Thu Aug 25 13:10:02 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
0.000644	106.185222	0.000000
0.432593	111.742668	0.005005
0.258459	117.189430	0.010010
0.157300	118.502344	0.015014
0.341182	111.848472	0.020019
0.416844	107.840666	0.025024
0.246025	99.160602	0.030029
0.128988	96.669969	0.035034
0.093292	93.660387	0.040038
-0.195834	70.958006	0.045043
-0.433658	67.328359	0.050048
-0.783736	64.776166	0.055053
-1.058802	48.873736	0.060058
-1.628822	36.348988	0.065062
-1.349259	27.699634	0.070067
-2.100332	21.252397	0.075072
-2.418940	18.961037	0.080077
-2.450693	12.350480	0.085082
-2.881859	14.746481	0.090086
-3.223343	8.940595	0.095091
-3.022517	6.950667	0.100096
-3.817725	-9.752905	0.105101
-4.065429	-10.963871	0.110106
-4.576608	-2.341700	0.115110
-4.234031	-4.856874	0.120115
-5.242215	2.748507	0.125120
-5.481575	2.846033	0.130125
-5.811984	-6.248738	0.135130
-6.020739	-2.239264	0.140134
-5.644173	-7.189537	0.145139
-6.144239	-10.287696	0.150144
-7.034398	-5.004031	0.155149
-7.253447	-2.467260	0.160154
-7.512229	-0.364027	0.165158
-7.375875	-13.515109	0.170163
-7.790046	-1.602002	0.175168
-7.672438	0.034132	0.180173
-7.455668	-8.361756	0.185178
-7.984705	1.506575	0.190182
-8.261163	-6.021092	0.195187
-8.653227	-6.399515	0.200192
-8.678027	1.361837	0.205197
-9.362686	5.021932	0.210202
-10.218271	5.019856	0.215206
-10.148554	-1.885006	0.220211
-10.289055	-1.777660	0.225216
-10.450217	-1.262114	0.230221
-10.246284	-1.768720	0.235226
-10.422473	0.524053	0.240230
-10.145722	-3.597493	0.245235
-11.228521	-6.715081	0.250240
-11.620652	0.550166	0.255245
-11.703938	1.259155	0.260250
-12.057930	6.575876	0.265254
-12.719179	-1.429344	0.270259
-12.778498	4.682769	0.275264
-13.130592	-6.857359	0.280269
-13.120413	1.635670	0.285274
-13.426475	1.278573	0.290278
-13.277578	-5.262205	0.295283
-13.522881	-0.541485	0.300288
-13.594379	-0.058971	0.305293
-14.457355	-6.662669	0.310298
-14.576664	-5.663298	0.315302
-14.393299	-12.810589	0.320307
-14.727359	2.775755	0.325312
-15.431551	-2.008348	0.330317
-15.428722	-7.947269	0.335322
-15.869046	0.186073	0.340326
-15.525523	-6.404181	0.345331
-16.342584	6.350342	0.350336
-16.831998	0.640405	0.355341
-16.894033	-0.450956	0.360346
-17.339294	-5.142749	0.365350
-17.514597	8.245218	0.370355
-17.338507	0.646642	0.375360
-17.781445	0.307828	0.380365
-18.612355	-4.845562	0.385370
-18.791766	-5.943841	0.390374
-18.722533	-10.817486	0.395379
-19.258248	-3.381046	0.400384
-19.003971	-1.136737	0.405389
-19.005718	-7.135053	0.410394
-19.205828	-2.608077	0.415398
-18.917644	-7.130048	0.420403
-20.004257	-8.089348	0.425408
-20.389824	-1.065577	0.430413
-19.948510	-3.621533	0.435418
-21.134764	-1.917148	0.440422
-21.547555	-8.341444	0.445427
-21.683151	-0.891765	0.450432
-21.881714	7.399854	0.455437
-21.841122	-2.952114	0.460442
-21.827044	-1.185864	0.465446
-21.835874	-7.369732	0.470451
-22.278226	-0.935015	0.475456
-23.060048	-3.767564	0.480461
-23.247527	-6.500245	0.485466
-23.502807	-4.505129	0.490470
-23.222299	-11.680296	0.495475
-23.483167	-6.219982	0.500480
-24.319346	-11.280795	0.505485
-24.617773	-7.165524	0.510490
-25.249150	-3.931395	0.515494
-24.775991	-6.584089	0.520499
-25.082432	-3.574879	0.525504
-25.123096	-6.491917	0.530509
-24.903018	-6.548635	0.535514
-25.505949	3.410369	0.540518
-26.084662	-6.787614	0.545523
-26.477239	-4.998777	0.550528
-26.583455	-0.397926	0.555533
-26.986367	-8.778977	0.560538
-28.116995	-9.861093	0.565542
-27.558422	-0.223286	0.570547
-27.163345	0.129176	0.575552
-27.790832	-3.328670	0.580557
-27.871073	-12.336081	0.585562
-27.958856	-6.475778	0.590566
-28.207495	-13.678767	0.595571
-29.029109	-0.278127	0.600576
-29.522618	2.693955	0.605581
-29.301350	-5.322986	0.610586
-29.363871	-1.576871	0.615590
-29.593964	-9.244678	0.620595
-30.195976	-3.449336	0.625600
-30.672954	0.523069	0.630605
-30.582521	-3.278217	0.635610
-30.874438	5.186215	0.640614
-30.413963	-6.610941	0.645619
-30.994315	-0.866449	0.650624
-31.930757	1.257542	0.655629
-31.698208	1.088138	0.660634
-31.916008	-1.601829	0.665638
-32.199932	-6.549854	0.670643
-32.892728	-2.942268	0.675648
-33.516593	-9.535971	0.680653
-33.483963	-3.112402	0.685658
-33.522275	1.480973	0.690662
-33.521393	-0.993320	0.695667
-33.504803	-3.397307	0.700672
-33.900794	-3.531504	0.705677
-34.135808	-6.699664	0.710682
-35.075933	0.464782	0.715686
-34.794284	-11.383446	0.720691
-35.332080	-2.908966	0.725696
-35.023513	-4.982213	0.730701
-35.022370	-8.405675	0.735706
-35.858702	1.719612	0.740710
-36.494961	-2.129165	0.745715
-36.906795	-5.475266	0.750720
-37.053286	-9.198300	0.755725
-36.571394	-4.743382	0.760730
-36.924501	4.034359	0.765734
-36.796068	-1.237707	0.770739
-37.558300	-4.364389	0.775744
-37.803907	-0.045420	0.780749
-37.852939	3.499264	0.785754
-38.355565	5.261053	0.790758
-38.597161	-1.436841	0.795763
-38.884394	-3.603397	0.800768
-39.312719	2.269136	0.805773
-39.118173	-0.086804	0.810778
-39.598315	-9.446010	0.815782
-39.274036	-4.833519	0.820787
-40.281106	-1.445611	0.825792
-40.645402	-1.116537	0.830797
-40.507828	-4.542393	0.835802
-40.853968	2.095549	0.840806
-40.857280	0.086988	0.845811
-41.694252	-0.452679	0.850816
-42.245921	-0.603612	0.855821
-41.724452	-7.221747	0.860826
-42.237887	-1.598472	0.865830
-42.221159	-6.422761	0.870835
-42.319881	12.119636	0.875840
-42.862054	8.186512	0.880845
-43.323578	-1.552103	0.885850
-43.590542	5.231623	0.890854
-43.912360	8.426743	0.895859
-43.895260	4.358533	0.900864
-43.666632	-1.704353	0.905869
-43.938146	-1.668228	0.910874
-45.009299	3.359062	0.915878
-45.288447	4.532176	0.920883
-45.316451	-4.205011	0.925888
-45.639223	-1.879779	0.930893
-45.631470	-2.032944	0.935898
-45.452288	6.623431	0.940902
-45.695355	-3.541720	0.945907
-46.424005	0.982650	0.950912
-46.910468	6.016405	0.955917
-46.670778	0.951535	0.960922
-47.005684	-7.145939	0.965926
-47.205585	-6.833132	0.970931
-48.293692	6.011316	0.975936
-48.321893	0.023472	0.980941
-48.303119	-3.538795	0.985946
-48.170291	6.798474	0.990950
-48.533648	-0.930711	0.995955
-48.250352	3.805262	1.000960
-49.159906	9.288126	1.005965
-49.412330	-6.567173	1.010970
-49.870369	5.881158	1.015974
-50.097377	1.519002	1.020979
-50.056308	6.264456	1.025984
-50.242453	5.198870	1.030989
-50.271839	-3.772220	1.035994
-50.915011	0.305321	1.040998
-50.883271	-2.205444	1.046003
-51.054577	3.674275	1.051008
-51.707131	3.605589	1.056013
-52.072342	-2.544586	1.061018
-52.491358	-5.380193	1.066022
-52.674823	-1.520216	1.071027
-52.927151	5.571266	1.076032
-52.954053	8.552497	1.081037
-52.637845	-10.571481	1.086042
-53.137638	-9.474528	1.091046
-53.621423	-2.267688	1.096051
-53.821576	5.843843	1.101056
-54.802176	5.700006	1.106061
-54.314330	0.725968	1.111066
-54.530971	6.479913	1.116070
-54.972852	5.482872	1.121075
-55.382865	9.495407	1.126080
-56.003047	1.891884	1.131085
-55.790120	-6.848250	1.136090
-56.148496	10.823663	1.141094
-56.210734	2.670808	1.146099
-55.870594	4.844715	1.151104
-55.904577	7.852365	1.156109
-56.853243	-1.740317	1.161114
-57.433438	6.633242	1.166118
-57.092963	6.206481	1.171123
-57.405679	10.516985	1.176128
-58.308181	3.909991	1.181133
-58.287563	3.511200	1.186138
-58.684544	12.526774	1.191142
-58.963254	2.155234	1.196147
-59.131591	1.896782	1.201152
-59.123290	1.933358	1.206157
-58.995498	-3.158271	1.211162
-59.610358	-0.822074	1.216166
-59.897843	-3.706765	1.221171
-60.253402	5.349772	1.226176
-60.501602	6.132057	1.231181
-60.522584	-1.438800	1.236186
-60.763779	12.532131	1.241190
-61.343417	8.892782	1.246195
-61.442402	5.921607	1.251200
-61.765273	8.927066	1.256205
-61.713100	3.451813	1.261210
-62.284649	14.266449	1.266214
-62.129454	-1.519843	1.271219
-62.667863	7.903867	1.276224
-62.984655	7.535798	1.281229
-63.201669	2.488704	1.286234
-63.560318	1.889911	1.291238
-63.302103	-0.219740	1.296243
-63.944882	4.015928	1.301248
-64.466408	3.882420	1.306253
-64.391765	-6.060425	1.311258
-64.938539	10.040142	1.316262
-64.675663	-2.251239	1.321267
-65.026137	3.504692	1.326272
-65.697227	13.835050	1.331277
-66.017038	-3.183449	1.336282
-66.512892	11.093139	1.341286
-66.190002	5.543830	1.346291
-66.484415	-1.452671	1.351296
-66.871980	-0.313189	1.356301
-66.315060	-1.517350	1.361306
-66.810476	7.171957	1.366310
-67.385177	-6.089174	1.371315
-67.563369	-2.040197	1.376320
-67.506429	1.364495	1.381325
-68.075565	5.886019	1.386330
-68.783568	4.620627	1.391334
-69.204739	3.813331	1.396339
-69.166408	-2.248212	1.401344
-69.400446	-4.283896	1.406349
-69.233727	3.982121	1.411354
-69.442241	1.009126	1.416358
-69.586547	-0.180074	1.421363
-70.339529	-0.346918	1.426368
-70.827897	7.759152	1.431373
-70.619596	7.808683	1.436378
-70.996353	12.404469	1.441382
-70.884069	-1.087695	1.446387
-71.008271	4.626456	1.451392
-72.113120	7.539305	1.456397
-72.073549	3.492886	1.461402
-72.405538	11.065089	1.466406
-72.433233	-2.778464	1.471411
-72.496602	4.830740	1.476416
-72.738198	1.217521	1.481421
-73.435088	1.529108	1.486426
-73.984820	4.323339	1.491430
-73.968264	2.409741	1.496435
-74.406769	4.170975	1.501440
-73.890566	15.191661	1.506445
-73.966065	5.303975	1.511450
-74.106411	7.122896	1.516454
-74.758079	3.083546	1.521459
-75.140368	-1.586472	1.526464
-75.287874	5.988460	1.531469
-75.748071	3.817368	1.536474
-76.617179	11.752144	1.541478
-76.666257	3.844000	1.546483
-76.466368	0.791195	1.551488
-77.167473	10.202434	1.556493
-76.765515	2.157180	1.561498
-77.519513	6.005314	1.566502
-76.856816	2.823043	1.571507
-77.230384	3.634464	1.576512
-78.148967	4.322475	1.581517
-78.129719	5.160932	1.586522
-78.506238	6.523310	1.591526
-78.465565	-1.870294	1.596531
-78.445333	2.353237	1.601536
-79.548246	12.184941	1.606541
-79.430857	6.247051	1.611546
-80.088798	6.438640	1.616550
-79.798817	7.348571	1.621555
-80.052191	-2.669428	1.626560
-80.773860	13.420580	1.631565
-80.978414	-1.088127	1.636570
-81.242770	3.366658	1.641574
-81.195396	1.055925	1.646579
-81.259311	14.473893	1.651584
-81.227871	14.693505	1.656589
-81.417611	8.031779	1.661594
-82.519878	11.466247	1.666598
-82.554390	11.259593	1.671603
-82.569319	5.934060	1.676608
-82.693072	12.907321	1.681613
-83.314506	9.698468	1.686618
-83.714357	2.715324	1.691622
-84.006547	2.248488	1.696627
-84.363976	7.638514	1.701632
-84.378625	9.247914	1.706637
-84.653961	10.404613	1.711642
-84.617814	11.275223	1.716646
-84.596610	7.984658	1.721651
-85.332650	2.531671	1.726656
-85.638653	3.784924	1.731661
-85.389897	2.546790	1.736666
-85.797382	-2.647627	1.741670
-85.958684	10.051603	1.746675
-86.714793	10.271229	1.751680
-86.963009	7.943536	1.756685
-86.554034	2.738245	1.761690
-86.792818	0.174956	1.766694
-87.752420	3.125159	1.771699
-87.836056	-3.110261	1.776704
-88.599113	2.457217	1.781709
-88.427593	3.657793	1.786714
-88.757856	5.050890	1.791718
-88.628428	6.071400	1.796723
-88.716019	1.965812	1.801728
-88.811951	10.260330	1.806733
-89.412667	3.128326	1.811738
-89.828287	0.943924	1.816742
-90.106522	2.990095	1.821747
-89.972590	3.351835	1.826752
-90.276725	4.095430	1.831757
-90.815951	8.672380	1.836762
-91.607309	10.697713	1.841766
-91.539784	-0.231112	1.846771
-91.429758	11.754886	1.851776
-91.521521	8.073896	1.856781
-91.682197	8.181241	1.861786
-91.990132	3.898207	1.866790
-92.769599	5.918513	1.871795
-93.001105	1.446333	1.876800
-93.482467	7.431583	1.881805
-93.076218	0.157617	1.886810
-93.331510	3.434061	1.891814
-93.562293	1.584530	1.896819
-94.278538	13.779093	1.901824
-94.832710	3.520322	1.906829
-94.804020	-1.897464	1.911834
-94.662620	4.717869	1.916838
-95.085595	0.566758	1.921843
-95.311442	1.269611	1.926848
-94.994498	11.369220	1.931853
-95.441146	-4.316434	1.936858
-95.866059	8.044448	1.941862
-96.197973	5.055987	1.946867
-96.143997	9.660212	1.951872
-96.990433	6.480289	1.956877
-97.330618	-0.088257	1.961882
-97.451443	6.827594	1.966886
-97.638619	3.420985	1.971891
-97.429594	-2.961533	1.976896
-97.628240	11.432999	1.981901
-97.740074	-2.843458	1.986906
-98.837974	5.962399	1.991910
-99.228786	-2.331957	1.996915
-98.941836	3.093108	2.006912
-98.908454	-0.555288	2.016909
-97.803016	1.317729	2.026906
-98.026650	-1.536455	2.036902
-97.844850	2.619565	2.046899
-97.082602	2.705857	2.056896
-95.878252	-4.132277	2.066893
-95.434649	4.674256	2.076890
-95.146265	1.480081	2.086886
-95.180735	14.121726	2.096883
-94.588113	5.098613	2.106880
-93.937289	2.306980	2.116877
-93.174981	5.519898	2.126874
-92.483635	-3.268423	2.136870
-92.400958	5.119492	2.146867
-91.916803	8.733958	2.156864
-91.187531	-1.932487	2.166861
-90.867948	2.379342	2.176858
-90.458643	0.908519	2.186854
-89.669728	1.963153	2.196851
-89.274745	1.698344	2.206848
-88.250516	0.802746	2.216845
-87.788569	-0.242334	2.226842
-87.906388	-0.784755	2.236838
-87.618334	3.994516	2.246835
-87.051455	-0.234822	2.256832
-86.685295	-0.729533	2.266829
-85.871775	1.100529	2.276826
-85.166002	1.674012	2.286822
-84.388051	3.902456	2.296819
-84.294217	3.276186	2.306816
-83.931678	1.030241	2.316813
-83.256085	7.947254	2.326810
-83.045294	4.106331	2.336806
-82.169869	-2.065707	2.346803
-81.404364	-0.218618	2.356800
-81.328522	-2.163047	2.366797
-81.069148	-1.538625	2.376794
-79.913623	0.282198	2.386790
-80.063925	-3.270894	2.396787
-79.582362	4.946815	2.406784
-78.541336	-2.207851	2.416781
-78.234139	-9.314056	2.426778
-77.414340	-3.461853	2.436774
-77.363505	-0.628465	2.446771
-77.090116	-3.151880	2.456768
-76.075580	0.889499	2.466765
-75.698843	1.153407	2.476762
-75.565180	3.641197	2.486758
-74.790815	2.186033	2.496755
-74.182428	8.929845	2.506752
-73.273791	-2.262051	2.516749
-73.102868	-0.318629	2.526746
-73.120430	4.660584	2.536742
-72.193182	3.213144	2.546739
-71.446420	-0.474172	2.556736
-71.289884	-1.056413	2.566733
-70.761461	-1.177403	2.576730
-69.999333	1.725099	2.586726
-69.988169	0.709471	2.596723
-69.375544	-4.635770	2.606720
-68.564186	-4.123179	2.616717
-68.311341	1.874882	2.626714
-67.421799	0.411176	2.636710
-67.062242	-2.239781	2.646707
-66.815228	1.700114	2.656704
-66.389286	-4.208257	2.666701
-65.664689	-0.827870	2.676698
-65.427905	-0.437494	2.686694
-64.533077	0.632225	2.696691
-64.179868	-5.394630	2.706688
-63.861037	1.372376	2.716685
-62.887138	-2.584948	2.726682
-62.623101	-0.944386	2.736678
-62.579415	5.472923	2.746675
-61.501226	3.086334	2.756672
-61.388731	-0.314699	2.766669
-60.348268	-1.428249	2.776666
-59.910908	3.733110	2.786662
-59.829058	2.871132	2.796659
-59.590678	6.086951	2.806656
-58.561036	2.833652	2.816653
-58.353402	1.286724	2.826650
-57.655622	0.679865	2.836646
-56.940769	5.604509	2.846643
-57.019653	1.777296	2.856640
-55.975913	-4.341917	2.866637
-55.498202	-4.166689	2.876634
-55.454415	0.980310	2.886630
-54.797809	3.189757	2.896627
-54.332574	9.452318	2.906624
-53.840540	4.794380	2.916621
-53.023656	8.109626	2.926618
-52.796354	3.692740	2.936614
-51.701831	2.415497	2.946611
-51.285799	-0.976075	2.956608
-51.220767	-0.146971	2.966605
-51.252490	5.702444	2.976602
-49.888741	8.735599	2.986598
-49.846358	10.258837	2.996595
-49.241323	1.566400	3.006592
-48.128077	-5.808655	3.016589
-47.841748	-2.175862	3.026586
-47.806685	-1.234356	3.036582
-47.279448	3.719684	3.046579
-46.629179	2.575407	3.056576
-46.597117	2.655736	3.066573
-45.420277	-1.064120	3.076570
-45.040641	3.171779	3.086566
-44.811844	3.503218	3.096563
-44.246386	6.446043	3.106560
-43.525280	1.752214	3.116557
-43.409726	-0.455032	3.126554
-42.536165	0.250556	3.136550
-42.355860	-2.359644	3.146547
-41.408520	2.414531	3.156544
-41.089552	-1.094881	3.166541
-40.990794	0.270636	3.176538
-40.149342	4.098387	3.186534
-39.780664	7.756293	3.196531
-39.216194	2.839916	3.206528
-38.316114	2.014461	3.216525
-38.378872	2.163500	3.226522
-37.525426	-4.676668	3.236518
-36.746303	-2.901401	3.246515
-36.604332	-1.960807	3.256512
-36.470508	2.190062	3.266509
-35.530155	-0.447359	3.276506
-35.265458	-1.981053	3.286502
-34.472948	1.990583	3.296499
-33.805763	-3.518429	3.306496
-33.833935	0.369551	3.316493
-33.215631	-1.089667	3.326490
-32.262412	2.739580	3.336486
-32.088926	0.276167	3.346483
-32.119454	2.872048	3.356480
-31.063129	1.879560	3.366477
-30.731100	-6.915817	3.376474
-29.749790	-0.908346	3.386470
-29.532825	4.464946	3.396467
-29.174424	-1.093888	3.406464
-29.002188	-4.054451	3.416461
-28.177072	9.390189	3.426458
-27.516105	0.277173	3.436454
-26.369716	0.645407	3.446451
-26.679565	5.987202	3.456448
-26.454150	2.188337	3.466445
-25.694439	1.701658	3.476442
-24.977476	-2.931332	3.486438
-24.861647	1.624670	3.496435
-23.868705	7.592308	3.506432
-23.586418	-0.564882	3.516429
-23.303952	0.787690	3.526426
-22.011245	-3.609224	3.536422
-22.300075	-1.286486	3.546419
-22.065089	-0.838807	3.556416
-20.849519	-2.363095	3.566413
-20.506339	3.893250	3.576410
-20.196595	-1.258814	3.586406
-19.661232	3.038218	3.596403
-19.398820	-6.104215	3.606400
-18.567769	1.989050	3.616397
-17.950028	5.614269	3.626394
-17.877864	0.781365	3.636390
-16.793799	7.308101	3.646387
-16.679603	8.062979	3.656384
-16.226180	-3.041754	3.666381
-15.257779	9.845078	3.676378
-14.971049	2.479145	3.686374
-14.950962	-0.932753	3.696371
-13.834427	-0.974823	3.706368
-13.443734	-0.494519	3.716365
-13.107950	0.849700	3.726362
-12.408776	5.722952	3.736358
-12.123496	-3.666987	3.746355
-11.879086	-2.739276	3.756352
-10.843700	5.125572	3.766349
-10.248752	-5.884124	3.776346
-10.502886	3.582942	3.786342
-9.527941	-0.422059	3.796339
-9.031920	4.118725	3.806336
-8.680853	3.439481	3.816333
-7.613829	-3.678073	3.826330
-7.479533	-0.214693	3.836326
-7.311887	6.043814	3.846323
-6.475047	9.099346	3.856320
-6.330430	5.005861	3.866317
-5.570242	-3.352919	3.876314
-5.083458	2.738375	3.886310
-4.758226	12.130509	3.896307
-4.157739	19.037130	3.906304
-3.823954	18.620355	3.916301
-3.301463	27.949913	3.926298
-2.891001	35.266453	3.936294
-2.445057	56.987882	3.946291
-2.128125	64.328592	3.956288
-1.469509	75.968369	3.966285
-0.889749	92.606681	3.976282
-0.510328	104.100152	3.986278
0.000000	122.325487	3.991283
0.000800	117.231573	3.996288
0.114784	134.908700	4.001293
-0.032574	139.288240	4.006298
0.477900	133.896164	4.011302
0.389076	150.168722	4.016307
0.240377	140.735353	4.021312
0.106960	157.935568	4.026317
0.496718	163.474330	4.031322
0.734778	160.288965	4.036326
0.198749	160.958163	4.041331
0.414622	158.016723	4.046336
0.474268	165.477010	4.051341
0.536735	157.655722	4.056346
0.925390	164.115321	4.061350
0.786128	173.511383	4.066355
0.872689	176.411590	4.071360
1.022337	188.957830	4.076365
0.464494	174.985218	4.081370
0.712911	177.005840	4.086374
0.889230	190.193317	4.091379
1.526695	182.535031	4.096384
0.838585	183.595059	4.101389
1.048192	184.618838	4.106394
0.720656	177.462932	4.111398
0.975276	184.218790	4.116403
0.841588	185.464038	4.121408
0.964299	196.612940	4.126413
1.063071	194.800336	4.131418
1.074811	189.464238	4.136422
0.978884	191.235088	4.141427
1.113006	191.773978	4.146432
0.869205	192.596710	4.151437
1.125253	187.497586	4.156442
1.311122	184.798127	4.161446
1.085231	193.502245	4.166451
1.020246	187.159425	4.171456
1.152334	193.909175	4.176461
0.750309	191.773233	4.181466
1.247385	189.189531	4.186470
1.367895	194.887550	4.191475
1.328486	184.949809	4.196480
1.609427	200.332398	4.201485
0.929401	193.149455	4.206490
1.101318	181.292980	4.211494
1.059692	196.355941	4.216499
1.367659	191.960536	4.221504
1.386367	196.250794	4.226509
1.408081	193.244855	4.231514
1.277845	184.371727	4.236518
1.464820	181.817631	4.241523
0.872388	172.539192	4.246528
1.199522	186.364270	4.251533
1.141338	190.625446	4.256538
1.337782	184.985159	4.261542
1.128696	190.927809	4.266547
1.507903	192.937432	4.271552
1.360338	196.870922	4.276557
1.442583	196.408687	4.281562
1.722544	187.616823	4.286566
1.726146	187.843963	4.291571
1.568593	190.545135	4.296576
1.372797	177.831937	4.301581
1.270374	193.882035	4.306586
1.406932	189.763427	4.311590
1.616673	196.516830	4.316595
1.284862	193.626394	4.321600
1.599318	197.031907	4.326605
1.297566	188.650730	4.331610
1.385891	187.595911	4.336614
1.429118	189.762580	4.341619
1.889152	181.790404	4.346624
1.672407	193.837225	4.351629
1.501672	193.126721	4.356634
1.996735	192.001847	4.361638
1.586449	186.890063	4.366643
1.635362	186.040740	4.371648
1.657212	181.047915	4.376653
1.387050	181.678621	4.381658
1.636283	189.140853	4.386662
1.568872	194.077364	4.391667
1.789244	188.781345	4.396672
1.493976	191.636974	4.401677
1.436721	184.831029	4.406682
1.712297	190.590173	4.411686
1.601252	196.248541	4.416691
1.698550	186.460225	4.421696
1.539125	191.192850	4.426701
1.495563	188.491373	4.431706
1.565025	190.245801	4.436710
1.266843	199.787001	4.441715
1.776304	195.999113	4.446720
1.782176	191.900980	4.451725
1.432847	183.128620	4.456730
1.475154	202.987412	4.461734
1.526497	219.557616	4.466739
1.548684	205.323256	4.471744
1.626711	214.796027	4.476749
1.599607	222.023154	4.481754
2.276046	216.756913	4.486758
1.684892	222.269046	4.491763
2.080760	221.378014	4.496768
1.876384	223.681560	4.501773
2.079649	215.540788	4.506778
1.979721	215.246303	4.511782
1.830542	226.048675	4.516787
1.955990	217.587895	4.521792
2.054211	216.237291	4.526797
1.731833	228.110857	4.531802
1.642946	210.875624	4.536806
2.044167	221.772094	4.541811
2.007813	220.290712	4.546816
2.049423	217.338600	4.551821
1.857356	210.019084	4.556826
1.961373	214.213722	4.561830
1.846896	227.165210	4.566835
2.183497	232.984410	4.571840
2.140897	221.288071	4.576845
2.323209	230.418639	4.581850
2.206623	219.951960	4.586854
2.200288	229.555018	4.591859
2.166172	211.817648	4.596864
2.118845	215.358944	4.601869
1.900448	218.284792	4.606874
2.126639	234.985805	4.611878
2.271021	237.927583	4.616883
2.309213	234.311604	4.621888
2.239646	240.561447	4.626893
2.417906	232.731474	4.631898
2.425811	219.853450	4.636902
1.935714	225.906580	4.641907
2.139166	232.600870	4.646912
2.269833	240.265201	4.651917
2.262143	239.083052	4.656922
2.368742	246.896691	4.661926
2.385391	242.024889	4.666931
2.535408	236.053333	4.671936
2.343426	237.560822	4.676941
2.582389	244.999376	4.681946
2.631677	235.474824	4.686950
1.900364	226.958448	4.691955
2.528380	237.136011	4.696960
1.931549	246.717700	4.701965
2.018437	244.682322	4.706970
2.469781	238.881856	4.711974
2.204866	243.583566	4.716979
2.231926	239.096119	4.721984
2.427126	241.087120	4.726989
2.685907	243.381377	4.731994
2.965714	241.540404	4.736998
2.531203	243.101712	4.742003
2.726193	239.514949	4.747008
2.877033	248.179050	4.752013
2.824480	248.677586	4.757018
2.766425	244.969115	4.762022
2.612621	256.452450	4.767027
2.259110	248.114156	4.772032
2.169981	252.785162	4.777037
2.824765	249.702171	4.782042
2.963071	245.301697	4.787046
2.761649	251.550056	4.792051
2.823830	236.591219	4.797056
2.800447	239.587758	4.802061
2.727311	251.045795	4.807066
2.959230	250.509487	4.812070
2.340948	246.863481	4.817075
2.792227	249.121251	4.822080
2.844070	242.412087	4.827085
2.780272	254.688091	4.832090
2.574774	249.379684	4.837094
2.530298	242.935553	4.842099
2.905064	242.050991	4.847104
2.732859	237.851033	4.852109
2.598134	240.738464	4.857114
2.832853	252.167250	4.862118
2.760063	258.221448	4.867123
2.708966	247.453421	4.872128
2.851883	245.184633	4.877133
2.572518	253.077732	4.882138
3.167988	240.091814	4.887142
2.875680	253.090166	4.892147
2.888231	245.273496	4.897152
2.817740	249.941582	4.902157
2.579438	246.615698	4.907162
2.918023	249.327731	4.912166
2.545721	253.505257	4.917171
2.715467	250.064819	4.922176
3.055159	254.418697	4.927181
2.867361	266.195272	4.932186
3.415544	270.234908	4.937190
3.077908	262.919195	4.942195
3.156315	268.206210	4.947200
2.812454	258.132629	4.952205
2.922668	259.788929	4.957210
3.118099	270.103892	4.962214
3.032504	276.701115	4.967219
3.482538	272.884556	4.972224
3.465831	270.026995	4.977229
2.846281	259.702373	4.982234
2.895895	252.952425	4.987238
3.186411	266.969969	4.992243
3.420002	272.514251	4.997248
3.197279	271.663189	5.002253
3.213990	270.951787	5.007258
3.582394	272.725826	5.012262
3.153491	263.282510	5.017267
2.778543	257.541897	5.022272
2.912729	264.595071	5.027277
2.885681	274.922749	5.032282
3.325707	267.769934	5.037286
3.496899	273.434726	5.042291
3.744744	272.323271	5.047296
3.650498	279.943763	5.052301
3.136691	277.496287	5.057306
3.463125	272.591758	5.062310
3.456485	270.381203	5.067315
3.068742	269.878706	5.072320
3.493178	268.198571	5.077325
3.130377	276.294580	5.082330
3.497771	272.161933	5.087334
3.349270	283.964000	5.092339
3.687068	285.467584	5.097344
3.580709	272.110705	5.102349
3.395229	275.822359	5.107354
3.582129	278.776465	5.112358
3.364098	275.611919	5.117363
3.574711	266.058910	5.122368
3.367175	277.034976	5.127373
3.362312	282.410973	5.132378
3.177508	274.916283	5.137382
3.393207	281.542232	5.142387
3.284639	275.816826	5.147392
3.585277	279.230848	5.152397
3.386818	288.120543	5.157402
3.571405	274.493447	5.162406
3.014657	282.309793	5.167411
3.453935	272.796885	5.172416
3.379825	278.490622	5.177421
3.625462	277.939508	5.182426
3.392181	279.352230	5.187430
3.538044	289.829998	5.192435
3.808751	290.126023	5.197440
3.750995	300.816038	5.202445
3.431155	300.109909	5.207450
3.727204	295.779622	5.212454
3.753889	306.181158	5.217459
3.922400	300.070639	5.222464
4.025688	302.297515	5.227469
3.566703	303.103347	5.232474
3.721308	298.026412	5.237478
3.555181	302.662039	5.242483
3.759052	306.594275	5.247488
3.928985	308.567096	5.252493
4.144118	302.186674	5.257498
3.681789	301.537672	5.262502
3.413750	295.558829	5.267507
3.685460	304.131251	5.272512
3.617158	300.778722	5.277517
3.587012	303.162550	5.282522
3.811328	305.623570	5.287526
3.323109	311.341069	5.292531
3.599805	302.869206	5.297536
3.887003	309.816165	5.302541
4.011723	310.739354	5.307546
4.054095	306.477285	5.312550
3.818630	305.400423	5.317555
3.810095	301.839209	5.322560
4.151793	309.467341	5.327565
3.931433	312.671928	5.332570
3.936260	302.951822	5.337574
4.048248	322.483447	5.342579
3.960963	317.466554	5.347584
4.163909	318.750818	5.352589
4.059302	331.881173	5.357594
4.511935	323.941731	5.362598
3.699454	309.151514	5.367603
3.813452	317.166510	5.372608
4.343224	326.112971	5.377613
4.216459	328.717589	5.382618
4.299954	319.333169	5.387622
4.412031	328.190048	5.392627
4.487570	320.790592	5.397632
3.909072	305.903604	5.402637
3.770823	310.911359	5.407642
4.287736	308.729502	5.412646
4.200640	322.828401	5.417651
4.265914	330.389118	5.422656
4.364673	333.964499	5.427661
4.481541	330.026118	5.432666
4.399696	315.627631	5.437670
4.059882	318.233990	5.442675
4.171053	309.408399	5.447680
4.389681	327.958357	5.452685
4.622395	329.478408	5.457690
4.520607	315.332989	5.462694
4.206378	311.114136	5.467699
4.211530	304.171814	5.472704
4.249438	317.621523	5.477709
4.450105	320.465909	5.482714
4.759671	321.667028	5.487718
4.208725	314.441664	5.492723
4.326959	308.414951	5.497728
4.550042	319.769672	5.502733
4.289141	319.649106	5.507738
4.300549	318.403847	5.512742
4.308333	322.692683	5.517747
4.350826	332.541253	5.522752
4.516280	335.761326	5.527757
4.238466	334.333586	5.532762
4.649709	328.197681	5.537766
4.670358	332.035241	5.542771
4.591899	333.999526	5.547776
4.811103	325.906827	5.552781
4.733365	330.500138	5.557786
4.481095	321.687191	5.562790
4.430036	324.336895	5.567795
4.544216	327.489069	5.572800
4.482131	331.839477	5.577805
4.106730	337.925295	5.582810
4.467433	336.251976	5.587814
4.882560	333.703240	5.592819
4.442517	318.256699	5.597824
4.657543	326.230559	5.602829
4.579902	327.416414	5.607834
4.835003	328.078725	5.612838
4.375270	335.516054	5.617843
4.657126	329.153643	5.622848
4.554219	327.957932	5.627853
4.556675	330.048746	5.632858
4.652266	334.175129	5.637862
4.726861	350.944296	5.642867
5.198720	357.685166	5.647872
4.756851	342.245218	5.652877
4.418844	333.524794	5.657882
4.940087	338.539962	5.662886
4.822069	355.355131	5.667891
4.947219	354.348319	5.672896
5.508399	353.187766	5.677901
4.866685	346.473332	5.682906
5.014985	339.011847	5.687910
4.741584	336.684888	5.692915
4.656000	336.619112	5.697920
4.437868	335.580663	5.702925
4.902879	348.517376	5.707930
5.030091	339.531066	5.712934
4.897301	352.469695	5.717939
5.313817	350.787629	5.722944
5.272039	353.084699	5.727949
4.251596	358.964698	5.732954
4.898815	360.100260	5.737958
5.017203	358.050443	5.742963
5.398366	354.023190	5.747968
5.296104	355.393242	5.752973
4.542692	357.207011	5.757978
5.231962	344.510049	5.762982
4.827828	356.858430	5.767987
4.844079	352.995921	5.772992
4.813054	359.708014	5.777997
4.857239	357.391405	5.783002
4.844394	349.594488	5.788006
5.100979	346.004381	5.793011
4.905125	359.319900	5.798016
5.280182	367.075711	5.803021
4.949077	373.898102	5.808026
5.153278	377.602507	5.813030
5.010552	385.993123	5.818035
4.946195	377.106414	5.823040
5.307043	374.502901	5.828045
5.330090	382.114550	5.833050
5.332758	377.782753	5.838054
5.600671	380.885539	5.843059
5.451078	382.658489	5.848064
5.310184	379.671668	5.853069
5.307331	381.668406	5.858074
5.463743	376.622805	5.863078
5.386723	382.994091	5.868083
5.705931	374.553499	5.873088
5.443233	365.599792	5.878093
5.085911	361.229487	5.883098
5.239478	362.303187	5.888102
5.274176	373.390058	5.893107
5.360418	384.003777	5.898112
5.814008	377.582803	5.903117
5.575781	378.170546	5.908122
5.645925	377.707039	5.913126
5.392096	370.938149	5.918131
5.367756	373.491923	5.923136
5.462096	380.763363	5.928141
5.534457	379.508549	5.933146
5.505404	385.062379	5.938150
5.275869	383.048088	5.943155
5.133898	382.643125	5.948160
5.562586	376.754414	5.953165
5.261072	386.520867	5.958170
5.346515	376.452723	5.963174
5.297025	385.603871	5.968179
5.380666	385.138248	5.973184
5.345726	383.827478	5.978189
4.973743	390.785997	5.983194
5.553217	392.884491	5.988198
5.624803	400.675210	5.993203
5.680354	401.976246	5.998208
5.929174	407.062591	6.003213
5.878763	411.629494	6.008218
5.673157	405.672470	6.013222
5.664191	411.327567	6.018227
5.688163	411.731858	6.023232
5.837914	401.372042	6.028237
5.187036	402.056079	6.033242
5.661174	409.812204	6.038246
5.703585	411.042531	6.043251
5.801861	402.943435	6.048256
5.590840	403.748385	6.053261
5.582013	419.407524	6.058266
5.497025	407.009004	6.063270
5.292147	408.809602	6.068275
5.356394	415.639669	6.073280
5.862559	418.467845	6.078285
5.716013	420.572524	6.083290
5.756677	414.371262	6.088294
6.142091	420.053159	6.093299
5.983666	406.925806	6.098304
5.665963	401.081263	6.103309
5.442055	403.451168	6.108314
5.618844	408.637387	6.113318
5.446018	414.457368	6.118323
5.653854	412.178388	6.123328
5.874807	406.587977	6.128333
5.495674	400.851138	6.133338
5.279320	404.823926	6.138342
5.362606	408.923779	6.143347
5.672724	402.382903	6.148352
5.546400	411.387910	6.153357
5.533576	419.188698	6.158362
5.918079	404.625321	6.163366
5.418050	411.885492	6.168371
5.472840	407.425296	6.173376
5.427010	402.186742	6.178381
5.097091	411.992462	6.183386
5.350929	413.040962	6.188390
5.552099	411.883027	6.193395
5.495224	425.948797	6.198400
5.797207	443.391125	6.203405
5.622887	447.487054	6.208410
5.928874	442.781842	6.213414
5.816139	430.178839	6.218419
5.811888	416.119301	6.223424
6.043925	416.639692	6.228429
5.501026	420.948393	6.233434
5.345885	413.249675	6.238438
5.568763	416.020992	6.243443
5.818974	416.181022	6.248448
5.785816	413.664547	6.253453
5.670589	419.111663	6.258458
5.663447	410.836085	6.263462
5.827034	412.648556	6.268467
5.938113	419.863604	6.273472
5.829351	407.668131	6.278477
5.480607	416.347312	6.283482
5.343223	418.336657	6.288486
5.916985	414.079892	6.293491
5.514155	412.462919	6.298496
6.019400	412.418471	6.303501
5.809929	413.764195	6.308506
5.970874	407.578892	6.313510
5.925565	413.938893	6.318515
5.882288	408.949881	6.323520
5.985459	415.913059	6.328525
5.689660	410.606097	6.333530
6.138559	400.715118	6.338534
5.750004	391.970947	6.343539
5.507098	382.422494	6.348544
5.584254	385.928501	6.353549
5.639926	380.560152	6.358554
5.386235	385.513247	6.363558
5.184423	387.822740	6.368563
5.614778	405.377798	6.373568
5.808026	410.637371	6.378573
5.917275	415.726603	6.383578
5.873014	409.494356	6.388582
5.803509	415.402555	6.393587
5.556535	404.990998	6.398592
5.805045	396.558310	6.403597
5.819612	397.777179	6.408602
5.489782	383.196024	6.413606
5.710246	390.580588	6.418611
5.399979	394.928765	6.423616
5.832118	393.921309	6.428621
5.823030	406.460935	6.433626
5.652420	394.566234	6.438630
5.623636	393.583538	6.443635
5.409922	380.493342	6.448640
5.665270	408.728459	6.453645
5.876560	406.825436	6.458650
5.977600	395.982860	6.463654
5.121564	386.027419	6.468659
5.785063	393.386864	6.473664
5.858024	394.571273	6.478669
5.554657	396.687865	6.483674
5.663508	391.219430	6.488678
5.498374	388.938777	6.493683
5.851763	403.614147	6.498688
6.104379	403.251767	6.503693
5.705001	398.799454	6.508698
5.557596	387.840782	6.513702
5.516148	381.978272	6.518707
5.647496	387.858157	6.523712
5.366212	387.155474	6.528717
5.684306	388.870966	6.533722
5.569613	389.822179	6.538726
5.702839	399.014310	6.543731
5.619117	390.083171	6.548736
5.808471	398.845717	6.553741
5.878327	406.029252	6.558746
5.563311	390.309952	6.563750
5.553572	387.014671	6.568755
5.301170	391.530957	6.573760
5.901194	402.016729	6.578765
5.844718	408.001981	6.583770
5.790774	390.071382	6.588774
5.558507	389.664747	6.593779
5.601132	388.753122	6.598784
5.804811	381.292435	6.603789
5.668969	389.837002	6.608794
5.870819	388.606194	6.613798
5.865488	386.132820	6.618803
5.734147	382.891395	6.623808
5.842004	385.623780	6.628813
5.336584	389.312817	6.633818
5.483654	385.597488	6.638822
5.308994	379.448958	6.643827
5.520317	386.904557	6.648832
5.841793	394.709906	6.653837
5.591635	391.309920	6.658842
5.726750	381.727549	6.663846
5.399241	380.500585	6.668851
5.656323	394.555106	6.673856
5.631162	404.749682	6.678861
5.774998	406.647507	6.683866
6.312249	399.792626	6.688870
5.655118	390.913362	6.693875
5.460550	382.591231	6.698880
5.829001	386.421767	6.703885
5.938319	387.087938	6.708890
5.582207	384.796078	6.713894
5.132021	383.417488	6.718899
5.141402	382.583840	6.723904
5.486670	397.861606	6.728909
5.567571	405.660359	6.733914
5.711350	410.671411	6.738918
5.577714	403.665373	6.743923
6.018620	407.405465	6.748928
6.297399	404.631304	6.753933
5.837269	395.718007	6.758938
5.743248	386.816957	6.763942
5.601603	385.975334	6.768947
5.567627	382.522496	6.773952
5.711056	377.520058	6.778957
5.479195	377.372795	6.783962
5.920636	380.685680	6.788966
5.772130	378.354966	6.793971
5.426736	374.764256	6.798976
5.639654	373.889227	6.803981
5.516498	380.198136	6.808986
5.719015	376.989827	6.813990
5.776380	383.874746	6.818995
5.298324	381.250807	6.824000
5.634422	375.022254	6.829005
5.481149	380.083003	6.834010
5.770004	391.218652	6.839014
5.689432	388.839326	6.844019
5.327649	392.534333	6.849024
5.638982	403.059011	6.854029
6.100892	408.706771	6.859034
5.484508	397.600103	6.864038
5.541370	392.424559	6.869043
6.177669	394.631212	6.874048
6.068162	391.636307	6.879053
5.724459	391.946340	6.884058
5.634939	387.540398	6.889062
5.606271	387.184123	6.894067
5.213899	383.075575	6.899072
5.772216	381.643379	6.904077
5.471065	383.398945	6.909082
5.859856	378.468799	6.914086
5.984243	390.130101	6.919091
5.556869	384.685571	6.924096
5.989206	380.928711	6.929101
5.530276	381.611147	6.934106
5.581984	388.455824	6.939110
5.585769	389.173333	6.944115
5.754391	388.200837	6.949120
5.892544	377.684661	6.954125
5.638979	384.526545	6.959130
5.735589	380.189521	6.964134
5.367504	378.921456	6.969139
5.769712	387.432343	6.974144
5.503016	379.618236	6.979149
5.363880	392.181392	6.984154
5.599631	382.058056	6.989158
5.830866	372.185377	6.994163
5.501531	385.534484	6.999168
6.132645	382.043881	7.004173
5.227917	390.205868	7.009178
5.346369	387.599202	7.014182
5.680712	388.309212	7.019187
5.617685	394.542265	7.024192
5.775305	373.585545	7.029197
5.319582	390.991511	7.034202
5.807573	386.466610	7.039206
5.772858	402.487304	7.044211
5.340207	384.461018	7.049216
6.036342	393.175798	7.054221
5.715334	400.366786	7.059226
5.526238	384.099401	7.064230
5.508058	386.329500	7.069235
5.432236	401.872568	7.074240
5.744400	409.236444	7.079245
5.917556	410.335552	7.084250
5.523864	408.008447	7.089254
5.798701	400.906772	7.094259
5.496464	391.766253	7.099264
5.904011	399.026593	7.104269
5.498370	399.817742	7.109274
5.495294	398.403899	7.114278
5.768331	413.325991	7.119283
5.764112	419.556166	7.124288
5.652033	394.500209	7.129293
5.764335	402.265566	7.134298
5.302163	403.650883	7.139302
5.763108	400.088859	7.144307
5.871510	404.301838	7.149312
5.461456	397.851653	7.154317
5.719618	401.177439	7.159322
5.680871	396.554725	7.164326
5.712460	399.507875	7.169331
5.703109	399.718064	7.174336
5.573102	384.811362	7.179341
5.345537	400.280125	7.184346
5.736775	402.882689	7.189350
6.083552	398.218554	7.194355
5.845595	395.481062	7.199360
5.514203	389.379233	7.204365
5.531322	392.992727	7.209370
5.400572	380.857666	7.214374
5.776718	391.792972	7.219379
5.684822	402.849075	7.224384
5.973757	393.046439	7.229389
5.493770	398.139400	7.234394
5.714319	383.073368	7.239398
5.916930	389.745702	7.244403
5.597683	386.774169	7.249408
5.911794	386.601476	7.254413
5.242280	379.141556	7.259418
5.711695	376.419789	7.264422
5.638210	387.289496	7.269427
5.167786	382.683800	7.274432
5.793684	395.193533	7.279437
5.955624	412.512236	7.284442
5.946047	397.108915	7.289446
5.986343	390.572352	7.294451
5.346365	382.952775	7.299456
5.233255	377.740589	7.304461
5.532285	399.160276	7.309466
6.193250	392.523303	7.314470
5.947316	397.598576	7.319475
5.779634	384.346137	7.324480
5.440357	379.447804	7.329485
5.502379	384.515952	7.334490
5.691396	385.811895	7.339494
5.600442	382.776119	7.344499
5.409541	386.827175	7.349504
5.598880	380.409637	7.354509
5.679135	391.002151	7.359514
5.791810	391.810169	7.364518
5.680483	382.601777	7.369523
5.101359	386.954111	7.374528
5.810691	396.479931	7.379533
5.459924	413.916932	7.384538
5.787739	419.756553	7.389542
5.976891	412.000728	7.394547
5.841765	408.829496	7.399552
5.719842	392.108641	7.404557
5.749217	391.774910	7.409562
5.501789	386.985574	7.414566
5.634974	384.262702	7.419571
5.425650	387.244104	7.424576
6.066635	398.501761	7.429581
5.569524	393.925554	7.434586
5.704486	388.291672	7.439590
5.655722	392.348934	7.444595
5.290807	392.238337	7.449600
6.019128	380.069920	7.454605
5.751085	383.946396	7.459610
5.571630	382.886064	7.464614
5.380688	385.092611	7.469619
5.412138	389.178434	7.474624
6.016770	400.090601	7.479629
5.710303	401.979883	7.484634
5.521790	391.400983	7.489638
5.812057	381.288089	7.494643
5.605554	386.123057	7.499648
5.820183	390.610461	7.504653
5.756462	383.451104	7.509658
5.988071	386.113478	7.514662
5.704038	376.125371	7.519667
5.465987	388.571141	7.524672
5.422258	379.345831	7.529677
5.440481	385.249767	7.534682
5.705741	373.951193	7.539686
6.176443	379.369771	7.544691
5.594285	381.216822	7.549696
6.031403	379.680226	7.554701
5.653657	382.093216	7.559706
5.576266	380.637233	7.564710
5.631597	379.163619	7.569715
5.522082	388.612082	7.574720
5.714495	377.976670	7.579725
5.691132	377.932783	7.584730
5.692350	375.002793	7.589734
5.743616	377.804156	7.594739
5.421979	372.115266	7.599744
5.681649	374.352452	7.604749
5.652928	385.240454	7.609754
5.533588	380.706305	7.614758
5.814173	379.890278	7.619763
5.359302	389.807314	7.624768
5.441407	381.704433	7.629773
5.428984	381.203240	7.634778
5.328753	390.507877	7.639782
5.766501	406.989238	7.644787
5.816933	404.605204	7.649792
5.986009	396.725978	7.654797
5.755848	390.393146	7.659802
5.818314	382.147805	7.664806
5.852244	373.562081	7.669811
5.709173	377.286094	7.674816
6.071095	375.109530	7.679821
5.667274	379.329990	7.684826
5.656805	372.564100	7.689830
5.483797	374.036990	7.694835
5.582186	384.778523	7.699840
6.039924	371.779288	7.704845
5.590407	368.632011	7.709850
5.430248	365.398268	7.714854
5.788006	374.764020	7.719859
5.502671	378.304673	7.724864
5.966558	376.143772	7.729869
5.757919	383.323475	7.734874
5.692471	381.330933	7.739878
5.690677	375.639386	7.744883
5.330992	386.278680	7.749888
5.647564	367.043501	7.754893
5.652045	375.797036	7.759898
5.575565	374.660458	7.764902
5.565007	374.500667	7.769907
5.299884	371.682012	7.774912
5.458893	375.795304	7.779917
5.619931	379.920934	7.784922
5.732402	368.712743	7.789926
5.332663	378.051645	7.794931
5.452903	381.724912	7.799936
5.843850	388.551239	7.804941
5.654879	397.955207	7.809946
5.667785	406.137946	7.814950
5.898678	396.521578	7.819955
5.768445	394.276586	7.824960
5.836102	380.791119	7.829965
5.477913	374.082873	7.834970
5.554937	377.854661	7.839974
5.583960	379.083920	7.844979
5.422198	387.626221	7.849984
5.951216	389.950925	7.854989
5.761734	396.093057	7.859994
5.865292	378.286492	7.864998
5.867203	378.896724	7.870003
5.493659	375.478108	7.875008
5.836141	379.404462	7.880013
5.716381	375.066537	7.885018
5.692376	373.738235	7.890022
5.555726	373.829160	7.895027
5.272642	378.226861	7.900032
5.337147	369.759737	7.905037
5.364769	380.645237	7.910042
5.838198	392.391062	7.915046
5.875239	396.007763	7.920051
5.617823	393.197388	7.925056
5.934671	388.623369	7.930061
5.711571	379.736219	7.935066
5.309675	371.323187	7.940070
5.958472	379.811254	7.945075
5.589971	381.514096	7.950080
5.575708	369.484181	7.955085
