Thu Aug 25 13:15:43 2022

Number of Points = 9925

Depth (nm)	Load (N)	Time (s)
2.288302	101.844924	0.000000
2.328595	101.496832	0.005005
2.365213	94.790116	0.010010
2.300331	95.306397	0.015014
1.838251	102.816754	0.020019
1.950159	95.683786	0.025024
1.720120	80.365919	0.030029
1.377956	84.310886	0.035034
1.551576	74.561304	0.040038
1.092656	69.115493	0.045043
0.872934	56.728850	0.050048
0.514093	47.334795	0.055053
0.287412	49.078657	0.060058
0.078346	41.727081	0.065062
-0.213204	33.556361	0.070067
-0.961013	26.494847	0.075072
-1.184466	23.286905	0.080077
-1.757636	19.950260	0.085082
-1.585659	22.264412	0.090086
-2.069395	19.344027	0.095091
-2.116345	18.696392	0.100096
-2.117221	21.217961	0.105101
-2.441478	24.062282	0.110106
-2.752843	26.183245	0.115110
-3.551575	32.097997	0.120115
-3.840745	31.814182	0.125120
-3.586943	24.478676	0.130125
-4.359039	21.467430	0.135130
-4.785978	17.630144	0.140134
-4.796094	22.997387	0.145139
-5.007486	16.668083	0.150144
-5.299531	20.209713	0.155149
-5.515709	23.024445	0.160154
-5.199101	23.515751	0.165158
-5.357493	23.423418	0.170163
-5.451875	24.896612	0.175168
-5.987602	13.527626	0.180173
-6.863025	26.772184	0.185178
-6.957113	18.877418	0.190182
-6.790053	22.448354	0.195187
-7.067217	27.079153	0.200192
-7.679066	21.885110	0.205197
-8.363553	18.037558	0.210202
-8.016662	19.637765	0.215206
-8.348955	24.865662	0.220211
-8.144313	25.450442	0.225216
-8.424830	23.725758	0.230221
-9.570911	23.136443	0.235226
-9.278051	21.416833	0.240230
-9.443070	26.017406	0.245235
-9.686172	26.574263	0.250240
-9.635747	22.877319	0.255245
-10.616025	30.396072	0.260250
-11.057246	30.949170	0.265254
-10.861286	30.472284	0.270259
-10.984859	26.293235	0.275264
-10.907411	21.668237	0.280269
-11.158199	31.173434	0.285274
-11.598525	23.513250	0.290278
-11.938838	27.872368	0.295283
-12.794756	30.863268	0.300288
-12.750323	17.302637	0.305293
-12.970390	28.340608	0.310298
-12.606421	18.042376	0.315302
-13.413987	25.429662	0.320307
-13.719850	32.646594	0.325312
-13.895367	12.843512	0.330317
-14.037372	32.680344	0.335322
-14.045926	33.637051	0.340326
-14.129279	23.984709	0.345331
-14.772490	26.730309	0.350336
-15.216669	33.646208	0.355341
-15.757033	26.466772	0.360346
-15.583692	27.954966	0.365350
-15.692191	38.181357	0.370355
-15.711053	35.767102	0.375360
-16.224317	27.719710	0.380365
-16.826550	27.769687	0.385370
-16.875448	30.596175	0.390374
-16.911815	30.209476	0.395379
-17.476778	33.040893	0.400384
-17.273484	32.018689	0.405389
-18.098967	31.372815	0.410394
-18.134858	28.534121	0.415398
-18.300352	27.031860	0.420403
-18.199062	27.189906	0.425408
-18.419851	26.620130	0.430413
-19.523883	28.150280	0.435418
-19.500914	23.033943	0.440422
-19.557489	26.010330	0.445427
-19.669641	28.340526	0.450432
-19.817818	23.263659	0.455437
-20.156099	33.652601	0.460442
-20.590478	25.706746	0.465446
-21.248761	22.228414	0.470451
-21.301381	28.861497	0.475456
-21.177598	27.937174	0.480461
-21.568397	28.786093	0.485466
-21.786907	24.735816	0.490470
-22.272749	26.127976	0.495475
-22.994936	24.966043	0.500480
-22.752423	24.311020	0.505485
-22.931138	29.983092	0.510490
-22.815135	32.407254	0.515494
-23.216506	28.705168	0.520499
-23.413717	29.821150	0.525504
-23.578680	23.411803	0.530509
-24.358793	32.310236	0.535514
-24.239101	25.214043	0.540518
-24.166234	35.953019	0.545523
-24.463885	33.202794	0.550528
-24.959563	25.582921	0.555533
-25.441844	25.009824	0.560538
-25.546651	21.438444	0.565542
-25.701731	31.033048	0.570547
-26.126263	30.188310	0.575552
-26.668044	26.546190	0.580557
-26.800836	32.685632	0.585562
-27.037717	24.911315	0.590566
-27.360117	27.979974	0.595571
-27.363648	32.599537	0.600576
-27.237647	25.303038	0.605581
-27.225462	33.185148	0.610586
-28.238629	25.491334	0.615590
-28.337956	31.094019	0.620595
-28.828192	29.959018	0.625600
-28.403265	20.189075	0.630605
-28.880010	35.332707	0.635610
-29.035869	24.644519	0.640614
-29.530622	29.761831	0.645619
-30.171712	30.722734	0.650624
-29.667840	27.536874	0.655629
-30.625515	35.669024	0.660634
-30.698944	28.242420	0.665638
-31.096605	31.288070	0.670643
-31.623779	34.224299	0.675648
-31.476714	23.558251	0.680653
-31.669152	32.064045	0.685658
-31.799244	29.812753	0.690662
-31.938722	33.912613	0.695667
-32.495195	34.844440	0.700672
-32.585144	24.693257	0.705677
-32.952155	29.195765	0.710682
-32.932241	30.613086	0.715686
-33.114219	31.695043	0.720691
-33.345882	22.065942	0.725696
-34.140452	23.981041	0.730701
-34.443900	33.070544	0.735706
-34.400863	15.441529	0.740710
-34.471464	27.202728	0.745715
-34.524041	31.614840	0.750720
-34.581187	26.106093	0.755725
-35.269180	33.316459	0.760730
-35.351449	24.084731	0.765734
-35.738316	19.697001	0.770739
-36.599373	25.681630	0.775744
-36.025165	18.849583	0.780749
-36.949322	25.328155	0.785754
-37.112155	23.461646	0.790758
-37.361147	28.584742	0.795763
-37.613268	27.118202	0.800768
-37.316807	23.037857	0.805773
-37.898815	22.388638	0.810778
-37.862820	25.907343	0.815782
-38.566460	23.103674	0.820787
-39.141555	30.052740	0.825792
-39.009278	31.604316	0.830797
-38.966502	23.061679	0.835802
-39.076763	33.196592	0.840806
-39.259095	21.291341	0.845811
-40.131695	35.617471	0.850816
-40.324554	27.206667	0.855821
-40.419659	34.014087	0.860826
-40.334018	30.754551	0.865830
-40.584598	31.995955	0.870835
-41.561629	33.335365	0.875840
-41.785672	32.687005	0.880845
-42.036056	33.327262	0.885850
-41.782642	28.380461	0.890854
-42.144661	24.219793	0.895859
-42.127104	28.636733	0.900864
-42.214495	25.372673	0.905869
-43.020678	30.241387	0.910874
-43.440478	27.719112	0.915878
-43.361392	32.426971	0.920883
-43.624256	36.827740	0.925888
-43.420311	22.884609	0.930893
-43.740429	33.223247	0.935898
-44.234647	33.917528	0.940902
-45.042995	37.138261	0.945907
-45.192833	37.990555	0.950912
-44.849324	23.522516	0.955917
-45.240429	34.501867	0.960922
-45.820838	22.136968	0.965926
-46.033493	16.282430	0.970931
-46.598525	31.629718	0.975936
-46.224149	22.022719	0.980941
-46.690539	30.033596	0.985946
-46.822651	27.130885	0.990950
-46.657765	24.485360	0.995955
-47.282133	25.953011	1.000960
-47.471352	23.125687	1.005965
-47.973038	33.638308	1.010970
-47.932217	25.573706	1.015974
-48.306752	27.410337	1.020979
-48.822027	24.630939	1.025984
-49.042100	26.981208	1.030989
-49.625784	26.971333	1.035994
-49.252252	20.110617	1.040998
-49.259660	26.701812	1.046003
-49.845951	29.122118	1.051008
-49.982090	20.572716	1.056013
-50.989417	28.209604	1.061018
-50.808628	32.724356	1.066022
-50.939331	29.150705	1.071027
-51.127319	31.578205	1.076032
-50.860345	23.471841	1.081037
-51.443601	27.543158	1.086042
-51.838158	24.466433	1.091046
-51.943448	28.956406	1.096051
-52.616493	29.523684	1.101056
-52.413811	24.296930	1.106061
-53.247266	28.761792	1.111066
-53.839992	24.377845	1.116070
-53.708170	26.391401	1.121075
-53.987553	27.884091	1.126080
-54.025875	22.211045	1.131085
-53.871764	34.038277	1.136090
-54.517408	23.284467	1.141094
-54.412881	30.636411	1.146099
-54.690463	16.964888	1.151104
-55.369284	17.112290	1.156109
-55.838297	29.771149	1.161114
-55.494383	26.445836	1.166118
-55.380174	31.777780	1.171123
-56.103834	25.459140	1.176128
-56.508615	29.360123	1.181133
-56.909491	40.654221	1.186138
-57.175420	33.450769	1.191142
-57.157126	21.615325	1.196147
-57.228426	28.795500	1.201152
-57.085873	28.184612	1.206157
-57.724612	28.483922	1.211162
-58.012989	20.353845	1.216166
-58.318785	23.935595	1.221171
-58.981783	32.932737	1.226176
-58.844412	29.193696	1.231181
-59.297286	31.646882	1.236186
-59.881645	19.345882	1.241190
-59.937279	26.887434	1.246195
-60.006434	21.855136	1.251200
-59.803491	24.657981	1.256205
-60.241101	28.279368	1.261210
-60.269659	32.418796	1.266214
-60.709470	26.739054	1.271219
-60.824032	28.370435	1.276224
-60.919314	26.344645	1.281229
-62.141896	30.993866	1.286234
-62.658368	28.970796	1.291238
-62.676282	23.171165	1.296243
-62.842059	31.948028	1.301248
-62.703677	28.322724	1.306253
-62.678603	36.329363	1.311258
-63.094044	26.460139	1.316262
-63.162130	22.506518	1.321267
-63.662895	23.334704	1.326272
-63.915590	25.013039	1.331277
-64.658714	30.707108	1.336282
-64.597054	25.711260	1.341286
-64.715749	23.622699	1.346291
-64.677921	26.248934	1.351296
-64.859633	24.287307	1.356301
-65.248017	32.687761	1.361306
-65.840560	25.228604	1.366310
-65.913862	35.990479	1.371315
-66.207781	33.401024	1.376320
-66.178225	29.875030	1.381325
-67.095862	33.236274	1.386330
-67.169879	28.941894	1.391334
-67.419633	25.174927	1.396339
-67.874106	27.441701	1.401344
-67.772199	21.816286	1.406349
-67.689097	34.103897	1.411354
-68.104520	24.433989	1.416358
-67.974263	28.700392	1.421363
-68.542336	36.126088	1.426368
-68.740466	30.822931	1.431373
-69.011516	28.755079	1.436378
-69.195961	20.276523	1.441382
-69.879623	22.069842	1.446387
-70.301437	29.475782	1.451392
-70.371375	24.734673	1.456397
-70.513476	27.281533	1.461402
-70.229255	24.240822	1.466406
-70.556108	30.578349	1.471411
-71.928982	38.098513	1.476416
-71.668483	32.606433	1.481421
-72.260439	33.648227	1.486426
-72.292853	28.157752	1.491430
-71.828769	24.032160	1.496435
-72.365168	24.445149	1.501440
-71.916006	15.690144	1.506445
-72.839198	29.147833	1.511450
-72.831589	27.330548	1.516454
-73.223761	28.992773	1.521459
-73.773919	32.951337	1.526464
-73.890176	31.349614	1.531469
-74.481740	29.480681	1.536474
-74.705426	21.770741	1.541478
-74.665159	27.009864	1.546483
-75.026894	32.039895	1.551488
-74.786403	34.011113	1.556493
-75.753989	32.653517	1.561498
-76.304946	21.736178	1.566502
-76.298398	26.325685	1.571507
-76.619970	32.184657	1.576512
-76.569135	20.353608	1.581517
-76.375007	29.830215	1.586522
-76.342834	21.279752	1.591526
-76.839811	10.961404	1.596531
-77.805312	32.433211	1.601536
-77.594591	25.635970	1.606541
-77.755245	28.473640	1.611546
-77.903964	29.281466	1.616550
-78.549771	20.729669	1.621555
-79.212813	25.670868	1.626560
-79.151773	18.909738	1.631565
-79.023620	30.579681	1.636570
-79.316752	27.101086	1.641574
-79.280103	19.018160	1.646579
-79.956140	34.110757	1.651584
-80.435982	22.299584	1.656589
-80.919740	24.744954	1.661594
-81.112665	25.543888	1.666598
-81.250440	19.883263	1.671603
-81.371251	24.831249	1.676608
-81.100605	19.574865	1.681613
-81.439762	25.506193	1.686618
-81.947346	18.014747	1.691622
-81.798537	19.415033	1.696627
-82.834607	27.704998	1.701632
-82.482341	20.853943	1.706637
-82.667151	28.548614	1.711642
-82.928608	25.960402	1.716646
-83.415742	11.834503	1.721651
-83.827501	22.310878	1.726656
-83.930161	18.792949	1.731661
-84.395241	32.501561	1.736666
-84.918444	24.148852	1.741670
-84.900232	35.168469	1.746675
-85.284663	28.891591	1.751680
-85.113167	26.877783	1.756685
-85.368614	30.261820	1.761690
-85.394509	25.441044	1.766694
-86.032221	19.592999	1.771699
-86.719190	24.053891	1.776704
-86.660878	21.029596	1.781709
-86.375821	25.474221	1.786714
-86.855381	28.760496	1.791718
-86.864193	15.467646	1.796723
-87.431175	26.816236	1.801728
-87.894965	21.583183	1.806733
-88.475617	22.382759	1.811738
-88.477081	24.689282	1.816742
-88.210108	15.839439	1.821747
-88.535881	33.031674	1.826752
-88.652579	23.337108	1.831757
-89.575707	29.227062	1.836762
-89.973769	25.394749	1.841766
-89.897495	26.053425	1.846771
-90.112463	35.201829	1.851776
-89.681646	28.477668	1.856781
-90.031562	29.408770	1.861786
-90.556217	30.199572	1.866790
-90.994719	22.792213	1.871795
-91.276703	30.451491	1.876800
-91.542842	23.656205	1.881805
-92.230140	25.067280	1.886810
-92.630011	23.260061	1.891814
-92.134868	22.859681	1.896819
-92.578988	31.512476	1.901824
-92.234275	15.538307	1.906829
-92.541252	27.694044	1.911834
-93.017504	22.788812	1.916838
-93.892293	18.857193	1.921843
-94.253641	25.111538	1.926848
-94.002026	15.277007	1.931853
-94.327833	28.916337	1.936858
-94.430942	20.418711	1.941862
-94.272815	17.616058	1.946867
-95.403773	26.664376	1.951872
-95.594093	17.572974	1.956877
-95.727363	25.189964	1.961882
-95.610035	20.485954	1.966886
-95.767991	9.181177	1.971891
-96.197516	22.378008	1.976896
-96.101892	18.158291	1.981901
-96.897978	25.765245	1.986906
-97.119997	31.153034	1.991910
-97.251854	24.814436	1.996915
-97.196425	22.346328	2.006912
-97.241486	24.089170	2.016909
-96.936630	20.962104	2.026906
-96.322874	17.834152	2.036902
-96.144426	16.399500	2.046899
-95.497508	24.122454	2.056896
-94.951064	22.934249	2.066893
-94.185777	21.265091	2.076890
-93.605482	25.909866	2.086886
-93.341776	25.995077	2.096883
-92.937573	24.727790	2.106880
-92.361547	31.916993	2.116877
-91.976768	29.844955	2.126874
-90.961074	24.721654	2.136870
-90.663625	28.713831	2.146867
-90.607224	27.000527	2.156864
-89.614778	33.231156	2.166861
-89.303807	30.118968	2.176858
-89.020037	28.138787	2.186854
-88.090109	25.974994	2.196851
-87.861434	32.895507	2.206848
-87.286262	30.033361	2.216845
-86.272139	28.211171	2.226842
-86.160853	24.990889	2.236838
-85.931597	30.647352	2.246835
-85.424414	25.179243	2.256832
-84.847158	30.062083	2.266829
-84.361959	28.693406	2.276826
-83.678520	31.522702	2.286822
-83.421686	30.050424	2.296819
-82.231773	29.879632	2.306816
-82.189914	28.098914	2.316813
-82.145405	28.094927	2.326810
-81.219509	29.023556	2.336806
-80.492837	30.518763	2.346803
-80.621709	32.550339	2.356800
-79.696333	32.820143	2.366797
-79.456450	29.886989	2.376794
-78.698618	32.102744	2.386790
-77.719208	28.299772	2.396787
-77.792348	24.984844	2.406784
-77.857190	32.299809	2.416781
-77.021523	24.214298	2.426778
-75.868146	29.019537	2.436774
-75.271635	32.109544	2.446771
-75.396851	28.324435	2.456768
-75.169529	24.154633	2.466765
-74.549251	29.882876	2.476762
-73.865171	30.212664	2.486758
-72.693680	24.554934	2.496755
-72.543068	28.240667	2.506752
-72.531847	22.352924	2.516749
-71.770674	24.159507	2.526746
-71.067721	31.357334	2.536742
-70.969713	30.483317	2.546739
-70.317546	26.060045	2.556736
-69.795709	22.883140	2.566733
-69.170800	25.816643	2.576730
-68.260196	19.509208	2.586726
-68.068764	27.962444	2.596723
-68.118715	31.217103	2.606720
-67.560578	31.778870	2.616717
-66.941991	31.719777	2.626714
-65.648137	29.267711	2.636710
-65.134855	29.719298	2.646707
-65.383165	26.406473	2.656704
-65.352632	29.062474	2.666701
-64.516956	24.280996	2.676698
-63.673290	23.039885	2.686694
-62.418565	22.776578	2.696691
-62.387992	28.784123	2.706688
-62.287246	27.374317	2.716685
-62.372564	25.461471	2.726682
-61.308928	24.683241	2.736678
-60.560299	26.583657	2.746675
-59.666720	29.323008	2.756672
-59.711973	28.322552	2.766669
-59.683968	28.533394	2.776666
-58.760280	28.736941	2.786662
-58.338273	31.889139	2.796659
-57.667160	34.042457	2.806656
-56.582731	28.179789	2.816653
-56.722073	37.182206	2.826650
-56.539816	32.062783	2.836646
-56.025063	28.978854	2.846643
-55.088228	26.725283	2.856640
-54.343330	32.275611	2.866637
-53.870903	34.523417	2.876634
-54.049407	34.582884	2.886630
-53.394696	38.050249	2.896627
-52.363050	22.448476	2.906624
-52.609664	30.932338	2.916621
-51.197316	27.543041	2.926618
-51.131278	32.952649	2.936614
-50.990263	21.988730	2.946611
-50.247243	32.614197	2.956608
-49.872357	30.128726	2.966605
-49.045336	25.855456	2.976602
-48.141951	26.242751	2.986598
-47.864508	26.531718	2.996595
-47.884091	27.149162	3.006592
-47.546981	24.533396	3.016589
-46.629890	29.258454	3.026586
-46.297131	29.776341	3.036582
-45.674805	25.379920	3.046579
-45.056860	27.389514	3.056576
-44.807067	30.239243	3.066573
-44.008233	27.921765	3.076570
-43.762927	30.312864	3.086566
-43.274446	26.022946	3.096563
-42.225599	27.803465	3.106560
-42.251821	32.904412	3.116557
-42.034630	28.061451	3.126554
-40.977053	22.687670	3.136550
-40.785562	29.794578	3.146547
-39.951349	37.589570	3.156544
-39.584163	37.034508	3.166541
-39.392647	35.087788	3.176538
-38.382255	30.408814	3.186534
-37.913110	27.933918	3.196531
-37.882731	30.263659	3.206528
-37.291711	40.716544	3.216525
-36.379144	34.430974	3.226522
-36.435402	36.562047	3.236518
-35.132956	26.559727	3.246515
-34.786705	27.151528	3.256512
-34.765378	26.786873	3.266509
-34.595604	22.657767	3.276506
-33.417513	27.227890	3.286502
-32.992421	20.676580	3.296499
-32.818387	26.686991	3.306496
-31.745609	21.035228	3.316493
-31.739698	24.483874	3.326490
-31.455975	27.486679	3.336486
-30.326480	25.069875	3.346483
-30.148336	24.794691	3.356480
-29.799288	29.675280	3.366477
-29.061503	24.133026	3.376474
-28.601377	26.233873	3.386470
-28.430918	22.247211	3.396467
-27.464271	30.119654	3.406464
-27.093513	26.757346	3.416461
-26.529406	31.702441	3.426458
-26.238787	29.505776	3.436454
-25.790907	27.803992	3.446451
-25.181168	27.271115	3.456448
-24.802451	26.657226	3.466445
-23.654123	27.398955	3.476442
-23.309466	22.855973	3.486438
-23.134062	26.145014	3.496435
-22.934823	29.585544	3.506432
-21.893848	25.674729	3.516429
-21.870648	33.790032	3.526426
-20.758211	25.287354	3.536422
-20.222605	27.439731	3.546419
-20.261591	26.755074	3.556416
-19.985091	24.722180	3.566413
-19.061367	26.097819	3.576410
-18.912439	30.664472	3.586406
-18.038749	30.467209	3.596403
-17.574046	26.041633	3.606400
-16.912279	25.728688	3.616397
-16.192340	31.314610	3.626394
-15.845841	25.687945	3.636390
-15.876710	25.280784	3.646387
-15.643184	28.573390	3.656384
-14.605350	34.027141	3.666381
-13.712079	26.876615	3.676378
-13.111198	32.769464	3.686374
-13.305301	33.068960	3.696371
-12.854716	32.453315	3.706368
-12.103952	31.106387	3.716365
-11.431138	26.752742	3.726362
-11.208333	24.047180	3.736358
-10.442477	34.564539	3.746355
-9.984894	29.832799	3.756352
-9.701195	21.795761	3.766349
-9.146098	30.280723	3.776346
-8.447647	34.507851	3.786342
-8.071389	35.661992	3.796339
-7.521701	32.883037	3.806336
-7.133799	35.631935	3.816333
-6.659096	27.770875	3.826330
-5.835473	31.740805	3.836326
-5.727852	25.004817	3.846323
-5.206220	31.385256	3.856320
-4.537607	33.551642	3.866317
-4.183854	36.622672	3.876314
-3.372601	39.831098	3.886310
-3.005541	37.308840	3.896307
-2.785054	43.121910	3.906304
-2.357499	50.654345	3.916301
-1.848808	62.989164	3.926298
-1.602853	69.339951	3.936294
-0.935731	78.802082	3.946291
-0.531972	91.254733	3.956288
-0.243492	103.066545	3.966285
0.000000	115.248521	3.971290
0.160481	132.418459	3.976294
0.690893	138.431880	3.981299
0.780450	148.583011	3.986304
1.372225	137.900999	3.991309
1.353114	141.121475	3.996314
1.313051	151.330882	4.001318
1.157464	150.972350	4.006323
1.145241	154.340448	4.011328
1.042565	152.473989	4.016333
1.218807	153.117008	4.021338
1.471219	150.720345	4.026342
1.371141	158.436601	4.031347
1.123318	161.765683	4.036352
1.372867	155.882970	4.041357
1.368509	164.511222	4.046362
1.407324	156.408907	4.051366
1.500546	154.518082	4.056371
1.445878	162.236716	4.061376
1.645361	158.810621	4.066381
1.457724	158.719706	4.071386
1.471221	151.772980	4.076390
1.635327	154.199114	4.081395
1.521698	158.174730	4.086400
1.502614	162.625920	4.091405
1.556281	161.877093	4.096410
1.329515	160.147137	4.101414
1.536457	149.727897	4.106419
1.370430	160.181674	4.111424
1.486663	150.396750	4.116429
1.458244	150.170155	4.121434
1.399443	154.374463	4.126438
1.480560	152.273561	4.131443
1.488124	157.837393	4.136448
1.643989	158.752528	4.141453
1.498506	151.678849	4.146458
1.640971	159.043888	4.151462
1.764553	158.553029	4.156467
1.799842	164.356131	4.161472
1.500459	149.352794	4.166477
1.745864	153.044361	4.171482
1.460125	155.091720	4.176486
1.902450	159.283952	4.181491
1.544877	165.126462	4.186496
1.532396	151.660067	4.191501
1.585171	157.406643	4.196506
1.336819	159.008377	4.201510
1.359848	150.563685	4.206515
1.365077	161.009612	4.211520
1.805416	165.319217	4.216525
1.840447	176.779225	4.221530
1.856228	174.476584	4.226534
1.899657	171.283748	4.231539
1.833327	171.695852	4.236544
1.627999	172.499898	4.241549
1.672082	171.853814	4.246554
1.629890	170.686566	4.251558
1.985035	176.594583	4.256563
1.909545	180.975521	4.261568
2.023000	165.606925	4.266573
2.421129	174.229068	4.271578
2.188879	169.541822	4.276582
2.013267	163.393523	4.281587
1.606518	153.845564	4.286592
1.536185	155.194777	4.291597
1.880242	170.855335	4.296602
1.758688	180.827587	4.301606
2.144873	175.208200	4.306611
2.044246	173.528082	4.311616
2.159600	177.281160	4.316621
2.207710	170.297366	4.321626
1.978669	168.403248	4.326630
2.215292	166.524755	4.331635
2.149075	174.422377	4.336640
2.237088	169.242021	4.341645
2.005139	156.670560	4.346650
1.911704	157.526677	4.351654
2.246937	169.417378	4.356659
1.910878	172.500856	4.361664
1.965405	176.456456	4.366669
2.324594	168.924042	4.371674
2.387732	176.864672	4.376678
2.392495	170.678618	4.381683
1.935003	174.366424	4.386688
2.097448	178.830306	4.391693
2.405734	181.638820	4.396698
2.107119	183.305380	4.401702
2.409043	178.275005	4.406707
2.207865	180.416687	4.411712
2.290177	176.999456	4.416717
2.502245	182.249676	4.421722
2.226678	171.447274	4.426726
2.374144	167.741422	4.431731
1.981095	170.849648	4.436736
2.634210	178.011298	4.441741
2.232629	174.834402	4.446746
2.032391	178.738169	4.451750
2.602107	176.839124	4.456755
2.317755	178.895759	4.461760
2.365365	178.907192	4.466765
1.923027	177.777329	4.471770
1.931087	172.922715	4.476774
2.362603	178.173352	4.481779
2.158623	186.133693	4.486784
2.259073	170.216631	4.491789
2.613889	175.286293	4.496794
2.397400	176.775467	4.501798
2.768151	170.538397	4.506803
2.641759	175.620180	4.511808
2.685155	178.062067	4.516813
2.527373	178.235396	4.521818
2.580100	169.298817	4.526822
2.792022	179.127069	4.531827
2.213327	178.458338	4.536832
2.258959	171.930517	4.541837
2.342566	172.135629	4.546842
2.466928	173.511286	4.551846
2.009653	169.267427	4.556851
2.187294	180.395042	4.561856
2.642097	187.053086	4.566861
2.644137	193.810546	4.571866
2.556917	195.304779	4.576870
2.910299	197.672789	4.581875
2.794618	205.537045	4.586880
2.977742	206.343505	4.591885
2.659376	192.244789	4.596890
2.515380	202.116164	4.601894
2.923080	191.810979	4.606899
2.830594	204.265435	4.611904
3.104518	193.332630	4.616909
3.072875	195.055440	4.621914
2.804206	183.736250	4.626918
2.580061	183.616252	4.631923
2.641932	194.091290	4.636928
2.956305	191.156560	4.641933
3.103824	191.414934	4.646938
2.991098	188.227579	4.651942
2.512339	180.680916	4.656947
2.766829	190.622729	4.661952
3.068827	187.803834	4.666957
3.000803	201.241560	4.671962
2.737162	182.008923	4.676966
2.716487	190.285400	4.681971
2.817584	193.850887	4.686976
3.143539	188.528839	4.691981
3.154768	199.400962	4.696986
2.572303	203.484847	4.701990
2.917030	192.961735	4.706995
2.646961	201.150740	4.712000
2.933349	198.707618	4.717005
2.792820	197.574759	4.722010
2.642633	205.691198	4.727014
3.090966	202.586778	4.732019
2.982807	202.473918	4.737024
2.847092	197.711427	4.742029
3.317765	197.267427	4.747034
3.097127	204.483729	4.752038
2.776815	194.703903	4.757043
2.796513	202.344463	4.762048
3.305574	203.950917	4.767053
2.932909	204.629321	4.772058
3.023405	214.188711	4.777062
3.129513	212.232585	4.782067
3.193630	217.787575	4.787072
3.450830	226.596342	4.792077
3.674158	226.251207	4.797082
3.112282	212.288707	4.802086
3.188026	207.442461	4.807091
3.151834	207.552446	4.812096
3.351093	211.861870	4.817101
3.367298	210.210900	4.822106
3.206558	209.229906	4.827110
3.143482	203.987790	4.832115
3.296186	216.584174	4.837120
3.601704	214.223475	4.842125
3.287688	214.342189	4.847130
3.424009	214.077126	4.852134
3.157261	208.553704	4.857139
2.905322	223.750861	4.862144
3.256580	233.155508	4.867149
3.180014	226.191226	4.872154
3.189816	221.494516	4.877158
3.564197	224.495164	4.882163
3.109914	228.612756	4.887168
3.280801	225.191129	4.892173
3.416018	230.991251	4.897178
3.401754	227.516375	4.902182
3.421309	227.946662	4.907187
3.347110	226.101044	4.912192
3.501379	221.429155	4.917197
3.225771	223.345219	4.922202
3.151634	229.086392	4.927206
3.769772	234.026227	4.932211
3.710102	243.394022	4.937216
3.596474	231.512663	4.942221
3.419511	240.272401	4.947226
3.562705	255.606995	4.952230
3.618492	242.908132	4.957235
3.843173	247.783066	4.962240
3.911324	245.484865	4.967245
3.642688	244.378402	4.972250
3.374140	240.098629	4.977254
3.865306	242.369126	4.982259
3.654265	244.740154	4.987264
3.887297	237.410978	4.992269
3.816964	228.477832	4.997274
3.344547	224.736213	5.002278
3.756880	230.445459	5.007283
3.723947	251.027923	5.012288
3.708319	252.422356	5.017293
4.267827	258.314199	5.022298
3.696195	241.581707	5.027302
4.213562	235.577911	5.032307
3.474458	230.131655	5.037312
3.275033	229.621800	5.042317
3.882625	250.727175	5.047322
3.603864	252.520346	5.052326
3.818466	240.922917	5.057331
4.166452	248.306413	5.062336
4.390225	245.360558	5.067341
4.010219	245.720569	5.072346
3.687345	236.564391	5.077350
3.926308	233.438986	5.082355
3.888349	251.007131	5.087360
3.986764	248.799102	5.092365
4.035109	253.125853	5.097370
3.922991	243.367164	5.102374
4.279955	242.219631	5.107379
4.008477	250.437353	5.112384
3.770115	239.977098	5.117389
4.269116	248.213307	5.122394
3.944988	249.276420	5.127398
4.468320	245.907137	5.132403
3.722729	243.793383	5.137408
3.994349	248.398367	5.142413
4.140959	248.976428	5.147418
4.092759	254.681908	5.152422
4.154082	249.331701	5.157427
4.334985	253.941408	5.162432
3.923777	246.020296	5.167437
4.155712	246.882386	5.172442
4.116147	254.595530	5.177446
4.290513	241.004878	5.182451
3.938028	250.586238	5.187456
4.255513	248.283772	5.192461
4.175472	247.840634	5.197466
3.693256	253.414796	5.202470
3.892994	245.413778	5.207475
3.738901	255.128574	5.212480
3.821319	255.356020	5.217485
3.840784	248.683572	5.222490
4.297342	267.692880	5.227494
4.167081	270.440403	5.232499
4.088843	276.030371	5.237504
4.264435	272.196703	5.242509
4.762164	276.554292	5.247514
4.574405	273.916526	5.252518
4.780942	265.386078	5.257523
4.338295	270.001738	5.262528
4.114186	257.381520	5.267533
4.424418	264.017952	5.272538
4.211251	265.285146	5.277542
4.303330	265.469949	5.282547
4.414418	274.118131	5.287552
4.408222	271.429771	5.292557
4.529942	271.236600	5.297562
4.084640	275.381269	5.302566
4.419737	258.206132	5.307571
4.500021	260.559992	5.312576
4.607159	267.683834	5.317581
4.454770	269.919123	5.322586
4.470536	263.576286	5.327590
4.461802	261.037025	5.332595
4.507682	260.868391	5.337600
4.292700	267.479545	5.342605
4.271070	275.952367	5.347610
4.322568	276.115053	5.352614
4.346195	269.473584	5.357619
4.273327	278.460644	5.362624
4.747089	291.550953	5.367629
5.040934	292.406510	5.372634
5.002931	284.357302	5.377638
4.896105	272.152141	5.382643
4.820212	271.553325	5.387648
4.454783	275.103339	5.392653
4.705980	266.360245	5.397658
4.495192	265.225735	5.402662
4.911459	266.286740	5.407667
4.635298	272.515169	5.412672
4.805000	269.324678	5.417677
4.426780	269.323734	5.422682
4.506772	280.188296	5.427686
5.005472	288.601745	5.432691
5.002938	290.797738	5.437696
5.044631	287.010357	5.442701
4.904260	278.917078	5.447706
4.364485	278.580773	5.452710
4.683482	287.607682	5.457715
4.539708	289.965013	5.462720
5.137110	293.971625	5.467725
4.777825	285.447562	5.472730
4.825690	286.664368	5.477734
4.807057	293.213129	5.482739
4.867818	294.127353	5.487744
5.175160	295.623049	5.492749
5.023628	293.786377	5.497754
4.772541	300.634159	5.502758
5.160133	287.715594	5.507763
4.949977	289.814402	5.512768
4.918144	293.843671	5.517773
5.098519	289.442927	5.522778
5.045549	292.906021	5.527782
4.996637	292.967379	5.532787
4.816666	293.172660	5.537792
4.876027	298.601868	5.542797
5.180176	294.273480	5.547802
4.598249	287.843944	5.552806
4.822734	282.616862	5.557811
4.896850	296.880291	5.562816
4.967243	302.307771	5.567821
5.228738	316.241294	5.572826
4.973032	319.473561	5.577830
5.229054	317.791334	5.582835
5.325310	319.690273	5.587840
4.898272	320.503753	5.592845
5.275816	321.254446	5.597850
5.281365	326.992657	5.602854
5.944608	324.632844	5.607859
5.453934	310.269960	5.612864
5.052652	303.483077	5.617869
5.303967	302.861468	5.622874
5.252613	310.804278	5.627878
5.372764	322.532623	5.632883
5.459847	318.573605	5.637888
5.188425	311.896089	5.642893
5.202565	316.731262	5.647898
5.164093	320.973554	5.652902
5.404011	318.297247	5.657907
5.512479	323.832666	5.662912
5.349492	318.131597	5.667917
5.778014	313.106660	5.672922
5.422796	315.294640	5.677926
5.232618	318.348958	5.682931
5.552129	324.423962	5.687936
5.155645	309.755249	5.692941
5.630777	318.397035	5.697946
5.708179	317.521094	5.702950
5.278470	316.177267	5.707955
5.573756	316.937685	5.712960
5.181479	315.059635	5.717965
5.181295	313.626363	5.722970
5.318960	319.888049	5.727974
5.389801	319.494036	5.732979
5.269825	317.737841	5.737984
5.416340	321.508214	5.742989
5.439438	322.564384	5.747994
5.283100	321.557383	5.752998
5.460895	320.175320	5.758003
5.611564	328.061174	5.763008
6.039606	333.423136	5.768013
5.970202	321.772074	5.773018
5.461878	325.145165	5.778022
5.533738	325.497655	5.783027
5.578274	322.877270	5.788032
5.436589	326.408056	5.793037
5.736016	326.813478	5.798042
5.711018	334.309234	5.803046
5.964741	338.296936	5.808051
5.903833	346.497529	5.813056
5.617475	336.917953	5.818061
5.760820	344.887221	5.823066
5.372654	351.493903	5.828070
6.111244	345.816085	5.833075
6.007475	348.271561	5.838080
6.024004	341.045870	5.843085
5.643048	334.518388	5.848090
5.535918	343.697515	5.853094
6.092019	348.916028	5.858099
6.123072	348.199211	5.863104
6.182424	345.294921	5.868109
6.131189	329.436285	5.873114
5.903930	331.465009	5.878118
5.785350	320.274080	5.883123
5.682357	322.251695	5.888128
5.894640	333.718834	5.893133
6.276551	343.305403	5.898138
5.927223	346.564999	5.903142
6.131747	338.635959	5.908147
5.944831	340.092039	5.913152
6.098553	335.233541	5.918157
6.017060	327.839711	5.923162
5.390173	332.496909	5.928166
6.141446	344.078926	5.933171
5.983289	344.568698	5.938176
5.852548	358.342242	5.943181
6.265081	349.526372	5.948186
6.107241	345.738603	5.953190
6.258792	349.720169	5.958195
5.995839	347.736430	5.963200
6.181873	348.298827	5.968205
5.981496	352.044463	5.973210
5.805465	358.292035	5.978214
6.074979	358.974233	5.983219
6.047193	358.551379	5.988224
6.093536	355.101784	5.993229
6.410040	353.270869	5.998234
6.175512	361.697993	6.003238
6.039684	343.232950	6.008243
5.650584	363.488525	6.013248
5.724534	357.734501	6.018253
6.071628	352.984909	6.023258
6.148309	353.336644	6.028262
6.373287	352.481872	6.033267
6.276984	357.571648	6.038272
6.074274	352.914527	6.043277
6.183238	350.818730	6.048282
6.618584	355.926448	6.053286
6.452237	347.090546	6.058291
6.672123	351.921966	6.063296
6.642907	356.074229	6.068301
6.467330	344.705549	6.073306
6.068812	350.592500	6.078310
6.412226	350.206401	6.083315
6.503623	347.901381	6.088320
5.967523	343.416724	6.093325
5.892842	332.895967	6.098330
6.080665	346.587950	6.103334
6.267646	348.254373	6.108339
6.329353	352.420864	6.113344
6.167696	336.987656	6.118349
5.748688	326.451248	6.123354
5.907515	345.440847	6.128358
6.151978	349.312941	6.133363
5.910282	348.942586	6.138368
6.128663	349.072798	6.143373
6.287057	342.796173	6.148378
6.044969	358.846134	6.153382
6.297905	354.557394	6.158387
6.076670	354.819762	6.163392
6.105586	353.878648	6.168397
5.977475	344.185686	6.173402
6.285187	359.937529	6.178406
6.050483	353.722490	6.183411
5.870746	349.175669	6.188416
6.305108	362.462033	6.193421
6.090024	364.988739	6.198426
6.072020	356.784501	6.203430
6.012801	354.964997	6.208435
6.232393	361.457475	6.213440
6.438055	350.396062	6.218445
6.425035	357.070520	6.223450
5.998553	358.908994	6.228454
6.423128	349.999487	6.233459
6.308764	347.084449	6.238464
6.243964	351.716860	6.243469
6.244931	357.620317	6.248474
6.400374	356.390454	6.253478
6.325161	354.000803	6.258483
6.150375	348.333212	6.263488
6.210122	351.063633	6.268493
6.314677	342.362461	6.273498
5.898647	345.145280	6.278502
6.085341	346.530167	6.283507
6.249562	355.160573	6.288512
6.228462	357.859368	6.293517
6.306967	346.637542	6.298522
6.222456	347.207526	6.303526
6.006276	337.360684	6.308531
6.122114	329.869495	6.313536
6.143353	340.642057	6.318541
6.104244	338.018957	6.323546
5.991877	347.603876	6.328550
6.569224	342.248722	6.333555
6.342834	339.541067	6.338560
6.035541	328.560038	6.343565
5.751471	326.826388	6.348570
5.819651	344.608955	6.353574
6.067292	346.838525	6.358579
5.886006	358.240793	6.363584
6.029373	353.956565	6.368589
6.360794	354.635390	6.373594
6.298287	359.393997	6.378598
6.226323	350.935619	6.383603
6.288385	353.532797	6.388608
6.011653	358.331296	6.393613
6.187602	353.143436	6.398618
6.066205	358.939513	6.403622
6.011442	350.567027	6.408627
6.177393	349.310207	6.413632
6.040829	356.522890	6.418637
6.065794	346.347188	6.423642
6.489595	352.054677	6.428646
6.216471	345.136964	6.433651
6.163375	351.849338	6.438656
5.897226	359.044359	6.443661
6.218431	355.308084	6.448666
5.971676	357.558169	6.453670
5.931401	348.696185	6.458675
6.030919	350.284561	6.463680
6.131824	346.740995	6.468685
6.163704	352.297915	6.473690
5.982786	344.755137	6.478694
5.983297	355.214573	6.483699
6.016595	353.007242	6.488704
5.967245	350.300321	6.493709
5.886334	349.025231	6.498714
5.604563	359.832625	6.503718
6.009866	357.763164	6.508723
6.357573	365.713078	6.513728
5.945123	369.691266	6.518733
6.467644	374.383525	6.523738
6.610107	369.552092	6.528742
6.722032	362.605681	6.533747
6.513452	345.911122	6.538752
6.194013	359.435816	6.543757
6.365592	365.347346	6.548762
6.153895	369.025155	6.553766
6.113330	359.245700	6.558771
6.016243	355.407280	6.563776
5.934068	355.587748	6.568781
6.177270	358.343211	6.573786
5.882332	360.781185	6.578790
6.131775	357.049825	6.583795
6.215625	352.917295	6.588800
6.074547	355.448222	6.593805
5.825829	348.985439	6.598810
5.800910	367.462837	6.603814
6.212532	350.829291	6.608819
6.103178	355.244052	6.613824
6.188933	361.437954	6.618829
6.297647	354.916002	6.623834
5.914828	352.539745	6.628838
6.195913	364.568777	6.633843
6.251550	368.663455	6.638848
6.511695	364.737423	6.643853
6.319872	358.870013	6.648858
6.387432	362.469264	6.653862
6.540202	365.726126	6.658867
6.064023	364.997032	6.663872
6.354076	367.871708	6.668877
6.299771	352.583022	6.673882
6.167459	366.072074	6.678886
6.326045	349.772411	6.683891
6.519036	354.199912	6.688896
6.525572	351.538020	6.693901
6.584016	349.162231	6.698906
6.530930	347.287982	6.703910
6.159541	340.259114	6.708915
6.095578	329.293744	6.713920
6.095090	328.467973	6.718925
6.216212	318.764449	6.723930
5.873966	329.707853	6.728934
6.042169	325.448215	6.733939
6.168380	325.273322	6.738944
6.206802	333.167274	6.743949
6.070212	324.794966	6.748954
5.926471	339.076743	6.753958
6.498529	336.803984	6.758963
6.220774	334.221439	6.763968
5.961078	338.577492	6.768973
6.056058	322.464994	6.773978
6.249197	347.159917	6.778982
6.208913	341.531366	6.783987
6.075553	335.480794	6.788992
6.040796	343.857626	6.793997
6.406930	347.941615	6.799002
5.964781	342.344391	6.804006
6.302826	346.698543	6.809011
5.898052	343.677143	6.814016
5.914605	346.256140	6.819021
6.750034	339.262819	6.824026
6.453731	340.571519	6.829030
6.136145	339.466392	6.834035
5.860464	334.450542	6.839040
5.903705	332.921878	6.844045
6.245397	334.051520	6.849050
5.654968	339.263004	6.854054
6.395780	350.349945	6.859059
5.889889	359.990201	6.864064
6.137599	355.657986	6.869069
6.192934	356.073178	6.874074
5.998112	360.488676	6.879078
6.127914	356.130641	6.884083
6.632640	361.284439	6.889088
5.935621	359.685091	6.894093
6.565948	355.688406	6.899098
6.170405	360.768119	6.904102
6.187366	353.748003	6.909107
6.146433	359.699156	6.914112
6.110668	355.955534	6.919117
6.178078	352.999359	6.924122
6.327530	355.396179	6.929126
5.978390	351.423242	6.934131
6.213789	347.934535	6.939136
6.213836	349.680868	6.944141
5.999967	340.352530	6.949146
5.983008	348.479798	6.954150
5.817964	355.886772	6.959155
6.069758	354.309610	6.964160
5.964425	358.609844	6.969165
6.193935	357.903062	6.974170
6.117991	361.259036	6.979174
6.118519	362.043491	6.984179
6.086238	368.683006	6.989184
6.239115	368.513426	6.994189
6.352245	358.513733	6.999194
6.022359	353.091910	7.004198
6.147427	353.274708	7.009203
6.053967	357.819861	7.014208
5.824075	354.404055	7.019213
6.264206	360.438026	7.024218
6.014964	358.236997	7.029222
6.324084	355.964303	7.034227
6.331252	358.677652	7.039232
6.147227	359.706164	7.044237
6.555638	351.210486	7.049242
6.406577	361.566808	7.054246
6.467623	354.416395	7.059251
6.382082	360.472616	7.064256
6.148950	352.827282	7.069261
6.308211	341.175182	7.074266
5.788874	339.152518	7.079270
5.837741	343.292544	7.084275
5.961504	355.725879	7.089280
6.345210	349.084911	7.094285
6.076571	347.548162	7.099290
6.177666	355.622134	7.104294
6.085092	350.039740	7.109299
6.370787	356.490221	7.114304
6.233669	352.170844	7.119309
6.243006	356.971979	7.124314
6.075624	362.202609	7.129318
6.174366	360.200164	7.134323
6.177820	358.345529	7.139328
6.171536	359.687886	7.144333
6.435501	354.119232	7.149338
6.155233	366.416556	7.154342
6.302469	353.965883	7.159347
6.177301	343.313822	7.164352
5.593837	340.165393	7.169357
6.414644	339.062240	7.174362
5.990972	351.989478	7.179366
6.449587	350.186918	7.184371
6.457563	343.146068	7.189376
5.921652	342.353565	7.194381
6.144933	335.895928	7.199386
6.016449	355.651907	7.204390
6.452857	352.853057	7.209395
6.215361	326.086265	7.214400
5.610641	332.033992	7.219405
5.838047	340.461498	7.224410
5.880451	351.958430	7.229414
6.170972	360.537411	7.234419
6.434932	357.977556	7.239424
5.926549	349.255356	7.244429
6.255172	350.175070	7.249434
6.061359	353.214144	7.254438
5.849177	348.653424	7.259443
6.310082	354.266513	7.264448
6.102082	352.691788	7.269453
5.995892	357.634413	7.274458
6.034555	364.190042	7.279462
5.959325	360.120401	7.284467
6.147843	349.504611	7.289472
6.085848	351.523263	7.294477
6.527375	360.549994	7.299482
6.235976	352.910625	7.304486
6.072708	363.620359	7.309491
6.142447	360.717603	7.314496
5.783353	358.875479	7.319501
6.067425	356.575071	7.324506
6.137746	359.791066	7.329510
6.055815	354.773328	7.334515
6.395869	355.966505	7.339520
6.091046	355.681972	7.344525
6.393825	350.670399	7.349530
6.098746	358.316052	7.354534
6.185517	354.338091	7.359539
6.492343	362.651921	7.364544
6.214221	363.802747	7.369549
6.354899	361.040740	7.374554
6.489959	364.803426	7.379558
6.277229	361.122332	7.384563
6.051147	354.371256	7.389568
5.935333	358.211213	7.394573
6.183019	355.853230	7.399578
6.090914	362.185733	7.404582
6.075275	358.461104	7.409587
6.308764	358.579457	7.414592
6.245982	351.891383	7.419597
6.337168	351.721978	7.424602
5.869493	364.830130	7.429606
5.984626	353.608888	7.434611
6.289033	355.408777	7.439616
6.003590	362.416993	7.444621
6.372174	350.678305	7.449626
5.877871	358.991102	7.454630
6.126321	349.751677	7.459635
6.157254	344.776371	7.464640
6.190320	357.600412	7.469645
6.209393	351.497476	7.474650
6.248959	351.320339	7.479654
6.327407	356.920585	7.484659
6.431220	356.344231	7.489664
6.157196	367.719905	7.494669
6.039674	357.411495	7.499674
6.254852	358.807739	7.504678
5.952012	360.769213	7.509683
6.425063	354.085771	7.514688
6.300158	363.470178	7.519693
6.196764	354.893333	7.524698
5.947381	362.829228	7.529702
6.232347	357.883720	7.534707
6.056658	352.308020	7.539712
6.056740	357.841449	7.544717
6.155359	358.012572	7.549722
6.000451	353.718129	7.554726
6.189025	346.414858	7.559731
6.003235	362.756565	7.564736
6.397811	363.934872	7.569741
6.024558	358.706508	7.574746
6.251108	360.278145	7.579750
6.287032	369.956903	7.584755
6.194706	361.950974	7.589760
5.815007	363.187319	7.594765
5.942577	358.794831	7.599770
6.060203	366.793449	7.604774
5.977489	356.916194	7.609779
5.862106	353.039511	7.614784
5.935431	361.601902	7.619789
6.292455	351.987952	7.624794
6.292453	350.621089	7.629798
6.183698	359.835282	7.634803
6.333671	355.834763	7.639808
6.235231	367.341117	7.644813
6.351275	351.513201	7.649818
6.218823	358.212700	7.654822
5.780437	362.653705	7.659827
6.158372	364.983089	7.664832
5.617458	361.131948	7.669837
5.937016	354.475718	7.674842
5.691376	351.498989	7.679846
6.203340	364.880766	7.684851
6.433901	369.783287	7.689856
6.321915	367.038720	7.694861
6.265880	360.137609	7.699866
5.952246	359.481125	7.704870
6.273730	354.545716	7.709875
6.395972	353.526703	7.714880
5.779097	361.504357	7.719885
6.078075	352.741080	7.724890
6.053832	363.226546	7.729894
5.990730	352.893792	7.734899
6.502528	364.253910	7.739904
6.222783	363.721834	7.744909
6.116864	358.268081	7.749914
6.402533	360.273391	7.754918
6.291187	358.604427	7.759923
6.209018	355.345813	7.764928
6.065952	363.138498	7.769933
6.234420	351.279299	7.774938
6.444500	356.017343	7.779942
6.235235	359.542905	7.784947
6.314393	360.080917	7.789952
6.224401	354.691111	7.794957
6.610939	353.526282	7.799962
6.085876	359.739954	7.804966
6.221288	352.944894	7.809971
6.298822	348.376747	7.814976
6.159127	351.995813	7.819981
6.126404	355.664560	7.824986
5.951463	354.375728	7.829990
6.062880	358.085168	7.834995
6.317316	357.649733	7.840000
6.143531	358.119807	7.845005
6.248855	349.380546	7.850010
6.292273	362.706017	7.855014
6.058957	357.784765	7.860019
6.149976	348.737690	7.865024
6.136600	353.339898	7.870029
6.246190	347.637242	7.875034
5.981263	357.312510	7.880038
6.008821	364.015415	7.885043
6.111363	349.486786	7.890048
5.961129	353.835183	7.895053
6.236095	346.186175	7.900058
5.992265	356.079604	7.905062
