Thu Aug 25 13:12:44 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
1.044060	95.472133	0.000000
0.543053	84.372960	0.005005
0.459548	94.234871	0.010010
0.602935	79.152775	0.015014
0.193465	71.554229	0.020019
0.078133	65.171947	0.025024
0.316871	67.380797	0.030029
-0.511520	53.659545	0.035034
-0.451310	55.415471	0.040038
-1.067210	44.913296	0.045043
-1.525909	43.672172	0.050048
-1.092923	31.164347	0.055053
-1.535525	23.219834	0.060058
-1.904038	21.325499	0.065062
-2.165103	13.384185	0.070067
-2.701718	18.039883	0.075072
-2.950538	1.462729	0.080077
-3.357938	4.304322	0.085082
-3.299532	5.810588	0.090086
-3.851847	7.172097	0.095091
-4.626033	3.316515	0.100096
-4.293176	-0.440436	0.105101
-4.699814	5.381305	0.110106
-4.583440	4.904298	0.115110
-5.219960	-6.100819	0.120115
-5.729207	3.811930	0.125120
-5.431208	-2.847061	0.130125
-6.041610	4.389173	0.135130
-6.018500	-3.625133	0.140134
-6.645915	2.512775	0.145139
-7.339892	2.336743	0.150144
-7.319050	-3.712508	0.155149
-7.762600	-1.377782	0.160154
-7.499047	0.874627	0.165158
-7.397277	2.184272	0.170163
-8.003383	7.480445	0.175168
-7.599948	-4.643073	0.180173
-8.104808	8.287223	0.185178
-8.306582	3.658581	0.190182
-8.647991	-1.438566	0.195187
-9.121798	2.941531	0.200192
-9.348898	-2.227310	0.205197
-10.204185	12.441019	0.210202
-10.208184	2.096097	0.215206
-10.244389	-1.666303	0.220211
-10.897247	0.979629	0.225216
-10.380989	-9.544877	0.230221
-10.599988	-1.139268	0.235226
-11.431371	1.287863	0.240230
-11.741202	4.585569	0.245235
-11.855614	3.875802	0.250240
-11.650176	-2.743376	0.255245
-11.829646	6.073661	0.260250
-12.286393	1.836147	0.265254
-13.127335	4.761487	0.270259
-13.111310	10.488532	0.275264
-12.924918	-0.022261	0.280269
-13.694627	5.448242	0.285274
-13.769018	17.013953	0.290278
-13.492291	3.609974	0.295283
-14.483916	5.049807	0.300288
-14.739587	-2.936637	0.305293
-14.999659	7.519205	0.310298
-15.398218	9.008485	0.315302
-14.959249	-0.532640	0.320307
-15.498206	6.736692	0.325312
-15.418036	-1.023961	0.330317
-16.004614	7.461392	0.335322
-16.486816	3.180410	0.340326
-16.517159	6.972167	0.345331
-16.224050	13.057596	0.350336
-16.336128	-2.810145	0.355341
-17.614043	1.290979	0.360346
-17.691056	-0.959074	0.365350
-17.670374	-4.119780	0.370355
-18.054874	10.386196	0.375360
-17.997551	4.625458	0.380365
-18.931097	5.825237	0.385370
-19.330740	-3.992615	0.390374
-19.170920	-0.781152	0.395379
-19.443698	7.898644	0.400384
-19.325493	-5.682970	0.405389
-19.443310	0.210575	0.410394
-19.540821	1.905786	0.415398
-19.748355	0.251989	0.420403
-20.430925	1.988249	0.425408
-20.608068	-1.758396	0.430413
-20.609805	3.936628	0.435418
-21.118450	-0.767318	0.440422
-21.837690	-4.286654	0.445427
-21.884842	0.997868	0.450432
-22.120416	-2.397935	0.455437
-22.236872	2.277348	0.460442
-21.918881	1.202436	0.465446
-22.859546	-0.241578	0.470451
-23.165270	0.875650	0.475456
-23.155364	4.059983	0.480461
-23.728213	-0.086571	0.485466
-23.614424	2.227268	0.490470
-23.314495	-2.350266	0.495475
-24.639774	-3.661250	0.500480
-25.016266	-3.858552	0.505485
-25.241400	-1.355567	0.510490
-25.084881	0.097360	0.515494
-25.433693	-3.628714	0.520499
-25.536550	-1.945321	0.525504
-25.343532	1.042641	0.530509
-25.781560	6.122653	0.535514
-26.217014	-0.367634	0.540518
-26.364808	0.595135	0.545523
-26.400222	3.821370	0.550528
-26.517389	0.286791	0.555533
-27.603549	8.239815	0.560538
-27.625856	-0.824072	0.565542
-27.909543	2.494848	0.570547
-28.222796	12.690104	0.575552
-27.677798	-2.078358	0.580557
-28.435882	-0.463144	0.585562
-29.241336	8.727223	0.590566
-28.961496	1.476288	0.595571
-29.280544	8.486537	0.600576
-29.107006	2.878434	0.605581
-29.436017	-1.882130	0.610586
-30.164265	-3.169600	0.615590
-30.531661	3.949464	0.620595
-30.900100	9.942393	0.625600
-30.767992	-3.400955	0.630605
-31.031339	-0.275048	0.635610
-30.801446	-11.295688	0.640614
-31.427591	-7.321996	0.645619
-31.957766	1.107060	0.650624
-32.220387	1.072251	0.655629
-32.245796	-0.929623	0.660634
-32.165631	-2.482965	0.665638
-32.513929	-7.208868	0.670643
-33.282188	5.155253	0.675648
-33.228824	1.736324	0.680653
-33.475548	-4.603196	0.685658
-33.787724	1.526447	0.690662
-33.595901	-1.680057	0.695667
-35.017161	8.783718	0.700672
-34.906035	-6.290083	0.705677
-35.160866	5.300726	0.710682
-35.059815	-2.045580	0.715686
-35.139053	-1.757944	0.720691
-35.470225	2.106256	0.725696
-35.201696	-2.244895	0.730701
-35.689391	2.200653	0.735706
-36.531701	3.354500	0.740710
-36.621232	-1.899169	0.745715
-36.924448	8.379933	0.750720
-36.672531	7.910162	0.755725
-37.286312	4.326845	0.760730
-37.743164	0.636682	0.765734
-37.481673	-5.706538	0.770739
-38.399989	-3.509395	0.775744
-38.254031	-4.085951	0.780749
-38.568014	10.598801	0.785754
-38.571980	2.547609	0.790758
-39.083853	1.612216	0.795763
-39.730774	7.357712	0.800768
-39.635980	2.239676	0.805773
-39.986658	5.727282	0.810778
-40.166444	-0.834700	0.815782
-39.920453	-2.955029	0.820787
-40.584164	8.535333	0.825792
-40.863607	1.906707	0.830797
-41.255984	-2.435802	0.835802
-41.532122	-4.322459	0.840806
-41.183699	-5.930488	0.845811
-41.926399	7.211079	0.850816
-41.936325	-0.484836	0.855821
-42.649796	1.961787	0.860826
-42.753936	-0.410566	0.865830
-42.591039	-1.034069	0.870835
-43.114040	1.246668	0.875840
-42.660214	-3.228429	0.880845
-43.059620	-4.640190	0.885850
-43.691420	8.366942	0.890854
-43.810112	4.475097	0.895859
-44.072713	8.929670	0.900864
-44.488553	-3.296432	0.905869
-45.151705	6.251289	0.910874
-45.520290	-0.470936	0.915878
-45.412117	-0.870729	0.920883
-45.790093	4.551051	0.925888
-45.738998	-0.547481	0.930893
-45.753142	-3.019357	0.935898
-45.791507	-1.592843	0.940902
-46.528098	-4.274224	0.945907
-47.100629	2.649190	0.950912
-47.153259	3.052880	0.955917
-47.416892	2.300055	0.960922
-47.339402	10.795254	0.965926
-47.953180	-2.361618	0.970931
-48.685065	12.116530	0.975936
-48.582717	-4.262532	0.980941
-48.804161	-2.873770	0.985946
-48.811039	-5.100010	0.990950
-48.548729	-10.326548	0.995955
-49.031380	5.083819	1.000960
-49.414374	-8.995064	1.005965
-49.850036	2.383630	1.010970
-49.950979	1.978639	1.015974
-49.861007	-9.137137	1.020979
-50.449030	-2.692189	1.025984
-51.020155	-7.765992	1.030989
-51.335489	-8.969461	1.035994
-51.620376	-6.605811	1.040998
-51.807370	-3.226112	1.046003
-51.717151	5.934644	1.051008
-51.574447	0.922998	1.056013
-52.450614	-7.804613	1.061018
-52.915851	-4.074432	1.066022
-52.972937	-7.817739	1.071027
-53.199765	-3.144147	1.076032
-53.071308	-3.648358	1.081037
-53.633918	1.672636	1.086042
-53.368999	1.279921	1.091046
-54.106779	-2.391532	1.096051
-54.539427	4.693463	1.101056
-54.480219	-5.072893	1.106061
-54.544848	-4.863477	1.111066
-54.883851	-5.398846	1.116070
-55.714839	-9.160097	1.121075
-55.985772	-1.714465	1.126080
-55.925361	-6.393674	1.131085
-56.146354	6.102997	1.136090
-56.385969	1.451813	1.141094
-56.448850	-0.335380	1.146099
-56.550662	-2.423359	1.151104
-56.987111	-1.428016	1.156109
-57.791565	0.434912	1.161114
-57.796767	2.995186	1.166118
-57.468884	-10.059289	1.171123
-57.768096	-1.511399	1.176128
-57.868782	-4.564502	1.181133
-58.664498	-11.175503	1.186138
-59.000584	-6.181071	1.191142
-59.037914	-5.748141	1.196147
-59.563788	-4.912794	1.201152
-59.328263	-9.062618	1.206157
-59.864300	-7.814390	1.211162
-60.594754	-9.598221	1.216166
-60.393238	-9.974674	1.221171
-60.741518	-3.712825	1.226176
-61.046908	-8.496069	1.231181
-60.949550	-7.625497	1.236186
-60.870496	-8.479473	1.241190
-61.619371	-16.670201	1.246195
-62.143425	-6.397635	1.251200
-62.147871	-7.703600	1.256205
-62.350327	-12.996518	1.261210
-62.677146	-21.383089	1.266214
-62.337668	-15.029692	1.271219
-62.871054	-3.221236	1.276224
-63.680317	-2.825541	1.281229
-63.819199	-5.711306	1.286234
-63.842825	-8.273444	1.291238
-63.881076	-8.137764	1.296243
-64.326507	-5.204791	1.301248
-64.743849	-10.698158	1.306253
-65.196626	-7.204048	1.311258
-65.456563	-11.016810	1.316262
-65.212303	-12.950204	1.321267
-65.484150	-3.008220	1.326272
-65.481857	-9.655674	1.331277
-66.470523	-4.603282	1.336282
-67.060231	-10.531550	1.341286
-66.801360	-12.571638	1.346291
-66.911923	-1.642521	1.351296
-67.078429	-16.726592	1.356301
-66.791651	-2.202424	1.361306
-66.915174	-12.462165	1.366310
-67.521621	-12.746820	1.371315
-68.311485	-7.213049	1.376320
-68.071589	-11.989983	1.381325
-68.650247	-9.602448	1.386330
-69.032314	3.450970	1.391334
-69.448824	-8.395367	1.396339
-69.837379	-6.559641	1.401344
-70.038979	-16.971660	1.406349
-70.265761	-9.567750	1.411354
-70.263864	-9.428869	1.416358
-70.412549	-1.907479	1.421363
-70.480939	2.621066	1.426368
-70.297558	-7.541233	1.431373
-71.170036	-9.128803	1.436378
-71.720174	-7.017820	1.441382
-71.692156	-9.445681	1.446387
-72.173245	-2.824499	1.451392
-71.860639	-5.499433	1.456397
-71.426118	-7.256995	1.461402
-72.326729	-10.380909	1.466406
-72.494714	-11.148720	1.471411
-73.135051	-12.778991	1.476416
-73.125517	-10.357070	1.481421
-73.879305	-9.052575	1.486426
-73.956776	-2.203570	1.491430
-74.295506	-10.496530	1.496435
-74.281466	0.042904	1.501440
-74.108760	-6.764131	1.506445
-74.702339	-8.756071	1.511450
-75.345478	-2.198083	1.516454
-75.398656	-10.532622	1.521459
-75.464572	-7.092802	1.526464
-75.606966	-2.081262	1.531469
-76.338017	-3.194281	1.536474
-76.772465	-1.829091	1.541478
-76.936013	-11.462462	1.546483
-77.313851	-5.123216	1.551488
-77.117023	-7.504760	1.556493
-77.465401	-11.265698	1.561498
-77.245978	-4.238588	1.566502
-77.185620	-6.469035	1.571507
-78.091074	-5.204050	1.576512
-78.442372	-7.831903	1.581517
-78.683017	-0.944675	1.586522
-79.083741	0.643022	1.591526
-78.775682	-10.304442	1.596531
-79.972159	-1.236308	1.601536
-80.086627	-7.533271	1.606541
-80.204694	-6.847245	1.611546
-80.111719	-1.942188	1.616550
-80.305315	-0.934277	1.621555
-80.246216	1.492534	1.626560
-80.391156	-2.955182	1.631565
-81.259995	5.400391	1.636570
-81.362567	-4.131806	1.641574
-81.426637	-7.592443	1.646579
-81.790209	-3.859208	1.651584
-82.253530	-5.745007	1.656589
-82.907999	-2.814080	1.661594
-83.170328	-2.649616	1.666598
-83.121776	-4.824429	1.671603
-83.452811	-4.279039	1.676608
-83.728970	-2.362847	1.681613
-83.582892	-2.392091	1.686618
-83.193630	1.954012	1.691622
-83.200868	-4.688786	1.696627
-84.167066	-4.993001	1.701632
-84.230358	-4.442107	1.706637
-85.033149	-9.530226	1.711642
-85.691222	-2.580755	1.716646
-86.041730	-11.042711	1.721651
-86.246077	1.843653	1.726656
-86.014059	-8.845122	1.731661
-86.008552	-0.939768	1.736666
-86.070222	4.505216	1.741670
-86.316731	-1.056049	1.746675
-86.736787	12.465237	1.751680
-87.203584	-0.429922	1.756685
-87.539909	1.929134	1.761690
-87.651096	6.850365	1.766694
-87.328919	-3.669042	1.771699
-88.175812	1.111202	1.776704
-88.907129	-7.509386	1.781709
-88.930526	1.893795	1.786714
-89.126652	2.199747	1.791718
-88.832666	-1.829525	1.796723
-89.464555	1.806548	1.801728
-89.295136	-8.302941	1.806733
-89.588487	-3.030466	1.811738
-90.256064	-1.236439	1.816742
-90.300277	-13.359406	1.821747
-90.306087	0.264641	1.826752
-91.051210	-5.775316	1.831757
-91.709681	-4.201016	1.836762
-91.934990	2.234556	1.841766
-92.015018	-13.407232	1.846771
-92.455132	1.714888	1.851776
-92.486453	-6.002979	1.856781
-92.313338	-4.881686	1.861786
-92.238926	-1.400578	1.866790
-92.213160	-4.467166	1.871795
-93.167336	5.315981	1.876800
-93.584442	-4.375738	1.881805
-94.087321	1.188998	1.886810
-94.124849	-5.784411	1.891814
-93.747459	-13.278415	1.896819
-94.038661	-0.406918	1.901824
-94.550731	-0.545008	1.906829
-94.823750	-3.805224	1.911834
-95.143818	-5.242068	1.916838
-95.138688	-13.070048	1.921843
-95.576189	-3.371028	1.926848
-96.199282	-7.756474	1.931853
-96.457339	-4.004971	1.936858
-96.503811	-4.541884	1.941862
-96.642234	-11.293837	1.946867
-97.140259	3.739282	1.951872
-96.807842	-2.564431	1.956877
-97.008871	-1.536373	1.961882
-97.511580	-9.354382	1.966886
-97.899979	-9.429592	1.971891
-98.208112	-3.256292	1.976896
-98.216400	-8.544832	1.981901
-98.954455	-10.463511	1.986906
-99.348580	1.133299	1.991910
-99.514287	-7.889126	1.996915
-99.227599	0.359709	2.006912
-99.378344	1.035844	2.016909
-98.622678	1.050430	2.026906
-98.309901	0.861982	2.036902
-97.626544	2.196206	2.046899
-97.011659	1.887559	2.056896
-97.053110	2.524395	2.066893
-96.377812	1.978199	2.076890
-95.840603	-0.960234	2.086886
-95.238055	-1.019857	2.096883
-94.456438	4.040160	2.106880
-94.057398	3.587937	2.116877
-94.106731	9.912238	2.126874
-93.095404	-3.041091	2.136870
-92.844827	0.923709	2.146867
-92.248376	1.286360	2.156864
-91.528954	-1.937217	2.166861
-91.585447	7.663726	2.176858
-90.374606	3.884806	2.186854
-90.145543	3.614441	2.196851
-89.836036	-4.477194	2.206848
-88.812130	6.120214	2.216845
-88.547061	-0.557949	2.226842
-88.437392	6.219777	2.236838
-87.745537	0.276198	2.246835
-87.059426	4.752464	2.256832
-87.070921	7.107898	2.266829
-86.422880	7.551165	2.276826
-85.549667	4.857858	2.286822
-84.764729	3.141398	2.296819
-84.593368	1.663633	2.306816
-84.513949	1.844371	2.316813
-83.631106	0.274129	2.326810
-83.130702	7.022309	2.336806
-82.876118	7.181936	2.346803
-82.154492	5.836528	2.356800
-81.512300	6.863590	2.366797
-81.463036	6.041687	2.376794
-80.578406	3.714058	2.386790
-79.950983	0.200786	2.396787
-79.921662	1.317544	2.406784
-79.139502	3.703842	2.416781
-78.833621	3.114162	2.426778
-77.819704	-1.137582	2.436774
-77.327190	-5.161906	2.446771
-77.462910	8.309851	2.456768
-76.918418	2.595269	2.466765
-75.990780	0.264070	2.476762
-76.038290	-0.390614	2.486758
-75.155919	3.994713	2.496755
-74.960623	6.333584	2.506752
-74.029257	2.997602	2.516749
-73.440881	6.012982	2.526746
-73.313142	0.680485	2.536742
-72.263778	-1.295986	2.546739
-71.808044	1.803534	2.556736
-71.948984	3.197228	2.566733
-71.466464	9.111908	2.576730
-70.576553	8.535255	2.586726
-70.231015	5.630023	2.596723
-69.354930	5.701770	2.606720
-69.174629	7.811741	2.616717
-69.089645	6.521739	2.626714
-67.704998	5.107290	2.636710
-67.417140	6.294412	2.646707
-67.702716	6.864962	2.656704
-66.793991	10.932548	2.666701
-66.219283	5.523678	2.676698
-65.310135	-0.244872	2.686694
-64.883301	0.869788	2.696691
-64.855590	3.710090	2.706688
-64.240547	-2.383011	2.716685
-63.402167	3.900397	2.726682
-63.421950	7.818864	2.736678
-62.295355	3.077460	2.746675
-61.940145	1.225596	2.756672
-61.804162	0.431287	2.766669
-61.130848	4.532592	2.776666
-60.273446	9.035876	2.786662
-60.098704	12.417013	2.796659
-59.938462	7.063581	2.806656
-58.947194	-0.574177	2.816653
-58.877395	13.720694	2.826650
-57.899045	8.343612	2.836646
-57.357337	9.380085	2.846643
-57.451331	8.843558	2.856640
-56.828503	7.811407	2.866637
-56.081848	6.778861	2.876634
-55.307487	12.736515	2.886630
-54.839328	8.221825	2.896627
-54.812046	1.847015	2.906624
-54.358644	3.261624	2.916621
-53.361999	10.226660	2.926618
-53.084503	1.306902	2.936614
-52.901640	2.611845	2.946611
-51.827433	6.064290	2.956608
-51.712473	3.591165	2.966605
-51.331646	2.219963	2.976602
-50.423721	-0.104978	2.986598
-50.311836	5.503479	2.996595
-49.103251	5.472445	3.006592
-48.726561	1.878084	3.016589
-48.639463	-5.979130	3.026586
-48.604079	-6.684816	3.036582
-47.773445	-12.862379	3.046579
-46.919345	-6.996419	3.056576
-46.172375	-12.869434	3.066573
-45.801241	-6.411446	3.076570
-46.114142	-1.002529	3.086566
-45.448278	0.096855	3.096563
-44.552695	-1.931545	3.106560
-43.650991	-1.828963	3.116557
-43.451436	-0.865591	3.126554
-43.015580	-3.116564	3.136550
-42.569950	-4.757679	3.146547
-42.280478	4.427927	3.156544
-41.658227	8.081070	3.166541
-41.288027	-2.446625	3.176538
-40.709789	0.247228	3.186534
-40.172346	2.621189	3.196531
-39.067781	-1.103058	3.206528
-38.830428	-1.533112	3.216525
-38.635007	-1.513101	3.226522
-38.407917	-5.004825	3.236518
-37.616070	2.578346	3.246515
-37.023629	-1.667544	3.256512
-36.205849	-0.047098	3.266509
-35.853061	2.396978	3.276506
-35.809526	-0.666842	3.286502
-35.277852	-1.523149	3.296499
-34.160290	-6.953717	3.306496
-33.863430	3.136727	3.316493
-33.711370	0.036897	3.326490
-33.194627	-4.399872	3.336486
-32.709597	-3.734655	3.346483
-31.537639	-3.630067	3.356480
-31.143935	1.278495	3.366477
-31.039602	2.069886	3.376474
-31.221817	5.535464	3.386470
-30.097743	2.996091	3.396467
-29.662312	4.014372	3.406464
-28.792167	1.327886	3.416461
-28.740795	0.819267	3.426458
-28.388395	7.286533	3.436454
-27.264756	3.077789	3.446451
-27.202852	8.741597	3.456448
-26.074694	-1.274465	3.466445
-25.625663	-0.416705	3.476442
-25.461302	0.415965	3.486438
-25.342368	-5.041865	3.496435
-24.679104	1.402034	3.506432
-23.955798	3.572645	3.516429
-23.798301	7.628062	3.526426
-22.761968	6.093965	3.536422
-22.621883	3.800636	3.546419
-22.244965	0.713090	3.556416
-21.294654	-2.898287	3.566413
-21.148097	-1.619332	3.576410
-20.143692	4.327623	3.586406
-19.668351	6.423045	3.596403
-19.617778	3.871308	3.606400
-19.372706	5.423099	3.616397
-18.511778	8.611193	3.626394
-18.106351	4.280563	3.636390
-17.320390	1.714973	3.646387
-17.074955	3.618335	3.656384
-16.768551	-0.604911	3.666381
-15.621625	6.437954	3.676378
-15.296261	6.545311	3.686374
-15.320149	3.010546	3.696371
-14.636621	6.099722	3.706368
-14.015395	7.263124	3.716365
-13.582200	3.390645	3.726362
-12.360774	-0.839754	3.736358
-12.185503	3.716561	3.746355
-12.403230	5.039923	3.756352
-11.877803	2.651371	3.766349
-11.323756	0.933080	3.776346
-10.242165	-3.265905	3.786342
-9.421319	-3.473767	3.796339
-9.350137	9.167290	3.806336
-9.153918	2.718491	3.816333
-8.696041	3.764934	3.826330
-8.020777	0.909411	3.836326
-7.575270	3.538534	3.846323
-6.426835	4.885428	3.856320
-5.985611	6.865820	3.866317
-5.854019	8.929572	3.876314
-5.635858	4.929226	3.886310
-5.692884	2.682620	3.896307
-4.939057	10.870475	3.906304
-4.146502	20.319394	3.916301
-3.925604	27.577054	3.926298
-3.243980	35.627345	3.936294
-2.950340	47.752066	3.946291
-2.378688	69.213177	3.956288
-1.838027	75.232820	3.966285
-1.383364	90.034500	3.976282
-0.865649	97.340719	3.986278
-0.654737	119.004132	3.996275
0.000000	136.771537	4.001280
0.334060	130.837683	4.006285
-0.140593	145.860938	4.011290
0.291728	154.825804	4.016294
0.179911	166.903684	4.021299
0.336813	166.347555	4.026304
0.345273	174.138633	4.031309
0.458785	175.323064	4.036314
0.440221	164.119777	4.041318
0.878731	185.985653	4.046323
0.677873	188.285541	4.051328
0.927101	193.292726	4.056333
0.644358	192.068315	4.061338
0.541893	189.727310	4.066342
0.926342	184.551183	4.071347
0.780949	195.663056	4.076352
1.183947	195.375256	4.081357
1.218456	190.696888	4.086362
1.039387	189.263242	4.091366
1.238047	195.585000	4.096371
1.002726	189.484070	4.101376
1.301167	195.027718	4.106381
0.980570	204.392155	4.111386
1.197322	198.524116	4.116390
1.044768	184.972122	4.121395
0.673961	184.226588	4.126400
1.195144	190.478828	4.131405
0.944909	197.924466	4.136410
1.311440	192.814420	4.141414
1.034206	198.992441	4.146419
0.763436	200.385782	4.151424
1.276729	193.284855	4.156429
1.248010	191.894091	4.161434
1.160807	202.082513	4.166438
1.261923	197.855622	4.171443
1.039567	196.026954	4.176448
1.129914	194.060706	4.181453
0.851086	197.002408	4.186458
0.948707	187.555795	4.191462
1.111460	189.219736	4.196467
0.819757	190.923245	4.201472
1.360913	191.929939	4.206477
0.900822	197.102047	4.211482
1.025360	194.013620	4.216486
1.004532	203.188718	4.221491
1.006442	192.807957	4.226496
1.430545	206.646391	4.231501
1.167431	220.143249	4.236506
1.350819	216.953847	4.241510
1.561237	220.540244	4.246515
1.275348	212.112341	4.251520
1.488595	215.179430	4.256525
1.247389	214.207941	4.261530
1.324528	210.380279	4.266534
1.432844	207.392469	4.271539
1.455907	216.396179	4.276544
1.725531	213.171119	4.281549
1.850236	214.891645	4.286554
1.784491	198.228675	4.291558
1.527391	199.053554	4.296563
1.423709	200.645345	4.301568
1.600440	196.846375	4.306573
1.410738	199.112878	4.311578
1.401615	194.944390	4.316582
1.379405	188.892328	4.321587
1.243330	197.860850	4.326592
1.477319	196.289717	4.331597
1.300461	202.641840	4.336602
1.642860	213.022389	4.341606
1.586084	228.331423	4.346611
1.680360	222.577479	4.351616
1.919655	218.319441	4.356621
1.263387	213.350660	4.361626
1.442753	218.419419	4.366630
1.637481	210.330671	4.371635
1.425749	216.384538	4.376640
1.900799	212.728652	4.381645
1.761484	217.894799	4.386650
1.761040	221.431976	4.391654
1.736277	214.272973	4.396659
1.982281	216.733808	4.401664
2.054758	213.878164	4.406669
1.876518	210.141136	4.411674
1.651956	204.367550	4.416678
1.176996	205.432211	4.421683
1.544697	223.259560	4.426688
2.125801	214.420562	4.431693
2.119573	223.742081	4.436698
2.341087	214.775923	4.441702
1.944449	210.424535	4.446707
1.841813	202.638650	4.451712
1.624791	185.214771	4.456717
2.115942	203.551112	4.461722
1.764125	194.810838	4.466726
1.702580	204.666206	4.471731
1.841773	212.753199	4.476736
2.030592	209.414248	4.481741
1.780009	211.769387	4.486746
2.044916	213.053487	4.491750
2.065681	213.588053	4.496755
1.988702	221.750050	4.501760
1.978894	212.098789	4.506765
2.139962	219.492648	4.511770
1.870475	224.954444	4.516774
2.009701	219.481365	4.521779
2.033609	217.370497	4.526784
2.225302	217.280323	4.531789
1.819812	231.274068	4.536794
1.822331	215.176200	4.541798
2.132245	217.484649	4.546803
1.681163	220.915260	4.551808
2.229688	214.042926	4.556813
1.999312	221.827154	4.561818
2.272367	218.383253	4.566822
2.052455	221.945325	4.571827
1.628448	222.207887	4.576832
2.060376	215.686022	4.581837
2.097174	217.784159	4.586842
1.804310	220.519253	4.591846
2.050717	223.888037	4.596851
2.179215	241.370062	4.601856
2.297318	241.728023	4.606861
2.427142	248.633236	4.611866
2.113779	243.525295	4.616870
2.263680	233.197256	4.621875
2.288581	240.023990	4.626880
2.510165	236.274932	4.631885
2.309639	244.978325	4.636890
2.601264	242.309807	4.641894
2.283918	229.530258	4.646899
2.413711	228.358269	4.651904
2.002204	218.184640	4.656909
2.216940	231.771155	4.661914
2.496537	235.593493	4.666918
2.442001	242.995833	4.671923
2.455763	256.680296	4.676928
2.680674	246.919473	4.681933
2.198664	246.226161	4.686938
2.218225	245.742170	4.691942
2.457574	251.016679	4.696947
2.190628	253.754045	4.701952
2.614472	245.195940	4.706957
2.609409	250.258803	4.711962
2.783506	246.805091	4.716966
2.528669	240.530027	4.721971
2.693800	247.296827	4.726976
2.878365	248.397362	4.731981
2.660212	243.726929	4.736986
2.760608	233.659750	4.741990
2.606282	224.505698	4.746995
2.381672	229.109400	4.752000
2.542579	221.617578	4.757005
2.514575	236.577255	4.762010
2.449844	238.877968	4.767014
2.582983	241.938630	4.772019
2.593008	252.599074	4.777024
2.428704	243.266238	4.782029
2.634444	245.072148	4.787034
2.906908	251.379199	4.792038
2.863214	250.164787	4.797043
2.785687	248.712062	4.802048
2.920839	238.535029	4.807053
2.423088	252.185735	4.812058
2.907266	248.060168	4.817062
2.602533	244.111994	4.822067
2.691849	251.491798	4.827072
2.719463	246.681616	4.832077
2.397082	248.257056	4.837082
2.340984	250.214726	4.842086
2.425295	246.610563	4.847091
2.888230	255.409329	4.852096
2.997522	259.894283	4.857101
3.118283	257.293663	4.862106
2.889171	252.906524	4.867110
2.903619	253.650893	4.872115
2.552844	252.035333	4.877120
2.869966	246.784313	4.882125
2.839612	265.373274	4.887130
2.789812	278.726021	4.892134
3.131850	270.342077	4.897139
2.945386	276.622963	4.902144
3.543906	260.593026	4.907149
2.945275	265.650816	4.912154
2.869728	263.235981	4.917158
3.107483	264.847049	4.922163
3.049218	264.283500	4.927168
3.306756	265.315654	4.932173
2.888409	263.891018	4.937178
2.952138	272.534037	4.942182
3.174721	264.216269	4.947187
2.922231	276.597843	4.952192
3.433162	271.661306	4.957197
2.958793	276.889459	4.962202
2.993388	266.687035	4.967206
3.036852	261.665554	4.972211
2.981419	276.215102	4.977216
3.335539	265.946797	4.982221
2.721152	271.241180	4.987226
3.112530	275.349739	4.992230
2.881986	277.682764	4.997235
2.668669	278.551407	5.002240
3.040566	266.141576	5.007245
3.277670	267.556590	5.012250
2.788244	265.627388	5.017254
3.386844	279.210743	5.022259
3.483095	296.498555	5.027264
3.639925	283.881959	5.032269
3.506177	282.409565	5.037274
3.391130	275.239374	5.042278
3.329415	277.292841	5.047283
3.211911	280.819896	5.052288
3.340063	271.362128	5.057293
3.352743	268.145678	5.062298
3.457329	276.260268	5.067302
3.238106	274.370989	5.072307
3.287089	285.946019	5.077312
3.431356	286.885188	5.082317
3.508281	297.842067	5.087322
3.623566	294.625355	5.092326
3.543600	290.338228	5.097331
3.130525	290.149816	5.102336
3.633357	295.844973	5.107341
3.775381	294.202818	5.112346
3.693768	291.067578	5.117350
3.630930	279.728784	5.122355
3.232485	278.342158	5.127360
3.563688	273.636264	5.132365
3.593173	281.791098	5.137370
3.767139	297.665163	5.142374
3.730921	280.428003	5.147379
3.609059	290.099875	5.152384
3.739925	266.432983	5.157389
3.224659	284.050717	5.162394
3.696291	296.021449	5.167398
3.862959	293.717359	5.172403
3.414685	294.736713	5.177408
3.695715	289.485008	5.182413
3.649129	298.123178	5.187418
3.619203	299.361729	5.192422
3.777043	295.863097	5.197427
3.512707	304.513240	5.202432
3.938551	300.102566	5.207437
3.945486	303.875889	5.212442
3.502332	301.724294	5.217446
3.555828	312.624740	5.222451
3.438406	300.993921	5.227456
3.705796	291.318169	5.232461
3.560064	304.603707	5.237466
3.542873	304.362759	5.242470
4.054853	302.687948	5.247475
3.483477	300.999378	5.252480
3.853656	298.884868	5.257485
3.727048	301.555958	5.262490
3.426263	306.418393	5.267494
4.074342	317.871102	5.272499
3.731461	321.455625	5.277504
4.013908	320.440049	5.282509
3.846976	332.640574	5.287514
4.031103	331.406280	5.292518
4.142107	322.830715	5.297523
4.352858	335.396018	5.302528
3.995769	310.843717	5.307533
3.951198	316.523406	5.312538
3.909130	312.483441	5.317542
4.308632	308.918468	5.322547
3.930711	302.039395	5.327552
3.793608	301.921641	5.332557
4.181925	314.728033	5.337562
4.353487	317.418849	5.342566
4.384952	305.334419	5.347571
4.095477	301.285764	5.352576
4.594114	307.876943	5.357581
4.318277	312.324174	5.362586
4.086851	308.063937	5.367590
4.300912	300.728272	5.372595
4.283521	310.526159	5.377600
4.264175	306.027045	5.382605
3.846759	308.734210	5.387610
3.955170	305.986819	5.392614
4.127196	308.174513	5.397619
3.845130	304.732149	5.402624
3.945769	300.176271	5.407629
3.989967	315.751139	5.412634
4.473710	326.210851	5.417638
4.714895	317.966075	5.422643
4.005768	320.801207	5.427648
4.458248	327.168666	5.432653
4.356771	324.988844	5.437658
4.157172	330.762432	5.442662
4.159965	331.252360	5.447667
4.320244	331.445524	5.452672
4.414146	327.083688	5.457677
4.430262	330.703716	5.462682
4.100133	324.848552	5.467686
4.173404	332.401750	5.472691
4.515102	325.988897	5.477696
4.726304	328.442544	5.482701
4.483385	328.316059	5.487706
4.586812	332.324212	5.492710
4.437577	326.266695	5.497715
4.318845	330.534288	5.502720
4.449128	328.384593	5.507725
4.432888	325.811757	5.512730
4.342061	331.036780	5.517734
4.594893	332.914417	5.522739
4.540957	329.262294	5.527744
4.410950	326.520618	5.532749
4.533524	327.792226	5.537754
4.796664	330.905303	5.542758
4.673682	331.677535	5.547763
4.137520	333.030208	5.552768
4.541534	327.297305	5.557773
4.435856	327.734624	5.562778
4.523657	329.578005	5.567782
4.589919	320.946174	5.572787
4.330779	320.274889	5.577792
4.438203	327.854372	5.582797
4.487220	338.290453	5.587802
4.856075	349.967270	5.592806
4.719037	348.432110	5.597811
4.748524	351.230615	5.602816
4.762559	347.017333	5.607821
5.167919	355.730255	5.612826
4.632183	351.087406	5.617830
4.863166	348.896621	5.622835
4.693761	358.544341	5.627840
5.057433	355.737965	5.632845
4.826752	346.130730	5.637850
4.821889	352.294603	5.642854
4.756216	349.194822	5.647859
4.605326	355.014571	5.652864
4.448668	354.592989	5.657869
4.559763	355.689223	5.662874
4.843180	359.374945	5.667878
4.617181	354.541193	5.672883
4.704225	357.685030	5.677888
4.882605	353.806673	5.682893
4.637387	360.207529	5.687898
4.777378	363.703747	5.692902
4.796235	353.060804	5.697907
4.854706	369.221954	5.702912
5.049595	370.241784	5.707917
5.350811	369.178971	5.712922
5.048115	364.363561	5.717926
4.905938	353.185851	5.722931
4.893772	363.887804	5.727936
5.058624	360.505123	5.732941
5.372656	377.936065	5.737946
5.214873	363.267922	5.742950
5.010579	355.510553	5.747955
4.756577	367.696269	5.752960
5.032736	362.764853	5.757965
5.158510	384.414211	5.762970
5.272779	383.447130	5.767974
5.373225	375.423701	5.772979
4.976382	378.535787	5.777984
5.331156	374.034987	5.782989
5.390431	368.881280	5.787994
5.133648	369.063859	5.792998
5.557293	372.268857	5.798003
5.313804	367.497954	5.803008
4.974205	368.582545	5.808013
5.300444	368.670611	5.813018
5.070160	377.119296	5.818022
5.478146	374.584391	5.823027
5.446567	372.915644	5.828032
5.250150	365.682233	5.833037
5.019994	369.375656	5.838042
5.113794	370.145562	5.843046
5.181032	375.842554	5.848051
4.826225	384.851769	5.853056
4.994803	368.019046	5.858061
5.354097	375.043381	5.863066
5.251849	376.973493	5.868070
5.228904	367.463416	5.873075
4.897510	386.197748	5.878080
5.131527	379.437907	5.883085
5.589452	398.270049	5.888090
5.631368	402.556782	5.893094
6.007213	399.830751	5.898099
5.796423	396.063982	5.903104
5.626183	383.175851	5.908109
5.440603	375.045372	5.913114
5.094967	375.994865	5.918118
5.293297	368.848303	5.923123
5.576640	387.894454	5.928128
5.879054	386.366369	5.933133
5.792372	384.582865	5.938138
5.249406	384.544520	5.943142
5.826305	378.996490	5.948147
5.464095	373.677861	5.953152
5.718830	371.325159	5.958157
5.675740	367.614380	5.963162
5.608622	375.759083	5.968166
5.502004	380.432924	5.973171
5.787333	388.652127	5.978176
6.426365	382.657751	5.983181
6.088855	384.488680	5.988186
5.605911	381.789638	5.993190
5.932967	367.178407	5.998195
5.597312	372.584175	6.003200
5.861096	375.482018	6.008205
5.571322	373.739828	6.013210
5.523340	373.601782	6.018214
5.812341	370.193319	6.023219
5.784635	375.130048	6.028224
5.813823	378.311428	6.033229
5.858114	376.779493	6.038234
5.616030	372.410176	6.043238
5.904891	370.352692	6.048243
5.840915	367.499421	6.053248
5.653148	370.812870	6.058253
5.595839	375.191076	6.063258
5.758675	383.340882	6.068262
5.688856	372.037925	6.073267
5.270918	377.067434	6.078272
5.671785	368.851401	6.083277
5.486370	372.816233	6.088282
5.537079	369.799455	6.093286
5.999984	379.101337	6.098291
5.424727	389.018312	6.103296
5.778790	389.367781	6.108301
6.002797	405.202463	6.113306
5.456140	383.410156	6.118310
5.710184	385.009192	6.123315
5.905891	398.105257	6.128320
6.161357	397.932321	6.133325
5.485539	394.118188	6.138330
5.405380	377.789512	6.143334
5.368035	387.438703	6.148339
5.535120	401.440948	6.153344
5.949586	391.947748	6.158349
5.916313	397.736427	6.163354
5.788722	392.729054	6.168358
6.114852	393.680864	6.173363
5.773919	391.003864	6.178368
5.767255	369.924254	6.183373
5.395021	376.297559	6.188378
5.541652	389.436109	6.193382
5.841697	390.075623	6.198387
6.013367	404.975682	6.203392
5.876154	393.936377	6.208397
5.516606	379.651019	6.213402
5.324069	388.650630	6.218406
5.492290	404.234617	6.223411
5.751751	404.212920	6.228416
5.766023	400.809531	6.233421
5.971029	396.379649	6.238426
5.781992	396.020088	6.243430
5.578482	403.828659	6.248435
6.028731	397.743631	6.253440
5.953455	386.644005	6.258445
5.916206	399.099510	6.263450
5.936833	393.698745	6.268454
5.642966	381.719022	6.273459
5.526629	385.695180	6.278464
5.907055	388.799382	6.283469
5.856846	380.261704	6.288474
5.719013	379.887793	6.293478
5.963669	371.560189	6.298483
5.349498	373.621131	6.303488
5.423395	375.640706	6.308493
5.435873	388.249768	6.313498
5.434263	392.619250	6.318502
5.850397	393.711986	6.323507
5.571850	396.292999	6.328512
5.891235	400.235693	6.333517
5.864194	394.203301	6.338522
5.783624	403.761195	6.343526
5.898846	398.532274	6.348531
5.877352	395.757765	6.353536
5.924861	388.859459	6.358541
5.777253	404.821970	6.363546
5.572068	399.915340	6.368550
5.773056	392.167223	6.373555
5.726082	401.365502	6.378560
5.977335	399.551195	6.383565
5.942943	402.008531	6.388570
5.611710	390.645278	6.393574
5.597188	387.635554	6.398579
5.818767	398.256610	6.403584
5.974937	379.679382	6.408589
5.603440	380.509536	6.413594
5.063237	383.299227	6.418598
5.858305	398.326238	6.423603
5.559982	404.042550	6.428608
5.862559	392.118069	6.433613
5.917986	406.656682	6.438618
6.193299	409.846962	6.443622
6.001824	391.014135	6.448627
5.647168	383.868786	6.453632
5.494636	377.334029	6.458637
6.131691	372.934538	6.463642
5.959617	381.706307	6.468646
5.690993	373.864095	6.473651
5.741339	378.000801	6.478656
5.763993	376.041975	6.483661
5.794718	376.793290	6.488666
5.580956	373.830605	6.493670
5.692858	373.955417	6.498675
5.409865	384.142981	6.503680
5.326527	379.315344	6.508685
5.701729	394.151866	6.513690
5.722136	391.975086	6.518694
5.857905	394.921464	6.523699
5.705887	401.924681	6.528704
5.616965	399.268307	6.533709
6.084760	403.716109	6.538714
5.897555	396.908360	6.543718
5.712957	379.317855	6.548723
5.757032	389.783216	6.553728
5.752104	372.727730	6.558733
5.540686	377.503414	6.563738
5.629415	390.986404	6.568742
6.021710	388.346385	6.573747
5.754034	396.174498	6.578752
5.545961	388.689797	6.583757
5.462604	397.609029	6.588762
5.552170	401.277676	6.593766
5.911561	389.258872	6.598771
5.727714	398.013511	6.603776
5.832063	399.107641	6.608781
6.139900	401.084237	6.613786
5.573595	390.526628	6.618790
5.731562	392.346367	6.623795
5.501697	398.668898	6.628800
5.848612	401.319597	6.633805
5.849855	399.769094	6.638810
5.535380	400.517548	6.643814
5.494341	393.775486	6.648819
5.815693	408.993790	6.653824
5.919465	396.461360	6.658829
6.162757	406.500037	6.663834
5.666493	398.952915	6.668838
5.762381	388.478220	6.673843
5.544075	376.825193	6.678848
6.124888	400.295246	6.683853
5.514664	395.104058	6.688858
5.881851	398.124912	6.693862
5.787769	383.510048	6.698867
5.747764	387.338202	6.703872
5.607732	380.010527	6.708877
5.830028	371.202360	6.713882
5.588218	381.709344	6.718886
6.127327	379.340561	6.723891
5.468068	389.533296	6.728896
5.461037	381.396987	6.733901
5.840517	394.960978	6.738906
5.768774	388.793219	6.743910
6.315085	388.087483	6.748915
5.781729	382.105951	6.753920
5.822908	377.157563	6.758925
5.928290	374.685889	6.763930
5.901408	373.475162	6.768934
5.713606	369.790220	6.773939
5.781400	373.519221	6.778944
6.136904	366.702383	6.783949
5.978088	375.307553	6.788954
6.219348	380.410954	6.793958
5.721980	376.999146	6.798963
5.488720	378.117698	6.803968
5.661429	376.587789	6.808973
6.070972	375.226422	6.813978
5.897676	369.947800	6.818982
5.921503	374.854307	6.823987
5.848391	375.922456	6.828992
5.674746	364.914188	6.833997
5.838385	368.030206	6.839002
5.140103	369.515853	6.844006
5.684817	369.430480	6.849011
5.793425	374.643251	6.854016
5.776374	367.482978	6.859021
5.957917	371.633929	6.864026
5.695685	374.142778	6.869030
5.696040	374.582467	6.874035
6.028249	381.582575	6.879040
5.661899	372.762230	6.884045
6.032324	378.304149	6.889050
5.951436	375.858497	6.894054
5.806764	359.172941	6.899059
5.658684	365.368749	6.904064
5.821382	357.727889	6.909069
5.761333	360.303137	6.914074
5.322980	343.397848	6.919078
5.460529	370.417524	6.924083
5.438672	380.149708	6.929088
5.447522	370.027192	6.934093
5.472995	363.929633	6.939098
5.580741	375.580938	6.944102
5.489638	374.715639	6.949107
5.583874	371.400969	6.954112
5.442037	364.253921	6.959117
5.873321	371.463133	6.964122
5.917340	374.544110	6.969126
5.900299	371.218400	6.974131
5.753657	372.396148	6.979136
6.082128	382.374008	6.984141
5.817720	370.813631	6.989146
5.940540	376.736038	6.994150
5.579334	377.121644	6.999155
5.484209	380.442727	7.004160
5.742882	378.997428	7.009165
5.729839	377.101144	7.014170
5.696612	374.442375	7.019174
5.551485	374.518872	7.024179
5.665464	373.061442	7.029184
5.797732	380.868015	7.034189
6.068751	376.579659	7.039194
5.774804	376.755405	7.044198
5.962463	372.745873	7.049203
5.825036	380.341595	7.054208
5.943282	387.273985	7.059213
6.354606	381.495626	7.064218
5.723920	380.167526	7.069222
5.941528	373.666527	7.074227
5.838552	382.838769	7.079232
5.754023	375.464434	7.084237
5.655553	367.696807	7.089242
5.976822	374.084842	7.094246
5.904751	356.362831	7.099251
5.564818	363.041126	7.104256
5.804536	360.089651	7.109261
5.361853	356.343404	7.114266
5.757329	364.263758	7.119270
5.642015	362.124065	7.124275
5.425782	370.529416	7.129280
5.734096	377.121967	7.134285
6.015683	383.614302	7.139290
5.709454	382.007569	7.144294
5.774251	375.236276	7.149299
5.735966	374.982813	7.154304
5.625088	375.965127	7.159309
5.774370	376.305551	7.164314
5.734104	372.945514	7.169318
5.632820	371.449044	7.174323
5.380576	381.831110	7.179328
5.583602	371.934440	7.184333
5.521629	370.001529	7.189338
5.553221	380.585902	7.194342
5.871529	375.543472	7.199347
5.737627	376.519902	7.204352
5.554485	378.937264	7.209357
5.518111	377.218646	7.214362
5.814963	378.244648	7.219366
5.759603	374.225734	7.224371
5.789882	376.511578	7.229376
5.515659	377.082876	7.234381
5.762944	376.136084	7.239386
5.424713	375.126003	7.244390
5.705066	371.019688	7.249395
5.613565	377.162342	7.254400
5.674533	379.547784	7.259405
5.604823	371.883219	7.264410
5.475536	378.838571	7.269414
6.077700	376.744653	7.274419
5.606796	386.167538	7.279424
5.764093	380.330901	7.284429
5.596226	371.264318	7.289434
5.631078	386.467380	7.294438
5.938193	379.819474	7.299443
5.932028	379.162335	7.304448
5.651795	372.688718	7.309453
5.702340	374.927093	7.314458
5.641178	385.940463	7.319462
5.610754	380.462278	7.324467
5.577974	389.762733	7.329472
5.914329	392.326498	7.334477
6.011915	400.521338	7.339482
5.563084	390.432553	7.344486
5.800808	383.330435	7.349491
5.587519	383.278403	7.354496
5.642852	387.721221	7.359501
6.108998	386.259234	7.364506
5.766793	394.481848	7.369510
5.905759	374.967660	7.374515
5.644503	376.166530	7.379520
5.646828	372.666939	7.384525
5.790682	373.153749	7.389530
5.241417	381.854900	7.394534
5.904317	391.312119	7.399539
5.668717	392.826517	7.404544
5.940937	393.419769	7.409549
6.175247	384.790052	7.414554
5.827255	379.311002	7.419558
5.828840	368.936518	7.424563
5.792917	370.384827	7.429568
6.033464	379.057143	7.434573
5.974735	372.352663	7.439578
5.856927	377.983734	7.444582
5.937774	374.456020	7.449587
5.917991	373.187232	7.454592
6.103381	376.714306	7.459597
6.241783	377.822082	7.464602
5.869190	373.131519	7.469606
5.782363	364.571111	7.474611
5.572496	363.243518	7.479616
5.745541	370.467880	7.484621
5.835638	366.220529	7.489626
5.604123	365.560733	7.494630
5.605004	362.592894	7.499635
5.531478	366.843920	7.504640
5.677595	368.159300	7.509645
5.466603	375.722253	7.514650
5.373943	375.401377	7.519654
5.383006	375.776426	7.524659
5.572829	383.289237	7.529664
5.581045	379.146464	7.534669
5.868863	372.963504	7.539674
5.566251	378.044549	7.544678
5.960290	366.991628	7.549683
5.833402	372.361522	7.554688
5.942404	379.785752	7.559693
5.801570	375.131645	7.564698
5.739792	371.525036	7.569702
5.620206	377.070961	7.574707
5.333406	376.021184	7.579712
5.496909	377.052259	7.584717
5.744204	371.157230	7.589722
5.576803	384.079218	7.594726
5.473696	375.518191	7.599731
5.334369	386.271719	7.604736
5.651191	391.913792	7.609741
5.644247	390.456324	7.614746
5.726495	410.476831	7.619750
6.140965	408.687571	7.624755
5.778625	395.057553	7.629760
5.851939	402.098232	7.634765
5.844508	381.265508	7.639770
5.694462	381.111815	7.644774
5.909991	376.199386	7.649779
5.581730	383.312469	7.654784
5.861887	371.242815	7.659789
5.685854	374.437365	7.664794
5.434583	384.158039	7.669798
5.956163	377.432238	7.674803
5.782203	374.124787	7.679808
5.617917	376.959984	7.684813
5.997390	376.615755	7.689818
5.623806	382.261592	7.694822
5.868751	373.785242	7.699827
5.670074	376.853623	7.704832
5.594695	381.813643	7.709837
5.828088	384.871277	7.714842
5.172606	381.085599	7.719846
5.842204	384.859519	7.724851
5.951253	395.833572	7.729856
5.573286	393.108589	7.734861
6.064960	390.500456	7.739866
6.003813	392.699384	7.744870
5.928556	381.992074	7.749875
5.663205	376.386178	7.754880
5.658293	381.790749	7.759885
5.944348	376.563542	7.764890
5.695502	381.006561	7.769894
5.698165	377.472114	7.774899
5.857360	377.478782	7.779904
5.549876	385.022055	7.784909
5.873234	370.095018	7.789914
5.608838	377.147470	7.794918
5.943579	378.654765	7.799923
5.750038	376.163486	7.804928
5.833930	377.899915	7.809933
5.551722	374.735977	7.814938
5.775848	388.188259	7.819942
5.864833	379.524365	7.824947
5.861542	381.685752	7.829952
5.711139	380.747485	7.834957
5.858153	377.054375	7.839962
5.651538	372.223909	7.844966
5.661721	374.642619	7.849971
5.359926	371.665253	7.854976
5.825514	374.958595	7.859981
6.051818	377.843328	7.864986
5.787512	375.075228	7.869990
6.055056	370.024934	7.874995
5.845257	376.486687	7.880000
5.810629	377.488693	7.885005
6.013198	367.864186	7.890010
5.577240	372.516858	7.895014
5.556207	369.463864	7.900019
5.685560	375.173270	7.905024
5.470283	366.243835	7.910029
5.477139	371.247916	7.915034
5.517160	375.898780	7.920038
5.421266	376.473776	7.925043
5.705535	381.886823	7.930048
5.465227	375.894180	7.935053
5.718694	376.291048	7.940058
5.707302	397.870162	7.945062
5.659433	396.219784	7.950067