5.627805	377.907546	7.960090
5.788515	381.833906	7.965094
5.849813	382.352573	7.970099
5.779511	365.645802	7.975104
5.602883	376.284883	7.980109
5.573255	378.918583	7.985114
5.306251	375.363048	7.990118
5.484584	382.693435	7.995136
5.827106	394.820933	8.000154
5.792925	393.876313	8.005171
5.952206	384.226184	8.010189
5.467566	383.105993	8.015206
5.614792	381.325076	8.020224
5.674549	380.119589	8.025242
6.098419	378.273238	8.030259
5.483949	378.470407	8.035277
5.353485	376.499473	8.040294
5.897199	382.192397	8.045312
5.776183	386.752414	8.050330
6.023555	376.138601	8.055347
5.779611	386.161570	8.060365
5.620004	385.422793	8.065382
5.647545	376.850489	8.070400
5.484217	382.912966	8.075418
5.996308	392.022230	8.080435
5.875432	386.900338	8.085453
5.861206	384.295816	8.090470
5.992368	373.188979	8.095488
5.767628	376.856385	8.100506
5.976083	378.262663	8.105523
5.953323	377.556093	8.110541
5.587891	377.556455	8.115558
5.644148	382.281197	8.120576
5.566903	381.138201	8.125594
5.604164	385.392555	8.130611
5.470470	384.324674	8.135629
5.640081	394.399615	8.140646
5.761517	403.172466	8.145664
5.630480	401.703385	8.150682
5.575369	401.595167	8.155699
5.888102	402.357111	8.160717
6.141720	400.619482	8.165734
6.066515	397.746805	8.170752
5.723208	411.619613	8.175770
6.008822	401.233321	8.180787
6.141596	413.400007	8.185805
5.776267	408.278540	8.190822
5.782475	401.132819	8.195840
5.767777	417.207363	8.200858
5.961881	410.991553	8.205875
5.972220	406.694842	8.210893
5.959629	410.221719	8.215910
6.198537	407.561754	8.220928
5.563578	398.522046	8.225946
5.947585	390.288356	8.230963
5.785105	394.012282	8.235981
5.582184	410.668570	8.240998
6.009826	402.986609	8.246016
6.030465	404.586416	8.251034
6.169158	399.146143	8.256051
6.115420	410.392163	8.261069
5.733145	399.204811	8.266086
6.045754	401.711914	8.271104
5.867842	408.947474	8.276122
5.921242	406.565880	8.281139
6.123658	410.649199	8.286157
5.755778	411.486224	8.291174
6.083521	411.715647	8.296192
5.608113	410.934831	8.301210
5.633095	403.849283	8.306227
5.850334	407.131869	8.311245
5.983557	418.187657	8.316262
6.025531	406.605629	8.321280
5.807997	408.681405	8.326298
5.911916	403.341253	8.331315
6.001308	409.105369	8.336333
5.687783	398.670942	8.341350
6.145219	397.216956	8.346368
6.172707	404.136313	8.351386
5.873084	396.880723	8.356403
6.017009	401.702186	8.361421
5.678079	408.101450	8.366438
5.934659	404.927482	8.371456
6.019363	408.316039	8.376474
5.730287	405.609412	8.381491
6.200132	410.534445	8.386509
5.833985	415.596774	8.391526
5.933052	414.618653	8.396544
6.003049	416.863972	8.401562
5.931598	421.656070	8.406579
6.577647	426.323129	8.411597
6.083416	423.225769	8.416614
5.955993	409.615873	8.421632
5.876724	424.059541	8.426650
6.065837	434.876211	8.431667
6.338547	428.076884	8.436685
6.235730	435.982336	8.441702
6.235265	422.522951	8.446720
5.936191	422.288856	8.451738
6.076596	422.184718	8.456755
6.013597	430.800290	8.461773
6.108803	435.193898	8.466790
5.983940	430.564919	8.471808
6.002250	432.976127	8.476826
6.076267	438.079949	8.481843
6.440161	425.841562	8.486861
5.999158	440.439748	8.491878
6.362076	430.580964	8.496896
6.173713	439.913608	8.501914
6.126609	433.192789	8.506931
6.528203	430.813441	8.511949
6.047234	439.014826	8.516966
6.192749	429.332116	8.521984
6.353203	437.208942	8.527002
6.243199	439.188980	8.532019
6.508303	428.155796	8.537037
6.179368	441.275301	8.542054
6.553443	433.033681	8.547072
6.167996	426.694076	8.552090
6.338071	436.055764	8.557107
6.398109	434.073909	8.562125
5.918919	428.033012	8.567143
6.241930	423.627348	8.572160
6.084102	434.072347	8.577178
6.367276	437.114237	8.582195
6.356601	434.887844	8.587213
6.107983	435.239129	8.592231
6.542555	430.367865	8.597248
6.360614	431.772199	8.602266
6.285464	434.986994	8.607283
6.696871	432.855414	8.612301
6.282808	433.958449	8.617319
6.474899	415.100930	8.622336
6.329089	419.885743	8.627354
6.176590	422.238506	8.632371
6.397679	427.865231	8.637389
6.184605	437.902327	8.642407
6.172264	439.220129	8.647424
6.640413	436.429569	8.652442
6.529490	443.238085	8.657459
6.737698	425.053366	8.662477
6.369215	418.973035	8.667495
6.400624	410.359085	8.672512
5.993846	410.353302	8.677530
5.832337	427.735256	8.682547
6.422174	427.513365	8.687565
6.086231	430.074750	8.692583
6.278466	422.467533	8.697600
6.099323	433.020012	8.702618
6.204880	435.729972	8.707635
6.113424	430.316282	8.712653
6.237869	441.405018	8.717671
6.507651	434.265324	8.722688
6.011988	436.810709	8.727706
6.174091	440.748874	8.732723
6.805921	444.367292	8.737741
6.330816	445.754445	8.742759
6.553132	440.594545	8.747776
6.445995	445.600521	8.752794
6.398857	450.912677	8.757811
6.625675	454.058072	8.762829
6.537941	455.517075	8.767847
6.129219	445.081757	8.772864
6.727672	451.990569	8.777882
6.676605	461.314335	8.782899
6.800739	452.726861	8.787917
6.301736	448.702446	8.792935
6.337475	438.478358	8.797952
6.467284	450.806478	8.802970
6.482518	469.413624	8.807987
6.654535	453.522486	8.813005
6.497373	464.772122	8.818023
6.810228	454.397310	8.823040
6.778042	455.232233	8.828058
6.382918	455.638031	8.833075
6.635559	444.316459	8.838093
6.311425	443.773869	8.843111
6.582560	446.748219	8.848128
6.911548	462.869941	8.853146
6.680858	456.638621	8.858163
6.737415	438.755357	8.863181
6.570283	442.808222	8.868199
6.557170	440.541186	8.873216
6.502723	432.265721	8.878234
6.542288	443.023777	8.883251
6.810392	446.718119	8.888269
6.653940	443.299592	8.893287
6.947210	437.263894	8.898304
6.714712	438.281678	8.903322
6.466576	444.079755	8.908339
6.644404	432.807780	8.913357
6.732503	438.382763	8.918375
6.485682	430.011209	8.923392
6.773604	440.654613	8.928410
6.673473	452.374983	8.933427
6.840703	447.129039	8.938445
6.545726	452.587322	8.943463
6.608702	456.695655	8.948480
6.689390	461.066298	8.953498
6.708763	466.907676	8.958515
6.739304	458.319084	8.963533
6.641597	466.047025	8.968551
6.765110	462.546760	8.973568
6.954154	463.460629	8.978586
6.527916	469.681092	8.983603
7.138208	461.888438	8.988621
6.666104	457.913454	8.993639
6.766297	461.094470	8.998656
6.839402	467.807890	9.003674
6.687382	466.209549	9.008691
6.807888	464.237152	9.013709
6.846086	475.165854	9.018727
6.871652	470.115666	9.023744
6.637014	468.363013	9.028762
6.513799	472.191255	9.033779
6.893596	466.397608	9.038797
6.702246	466.105610	9.043815
6.813148	462.399039	9.048832
6.982269	458.071127	9.053850
7.044968	472.135987	9.058867
6.948521	465.164113	9.063885
7.008117	464.921159	9.068903
7.057255	456.320187	9.073920
6.718700	447.221391	9.078938
6.714199	461.707022	9.083955
6.742965	449.830393	9.088973
6.884447	461.891607	9.093991
6.928922	465.393775	9.099008
6.933337	462.688491	9.104026
6.780841	464.391169	9.109043
6.921421	470.989878	9.114061
6.507260	471.218780	9.119079
6.939261	463.372010	9.124096
6.816799	463.769801	9.129114
6.624151	468.852298	9.134131
6.761171	460.348007	9.139149
6.806649	461.631505	9.144167
6.892047	466.837694	9.149184
7.172686	466.190880	9.154202
6.970010	467.181903	9.159219
6.975234	465.208633	9.164237
6.912267	466.707937	9.169255
6.974820	462.046429	9.174272
6.783385	457.437340	9.179290
6.715493	465.580328	9.184307
7.210847	472.486367	9.189325
6.925111	467.368191	9.194343
6.616642	466.049980	9.199360
6.906440	462.684607	9.204378
6.834431	470.086634	9.209395
6.900972	484.586399	9.214413
7.210022	489.729151	9.219431
6.774246	499.851666	9.224448
7.393218	496.283234	9.229466
7.170979	493.449357	9.234483
7.107604	494.055640	9.239501
7.127486	487.125492	9.244519
7.072917	489.989935	9.249536
7.211650	481.479055	9.254554
6.829166	476.688457	9.259571
6.846179	481.908520	9.264589
7.195620	487.253224	9.269607
7.120246	485.573445	9.274624
7.231082	480.718176	9.279642
7.116133	497.928803	9.284659
7.218174	491.645339	9.289677
7.153662	487.685382	9.294695
6.869131	490.415444	9.299712
7.001924	492.073425	9.304730
7.112067	493.305769	9.309747
7.231067	479.814999	9.314765
7.122918	488.339843	9.319783
7.140037	491.423427	9.324800
7.297497	490.546606	9.329818
6.908536	497.853138	9.334835
7.445576	486.777312	9.339853
7.035568	490.022492	9.344871
6.791771	490.988400	9.349888
6.898677	487.153064	9.354906
7.169752	493.456782	9.359923
7.447569	485.634160	9.364941
7.425868	491.570342	9.369959
6.947957	496.214707	9.374976
7.267366	485.766266	9.379994
6.911237	487.456671	9.385011
7.185607	485.030977	9.390029
7.003043	484.901703	9.395047
7.069644	490.950281	9.400064
7.152035	502.597906	9.405082
6.968830	511.229194	9.410099
7.232748	508.555828	9.415117
7.438055	509.637564	9.420135
7.593068	524.978719	9.425152
7.682761	526.510913	9.430170
7.374279	514.317853	9.435187
7.405345	500.619940	9.440205
7.315164	494.578030	9.445223
7.024105	496.258239	9.450240
7.492685	509.063493	9.455258
7.400833	510.636754	9.460275
7.372421	509.053755	9.465293
7.235852	500.055828	9.470311
7.143238	523.025443	9.475328
7.213815	522.190635	9.480346
7.057832	530.012941	9.485363
7.508624	522.835384	9.490381
7.582993	519.330184	9.495399
7.451260	527.372751	9.500416
7.373923	519.359607	9.505434
7.283180	525.767363	9.510451
7.488080	521.894575	9.515469
7.497578	526.544631	9.520487
7.517891	522.599778	9.525504
7.633181	521.230947	9.530522
7.648881	519.887188	9.535539
7.515180	516.906892	9.540557
7.684924	521.377206	9.545575
7.813937	523.547020	9.550592
7.662789	502.038677	9.555610
7.405908	503.315904	9.560627
7.254902	500.754885	9.565645
7.435175	513.229776	9.570663
7.546670	516.885554	9.575680
7.677417	520.715041	9.580698
7.682584	515.863696	9.585715
7.648481	497.028907	9.590733
7.429140	489.893243	9.595751
7.431687	490.710103	9.600768
7.540055	499.980507	9.605786
7.636258	510.928544	9.610803
7.640169	514.787370	9.615821
7.959804	502.820951	9.620839
7.059740	504.514529	9.625856
7.565982	509.304500	9.630874
7.426579	510.891523	9.635891
7.484655	515.398265	9.640909
7.857016	511.019562	9.645927
7.791886	523.466638	9.650944
7.692140	514.544984	9.655962
7.847534	513.311881	9.660979
7.621610	501.607665	9.665997
7.988126	489.046933	9.671015
7.370828	493.176653	9.676032
7.292642	489.641713	9.681050
7.850392	510.013189	9.686067
7.853639	513.275675	9.691085
7.918187	499.496778	9.696103
7.652412	501.892545	9.701120
7.456619	495.314920	9.706138
7.815198	500.976930	9.711155
7.459879	497.624264	9.716173
7.427452	501.078528	9.721191
7.534630	511.018151	9.726208
7.965484	506.538766	9.731226
7.912002	514.922515	9.736243
7.826800	522.639054	9.741261
7.999942	517.751922	9.746279
8.129046	516.532406	9.751296
7.860991	493.786386	9.756314
7.513192	493.556769	9.761331
7.075039	492.833227	9.766349
7.598192	501.625236	9.771367
8.011575	511.573687	9.776384
8.258627	513.573529	9.781402
7.870378	515.606637	9.786419
7.657119	515.324382	9.791437
7.877813	521.746457	9.796455
7.692458	517.155335	9.801472
7.844837	515.755447	9.806490
7.970015	521.321490	9.811507
7.628875	521.876621	9.816525
7.896441	521.736780	9.821543
7.819819	521.483610	9.826560
7.718228	516.891986	9.831578
7.776987	522.597824	9.836595
7.572366	519.357241	9.841613
7.638334	515.559871	9.846631
7.494038	527.359793	9.851648
7.861585	526.197590	9.856666
7.964841	523.681938	9.861683
7.396342	519.747289	9.866701
7.934927	517.763030	9.871719
7.609742	519.316046	9.876736
7.729990	537.733241	9.881754
7.893195	541.178952	9.886771
7.601002	546.195016	9.891789
8.079203	543.393398	9.896807
7.865261	547.683993	9.901824
7.901140	548.719694	9.906842
8.287013	546.806696	9.911859
8.148558	542.220842	9.916877
8.180327	542.288359	9.921895
8.020253	549.530648	9.926912
8.063859	546.651955	9.931930
8.217245	551.572961	9.936947
7.923093	542.129490	9.941965
8.238264	543.793615	9.946983
7.840606	552.464834	9.952000
7.944123	551.564904	9.957018
8.014456	555.703664	9.962035
8.030421	552.548435	9.967053
8.207961	556.600971	9.972071
7.949852	553.280401	9.977088
7.945177	536.915102	9.982106
7.983369	549.137725	9.987123
7.724099	549.206660	9.992141
8.409304	548.657402	9.997159
8.112240	554.011902	10.002176
7.883129	542.481726	10.007194
8.063891	540.944847	10.012211
8.076959	549.567492	10.017229
8.184228	548.212539	10.022247
8.014624	543.745174	10.027264
8.136335	541.286588	10.032282
8.236353	546.742972	10.037299
8.299683	547.152681	10.042317
8.316825	545.704552	10.047335
8.325366	553.551584	10.052352
8.250729	546.336421	10.057370
8.444480	547.880715	10.062387
8.406018	556.353648	10.067405
8.323225	551.134223	10.072423
8.344889	547.905518	10.077440
7.974937	548.174831	10.082458
8.157733	545.987539	10.087475
8.088570	546.414850	10.092493
8.372085	545.578236	10.097511
8.297569	552.863926	10.102528
7.974176	542.071200	10.107546
8.333525	538.502412	10.112563
8.179527	543.421084	10.117581
8.478020	549.808889	10.122599
8.184563	545.597613	10.127616
8.031989	545.318473	10.132634
8.261074	541.798496	10.137651
8.041954	552.167961	10.142669
8.062121	543.173857	10.147687
8.222290	555.042858	10.152704
8.869341	555.373733	10.157722
8.469379	551.554682	10.162739
8.221116	541.788441	10.167757
8.080932	546.004364	10.172775
8.218812	557.791653	10.177792
8.343177	569.685209	10.182810
8.578250	566.795448	10.187827
8.137106	567.561908	10.192845
8.476700	559.271984	10.197863
8.715901	570.563725	10.202880
8.364751	572.332252	10.207898
8.580904	566.469539	10.212915
8.315647	565.261314	10.217933
8.431388	556.580431	10.222951
8.297905	559.574015	10.227968
8.576736	565.753468	10.232986
8.684140	565.200065	10.238003
8.253456	572.610995	10.243021
8.221614	575.108975	10.248039
8.471634	566.258727	10.253056
8.456846	570.761121	10.258074
8.461133	560.191597	10.263091
8.401386	561.658847	10.268109
8.741230	564.622452	10.273127
8.266704	563.131436	10.278144
8.041736	567.035601	10.283162
8.353852	557.288849	10.288179
8.189304	563.007596	10.293197
8.555394	568.608491	10.298215
8.313036	576.949278	10.303232
8.628677	585.366743	10.308250
8.535370	584.292522	10.313267
8.487856	596.979885	10.318285
9.074118	591.532545	10.323303
9.041342	583.932112	10.328320
8.634637	576.503878	10.333338
8.532530	569.311945	10.338355
8.315238	569.828738	10.343373
8.935076	582.490425	10.348391
8.724643	588.093293	10.353408
8.657600	583.852846	10.358426
8.374258	581.419847	10.363443
8.666658	586.533678	10.368461
8.813311	581.843183	10.373479
8.760099	584.129918	10.378496
8.550278	589.792651	10.383514
8.806316	590.061714	10.388531
8.843399	592.321680	10.393549
8.780191	587.036060	10.398567
8.922983	587.717342	10.403584
8.993089	587.611594	10.408602
8.867903	578.283641	10.413619
8.723614	575.749962	10.418637
8.882345	574.683589	10.423655
8.467341	565.691384	10.428672
8.653317	575.520867	10.433690
9.140164	589.838100	10.438707
8.981314	585.012434	10.443725
8.157013	567.440623	10.448743
8.866647	579.147811	10.453760
8.904400	587.548857	10.458778
8.973796	586.938293	10.463795
8.891860	588.765626	10.468813
8.730171	587.055180	10.473831
9.033774	591.132154	10.478848
9.128877	598.940396	10.483866
8.916316	586.789062	10.488883
8.528891	589.734075	10.493901
8.610554	589.806398	10.498919
8.552615	594.280845	10.503936
8.936312	600.355517	10.508954
9.273444	586.095189	10.513971
8.811934	597.032832	10.518989
8.446608	601.296666	10.524007
9.078212	593.844598	10.529024
8.690943	596.906353	10.534042
9.174136	593.100400	10.539059
9.131717	597.307329	10.544077
9.057691	594.639562	10.549095
9.164261	590.624375	10.554112
8.822860	593.833578	10.559130
8.748547	595.157945	10.564147
8.747042	600.447216	10.569165
8.820577	599.892807	10.574183
9.042592	585.726255	10.579200
8.852715	594.876179	10.584218
9.089131	587.807924	10.589235
8.956012	596.267304	10.594253
8.850034	586.346201	10.599271
9.272563	588.694098	10.604288
9.050282	601.323640	10.609306
9.102037	592.618051	10.614323
9.353713	597.552073	10.619341
9.225560	600.781513	10.624359
9.081592	590.553937	10.629376
9.119273	584.141669	10.634394
8.910871	578.414898	10.639411
9.023694	594.804137	10.644429
9.228421	608.802671	10.649447
9.371490	605.299314	10.654464
9.254464	591.829661	10.659482
9.304387	590.420574	10.664499
9.078324	587.536788	10.669517
9.033667	592.801260	10.674535
9.102600	601.023858	10.679552
9.324251	610.450139	10.684570
9.481820	605.511775	10.689587
8.934909	589.376553	10.694605
9.206738	596.955134	10.699623
9.558766	603.334570	10.704640
9.328074	611.417926	10.709658
9.192675	593.454129	10.714675
9.264559	591.713398	10.719693
9.058673	590.360170	10.724711
9.332496	599.292278	10.729728
9.066680	622.494286	10.734746
9.922054	611.119198	10.739763
9.242249	606.056413	10.744781
8.912677	600.992403	10.749799
9.425499	612.080355	10.754816
9.351474	616.248059	10.759834
9.383278	609.622108	10.764851
9.410447	615.042590	10.769869
9.312859	618.043183	10.774887
9.381398	615.728617	10.779904
9.300496	626.385737	10.784922
9.543434	614.393391	10.789939
9.729477	621.527832	10.794957
9.539153	609.133157	10.799975
9.883701	586.240544	10.804992
9.041415	593.731751	10.810010
9.083507	591.957818	10.815027
9.363502	610.984375	10.820045
9.270188	613.129074	10.825063
9.500804	611.675896	10.830080
9.479971	616.516920	10.835098
9.552741	613.220236	10.840115
9.164417	614.328716	10.845133
9.306837	618.105902	10.850151
9.168215	615.135828	10.855168
9.237814	618.394249	10.860186
9.529614	621.075056	10.865203
9.515500	615.254717	10.870221
9.254057	617.529900	10.875239
9.390064	614.687212	10.880256
9.281937	622.953340	10.885274
9.189265	628.941713	10.890291
9.527100	633.363628	10.895309
9.532131	634.767085	10.900327
9.451803	645.771267	10.905344
9.472361	641.977828	10.910362
9.772080	638.011263	10.915379
9.944679	633.998345	10.920397
9.658448	651.018204	10.925415
10.048013	635.531478	10.930432
9.908579	645.295219	10.935450
9.897744	633.557216	10.940467
9.427504	625.624519	10.945485
9.217250	623.817537	10.950503
9.898629	635.204142	10.955520
9.698509	643.898104	10.960538
9.856547	648.278765	10.965555
10.196183	642.475575	10.970573
10.159867	634.689482	10.975591
9.713477	626.494272	10.980608
9.565569	618.589971	10.985626
9.601266	617.426108	10.990643
9.893593	616.919469	10.995661
9.298533	613.954638	11.000679
9.683617	620.679196	11.005696
9.803497	635.132857	11.010714
9.857219	636.168923	11.015731
9.914964	634.502987	11.020749
10.089439	641.481457	11.025767
10.120782	618.896652	11.030784
9.723084	610.330902	11.035802
9.884703	612.038027	11.040819
9.809402	612.560977	11.045837
9.378620	614.818510	11.050855
9.823678	621.899746	11.055872
9.668693	638.406724	11.060890
9.808083	644.825803	11.065907
9.641308	629.994294	11.070925
9.694279	644.499471	11.075943
10.183637	642.472419	11.080960
9.864600	647.107709	11.085978
10.057852	647.089964	11.090995
10.209998	640.391498	11.096013
10.049325	639.425658	11.101031
10.200904	636.211297	11.106048
10.241892	638.357047	11.111066
10.228933	638.131770	11.116083
9.891885	624.084339	11.121101
9.706692	629.421333	11.126119
10.155980	632.531904	11.131136
9.851034	631.632851	11.136154
9.846350	634.517904	11.141171
9.735758	638.738680	11.146189
9.863735	637.427813	11.151207
10.036232	623.789698	11.156224
9.896195	637.536158	11.161242
9.922057	632.750966	11.166259
10.074161	636.394095	11.171277
9.638881	644.014057	11.176295
9.838298	638.718833	11.181312
9.851381	643.892222	11.186330
10.014965	649.363924	11.191347
10.346151	660.032239	11.196365
9.950011	677.198732	11.201383
10.436052	662.788779	11.206400
10.104775	656.857172	11.211418
9.826522	660.911717	11.216435
10.186056	659.116444	11.221453
9.980798	669.111418	11.226471
9.861597	672.812841	11.231488
10.193972	672.129513	11.236506
10.095191	669.822220	11.241523
10.482899	664.462773	11.246541
10.108981	670.946507	11.251559
10.682835	660.622201	11.256576
10.493688	666.600456	11.261594
10.240311	666.416003	11.266611
10.361646	666.636745	11.271629
10.334529	670.367921	11.276647
10.374179	664.504428	11.281664
10.367053	666.503085	11.286682
9.778358	659.141200	11.291699
10.403378	667.431336	11.296717
10.356263	673.977478	11.301735
10.283755	659.724468	11.306752
10.494806	669.411218	11.311770
10.294887	667.874012	11.316787
10.554656	659.830079	11.321805
10.324386	665.571779	11.326823
10.770102	664.716057	11.331840
10.689925	662.595200	11.336858
10.257385	665.802915	11.341875
10.573662	661.202589	11.346893
10.461259	666.051661	11.351911
10.265018	658.012904	11.356928
10.393523	658.636466	11.361946
10.144022	659.035231	11.366963
10.230555	663.042090	11.371981
10.088137	669.798822	11.376999
10.377050	664.369647	11.382016
10.580566	658.783439	11.387034
10.188333	665.355248	11.392051
10.487609	657.361930	11.397069
10.304962	662.521810	11.402087
10.463456	664.068483	11.407104
10.696288	673.786537	11.412122
10.506226	671.764946	11.417139
10.989394	654.985433	11.422157
10.564595	665.573381	11.427175
10.653004	659.847418	11.432192
10.836196	655.378398	11.437210
10.250368	660.655095	11.442227
10.663843	668.082125	11.447245
10.351718	656.539636	11.452263
10.595606	665.088303	11.457280
10.780278	673.258086	11.462298
10.459013	682.131994	11.467315
11.051767	675.680063	11.472333
10.779273	667.785792	11.477351
10.482232	660.050006	11.482368
10.491706	661.544288	11.487386
10.577688	682.254965	11.492403
10.639476	690.664917	11.497421
10.827212	695.056716	11.502439
10.651084	685.253847	11.507456
10.652727	689.374999	11.512474
10.546037	703.311945	11.517491
10.965477	694.110040	11.522509
11.136604	694.111541	11.527527
11.114283	687.181615	11.532544
11.175733	687.080380	11.537562
10.794458	673.443783	11.542579
10.774277	660.312357	11.547597
10.800705	667.216203	11.552615
10.425415	674.091474	11.557632
10.949710	683.823828	11.562650
10.594269	692.668382	11.567667
10.749590	685.177291	11.572685
10.818266	690.711214	11.577703
11.302383	685.068411	11.582720
11.076888	674.847248	11.587738
11.034842	686.640722	11.592755
11.099701	693.396545	11.597773
10.905387	691.546033	11.602791
10.847531	694.357375	11.607808
11.069802	685.666051	11.612826
10.913182	693.901940	11.617843
10.993495	696.675856	11.622861
10.825093	689.582624	11.627879
10.658260	691.319127	11.632896
10.971720	692.996158	11.637914
10.843101	692.669081	11.642931
10.954278	696.324946	11.647949
11.107038	698.443724	11.652967
10.920084	694.692254	11.657984
11.154962	686.216706	11.663002
11.053203	694.563921	11.668019
11.405458	687.247102	11.673037
11.264364	689.645450	11.678055
10.854775	683.060227	11.683072
11.115455	692.215348	11.688090
11.120076	690.807039	11.693107
11.311260	681.893368	11.698125
11.233771	679.951969	11.703143
10.783475	671.870959	11.708160
11.016175	683.990615	11.713178
11.336021	687.001556	11.718195
11.538434	684.691252	11.723213
10.999715	687.631584	11.728231
11.305459	687.006076	11.733248
11.246189	679.185691	11.738266
11.084299	691.761653	11.743283
11.180264	687.378875	11.748301
10.861549	681.107619	11.753319
10.914100	690.257479	11.758336
11.045224	681.157558	11.763354
10.858691	695.368941	11.768371
11.431152	705.144253	11.773389
11.655228	706.948900	11.778407
11.353549	719.385836	11.783424
11.930083	706.703684	11.788442
11.000992	696.532787	11.793459
11.170239	690.465942	11.798477
11.356428	688.338062	11.803495
11.298627	697.877602	11.808512
11.331426	698.879080	11.813530
11.333411	713.427016	11.818547
11.732143	703.761288	11.823565
11.403804	692.161356	11.828583
11.600028	697.530129	11.833600
11.298467	691.139417	11.838618
11.272377	688.116986	11.843635
11.513107	705.761236	11.848653
11.656381	712.107147	11.853671
11.215027	710.500467	11.858688
11.624133	712.992496	11.863706
11.605389	712.799682	11.868723
11.071622	709.468623	11.873741
11.461793	717.991240	11.878759
11.349257	717.336592	11.883776
11.438609	712.929598	11.888794
11.198345	718.997930	11.893811
11.336265	720.453157	11.898829
11.420735	720.682832	11.903847
11.362019	717.520339	11.908864
11.432342	714.845717	11.913882
11.459503	719.215343	11.918899
11.334319	709.666413	11.923917
11.601447	720.243814	11.928935
11.841247	734.192769	11.933952
11.884631	730.692384	11.938970
11.369981	723.101118	11.943987
11.754184	728.389956	11.949005
12.001441	733.409915	11.954023
11.829920	720.800776	11.959040
11.719790	713.837261	11.964058
11.611898	708.807916	11.969075
11.558510	715.932571	11.974093
11.337162	716.434224	11.979111
11.754055	729.424461	11.984128
12.125366	731.651013	11.989146
11.812241	734.925238	11.994163
11.891346	737.977062	11.999181
12.293046	727.720717	12.004199
11.901120	721.063283	12.009216
11.889337	716.776276	12.014234
11.835217	718.100644	12.019251
11.896675	716.487768	12.024269
11.753144	707.304633	12.029287
11.559194	713.697069	12.034304
11.848753	713.604274	12.039322
12.066056	734.938226	12.044339
11.989360	731.623912	12.049357
11.988229	716.078409	12.054375
11.547653	720.177335	12.059392
11.867509	726.161067	12.064410
11.979512	733.509126	12.069427
12.180369	737.946217	12.074445
12.064912	739.927142	12.079463
11.817912	733.606761	12.084480
12.205705	739.838631	12.089498
11.858757	746.438088	12.094515
11.878573	740.495626	12.099533
12.242714	742.104760	12.104551
12.112429	742.115616	12.109568
11.907182	729.858896	12.114586
11.513523	736.926419	12.119603
12.118520	743.177908	12.124621
11.908547	738.237133	12.129639
12.153930	743.585595	12.134656
12.404979	741.876738	12.139674
12.285564	741.516660	12.144691
12.319773	742.047701	12.149709
12.662233	741.290206	12.154727
12.031868	728.999107	12.159744
12.191782	722.794858	12.164762
11.998147	725.138326	12.169779
12.245379	738.114126	12.174797
12.220370	740.620526	12.179815
12.081717	740.698966	12.184832
12.241863	737.663126	12.189850
12.019331	741.172468	12.194867
11.858576	741.222812	12.199885
12.030643	732.507773	12.204903
12.267733	739.697379	12.209920
11.995297	741.939586	12.214938
12.308091	737.690083	12.219955
12.004098	735.519077	12.224973
12.094607	744.612524	12.229991
11.763939	749.208636	12.235008
12.133202	750.188959	12.240026
12.423091	763.754546	12.245043
12.406130	771.321643	12.250061
12.426345	767.787010	12.255079
12.446421	768.806265	12.260096
12.463568	766.493420	12.265114
12.376653	769.511301	12.270131
12.666886	773.416841	12.275149
12.785422	764.707017	12.280167
12.309312	747.557003	12.285184
12.341345	741.114006	12.290202
12.195689	746.864565	12.295219
12.180531	753.815986	12.300237
12.248716	754.777210	12.305255
12.169439	764.531591	12.310272
12.381443	762.914057	12.315290
12.547034	756.683660	12.320307
12.300510	762.446873	12.325325
12.441483	763.567107	12.330343
12.370815	768.283435	12.335360
12.822286	763.620874	12.340378
12.803381	758.407158	12.345395
12.318698	758.404113	12.350413
12.863030	756.920705	12.355431
12.571692	759.143786	12.360448
12.806683	754.291081	12.365466
12.519351	764.955381	12.370483
12.422541	761.054073	12.375501
12.613590	758.824436	12.380519
12.435695	766.868031	12.385536
12.557472	760.865405	12.390554
12.576013	762.175236	12.395571
12.824110	771.714226	12.400589
12.996820	769.834602	12.405607
12.618011	765.576686	12.410624
12.823477	759.087574	12.415642
12.921360	762.407862	12.420659
12.565110	762.179564	12.425677
13.396642	762.408956	12.430695
12.989364	765.723185	12.435712
13.102752	760.258366	12.440730
12.891723	755.718542	12.445747
13.180062	755.717457	12.450765
13.047592	750.695108	12.455783
12.850193	755.863637	12.460800
13.050311	757.933976	12.465818
12.803608	768.326823	12.470835
12.599207	763.139013	12.475853
12.877869	757.064470	12.480871
12.877661	760.826164	12.485888
12.813550	767.173029	12.490906
12.892701	763.723837	12.495923
12.496328	769.377985	12.500941
12.701259	759.471191	12.505959
12.629289	763.799555	12.510976
12.602410	776.670006	12.515994
12.980362	784.850583	12.521011
13.293135	788.336025	12.526029
13.293801	787.786716	12.531047
13.030904	786.761144	12.536064
13.084991	783.864991	12.541082
13.487512	783.296902	12.546099
13.203511	779.175608	12.551117
13.137104	767.676600	12.556135
13.133698	767.364617	12.561152
13.166323	763.585041	12.566170
13.282582	763.276400	12.571187
12.935552	763.624175	12.576205
13.048176	774.860138	12.581223
13.262314	784.578026	12.586240
13.391533	788.906432	12.591258
13.560256	776.840397	12.596275
12.998650	767.631216	12.601293
13.194577	768.042245	12.606311
13.019618	764.228921	12.611328
13.063113	776.747516	12.616346
13.598632	778.579114	12.621363
13.386859	782.790530	12.626381
13.537689	776.379400	12.631399
12.803544	766.285216	12.636416
13.144060	779.461028	12.641434
13.143083	771.085509	12.646451
12.687825	776.124030	12.651469
13.375071	787.768593	12.656487
13.544525	782.361254	12.661504
13.124714	793.431340	12.666522
13.717127	785.543517	12.671539
13.175818	787.026274	12.676557
13.354797	780.945251	12.681575
13.293900	781.503818	12.686592
13.277416	780.209264	12.691610
13.501222	788.114190	12.696627
13.375737	787.070244	12.701645
13.289567	778.768031	12.706663
13.484363	782.723240	12.711680
13.127878	788.730910	12.716698
13.375034	791.819530	12.721715
13.557847	804.994822	12.726733
13.830193	817.752149	12.731751
14.018021	807.649189	12.736768
13.454206	790.462382	12.741786
13.641270	786.803772	12.746803
13.670590	783.223528	12.751821
13.584773	781.267643	12.756839
13.633902	779.953341	12.761856
13.440084	784.581670	12.766874
13.869799	775.785216	12.771891
13.552400	788.669636	12.776909
13.453140	777.059003	12.781927
13.548296	798.869764	12.786944
13.781638	804.371611	12.791962
14.115176	799.238364	12.796979
13.914168	797.092241	12.801997
13.764238	790.873397	12.807015
13.820267	774.690876	12.812032
13.377864	785.000784	12.817050
14.212878	791.522367	12.822067
13.626983	799.263824	12.827085
13.690233	787.230087	12.832103
13.850791	788.501890	12.837120
14.095589	794.383795	12.842138
13.595857	786.433556	12.847155
13.321409	798.039452	12.852173
13.761912	810.615790	12.857191
13.811165	807.130249	12.862208
13.911798	811.791347	12.867226
13.739533	812.847051	12.872243
13.579324	809.877171	12.877261
13.950634	805.703691	12.882279
14.273250	811.945799	12.887296
13.623827	811.687694	12.892314
14.050659	809.298031	12.897331
13.695866	821.749672	12.902349
13.755532	808.978015	12.907367
13.770555	813.049761	12.912384
14.066087	812.558395	12.917402
13.990172	811.740214	12.922419
13.905062	809.011035	12.927437
14.132978	803.569284	12.932455
14.023532	817.244817	12.937472
13.925900	827.166211	12.942490
14.335756	826.675868	12.947507
14.066307	831.271876	12.952525
14.465918	828.406788	12.957543
14.491268	813.535557	12.962560
14.197412	812.880912	12.967578
14.009583	804.036031	12.972595
14.197516	806.758388	12.977613
14.231617	797.676765	12.982631
14.049441	805.519074	12.987648
13.831050	809.930351	12.992666
14.122122	816.221584	12.997683
14.015668	832.033163	13.002701
14.489032	822.914263	13.007719
14.877521	823.490786	13.012736
14.344847	828.210087	13.017754
14.687648	823.359408	13.022771
14.769977	818.470644	13.027789
14.603967	807.656254	13.032807
14.758515	789.965571	13.037824
14.405022	799.813429	13.042842
14.565824	796.111595	13.047859
14.413041	799.445917	13.052877
14.320704	790.014875	13.057895
14.529340	801.122201	13.062912
14.288189	804.896408	13.067930
14.067561	800.746244	13.072947
14.432268	802.727685	13.077965
14.610623	808.367538	13.082983
14.769117	800.093254	13.088000
14.473335	810.127736	13.093018
14.735479	802.474691	13.098035
14.211471	812.516531	13.103053
14.565958	811.858136	13.108071
14.371231	809.329170	13.113088
14.459317	812.373288	13.118106
14.292194	803.783942	13.123123
14.585931	816.285449	13.128141
14.792076	825.966741	13.133159
15.026587	809.472198	13.138176
14.478977	812.865228	13.143194
14.503635	806.644271	13.148211
14.271932	812.035944	13.153229
14.501598	820.829914	13.158247
14.761481	829.025855	13.163264
14.623351	837.457731	13.168282
14.870938	829.216812	13.173299
14.678849	837.010194	13.178317
14.513450	835.656915	13.183335
14.863614	836.381456	13.188352
14.823979	843.778566	13.193370
15.039777	842.059444	13.198387
14.915617	841.356119	13.203405
14.744631	838.997001	13.208423
14.892869	837.985907	13.213440
14.890405	839.422113	13.218458
15.101086	834.689962	13.223475
15.054341	837.928781	13.228493
15.001947	832.164862	13.233511
15.264479	829.507445	13.238528
14.620488	842.739723	13.243546
14.790709	840.929911	13.248563
14.769628	847.118582	13.253581
14.795799	840.648065	13.258599
14.701193	833.404356	13.263616
14.823741	836.547222	13.268634
15.002688	829.251188	13.273651
15.176646	835.993127	13.278669
14.717274	837.709206	13.283687
15.133583	831.796112	13.288704
14.969123	836.684945	13.293722
15.277306	831.836531	13.298739
15.253862	841.042557	13.303757
14.617205	838.324049	13.308775
14.824941	830.505945	13.313792
14.943581	838.045513	13.318810
15.073036	850.452861	13.323827
15.237242	847.422678	13.328845
15.427927	852.978562	13.333863
15.643080	848.277265	13.338880
15.169724	843.128415	13.343898
15.194535	831.043866	13.348915
15.140363	836.956848	13.353933
15.107133	845.646851	13.358951
15.322425	847.291940	13.363968
15.486956	848.313813	13.368986
15.442544	848.383800	13.374003
15.293206	835.635402	13.379021
15.361274	843.457455	13.384039
15.505924	841.074130	13.389056
15.411710	836.250892	13.394074
15.327441	823.078893	13.399091
15.428692	831.845650	13.404109
15.377299	842.886445	13.409127
15.783987	850.021122	13.414144
15.271410	842.107584	13.419162
15.238120	828.268023	13.424179
15.457412	840.718094	13.429197
15.596980	855.550706	13.434215
15.689912	852.323403	13.439232
15.636172	857.371622	13.444250
15.355644	850.359011	13.449267
15.454345	847.345403	13.454285
15.583198	847.495541	13.459303
15.828879	855.248745	13.464320
15.350945	854.979550	13.469338
15.871697	858.151549	13.474355
15.933366	853.341753	13.479373
15.326926	841.043672	13.484391
15.799104	838.577472	13.489408
15.696653	837.832876	13.494426
15.256490	835.746309	13.499443
15.795264	840.483936	13.504461
15.466853	854.657713	13.509479
15.709402	840.680249	13.514496
15.461929	854.102877	13.519514
15.633444	852.056173	13.524531
15.851672	855.310285	13.529549
15.637220	863.378585	13.534567
15.903603	856.867270	13.539584
15.777262	849.625371	13.544602
15.795057	857.985489	13.549619
16.223336	854.207021	13.554637
15.584381	859.283814	13.559655
15.598273	860.275640	13.564672
15.299859	848.860268	13.569690
15.258263	852.701049	13.574707
15.472688	860.781049	13.579725
15.082924	875.428365	13.584743
15.688809	873.944773	13.589760
16.007833	880.111726	13.594778
16.307588	878.019680	13.599795
16.104937	870.392091	13.604813
16.329948	872.474323	13.609831
16.253834	874.616359	13.614848
15.965402	881.913608	13.619866
15.988269	877.564327	13.624883
16.120050	878.054839	13.629901
16.062490	881.983336	13.634919
16.297165	872.857626	13.639936
15.968691	879.675146	13.644954
15.786548	873.985192	13.649971
16.684431	869.331558	13.654989
16.284248	869.125921	13.660007
16.115596	867.438629	13.665024
16.128835	879.567556	13.670042
16.183096	871.410558	13.675059
16.308297	872.239776	13.680077
16.210899	873.996976	13.685095
16.127105	874.619095	13.690112
16.136792	876.327959	13.695130
16.181034	875.386806	13.700147
15.785802	878.102712	13.705165
16.184913	880.946630	13.710183
17.068505	888.637772	13.715200
16.557954	880.301016	13.720218
16.247602	873.097405	13.725235
16.102795	866.887200	13.730253
16.296415	870.634327	13.735271
16.686134	880.940148	13.740288
16.488512	872.014716	13.745306
16.194522	873.117898	13.750323
16.590241	877.619169	13.755341
16.514266	885.466964	13.760359
16.532572	886.821024	13.765376
16.532770	885.069405	13.770394
16.474665	898.421370	13.775411
16.713583	890.213340	13.780429
16.657173	894.403596	13.785447
16.716239	896.297233	13.790464
16.742062	894.582624	13.795482
16.498380	874.776712	13.800499
16.722384	877.165220	13.805517
16.360871	878.471489	13.810535
16.892910	887.069791	13.815552
16.802673	884.120494	13.820570
16.575922	884.944894	13.825587
16.600396	877.382705	13.830605
16.502973	898.207576	13.835623
17.031485	890.140369	13.840640
16.698587	893.622851	13.845658
16.864211	895.452454	13.850675
17.027458	897.550678	13.855693
16.837919	895.323849	13.860711
16.924251	887.133415	13.865728
16.722135	888.477828	13.870746
16.627615	897.300537	13.875763
17.068401	887.959487	13.880781
16.822817	897.171943	13.885799
16.912544	887.106400	13.890816
16.863507	895.142486	13.895834
16.737103	889.308092	13.900851
16.914282	887.475095	13.905869
16.736593	883.131989	13.910887
16.982993	886.031393	13.915904
17.265215	897.638499	13.920922
16.820392	889.051595	13.925939
17.164741	892.225992	13.930957
16.783030	898.240807	13.935975
16.720711	893.734453	13.940992
17.281284	900.826104	13.946010
16.951911	907.088346	13.951027
17.135742	888.531428	13.956045
17.054412	890.207217	13.961063
17.304901	885.143762	13.966080
16.644902	892.126841	13.971098
16.890550	897.812984	13.976115
17.613956	891.662403	13.981133
17.042598	897.874191	13.986151
16.820118	891.010262	13.991168
17.264291	908.660709	13.996186
17.212116	917.202233	14.001203
17.693519	914.886059	14.006221
17.640564	923.920023	14.011239
17.644876	901.547383	14.016256
17.236758	891.136954	14.021274
17.287425	891.662266	14.026291
17.551374	885.536336	14.031309
17.040933	886.805978	14.036327
17.113975	897.287659	14.041344
17.431307	904.493163	14.046362
17.259489	911.273528	14.051379
17.542614	907.823909	14.056397
17.326669	908.832813	14.061415
17.476632	910.999393	14.066432
17.856107	905.256150	14.071450
17.762579	905.469533	14.076467
17.897200	910.967946	14.081485
17.822477	898.573892	14.086503
17.551430	883.275664	14.091520
17.619468	877.909434	14.096538
17.406474	884.554226	14.101555
17.733608	884.550220	14.106573
17.864655	895.060682	14.111591
17.247249	888.441669	14.116608
17.491524	890.464080	14.121626
17.573903	905.138433	14.126643
18.012657	905.208459	14.131661
17.669956	906.710601	14.136679
17.388937	900.032568	14.141696
17.624205	894.425533	14.146714
17.605509	915.932379	14.151731
17.647984	898.865072	14.156749
17.657752	900.198379	14.161767
17.764714	903.103854	14.166784
17.944299	901.163179	14.171802
17.585523	902.973958	14.176819
17.692345	900.817461	14.181837
17.612668	904.313921	14.186855
17.715064	895.622341	14.191872
17.356223	903.334580	14.196890
17.445376	920.702986	14.201907
17.862663	918.188570	14.206925
18.017695	931.800662	14.211943
18.215683	923.826251	14.216960
18.070543	918.704851	14.221978
18.080446	927.249278	14.226995
18.405319	920.870790	14.232013
18.127214	926.954589	14.237031
18.401156	927.769973	14.242048
18.016671	921.376390	14.247066
17.759025	930.991548	14.252083
17.860775	930.218110	14.257101
17.908319	929.083929	14.262119
17.994819	927.609124	14.267136
18.083991	928.055819	14.272154
17.994527	921.423506	14.277171
18.181244	924.022993	14.282189
17.949454	920.818152	14.287207
18.072327	931.008019	14.292224
17.959789	939.110879	14.297242
18.183387	948.511788	14.302259
18.744290	945.122784	14.307277
18.527816	942.483595	14.312295
18.525410	946.368751	14.317312
18.632821	937.906743	14.322330
18.391226	937.000904	14.327347
18.358689	931.909195	14.332365
18.189623	932.970718	14.337383
18.219826	943.225604	14.342400
18.452443	944.845897	14.347418
18.523696	942.666566	14.352435
18.670445	944.852588	14.357453
18.699005	953.053271	14.362471
18.357777	949.682532	14.367488
18.780044	945.759817	14.372506
18.648352	940.241821	14.377523
18.451345	945.041107	14.382541
18.962760	942.114302	14.387559
18.537075	941.830607	14.392576
18.578573	939.539171	14.397594
18.947426	936.666262	14.402611
18.814526	934.203332	14.407629
18.785814	928.940608	14.412647
18.544395	930.247000	14.417664
18.616928	935.123976	14.422682
18.860709	941.558365	14.427699
18.965413	937.868447	14.432717
18.950189	935.977225	14.437735
18.752219	947.189376	14.442752
19.012937	949.026177	14.447770
19.111666	941.900458	14.452787
18.886848	925.389411	14.457805
18.588467	918.811922	14.462823
18.318996	921.943639	14.467840
18.711937	939.703131	14.472858
18.602433	934.472000	14.477875
18.789497	936.591744	14.482893
18.859651	945.158298	14.487911
18.943265	951.166497	14.492928
18.735552	940.835095	14.497946
18.753383	942.713107	14.502963
18.643595	941.893915	14.507981
19.179121	955.926101	14.512999
19.102503	955.868587	14.518016
19.125467	938.075295	14.523034
19.175715	945.212207	14.528051
18.774606	957.532340	14.533069
18.801279	958.178180	14.538087
19.280105	966.794326	14.543104
19.624317	957.645099	14.548122
19.300038	964.395721	14.553139
19.486010	967.632816	14.558157
19.481439	955.546475	14.563175
18.854961	947.612865	14.568192
19.315668	945.454567	14.573210
19.451339	959.754536	14.578227
19.512775	962.891219	14.583245
19.589842	950.580647	14.588263
19.315030	941.739859	14.593280
19.423700	929.477999	14.598298
18.993118	939.839793	14.603315
19.589358	941.002320	14.608333
19.631463	951.602491	14.613351
19.593522	947.275345	14.618368
19.449031	925.468797	14.623386
19.580924	928.518695	14.628403
19.570920	928.794733	14.633421
19.214025	931.539354	14.638439
19.225380	946.796081	14.643456
19.662977	951.966165	14.648474
19.689999	959.393904	14.653491
19.790572	965.462568	14.658509
20.014092	958.784359	14.663527
19.595758	947.851624	14.668544
19.760696	955.118896	14.673562
19.491596	956.224495	14.678579
19.869122	956.521868	14.683597
20.093590	952.649078	14.688615
19.339485	943.741369	14.693632
19.753034	953.200883	14.698650
19.704426	960.804578	14.703667
19.755337	957.211449	14.708685
20.472730	960.759764	14.713703