6.258482	359.287052	7.910067
6.134032	362.191871	7.915072
6.070162	357.680679	7.920077
6.063442	355.397358	7.925082
6.035974	353.696269	7.930086
5.994741	352.320046	7.935091
5.809128	356.098172	7.940096
5.929425	355.541382	7.945101
6.285079	352.524226	7.950106
5.914677	353.588267	7.955110
6.254579	359.799297	7.960115
6.293056	359.657133	7.965120
6.157284	352.218012	7.970125
6.228977	355.462766	7.975142
6.100015	350.493632	7.980160
6.186844	360.916020	7.985178
6.283547	356.293374	7.990195
6.055138	355.360253	7.995213
6.397429	354.394518	8.000230
6.558031	355.511648	8.005248
6.236236	362.302671	8.010266
6.434399	355.385672	8.015283
5.967746	360.889752	8.020301
6.348219	358.554748	8.025318
6.681224	361.206965	8.030336
6.137352	363.895588	8.035354
6.132485	356.871546	8.040371
6.119489	365.678051	8.045389
6.144618	357.633156	8.050406
6.080215	366.697021	8.055424
6.550959	354.107444	8.060442
6.654952	352.424821	8.065459
6.459207	362.225619	8.070477
6.353353	346.933545	8.075494
6.701223	355.323749	8.080512
6.586484	360.580190	8.085530
6.627463	348.395619	8.090547
6.074865	349.094326	8.095565
6.379131	333.160503	8.100582
6.159406	342.422258	8.105600
6.058964	344.296643	8.110618
6.421159	348.818802	8.115635
6.530279	361.453037	8.120653
6.308126	338.605378	8.125670
6.132515	338.266735	8.130688
6.130115	348.100346	8.135706
6.509392	352.219049	8.140723
6.594452	358.703331	8.145741
6.447407	353.576086	8.150758
6.305798	343.774320	8.155776
6.110439	331.011419	8.160794
6.708889	334.571922	8.165811
6.292616	330.121173	8.170829
6.307979	325.795297	8.175846
6.431673	336.202427	8.180864
6.125610	331.614491	8.185882
6.649856	340.216890	8.190899
6.300372	348.116760	8.195917
6.107416	335.249339	8.200934
6.180663	350.401165	8.205952
6.383808	362.364272	8.210970
6.514961	351.443652	8.215987
6.742679	366.820595	8.221005
6.408423	359.220165	8.226022
6.562099	351.540134	8.231040
6.526578	351.555075	8.236058
6.185115	343.627584	8.241075
6.120828	355.664145	8.246093
6.110499	358.281794	8.251110
6.287430	360.712315	8.256128
6.423364	370.994473	8.261146
6.363463	366.781364	8.266163
5.789667	368.641556	8.271181
6.427610	362.012250	8.276198
6.576563	361.641687	8.281216
6.255964	369.246711	8.286234
6.399744	364.477833	8.291251
6.510393	360.806039	8.296269
6.363139	366.354751	8.301286
6.805412	363.703955	8.306304
6.606046	368.995748	8.311322
6.676594	363.480963	8.316339
6.560978	369.636935	8.321357
6.291865	373.405959	8.326374
6.354634	365.503483	8.331392
6.100648	370.428300	8.336410
6.380933	373.612634	8.341427
6.480564	372.533442	8.346445
6.791734	365.440945	8.351462
6.608697	357.091000	8.356480
6.513303	366.390091	8.361498
6.821303	370.336931	8.366515
6.548899	373.639419	8.371533
6.141949	364.002290	8.376550
6.355444	367.443237	8.381568
6.692993	374.468624	8.386586
6.643896	384.328507	8.391603
6.884038	381.908192	8.396621
6.622331	375.994187	8.401638
6.549504	369.217471	8.406656
6.460449	375.451332	8.411674
6.523085	369.735816	8.416691
6.819642	380.759663	8.421709
6.670577	376.469004	8.426726
6.835751	367.799412	8.431744
6.654837	377.424328	8.436762
6.802770	356.658265	8.441779
6.699605	368.038218	8.446797
6.610490	360.932702	8.451814
6.638175	368.072907	8.456832
6.584243	368.586187	8.461850
7.105772	365.105632	8.466867
6.625303	369.182322	8.471885
6.582847	368.964824	8.476902
6.517377	358.368492	8.481920
6.500751	368.879676	8.486938
6.659595	362.615766	8.491955
6.603045	369.220068	8.496973
6.678435	377.952772	8.501990
6.999684	375.914219	8.507008
6.664389	371.886266	8.512026
6.925642	366.559348	8.517043
6.838848	359.939455	8.522061
6.693702	365.115456	8.527078
6.898370	359.718511	8.532096
6.603056	369.099420	8.537114
7.140665	369.567353	8.542131
6.871233	364.572888	8.547149
7.056473	369.829667	8.552166
6.873138	372.329260	8.557184
6.682174	374.063199	8.562202
6.823806	369.960522	8.567219
6.796765	370.321268	8.572237
6.872670	365.203269	8.577255
6.965836	366.586581	8.582272
6.851560	375.402648	8.587290
6.730700	367.901322	8.592307
6.513794	374.729564	8.597325
6.401837	369.934483	8.602343
6.632833	357.177343	8.607360
6.626637	369.476207	8.612378
6.589520	366.913145	8.617395
6.613762	374.101229	8.622413
6.755053	380.081254	8.627431
6.994414	388.198145	8.632448
6.839029	391.419186	8.637466
6.716399	384.041205	8.642483
6.663201	384.582773	8.647501
6.769271	394.128019	8.652519
7.136873	385.489817	8.657536
6.926455	385.749909	8.662554
6.996918	384.252415	8.667571
7.006953	386.737491	8.672589
6.730559	393.104852	8.677607
7.239527	382.910801	8.682624
6.967167	382.063459	8.687642
7.045404	375.487130	8.692659
7.157974	384.425448	8.697677
7.189917	375.997629	8.702695
7.227497	365.056948	8.707712
6.844861	376.016797	8.712730
6.558966	372.754266	8.717747
6.705454	367.912380	8.722765
6.786136	385.717064	8.727783
7.007147	382.034286	8.732800
6.923283	397.542124	8.737818
7.295295	381.367272	8.742835
7.358648	381.909513	8.747853
6.769598	378.590339	8.752871
7.038226	375.177808	8.757888
7.197674	373.688463	8.762906
6.851149	366.481266	8.767923
6.936870	367.370291	8.772941
6.633688	379.239175	8.777959
7.010817	376.544936	8.782976
7.063206	388.332868	8.787994
7.289131	379.095181	8.793011
6.980933	387.534546	8.798029
6.880901	384.100882	8.803047
7.110252	375.916684	8.808064
6.948402	385.014761	8.813082
6.977657	378.332499	8.818099
7.026526	386.264643	8.823117
6.923323	382.976641	8.828135
6.869521	385.152987	8.833152
7.169138	384.288610	8.838170
7.150370	386.478402	8.843187
7.026024	384.882044	8.848205
6.691011	387.553725	8.853223
6.831123	385.423633	8.858240
6.954253	387.985662	8.863258
6.897261	384.576812	8.868275
6.836757	384.560954	8.873293
6.743672	395.437579	8.878311
7.223544	397.713344	8.883328
7.194548	404.546869	8.888346
7.306748	409.098745	8.893363
7.726296	408.101968	8.898381
7.569422	407.034562	8.903399
7.292351	383.557985	8.908416
6.958793	391.439600	8.913434
6.967339	385.151894	8.918451
6.995767	384.396278	8.923469
6.987108	402.262312	8.928487
7.189531	408.406336	8.933504
7.223517	410.635202	8.938522
7.472188	411.031644	8.943539
7.586060	408.605863	8.948557
7.123281	400.375466	8.953575
7.192550	380.325436	8.958592
7.028783	385.567476	8.963610
7.406153	395.638253	8.968627
7.520295	406.990494	8.973645
7.480163	405.115855	8.978663
7.169261	388.836560	8.983680
7.158972	390.520102	8.988698
6.752571	384.269009	8.993715
7.179226	389.566863	8.998733
7.190400	394.475387	9.003751
7.593905	397.574148	9.008768
7.301675	402.066315	9.013786
6.996958	402.688316	9.018803
7.489744	403.068601	9.023821
7.393138	410.515471	9.028839
7.495997	406.614518	9.033856
7.283780	410.898492	9.038874
7.313214	413.046022	9.043891
7.645954	416.446205	9.048909
7.313195	415.248567	9.053927
7.326479	403.544819	9.058944
6.997643	412.022142	9.063962
6.964422	400.600233	9.068979
7.359468	401.813174	9.073997
7.238701	408.869359	9.079015
7.443301	400.405010	9.084032
7.394834	404.303569	9.089050
7.263494	397.037399	9.094067
7.559639	398.846497	9.099085
7.249895	400.548557	9.104103
7.399822	402.718231	9.109120
7.415147	404.236817	9.114138
6.905391	401.719401	9.119155
7.227770	394.644071	9.124173
7.385610	412.395668	9.129191
7.135225	406.912219	9.134208
7.535740	404.880178	9.139226
7.478563	416.584311	9.144243
7.525435	408.640126	9.149261
7.270862	423.281651	9.154279
7.689128	425.276742	9.159296
7.357792	425.293852	9.164314
7.578052	428.026859	9.169331
7.642813	424.258102	9.174349
7.463672	411.959655	9.179367
7.348875	414.552655	9.184384
7.644686	424.721433	9.189402
7.454799	424.940440	9.194419
7.797895	424.081872	9.199437
7.440698	424.541685	9.204455
7.573998	426.846509	9.209472
7.743282	416.797178	9.214490
7.682457	414.859510	9.219507
7.432092	406.128775	9.224525
7.286898	419.093228	9.229543
7.442441	419.431679	9.234560
7.236766	425.159973	9.239578
7.309872	432.690714	9.244595
7.504086	427.693014	9.249613
7.521329	434.563486	9.254631
7.720973	425.541330	9.259648
7.766093	429.860728	9.264666
7.207337	436.243942	9.269683
7.924992	432.369732	9.274701
7.790095	430.935967	9.279719
7.490842	426.823461	9.284736
7.748311	431.204261	9.289754
7.734220	438.568788	9.294771
7.677557	431.937836	9.299789
7.474773	436.371815	9.304807
7.752553	436.451277	9.309824
7.909262	433.816811	9.314842
7.443415	434.069588	9.319859
7.617668	432.243407	9.324877
7.390967	444.983966	9.329895
7.579956	438.469155	9.334912
7.648057	437.849330	9.339930
7.255711	431.050070	9.344947
7.733051	424.931893	9.349965
7.707691	444.151255	9.354983
7.541594	452.981792	9.360000
7.856659	450.070051	9.365018
7.710216	450.787174	9.370035
7.843114	453.470758	9.375053
7.814857	458.186663	9.380071
7.951009	454.577126	9.385088
8.168556	450.131180	9.390106
7.772468	437.137724	9.395123
7.508684	422.769724	9.400141
7.923677	429.173935	9.405159
7.519118	433.125138	9.410176
8.119748	436.180398	9.415194
7.754601	437.796469	9.420211
8.016773	437.256689	9.425229
7.666714	441.174108	9.430247
8.077388	439.765314	9.435264
7.764575	423.246449	9.440282
7.944923	420.769225	9.445299
8.126759	427.920015	9.450317
7.886307	423.293374	9.455335
7.692478	431.396107	9.460352
7.490186	426.299588	9.465370
7.543093	449.871120	9.470387
8.063980	441.698019	9.475405
8.094341	461.647119	9.480423
7.958126	454.943417	9.485440
8.117620	452.721919	9.490458
7.673026	457.900684	9.495475
8.151076	457.841470	9.500493
8.210571	457.342913	9.505511
7.934918	441.070671	9.510528
7.783518	432.687331	9.515546
7.707107	445.467458	9.520563
8.265089	456.690230	9.525581
7.948826	464.802693	9.530599
8.138244	462.346134	9.535616
8.171201	447.619198	9.540634
7.892324	439.505134	9.545651
7.786374	431.026312	9.550669
7.637193	436.581658	9.555687
7.732598	453.143885	9.560704
8.344333	452.151708	9.565722
7.947313	461.532821	9.570739
8.129426	452.320896	9.575757
8.247060	453.056603	9.580775
8.311101	462.908271	9.585792
8.290186	451.869406	9.590810
8.286092	449.282223	9.595827
7.936639	437.669999	9.600845
7.983910	432.988808	9.605863
8.063278	441.029806	9.610880
8.078354	435.997055	9.615898
8.160046	445.798611	9.620915
8.233381	445.395714	9.625933
7.912032	445.092526	9.630951
7.741970	453.948930	9.635968
7.978738	450.803307	9.640986
7.949417	462.133880	9.646003
8.007329	454.755984	9.651021
8.359882	457.846960	9.656039
7.870466	465.494254	9.661056
8.256543	454.524162	9.666074
7.901555	456.760330	9.671091
8.009280	461.502267	9.676109
8.076288	457.941432	9.681127
7.900808	453.916823	9.686144
8.230255	451.940092	9.691162
8.278660	456.098037	9.696179
8.088678	446.679331	9.701197
7.940219	457.839221	9.706215
8.161650	462.717976	9.711232
8.420408	446.788026	9.716250
8.313065	459.042840	9.721267
8.277940	450.360410	9.726285
8.130655	459.172223	9.731303
8.002033	455.654663	9.736320
8.311093	450.225556	9.741338
8.102791	466.333612	9.746355
8.434226	471.491777	9.751373
8.538296	474.571197	9.756391
8.390559	462.706447	9.761408
8.439964	450.122859	9.766426
8.255770	454.979960	9.771443
8.389360	453.715564	9.776461
8.171802	446.459726	9.781479
7.983751	460.099947	9.786496
8.402453	468.703166	9.791514
8.175760	475.656055	9.796531
8.476093	478.493287	9.801549
8.550269	481.321774	9.806567
8.454947	476.798610	9.811584
8.234339	473.932926	9.816602
8.483856	482.467987	9.821619
8.436146	477.801665	9.826637
8.423151	475.067551	9.831655
8.361018	485.999341	9.836672
8.558343	480.549863	9.841690
8.445477	472.870516	9.846707
8.226130	476.669634	9.851725
8.219637	477.383766	9.856743
8.193921	494.965390	9.861760
8.471557	484.012271	9.866778
8.348926	482.829042	9.871795
8.558591	481.969287	9.876813
8.447842	482.235855	9.881831
8.015657	487.163377	9.886848
8.616157	480.656659	9.891866
8.118289	482.984644	9.896883
8.483798	480.888652	9.901901
8.470027	478.426057	9.906919
8.163030	483.390768	9.911936
8.245055	483.980578	9.916954
8.057698	479.351915	9.921971
8.713709	486.172816	9.926989
8.789431	499.156361	9.932007
8.584827	491.844828	9.937024
8.678731	479.146951	9.942042
8.510582	484.604299	9.947059
8.659189	482.150975	9.952077
8.619476	482.002473	9.957095
8.145727	481.603243	9.962112
8.439010	489.137380	9.967130
8.783513	501.491839	9.972147
8.831909	503.961454	9.977165
8.874434	487.831819	9.982183
8.568996	489.249192	9.987200
8.713213	487.670706	9.992218
8.777689	483.832554	9.997235
8.764426	470.312037	10.002253
8.483505	480.385019	10.007271
8.473834	485.104331	10.012288
8.690218	488.970880	10.017306
8.490658	487.594579	10.022323
8.700508	501.109371	10.027341
9.299825	495.262391	10.032359
8.684491	500.480543	10.037376
8.697867	488.379096	10.042394
9.030140	482.889538	10.047411
8.632406	487.073211	10.052429
9.047985	485.474298	10.057447
8.748304	485.205584	10.062464
8.794683	486.580457	10.067482
8.754164	480.780083	10.072499
8.738240	486.254606	10.077517
8.999557	481.659784	10.082535
8.731694	484.204194	10.087552
8.911728	479.577927	10.092570
8.782127	473.318146	10.097587
8.659274	477.493462	10.102605
8.658447	475.208718	10.107623
8.668472	481.348199	10.112640
8.838860	476.783404	10.117658
8.934618	479.393916	10.122675
8.683359	488.259903	10.127693
8.820030	475.066183	10.132711
8.834456	482.230601	10.137728
9.156240	482.334726	10.142746
8.788708	480.596583	10.147763
8.627794	485.257542	10.152781
9.264434	473.348783	10.157799
8.607908	484.036034	10.162816
8.796394	480.238412	10.167834
8.729817	470.573141	10.172851
8.814152	484.277999	10.177869
9.028871	498.098137	10.182887
9.032392	503.784212	10.187904
9.398332	488.437030	10.192922
9.136457	477.082456	10.197939
8.704463	482.694751	10.202957
9.031327	486.313617	10.207975
8.879161	482.023419	10.212992
8.715140	473.455846	10.218010
9.158064	481.266332	10.223027
8.848530	484.038176	10.228045
9.214363	496.253591	10.233063
8.807821	486.641578	10.238080
9.091616	492.643494	10.243098
9.233880	490.699244	10.248115
8.683817	492.079207	10.253133
9.088079	493.243374	10.258151
9.422672	498.713474	10.263168
9.175941	486.984139	10.268186
8.813825	481.464524	10.273203
8.749065	486.113574	10.278221
9.268804	491.567286	10.283239
8.803242	501.498797	10.288256
9.357088	501.768533	10.293274
9.573848	496.978718	10.298291
9.280884	497.163383	10.303309
9.236727	481.116763	10.308327
8.965918	486.135765	10.313344
8.904333	480.587998	10.318362
9.206843	480.139725	10.323379
8.946316	485.532653	10.328397
9.367351	490.544242	10.333415
9.158443	500.599641	10.338432
9.137276	487.288632	10.343450
9.463796	492.665321	10.348467
9.319309	487.117918	10.353485
9.193591	478.648483	10.358503
9.118142	480.957619	10.363520
9.183583	473.266114	10.368538
8.906370	488.315179	10.373555
9.183716	492.686568	10.378573
9.334972	501.173918	10.383591
9.141880	507.373634	10.388608
9.523902	503.451011	10.393626
9.555326	501.189613	10.398643
9.084171	495.598716	10.403661
9.298291	499.077460	10.408679
9.647031	493.560073	10.413696
9.623785	491.673312	10.418714
9.497105	476.791485	10.423731
9.127047	483.523845	10.428749
9.367926	478.569311	10.433767
9.105529	476.164606	10.438784
9.101428	481.069235	10.443802
8.892085	486.223772	10.448819
9.163889	494.629115	10.453837
9.423012	494.209731	10.458855
9.448943	500.798003	10.463872
9.435406	509.191257	10.468890
9.470211	496.963371	10.473907
9.354298	501.787695	10.478925
9.678512	495.538853	10.483943
9.545800	496.995435	10.488960
9.550842	503.056810	10.493978
9.506363	500.475947	10.498995
9.751102	499.979922	10.504013
9.471181	488.180047	10.509031
9.216661	480.917364	10.514048
9.047214	482.771017	10.519066
9.356500	485.439592	10.524083
9.214687	491.637580	10.529101
9.422696	498.793765	10.534119
9.224125	502.703241	10.539136
9.518728	505.251044	10.544154
9.653260	500.609811	10.549171
9.365724	495.495070	10.554189
9.478640	499.683943	10.559207
9.642052	500.100057	10.564224
9.230732	504.958044	10.569242
9.306459	495.071650	10.574259
9.388303	500.511924	10.579277
9.619146	494.476526	10.584295
9.282627	505.921531	10.589312
9.632679	500.343976	10.594330
9.703332	500.389619	10.599347
9.482770	499.351120	10.604365
9.512044	501.605982	10.609383
9.746490	516.568592	10.614400
9.651837	510.921856	10.619418
9.551176	514.724476	10.624435
10.004254	520.819799	10.629453
9.927162	511.673702	10.634471
9.797599	505.549603	10.639488
9.592267	506.954449	10.644506
9.843120	502.566387	10.649523
9.628200	502.634683	10.654541
9.818064	504.630856	10.659559
9.489445	505.401771	10.664576
9.413429	507.991865	10.669594
9.684680	501.050735	10.674611
9.733778	512.798240	10.679629
9.497035	524.038276	10.684647
9.680271	530.103298	10.689664
9.889180	527.340720	10.694682
9.838901	522.043632	10.699699
9.843196	534.085346	10.704717
9.677535	529.222898	10.709735
9.771838	525.342194	10.714752
9.804202	528.252978	10.719770
9.929603	523.714155	10.724787
9.942737	531.538355	10.729805
9.625930	531.546876	10.734823
9.891853	525.647981	10.739840
9.559986	528.000455	10.744858
10.073726	529.220055	10.749875
9.699760	528.808345	10.754893
9.785167	518.150410	10.759911
9.921339	520.697792	10.764928
10.065848	523.026119	10.769946
10.342836	518.927446	10.774963
10.079380	523.980019	10.779981
10.053689	516.725649	10.784999
9.894906	509.429019	10.790016
9.464557	517.729795	10.795034
9.642921	518.582221	10.800051
9.987391	522.248829	10.805069
10.009182	530.920578	10.810087
9.912575	519.994515	10.815104
10.092384	524.580009	10.820122
9.822122	520.810075	10.825139
9.685113	525.732385	10.830157
9.750365	526.539419	10.835175
9.932503	521.553052	10.840192
9.761307	529.895279	10.845210
9.585598	520.130316	10.850227
9.759885	526.572277	10.855245
9.809097	542.365501	10.860263
9.992315	551.886122	10.865280
9.971839	550.011544	10.870298
10.247090	540.841785	10.875315
10.100024	557.331646	10.880333
10.049122	550.930120	10.885351
9.953103	543.740407	10.890368
10.416816	548.224620	10.895386
10.233884	550.339168	10.900403
10.429555	555.464980	10.905421
10.254823	551.437076	10.910439
10.251118	535.251526	10.915456
9.946900	538.925100	10.920474
10.531646	542.999031	10.925491
10.171469	539.792288	10.930509
10.089507	525.641868	10.935527
10.189090	528.081376	10.940544
9.869240	536.951823	10.945562
9.949647	539.498477	10.950579
10.270791	552.639268	10.955597
10.080219	552.728996	10.960615
10.435767	554.964301	10.965632
10.468832	560.961344	10.970650
10.344568	558.553919	10.975667
10.407632	552.626840	10.980685
10.400358	556.184464	10.985703
10.527914	552.462646	10.990720
10.071310	545.966898	10.995738
10.244644	546.839049	11.000755
10.286296	549.549566	11.005773
10.098058	554.584052	11.010791
10.426403	545.844626	11.015808
10.247048	553.626412	11.020826
10.291555	551.053690	11.025843
10.605957	553.320688	11.030861
10.807944	553.295262	11.035879
10.567878	543.186921	11.040896
10.289336	547.001640	11.045914
10.486895	543.010081	11.050931
10.206015	537.398826	11.055949
10.378595	540.846217	11.060967
10.796174	547.862290	11.065984
10.304646	550.104084	11.071002
10.557561	537.106698	11.076019
10.092636	538.492259	11.081037
10.414133	544.090657	11.086055
10.580469	538.873232	11.091072
10.426224	550.491677	11.096090
10.570362	553.561677	11.101107
10.604101	548.806835	11.106125
10.509523	551.769071	11.111143
10.560518	547.544855	11.116160
10.040967	560.110474	11.121178
10.389231	543.797187	11.126195
10.577060	547.087557	11.131213
10.156907	550.804544	11.136231
10.412564	547.491843	11.141248
10.390116	544.434154	11.146266
10.451123	536.424581	11.151283
10.367125	548.139315	11.156301
10.338651	552.646997	11.161319
10.382446	550.430991	11.166336
10.460144	564.376790	11.171354
10.915539	567.552658	11.176371
10.681811	565.708336	11.181389
10.617541	562.111244	11.186407
10.428996	559.212120	11.191424
10.347926	574.899554	11.196442
10.658790	572.493378	11.201459
10.789051	570.841333	11.206477
10.771947	573.119249	11.211495
10.751841	573.283253	11.216512
10.471489	579.648144	11.221530
10.736162	570.912371	11.226547
10.862540	577.238781	11.231565
10.923867	576.067749	11.236583
11.080952	570.977997	11.241600
10.733029	579.799215	11.246618
10.776602	573.752106	11.251635
10.920324	570.390667	11.256653
10.889905	577.719940	11.261671
10.739432	575.382891	11.266688
10.966333	574.671910	11.271706
10.930675	566.838415	11.276723
10.837255	573.252910	11.281741
11.047970	583.760158	11.286759
11.184399	567.849267	11.291776
10.994945	560.144013	11.296794
10.846234	556.206704	11.301811
11.046640	556.137344	11.306829
10.765678	547.269323	11.311847
10.919767	547.103079	11.316864
10.475426	554.112190	11.321882
10.512442	562.248240	11.326899
10.495507	580.428173	11.331917
10.852212	573.943840	11.336935
11.020076	573.362029	11.341952
10.925329	583.285978	11.346970
10.892675	582.265370	11.351987
10.989642	578.614610	11.357005
10.541043	583.027180	11.362023
11.012145	585.556808	11.367040
10.710978	585.263078	11.372058
11.001335	585.624592	11.377075
10.985240	574.562805	11.382093
10.766273	587.210735	11.387111
10.869874	579.478492	11.392128
11.269576	596.611710	11.397146
11.066783	590.798856	11.402163
11.012503	578.758441	11.407181
10.892025	579.676628	11.412199
11.050497	583.564894	11.417216
11.283491	600.367631	11.422234
11.366862	596.561208	11.427251
11.407476	579.765916	11.432269
11.096680	582.705230	11.437287
11.110570	576.839495	11.442304
11.444364	570.668021	11.447322
11.295985	580.379466	11.452339
11.276559	570.851920	11.457357
11.308729	573.510279	11.462375
11.355168	559.380740	11.467392
11.478045	573.780213	11.472410
10.962253	565.362386	11.477427
11.080994	566.236779	11.482445
10.675041	578.516371	11.487463
11.467350	578.133365	11.492480
11.056796	572.050113	11.497498
11.238298	579.021136	11.502515
11.271138	585.040313	11.507533
11.284899	588.408457	11.512551
11.310052	592.279743	11.517568
11.063085	588.067489	11.522586
11.062744	598.484738	11.527603
11.170431	602.453549	11.532621
11.158525	604.591799	11.537639
11.281135	608.627700	11.542656
11.349897	600.705247	11.547674
10.833555	616.249477	11.552691
11.016181	602.171150	11.557709
11.130388	603.781557	11.562727
11.185370	600.345654	11.567744
11.563377	608.093784	11.572762
11.267206	612.974783	11.577779
11.537401	609.861764	11.582797
11.615073	610.401769	11.587815
11.700724	608.229691	11.592832
11.744410	594.693845	11.597850
11.430484	601.540530	11.602867
11.517743	589.743018	11.607885
11.495779	600.460302	11.612903
10.924814	596.623857	11.617920
11.207578	609.395162	11.622938
11.384537	612.419004	11.627955
11.592448	617.640747	11.632973
11.690678	627.275709	11.637991
11.377168	611.069204	11.643008
11.431804	623.279816	11.648026
11.676349	621.041815	11.653043
11.661497	621.381722	11.658061
11.698117	626.677642	11.663079
12.111047	616.930852	11.668096
11.916227	624.014503	11.673114
11.933440	614.067783	11.678131
11.762445	599.356899	11.683149
11.798084	597.640781	11.688167
11.319508	593.632071	11.693184
11.501300	598.955731	11.698202
11.298258	610.092710	11.703219
11.981374	610.802941	11.708237
11.903162	617.994552	11.713255
12.081145	619.613903	11.718272
11.901462	601.552916	11.723290
11.551218	599.629016	11.728307
11.723325	599.324249	11.733325
11.767063	588.461362	11.738343
11.944975	588.726885	11.743360
11.537452	596.449765	11.748378
11.183440	609.112558	11.753395
11.597292	606.920615	11.758413
11.775591	613.033776	11.763431
11.803409	617.131868	11.768448
11.530696	623.814313	11.773466
11.560110	623.437229	11.778483
12.195859	618.247220	11.783501
11.684018	610.683974	11.788519
11.918579	623.071523	11.793536
11.860470	618.476221	11.798554
11.517580	617.867135	11.803571
11.660523	617.560626	11.808589
11.707784	620.592168	11.813607
12.095476	615.595659	11.818624
12.118446	608.450392	11.823642
11.854181	616.182393	11.828659
12.330107	616.764140	11.833677
11.862076	621.574239	11.838695
11.830908	612.881642	11.843712
11.818546	615.931992	11.848730
12.041032	617.430762	11.853747
11.947785	619.651186	11.858765
11.900798	615.032052	11.863783
11.914153	619.851933	11.868800
12.303064	635.708781	11.873818
12.177846	630.079419	11.878835
12.070383	617.999973	11.883853
11.784731	627.909677	11.888871
12.201448	624.477053	11.893888
12.515424	638.073465	11.898906
12.486928	634.505468	11.903923
12.266661	618.767183	11.908941
12.423590	613.137801	11.913959
12.303695	606.264228	11.918976
12.791282	616.642909	11.923994
12.224735	616.356044	11.929011
12.213349	602.712057	11.934029
12.155270	611.516280	11.939047
12.273890	606.438856	11.944064
12.163726	611.726212	11.949082
12.172857	610.891559	11.954099
11.965279	611.656137	11.959117
11.855055	624.542676	11.964135
12.010894	624.937890	11.969152
12.258343	614.756280	11.974170
12.420251	624.810454	11.979187
12.104818	619.924110	11.984205
12.141446	611.530160	11.989223
11.995199	618.688250	11.994240
12.346778	624.168350	11.999258
11.970228	636.607476	12.004275
12.441916	636.476677	12.009293
12.248993	639.766760	12.014311
12.159248	643.959017	12.019328
12.507828	638.772970	12.024346
12.141052	645.978247	12.029363
12.301541	638.997614	12.034381
12.513216	641.820362	12.039399
12.358715	641.554144	12.044416
12.550288	635.865678	12.049434
12.147791	648.062725	12.054451
12.419444	646.950252	12.059469
12.423089	647.473454	12.064487
12.306625	645.061640	12.069504
12.461971	644.948847	12.074522
12.390728	649.526370	12.079539
12.511412	642.671893	12.084557
12.669964	637.856447	12.089575
12.143503	644.786941	12.094592
12.830673	639.532065	12.099610
12.755221	643.554825	12.104627
12.416219	643.715146	12.109645
12.472419	638.909425	12.114663
12.392888	644.251951	12.119680
12.595367	635.554294	12.124698
12.366919	646.221906	12.129715
12.933206	657.743306	12.134733
13.082314	654.936429	12.139751
12.812863	645.047230	12.144768
12.689309	634.166345	12.149786
12.312513	641.540447	12.154803
12.328277	641.329603	12.159821
12.453929	653.598537	12.164839
12.331714	656.918571	12.169856
12.966276	656.885328	12.174874
12.883665	660.053990	12.179891
13.223119	667.353750	12.184909
13.174766	663.331265	12.189927
12.861653	654.016948	12.194944
13.121373	640.021186	12.199962
12.716161	652.303867	12.204979
12.630512	649.158233	12.209997
12.715982	637.307321	12.215015
12.326202	645.008507	12.220032
12.808608	653.784872	12.225050
12.963181	656.928994	12.230067
12.838342	658.232877	12.235085
13.422302	652.785884	12.240103
12.712574	650.192467	12.245120
12.992794	660.578417	12.250138
13.035258	660.596919	12.255155
12.640998	654.823511	12.260173
13.163735	657.723757	12.265191
12.989545	670.980113	12.270208
13.192143	664.608255	12.275226
12.741007	664.896600	12.280243
13.019502	669.760159	12.285261
13.175433	657.153423	12.290279
13.095293	664.354822	12.295296
13.003964	653.765523	12.300314
12.969383	651.470266	12.305331
12.841837	660.752457	12.310349
12.799765	661.046136	12.315367
12.599897	664.763346	12.320384
12.889480	664.115124	12.325402
12.885523	663.604412	12.330419
12.793366	670.268052	12.335437
13.278622	660.954875	12.340455
12.763921	671.922973	12.345472
13.255142	664.354023	12.350490
13.287821	659.586696	12.355507
12.817743	660.793192	12.360525
12.984771	660.179951	12.365543
13.225968	672.547559	12.370560
13.579992	674.426512	12.375578
13.489053	671.815034	12.380595
13.689593	667.210753	12.385613
13.300019	661.250415	12.390631
13.146330	661.495311	12.395648
13.400863	656.166204	12.400666
13.170181	655.700483	12.405683
13.333257	658.291006	12.410701
13.503068	653.180302	12.415719
13.015393	663.086965	12.420736
13.227609	654.999999	12.425754
13.326796	665.714119	12.430771
13.192449	660.821482	12.435789
13.356850	651.359765	12.440807
13.318942	655.076843	12.445824
13.512725	655.866901	12.450842
13.191300	661.679678	12.455859
13.431645	658.659690	12.460877
13.114050	654.890832	12.465895
13.105754	673.953132	12.470912
13.479751	673.705095	12.475930
13.481931	684.421802	12.480947
13.469798	680.819673	12.485965
13.536079	687.903466	12.490983
13.409710	683.719631	12.496000
13.472882	691.681228	12.501018
13.547384	694.074195	12.506035
13.963639	678.327647	12.511053
13.869610	682.750959	12.516071
13.682823	681.243253	12.521088
13.784595	668.840655	12.526106
13.473913	662.782749	12.531123
13.471814	672.228327	12.536141
13.725931	664.955303	12.541159
13.341348	682.344030	12.546176
13.751061	686.088812	12.551194
13.928937	687.070712	12.556211
13.491815	688.600251	12.561229
14.117379	679.435495	12.566247
13.412255	674.250430	12.571264
13.398734	670.004736	12.576282
13.353343	682.063803	12.581299
13.529011	684.469320	12.586317
13.739035	687.178725	12.591335
13.439651	691.429086	12.596352
13.663698	689.169042	12.601370
13.660699	689.945751	12.606387
13.884342	687.423838	12.611405
13.890223	677.920673	12.616423
13.718440	693.199544	12.621440
13.995533	689.971821	12.626458
14.019251	687.099379	12.631475
13.429722	697.085135	12.636493
13.869410	682.332149	12.641511
13.932076	697.075672	12.646528
13.791300	685.809289	12.651546
13.975739	692.252875	12.656563
13.719976	690.026982	12.661581
13.764735	689.088913	12.666599
13.654365	693.290725	12.671616
13.673186	691.024966	12.676634
14.296360	694.546956	12.681651
13.786431	700.026362	12.686669
14.075265	700.025197	12.691687
14.017900	713.597798	12.696704
14.388453	704.857994	12.701722
14.091383	696.358497	12.706739
14.240692	685.460075	12.711757
14.285408	687.384336	12.716775
13.856139	691.582464	12.721792
14.260429	682.458687	12.726810
13.963674	678.244744	12.731827
13.980306	686.980494	12.736845
13.895934	676.790879	12.741863
13.990248	697.465527	12.746880
14.371097	702.960002	12.751898
14.476129	694.293363	12.756915
14.333654	688.347949	12.761933
14.284844	680.109365	12.766951
13.882019	686.758571	12.771968
13.978569	676.679465	12.776986
14.308403	697.241472	12.782003
14.205069	708.309242	12.787021
14.378212	708.928966	12.792039
13.988312	704.685429	12.797056
14.507252	703.862414	12.802074
14.488818	702.606040	12.807091
14.155385	693.329600	12.812109
14.176866	694.932453	12.817127
14.336180	702.269920	12.822144
14.290058	711.091253	12.827162
14.233341	710.333185	12.832179
14.076251	709.044887	12.837197
14.507215	706.187529	12.842215
14.376302	718.354695	12.847232
13.956772	712.048738	12.852250
14.083947	712.085526	12.857267
13.953237	711.881851	12.862285
14.325816	712.123187	12.867303
14.386457	712.539631	12.872320
14.343970	714.944619	12.877338
14.392474	712.500636	12.882355
14.386713	727.775616	12.887373
14.663099	729.597311	12.892391
14.461298	730.979530	12.897408
14.660212	729.629140	12.902426
14.541075	721.878084	12.907443
14.201723	722.944181	12.912461
14.687901	722.691190	12.917479
14.826487	721.915144	12.922496
14.957664	727.196279	12.927514
14.597872	717.005612	12.932531
14.526704	717.373280	12.937549
14.669988	725.363366	12.942567
15.013021	736.623150	12.947584
14.841881	722.622246	12.952602
15.051808	718.262635	12.957619
14.721008	709.276109	12.962637
14.448551	705.607465	12.967655
14.393883	704.596611	12.972672
14.594171	723.575791	12.977690
14.612876	728.379084	12.982707
14.843546	729.968100	12.987725
14.461738	736.888588	12.992743
14.719514	735.759350	12.997760
14.971140	736.676048	13.002778
15.047505	732.567735	13.007795
15.225849	738.813477	13.012813
15.036376	728.144835	13.017831
15.069872	730.077170	13.022848
14.370486	718.749965	13.027866
14.942953	717.710279	13.032883
14.756840	724.467556	13.037901
14.880051	713.418571	13.042919
15.231710	731.143273	13.047936
15.058409	727.875657	13.052954
15.441450	720.658151	13.057971
14.904081	720.328842	13.062989
15.213281	713.144998	13.068007
15.430831	715.335674	13.073024
14.970362	707.357237	13.078042
14.866725	700.869245	13.083059
14.983145	699.127838	13.088077
14.820254	704.739064	13.093095
14.953255	702.527998	13.098112
14.907972	717.575630	13.103130
15.388357	718.655302	13.108147
15.200810	724.434501	13.113165
14.939160	721.799269	13.118183
15.225702	724.465133	13.123200
15.296542	718.158081	13.128218
15.234598	717.811088	13.133235
15.179167	721.960118	13.138253
15.607197	717.496906	13.143271
15.003837	707.271823	13.148288
15.008160	718.619379	13.153306
15.359872	717.863590	13.158323
15.146254	720.443715	13.163341
15.396894	720.555833	13.168359
15.226626	721.690112	13.173376
15.011878	726.744579	13.178394
14.828049	713.765001	13.183411
15.063899	723.583581	13.188429
15.339605	725.698874	13.193447
15.618436	721.350557	13.198464
14.935595	716.032599	13.203482
15.628854	727.038687	13.208499
15.478264	727.491382	13.213517
15.800244	731.076350	13.218535
15.541701	720.942401	13.223552
15.427911	726.426019	13.228570
15.579664	718.121280	13.233587
15.486796	723.213454	13.238605
15.730354	723.386642	13.243623
15.813234	725.052462	13.248640
15.611152	720.157798	13.253658
15.906633	718.621864	13.258675
15.738053	728.346022	13.263693
15.689400	715.944869	13.268711
15.878612	696.822437	13.273728
15.172359	700.079350	13.278746
15.749201	704.182960	13.283763
15.521076	719.751550	13.288781
15.483043	722.222113	13.293799
15.764554	719.994088	13.298816
15.524817	724.598031	13.303834
15.368630	724.493023	13.308851
15.446308	727.589245	13.313869
15.672680	728.374199	13.318887
15.986370	722.470912	13.323904
15.455693	728.199731	13.328922
15.676393	724.731527	13.333939
15.557262	714.828204	13.338957
15.390817	724.129146	13.343975
15.562930	713.350211	13.348992
15.495529	721.139775	13.354010
15.635374	722.547360	13.359027
16.137773	728.748637	13.364045
15.833022	734.536734	13.369063
15.799258	732.743115	13.374080
15.902348	745.697305	13.379098
16.121374	740.664072	13.384115
16.161548	726.888834	13.389133
16.003304	724.912746	13.394151
16.097887	719.198425	13.399168
15.575837	720.277368	13.404186
16.057144	715.458669	13.409203
16.007010	718.840004	13.414221
15.833350	715.648186	13.419239
16.317471	734.901645	13.424256
15.837139	724.123943	13.429274
16.147653	717.735158	13.434291
15.817854	724.688518	13.439309
16.140947	741.218495	13.444327
16.280265	733.852976	13.449344
16.272703	738.199637	13.454362
16.208686	738.152772	13.459379
15.931912	720.252045	13.464397
16.022781	732.220369	13.469415
16.043082	734.688106	13.474432
16.242784	733.473292	13.479450
16.325218	739.450037	13.484467
16.126024	733.052745	13.489485
16.257548	731.873860	13.494503
16.471555	738.587387	13.499520
16.330449	744.857935	13.504538
16.216875	735.165171	13.509555
16.489508	732.531434	13.514573
16.224305	730.802478	13.519591
16.552048	736.538815	13.524608
16.076776	730.809632	13.529626
16.251117	739.293479	13.534643
16.371853	747.511172	13.539661
16.657140	737.519225	13.544679
16.485891	742.749918	13.549696
16.016662	746.089624	13.554714
16.480975	739.790344	13.559731
16.282207	749.206817	13.564749
16.236034	746.376874	13.569767
16.459526	738.395402	13.574784
16.007687	743.919369	13.579802
16.164879	737.557755	13.584819
16.219503	751.504160	13.589837
16.102128	743.645521	13.594855
16.374258	748.642645	13.599872
16.284296	758.177775	13.604890
16.267200	764.072292	13.609907
16.677048	762.859265	13.614925
16.656148	773.156760	13.619943
16.886305	767.872465	13.624960
16.689522	776.736372	13.629978
16.986209	771.937117	13.634995
16.943149	767.793858	13.640013
16.813469	768.517835	13.645031
16.964932	753.529081	13.650048
16.224909	739.917100	13.655066
16.373346	755.552954	13.660083
16.660387	753.377707	13.665101
16.568870	766.021574	13.670119
16.815050	763.518210	13.675136
16.813923	772.518718	13.680154
16.789853	764.156297	13.685171
16.852459	768.337337	13.690189
16.767016	762.423988	13.695207
16.795107	762.558353	13.700224
16.809288	762.095289	13.705242
16.712058	757.319887	13.710259
17.126265	762.348403	13.715277
16.832575	764.814847	13.720295
16.858315	757.473425	13.725312
17.152149	760.942887	13.730330
17.286318	754.689017	13.735347
17.242933	760.811715	13.740365
17.188101	759.914493	13.745383
17.088787	754.606084	13.750400
17.267604	756.490406	13.755418
17.311892	752.437608	13.760435
17.145770	757.241465	13.765453
17.007789	759.610928	13.770471
17.094201	751.862368	13.775488
16.928103	761.535662	13.780506
17.180004	759.343830	13.785523
17.212975	757.195767	13.790541
17.233781	762.500517	13.795559
17.202934	760.640165	13.800576
17.062324	763.354025	13.805594
16.987600	761.427964	13.810611
17.165661	758.414562	13.815629
17.435152	769.547033	13.820647
17.195363	762.499679	13.825664
17.182322	758.575782	13.830682
17.259651	761.088237	13.835699
17.065535	764.829813	13.840717
16.916156	763.499277	13.845735
17.067995	755.879320	13.850752
17.218178	768.236009	13.855770
16.969867	763.064552	13.860787
17.110169	770.824750	13.865805
17.319769	785.501143	13.870823
17.688035	781.561680	13.875840
17.513718	786.729750	13.880858
17.800768	791.377407	13.885875
17.967707	772.788563	13.890893
17.352584	772.398852	13.895911
17.603976	760.329356	13.900928
17.197405	754.371650	13.905946
17.230139	772.783840	13.910963
17.277186	774.537330	13.915981
17.329552	783.813487	13.920999
17.516095	780.716701	13.926016
17.506805	782.109787	13.931034
17.508244	782.557599	13.936051
17.652509	776.838631	13.941069
17.635881	785.642756	13.946087
17.811279	781.332722	13.951104
17.961934	779.926772	13.956122
17.648767	784.592729	13.961139
18.076480	782.272360	13.966157
17.741416	780.305036	13.971175
17.782844	778.338683	13.976192
17.851478	780.934555	13.981210
17.858574	776.051283	13.986227
17.582511	773.175303	13.991245
17.851838	786.561072	13.996263
17.775897	774.675398	14.001280
17.850239	779.103912	14.006298
17.630780	784.171756	14.011315
17.772895	780.829465	14.016333
17.522336	785.065886	14.021351
17.772968	779.857275	14.026368
17.955559	781.674737	14.031386
18.049887	780.104042	14.036403
17.982175	771.205653	14.041421
17.831495	783.372805	14.046439
18.134645	782.744543	14.051456
18.286922	783.010930	14.056474
17.898049	777.978257	14.061491
18.242898	776.642868	14.066509
18.052074	781.706225	14.071527
18.156426	777.180103	14.076544
18.093467	767.750791	14.081562
17.878950	774.045475	14.086579
18.022955	771.198355	14.091597
17.931910	785.035064	14.096615
17.941974	790.455116	14.101632
18.221258	795.678351	14.106650
17.912264	795.417402	14.111667
18.337716	789.499738	14.116685
18.298720	794.321557	14.121703
18.565148	788.933742	14.126720
18.179596	793.071395	14.131738
18.158926	793.932929	14.136755
18.389958	792.457580	14.141773
18.093993	802.889709	14.146791
18.246411	801.376183	14.151808
18.419785	793.210034	14.156826
18.057148	801.942147	14.161843
18.200963	805.031176	14.166861
18.165211	797.169192	14.171879
18.323666	792.344253	14.176896
18.198213	783.757864	14.181914
18.540892	793.174734	14.186931
18.610664	789.648114	14.191949
18.379799	798.296463	14.196967
18.751329	801.293008	14.201984
18.743395	794.206158	14.207002
18.523336	796.200318	14.212019
18.596362	794.711855	14.217037
18.018414	802.019709	14.222055
18.523607	801.362947	14.227072
18.927185	811.631827	14.232090
18.700855	806.936600	14.237107
18.617578	808.442267	14.242125
18.357384	814.210786	14.247143
18.497326	819.487419	14.252160
18.957372	816.180515	14.257178
18.784518	822.907349	14.262195
18.878793	821.443958	14.267213
18.943232	821.960796	14.272231
18.731001	825.604236	14.277248
19.139447	817.805191	14.282266
18.723346	821.284911	14.287283
18.830251	812.510623	14.292301
19.039054	808.700281	14.297319
18.921459	810.463792	14.302336
18.890172	800.082750	14.307354
18.865685	800.247444	14.312371
18.868628	803.241778	14.317389
19.206404	817.124935	14.322407
18.909296	813.602144	14.327424
18.982617	794.857530	14.332442
19.283212	792.291988	14.337459
18.888675	796.232231	14.342477
18.864766	800.155432	14.347495
19.090373	807.179595	14.352512
19.396502	805.512596	14.357530
19.197416	808.292431	14.362547
18.835726	800.172241	14.367565
19.001128	802.181748	14.372583
18.836478	818.355866	14.377600
19.079214	816.335878	14.382618
18.860173	819.071503	14.387635
19.308606	814.844914	14.392653
19.076452	816.667401	14.397671
18.831673	813.186904	14.402688
18.951678	808.980216	14.407706
18.449757	815.512451	14.412723
18.838177	824.259445	14.417741
19.288197	842.287587	14.422759
19.391241	839.525769	14.427776
19.849592	835.124050	14.432794
19.842492	839.830430	14.437811
19.570196	825.141543	14.442829
19.513487	823.083263	14.447847
19.212008	813.555598	14.452864
19.482038	804.812560	14.457882
19.101318	822.144012	14.462899
19.487293	822.323290	14.467917
19.918673	832.120763	14.472935
19.431477	822.230867	14.477952
19.736761	807.296863	14.482970
19.678502	817.953692	14.487987
19.424930	816.030399	14.493005
19.484230	806.739704	14.498023
19.295816	808.902478	14.503040
19.621481	817.094406	14.508058
19.885357	834.763538	14.513075
19.891463	825.878802	14.518093
19.566532	817.099587	14.523111
19.250620	817.634992	14.528128
19.706266	828.473243	14.533146
19.509672	841.439743	14.538163
19.587104	846.098166	14.543181
19.331937	841.811395	14.548199
19.656308	837.847239	14.553216
19.774207	835.076783	14.558234
19.717288	837.070634	14.563251
20.086159	831.502652	14.568269
19.901761	836.315705	14.573287
19.762951	842.690071	14.578304
20.024168	831.060806	14.583322
19.631601	837.683214	14.588339
19.996207	838.080438	14.593357
19.963973	829.593032	14.598375
19.730351	838.409092	14.603392
19.766913	829.936153	14.608410
19.581403	835.052342	14.613427
19.907860	847.217363	14.618445
20.195273	848.582902	14.623463
20.187886	865.827500	14.628480
20.283073	859.122104	14.633498
20.046925	862.093948	14.638515
20.436125	845.998037	14.643533
20.532889	838.276220	14.648551
20.438254	841.128058	14.653568
20.339875	828.390631	14.658586