6.008415	402.448459	7.955072
5.870327	391.659236	7.960077
5.877287	370.536361	7.965082
5.724593	379.748030	7.970086
5.849057	377.456868	7.975091
5.514300	378.066126	7.980096
5.353131	377.240279	7.985101
6.038302	383.713674	7.990106
5.723443	398.936736	7.995110
6.183361	383.368180	8.000115
5.952334	378.591819	8.005133
5.566935	377.067983	8.010150
5.643424	375.014193	8.015168
5.851898	372.011930	8.020186
5.910543	375.306797	8.025203
6.212996	375.363521	8.030221
5.890454	369.272917	8.035238
5.977141	376.949899	8.040256
5.716782	379.821384	8.045274
5.623809	376.964180	8.050291
5.507074	378.042779	8.055309
5.677699	378.306348	8.060326
5.656930	372.701785	8.065344
5.589143	382.290118	8.070362
5.751713	366.400603	8.075379
5.577062	380.111323	8.080397
5.779435	376.065458	8.085414
6.251585	383.719917	8.090432
5.830639	385.130199	8.095450
5.999363	381.717602	8.100467
5.776403	382.222716	8.105485
5.634455	379.884419	8.110502
5.762057	373.249920	8.115520
5.383687	387.794129	8.120538
5.791249	391.510851	8.125555
5.884184	400.367120	8.130573
5.941178	397.562154	8.135590
6.105413	398.640912	8.140608
5.878146	409.469217	8.145626
5.987278	404.093597	8.150643
6.259791	394.375292	8.155661
6.013166	385.801823	8.160678
5.493574	382.806337	8.165696
5.601966	388.523349	8.170714
5.862130	395.598810	8.175731
5.869341	409.028597	8.180749
6.128721	406.135115	8.185766
5.838517	400.534890	8.190784
6.218735	412.148474	8.195802
6.111078	393.148662	8.200819
5.628879	398.481692	8.205837
5.714168	402.756988	8.210854
5.988264	405.257564	8.215872
6.421453	409.431016	8.220890
6.149376	400.053652	8.225907
5.708663	384.375407	8.230925
5.589736	394.754389	8.235942
5.918959	397.678666	8.240960
5.973771	405.007209	8.245978
6.317662	396.757774	8.250995
6.184683	406.179611	8.256013
5.816766	406.868383	8.261030
6.361249	396.990700	8.266048
5.917351	391.528166	8.271066
5.914810	388.994457	8.276083
6.059086	401.146769	8.281101
5.921238	404.709110	8.286118
6.165514	400.186465	8.291136
6.155055	407.720892	8.296154
5.943180	405.926872	8.301171
5.858350	403.235643	8.306189
5.790159	410.854856	8.311206
6.016081	399.452357	8.316224
5.913652	405.890364	8.321242
5.914823	398.284755	8.326259
6.208762	401.908829	8.331277
5.904828	402.189949	8.336294
6.047792	401.154521	8.341312
6.163436	404.121730	8.346330
6.026788	395.455287	8.351347
6.059070	398.700641	8.356365
5.841405	411.263114	8.361382
6.122425	398.848448	8.366400
5.874232	404.949536	8.371418
6.035848	396.308943	8.376435
5.982671	401.249710	8.381453
5.968037	403.457856	8.386470
5.942584	388.418281	8.391488
5.884098	402.694635	8.396506
5.808285	398.635546	8.401523
6.221183	405.570317	8.406541
6.459854	426.146380	8.411558
6.573414	414.266020	8.416576
6.150049	413.887362	8.421594
5.922905	393.915359	8.426611
6.188122	405.199823	8.431629
5.817020	401.789752	8.436646
6.048126	418.905116	8.441664
6.408737	430.206208	8.446682
6.365982	423.702523	8.451699
6.235066	415.966125	8.456717
5.937429	419.676580	8.461734
6.088526	418.614630	8.466752
6.087991	421.470658	8.471770
6.215614	423.555534	8.476787
6.473668	425.664154	8.481805
6.490941	426.235771	8.486822
6.560245	419.108622	8.491840
6.076244	420.137471	8.496858
6.109929	416.515653	8.501875
6.451747	414.978858	8.506893
6.357796	428.392952	8.511910
6.386070	418.927494	8.516928
6.098523	420.405239	8.521946
6.375059	413.753702	8.526963
6.315408	408.139441	8.531981
6.222128	422.134087	8.536998
6.082914	423.301416	8.542016
6.313429	424.934675	8.547034
6.459743	420.190690	8.552051
6.698358	435.537662	8.557069
5.912122	418.414532	8.562087
6.125464	428.324912	8.567104
6.219030	429.509417	8.572122
6.505522	433.500735	8.577139
6.527395	430.426714	8.582157
6.373930	433.814785	8.587175
6.375008	425.966184	8.592192
6.240191	427.527296	8.597210
6.437420	429.497126	8.602227
6.361006	430.484204	8.607245
6.187929	438.697369	8.612263
6.154569	433.489232	8.617280
6.379837	425.103737	8.622298
6.343498	430.767701	8.627315
6.560800	431.904418	8.632333
6.420439	435.792204	8.637351
6.361558	416.245088	8.642368
6.579766	424.545261	8.647386
6.504264	425.418588	8.652403
6.666523	421.262234	8.657421
6.286396	425.856608	8.662439
6.468420	430.246141	8.667456
6.592444	431.195503	8.672474
6.493388	429.393272	8.677491
6.389242	434.566094	8.682509
6.373662	429.692839	8.687527
6.422382	430.616131	8.692544
6.315055	430.613985	8.697562
6.074526	429.932128	8.702579
6.499105	428.249822	8.707597
6.408973	433.171142	8.712615
6.254936	432.147533	8.717632
6.290967	436.869207	8.722650
6.507802	429.753652	8.727667
6.650566	431.040902	8.732685
6.092641	431.418622	8.737703
6.386520	428.967851	8.742720
6.597465	427.009752	8.747738
6.674091	436.433477	8.752755
6.862267	429.587498	8.757773
6.443795	439.079330	8.762791
6.936191	426.331727	8.767808
7.125310	428.069300	8.772826
6.722508	433.143750	8.777843
6.900641	431.853504	8.782861
6.554692	423.216685	8.787879
6.737647	424.888953	8.792896
6.748421	428.418546	8.797914
6.681079	429.637730	8.802931
6.914301	427.354252	8.807949
6.306066	423.653130	8.812967
6.358874	423.237734	8.817984
6.729819	426.051339	8.823002
6.734658	425.851739	8.828019
6.655342	424.737529	8.833037
6.576943	432.686551	8.838055
6.845861	434.648305	8.843072
6.851344	428.673541	8.848090
6.753602	435.353819	8.853107
6.850181	425.599947	8.858125
6.450790	414.235453	8.863143
6.502898	422.271319	8.868160
6.836785	431.683136	8.873178
6.523601	431.230411	8.878195
7.058670	431.638849	8.883213
6.556735	426.867044	8.888231
6.696443	433.412288	8.893248
6.778378	426.665006	8.898266
6.353285	432.519268	8.903283
6.330491	428.827402	8.908301
6.573639	430.193597	8.913319
6.663181	433.871793	8.918336
6.505110	434.291004	8.923354
6.470693	437.606775	8.928371
6.603409	423.949862	8.933389
6.407366	438.351937	8.938407
6.363813	432.589981	8.943424
6.690284	447.430898	8.948442
6.695113	452.166933	8.953459
6.784642	452.878706	8.958477
7.176169	452.776309	8.963495
6.990600	451.356855	8.968512
6.755678	430.057449	8.973530
6.767628	430.166001	8.978547
6.584754	433.826921	8.983565
6.285175	436.720339	8.988583
6.714854	441.718005	8.993600
6.845101	453.724229	8.998618
6.875287	463.511848	9.003635
6.695340	452.131882	9.008653
7.157408	450.683539	9.013671
6.853415	448.301194	9.018688
7.021389	448.741903	9.023706
6.403178	460.720235	9.028723
6.638307	454.621120	9.033741
6.975814	454.441981	9.038759
7.029743	465.245196	9.043776
7.201648	454.191949	9.048794
7.035294	463.271911	9.053811
6.861848	460.042296	9.058829
6.917232	460.456465	9.063847
6.967143	463.913662	9.068864
6.896360	456.417131	9.073882
6.671350	456.960438	9.078899
7.168544	463.462305	9.083917
6.895884	468.068254	9.088935
6.640880	462.790694	9.093952
6.962856	460.982451	9.098970
6.781136	456.352969	9.103987
6.952396	464.108255	9.109005
6.635958	456.277832	9.114023
6.839740	455.182379	9.119040
7.031584	448.692420	9.124058
7.015628	456.751589	9.129075
7.165885	455.446773	9.134093
6.919377	457.322031	9.139111
6.855531	449.625602	9.144128
6.927574	453.688393	9.149146
6.820813	458.748024	9.154163
6.678644	461.765104	9.159181
7.151584	459.298897	9.164199
6.833666	462.545484	9.169216
7.218665	471.652671	9.174234
7.335570	467.184678	9.179251
6.962253	454.951390	9.184269
7.101397	461.556692	9.189287
6.685951	464.995284	9.194304
7.235976	466.259751	9.199322
6.939161	480.504081	9.204339
7.402671	481.728456	9.209357
7.479717	481.340819	9.214375
7.204296	466.895761	9.219392
7.247134	462.704460	9.224410
7.127887	456.840747	9.229427
6.745289	458.469087	9.234445
6.741439	457.914246	9.239463
7.417609	469.270060	9.244480
7.588482	462.417312	9.249498
7.287492	463.856142	9.254515
7.223341	464.677201	9.259533
7.336109	466.773876	9.264551
6.999943	458.012432	9.269568
7.304466	457.567064	9.274586
6.940427	464.809780	9.279603
7.009245	455.236965	9.284621
7.364534	450.049979	9.289639
6.573496	460.685783	9.294656
7.329699	467.951794	9.299674
7.290294	478.466686	9.304691
7.383239	478.543614	9.309709
7.335151	466.467641	9.314727
7.127032	466.560182	9.319744
7.145201	463.417308	9.324762
7.293995	477.430873	9.329779
7.106004	477.864240	9.334797
7.527468	482.629678	9.339815
7.367752	483.134353	9.344832
7.361132	467.820363	9.349850
7.127768	471.394527	9.354867
7.129166	469.743808	9.359885
7.528668	477.195098	9.364903
7.358404	481.488363	9.369920
7.322207	468.706787	9.374938
7.325594	469.274269	9.379955
7.122638	466.304895	9.384973
6.972046	471.425046	9.389991
6.936121	477.754829	9.395008
7.182570	476.368670	9.400026
7.537978	476.925178	9.405043
7.821246	483.309094	9.410061
7.918297	475.174037	9.415079
7.629943	469.074886	9.420096
7.149939	467.016760	9.425114
7.161445	469.722588	9.430131
7.199341	475.841991	9.435149
7.485776	471.615676	9.440167
7.161111	476.816750	9.445184
7.688316	471.375606	9.450202
7.790559	479.993773	9.455219
7.328733	475.979369	9.460237
7.427111	468.181776	9.465255
7.369749	473.798556	9.470272
7.253481	476.505469	9.475290
7.526940	484.771767	9.480307
7.766078	486.684545	9.485325
7.640703	478.546467	9.490343
7.384629	464.508630	9.495360
7.263235	460.160026	9.500378
7.386745	468.976826	9.505395
7.440860	480.692041	9.510413
7.721826	478.644071	9.515431
7.480207	480.995088	9.520448
7.631970	482.448188	9.525466
7.594620	486.928911	9.530483
7.578325	482.204076	9.535501
7.238174	469.448032	9.540519
7.327872	477.727340	9.545536
7.661213	480.114502	9.550554
7.321419	476.257702	9.555571
7.536828	494.644222	9.560589
7.491370	480.513413	9.565607
7.273684	479.013784	9.570624
7.358640	484.813394	9.575642
7.396761	486.423154	9.580659
7.668562	485.184499	9.585677
7.600486	479.325385	9.590695
7.379698	483.601321	9.595712
7.366702	481.252272	9.600730
7.368856	472.961673	9.605747
7.670095	484.641327	9.610765
7.963492	471.192731	9.615783
7.437009	480.471136	9.620800
7.639563	473.288375	9.625818
7.413927	475.296062	9.630835
7.517550	478.375620	9.635853
7.568153	475.959803	9.640871
7.994980	500.129307	9.645888
7.759579	485.769480	9.650906
7.635763	480.282014	9.655923
7.568849	488.336558	9.660941
7.768615	488.226336	9.665959
7.773725	489.194333	9.670976
7.654432	491.753402	9.675994
7.794017	499.403214	9.681011
7.576375	482.001588	9.686029
7.909315	482.842481	9.691047
8.024105	494.570290	9.696064
7.601076	489.666185	9.701082
7.614420	483.141066	9.706099
7.609912	499.498166	9.711117
8.204222	490.613009	9.716135
7.624136	485.518920	9.721152
7.342671	485.086470	9.726170
7.703257	503.920464	9.731187
7.802998	505.577375	9.736205
7.943265	501.392891	9.741223
7.953252	509.485887	9.746240
8.139743	507.080334	9.751258
8.314728	488.799835	9.756275
7.840488	490.808607	9.761293
8.105127	482.101338	9.766311
7.918399	473.382745	9.771328
7.792462	475.128660	9.776346
8.162476	481.091888	9.781363
7.864646	487.320701	9.786381
8.071084	470.875114	9.791399
7.888730	481.611219	9.796416
7.938554	477.122177	9.801434
7.936608	475.749690	9.806451
7.804809	481.315019	9.811469
7.861069	482.543243	9.816487
8.212818	478.669609	9.821504
7.820129	484.878569	9.826522
7.590444	485.154369	9.831539
7.650367	491.876236	9.836557
8.057744	478.239364	9.841575
7.631180	485.321472	9.846592
7.698390	483.237565	9.851610
8.124625	495.771794	9.856627
8.011750	490.408842	9.861645
8.227687	476.760941	9.866663
8.266466	479.831723	9.871680
8.057329	480.890092	9.876698
8.131303	484.081592	9.881715
8.216898	473.647766	9.886733
7.919606	467.474278	9.891751
7.738583	481.318617	9.896768
7.644378	475.583518	9.901786
7.890049	488.146033	9.906803
7.808375	496.234450	9.911821
8.388011	505.588868	9.916839
8.139335	514.145270	9.921856
8.268516	509.056809	9.926874
8.108385	486.672650	9.931891
7.863320	489.074700	9.936909
8.002470	486.269471	9.941927
8.087654	498.879228	9.946944
8.288784	507.579744	9.951962
8.136543	506.593719	9.956979
8.313895	503.662581	9.961997
8.505141	500.722956	9.967015
7.961720	482.551868	9.972032
8.109286	482.143715	9.977050
8.151758	483.598160	9.982067
7.833228	494.475529	9.987085
8.317628	487.898693	9.992103
8.365267	504.231849	9.997120
8.233206	505.192937	10.002138
8.186638	499.904799	10.007155
8.164249	506.513337	10.012173
8.206170	503.085870	10.017191
8.119003	499.085342	10.022208
8.197853	504.062256	10.027226
8.212897	507.812100	10.032243
8.118745	513.507240	10.037261
8.467648	506.352027	10.042279
8.463407	505.510070	10.047296
8.483178	504.932591	10.052314
8.327599	493.315253	10.057331
7.760194	492.343783	10.062349
8.371026	487.381834	10.067367
8.306682	501.192128	10.072384
8.221065	507.766392	10.077402
8.542639	515.100520	10.082419
8.365686	503.710584	10.087437
8.380123	495.853548	10.092455
8.245806	504.530882	10.097472
8.123382	504.591061	10.102490
8.205764	502.293338	10.107507
8.049199	510.380873	10.112525
7.828208	505.874295	10.117543
8.136118	506.135291	10.122560
8.215388	502.796646	10.127578
8.628313	505.414338	10.132595
8.321201	515.889147	10.137613
8.286460	505.963303	10.142631
8.268473	516.588471	10.147648
7.871776	512.437623	10.152666
8.517471	504.841436	10.157683
8.118497	505.670776	10.162701
8.186567	518.961723	10.167719
8.196579	528.714669	10.172736
8.495734	528.323788	10.177754
8.957222	534.455738	10.182771
8.724015	538.995563	10.187789
8.239155	522.926483	10.192807
8.822714	519.095414	10.197824
8.300714	528.805485	10.202842
8.854771	520.731346	10.207859
8.685171	521.130275	10.212877
8.378665	512.872239	10.217895
8.480543	510.041288	10.222912
7.997451	505.821927	10.227930
8.487788	528.182721	10.232947
8.707886	529.502042	10.237965
8.532935	533.338464	10.242983
9.030693	533.168930	10.248000
8.573780	529.150588	10.253018
8.443856	514.297688	10.258035
8.690682	525.408386	10.263053
8.825276	526.160439	10.268071
8.652674	511.408901	10.273088
8.529450	508.155631	10.278106
8.434014	506.804101	10.283123
8.505017	529.612448	10.288141
8.719334	528.392264	10.293159
8.726320	537.359898	10.298176
8.587141	546.359904	10.303194
8.855920	536.853545	10.308211
8.648084	540.007159	10.313229
8.836065	540.820275	10.318247
8.573044	524.435571	10.323264
8.506787	530.962629	10.328282
8.643801	532.642105	10.333299
8.813413	543.058015	10.338317
8.588492	535.939049	10.343335
8.735126	539.321146	10.348352
8.684305	544.889586	10.353370
8.680394	535.694195	10.358387
8.378029	543.085069	10.363405
8.294016	537.474584	10.368423
8.411776	527.237658	10.373440
8.464273	531.505500	10.378458
8.739799	527.094690	10.383475
8.846134	535.434534	10.388493
8.911164	541.559175	10.393511
9.177788	541.492126	10.398528
8.789855	533.698117	10.403546
9.208378	525.550538	10.408563
9.155620	524.949710	10.413581
8.771460	531.403502	10.418599
9.087217	529.006094	10.423616
9.204224	533.951791	10.428634
8.937830	523.030290	10.433651
9.036890	529.468330	10.438669
8.715262	530.512770	10.443687
8.989083	528.229229	10.448704
8.909233	528.396346	10.453722
9.162357	518.576871	10.458739
8.749560	529.528991	10.463757
8.745060	524.931684	10.468775
8.860045	520.672261	10.473792
9.028315	529.497856	10.478810
8.973105	528.673351	10.483827
8.541459	532.881350	10.488845
8.640619	532.922590	10.493863
8.641501	522.047575	10.498880
8.943934	528.564203	10.503898
8.863278	528.848211	10.508915
8.781314	523.840165	10.513933
8.820595	531.464682	10.518951
8.992243	527.979015	10.523968
8.962062	530.300066	10.528986
9.231511	528.001431	10.534003
9.406711	526.171998	10.539021
9.239852	528.138924	10.544039
9.257771	527.419725	10.549056
9.025183	526.020256	10.554074
9.196298	527.233643	10.559091
9.151241	534.091894	10.564109
8.957887	530.291033	10.569127
9.176767	518.876937	10.574144
8.883785	524.593766	10.579162
8.726545	516.296562	10.584179
8.590632	532.011566	10.589197
8.747658	537.471699	10.594215
9.476327	547.260378	10.599232
8.943868	557.798921	10.604250
8.976645	548.944912	10.609267
9.387953	560.569502	10.614285
9.236124	554.057613	10.619303
9.539734	548.607297	10.624320
9.260310	545.795058	10.629338
9.415847	538.850009	10.634355
9.247056	521.816229	10.639373
9.240609	518.336378	10.644391
9.170853	517.116523	10.649408
8.884425	526.177460	10.654426
9.337074	530.117519	10.659443
9.024335	528.553883	10.664461
8.671159	545.688332	10.669479
9.084205	546.570326	10.674496
9.191938	561.089005	10.679514
9.486168	555.810570	10.684531
9.233507	562.505700	10.689549
9.140767	557.896964	10.694567
9.452100	551.101069	10.699584
9.468638	544.812111	10.704602
9.577969	554.852466	10.709619
9.205721	554.361655	10.714637
9.328040	560.647740	10.719655
9.455158	556.695675	10.724672
9.289478	563.355088	10.729690
9.402060	564.757529	10.734707
9.390423	555.629610	10.739725
9.349583	558.542468	10.744743
9.502715	552.989496	10.749760
9.284990	561.818781	10.754778
9.186715	554.818820	10.759795
9.050960	550.346213	10.764813
9.235838	561.211020	10.769831
9.593324	551.211074	10.774848
9.628719	556.564038	10.779866
9.679057	557.884713	10.784883
9.588220	552.461485	10.789901
9.411244	556.500201	10.794919
9.790360	554.522050	10.799936
9.522201	560.588450	10.804954
9.415231	558.800068	10.809971
9.499377	546.349874	10.814989
9.240119	550.426726	10.820007
9.288661	554.272317	10.825024
9.612220	550.374682	10.830042
9.333824	549.140177	10.835059
9.756694	551.103069	10.840077
9.223920	556.500874	10.845095
9.452768	549.083589	10.850112
9.523462	555.204192	10.855130
9.588841	552.937529	10.860147
9.641928	544.702031	10.865165
9.545406	557.485467	10.870183
9.596541	547.811232	10.875200
9.471111	547.900284	10.880218
9.540487	545.118601	10.885235
9.768951	548.298530	10.890253
9.638064	552.891755	10.895271
9.666274	550.179636	10.900288
9.362411	556.289498	10.905306
9.431557	543.071643	10.910323
9.293317	562.798050	10.915341
9.413126	561.497998	10.920359
9.930778	575.602170	10.925376
9.757697	571.422583	10.930394
9.715711	573.849630	10.935411
9.708950	567.150906	10.940429
9.506374	583.927280	10.945447
9.821857	583.363427	10.950464
9.556084	575.471364	10.955482
9.976581	570.643355	10.960499
9.943287	586.881970	10.965517
10.005933	583.886741	10.970535
10.058868	574.032329	10.975552
10.142556	577.881886	10.980570
9.880350	575.461419	10.985587
10.083257	560.313336	10.990605
9.341604	552.281250	10.995623
9.625975	564.156103	11.000640
9.807260	571.739453	11.005658
9.758491	579.825908	11.010675
9.595871	578.869907	11.015693
9.517118	584.960287	11.020711
9.633773	573.088804	11.025728
9.878250	579.712361	11.030746
9.534451	581.293606	11.035763
9.990623	578.833166	11.040781
9.693449	577.973986	11.045799
10.065407	573.219853	11.050816
9.642416	579.127482	11.055834
9.785478	576.621426	11.060851
10.052498	566.790280	11.065869
9.593176	573.568287	11.070887
10.226964	582.747004	11.075904
10.000023	585.007372	11.080922
10.331547	586.337641	11.085939
10.045847	574.920517	11.090957
10.159814	577.187431	11.095975
10.101432	568.817909	11.100992
10.147703	572.502914	11.106010
9.826934	573.108565	11.111027
9.933802	576.537925	11.116045
9.727659	583.355162	11.121063
10.036297	583.022756	11.126080
10.329400	596.452071	11.131098
9.903398	587.013519	11.136115
10.257511	585.045594	11.141133
9.828813	583.992427	11.146151
10.327064	576.431935	11.151168
9.791399	582.906327	11.156186
9.930991	586.485195	11.161203
10.574988	595.760149	11.166221
10.155260	604.756805	11.171239
10.708134	600.984175	11.176256
10.396009	589.855204	11.181274
10.409624	582.787208	11.186291
10.413407	586.409446	11.191309
10.252077	572.400860	11.196327
9.863831	577.406798	11.201344
10.234042	579.138103	11.206362
9.981110	577.827024	11.211379
10.286990	573.607106	11.216397
9.813995	578.885099	11.221415
10.083697	578.861749	11.226432
10.241666	591.624270	11.231450
10.449462	602.810559	11.236467
10.366238	597.329320	11.241485
10.605258	608.245633	11.246503
10.529747	587.126189	11.251520
10.029557	589.101168	11.256538
10.267307	589.521480	11.261555
10.091074	580.106914	11.266573
10.162219	591.737484	11.271591
10.489133	610.406453	11.276608
10.423115	606.412055	11.281626
10.169062	606.486547	11.286643
10.680863	598.750353	11.291661
10.638630	605.090638	11.296679
10.745177	593.779302	11.301696
10.228946	588.091355	11.306714
10.205350	583.011031	11.311731
10.465061	583.099700	11.316749
10.488820	598.477321	11.321767
10.671384	591.111452	11.326784
10.414568	586.455832	11.331802
10.391031	591.726523	11.336819
11.038373	585.982499	11.341837
10.440646	585.596442	11.346855
10.612783	575.581342	11.351872
10.169228	577.317072	11.356890
10.403537	576.500851	11.361907
10.372176	577.335712	11.366925
10.877672	587.124666	11.371943
10.611235	584.831092	11.376960
10.492029	575.035209	11.381978
10.316827	577.019227	11.386995
10.468822	587.201238	11.392013
10.813719	595.547913	11.397031
10.557257	601.079163	11.402048
10.680028	594.284394	11.407066
10.496478	597.793974	11.412083
10.298871	600.359016	11.417101
10.406462	605.334611	11.422119
10.474919	602.467856	11.427136
10.379500	591.251282	11.432154
10.566903	597.710219	11.437171
10.614013	594.591190	11.442189
10.569771	597.469874	11.447207
10.438813	596.862360	11.452224
10.384469	591.954110	11.457242
10.705247	600.462356	11.462259
10.540967	585.302355	11.467277
10.764668	587.754048	11.472295
11.059074	594.092077	11.477312
11.198615	591.151070	11.482330
10.789812	593.679775	11.487347
10.542885	600.440293	11.492365
10.806541	599.048272	11.497383
10.372804	589.696137	11.502400
10.404366	603.996412	11.507418
10.396516	614.645296	11.512435
11.014401	615.892831	11.517453
11.101779	623.475137	11.522471
10.812702	617.316088	11.527488
11.263449	625.712464	11.532506
10.925735	626.869882	11.537523
10.831430	612.355303	11.542541
10.687495	606.504876	11.547559
10.933600	613.506887	11.552576
11.143651	617.620676	11.557594
11.077702	617.760370	11.562611
10.659376	607.282344	11.567629
11.082803	613.480244	11.572647
10.900060	620.716708	11.577664
11.204207	620.609066	11.582682
10.905616	617.238085	11.587699
11.161071	602.763387	11.592717
11.068211	604.374745	11.597735
10.878259	600.601737	11.602752
11.117952	599.917215	11.607770
10.672518	612.673307	11.612787
11.206445	608.764789	11.617805
11.338655	607.879357	11.622823
10.940859	609.759399	11.627840
11.142007	602.832426	11.632858
10.943714	600.357760	11.637875
10.871319	603.133558	11.642893
11.206057	613.848685	11.647911
10.860887	628.211162	11.652928
11.147604	621.296021	11.657946
10.781842	621.927658	11.662963
11.282638	626.803782	11.667981
11.312211	620.298160	11.672999
11.206847	619.355276	11.678016
11.764093	623.297903	11.683034
10.980036	621.429409	11.688051
11.104739	620.172767	11.693069
11.320169	625.920422	11.698087
11.046469	624.262299	11.703104
11.087051	621.377818	11.708122
10.915827	636.558803	11.713139
11.032565	620.890838	11.718157
11.358321	619.230310	11.723175
11.186118	623.334565	11.728192
11.435360	619.363352	11.733210
11.243403	625.796531	11.738227
11.198349	621.966102	11.743245
11.097882	620.631131	11.748263
11.150362	622.582636	11.753280
11.066506	613.238785	11.758298
11.144982	627.941984	11.763315
11.125457	617.710737	11.768333
11.161894	628.459987	11.773351
11.448585	623.520385	11.778368
11.718506	611.097843	11.783386
11.245829	616.587235	11.788403
11.153362	616.557514	11.793421
11.250762	618.839652	11.798439
11.109821	631.358701	11.803456
11.829657	641.527513	11.808474
11.612871	635.439182	11.813491
11.592669	620.793065	11.818509
11.286057	617.224524	11.823527
11.152882	627.031517	11.828544
11.598780	642.560785	11.833562
11.687475	641.101500	11.838579
11.486191	639.479366	11.843597
11.712022	641.946512	11.848615
11.202696	644.453104	11.853632
11.635679	646.285034	11.858650
11.441303	655.631415	11.863667
11.399751	654.413443	11.868685
11.618673	644.416221	11.873703
11.463495	648.871264	11.878720
11.968686	644.320300	11.883738
11.991588	654.361630	11.888755
11.406521	639.974413	11.893773
11.231141	637.827512	11.898791
11.456612	638.877756	11.903808
11.623949	647.864502	11.908826
11.780963	651.216591	11.913843
11.763470	648.887160	11.918861
11.880983	640.644681	11.923879
11.415260	650.387025	11.928896
11.479294	635.213299	11.933914
11.442331	644.901085	11.938931
11.432405	646.240677	11.943949
11.776002	648.001405	11.948967
11.657141	653.754110	11.953984
11.593255	659.596032	11.959002
11.617539	653.624559	11.964019
11.388351	652.256105	11.969037
11.829321	645.379903	11.974055
11.528450	654.686165	11.979072
11.381650	668.667298	11.984090
11.941267	678.125930	11.989107
12.129861	673.444682	11.994125
12.014429	668.918367	11.999143
12.083142	670.671674	12.004160
12.350000	655.829072	12.009178
11.883211	646.119167	12.014195
11.880734	647.517552	12.019213
12.073618	646.651013	12.024231
11.587783	652.600070	12.029248
11.859827	638.495130	12.034266
11.935523	645.085195	12.039283
11.913616	648.376954	12.044301
11.872698	651.659070	12.049319
11.974414	663.900280	12.054336
11.887239	658.627924	12.059354
12.123995	662.109533	12.064371
12.006465	663.702671	12.069389
11.929383	667.517476	12.074407
12.061885	670.750333	12.079424
12.185177	674.240254	12.084442
12.265347	662.052535	12.089459
12.096922	653.684436	12.094477
12.380900	643.490828	12.099495
11.701558	647.141215	12.104512
11.981886	641.255861	12.109530
12.312321	651.820207	12.114547
11.952567	657.099414	12.119565
12.404883	650.609597	12.124583
12.013388	652.062622	12.129600
12.128813	643.082008	12.134618
11.949675	651.438231	12.139635
11.985753	664.614379	12.144653
12.408906	669.016684	12.149671
12.281672	668.436987	12.154688
12.266125	672.043335	12.159706
12.076953	663.930947	12.164723
12.471375	666.393772	12.169741
12.199480	670.737720	12.174759
11.819133	661.645426	12.179776
12.285134	667.101370	12.184794
12.644973	673.561720	12.189811
12.584520	664.630743	12.194829
12.301079	650.612826	12.199847
12.036842	649.470770	12.204864
12.153702	657.064250	12.209882
12.227505	659.959162	12.214899
12.089390	665.544473	12.219917
12.354560	661.769572	12.224935
12.176513	667.944965	12.229952
12.398733	665.884088	12.234970
12.554589	666.213092	12.239987
12.104564	666.135251	12.245005
12.464788	664.131647	12.250023
12.640389	664.713178	12.255040
12.581149	665.962667	12.260058
12.642996	661.575837	12.265075
12.447965	657.702627	12.270093
12.751046	652.037768	12.275111
12.367404	659.791719	12.280128
12.720618	664.971843	12.285146
12.433641	660.803769	12.290163
12.429181	668.946439	12.295181
12.594386	661.472807	12.300199
12.609629	657.986375	12.305216
12.500476	664.832628	12.310234
12.302400	660.852597	12.315251
12.341460	665.286678	12.320269
12.906811	665.848169	12.325287
12.548480	665.500341	12.330304
12.236249	658.208813	12.335322
12.458745	658.372741	12.340339
12.328440	659.021137	12.345357
12.478061	663.270637	12.350375
12.340568	676.799037	12.355392
12.048853	673.133477	12.360410
12.896560	684.187998	12.365427
12.852369	686.321915	12.370445
12.915164	686.236309	12.375463
12.505135	685.224392	12.380480
12.893327	698.225473	12.385498
12.977335	687.977965	12.390515
12.725338	687.780734	12.395533
12.777409	692.260121	12.400551
13.143472	690.334494	12.405568
12.773999	687.482692	12.410586
13.007285	685.514753	12.415603
12.660945	677.635268	12.420621
12.683932	680.670690	12.425639
12.995834	685.570114	12.430656
12.839289	686.345698	12.435674
13.293146	685.753851	12.440691
12.748817	681.761794	12.445709
12.856239	671.908258	12.450727
12.934723	673.562204	12.455744
12.869005	679.435979	12.460762
12.854175	687.378309	12.465779
12.752530	685.191447	12.470797
12.794581	684.926054	12.475815
12.819757	685.931944	12.480832
12.966563	688.761774	12.485850
13.209214	683.876392	12.490867
12.760106	691.577498	12.495885
13.188990	689.862936	12.500903
13.062095	689.671350	12.505920
13.211676	687.593449	12.510938
13.393695	689.654054	12.515955
12.778333	688.200936	12.520973
13.175325	682.107941	12.525991
13.278565	684.890947	12.531008
12.957683	691.694645	12.536026
13.260598	679.740259	12.541043
13.100536	684.985031	12.546061
13.267676	687.104771	12.551079
13.062734	688.522258	12.556096
13.152453	682.237565	12.561114
13.131325	682.262939	12.566131
13.108883	688.120468	12.571149
13.332458	682.925650	12.576167
13.229581	694.526748	12.581184
13.325684	683.166498	12.586202
13.221158	686.313419	12.591219
13.043796	684.491871	12.596237
13.307413	679.767309	12.601255
13.228623	688.066801	12.606272
13.052968	689.669048	12.611290
13.271531	687.873830	12.616307
13.250789	689.051017	12.621325
13.220838	682.791385	12.626343
12.996604	684.757850	12.631360
13.036694	689.056076	12.636378
13.305154	685.757183	12.641395
13.213624	690.902856	12.646413
13.379662	684.328492	12.651431
13.381684	690.617692	12.656448
13.578780	696.715383	12.661466
13.434474	693.951378	12.666483
13.260678	696.323354	12.671501
13.533347	694.649046	12.676519
13.593734	713.053769	12.681536
13.121104	706.046130	12.686554
13.480505	703.556654	12.691571
13.394016	716.142970	12.696589
13.629561	719.485924	12.701607
13.825513	713.127770	12.706624
13.588831	715.844119	12.711642
13.676344	712.475741	12.716659
13.447320	720.603126	12.721677
13.595201	713.804378	12.726695
13.764483	723.819656	12.731712
13.790423	723.512605	12.736730
13.653634	710.203815	12.741747
13.667642	708.118751	12.746765
13.852977	710.387123	12.751783
13.716564	688.633314	12.756800
13.738385	690.154127	12.761818
13.541804	686.599891	12.766835
13.922639	687.824612	12.771853
13.830356	693.194467	12.776871
13.683807	686.583872	12.781888
13.422473	694.160883	12.786906
13.562058	694.126362	12.791923
13.209304	707.833681	12.796941
13.674468	709.843613	12.801959
13.768890	707.828001	12.806976
13.762910	708.112935	12.811994
13.872333	711.137975	12.817011
13.908801	709.005210	12.822029
13.803405	702.138851	12.827047
13.561741	710.760520	12.832064
13.842780	710.082139	12.837082
14.230857	707.720714	12.842099
13.610375	707.098377	12.847117
13.712891	707.271636	12.852135
13.850202	706.016169	12.857152
13.753528	715.467195	12.862170
14.108670	712.309350	12.867187
13.987861	725.585864	12.872205
13.842194	704.177470	12.877223
13.932563	708.130151	12.882240
13.734271	715.690982	12.887258
14.075708	700.839813	12.892275
13.967619	709.402683	12.897293
14.049920	714.107714	12.902311
13.812540	701.767750	12.907328
13.686451	721.331481	12.912346
14.564562	728.644772	12.917363
14.324669	731.156498	12.922381
14.332321	723.622318	12.927399
14.432438	708.720590	12.932416
14.220761	709.716253	12.937434
14.345109	705.969718	12.942451
13.825032	703.681155	12.947469
13.974427	715.223806	12.952487
14.270411	703.459839	12.957504
14.252459	703.756116	12.962522
13.781738	712.798684	12.967539
14.020432	716.469349	12.972557
13.932629	722.494922	12.977575
14.213403	726.834342	12.982592
14.346827	737.199231	12.987610
14.381584	729.515634	12.992627
14.569275	731.133540	12.997645
14.445975	730.373342	13.002663
14.422086	725.450816	13.007680
14.165285	733.576247	13.012698
14.400691	731.857281	13.017715
14.373208	728.566879	13.022733
14.154301	734.833904	13.027751
14.479799	727.076353	13.032768
14.792503	728.027727	13.037786
14.813304	722.615359	13.042803
14.812392	726.225737	13.047821
14.280247	722.856614	13.052839
14.565249	719.381552	13.057856
14.680055	719.335135	13.062874
14.114888	717.908863	13.067891
14.405483	724.187575	13.072909
14.356321	727.076518	13.077927
14.712834	727.803276	13.082944
14.595794	735.676436	13.087962
14.651463	728.690156	13.092979
14.542728	742.390826	13.097997
14.270264	736.541560	13.103015
14.615089	728.591631	13.108032
14.355273	739.968037	13.113050
14.725787	734.699688	13.118067
14.638444	734.034843	13.123085
14.751678	734.780784	13.128103
14.528600	732.723396	13.133120
14.682544	734.741068	13.138138
14.624181	736.801472	13.143155
14.611431	733.530850	13.148173
14.464862	725.465408	13.153191
14.747971	728.340161	13.158208
14.435713	738.617089	13.163226
14.239683	727.977929	13.168243
14.328441	735.152965	13.173261
14.822370	746.303981	13.178279
14.873865	748.091551	13.183296
14.748068	762.583867	13.188314
14.847072	753.968691	13.193331
14.701153	749.516561	13.198349
14.688462	756.171009	13.203367
15.027349	750.910767	13.208384
14.861812	764.967496	13.213402
15.166513	757.781239	13.218419
15.147057	754.890364	13.223437
15.391595	758.840991	13.228455
15.162453	746.259862	13.233472
14.842464	748.279207	13.238490
14.942338	737.925041	13.243507
15.083698	746.521429	13.248525
15.044939	745.056859	13.253543
15.032626	746.469416	13.258560
14.993774	752.455770	13.263578
15.435851	749.363194	13.268595
15.053264	743.458596	13.273613
15.081091	731.256940	13.278631
15.215955	726.565162	13.283648
14.934926	733.782356	13.288666
15.116314	743.735788	13.293683
15.208663	748.003749	13.298701
15.215132	743.688692	13.303719
15.102159	748.556872	13.308736
15.356045	754.752984	13.313754
15.262766	747.584905	13.318771
15.047425	734.537715	13.323789
15.163305	743.027640	13.328807
15.498013	738.433935	13.333824
15.535052	744.348436	13.338842
15.144161	741.588344	13.343859
15.242422	726.339750	13.348877
15.213311	735.707617	13.353895
15.367279	740.029039	13.358912
15.256071	749.059479	13.363930
15.072668	750.344207	13.368947
15.204296	743.576396	13.373965
15.351104	747.046867	13.378983
15.494548	741.646835	13.384000
15.220676	748.440033	13.389018
15.526315	741.300974	13.394035
15.704923	741.856790	13.399053
15.518514	757.485229	13.404071
15.499315	748.522499	13.409088
15.596665	747.491043	13.414106
15.454279	754.560289	13.419123
15.597051	747.727614	13.424141
15.540407	757.674167	13.429159
15.078564	746.817866	13.434176
15.599844	748.569700	13.439194
15.123837	751.083709	13.444211
15.570381	748.460652	13.449229
15.489426	758.950661	13.454247
15.718727	748.932819	13.459264
15.284393	753.144446	13.464282
15.031559	746.493677	13.469299
15.260369	753.482673	13.474317
15.344248	764.647454	13.479335
15.604522	773.881637	13.484352
15.838875	775.340755	13.489370
15.843072	768.946354	13.494387
15.707010	766.146331	13.499405
15.533928	777.767950	13.504423
15.493867	772.283050	13.509440
15.442605	773.174688	13.514458
15.632580	774.072710	13.519475
15.976742	763.822267	13.524493
15.728856	773.555793	13.529511
15.774085	765.441347	13.534528
15.697221	770.527940	13.539546
15.701128	773.900885	13.544563
15.866223	771.782674	13.549581
16.026295	765.392253	13.554599
15.944397	771.786150	13.559616
15.778169	774.829143	13.564634
15.734497	779.557084	13.569651
16.217383	771.989451	13.574669
15.907705	776.673862	13.579687
16.345580	780.922409	13.584704
15.837883	779.932099	13.589722
15.724180	766.815312	13.594739
15.966184	779.681566	13.599757
16.284531	786.874300	13.604775
16.336292	781.507556	13.609792
15.989547	772.504615	13.614810
15.935954	784.467282	13.619827
16.271144	788.955983	13.624845
16.147725	789.928355	13.629863
16.582613	779.427001	13.634880
16.180825	774.737240	13.639898
16.075364	777.401480	13.644915
16.318881	772.500160	13.649933
15.624234	774.253159	13.654951
16.041461	775.566859	13.659968
16.404863	786.239729	13.664986
16.414502	789.902116	13.670003
16.447535	791.648402	13.675021
15.868497	801.714698	13.680039
16.612885	797.003141	13.685056
16.248995	801.774948	13.690074
16.407388	793.402916	13.695091
16.622699	795.341551	13.700109
16.297375	795.417742	13.705127
16.338830	790.791075	13.710144
16.160850	795.969258	13.715162
16.505645	793.643006	13.720179
16.488216	791.398754	13.725197
16.271875	794.238161	13.730215
16.482359	801.769696	13.735232
16.478204	794.344636	13.740250
16.734055	798.965692	13.745267
16.696599	790.406594	13.750285
16.259198	795.404514	13.755303
16.524438	797.272210	13.760320
16.824866	793.081498	13.765338
16.442114	798.610505	13.770355
16.541880	784.841714	13.775373
16.516183	810.669926	13.780391
16.394188	788.923203	13.785408
16.824309	795.861740	13.790426
16.730873	799.047968	13.795443
17.058923	796.023744	13.800461
16.653186	799.445097	13.805479
16.903276	793.580211	13.810496
16.891907	790.539739	13.815514
16.604891	792.847416	13.820531
16.994394	796.191509	13.825549
17.043477	794.684768	13.830567
16.832865	780.510170	13.835584
16.974437	769.669766	13.840602
16.336965	765.616543	13.845619
16.416253	775.494470	13.850637
17.113379	792.234218	13.855655
16.668285	795.522880	13.860672
16.883167	798.960606	13.865690
16.821281	795.457828	13.870707
17.106492	794.349597	13.875725
17.056225	792.823709	13.880743
17.166673	788.246194	13.885760
17.271678	787.718469	13.890778
16.871874	792.947186	13.895795
16.779279	792.955355	13.900813
16.821915	790.026343	13.905831
16.931870	788.573183	13.910848
16.697314	786.602794	13.915866
16.664763	790.454830	13.920883
16.871653	789.365182	13.925901
16.717864	795.091846	13.930919
16.637832	784.077869	13.935936
16.772640	782.276829	13.940954
16.658879	803.463974	13.945971
17.171627	801.348094	13.950989
17.205416	820.599703	13.956007
17.107449	822.805179	13.961024
17.303143	810.132195	13.966042
16.843264	819.911585	13.971059
16.926064	816.143134	13.976077
17.307793	816.875413	13.981095
17.237593	815.684010	13.986112
17.511825	807.047665	13.991130
16.741396	811.637016	13.996147
17.234598	813.569984	14.001165
16.988289	815.019208	14.006183
17.338647	825.287042	14.011200
17.261149	831.427803	14.016218
17.690753	834.702503	14.021235
17.511946	827.857065	14.026253
17.771712	822.514524	14.031271
17.196257	812.799462	14.036288
17.713828	808.947114	14.041306
17.603019	821.663548	14.046323
17.518117	818.464177	14.051341
17.559844	813.720696	14.056359
17.486927	817.749478	14.061376
17.884798	806.714258	14.066394
17.402719	809.393329	14.071411
17.685958	807.531161	14.076429
17.972315	804.349364	14.081447
17.725428	803.961981	14.086464
18.122711	798.162394	14.091482
17.648877	807.000369	14.096499
17.992859	807.801678	14.101517
17.604385	802.333488	14.106535
17.652800	807.933800	14.111552
17.880206	813.035849	14.116570
17.700789	813.606737	14.121587
17.631749	804.752775	14.126605
17.690574	806.839007	14.131623
17.453325	800.637060	14.136640
17.590602	808.429379	14.141658
17.504219	807.338343	14.146675
17.552872	804.982749	14.151693
17.613564	806.541664	14.156711
17.652962	815.857813	14.161728
17.952874	824.454643	14.166746
17.999406	826.555428	14.171763
18.177345	822.469108	14.176781
18.110929	813.068771	14.181799
17.712454	812.004541	14.186816
17.986492	816.578571	14.191834
17.919041	820.145745	14.196851
17.962782	815.648103	14.201869
17.828275	823.836466	14.206887
17.704070	831.720258	14.211904
18.093465	824.817354	14.216922
18.080240	837.240796	14.221939
18.079637	835.959590	14.226957
17.805824	840.704671	14.231975
18.046382	838.947018	14.236992
18.397405	835.281707	14.242010
18.376353	841.565108	14.247027
18.406550	834.027350	14.252045
18.568522	830.893439	14.257063
18.295665	834.792603	14.262080
18.415536	838.081118	14.267098
18.442543	824.102788	14.272115
18.185467	810.329925	14.277133
18.082772	810.664728	14.282151
17.936200	824.393480	14.287168
18.454021	825.599904	14.292186
18.407705	832.837169	14.297203
18.283813	833.257345	14.302221
18.297146	824.403090	14.307239
18.088399	831.069349	14.312256
18.764411	825.090382	14.317274
18.494413	826.262449	14.322291
18.407505	823.016054	14.327309
18.558382	821.130441	14.332327
18.680932	833.592568	14.337344
18.253074	826.546308	14.342362
18.706358	832.894244	14.347379
18.584138	824.414682	14.352397
18.437042	818.678292	14.357415
18.263273	829.747780	14.362432
18.555482	824.905090	14.367450
18.408515	831.517488	14.372467
18.412631	829.986232	14.377485
18.552296	824.242780	14.382503
18.916965	824.700018	14.387520
18.953429	827.919548	14.392538
18.648707	828.664706	14.397555
18.796998	828.319548	14.402573
18.743605	824.070655	14.407591
18.721537	823.837397	14.412608
18.640075	829.997714	14.417626
18.759109	827.268168	14.422643
18.496325	831.105791	14.427661
18.381427	836.614933	14.432679
18.275785	829.382486	14.437696
18.465400	839.981631	14.442714
18.695162	850.416699	14.447731
18.542236	854.628440	14.452749
18.682999	850.323874	14.457767
18.627896	859.534930	14.462784
19.169163	842.702021	14.467802
18.832142	849.710281	14.472819
18.664630	859.803651	14.477837
19.033665	854.093681	14.482855
18.845075	858.478271	14.487872
18.470427	847.791285	14.492890
19.079689	853.944374	14.497907
18.807423	871.618731	14.502925
19.258840	874.224136	14.507943
19.024295	879.278660	14.512960
19.361896	875.536548	14.517978
19.157454	866.539666	14.522995
19.692909	878.425883	14.528013
19.338937	858.223918	14.533031
19.160482	859.432138	14.538048
19.356268	854.699222	14.543066
19.296817	853.162145	14.548083
19.067871	839.750931	14.553101
19.081321	841.774848	14.558119
19.382804	858.131673	14.563136
19.619097	856.362063	14.568154
19.530992	853.156876	14.573171
19.257191	844.625314	14.578189
19.406404	845.643337	14.583207
19.275231	848.444161	14.588224
18.946255	832.523949	14.593242
19.610442	855.331292	14.598259
19.351541	871.274150	14.603277
19.608897	867.976963	14.608295
19.712529	872.760746	14.613312
19.688723	864.893760	14.618330
19.505060	858.355189	14.623347
19.246398	858.433558	14.628365
19.819058	857.239260	14.633383
19.590353	868.345782	14.638400
19.520529	862.127049	14.643418
19.667649	866.263380	14.648435
19.493775	860.445963	14.653453
19.539771	869.174119	14.658471
19.458581	873.292573	14.663488
19.709838	870.870512	14.668506
19.596130	866.732046	14.673523
19.239359	867.725204	14.678541
19.721315	871.865880	14.683559
19.556068	867.385190	14.688576
19.843073	869.536666	14.693594
19.979562	866.514040	14.698611
19.809560	870.046797	14.703629
19.383415	866.834611	14.708647
