510644
368.903912	20466.075659	29.515661
369.904137	20486.762950	29.520679
370.221230	20516.826238	29.525696
370.355037	20548.226176	29.530714
370.997399	20574.517108	29.535732
371.274190	20599.551122	29.540749
371.421453	20632.086387	29.545767
371.899212	20664.955359	29.550784
372.186964	20699.970803	29.555802
372.543423	20725.813888	29.560820
372.991583	20763.508588	29.565837
373.307463	20787.443636	29.570855
373.910268	20812.369989	29.575872
373.882173	20847.725817	29.580890
374.826313	20881.937425	29.585908
375.093421	20912.647310	29.590925
375.316815	20940.868300	29.595943
375.773515	20972.414208	29.600960
375.791626	21013.626631	29.605978
376.533792	21048.021809	29.610996
376.859018	21082.393896	29.616013
377.083449	21112.826444	29.621031
377.718750	21148.363231	29.626048
378.085943	21178.451275	29.631066
378.540507	21198.011632	29.636084
378.414346	21229.744028	29.641101
379.074836	21264.582039	29.646119
379.960912	21294.867000	29.651136
379.965428	21327.729064	29.656154
380.790073	21355.420488	29.661172
380.989684	21389.256750	29.666189
381.047711	21416.796641	29.671207
381.727105	21450.456758	29.676224
381.953447	21492.067228	29.681242
382.710792	21517.349386	29.686260
382.670721	21554.174278	29.691277
382.964161	21575.921227	29.696295
383.327048	21607.792461	29.701312
383.354589	21645.775885	29.706330
384.030255	21679.203186	29.711348
384.243498	21714.472212	29.716365
384.523830	21750.451126	29.721383
385.289570	21791.295315	29.726400
385.660434	21830.558568	29.731418
386.106062	21861.393615	29.736436
386.347062	21896.393230	29.741453
387.161836	21927.612872	29.746471
387.301123	21956.214975	29.751488
387.391970	22000.122496	29.756506
388.268252	22035.300875	29.761524
388.736842	22062.189706	29.766541
389.122360	22093.571629	29.771559
389.414161	22125.897150	29.776576
389.515326	22162.018614	29.781594
390.081867	22192.133845	29.786612
390.643866	22215.280129	29.791629
390.486800	22248.213261	29.796647
391.172181	22278.537489	29.801664
391.645375	22318.284872	29.806682
391.968329	22342.271247	29.811700
392.257538	22379.147195	29.816717
392.726995	22422.522429	29.821735
393.140427	22443.272102	29.826752
393.499700	22481.982395	29.831770
393.935311	22504.839187	29.836788
394.112804	22528.128211	29.841805
394.374057	22563.328037	29.846823
394.885876	22584.725939	29.851840
395.649355	22634.248181	29.856858
395.579709	22659.560233	29.861876
396.004945	22692.472400	29.866893
396.503908	22732.311361	29.871911
396.944944	22771.097877	29.876928
396.983682	22809.606254	29.881946
397.646499	22835.429387	29.886964
398.229383	22858.389899	29.891981
398.283502	22902.109275	29.896999
398.866917	22936.646349	29.902016
399.360502	22984.473989	29.907034
399.901132	23012.300689	29.912052
400.222209	23052.060729	29.917069
400.467244	23077.102852	29.922087
401.340546	23106.590063	29.927104
401.503133	23156.921790	29.932122
401.715307	23177.242456	29.937140
402.167939	23208.065860	29.942157
402.287690	23252.641451	29.947175
403.117307	23284.720317	29.952192
403.317666	23322.679876	29.957210
403.805440	23357.744518	29.962228
404.020032	23387.152064	29.967245
404.396307	23426.379708	29.972263
405.148577	23464.139342	29.977280
405.359722	23510.508500	29.982298
405.840162	23550.402554	29.987316
406.305652	23583.366762	29.992333
406.696289	23612.936644	29.997351
407.200417	23651.070423	30.002368
407.241070	23694.534551	30.007386
407.710179	23723.909046	30.012404
408.265532	23758.527773	30.017421
408.723387	23805.705766	30.022439
409.528042	23842.370980	30.027456
409.591945	23879.379786	30.032474
410.160002	23913.870406	30.037492
410.701361	23946.083959	30.042509
410.855159	23986.390253	30.047527
411.720499	24013.270134	30.052544
412.126257	24049.239877	30.057562
412.515127	24082.368577	30.062580
412.750890	24108.001154	30.067597
412.603136	24156.538725	30.072615
413.614448	24179.079764	30.077632
413.578665	24220.597967	30.082650
413.887253	24262.687947	30.087668
414.519578	24292.227297	30.092685
414.990462	24342.715943	30.097703
415.413508	24372.604169	30.102720
415.601466	24412.267694	30.107738
415.730490	24451.378087	30.112756
416.588829	24484.598227	30.117773
416.870531	24528.860592	30.122791
417.274740	24561.311485	30.127808
417.796598	24608.373910	30.132826
418.068143	24642.975426	30.137844
418.524315	24682.433163	30.142861
419.174191	24723.800772	30.147879
419.414945	24755.316993	30.152896
419.780880	24797.727735	30.157914
420.261344	24830.584218	30.162932
420.878449	24866.408569	30.167949
421.053128	24904.375147	30.172967
421.619425	24940.529894	30.177984
421.901458	24977.936299	30.183002
422.113334	25005.968944	30.188020
422.594928	25037.005502	30.193037
423.110919	25080.840561	30.198055
423.516584	25121.330874	30.203072
423.282413	25163.659429	30.208090
424.013917	25191.926932	30.213108
424.603319	25234.998772	30.218125
424.890696	25278.004254	30.223143
425.640564	25319.237350	30.228160
425.729612	25356.725245	30.233178
426.244576	25398.778959	30.238196
426.842526	25440.402650	30.243213
427.168096	25482.840118	30.248231
427.530692	25516.329212	30.253248
428.141642	25572.866115	30.258266
428.485821	25608.070944	30.263284
428.959157	25650.517219	30.268301
429.231699	25699.435071	30.273319
429.291960	25735.607307	30.278336
429.961251	25791.977686	30.283354
430.313304	25844.207749	30.288372
431.355889	25871.428922	30.293389
431.426576	25922.729976	30.298407
432.617469	25957.455192	30.303424
432.932126	26008.888892	30.308442
433.060520	26044.577005	30.313460
433.549427	26068.541853	30.318477
433.896544	26116.096537	30.323495
434.068346	26155.987226	30.328512
434.670075	26196.746032	30.333530
435.200921	26241.567224	30.338548
436.136287	26277.040869	30.343565
436.088554	26318.040687	30.348583
436.503550	26357.059422	30.353600
436.921726	26402.145103	30.358618
437.567872	26454.103150	30.363636
438.056739	26490.165360	30.368653
438.226584	26533.337286	30.373671
439.172096	26577.462250	30.378688
439.560109	26608.781333	30.383706
439.459702	26657.469184	30.388724
440.118938	26692.689756	30.393741
440.837951	26733.007813	30.398759
441.366786	26775.460396	30.403776
441.579673	26815.010972	30.408794
441.784736	26865.926786	30.413812
442.431743	26888.572176	30.418829
442.675449	26935.449742	30.423847
443.437539	26974.446901	30.428864
443.725504	27026.190740	30.433882
443.719996	27059.411383	30.438900
444.684617	27104.356152	30.443917
444.983331	27146.599059	30.448935
445.591695	27184.868572	30.453952
445.945007	27229.504860	30.458970
446.060337	27276.561330	30.463988
446.773481	27306.819293	30.469005
447.347042	27358.165297	30.474023
447.654811	27397.942322	30.479040
447.926058	27440.512486	30.484058
448.564938	27487.165093	30.489076
449.067385	27532.752047	30.494093
449.412070	27576.663585	30.499111
449.699856	27609.080721	30.504128
450.505063	27655.928884	30.509146
450.303866	27696.715334	30.514164
451.260263	27729.691599	30.519181
451.578809	27767.634686	30.524199
452.290262	27802.172699	30.529216
452.664902	27843.374899	30.534234
452.979002	27892.999435	30.539252
453.562221	27922.924708	30.544269
453.887898	27963.749260	30.549287
454.140911	28005.324793	30.554304
454.689468	28047.182797	30.559322
454.994806	28089.919634	30.564340
455.513259	28132.231296	30.569357
455.773252	28187.269233	30.574375
456.188640	28220.027634	30.579392
456.858430	28269.388788	30.584410
457.247192	28310.425378	30.589428
458.004900	28349.312083	30.594445
458.348213	28398.787893	30.599463
458.343808	28449.083102	30.604480
459.155658	28490.218126	30.609498
459.534125	28544.144963	30.614516
460.235090	28588.154571	30.619533
460.438379	28633.026013	30.624551
461.121820	28683.176135	30.629568
461.522752	28723.238229	30.634586
462.100121	28781.198873	30.639604
462.691894	28811.427512	30.644621
463.542339	28860.660662	30.649639
463.289280	28907.045353	30.654656
464.091221	28939.554732	30.659674
464.144027	28997.307383	30.664692
464.736316	29040.652319	30.669709
465.100902	29094.304652	30.674727
465.550583	29149.340743	30.679744
466.034716	29195.022763	30.684762
466.249645	29253.256422	30.689780
467.352609	29304.069276	30.694797
467.478532	29356.748302	30.699815
467.662508	29396.567562	30.704832
468.601092	29442.216878	30.709850
468.831976	29497.035325	30.714868
469.507489	29534.401117	30.719885
470.326133	29592.465324	30.724903
470.329238	29646.377990	30.729920
471.015837	29691.359355	30.734938
471.772591	29735.482789	30.739956
472.481270	29778.299033	30.744973
472.498011	29825.933061	30.749991
472.884919	29876.100934	30.755008
473.491099	29918.497357	30.760026
473.894418	29968.195110	30.765044
474.495171	30002.602461	30.770061
475.205677	30055.065283	30.775079
475.273201	30098.172252	30.780096
476.300650	30149.106484	30.785114
476.296701	30199.349003	30.790132
476.567035	30241.267698	30.795149
477.220306	30289.972550	30.800167
477.361189	30339.952513	30.805184
478.172271	30383.221757	30.810202
478.675190	30432.102207	30.815220
479.134548	30481.134988	30.820237
479.778091	30518.039785	30.825255
480.233972	30569.962223	30.830272
481.015624	30614.279601	30.835290
481.006349	30661.679411	30.840308
481.712184	30692.904388	30.845325
482.421930	30742.018679	30.850343
482.352049	30785.742822	30.855360
483.104724	30821.196080	30.860378
483.464081	30867.388103	30.865396
484.119442	30907.680097	30.870413
484.351410	30956.945588	30.875431
484.837799	30998.433716	30.880448
485.635388	31041.763345	30.885466
485.745643	31086.819053	30.890484
486.259560	31129.169193	30.895501
486.560208	31182.470307	30.900519
487.137202	31228.489969	30.905536
487.949763	31273.600447	30.910554
487.905016	31321.253863	30.915572
488.440556	31366.856771	30.920589
488.873263	31421.256755	30.925607
489.591524	31472.463931	30.930624
490.017732	31523.799159	30.935642
490.150610	31571.817276	30.940660
491.003140	31623.351491	30.945677
491.623659	31678.968124	30.950695
491.726314	31732.162576	30.955712
492.394271	31769.388189	30.960730
492.941235	31838.014446	30.965748
493.598355	31884.712093	30.970765
494.098068	31938.590862	30.975783
494.122546	31991.968911	30.980800
495.347158	32042.978068	30.985818
495.403142	32102.970507	30.990836
495.732914	32142.829102	30.995853
496.648827	32202.832547	31.000871
497.178578	32251.068232	31.005888
497.505638	32299.569689	31.010906
498.363126	32351.541146	31.015924
498.519687	32406.195576	31.020941
499.026343	32459.069400	31.025959
499.505206	32511.404014	31.030976
500.396894	32564.622411	31.035994
500.697591	32610.802198	31.041012
501.208384	32660.559097	31.046029
501.821745	32711.279977	31.051047
502.148675	32761.344086	31.056064
502.598874	32813.393127	31.061082
503.072972	32869.920964	31.066100
503.704819	32910.890665	31.071117
504.388227	32974.504768	31.076135
504.607893	33023.151164	31.081152
505.250946	33078.142094	31.086170
505.494728	33125.691206	31.091188
506.397377	33178.043300	31.096205
507.060138	33239.050349	31.101223
507.293679	33288.447537	31.106240
508.011899	33335.385423	31.111258
508.596830	33387.737223	31.116276
508.807871	33441.431146	31.121293
509.495047	33491.763013	31.126311
509.547223	33546.316636	31.131328
510.293918	33584.740721	31.136346
510.920540	33650.780913	31.141364
511.019041	33702.457317	31.146381
511.823710	33747.498506	31.151399
512.470419	33803.584540	31.156416
512.972354	33851.840909	31.161434
513.597817	33908.006419	31.166452
514.061774	33958.734745	31.171469
514.409014	34004.651083	31.176487
514.466782	34056.378991	31.181504
515.367645	34107.677821	31.186522
515.967128	34168.254897	31.191540
516.559712	34211.781272	31.196557
517.000749	34266.370690	31.201575
517.131796	34311.240394	31.206592
518.032499	34344.672190	31.211610
518.452347	34410.367790	31.216628
519.025681	34456.414087	31.221645
519.510248	34499.376290	31.226663
519.936736	34552.868587	31.231680
520.387476	34606.711290	31.236698
521.185566	34658.779955	31.241716
521.455448	34706.884942	31.246733
521.843908	34766.377664	31.251751
521.811306	34820.587457	31.256768
522.683453	34879.252334	31.261786
523.020571	34934.732294	31.266804
523.683275	34995.978376	31.271821
524.326253	35054.900930	31.276839
524.611360	35115.631121	31.281856
525.418376	35164.241043	31.286874
526.068807	35236.124771	31.291892
526.641711	35291.650932	31.296909
527.068822	35349.931565	31.301927
527.543710	35406.725313	31.306944
528.228004	35456.322531	31.311962
528.678217	35520.474019	31.316980
529.319116	35581.446997	31.321997
530.222622	35636.821114	31.327015
530.464162	35701.353594	31.332032
530.921740	35750.361029	31.337050
531.258120	35799.849141	31.342068
532.060534	35864.793792	31.347085
532.951298	35911.394223	31.352103
533.533124	35977.834396	31.357120
533.773205	36035.867984	31.362138
534.294368	36083.500437	31.367156
534.683763	36154.897010	31.372173
535.492761	36201.561467	31.377191
535.687877	36259.103176	31.382208
536.351327	36321.952722	31.387226
537.001596	36371.095808	31.392244
537.637814	36423.276353	31.397261
538.355510	36484.145037	31.402279
538.598095	36544.898608	31.407296
538.921002	36603.148402	31.412314
539.857475	36658.899409	31.417332
540.152616	36712.044632	31.422349
540.667657	36765.958608	31.427367
541.442951	36831.226613	31.432384
541.854090	36891.524782	31.437402
542.496663	36953.102136	31.442420
542.849235	37010.109009	31.447437
543.694058	37061.695658	31.452455
543.819718	37133.882964	31.457472
544.347622	37189.952282	31.462490
545.632703	37246.269919	31.467508
545.668910	37301.505958	31.472525
546.238989	37350.379295	31.477543
547.006235	37417.863571	31.482560
547.487947	37479.973511	31.487578
548.194021	37529.236987	31.492596
548.543473	37588.648832	31.497613
549.238743	37642.170016	31.502631
549.223536	37696.732175	31.507648
549.945773	37752.468992	31.512666
550.640514	37816.057882	31.517684
551.145199	37880.245855	31.522701
552.029272	37926.914963	31.527719
552.106364	37983.961240	31.532736
552.722889	38040.063161	31.537754
553.168650	38080.458584	31.542772
553.480804	38140.554429	31.547789
553.948635	38202.175376	31.552807
554.661118	38263.315520	31.557824
555.604172	38316.565595	31.562842
555.915450	38371.565257	31.567860
556.282991	38433.834952	31.572877
557.125909	38491.072494	31.577895
557.410810	38553.614753	31.582912
557.796819	38608.527428	31.587930
558.426620	38665.760867	31.592948
558.766594	38735.599107	31.597965
559.727691	38795.025986	31.602983
560.218264	38859.415121	31.608000
560.441160	38916.535881	31.613018
561.229329	38986.443862	31.618036
561.830295	39060.865098	31.623053
562.497107	39117.828328	31.628071
563.202369	39187.262993	31.633088
563.836948	39248.266345	31.638106
564.194319	39305.620031	31.643124
564.719603	39370.479551	31.648141
565.383820	39430.296170	31.653159
566.167192	39499.125134	31.658176
566.844572	39557.700515	31.663194
567.513012	39620.660094	31.668212
567.702627	39684.567582	31.673229
568.346951	39751.186688	31.678247
568.804797	39814.641476	31.683264
569.307180	39878.608061	31.688282
570.395706	39941.970770	31.693300
570.227681	40008.768484	31.698317
571.231697	40073.137722	31.703335
571.913234	40139.081812	31.708352
572.081226	40204.240098	31.713370
573.097619	40263.377743	31.718388
573.990542	40333.710032	31.723405
574.708231	40396.385868	31.728423
575.412236	40455.357930	31.733440
575.589138	40514.488596	31.738458
576.174988	40565.232424	31.743476
576.730673	40630.230071	31.748493
577.492780	40699.894662	31.753511
578.021096	40757.054633	31.758528
578.500136	40818.251179	31.763546
578.899189	40876.532170	31.768564
579.744547	40940.675834	31.773581
580.390587	40989.804789	31.778599
580.811249	41050.745496	31.783616
581.346475	41119.182040	31.788634
582.052904	41180.002456	31.793652
582.492429	41245.020121	31.798669
583.130826	41306.667419	31.803687
583.720550	41374.147528	31.808704
584.176406	41439.517391	31.813722
585.086667	41498.004583	31.818740
585.117953	41552.607071	31.823757
585.663465	41617.217105	31.828775
586.356864	41685.055091	31.833792
587.083027	41756.815837	31.838810
587.472161	41807.327709	31.843828
588.324075	41883.945588	31.848845
588.970170	41944.600476	31.853863
589.640849	42007.319904	31.858880
590.322092	42082.997504	31.863898
591.001787	42128.980278	31.868916
591.201389	42180.471421	31.873933
591.644456	42238.236813	31.878951
592.245324	42290.987276	31.883968
592.568720	42358.322364	31.888986
593.350623	42420.468954	31.894004
593.555451	42499.024551	31.899021
594.323080	42561.648148	31.904039
594.884643	42617.574373	31.909056
595.307960	42681.207310	31.914074
595.859177	42750.329523	31.919092
596.649471	42817.371510	31.924109
597.157946	42882.389530	31.929127
598.139012	42952.659474	31.934144
598.551405	43026.794807	31.939162
599.294132	43092.320719	31.944180
599.853162	43166.851016	31.949197
600.273271	43224.274693	31.954215
601.454993	43297.752805	31.959232
601.936297	43360.765067	31.964250
602.176639	43417.831559	31.969268
602.747389	43484.157242	31.974285
603.810830	43556.079744	31.979303
604.307385	43631.260237	31.984320
604.653025	43690.594376	31.989338
605.100457	43758.989597	31.994356
605.915021	43834.165250	31.999373
606.561851	43902.694144	32.004391
606.979585	43972.834154	32.009408
607.354872	44048.983860	32.014426
607.950910	44121.145850	32.019444
608.570371	44198.769610	32.024461
609.139534	44255.451502	32.029479
610.193066	44341.262536	32.034496
610.572146	44419.057543	32.039514
611.507385	44495.595494	32.044532
611.773006	44569.442672	32.049549
612.802814	44641.424551	32.054567
613.466300	44711.635929	32.059584
613.825276	44787.423821	32.064602
614.679518	44848.490517	32.069620
614.858386	44924.572757	32.074637
615.539266	45002.670440	32.079655
616.391963	45076.705680	32.084672
616.661273	45148.979087	32.089690
617.848870	45215.206984	32.094708
618.355917	45298.855308	32.099725
618.796422	45362.524838	32.104743
619.756244	45429.212867	32.109760
620.289790	45510.036514	32.114778
621.178853	45581.271703	32.119796
621.569983	45657.740691	32.124813
622.490479	45723.360354	32.129831
622.970293	45786.038086	32.134848
623.761985	45861.458192	32.139866
624.652611	45921.883192	32.144884
625.019048	45984.724731	32.149901
625.520957	46067.971857	32.154919
626.298430	46125.758208	32.159936
626.749228	46202.327242	32.164954
627.744593	46263.185903	32.169972
627.945736	46331.621219	32.174989
628.531576	46396.877733	32.180007
629.075183	46454.847053	32.185024
629.932901	46540.621249	32.190042
630.667861	46589.571522	32.195060
631.066633	46666.877784	32.200077
631.762272	46729.948191	32.205095
632.407947	46799.049141	32.210112
632.692227	46868.447294	32.215130
633.408462	46934.716114	32.220148
634.109323	46993.149306	32.225165
634.965762	47059.662237	32.230183
635.453786	47125.284116	32.235200
635.735191	47191.008133	32.240218
