Thu Aug 25 13:18:42 2022

Number of Points = 9924

Depth (nm)	Load (N)	Time (s)
1.611802	101.651080	0.000000
1.888594	116.047150	0.005005
2.020148	122.961476	0.010010
2.056341	117.532977	0.015014
2.188966	115.879591	0.020019
1.714009	101.356198	0.025024
1.860263	102.003915	0.030029
1.614905	99.748522	0.035034
1.535613	83.024431	0.040038
0.866821	76.393433	0.045043
0.866803	67.556902	0.050048
0.521673	63.925082	0.055053
0.102680	50.582544	0.060058
0.276697	48.824602	0.065062
-0.261189	37.645743	0.070067
-0.101194	27.945760	0.075072
-0.677062	23.331366	0.080077
-1.094620	24.687518	0.085082
-0.997943	18.670603	0.090086
-1.699381	13.088789	0.095091
-2.201641	12.708646	0.100096
-2.389564	8.261264	0.105101
-2.620568	9.651461	0.110106
-2.795179	-5.140367	0.115110
-3.465870	3.623862	0.120115
-3.260096	3.246679	0.125120
-3.328166	-4.857813	0.130125
-4.270181	1.639376	0.135130
-4.421436	4.399644	0.140134
-4.919630	-2.172631	0.145139
-5.054646	-1.901630	0.150144
-4.862738	2.959398	0.155149
-5.023527	-6.699796	0.160154
-4.812545	-2.714959	0.165158
-5.406634	3.651787	0.170163
-6.115796	-1.871863	0.175168
-6.258963	1.421814	0.180173
-6.417393	4.825452	0.185178
-6.368096	-1.538375	0.190182
-7.071508	-6.775022	0.195187
-7.755071	-5.010196	0.200192
-7.458690	0.381793	0.205197
-8.220404	-1.121964	0.210202
-7.297098	-11.327501	0.215206
-7.668477	-0.772023	0.220211
-8.532888	-6.575069	0.225216
-8.519716	-7.947135	0.230221
-8.873267	-2.415348	0.235226
-8.851566	-13.991900	0.240230
-9.665540	-12.703353	0.245235
-10.005830	-1.988231	0.250240
-10.478081	-13.936644	0.255245
-10.761664	-2.255966	0.260250
-10.440421	-5.900431	0.265254
-10.434532	-11.343124	0.270259
-10.936342	-12.577553	0.275264
-10.650764	-19.003705	0.280269
-11.884213	-11.518055	0.285274
-11.925674	-14.574175	0.290278
-12.134009	-7.309253	0.295283
-11.949223	-4.924342	0.300288
-11.894784	-9.580537	0.305293
-13.206643	0.097238	0.310298
-13.319184	-4.947248	0.315302
-13.196820	-5.377801	0.320307
-13.151123	-1.332265	0.325312
-13.351137	4.074226	0.330317
-13.969547	1.519791	0.335322
-14.633221	-13.312460	0.340326
-14.677068	-5.598745	0.345331
-15.285054	-5.003700	0.350336
-14.951640	-7.517442	0.355341
-14.894576	-9.073556	0.360346
-14.928090	-7.888310	0.365350
-15.633459	-5.721433	0.370355
-16.116725	-11.245672	0.375360
-16.214890	1.010235	0.380365
-16.462674	-1.273239	0.385370
-16.560555	-11.002397	0.390374
-17.470807	-10.287225	0.395379
-17.547873	-7.671461	0.400384
-17.712348	-8.651859	0.405389
-17.966416	-6.717045	0.410394
-17.975091	-5.519873	0.415398
-18.067468	-5.480180	0.420403
-18.296742	-3.871955	0.425408
-18.817659	-5.831057	0.430413
-19.533556	5.854087	0.435418
-19.330750	-3.612139	0.440422
-19.724185	-0.089423	0.445427
-19.542057	3.741748	0.450432
-19.371680	-6.621069	0.455437
-20.529033	5.348379	0.460442
-20.661351	-1.040775	0.465446
-20.705658	4.597585	0.470451
-20.880557	-0.588993	0.475456
-20.816134	-8.942033	0.480461
-21.215209	-2.055349	0.485466
-21.944088	-1.011089	0.490470
-22.378797	3.040116	0.495475
-22.334312	7.149119	0.500480
-22.015070	0.398146	0.505485
-22.467317	6.543351	0.510490
-22.985216	-3.999528	0.515494
-23.428420	-1.158716	0.520499
-23.701752	-6.086259	0.525504
-23.029033	0.480632	0.530509
-23.768443	1.396829	0.535514
-24.640573	-5.955252	0.540518
-24.820689	-0.485441	0.545523
-25.253526	0.692769	0.550528
-25.052269	-6.761055	0.555533
-24.945847	-1.450035	0.560538
-24.906984	-10.086973	0.565542
-26.167903	-2.736220	0.570547
-26.649624	5.621913	0.575552
-26.396707	-1.707129	0.580557
-26.707526	3.238994	0.585562
-26.619681	-2.488626	0.590566
-26.674781	5.033866	0.595571
-27.206602	-0.773834	0.600576
-27.612926	-10.419861	0.605581
-28.421907	-3.111447	0.610586
-27.856650	-2.035838	0.615590
-28.189986	-0.667573	0.620595
-28.172049	-2.578226	0.625600
-28.842910	-8.718480	0.630605
-29.542705	-1.104468	0.635610
-29.292227	-7.205583	0.640614
-29.400983	0.973887	0.645619
-29.465309	4.675993	0.650624
-29.494909	-6.889359	0.655629
-30.314158	2.768182	0.660634
-30.820265	-5.403716	0.665638
-31.168147	0.652368	0.670643
-31.408991	2.515508	0.675648
-31.064448	-0.253081	0.680653
-31.216237	2.330100	0.685658
-31.798391	0.839340	0.690662
-32.396767	-2.044100	0.695667
-32.256830	5.403540	0.700672
-32.385839	-7.158642	0.705677
-32.514396	11.499170	0.710682
-32.539811	-1.152015	0.715686
-33.133543	8.954251	0.720691
-33.690451	2.599986	0.725696
-33.384358	3.263782	0.730701
-34.164002	-0.508749	0.735706
-35.095274	7.505370	0.740710
-34.952569	-1.938784	0.745715
-34.854839	1.469010	0.750720
-35.175326	-1.204870	0.755725
-35.029742	-1.629570	0.760730
-35.182609	-2.880707	0.765734
-35.460690	0.867545	0.770739
-36.060284	6.441049	0.775744
-36.778001	-1.020648	0.780749
-36.942875	-1.384049	0.785754
-37.128593	3.963254	0.790758
-36.895408	-6.548608	0.795763
-37.145085	-4.563862	0.800768
-36.961034	-7.826161	0.805773
-37.867722	-3.337171	0.810778
-38.299007	-4.775639	0.815782
-38.077027	-3.374160	0.820787
-38.281612	1.374982	0.825792
-38.581189	-3.703473	0.830797
-39.538549	6.200338	0.835802
-39.831083	-2.894044	0.840806
-39.799297	-4.234225	0.845811
-39.860220	1.663002	0.850816
-39.671358	-2.017669	0.855821
-40.046000	4.264073	0.860826
-40.495311	-4.372306	0.865830
-40.829525	1.365260	0.870835
-40.899385	4.792985	0.875840
-41.406810	0.813285	0.880845
-41.598946	-2.197081	0.885850
-41.470434	-1.467495	0.890854
-42.083965	3.962658	0.895859
-42.442493	0.298153	0.900864
-42.428076	-3.997430	0.905869
-42.945654	7.840139	0.910874
-42.907072	-3.881430	0.915878
-43.456931	-1.577565	0.920883
-44.137354	4.660339	0.925888
-44.190004	-4.487446	0.930893
-44.764498	-2.802983	0.935898
-44.396596	-8.650412	0.940902
-44.439300	-3.638733	0.945907
-44.775616	-4.819997	0.950912
-44.334827	-8.033937	0.955917
-44.969702	1.341613	0.960922
-45.609169	0.416657	0.965926
-45.840983	6.100215	0.970931
-46.011772	4.304554	0.975936
-45.823628	-4.589894	0.980941
-46.350745	3.857609	0.985946
-46.639714	-3.993968	0.990950
-47.346966	-3.180886	0.995955
-47.260666	-4.336619	1.000960
-47.411027	-4.370098	1.005965
-48.202418	2.188915	1.010970
-48.461336	-12.222694	1.015974
-48.512028	-4.938180	1.020979
-48.891008	1.059502	1.025984
-48.900990	-7.547635	1.030989
-48.642363	-4.297932	1.035994
-48.799918	-4.931400	1.040998
-49.697625	-3.088725	1.046003
-50.364163	-1.661924	1.051008
-50.204443	-2.114149	1.056013
-50.601497	-2.362076	1.061018
-50.543488	-8.398231	1.066022
-50.517451	3.895161	1.071027
-50.760911	-0.094259	1.076032
-51.128961	0.112015	1.081037
-51.933292	5.600540	1.086042
-51.760429	1.558542	1.091046
-51.711392	-9.234514	1.096051
-52.874111	7.645943	1.101056