19.629286	873.473838	14.713664
19.764451	863.271863	14.718682
19.764261	863.300268	14.723699
19.807406	882.859752	14.728717
20.357314	884.222102	14.733735
19.925497	878.034833	14.738752
19.834579	871.481726	14.743770
19.965097	877.624625	14.748787
20.408149	887.776984	14.753805
19.884497	873.802839	14.758823
19.712388	878.771840	14.763840
20.211821	884.071133	14.768858
20.220151	890.993742	14.773875
20.186018	891.813272	14.778893
20.331317	884.206965	14.783911
20.161486	885.259199	14.788928
20.159713	880.121722	14.793946
20.418382	879.970712	14.798963
20.137393	874.059619	14.803981
20.272377	880.031403	14.808999
19.922844	882.358353	14.814016
19.753827	877.512173	14.819034
20.474625	885.822179	14.824051
20.254348	893.960896	14.829069
20.641659	883.757273	14.834087
20.271675	885.743440	14.839104
20.322403	895.906780	14.844122
20.449592	887.981412	14.849139
20.393217	888.198503	14.854157
20.514145	889.801637	14.859175
20.700457	898.678239	14.864192
20.290633	892.522234	14.869210
20.499474	883.476369	14.874227
20.299047	891.233272	14.879245
20.578105	882.356290	14.884263
20.507105	884.472341	14.889280
20.627861	888.344559	14.894298
20.817704	888.661931	14.899315
20.426687	897.884612	14.904333
20.281177	887.903326	14.909351
20.817621	886.067751	14.914368
20.447237	889.067010	14.919386
20.832538	890.363631	14.924403
20.507405	894.744376	14.929421
20.747070	890.506357	14.934439
20.669900	893.210363	14.939456
20.472164	895.582961	14.944474
20.580306	896.263433	14.949491
20.166492	892.746348	14.954509
20.587278	898.714385	14.959527
20.866467	915.645965	14.964544
20.738442	913.857690	14.969562
21.084134	917.019319	14.974579
20.956477	920.690621	14.979597
20.988195	907.762388	14.984615
21.029017	917.223536	14.989632
20.921102	923.507951	14.994650
20.927902	916.608152	14.999667
21.170124	907.471837	15.004685
21.171323	916.689880	15.009703
21.096199	911.027392	15.014720
21.408962	916.368565	15.019738
21.064077	904.480812	15.024755
21.141388	917.249892	15.029773
21.317496	904.226453	15.034791
21.236765	894.818848	15.039808
21.034752	889.933652	15.044826
21.112275	893.730593	15.049843
21.378286	901.761563	15.054861
21.362381	902.022808	15.059879
21.475654	904.195197	15.064896
21.232794	897.665886	15.069914
21.381655	883.580053	15.074931
21.456414	888.630299	15.079949
21.343107	877.492088	15.084967
21.287601	879.176514	15.089984
21.071491	884.108229	15.095002
21.174686	898.100866	15.100019
21.172603	899.994678	15.105037
21.131812	907.291068	15.110055
21.151009	907.010317	15.115072
21.064265	908.560783	15.120090
21.551957	899.313428	15.125107
21.441321	905.055456	15.130125
21.249017	914.300660	15.135143
21.367520	905.799123	15.140160
21.358832	911.285335	15.145178
21.828757	921.547115	15.150195
21.783683	923.308807	15.155213
21.726646	920.146078	15.160231
21.454861	904.156880	15.165248
21.454161	919.522830	15.170266
21.900651	923.662762	15.175283
21.780532	936.191385	15.180301
22.029939	929.139958	15.185319
21.794128	927.529519	15.190336
21.611168	924.923014	15.195354
21.964466	918.218238	15.200371
21.774220	928.473002	15.205389
21.771464	924.661128	15.210407
22.093719	931.108525	15.215424
21.541265	936.477967	15.220442
22.009460	931.610830	15.225459
21.933835	936.564730	15.230477
22.120668	936.494403	15.235495
22.408237	931.541956	15.240512
22.421992	930.820237	15.245530
22.282204	904.478073	15.250547
21.772194	906.584013	15.255565
21.802574	901.886468	15.260583
22.073795	907.833760	15.265600
22.189229	912.735628	15.270618
22.348526	902.138523	15.275635
21.766825	900.613838	15.280653
22.093982	915.420324	15.285671
22.185399	922.626577	15.290688
21.823480	929.632458	15.295706
22.126723	921.966674	15.300723
22.074238	925.727186	15.305741
22.309127	928.909333	15.310759
22.090238	920.378599	15.315776
22.239786	923.722442	15.320794
22.429606	926.652870	15.325811
22.237304	934.395895	15.330829
22.325391	924.971291	15.335847
22.484807	931.229603	15.340864
22.555352	933.386599	15.345882
22.356112	923.164399	15.350899
22.091141	927.308505	15.355917
22.077255	926.736286	15.360935
22.489786	934.264624	15.365952
22.433567	946.347733	15.370970
22.749665	945.667008	15.375987
22.762706	949.578207	15.381005
22.490188	951.930970	15.386023
22.853162	950.024736	15.391040
22.511450	951.444737	15.396058
22.820031	951.052372	15.401075
23.035315	950.709339	15.406093
22.910801	935.486004	15.411111
22.619608	926.897166	15.416128
22.478188	937.153753	15.421146
22.823922	945.579358	15.426163
22.683374	950.884267	15.431181
22.904814	947.204522	15.436199
22.856049	942.456249	15.441216
22.586641	954.402350	15.446234
22.981887	951.629508	15.451251
22.938265	954.757465	15.456269
22.954908	947.404823	15.461287
22.643348	948.779073	15.466304
22.677510	949.553191	15.471322
22.989321	957.018423	15.476339
22.853731	953.691267	15.481357
22.846079	952.404846	15.486375
23.153103	952.135804	15.491392
22.869806	963.225691	15.496410
22.946987	950.615358	15.501427
23.146826	962.569995	15.506445
23.125408	970.866941	15.511463
23.489607	978.904653	15.516480
23.077878	965.648217	15.521498
23.470390	962.361396	15.526515
23.516752	954.975691	15.531533
23.243123	948.223960	15.536551
23.595872	943.049855	15.541568
23.001803	953.004979	15.546586
23.506884	946.812908	15.551603
23.048644	953.070170	15.556621
23.139836	949.619119	15.561639
23.457095	960.933652	15.566656
23.568403	966.183326	15.571674
23.233889	962.180422	15.576691
23.498054	964.720504	15.581709
23.358087	971.000490	15.586727
23.296359	957.989030	15.591744
23.537952	964.433298	15.596762
23.585509	968.547381	15.601779
23.251520	968.621774	15.606797
23.417074	974.999063	15.611815
23.742612	973.818230	15.616832
23.576422	971.856044	15.621850
23.563295	963.356168	15.626867
23.992279	967.473607	15.631885
23.213096	971.354299	15.636903
23.632340	965.248255	15.641920
23.352800	973.951726	15.646938
23.665231	977.402605	15.651955
23.948359	991.594346	15.656973
24.236180	992.767390	15.661991
24.353727	980.838691	15.667008
23.778451	985.896136	15.672026
24.248402	968.553564	15.677043
24.048908	968.881444	15.682061
23.720213	966.913161	15.687079
23.896642	961.157594	15.692096
24.042561	961.933138	15.697114
23.865365	955.699636	15.702131
24.148454	966.337861	15.707149
24.100129	973.102117	15.712167
24.300798	969.725429	15.717184
24.135512	971.938315	15.722202
24.148302	968.231295	15.727219
24.315270	971.569262	15.732237
23.994791	977.956430	15.737255
24.374478	979.383328	15.742272
24.472789	986.266628	15.747290
24.029139	974.025066	15.752307
24.368142	974.764046	15.757325
24.294880	983.536190	15.762343
25.023952	986.019213	15.767360
24.235287	976.375337	15.772378
24.479060	970.126368	15.777395
24.559298	965.932245	15.782413
24.463916	958.900113	15.787431
24.309189	948.970731	15.792448
24.655748	964.512690	15.797466
24.590527	971.522595	15.802483
24.270298	957.961488	15.807501
24.353470	982.516857	15.812519
24.896989	981.298715	15.817536
24.726804	988.179901	15.822554
24.659031	988.752237	15.827571
24.831476	980.068640	15.832589
24.664075	973.476985	15.837607
24.787305	970.696265	15.842624
24.766126	965.479752	15.847642
24.521506	966.950815	15.852659
25.115760	975.378523	15.857677
24.532822	976.738489	15.862695
24.596919	983.671331	15.867712
24.662844	989.726557	15.872730
24.734474	987.790226	15.877747
24.860622	983.020849	15.882765
24.849642	986.254153	15.887783
24.828583	984.856218	15.892800
24.966696	985.431011	15.897818
24.843010	982.225063	15.902835
24.950115	975.154888	15.907853
25.108155	987.804071	15.912871
25.077189	978.013075	15.917888
25.160137	983.358718	15.922906
25.173111	985.480558	15.927923
25.165536	980.192480	15.932941
24.847194	984.654236	15.937959
24.832981	985.805172	15.942976
24.928049	981.652904	15.947994
24.634184	988.231570	15.953011
25.122551	1009.921078	15.958029
25.321675	1009.208183	15.963047
25.444174	1006.396014	15.968064
25.391885	1010.831871	15.973082
25.171283	1012.343357	15.978099
25.301902	1005.897504	15.983117
25.394889	1012.961534	15.988135
25.532461	1006.498812	15.993152
25.687722	1006.969930	15.998170
25.523699	1019.047888	16.003187
25.700550	1007.965122	16.008205
25.425424	1020.227749	16.013223
25.275619	1006.434772	16.018240
25.491240	1007.347724	16.023258
25.466404	1008.374091	16.028275
25.660060	1006.633238	16.033293
25.153862	1002.379507	16.038311
25.531692	1000.900138	16.043328
25.618842	1010.663353	16.048346
25.348151	1008.714381	16.053363
25.739626	1022.895483	16.058381
25.860324	1035.010895	16.063399
25.920381	1021.390158	16.068416
26.045405	1032.974703	16.073434
25.927620	1032.923701	16.078451
26.095153	1017.824955	16.083469
25.888611	1015.790190	16.088487
25.996665	1021.782021	16.093504
26.123141	1023.409545	16.098522
25.785255	1007.335933	16.103539
26.231709	1007.294359	16.108557
26.275553	1002.380079	16.113575
26.259692	999.135143	16.118592
26.288479	1009.803770	16.123610
25.902143	998.531531	16.128627
25.964660	993.879421	16.133645
26.017188	1003.010570	16.138663
26.247939	1006.572085	16.143680
26.301947	1023.854637	16.148698
25.971941	1023.218333	16.153715
26.440003	1024.195877	16.158733
26.483686	1022.809887	16.163751
26.219348	1014.989989	16.168768
26.470778	1014.376198	16.173786
26.456940	1019.263635	16.178803
26.727722	1015.632951	16.183821
26.582126	1017.138996	16.188839
26.327501	1006.988543	16.193856
26.239224	1010.745214	16.198874
26.246692	1020.887000	16.203891
26.359885	1011.044997	16.208909
26.346585	1014.644751	16.213927
26.560086	1013.601393	16.218944
26.621519	1015.819788	16.223962
26.292096	1023.205630	16.228979
26.538922	1016.627955	16.233997
26.020520	1012.417160	16.239015
26.435330	1014.122586	16.244032
26.828716	1019.359639	16.249050
26.926255	1024.371641	16.254067
26.828092	1014.351307	16.259085
26.772314	1022.129785	16.264103
27.075737	1020.529527	16.269120
27.123615	1014.386975	16.274138
26.838959	1009.378992	16.279155
26.997310	1013.500973	16.284173
26.478152	1020.843957	16.289191
26.766669	1014.436480	16.294208
26.984967	1023.459614	16.299226
27.219059	1047.480174	16.304243
27.138743	1038.305963	16.309261
27.159574	1040.312967	16.314279
27.215819	1043.507346	16.319296
27.129386	1039.086849	16.324314
26.857373	1042.556726	16.329331
27.018091	1032.328560	16.334349
27.214780	1035.422035	16.339367
27.533820	1032.291883	16.344384
27.613305	1030.673060	16.349402
27.187461	1038.149757	16.354419
27.470894	1032.083905	16.359437
27.635359	1042.570343	16.364455
27.496726	1031.644291	16.369472
26.897886	1016.072316	16.374490
27.062260	1023.320829	16.379507
27.029555	1029.189546	16.384525
27.069231	1035.602359	16.389543
27.215917	1037.627515	16.394560
27.211798	1039.531128	16.399578
27.154234	1035.497438	16.404595
27.469856	1043.476517	16.409613
27.749242	1048.709349	16.414631
27.227601	1057.595962	16.419648
27.793981	1052.341016	16.424666
27.423106	1054.586123	16.429683
27.595845	1047.243697	16.434701
27.765054	1068.756059	16.439719
27.534209	1063.610238	16.444736
27.852471	1054.985811	16.449754
27.679396	1062.299835	16.454771
27.380226	1047.640269	16.459789
27.768804	1059.931483	16.464807
27.666011	1052.332416	16.469824
27.869174	1063.633333	16.474842
27.970265	1071.586075	16.479859
28.221859	1068.299223	16.484877
28.217830	1078.143034	16.489895
28.066338	1071.138584	16.494912
28.312660	1059.590454	16.499930
28.323391	1062.564743	16.504947
28.188601	1046.730681	16.509965
27.961332	1052.169131	16.514983
27.747741	1065.081727	16.520000
28.174622	1068.937581	16.525018
28.130225	1077.673689	16.530035
28.425075	1070.144860	16.535053
28.761536	1082.608361	16.540071
28.232001	1071.803493	16.545088
28.557628	1065.974021	16.550106
28.317297	1070.821217	16.555123
28.425310	1071.555367	16.560141
28.180244	1070.703776	16.565159
28.281763	1073.313540	16.570176
28.690888	1079.131983	16.575194
28.765222	1070.722497	16.580211
28.655010	1081.592829	16.585229
28.583603	1074.686287	16.590247
28.528701	1070.456507	16.595264
28.540027	1068.823113	16.600282
28.465104	1069.803681	16.605299
28.646807	1061.415247	16.610317
28.587305	1065.315747	16.615335
28.199754	1065.865602	16.620352
28.778326	1064.654586	16.625370
28.388789	1065.327832	16.630387
28.481304	1062.867500	16.635405
28.645912	1070.718769	16.640423
28.253674	1072.307646	16.645440
28.984147	1088.259789	16.650458
28.484340	1095.353611	16.655475
28.941980	1097.099674	16.660493
28.982799	1090.759382	16.665511
28.598470	1085.931099	16.670528
29.114499	1083.729465	16.675546
28.938054	1093.720222	16.680563
28.807036	1090.215594	16.685581
29.361721	1082.930079	16.690599
28.906966	1093.302121	16.695616
29.123244	1080.300664	16.700634
29.045063	1094.634306	16.705651
29.006411	1096.795807	16.710669
29.337169	1112.974705	16.715687
29.338286	1111.245074	16.720704
29.705745	1105.093446	16.725722
29.622176	1106.911682	16.730739
29.303021	1101.871207	16.735757
29.576084	1097.104029	16.740775
29.463498	1092.419366	16.745792
29.688772	1085.788236	16.750810
29.533643	1090.757791	16.755827
29.452101	1082.322227	16.760845
29.598170	1096.911078	16.765863
29.818339	1094.932527	16.770880
29.684708	1083.402885	16.775898
29.605721	1087.808229	16.780915
29.938988	1091.277957	16.785933
29.918632	1077.149054	16.790951
29.296746	1079.231516	16.795968
29.857240	1093.667067	16.800986
30.072140	1107.784383	16.806003
29.784290	1096.761746	16.811021
30.055823	1092.064239	16.816039
29.776955	1082.308871	16.821056
30.200518	1080.200622	16.826074
29.779637	1080.304408	16.831091
29.620392	1088.162243	16.836109
30.011867	1100.866453	16.841127
30.051159	1107.623344	16.846144
30.511283	1107.188298	16.851162
30.249448	1112.300813	16.856179
30.187547	1115.870331	16.861197
30.397503	1106.540149	16.866215
30.256346	1096.599091	16.871232
30.050366	1085.096563	16.876250
29.867388	1087.851891	16.881267
30.192861	1097.508384	16.886285
30.259521	1108.079614	16.891303
30.228034	1105.313648	16.896320
30.495241	1103.927345	16.901338
30.429610	1110.896342	16.906355
30.517096	1107.597323	16.911373
30.328174	1108.349595	16.916391
30.119329	1114.757192	16.921408
30.370338	1100.251229	16.926426
30.540315	1118.096386	16.931443
30.298411	1100.871531	16.936461
30.494683	1101.386721	16.941479
30.593148	1106.900387	16.946496
30.759946	1104.179095	16.951514
30.319547	1102.714305	16.956531
30.302261	1098.043112	16.961549
30.562286	1113.371536	16.966567
30.573902	1123.979803	16.971584
30.821033	1120.864058	16.976602
30.627293	1126.549749	16.981619
30.583536	1130.586656	16.986637
30.981429	1125.118238	16.991655
30.811209	1142.316113	16.996672
30.593320	1130.054850	17.001690
30.722090	1135.008339	17.006707
30.606681	1130.197873	17.011725
30.796339	1123.641739	17.016743
30.841739	1145.107318	17.021760
31.464293	1152.965771	17.026778
31.542143	1147.354981	17.031795
31.417691	1145.673423	17.036813
31.323361	1130.546181	17.041831
31.347443	1130.539224	17.046848
31.070648	1126.038075	17.051866
31.190261	1126.868243	17.056883
31.025111	1141.190301	17.061901
31.608849	1147.186542	17.066919
31.421306	1154.581768	17.071936
31.558928	1151.233860	17.076954
31.795234	1143.057746	17.081971
31.504498	1135.450219	17.086989
31.548821	1130.008794	17.092007
31.394464	1126.593025	17.097024
31.244241	1129.226460	17.102042
31.597297	1144.622387	17.107059
31.623622	1147.610027	17.112077
31.789983	1141.704496	17.117095
31.611077	1152.980122	17.122112
31.454309	1150.325298	17.127130
31.599219	1146.506020	17.132147
31.498220	1157.539063	17.137165
31.739982	1148.494219	17.142183
31.577279	1152.152123	17.147200
31.709961	1143.297947	17.152218
31.820592	1147.989186	17.157235
31.730066	1150.256654	17.162253
31.959847	1149.359064	17.167271
31.994814	1158.142740	17.172288
32.122886	1165.990308	17.177306
32.011958	1162.047004	17.182323
32.183838	1175.233810	17.187341
32.385920	1162.209271	17.192359
31.913791	1175.474888	17.197376
32.217039	1172.104182	17.202394
32.132547	1175.336414	17.207411
32.022385	1165.589283	17.212429
32.151900	1165.420636	17.217447
32.231915	1167.875988	17.222464
32.240195	1167.205612	17.227482
32.424009	1162.938408	17.232499
32.094653	1170.169661	17.237517
32.634562	1162.539280	17.242535
32.396805	1169.923444	17.247552
32.466048	1167.637162	17.252570
32.460682	1168.616305	17.257587
32.326259	1157.597995	17.262605
32.626697	1174.166720	17.267623
32.339317	1162.623244	17.272640
32.423290	1163.572610	17.277658
32.589992	1172.158922	17.282675
32.504866	1191.618917	17.287693
33.147509	1181.747518	17.292711
32.892294	1193.060372	17.297728
33.150011	1187.367738	17.302746
33.104966	1176.884541	17.307763
32.496596	1167.941325	17.312781
33.149981	1172.272970	17.317799
32.890486	1184.880410	17.322816
33.303042	1176.380011	17.327834
33.076158	1157.742058	17.332851
33.019029	1157.107177	17.337869
32.908959	1164.269356	17.342887
32.977921	1172.164059	17.347904
32.978472	1174.770721	17.352922
33.455105	1177.659410	17.357939
33.148495	1178.502709	17.362957
33.377581	1184.557685	17.367975
33.302616	1186.257813	17.372992
33.173208	1184.441324	17.378010
33.194907	1188.774111	17.383027
33.220950	1190.404762	17.388045
33.693171	1184.167264	17.393063
33.201304	1191.597562	17.398080
33.631700	1185.243537	17.403098
33.987587	1177.036048	17.408115
33.490838	1188.033281	17.413133
33.358350	1178.485307	17.418151
33.669076	1177.900092	17.423168
33.544017	1184.480785	17.428186
33.807062	1175.827080	17.433203
33.661386	1191.373775	17.438221
33.619442	1182.594277	17.443239
33.404504	1185.367251	17.448256
33.535913	1179.489276	17.453274
33.723472	1176.281866	17.458291
33.397974	1192.674115	17.463309
34.227422	1188.725485	17.468327
34.162574	1201.820009	17.473344
34.224357	1210.182928	17.478362
33.830288	1207.076109	17.483379
33.709043	1211.156734	17.488397
33.859045	1207.415543	17.493415
34.139456	1214.677513	17.498432
34.037739	1206.841518	17.503450
34.329020	1203.690439	17.508467
34.002463	1208.737380	17.513485
34.119014	1201.589893	17.518503
34.342382	1206.260329	17.523520
34.129247	1201.578767	17.528538
33.665355	1195.582611	17.533555
33.903726	1207.430387	17.538573
34.368303	1217.980364	17.543591
34.519150	1225.158493	17.548608
34.111543	1225.619974	17.553626
34.728247	1218.059591	17.558643
34.166054	1231.721226	17.563661
34.220770	1225.580687	17.568679
34.609463	1230.619715	17.573696
34.759113	1221.172686	17.578714
35.044258	1223.242443	17.583731
34.848579	1219.549099	17.588749
34.767742	1213.546570	17.593767
35.002642	1207.336779	17.598784
35.298637	1216.985332	17.603802
35.078942	1203.837490	17.608819
34.959663	1215.097502	17.613837
34.853123	1213.914921	17.618855
34.767357	1210.933372	17.623872
34.639892	1224.460615	17.628890
35.092680	1210.724551	17.633907
34.631103	1216.550067	17.638925
34.805030	1211.757364	17.643943
34.880655	1218.294003	17.648960
34.776249	1209.637891	17.653978
35.147757	1219.558646	17.658995
35.071430	1235.309115	17.664013
35.099903	1238.488944	17.669031
35.336413	1237.180027	17.674048
35.523075	1237.905018	17.679066
35.693059	1231.812691	17.684083
35.564313	1242.559789	17.689101
36.010134	1236.992307	17.694119
35.510745	1223.553745	17.699136
35.221757	1225.688210	17.704154
35.836469	1221.905765	17.709171
35.628595	1234.479906	17.714189
35.566226	1232.356252	17.719207
36.004525	1227.515812	17.724224
35.904482	1217.612427	17.729242
36.019512	1209.663574	17.734259
35.337343	1213.667976	17.739277
35.700226	1211.351462	17.744295
35.863581	1220.225509	17.749312
36.015185	1230.805595	17.754330
35.921754	1217.293965	17.759347
35.815126	1230.177299	17.764365
35.793081	1225.620431	17.769383
35.958924	1225.247269	17.774400
36.007713	1234.382278	17.779418
35.864500	1231.962012	17.784435
35.960495	1229.602100	17.789453
35.824951	1224.024720	17.794471
35.840248	1225.136333	17.799488
35.983342	1227.733294	17.804506
36.058348	1224.824387	17.809523
36.310759	1248.343714	17.814541
36.139774	1250.181972	17.819559
36.485343	1251.080889	17.824576
36.354319	1258.047565	17.829594
36.529423	1248.555506	17.834611
36.228520	1254.213844	17.839629
36.102916	1242.648126	17.844647
36.280756	1249.266594	17.849664
36.714172	1253.127777	17.854682
36.337600	1256.686663	17.859699
36.588578	1255.722629	17.864717
36.715216	1256.611664	17.869735
36.608867	1256.328487	17.874752
36.666554	1247.239848	17.879770
36.797144	1254.544243	17.884787
36.492231	1245.572378	17.889805
37.053587	1267.089814	17.894823
36.992721	1269.652462	17.899840
36.815705	1272.223841	17.904858
36.786380	1277.953249	17.909875
36.503771	1276.088168	17.914893
36.801949	1264.919959	17.919911
37.010621	1269.927241	17.924928
37.018879	1274.429419	17.929946
37.034118	1268.604330	17.934963
36.965043	1275.192064	17.939981
36.958659	1272.863967	17.944999
37.176497	1271.718925	17.950016
37.253141	1271.517534	17.955034
37.287786	1264.064107	17.960051
37.221640	1279.753058	17.965069
37.136825	1294.311970	17.970087
37.739338	1294.851883	17.975104
37.431922	1296.866162	17.980122
37.738329	1290.613580	17.985139
37.519427	1292.115354	17.990157
37.405774	1292.975765	17.995175
37.774625	1280.654029	18.000192
37.442164	1290.016064	18.005210
37.648225	1290.201510	18.010227
37.814809	1283.645777	18.015245
37.734126	1285.454111	18.020263
37.759056	1287.813964	18.025280
37.589287	1295.765062	18.030298
37.724624	1291.868355	18.035315
37.475541	1296.887402	18.040333
37.645302	1289.961926	18.045351
37.994721	1291.715497	18.050368
38.028773	1318.144175	18.055386
38.242919	1310.280738	18.060403
38.664341	1312.707866	18.065421
38.106856	1302.611007	18.070439
38.380718	1283.449481	18.075456
38.596349	1292.492106	18.080474
38.463774	1282.256098	18.085491
38.503936	1283.430094	18.090509
38.175336	1282.717817	18.095527
38.488342	1284.641201	18.100544
38.184896	1285.335680	18.105562
38.343868	1283.748564	18.110579
38.318646	1287.681612	18.115597
38.832055	1304.450629	18.120615
38.663834	1299.686262	18.125632
38.546941	1308.307605	18.130650
38.685169	1312.091969	18.135667
38.893421	1316.446053	18.140685
38.835829	1312.033594	18.145703
39.158428	1295.625856	18.150720
38.919506	1288.868557	18.155738
38.484933	1288.750417	18.160755
38.840386	1304.082989	18.165773
38.710021	1311.437762	18.170791
39.011415	1301.111659	18.175808
38.875196	1318.465327	18.180826
39.093230	1307.315961	18.185843
38.929759	1313.779638	18.190861
38.636876	1309.375640	18.195879
39.029985	1311.371686	18.200896
39.022732	1313.345250	18.205914
39.061870	1303.745072	18.210931
38.933395	1306.892697	18.215949
39.070319	1323.543986	18.220967
39.518148	1313.763001	18.225984
39.756525	1337.581302	18.231002
39.626594	1322.270119	18.236019
39.359257	1312.717953	18.241037
39.175614	1309.732788	18.246055
39.144611	1320.527737	18.251072
38.999665	1339.946771	18.256090
39.504798	1334.164831	18.261107
39.634810	1334.721969	18.266125
39.671741	1336.587623	18.271143
39.520046	1335.099672	18.276160
39.483527	1329.358415	18.281178
39.446271	1327.442263	18.286195
39.362171	1340.356861	18.291213
39.542114	1345.766313	18.296231
39.957234	1350.116398	18.301248
39.735196	1355.109132	18.306266
40.081362	1353.757779	18.311283
40.269978	1353.150664	18.316301
40.169991	1358.730217	18.321319
40.476386	1351.657072	18.326336
40.011128	1352.421089	18.331354
40.344118	1348.575457	18.336371
40.592923	1350.256431	18.341389
40.455845	1342.397514	18.346407
40.427651	1344.582654	18.351424
40.447727	1348.530710	18.356442
40.395692	1353.304297	18.361459
40.703268	1344.937036	18.366477
40.543019	1348.802888	18.371495
40.563028	1339.634895	18.376512
40.345510	1343.705386	18.381530
40.561096	1339.164908	18.386547
40.307475	1341.713584	18.391565
40.457842	1355.629759	18.396583
40.592679	1343.546625	18.401600
40.396190	1342.103562	18.406618
40.485927	1344.570038	18.411635
40.557951	1343.138556	18.416653
40.362678	1357.427636	18.421671
41.190629	1357.389410	18.426688
40.834851	1367.856560	18.431706
40.925357	1379.683434	18.436723
41.012529	1371.678911	18.441741
40.865043	1377.584661	18.446759
41.016405	1358.309699	18.451776
41.452014	1369.987820	18.456794
41.109609	1368.665450	18.461811
41.291183	1363.764207	18.466829
41.198923	1370.986796	18.471847
41.215163	1365.937879	18.476864
40.924915	1373.352442	18.481882
41.162110	1368.764389	18.486899
41.584951	1376.913020	18.491917
41.602184	1388.470502	18.496935
41.719015	1382.910338	18.501952
41.237437	1378.696840	18.506970
41.082941	1380.885993	18.511987
41.857599	1375.885512	18.517005
41.590592	1387.250832	18.522023
41.897940	1387.249989	18.527040
41.898682	1392.040565	18.532058
41.536169	1377.292817	18.537075
41.816086	1380.010380	18.542093
41.627573	1388.257958	18.547111
41.947561	1391.187004	18.552128
41.976445	1375.595262	18.557146
41.789490	1385.426875	18.562163
41.919358	1390.550685	18.567181
41.895743	1394.688641	18.572199
41.867472	1401.513036	18.577216
42.499569	1408.950368	18.582234
42.191105	1412.618539	18.587251
42.397209	1404.178783	18.592269
42.132279	1400.704543	18.597287
42.581762	1399.810390	18.602304
42.475772	1402.007726	18.607322
42.556113	1406.170425	18.612339
42.286901	1405.275261	18.617357
42.542753	1408.896044	18.622375
42.634363	1399.069833	18.627392
42.361892	1404.051547	18.632410
42.321741	1411.556335	18.637427
42.151051	1402.961010	18.642445
42.254529	1404.446999	18.647463
42.610711	1399.101805	18.652480
42.472833	1406.946965	18.657498
42.957116	1419.586366	18.662515
43.198243	1416.114890	18.667533
42.901111	1426.392997	18.672551
43.024270	1422.283565	18.677568
42.925539	1423.425680	18.682586
42.966196	1428.525606	18.687603
43.233867	1424.324101	18.692621
42.983289	1430.397507	18.697639
43.169859	1427.688848	18.702656
43.371571	1417.779102	18.707674
43.372454	1418.653133	18.712691
43.566870	1416.710141	18.717709
43.087231	1419.723449	18.722727
43.148935	1417.564554	18.727744
43.531893	1423.210478	18.732762
43.382959	1427.093509	18.737779
43.478076	1421.366314	18.742797
43.298244	1425.497194	18.747815
43.599998	1425.150073	18.752832
43.482062	1420.036953	18.757850
43.210425	1419.927999	18.762867
43.642077	1431.407956	18.767885
43.549456	1447.685052	18.772903
43.593343	1450.385955	18.777920
43.641711	1451.391410	18.782938
43.645741	1452.810930	18.787955
43.529510	1449.202924	18.792973
44.007797	1450.118929	18.797991
43.790177	1453.318418	18.803008
43.833326	1465.616694	18.808026
43.830049	1475.880348	18.813043
44.421260	1476.201122	18.818061
44.447330	1471.153792	18.823079
44.675764	1475.974991	18.828096
44.637505	1478.840255	18.833114
44.774616	1474.823304	18.838131
44.938682	1458.784255	18.843149
44.220010	1450.034910	18.848167
44.362148	1447.077578	18.853184
44.390317	1454.928303	18.858202
44.739773	1468.387320	18.863219
44.815579	1459.182119	18.868237
44.623932	1475.828223	18.873255
44.791181	1471.588790	18.878272
44.493479	1471.247223	18.883290
44.439608	1461.740431	18.888307
44.762437	1456.432005	18.893325
44.890427	1464.033553	18.898343
44.578368	1463.555374	18.903360
44.767344	1459.031659	18.908378
44.768358	1466.482681	18.913395
44.919933	1464.312856	18.918413
45.206045	1475.380122	18.923431
45.247648	1491.841366	18.928448
45.206454	1482.837530	18.933466
44.971552	1488.113197	18.938483
45.169912	1494.741166	18.943501
45.354039	1492.436843	18.948519
45.172921	1487.595547	18.953536
45.607052	1487.928309	18.958554
45.515456	1495.741008	18.963571
45.552654	1493.655375	18.968589
45.353848	1492.989028	18.973607
45.340202	1493.644423	18.978624
45.784281	1492.034710	18.983642
45.926771	1488.588142	18.988659
45.696032	1492.588151	18.993677
45.906087	1493.139065	18.998695
46.115992	1487.150856	19.003712
45.941459	1484.524012	19.008730
45.790330	1489.161675	19.013747
45.554146	1484.603576	19.018765
45.769227	1490.916484	19.023783
45.702680	1486.884099	19.028800
45.770094	1478.008424	19.033818
45.398434	1509.963913	19.038835
45.870660	1506.557203	19.043853
45.992800	1502.564683	19.048871
45.982263	1507.473827	19.053888
45.950538	1513.939026	19.058906
46.277516	1522.778120	19.063923
46.139894	1521.985416	19.068941
46.492021	1533.528393	19.073959
46.626840	1532.601480	19.078976
46.579880	1532.138571	19.083994
46.337153	1523.996310	19.089011
46.715404	1530.734970	19.094029
46.664755	1522.688853	19.099047
46.709390	1525.178201	19.104064
46.404324	1523.531217	19.109082
46.381403	1536.111306	19.114099
46.822365	1529.840716	19.119117
47.153590	1536.813975	19.124135
46.941937	1546.665326	19.129152
47.171781	1546.749215	19.134170
47.194372	1554.430434	19.139187
47.209179	1542.631073	19.144205
47.317967	1540.982365	19.149223
47.136314	1545.968825	19.154240
47.606303	1535.931770	19.159258
47.169402	1536.580893	19.164275
47.276589	1541.339051	19.169293
47.346517	1545.815855	19.174311
47.441427	1545.422241	19.179328
47.702554	1545.346586	19.184346
47.676209	1551.309156	19.189363
47.684439	1553.520174	19.194381
48.098363	1544.697479	19.199399
47.498655	1555.733159	19.204416
47.776994	1543.245534	19.209434
47.834138	1548.712160	19.214451
47.806931	1552.554055	19.219469
47.884073	1549.228172	19.224487
47.628744	1548.333982	19.229504
48.200861	1542.200637	19.234522
47.969209	1547.166527	19.239539
48.026429	1542.224755	19.244557
48.200219	1539.868395	19.249575
47.896764	1545.467260	19.254592
48.417687	1541.276545	19.259610
47.892511	1549.425457	19.264627
47.955537	1547.190596	19.269645
48.207303	1538.267072	19.274663
47.714878	1547.594339	19.279680
48.035679	1548.490841	19.284698
48.310344	1560.235330	19.289715
48.345699	1562.906027	19.294733
48.497310	1566.012971	19.299751
48.456955	1571.359172	19.304768
48.146503	1576.416316	19.309786
48.022556	1570.070109	19.314803
48.461233	1580.558085	19.319821
48.365754	1582.457134	19.324839
48.174897	1601.362909	19.329856
48.804816	1599.733538	19.334874
48.803494	1597.540313	19.339891
48.943625	1590.695107	19.344909
49.242553	1604.780715	19.349927
49.191173	1616.147111	19.354944
49.364773	1613.746587	19.359962
49.546130	1600.747068	19.364979
48.914883	1592.785574	19.369997
49.442736	1600.813708	19.375015
49.416344	1610.503517	19.380032
49.454293	1605.208121	19.385050
49.530855	1620.142824	19.390067
49.934116	1617.693693	19.395085
49.618649	1598.368530	19.400103
49.440711	1601.050559	19.405120
49.790871	1602.220190	19.410138
49.740091	1607.899413	19.415155
49.862964	1610.569030	19.420173
50.123443	1617.136816	19.425191
49.815165	1611.217128	19.430208
49.762643	1593.024799	19.435226
49.586103	1602.100620	19.440243
50.046013	1605.392810	19.445261
50.370771	1607.573178	19.450279
49.868497	1610.514319	19.455296
50.185237	1602.656772	19.460314
50.141298	1613.245630	19.465331
49.973269	1607.436521	19.470349
50.264593	1608.735297	19.475367
49.776058	1616.042164	19.480384
50.220219	1607.022186	19.485402
50.053376	1609.740350	19.490419
50.371959	1629.614123	19.495437
50.340286	1627.211042	19.500455
50.017725	1642.804777	19.505472
50.586917	1633.771509	19.510490
50.627812	1638.186609	19.515507
50.453306	1635.499775	19.520525
50.842866	1632.459464	19.525543
50.478198	1632.245156	19.530560
50.573274	1641.354185	19.535578
50.981947	1657.152121	19.540595
51.035706	1657.209946	19.545613
51.128369	1661.313967	19.550631
51.022530	1660.421597	19.555648
51.301592	1652.907622	19.560666
51.524817	1651.922668	19.565683
51.473467	1655.960883	19.570701
51.569414	1656.917867	19.575719
51.528910	1658.713632	19.580736
51.739401	1652.419144	19.585754
51.522063	1657.600585	19.590771
51.595875	1655.382957	19.595789
51.318594	1648.372740	19.600807
51.659280	1644.775163	19.605824
51.636355	1652.873834	19.610842
51.532540	1651.779164	19.615859
51.624983	1644.354396	19.620877
51.664133	1651.405021	19.625895
51.468547	1654.329678	19.630912
51.564901	1652.335750	19.635930
52.070586	1645.300698	19.640947
51.722883	1647.696890	19.645965
51.574287	1645.548825	19.650983
51.806793	1656.990696	19.656000
52.034716	1663.920227	19.661018
51.898045	1662.925384	19.666035
51.972757	1672.798213	19.671053
52.119523	1664.228769	19.676071
51.789956	1669.891727	19.681088
52.132223	1678.094149	19.686106
52.344769	1682.438183	19.691123
52.577227	1696.114530	19.696141
52.584360	1691.969563	19.701159
52.667380	1703.179250	19.706176
52.859259	1702.268636	19.711194
52.618499	1697.013724	19.716211
52.476669	1693.513828	19.721229
52.705959	1694.077515	19.726247
52.276731	1694.532925	19.731264
52.712399	1691.611619	19.736282
52.754919	1702.821339	19.741299
52.648811	1707.594023	19.746317
53.004368	1712.941357	19.751335
53.008935	1721.837376	19.756352
52.831300	1715.572117	19.761370
53.075840	1711.282646	19.766387
52.939275	1723.325216	19.771405
53.377404	1708.432817	19.776423
53.338687	1723.751763	19.781440
53.536339	1735.019253	19.786458
53.841637	1732.746412	19.791475
53.400133	1736.160919	19.796493
53.692924	1733.255681	19.801511
53.579090	1739.374041	19.806528
53.795372	1735.821185	19.811546
53.520879	1733.702302	19.816563
53.404568	1742.850814	19.821581
53.818205	1731.635822	19.826599
53.937696	1732.952062	19.831616
54.049140	1730.485517	19.836634
54.049057	1725.385404	19.841651
53.944552	1726.096071	19.846669
53.821710	1730.779859	19.851687
53.939021	1739.235318	19.856704
54.478599	1749.275213	19.861722
54.371215	1760.230726	19.866739
53.906333	1760.388747	19.871757
54.563417	1756.829943	19.876775
54.550626	1753.423433	19.881792
54.719149	1749.218452	19.886810
54.738862	1744.705405	19.891827
54.577959	1751.563337	19.896845
54.679591	1752.052348	19.901863
54.721477	1755.555236	19.906880
54.642486	1754.819611	19.911898
54.901660	1740.930429	19.916915
54.409568	1751.693731	19.921933
54.859718	1756.792714	19.926951
54.785687	1770.501357	19.931968
55.097809	1772.535394	19.936986
55.338715	1769.751895	19.942003
54.994349	1781.703977	19.947021
55.264978	1780.383364	19.952039
54.963267	1781.188050	19.957056
55.117016	1775.328471	19.962074
55.245168	1773.215932	19.967091
55.021354	1779.373629	19.972109
55.465929	1767.626714	19.977127
55.272497	1772.220581	19.982144
55.491537	1795.641708	19.987162
55.415043	1801.025201	19.992179
55.486001	1801.951392	19.997197
55.920226	1799.579442	20.002215
55.837259	1795.682113	20.007232
55.416822	1803.972529	20.012250
55.923905	1794.163065	20.017267
55.971315	1795.168689	20.022285
56.016972	1791.342733	20.027303
55.985002	1784.619098	20.032320
55.666292	1797.832731	20.037338
56.139384	1804.714437	20.042355
55.977853	1820.519798	20.047373
56.216497	1823.969780	20.052391
56.100625	1823.902694	20.057408
56.322952	1821.090538	20.062426
56.760756	1815.625129	20.067443
56.535756	1822.654087	20.072461
56.391039	1824.709209	20.077479
56.532185	1821.616262	20.082496
56.437844	1824.862778	20.087514
56.836402	1833.987477	20.092531
56.606377	1848.929377	20.097549
56.833188	1843.134074	20.102567
56.990115	1845.239774	20.107584
57.189092	1842.538578	20.112602
57.251534	1831.217591	20.117619
56.889525	1844.469602	20.122637
57.052242	1838.201472	20.127655
57.083528	1838.755158	20.132672
56.992597	1848.433115	20.137690
57.116406	1840.902358	20.142707
57.089622	1850.948989	20.147725
57.579494	1847.144948	20.152743
57.768790	1862.522969	20.157760
57.780824	1863.111233	20.162778
57.996781	1857.866774	20.167795
57.889514	1857.684723	20.172813
57.901945	1866.241887	20.177831
58.176316	1856.162714	20.182848
57.764685	1845.761808	20.187866
58.170904	1847.263523	20.192883
58.033433	1851.280558	20.197901
58.259130	1857.762358	20.202919
58.061382	1851.105699	20.207936
57.792781	1854.928670	20.212954
58.415452	1847.556453	20.217971
58.039660	1847.119808	20.222989
58.014753	1853.410480	20.228007
58.637168	1855.743073	20.233024
58.056860	1854.413755	20.238042
58.284290	1853.368168	20.243059
58.241944	1856.066863	20.248077
58.498431	1864.658377	20.253095
58.457303	1875.606736	20.258112
58.181258	1883.416942	20.263130
58.652919	1878.851989	20.268147
58.348927	1880.360831	20.273165
58.500385	1885.500336	20.278183
59.022023	1885.068262	20.283200
59.025243	1899.007914	20.288218
59.414395	1912.208564	20.293235
59.671131	1902.353051	20.298253
59.469551	1891.174385	20.303271
59.177309	1878.157342	20.308288
58.839698	1884.067797	20.313306
59.099686	1880.530157	20.318323
59.025641	1899.607306	20.323341
58.930333	1897.946358	20.328359
59.671697	1905.180575	20.333376
59.274041	1901.446144	20.338394
59.503143	1908.388209	20.343411
59.626268	1904.367042	20.348429
59.266167	1903.748043	20.353447
59.405281	1919.257060	20.358464
59.695164	1929.452951	20.363482
59.848187	1924.196241	20.368499
59.578954	1927.782624	20.373517
59.994624	1920.647951	20.378535
60.085548	1922.681945	20.383552
59.794545	1939.886883	20.388570
60.194250	1946.303580	20.393587
60.492614	1949.157207	20.398605
60.320270	1959.438158	20.403623
60.650772	1953.585546	20.408640
60.568705	1960.279716	20.413658
60.816250	1949.573485	20.418675
60.623132	1956.947821	20.423693
60.630510	1942.056441	20.428711
60.666868	1941.015536	20.433728
60.731640	1952.821573	20.438746
60.906358	1942.862115	20.443763
60.750588	1946.285547	20.448781
60.888390	1947.321202	20.453799
60.937525	1946.587588	20.458816
60.683667	1945.923537	20.463834
60.911474	1957.167506	20.468851
61.145501	1961.315724	20.473869
61.182680	1966.542590	20.478887
61.312708	1971.158418	20.483904
60.854894	1982.793867	20.488922
61.364279	1978.453371	20.493939
61.491488	1978.449193	20.498957
61.461836	1967.514962	20.503975
61.667564	1970.768144	20.508992
61.622891	1989.234825	20.514010
61.934443	2000.554070	20.519027
62.350501	1987.097746	20.524045
62.144059	1989.484474	20.529063
62.354855	1980.895379	20.534080
62.273980	1975.372319	20.539098
61.984216	1964.229515	20.544115
62.033009	1962.258785	20.549133
62.365402	1981.909863	20.554151
62.415565	1982.968720	20.559168
62.410603	1989.764438	20.564186
62.636131	1992.105580	20.569203
61.821058	1984.093809	20.574221
62.317388	1986.420926	20.579239
62.302956	1981.805864	20.584256
62.409816	1989.158463	20.589274
62.867478	1976.064886	20.594291
62.495479	1985.979472	20.599309
62.657108	1985.742666	20.604327
62.890800	1989.070371	20.609344
62.913299	2000.573770	20.614362
62.879268	2009.722151	20.619379
63.337495	2004.692176	20.624397
62.990312	2004.083773	20.629415
63.051897	1995.764220	20.634432
63.193272	1999.276817	20.639450
63.116434	1995.937104	20.644467
63.443447	1997.287128	20.649485
63.293209	1995.196086	20.654503
63.721194	1998.288209	20.659520
63.606968	2002.399474	20.664538
63.515808	1993.507359	20.669555
63.621127	1990.265351	20.674573
63.611564	1993.438649	20.679591
63.558259	2013.563633	20.684608
63.736599	2019.020883	20.689626
63.993614	2017.169014	20.694643
64.237310	2016.733143	20.699661
63.919861	2018.850066	20.704679
64.232759	2024.279923	20.709696
64.194946	2017.269915	20.714714
64.179669	2023.963112	20.719731
64.454413	2028.758270	20.724749
64.265345	2027.168809	20.729767
64.163199	2024.432706	20.734784
64.021849	2021.450262	20.739802
64.174029	2041.612517	20.744819
64.604805	2042.545468	20.749837
64.432235	2050.064957	20.754855
64.559353	2044.263117	20.759872
64.463171	2047.124922	20.764890
64.358906	2044.777343	20.769907
64.681215	2064.089237	20.774925
64.616950	2068.303151	20.779943
64.967427	2065.903260	20.784960
64.979560	2075.912359	20.789978
65.084858	2065.446114	20.794995
65.365145	2070.912656	20.800013
65.073049	2070.623850	20.805031
65.472226	2070.210959	20.810048
65.209964	2085.486335	20.815066
65.613083	2097.069029	20.820083
65.647090	2092.610465	20.825101
65.945462	2093.542071	20.830119
65.952784	2086.240918	20.835136
66.170992	2089.552132	20.840154
66.249954	2086.020721	20.845171
66.405660	2081.394758	20.850189
65.994966	2085.969090	20.855207
66.346311	2078.632978	20.860224
66.136511	2090.718829	20.865242
66.281588	2085.122462	20.870259
66.240832	2081.003845	20.875277
65.971697	2085.656992	20.880295
66.429007	2083.972568	20.885312
66.049106	2091.508778	20.890330
66.076343	2087.979158	20.895347
66.189881	2079.629334	20.900365
66.020973	2104.831702	20.905383
66.430372	2111.549923	20.910400
66.623449	2107.202144	20.915418
66.422852	2116.698595	20.920435
66.843843	2129.730302	20.925453
66.943050	2138.715850	20.930471
67.240943	2133.770926	20.935488
67.364435	2141.209351	20.940506
67.145320	2140.075906	20.945523
67.653823	2137.534472	20.950541
67.427382	2130.749649	20.955559
67.507565	2125.419079	20.960576
67.538116	2138.773918	20.965594
67.575739	2135.419403	20.970611
67.811866	2121.063284	20.975629
67.278939	2133.707916	20.980647
67.644564	2132.227216	20.985664
67.241094	2133.675918	20.990682
67.627004	2137.150230	20.995699
67.441607	2131.634030	21.000717
67.463633	2144.725099	21.005735
68.321468	2145.004117	21.010752
68.497302	2154.413207	21.015770
68.290134	2159.735221	21.020787
68.194110	2148.811278	21.025805
68.037008	2151.464876	21.030823
68.257007	2144.572229	21.035840
68.420990	2149.258530	21.040858
68.443242	2155.699722	21.045875
68.353693	2147.214413	21.050893
68.545451	2163.889454	21.055911
68.890642	2172.075866	21.060928
68.592683	2176.234892	21.065946
68.501982	2174.756249	21.070963
68.664056	2176.419332	21.075981
68.780852	2177.587692	21.080999
68.662362	2170.984774	21.086016
68.581325	2179.244279	21.091034
68.953856	2187.467443	21.096051
69.458974	2195.553062	21.101069
69.376331	2202.323158	21.106087
69.182625	2197.603573	21.111104
69.769615	2195.838856	21.116122
69.692788	2195.036595	21.121139
69.809027	2193.471875	21.126157