636.445066	47253.514728	32.245236
637.063885	47326.619730	32.250253
637.568291	47392.935716	32.255271
638.173583	47466.947958	32.260288
638.588740	47540.465126	32.265306
639.768343	47613.964037	32.270324
640.263473	47676.549712	32.275341
640.690852	47752.431741	32.280359
641.555424	47827.397806	32.285376
641.990105	47901.975934	32.290394
642.604596	47980.562470	32.295412
643.065719	48055.004100	32.300429
643.958136	48140.981361	32.305447
644.576812	48213.140247	32.310464
644.892951	48289.402099	32.315482
645.772868	48362.020346	32.320500
646.451787	48447.924645	32.325517
647.227165	48529.809372	32.330535
648.072111	48597.562302	32.335552
648.289380	48689.543843	32.340570
648.865077	48770.505368	32.345588
649.790191	48848.394589	32.350605
650.229890	48922.842400	32.355623
651.396844	48999.922395	32.360640
651.942408	49085.634860	32.365658
652.350628	49162.157251	32.370676
653.049422	49251.674086	32.375693
653.826093	49322.881676	32.380711
654.433226	49404.688320	32.385728
654.689274	49485.170964	32.390746
656.003060	49562.824589	32.395764
656.495781	49640.398270	32.400781
657.127342	49724.612808	32.405799
657.850072	49804.675498	32.410816
658.567351	49884.498892	32.415834
659.165142	49960.576666	32.420852
660.039513	50033.707241	32.425869
660.376299	50121.265807	32.430887
661.523644	50198.669251	32.435904
661.891464	50276.701205	32.440922
662.870993	50357.826525	32.445940
663.299378	50434.596745	32.450957
664.096116	50510.575576	32.455975
664.740079	50590.197766	32.460992
665.239911	50663.034663	32.466010
665.878918	50742.069716	32.471028
666.400381	50818.181249	32.476045
667.267966	50907.526221	32.481063
668.284406	50982.004252	32.486080
668.892863	51068.125510	32.491098
669.285545	51141.923470	32.496116
670.150182	51206.745083	32.501133
670.457186	51304.803640	32.506151
671.122796	51376.775267	32.511168
671.966776	51456.122335	32.516186
672.969705	51537.305069	32.521204
673.463479	51618.871542	32.526221
674.051037	51705.011088	32.531239
674.748807	51768.443027	32.536256
675.171292	51850.211302	32.541274
676.176999	51929.091725	32.546292
676.594908	52006.723008	32.551309
677.005810	52082.931925	32.556327
678.231477	52153.799494	32.561344
678.223208	52228.169899	32.566362
678.858520	52302.895349	32.571380
679.401190	52377.844361	32.576397
680.413286	52463.078631	32.581415
680.962651	52537.084270	32.586432
681.722240	52630.477229	32.591450
682.622568	52709.598264	32.596468
683.580029	52780.402164	32.601485
684.073381	52873.597328	32.606503
684.453711	52946.865060	32.611520
685.202854	53029.440564	32.616538
685.914829	53103.580724	32.621556
686.883989	53185.546481	32.626573
687.090163	53272.593139	32.631591
687.727228	53343.018610	32.636608
688.284886	53431.795307	32.641626
689.032531	53515.897807	32.646644
689.690469	53608.500586	32.651661
690.254171	53696.353437	32.656679
691.442337	53783.640544	32.661696
692.303954	53873.155990	32.666714
692.577767	53961.979135	32.671732
693.426588	54045.143768	32.676749
694.005193	54140.102484	32.681767
694.589859	54225.517662	32.686784
695.478354	54321.358827	32.691802
696.189261	54414.874070	32.696820
696.914000	54493.383114	32.701837
697.329894	54594.450630	32.706855
698.361992	54668.836682	32.711872
699.394042	54766.277223	32.716890
699.505283	54853.205344	32.721908
700.787714	54940.817368	32.726925
701.207608	55036.905677	32.731943
702.233302	55124.571240	32.736960
702.770186	55211.453001	32.741978
703.545942	55299.936756	32.746996
704.218508	55394.063071	32.752013
704.733471	55483.189559	32.757031
705.890983	55567.633861	32.762048
706.369625	55665.069822	32.767066
706.787710	55748.504066	32.772084
707.830073	55817.911474	32.777101
708.425203	55919.810919	32.782119
709.702395	56009.446548	32.787136
710.102197	56096.004919	32.792154
710.995850	56178.897867	32.797172
711.501115	56263.010089	32.802189
711.802771	56353.907312	32.807207
712.956225	56439.051500	32.812224
713.770801	56525.913544	32.817242
714.430970	56621.103550	32.822260
715.110799	56707.006377	32.827277
716.096341	56794.918532	32.832295
716.568743	56874.436928	32.837312
717.322441	56960.613897	32.842330
717.872980	57039.797827	32.847348
718.942865	57134.077623	32.852365
719.498857	57222.957330	32.857383
719.718494	57301.611670	32.862400
720.952286	57390.480788	32.867418
721.611785	57486.636344	32.872436
722.458094	57572.744040	32.877453
722.944578	57658.022312	32.882471
723.614301	57737.392403	32.887488
724.400485	57822.149636	32.892506
725.070494	57914.684960	32.897524
725.863206	57990.688475	32.902541
726.592214	58072.487134	32.907559
726.885549	58158.632879	32.912576
727.985524	58243.677902	32.917594
728.192638	58321.875484	32.922612
729.055092	58405.356955	32.927629
729.932890	58497.412585	32.932647
730.655250	58581.815370	32.937664
731.349538	58676.248614	32.942682
732.136579	58766.654845	32.947700
732.908560	58853.937024	32.952717
733.333471	58939.938347	32.957735
734.188339	59027.917071	32.962752
734.628871	59120.220761	32.967770
735.046770	59213.819571	32.972788
736.289297	59311.169631	32.977805
736.993215	59408.268955	32.982823
737.631785	59504.790245	32.987840
738.483274	59600.854489	32.992858
738.835741	59701.776153	32.997876
740.126086	59790.208466	33.002893
740.812542	59882.362593	33.007911
741.299677	59981.460354	33.012928
742.141853	60087.389704	33.017946
742.810759	60185.915467	33.022964
743.932684	60271.660414	33.027981
744.758266	60376.909994	33.032999
745.351394	60478.993513	33.038016
746.115117	60576.043796	33.043034
746.490487	60676.029059	33.048052
747.564522	60778.013192	33.053069
748.414872	60868.727450	33.058087
749.409094	60968.180223	33.063104
750.326285	61067.246669	33.068122
750.496135	61173.051771	33.073140
751.649463	61257.871056	33.078157
752.598154	61362.181381	33.083175
753.275854	61451.779074	33.088192
754.012335	61540.310754	33.093210
754.550868	61646.313354	33.098228
755.616465	61729.014729	33.103245
756.093389	61827.380885	33.108263
756.971404	61930.210744	33.113280
757.755062	62021.389128	33.118298
758.365971	62128.331996	33.123316
759.482851	62213.850270	33.128333
760.323086	62310.965023	33.133351
760.986776	62396.890402	33.138368
761.826900	62498.747346	33.143386
762.358619	62605.983208	33.148404
763.030317	62691.142370	33.153421
764.139385	62793.629432	33.158439
765.015927	62888.328849	33.163456
765.504289	62982.323420	33.168474
766.405637	63081.919501	33.173492
767.294372	63172.851422	33.178509
768.216440	63264.924290	33.183527
768.879234	63352.916875	33.188544
769.602056	63446.585272	33.193562
769.998070	63549.370685	33.198580
771.123410	63638.279424	33.203597
772.183905	63734.599219	33.208615
772.668862	63822.570658	33.213632
773.365388	63912.649066	33.218650
774.112411	64003.435267	33.223668
774.993567	64096.302614	33.228685
775.651529	64197.872138	33.233703
775.857999	64287.996977	33.238720
776.746471	64364.961112	33.243738
777.296896	64463.630024	33.248756
778.069567	64556.794618	33.253773
779.032170	64658.881750	33.258791
779.504128	64758.728995	33.263808
780.383544	64843.970573	33.268826
780.990436	64944.303902	33.273844
782.163250	65048.689502	33.278861
782.741924	65142.817300	33.283879
783.507460	65246.438126	33.288896
784.422910	65343.761778	33.293914
784.936068	65446.207370	33.298932
785.691351	65551.040293	33.303949
786.585154	65648.767370	33.308967
787.375746	65760.243366	33.313984
788.053500	65856.226004	33.319002
788.583429	65969.351868	33.324020
789.982137	66072.218468	33.329037
790.808298	66170.091100	33.334055
791.626649	66268.142609	33.339072
792.743038	66373.080662	33.344090
793.497889	66479.702926	33.349108
794.073782	66577.325068	33.354125
794.680692	66684.585501	33.359143
795.265490	66788.867728	33.364160
796.501830	66887.837543	33.369178
797.149430	66998.708200	33.374196
798.154551	67103.945268	33.379213
798.533322	67207.020479	33.384231
799.342924	67315.347177	33.389248
800.776527	67416.827118	33.394266
801.447093	67521.282514	33.399284
801.955695	67622.642184	33.404301
802.920800	67739.297792	33.409319
803.609577	67849.405874	33.414336
804.699553	67946.376545	33.419354
805.338565	68057.746998	33.424372
806.296478	68165.218260	33.429389
807.354179	68270.977416	33.434407
807.803601	68373.565019	33.439424
808.813766	68474.843172	33.444442
809.826508	68589.861548	33.449460
810.392838	68680.110179	33.454477
811.414057	68791.069358	33.459495
812.083402	68895.042950	33.464512
813.398996	68994.109774	33.469530
814.025066	69100.098211	33.474548
814.914061	69198.713391	33.479565
815.660740	69301.270787	33.484583
816.030728	69411.264474	33.489600
817.316601	69503.733516	33.494618
817.914507	69614.572539	33.499636
818.934664	69717.012766	33.504653
819.553127	69816.793449	33.509671
820.427610	69921.739516	33.514688
821.258026	70019.113199	33.519706
822.115283	70126.766660	33.524724
822.976313	70230.316642	33.529741
824.043614	70322.651845	33.534759
824.687317	70430.365327	33.539776
825.492340	70541.650781	33.544794
826.236724	70639.876123	33.549812
827.248824	70738.351204	33.554829
828.005353	70825.176973	33.559847
828.474678	70946.445992	33.564864
829.604890	71047.804014	33.569882
829.994451	71156.915430	33.574900
830.853583	71258.329377	33.579917
831.842809	71350.237147	33.584935
832.485209	71452.458354	33.589952
833.449470	71540.659797	33.594970
834.246402	71642.882875	33.599988
834.577867	71749.308135	33.605005
835.618245	71854.850229	33.610023
836.336464	71960.848485	33.615040
837.102655	72065.345127	33.620058
837.799266	72170.359698	33.625076
838.903220	72265.115103	33.630093
839.679463	72383.011618	33.635111
840.342248	72502.041003	33.640128
841.380617	72609.093640	33.645146
842.158227	72719.126004	33.650164
843.118740	72825.229103	33.655181
843.525288	72945.934495	33.660199
844.373640	73064.316713	33.665216
845.278754	73177.788819	33.670234
846.198059	73302.810648	33.675252
846.931895	73408.140934	33.680269
847.841115	73528.453600	33.685287
848.840830	73651.513880	33.690304
849.627277	73770.554903	33.695322
850.391913	73890.727177	33.700340
851.607523	74007.447444	33.705357
852.762533	74130.764272	33.710375
852.963854	74252.001690	33.715392
854.212602	74357.001754	33.720410
854.933303	74483.947519	33.725428
855.793800	74604.766647	33.730445
856.530477	74722.527685	33.735463
857.495507	74842.077502	33.740480
858.662463	74960.468881	33.745498
858.926513	75072.174691	33.750516
859.742638	75204.074338	33.755533
860.978715	75328.929336	33.760551
861.764670	75448.636550	33.765568
862.889790	75567.898505	33.770586
863.575083	75688.027888	33.775604
864.515662	75812.766715	33.780621
865.632395	75932.525612	33.785639
865.926047	76069.198189	33.790656
867.413323	76182.883166	33.795674
868.184748	76300.366946	33.800692
868.967407	76427.160119	33.805709
870.051288	76547.420904	33.810727
870.898142	76675.497276	33.815744
871.607709	76784.923532	33.820762
872.803535	76914.453841	33.825780
873.686370	77028.984393	33.830797
874.813205	77140.246911	33.835815
875.552794	77268.659556	33.840832
876.219710	77383.998146	33.845850
877.166269	77505.070062	33.850868
878.581074	77615.757363	33.855885
879.101983	77729.460747	33.860903
880.088350	77854.670457	33.865920
880.642191	77953.611156	33.870938
881.664287	78087.240718	33.875956
882.433156	78201.375953	33.880973
883.436955	78311.509662	33.885991
883.928025	78438.978549	33.891008
885.260041	78557.347029	33.896026
886.137840	78671.771198	33.901044
886.807477	78791.625273	33.906061
887.906634	78904.736213	33.911079
888.753253	79029.593075	33.916096
889.369500	79138.599898	33.921114
890.269724	79248.576192	33.926132
890.969818	79361.219388	33.931149
892.169145	79464.257826	33.936167
892.608751	79580.920746	33.941184
893.809670	79685.948788	33.946202
894.631114	79806.252227	33.951220
895.633258	79930.138599	33.956237
896.280454	80046.428896	33.961255
897.380937	80159.582743	33.966272
898.205894	80268.168561	33.971290
898.805946	80383.010671	33.976308
899.830232	80512.901436	33.981325
900.577224	80631.877128	33.986343
901.466102	80758.217442	33.991360
902.383090	80882.881538	33.996378
903.214704	81005.253681	34.001396
904.271820	81136.092414	34.006413
905.176455	81258.010784	34.011431
905.920463	81388.152199	34.016448
907.018494	81522.217122	34.021466
908.066283	81650.715780	34.026484
908.889796	81772.167617	34.031501
909.799029	81903.831277	34.036519
910.974579	82042.219685	34.041536
911.785834	82168.033658	34.046554
912.331609	82295.334161	34.051572
913.174085	82422.702811	34.056589
914.242028	82556.055137	34.061607
915.031455	82691.631006	34.066624
916.006218	82822.845207	34.071642
917.136030	82946.294054	34.076660
917.661522	83090.148977	34.081677
918.611240	83219.949823	34.086695
919.852435	83359.436710	34.091712
920.381812	83495.107798	34.096730
921.947587	83632.631913	34.101748
922.423237	83774.850878	34.106765
923.942449	83905.047158	34.111783
924.516430	84031.413338	34.116800
925.465201	84163.613426	34.121818
926.718673	84300.543421	34.126836
927.408309	84436.117837	34.131853
928.374168	84567.240055	34.136871
929.376329	84712.092857	34.141888
930.364348	84844.441981	34.146906
931.370550	84980.374871	34.151924
931.876720	85114.004457	34.156941
932.988729	85249.212441	34.161959
934.104730	85384.610506	34.166976
935.033424	85530.011112	34.171994
936.028891	85656.977335	34.177012
936.764868	85787.558177	34.182029
937.982679	85931.546974	34.187047
938.807396	86070.630655	34.192064
939.663614	86203.842959	34.197082
941.102460	86331.426987	34.202100
941.735371	86458.162013	34.207117
942.600061	86594.644162	34.212135
943.880304	86723.800733	34.217152
944.933133	86864.132363	34.222170
945.651640	86991.933436	34.227188
946.801586	87119.730876	34.232205
947.950781	87243.892014	34.237223
948.713835	87382.269255	34.242240
949.547138	87506.861137	34.247258
950.477190	87644.985361	34.252276
951.321991	87769.791987	34.257293
952.246722	87887.223809	34.262311
952.977026	88015.116185	34.267328
953.956065	88136.912583	34.272346
954.930909	88254.654838	34.277364
955.760780	88393.469904	34.282381
956.621072	88516.553745	34.287399
957.883487	88639.473751	34.292416
958.705155	88769.382754	34.297434
959.508852	88900.879275	34.302452
960.341822	89038.695696	34.307469
961.273415	89163.976183	34.312487
962.400212	89302.622271	34.317504
962.940237	89442.184641	34.322522
964.233983	89561.808486	34.327540
964.676850	89715.290039	34.332557
965.783177	89856.261140	34.337575
966.688835	90003.829228	34.342592
967.658421	90141.249134	34.347610
968.992693	90278.688612	34.352628
970.052330	90430.188874	34.357645
970.375324	90567.433142	34.362663
971.657044	90722.816309	34.367680
972.310993	90871.708123	34.372698
973.537972	91010.739307	34.377716
974.266607	91167.922348	34.382733
975.218871	91305.705146	34.387751
976.333756	91460.623937	34.392768
977.143802	91616.529140	34.397786
978.515997	91762.892099	34.402804
979.491173	91920.192527	34.407821
980.588071	92071.188193	34.412839
981.661369	92219.564683	34.417856
982.388256	92376.450058	34.422874
983.367498	92528.239555	34.427892
984.291603	92687.212308	34.432909
985.530785	92834.653234	34.437927
986.440548	92984.960253	34.442944
987.666748	93140.351787	34.447962
988.457101	93295.799671	34.452980
989.448001	93451.407066	34.457997
990.746990	93597.017088	34.463015
991.889844	93752.044507	34.468032
992.601640	93903.540443	34.473050
994.008981	94047.728682	34.478068
994.795450	94202.839512	34.483085
995.825254	94350.738761	34.488103
997.284853	94503.451463	34.493120
997.469322	94659.229222	34.498138
998.723392	94805.004066	34.503156
1000.241263	94958.077471	34.508173
1001.097158	95115.742461	34.513191
1001.828964	95254.794341	34.518208
1002.642979	95408.588592	34.523226
1003.904975	95555.341739	34.528244
1004.993558	95717.688753	34.533261
1005.834512	95867.044466	34.538279
1007.190576	96022.911783	34.543296
1008.149342	96179.843490	34.548314
1009.325015	96318.868623	34.553332
1010.172014	96470.786843	34.558349
1011.283795	96623.336182	34.563367
1012.272450	96772.951947	34.568384
1013.332727	96928.426383	34.573402
1014.587953	97058.366012	34.578420
1015.834837	97218.325476	34.583437
1016.409563	97362.735401	34.588455
1017.799035	97499.640618	34.593472
1018.360860	97650.962640	34.598490
1019.606713	97782.960329	34.603508
1020.437977	97911.879628	34.608525
1021.023808	98056.024746	34.613543
1022.422634	98194.059725	34.618560
1023.193678	98337.746102	34.623578
1024.272841	98474.057562	34.628596
1025.067500	98614.356717	34.633613
1025.971107	98760.204691	34.638631
1027.080214	98900.684055	34.643648
1027.890257	99051.492105	34.648666
1028.802586	99201.410113	34.653684
1029.639693	99358.693470	34.658701
1031.088675	99511.279888	34.663719
1032.118267	99657.023456	34.668736
1032.707974	99815.843716	34.673754
1034.276222	99970.581491	34.678772
1035.130788	100133.393320	34.683789
1035.964957	100283.721589	34.688807
1037.292864	100436.635589	34.693824
1037.729748	100613.232589	34.698842
1039.099516	100762.376240	34.703860
1040.323694	100934.579260	34.708877
1041.284607	101097.036950	34.713895
1042.464897	101247.467608	34.718912
1043.144507	101418.211703	34.723930
1044.416869	101578.759329	34.728948
1045.830361	101742.835568	34.733965
1046.616981	101901.990139	34.738983
1047.871583	102065.877333	34.744000
1048.747723	102234.236707	34.749018
1050.201044	102391.780522	34.754036
1051.102403	102557.855458	34.759053
1052.243301	102718.441895	34.764071
1053.496431	102869.882852	34.769088
1054.371218	103047.451331	34.774106
1055.267290	103204.807321	34.779124
1056.679921	103361.753530	34.784141
1057.558447	103526.290054	34.789159
1058.715796	103684.571005	34.794176
1059.838079	103855.841597	34.799194
1060.928227	104019.624709	34.804212
1062.243037	104178.048172	34.809229
1063.105464	104343.466099	34.814247
1064.468570	104496.012991	34.819264
1065.447794	104658.218986	34.824282
1066.669995	104819.271928	34.829300
1067.867020	104972.671147	34.834317
1068.829538	105130.507592	34.839335
1070.138600	105293.666688	34.844352
1071.152871	105456.758606	34.849370
1071.938264	105600.550500	34.854388
1073.147227	105758.085010	34.859405
1074.131994	105925.634414	34.864423
1075.342101	106083.918367	34.869440
1076.490374	106244.254215	34.874458
1077.655386	106391.755977	34.879476
1078.771518	106555.369772	34.884493
1079.212591	106720.383412	34.889511
1080.928022	106867.395286	34.894528
1081.995179	107026.276590	34.899546
1082.975863	107183.612483	34.904564
1084.416975	107339.913302	34.909581
1085.104299	107495.572013	34.914599
1086.573821	107644.515098	34.919616
1087.435567	107800.794584	34.924634
1088.660554	107950.132326	34.929652
1089.830321	108109.776073	34.934669
1090.752922	108269.890396	34.939687
1091.539033	108411.994727	34.944704
1092.421055	108561.300027	34.949722