19.695155	950.706994	14.718720
19.724799	952.251789	14.723738
19.848747	952.601516	14.728755
20.090377	963.766892	14.733773
20.259230	954.657765	14.738791
19.956453	946.610322	14.743808
19.535097	931.038951	14.748826
19.809464	944.471406	14.753843
19.694152	958.334162	14.758861
20.190263	958.669762	14.763879
19.755481	974.435077	14.768896
19.930178	958.337940	14.773914
20.094242	960.944138	14.778931
19.805386	967.152714	14.783949
20.155881	959.757164	14.788967
19.769864	961.120927	14.793984
19.975174	960.302860	14.799002
20.061265	955.801641	14.804019
19.808743	957.087683	14.809037
20.139421	967.099842	14.814055
20.438409	978.306734	14.819072
20.360437	972.837117	14.824090
20.025953	971.144239	14.829107
20.159591	975.834923	14.834125
20.213726	973.702452	14.839143
20.297041	984.368772	14.844160
20.319673	983.696092	14.849178
20.184502	987.911333	14.854195
20.276258	985.542588	14.859213
20.676848	988.013899	14.864231
20.547735	984.600452	14.869248
20.695058	978.375996	14.874266
20.427507	981.507422	14.879283
20.607599	984.325711	14.884301
20.196469	980.568278	14.889319
20.235026	982.023315	14.894336
20.353815	988.417343	14.899354
20.452324	981.518866	14.904371
20.482398	984.553168	14.909389
20.597379	986.595847	14.914407
20.373816	987.018957	14.919424
20.512897	991.080774	14.924442
20.388905	983.409254	14.929459
20.416916	984.159029	14.934477
20.284045	988.260299	14.939495
20.552812	1009.050017	14.944512
20.894056	1013.960654	14.949530
20.820675	1015.335400	14.954547
20.731209	1020.458692	14.959565
20.981010	1003.317776	14.964583
20.856932	1011.630765	14.969600
20.812330	1008.229319	14.974618
20.867893	1000.889429	14.979635
20.939798	1004.674590	14.984653
21.241957	1003.345874	14.989671
20.833729	1009.166060	14.994688
20.897500	1005.709764	14.999706
21.297032	996.409835	15.004723
20.880110	1001.451880	15.009741
21.127459	1006.954751	15.014759
21.274884	1001.809580	15.019776
21.251839	999.531405	15.024794
21.043398	979.110772	15.029811
21.105961	980.423189	15.034829
21.004510	977.459854	15.039847
21.236160	995.979991	15.044864
21.198898	995.850037	15.049882
20.856018	1000.050487	15.054899
20.969391	1004.668613	15.059917
21.308670	1002.185343	15.064935
21.025802	1010.305455	15.069952
21.043647	1005.956930	15.074970
21.147567	1005.120032	15.079987
20.801248	1000.598186	15.085005
21.128669	998.321907	15.090023
21.236026	1001.722807	15.095040
21.170990	1004.143995	15.100058
20.877752	1007.361503	15.105075
21.284660	1023.484148	15.110093
21.354644	1018.287988	15.115111
21.640603	1026.066515	15.120128
21.638878	1030.513328	15.125146
21.674169	1027.815745	15.130163
21.684923	1021.196096	15.135181
21.626671	1020.091109	15.140199
21.615276	1016.738108	15.145216
21.462176	1004.665537	15.150234
21.535013	1009.151157	15.155251
21.705275	1022.016144	15.160269
21.683246	1016.635581	15.165287
21.846406	1021.694045	15.170304
21.714947	1022.970592	15.175322
21.737180	1003.220706	15.180339
21.311532	1000.712113	15.185357
21.673977	1013.657439	15.190375
22.036534	1017.617976	15.195392
21.776674	1023.743131	15.200410
22.088384	1022.334021	15.205427
21.569911	1010.577473	15.210445
21.600900	1013.706313	15.215463
21.517502	1017.591550	15.220480
21.541690	1014.447574	15.225498
21.785369	1018.101681	15.230515
21.933378	1017.986881	15.235533
21.768775	1017.166807	15.240551
21.821981	1025.224802	15.245568
21.781584	1022.816796	15.250586
22.043548	1016.400792	15.255603
21.692348	1029.757751	15.260621
21.745159	1020.442704	15.265639
22.110057	1029.979311	15.270656
22.177021	1042.791069	15.275674
22.504095	1036.513183	15.280691
21.984577	1018.511309	15.285709
22.283482	1014.503763	15.290727
22.207135	1024.374595	15.295744
22.178457	1018.616367	15.300762
22.346124	1011.454573	15.305779
22.097415	1018.568924	15.310797
22.473219	1018.689839	15.315815
22.241715	1018.536669	15.320832
22.386318	1018.823200	15.325850
22.393220	1016.486680	15.330867
22.233913	1024.521166	15.335885
22.279940	1017.873900	15.340903
22.757264	1041.480737	15.345920
22.827997	1029.445665	15.350938
22.555425	1021.671172	15.355955
22.236772	1017.372210	15.360973
22.510995	1017.853032	15.365991
22.398366	1010.103979	15.371008
22.154314	1017.949763	15.376026
22.917645	1035.850140	15.381043
22.653071	1049.477570	15.386061
22.604536	1035.349896	15.391079
22.548274	1031.975519	15.396096
22.325504	1039.997864	15.401114
22.946601	1036.987585	15.406131
22.457267	1037.897316	15.411149
22.813380	1031.883131	15.416167
22.897799	1035.429647	15.421184
22.691635	1035.455547	15.426202
22.884280	1039.884533	15.431219
22.853204	1034.435952	15.436237
23.076799	1039.153586	15.441255
23.209921	1042.528366	15.446272
22.738198	1024.670480	15.451290
23.028828	1021.188105	15.456307
22.890020	1037.374173	15.461325
22.980034	1038.066897	15.466343
23.126831	1034.821655	15.471360
23.284106	1030.495461	15.476378
23.258661	1019.125576	15.481395
22.661287	1015.788644	15.486413
23.042524	1009.959883	15.491431
23.049070	1004.275038	15.496448
22.602454	1009.930821	15.501466
22.926743	1023.756310	15.506483
23.032234	1034.526485	15.511501
22.799493	1030.646415	15.516519
23.049674	1030.701805	15.521536
22.913876	1030.183337	15.526554
22.939833	1039.956095	15.531571
22.742065	1038.576313	15.536589
22.955692	1034.165548	15.541607
22.959141	1046.428669	15.546624
23.052741	1051.703173	15.551642
23.307412	1053.891235	15.556659
23.356506	1064.405170	15.561677
23.168934	1057.163312	15.566695
23.273204	1060.116573	15.571712
23.473323	1059.002661	15.576730
23.797519	1054.211641	15.581747
23.340664	1070.084643	15.586765
23.409356	1058.927206	15.591783
23.692940	1055.647905	15.596800
23.405294	1058.145005	15.601818
23.784801	1047.232375	15.606835
23.459879	1049.056800	15.611853
23.557600	1053.781535	15.616871
23.438545	1054.181960	15.621888
23.346713	1059.545481	15.626906
23.214141	1058.559436	15.631923
23.244147	1069.423511	15.636941
23.937334	1072.259257	15.641959
24.309134	1080.182152	15.646976
23.750031	1066.115512	15.651994
23.798664	1063.661993	15.657011
23.837031	1053.957862	15.662029
23.933537	1056.199108	15.667047
24.049457	1054.445121	15.672064
23.812639	1064.486287	15.677082
24.008087	1061.602656	15.682099
23.635293	1065.356516	15.687117
24.009879	1077.962307	15.692135
24.260172	1076.515477	15.697152
23.887226	1081.212974	15.702170
24.207234	1078.174122	15.707187
24.371948	1079.060277	15.712205
23.829405	1064.782755	15.717223
24.062027	1066.194770	15.722240
23.834209	1077.042439	15.727258
24.200719	1081.867084	15.732275
24.163206	1080.743064	15.737293
24.237486	1072.087363	15.742311
24.306051	1075.715268	15.747328
24.118965	1078.398592	15.752346
24.348362	1074.935268	15.757363
24.134287	1077.102099	15.762381
24.358147	1086.635587	15.767399
24.255475	1080.339808	15.772416
24.333408	1079.551160	15.777434
24.711793	1081.356916	15.782451
24.768232	1073.975832	15.787469
24.363985	1076.308161	15.792487
24.939096	1073.175690	15.797504
24.449793	1078.715104	15.802522
24.701403	1069.078542	15.807539
24.819921	1064.054650	15.812557
24.304780	1063.570369	15.817575
24.643172	1066.291284	15.822592
24.577328	1075.882780	15.827610
24.844070	1066.114458	15.832627
24.825591	1075.218838	15.837645
24.519933	1068.430990	15.842663
24.794111	1055.332050	15.847680
24.888407	1061.351236	15.852698
24.329591	1053.760436	15.857715
24.436180	1071.523899	15.862733
24.677282	1066.234641	15.867751
24.520298	1062.781363	15.872768
24.530959	1084.340617	15.877786
24.802587	1079.974404	15.882803
24.623730	1075.388431	15.887821
24.683002	1078.796880	15.892839
24.885225	1076.256177	15.897856
24.070274	1082.149578	15.902874
24.737352	1086.990249	15.907891
25.028370	1090.217221	15.912909
24.844459	1094.670503	15.917927
25.147239	1088.693059	15.922944
24.911733	1095.038491	15.927962
25.033757	1100.311712	15.932979
24.939929	1104.536282	15.937997
25.077842	1103.463673	15.943015
25.076807	1095.416224	15.948032
25.203160	1103.784696	15.953050
25.040423	1093.884828	15.958067
25.377583	1094.586171	15.963085
25.417389	1095.040605	15.968103
25.415231	1086.889191	15.973120
25.274650	1086.103220	15.978138
25.236104	1082.555640	15.983155
25.198718	1087.588738	15.988173
25.132590	1091.120982	15.993191
25.781509	1101.727157	15.998208
25.356184	1097.911961	16.003226
25.043567	1092.217132	16.008243
25.375948	1108.247386	16.013261
25.598078	1122.953673	16.018279
26.141354	1113.189338	16.023296
25.836714	1110.986827	16.028314
25.233659	1103.178868	16.033331
25.536637	1115.612864	16.038349
25.579111	1113.510607	16.043367
25.555057	1111.112652	16.048384
25.747520	1110.141952	16.053402
25.609856	1109.718450	16.058419
26.065643	1113.159458	16.063437
25.980020	1109.306815	16.068455
26.215586	1103.769098	16.073472
26.014672	1107.603337	16.078490
25.898784	1105.087224	16.083507
25.969499	1093.730627	16.088525
25.773836	1103.733809	16.093543
26.011368	1110.718364	16.098560
25.923988	1109.526414	16.103578
26.103041	1107.380667	16.108595
25.969397	1102.976956	16.113613
25.812589	1113.059264	16.118631
26.063956	1096.432424	16.123648
25.647321	1107.079315	16.128666
25.852722	1109.082595	16.133683
25.671090	1110.900354	16.138701
25.954756	1114.516657	16.143719
26.068676	1103.301612	16.148736
25.959862	1103.091347	16.153754
26.116971	1115.343064	16.158771
26.398043	1116.242550	16.163789
26.579516	1125.287225	16.168807
26.484302	1123.092927	16.173824
26.048593	1109.483459	16.178842
26.301171	1119.713074	16.183859
26.575233	1114.970919	16.188877
26.391606	1125.691771	16.193895
26.470610	1132.164669	16.198912
26.338927	1130.891294	16.203930
26.699113	1134.268387	16.208947
26.816972	1124.580167	16.213965
26.153707	1119.435743	16.218983
26.434828	1123.869823	16.224000
26.312762	1130.289015	16.229018
26.670723	1130.636796	16.234035
26.799935	1121.536951	16.239053
26.446413	1130.116324	16.244071
26.500675	1129.227238	16.249088
26.679648	1128.952947	16.254106
26.405045	1133.991666	16.259123
26.811275	1131.406368	16.264141
26.836443	1135.066332	16.269159
26.677310	1131.417711	16.274176
26.773787	1127.520754	16.279194
26.583025	1133.063903	16.284211
26.769234	1132.422395	16.289229
26.263963	1126.934470	16.294247
26.876122	1140.329928	16.299264
26.855196	1147.702140	16.304282
26.692465	1143.344004	16.309299
27.396704	1152.524544	16.314317
27.436951	1153.808912	16.319335
27.791852	1152.159488	16.324352
27.390763	1149.015846	16.329370
27.336452	1143.447793	16.334387
27.271035	1129.316377	16.339405
27.097468	1132.310024	16.344423
27.222121	1132.113674	16.349440
26.819275	1131.845332	16.354458
26.865298	1148.930376	16.359475
27.098635	1148.278327	16.364493
27.399577	1147.479983	16.369511
27.578552	1150.838133	16.374528
27.365459	1151.246982	16.379546
27.070212	1145.852381	16.384563
27.834838	1152.015888	16.389581
27.361208	1155.684576	16.394599
27.675068	1142.087035	16.399616
27.358039	1142.644717	16.404634
27.501467	1138.024012	16.409651
27.537535	1145.529310	16.414669
27.432888	1145.318392	16.419687
27.595557	1144.743689	16.424704
27.424720	1144.839796	16.429722
27.483109	1148.308359	16.434739
27.697590	1149.038393	16.439757
27.617122	1152.828524	16.444775
27.910125	1164.702366	16.449792
28.226060	1167.474154	16.454810
27.849116	1155.146209	16.459827
27.988632	1155.787000	16.464845
27.887955	1143.573573	16.469863
27.849702	1146.706973	16.474880
27.921927	1157.548708	16.479898
27.601358	1163.689734	16.484915
27.961037	1164.453826	16.489933
27.746218	1173.443847	16.494951
27.777428	1166.514816	16.499968
28.222945	1164.860661	16.504986
27.983061	1171.194183	16.510003
28.299444	1169.863227	16.515021
27.812259	1172.644077	16.520039
28.022689	1171.863069	16.525056
27.980374	1170.294814	16.530074
28.036943	1169.282284	16.535091
28.300136	1164.485013	16.540109
28.228607	1170.271433	16.545127
28.240717	1170.342032	16.550144
28.277465	1164.945903	16.555162
28.158781	1170.581916	16.560179
28.488555	1183.074879	16.565197
28.249097	1180.432943	16.570215
28.654510	1192.099838	16.575232
29.011425	1188.992066	16.580250
28.378973	1179.052131	16.585267
28.544207	1173.134080	16.590285
28.514046	1174.615680	16.595303
28.492640	1176.323132	16.600320
28.852640	1181.363426	16.605338
28.472760	1181.744757	16.610355
28.920122	1183.028460	16.615373
28.673625	1180.147778	16.620391
28.792168	1173.366013	16.625408
28.762786	1179.272068	16.630426
28.898011	1190.419543	16.635443
29.115472	1179.850969	16.640461
28.829913	1173.454419	16.645479
28.658587	1176.450878	16.650496
29.033524	1178.973575	16.655514
28.925036	1191.358478	16.660531
29.108146	1179.608665	16.665549
29.208699	1181.028758	16.670567
29.065761	1180.675511	16.675584
28.840311	1161.342965	16.680602
29.052110	1181.974548	16.685619
29.012330	1179.825208	16.690637
29.010421	1188.059176	16.695655
29.004140	1183.237846	16.700672
29.254777	1187.528391	16.705690
29.145901	1182.950361	16.710707
29.323873	1182.332233	16.715725
29.160086	1180.293843	16.720743
29.157096	1180.859129	16.725760
29.581821	1179.337623	16.730778
29.233564	1192.763672	16.735795
29.281710	1186.157038	16.740813
29.544509	1180.441456	16.745831
29.017214	1185.860618	16.750848
29.205764	1179.901041	16.755866
29.180846	1182.221290	16.760883
29.405384	1190.839515	16.765901
29.553585	1202.534093	16.770919
29.658878	1210.287356	16.775936
29.670420	1207.861719	16.780954
29.582483	1211.839231	16.785971
29.887982	1199.158171	16.790989
29.595129	1202.432460	16.796007
29.606894	1204.475556	16.801024
29.779264	1203.949827	16.806042
29.622448	1210.835255	16.811059
29.554362	1199.475091	16.816077
29.567454	1211.045671	16.821095
29.793023	1204.565872	16.826112
30.226553	1199.969129	16.831130
29.607983	1209.271743	16.836147
29.767356	1199.479144	16.841165
29.830598	1200.507440	16.846183
29.961346	1220.608950	16.851200
30.478596	1213.341809	16.856218
29.982133	1212.870376	16.861235
30.264481	1206.741454	16.866253
30.083696	1200.871295	16.871271
29.881340	1209.291317	16.876288
30.065178	1209.552769	16.881306
30.090513	1221.642162	16.886323
30.573089	1221.960953	16.891341
30.445343	1222.637309	16.896359
30.197981	1226.611399	16.901376
30.629396	1226.884555	16.906394
30.464879	1227.374161	16.911411
30.653042	1227.533946	16.916429
30.784295	1219.699252	16.921447
30.496690	1219.100418	16.926464
30.437405	1204.456724	16.931482
30.378055	1207.252601	16.936499
30.645662	1209.662726	16.941517
30.658424	1216.979195	16.946535
30.377808	1227.191422	16.951552
30.762429	1222.106858	16.956570
30.668831	1224.371599	16.961587
31.089089	1224.523423	16.966605
31.076077	1218.204080	16.971623
30.737205	1209.436312	16.976640
30.789208	1206.871788	16.981658
30.909909	1203.043605	16.986675
30.913849	1201.288213	16.991693
30.838953	1203.976069	16.996711
30.841636	1210.505137	17.001728
31.085214	1223.787987	17.006746
30.631109	1230.066727	17.011763
30.963206	1229.800004	17.016781
31.064203	1229.904015	17.021799
30.973831	1219.304750	17.026816
31.237921	1222.125696	17.031834
30.865405	1219.523537	17.036851
31.067145	1219.671727	17.041869
31.130505	1215.764160	17.046887
31.196089	1221.513334	17.051904
31.115290	1225.533913	17.056922
31.078589	1216.157047	17.061939
30.983709	1216.496882	17.066957
30.790796	1215.431916	17.071975
30.898411	1241.624829	17.076992
31.674761	1235.055568	17.082010
31.046107	1249.557575	17.087027
31.408791	1241.547752	17.092045
31.674256	1241.619683	17.097063
31.348756	1247.565844	17.102080
31.931025	1240.632500	17.107098
31.312746	1239.299651	17.112115
31.303455	1234.513494	17.117133
31.331430	1238.330835	17.122151
31.646315	1256.891853	17.127168
32.023703	1268.414860	17.132186
31.588853	1274.646416	17.137203
31.952938	1271.742642	17.142221
32.229350	1266.378363	17.147239
32.006458	1251.324747	17.152256
31.806950	1244.002629	17.157274
32.154493	1235.928906	17.162291
31.798934	1240.655279	17.167309
32.057289	1238.919985	17.172327
31.984992	1240.468154	17.177344
32.109070	1243.352067	17.182362
31.919775	1255.140584	17.187379
31.852721	1256.460706	17.192397
32.158798	1263.573442	17.197415
32.084024	1267.511033	17.202432
32.421897	1262.537928	17.207450
32.263138	1258.557850	17.212467
32.236455	1254.790619	17.217485
32.579253	1259.843098	17.222503
32.329294	1262.593106	17.227520
32.505811	1260.403556	17.232538
32.491768	1257.429635	17.237555
32.272614	1254.775039	17.242573
32.343490	1262.764100	17.247591
32.463416	1270.960082	17.252608
32.484715	1253.507576	17.257626
32.242569	1262.217890	17.262643
32.403623	1250.774454	17.267661
32.118933	1259.087475	17.272679
32.238123	1262.770604	17.277696
32.424413	1254.712670	17.282714
32.513726	1269.638711	17.287731
32.900069	1279.926358	17.292749
32.784142	1279.616216	17.297767
32.818129	1290.429307	17.302784
32.821044	1278.758156	17.307802
33.014979	1285.329873	17.312819
33.258526	1284.363784	17.317837
32.885275	1275.743387	17.322855
32.918963	1284.375780	17.327872
33.128361	1285.242321	17.332890
33.136076	1281.920991	17.337907
32.874929	1281.185460	17.342925
33.137169	1273.393339	17.347943
32.963202	1287.006754	17.352960
33.042980	1278.902378	17.357978
33.066720	1277.513119	17.362995
33.171301	1279.428069	17.368013
33.145170	1266.647436	17.373031
32.959825	1281.433475	17.378048
33.152528	1267.602348	17.383066
33.589077	1274.719894	17.388083
33.511071	1284.051466	17.393101
33.200187	1274.651253	17.398119
33.064624	1280.485612	17.403136
33.646644	1287.741324	17.408154
33.889952	1302.640108	17.413171
33.301103	1278.977633	17.418189
33.315606	1291.573719	17.423207
33.511071	1297.012223	17.428224
33.609413	1298.369553	17.433242
33.774140	1293.688665	17.438259
33.851428	1304.242507	17.443277
33.909260	1297.287163	17.448295
33.677526	1300.340446	17.453312
33.610104	1297.693630	17.458330
33.606019	1303.015073	17.463347
33.598883	1287.507884	17.468365
33.750488	1295.607392	17.473383
33.982273	1303.205173	17.478400
34.237407	1302.789555	17.483418
34.010446	1301.212346	17.488435
33.823990	1296.204612	17.493453
34.267131	1288.220034	17.498471
34.134647	1302.855792	17.503488
33.870107	1300.568076	17.508506
34.071068	1305.273547	17.513523
33.682513	1317.213249	17.518541
34.278134	1316.075227	17.523559
34.252827	1322.378338	17.528576
34.561205	1323.614397	17.533594
34.598299	1319.026086	17.538611
34.516346	1323.428735	17.543629
34.691127	1311.250934	17.548647
34.657482	1317.773109	17.553664
34.384456	1321.344125	17.558682
34.562816	1317.822477	17.563699
34.227320	1315.539564	17.568717
34.635151	1313.847118	17.573735
34.686814	1318.803211	17.578752
34.809656	1322.025015	17.583770
34.574059	1314.424489	17.588787
34.424322	1314.839195	17.593805
34.855160	1310.302809	17.598823
34.463105	1317.698524	17.603840
34.760544	1320.725708	17.608858
34.726771	1319.168725	17.613875
34.434960	1316.282497	17.618893
34.678290	1307.846358	17.623911
35.105693	1336.469866	17.628928
34.916930	1348.895859	17.633946
35.214315	1340.918314	17.638963
35.285323	1343.087850	17.643981
35.318141	1344.701613	17.648999
35.075655	1329.505828	17.654016
35.089813	1332.318611	17.659034
35.616786	1336.411256	17.664051
35.331007	1328.297857	17.669069
35.302508	1318.758700	17.674087
35.052413	1318.138205	17.679104
35.310793	1328.543763	17.684122
35.308267	1330.746910	17.689139
35.222890	1336.866926	17.694157
35.597600	1333.671131	17.699175
35.360041	1335.977377	17.704192
35.279152	1335.472388	17.709210
35.369330	1324.093661	17.714227
35.173609	1335.476122	17.719245
35.748933	1327.070013	17.724263
35.489729	1338.257286	17.729280
35.291080	1342.886515	17.734298
35.994936	1345.417666	17.739315
35.693807	1359.240414	17.744333
35.905827	1357.433470	17.749351
35.785201	1359.677215	17.754368
36.146401	1364.057782	17.759386
36.467785	1348.691581	17.764403
35.954372	1348.320633	17.769421
35.972321	1332.866281	17.774439
35.957841	1336.109603	17.779456
35.914311	1348.295082	17.784474
36.109693	1348.561039	17.789491
36.450443	1363.280499	17.794509
36.868074	1356.316099	17.799527
36.504257	1335.439699	17.804544
36.116390	1331.886836	17.809562
35.909336	1337.082292	17.814579
36.089071	1326.112427	17.819597
36.163868	1345.711584	17.824615
36.299104	1355.991279	17.829632
36.383226	1355.870708	17.834650
36.600061	1348.066733	17.839667
36.237544	1350.237918	17.844685
36.556730	1359.785021	17.849703
36.575494	1351.036893	17.854720
36.461110	1356.823775	17.859738
36.233127	1354.293629	17.864755
36.141697	1353.285342	17.869773
36.342947	1352.502609	17.874791
36.685788	1366.031956	17.879808
36.707957	1381.249488	17.884826
36.691768	1380.642839	17.889843
36.694342	1384.397915	17.894861
37.004086	1377.781784	17.899879
37.111732	1382.760683	17.904896
36.966803	1374.195988	17.909914
37.185009	1369.210043	17.914931
37.098496	1383.797637	17.919949
37.171372	1372.402655	17.924967
37.166914	1375.903200	17.929984
37.092954	1379.278931	17.935002
37.376401	1370.972183	17.940019
37.043861	1379.008721	17.945037
37.034191	1373.058044	17.950055
36.781004	1372.848304	17.955072
37.198257	1379.252518	17.960090
36.913810	1376.803802	17.965107
36.903086	1369.328973	17.970125
36.804492	1380.510044	17.975143
37.239017	1394.043984	17.980160
36.916838	1395.893260	17.985178
37.458310	1393.864274	17.990195
37.419469	1393.466309	17.995213
37.251220	1395.424018	18.000231
37.950652	1403.185268	18.005248
37.631497	1408.385684	18.010266
37.901588	1408.627313	18.015283
37.659324	1407.087208	18.020301
38.117661	1406.769145	18.025319
38.071671	1396.519443	18.030336
37.877083	1397.080039	18.035354
37.954105	1384.447269	18.040371
37.639288	1400.421390	18.045389
37.851977	1403.477647	18.050407
38.533024	1407.192703	18.055424
38.172132	1420.425233	18.060442
38.459201	1405.733420	18.065459
38.140668	1394.301913	18.070477
38.060293	1393.194057	18.075495
38.377958	1382.066842	18.080512
38.210204	1396.708203	18.085530
38.460107	1406.124169	18.090547
38.225035	1404.090610	18.095565
38.224500	1406.369196	18.100583
38.252775	1411.512024	18.105600
38.497073	1414.828430	18.110618
38.593030	1407.068615	18.115635
38.519088	1407.626089	18.120653
38.344081	1405.144443	18.125671
38.838437	1402.251798	18.130688
38.688116	1409.382448	18.135706
38.654146	1413.989050	18.140723
38.600774	1411.450474	18.145741
38.782392	1404.627179	18.150759
38.419682	1401.830944	18.155776
38.215836	1408.086315	18.160794
38.524267	1408.375589	18.165811
38.467795	1423.362470	18.170829
38.896823	1432.725137	18.175847
38.827824	1427.885165	18.180864
38.883629	1434.390211	18.185882
38.723293	1435.693403	18.190899
38.787973	1436.629965	18.195917
38.658886	1438.054498	18.200935
39.569712	1441.717781	18.205952
39.328982	1443.516429	18.210970
39.313795	1430.860202	18.215987
39.140106	1425.525368	18.221005
39.359795	1439.806247	18.226023
39.474850	1445.143781	18.231040
39.397971	1456.491919	18.236058
39.830298	1446.435503	18.241075
39.554846	1432.403030	18.246093
39.392791	1431.371087	18.251111
39.624382	1429.112925	18.256128
39.562126	1436.434925	18.261146
39.754353	1441.309066	18.266163
39.797093	1448.725079	18.271181
39.550566	1440.529736	18.276199
39.893791	1439.412317	18.281216
40.046359	1445.810685	18.286234
39.984613	1421.121806	18.291251
39.931944	1434.059891	18.296269
39.973066	1429.751800	18.301287
40.010864	1421.193168	18.306304
39.953645	1427.842159	18.311322
40.051923	1422.496275	18.316339
39.808885	1431.471910	18.321357
40.125828	1448.297033	18.326375
40.497950	1444.527242	18.331392
40.586096	1442.989017	18.336410
40.472467	1435.293587	18.341427
40.114006	1428.053105	18.346445
40.209019	1415.770960	18.351463
40.229313	1427.047048	18.356480
40.217776	1441.499861	18.361498
40.459015	1430.633910	18.366515
40.342972	1440.375484	18.371533
40.399506	1445.425528	18.376551
40.470059	1445.303926	18.381568
40.650424	1448.043348	18.386586
40.575350	1442.528949	18.391603
40.720095	1449.398781	18.396621
40.631368	1449.179053	18.401639
40.992654	1437.161302	18.406656
40.509636	1436.886579	18.411674
40.827820	1436.697777	18.416691
41.052440	1431.713965	18.421709
40.651038	1453.505491	18.426727
40.478536	1446.863901	18.431744
40.574307	1464.910330	18.436762
40.945460	1468.424632	18.441779
40.960756	1469.605629	18.446797
40.714258	1475.454276	18.451815
41.134665	1460.179768	18.456832
40.773975	1468.722554	18.461850
40.780228	1465.975803	18.466867
40.988500	1477.231939	18.471885
41.680443	1490.381622	18.476903
41.643674	1486.265610	18.481920
41.229292	1490.199650	18.486938
41.451203	1491.064242	18.491955
41.471136	1490.237324	18.496973
41.349969	1494.838672	18.501991
41.869370	1485.898427	18.507008
41.825873	1489.468230	18.512026
41.563205	1487.047646	18.517043
41.777600	1483.924283	18.522061
41.702866	1477.942738	18.527079
42.024974	1471.406690	18.532096
41.818744	1484.558228	18.537114
41.774680	1485.413995	18.542131
41.927795	1482.385444	18.547149
41.877971	1483.649232	18.552167
41.883717	1482.770886	18.557184
41.769737	1485.180871	18.562202
41.630038	1481.323996	18.567219
41.885061	1490.767608	18.572237
41.949294	1488.112761	18.577255
42.202210	1487.025267	18.582272
41.512129	1487.313186	18.587290
41.917897	1510.938169	18.592307
41.778912	1512.705103	18.597325
42.101664	1519.199916	18.602343
42.049906	1514.499237	18.607360
42.091513	1512.214023	18.612378
42.225929	1527.136368	18.617395
42.822600	1523.312444	18.622413
42.933053	1527.599787	18.627431
42.824042	1519.856257	18.632448
42.637106	1517.928758	18.637466
42.329124	1511.668149	18.642483
42.352938	1513.125540	18.647501
42.574948	1521.274083	18.652519
43.030497	1519.075500	18.657536
42.844407	1529.989493	18.662554
42.784696	1519.820768	18.667571
43.005562	1520.000681	18.672589
42.989911	1523.446201	18.677607
43.214119	1516.515201	18.682624
42.920144	1517.290198	18.687642
43.124052	1528.515490	18.692659
42.991283	1516.994836	18.697677
42.931980	1525.458869	18.702695
43.089380	1519.207400	18.707712
43.084882	1524.712019	18.712730
43.335032	1520.822459	18.717747
43.438563	1514.377449	18.722765
43.479316	1531.113372	18.727783
43.757186	1533.124282	18.732800
43.310793	1533.961031	18.737818
43.659002	1536.996079	18.742835
44.023290	1537.579576	18.747853
43.621312	1526.527150	18.752871
43.328314	1522.782651	18.757888
43.373680	1539.268537	18.762906
43.422537	1544.925758	18.767923
43.734378	1535.418373	18.772941
43.592388	1543.406194	18.777959
44.078248	1543.853873	18.782976
43.803194	1541.195369	18.787994
43.868304	1547.045713	18.793011
43.919330	1535.328985	18.798029
43.976731	1540.782884	18.803047
43.847061	1543.151151	18.808064
43.833004	1546.400757	18.813082
44.146532	1553.824883	18.818099
44.170356	1555.904002	18.823117
44.055945	1563.874888	18.828135
44.418378	1561.760320	18.833152
44.703911	1567.898046	18.838170
44.684557	1568.276550	18.843187
44.733928	1564.143868	18.848205
44.504565	1558.369569	18.853223
44.738381	1560.223274	18.858240
44.968846	1563.223122	18.863258
44.786145	1569.276410	18.868275
44.738283	1555.927744	18.873293
44.580661	1562.264294	18.878311
44.847967	1562.111865	18.883328
44.485718	1559.224009	18.888346
44.553813	1559.320554	18.893363
44.794288	1548.284229	18.898381
44.394724	1559.970183	18.903399
44.440938	1561.083223	18.908416
44.740158	1574.256626	18.913434
44.837483	1580.651074	18.918451
45.043861	1579.675014	18.923469
44.763217	1585.841488	18.928487
45.214629	1585.944252	18.933504
45.288257	1580.103539	18.938522
44.882425	1580.599402	18.943539
45.216633	1559.278843	18.948557
45.226085	1581.552137	18.953575
45.103915	1576.613151	18.958592
45.212479	1593.871868	18.963610
45.559156	1604.680343	18.968627
45.824397	1597.758662	18.973645
45.845317	1607.141178	18.978663
45.699301	1605.866858	18.983680
46.092767	1602.604959	18.988698
45.753650	1589.570158	18.993715
45.775788	1576.425115	18.998733
45.709165	1588.200943	19.003751
45.952184	1596.018007	19.008768
46.071566	1594.206618	19.013786
46.276546	1594.534195	19.018803
46.313298	1584.435532	19.023821
46.048467	1579.275887	19.028839
45.741324	1572.822610	19.033856
46.210147	1582.349545	19.038874
46.263400	1600.588975	19.043891
46.275313	1599.346719	19.048909
46.187893	1605.268320	19.053927
46.187523	1598.028472	19.058944
46.424634	1598.852816	19.063962
46.246432	1605.097926	19.068979
46.286565	1596.144347	19.073997
45.997862	1598.761613	19.079015
46.373431	1593.037700	19.084032
46.709060	1593.243816	19.089050
46.301140	1605.391882	19.094067
46.736128	1608.425969	19.099085
46.714505	1618.045543	19.104103
46.836913	1615.952795	19.109120
46.828916	1616.487320	19.114138
47.429466	1629.512562	19.119155
47.334638	1615.199166	19.124173
47.118797	1612.083224	19.129191
46.922760	1595.860553	19.134208
47.123301	1608.913735	19.139226
46.922010	1614.102056	19.144243
47.155099	1610.148875	19.149261
46.907005	1619.601949	19.154279
47.292361	1621.450854	19.159296
47.461538	1610.886435	19.164314
47.231446	1614.684325	19.169331
47.195480	1608.106494	19.174349
47.069224	1613.046360	19.179367
46.878313	1614.786723	19.184384
47.042541	1616.897503	19.189402
47.109388	1634.023932	19.194419
47.464955	1635.820698	19.199437
47.669006	1648.055958	19.204455
47.828699	1649.192253	19.209472
47.888990	1635.618287	19.214490
47.769917	1644.145392	19.219507
47.972272	1634.550961	19.224525
47.789848	1635.557808	19.229543
47.889982	1646.597451	19.234560
48.061213	1637.695899	19.239578
47.790066	1640.461908	19.244595
47.941293	1646.134681	19.249613
48.176964	1663.310431	19.254631
48.098953	1666.229231	19.259648
48.482708	1661.453968	19.264666
48.363228	1661.816601	19.269683
48.317691	1655.571631	19.274701
48.333836	1660.397676	19.279719
48.293684	1661.549501	19.284736
48.474252	1654.066675	19.289754
48.596044	1655.773830	19.294771
48.348664	1655.247576	19.299789
48.315243	1666.447019	19.304807
48.372604	1660.656169	19.309824
48.510918	1667.362981	19.314842
48.552739	1663.799537	19.319859
48.542815	1670.965103	19.324877
48.774259	1679.282664	19.329895
48.552808	1683.962892	19.334912
48.746676	1670.184925	19.339930
48.775877	1681.172582	19.344947
49.126784	1679.473242	19.349965
49.055397	1680.683615	19.354983
49.166004	1684.030485	19.360000
49.302229	1680.382816	19.365018
49.033980	1684.189855	19.370035
49.042229	1677.450427	19.375053
49.313014	1689.160834	19.380071
49.092487	1711.441917	19.385088
49.556553	1703.141433	19.390106
49.572945	1707.689725	19.395123
49.922629	1704.803919	19.400141
49.730341	1705.017004	19.405159
49.691971	1701.961609	19.410176
49.765798	1690.597834	19.415194
49.680132	1695.786999	19.420211
49.682420	1696.910086	19.425229
49.758589	1695.395809	19.430247
49.454162	1704.229710	19.435264
50.029362	1694.876652	19.440282
49.961708	1703.581933	19.445299
49.915962	1694.121021	19.450317
50.017483	1695.976531	19.455335
50.529819	1715.532790	19.460352
50.271599	1708.469004	19.465370
50.195232	1704.463294	19.470387
50.408058	1703.640861	19.475405
50.142572	1710.467762	19.480423
50.228561	1724.365848	19.485440
50.678233	1718.355713	19.490458
50.755121	1717.327346	19.495475
50.567473	1716.807512	19.500493
50.936939	1719.886601	19.505511
50.920285	1727.902207	19.510528
50.548235	1718.517654	19.515546
50.223711	1722.447134	19.520563
50.449895	1719.274543	19.525581
50.649130	1723.406003	19.530599
50.166500	1717.390449	19.535616
50.653347	1727.438533	19.540634
50.709381	1738.409398	19.545651
51.011194	1744.708746	19.550669
51.128264	1743.680393	19.555687
50.969221	1746.864383	19.560704
51.431530	1737.383813	19.565722
51.334592	1739.254641	19.570739
51.385375	1737.431894	19.575757
51.413358	1740.384596	19.580775
51.374347	1740.321186	19.585792
51.681682	1737.072758	19.590810
51.448655	1744.380611	19.595827
51.343816	1740.038505	19.600845
51.619754	1740.380216	19.605863
51.418967	1740.061268	19.610880
51.483852	1737.819719	19.615898
51.788317	1743.304402	19.620915
51.847922	1746.065946	19.625933
51.994948	1754.163224	19.630951
51.652446	1760.913843	19.635968
52.235574	1762.220504	19.640986
51.716785	1764.820189	19.646003
51.644800	1759.958502	19.651021
52.173765	1755.031067	19.656039
51.892333	1753.774796	19.661056
52.194323	1753.310800	19.666074
51.667274	1770.508315	19.671091
52.108304	1763.407541	19.676109
52.281296	1757.406026	19.681127
51.964009	1778.487290	19.686144
52.295311	1776.895161	19.691162
52.385803	1785.635668	19.696179
52.439569	1786.608675	19.701197
52.580274	1773.366012	19.706215
52.445038	1784.076518	19.711232
52.746539	1772.837978	19.716250
52.585999	1775.592989	19.721267
52.550726	1781.304494	19.726285
52.853242	1786.417087	19.731303
53.107708	1800.213091	19.736320
53.505599	1796.893656	19.741338
53.134429	1798.564442	19.746355
53.176286	1795.783659	19.751373
53.265319	1799.323292	19.756391
52.948229	1797.564486	19.761408
53.235185	1792.119499	19.766426
53.442154	1784.424186	19.771443
53.535191	1792.990717	19.776461
54.006319	1787.901911	19.781479
53.526752	1793.481043	19.786496
53.452852	1786.464092	19.791514
53.807426	1783.858392	19.796531
53.510044	1787.139807	19.801549
53.746239	1790.242944	19.806567
53.867108	1792.521496	19.811584
54.027845	1789.229750	19.816602
53.973336	1792.589886	19.821619
53.691786	1794.985138	19.826637
53.822873	1788.368444	19.831655
53.699054	1798.259763	19.836672
53.909684	1791.576953	19.841690
53.977823	1787.744257	19.846707
53.735737	1802.476495	19.851725
54.245314	1810.046750	19.856743
54.085601	1821.190332	19.861760
54.521231	1816.138639	19.866778
54.104426	1819.091608	19.871795
53.986508	1815.897167	19.876813
54.390508	1814.470382	19.881831
54.022370	1809.860222	19.886848
54.488316	1813.211409	19.891866
54.730167	1830.654613	19.896883
54.869004	1839.532749	19.901901
55.040262	1828.879508	19.906919
54.488872	1832.759343	19.911936
54.526615	1828.375940	19.916954
54.407115	1834.757110	19.921971
54.393750	1839.613074	19.926989
54.666022	1838.746606	19.932007
54.965790	1856.628916	19.937024
55.376370	1854.872870	19.942042
55.170459	1858.809044	19.947059
55.268161	1858.689499	19.952077
55.235140	1861.607594	19.957095
55.101713	1866.132057	19.962112
55.283847	1860.444679	19.967130
55.303257	1855.111023	19.972147
54.942886	1864.884795	19.977165
55.447589	1847.368598	19.982183
55.623966	1869.868579	19.987200
55.981084	1872.444665	19.992218
56.075616	1872.682248	19.997235
55.516756	1856.655049	20.002253
55.932908	1874.534923	20.007271
55.855240	1874.196683	20.012288
56.033663	1878.284100	20.017306
55.832112	1881.408496	20.022323
55.913625	1880.966416	20.027341
56.255110	1876.333428	20.032359
56.157687	1877.674134	20.037376
55.861994	1873.721685	20.042394
55.985605	1873.938931	20.047411
55.955923	1870.819025	20.052429
56.543618	1887.384377	20.057447
56.491193	1894.484101	20.062464
56.776241	1900.773508	20.067482
56.660708	1898.149921	20.072499
56.604669	1901.147373	20.077517
56.875744	1900.116976	20.082535
56.911384	1897.804243	20.087552
57.076118	1898.065543	20.092570
57.115760	1903.351909	20.097587
56.975486	1895.490029	20.102605
56.862545	1890.246532	20.107623
56.875675	1895.335063	20.112640
56.826814	1899.151958	20.117658
56.903345	1898.843212	20.122675
56.859820	1899.683134	20.127693
57.318256	1894.987634	20.132711
57.041580	1895.532701	20.137728
56.962094	1892.843503	20.142746
57.515191	1910.856603	20.147763
57.275950	1918.181280	20.152781
57.226105	1922.042519	20.157799
57.810415	1916.105907	20.162816
57.830351	1927.887332	20.167834
57.787101	1920.909710	20.172851
57.812639	1930.250644	20.177869
58.023345	1923.425751	20.182887
57.700245	1921.061916	20.187904
57.787393	1931.579867	20.192922
58.189976	1921.676181	20.197939
57.770069	1927.823562	20.202957
58.100045	1924.628362	20.207975
58.049398	1933.728750	20.212992
57.925359	1939.350063	20.218010
58.145836	1941.840262	20.223027
58.027810	1953.176224	20.228045
58.013052	1945.430368	20.233063
58.100027	1949.667838	20.238080
58.186929	1953.198367	20.243098
58.523424	1961.120876	20.248115
58.749823	1971.004761	20.253133
58.785809	1973.770041	20.258151
59.036835	1981.210451	20.263168
58.879910	1976.295736	20.268186
59.148279	1972.349572	20.273203
59.021495	1971.703421	20.278221
58.999022	1969.554431	20.283239
59.102818	1970.718440	20.288256
59.630904	1974.855245	20.293274
59.135989	1966.644923	20.298291
58.924932	1971.033242	20.303309
59.184070	1968.660236	20.308327
59.400634	1967.436388	20.313344
58.853343	1973.991935	20.318362
59.369081	1962.214745	20.323379
59.053013	1977.842409	20.328397
59.123690	1974.066085	20.333415
59.609191	1986.427908	20.338432
59.852714	1992.203105	20.343450
59.701256	1996.660993	20.348467
59.736880	2000.792903	20.353485
60.141876	1992.482606	20.358503
59.895488	1995.071206	20.363520
59.559141	1993.971856	20.368538
60.013507	1994.863174	20.373555
59.967258	1998.799612	20.378573
59.799709	1990.979836	20.383591
59.785189	2000.923575	20.388608
59.982717	2006.567117	20.393626
60.541935	2007.868075	20.398643
60.082375	2015.293587	20.403661
60.586772	2012.951583	20.408679
60.543327	2008.501956	20.413696
60.539678	2012.949314	20.418714
60.535918	2009.067871	20.423731
60.197080	2017.222453	20.428749
60.542966	2021.119551	20.433767
60.738116	2036.862848	20.438784
60.726534	2045.846711	20.443802
61.277815	2041.010385	20.448819
60.767743	2043.652928	20.453837
61.199228	2048.205705	20.458855
60.963960	2039.238245	20.463872
61.261214	2038.443598	20.468890
61.261685	2038.497088	20.473907
60.953238	2045.289817	20.478925
61.347625	2040.462292	20.483943
61.450620	2035.109175	20.488960
61.152533	2047.256110	20.493978
61.585107	2053.478272	20.498995
61.538794	2063.098797	20.504013
61.654570	2065.741128	20.509031
61.593795	2063.033192	20.514048
61.598868	2072.266943	20.519066
61.895789	2061.451853	20.524083
61.796403	2066.283484	20.529101
61.834277	2062.711112	20.534119
61.954295	2063.708471	20.539136
61.553687	2075.915671	20.544154
62.022226	2082.668740	20.549171
61.997302	2090.979318	20.554189
62.263740	2081.068471	20.559207
62.498342	2079.043306	20.564224
61.899700	2081.197917	20.569242
62.366410	2081.137331	20.574259
62.555856	2096.537563	20.579277
62.623334	2113.484455	20.584295
62.646574	2105.192888	20.589312
62.837522	2109.038534	20.594330
63.145611	2105.818327	20.599347
63.277569	2109.442822	20.604365
63.170774	2107.288090	20.609383
63.086037	2101.844435	20.614400
63.024388	2103.021749	20.619418
63.129543	2098.264772	20.624435
63.218172	2100.696749	20.629453
63.113294	2102.404743	20.634471
63.404399	2104.082259	20.639488
63.385865	2093.411255	20.644506
63.333840	2093.081617	20.649523
63.509658	2095.768199	20.654541
63.422374	2092.852955	20.659559
63.834582	2098.349273	20.664576
63.876492	2098.033323	20.669594
63.591537	2086.902249	20.674611
63.477453	2096.975259	20.679629
63.388282	2089.070571	20.684647
63.604981	2092.075822	20.689664
63.562292	2111.119819	20.694682
63.658065	2113.585395	20.699699
63.628060	2111.535406	20.704717
63.680211	2117.883470	20.709735
64.120074	2127.068067	20.714752
64.093437	2146.497783	20.719770
64.345171	2152.962927	20.724787
64.464322	2143.728429	20.729805
64.617524	2152.961107	20.734823
64.750924	2144.724852	20.739840
64.299594	2146.572344	20.744858
64.515887	2145.474770	20.749875
64.308097	2137.118390	20.754893
64.393382	2141.109997	20.759911
64.623991	2149.853978	20.764928
64.667588	2160.271580	20.769946
65.138363	2160.645896	20.774963
64.863614	2169.926694	20.779981
64.806032	2170.235454	20.784999
65.397545	2164.685830	20.790016
64.931416	2168.340920	20.795034
64.799957	2166.351004	20.800051
65.098536	2177.239952	20.805069
65.120939	2186.013415	20.810087
65.535110	2179.257544	20.815104
65.709816	2180.965928	20.820122
65.650636	2178.055735	20.825139
65.834796	2180.308639	20.830157
65.517906	2178.322526	20.835175
65.788610	2185.968239	20.840192
65.844581	2204.128955	20.845210
66.316752	2204.067514	20.850227
66.168600	2204.040138	20.855245
66.128434	2200.296913	20.860263
66.324647	2200.458604	20.865280
66.325565	2206.461245	20.870298
66.545614	2202.557319	20.875315
66.598407	2196.722826	20.880333
66.439173	2198.764422	20.885351
66.576115	2193.068239	20.890368
66.482618	2194.667152	20.895386
66.623939	2194.105231	20.900403
66.497879	2191.789390	20.905421
66.476637	2197.221093	20.910439
66.835679	2195.776075	20.915456
66.612054	2213.526129	20.920474
66.739061	2218.293926	20.925491
66.863264	2218.410089	20.930509
66.996458	2218.499595	20.935527
67.240825	2227.522351	20.940544
66.648183	2226.624100	20.945562
66.906000	2224.778335	20.950579
67.354650	2248.252394	20.955597
67.223859	2246.846242	20.960615
67.366708	2243.228982	20.965632
67.555626	2251.572409	20.970650
67.390817	2250.657625	20.975667
67.416150	2252.929110	20.980685
67.531260	2255.628384	20.985703
67.977817	2241.182327	20.990720
67.599391	2248.330110	20.995738
68.032269	2263.379893	21.000755
68.251994	2267.823880	21.005773
68.085672	2264.374986	21.010791
68.357402	2276.388615	21.015808
68.209841	2272.397088	21.020826
68.279969	2272.720558	21.025843
68.342356	2273.133611	21.030861
68.407551	2274.344718	21.035879
68.506967	2262.689368	21.040896
68.047231	2270.642079	21.045914
68.001055	2274.001000	21.050931
68.698881	2282.854900	21.055949
68.940168	2294.409364	21.060967
68.953076	2291.819249	21.065984
69.039848	2300.323883	21.071002
68.835983	2295.220756	21.076019
69.277632	2290.382604	21.081037
69.111370	2288.095142	21.086055
69.192575	2292.128451	21.091072
69.146035	2295.358032	21.096090
69.363361	2289.428297	21.101107