69.644358	2196.723164	21.131175
69.828917	2193.175189	21.136192
69.776050	2196.604638	21.141210
69.646728	2195.207791	21.146227
69.923464	2202.874719	21.151245
69.935421	2214.304161	21.156263
70.224521	2218.832009	21.161280
70.423307	2221.669721	21.166298
70.062101	2224.715100	21.171315
70.317865	2212.984853	21.176333
70.195498	2226.530989	21.181351
70.135606	2218.362921	21.186368
70.149087	2222.896079	21.191386
70.611679	2238.452531	21.196403
70.884155	2243.314380	21.201421
70.861082	2247.004283	21.206439
70.596274	2245.556068	21.211456
70.983784	2239.858549	21.216474
71.000813	2242.428068	21.221491
70.807807	2228.823969	21.226509
71.179682	2242.857622	21.231527
71.194584	2237.496217	21.236544
70.934265	2242.245863	21.241562
70.858932	2247.859701	21.246579
71.429965	2260.277807	21.251597
71.302093	2264.312366	21.256615
71.606702	2264.756966	21.261632
71.789971	2262.724105	21.266650
71.336144	2273.175580	21.271667
71.542754	2258.016016	21.276685
71.435375	2268.514204	21.281703
71.649849	2268.193369	21.286720
71.721374	2273.342353	21.291738
71.514562	2289.486610	21.296755
71.983323	2282.880015	21.301773
71.781265	2288.873516	21.306791
72.172155	2290.103091	21.311808
72.145789	2292.041884	21.316826
72.146440	2304.281115	21.321843
72.409179	2306.392386	21.326861
72.533171	2306.426586	21.331879
72.555796	2314.688849	21.336896
72.658115	2308.906589	21.341914
72.833694	2318.192716	21.346931
72.792985	2301.152953	21.351949
72.619026	2314.644115	21.356967
73.070607	2309.059624	21.361984
72.971931	2317.113653	21.367002
72.937062	2318.529868	21.372019
73.271246	2310.915457	21.377037
73.145611	2315.176917	21.382055
72.921919	2318.696275	21.387072
73.467301	2332.627069	21.392090
73.321315	2342.323385	21.397107
73.599696	2332.603115	21.402125
73.197771	2341.411634	21.407143
73.635719	2333.597902	21.412160
73.933565	2336.461142	21.417178
73.473317	2339.225383	21.422195
73.775937	2332.540648	21.427213
73.876476	2340.793872	21.432231
74.067337	2347.732632	21.437248
74.297949	2340.361675	21.442266
74.056499	2352.250669	21.447283
74.097751	2344.205566	21.452301
74.141191	2351.877548	21.457319
74.092806	2348.265043	21.462336
74.624276	2347.919791	21.467354
73.980926	2346.467753	21.472371
74.522027	2366.187550	21.477389
74.827017	2372.505620	21.482407
74.409925	2379.366055	21.487424
74.843601	2374.333514	21.492442
75.073894	2376.579276	21.497459
75.039889	2371.351739	21.502477
74.577735	2380.914556	21.507495
74.651817	2392.921415	21.512512
75.259222	2394.177042	21.517530
75.120970	2401.012735	21.522547
75.300810	2395.584413	21.527565
75.239611	2399.857890	21.532583
75.416663	2399.577634	21.537600
75.493682	2400.581810	21.542618
75.554866	2418.719891	21.547635
75.898875	2420.319775	21.552653
75.921344	2422.695944	21.557671
75.952345	2424.253341	21.562688
76.286557	2420.868086	21.567706
75.830570	2418.518753	21.572723
76.032585	2415.763342	21.577741
76.069646	2423.584692	21.582759
75.929797	2412.452839	21.587776
76.169947	2425.765584	21.592794
76.505953	2445.296672	21.597811
76.861017	2437.186581	21.602829
76.848958	2443.428105	21.607847
76.627681	2440.612763	21.612864
76.798848	2442.485907	21.617882
77.049043	2439.347364	21.622899
77.162939	2434.355438	21.627917
77.104816	2439.957172	21.632935
76.868369	2432.214340	21.637952
77.088451	2432.230330	21.642970
77.141305	2432.190460	21.647987
77.357084	2437.178021	21.653005
77.213141	2437.011178	21.658023
76.970408	2430.724306	21.663040
77.064167	2431.381843	21.668058
77.196137	2453.510837	21.673075
77.544889	2461.873566	21.678093
77.502581	2455.725715	21.683111
77.368459	2454.083421	21.688128
77.484609	2463.609331	21.693146
77.505044	2472.190779	21.698163
77.905701	2481.268139	21.703181
78.258753	2486.164773	21.708199
77.812244	2484.514608	21.713216
78.218373	2479.656784	21.718234
78.234555	2483.921314	21.723251
78.168458	2478.537810	21.728269
78.162848	2503.516315	21.733287
78.173992	2505.029488	21.738304
78.570179	2507.448113	21.743322
78.441907	2514.411687	21.748339
78.703240	2513.152446	21.753357
78.885461	2522.633319	21.758375
78.445613	2531.810828	21.763392
79.057701	2533.984170	21.768410
79.037863	2535.691568	21.773427
79.417178	2528.890592	21.778445
79.521909	2528.552229	21.783463
79.447927	2532.527907	21.788480
79.599947	2515.202098	21.793498
79.242541	2526.856882	21.798515
79.135444	2515.195914	21.803533
79.239002	2527.463361	21.808551
79.893797	2543.835812	21.813568
79.951260	2535.860674	21.818586
80.221418	2552.867813	21.823603
80.048415	2543.912502	21.828621
80.460201	2541.215734	21.833639
79.946451	2549.634732	21.838656
80.177918	2544.416050	21.843674
80.022836	2539.803943	21.848691
80.159544	2541.988642	21.853709
80.056955	2552.517807	21.858727
80.460437	2569.207395	21.863744
80.497372	2578.136641	21.868762
80.535851	2574.144367	21.873779
80.811020	2571.724648	21.878797
80.573895	2579.008291	21.883815
80.489962	2587.707142	21.888832
80.638153	2583.170600	21.893850
80.963971	2591.031999	21.898867
80.991996	2594.268950	21.903885
81.120469	2599.244986	21.908903
81.369708	2613.418077	21.913920
81.821370	2614.338320	21.918938
81.719179	2621.076918	21.923955
82.049590	2611.847020	21.928973
82.277358	2608.260632	21.933991
81.870224	2614.409460	21.939008
82.130793	2611.483882	21.944026
82.019410	2620.146019	21.949043
81.905905	2609.114070	21.954061
82.232893	2607.159651	21.959079
82.193841	2616.511120	21.964096
82.065395	2608.429363	21.969114
82.347010	2611.503497	21.974131
82.316822	2607.190578	21.979149
82.229990	2605.869100	21.984167
82.217043	2615.595219	21.989184
82.772920	2624.193847	21.994202
82.795640	2634.406748	21.999219
82.556278	2636.325293	22.004237
82.696037	2625.143189	22.009255
82.699635	2639.828210	22.014272
82.741693	2632.098468	22.019290
82.782666	2644.066496	22.024307
83.166594	2655.204384	22.029325
83.603681	2650.013424	22.034343
83.453825	2665.296929	22.039360
83.346809	2660.737229	22.044378
83.524669	2664.626137	22.049395
83.249362	2662.125373	22.054413
83.305138	2664.793035	22.059431
83.673669	2680.648663	22.064448
83.756682	2684.419876	22.069466
83.864246	2682.480890	22.074483
83.616305	2690.012454	22.079501
83.644225	2690.894936	22.084519
83.880775	2696.040280	22.089536
84.076266	2700.365141	22.094554
84.104672	2703.482117	22.099571
84.400849	2713.563847	22.104589
84.385196	2713.525242	22.109607
84.490977	2711.305632	22.114624
84.563720	2727.068771	22.119642
84.864367	2727.570815	22.124659
85.000701	2734.571922	22.129677
85.130590	2732.231754	22.134695
84.641163	2745.419172	22.139712
85.154584	2732.066975	22.144730
85.231856	2730.861807	22.149747
85.301228	2734.556263	22.154765
85.657777	2732.486733	22.159783
85.612196	2750.834403	22.164800
85.564755	2754.307295	22.169818
85.767975	2758.997077	22.174835
85.637900	2754.592461	22.179853
86.061339	2741.655190	22.184871
86.125347	2759.070408	22.189888
85.981899	2752.556403	22.194906
86.105550	2749.655410	22.199923
86.411291	2756.860385	22.204941
86.274982	2741.198653	22.209959
86.275237	2753.804369	22.214976
86.305872	2744.555090	22.219994
86.312586	2756.427562	22.225011
86.539941	2772.059207	22.230029
86.743389	2767.103658	22.235047
86.549606	2779.174835	22.240064
86.631085	2768.061741	22.245082
86.993083	2775.620871	22.250099
86.810057	2789.691391	22.255117
87.290585	2785.490942	22.260135
87.253510	2795.590211	22.265152
87.320353	2790.876991	22.270170
87.704938	2791.312232	22.275187
87.492814	2794.747809	22.280205
87.506892	2788.259610	22.285223
87.175868	2797.353923	22.290240
87.685508	2793.073163	22.295258
87.507204	2807.105082	22.300275
87.888144	2813.335661	22.305293
87.852516	2827.809204	22.310311
87.820775	2830.231794	22.315328
87.991948	2814.158863	22.320346
88.230500	2824.502179	22.325363
88.229157	2836.028784	22.330381
88.278449	2842.904698	22.335399
88.397731	2837.842381	22.340416
88.423133	2845.258592	22.345434
88.545933	2844.702771	22.350451
88.781660	2838.252421	22.355469
88.331786	2834.945746	22.360487
88.673552	2853.261240	22.365504
88.731807	2860.381940	22.370522
89.065483	2868.800878	22.375539
89.077484	2870.313947	22.380557
88.995301	2867.382059	22.385575
89.008660	2876.012151	22.390592
89.481861	2876.644976	22.395610
89.514468	2888.674444	22.400627
89.405412	2888.186510	22.405645
89.758990	2896.990556	22.410663
89.479120	2887.565760	22.415680
89.642164	2896.516436	22.420698
89.977219	2895.981015	22.425715
89.827648	2911.113186	22.430733
89.950812	2912.397377	22.435751
90.179062	2911.070700	22.440768
90.099700	2912.329808	22.445786
90.648602	2919.534628	22.450803
90.743381	2928.852667	22.455821
90.982549	2929.847250	22.460839
90.896091	2937.388336	22.465856
91.232699	2943.584875	22.470874
90.963164	2935.929070	22.475891
91.085316	2934.322330	22.480909
91.232855	2933.245013	22.485927
91.051688	2935.466937	22.490944
91.012056	2930.158057	22.495962
91.408809	2919.311096	22.500979
91.293521	2926.796726	22.505997
91.518282	2942.712984	22.511015
91.517258	2951.891391	22.516032
91.496639	2948.103979	22.521050
91.872598	2946.356475	22.526067
91.771565	2956.967693	22.531085
92.158949	2949.900173	22.536103
91.932214	2954.758367	22.541120
91.816599	2958.194635	22.546138
92.172928	2970.482750	22.551155
91.950951	2976.514317	22.556173
92.348776	2968.659257	22.561191
92.564048	2983.888983	22.566208
92.494705	3000.378459	22.571226
92.935922	3001.934761	22.576243
92.811173	3001.193628	22.581261
92.915096	2998.210468	22.586279
93.163424	3000.343017	22.591296
93.239021	2998.434255	22.596314
93.328864	2996.248670	22.601331
93.332226	2995.588465	22.606349
93.586044	3005.979993	22.611367
93.601416	3006.738208	22.616384
93.181390	3017.674030	22.621402
93.734136	3025.118163	22.626419
93.339125	3031.555606	22.631437
93.504753	3023.588557	22.636455
93.837962	3034.668346	22.641472
93.799612	3042.186157	22.646490
94.247166	3042.832475	22.651507
94.354505	3040.713580	22.656525
94.422677	3040.403031	22.661543
94.211996	3039.012550	22.666560
94.203459	3052.102755	22.671578
94.696989	3053.786585	22.676595
94.584893	3065.999810	22.681613
94.518625	3063.513583	22.686631
94.743196	3067.846602	22.691648
94.473883	3071.278566	22.696666
95.187876	3058.715327	22.701683
94.865210	3070.308205	22.706701
95.179785	3075.693933	22.711719
95.338156	3085.664901	22.716736
95.208438	3085.237010	22.721754
95.570803	3084.185996	22.726771
95.539161	3086.835854	22.731789
95.534078	3088.102275	22.736807
95.568227	3091.278387	22.741824
95.758680	3112.117593	22.746842
95.985728	3108.079878	22.751859
95.637947	3114.961292	22.756877
96.084617	3111.397323	22.761895
96.286414	3111.261524	22.766912
96.176420	3131.238825	22.771930
96.835597	3127.209153	22.776947
96.571554	3130.356240	22.781965
96.320122	3132.226228	22.786983
96.594773	3136.232637	22.792000
96.678184	3138.151165	22.797018
97.196818	3137.738477	22.802035
96.947624	3160.354149	22.807053
97.098565	3155.046908	22.812071
97.386662	3163.160656	22.817088
97.327169	3153.748537	22.822106
97.562282	3146.622736	22.827123
97.402395	3151.378977	22.832141
97.635366	3166.280991	22.837159
97.880889	3172.539224	22.842176
98.013848	3181.393755	22.847194
97.815999	3180.411567	22.852211
98.127856	3180.769838	22.857229
98.032662	3170.075551	22.862247
98.571755	3166.162528	22.867264
98.347399	3173.517004	22.872282
98.327840	3184.920436	22.877299
98.172645	3186.276663	22.882317
98.436887	3194.432037	22.887335
98.825213	3196.410114	22.892352
98.636367	3205.425543	22.897370
99.031409	3203.804432	22.902387
98.977651	3212.849201	22.907405
99.334657	3227.447769	22.912423
99.512459	3224.857000	22.917440
99.213022	3233.798238	22.922458
99.718962	3227.791480	22.927475
99.444502	3225.470410	22.932493
99.449436	3224.658450	22.937511
99.575118	3222.842818	22.942528
99.327388	3244.448362	22.947546
99.542403	3245.459372	22.952563
99.753744	3258.521591	22.957581
99.730205	3261.425863	22.962599
99.831875	3267.659323	22.967616
99.871042	3277.049380	22.972634
99.999245	3278.743123	22.977651
100.089859	3288.062001	22.982669
100.637195	3304.016417	22.987687
100.800203	3296.813478	22.992704
100.753718	3304.777707	22.997722
100.948349	3301.240562	23.002739
101.017176	3300.263931	23.007757
101.236509	3297.559331	23.012775
101.268329	3311.381970	23.017792
101.359973	3316.720634	23.022810
101.568936	3320.005118	23.027827
101.907859	3321.397568	23.032845
101.384554	3317.811929	23.037863
101.733765	3318.723013	23.042880
101.681929	3329.266772	23.047898
101.737499	3309.698571	23.052915
101.970353	3320.784790	23.057933
102.102294	3335.740648	23.062951
102.202480	3336.608684	23.067968
102.385289	3338.546380	23.072986
102.249046	3340.897035	23.078003
102.470286	3337.374653	23.083021
102.761980	3341.517314	23.088039
102.557964	3337.682802	23.093056
102.681052	3343.837182	23.098074
102.885386	3364.507222	23.103091
103.063038	3371.202256	23.108109
102.778060	3371.310002	23.113127
103.053750	3364.278759	23.118144
103.036006	3380.605840	23.123162
103.345436	3390.322901	23.128179
103.570850	3392.348617	23.133197
103.379216	3400.089437	23.138215
103.705512	3387.406805	23.143232
103.302877	3397.080769	23.148250
103.467944	3413.767463	23.153267
104.241112	3414.608974	23.158285
103.929478	3415.863475	23.163303
104.500289	3416.528374	23.168320
104.623075	3419.229838	23.173338
104.707478	3423.019926	23.178355
104.828673	3428.473933	23.183373
104.994959	3433.106552	23.188391
105.207469	3427.382423	23.193408
105.281919	3437.183667	23.198426
105.333220	3435.133476	23.203443
105.341051	3424.893187	23.208461
105.354195	3428.183119	23.213479
105.530385	3430.538494	23.218496
105.034999	3433.519874	23.223514
105.517649	3433.078100	23.228531
105.185852	3425.270870	23.233549
105.239868	3451.996248	23.238567
105.927730	3448.593273	23.243584
105.840183	3455.307793	23.248602
105.796746	3458.243621	23.253619
106.225294	3476.435683	23.258637
106.158631	3483.068034	23.263655
106.550684	3483.394810	23.268672
106.628135	3488.691560	23.273690
106.557152	3481.730367	23.278707
106.469832	3483.713556	23.283725
106.844643	3503.987759	23.288743
106.777087	3508.985290	23.293760
106.813274	3511.940215	23.298778
106.965984	3511.019870	23.303795
107.058721	3514.818140	23.308813
107.187328	3524.478382	23.313831
107.345873	3531.343754	23.318848
107.482433	3537.284616	23.323866
107.286766	3532.132570	23.328883
107.707306	3535.134597	23.333901
107.863243	3556.623613	23.338919
108.107215	3554.252842	23.343936
108.060897	3559.742601	23.348954
108.287925	3565.180069	23.353971
108.488030	3557.336793	23.358989
108.506936	3555.945023	23.364007
108.520222	3560.661615	23.369024
108.351416	3560.362933	23.374042
108.243873	3580.343502	23.379059
108.779895	3577.926972	23.384077
108.721330	3586.745425	23.389095
108.881869	3578.722117	23.394112
108.757286	3587.674010	23.399130
109.045496	3606.500517	23.404147
109.163311	3610.812517	23.409165
109.104405	3609.196208	23.414183
109.273935	3613.335977	23.419200
109.214308	3634.325438	23.424218
109.544877	3627.654787	23.429235
109.705125	3632.828137	23.434253
109.565992	3654.417155	23.439271
109.975738	3656.571839	23.444288
110.047579	3663.684414	23.449306
110.067806	3662.002045	23.454323
110.211715	3676.123035	23.459341
110.439069	3692.244712	23.464359
110.764901	3683.078114	23.469376
110.813273	3683.256733	23.474394
110.834592	3678.108526	23.479411
110.997547	3690.695718	23.484429
111.188610	3699.017447	23.489447
111.012327	3701.481737	23.494464
110.912259	3709.501884	23.499482
111.258113	3701.982911	23.504499
111.541766	3715.393955	23.509517
111.594332	3721.294378	23.514535
112.050355	3726.891712	23.519552
112.105852	3730.137188	23.524570
112.069672	3737.156244	23.529587
112.078539	3725.911902	23.534605
112.183134	3736.999533	23.539623
112.371553	3740.135809	23.544640
112.741000	3744.654614	23.549658
112.360983	3756.727211	23.554675
112.587154	3752.771555	23.559693
112.505126	3765.971637	23.564711
112.938290	3772.611009	23.569728
113.192602	3781.857149	23.574746
112.780687	3784.181610	23.579763
113.308554	3783.562301	23.584781
113.209002	3781.570425	23.589799
113.465099	3788.527928	23.594816
113.681403	3801.959057	23.599834
113.776079	3810.437975	23.604851
113.874528	3816.072419	23.609869
113.895172	3803.509979	23.614887
114.066202	3807.864190	23.619904
114.249066	3808.432067	23.624922
114.394148	3817.647993	23.629939
114.635842	3818.355003	23.634957
114.444336	3825.818224	23.639975
114.264741	3826.988939	23.644992
114.534186	3824.358476	23.650010
114.714464	3839.291395	23.655027
114.935468	3834.345431	23.660045
114.943274	3854.513395	23.665063
114.749951	3831.830407	23.670080
115.178055	3847.317904	23.675098
115.039022	3856.941345	23.680115
115.490589	3868.691195	23.685133
115.500941	3876.498421	23.690151
115.625616	3871.586477	23.695168
115.971959	3886.622830	23.700186
116.023371	3896.756196	23.705203
115.822280	3896.449940	23.710221
115.881255	3899.795906	23.715239
116.080630	3900.269664	23.720256
116.149206	3907.288155	23.725274
116.163503	3918.109127	23.730291
116.803920	3923.090546	23.735309
116.675489	3924.549951	23.740327
116.757895	3927.854375	23.745344
117.284371	3937.951213	23.750362
116.959190	3947.228255	23.755379
116.976585	3943.087476	23.760397
117.301448	3956.407021	23.765415
117.260664	3953.604195	23.770432
117.526423	3967.974617	23.775450
117.863197	3970.727861	23.780467
118.036860	3968.327018	23.785485
117.909696	3972.380784	23.790503
118.004811	3971.005450	23.795520
118.191606	3982.105604	23.800538
118.105352	3990.284687	23.805555
118.562655	3988.224485	23.810573
118.724489	4006.275796	23.815591
118.345659	4010.605728	23.820608
118.652954	3999.844737	23.825626
118.706631	4014.857607	23.830643
118.790861	4021.570676	23.835661
119.499929	4026.737066	23.840679
118.847227	4031.068877	23.845696
119.038750	4025.660332	23.850714
118.898936	4040.902391	23.855731
119.047258	4040.225750	23.860749
119.228276	4061.386326	23.865767
119.497033	4063.566305	23.870784
119.657028	4071.186038	23.875802
120.292122	4090.899314	23.880819
120.505250	4099.792238	23.885837
120.714365	4096.830295	23.890855
120.703523	4100.206175	23.895872
120.678736	4095.125045	23.900890
120.715150	4087.581795	23.905907
120.747127	4092.548111	23.910925
120.769764	4104.860871	23.915943
121.195180	4118.698216	23.920960
121.276644	4114.910349	23.925978
121.145936	4124.551565	23.930995
121.639193	4115.165980	23.936013
121.688687	4121.227992	23.941031
121.572364	4127.969364	23.946048
121.829080	4132.430174	23.951066
121.616301	4140.947945	23.956083
121.822478	4132.746796	23.961101
122.183426	4153.872978	23.966119
122.418432	4160.919152	23.971136
122.559643	4164.208093	23.976154
122.308341	4173.230631	23.981171
122.042453	4168.667030	23.986189
122.099450	4176.400793	23.991207
122.437794	4195.059080	23.996224
122.746745	4201.737009	24.001242
122.840201	4215.658000	24.006259
123.194885	4214.895363	24.011277
122.844825	4212.551287	24.016295
123.029140	4233.111824	24.021312
123.620727	4234.673089	24.026330
123.211597	4240.147296	24.031347
123.647864	4257.947538	24.036365
123.891533	4261.356172	24.041383
123.809989	4265.882635	24.046400
123.834622	4264.584606	24.051418
123.765624	4284.853461	24.056435
124.256371	4295.893563	24.061453
124.310145	4289.550117	24.066471
124.401673	4306.047141	24.071488
124.750127	4313.258676	24.076506
125.033663	4317.753208	24.081523
125.005124	4313.761581	24.086541
125.306543	4317.767218	24.091559
125.438479	4324.858012	24.096576
126.037784	4328.315106	24.101594
125.640923	4349.437137	24.106611
126.002603	4342.388891	24.111629
125.920854	4352.025714	24.116647
125.960367	4348.550547	24.121664
126.138672	4349.706257	24.126682
126.229518	4342.555244	24.131699
126.396204	4340.439527	24.136717
126.501064	4350.798351	24.141735
126.434227	4361.613359	24.146752
126.784647	4364.045724	24.151770
126.337388	4367.085998	24.156787
126.744208	4386.497619	24.161805
127.196393	4378.466144	24.166823
126.958679	4395.576682	24.171840
127.288545	4399.994534	24.176858
127.346961	4411.307609	24.181875
127.424749	4423.002746	24.186893
127.459398	4423.694870	24.191911
127.585473	4430.325779	24.196928
128.031635	4434.128846	24.201946
128.234798	4447.578296	24.206963
127.897536	4446.772544	24.211981
128.319025	4453.956911	24.216999
128.334019	4468.089246	24.222016
128.597907	4473.619064	24.227034
128.625212	4483.655527	24.232051
128.933970	4482.186710	24.237069
129.166109	4496.910031	24.242087
129.411506	4497.303997	24.247104
129.413270	4503.474622	24.252122
129.514812	4502.085615	24.257139
129.853675	4500.277493	24.262157
129.953100	4497.351610	24.267175
129.879031	4505.951984	24.272192
130.264021	4510.667406	24.277210
129.849216	4523.187868	24.282227
129.892168	4524.380577	24.287245
130.371697	4522.395748	24.292263
130.274847	4529.093183	24.297280
130.557471	4539.275909	24.302298
130.779275	4541.318105	24.307315
130.830490	4546.938081	24.312333
130.658738	4556.980518	24.317351
131.189542	4568.547959	24.322368
131.324184	4576.222380	24.327386
131.268974	4577.891320	24.332403
131.310350	4584.374574	24.337421
131.511386	4585.621433	24.342439
131.506985	4603.266940	24.347456
131.780864	4601.222782	24.352474
132.012531	4601.075983	24.357491
132.050078	4627.190154	24.362509
131.999429	4619.095308	24.367527
132.009470	4624.106240	24.372544
132.456006	4635.948917	24.377562
132.365007	4652.323339	24.382579
132.488103	4646.101482	24.387597
132.699797	4647.201477	24.392615
132.668570	4657.777500	24.397632
132.877601	4668.694670	24.402650
132.629263	4680.100162	24.407667
132.984670	4685.839820	24.412685
133.294625	4699.951376	24.417703
133.340375	4704.315962	24.422720
133.487260	4712.095844	24.427738
133.848742	4715.950116	24.432755
134.088110	4716.869014	24.437773
134.426005	4716.370980	24.442791
134.321176	4733.034885	24.447808
134.505401	4750.376366	24.452826
134.607354	4745.606634	24.457843
134.906595	4740.742865	24.462861
134.678088	4742.843005	24.467879
134.716486	4757.849413	24.472896
135.254576	4770.691081	24.477914
135.490739	4775.669785	24.482931
135.358148	4770.456999	24.487949
135.770671	4779.356897	24.492967
135.778060	4789.030491	24.497984
136.158627	4795.135557	24.503002
136.350149	4793.183194	24.508019
136.290262	4806.128039	24.513037
136.358928	4803.146951	24.518055
136.172901	4794.050519	24.523072
135.977007	4809.605034	24.528090
136.331323	4814.117010	24.533107
136.087035	4826.393163	24.538125
136.688390	4836.724985	24.543143
136.493687	4853.958632	24.548160
136.653282	4860.483438	24.553178
137.317173	4873.179207	24.558195
137.582305	4884.157162	24.563213
138.089420	4900.807421	24.568231
138.033859	4902.103972	24.573248
138.346203	4898.200858	24.578266
138.300808	4896.699109	24.583283
138.591433	4901.167424	24.588301
138.597265	4897.277607	24.593319
138.620536	4893.148318	24.598336
138.588778	4915.261781	24.603354
139.094233	4924.974210	24.608371
138.834420	4922.751633	24.613389
139.325770	4927.106437	24.618407
138.980335	4933.199027	24.623424
139.722259	4933.957133	24.628442
139.776012	4947.335662	24.633459
139.511818	4944.678164	24.638477
139.799256	4943.765050	24.643495
139.962054	4948.379665	24.648512
140.222091	4944.753044	24.653530
140.172758	4953.479173	24.658547
140.179076	4971.710478	24.663565
140.440892	4964.952260	24.668583
140.409632	4978.157893	24.673600
140.518755	4991.341543	24.678618
141.088179	4995.857744	24.683635
140.813138	5008.476591	24.688653
141.026118	5004.030307	24.693671
141.436118	5024.628984	24.698688
141.413545	5025.377445	24.703706
141.383245	5028.324094	24.708723
141.242662	5031.603679	24.713741
141.730726	5041.899705	24.718759
141.650727	5049.948864	24.723776
141.776118	5053.047894	24.728794
142.111371	5067.269410	24.733811
142.142569	5072.946346	24.738829
142.105115	5075.660536	24.743847
142.244944	5085.591318	24.748864
142.486532	5096.203769	24.753882
142.759827	5096.429236	24.758899
142.831170	5111.620169	24.763917
143.222618	5116.517822	24.768935
143.590528	5127.012646	24.773952
143.507931	5121.867685	24.778970
143.633700	5112.024639	24.783987
143.745363	5127.187172	24.789005
143.883984	5140.606210	24.794023
143.921399	5149.887030	24.799040
143.975517	5150.563506	24.804058
144.542976	5150.263086	24.809075
144.273905	5171.886886	24.814093
144.511226	5170.511279	24.819111
144.733934	5183.822478	24.824128
144.805932	5191.718465	24.829146
145.283238	5190.835570	24.834163
145.445268	5199.989568	24.839181
145.765980	5194.983424	24.844199
145.413245	5203.463641	24.849216
145.681678	5210.429229	24.854234
145.978708	5218.788717	24.859251
146.142780	5229.419704	24.864269
146.443922	5221.645114	24.869287
146.321806	5227.327178	24.874304
146.234958	5232.605985	24.879322
146.693035	5242.603789	24.884339
146.585162	5246.954693	24.889357
146.872159	5246.088984	24.894375
147.107559	5280.421330	24.899392
147.266482	5278.259373	24.904410
147.267476	5274.853197	24.909427
147.469358	5282.994031	24.914445
147.702227	5284.971446	24.919463
147.817322	5296.055228	24.924480
147.603438	5309.504362	24.929498
147.696349	5315.989272	24.934515
147.867790	5333.481673	24.939533
148.257182	5330.323988	24.944551
148.223175	5338.757490	24.949568
148.654344	5358.961807	24.954586
148.594705	5352.373759	24.959603
148.883707	5360.119027	24.964621
149.042578	5373.033159	24.969639
149.123578	5380.460635	24.974656
149.063333	5392.831444	24.979674
149.351882	5385.661676	24.984691
149.364513	5410.085757	24.989709
149.805437	5412.068470	24.994727
149.622204	5420.875776	24.999744
149.553751	5428.064684	25.004762
149.865528	5428.539816	25.009779
149.940158	5459.829426	25.014797
150.429359	5459.771698	25.019815
150.776015	5468.966354	25.024832
150.969947	5475.482844	25.029850
151.011446	5479.377940	25.034867
151.177531	5490.482262	25.039885
151.285691	5494.483714	25.044903
151.642978	5506.584005	25.049920
151.826288	5509.326807	25.054938
152.105366	5505.283570	25.059955
152.000037	5507.961108	25.064973
152.148934	5527.783685	25.069991
152.234921	5528.663522	25.075008
152.660676	5535.550925	25.080026
152.832460	5529.914593	25.085043
152.575809	5539.292187	25.090061
152.502123	5537.700117	25.095079
152.775541	5557.168612	25.100096
153.238073	5560.641061	25.105114
153.318682	5554.315068	25.110131
153.073956	5567.425147	25.115149
153.396924	5579.101555	25.120167
153.677325	5578.618822	25.125184
153.351526	5592.218277	25.130202
154.029726	5598.437977	25.135219
153.796176	5618.276374	25.140237
153.978488	5613.184473	25.145255
154.184299	5633.582233	25.150272
154.041606	5639.138224	25.155290
154.754648	5653.301013	25.160307
154.652089	5661.770657	25.165325
154.495510	5673.926309	25.170343
154.919282	5682.225119	25.175360
155.196779	5699.101483	25.180378
155.522787	5704.918675	25.185395
155.340049	5723.417101	25.190413
155.819426	5718.660592	25.195431
156.125541	5736.681545	25.200448
155.931637	5745.648513	25.205466
156.683536	5741.774217	25.210483
156.577195	5747.753857	25.215501
156.883519	5764.931966	25.220519
157.069529	5771.266715	25.225536
157.041914	5782.095359	25.230554
157.540218	5772.424035	25.235571
157.375916	5780.562483	25.240589
157.652899	5790.134394	25.245607
158.010639	5803.491181	25.250624
157.549221	5815.884087	25.255642
158.108340	5804.760601	25.260659
158.238195	5814.563918	25.265677
158.271536	5820.022938	25.270695
158.415002	5831.686592	25.275712
158.389064	5838.307105	25.280730
158.934131	5848.449451	25.285747
158.967244	5853.936928	25.290765
158.815181	5847.858785	25.295783
158.873336	5858.434127	25.300800
159.320708	5875.577617	25.305818
159.280854	5877.525218	25.310835
159.135456	5897.678406	25.315853
159.015235	5908.534260	25.320871
160.363367	5914.428145	25.325888
160.286407	5929.213676	25.330906
160.562101	5926.190502	25.335923
160.699582	5933.789289	25.340941
160.912078	5947.036353	25.345959
161.348579	5960.055773	25.350976
161.083096	5957.991793	25.355994
161.696800	5955.761666	25.361011
161.402569	5957.304027	25.366029
161.031106	5958.918466	25.371047
161.464133	5965.416615	25.376064
161.631732	5985.700799	25.381082
162.124024	5984.013709	25.386099
161.894353	5995.432877	25.391117
162.292204	6004.711329	25.396135
162.391924	6002.085051	25.401152
162.190859	6021.726234	25.406170
162.536525	6028.026589	25.411187
162.917266	6038.169531	25.416205
162.569917	6047.577376	25.421223
162.889858	6056.145163	25.426240
162.973774	6059.465522	25.431258
163.371531	6070.647546	25.436275
163.461318	6088.529115	25.441293
163.672658	6094.042407	25.446311
163.918672	6101.845234	25.451328
163.733421	6111.669664	25.456346
164.311283	6113.350052	25.461363
164.366624	6132.335615	25.466381
164.472877	6139.525843	25.471399
164.615794	6146.309420	25.476416
164.749872	6158.154689	25.481434
164.872766	6164.354251	25.486451
165.131686	6175.861140	25.491469
165.314663	6201.323422	25.496487
165.750657	6200.409074	25.501504
165.646770	6204.036677	25.506522
166.134396	6215.337295	25.511539
166.523355	6227.448887	25.516557
166.554463	6227.968012	25.521575
167.008177	6228.187329	25.526592
166.485369	6231.586986	25.531610
166.863445	6235.527375	25.536627
167.410003	6249.366307	25.541645
167.094551	6254.842218	25.546663
167.277281	6250.435098	25.551680
167.544961	6275.435950	25.556698
167.391042	6269.421094	25.561715
167.527388	6285.928671	25.566733
167.731942	6292.835232	25.571751
168.276384	6297.226247	25.576768
168.199370	6322.379024	25.581786
168.405710	6319.726527	25.586803
168.709741	6325.064371	25.591821
168.813891	6336.251516	25.596839
168.988567	6349.239625	25.601856
169.009059	6356.235025	25.606874
169.409770	6366.453941	25.611891
169.529340	6377.809163	25.616909
169.583702	6383.359762	25.621927
169.892854	6390.862395	25.626944
170.026104	6398.383117	25.631962
169.839355	6393.440366	25.636979
170.390441	6427.753821	25.641997
170.534727	6428.173144	25.647015
170.609262	6438.929351	25.652032
170.840015	6452.679012	25.657050
171.323252	6454.181691	25.662067
171.420863	6466.474828	25.667085
171.571303	6465.920886	25.672103
171.685860	6479.180522	25.677120
171.655432	6490.499333	25.682138
172.167669	6485.971086	25.687156
171.994707	6496.863961	25.692173
172.192418	6506.985329	25.697191
172.628337	6511.172419	25.702208
172.733713	6524.831287	25.707226
172.723366	6528.920983	25.712244
173.137426	6535.769559	25.717261
172.899076	6540.996713	25.722279
173.437346	6557.119571	25.727296
173.387558	6556.688543	25.732314
173.476152	6575.255808	25.737332
173.872303	6581.782053	25.742349
173.925578	6592.074467	25.747367
174.134467	6590.965230	25.752384
173.918914	6602.562503	25.757402
174.163476	6617.576021	25.762420
174.578813	6626.365895	25.767437
174.034674	6641.802893	25.772455
174.649485	6651.555938	25.777472
174.878605	6659.601572	25.782490
175.037132	6682.445003	25.787508
175.392714	6678.155918	25.792525
175.765936	6693.338754	25.797543
175.745278	6695.381297	25.802560
175.937800	6703.486350	25.807578
176.201433	6716.931156	25.812596
176.438419	6718.017847	25.817613
176.197161	6728.624813	25.822631
176.628488	6735.170857	25.827648
176.944368	6752.335770	25.832666
177.280858	6753.305855	25.837684
177.526163	6766.627294	25.842701
177.230727	6771.812945	25.847719
177.503492	6772.344738	25.852736
177.981755	6785.752814	25.857754
177.645371	6803.544000	25.862772
178.181732	6811.964590	25.867789
178.242997	6837.718315	25.872807
178.548028	6831.034723	25.877824
178.671554	6837.913144	25.882842
178.840693	6857.288867	25.887860
179.315516	6866.249481	25.892877
179.536825	6871.537306	25.897895
179.362484	6861.648788	25.902912
179.143145	6881.663108	25.907930
179.715272	6897.474743	25.912948
180.129149	6902.580879	25.917965
179.709723	6915.570911	25.922983
180.503286	6924.582640	25.928000
180.781212	6935.332529	25.933018
180.627251	6941.569412	25.938036
181.222391	6940.450155	25.943053
181.184696	6963.094222	25.948071
181.167014	6969.663339	25.953088
181.513252	6973.820390	25.958106
181.462621	6984.268205	25.963124
181.731987	6989.043430	25.968141
181.759601	7002.970546	25.973159
182.252376	7010.902420	25.978176
182.347710	7026.905668	25.983194
182.491128	7033.143348	25.988212
182.657356	7037.388596	25.993229
182.791048	7060.940382	25.998247
182.866002	7062.099833	26.003264
183.399289	7074.558736	26.008282
183.514016	7076.371754	26.013300
183.826559	7086.977404	26.018317
183.911933	7103.440034	26.023335
183.901349	7100.518344	26.028352
184.375193	7107.398810	26.033370
184.555383	7124.146514	26.038388
184.907270	7124.716434	26.043405
184.456029	7135.874267	26.048423
184.751788	7139.414190	26.053440
185.058730	7154.595163	26.058458
184.912049	7156.745895	26.063476
185.398427	7159.949735	26.068493
185.659824	7175.327278	26.073511
185.710718	7185.898208	26.078528
185.648251	7211.674997	26.083546
186.078023	7214.530980	26.088564
186.257145	7221.438719	26.093581
186.657584	7234.628858	26.098599
186.982502	7230.117150	26.103616
186.713809	7250.868858	26.108634
186.639902	7261.241553	26.113652
187.255028	7257.830351	26.118669
187.096094	7285.125068	26.123687
187.575721	7286.871471	26.128704
187.521332	7292.641428	26.133722
187.744686	7306.263452	26.138740
188.111402	7311.193987	26.143757
188.231896	7328.854122	26.148775
188.652213	7331.597954	26.153792
188.601244	7345.496599	26.158810
188.569629	7368.809490	26.163828
188.948933	7371.026224	26.168845
189.083016	7391.664479	26.173863
189.422202	7396.267866	26.178880
189.911339	7406.811309	26.183898
189.869235	7424.367572	26.188916
190.163937	7418.490419	26.193933
190.564716	7438.073553	26.198951
190.840113	7438.728077	26.203968
190.861944	7446.045695	26.208986
191.034370	7448.389557	26.214004
191.235588	7459.881036	26.219021
191.365925	7472.403336	26.224039
191.394991	7483.217788	26.229056
191.909319	7491.724226	26.234074
192.131867	7498.199071	26.239092
192.240350	7502.030435	26.244109
191.943095	7506.531506	26.249127
192.085879	7523.036029	26.254144
192.437768	7533.897805	26.259162
192.406974	7557.706456	26.264180
192.928560	7562.609640	26.269197
193.089531	7571.828131	26.274215
193.363309	7588.987793	26.279232
193.582123	7591.599067	26.284250
193.914016	7604.601318	26.289268
194.057202	7615.170664	26.294285
194.180296	7629.992519	26.299303
193.873426	7632.758763	26.304320
194.510797	7644.147302	26.309338
194.384341	7661.227666	26.314356
195.033936	7675.335669	26.319373
194.932773	7681.611885	26.324391
195.018245	7701.099472	26.329408
195.588907	7712.239627	26.334426
195.452672	7720.216680	26.339444
196.061529	7729.185133	26.344461
196.223383	7748.834441	26.349479
196.276883	7762.969598	26.354496
196.086747	7763.892801	26.359514
196.114464	7782.966477	26.364532
196.433043	7799.936208	26.369549
196.780033	7813.340345	26.374567
197.468822	7835.271831	26.379584
197.313918	7839.946419	26.384602
197.220485	7858.136233	26.389620
197.805454	7856.718599	26.394637
198.180251	7863.065538	26.399655
198.274909	7891.988354	26.404672
198.609661	7894.369985	26.409690
198.758698	7911.426363	26.414708
199.086727	7917.202903	26.419725
199.095522	7918.941046	26.424743
199.488459	7937.777713	26.429760
199.947774	7947.274833	26.434778
199.860507	7954.199322	26.439796
200.229995	7950.640211	26.444813
200.583576	7947.882332	26.449831
200.055257	7950.781185	26.454848
200.543672	7964.106448	26.459866
200.629141	7978.685067	26.464884
200.949442	7969.981297	26.469901
200.795654	7990.599022	26.474919
201.169606	7996.510462	26.479936
201.529224	8006.919843	26.484954
201.117161	8029.901689	26.489972
201.609928	8027.257750	26.494989
201.332636	8045.703862	26.500007
201.636335	8064.002147	26.505024
202.156614	8071.358739	26.510042
202.302244	8082.827743	26.515060
202.322352	8099.797151	26.520077
202.668432	8125.097631	26.525095
202.899204	8138.678067	26.530112
203.632178	8151.851498	26.535130
203.489611	8162.428038	26.540148
203.578038	8177.511488	26.545165
204.194821	8187.151390	26.550183
204.099021	8195.737952	26.555200
204.600544	8211.103998	26.560218
204.717509	8226.647115	26.565236
204.438164	8226.517207	26.570253
204.867224	8236.230744	26.575271
205.283920	8258.909399	26.580288
205.727108	8267.749371	26.585306
205.743534	8279.462894	26.590324
206.007409	8292.296330	26.595341
206.286369	8293.142914	26.600359
206.238912	8313.485455	26.605376
206.519084	8329.659776	26.610394
206.831384	8326.924095	26.615412
207.133637	8349.204047	26.620429
207.126876	8363.232288	26.625447
207.293693	8376.611389	26.630464
207.551890	8385.404625	26.635482
207.419420	8389.469664	26.640500
207.912813	8409.989625	26.645517
207.949312	8418.991252	26.650535
208.191533	8441.129176	26.655552
208.609494	8438.193811	26.660570
208.830831	8460.391858	26.665588
208.649597	8470.864130	26.670605
208.897665	8488.584318	26.675623
209.068564	8496.583047	26.680640
209.869139	8515.776349	26.685658
209.630271	8529.433802	26.690676
210.079234	8541.929012	26.695693
210.310089	8550.657153	26.700711
210.249564	8571.039909	26.705728
210.843169	8574.460835	26.710746
210.908303	8592.074021	26.715764
211.250403	8599.483996	26.720781
211.636389	8603.613092	26.725799
211.887156	8624.284959	26.730816
211.858559	8637.492801	26.735834
211.874739	8638.364782	26.740852
212.209057	8655.781156	26.745869
212.336646	8665.488474	26.750887
212.297270	8684.854580	26.755904
212.694495	8692.606406	26.760922
212.824530	8708.330998	26.765940
213.000694	8719.495679	26.770957
213.339634	8727.458712	26.775975
213.225512	8749.794902	26.780992
213.728183	8752.646024	26.786010
214.233181	8770.310445	26.791028
214.438382	8786.932607	26.796045
214.650046	8791.486864	26.801063
214.752430	8800.699360	26.806080
214.899313	8810.324801	26.811098
215.319495	8822.013303	26.816116
215.598946	8830.673976	26.821133
215.448052	8843.342292	26.826151
215.649651	8865.247137	26.831168
215.724841	8870.665775	26.836186
216.004421	8879.070714	26.841204
216.411096	8885.264623	26.846221
216.757189	8893.264494	26.851239
216.629414	8917.661545	26.856256
217.025672	8923.942345	26.861274
217.072840	8941.984905	26.866292
217.472455	8950.538406	26.871309
217.597070	8968.767766	26.876327
217.631136	8987.986921	26.881344
218.138323	8998.942051	26.886362
218.114943	9014.334165	26.891380
218.167575	9026.156150	26.896397
219.013546	9038.700007	26.901415
218.667565	9062.493664	26.906432
219.024064	9063.808043	26.911450
219.556672	9085.320308	26.916468
219.653101	9091.689179	26.921485
219.817775	9110.660677	26.926503
220.074759	9115.498384	26.931520
219.837741	9133.131001	26.936538
220.085916	9154.517411	26.941556
220.201751	9171.700127	26.946573
220.976024	9188.618689	26.951591
220.856239	9204.730138	26.956608
221.301644	9222.685326	26.961626
221.874972	9237.210609	26.966644
221.748825	9252.356963	26.971661
222.077639	9261.992025	26.976679
222.173668	9281.141787	26.981696
222.370368	9300.241068	26.986714
222.591188	9305.539143	26.991732
223.096366	9326.314016	26.996749
223.423031	9341.323204	27.001767
223.503716	9349.020702	27.006784
223.571934	9355.555107	27.011802
223.756326	9371.464341	27.016820
224.249088	9390.766763	27.021837
224.887826	9399.845016	27.026855
224.510589	9414.254134	27.031872
224.907802	9422.296744	27.036890
225.360540	9442.720027	27.041908
225.029501	9449.869544	27.046925
225.538197	9458.488283	27.051943
225.784767	9476.468551	27.056960
226.041947	9493.335789	27.061978
226.364183	9504.806423	27.066996
226.396737	9521.705719	27.072013
226.770143	9528.811215	27.077031
226.802705	9543.983461	27.082048
226.802074	9556.874996	27.087066
227.082552	9574.853203	27.092084
227.416652	9586.985074	27.097101
227.741278	9604.804842	27.102119
227.759982	9620.310843	27.107136
227.834572	9635.069280	27.112154
228.199232	9649.618103	27.117172
228.167501	9674.225272	27.122189
228.817028	9678.865865	27.127207
228.637069	9708.784900	27.132224
229.304800	9703.761075	27.137242
229.451070	9717.415895	27.142260
229.522241	9735.376529	27.147277
229.914489	9751.872373	27.152295
230.131919	9765.680265	27.157312
230.555478	9780.737776	27.162330
230.283024	9795.629640	27.167348
230.438554	9815.152674	27.172365
231.022206	9816.147359	27.177383
231.121791	9833.756323	27.182400
231.412941	9855.863008	27.187418
231.210908	9872.379436	27.192436
231.856673	9888.845159	27.197453
232.033523	9895.252226	27.202471
232.218528	9926.210056	27.207488
232.337465	9938.274825	27.212506
232.978716	9957.144111	27.217524
233.266543	9979.911364	27.222541
233.712128	9989.436946	27.227559
233.503895	10002.948592	27.232576
233.406705	10026.480324	27.237594
234.040684	10039.790596	27.242612
234.090981	10061.212204	27.247629
234.495174	10076.298247	27.252647
234.306830	10093.456843	27.257664
234.513560	10112.201751	27.262682
235.649934	10134.312129	27.267700
235.608507	10149.856407	27.272717
235.664575	10165.726430	27.277735
236.103270	10176.636152	27.282752
236.094311	10195.487554	27.287770
236.730014	10203.231073	27.292788
236.672799	10223.823509	27.297805
236.966709	10234.222336	27.302823
237.005572	10261.398868	27.307840
237.684226	10265.394082	27.312858
237.964767	10281.140629	27.317876
237.894893	10292.395317	27.322893
238.147847	10306.198044	27.327911
238.357511	10331.065064	27.332928
238.605674	10340.331265	27.337946
239.062945	10348.974263	27.342964
239.293014	10371.113230	27.347981
239.820764	10375.075273	27.352999
239.683473	10397.297079	27.358016
240.048405	10407.924846	27.363034
240.185813	10419.639708	27.368052