20.541594	832.767642	14.663603
20.483261	830.750642	14.668621
20.232142	832.039609	14.673639
20.198311	838.924550	14.678656
20.207740	829.376566	14.683674
20.618271	834.935859	14.688691
20.449716	829.000796	14.693709
20.236200	829.444418	14.698727
20.319297	830.037229	14.703744
20.695607	825.619964	14.708762
20.299571	828.064582	14.713779
20.092159	836.598821	14.718797
20.208862	828.100703	14.723815
20.438510	825.552584	14.728832
20.633188	823.284501	14.733850
20.130552	832.732849	14.738867
20.189858	836.251695	14.743885
20.323387	831.067729	14.748903
20.503809	844.278121	14.753920
20.476285	852.225598	14.758938
20.776765	861.219921	14.763955
20.664428	859.517496	14.768973
20.967635	845.322253	14.773991
20.709774	839.581062	14.779008
20.880860	833.002641	14.784026
20.722462	837.309843	14.789043
20.530364	829.317705	14.794061
20.645749	826.235216	14.799079
20.380030	831.294542	14.804096
20.803258	848.212876	14.809114
20.831564	852.834816	14.814131
20.777978	857.775704	14.819149
21.132241	856.640809	14.824167
20.646160	858.831293	14.829184
21.152364	850.398372	14.834202
20.760506	854.101520	14.839219
20.893394	855.970959	14.844237
20.975801	847.260453	14.849255
20.890466	859.717223	14.854272
20.811927	849.394049	14.859290
20.762749	843.598070	14.864307
20.873618	859.375602	14.869325
21.085505	855.170287	14.874343
20.668741	859.325469	14.879360
21.023017	846.412964	14.884378
20.838873	862.470255	14.889395
20.709979	850.078425	14.894413
20.788990	851.151564	14.899431
20.274242	858.541057	14.904448
20.602088	872.204904	14.909466
21.041136	879.066265	14.914483
20.240960	879.955260	14.919501
20.860317	879.618284	14.924519
20.896888	890.572727	14.929536
21.667181	893.711940	14.934554
21.899141	898.295672	14.939571
21.489225	884.691819	14.944589
21.593953	875.785295	14.949607
21.531919	874.119169	14.954624
21.674637	869.577544	14.959642
21.863657	873.713555	14.964659
21.727893	885.957335	14.969677
21.864848	870.932886	14.974695
21.567183	870.436627	14.979712
21.921163	867.947918	14.984730
21.337150	855.100366	14.989747
21.471483	860.702942	14.994765
21.997541	860.857117	14.999783
21.358318	853.938581	15.004800
21.423325	848.834775	15.009818
21.556954	861.828446	15.014835
21.482259	875.867795	15.019853
21.863493	866.094277	15.024871
21.123779	871.054307	15.029888
21.567026	866.528714	15.034906
21.485913	866.907410	15.039923
21.496887	871.790850	15.044941
21.823884	863.010455	15.049959
21.658630	865.857582	15.054976
21.568449	877.109590	15.059994
21.500369	873.430981	15.065011
21.414395	872.207268	15.070029
21.608538	873.577955	15.075047
21.668093	878.734655	15.080064
21.737203	897.690392	15.085082
21.938381	891.400729	15.090099
22.382925	897.958274	15.095117
22.206678	889.884728	15.100135
21.677309	882.276774	15.105152
21.903976	893.173032	15.110170
22.438220	896.402879	15.115187
22.079822	888.736576	15.120205
22.296691	865.380792	15.125223
21.927598	876.114759	15.130240
22.071251	865.643153	15.135258
21.994309	873.705681	15.140275
21.928102	883.161416	15.145293
22.076222	877.858384	15.150311
22.116885	890.885578	15.155328
21.998859	888.808495	15.160346
22.374402	888.923136	15.165363
21.925671	895.254559	15.170381
22.135407	892.362406	15.175399
21.984791	889.223751	15.180416
22.230313	886.556370	15.185434
22.384876	883.966357	15.190451
22.463129	892.326474	15.195469
22.824740	884.837700	15.200487
22.308257	899.530118	15.205504
22.329541	895.332566	15.210522
22.711723	896.487598	15.215539
22.192456	890.039411	15.220557
22.388989	886.631768	15.225575
22.696971	895.157867	15.230592
22.478263	892.515882	15.235610
22.360874	897.924377	15.240627
22.470472	895.947331	15.245645
22.426740	898.702838	15.250663
22.489821	890.825328	15.255680
22.411309	887.924688	15.260698
22.540070	883.946988	15.265715
22.344538	894.571721	15.270733
22.541334	888.071303	15.275751
22.877307	892.755503	15.280768
22.557480	903.885717	15.285786
22.880785	904.204205	15.290803
22.695172	915.928789	15.295821
22.948392	907.481829	15.300839
22.801270	908.467325	15.305856
23.153209	908.355287	15.310874
23.209999	899.172235	15.315891
22.805469	886.757293	15.320909
22.666466	884.323731	15.325927
22.949203	890.133441	15.330944
23.131169	888.081940	15.335962
23.061796	881.433877	15.340979
22.746714	884.784171	15.345997
22.928364	894.690235	15.351015
22.925836	904.568355	15.356032
22.803245	908.841561	15.361050
22.917509	903.941463	15.366067
22.790429	912.706152	15.371085
23.277950	908.530223	15.376103
23.093384	909.187065	15.381120
23.244316	910.441446	15.386138
23.369904	907.467800	15.391155
23.061675	911.429260	15.396173
23.270646	900.240489	15.401191
23.280833	904.988359	15.406208
22.937328	914.541207	15.411226
23.155798	915.336876	15.416243
23.111261	907.094361	15.421261
23.289232	904.058859	15.426279
23.377262	908.466325	15.431296
23.100008	907.742802	15.436314
23.430395	910.991968	15.441331
23.430469	908.186312	15.446349
23.452275	902.944089	15.451367
23.603478	899.171156	15.456384
23.333559	907.708910	15.461402
23.686433	908.934808	15.466419
23.198574	910.393418	15.471437
23.605661	924.136409	15.476455
23.536206	925.983909	15.481472
23.551553	932.592933	15.486490
23.832778	922.626767	15.491507
23.772233	930.800363	15.496525
23.891639	921.815776	15.501543
23.702065	916.461498	15.506560
23.759354	931.281798	15.511578
23.888631	926.272043	15.516595
23.682501	908.729293	15.521613
23.895303	910.393709	15.526631
24.026095	903.209340	15.531648
23.618804	905.715693	15.536666
24.026173	906.074660	15.541683
23.723190	905.522428	15.546701
24.089345	912.240585	15.551719
23.826439	909.529782	15.556736
23.765272	930.273243	15.561754
23.846487	917.539172	15.566771
24.034725	925.168850	15.571789
23.985426	922.815903	15.576807
24.260605	924.943926	15.581824
23.918473	930.466539	15.586842
24.201815	932.934117	15.591859
24.078343	931.489054	15.596877
23.923347	926.852047	15.601895
24.143823	923.850907	15.606912
24.034517	929.545328	15.611930
24.030929	919.961464	15.616947
23.724306	933.529103	15.621965
24.271884	931.682250	15.626983
23.866634	925.831578	15.632000
23.841044	929.054470	15.637018
24.445684	936.164467	15.642035
24.279329	944.414608	15.647053
24.130419	956.878251	15.652071
24.421699	962.702426	15.657088
24.420734	970.737315	15.662106
24.650462	951.586172	15.667123
24.374710	949.562196	15.672141
24.335640	952.395878	15.677159
24.551891	962.119830	15.682176
24.430750	957.079872	15.687194
24.702621	947.875720	15.692211
24.641024	954.522055	15.697229
24.382318	947.253525	15.702247
24.627078	951.671160	15.707264
24.450497	959.433752	15.712282
24.660219	954.651230	15.717299
24.822528	956.232042	15.722317
24.772433	958.250084	15.727335
24.676751	947.806461	15.732352
24.825908	950.904146	15.737370
24.835039	945.585000	15.742387
24.829493	946.327405	15.747405
24.895653	943.618689	15.752423
24.716007	937.423391	15.757440
24.659846	953.924622	15.762458
24.667073	938.737401	15.767475
24.578948	933.906875	15.772493
24.555566	935.917573	15.777511
25.020987	956.079934	15.782528
24.996075	964.784459	15.787546
25.361566	966.210359	15.792563
25.134048	966.438423	15.797581
24.962289	966.051825	15.802599
25.028391	964.955760	15.807616
25.020285	970.391336	15.812634
24.900222	968.750072	15.817651
25.182519	961.131680	15.822669
25.202074	960.604652	15.827687
25.789690	959.464748	15.832704
25.470184	961.824808	15.837722
25.565498	957.006561	15.842739
25.174275	952.157246	15.847757
25.465111	939.854228	15.852775
25.097484	942.086123	15.857792
25.091533	950.049199	15.862810
25.152352	953.536273	15.867827
25.388578	956.008080	15.872845
25.386620	961.540522	15.877863
25.533329	960.561218	15.882880
25.649604	955.916416	15.887898
25.436702	958.111448	15.892915
25.437823	957.486320	15.897933
25.317790	954.929853	15.902951
25.627250	958.160216	15.907968
25.779381	960.225471	15.912986
25.831860	958.598200	15.918003
25.680702	954.187807	15.923021
25.829028	954.246528	15.928039
25.812011	944.383884	15.933056
25.636238	956.510903	15.938074
25.723303	951.738132	15.943091
26.081824	963.475324	15.948109
25.775945	963.579963	15.953127
25.869638	950.253768	15.958144
25.822404	962.575250	15.963162
25.631255	955.236170	15.968179
25.745611	955.928230	15.973197
25.557443	955.875569	15.978215
26.008619	953.248541	15.983232
25.748051	961.027448	15.988250
25.970309	960.449726	15.993267
26.062148	951.687197	15.998285
26.109532	958.111328	16.003303
25.941103	947.855831	16.008320
25.890068	957.094629	16.013338
25.766097	961.560572	16.018355
26.220047	974.968051	16.023373
26.323249	974.888673	16.028391
26.421169	975.330840	16.033408
26.374250	987.235716	16.038426
26.371315	981.047430	16.043443
26.414952	974.239612	16.048461
26.283168	968.901512	16.053479
26.054923	955.196556	16.058496
26.450458	975.603422	16.063514
26.408473	968.237810	16.068531
26.539532	980.395667	16.073549
26.212730	983.028278	16.078567
26.395682	981.361627	16.083584
26.525560	975.796332	16.088602
26.216467	984.892536	16.093619
26.231747	974.112770	16.098637
26.473837	979.174627	16.103655
26.507211	968.960084	16.108672
26.274365	974.285704	16.113690
26.390988	971.297672	16.118707
26.236535	973.477236	16.123725
26.575973	989.834466	16.128743
26.852263	989.746905	16.133760
26.728856	1000.562375	16.138778
27.063987	1001.387108	16.143795
27.005637	985.938716	16.148813
26.755683	978.040784	16.153831
26.579062	976.263211	16.158848
26.714951	990.727256	16.163866
26.892742	996.607095	16.168883
27.042315	996.097565	16.173901
26.937430	1001.065466	16.178919
27.137320	992.020895	16.183936
26.898527	995.564388	16.188954
27.351095	993.577777	16.193971
27.382226	987.422023	16.198989
26.794394	984.313983	16.204007
27.318184	983.051532	16.209024
27.105487	972.436876	16.214042
26.983166	966.762771	16.219059
26.826328	975.633141	16.224077
27.183881	989.311359	16.229095
27.227204	989.541170	16.234112
27.162883	992.445088	16.239130
27.072308	989.947117	16.244147
27.820154	994.440578	16.249165
27.568699	990.825390	16.254183
27.665516	990.270476	16.259200
27.340322	999.725824	16.264218
27.321782	989.917043	16.269235
27.671661	992.020747	16.274253
27.293139	995.734458	16.279271
27.313843	987.996091	16.284288
27.180022	986.088732	16.289306
27.434884	995.525781	16.294323
27.623499	986.167393	16.299341
27.475965	995.446577	16.304359
27.593859	994.405513	16.309376
27.620832	986.950193	16.314394
27.503768	991.916843	16.319411
28.105948	984.740638	16.324429
27.718874	997.222688	16.329447
27.689070	994.983444	16.334464
27.780488	990.266787	16.339482
27.492861	993.395044	16.344499
27.730631	985.518524	16.349517
27.583408	989.047669	16.354535
27.618593	990.383309	16.359552
27.928096	1002.295468	16.364570
27.974680	1007.971801	16.369587
28.256964	1003.805915	16.374605
28.455059	1007.116854	16.379623
28.024446	983.805556	16.384640
27.956324	987.473788	16.389658
27.642199	987.611278	16.394675
28.241821	992.815941	16.399693
28.248605	1006.508104	16.404711
27.957091	1016.125445	16.409728
28.067044	1020.283346	16.414746
28.257407	1020.038830	16.419763
28.303721	1014.073195	16.424781
28.223566	1023.430202	16.429799
28.753186	1006.882947	16.434816
28.415600	1017.186019	16.439834
28.294480	1019.578121	16.444851
28.789504	1022.220833	16.449869
28.411652	1015.403297	16.454887
28.574163	1022.355378	16.459904
28.712196	1010.312943	16.464922
28.541485	997.564637	16.469939
28.489820	989.045485	16.474957
28.248613	997.411522	16.479975
28.606228	1001.783085	16.484992
28.651785	1013.357902	16.490010
28.558473	1012.488787	16.495027
28.508078	1014.677299	16.500045
28.394867	1020.268217	16.505063
28.634974	1015.200045	16.510080
28.505803	1017.025352	16.515098
28.373955	1018.437658	16.520115
28.568858	1016.377804	16.525133
28.310747	1023.935443	16.530151
28.566249	1018.205281	16.535168
28.681447	1027.686320	16.540186
28.390626	1029.079353	16.545203
28.597558	1037.151128	16.550221
28.400014	1034.051359	16.555239
28.231068	1025.253913	16.560256
28.353586	1040.821494	16.565274
28.500721	1052.456162	16.570291
28.752721	1053.944033	16.575309
28.741995	1063.978165	16.580327
29.167210	1057.088439	16.585344
29.780533	1059.049887	16.590362
29.337193	1056.058055	16.595379
29.355096	1056.058315	16.600397
29.223440	1051.742674	16.605415
29.453884	1055.957446	16.610432
29.445767	1046.885476	16.615450
29.258106	1044.102901	16.620467
29.611458	1054.439754	16.625485
29.444659	1047.327200	16.630503
29.754822	1049.165728	16.635520
29.616715	1046.425883	16.640538
29.289599	1057.367980	16.645555
29.756000	1048.240599	16.650573
29.653960	1052.217122	16.655591
29.469197	1056.033034	16.660608
29.854349	1049.354721	16.665626
29.531839	1055.571747	16.670643
29.832311	1047.944159	16.675661
29.617507	1052.648423	16.680679
29.555474	1041.786052	16.685696
29.861826	1038.853491	16.690714
29.500454	1044.369686	16.695731
29.402652	1040.512658	16.700749
29.431421	1036.730476	16.705767
29.512617	1040.280647	16.710784
29.830968	1044.973961	16.715802
29.702062	1052.252586	16.720819
29.788069	1049.600705	16.725837
29.626695	1068.819959	16.730855
29.866413	1072.225377	16.735872
29.864587	1076.852096	16.740890
30.147819	1075.286493	16.745907
30.260681	1069.139996	16.750925
30.118814	1072.636758	16.755943
30.062930	1068.921483	16.760960
30.323518	1064.563318	16.765978
30.391306	1068.005140	16.770995
30.321852	1067.283766	16.776013
30.399015	1071.206970	16.781031
30.565083	1069.767025	16.786048
30.633462	1071.387811	16.791066
30.305212	1073.695606	16.796083
30.897066	1061.332717	16.801101
30.393488	1055.942387	16.806119
30.141005	1047.751323	16.811136
30.231852	1043.754281	16.816154
30.192362	1067.082324	16.821171
30.659960	1067.747447	16.826189
30.254923	1065.500712	16.831207
30.221957	1063.173590	16.836224
30.239476	1053.258136	16.841242
30.093624	1064.298073	16.846259
30.377429	1053.252119	16.851277
30.475428	1066.361979	16.856295
30.663089	1086.271354	16.861312
31.162215	1076.447691	16.866330
30.646135	1083.667067	16.871347
31.298359	1076.855379	16.876365
30.568506	1073.772731	16.881383
30.235926	1065.723599	16.886400
30.787364	1078.633033	16.891418
30.700539	1079.104149	16.896435
30.791707	1083.223981	16.901453
30.923866	1089.770580	16.906471
30.524181	1088.144712	16.911488
31.174582	1086.903443	16.916506
30.970313	1087.418207	16.921523
31.077955	1082.736854	16.926541
31.172586	1091.899249	16.931559
31.074154	1089.086907	16.936576
31.509219	1086.654893	16.941594
31.571774	1092.442363	16.946611
31.213230	1084.820179	16.951629
31.609863	1087.238470	16.956647
31.103640	1084.998118	16.961664
31.414948	1083.055721	16.966682
31.434051	1085.571033	16.971699
31.476221	1087.681933	16.976717
31.485865	1082.832893	16.981735
31.334621	1082.430454	16.986752
31.671377	1068.485405	16.991770
31.207548	1076.974724	16.996787
31.516485	1068.020330	17.001805
31.511470	1073.685833	17.006823
31.729253	1077.798450	17.011840
31.991252	1070.195815	17.016858
31.382406	1068.056753	17.021875
31.542018	1077.821201	17.026893
31.842731	1081.684135	17.031911
31.779212	1087.469264	17.036928
32.048133	1086.107879	17.041946
31.799634	1074.646683	17.046963
31.614887	1069.023353	17.051981
31.832999	1092.352095	17.056999
31.728506	1092.472520	17.062016
32.217527	1095.172990	17.067034
31.967402	1098.715122	17.072051
31.974382	1099.193633	17.077069
32.245233	1106.368620	17.082087
32.109677	1106.642239	17.087104
32.024899	1108.574211	17.092122
32.253950	1097.631485	17.097139
32.288133	1102.255725	17.102157
32.125787	1092.216948	17.107175
32.271620	1104.965882	17.112192
32.173225	1101.222545	17.117210
31.976997	1095.695682	17.122227
32.322052	1098.917339	17.127245
32.498721	1090.810499	17.132263
32.308770	1101.361895	17.137280
32.054069	1093.543552	17.142298
32.119044	1090.005001	17.147315
32.344238	1105.796399	17.152333
32.717890	1099.691084	17.157351
31.863222	1100.695926	17.162368
32.078812	1111.120670	17.167386
32.322081	1120.890970	17.172403
32.529818	1116.465332	17.177421
32.686205	1119.432522	17.182439
32.556559	1126.263157	17.187456
32.841587	1123.677916	17.192474
32.790005	1114.347627	17.197491
32.662052	1121.212709	17.202509
33.298188	1117.742459	17.207527
33.071946	1108.348017	17.212544
33.009829	1112.608641	17.217562
32.619698	1116.655564	17.222579
32.931326	1120.488393	17.227597
33.269611	1110.541585	17.232615
33.206207	1117.589062	17.237632
33.289698	1108.218678	17.242650
32.958634	1107.812854	17.247667
33.136546	1105.982876	17.252685
33.412719	1118.114935	17.257703
32.949041	1116.464376	17.262720
33.368984	1106.889796	17.267738
33.096501	1106.424299	17.272755
33.373218	1112.768371	17.277773
33.234339	1107.077881	17.282791
33.062761	1112.296109	17.287808
33.154228	1117.318487	17.292826
33.055747	1121.225039	17.297843
33.096518	1122.288407	17.302861
33.240852	1123.720568	17.307879
33.592855	1128.437035	17.312896
33.638200	1123.557142	17.317914
33.553079	1134.294110	17.322931
33.441849	1136.132396	17.327949
33.898785	1124.585889	17.332967
33.597785	1137.559494	17.337984
33.824857	1123.742043	17.343002
33.698918	1132.345710	17.348019
33.631874	1138.339697	17.353037
33.823102	1121.419310	17.358055
33.623196	1132.218442	17.363072
33.923475	1128.409480	17.368090
33.925249	1130.324738	17.373107
33.821817	1134.730700	17.378125
33.822306	1125.966619	17.383143
33.519649	1131.997519	17.388160
33.777496	1119.667987	17.393178
33.828318	1140.163766	17.398195
33.768959	1151.089217	17.403213
34.221442	1154.221467	17.408231
34.287447	1160.377657	17.413248
34.147832	1151.458785	17.418266
34.214231	1152.338253	17.423283
34.350864	1151.224815	17.428301
34.566118	1152.923586	17.433319
34.891391	1148.492148	17.438336
34.685445	1143.162458	17.443354
34.541756	1149.228419	17.448371
34.040028	1134.777200	17.453389
34.734916	1136.258806	17.458407
34.744363	1147.403854	17.463424
34.509989	1139.096298	17.468442
35.004005	1142.080024	17.473459
34.584551	1134.457894	17.478477
34.568081	1123.285370	17.483495
34.598743	1130.037239	17.488512
34.646944	1136.328758	17.493530
34.673253	1136.400287	17.498547
34.570574	1138.230922	17.503565
34.641712	1143.950790	17.508583
34.570916	1151.037309	17.513600
34.594252	1147.653597	17.518618
35.183620	1147.554854	17.523635
35.064505	1154.475370	17.528653
34.802587	1136.934824	17.533671
34.790628	1154.991483	17.538688
35.108071	1152.757775	17.543706
34.813091	1145.352831	17.548723
34.789703	1148.442870	17.553741
35.188854	1140.926017	17.558759
35.019200	1141.012470	17.563776
34.812774	1143.481072	17.568794
34.905318	1156.393031	17.573811
34.796606	1176.699246	17.578829
35.199611	1171.520299	17.583847
35.209392	1175.372030	17.588864
35.310114	1171.928850	17.593882
35.349976	1167.545281	17.598899
35.527723	1166.905097	17.603917
35.679784	1162.929997	17.608935
35.509004	1170.180516	17.613952
35.112845	1172.382194	17.618970
35.461879	1163.168998	17.623987
35.276525	1171.573704	17.629005
35.671598	1164.735998	17.634023
35.352153	1173.351068	17.639040
35.731260	1182.203843	17.644058
36.105803	1186.938885	17.649075
35.848735	1185.338002	17.654093
35.715924	1181.827265	17.659111
36.002159	1193.077303	17.664128
35.971555	1188.802602	17.669146
36.177011	1185.100006	17.674163
35.996864	1192.064814	17.679181
36.067145	1182.617564	17.684199
35.852491	1182.521712	17.689216
36.038804	1178.639075	17.694234
36.224339	1189.349449	17.699251
35.828681	1193.750715	17.704269
36.317420	1186.352355	17.709287
36.048074	1195.202590	17.714304
35.898081	1185.881371	17.719322
36.075527	1177.294673	17.724339
36.077050	1194.030093	17.729357
36.068318	1183.194000	17.734375
36.083723	1191.611444	17.739392
36.513810	1195.952765	17.744410
36.572928	1207.124783	17.749427
36.501584	1210.389610	17.754445
36.578045	1203.115799	17.759463
36.337544	1206.631198	17.764480
37.023033	1205.987202	17.769498
37.047717	1204.821870	17.774515
36.507364	1193.453663	17.779533
37.005197	1184.539045	17.784551
36.558692	1185.066517	17.789568
36.819708	1186.066978	17.794586
36.953339	1198.653785	17.799603
36.625823	1194.769595	17.804621
36.840459	1205.191388	17.809639
36.733393	1202.970535	17.814656
37.238995	1209.932054	17.819674
37.225331	1204.900434	17.824691
37.174482	1202.648681	17.829709
36.910177	1200.348319	17.834727
36.838816	1207.494911	17.839744
36.845129	1203.750927	17.844762
36.982331	1196.802129	17.849779
37.190831	1200.048355	17.854797
37.256396	1208.154981	17.859815
37.506174	1200.219679	17.864832
36.988653	1207.294159	17.869850
36.960984	1202.277357	17.874867
37.119773	1199.380514	17.879885
37.076120	1203.253246	17.884903
37.354866	1214.952610	17.889920
37.144405	1227.410305	17.894938
37.823018	1223.428434	17.899955
37.615265	1227.904414	17.904973
37.450686	1223.817959	17.909991
37.574992	1231.549306	17.915008
37.484723	1223.301187	17.920026
37.965589	1218.835886	17.925043
37.927155	1222.313316	17.930061
38.073558	1226.238329	17.935079
37.921950	1222.708439	17.940096
37.834478	1218.909715	17.945114
38.160317	1211.861926	17.950131
37.497461	1221.752159	17.955149
37.492491	1216.428830	17.960167
37.838764	1225.567647	17.965184
37.411506	1230.122201	17.970202
37.735511	1227.167909	17.975219
37.864125	1242.737867	17.980237
38.195501	1251.755951	17.985255
38.012776	1239.937192	17.990272
38.637582	1238.008780	17.995290
38.623284	1234.886577	18.000307
38.149918	1243.396404	18.005325
38.563685	1234.655884	18.010343
38.783339	1240.172626	18.015360
38.416141	1247.264596	18.020378
38.599569	1238.260351	18.025395
38.632888	1233.928286	18.030413
38.518321	1235.382084	18.035431
38.526618	1236.220166	18.040448
38.504686	1242.380695	18.045466
38.897898	1237.354747	18.050483
39.104577	1247.026704	18.055501
38.759677	1236.019179	18.060519
38.794061	1239.816575	18.065536
38.565320	1230.062686	18.070554
38.920216	1229.012880	18.075571
39.169352	1232.410541	18.080589
38.835120	1230.840679	18.085607
38.947875	1234.748874	18.090624
38.814514	1241.949377	18.095642
39.317350	1230.521846	18.100659
39.046157	1232.372582	18.105677
38.951091	1236.067178	18.110695
39.265315	1229.601889	18.115712
38.899473	1237.826614	18.120730
39.101767	1235.538351	18.125747
38.871316	1234.974744	18.130765
39.122119	1226.064094	18.135783
38.809094	1230.802729	18.140800
38.533085	1239.723460	18.145818
39.374304	1256.302130	18.150835
39.356865	1257.964783	18.155853
39.758657	1256.939186	18.160871
39.726228	1260.800704	18.165888
39.267408	1257.309472	18.170906
39.326158	1257.464284	18.175923
39.577946	1262.183863	18.180941
39.441886	1261.958929	18.185959
39.614553	1249.901438	18.190976
39.712163	1259.527373	18.195994
39.715862	1249.471959	18.201011
39.756948	1261.663040	18.206029
39.883381	1267.920258	18.211047
40.007020	1261.601587	18.216064
39.934712	1271.923204	18.221082
40.078564	1265.781252	18.226099
40.078616	1264.944835	18.231117
39.870006	1275.616025	18.236135
40.095765	1283.031687	18.241152
40.197488	1285.284765	18.246170
40.118421	1278.136281	18.251187
40.255665	1278.373473	18.256205
39.927273	1281.574440	18.261223
40.405929	1277.267268	18.266240
40.240854	1272.458174	18.271258
40.116753	1266.266682	18.276275
40.081829	1280.672515	18.281293
40.401712	1281.057823	18.286311
40.462200	1274.745886	18.291328
40.572945	1283.104252	18.296346
40.179448	1270.769365	18.301363
40.074454	1274.446589	18.306381
39.921798	1295.873864	18.311399
40.578302	1288.474424	18.316416
40.710825	1302.213388	18.321434
40.955335	1302.474801	18.326451
40.915090	1293.758047	18.331469
40.921546	1293.577057	18.336487
40.971144	1297.078580	18.341504
40.703765	1307.752685	18.346522
41.280902	1293.902348	18.351539
41.083929	1302.668710	18.356557
40.933986	1292.810920	18.361575
41.350828	1287.976924	18.366592
41.164989	1300.973630	18.371610
41.376784	1291.014982	18.376627
41.657191	1287.224880	18.381645
41.352292	1281.686582	18.386663
41.474397	1294.893823	18.391680
41.549645	1287.269861	18.396698
41.371205	1291.880124	18.401715
41.747083	1290.120100	18.406733
41.406299	1289.037271	18.411751
41.358081	1279.384465	18.416768
41.456304	1293.554845	18.421786
41.520635	1289.814376	18.426803
41.510780	1295.329224	18.431821
41.565668	1297.012107	18.436839
41.976329	1287.659799	18.441856
41.810403	1288.184341	18.446874
41.844250	1287.500424	18.451891
41.769330	1292.144963	18.456909
41.722166	1289.359271	18.461927
41.848712	1281.717807	18.466944
41.780644	1286.762072	18.471962
41.975915	1286.987017	18.476979
41.897864	1289.558606	18.481997
42.038790	1299.316636	18.487015
41.859379	1299.884317	18.492032
41.857642	1302.838442	18.497050
42.055945	1307.683183	18.502067
42.416158	1310.971935	18.507085
41.946225	1310.887675	18.512103
41.936213	1306.029030	18.517120
41.996954	1316.522339	18.522138
41.784625	1302.786218	18.527155
41.902567	1314.062700	18.532173
41.945993	1333.969702	18.537191
42.183846	1339.212214	18.542208
42.211725	1330.162864	18.547226
42.480698	1330.865430	18.552243
42.417871	1331.837741	18.557261
42.438092	1360.329378	18.562279
42.979069	1350.852475	18.567296
42.873412	1345.595377	18.572314
42.878436	1360.029731	18.577331
43.289202	1353.038011	18.582349
43.174318	1345.503776	18.587367
43.047142	1329.216926	18.592384
42.845192	1328.273294	18.597402
42.739825	1333.547488	18.602419
43.140140	1334.207384	18.607437
42.966485	1345.911440	18.612455
43.324203	1348.209627	18.617472
43.374361	1350.379270	18.622490
43.224017	1357.134338	18.627507
43.324571	1350.188066	18.632525
43.385798	1355.010113	18.637543
43.370743	1344.850283	18.642560
43.461462	1355.439907	18.647578
43.541093	1354.439533	18.652595
43.271013	1352.982690	18.657613
43.218703	1365.191631	18.662631
43.531686	1347.545024	18.667648
43.334982	1357.049859	18.672666
43.458690	1351.239250	18.677683
43.644012	1347.858525	18.682701
43.588195	1352.976632	18.687719
43.649006	1342.814384	18.692736
43.697093	1348.698881	18.697754
43.294557	1349.727573	18.702771
43.783453	1361.501409	18.707789
43.687587	1371.706850	18.712807
43.705801	1385.406980	18.717824
43.883115	1378.167793	18.722842
43.521164	1378.593656	18.727859
44.174348	1372.943091	18.732877
44.008981	1380.252809	18.737895
44.022624	1390.485286	18.742912
44.435095	1397.612955	18.747930
44.115681	1396.520459	18.752947
44.273835	1390.417251	18.757965
44.488449	1399.188605	18.762983
44.606214	1393.511464	18.768000
44.929205	1387.268817	18.773018
44.598239	1384.915756	18.778035
44.970269	1377.614501	18.783053
44.486870	1378.163538	18.788071
44.692041	1384.238039	18.793088
44.967336	1385.340421	18.798106
44.787752	1383.257145	18.803123
44.840410	1382.990017	18.808141
44.681228	1387.758240	18.813159
45.112179	1375.451906	18.818176
45.281227	1389.876365	18.823194
44.578849	1391.570601	18.828211
45.084281	1378.185889	18.833229
44.987088	1385.702688	18.838247
45.103007	1387.565374	18.843264
44.895875	1390.141422	18.848282
44.926508	1390.329044	18.853299
44.887862	1383.758034	18.858317
44.944244	1377.967433	18.863335
45.209604	1385.689371	18.868352
45.453618	1383.962622	18.873370
45.191996	1381.185270	18.878387
45.360468	1388.426907	18.883405
45.155556	1410.070797	18.888423
45.428389	1412.038295	18.893440
45.192250	1413.432257	18.898458
45.239069	1412.664248	18.903475
45.231418	1413.555332	18.908493
45.424554	1420.408093	18.913511
45.395592	1419.683517	18.918528
45.742016	1421.286020	18.923546
46.123675	1430.207950	18.928563
46.059229	1423.303281	18.933581
45.741441	1432.842907	18.938599
46.031068	1435.631478	18.943616
46.176885	1433.049068	18.948634
45.962098	1429.349146	18.953651
46.135859	1433.708595	18.958669
46.433813	1431.809282	18.963687
46.496727	1431.761462	18.968704
46.226942	1426.716256	18.973722
46.381344	1434.319895	18.978739
46.286280	1436.720593	18.983757
45.934041	1433.099013	18.988775
46.183539	1429.379999	18.993792
46.669665	1434.315385	18.998810
46.371176	1430.899988	19.003827
46.358169	1425.833487	19.008845
46.467487	1432.778284	19.013863
46.530492	1428.703463	19.018880
46.699151	1426.171127	19.023898
46.574438	1432.306798	19.028915
46.626954	1428.905838	19.033933
46.524938	1436.663265	19.038951
46.582113	1437.408488	19.043968
46.853013	1445.811268	19.048986
46.611504	1447.682622	19.054003
46.814853	1450.995977	19.059021
46.796648	1446.921252	19.064039
47.042630	1445.108979	19.069056
47.430278	1443.766838	19.074074
46.876683	1450.061233	19.079091
47.311853	1444.287006	19.084109
46.944520	1440.289075	19.089127
46.992157	1460.965610	19.094144
47.525054	1460.623239	19.099162
47.339505	1466.402362	19.104179
47.198151	1465.001084	19.109197
47.557982	1467.791285	19.114215
47.642420	1462.308700	19.119232
47.602238	1467.995618	19.124250
47.450496	1478.181470	19.129267
47.607056	1458.602570	19.134285
47.491486	1462.480314	19.139303
47.591167	1474.596086	19.144320
48.063749	1477.987189	19.149338
47.433756	1498.163993	19.154355
47.859515	1479.584359	19.159373
47.757176	1492.047389	19.164391
48.079412	1495.231667	19.169408
48.417720	1486.360830	19.174426
48.081836	1487.420114	19.179443
47.611396	1486.398613	19.184461
47.770288	1484.382220	19.189479
48.141325	1485.277095	19.194496
48.518152	1489.128193	19.199514
48.123651	1509.542681	19.204531
48.109654	1518.422499	19.209549
48.796104	1513.378936	19.214567
49.081210	1504.702627	19.219584
48.826046	1503.104572	19.224602
48.664648	1506.954790	19.229619
48.810087	1498.720109	19.234637
48.430503	1502.550859	19.239655
48.926794	1503.621780	19.244672
48.920817	1502.660058	19.249690
49.116628	1513.359549	19.254707
48.852192	1490.984119	19.259725
49.186680	1493.175507	19.264743
49.051743	1487.487433	19.269760
48.860484	1474.978701	19.274778
49.027889	1489.062654	19.279795
49.208409	1489.526609	19.284813
49.362671	1497.840387	19.289831
49.085688	1498.634810	19.294848
49.478052	1498.983520	19.299866
49.036764	1495.426373	19.304883
49.344152	1494.759554	19.309901
49.433384	1499.138575	19.314919
49.329995	1500.663231	19.319936
49.640514	1493.519897	19.324954
49.435419	1500.561320	19.329971
49.457180	1496.698084	19.334989
49.538677	1500.731162	19.340007
49.549988	1509.859487	19.345024
49.409694	1498.428404	19.350042
49.369504	1505.627038	19.355059
49.648712	1517.083519	19.360077
49.769467	1528.299733	19.365095
49.781479	1541.795817	19.370112
50.097675	1532.704348	19.375130
49.919769	1537.939471	19.380147
49.952421	1528.747255	19.385165
50.211171	1529.189486	19.390183
50.061855	1534.517964	19.395200
50.322307	1530.487928	19.400218
49.740724	1532.901747	19.405235
49.955897	1547.833528	19.410253
50.180600	1546.914561	19.415271
50.423203	1557.423702	19.420288
50.625038	1556.079105	19.425306
50.522961	1550.490010	19.430323
50.327888	1544.751376	19.435341
50.756689	1549.380180	19.440359
50.648166	1549.204578	19.445376
51.018922	1539.132520	19.450394
50.499021	1537.642215	19.455411
50.899536	1536.440070	19.460429
51.058617	1538.539019	19.465447
50.840013	1544.812520	19.470464
50.990874	1538.988129	19.475482
51.146585	1541.630433	19.480499
51.164634	1547.967849	19.485517
51.124320	1541.523280	19.490535
50.798582	1559.894611	19.495552
51.418851	1566.055625	19.500570
51.357065	1574.131874	19.505587
51.351499	1568.502404	19.510605
51.431782	1562.357687	19.515623
51.611333	1569.465111	19.520640
51.638473	1566.383697	19.525658
51.323253	1571.409958	19.530675
51.503639	1576.421691	19.535693
51.584462	1566.631741	19.540711
51.214471	1575.412720	19.545728
51.560919	1565.019391	19.550746
51.446893	1568.795925	19.555763
52.126871	1587.618815	19.560781
52.258998	1593.405014	19.565799
51.727616	1587.087864	19.570816
51.662330	1586.561486	19.575834
51.775750	1588.942164	19.580851
51.981790	1589.875520	19.585869
52.300096	1598.797993	19.590887
52.101435	1589.973364	19.595904
52.243017	1594.801822	19.600922
52.023341	1593.599007	19.605939
52.160899	1594.934433	19.610957
52.569965	1588.820250	19.615975
52.354691	1591.422849	19.620992
52.377625	1585.640578	19.626010
52.067222	1589.791885	19.631027
52.119843	1612.686464	19.636045
52.748140	1611.776848	19.641063
52.748433	1620.073778	19.646080
52.928265	1617.646968	19.651098
52.991142	1618.959380	19.656115
52.851507	1610.478962	19.661133
52.884806	1611.322612	19.666151
52.752543	1618.658800	19.671168
52.970757	1607.641719	19.676186
52.929668	1605.738699	19.681203
53.178837	1604.620226	19.686221
53.544578	1602.451484	19.691239
53.157561	1614.930799	19.696256
53.215524	1609.616428	19.701274
53.155044	1613.154196	19.706291
53.163176	1610.047349	19.711309
53.268752	1617.646091	19.716327
53.346529	1632.116605	19.721344
53.593833	1628.959659	19.726362
53.291028	1626.674741	19.731379
53.458496	1631.451814	19.736397
53.516133	1633.626631	19.741415
53.243344	1633.928070	19.746432
53.821083	1640.323005	19.751450
53.820025	1647.048479	19.756467
53.898833	1647.916560	19.761485
54.185002	1648.455491	19.766503
54.201678	1646.641253	19.771520
54.221466	1646.723273	19.776538
54.042769	1647.975701	19.781555
54.265713	1650.582239	19.786573
54.448443	1644.071128	19.791591
54.406670	1647.381897	19.796608
54.200985	1649.181382	19.801626
54.190239	1649.852044	19.806643
54.126000	1650.221800	19.811661
54.531049	1645.310656	19.816679
54.564243	1643.585354	19.821696
54.324916	1650.692163	19.826714
54.658638	1651.870620	19.831731
54.661742	1653.905653	19.836749
54.976378	1660.985637	19.841767
54.490076	1671.990921	19.846784
54.691474	1684.138238	19.851802
55.021872	1666.961987	19.856819
54.699049	1673.718949	19.861837
55.209282	1661.898644	19.866855
54.853568	1663.270331	19.871872
54.883775	1667.519778	19.876890
55.101523	1671.118113	19.881907
54.925745	1670.378657	19.886925
55.258858	1680.684330	19.891943
55.241519	1681.930416	19.896960
55.441864	1686.140586	19.901978
55.716439	1688.287734	19.906995
55.613392	1688.906582	19.912013
55.901583	1684.338804	19.917031
55.916053	1685.441043	19.922048
55.847174	1675.854379	19.927066
55.697750	1676.262730	19.932083
55.688167	1684.649604	19.937101
55.849750	1679.189583	19.942119
55.872029	1679.204937	19.947136
55.857838	1678.216089	19.952154
55.782692	1680.736783	19.957171
55.477566	1686.291701	19.962189
55.600575	1681.468921	19.967207
55.585624	1703.155990	19.972224
56.002009	1711.911666	19.977242
56.306594	1708.537436	19.982259
56.122138	1712.968857	19.987277
56.466099	1708.849955	19.992295
56.452323	1707.886288	19.997312
56.513557	1706.929805	20.002330
56.381075	1706.792671	20.007347
56.517584	1711.514652	20.012365
56.592099	1716.268439	20.017383
56.872408	1729.391250	20.022400
56.543499	1730.575695	20.027418
56.954273	1725.979233	20.032435
56.868615	1731.143151	20.037453
56.986819	1729.732745	20.042471
56.895767	1739.274881	20.047488
57.046031	1737.218783	20.052506
57.078057	1732.059928	20.057523
56.918622	1732.611869	20.062541
57.163906	1726.450711	20.067559
57.167295	1732.190850	20.072576
57.531552	1729.157583	20.077594
57.536710	1718.536753	20.082611
57.397459	1732.788872	20.087629
57.603410	1748.233538	20.092647
57.347520	1755.330359	20.097664
57.325161	1758.066870	20.102682
57.894909	1750.333676	20.107699
57.829510	1752.168000	20.112717
58.002957	1751.405386	20.117735
57.598025	1752.892095	20.122752
57.925213	1753.901159	20.127770
57.939190	1745.301929	20.132787
57.913011	1744.352828	20.137805
58.038085	1741.170828	20.142823
58.236072	1749.462092	20.147840
57.987600	1748.560442	20.152858
58.191988	1757.728075	20.157875
58.315332	1767.839432	20.162893
58.347663	1771.261697	20.167911
58.512777	1776.695628	20.172928
58.446983	1774.187352	20.177946
58.542950	1765.319631	20.182963
58.694269	1770.774657	20.187981
58.669325	1766.284322	20.192999
58.273637	1770.651017	20.198016
58.619581	1778.818121	20.203034
58.870735	1784.001872	20.208051
58.687001	1781.000801	20.213069
58.516581	1788.986862	20.218087
58.934042	1797.953865	20.223104
59.091341	1795.508469	20.228122
59.199951	1783.154524	20.233139
59.001883	1792.792355	20.238157
59.270341	1789.871923	20.243175
59.002924	1795.013841	20.248192
58.940700	1799.899534	20.253210
59.040474	1802.866241	20.258227
58.952681	1813.581942	20.263245
59.157741	1823.970881	20.268263
59.163846	1815.514872	20.273280
59.239147	1823.828548	20.278298
59.481335	1830.919951	20.283315
59.891026	1830.211845	20.288333
59.932240	1845.575100	20.293351
60.601961	1842.017397	20.298368
60.374361	1838.262588	20.303386
60.108217	1812.857246	20.308403
60.358765	1813.060913	20.313421
60.090741	1803.385454	20.318439
59.734388	1809.008399	20.323456
59.992194	1820.553641	20.328474
60.568478	1823.275270	20.333491
60.570351	1839.099150	20.338509
60.483018	1842.909431	20.343527
60.380815	1838.630012	20.348544
60.359274	1843.364167	20.353562
60.678880	1818.296263	20.358579
60.853526	1836.728344	20.363597
60.663349	1831.007787	20.368615
60.660041	1836.676420	20.373632
60.443937	1833.225944	20.378650
60.820774	1831.762385	20.383667
60.471822	1834.976139	20.388685
60.605497	1840.244589	20.393703
60.942805	1848.592971	20.398720
61.015914	1862.360611	20.403738
61.191212	1849.781562	20.408755
61.257921	1864.809458	20.413773
60.998849	1862.445068	20.418791
61.248090	1856.715622	20.423808
61.554583	1861.297394	20.428826
61.771536	1855.175348	20.433843
61.685789	1861.368180	20.438861
61.743906	1854.895453	20.443879
61.854489	1858.687353	20.448896
61.743383	1867.724580	20.453914
62.036433	1860.511250	20.458931
61.841796	1876.744673	20.463949
61.911086	1878.488476	20.468967
62.060925	1881.564125	20.473984
62.173060	1883.963981	20.479002
62.356662	1877.007650	20.484019
62.066632	1877.782041	20.489037
62.184088	1880.865920	20.494055
62.366042	1879.555975	20.499072
62.081808	1870.021885	20.504090
62.346696	1878.738258	20.509107
61.913184	1881.583389	20.514125
62.116774	1871.411096	20.519143
62.150818	1887.438275	20.524160
62.479830	1898.918759	20.529178
62.615256	1898.550287	20.534195
62.689690	1902.616123	20.539213
62.659541	1899.559408	20.544231
62.778837	1893.408465	20.549248
63.099438	1904.830306	20.554266
63.198837	1909.832728	20.559283
63.020214	1919.896801	20.564301
63.189707	1925.557324	20.569319
63.375409	1924.234166	20.574336
63.422423	1929.282673	20.579354
63.128017	1926.409378	20.584371
63.427376	1926.671676	20.589389
63.306838	1922.511883	20.594407
63.788206	1924.229001	20.599424
63.753128	1924.830896	20.604442
63.591033	1919.364705	20.609459
63.699645	1911.498549	20.614477
63.576582	1909.611497	20.619495
63.457914	1909.191310	20.624512
63.519844	1921.382731	20.629530
64.027209	1925.604821	20.634547
63.930696	1939.436968	20.639565
64.150658	1950.382263	20.644583
63.833094	1932.057489	20.649600
63.625925	1939.582281	20.654618
64.235309	1939.388879	20.659635
64.401531	1939.624696	20.664653
64.072067	1942.320981	20.669671
64.494848	1945.372815	20.674688
64.560784	1950.194285	20.679706
64.709436	1952.443251	20.684723
64.574837	1947.124234	20.689741
64.527074	1953.219622	20.694759
64.983878	1944.866521	20.699776
65.239881	1944.646427	20.704794
65.018653	1949.509732	20.709811
65.431460	1958.837333	20.714829
64.920762	1952.538903	20.719847
65.228825	1948.864260	20.724864
65.192287	1955.592253	20.729882
65.129289	1948.983822	20.734899
65.152841	1956.289424	20.739917
65.053775	1952.997326	20.744935
65.002877	1945.913595	20.749952
64.960464	1958.193978	20.754970
65.330787	1966.998025	20.759987
65.485473	1970.644173	20.765005
65.473925	1973.558917	20.770023
65.777155	1975.275545	20.775040
65.554142	1982.638724	20.780058
65.613952	1978.980878	20.785075
66.183984	1989.110744	20.790093
66.194372	1993.035145	20.795111
65.744954	1997.539709	20.800128
66.242143	2005.241375	20.805146
66.200273	1993.567319	20.810163
66.271711	1998.498402	20.815181
66.091327	1996.904365	20.820199
66.268510	1991.678509	20.825216
66.058968	1999.670793	20.830234
66.250286	2002.935640	20.835251
66.533376	2012.021640	20.840269
66.586738	2021.901089	20.845287
66.633560	2022.206111	20.850304
66.724756	2021.604707	20.855322
66.580992	2014.522874	20.860339
66.989852	2015.080467	20.865357
66.905621	2023.365577	20.870375
67.400118	2006.964930	20.875392
67.143166	2015.731568	20.880410
67.161027	2019.670584	20.885427
67.264673	2034.351981	20.890445
67.332439	2039.577164	20.895463
67.720828	2044.316579	20.900480
67.779342	2041.757230	20.905498
67.650453	2037.835422	20.910515
67.845644	2035.283065	20.915533
67.747692	2040.875065	20.920551
67.983593	2035.980849	20.925568
67.844842	2048.579369	20.930586
67.913836	2040.233331	20.935603
67.798297	2039.534918	20.940621
67.511735	2042.120347	20.945639
67.849182	2037.819339	20.950656
67.818814	2035.412783	20.955674
67.895491	2044.616352	20.960691
67.761447	2041.601139	20.965709
68.120285	2056.075302	20.970727
68.081003	2051.833315	20.975744
68.107016	2056.780999	20.980762
68.195273	2059.067846	20.985779
68.343599	2067.531153	20.990797
68.261932	2080.092346	20.995815
68.792968	2087.012354	21.000832
68.811682	2085.185128	21.005850
68.737728	2090.441997	21.010867
68.974364	2091.133882	21.015885
68.962928	2096.387270	21.020903
68.880536	2084.110384	21.025920
68.909024	2086.245639	21.030938
69.124705	2089.093240	21.035955
69.304942	2097.643088	21.040973
69.253498	2104.259854	21.045991
69.181517	2112.836600	21.051008
69.641862	2114.096245	21.056026
69.459095	2114.055355	21.061043
69.738296	2108.273794	21.066061
69.513228	2103.281355	21.071079
69.806010	2096.626596	21.076096
69.857140	2106.269737	21.081114
70.125144	2106.852558	21.086131
70.203003	2101.724289	21.091149
69.972552	2104.717535	21.096167