-52.960571	1.452085	1.106061
-53.422839	5.513938	1.111066
-53.317012	-1.295345	1.116070
-53.491393	-1.888210	1.121075
-53.684878	4.032951	1.126080
-53.480230	-3.620722	1.131085
-53.747449	-2.057171	1.136090
-54.220534	2.870084	1.141094
-54.292711	-1.908642	1.146099
-54.686470	-2.732890	1.151104
-54.476115	-2.958931	1.156109
-55.900874	-5.453455	1.161114
-55.859823	1.009925	1.166118
-56.132589	4.036006	1.171123
-56.396700	1.318493	1.176128
-56.315284	-0.785605	1.181133
-56.284336	5.325018	1.186138
-56.254221	-2.101991	1.191142
-56.871018	-2.037075	1.196147
-57.416991	1.569655	1.201152
-57.701188	0.481465	1.206157
-57.799374	9.393275	1.211162
-58.098162	0.230272	1.216166
-58.538305	-2.459659	1.221171
-59.123707	1.210196	1.226176
-59.110759	-0.149180	1.231181
-58.919200	3.373625	1.236186
-59.173629	1.641691	1.241190
-59.139153	-5.729052	1.246195
-59.979369	9.496845	1.251200
-60.199336	1.583834	1.256205
-60.540528	2.073804	1.261210
-60.770208	5.880913	1.266214
-60.572148	6.890668	1.271219
-60.682767	3.627082	1.276224
-61.313420	2.523575	1.281229
-62.162833	-1.310787	1.286234
-62.111411	-8.314022	1.291238
-61.950679	-6.311324	1.296243
-62.254053	-3.293103	1.301248
-62.284444	2.795492	1.306253
-63.085509	15.547520	1.311258
-63.334482	9.980241	1.316262
-63.440742	3.140914	1.321267
-63.305415	1.132773	1.326272
-63.256295	-4.262910	1.331277
-64.136179	15.600962	1.336282
-64.827849	-1.773736	1.341286
-65.019365	6.655984	1.346291
-65.304206	5.166097	1.351296
-64.980332	4.428721	1.356301
-65.121967	4.957026	1.361306
-65.359176	4.775803	1.366310
-65.655902	4.360296	1.371315
-66.120707	-0.148101	1.376320
-66.465546	0.804350	1.381325
-66.436179	10.072662	1.386330
-66.739700	0.980004	1.391334
-67.095714	-0.767651	1.396339
-67.475392	8.412892	1.401344
-67.748225	11.606665	1.406349
-67.868984	14.498198	1.411354
-67.701122	12.937377	1.416358
-68.296596	4.475760	1.421363
-69.068263	9.443474	1.426368
-69.249389	7.807621	1.431373
-69.383597	14.902747	1.436378
-69.232676	9.532238	1.441382
-69.024869	9.018694	1.446387
-69.854858	7.085876	1.451392
-70.537988	4.149279	1.456397
-70.999449	8.609641	1.461402
-70.671864	-0.642015	1.466406
-70.707623	3.767461	1.471411
-71.237150	6.463614	1.476416
-70.627530	2.280414	1.481421
-71.367680	-0.735833	1.486426
-72.036128	0.805165	1.491430
-72.116693	-4.741040	1.496435
-72.086611	6.735466	1.501440
-72.384705	-8.267955	1.506445
-73.276072	-1.326281	1.511450
-73.353598	1.397124	1.516454
-73.330424	3.351774	1.521459
-73.633124	-0.296167	1.526464
-73.957271	0.839705	1.531469
-74.184371	-1.339439	1.536474
-74.453240	1.012149	1.541478
-74.496712	-0.135905	1.546483
-75.656083	7.967740	1.551488
-75.572228	3.110781	1.556493
-76.049301	-2.506174	1.561498
-75.812857	-0.572287	1.566502
-75.780030	-0.153576	1.571507
-75.980515	4.610743	1.576512
-75.711788	-4.919592	1.581517
-76.256095	-4.967273	1.586522
-77.321010	4.380749	1.591526
-77.278747	7.980731	1.596531
-77.450234	5.710615	1.601536
-77.499824	-8.252899	1.606541
-77.860411	12.890019	1.611546
-78.546409	3.971186	1.616550
-78.469977	5.607442	1.621555
-78.869652	11.788704	1.626560
-78.849496	4.790364	1.631565
-78.824153	4.972964	1.636570
-78.892831	6.277615	1.641574
-79.678942	7.245427	1.646579
-80.081255	4.790015	1.651584
-80.125542	7.201327	1.656589
-80.163582	4.612907	1.661594
-80.456664	10.657244	1.666598
-81.133694	12.082528	1.671603
-81.452363	3.571214	1.676608
-81.137356	4.882184	1.681613
-81.404359	5.876224	1.686618
-81.660755	4.498940	1.691622
-82.085765	2.268549	1.696627
-82.468512	9.937293	1.701632
-82.529264	-2.895010	1.706637
-82.513909	3.559741	1.711642
-83.060631	3.670626	1.716646
-83.683527	-1.664050	1.721651
-84.168713	4.059207	1.726656
-84.393823	-1.002439	1.731661
-84.391213	18.096729	1.736666
-84.531824	1.404482	1.741670
-84.359101	1.010330	1.746675
-84.917863	6.156656	1.751680
-84.842671	2.560235	1.756685
-85.470549	1.848603	1.761690
-85.386930	1.737333	1.766694
-85.540505	0.698280	1.771699
-86.748079	7.066243	1.776704
-86.928464	2.484807	1.781709
-86.769121	6.794110	1.786714
-86.978976	9.550906	1.791718
-86.847879	5.477487	1.796723
-87.231749	9.416324	1.801728
-87.241994	2.840366	1.806733
-88.337506	3.704797	1.811738
-88.692268	4.671459	1.816742
-88.453069	-1.503819	1.821747
-88.932551	-3.523193	1.826752
-88.745067	-1.546833	1.831757
-89.411984	-0.376235	1.836762
-89.211649	2.234029	1.841766
-89.335134	0.326553	1.846771
-90.301821	0.914534	1.851776
-90.465073	-1.742851	1.856781
-90.519841	-2.560103	1.861786
-90.750712	9.482478	1.866790
-90.309564	-2.583742	1.871795
-91.234005	-6.618315	1.876800
-91.105605	-6.587905	1.881805
-91.456617	-5.188395	1.886810
-91.687486	1.390358	1.891814
-92.218201	-2.626815	1.896819
-92.937562	-3.808169	1.901824
-93.217106	-0.179910	1.906829
-93.532037	-1.032327	1.911834
-93.268390	5.437302	1.916838
-93.213407	7.247762	1.921843
-93.660276	2.543568	1.926848
-93.757822	4.428548	1.931853
-93.799946	1.128921	1.936858
-94.602464	-1.576993	1.941862
-94.528047	3.112613	1.946867
-95.026808	-0.460313	1.951872
-94.983723	-9.860374	1.956877
-95.760760	-3.572531	1.961882
-96.188257	-0.443111	1.966886
-96.325136	3.466515	1.971891
-96.284950	-0.456616	1.976896
-96.351457	-0.272278	1.981901
-96.477346	4.138665	1.986906
-96.309794	-3.597779	1.991910
-96.922340	-4.606043	1.996915
-97.821166	-4.105230	2.006912
-97.081861	-6.540096	2.016909
-96.561522	-3.099200	2.026906
-96.783249	-4.952657	2.036902
-95.785179	-10.317117	2.046899
-95.370796	0.534066	2.056896
-94.436944	-1.677860	2.066893
-94.392814	-0.291117	2.076890
-93.853298	-1.316678	2.086886
-92.729053	-4.648165	2.096883
-92.631040	1.735286	2.106880
-92.490310	1.681375	2.116877
-91.906783	2.894901	2.126874
-91.218650	-0.051470	2.136870
-91.040288	-7.409927	2.146867
-89.905662	2.080282	2.156864
-89.912144	-0.564012	2.166861
-88.948352	-0.436443	2.176858
-88.410829	-0.767940	2.186854
-88.284018	-3.955809	2.196851
-88.202503	-1.016357	2.206848
-87.566783	4.421195	2.216845
-86.316877	3.667628	2.226842
-85.792024	2.964314	2.236838
-85.388966	-5.614116	2.246835
-85.529093	-6.371624	2.256832
-85.247609	-6.764371	2.266829
-84.380409	-7.632200	2.276826
-83.041562	-0.999683	2.286822
-83.244563	-4.427312	2.296819
-82.742442	-9.172365	2.306816
-82.631433	1.457092	2.316813
-81.851000	-7.224818	2.326810
-81.160830	-4.738701	2.336806
-80.674356	-6.047389	2.346803
-80.474148	-4.019860	2.356800
-79.507788	-3.357332	2.366797
-78.748554	-6.061417	2.376794
-78.774783	-9.089089	2.386790
-78.829218	-6.299398	2.396787
-77.820395	-0.502156	2.406784
-77.319835	-4.455011	2.416781
-76.261261	-4.668578	2.426778
-76.082336	-2.514169	2.436774