240.602917	10435.459717	27.373069
240.699987	10441.210080	27.378087
240.949193	10469.149653	27.383104
241.104806	10480.397548	27.388122
241.181833	10496.068803	27.393140
241.264327	10518.777312	27.398157
241.851563	10531.283778	27.403175
241.884656	10551.603511	27.408192
241.935077	10573.208821	27.413210
242.419173	10593.041155	27.418228
242.280721	10602.604865	27.423245
242.823193	10619.927320	27.428263
243.202205	10639.419364	27.433280
243.334195	10654.914791	27.438298
243.780029	10671.267281	27.443316
243.846139	10681.818872	27.448333
244.126659	10698.055192	27.453351
244.152252	10708.988893	27.458368
244.388794	10729.103283	27.463386
244.682955	10746.726831	27.468404
244.658390	10753.576227	27.473421
244.706911	10768.926947	27.478439
244.903852	10796.793100	27.483456
245.133836	10816.548649	27.488474
245.613725	10839.034257	27.493492
245.984255	10864.164124	27.498509
246.212162	10871.817084	27.503527
246.398776	10907.503174	27.508544
246.800525	10929.887459	27.513562
247.115577	10938.897188	27.518580
247.458844	10961.435921	27.523597
247.423927	10972.941305	27.528615
247.845892	10994.690983	27.533632
248.222673	11015.456279	27.538650
248.824656	11028.251268	27.543668
249.000628	11050.781582	27.548685
249.357230	11061.420500	27.553703
249.181108	11084.271250	27.558720
249.392026	11096.600227	27.563738
249.997594	11109.078949	27.568756
250.213767	11132.294581	27.573773
250.381061	11136.240630	27.578791
250.697532	11154.833613	27.583808
250.683061	11180.216830	27.588826
251.244448	11185.859952	27.593844
251.334491	11214.018184	27.598861
251.527113	11226.789023	27.603879
251.535347	11238.853027	27.608896
252.161605	11259.172177	27.613914
252.158819	11271.452647	27.618932
252.444406	11301.114991	27.623949
252.969743	11312.545449	27.628967
252.590447	11327.752081	27.633984
253.114222	11350.225114	27.639002
253.485266	11364.941631	27.644020
253.827457	11385.592764	27.649037
254.000524	11420.789356	27.654055
254.508283	11425.237881	27.659072
254.741550	11442.944249	27.664090
255.346187	11457.106388	27.669108
255.224998	11477.268146	27.674125
255.464756	11487.985606	27.679143
256.124879	11505.429389	27.684160
256.035570	11518.099339	27.689178
256.473823	11532.985447	27.694196
256.305511	11551.544248	27.699213
256.944368	11575.152078	27.704231
256.816083	11588.538661	27.709248
256.946691	11597.833373	27.714266
257.393215	11626.991051	27.719284
257.750033	11641.081631	27.724301
258.366953	11659.151235	27.729319
258.100075	11661.526559	27.734336
258.359941	11690.445171	27.739354
258.757394	11709.063910	27.744372
258.926074	11730.367831	27.749389
259.069433	11747.968578	27.754407
259.384987	11757.941727	27.759424
259.347926	11786.354398	27.764442
259.795856	11812.070219	27.769460
260.295756	11832.267687	27.774477
260.353078	11850.137783	27.779495
260.438821	11864.656240	27.784512
260.848078	11883.424874	27.789530
261.182066	11895.905615	27.794548
261.860874	11924.800009	27.799565
262.257410	11939.276152	27.804583
261.994078	11942.680383	27.809600
262.041924	11968.380149	27.814618
262.502076	11982.502164	27.819636
262.460029	12001.417400	27.824653
263.222774	12017.566691	27.829671
263.321063	12027.321396	27.834688
263.390931	12049.844267	27.839706
264.081827	12065.490137	27.844724
263.945795	12082.165527	27.849741
264.306549	12102.530340	27.854759
264.799788	12107.830746	27.859776
265.330375	12140.926437	27.864794
265.649995	12150.062344	27.869812
265.490189	12177.054880	27.874829
265.618566	12186.116555	27.879847
266.216653	12197.400373	27.884864
265.934269	12217.073451	27.889882
266.421789	12234.036546	27.894900
266.706151	12261.272245	27.899917
267.016022	12273.008614	27.904935
267.693639	12284.431601	27.909952
267.584956	12314.870970	27.914970
268.143809	12319.693802	27.919988
268.287445	12350.876841	27.925005
268.085173	12362.447184	27.930023
268.540019	12381.648111	27.935040
268.441323	12402.170483	27.940058
268.987810	12423.169692	27.945076
269.381782	12450.293758	27.950093
269.494250	12475.560940	27.955111
270.132409	12491.884890	27.960128
270.140225	12515.059079	27.965146
270.585679	12539.787875	27.970164
270.507312	12558.377783	27.975181
270.751751	12579.885530	27.980199
271.380386	12595.367913	27.985216
271.386580	12627.135038	27.990234
271.785209	12644.314531	27.995252
272.077451	12666.506462	28.000269
272.887719	12686.542544	28.005287
273.132105	12701.958893	28.010304
273.017475	12724.603047	28.015322
273.521552	12739.940852	28.020340
273.493938	12762.937736	28.025357
273.735614	12781.420886	28.030375
274.383643	12787.022501	28.035392
274.356365	12812.769919	28.040410
274.344648	12833.285448	28.045428
274.969166	12852.959225	28.050445
275.471154	12874.199593	28.055463
275.676733	12894.485358	28.060480
275.944200	12924.301516	28.065498
276.152978	12929.419348	28.070516
276.517013	12953.754069	28.075533
276.518488	12977.842456	28.080551
277.216834	12990.241583	28.085568
277.134524	13008.153595	28.090586
277.718203	13019.013843	28.095604
277.899936	13053.403690	28.100621
277.884732	13065.273582	28.105639
278.485935	13081.745940	28.110656
278.845840	13106.220455	28.115674
279.137412	13112.228539	28.120692
279.287210	13137.525494	28.125709
279.450019	13160.767773	28.130727
279.923702	13160.538804	28.135744
279.889927	13185.371938	28.140762
280.277830	13203.497850	28.145780
280.368792	13215.941744	28.150797
280.308915	13238.628462	28.155815
281.050095	13252.906360	28.160832
281.187849	13278.328551	28.165850
281.278188	13298.654907	28.170868
281.592246	13312.766068	28.175885
281.897948	13333.747166	28.180903
282.523063	13352.492923	28.185920
282.489529	13382.619066	28.190938
282.534992	13405.393696	28.195956
283.129999	13422.306284	28.200973
283.138641	13445.756226	28.205991
283.645579	13469.336567	28.211008
283.916998	13491.059025	28.216026
284.211299	13508.100904	28.221044
284.916020	13536.696854	28.226061
285.070218	13556.842951	28.231079
285.340468	13575.129760	28.236096
285.775236	13602.902799	28.241114
285.844546	13623.564391	28.246132
286.077909	13639.662207	28.251149
286.205109	13657.314633	28.256167
286.631820	13680.449889	28.261184
287.156466	13699.874917	28.266202
287.311974	13720.185200	28.271220
287.354512	13747.100900	28.276237
287.549191	13763.751225	28.281255
288.259395	13782.048267	28.286272
288.219262	13802.689300	28.291290
288.799950	13827.092263	28.296308
289.173681	13854.341518	28.301325
288.992601	13877.408004	28.306343
289.689253	13900.138064	28.311360
289.810814	13913.022910	28.316378
289.843240	13945.186049	28.321396
290.458928	13966.147709	28.326413
290.630495	13993.719377	28.331431
291.123849	14013.910730	28.336448
291.422491	14037.916012	28.341466
291.462841	14058.083632	28.346484
292.296445	14083.189460	28.351501
292.539100	14098.910395	28.356519
292.732231	14123.374448	28.361536
293.120511	14150.858708	28.366554
293.159821	14160.266884	28.371572
293.497180	14187.948661	28.376589
293.480512	14201.246964	28.381607
293.992143	14220.207161	28.386624
294.018194	14246.933504	28.391642
294.534871	14272.922977	28.396660
295.020986	14289.850240	28.401677
294.967930	14321.784227	28.406695
295.369705	14334.056997	28.411712
295.252802	14357.584574	28.416730
295.713705	14396.262949	28.421748
296.478314	14413.667794	28.426765
296.474630	14445.294227	28.431783
297.126269	14464.804365	28.436800
297.126508	14486.873625	28.441818
297.420974	14505.555465	28.446836
297.739632	14528.711838	28.451853
297.730100	14558.125488	28.456871
298.413175	14576.831795	28.461888
298.814567	14608.505582	28.466906
298.994727	14627.467578	28.471924
299.573425	14641.579329	28.476941
299.410998	14659.423329	28.481959
300.073025	14678.720460	28.486976
300.184390	14694.891969	28.491994
300.065640	14725.103062	28.497012
300.581283	14739.073168	28.502029
300.890062	14770.869111	28.507047
301.271263	14787.295303	28.512064
301.568084	14805.774942	28.517082
302.059447	14843.700953	28.522100
302.267060	14856.771927	28.527117
302.181135	14877.828707	28.532135
303.047810	14901.303942	28.537152
303.124343	14925.082999	28.542170
303.094406	14948.225006	28.547188
303.560443	14969.400711	28.552205
303.961954	14995.080751	28.557223
304.021717	15021.370213	28.562240
304.549012	15045.227248	28.567258
304.994075	15065.556770	28.572276
305.387849	15088.525193	28.577293
305.682299	15110.905970	28.582311
305.974943	15130.049816	28.587328
306.420148	15154.380955	28.592346
306.466694	15171.153621	28.597364
306.999810	15193.869787	28.602381
307.258833	15225.045779	28.607399
307.524735	15243.533843	28.612416
307.514282	15267.513292	28.617434
307.926110	15285.631125	28.622452
308.303647	15310.911081	28.627469
308.887355	15340.956258	28.632487
308.890700	15361.952211	28.637504
309.196530	15383.412453	28.642522
309.664680	15408.738353	28.647540
310.197039	15433.201478	28.652557
310.353562	15460.082785	28.657575
310.486392	15476.567426	28.662592
310.897281	15509.204511	28.667610
311.036082	15525.732475	28.672628
311.531560	15552.270248	28.677645
311.777524	15584.108965	28.682663
312.138876	15598.760809	28.687680
312.812338	15626.739441	28.692698
312.858816	15646.004482	28.697716
313.315803	15673.559130	28.702733
313.506272	15698.900485	28.707751
313.753712	15708.317878	28.712768
314.471478	15732.452297	28.717786
314.236155	15762.515889	28.722804
314.948577	15784.073967	28.727821
315.334137	15812.385383	28.732839
315.596849	15824.864084	28.737856
315.646852	15846.282800	28.742874
315.459700	15882.090481	28.747892
316.453156	15896.965695	28.752909
316.300380	15928.223128	28.757927
316.960605	15945.468854	28.762944
317.444134	15979.886184	28.767962
317.308271	15999.360171	28.772980
318.158967	16037.172247	28.777997
318.100991	16046.833471	28.783015
318.232478	16069.654650	28.788032
318.654909	16103.639590	28.793050
318.668818	16131.760177	28.798068
319.606810	16151.015569	28.803085
319.574523	16173.932011	28.808103
320.215920	16201.891239	28.813120
320.425220	16223.184351	28.818138
320.655365	16246.236645	28.823156
321.532060	16264.614224	28.828173
321.428978	16279.089820	28.833191
321.846512	16296.560229	28.838208
322.484966	16323.143000	28.843226
322.500398	16344.791938	28.848244
322.692806	16364.347528	28.853261
323.162103	16387.450968	28.858279
323.356209	16404.896463	28.863296
323.482740	16419.017188	28.868314
323.433420	16447.748255	28.873332
324.447068	16470.482259	28.878349
324.534910	16481.722220	28.883367
324.661292	16516.474403	28.888384
325.164448	16545.280157	28.893402
325.377873	16576.743434	28.898420
325.891624	16589.713940	28.903437
326.201660	16620.369366	28.908455
326.525304	16639.863618	28.913472
326.861954	16660.098108	28.918490
326.870527	16688.618318	28.923508
327.174896	16714.773865	28.928525
327.575030	16746.950430	28.933543
327.955922	16776.732722	28.938560
328.350687	16796.749788	28.943578
328.694658	16832.100166	28.948596
329.027621	16861.858512	28.953613
329.347063	16880.134458	28.958631
329.432293	16909.230480	28.963648
329.967308	16940.909296	28.968666
330.212821	16964.926567	28.973684
330.766271	16986.709890	28.978701
331.011303	17016.400124	28.983719
331.185803	17049.316904	28.988736
331.771594	17074.487594	28.993754
332.199996	17105.798032	28.998772
332.467318	17125.800657	29.003789
333.162335	17153.626525	29.008807
333.192929	17183.053696	29.013824
333.725196	17203.128610	29.018842
333.683768	17226.774216	29.023860
334.141607	17252.729569	29.028877
334.465700	17280.556867	29.033895
334.943037	17303.691732	29.038912
334.818886	17325.189908	29.043930
335.292343	17355.659811	29.048948
335.785635	17388.198732	29.053965
336.169931	17419.984068	29.058983
336.536444	17446.882633	29.064000
336.722348	17474.125392	29.069018
336.951402	17506.251055	29.074036
337.526780	17528.953887	29.079053
337.858905	17559.136700	29.084071
337.868488	17590.134485	29.089088
338.598864	17615.990778	29.094106
339.170265	17649.440241	29.099124
339.141620	17669.350807	29.104141
339.549056	17685.263660	29.109159
340.060479	17718.166705	29.114176
339.974286	17741.011321	29.119194
340.612016	17771.096054	29.124212
341.119663	17795.717674	29.129229
341.129713	17818.717876	29.134247
341.288572	17845.693745	29.139264
342.043700	17876.442537	29.144282
342.389138	17909.125525	29.149300
342.563120	17927.690581	29.154317
343.038275	17954.376991	29.159335
343.448848	17988.648235	29.164352
343.613342	18000.290868	29.169370
343.805115	18029.510867	29.174388
344.052758	18050.376713	29.179405
344.539064	18071.679011	29.184423
345.012835	18107.778966	29.189440
345.389562	18120.064403	29.194458
345.823449	18156.094886	29.199476
346.291978	18169.079858	29.204493
346.588897	18197.784553	29.209511
346.504401	18225.152851	29.214528
347.393799	18234.849977	29.219546
347.599487	18266.001333	29.224564
347.929863	18280.669546	29.229581
348.383634	18305.199171	29.234599
348.190698	18329.823810	29.239616
348.942029	18353.454008	29.244634
349.195672	18387.592598	29.249652
349.403456	18411.131115	29.254669
349.775845	18433.822582	29.259687
350.070960	18470.001737	29.264704
350.484523	18495.542408	29.269722
350.662156	18522.446780	29.274740
350.968023	18555.320267	29.279757
351.277074	18581.395471	29.284775
351.598536	18620.969699	29.289792
352.150516	18657.165826	29.294810
352.282459	18679.339284	29.299828
352.690518	18716.328827	29.304845
353.380943	18741.504248	29.309863
353.654287	18772.216209	29.314880
353.688930	18792.699244	29.319898
353.772626	18840.303130	29.324916
354.407955	18873.144499	29.329933
354.864956	18890.389948	29.334951
355.152582	18936.426902	29.339968
356.112596	18963.809522	29.344986
356.100078	19001.339322	29.350004
356.415630	19022.353518	29.355021
356.955455	19050.136924	29.360039
356.843639	19090.392804	29.365056
357.272526	19120.638699	29.370074
357.819231	19154.789588	29.375092
358.397823	19183.609561	29.380109
358.780809	19206.123368	29.385127
358.964352	19235.567592	29.390144
359.511398	19262.623611	29.395162
359.585926	19288.325832	29.400180
360.051909	19318.888438	29.405197
360.757979	19344.510762	29.410215
361.335097	19386.788483	29.415232
361.190831	19409.094487	29.420250
361.960277	19439.843512	29.425268
362.066009	19458.155363	29.430285
362.729949	19491.416597	29.435303
362.950377	19527.375646	29.440320
363.387441	19548.788363	29.445338
363.636223	19579.846614	29.450356
363.925912	19600.378997	29.455373
364.284177	19625.474913	29.460391
364.406397	19666.472435	29.465408
364.991906	19687.065978	29.470426
365.294914	19717.357787	29.475444
365.469024	19743.202959	29.480461
366.109464	19767.616733	29.485479
366.003681	19800.506251	29.490496
366.878826	19833.545442	29.495514
367.289778	19859.890707	29.500532
367.569605	19887.311672	29.505549
367.764717	19908.194052	29.510567
367.772434	19936.295839	29.515584
368.282840	19957.906015	29.520602
368.797565	19998.495252	29.525620
369.201442	20028.936015	29.530637
369.631951	20041.012060	29.535655
369.762061	20084.220577	29.540672
369.758757	20107.389839	29.545690
370.560857	20139.695443	29.550708
370.729520	20177.729843	29.555725
371.220336	20203.639741	29.560743
371.730929	20231.530498	29.565760
372.157918	20250.443545	29.570778
372.353342	20284.626158	29.575796
372.727719	20320.777368	29.580813
373.275702	20355.890529	29.585831
373.542230	20394.516573	29.590848
373.997664	20416.489689	29.595866
374.258231	20452.696879	29.600884
374.596010	20490.547437	29.605901
374.727875	20518.049324	29.610919
375.135002	20552.294017	29.615936
375.487915	20581.075580	29.620954
376.051204	20621.987054	29.625972
376.129402	20655.992806	29.630989
377.192576	20686.438729	29.636007
377.387068	20720.571699	29.641024
377.303526	20752.429429	29.646042
378.128768	20779.835710	29.651060
377.996631	20814.898263	29.656077
379.015814	20850.494520	29.661095
379.296406	20888.841321	29.666112
379.487189	20918.192159	29.671130
380.106867	20950.186476	29.676148
380.311761	20992.210040	29.681165
380.772431	21024.084059	29.686183
381.096729	21071.579848	29.691200
381.858059	21096.033208	29.696218
382.244640	21120.020862	29.701236
382.233303	21150.907511	29.706253
383.076106	21186.911117	29.711271
383.512746	21222.327599	29.716288
383.506262	21251.216986	29.721306
384.337421	21274.339052	29.726324
384.592780	21312.854913	29.731341
385.260431	21346.352499	29.736359
385.498211	21370.787110	29.741376
385.701754	21390.905195	29.746394
386.449310	21419.177547	29.751412
386.344949	21441.713390	29.756429
387.019466	21470.268956	29.761447
386.973816	21510.904860	29.766464
387.487797	21532.749999	29.771482
388.144189	21575.083201	29.776500
388.480076	21607.565344	29.781517
388.912126	21622.213820	29.786535
388.886438	21661.892788	29.791552
389.530806	21689.745702	29.796570
390.286263	21721.732642	29.801588
390.325215	21752.884058	29.806605
390.651429	21783.737779	29.811623
391.071499	21813.793324	29.816640
391.597995	21841.033041	29.821658
391.714895	21864.450925	29.826676
392.098355	21907.781721	29.831693
392.488256	21937.804267	29.836711
392.617690	21971.482000	29.841728
393.106914	22000.907756	29.846746
393.683681	22034.458659	29.851764
393.899080	22064.925772	29.856781
394.433481	22094.572068	29.861799
394.486436	22135.832009	29.866816
395.187331	22161.364041	29.871834
395.645664	22189.638569	29.876852
395.738743	22219.809137	29.881869
396.396724	22255.812049	29.886887
396.789391	22279.035574	29.891904
397.187039	22307.288181	29.896922
397.709378	22332.387124	29.901940
397.669813	22374.767859	29.906957
398.507332	22411.204213	29.911975
398.996968	22444.548296	29.916992
398.971258	22473.777379	29.922010
399.759326	22506.354462	29.927028
399.712335	22548.382869	29.932045
400.175868	22581.055141	29.937063
400.630681	22614.038463	29.942080
401.128163	22637.056420	29.947098
401.206571	22668.525361	29.952116
401.648299	22716.335289	29.957133
402.063088	22751.650508	29.962151
402.682422	22793.265430	29.967168
402.807593	22830.774628	29.972186
403.327143	22864.696084	29.977204
403.719223	22908.609069	29.982221
404.058646	22940.713698	29.987239
404.347082	22977.584647	29.992256
404.788517	23013.578620	29.997274
405.574374	23054.479222	30.002292
405.862170	23100.987170	30.007309
406.435256	23127.848530	30.012327
406.771632	23167.555939	30.017344
406.804975	23207.152914	30.022362
407.721114	23239.957588	30.027380
407.998216	23287.946336	30.032397
408.639095	23321.198689	30.037415
408.721800	23361.211624	30.042432
409.110700	23389.024793	30.047450
409.634286	23428.400076	30.052468
410.216667	23468.815223	30.057485
410.376832	23503.154257	30.062503
410.621167	23544.096451	30.067520
411.240928	23582.774492	30.072538
411.850614	23617.409831	30.077556
411.788106	23653.427020	30.082573
412.098198	23705.253747	30.087591
412.803758	23726.944910	30.092608
413.275329	23768.231131	30.097626
414.121120	23811.392548	30.102644
414.262253	23847.188608	30.107661
414.897486	23887.280355	30.112679
415.134418	23914.347094	30.117696
415.206832	23957.604686	30.122714
415.957470	23990.019438	30.127732
416.334475	24029.020741	30.132749
416.312885	24066.068650	30.137767
417.041928	24108.705523	30.142784
417.794578	24147.389120	30.147802
418.072567	24181.003082	30.152820
417.985435	24222.794838	30.157837
418.749995	24257.154248	30.162855
419.573562	24297.489058	30.167872
420.062825	24336.403861	30.172890
420.516329	24357.117747	30.177908
420.569543	24400.663681	30.182925
421.196212	24422.810327	30.187943
421.634938	24454.882877	30.192960
422.073633	24490.873622	30.197978
422.722876	24517.775482	30.202996
422.897885	24541.724572	30.208013
423.138840	24573.828290	30.213031
424.068951	24609.047118	30.218048
423.972821	24629.215415	30.223066
424.086112	24663.108766	30.228084
424.422276	24696.240506	30.233101
424.706755	24745.590316	30.238119
425.333853	24778.897810	30.243136
425.689952	24826.985307	30.248154
425.981059	24859.226978	30.253172
426.689602	24902.683994	30.258189
427.122296	24931.427764	30.263207
427.365652	24981.226973	30.268224
427.910863	25023.073021	30.273242
428.084127	25047.951991	30.278260
428.532221	25088.517837	30.283277
429.470071	25133.582575	30.288295
429.736223	25166.921970	30.293312
429.953115	25222.116703	30.298330
430.692510	25253.366097	30.303348
430.802608	25296.437393	30.308365
430.965831	25340.119805	30.313383
431.556976	25381.561253	30.318400
431.812661	25424.489942	30.323418
432.591135	25470.111266	30.328436
433.245251	25505.760412	30.333453
433.638032	25544.547310	30.338471
434.124085	25593.172433	30.343488
434.435176	25635.372421	30.348506
434.856763	25673.946497	30.353524
435.241238	25712.008224	30.358541
435.881767	25754.719337	30.363559
436.488290	25793.062436	30.368576
436.456700	25832.333475	30.373594
437.288474	25875.476249	30.378612
437.504474	25913.627944	30.383629
437.933335	25957.586086	30.388647
438.583924	25999.897980	30.393664
439.044264	26039.155570	30.398682
439.434568	26075.213607	30.403700
439.936420	26120.968213	30.408717
440.182411	26155.468975	30.413735
441.195107	26190.810363	30.418752
441.223528	26233.416120	30.423770
441.784843	26270.762307	30.428788
441.992599	26318.990357	30.433805
442.299056	26358.278990	30.438823
443.107887	26397.887182	30.443840
443.426641	26438.071508	30.448858
443.951918	26472.977800	30.453876
444.347183	26523.123588	30.458893
444.801142	26557.181646	30.463911
445.464794	26599.973086	30.468928
445.981087	26646.434484	30.473946
446.474112	26681.826527	30.478964
446.842522	26710.089920	30.483981
447.298941	26755.088321	30.488999
448.014880	26786.274242	30.494016
448.314520	26818.871641	30.499034
448.455258	26852.302982	30.504052
448.916893	26890.304276	30.509069
449.565244	26928.605054	30.514087
450.189205	26963.218639	30.519104
450.167350	27006.149909	30.524122
450.688983	27039.174278	30.529140
451.299704	27078.214395	30.534157
452.069351	27109.316557	30.539175
452.402097	27132.043136	30.544192
452.866503	27167.307780	30.549210
453.003120	27199.564740	30.554228
453.218185	27231.916911	30.559245
453.543753	27264.719539	30.564263
454.321701	27295.087514	30.569280
454.581744	27336.862928	30.574298
454.923908	27372.248201	30.579316
455.487565	27418.059256	30.584333
455.501678	27452.023376	30.589351
456.329630	27491.630711	30.594368
456.461202	27545.334529	30.599386
456.933275	27584.561669	30.604404
457.444608	27635.014368	30.609421
457.614651	27679.459216	30.614439
458.301167	27726.092357	30.619456
458.851180	27773.726679	30.624474
459.318988	27810.786955	30.629492
459.540104	27868.105631	30.634509
459.620393	27916.863083	30.639527
460.633940	27969.134141	30.644544
460.743051	28015.934231	30.649562
461.564638	28065.321770	30.654580
461.810272	28116.019535	30.659597
461.904197	28168.561556	30.664615
462.761706	28208.228862	30.669632
463.179639	28264.740371	30.674650
463.495669	28306.591170	30.679668
464.209771	28359.997302	30.684685
464.891486	28417.782641	30.689703
465.399814	28454.369999	30.694720
465.905048	28510.855872	30.699738
466.332089	28556.020870	30.704756
466.914056	28597.843253	30.709773
467.254580	28651.548851	30.714791
467.748166	28685.932947	30.719808
468.060404	28749.946278	30.724826
468.898207	28791.172744	30.729844
469.490134	28837.937014	30.734861
470.157348	28881.497521	30.739879
470.520381	28924.682260	30.744896
470.746728	28968.141337	30.749914
471.257854	29004.735561	30.754932
471.962744	29048.138818	30.759949
472.187252	29102.135569	30.764967
473.012551	29148.269819	30.769984
473.076109	29197.089824	30.775002
473.549296	29237.388214	30.780020
473.816484	29280.784666	30.785037
474.692435	29330.160420	30.790055
475.088680	29364.345982	30.795072
475.188076	29427.813220	30.800090
475.855018	29470.888294	30.805108
476.343118	29510.293605	30.810125
477.110659	29561.026975	30.815143
477.790586	29604.922046	30.820160
477.814306	29655.664691	30.825178
478.333831	29705.704006	30.830196
479.039176	29749.323593	30.835213
479.064662	29795.464464	30.840231
479.502615	29836.433274	30.845248
479.940772	29890.063602	30.850266
480.142674	29935.740988	30.855284
480.935124	29982.741947	30.860301
481.638636	30032.190643	30.865319
482.329109	30065.952008	30.870336
483.046728	30115.044700	30.875354
483.480296	30146.596044	30.880372
484.044808	30191.306930	30.885389
484.311359	30228.295631	30.890407
484.623894	30263.930745	30.895424
484.951990	30312.143031	30.900442
485.205603	30359.159709	30.905460
485.811487	30404.680036	30.910477
486.373479	30453.159444	30.915495
486.921536	30499.953324	30.920512
487.571983	30540.972429	30.925530
488.051210	30582.979295	30.930548
488.363504	30626.605405	30.935565
488.534859	30670.632971	30.940583
489.500753	30710.781212	30.945600
489.476554	30760.756526	30.950618
489.773163	30826.118908	30.955636
490.950460	30872.126027	30.960653
491.425651	30920.936203	30.965671
491.905015	30967.830401	30.970688
492.015801	31017.538650	30.975706
492.405168	31066.628118	30.980724
493.519789	31117.627030	30.985741
493.763760	31170.671570	30.990759
494.176929	31207.082750	30.995776
494.651049	31274.334201	31.000794
494.985333	31327.131093	31.005812
495.618760	31374.615283	31.010829
496.110773	31423.013094	31.015847
496.795414	31473.473341	31.020864
497.156742	31531.747462	31.025882
497.636219	31583.801584	31.030900
498.374333	31639.798053	31.035917
498.500052	31679.144137	31.040935
499.240312	31727.427913	31.045952
500.192963	31775.109570	31.050970
500.134086	31827.387701	31.055988
500.557410	31873.938696	31.061005
501.086124	31936.366480	31.066023
501.792003	31985.952224	31.071040
502.256343	32032.313814	31.076058
502.796812	32092.666640	31.081076
503.609286	32145.662552	31.086093
503.729550	32189.713976	31.091111
504.258208	32238.778069	31.096128
505.030185	32295.871019	31.101146
505.545530	32349.286983	31.106164
505.791572	32394.153642	31.111181
506.403667	32445.386248	31.116199
507.019734	32494.892438	31.121216
507.249248	32550.111211	31.126234
508.020809	32601.850276	31.131252
508.630178	32646.553096	31.136269
509.177686	32704.219697	31.141287
509.665173	32751.887934	31.146304
510.123583	32793.655958	31.151322
510.470292	32849.729620	31.156340
511.389359	32896.780565	31.161357
511.386466	32943.780028	31.166375
511.907335	33009.322756	31.171392
512.535729	33044.280937	31.176410
512.944110	33103.424535	31.181428
513.362608	33155.188654	31.186445
513.824055	33212.326418	31.191463
514.555961	33263.731927	31.196480
515.645645	33320.954937	31.201498
515.799965	33362.044657	31.206516
516.503144	33398.717706	31.211533
516.691544	33448.350032	31.216551
517.306828	33488.564865	31.221568
517.862477	33522.719655	31.226586
518.317468	33576.508573	31.231604
518.649117	33619.455089	31.236621
518.893004	33672.954874	31.241639
519.446265	33728.606542	31.246656
519.907935	33787.901779	31.251674
520.128907	33834.956683	31.256692
521.343573	33893.173269	31.261709
521.448319	33937.863037	31.266727
521.854122	33992.134906	31.271744
522.411675	34035.363013	31.276762
522.981087	34090.659047	31.281780
523.753243	34145.626312	31.286797
524.318438	34211.292293	31.291815
524.237662	34257.010757	31.296832
525.347863	34323.451597	31.301850
525.598074	34378.893219	31.306868
526.411027	34433.279486	31.311885
526.986867	34488.385876	31.316903
527.525775	34533.584266	31.321920
528.156801	34586.526243	31.326938
528.396175	34642.653102	31.331956
529.270007	34690.151411	31.336973
529.641444	34751.695400	31.341991
530.185473	34816.664754	31.347008
530.773930	34863.487355	31.352026
531.038339	34926.117160	31.357044
531.697145	34975.590879	31.362061
532.108605	35031.451549	31.367079
532.532879	35090.610872	31.372096
533.364587	35143.118149	31.377114
533.704143	35207.589607	31.382132
534.394817	35251.842623	31.387149
534.807673	35311.567086	31.392167
535.284914	35379.653162	31.397184
535.886230	35428.005141	31.402202
536.104207	35499.091334	31.407220
537.230581	35547.045201	31.412237
537.820108	35606.559457	31.417255
538.396751	35668.276300	31.422272
538.992069	35723.073021	31.427290
539.527217	35775.862262	31.432308
540.161219	35832.151763	31.437325
540.720352	35883.476891	31.442343
541.048397	35950.431041	31.447360
541.710881	35994.550912	31.452378
542.142790	36052.415481	31.457396
543.192093	36094.091163	31.462413
543.331207	36158.786587	31.467431
543.582939	36218.096208	31.472448
544.030266	36248.560671	31.477466
544.788184	36322.543256	31.482484
545.291663	36366.922758	31.487501
546.096782	36433.297848	31.492519
546.287007	36491.131903	31.497536
547.211175	36537.127853	31.502554
547.483407	36603.447820	31.507572
548.139510	36653.520252	31.512589
548.913658	36710.934637	31.517607
549.120854	36772.548130	31.522624
549.963746	36826.196006	31.527642
550.558659	36885.523286	31.532660
551.367365	36936.198491	31.537677
551.889680	36990.301682	31.542695
552.129276	37032.978642	31.547712
553.041351	37079.647934	31.552730
553.258129	37131.965546	31.557748
554.055272	37174.719874	31.562765
554.192925	37226.499970	31.567783
554.669100	37285.252548	31.572800
555.060024	37325.718467	31.577818
555.485482	37381.121481	31.582836
555.787940	37432.876262	31.587853
556.203957	37490.020001	31.592871
556.916460	37559.789855	31.597888
557.787209	37622.085982	31.602906
558.345682	37677.627017	31.607924
558.883994	37736.206683	31.612941
558.981735	37793.242985	31.617959
559.556037	37853.992660	31.622976
560.180841	37915.961387	31.627994
560.386622	37983.434280	31.633012
561.478981	38045.285887	31.638029
562.033221	38109.315099	31.643047
562.424863	38174.950899	31.648064
563.358930	38226.387336	31.653082
563.786110	38292.530152	31.658100
564.691326	38351.964651	31.663117
564.947527	38417.616079	31.668135
565.335711	38489.109219	31.673152
565.909035	38543.499223	31.678170
566.502413	38620.361222	31.683188
567.363587	38674.896190	31.688205
568.036168	38742.304668	31.693223
568.655173	38804.359064	31.698240
569.635929	38862.562622	31.703258
569.987385	38915.382030	31.708276
570.268717	38986.722803	31.713293
571.166032	39045.091695	31.718311
571.469861	39108.303021	31.723328
572.051502	39161.314642	31.728346
572.838640	39222.958140	31.733364
573.295756	39285.425035	31.738381
574.163628	39344.204085	31.743399
574.594440	39409.350540	31.748416
575.433196	39462.721047	31.753434
575.462736	39528.879322	31.758452
576.394472	39590.469597	31.763469
577.154675	39644.940608	31.768487
577.454618	39709.944032	31.773504
578.002876	39759.035024	31.778522
578.638884	39823.372707	31.783540
579.060168	39871.807149	31.788557
579.612935	39936.322632	31.793575
579.957723	40006.803041	31.798592
580.453431	40073.136605	31.803610
581.159081	40136.446096	31.808628
581.810039	40212.912607	31.813645
582.506570	40273.466517	31.818663
583.159854	40341.863254	31.823680
583.648291	40395.537565	31.828698
584.226559	40467.804317	31.833716
584.974950	40521.318062	31.838733
585.965571	40586.544797	31.843751
585.974032	40648.358556	31.848768
587.026657	40717.971468	31.853786
587.440477	40776.015961	31.858804
587.571714	40834.041620	31.863821
588.411058	40901.361101	31.868839
588.892417	40962.361714	31.873856
589.530031	41019.492692	31.878874
590.234395	41076.442602	31.883892
590.854200	41147.338984	31.888909
591.321579	41208.665026	31.893927
591.714108	41263.659358	31.898944
592.668921	41322.986694	31.903962
593.141295	41376.476186	31.908980
593.678563	41438.639430	31.913997
594.152647	41500.502835	31.919015
594.947687	41557.680133	31.924032
595.537855	41617.153918	31.929050
596.179273	41673.153877	31.934068
596.564789	41735.335401	31.939085
597.301728	41794.065656	31.944103
597.691827	41852.445600	31.949120
598.219489	41910.057827	31.954138
598.708900	41982.444682	31.959156
599.186201	42045.403312	31.964173
599.904960	42112.435474	31.969191
600.410179	42187.938692	31.974208
601.329258	42238.659591	31.979226
601.770497	42314.812079	31.984244
601.805496	42387.859649	31.989261
602.681213	42449.871544	31.994279
603.484364	42521.983335	31.999296
604.268175	42599.986977	32.004314
604.699632	42668.495275	32.009332
605.293486	42736.092846	32.014349
606.050086	42802.729024	32.019367
606.574348	42887.554806	32.024384
607.249608	42947.758889	32.029402
608.111431	43017.244510	32.034420
608.576357	43084.641956	32.039437
609.372920	43150.260898	32.044455
609.962650	43217.993414	32.049472
610.400852	43287.615804	32.054490
610.897998	43361.321604	32.059508
611.460472	43423.556066	32.064525
612.036871	43484.738528	32.069543
612.727208	43569.705365	32.074560
613.712854	43634.252453	32.079578
613.847289	43707.579760	32.084596
614.505400	43786.486483	32.089613
615.623867	43846.933537	32.094631
615.895034	43926.325155	32.099648
616.585410	43988.737255	32.104666
617.449003	44057.346623	32.109684
618.042057	44134.133097	32.114701
619.203897	44196.838821	32.119719
619.436676	44268.558553	32.124736
619.953784	44337.760713	32.129754
620.769334	44403.880096	32.134772
620.890075	44475.023438	32.139789
621.880991	44538.338841	32.144807
622.361672	44604.738983	32.149824
623.232652	44672.349643	32.154842
623.876593	44737.864330	32.159860
624.358332	44808.591636	32.164877
624.944742	44878.347599	32.169895
625.362028	44942.715484	32.174912
626.333047	45020.578107	32.179930
626.953491	45090.664663	32.184948
627.276010	45153.782851	32.189965
628.083219	45213.067812	32.194983
628.619943	45288.323587	32.200000
629.359226	45356.349136	32.205018
629.911769	45427.200146	32.210036
630.450997	45501.317596	32.215053
631.360042	45567.052548	32.220071
631.812202	45632.663143	32.225088
632.917418	45702.030449	32.230106
633.410522	45764.440442	32.235124
633.551712	45824.078031	32.240141
634.415141	45876.669437	32.245159
635.211794	45949.843440	32.250176
635.448011	46004.013645	32.255194
636.104625	46071.712703	32.260212
636.545258	46138.965011	32.265229
637.666807	46196.090449	32.270247
637.920735	46263.511541	32.275264
638.757214	46329.740866	32.280282
639.313340	46396.058573	32.285300
639.088702	46467.445764	32.290317
640.257194	46529.979843	32.295335
640.886891	46607.597762	32.300352
641.435364	46695.451754	32.305370
642.051585	46764.228337	32.310388
642.786666	46841.197934	32.315405
643.279091	46908.235655	32.320423
644.275000	46991.181158	32.325440
644.905618	47065.915733	32.330458
645.333052	47143.744300	32.335476
645.727980	47216.479214	32.340493
646.800182	47294.586903	32.345511
647.299690	47367.849989	32.350528
647.984401	47445.905007	32.355546
648.825112	47520.272878	32.360564
649.309534	47599.492216	32.365581
650.195078	47667.824469	32.370599
650.402944	47755.584073	32.375616
651.265208	47832.106912	32.380634
652.011208	47906.611081	32.385652
652.813404	47981.290163	32.390669
653.435288	48059.831616	32.395687
654.052958	48149.591013	32.400704
654.794106	48216.884663	32.405722
655.534873	48296.521793	32.410740
655.890296	48369.412089	32.415757
656.968288	48446.137291	32.420775
657.352789	48519.839651	32.425792
657.969689	48595.517743	32.430810
658.885881	48682.183013	32.435828
659.179054	48760.803661	32.440845
659.858107	48833.973744	32.445863
660.575545	48918.716067	32.450880
660.962437	49001.163221	32.455898
661.952597	49072.216478	32.460916
662.511055	49161.248877	32.465933
663.433406	49238.216222	32.470951
663.995723	49326.185742	32.475968
664.421731	49406.103792	32.480986
665.526432	49478.614543	32.486004
666.443257	49567.522798	32.491021
667.188879	49645.911119	32.496039
667.389145	49702.816351	32.501056
668.109190	49794.413641	32.506074
668.910387	49857.299094	32.511092
669.481762	49946.699478	32.516109
670.711968	50014.206534	32.521127
671.163789	50093.566144	32.526144
671.546128	50169.298807	32.531162
672.461647	50242.012423	32.536180
672.984447	50324.588558	32.541197
673.779680	50392.797558	32.546215
674.423161	50466.889522	32.551232
675.011978	50545.887562	32.556250
675.740854	50624.174267	32.561268
675.845572	50692.504943	32.566285
676.857694	50760.326734	32.571303
677.604064	50842.236975	32.576320
678.084722	50912.850534	32.581338
678.780339	50982.842200	32.586356
679.192288	51068.437512	32.591373
679.996886	51136.413124	32.596391
680.827976	51215.527363	32.601408
681.336855	51295.546535	32.606426
682.154317	51355.396346	32.611444
682.658082	51433.429973	32.616461
683.408804	51512.260417	32.621479
683.904284	51602.368774	32.626496
684.380439	51671.941303	32.631514
685.149303	51762.538980	32.636532
686.059223	51841.870797	32.641549
686.486000	51926.150804	32.646567
687.071635	52013.095481	32.651584
687.797664	52100.822108	32.656602
688.750723	52179.895213	32.661620
689.298034	52266.087513	32.666637
690.342142	52352.651599	32.671655
690.714628	52433.164286	32.676672
691.252586	52527.781245	32.681690
692.858042	52604.450312	32.686708
693.143931	52684.249728	32.691725
693.499634	52767.246694	32.696743
694.017412	52859.995116	32.701760
695.252195	52954.922314	32.706778
695.943064	53028.755564	32.711796
696.691859	53119.488199	32.716813
697.190188	53200.970971	32.721831
698.136983	53278.517404	32.726848
698.515981	53363.841525	32.731866
699.360039	53458.370004	32.736884
699.936489	53547.258184	32.741901
700.656792	53639.250240	32.746919
701.619424	53715.612284	32.751936
702.259198	53809.117371	32.756954
702.929170	53891.771668	32.761972
703.431965	53976.154710	32.766989
704.213656	54065.069655	32.772007
704.902485	54164.928295	32.777024
705.671263	54245.366139	32.782042
706.578491	54339.299731	32.787060
707.109171	54426.053108	32.792077
708.015720	54521.145603	32.797095
709.087593	54596.360623	32.802112
710.007883	54692.514813	32.807130
710.687306	54772.196383	32.812148
710.888297	54856.496930	32.817165
711.895000	54934.906413	32.822183
712.564653	55015.697803	32.827200
713.060427	55106.458708	32.832218
714.185673	55180.509115	32.837236
714.362093	55282.648688	32.842253
715.345584	55362.050464	32.847271
715.948353	55446.878738	32.852288
716.502028	55542.606482	32.857306
717.430480	55629.162734	32.862324
717.930471	55707.869290	32.867341
718.614246	55793.065828	32.872359
719.729897	55874.151020	32.877376
720.146122	55961.902539	32.882394
721.124793	56040.712435	32.887412
721.980573	56135.604159	32.892429
722.581878	56212.682685	32.897447
723.288887	56296.915410	32.902464
723.831234	56391.110435	32.907482
724.623417	56474.235563	32.912500
725.082929	56550.077944	32.917517
725.990307	56644.552230	32.922535
726.858973	56708.787186	32.927552
727.207435	56793.539813	32.932570
727.790844	56866.977794	32.937588
728.433617	56954.248115	32.942605
729.108143	57029.925433	32.947623
730.109431	57115.292137	32.952640
730.592752	57206.607255	32.957658
731.552392	57295.708912	32.962676
732.492263	57378.244428	32.967693
732.803774	57469.998838	32.972711
733.797514	57549.912595	32.977728
733.599173	57655.171589	32.982746
734.677183	57737.079104	32.987764
735.785518	57831.710129	32.992781
736.121718	57936.519548	32.997799
736.985553	58026.170560	33.002816
737.819617	58132.902903	33.007834
738.938617	58221.685549	33.012852
739.442589	58320.868944	33.017869
740.400129	58410.620634	33.022887
740.673719	58503.600133	33.027904
741.314917	58607.415288	33.032922
742.380122	58697.436001	33.037940
743.096877	58790.866213	33.042957
743.773958	58891.145139	33.047975
745.045965	58989.318540	33.052992
745.526954	59085.381891	33.058010
746.013806	59177.659643	33.063028
746.932845	59287.637133	33.068045
747.623969	59377.022691	33.073063
748.854218	59465.450665	33.078080
749.132723	59562.788208	33.083098
749.948707	59651.952671	33.088116
751.229697	59765.496198	33.093133
751.659429	59858.994439	33.098151
752.642097	59951.178483	33.103168
753.534800	60055.118660	33.108186
754.526547	60150.403614	33.113204
755.093833	60232.886912	33.118221
755.889126	60318.651610	33.123239
756.711296	60418.458338	33.128256
757.251121	60516.834824	33.133274
757.948634	60606.394778	33.138292
758.873352	60694.412956	33.143309
759.473560	60799.895954	33.148327
760.227536	60890.460892	33.153344
760.854344	60990.376494	33.158362
761.726360	61085.360994	33.163380
762.156795	61184.586511	33.168397
762.966217	61279.486611	33.173415
764.237407	61378.277406	33.178432
764.516164	61483.959259	33.183450
765.149463	61571.139986	33.188468
766.059269	61677.686031	33.193485
766.776240	61775.811913	33.198503
767.710271	61876.189404	33.203520
768.445927	61986.087416	33.208538
768.925422	62078.193630	33.213556
770.105508	62176.489129	33.218573
770.423494	62279.895653	33.223591
771.731092	62374.842217	33.228608
772.065729	62472.416681	33.233626
773.041392	62580.336314	33.238644
773.924547	62680.623739	33.243661
774.360625	62780.854969	33.248679
775.275909	62874.396209	33.253696
775.935435	62970.991170	33.258714
776.987988	63055.617238	33.263732
777.555880	63156.987824	33.268749
777.995642	63254.162721	33.273767
779.340356	63341.497810	33.278784
779.742412	63446.725551	33.283802
780.466630	63532.829042	33.288820
781.318751	63631.751399	33.293837
781.724064	63737.340700	33.298855
782.924571	63835.512930	33.303872
783.264625	63945.899355	33.308890
784.070157	64038.044046	33.313908
784.637185	64140.760873	33.318925
785.683065	64248.277870	33.323943
786.654188	64362.853276	33.328960
787.399756	64471.969316	33.333978
788.163212	64563.767994	33.338996
788.995379	64666.198541	33.344013
789.606146	64781.883216	33.349031
790.568823	64888.934825	33.354048
791.145346	64992.445010	33.359066
791.931640	65105.115441	33.364084
792.979691	65216.099308	33.369101
793.530725	65331.124757	33.374119