1093.828841	108694.139929	34.954740
1094.615158	108842.738607	34.959757
1095.548603	109004.427047	34.964775
1096.588365	109162.396717	34.969792
1097.922184	109312.560216	34.974810
1098.970641	109452.307063	34.979828
1100.254477	109607.044871	34.984845
1100.943358	109771.324063	34.989863
1102.090418	109930.979687	34.994880
1103.117995	110082.018705	34.999898
1104.531028	110238.489095	35.004916
1105.468498	110397.393392	35.009933
1106.291396	110561.059247	35.014951
1108.262212	110729.568070	35.019968
1108.929353	110879.360712	35.024986
1109.992778	111046.047434	35.030004
1110.973173	111199.546179	35.035021
1112.023631	111378.005195	35.040039
1113.368302	111541.517784	35.045056
1114.322978	111702.644554	35.050074
1115.469423	111868.434380	35.055092
1116.778339	112028.277000	35.060109
1117.655117	112204.662100	35.065127
1118.997957	112363.752655	35.070144
1120.151698	112531.776469	35.075162
1121.082128	112690.311598	35.080180
1122.122694	112863.313464	35.085197
1123.602540	113043.806125	35.090215
1124.724869	113206.790381	35.095232
1125.799099	113379.142632	35.100250
1127.105678	113543.811702	35.105268
1128.227646	113704.553423	35.110285
1129.184201	113878.423016	35.115303
1130.480501	114049.082233	35.120320
1131.404963	114224.822871	35.125338
1132.398848	114397.585680	35.130356
1133.845715	114568.109598	35.135373
1134.898214	114737.605307	35.140391
1135.794338	114906.441389	35.145408
1136.894665	115083.059100	35.150426
1138.226217	115268.456294	35.155444
1139.646492	115429.057401	35.160461
1140.462789	115610.554426	35.165479
1141.728349	115784.815885	35.170496
1142.875290	115969.319600	35.175514
1143.614651	116139.619076	35.180532
1144.975815	116315.339342	35.185549
1146.404566	116496.072575	35.190567
1147.798339	116673.260723	35.195584
1148.673092	116848.425458	35.200602
1149.527911	117023.479977	35.205620
1150.738317	117201.549142	35.210637
1151.928593	117390.226073	35.215655
1153.200820	117560.778366	35.220672
1154.615219	117748.851225	35.225690
1155.547316	117916.033673	35.230708
1156.868937	118091.045435	35.235725
1157.768544	118277.222775	35.240743
1159.160210	118440.745951	35.245760
1160.358743	118625.064343	35.250778
1161.603762	118806.725306	35.255796
1162.655303	118974.172762	35.260813
1163.652884	119160.973301	35.265831
1165.096048	119332.102950	35.270848
1166.385688	119506.289026	35.275866
1167.762966	119688.402795	35.280884
1168.523517	119842.339645	35.285901
1169.183736	120006.022062	35.290919
1170.952816	120166.132039	35.295936
1171.887513	120341.620568	35.300954
1172.727353	120502.143789	35.305972
1174.203974	120669.291049	35.310989
1174.970280	120850.047152	35.316007
1176.328805	121003.146579	35.321024
1177.160189	121177.614872	35.326042
1178.418419	121359.323825	35.331060
1180.140963	121536.140518	35.336077
1180.924198	121709.756119	35.341095
1181.848678	121891.595899	35.346112
1183.076117	122075.177743	35.351130
1184.249578	122249.330852	35.356148
1185.359745	122447.736811	35.361165
1186.436381	122630.647137	35.366183
1187.499731	122808.321186	35.371200
1188.919365	122999.805805	35.376218
1190.031989	123189.055957	35.381236
1191.243516	123378.773588	35.386253
1192.488074	123572.977779	35.391271
1193.630163	123757.963533	35.396288
1195.012311	123944.523691	35.401306
1195.868923	124140.542041	35.406324
1197.108193	124338.937192	35.411341
1198.564038	124533.417420	35.416359
1199.899280	124718.390038	35.421376
1200.898798	124925.832891	35.426394
1202.405584	125112.683413	35.431412
1203.538761	125304.870865	35.436429
1204.745625	125504.101418	35.441447
1205.889277	125702.036117	35.446464
1207.026706	125895.227928	35.451482
1208.443088	126089.658344	35.456500
1209.549572	126285.419560	35.461517
1211.121712	126496.117378	35.466535
1212.088498	126682.704374	35.471552
1213.287077	126880.560031	35.476570
1214.883556	127076.197549	35.481588
1215.865962	127279.760065	35.486605
1217.108353	127477.357970	35.491623
1218.311156	127677.157902	35.496640
1219.447653	127876.677363	35.501658
1220.788491	128080.885484	35.506676
1222.115776	128271.356254	35.511693
1222.910720	128473.126945	35.516711
1224.327838	128686.131177	35.521728
1225.365635	128876.231314	35.526746
1226.719050	129083.335105	35.531764
1228.113263	129279.839281	35.536781
1229.589035	129486.164625	35.541799
1230.741198	129689.344295	35.546816
1232.152613	129884.199154	35.551834
1233.257803	130088.872564	35.556852
1234.719812	130286.677633	35.561869
1235.810255	130485.176185	35.566887
1236.938593	130692.640230	35.571904
1238.520823	130881.496775	35.576922
1239.302677	131094.980446	35.581940
1240.729948	131285.791631	35.586957
1241.766463	131491.129563	35.591975
1243.303019	131696.567827	35.596992
1244.682603	131884.305821	35.602010
1245.407211	132090.164879	35.607028
1247.177516	132291.915058	35.612045
1248.223319	132482.626252	35.617063
1249.606839	132682.357837	35.622080
1250.791894	132868.201819	35.627098
1251.792865	133059.569659	35.632116
1253.127876	133242.371804	35.637133
1254.294222	133425.670597	35.642151
1255.336296	133615.752827	35.647168
1256.538110	133810.746900	35.652186
1257.661348	134011.045479	35.657204
1259.221072	134204.843232	35.662221
1260.496691	134401.566747	35.667239
1261.554471	134597.310086	35.672256
1262.974425	134800.535037	35.677274
1263.769177	135000.927528	35.682292
1265.256859	135193.928708	35.687309
1266.367588	135404.298174	35.692327
1267.517940	135601.693702	35.697344
1269.007123	135806.384325	35.702362
1269.433592	136021.025948	35.707380
1271.451155	136233.845990	35.712397
1272.751709	136443.695645	35.717415
1273.853553	136656.013815	35.722432
1275.308333	136864.648409	35.727450
1276.085349	137094.607642	35.732468
1277.583516	137304.709469	35.737485
1278.922185	137535.661626	35.742503
1280.011319	137736.045390	35.747520
1281.439745	137956.186288	35.752538
1282.527866	138177.130219	35.757556
1283.816099	138402.320504	35.762573
1285.065240	138628.266721	35.767591
1286.288344	138852.949057	35.772608
1287.694513	139081.131764	35.777626
1289.135319	139315.363546	35.782644
1290.810605	139536.336159	35.787661
1291.851950	139754.997806	35.792679
1293.063656	139985.360027	35.797696
1294.647684	140206.045455	35.802714
1295.846986	140437.160550	35.807732
1297.428627	140662.239487	35.812749
1298.453288	140891.112428	35.817767
1299.862342	141114.583358	35.822784
1301.618799	141337.797882	35.827802
1302.622135	141568.492189	35.832820
1304.016145	141783.389336	35.837837
1305.426762	142015.011917	35.842855
1306.944985	142242.303700	35.847872
1308.158970	142458.424978	35.852890
1309.569266	142689.035481	35.857908
1310.606171	142909.488854	35.862925
1312.108885	143129.591081	35.867943
1313.326149	143360.742594	35.872960
1314.961736	143583.250131	35.877978
1316.250097	143809.100170	35.882996
1317.536194	144025.724658	35.888013
1319.074671	144252.743266	35.893031
1320.064697	144474.975061	35.898048
1321.563643	144697.610468	35.903066
1322.653275	144924.651592	35.908084
1324.430368	145152.233418	35.913101
1325.866121	145377.813570	35.918119
1326.830623	145587.907880	35.923136
1328.484523	145813.633501	35.928154
1329.850039	146032.564117	35.933172
1331.060603	146251.113764	35.938189
1332.402148	146474.555791	35.943207
1333.504254	146685.826131	35.948224
1334.962166	146908.985276	35.953242
1336.290941	147137.369540	35.958260
1337.286193	147351.502442	35.963277
1339.135604	147563.433616	35.968295
1340.021502	147773.358706	35.973312
1341.605273	147987.655939	35.978330
1342.820130	148197.353528	35.983348
1343.872785	148408.663946	35.988365
1345.506479	148617.015659	35.993383
1346.713189	148837.036390	35.998400
1347.978221	149047.173736	36.003418
1349.070843	149263.837743	36.008436
1350.419695	149476.819594	36.013453
1351.849055	149697.532518	36.018471
1353.050856	149917.990020	36.023488
1354.728869	150145.482112	36.028506
1355.802191	150372.422449	36.033524
1356.959804	150584.461211	36.038541
1358.392408	150813.860437	36.043559
1359.734311	151043.465223	36.048576
1361.209850	151274.420954	36.053594
1362.364823	151513.335935	36.058612
1364.205853	151742.548169	36.063629
1365.751687	151968.583361	36.068647
1366.631396	152205.373790	36.073664
1368.020081	152440.549605	36.078682
1369.382320	152670.094477	36.083700
1370.305273	152907.820453	36.088717
1371.628087	153152.542683	36.093735
1373.095763	153394.691801	36.098752
1374.614947	153636.732338	36.103770
1375.933629	153879.452689	36.108788
1377.079344	154128.903671	36.113805
1378.752783	154377.194126	36.118823
1380.247784	154639.718491	36.123840
1381.836825	154881.651799	36.128858
1383.353109	155121.464848	36.133876
1384.897659	155374.514771	36.138893
1386.513325	155607.624293	36.143911
1387.666291	155864.672928	36.148928
1389.162188	156102.741348	36.153946
1390.513167	156339.640115	36.158964
1391.740426	156588.936538	36.163981
1393.123855	156836.318044	36.168999
1394.620305	157083.276653	36.174016
1396.180615	157331.698891	36.179034
1397.563963	157575.008414	36.184052
1399.358754	157820.361884	36.189069
1400.525628	158060.101874	36.194087
1401.733103	158315.095936	36.199104
1403.528947	158557.138807	36.204122
1404.752091	158795.476421	36.209140
1406.060000	159038.676660	36.214157
1407.970651	159285.846006	36.219175
1409.264182	159535.029928	36.224192
1410.667872	159785.225934	36.229210
1412.175600	160020.692661	36.234228
1413.708869	160258.923891	36.239245
1415.276530	160492.123216	36.244263
1416.573600	160744.244073	36.249280
1418.129956	160982.880688	36.254298
1419.365211	161221.746199	36.259316
1420.543025	161460.977078	36.264333
1421.936130	161697.648698	36.269351
1423.492688	161948.032474	36.274368
1425.110522	162205.072960	36.279386
1426.845268	162447.064211	36.284404
1427.900653	162680.643711	36.289421
1429.790745	162929.785659	36.294439
1431.156467	163161.083808	36.299456
1432.587339	163404.205335	36.304474
1433.820312	163622.436211	36.309492
1434.953338	163830.437636	36.314509
1436.642813	164050.769518	36.319527
1437.638520	164284.973466	36.324544
1439.084640	164505.027532	36.329562
1440.318659	164738.053096	36.334580
1441.573820	164971.876029	36.339597
1443.177279	165202.877432	36.344615
1444.556525	165442.649894	36.349632
1445.853383	165677.547933	36.354650
1447.262238	165918.434724	36.359668
1448.421491	166159.856596	36.364685
1450.031469	166408.090355	36.369703
1451.301629	166666.319711	36.374720
1452.724223	166904.795414	36.379738
1454.222646	167163.041670	36.384756
1455.169458	167414.709370	36.389773
1456.913578	167673.426917	36.394791
1457.897034	167940.555565	36.399808
1459.479482	168197.941756	36.404826
1461.278965	168467.039656	36.409844
1462.480917	168730.493010	36.414861
1463.909480	169005.021841	36.419879
1465.441362	169275.789874	36.424896
1467.262468	169542.679086	36.429914
1468.846330	169809.466734	36.434932
1469.767962	170081.082398	36.439949
1471.403390	170352.460366	36.444967
1472.689243	170634.750321	36.449984
1474.399629	170899.261951	36.455002
1476.187879	171178.212079	36.460020
1477.536355	171457.651088	36.465037
1479.446829	171721.359736	36.470055
1480.347898	171997.607477	36.475072
1481.894135	172268.384117	36.480090
1483.618851	172542.320904	36.485108
1484.969239	172822.793110	36.490125
1486.718309	173097.616891	36.495143
1488.364377	173388.520551	36.500160
1489.662103	173667.137442	36.505178
1491.321539	173936.962514	36.510196
1492.507648	174217.020977	36.515213
1494.436310	174490.767561	36.520231
1496.007250	174771.402633	36.525248
1497.466678	175041.186539	36.530266
1499.244542	175322.426040	36.535284
1500.598496	175601.180517	36.540301
1502.243024	175865.274773	36.545319
1504.092871	176149.108982	36.550336
1505.277080	176425.391243	36.555354
1506.782234	176698.652767	36.560372
1508.025294	176974.445090	36.565389
1509.957496	177244.898688	36.570407
1511.123287	177517.174700	36.575424
1513.101990	177797.222841	36.580442
1514.321996	178071.396909	36.585460
1515.953499	178344.567745	36.590477
1517.613697	178613.366608	36.595495
1518.980560	178891.152094	36.600512
1520.292613	179169.581971	36.605530
1522.030619	179451.298537	36.610548
1523.393377	179736.071647	36.615565
1525.452114	180002.805941	36.620583
1526.694861	180279.929446	36.625600
1528.211723	180555.994980	36.630618
1529.838845	180825.262840	36.635636
1531.345491	181104.150799	36.640653
1532.659908	181366.840300	36.645671
1534.269516	181638.475295	36.650688
1535.792736	181895.495212	36.655706
1537.807821	182145.124137	36.660724
1539.020585	182405.699000	36.665741
1540.506424	182660.009218	36.670759
1541.711023	182929.628635	36.675776
1543.215973	183181.956159	36.680794
1545.027133	183442.770362	36.685812
1546.250978	183710.585634	36.690829
1547.288537	183981.732635	36.695847
1549.097604	184247.679860	36.700864
1550.330151	184595.959783	36.705882
1552.166847	184879.099454	36.710900
1553.371089	185155.201758	36.715917
1554.880315	185435.803528	36.720935
1556.266906	185726.864342	36.725952
1557.918892	186012.423592	36.730970
1559.435887	186294.372643	36.735988
1560.689734	186597.622968	36.741005
1562.233034	186885.614556	36.746023
1563.994569	187187.898131	36.751040
1565.443564	187482.713177	36.756058
1567.353575	187778.980858	36.761076
1568.707318	188085.521722	36.766093
1570.462852	188382.272412	36.771111
1571.774553	188685.468743	36.776128
1573.398574	188990.623617	36.781146
1575.273969	189294.241374	36.786164
1576.495244	189605.125154	36.791181
1578.452302	189911.830593	36.796199
1580.072570	190215.998729	36.801216
1581.157157	190524.518752	36.806234
1583.606015	190829.447818	36.811252
1585.190010	191136.011651	36.816269
1586.582762	191436.789478	36.821287
1588.161006	191740.256888	36.826304
1589.569238	192051.067052	36.831322
1591.544920	192358.741108	36.836340
1593.138505	192679.887342	36.841357
1594.686424	192979.476224	36.846375
1596.224951	193291.843943	36.851392
1597.838923	193602.473354	36.856410
1600.091095	193915.061117	36.861428
1601.017726	194219.525522	36.866445
1602.885641	194534.816617	36.871463
1604.446881	194835.093537	36.876480
1606.343383	195150.610225	36.881498
1608.087692	195454.619262	36.886516
1609.280004	195762.703380	36.891533
1611.180662	196068.289592	36.896551
1613.246846	196381.217001	36.901568
1614.622179	196689.706344	36.906586
1616.240006	196988.658203	36.911604
1617.718257	197301.273214	36.916621
1619.560706	197608.370530	36.921639
1621.445797	197919.449888	36.926656
1622.976562	198226.698870	36.931674
1624.595787	198522.148166	36.936692
1626.390943	198823.971784	36.941709
1627.644262	199122.807152	36.946727
1629.266066	199431.720828	36.951744
1630.943646	199744.639904	36.956762
1632.887842	200041.641548	36.961780
1634.640204	200352.492533	36.966797
1636.218665	200651.229069	36.971815
1637.845421	200955.572482	36.976832
1639.417392	201256.571917	36.981850
1641.262326	201545.793286	36.986868
1642.487895	201843.012212	36.991885
1644.130656	202123.222937	36.996903
1645.604031	202407.702828	37.001920
1647.269650	202697.868650	37.006938
1649.296622	202983.151903	37.011956
1650.472477	203280.330195	37.016973
1652.047899	203561.722207	37.021991
1653.807295	203845.524503	37.027008
1655.177223	204145.645902	37.032026
1656.950658	204435.060871	37.037044
1658.403017	204731.182043	37.042061
1659.937133	205039.712837	37.047079
1661.709817	205344.523355	37.052096
1662.933607	205653.357674	37.057114
1664.803108	205957.747500	37.062132
1666.350542	206270.799771	37.067149
1667.819188	206579.343094	37.072167
1669.605396	206898.226998	37.077184
1671.219246	207216.071404	37.082202
1673.104349	207531.257287	37.087220
1674.723421	207862.870264	37.092237
1676.269203	208178.973834	37.097255
1678.247571	208499.608108	37.102272
1679.698924	208831.731336	37.107290
1681.620258	209153.112082	37.112308
1683.199951	209469.212004	37.117325
1684.710678	209800.819146	37.122343
1686.414171	210121.193648	37.127360
1688.193933	210456.798640	37.132378
1689.553086	210788.506926	37.137396
1691.014015	211129.268713	37.142413
1693.137614	211461.188396	37.147431
1694.862076	211802.748042	37.152448
1696.892423	212147.054596	37.157466
1698.662462	212482.053749	37.162484
1700.341620	212823.774028	37.167501
1701.932632	213158.547862	37.172519
1703.780489	213494.120154	37.177536
1705.170162	213837.919056	37.182554
1707.362831	214172.193255	37.187572
1709.172963	214516.917746	37.192589
1710.752614	214853.015940	37.197607
1712.408197	215189.077135	37.202624
1714.213868	215532.050357	37.207642
1716.173218	215864.838285	37.212660
1718.214195	216215.980666	37.217677
1719.711207	216551.051595	37.222695
1721.706023	216885.054111	37.227712
1723.600284	217227.862338	37.232730
1725.371543	217545.870431	37.237748
1727.204127	217887.901226	37.242765
1728.652116	218215.512174	37.247783
1730.788669	218555.209450	37.252800
1731.889149	218884.373982	37.257818
1734.203861	219217.616538	37.262836
1735.976355	219556.660006	37.267853
1737.705969	219884.456374	37.272871
1739.500544	220211.328174	37.277888
1741.516332	220555.592646	37.282906
1743.161009	220866.610648	37.287924
1744.999577	221189.716139	37.292941
1746.879450	221529.886788	37.297959
1748.540515	221845.754701	37.302976
1750.155511	222170.114863	37.307994
1751.674933	222497.589357	37.313012
1753.422758	222822.487775	37.318029
1755.190471	223146.900466	37.323047
1757.156143	223472.272993	37.328064
1758.765997	223787.666636	37.333082
1760.137895	224093.291575	37.338100
1762.278431	224411.549111	37.343117
1763.701057	224720.163842	37.348135
1765.594509	225030.127537	37.353152
1767.374156	225333.935853	37.358170
1768.731234	225649.064304	37.363188
1770.541696	225974.562877	37.368205
1772.162577	226284.111930	37.373223
1774.124062	226607.452885	37.378240
1775.669274	226938.124511	37.383258
1777.372724	227262.953799	37.388276
1778.957429	227594.940160	37.393293
1780.531536	227934.777973	37.398311
1782.697908	228260.957263	37.403328
1784.305868	228597.436287	37.408346
1786.205341	228932.472379	37.413364
1787.748699	229278.716469	37.418381
1789.432691	229621.559698	37.423399
1791.084382	229956.558015	37.428416
1792.623923	230312.252615	37.433434
1794.597019	230662.010893	37.438452
1796.516478	231020.719604	37.443469
1798.293647	231376.706771	37.448487
1800.504036	231724.445884	37.453504
1802.054733	232095.964509	37.458522
1803.831431	232442.653306	37.463540
1805.511881	232798.502361	37.468557
1807.241253	233170.449596	37.473575
1809.719883	233518.679119	37.478592
1811.342584	233895.215210	37.483610
1813.082289	234252.222547	37.488628
1815.210322	234615.316561	37.493645
1816.720624	234971.673315	37.498663
1818.779138	235333.227968	37.503680
1820.480891	235692.069116	37.508698
1822.599251	236063.038533	37.513716
1824.237133	236431.898052	37.518733
1826.298867	236804.882482	37.523751
1828.215364	237163.739415	37.528768
1829.929407	237526.666827	37.533786