-75.939826	-6.426760	2.446771
-74.825289	-4.279568	2.456768
-74.781199	2.128172	2.466765
-74.566719	0.066981	2.476762
-73.740463	-4.789050	2.486758
-73.030572	-4.596354	2.496755
-72.288563	1.473947	2.506752
-71.842170	-1.098756	2.516749
-71.659910	1.897771	2.526746
-71.478038	-6.335555	2.536742
-70.573640	-4.507064	2.546739
-69.647314	-1.931236	2.556736
-69.725646	-0.021621	2.566733
-69.447544	-2.821380	2.576730
-68.629406	-5.547364	2.586726
-68.120898	-3.907099	2.596723
-67.804951	-4.565007	2.606720
-67.180361	-0.744464	2.616717
-66.805090	1.090909	2.626714
-65.721963	1.627436	2.636710
-65.206466	-3.189405	2.646707
-65.283733	3.446428	2.656704
-65.160229	-2.316360	2.666701
-64.240909	-7.544935	2.676698
-63.577307	-4.322888	2.686694
-62.483147	-4.374134	2.696691
-62.550398	0.882128	2.706688
-62.545295	-3.921265	2.716685
-62.002399	1.014479	2.726682
-61.133683	-7.177580	2.736678
-60.670686	2.120097	2.746675
-60.009714	0.118826	2.756672
-59.890268	0.122103	2.766669
-59.018511	-2.127607	2.776666
-58.434275	2.269468	2.786662
-58.262046	-0.589730	2.796659
-57.653001	0.293515	2.806656
-57.279563	0.041583	2.816653
-56.789937	-3.589609	2.826650
-55.810599	-2.913272	2.836646
-55.359613	-7.948088	2.846643
-55.238809	-5.724383	2.856640
-54.843406	-10.015555	2.866637
-54.331545	-6.858430	2.876634
-53.559351	-8.908805	2.886630
-52.596657	-6.215128	2.896627
-52.450676	-9.101890	2.906624
-52.463759	-10.554050	2.916621
-51.730747	-8.198187	2.926618
-51.121951	-2.059495	2.936614
-50.612857	-12.219439	2.946611
-49.939620	-9.733834	2.956608
-49.476660	-8.026242	2.966605
-49.382046	-7.021211	2.976602
-48.311803	-7.318966	2.986598
-48.368927	-6.458054	2.996595
-47.629830	-8.094595	3.006592
-46.704678	-9.164738	3.016589
-46.280492	-16.951352	3.026586
-46.268091	-14.051757	3.036582
-46.208988	-7.206044	3.046579
-45.365835	-4.655195	3.056576
-44.728421	-5.106878	3.066573
-43.990951	-6.033572	3.076570
-43.658736	-2.050007	3.086566
-42.947559	-7.635610	3.096563
-42.596799	-1.713078	3.106560
-42.253981	-1.133411	3.116557
-40.996404	-4.840579	3.126554
-40.810032	-7.220483	3.136550
-40.459596	-1.500641	3.146547
-40.181803	-8.957043	3.156544
-39.872717	-8.451286	3.166541
-38.847493	-14.672138	3.176538
-38.789514	-1.927772	3.186534
-37.911537	-7.631376	3.196531
-37.470668	-6.715444	3.206528
-37.344279	-13.923206	3.216525
-36.362563	-5.150299	3.226522
-35.945515	1.170496	3.236518
-36.067520	-3.308871	3.246515
-35.140352	-1.008770	3.256512
-34.728324	-2.654252	3.266509
-34.094630	-6.317520	3.276506
-33.733129	-5.975198	3.286502
-33.048009	-1.831515	3.296499
-32.394904	-2.272985	3.306496
-32.200360	-3.396546	3.316493
-31.434622	-1.790246	3.326490
-30.607071	-4.574724	3.336486
-30.622687	-4.610472	3.346483
-30.426422	-7.026773	3.356480
-29.533841	-2.833233	3.366477
-29.385011	-4.947494	3.376474
-28.291454	-0.183557	3.386470
-27.964984	-9.317026	3.396467
-27.732476	-4.655764	3.406464
-27.229141	-12.822249	3.416461
-26.616173	-4.146786	3.426458
-25.791659	-13.253751	3.436454
-25.212151	-6.058752	3.446451
-25.181209	-9.355144	3.456448
-25.163406	-6.747833	3.466445
-23.933886	-8.157103	3.476442
-23.567769	-10.790085	3.486438
-22.728359	-13.205784	3.496435
-22.444585	-8.340312	3.506432
-22.024344	-4.053756	3.516429
-21.614027	-5.439208	3.526426
-20.383646	-14.742813	3.536422
-20.208694	-6.252145	3.546419
-20.570081	-7.861976	3.556416
-20.173771	-14.038140	3.566413
-19.288118	-6.827752	3.576410
-18.179331	-8.816822	3.586406
-17.761224	-9.680804	3.596403
-17.402116	-1.488252	3.606400
-17.297182	-12.513043	3.616397
-16.509321	-7.853265	3.626394
-16.158931	-10.312720	3.636390
-15.439523	-4.919953	3.646387
-15.018215	-8.955422	3.656384
-14.741781	-9.762361	3.666381
-13.731669	-9.721237	3.676378
-13.460992	-7.587538	3.686374
-13.156054	-9.637559	3.696371
-12.122225	-19.483740	3.706368
-11.923245	-16.569029	3.716365
-11.882227	-6.343586	3.726362
-11.349222	-12.218052	3.736358
-10.770789	-2.998646	3.746355
-9.611838	-6.775888	3.756352
-9.140955	-7.850880	3.766349
-9.310943	-5.404214	3.776346
-8.766832	-3.449572	3.786342
-7.737283	-6.832737	3.796339
-7.736357	-3.066528	3.806336
-7.009180	-4.783561	3.816333
-6.057551	-11.445880	3.826330
-5.896220	-11.287606	3.836326
-5.981615	-9.671491	3.846323
-5.058284	-9.271478	3.856320
-4.602415	-6.460371	3.866317
-3.672552	1.050375	3.876314
-3.415568	5.935889	3.886310
-3.396232	10.842801	3.896307
-3.348854	20.148595	3.906304
-2.682112	31.242206	3.916301
-2.021455	48.289127	3.926298
-1.727607	59.878342	3.936294
-0.985521	84.366445	3.946291
-0.622815	100.655470	3.956288
0.000000	116.859686	3.961293
0.316930	119.736444	3.966298
0.362076	119.106013	3.971302
0.438550	118.366268	3.976307
0.544249	119.798632	3.981312
0.605454	145.314429	3.986317
1.030936	147.433855	3.991322
1.081935	133.169719	3.996326
0.725087	131.551893	4.001331
1.012236	120.091853	4.006336
0.782092	125.749877	4.011341
0.883378	118.656517	4.016346
0.831832	123.555723	4.021350
0.690454	131.398676	4.026355
0.726080	131.601813	4.031360
0.709180	141.750655	4.036365
1.072440	145.790762	4.041370
0.866842	150.337620	4.046374
1.102770	154.783663	4.051379
1.374688	142.512898	4.056384
1.097383	139.674040	4.061389
1.268649	129.497667	4.066394
0.809338	135.308661	4.071398
0.651636	130.818547	4.076403
1.149695	134.726799	4.081408
0.786685	141.576249	4.086413
1.032007	132.802488	4.091418
1.168797	138.026533	4.096422
1.109712	136.795493	4.101427
1.039057	127.217018	4.106432
0.915421	140.062313	4.111437
1.251197	139.307251	4.116442
1.109906	137.766383	4.121446
1.300702	129.228960	4.126451
1.365795	127.690559	4.131456
1.288414	136.061332	4.136461
1.134855	137.635559	4.141466
1.230356	131.830764	4.146470
1.242840	137.191346	4.151475
1.321287	128.437405	4.156480
1.107308	132.824219	4.161485
0.934187	125.970005	4.166490
0.906669	135.506732	4.171494
1.121742	142.461763	4.176499
1.379787	139.728853	4.181504
1.271778	150.879078	4.186509
1.341353	151.728639	4.191514
1.354873	143.022830	4.196518
1.710090	140.230401	4.201523
1.469575	138.353899	4.206528
1.163710	135.658723	4.211533
1.119350	130.040359	4.216538
0.930222	135.919753	4.221542
1.246416	153.337431	4.226547
1.591812	138.486155	4.231552
1.492486	155.617757	4.236557
1.334975	152.029290	4.241562
1.822588	144.489407	4.246566
1.242698	138.265241	4.251571
1.526839	133.895725	4.256576
1.061106	151.477043	4.261581
1.531092	147.274561	4.266586
1.875455	146.483351	4.271590
1.547029	155.064311	4.276595
1.513591	132.527424	4.281600
1.101593	143.102007	4.286605
1.360645	155.707018	4.291610
1.802416	147.528901	4.296614
1.496231	155.967170	4.301619
1.846059	149.388521	4.306624
1.591875	157.071987	4.311629