794.419525	65439.209572	33.379136
795.413667	65547.753189	33.384154
796.351844	65661.383642	33.389172
796.905604	65776.556301	33.394189
797.528872	65894.333400	33.399207
798.407934	66002.194214	33.404224
799.577830	66112.890682	33.409242
800.103617	66224.378607	33.414260
800.994960	66324.869210	33.419277
801.772828	66443.751623	33.424295
803.150808	66549.023073	33.429312
803.825555	66659.159979	33.434330
804.471641	66772.980424	33.439348
805.617939	66874.731219	33.444365
806.220835	66980.100492	33.449383
807.252580	67089.961750	33.454400
807.856906	67200.206986	33.459418
808.656048	67309.649737	33.464436
809.976175	67412.280868	33.469453
810.674105	67514.300695	33.474471
811.602801	67621.305803	33.479488
812.254096	67732.919945	33.484506
813.268382	67832.276508	33.489524
814.319709	67937.389541	33.494541
814.997600	68039.180314	33.499559
815.903516	68143.291211	33.504576
816.642360	68242.071972	33.509594
817.222160	68334.482855	33.514612
818.322474	68438.235246	33.519629
818.826157	68543.404846	33.524647
819.956397	68637.541542	33.529664
820.305706	68745.883100	33.534682
821.594809	68852.792562	33.539700
822.187986	68957.968828	33.544717
822.847552	69065.997198	33.549735
823.774145	69165.746215	33.554752
824.588571	69274.808657	33.559770
825.613149	69386.770411	33.564788
826.203526	69482.121826	33.569805
826.514459	69584.406721	33.574823
827.655900	69711.175131	33.579840
828.933940	69797.396672	33.584858
829.571749	69914.651657	33.589876
830.436577	70010.525599	33.594893
830.667970	70116.529403	33.599911
831.599607	70212.710240	33.604928
832.437100	70310.907187	33.609946
833.010957	70417.884423	33.614964
834.088823	70523.377389	33.619981
834.736059	70633.408886	33.624999
835.808285	70726.593371	33.630016
836.790633	70834.724171	33.635034
837.483508	70943.635312	33.640052
838.420147	71040.185690	33.645069
838.936812	71157.712179	33.650087
839.919026	71264.426284	33.655104
841.108417	71377.453625	33.660122
841.557281	71472.638142	33.665140
842.769413	71575.403959	33.670157
843.354053	71693.935418	33.675175
844.251910	71798.144498	33.680192
845.285688	71907.386206	33.685210
845.629062	72016.977117	33.690228
846.918255	72125.356477	33.695245
847.488973	72249.440103	33.700263
848.638057	72351.750189	33.705280
849.092776	72468.316958	33.710298
849.694751	72584.848515	33.715316
851.102878	72695.377426	33.720333
851.977050	72813.121277	33.725351
852.518351	72925.674089	33.730368
853.438903	73038.674630	33.735386
854.418064	73152.515096	33.740404
855.172250	73265.150003	33.745421
856.003242	73389.451517	33.750439
856.820374	73497.264423	33.755456
857.730838	73615.462119	33.760474
858.370601	73739.757209	33.765492
859.313464	73854.986980	33.770509
860.143505	73981.229346	33.775527
861.312628	74097.286047	33.780544
861.828681	74218.752778	33.785562
862.643642	74342.554570	33.790580
863.696353	74469.093696	33.795597
864.588478	74598.711236	33.800615
865.612089	74716.503402	33.805632
866.653419	74831.924618	33.810650
867.330686	74955.548122	33.815668
868.486449	75072.231802	33.820685
869.465729	75196.303130	33.825703
870.352239	75312.738670	33.830720
871.265372	75421.874306	33.835738
871.933777	75546.084586	33.840756
872.851447	75657.323205	33.845773
873.244310	75774.522056	33.850791
873.933889	75905.342967	33.855808
875.674101	76020.102464	33.860826
876.172037	76148.699766	33.865844
877.406403	76267.998447	33.870861
878.292782	76395.510029	33.875879
879.077528	76509.914502	33.880896
879.945962	76622.241526	33.885914
881.001190	76740.518915	33.890932
882.057738	76862.178897	33.895949
882.382162	76971.615621	33.900967
883.507090	77088.768838	33.905984
884.473980	77200.006055	33.911002
885.346605	77333.630101	33.916020
886.240512	77447.882061	33.921037
886.726907	77561.412885	33.926055
887.828481	77680.675190	33.931072
888.694817	77796.427757	33.936090
889.189751	77920.371970	33.941108
890.241360	78027.963496	33.946125
891.195764	78147.073512	33.951143
892.071075	78247.485216	33.956160
893.326379	78362.482498	33.961178
893.748417	78478.535531	33.966196
894.521604	78584.424572	33.971213
895.765558	78711.422194	33.976231
896.674994	78821.344760	33.981248
897.592265	78934.497055	33.986266
898.329337	79058.547818	33.991284
898.992571	79164.544976	33.996301
899.734435	79288.900069	34.001319
900.801321	79417.588273	34.006336
901.832721	79539.973479	34.011354
902.686337	79661.981652	34.016372
903.695902	79785.118827	34.021389
904.473198	79902.629810	34.026407
905.163103	80036.054812	34.031424
905.799518	80148.939294	34.036442
906.851779	80279.040053	34.041460
907.744733	80410.445968	34.046477
908.695007	80538.435448	34.051495
909.777787	80676.236288	34.056512
911.063333	80803.997113	34.061530
911.509981	80925.884479	34.066548
912.754854	81059.012075	34.071565
913.280491	81188.680056	34.076583
914.408655	81326.375622	34.081600
915.484623	81447.811957	34.086618
916.426212	81581.230237	34.091636
917.447533	81718.374301	34.096653
918.538033	81851.149712	34.101671
918.878016	81985.867751	34.106688
920.192838	82107.168162	34.111706
921.008938	82235.680498	34.116724
922.017886	82368.851211	34.121741
923.061586	82502.954712	34.126759
924.281625	82641.250468	34.131776
924.999527	82758.351872	34.136794
925.896438	82890.617632	34.141812
927.032263	83012.722839	34.146829
927.844304	83150.274036	34.151847
928.697687	83275.148768	34.156864
930.035832	83401.481300	34.161882
930.806567	83531.489059	34.166900
931.711252	83654.710217	34.171917
932.656472	83772.882551	34.176935
933.225618	83907.130308	34.181952
934.511089	84037.097779	34.186970
935.073321	84178.316931	34.191988
936.297210	84308.219244	34.197005
937.422320	84428.266775	34.202023
937.765944	84567.380637	34.207040
939.127498	84698.137469	34.212058
939.793414	84841.599125	34.217076
941.048297	84962.401512	34.222093
941.983198	85097.446530	34.227111
942.732669	85229.720808	34.232128
943.951953	85363.784849	34.237146
944.300750	85506.754575	34.242164
945.494357	85632.067780	34.247181
947.017308	85766.124150	34.252199
947.483207	85899.953819	34.257216
948.397653	86021.003997	34.262234
949.234808	86162.645967	34.267252
950.320616	86300.473443	34.272269
951.251302	86421.712821	34.277287
952.290882	86565.263871	34.282304
953.348310	86673.989771	34.287322
954.034589	86794.876128	34.292340
954.860774	86931.023808	34.297357
955.956954	87049.895510	34.302375
956.919093	87176.151319	34.307392
958.080838	87292.339871	34.312410
958.708677	87434.793783	34.317428
959.593763	87562.279871	34.322445
960.814552	87681.109270	34.327463
961.729393	87821.695265	34.332480
962.890698	87939.255083	34.337498
963.622819	88075.055273	34.342516
964.172062	88205.080578	34.347533
965.206274	88344.915348	34.352551
966.202166	88477.647272	34.357568
967.176560	88609.572087	34.362586
968.553432	88760.393324	34.367604
969.445048	88890.811584	34.372621
970.018345	89025.170911	34.377639
971.056486	89158.076683	34.382656
972.389663	89306.144769	34.387674
973.150131	89429.146712	34.392692
973.820632	89574.873937	34.397709
974.813737	89717.142204	34.402727
976.118640	89864.685201	34.407744
977.026053	90000.099192	34.412762
978.084317	90148.252510	34.417780
978.641103	90293.785581	34.422797
979.697968	90434.019475	34.427815
980.872623	90602.434803	34.432832
982.001907	90734.458802	34.437850
982.888655	90884.201482	34.442868
983.887256	91029.326732	34.447885
985.034816	91173.808328	34.452903
985.588937	91323.858745	34.457920
987.087708	91474.737913	34.462938
988.433763	91617.910457	34.467956
988.882379	91764.633573	34.472973
990.332953	91902.848119	34.477991
991.017579	92049.675075	34.483008
991.969803	92188.412548	34.488026
993.105668	92344.359269	34.493044
993.758449	92494.754899	34.498061
994.941584	92642.964237	34.503079
996.142519	92786.950822	34.508096
997.493005	92934.717105	34.513114
998.338575	93072.461303	34.518132
999.369485	93227.465667	34.523149
1000.433094	93364.771441	34.528167
1001.454920	93510.475233	34.533184
1002.456850	93655.168822	34.538202
1003.537573	93804.679982	34.543220
1004.292499	93952.785227	34.548237
1005.408866	94084.306052	34.553255
1006.528165	94240.049506	34.558272
1007.566961	94375.513063	34.563290
1008.610717	94518.252133	34.568308
1009.969694	94659.966494	34.573325
1010.935301	94808.663941	34.578343
1011.883181	94937.831760	34.583360
1012.612904	95073.688992	34.588378
1013.758776	95222.778488	34.593396
1014.587381	95367.545226	34.598413
1015.628728	95504.445659	34.603431
1016.413216	95650.247355	34.608448
1017.646924	95795.573766	34.613466
1018.624702	95936.339529	34.618484
1019.555552	96079.027357	34.623501
1020.615146	96210.426603	34.628519
1021.177901	96355.049379	34.633536
1022.558402	96489.568593	34.638554
1023.528021	96614.911699	34.643572
1024.040163	96751.215900	34.648589
1025.260331	96886.776017	34.653607
1026.224965	97037.588460	34.658624
1027.230660	97175.896155	34.663642
1028.397366	97326.044509	34.668660
1029.521803	97468.797042	34.673677
1030.598461	97611.735170	34.678695
1031.332116	97757.934858	34.683712
1032.810177	97902.446747	34.688730
1033.505320	98056.082435	34.693748
1034.534265	98202.111158	34.698765
1035.593751	98352.813570	34.703783
1036.693345	98504.093556	34.708800
1037.542066	98653.537324	34.713818
1038.739164	98795.891427	34.718836
1039.242072	98955.912779	34.723853
1040.711682	99109.723841	34.728871
1041.691290	99274.159897	34.733888
1042.645399	99428.585637	34.738906
1043.713180	99582.132253	34.743924
1044.298450	99745.047763	34.748941
1045.708542	99907.112334	34.753959
1046.745635	100071.796999	34.758976
1047.743705	100226.878904	34.763994
1048.826404	100401.789017	34.769012
1050.072236	100557.695798	34.774029
1051.050977	100713.657821	34.779047
1052.396882	100877.005068	34.784064
1053.167843	101043.752113	34.789082
1054.413197	101208.409919	34.794100
1055.241840	101368.962681	34.799117
1056.674430	101524.882873	34.804135
1057.793382	101687.559718	34.809152
1058.960205	101858.077765	34.814170
1059.921753	102004.692010	34.819188
1060.500005	102174.023321	34.824205
1062.142483	102333.122135	34.829223
1062.997397	102497.505202	34.834240
1063.789453	102656.966931	34.839258
1065.288259	102833.156109	34.844276
1065.972916	102995.996142	34.849293
1067.247307	103150.896443	34.854311
1068.106872	103330.953955	34.859328
1069.412867	103502.181376	34.864346
1070.973173	103662.478572	34.869364
1071.807311	103828.532423	34.874381
1072.885933	103992.127103	34.879399
1074.147574	104157.583131	34.884416
1075.216619	104310.276736	34.889434
1076.261395	104473.270456	34.894452
1077.409084	104641.472766	34.899469
1079.008934	104787.289277	34.904487
1079.715469	104954.192833	34.909504
1080.643980	105119.832541	34.914522
1082.169239	105273.486133	34.919540
1082.848942	105435.197612	34.924557
1084.069974	105589.179218	34.929575
1085.013987	105751.370693	34.934592
1086.044001	105914.348309	34.939610
1087.147234	106072.737785	34.944628
1088.031041	106238.466028	34.949645
1089.178742	106389.178614	34.954663
1090.272593	106556.054758	34.959680
1091.206244	106719.266865	34.964698
1092.123583	106870.410720	34.969716
1093.208009	107028.236955	34.974733
1094.284652	107169.834292	34.979751
1095.248113	107334.934028	34.984768
1096.493458	107496.338450	34.989786
1097.684781	107653.618236	34.994804
1098.652124	107813.140224	34.999821
1100.029889	107975.819575	35.004839
1100.655686	108136.740672	35.009856
1102.007408	108303.394694	35.014874
1102.957029	108458.433438	35.019892
1104.000978	108628.142553	35.024909
1104.999651	108780.955900	35.029927
1106.171105	108953.157460	35.034944
1107.400258	109126.466768	35.039962
1108.685689	109288.253672	35.044980
1109.314396	109463.193064	35.049997
1111.004195	109630.853033	35.055015
1111.848076	109807.041256	35.060032
1112.766415	109979.617195	35.065050
1114.047393	110154.686173	35.070068
1115.034554	110322.040947	35.075085
1116.277805	110496.508813	35.080103
1118.005220	110669.024863	35.085120
1118.716180	110852.340807	35.090138
1119.724483	111018.731752	35.095156
1120.755158	111203.584670	35.100173
1121.940676	111376.670899	35.105191
1122.997750	111550.881403	35.110208
1123.941494	111737.678347	35.115226
1125.584155	111908.324051	35.120244
1126.440945	112092.371770	35.125261
1127.824948	112276.109615	35.130279
1129.075504	112447.757750	35.135296
1129.668894	112622.553335	35.140314
1131.548340	112804.237872	35.145332
1132.285684	112980.471124	35.150349
1133.573902	113156.821913	35.155367
1134.855431	113342.699202	35.160384
1135.657197	113519.952276	35.165402
1137.225770	113698.836377	35.170420
1138.246519	113875.803246	35.175437
1139.668535	114047.330648	35.180455
1141.060632	114232.713222	35.185472
1142.280141	114401.724733	35.190490
1143.413764	114566.679233	35.195508
1144.317772	114736.870465	35.200525
1145.171697	114911.788436	35.205543
1146.678552	115091.741698	35.210560
1147.425524	115263.900471	35.215578
1148.661212	115449.224879	35.220596
1149.737039	115624.948583	35.225613
1151.055138	115795.967701	35.230631
1152.142916	115972.756587	35.235648
1153.253768	116162.315007	35.240666
1154.744924	116342.416316	35.245684
1155.737962	116526.858180	35.250701
1157.007207	116699.791641	35.255719
1158.359715	116882.073486	35.260736
1159.505904	117057.792924	35.265754
1160.585272	117229.578957	35.270772
1161.268078	117410.230513	35.275789
1162.954440	117578.435027	35.280807
1163.983882	117751.220604	35.285824
1164.705555	117939.301464	35.290842
1166.128436	118124.571752	35.295860
1167.360420	118286.178664	35.300877
1168.603327	118452.186003	35.305895
1169.384735	118623.175156	35.310912
1170.067505	118798.810326	35.315930
1171.582654	118968.620670	35.320948
1172.337049	119141.633202	35.325965
1173.626560	119311.683343	35.330983
1174.804032	119485.240052	35.336000
1175.750338	119676.516199	35.341018
1177.111892	119855.614344	35.346036
1178.158695	120042.436908	35.351053
1179.702583	120221.558946	35.356071
1180.942724	120402.733583	35.361088
1181.539022	120585.849184	35.366106
1182.829788	120776.315742	35.371124
1184.040467	120960.985986	35.376141
1184.910641	121145.088835	35.381159
1186.253707	121328.192499	35.386176
1187.413477	121539.043098	35.391194
1188.971630	121725.489240	35.396212
1190.121811	121917.708575	35.401229
1191.138490	122116.343236	35.406247
1192.302671	122311.556078	35.411264
1193.409042	122509.303371	35.416282
1194.495385	122704.974335	35.421300
1195.570443	122897.425852	35.426317
1197.095886	123107.720154	35.431335
1198.214667	123307.372349	35.436352
1199.584401	123516.044017	35.441370
1200.768644	123705.222055	35.446388
1201.766519	123909.336282	35.451405
1203.000132	124115.063840	35.456423
1204.904629	124308.825838	35.461440
1205.867842	124510.918754	35.466458
1207.502799	124710.522495	35.471476
1208.263619	124912.293883	35.476493
1209.215417	125117.043065	35.481511
1210.585840	125317.198662	35.486528
1212.048451	125531.702008	35.491546
1213.500734	125722.585586	35.496564
1214.561151	125933.804735	35.501581
1216.017789	126136.234455	35.506599
1217.597952	126320.884293	35.511616
1218.488124	126525.117326	35.516634
1220.145912	126717.571909	35.521652
1221.521922	126911.885741	35.526669
1222.352039	127111.107022	35.531687
1223.621375	127310.628430	35.536704
1224.793436	127509.011491	35.541722
1226.214042	127693.349879	35.546740
1227.178189	127896.398173	35.551757
1228.453221	128099.221162	35.556775
1230.106716	128290.123152	35.561792
1230.930989	128485.203124	35.566810
1232.354446	128676.840695	35.571828
1233.792409	128876.051358	35.576845
1234.651114	129079.299499	35.581863
1236.332459	129267.524465	35.586880
1237.304240	129478.217193	35.591898
1238.453154	129662.429108	35.596916
1239.675995	129870.432721	35.601933
1240.727861	130062.083971	35.606951
1242.435050	130261.969514	35.611968
1243.335907	130463.593598	35.616986
1244.922343	130658.120151	35.622004
1246.306733	130850.687169	35.627021
1247.388923	131050.598089	35.632039
1248.890732	131240.230170	35.637056
1249.693851	131427.041447	35.642074
1250.958656	131608.490192	35.647092
1252.251295	131797.954440	35.652109
1253.399168	131987.886273	35.657127
1254.297135	132168.734974	35.662144
1255.811566	132353.028046	35.667162
1256.859089	132536.354513	35.672180
1258.546058	132724.504871	35.677197
1259.144253	132924.182928	35.682215
1260.873258	133110.044373	35.687232
1261.703622	133315.613543	35.692250
1262.868939	133502.186632	35.697268
1264.301049	133691.231164	35.702285
1265.666166	133888.661764	35.707303
1266.825492	134088.130334	35.712320
1267.788821	134296.715923	35.717338
1269.365670	134488.050605	35.722356
1270.582029	134691.814586	35.727373
1271.589192	134897.096890	35.732391
1273.000819	135099.284049	35.737408
1273.723597	135313.634929	35.742426
1275.135424	135524.922303	35.747444
1277.287954	135736.564228	35.752461
1277.813336	135951.215500	35.757479
1279.397563	136158.519665	35.762496
1280.505571	136379.921495	35.767514
1281.858616	136590.131690	35.772532
1283.186183	136805.283195	35.777549
1284.503812	137020.107324	35.782567
1285.917576	137230.272867	35.787584
1286.898487	137450.379982	35.792602
1288.339584	137663.144671	35.797620
1289.841116	137891.027556	35.802637
1290.701222	138110.116109	35.807655
1292.237303	138321.866410	35.812672
1293.300375	138549.833833	35.817690
1294.733994	138766.043801	35.822708
1296.112399	138985.562926	35.827725
1297.695099	139212.601956	35.832743
1299.292703	139434.385839	35.837760
1300.406526	139652.160100	35.842778
1301.578160	139865.344965	35.847796
1302.886340	140085.146676	35.852813
1304.215670	140310.860007	35.857831
1305.704303	140532.970638	35.862848
1307.151667	140755.888284	35.867866
1308.720082	140973.825833	35.872884
1309.461872	141187.045780	35.877901
1310.963242	141409.589947	35.882919
1312.476304	141621.256976	35.887936
1313.538090	141844.303443	35.892954
1314.827278	142065.690848	35.897972
1316.686193	142286.723555	35.902989
1317.596639	142511.700452	35.908007
1319.200857	142730.084446	35.913024
1320.325040	142950.207136	35.918042
1321.222261	143172.841187	35.923060
1322.686112	143391.871961	35.928077
1324.116508	143620.173860	35.933095
1325.542747	143845.190295	35.938112
1327.031191	144068.903443	35.943130
1328.452578	144290.762384	35.948148
1330.177625	144503.093919	35.953165
1331.133950	144732.858507	35.958183
1332.435916	144953.914081	35.963200
1333.698724	145170.242605	35.968218
1335.131818	145389.883422	35.973236
1336.669208	145619.154916	35.978253
1337.734503	145837.636782	35.983271
1339.545518	146035.301733	35.988288
1340.173097	146243.090784	35.993306
1341.463611	146441.993774	35.998324
1343.298931	146649.227333	36.003341
1344.352344	146859.274921	36.008359
1346.012685	147061.447831	36.013376
1347.201288	147267.135057	36.018394
1348.293219	147469.918920	36.023412
1349.487610	147680.417373	36.028429
1350.874098	147896.687182	36.033447
1352.070682	148107.567784	36.038464
1353.153867	148326.615781	36.043482
1354.582726	148541.701165	36.048500
1356.169332	148766.713995	36.053517
1357.516208	148994.735463	36.058535
1358.644965	149218.692191	36.063552
1360.390359	149442.566026	36.068570
1361.231728	149672.738481	36.073588
1362.758956	149892.231117	36.078605
1364.161935	150121.784464	36.083623
1365.502585	150353.772962	36.088640
1366.824557	150577.083108	36.093658
1367.948505	150824.123788	36.098676
1369.577475	151050.307302	36.103693
1370.578004	151288.534731	36.108711
1372.212995	151528.123643	36.113728
1373.424522	151767.526004	36.118746
1375.090458	151997.363385	36.123764
1376.262461	152241.813375	36.128781
1378.031120	152488.379765	36.133799
1379.395316	152720.844200	36.138816
1380.975855	152956.715784	36.143834
1382.476792	153198.998575	36.148852
1384.086337	153428.139787	36.153869
1385.185120	153669.345076	36.158887
1386.674839	153907.875204	36.163904
1388.294744	154139.619955	36.168922
1389.435580	154375.985164	36.173940
1391.204875	154600.878898	36.178957
1392.085173	154846.921780	36.183975
1393.678790	155091.305339	36.188992
1395.343070	155334.307867	36.194010
1396.561266	155564.572488	36.199028
1398.234728	155801.748754	36.204045
1399.909991	156043.965451	36.209063
1401.085167	156265.619929	36.214080
1402.162918	156512.083221	36.219098
1403.704531	156751.734022	36.224116
1405.319533	156978.958791	36.229133
1406.417507	157236.263272	36.234151
1408.217595	157464.920826	36.239168
1409.550135	157703.046692	36.244186
1410.559405	157944.931036	36.249204
1412.290090	158183.313850	36.254221
1413.991795	158422.857390	36.259239
1415.614163	158660.510017	36.264256
1416.408720	158894.446494	36.269274
1417.955209	159143.970185	36.274292
1419.593523	159373.917063	36.279309
1420.640093	159618.823662	36.284327
1422.052434	159848.236379	36.289344
1423.780780	160088.937506	36.294362
1425.304133	160331.042758	36.299380
1426.752280	160573.313061	36.304397
1427.884008	160812.904272	36.309415
1429.125593	161048.949808	36.314432
1430.795547	161292.038755	36.319450
1431.659036	161529.922651	36.324468
1433.472958	161745.631502	36.329485
1434.837859	161990.472085	36.334503
1436.274080	162228.764063	36.339520
1437.957581	162456.087034	36.344538
1439.281965	162686.006203	36.349556
1440.571759	162917.518597	36.354573
1442.162862	163145.417061	36.359591
1443.495765	163378.168547	36.364608
1445.233695	163607.010533	36.369626
1446.346417	163832.751732	36.374644
1447.714709	164061.107207	36.379661
1449.212334	164308.144821	36.384679
1450.428260	164541.985185	36.389696
1452.152294	164784.113733	36.394714
1453.274016	165019.075082	36.399732
1455.173816	165268.452895	36.404749
1456.361239	165505.983027	36.409767
1457.353628	165748.597733	36.414784
1458.867852	165999.638332	36.419802
1460.183265	166258.151190	36.424820
1462.020760	166499.214246	36.429837
1463.378500	166757.531893	36.434855
1464.616820	167015.259744	36.439872
1466.220126	167266.989307	36.444890
1467.547607	167526.888935	36.449908
1469.215217	167778.407111	36.454925
1470.511527	168036.523224	36.459943
1472.068456	168304.884051	36.464960
1473.725676	168560.469654	36.469978
1475.130858	168830.468723	36.474996
1476.789198	169089.039842	36.480013
1478.342873	169347.653659	36.485031
1479.467080	169607.706912	36.490048
1481.296660	169871.459868	36.495066
1482.411602	170151.375035	36.500084
1484.118511	170410.717753	36.505101
1485.422702	170678.707857	36.510119
1486.917990	170948.294288	36.515136
1488.953544	171207.715310	36.520154
1490.412385	171478.325145	36.525172
1491.997783	171751.696909	36.530189
1493.324831	172014.152029	36.535207
1494.844370	172278.444480	36.540224
1496.714809	172544.790739	36.545242
1498.385413	172816.718117	36.550260
1499.728524	173072.558786	36.555277
1501.622316	173336.669290	36.560295
1503.016455	173592.592555	36.565312
1504.699457	173847.595282	36.570330
1505.610864	174116.192147	36.575348
1507.730922	174381.921464	36.580365
1509.505618	174639.286902	36.585383
1510.660253	174900.496149	36.590400
1512.030041	175149.698218	36.595418
1513.705400	175413.265658	36.600436
1515.327107	175670.874181	36.605453
1516.625831	175944.673552	36.610471
1518.118457	176196.424623	36.615488
1519.777027	176459.655182	36.620506
1521.287332	176722.198666	36.625524
1522.854661	176982.727695	36.630541
1524.386007	177239.428224	36.635559
1525.702792	177500.074248	36.640576
1527.789194	177763.800645	36.645594
1528.941794	178031.051824	36.650612
1530.341136	178288.207908	36.655629
1531.743226	178557.986785	36.660647
1533.314815	178817.936577	36.665664
1535.037812	179056.859748	36.670682
1536.394120	179298.075937	36.675700
1537.948699	179552.493896	36.680717
1539.498931	179807.014851	36.685735
1540.341894	180043.132274	36.690752
1542.020992	180296.745526	36.695770
1543.911378	180549.183513	36.700788
1545.657851	180793.491985	36.705805
1546.954699	181060.297921	36.710823
1548.190976	181316.853281	36.715840
1550.255130	181565.711132	36.720858
1551.623475	181822.298012	36.725876
1552.975999	182080.818340	36.730893
1554.548275	182345.375190	36.735911
1555.945735	182606.277364	36.740928
1557.468150	182873.662710	36.745946
1558.771014	183141.540334	36.750964
1560.411548	183411.016763	36.755981
1562.508880	183672.650440	36.760999
1563.876277	183955.886423	36.766016
1565.285428	184220.702515	36.771034
1566.607763	184566.530084	36.776052
1568.228690	184843.480775	36.781069
1569.763969	185114.654642	36.786087
1571.283744	185401.350537	36.791104
1573.257211	185680.000875	36.796122
1574.573735	185953.547929	36.801140
1576.003140	186240.082505	36.806157
1577.817362	186514.137324	36.811175
1579.372930	186808.679925	36.816192
1581.214917	187085.449626	36.821210
1582.653137	187380.748762	36.826228
1584.437059	187663.828150	36.831245
1585.991597	187942.016623	36.836263
1587.131027	188234.672471	36.841280
1588.992466	188520.967725	36.846298
1590.651110	188803.485462	36.851316
1592.518269	189096.512287	36.856333
1594.009539	189382.867679	36.861351
1595.556158	189678.359184	36.866368
1597.577350	189958.206846	36.871386
1599.477025	190246.684898	36.876404
1600.764950	190524.819865	36.881421
1602.641219	190814.064990	36.886439
1603.974108	191104.462681	36.891456
1605.773314	191386.710731	36.896474
1607.699108	191668.380820	36.901492
1609.205307	191960.048880	36.906509
1610.692762	192232.339834	36.911527
1611.890043	192530.737976	36.916544
1614.123572	192815.131212	36.921562
1615.518057	193095.439859	36.926580
1617.177423	193383.912171	36.931597
1618.928112	193670.795980	36.936615
1620.322494	193951.817746	36.941632
1622.259001	194237.378274	36.946650
1623.492801	194519.366230	36.951668
1624.941196	194808.814556	36.956685
1626.695472	195096.005727	36.961703
1628.376506	195386.180924	36.966720
1630.033914	195672.778842	36.971738
1631.765766	195968.281604	36.976756
1633.332310	196268.129114	36.981773
1635.061897	196551.847179	36.986791
1636.474412	196846.004677	36.991808
1637.974885	197136.262563	36.996826
1639.958372	197417.478646	37.001844
1641.360544	197708.261087	37.006861
1643.266493	197991.166914	37.011879
1644.372006	198261.904061	37.016896
1645.926606	198544.484888	37.021914
1647.622307	198813.885963	37.026932
1649.299553	199093.501985	37.031949
1651.136899	199361.179913	37.036967
1652.150400	199651.798265	37.041984
1654.102734	199933.125467	37.047002
1655.336464	200218.299734	37.052020
1656.503622	200514.636478	37.057037
1658.355303	200801.213781	37.062055
1660.120557	201105.485083	37.067072
1661.907634	201401.497765	37.072090
1663.789715	201704.126109	37.077108
1664.738165	202005.580166	37.082125
1666.604288	202305.697213	37.087143
1668.069879	202609.332187	37.092160
1669.889399	202919.516944	37.097178
1671.632378	203232.356075	37.102196
1673.097207	203541.047831	37.107213
1675.009492	203854.217145	37.112231
1676.847502	204173.698469	37.117248
1678.508888	204489.041911	37.122266
1679.920952	204801.630570	37.127284
1681.354787	205132.353931	37.132301
1683.249314	205448.881740	37.137319
1685.066337	205777.742574	37.142336
1686.685883	206096.727680	37.147354
1688.309369	206424.248050	37.152372
1689.922924	206754.412383	37.157389
1691.843287	207072.919999	37.162407
1693.709904	207412.292420	37.167424
1695.468172	207742.029110	37.172442
1697.362070	208066.588198	37.177460
1698.628649	208406.564034	37.182477
1700.793108	208726.915550	37.187495
1702.260626	209058.325359	37.192512
1704.581407	209390.821433	37.197530
1705.966927	209709.924319	37.202548
1707.509015	210046.226576	37.207565
1709.218411	210375.669557	37.212583
1710.968598	210710.238043	37.217600
1713.217343	211045.592626	37.222618
1714.755040	211368.382534	37.227636
1716.226122	211704.977330	37.232653
1718.233500	212033.308635	37.237671
1720.032884	212378.769443	37.242688
1721.658728	212696.593267	37.247706
1723.703368	213031.169062	37.252724
1725.165964	213349.958997	37.257741
1727.152533	213685.179619	37.262759
1729.052173	214009.719207	37.267776
1730.476479	214346.959119	37.272794
1732.634533	214672.703635	37.277812
1733.922316	215016.087806	37.282829
1736.192906	215327.741574	37.287847
1737.844408	215669.164098	37.292864
1739.470431	215985.237870	37.297882
1741.486934	216321.294393	37.302900
1742.427182	216647.383445	37.307917
1744.806802	216962.882697	37.312935
1746.618154	217312.563099	37.317952
1748.255423	217628.737824	37.322970
1750.198493	217965.645290	37.327988
1751.869906	218308.057316	37.333005
1753.791062	218614.687102	37.338023
1755.225787	218950.480699	37.343040
1756.965548	219265.420880	37.348058
1759.019748	219569.185054	37.353076
1760.464169	219887.829907	37.358093
1762.635551	220196.275743	37.363111
1763.907345	220500.924848	37.368128
1766.063207	220798.652842	37.373146
1767.522159	221103.018826	37.378164
1769.221168	221427.670573	37.383181
1770.743981	221732.052156	37.388199
1772.393033	222050.132254	37.393216
1774.298736	222364.818934	37.398234
1775.906583	222685.573059	37.403252
1777.233417	223011.909310	37.408269
1779.473892	223337.874013	37.413287
1780.998453	223671.292575	37.418304
1782.621255	223999.792819	37.423322
1784.658122	224333.207503	37.428340
1785.969400	224668.361617	37.433357
1788.020504	225003.577805	37.438375
1790.057774	225341.488999	37.443392
1791.689024	225689.930209	37.448410
1793.564697	226028.425567	37.453428
1795.069494	226368.401567	37.458445
1796.754541	226703.395534	37.463463
1798.646058	227057.765868	37.468480
1800.271761	227422.644220	37.473498
1802.488189	227767.945144	37.478516
1804.072960	228114.665850	37.483533
1805.874306	228462.724401	37.488551
1807.593721	228824.971136	37.493568
1809.459717	229188.769871	37.498586
1811.606866	229536.951812	37.503604
1813.067009	229908.307982	37.508621
1815.144731	230257.364251	37.513639
1817.256703	230613.477323	37.518656
1819.075588	230983.252628	37.523674
1821.008108	231348.005378	37.528692
1822.596995	231701.075072	37.533709
1824.694245	232056.605416	37.538727
1826.687940	232418.223294	37.543744
1828.048219	232779.431980	37.548762
1830.458173	233143.550046	37.553780
1831.977591	233504.555509	37.558797
1833.975905	233856.238769	37.563815
1835.522336	234222.828321	37.568832
1837.650019	234595.042482	37.573850
1839.668922	234946.670872	37.578868
1841.458357	235311.087569	37.583885
1843.469292	235670.540953	37.588903
1845.249958	236037.041468	37.593920
1847.315705	236400.448575	37.598938
1849.077561	236767.103738	37.603956
1851.153983	237118.746550	37.608973
1852.873371	237476.770374	37.613991
1854.721870	237834.240136	37.619008
1856.473292	238201.632086	37.624026
1858.146360	238567.816499	37.629044
1860.099311	238928.825172	37.634061
1862.290984	239287.154094	37.639079
1864.306816	239654.553715	37.644096
1865.982424	240016.671382	37.649114
1868.167583	240373.501150	37.654132
1869.901984	240725.142488	37.659149
1871.917017	241087.408835	37.664167
1873.793888	241451.550732	37.669184
1875.170142	241809.622855	37.674202
1877.543851	242161.619436	37.679220
1879.102426	242519.814407	37.684237
1880.890906	242869.691445	37.689255
1883.036569	243212.653232	37.694272
1885.023967	243561.431160	37.699290
1886.789025	243895.687412	37.704308
1888.360868	244236.146307	37.709325
1890.283291	244562.629003	37.714343
1892.456554	244910.613596	37.719360
1893.754668	245252.180608	37.724378
1896.097194	245590.636903	37.729396
1897.499828	245933.431150	37.734413
1899.479697	246281.621467	37.739431
1901.381768	246638.688864	37.744448
1903.110408	246996.900446	37.749466
1905.352521	247346.495738	37.754484
1906.999964	247709.621351	37.759501
1908.777317	248069.804629	37.764519
1910.420225	248421.777835	37.769536
1911.779675	248798.079354	37.774554
1914.107503	249164.677266	37.779572
1915.944086	249539.505381	37.784589
1918.040003	249916.756095	37.789607
1919.867563	250286.833732	37.794624
1921.682697	250665.828605	37.799642
1923.855673	251047.967248	37.804660
1925.411233	251423.825683	37.809677
1927.629143	251814.185667	37.814695
1929.835159	252193.852349	37.819712
1931.388385	252586.575124	37.824730
1933.821758	252973.138948	37.829748
1935.750443	253355.868875	37.834765
1937.564704	253745.575726	37.839783
1939.692859	254140.033286	37.844800
1941.591386	254521.037519	37.849818
1943.875097	254912.318794	37.854836
1945.647130	255294.255142	37.859853
1947.828852	255683.238654	37.864871
1949.621398	256083.382228	37.869888
1951.412581	256466.429894	37.874906
1953.707471	256851.150293	37.879924
1955.714144	257245.439984	37.884941
1957.505543	257641.133785	37.889959
1959.371121	258027.111652	37.894976
1961.616875	258436.905467	37.899994
1963.721883	258813.902384	37.905012
1965.529155	259212.128741	37.910029
1967.396129	259604.553143	37.915047
1969.626048	259996.132050	37.920064
1971.353683	260397.008533	37.925082
1973.445144	260781.469003	37.930100
1975.781887	261187.987876	37.935117
1977.484346	261575.427548	37.940135
1979.747054	261975.960774	37.945152
1981.372148	262373.112546	37.950170
1983.610099	262763.664669	37.955188
1985.378108	263173.897426	37.960205
1987.581714	263578.828165	37.965223
1989.501990	263961.856588	37.970240
1991.230950	264363.505869	37.975258
1993.271679	264760.075776	37.980276
1995.500995	265156.106672	37.985293
1997.630076	265566.527573	37.990311
1999.559424	265964.888169	37.995328
2001.410871	266355.411131	38.000346
2003.455078	266759.516120	38.005364
2005.397222	267157.031774	38.010381
2007.569340	267563.246917	38.015399
2009.509397	267962.435899	38.020416
2011.269513	268364.368987	38.025434
2013.526301	268752.126655	38.030452
2015.219315	269144.085422	38.035469
2017.206694	269527.843725	38.040487
2019.133800	269912.981348	38.045504
2021.101227	270294.834725	38.050522
2023.327182	270678.855642	38.055540
2024.789943	271065.889649	38.060557
2026.674892	271450.849521	38.065575
2028.918391	271842.685092	38.070592
2030.947582	272241.612870	38.075610
2032.953187	272628.580468	38.080628
2034.837294	273038.727395	38.085645
2036.731673	273438.737395	38.090663
2038.681650	273844.222506	38.095680
2040.747480	274259.084284	38.100698
2042.600302	274660.694955	38.105716
2044.374497	275077.477610	38.110733
2046.540618	275512.202759	38.115751
2048.823049	275919.555779	38.120768
2050.859120	276338.881394	38.125786
2053.007737	276769.462952	38.130804
2055.705849	277183.271222	38.135821
2057.459272	277609.034054	38.140839
2059.396599	278027.324928	38.145856
2061.394998	278459.596789	38.150874
2063.571287	278887.800555	38.155892
2065.740754	279315.012573	38.160909
2067.388482	279738.088256	38.165927
2069.738259	280162.499209	38.170944
2071.596489	280599.275614	38.175962
2074.089928	281025.944651	38.180980
2076.314107	281468.423166	38.185997
2078.373528	281916.435283	38.191015
2080.598263	282336.307643	38.196032
2082.717133	282772.674679	38.201050
2085.034261	283206.621010	38.206068
2086.997587	283633.586023	38.211085
2088.908594	284074.929241	38.216103
2091.067961	284513.462939	38.221120
2093.004599	284951.597010	38.226138
2095.626274	285406.710480	38.231156
2098.142638	285835.733703	38.236173
2099.991294	286278.443653	38.241191
2101.974272	286707.493967	38.246208
2103.986741	287148.902887	38.251226
2106.275969	287574.827209	38.256244
2108.696038	288017.410732	38.261261
2110.934788	288460.146567	38.266279
2113.219275	288878.013933	38.271296
2115.246466	289329.562342	38.276314
2117.308203	289752.257799	38.281332
2119.500480	290191.357974	38.286349
2121.743235	290627.222550	38.291367
2123.908400	291054.539580	38.296384
2126.238976	291492.491774	38.301402
2128.064426	291917.824747	38.306420
2130.531508	292353.413538	38.311437
2132.396024	292787.138455	38.316455
2134.935285	293222.836653	38.321472
2136.758489	293660.192475	38.326490
2138.953739	294092.967579	38.331508
2141.045632	294513.822781	38.336525
2143.227255	294958.399640	38.341543
2145.024613	295386.251247	38.346560
2147.587783	295816.417204	38.351578
2149.597071	296252.277453	38.356596
2151.799921	296674.496023	38.361613
2153.605237	297128.965691	38.366631
2155.954479	297542.040622	38.371648
2158.284064	297960.345460	38.376666
2160.086845	298361.237630	38.381684
2162.135121	298770.415543	38.386701
2164.503219	299179.718112	38.391719
2166.857289	299589.908380	38.396736
2168.624405	299998.334176	38.401754
2170.303928	300411.238647	38.406772
2172.439085	300823.687899	38.411789
2175.024731	301256.372427	38.416807
2176.961203	301671.207175	38.421824
2178.990903	302106.688096	38.426842
2181.314099	302531.889163	38.431860
2183.395943	302960.881587	38.436877
2185.650615	303403.500651	38.441895
2187.723005	303835.076666	38.446912
2189.734562	304280.290177	38.451930
2191.582571	304715.016270	38.456948
2193.530620	305156.348315	38.461965
2195.823905	305606.303866	38.466983
2198.174519	306066.603041	38.472000
2200.279401	306520.387503	38.477018
2202.619304	306990.122583	38.482036
2204.963801	307442.515877	38.487053
2207.180244	307905.941234	38.492071
2209.431195	308370.016786	38.497088
2211.259907	308826.463145	38.502106
2213.534390	309289.409467	38.507124
2216.002829	309761.839234	38.512141
2218.189853	310235.958204	38.517159
2220.519873	310702.156508	38.522176
2222.777036	311178.361819	38.527194
2224.961460	311644.878233	38.532212
2227.804670	312113.088999	38.537229
2229.639122	312599.955188	38.542247
2232.052254	313064.975022	38.547264
2234.583760	313546.265541	38.552282
2236.623131	314022.983567	38.557300
2238.788530	314495.032512	38.562317
2241.215607	314969.598926	38.567335
2243.133796	315444.519157	38.572352
2245.757833	315939.119219	38.577370
2247.854412	316408.494246	38.582388
2250.553812	316892.616156	38.587405
2252.829342	317368.322953	38.592423
2254.872140	317844.238684	38.597440
2257.318089	318328.206887	38.602458
2259.658997	318815.612049	38.607476
2262.001738	319287.303363	38.612493
2264.123236	319768.641773	38.617511
2266.689462	320243.688111	38.622528
2268.994961	320730.366686	38.627546
2271.119665	321218.006885	38.632564
2273.580125	321686.811340	38.637581
2275.648775	322163.411224	38.642599
2278.132998	322647.096327	38.647616
2280.683715	323129.775837	38.652634
2282.779416	323597.854755	38.657652
2285.345292	324069.813131	38.662669
2287.525893	324552.889185	38.667687
2289.809768	325028.432950	38.672704
2292.087676	325489.154374	38.677722
2294.340060	325979.788791	38.682740
2297.005325	326458.326230	38.687757
2299.045628	326925.563746	38.692775
2301.088681	327402.918664	38.697792
2303.750534	327891.512047	38.702810
2305.469976	328357.844231	38.707828
2308.231771	328831.390731	38.712845
2310.145055	329296.412949	38.717863
2312.408716	329745.924430	38.722880
2314.515620	330193.222702	38.727898
2316.495195	330655.579869	38.732916
2319.016250	331110.438984	38.737933
2320.862241	331567.098037	38.742951
2323.054165	332045.717491	38.747968
2325.553057	332510.913826	38.752986
2327.825382	332984.156183	38.758004
2330.278361	333451.326848	38.763021
2332.232766	333941.451050	38.768039
2334.369078	334414.772789	38.773056
2336.726826	334895.207288	38.778074
2338.633394	335403.279372	38.783092
2341.370996	335901.144174	38.788109
2343.408780	336389.168368	38.793127
2345.824620	336894.705087	38.798144
2348.143496	337398.677336	38.803162
2350.226692	337911.557065	38.808180
2352.739264	338413.760092	38.813197
2355.066730	338931.888220	38.818215
2357.809514	339454.940493	38.823232
2360.093362	339958.324350	38.828250
2362.492966	340472.994760	38.833268
2364.711752	340987.204069	38.838285
2367.161427	341519.554320	38.843303
2369.372930	342044.553490	38.848320
2372.584582	342568.424572	38.853338
2374.291523	343097.924980	38.858356
2376.887512	343613.989301	38.863373
2379.451105	344147.321176	38.868391
2382.141510	344678.520045	38.873408
2384.930047	345197.015618	38.878426
2386.876600	345720.960346	38.883444
2389.208883	346242.047170	38.888461
2391.815742	346783.978071	38.893479
2394.191761	347305.574051	38.898496
2396.738974	347846.634874	38.903514
2398.985522	348375.435802	38.908532
2401.309413	348899.347716	38.913549
2403.941758	349430.049184	38.918567
2406.612703	349972.779964	38.923584
2409.060003	350510.617772	38.928602
2411.572812	351042.148420	38.933620
2413.844643	351577.029452	38.938637
2416.534560	352107.652787	38.943655
2419.049568	352646.686733	38.948672
2421.720202	353168.421728	38.953690
2423.845521	353709.628304	38.958708
2426.456334	354236.019995	38.963725
2428.441287	354774.137306	38.968743
2430.766649	355302.381134	38.973760
2434.090794	355832.868153	38.978778
2436.329247	356368.864925	38.983796
2439.081631	356907.256355	38.988813
2441.295455	357436.368594	38.993831
2443.514399	357963.088097	38.998848
2446.072280	358490.734129	39.003866
2448.426689	359026.286210	39.008884
2451.123575	359552.244451	39.013901
2453.811352	360100.830291	39.018919
2456.386488	360622.834717	39.023936
2459.264890	361140.980636	39.028954
2461.249909	361666.734434	39.033972
2463.474344	362184.711059	39.038989
2466.035011	362708.227356	39.044007
2468.958797	363244.147234	39.049024
2471.695247	363757.403449	39.054042
2473.999268	364259.338892	39.059060
2476.318649	364747.932625	39.064077
2479.071249	365242.101904	39.069095
2480.745556	365724.723119	39.074112
2483.438539	366211.839916	39.079130
2486.164167	366703.885020	39.084148
2488.414443	367195.920017	39.089165
2490.407893	367698.553891	39.094183
2492.794000	368197.873905	39.099200
2495.652128	368701.444457	39.104218
2497.635784	369216.038843	39.109236
2500.194204	369714.722335	39.114253
2502.736801	370230.401694	39.119271