1831.944224	237888.327407	37.538804
1833.703693	238255.413094	37.543821
1835.410082	238631.601123	37.548839
1837.425241	238996.588237	37.553856
1839.387953	239351.294704	37.558874
1841.257599	239725.601351	37.563892
1843.337003	240093.422215	37.568909
1845.403177	240467.900340	37.573927
1846.991130	240823.552694	37.578944
1848.803067	241189.153014	37.583962
1850.276115	241560.623188	37.588980
1852.381934	241915.964364	37.593997
1853.893881	242299.468472	37.599015
1856.200811	242651.449283	37.604032
1857.984622	243028.609693	37.609050
1859.786301	243402.007034	37.614068
1861.755816	243762.167922	37.619085
1863.296995	244143.047869	37.624103
1865.729003	244509.689125	37.629120
1867.668530	244889.387685	37.634138
1869.412983	245250.978445	37.639156
1871.601397	245620.704202	37.644173
1873.128149	245980.981375	37.649191
1875.101989	246354.371936	37.654208
1877.034112	246714.558923	37.659226
1878.885330	247082.937528	37.664244
1880.864533	247444.004848	37.669261
1882.395270	247795.183850	37.674279
1884.527154	248134.125732	37.679296
1886.431479	248475.007758	37.684314
1888.043461	248822.209251	37.689332
1890.106241	249166.113418	37.694349
1891.862390	249522.461173	37.699367
1893.413936	249869.339765	37.704384
1895.407236	250226.715804	37.709402
1897.081861	250581.321293	37.714420
1899.020262	250936.773801	37.719437
1900.871668	251303.085771	37.724455
1902.781885	251661.030453	37.729472
1904.425930	252020.387654	37.734490
1906.325900	252387.680130	37.739508
1908.366113	252752.968430	37.744525
1910.120555	253135.980111	37.749543
1911.834929	253507.642543	37.754560
1913.618169	253882.773255	37.759578
1915.732779	254260.899307	37.764596
1917.986373	254644.311491	37.769613
1919.870175	255023.513054	37.774631
1921.722529	255406.071456	37.779648
1923.726275	255786.369785	37.784666
1925.339612	256184.661308	37.789684
1927.575705	256573.100189	37.794701
1929.061604	256971.612471	37.799719
1931.046782	257355.541495	37.804736
1933.371388	257753.615301	37.809754
1935.110558	258153.862307	37.814772
1937.356012	258534.190903	37.819789
1938.798554	258933.237163	37.824807
1941.319252	259337.422114	37.829824
1943.448147	259732.116457	37.834842
1945.479124	260124.513379	37.839860
1947.382523	260506.133852	37.844877
1949.092120	260920.905170	37.849895
1951.057692	261324.636716	37.854912
1953.186519	261720.137094	37.859930
1955.212849	262112.121531	37.864948
1957.671944	262513.460184	37.869965
1959.352650	262921.878670	37.874983
1961.547233	263308.701765	37.880000
1963.613318	263708.167120	37.885018
1965.507320	264112.001193	37.890036
1967.640492	264502.182269	37.895053
1969.218859	264894.379028	37.900071
1971.498635	265294.592262	37.905088
1973.422436	265689.957615	37.910106
1975.286357	266108.824774	37.915124
1977.360790	266502.715622	37.920141
1979.518666	266899.919076	37.925159
1981.385015	267293.331346	37.930176
1983.389874	267703.000783	37.935194
1985.099450	268102.555323	37.940212
1987.085310	268496.324950	37.945229
1989.038193	268908.156191	37.950247
1991.148720	269313.535246	37.955264
1993.434912	269714.440402	37.960282
1995.291855	270124.808166	37.965300
1997.323112	270525.622662	37.970317
1999.136778	270935.383980	37.975335
2001.413206	271337.451769	37.980352
2003.305693	271734.345946	37.985370
2005.122155	272142.094853	37.990388
2007.377269	272544.617600	37.995405
2009.129924	272953.947294	38.000423
2011.445109	273357.802875	38.005440
2013.335129	273749.481810	38.010458
2014.898756	274143.927431	38.015476
2017.556939	274533.171422	38.020493
2019.108925	274904.326629	38.025511
2020.850379	275287.920105	38.030528
2023.376287	275678.830124	38.035546
2024.978925	276062.822603	38.040564
2027.407682	276453.769461	38.045581
2028.941229	276845.997276	38.050599
2030.663690	277234.079489	38.055616
2032.867606	277632.090306	38.060634
2034.670611	278053.119281	38.065652
2036.565533	278442.412867	38.070669
2038.566177	278861.781201	38.075687
2040.437908	279266.006569	38.080704
2042.731679	279678.950373	38.085722
2044.552086	280095.191095	38.090740
2046.705643	280517.802199	38.095757
2048.716312	280944.140828	38.100775
2050.810346	281353.271992	38.105792
2052.604671	281782.534526	38.110810
2054.763291	282212.931029	38.115828
2056.690632	282638.053816	38.120845
2058.888728	283075.142920	38.125863
2061.000840	283500.206232	38.130880
2062.811744	283948.802969	38.135898
2065.118422	284381.880170	38.140916
2067.088476	284819.019422	38.145933
2069.084850	285262.322241	38.150951
2070.944896	285699.650815	38.155968
2073.306262	286140.224549	38.160986
2075.350263	286597.730979	38.166004
2077.890341	287034.004933	38.171021
2080.124404	287494.751032	38.176039
2081.992597	287933.739518	38.181056
2084.434269	288382.944351	38.186074
2086.447918	288837.037416	38.191092
2088.196295	289281.596235	38.196109
2090.501059	289731.701743	38.201127
2092.485590	290189.293708	38.206144
2094.698491	290636.131695	38.211162
2097.091495	291092.713691	38.216180
2099.371529	291534.177302	38.221197
2101.429529	291983.314948	38.226215
2103.344551	292438.006695	38.231232
2106.042027	292889.576618	38.236250
2108.199212	293345.772440	38.241268
2110.067777	293778.143828	38.246285
2112.466822	294232.568551	38.251303
2114.634162	294692.383131	38.256320
2116.764483	295123.865887	38.261338
2119.049735	295571.823881	38.266356
2121.045131	296031.680201	38.271373
2123.317687	296470.569518	38.276391
2125.240048	296923.169069	38.281408
2127.330169	297370.483476	38.286426
2129.401846	297819.726697	38.291444
2131.899468	298277.201404	38.296461
2133.834535	298718.410951	38.301479
2136.177973	299169.733331	38.306496
2138.373416	299608.508659	38.311514
2140.438484	300059.562645	38.316532
2142.752163	300508.771565	38.321549
2144.548138	300954.376745	38.326567
2146.663388	301402.466895	38.331584
2148.930974	301846.772359	38.336602
2151.087735	302302.286516	38.341620
2153.156732	302740.167620	38.346637
2155.504149	303183.180104	38.351655
2157.582539	303611.025315	38.356672
2159.809400	304026.836774	38.361690
2161.568854	304449.013394	38.366708
2163.470286	304867.813602	38.371725
2165.613995	305298.782267	38.376743
2167.797534	305734.868612	38.381760
2170.098511	306167.836015	38.386778
2172.120871	306608.229886	38.391796
2174.374364	307040.308776	38.396813
2176.066028	307476.456956	38.401831
2178.211031	307918.546112	38.406848
2180.542767	308357.276969	38.411866
2182.690670	308805.779496	38.416884
2184.813651	309252.733487	38.421901
2187.156451	309701.933345	38.426919
2189.130252	310150.780642	38.431936
2191.476039	310601.037672	38.436954
2193.280393	311062.466741	38.441972
2195.595052	311531.857254	38.446989
2197.850470	311989.653396	38.452007
2199.972672	312461.882008	38.457024
2202.429139	312922.810134	38.462042
2204.419037	313393.425675	38.467060
2206.762239	313862.229957	38.472077
2209.355506	314329.924405	38.477095
2211.198568	314808.136884	38.482112
2213.507422	315282.693048	38.487130
2215.732090	315770.454285	38.492148
2217.903859	316237.814329	38.497165
2219.999360	316717.667439	38.502183
2222.376321	317203.688910	38.507200
2224.544094	317678.774688	38.512218
2226.965434	318175.614728	38.517236
2229.457689	318656.526696	38.522253
2231.581837	319139.038925	38.527271
2233.902991	319635.801875	38.532288
2236.242154	320113.904861	38.537306
2238.728510	320606.443712	38.542324
2240.578106	321085.627472	38.547341
2242.661287	321572.940115	38.552359
2245.074153	322062.149440	38.557376
2247.555773	322554.463402	38.562394
2250.111719	323046.962941	38.567412
2252.052712	323537.776675	38.572429
2254.608667	324022.170332	38.577447
2256.923809	324519.460306	38.582464
2259.358344	325015.456919	38.587482
2261.562083	325496.944980	38.592500
2263.847278	325985.112941	38.597517
2266.047578	326473.592754	38.602535
2268.438792	326967.821567	38.607552
2270.801244	327456.492398	38.612570
2272.891216	327955.170776	38.617588
2275.087592	328440.481110	38.622605
2277.519355	328930.416855	38.627623
2279.958635	329429.605482	38.632640
2282.013837	329905.482035	38.637658
2284.291098	330404.429828	38.642676
2286.849690	330899.623256	38.647693
2289.250243	331398.665767	38.652711
2291.122038	331892.939077	38.657728
2294.164586	332375.074334	38.662746
2296.097832	332869.832723	38.667764
2298.274643	333362.415651	38.672781
2300.309479	333849.611090	38.677799
2302.662506	334354.963975	38.682816
2305.044465	334836.257836	38.687834
2307.684474	335329.706330	38.692852
2309.950073	335799.438807	38.697869
2311.675411	336262.198127	38.702887
2314.111998	336732.247051	38.707904
2316.270023	337193.202061	38.712922
2318.623032	337667.006034	38.717940
2320.643383	338136.493158	38.722957
2323.275638	338603.950776	38.727975
2325.543312	339085.942056	38.732992
2327.867385	339563.352596	38.738010
2329.833179	340050.881925	38.743028
2332.159175	340529.319068	38.748045
2334.565373	341019.606781	38.753063
2336.388013	341509.776044	38.758080
2338.718643	341999.453191	38.763098
2341.234408	342507.456092	38.768116
2343.608545	343004.137368	38.773133
2346.014338	343511.559437	38.778151
2348.356939	344011.299764	38.783168
2351.034801	344509.078369	38.788186
2352.815397	345018.782214	38.793204
2355.115992	345528.726739	38.798221
2357.669625	346056.654019	38.803239
2360.016549	346576.186406	38.808256
2362.304338	347089.862318	38.813274
2364.913811	347610.605465	38.818292
2366.791309	348133.204592	38.823309
2369.456145	348652.401296	38.828327
2371.792731	349190.328757	38.833344
2374.713471	349715.858422	38.838362
2376.937921	350241.919591	38.843380
2379.471625	350766.630772	38.848397
2381.855495	351302.436873	38.853415
2384.355178	351846.861748	38.858432
2386.596190	352359.955208	38.863450
2389.108267	352901.799490	38.868468
2391.285965	353426.091907	38.873485
2394.068328	353964.148914	38.878503
2396.406889	354506.576029	38.883520
2399.115747	355043.789481	38.888538
2401.471987	355583.888211	38.893556
2403.962819	356115.413320	38.898573
2406.426548	356646.249112	38.903591
2408.753382	357194.284450	38.908608
2411.263221	357729.986925	38.913626
2413.920803	358258.102924	38.918644
2416.272505	358802.049808	38.923661
2418.798139	359337.975103	38.928679
2421.610037	359869.765165	38.933696
2424.027020	360403.255200	38.938714
2426.479702	360930.342793	38.943732
2428.706219	361477.834940	38.948749
2431.151603	362010.125974	38.953767
2433.548008	362548.675450	38.958784
2435.994180	363074.332101	38.963802
2438.613902	363622.635560	38.968820
2440.826210	364152.972902	38.973837
2443.280072	364683.364220	38.978855
2445.901755	365233.157789	38.983872
2448.339353	365776.304627	38.988890
2450.843986	366294.544779	38.993908
2453.091446	366843.200520	38.998925
2455.885024	367381.978642	39.003943
2458.058273	367926.798703	39.008960
2460.607627	368452.848409	39.013978
2463.505688	368988.108169	39.018996
2465.514646	369533.531213	39.024013
2468.077294	370071.306122	39.029031
2470.529276	370602.753446	39.034048
2472.846684	371102.944804	39.039066
2475.447573	371612.077610	39.044084
2478.124636	372126.535246	39.049101
2480.324407	372627.528290	39.054119
2482.545033	373143.153168	39.059136
2484.766146	373656.994797	39.064154
2487.488797	374166.289357	39.069172
2489.651406	374674.293930	39.074189
2491.834472	375204.655803	39.079207
2494.381326	375731.479682	39.084224
2496.817755	376261.857173	39.089242
2499.239985	376792.986394	39.094260
2501.892547	377327.716872	39.099277
2504.124741	377871.849731	39.104295
2506.522085	378412.247291	39.109312
2508.889503	378959.731054	39.114330
2511.311160	379499.266689	39.119348
2513.830791	380063.776119	39.124365
2516.270311	380621.421782	39.129383
2518.635894	381176.306307	39.134400
2521.112655	381744.484047	39.139418
2524.021272	382316.026293	39.144436
2526.447914	382904.042974	39.149453
2528.948416	383478.662473	39.154471
2531.425027	384041.369814	39.159488
2534.158850	384624.157900	39.164506
2536.689740	385195.391120	39.169524
2538.979343	385789.314042	39.174541
2541.581833	386368.208029	39.179559
2544.358711	386955.291286	39.184576
2546.371263	387547.392821	39.189594
2549.532614	388131.450992	39.194612
2551.666471	388729.683916	39.199629
2554.318086	389318.123776	39.204647
2556.907515	389920.130673	39.209664
2559.492517	390525.870753	39.214682
2562.261893	391121.591588	39.219700
2565.123537	391724.321806	39.224717
2567.640268	392323.901087	39.229735
2570.212411	392929.684741	39.234752
2573.023683	393535.517073	39.239770
2575.778109	394127.774080	39.244788
2578.247766	394747.299525	39.249805
2580.869656	395343.141874	39.254823
2583.969655	395938.489524	39.259840
2586.737001	396539.038054	39.264858
2589.211389	397138.149053	39.269876
2591.704048	397746.708426	39.274893
2594.583614	398336.208453	39.279911
2597.160587	398941.787562	39.284928
2599.518784	399541.361513	39.289946
2602.632794	400136.195579	39.294964
2605.427008	400740.782704	39.299981
2607.825677	401337.621146	39.304999
2610.317034	401926.786937	39.310016
2612.815907	402524.388669	39.315034
2615.480531	403123.315337	39.320052
2618.142785	403730.526599	39.325069
2620.907210	404326.723618	39.330087
2623.689221	404929.430460	39.335104
2626.290215	405528.556485	39.340122
2628.686245	406116.515028	39.345140
2631.795283	406729.243257	39.350157
2634.595577	407326.923671	39.355175
2637.117322	407909.805711	39.360192
2639.782264	408510.562021	39.365210
2642.697414	409098.917060	39.370228
2645.149057	409679.233470	39.375245
2647.671954	410248.847871	39.380263
2650.484055	410809.548329	39.385280
2652.886718	411360.635273	39.390298
2655.660752	411908.361745	39.395316
2658.107504	412479.750943	39.400333
2660.734149	413034.655677	39.405351
2663.182537	413591.648059	39.410368
2665.265348	414169.979753	39.415386
2668.045714	414733.163177	39.420404
2670.090178	415318.096350	39.425421
2672.773249	415902.660657	39.430439
2675.722331	416489.241031	39.435456
2678.090111	417087.377417	39.440474
2680.617706	417681.476222	39.445492
2683.152331	418281.525077	39.450509
2685.937329	418891.480737	39.455527
2688.546591	419500.181730	39.460544
2690.827178	420110.079459	39.465562
2693.796730	420725.667045	39.470580
2696.392549	421353.684006	39.475597
2698.862162	421980.184556	39.480615
2701.499869	422613.870543	39.485632
2704.269768	423247.667930	39.490650
2706.585547	423879.494160	39.495668
2709.540960	424536.025962	39.500685
2711.948395	425177.151167	39.505703
2714.599817	425828.885461	39.510720
2717.415511	426495.486879	39.515738
2720.158979	427136.699353	39.520756
2723.015659	427813.411854	39.525773
2725.577687	428473.465764	39.530791
2728.516857	429144.913365	39.535808
2731.057672	429817.209248	39.540826
2733.759483	430498.807955	39.545844
2736.811270	431163.800514	39.550861
2739.450783	431845.311670	39.555879
2742.356133	432514.627824	39.560896
2744.968323	433204.131661	39.565914
2748.105153	433890.193529	39.570932
2750.658983	434566.518464	39.575949
2753.372523	435251.284251	39.580967
2756.501591	435939.295707	39.585984
2759.379894	436618.175817	39.591002
2762.144753	437308.974043	39.596020
2765.175290	438006.172929	39.601037
2768.060946	438681.037234	39.606055
2771.062240	439365.812213	39.611072
2773.946615	440056.440928	39.616090
2776.985965	440730.348898	39.621108
2779.706458	441410.698070	39.626125
2782.322954	442097.049943	39.631143
2785.085984	442767.947110	39.636160
2787.916264	443448.406579	39.641178
2791.018714	444130.162161	39.646196
2793.647705	444811.815013	39.651213
2796.203759	445493.706478	39.656231
2799.603136	446171.703376	39.661248
2802.291803	446855.694904	39.666266
2805.041382	447531.571195	39.671284
2807.941981	448216.892271	39.676301
2810.433320	448897.656209	39.681319
2813.517001	449569.162341	39.686336
2816.369489	450256.433078	39.691354
2819.368847	450938.050029	39.696372
2822.284621	451613.443936	39.701389
2825.089729	452295.998570	39.706407
2828.092486	452958.100277	39.711424
2830.841828	453635.260628	39.716442
2833.668116	454280.933447	39.721460
2836.305688	454918.081115	39.726477
2838.604723	455560.911983	39.731495
2841.726305	456195.766911	39.736512
2844.722031	456842.126305	39.741530
2847.029593	457482.007968	39.746548
2849.649796	458129.135196	39.751565
2852.283802	458793.849240	39.756583
2855.348804	459447.771494	39.761600
2857.771819	460121.651965	39.766618
2860.713258	460782.557087	39.771636
2863.300781	461456.409681	39.776653
2865.833816	462125.652456	39.781671
2869.325689	462811.318861	39.786688
2871.768425	463495.607921	39.791706
2874.689228	464181.762085	39.796724
2877.743206	464874.123183	39.801741
2880.101019	465564.496209	39.806759
2883.508389	466269.608452	39.811776
2886.079202	466981.026202	39.816794
2888.727987	467686.701463	39.821812
2891.573280	468395.140523	39.826829
2894.246375	469117.446237	39.831847
2897.422237	469829.655612	39.836864
2900.329247	470565.075003	39.841882
2903.093909	471287.623948	39.846900
2906.118924	472022.404575	39.851917
2909.174203	472760.979617	39.856935
2912.235876	473486.006597	39.861952
2914.921789	474233.648407	39.866970
2918.121764	474968.671344	39.871988
2921.160562	475709.382901	39.877005
2923.765048	476452.648821	39.882023
2926.946356	477197.554360	39.887040
2930.275461	477943.813391	39.892058
2933.115324	478687.895936	39.897076
2936.152821	479426.519309	39.902093
2939.238849	480177.549835	39.907111
2942.529371	480927.655726	39.912128
2945.221532	481676.760956	39.917146
2948.231894	482424.067111	39.922164
2951.444183	483171.255466	39.927181
2954.371957	483921.626951	39.932199
2957.560606	484662.498819	39.937216
2960.163585	485409.876033	39.942234
2963.225493	486161.377367	39.947252
2966.421150	486913.727848	39.952269
2969.347934	487670.919658	39.957287
2972.857343	488413.222846	39.962304
2975.936031	489170.669010	39.967322
2979.047703	489909.132970	39.972340
2981.930494	490647.949246	39.977357
2984.925471	491407.311225	39.982375
2988.354218	492137.910586	39.987392
2990.978770	492883.003170	39.992410
2994.009525	493626.685811	39.997428
2997.231677	494373.171683	40.002445
3000.276789	495122.215745	40.007463
3003.459226	495854.584891	40.012480
3006.256648	496599.967682	40.017498
3009.494193	497339.554950	40.022516
3012.691336	498075.839039	40.027533
3015.460456	498803.444210	40.032551
3018.372061	499542.266524	40.037568
3021.818066	500289.122109	40.042586
3024.782605	501034.303287	40.047604
3027.650381	501758.624681	40.052621
3030.399805	502486.149237	40.057639
3033.412895	503183.149242	40.062656
3036.185199	503896.356959	40.067674
3039.079993	504595.672035	40.072692
3042.054049	505299.821322	40.077709
3044.950316	506011.143060	40.082727
3048.049588	506707.354021	40.087744
3050.406355	507439.216133	40.092762
3053.674292	508150.020335	40.097780
3056.397997	508873.349445	40.102797
3059.289622	509596.162405	40.107815
3062.569089	510325.919457	40.112832