1.658040	155.745390	4.316634
1.812316	145.277438	4.321638
1.441931	148.024605	4.326643
1.565513	158.458333	4.331648
1.655070	154.688784	4.336653
1.783329	147.417178	4.341658
1.619508	151.520887	4.346662
1.581799	150.378246	4.351667
1.451226	152.034296	4.356672
1.590323	162.927510	4.361677
1.618325	155.244497	4.366682
1.806197	161.767193	4.371686
1.563535	157.543488	4.376691
1.460803	158.568745	4.381696
1.535909	155.639865	4.386701
1.627911	149.550871	4.391706
1.574664	153.994765	4.396710
1.281434	159.229244	4.401715
1.627003	145.959833	4.406720
1.671509	159.247040	4.411725
2.064318	165.456051	4.416730
1.945750	173.947191	4.421734
1.687547	167.175896	4.426739
2.021387	168.797148	4.431744
1.622001	172.137329	4.436749
2.049976	177.844118	4.441754
2.138036	180.924427	4.446758
1.890831	175.720651	4.451763
2.136182	169.031812	4.456768
1.214455	179.448996	4.461773
1.789823	183.614068	4.466778
1.893240	176.757636	4.471782
2.107885	181.143744	4.476787
2.464676	179.705170	4.481792
2.392959	178.675425	4.486797
1.904415	176.543547	4.491802
2.252975	176.571102	4.496806
1.887190	180.826687	4.501811
2.078783	175.408624	4.506816
2.178525	184.900128	4.511821
2.055970	178.658076	4.516826
2.561575	180.980092	4.521830
1.921307	171.054236	4.526835
1.903544	163.008224	4.531840
1.862458	166.690904	4.536845
2.192836	176.307620	4.541850
2.320301	177.907424	4.546854
1.836991	183.943660	4.551859
1.973739	170.830337	4.556864
1.832227	178.727116	4.561869
1.942250	173.438896	4.566874
2.303703	178.956788	4.571878
1.942108	177.187840	4.576883
2.232648	171.159481	4.581888
1.977384	180.143448	4.586893
2.170699	184.776511	4.591898
2.285412	181.034653	4.596902
2.092551	177.027770	4.601907
2.243881	184.663531	4.606912
2.274921	199.822685	4.611917
2.350633	196.324219	4.616922
2.339724	203.915804	4.621926
2.603370	206.693356	4.626931
2.551789	188.313318	4.631936
2.216537	189.121903	4.636941
2.372717	190.483088	4.641946
2.666909	198.359066	4.646950
2.464908	184.998247	4.651955
1.790024	186.685799	4.656960
2.075709	203.219277	4.661965
2.005873	206.995056	4.666970
2.454799	196.936496	4.671974
2.367417	201.531284	4.676979
2.472108	193.627427	4.681984
2.416971	206.136166	4.686989
2.360539	204.525049	4.691994
2.567851	190.590722	4.696998
2.584878	205.071858	4.702003
2.316506	200.216246	4.707008
2.792063	202.441730	4.712013
2.522194	198.222278	4.717018
2.590664	200.641261	4.722022
2.569366	212.303130	4.727027
2.777072	201.864739	4.732032
2.748388	204.735550	4.737037
2.325909	211.417171	4.742042
2.920935	208.618797	4.747046
2.325934	214.188480	4.752051
2.707087	207.298012	4.757056
2.776049	207.875584	4.762061
2.478194	202.220984	4.767066
2.864041	210.576161	4.772070
2.724420	229.039783	4.777075
3.071094	221.705450	4.782080
3.046836	220.222171	4.787085
2.442448	212.647707	4.792090
2.633833	210.431439	4.797094
2.400935	223.094594	4.802099
2.676591	227.771716	4.807104
2.799054	231.662906	4.812109
2.620231	223.999613	4.817114
2.962899	227.460825	4.822118
2.430455	224.658764	4.827123
2.773585	229.122830	4.832128
2.592682	223.905488	4.837133
2.689032	234.397312	4.842138
2.888812	233.600278	4.847142
2.966677	233.293753	4.852147
2.853114	232.416097	4.857152
2.975525	225.917344	4.862157
2.948866	234.805408	4.867162
2.688266	228.113561	4.872166
2.293781	238.571559	4.877171
2.832762	243.757930	4.882176
3.119615	253.460603	4.887181
3.102515	251.156771	4.892186
3.123305	257.683535	4.897190
2.819659	250.542834	4.902195
3.317411	257.864916	4.907200
2.944753	263.864858	4.912205
2.753014	254.400201	4.917210
3.083037	252.734857	4.922214
2.796092	249.894327	4.927219
3.203108	249.542557	4.932224
2.920425	241.816434	4.937229
3.084932	248.374461	4.942234
3.368322	254.936012	4.947238
3.055156	257.411633	4.952243
3.077136	251.276627	4.957248
3.278817	246.891530	4.962253
3.302051	248.102703	4.967258
3.335799	245.851017	4.972262
3.312151	252.144292	4.977267
3.496138	258.515770	4.982272
3.154813	255.187041	4.987277
3.040023	256.334417	4.992282
3.349716	252.274087	4.997286
3.300577	257.283685	5.002291
3.327219	245.465740	5.007296
3.546930	245.722296	5.012301
2.993839	248.649967	5.017306
3.200989	249.822833	5.022310
3.044894	250.467307	5.027315
2.969030	244.236900	5.032320
3.665477	266.302863	5.037325
3.862873	270.916326	5.042330
3.656912	262.690945	5.047334
3.314321	255.252618	5.052339
3.215554	248.345578	5.057344
3.245807	247.942107	5.062349
3.499320	254.922797	5.067354
3.620003	252.094331	5.072358
3.312373	254.420386	5.077363
3.613105	252.645734	5.082368
3.591333	259.043123	5.087373
3.289663	256.518116	5.092378
3.352319	268.423138	5.097382
3.103831	277.776258	5.102387
3.655590	270.479377	5.107392
3.709022	275.770309	5.112397
3.608301	274.055390	5.117402
3.774316	272.029756	5.122406
3.622004	274.745938	5.127411
3.757927	273.996872	5.132416
3.629383	277.804012	5.137421
3.487339	277.550924	5.142426
3.395258	266.694385	5.147430
3.337662	276.837024	5.152435
3.471254	267.897202	5.157440
3.092979	270.993643	5.162445
3.534981	276.286970	5.167450
3.866262	273.393865	5.172454
3.508335	275.205773	5.177459
3.799755	271.493158	5.182464
3.955360	279.577552	5.187469
3.564894	278.993221	5.192474
3.776728	282.579348	5.197478
3.687526	294.669535	5.202483
3.591645	298.911332	5.207488
3.855457	301.574975	5.212493
3.717581	303.482125	5.217498
4.294897	304.622307	5.222502
3.920805	303.848743	5.227507
4.259581	299.034020	5.232512
3.799384	289.892986	5.237517
3.912991	286.436023	5.242522
4.117170	284.768246	5.247526
3.606258	284.307192	5.252531
3.814638	282.806440	5.257536
4.315873	289.378165	5.262541
3.818290	284.106016	5.267546
4.099434	286.380955	5.272550
3.946123	297.734527	5.277555
4.179646	296.286783	5.282560
3.757701	280.688730	5.287565
3.954699	303.449937	5.292570
4.245883	288.429857	5.297574
4.437514	298.150638	5.302579
4.162968	286.357709	5.307584
3.950551	282.043812	5.312589
3.853998	283.346524	5.317594
3.977293	287.076241	5.322598
4.230003	290.738225	5.327603
4.173801	297.020797	5.332608
4.433152	293.613765	5.337613
4.004006	299.056246	5.342618
4.452959	301.374498	5.347622
3.969147	291.481010	5.352627
4.294190	293.568734	5.357632
4.288463	291.437125	5.362637
3.926517	293.790678	5.367642
4.182623	292.374198	5.372646
4.585492	299.679526	5.377651
4.242825	289.820872	5.382656
4.403317	290.915628	5.387661
4.477318	286.129738	5.392666
4.177467	279.535772	5.397670
4.078591	277.127688	5.402675
3.992557	293.377798	5.407680
4.283530	295.059564	5.412685
4.216593	303.533185	5.417690
4.554344	289.201849	5.422694
4.416102	300.407526	5.427699
4.603077	304.231675	5.432704
4.636309	294.228700	5.437709
4.545454	295.059110	5.442714
4.653106	289.375749	5.447718
4.264099	282.656543	5.452723