2505.054404	370757.078180	39.124288
2507.522763	371277.614760	39.129306
2509.588835	371807.781986	39.134324
2512.209417	372331.442139	39.139341
2514.950033	372867.133637	39.144359
2517.197292	373406.641556	39.149376
2520.250835	373946.266091	39.154394
2522.693176	374496.742820	39.159412
2525.182087	375019.105453	39.164429
2527.787508	375567.482887	39.169447
2529.770015	376113.691956	39.174464
2532.142170	376659.297004	39.179482
2534.523790	377227.612433	39.184500
2537.289891	377771.917226	39.189517
2539.602884	378345.969826	39.194535
2541.981328	378915.642900	39.199552
2545.007807	379477.324688	39.204570
2547.415607	380054.263602	39.209588
2550.262409	380632.463584	39.214605
2552.560215	381206.050881	39.219623
2555.198712	381782.636907	39.224640
2557.521816	382358.600925	39.229658
2560.011029	382941.111044	39.234676
2562.897137	383522.532850	39.239693
2565.277710	384111.972738	39.244711
2567.760615	384696.925826	39.249728
2570.635066	385293.250816	39.254746
2572.878050	385882.595215	39.259764
2575.910902	386486.287146	39.264781
2578.426202	387069.129125	39.269799
2580.734208	387665.511882	39.274816
2583.665151	388259.301472	39.279834
2586.027162	388870.839724	39.284852
2588.752868	389459.416637	39.289869
2591.623864	390058.135226	39.294887
2594.230156	390664.780126	39.299904
2597.183605	391265.988242	39.304922
2599.379029	391867.097567	39.309940
2602.401057	392460.417022	39.314957
2605.333425	393059.001777	39.319975
2607.969597	393657.415492	39.324992
2610.247955	394247.161885	39.330010
2612.714600	394852.913711	39.335028
2615.501037	395447.360813	39.340045
2618.182806	396051.934724	39.345063
2620.483611	396650.781541	39.350080
2623.417454	397249.615425	39.355098
2626.030000	397850.762345	39.360116
2628.728996	398435.934641	39.365133
2631.576421	399038.026781	39.370151
2634.176811	399635.130749	39.375168
2636.584994	400237.159311	39.380186
2639.205565	400842.580885	39.385204
2641.711513	401437.274167	39.390221
2644.265598	402015.495159	39.395239
2646.859984	402609.385023	39.400256
2649.694209	403180.396424	39.405274
2652.235057	403754.121684	39.410292
2654.572497	404328.269107	39.415309
2657.479381	404889.408086	39.420327
2659.616995	405471.604195	39.425344
2662.721831	406053.886961	39.430362
2665.322320	406638.713007	39.435380
2667.608515	407216.893438	39.440397
2670.344947	407814.267201	39.445415
2672.490083	408405.139456	39.450432
2675.209903	408981.283277	39.455450
2678.092185	409592.298136	39.460468
2680.633433	410201.578494	39.465485
2683.398321	410796.185360	39.470503
2685.808904	411414.710927	39.475520
2688.294504	412017.625209	39.480538
2691.267416	412638.506877	39.485556
2693.490718	413266.873740	39.490573
2696.763055	413882.006902	39.495591
2699.145263	414514.308730	39.500608
2702.054112	415141.451143	39.505626
2704.950876	415761.647249	39.510644
2707.393052	416401.673263	39.515661
2709.847570	417030.955259	39.520679
2712.915877	417657.694761	39.525696
2715.998133	418312.988724	39.530714
2718.398305	418954.106913	39.535732
2721.056815	419600.525705	39.540749
2724.387565	420229.018231	39.545767
2727.112346	420889.596999	39.550784
2730.229426	421526.022944	39.555802
2732.642872	422166.129467	39.560820
2735.393122	422805.506003	39.565837
2738.846298	423452.387661	39.570855
2741.199514	424101.342146	39.575872
2744.376300	424740.237339	39.580890
2747.141230	425384.434851	39.585908
2749.788038	426031.714233	39.590925
2752.886467	426674.149969	39.595943
2755.527518	427315.777232	39.600960
2758.550944	427950.600685	39.605978
2761.389643	428608.989227	39.610996
2764.003677	429242.470599	39.616013
2767.115148	429882.728291	39.621031
2769.645840	430535.641817	39.626048
2772.346496	431168.693958	39.631066
2775.415631	431810.664510	39.636084
2778.347072	432455.819541	39.641101
2781.278825	433083.972135	39.646119
2783.655551	433737.358665	39.651136
2786.761067	434378.935497	39.656154
2789.945449	435010.321378	39.661172
2792.538948	435656.231092	39.666189
2795.532883	436296.649677	39.671207
2798.232520	436949.876561	39.676224
2801.033319	437573.456461	39.681242
2803.933779	438209.429514	39.686260
2806.479966	438856.703354	39.691277
2809.763852	439491.007097	39.696295
2812.315118	440132.628398	39.701312
2815.054864	440762.528535	39.706330
2817.760375	441402.869764	39.711348
2820.652533	442045.584531	39.716365
2823.673487	442677.144032	39.721383
2826.222947	443319.312640	39.726400
2829.197878	443964.170429	39.731418
2832.002707	444598.880149	39.736436
2834.480312	445205.436627	39.741453
2837.072755	445811.399510	39.746471
2839.938989	446423.309318	39.751488
2842.574230	447035.790200	39.756506
2845.548660	447642.288938	39.761524
2847.915831	448252.346675	39.766541
2850.549736	448868.603609	39.771559
2853.269934	449507.548408	39.776576
2855.693818	450137.125198	39.781594
2858.950100	450773.769856	39.786612
2861.493924	451417.824110	39.791629
2864.127034	452061.235252	39.796647
2866.975889	452709.637853	39.801664
2869.655698	453375.207471	39.806682
2872.437894	454026.096347	39.811700
2874.989354	454694.311715	39.816717
2877.921501	455360.422986	39.821735
2880.700616	456042.028846	39.826752
2883.573472	456713.246286	39.831770
2886.358925	457403.176485	39.836788
2889.528247	458097.712864	39.841805
2892.193142	458781.651516	39.846823
2895.262181	459488.663538	39.851840
2898.413963	460187.357481	39.856858
2901.513667	460867.965815	39.861876
2904.364013	461575.329524	39.866893
2907.057548	462278.803125	39.871911
2910.663285	462977.715290	39.876928
2913.187730	463684.587886	39.881946
2916.149828	464388.385792	39.886964
2918.979151	465092.275881	39.891981
2922.363181	465795.948761	39.896999
2925.517391	466516.779116	39.902016
2927.825727	467218.895489	39.907034
2931.078101	467949.282902	39.912052
2934.251830	468668.705311	39.917069
2937.815874	469368.768785	39.922087
2940.507745	470093.953996	39.927104
2943.636209	470811.373280	39.932122
2946.668792	471514.958438	39.937140
2949.786895	472227.274180	39.942157
2952.680162	472934.551365	39.947175
2955.989080	473652.573571	39.952192
2959.026657	474363.950789	39.957210
2962.103889	475061.223686	39.962228
2965.328675	475788.138304	39.967245
2968.304787	476489.952748	39.972263
2971.562340	477203.639878	39.977280
2974.475910	477906.611615	39.982298
2977.564592	478607.558962	39.987316
2980.072239	479321.318551	39.992333
2983.904856	480034.687472	39.997351
2986.435674	480719.650632	40.002368
2989.574517	481427.470363	40.007386
2992.976861	482124.079395	40.012404
2995.785523	482833.550118	40.017421
2998.807702	483523.252119	40.022439
3001.761219	484219.283217	40.027456
3004.789436	484924.895193	40.032474
3007.679301	485611.249667	40.037492
3010.507071	486320.305611	40.042509
3013.814534	487024.266175	40.047527
3017.161984	487730.858102	40.052544
3019.659194	488421.480554	40.057562
3023.061207	489112.937643	40.062580
3025.633371	489815.322667	40.067597
3029.139883	490509.873011	40.072615
3032.171510	491188.751440	40.077632
3035.314165	491865.365879	40.082650
3038.487339	492517.519694	40.087668
3041.056759	493168.530879	40.092685
3043.927643	493817.603334	40.097703
3046.871859	494465.125391	40.102720
3049.969802	495140.490629	40.107738
3052.968103	495792.931206	40.112756
3055.638712	496466.037009	40.117773
3058.594536	497133.277710	40.122791
3061.547849	497801.294030	40.127808
3064.408156	498481.728783	40.132826
3067.537124	499160.781073	40.137844
3070.271430	499864.125709	40.142861
3072.863644	500545.160552	40.147879
3075.968512	501254.470414	40.152896
3079.111876	501964.192470	40.157914
3082.076443	502675.518056	40.162932
3084.861551	503393.227752	40.167949
3088.133870	504120.688467	40.172967
3091.037093	504835.137277	40.177984
3093.906378	505582.814956	40.183002
3097.057613	506313.906333	40.188020
3099.836093	507060.111781	40.193037
3103.294187	507809.190188	40.198055
3106.532051	508565.406761	40.203072
3109.138695	509313.331093	40.208090
3112.755767	510061.007329	40.213108
3115.571965	510831.302344	40.218125
3118.824205	511589.617074	40.223143
3122.115098	512359.351147	40.228160
3125.042027	513136.089732	40.233178
3128.850457	513899.572393	40.238196
3131.576926	514670.875474	40.243213
3134.732873	515442.520762	40.248231
3137.918376	516228.145733	40.253248
3140.931204	517019.534321	40.258266
3143.965015	517789.910166	40.263284
3146.940953	518589.257069	40.268301
3150.445661	519381.587740	40.273319
3153.768748	520173.247033	40.278336
3156.750864	520970.994790	40.283354
3160.226404	521758.616863	40.288372
3163.261940	522550.533205	40.293389
3166.593030	523342.306268	40.298407
3169.922932	524149.609718	40.303424
3173.403876	524951.263341	40.308442
3176.743235	525738.169582	40.313460
3179.876353	526538.827017	40.318477
3182.566948	527330.462500	40.323495
3185.917561	528128.226433	40.328512
3189.038763	528939.138203	40.333530
3192.258704	529731.701520	40.338548
3195.449796	530542.101168	40.343565
3198.822639	531346.294982	40.348583
3202.245464	532147.116789	40.353600
3205.444989	532951.439058	40.358618
3208.757923	533753.283342	40.363636
3211.442592	534564.615211	40.368653
3214.761460	535360.032111	40.373671
3218.554576	536176.159540	40.378688
3221.679098	536982.450098	40.383706
3224.807324	537779.703942	40.388724
3228.021180	538585.728355	40.393741
3230.828831	539401.150508	40.398759
3234.401432	540202.649340	40.403776
3237.542101	541007.627386	40.408794
3240.810728	541821.917568	40.413812
3243.965565	542623.126654	40.418829
3246.798498	543394.581684	40.423847
3250.068553	544161.154433	40.428864
3253.360487	544950.151600	40.433882
3256.258921	545718.693033	40.438900
3259.432617	546498.379835	40.443917
3262.315917	547280.871640	40.448935
3265.766216	548052.642377	40.453952
3268.950455	548842.009468	40.458970
3272.193462	549633.924219	40.463988
3275.174274	550432.197069	40.469005
3278.798498	551231.319869	40.474023
3281.565242	552044.111731	40.479040
3284.352659	552858.249653	40.484058
3287.757805	553677.700542	40.489076
3290.924085	554497.684490	40.494093
3294.160928	555329.681600	40.499111
3297.781011	556163.064717	40.504128
3300.713618	557002.962450	40.509146
3304.024357	557837.079011	40.514164
3307.518256	558695.412199	40.519181
3310.624290	559544.423994	40.524199
3314.114102	560394.667667	40.529216
3317.063577	561265.726017	40.534234
3320.573455	562116.092838	40.539252
3324.196334	562995.383961	40.544269
3326.942989	563855.011031	40.549287
3330.900327	564736.122442	40.554304
3334.051085	565619.997627	40.559322
3337.640564	566485.759118	40.564340
3341.200521	567372.441342	40.569357
3344.783685	568254.595613	40.574375
3348.380354	569138.582675	40.579392
3351.406258	570011.877602	40.584410
3354.956892	570892.532635	40.589428
3358.095034	571768.579219	40.594445
3361.489233	572661.435469	40.599463
3365.515901	573551.520215	40.604480
3368.631654	574442.277910	40.609498
3371.931470	575323.379181	40.614516
3375.770615	576225.391855	40.619533
3378.797206	577104.344898	40.624551
3382.794274	577990.030997	40.629568
3386.332337	578888.374410	40.634586
3390.148600	579779.349164	40.639604
3393.213417	580655.415500	40.644621
3396.144049	581547.687106	40.649639
3400.263870	582429.599392	40.654656
3403.331087	583320.356155	40.659674
3406.841118	584207.721603	40.664692
3410.385265	585097.459637	40.669709
3413.497645	585989.592322	40.674727
3417.312795	586866.546194	40.679744
3420.682174	587765.191459	40.684762
3424.091199	588647.313199	40.689780
3428.071568	589532.721929	40.694797
3431.346393	590420.766748	40.699815
3435.451135	591297.016420	40.704832
3438.132500	592179.362553	40.709850
3442.039830	593069.637429	40.714868
3445.978530	593939.102367	40.719885
3448.939526	594821.136589	40.724903
3452.752239	595680.089381	40.729920
3455.627976	596557.097970	40.734938
3459.431269	597431.691562	40.739956
3462.894424	598297.527460	40.744973
3466.258421	599169.498789	40.749991
3469.927892	600051.983895	40.755008
3473.213106	600909.130783	40.760013
3476.724023	601722.588633	40.765018
3480.134436	602493.764240	40.770023
3483.259021	603211.137212	40.775028
3486.220905	603867.494423	40.780032
3489.254695	604488.326674	40.785037
3492.143823	605035.602462	40.790042
3494.565567	605533.496531	40.795047
3496.743606	605983.981997	40.800052
3499.065080	606379.751346	40.805056
3501.463065	606723.772537	40.810061
3503.585906	607023.908685	40.815066
3505.956764	607273.079375	40.820071
3507.192654	607472.854968	40.825076
3509.201814	607636.594406	40.830080
3510.685709	607761.001337	40.835085
3511.728788	607839.462027	40.840090
3513.376049	607895.471135	40.845095
3514.483384	607924.856623	40.850100
3515.504367	607910.542871	40.855104
3516.378098	607874.845825	40.860109
3517.574178	607812.290226	40.865114
3518.564992	607714.355394	40.870119
3519.204067	607599.969316	40.875124
3519.819273	607458.276566	40.880128
3520.499620	607302.366704	40.885133
3521.202957	607131.895544	40.890138
3521.940733	606944.909821	40.895143
3521.875235	606753.544452	40.900148
3522.301703	606525.082893	40.905152
3522.695219	606290.968874	40.910157
3522.898596	606063.632440	40.915162
3523.054359	605814.587698	40.920167
3523.663418	605552.559362	40.925172
3523.659906	605277.362882	40.930176
3523.792752	605012.193516	40.935181
3523.590481	604720.003487	40.940186
3523.642633	604439.072537	40.945191
3524.032204	604154.378781	40.950196
3523.982804	603850.532671	40.955200
3523.953980	603561.384938	40.960205
3523.766912	603256.242000	40.965210
3523.946340	602960.740287	40.970215
3523.741999	602656.983518	40.975220
3523.310635	602343.895596	40.980224
3523.081655	602047.531023	40.985229
3522.957401	601740.682359	40.990234
3523.361800	601438.546427	40.995239
3522.733199	601137.714323	41.000244
3523.561636	600828.738063	41.005248
3522.966257	600521.676967	41.010253
3522.906925	600211.519947	41.015258
3522.632954	599890.826050	41.020263
3522.194108	599603.184255	41.025268
3522.359916	599298.270803	41.030272
3522.098511	598999.572363	41.035277
3521.707152	598700.735568	41.040282
3521.980175	598404.790041	41.045287
3521.297277	598113.090698	41.050292
3521.254007	597807.465838	41.055296
3521.099715	597517.069126	41.060301
3520.639739	597223.708249	41.065306
3520.655801	596924.206646	41.070311
3519.988883	596647.684759	41.075316
3519.729293	596361.077951	41.080320
3519.592356	596093.571482	41.085325
3519.692915	595810.949263	41.090330
3519.335301	595533.648910	41.095335
3519.105387	595270.592797	41.100340
3519.038861	594994.034045	41.105344
3518.674202	594735.192167	41.110349
3518.724000	594476.429435	41.115354
3518.276844	594210.676792	41.120359
3517.882744	593954.875432	41.125364
3517.917825	593680.169754	41.130368
3517.657431	593434.451713	41.135373
3517.395509	593204.004175	41.140378
3517.123252	592953.218334	41.145383
3516.571541	592713.339234	41.150388
3516.581985	592464.350963	41.155392
3516.490415	592243.122442	41.160397
3516.109145	591999.193537	41.165402
3516.198469	591774.821455	41.170407
3515.534543	591554.319385	41.175412
3515.842947	591320.235664	41.180416
3515.394446	591097.336126	41.185421
3514.977117	590879.286386	41.190426
3514.983977	590668.880821	41.195431
3514.780315	590458.053174	41.200436
3514.522672	590248.732802	41.205440
3514.429644	590038.280436	41.210445
3513.988727	589831.635899	41.215450
3514.426331	589627.104641	41.220455
3513.607520	589430.181102	41.225460
3513.820534	589228.934080	41.230464
3513.154506	589032.730963	41.235469
3512.973986	588838.452597	41.240474
3512.833427	588648.022672	41.245479
3512.757156	588469.504820	41.250484
3512.762909	588288.365596	41.255488
3512.574952	588110.711126	41.260493
3512.424465	587934.901939	41.265498
3512.194653	587755.444253	41.270503
3511.702729	587583.641464	41.275508
3511.978599	587408.508767	41.280512
3511.779629	587240.663707	41.285517
3511.540651	587075.177642	41.290522
3511.570386	586910.649336	41.295527
3511.024564	586744.554726	41.300532
3510.898957	586585.307855	41.305536
3511.035356	586426.468746	41.310541
3510.458604	586282.974410	41.315546
3510.796684	586119.538647	41.320551
3510.488136	585971.036613	41.325556
3510.555724	585807.588347	41.330560
3510.099029	585673.539760	41.335565
3510.004633	585524.296492	41.340570
3510.165962	585374.058906	41.345575
3509.830995	585243.494500	41.350580
3509.863461	585093.573938	41.355584
3509.731420	584963.776431	41.360589
3509.268030	584818.691315	41.365594
3509.137091	584692.800077	41.370599
3509.103601	584562.230539	41.375604
3509.242507	584431.532244	41.380608
3508.967695	584301.949716	41.385613
3508.644036	584169.716576	41.390618
3508.673445	584042.489510	41.395623
3508.588669	583932.472681	41.400628
3508.461028	583796.494941	41.405632
3508.229145	583689.255738	41.410637
3508.244687	583574.056355	41.415642
3508.349407	583447.161529	41.420647
3508.156101	583333.446045	41.425652
3507.990705	583220.627383	41.430656
3508.142127	583097.180264	41.435661
3507.927891	582988.678180	41.440666
3507.743867	582878.215130	41.445671
3507.614549	582779.623970	41.450676
3507.957336	582658.247607	41.455680
3507.686321	582544.636393	41.460685
3507.426452	582444.508485	41.465690
3507.352324	582350.717783	41.470695
3507.121288	582251.385775	41.475700
3507.274077	582149.636481	41.480704
3507.252502	582044.103139	41.485709
3507.044628	581945.566941	41.490714
3506.917883	581842.705370	41.495719
3506.901662	581762.237143	41.500724
3507.036113	581657.026677	41.505728
3506.766481	581564.212485	41.510733
3506.600064	581463.910660	41.515738
3506.957822	581366.684772	41.520743
3506.555869	581272.384631	41.525748
3506.662971	581185.224316	41.530752
3506.381276	581092.107207	41.535757
3506.318664	581005.824404	41.540762
3506.229673	580919.946185	41.545767
3505.889916	580834.758347	41.550772
3506.067360	580749.138004	41.555776
3506.104253	580671.511658	41.560781
3505.743715	580582.514287	41.565786
3505.994254	580499.036739	41.570791
3505.805598	580423.148791	41.575796
3505.842477	580350.785298	41.580800
3505.639493	580272.140631	41.585805
3505.449489	580197.204093	41.590810
3505.737486	580119.083325	41.595815
3505.516654	580039.487043	41.600820
3505.735320	579960.423234	41.605824
3505.705727	579877.034952	41.610829
3505.173484	579811.225777	41.615834
3505.811144	579730.941466	41.620839
3504.995329	579656.399994	41.625844
3504.906469	579592.074772	41.630848
3505.070562	579512.213949	41.635853
3504.989096	579443.573993	41.640858
3505.245455	579378.992979	41.645863
3505.200061	579320.225871	41.650868
3505.082347	579237.699102	41.655872
3504.816595	579174.652849	41.660877
3504.850349	579119.884262	41.665882
3505.004047	579052.960374	41.670887
3504.699940	579002.055421	41.675892
3504.800014	578929.823257	41.680896
3504.617753	578860.342906	41.685901
3504.334425	578806.274308	41.690906
3504.841755	578747.568227	41.695911
3504.412376	578689.810698	41.700916
3504.803358	578628.213386	41.705920
3504.487805	578557.448037	41.710925
3504.472299	578497.367962	41.715930
3504.730595	578440.253924	41.720935
3504.291332	578386.558737	41.725940
3504.194132	578328.446489	41.730944
3504.468260	578275.441696	41.735949
3504.141977	578208.688088	41.740954
3504.115223	578145.799270	41.745959
3504.159900	578107.574825	41.750964
3504.395114	578045.146030	41.755968
3504.351570	577981.807524	41.760973
3504.300788	577938.180707	41.765978
3504.592476	577874.488258	41.770983
3504.489173	577823.345915	41.775988
3504.365315	577759.216217	41.780992
3504.251317	577699.799277	41.785997
3504.096596	577652.024642	41.791002
3504.121551	577601.764047	41.796007
3504.027006	577544.449813	41.801012
3504.464422	577496.431475	41.806016
3503.897939	577446.764213	41.811021
3503.930840	577382.357064	41.816026
3503.958082	577338.866186	41.821031
3504.059447	577286.736400	41.826036
3504.229025	577229.931003	41.831040
3504.192373	577180.731471	41.836045
3503.487293	577132.539072	41.841050
3503.980922	577078.541288	41.846055
3503.812847	577036.534375	41.851060
3503.609354	576983.347339	41.856064
3503.800130	576933.007663	41.861069
3503.442686	576896.296571	41.866074
3503.668111	576843.844375	41.871079
3503.468788	576805.001551	41.876084
3503.588408	576755.625244	41.881088
3503.808426	576706.132704	41.886093
3503.596722	576664.131217	41.891098
3504.075690	576602.809980	41.896103
3503.259612	576556.739214	41.901108
3503.461917	576511.261475	41.906112
3503.398064	576471.092122	41.911117
3503.343933	576443.762494	41.916122
3503.687168	576400.870683	41.921127
3503.673926	576360.693023	41.926132
3503.656046	576312.339504	41.931136
3503.594412	576264.243429	41.936141
3503.082031	576211.953786	41.941146
3503.189579	576168.395656	41.946151
3503.530429	576143.361205	41.951156
3503.397468	576090.459889	41.956160
3503.731171	576042.200736	41.961165
3503.214449	576016.045979	41.966170
3503.610502	575968.729871	41.971175
3503.026041	575926.232096	41.976180
3503.494666	575875.994744	41.981184
3503.541825	575834.551657	41.986189
3503.240400	575799.232821	41.991194
3503.447966	575762.429692	41.996199
3503.337220	575721.813511	42.001204
3503.678723	575691.109323	42.006208
3503.777529	575632.751802	42.011213
3503.435880	575596.736304	42.016218
3503.170607	575544.956747	42.021223
3503.251581	575509.175894	42.026228
3503.668406	575464.814207	42.031232
3503.237394	575419.932726	42.036237
3502.989543	575369.955624	42.041242
3503.278910	575344.927450	42.046247
3503.353260	575306.688829	42.051252
3503.229470	575267.728551	42.056256
3503.132633	575224.600057	42.061261
3503.225511	575192.930040	42.066266
3503.222448	575147.228063	42.071271
3503.062833	575128.440189	42.076276
3503.249531	575075.785139	42.081280
3503.072046	575043.003109	42.086285
3503.095352	574996.042199	42.091290
3503.235393	574959.046334	42.096295
3503.073936	574927.365163	42.101300
3503.112409	574893.696075	42.106304
3503.104114	574854.967158	42.111309
3503.329604	574818.960850	42.116314
3502.930046	574777.483375	42.121319
3503.173850	574744.985802	42.126324
3503.447744	574704.657010	42.131328
3503.104875	574664.976357	42.136333
3503.250588	574627.978521	42.141338
3503.085175	574578.035192	42.146343
3503.069431	574549.842078	42.151348
3503.007801	574517.441769	42.156352
3503.294313	574480.672291	42.161357
3502.868919	574442.007163	42.166362
3502.823036	574413.015691	42.171367
3502.712031	574376.408358	42.176372
3502.853921	574346.183260	42.181376
3502.842770	574304.442643	42.186381
3503.096350	574282.929695	42.191386
3503.128153	574233.806925	42.196391
3502.954258	574209.551061	42.201396
3503.160281	574172.341620	42.206400
3503.170985	574129.643678	42.211405
3502.705348	574088.575377	42.216410
3502.639834	574055.221081	42.221415
3502.383299	574033.084992	42.226420
3502.366365	573995.056892	42.231424
3502.331387	573974.792610	42.236429
3502.606833	573948.810244	42.241434
3503.126399	573920.582050	42.246439
3502.818681	573886.512527	42.251444
3502.877287	573844.859657	42.256448
3502.818520	573822.441373	42.261453
3502.474722	573797.709452	42.266458
3503.037253	573762.951605	42.271463
3503.118916	573726.663265	42.276468
3502.933712	573691.871571	42.281472
3502.898468	573657.307197	42.286477
3502.880788	573634.731597	42.291482
3502.880843	573601.114841	42.296487
3502.939930	573565.481781	42.301492
3502.847067	573524.001933	42.306496
3503.144401	573490.890299	42.311501
3502.576418	573463.433082	42.316506
3503.220568	573426.855150	42.321511
3503.221571	573393.087105	42.326516
3502.794164	573357.579620	42.331520
3502.806665	573314.777976	42.336525
3502.668850	573285.547110	42.341530
3502.834186	573240.714266	42.346535
3502.373957	573221.117225	42.351540
3502.548109	573190.934179	42.356544
3502.747906	573147.851745	42.361549
3502.435920	573135.406588	42.366554
3502.997702	573104.761304	42.371559
3502.844024	573081.954981	42.376564
3502.761807	573044.485840	42.381568
3502.909864	573008.034293	42.386573
3502.550355	572985.059244	42.391578
3503.144926	572953.404887	42.396583
3502.829113	572909.348433	42.401588
3502.798788	572880.651671	42.406592
3502.583631	572849.926450	42.411597
3502.616173	572820.266333	42.416602
3502.781135	572783.159110	42.421607
3502.722243	572760.989637	42.426612
3502.480771	572722.691305	42.431616
3503.026296	572688.785862	42.436621
3502.431281	572660.427712	42.441626
3502.470024	572625.346844	42.446631
3502.744480	572604.831026	42.451636
3502.645345	572580.258914	42.456640
3502.595510	572544.338604	42.461645
3502.584071	572519.752651	42.466650
3502.897322	572487.087217	42.471655
3502.733573	572467.843957	42.476660
3502.474191	572436.572559	42.481664
3502.790572	572399.390234	42.486669
3502.293565	572370.464062	42.491674
3502.570351	572342.671346	42.496679
3502.661124	572319.574378	42.501684
3502.823560	572292.752835	42.506688
3502.786833	572262.901373	42.511693
3502.621578	572235.328039	42.516698
3503.144310	572192.040960	42.521703
3502.508373	572166.999887	42.526708
3502.611908	572133.212068	42.531712
3502.809900	572109.445562	42.536717
3502.525155	572084.399586	42.541722
3502.632699	572044.338253	42.546727
3502.650656	572022.908044	42.551732
3502.462691	571991.022080	42.556736
3502.506460	571966.827754	42.561741
3502.295268	571932.536545	42.566746
3502.566413	571902.937099	42.571751
3502.583301	571884.517704	42.576756
3502.471394	571847.099440	42.581760
3502.700070	571824.782823	42.586765
3502.519560	571800.673387	42.591770
3502.520784	571761.229866	42.596775
3502.518461	571739.350653	42.601780
3501.842149	571699.962656	42.606784
3502.317091	571685.937590	42.611789
3502.163951	571667.293510	42.616794
3502.639852	571638.263562	42.621799
3502.620241	571608.206977	42.626804
3502.646588	571575.232501	42.631808
3502.601125	571533.185962	42.636813
3502.330635	571518.022637	42.641818
3502.641806	571496.495418	42.646823
3502.265793	571470.759788	42.651828
3502.329757	571434.968739	42.656832
3502.164150	571428.169597	42.661837
3502.121207	571393.298440	42.666842
3502.385909	571374.839480	42.671847
3502.405405	571355.565693	42.676852
3502.221668	571327.441024	42.681856
3502.116219	571309.391114	42.686861
3502.009475	571279.096361	42.691866
3502.285362	571255.717376	42.696871
3502.145481	571238.475691	42.701876
3502.424619	571212.085026	42.706880
3502.076220	571181.727422	42.711885
3502.063172	571169.082819	42.716890
3502.361801	571148.209310	42.721895
3501.962638	571126.892810	42.726900
3502.272419	571107.272112	42.731904
3502.433376	571083.408890	42.736909
3501.704464	571058.480277	42.741914
3502.264631	571025.822247	42.746919
3502.380232	571019.380384	42.751924
3502.591324	570980.754514	42.756928
3502.843316	570968.519928	42.761933
3502.581743	570929.415731	42.766938
3502.454301	570893.401978	42.771943
3502.674071	570873.192716	42.776948
3502.258246	570835.467341	42.781952
3502.562140	570817.151915	42.786957
3502.561468	570793.714848	42.791962
3502.307251	570758.222353	42.796967
3502.351883	570737.538363	42.801972
3502.496116	570712.221560	42.806977
3502.298459	570683.143926	42.811981
3502.136578	570665.402943	42.816986
3502.097355	570637.053232	42.821991
3501.751890	570620.896687	42.826996
3501.924440	570600.895076	42.832001
3502.154665	570570.244639	42.837005
3501.933544	570554.068561	42.842010
3502.542010	570519.042713	42.847015
3502.440120	570506.963333	42.852020
3502.268287	570494.292618	42.857025
3502.434225	570456.976927	42.862029
3502.116456	570434.291328	42.867034
3502.552960	570395.929375	42.872039
3502.451625	570385.355432	42.877044
3502.240712	570361.849969	42.882049
3502.381830	570328.803766	42.887053
3502.056068	570314.249745	42.892058
3502.671149	570280.828177	42.897063
3502.322783	570271.346713	42.902068
3502.170250	570242.762794	42.907073
3502.038244	570211.515567	42.912077
3502.341819	570199.071340	42.917082
3502.427037	570163.523936	42.922087
3502.420716	570148.769197	42.927092
3502.436986	570114.135829	42.932097
3502.309649	570091.871487	42.937101
3502.108924	570063.696173	42.942106
3502.265430	570036.518933	42.947111
3502.483872	570025.944857	42.952116
3501.812028	569997.692460	42.957121
3502.182390	569974.697613	42.962125
3501.966948	569952.396583	42.967130
3502.120501	569936.361820	42.972135
3502.243963	569901.108765	42.977140
3502.220418	569881.538079	42.982145
3502.295525	569861.851557	42.987149
3501.902936	569847.457959	42.992154
3502.145210	569833.717959	42.997159
3502.107424	569812.091556	43.002164
3501.968845	569789.627620	43.007169
3502.281379	569759.263295	43.012173
3502.004383	569744.901689	43.017178
3502.034612	569714.631569	43.022183
3502.087491	569699.264701	43.027188
3501.910678	569670.382001	43.032193
3501.984346	569659.679645	43.037197
3501.702616	569644.314820	43.042202
3502.140433	569619.903352	43.047207
3502.183172	569606.495424	43.052212
3502.124126	569579.400991	43.057217
3502.178150	569549.528252	43.062221
3501.843899	569535.376102	43.067226
3501.911302	569519.755762	43.072231
3502.445047	569497.186150	43.077236
3502.175556	569474.792255	43.082241
3502.249304	569455.205632	43.087245
3501.981169	569430.101041	43.092250
3502.342258	569399.477212	43.097255
3502.030843	569378.043344	43.102260
3502.162401	569359.752535	43.107265
3502.286796	569336.594093	43.112269
3501.998848	569320.577297	43.117274
3502.215586	569297.705499	43.122279
3502.268095	569269.990578	43.127284
3502.066651	569248.489083	43.132289
3502.257618	569234.405034	43.137293
3502.271020	569211.615046	43.142298
3502.403388	569189.960870	43.147303
3502.303713	569171.705911	43.152308
3502.482401	569142.916888	43.157313
3502.326565	569103.488761	43.162317
3502.137514	569088.610642	43.167322
3502.300463	569065.997764	43.172327
3502.519080	569036.750486	43.177332
3501.778728	569005.042935	43.182337
3502.353806	568990.547180	43.187341
3502.307298	568971.530672	43.192346
3502.026890	568941.307076	43.197351
3501.897664	568921.952054	43.202356
3502.051993	568897.382593	43.207361
3501.850459	568876.934510	43.212365
3502.273804	568870.995479	43.217370
3502.221829	568835.866972	43.222375
3502.098777	568822.484048	43.227380
3502.224889	568796.764291	43.232385
3502.326763	568772.403544	43.237389
3502.006035	568755.638150	43.242394
3501.788770	568723.898244	43.247399
3501.887901	568718.110211	43.252404
3502.235277	568691.351713	43.257409
3502.107258	568665.219628	43.262413
3502.000810	568644.806463	43.267418
3502.304513	568616.398149	43.272423
3502.169347	568591.471722	43.277428
3502.046168	568582.706596	43.282433
3502.024842	568552.592065	43.287437
3501.726403	568539.236229	43.292442
3501.986310	568512.039221	43.297447
3502.165675	568504.582048	43.302452
3501.991267	568490.955783	43.307457
3502.074280	568478.142605	43.312461
3502.059890	568446.370217	43.317466
3501.991027	568417.969460	43.322471
3501.848399	568414.076360	43.327476
3502.011324	568380.167793	43.332481
3501.515173	568362.626093	43.337485
3501.646563	568342.928171	43.342490
3501.825508	568330.200226	43.347495
3502.335229	568323.394056	43.352500
3501.667363	568292.426165	43.357505
3501.853919	568274.074837	43.362509
3501.747920	568268.469239	43.367514
3501.844226	568239.540244	43.372519
3501.925237	568217.641279	43.377524
3501.612532	568213.624104	43.382529
3501.760554	568196.433229	43.387533
3501.443957	568174.897528	43.392538
3501.664906	568163.668777	43.397543
3501.865918	568157.412752	43.402548
3501.832282	568144.065258	43.407553
3502.046934	568111.402771	43.412557
3502.270291	568099.721795	43.417562
3501.916607	568071.214114	43.422567
3502.266250	568045.156544	43.427572
3501.960169	568050.575623	43.432577
3502.137610	568011.192048	43.437581
3501.963012	567998.820200	43.442586
3501.880930	567972.428366	43.447591
3502.083056	567964.816690	43.452596
3501.559398	567942.961532	43.457601
3501.956201	567922.920207	43.462605
3501.847418	567918.519654	43.467610
3501.740287	567882.894870	43.472615
3501.584872	567878.401194	43.477620
3501.734175	567865.627172	43.482625
3501.869636	567847.383551	43.487629
3501.490676	567832.784493	43.492634
3501.772529	567814.919533	43.497639
3501.948023	567805.605128	43.502644
3502.015199	567783.456503	43.507649
3502.315903	567764.534322	43.512653
3502.405908	567741.227450	43.517658
3502.215551	567715.002554	43.522663
3502.260224	567704.704515	43.527668
3501.717258	567675.221441	43.532673
3502.045029	567644.045956	43.537677
3502.175368	567629.065819	43.542682
3501.903478	567616.708770	43.547687
3502.121904	567588.712863	43.552692
3501.893539	567573.939332	43.557697
3502.215650	567557.573703	43.562701
3502.050799	567530.942794	43.567706
3501.948844	567512.886363	43.572711
3502.164892	567487.902643	43.577716
3502.212277	567472.182254	43.582721
3502.154209	567440.514326	43.587725
3501.595527	567428.503117	43.592730
3501.653333	567394.557887	43.597735
3501.990776	567374.575093	43.602740
3501.664299	567373.672274	43.607745
3501.466621	567349.003939	43.612749
3501.502805	567346.086556	43.617754
3501.668634	567330.799274	43.622759
3501.711368	567300.822064	43.627764
3501.851792	567292.717574	43.632769
3501.860307	567277.956835	43.637773
3501.795990	567265.767767	43.642778
3501.887239	567250.441836	43.647783
3501.950166	567231.555955	43.652788
3501.633699	567212.377938	43.657793
3501.470273	567202.965424	43.662797
3501.608205	567187.632112	43.667802
3502.056707	567173.254277	43.672807
3501.714800	567171.801626	43.677812
3501.752961	567141.372896	43.682817
3501.801479	567126.003277	43.687821
3502.005435	567112.115421	43.692826
3501.693499	567087.363983	43.697831
3501.778433	567074.197527	43.702836
3501.676357	567059.001971	43.707841
3501.718434	567046.042995	43.712845
3501.322863	567030.642267	43.717850
3502.076184	567007.782455	43.722855
3501.710104	566999.706738	43.727860
3501.847221	566989.494018	43.732865
3501.821742	566971.173769	43.737869
3501.714973	566954.020877	43.742874
3502.049644	566931.728397	43.747879
3501.751043	566908.229578	43.752884
3501.745575	566896.131328	43.757889
3502.043081	566882.730609	43.762893
3502.132594	566861.279578	43.767898
3502.143584	566840.694249	43.772903
3501.795241	566825.938516	43.777908
3501.944368	566806.536427	43.782913
3501.904862	566782.243787	43.787917
3501.700137	566776.903918	43.792922
3501.545720	566765.180246	43.797927
3501.579722	566736.960088	43.802932
3501.736889	566725.037053	43.807937
3501.579278	566703.122317	43.812941
3501.949983	566685.542953	43.817946
3501.874294	566670.794602	43.822951
3501.705966	566658.972587	43.827956
3501.697019	566643.360288	43.832961
3502.391547	566622.918739	43.837965
3502.094138	566600.523615	43.842970
3501.793875	566589.073589	43.847975
3502.119077	566569.141527	43.852980
3501.625571	566562.892806	43.857985
3501.759808	566538.371673	43.862989
3502.022478	566530.950414	43.867994
3501.944849	566507.868084	43.872999
3501.664617	566493.000867	43.878004
3501.373366	566481.850558	43.883009
3501.319440	566446.263233	43.888013
3501.577824	566434.324075	43.893018
3501.576263	566413.539126	43.898023
3501.811758	566413.351667	43.903028
3501.533159	566395.220694	43.908033
3502.025117	566383.797234	43.913037
3501.637076	566371.657832	43.918042
3501.534144	566355.557778	43.923047
3501.420638	566351.006747	43.928052
3501.567628	566333.260999	43.933057
3501.756340	566307.977771	43.938061
3501.595502	566300.371540	43.943066
3501.529195	566279.947917	43.948071
3501.692674	566277.211191	43.953076
3501.713020	566269.325583	43.958081
3501.938509	566239.417469	43.963085
3501.468437	566226.437227	43.968090
3501.849823	566209.307332	43.973095
3501.863914	566179.030456	43.978100
3502.010216	566187.090846	43.983105
3501.656499	566162.143132	43.988109
3501.832074	566143.940764	43.993114
3501.973465	566130.412962	43.998119
3501.938712	566108.829344	44.003124
3501.456839	566098.511778	44.008129
3501.284464	566078.204795	44.013133
3501.594886	566060.784532	44.018138
3501.550379	566055.218452	44.023143
3501.894997	566036.587832	44.028148
3501.595062	566031.463330	44.033153
3501.553828	566013.244444	44.038157
3501.815581	566004.166145	44.043162
3501.343252	565984.357757	44.048167
3501.649042	565979.690824	44.053172
3501.114943	565957.783326	44.058177
3501.605195	565931.447985	44.063181
3501.867523	565925.582837	44.068186
3501.528988	565922.623260	44.073191
3501.367589	565896.941999	44.078196
3501.289202	565884.100972	44.083201
3501.721961	565880.267687	44.088205
3501.761578	565872.228173	44.093210
3501.952766	565859.445393	44.098215
3501.849292	565859.260709	44.103220
3501.333667	565830.069896	44.108225
3501.922414	565812.655959	44.113229
3501.477481	565807.855276	44.118234
3501.464736	565773.665284	44.123239
3501.664496	565765.550453	44.128244
3501.533234	565758.993622	44.133249
3501.464219	565739.623851	44.138253
3501.417618	565730.392709	44.143258
3501.258035	565713.296445	44.148263
3501.391311	565724.723181	44.153268
3501.064430	565708.054732	44.158273
3501.664999	565685.316622	44.163277
3501.647141	565680.549539	44.168282
3501.575625	565674.033529	44.173287
3501.403963	565653.173392	44.178292
3501.120780	565638.104701	44.183297
3501.469727	565639.606605	44.188301
3501.407346	565637.507547	44.193306
3501.287599	565607.049266	44.198311
3501.649110	565591.277219	44.203316
3501.058902	565591.720924	44.208321
3501.676898	565582.988280	44.213325
3501.304323	565565.222163	44.218330
3501.231477	565554.388283	44.223335
3501.477460	565541.948054	44.228340
3501.566456	565536.360855	44.233345
3501.480175	565517.495508	44.238349
3501.414131	565511.380228	44.243354
3501.311322	565513.354450	44.248359
3501.436468	565504.397537	44.253364
3501.617266	565489.708006	44.258369
3501.900590	565461.044092	44.263373
3501.549563	565458.638656	44.268378
3501.630557	565428.048104	44.273383
3501.537733	565423.142005	44.278388
3501.096688	565433.252929	44.283393
3501.445797	565410.001284	44.288397
3501.511903	565395.229143	44.293402
3501.650303	565385.065023	44.298407
3501.655745	565368.595185	44.303412
3501.769177	565351.656549	44.308417
3501.723242	565351.563282	44.313421
3501.466000	565329.109210	44.318426
3501.483624	565311.834020	44.323431
3501.500021	565299.630266	44.328436
3501.515129	565296.113136	44.333441
3501.691994	565276.202049	44.338445
3501.434307	565266.852905	44.343450
3501.861283	565255.388290	44.348455
3501.680441	565232.821667	44.353460
3501.484540	565231.647204	44.358465
3501.943212	565217.867898	44.363469
3501.339534	565195.517936	44.368474
3501.693519	565193.052441	44.373479
3501.669954	565180.503332	44.378484
3501.439994	565155.835372	44.383489
3501.464197	565139.362276	44.388493
3501.423209	565136.355980	44.393498
3501.428966	565122.747788	44.398503
3501.529155	565110.480525	44.403508
3501.426211	565097.893525	44.408513
3501.539689	565085.222466	44.413517
3501.704367	565067.873714	44.418522
3501.663661	565055.578207	44.423527
3501.673953	565045.986146	44.428532
3501.661085	565032.983301	44.433537
3501.955610	565023.798693	44.438541
3501.750041	565007.060060	44.443546
3501.540304	564977.718858	44.448551
3501.604618	564972.637367	44.453556
3501.227339	564963.407098	44.458561
3501.319564	564936.529188	44.463565
3501.444537	564937.513867	44.468570
3501.454215	564932.641748	44.473575
3501.793049	564917.725942	44.478580
3501.702412	564904.082352	44.483585
3501.620638	564879.691913	44.488589
3501.552484	564870.814944	44.493594
3501.260410	564856.951726	44.498599
3501.183753	564845.013105	44.503604
3500.792226	564839.852180	44.508609
3501.654710	564839.466258	44.513613
3501.701622	564834.287002	44.518618
3501.540266	564800.669720	44.523623
3501.554548	564801.420651	44.528628
3501.641580	564787.548298	44.533633
3501.859173	564762.960177	44.538637
3501.664196	564754.705500	44.543642
3501.768716	564737.265235	44.548647
3501.508886	564724.350865	44.553652
3501.243215	564723.990665	44.558657
3501.645068	564703.440871	44.563661
3501.891494	564696.221837	44.568666
3501.703672	564673.655220	44.573671
3501.419520	564647.438041	44.578676
3501.623460	564641.430738	44.583681
3501.675545	564625.906612	44.588685
3501.089490	564611.938419	44.593690
3501.034444	564604.766459	44.598695
3501.384552	564602.201020	44.603700
3501.222698	564600.117325	44.608705
3501.433876	564591.849252	44.613709
3501.323142	564575.647523	44.618714
3501.164869	564558.549354	44.623719
3501.835765	564557.440171	44.628724
3501.097645	564547.462560	44.633729
3501.357470	564533.512678	44.638733
3501.415538	564525.218280	44.643738
3501.316182	564516.797844	44.648743
3501.453449	564527.220855	44.653748
3501.483645	564504.870898	44.658753
3501.685836	564482.293153	44.663757
3501.437702	564482.633201	44.668762
3501.280376	564472.363873	44.673767
3501.558117	564447.012471	44.678772
3501.051138	564431.073342	44.683777
3501.373298	564435.542240	44.688781
3501.180038	564438.685711	44.693786
3501.770042	564421.369935	44.698791
3501.738659	564409.624648	44.703796
3501.697100	564399.035871	44.708801
3501.627807	564384.584904	44.713805
3501.519107	564364.315185	44.718810
3501.486948	564356.737777	44.723815
3501.469093	564340.621630	44.728820
3501.642402	564328.693617	44.733825
3501.634983	564304.792499	44.738829
3501.305521	564309.865462	44.743834
3501.322992	564283.299021	44.748839
3501.349483	564271.845837	44.753844
3501.001745	564281.189943	44.758849
3501.436284	564266.810711	44.763853
3501.339364	564260.498740	44.768858
3501.632325	564228.265020	44.773863
3501.580298	564220.288907	44.778868