69.636384	2278.339085	21.106125
69.382186	2289.254740	21.111143
69.122021	2285.599618	21.116160
69.312231	2296.492992	21.121178
69.292194	2310.202997	21.126195
69.694892	2316.149039	21.131213
69.340122	2314.026820	21.136231
70.029524	2312.590000	21.141248
69.957297	2313.541746	21.146266
69.719952	2312.341649	21.151283
70.222333	2322.419197	21.156301
69.764980	2327.095522	21.161319
70.308812	2326.521033	21.166336
70.310943	2335.654385	21.171354
70.494265	2340.233493	21.176371
70.602722	2329.949591	21.181389
70.557236	2343.897160	21.186407
70.691005	2336.001621	21.191424
70.736274	2334.100774	21.196442
70.583241	2335.276640	21.201459
70.897742	2338.923081	21.206477
70.893057	2332.403205	21.211495
70.465489	2329.875783	21.216512
70.764469	2339.126747	21.221530
70.912192	2358.257950	21.226547
70.962380	2346.733347	21.231565
70.905781	2351.271144	21.236583
70.905305	2353.006991	21.241600
71.404396	2366.465275	21.246618
71.346820	2378.300169	21.251635
71.416197	2380.340685	21.256653
71.355200	2386.192125	21.261671
71.567543	2377.832932	21.266688
71.648845	2383.384338	21.271706
71.269503	2385.081705	21.276723
71.520319	2374.592419	21.281741
71.534059	2394.281191	21.286759
71.847660	2404.647165	21.291776
72.202468	2395.871128	21.296794
72.088129	2410.504945	21.301811
72.380003	2395.069885	21.306829
72.255293	2399.021859	21.311847
72.345128	2400.547881	21.316864
72.552950	2407.218832	21.321882
72.525887	2408.261347	21.326899
72.673904	2403.936275	21.331917
72.572700	2404.056193	21.336935
72.470308	2404.201546	21.341952
72.922533	2419.270523	21.346970
72.982301	2423.001076	21.351987
72.811558	2416.841735	21.357005
73.135786	2426.480148	21.362023
72.965176	2423.902986	21.367040
73.047779	2421.936314	21.372058
72.996969	2417.673951	21.377075
73.294058	2416.393272	21.382093
73.141451	2421.201774	21.387111
73.072662	2416.131104	21.392128
73.418452	2429.884881	21.397146
73.321387	2444.386619	21.402163
73.773145	2444.574554	21.407181
73.662321	2441.489354	21.412199
73.817748	2442.010924	21.417216
73.749141	2443.842669	21.422234
73.394058	2442.544232	21.427251
73.954447	2451.416593	21.432269
74.174776	2458.940915	21.437287
74.214630	2463.170108	21.442304
74.431464	2469.350470	21.447322
74.216687	2472.164583	21.452339
74.686215	2458.835180	21.457357
74.397263	2466.139462	21.462375
74.248217	2465.108576	21.467392
74.633001	2460.519155	21.472410
74.241832	2459.993310	21.477427
74.638135	2463.147228	21.482445
74.901535	2488.632676	21.487463
74.989915	2484.092843	21.492480
75.154455	2482.637246	21.497498
74.817817	2479.713663	21.502515
74.973124	2483.684908	21.507533
74.920222	2492.369322	21.512551
75.231224	2478.231522	21.517568
75.056236	2489.109639	21.522586
75.270340	2498.613849	21.527603
75.931423	2506.618305	21.532621
75.277028	2508.393494	21.537639
75.148003	2502.805161	21.542656
75.581596	2498.930839	21.547674
75.816095	2514.245467	21.552691
75.872940	2495.608945	21.557709
75.873430	2507.595789	21.562727
75.877429	2521.330594	21.567744
75.884786	2520.865399	21.572762
75.950923	2534.091808	21.577779
76.245023	2522.765589	21.582797
76.197229	2526.364677	21.587815
76.289399	2522.155635	21.592832
76.351747	2533.340614	21.597850
76.645840	2545.328826	21.602867
76.938831	2547.126023	21.607885
76.789150	2548.001543	21.612903
76.879741	2550.370151	21.617920
77.382741	2540.437771	21.622938
77.005788	2545.884278	21.627955
76.946659	2542.866710	21.632973
76.793280	2551.352276	21.637991
76.944837	2544.656350	21.643008
77.231018	2542.544150	21.648026
76.945968	2542.465630	21.653043
77.237397	2552.301774	21.658061
77.435093	2570.686835	21.663079
77.492726	2564.153956	21.668096
77.523917	2561.554626	21.673114
77.454981	2562.972979	21.678131
77.820531	2567.791869	21.683149
77.582751	2572.998806	21.688167
77.810556	2561.733448	21.693184
78.193638	2577.877012	21.698202
77.936252	2585.097492	21.703219
78.533710	2583.561437	21.708237
77.836209	2585.599035	21.713255
77.815207	2598.886486	21.718272
78.252438	2584.327995	21.723290
77.801224	2594.858089	21.728307
78.298800	2601.549995	21.733325
78.854225	2611.187003	21.738343
78.655093	2619.897545	21.743360
78.694939	2614.951826	21.748378
79.036318	2612.111366	21.753395
79.277389	2606.382958	21.758413
79.295013	2608.258020	21.763431
78.790339	2613.475222	21.768448
78.837728	2615.033162	21.773466
78.995318	2620.430662	21.778483
79.500130	2622.062121	21.783501
79.584804	2634.985865	21.788519
79.204978	2636.976854	21.793536
79.648845	2631.813180	21.798554
79.396100	2634.238746	21.803571
79.754635	2642.622061	21.808589
79.804826	2640.073397	21.813607
79.933480	2629.808253	21.818624
80.106521	2642.140580	21.823642
79.768300	2661.818507	21.828659
80.004649	2657.839339	21.833677
80.086952	2659.473873	21.838695
80.082917	2660.203490	21.843712
80.160222	2657.297086	21.848730
80.109048	2671.286830	21.853747
80.623297	2684.619889	21.858765
80.814966	2690.267720	21.863783
80.750420	2688.248326	21.868800
80.679363	2690.699089	21.873818
80.881489	2684.626423	21.878835
81.027507	2685.594494	21.883853
81.003213	2686.866991	21.888871
81.010886	2685.344425	21.893888
81.262006	2671.493599	21.898906
80.935209	2694.613151	21.903923
81.093919	2697.987394	21.908941
81.459844	2705.062925	21.913959
81.381619	2713.940784	21.918976
81.226387	2708.170279	21.923994
81.451273	2713.225865	21.929011
81.288324	2728.445136	21.934029
81.875342	2731.136827	21.939047
81.943249	2733.344892	21.944064
82.155977	2722.744593	21.949082
81.982431	2719.609205	21.954099
82.442931	2731.429443	21.959117
82.490982	2735.512232	21.964135
81.999906	2727.411423	21.969152
82.565436	2725.198625	21.974170
82.503740	2732.012920	21.979187
82.853560	2747.148715	21.984205
82.777366	2750.468240	21.989223
82.410671	2748.417272	21.994240
82.805344	2748.238571	21.999258
82.898203	2752.061849	22.004275
82.877037	2759.905032	22.009293
82.938445	2755.233641	22.014311
82.696806	2752.967397	22.019328
83.367040	2750.416261	22.024346
83.155228	2754.123151	22.029363
83.515814	2764.403067	22.034381
83.890898	2764.287402	22.039399
83.648589	2770.413554	22.044416
84.060773	2770.490916	22.049434
83.722601	2766.327146	22.054451
83.572249	2767.038661	22.059469
83.724749	2770.224519	22.064487
83.770065	2775.077855	22.069504
84.062742	2767.476005	22.074522
84.023572	2770.710829	22.079539
83.958269	2767.637379	22.084557
84.403733	2782.174325	22.089575
84.383997	2792.930459	22.094592
83.959547	2792.656000	22.099610
84.163026	2792.220039	22.104627
84.297159	2790.242098	22.109645
84.326890	2806.169796	22.114663
84.524732	2814.442650	22.119680
84.788049	2827.726756	22.124698
84.906790	2820.193166	22.129715
84.792306	2818.642385	22.134733
84.947477	2827.603669	22.139751
85.123000	2837.975744	22.144768
85.382499	2838.162245	22.149786
85.288585	2843.782275	22.154803
85.074117	2846.811018	22.159821
85.332099	2839.555444	22.164839
85.708853	2851.070106	22.169856
85.679024	2859.779488	22.174874
85.738023	2861.850091	22.179891
85.675351	2860.354313	22.184909
86.385432	2861.931543	22.189927
85.868497	2867.690447	22.194944
86.050860	2865.452446	22.199962
86.193254	2864.271722	22.204979
86.359952	2870.277017	22.209997
86.807464	2871.324112	22.215015
86.608403	2880.517667	22.220032
87.092375	2873.207736	22.225050
87.020311	2877.454561	22.230067
87.249201	2872.378156	22.235085
87.132517	2864.322783	22.240103
87.227014	2877.273568	22.245120
87.107555	2876.477893	22.250138
87.541762	2873.783816	22.255155
87.001048	2876.642743	22.260173
87.184315	2868.537219	22.265191
87.362916	2867.413946	22.270208
87.581461	2878.539950	22.275226
87.409383	2861.128803	22.280243
87.651888	2869.227407	22.285261
87.772595	2876.363518	22.290279
87.607042	2882.458746	22.295296
87.695544	2889.016009	22.300314
87.824150	2888.904241	22.305331
87.861428	2891.877770	22.310349
88.126612	2897.160654	22.315367
88.011724	2899.621469	22.320384
88.038936	2916.098838	22.325402
88.607989	2916.495652	22.330419
88.196792	2922.190664	22.335437
88.114337	2919.214562	22.340455
88.217242	2938.438621	22.345472
88.345258	2927.750475	22.350490
88.493446	2949.615514	22.355507
88.672751	2946.872987	22.360525
88.805269	2947.489692	22.365543
88.710264	2959.993636	22.370560
89.184957	2958.637753	22.375578
89.549181	2965.300189	22.380595
89.477704	2963.881531	22.385613
89.847119	2965.079740	22.390631
90.166085	2970.549906	22.395648
89.917970	2969.458762	22.400666
90.306064	2967.292672	22.405683
89.826455	2965.076308	22.410701
90.217005	2962.698367	22.415719
89.710522	2961.215300	22.420736
90.189576	2961.831369	22.425754
89.842509	2961.327004	22.430771
90.023395	2961.409043	22.435789
90.356257	2954.479406	22.440807
90.164044	2975.409911	22.445824
90.544870	2990.559991	22.450842
90.268756	2989.668918	22.455859
90.329126	2989.428967	22.460877
90.609033	2986.437112	22.465895
90.486345	3002.998014	22.470912
90.616308	3009.368921	22.475930
91.167434	3011.643344	22.480947
90.808846	3023.061855	22.485965
91.271551	3020.893538	22.490983
91.509216	3037.827263	22.496000
91.543419	3036.477260	22.501018
91.861162	3035.420553	22.506035
91.614209	3042.690080	22.511053
91.834734	3036.611257	22.516071
91.824515	3038.165635	22.521088
91.991207	3044.833798	22.526106
92.418213	3036.039829	22.531123
92.007809	3039.919921	22.536141
91.964623	3030.659903	22.541159
92.174127	3051.540184	22.546176
92.130698	3061.151321	22.551194
92.638994	3059.307262	22.556211
92.596759	3062.255401	22.561229
92.744449	3064.173258	22.566247
92.558748	3056.684110	22.571264
92.327153	3071.074866	22.576282
92.869014	3076.282894	22.581299
92.842798	3089.735648	22.586317
93.033628	3084.901864	22.591335
92.831408	3085.435298	22.596352
92.918512	3096.077031	22.601370
93.250400	3101.794555	22.606387
93.343837	3110.459497	22.611405
93.456399	3107.383372	22.616423
93.505208	3104.399298	22.621440
93.765055	3123.365405	22.626458
93.970554	3127.676115	22.631475
93.959492	3137.329565	22.636493
94.219938	3131.796800	22.641511
94.366144	3133.692804	22.646528
94.419178	3128.672284	22.651546
94.571376	3123.074418	22.656563
94.445373	3124.239787	22.661581
94.501475	3126.979999	22.666599
94.682777	3128.163504	22.671616
94.770325	3131.293321	22.676634
95.154975	3124.488069	22.681651
94.862380	3123.410196	22.686669
95.021892	3126.487707	22.691687
95.092835	3141.875839	22.696704
94.976650	3149.913984	22.701722
95.183606	3148.319127	22.706739
94.988668	3152.029767	22.711757
95.391371	3146.960773	22.716775
95.587513	3140.699516	22.721792
95.612250	3160.207496	22.726810
95.953596	3164.121339	22.731827
95.773588	3171.961180	22.736845
95.946286	3169.191249	22.741863
96.142654	3168.251394	22.746880
95.926431	3174.764971	22.751898
95.964970	3165.814018	22.756915
95.844791	3178.845996	22.761933
96.498829	3186.548863	22.766951
96.808153	3196.786558	22.771968
96.557293	3196.892052	22.776986
96.437828	3198.447777	22.782003
96.166018	3203.256224	22.787021
96.407821	3203.376065	22.792039
97.033268	3225.292917	22.797056
97.079684	3222.820514	22.802074
97.060198	3215.330509	22.807091
97.040985	3217.981534	22.812109
97.323058	3229.277709	22.817127
97.279181	3239.782233	22.822144
97.075726	3239.570987	22.827162
97.634862	3237.835727	22.832179
97.537627	3242.818835	22.837197
97.723134	3259.543157	22.842215
97.739274	3260.755703	22.847232
98.248012	3257.844736	22.852250
98.306691	3261.632447	22.857267
98.308543	3259.353240	22.862285
98.524003	3253.158357	22.867303
98.621135	3263.631335	22.872320
98.647779	3254.098292	22.877338
98.741803	3261.595394	22.882355
98.886829	3278.471264	22.887373
99.034009	3286.979526	22.892391
99.117612	3279.400749	22.897408
99.193638	3289.116387	22.902426
99.308853	3277.107561	22.907443
99.140325	3279.510548	22.912461
99.591752	3289.037966	22.917479
99.862595	3274.271425	22.922496
99.530925	3277.356476	22.927514
99.363858	3278.550382	22.932531
99.544914	3294.773587	22.937549
99.798807	3299.155664	22.942567
99.913317	3305.873131	22.947584
99.726074	3305.299528	22.952602
99.942823	3304.441692	22.957619
100.175990	3320.773538	22.962637
100.101715	3328.577945	22.967655
100.289265	3320.269546	22.972672
100.077417	3325.933452	22.977690
100.349341	3334.447443	22.982707
100.515907	3349.722925	22.987725
101.053901	3349.458641	22.992743
101.104892	3358.790016	22.997760
100.815720	3351.061296	23.002778
101.017774	3346.456093	23.007795
101.056688	3354.072338	23.012813
101.208503	3368.706265	23.017831
101.443156	3371.380666	23.022848
101.248922	3379.014510	23.027866
101.852479	3367.137432	23.032883
101.775544	3364.652771	23.037901
101.688014	3364.546456	23.042919
101.608973	3362.854354	23.047936
101.797038	3390.290842	23.052954
102.352702	3393.176926	23.057971
102.251370	3393.520967	23.062989
102.098229	3396.360284	23.068007
102.249751	3394.692027	23.073024
102.165986	3404.158163	23.078042
102.421427	3406.946095	23.083059
102.723726	3419.069326	23.088077
102.483365	3412.699610	23.093095
102.896727	3421.835368	23.098112
102.968025	3430.746967	23.103130
103.084826	3434.809675	23.108147
103.172068	3446.467921	23.113165
103.339930	3442.480374	23.118183
103.486917	3443.685058	23.123200
102.998657	3453.145153	23.128218
103.829171	3458.566888	23.133235
103.989265	3462.846917	23.138253
103.532307	3472.128521	23.143271
103.730009	3470.247862	23.148288
103.534462	3476.654150	23.153306
104.036513	3477.740083	23.158323
104.204853	3488.618668	23.163341
104.343184	3490.033028	23.168359
104.404623	3484.670211	23.173376
104.420571	3487.763963	23.178394
104.588185	3502.660654	23.183411
105.023078	3510.432713	23.188429
104.942935	3513.080702	23.193447
105.156887	3512.482113	23.198464
105.192704	3520.521859	23.203482
105.434345	3510.298485	23.208499
105.104480	3511.678883	23.213517
105.557966	3530.372044	23.218535
105.573938	3532.777723	23.223552
105.656467	3539.112060	23.228570
105.788954	3541.739366	23.233587
105.679897	3544.489736	23.238605
105.490294	3537.720639	23.243623
106.246028	3556.110813	23.248640
106.117879	3564.330927	23.253658
106.429236	3560.488157	23.258675
106.537652	3562.513224	23.263693
106.391176	3563.347257	23.268711
106.667136	3567.441874	23.273728
106.844381	3578.259148	23.278746
106.758845	3587.201708	23.283763
107.164828	3589.306411	23.288781
107.353300	3585.795365	23.293799
107.371113	3578.318304	23.298816
107.098906	3586.242208	23.303834
107.225507	3583.754037	23.308851
107.150129	3580.716745	23.313869
107.287780	3600.384264	23.318887
107.714891	3591.662606	23.323904
107.682759	3606.682210	23.328922
107.782916	3598.501004	23.333939
107.788267	3609.963868	23.338957
107.911900	3620.893726	23.343975
108.247016	3615.292302	23.348992
107.908618	3633.301611	23.354010
108.122954	3621.466408	23.359027
108.097214	3636.314593	23.364045
108.110289	3652.425558	23.369063
108.484718	3651.792354	23.374080
108.912483	3653.101411	23.379098
108.394143	3667.960513	23.384115
108.864689	3673.501837	23.389133
108.995611	3674.346074	23.394151
109.428475	3661.182509	23.399168
109.077952	3678.208984	23.404186
109.315903	3697.396912	23.409203
109.989152	3701.192592	23.414221
109.947473	3703.875615	23.419239
110.251547	3701.141835	23.424256
110.040703	3697.507103	23.429274
110.175339	3695.415357	23.434291
110.480108	3693.644156	23.439309
110.136733	3700.218874	23.444327
110.457667	3693.057256	23.449344
110.504914	3700.047385	23.454362
110.802426	3705.306505	23.459379
110.734756	3717.854036	23.464397
110.887980	3719.635374	23.469415
111.045703	3716.056524	23.474432
110.879033	3717.502904	23.479450
110.795590	3715.628390	23.484467
111.055010	3729.724954	23.489485
111.117486	3741.535620	23.494503
111.348893	3746.022333	23.499520
111.237088	3753.192061	23.504538
111.708421	3764.443140	23.509555
111.735370	3772.048809	23.514573
111.609338	3774.318950	23.519591
111.670227	3777.970699	23.524608
111.915561	3786.034553	23.529626
112.204623	3796.654528	23.534643
112.454338	3803.654009	23.539661
112.384630	3813.219160	23.544679
112.548981	3806.220909	23.549696
112.543564	3817.625621	23.554714
112.764655	3815.807546	23.559731
113.016710	3822.831919	23.564749
113.111996	3825.682885	23.569767
112.853881	3821.440041	23.574784
113.483115	3840.383751	23.579802
113.547835	3843.217413	23.584819
114.157887	3840.451458	23.589837
113.797156	3855.428057	23.594855
113.865059	3849.543319	23.599872
114.008461	3852.588758	23.604890
114.155918	3848.806326	23.609907
114.097818	3843.493695	23.614925
113.736470	3852.220773	23.619943
114.365162	3855.578418	23.624960
114.156061	3867.049791	23.629978
114.447388	3875.283237	23.634995
114.595619	3874.230946	23.640013
114.633900	3889.533296	23.645031
114.741242	3897.565160	23.650048
114.935736	3896.136323	23.655066
115.259768	3900.113012	23.660083
115.548957	3895.307793	23.665101
115.409184	3900.253556	23.670119
115.455920	3912.758047	23.675136
115.552206	3924.086921	23.680154
115.611838	3924.270028	23.685171
115.940305	3923.012740	23.690189
115.955724	3929.518704	23.695207
116.087232	3918.725266	23.700224
115.937720	3921.980739	23.705242
115.987572	3935.523208	23.710259
116.598345	3948.008798	23.715277
116.427839	3946.640296	23.720295
116.190645	3943.094865	23.725312
116.379352	3948.326914	23.730330
116.651425	3950.389512	23.735347
117.229653	3955.487941	23.740365
117.110868	3962.071756	23.745383
117.143100	3969.162189	23.750400
117.328623	3970.073640	23.755418
117.189364	3972.705706	23.760435
117.344787	3973.950138	23.765453
117.484688	3986.780974	23.770471
117.942126	3987.368907	23.775488
117.704526	3989.549235	23.780506
117.644763	3983.709705	23.785523
117.636350	3992.981272	23.790541
117.887694	4014.484235	23.795559
117.891251	4015.209561	23.800576
118.183351	4031.744296	23.805594
118.482288	4044.657576	23.810611
118.653624	4035.672763	23.815629
118.476348	4042.922304	23.820647
118.783034	4051.241803	23.825664
119.006327	4063.210555	23.830682
118.649648	4062.152133	23.835699
119.304709	4064.120023	23.840717
119.288185	4085.977521	23.845735
119.582258	4084.675107	23.850752
119.993400	4083.786782	23.855770
119.811974	4081.375208	23.860787
120.090902	4083.850238	23.865805
119.526735	4089.383349	23.870823
120.017307	4101.540672	23.875840
120.170829	4105.307388	23.880858
120.244598	4106.940235	23.885875
120.749817	4109.477665	23.890893
120.821292	4125.317918	23.895911
120.936591	4136.044225	23.900928
121.219562	4138.348183	23.905946
121.250020	4136.373714	23.910963
121.493653	4140.167353	23.915981
121.022746	4137.491794	23.920999
121.491788	4132.421605	23.926016
121.236918	4132.998037	23.931034
121.506808	4153.980606	23.936051
121.227398	4150.612195	23.941069
121.686207	4163.655178	23.946087
121.887314	4165.479561	23.951104
121.751482	4174.935318	23.956122
121.922906	4186.306243	23.961139
122.047410	4190.598335	23.966157
122.418183	4204.816707	23.971175
122.436038	4206.881285	23.976192
122.620745	4210.289617	23.981210
122.840754	4212.369872	23.986227
122.994246	4210.429779	23.991245
122.748935	4225.454885	23.996263
123.267629	4228.637291	24.001280
123.231648	4236.597067	24.006298
123.578037	4239.932727	24.011315
123.739559	4239.253950	24.016333
123.354678	4250.109189	24.021351
123.963125	4256.815912	24.026368
123.837715	4253.549612	24.031386
123.928437	4266.394665	24.036403
124.025275	4262.089795	24.041421
124.265046	4265.915631	24.046439
124.465361	4274.674862	24.051456
124.796179	4276.444215	24.056474
124.615576	4285.635588	24.061491
124.957429	4274.101941	24.066509
124.750989	4284.077004	24.071527
124.626180	4282.385673	24.076544
125.309608	4285.820050	24.081562
125.490670	4302.511312	24.086579
125.556585	4300.824820	24.091597
125.407737	4319.628946	24.096615
125.427913	4305.077602	24.101632
125.588918	4305.222737	24.106650
125.585893	4329.161671	24.111667
126.346033	4322.865310	24.116685
126.056279	4336.748521	24.121703
125.923126	4335.708722	24.126720
126.294283	4335.918784	24.131738
126.154172	4354.352272	24.136755
126.611729	4360.303027	24.141773
126.356505	4361.788582	24.146791
126.529847	4369.119051	24.151808
126.746141	4373.507281	24.156826
126.874358	4372.088791	24.161843
127.307812	4384.981240	24.166861
127.111426	4402.640790	24.171879
127.213070	4392.574581	24.176896
127.347490	4414.673970	24.181914
127.696905	4416.677159	24.186931
127.654543	4427.775551	24.191949
127.705597	4434.430780	24.196967
127.790103	4445.171564	24.201984
128.449409	4441.491897	24.207002
127.927966	4453.899542	24.212019
128.230713	4454.732680	24.217037
128.484356	4468.032135	24.222055
128.650121	4472.987003	24.227072
129.167263	4461.558349	24.232090
128.899936	4480.185501	24.237107
129.206241	4491.226151	24.242125
129.381381	4496.034358	24.247143
129.591508	4505.707544	24.252160
129.299747	4506.277141	24.257178
129.663224	4523.356684	24.262195
130.097980	4525.318107	24.267213
129.820384	4533.050720	24.272231
130.118142	4530.182078	24.277248
130.296720	4527.903434	24.282266
130.223526	4560.249933	24.287283
130.377093	4555.178548	24.292301
130.798960	4553.414172	24.297319
130.773151	4551.290649	24.302336
131.247232	4555.862649	24.307354
131.255986	4566.722693	24.312371
131.315158	4576.173359	24.317389
131.704228	4581.633035	24.322407
131.313944	4579.954858	24.327424
131.435717	4574.111949	24.332442
131.712315	4580.855001	24.337459
131.927843	4594.911768	24.342477
131.958779	4597.331026	24.347495
132.055713	4606.526428	24.352512
132.477089	4598.480682	24.357530
132.186451	4601.284910	24.362547
132.201452	4608.630812	24.367565
132.545603	4618.614495	24.372583
132.557417	4623.568271	24.377600
132.853126	4622.028827	24.382618
132.736296	4635.588461	24.387635
132.881646	4641.821804	24.392653
133.444533	4653.968170	24.397671
133.220717	4653.558076	24.402688
133.065715	4650.447853	24.407706
133.295909	4671.954909	24.412723
133.514463	4669.060777	24.417741
133.655142	4674.802446	24.422759
133.697033	4695.082736	24.427776
134.237016	4697.018223	24.432794
134.182430	4703.693257	24.437811
134.647483	4702.603911	24.442829
134.627893	4706.429438	24.447847
134.541403	4724.311978	24.452864
134.934792	4715.374112	24.457882
134.594252	4729.448656	24.462899
135.058839	4722.021079	24.467917
135.120600	4737.418317	24.472935
135.145025	4745.375164	24.477952
135.434355	4749.543713	24.482970
135.668153	4758.717751	24.487987
135.950628	4768.045151	24.493005
136.120680	4767.219818	24.498023
135.998227	4774.274824	24.503040
135.762147	4761.821321	24.508058
136.159537	4782.734138	24.513075
136.207953	4793.815375	24.518093
136.595469	4800.266513	24.523111
136.529075	4803.613286	24.528128
137.020767	4817.043001	24.533146
136.702874	4824.946189	24.538163
136.944208	4821.830663	24.543181
137.225154	4827.591441	24.548199
137.530785	4850.270593	24.553216
137.524435	4846.007004	24.558234
137.809040	4848.727462	24.563251
137.387931	4844.096405	24.568269
137.983630	4865.486454	24.573287
138.111988	4875.564060	24.578304
138.031331	4873.651110	24.583322
138.188086	4894.718548	24.588339
138.739450	4889.313286	24.593357
138.698788	4892.943291	24.598375
138.732915	4901.384796	24.603392
138.975117	4915.355562	24.608410
138.741358	4929.902797	24.613427
139.183604	4933.605514	24.618445
138.967653	4924.510484	24.623463
139.277004	4950.661394	24.628480
139.817422	4945.128412	24.633498
140.017354	4959.178434	24.638515
139.978123	4946.046869	24.643533
140.033715	4962.237561	24.648551
140.215739	4973.828279	24.653568
140.454113	4971.723293	24.658586
140.583729	4972.444691	24.663603
140.849307	4987.996448	24.668621
140.930308	4988.652861	24.673639
140.771184	5007.670797	24.678656
141.075718	5010.318713	24.683674
140.652606	5012.244132	24.688691
140.890054	5023.112812	24.693709
141.150384	5024.142018	24.698727
141.353066	5044.668973	24.703744
141.509590	5053.160818	24.708762
141.661232	5064.147133	24.713779
141.747310	5062.561579	24.718797
142.327053	5069.487752	24.723815
142.438625	5079.141962	24.728832
142.488128	5080.141068	24.733850
142.948635	5076.422977	24.738867
142.783953	5082.177892	24.743885
142.666446	5077.833809	24.748903
142.876740	5101.317356	24.753920
142.959703	5102.756301	24.758938
143.140163	5104.435656	24.763955
142.907130	5119.443790	24.768973
143.501154	5121.124645	24.773991
143.521291	5127.822850	24.779008
144.024763	5138.899295	24.784026
143.997099	5152.884112	24.789043
143.997809	5155.882680	24.794061
144.341274	5153.597067	24.799079
143.876091	5162.028532	24.804096
144.386513	5169.041361	24.809114
144.740592	5176.321745	24.814131
144.811901	5183.535950	24.819149
144.965887	5186.630462	24.824167
145.096192	5206.079909	24.829184
144.951997	5209.135910	24.834202
145.292544	5210.764943	24.839219
145.472256	5228.486321	24.844237
145.707583	5224.576202	24.849255
145.592558	5236.863886	24.854272
146.032865	5247.044344	24.859290
146.032382	5259.273062	24.864307
146.248733	5261.240375	24.869325
146.496067	5270.955489	24.874343
146.709579	5283.949324	24.879360
146.906965	5281.935953	24.884378
147.058661	5280.204366	24.889395
146.889777	5292.860380	24.894413
147.072073	5301.780761	24.899431
147.106560	5306.724858	24.904448
147.439143	5308.250978	24.909466
147.932913	5322.712958	24.914483
147.952517	5340.102829	24.919501
148.285888	5336.849689	24.924519
148.336433	5337.264670	24.929536
148.407647	5331.839802	24.934554
148.666088	5349.283807	24.939571
148.531310	5368.569774	24.944589
149.108488	5364.845975	24.949607
148.943921	5368.006206	24.954624
148.689577	5362.966936	24.959642
149.043099	5385.920193	24.964659
149.115224	5387.869078	24.969677
149.277902	5391.549398	24.974695
149.053082	5407.866488	24.979712
149.534674	5415.471066	24.984730
149.900804	5420.483190	24.989747
149.709583	5445.943010	24.994765
150.150390	5438.250556	24.999783
149.861614	5444.545872	25.004800
150.060831	5462.185505	25.009818
150.498500	5471.034395	25.014835
150.980513	5493.415243	25.019853
150.768509	5493.505187	25.024871
150.774626	5504.296756	25.029888
151.060405	5502.784049	25.034906
151.488732	5512.357298	25.039923
151.668012	5520.691120	25.044941
151.847478	5530.363342	25.049959
151.958681	5526.437881	25.054976
151.938362	5537.707111	25.059994
152.310884	5537.216199	25.065011
152.204176	5549.114519	25.070029
152.648691	5548.129358	25.075047
152.562403	5546.131989	25.080064
152.911583	5540.360473	25.085082
153.226805	5561.233396	25.090099
153.046458	5575.204575	25.095117
153.470304	5574.503594	25.100135
153.636012	5574.698512	25.105152
153.276018	5581.421712	25.110170
153.979754	5579.306887	25.115187
153.522935	5593.416093	25.120205
153.657436	5598.713931	25.125223
153.591745	5606.631608	25.130240
154.105135	5611.611245	25.135258
154.012000	5611.972981	25.140275
154.398498	5626.736110	25.145293
154.535633	5649.433184	25.150311
154.443586	5648.260602	25.155328
154.508773	5660.454047	25.160346
155.503809	5665.127805	25.165363
155.210218	5675.903294	25.170381
155.377403	5685.337614	25.175399
155.597378	5704.672530	25.180416
155.688780	5708.064195	25.185434
155.554083	5701.516127	25.190451
155.684542	5731.793572	25.195469
156.307479	5733.684613	25.200487
156.424386	5746.371928	25.205504
156.661797	5759.280284	25.210522
156.954575	5755.550454	25.215539
156.687343	5753.382538	25.220557
157.165641	5767.187545	25.225575
156.930912	5785.340569	25.230592
157.215276	5789.885785	25.235610
157.390728	5796.048517	25.240627
157.602997	5816.044510	25.245645
157.564344	5813.938635	25.250663
157.780250	5827.516474	25.255680
157.886253	5843.194974	25.260698
158.583162	5838.514779	25.265715
158.355770	5867.866772	25.270733
158.618812	5863.949019	25.275751
159.021150	5858.383733	25.280768
158.873441	5863.526986	25.285786
159.033311	5891.233674	25.290803
159.261495	5894.158846	25.295821
159.501173	5891.419051	25.300839
159.905761	5900.178631	25.305856
159.887052	5910.150423	25.310874
160.174049	5913.716671	25.315891
159.796844	5912.708701	25.320909
160.138681	5927.636907	25.325927
160.268065	5938.687213	25.330944
160.282379	5933.725652	25.335962
160.597286	5945.416126	25.340979
160.418416	5966.044929	25.345997
161.094076	5966.882855	25.351015
161.377441	5987.126750	25.356032
161.401538	5986.551515	25.361050
161.511488	5991.133576	25.366067
161.504354	5999.127481	25.371085
161.752998	6010.541114	25.376103
161.951392	6011.033964	25.381120
161.777559	6030.781318	25.386138
162.329096	6035.218448	25.391155
162.425881	6040.039340	25.396173
162.215860	6047.900900	25.401191
162.752099	6061.337184	25.406208
162.865938	6070.331800	25.411226
163.418326	6063.237173	25.416243
162.824612	6082.908308	25.421261
163.644815	6083.606796	25.426279
163.797093	6090.578232	25.431296
163.547391	6092.252463	25.436314
164.095815	6107.631437	25.441331
163.920631	6108.476394	25.446349
164.175620	6111.697295	25.451367
164.398182	6118.395719	25.456384
164.226439	6133.101501	25.461402
164.396867	6141.200236	25.466419
164.498710	6149.593828	25.471437
165.116754	6161.757818	25.476455
165.087306	6170.964338	25.481472
165.229943	6184.601273	25.486490
165.747520	6186.619357	25.491507
165.884984	6193.492135	25.496525
165.701260	6194.733031	25.501543
166.067784	6215.914342	25.506560
166.043158	6223.819539	25.511578
166.416001	6229.155984	25.516595
166.263582	6240.500007	25.521613
166.866244	6237.242404	25.526631
166.885271	6248.947857	25.531648
167.019284	6268.502027	25.536666
167.031589	6272.692230	25.541683
167.427030	6288.442570	25.546701
167.411813	6291.001868	25.551719
167.731460	6306.069602	25.556736
167.909731	6315.382553	25.561754
168.415028	6324.650589	25.566771
168.299305	6330.395067	25.571789
168.175300	6332.813574	25.576807
168.473168	6349.737799	25.581824
168.499411	6355.993545	25.586842
168.738467	6372.058883	25.591859
168.881998	6382.630563	25.596877
168.919408	6388.366853	25.601895
169.477355	6404.622179	25.606912
169.815356	6414.854044	25.611930
169.975320	6411.596315	25.616947
170.303328	6412.087812	25.621965
170.247180	6427.003011	25.626983
170.531844	6428.849261	25.632000
170.447674	6441.849516	25.637018
170.805989	6443.109688	25.642035
170.976662	6458.213513	25.647053
170.775690	6456.941139	25.652071
171.167471	6456.715519	25.657088
170.881893	6480.291148	25.662106
171.529899	6486.253810	25.667123
171.733674	6495.682816	25.672141
171.860428	6508.586938	25.677159
171.915631	6512.315891	25.682176
172.113278	6525.660346	25.687194
172.664317	6538.854744	25.692212
172.779487	6541.778785	25.697229
172.661552	6540.607044	25.702247
172.984254	6545.089620	25.707264
172.780321	6567.273032	25.712282
173.403800	6566.695429	25.717300
173.452653	6562.167088	25.722317
173.559331	6586.779984	25.727335
173.955079	6592.321300	25.732352
173.681383	6601.320065	25.737370
173.530444	6598.998083	25.742388
173.789704	6619.369571	25.747405
174.059143	6625.798819	25.752423
174.540746	6647.199365	25.757440
174.497183	6652.339149	25.762458
174.764674	6648.979298	25.767476
174.715681	6670.112582	25.772493
175.243816	6673.095067	25.777511
175.209369	6684.386156	25.782528
175.615258	6693.818327	25.787546
175.811567	6704.713395	25.792564
175.443328	6715.867383	25.797581
175.868878	6724.049526	25.802599
176.242092	6724.193009	25.807616
176.378188	6751.355425	25.812634
176.567546	6747.922561	25.817652
176.601264	6754.202526	25.822669
176.766690	6769.332684	25.827687
176.984788	6768.948014	25.832704
177.185873	6791.895349	25.837722
177.338736	6791.943920	25.842740
177.793229	6812.613353	25.847757
177.777696	6829.707080	25.852775
178.280475	6834.439324	25.857792
178.427186	6833.532322	25.862810
178.650915	6849.265848	25.867828
178.732692	6852.466664	25.872845
178.589491	6849.632021	25.877863
179.069153	6858.683363	25.882880
179.257663	6878.554806	25.887898
179.609782	6864.864924	25.892916
179.871326	6886.672737	25.897933
179.841085	6895.324130	25.902951
180.128336	6907.426793	25.907968
179.729568	6906.901990	25.912986
180.428563	6920.026131	25.918004
180.540964	6930.423061	25.923021
180.623410	6932.714596	25.928039
180.819353	6936.866711	25.933056
181.065495	6955.261247	25.938074
181.149027	6958.376569	25.943092
181.195368	6973.632886	25.948109
181.164944	6979.228456	25.953127
181.539598	6983.570411	25.958144
181.958631	7003.317482	25.963162
181.880181	7003.370722	25.968180
182.183808	7011.600507	25.973197
182.272085	7028.113067	25.978215
182.491458	7025.190028	25.983232
182.709547	7056.491402	25.988250
182.853305	7055.294415	25.993268
182.839882	7068.167223	25.998285
183.144637	7088.901465	26.003303
183.703148	7081.016258	26.008320
183.546656	7106.466625	26.013338
184.046784	7117.175437	26.018356
183.914776	7125.527187	26.023373
184.408089	7144.732407	26.028391
184.652723	7136.637480	26.033408
184.707647	7149.060822	26.038426
185.276008	7169.608640	26.043444
185.329215	7173.915761	26.048461
185.276714	7168.481321	26.053479
185.373218	7174.315935	26.058496
185.551378	7188.377396	26.063514
185.555287	7196.531096	26.068532
185.960892	7205.294302	26.073549
186.082189	7223.358242	26.078567
186.446322	7220.099955	26.083584
186.498649	7226.383481	26.088602
186.597420	7245.224425	26.093620
186.963705	7251.569269	26.098637
186.981738	7255.001127	26.103655
187.154153	7255.959000	26.108672
187.687050	7277.077590	26.113690
187.483100	7274.880634	26.118708
187.562588	7278.176591	26.123725
187.438393	7297.633400	26.128743
187.941480	7294.744797	26.133760
188.343612	7322.440947	26.138778
188.195006	7329.333711	26.143796
188.546761	7341.855903	26.148813
188.652175	7351.906898	26.153831
188.804659	7355.084096	26.158848
189.070323	7361.621532	26.163866
189.167138	7382.451820	26.168884
189.274372	7391.643852	26.173901
189.518414	7411.052564	26.178919
189.773247	7422.355613	26.183936
190.311436	7440.607016	26.188954
190.174911	7449.430012	26.193972
190.588040	7464.768183	26.198989
190.738363	7482.752062	26.204007
190.789057	7479.896417	26.209024
191.139024	7501.353308	26.214042
191.144393	7505.945818	26.219060
191.405568	7515.906204	26.224077
191.286302	7528.281322	26.229095
191.646471	7535.110244	26.234112
192.199946	7550.180254	26.239130
192.151309	7566.316961	26.244148
192.316139	7578.603409	26.249165
192.402766	7593.932853	26.254183
192.994971	7609.833455	26.259200
193.135586	7614.723663	26.264218
193.321134	7635.628733	26.269236
193.531262	7640.312323	26.274253
193.610483	7643.504205	26.279271
193.976100	7662.976220	26.284288
194.085258	7676.240662	26.289306
194.285289	7680.799563	26.294324
194.537046	7695.272923	26.299341
194.483828	7706.668603	26.304359
194.813252	7716.820457	26.309376
195.113814	7719.030566	26.314394
194.977218	7723.496988	26.319412
195.278407	7746.912858	26.324429
195.478264	7757.384951	26.329447
195.974713	7762.680384	26.334464
196.070256	7784.139577	26.339482
196.184856	7784.383570	26.344500
196.599568	7795.939622	26.349517
196.845257	7805.230139	26.354535
196.707792	7813.570426	26.359552
197.132003	7828.591459	26.364570
197.176186	7836.837001	26.369588
197.253789	7841.130986	26.374605
197.394864	7861.579191	26.379623
197.814408	7870.536269	26.384640
197.872371	7893.147491	26.389658
198.220452	7899.365971	26.394676
198.623812	7903.050136	26.399693
198.557800	7920.136996	26.404711
198.574901	7928.857226	26.409728
199.098409	7946.148523	26.414746
198.965676	7950.797506	26.419764
199.023538	7957.995966	26.424781
199.009121	7977.774100	26.429799
199.630797	7984.827419	26.434816
199.761262	7998.050869	26.439834
199.810209	8008.319435	26.444852
200.100892	8022.177636	26.449869
200.143159	8023.989410	26.454887
200.648642	8043.970308	26.459904
200.812176	8054.798698	26.464922
200.993811	8063.010180	26.469940
201.562641	8078.441284	26.474957
201.626184	8095.242813	26.479975
201.794504	8094.363937	26.484992
202.265899	8102.956254	26.490010
202.073411	8114.380317	26.495028
202.024580	8120.847320	26.500045
202.216260	8136.564868	26.505063
202.507540	8149.450680	26.510080
202.970819	8162.940980	26.515098
202.752454	8178.845927	26.520116
203.312907	8185.586888	26.525133
203.389278	8202.187606	26.530151
203.825798	8215.082282	26.535168
204.160189	8219.399270	26.540186
204.073097	8229.872384	26.545204
204.399085	8240.725947	26.550221
204.068828	8257.519858	26.555239
204.655086	8272.124382	26.560256
204.866752	8276.539537	26.565274
205.103671	8301.039604	26.570292
205.339917	8306.991599	26.575309
205.364003	8322.280931	26.580327
205.614032	8338.529381	26.585344
205.990293	8356.440830	26.590362
206.390583	8367.368072	26.595380
206.684277	8375.009637	26.600397
206.538687	8398.515266	26.605415
206.931627	8402.538981	26.610432
207.071175	8414.504758	26.615450
207.192880	8427.931946	26.620468
207.720479	8436.019940	26.625485
207.799616	8448.591907	26.630503
207.869086	8463.596415	26.635520
208.221602	8463.765261	26.640538
208.119416	8478.967159	26.645556
208.628506	8487.711609	26.650573
208.461838	8500.748336	26.655591
208.814961	8518.742497	26.660608
208.941039	8530.486300	26.665626
209.192466	8540.313008	26.670644
209.732026	8552.512986	26.675661
209.777932	8564.591402	26.680679
209.944338	8585.737334	26.685696
210.164041	8589.279921	26.690714
210.355933	8607.798262	26.695732
210.860149	8603.415933	26.700749
210.740885	8627.100844	26.705767
210.887269	8637.168221	26.710784
211.473613	8645.869072	26.715802
211.402545	8666.000950	26.720820
212.069275	8659.610426	26.725837
212.031301	8672.169319	26.730855
212.076055	8688.263958	26.735872
212.562955	8700.339681	26.740890
212.550649	8718.463898	26.745908
212.890741	8723.815676	26.750925
212.676771	8728.127128	26.755943
212.909846	8746.645471	26.760960
213.411152	8748.094941	26.765978
213.326141	8774.935048	26.770996
213.978991	8780.916651	26.776013
214.336784	8781.034158	26.781031
213.761620	8799.016152	26.786048
214.382876	8810.856207	26.791066
214.487017	8817.706772	26.796084
214.524881	8833.038567	26.801101
215.149981	8854.952772	26.806119
215.229357	8868.336395	26.811136
215.424015	8878.554202	26.816154
215.339475	8892.898063	26.821172
215.622569	8901.018250	26.826189
215.926297	8916.857826	26.831207
216.119398	8937.892631	26.836224
216.330659	8943.785601	26.841242
216.590855	8963.262872	26.846260
216.911654	8974.057692	26.851277
216.694137	8991.229259	26.856295
217.367429	9005.552364	26.861312
217.520448	9020.970464	26.866330
217.785123	9030.852189	26.871348
217.884632	9046.970134	26.876365
218.495070	9064.431982	26.881383
218.097199	9070.079431	26.886400
218.662317	9071.433686	26.891418
218.562470	9095.851796	26.896436
219.074157	9106.092682	26.901453
219.488727	9123.386361	26.906471
219.126990	9145.111359	26.911488
219.943575	9155.036139	26.916506
220.018648	9183.234647	26.921524
220.050868	9184.397708	26.926541
220.280061	9198.291681	26.931559
220.081642	9218.974532	26.936576
220.906985	9229.147406	26.941594
221.080616	9249.127919	26.946612
221.263150	9263.711227	26.951629
221.287498	9269.924054	26.956647
221.245408	9293.490375	26.961664
221.915276	9302.715196	26.966682
221.794962	9318.005866	26.971700
222.332918	9345.254375	26.976717
222.907338	9357.765155	26.981735
223.046843	9380.968464	26.986752
223.159708	9390.488968	26.991770
223.425665	9398.463664	26.996788
223.737025	9414.469807	27.001805
224.224813	9431.035590	27.006823
224.007486	9446.954086	27.011840
224.556288	9450.170596	27.016858
224.924814	9453.465866	27.021876
224.957252	9470.882878	27.026893
224.934149	9476.156005	27.031911
225.141756	9500.074982	27.036928
225.185042	9507.560488	27.041946
225.645834	9524.856773	27.046964
226.048760	9529.311728	27.051981
226.246079	9545.784192	27.056999
226.037786	9553.899552	27.062016
226.615258	9565.251247	27.067034
226.930283	9580.998057	27.072052
227.083309	9593.208757	27.077069
227.448885	9605.622970	27.082087
227.140024	9617.410336	27.087104
227.843002	9632.768049	27.092122
228.290847	9643.451793	27.097140
228.223289	9661.045673	27.102157
228.577046	9676.565481	27.107175
228.648367	9680.826144	27.112192
228.823591	9684.372753	27.117210
228.672327	9699.299172	27.122228
229.031503	9712.323832	27.127245
229.333185	9730.589290	27.132263
229.632385	9743.124501	27.137280
229.994325	9753.193446	27.142298
229.845884	9761.615259	27.147316
229.781095	9776.667118	27.152333
230.350984	9791.439593	27.157351
230.617989	9820.231005	27.162368
230.695346	9827.184016	27.167386
230.828128	9849.081798	27.172404
231.323023	9867.730742	27.177421
231.417847	9882.751368	27.182439
231.486234	9901.012493	27.187456
232.018015	9918.203301	27.192474
232.274418	9940.391250	27.197492
232.400489	9953.250522	27.202509
233.089592	9960.455068	27.207527
232.810564	9990.648925	27.212544
233.558335	9993.480731	27.217562
233.565181	10003.037101	27.222580
233.874383	10024.250707	27.227597
234.295684	10029.002860	27.232615
234.205648	10053.682754	27.237632
234.483020	10064.532373	27.242650
234.870252	10080.088319	27.247668
235.046242	10098.373827	27.252685
235.379595	10107.017120	27.257703
235.595498	10130.414628	27.262720
235.730958	10130.917455	27.267738
235.744872	10152.013276	27.272756
235.836468	10174.565169	27.277773
236.946425	10181.748078	27.282791
236.520560	10202.657095	27.287808
236.970253	10222.737491	27.292826
237.105479	10224.354943	27.297844
237.653837	10245.651320	27.302861
237.619061	10258.008701	27.307879
237.781490	10286.090995	27.312896
238.076915	10288.659017	27.317914
238.498021	10292.966065	27.322932
238.789322	10320.043089	27.327949
238.766443	10328.717030	27.332967
239.113888	10356.044225	27.337984
239.708271	10368.530459	27.343002