4.393647	285.018510	5.457728
4.603335	295.897582	5.462733
4.464264	302.120372	5.467738
4.282209	301.345194	5.472742
4.463922	304.341247	5.477747
4.508861	300.914023	5.482752
4.467468	304.353165	5.487757
4.228188	306.640043	5.492762
4.759959	299.055211	5.497766
4.359795	307.581043	5.502771
4.475768	309.461076	5.507776
4.528053	308.908615	5.512781
4.546613	303.830844	5.517786
4.900633	300.446944	5.522790
4.884317	305.141358	5.527795
4.408590	309.920410	5.532800
4.665077	298.104384	5.537805
4.816334	305.888908	5.542810
4.628290	302.311522	5.547814
4.621354	308.383894	5.552819
4.588293	300.729368	5.557824
4.634763	301.095327	5.562829
4.344390	299.963790	5.567834
4.785998	294.696349	5.572838
4.327217	306.069313	5.577843
4.446682	302.250753	5.582848
4.465200	304.326392	5.587853
4.515765	303.356577	5.592858
4.706791	310.859619	5.597862
4.501653	323.904483	5.602867
5.053589	330.828955	5.607872
4.842592	325.388502	5.612877
4.674469	324.380182	5.617882
4.978326	326.857216	5.622886
5.064475	341.688309	5.627891
4.896123	333.428528	5.632896
5.222074	334.130358	5.637901
4.833860	330.321731	5.642906
4.968512	325.690847	5.647910
4.772206	335.636949	5.652915
4.754826	328.109671	5.657920
5.199979	330.751234	5.662925
4.776886	337.578534	5.667930
4.753710	318.507361	5.672934
4.701259	332.711578	5.677939
4.569155	334.639974	5.682944
4.726078	330.021418	5.687949
4.567089	333.238540	5.692954
5.047281	326.205956	5.697958
5.035894	331.326722	5.702963
5.146068	330.667112	5.707968
5.170865	328.967324	5.712973
4.767833	331.017264	5.717978
4.878503	322.084169	5.722982
5.127175	342.606834	5.727987
5.288485	349.994323	5.732992
5.327494	352.857715	5.737997
4.960082	346.644478	5.743002
5.350354	337.591635	5.748006
5.348343	350.092151	5.753011
5.322752	344.635299	5.758016
5.159502	337.950303	5.763021
4.947371	338.420058	5.768026
5.200557	344.559257	5.773030
5.111441	355.406086	5.778035
5.361275	354.113973	5.783040
5.706527	355.201932	5.788045
5.247186	347.769203	5.793050
5.052046	341.244231	5.798054
5.132827	349.675746	5.803059
5.273637	343.439830	5.808064
5.179612	353.607204	5.813069
5.193517	350.127883	5.818074
5.103310	350.945539	5.823078
5.040184	349.012747	5.828083
5.340736	353.173461	5.833088
5.422743	361.936992	5.838093
5.125573	353.833430	5.843098
5.336816	359.890618	5.848102
5.306693	359.854117	5.853107
5.585481	361.060059	5.858112
5.640227	357.299085	5.863117
5.419903	353.587538	5.868122
5.695484	355.211608	5.873126
5.525036	359.923859	5.878131
5.511025	354.439878	5.883136
5.613480	350.370867	5.888141
5.692604	359.331006	5.893146
5.578902	363.439566	5.898150
5.341143	366.751295	5.903155
5.456797	361.987333	5.908160
5.549910	352.180592	5.913165
5.661047	348.739823	5.918170
5.633452	360.785600	5.923174
5.753116	355.714120	5.928179
5.584516	350.089842	5.933184
5.805342	350.691082	5.938189
5.945739	352.564129	5.943194
5.740763	349.217182	5.948198
5.562703	355.873216	5.953203
5.833417	357.804941	5.958208
6.088847	351.320104	5.963213
5.940525	357.835435	5.968218
5.788128	351.294271	5.973222
5.731874	352.967169	5.978227
5.502496	352.797369	5.983232
5.770063	351.597393	5.988237
5.697079	355.671097	5.993242
5.857378	341.731363	5.998246
5.852389	353.976078	6.003251
5.811952	351.005157	6.008256
6.036780	346.603754	6.013261
5.599304	350.490951	6.018266
5.662519	353.353714	6.023270
5.836164	357.493183	6.028275
5.597125	355.224111	6.033280
5.760538	364.190029	6.038285
5.804014	360.475114	6.043290
5.849412	358.487351	6.048294
5.758779	365.512515	6.053299
5.535152	359.409625	6.058304
5.731874	345.027573	6.063309
5.416800	361.592049	6.068314
5.749477	349.058517	6.073318
5.593422	353.047157	6.078323
5.720906	354.827313	6.083328
5.848496	358.322248	6.088333
5.861627	358.320100	6.093338
5.883139	348.195542	6.098342
5.636709	353.425908	6.103347
5.493586	363.895217	6.108352
5.536964	351.808818	6.113357
5.151837	353.821153	6.118362
5.441202	354.652105	6.123366
5.633109	353.539916	6.128371
5.348039	360.649327	6.133376
5.464229	355.885283	6.138381
5.713545	359.269396	6.143386
5.622157	349.811111	6.148390
5.785401	359.757841	6.153395
5.786674	351.338594	6.158400
5.641912	349.450231	6.163405
5.407684	355.551903	6.168410
5.634116	354.794981	6.173414
5.548887	361.936359	6.178419
5.902033	369.088150	6.183424
5.881014	368.195988	6.188429
5.576303	365.317092	6.193434
6.088054	357.507576	6.198438
5.946837	354.096853	6.203443
5.868959	356.605228	6.208448
6.034688	360.723791	6.213453
5.462803	368.023680	6.218458
5.552255	353.971647	6.223462
5.751344	353.491099	6.228467
5.184711	357.787685	6.233472
5.629115	346.505346	6.238477
5.321422	364.157026	6.243482
5.791040	370.138933	6.248486
6.098307	373.295664	6.253491
5.461970	360.410900	6.258496
5.646899	356.547270	6.263501
5.708447	372.812295	6.268506
6.163487	368.751313	6.273510
5.603756	364.165938	6.278515
5.541625	358.955258	6.283520
5.719115	355.617989	6.288525
5.344775	363.045116	6.293530
5.867563	361.007866	6.298534
5.830093	370.097012	6.303539
5.728474	370.176120	6.308544
5.946189	357.078449	6.313549
5.481562	359.359511	6.318554
6.120239	354.320610	6.323558
6.122041	351.485444	6.328563
5.576526	345.458304	6.333568
5.945373	348.197248	6.338573
5.737655	346.264964	6.343578
5.761101	341.910933	6.348582
5.586806	356.244994	6.353587
5.767188	352.907272	6.358592
5.860794	349.399646	6.363597
5.730922	345.790990	6.368602
5.480229	344.124873	6.373606
5.545321	347.945982	6.378611
5.382107	354.042856	6.383616
5.561833	348.588634	6.388621
5.751164	346.204989	6.393626
5.785721	342.121307	6.398630
5.734828	338.427510	6.403635
5.609020	347.897490	6.408640
6.006614	343.696814	6.413645
5.965513	354.906288	6.418650
5.811541	349.371470	6.423654
5.867892	350.754636	6.428659
5.679493	347.028596	6.433664
6.051202	348.327549	6.438669
5.920409	358.557636	6.443674
6.222979	351.616148	6.448678
5.920284	349.417163	6.453683
5.996376	345.592735	6.458688
6.067146	343.414332	6.463693
5.681173	343.901833	6.468698
5.750458	332.912400	6.473702
5.033428	336.609271	6.478707
5.508150	334.949722	6.483712
5.549664	339.660396	6.488717
5.597480	342.259808	6.493722
5.707010	352.101052	6.498726
5.888146	352.398455	6.503731
5.329480	343.541747	6.508736
5.586756	347.930709	6.513741
5.643516	352.351088	6.518746
5.770474	350.255632	6.523750
5.853276	349.932512	6.528755
5.672641	352.741731	6.533760
6.191668	342.804986	6.538765
5.844229	350.623372	6.543770
5.768581	349.312653	6.548774
5.780905	346.425217	6.553779
5.739694	346.074071	6.558784
5.849031	347.303398	6.563789
5.540828	352.053049	6.568794
5.514389	344.435433	6.573798
5.726310	345.281683	6.578803
5.574924	352.354326	6.583808
5.823342	343.399638	6.588813