3501.667873	564218.417226	44.783873
3501.833753	564189.065532	44.788877
3501.292947	564189.300694	44.793882
3501.697700	564173.419543	44.798887
3501.816907	564151.908657	44.803892
3501.362074	564145.100204	44.808897
3501.385443	564132.040473	44.813901
3501.041665	564114.267634	44.818906
3501.507372	564105.607918	44.823911
3501.510182	564097.020560	44.828916
3501.379631	564094.279075	44.833921
3501.594506	564069.890782	44.838925
3501.513569	564056.043818	44.843930
3501.768175	564048.170300	44.848935
3501.921914	564032.629494	44.853940
3501.512282	564021.796620	44.858945
3501.508036	564006.380909	44.863949
3501.219795	564004.919458	44.868954
3501.402637	563980.033824	44.873959
3501.590648	563963.131729	44.878964
3501.206101	563971.929456	44.883969
3501.712609	563948.851161	44.888973
3501.751119	563933.428670	44.893978
3501.421745	563927.855888	44.898983
3501.722709	563923.239110	44.903988
3501.647563	563896.937352	44.908993
3501.855179	563891.431256	44.913997
3501.183378	563877.073849	44.919002
3501.327657	563864.748167	44.924007
3501.680684	563854.599379	44.929012
3501.552135	563849.597767	44.934017
3501.586148	563826.593095	44.939021
3501.379194	563814.372486	44.944026
3501.553827	563808.519988	44.949031
3501.414846	563792.974407	44.954036
3501.017158	563778.322941	44.959041
3501.233539	563771.861292	44.964045
3500.649098	563771.249590	44.969050
3500.773392	563766.610153	44.974055
3501.397569	563771.684916	44.979060
3501.137684	563767.607709	44.984065
3501.270127	563750.161605	44.989069
3501.159877	563738.227101	44.994074
3501.540427	563724.508469	44.999079
3501.889289	563725.307599	45.004084
3501.196585	563714.368038	45.009089
3501.382254	563689.933302	45.014093
3501.089208	563690.230174	45.019098
3501.162047	563685.548531	45.024103
3501.009901	563670.155497	45.029108
3501.385372	563675.319401	45.034113
3501.313553	563666.793611	45.039117
3501.131311	563656.627895	45.044122
3501.497250	563646.828432	45.049127
3501.498535	563639.546636	45.054132
3500.903302	563623.871285	45.059137
3501.276296	563613.920039	45.064141
3501.502261	563608.360724	45.069146
3501.540627	563605.442062	45.074151
3501.615644	563598.148714	45.079156
3501.458338	563568.645115	45.084161
3501.724366	563556.249858	45.089165
3501.617223	563553.805894	45.094170
3501.426666	563529.730947	45.099175
3501.374295	563520.699828	45.104180
3501.363517	563515.729879	45.109185
3501.669695	563513.773693	45.114189
3501.088674	563497.593767	45.119194
3501.415257	563474.894195	45.124199
3501.744916	563470.473628	45.129204
3501.131861	563453.796465	45.134209
3501.298309	563443.375178	45.139213
3501.383153	563438.239592	45.144218
3501.460703	563430.242683	45.149223
3501.456090	563423.413642	45.154228
3501.640087	563410.177338	45.159233
3501.724407	563394.746975	45.164237
3501.328351	563383.810946	45.169242
3501.145234	563364.053312	45.174247
3501.385595	563358.491628	45.179252
3501.513534	563363.141960	45.184257
3501.515350	563343.455819	45.189261
3501.031350	563333.035680	45.194266
3501.520760	563325.828038	45.199271
3501.303634	563317.374928	45.204276
3501.503852	563306.596706	45.209281
3501.554980	563290.367888	45.214285
3500.950701	563280.569136	45.219290
3501.017001	563288.091632	45.224295
3501.388713	563264.129115	45.229300
3501.527628	563263.404301	45.234305
3501.378904	563239.422655	45.239309
3501.486350	563233.580374	45.244314
3501.002395	563224.817373	45.249319
3501.448983	563232.581771	45.254324
3500.985188	563222.761009	45.259329
3501.330706	563199.706407	45.264333
3501.269132	563191.630645	45.269338
3501.385413	563200.400874	45.274343
3501.421193	563195.674609	45.279348
3501.274010	563176.463457	45.284353
3501.616450	563160.440017	45.289357
3501.323128	563161.289361	45.294362
3501.644255	563151.245392	45.299367
3501.476847	563141.076908	45.304372
3501.570241	563115.349682	45.309377
3501.548294	563107.418327	45.314381
3501.127082	563086.592605	45.319386
3501.226346	563071.812342	45.324391
3501.453594	563066.302790	45.329396
3501.561187	563064.528236	45.334401
3501.512520	563044.598384	45.339405
3501.319449	563036.894614	45.344410
3501.355540	563025.438708	45.349415
3501.573428	563022.943821	45.354420
3501.395392	563014.835923	45.359425
3501.570409	562992.510654	45.364429
3501.092449	562980.482199	45.369434
3501.418391	562976.514014	45.374439
3501.745382	562965.213455	45.379444
3501.250958	562959.063362	45.384449
3501.634151	562945.293187	45.389453
3501.670420	562943.077779	45.394458
3501.456211	562910.467730	45.399463
3501.496627	562902.576708	45.404468
3501.424459	562904.345693	45.409473
3501.274811	562877.852406	45.414477
3501.308154	562877.997829	45.419482
3501.070156	562864.174006	45.424487
3501.447781	562845.834468	45.429492
3501.597483	562857.562777	45.434497
3501.236032	562842.854248	45.439501
3501.320635	562832.093665	45.444506
3501.187699	562827.142521	45.449511
3501.222543	562819.051429	45.454516
3501.364823	562804.615653	45.459521
3501.193677	562783.599635	45.464525
3501.575021	562781.380472	45.469530
3501.223727	562777.769199	45.474535
3501.881077	562774.954452	45.479540
3501.498673	562756.783811	45.484545
3501.202919	562737.193391	45.489549
3501.617857	562734.968969	45.494554
3501.387828	562720.038854	45.499559
3501.628269	562702.976081	45.504564
3501.291579	562697.202964	45.509569
3501.349019	562690.162908	45.514573
3500.846111	562673.065633	45.519578
3501.144237	562660.162194	45.524583
3501.261005	562654.870609	45.529588
3501.211107	562651.362846	45.534593
3501.534343	562651.061177	45.539597
3501.043531	562632.455293	45.544602
3501.111622	562613.711784	45.549607
3501.653357	562610.915072	45.554612
3501.098758	562609.947080	45.559617
3500.675504	562606.296781	45.564621
3500.892804	562611.084109	45.569626
3501.082518	562609.095760	45.574631
3501.412576	562594.278816	45.579636
3501.361551	562581.680984	45.584641
3501.700175	562566.310221	45.589645
3501.605082	562558.088595	45.594650
3501.606478	562537.497163	45.599655
3501.618014	562535.888214	45.604660
3501.750052	562537.575108	45.609665
3501.923984	562512.185526	45.614669
3501.715094	562501.219409	45.619674
3501.364181	562478.523377	45.624679
3501.747820	562458.625392	45.629684
3501.840489	562457.907759	45.634689
3501.841161	562427.422353	45.639693
3501.681803	562414.238602	45.644698
3501.692690	562409.566135	45.649703
3501.441341	562385.799676	45.654708
3501.064477	562369.636491	45.659713
3500.644958	562360.260088	45.664717
3501.061746	562363.057627	45.669722
3501.585985	562358.606227	45.674727
3501.715076	562351.353873	45.679732
3501.537104	562332.648382	45.684737
3501.537294	562321.448518	45.689741
3501.319889	562317.916618	45.694746
3500.761750	562286.513736	45.699751
3500.990753	562274.876269	45.704756
3501.034513	562286.471041	45.709761
3500.826355	562276.659740	45.714765
3501.615313	562276.737269	45.719770
3501.770835	562278.571201	45.724775
3501.869993	562258.767574	45.729780
3501.644233	562249.260344	45.734785
3501.262912	562231.540731	45.739789
3501.590158	562208.386593	45.744794
3501.204710	562191.069355	45.749799
3501.227197	562184.134908	45.754804
3501.255976	562191.663973	45.759809
3501.408492	562176.824035	45.764813
3501.590577	562141.236901	45.769818
3501.196909	562081.029287	45.774823
3501.108941	561975.671742	45.779828
3501.129047	561833.029123	45.784833
3500.450333	561629.218053	45.789837
3500.163042	561394.653396	45.794842
3499.683635	561101.095657	45.799847
3499.268376	560768.240776	45.804852
3498.643132	560386.835442	45.809857
3497.857580	559960.484005	45.814861
3497.826499	559502.300760	45.819866
3496.621570	558998.617481	45.824871
3496.041489	558441.410251	45.829876
3494.504923	557860.310607	45.834881
3493.782836	557221.575083	45.839885
3492.501838	556553.397286	45.844890
3491.426047	555847.361506	45.849895
3490.387349	555095.949339	45.854900
3488.897936	554313.350921	45.859905
3487.830912	553485.149767	45.864909
3486.446035	552615.674575	45.869914
3484.425037	551714.215683	45.874919
3483.091518	550776.989915	45.879924
3481.192007	549813.234866	45.884929
3480.099630	548799.450180	45.889933
3478.403095	547769.182874	45.894938
3475.931759	546705.206778	45.899943
3474.502257	545602.451617	45.904948
3472.488470	544481.029219	45.909953
3470.365028	543306.806033	45.914957
3468.256956	542128.948460	45.919962
3465.825083	540904.391631	45.924967
3463.850744	539661.580289	45.929972
3461.455410	538398.986298	45.934977
3459.101827	537094.840948	45.939981
3456.857546	535771.922078	45.944986
3454.124675	534434.495981	45.949991
3452.197927	533065.441122	45.954996
3449.301138	531679.224074	45.960001
3446.732502	530270.047779	45.965005
3444.215537	528842.229317	45.970010
3441.820547	527388.600577	45.975015
3438.697503	525910.193389	45.980020
3435.948034	524432.217620	45.985025
3433.491560	522928.286885	45.990029
3430.138109	521412.183998	45.995034
3427.496709	519884.107716	46.000039
3424.479369	518323.107916	46.005044
3421.408072	516763.751981	46.010049
3418.515154	515183.522096	46.015053
3415.329636	513583.393243	46.020058
3412.001655	511982.294862	46.025063
3409.170734	510374.378940	46.030068
3406.051197	508760.422729	46.035073
3402.840077	507113.510140	46.040077
3399.679384	505461.807708	46.045082
3396.228143	503811.472888	46.050087
3393.156778	502146.205779	46.055092
3389.594834	500474.313542	46.060097
3386.437904	498782.533188	46.065101
3383.354400	497088.778985	46.070106
3379.334157	495385.334519	46.075111
3376.275230	493674.122351	46.080116
3372.762270	491973.085173	46.085121
3369.818561	490250.557144	46.090125
3366.059863	488521.697754	46.095130
3362.159511	486791.249783	46.100135
3358.936424	485051.660312	46.105140
3354.824735	483325.805739	46.110145
3351.880627	481584.772645	46.115149
3348.486765	479846.344823	46.120154
3344.432083	478095.093035	46.125159
3341.456943	476335.493351	46.130164
3337.743891	474597.854490	46.135169
3334.208982	472830.122772	46.140173
3330.381975	471074.074945	46.145178
3326.657883	469323.333822	46.150183
3322.967785	467552.729282	46.155188
3319.305175	465796.193709	46.160193
3315.933461	464026.327493	46.165197
3312.136891	462256.543977	46.170202
3307.915471	460491.246073	46.175207
3304.388657	458723.582793	46.180212
3300.705003	456962.998747	46.185217
3297.437504	455194.731888	46.190221
3293.474800	453427.002419	46.195226
3289.614798	451663.230349	46.200231
3285.943536	449898.646354	46.205236
3282.114386	448147.633285	46.210241
3278.282230	446374.071671	46.215245
3275.106729	444608.437921	46.220250
3271.184606	442851.360315	46.225255
3267.564166	441082.774680	46.230260
3263.409163	439327.426459	46.235265
3259.840529	437564.528496	46.240269
3256.349576	435803.278573	46.245274
3252.356683	434046.707764	46.250279
3248.356844	432279.844382	46.255284
3244.622004	430523.370373	46.260289
3241.072070	428787.590275	46.265293
3237.440399	427029.015608	46.270298
3233.108577	425275.261910	46.275303
3229.497601	423530.570525	46.280308
3225.617204	421787.394148	46.285313
3221.966542	420043.172124	46.290317
3218.122640	418304.056284	46.295322
3214.272854	416577.778446	46.300327
3210.852439	414846.626813	46.305332
3207.161930	413113.145331	46.310337
3203.169955	411376.528109	46.315341
3199.688123	409642.431518	46.320346
3195.358949	407917.766042	46.325351
3191.944330	406193.330606	46.330356
3188.070839	404463.557297	46.335361
3184.093756	402738.234407	46.340365
3180.541677	401030.576767	46.345370
3176.243150	399323.213742	46.350375
3173.123887	397606.405587	46.355380
3168.868189	395908.733988	46.360385
3165.611878	394190.277799	46.365389
3161.786047	392490.214605	46.370394
3157.739925	390788.543570	46.375399
3154.046239	389088.450724	46.380404
3150.110792	387396.605756	46.385409
3146.450040	385686.755170	46.390413
3142.466639	384000.655457	46.395418
3139.021033	382324.999586	46.400423
3134.627372	380636.102374	46.405428
3131.323666	378958.251727	46.410433
3127.630920	377282.844151	46.415437
3123.897962	375608.810797	46.420442
3119.912239	373933.773335	46.425447
3116.296856	372260.048465	46.430452
3112.395450	370592.643030	46.435457
3108.636551	368932.076619	46.440461
3104.861371	367272.050325	46.445466
3100.880820	365617.269929	46.450471
3097.443294	363953.518484	46.455476
3093.408203	362309.840146	46.460481
3089.765740	360655.005960	46.465485
3085.945928	359016.423481	46.470490
3081.962191	357379.455596	46.475495
3078.493592	355744.785363	46.480500
3074.421596	354109.767844	46.485505
3070.968413	352477.695277	46.490509
3067.431229	350846.670948	46.495514
3063.571620	349220.927849	46.500519
3060.085583	347602.850384	46.505524
3056.049925	345975.347960	46.510529
3052.433367	344354.082970	46.515533
3048.513417	342737.517667	46.520538
3044.932885	341128.985900	46.525543
3041.247301	339507.937004	46.530548
3037.509107	337912.226507	46.535553
3033.847352	336294.359851	46.540557
3030.183264	334683.949890	46.545562
3026.039381	333090.000181	46.550567
3022.518127	331481.464817	46.555572
3018.948938	329889.783587	46.560577
3014.986159	328291.866980	46.565581
3011.292531	326691.859565	46.570586
3007.453680	325104.911583	46.575591
3003.695616	323518.423408	46.580596
3000.062113	321946.635550	46.585601
2996.712528	320359.683674	46.590605
2992.937294	318787.190434	46.595610
2989.240422	317203.458822	46.600615
2985.261279	315638.950020	46.605620
2981.854264	314067.478320	46.610625
2978.394284	312491.609908	46.615629
2974.535727	310914.427433	46.620634
2970.717577	309344.489596	46.625639
2966.808348	307782.047654	46.630644
2963.019544	306219.919143	46.635649
2959.151095	304673.736768	46.640653
2955.814370	303114.241476	46.645658
2952.027251	301564.950477	46.650663
2948.169685	300021.046716	46.655668
2944.552349	298470.062258	46.660673
2941.009921	296930.349436	46.665677
2937.576331	295390.577886	46.670682
2933.711177	293848.669391	46.675687
2929.835753	292311.838925	46.680692
2926.044981	290773.759931	46.685697
2922.701916	289245.831747	46.690701
2918.766480	287707.827706	46.695706
2915.229095	286178.380686	46.700711
2912.005501	284647.678547	46.705716
2908.130604	283128.296797	46.710721
2904.235896	281599.159967	46.715725
2900.681212	280077.168163	46.720730
2896.813219	278567.160460	46.725735
2893.563496	277048.649671	46.730740
2889.478343	275521.150587	46.735745
2885.534104	273996.375988	46.740749
2882.312886	272490.913518	46.745754
2878.177088	270987.044620	46.750759
2875.222207	269464.836037	46.755764
2871.242107	267961.223559	46.760769
2867.668692	266459.127984	46.765773
2864.098037	264953.418704	46.770778
2859.841557	263461.494465	46.775783
2856.663912	261959.551190	46.780788
2852.580118	260475.631301	46.785793
2849.041916	258977.015304	46.790797
2845.323295	257494.274103	46.795802
2841.578501	256012.767411	46.800807
2838.273774	254515.411620	46.805812
2834.356415	253042.965475	46.810817
2830.933414	251564.289681	46.815821
2827.158165	250093.116688	46.820826
2823.670588	248619.618883	46.825831
2820.444336	247133.002868	46.830836
2816.405401	245662.979675	46.835841
2813.032059	244184.895528	46.840845
2809.227607	242710.434142	46.845850
2805.225075	241238.592135	46.850855
2801.795343	239759.062416	46.855860
2797.869346	238314.443399	46.860865
2794.349679	236836.084561	46.865869
2790.815424	235379.242815	46.870874
2787.112403	233931.590905	46.875879
2783.611663	232457.593471	46.880884
2779.792818	231008.168483	46.885889
2776.601897	229551.867504	46.890893
2772.907806	228105.295677	46.895898
2769.263774	226664.801591	46.900903
2765.809701	225201.711418	46.905908
2761.722732	223755.886323	46.910913
2758.115580	222308.204045	46.915917
2754.573406	220860.207411	46.920922
2750.481082	219422.206425	46.925927
2747.617347	217980.093952	46.930932
2743.721001	216544.972253	46.935937
2739.791201	215113.527601	46.940941
2735.860503	213668.436900	46.945946
2732.510320	212242.362659	46.950951
2728.768957	210803.851004	46.955956
2725.224608	209391.981075	46.960961
2721.601314	207965.283229	46.965965
2718.146164	206536.937669	46.970970
2714.510139	205117.798080	46.975975
2711.198887	203697.344164	46.980980
2706.900831	202278.710538	46.985985
2703.511728	200859.665851	46.990989
2699.976083	199446.335173	46.995994
2696.279022	198032.864014	47.000999
2692.491092	196630.192646	47.006004
2688.804102	195218.656936	47.011009
2685.177450	193807.355553	47.016013
2681.144808	192409.120446	47.021018
2677.653278	191006.741880	47.026023
2674.298249	189608.585586	47.031028
2670.559675	188225.530508	47.036033
2667.051941	186833.467621	47.041037
2663.039785	185446.441827	47.046042
2659.759195	184060.720795	47.051047
2656.564709	182670.549479	47.056052
2652.660688	181287.511558	47.061057
2649.140682	179900.843849	47.066061
2645.468496	178513.024490	47.071066
2641.507605	177144.419598	47.076071
2638.263298	175755.673703	47.081076
2634.522452	174367.627103	47.086081
2630.834760	172988.940161	47.091085
2627.432910	171617.043352	47.096090
2623.847829	170245.339877	47.101095
2620.334049	168877.074786	47.106100
2616.435810	167502.530922	47.111105
2612.819406	166134.079600	47.116109
2608.973710	164761.617949	47.121114
2605.406513	163398.419723	47.126119
2601.992852	162044.339051	47.131124
2598.336844	160683.718735	47.136129
2594.527824	159321.967878	47.141133
2590.814212	157964.050229	47.146138
2587.146887	156610.966557	47.151143
2583.807753	155270.983736	47.156148
2579.737905	153925.508025	47.161153
2576.390837	152571.335100	47.166157
2572.830418	151222.140379	47.171162
2568.842633	149885.847526	47.176167
2565.591099	148539.864748	47.181172
2561.661487	147212.587907	47.186177
2558.397749	145839.240574	47.191181
2554.986235	144468.217933	47.196186
2551.019606	143138.265291	47.201191
2547.818028	141787.743330	47.206196
2544.000118	140466.656933	47.211201
2540.422420	139127.489767	47.216205
2536.819105	137788.949648	47.221210
2533.089024	136483.240332	47.226215
2529.793271	135164.752749	47.231220
2526.182827	133844.877025	47.236225
2522.180463	132515.827853	47.241229
2519.119410	131186.607945	47.246234
2514.753422	129883.137249	47.251239
2511.521917	128552.358843	47.256244
2508.023689	127244.495785	47.261249
2504.082417	125936.933879	47.266253
2500.553376	124624.655851	47.271258
2496.785453	123315.675391	47.276263
2493.383457	122022.527076	47.281268
2489.680293	120706.716469	47.286273
2485.791859	119407.193524	47.291277
2482.301995	118110.233530	47.296282
2478.913498	116821.529267	47.301287
2475.344230	115529.260696	47.306292
2471.619206	114234.175018	47.311297
2468.086788	112945.322461	47.316301
2464.499984	111655.227277	47.321306
2460.687357	110377.978649	47.326311
2457.394695	109092.011287	47.331316
2453.463415	107806.483335	47.336321
2450.098158	106530.258223	47.341325
2446.618000	105247.170402	47.346330
2443.100319	103966.857214	47.351335
2439.707761	102684.971626	47.356340
2435.948932	101405.861996	47.361345
2432.182601	100132.827896	47.366349
2428.898356	98852.943052	47.371354
2424.878758	97583.289730	47.376359
2421.545072	96312.397730	47.381364
2417.461436	95046.732022	47.386369
2414.109977	93779.617865	47.391373
2410.527035	92509.453096	47.396378
2406.551254	91262.807921	47.401383
2402.937279	90002.155208	47.406388
2399.172278	88744.526607	47.411393
2395.681548	87483.147466	47.416397
2392.112863	86239.950930	47.421402
2388.234707	84998.862820	47.426407
2384.840865	83747.983150	47.431412
2381.121425	82516.301166	47.436417
2377.648541	81272.503176	47.441421
2374.289011	80036.274320	47.446426
2370.340781	78808.752695	47.451431
2366.922863	77573.429616	47.456436
2363.148009	76343.310499	47.461441
2359.749452	75115.969114	47.466445
2356.049867	73889.987637	47.471450
2351.823162	72665.008075	47.476455
2348.455643	71440.242492	47.481460
2345.000378	70238.529175	47.486465
2341.412667	69025.737767	47.491469
2337.547617	67802.546768	47.496474
2333.644313	66593.632163	47.501479
2330.026603	65394.542993	47.506484
2326.328977	64200.714818	47.511489
2322.797733	63010.204761	47.516493
2319.740565	61814.403257	47.521498
2315.577069	60628.757773	47.526503
2312.080092	59439.543084	47.531508
2308.549376	58254.255877	47.536513
2304.749061	57076.987506	47.541517
2300.931959	55885.369883	47.546522
2297.110630	54719.723570	47.551527
2293.469193	53542.464444	47.556532
2289.957686	52383.730018	47.561537
2286.489216	51224.881146	47.566541
2282.445464	50057.134279	47.571546
2278.813529	48900.114315	47.576551
2275.484953	47747.525988	47.581556
2272.031467	46598.345122	47.586561
2268.152940	45451.419891	47.591565
2264.462853	44302.170750	47.596570
2260.350515	43171.316289	47.601575
2256.925606	42024.565342	47.606580
2253.356119	40897.628967	47.611585
2249.433409	39781.482969	47.616589
2245.575012	38655.176357	47.621594
2241.628118	37535.782682	47.626599
2238.185866	36422.796368	47.631604
2234.475207	35323.437544	47.636609
2230.667509	34219.916277	47.641613
2226.906275	33118.948915	47.646618
2222.927810	32035.883300	47.651623
2219.533279	30945.658622	47.656628
2215.273332	29876.210607	47.661633
2211.700921	28810.259085	47.666637
2207.999958	27745.136940	47.671642
2204.424465	26697.799150	47.676647
2200.327265	25634.559940	47.681652
2196.338253	24590.772690	47.686657
2192.227700	23555.503801	47.691661
2188.077736	22533.858246	47.696666
2183.365232	21534.373138	47.701671
2178.209863	20572.007971	47.706676
2172.843627	19631.506321	47.711681
2167.189232	18721.542263	47.716685
2162.104997	17833.509295	47.721690
2157.040720	16985.528258	47.726695
2152.108080	16149.970372	47.731700
2147.245760	15351.583180	47.736705
2142.553300	14577.906160	47.741709
2138.456872	13833.486070	47.746714
2133.347912	13107.379198	47.751719
2128.991093	12399.649389	47.756724
2124.978638	11716.082308	47.761729
2120.697381	11057.664087	47.766733
2116.677129	10421.232292	47.771738
2112.406743	9801.211113	47.776743
2108.265688	9173.830660	47.781748
2104.568557	8593.922646	47.786753
2100.622892	8017.268462	47.791757
2096.719104	7442.746279	47.796762
2092.981528	6897.875352	47.801767
2089.003944	6345.731253	47.806772
2085.277523	5817.826061	47.811777
2081.357884	5308.559185	47.816781
2077.618770	4794.660984	47.821786
2073.845966	4301.545288	47.826791
2069.869211	3801.376892	47.831796
2066.165521	3333.098893	47.836801
2062.097203	2872.247096	47.841805
2058.433571	2412.891031	47.846810
2054.331434	1965.477727	47.851815
2050.031862	1536.996059	47.856820
2045.919482	1139.863426	47.861825
2041.532663	741.700452	47.866829
2035.528055	397.060373	47.871834
2028.044302	134.032355	47.876839
2012.464617	127.250674	47.881844
2000.219553	139.272004	47.886849
1993.448711	143.093481	47.891853
1990.943654	141.849724	47.896858
1989.103820	149.809916	47.901863
1988.524696	146.382308	47.906868
1987.857280	148.628640	47.911873
1986.419411	153.605705	47.916877
1984.219706	142.809969	47.921882
1981.288063	147.356365	47.926887
1978.225683	149.964797	47.931892
1974.495720	150.921756	47.936897
1970.903100	150.756206	47.941901
1967.828698	138.774858	47.946906
1965.154033	154.610785	47.951911
1962.223588	135.662269	47.956916
1958.664650	139.936656	47.961921
1954.886031	143.726550	47.966925
1952.138688	139.556191	47.971930
1948.719661	144.678746	47.976935
1945.307210	144.114842	47.981940
1942.080224	146.489606	47.986945
1938.539025	141.494319	47.991949
1935.578907	144.570828	47.996954
1932.081392	147.592222	48.001959
1928.735395	147.457699	48.006964
1925.684081	146.774013	48.011969
1921.912494	148.499990	48.016973
1918.414471	140.017724	48.021978
1914.908321	144.878668	48.026983
1911.538995	146.971985	48.031988
1908.784754	146.058314	48.036993
1905.211649	143.289052	48.041997
1901.444612	140.113528	48.047002
1898.001335	138.735028	48.052007
1894.725028	144.331988	48.057012
1891.334332	142.673171	48.062017
1887.897283	138.253245	48.067021
1884.743938	134.371074	48.072026
1880.816423	145.843957	48.077031
1877.428142	138.508830	48.082036
1874.203186	146.701605	48.087041
1870.901538	144.914961	48.092045
1867.606048	144.753571	48.097050
1863.955362	139.854542	48.102055
1860.618705	136.194058	48.107060
1857.147585	143.849538	48.112065
1853.609994	141.868862	48.117069
1849.786219	139.448904	48.122074
1846.760215	141.472694	48.127079
1842.984515	140.870753	48.132084
1839.804927	140.678579	48.137089
1836.038254	140.435906	48.142093
1832.720628	135.927708	48.147098
1829.080276	139.253066	48.152103
1825.879718	140.782144	48.157108
1822.232964	139.856303	48.162113
1818.817635	140.536281	48.167117
1815.642227	137.907302	48.172122
1811.990078	136.026829	48.177127
1808.533257	137.453642	48.182132
1805.065968	136.154864	48.187137
1801.439133	132.865688	48.192141
1798.252465	129.944241	48.197146
1794.702749	143.408192	48.202151
1791.336674	139.853578	48.207156
1787.763132	139.821150	48.212161
1784.487853	139.042838	48.217165
1780.850005	136.021156	48.222170
1777.150493	146.664263	48.227175
1773.871765	136.262089	48.232180
1770.526859	143.344167	48.237185
1766.696187	149.125998	48.242189
1763.260293	142.620964	48.247194
1760.078070	147.108548	48.252199
1756.379187	140.809194	48.257204
1753.195966	143.180326	48.262209
1749.371725	137.172685	48.267213
1746.054428	135.205030	48.272218
1742.433194	145.247421	48.277223
1738.874296	140.947861	48.282228
1735.641164	137.799581	48.287233
1731.794345	142.590502	48.292237
1728.589093	143.971643	48.297242
1725.010220	140.773067	48.302247
1721.857849	130.373290	48.307252
1718.244840	134.317680	48.312257
1714.714805	137.508748	48.317261
1711.499938	127.536384	48.322266
1707.663629	131.215159	48.327271
1704.001742	134.458503	48.332276
1700.586298	132.341705	48.337281
1696.819040	133.564031	48.342285
1693.805426	132.975758	48.347290
1690.198481	146.508804	48.352295
1686.906075	135.105869	48.357300
1683.699339	141.277307	48.362305
1679.727125	138.693980	48.367309
1676.060913	133.000170	48.372314
1672.599603	131.513835	48.377319
1669.374001	127.905644	48.382324
1665.587994	124.559173	48.387329
1661.951245	126.105944	48.392333
1658.971360	128.195335	48.397338
1655.486604	140.911975	48.402343
1651.850998	129.727292	48.407348
1648.765981	135.452569	48.412353
1645.054723	131.531243	48.417357
1641.592183	121.018691	48.422362
1637.984999	132.960369	48.427367
1634.145044	123.762930	48.432372
1630.775304	136.211629	48.437377
1627.142273	127.228586	48.442381
1623.624387	119.594303	48.447386
1620.320509	131.966253	48.452391
1616.777886	127.825552	48.457396
1613.835739	133.053901	48.462401
1609.836189	120.885302	48.467405
1606.350569	120.573415	48.472410
1602.685419	125.728257	48.477415
1599.146595	121.504710	48.482420
1596.094763	126.351586	48.487425
1592.103273	127.257858	48.492429
1588.996695	129.091844	48.497434
1585.254074	122.679188	48.502439
1581.808642	121.418198	48.507444
1578.570192	126.047507	48.512449
1574.723021	141.703141	48.517453
1571.336710	127.913607	48.522458
1568.105687	131.405942	48.527463
1564.409492	127.896753	48.532468
1561.020631	123.004327	48.537473
1557.464038	125.095423	48.542477
1554.168603	120.539563	48.547482
1550.416923	125.309322	48.552487
1547.055159	125.402023	48.557492
1543.610027	121.796599	48.562497
1539.765718	125.261542	48.567501
1536.880782	121.021098	48.572506
1532.987797	119.766898	48.577511
1529.476903	128.137382	48.582516
1526.246899	124.428689	48.587521
1522.326800	127.728326	48.592525
1518.845769	118.180529	48.597530
1515.425439	130.671970	48.602535
1511.734778	124.466352	48.607540
1508.955425	117.058216	48.612545
1504.837219	120.518584	48.617549
1501.437724	117.276202	48.622554
1497.986601	120.277810	48.627559
1494.036483	127.714118	48.632564
1491.012731	120.094299	48.637569
1487.579118	128.136316	48.642573
1483.613315	115.548040	48.647578
1480.213524	121.370082	48.652583
1477.288489	112.247820	48.657588
1473.719315	108.734609	48.662593
1470.027707	117.579491	48.667597
1466.514465	115.531871	48.672602
1463.064711	123.013257	48.677607
1459.157014	120.321847	48.682612
1456.480345	119.149382	48.687617
1452.779785	112.856756	48.692621
1449.246637	111.078020	48.697626
1445.347875	115.212758	48.702631
1442.098880	113.297795	48.707636
1438.612888	111.654054	48.712641
1434.687646	119.526257	48.717645
1431.553718	110.914448	48.722650
1428.117846	114.679336	48.727655
1424.527283	112.507790	48.732660
1420.847272	107.265517	48.737665
1417.600544	114.110843	48.742669
1414.087209	118.795880	48.747674
1410.427040	118.258277	48.752679
1406.969038	110.469179	48.757684
1404.040029	110.959271	48.762689
1400.077982	115.243139	48.767693
1396.438518	106.587089	48.772698
1392.799096	117.822004	48.777703
1389.730928	111.857532	48.782708
1385.742389	111.437780	48.787713
1382.075247	114.213805	48.792717
1379.063653	118.377378	48.797722
1375.565511	113.416708	48.802727
1371.745609	117.940934	48.807732
1368.614202	106.221880	48.812737
1365.073643	117.431835	48.817741
1361.519583	109.610336	48.822746
1358.109868	117.768868	48.827751
1354.763469	111.993497	48.832756
1351.553225	106.633424	48.837761
1347.159344	122.127900	48.842765
1343.810304	114.230019	48.847770
1340.573289	120.918819	48.852775
1336.860031	117.481999	48.857780
1333.479179	111.870221	48.862785
1330.178851	110.944118	48.867789
1326.672716	105.965739	48.872794
1322.708070	115.432383	48.877799
1319.419565	108.031251	48.882804
1316.086625	97.742183	48.887809
1312.603527	114.454532	48.892813
1309.264361	117.704435	48.897818
1305.532512	117.662158	48.902823
1302.160741	114.766695	48.907828
1298.699813	110.901241	48.912833
1294.992898	114.850973	48.917837
1291.673642	109.906627	48.922842
1288.147953	115.178944	48.927847
1284.436963	118.177007	48.932852
1281.018925	108.907365	48.937857
1276.991241	114.713859	48.942861
1273.499354	116.276053	48.947866
1270.000099	108.116977	48.952871
1266.973336	118.335346	48.957876
1264.062699	107.666966	48.962881
1260.132374	113.018454	48.967885
1256.629179	114.493837	48.972890
1253.119447	115.799398	48.977895
1249.555361	110.387184	48.982900
1245.949864	115.064554	48.987905
1242.262970	108.488300	48.992909
1239.091795	103.992204	48.997914
1235.448587	112.465737	49.002919
1231.933502	106.672530	49.007924
1228.665696	100.907056	49.012929
1224.669685	107.521710	49.017933
1221.219779	104.084842	49.022938
1217.932921	119.526277	49.027943
1214.447331	113.975235	49.032948
1211.188465	115.032725	49.037953
1206.933020	111.876996	49.042957
1203.950898	112.713990	49.047962
1200.418848	114.788708	49.052967
1196.850691	113.771700	49.057972
1193.201276	110.748897	49.062977
1189.670355	112.665250	49.067981
1186.553345	110.960673	49.072986
1183.111287	117.263991	49.077991
1179.382075	116.158305	49.082996
1176.531502	99.937549	49.088001
1172.316323	109.506738	49.093005
1169.330645	110.717630	49.098010
1165.712025	112.173149	49.103015
1161.815688	109.815451	49.108020
1158.289451	107.339703	49.113025
1154.936899	115.293184	49.118029
1151.797610	104.489801	49.123034
1147.702590	116.087180	49.128039
1143.903695	112.160800	49.133044
1140.946146	109.662465	49.138049
1137.374453	110.060260	49.143053
1133.765578	103.943249	49.148058
1130.395132	110.149946	49.153063
1126.945189	105.697534	49.158068
1123.530774	107.000873	49.163073
1119.800353	110.514574	49.168077
1116.418475	102.134705	49.173082
1112.672221	113.879975	49.178087
1109.249017	112.995333	49.183092
1105.943482	111.693629	49.188097
1102.631279	112.632953	49.193101
1098.962533	100.843117	49.198106
1095.168614	106.894656	49.203111
1091.785305	111.682825	49.208116
1088.490645	116.343220	49.213121
1084.885248	118.375676	49.218125
1081.513654	105.248485	49.223130
1077.997483	112.588513	49.228135
1074.426976	110.692377	49.233140
1071.012712	115.197493	49.238145
1067.395511	117.772817	49.243149
1063.947796	110.592870	49.248154
1060.021046	116.570306	49.253159
1056.769711	111.428752	49.258164
1053.485422	106.830208	49.263169
1049.860661	112.665451	49.268173
1045.940440	105.705028	49.273178
1042.544598	110.941272	49.278183
1038.941210	112.755127	49.283188
1035.718104	106.533465	49.288193
1032.584264	115.256346	49.293197
1029.220825	112.125558	49.298202
1025.443997	111.603203	49.303207
1022.131478	110.656970	49.308212
1018.483492	105.074489	49.313217
1014.592330	114.861929	49.318221
1011.358555	108.366694	49.323226
1007.582801	107.660677	49.328231
1004.207295	104.525462	49.333236
1000.937074	94.612698	49.338241
997.391439	100.397599	49.343245
994.013072	102.897587	49.348250
990.327429	105.619697	49.353255
986.755283	109.690805	49.358260
983.343790	93.548474	49.363265
979.385257	108.117497	49.368269
976.303199	97.700709	49.373274
972.771131	103.056380	49.378279
969.501145	111.781610	49.383284
965.732399	107.246298	49.388289
962.319269	104.996530	49.393293
958.860319	96.347220	49.398298
955.558256	111.133010	49.403303
952.217352	100.386593	49.408308
948.328596	107.069975	49.413313
944.584312	110.370770	49.418317
940.987641	108.298447	49.423322
937.649538	100.617331	49.428327
934.231208	106.714522	49.433332
930.929625	108.006588	49.438337
927.242604	111.500907	49.443341
924.037960	97.347890	49.448346
920.393371	110.067567	49.453351
916.381445	106.933958	49.458356
913.346908	108.440484	49.463361
909.709671	113.303273	49.468365
906.298751	109.838275	49.473370
902.469507	106.451437	49.478375
899.186293	115.953892	49.483380
896.035155	105.006937	49.488385
892.188925	111.022445	49.493389
889.100790	96.515837	49.498394
885.225936	110.125808	49.503399
881.419252	111.057211	49.508404
878.552238	100.477073	49.513409
874.617332	107.221492	49.518413
871.108965	112.228633	49.523418
867.863807	101.729856	49.528423
864.080646	104.473610	49.533428
860.744246	92.948236	49.538433
857.026703	100.269238	49.543437
853.518311	94.756724	49.548442
850.054991	98.190730	49.553447
846.608411	100.533766	49.558452
843.301217	98.735700	49.563457
839.581286	109.331626	49.568461
836.360585	99.135925	49.573466
832.918741	106.249247	49.578471
828.731895	99.811580	49.583476
825.600847	96.090816	49.588481
821.905780	104.082203	49.593485
818.695717	95.555336	49.598490
815.219183	104.686277	49.603495
811.642871	103.559961	49.608500
808.515546	101.104143	49.613505
804.650671	107.995812	49.618509
801.374255	99.162960	49.623514
797.546172	103.941774	49.628519
794.020871	108.967410	49.633524
790.444511	105.901695	49.638529
787.265128	115.318316	49.643533
783.805164	95.203603	49.648538
780.027751	103.840659	49.653543
776.361747	111.530114	49.658548
772.886896	108.021396	49.663553
769.345627	105.643069	49.668557
766.324556	103.407912	49.673562
762.800630	100.555465	49.678567
759.375076	98.064108	49.683572
755.986392	98.933268	49.688577
752.085485	110.475066	49.693581
748.367066	104.255152	49.698586
745.068414	98.962943	49.703591
741.440025	107.326735	49.708596
738.099616	92.461067	49.713601
734.329380	103.533143	49.718605
731.086823	93.166904	49.723610
727.718999	90.910133	49.728615
724.068784	96.259076	49.733620
720.905426	96.175459	49.738625
717.112119	105.669253	49.743629
713.539645	92.016874	49.748634
709.946756	101.909559	49.753639
706.239688	112.408600	49.758644
703.151914	97.164853	49.763649
699.643465	106.022412	49.768653
696.025603	95.639030	49.773658
692.229869	98.039963	49.778663
688.938176	104.563494	49.783668
685.742921	91.367756	49.788673
681.849050	98.264006	49.793677
678.401515	92.666106	49.798682
675.426959	103.996412	49.803687
671.566671	100.880298	49.808692
668.316397	107.362548	49.813697
664.731382	104.007171	49.818701
660.522729	101.863122	49.823706
657.473987	101.979879	49.828711
653.885121	102.636813	49.833716
650.532617	103.320007	49.838721
646.736620	104.556720	49.843725
643.784341	107.315970	49.848730
640.150334	100.968991	49.853735
636.349861	105.107616	49.858740
633.126462	98.756448	49.863745
629.667577	107.030454	49.868749
626.160030	102.723311	49.873754
622.585769	100.881730	49.878759
618.650999	98.160125	49.883764
615.594516	96.999933	49.888769
611.887093	95.413332	49.893773
608.312885	97.852372	49.898778
605.118500	91.977571	49.903783
601.470472	100.701991	49.908788
598.056246	98.120337	49.913793
594.240534	97.404930	49.918797
591.018129	88.725070	49.923802
587.457139	95.566055	49.928807
584.005977	95.151068	49.933812
580.427951	90.769563	49.938817
576.719427	112.690191	49.943821
573.163542	101.458751	49.948826
569.870078	100.025637	49.953831
566.724677	100.980150	49.958836
563.009880	87.625393	49.963841
559.433365	90.007863	49.968845
556.083530	92.003650	49.973850
552.420926	95.393038	49.978855
548.358434	95.937528	49.983860
545.349680	94.731919	49.988865
542.030954	104.157769	49.993869
538.716822	104.936235	49.998874
534.990787	104.162515	50.003879
531.500507	99.412940	50.008884
528.372091	93.831563	50.013889
524.467151	90.633924	50.018893
520.960243	92.021565	50.023898
517.168049	94.944039	50.028903
513.826187	103.484493	50.033908
510.561294	97.155693	50.038913
506.755959	99.485436	50.043917
503.041268	101.506750	50.048922
499.680152	105.010293	50.053927
496.159810	94.206770	50.058932
492.809017	97.702370	50.063937
489.147651	102.262194	50.068941
485.431493	101.442654	50.073946
482.489713	100.928940	50.078951
479.169240	108.456804	50.083956
475.673108	101.509329	50.088961
471.601690	100.966905	50.093965
468.437922	93.919922	50.098970
464.748004	93.368367	50.103975
461.059394	93.775240	50.108980
458.157177	101.183812	50.113985
454.642428	102.591690	50.118989
450.797143	101.754424	50.123994
447.225590	101.526027	50.128999
443.573468	107.767562	50.134004
440.341927	106.210900	50.139009
437.008798	99.687172	50.144013
433.509868	98.770353	50.149018
430.106097	102.163540	50.154023
425.892116	94.319278	50.159028
422.666028	96.612110	50.164033
419.291171	100.086194	50.169037
415.684811	88.403996	50.174042
412.337030	94.423859	50.179047
408.455569	94.620512	50.184052
405.214438	88.936616	50.189057
401.669205	99.552767	50.194061
398.562060	87.349452	50.199066
394.611885	94.159712	50.204071
391.057725	90.388328	50.209076
387.766602	92.972935	50.214081
384.298579	98.328263	50.219085
380.430890	88.838398	50.224090
377.353579	96.410458	50.229095
373.799815	94.410744	50.234100
370.147970	93.612817	50.239105
367.011771	93.952181	50.244109
363.688542	92.669343	50.249114
359.998122	84.632378	50.254119
356.257795	92.640497	50.259124
352.549397	93.373220	50.264129
349.115623	95.644824	50.269133
345.921503	90.187709	50.274138
342.294935	102.540887	50.279143
338.446881	91.927983	50.284148
335.194890	88.621825	50.289153
331.656970	97.240498	50.294157
328.454792	87.013653	50.299162
324.706829	94.554739	50.304167
320.791557	93.984761	50.309172
318.102890	89.125532	50.314177
314.063987	92.134189	50.319181
310.587698	95.405898	50.324186
306.804674	87.506851	50.329191
303.582793	93.478553	50.334196
300.261616	87.253576	50.339201
296.584914	93.021277	50.344205
293.482515	95.494096	50.349210
289.940195	95.979364	50.354215
286.110090	102.172903	50.359220
282.768980	88.145981	50.364225
279.065108	93.354789	50.369229
275.721922	94.020843	50.374234
272.106723	95.903275	50.379239
268.400950	91.377402	50.384244
265.156327	84.260915	50.389249
261.727766	89.705015	50.394253
257.951548	97.127164	50.399258
254.361898	88.897290	50.404263
250.964565	94.039107	50.409268
247.372146	88.606462	50.414273
243.757728	105.855315	50.419277
240.574347	92.252960	50.424282
237.466381	86.418558	50.429287
233.796187	86.050675	50.434292
230.547798	85.265535	50.439297
226.746327	95.295448	50.444301
222.901870	94.084827	50.449306
219.251276	96.887160	50.454311
215.784836	85.999404	50.459316
212.917415	83.654954	50.464321
209.065674	89.842417	50.469325
205.771665	87.634400	50.474330
202.039842	85.640507	50.479335
198.239330	94.012454	50.484340
195.284976	83.152057	50.489345
191.795847	88.697418	50.494349
188.320254	86.381813	50.499354
184.810394	84.324681	50.504359
181.065137	90.498636	50.509364
177.992503	84.522681	50.514369
173.805184	88.965698	50.519373
170.176157	84.361410	50.524378
166.767697	91.343158	50.529383
163.273899	91.605737	50.534388
160.025259	89.618424	50.539393
156.612464	89.333636	50.544397
153.381605	85.451595	50.549402
150.172522	90.003963	50.554407
145.617771	96.304753	50.559412
142.386981	90.508613	50.564417
138.927226	93.879036	50.569421
135.453738	93.113377	50.574426
132.124924	93.789888	50.579431
128.172103	90.147516	50.584436
125.075250	85.425072	50.589441
121.390254	92.352082	50.594445
117.812234	90.802369	50.599450
114.464940	88.109187	50.604455
110.843395	94.352374	50.609460
107.601006	89.988098	50.614465
104.231383	95.445166	50.619469
100.753904	87.624905	50.624474
96.995841	84.736655	50.629479
93.433034	98.459327	50.634484
90.208153	89.027094	50.639489
86.634856	98.692275	50.644493
82.836992	94.737742	50.649498
79.311258	100.197132	50.654503
75.945225	93.248443	50.659508
72.240640	95.160778	50.664513
68.857640	87.252963	50.669517
65.387388	96.256594	50.674522
62.003204	84.530280	50.679527
58.663940	89.789615	50.684532
54.788660	85.571977	50.689537
51.575961	89.710488	50.694541
48.093270	84.150012	50.699546
44.689767	76.748466	50.704551
40.924723	80.157263	50.709556
37.465258	88.735263	50.714561
33.873284	88.437468	50.719565
30.148506	88.223757	50.724570
26.702177	84.843768	50.729575
23.449961	90.117951	50.734580
20.162420	77.892461	50.739585
16.529212	92.799944	50.744589
13.130598	83.594288	50.749594
9.256413	75.814085	50.754599
5.651493	89.824951	50.759604
2.504514	87.767987	50.764609