239.863519	10380.169821	27.348020
239.929255	10389.404571	27.353037
240.509569	10399.651210	27.358055
239.965716	10414.971236	27.363072
240.425434	10430.424553	27.368090
240.821618	10444.362761	27.373108
240.712303	10463.735296	27.378125
241.302578	10473.105786	27.383143
241.361753	10482.414233	27.388160
241.981660	10492.859960	27.393178
241.753014	10511.907069	27.398196
242.061537	10533.863376	27.403213
242.672895	10545.579793	27.408231
242.601845	10561.163727	27.413248
243.044110	10573.023478	27.418266
243.570717	10593.139588	27.423284
243.580415	10600.204528	27.428301
244.139371	10612.109175	27.433319
243.942273	10632.884950	27.438336
244.088819	10640.970453	27.443354
244.283164	10644.173236	27.448372
244.493887	10661.689731	27.453389
244.865907	10674.122593	27.458407
244.804885	10685.480269	27.463424
245.096944	10713.631309	27.468442
245.684358	10721.262564	27.473460
245.723639	10745.544205	27.478477
246.058147	10757.692504	27.483495
246.014647	10782.574466	27.488512
246.581057	10785.791612	27.493530
246.897248	10793.070690	27.498548
246.608327	10799.790946	27.503565
247.232283	10832.983322	27.508583
247.077906	10849.186801	27.513600
247.628240	10864.449458	27.518618
248.096462	10884.543452	27.523636
247.946092	10905.567972	27.528653
248.235154	10911.907229	27.533671
248.516195	10929.368752	27.538688
248.673137	10944.055268	27.543706
249.178851	10968.763029	27.548724
249.321003	10988.425103	27.553741
249.646338	10998.178381	27.558759
249.751864	11029.472506	27.563776
250.241699	11034.593095	27.568794
250.612281	11066.613058	27.573812
250.852578	11066.505859	27.578829
251.007693	11088.701565	27.583847
250.885285	11108.357844	27.588864
251.559379	11126.247409	27.593882
251.823434	11153.513048	27.598900
251.868904	11164.990110	27.603917
252.173314	11175.523535	27.608935
252.394625	11206.544049	27.613952
252.577147	11216.935552	27.618970
252.871223	11233.160682	27.623988
252.953440	11253.735506	27.629005
253.561312	11275.276345	27.634023
253.652608	11290.102879	27.639040
254.102486	11307.329901	27.644058
254.776353	11329.975115	27.649076
255.025298	11340.612051	27.654093
255.230916	11346.541402	27.659111
255.210202	11375.487638	27.664128
255.555637	11375.231346	27.669146
255.996958	11382.194231	27.674164
255.967689	11403.004562	27.679181
256.634854	11415.315898	27.684199
256.676971	11423.446518	27.689216
256.641090	11441.431814	27.694234
257.379230	11448.525057	27.699252
256.898009	11473.498606	27.704269
257.609437	11481.597030	27.709287
258.082788	11506.673703	27.714304
257.707533	11506.934489	27.719322
258.139240	11522.222582	27.724340
258.098756	11552.195276	27.729357
258.589887	11568.033009	27.734375
259.175551	11598.937099	27.739392
259.164965	11608.054940	27.744410
259.202972	11634.463060	27.749428
259.482446	11657.018881	27.754445
259.894579	11667.598862	27.759463
260.402666	11685.909681	27.764480
260.437496	11696.634041	27.769498
260.825245	11715.544760	27.774516
261.123081	11731.766575	27.779533
261.489919	11750.349043	27.784551
261.280137	11768.428206	27.789568
261.579900	11775.018697	27.794586
262.239884	11789.964950	27.799604
262.235274	11813.238057	27.804621
262.731247	11822.194548	27.809639
262.731544	11843.783851	27.814656
262.842556	11856.634157	27.819674
263.405192	11864.291868	27.824692
263.568102	11889.963972	27.829709
263.747525	11902.724649	27.834727
264.482726	11917.248714	27.839744
264.372544	11926.562302	27.844762
264.546755	11944.183604	27.849780
264.683297	11966.316943	27.854797
264.626470	11983.396603	27.859815
265.030535	12010.136311	27.864832
265.105746	12028.044767	27.869850
265.880798	12046.759364	27.874868
266.139463	12072.650392	27.879885
266.392138	12086.129164	27.884903
266.519242	12114.516557	27.889920
266.357060	12136.886358	27.894938
267.099134	12160.368177	27.899956
267.201573	12187.588003	27.904973
267.570342	12200.837100	27.909991
268.141066	12217.382890	27.915008
268.174782	12234.404385	27.920026
268.836186	12248.697116	27.925044
269.010390	12286.670804	27.930061
269.645853	12290.796323	27.935079
269.928015	12303.942220	27.940096
270.108373	12330.679532	27.945114
270.322162	12326.291321	27.950132
270.211947	12355.777280	27.955149
270.496451	12367.021844	27.960167
270.939672	12380.313087	27.965184
271.187898	12392.646485	27.970202
271.630523	12411.839827	27.975220
271.898452	12434.414177	27.980237
271.685103	12442.913670	27.985255
271.964121	12466.847349	27.990272
272.160666	12486.464573	27.995290
272.801349	12510.344811	28.000308
272.653774	12541.150576	28.005325
272.992680	12561.721353	28.010343
273.776423	12581.950895	28.015360
273.832046	12602.449252	28.020378
273.830194	12614.856705	28.025396
274.439160	12638.198921	28.030413
274.517865	12664.106320	28.035431
275.204740	12683.997463	28.040448
275.313398	12707.348664	28.045466
275.785622	12709.734591	28.050484
275.757558	12741.396694	28.055501
276.218865	12761.553779	28.060519
276.523718	12776.843817	28.065536
276.594667	12802.430515	28.070554
276.953022	12806.372189	28.075572
276.967496	12832.776196	28.080589
277.111602	12849.859899	28.085607
277.583521	12868.487011	28.090624
277.676754	12895.087189	28.095642
278.405380	12910.888851	28.100660
278.374802	12932.171599	28.105677
278.772833	12960.340979	28.110695
278.842636	12974.954306	28.115712
279.617033	12995.520496	28.120730
279.938500	13010.978649	28.125748
279.999207	13028.805061	28.130765
279.906489	13039.335423	28.135783
280.369340	13056.426225	28.140800
280.598842	13070.923030	28.145818
280.843353	13086.431195	28.150836
280.826189	13111.915269	28.155853
281.035366	13126.191086	28.160871
281.711189	13145.121272	28.165888
282.098037	13171.274784	28.170906
282.282032	13189.694678	28.175924
282.963389	13214.472614	28.180941
282.804300	13225.278745	28.185959
283.282336	13250.745435	28.190976
283.415015	13266.511272	28.195994
284.083701	13288.392269	28.201012
284.098347	13303.968199	28.206029
284.642376	13316.868512	28.211047
284.935849	13329.909138	28.216064
284.771216	13358.006191	28.221082
285.367016	13374.798552	28.226100
285.617851	13398.216756	28.231117
285.711182	13413.714133	28.236135
286.025402	13425.068361	28.241152
286.123445	13458.107741	28.246170
286.674514	13475.772493	28.251188
286.880387	13509.508781	28.256205
287.140718	13527.850728	28.261223
287.496699	13546.638780	28.266240
287.722770	13565.876692	28.271258
288.111438	13580.926872	28.276276
288.073409	13608.120215	28.281293
288.491161	13633.271585	28.286311
288.974603	13655.447300	28.291328
289.536800	13678.908659	28.296346
289.700987	13687.523259	28.301364
289.616773	13716.347226	28.306381
289.879502	13733.324718	28.311399
290.233970	13766.921338	28.316416
290.671057	13777.593339	28.321434
290.856947	13798.659981	28.326452
291.003348	13821.021324	28.331469
291.510832	13846.487360	28.336487
291.576751	13867.594978	28.341504
291.748018	13892.655822	28.346522
292.468803	13915.050465	28.351540
292.659764	13941.172562	28.356557
292.866278	13965.081594	28.361575
293.510546	13983.006974	28.366592
293.819903	14006.682040	28.371610
293.914660	14036.242715	28.376628
294.271512	14056.954421	28.381645
294.812169	14078.158444	28.386663
295.183114	14088.664127	28.391680
295.460896	14113.215911	28.396698
295.716785	14125.056571	28.401716
295.800897	14154.938068	28.406733
295.954447	14167.716958	28.411751
296.450954	14185.630936	28.416768
296.497894	14218.376460	28.421786
296.744122	14238.414061	28.426804
296.930033	14259.664382	28.431821
297.592037	14279.384245	28.436839
297.692384	14298.626801	28.441856
298.398143	14328.433299	28.446874
298.443340	14343.051532	28.451892
298.940355	14353.329176	28.456909
298.718549	14384.673806	28.461927
299.238226	14400.136783	28.466944
299.750192	14434.878431	28.471962
299.540824	14446.053160	28.476980
300.584880	14463.164725	28.481997
300.273549	14491.213788	28.487015
300.670185	14502.151504	28.492032
301.096813	14528.442772	28.497050
301.026704	14547.882822	28.502068
301.418619	14557.993865	28.507085
301.774831	14588.360835	28.512103
302.016091	14613.639053	28.517120
302.603229	14640.375903	28.522138
302.837546	14659.424136	28.527156
302.877110	14678.247081	28.532173
303.182573	14702.466834	28.537191
303.438751	14724.237245	28.542208
304.208675	14758.023192	28.547226
304.336749	14771.472862	28.552244
304.771383	14786.905260	28.557261
304.737984	14808.474786	28.562279
305.219039	14834.868488	28.567296
305.626338	14859.814674	28.572314
306.146912	14875.663202	28.577332
306.504108	14892.311106	28.582349
306.141287	14917.592763	28.587367
307.046757	14930.077517	28.592384
307.477860	14953.440971	28.597402
307.482201	14974.009923	28.602420
307.748257	14997.440342	28.607437
307.932107	15027.759211	28.612455
308.247022	15037.370932	28.617472
308.895716	15072.019683	28.622490
308.917114	15095.501179	28.627508
309.448257	15120.835724	28.632525
309.506580	15146.449656	28.637543
310.324130	15160.372722	28.642560
310.402472	15180.835555	28.647578
310.757899	15205.101809	28.652596
311.168377	15220.077231	28.657613
310.942093	15255.858239	28.662631
311.427813	15275.309868	28.667648
311.938338	15300.587873	28.672666
312.197002	15320.406738	28.677684
312.675591	15331.654242	28.682701
312.673110	15360.944791	28.687719
312.786185	15384.071181	28.692736
313.289271	15408.396680	28.697754
313.571005	15427.883576	28.702772
313.866854	15453.388069	28.707789
313.842634	15481.425189	28.712807
314.452676	15515.079603	28.717824
314.663043	15542.464188	28.722842
314.745907	15564.588014	28.727860
315.077061	15607.025446	28.732877
315.683398	15633.760679	28.737895
316.409538	15646.700377	28.742912
316.602740	15673.102426	28.747930
316.753305	15696.810778	28.752948
317.362794	15711.044776	28.757965
317.645852	15746.089969	28.762983
317.894090	15763.876925	28.768000
318.398474	15779.640306	28.773018
318.558674	15811.050605	28.778036
319.117978	15821.429830	28.783053
319.346639	15846.910629	28.788071
319.465134	15855.138565	28.793088
319.633762	15896.664050	28.798106
320.156581	15914.521838	28.803124
320.513429	15930.207384	28.808141
320.868914	15954.828322	28.813159
321.288883	15969.701774	28.818176
321.441126	15990.062299	28.823194
321.248927	16016.724172	28.828212
321.662037	16024.129058	28.833229
321.386532	16060.724672	28.838247
322.273851	16083.332662	28.843264
322.002743	16118.623262	28.848282
323.019352	16147.003665	28.853300
323.220388	16167.596777	28.858317
323.462581	16206.906807	28.863335
323.715452	16230.855628	28.868352
324.691272	16267.628323	28.873370
324.472756	16282.491486	28.878388
325.160515	16298.630854	28.883405
325.099334	16329.738720	28.888423
325.306492	16346.654594	28.893440
325.931327	16375.845265	28.898458
326.324152	16412.283164	28.903476
326.918633	16427.698164	28.908493
326.829809	16459.508598	28.913511
327.223258	16481.430061	28.918528
327.354716	16519.826317	28.923546
328.052106	16542.410905	28.928564
328.043085	16570.870471	28.933581
328.623697	16596.483484	28.938599
329.119043	16622.248864	28.943616
329.553917	16651.874001	28.948634
329.512441	16670.326251	28.953652
330.089934	16694.480640	28.958669
330.408605	16726.837281	28.963687
330.858035	16754.543060	28.968704
331.036552	16772.673519	28.973722
331.470416	16802.400120	28.978740
331.768473	16822.050118	28.983757
331.764768	16851.864288	28.988775
332.148798	16872.739028	28.993792
332.678999	16909.510107	28.998810
333.186282	16931.117346	29.003828
333.540804	16963.064469	29.008845
333.872684	16988.066297	29.013863
334.231171	17014.655921	29.018880
334.573460	17035.966945	29.023898
334.556783	17070.107601	29.028916
335.322213	17084.245546	29.033933
335.693514	17119.033043	29.038951
336.010672	17132.388416	29.043968
336.408783	17160.222843	29.048986
336.209596	17187.348583	29.054004
337.195659	17211.471207	29.059021
337.275257	17232.659349	29.064039
337.517935	17260.549854	29.069056
337.509407	17286.098136	29.074074
337.429516	17309.023324	29.079092
338.348954	17337.332267	29.084109
338.438135	17367.609636	29.089127
338.817398	17400.400125	29.094144
339.443504	17433.777419	29.099162
339.640834	17462.035405	29.104180
340.036738	17482.100327	29.109197
340.320565	17520.389418	29.114215
340.513821	17551.231968	29.119232
340.905980	17569.585563	29.124250
341.576896	17602.836099	29.129268
342.137192	17637.057946	29.134285
341.858517	17653.179267	29.139303
342.497177	17683.731151	29.144320
343.126419	17701.656055	29.149338
342.960003	17737.078505	29.154356
343.723303	17754.047481	29.159373
344.218275	17773.364366	29.164391
344.099435	17792.196213	29.169408
344.848412	17814.701562	29.174426
345.049090	17843.983007	29.179444
345.827864	17869.408735	29.184461
345.774627	17887.402810	29.189479
346.022449	17909.096007	29.194496
346.242580	17931.368457	29.199514
346.514793	17955.016305	29.204532
347.152238	17980.540127	29.209549
347.196988	18004.855415	29.214567
347.636681	18033.063634	29.219584
347.840253	18054.207984	29.224602
347.810728	18083.431085	29.229620
348.598354	18113.227480	29.234637
348.934742	18137.832082	29.239655
349.212276	18174.822035	29.244672
349.466219	18199.054258	29.249690
349.643612	18247.728591	29.254708
350.453592	18265.158206	29.259725
350.889366	18303.147066	29.264743
350.981363	18323.740602	29.269760
351.271911	18349.906785	29.274778
351.087479	18378.320668	29.279796
351.675845	18416.829165	29.284813
352.192670	18449.214503	29.289831
352.610963	18480.427609	29.294848
353.240601	18513.900976	29.299866
353.254878	18555.709050	29.304884
353.280336	18579.649016	29.309901
354.082542	18617.795895	29.314919
354.292544	18646.862286	29.319936
354.833424	18680.817354	29.324954
355.086456	18710.313023	29.329972
355.887117	18739.148041	29.334989
356.113465	18775.559603	29.340007
356.342917	18806.619597	29.345024
356.767680	18830.907981	29.350042
356.956287	18863.806619	29.355060
357.568651	18889.253433	29.360077
358.251100	18920.754393	29.365095
358.481488	18954.872294	29.370112
358.892770	18974.020267	29.375130
358.932742	19012.609525	29.380148
359.559695	19033.726527	29.385165
360.097321	19060.947951	29.390183
360.340835	19096.435016	29.395200
360.749191	19108.810835	29.400218
360.828323	19139.730640	29.405236
360.730933	19160.171506	29.410253
361.732266	19197.479642	29.415271
361.637538	19243.210720	29.420288
362.281660	19262.764759	29.425306
362.155389	19297.722546	29.430324
362.967919	19328.571998	29.435341
363.264580	19363.962774	29.440359
363.365072	19389.414605	29.445376
363.737000	19421.994842	29.450394
364.133965	19455.455728	29.455412
364.544478	19478.521463	29.460429
365.149996	19518.356226	29.465447
365.500227	19550.232460	29.470464
365.979550	19587.692607	29.475482
366.132333	19620.964576	29.480500
366.584097	19639.253927	29.485517
366.870963	19674.122401	29.490535
367.215182	19707.111808	29.495552
367.632154	19724.338937	29.500570
367.965142	19759.882690	29.505588
368.440027	19784.606675	29.510605
368.871148	19809.937765	29.515623
369.018751	19833.879089	29.520640
369.744854	19856.946382	29.525658
370.061951	19888.525088	29.530676
370.053503	19907.063683	29.535693
370.730069	19944.430437	29.540711
370.986686	19970.869470	29.545728
371.198981	20001.169553	29.550746
371.464677	20029.363689	29.555764
371.850224	20057.861320	29.560781
372.054196	20087.467842	29.565799
372.179112	20139.661696	29.570816
372.659225	20168.081492	29.575834
373.083527	20200.218863	29.580852
373.279897	20230.900889	29.585869
373.809064	20263.988628	29.590887
374.320660	20315.092508	29.595904
374.802090	20359.731338	29.600922
375.185136	20382.113749	29.605940
375.638307	20415.832839	29.610957
376.219873	20451.187269	29.615975
376.157753	20484.791324	29.620992
376.751697	20510.167316	29.626010
377.177072	20546.601542	29.631028
377.465128	20587.259041	29.636045
378.214988	20617.905521	29.641063
378.103861	20654.885223	29.646080
379.177383	20685.462156	29.651098
379.330989	20719.039138	29.656116
379.317518	20756.831443	29.661133
379.961951	20787.020821	29.666151
380.151231	20825.261697	29.671168
380.911392	20852.027422	29.676186
381.156428	20888.168288	29.681204
381.767847	20920.593451	29.686221
381.949453	20946.780171	29.691239
382.104364	20992.526764	29.696256
382.794505	21016.321362	29.701274
383.139973	21051.157827	29.706292
383.387741	21078.629650	29.711309
384.414279	21112.234850	29.716327
384.510654	21145.947894	29.721344
384.712248	21175.202588	29.726362
385.174056	21211.392233	29.731380
385.619297	21245.177172	29.736397
385.925802	21266.523700	29.741415
386.288474	21307.859721	29.746432
386.863156	21325.790189	29.751450
386.827038	21353.205764	29.756468
387.205763	21397.553423	29.761485
387.666170	21426.496250	29.766503
387.917550	21467.098122	29.771520
388.434428	21497.656094	29.776538
388.633573	21534.171813	29.781556
389.006109	21564.998925	29.786573
389.805263	21605.066655	29.791591
390.314481	21647.530430	29.796608
390.593113	21667.466373	29.801626
390.723396	21700.391533	29.806644
390.971103	21736.571447	29.811661
391.932832	21773.334645	29.816679
392.044908	21805.416123	29.821696
392.500296	21835.428201	29.826714
392.971875	21858.114360	29.831732
393.196972	21893.482983	29.836749
393.596117	21917.362163	29.841767
393.815236	21952.055719	29.846784
394.528344	21977.111637	29.851802
394.747909	22001.922634	29.856820
394.873722	22035.228178	29.861837
395.376494	22074.553435	29.866855
395.753737	22100.704721	29.871872
396.185481	22130.487154	29.876890
396.532505	22176.181117	29.881908
397.149757	22204.323298	29.886925
397.271049	22239.607696	29.891943
397.639949	22276.243527	29.896960
398.343124	22296.998250	29.901978
398.522639	22335.110879	29.906996
398.460295	22370.007225	29.912013
399.452857	22413.704949	29.917031
399.663197	22448.198543	29.922048
400.010567	22483.365817	29.927066
400.639915	22512.391193	29.932084
400.951161	22548.076075	29.937101
401.547722	22582.724252	29.942119
401.658913	22611.881487	29.947136
401.859617	22651.090906	29.952154
402.699160	22687.154576	29.957172
402.891240	22721.986412	29.962189
402.695666	22767.450774	29.967207
403.289631	22816.298644	29.972224
404.057378	22837.719958	29.977242
404.549350	22884.347024	29.982260
404.675793	22926.045694	29.987277
405.235710	22967.196303	29.992295
405.778560	23011.863097	29.997312
406.374629	23041.747540	30.002330
406.632897	23074.623337	30.007348
407.092608	23121.116990	30.012365
407.857825	23156.624431	30.017383
407.638919	23207.629034	30.022400
408.142169	23233.648331	30.027418
408.652162	23263.742485	30.032436
408.939185	23311.281021	30.037453
409.621012	23344.198345	30.042471
410.011255	23384.238933	30.047488
410.654119	23427.848321	30.052506
410.732830	23459.229938	30.057524
411.494214	23504.147973	30.062541
412.009245	23531.467583	30.067559
412.276099	23564.747276	30.072576
412.661687	23591.411080	30.077594
413.063597	23623.551202	30.082612
413.282212	23666.582994	30.087629
413.793904	23704.658851	30.092647
413.988692	23736.243898	30.097664
414.556121	23771.208355	30.102682
414.895702	23817.299050	30.107700
415.230657	23861.937118	30.112717
415.505843	23889.484367	30.117735
416.311302	23936.235414	30.122752
416.596210	23972.824327	30.127770
417.063330	24008.834977	30.132788
417.682892	24052.626324	30.137805
418.051531	24069.953288	30.142823
418.092965	24110.365938	30.147840
418.619267	24155.657191	30.152858
419.247958	24187.838533	30.157876
419.299456	24239.820847	30.162893
419.703647	24264.643661	30.167911
420.184714	24303.401643	30.172928
420.667429	24341.647559	30.177946
421.183048	24379.622974	30.182964
421.629278	24417.603010	30.187981
422.166957	24443.157163	30.192999
422.492355	24483.165872	30.198016
422.684933	24517.261368	30.203034
423.517871	24547.022492	30.208052
423.578406	24589.499623	30.213069
424.165592	24628.273210	30.218087
424.884269	24662.343426	30.223104
425.057320	24691.809987	30.228122
425.765500	24718.184618	30.233140
425.174125	24757.029298	30.238157
426.068394	24791.792674	30.243175
426.577667	24835.849475	30.248192
426.832194	24877.980846	30.253210
427.202476	24922.255517	30.258228
427.768243	24965.981449	30.263245
428.350063	24999.877763	30.268263
428.986508	25045.318087	30.273280
429.137126	25077.683174	30.278298
429.786738	25113.926335	30.283316
429.940273	25159.518392	30.288333
430.011325	25198.102170	30.293351
430.602219	25240.636641	30.298368
430.682045	25283.301808	30.303386
431.385972	25323.796405	30.308404
432.179580	25380.038760	30.313421
432.383874	25415.568552	30.318439
432.974417	25461.389877	30.323456
433.319266	25504.728150	30.328474
433.533813	25549.951299	30.333492
434.209026	25600.562812	30.338509
435.102706	25638.304432	30.343527
435.719884	25688.274302	30.348544
436.225240	25716.660160	30.353562
436.333178	25750.227484	30.358580
436.387431	25784.719671	30.363597
437.111887	25829.174700	30.368615
437.511331	25864.428235	30.373632
437.971576	25902.946081	30.378650
438.723688	25940.293319	30.383668
438.765465	26001.237190	30.388685
439.462396	26025.586563	30.393703
439.662365	26068.070248	30.398720
440.152674	26112.436174	30.403738
440.740841	26145.284287	30.408756
440.986326	26195.048184	30.413773
441.630753	26235.749856	30.418791
442.220353	26269.596526	30.423808
442.249350	26313.055525	30.428826
443.256745	26354.547485	30.433844
443.295465	26404.262119	30.438861
443.988378	26439.894145	30.443879
444.465980	26466.648474	30.448896
444.707164	26506.175090	30.453914
445.254121	26540.939005	30.458932
445.869001	26594.716249	30.463949
446.686639	26626.802375	30.468967
446.816201	26662.756879	30.473984
447.132877	26707.663245	30.479002
447.712364	26731.355595	30.484020
447.795863	26779.547268	30.489037
448.166643	26817.771172	30.494055
448.781322	26848.195596	30.499072
448.961845	26895.108282	30.504090
449.820939	26931.056441	30.509108
450.058497	26975.065661	30.514125
450.519119	27002.398511	30.519143
451.014374	27038.005664	30.524160
451.195542	27079.135530	30.529178
451.678844	27108.664466	30.534196
452.374380	27155.819428	30.539213
452.546737	27188.443622	30.544231
452.896139	27224.036022	30.549248
453.006680	27266.555184	30.554266
453.782348	27317.957953	30.559284
454.536194	27358.821715	30.564301
454.700307	27401.509740	30.569319
454.808328	27433.436508	30.574336
455.282726	27475.437719	30.579354
456.190389	27519.905686	30.584372
456.682926	27569.975564	30.589389
456.973151	27612.770690	30.594407
457.675690	27656.455732	30.599424
457.674161	27699.498995	30.604442
458.552192	27746.064210	30.609460
458.865792	27799.948716	30.614477
459.099200	27828.936341	30.619495
459.776233	27875.242584	30.624512
460.406959	27923.344929	30.629530
460.939492	27962.417898	30.634548
461.381831	28009.450157	30.639565
461.724207	28046.492530	30.644583
462.250857	28084.915623	30.649600
462.454684	28133.445607	30.654618
463.082651	28171.448469	30.659636
463.356442	28223.570523	30.664653
464.095931	28265.380142	30.669671
464.434893	28302.404551	30.674688
464.791985	28363.362990	30.679706
465.257553	28407.440720	30.684724
465.789950	28461.381190	30.689741
466.845408	28493.976606	30.694759
467.425355	28544.509244	30.699776
467.612609	28584.212677	30.704794
468.104407	28616.757514	30.709812
468.527208	28660.273609	30.714829
469.187696	28697.968954	30.719847
469.411107	28740.764263	30.724864
469.922119	28781.163235	30.729882
470.597896	28821.492234	30.734900
470.949400	28877.585965	30.739917
471.689258	28914.649824	30.744935
472.130777	28948.593674	30.749952
472.345334	29000.107525	30.754970
472.962194	29032.974769	30.759988
473.147514	29079.771618	30.765005
473.909214	29120.081426	30.770023
474.470039	29161.560561	30.775040
474.457997	29204.640234	30.780058
475.297251	29232.093756	30.785076
475.812341	29273.580280	30.790093
475.680605	29318.050610	30.795111
476.943420	29365.128143	30.800128
477.254265	29411.950335	30.805146
477.475611	29453.969956	30.810164
477.928112	29501.111505	30.815181
478.519401	29549.811711	30.820199
478.905035	29582.235642	30.825216
479.115202	29631.836450	30.830234
479.366039	29670.792446	30.835252
480.413910	29725.572073	30.840269
480.389089	29770.001346	30.845287
480.663845	29814.251047	30.850304
481.573580	29867.680981	30.855322
481.838431	29912.463429	30.860340
482.513348	29958.028799	30.865357
483.031931	30010.780778	30.870375
483.704820	30037.275312	30.875392
483.722830	30085.162627	30.880410
484.539536	30122.235592	30.885428
485.160162	30167.361114	30.890445
485.290747	30213.113444	30.895463
486.176342	30256.598358	30.900480
486.158340	30300.673707	30.905498
486.741631	30348.498380	30.910516
487.385016	30386.041464	30.915533
487.753541	30436.011327	30.920551
488.513655	30480.470900	30.925568
488.455476	30535.704056	30.930586
488.905115	30574.700154	30.935604
489.707779	30630.904992	30.940621
489.994135	30674.263388	30.945639
490.857463	30724.409309	30.950656
491.021720	30778.236505	30.955674
491.613954	30825.346547	30.960692
492.370270	30871.008647	30.965709
492.653728	30916.529976	30.970727
493.159688	30971.878225	30.975744
493.573722	31027.904788	30.980762
493.974481	31063.780270	30.985780
495.005060	31110.676909	30.990797
495.282298	31159.221481	30.995815
496.078593	31207.653263	31.000832
496.217952	31264.583230	31.005850
496.873210	31309.939720	31.010868
497.030420	31354.520884	31.015885
497.665424	31408.042079	31.020903
498.425111	31447.655038	31.025920
498.453813	31505.658724	31.030938
499.075504	31550.464683	31.035956
499.876464	31604.169008	31.040973
500.124937	31651.341086	31.045991
500.620080	31705.011385	31.051008
501.528980	31758.383112	31.056026
501.989278	31808.051099	31.061044
502.344249	31859.265589	31.066061
502.875399	31906.710064	31.071079
503.605785	31945.620512	31.076096
503.919282	32001.804525	31.081114
504.346585	32049.556398	31.086132
505.344709	32092.490176	31.091149
505.400299	32147.931057	31.096167
506.112274	32194.759927	31.101184
506.359621	32243.343316	31.106202
506.891511	32288.474703	31.111220
507.396766	32337.814488	31.116237
508.052489	32391.107370	31.121255
508.615338	32433.250230	31.126272
508.879344	32490.088153	31.131290
509.292676	32544.380340	31.136308
509.837084	32587.632761	31.141325
510.812171	32645.206893	31.146343
511.565917	32671.527756	31.151360
511.507616	32735.352169	31.156378
511.929818	32785.844000	31.161396
512.753786	32829.641094	31.166413
512.862520	32884.645695	31.171431
513.541711	32928.965123	31.176448
514.027687	32989.474432	31.181466
514.615415	33030.963413	31.186484
515.413747	33077.420368	31.191501
515.693015	33128.396933	31.196519
516.214756	33173.740452	31.201536
516.973620	33213.654040	31.206554
517.158013	33255.333081	31.211572
517.728115	33294.169988	31.216589
517.995438	33346.761136	31.221607
518.682665	33393.046523	31.226624
518.967501	33445.325381	31.231642
519.337252	33491.477361	31.236660
520.050987	33532.966566	31.241677
520.196170	33587.505765	31.246695
521.020075	33639.005215	31.251712
522.094816	33685.091460	31.256730
522.393244	33742.338338	31.261748
523.088629	33785.411521	31.266765
522.839988	33828.152140	31.271783
523.833322	33883.868016	31.276800
523.997639	33943.001570	31.281818
524.658585	33992.611696	31.286836
525.619473	34046.170789	31.291853
525.836230	34095.996145	31.296871
526.369726	34146.815230	31.301888
526.794320	34200.521935	31.306906
527.377836	34254.159629	31.311924
528.355264	34308.311121	31.316941
528.451011	34366.596727	31.321959
528.852602	34417.677382	31.326976
529.513747	34469.710164	31.331994
529.996863	34520.601266	31.337012
530.477284	34569.811082	31.342029
530.786600	34637.668122	31.347047
531.640212	34689.633365	31.352064
532.097122	34748.590570	31.357082
532.768417	34806.490078	31.362100
533.493587	34849.857938	31.367117
533.791151	34903.731748	31.372135
534.398032	34965.757903	31.377152
535.111992	35028.772794	31.382170
535.360197	35072.298009	31.387188
536.150480	35120.676545	31.392205
536.706403	35183.704004	31.397223
537.724078	35239.748434	31.402240
538.346025	35287.312774	31.407258
538.661640	35336.815744	31.412276
539.634167	35378.388181	31.417293
539.798739	35422.685962	31.422311
540.251569	35471.200347	31.427328
541.093063	35520.918563	31.432346
541.566600	35574.956203	31.437364
542.184834	35618.614273	31.442381
542.566488	35678.774569	31.447399
543.185998	35716.887371	31.452416
543.679171	35769.809582	31.457434
543.991313	35817.063216	31.462452
544.629446	35858.227384	31.467469
544.717565	35910.789738	31.472487
545.381743	35952.373655	31.477504
546.079283	36012.314696	31.482522
546.571533	36061.741103	31.487540
547.293016	36119.022988	31.492557
547.508476	36181.569259	31.497575
548.186313	36227.571454	31.502592
548.324017	36276.333046	31.507610
549.277906	36330.853812	31.512628
549.971231	36382.323478	31.517645
550.431788	36435.581255	31.522663
550.998843	36498.079710	31.527680
551.603095	36540.192665	31.532698
552.030336	36590.869837	31.537716
552.639675	36647.247505	31.542733
553.013819	36684.110516	31.547751
553.599578	36738.791152	31.552768
554.068345	36780.148031	31.557786
554.588469	36835.591670	31.562804
555.243721	36889.528300	31.567821
555.445814	36935.751967	31.572839
556.270141	36993.797865	31.577856
557.004928	37035.480331	31.582874
557.122702	37096.685044	31.587892
558.160813	37145.731267	31.592909
558.654051	37198.821416	31.597927
558.789949	37259.998462	31.602944
559.482684	37305.222857	31.607962
560.282804	37370.785863	31.612980
560.697170	37423.465246	31.617997
561.546743	37477.145274	31.623015
561.698070	37527.829932	31.628032
562.885726	37586.244209	31.633050
563.136227	37637.900070	31.638068
563.567825	37693.208024	31.643085
564.146517	37752.875345	31.648103
564.588022	37804.874785	31.653120
565.150039	37861.895421	31.658138
565.404877	37935.317306	31.663156
566.536930	37987.107858	31.668173
566.870530	38041.464531	31.673191
567.438734	38100.268110	31.678208
567.854057	38156.427180	31.683226
568.228292	38220.820025	31.688244
568.856560	38278.457437	31.693261
569.513983	38338.227876	31.698279
569.940748	38398.945232	31.703296
570.589510	38472.187096	31.708314
571.526398	38532.224171	31.713332
572.043978	38604.430948	31.718349
572.356390	38664.749585	31.723367
572.883977	38725.521630	31.728384
573.591038	38784.210467	31.733402
574.710642	38851.353188	31.738420
575.133674	38912.274935	31.743437
575.701926	38974.894229	31.748455
576.356611	39031.618862	31.753472
577.051794	39092.656593	31.758490
577.273406	39146.192489	31.763508
577.975992	39210.220653	31.768525
578.695112	39273.980807	31.773543
578.744466	39322.238233	31.778560
579.636192	39391.448344	31.783578
580.093790	39452.492676	31.788596
581.210818	39509.437058	31.793613
581.403976	39572.521566	31.798631
581.911081	39632.945211	31.803648
582.586008	39690.168003	31.808666
583.326822	39745.730013	31.813684
584.007830	39812.236091	31.818701
584.627473	39867.728851	31.823719
584.895243	39932.067560	31.828736
585.821217	39986.001152	31.833754
586.184173	40056.953151	31.838772
586.929802	40104.843970	31.843789
587.347646	40176.628894	31.848807
587.866431	40239.019253	31.853824
588.513269	40286.445294	31.858842
588.955405	40355.096448	31.863860
589.675264	40411.251604	31.868877
590.201789	40480.895514	31.873895
590.516086	40542.439673	31.878912
591.336719	40592.330983	31.883930
591.578292	40647.138653	31.888948
592.301499	40710.978268	31.893965
592.597546	40768.946272	31.898983
593.323104	40836.239055	31.904000
594.014530	40890.774498	31.909018
594.515644	40959.393013	31.914036
595.025954	41016.910698	31.919053
596.054485	41085.763238	31.924071
596.702875	41151.152727	31.929088
597.229059	41195.797840	31.934106
597.278057	41263.001828	31.939124
598.207542	41326.545298	31.944141
598.919129	41396.960044	31.949159
599.019429	41458.451744	31.954176
599.751845	41527.086408	31.959194
600.284035	41592.748399	31.964212
600.935853	41657.316644	31.969229
601.649027	41718.788986	31.974247
602.179238	41793.565871	31.979264
603.072736	41862.252251	31.984282
603.411982	41934.181735	31.989300
604.113733	41993.012856	31.994317
604.666272	42070.095750	31.999335
605.293828	42131.127262	32.004352
606.051348	42213.700177	32.009370
606.601686	42280.620033	32.014388
607.155171	42336.104106	32.019405
607.587411	42410.278581	32.024423
608.049727	42486.472589	32.029440
609.182258	42543.194745	32.034458
609.467597	42629.068910	32.039476
610.238812	42695.006676	32.044493
610.854338	42763.201768	32.049511
611.394354	42836.431010	32.054528
612.180547	42900.298741	32.059546
613.005742	42980.922118	32.064564
613.306989	43051.286232	32.069581
614.031733	43106.011700	32.074599
614.296533	43183.459795	32.079616
615.200103	43245.842698	32.084634
616.088426	43320.720471	32.089652
616.521906	43397.605253	32.094669
617.274943	43460.727087	32.099687
617.960384	43534.707542	32.104704
618.811863	43596.688447	32.109722
619.204204	43663.896563	32.114740
619.524319	43742.210836	32.119757
620.334912	43806.014100	32.124775
621.137329	43874.170687	32.129792
622.012110	43935.029294	32.134810
622.761402	44001.828307	32.139828
623.250960	44071.426085	32.144845
623.984415	44133.464922	32.149863
624.513991	44201.715844	32.154880
624.864712	44256.142168	32.159898
625.887462	44329.819420	32.164916
626.308452	44394.431795	32.169933
626.930365	44458.968611	32.174951
627.343110	44538.359166	32.179968
628.029100	44589.235758	32.184986
628.972396	44651.413964	32.190004
629.758445	44723.440650	32.195021
629.921333	44779.004646	32.200039
630.818402	44854.759144	32.205056
631.471042	44919.621413	32.210074
632.064735	44990.464554	32.215092
632.741540	45044.525444	32.220109
633.290302	45099.112576	32.225127
633.565037	45158.468083	32.230144
634.342621	45228.169846	32.235162
635.062616	45282.698980	32.240180
635.445842	45342.480787	32.245197
636.188775	45403.028775	32.250215
636.683558	45465.254178	32.255232
637.641727	45535.940750	32.260250
637.847123	45605.132337	32.265268
638.259290	45668.579481	32.270285
639.113102	45727.586442	32.275303
639.991422	45795.477636	32.280320
640.493028	45866.590999	32.285338
641.123524	45935.501946	32.290356
641.503016	46007.710291	32.295373
642.228711	46071.052535	32.300391
642.753885	46155.719734	32.305408
643.579162	46226.815175	32.310426
644.105978	46306.921610	32.315444
644.368988	46380.756210	32.320461
645.274758	46454.047565	32.325479
645.692694	46533.222937	32.330496
646.261779	46604.492537	32.335514
647.412990	46680.934568	32.340532
647.978752	46762.934369	32.345549
648.777218	46834.738129	32.350567
648.873776	46921.366856	32.355584
650.004381	46978.802795	32.360602
650.684089	47066.859053	32.365620
651.265588	47145.068334	32.370637
651.872745	47218.921361	32.375655
652.555622	47309.660423	32.380672
653.444669	47384.317573	32.385690
654.125161	47459.254357	32.390708
654.520610	47530.484470	32.395725
655.509364	47608.163414	32.400743
656.131271	47690.714501	32.405760
656.666335	47757.830250	32.410778
657.305589	47825.638446	32.415796
657.727332	47907.335956	32.420813
658.415615	47987.524263	32.425831
659.302173	48070.003646	32.430848
659.902879	48148.238675	32.435866
660.794178	48230.901368	32.440884
661.318265	48312.710835	32.445901
662.208727	48380.120723	32.450919
662.787149	48466.274958	32.455936
663.245277	48526.907536	32.460954
664.263084	48607.476630	32.465972
664.990438	48690.843620	32.470989
665.588645	48751.170153	32.476007
666.220662	48839.949327	32.481024
666.788478	48907.670695	32.486042
667.778518	48987.201556	32.491060
668.004904	49068.313781	32.496077
668.950374	49128.276910	32.501095
669.487492	49212.592981	32.506112
670.230600	49282.293623	32.511130
670.698808	49369.126508	32.516148
671.122542	49447.336748	32.521165
671.969923	49518.445336	32.526183
672.638028	49600.072343	32.531200
673.240401	49679.780198	32.536218
674.688412	49758.913009	32.541236
675.101585	49836.392291	32.546253
675.708988	49899.409393	32.551271
676.254583	49977.108838	32.556288
676.989339	50058.638453	32.561306
677.717760	50126.249681	32.566324
678.259403	50197.927071	32.571341
678.807000	50256.196506	32.576359
679.648684	50340.487993	32.581376
680.463230	50404.859689	32.586394
680.558583	50468.641870	32.591412
681.142670	50546.590292	32.596429
682.277368	50618.543093	32.601447
682.666612	50700.382170	32.606464
683.313287	50778.840409	32.611482
684.183363	50850.354497	32.616500
684.605601	50933.125672	32.621517
685.129309	51011.331879	32.626535
685.666180	51092.383611	32.631552
686.849853	51176.675205	32.636570
687.389979	51262.807930	32.641588
687.663457	51344.585151	32.646605
688.752181	51419.565835	32.651623
689.357243	51505.588050	32.656640
690.052250	51598.094860	32.661658
690.812932	51670.565080	32.666676
691.138774	51764.079492	32.671693
691.976481	51839.069200	32.676711
692.552936	51931.500985	32.681728
693.540230	52017.022298	32.686746
694.318606	52109.467462	32.691764
694.861444	52193.869425	32.696781
695.843513	52279.569693	32.701799
696.443045	52373.056340	32.706816
697.446247	52452.755246	32.711834
698.022960	52540.203131	32.716852
698.589932	52619.040735	32.721869
699.452021	52703.457820	32.726887
700.278135	52790.987814	32.731904
700.722972	52876.470663	32.736922
701.545340	52950.485520	32.741940
702.098572	53045.671646	32.746957
703.017640	53127.480563	32.751975
703.895409	53215.541926	32.756992
704.307980	53293.722557	32.762010
705.185637	53376.874031	32.767028
706.015626	53461.640582	32.772045
706.700501	53543.228172	32.777063
707.270710	53634.522275	32.782080
707.935332	53716.303478	32.787098
708.681745	53802.020900	32.792116
709.172501	53887.721716	32.797133
710.315346	53981.268898	32.802151
710.646128	54061.977165	32.807168
711.558606	54144.828472	32.812186
712.411653	54230.726927	32.817204
712.989142	54319.079910	32.822221
713.721159	54393.094466	32.827239
714.503842	54494.262368	32.832256
714.990198	54577.643887	32.837274
715.947879	54660.648130	32.842292
716.321356	54746.079317	32.847309
717.339862	54831.213621	32.852327
718.239601	54931.244933	32.857344
718.634367	55018.078673	32.862362
719.296151	55098.757622	32.867380
719.587317	55198.461352	32.872397
720.847113	55282.819057	32.877415
721.504041	55365.290639	32.882432
722.041339	55454.078152	32.887450
723.036494	55544.794128	32.892468
723.416779	55632.727222	32.897485
724.419781	55723.854010	32.902503
725.362364	55807.339269	32.907520
725.834278	55882.772514	32.912538
726.461776	55963.434445	32.917556
727.288050	56041.673268	32.922573
727.939840	56123.528063	32.927591
728.753903	56206.895613	32.932608
729.138273	56294.836832	32.937626
729.905718	56380.712156	32.942644
730.485372	56469.572756	32.947661
731.204910	56539.729028	32.952679
732.158751	56638.309722	32.957696
732.336171	56727.443117	32.962714
733.427466	56807.902358	32.967732
733.797795	56913.220916	32.972749
734.642844	57006.105123	32.977767
735.367977	57103.717236	32.982784
735.686474	57201.374435	32.987802
736.465947	57298.004158	32.992820
737.216538	57408.214645	32.997837
737.883763	57503.464044	33.002855
738.707963	57606.980388	33.007872
739.470697	57716.519495	33.012890
740.784470	57799.175074	33.017908
741.715758	57903.707576	33.022925
742.358585	58003.810939	33.027943
742.981211	58096.696202	33.032960
743.525965	58205.246319	33.037978
744.712585	58290.626093	33.042996
745.730120	58387.678605	33.048013
746.195122	58485.197791	33.053031
746.852540	58585.756986	33.058048
747.792005	58686.443325	33.063066
748.536692	58779.596913	33.068084
749.375445	58889.933259	33.073101
750.621844	58967.603107	33.078119
751.312370	59065.481733	33.083136
751.859321	59158.319613	33.088154
752.633604	59239.729058	33.093172
753.229812	59341.756759	33.098189
754.202492	59440.656077	33.103207
754.792210	59526.285576	33.108224
755.427151	59623.592822	33.113242
755.913788	59715.011764	33.118260
756.985364	59816.530262	33.123277
757.826526	59919.338548	33.128295
758.414714	60016.205267	33.133312
759.146501	60112.935945	33.138330
760.135671	60202.948763	33.143348
760.792610	60306.502790	33.148365
761.443828	60411.634282	33.153383
762.282070	60492.006115	33.158400
762.928673	60600.373703	33.163418
764.047774	60695.748399	33.168436
764.668440	60795.499552	33.173453
765.249263	60887.832288	33.178471
766.302418	60978.673487	33.183488
766.638182	61080.109876	33.188506
767.879047	61176.594113	33.193524
768.170684	61282.184424	33.198541
769.032622	61381.311470	33.203559
770.354849	61481.601211	33.208576
770.681350	61586.560680	33.213594
771.770158	61673.961585	33.218612
771.993483	61769.860518	33.223629
772.929103	61878.289744	33.228647
773.729958	61985.480827	33.233664
774.293818	62081.333970	33.238682
775.278750	62176.558151	33.243700
775.905328	62270.142284	33.248717
776.613274	62358.915622	33.253735
777.413583	62452.644158	33.258752
778.102502	62554.164219	33.263770
778.851733	62652.649307	33.268788
779.994920	62741.678709	33.273805
780.560996	62840.864249	33.278823
781.239994	62935.214993	33.283840
781.887156	63034.451911	33.288858
782.855792	63137.032056	33.293876
783.496832	63233.504275	33.298893
784.199898	63343.685559	33.303911
785.003165	63431.137356	33.308928
785.667729	63548.384215	33.313946
786.327709	63639.182769	33.318964
787.318325	63745.060250	33.323981
787.831672	63849.759428	33.328999
788.475979	63958.616835	33.334016
789.451954	64082.641983	33.339034
790.791349	64186.662438	33.344052
791.366038	64290.581490	33.349069