5.818393	351.066284	6.593818
6.200427	354.208133	6.598822
6.021855	359.101995	6.603827
5.829722	347.634644	6.608832
5.681356	332.174019	6.613837
5.523289	335.688396	6.618842
5.894236	330.799020	6.623846
5.723379	329.689885	6.628851
5.654326	337.252671	6.633856
5.669849	332.893556	6.638861
5.573319	342.074202	6.643866
5.991229	337.297691	6.648870
5.769945	332.507433	6.653875
5.527309	331.434854	6.658880
5.711278	335.275301	6.663885
5.672766	345.161883	6.668890
5.719174	351.222748	6.673894
5.729536	353.116169	6.678899
5.672984	352.384602	6.683904
5.744258	341.701744	6.688909
5.581816	354.607059	6.693914
5.699061	352.873801	6.698918
5.806560	353.711102	6.703923
5.933124	356.475353	6.708928
5.919192	343.334891	6.713933
5.630099	343.493993	6.718938
5.598267	327.597488	6.723942
5.775342	330.018455	6.728947
5.246261	337.393885	6.733952
5.646915	350.207807	6.738957
5.599997	351.202183	6.743962
5.945651	348.917434	6.748966
5.771383	352.915255	6.753971
5.635309	352.284735	6.758976
5.903941	353.454302	6.763981
5.297785	357.108495	6.768986
5.283540	347.593831	6.773990
5.474805	357.621593	6.778995
5.576850	353.941797	6.784000
5.672761	353.319223	6.789005
5.567098	352.275804	6.794010
5.662466	358.094876	6.799014
5.450075	357.368743	6.804019
5.573385	354.644256	6.809024
5.805034	358.018481	6.814029
5.909106	355.641865	6.819034
5.558755	350.435216	6.824038
5.665159	350.889864	6.829043
5.617281	355.089352	6.834048
5.726509	349.253861	6.839053
5.444574	356.948088	6.844058
5.342728	351.269058	6.849062
5.725654	354.126023	6.854067
5.819555	367.162030	6.859072
6.056932	360.581939	6.864077
5.752324	357.712521	6.869082
5.886988	343.204148	6.874086
5.569318	352.321368	6.879091
5.474296	356.556717	6.884096
5.801799	347.089751	6.889101
5.765542	354.609440	6.894106
5.763502	344.675239	6.899110
5.591412	354.171457	6.904115
5.660492	356.444830	6.909120
5.836535	343.363190	6.914125
5.739830	345.823891	6.919130
5.894524	354.234336	6.924134
5.536137	357.172649	6.929139
5.513334	359.419288	6.934144
5.835357	349.130583	6.939149
5.479579	357.776038	6.944154
5.672037	355.777889	6.949158
5.780158	358.582996	6.954163
5.497772	356.254276	6.959168
5.880702	359.959148	6.964173
5.735986	360.332916	6.969178
5.435933	352.210823	6.974182
5.670819	363.035367	6.979187
6.092785	366.000115	6.984192
6.171888	357.223812	6.989197
6.036338	356.615357	6.994202
6.243687	355.469110	6.999206
5.795962	341.937860	7.004211
5.914341	349.718063	7.009216
5.868649	342.476796	7.014221
5.944213	354.914540	7.019226
5.883903	338.566895	7.024230
6.013546	344.383757	7.029235
5.618161	347.201311	7.034240
6.123665	337.320474	7.039245
5.672255	333.088303	7.044250
5.320015	328.445118	7.049254
5.597721	335.029735	7.054259
5.643533	345.494741	7.059264
5.765808	339.056082	7.064269
5.461145	352.363338	7.069274
5.854469	345.777802	7.074278
5.756620	347.311681	7.079283
5.529060	355.288460	7.084288
5.751395	343.446117	7.089293
5.640003	352.575311	7.094298
5.498292	348.225009	7.099302
5.628077	351.615194	7.104307
5.546366	351.077398	7.109312
5.566775	346.799774	7.114317
5.619859	348.291022	7.119322
5.694610	348.219106	7.124326
5.904561	348.720808	7.129331
5.418661	352.419435	7.134336
5.990552	349.213366	7.139341
5.726123	349.099678	7.144346
5.898529	352.932449	7.149350
5.490130	351.360645	7.154355
5.312441	347.848068	7.159360
5.811046	348.766462	7.164365
5.660037	354.443798	7.169370
5.797991	357.560613	7.174374
5.735673	349.727148	7.179379
5.605357	352.360800	7.184384
5.818655	345.955334	7.189389
5.694915	361.572321	7.194394
5.624689	339.993249	7.199398
5.871527	338.053022	7.204403
5.563126	346.839749	7.209408
5.733734	339.700638	7.214413
5.791395	344.462568	7.219418
5.681489	344.191789	7.224422
5.957434	341.231412	7.229427
5.757203	349.387409	7.234432
5.879614	349.317517	7.239437
5.637385	350.215941	7.244442
6.006525	353.654047	7.249446
5.864970	353.062352	7.254451
5.750441	351.969700	7.259456
6.251822	342.839334	7.264461
6.141923	343.625272	7.269466
5.639254	331.592803	7.274470
5.820961	323.034565	7.279475
5.652302	321.168931	7.284480
6.257889	313.980661	7.289485
5.669850	323.168702	7.294490
5.711689	321.444099	7.299494
5.914870	312.993234	7.304499
5.576480	326.277281	7.309504
5.705541	320.834171	7.314509
5.748209	321.093156	7.319514
5.929518	316.758691	7.324518
5.843056	322.081046	7.329523
5.904486	331.515354	7.334528
5.986234	323.017071	7.339533
5.581428	333.324877	7.344538
5.701192	317.556493	7.349542
5.469016	318.269838	7.354547
5.299480	324.158879	7.359552
5.320459	324.095389	7.364557
5.422385	329.223711	7.369562
5.615644	331.192879	7.374566
5.668013	335.183661	7.379571
5.778414	339.855067	7.384576
5.955485	331.572804	7.389581
5.713966	323.982568	7.394586
5.457171	327.022019	7.399590
5.620791	322.506822	7.404595
5.766562	337.837947	7.409600
6.091505	324.280563	7.414605
5.607468	332.177292	7.419610
5.733342	328.180548	7.424614
5.803248	324.303308	7.429619
5.394227	329.331347	7.434624
5.601966	334.471566	7.439629
5.340199	345.956060	7.444634
5.713498	345.359629	7.449638
6.030018	351.862239	7.454643
5.580172	356.067758	7.459648
5.548532	351.140211	7.464653
5.981064	350.110547	7.469658
6.049973	345.869617	7.474662
5.904380	339.428634	7.479667
5.701871	329.434101	7.484672
5.635629	331.589464	7.489677
5.362751	338.092665	7.494682
5.880023	339.590278	7.499686
5.674060	340.144489	7.504691
5.529253	337.487324	7.509696
6.146207	346.122738	7.514701
5.680507	337.052146	7.519706
5.423862	329.938851	7.524710
5.541697	333.666270	7.529715
5.751863	341.235931	7.534720
6.080405	338.472962	7.539725
5.657321	338.852379	7.544730
5.616825	329.787938	7.549734
6.059210	319.546831	7.554739
5.298071	330.486283	7.559744
5.801325	341.170687	7.564749
5.754332	347.027880	7.569754
5.655923	340.256793	7.574758
5.532810	340.054524	7.579763
5.541017	354.182814	7.584768
5.664765	346.940307	7.589773
5.395687	355.695567	7.594778
5.913821	343.474675	7.599782
5.838063	350.310837	7.604787
5.723620	354.615668	7.609792
6.057329	345.375527	7.614797
5.675186	348.700383	7.619802
5.759911	352.028023	7.624806
6.032980	345.610029	7.629811
5.575195	339.132536	7.634816
5.859317	323.673760	7.639821
5.639423	328.741771	7.644826
5.371933	324.468131	7.649830
5.596287	326.581126	7.654835
5.551205	341.255606	7.659840
5.773849	339.505836	7.664845
5.850904	352.819726	7.669850
5.810169	342.518257	7.674854
5.962482	346.907844	7.679859
6.086800	332.315678	7.684864
5.899255	318.525377	7.689869
5.656187	325.599719	7.694874
5.434197	333.360477	7.699878
5.674310	317.022730	7.704883
5.559843	320.947898	7.709888
5.622870	321.403015	7.714893
5.532581	337.163439	7.719898
5.791934	340.612416	7.724902
5.774161	342.652616	7.729907