70.108492	2097.560286	21.101184
70.130076	2110.297844	21.106202
70.406242	2117.428223	21.111219
70.423711	2121.083276	21.116237
70.003100	2128.439600	21.121255
70.519882	2125.193007	21.126272
70.232934	2130.464322	21.131290
70.627211	2127.931257	21.136307
70.716193	2116.372331	21.141325
70.654625	2124.215244	21.146343
70.886544	2120.025433	21.151360
70.268326	2126.974023	21.156378
70.432553	2141.254664	21.161395
70.903262	2145.731880	21.166413
70.689595	2158.329589	21.171431
70.795092	2156.914829	21.176448
71.208322	2158.156610	21.181466
71.185417	2172.027900	21.186483
71.577927	2171.748544	21.191501
71.378419	2180.392644	21.196519
71.547683	2175.840219	21.201536
71.649194	2165.727938	21.206554
71.602912	2176.339513	21.211571
71.901474	2168.389831	21.216589
71.656699	2170.103966	21.221607
71.739924	2179.252925	21.226624
72.087857	2171.093518	21.231642
71.852679	2171.139742	21.236659
72.168925	2165.655342	21.241677
72.074016	2174.775399	21.246695
72.126660	2186.734906	21.251712
72.082376	2198.693826	21.256730
72.175859	2195.447263	21.261747
72.531357	2191.610491	21.266765
72.398705	2192.218214	21.271783
72.546700	2191.519535	21.276800
72.520549	2186.019340	21.281818
72.697993	2187.979778	21.286835
72.478544	2192.258995	21.291853
72.591271	2196.265244	21.296871
72.507474	2208.807925	21.301888
73.139052	2216.649588	21.306906
73.120822	2215.399388	21.311923
73.216450	2221.544991	21.316941
73.105901	2222.187124	21.321959
73.060934	2208.152663	21.326976
73.410319	2214.195385	21.331994
73.361389	2214.925703	21.337011
73.348017	2212.295534	21.342029
73.472049	2226.607789	21.347047
73.495895	2237.173696	21.352064
73.688702	2242.606585	21.357082
73.889493	2247.889889	21.362099
74.199241	2246.215883	21.367117
73.886376	2239.832702	21.372135
73.692454	2240.932907	21.377152
74.409109	2242.991924	21.382170
73.960216	2239.568373	21.387187
73.874307	2228.333448	21.392205
74.062614	2241.057602	21.397223
74.155368	2250.173544	21.402240
74.497140	2255.627284	21.407258
74.555067	2271.344924	21.412275
74.762044	2258.697504	21.417293
74.544589	2254.710623	21.422311
74.469027	2252.920243	21.427328
74.997949	2252.348090	21.432346
74.579938	2264.744339	21.437363
75.150885	2260.274140	21.442381
75.009885	2265.390072	21.447399
74.983139	2271.340251	21.452416
75.488559	2279.728775	21.457434
75.022979	2287.231076	21.462451
75.443847	2278.984448	21.467469
75.313322	2291.364078	21.472487
75.293314	2290.675936	21.477504
75.663007	2284.324668	21.482522
75.441090	2289.046149	21.487539
75.317647	2280.635466	21.492557
75.446380	2290.676840	21.497575
75.954790	2297.578382	21.502592
75.896946	2294.548032	21.507610
75.849222	2305.690133	21.512627
76.033910	2307.273873	21.517645
76.157891	2303.097775	21.522663
75.926380	2301.357072	21.527680
76.280784	2308.484738	21.532698
76.267383	2326.858413	21.537715
76.394582	2322.445099	21.542733
76.676284	2323.650689	21.547751
76.713030	2321.883736	21.552768
76.339988	2317.861251	21.557786
76.658553	2316.302633	21.562803
76.555222	2324.947514	21.567821
76.731016	2331.711816	21.572839
76.901298	2336.886306	21.577856
76.986704	2345.312261	21.582874
77.335852	2345.216439	21.587891
77.327622	2341.919506	21.592909
77.319327	2350.723096	21.597927
77.499526	2340.554203	21.602944
77.437392	2339.263531	21.607962
77.704970	2347.559950	21.612979
77.841783	2343.798438	21.617997
77.692789	2349.508995	21.623015
77.568991	2345.652600	21.628032
77.861057	2339.386066	21.633050
77.550679	2351.099572	21.638067
77.716252	2359.497193	21.643085
77.786249	2370.526207	21.648103
77.550263	2365.548030	21.653120
78.080856	2365.284911	21.658138
78.140646	2373.645458	21.663155
78.481721	2383.072891	21.668173
78.652491	2389.200466	21.673191
78.502317	2391.925537	21.678208
78.789645	2383.810247	21.683226
78.691100	2384.592531	21.688243
78.501411	2383.416524	21.693261
78.895875	2382.893839	21.698279
78.451242	2382.897131	21.703296
78.941048	2382.776115	21.708314
78.481301	2379.878152	21.713331
78.951928	2396.740034	21.718349
79.276241	2407.634544	21.723367
78.979419	2407.406374	21.728384
79.247934	2402.292335	21.733402
78.870625	2410.639321	21.738419
79.498634	2419.463186	21.743437
79.622277	2423.234223	21.748455
79.967322	2433.065044	21.753472
79.888647	2429.586609	21.758490
80.069076	2436.703709	21.763507
80.255571	2431.261651	21.768525
80.157590	2428.777263	21.773543
79.994479	2435.572607	21.778560
80.540931	2432.460182	21.783578
80.265650	2433.393246	21.788595
80.346598	2422.094185	21.793613
80.619052	2427.060171	21.798631
80.135818	2426.668683	21.803648
80.700625	2422.328809	21.808666
80.465991	2423.829918	21.813683
80.354049	2435.588136	21.818701
80.330490	2438.154508	21.823719
80.523525	2449.129576	21.828736
80.850411	2445.265673	21.833754
80.511159	2451.662544	21.838771
80.917688	2464.636718	21.843789
81.124030	2472.725017	21.848807
81.142986	2472.340064	21.853824
81.448340	2466.869905	21.858842
81.383985	2476.430341	21.863859
81.498060	2473.477178	21.868877
81.502028	2468.013207	21.873895
81.670232	2479.490853	21.878912
81.546410	2494.274543	21.883930
81.657524	2496.172816	21.888947
81.914702	2490.441926	21.893965
82.182002	2481.565946	21.898983
82.101518	2497.094008	21.904000
82.155522	2497.363196	21.909018
82.005055	2500.883674	21.914035
82.414009	2504.954047	21.919053
82.593752	2504.045234	21.924071
82.700750	2517.811223	21.929088
82.834880	2521.558545	21.934106
82.804919	2517.905186	21.939123
82.599446	2515.585965	21.944141
82.473200	2515.978077	21.949159
82.566065	2518.040175	21.954176
82.801779	2512.489384	21.959194
82.868454	2530.806536	21.964211
82.824335	2540.079784	21.969229
83.084015	2542.172559	21.974247
83.004937	2550.400294	21.979264
83.507932	2529.696020	21.984282
83.439550	2534.270420	21.989299
83.394856	2529.732491	21.994317
83.683365	2533.376725	21.999335
83.444611	2558.499053	22.004352
83.652810	2555.613189	22.009370
83.952397	2550.781449	22.014387
83.484662	2559.559282	22.019405
84.441413	2560.513945	22.024423
83.816107	2560.387736	22.029440
83.943394	2561.365044	22.034458
84.271710	2565.126138	22.039475
84.501493	2582.770779	22.044493
84.278261	2580.482738	22.049511
84.480735	2581.138965	22.054528
84.689877	2589.832858	22.059546
84.691712	2590.132314	22.064563
84.728561	2590.940736	22.069581
85.013295	2583.971445	22.074599
84.645680	2594.068659	22.079616
84.932036	2599.458595	22.084634
84.941593	2606.757185	22.089651
85.073670	2614.188079	22.094669
85.481410	2613.858989	22.099687
85.321415	2610.352230	22.104704
85.580530	2607.597252	22.109722
85.519271	2613.527701	22.114739
85.691789	2609.760540	22.119757
85.839161	2619.092199	22.124775
85.678862	2629.444163	22.129792
85.852850	2627.011822	22.134810
86.329910	2629.550286	22.139827
86.300631	2632.868747	22.144845
86.324009	2618.510798	22.149863
86.328029	2636.670598	22.154880
86.544456	2632.722964	22.159898
86.621964	2622.112359	22.164915
86.271872	2622.807817	22.169933
86.704693	2621.272303	22.174951
86.234522	2631.060521	22.179968
86.592488	2633.242062	22.184986
86.770279	2640.946703	22.190003
86.797756	2639.979679	22.195021
87.005252	2647.269367	22.200039
87.012583	2647.050353	22.205056
87.135663	2651.102424	22.210074
86.912530	2648.823827	22.215091
87.064180	2669.908384	22.220109
87.340993	2673.444014	22.225127
87.275820	2674.590353	22.230144
87.389005	2675.775028	22.235162
87.525946	2674.977066	22.240179
87.804460	2687.722121	22.245197
88.070227	2685.562605	22.250215
87.935379	2695.456130	22.255232
88.055024	2687.783590	22.260250
88.292454	2688.219725	22.265267
87.840621	2695.738978	22.270285
88.412279	2694.844502	22.275303
87.898776	2698.090498	22.280320
88.181231	2715.354590	22.285338
88.239170	2714.382789	22.290355
88.263336	2721.107870	22.295373
88.835066	2727.551483	22.300391
88.520623	2737.526824	22.305408
88.469994	2733.740943	22.310426
88.829646	2735.764424	22.315443
89.178079	2732.439947	22.320461
89.272937	2739.071898	22.325479
89.252854	2736.395361	22.330496
88.891023	2736.833856	22.335514
89.346209	2746.584470	22.340531
89.378576	2751.013737	22.345549
89.600594	2750.855771	22.350567
89.785731	2750.927672	22.355584
89.664237	2753.563087	22.360602
89.725174	2756.428727	22.365619
89.652087	2755.875131	22.370637
89.966479	2768.693528	22.375655
90.216595	2773.473739	22.380672
90.008149	2771.312760	22.385690
90.527170	2782.079150	22.390707
90.060089	2778.828777	22.395725
90.416378	2768.774083	22.400743
90.252862	2785.341161	22.405760
90.655275	2802.100489	22.410778
90.850955	2803.319590	22.415795
91.400442	2805.316494	22.420813
91.297128	2797.025507	22.425831
91.558176	2800.254326	22.430848
91.206246	2802.897445	22.435866
91.917460	2797.590845	22.440883
91.133988	2799.310532	22.445901
91.650622	2801.817572	22.450919
91.514860	2796.006119	22.455936
91.512412	2795.037463	22.460954
91.402953	2791.983553	22.465971
91.644017	2805.896036	22.470989
91.776757	2813.077569	22.476007
91.912827	2814.028266	22.481024
91.953521	2821.685027	22.486042
92.449459	2817.494722	22.491059
92.356592	2816.739070	22.496077
92.653964	2812.090667	22.501095
92.675811	2817.253834	22.506112
92.520513	2808.617493	22.511130
92.478297	2813.651823	22.516147
92.375612	2830.821713	22.521165
92.561707	2836.678764	22.526183
92.710446	2843.501153	22.531200
92.513625	2845.873794	22.536218
92.785278	2844.139423	22.541235
92.804776	2867.896119	22.546253
92.931297	2868.494821	22.551271
93.202504	2870.219711	22.556288
93.134340	2878.840410	22.561306
93.429176	2881.404305	22.566323
93.429619	2889.190492	22.571341
93.618263	2887.387061	22.576359
93.650280	2893.372425	22.581376
93.758896	2893.229069	22.586394
94.111809	2895.285186	22.591411
94.054263	2909.604340	22.596429
94.202610	2908.447930	22.601447
94.379752	2907.204947	22.606464
94.581982	2915.852738	22.611482
94.846854	2906.310971	22.616499
94.800290	2912.987237	22.621517
95.062349	2908.644181	22.626535
95.256169	2901.408109	22.631552
95.285691	2905.332867	22.636570
95.369438	2904.480105	22.641587
94.954967	2916.118755	22.646605
94.828936	2903.024376	22.651623
95.140426	2905.633008	22.656640
95.052788	2911.731811	22.661658
94.915217	2902.265722	22.666675
94.942765	2917.830876	22.671693
95.251696	2928.122120	22.676711
95.434816	2926.682515	22.681728
95.512029	2939.752815	22.686746
95.819736	2946.294684	22.691763
95.902098	2958.688761	22.696781
96.165285	2966.629503	22.701799
95.917626	2960.153786	22.706816
96.013106	2958.068260	22.711834
96.046206	2961.462226	22.716851
96.074508	2975.521797	22.721869
96.530146	2983.975265	22.726887
96.251114	2983.384490	22.731904
96.379818	2992.018587	22.736922
96.544376	2988.157908	22.741939
96.687347	2997.332642	22.746957
96.747941	3000.034252	22.751975
97.314899	3002.394563	22.756992
96.881929	2999.934172	22.762010
97.506597	3008.506356	22.767027
97.224606	3011.264796	22.772045
97.679427	3015.586911	22.777063
97.615380	3020.675219	22.782080
97.389590	3021.761526	22.787098
97.833805	3026.347272	22.792115
97.796497	3022.205746	22.797133
97.934710	3021.656911	22.802151
98.160017	3025.415304	22.807168
98.036887	3043.282968	22.812186
98.247092	3037.057425	22.817203
98.290023	3044.518244	22.822221
98.537955	3039.580843	22.827239
98.618145	3036.654990	22.832256
98.464866	3037.862499	22.837274
98.681013	3047.543415	22.842291
98.925053	3063.431431	22.847309
98.689203	3070.525627	22.852327
99.095930	3066.724834	22.857344
98.869099	3076.090107	22.862362
99.066420	3067.417334	22.867379
99.215398	3078.046192	22.872397
99.564196	3087.498036	22.877415
99.938411	3085.450888	22.882432
99.654272	3084.589474	22.887450
100.095620	3084.229863	22.892467
99.646464	3097.240713	22.897485
99.926048	3090.354096	22.902503
99.925792	3086.285657	22.907520
99.860282	3104.772445	22.912538
99.857005	3103.753402	22.917555
100.546768	3111.911438	22.922573
100.460632	3104.526616	22.927591
100.405199	3106.706702	22.932608
100.461043	3115.920397	22.937626
100.617499	3127.842171	22.942643
101.076540	3137.207333	22.947661
101.408699	3137.189921	22.952679
101.184080	3134.002495	22.957696
101.289711	3132.783326	22.962714
101.357781	3131.011387	22.967731
101.305466	3135.504515	22.972749
101.461704	3131.405235	22.977767
101.629045	3126.903373	22.982784
101.682971	3132.898009	22.987802
101.635770	3139.350365	22.992819
101.955361	3148.437537	22.997837
102.013902	3153.326770	23.002855
101.652406	3154.541658	23.007872
101.836907	3163.391189	23.012890
101.742107	3148.962958	23.017907
101.981387	3168.178496	23.022925
102.010366	3182.168685	23.027943
102.304010	3177.738554	23.032960
102.193112	3188.667005	23.037978
102.216963	3202.437075	23.042995
102.614855	3203.924368	23.048013
102.311406	3208.538922	23.053031
102.796921	3205.581103	23.058048
102.990956	3219.949463	23.063066
103.324294	3231.262842	23.068083
103.380368	3231.465435	23.073101
103.096927	3228.770116	23.078119
103.564969	3231.048112	23.083136
103.462411	3242.609697	23.088154
103.890899	3259.011865	23.093171
103.954209	3258.424258	23.098189
103.981544	3257.318348	23.103207
104.231218	3245.705117	23.108224
104.200906	3238.472463	23.113242
104.614836	3245.086175	23.118259
104.645081	3247.139230	23.123277
104.414935	3242.598613	23.128295
104.819142	3261.605349	23.133312
104.968981	3264.965301	23.138330
104.984706	3274.895523	23.143347
105.173273	3275.620237	23.148365
105.057801	3271.535088	23.153383
105.234646	3265.560882	23.158400
105.078030	3270.228198	23.163418
105.282408	3264.981933	23.168435
105.189168	3275.008132	23.173453
105.200071	3291.589379	23.178471
105.368007	3288.469831	23.183488
105.457457	3301.446944	23.188506
105.848877	3289.382225	23.193523
106.061238	3304.300128	23.198541
105.960904	3316.328540	23.203559
105.853005	3318.046586	23.208576
106.111472	3319.634640	23.213594
106.215445	3307.201471	23.218611
106.518430	3327.070016	23.223629
106.421454	3354.614198	23.228647
106.753224	3342.779728	23.233664
107.098559	3350.420548	23.238682
106.800372	3350.697582	23.243699
106.984573	3343.270309	23.248717
106.983348	3350.545639	23.253735
107.388498	3353.995016	23.258752
107.378537	3358.434220	23.263770
107.510292	3357.775918	23.268787
107.775277	3355.098815	23.273805
107.301092	3368.962821	23.278823
107.614911	3362.250646	23.283840
107.856562	3369.472152	23.288858
107.973255	3386.112661	23.293875
107.859908	3386.111391	23.298893
107.964696	3388.509444	23.303911
108.103608	3383.371246	23.308928
108.191379	3389.019785	23.313946
108.113104	3397.118372	23.318963
108.501519	3404.114895	23.323981
108.561079	3413.381817	23.328999
108.918425	3410.690236	23.334016
108.850365	3413.535159	23.339034
108.975556	3423.227372	23.344051
109.080093	3423.775880	23.349069
108.949745	3432.977875	23.354087
109.044638	3433.575239	23.359104
109.305582	3434.282308	23.364122
109.825063	3452.788273	23.369139
109.963234	3452.555063	23.374157
109.792294	3464.484164	23.379175
110.400023	3450.368572	23.384192
109.952960	3455.725325	23.389210
110.153483	3454.781647	23.394227
110.453087	3452.992340	23.399245
110.387647	3453.374945	23.404263
110.601242	3448.947821	23.409280
110.301344	3459.050688	23.414298
110.224470	3459.425615	23.419315
110.501080	3471.559202	23.424333
110.378057	3481.501806	23.429351
110.555510	3477.743161	23.434368
110.903436	3496.036168	23.439386
111.361884	3500.866000	23.444403
111.442649	3498.296646	23.449421
111.492604	3507.962815	23.454439
111.213879	3504.790112	23.459456
111.745707	3520.844916	23.464474
111.846214	3522.830181	23.469491
111.919476	3522.654484	23.474509
111.744629	3532.131788	23.479527
111.769437	3520.903961	23.484544
112.169617	3537.522291	23.489562
112.295741	3545.781456	23.494579
112.591072	3552.331799	23.499597
112.595075	3555.351677	23.504615
112.429667	3552.148587	23.509632
112.429830	3557.075483	23.514650
112.398098	3569.781393	23.519667
112.900842	3568.973427	23.524685
112.822830	3583.810801	23.529703
113.134249	3595.812766	23.534720
113.237950	3603.169605	23.539738
113.440408	3603.491304	23.544755
113.748323	3595.782570	23.549773
113.587102	3611.781905	23.554791
113.781524	3618.771029	23.559808
113.756454	3614.516978	23.564826
113.821900	3625.272873	23.569843
114.108874	3627.377283	23.574861
114.125773	3628.334069	23.579879
114.297606	3637.103753	23.584896
114.479985	3656.208786	23.589914
114.512592	3659.741839	23.594931
114.969825	3655.689974	23.599949
114.884883	3655.737911	23.604967
114.896498	3646.096554	23.609984
114.902781	3656.527165	23.615002
115.369279	3673.068947	23.620019
115.038548	3681.756416	23.625037
115.083403	3680.246879	23.630055
115.251776	3684.181617	23.635072
115.512374	3685.169665	23.640090
115.889781	3708.868238	23.645107
115.776899	3701.301137	23.650125
116.140725	3707.480982	23.655143
116.033034	3703.855342	23.660160
116.284350	3699.892542	23.665178
116.295692	3699.991678	23.670195
116.430300	3708.391624	23.675213
116.219375	3718.398630	23.680231
116.594758	3720.706988	23.685248
116.714060	3716.749086	23.690266
116.978077	3720.523655	23.695283
117.123461	3722.123149	23.700301
116.964620	3725.660958	23.705319
117.166425	3739.697098	23.710336
117.429293	3732.730793	23.715354
117.203075	3744.031156	23.720371
117.567492	3735.353981	23.725389
117.535648	3743.578014	23.730407
117.271238	3742.328400	23.735424
117.852233	3756.289364	23.740442
117.876086	3763.008570	23.745459
117.679452	3760.678332	23.750477
117.907410	3783.765990	23.755495
118.154956	3784.784496	23.760512
118.334155	3790.589281	23.765530
118.210366	3793.929074	23.770547
118.295240	3802.387357	23.775565
118.668975	3819.972780	23.780583
118.694693	3817.402537	23.785600
118.883511	3828.770497	23.790618
119.019105	3842.469889	23.795635
119.504889	3830.509970	23.800653
119.604646	3839.562492	23.805671
119.448176	3846.477266	23.810688
119.731692	3845.896175	23.815706
119.909911	3855.801257	23.820723
119.897704	3858.744816	23.825741
119.989227	3861.817318	23.830759
120.137947	3857.605423	23.835776
120.324331	3860.161199	23.840794
120.561061	3880.463687	23.845811
120.553758	3878.087990	23.850829
120.352665	3882.532016	23.855847
120.814423	3887.844359	23.860864
120.998715	3875.129925	23.865882
120.807399	3894.868215	23.870899
121.009541	3897.121672	23.875917
120.879122	3915.000807	23.880935
121.064816	3918.509926	23.885952
121.340673	3917.216691	23.890970
121.259002	3933.592082	23.895987
121.648800	3925.905100	23.901005
121.682202	3945.380980	23.906023
121.464176	3956.538154	23.911040
121.912364	3955.003282	23.916058
122.224464	3960.970371	23.921075
122.186526	3963.422425	23.926093
122.375811	3983.912376	23.931111
122.574930	3987.940211	23.936128
122.920200	3983.369229	23.941146
122.663494	3977.386960	23.946163
123.048290	3987.404945	23.951181
123.167487	4007.183089	23.956199
123.042499	4010.775621	23.961216
123.612824	4005.920019	23.966234
123.441138	4010.122739	23.971251
123.440818	4013.878811	23.976269
123.590847	4017.314628	23.981287
123.570805	4026.307102	23.986304
124.236728	4019.466926	23.991322
124.386012	4028.243489	23.996339
124.421201	4028.326265	24.001357
124.574204	4032.872672	24.006375
124.634392	4030.205462	24.011392
124.761937	4021.956654	24.016410
124.501822	4026.848701	24.021427
124.766551	4050.814730	24.026445
125.121426	4043.717106	24.031463
125.052504	4048.276190	24.036480
125.497756	4054.339236	24.041498
125.400778	4058.994254	24.046515
125.166452	4051.430251	24.051533
125.201457	4060.218421	24.056551
125.361155	4074.466584	24.061568
125.817604	4071.178602	24.066586
125.502453	4085.015080	24.071603
125.531600	4088.201553	24.076621
125.578718	4097.350831	24.081639
125.741524	4107.949720	24.086656
125.879918	4109.004285	24.091674
126.089469	4133.010632	24.096691
126.431341	4136.318567	24.101709
126.577033	4140.525253	24.106727
126.587258	4155.901644	24.111744
127.115892	4152.990580	24.116762
127.273722	4150.238613	24.121779
127.167824	4159.904296	24.126797
127.431968	4163.454833	24.131815
127.240596	4180.939756	24.136832
127.426454	4173.442443	24.141850
127.933925	4175.449245	24.146867
128.026053	4189.506073	24.151885
127.973535	4195.675559	24.156903
128.050424	4199.375384	24.161920
128.114636	4197.856460	24.166938
128.117071	4201.018730	24.171955
128.530314	4216.597173	24.176973
129.104833	4218.779706	24.181991
129.082851	4224.594054	24.187008
129.338218	4220.475843	24.192026
129.069017	4226.849734	24.197043
129.362401	4219.174578	24.202061
129.395938	4233.467883	24.207079
129.066226	4246.053658	24.212096
129.466121	4237.661079	24.217114
129.654067	4248.442342	24.222131
129.745487	4250.448049	24.227149
130.086755	4262.032287	24.232167
129.891176	4277.235855	24.237184
129.857386	4270.962893	24.242202
130.090760	4274.912827	24.247219
130.403058	4288.209256	24.252237
130.961291	4289.621021	24.257255
130.793855	4299.422677	24.262272
131.242813	4292.543793	24.267290
131.101463	4297.849739	24.272307
130.989117	4305.654206	24.277325
131.489336	4305.720944	24.282343
131.566829	4314.628838	24.287360
131.461022	4320.472132	24.292378
131.285236	4321.957861	24.297395
131.454652	4335.595511	24.302413
131.893768	4338.780930	24.307431
131.816798	4345.746568	24.312448
132.283814	4342.308530	24.317466
132.391712	4364.172094	24.322483
132.189125	4363.667143	24.327501
132.513096	4373.508641	24.332519
132.398660	4385.277984	24.337536
132.793797	4384.704641	24.342554
132.934032	4403.040574	24.347571
132.886526	4387.638068	24.352589
133.189543	4386.151158	24.357607
133.261146	4396.152151	24.362624
133.420934	4401.682405	24.367642
133.707867	4411.412936	24.372659
133.886698	4424.610430	24.377677
134.029369	4418.407622	24.382695
133.933754	4424.602876	24.387712
134.197590	4425.580990	24.392730
134.193997	4449.138208	24.397747
134.090413	4448.608276	24.402765
134.349194	4437.674656	24.407783
134.788541	4453.028261	24.412800
134.954927	4457.979863	24.417818
135.188294	4462.169732	24.422835
134.779275	4465.939424	24.427853
135.431501	4465.404714	24.432871
135.169620	4470.805348	24.437888
135.456989	4468.979983	24.442906
135.324101	4480.019976	24.447923
135.528119	4483.469518	24.452941
135.768841	4490.271807	24.457959
135.710320	4509.939456	24.462976
135.879446	4503.637780	24.467994
136.050447	4503.210025	24.473011
135.949066	4532.694765	24.478029
136.396401	4533.363210	24.483047
136.727172	4538.598417	24.488064
136.819896	4542.280049	24.493082
137.273527	4551.738334	24.498099
136.822856	4559.693764	24.503117
137.277307	4549.767909	24.508135
137.333602	4559.171657	24.513152
137.577462	4564.619347	24.518170
137.899109	4582.548261	24.523187
137.989438	4583.749269	24.528205
137.971415	4583.142798	24.533223
137.575554	4597.787746	24.538240
138.092695	4600.392818	24.543258
138.292507	4613.116843	24.548275
138.418929	4614.189096	24.553293
138.693635	4621.020831	24.558311
138.705066	4630.352732	24.563328
138.810269	4635.377098	24.568346
139.072112	4639.925545	24.573363
139.152534	4642.128723	24.578381
139.637202	4649.180095	24.583399
139.591617	4668.631247	24.588416
139.620458	4664.737815	24.593434
139.821847	4655.495477	24.598451
139.676728	4662.768625	24.603469
139.952558	4679.972503	24.608487
140.156637	4683.952369	24.613504
140.333547	4677.273788	24.618522
140.451530	4679.830928	24.623539
140.570384	4705.020151	24.628557
140.725217	4703.367040	24.633575
140.941957	4713.459104	24.638592
140.835905	4712.298246	24.643610
141.193826	4729.959632	24.648627
141.289385	4726.693353	24.653645
141.598629	4729.457275	24.658663
141.531254	4730.695627	24.663680
141.721118	4735.741479	24.668698
141.918624	4754.583308	24.673715
142.007259	4767.088119	24.678733
142.075483	4765.678998	24.683751
142.255538	4766.184152	24.688768
142.396661	4783.188274	24.693786
142.858273	4785.480107	24.698803
142.594396	4796.777552	24.703821
143.130805	4792.946619	24.708839
143.047303	4788.805613	24.713856
142.942083	4785.551839	24.718874
143.090180	4797.801147	24.723891
143.097154	4816.262539	24.728909
143.517371	4808.551484	24.733927
143.342578	4810.807291	24.738944
143.200634	4824.339418	24.743962
143.666339	4826.788442	24.748979
143.677660	4838.478401	24.753997
144.100891	4848.904350	24.759015
144.359599	4864.870564	24.764032
144.503112	4864.481831	24.769050
144.687637	4859.686448	24.774067
144.572713	4879.899945	24.779085
145.084955	4884.431322	24.784103
145.203566	4890.870949	24.789120
145.120697	4892.304288	24.794138
145.062671	4902.638367	24.799155
145.407978	4914.967337	24.804173
145.740100	4906.199970	24.809191
145.743608	4923.039546	24.814208
145.755293	4932.292648	24.819226
145.946104	4937.164797	24.824243
146.201784	4947.004680	24.829261
146.392221	4951.769569	24.834279
146.731692	4960.595702	24.839296
146.383839	4966.211971	24.844314
146.625448	4962.714435	24.849331
146.759528	4979.271613	24.854349
147.049797	4976.596628	24.859367
147.329472	4994.472550	24.864384
147.374991	4995.286035	24.869402
147.678769	5007.504781	24.874419
147.811244	5014.229528	24.879437
147.763248	5011.130890	24.884455
148.021774	5032.176203	24.889472
148.085599	5041.493793	24.894490
148.167158	5045.278286	24.899507
148.160187	5056.134758	24.904525
148.534920	5065.646709	24.909543
148.606288	5073.135473	24.914560
148.523464	5071.910978	24.919578
149.197839	5086.615922	24.924595
149.243978	5098.590999	24.929613
149.442392	5090.188560	24.934631
149.361950	5097.028765	24.939648
149.602088	5113.159093	24.944666
150.202977	5116.612870	24.949683
150.005859	5127.584401	24.954701
150.134126	5124.982124	24.959719
150.128333	5133.268993	24.964736
150.461737	5148.254680	24.969754
150.663682	5144.125692	24.974771
150.504854	5158.058442	24.979789
150.924205	5160.666291	24.984807
151.159210	5167.393971	24.989824
150.893471	5174.266391	24.994842
151.629139	5174.599284	24.999859
151.354576	5183.723746	25.004877
151.653880	5197.420609	25.009895
151.746170	5200.916203	25.014912
151.776246	5202.682255	25.019930
152.017807	5208.487195	25.024947
151.746306	5214.909138	25.029965
152.035024	5224.333636	25.034983
152.380096	5229.033337	25.040000
152.473450	5248.576978	25.045018
152.974531	5240.404835	25.050035
152.946527	5244.361208	25.055053
153.464960	5252.805906	25.060071
153.355490	5264.028944	25.065088
153.535614	5269.976106	25.070106
153.656726	5270.995568	25.075123
153.589107	5280.838931	25.080141
153.816133	5270.389595	25.085159
154.072155	5291.328275	25.090176
153.760090	5298.043855	25.095194
154.475582	5300.261258	25.100211
154.164961	5307.295434	25.105229
154.511666	5315.366174	25.110247
154.395922	5317.322383	25.115264
154.761804	5325.958315	25.120282
154.999677	5322.682261	25.125299
155.015693	5343.589155	25.130317
155.420186	5331.884053	25.135335
155.508571	5351.103450	25.140352
155.544362	5357.691953	25.145370
156.107542	5365.612006	25.150387
155.813843	5367.662389	25.155405
156.115914	5375.411858	25.160423
156.528257	5386.928862	25.165440
156.213988	5395.264176	25.170458
156.544350	5400.105118	25.175475
156.761373	5413.944457	25.180493
156.918338	5407.199289	25.185511
157.240443	5421.928128	25.190528
156.970196	5423.687588	25.195546
157.036099	5438.904821	25.200563
157.434838	5442.137800	25.205581
158.062042	5461.866349	25.210599
158.080020	5460.888037	25.215616
157.908457	5460.933764	25.220634
158.233823	5464.225591	25.225651
158.306166	5486.238122	25.230669
158.735107	5492.152690	25.235687
158.643813	5487.330908	25.240704
159.023022	5495.415576	25.245722
159.021012	5511.104380	25.250739
159.221801	5521.707615	25.255757
159.277245	5514.864672	25.260775
159.399482	5532.459591	25.265792
159.428767	5547.998317	25.270810
159.664943	5539.577130	25.275827
159.750402	5546.265246	25.280845
159.686889	5567.778308	25.285863
160.238269	5563.824920	25.290880
160.213797	5581.458653	25.295898
160.538326	5593.702952	25.300915
160.536548	5603.368870	25.305933
160.978391	5605.086236	25.310951
161.174342	5616.173254	25.315968
161.270097	5627.717911	25.320986
161.584161	5620.051557	25.326003
161.768040	5633.047110	25.331021
162.092700	5650.379992	25.336039
162.227146	5639.926010	25.341056
161.904590	5650.276700	25.346074
162.553774	5654.303846	25.351091
162.292349	5659.786831	25.356109
162.459181	5670.310241	25.361127
162.545295	5676.332242	25.366144
162.846726	5687.308078	25.371162
163.292139	5697.506915	25.376179
163.343257	5702.312768	25.381197
163.336896	5695.697252	25.386215
163.264070	5698.413853	25.391232
163.545857	5712.328504	25.396250
163.655164	5723.713263	25.401267
163.813024	5718.183168	25.406285
163.793285	5727.845653	25.411303
164.422391	5736.544715	25.416320
164.125487	5740.275003	25.421338
164.208940	5749.482552	25.426355
164.682695	5758.815205	25.431373
164.820432	5765.946619	25.436391
164.968434	5772.435618	25.441408
165.288088	5789.314852	25.446426
165.345147	5795.925434	25.451443
165.679394	5804.149866	25.456461
165.575172	5816.837132	25.461479
165.737256	5819.112891	25.466496
165.662919	5828.484094	25.471514
165.981409	5840.208648	25.476531
166.247629	5851.477360	25.481549
166.576538	5854.983361	25.486567
166.543922	5866.235764	25.491584
166.454102	5875.565224	25.496602
166.851104	5888.726443	25.501619
167.477173	5891.330425	25.506637
167.087524	5900.271241	25.511655
167.528663	5918.612067	25.516672
167.484236	5932.956798	25.521690
168.094190	5924.811491	25.526707
168.110532	5940.365205	25.531725
167.853196	5948.347767	25.536743
168.349735	5950.839468	25.541760
168.450186	5971.815927	25.546778
168.876067	5974.915324	25.551795
169.026955	5972.217838	25.556813
168.984313	5987.054783	25.561831
169.153972	5995.784910	25.566848
169.191605	6001.262184	25.571866
169.564307	6018.127005	25.576883
169.755543	6030.537690	25.581901
169.846708	6036.514824	25.586919
170.016464	6042.059799	25.591936
170.106326	6060.907214	25.596954
170.789700	6054.991642	25.601971
170.803108	6065.293089	25.606989
170.770620	6081.848950	25.612007
171.207512	6084.106944	25.617024
171.104502	6092.867207	25.622042
171.522068	6101.489099	25.627059
171.498276	6111.130323	25.632077
172.029923	6102.018610	25.637095
172.104918	6103.556739	25.642112
172.228400	6117.395483	25.647130
172.052728	6127.773938	25.652147
172.517674	6129.958094	25.657165
172.675360	6136.979198	25.662183
172.717126	6146.168223	25.667200
172.836098	6156.412146	25.672218
173.105304	6146.546020	25.677236
173.515213	6170.703600	25.682253
173.354276	6180.691494	25.687271
173.461816	6184.074400	25.692288
173.537266	6197.961767	25.697306
173.867458	6202.348375	25.702324
173.958954	6218.575572	25.707341
174.209096	6217.541908	25.712359
174.346354	6225.645865	25.717376
174.173450	6240.534990	25.722394
174.731622	6246.606340	25.727412
174.945950	6254.117387	25.732429
174.685957	6265.042626	25.737447
175.098024	6257.092328	25.742464
175.346061	6280.161066	25.747482
175.298897	6292.063152	25.752500
175.337446	6289.509491	25.757517
175.862579	6310.555549	25.762535
176.380412	6314.982238	25.767552
176.107798	6317.143065	25.772570
176.055491	6333.986371	25.777588
176.668517	6343.490071	25.782605
176.508564	6352.360396	25.787623
177.080697	6363.243722	25.792640
177.188016	6359.375518	25.797658
176.883292	6379.989751	25.802676
177.697939	6390.872983	25.807693
177.521592	6403.871851	25.812711
177.935682	6408.141191	25.817728
178.144024	6416.723402	25.822746
178.205232	6424.454230	25.827764
178.581251	6420.607054	25.832781
178.853917	6445.326313	25.837799
179.033719	6450.898251	25.842816
178.917149	6457.258473	25.847834
178.791724	6454.168563	25.852852
179.373039	6472.579533	25.857869
179.324755	6485.438437	25.862887
179.519970	6493.331396	25.867904
179.869625	6497.307796	25.872922
179.930024	6510.294905	25.877940
180.302525	6524.824172	25.882957
180.533367	6534.179494	25.887975
180.314504	6527.843202	25.892992
180.827196	6550.918173	25.898010
180.890740	6555.902242	25.903028
181.257525	6559.841247	25.908045
181.288858	6579.421281	25.913063
181.442082	6573.781166	25.918080
181.500706	6577.272827	25.923098
181.725112	6605.061997	25.928116
182.005196	6598.701181	25.933133
182.116596	6627.950768	25.938151
182.298945	6627.792679	25.943168
182.355855	6641.557012	25.948186
182.677482	6663.961237	25.953204
183.148332	6664.228323	25.958221
183.290571	6667.302824	25.963239
183.517033	6674.303890	25.968256
183.557770	6683.202915	25.973274
183.469179	6683.002036	25.978292
183.601632	6703.080927	25.983309
183.674441	6719.478809	25.988327
184.477033	6728.867778	25.993344
184.312343	6730.304607	25.998362
184.679571	6751.334871	26.003380
184.857625	6759.773615	26.008397
185.129005	6783.445449	26.013415
185.389213	6777.068745	26.018432
185.455878	6764.266556	26.023450
185.472939	6784.802420	26.028468
185.738491	6792.116251	26.033485
185.795652	6810.085633	26.038503
185.892680	6821.248860	26.043520
186.213809	6825.198232	26.048538
186.269390	6827.506587	26.053556
186.726959	6848.794301	26.058573
186.470989	6854.636671	26.063591
186.547972	6867.394138	26.068608
187.071803	6878.705206	26.073626
187.321259	6882.286992	26.078644
187.416933	6886.107538	26.083661
187.357745	6914.140488	26.088679
187.540703	6915.554438	26.093696
187.817654	6928.094363	26.098714
187.949576	6934.488430	26.103732
188.479691	6952.699548	26.108749
188.543586	6968.322449	26.113767
188.680542	6972.348059	26.118784
189.173593	6984.705795	26.123802
189.486673	6985.944676	26.128820
189.474652	6984.017596	26.133837
189.291008	6991.272445	26.138855
189.316576	7004.846232	26.143872
189.555090	7008.931706	26.148890
189.935818	7028.006041	26.153908
190.296671	7028.874396	26.158925
190.281493	7054.005771	26.163943
190.695927	7068.121657	26.168960
191.049322	7075.996401	26.173978
191.133290	7092.111900	26.178996
191.275544	7087.682451	26.184013
191.667130	7105.580789	26.189031
191.843593	7116.785419	26.194048
192.157906	7119.204811	26.199066
192.043582	7127.045513	26.204084
192.558616	7139.725074	26.209101
192.277115	7157.047009	26.214119
192.658859	7148.008778	26.219136
193.028498	7168.957063	26.224154
193.163563	7179.123268	26.229172
193.177936	7175.951354	26.234189
193.242768	7190.987106	26.239207
193.218464	7197.156339	26.244224
194.008239	7215.364925	26.249242
194.051092	7231.799525	26.254260
193.812450	7236.543837	26.259277
194.173389	7249.872691	26.264295
194.926621	7257.122937	26.269312
195.132717	7263.821194	26.274330
195.107460	7287.508579	26.279348
195.235239	7283.589622	26.284365
195.658340	7299.642703	26.289383
195.661242	7302.303479	26.294400
195.902807	7309.927501	26.299418
196.014742	7321.871625	26.304436
196.497802	7339.920023	26.309453
196.255883	7345.864526	26.314471
196.392957	7354.584621	26.319488
196.813304	7370.376167	26.324506
196.426388	7377.795604	26.329524
197.352673	7393.353218	26.334541
197.357171	7391.322484	26.339559
197.277062	7401.948714	26.344576
197.701706	7417.278708	26.349594
197.536338	7426.892289	26.354612
197.655934	7450.036287	26.359629
198.198792	7451.801149	26.364647
198.383745	7474.057295	26.369664
198.622390	7473.199000	26.374682
198.521079	7489.227063	26.379700
198.957561	7503.342987	26.384717
199.268545	7513.939584	26.389735
199.584169	7535.149307	26.394752
199.713421	7530.642864	26.399770
200.059161	7542.099051	26.404788
200.216377	7554.598179	26.409805
200.640820	7549.382516	26.414823
200.488622	7560.455797	26.419840
200.852152	7558.577162	26.424858
200.742165	7591.098895	26.429876
200.817990	7587.364806	26.434893
201.552732	7596.569119	26.439911
201.448726	7600.661029	26.444928
201.689205	7606.621597	26.449946
201.698404	7617.006655	26.454964
202.081034	7634.253408	26.459981
202.112207	7633.841178	26.464999
202.318097	7652.732032	26.470016
202.487564	7659.982337	26.475034
202.833382	7676.212020	26.480052
202.883682	7683.316837	26.485069
203.261918	7680.482463	26.490087
203.148248	7719.940996	26.495104
203.391529	7720.729937	26.500122
203.688460	7736.989431	26.505140
204.090265	7744.768482	26.510157
203.728764	7760.360828	26.515175
203.986906	7769.074781	26.520192
204.375309	7789.114760	26.525210
204.648275	7802.189447	26.530228
204.817959	7818.636272	26.535245
204.856287	7827.870874	26.540263
205.120143	7845.051191	26.545280
205.529036	7851.919945	26.550298
206.069061	7872.444548	26.555316
206.376253	7884.446845	26.560333
206.683386	7889.509928	26.565351
207.026503	7906.235896	26.570368
206.890165	7902.048792	26.575386
206.810679	7911.207181	26.580404
207.184495	7933.055445	26.585421
207.533358	7938.506638	26.590439
208.005222	7963.392470	26.595456
207.928650	7969.930056	26.600474
208.220702	7965.805267	26.605492
208.203762	7974.568725	26.610509
208.689544	7992.156404	26.615527
208.280845	8001.385354	26.620544
209.053554	8005.298967	26.625562
208.902291	8021.976205	26.630580
209.408467	8029.366490	26.635597
209.707385	8037.606933	26.640615
209.327275	8055.317692	26.645632
209.942520	8060.389382	26.650650
209.834357	8074.496355	26.655668
210.112602	8099.488472	26.660685
210.482652	8101.075260	26.665703
210.844903	8126.177380	26.670720
210.767255	8128.661467	26.675738
210.796504	8136.379078	26.680756
211.243162	8158.222512	26.685773
211.707684	8171.289553	26.690791
211.647935	8191.021321	26.695808
212.020592	8196.598305	26.700826
211.901502	8206.034556	26.705844
212.423919	8222.240212	26.710861
212.923430	8234.638821	26.715879
212.735240	8252.010303	26.720896
213.248360	8256.441364	26.725914
213.344720	8269.398822	26.730932
213.466801	8271.766397	26.735949
213.739812	8292.478526	26.740967
213.956500	8294.076728	26.745984
213.807336	8301.200401	26.751002
214.092012	8320.186938	26.756020
214.651843	8319.758175	26.761037
214.934830	8327.792872	26.766055
214.700765	8346.219801	26.771072
215.089447	8359.545113	26.776090
215.041880	8356.193271	26.781108
215.380378	8375.559762	26.786125
215.884379	8388.617615	26.791143
215.947385	8401.334133	26.796160
216.063432	8407.219739	26.801178
216.461556	8415.997312	26.806196
216.458648	8430.062809	26.811213
216.520622	8440.781034	26.816231
216.550006	8455.075121	26.821248
217.091164	8469.333247	26.826266
217.645683	8480.615239	26.831284
217.800980	8496.341929	26.836301
218.157210	8519.825900	26.841319
218.081783	8517.649704	26.846336
218.210725	8536.247270	26.851354
218.652460	8541.021087	26.856372
218.753709	8558.536944	26.861389
219.354076	8563.693192	26.866407
219.461315	8566.662995	26.871424
219.771076	8578.065477	26.876442
220.011002	8588.815897	26.881460
219.783291	8600.510965	26.886477
220.095578	8614.347265	26.891495
220.487310	8627.583892	26.896512
220.657363	8639.687094	26.901530
220.852945	8642.444166	26.906548
220.592307	8665.658723	26.911565
221.169748	8678.818936	26.916583
221.183930	8700.203509	26.921600
221.468826	8714.066275	26.926618
222.085039	8724.555765	26.931636
222.060484	8731.221231	26.936653
222.277996	8730.119928	26.941671
222.465565	8745.485010	26.946688
222.778747	8765.881969	26.951706
223.231470	8782.711535	26.956724
223.383837	8795.111231	26.961741
223.374295	8803.836035	26.966759
223.712279	8817.415884	26.971776
223.871944	8829.978635	26.976794
224.488614	8848.553782	26.981812
224.561420	8862.213091	26.986829
224.704002	8864.451242	26.991847
224.891852	8873.053596	26.996864
225.019931	8888.683852	27.001882
225.396295	8896.312672	27.006900
225.157595	8923.126521	27.011917
225.908905	8924.416863	27.016935
225.912187	8950.703471	27.021952
226.360679	8960.180637	27.026970
226.702914	8966.766626	27.031988
226.649326	8988.929359	27.037005
226.986640	8985.463436	27.042023
227.301514	9000.139449	27.047040
227.483842	9006.744188	27.052058
227.811139	9018.182082	27.057076
227.749332	9042.234206	27.062093
227.838398	9047.334927	27.067111
227.864627	9068.370737	27.072128
228.305984	9073.732004	27.077146
228.446613	9081.593581	27.082164
228.452036	9097.609470	27.087181
229.206715	9102.454386	27.092199
229.124663	9117.154784	27.097216
229.204244	9138.659064	27.102234
229.710692	9138.983767	27.107252
230.062673	9155.823140	27.112269
230.133599	9172.390828	27.117287
230.202215	9174.968961	27.122304
230.451417	9199.281981	27.127322
230.850378	9204.949870	27.132340
230.899654	9225.887529	27.137357
231.077519	9235.220951	27.142375
231.155082	9253.274757	27.147392
231.292283	9263.504921	27.152410
231.910919	9289.319891	27.157428
232.035942	9306.580146	27.162445
232.281057	9321.317857	27.167463
232.398666	9342.494370	27.172480
232.491583	9349.738386	27.177498
233.231896	9360.672924	27.182516
233.330116	9380.198084	27.187533
233.700792	9393.675357	27.192551
233.881952	9405.622610	27.197568
234.217474	9420.099966	27.202586
234.566281	9431.111663	27.207604
234.514271	9455.248034	27.212621
234.792841	9460.413902	27.217639
235.015790	9476.279219	27.222656
235.078108	9494.023071	27.227674
235.363462	9499.955120	27.232692
235.992683	9517.676491	27.237709
236.382218	9530.026894	27.242727
236.454136	9540.766298	27.247744
236.454345	9563.360158	27.252762
237.207266	9562.588548	27.257780
237.447515	9587.070817	27.262797
237.594426	9597.571176	27.267815
237.290221	9604.122894	27.272832
237.803562	9624.719929	27.277850
238.194639	9624.794340	27.282868
238.203986	9643.446480	27.287885
238.453193	9654.082400	27.292903
238.532304	9674.182345	27.297920
238.475307	9683.047604	27.302938
238.820691	9691.508837	27.307956
239.206147	9717.591420	27.312973
239.404018	9735.061676	27.317991
239.669149	9750.434383	27.323008
239.802314	9766.822351	27.328026
240.574694	9785.989736	27.333044
240.795635	9794.331585	27.338061
240.672174	9811.618604	27.343079