3065.701264	511069.845259	40.117850
3068.848755	511809.303119	40.122868
3071.406237	512547.657249	40.127885
3074.493885	513300.171296	40.132903
3077.593160	514056.464381	40.137920
3080.605347	514810.718325	40.142938
3083.342906	515568.845513	40.147956
3086.474555	516336.271202	40.152973
3089.039583	517106.960090	40.157991
3092.084890	517890.048174	40.163008
3095.342158	518684.519481	40.168026
3098.137719	519481.730881	40.173044
3101.410284	520268.416265	40.178061
3104.674147	521070.889201	40.183079
3107.612531	521870.299506	40.188096
3110.619020	522676.938458	40.193114
3113.933887	523489.812265	40.198132
3117.164328	524304.860702	40.203149
3119.926634	525132.795188	40.208167
3123.707804	525947.355337	40.213184
3126.529071	526769.651748	40.218202
3129.491527	527600.716350	40.223220
3132.783285	528424.895593	40.228237
3135.757127	529256.858336	40.233255
3139.245284	530093.358806	40.238272
3142.718518	530933.775585	40.243290
3145.920196	531768.304823	40.248308
3149.298874	532597.379533	40.253325
3152.332566	533436.196413	40.258343
3155.712403	534269.281105	40.263360
3158.595373	535106.506470	40.268378
3161.973880	535951.180424	40.273396
3165.684124	536771.198843	40.278413
3168.732504	537618.575123	40.283431
3171.880356	538453.080034	40.288448
3175.289107	539286.435237	40.293466
3178.358223	540115.271788	40.298484
3181.604265	540961.439914	40.303501
3184.331559	541807.582021	40.308519
3187.987821	542640.024217	40.313536
3191.256323	543486.821227	40.318554
3194.204948	544332.105635	40.323572
3197.823686	545169.602472	40.328589
3200.891907	546019.268312	40.333607
3204.115635	546854.405421	40.338624
3207.362107	547695.451022	40.343642
3210.689765	548531.561555	40.348660
3214.169791	549368.142895	40.353677
3217.576027	550209.893730	40.358695
3220.731553	551042.098543	40.363712
3224.157831	551875.307141	40.368730
3227.172865	552721.006603	40.373748
3230.581411	553544.727726	40.378765
3233.619542	554387.048326	40.383783
3236.977088	555219.134689	40.388800
3240.285361	556042.098975	40.393818
3242.989385	556865.351723	40.398836
3246.594507	557669.463309	40.403853
3249.844406	558464.355542	40.408871
3252.859596	559254.120192	40.413888
3256.044300	560038.795165	40.418906
3258.716699	560835.372226	40.423924
3261.732408	561630.489117	40.428941
3264.811959	562438.867490	40.433959
3268.248343	563255.299237	40.438976
3271.508260	564066.592599	40.443994
3274.562092	564890.232598	40.449012
3277.954993	565711.407477	40.454029
3280.534426	566532.000414	40.459047
3283.646234	567363.468169	40.464064
3286.723741	568207.999758	40.469082
3290.032183	569062.046035	40.474100
3293.494764	569911.398934	40.479117
3296.234735	570768.761176	40.484135
3299.782176	571628.635810	40.489152
3303.206975	572502.629220	40.494170
3306.233246	573388.579022	40.499188
3309.587369	574256.342610	40.504205
3312.906454	575145.612110	40.509223
3316.240203	576022.200167	40.514240
3319.623766	576911.470159	40.519258
3322.974961	577809.079316	40.524276
3326.192926	578706.287061	40.529293
3329.318965	579611.790249	40.534311
3332.759794	580523.572464	40.539328
3336.292731	581429.563992	40.544346
3339.599592	582347.768407	40.549364
3343.068715	583252.070130	40.554381
3346.613465	584173.985303	40.559399
3350.000209	585092.847981	40.564416
3353.641744	586013.693222	40.569434
3357.317512	586940.153789	40.574452
3360.494775	587845.221028	40.579469
3363.922086	588766.116614	40.584487
3367.481170	589682.815357	40.589504
3370.790011	590608.669681	40.594522
3373.944596	591522.177032	40.599540
3377.497122	592449.783229	40.604557
3380.429580	593388.496268	40.609575
3384.230801	594320.047588	40.614592
3387.968178	595249.829108	40.619610
3391.298971	596182.139827	40.624628
3394.943239	597104.431511	40.629645
3398.404423	598028.518798	40.634663
3402.132006	598962.818852	40.639680
3405.843392	599889.649280	40.644698
3408.873322	600817.951906	40.649716
3412.625376	601733.330326	40.654733
3416.440747	602653.609627	40.659751
3420.063196	603577.929999	40.664768
3423.211872	604489.366830	40.669786
3426.595425	605409.718303	40.674804
3430.379656	606322.390836	40.679821
3433.963691	607239.703303	40.684839
3437.375622	608157.658991	40.689856
3441.293966	609064.479196	40.694874
3444.486250	609978.215278	40.699892
3447.607822	610873.377648	40.704909
3451.113498	611790.592297	40.709927
3454.796668	612703.657122	40.714944
3458.513988	613594.696023	40.719962
3461.718008	614504.730931	40.724980
3465.192043	615415.289224	40.729997
3468.773064	616316.526596	40.735015
3471.993692	617203.347167	40.740020
3475.609616	618054.810642	40.745024
3478.650235	618874.716309	40.750029
3481.721648	619626.159248	40.755034
3484.704125	620315.617549	40.760039
3487.408864	620969.906650	40.765044
3490.707621	621559.278846	40.770048
3493.266736	622092.244894	40.775053
3495.537548	622563.998922	40.780058
3498.169814	622996.171800	40.785063
3499.888521	623374.985565	40.790068
3502.763769	623697.426255	40.795072
3504.279364	623997.348784	40.800077
3506.186669	624225.097719	40.805082
3507.873795	624406.289133	40.810087
3509.260937	624565.254706	40.815092
3510.717891	624695.446724	40.820096
3512.106610	624778.863100	40.825101
3513.305714	624818.270166	40.830106
3514.425626	624838.915797	40.835111
3515.253646	624826.353661	40.840116
3516.718093	624780.188861	40.845120
3517.360324	624720.321616	40.850125
3518.151122	624630.372340	40.855130
3518.741986	624511.792769	40.860135
3519.113538	624386.754853	40.865140
3519.496146	624228.258495	40.870144
3520.455082	624073.464453	40.875149
3521.116614	623895.594681	40.880154
3521.629242	623710.953703	40.885159
3522.016550	623491.572856	40.890164
3522.495310	623265.580994	40.895168
3522.260456	623030.306922	40.900173
3522.266902	622785.450870	40.905178
3522.546412	622539.047779	40.910183
3523.039041	622288.809535	40.915188
3523.695994	622024.105349	40.920192
3523.301530	621742.377097	40.925197
3523.554747	621461.288746	40.930202
3523.705515	621178.260404	40.935207
3523.373451	620887.806920	40.940212
3523.286870	620598.605256	40.945216
3523.150856	620309.652621	40.950221
3522.927352	620010.664375	40.955226
3523.091066	619719.199875	40.960231
3522.930073	619421.732711	40.965236
3523.131360	619119.703683	40.970240
3522.934425	618828.669061	40.975245
3522.863304	618520.769065	40.980250
3522.951395	618214.733258	40.985255
3522.527450	617910.816650	40.990260
3522.547408	617607.520902	40.995264
3522.354981	617308.346509	41.000269
3522.347378	617008.684523	41.005274
3521.696593	616705.516170	41.010279
3521.480837	616409.366713	41.015284
3521.814665	616111.923194	41.020288
3521.385940	615823.685589	41.025293
3520.925056	615520.351666	41.030298
3521.159467	615241.089445	41.035303
3520.725175	614950.028791	41.040308
3521.022731	614660.544653	41.045312
3520.445145	614375.937344	41.050317
3519.711837	614080.749679	41.055322
3519.861773	613809.858227	41.060327
3519.595209	613534.175873	41.065332
3519.598242	613251.645428	41.070336
3519.349468	612984.893175	41.075341
3519.053682	612707.443156	41.080346
3519.071199	612447.433848	41.085351
3518.937592	612180.742341	41.090356
3518.554208	611901.334142	41.095360
3518.673486	611642.888092	41.100365
3518.574629	611382.619643	41.105370
3517.897141	611120.685012	41.110375
3517.718188	610859.165682	41.115380
3517.295679	610606.527935	41.120384
3517.248031	610373.876323	41.125389
3517.047696	610119.341642	41.130394
3516.554380	609886.148500	41.135399
3516.548843	609646.072940	41.140404
3516.457506	609404.804964	41.145408
3516.240045	609166.201443	41.150413
3516.227266	608931.011005	41.155418
3515.670644	608705.752276	41.160423
3515.119774	608480.337644	41.165428
3515.319851	608254.900671	41.170432
3515.133344	608046.023768	41.175437
3514.493782	607825.209837	41.180442
3514.867175	607610.934942	41.185447
3514.461175	607407.331006	41.190452
3514.459900	607188.404252	41.195456
3514.231768	606985.114255	41.200461
3513.934246	606788.833887	41.205466
3514.069453	606575.324908	41.210471
3513.638668	606379.407699	41.215476
3513.721635	606177.003499	41.220480
3513.171917	605979.846696	41.225485
3513.001539	605783.227113	41.230490
3512.999168	605598.783820	41.235495
3512.607260	605416.749378	41.240500
3512.337194	605230.140163	41.245504
3512.355816	605050.836631	41.250509
3512.416638	604873.524562	41.255514
3512.398896	604708.479123	41.260519
3511.918626	604520.789285	41.265524
3511.870299	604336.630813	41.270528
3511.604426	604177.419388	41.275533
3511.298644	604004.652671	41.280538
3511.575076	603840.297896	41.285543
3511.128292	603674.652589	41.290548
3511.031987	603505.297221	41.295552
3510.996448	603350.540312	41.300557
3510.612484	603197.136537	41.305562
3510.645004	603037.160421	41.310567
3510.578457	602885.954144	41.315572
3510.221554	602730.787884	41.320576
3509.982645	602589.211847	41.325581
3509.840951	602444.315976	41.330586
3509.967709	602302.678875	41.335591
3509.891492	602159.470220	41.340596
3509.891647	602010.993127	41.345600
3509.627665	601873.314633	41.350605
3509.474891	601736.617824	41.355610
3509.294125	601608.781579	41.360615
3509.070685	601473.793901	41.365620
3509.062964	601333.215605	41.370624
3509.117564	601208.490582	41.375629
3508.337691	601074.635711	41.380634
3508.378703	600957.016570	41.385639
3508.112567	600836.741486	41.390644
3508.238573	600709.697100	41.395648
3508.385276	600589.254532	41.400653
3508.071037	600472.686476	41.405658
3508.205091	600356.597601	41.410663
3507.782078	600254.258609	41.415668
3508.034310	600130.440808	41.420672
3507.821449	600018.807009	41.425677
3507.806568	599905.639472	41.430682
3507.951750	599800.454292	41.435687
3507.156520	599686.855791	41.440692
3507.146677	599574.084321	41.445696
3507.438410	599482.087500	41.450701
3507.141581	599373.463267	41.455706
3507.160769	599270.695147	41.460711
3507.169654	599171.081207	41.465716
3507.311559	599066.339691	41.470720
3506.855791	598971.051355	41.475725
3506.925178	598871.725464	41.480730
3507.278019	598764.845525	41.485735
3507.183771	598669.047407	41.490740
3507.064758	598563.440604	41.495744
3506.588614	598472.255818	41.500749
3506.545656	598370.740115	41.505754
3506.592816	598285.328984	41.510759
3506.460416	598198.643635	41.515764
3506.422223	598096.323559	41.520768
3505.891029	598011.401113	41.525773
3505.987611	597918.770316	41.530778
3506.104390	597819.777528	41.535783
3506.291386	597750.510591	41.540788
3506.301841	597666.952534	41.545792
3505.736912	597583.183378	41.550797
3505.444000	597505.128469	41.555802
3505.681647	597412.220848	41.560807
3505.855067	597336.945505	41.565812
3506.124204	597263.957690	41.570816
3505.689246	597179.414021	41.575821
3505.847009	597097.931212	41.580826
3506.012726	597010.138091	41.585831
3505.991360	596930.884944	41.590836
3505.530474	596845.841984	41.595840
3505.646088	596764.012715	41.600845
3505.438313	596681.482340	41.605850
3505.579635	596611.063495	41.610855
3505.156012	596539.630975	41.615860
3505.487365	596464.374800	41.620864
3505.153181	596398.184648	41.625869
3504.919482	596325.619454	41.630874
3504.725486	596254.800026	41.635879
3504.854131	596184.430396	41.640884
3505.047629	596107.390682	41.645888
3504.737070	596054.163137	41.650893
3504.526570	595977.085489	41.655898
3504.366932	595913.468757	41.660903
3504.524790	595865.825196	41.665908
3504.678668	595801.708131	41.670912
3504.618522	595740.678590	41.675917
3504.359819	595673.620867	41.680922
3504.654830	595629.159495	41.685927
3504.279002	595567.727646	41.690932
3504.552176	595497.130566	41.695936
3504.322135	595441.684094	41.700941
3504.501454	595386.023115	41.705946
3504.321060	595316.797683	41.710951
3504.437123	595266.353764	41.715956
3504.492012	595198.643113	41.720960
3504.134383	595139.208960	41.725965
3504.269120	595089.812877	41.730970
3504.486762	595028.184977	41.735975
3504.282848	594980.694153	41.740980
3503.962807	594915.894677	41.745984
3504.115485	594860.285186	41.750989
3504.290132	594814.837682	41.755994
3504.391492	594750.171629	41.760999
3504.223126	594700.520655	41.766004
3504.273421	594630.653755	41.771008
3504.207703	594577.280369	41.776013
3504.249867	594520.184022	41.781018
3504.057830	594463.775009	41.786023
3504.597729	594406.850640	41.791028
3504.249970	594350.365211	41.796032
3503.728045	594296.661098	41.801037
3504.038026	594248.435630	41.806042
3504.239346	594195.018582	41.811047
3503.918215	594139.379235	41.816052
3504.123466	594084.208198	41.821056
3503.780430	594029.623398	41.826061
3504.268712	593974.708036	41.831066
3504.177811	593910.617837	41.836071
3503.927602	593867.586545	41.841076
3503.970763	593805.878686	41.846080
3503.874581	593756.712847	41.851085
3503.745275	593702.243206	41.856090
3503.992496	593655.627513	41.861095
3503.622699	593616.169781	41.866100
3503.698266	593563.820974	41.871104
3503.811321	593522.885083	41.876109
3503.821792	593468.091894	41.881114
3503.593889	593418.844923	41.886119
3503.337251	593374.710800	41.891124
3503.771864	593325.910756	41.896128
3503.477952	593281.281230	41.901133
3503.841509	593241.957893	41.906138
3503.853887	593187.713900	41.911143
3503.842070	593138.231514	41.916148
3503.908239	593085.481152	41.921152
3503.549180	593034.149318	41.926157
3503.271701	592983.706032	41.931162
3503.366341	592937.712093	41.936167
3503.514340	592891.459183	41.941172
3503.515332	592856.498539	41.946176
3503.716992	592813.742964	41.951181
3503.173615	592761.937768	41.956186
3503.404306	592715.220386	41.961191
3503.290695	592673.865893	41.966196
3503.486381	592637.822262	41.971200
3503.089648	592586.794694	41.976205
3503.104295	592539.359002	41.981210
3503.170220	592495.821967	41.986215
3503.344635	592466.542997	41.991220
3503.276772	592405.245116	41.996224
3503.407476	592371.765270	42.001229
3503.015530	592338.216758	42.006234
3503.155636	592292.914188	42.011239
3503.342069	592247.453916	42.016244
3503.422636	592206.918783	42.021248
3503.543154	592179.851399	42.026253
3503.435921	592135.338175	42.031258
3503.066315	592079.795853	42.036263
3503.120808	592047.779526	42.041268
3503.114888	591999.593303	42.046272
3503.254831	591965.960475	42.051277
3502.889299	591911.869277	42.056282
3503.137085	591875.464302	42.061287
3503.233379	591848.850690	42.066292
3503.317546	591804.606719	42.071296
3503.317850	591765.785577	42.076301
3502.839443	591724.534538	42.081306
3503.388674	591681.219194	42.086311
3503.107066	591655.615928	42.091316
3503.595097	591613.411906	42.096320
3503.024559	591573.176534	42.101325
3502.890550	591528.113957	42.106330
3503.343166	591490.423338	42.111335
3503.129155	591457.896203	42.116340
3503.110577	591417.573961	42.121344
3503.233878	591372.720973	42.126349
3502.954980	591339.953157	42.131354
3503.174816	591303.600708	42.136359
3502.806950	591257.671865	42.141364
3502.806635	591222.706097	42.146368
3502.988043	591194.274167	42.151373
3502.755945	591156.038189	42.156378
3502.904104	591112.081930	42.161383
3502.596177	591077.163776	42.166388
3502.903375	591042.349729	42.171392
3502.578568	591018.505022	42.176397
3502.343580	590995.648126	42.181402
3503.366945	590956.062983	42.186407
3502.620063	590929.077950	42.191412
3502.666253	590887.491205	42.196416
3502.784548	590857.014323	42.201421
3503.088713	590823.903304	42.206426
3503.009726	590782.235529	42.211431
3503.037743	590755.179017	42.216436
3503.178119	590712.825428	42.221440
3502.657764	590666.467026	42.226445
3503.054104	590640.104098	42.231450
3502.923455	590588.324067	42.236455
3502.470050	590561.642911	42.241460
3502.903035	590522.198568	42.246464
3502.723066	590481.797852	42.251469
3502.834426	590452.974134	42.256474
3503.055349	590421.427924	42.261479
3502.794075	590385.698664	42.266484
3503.006422	590353.853008	42.271488
3502.630573	590326.507867	42.276493
3502.757685	590284.505356	42.281498
3502.585331	590255.925858	42.286503
3502.193041	590223.072165	42.291508
3502.753534	590193.876949	42.296512
3502.285376	590159.181259	42.301517
3502.177771	590131.994086	42.306522
3502.522974	590104.936455	42.311527
3502.106820	590078.799371	42.316532
3502.230663	590059.040658	42.321536
3502.335464	590031.118631	42.326541
3502.439549	589995.030361	42.331546
3502.452786	589976.591386	42.336551
3502.260149	589943.204628	42.341556
3502.435280	589917.726220	42.346560
3502.431974	589893.979060	42.351565
3502.218711	589863.451001	42.356570
3502.525590	589831.889630	42.361575
3502.558464	589807.335012	42.366580
3502.443375	589776.791361	42.371584
3502.106263	589743.526771	42.376589
3502.288272	589730.471908	42.381594
3502.661359	589700.002026	42.386599
3502.636978	589673.902916	42.391604
3502.538037	589641.602808	42.396608
3502.752887	589621.328053	42.401613
3502.296650	589591.588732	42.406618
3502.417938	589555.997324	42.411623
3502.361699	589527.297538	42.416628
3502.311805	589488.526133	42.421632
3502.659146	589464.172087	42.426637
3502.561145	589435.228074	42.431642
3502.825994	589417.049425	42.436647
3502.576866	589396.295651	42.441652
3502.442408	589353.879487	42.446656
3502.158502	589316.296413	42.451661
3502.412236	589285.443199	42.456666
3502.417006	589252.524475	42.461671
3502.289176	589237.864043	42.466676
3502.389728	589204.479269	42.471680
3502.439172	589179.068873	42.476685
3502.140678	589153.211771	42.481690
3502.325758	589122.669448	42.486695
3502.349992	589098.816027	42.491700
3502.415122	589067.340322	42.496704
3502.531387	589047.029799	42.501709
3502.601531	589024.722271	42.506714
3502.752816	588988.472948	42.511719
3502.382758	588960.021133	42.516724
3502.441669	588927.894633	42.521728
3502.178975	588903.734903	42.526733
3502.277500	588868.295105	42.531738
3502.512818	588838.495704	42.536743
3502.172420	588819.659090	42.541748
3502.292277	588788.675073	42.546752
3502.273219	588763.274410	42.551757
3502.105045	588744.661270	42.556762
3502.620102	588708.604671	42.561767
3502.403404	588686.692030	42.566772
3502.210250	588646.486928	42.571776
3502.445896	588620.394732	42.576781
3502.660170	588601.270602	42.581786
3502.617555	588563.647191	42.586791
3502.467029	588542.024551	42.591796
3502.249198	588509.288686	42.596800
3502.116779	588480.247283	42.601805
3502.067903	588459.510512	42.606810
3502.347304	588439.273560	42.611815
3502.070895	588416.367563	42.616820
3502.743604	588385.245859	42.621824
3502.467087	588370.407065	42.626829
3502.601372	588348.088117	42.631834
3502.447462	588318.398242	42.636839
3502.534453	588284.211029	42.641844
3502.714054	588256.773808	42.646848
3502.580488	588217.810500	42.651853
3502.479323	588188.212238	42.656858
3502.604218	588161.985929	42.661863
3502.252205	588127.115223	42.666868
3502.645840	588095.685559	42.671872
3502.303937	588075.494948	42.676877
3502.351800	588040.160581	42.681882
3502.342593	588003.782728	42.686887