5.853731	347.936310	7.734912
6.281913	341.683843	7.739917
5.677037	323.494763	7.744922
5.773162	326.301745	7.749926
5.745134	324.217920	7.754931
5.248221	319.309495	7.759936
5.639064	319.400031	7.764941
5.493942	323.371133	7.769946
5.625553	336.176577	7.774950
5.849503	339.311554	7.779955
6.009522	353.352781	7.784960
5.736320	335.652737	7.789965
5.589523	335.049208	7.794970
5.578188	328.283466	7.799974
5.826899	329.452989	7.804979
5.394099	331.055165	7.809984
5.564966	339.251093	7.814989
5.723472	343.465699	7.819994
5.649340	338.693513	7.824998
5.772747	344.558810	7.830003
5.607132	346.030538	7.835008
6.292498	341.870197	7.840013
5.276161	345.458938	7.845018
5.400946	348.995441	7.850022
5.639633	345.578982	7.855027
5.461652	346.935586	7.860032
5.951194	348.200258	7.865037
5.714586	353.492362	7.870042
5.580268	352.564167	7.875046
5.611365	341.476305	7.880051
5.550352	352.024493	7.885056
5.660372	344.391824	7.890061
5.519638	347.941454	7.895066
5.340052	352.294458	7.900070
5.660265	348.194492	7.905075
5.538905	348.339969	7.910080
5.963389	349.697094	7.915085
5.628807	353.008172	7.920090
5.684177	343.071305	7.925094
5.487674	344.626968	7.930099
5.563701	347.358006	7.935104
5.610744	343.579259	7.940109
5.719878	352.284750	7.945114
5.713493	354.898984	7.950118
5.738838	349.317088	7.955123
5.757468	346.884256	7.960128
5.802536	348.989525	7.965146
5.893833	353.257497	7.970163
5.684687	349.042521	7.975181
5.819597	347.702185	7.980198
5.807876	354.384675	7.985216
5.783393	347.915955	7.990234
6.251192	344.652097	7.995251
6.004255	353.627807	8.000269
5.697126	344.107574	8.005286
5.927762	349.808517	8.010304
5.995789	344.208918	8.015322
6.005357	347.839606	8.020339
5.875121	338.361087	8.025357
5.678547	351.734344	8.030374
5.511525	353.224695	8.035392
6.070979	348.261299	8.040410
6.068568	348.716015	8.045427
5.963171	346.820048	8.050445
5.722473	342.464852	8.055462
5.631203	350.346370	8.060480
5.688941	346.095891	8.065498
5.800823	348.079022	8.070515
5.583708	351.896705	8.075533
5.775982	346.078824	8.080550
5.525909	354.064119	8.085568
5.658150	347.163751	8.090586
5.630280	352.813681	8.095603
5.211784	351.938744	8.100621
5.324754	359.864003	8.105638
5.589208	364.805425	8.110656
5.891469	369.983920	8.115674
5.739299	380.655220	8.120691
5.966956	371.376225	8.125709
6.124884	376.776148	8.130726
5.654694	375.660003	8.135744
5.833201	373.659591	8.140762
5.987084	375.396306	8.145779
5.920802	382.658548	8.150797
6.161860	372.859907	8.155814
5.919284	391.703031	8.160832
5.983020	379.940880	8.165850
6.174261	375.549558	8.170867
5.953934	379.380373	8.175885
6.142534	368.090965	8.180902
5.616798	368.886449	8.185920
5.846685	368.392753	8.190938
5.808546	373.425769	8.195955
5.631981	363.875601	8.200973
5.833225	376.653223	8.205990
5.990626	375.202065	8.211008
6.244694	370.362249	8.216026
6.287142	366.350844	8.221043
5.945492	375.874730	8.226061
6.243945	374.994755	8.231078
6.207297	367.432884	8.236096
5.868954	359.659514	8.241114
5.769268	367.706457	8.246131
5.570758	374.484492	8.251149
5.998275	368.667615	8.256166
5.943469	371.352199	8.261184
5.802102	377.938247	8.266202
5.803565	373.422028	8.271219
5.852819	382.505978	8.276237
5.892670	373.859159	8.281254
5.651434	377.844726	8.286272
5.837889	376.613075	8.291290
6.227217	367.479162	8.296307
5.899412	374.952788	8.301325
6.000884	367.631205	8.306342
5.918209	374.346910	8.311360
5.993466	376.080165	8.316378
6.142946	375.087834	8.321395
5.985749	388.335030	8.326413
5.925418	392.241764	8.331430
5.906728	396.195623	8.336448
5.915673	394.234398	8.341466
6.342025	386.262309	8.346483
6.166196	395.750757	8.351501
6.408925	400.342148	8.356518
6.471861	394.241563	8.361536
6.397751	379.982707	8.366554
6.259172	375.008753	8.371571
5.971620	381.459918	8.376589
6.283362	372.805213	8.381606
5.906024	377.427479	8.386624
5.695225	367.115821	8.391642
6.009906	372.027286	8.396659
6.594803	395.023137	8.401677
6.775096	386.035574	8.406694
6.170565	376.262122	8.411712
6.140008	378.737783	8.416730
6.195780	378.205096	8.421747
6.147670	373.908080	8.426765
6.317039	378.006037	8.431782
6.069392	379.641564	8.436800
6.133634	377.337166	8.441818
6.110418	367.267514	8.446835
5.949019	377.381689	8.451853
6.101509	374.855184	8.456870
6.214579	392.197245	8.461888
6.363379	385.726608	8.466906
6.224002	382.990215	8.471923
6.156475	384.837360	8.476941
6.311342	389.521408	8.481958
6.425627	392.681268	8.486976
6.122057	391.640001	8.491994
6.320406	382.861048	8.497011
6.337555	398.252102	8.502029
6.323133	387.474168	8.507046
6.332273	386.191404	8.512064
6.149733	381.110728	8.517082
6.334747	382.763672	8.522099
6.521177	402.309597	8.527117
6.864542	388.528116	8.532134
6.371157	384.868901	8.537152
5.978773	381.124436	8.542170
5.952126	373.002425	8.547187
6.213291	385.590787	8.552205
6.501280	385.769633	8.557223
6.647600	393.020660	8.562240
6.580826	383.317580	8.567258
6.637197	373.039798	8.572275
6.166726	376.758328	8.577293
6.288845	358.694450	8.582311
6.421210	370.779125	8.587328
6.422486	372.833236	8.592346
6.348768	366.122919	8.597363
6.214191	365.323415	8.602381
6.243134	364.390995	8.607399
5.962620	377.919434	8.612416
6.448667	385.164565	8.617434
6.498404	384.096343	8.622451
6.484107	397.851326	8.627469
6.564857	394.155802	8.632487
6.538357	385.311092	8.637504
6.216263	385.421426	8.642522
6.516186	383.954248	8.647539
6.361622	402.190309	8.652557
6.598482	391.600217	8.657575
6.567310	397.869210	8.662592
6.458587	394.291733	8.667610
6.511765	375.228794	8.672627
6.396548	386.348738	8.677645
6.562437	385.656789	8.682663
6.667723	390.149792	8.687680
6.289986	373.347629	8.692698
6.663460	384.384692	8.697715
6.328420	381.754694	8.702733
6.670599	377.181935	8.707751
6.548443	379.103909	8.712768
6.221937	382.695744	8.717786
6.659484	383.958831	8.722803
6.625305	391.967120	8.727821
6.654859	387.891459	8.732839
6.688128	381.296915	8.737856
5.964836	375.726617	8.742874
6.650633	382.811064	8.747891
6.688894	394.866319	8.752909
6.838933	386.773423	8.757927
6.872691	392.448423	8.762944
6.428740	375.173801	8.767962
6.679955	368.349457	8.772979
6.374609	374.705579	8.777997
6.593054	382.996170	8.783015
6.441489	385.620178	8.788032
6.467914	392.927858	8.793050
6.628180	386.174562	8.798067
6.366471	400.763564	8.803085
6.578711	386.210532	8.808103
6.801259	400.398617	8.813120
6.668335	403.130158	8.818138
7.264333	396.024568	8.823155
6.813592	396.388585	8.828173
6.748480	381.011177	8.833191
6.774019	368.298821	8.838208
6.120752	371.601028	8.843226
6.643675	377.101552	8.848243
6.475121	391.480294	8.853261
6.551195	394.144375	8.858279
6.583190	388.604055	8.863296
6.739903	398.144542	8.868314