240.919329	9822.513847	27.348096
241.367533	9844.191686	27.353114
241.583248	9850.153701	27.358132
241.555649	9872.101867	27.363149
242.152723	9888.057325	27.368167
242.132159	9907.058571	27.373184
242.279369	9913.116589	27.378202
242.840583	9926.134992	27.383220
242.617048	9945.468027	27.388237
243.382180	9966.960592	27.393255
243.330286	9976.099886	27.398272
243.570559	10000.765825	27.403290
243.888473	10003.857569	27.408308
244.186573	10038.877170	27.413325
244.558433	10037.622160	27.418343
244.758489	10053.943068	27.423360
244.863325	10069.022248	27.428378
245.516704	10074.862098	27.433396
245.722567	10084.065262	27.438413
245.610283	10093.539291	27.443431
246.198931	10104.977960	27.448448
246.466155	10117.038485	27.453466
246.503668	10120.436242	27.458484
246.760370	10136.000034	27.463501
246.908983	10147.817092	27.468519
247.077435	10154.399155	27.473536
247.245790	10172.730114	27.478554
247.803729	10191.685229	27.483572
247.908657	10202.520882	27.488589
247.715190	10215.190407	27.493607
248.424368	10221.125759	27.498624
248.639243	10249.108182	27.503642
248.641932	10252.195672	27.508660
249.243010	10272.596547	27.513677
249.158724	10273.136957	27.518695
249.372082	10297.949591	27.523712
249.463345	10314.723502	27.528730
250.164731	10329.409480	27.533748
250.251266	10341.091141	27.538765
250.304236	10368.985438	27.543783
250.579407	10383.990826	27.548800
250.633845	10401.888334	27.553818
251.554472	10417.749357	27.558836
251.324689	10434.368430	27.563853
251.374081	10450.808013	27.568871
252.143549	10461.132395	27.573888
252.109935	10490.401319	27.578906
252.494033	10501.499690	27.583924
252.925129	10514.447322	27.588941
252.998257	10540.109513	27.593959
253.469084	10550.404948	27.598976
253.541614	10566.136881	27.603994
254.030212	10568.276829	27.609012
254.096669	10586.314719	27.614029
254.205114	10599.322426	27.619047
254.238513	10623.358514	27.624064
254.342096	10649.511816	27.629082
255.303285	10661.091393	27.634100
255.710530	10681.747266	27.639117
255.731731	10699.587114	27.644135
256.269450	10708.757546	27.649152
255.999554	10725.575771	27.654170
256.300239	10732.787778	27.659188
256.460464	10753.918167	27.664205
256.881144	10771.029262	27.669223
257.365178	10786.592717	27.674240
257.417747	10805.239245	27.679258
257.955582	10816.326351	27.684276
257.962543	10838.898590	27.689293
258.293268	10849.579259	27.694311
258.632468	10862.778345	27.699328
258.851888	10881.269351	27.704346
259.010097	10889.103676	27.709364
259.401672	10909.238097	27.714381
259.465409	10923.092948	27.719399
259.853772	10934.677176	27.724416
260.188374	10956.651971	27.729434
260.237140	10964.721346	27.734452
260.891414	10984.495779	27.739469
260.990977	10991.954108	27.744487
261.236200	11002.275662	27.749504
261.336142	11031.868687	27.754522
261.658814	11041.123492	27.759540
262.042502	11051.584420	27.764557
262.159372	11074.708094	27.769575
262.453794	11081.842277	27.774592
262.738634	11091.668245	27.779610
262.833062	11101.482998	27.784628
263.389024	11119.779427	27.789645
263.632631	11139.972009	27.794663
263.754807	11141.575794	27.799680
263.936458	11158.377350	27.804698
264.211682	11170.323628	27.809716
264.109353	11181.902779	27.814733
264.513047	11202.427163	27.819751
264.657117	11225.499397	27.824768
264.674456	11240.580596	27.829786
265.367399	11268.631746	27.834804
265.580193	11287.124190	27.839821
265.650667	11298.850014	27.844839
266.029380	11299.592638	27.849856
266.230301	11342.473487	27.854874
266.559233	11351.421174	27.859892
267.142729	11368.589409	27.864909
267.242418	11384.361980	27.869927
267.653662	11404.774884	27.874944
267.697035	11425.346483	27.879962
268.030707	11446.428379	27.884980
268.231874	11462.933487	27.889997
268.479156	11482.206980	27.895015
268.732686	11489.199313	27.900032
268.889224	11516.441241	27.905050
269.425311	11534.087548	27.910068
269.531729	11549.669743	27.915085
269.970771	11572.481474	27.920103
270.317215	11582.575926	27.925120
270.477338	11613.136165	27.930138
270.907704	11637.256619	27.935156
271.114128	11647.748807	27.940173
271.244341	11666.024048	27.945191
271.694884	11678.678931	27.950208
271.882656	11706.149911	27.955226
272.469793	11718.423445	27.960244
272.539224	11733.095849	27.965261
272.456310	11751.199307	27.970279
272.697579	11769.671977	27.975296
273.238631	11790.889132	27.980314
273.555543	11813.417145	27.985332
273.715423	11826.922882	27.990349
273.826596	11843.057178	27.995367
274.594616	11866.092454	28.000384
274.914398	11888.661159	28.005402
275.052236	11908.596412	28.010420
275.720479	11918.511169	28.015437
275.636338	11940.562184	28.020455
275.922242	11948.301163	28.025472
276.276008	11961.962932	28.030490
276.145972	11979.518226	28.035508
276.720101	11986.166852	28.040525
276.979991	12015.767946	28.045543
277.227776	12029.136905	28.050560
277.322786	12054.065134	28.055578
277.501833	12070.754233	28.060596
277.989829	12084.922413	28.065613
278.494944	12114.494720	28.070631
278.689596	12118.591355	28.075648
278.643731	12141.546050	28.080666
278.825568	12164.853512	28.085684
279.468891	12182.483631	28.090701
279.516675	12202.155417	28.095719
280.346118	12215.796539	28.100736
280.448659	12235.936609	28.105754
280.305302	12244.608190	28.110772
281.129529	12259.702750	28.115789
280.896884	12273.203982	28.120807
281.273392	12281.841511	28.125824
281.479660	12304.008507	28.130842
281.731687	12323.458955	28.135860
282.262658	12337.500597	28.140877
282.338616	12345.762089	28.145895
282.521841	12372.505295	28.150912
282.738921	12395.520159	28.155930
282.774042	12415.269938	28.160948
283.476101	12433.999491	28.165965
283.854689	12449.186117	28.170983
284.126205	12456.409674	28.176000
284.428567	12482.613331	28.181018
284.578307	12494.378007	28.186036
285.113204	12513.424347	28.191053
285.146801	12536.224970	28.196071
285.382299	12547.230993	28.201088
285.580698	12577.868903	28.206106
285.738650	12598.891195	28.211124
285.966605	12623.271987	28.216141
286.233802	12643.847747	28.221159
286.701694	12668.099432	28.226176
287.339132	12682.361494	28.231194
287.341659	12704.819821	28.236212
287.565550	12727.275078	28.241229
288.042825	12756.732755	28.246247
288.573366	12764.184274	28.251264
288.597298	12781.706720	28.256282
288.790809	12810.574195	28.261300
289.332884	12822.779723	28.266317
289.516337	12847.584617	28.271335
289.720187	12872.894771	28.276352
289.992198	12882.142632	28.281370
290.087469	12906.563520	28.286388
290.610168	12918.367932	28.291405
291.093995	12946.078552	28.296423
291.671949	12959.506978	28.301440
291.632978	12975.087861	28.306458
291.740515	13002.368030	28.311476
292.038571	13019.235116	28.316493
292.471354	13043.972789	28.321511
293.241464	13065.123921	28.326528
293.457701	13087.066059	28.331546
293.548424	13103.040422	28.336564
294.013782	13120.626666	28.341581
293.987478	13145.325858	28.346599
294.086709	13161.188409	28.351616
294.726190	13169.276721	28.356634
294.710362	13192.066928	28.361652
295.106649	13219.194807	28.366669
295.529876	13233.528737	28.371687
295.598247	13244.349763	28.376704
295.855200	13268.963691	28.381722
296.235935	13297.455203	28.386740
296.586561	13316.619643	28.391757
296.717736	13343.280793	28.396775
296.875657	13356.465817	28.401792
297.477366	13385.762872	28.406810
297.692615	13412.903597	28.411828
297.712914	13421.003745	28.416845
297.933117	13448.721658	28.421863
298.615717	13477.166154	28.426880
298.868788	13488.368927	28.431898
299.129061	13520.050285	28.436916
299.588805	13546.110756	28.441933
300.093004	13556.023655	28.446951
300.399326	13581.849251	28.451968
300.605963	13594.335202	28.456986
300.817727	13610.477354	28.462004
301.141678	13622.019644	28.467021
301.466127	13634.278736	28.472039
301.753481	13646.044677	28.477056
302.185244	13667.947410	28.482074
302.284378	13696.212043	28.487092
302.281618	13707.205534	28.492109
302.932679	13730.280360	28.497127
303.134409	13747.665314	28.502144
303.381707	13764.863137	28.507162
303.707079	13789.621767	28.512180
303.878547	13808.252634	28.517197
304.211402	13830.246842	28.522215
304.453947	13847.322319	28.527232
304.610460	13860.770033	28.532250
304.622513	13893.068822	28.537268
305.127672	13909.433706	28.542285
305.587822	13938.137964	28.547303
305.716505	13964.446671	28.552320
306.151659	13993.281251	28.557338
306.774717	14024.025512	28.562356
307.095418	14033.102088	28.567373
307.146340	14059.568379	28.572391
307.449889	14085.186659	28.577408
307.784606	14097.905526	28.582426
308.082748	14126.850199	28.587444
308.304780	14150.722266	28.592461
308.768046	14175.134512	28.597479
308.919913	14210.721650	28.602496
309.125653	14228.017988	28.607514
309.588132	14264.709288	28.612532
309.941547	14286.906082	28.617549
310.570230	14308.781866	28.622567
311.127939	14334.572264	28.627584
311.699033	14352.215726	28.632602
311.352754	14366.064689	28.637620
311.600044	14386.509657	28.642637
312.085150	14416.053955	28.647655
312.196160	14434.274869	28.652672
312.679576	14455.860920	28.657690
313.078714	14484.853479	28.662708
313.680799	14502.590129	28.667725
313.763079	14527.125670	28.672743
313.872134	14557.818667	28.677760
314.104936	14567.228243	28.682778
314.432170	14591.084383	28.687796
314.727148	14615.893064	28.692813
315.441653	14629.446564	28.697831
315.534967	14653.958432	28.702848
316.195688	14678.353026	28.707866
316.482729	14694.856974	28.712884
316.918211	14717.309863	28.717901
317.207820	14742.163764	28.722919
317.297081	14764.724631	28.727936
317.713163	14780.182019	28.732954
317.984800	14804.599824	28.737972
318.102931	14814.365416	28.742989
318.299233	14834.506187	28.748007
318.231875	14857.843356	28.753024
318.660697	14870.724860	28.758042
319.354860	14908.085394	28.763060
319.453600	14931.595605	28.768077
319.811605	14957.920291	28.773095
319.998102	14982.907512	28.778112
320.764656	15004.550897	28.783130
320.643587	15022.091801	28.788148
320.904208	15053.355604	28.793165
321.099157	15079.418597	28.798183
321.752425	15105.703552	28.803200
321.981201	15120.830513	28.808218
322.264929	15143.765624	28.813236
322.870250	15167.717888	28.818253
323.353238	15198.347022	28.823271
323.566320	15214.048166	28.828288
324.092725	15224.836467	28.833306
324.292818	15240.618624	28.838324
324.171149	15269.416026	28.843341
324.442406	15294.185087	28.848359
324.620185	15317.784456	28.853376
325.131786	15333.145214	28.858394
325.356859	15356.329800	28.863412
325.797516	15380.674490	28.868429
326.057942	15405.066392	28.873447
326.564617	15434.567830	28.878464
326.707205	15457.497001	28.883482
327.022962	15490.227823	28.888500
327.437237	15503.993211	28.893517
327.636062	15532.165985	28.898535
327.883604	15568.204939	28.903552
328.475200	15594.816062	28.908570
328.736225	15624.223620	28.913588
329.110688	15647.419900	28.918605
329.783923	15673.209803	28.923623
329.781086	15698.268674	28.928640
330.500440	15720.435080	28.933658
330.462029	15741.516867	28.938676
330.977213	15773.503139	28.943693
331.434772	15790.183460	28.948711
331.432439	15817.873346	28.953728
332.198764	15844.135290	28.958746
332.250739	15867.871903	28.963764
332.572741	15885.350508	28.968781
333.107059	15912.040530	28.973799
333.258500	15941.674195	28.978816
333.824554	15965.895758	28.983834
333.689568	15986.215970	28.988852
333.961606	16013.304119	28.993869
334.683278	16035.574755	28.998887
334.935866	16069.674584	29.003904
335.075758	16091.802692	29.008922
335.425235	16123.259619	29.013940
335.688139	16155.137599	29.018957
336.417361	16176.447048	29.023975
336.653062	16193.386722	29.028992
337.097399	16222.197959	29.034010
337.308919	16247.903037	29.039028
337.695428	16277.863622	29.044045
338.307210	16303.550295	29.049063
338.276644	16318.358759	29.054080
338.937683	16342.281657	29.059098
338.878969	16379.996722	29.064116
339.084086	16398.391112	29.069133
339.862287	16427.507269	29.074151
340.371583	16452.057345	29.079168
340.705859	16474.127018	29.084186
340.911875	16499.075253	29.089204
340.867574	16532.578073	29.094221
341.162462	16550.803780	29.099239
341.614146	16584.636446	29.104256
342.091124	16603.200068	29.109274
342.227696	16629.624904	29.114292
342.831443	16652.574861	29.119309
343.428134	16675.086914	29.124327
343.456528	16700.615977	29.129344
343.958708	16720.154911	29.134362
344.527659	16746.354251	29.139380
344.665528	16770.618633	29.144397
344.948397	16779.503454	29.149415
345.372746	16808.517689	29.154432
345.693659	16822.440783	29.159450
345.612628	16839.503286	29.164468
346.109465	16861.393170	29.169485
346.486640	16879.021963	29.174503
346.643208	16908.270967	29.179520
347.006021	16943.924888	29.184538
347.438012	16963.017069	29.189556
347.650255	16982.592210	29.194573
347.873093	17014.155711	29.199591
348.492215	17050.060269	29.204608
348.915863	17069.791899	29.209626
348.994147	17097.429932	29.214644
349.184035	17137.318556	29.219661
349.443106	17155.496749	29.224679
349.960109	17193.584378	29.229696
350.203098	17219.529035	29.234714
350.843091	17253.093322	29.239732
350.695534	17285.473355	29.244749
351.506232	17312.409463	29.249767
351.663500	17340.483997	29.254784
352.406987	17374.701915	29.259802
353.211792	17391.392407	29.264820
353.037570	17421.230971	29.269837
353.567990	17451.129774	29.274855
353.920523	17473.121922	29.279872
354.062562	17506.613033	29.284890
354.645452	17537.533476	29.289908
354.843571	17559.259312	29.294925
355.177483	17585.960936	29.299943
355.479150	17616.363311	29.304960
355.492916	17636.260802	29.309978
356.130599	17666.989665	29.314996
356.489940	17709.411467	29.320013
356.975191	17738.262782	29.325031
357.408380	17763.142320	29.330048
357.869755	17797.152479	29.335066
358.237608	17818.062339	29.340084
358.353590	17845.663946	29.345101
359.026741	17866.911401	29.350119
359.261400	17912.751970	29.355136
359.904503	17925.601962	29.360154
360.169984	17951.329282	29.365172
360.428312	17988.366070	29.370189
360.717559	18000.810363	29.375207
361.234593	18039.544037	29.380224
361.237826	18061.458900	29.385242
362.134952	18084.743657	29.390260
362.190886	18119.847648	29.395277
362.503068	18138.448038	29.400295
362.835532	18179.207245	29.405312
362.955671	18196.574260	29.410330
363.285239	18226.215113	29.415348
363.865297	18267.997076	29.420365
364.398163	18287.927640	29.425383
364.605623	18310.259342	29.430400
364.905347	18346.077348	29.435418
365.611128	18364.622619	29.440436
365.658201	18399.469480	29.445453
365.944145	18422.818791	29.450471
366.230055	18459.296204	29.455488
366.797459	18486.587940	29.460506
367.404318	18517.392475	29.465524
367.410834	18546.869618	29.470541
367.801018	18560.189252	29.475559
367.800569	18590.324591	29.480576
368.060317	18624.544678	29.485594
369.211371	18657.456436	29.490612
368.890182	18684.710743	29.495629
369.257729	18701.780428	29.500647
369.442438	18746.076624	29.505664
369.869014	18775.463044	29.510682
370.599676	18811.075413	29.515700
370.627093	18841.781692	29.520717
370.682723	18874.075681	29.525735
371.397205	18915.724259	29.530752
372.333755	18942.680831	29.535770
372.928411	18976.090939	29.540788
372.681987	19007.295255	29.545805
373.127358	19026.937026	29.550823
373.626628	19064.020251	29.555840
373.823817	19098.137247	29.560858
374.367926	19123.898288	29.565876
374.387878	19160.330222	29.570893
374.911211	19188.684932	29.575911
375.680300	19224.980688	29.580928
375.696809	19253.313794	29.585946
376.341770	19279.476225	29.590964
376.411366	19320.449578	29.595981
376.942826	19346.263438	29.600999
377.626380	19381.524107	29.606016
377.593639	19415.873530	29.611034
378.182682	19448.982066	29.616052
378.477210	19483.463566	29.621069
379.283516	19505.513296	29.626087
379.579557	19534.403231	29.631104
379.686773	19568.648866	29.636122
380.187282	19610.995836	29.641140
380.611978	19636.700442	29.646157
380.724222	19666.030034	29.651175
381.229628	19696.447970	29.656192
381.521787	19734.392573	29.661210
381.790565	19772.214551	29.666228
382.297029	19806.518107	29.671245
382.556494	19844.771313	29.676263
383.571660	19861.904844	29.681280
383.993630	19904.207888	29.686298
383.977252	19923.815482	29.691316
384.464004	19962.014361	29.696333
384.930865	19985.406703	29.701351
385.353844	20019.275120	29.706368
385.564420	20045.272847	29.711386
385.822490	20080.544561	29.716404
386.390089	20111.850581	29.721421
386.589923	20141.350391	29.726439
387.396659	20175.885561	29.731456
387.673643	20205.878839	29.736474
388.004105	20229.539248	29.741492
388.327026	20278.347426	29.746509
388.988565	20300.344911	29.751527
389.366145	20324.193920	29.756544
389.575354	20367.491663	29.761562
390.073809	20385.313144	29.766580
390.161683	20419.076785	29.771597
390.684871	20444.173106	29.776615
391.140187	20473.342755	29.781632
391.642216	20510.573611	29.786650
391.880434	20539.537268	29.791668
392.477603	20572.545338	29.796685
392.676334	20604.048926	29.801703
393.336538	20635.385505	29.806720
393.097238	20661.928391	29.811738
393.872041	20685.665073	29.816756
394.172508	20715.598585	29.821773
394.294893	20745.004020	29.826791
395.003043	20769.313579	29.831808
395.045962	20803.495616	29.836826
395.521031	20828.081856	29.841844
396.092295	20871.387181	29.846861
396.370786	20898.392665	29.851879
396.678270	20923.295922	29.856896
396.939433	20958.195937	29.861914
397.305858	20984.903436	29.866932
397.410603	21032.250182	29.871949
398.001887	21060.363175	29.876967
398.785855	21103.067029	29.881984
399.027748	21137.117382	29.887002
399.205520	21167.734244	29.892020
400.082973	21199.903331	29.897037
400.195877	21234.789148	29.902055
400.789860	21274.010022	29.907072
400.807308	21309.252123	29.912090
401.838089	21340.102118	29.917108
402.108217	21374.003130	29.922125
402.225273	21407.226813	29.927143
402.837571	21438.521627	29.932160
402.980104	21481.598472	29.937178
403.723387	21500.797989	29.942196
403.950764	21533.063127	29.947213
404.381786	21572.133198	29.952231
404.828444	21609.911889	29.957248
405.320143	21648.820959	29.962266
405.925205	21678.765092	29.967284
405.829898	21718.764597	29.972301
406.334512	21748.124293	29.977319
406.724252	21776.415206	29.982336
406.992832	21817.065608	29.987354
407.444438	21850.313457	29.992372
407.824697	21895.003157	29.997389
408.018763	21939.298764	30.002407
409.056875	21977.194035	30.007424
409.120036	22010.515635	30.012442
409.857171	22049.127978	30.017460
410.244210	22081.337408	30.022477
410.524536	22119.920341	30.027495
411.143840	22154.387242	30.032512
411.429617	22195.989872	30.037530
411.908604	22216.893342	30.042548
412.307573	22245.164523	30.047565
412.531405	22284.969848	30.052583
413.221651	22313.321880	30.057600
413.669168	22352.852187	30.062618
413.834329	22391.163016	30.067636
414.444452	22427.527504	30.072653
415.164887	22461.896954	30.077671
415.499802	22498.380506	30.082688
415.862700	22526.006886	30.087706
415.983729	22555.370991	30.092724
416.541558	22589.702942	30.097741
417.218550	22624.679782	30.102759
417.491595	22654.506784	30.107776
417.790762	22684.980597	30.112794
418.446419	22720.453829	30.117812
418.380242	22760.640439	30.122829
418.499109	22794.333770	30.127847
419.313050	22828.657614	30.132864
419.441455	22867.259475	30.137882
420.182437	22900.615417	30.142900
420.569885	22938.905123	30.147917
420.585564	22978.763398	30.152935
421.630545	23005.417892	30.157952
421.802914	23040.676716	30.162970
422.084438	23077.542521	30.167988
423.107247	23100.592395	30.173005
423.293036	23125.075144	30.178023
423.850435	23147.464951	30.183040
423.763978	23187.522896	30.188058
424.315167	23219.765333	30.193076
424.730878	23252.509301	30.198093
425.249829	23295.057182	30.203111
425.816308	23327.562805	30.208128
425.729117	23362.237252	30.213146
426.108172	23390.355202	30.218164
426.689739	23430.593365	30.223181
427.091841	23467.011296	30.228199
427.407551	23512.826932	30.233216
427.834065	23549.677219	30.238234
428.310055	23580.516501	30.243252
428.920578	23620.674682	30.248269
429.224179	23668.230378	30.253287
429.919422	23698.921754	30.258304
430.285530	23735.604905	30.263322
430.722362	23757.401307	30.268340
431.162415	23798.882012	30.273357
431.435838	23843.201022	30.278375
431.702380	23873.871344	30.283392
431.794754	23925.877985	30.288410
432.245479	23969.790341	30.293428
432.762721	24014.728760	30.298445
433.650826	24056.323084	30.303463
434.509091	24082.439521	30.308480
434.666034	24123.522882	30.313498
435.358413	24166.835388	30.318516
435.524201	24193.869327	30.323533
435.954232	24239.144204	30.328551
436.681243	24273.591587	30.333568
436.777177	24309.490253	30.338586
437.014699	24349.177481	30.343604
437.499717	24384.920546	30.348621
437.786893	24437.302452	30.353639
438.558609	24467.376353	30.358656
438.903068	24505.846424	30.363674
439.235119	24550.075661	30.368692
440.054413	24603.644893	30.373709
440.249208	24637.992996	30.378727
440.928245	24674.837401	30.383744
441.060856	24702.705093	30.388762
441.672782	24742.713635	30.393780
442.181207	24781.354462	30.398797
442.443246	24832.414206	30.403815
443.380813	24852.490254	30.408832
443.655384	24908.471266	30.413850
444.109506	24944.150650	30.418868
444.955362	24972.696966	30.423885
445.053781	25017.128137	30.428903
445.459946	25049.143451	30.433920
445.837815	25081.643549	30.438938
446.395785	25118.874278	30.443956
447.263424	25155.702665	30.448973
447.347139	25195.706366	30.453991
447.483847	25219.245073	30.459008
448.172695	25259.438510	30.464026
448.265493	25299.908661	30.469044
448.901782	25334.075045	30.474061
449.257540	25377.828401	30.479079
450.042598	25417.507816	30.484096
450.307700	25451.542942	30.489114
450.094149	25487.485863	30.494132
450.961872	25522.039749	30.499149
451.539188	25562.801092	30.504167
451.941512	25599.102782	30.509184
452.082658	25638.188296	30.514202
452.498421	25667.744636	30.519220
453.113201	25710.048795	30.524237
453.440290	25750.976110	30.529255
453.983112	25792.849316	30.534272
454.264901	25828.645739	30.539290
454.904064	25872.526418	30.544308
455.186218	25905.238757	30.549325
455.390234	25948.163914	30.554343
455.988663	25988.278167	30.559360
456.295186	26032.868580	30.564378
456.039892	26076.896120	30.569396
457.391012	26121.778160	30.574413
458.049345	26180.881596	30.579431
458.634499	26219.721727	30.584448
459.127237	26258.133999	30.589466
459.217994	26300.129623	30.594484
460.322773	26345.341471	30.599501
460.644010	26386.650199	30.604519
461.217531	26426.282569	30.609536
461.757789	26470.546609	30.614554
461.723106	26505.768099	30.619572
462.495506	26536.388526	30.624589
462.724461	26587.066035	30.629607
463.647227	26630.739614	30.634624
463.853981	26670.992411	30.639642
463.937781	26706.562267	30.644660
464.609037	26755.932148	30.649677
465.334093	26802.873050	30.654695
465.676055	26842.801636	30.659712
465.677274	26882.682545	30.664730
466.337697	26931.883902	30.669748
467.151752	26969.191699	30.674765
467.480235	27012.952862	30.679783
467.933973	27059.159447	30.684800
468.733189	27091.672628	30.689818
468.889667	27140.390908	30.694836
469.365847	27174.920463	30.699853
469.874985	27227.925841	30.704871
470.490402	27275.498089	30.709888
471.135339	27301.304499	30.714906
470.919867	27355.826843	30.719924
471.400036	27392.454538	30.724941
471.601280	27450.388130	30.729959
472.762888	27491.971993	30.734976
473.414092	27541.245795	30.739994
473.742919	27585.412649	30.745012
474.133695	27629.487728	30.750029
474.896627	27676.576409	30.755047
474.825609	27717.209771	30.760064
475.324334	27763.012712	30.765082
475.902566	27810.238080	30.770100
476.566117	27847.691154	30.775117
476.996049	27894.219394	30.780135
477.382882	27943.624065	30.785152
477.753918	27979.429262	30.790170
477.984854	28023.403814	30.795188
478.966229	28071.249277	30.800205
479.676991	28116.261317	30.805223
479.670583	28167.757068	30.810240
480.378121	28213.869633	30.815258
480.755598	28255.438815	30.820276
481.020298	28292.727629	30.825293
481.395618	28342.899881	30.830311
482.215152	28390.588138	30.835328
482.864571	28430.003939	30.840346
482.710063	28478.243171	30.845364
483.443222	28520.262847	30.850381
484.181281	28558.912834	30.855399
484.398908	28601.032384	30.860416
484.832495	28636.860539	30.865434
485.062279	28689.369870	30.870452
485.868112	28722.295476	30.875469
486.212681	28778.510062	30.880487
486.545891	28834.094488	30.885504
487.555830	28869.459844	30.890522
487.530854	28928.747808	30.895540
488.156661	28965.943362	30.900557
488.449192	29008.854780	30.905575
489.011319	29054.745496	30.910592
489.643126	29103.299187	30.915610
490.245803	29158.064801	30.920628
490.846182	29203.292472	30.925645
490.986150	29252.941238	30.930663
491.534835	29296.811863	30.935680
492.120510	29343.394854	30.940698
492.271414	29402.448039	30.945716
493.045606	29456.517547	30.950733
493.277744	29505.197997	30.955751
494.050488	29557.675074	30.960768
494.596309	29605.149859	30.965786
494.963146	29663.348221	30.970804
495.522674	29711.478507	30.975821
496.271040	29751.247978	30.980839
496.724917	29811.677154	30.985856
497.172404	29857.252590	30.990874
497.391834	29916.580971	30.995892
497.937322	29973.310979	31.000909
498.055205	30016.371953	31.005927
499.072416	30074.166187	31.010944
499.390783	30134.851421	31.015962
499.935330	30192.618876	31.020980
500.744001	30232.639006	31.025997
501.185573	30296.921233	31.031015
501.842423	30337.249806	31.036032
502.351803	30383.531027	31.041050
502.661828	30433.920888	31.046068
503.312480	30489.226165	31.051085
503.825587	30536.417431	31.056103
504.170182	30584.084021	31.061120
504.901779	30639.895383	31.066138
505.070954	30701.850978	31.071156
505.710728	30742.296802	31.076173
506.536819	30794.231339	31.081191
506.898570	30845.941620	31.086208
507.539127	30895.117670	31.091226
508.031105	30944.102174	31.096244
508.331182	30993.199031	31.101261
509.457377	31033.234195	31.106279
509.789614	31087.642702	31.111296
510.366462	31125.646345	31.116314
510.578722	31180.497435	31.121332
511.386289	31227.745302	31.126349
511.734237	31273.876789	31.131367
512.253890	31311.023660	31.136384
512.723384	31357.439737	31.141402
513.043299	31401.369626	31.146420
513.618181	31455.753736	31.151437
514.175943	31513.744063	31.156455
514.511424	31558.038506	31.161472
515.325521	31605.760342	31.166490
515.878326	31655.893882	31.171508
516.269966	31696.285603	31.176525
516.801749	31743.476688	31.181543
517.344483	31790.836854	31.186560
517.872291	31829.487969	31.191578
518.019584	31867.320016	31.196596
518.684437	31911.260174	31.201613
519.218394	31957.547377	31.206631
519.878914	32006.520631	31.211648
520.289328	32049.445175	31.216666
520.680498	32101.293050	31.221684
521.106963	32143.399746	31.226701
521.809763	32186.885685	31.231719
522.104962	32241.713934	31.236736
522.710917	32295.286157	31.241754
523.023371	32349.245874	31.246772
523.673410	32396.925676	31.251789
524.394438	32442.754759	31.256807
524.849316	32499.828283	31.261824
525.176222	32545.460115	31.266842
525.909775	32590.889272	31.271860
526.082238	32644.169926	31.276877
527.029332	32701.318638	31.281895
527.137192	32753.756204	31.286912
527.633887	32807.555482	31.291930
528.571306	32873.784768	31.296948
529.116247	32922.158698	31.301965
529.452010	32973.018509	31.306983
529.648885	33022.477701	31.312000
530.345763	33080.444267	31.317018
530.593020	33140.770062	31.322036
531.684929	33189.444600	31.327053
532.583531	33238.004114	31.332071
532.885172	33295.628552	31.337088
533.546464	33357.085033	31.342106
533.571112	33409.474046	31.347124
534.399487	33461.806855	31.352141
535.170513	33506.713698	31.357159
535.663779	33562.058099	31.362176
536.055473	33612.284784	31.367194
536.568452	33664.420923	31.372212
537.174478	33722.232785	31.377229
537.685952	33771.170285	31.382247
537.838453	33834.617220	31.387264
538.694560	33888.521037	31.392282
539.027325	33944.770403	31.397300
539.493452	34012.847388	31.402317
540.336237	34056.340571	31.407335
541.081477	34112.159077	31.412352
541.727558	34160.817176	31.417370
542.196428	34218.278851	31.422388
542.792359	34257.322096	31.427405
543.533815	34324.800579	31.432423
543.726663	34380.845408	31.437440
544.182627	34432.846956	31.442458
544.894558	34474.749229	31.447476
545.429829	34534.205639	31.452493
546.112806	34582.169761	31.457511
546.458391	34646.233805	31.462528
547.077648	34684.724114	31.467546
547.575291	34744.022616	31.472564
548.145123	34799.086393	31.477581
549.065437	34845.098154	31.482599
549.273794	34906.351887	31.487616
549.733974	34955.521462	31.492634
550.236240	35010.305523	31.497652
551.169363	35061.146362	31.502669
551.634308	35109.367126	31.507687
551.980937	35168.153027	31.512704
552.547238	35220.449048	31.517722
553.222782	35268.333692	31.522740
553.612069	35311.236585	31.527757
554.233926	35367.716340	31.532775
554.608567	35413.346903	31.537792
555.354452	35460.278850	31.542810
555.506417	35506.191081	31.547828
555.945004	35552.077491	31.552845
556.715832	35609.350218	31.557863
556.917457	35672.086789	31.562880
557.457646	35727.138648	31.567898
557.981067	35787.871352	31.572916
558.457665	35850.748751	31.577933
559.391191	35904.512795	31.582951
559.706448	35965.000391	31.587968
560.230978	36024.171795	31.592986
561.051489	36082.190462	31.598004
561.390289	36138.027374	31.603021
562.077275	36196.952505	31.608039
562.443358	36258.444676	31.613056
563.249164	36314.607269	31.618074
563.855415	36378.793787	31.623092
564.409132	36447.117788	31.628109
565.599119	36495.481068	31.633127
565.376186	36556.162123	31.638144
565.934979	36607.058963	31.643162
566.731875	36670.356534	31.648180
567.235326	36733.365116	31.653197
567.962147	36791.956838	31.658215
568.186532	36864.064510	31.663232
568.714791	36919.899085	31.668250
569.679548	36979.883135	31.673268
569.948391	37057.802004	31.678285
570.947589	37103.566008	31.683303
571.176063	37171.791498	31.688320
571.622618	37234.393117	31.693338
572.476511	37297.329502	31.698356
572.628280	37361.881026	31.703373
573.366679	37423.077937	31.708391
574.130423	37485.023554	31.713408
574.538702	37552.400033	31.718426
575.022983	37617.576867	31.723444
575.961207	37676.688047	31.728461
577.022807	37741.945579	31.733479
577.332158	37799.094092	31.738496
577.580492	37862.550656	31.743514
578.195555	37920.568540	31.748532
579.010214	37984.240302	31.753549
579.413082	38041.672025	31.758567
580.266669	38115.582459	31.763584
580.259703	38180.433215	31.768602
581.366887	38225.082369	31.773620
581.821685	38298.897793	31.778637
582.468517	38350.417354	31.783655
582.744695	38431.710620	31.788672
583.580632	38494.444633	31.793690
584.384614	38553.800580	31.798708
585.246271	38609.473496	31.803725
585.407687	38667.830039	31.808743
586.311381	38728.385033	31.813760
586.999769	38787.481473	31.818778
587.399532	38841.089845	31.823796
588.008828	38908.780569	31.828813
588.509351	38965.124383	31.833831
588.758150	39022.323559	31.838848
589.697541	39077.530180	31.843866
589.910607	39144.474225	31.848884
590.542506	39204.269967	31.853901
591.210103	39265.761453	31.858919
591.981833	39323.031301	31.863936
592.163536	39375.334443	31.868954
593.006102	39425.112082	31.873972
593.483487	39494.539124	31.878989
594.319982	39549.826304	31.884007
594.618187	39609.612183	31.889024
594.822279	39663.866674	31.894042
595.759034	39714.977274	31.899060
596.245548	39782.449635	31.904077
597.237483	39841.311682	31.909095
597.812551	39904.223441	31.914112
598.479485	39966.665649	31.919130
598.787478	40024.250294	31.924148
599.440704	40086.682345	31.929165
599.723911	40139.186450	31.934183
600.490153	40206.647937	31.939200
600.938843	40281.849763	31.944218
601.867514	40338.686625	31.949236
602.706862	40411.494029	31.954253
602.977726	40470.262000	31.959271
603.621044	40533.892193	31.964288
604.252699	40592.344688	31.969306
604.777506	40653.154118	31.974324
605.371141	40730.851921	31.979341
605.973378	40799.068237	31.984359
606.626493	40851.699533	31.989376
607.091172	40931.606523	31.994394
608.046413	40985.740335	31.999412
608.874406	41060.309902	32.004429
609.330755	41119.164408	32.009447
609.750012	41192.830777	32.014464
610.280350	41258.473021	32.019482
611.067834	41319.768108	32.024500
611.403597	41400.525524	32.029517
611.935823	41461.544751	32.034535
612.463643	41526.448202	32.039552
613.170229	41604.226280	32.044570
613.998804	41674.035325	32.049588
614.355328	41736.860085	32.054605
615.391578	41809.540102	32.059623
616.130377	41877.788983	32.064640
616.359097	41941.146651	32.069658
616.913145	42009.140256	32.074676
617.670521	42092.123773	32.079693
618.177251	42149.512104	32.084711
619.059032	42222.065878	32.089728
619.415742	42293.114567	32.094746
620.396064	42355.520826	32.099764
620.947525	42434.287521	32.104781
621.358167	42499.730838	32.109799
622.179339	42561.485832	32.114816
622.556107	42641.735374	32.119834
623.559710	42703.917597	32.124852
624.300021	42778.000713	32.129869
624.718329	42845.278119	32.134887
625.558409	42909.548506	32.139904
625.809495	42975.789882	32.144922
626.455777	43036.656451	32.149940
627.314764	43098.071789	32.154957
628.057223	43176.678386	32.159975
628.658052	43236.502644	32.164992
629.112006	43307.969474	32.170010
630.011504	43372.206597	32.175028
630.722787	43436.441757	32.180045
631.337557	43490.483241	32.185063
632.013368	43564.148969	32.190080
632.020736	43627.356369	32.195098
633.223310	43688.080677	32.200116
633.923292	43759.080306	32.205133
634.279244	43813.915826	32.210151
634.638910	43874.614518	32.215168
635.063071	43943.741344	32.220186
635.743295	44006.464921	32.225204
636.656875	44060.827870	32.230221
637.072716	44132.670192	32.235239
638.014284	44190.451140	32.240256
638.108633	44255.063600	32.245274
639.177911	44324.558663	32.250292
639.458440	44394.341929	32.255309
640.024695	44468.508544	32.260327
640.815585	44532.898865	32.265344
641.277280	44612.743708	32.270362
642.194696	44672.136384	32.275380
643.114206	44750.720811	32.280397
643.361941	44821.573250	32.285415
644.212955	44889.446935	32.290432
644.644886	44960.017940	32.295450
645.324480	45028.361689	32.300468
645.957252	45109.959035	32.305485
646.281211	45174.373721	32.310503
647.512831	45245.800877	32.315520
647.969097	45327.749271	32.320538
648.891509	45397.156804	32.325556
649.253942	45463.103463	32.330573
649.750124	45535.551309	32.335591
650.407518	45610.599375	32.340608
651.081542	45693.558767	32.345626
652.160368	45767.908770	32.350644
652.810198	45846.956782	32.355661
653.239097	45909.269583	32.360679
654.061386	45983.445392	32.365696
654.132962	46059.105425	32.370714
655.147865	46133.555211	32.375732
655.753802	46213.364177	32.380749
656.590402	46293.244845	32.385767
657.590855	46367.033430	32.390784
658.002994	46442.736305	32.395802
658.794004	46513.047185	32.400820
659.352922	46588.721236	32.405837
659.943594	46652.990837	32.410855
660.587618	46725.052435	32.415872
660.968407	46806.866197	32.420890
661.992183	46883.373080	32.425908
662.904017	46958.214974	32.430925
663.635465	47034.483468	32.435943
664.568498	47107.038754	32.440960
664.923573	47177.261811	32.445978
666.045847	47242.069810	32.450996
666.372526	47315.271110	32.456013
666.977399	47384.633265	32.461031
667.680633	47459.901717	32.466048
668.308671	47532.259399	32.471066
669.055917	47592.844159	32.476084
669.565361	47661.178244	32.481101
670.189218	47737.193912	32.486119
670.932782	47799.797940	32.491136
671.259309	47885.116296	32.496154
672.038205	47954.471916	32.501172
672.743659	48025.338637	32.506189
673.308718	48110.905177	32.511207
674.299569	48172.990686	32.516224
674.562849	48255.947868	32.521242
675.352248	48328.985063	32.526260
676.496582	48390.971211	32.531277
676.794635	48475.151111	32.536295
677.800055	48549.306633	32.541312
678.092112	48611.173782	32.546330
678.642605	48678.517521	32.551348
679.306470	48747.058437	32.556365
679.776341	48822.551408	32.561383
680.969653	48894.280785	32.566400
681.390682	48967.327094	32.571418
681.718848	49034.611795	32.576436
682.521738	49101.101092	32.581453
683.205560	49185.938122	32.586471
684.135204	49256.039633	32.591488
684.665077	49331.208539	32.596506
685.091764	49415.257861	32.601524
685.669111	49491.337258	32.606541
686.493188	49568.453852	32.611559
687.460416	49647.908252	32.616576
688.161663	49732.029620	32.621594
688.621335	49809.741885	32.626612
689.259415	49890.684904	32.631629
689.857209	49960.422947	32.636647
690.746565	50042.333151	32.641664
691.017176	50132.768260	32.646682
692.018651	50201.678235	32.651700
692.816943	50284.318526	32.656717
693.504393	50376.131901	32.661735
693.914559	50448.020407	32.666752
694.783024	50540.014884	32.671770
695.655104	50623.499008	32.676788
696.217242	50703.260917	32.681805
696.859033	50791.419601	32.686823
697.917253	50873.002596	32.691840
698.419329	50963.746379	32.696858
699.136745	51040.922559	32.701876
699.613643	51131.848109	32.706893
700.258244	51219.343603	32.711911
701.055378	51300.513415	32.716928
701.840038	51395.915918	32.721946
702.123758	51474.110574	32.726964
703.218786	51559.771446	32.731981
703.889334	51664.456389	32.736999
704.491136	51750.296442	32.742016
705.195115	51840.670341	32.747034
706.013859	51922.414748	32.752052
706.859762	52006.679912	32.757069
707.413182	52105.665005	32.762087
708.387927	52191.758335	32.767104
709.067519	52273.462486	32.772122
709.773857	52367.305634	32.777140
710.883915	52455.169491	32.782157
711.306864	52543.609534	32.787175
712.134404	52630.765288	32.792192
712.820268	52705.743523	32.797210
713.413985	52796.878741	32.802228
714.470238	52881.088805	32.807245
715.006860	52977.688284	32.812263
715.670415	53044.761238	32.817280
716.738560	53140.601065	32.822298
716.989318	53231.582857	32.827316
718.457254	53302.321027	32.832333
718.617861	53390.235826	32.837351
719.184081	53461.982621	32.842368
719.973256	53552.590249	32.847386
720.612048	53640.272896	32.852404
721.221416	53719.461854	32.857421
721.954908	53811.211924	32.862439
722.556355	53893.598404	32.867456
723.259158	53987.328343	32.872474
724.096588	54089.561637	32.877492
725.124488	54170.331896	32.882509
725.314184	54246.196421	32.887527
725.944670	54319.859543	32.892544
726.943316	54413.905556	32.897562
727.509751	54492.996250	32.902580
728.482204	54563.088047	32.907597
729.130420	54654.291524	32.912615
729.844282	54735.821665	32.917632
730.601762	54816.345372	32.922650
731.248290	54906.221123	32.927668
732.063139	54985.913729	32.932685
732.751891	55078.435130	32.937703
733.204207	55161.444249	32.942720
734.167797	55247.607454	32.947738
734.634681	55338.810314	32.952756
735.639632	55432.568266	32.957773
736.102796	55520.279047	32.962791
736.827894	55607.493473	32.967808
737.418463	55702.943828	32.972826
738.116286	55799.029619	32.977844
739.311600	55884.684195	32.982861
740.137758	55977.225541	32.987879
740.913566	56074.376106	32.992896
741.333215	56178.360920	32.997914
741.894064	56261.211308	33.002932
742.902221	56357.434282	33.007949
743.320571	56453.515837	33.012967
744.423321	56546.971725	33.017984
745.254345	56642.698289	33.023002
745.901660	56740.118502	33.028020
747.116947	56829.475735	33.033037
747.547665	56927.228084	33.038055
747.913201	57021.921489	33.043072
749.145725	57108.150552	33.048090
749.625239	57208.067243	33.053108
750.597991	57301.824903	33.058125
751.645182	57414.678720	33.063143
751.922261	57503.539813	33.068160
753.033615	57590.833880	33.073178
753.925446	57693.093078	33.078196
754.789749	57776.837884	33.083213
755.266843	57874.333645	33.088231
756.306913	57961.583255	33.093248
757.297412	58054.885361	33.098266
757.583418	58148.652586	33.103284
758.597649	58239.983290	33.108301
759.570530	58339.586890	33.113319
759.916641	58423.630279	33.118336
760.822943	58508.814130	33.123354
761.377225	58611.573122	33.128372
762.431322	58702.804387	33.133389
763.409432	58792.421232	33.138407
764.050923	58885.749542	33.143424
764.601692	58975.174472	33.148442
765.039045	59064.680785	33.153460
766.201686	59158.972901	33.158477
766.915296	59264.690909	33.163495
767.611823	59344.941844	33.168512
768.564771	59443.534030	33.173530
769.141552	59550.901411	33.178548
770.302373	59629.150040	33.183565
770.497164	59717.247243	33.188583
771.422490	59816.408601	33.193600
772.607842	59913.845938	33.198618
772.851590	60008.513100	33.203636
773.648628	60097.390867	33.208653
774.510058	60198.658932	33.213671
775.134288	60295.052621	33.218688
776.266546	60380.302576	33.223706
776.596177	60473.774405	33.228724
777.172626	60559.763995	33.233741
778.287476	60648.530693	33.238759
778.773157	60741.428402	33.243776
779.563257	60825.783994	33.248794
780.174146	60929.588307	33.253812
781.194869	61011.838519	33.258829
781.724412	61105.851144	33.263847
782.342809	61207.528564	33.268864
783.401198	61295.141708	33.273882
783.858264	61399.813988	33.278900
784.623866	61495.880067	33.283917
785.571555	61609.249960	33.288935
786.345467	61706.733512	33.293952
787.629256	61800.592691	33.298970
788.099558	61898.554995	33.303988
789.041975	61982.169041	33.309005
789.113533	62102.223864	33.314023
790.232477	62208.270872	33.319040
791.379528	62307.464513	33.324058
792.171728	62413.050804	33.329076
792.716238	62502.084395	33.334093
793.429489	62617.964461	33.339111
794.557388	62722.461311	33.344128
794.984103	62829.106809	33.349146
795.730483	62928.523930	33.354164