3501.985081	587989.507273	42.691892
3502.092049	587958.122025	42.696896
3502.278274	587939.251661	42.701901
3501.896910	587911.600605	42.706906
3502.198658	587888.552999	42.711911
3502.092009	587874.288285	42.716916
3502.431124	587844.570148	42.721920
3502.240916	587818.542598	42.726925
3502.102334	587786.994802	42.731930
3501.896657	587755.256961	42.736935
3501.890625	587756.159767	42.741940
3502.279911	587723.827722	42.746944
3502.489321	587705.704985	42.751949
3501.903071	587682.946093	42.756954
3501.960002	587660.888379	42.761959
3501.789713	587641.271459	42.766964
3502.146917	587611.148970	42.771968
3502.108338	587590.759705	42.776973
3502.109674	587555.982256	42.781978
3502.035834	587538.053853	42.786983
3502.193159	587515.028034	42.791988
3502.217407	587485.909365	42.796993
3502.035245	587458.626905	42.801997
3501.926629	587443.059029	42.807002
3502.097725	587416.923922	42.812007
3502.000939	587396.894175	42.817012
3502.069552	587379.394248	42.822017
3502.222166	587350.956719	42.827021
3501.840241	587348.861480	42.832026
3502.269852	587308.303501	42.837031
3502.064603	587305.378836	42.842036
3502.455564	587271.441591	42.847041
3502.385115	587243.239101	42.852045
3502.072550	587227.201672	42.857050
3501.981465	587186.173397	42.862055
3501.931664	587171.648308	42.867060
3501.762901	587140.253690	42.872065
3502.001591	587123.779140	42.877069
3501.839707	587103.057443	42.882074
3502.208367	587088.416713	42.887079
3502.291736	587072.818293	42.892084
3502.141425	587045.529817	42.897089
3502.158932	587025.531632	42.902093
3502.007912	586992.680518	42.907098
3502.074858	586968.915966	42.912103
3501.701275	586956.245305	42.917108
3501.981747	586926.884630	42.922113
3502.363814	586915.098074	42.927117
3502.355858	586892.798375	42.932122
3502.341867	586865.989281	42.937127
3502.241494	586840.045570	42.942132
3501.948368	586822.651413	42.947137
3501.953612	586786.166996	42.952141
3501.839954	586773.706063	42.957146
3502.041694	586751.724097	42.962151
3501.621888	586728.536262	42.967156
3501.826820	586711.515101	42.972161
3501.807369	586689.517473	42.977165
3501.966338	586677.164155	42.982170
3502.061840	586635.553369	42.987175
3501.951917	586634.818699	42.992180
3502.158414	586590.233576	42.997185
3502.118992	586578.512549	43.002189
3502.094665	586552.305686	43.007194
3502.069044	586525.196876	43.012199
3501.959042	586515.892380	43.017204
3502.064087	586486.608059	43.022209
3502.109154	586468.208259	43.027213
3501.794464	586435.481282	43.032218
3502.394880	586413.686893	43.037223
3501.901086	586395.371209	43.042228
3502.083640	586378.603610	43.047233
3502.219088	586365.301401	43.052237
3501.433438	586329.490378	43.057242
3501.600886	586311.522233	43.062247
3501.978525	586305.098224	43.067252
3501.812813	586275.454727	43.072257
3501.887951	586271.082671	43.077261
3502.076819	586252.158855	43.082266
3502.223759	586214.998852	43.087271
3501.999480	586204.759725	43.092276
3502.093865	586181.089400	43.097281
3501.786910	586151.217058	43.102285
3501.945760	586141.719861	43.107290
3502.119332	586108.013452	43.112295
3501.965210	586094.455474	43.117300
3502.303215	586070.446117	43.122305
3502.082140	586055.545370	43.127309
3502.210848	586030.415928	43.132314
3501.880406	585996.036192	43.137319
3501.679801	585990.804999	43.142324
3501.509807	585959.256813	43.147329
3501.518420	585946.575344	43.152333
3501.832546	585938.908085	43.157338
3502.139944	585905.430724	43.162343
3501.944679	585893.883680	43.167348
3502.077345	585871.309314	43.172353
3501.966559	585852.231174	43.177357
3501.905869	585830.689331	43.182362
3501.812028	585805.644282	43.187367
3501.978570	585791.233890	43.192372
3502.116667	585765.651298	43.197377
3501.804244	585729.263126	43.202381
3501.946985	585720.569995	43.207386
3501.847164	585708.356278	43.212391
3502.241872	585706.189424	43.217396
3501.813464	585674.029255	43.222401
3502.167815	585658.336331	43.227405
3501.941320	585628.099139	43.232410
3502.053985	585602.770741	43.237415
3501.888488	585582.297317	43.242420
3501.802169	585555.295827	43.247425
3501.836697	585548.373689	43.252429
3501.867044	585528.871958	43.257434
3502.335140	585493.363393	43.262439
3501.800331	585485.527806	43.267444
3501.875977	585453.087704	43.272449
3502.116749	585436.810769	43.277453
3501.784580	585410.248321	43.282458
3502.052847	585386.098003	43.287463
3501.681382	585370.067042	43.292468
3501.859218	585355.754553	43.297473
3501.703290	585332.722978	43.302477
3501.632982	585313.838055	43.307482
3501.385040	585290.720533	43.312487
3501.695142	585277.139089	43.317492
3501.684116	585266.214160	43.322497
3501.837731	585241.880960	43.327501
3501.542088	585234.759630	43.332506
3502.017847	585219.698684	43.337511
3501.408820	585195.384359	43.342516
3502.031590	585182.104773	43.347521
3502.218661	585154.558334	43.352525
3501.993306	585146.473636	43.357530
3502.145967	585115.323673	43.362535
3502.149364	585099.985549	43.367540
3501.612716	585075.759887	43.372545
3501.694294	585058.504825	43.377549
3501.495587	585038.135818	43.382554
3501.474485	585023.803873	43.387559
3501.314199	584999.017977	43.392564
3501.321580	584990.545919	43.397569
3501.645188	584979.618514	43.402573
3501.283576	584971.805602	43.407578
3501.499026	584937.236947	43.412583
3501.267596	584940.430767	43.417588
3501.281217	584938.674203	43.422593
3501.663073	584911.597934	43.427597
3501.051022	584900.315487	43.432602
3501.506361	584899.041221	43.437607
3501.252616	584892.765215	43.442612
3501.617227	584872.257713	43.447617
3501.479351	584858.495166	43.452621
3501.343193	584855.258295	43.457626
3501.938738	584831.857570	43.462631
3501.710255	584828.284258	43.467636
3501.390265	584802.670780	43.472641
3501.939491	584786.394784	43.477645
3501.796018	584772.482631	43.482650
3501.799222	584745.314775	43.487655
3501.777234	584736.245622	43.492660
3501.506879	584712.579015	43.497665
3501.683595	584688.291099	43.502669
3501.451997	584683.966361	43.507674
3501.529051	584661.799190	43.512679
3501.612378	584657.625708	43.517684
3501.603814	584640.033207	43.522689
3502.090750	584617.450999	43.527693
3501.322964	584598.272879	43.532698
3501.627849	584577.673915	43.537703
3501.304918	584565.794548	43.542708
3501.392378	584563.825881	43.547713
3501.570559	584546.204036	43.552717
3501.224733	584546.959727	43.557722
3501.454288	584524.317313	43.562727
3501.311486	584521.281882	43.567732
3501.352137	584489.897026	43.572737
3501.406360	584483.723016	43.577741
3501.491392	584476.140677	43.582746
3501.470452	584443.161305	43.587751
3501.527615	584442.450490	43.592756
3501.231322	584436.632002	43.597761
3501.299328	584413.362982	43.602765
3501.229104	584405.654488	43.607770
3501.523581	584403.252425	43.612775
3501.552724	584396.631156	43.617780
3501.880829	584377.582084	43.622785
3501.795429	584367.068891	43.627789
3501.576296	584349.157960	43.632794
3501.545206	584321.643533	43.637799
3501.679895	584322.073490	43.642804
3501.405502	584289.033024	43.647809
3501.702467	584288.635594	43.652813
3501.838043	584264.603803	43.657818
3501.667541	584233.201096	43.662823
3501.955178	584234.008157	43.667828
3501.528234	584205.903679	43.672833
3501.726201	584192.338426	43.677837
3501.777447	584166.815805	43.682842
3501.797115	584159.945240	43.687847
3501.884526	584138.878184	43.692852
3501.966085	584119.917334	43.697857
3501.833434	584096.578757	43.702861
3501.526972	584079.683580	43.707866
3502.031827	584055.292839	43.712871
3502.010846	584038.102332	43.717876
3501.716300	584021.806731	43.722881
3501.759523	584003.603585	43.727885
3501.744566	583990.071368	43.732890
3501.603763	583956.858634	43.737895
3501.854477	583952.107312	43.742900
3501.553837	583926.187992	43.747905
3501.741191	583909.415866	43.752909
3501.485186	583905.044506	43.757914
3501.969543	583877.147618	43.762919
3501.475214	583869.505047	43.767924
3501.329937	583854.840089	43.772929
3501.468114	583818.625762	43.777933
3501.563132	583819.863995	43.782938
3501.876258	583803.723714	43.787943
3500.969397	583800.055600	43.792948
3501.424893	583781.887893	43.797953
3501.500593	583781.625295	43.802957
3501.543440	583764.173738	43.807962
3501.557608	583735.146909	43.812967
3501.712542	583735.222823	43.817972
3501.744755	583708.499023	43.822977
3501.696281	583693.066784	43.827981
3501.857860	583688.579928	43.832986
3501.873363	583663.863789	43.837991
3501.377844	583644.641430	43.842996
3501.479088	583625.576392	43.848001
3501.620518	583608.159306	43.853005
3501.539345	583592.681908	43.858010
3501.670340	583580.429734	43.863015
3501.471969	583575.096772	43.868020
3501.193129	583541.352937	43.873025
3501.148598	583529.378794	43.878029
3501.375495	583526.886847	43.883034
3501.274360	583531.263816	43.888039
3501.530530	583523.453548	43.893044
3501.260598	583496.325299	43.898049
3500.909344	583485.251264	43.903053
3501.199864	583489.015594	43.908058
3501.247725	583489.459159	43.913063
3501.441427	583462.609256	43.918068
3501.318693	583446.486460	43.923073
3501.658936	583433.700110	43.928077
3501.365513	583431.740654	43.933082
3501.569181	583407.646216	43.938087
3501.151077	583412.473824	43.943092
3501.875700	583406.645580	43.948097
3501.530310	583383.840047	43.953101
3501.380775	583367.220021	43.958106
3501.808843	583341.085140	43.963111
3501.366607	583330.476346	43.968116
3501.511425	583323.736086	43.973121
3501.586970	583297.606081	43.978125
3501.352293	583288.970028	43.983130
3501.419816	583274.521683	43.988135
3501.231104	583265.577640	43.993140
3501.557719	583239.909558	43.998145
3501.658939	583229.616756	44.003149
3501.346321	583217.182872	44.008154
3501.310641	583204.956336	44.013159
3501.366893	583209.559484	44.018164
3500.980592	583190.920828	44.023169
3501.345707	583163.291432	44.028173
3501.263804	583155.383360	44.033178
3501.495430	583155.647817	44.038183
3501.518237	583140.755104	44.043188
3501.489403	583123.564394	44.048193
3501.647992	583113.713700	44.053197
3501.412181	583100.365308	44.058202
3501.399309	583076.554655	44.063207
3501.195627	583067.011210	44.068212
3501.436747	583064.867860	44.073217
3501.392080	583052.291637	44.078221
3501.273515	583039.175501	44.083226
3501.857542	583033.569569	44.088231
3501.716247	583017.047989	44.093236
3501.267632	583000.875220	44.098241
3501.647153	582980.211468	44.103245
3501.655412	582965.621586	44.108250
3502.198526	582959.821484	44.113255
3501.872511	582941.022583	44.118260
3501.695993	582912.925776	44.123265
3501.731835	582899.885601	44.128269
3501.527451	582891.745825	44.133274
3501.744812	582879.529503	44.138279
3501.309548	582863.705372	44.143284
3501.413393	582832.456304	44.148289
3501.374837	582832.963538	44.153293
3501.310882	582817.081294	44.158298
3501.054904	582793.458431	44.163303
3501.528177	582793.835520	44.168308
3501.257246	582786.157266	44.173313
3501.433869	582769.034151	44.178317
3501.426550	582756.802684	44.183322
3501.958083	582741.880037	44.188327
3501.777359	582729.174315	44.193332
3501.679630	582700.563316	44.198337
3501.214386	582693.216174	44.203341
3501.651658	582679.210581	44.208346
3501.908437	582653.602186	44.213351
3501.486770	582639.379883	44.218356
3501.089040	582628.763451	44.223361
3501.504215	582612.705743	44.228365
3501.188884	582598.717434	44.233370
3501.513188	582579.415180	44.238375
3501.318810	582573.078426	44.243380
3501.145380	582569.345364	44.248385
3501.534309	582545.571019	44.253389
3501.127132	582539.016841	44.258394
3501.734154	582535.412432	44.263399
3500.907893	582525.865576	44.268404
3500.893588	582506.666263	44.273409
3501.329119	582495.267694	44.278413
3501.343022	582495.566204	44.283418
3501.180584	582483.809893	44.288423
3501.209331	582476.234977	44.293428
3501.032960	582453.952571	44.298433
3501.160682	582453.481272	44.303437
3501.124491	582441.404372	44.308442
3500.986992	582446.088263	44.313447
3501.379860	582444.973898	44.318452
3501.481155	582425.806508	44.323457
3501.490045	582408.207707	44.328461
3501.185916	582414.572107	44.333466
3501.008106	582389.933465	44.338471
3501.479156	582386.901748	44.343476
3501.382241	582370.622934	44.348481
3501.480046	582360.179451	44.353485
3501.046052	582345.306939	44.358490
3501.179514	582324.630294	44.363495
3501.616226	582328.322036	44.368500
3501.195247	582322.321373	44.373505
3501.539090	582301.461390	44.378509
3501.049573	582285.945719	44.383514
3501.220775	582277.044878	44.388519
3501.148318	582284.275572	44.393524
3501.206311	582267.069954	44.398529
3501.478618	582247.925656	44.403533
3501.477184	582244.867493	44.408538
3501.871517	582237.335533	44.413543
3501.113622	582214.090704	44.418548
3501.124649	582203.560367	44.423553
3501.536434	582196.025651	44.428557
3501.356119	582193.847745	44.433562
3501.330138	582168.332564	44.438567
3501.099145	582167.165292	44.443572
3501.303778	582159.462391	44.448577
3501.448940	582136.326905	44.453581
3501.137648	582127.350962	44.458586
3500.736496	582120.093687	44.463591
3501.097027	582127.808293	44.468596
3501.041515	582129.070249	44.473601
3501.320366	582109.924690	44.478605
3501.594172	582089.526482	44.483610
3501.567296	582081.508764	44.488615
3501.729490	582066.191721	44.493620
3501.641427	582045.298501	44.498625
3501.604068	582032.068199	44.503629
3501.497555	582024.514117	44.508634
3501.547320	582008.061429	44.513639
3501.566522	581998.632624	44.518644
3501.377844	581973.042153	44.523649
3501.398685	581952.482690	44.528653
3501.405166	581958.899068	44.533658
3501.470456	581931.463873	44.538663
3501.509865	581922.633487	44.543668
3501.393338	581925.509388	44.548673
3501.484657	581894.008938	44.553677
3501.444535	581888.048771	44.558682
3501.537095	581876.753320	44.563687
3501.639699	581861.946681	44.568692
3501.296947	581851.320903	44.573697
3501.484168	581842.667895	44.578701
3501.597023	581826.556035	44.583706
3501.567999	581810.616744	44.588711
3501.594529	581802.239513	44.593716
3501.059183	581778.908836	44.598721
3501.175900	581763.799034	44.603725
3501.477115	581754.025107	44.608730
3501.487060	581747.405248	44.613735
3501.676598	581739.353450	44.618740
3501.488028	581729.254967	44.623745
3501.881883	581713.951358	44.628749
3501.092469	581688.303725	44.633754
3501.593598	581672.231219	44.638759
3501.567408	581663.711710	44.643764
3501.167076	581639.106177	44.648769
3501.564137	581636.587209	44.653773
3501.332261	581630.205635	44.658778
3501.400706	581602.568578	44.663783
3501.487779	581596.137125	44.668788
3501.325599	581590.847679	44.673793
3501.216477	581566.697845	44.678797
3501.263690	581562.328284	44.683802
3502.056988	581543.051185	44.688807
3501.820223	581546.447367	44.693812
3501.506547	581520.424140	44.698817
3501.662599	581513.029218	44.703821
3501.307815	581489.820119	44.708826
3501.319007	581464.999448	44.713831
3501.446969	581458.812218	44.718836
3501.218868	581444.006579	44.723841
3501.447614	581430.834236	44.728845
3501.388069	581416.603881	44.733850
3501.818982	581411.823303	44.738855
3501.534600	581386.547270	44.743860
3501.650697	581392.746282	44.748865
3501.718245	581369.521048	44.753869
3501.369676	581366.165932	44.758874
3501.599621	581347.979352	44.763879
3501.370803	581326.755801	44.768884
3501.004791	581311.169309	44.773889
3501.348620	581304.296430	44.778893
3501.418066	581306.942859	44.783898
3501.272820	581281.745115	44.788903
3501.214413	581261.748296	44.793908
3501.133424	581265.972590	44.798913
3501.414414	581275.705826	44.803917
3501.288051	581252.009260	44.808922
3501.281681	581230.901170	44.813927
3501.152079	581224.152392	44.818932
3501.341296	581219.359376	44.823937
3501.406086	581201.649636	44.828941
3501.333361	581188.473993	44.833946
3501.285943	581184.018796	44.838951
3501.208950	581181.122572	44.843956
3500.964496	581157.143421	44.848961
3501.553235	581146.471625	44.853965
3501.186983	581149.687608	44.858970
3501.364906	581140.433821	44.863975
3501.403617	581122.527469	44.868980
3501.550661	581108.715688	44.873985
3501.775681	581099.504645	44.878989
3501.688592	581078.408883	44.883994
3501.337124	581059.911596	44.888999
3501.401655	581063.661951	44.894004
3501.533568	581053.061480	44.899009
3501.724319	581034.730092	44.904013
3501.408490	581026.104948	44.909018
3501.391467	580998.379462	44.914023
3501.390294	580995.671900	44.919028
3501.267206	580982.002473	44.924033
3501.395819	580957.062025	44.929037
3501.193894	580957.093470	44.934042
3501.286539	580946.499036	44.939047
3501.517447	580944.707868	44.944052
3501.061388	580921.613690	44.949057
3501.525711	580907.601634	44.954061
3501.451392	580907.211997	44.959066
3501.669521	580888.224247	44.964071
3501.248578	580874.300399	44.969076
3501.114067	580866.900328	44.974081
3501.567105	580849.279757	44.979085
3500.925246	580840.906002	44.984090
3501.353785	580824.292058	44.989095
3501.480403	580817.302410	44.994100
3501.360631	580803.983238	44.999105
3501.642382	580786.890765	45.004109
3501.372647	580784.676415	45.009114
3501.100113	580762.756626	45.014119
3501.028175	580744.515966	45.019124
3501.349226	580743.061670	45.024129
3501.319897	580733.839943	45.029133
3501.145997	580729.304051	45.034138
3501.162100	580709.495157	45.039143
3501.568739	580700.907244	45.044148
3501.081020	580689.651154	45.049153
3501.383720	580679.525054	45.054157
3501.239810	580676.087589	45.059162
3501.251676	580656.028548	45.064167
3501.152146	580665.922094	45.069172
3501.129979	580654.593190	45.074177
3501.363128	580636.104087	45.079181
3500.918625	580622.183605	45.084186
3501.574627	580617.467787	45.089191
3501.553349	580613.960989	45.094196
3501.379799	580599.998122	45.099201
3501.450467	580571.405429	45.104205
3501.360275	580580.946589	45.109210
3501.301081	580561.650632	45.114215
3501.307319	580538.884530	45.119220
3501.516076	580536.896187	45.124225
3501.424208	580517.504974	45.129229
3501.333820	580512.604935	45.134234
3501.786874	580498.443696	45.139239
3501.400853	580492.336278	45.144244
3501.118083	580475.181146	45.149249
3501.448045	580461.139390	45.154253
3501.361970	580451.976444	45.159258
3501.556714	580441.365568	45.164263
3501.913196	580425.765168	45.169268
3501.581955	580418.295264	45.174273
3501.497274	580392.384016	45.179277
3501.484867	580385.967413	45.184282
3501.541949	580369.711723	45.189287
3501.565049	580357.723568	45.194292
3501.384263	580341.655456	45.199297
3501.561984	580324.077093	45.204301
3501.608756	580312.737063	45.209306
3501.773664	580298.971627	45.214311
3501.851751	580296.552370	45.219316
3501.799312	580273.343597	45.224321
3501.852077	580254.380615	45.229325
3501.759437	580239.151031	45.234330
3501.365361	580220.358133	45.239335
3501.496687	580196.970039	45.244340
3501.229766	580183.021242	45.249345
3501.569919	580166.921584	45.254349
3501.287381	580165.009978	45.259354