791.314049	64404.576546	33.354087
792.665154	64508.381249	33.359104
793.454048	64624.227196	33.364122
794.484236	64735.585232	33.369140
795.552602	64847.849443	33.374157
796.314389	64953.989430	33.379175
797.333774	65069.389813	33.384192
797.729976	65180.975710	33.389210
798.434274	65282.371451	33.394228
799.559061	65394.717892	33.399245
800.637093	65504.020542	33.404263
801.097917	65604.404728	33.409280
802.268701	65717.922997	33.414298
802.767747	65819.125102	33.419316
803.561171	65923.428143	33.424333
804.161870	66035.498608	33.429351
805.533969	66142.143143	33.434368
806.204244	66252.848772	33.439386
807.184227	66359.182069	33.444404
808.158477	66469.695420	33.449421
808.751256	66574.032546	33.454439
809.633635	66691.044605	33.459456
810.293565	66792.427990	33.464474
811.171065	66895.607508	33.469492
812.122560	67002.315172	33.474509
812.771046	67111.153806	33.479527
813.858551	67215.833964	33.484544
814.094320	67317.444136	33.489562
815.426349	67433.559743	33.494580
816.020371	67534.601815	33.499597
816.350876	67649.336633	33.504615
817.515871	67747.592843	33.509632
818.736992	67872.680826	33.514650
819.308187	67982.915574	33.519668
820.407891	68090.750605	33.524685
820.935202	68194.762658	33.529703
822.129818	68294.358662	33.534720
822.707834	68397.413817	33.539738
823.213352	68512.834242	33.544756
824.399190	68627.439480	33.549773
825.271651	68739.979427	33.554791
825.960950	68838.972807	33.559808
826.778201	68948.628599	33.564826
827.898764	69060.763837	33.569844
828.694272	69160.267371	33.574861
829.316692	69266.845983	33.579879
829.935168	69374.020866	33.584896
830.897599	69476.659191	33.589914
831.731591	69574.771553	33.594932
832.679620	69668.028653	33.599949
833.486615	69766.063645	33.604967
834.023764	69866.363868	33.609984
834.355095	69976.087417	33.615002
835.709680	70089.032634	33.620020
836.754746	70191.299897	33.625037
837.623328	70296.267435	33.630055
838.590651	70398.218401	33.635072
839.053421	70499.210261	33.640090
839.761747	70613.918022	33.645108
840.803314	70720.227971	33.650125
841.309252	70834.917730	33.655143
842.261383	70942.395091	33.660160
842.984071	71053.733649	33.665178
844.118063	71161.968662	33.670196
845.009513	71275.789418	33.675213
845.506538	71385.150962	33.680231
846.522280	71497.243416	33.685248
847.159371	71617.108789	33.690266
847.805536	71725.701142	33.695284
848.680404	71840.096871	33.700301
849.559731	71973.059935	33.705319
850.584146	72088.889852	33.710336
851.250379	72207.170151	33.715354
852.134284	72318.982763	33.720372
853.266331	72438.951679	33.725389
853.681171	72556.462298	33.730407
854.880542	72674.889187	33.735424
855.766438	72808.944675	33.740442
856.475738	72935.150296	33.745460
857.376935	73051.497680	33.750477
858.372115	73188.109156	33.755495
859.439000	73308.826832	33.760512
860.418981	73428.203386	33.765530
860.851428	73546.171596	33.770548
862.100837	73662.074469	33.775565
862.409384	73785.712285	33.780583
863.849598	73902.130974	33.785600
864.290519	74028.928442	33.790618
865.167251	74164.664141	33.795636
866.085884	74277.999512	33.800653
867.139939	74407.299404	33.805671
868.091053	74527.394709	33.810688
868.973301	74647.412665	33.815706
869.570458	74773.467180	33.820724
870.642803	74896.711844	33.825741
871.189416	75028.982217	33.830759
872.648507	75141.704592	33.835776
873.773770	75270.351464	33.840794
874.135761	75403.501268	33.845812
875.317252	75515.457978	33.850829
876.313229	75651.537174	33.855847
877.138807	75770.340279	33.860864
877.871897	75885.636878	33.865882
878.512681	76006.509387	33.870900
879.239575	76122.618672	33.875917
880.360488	76247.597319	33.880935
881.614707	76367.894019	33.885952
882.806648	76494.686803	33.890970
883.249328	76611.628067	33.895988
884.411445	76724.238844	33.901005
885.154408	76852.484369	33.906023
886.191318	76981.951251	33.911040
887.036255	77085.745722	33.916058
887.601760	77205.672577	33.921076
889.109945	77314.937946	33.926093
889.806284	77439.000428	33.931111
890.386745	77538.480228	33.936128
891.268660	77652.950236	33.941146
891.926850	77761.438372	33.946164
893.169127	77866.706433	33.951181
893.853675	77980.461283	33.956199
894.692315	78095.636664	33.961216
896.008831	78206.189757	33.966234
896.394214	78322.285835	33.971252
897.383824	78425.391290	33.976269
898.220731	78548.359942	33.981287
899.277094	78669.989915	33.986304
900.180607	78795.457617	33.991322
900.809137	78906.222586	33.996340
901.788493	79032.034207	34.001357
902.706225	79150.558818	34.006375
903.594412	79269.785349	34.011392
904.718975	79395.930612	34.016410
905.081393	79521.068244	34.021428
906.214235	79645.274990	34.026445
906.932066	79778.884386	34.031463
908.169485	79896.221903	34.036480
908.925527	80016.979952	34.041498
909.800906	80146.854369	34.046516
910.524937	80273.674444	34.051533
911.492094	80418.409525	34.056551
912.422638	80537.178745	34.061568
913.485910	80667.064165	34.066586
914.240084	80801.052838	34.071604
915.611859	80926.773554	34.076621
916.529249	81065.881795	34.081639
917.058796	81187.491211	34.086656
918.377540	81316.250036	34.091674
919.134131	81447.593427	34.096692
920.285795	81574.276398	34.101709
921.023799	81710.172415	34.106727
922.074837	81838.430732	34.111744
922.768316	81964.617044	34.116762
923.875046	82097.897836	34.121780
924.767745	82227.639774	34.126797
925.572479	82359.385307	34.131815
926.562031	82490.418318	34.136832
927.703483	82621.301446	34.141850
928.699533	82752.676748	34.146868
929.726878	82880.740762	34.151885
930.240670	83019.769752	34.156903
931.515566	83159.111052	34.161920
932.497353	83287.703522	34.166938
933.401006	83406.362293	34.171956
934.192526	83541.853223	34.176973
934.910446	83671.223637	34.181991
936.069183	83816.604973	34.187008
937.285851	83941.919858	34.192026
937.789650	84074.353971	34.197044
938.811883	84203.299006	34.202061
939.989305	84348.299977	34.207079
941.039886	84466.103833	34.212096
942.026611	84599.529130	34.217114
942.681059	84728.344032	34.222132
943.978104	84859.643852	34.227149
944.929705	84992.480911	34.232167
945.800313	85118.514013	34.237184
946.524652	85243.303412	34.242202
947.612651	85378.693206	34.247220
948.885653	85504.031402	34.252237
949.579980	85636.899026	34.257255
950.243530	85766.895589	34.262272
951.623683	85891.445703	34.267290
952.304888	86011.062389	34.272308
953.288120	86133.559487	34.277325
953.973275	86260.323532	34.282343
954.979901	86379.434586	34.287360
955.682667	86506.640464	34.292378
956.730549	86637.759235	34.297396
957.416874	86763.067983	34.302413
958.718481	86891.043479	34.307431
959.510403	87028.109336	34.312448
960.348019	87154.980107	34.317466
961.173636	87290.394507	34.322484
962.031498	87418.885315	34.327501
963.116308	87559.126595	34.332519
963.974124	87698.897180	34.337536
965.274130	87829.741018	34.342554
965.723248	87976.774967	34.347572
966.719336	88112.800088	34.352589
967.993431	88257.273095	34.357607
968.908932	88405.440071	34.362624
969.714968	88545.729680	34.367642
970.500287	88690.091230	34.372660
971.527845	88834.111400	34.377677
972.942015	88981.594867	34.382695
973.794144	89127.253410	34.387712
974.716854	89264.068357	34.392730
975.919620	89419.862726	34.397748
976.864422	89564.925923	34.402765
977.886709	89704.097216	34.407783
978.517159	89851.542932	34.412800
979.776538	89995.975984	34.417818
980.443047	90150.362634	34.422836
981.845696	90290.959913	34.427853
982.559688	90444.478829	34.432871
983.251654	90596.519140	34.437888
984.869269	90741.989635	34.442906
985.890599	90908.085973	34.447924
986.777151	91046.460925	34.452941
988.062751	91181.960390	34.457959
989.150383	91328.048997	34.462976
990.067615	91478.132006	34.467994
991.254217	91620.923916	34.473012
992.312058	91762.190393	34.478029
993.455597	91907.360486	34.483047
994.277798	92050.781814	34.488064
995.297354	92195.617809	34.493082
996.332979	92339.691503	34.498100
997.377837	92478.631219	34.503117
998.490069	92613.872694	34.508135
999.264592	92757.317479	34.513152
1000.447101	92904.121248	34.518170
1001.220794	93045.805720	34.523188
1002.377386	93195.492128	34.528205
1003.395069	93333.856930	34.533223
1004.310952	93494.520964	34.538240
1005.438236	93623.807274	34.543258
1006.569622	93777.987436	34.548276
1007.276632	93923.767780	34.553293
1008.209913	94066.433298	34.558311
1009.297102	94215.805968	34.563328
1010.470497	94356.483232	34.568346
1011.356434	94502.783329	34.573364
1012.066611	94646.994826	34.578381
1013.268780	94797.188875	34.583399
1014.192591	94954.132628	34.588416
1015.532694	95094.026593	34.593434
1016.390622	95244.834426	34.598452
1017.395265	95386.670909	34.603469
1018.103660	95533.637431	34.608487
1019.060459	95668.485614	34.613504
1020.382386	95811.719401	34.618522
1021.010607	95948.901906	34.623540
1022.003869	96085.622225	34.628557
1023.274105	96224.429363	34.633575
1024.251719	96378.291532	34.638592
1025.318189	96503.555609	34.643610
1026.114799	96646.469804	34.648628
1026.895550	96801.340932	34.653645
1028.006198	96951.724423	34.658663
1028.946214	97102.629725	34.663680
1029.820645	97251.505092	34.668698
1030.874523	97412.763453	34.673716
1032.047527	97567.830447	34.678733
1032.935485	97716.325573	34.683751
1033.758190	97875.873088	34.688768
1034.627824	98031.813828	34.693786
1036.025978	98196.432330	34.698804
1036.874788	98350.641150	34.703821
1038.024423	98525.023493	34.708839
1038.925119	98682.052766	34.713856
1040.134521	98845.220934	34.718874
1041.306508	99008.890200	34.723892
1042.284585	99170.194649	34.728909
1043.089467	99328.522486	34.733927
1044.078388	99496.951549	34.738944
1045.163975	99657.709152	34.743962
1046.258498	99840.144776	34.748980
1047.058304	100006.514302	34.753997
1048.593466	100177.942052	34.759015
1049.656119	100342.509950	34.764032
1050.859360	100504.394328	34.769050
1051.835692	100670.587483	34.774068
1052.615379	100852.748457	34.779085
1053.898701	101011.808311	34.784103
1054.888064	101185.063700	34.789120
1056.393727	101354.169488	34.794138
1057.382899	101524.827683	34.799156
1058.604112	101693.852973	34.804173
1059.613771	101858.804469	34.809191
1060.554682	102021.586869	34.814208
1061.921225	102190.097497	34.819226
1063.030477	102357.901233	34.824244
1064.018237	102524.583768	34.829261
1065.334108	102687.906642	34.834279
1066.226974	102856.152498	34.839296
1067.147653	103019.069761	34.844314
1068.089454	103182.732567	34.849332
1069.364973	103363.637973	34.854349
1070.545751	103521.724344	34.859367
1071.721694	103687.774659	34.864384
1072.778117	103853.907906	34.869402
1074.028668	104022.927794	34.874420
1075.005076	104189.658475	34.879437
1076.112878	104352.362757	34.884455
1076.961022	104512.166868	34.889472
1078.148168	104688.135638	34.894490
1079.398389	104848.005188	34.899508
1080.077052	105011.971713	34.904525
1081.645004	105179.857280	34.909543
1082.541467	105350.536898	34.914560
1083.450058	105509.436007	34.919578
1084.829048	105677.049309	34.924596
1085.456975	105849.688125	34.929613
1086.278329	106016.743730	34.934631
1087.463357	106181.600302	34.939648
1088.605508	106362.593396	34.944666
1089.605429	106528.888109	34.949684
1090.863539	106689.906300	34.954701
1091.822168	106841.664849	34.959719
1092.700135	107014.625448	34.964736
1093.991138	107172.660888	34.969754
1095.263128	107338.650643	34.974772
1095.929820	107506.054729	34.979789
1097.029763	107667.977213	34.984807
1098.050698	107843.924875	34.989824
1099.325729	108011.629268	34.994842
1100.466814	108172.127437	34.999860
1101.418631	108350.941653	35.004877
1102.342527	108517.257852	35.009895
1103.489550	108685.264516	35.014912
1104.744657	108858.504986	35.019930
1105.937164	109035.306802	35.024948
1106.597915	109218.977143	35.029965
1107.919024	109387.936375	35.034983
1109.104230	109577.233005	35.040000
1110.468115	109750.955427	35.045018
1111.722264	109933.090938	35.050036
1112.645259	110097.880339	35.055053
1113.667386	110278.937995	35.060071
1115.143255	110455.322146	35.065088
1115.858056	110641.882832	35.070106
1117.480273	110823.102957	35.075124
1118.380081	111004.665373	35.080141
1119.417493	111166.398214	35.085159
1120.895231	111354.187467	35.090176
1121.909510	111532.982691	35.095194
1123.236393	111705.667884	35.100212
1124.274087	111887.961443	35.105229
1125.351637	112063.642311	35.110247
1126.391484	112234.345849	35.115264
1127.499963	112425.153469	35.120282
1129.129632	112600.712478	35.125300
1129.814984	112787.390416	35.130317
1130.903203	112958.140537	35.135335
1132.072707	113150.350183	35.140352
1133.084064	113336.409201	35.145370
1134.567130	113514.202357	35.150388
1135.415854	113699.654564	35.155405
1136.795557	113881.701710	35.160423
1137.887587	114073.294222	35.165440
1138.974584	114243.581302	35.170458
1139.980855	114426.564740	35.175476
1141.111551	114628.148251	35.180493
1142.421619	114800.787400	35.185511
1143.713086	114986.569984	35.190528
1144.648904	115184.534309	35.195546
1145.831715	115361.495607	35.200564
1147.054669	115556.220792	35.205581
1148.436679	115738.137250	35.210599
1149.695549	115925.565808	35.215616
1150.430849	116110.984497	35.220634
1151.785365	116287.314519	35.225652
1152.530936	116478.009787	35.230669
1154.239894	116670.457765	35.235687
1155.629423	116850.780330	35.240704
1156.595888	117037.461166	35.245722
1157.878535	117220.021905	35.250740
1158.506555	117410.232957	35.255757
1159.696678	117590.818597	35.260775
1161.339652	117787.658607	35.265792
1162.368101	117972.989858	35.270810
1163.887168	118152.372426	35.275828
1164.700234	118336.762489	35.280845
1166.175394	118518.855408	35.285863
1167.402143	118693.377461	35.290880
1168.173827	118858.217222	35.295898
1169.314536	119029.824178	35.300916
1170.620437	119209.067507	35.305933
1172.066665	119382.467474	35.310951
1172.848725	119550.251415	35.315968
1173.805844	119719.695750	35.320986
1174.999030	119892.211643	35.326004
1175.783739	120077.946421	35.331021
1177.012701	120257.637960	35.336039
1178.353281	120434.725130	35.341056
1179.466289	120613.700744	35.346074
1180.545544	120799.989065	35.351092
1181.480035	120982.520771	35.356109
1182.661442	121169.670141	35.361127
1183.689105	121368.438793	35.366144
1185.198189	121561.272474	35.371162
1186.264038	121751.652100	35.376180
1187.420269	121944.060855	35.381197
1188.471558	122133.911821	35.386215
1189.666574	122332.215156	35.391232
1190.422093	122530.017433	35.396250
1192.139805	122732.782405	35.401268
1193.199420	122936.146179	35.406285
1194.601392	123133.913695	35.411303
1195.769517	123330.602444	35.416320
1196.843365	123543.392699	35.421338
1198.152451	123736.458570	35.426356
1199.137860	123943.797128	35.431373
1200.765702	124147.547498	35.436391
1202.108899	124349.009198	35.441408
1203.479764	124557.952472	35.446426
1204.774089	124746.661425	35.451444
1205.753417	124957.634436	35.456461
1207.004829	125148.331054	35.461479
1207.941573	125358.475508	35.466496
1209.039440	125563.812981	35.471514
1210.390445	125766.130498	35.476532
1211.681415	125977.998819	35.481549
1212.922466	126192.083549	35.486567
1214.141604	126398.395791	35.491584
1215.046595	126605.024669	35.496602
1216.585663	126810.261251	35.501620
1217.460155	127021.565790	35.506637
1218.552036	127228.244649	35.511655
1219.896433	127446.937807	35.516672
1221.222828	127662.082510	35.521690
1222.739601	127873.303522	35.526708
1223.915243	128088.029963	35.531725
1225.254852	128293.152837	35.536743
1226.841675	128507.157313	35.541760
1228.067473	128717.984069	35.546778
1229.407813	128915.687650	35.551796
1230.432305	129130.823704	35.556813
1231.751529	129330.359554	35.561831
1233.112707	129535.053705	35.566848
1234.578107	129748.563272	35.571866
1235.490056	129947.518693	35.576884
1236.811024	130147.514866	35.581901
1238.556774	130360.920170	35.586919
1240.047415	130558.024203	35.591936
1240.727679	130763.972758	35.596954
1242.291282	130959.734954	35.601972
1243.360564	131167.616588	35.606989
1244.425545	131360.451533	35.612007
1245.988029	131550.773287	35.617024
1247.082719	131765.962323	35.622042
1248.509573	131951.828043	35.627060
1249.807460	132163.332944	35.632077
1250.544051	132344.474046	35.637095
1251.941981	132527.580623	35.642112
1252.976505	132727.227504	35.647130
1254.613194	132912.125486	35.652148
1255.704135	133093.620246	35.657165
1256.690142	133285.372108	35.662183
1258.197862	133490.785258	35.667200
1259.265441	133679.899447	35.672218
1260.545162	133872.826014	35.677236
1261.709912	134072.420508	35.682253
1262.750036	134261.414571	35.687271
1264.175633	134464.243787	35.692288
1265.001358	134681.075275	35.697306
1266.763844	134873.181918	35.702324
1267.879021	135079.069874	35.707341
1268.843932	135285.185322	35.712359
1270.362588	135484.857584	35.717376
1271.510380	135701.288248	35.722394
1272.835533	135907.654683	35.727412
1274.075813	136128.032061	35.732429
1275.213633	136333.046569	35.737447
1276.517444	136543.429176	35.742464
1277.499653	136762.809443	35.747482
1278.975672	136979.918099	35.752500
1279.814514	137196.480329	35.757517
1281.209843	137413.222954	35.762535
1283.308865	137640.401915	35.767552
1283.871270	137860.830241	35.772570
1285.264151	138076.078902	35.777588
1286.602693	138301.489286	35.782605
1288.254326	138531.128391	35.787623
1289.592578	138748.558743	35.792640
1290.494003	138968.292000	35.797658
1292.345255	139189.057817	35.802676
1293.640344	139411.548808	35.807693
1294.818823	139624.579188	35.812711
1296.179636	139845.183708	35.817728
1297.503115	140074.209065	35.822746
1299.256778	140308.269890	35.827764
1300.492561	140504.023021	35.832781
1301.302248	140732.637006	35.837799
1303.133557	140958.655486	35.842816
1304.154308	141177.428403	35.847834
1305.500166	141402.268531	35.852852
1306.778217	141623.744464	35.857869
1308.223982	141847.631867	35.862887
1309.536585	142067.606843	35.867904
1311.120109	142299.622554	35.872922
1312.475697	142514.148221	35.877940
1314.230852	142728.739192	35.882957
1315.141491	142951.826994	35.887975
1316.773935	143173.470201	35.892992
1318.049232	143387.276116	35.898010
1319.625648	143589.334092	35.903028
1320.775408	143801.625744	35.908045
1322.101536	144033.042587	35.913063
1323.804172	144241.391258	35.918080
1324.384033	144455.602509	35.923098
1325.889872	144660.772674	35.928116
1327.499749	144878.682841	35.933133
1328.534211	145100.022024	35.938151
1329.894885	145308.948999	35.943168
1331.229678	145533.504928	35.948186
1332.609359	145754.386767	35.953204
1334.141398	145962.388444	35.958221
1335.373829	146176.530173	35.963239
1336.687180	146390.253970	35.968256
1337.822633	146608.144228	35.973274
1339.123335	146802.008067	35.978292
1340.653616	147001.586405	35.983309
1341.620398	147215.977094	35.988327
1343.191295	147416.147214	35.993344
1344.119042	147617.814964	35.998362
1345.502305	147821.404944	36.003380
1346.788877	148029.009070	36.008397
1348.050890	148250.453031	36.013415
1349.474544	148460.271331	36.018432
1350.586124	148676.574621	36.023450
1351.846123	148890.050411	36.028468
1353.252851	149111.399151	36.033485
1354.286922	149338.138231	36.038503
1356.200778	149549.953058	36.043520
1356.953430	149773.513970	36.048538
1358.509240	149997.242034	36.053556
1359.744064	150226.314368	36.058573
1361.097280	150463.556343	36.063591
1362.472980	150696.315062	36.068608
1363.636668	150922.215413	36.073626
1365.015011	151152.741612	36.078644
1366.681303	151387.679145	36.083661
1367.649857	151647.035165	36.088679
1369.240981	151869.204040	36.093696
1370.547708	152110.458901	36.098714
1372.018911	152357.705914	36.103732
1373.332099	152583.500787	36.108749
1374.760235	152839.439249	36.113767
1376.207539	153081.602945	36.118784
1377.401699	153319.072442	36.123802
1378.628084	153568.736873	36.128820
1380.386791	153816.706927	36.133837
1381.392226	154064.884823	36.138855
1382.957955	154305.372260	36.143872
1384.464394	154557.269439	36.148890
1386.378343	154803.556513	36.153908
1387.883968	155045.084685	36.158925
1389.127682	155297.267403	36.163943
1390.609619	155531.540088	36.168960
1391.687411	155783.662017	36.173978
1393.629130	156021.063718	36.178996
1395.212780	156263.816089	36.184013
1396.068790	156513.944716	36.189031
1398.134482	156750.631737	36.194048
1399.251050	156995.478678	36.199066
1400.832485	157235.010888	36.204084
1402.161150	157474.634399	36.209101
1403.710680	157726.792296	36.214119
1405.329082	157957.917542	36.219136
1406.755004	158200.727854	36.224154
1408.047470	158441.363772	36.229172
1409.550167	158675.340864	36.234189
1411.112478	158926.181442	36.239207
1412.519494	159161.254457	36.244224
1413.838978	159407.361589	36.249242
1415.203756	159633.086573	36.254260
1416.633110	159872.208608	36.259277
1417.370138	160120.250563	36.264295
1418.921815	160359.774267	36.269312
1420.559280	160596.543221	36.274330
1422.014926	160845.605464	36.279348
1423.493256	161084.635579	36.284365
1424.849143	161333.461440	36.289383
1426.762908	161572.806106	36.294400
1427.909757	161815.598001	36.299418
1429.454689	162066.212618	36.304436
1431.083873	162305.528382	36.309453
1432.434722	162540.863986	36.314471
1433.722655	162764.682347	36.319488
1434.908565	162988.872932	36.324506
1436.243901	163213.523347	36.329524
1437.982172	163439.774652	36.334541
1439.041840	163664.152350	36.339559
1439.986019	163905.917272	36.344576
1441.396220	164133.796627	36.349594
1442.902096	164371.463313	36.354612
1444.228069	164608.930467	36.359629
1445.763651	164854.846828	36.364647
1447.344316	165101.925099	36.369664
1448.453974	165342.717064	36.374682
1449.939048	165587.653666	36.379700
1451.910550	165836.958805	36.384717
1453.003826	166092.915664	36.389735
1454.146340	166340.854182	36.394752
1455.425749	166592.378023	36.399770
1457.047965	166846.972516	36.404788
1458.672068	167097.390401	36.409805
1459.760712	167358.824960	36.414823
1461.332998	167622.482926	36.419840
1462.709964	167882.287186	36.424858
1464.070997	168148.570345	36.429876
1466.038897	168413.146992	36.434893
1467.198309	168680.441358	36.439911
1468.827294	168946.266537	36.444928
1470.511779	169216.553405	36.449946
1471.888818	169479.804356	36.454964
1473.273473	169734.306657	36.459981
1474.929085	170012.892294	36.464999
1476.171884	170273.335602	36.470016
1477.992398	170546.945477	36.475034
1479.661584	170814.409089	36.480052
1480.905151	171073.813883	36.485069
1482.519969	171344.106731	36.490087
1484.133193	171619.771867	36.495104
1485.793230	171887.989873	36.500122
1487.335702	172150.576762	36.505140
1489.201415	172424.046680	36.510157
1490.005271	172683.398796	36.515175
1491.583116	172952.420635	36.520192
1493.209577	173224.178525	36.525210
1494.307940	173504.959319	36.530228
1496.353040	173763.130310	36.535245
1497.307031	174043.643561	36.540263
1498.984391	174316.667040	36.545280
1500.608320	174595.350446	36.550298
1501.740060	174871.077006	36.555316
1503.647018	175141.629314	36.560333
1505.216704	175420.324050	36.565351
1506.384530	175701.914336	36.570368
1508.311916	175980.821655	36.575386
1509.595316	176256.618032	36.580404
1510.857888	176530.145577	36.585421
1512.717309	176811.529798	36.590439
1513.988154	177096.130893	36.595456
1515.383960	177376.395904	36.600474
1517.143261	177662.522457	36.605492
1518.916526	177941.866747	36.610509
1520.430184	178224.325635	36.615527
1521.976972	178503.021460	36.620544
1523.493177	178774.840274	36.625562
1525.035100	179065.475415	36.630580
1526.704147	179330.236929	36.635597
1527.808162	179605.322900	36.640615
1529.486006	179880.548487	36.645632
1531.154121	180167.510207	36.650650
1532.491110	180443.324212	36.655668
1533.886069	180702.748323	36.660685
1535.514712	180974.378426	36.665703
1536.782326	181245.532475	36.670720
1538.558213	181504.518254	36.675738
1539.943586	181764.683393	36.680756
1541.246769	182036.291343	36.685773
1542.641846	182308.546048	36.690791
1543.835494	182580.807661	36.695808
1545.471987	182861.915613	36.700826
1547.534957	183143.694199	36.705844
1548.726740	183412.859831	36.710861
1550.226461	183701.306435	36.715879
1551.638553	183975.442683	36.720896
1553.602788	184263.945230	36.725914
1554.838468	184556.575669	36.730932
1556.432244	184839.727885	36.735949
1557.762287	185191.448910	36.740967
1559.509165	185500.689285	36.745984
1561.202448	185793.480267	36.751002
1562.311199	186087.125540	36.756020
1563.847137	186386.978433	36.761037
1565.059611	186685.231841	36.766055
1566.671983	186995.589881	36.771072
1568.559405	187295.415740	36.776090
1570.171508	187602.499032	36.781108
1571.690504	187913.102932	36.786125
1573.371824	188217.560954	36.791143
1574.905329	188523.338345	36.796160
1576.732847	188829.807163	36.801178
1578.065543	189142.501068	36.806196
1579.840619	189455.228205	36.811213
1581.231227	189774.544216	36.816231
1582.998942	190089.560254	36.821248
1584.534016	190393.234217	36.826266
1586.483694	190704.260992	36.831284
1587.935742	191017.601705	36.836301
1589.657235	191336.844792	36.841319
1591.508775	191643.418887	36.846336
1592.991140	191954.826854	36.851354
1594.204299	192280.578341	36.856372
1596.342374	192586.551137	36.861389
1597.879544	192901.356612	36.866407
1599.814560	193210.969629	36.871424
1601.500254	193514.983406	36.876442
1602.578619	193837.610291	36.881460
1604.378237	194143.995414	36.886477
1606.026262	194456.628257	36.891495
1607.468921	194774.425020	36.896512
1609.310196	195083.371318	36.901530
1611.062530	195400.841682	36.906548
1612.656781	195716.407019	36.911565
1614.405959	196026.893946	36.916583
1616.163985	196345.153035	36.921600
1617.560116	196666.085837	36.926618
1619.410975	196981.080426	36.931636
1621.055841	197280.917750	36.936653
1622.782884	197596.618897	36.941671
1624.103484	197906.211700	36.946688
1625.904693	198222.359804	36.951706
1627.587568	198523.463782	36.956724
1628.880653	198846.779828	36.961741
1630.766109	199157.912507	36.966759
1632.387130	199470.306485	36.971776
1634.078566	199768.210882	36.976794
1635.626673	200090.270274	36.981812
1637.341518	200408.239866	36.986829
1639.187275	200716.612950	36.991847
1640.446907	201008.719277	36.996864
1642.115010	201323.700468	37.001882
1643.503893	201615.152556	37.006900
1645.200348	201921.341195	37.011917
1647.313313	202212.807981	37.016935
1648.516749	202507.491286	37.021952
1650.466851	202797.536576	37.026970
1652.042272	203095.871394	37.031988
1653.558388	203389.973743	37.037005
1655.254514	203689.255926	37.042023
1656.599454	204001.548909	37.047040
1658.589008	204291.336320	37.052058
1660.031046	204596.603919	37.057076
1661.824925	204908.751892	37.062093
1663.630475	205207.943078	37.067111
1664.656226	205527.960081	37.072128
1666.473947	205836.498538	37.077146
1668.188578	206146.018893	37.082164
1670.100703	206456.829745	37.087181
1671.655686	206778.721846	37.092199
1673.255975	207096.263403	37.097216
1674.691598	207407.709031	37.102234
1676.068381	207739.842442	37.107252
1678.317628	208069.502699	37.112269
1679.770331	208391.717914	37.117287
1681.390331	208723.458994	37.122304
1683.108361	209040.705315	37.127322
1684.497871	209370.374855	37.132340
1686.458927	209700.107795	37.137357
1688.505546	210025.636205	37.142375
1689.997247	210366.189049	37.147392
1691.814157	210699.299025	37.152410
1693.535479	211025.692440	37.157428
1695.517312	211370.132742	37.162445
1697.347950	211688.837943	37.167463
1698.614195	212034.127699	37.172480
1700.461104	212367.793752	37.177498
1702.452509	212704.460572	37.182516
1704.007720	213038.985886	37.187533
1705.897773	213359.791974	37.192551
1707.505699	213707.976862	37.197568
1709.303809	214029.890314	37.202586
1711.188540	214368.353720	37.207604
1712.817339	214707.238538	37.212621
1714.794619	215031.893820	37.217639
1716.317908	215370.541685	37.222656
1718.051793	215708.521777	37.227674
1720.034019	216046.691907	37.232692
1721.636658	216378.545333	37.237709
1723.288929	216708.206500	37.242727
1724.793692	217049.983224	37.247744
1726.724377	217385.291749	37.252762
1728.764323	217723.377824	37.257780
1730.536148	218065.088022	37.262797
1732.263160	218400.708492	37.267815
1733.770393	218733.391282	37.272832
1735.971549	219063.653897	37.277850
1737.147283	219407.668274	37.282868
1738.723512	219743.059003	37.287885
1740.996222	220073.971404	37.292903
1742.859790	220408.860189	37.297920
1744.471593	220747.395877	37.302938
1746.056088	221077.171573	37.307956
1748.042243	221420.628114	37.312973
1749.810695	221746.615443	37.317991
1751.840605	222085.035341	37.323008
1753.660738	222406.950110	37.328026
1755.202012	222737.063296	37.333044
1756.569340	223071.725694	37.338061
1758.678077	223380.334570	37.343079
1760.107413	223699.313055	37.348096
1761.657141	224013.496772	37.353114
1763.756013	224325.994130	37.358132
1765.523622	224650.534076	37.363149
1767.311318	224961.251072	37.368167
1768.883123	225280.588440	37.373184
1770.592847	225601.072813	37.378202
1772.284301	225924.049638	37.383220
1773.592835	226240.252668	37.388237
1775.535543	226568.118526	37.393255
1777.109001	226902.418556	37.398272
1779.032811	227237.527455	37.403290
1780.728682	227569.521864	37.408308
1782.106620	227907.967787	37.413325
1783.925065	228251.146071	37.418343
1786.016999	228601.775668	37.423360
1787.391014	228953.330436	37.428378
1789.240213	229295.080989	37.433396
1791.131397	229642.210511	37.438413
1792.969133	229992.727001	37.443431
1794.513244	230354.111403	37.448448
1796.215491	230702.997536	37.453466
1798.327010	231063.937163	37.458484
1799.970923	231424.721141	37.463501
1801.716626	231777.842404	37.468519
1803.602832	232150.731152	37.473536
1805.796276	232510.234529	37.478554
1807.605643	232875.945522	37.483572
1809.311997	233244.060352	37.488589
1811.345252	233600.895252	37.493607
1812.938619	233974.133403	37.498624
1814.951836	234333.587490	37.503642
1816.924727	234696.502519	37.508660
1818.745605	235072.219137	37.513677
1820.594903	235430.834234	37.518695
1822.434160	235809.570346	37.523712
1824.082152	236168.698943	37.528730
1826.184980	236537.333217	37.533748
1828.080061	236908.108127	37.538765
1829.973132	237275.605891	37.543783
1831.515560	237644.479113	37.548800
1833.927396	238017.559892	37.553818
1836.025460	238374.812115	37.558836
1837.794384	238747.382948	37.563853
1839.567864	239101.382658	37.568871
1841.542561	239457.357331	37.573888
1843.288263	239825.129184	37.578906
1845.167590	240189.373977	37.583924
1847.178702	240559.821487	37.588941
1849.404718	240921.292885	37.593959
1851.223025	241286.002990	37.598976
1852.519463	241644.011565	37.603994
1854.901131	242021.029242	37.609012
1856.496933	242373.375804	37.614029
1858.319683	242736.254040	37.619047
1860.334665	243116.096305	37.624064
1862.533026	243461.132463	37.629082
1864.129709	243824.374588	37.634100
1866.375951	244179.055284	37.639117
1868.329625	244533.654162	37.644135
1869.921906	244896.310905	37.649152
1871.540727	245249.944854	37.654170
1873.499966	245615.972296	37.659188
1875.560886	245978.528385	37.664205
1877.743209	246334.434705	37.669223
1879.421878	246691.968742	37.674240
1881.355184	247034.931971	37.679258
1883.123136	247377.996653	37.684276
1884.892389	247725.404325	37.689293
1886.418516	248062.688387	37.694311
1888.706314	248397.414001	37.699328
1890.408812	248738.581157	37.704346
1892.023656	249067.746060	37.709364
1893.593079	249417.417074	37.714381
1895.628136	249761.375214	37.719399
1897.588971	250112.228245	37.724416
1899.325612	250460.829416	37.729434
1901.414699	250820.322977	37.734452
1903.043483	251175.340794	37.739469
1904.931196	251537.912478	37.744487
1906.697930	251894.253383	37.749504
1908.241610	252249.485278	37.754522
1910.385216	252616.281878	37.759540
1911.699400	252997.991144	37.764557
1914.086928	253369.624839	37.769575
1915.989633	253741.739868	37.774592
1917.544673	254119.318849	37.779610
1919.580617	254497.456612	37.784628
1921.097669	254884.158596	37.789645
1923.430132	255277.666460	37.794663
1925.504397	255655.287025	37.799680
1927.306989	256052.584119	37.804698
1929.502697	256438.692846	37.809716
1931.356577	256830.645346	37.814733
1933.287566	257220.831930	37.819751
1934.962085	257616.239221	37.824768
1937.097094	258016.856578	37.829786
1939.530183	258409.882010	37.834804
1941.055966	258802.362333	37.839821
1943.168406	259194.292391	37.844839
1945.119686	259592.520293	37.849856
1947.155221	259994.569128	37.854874
1948.906341	260389.904624	37.859892
1951.114010	260793.650995	37.864909
1953.453865	261190.872846	37.869927
1955.415603	261605.551459	37.874944
1957.383904	261995.056223	37.879962
1959.263190	262392.498289	37.884980
1961.343352	262791.126673	37.889997
1963.371752	263184.503976	37.895015
1965.296833	263582.467921	37.900032
1967.505437	263983.027558	37.905050
1969.255183	264381.955713	37.910068
1971.433543	264787.825468	37.915085
1973.288116	265196.995377	37.920103
1975.420517	265588.645647	37.925120
1977.434987	265995.095031	37.930138
1979.459274	266386.708316	37.935156
1981.296660	266796.737976	37.940173
1983.461644	267192.948617	37.945191
1985.343650	267595.449956	37.950208
1987.544688	267993.074001	37.955226
1989.485226	268391.753080	37.960244
1991.588183	268802.951777	37.965261
1993.909697	269199.053410	37.970279
1996.072107	269581.285554	37.975296
1997.806248	269977.018593	37.980314
1999.903969	270373.835930	37.985332
2001.629575	270769.439865	37.990349
2003.772153	271169.929336	37.995367
2005.945401	271560.100850	38.000384
2007.413351	271960.158952	38.005402
2009.693027	272359.148525	38.010420
2011.681440	272758.461200	38.015437
2013.314724	273148.887853	38.020455
2015.581208	273521.283477	38.025472
2017.341637	273909.756578	38.030490
2019.400143	274282.232171	38.035508
2021.476375	274662.068309	38.040525
2023.333760	275045.086092	38.045543
2025.431959	275427.734257	38.050560
2026.730684	275810.632686	38.055578
2029.085329	276203.598690	38.060596
2031.215308	276607.061023	38.065613
2032.827858	276994.831495	38.070631
2035.205294	277388.600738	38.075648
2037.310990	277788.073714	38.080666
2039.003630	278181.666743	38.085684
2040.801473	278597.309772	38.090701
2042.684255	279003.388695	38.095719
2044.819311	279408.689521	38.100736
2046.462138	279829.479843	38.105754
2048.931954	280247.091048	38.110772
2051.123936	280660.959584	38.115789
2052.884324	281083.933726	38.120807
2055.026234	281490.898138	38.125824
2056.830092	281919.904457	38.130842
2059.101850	282345.508407	38.135860
2061.369905	282777.281096	38.140877
2063.302724	283209.027425	38.145895
2065.596085	283634.366325	38.150912
2067.551781	284068.414594	38.155930
2069.746368	284505.622312	38.160948
2071.782370	284936.427632	38.165965
2073.819872	285369.896254	38.170983
2076.064208	285801.958542	38.176000
2078.004030	286240.769328	38.181018
2080.255451	286676.049733	38.186036
2082.411899	287114.668522	38.191053
2084.884921	287561.436487	38.196071
2086.913076	287988.846240	38.201088
2089.095021	288435.399843	38.206106
2090.928982	288876.647193	38.211124
2093.058778	289321.298444	38.216141
2094.870794	289762.441546	38.221159
2097.303500	290201.605532	38.226176
2099.431093	290649.523225	38.231194
2101.731964	291094.922312	38.236212
2103.798602	291546.880182	38.241229
2105.952933	291990.746918	38.246247
2108.270892	292418.995334	38.251264
2110.599155	292869.480652	38.256282
2112.747661	293310.469596	38.261300
2114.952322	293758.047780	38.266317
2117.114226	294189.634024	38.271335
2119.268768	294633.405051	38.276352
2121.373340	295076.038045	38.281370
2123.714841	295506.012413	38.286388
2125.999047	295945.614822	38.291405
2128.049286	296379.081113	38.296423
2130.429867	296820.108896	38.301440
2132.398747	297254.749132	38.306458
2134.312600	297684.520189	38.311476
2136.755403	298128.777683	38.316493
2138.711702	298569.274268	38.321511
2140.816762	298992.379263	38.326528
2142.918806	299442.315531	38.331546
2145.428796	299863.522628	38.336564
2147.757074	300302.855537	38.341581
2149.513708	300736.181596	38.346599
2152.042670	301165.448496	38.351616
2154.091068	301607.099340	38.356634
2156.192409	302031.526707	38.361652
2158.379422	302437.685061	38.366669
2160.286492	302844.848733	38.371687
2162.772830	303245.546948	38.376704
2164.420703	303656.781104	38.381722
2166.601807	304060.262386	38.386740
2168.910364	304466.969807	38.391757
2170.649922	304883.866011	38.396775
2172.768060	305299.303465	38.401792
2174.484229	305720.257966	38.406810
2176.794297	306144.035190	38.411828
2179.123803	306569.633422	38.416845
2181.051506	307010.343200	38.421863
2182.972679	307431.733579	38.426880
2185.233670	307875.632585	38.431898
2187.410124	308303.625909	38.436916
2189.594961	308757.707308	38.441933
2191.855666	309205.807805	38.446951
2194.307363	309640.345712	38.451968
2196.131148	310098.126059	38.456986
2198.429633	310540.878100	38.462004
2200.472881	310996.077389	38.467021
2202.104712	311451.793540	38.472039
2204.473406	311905.181900	38.477056
2207.008824	312378.006640	38.482074
2209.020847	312835.756484	38.487092
2211.371627	313309.159037	38.492109
2213.490787	313782.339185	38.497127
2216.113951	314244.243283	38.502144
2218.042434	314722.265671	38.507162
2220.501490	315181.292735	38.512180
2222.649719	315654.931135	38.517197
2224.981563	316147.544254	38.522215
2227.471568	316628.757821	38.527232
2229.700177	317102.672888	38.532250
2231.933659	317573.815975	38.537268
2234.246870	318051.184376	38.542285
2236.090907	318534.609963	38.547303
2238.121653	319012.671875	38.552320
2240.531710	319495.008565	38.557338
2242.983928	319983.474314	38.562356
2245.308330	320462.971443	38.567373
2247.499378	320954.943483	38.572391
2249.865635	321445.562912	38.577408
2251.832364	321930.022279	38.582426
2254.343357	322425.809559	38.587444
2256.670107	322912.155137	38.592461
2258.893568	323408.356364	38.597479
2261.514141	323895.380333	38.602496
2263.757298	324400.751905	38.607514
2266.115270	324881.563407	38.612532
2268.887130	325365.095529	38.617549
2270.556919	325866.884971	38.622567
2272.803630	326346.783147	38.627584
2275.060645	326847.656628	38.632602
2277.582928	327334.933884	38.637620
2280.006080	327825.899541	38.642637
2282.227785	328324.045274	38.647655
2284.695080	328815.093246	38.652672
2286.829321	329300.123658	38.657690
2288.873119	329788.308099	38.662708
2291.139547	330278.557287	38.667725
2293.570502	330778.947688	38.672743
2295.901770	331266.383571	38.677760
2298.116824	331761.365982	38.682778
2300.226934	332255.622714	38.687796
2302.609053	332756.603768	38.692813
2304.937037	333247.820059	38.697831
2307.141447	333746.583418	38.702848
2309.500883	334209.193083	38.707866
2311.491896	334684.081467	38.712884
2314.046829	335147.333812	38.717901
2316.148917	335631.197816	38.722919
2318.534421	336095.124303	38.727936
2320.584708	336575.838621	38.732954
2322.545356	337055.038730	38.737972
2324.891088	337543.303645	38.742989
2327.288960	338035.079492	38.748007
2329.495414	338509.986040	38.753024
2331.835710	339004.116527	38.758042
2334.010060	339496.186343	38.763060
2336.433643	339998.659982	38.768077
2338.799865	340507.755155	38.773095
2341.279604	340999.730973	38.778112
2343.289865	341504.352918	38.783130
2345.716558	342014.710270	38.788148
2348.187433	342522.009880	38.793165
2350.247133	343034.793629	38.798183
2352.698696	343556.181775	38.803200
2355.414782	344071.307398	38.808218
2357.223871	344587.860496	38.813236
2359.939237	345112.353649	38.818253
2362.486570	345642.824343	38.823271
2364.892067	346156.293275	38.828288
2366.839315	346679.741113	38.833306
2369.606622	347209.265159	38.838324
2372.125427	347736.055711	38.843341
2374.224546	348277.027401	38.848359
2376.856529	348806.090721	38.853376
2379.403317	349340.306165	38.858394
2381.663357	349871.641843	38.863412
2384.250806	350406.036363	38.868429
2386.587504	350939.548539	38.873447
2388.836785	351473.547326	38.878464
2391.573681	352009.616086	38.883482
2393.742446	352553.294791	38.888500
2396.512488	353089.010688	38.893517
2398.871696	353631.500315	38.898535
2401.369557	354169.420888	38.903552
2404.030363	354713.061684	38.908570
2406.254481	355254.555796	38.913588
2408.874640	355791.339338	38.918605
2411.139834	356331.312626	38.923623
2413.950828	356865.309898	38.928640
2416.425213	357409.921425	38.933658
2418.705510	357952.348280	38.938676
2421.396250	358478.199232	38.943693
2423.990227	359019.315991	38.948711
2426.505409	359555.340500	38.953728
2428.645222	360090.704497	38.958746
2431.256437	360627.860929	38.963764
2433.767599	361153.085150	38.968781
2436.358144	361690.175072	38.973799
2438.950484	362230.676692	38.978816
2441.346213	362755.814661	38.983834
2443.352497	363291.066091	38.988852
2446.440538	363825.682384	38.993869
2448.625039	364361.342631	38.998887
2451.079878	364901.867385	39.003904
2453.406200	365435.407552	39.008922
2455.823846	365962.131832	39.013940
2458.772875	366497.252950	39.018957
2460.733805	367037.029450	39.023975
2463.540976	367565.082561	39.028992
2466.186486	368092.695054	39.034010
2468.251082	368614.078933	39.039028
2470.662956	369132.839592	39.044045
2473.372083	369649.466407	39.049063
2475.721020	370158.285067	39.054080
2478.351081	370655.673634	39.059098
2480.379500	371158.772438	39.064116
2483.047435	371659.355070	39.069133
2485.101490	372171.046229	39.074151
2487.561292	372677.546493	39.079168
2489.937898	373183.366381	39.084186
2492.199265	373710.147409	39.089204
2494.642994	374217.812518	39.094221