796.786163	63037.591364	33.359181
797.859156	63133.932173	33.364199
798.321011	63243.694896	33.369216
799.517515	63344.075071	33.374234
800.504387	63447.900680	33.379252
801.013389	63555.220099	33.384269
801.600231	63651.911249	33.389287
802.586401	63754.161901	33.394304
803.267910	63872.667336	33.399322
804.389962	63970.529391	33.404340
805.181883	64075.932834	33.409357
805.957208	64187.499193	33.414375
806.688414	64296.331705	33.419392
807.826473	64390.115831	33.424410
808.459561	64498.217539	33.429428
809.153676	64597.567165	33.434445
810.571840	64701.096180	33.439463
811.467756	64815.292770	33.444480
812.364294	64917.524205	33.449498
812.911541	65009.795082	33.454516
813.680076	65117.416070	33.459533
814.316365	65212.718976	33.464551
815.058339	65318.540625	33.469568
816.174594	65420.416803	33.474586
816.809643	65525.945837	33.479604
817.542789	65621.975860	33.484621
818.605739	65712.041273	33.489639
819.500898	65830.408486	33.494656
820.067822	65926.288415	33.499674
820.938197	66038.873726	33.504692
821.490878	66142.221268	33.509709
822.573164	66249.456040	33.514727
823.118525	66347.708848	33.519744
824.240019	66444.789156	33.524762
825.242174	66560.813069	33.529780
825.614533	66661.303834	33.534797
826.398244	66766.580473	33.539815
827.442347	66874.273385	33.544832
828.433281	66979.727392	33.549850
829.116608	67076.346867	33.554868
829.793841	67178.292497	33.559885
830.708022	67278.472908	33.564903
831.467082	67394.469021	33.569920
832.291140	67484.774384	33.574938
833.035465	67581.322895	33.579956
833.270840	67678.546640	33.584973
834.421025	67779.749444	33.589991
835.385576	67894.696236	33.595008
835.882863	67986.168913	33.600026
836.638732	68105.157320	33.605044
837.481069	68203.161791	33.610061
838.782109	68307.458296	33.615079
839.376871	68427.195246	33.620096
839.906419	68533.145778	33.625114
840.651870	68638.239789	33.630132
841.526801	68756.940285	33.635149
842.508477	68864.328379	33.640167
842.939221	68996.213031	33.645184
844.061400	69100.756034	33.650202
844.930217	69223.562777	33.655220
845.759950	69342.133725	33.660237
846.847026	69445.664149	33.665255
847.758204	69559.752869	33.670272
848.615828	69671.501242	33.675290
849.720638	69791.107633	33.680308
850.298621	69908.853074	33.685325
851.174871	70020.720341	33.690343
852.241446	70144.285662	33.695360
853.183733	70244.289526	33.700378
853.942623	70367.688784	33.705396
855.306811	70482.432493	33.710413
855.962705	70597.211625	33.715431
856.383032	70710.938969	33.720448
857.643085	70819.355382	33.725466
858.452461	70931.540973	33.730484
859.156374	71044.744092	33.735501
860.486548	71158.482889	33.740519
860.993932	71277.125757	33.745536
862.192054	71391.418174	33.750554
862.776978	71501.804896	33.755572
863.964883	71624.534956	33.760589
864.810390	71726.763382	33.765607
865.678158	71847.150861	33.770624
866.503363	71948.788052	33.775642
867.225122	72063.284626	33.780660
868.055025	72177.004830	33.785677
869.250523	72290.199650	33.790695
869.947514	72407.462690	33.795712
870.711615	72524.880393	33.800730
871.442078	72631.449333	33.805748
872.302708	72746.003106	33.810765
873.292464	72857.320027	33.815783
874.606613	72979.276651	33.820800
875.363465	73097.495974	33.825818
876.073149	73211.315429	33.830836
876.712783	73333.873270	33.835853
877.824206	73445.756240	33.840871
878.685868	73565.177174	33.845888
879.593021	73680.348325	33.850906
880.590694	73780.204908	33.855924
881.171428	73905.966503	33.860941
882.208167	74019.155537	33.865959
882.747428	74137.717527	33.870976
883.880518	74262.152991	33.875994
884.827395	74376.066929	33.881012
885.476069	74490.914706	33.886029
886.401220	74605.365016	33.891047
887.620422	74724.633799	33.896064
888.233368	74838.829986	33.901082
889.128900	74957.162470	33.906100
889.889382	75072.970570	33.911117
891.033153	75170.554739	33.916135
891.382953	75287.694761	33.921152
892.379855	75399.958485	33.926170
893.455311	75510.981666	33.931188
894.297953	75624.803199	33.936205
895.099771	75741.279050	33.941223
895.758184	75861.628707	33.946240
896.689745	75980.112032	33.951258
897.690166	76089.692591	33.956276
898.603058	76212.043403	33.961293
899.955604	76319.403622	33.966311
900.362118	76442.518803	33.971328
901.060087	76558.077018	33.976346
902.372927	76680.912021	33.981364
903.201467	76801.125187	33.986381
903.957067	76922.528405	33.991399
904.743644	77043.813301	33.996416
905.035269	77158.854963	34.001434
906.282038	77298.817397	34.006452
907.200599	77433.105998	34.011469
908.271619	77560.049245	34.016487
909.042876	77676.804176	34.021504
909.820251	77816.969432	34.026522
911.032632	77954.495637	34.031540
911.589896	78083.181283	34.036557
912.843589	78212.822627	34.041575
913.850454	78356.501838	34.046592
914.651750	78477.208010	34.051610
915.866897	78614.851093	34.056628
916.780855	78758.876327	34.061645
918.192022	78872.939064	34.066663
918.628761	79013.417105	34.071680
919.669675	79143.172143	34.076698
920.581701	79270.490213	34.081716
921.246416	79396.035936	34.086733
922.365445	79519.027975	34.091751
923.374131	79661.750829	34.096768
924.534094	79782.773927	34.101786
925.622044	79913.855451	34.106804
926.767865	80040.430965	34.111821
927.545240	80159.285823	34.116839
928.388196	80288.266362	34.121856
929.069095	80409.848622	34.126874
929.896657	80540.859834	34.131892
931.225643	80675.201238	34.136909
932.248048	80798.746163	34.141927
933.185584	80929.285867	34.146944
934.120328	81058.116211	34.151962
935.035045	81181.920405	34.156980
935.850940	81315.280954	34.161997
936.840521	81431.092568	34.167015
937.829649	81566.289644	34.172032
938.967922	81692.658406	34.177050
939.518673	81819.094384	34.182068
940.424439	81944.537757	34.187085
941.467202	82083.732648	34.192103
942.303088	82202.080170	34.197120
943.380517	82342.398549	34.202138
944.353427	82478.324726	34.207156
945.120755	82601.968162	34.212173
945.960516	82729.351234	34.217191
946.741007	82865.334729	34.222208
948.007452	82997.885097	34.227226
948.824058	83120.065958	34.232244
949.880620	83263.547121	34.237261
950.638899	83392.022916	34.242279
951.621538	83522.744896	34.247296
952.301151	83648.801376	34.252314
953.820953	83778.933589	34.257332
954.131394	83899.904604	34.262349
955.482101	84032.395892	34.267367
956.529162	84151.149249	34.272384
957.238472	84283.133910	34.277402
958.211298	84397.046879	34.282420
959.257514	84529.550121	34.287437
960.363097	84655.430282	34.292455
961.172900	84776.301452	34.297472
961.773213	84899.968284	34.302490
962.887649	85041.675277	34.307508
963.594578	85189.212294	34.312525
964.016058	85308.055691	34.317543
965.085219	85447.566911	34.322560
966.470246	85594.049448	34.327578
967.540297	85743.407836	34.332596
968.452806	85881.855901	34.337613
969.193023	86024.716061	34.342631
970.629103	86155.062169	34.347648
971.215478	86300.659556	34.352666
971.984127	86446.812044	34.357684
972.968233	86596.745830	34.362701
974.510066	86739.864142	34.367719
975.655143	86876.290980	34.372736
976.138206	87019.361002	34.377754
977.525502	87166.205900	34.382772
978.215531	87309.435015	34.387789
978.901960	87449.560636	34.392807
980.300067	87592.008622	34.397824
980.971453	87750.639927	34.402842
982.246507	87899.533672	34.407860
983.112777	88040.837848	34.412877
984.382498	88187.541499	34.417895
985.008443	88338.718806	34.422912
986.190023	88480.026401	34.427930
987.334080	88632.822256	34.432948
988.047553	88783.798031	34.437965
989.155816	88921.862237	34.442983
990.571344	89079.028120	34.448000
991.483308	89235.133085	34.453018
992.713717	89375.524817	34.458036
993.346055	89529.013708	34.463053
994.331933	89679.938696	34.468071
995.388411	89824.136447	34.473088
996.224565	89966.949951	34.478106
997.334098	90112.027927	34.483124
998.109749	90270.618312	34.488141
999.498259	90415.806161	34.493159
1000.253152	90565.238244	34.498176
1001.059104	90707.502348	34.503194
1002.393855	90861.445720	34.508212
1003.226567	91012.071855	34.513229
1004.320828	91164.153326	34.518247
1005.467849	91314.693735	34.523264
1006.571485	91472.111084	34.528282
1007.349369	91625.461126	34.533300
1008.639285	91784.105678	34.538317
1009.483879	91917.902984	34.543335
1010.700398	92063.125668	34.548352
1011.686929	92219.817433	34.553370
1012.902820	92359.452181	34.558388
1014.328583	92511.564539	34.563405
1015.341931	92646.884924	34.568423
1016.073109	92789.753517	34.573440
1016.734471	92944.662073	34.578458
1018.012604	93083.187673	34.583476
1018.838543	93225.599840	34.588493
1019.819291	93361.296053	34.593511
1021.120662	93494.635814	34.598528
1021.543629	93636.149671	34.603546
1022.730315	93772.030927	34.608564
1023.594860	93921.487635	34.613581
1024.775871	94054.138849	34.618599
1025.658364	94199.512664	34.623616
1026.542574	94344.468605	34.628634
1027.749375	94488.309984	34.633652
1028.826648	94637.293200	34.638669
1029.533345	94782.836702	34.643687
1030.631677	94928.395621	34.648704
1031.467898	95077.862333	34.653722
1032.701749	95227.394264	34.658740
1033.485141	95387.581711	34.663757
1034.545169	95533.314235	34.668775
1035.787971	95677.447010	34.673792
1036.542603	95843.193336	34.678810
1037.915009	95995.407225	34.683828
1038.430029	96154.854698	34.688845
1039.506067	96309.448909	34.693863
1040.733685	96461.675048	34.698880
1041.362015	96632.997491	34.703898
1042.334869	96798.055511	34.708916
1043.708366	96964.078457	34.713933
1044.823112	97142.299534	34.718951
1046.179794	97289.996628	34.723968
1046.918354	97463.486672	34.728986
1048.027384	97618.373678	34.734004
1048.971128	97787.155670	34.739021
1050.346232	97950.496055	34.744039
1051.411842	98113.201180	34.749056
1052.610296	98287.396997	34.754074
1053.551549	98447.030117	34.759092
1054.380147	98606.808441	34.764109
1055.563312	98790.567900	34.769127
1056.689796	98947.613730	34.774144
1058.234729	99113.050550	34.779162
1059.151942	99277.851213	34.784180
1060.046805	99434.504652	34.789197
1061.029678	99613.254562	34.794215
1062.269370	99762.692839	34.799232
1063.359129	99941.275697	34.804250
1064.576740	100103.967093	34.809268
1066.051243	100272.881880	34.814285
1066.799375	100429.981471	34.819303
1068.052737	100575.364462	34.824320
1068.795035	100754.893639	34.829338
1069.974794	100915.148182	34.834356
1071.593994	101077.109637	34.839373
1072.561649	101236.574891	34.844391
1073.668869	101394.548405	34.849408
1074.291549	101556.363971	34.854426
1075.601987	101726.947457	34.859444
1076.739306	101871.606357	34.864461
1077.792898	102044.488446	34.869479
1078.732605	102198.891383	34.874496
1079.915280	102365.910174	34.879514
1081.199016	102530.669877	34.884532
1082.138044	102686.469843	34.889549
1082.825958	102848.104028	34.894567
1084.381701	103018.592387	34.899584
1085.252803	103189.505780	34.904602
1086.419224	103343.992667	34.909620
1087.531887	103506.298929	34.914637
1088.158320	103670.596636	34.919655
1089.256972	103834.301379	34.924672
1090.791626	103999.371407	34.929690
1091.728248	104151.488967	34.934708
1093.118409	104302.572587	34.939725
1093.949949	104453.414681	34.944743
1094.967032	104596.798287	34.949760
1095.866601	104761.172688	34.954778
1096.500323	104919.554068	34.959796
1097.906597	105069.434055	34.964813
1098.592700	105234.820506	34.969831
1099.757795	105402.022048	34.974848
1100.862453	105577.069958	34.979866
1102.364064	105730.627752	34.984884
1103.338158	105898.191316	34.989901
1104.468261	106065.807359	34.994919
1105.593112	106219.870143	34.999936
1106.692868	106390.180688	35.004954
1107.656240	106561.185480	35.009972
1108.676426	106721.733769	35.014989
1109.766984	106899.732473	35.020007
1110.875289	107072.771323	35.025024
1112.064004	107252.645853	35.030042
1112.909301	107426.019304	35.035060
1113.926514	107595.156788	35.040077
1114.997905	107776.307785	35.045095
1116.662394	107956.834292	35.050112
1117.260791	108131.860375	35.055130
1118.728888	108323.489780	35.060148
1120.053918	108492.634179	35.065165
1120.815834	108676.374488	35.070183
1122.186109	108861.669048	35.075200
1123.507226	109046.427004	35.080218
1124.428896	109212.467786	35.085236
1125.985997	109396.873621	35.090253
1126.858204	109586.206511	35.095271
1127.886851	109757.571917	35.100288
1129.123963	109931.162800	35.105306
1130.174980	110122.727860	35.110324
1131.306341	110298.924116	35.115341
1132.425203	110496.263332	35.120359
1134.055372	110676.111750	35.125376
1135.163886	110852.910375	35.130394
1136.005384	111041.850056	35.135412
1137.515600	111216.621933	35.140429
1138.655575	111399.759250	35.145447
1139.933764	111572.172322	35.150464
1141.192282	111750.841524	35.155482
1142.415860	111930.620427	35.160500
1143.721888	112112.327687	35.165517
1144.916599	112284.528978	35.170535
1145.857312	112451.406270	35.175552
1146.988126	112625.458118	35.180570
1147.893723	112794.232157	35.185588
1149.637594	112971.385651	35.190605
1150.489644	113154.843315	35.195623
1151.342551	113334.015072	35.200640
1152.428768	113505.757228	35.205658
1153.936390	113685.995023	35.210676
1155.028198	113858.625755	35.215693
1156.153935	114036.071452	35.220711
1157.585782	114208.409632	35.225728
1158.546210	114386.301441	35.230746
1159.641878	114571.047112	35.235764
1161.046881	114736.073900	35.240781
1161.722308	114921.610054	35.245799
1162.946629	115097.181033	35.250816
1164.208769	115280.115876	35.255834
1165.528012	115460.226997	35.260852
1166.827329	115633.340910	35.265869
1167.714006	115816.083513	35.270887
1168.513681	115979.777394	35.275904
1170.326216	116138.252713	35.280922
1171.040709	116309.799790	35.285940
1172.327626	116474.256682	35.290957
1173.110838	116653.290602	35.295975
1174.400506	116814.425434	35.300992
1175.435094	116992.102510	35.306010
1176.391247	117164.123021	35.311028
1177.685227	117337.321772	35.316045
1178.485099	117521.785938	35.321063
1179.832508	117702.968911	35.326080
1181.036377	117882.285293	35.331098
1182.124890	118073.454905	35.336116
1183.378518	118250.469406	35.341133
1184.515242	118437.701195	35.346151
1185.501081	118624.843367	35.351168
1186.818238	118812.454650	35.356186
1187.470589	119010.813201	35.361204
1189.442372	119201.647247	35.366221
1190.480701	119396.103954	35.371239
1191.542113	119582.680855	35.376256
1192.901010	119779.791151	35.381274
1193.679997	119980.798676	35.386292
1195.081358	120166.551411	35.391309
1196.070965	120367.781672	35.396327
1197.057001	120574.874000	35.401344
1198.569384	120771.724306	35.406362
1199.944059	120984.263287	35.411380
1201.522878	121171.286929	35.416397
1202.363130	121378.431719	35.421415
1203.712165	121575.222852	35.426432
1205.583786	121775.789519	35.431450
1206.600890	121966.012807	35.436468
1207.862710	122170.431838	35.441485
1209.071129	122374.149895	35.446503
1210.197905	122556.240096	35.451520
1211.686364	122754.283854	35.456538
1212.684275	122956.731235	35.461556
1213.885750	123147.311911	35.466573
1215.292136	123344.838655	35.471591
1215.989373	123538.811152	35.476608
1217.478763	123746.272665	35.481626
1218.475054	123949.448435	35.486644
1220.124992	124144.238864	35.491661
1221.217951	124342.923286	35.496679
1222.666175	124548.505142	35.501696
1223.785844	124747.136628	35.506714
1224.879456	124946.711960	35.511732
1225.998935	125150.483439	35.516749
1227.301819	125347.033977	35.521767
1228.739845	125555.908342	35.526784
1229.944892	125740.855196	35.531802
1231.269768	125954.988894	35.536820
1232.223498	126153.983072	35.541837
1233.361767	126360.269622	35.546855
1234.425512	126562.065027	35.551872
1236.239657	126760.800580	35.556890
1237.227272	126966.923445	35.561908
1238.227684	127172.842339	35.566925
1239.924012	127375.012108	35.571943
1241.235135	127581.962798	35.576960
1242.568654	127781.133721	35.581978
1243.670583	127985.391401	35.586996
1244.549241	128178.951506	35.592013
1245.967573	128393.514547	35.597031
1247.097854	128596.603521	35.602048
1248.894612	128795.097747	35.607066
1250.383557	129000.137156	35.612084
1251.330443	129178.618282	35.617101
1252.093906	129363.041356	35.622119
1253.501076	129553.162785	35.627136
1255.055700	129733.175145	35.632154
1256.450182	129927.639476	35.637172
1257.213360	130109.236425	35.642189
1258.496962	130304.379602	35.647207
1259.572056	130493.250336	35.652224
1260.796397	130689.077007	35.657242
1262.092403	130890.438088	35.662260
1263.449284	131082.350527	35.667277
1264.556445	131277.703373	35.672295
1265.563509	131479.670715	35.677312
1267.148948	131676.993317	35.682330
1268.640757	131889.088168	35.687348
1269.772219	132084.516969	35.692365
1270.954286	132285.445571	35.697383
1271.978540	132486.666261	35.702400
1273.509863	132690.371617	35.707418
1274.824483	132902.448361	35.712436
1276.245628	133108.862920	35.717453
1277.372115	133322.087748	35.722471
1278.702789	133525.346192	35.727488
1280.112486	133731.917717	35.732506
1281.237371	133930.756387	35.737524
1282.299729	134151.405648	35.742541
1283.526988	134364.518186	35.747559
1284.455366	134579.949899	35.752576
1285.761587	134786.618633	35.757594
1287.647760	135006.699020	35.762612
1288.905276	135225.203884	35.767629
1290.449331	135434.287418	35.772647
1291.603659	135656.122471	35.777664
1292.901973	135869.675132	35.782682
1294.184981	136084.170226	35.787700
1295.540911	136302.144588	35.792717
1297.135748	136525.095059	35.797735
1298.504627	136734.427703	35.802752
1300.324731	136940.188254	35.807770
1301.261419	137162.419995	35.812788
1302.362931	137375.147553	35.817805
1304.073035	137582.400227	35.822823
1305.480701	137787.416943	35.827840
1306.556888	137994.910278	35.832858
1308.272301	138212.279013	35.837876
1309.289975	138418.070203	35.842893
1310.811294	138620.483963	35.847911
1312.109849	138840.293961	35.852928
1313.448261	139048.829599	35.857946
1314.480999	139250.370760	35.862964
1316.127732	139467.552999	35.867981
1317.340970	139662.709672	35.872999
1318.638825	139887.461303	35.878016
1319.984768	140093.512975	35.883034
1321.839776	140306.072383	35.888052
1322.655002	140515.419722	35.893069
1324.011776	140727.411752	35.898087
1325.027997	140935.434982	35.903104
1326.766251	141135.020768	35.908122
1328.263116	141358.669392	35.913140
1329.290826	141578.623214	35.918157
1330.306317	141781.281832	35.923175
1331.610819	141983.464549	35.928192
1332.623705	142198.676958	35.933210
1334.171257	142438.110588	35.938228
1335.390517	142645.576298	35.943245
1337.024320	142858.879530	35.948263
1337.725528	143062.290661	35.953280
1339.372637	143276.570859	35.958298
1340.852827	143485.154181	35.963316
1341.901268	143694.783218	35.968333
1343.100901	143897.282092	35.973351
1344.262643	144116.185518	35.978368
1345.567066	144314.430614	35.983386
1347.122929	144531.015007	35.988404
1348.073852	144740.790596	35.993421
1349.395257	144960.218452	35.998439
1350.615657	145187.138694	36.003456
1351.841080	145402.737789	36.008474
1353.246933	145642.703919	36.013492
1354.450435	145866.888319	36.018509
1355.968430	146084.906787	36.023527
1357.209809	146324.622622	36.028544
1358.340271	146557.211106	36.033562
1359.960246	146789.127467	36.038580
1360.974648	147021.875820	36.043597
1362.554126	147253.483278	36.048615
1364.196924	147492.773589	36.053632
1365.161665	147728.477555	36.058650
1366.525738	147974.312349	36.063668
1367.633733	148217.954439	36.068685
1369.397433	148466.051754	36.073703
1370.982244	148722.441328	36.078720
1372.606408	148964.292505	36.083738
1373.667111	149193.692248	36.088756
1374.960166	149445.244141	36.093773
1376.845718	149686.105681	36.098791
1378.046890	149928.623994	36.103808
1379.154393	150176.413071	36.108826
1381.053865	150422.670355	36.113844
1381.999988	150669.116058	36.118861
1383.655028	150907.531200	36.123879
1385.143459	151159.783986	36.128896
1386.292038	151406.442491	36.133914
1387.791872	151655.738164	36.138932
1389.214273	151906.240286	36.143949
1390.629752	152146.932369	36.148967
1391.946438	152406.580081	36.153984
1393.403265	152656.318559	36.159002
1394.832813	152907.687237	36.164020
1396.345027	153150.018696	36.169037
1398.087812	153397.900468	36.174055
1399.405620	153659.724458	36.179072
1400.811412	153898.432576	36.184090
1402.388026	154139.069858	36.189108
1403.896786	154393.174654	36.194125
1405.432946	154640.726032	36.199143
1406.581958	154888.085185	36.204160
1408.177037	155131.503783	36.209178
1409.764405	155375.305442	36.214196
1410.901325	155618.493124	36.219213
1412.507209	155859.755008	36.224231
1413.818194	156111.765593	36.229248
1415.388676	156342.511172	36.234266
1416.774095	156591.224238	36.239284
1418.185021	156847.500432	36.244301
1419.602334	157088.009768	36.249319
1421.175287	157338.029555	36.254336
1422.523889	157571.340903	36.259354
1424.212638	157818.881753	36.264372
1425.483691	158057.932553	36.269389
1427.159749	158296.895513	36.274407
1428.470040	158545.780770	36.279424
1429.817585	158781.750221	36.284442
1431.367821	159022.271829	36.289460
1432.528478	159265.635619	36.294477
1433.814958	159489.886918	36.299495
1435.557738	159723.881122	36.304512
1436.832328	159942.676913	36.309530
1438.550371	160164.197060	36.314548
1439.553089	160396.709997	36.319565
1441.075215	160620.852305	36.324583
1442.467020	160856.771924	36.329600
1443.947225	161092.462761	36.334618
1445.618418	161326.004400	36.339636
1446.658307	161557.893695	36.344653
1448.182201	161793.262892	36.349671
1449.644766	162032.895652	36.354688
1451.177714	162280.783301	36.359706
1452.516129	162517.707679	36.364724
1453.369741	162758.784207	36.369741
1454.851457	163002.835752	36.374759
1456.467580	163257.150979	36.379776
1457.951072	163503.730626	36.384794
1459.240057	163748.322949	36.389812
1460.666681	164019.112299	36.394829
1462.274452	164250.617570	36.399847
1463.630454	164499.912477	36.404864
1464.985503	164771.376286	36.409882
1466.992951	165020.571161	36.414900
1468.138293	165282.560245	36.419917
1469.725690	165541.599046	36.424935
1471.306491	165793.186991	36.429952
1472.664277	166053.266695	36.434970
1474.386705	166311.500082	36.439988
1475.441529	166580.199421	36.445005
1477.164063	166835.260572	36.450023
1478.650857	167100.567764	36.455040
1480.036193	167368.545478	36.460058
1481.564935	167624.947609	36.465076
1482.680063	167895.013810	36.470093
1484.281499	168158.973861	36.475111
1486.330961	168434.838055	36.480128
1487.516827	168697.011369	36.485146
1489.315630	168963.013111	36.490164
1490.416270	169238.038510	36.495181
1492.023726	169498.713962	36.500199
1493.552555	169772.810948	36.505216
1494.785140	170043.730210	36.510234
1496.897048	170313.827182	36.515252
1498.260334	170587.432512	36.520269
1499.947028	170852.595221	36.525287
1501.275906	171115.376954	36.530304
1503.238623	171386.364583	36.535322
1504.757345	171646.413879	36.540340
1506.037676	171919.351363	36.545357
1507.887882	172189.749980	36.550375
1509.039624	172447.675441	36.555392
1510.936132	172707.377163	36.560410
1512.273367	172975.154198	36.565428
1513.575928	173239.928193	36.570445
1515.302595	173505.131921	36.575463
1516.957073	173776.036510	36.580480
1518.146480	174040.602342	36.585498
1519.812543	174303.037375	36.590516
1521.350962	174580.845186	36.595533
1522.565633	174839.314642	36.600551
1524.594285	175105.555764	36.605568
1526.151612	175372.773096	36.610586
1527.367060	175640.095603	36.615604
1528.816499	175918.074288	36.620621
1530.359543	176191.099620	36.625639
1532.108591	176455.382546	36.630656
1533.436445	176725.446501	36.635674
1535.364178	176973.626951	36.640692
1536.119657	177230.448771	36.645709
1537.864767	177472.564008	36.650727
1539.122709	177722.705458	36.655744
1540.588581	177992.142312	36.660762
1542.224514	178242.454688	36.665780
1543.784819	178502.735359	36.670797
1545.362496	178767.077665	36.675815
1546.882738	179021.372373	36.680832
1548.017631	179291.119016	36.685850
1549.358430	179560.529482	36.690868
1550.928257	179827.746115	36.695885
1551.829064	180109.011611	36.700903
1553.815431	180391.555759	36.705920
1555.538352	180673.227694	36.710938
1556.876255	180954.579784	36.715956
1558.469283	181241.023214	36.720973
1559.664744	181532.406193	36.725991
1561.929299	181815.444537	36.731008
1563.027937	182112.228897	36.736026
1564.669448	182410.402331	36.741044
1566.579047	182695.098961	36.746061
1567.955394	182979.879894	36.751079
1569.843636	183274.614001	36.756096
1571.326028	183574.441460	36.761114
1573.058010	183848.247849	36.766132
1574.935170	184148.447056	36.771149
1576.303338	184439.380036	36.776167
1577.757464	184731.214773	36.781184
1579.307229	185028.724776	36.786202
1581.072419	185315.991488	36.791220
1582.493685	185691.295681	36.796237
1584.200595	185996.505269	36.801255
1585.831061	186278.385703	36.806272
1587.648211	186577.356896	36.811290
1589.710578	186875.909567	36.816308
1590.753239	187171.676315	36.821325
1592.562630	187458.256211	36.826343
1594.460700	187751.960308	36.831360
1595.838049	188064.059935	36.836378
1597.438238	188357.151885	36.841396
1599.036815	188653.496055	36.846413
1600.708206	188951.201217	36.851431
1602.424110	189246.106195	36.856448
1603.899324	189542.751419	36.861466
1605.782605	189824.906246	36.866484
1606.814553	190130.233023	36.871501
1608.627827	190422.738167	36.876519
1610.259531	190729.750673	36.881536
1611.727777	191037.449969	36.886554
1613.407730	191335.947345	36.891572
1615.341484	191624.677323	36.896589
1617.188596	191925.969460	36.901607
1618.928010	192222.021251	36.906624
1620.287478	192513.383274	36.911642
1622.084465	192811.154713	36.916660
1623.842507	193113.581312	36.921677
1625.488452	193402.741488	36.926695
1627.194996	193697.887467	36.931712
1628.688795	194000.027302	36.936730
1630.781588	194288.255894	36.941748
1632.354351	194579.513035	36.946765
1634.012057	194876.777610	36.951783
1635.133694	195146.185342	36.956800
1637.030180	195460.356479	36.961818
1639.068048	195741.382813	36.966836
1640.682102	196034.694133	36.971853
1642.184011	196327.744204	36.976871
1644.029232	196584.239155	36.981888
1645.084278	196853.762231	36.986906
1646.946608	197125.674235	36.991924
1648.566952	197397.497611	36.996941
1650.119939	197675.606258	37.001959
1651.490693	197937.131193	37.006976
1653.123284	198215.152187	37.011994
1654.953042	198491.593325	37.017012
1656.617231	198777.611991	37.022029
1657.912940	199057.414573	37.027047
1659.818649	199335.953703	37.032064
1661.049958	199623.896016	37.037082
1662.779444	199912.649959	37.042100
1664.430908	200202.712139	37.047117
1665.654040	200496.296566	37.052135
1667.508058	200786.988540	37.057152
1669.119571	201091.080565	37.062170
1670.664175	201388.045559	37.067188
1672.456484	201696.631987	37.072205
1674.187413	202015.059302	37.077223
1675.900837	202298.688580	37.082240
1677.448286	202615.519936	37.087258
1679.134706	202927.351204	37.092276
1680.639518	203232.505145	37.097293
1682.408834	203542.012849	37.102311
1684.444019	203853.587877	37.107328
1685.971563	204178.477666	37.112346
1687.607637	204492.859682	37.117364
1689.373621	204805.723108	37.122381
1690.778305	205126.340622	37.127399
1692.630966	205440.969670	37.132416
1694.040877	205761.968407	37.137434
1695.578302	206094.861662	37.142452
1697.539722	206422.329056	37.147469
1699.268097	206753.262824	37.152487
1700.899568	207080.122361	37.157504
1702.786802	207403.004870	37.162522
1704.583092	207741.804428	37.167540
1706.467489	208060.522189	37.172557
1708.035504	208391.102378	37.177575
1709.711425	208716.763309	37.182592
1711.149305	209051.962744	37.187610
1713.088988	209385.305866	37.192628
1714.668422	209724.218321	37.197645
1716.381704	210058.080401	37.202663
1718.552539	210392.811220	37.207680
1720.137767	210733.172038	37.212698
1722.035262	211060.960495	37.217716
1723.580102	211393.758195	37.222733
1725.213357	211723.976680	37.227751
1727.258568	212057.458925	37.232768
1729.098015	212405.758609	37.237786
1730.481148	212732.613236	37.242804
1732.512269	213055.581648	37.247821
1733.973864	213400.232599	37.252839
1735.450571	213739.267318	37.257856
1737.464151	214086.652375	37.262874
1739.167554	214428.218043	37.267892
1741.095408	214756.081684	37.272909
1742.986523	215097.085097	37.277927
1744.657009	215438.174134	37.282944
1746.847081	215768.334717	37.287962
1748.333605	216104.346916	37.292980
1750.221329	216433.310528	37.297997
1751.786294	216775.103026	37.303015
1753.814366	217110.700962	37.308032
1755.218386	217444.923354	37.313050
1756.954375	217769.542140	37.318068
1759.012170	218082.475763	37.323085
1760.351039	218406.471160	37.328103
1762.353555	218722.640080	37.333120
1764.024325	219027.734137	37.338138
1765.255415	219353.423555	37.343156
1767.262929	219679.118648	37.348173
1769.048713	219998.853240	37.353191
1770.738220	220330.873168	37.358208
1772.642150	220652.926703	37.363226
1774.570222	220972.029711	37.368244
1776.299904	221301.020638	37.373261
1777.606097	221624.209606	37.378279
1779.532038	221948.546485	37.383296
1781.169822	222289.746030	37.388314
1782.409391	222629.356710	37.393332
1784.147776	222964.392888	37.398349
1786.096167	223320.329226	37.403367
1787.660403	223664.233397	37.408384
1789.528246	224019.572750	37.413402
1791.348843	224372.379128	37.418420
1793.428564	224720.775482	37.423437
1795.206244	225080.549340	37.428455
1797.218451	225429.464364	37.433472
1799.363717	225782.372408	37.438490
1801.153667	226139.299075	37.443508
1802.974926	226475.922954	37.448525
1804.896738	226831.939783	37.453543
1806.646531	227185.595498	37.458560
1808.634309	227542.211596	37.463578
1810.160383	227894.682796	37.468596
1811.817321	228251.223493	37.473613
1813.817927	228603.010570	37.478631
1815.625929	228968.139405	37.483648
1817.656669	229321.877662	37.488666
1819.242684	229681.477504	37.493684
1821.675408	230033.856992	37.498701
1823.178618	230406.832012	37.503719
1824.993134	230756.970762	37.508736
1827.203575	231122.594630	37.513754
1828.495134	231473.246733	37.518772
1830.912625	231834.773184	37.523789
1832.815357	232207.989574	37.528807
1834.712519	232565.633996	37.533824
1836.627400	232913.774357	37.538842
1838.614119	233280.956166	37.543860
1840.173991	233640.583343	37.548877
1842.068141	233990.606100	37.553895
1844.295391	234343.320087	37.558912
1845.908929	234705.326010	37.563930
1847.718487	235067.580400	37.568948
1849.892383	235422.715217	37.573965
1851.921284	235780.488996	37.578983
1853.608341	236134.124322	37.584000
1855.569903	236474.760477	37.589018
1857.081717	236844.934950	37.594036
1858.754175	237204.566788	37.599053
1860.681478	237560.322425	37.604071
1862.591373	237916.842514	37.609088
1864.592138	238281.985201	37.614106
1866.332506	238644.475436	37.619124
1868.230760	238998.074713	37.624141
1870.541906	239359.738074	37.629159
1872.063724	239714.055883	37.634176
1874.033382	240076.889525	37.639194
1875.638915	240433.454226	37.644212
1877.897019	240790.475218	37.649229
1879.609237	241152.128335	37.654247
1881.166606	241509.740650	37.659264
1883.306923	241851.282608	37.664282
1885.526929	242194.056380	37.669300
1886.974720	242525.773105	37.674317
1888.952844	242867.694649	37.679335
1890.869452	243212.699088	37.684352
1892.468053	243545.025837	37.689370
1894.370822	243895.772487	37.694388
1896.064928	244240.886364	37.699405
1897.565888	244589.459306	37.704423
1899.655035	244933.163895	37.709440
1901.073700	245296.609226	37.714458
1902.950305	245661.887464	37.719476
1904.815657	246018.631472	37.724493
1906.591972	246385.575251	37.729511
1908.656501	246753.692564	37.734528
1910.720126	247128.413982	37.739546
1912.071714	247509.647506	37.744564
1914.293933	247882.386588	37.749581
1915.857890	248260.689426	37.754599
1917.764443	248642.799016	37.759616
1919.745513	249031.322901	37.764634
1921.508013	249420.591372	37.769652
1923.599726	249808.511922	37.774669
1925.709509	250191.424516	37.779687
1927.494405	250592.143115	37.784704
1929.539347	250982.659218	37.789722
1931.256577	251376.324677	37.794740
1933.591713	251773.677348	37.799757
1935.460467	252178.239884	37.804775
1937.390984	252570.700436	37.809792
1939.968438	252962.804716	37.814810
1941.688504	253362.662598	37.819828
1943.569171	253755.661231	37.824845
1945.947575	254157.471430	37.829863
1947.657442	254552.806124	37.834880
1950.029654	254946.384974	37.839898
1952.066431	255338.643513	37.844916
1953.916403	255734.537120	37.849933
1956.006173	256134.024399	37.854951
1958.132254	256531.752118	37.859968
1960.281679	256918.247743	37.864986
1961.741772	257316.001061	37.870004
1964.251001	257703.200050	37.875021
1966.458545	258094.077358	37.880039
1967.894498	258503.083230	37.885056
1970.318172	258885.389599	37.890074
1972.190685	259286.678969	37.895092
1973.957558	259667.841003	37.900109
1976.278778	260070.403754	37.905127
1978.277078	260466.817991	37.910144
1980.166230	260848.388863	37.915162
1982.104649	261247.197403	37.920180
1984.309615	261639.358843	37.925197
1986.208959	262030.474537	37.930215
1988.317924	262436.821334	37.935232
1990.565154	262822.342638	37.940250
1992.404167	263215.495530	37.945268
1994.185657	263598.496178	37.950285
1996.506614	263980.522063	37.955303
1998.379496	264386.822238	37.960320
2000.842250	264763.489226	37.965338
2002.807632	265159.790003	37.970356
2004.703588	265546.423073	37.975373
2006.730994	265923.712686	37.980391
2008.561914	266321.731689	37.985408
2010.882440	266690.743317	37.990426
2012.652845	267079.447400	37.995444
2014.660578	267457.394612	38.000461
2016.913457	267816.303945	38.005479
2018.422458	268193.665942	38.010496
2020.764762	268554.793565	38.015514
2022.312799	268920.234773	38.020532
2024.301828	269283.116546	38.025549
2026.304777	269640.229382	38.030567
2028.045704	270023.414641	38.035584
2030.214767	270397.819874	38.040602
2032.207232	270777.762478	38.045620
2034.332324	271153.822295	38.050637
2035.936866	271534.355724	38.055655
2038.121099	271916.625421	38.060672
2039.890520	272294.031290	38.065690
2041.776274	272696.255682	38.070708
2044.213583	273083.102916	38.075725
2045.490399	273486.003006	38.080743
2047.838669	273886.447835	38.085760
2049.767928	274280.454777	38.090778
2052.091773	274684.074185	38.095796
2053.826992	275092.583630	38.100813
2055.715585	275493.752923	38.105831
2057.893452	275917.756879	38.110848
2060.051379	276325.533692	38.115866
2062.263089	276748.486729	38.120884
2064.689972	277161.067789	38.125901
2066.845826	277572.292331	38.130919
2068.636242	277995.990255	38.135936
2070.564376	278409.556981	38.140954
2072.655538	278833.660364	38.145972
2074.477319	279257.397213	38.150989
2076.807034	279675.846266	38.156007
2079.098545	280101.638044	38.161024
2081.478577	280533.203503	38.166042
2083.240637	280958.616090	38.171060
2085.419829	281390.588858	38.176077
2087.666596	281821.405752	38.181095
2089.374811	282242.299096	38.186112
2091.466468	282674.938116	38.191130
2093.819327	283112.790131	38.196148
2095.905232	283544.942256	38.201165
2098.196178	283974.951984	38.206183
2100.303018	284406.384483	38.211200
2102.541050	284835.609956	38.216218
2104.642433	285274.604991	38.221236
2106.494875	285705.967534	38.226253
2108.961035	286134.971365	38.231271
2110.545893	286581.326383	38.236288
2112.675810	287016.166627	38.241306
2115.109910	287457.177477	38.246324
2117.294115	287902.388728	38.251341
2119.837476	288335.885947	38.256359
2121.604412	288777.830161	38.261376
2123.978159	289216.197781	38.266394
2126.194206	289658.014873	38.271412
2128.101424	290085.734400	38.276429
2130.543091	290522.838194	38.281447
2132.383000	290971.179580	38.286464
2134.454836	291404.729572	38.291482
2136.833021	291838.457102	38.296500
2138.854125	292286.278167	38.301517
2141.179819	292720.947076	38.306535
2142.903461	293159.591683	38.311552
2145.171793	293598.452549	38.316570
2147.766533	294042.362388	38.321588
2149.653773	294482.850493	38.326605
2152.285709	294916.465324	38.331623
2154.028298	295353.313516	38.336640
2156.113835	295790.663326	38.341658
2158.057330	296216.505701	38.346676
2160.113575	296617.878393	38.351693
2162.325125	297028.109797	38.356711
2164.091731	297455.163858	38.361728
2166.288804	297869.377334	38.366746
2168.361187	298291.401230	38.371764
2170.275262	298725.784937	38.376781
2172.415583	299155.966365	38.381799
2174.586087	299580.300727	38.386816
2176.400449	300028.373331	38.391834
2178.832155	300469.008975	38.396852
2180.996667	300911.104472	38.401869
2182.735813	301354.989143	38.406887
2185.307565	301807.498010	38.411904
2187.258453	302261.572531	38.416922
2189.613405	302706.872740	38.421940
2191.432597	303159.005470	38.426957
2193.713797	303622.662962	38.431975
2196.019855	304092.430165	38.436992
2198.275765	304543.670230	38.442010
2200.160118	305015.246534	38.447028
2202.235946	305481.762487	38.452045
2204.845771	305951.642822	38.457063
2206.716733	306433.716973	38.462080
2209.346849	306918.485288	38.467098
2211.578969	307380.897866	38.472116
2213.681203	307870.968412	38.477133
2215.999634	308348.080515	38.482151
2218.315319	308819.502755	38.487168
2220.375763	309296.468293	38.492186
2222.901736	309782.392265	38.497204
2225.031736	310264.769095	38.502221
2227.434399	310746.666936	38.507239
2229.653439	311232.674991	38.512256
2231.787291	311724.808175	38.517274
2234.110492	312211.018306	38.522292
2236.359163	312701.930413	38.527309
2238.620182	313185.932044	38.532327
2240.828468	313674.708271	38.537344
2243.066630	314169.514966	38.542362
2245.758233	314660.387742	38.547380
2247.770742	315162.959652	38.552397
2250.357231	315652.746859	38.557415
2252.276800	316139.790695	38.562432
2254.914154	316632.198630	38.567450
2257.520020	317128.844154	38.572468
2259.310870	317622.667818	38.577485
2261.887048	318113.952260	38.582503
2264.308754	318607.209396	38.587520
2266.619162	319097.382410	38.592538
2268.939156	319587.472263	38.597556
2271.171442	320083.076896	38.602573
2273.684977	320553.814240	38.607591
2276.340477	321051.219285	38.612608
2278.498147	321542.707829	38.617626
2280.829600	322015.817374	38.622644
2282.972558	322504.404275	38.627661
2285.175993	322987.571272	38.632679
2287.830091	323476.878823	38.637696
2289.986308	323962.477791	38.642714
2292.551084	324442.424964	38.647732
2294.825631	324936.291068	38.652749
2296.711805	325404.179369	38.657767
2299.341781	325896.658847	38.662784
2301.490319	326383.194413	38.667802
2304.077327	326856.208359	38.672820
2306.322284	327344.670843	38.677837
2308.637872	327804.827212	38.682855
2311.021819	328265.449606	38.687872
2312.932149	328725.607935	38.692890
2315.309184	329167.725561	38.697908
2317.054877	329624.600946	38.702925
2319.668075	330071.643969	38.707943
2321.649889	330536.539352	38.712960
2323.835718	330997.490358	38.717978
2326.340870	331464.423720	38.722996
2328.464500	331940.873598	38.728013
2330.656992	332403.810780	38.733031
2332.902555	332877.033456	38.738048
2335.244154	333362.868327	38.743066
2337.684770	333835.465017	38.748084
2339.872106	334329.708134	38.753101
2341.934554	334812.473103	38.758119
2344.183983	335303.345175	38.763136
2346.563399	335793.023560	38.768154
2348.620132	336290.837582	38.773172
2351.013400	336805.282631	38.778189
2353.195449	337312.600529	38.783207
2355.608006	337821.042060	38.788224
2357.827936	338339.246471	38.793242
2360.347671	338854.555762	38.798260
2362.850371	339364.635407	38.803277
2365.167082	339891.958476	38.808295
2367.873028	340412.364860	38.813312
2369.778868	340929.921328	38.818330
2372.583614	341454.507043	38.823348
2374.457112	341987.523848	38.828365
2377.265304	342514.020605	38.833383
2380.115445	343041.086112	38.838400
2382.169324	343576.129899	38.843418
2384.603681	344097.588886	38.848436
2387.057487	344632.147886	38.853453
2389.557390	345157.232248	38.858471
2392.148587	345702.758890	38.863488
2394.698703	346230.557515	38.868506
2397.245531	346761.543499	38.873524
2399.796419	347290.542520	38.878541
2401.957485	347827.632403	38.883559
2404.537920	348357.395910	38.888576
2406.738273	348899.990069	38.893594
2409.679184	349423.036654	38.898612
2411.866574	349952.303479	38.903629
2414.058247	350487.342055	38.908647
2416.536555	351029.553120	38.913664
2419.205185	351571.623904	38.918682
2421.773349	352100.897492	38.923700
2423.990818	352641.727734	38.928717
2426.601124	353170.824905	38.933735
2429.372442	353709.522129	38.938752
2431.443512	354239.928098	38.943770
2433.955583	354777.430748	38.948788
2436.685495	355314.763361	38.953805
2438.894280	355848.669809	38.958823
2441.316615	356389.251603	38.963840
2443.321694	356930.725791	38.968858
2446.326272	357464.429234	38.973876
2448.491814	358013.210710	38.978893
2450.772245	358554.765323	38.983911
2453.203634	359090.557977	38.988928
2455.545283	359638.801034	38.993946
2458.798997	360177.665022	38.998964
2461.327229	360717.393252	39.003981
2463.508095	361246.292443	39.008999
2466.088334	361792.101680	39.014016
2468.308946	362342.063145	39.019034
2470.888275	362851.735541	39.024052
2473.117326	363380.614539	39.029069
2475.448670	363885.061496	39.034087
2477.987134	364403.938704	39.039104
2480.204622	364921.488352	39.044122
2482.952665	365425.716792	39.049140
2484.893864	365947.853089	39.054157
2487.496660	366469.090858	39.059175
2489.629188	366995.739808	39.064192
2492.122634	367529.722225	39.069210
2494.204861	368051.443433	39.074228
2497.204563	368600.936408	39.079245
2499.357540	369151.007276	39.084263
2501.791226	369681.816436	39.089280
2504.186052	370235.857219	39.094298
2506.752789	370778.686021	39.099316
2509.303858	371333.871497	39.104333