3501.193583	580145.116967	45.264359
3501.058550	580123.926594	45.269364
3501.619560	580123.337319	45.274369
3501.425073	580111.984655	45.279373
3501.544759	580091.807450	45.284378
3501.615072	580078.758562	45.289383
3501.355964	580070.123803	45.294388
3501.442065	580055.166897	45.299393
3501.485491	580040.918678	45.304397
3500.903845	580045.622867	45.309402
3501.096793	580030.749515	45.314407
3501.319521	580007.798044	45.319412
3500.928200	579998.331422	45.324417
3501.568609	579988.151901	45.329421
3501.140366	579994.938250	45.334426
3501.317762	579973.648603	45.339431
3501.371439	579953.732195	45.344436
3501.087422	579959.142080	45.349441
3501.226106	579952.450877	45.354445
3500.888277	579930.238773	45.359450
3501.340101	579931.622252	45.364455
3501.688780	579920.284771	45.369460
3501.313492	579910.163669	45.374465
3501.299740	579885.493802	45.379469
3501.327610	579879.672364	45.384474
3501.175782	579868.513366	45.389479
3501.383359	579868.881964	45.394484
3501.376007	579847.119494	45.399489
3501.269175	579838.460749	45.404493
3501.323971	579832.885810	45.409498
3501.229406	579815.399356	45.414503
3501.479351	579791.239668	45.419508
3501.266724	579789.116481	45.424513
3501.631622	579790.714154	45.429517
3500.899171	579778.542608	45.434522
3500.754530	579760.863310	45.439527
3500.562556	579751.465606	45.444532
3500.997263	579753.052371	45.449537
3500.935813	579755.719634	45.454541
3500.858801	579768.569116	45.459546
3500.863421	579763.001986	45.464551
3501.406290	579754.191462	45.469556
3500.883899	579736.370591	45.474561
3500.957326	579719.710222	45.479565
3500.997467	579716.394127	45.484570
3501.022814	579707.764764	45.489575
3501.407963	579707.253109	45.494580
3501.373765	579705.152159	45.499585
3501.450557	579675.653560	45.504589
3501.117382	579678.162731	45.509594
3501.146846	579677.004619	45.514599
3501.191858	579670.929657	45.519604
3501.130839	579644.812377	45.524609
3501.074434	579631.281302	45.529613
3500.999318	579630.741302	45.534618
3501.308602	579637.111686	45.539623
3501.328638	579632.996352	45.544628
3500.965638	579611.389313	45.549633
3500.951721	579587.922350	45.554637
3500.947313	579596.046813	45.559642
3501.084077	579589.706725	45.564647
3501.107338	579591.357835	45.569652
3500.766108	579585.543796	45.574657
3500.889125	579577.902015	45.579661
3501.336325	579561.483863	45.584666
3500.937051	579552.218693	45.589671
3501.091287	579547.580871	45.594676
3501.206064	579539.840056	45.599681
3501.228778	579540.839338	45.604685
3501.107337	579518.642731	45.609690
3501.149294	579508.205295	45.614695
3501.365362	579495.082790	45.619700
3501.013932	579507.925324	45.624705
3501.289143	579489.076706	45.629709
3500.975331	579472.927835	45.634714
3501.037334	579462.537370	45.639719
3501.101102	579458.214543	45.644724
3501.091474	579456.711482	45.649729
3501.172885	579459.857964	45.654733
3501.208322	579440.645562	45.659738
3500.769780	579422.660634	45.664743
3500.682427	579420.417495	45.669748
3500.743607	579414.289717	45.674753
3501.032283	579412.138238	45.679757
3500.792756	579418.444098	45.684762
3500.934755	579425.191794	45.689767
3501.062225	579412.133190	45.694772
3501.429685	579411.223102	45.699777
3501.166782	579396.219573	45.704781
3500.968163	579387.023193	45.709786
3501.141051	579381.730457	45.714791
3501.101913	579372.057798	45.719796
3501.222262	579373.242425	45.724801
3501.375510	579347.893329	45.729805
3501.084708	579341.569793	45.734810
3501.443993	579339.557707	45.739815
3501.286453	579324.988948	45.744820
3500.960686	579296.103910	45.749825
3500.929107	579232.921008	45.754829
3500.824163	579140.211176	45.759834
3500.418529	578997.949159	45.764839
3500.622602	578787.184082	45.769844
3499.885492	578552.238374	45.774849
3499.583977	578261.950613	45.779853
3499.153571	577936.266118	45.784858
3498.758951	577546.867719	45.789863
3498.262001	577121.307480	45.794868
3497.183911	576654.790564	45.799873
3496.735439	576138.394246	45.804877
3495.795543	575597.068690	45.809882
3494.800234	574993.818515	45.814887
3494.008642	574365.318476	45.819892
3492.742979	573685.931212	45.824897
3491.403273	572960.954048	45.829901
3490.332020	572224.347132	45.834906
3488.953350	571420.293626	45.839911
3487.802900	570589.096696	45.844916
3486.562332	569723.522609	45.849921
3485.380592	568810.991637	45.854925
3483.701276	567871.960766	45.859930
3481.994873	566889.431542	45.864935
3480.265389	565870.220807	45.869940
3478.220132	564833.495939	45.874945
3476.657548	563744.929819	45.879949
3474.788273	562639.887616	45.884954
3472.826695	561497.035323	45.889959
3470.822017	560316.555548	45.894964
3468.605847	559111.575641	45.899969
3466.766711	557878.429386	45.904973
3464.153832	556621.659988	45.909978
3461.999349	555344.987594	45.914983
3459.880519	554045.054956	45.919988
3457.436022	552705.626127	45.924993
3455.022343	551335.178713	45.929997
3452.599964	549960.405282	45.935002
3450.245938	548553.688775	45.940007
3447.829448	547118.458908	45.945012
3444.947252	545673.528769	45.950017
3442.301897	544204.249595	45.955021
3439.233530	542712.326533	45.960026
3436.692493	541203.842311	45.965031
3434.370441	539684.878152	45.970036
3430.768841	538152.042251	45.975041
3428.150085	536592.595835	45.980045
3425.559924	535024.900783	45.985050
3422.621821	533437.133391	45.990055
3419.388589	531834.464859	45.995060
3416.402839	530219.273265	46.000065
3413.286412	528589.096209	46.005069
3410.040007	526957.377006	46.010074
3407.020647	525298.168837	46.015079
3404.070376	523635.215882	46.020084
3400.779288	521963.341986	46.025089
3397.624295	520281.916179	46.030093
3393.864618	518583.038706	46.035098
3390.913768	516877.320230	46.040103
3387.604997	515174.267926	46.045108
3384.340977	513461.216941	46.050113
3381.208202	511736.084036	46.055117
3377.592728	509995.532879	46.060122
3373.996430	508257.788756	46.065127
3370.837723	506503.015515	46.070132
3367.210247	504759.954033	46.075137
3363.471685	503003.831550	46.080141
3360.039535	501248.001882	46.085146
3356.469399	499476.235414	46.090151
3353.284647	497705.455227	46.095156
3349.470585	495920.577263	46.100161
3345.972753	494138.110016	46.105165
3342.235106	492356.830047	46.110170
3338.689617	490578.489609	46.115175
3335.389362	488787.578625	46.120180
3331.405815	487009.594664	46.125185
3327.790703	485214.121117	46.130189
3324.152830	483427.737744	46.135194
3320.791338	481637.063537	46.140199
3317.389260	479838.812992	46.145204
3313.365242	478037.270549	46.150209
3309.676011	476224.452780	46.155213
3306.033067	474443.015398	46.160218
3302.491019	472650.849855	46.165223
3299.067903	470839.760521	46.170228
3294.846356	469040.326698	46.175233
3291.389671	467231.372776	46.180237
3287.530007	465430.225339	46.185242
3283.751234	463624.369549	46.190247
3279.939395	461820.349044	46.195252
3276.092218	460034.912546	46.200257
3272.465125	458231.293185	46.205261
3268.673800	456433.887131	46.210266
3265.242797	454636.694592	46.215271
3261.366036	452839.741960	46.220276
3257.281265	451050.333359	46.225281
3253.443041	449250.784336	46.230285
3249.647743	447469.274919	46.235290
3246.219049	445678.824062	46.240295
3242.290509	443896.682040	46.245300
3238.482927	442111.563380	46.250305
3234.697413	440317.355675	46.255309
3230.638077	438544.749374	46.260314
3227.040962	436764.457858	46.265319
3223.270020	434988.738965	46.270324
3219.625038	433219.169884	46.275329
3215.916256	431456.290121	46.280333
3211.952924	429686.095303	46.285338
3207.936313	427913.773553	46.290343
3204.061632	426149.635067	46.295348
3200.340350	424408.178961	46.300353
3196.842008	422630.444096	46.305357
3192.947638	420886.230016	46.310362
3188.595448	419138.898046	46.315367
3185.428639	417391.132833	46.320372
3181.459065	415643.753648	46.325377
3177.883715	413889.423867	46.330381
3173.768518	412148.881397	46.335386
3170.084657	410402.044638	46.340391
3166.560600	408663.261126	46.345396
3162.521195	406945.068939	46.350401
3158.807013	405204.572629	46.355405
3155.024573	403480.594858	46.360410
3151.103092	401760.567435	46.365415
3147.024600	400045.611781	46.370420
3143.530210	398327.849546	46.375425
3139.742380	396616.300662	46.380429
3135.906575	394898.138307	46.385434
3131.764747	393190.509400	46.390439
3127.958193	391490.880426	46.395444
3124.308369	389798.419162	46.400449
3120.928792	388090.694591	46.405453
3116.764704	386409.252017	46.410458
3113.225863	384713.051066	46.415463
3109.502783	383016.334136	46.420468
3105.688554	381331.454146	46.425473
3101.626956	379650.465149	46.430477
3097.911436	377974.901642	46.435482
3094.210376	376301.947756	46.440487
3090.736611	374629.031942	46.445492
3086.742122	372965.238863	46.450497
3082.868438	371293.349793	46.455501
3078.928440	369633.284970	46.460506
3075.284622	367974.752584	46.465511
3071.955191	366316.125167	46.470516
3067.742667	364675.046617	46.475521
3064.130832	363018.383375	46.480525
3060.402719	361380.322435	46.485530
3056.613517	359725.358030	46.490535
3053.104501	358082.940710	46.495540
3049.164975	356439.155520	46.500545
3045.990930	354799.077562	46.505549
3042.132255	353165.426248	46.510554
3038.028243	351536.126836	46.515559
3034.201052	349911.277355	46.520564
3030.650260	348285.591889	46.525569
3027.192203	346658.235725	46.530573
3023.100113	345033.747156	46.535578
3018.951414	343414.783299	46.540583
3015.599658	341796.406891	46.545588
3012.047251	340193.116349	46.550593
3008.456375	338592.098651	46.555597
3004.040356	336981.246284	46.560602
3000.786036	335365.334497	46.565607
2996.912808	333768.319577	46.570612
2992.972748	332175.519890	46.575617
2989.263004	330573.003325	46.580621
2985.769524	328981.883303	46.585626
2981.936264	327401.409770	46.590631
2978.523804	325802.594526	46.595636
2974.476692	324229.966117	46.600641
2971.037949	322651.000662	46.605645
2967.541452	321078.955255	46.610650
2963.349347	319497.623507	46.615655
2959.992643	317918.647458	46.620660
2956.092978	316348.757334	46.625665
2952.603241	314776.941446	46.630669
2948.421332	313210.828253	46.635674
2944.885562	311647.054720	46.640679
2941.602356	310094.157287	46.645684
2937.576997	308540.867631	46.650689
2933.541273	306971.116183	46.655693
2930.044535	305425.662020	46.660698
2926.653523	303873.323788	46.665703
2923.039105	302333.062967	46.670708
2919.292629	300786.593263	46.675713
2915.663854	299237.999203	46.680717
2912.133900	297694.589383	46.685722
2907.921182	296157.505500	46.690727
2904.540061	294612.486974	46.695732
2900.962910	293088.331297	46.700737
2897.151211	291546.431273	46.705741
2893.788652	290014.350141	46.710746
2889.936863	288485.159343	46.715751
2886.709232	286948.783013	46.720756
2882.547116	285420.587183	46.725761
2878.875189	283900.070442	46.730765
2875.020228	282371.020331	46.735770
2871.568506	280852.185431	46.740775
2867.878982	279333.483538	46.745780
2863.842532	277816.689353	46.750785
2860.055053	276296.898542	46.755789
2856.375694	274793.204391	46.760794
2853.010591	273283.704684	46.765799
2849.245778	271776.506763	46.770804
2845.400492	270294.809110	46.775809
2842.181461	268777.086242	46.780813
2838.669771	267293.632965	46.785818
2834.720856	265788.479174	46.790823
2831.073476	264291.607955	46.795828
2827.360592	262806.821198	46.800833
2824.020081	261308.561289	46.805837
2820.125082	259824.985302	46.810842
2816.147600	258333.585571	46.815847
2812.795731	256859.412209	46.820852
2809.175983	255379.610362	46.825857
2805.291818	253904.672280	46.830861
2801.758612	252435.546800	46.835866
2798.189407	250951.667138	46.840871
2794.577317	249488.536039	46.845876
2790.764610	248013.963206	46.850881
2787.210712	246548.658864	46.855885
2783.755796	245074.159366	46.860890
2779.726175	243615.045395	46.865895
2776.107883	242153.030489	46.870900
2772.562837	240695.044677	46.875905
2769.046596	239236.103922	46.880909
2765.417146	237782.139887	46.885914
2761.751754	236325.500709	46.890919
2758.426621	234871.553120	46.895924
2754.175832	233424.214340	46.900929
2750.901166	231966.123567	46.905933
2747.533918	230528.240600	46.910938
2743.772992	229077.580082	46.915943
2739.907325	227637.605430	46.920948
2736.224533	226183.974949	46.925953
2732.657712	224755.769365	46.930957
2729.090124	223308.411351	46.935962
2725.378549	221870.296567	46.940967
2721.859152	220438.979055	46.945972
2717.967576	219017.171072	46.950977
2714.031767	217578.028708	46.955981
2710.712860	216148.497292	46.960986
2706.753835	214730.964366	46.965991
2703.275208	213307.580027	46.970996
2699.276214	211884.359329	46.976001
2696.234017	210461.504906	46.981005
2692.619645	209051.226672	46.986010
2688.801829	207650.156591	46.991015
2685.265441	206241.486895	46.996020
2681.589582	204836.566469	47.001025
2677.890248	203423.178792	47.006029
2674.499657	202009.193143	47.011034
2670.590748	200607.065702	47.016039
2667.049135	199206.216881	47.021044
2663.171782	197809.100220	47.026049
2659.802536	196405.193970	47.031053
2656.110439	195010.519903	47.036058
2652.826490	193619.590754	47.041063
2648.882561	192221.725739	47.046068
2645.210572	190839.469672	47.051073
2642.076894	189445.482415	47.056077
2638.297227	188060.067461	47.061082
2634.775147	186674.629620	47.066087
2631.336028	185289.298712	47.071092
2627.282584	183909.226275	47.076097
2623.991797	182515.863708	47.081101
2620.087650	181136.290964	47.086106
2616.579553	179748.910649	47.091111
2613.067319	178366.492027	47.096116
2609.622950	176990.908431	47.101121
2605.878586	175617.227266	47.106125
2602.063265	174238.907968	47.111130
2597.990450	172881.733949	47.116135
2595.069524	171505.282765	47.121140
2591.193920	170146.483814	47.126145
2587.558471	168787.672147	47.131149
2583.898897	167413.907270	47.136154
2580.329927	166048.365150	47.141159
2576.626103	164681.840053	47.146164
2573.239863	163337.491567	47.151169
2569.516325	161976.880008	47.156173
2565.556696	160626.809188	47.161178
2562.373595	159267.303502	47.166183
2558.843949	157915.263772	47.171188
2554.585225	156582.344445	47.176193
2551.170758	155224.250842	47.181197
2547.717299	153885.272126	47.186202
2544.006904	152547.344807	47.191207
2540.679520	151202.173744	47.196212
2537.139419	149859.893825	47.201217
2533.124235	148524.504071	47.206221
2529.728796	147176.618448	47.211226
2525.958647	145776.807418	47.216231
2522.615989	144440.411403	47.221236
2519.006041	143112.388589	47.226241
2515.584445	141775.795971	47.231245
2512.252661	140453.259665	47.236250
2508.173777	139130.265810	47.241255
2504.641909	137802.961194	47.246260
2501.105634	136478.124931	47.251265
2497.313986	135152.654327	47.256269
2493.871468	133839.355107	47.261274
2490.029373	132507.100670	47.266279
2486.687031	131191.612525	47.271284
2482.710677	129890.052326	47.276289
2479.199305	128563.273334	47.281293
2475.563608	127261.015283	47.286298
2471.732764	125947.508363	47.291303
2468.195991	124646.003964	47.296308
2464.458153	123349.863617	47.301313
2460.948412	122046.251362	47.306317
2457.141314	120753.640261	47.311322
2453.685251	119473.568854	47.316327
2450.119297	118173.998807	47.321332
2446.602146	116885.426880	47.326337
2442.847818	115597.279487	47.331341
2439.294290	114302.418844	47.336346
2435.682904	113021.942606	47.341351
2431.973334	111741.526845	47.346356
2428.730555	110468.000141	47.351361
2425.065539	109191.190611	47.356365
2421.308058	107917.327832	47.361370
2417.337738	106640.837257	47.366375
2413.994590	105365.707040	47.371380
2410.241370	104104.671669	47.376385
2406.641223	102822.584412	47.381389
2403.081037	101567.855655	47.386394
2399.427603	100308.982178	47.391399
2395.536337	99050.677476	47.396404
2391.991884	97794.477311	47.401409
2388.302594	96541.056145	47.406413
2384.936276	95292.285325	47.411418
2381.496462	94048.430122	47.416423
2377.683438	92802.764356	47.421428
2374.075170	91561.843938	47.426433
2370.529214	90309.630405	47.431437
2366.548664	89063.965906	47.436442
2362.802703	87831.873016	47.441447
2359.422487	86605.503949	47.446452
2355.664850	85381.061847	47.451457
2351.942068	84148.217971	47.456461
2348.470286	82924.241534	47.461466
2344.517616	81711.494687	47.466471
2341.080710	80496.127868	47.471476
2337.592848	79286.156162	47.476481
2334.122339	78058.542060	47.481485
2330.629321	76865.695801	47.486490
2326.504890	75648.413642	47.491495
2323.187597	74437.358509	47.496500
2319.136361	73237.050498	47.501505
2315.356480	72036.042839	47.506509
2311.607244	70836.341811	47.511514
2308.157832	69654.373342	47.516519
2304.925092	68468.736214	47.521524
2301.153185	67280.635065	47.526529
2297.381943	66104.382442	47.531533
2294.200743	64920.132275	47.536538
2290.426411	63738.258039	47.541543
2286.873165	62571.173438	47.546548
2283.014391	61392.983544	47.551553
2279.305992	60227.549992	47.556557
2275.550086	59050.699626	47.561562
2271.876544	57890.435666	47.566567
2268.313991	56723.731469	47.571572
2264.648934	55576.299313	47.576577
2261.213497	54417.415382	47.581581
2257.480797	53269.971631	47.586586
2253.739022	52124.818182	47.591591
2250.022756	50969.985637	47.596596
2246.384530	49829.527681	47.601601
2242.865921	48686.138769	47.606605
2239.267639	47561.872603	47.611610
2235.330481	46430.972942	47.616615
2231.587443	45301.082353	47.621620
2227.768612	44185.180369	47.626625
2224.250322	43064.505594	47.631629
2220.551016	41952.507769	47.636634
2217.123821	40854.441289	47.641639
2213.205217	39732.565070	47.646644
2209.165959	38639.054976	47.651649
2206.033622	37545.229866	47.656653
2202.137722	36445.195821	47.661658
2198.538533	35364.430132	47.666663
2194.959258	34273.453549	47.671668
2190.907242	33197.268047	47.676673
2187.227559	32118.594691	47.681677
2183.398412	31051.414732	47.686682
2179.229402	29994.089740	47.691687
2176.029648	28931.039625	47.696692
2171.770013	27888.589597	47.701697
2168.017567	26835.474164	47.706701
2164.065849	25794.324768	47.711706
2160.071323	24768.384717	47.716711
2156.456877	23741.658121	47.721716
2152.292801	22736.451611	47.726721
2148.533993	21732.461311	47.731725
2144.844722	20743.302274	47.736730
2141.004408	19749.801367	47.741735
2136.972545	18768.035201	47.746740
2132.743574	17813.913364	47.751745
2128.836023	16854.550292	47.756749
2124.876372	15919.897515	47.761754
2120.473544	14992.376077	47.766759
2116.389945	14056.177198	47.771764
2111.607163	13168.099672	47.776769
2106.570312	12302.201597	47.781773
2101.484426	11460.189221	47.786778
2096.255969	10652.935530	47.791783
2091.512957	9857.837346	47.796788
2086.248743	9091.934977	47.801793
2081.418805	8364.286412	47.806797
2076.577014	7658.001324	47.811802
2072.184355	6978.350988	47.816807
2067.058697	6322.570961	47.821812
2061.736610	5701.955514	47.826817
2057.695816	5099.718470	47.831821
2053.340463	4532.484640	47.836826
2048.451932	3978.725132	47.841831
2044.144290	3458.032641	47.846836