2496.941046	374747.557315	39.099239
2499.244872	375279.672269	39.104256
2501.865413	375817.579258	39.109274
2504.029230	376355.293618	39.114292
2506.844688	376893.249943	39.119309
2509.244049	377435.490974	39.124327
2511.949855	377979.851552	39.129344
2514.423739	378526.491702	39.134362
2516.663817	379079.160441	39.139380
2519.382819	379622.471955	39.144397
2521.582117	380187.535444	39.149415
2523.890024	380735.523471	39.154432
2526.319097	381303.692993	39.159450
2528.836295	381887.108912	39.164468
2531.824636	382453.418169	39.169485
2534.523840	383030.726621	39.174503
2537.082529	383605.891374	39.179520
2539.631918	384158.150468	39.184538
2542.268391	384752.879139	39.189556
2544.810231	385316.054644	39.194573
2547.272243	385895.158737	39.199591
2549.875029	386482.989329	39.204608
2552.720570	387058.385489	39.209626
2555.067293	387641.316431	39.214644
2558.096257	388223.418057	39.219661
2560.343676	388807.577996	39.224679
2563.010281	389398.976133	39.229696
2565.885969	389977.743581	39.234714
2568.250908	390568.781040	39.239732
2570.692031	391151.336005	39.244749
2573.191042	391741.210173	39.249767
2575.872898	392331.952865	39.254784
2578.888639	392918.679569	39.259802
2581.070557	393526.078945	39.264820
2583.901754	394111.235919	39.269837
2586.335323	394704.136463	39.274855
2589.425005	395307.095917	39.279872
2592.405529	395899.729325	39.284890
2594.657442	396493.120024	39.289908
2597.360781	397082.274050	39.294925
2600.362980	397669.949164	39.299943
2602.827535	398248.126163	39.304960
2605.561155	398839.357492	39.309978
2608.265130	399430.173521	39.314996
2611.108818	400017.206961	39.320013
2613.663249	400602.246103	39.325031
2615.997053	401184.926010	39.330048
2618.737506	401773.297561	39.335066
2621.333072	402362.081579	39.340084
2623.785559	402951.986259	39.345101
2626.564840	403537.472085	39.350119
2628.735344	404138.574916	39.355136
2631.566035	404724.528123	39.360154
2634.196122	405321.782639	39.365172
2637.227717	405914.302850	39.370189
2639.703362	406510.335367	39.375207
2642.476838	407113.996903	39.380224
2645.230986	407682.730592	39.385242
2647.345891	408248.159508	39.390260
2649.947205	408814.155668	39.395277
2652.423053	409365.939191	39.400295
2655.358568	409932.815646	39.405312
2657.952576	410491.989912	39.410330
2660.151165	411062.848086	39.415348
2662.652105	411630.608505	39.420365
2665.461961	412202.100029	39.425383
2667.812435	412776.228336	39.430400
2670.338937	413346.823282	39.435418
2672.784235	413945.541740	39.440436
2675.379499	414531.320887	39.445453
2677.726582	415134.169399	39.450471
2679.998195	415740.654550	39.455488
2683.119775	416339.402360	39.460506
2685.455988	416952.064138	39.465524
2688.151500	417559.644741	39.470541
2690.617602	418187.474107	39.475559
2693.294220	418814.796563	39.480576
2695.916394	419435.787051	39.485594
2698.465709	420068.199574	39.490612
2701.142114	420712.659165	39.495629
2703.795450	421353.056801	39.500647
2706.586267	422006.408701	39.505664
2709.394352	422641.786461	39.510682
2712.075292	423301.788864	39.515700
2714.919315	423954.766853	39.520717
2717.993010	424610.620446	39.525735
2720.208801	425269.114908	39.530752
2723.371824	425919.906757	39.535770
2725.703343	426595.933628	39.540788
2728.505906	427263.775460	39.545805
2731.428990	427927.380312	39.550823
2734.126624	428598.024806	39.555840
2736.952725	429272.822086	39.560858
2739.646708	429946.606075	39.565876
2742.599695	430612.340406	39.570893
2745.313902	431300.480251	39.575911
2748.097056	431982.621229	39.580928
2751.127149	432659.190907	39.585946
2753.794191	433332.660468	39.590964
2756.348618	434022.447483	39.595981
2759.492495	434697.210013	39.600999
2762.381691	435394.930590	39.606016
2765.285707	436063.972466	39.611034
2767.947227	436751.522535	39.616052
2771.050532	437434.987068	39.621069
2773.943657	438120.026180	39.626087
2776.375910	438803.243217	39.631104
2779.294151	439483.328222	39.636122
2782.305236	440179.035326	39.641140
2784.978456	440863.655478	39.646157
2787.664925	441539.206074	39.651175
2790.583130	442236.215090	39.656192
2793.211192	442902.986307	39.661210
2795.821338	443598.729474	39.666228
2798.842031	444291.402194	39.671245
2802.297031	444978.627178	39.676263
2804.858279	445667.481317	39.681280
2807.521501	446345.031354	39.686298
2810.902921	447027.948517	39.691316
2814.135738	447710.661235	39.696333
2816.999741	448387.699670	39.701351
2819.536268	449057.896522	39.706368
2822.288034	449729.701043	39.711386
2825.164037	450414.235392	39.716404
2827.769789	451087.627544	39.721421
2830.657282	451742.421116	39.726439
2833.515510	452401.183542	39.731456
2836.451293	453035.929317	39.736474
2839.261738	453680.263557	39.741492
2841.532370	454321.579328	39.746509
2844.574140	454964.114026	39.751527
2846.879859	455606.538346	39.756544
2849.763915	456255.814158	39.761562
2852.485995	456903.778788	39.766580
2855.285648	457563.265028	39.771597
2858.052340	458223.690218	39.776615
2861.047651	458892.028238	39.781632
2863.586291	459561.017303	39.786650
2866.647427	460240.193122	39.791668
2869.270059	460920.974856	39.796685
2872.096017	461594.330557	39.801703
2874.445203	462284.183264	39.806720
2877.494557	462971.678390	39.811738
2879.926403	463668.172346	39.816756
2882.978746	464387.193044	39.821773
2886.043654	465087.262658	39.826791
2888.633992	465791.564318	39.831808
2891.274076	466516.208157	39.836826
2894.502973	467246.125731	39.841844
2897.062634	467956.494600	39.846861
2900.280011	468679.289215	39.851879
2903.102376	469413.764612	39.856896
2905.919092	470149.216767	39.861914
2908.856509	470883.759728	39.866932
2911.570819	471625.465491	39.871949
2914.832590	472362.412627	39.876967
2917.513701	473118.628830	39.881984
2920.823181	473864.526208	39.887002
2924.161397	474616.434989	39.892020
2926.884231	475366.741090	39.897037
2929.895461	476112.328824	39.902055
2932.788596	476868.537334	39.907072
2936.016802	477626.522759	39.912090
2938.884480	478380.899045	39.917108
2942.045445	479129.497739	39.922125
2944.988055	479881.774521	39.927143
2948.227071	480642.889926	39.932160
2951.124387	481389.607980	39.937178
2954.193054	482137.473114	39.942196
2957.413131	482900.346340	39.947213
2960.546060	483651.857832	39.952231
2963.791399	484400.896684	39.957248
2966.751098	485149.238508	39.962266
2969.753222	485892.700548	39.967284
2972.661954	486651.154805	39.972301
2975.508145	487399.354445	39.977319
2978.464258	488162.210091	39.982336
2981.668826	488908.365390	39.987354
2984.819413	489647.994587	39.992372
2987.825140	490404.836403	39.997389
2990.640007	491157.137172	40.002407
2994.286262	491900.758889	40.007424
2997.676035	492643.477361	40.012442
3000.497010	493376.931554	40.017460
3002.836023	494122.762337	40.022477
3006.284245	494868.734780	40.027495
3009.062025	495616.788594	40.032512
3012.251555	496360.259182	40.037530
3015.394557	497094.435900	40.042548
3018.586540	497841.909355	40.047565
3021.262857	498583.132733	40.052583
3024.264386	499323.562966	40.057600
3027.192424	500067.792631	40.062618
3030.488457	500798.638686	40.067636
3033.276157	501506.777865	40.072653
3036.181412	502220.450451	40.077671
3038.971470	502919.712536	40.082688
3042.129467	503633.527235	40.087706
3045.088182	504340.443616	40.092724
3047.995567	505044.163043	40.097741
3051.138634	505758.628860	40.102759
3053.641669	506484.378788	40.107776
3056.452146	507214.571526	40.112794
3059.510536	507933.670348	40.117812
3062.193451	508675.982163	40.122829
3065.334527	509408.826867	40.127847
3068.168897	510164.567932	40.132864
3071.068920	510914.171953	40.137882
3074.462861	511668.838890	40.142900
3077.019330	512433.453139	40.147917
3079.700765	513194.032911	40.152935
3082.961777	513969.063407	40.157952
3086.309205	514750.322365	40.162970
3089.148975	515519.398140	40.167988
3091.704376	516313.513769	40.173005
3094.722937	517095.243834	40.178023
3097.992276	517900.216231	40.183040
3101.247942	518703.986996	40.188058
3104.663858	519507.936461	40.193076
3107.499431	520319.016039	40.198093
3110.799686	521135.603378	40.203111
3113.893962	521952.474936	40.208128
3117.142336	522757.513250	40.213146
3120.564516	523577.350267	40.218164
3123.530323	524403.891244	40.223181
3127.040400	525231.501666	40.228199
3130.383079	526053.459582	40.233216
3132.917751	526866.801510	40.238234
3136.687993	527695.774506	40.243252
3139.650763	528520.250380	40.248269
3143.519617	529348.651552	40.253287
3146.634505	530176.716328	40.258304
3149.762770	531002.466424	40.263322
3153.108525	531822.605946	40.268340
3156.054753	532652.046086	40.273357
3159.488004	533467.749139	40.278375
3162.631176	534293.688771	40.283392
3165.809529	535117.159938	40.288410
3169.318811	535938.468143	40.293428
3172.529364	536769.910744	40.298445
3175.580149	537594.246347	40.303463
3178.995092	538417.768868	40.308480
3182.190455	539253.870028	40.313498
3185.470186	540073.441350	40.318516
3188.930226	540903.620371	40.323533
3191.866986	541720.177295	40.328551
3195.479223	542543.449731	40.333568
3198.332365	543372.757351	40.338586
3201.082131	544189.884709	40.343604
3205.063764	545030.043417	40.348621
3208.049264	545853.094736	40.353639
3211.329254	546674.841399	40.358656
3214.303163	547511.728655	40.363674
3217.963104	548325.681897	40.368692
3220.688611	549146.748302	40.373709
3223.916637	549976.406651	40.378727
3227.640777	550797.958180	40.383744
3230.635700	551635.964129	40.388762
3233.975109	552451.848293	40.393780
3237.104774	553284.855902	40.398797
3240.636871	554105.060228	40.403815
3243.835411	554909.220301	40.408832
3246.784654	555709.606252	40.413850
3250.174397	556485.411281	40.418868
3253.415203	557261.890851	40.423885
3256.417790	558046.325128	40.428903
3259.996499	558822.750268	40.433920
3262.413962	559612.634564	40.438938
3265.702081	560392.309293	40.443956
3269.173297	561179.769618	40.448973
3271.879968	561970.553083	40.453991
3275.475770	562774.268778	40.459008
3278.114250	563588.597876	40.464026
3281.455087	564389.487484	40.469044
3284.661051	565207.221113	40.474061
3287.812309	566036.223716	40.479079
3291.224261	566865.677111	40.484096
3294.303790	567691.417620	40.489114
3297.540886	568522.131306	40.494132
3300.633708	569366.725626	40.499149
3303.861709	570214.991231	40.504167
3307.471042	571066.838590	40.509184
3310.487267	571920.617126	40.514202
3314.162075	572779.183613	40.519220
3316.962867	573635.319487	40.524237
3320.518482	574504.683993	40.529255
3324.302706	575375.296859	40.534272
3327.148121	576252.093409	40.539290
3330.565406	577129.782760	40.544308
3334.021897	578017.902832	40.549325
3337.290675	578886.722856	40.554343
3340.602927	579774.825654	40.559360
3344.149725	580654.068197	40.564378
3347.644768	581550.852905	40.569396
3350.845090	582448.361021	40.574413
3354.144180	583340.680343	40.579431
3357.663287	584234.092805	40.584448
3360.948008	585136.268147	40.589466
3364.389534	586031.145914	40.594484
3367.572262	586933.138748	40.599501
3370.911758	587846.178288	40.604519
3374.513492	588758.550213	40.609536
3378.415315	589663.302204	40.614554
3381.872676	590558.503599	40.619572
3385.530623	591476.333393	40.624589
3388.577308	592385.836735	40.629607
3392.380370	593283.404679	40.634624
3395.940937	594202.414671	40.639642
3399.528959	595105.807101	40.644660
3402.827918	596005.422036	40.649677
3406.211162	596912.338459	40.654695
3409.658111	597815.521745	40.659712
3413.237903	598705.474884	40.664730
3416.574384	599619.305714	40.669748
3419.925265	600532.305756	40.674765
3423.560977	601443.084939	40.679783
3427.207450	602337.710559	40.684800
3430.583529	603242.483026	40.689818
3434.381928	604143.317722	40.694836
3437.593653	605044.664667	40.699853
3441.060058	605948.437772	40.704871
3444.787833	606840.415852	40.709888
3448.193587	607743.940725	40.714906
3451.971294	608627.723494	40.719924
3455.109737	609524.847433	40.724941
3458.827843	610429.781695	40.729959
3462.077888	611311.069979	40.734976
3465.467939	612208.366454	40.739994
3468.871962	613093.514595	40.745012
3472.231778	613982.100944	40.750016
3475.670624	614826.269307	40.755021
3478.939391	615616.318729	40.760026
3481.832738	616365.886584	40.765031
3485.131773	617049.375386	40.770036
3488.447552	617689.893840	40.775040
3490.973163	618272.937071	40.780045
3493.462548	618788.005468	40.785050
3495.820110	619264.849724	40.790055
3498.343320	619685.344710	40.795060
3500.700164	620050.298791	40.800064
3502.876494	620360.069983	40.805069
3504.755194	620623.722984	40.810074
3506.496945	620868.958751	40.815079
3508.131918	621059.860525	40.820084
3509.581969	621199.990019	40.825088
3510.971643	621313.404855	40.830093
3512.519597	621381.691087	40.835098
3513.640895	621416.628791	40.840103
3514.543751	621417.186826	40.845108
3515.529341	621400.649907	40.850112
3516.546554	621354.039544	40.855117
3517.659117	621293.029039	40.860122
3518.222131	621197.439869	40.865127
3518.977238	621070.251939	40.870132
3519.576176	620945.584275	40.875136
3519.826641	620803.087255	40.880141
3520.415840	620620.224517	40.885146
3521.281344	620446.806146	40.890151
3521.494607	620242.565641	40.895156
3521.305388	620028.143192	40.900160
3521.454512	619813.413429	40.905165
3522.067512	619589.064787	40.910170
3522.299187	619356.727481	40.915175
3522.399647	619106.669801	40.920180
3522.471012	618850.215448	40.925184
3522.645592	618587.193364	40.930189
3523.030345	618329.727319	40.935194
3523.221025	618057.195737	40.940199
3523.311638	617767.484126	40.945204
3523.401322	617488.357283	40.950208
3523.318690	617209.999092	40.955213
3523.487494	616907.908039	40.960218
3523.357170	616612.350914	40.965223
3523.337354	616310.471169	40.970228
3523.093413	616012.615314	40.975232
3523.209727	615713.394902	40.980237
3522.979887	615402.175072	40.985242
3522.791803	615108.681637	40.990247
3522.438386	614806.358907	40.995252
3522.585780	614505.198338	41.000256
3522.472824	614221.163811	41.005261
3522.363503	613913.277877	41.010266
3521.890516	613613.587180	41.015271
3521.468756	613314.429428	41.020276
3521.647519	613022.967275	41.025280
3521.368461	612722.919855	41.030285
3520.945724	612430.084884	41.035290
3520.953218	612138.174049	41.040295
3520.993303	611862.248164	41.045300
3520.595762	611573.134088	41.050304
3520.191178	611286.762753	41.055309
3520.352314	611005.244835	41.060314
3520.012501	610728.097488	41.065319
3520.064674	610452.431368	41.070324
3519.430856	610172.464707	41.075328
3519.261775	609903.818789	41.080333
3519.466128	609635.357438	41.085338
3519.153997	609372.670603	41.090343
3518.781302	609089.732925	41.095348
3518.329782	608828.304080	41.100352
3518.073921	608574.389666	41.105357
3518.061454	608305.827217	41.110362
3517.725840	608061.314899	41.115367
3517.595073	607806.811722	41.120372
3517.380976	607557.516944	41.125376
3516.910196	607318.909951	41.130381
3516.665007	607064.606301	41.135386
3516.257603	606831.029939	41.140391
3516.257891	606603.287003	41.145396
3516.033114	606370.121801	41.150400
3515.776020	606138.757199	41.155405
3515.817492	605915.044465	41.160410
3515.693704	605697.205673	41.165415
3515.008069	605464.192044	41.170420
3515.061497	605261.074130	41.175424
3515.222161	605045.078137	41.180429
3514.727703	604838.135325	41.185434
3514.579492	604620.277611	41.190439
3514.527828	604406.552837	41.195444
3514.091949	604202.890230	41.200448
3513.874715	604004.392922	41.205453
3513.896560	603803.352710	41.210458
3513.460243	603612.787595	41.215463
3513.413168	603405.596081	41.220468
3513.448446	603220.454038	41.225472
3513.029991	603029.074806	41.230477
3512.869101	602837.451624	41.235482
3512.225766	602648.152131	41.240487
3512.567971	602470.504789	41.245492
3512.410903	602300.038396	41.250496
3512.089008	602117.134368	41.255501
3512.022405	601935.037958	41.260506
3511.396374	601774.845145	41.265511
3511.526128	601607.575454	41.270516
3511.412400	601447.297520	41.275520
3511.002855	601278.255157	41.280525
3511.432417	601122.241358	41.285530
3511.172854	600964.781465	41.290535
3511.287316	600797.551234	41.295540
3510.874354	600625.746148	41.300544
3510.486094	600480.461166	41.305549
3510.441514	600331.116343	41.310554
3510.309139	600195.046862	41.315559
3510.356981	600040.628209	41.320564
3510.370588	599886.613059	41.325568
3509.738903	599742.106680	41.330573
3510.055157	599605.008376	41.335578
3509.856426	599466.387016	41.340583
3509.633354	599304.892018	41.345588
3509.415023	599174.929573	41.350592
3509.337294	599049.999328	41.355597
3509.152936	598914.922506	41.360602
3508.993834	598789.551363	41.365607
3509.067914	598656.833634	41.370612
3508.861910	598524.908911	41.375616
3508.898802	598404.608639	41.380621
3508.919356	598281.205767	41.385626
3508.436372	598157.830103	41.390631
3508.540495	598035.712889	41.395636
3508.777576	597905.112873	41.400640
3508.431968	597785.365950	41.405645
3508.266456	597657.979798	41.410650
3508.182928	597544.647415	41.415655
3508.042871	597432.674408	41.420660
3507.846388	597314.000249	41.425664
3507.592010	597206.398415	41.430669
3507.466899	597096.822679	41.435674
3507.628259	597002.471481	41.440679
3507.511837	596893.843555	41.445684
3507.494888	596787.852570	41.450688
3507.291771	596671.976046	41.455693
3506.929846	596574.398303	41.460698
3506.977970	596478.758339	41.465703
3506.869545	596375.080715	41.470708
3507.146039	596277.350361	41.475712
3506.758199	596178.371044	41.480717
3506.837610	596080.369257	41.485722
3506.725600	595981.244834	41.490727
3506.307525	595896.488010	41.495732
3506.437905	595809.992371	41.500736
3506.227291	595723.949919	41.505741
3506.616316	595626.296118	41.510746
3506.103765	595548.110910	41.515751
3506.208330	595447.795944	41.520756
3506.174535	595358.918723	41.525760
3506.190391	595278.946383	41.530765
3506.184859	595190.263632	41.535770
3505.781435	595106.750096	41.540775
3505.481347	595026.875324	41.545780
3505.695770	594946.819366	41.550784
3505.631259	594874.868825	41.555789
3505.414831	594787.367454	41.560794
3505.582514	594713.526656	41.565799
3505.598476	594643.815475	41.570804
3505.483950	594570.668819	41.575808
3505.261177	594488.874934	41.580813
3505.603056	594413.953169	41.585818
3505.281770	594354.659217	41.590823
3505.269986	594270.627172	41.595828
3505.298990	594194.901419	41.600832
3505.181085	594128.513089	41.605837
3505.532990	594058.845724	41.610842
3505.304142	593991.822834	41.615847
3504.985317	593913.645395	41.620852
3505.057706	593844.521142	41.625856
3504.980290	593780.928906	41.630861
3505.038063	593702.640965	41.635866
3504.689808	593645.801330	41.640871
3504.833381	593573.058222	41.645876
3504.912495	593507.937393	41.650880
3505.007650	593444.766928	41.655885
3505.327241	593375.150237	41.660890
3504.869059	593314.770048	41.665895
3504.872665	593241.846228	41.670900
3504.924636	593177.779409	41.675904
3504.722403	593124.720635	41.680909
3505.078914	593047.583239	41.685914
3505.080454	592990.134487	41.690919
3504.823166	592914.544578	41.695924
3504.726999	592841.333105	41.700928
3504.274650	592783.252983	41.705933
3504.667118	592722.335769	41.710938
3504.503441	592661.104450	41.715943
3504.185299	592604.254562	41.720948
3504.261134	592545.689878	41.725952
3504.200573	592495.510938	41.730957
3504.592313	592431.687067	41.735962
3504.218026	592371.939585	41.740967
3504.232568	592321.647912	41.745972
3504.375993	592271.886838	41.750976
3503.737028	592218.791663	41.755981
3503.955855	592157.848296	41.760986
3503.525196	592113.986653	41.765991
3503.740585	592057.300905	41.770996
3504.024105	592001.355565	41.776000
3503.671336	591964.894537	41.781005
3504.220109	591913.365347	41.786010
3504.079119	591859.990182	41.791015
3504.003277	591808.958866	41.796020
3503.965160	591747.051503	41.801024
3504.181899	591705.992306	41.806029
3503.838960	591650.744175	41.811034
3503.863961	591601.349149	41.816039
3503.804397	591552.668413	41.821044
3504.044655	591497.729066	41.826048
3503.655247	591449.900915	41.831053
3503.641314	591400.711425	41.836058
3503.865096	591354.289790	41.841063
3503.903951	591304.240016	41.846068
3504.041267	591250.116998	41.851072
3503.426225	591205.028107	41.856077
3503.299955	591154.502505	41.861082
3503.636334	591115.876982	41.866087
3503.528785	591061.941579	41.871092
3503.886098	591028.572438	41.876096
3503.500310	590974.379522	41.881101
3503.491963	590930.597305	41.886106
3503.486399	590885.612177	41.891111
3503.358726	590837.890669	41.896116
3503.289154	590799.628049	41.901120
3503.052427	590754.478124	41.906125
3503.406377	590708.634512	41.911130
3503.570050	590681.205964	41.916135
3503.068017	590639.603801	41.921140
3503.532076	590593.441905	41.926144
3503.349775	590561.608491	41.931149
3503.253863	590516.686042	41.936154
3503.353804	590478.846659	41.941159
3503.537531	590427.016738	41.946164
3503.239878	590382.425854	41.951168
3503.245088	590347.306116	41.956173
3503.469171	590306.390725	41.961178
3503.028987	590259.767577	41.966183
3503.030762	590222.794319	41.971188
3503.041306	590183.114215	41.976192
3503.152622	590143.468311	41.981197
3503.066710	590103.853093	41.986202
3503.198762	590068.111424	41.991207
3502.745938	590026.699596	41.996212
3502.773937	589987.016042	42.001216
3503.052998	589962.673825	42.006221
3503.018618	589930.815423	42.011226
3502.906491	589900.872894	42.016231
3502.949457	589863.541262	42.021236
3503.093251	589828.748875	42.026240
3503.035368	589793.286491	42.031245
3503.001505	589749.052554	42.036250
3502.888857	589722.766989	42.041255
3503.213670	589678.476692	42.046260
3502.909256	589641.298800	42.051264
3502.980201	589608.220543	42.056269
3503.365691	589563.870190	42.061274
3503.043369	589539.821441	42.066279
3503.399558	589496.477432	42.071284
3503.241880	589444.195141	42.076288
3502.983379	589408.562446	42.081293
3503.030030	589374.334910	42.086298
3503.435157	589344.811006	42.091303
3503.045338	589300.430466	42.096308
3503.264634	589264.722603	42.101312
3503.040674	589226.328225	42.106317
3503.446808	589182.574324	42.111322
3503.282894	589147.126394	42.116327
3503.355880	589100.367906	42.121332
3503.303514	589062.597473	42.126336
3502.817473	589024.794496	42.131341
3503.102526	588976.248664	42.136346
3503.354208	588952.559816	42.141351
3502.925541	588909.085626	42.146356
3503.015933	588866.782747	42.151360
3502.881518	588836.039068	42.156365
3503.075980	588790.663199	42.161370
3502.787721	588760.444411	42.166375
3502.726859	588730.941576	42.171380
3503.021468	588706.042939	42.176384
3502.829559	588658.522258	42.181389
3502.818796	588620.443142	42.186394
3502.713289	588596.458609	42.191399
3502.682428	588554.073251	42.196404
3502.933568	588517.506135	42.201408
3503.096834	588483.908941	42.206413
3502.834818	588443.964420	42.211418
3502.598690	588422.054312	42.216423
3502.678500	588389.572231	42.221428
3502.939918	588356.009404	42.226432
3502.632704	588318.326322	42.231437
3502.987930	588282.143003	42.236442
3502.616680	588257.347429	42.241447
3503.087874	588225.705617	42.246452
3503.206233	588192.916272	42.251456
3502.796010	588163.165855	42.256461
3503.051628	588110.662186	42.261466
3502.960941	588072.743966	42.266471
3502.563181	588050.357285	42.271476
3502.985300	588020.877232	42.276480
3502.628793	587988.412049	42.281485
3502.856191	587953.951332	42.286490
3502.610714	587916.708186	42.291495
3502.703700	587884.924068	42.296500
3502.770760	587850.888967	42.301504
3502.408203	587825.289287	42.306509
3502.768919	587797.321525	42.311514
3502.723027	587764.055461	42.316519
3502.320594	587730.945253	42.321524
3502.712840	587697.510271	42.326528
3502.376704	587670.553110	42.331533
3502.687685	587639.084969	42.336538
3502.822266	587610.500638	42.341543
3502.785000	587573.073430	42.346548
3502.558074	587545.848331	42.351552
3502.515994	587524.156629	42.356557
3502.736512	587489.495070	42.361562
3502.638087	587450.473433	42.366567
3502.616251	587419.708137	42.371572
3502.512543	587389.506785	42.376576
3503.054612	587373.185666	42.381581
3502.658751	587329.549671	42.386586
3502.450187	587303.122889	42.391591
3502.418482	587275.515807	42.396596
3502.674374	587228.570319	42.401600
3502.209821	587205.390530	42.406605
3502.416483	587177.495372	42.411610
3502.293084	587155.264403	42.416615
3502.741832	587130.989533	42.421620
3502.800396	587094.748414	42.426624
3502.459094	587065.034322	42.431629
3502.593696	587038.152342	42.436634
3502.442080	587002.545135	42.441639
3502.276655	586975.359106	42.446644
3502.789111	586944.959968	42.451648
3502.344621	586910.450639	42.456653
3502.548652	586887.817137	42.461658
3502.793074	586866.430135	42.466663
3502.320577	586829.469321	42.471668
3502.752869	586804.945726	42.476672
3502.740964	586771.771542	42.481677
3502.686982	586733.742682	42.486682
3502.553401	586710.059060	42.491687
3502.857012	586680.243100	42.496692
3502.452677	586650.938652	42.501696
3502.536382	586622.008871	42.506701
3502.451035	586598.718391	42.511706
3502.419540	586582.034714	42.516711
3502.298349	586534.443564	42.521716
3502.662271	586506.171293	42.526720
3502.169196	586482.443142	42.531725
3502.370116	586452.943311	42.536730
3502.391407	586431.039057	42.541735
3502.381088	586416.506821	42.546740
3503.037242	586370.096462	42.551744
3502.633809	586338.986833	42.556749
3502.649325	586308.563376	42.561754
3502.439310	586285.041129	42.566759
3501.850017	586251.304100	42.571764
3501.877921	586222.281747	42.576768
3502.014367	586205.671476	42.581773
3502.505536	586182.941508	42.586778
3501.940185	586172.003939	42.591783
3502.423604	586147.320523	42.596788
3502.414074	586106.776641	42.601792
3502.396012	586092.896717	42.606797
3502.265381	586066.805574	42.611802
3502.147799	586056.499542	42.616807
3502.155855	586018.308134	42.621812
3502.227383	585988.426329	42.626816
3502.367652	585973.769725	42.631821
3502.133549	585936.467900	42.636826
3502.237879	585910.790721	42.641831
3502.060670	585885.357970	42.646836
3502.175727	585872.258857	42.651840
3502.002235	585846.374363	42.656845
3502.183657	585821.837662	42.661850
3502.188879	585799.784296	42.666855
3502.082488	585776.695826	42.671860
3502.719362	585747.025698	42.676864
3502.345722	585727.888226	42.681869
3502.537077	585694.829350	42.686874
3502.191066	585670.174282	42.691879
3502.103441	585640.967965	42.696884
3502.512982	585611.333008	42.701888
3502.413057	585590.147699	42.706893
3502.757183	585561.324757	42.711898
3502.353524	585536.778640	42.716903
3502.371558	585506.553037	42.721908
3502.429514	585470.657462	42.726912
3502.235311	585455.651485	42.731917
3502.180347	585427.441908	42.736922
3501.934514	585404.875661	42.741927
3502.134915	585398.228258	42.746932
3502.446816	585368.407424	42.751936
3501.967645	585354.398160	42.756941
3502.065083	585323.307574	42.761946
3502.113637	585297.487310	42.766951
3502.235391	585269.249700	42.771956
3502.482176	585250.114643	42.776960
3502.116977	585230.674247	42.781965
3502.333020	585201.469406	42.786970
3502.112577	585185.715330	42.791975
3501.745361	585156.350937	42.796980
3502.426613	585137.398375	42.801985
3502.280671	585112.259669	42.806989
3502.645777	585084.234152	42.811994
3502.222675	585062.797606	42.816999
3502.139650	585029.629246	42.822004
3502.156646	584996.244658	42.827009
3502.403351	584979.013813	42.832013
3502.280477	584942.643544	42.837018
3502.332132	584918.475967	42.842023
3502.372147	584897.518055	42.847028
3502.205455	584865.013881	42.852033
3501.937624	584855.030944	42.857037
3502.202394	584818.248797	42.862042
3501.918202	584805.210821	42.867047
3502.192995	584778.050745	42.872052
3502.115619	584749.291561	42.877057
3502.242491	584732.630427	42.882061
3502.396027	584721.980007	42.887066
3502.286657	584690.017718	42.892071
3502.420884	584659.520990	42.897076
3502.445445	584631.948550	42.902081
3502.582599	584612.177899	42.907085
3502.216802	584583.463367	42.912090
3502.125803	584553.151927	42.917095
3501.902356	584532.936254	42.922100
3502.239434	584519.951192	42.927105
3502.079193	584490.251904	42.932109
3502.222018	584466.119203	42.937114
3502.427762	584442.678369	42.942119
3502.241326	584413.885228	42.947124
3502.707177	584390.303370	42.952129
3502.317223	584369.762546	42.957133
3502.232708	584329.975689	42.962138
3502.408584	584305.185829	42.967143
3502.202570	584283.262682	42.972148
3502.276405	584244.403159	42.977153
3502.113276	584237.059988	42.982157
3502.247387	584203.303792	42.987162
3502.196207	584177.997748	42.992167
3502.405753	584159.167371	42.997172
3502.213284	584130.224048	43.002177
3501.933936	584110.116587	43.007181
3502.182526	584087.370076	43.012186
3502.299991	584073.817294	43.017191
3502.103480	584045.977178	43.022196
3501.951486	584018.982198	43.027201
3502.081287	583998.209042	43.032205
3502.247008	583976.277296	43.037210
3502.233268	583950.263087	43.042215
3501.964226	583926.995631	43.047220
3501.949825	583905.793693	43.052225
3501.923695	583893.215567	43.057229
3501.958881	583869.699918	43.062234
3502.199722	583844.999121	43.067239
3502.098375	583824.913439	43.072244
3502.815119	583796.929925	43.077249
3501.991669	583782.120277	43.082253
3501.973000	583758.111524	43.087258
3502.461134	583732.720144	43.092263
3502.514049	583708.649963	43.097268
3501.926839	583672.498456	43.102273
3501.580596	583670.998495	43.107277
3502.042066	583639.595585	43.112282
3501.861546	583618.168414	43.117287
3502.044089	583594.879788	43.122292
3502.428766	583572.211197	43.127297
3501.757173	583558.229707	43.132301
3501.989141	583527.714557	43.137306
3501.706775	583508.408540	43.142311
3501.902184	583498.652726	43.147316
3501.941312	583474.233279	43.152321
3501.824218	583459.463160	43.157325
3501.893904	583429.775188	43.162330
3502.297390	583413.118942	43.167335
3501.943999	583384.900632	43.172340
3502.144251	583359.352875	43.177345
3501.577213	583342.196545	43.182349
3502.298406	583319.274305	43.187354
3501.862512	583309.466622	43.192359
3501.646450	583292.806785	43.197364
3501.855487	583263.648019	43.202369
3501.815660	583249.667633	43.207373
3501.958046	583231.648264	43.212378
3501.800394	583195.026984	43.217383
3501.898162	583195.563054	43.222388
3501.880203	583157.917189	43.227393
3501.820512	583154.868418	43.232397
3501.799965	583143.341320	43.237402
3501.744137	583117.732772	43.242407
3501.497744	583105.890020	43.247412
3501.900385	583083.067221	43.252417
3501.428749	583082.789939	43.257421
3501.941913	583053.583074	43.262426
3502.215887	583035.041494	43.267431
3501.771143	583010.646529	43.272436
3501.689176	582988.450744	43.277441
3502.101656	582983.473224	43.282445
3501.756162	582958.661571	43.287450
3502.174703	582938.944188	43.292455
3501.960661	582917.370494	43.297460
3501.858181	582888.209301	43.302465
3501.797763	582858.690526	43.307469
3501.757169	582842.754567	43.312474
3502.099192	582826.859038	43.317479
3501.800833	582807.253491	43.322484
3501.675262	582783.259322	43.327489
3501.669255	582770.576501	43.332493
3501.817183	582754.560810	43.337498
3501.757004	582738.527496	43.342503
3501.865397	582732.644869	43.347508
3502.107783	582703.980742	43.352513
3501.541716	582692.738986	43.357517
3501.954107	582669.613007	43.362522
3501.874699	582651.025759	43.367527
3501.402826	582637.262538	43.372532
3501.550477	582617.436528	43.377537
3501.543663	582612.474255	43.382541
3501.497842	582588.667731	43.387546
3502.021153	582564.471380	43.392551
3501.857094	582565.098546	43.397556
3501.917217	582540.573479	43.402561
3501.843420	582516.871442	43.407565
3501.515882	582491.053242	43.412570
3501.889141	582485.981362	43.417575
3501.719793	582469.262840	43.422580
3501.966904	582445.109406	43.427585
3501.799019	582421.973354	43.432589
3501.983996	582406.903926	43.437594
3501.565712	582395.037145	43.442599
3501.818591	582376.798567	43.447604
3502.240585	582371.117398	43.452609
3501.734951	582339.360625	43.457613
3501.665896	582332.352418	43.462618
3501.731240	582304.366687	43.467623
3501.440546	582290.374166	43.472628
3501.808478	582277.632320	43.477633
3501.709195	582264.762957	43.482637
3501.215876	582243.281737	43.487642
3501.765114	582243.145652	43.492647
3501.694367	582216.835446	43.497652
3501.511372	582194.252769	43.502657
3501.688866	582184.548732	43.507661
3501.935261	582167.062859	43.512666
3501.810891	582155.500822	43.517671
3501.890099	582132.074855	43.522676
3501.937534	582111.110474	43.527681
3502.127420	582092.329778	43.532685
3501.608412	582073.359052	43.537690
3501.891453	582048.898317	43.542695
3501.767049	582036.533979	43.547700
3501.869226	582015.159767	43.552705
3501.742680	581997.481245	43.557709
3501.641607	581987.319216	43.562714
3502.196600	581961.712768	43.567719
3502.068615	581950.401766	43.572724
3502.025944	581923.785651	43.577729
3501.643580	581915.121501	43.582733
3502.221730	581896.430187	43.587738
3501.992036	581864.277948	43.592743
3501.490737	581834.323981	43.597748
3501.717675	581806.010902	43.602753
3501.838121	581805.691159	43.607757
3501.907109	581790.488613	43.612762
3501.783351	581774.213148	43.617767
3501.634762	581756.988925	43.622772
3502.049542	581740.428672	43.627777
3501.613669	581719.238276	43.632781
3501.527575	581693.079635	43.637786
3501.816888	581686.616651	43.642791
3501.592521	581662.134108	43.647796
3501.805625	581651.020168	43.652801
3501.606823	581637.363419	43.657805
3501.759661	581617.635082	43.662810
3501.738809	581604.100889	43.667815
3501.252773	581586.377630	43.672820
3501.825431	581569.942857	43.677825
3501.837504	581556.002350	43.682829
3501.652500	581543.546655	43.687834
3501.875007	581531.077381	43.692839
3501.613828	581510.410800	43.697844
3501.920608	581489.956226	43.702849
3501.943102	581471.752174	43.707853
3502.084917	581448.766223	43.712858
3501.797464	581435.273501	43.717863
3501.475230	581425.897616	43.722868
3501.358239	581415.286295	43.727873
3501.986893	581400.296557	43.732877
3501.736007	581381.733979	43.737882
3501.996198	581356.723754	43.742887
3501.532856	581332.879514	43.747892
3502.099977	581317.046909	43.752897
3501.511548	581296.431086	43.757901
3501.479678	581290.970739	43.762906
3501.543780	581266.341944	43.767911
3501.491577	581256.171602	43.772916
3501.759353	581247.405291	43.777921
3501.862594	581224.775885	43.782925
3501.716269	581214.369518	43.787930
3501.993362	581194.821565	43.792935
3501.661208	581184.343939	43.797940
3502.001967	581170.100862	43.802945
3501.842630	581140.342256	43.807949
3501.757897	581122.806219	43.812954
3501.830058	581096.019739	43.817959
3501.257756	581091.145185	43.822964
3501.877943	581067.782817	43.827969
3501.637724	581046.209556	43.832973
3501.412579	581051.208615	43.837978
3501.719419	581031.505301	43.842983
3501.466617	581011.538452	43.847988
3501.806342	580988.019196	43.852993
3501.843031	580980.692753	43.857997
3501.633081	580968.390734	43.863002
3501.543443	580948.448405	43.868007
3501.555226	580935.961262	43.873012
3501.881079	580915.753356	43.878017
3501.757236	580898.774635	43.883021
3501.652372	580876.126909	43.888026
3501.571467	580867.515090	43.893031
3501.684664	580842.426402	43.898036
3501.885800	580822.087397	43.903041
3501.934592	580820.224428	43.908045
3501.347413	580794.492990	43.913050
3501.767243	580786.153824	43.918055
3501.415866	580767.004217	43.923060
3501.636497	580752.177677	43.928065
3501.545271	580747.628902	43.933069
3501.242507	580726.365649	43.938074
3501.450936	580715.000791	43.943079
3501.449770	580705.724529	43.948084
3501.726361	580687.178610	43.953089
3502.017282	580662.663444	43.958093
3501.759526	580649.114976	43.963098
3501.927958	580634.848010	43.968103
3501.386420	580626.909727	43.973108
3501.914957	580601.855852	43.978113
3501.569493	580590.076026	43.983117
3501.392925	580570.347178	43.988122
3501.857231	580555.081138	43.993127
3501.968358	580543.731316	43.998132
3501.626133	580515.002484	44.003137
3501.405852	580510.273213	44.008141
3501.534226	580496.714339	44.013146
3501.878797	580483.572942	44.018151
3501.722175	580464.091505	44.023156
3501.799704	580448.384346	44.028161
3501.655640	580431.708932	44.033165
3501.420434	580423.672471	44.038170
3501.852972	580396.025664	44.043175
3501.073548	580378.697336	44.048180
3501.474204	580365.948185	44.053185
3501.897480	580360.315939	44.058189
3501.197653	580339.114014	44.063194
3501.421294	580331.356764	44.068199
3501.237936	580319.100010	44.073204
3501.459348	580287.875554	44.078209
3501.521868	580294.334313	44.083213
3501.287760	580294.571399	44.088218
3501.551242	580269.959367	44.093223
3501.318598	580255.052591	44.098228
3501.526817	580243.235984	44.103233
3501.658150	580232.484420	44.108237
3501.444118	580213.512964	44.113242
3501.858301	580200.761509	44.118247
3501.522793	580190.885202	44.123252
3501.402372	580167.937592	44.128257
3501.637449	580176.575821	44.133261
3501.549266	580158.086044	44.138266
3501.676923	580125.020424	44.143271
3501.383720	580122.157755	44.148276
3501.902226	580099.711864	44.153281
3501.650775	580091.878282	44.158285
3501.690499	580074.120549	44.163290
3501.893501	580046.558903	44.168295
3501.730947	580048.539898	44.173300
3501.553200	580013.716454	44.178305
3501.817846	580005.100091	44.183309
3501.584681	579993.853676	44.188314
3502.058481	579971.815683	44.193319
3501.753301	579958.875534	44.198324
3501.886049	579928.716993	44.203329
3501.639528	579923.239382	44.208333
3501.748995	579899.503090	44.213338
3501.695468	579877.146176	44.218343
3501.759115	579872.622977	44.223348
3501.788938	579842.380000	44.228353
3502.042466	579828.951186	44.233357
3501.704285	579812.204894	44.238362
3501.901364	579793.870503	44.243367
3501.424801	579773.785964	44.248372
3501.417651	579755.533583	44.253377
3501.375114	579757.445721	44.258381
3501.379651	579741.999709	44.263386
3501.830184	579716.755451	44.268391
3502.051438	579702.428886	44.273396
3502.149389	579681.652603	44.278401
3501.860454	579677.234589	44.283405
3501.631246	579646.730691	44.288410
3501.512661	579635.817032	44.293415
3501.714190	579626.909361	44.298420
3501.799904	579604.429837	44.303425
3501.610423	579593.075892	44.308429
3501.292790	579571.010387	44.313434
3501.487056	579555.684899	44.318439
3501.473001	579550.371353	44.323444
3501.767197	579527.157014	44.328449
3501.573849	579512.192948	44.333453
3501.487624	579507.241698	44.338458
3502.056689	579482.279268	44.343463
3501.681521	579465.337642	44.348468
3501.457053	579447.168876	44.353473
3501.291551	579442.831769	44.358477
3501.219654	579431.910611	44.363482
3501.843456	579421.382168	44.368487
3501.565641	579408.687840	44.373492
3502.054868	579388.953107	44.378497
3501.377913	579365.639507	44.383501
3501.625391	579344.237437	44.388506
3501.705042	579336.502005	44.393511
3501.533491	579319.829219	44.398516
3501.695143	579300.797473	44.403521
3501.544124	579288.434227	44.408525
3501.271976	579277.494073	44.413530
3501.693305	579254.810931	44.418535
3501.416914	579258.464779	44.423540
3501.642927	579240.726743	44.428545
3501.436851	579221.551752	44.433549
3501.088691	579216.039530	44.438554
3502.180518	579204.886078	44.443559
3502.045824	579194.776892	44.448564
3501.511340	579157.900264	44.453569
3501.491657	579132.427296	44.458573
3501.440775	579127.470352	44.463578
3501.662048	579123.574152	44.468583
3501.107388	579110.471415	44.473588
3501.367550	579100.350566	44.478593
3501.520329	579088.591552	44.483597
3501.578013	579076.797242	44.488602
3501.902252	579054.580220	44.493607
3501.796241	579036.843615	44.498612
3501.465233	579014.478196	44.503617
3501.198783	579012.212855	44.508621
3501.572682	579013.708969	44.513626
3501.266099	578981.760991	44.518631
3501.190431	578968.783807	44.523636
3501.266040	578957.788974	44.528641
3501.386330	578968.251502	44.533645
3501.343011	578947.295333	44.538650
3501.624654	578932.607286	44.543655
3501.467326	578929.372010	44.548660
3501.287240	578907.083083	44.553665
3501.872143	578884.473919	44.558669
3501.590436	578876.945112	44.563674
3501.358853	578853.811566	44.568679
3501.404028	578847.836464	44.573684
3501.671824	578845.136516	44.578689
3501.284941	578822.829597	44.583693
3501.422569	578799.487767	44.588698
3501.780319	578798.378580	44.593703
3501.538981	578786.028895	44.598708
3501.517092	578769.331887	44.603713
3501.250346	578765.913064	44.608717
3501.760586	578752.141917	44.613722
3501.781479	578732.780148	44.618727
3501.340255	578718.806641	44.623732
3501.698522	578707.065254	44.628737
3501.724334	578689.207185	44.633741
3501.125670	578670.744587	44.638746
3501.697613	578663.583703	44.643751
3501.779858	578642.807939	44.648756
3501.369544	578627.224628	44.653761
3501.483444	578622.542610	44.658765
3501.550402	578611.398333	44.663770
3501.434531	578597.674723	44.668775
3500.948146	578591.130606	44.673780
3501.442156	578567.933189	44.678785
3501.586445	578556.576160	44.683789
3501.472395	578551.428225	44.688794
3501.872865	578533.812252	44.693799
3501.249065	578516.757591	44.698804
3501.513981	578509.343691	44.703809
3501.538951	578498.406475	44.708813
3501.481966	578469.878526	44.713818
3501.782180	578460.804042	44.718823
3501.562884	578456.725721	44.723828
3501.445870	578441.798435	44.728833
3501.437137	578428.459090	44.733837
3501.452246	578421.535559	44.738842
3501.307999	578404.355605	44.743847
3501.860980	578401.962039	44.748852
3501.459524	578371.280963	44.753857
3501.357832	578356.250861	44.758861