2511.548640	371888.561710	39.109351
2514.350496	372451.540109	39.114368
2516.753913	373009.527446	39.119386
2519.342824	373573.326966	39.124404
2522.207479	374127.875102	39.129421
2524.575164	374695.182313	39.134439
2527.145574	375264.168681	39.139456
2529.834430	375830.185872	39.144474
2532.472407	376396.705792	39.149492
2535.035296	376961.908218	39.154509
2537.808529	377528.307064	39.159527
2540.502752	378097.771325	39.164544
2542.995276	378679.211060	39.169562
2545.643282	379243.389120	39.174580
2548.446555	379823.665842	39.179597
2550.739843	380396.689376	39.184615
2553.529987	380973.067332	39.189632
2556.372067	381544.409460	39.194650
2558.733473	382113.939958	39.199668
2561.454285	382696.698332	39.204685
2564.132317	383268.078686	39.209703
2566.774258	383841.554004	39.214720
2569.233047	384426.238851	39.219738
2571.551851	384995.560128	39.224756
2574.648932	385577.256996	39.229773
2577.081095	386157.373132	39.234791
2579.931398	386738.144878	39.239808
2582.250445	387319.391438	39.244826
2584.789496	387892.132632	39.249844
2587.706776	388477.816572	39.254861
2590.059766	389059.827518	39.259879
2592.944291	389643.615318	39.264896
2595.336039	390229.694470	39.269914
2597.907479	390811.680541	39.274932
2600.678161	391404.204590	39.279949
2602.693668	391989.186472	39.284967
2606.016248	392572.380199	39.289984
2608.400870	393166.136888	39.295002
2611.142770	393759.367408	39.300020
2613.670822	394348.009404	39.305037
2616.463534	394932.494610	39.310055
2618.945972	395526.734532	39.315072
2621.066674	396118.383622	39.320090
2623.789307	396695.951290	39.325108
2626.608687	397279.412696	39.330125
2629.350804	397890.106654	39.335143
2632.066786	398483.830698	39.340160
2634.206030	399065.582317	39.345178
2636.943685	399664.638649	39.350196
2639.494411	400260.671720	39.355213
2642.034665	400859.525574	39.360231
2644.653459	401446.963274	39.365248
2647.057091	402037.557643	39.370266
2650.031776	402609.270353	39.375284
2652.691906	403168.871311	39.380301
2654.558536	403746.903315	39.385319
2657.796273	404319.695922	39.390336
2660.293115	404894.968418	39.395354
2662.733945	405478.331913	39.400372
2665.595206	406063.335053	39.405389
2667.938116	406657.208915	39.410407
2670.826315	407233.574670	39.415424
2673.158225	407821.852999	39.420442
2675.428650	408415.286442	39.425460
2678.125062	409016.631767	39.430477
2680.204137	409626.253824	39.435495
2682.984805	410242.124182	39.440512
2685.979274	410862.143016	39.445530
2688.658676	411477.893159	39.450548
2691.389394	412104.646572	39.455565
2693.845433	412731.273028	39.460583
2696.381232	413341.478404	39.465600
2699.430693	413975.058136	39.470618
2701.734280	414611.214433	39.475636
2704.573313	415251.466443	39.480653
2707.769754	415894.779356	39.485671
2710.914066	416532.365348	39.490688
2713.479796	417167.291346	39.495706
2716.206123	417808.798685	39.500724
2718.685267	418447.998603	39.505741
2721.306456	419102.278391	39.510759
2724.478560	419748.916207	39.515776
2727.395637	420401.136566	39.520794
2729.621007	421045.353487	39.525812
2732.738324	421702.153845	39.530829
2735.826551	422357.420795	39.535847
2738.328540	423002.645604	39.540864
2741.177255	423651.588019	39.545882
2743.711440	424323.614814	39.550900
2746.687301	424967.287541	39.555917
2749.802363	425631.798405	39.560935
2752.885121	426283.855588	39.565952
2755.659686	426941.096363	39.570970
2758.510754	427594.562685	39.575988
2761.263627	428241.602956	39.581005
2763.600485	428890.911420	39.586023
2766.742533	429548.868036	39.591040
2769.973677	430209.113933	39.596058
2772.709702	430865.927548	39.601076
2775.544800	431505.923461	39.606093
2778.396904	432159.693532	39.611111
2781.364907	432809.835257	39.616128
2784.262645	433471.387770	39.621146
2787.011718	434099.081755	39.626164
2790.068111	434744.444887	39.631181
2793.343279	435392.935737	39.636199
2795.762315	436035.727490	39.641216
2798.714327	436682.001889	39.646234
2801.401704	437324.253564	39.651252
2804.324653	437966.396182	39.656269
2806.544233	438609.435432	39.661287
2809.565314	439242.829231	39.666304
2812.792208	439890.567979	39.671322
2815.325005	440540.565251	39.676340
2818.208656	441185.433364	39.681357
2821.176592	441837.035101	39.686375
2823.555356	442470.066569	39.691392
2826.676577	443113.668894	39.696410
2829.257564	443746.625118	39.701428
2832.495324	444388.952526	39.706445
2835.245235	445008.656211	39.711463
2837.782324	445603.877211	39.716480
2840.369529	446220.383494	39.721498
2842.925679	446841.822963	39.726516
2845.636376	447452.662502	39.731533
2848.575275	448073.898933	39.736551
2851.104940	448681.745897	39.741568
2853.995594	449307.694089	39.746586
2856.912769	449948.360326	39.751604
2859.468695	450566.389536	39.756621
2862.130078	451211.291829	39.761639
2864.842845	451844.601052	39.766656
2867.946203	452480.249943	39.771674
2870.594427	453134.373892	39.776692
2873.279671	453786.549503	39.781709
2875.639984	454456.167483	39.786727
2878.972759	455115.764571	39.791744
2881.601519	455783.119318	39.796762
2884.719692	456452.189098	39.801780
2887.636589	457121.315095	39.806797
2890.558262	457802.678899	39.811815
2893.284517	458474.962067	39.816832
2896.327405	459158.776843	39.821850
2899.032840	459843.374160	39.826868
2901.981862	460542.439271	39.831885
2904.623375	461231.835453	39.836903
2907.702057	461935.566500	39.841920
2910.698039	462636.455764	39.846938
2913.667803	463330.004246	39.851956
2916.916633	464028.727626	39.856973
2919.654314	464730.175782	39.861991
2922.527906	465444.538493	39.867008
2925.705691	466146.817029	39.872026
2928.314326	466867.970481	39.877044
2931.427162	467580.590092	39.882061
2934.419815	468290.675893	39.887079
2937.371666	469013.901654	39.892096
2940.554389	469732.873470	39.897114
2943.727639	470460.489715	39.902132
2946.613292	471171.476551	39.907149
2949.747290	471891.016824	39.912167
2952.634698	472616.917524	39.917184
2956.059452	473332.364858	39.922202
2958.747077	474052.685860	39.927220
2961.582216	474770.581927	39.932237
2964.914054	475502.938795	39.937255
2967.693877	476222.291120	39.942272
2971.133302	476946.297116	39.947290
2973.843000	477659.394912	39.952308
2976.921633	478387.323757	39.957325
2979.969722	479111.342707	39.962343
2983.152742	479833.845680	39.967360
2986.616450	480542.864962	39.972378
2989.547813	481272.346932	39.977396
2992.446491	481991.771168	39.982413
2995.539031	482696.870434	39.987431
2998.301298	483420.180823	39.992448
3001.722410	484122.946791	39.997466
3004.470554	484838.231694	40.002484
3007.467715	485552.184897	40.007501
3010.722874	486277.249530	40.012519
3013.237212	486986.374900	40.017536
3016.404432	487700.856497	40.022554
3019.528636	488429.416453	40.027572
3022.546348	489134.031044	40.032589
3025.789696	489864.165882	40.037607
3028.441534	490580.053432	40.042624
3031.503015	491272.976897	40.047642
3034.374225	491979.244527	40.052660
3037.086086	492651.761866	40.057677
3040.061752	493342.941249	40.062695
3042.945884	494029.721919	40.067712
3046.005666	494721.327798	40.072730
3049.168605	495412.532865	40.077748
3052.105770	496097.749372	40.082765
3054.650320	496793.669078	40.087783
3057.836336	497504.156273	40.092800
3060.533551	498210.154723	40.097818
3063.744264	498925.301395	40.102836
3066.599199	499632.163015	40.107853
3069.486461	500363.045382	40.112871
3072.421924	501087.944231	40.117888
3075.176849	501817.062751	40.122906
3078.247245	502551.077558	40.127924
3081.058764	503284.441232	40.132941
3084.263663	504039.747057	40.137959
3086.957859	504797.759851	40.142976
3089.948376	505549.497147	40.147994
3092.709989	506323.117193	40.153012
3095.970133	507097.774330	40.158029
3099.604084	507874.544234	40.163047
3102.398836	508649.943768	40.168064
3106.099935	509434.263745	40.173082
3108.869452	510221.250883	40.178100
3111.792248	511009.276378	40.183117
3114.616801	511794.959225	40.188135
3118.160278	512597.936516	40.193152
3121.364512	513384.576584	40.198170
3124.711295	514188.548556	40.203188
3128.296809	514986.905256	40.208205
3131.602642	515795.717598	40.213223
3134.243773	516588.346737	40.218240
3137.670831	517377.338175	40.223258
3141.089019	518201.575710	40.228276
3144.324295	519000.808680	40.233293
3148.015376	519792.986703	40.238311
3150.879412	520597.310571	40.243328
3154.216894	521401.009868	40.248346
3157.273902	522201.890647	40.253364
3160.688396	523010.808727	40.258381
3164.244395	523805.334463	40.263399
3167.041809	524607.016317	40.268416
3170.463468	525413.275195	40.273434
3173.729789	526213.178967	40.278452
3176.783135	527022.060258	40.283469
3180.266367	527815.904947	40.288487
3183.565718	528619.626146	40.293504
3187.028030	529412.121807	40.298522
3189.857087	530216.421283	40.303540
3193.016748	531014.843867	40.308557
3196.328389	531823.137150	40.313575
3198.936977	532616.776560	40.318592
3202.639685	533422.699347	40.323610
3205.704730	534240.470863	40.328628
3209.042947	535052.574705	40.333645
3212.341467	535858.157042	40.338663
3215.456369	536660.855916	40.343680
3219.049417	537461.672612	40.348698
3222.076735	538271.160774	40.353716
3225.355673	539075.538838	40.358733
3228.199423	539869.946400	40.363751
3231.606482	540690.362158	40.368768
3234.984682	541482.577113	40.373786
3238.367911	542294.411192	40.378804
3241.252189	543107.274127	40.383821
3244.903561	543891.566940	40.388839
3247.567132	544668.840816	40.393856
3251.055065	545426.472886	40.398874
3253.897780	546202.920301	40.403892
3257.131352	546959.244199	40.408909
3260.543451	547733.299281	40.413927
3263.282742	548508.263415	40.418944
3266.882095	549278.380160	40.423962
3270.551566	550051.847431	40.428980
3273.631391	550831.976805	40.433997
3276.704865	551597.967697	40.439015
3279.743506	552378.956884	40.444032
3283.244875	553158.770539	40.449050
3286.098743	553960.893116	40.454068
3289.057495	554748.960353	40.459085
3292.605909	555552.422184	40.464103
3295.348357	556352.497822	40.469120
3299.003600	557171.221318	40.474138
3301.918261	557994.865409	40.479156
3305.234966	558820.544345	40.484173
3308.950897	559640.892268	40.489191
3312.088431	560474.751517	40.494208
3314.823901	561300.698924	40.499226
3318.344766	562141.143778	40.504244
3321.724055	562984.005111	40.509261
3325.359490	563832.976734	40.514279
3328.238778	564684.759515	40.519296
3331.884107	565543.772303	40.524314
3335.431056	566392.721321	40.529332
3337.996484	567249.022314	40.534349
3341.578374	568123.126298	40.539367
3345.236530	568997.903014	40.544384
3348.802792	569857.458413	40.549402
3352.260653	570725.226012	40.554420
3355.722256	571589.122905	40.559437
3359.011375	572450.228425	40.564455
3362.747219	573334.721269	40.569472
3365.823023	574200.882197	40.574490
3369.601661	575081.828816	40.579508
3372.868702	575964.988143	40.584525
3376.501226	576835.763092	40.589543
3379.996592	577713.095570	40.594560
3383.070974	578583.571698	40.599578
3387.010911	579462.748195	40.604596
3390.122024	580340.034121	40.609613
3393.826547	581216.257677	40.614631
3397.314573	582104.597729	40.619648
3401.130282	582977.963717	40.624666
3404.757511	583839.589727	40.629684
3408.208704	584723.724067	40.634701
3411.409380	585577.480694	40.639719
3414.801123	586452.885763	40.644736
3418.107020	587322.635615	40.649754
3421.635107	588196.179581	40.654772
3425.334111	589073.424611	40.659789
3428.990557	589939.361262	40.664807
3432.161366	590804.005080	40.669824
3435.408143	591668.217737	40.674842
3439.105985	592543.131652	40.679860
3442.243045	593422.557732	40.684877
3446.132041	594286.108779	40.689895
3449.623897	595167.083732	40.694912
3452.753982	596033.858022	40.699930
3456.397777	596899.232551	40.704948
3459.717151	597761.840407	40.709965
3463.331444	598633.419105	40.714983
3466.456161	599510.544000	40.720000
3469.970172	600380.195901	40.725018
3473.137116	601231.170364	40.730023
3476.371583	602052.204227	40.735028
3480.394409	602820.859112	40.740032
3483.533429	603546.864673	40.745037
3486.044573	604216.480835	40.750042
3488.877440	604831.671264	40.755047
3491.429983	605391.589207	40.760052
3494.411356	605903.636431	40.765056
3496.856725	606353.464404	40.770061
3498.874695	606765.524237	40.775066
3501.280453	607116.684514	40.780071
3502.904933	607425.790601	40.785076
3505.845401	607688.417152	40.790080
3507.266880	607909.712290	40.795085
3508.452711	608075.274154	40.800090
3510.221015	608212.034737	40.805095
3511.225762	608317.454915	40.810100
3512.849051	608378.666475	40.815104
3513.779421	608425.182398	40.820109
3515.230191	608431.807178	40.825114
3516.409127	608411.417868	40.830119
3517.058942	608355.002270	40.835124
3518.377297	608282.677800	40.840128
3519.028038	608185.150474	40.845133
3519.468169	608055.946339	40.850138
3520.375581	607914.563989	40.855143
3520.500747	607756.446793	40.860148
3521.610334	607574.615611	40.865152
3521.845169	607390.016959	40.870157
3522.451351	607194.002817	40.875162
3522.430153	606964.720204	40.880167
3522.496841	606750.774984	40.885172
3522.792624	606501.874524	40.890176
3523.299784	606260.438408	40.895181
3523.578892	606003.875034	40.900186
3523.590328	605738.992903	40.905191
3523.006471	605476.148058	40.910196
3523.516950	605208.873074	40.915200
3523.561834	604921.602266	40.920205
3523.936143	604651.782666	40.925210
3524.108035	604360.073711	40.930215
3523.655246	604078.560916	40.935220
3523.911386	603780.668368	40.940224
3523.582059	603484.359869	40.945229
3523.469768	603188.559387	40.950234
3523.703527	602883.939551	40.955239
3523.328506	602603.975816	40.960244
3522.969575	602293.576604	40.965248
3523.038592	602003.418824	40.970253
3522.948094	601705.921329	40.975258
3522.833429	601407.017831	40.980263
3522.514773	601105.084756	40.985268
3522.545285	600813.398463	40.990272
3522.646594	600519.740997	40.995277
3521.962014	600218.390062	41.000282
3521.925646	599916.478635	41.005287
3521.812345	599629.687052	41.010292
3521.535031	599342.813153	41.015296
3521.411950	599063.365849	41.020301
3521.325865	598776.246347	41.025306
3520.910634	598479.859279	41.030311
3520.806347	598203.840337	41.035316
3520.194070	597921.085038	41.040320
3520.037111	597642.206035	41.045325
3519.676956	597376.168165	41.050330
3519.884754	597102.524806	41.055335
3519.738966	596835.338333	41.060340
3519.238466	596576.862527	41.065344
3519.216121	596303.635023	41.070349
3519.040229	596046.046845	41.075354
3518.750664	595784.564490	41.080359
3518.347585	595525.847508	41.085364
3518.386684	595273.715112	41.090368
3517.938405	595028.613552	41.095373
3517.789565	594785.863253	41.100378
3517.352058	594543.653327	41.105383
3517.279379	594303.033491	41.110388
3517.036635	594066.591528	41.115392
3516.771595	593828.495095	41.120397
3516.757723	593591.556079	41.125402
3516.605633	593366.653644	41.130407
3516.174524	593143.943760	41.135412
3515.841970	592914.351993	41.140416
3515.234012	592705.033667	41.145421
3515.287908	592490.498764	41.150426
3515.456345	592272.886206	41.155431
3515.007272	592067.788179	41.160436
3515.217981	591858.124956	41.165440
3514.952933	591652.339027	41.170445
3514.738043	591450.949516	41.175450
3514.604101	591228.153340	41.180455
3514.392824	591040.481391	41.185460
3513.847573	590841.887342	41.190464
3513.647699	590652.353282	41.195469
3513.094551	590474.794390	41.200474
3513.394761	590285.075494	41.205479
3512.943677	590097.975684	41.210484
3512.743609	589925.412593	41.215488
3513.094863	589745.295483	41.220493
3512.741014	589567.039167	41.225498
3512.381501	589391.386139	41.230503
3512.292001	589220.197371	41.235508
3512.329113	589053.194867	41.240512
3512.413176	588880.420351	41.245517
3512.254983	588712.240593	41.250522
3512.489601	588541.140731	41.255527
3511.869747	588372.226154	41.260532
3511.654200	588214.920969	41.265536
3511.524063	588046.475948	41.270541
3511.306921	587894.979018	41.275546
3511.179739	587747.675185	41.280551
3510.607039	587590.917888	41.285556
3510.420503	587435.801762	41.290560
3510.429917	587288.420235	41.295565
3510.241189	587153.395529	41.300570
3510.725760	587008.541814	41.305575
3510.242530	586874.411620	41.310580
3509.907017	586724.069503	41.315584
3509.852094	586598.037710	41.320589
3509.707088	586463.699234	41.325594
3510.009717	586329.339241	41.330599
3509.305648	586193.631442	41.335604
3509.379226	586068.876500	41.340608
3509.620787	585948.454200	41.345613
3509.176471	585820.269069	41.350618
3509.210844	585700.628214	41.355623
3509.172086	585573.679904	41.360628
3509.165358	585455.095315	41.365632
3509.021973	585333.222785	41.370637
3508.683522	585210.577437	41.375642
3508.906021	585096.865093	41.380647
3508.466930	584975.686399	41.385652
3508.556170	584865.851971	41.390656
3508.139399	584748.025552	41.395661
3508.078437	584652.397603	41.400666
3508.390743	584534.454912	41.405671
3508.115892	584428.582782	41.410676
3508.193585	584316.539125	41.415680
3507.795380	584203.465934	41.420685
3507.671933	584106.289064	41.425690
3507.717346	583996.853800	41.430695
3507.763372	583914.987788	41.435700
3507.388351	583808.774439	41.440704
3507.152907	583718.328859	41.445709
3507.102064	583612.062930	41.450714
3507.171342	583510.740052	41.455719
3506.927360	583420.794656	41.460724
3506.763516	583323.266263	41.465728
3507.131916	583244.954276	41.470733
3506.925988	583152.193395	41.475738
3506.920310	583060.302802	41.480743
3506.697536	582988.147364	41.485748
3506.625315	582901.078538	41.490752
3506.754533	582809.014362	41.495757
3506.494124	582718.764999	41.500762
3506.409545	582643.327024	41.505767
3506.396991	582568.679418	41.510772
3506.403408	582481.394447	41.515776
3506.261417	582399.496422	41.520781
3505.886419	582315.929614	41.525786
3506.411093	582241.797437	41.530791
3505.927116	582168.524347	41.535796
3506.334965	582088.092270	41.540800
3506.293397	582020.865669	41.545805
3505.782431	581948.347385	41.550810
3505.754483	581860.862332	41.555815
3505.732089	581798.043463	41.560820
3505.581496	581722.007859	41.565824
3506.132378	581641.700589	41.570829
3506.005492	581580.200415	41.575834
3506.075749	581493.499322	41.580839
3505.879075	581433.713968	41.585844
3505.832554	581359.815594	41.590848
3505.559743	581285.651262	41.595853
3505.517711	581215.862701	41.600858
3505.587975	581149.215001	41.605863
3505.472871	581087.710248	41.610868
3505.672611	581009.910194	41.615872
3505.406206	580936.895772	41.620877
3505.453081	580876.016361	41.625882
3505.211034	580807.510040	41.630887
3505.092085	580748.460968	41.635892
3505.062849	580686.238569	41.640896
3505.465055	580623.196229	41.645901
3504.827349	580562.472259	41.650906
3505.658334	580505.680268	41.655911
3505.369248	580452.723579	41.660916
3505.097419	580372.234868	41.665920
3505.283852	580310.578376	41.670925
3504.823060	580241.551167	41.675930
3504.650303	580172.328066	41.680935
3504.554390	580127.412966	41.685940
3504.894772	580075.459266	41.690944
3504.634825	580025.304125	41.695949
3504.743582	579973.285867	41.700954
3504.821317	579915.254678	41.705959
3504.711558	579864.874749	41.710964
3504.405289	579806.150826	41.715968
3504.546473	579748.610315	41.720973
3504.402513	579701.193658	41.725978
3504.658454	579644.487171	41.730983
3504.231943	579598.518373	41.735988
3504.636852	579540.534378	41.740992
3504.677728	579490.781129	41.745997
3504.374886	579433.057660	41.751002
3504.606154	579386.433525	41.756007
3504.226990	579335.641978	41.761012
3504.161635	579285.453078	41.766016
3504.538586	579239.758386	41.771021
3504.087985	579196.600047	41.776026
3504.438603	579148.602225	41.781031
3504.328705	579103.735327	41.786036
3504.200384	579050.345624	41.791040
3504.297809	579003.540211	41.796045
3504.068246	578961.550012	41.801050
3504.396202	578900.415240	41.806055
3504.318587	578852.934449	41.811060
3504.247115	578801.891762	41.816064
3504.282185	578751.534306	41.821069
3503.922521	578708.861374	41.826074
3504.300721	578666.775054	41.831079
3504.106881	578617.907181	41.836084
3504.369548	578563.450984	41.841088
3504.470409	578518.498632	41.846093
3503.909974	578471.643373	41.851098
3503.594137	578421.590048	41.856103
3503.785271	578377.575921	41.861108
3504.318255	578348.754763	41.866112
3504.461619	578297.325112	41.871117
3503.936148	578255.579127	41.876122
3504.070328	578206.808636	41.881127
3503.882577	578164.959364	41.886132
3503.731701	578118.289364	41.891136
3503.550344	578076.739686	41.896141
3503.702416	578043.664010	41.901146
3503.949918	578000.341750	41.906151
3504.014126	577961.511768	41.911156
3504.322063	577913.364849	41.916160
3504.003864	577874.142947	41.921165
3503.772780	577829.089249	41.926170
3503.931791	577772.538873	41.931175
3504.051197	577741.975202	41.936180
3504.002848	577683.952117	41.941184
3504.198717	577645.301080	41.946189
3503.948822	577604.713333	41.951194
3503.818448	577555.429639	41.956199
3504.070503	577523.941814	41.961204
3503.949311	577480.725339	41.966208
3503.786902	577435.308219	41.971213
3503.662656	577396.455580	41.976218
3503.580958	577339.689862	41.981223
3504.265051	577310.541468	41.986228
3503.961573	577263.691128	41.991232
3503.697333	577214.276385	41.996237
3503.548985	577181.746711	42.001242
3503.891043	577141.265379	42.006247
3503.359278	577100.770028	42.011252
3503.458416	577061.881307	42.016256
3503.951442	577026.592493	42.021261
3503.255734	576997.257716	42.026266
3503.559490	576947.000612	42.031271
3503.488913	576915.110080	42.036276
3503.780176	576878.498032	42.041280
3503.684045	576834.021150	42.046285
3503.594592	576803.236770	42.051290
3503.285922	576751.068123	42.056295
3503.304976	576722.272973	42.061300
3503.078436	576696.927062	42.066304
3503.331309	576658.564678	42.071309
3503.370494	576650.582896	42.076314
3503.172960	576596.891335	42.081319
3503.302039	576574.900506	42.086324
3503.300473	576542.847644	42.091328
3503.372722	576500.148923	42.096333
3503.364997	576468.197133	42.101338
3503.459225	576433.018962	42.106343
3503.419290	576400.921531	42.111348
3503.266580	576368.390180	42.116352
3503.195018	576328.873500	42.121357
3503.698268	576296.690856	42.126362
3503.562567	576245.847206	42.131367
3503.624454	576216.893576	42.136372
3503.427254	576176.493071	42.141376
3503.189659	576138.356075	42.146381
3503.324798	576112.099531	42.151386
3503.113711	576075.914544	42.156391
3503.187372	576048.714359	42.161396
3503.279666	576010.425031	42.166400
3503.677298	575981.819619	42.171405
3503.472365	575947.288662	42.176410
3503.116554	575915.239225	42.181415
3503.460092	575880.521992	42.186420
3503.594206	575834.500233	42.191424
3503.734330	575804.379529	42.196429
3503.206681	575768.744687	42.201434
3503.169831	575734.838942	42.206439
3503.405628	575708.816547	42.211444
3503.407148	575670.590419	42.216448
3503.567212	575638.108390	42.221453
3503.190064	575600.743867	42.226458
3503.858582	575560.857966	42.231463
3503.463592	575520.787020	42.236468
3503.345275	575492.762684	42.241472
3503.024023	575459.653061	42.246477
3502.976900	575418.373548	42.251482
3503.206616	575383.572247	42.256487
3503.372188	575367.994661	42.261492
3503.147386	575337.428093	42.266496
3503.357207	575306.642997	42.271501
3503.159362	575270.152348	42.276506
3503.170855	575239.899744	42.281511
3502.969064	575201.703809	42.286516
3503.264105	575181.088998	42.291520
3503.641358	575147.869262	42.296525
3502.983225	575111.450055	42.301530
3503.000571	575079.089063	42.306535
3503.690016	575060.168248	42.311540
3503.422980	575025.945180	42.316544
3503.462525	574982.342793	42.321549
3503.471713	574947.975970	42.326554
3503.399352	574905.695159	42.331559
3503.288775	574874.407118	42.336564
3503.270582	574838.087660	42.341568
3502.954154	574813.654597	42.346573
3503.004421	574789.615677	42.351578
3503.341238	574743.908963	42.356583
3503.281775	574718.582645	42.361588
3503.189944	574688.194206	42.366592
3503.235853	574646.696648	42.371597
3503.235385	574622.916154	42.376602
3503.304165	574590.646061	42.381607
3503.098267	574554.555716	42.386612
3503.155491	574526.200515	42.391616
3503.227470	574495.384588	42.396621
3502.744315	574467.615421	42.401626
3502.777043	574435.902398	42.406631
3502.958745	574412.494348	42.411636
3502.933916	574385.957770	42.416640
3503.281932	574354.496256	42.421645
3502.831775	574326.169701	42.426650
3502.962934	574293.036097	42.431655
3502.495915	574260.046080	42.436660
3503.026518	574238.589985	42.441664
3503.084745	574212.591904	42.446669
3502.860672	574184.932054	42.451674
3503.066499	574148.173985	42.456679
3503.323809	574127.111607	42.461684
3502.978812	574102.229920	42.466688
3502.718410	574064.340332	42.471693
3502.858419	574039.683721	42.476698
3503.349020	574034.539520	42.481703
3502.965278	573994.662082	42.486708
3502.606299	573961.102404	42.491712
3503.013756	573927.673674	42.496717
3503.208425	573907.122408	42.501722
3503.063925	573873.880153	42.506727
3502.907166	573850.323159	42.511732
3502.796093	573822.644758	42.516736
3502.546042	573787.612508	42.521741
3502.727691	573773.033684	42.526746
3503.000145	573752.219110	42.531751
3502.920636	573724.234492	42.536756
3502.673355	573700.239773	42.541760
3502.441194	573672.178542	42.546765
3502.814175	573653.605904	42.551770
3502.938327	573629.251924	42.556775
3502.768195	573601.030297	42.561780
3502.992749	573579.169232	42.566784
3502.985428	573550.771505	42.571789
3503.107911	573526.267041	42.576794
3502.553537	573484.758716	42.581799
3502.985654	573462.212704	42.586804
3502.459484	573438.461728	42.591808
3502.705603	573408.368246	42.596813
3502.719622	573392.259707	42.601818
3502.857119	573365.645187	42.606823
3502.770467	573330.134399	42.611828
3502.937217	573300.855849	42.616832
3502.823378	573284.817321	42.621837
3502.596190	573265.133654	42.626842
3502.956368	573231.158330	42.631847
3502.717998	573196.323129	42.636852
3502.497277	573185.519489	42.641856
3502.828514	573150.093337	42.646861
3502.879912	573139.497994	42.651866
3502.860009	573117.072139	42.656871
3502.987826	573081.025278	42.661876
3502.988221	573060.753735	42.666880
3502.774426	573031.734688	42.671885
3502.881148	573004.722718	42.676890
3503.055661	572976.495836	42.681895
3502.568105	572954.042411	42.686900
3502.487143	572924.600907	42.691904
3502.562025	572902.812116	42.696909
3502.804035	572879.190765	42.701914
3502.891914	572858.453586	42.706919
3502.997343	572830.538207	42.711924
3502.595221	572805.612422	42.716928
3502.993184	572778.955809	42.721933
3502.868138	572759.154939	42.726938
3503.060553	572734.386945	42.731943
3502.519719	572716.407237	42.736948
3502.839255	572687.805718	42.741952
3502.546292	572659.199522	42.746957
3502.364304	572639.858953	42.751962
3502.692021	572621.944030	42.756967
3502.575255	572589.948142	42.761972
3502.614216	572566.709137	42.766976
3503.120145	572546.608541	42.771981
3502.682946	572533.379348	42.776986
3502.602559	572495.807628	42.781991
3503.322584	572467.193127	42.786996
3502.377610	572453.039632	42.792001
3502.622360	572426.556685	42.797005
3502.729237	572401.851518	42.802010
3502.885897	572374.428807	42.807015
3502.969811	572350.279096	42.812020
3502.522407	572324.305554	42.817025
3502.957326	572290.917900	42.822029
3502.505633	572269.160034	42.827034
3502.479028	572253.156592	42.832039
3502.665627	572222.567474	42.837044
3502.384343	572198.524713	42.842049
3502.859438	572172.908417	42.847053
3502.903806	572162.413625	42.852058
3502.695898	572125.111519	42.857063
3503.026096	572110.958972	42.862068
3502.480098	572078.878204	42.867073
3502.602387	572064.356653	42.872077
3502.580650	572038.617000	42.877082
3502.724931	572019.374913	42.882087
3502.609745	571988.581439	42.887092
3502.342895	571976.679865	42.892097
3502.755434	571940.936152	42.897101
3502.271584	571925.907001	42.902106
3502.307171	571901.563166	42.907111
3502.165627	571884.222263	42.912116
3502.157352	571866.459043	42.917121
3502.098155	571841.477531	42.922125
3501.936774	571848.979805	42.927130
3501.935766	571815.809455	42.932135
3502.214153	571806.682854	42.937140
3502.149834	571800.670942	42.942145
3502.310761	571776.056334	42.947149
3502.043598	571768.269548	42.952154
3502.072753	571751.554129	42.957159
3502.403618	571723.851707	42.962164
3502.012085	571724.866295	42.967169
3502.300178	571698.073784	42.972173
3502.023328	571686.976394	42.977178
3502.609410	571674.088057	42.982183
3502.377758	571651.993513	42.987188
3502.306667	571635.092863	42.992193
3502.430267	571616.204611	42.997197
3502.438670	571602.603571	43.002202
3502.330145	571570.703896	43.007207
3501.896558	571558.978499	43.012212
3501.980323	571546.469646	43.017217
3502.361357	571527.490819	43.022221
3502.290311	571512.246036	43.027226
3502.693408	571501.493822	43.032231
3502.056769	571471.834325	43.037236
3501.947770	571459.204959	43.042241
3502.340186	571432.295149	43.047245
3501.998656	571420.555218	43.052250
3502.324371	571404.896979	43.057255
3502.547991	571397.986712	43.062260
3502.461988	571378.628993	43.067265
3502.225048	571361.001101	43.072269
3502.169842	571350.721866	43.077274
3502.003724	571316.220898	43.082279
3502.413629	571308.428320	43.087284
3502.414059	571293.322624	43.092289
3502.543784	571269.163462	43.097293
3502.289660	571250.132914	43.102298
3502.684916	571231.502667	43.107303
3502.593992	571203.664183	43.112308
3502.045315	571195.268608	43.117313
3502.305702	571167.174375	43.122317
3502.565215	571154.788174	43.127322
3502.259961	571135.062835	43.132327
3502.325731	571113.171676	43.137332
3502.592347	571109.265635	43.142337
3501.952634	571070.923503	43.147341
3502.069503	571067.241599	43.152346
3502.322472	571043.514363	43.157351
3502.371644	571019.919309	43.162356
3502.334021	571007.629585	43.167361
3502.520730	570982.055705	43.172365
3502.437210	570962.094660	43.177370
3502.323717	570940.130822	43.182375
3502.744512	570926.263764	43.187380
3502.824099	570914.256734	43.192385
3502.545472	570886.647565	43.197389
3502.487161	570865.126633	43.202394
3502.337243	570851.449076	43.207399
3502.667861	570826.856082	43.212404
3502.096171	570807.774068	43.217409
3502.359541	570782.438691	43.222413
3502.335012	570768.390125	43.227418
3502.411529	570750.310792	43.232423
3502.715335	570733.099265	43.237428
3502.144737	570715.321787	43.242433
3502.721626	570704.240535	43.247437
3502.597392	570669.731066	43.252442
3502.204350	570648.462804	43.257447
3502.709323	570634.632422	43.262452
3502.511934	570621.664635	43.267457
3502.285181	570581.048049	43.272461
3502.467199	570571.835156	43.277466
3502.481104	570545.484311	43.282471
3502.570922	570523.487889	43.287476
3502.140301	570508.448541	43.292481
3502.371230	570496.517790	43.297485
3502.460360	570475.023262	43.302490
3502.481161	570447.968481	43.307495
3502.535467	570417.595965	43.312500
3502.310724	570413.967256	43.317505
3502.433604	570390.409569	43.322509
3502.336504	570372.306591	43.327514
3502.496129	570345.932507	43.332519
3502.949889	570326.338058	43.337524
3502.338138	570302.744469	43.342529
3502.686978	570282.714647	43.347533
3502.749358	570253.645348	43.352538
3502.799946	570239.433822	43.357543
3502.720608	570210.236000	43.362548
3502.168332	570189.844993	43.367553
3502.353341	570165.925807	43.372557
3502.274953	570143.553435	43.377562
3502.504428	570118.824165	43.382567
3502.593599	570107.718205	43.387572
3502.042452	570096.411196	43.392577
3502.450314	570080.487358	43.397581
3502.570380	570059.940824	43.402586
3502.473832	570040.733056	43.407591
3502.832375	570011.767415	43.412596
3502.527971	569999.066602	43.417601
3502.410690	569961.994210	43.422605
3502.700173	569948.999738	43.427610
3502.558202	569936.875748	43.432615
3502.443074	569908.586180	43.437620
3502.600701	569887.079842	43.442625
3502.372698	569862.923445	43.447629
3502.283561	569845.470871	43.452634
3502.222233	569824.751508	43.457639
3502.435756	569791.792703	43.462644
3502.175239	569795.145953	43.467649
3501.939629	569760.902111	43.472653
3501.983009	569751.509468	43.477658
3501.792316	569749.581727	43.482663
3502.248634	569736.209594	43.487668
3502.386080	569718.420257	43.492673
3502.406727	569700.398193	43.497677
3502.545513	569680.801692	43.502682
3502.095696	569670.130910	43.507687
3502.373732	569639.018672	43.512692
3502.556291	569632.214147	43.517697
3502.345731	569607.201223	43.522701
3502.339853	569592.495804	43.527706
3502.328497	569572.169709	43.532711
3502.120218	569546.955528	43.537716
3501.812956	569546.953279	43.542721
3501.968004	569528.859743	43.547725
3502.377540	569515.695437	43.552730
3502.206492	569498.907641	43.557735
3502.404118	569474.181962	43.562740
3502.054398	569470.974028	43.567745
3502.149038	569441.947821	43.572749
3502.239199	569436.713598	43.577754
3502.116080	569423.532070	43.582759
3502.344261	569390.921173	43.587764
3502.296881	569378.079103	43.592769
3502.316623	569354.886764	43.597773
3502.191850	569340.651347	43.602778
3502.235485	569322.022778	43.607783
3502.150089	569297.089997	43.612788
3501.806170	569296.240191	43.617793
3501.806228	569284.494854	43.622797
3501.964452	569263.539382	43.627802
3502.377981	569256.347174	43.632807
3502.503609	569246.489519	43.637812
3502.316071	569233.016683	43.642817
3502.197279	569212.054229	43.647821
3502.200530	569185.199988	43.652826
3502.022476	569179.806802	43.657831
3502.193360	569152.725503	43.662836
3502.259273	569141.019918	43.667841
3502.126775	569122.167590	43.672845
3502.091779	569103.751736	43.677850
3502.108590	569096.019118	43.682855
3502.175821	569085.166570	43.687860
3502.494936	569060.019455	43.692865
3502.585046	569047.908438	43.697869
3502.075478	569027.609070	43.702874
3502.025551	569012.006293	43.707879
3502.321182	568986.712105	43.712884
3501.907819	568974.679718	43.717889
3501.852273	568965.954430	43.722893
3502.215641	568943.912216	43.727898
3502.025729	568936.061222	43.732903
3501.925115	568918.006693	43.737908
3502.147242	568906.226253	43.742913
3502.257369	568887.235220	43.747917
3501.994925	568885.720109	43.752922
3501.673177	568864.086017	43.757927
3501.782503	568842.334300	43.762932
3502.111872	568836.811433	43.767937
3502.129753	568826.066746	43.772941
3502.128184	568801.872716	43.777946
3502.114749	568788.321945	43.782951
3502.203101	568779.724606	43.787956
3501.803420	568765.631842	43.792961
3502.086748	568762.324744	43.797965
3502.360469	568758.165820	43.802970
3501.985432	568740.153911	43.807975
3502.441253	568707.706274	43.812980
3501.624701	568692.373496	43.817985
3501.857160	568677.378667	43.822989
3502.155897	568677.281679	43.827994
3502.171477	568665.031323	43.832999
3502.228630	568652.523473	43.838004
3501.839992	568646.008446	43.843009
3501.677473	568613.908189	43.848013
3502.164386	568610.017062	43.853018
3502.115027	568603.750149	43.858023
3502.402071	568581.668979	43.863028
3502.359114	568558.233853	43.868033
3502.073033	568542.918340	43.873037
3502.319811	568525.461443	43.878042
3502.137151	568525.791087	43.883047
3502.260371	568498.063143	43.888052
3502.411782	568475.902581	43.893057
3502.158797	568452.851452	43.898061
3502.440649	568443.771840	43.903066
3502.228950	568431.506568	43.908071
3502.457634	568397.888837	43.913076
3502.160765	568384.080715	43.918081
3502.228858	568365.396577	43.923085
3502.005056	568349.418504	43.928090
3502.054986	568338.266773	43.933095
3502.171812	568321.582844	43.938100
3502.166847	568298.944412	43.943105
3502.367570	568291.584084	43.948109
3502.407002	568284.851338	43.953114
3501.776018	568266.577511	43.958119
3502.161674	568240.966427	43.963124
3501.809811	568222.849688	43.968129
3501.969853	568217.453393	43.973133
3502.195851	568207.528962	43.978138
3501.919748	568194.068751	43.983143
3502.199034	568173.544154	43.988148
3502.011501	568162.680367	43.993153
3502.217401	568150.198917	43.998157
3502.098975	568131.995344	44.003162
3502.164086	568128.872775	44.008167
3502.025843	568110.170281	44.013172
3501.962102	568103.001771	44.018177
3502.444551	568080.989493	44.023181
3502.500283	568072.195932	44.028186
3502.244847	568047.939607	44.033191
3502.456557	568031.692215	44.038196
3502.096184	568012.271305	44.043201
3502.230227	567983.837648	44.048205
3502.175718	567978.273986	44.053210
3501.827133	567964.071852	44.058215
3501.847034	567945.796160	44.063220
3501.903018	567943.478155	44.068225
3501.768485	567926.079961	44.073229
3502.010550	567916.303366	44.078234
3501.494023	567909.054921	44.083239
3501.927631	567898.344778	44.088244
3501.614308	567888.654983	44.093249
3502.302365	567861.138404	44.098253
3501.946023	567862.449009	44.103258
3501.787368	567856.650571	44.108263
3502.085563	567828.843466	44.113268
3501.678935	567819.921194	44.118273
3502.140855	567811.917331	44.123277
3502.478249	567789.475377	44.128282
3502.314027	567781.719977	44.133287
3502.456966	567754.689962	44.138292
3502.352800	567740.248542	44.143297
3501.888182	567720.793236	44.148301
3501.515808	567697.458057	44.153306
3501.654000	567684.283885	44.158311
3502.063543	567671.970885	44.163316
3501.892849	567672.800685	44.168321
3501.830771	567660.561401	44.173325
3502.103225	567651.081034	44.178330
3501.916424	567641.371251	44.183335
3502.125179	567617.945064	44.188340
3502.086213	567616.194043	44.193345
3501.715747	567607.366354	44.198349
3502.291821	567585.689902	44.203354
3502.058865	567581.910972	44.208359
3502.329270	567570.422828	44.213364
3502.323148	567547.481897	44.218369
3501.843026	567534.605019	44.223373
3502.002978	567518.917208	44.228378
3502.151938	567502.528279	44.233383
3502.099793	567483.510102	44.238388
3501.994744	567479.560538	44.243393
3502.080688	567464.436436	44.248397
3502.555905	567454.271594	44.253402
3502.230160	567435.396512	44.258407
3502.217410	567418.731535	44.263412
3501.919798	567400.303811	44.268417
3502.055474	567375.583317	44.273421
3501.873040	567368.483107	44.278426
3502.075162	567367.045771	44.283431
3502.221517	567347.142910	44.288436
3502.582934	567345.580265	44.293441
3502.083927	567314.633432	44.298445
3502.488598	567291.125754	44.303450
3502.335824	567278.799840	44.308455
3502.489426	567257.490032	44.313460
3502.181074	567244.836987	44.318465
3502.237283	567216.765027	44.323469
3502.330429	567209.922852	44.328474
3502.650416	567196.117277	44.333479
3502.343459	567165.842855	44.338484
3502.740755	567148.360348	44.343489
3502.186417	567131.227394	44.348493
3502.514049	567105.622868	44.353498
3501.758686	567088.320465	44.358503
3502.063840	567081.495275	44.363508
3502.109281	567056.637596	44.368513
3502.107614	567046.597152	44.373517
3502.529487	567030.566515	44.378522
3501.961158	567015.242889	44.383527
3502.104033	567003.171681	44.388532
3502.079432	566970.944883	44.393537
3502.014339	566962.119163	44.398541
3502.232111	566955.558576	44.403546
3502.366967	566944.693445	44.408551
3502.338955	566914.926998	44.413556
3501.906241	566904.953815	44.418561
3502.392834	566888.611643	44.423565
3502.127484	566884.184897	44.428570
3502.065901	566851.762733	44.433575
3502.154375	566840.302308	44.438580
3501.798964	566839.755330	44.443585
3501.705747	566824.357176	44.448589
3501.811744	566803.154383	44.453594
3501.726517	566809.292520	44.458599
3501.749176	566794.227640	44.463604
3501.602642	566779.892050	44.468609
3501.545030	566763.082529	44.473613
3501.866496	566757.660320	44.478618
3501.662607	566762.059881	44.483623
3501.958290	566750.617178	44.488628
3501.847086	566735.422535	44.493633
3501.409520	566715.961303	44.498637
3501.380460	566718.827413	44.503642
3501.140649	566719.166039	44.508647
3501.695420	566711.297519	44.513652
3501.679238	566706.731344	44.518657
3501.551471	566697.613991	44.523661
3502.014071	566676.907470	44.528666
3501.915313	566677.826503	44.533671
3501.966290	566677.667829	44.538676
3502.179898	566649.770706	44.543681
3501.504289	566636.120105	44.548685
3502.015076	566637.696925	44.553690
3501.655847	566623.846235	44.558695
3501.716411	566601.897102	44.563700
3501.527060	566598.161235	44.568705
3502.064642	566597.625259	44.573709
3502.176613	566575.818656	44.578714
3501.382973	566568.763297	44.583719
3501.764195	566545.910442	44.588724
3501.678940	566549.488253	44.593729
3501.957752	566532.525394	44.598733
3502.249114	566520.129239	44.603738
3501.566710	566513.960153	44.608743
3501.978268	566495.871970	44.613748
3501.832696	566498.806554	44.618753
3501.674994	566477.142333	44.623757
3501.765932	566456.393110	44.628762
3501.519369	566458.891641	44.633767
3501.958619	566463.943858	44.638772
3502.319751	566450.733432	44.643777
3502.224795	566433.577830	44.648781
3502.350623	566409.358871	44.653786
3502.166929	566388.200606	44.658791
3502.315997	566376.830662	44.663796
3502.144594	566362.498442	44.668801
3501.876570	566345.972239	44.673805
3501.972430	566336.317581	44.678810
3501.831351	566316.307265	44.683815
3501.800836	566296.781692	44.688820
3502.189537	566295.616297	44.693825
3502.059635	566276.809117	44.698829
3501.921603	566258.555449	44.703834
3502.078465	566253.409772	44.708839
3502.126974	566232.014095	44.713844
3501.865735	566214.131064	44.718849
3501.882036	566206.547211	44.723853
3502.120726	566195.665146	44.728858
3501.854780	566183.707203	44.733863
3502.129990	566170.459684	44.738868
3502.028281	566166.810390	44.743873
3501.983913	566152.307430	44.748877
3501.991543	566135.888455	44.753882
3502.087505	566139.990340	44.758887
3501.820798	566110.359554	44.763892
3501.630445	566097.285147	44.768897