2038.144309	2993.454750	47.851841
2032.710666	2546.516927	47.856845
2027.839932	2142.592126	47.861850
2022.576432	1754.966667	47.866855
2017.842530	1409.386777	47.871860
2011.901073	1101.581489	47.876865
2006.955707	798.627866	47.881869
2002.532449	551.282597	47.886874
1997.784437	331.384438	47.891879
1992.577359	153.162244	47.896884
1982.694781	146.507797	47.901889
1973.951953	143.642485	47.906893
1968.801298	139.338703	47.911898
1965.759573	150.976595	47.916903
1963.729671	139.647981	47.921908
1962.555233	146.304863	47.926913
1960.663865	143.949392	47.931917
1958.193109	140.918932	47.936922
1955.592644	138.645946	47.941927
1953.060820	134.138036	47.946932
1949.987589	136.994855	47.951937
1946.610676	137.311169	47.956941
1943.333187	134.429097	47.961946
1939.916775	136.523347	47.966951
1937.175222	133.959223	47.971956
1933.849033	140.092243	47.976961
1930.513993	139.373759	47.981965
1927.325451	143.381286	47.986970
1923.702241	150.810509	47.991975
1920.459910	129.373314	47.996980
1916.851464	142.982379	48.001985
1913.633007	141.919781	48.006989
1910.508937	141.636540	48.011994
1906.666214	147.486555	48.016999
1904.109127	129.374914	48.022004
1900.512505	137.632069	48.027009
1897.456861	140.593721	48.032013
1894.333408	134.802135	48.037018
1890.603606	145.927597	48.042023
1887.058278	142.884968	48.047028
1883.863491	138.215057	48.052033
1880.288711	141.542696	48.057037
1877.223293	134.368926	48.062042
1873.490795	135.927347	48.067047
1869.668529	136.819591	48.072052
1866.171285	144.270246	48.077057
1863.101804	143.908872	48.082061
1859.364906	133.581426	48.087066
1855.544361	129.385947	48.092071
1852.442022	126.729605	48.097076
1849.233519	138.444231	48.102081
1845.991590	142.735388	48.107085
1843.067253	126.823167	48.112090
1839.210097	132.884271	48.117095
1835.696877	140.878450	48.122100
1832.535560	135.266822	48.127105
1829.172777	133.600396	48.132109
1825.519837	135.576666	48.137114
1821.690478	134.252184	48.142119
1818.400524	134.709958	48.147124
1814.767842	136.322384	48.152129
1811.418934	140.769500	48.157133
1808.284443	133.258541	48.162138
1804.386669	141.429970	48.167143
1801.086186	130.205330	48.172148
1797.690302	139.987709	48.177153
1794.519765	132.355843	48.182157
1791.579317	123.311704	48.187162
1787.268088	131.614277	48.192167
1783.948182	131.681269	48.197172
1780.649435	135.788340	48.202177
1776.437710	135.732300	48.207181
1773.297632	129.212512	48.212186
1770.004008	138.108838	48.217191
1766.565233	133.106982	48.222196
1762.768764	137.763361	48.227201
1759.557647	135.851754	48.232205
1756.427965	121.585269	48.237210
1752.591114	135.195306	48.242215
1749.492730	131.152616	48.247220
1745.364373	135.481279	48.252225
1741.929968	131.633550	48.257229
1738.813893	127.419622	48.262234
1735.258024	133.772140	48.267239
1732.030977	126.108013	48.272244
1728.015276	137.458593	48.277249
1724.521511	132.332478	48.282253
1721.711774	125.735701	48.287258
1717.778674	129.151104	48.292263
1714.290944	129.586078	48.297268
1710.476499	131.916701	48.302273
1707.402648	130.192443	48.307277
1704.051009	127.572001	48.312282
1700.238987	134.505633	48.317287
1697.409084	123.960387	48.322292
1693.303262	125.042607	48.327297
1689.770799	131.078254	48.332301
1686.493063	120.349994	48.337306
1682.449695	126.146052	48.342311
1679.446429	119.753591	48.347316
1675.866639	128.023987	48.352321
1672.477509	130.547495	48.357325
1669.160581	127.032594	48.362330
1665.237657	135.853422	48.367335
1661.807112	127.806707	48.372340
1658.360488	134.749606	48.377345
1655.096838	126.654627	48.382349
1651.703722	125.736511	48.387354
1647.752816	122.925133	48.392359
1644.729323	117.820367	48.397364
1641.296203	127.266912	48.402369
1638.085841	131.065952	48.407373
1634.584066	125.558302	48.412378
1630.618603	132.215406	48.417383
1626.934120	130.830357	48.422388
1623.105061	130.619574	48.427393
1619.701665	125.393934	48.432397
1616.871404	127.273155	48.437402
1613.044212	136.227716	48.442407
1609.875179	123.033664	48.447412
1606.613772	123.218110	48.452417
1602.336833	131.094591	48.457421
1598.967435	117.295975	48.462426
1595.607044	135.694293	48.467431
1592.227746	122.049091	48.472436
1588.732480	130.562555	48.477441
1585.713015	124.311868	48.482445
1581.750158	122.881819	48.487450
1578.231409	129.051396	48.492455
1574.680133	123.526208	48.497460
1571.157865	124.884146	48.502465
1567.634314	119.427391	48.507469
1564.446157	115.651924	48.512474
1560.574568	124.664065	48.517479
1557.242957	122.157602	48.522484
1553.675413	119.235641	48.527489
1550.522245	119.320904	48.532493
1547.037799	114.082670	48.537498
1543.363576	115.891519	48.542503
1539.717455	115.164905	48.547508
1536.280541	119.284175	48.552513
1532.323775	122.257247	48.557517
1529.369015	119.505145	48.562522
1525.819203	123.964801	48.567527
1522.413352	117.366481	48.572532
1519.023170	120.127487	48.577537
1515.081361	122.772349	48.582541
1511.419464	122.225389	48.587546
1507.985583	124.676855	48.592551
1504.758277	116.437043	48.597556
1501.227387	117.574887	48.602561
1497.693494	115.774003	48.607565
1494.713387	118.954897	48.612570
1491.114207	120.609645	48.617575
1487.961540	113.841995	48.622580
1484.097437	113.348842	48.627585
1480.070472	126.643842	48.632589
1476.796504	111.602784	48.637594
1472.882982	117.134973	48.642599
1469.886651	110.320714	48.647604
1466.137596	119.959123	48.652609
1462.847539	110.352886	48.657613
1459.582399	111.439655	48.662618
1455.721063	122.883207	48.667623
1452.503556	115.249337	48.672628
1449.097630	112.963359	48.677633
1445.169567	111.951873	48.682637
1442.024385	121.837461	48.687642
1438.246858	116.936216	48.692647
1434.310716	108.763094	48.697652
1431.278400	114.201657	48.702657
1427.844852	121.259630	48.707661
1424.687634	110.439853	48.712666
1420.617819	122.871523	48.717671
1417.571925	107.971969	48.722676
1413.772872	113.369198	48.727681
1410.158094	108.932885	48.732685
1407.004950	111.653657	48.737690
1403.315474	111.873537	48.742695
1400.087855	112.739312	48.747700
1396.504676	117.213721	48.752705
1392.790382	123.439270	48.757709
1389.461111	110.055265	48.762714
1385.826698	118.568412	48.767719
1382.282540	121.432659	48.772724
1378.535385	124.005972	48.777729
1375.156724	109.775470	48.782733
1372.316760	113.206548	48.787738
1368.364282	107.889785	48.792743
1364.661577	111.373654	48.797748
1361.567305	119.840224	48.802753
1357.553950	123.670124	48.807757
1354.302779	107.945333	48.812762
1350.456287	121.708837	48.817767
1347.460789	103.447773	48.822772
1344.381378	114.202627	48.827777
1340.670016	116.890576	48.832781
1336.922384	119.789852	48.837786
1333.038638	109.507795	48.842791
1329.789648	105.732444	48.847796
1325.990781	117.473141	48.852801
1322.480076	112.875035	48.857805
1319.366460	116.883650	48.862810
1315.796314	123.140444	48.867815
1312.426749	114.366145	48.872820
1308.705533	116.793050	48.877825
1305.160133	104.119978	48.882829
1301.729517	112.572770	48.887834
1298.014366	118.785827	48.892839
1295.308805	112.157072	48.897844
1291.814486	112.071190	48.902849
1287.865660	116.375078	48.907853
1284.589860	115.052738	48.912858
1280.750457	120.285483	48.917863
1277.331425	108.114671	48.922868
1273.944379	114.020102	48.927873
1270.122481	105.341945	48.932877
1266.775796	115.708377	48.937882
1262.827309	116.857890	48.942887
1260.240223	117.401969	48.947892
1256.532907	117.653170	48.952897
1252.458925	113.216038	48.957901
1249.010381	106.697283	48.962906
1245.396775	113.093780	48.967911
1242.508416	106.560101	48.972916
1239.164243	111.949455	48.977921
1235.137099	115.417718	48.982925
1231.962306	102.183617	48.987930
1228.252016	114.587531	48.992935
1224.707629	107.874977	48.997940
1221.232895	109.848866	49.002945
1217.929576	108.378994	49.007949
1214.242006	103.878226	49.012954
1210.373381	111.156232	49.017959
1207.390753	104.055181	49.022964
1203.945035	109.368690	49.027969
1200.541641	118.949900	49.032973
1197.430523	103.162132	49.037978
1193.082336	106.399089	49.042983
1189.770187	98.077779	49.047988
1186.039814	101.331916	49.052993
1182.722519	109.997959	49.057997
1179.253692	105.475615	49.063002
1175.663513	104.999813	49.068007
1172.147753	107.094038	49.073012
1168.693251	110.918776	49.078017
1165.083740	103.798820	49.083021
1161.899710	103.911186	49.088026
1158.438492	106.433484	49.093031
1154.864241	100.700094	49.098036
1151.888104	101.216523	49.103041
1147.911750	110.431852	49.108045
1144.024112	100.093553	49.113050
1140.378043	104.916417	49.118055
1136.988102	103.517085	49.123060
1133.536316	104.402220	49.128065
1130.186513	104.828457	49.133069
1126.803879	109.407600	49.138074
1123.138639	112.692693	49.143079
1119.792005	107.986724	49.148084
1116.472577	108.009568	49.153089
1112.726937	112.186795	49.158093
1109.784940	107.278271	49.163098
1105.588971	109.722627	49.168103
1102.289147	102.025857	49.173108
1098.956200	103.382791	49.178113
1094.758383	109.975205	49.183117
1091.737911	102.706112	49.188122
1088.075338	104.946740	49.193127
1084.891040	95.099482	49.198132
1081.006211	99.668675	49.203137
1077.638922	108.377373	49.208141
1074.179242	99.512885	49.213146
1070.453440	102.630304	49.218151
1067.322159	101.032309	49.223156
1064.391675	101.133485	49.228161
1060.376853	109.317134	49.233165
1056.805231	102.232424	49.238170
1053.069706	106.917461	49.243175
1049.804274	103.230210	49.248180
1046.225748	99.993786	49.253185
1042.596534	106.946456	49.258189
1039.570989	95.024209	49.263194
1035.499050	99.125995	49.268199
1031.882918	103.991665	49.273204
1028.569639	101.074394	49.278209
1024.923514	108.463160	49.283213
1022.102036	97.217663	49.288218
1018.760209	100.471138	49.293223
1014.492363	98.010218	49.298228
1011.281908	101.037479	49.303233
1007.458075	104.021571	49.308237
1004.074099	96.888523	49.313242
1000.705038	98.365041	49.318247
997.224275	97.283707	49.323252
993.948087	98.407158	49.328257
990.050987	99.165911	49.333261
986.654140	95.110113	49.338266
982.784240	107.200552	49.343271
979.495866	97.860023	49.348276
976.356947	96.288567	49.353281
972.434236	98.576294	49.358285
969.386346	86.100751	49.363290
965.523364	97.506723	49.368295
961.849979	94.968570	49.373300
958.577507	104.886849	49.378305
955.166499	100.083455	49.383309
952.061404	105.245631	49.388314
948.249774	110.189398	49.393319
944.908918	91.141036	49.398324
940.991038	95.759748	49.403329
937.020687	101.294692	49.408333
933.684212	91.942734	49.413338
930.422701	96.354271	49.418343
927.036138	98.289144	49.423348
923.710159	93.674935	49.428353
920.319765	95.752781	49.433357
916.969845	91.034755	49.438362
912.796996	100.486573	49.443367
909.488088	101.805005	49.448372
906.024645	97.661587	49.453377
902.499535	102.051132	49.458381
899.510485	102.291245	49.463386
895.580246	99.834467	49.468391
891.555627	94.336229	49.473396
888.884926	87.002961	49.478401
885.155584	99.776945	49.483405
881.835935	89.922494	49.488410
877.589021	96.623916	49.493415
874.747656	99.185294	49.498420
870.892337	95.903697	49.503425
867.263256	100.758795	49.508429
864.165403	98.899367	49.513434
860.587812	97.412459	49.518439
856.760767	101.817661	49.523444
853.828743	107.281800	49.528449
849.939708	101.240320	49.533453
846.297066	89.228123	49.538458
842.755385	102.621316	49.543463
839.590238	99.712559	49.548468
836.322504	97.265963	49.553473
832.838556	110.428658	49.558477
829.630919	104.179245	49.563482
825.646470	98.880395	49.568487
821.733453	101.460899	49.573492
818.194306	100.762103	49.578497
814.968831	106.999880	49.583501
811.714605	83.508698	49.588506
807.869549	100.429590	49.593511
804.481532	92.655009	49.598516
800.593802	100.129134	49.603521
797.323048	107.155467	49.608525
794.181587	92.087669	49.613530
790.638545	96.717344	49.618535
787.133235	94.406049	49.623540
783.607469	102.374002	49.628545
779.917865	97.677583	49.633549
776.552895	97.454574	49.638554
773.064679	99.949592	49.643559
769.366787	93.508055	49.648564
765.498683	94.717948	49.653569
762.396970	94.928290	49.658573
758.873568	91.733973	49.663578
755.435962	96.423081	49.668583
752.032824	91.647014	49.673588
748.814532	86.095346	49.678593
745.034749	93.169764	49.683597
741.858568	87.484952	49.688602
738.365182	98.959669	49.693607
734.488395	99.389474	49.698612
730.984812	101.197204	49.703617
727.388817	93.790588	49.708621
724.235871	99.396925	49.713626
720.355895	92.351165	49.718631
716.770114	90.919382	49.723636
713.075304	90.950533	49.728641
709.485261	100.241552	49.733645
706.605020	91.188413	49.738650
703.030222	90.862247	49.743655
699.495922	95.879732	49.748660
696.077530	91.286414	49.753665
692.258532	96.032105	49.758669
688.918883	90.277998	49.763674
685.220277	95.501556	49.768679
681.935122	92.994471	49.773684
678.509970	92.641715	49.778689
674.633855	93.856063	49.783693
671.279146	89.151541	49.788698
667.895522	91.876993	49.793703
664.407668	98.545049	49.798708
661.291156	95.622413	49.803713
657.074889	93.223191	49.808717
653.980392	90.778009	49.813722
650.217844	96.660172	49.818727
646.779445	96.818875	49.823732
643.852064	89.519562	49.828737
640.061112	91.343856	49.833741
636.592731	80.250456	49.838746
632.361115	85.962470	49.843751
629.115954	88.397327	49.848756
625.922015	89.716833	49.853761
622.014586	105.764848	49.858765
619.183607	89.493722	49.863770
615.190078	91.261164	49.868775
611.725828	91.692852	49.873780
608.265473	92.190370	49.878785
604.656034	97.874563	49.883789
601.598329	87.526791	49.888794
597.700944	92.183552	49.893799
594.161857	89.912426	49.898804
590.950669	84.318579	49.903809
587.284315	91.660029	49.908813
583.745750	82.488579	49.913818
580.000698	83.559051	49.918823
576.641497	85.901053	49.923828
573.282548	86.996480	49.928833
570.256012	89.406608	49.933837
566.927065	82.277789	49.938842
563.036918	90.372478	49.943847
559.288017	85.963862	49.948852
555.992743	81.680357	49.953857
552.138675	90.876729	49.958861
548.597448	91.731790	49.963866
544.817391	90.036271	49.968871
541.556616	87.054016	49.973876
538.196043	86.580466	49.978881
534.684785	85.782500	49.983885
531.713447	84.026765	49.988890
527.846285	89.428639	49.993895
524.093551	99.184964	49.998900
520.743696	86.462678	50.003905
516.637196	87.482216	50.008909
513.664012	91.465905	50.013914
510.279821	88.493500	50.018919
506.719809	91.699058	50.023924
503.491732	88.376334	50.028929
499.662279	92.924415	50.033933
496.129486	91.474931	50.038938
492.665160	88.303110	50.043943
488.980334	90.079204	50.048948
485.508042	88.490532	50.053953
481.992377	92.163722	50.058957
478.908949	85.543823	50.063962
475.543377	93.989822	50.068967
471.918376	83.484186	50.073972
468.274140	88.822692	50.078977
464.772364	93.895275	50.083981
461.317330	84.201427	50.088986
457.585436	94.327836	50.093991
454.139853	93.899271	50.098996
450.376922	91.865747	50.104001
446.713305	94.252312	50.109005
443.711673	91.337074	50.114010
440.312238	88.202568	50.119015
436.756267	79.426226	50.124020
432.928027	79.646071	50.129025
429.934252	94.288671	50.134029
426.486034	96.024566	50.139034
422.324973	94.398267	50.144039
418.933532	86.754109	50.149044
415.942538	90.680504	50.154049
412.235289	87.163948	50.159053
408.841055	83.952710	50.164058
405.026627	92.848691	50.169063
401.383680	81.997884	50.174068
398.136505	82.993608	50.179073
394.625564	87.010942	50.184077
391.381779	82.311309	50.189082
387.506248	91.099807	50.194087
384.073940	87.840757	50.199092
380.614446	87.775072	50.204097
376.922056	95.161802	50.209101
373.648728	92.399880	50.214106
370.538546	95.272432	50.219111
366.711954	88.781640	50.224116
363.206496	85.325247	50.229121
358.883372	101.261276	50.234125
355.833306	89.748135	50.239130
352.556172	89.726663	50.244135
349.622846	98.810521	50.249140
345.950843	87.840902	50.254145
341.999822	89.965639	50.259149
338.602609	88.077361	50.264154
334.893739	98.253990	50.269159
331.564089	88.521578	50.274164
328.197783	85.695144	50.279169
323.915607	99.606271	50.284173
321.173009	88.152552	50.289178
317.698221	97.305416	50.294183
314.106036	94.621938	50.299188
310.786676	87.336700	50.304193
306.708147	92.297201	50.309197
303.860240	84.900151	50.314202
300.063351	93.287216	50.319207
296.512307	90.932663	50.324212
293.489254	86.350354	50.329217
289.251383	90.196857	50.334221
286.039597	91.731250	50.339226
282.438844	92.766583	50.344231
279.052351	83.318353	50.349236
275.542152	79.628622	50.354241
271.563550	91.938786	50.359245
268.582540	84.704971	50.364250
264.720886	86.281061	50.369255
261.585572	85.838769	50.374260
258.254362	80.883964	50.379265
254.332834	81.640524	50.384269
251.264277	76.932483	50.389274
247.605204	84.361492	50.394279
243.643825	79.881901	50.399284
240.550802	76.829195	50.404289
237.208960	87.426086	50.409293
233.761242	74.178271	50.414298
230.076881	91.235493	50.419303
226.158898	87.112947	50.424308
222.883540	69.038673	50.429313
219.399154	74.735042	50.434317
216.151427	83.766938	50.439322
212.568682	76.472389	50.444327
208.937316	81.628635	50.449332
205.539974	75.431354	50.454337
201.663353	82.432546	50.459341
198.487341	85.653991	50.464346
194.820438	88.433479	50.469351
191.209253	82.412072	50.474356
187.879611	78.029697	50.479361
183.904960	80.025324	50.484365
180.866558	77.277298	50.489370
177.778774	78.188019	50.494375
174.158226	77.593983	50.499380
170.641795	79.021116	50.504385
166.805625	92.707397	50.509389
163.415597	80.867952	50.514394
159.729867	82.109638	50.519399
156.061646	85.348096	50.524404
153.086811	80.473548	50.529409
149.453729	90.435879	50.534413
145.969845	82.122950	50.539418
142.393958	87.295841	50.544423
138.677675	79.702704	50.549428
135.400515	78.491734	50.554433
131.641335	90.081028	50.559437
128.849612	84.149570	50.564442
124.961158	81.019041	50.569447
121.444085	86.594017	50.574452
117.942199	79.071706	50.579457
114.200621	85.286140	50.584461
110.964862	86.985703	50.589466
107.363759	87.730094	50.594471
103.765108	79.634486	50.599476
100.605565	75.209680	50.604481
96.508287	82.577680	50.609485
93.171981	83.859563	50.614490
89.839942	95.581273	50.619495
86.197753	88.204343	50.624500
83.151221	79.291409	50.629505
79.061949	86.174104	50.634509
75.841560	80.816032	50.639514
72.294005	81.213523	50.644519
68.592340	79.018710	50.649524
65.593607	75.568480	50.654529
61.919851	80.386569	50.659533
58.482744	78.969732	50.664538
54.696815	83.840201	50.669543
51.343263	80.350653	50.674548
47.621384	83.822189	50.679553
43.910152	85.428590	50.684557
40.815003	79.955998	50.689562
37.185937	73.687529	50.694567
33.987556	77.994547	50.699572
30.585064	76.695685	50.704577
26.744464	82.954140	50.709581
23.247406	77.579327	50.714586
20.042987	79.644175	50.719591
16.376030	70.461483	50.724596
13.029256	70.821212	50.729601
9.002548	76.596298	50.734605
5.825527	70.399390	50.739610
1.770300	63.893990	50.744615