3501.191032	578339.676170	44.763866
3501.437461	578340.440008	44.768871
3501.457852	578322.080668	44.773876
3501.617197	578307.661686	44.778881
3501.515264	578302.712356	44.783885
3501.155104	578282.807536	44.788890
3501.433481	578267.667746	44.793895
3501.200112	578262.939559	44.798900
3501.489443	578249.453098	44.803905
3501.586894	578247.130711	44.808909
3501.346730	578229.815023	44.813914
3501.653324	578213.216293	44.818919
3501.114348	578191.433423	44.823924
3501.359138	578177.151377	44.828929
3501.640996	578174.248454	44.833933
3501.469140	578164.294604	44.838938
3501.443060	578140.274835	44.843943
3501.359292	578134.770896	44.848948
3501.421149	578128.592186	44.853953
3501.229853	578133.085715	44.858957
3500.922225	578105.849870	44.863962
3501.528491	578105.955622	44.868967
3500.947438	578098.523237	44.873972
3501.244767	578095.216642	44.878977
3501.092185	578085.109245	44.883981
3501.219061	578068.438088	44.888986
3501.843965	578064.428269	44.893991
3501.163212	578053.952022	44.898996
3501.015907	578038.527388	44.904001
3501.208718	578017.382096	44.909005
3501.253929	578016.572466	44.914010
3501.574010	577996.560795	44.919015
3501.063124	578008.477069	44.924020
3501.226997	577984.126342	44.929025
3501.289948	577966.161002	44.934029
3501.296727	577968.918368	44.939034
3501.654792	577961.940939	44.944039
3501.138150	577942.611677	44.949044
3501.428976	577920.899176	44.954049
3501.505498	577922.040690	44.959053
3501.328591	577916.952444	44.964058
3501.469737	577880.467519	44.969063
3501.232189	577889.331877	44.974068
3501.444581	577874.402492	44.979073
3501.601919	577868.359178	44.984077
3501.273913	577843.483176	44.989082
3501.361132	577839.808110	44.994087
3501.341119	577838.557265	44.999092
3500.880935	577816.259790	45.004097
3501.138359	577800.270002	45.009101
3501.606013	577799.243850	45.014106
3501.701497	577799.981167	45.019111
3501.223885	577773.272641	45.024116
3501.450906	577764.861060	45.029121
3501.485359	577759.388610	45.034125
3501.013920	577749.130132	45.039130
3501.016984	577726.158189	45.044135
3501.536385	577729.838595	45.049140
3501.185875	577718.558067	45.054145
3501.290207	577707.707982	45.059149
3501.166904	577699.250806	45.064154
3501.239309	577684.192584	45.069159
3501.039995	577668.073384	45.074164
3501.479287	577671.415239	45.079169
3501.313765	577669.735717	45.084173
3501.163256	577650.248400	45.089178
3501.375948	577634.716774	45.094183
3501.285124	577633.727757	45.099188
3501.304762	577625.599274	45.104193
3501.335495	577609.243401	45.109197
3501.199419	577599.283453	45.114202
3501.341516	577591.436740	45.119207
3501.023363	577594.846872	45.124212
3501.019736	577587.875597	45.129217
3501.104222	577567.849834	45.134221
3501.222356	577565.172977	45.139226
3501.168666	577544.015170	45.144231
3501.427332	577555.209742	45.149236
3500.894111	577535.882366	45.154241
3501.367052	577517.300490	45.159245
3500.934006	577504.427629	45.164250
3501.504372	577503.034296	45.169255
3500.971752	577499.957586	45.174260
3501.160816	577494.159896	45.179265
3501.451717	577481.023364	45.184269
3501.553546	577469.069986	45.189274
3501.095564	577452.840441	45.194279
3501.083565	577465.231029	45.199284
3501.258677	577455.924505	45.204289
3501.518518	577440.335083	45.209293
3501.362154	577440.409595	45.214298
3501.146074	577428.154772	45.219303
3501.130003	577430.364113	45.224308
3501.281245	577394.628385	45.229313
3501.276258	577387.757513	45.234317
3501.298825	577384.242877	45.239322
3501.508413	577377.539084	45.244327
3501.238604	577360.176524	45.249332
3501.294744	577347.979372	45.254337
3501.355583	577340.345816	45.259341
3501.302490	577337.194097	45.264346
3501.311141	577313.518227	45.269351
3501.189558	577309.474367	45.274356
3501.278107	577298.776828	45.279361
3501.507765	577300.797307	45.284365
3501.021773	577279.505950	45.289370
3501.635148	577257.541111	45.294375
3501.292726	577268.478830	45.299380
3501.217957	577255.449357	45.304385
3501.457648	577228.677552	45.309389
3501.347967	577217.409026	45.314394
3501.348401	577224.130062	45.319399
3501.311592	577219.822127	45.324404
3501.167223	577185.436056	45.329409
3501.632575	577182.905462	45.334413
3501.117262	577174.007587	45.339418
3501.664133	577167.250943	45.344423
3501.687755	577139.810485	45.349428
3501.606250	577136.763468	45.354433
3501.514389	577119.523191	45.359437
3501.326952	577104.956240	45.364442
3501.347889	577100.338279	45.369447
3501.722194	577099.276502	45.374452
3501.718518	577070.586175	45.379457
3501.552987	577063.690043	45.384461
3501.651000	577043.661229	45.389466
3501.653633	577027.660013	45.394471
3501.145532	577029.645397	45.399476
3501.290434	577004.844077	45.404481
3501.656198	576986.829829	45.409485
3501.194464	576978.976765	45.414490
3501.771221	576970.911192	45.419495
3501.371171	576959.236366	45.424500
3501.522547	576937.192647	45.429505
3501.050291	576933.805384	45.434509
3500.935359	576932.168001	45.439514
3501.376859	576918.004080	45.444519
3501.329438	576910.487475	45.449524
3501.135146	576891.306638	45.454529
3500.865738	576890.596270	45.459533
3500.774522	576895.626403	45.464538
3501.278090	576886.468699	45.469543
3501.466268	576872.845919	45.474548
3500.997921	576854.660896	45.479553
3501.315185	576855.112808	45.484557
3501.072920	576853.344839	45.489562
3501.141865	576832.116357	45.494567
3501.598190	576821.461189	45.499572
3501.429466	576802.627323	45.504577
3501.687891	576806.449156	45.509581
3501.311377	576794.820639	45.514586
3501.452542	576781.857179	45.519591
3501.210528	576770.859692	45.524596
3501.395726	576765.814634	45.529601
3501.478724	576747.894368	45.534605
3501.311027	576735.731542	45.539610
3501.359179	576718.569082	45.544615
3501.045144	576720.724822	45.549620
3501.451077	576698.289718	45.554625
3500.846579	576689.756520	45.559629
3501.160318	576685.042455	45.564634
3501.232902	576680.968014	45.569639
3501.046296	576684.809299	45.574644
3501.342108	576663.595194	45.579649
3501.307140	576656.477757	45.584653
3501.032578	576645.134110	45.589658
3501.233333	576640.387528	45.594663
3501.571581	576639.883115	45.599668
3501.388695	576608.360458	45.604673
3501.775141	576607.447222	45.609677
3501.398578	576595.918827	45.614682
3501.247825	576562.083613	45.619687
3501.149663	576567.917556	45.624692
3501.436005	576557.790324	45.629697
3501.183580	576547.546662	45.634701
3500.899634	576539.264205	45.639706
3501.270765	576519.241922	45.644711
3501.135024	576518.209665	45.649716
3501.116220	576512.795095	45.654721
3501.157368	576515.748091	45.659725
3501.104416	576502.714332	45.664730
3501.284731	576483.875527	45.669735
3501.218401	576487.999046	45.674740
3501.397099	576480.246158	45.679745
3501.311894	576472.384037	45.684749
3501.063667	576458.979462	45.689754
3501.464298	576441.911962	45.694759
3501.464134	576448.081778	45.699764
3501.431195	576421.200184	45.704769
3501.260119	576400.961482	45.709773
3501.155911	576390.092563	45.714778
3501.278026	576385.558815	45.719783
3501.104300	576384.582647	45.724788
3500.987017	576372.812841	45.729793
3501.328322	576354.851568	45.734797
3501.070118	576355.293140	45.739802
3501.252709	576346.736960	45.744807
3500.997478	576353.448323	45.749812
3501.162144	576339.728249	45.754817
3501.426416	576310.041011	45.759821
3500.936349	576251.527901	45.764826
3501.203445	576149.003631	45.769831
3500.750819	576010.372905	45.774836
3500.433594	575801.639724	45.779841
3500.005189	575557.854366	45.784845
3499.514723	575267.167503	45.789850
3499.289196	574932.634831	45.794855
3498.513336	574548.710698	45.799860
3497.996565	574127.405152	45.804865
3497.339993	573662.855868	45.809869
3496.405555	573160.698869	45.814874
3495.710794	572604.138794	45.819879
3494.491698	572017.775619	45.824884
3493.828038	571380.709977	45.829889
3492.564681	570723.226250	45.834893
3491.564644	570001.570926	45.839898
3490.376904	569246.119359	45.844903
3488.450826	568456.147914	45.849908
3487.288923	567622.027213	45.854913
3486.109550	566768.771370	45.859917
3484.370303	565875.725194	45.864922
3483.594681	564931.343765	45.869927
3481.650195	563969.844267	45.874932
3479.945241	562959.463971	45.879937
3478.179101	561904.858230	45.884941
3476.229320	560841.547028	45.889946
3474.622920	559720.567915	45.894951
3472.445706	558596.607714	45.899956
3470.358660	557430.221512	45.904961
3468.430510	556238.370757	45.909965
3466.208931	555014.887482	45.914970
3464.239570	553754.651238	45.919975
3461.772598	552482.950977	45.924980
3459.667870	551185.623818	45.929985
3457.491764	549856.646595	45.934989
3455.104056	548503.422863	45.939994
3453.031689	547122.393077	45.944999
3450.359436	545719.927972	45.950004
3447.826853	544285.091200	45.955009
3445.075831	542833.623276	45.960013
3442.140420	541356.759923	45.965018
3439.366708	539878.490045	45.970023
3436.706876	538379.296569	45.975028
3434.125602	536865.268202	45.980033
3430.943389	535318.990559	45.985037
3428.353050	533765.738609	45.990042
3425.410984	532195.589130	45.995047
3422.545742	530623.676436	46.000052
3419.718846	529015.309921	46.005057
3416.854388	527394.966445	46.010061
3412.925298	525768.092253	46.015066
3410.377581	524127.653843	46.020071
3407.071987	522482.950159	46.025076
3403.738318	520823.032916	46.030081
3400.947650	519151.688913	46.035085
3397.601643	517469.641336	46.040090
3394.515723	515768.140152	46.045095
3390.892144	514070.343646	46.050100
3387.651129	512367.135709	46.055105
3384.269350	510649.117236	46.060109
3380.913263	508932.194966	46.065114
3377.332184	507196.284556	46.070119
3374.321325	505459.769586	46.075124
3370.629570	503714.471885	46.080129
3366.970943	501971.984197	46.085133
3363.237136	500207.396728	46.090138
3360.290709	498451.607091	46.095143
3356.538605	496697.802360	46.100148
3352.920862	494919.587008	46.105153
3349.395205	493135.237051	46.110157
3345.943156	491363.387016	46.115162
3342.299515	489582.571265	46.120167
3338.662205	487805.838210	46.125172
3335.142562	486032.819774	46.130177
3331.677037	484236.299654	46.135181
3327.688955	482454.658166	46.140186
3324.292857	480663.473616	46.145191
3320.209155	478874.718980	46.150196
3316.928989	477082.149081	46.155201
3313.582901	475292.572234	46.160205
3309.578454	473492.333430	46.165210
3305.810927	471694.385038	46.170215
3302.352558	469914.594875	46.175220
3298.507329	468117.276644	46.180225
3294.892754	466309.460514	46.185229
3290.780834	464522.971806	46.190234
3287.554490	462722.597882	46.195239
3283.482848	460935.267541	46.200244
3279.537096	459136.042708	46.205249
3276.144811	457341.248967	46.210253
3272.264316	455548.724216	46.215258
3268.533670	453757.358643	46.220263
3264.879426	451975.466653	46.225268
3261.001711	450187.558719	46.230273
3257.473589	448389.950426	46.235277
3253.443152	446609.861381	46.240282
3250.169331	444818.998205	46.245287
3246.298671	443036.054915	46.250292
3242.178979	441240.773078	46.255297
3238.649328	439461.080037	46.260301
3234.763038	437683.857940	46.265306
3231.004007	435904.119194	46.270311
3227.420182	434127.024893	46.275316
3223.171635	432340.446465	46.280321
3219.585646	430566.319901	46.285325
3215.522823	428805.132267	46.290330
3211.867215	427047.779231	46.295335
3208.244687	425287.174738	46.300340
3204.260801	423508.984420	46.305345
3200.427062	421752.161485	46.310349
3196.546517	420007.262564	46.315354
3193.041263	418257.645476	46.320359
3188.951391	416502.344895	46.325364
3185.584522	414754.189672	46.330369
3181.641908	413018.356351	46.335373
3177.666322	411268.541265	46.340378
3174.396914	409522.837364	46.345383
3170.481681	407776.385430	46.350388
3166.563557	406032.434514	46.355393
3162.746173	404302.335576	46.360397
3158.967594	402574.077082	46.365402
3155.309311	400832.728893	46.370407
3151.568978	399106.740533	46.375412
3147.812672	397387.630676	46.380417
3144.219074	395661.162352	46.385421
3139.993364	393945.073327	46.390426
3135.997705	392219.332876	46.395431
3132.410946	390512.849684	46.400436
3128.481516	388807.443681	46.405441
3125.087874	387100.846447	46.410445
3120.771554	385403.341058	46.415450
3117.160981	383699.949394	46.420455
3113.369591	382001.373346	46.425460
3109.840176	380315.392577	46.430465
3105.574222	378620.758445	46.435469
3101.836491	376954.758907	46.440474
3098.426180	375276.641610	46.445479
3094.570091	373589.142612	46.450484
3090.869713	371915.155978	46.455489
3087.002908	370226.842834	46.460493
3083.299086	368576.662163	46.465498
3079.342091	366903.711687	46.470503
3075.617516	365245.795705	46.475508
3072.078166	363579.752095	46.480513
3068.741920	361916.809359	46.485517
3064.259504	360266.557221	46.490522
3060.696473	358607.506462	46.495527
3057.255021	356961.384180	46.500532
3053.013145	355309.453511	46.505537
3049.760406	353666.634487	46.510541
3045.700229	352032.956406	46.515546
3042.157938	350395.987423	46.520551
3038.588489	348760.414642	46.525556
3034.371907	347115.506258	46.530561
3031.021814	345485.457652	46.535565
3026.995800	343870.614969	46.540570
3023.516092	342232.955974	46.545575
3019.973317	340614.554594	46.550580
3015.858429	338989.200951	46.555585
3012.364064	337372.678552	46.560589
3008.158757	335768.453005	46.565594
3004.559019	334147.226871	46.570599
3000.676522	332546.092191	46.575604
2997.446480	330930.697367	46.580609
2993.786973	329325.984736	46.585613
2989.862204	327725.546464	46.590618
2986.125967	326131.093726	46.595623
2982.658366	324537.273687	46.600628
2978.510224	322944.770077	46.605633
2975.231129	321351.026660	46.610637
2971.363421	319766.194299	46.615642
2967.371839	318176.997852	46.620647
2963.595503	316601.220330	46.625652
2959.829157	315022.179615	46.630657
2956.726293	313441.326274	46.635661
2952.547851	311867.330106	46.640666
2949.181495	310290.940410	46.645671
2945.367284	308740.499643	46.650676
2941.355889	307166.195589	46.655681
2937.986504	305605.941767	46.660685
2933.994631	304046.042666	46.665690
2930.508228	302495.739506	46.670695
2926.945804	300936.723822	46.675700
2923.415648	299377.708843	46.680705
2919.312158	297820.011929	46.685709
2915.711392	296284.286625	46.690714
2912.385121	294721.597896	46.695719
2908.366334	293189.037745	46.700724
2904.718184	291639.019971	46.705729
2901.560523	290102.276153	46.710733
2897.625859	288560.321303	46.715738
2893.719572	287020.081611	46.720743
2890.042752	285484.632489	46.725748
2886.486343	283956.385291	46.730753
2882.798621	282421.352929	46.735757
2878.954816	280905.610111	46.740762
2875.078763	279365.857738	46.745767
2871.381808	277851.582645	46.750772
2867.881010	276327.775819	46.755777
2864.317449	274807.055984	46.760781
2860.448544	273302.447644	46.765786
2857.047988	271782.130980	46.770791
2853.465370	270269.607974	46.775796
2849.564995	268755.454273	46.780801
2846.138168	267247.313270	46.785805
2842.293179	265751.436888	46.790810
2838.776579	264244.944677	46.795815
2835.104233	262743.216978	46.800820
2831.273940	261248.063179	46.805825
2827.720625	259752.922690	46.810829
2824.119251	258268.873785	46.815834
2820.632887	256760.137995	46.820839
2816.957630	255272.067230	46.825844
2813.039712	253782.693815	46.830849
2809.434491	252286.176175	46.835853
2805.984355	250801.283277	46.840858
2802.392273	249320.549879	46.845863
2798.629578	247843.955902	46.850868
2794.898624	246369.254909	46.855873
2791.321298	244890.825740	46.860877
2787.382511	243412.340651	46.865882
2783.913650	241938.967788	46.870887
2780.032016	240478.664858	46.875892
2776.089055	238998.676382	46.880897
2772.840462	237537.214867	46.885901
2769.119206	236083.486856	46.890906
2765.323490	234615.476832	46.895911
2761.614353	233164.818016	46.900916
2758.103325	231717.002058	46.905921
2754.565748	230263.354467	46.910925
2751.044445	228807.740552	46.915930
2747.007837	227361.858081	46.920935
2743.834134	225923.938660	46.925940
2739.753986	224479.487700	46.930945
2736.393769	223025.628262	46.935949
2732.868096	221598.716534	46.940954
2729.249162	220152.566588	46.945959
2725.484248	218710.950009	46.950964
2721.551104	217287.980737	46.955969
2717.995187	215843.180521	46.960973
2714.102475	214418.787206	46.965978
2710.975463	212989.669623	46.970983
2707.328517	211558.882086	46.975988
2703.527430	210139.433395	46.980993
2700.074243	208706.337637	46.985997
2696.502957	207293.286496	46.991002
2692.657723	205870.583628	46.996007
2689.043189	204450.553785	47.001012
2685.409107	203042.863480	47.006017
2681.724289	201629.105112	47.011021
2678.151018	200224.356144	47.016026
2674.340140	198806.821030	47.021031
2671.141315	197402.267520	47.026036
2667.108862	196010.438179	47.031041
2663.632495	194599.308701	47.036045
2660.064051	193204.863180	47.041050
2656.276671	191797.683347	47.046055
2652.984397	190399.278677	47.051060
2649.420096	189002.257342	47.056065
2645.752688	187604.047072	47.061069
2642.454583	186216.899438	47.066074
2638.324269	184815.589509	47.071079
2634.964422	183434.141939	47.076084
2630.930609	182031.277307	47.081089
2627.687326	180654.103700	47.086093
2624.061819	179269.524529	47.091098
2620.313819	177883.483761	47.096103
2616.779162	176498.170220	47.101108
2613.170655	175119.179999	47.106113
2609.765890	173727.094308	47.111117
2605.929196	172360.242687	47.116122
2602.257675	170978.418913	47.121127
2598.242577	169603.204535	47.126132
2594.369691	168236.369623	47.131137
2591.248945	166863.142104	47.136141
2587.825671	165500.375656	47.141146
2584.229794	164139.165302	47.146151
2580.355571	162767.894279	47.151156
2577.074815	161414.022242	47.156161
2573.303209	160054.044336	47.161165
2569.595228	158697.216952	47.166170
2565.921515	157342.348714	47.171175
2562.177606	155988.285552	47.176180
2558.501610	154635.731845	47.181185
2555.193918	153282.859402	47.186189
2550.874339	151932.239080	47.191194
2547.490305	150592.627551	47.196199
2544.196321	149255.350750	47.201204
2540.502065	147917.609883	47.206209
2536.983737	146557.148635	47.211213
2532.995711	145166.741024	47.216218
2529.572138	143830.628200	47.221223
2525.940629	142500.449177	47.226228
2522.398828	141176.755513	47.231233
2518.985098	139846.601749	47.236237
2515.183771	138528.505072	47.241242
2511.643874	137188.916089	47.246247
2507.992467	135872.041326	47.251252
2504.385282	134548.035240	47.256257
2500.695127	133235.670233	47.261261
2497.171957	131924.908032	47.266266
2493.443030	130604.956667	47.271271
2490.203992	129298.109047	47.276276
2486.390875	127985.476632	47.281281
2483.004226	126670.885202	47.286285
2479.348063	125371.818558	47.291290
2475.868505	124047.264745	47.296295
2471.992636	122742.402450	47.301300
2467.947154	121439.008410	47.306305
2464.610971	120134.491096	47.311309
2460.855439	118842.418638	47.316314
2457.369375	117552.534806	47.321319
2453.372825	116259.608446	47.326324
2449.733376	114971.884300	47.331329
2446.868327	113688.864756	47.336333
2442.904978	112407.282650	47.341338
2439.021028	111116.744579	47.346343
2435.708850	109837.046713	47.351348
2431.873869	108579.916065	47.356353
2428.546990	107279.184058	47.361357
2424.468180	106005.213006	47.366362
2420.679889	104732.883834	47.371367
2417.442923	103471.397302	47.376372
2413.624605	102218.260559	47.381377
2410.354422	100942.409950	47.386381
2406.611504	99682.799235	47.391386
2402.994322	98429.496252	47.396391
2399.388351	97160.875221	47.401396
2395.225177	95911.861394	47.406401
2392.418470	94659.952698	47.411405
2388.376636	93408.859303	47.416410
2384.706126	92163.756196	47.421415
2381.006793	90914.464319	47.426420
2377.512714	89677.605527	47.431425
2373.624310	88429.564267	47.436429
2369.909558	87205.128446	47.441434
2366.635526	85968.325914	47.446439
2362.992442	84741.796511	47.451444
2359.461306	83509.191276	47.456449
2355.860191	82285.770470	47.461453
2352.165639	81065.998896	47.466458
2348.281077	79836.669261	47.471463
2344.700707	78606.952342	47.476468
2341.061223	77401.988967	47.481473
2337.176887	76187.490136	47.486477
2333.510729	74977.697324	47.491482
2330.131412	73776.142570	47.496487
2326.388514	72580.577778	47.501492
2322.997659	71383.335514	47.506497
2319.090561	70179.270277	47.511501
2315.179532	68993.658225	47.516506
2312.108153	67795.558615	47.521511
2308.709983	66606.636573	47.526516
2304.620413	65417.135257	47.531521
2301.199628	64234.757199	47.536525
2297.365659	63057.570284	47.541530
2293.443183	61879.449830	47.546535
2290.239137	60703.551115	47.551540
2286.400314	59543.101310	47.556545
2283.071737	58367.359207	47.561549
2278.943269	57207.122900	47.566554
2274.995244	56041.133855	47.571559
2271.694169	54883.240488	47.576564
2267.940292	53730.162728	47.581569
2264.777270	52582.035164	47.586573
2260.955913	51437.276630	47.591578
2257.183164	50292.547628	47.596583
2253.704329	49152.510394	47.601588
2249.715807	48005.499082	47.606593
2246.375034	46870.875195	47.611597
2242.280941	45745.152614	47.616602
2238.815596	44612.151764	47.621607
2235.216708	43495.957945	47.626612
2231.334701	42375.989832	47.631617
2227.840842	41258.902714	47.636621
2224.195427	40159.573462	47.641626
2220.216452	39044.748290	47.646631
2216.402661	37938.532326	47.651636
2212.405159	36847.711826	47.656641
2209.066427	35766.466650	47.661645
2205.334770	34673.686671	47.666650
2201.593220	33598.699937	47.671655
2197.927915	32522.146067	47.676660
2193.674824	31451.754096	47.681665
2190.064271	30390.803955	47.686669
2185.876101	29335.214024	47.691674
2182.377047	28282.478939	47.696679
2178.505613	27247.415044	47.701684
2174.456650	26208.090969	47.706689
2171.273604	25171.782920	47.711693
2167.209073	24152.259173	47.716698
2163.177276	23129.829722	47.721703
2159.946644	22118.546623	47.726708
2155.742458	21122.499621	47.731713
2151.959476	20131.352372	47.736717
2147.960013	19144.602405	47.741722
2144.415064	18158.008353	47.746727
2140.763727	17178.644019	47.751732
2136.534237	16211.215083	47.756737
2133.283598	15257.031111	47.761741
2129.414570	14305.198128	47.766746
2125.432077	13354.870820	47.771751
2121.460814	12420.377797	47.776756
2117.014969	11490.000323	47.781761
2113.304111	10581.086456	47.786765
2108.635794	9686.044464	47.791770
2104.555940	8801.088665	47.796775
2100.207443	7932.764594	47.801780
2095.667133	7089.366353	47.806785
2090.540094	6259.818311	47.811789
2084.027339	5503.570749	47.816794
2075.884246	4837.830863	47.821799
2068.528268	4199.802246	47.826804
2061.428196	3617.586424	47.831809
2054.651682	3084.379937	47.836813
2048.320265	2605.488134	47.841818
2042.918574	2171.597746	47.846823
2037.558280	1775.535379	47.851828
2032.136654	1428.854012	47.856833
2027.639977	1110.501282	47.861837
2022.903145	835.111001	47.866842
2018.131869	575.600595	47.871847
2013.787742	362.191350	47.876852
2009.242500	177.724248	47.881857
2000.467769	125.450921	47.886861
1990.688796	154.598207	47.891866
1985.095431	147.440321	47.896871
1982.219967	146.491747	47.901876
1980.510642	149.945120	47.906881
1979.319213	149.194960	47.911885
1977.691921	143.536269	47.916890
1975.795676	141.861818	47.921895
1973.209728	134.151099	47.926900
1970.108685	151.135712	47.931905
1967.167864	149.343130	47.936909
1963.847630	147.986416	47.941914
1960.690042	136.422993	47.946919
1957.342705	134.962953	47.951924
1954.231173	149.165024	47.956929
1950.699309	138.833957	47.961933
1947.528277	145.037643	47.966938
1944.301202	147.909078	47.971943
1941.753713	144.093371	47.976948
1938.105685	146.309320	47.981953
1935.039761	144.707172	47.986957
1931.628618	149.682897	47.991962
1927.928372	139.454120	47.996967
1924.568876	147.784933	48.001972
1921.077076	142.680611	48.006977
1917.430701	139.713928	48.011981
1914.912196	144.768282	48.016986
1911.537669	147.242007	48.021991
1907.765853	142.013824	48.026996
1904.236362	150.997686	48.032001
1900.865407	151.430175	48.037005
1897.539602	149.909834	48.042010
1894.389117	145.172903	48.047015
1891.608261	142.614972	48.052020
1887.405763	141.794987	48.057025
1883.547334	137.228957	48.062029
1880.157465	140.692211	48.067034
1876.717925	143.267872	48.072039
1873.820973	136.371500	48.077044
1870.221867	142.148632	48.082049
1867.132759	132.248207	48.087053
1864.314553	133.328222	48.092058
1860.242842	134.531625	48.097063
1857.002521	133.288996	48.102068
1852.959158	145.112153	48.107073
1849.710187	132.854376	48.112077
1846.611210	139.407487	48.117082
1842.988668	134.617894	48.122087
1839.728737	129.888621	48.127092
1835.742256	134.986041	48.132097
1832.400646	144.665037	48.137101
1829.183736	135.945755	48.142106
1825.388382	141.854853	48.147111
1822.026603	130.804347	48.152116
1818.516617	143.018621	48.157121
1815.428737	136.952600	48.162125
1811.977785	136.815489	48.167130
1808.039916	136.976046	48.172135
1804.899232	133.066541	48.177140
1800.934998	145.586031	48.182145
1798.020337	141.195055	48.187149
1794.596945	139.690020	48.192154
1791.119155	139.446381	48.197159
1788.043936	127.028562	48.202164
1784.015174	139.988433	48.207169
1780.737118	136.609812	48.212173
1777.119367	133.607065	48.217178
1773.551502	138.594702	48.222183
1770.280545	135.613618	48.227188
1766.574629	132.507610	48.232193
1763.118610	128.995492	48.237197
1759.345115	136.385028	48.242202
1755.986271	138.891148	48.247207
1753.110441	135.035127	48.252212
1749.693139	140.119435	48.257217
1745.955559	131.487997	48.262221
1741.920557	128.300620	48.267226
1738.645765	133.985903	48.272231
1735.559076	133.529213	48.277236
1731.790834	130.980317	48.282241
1728.682268	129.967053	48.287245
1725.246013	124.923722	48.292250
1720.975583	128.385619	48.297255
1717.587417	122.926630	48.302260
1714.275485	134.945408	48.307265
1711.099109	125.308647	48.312269
1707.526956	119.963881	48.317274
1703.811037	133.918876	48.322279
1700.550761	128.196261	48.327284
1696.837557	128.328028	48.332289
1693.587019	122.360279	48.337293
1689.872943	127.513193	48.342298
1686.530053	129.741582	48.347303
1683.496754	121.708654	48.352308
1679.704966	130.553276	48.357313
1676.148825	122.782516	48.362317
1672.518921	129.152995	48.367322
1669.053004	128.265281	48.372327
1665.601978	119.313784	48.377332
1662.328440	136.996159	48.382337
1658.675083	130.705474	48.387341
1655.053451	134.537269	48.392346
1651.264089	130.928660	48.397351
1647.687958	130.422044	48.402356
1644.524328	133.625326	48.407361
1641.218947	124.075224	48.412365
1638.176225	130.603759	48.417370
1634.556933	130.040625	48.422375
1631.066472	129.403545	48.427380
1627.203737	129.574558	48.432385
1623.606769	129.672340	48.437389
1620.368520	134.690694	48.442394
1616.496351	131.237432	48.447399
1613.427814	126.626986	48.452404
1609.317794	138.261319	48.457409
1605.948968	137.516622	48.462413
1602.665838	129.190619	48.467418
1599.620290	123.067432	48.472423
1595.998249	123.308356	48.477428
1592.242787	122.307794	48.482433
1588.645775	124.575985	48.487437
1585.074114	125.935353	48.492442
1581.498554	130.032049	48.497447
1578.443301	124.511516	48.502452
1575.289816	123.799567	48.507457
1571.761073	131.337518	48.512461
1567.951438	130.740922	48.517466
1564.096768	118.872312	48.522471
1560.658342	125.371046	48.527476
1556.804002	129.093757	48.532481
1553.667048	117.571575	48.537485
1550.331596	121.421886	48.542490
1546.657061	124.749453	48.547495
1543.723262	117.435015	48.552500
1540.211393	121.667290	48.557505
1536.531761	113.529933	48.562509
1532.747234	122.310181	48.567514
1529.140439	118.157345	48.572519
1525.744695	103.926321	48.577524
1522.842270	114.767365	48.582529
1518.915082	108.446837	48.587533
1515.329325	112.785598	48.592538
1511.936924	114.775009	48.597543
1508.324351	108.661514	48.602548
1504.724107	121.620819	48.607553
1501.107666	120.044862	48.612557
1497.880063	118.841489	48.617562
1494.444933	123.548998	48.622567
1490.987312	115.076347	48.627572
1487.382870	123.224130	48.632577
1483.933796	109.118529	48.637581
1480.275794	106.359488	48.642586
1476.711311	113.526557	48.647591
1473.573399	105.937205	48.652596
1469.531439	119.111192	48.657601
1466.443982	112.266934	48.662605
1463.101989	109.581825	48.667610
1459.456754	112.677037	48.672615
1456.188626	119.164962	48.677620
1452.271917	116.452750	48.682625
1448.747280	110.502689	48.687629
1445.403038	108.146976	48.692634
1441.954482	104.345905	48.697639
1438.618850	104.412338	48.702644
1434.545354	110.827006	48.707649
1431.144040	104.398896	48.712653
1427.777792	115.559338	48.717658
1424.345947	111.727181	48.722663
1421.350489	106.947177	48.727668
1417.585990	114.870088	48.732673
1413.983874	105.841111	48.737677
1410.421777	103.636573	48.742682
1406.529683	108.244786	48.747687
1403.630728	107.746157	48.752692
1399.691213	113.820320	48.757697
1396.618397	101.807273	48.762701
1393.009160	108.623858	48.767706
1388.869480	121.936554	48.772711
1385.761735	111.074278	48.777716
1382.689623	104.544035	48.782721
1379.094944	97.405881	48.787725
1375.483695	112.315849	48.792730
1371.661386	121.488046	48.797735
1368.138176	111.149566	48.802740
1364.502435	114.600836	48.807745
1361.385236	116.053661	48.812749
1358.153525	110.215975	48.817754
1354.622437	107.041637	48.822759
1351.160524	100.233895	48.827764
1347.507694	106.114498	48.832769
1343.601917	105.112251	48.837773
1340.453756	105.285416	48.842778
1336.793283	114.324717	48.847783
1333.212715	97.404993	48.852788
1329.730541	107.691403	48.857793
1326.664707	106.253953	48.862797
1323.178879	111.564246	48.867802
1319.424037	111.120525	48.872807
1315.597536	104.034503	48.877812
1312.536386	105.731673	48.882817
1308.837162	104.858462	48.887821
1305.497090	94.431239	48.892826
1302.162318	109.740878	48.897831
1298.679540	97.712953	48.902836
1294.694763	109.520753	48.907841
1291.322392	106.365888	48.912845
1287.754919	102.377843	48.917850
1284.208043	99.152220	48.922855
1281.204282	93.101711	48.927860
1277.441607	101.249006	48.932865
1273.785700	100.400666	48.937869
1270.430781	97.534150	48.942874
1266.940913	97.324222	48.947879
1263.345523	98.712725	48.952884
1259.919316	100.353161	48.957889
1256.232500	99.860850	48.962893
1252.771269	100.643048	48.967898
1249.105695	102.770222	48.972903
1245.960402	99.700052	48.977908
1242.489118	98.519095	48.982913
1238.802605	100.640058	48.987917
1235.299143	94.215366	48.992922
1231.752232	107.118922	48.997927
1228.585046	106.121323	49.002932
1224.640416	106.773557	49.007937
1221.151818	109.047046	49.012941
1217.941189	106.458522	49.017946
1214.160744	110.669666	49.022951
1211.223978	108.066746	49.027956
1207.362017	107.007074	49.032961
1204.118217	114.294868	49.037965
1200.542552	99.149346	49.042970
1196.658733	109.451212	49.047975
1193.406030	107.733006	49.052980
1189.370010	105.026930	49.057985
1186.060802	101.463575	49.062989
1182.838446	99.734295	49.067994
1179.644829	112.180754	49.072999
1176.075217	102.605783	49.078004
1172.512474	108.298329	49.083009
1168.785279	102.525631	49.088013
1165.587378	105.019390	49.093018
1161.837699	111.282218	49.098023
1158.351823	95.622781	49.103028
1154.489552	110.559443	49.108033
1151.080743	104.784364	49.113037
1147.783950	98.330515	49.118042
1143.982902	105.857425	49.123047
1140.785670	96.160899	49.128052
1137.461973	99.465314	49.133057
1133.992430	97.227409	49.138061
1130.384816	98.478665	49.143066
1126.793079	109.902274	49.148071
1123.304837	106.648550	49.153076
1119.584750	109.591079	49.158081
1116.235456	104.461608	49.163085
1113.060182	101.712559	49.168090
1109.156495	109.002446	49.173095
1105.526418	101.344755	49.178100
1102.209182	102.797338	49.183105
1098.714010	103.050218	49.188109
1095.595142	108.679623	49.193114
1091.754534	108.967605	49.198119
1088.284498	105.840761	49.203124
1085.055948	100.663925	49.208129
1081.268272	104.487098	49.213133
1077.862130	110.069733	49.218138
1074.272712	105.800465	49.223143
1070.675603	101.098961	49.228148
1066.900756	99.620739	49.233153
1063.822470	105.193177	49.238157
1060.655508	102.980694	49.243162
1056.874300	105.983435	49.248167
1053.680157	106.230331	49.253172
1049.763692	114.237263	49.258177
1046.067165	103.353417	49.263181
1042.716830	102.751558	49.268186
1038.742695	104.629719	49.273191
1035.640022	106.858667	49.278196
1032.358073	105.075493	49.283201
1028.674852	98.802418	49.288205
1025.245948	102.158142	49.293210
1021.589448	101.708632	49.298215
1018.352406	97.137441	49.303220
1014.323540	103.494649	49.308225
1011.214754	101.905838	49.313229
1007.898711	100.634222	49.318234
1004.702728	106.978091	49.323239
1001.104976	100.454360	49.328244
996.998665	91.862030	49.333249
993.512705	93.711231	49.338253
990.294884	94.233943	49.343258
986.545875	100.079099	49.348263
983.012433	99.075652	49.353268
979.917058	99.626653	49.358273
976.214065	99.513477	49.363277
972.797225	96.463774	49.368282
969.230728	103.928706	49.373287
965.646106	100.405393	49.378292
961.994324	101.733230	49.383297
958.923407	98.363609	49.388301
955.384903	98.556887	49.393306
951.722966	102.053528	49.398311
947.854635	96.983248	49.403316
944.183850	93.482927	49.408321
940.971720	93.678892	49.413325
938.069772	93.981318	49.418330
934.119021	95.422417	49.423335
930.695101	83.432915	49.428340
927.071449	103.388037	49.433345
923.283661	94.018193	49.438349
920.537315	88.832361	49.443354
916.671755	95.353861	49.448359
913.442573	102.557182	49.453364
909.890590	99.892501	49.458369
906.267488	112.611918	49.463373
902.659468	100.464579	49.468378
898.713664	97.716033	49.473383
895.622714	101.490291	49.478388
892.330204	105.185378	49.483393
888.565820	96.378207	49.488397
885.300613	101.220647	49.493402
881.511780	99.830114	49.498407
877.973157	96.973526	49.503412
874.364474	95.352305	49.508417
870.949542	99.281706	49.513421
867.769068	95.758427	49.518426
863.985207	97.999176	49.523431
860.267895	96.388642	49.528436
857.200519	95.517912	49.533441
853.853814	103.008576	49.538445
850.047159	98.004613	49.543450
846.222392	92.364401	49.548455
842.987583	85.989560	49.553460
839.748064	95.595846	49.558465
836.078153	97.761814	49.563469
832.788566	98.435025	49.568474
829.076138	95.536069	49.573479
825.484642	88.846921	49.578484
822.004510	91.900681	49.583489
818.715825	86.502410	49.588493
815.367916	95.970650	49.593498
811.676792	101.879569	49.598503
807.812146	87.984920	49.603508
804.318306	94.549493	49.608513
800.839345	91.699414	49.613517
797.582996	93.313409	49.618522
793.923473	105.940477	49.623527
790.747770	94.905601	49.628532
787.037327	95.195469	49.633537
783.865534	105.813079	49.638541
780.230710	96.216867	49.643546
776.366769	96.331456	49.648551
773.170688	95.642263	49.653556
769.608385	103.562189	49.658561
766.024031	104.525194	49.663565
762.538930	106.263611	49.668570
758.904316	104.127631	49.673575
755.495140	91.901775	49.678580
751.831630	103.298758	49.683585
748.647646	102.215366	49.688589
744.916784	102.122464	49.693594
741.146921	96.306019	49.698599
738.008382	90.906414	49.703604
734.290050	95.183933	49.708609
730.853557	97.367172	49.713613
727.790053	97.258356	49.718618
723.934897	97.112160	49.723623
720.610202	99.679698	49.728628
716.928240	97.019632	49.733633
713.807459	96.862842	49.738637
710.010571	90.161617	49.743642
706.242018	101.973701	49.748647
703.165978	91.793304	49.753652
699.619499	92.291651	49.758657
696.138156	91.855969	49.763661
692.526407	95.012644	49.768666
688.709357	95.053487	49.773671
685.557159	90.257164	49.778676
681.806641	92.081467	49.783681
678.223129	91.095471	49.788685
674.646250	81.271941	49.793690
671.349546	93.788432	49.798695
668.185312	87.389953	49.803700
664.418385	97.971074	49.808705
661.115726	94.792879	49.813709
657.669291	86.081567	49.818714
653.529729	92.810588	49.823719
650.468357	90.401380	49.828724
646.699232	92.510189	49.833729
643.380798	96.541613	49.838733
640.246602	96.089552	49.843738
636.522242	101.478546	49.848743
632.832233	97.838996	49.853748
629.307142	89.677860	49.858753
625.832581	100.504277	49.863757
622.545409	94.292749	49.868762
618.530711	95.395974	49.873767
615.670964	93.986601	49.878772
612.001035	94.592902	49.883777
608.228402	103.036207	49.888781
605.124009	90.297613	49.893786
601.099325	94.246666	49.898791
597.793152	98.282513	49.903796
594.215329	101.000471	49.908801
590.705421	97.158725	49.913805
587.407343	90.724291	49.918810
583.677996	100.774362	49.923815
580.620437	93.337302	49.928820
576.912863	89.105735	49.933825
573.445046	90.436546	49.938829
569.777417	91.238659	49.943834
566.224837	97.341103	49.948839
562.927715	97.980786	49.953844
559.295319	94.019030	49.958849
555.910619	93.232903	49.963853
552.777658	92.018203	49.968858
548.830770	102.564272	49.973863
545.472405	93.076738	49.978868
541.505905	93.944654	49.983873
538.040968	90.763449	49.988877
534.931014	91.149198	49.993882
531.162137	92.024132	49.998887
527.774798	90.608834	50.003892
524.111137	92.909984	50.008897
520.935214	85.624369	50.013901
517.240815	77.483479	50.018906
513.415608	98.476339	50.023911
510.466372	84.713731	50.028916
507.019603	91.182440	50.033921
503.074802	85.858586	50.038925
499.719252	85.194467	50.043930
496.442867	98.780350	50.048935
492.752834	91.208265	50.053940
489.076211	93.248864	50.058945
485.565077	91.751729	50.063949
482.242397	86.722756	50.068954
478.563920	96.518116	50.073959
474.928924	89.497413	50.078964
471.693026	87.359217	50.083969
468.388576	91.869405	50.088973
465.234200	86.886846	50.093978
461.609118	99.185903	50.098983
457.801841	80.040052	50.103988
453.908684	93.013855	50.108993
450.658266	94.845342	50.113997
446.909342	90.613982	50.119002
443.628760	88.160089	50.124007
440.498704	81.069808	50.129012
437.159263	89.837625	50.134017
433.089432	92.408076	50.139021
429.377487	86.174578	50.144026
425.526449	93.760179	50.149031
422.679995	92.851831	50.154036
419.223396	97.161238	50.159041
415.409297	89.020158	50.164045
412.630636	83.776288	50.169050
409.015888	94.099532	50.174055
405.132064	91.847710	50.179060
401.954331	88.605757	50.184065
397.965326	83.617913	50.189069
394.635585	79.159568	50.194074
390.691583	90.720811	50.199079
387.966111	83.269782	50.204084
384.166033	84.583103	50.209089
380.523154	89.326665	50.214093
377.318587	84.532340	50.219098
374.003124	92.790215	50.224103
370.397738	86.888070	50.229108
366.566383	94.132084	50.234113
362.508629	90.297155	50.239117
359.600209	84.450361	50.244122
356.403066	89.105130	50.249127
352.791095	88.870379	50.254132
349.336901	85.048485	50.259137
345.746809	84.883077	50.264141
342.312050	84.933787	50.269146
338.145815	85.542009	50.274151
335.035113	89.696020	50.279156
331.926880	84.934079	50.284161
328.031923	87.847346	50.289165
324.806413	84.821718	50.294170
320.852522	87.867607	50.299175
317.569409	85.914038	50.304180
314.041128	81.527955	50.309185
310.838994	75.344373	50.314189
307.026292	80.880200	50.319194
303.207587	89.346640	50.324199
300.362738	76.567539	50.329204
296.750124	87.637135	50.334209
292.824546	91.836549	50.339213
289.588743	83.747317	50.344218
286.122132	87.694501	50.349223
282.557413	82.450424	50.354228
278.927449	83.183478	50.359233
275.642460	87.042103	50.364237
272.291942	83.270440	50.369242
268.411133	92.025037	50.374247
264.660232	80.523681	50.379252
261.320555	84.406696	50.384257
257.922448	78.703093	50.389261
254.732847	84.698158	50.394266
250.634685	84.833844	50.399271
247.692228	78.764634	50.404276
244.345741	80.335992	50.409281
240.703394	82.380809	50.414285
237.255424	79.105325	50.419290
233.096302	84.575224	50.424295
230.119562	84.975011	50.429300
226.758295	83.897436	50.434305
223.000436	82.777585	50.439309
219.438210	81.946632	50.444314
215.790341	94.255657	50.449319
212.389375	80.639883	50.454324
208.928008	85.007056	50.459329
205.269618	97.735355	50.464333
202.232797	80.832311	50.469338
198.725886	92.584578	50.474343
195.276614	79.681906	50.479348
191.540260	93.599349	50.484353
187.401759	89.381682	50.489357
184.798445	82.411470	50.494362
180.925152	88.637053	50.499367
177.297178	90.480327	50.504372
173.791737	82.613723	50.509377
170.458979	88.011140	50.514381
167.191246	81.401291	50.519386
163.225401	90.118626	50.524391
159.880349	79.730675	50.529396
156.457264	80.804695	50.534401
152.558080	94.282583	50.539405
149.660892	82.343820	50.544410
145.840937	91.139547	50.549415
142.576958	93.289645	50.554420
138.872387	86.836828	50.559425
135.192886	89.339931	50.564429
132.014843	87.404776	50.569434
128.157528	88.442431	50.574439
125.099115	89.712435	50.579444
121.386540	91.363338	50.584449
117.802869	92.794730	50.589453
114.674456	85.631558	50.594458
110.892460	91.485359	50.599463
107.962483	80.785628	50.604468
103.991752	85.843251	50.609473
100.226474	83.544524	50.614477
96.628537	83.000793	50.619482
93.150862	83.403177	50.624487
90.290000	84.401795	50.629492
86.687304	85.602059	50.634497
82.896539	86.088300	50.639501
78.972936	87.506525	50.644506
75.749281	91.210075	50.649511
72.110043	90.388084	50.654516
68.900240	76.688652	50.659521
65.142565	84.772289	50.664525
62.089182	82.697407	50.669530
58.462191	87.470238	50.674535
54.801377	81.595908	50.679540
51.136276	80.793797	50.684545
47.818068	91.969210	50.689549
44.049585	79.420351	50.694554
40.914903	86.121894	50.699559
37.346293	85.709636	50.704564
33.784569	86.011315	50.709569
30.176055	85.108598	50.714573
27.033924	84.449189	50.719578
23.643766	81.806985	50.724583
20.214717	89.364584	50.729588
16.754932	88.672690	50.734593
12.772612	93.032971	50.739597
9.016330	84.237628	50.744602
5.528634	88.355898	50.749607
2.466877	88.427395	50.754612