3501.912646	566105.826370	44.773901
3502.135891	566088.319270	44.778906
3501.427060	566068.698525	44.783911
3501.736700	566054.642175	44.788916
3502.194710	566052.712810	44.793921
3501.508286	566044.987670	44.798925
3501.427740	566017.335841	44.803930
3501.815106	566016.220836	44.808935
3501.661589	565999.274577	44.813940
3501.760052	566004.480686	44.818945
3501.921930	566005.007573	44.823949
3502.037956	565985.558984	44.828954
3501.741816	565981.638780	44.833959
3501.735876	565974.911783	44.838964
3501.615563	565955.249050	44.843969
3501.385989	565936.858563	44.848973
3501.728308	565935.097889	44.853978
3501.351749	565936.713111	44.858983
3501.572696	565920.310692	44.863988
3501.922667	565925.929390	44.868993
3501.867716	565915.143176	44.873997
3502.217479	565895.005191	44.879002
3501.547345	565877.386395	44.884007
3501.710205	565878.565840	44.889012
3501.912794	565868.341819	44.894017
3501.909584	565857.898920	44.899021
3501.853231	565827.230361	44.904026
3501.864749	565832.701182	44.909031
3501.681371	565821.382665	44.914036
3501.674152	565798.890317	44.919041
3501.661005	565799.595200	44.924045
3501.857688	565795.949350	44.929050
3501.571163	565791.123825	44.934055
3501.546716	565772.550384	44.939060
3502.043697	565758.112929	44.944065
3502.039213	565755.452479	44.949069
3501.964240	565741.957964	44.954074
3501.732311	565726.529827	44.959079
3501.669525	565703.493683	44.964084
3502.415116	565712.715889	44.969089
3502.034259	565699.369561	44.974093
3502.179017	565676.551964	44.979098
3502.297414	565674.173540	44.984103
3502.038366	565650.163792	44.989108
3502.007310	565639.574423	44.994113
3501.970317	565619.044539	44.999117
3501.735200	565596.035123	45.004122
3501.526308	565598.226691	45.009127
3501.619343	565583.751750	45.014132
3501.848807	565587.832960	45.019137
3501.680654	565574.854911	45.024141
3501.657181	565556.080134	45.029146
3501.796764	565561.932738	45.034151
3502.204035	565543.693118	45.039156
3501.472066	565531.957983	45.044161
3501.882946	565515.224043	45.049165
3502.273796	565508.886634	45.054170
3502.100286	565498.771294	45.059175
3501.838141	565487.063085	45.064180
3501.962568	565489.202567	45.069185
3501.999967	565479.556337	45.074189
3502.217822	565452.760292	45.079194
3501.772986	565441.733328	45.084199
3501.974173	565436.931831	45.089204
3501.896095	565416.558643	45.094209
3501.697387	565397.509743	45.099213
3502.022772	565386.864421	45.104218
3501.794954	565397.243258	45.109223
3502.238463	565353.641478	45.114228
3502.072292	565355.023047	45.119233
3501.926208	565344.150128	45.124237
3502.059789	565327.107794	45.129242
3501.442224	565319.522032	45.134247
3501.543524	565305.095663	45.139252
3501.886363	565304.037764	45.144257
3501.824065	565301.838144	45.149261
3501.931205	565274.858156	45.154266
3501.478849	565268.401380	45.159271
3501.760889	565262.432324	45.164276
3502.194393	565256.288954	45.169281
3501.758596	565227.184454	45.174285
3502.070717	565216.892528	45.179290
3501.676924	565217.205053	45.184295
3501.385232	565200.028173	45.189300
3501.801429	565188.364252	45.194305
3501.945748	565183.872808	45.199309
3502.234172	565170.371031	45.204314
3501.667181	565161.973879	45.209319
3502.110490	565146.690467	45.214324
3502.139660	565144.777786	45.219329
3501.799403	565124.394861	45.224333
3502.212160	565105.651584	45.229338
3501.732833	565101.659294	45.234343
3501.564553	565093.300185	45.239348
3501.447244	565059.777071	45.244353
3501.715119	565065.559659	45.249357
3501.798619	565047.470301	45.254362
3501.682583	565045.429669	45.259367
3501.951477	565041.320389	45.264372
3502.016079	565026.999836	45.269377
3501.423427	565014.087522	45.274381
3501.798030	565012.321666	45.279386
3501.896364	565015.168281	45.284391
3502.060657	564981.199223	45.289396
3501.867967	564970.182604	45.294401
3501.623960	564976.296319	45.299405
3501.916322	564966.258321	45.304410
3501.662088	564952.690489	45.309415
3501.859599	564933.428251	45.314420
3501.696237	564933.554123	45.319425
3502.006245	564931.848565	45.324429
3501.289767	564893.497839	45.329434
3501.440173	564891.666589	45.334439
3501.874627	564881.003755	45.339444
3501.704674	564883.842131	45.344449
3501.554750	564887.631411	45.349453
3502.265339	564885.712587	45.354458
3501.774076	564862.842187	45.359463
3501.795781	564849.683010	45.364468
3501.942806	564841.525491	45.369473
3501.731528	564820.569530	45.374477
3501.774320	564815.842753	45.379482
3501.555073	564816.931405	45.384487
3501.774157	564812.980471	45.389492
3501.936545	564806.377121	45.394497
3502.013043	564790.949737	45.399501
3501.641852	564776.596577	45.404506
3501.626379	564768.866114	45.409511
3501.644388	564771.825772	45.414516
3501.748751	564751.272259	45.419521
3501.963020	564741.246276	45.424525
3501.669960	564730.295333	45.429530
3501.461357	564728.419754	45.434535
3502.204830	564722.679567	45.439540
3502.038725	564702.118036	45.444545
3501.664206	564697.908367	45.449549
3502.076254	564689.307606	45.454554
3501.720229	564672.541709	45.459559
3501.628834	564656.989753	45.464564
3501.901100	564651.373408	45.469569
3501.791429	564647.072104	45.474573
3501.552603	564622.755790	45.479578
3501.385852	564615.701652	45.484583
3501.336494	564609.432575	45.489588
3501.209642	564606.339069	45.494593
3501.100113	564614.842204	45.499597
3501.649308	564597.181482	45.504602
3501.461000	564601.830487	45.509607
3501.402208	564598.726340	45.514612
3501.558190	564595.337548	45.519617
3501.488776	564592.536342	45.524621
3501.977082	564571.018643	45.529626
3501.706062	564566.591891	45.534631
3502.046670	564558.654982	45.539636
3501.698065	564558.458319	45.544641
3501.407909	564533.848561	45.549645
3501.732374	564532.893896	45.554650
3501.528589	564525.745064	45.559655
3501.944874	564517.394584	45.564660
3501.931392	564510.918989	45.569665
3501.805688	564493.313403	45.574669
3501.851533	564474.626473	45.579674
3501.304208	564485.357353	45.584679
3501.264603	564481.396534	45.589684
3501.897445	564490.135205	45.594689
3501.427489	564470.022478	45.599693
3501.823488	564435.061537	45.604698
3501.793157	564441.342984	45.609703
3501.549802	564432.191706	45.614708
3501.724762	564427.494324	45.619713
3501.257445	564411.699523	45.624717
3501.874575	564394.278947	45.629722
3501.920490	564391.158375	45.634727
3501.851192	564394.232206	45.639732
3501.709896	564393.852488	45.644737
3501.303382	564371.620661	45.649741
3501.531118	564356.470347	45.654746
3501.711978	564353.931246	45.659751
3501.624608	564349.525917	45.664756
3501.695660	564354.586408	45.669761
3501.688459	564352.126921	45.674765
3502.278587	564325.019014	45.679770
3501.614505	564313.623531	45.684775
3501.825779	564311.330741	45.689780
3501.669912	564292.976343	45.694785
3501.445535	564289.496279	45.699789
3501.571684	564273.357438	45.704794
3501.440711	564275.888576	45.709799
3501.710681	564267.008426	45.714804
3501.823469	564267.995005	45.719809
3501.822793	564263.827166	45.724813
3501.926918	564233.279964	45.729818
3501.755838	564234.009632	45.734823
3501.364884	564207.707623	45.739828
3501.491548	564138.189462	45.744833
3501.114125	564047.307456	45.749837
3501.606097	563899.795193	45.754842
3501.084206	563707.846501	45.759847
3500.566969	563467.332693	45.764852
3500.131574	563170.454641	45.769857
3499.289581	562841.340415	45.774861
3499.284875	562462.214860	45.779866
3498.543059	562053.158014	45.784871
3497.670117	561592.273709	45.789876
3496.696639	561076.838740	45.794881
3496.094857	560533.444890	45.799885
3495.557761	559942.695958	45.804890
3494.209733	559293.468847	45.809895
3492.989207	558644.889570	45.814900
3492.397635	557926.691868	45.819905
3490.625455	557181.854693	45.824909
3489.720123	556391.511333	45.829914
3488.033623	555578.322971	45.834919
3486.398136	554709.388347	45.839924
3485.280971	553801.007074	45.844929
3483.718007	552874.331248	45.849933
3482.114957	551897.876388	45.854938
3480.402580	550904.569382	45.859943
3478.593656	549856.647324	45.864948
3476.511946	548792.538085	45.869953
3474.304276	547696.023170	45.874957
3472.320574	546562.513519	45.879962
3470.383643	545405.304646	45.884967
3468.508511	544230.977112	45.889972
3466.585707	543022.943451	45.894977
3463.954945	541782.857136	45.899981
3461.588621	540514.682833	45.904986
3459.492768	539227.267774	45.909991
3457.248432	537913.274544	45.914996
3454.801839	536574.717070	45.920001
3452.252664	535202.411763	45.925005
3449.968212	533820.605322	45.930010
3447.043341	532415.742935	45.935015
3444.567119	530990.265800	45.940020
3441.935927	529536.406660	45.945025
3439.564172	528073.129029	45.950029
3436.690119	526581.006932	45.955034
3433.454951	525085.599230	45.960039
3430.835217	523569.120239	45.965044
3428.195863	522037.910782	45.970049
3424.800960	520484.724741	45.975053
3422.005523	518924.916261	45.980058
3418.908318	517353.937560	45.985063
3415.775033	515757.579484	45.990068
3412.759198	514147.960112	45.995073
3409.633097	512547.094747	46.000077
3406.671910	510913.897703	46.005082
3403.481331	509281.806442	46.010087
3399.719643	507628.834582	46.015092
3396.847190	505978.153572	46.020097
3393.651486	504310.531917	46.025101
3390.514964	502636.298952	46.030106
3387.000407	500954.462284	46.035111
3383.874600	499262.579131	46.040116
3380.613766	497568.855355	46.045121
3376.887504	495858.401493	46.050125
3373.783505	494144.269992	46.055130
3370.577980	492428.442254	46.060135
3366.732946	490691.006568	46.065140
3363.589536	488946.291774	46.070145
3359.730743	487207.094826	46.075149
3356.235505	485461.076475	46.080154
3352.697396	483714.664808	46.085159
3349.028522	481971.916842	46.090164
3345.590338	480216.912035	46.095169
3341.822680	478473.335763	46.100173
3338.564623	476707.097856	46.105178
3334.757019	474947.018282	46.110183
3331.043827	473178.743843	46.115188
3327.540704	471417.625009	46.120193
3323.506621	469653.466357	46.125197
3320.468367	467884.259679	46.130202
3316.944745	466120.199651	46.135207
3312.675408	464348.634427	46.140212
3309.524132	462575.847746	46.145217
3305.896281	460807.250292	46.150221
3302.162597	459032.617051	46.155226
3298.158870	457255.312943	46.160231
3294.626959	455482.762933	46.165236
3291.077650	453695.510437	46.170241
3286.948027	451918.746246	46.175245
3283.478970	450145.649519	46.180250
3280.047958	448370.700610	46.185255
3275.990033	446589.700710	46.190260
3272.188298	444811.524673	46.195265
3268.359004	443039.865322	46.200269
3264.762712	441267.696069	46.205274
3261.004211	439495.991721	46.210279
3257.218496	437733.597457	46.215284
3253.452672	435954.267892	46.220289
3249.470550	434179.062651	46.225293
3245.946624	432417.303390	46.230298
3242.035577	430665.884217	46.235303
3238.409608	428902.963038	46.240308
3235.118096	427140.390323	46.245313
3230.879374	425381.054415	46.250317
3227.018024	423619.022222	46.255322
3223.326047	421857.318060	46.260327
3219.698283	420102.398843	46.265332
3215.855772	418345.083003	46.270337
3211.984983	416600.098518	46.275341
3208.306328	414850.832098	46.280346
3204.569469	413105.793013	46.285351
3200.595294	411359.990218	46.290356
3196.920473	409606.239376	46.295361
3193.133985	407873.063538	46.300365
3189.652913	406124.129185	46.305370
3185.731518	404382.433196	46.310375
3181.626372	402649.612926	46.315380
3178.148003	400926.306161	46.320385
3174.233050	399194.971246	46.325389
3170.620116	397460.719722	46.330394
3166.800313	395727.590843	46.335399
3163.009976	394016.716173	46.340404
3159.125083	392291.368255	46.345409
3155.328231	390581.723267	46.350413
3151.511288	388872.393754	46.355418
3147.405021	387162.839233	46.360423
3144.021233	385457.498081	46.365428
3140.173814	383744.395813	46.370433
3136.372639	382052.196407	46.375437
3132.376454	380346.204104	46.380442
3128.783741	378654.538298	46.385447
3124.933175	376965.928471	46.390452
3121.414643	375282.112878	46.395457
3117.382839	373598.526745	46.400461
3113.764420	371904.154406	46.405466
3110.120604	370230.284492	46.410471
3106.092914	368548.651472	46.415476
3102.568221	366872.835917	46.420481
3098.434472	365203.496682	46.425485
3094.595358	363519.659084	46.430490
3091.219076	361872.269521	46.435495
3087.167361	360207.486994	46.440500
3083.407227	358549.936750	46.445505
3079.988360	356894.225385	46.450509
3075.943381	355233.109469	46.455514
3072.144649	353590.650423	46.460519
3068.518887	351941.902366	46.465524
3065.016051	350292.058991	46.470529
3061.171922	348663.488490	46.475533
3057.270593	347011.127024	46.480538
3053.307817	345379.159732	46.485543
3049.880137	343754.657660	46.490548
3046.350086	342109.651897	46.495553
3042.421236	340485.252539	46.500557
3038.964050	338855.873224	46.505562
3035.172426	337223.700225	46.510567
3030.872354	335616.557550	46.515572
3027.581225	333988.892219	46.520577
3023.713116	332371.902852	46.525581
3019.796362	330756.683547	46.530586
3016.384727	329149.507810	46.535591
3012.047552	327539.307644	46.540596
3008.930600	325926.104278	46.545601
3005.188729	324328.197330	46.550605
3001.324454	322733.401876	46.555610
2997.873708	321133.087517	46.560615
2993.946569	319550.418167	46.565620
2990.548732	317935.983377	46.570625
2986.467552	316356.402348	46.575629
2982.928483	314764.645710	46.580634
2979.256372	313172.930533	46.585639
2975.262198	311599.150304	46.590644
2972.301010	310010.931383	46.595649
2968.255475	308428.020836	46.600653
2964.402814	306846.683108	46.605658
2960.758432	305282.186345	46.610663
2957.021043	303713.380481	46.615668
2953.055434	302132.346633	46.620673
2949.370668	300573.491619	46.625677
2945.546536	299013.468140	46.630682
2941.825070	297450.966540	46.635687
2938.130681	295907.558452	46.640692
2934.546658	294345.383018	46.645697
2931.221622	292795.954928	46.650701
2927.676450	291249.474309	46.655706
2923.581717	289702.964536	46.660711
2919.717258	288158.799311	46.665716
2916.268981	286601.701725	46.670721
2912.769869	285069.906177	46.675725
2909.022353	283523.731022	46.680730
2905.726776	281980.887973	46.685735
2901.772021	280443.435921	46.690740
2898.163541	278909.309351	46.695745
2894.350184	277380.759696	46.700749
2890.953597	275844.069286	46.705754
2887.074263	274306.101058	46.710759
2883.307271	272768.850646	46.715764
2879.188695	271236.745611	46.720769
2875.757661	269722.687049	46.725773
2872.017185	268206.869432	46.730778
2868.512983	266687.323869	46.735783
2864.673915	265169.080395	46.740788
2861.208849	263658.547961	46.745793
2857.061512	262155.587362	46.750797
2853.838848	260651.799592	46.755802
2850.260638	259145.501224	46.760807
2846.492952	257652.328473	46.765812
2842.719653	256146.227562	46.770817
2839.503468	254650.972836	46.775821
2835.604001	253154.153491	46.780826
2831.972114	251655.239586	46.785831
2828.276685	250171.448499	46.790836
2824.472200	248672.991794	46.795841
2820.818670	247190.950580	46.800845
2817.183727	245699.726217	46.805850
2813.465442	244215.430972	46.810855
2810.080258	242730.029153	46.815860
2806.524061	241258.270092	46.820865
2802.538200	239776.000298	46.825869
2798.691299	238301.952699	46.830874
2795.653404	236829.223284	46.835879
2791.697249	235355.892680	46.840884
2787.975723	233881.934166	46.845889
2784.258913	232420.450020	46.850893
2780.830497	230946.360765	46.855898
2777.183132	229481.904474	46.860903
2773.103708	228022.301649	46.865908
2769.985166	226551.162369	46.870913
2766.494482	225118.844447	46.875917
2762.461484	223656.455986	46.880922
2759.066274	222197.763431	46.885927
2755.319323	220749.315013	46.890932
2752.033684	219289.895980	46.895937
2747.843879	217846.463052	46.900941
2744.332174	216387.697423	46.905946
2740.458769	214940.046346	46.910951
2736.943164	213510.274453	46.915956
2733.375400	212054.665969	46.920961
2729.986168	210616.609536	46.925965
2726.584340	209174.360149	46.930970
2722.571389	207736.518572	46.935975
2718.879338	206304.289488	46.940980
2715.442479	204865.713926	46.945985
2712.006474	203443.829763	46.950989
2708.156393	202008.497899	46.955994
2704.331985	200568.920653	46.960999
2700.780711	199153.099278	46.966004
2697.211890	197724.763757	46.971009
2693.492539	196301.456885	46.976013
2689.714563	194887.876098	46.981018
2686.403962	193463.031981	46.986023
2682.627067	192058.929169	46.991028
2679.137795	190631.292797	46.996033
2675.592348	189224.105380	47.001037
2671.752793	187808.628930	47.006042
2668.368958	186398.166913	47.011047
2664.367392	184991.818223	47.016052
2660.991998	183576.962542	47.021057
2657.043535	182174.210068	47.026061
2653.846109	180775.434883	47.031066
2650.020383	179367.256214	47.036071
2646.274256	177976.350634	47.041076
2643.036627	176574.210151	47.046081
2639.006775	175178.849609	47.051085
2635.480446	173782.186537	47.056090
2632.114031	172395.821701	47.061095
2628.526994	171002.807489	47.066100
2624.754617	169610.751789	47.071105
2621.124214	168226.668881	47.076109
2617.467726	166834.151797	47.081114
2613.934488	165457.516155	47.086119
2610.247549	164076.757221	47.091124
2606.659375	162680.966301	47.096129
2603.097602	161311.548389	47.101133
2599.301853	159939.701710	47.106138
2595.742875	158565.035237	47.111143
2591.710149	157196.977344	47.116148
2588.252998	155820.409804	47.121153
2584.421170	154464.155846	47.126157
2580.974481	153095.643369	47.131162
2577.150326	151727.006636	47.136167
2573.638879	150380.701225	47.141172
2569.916948	149023.250756	47.146177
2566.693923	147667.245457	47.151181
2562.796181	146308.479325	47.156186
2559.438586	144882.542581	47.161191
2555.552768	143533.276932	47.166196
2552.544800	142181.747329	47.171201
2548.728468	140843.575530	47.176205
2544.840657	139500.133648	47.181210
2541.275225	138153.498538	47.186215
2537.406028	136811.822279	47.191220
2534.049367	135471.936794	47.196225
2530.315198	134144.782402	47.201229
2526.843648	132809.789933	47.206234
2523.356545	131472.652250	47.211239
2519.569444	130146.440400	47.216244
2515.935616	128809.776922	47.221249
2512.251941	127485.336176	47.226253
2508.537670	126159.352321	47.231258
2504.674479	124847.208972	47.236263
2501.291275	123534.956590	47.241268
2497.972502	122209.395835	47.246273
2494.544056	120903.329098	47.251277
2490.418802	119579.801696	47.256282
2486.953798	118264.762037	47.261287
2483.066081	116955.022102	47.266292
2479.587009	115662.811670	47.271297
2476.216059	114342.782446	47.276301
2472.539647	113039.110806	47.281306
2468.358645	111741.477106	47.286311
2465.068199	110451.353974	47.291316
2461.846145	109151.248714	47.296321
2458.159688	107864.879960	47.301325
2454.616365	106569.141841	47.306330
2451.441976	105271.742319	47.311335
2447.801531	103984.062550	47.316340
2444.145222	102684.041223	47.321345
2440.168517	101387.870500	47.326349
2436.079119	100099.572527	47.331354
2432.897700	98813.102671	47.336359
2429.001894	97535.247520	47.341364
2425.834789	96252.106335	47.346369
2422.198654	94977.389071	47.351373
2418.374987	93694.988784	47.356378
2414.864494	92421.716324	47.361383
2411.148213	91157.766610	47.366388
2407.144862	89885.337870	47.371393
2403.737665	88616.719482	47.376397
2399.815499	87350.103306	47.381402
2396.615111	86093.122036	47.386407
2392.756029	84840.744185	47.391412
2389.065748	83584.811733	47.396417
2385.438237	82346.593897	47.401421
2381.379123	81093.343745	47.406426
2378.215714	79841.647657	47.411431
2374.492427	78608.194158	47.416436
2371.022123	77370.120277	47.421441
2367.209481	76129.298224	47.426445
2363.402151	74904.482176	47.431450
2359.818868	73679.572281	47.436455
2356.046537	72437.567294	47.441460
2352.898441	71219.152846	47.446465
2348.896306	69995.366990	47.451469
2345.319417	68781.309979	47.456474
2341.951919	67554.797011	47.461479
2338.181172	66351.663124	47.466484
2335.013130	65134.432318	47.471489
2331.247546	63926.074172	47.476493
2327.406041	62700.262718	47.481498
2323.760610	61503.781966	47.486503
2320.218140	60302.653105	47.491508
2316.680647	59109.070090	47.496513
2312.590547	57914.381792	47.501517
2308.756346	56717.339243	47.506522
2305.526075	55521.765455	47.511527
2302.126187	54343.128998	47.516532
2298.317969	53152.269159	47.521537
2294.692856	51978.036405	47.526541
2290.843452	50803.599505	47.531546
2287.121614	49624.254273	47.536551
2283.318667	48456.069374	47.541556
2279.903979	47287.629546	47.546561
2276.035122	46122.047879	47.551565
2272.137215	44971.421658	47.556570
2268.742858	43806.570367	47.561575
2264.850234	42660.031876	47.566580
2261.105631	41513.136339	47.571585
2257.701414	40378.446563	47.576589
2254.184859	39232.452308	47.581594
2250.336023	38108.658767	47.586599
2246.464827	36972.146407	47.591604
2242.661653	35839.277852	47.596609
2239.258534	34714.450894	47.601613
2235.193012	33604.087057	47.606618
2231.649349	32484.712270	47.611623
2227.703906	31371.962766	47.616628
2223.886647	30278.981540	47.621633
2220.032190	29195.164051	47.626637
2216.217971	28109.458099	47.631642
2212.179061	27026.284358	47.636647
2208.206785	25953.416149	47.641652
2204.672908	24891.896447	47.646657
2200.824787	23832.699219	47.651661
2196.868802	22780.207814	47.656666
2192.957213	21736.133430	47.661671
2188.926892	20703.623525	47.666676
2185.107030	19679.597279	47.671681
2180.870354	18685.984971	47.676685
2176.650167	17684.725196	47.681690
2172.393820	16697.098086	47.686695
2168.309356	15741.818130	47.691700
2163.453657	14796.623205	47.696705
2157.872710	13899.135136	47.701709
2152.504724	13016.026671	47.706714
2147.400815	12156.747729	47.711719
2142.002741	11346.563142	47.716724
2136.901144	10543.008508	47.721729
2132.032725	9780.840807	47.726733
2126.857986	9040.998411	47.731738
2122.232668	8334.369510	47.736743
2117.654187	7653.796670	47.741748
2112.873893	7007.779329	47.746753
2107.761974	6396.207656	47.751757
2103.210294	5804.750789	47.756762
2097.884923	5256.101006	47.761767
2092.326189	4755.426466	47.766772
2086.673867	4268.229722	47.771777
2082.179176	3826.569587	47.776781
2076.987682	3415.629132	47.781786
2072.466878	3020.155328	47.786791
2067.594551	2664.384174	47.791796
2063.200011	2324.132263	47.796801
2059.053293	1999.602406	47.801805
2055.299227	1711.432804	47.806810
2051.542681	1424.907200	47.811815
2047.512271	1166.025635	47.816820
2043.813835	905.532861	47.821825
2039.672321	674.420753	47.826829
2035.808783	454.468344	47.831834
2031.829257	262.372471	47.836839
2025.399699	127.933817	47.841844
2014.250933	161.341964	47.846849
2006.321234	165.844587	47.851853
2002.136341	171.874703	47.856858
2000.234106	159.153026	47.861863
1997.548853	175.553709	47.866868
1996.238039	167.820629	47.871873
1994.080061	168.664423	47.876877
1991.686361	164.176052	47.881882
1989.184134	169.541067	47.886887
1985.888314	165.146399	47.891892
1982.675001	168.044147	47.896897
1979.304165	170.675470	47.901901
1976.091648	166.125397	47.906906
1973.201264	167.678603	47.911911
1969.658024	176.231157	47.916916
1966.265395	173.547464	47.921921
1963.193975	169.709329	47.926925
1959.755464	165.118692	47.931930
1956.346054	164.304300	47.936935
1952.788731	166.120065	47.941940
1949.835875	170.400798	47.946945
1946.356410	171.587432	47.951949
1942.779100	172.621694	47.956954
1940.047571	175.327002	47.961959
1936.501103	171.990330	47.966964
1932.635302	163.783847	47.971969
1929.597944	165.910572	47.976973
1926.041863	169.611804	47.981978
1923.178428	160.169604	47.986983
1919.728418	166.053112	47.991988
1916.241447	152.111422	47.996993
1912.139718	169.281106	48.001997
1908.359753	168.499405	48.007002
1905.497368	166.093439	48.012007
1902.278655	164.091257	48.017012
1898.729807	164.633847	48.022017
1895.615250	168.177409	48.027021
1892.254735	162.483066	48.032026
1889.151034	165.699054	48.037031
1885.312445	169.257840	48.042036
1881.845849	165.449932	48.047041
1878.171626	160.127397	48.052045
1874.582780	160.616141	48.057050
1871.229947	153.642413	48.062055
1867.287842	159.489041	48.067060
1864.501273	156.194840	48.072065
1861.244770	149.310450	48.077069
1857.443629	152.075585	48.082074
1854.741193	149.416811	48.087079
1850.710245	152.398249	48.092084
1847.268353	157.407283	48.097089
1843.887831	153.506827	48.102093
1840.258959	155.672354	48.107098
1836.899626	154.587568	48.112103
1833.492894	155.883081	48.117108
1829.599693	159.599130	48.122113
1826.451762	151.103185	48.127117
1822.503467	152.863112	48.132122
1819.282245	155.414119	48.137127
1815.912012	160.377147	48.142132
1812.588206	160.356187	48.147137
1809.409018	160.850449	48.152141
1805.741548	154.087340	48.157146
1802.019029	166.338045	48.162151
1798.419531	152.281137	48.167156
1794.904516	160.016206	48.172161
1791.608121	156.418986	48.177165
1788.233949	151.568403	48.182170
1784.944745	147.201249	48.187175
1781.328021	152.626813	48.192180
1778.197541	157.375156	48.197185
1774.695004	146.890886	48.202189
1770.668152	156.879617	48.207194
1767.581210	148.782286	48.212199
1763.900864	153.689451	48.217204
1760.139165	150.709242	48.222209
1757.026019	151.680417	48.227213
1753.385489	152.098194	48.232218
1750.094776	152.717498	48.237223
1746.537152	151.793491	48.242228
1742.911990	154.255871	48.247233
1739.231295	153.385929	48.252237
1736.296735	149.156284	48.257242
1732.902070	148.197288	48.262247
1729.043815	154.065639	48.267252
1725.538984	146.372255	48.272257
1722.314975	142.808028	48.277261
1718.630117	160.504147	48.282266
1714.967276	147.257648	48.287271
1711.143885	144.992649	48.292276
1707.749803	151.035142	48.297281
1704.640312	144.542268	48.302285
1701.040546	146.934245	48.307290
1697.870626	152.615784	48.312295
1694.217874	144.556412	48.317300
1690.423790	145.795530	48.322305
1687.235226	145.883161	48.327309
1683.818183	149.379202	48.332314
1680.479169	147.278860	48.337319
1676.825798	153.168947	48.342324
1673.018456	145.703268	48.347329
1669.808517	140.260703	48.352333
1666.237593	142.341286	48.357338
1662.960960	144.353665	48.362343
1658.963275	137.063322	48.367348
1655.266090	146.241167	48.372353
1652.706641	143.227870	48.377357
1649.047033	155.228308	48.382362
1645.592953	142.914142	48.387367
1641.607277	136.036391	48.392372
1638.066515	151.767372	48.397377
1634.825085	142.147157	48.402381
1631.166983	145.288625	48.407386
1627.902946	144.385152	48.412391
1624.604231	136.488707	48.417396
1620.717992	139.732324	48.422401
1617.432864	137.718487	48.427405
1614.033662	139.800685	48.432410
1610.442912	137.679655	48.437415
1606.537121	144.713445	48.442420
1603.277766	136.089495	48.447425
1599.795059	132.034278	48.452429
1596.281197	146.356312	48.457434
1592.870917	145.811106	48.462439
1589.232378	136.363799	48.467444
1586.104732	138.656610	48.472449
1582.653471	130.587903	48.477453
1578.615374	140.736635	48.482458
1575.473852	132.239792	48.487463
1572.004399	142.343820	48.492468
1568.145984	141.147408	48.497473
1564.823410	133.659693	48.502477
1561.011442	144.333038	48.507482
1557.977830	139.470372	48.512487
1554.505195	132.347843	48.517492
1550.983101	134.452458	48.522497
1547.669893	140.738604	48.527501
1544.001547	140.692562	48.532506
1540.450380	135.246504	48.537511
1536.825930	143.944751	48.542516
1533.085846	140.110179	48.547521
1530.123497	130.402037	48.552525
1526.288947	142.192593	48.557530
1523.038915	133.007219	48.562535
1519.350483	140.772662	48.567540
1515.888898	142.643188	48.572545
1512.486435	123.949061	48.577549
1508.862602	136.715898	48.582554
1505.510390	131.283009	48.587559
1502.009976	130.989229	48.592564
1498.373308	130.514292	48.597569
1495.323424	127.672720	48.602573
1491.381224	140.669733	48.607578
1487.825876	134.616896	48.612583
1484.092608	131.021731	48.617588
1481.013307	137.799641	48.622593
1477.702201	143.000285	48.627597
1474.251099	142.575406	48.632602
1470.373027	142.068660	48.637607
1466.785279	138.099538	48.642612
1463.378084	137.838637	48.647617
1459.981955	138.866848	48.652621
1456.403269	145.188247	48.657626
1452.989139	141.017943	48.662631
1449.565752	138.646144	48.667636
1445.838113	142.880587	48.672641
1442.911708	133.287076	48.677645
1439.016454	136.829568	48.682650
1435.364257	129.516891	48.687655
1431.549463	131.224426	48.692660
1428.019868	133.997824	48.697665
1425.054780	131.943449	48.702669
1421.462964	138.564311	48.707674
1418.230373	134.501650	48.712679
1414.464683	129.684023	48.717684
1410.991802	132.233409	48.722689
1407.613549	128.585868	48.727693
1403.903399	133.026398	48.732698
1400.789326	130.213887	48.737703
1397.158027	126.479407	48.742708
1393.343195	132.277788	48.747713
1389.867533	136.362072	48.752717
1386.367922	138.415766	48.757722
1383.041778	132.317603	48.762727
1379.351215	130.398950	48.767732
1375.797715	133.603224	48.772737
1372.457389	127.741409	48.777741
1368.900294	137.084068	48.782746
1365.731034	133.555691	48.787751
1362.157578	131.852837	48.792756
1358.113048	131.188690	48.797761
1354.783350	137.002895	48.802765
1351.423837	136.127115	48.807770
1348.153513	134.266081	48.812775
1344.283757	128.382746	48.817780
1340.599818	126.697195	48.822785
1337.625349	128.263731	48.827789
1333.512918	138.000222	48.832794
1330.324351	131.057949	48.837799
1327.260328	129.161465	48.842804
1323.354316	134.047143	48.847809
1320.269073	130.809357	48.852813
1316.320136	132.541098	48.857818
1312.877858	122.076086	48.862823
1309.488229	117.696358	48.867828
1305.879801	134.868036	48.872833
1302.633359	126.811678	48.877837
1299.001698	127.731277	48.882842
1295.557694	126.049313	48.887847
1292.061202	114.324110	48.892852
1287.973429	127.037069	48.897857
1284.906909	121.062825	48.902861
1281.430811	128.421764	48.907866
1277.694992	126.266622	48.912871
1274.450762	128.486023	48.917876
1270.760022	124.824176	48.922881
1267.248291	115.974118	48.927885
1263.920887	127.068402	48.932890
1260.556721	125.566946	48.937895
1256.989103	127.523759	48.942900
1253.614279	132.908449	48.947905
1249.898415	128.083093	48.952909
1246.325716	133.248820	48.957914
1242.716215	122.901768	48.962919
1239.734489	122.444623	48.967924
1235.880236	123.743947	48.972929
1232.358386	117.803038	48.977933
1229.070750	120.342465	48.982938
1225.637425	118.643038	48.987943
1222.035377	120.855194	48.992948
1217.871325	128.587611	48.997953
1214.633980	123.260243	49.002957
1210.988338	133.736799	49.007962
1207.630261	120.952227	49.012967
1204.323022	117.809350	49.017972
1201.326793	119.901361	49.022977
1197.697271	118.014355	49.027981
1193.598401	127.410236	49.032986
1190.495639	114.022548	49.037991
1187.193225	114.289518	49.042996
1182.876820	118.707969	49.048001
1179.584081	119.267661	49.053005
1176.290548	124.968682	49.058010
1172.780612	124.426569	49.063015
1169.430921	122.859604	49.068020
1166.193138	118.234692	49.073025
1162.747924	120.039494	49.078029
1158.826093	130.141677	49.083034
1155.169997	127.338175	49.088039
1151.277597	121.104127	49.093044
1147.922185	128.244890	49.098049
1145.199463	121.046261	49.103053
1141.452474	125.144625	49.108058
1138.134494	123.243669	49.113063
1134.574364	120.140409	49.118068
1130.506379	127.630023	49.123073
1127.345914	128.611959	49.128077
1123.891511	120.388913	49.133082
1120.525114	125.417975	49.138087
1116.938803	117.997048	49.143092
1113.426218	121.799290	49.148097
1109.510094	126.711936	49.153101
1105.760305	123.948434	49.158106
1102.888356	121.664443	49.163111
1099.661513	117.113775	49.168116
1096.002849	118.575523	49.173121
1092.224426	111.548526	49.178125
1088.270432	124.098228	49.183130
1085.217308	128.404361	49.188135
1081.730739	132.544236	49.193140
1078.318404	126.611552	49.198145
1075.042737	116.253445	49.203149
1071.464493	124.470011	49.208154
1067.941741	126.502125	49.213159
1064.522313	125.316282	49.218164
1060.386230	122.366502	49.223169
1057.322530	116.796869	49.228173
1053.698450	126.004564	49.233178
1050.325437	120.337825	49.238183
1046.901042	116.333809	49.243188
1043.255472	131.426404	49.248193
1039.673792	115.775704	49.253197
1036.185819	121.716020	49.258202
1032.664069	127.715413	49.263207
1029.441938	125.040173	49.268212
1025.380752	129.637035	49.273217
1022.163082	123.870053	49.278221
1018.514217	115.013102	49.283226
1015.337646	123.729953	49.288231
1012.035251	122.377107	49.293236
1008.346838	123.653717	49.298241
1004.740675	116.878202	49.303245
1000.954595	115.249908	49.308250
997.499581	118.192110	49.313255
994.645998	116.715213	49.318260
990.527799	120.919209	49.323265
987.395327	115.091447	49.328269
983.547472	113.665825	49.333274
980.491569	119.823251	49.338279
976.505004	117.947942	49.343284
973.041105	126.586405	49.348289
969.928792	121.027579	49.353293
966.187096	123.217398	49.358298
963.109753	120.260081	49.363303
959.374886	119.810214	49.368308
955.561275	124.589804	49.373313
952.383505	120.477604	49.378317
948.555934	125.892145	49.383322
945.019337	125.487171	49.388327
941.457058	123.624538	49.393332
938.085487	128.322266	49.398337
934.596578	117.282587	49.403341
931.260125	122.999892	49.408346
927.558118	122.586022	49.413351
924.340887	117.796629	49.418356
920.368926	123.815929	49.423361
917.328420	119.182368	49.428365
913.721879	118.595365	49.433370
910.160350	121.082867	49.438375
906.682232	120.425137	49.443380
903.032275	124.850085	49.448385
899.917565	107.329301	49.453389
896.409794	109.957087	49.458394
892.638799	123.572872	49.463399
889.293421	114.972185	49.468404
885.468112	128.175694	49.473409
881.884516	123.301311	49.478413
878.686241	125.535788	49.483418
875.509689	120.575525	49.488423
871.827339	119.491036	49.493428
867.856321	123.991580	49.498433
864.683596	118.606772	49.503437
861.438087	131.089902	49.508442
857.402973	128.652761	49.513447
853.939812	121.437295	49.518452
850.137712	124.427569	49.523457
846.913560	123.929413	49.528461
843.823702	129.025992	49.533466
840.117953	117.827319	49.538471
836.597684	120.017315	49.543476
833.045721	121.184039	49.548481
829.318284	119.344149	49.553485
825.824172	117.356991	49.558490
822.361447	122.844161	49.563495
819.386375	122.408254	49.568500
815.686468	127.970534	49.573505
812.316164	113.302436	49.578509
808.516788	125.771065	49.583514
805.009304	123.513921	49.588519
801.990165	118.598642	49.593524
797.960632	123.111538	49.598529
794.554387	121.996499	49.603533
791.032532	118.646935	49.608538
787.704360	120.775230	49.613543
784.191197	118.996719	49.618548
780.482048	123.706229	49.623553
777.121390	115.674305	49.628557
773.356189	117.697032	49.633562
769.810949	110.902592	49.638567
766.707972	109.793859	49.643572
762.891121	120.461866	49.648577
759.749967	107.539138	49.653581
755.957041	112.771146	49.658586
752.369392	109.276876	49.663591
749.047768	109.926661	49.668596
745.290812	112.435333	49.673601
742.266274	107.666459	49.678605
738.887123	115.339410	49.683610
734.940995	113.638213	49.688615
731.537246	118.296750	49.693620
727.718596	123.162635	49.698625
724.364506	107.871940	49.703629
720.777674	110.980413	49.708634
717.264982	118.155420	49.713639
714.532763	106.209565	49.718644
710.676196	125.220432	49.723649
706.995116	122.332441	49.728653
703.480813	118.598910	49.733658
700.015866	109.362125	49.738663
696.593483	113.792634	49.743668
692.700490	112.842447	49.748673
689.248699	113.357612	49.753677
685.776760	120.969180	49.758682
682.281395	116.011464	49.763687
679.264792	115.139174	49.768692
675.865105	115.734771	49.773697
672.286991	104.886366	49.778701
668.209849	124.770194	49.783706
664.478072	119.966568	49.788711
661.638500	115.058021	49.793716
657.668443	111.209221	49.798721
654.894039	105.331842	49.803725
651.002416	107.583225	49.808730
647.235115	111.722912	49.813735
643.794646	112.457787	49.818740
640.225801	113.032431	49.823745
636.799716	106.304814	49.828749
633.491878	110.556050	49.833754
630.298035	106.126949	49.838759
626.868989	106.097565	49.843764
622.787941	118.904592	49.848769
619.531686	105.338721	49.853773
615.894116	104.351729	49.858778
612.382923	106.666936	49.863783
609.042914	106.674235	49.868788
605.239708	105.798612	49.873793
601.839886	110.288893	49.878797
598.063697	110.661906	49.883802
594.657908	103.700172	49.888807
591.385143	102.817410	49.893812
587.822838	115.843764	49.898817
584.697403	107.351139	49.903821
580.882251	104.022289	49.908826
577.170490	106.536602	49.913831
573.715760	107.090236	49.918836
570.592985	99.957637	49.923841
567.414357	105.378245	49.928845
563.184986	108.157131	49.933850
559.524269	103.772705	49.938855
556.330435	96.999260	49.943860
552.737031	110.764491	49.948865
549.185917	104.524737	49.953869
545.659357	106.658875	49.958874
542.416316	105.954976	49.963879
539.005524	100.401941	49.968884
535.484606	107.511851	49.973889
531.971478	100.671363	49.978893
528.445278	102.058794	49.983898
524.860035	106.103572	49.988903
521.363182	103.392458	49.993908
517.516178	106.089330	49.998913
514.348710	102.719180	50.003917
510.975675	111.327723	50.008922
507.163528	106.141286	50.013927
504.007440	104.613851	50.018932
499.910219	110.187846	50.023937
496.363566	111.540527	50.028941
493.084831	107.403190	50.033946
489.591165	111.693070	50.038951
486.314314	103.369739	50.043956
482.403136	112.315682	50.048961
479.241619	109.343250	50.053965
476.029602	113.851617	50.058970
472.266195	113.251393	50.063975
468.954736	102.364488	50.068980
465.336224	116.073568	50.073985
461.656420	110.575353	50.078989
458.259739	103.229433	50.083994
454.610900	105.417558	50.088999
451.466399	101.303507	50.094004
447.636070	116.763710	50.099009
444.338960	109.142766	50.104013
440.829214	113.406708	50.109018
437.229904	109.072829	50.114023
433.958381	104.947041	50.119028
430.014796	110.379940	50.124033
426.782884	104.555321	50.129037
423.001048	115.660882	50.134042
419.204443	119.311695	50.139047
416.072400	107.520337	50.144052
412.600883	118.343176	50.149057
409.539935	119.771675	50.154061
406.281249	112.363030	50.159066
402.377280	121.678041	50.164071
398.585357	121.702419	50.169076
394.729681	126.175591	50.174081
391.494845	120.500138	50.179085
387.948864	108.985603	50.184090
384.119930	121.566558	50.189095
381.450675	116.378329	50.194100
377.956672	116.742034	50.199105
374.465027	115.305171	50.204109
370.578865	116.030866	50.209114
366.933646	112.321148	50.214119
364.168663	107.201707	50.219124
360.097883	119.187792	50.224129
356.589365	117.155622	50.229133
353.416925	118.000484	50.234138
349.340168	120.284156	50.239143
346.104127	116.380636	50.244148
343.090227	108.629951	50.249153
339.053868	104.152603	50.254157
335.824876	112.026783	50.259162
332.146131	117.019599	50.264167
328.446330	107.832432	50.269172
324.472472	110.916253	50.274177
321.384985	111.975612	50.279181
318.073044	108.681951	50.284186
315.093915	110.357096	50.289191
311.637817	108.522381	50.294196
307.757649	116.932015	50.299201
304.026682	111.147653	50.304205
300.629080	109.208866	50.309210
296.578586	114.598454	50.314215
293.334884	105.032971	50.319220
290.022263	110.490473	50.324225
286.557183	107.774478	50.329229
283.248956	108.536229	50.334234
279.260306	103.368059	50.339239
276.803597	98.769843	50.344244
272.828203	113.474527	50.349249
268.959102	117.171557	50.354253
265.367164	113.241563	50.359258
261.790879	112.887367	50.364263
258.797579	101.732418	50.369268
254.978269	115.795720	50.374273
251.560170	112.812948	50.379277
247.741110	109.934119	50.384282
244.416400	114.956928	50.389287
240.566438	116.040845	50.394292
237.391179	111.083797	50.399297
234.196040	117.680863	50.404301
230.911469	110.662332	50.409306
227.389926	110.394488	50.414311
223.708645	100.761545	50.419316
219.651659	114.624806	50.424321
216.252249	113.467792	50.429325
212.974479	107.394177	50.434330
209.572510	110.733310	50.439335
206.110658	113.873016	50.444340
202.501071	113.049492	50.449345
198.636102	106.144048	50.454349
195.256739	109.802351	50.459354
191.829493	118.647280	50.464359
188.664079	106.962495	50.469364
185.304988	110.734686	50.474369
181.875657	104.805053	50.479373
178.226645	109.552819	50.484378
174.211216	114.244094	50.489383
171.041351	112.684137	50.494388
166.922457	108.283079	50.499393
163.813069	113.569579	50.504397
160.640957	111.484789	50.509402
156.859029	113.178185	50.514407
153.682196	108.759263	50.519412
149.787313	104.898929	50.524417
146.217514	116.423785	50.529421
143.597459	113.705179	50.534426
139.414046	111.971823	50.539431
135.757497	111.747314	50.544436
132.299024	110.773594	50.549441
128.532730	114.460902	50.554445
125.765793	106.978505	50.559450
122.034701	123.252175	50.564455
118.716396	104.782905	50.569460
114.727918	115.702641	50.574465
111.642892	110.595465	50.579469
107.615664	106.933058	50.584474
104.076655	116.732004	50.589479
101.257552	111.197189	50.594484
97.667288	109.510132	50.599489
93.908876	110.358304	50.604493
90.425779	106.344898	50.609498
86.702614	116.489080	50.614503
83.189953	107.361303	50.619508
79.849141	107.818184	50.624513
76.526236	113.078051	50.629517
73.137589	100.795542	50.634522
69.493907	98.781507	50.639527
65.779451	98.101024	50.644532
61.968771	104.452889	50.649537
58.505786	104.868808	50.654541
55.777825	108.656059	50.659546
52.060062	114.477677	50.664551
48.231827	106.345332	50.669556
44.536393	108.724420	50.674561
41.088843	103.322893	50.679565
37.776087	105.050400	50.684570
34.455999	104.415710	50.689575
31.078486	113.556619	50.694580
27.514791	117.054037	50.699585
23.951199	103.767566	50.704589
20.441398	104.712859	50.709594
16.452450	106.074915	50.714599
13.545608	101.003140	50.719604
10.203402	98.530604	50.724609
6.110734	107.043244	50.729613
2.563360	112.670503	50.734618