6.924795	394.700941	8.873331
6.790690	396.590076	8.878349
6.735848	399.347252	8.883367
7.065977	395.372816	8.888384
6.578642	401.618608	8.893402
6.621496	392.949218	8.898419
6.820719	400.371838	8.903437
6.541650	397.972906	8.908455
6.928097	390.758141	8.913472
6.521237	395.662744	8.918490
6.571258	394.026440	8.923507
6.623177	392.866359	8.928525
6.772289	393.249998	8.933543
6.924396	390.849782	8.938560
6.827926	397.592903	8.943578
7.057425	396.812093	8.948595
6.674945	392.696848	8.953613
7.084333	402.204059	8.958631
6.653740	393.681432	8.963648
6.621489	392.493514	8.968666
6.727673	387.926169	8.973683
6.298412	404.942966	8.978701
6.363259	407.198557	8.983719
6.491381	401.703132	8.988736
6.482218	404.550980	8.993754
7.157023	407.982779	8.998771
6.988708	402.442281	9.003789
6.537429	403.667908	9.008807
6.934451	402.652569	9.013824
6.974121	414.237407	9.018842
7.230597	415.270094	9.023859
6.898736	405.210909	9.028877
6.538308	395.882034	9.033895
6.600755	400.372284	9.038912
6.744603	420.900034	9.043930
6.695719	418.364049	9.048947
7.199498	424.978420	9.053965
7.198778	420.128019	9.058983
7.212792	417.859887	9.064000
7.036378	419.541062	9.069018
6.905146	400.727893	9.074035
7.048223	405.704123	9.079053
6.626604	394.188420	9.084071
7.149612	408.922720	9.089088
6.833016	412.137471	9.094106
7.122268	418.551924	9.099123
7.104717	417.450063	9.104141
6.822187	418.554578	9.109159
7.131534	411.487582	9.114176
6.789102	412.102871	9.119194
7.096670	423.551067	9.124211
7.210722	420.768649	9.129229
7.359759	426.646503	9.134247
7.079636	415.029722	9.139264
6.781588	405.290284	9.144282
6.924085	408.221667	9.149299
7.029420	420.096019	9.154317
6.814666	416.838105	9.159335
7.258749	420.627944	9.164352
7.424575	432.669550	9.169370
7.617029	414.957508	9.174387
6.982234	406.094488	9.179405
7.220239	395.352738	9.184423
7.162222	396.766054	9.189440
7.082620	404.601586	9.194458
7.117473	397.404037	9.199475
6.901532	398.229877	9.204493
6.940521	407.760412	9.209511
7.170775	391.153303	9.214528
7.124465	401.416714	9.219546
7.212928	397.893548	9.224563
7.199934	403.487516	9.229581
7.062019	406.800501	9.234599
6.918919	400.826869	9.239616
7.135808	418.427241	9.244634
7.508230	416.402753	9.249651
7.632062	402.393729	9.254669
7.150177	402.652174	9.259687
7.258569	400.293520	9.264704
7.204432	403.350384	9.269722
7.000060	397.061309	9.274739
7.096298	400.422812	9.279757
7.179890	399.589123	9.284775
7.425108	390.872249	9.289792
7.202424	399.200407	9.294810
7.208725	390.991176	9.299827
7.097100	395.354066	9.304845
7.188167	396.021352	9.309863
7.656908	397.718205	9.314880
6.955154	399.273407	9.319898
7.412158	399.444706	9.324915
7.563671	406.780131	9.329933
7.235288	401.943203	9.334951
7.410656	400.454514	9.339968
7.199866	393.756196	9.344986
7.092997	402.921422	9.350003
7.607746	393.793092	9.355021
7.313329	399.655211	9.360039
7.653621	401.422681	9.365056
7.514859	405.146049	9.370074
7.466912	399.668743	9.375091
7.001742	401.966352	9.380109
6.911102	393.844892	9.385127
7.431638	401.131962	9.390144
7.567150	400.514199	9.395162
7.293318	397.467514	9.400179
7.117457	400.180536	9.405197
7.460201	402.386274	9.410215
7.178945	396.667817	9.415232
7.483913	414.172335	9.420250
7.769271	406.370649	9.425267
7.745867	396.247362	9.430285
7.491677	401.137514	9.435303
7.185204	396.710561	9.440320
7.041400	398.553880	9.445338
7.051571	409.524806	9.450355
7.509167	423.041772	9.455373
7.578255	426.644216	9.460391
7.738846	429.711622	9.465408
7.503351	411.526998	9.470426
7.261378	410.144722	9.475443
7.395082	416.987485	9.480461
7.047589	429.219967	9.485479
7.435889	421.932316	9.490496
7.445171	428.273875	9.495514
7.837742	425.053346	9.500531
8.008518	427.194514	9.505549
7.390480	425.625009	9.510567
7.719270	419.842519	9.515584
7.737610	418.750813	9.520602
7.496985	404.843072	9.525619
7.209996	404.607082	9.530637
7.336874	417.838194	9.535655
7.458168	417.453029	9.540672
7.726767	411.118245	9.545690
7.687977	420.657818	9.550707
7.428946	424.974384	9.555725
7.083573	424.845371	9.560743
7.319080	415.467295	9.565760
7.316042	430.208295	9.570778
7.439449	427.093054	9.575795
7.511851	418.939725	9.580813
7.481170	429.140744	9.585831
7.679469	424.098215	9.590848
7.924216	424.444781	9.595866
7.345658	427.672177	9.600883
7.582642	423.459867	9.605901
7.414308	422.441590	9.610919
7.729305	416.042731	9.615936
7.463946	419.767003	9.620954
7.649078	431.013483	9.625971
7.895883	436.219620	9.630989
7.668685	439.259425	9.636007
7.807156	426.740770	9.641024
7.859550	431.254694	9.646042
7.812939	425.455282	9.651059
7.867237	426.374481	9.656077
7.399947	425.431446	9.661095
7.607587	419.440723	9.666112
7.615384	433.236452	9.671130
7.566370	450.190558	9.676147
8.209557	452.342918	9.681165
8.043172	438.877950	9.686183
7.656170	426.924460	9.691200
7.765764	432.846365	9.696218
7.793069	426.214870	9.701235
7.964071	428.974535	9.706253
7.667874	433.905990	9.711271
7.742588	418.992630	9.716288
7.643266	430.157448	9.721306
7.739590	440.183941	9.726323
8.028361	433.890170	9.731341
7.765285	439.242467	9.736359
7.909120	437.790274	9.741376
7.663472	437.560430	9.746394
7.921396	450.654270	9.751411
8.060998	449.975904	9.756429
8.036960	445.182798	9.761447
7.984116	427.490243	9.766464
7.868068	426.381723	9.771482
7.597229	432.732459	9.776499
7.797152	437.046546	9.781517
7.985082	445.477646	9.786535
8.025940	447.209986	9.791552
7.924822	437.180902	9.796570
7.550419	438.063130	9.801587
7.846107	443.788625	9.806605
7.946999	444.037812	9.811623
8.049802	448.584867	9.816640
7.997742	446.844632	9.821658
8.189624	453.353248	9.826675
8.158134	446.371199	9.831693
8.100154	443.224416	9.836711
7.780545	429.171241	9.841728
8.017228	437.739864	9.846746
8.057559	447.364884	9.851763
8.227258	442.471996	9.856781
7.573503	440.756609	9.861799
7.944028	442.314221	9.866816
8.168633	450.682773	9.871834
7.858424	451.375064	9.876851
7.822087	447.461191	9.881869
8.202742	455.682220	9.886887
8.124578	446.750901	9.891904
8.147407	447.577202	9.896922
8.000885	446.094763	9.901939
8.114415	443.290333	9.906957
7.703818	457.587132	9.911975
7.768200	462.910221	9.916992
8.103716	449.448657	9.922010
7.745150	454.336242	9.927027
7.798702	444.570096	9.932045
8.172987	463.392384	9.937063
7.903409	459.101645	9.942080
8.020795	450.294319	9.947098
7.574291	455.426054	9.952115
8.138940	462.308610	9.957133
7.919249	475.758165	9.962151
8.242241	478.156355	9.967168
8.380764	476.859624	9.972186
8.518145	482.761413	9.977203
8.440097	482.786173	9.982221
8.429612	470.328696	9.987239
7.959878	456.964891	9.992256
8.098445	454.083954	9.997274
7.968427	465.531311	10.002291
8.442268	468.997765	10.007309
8.208785	478.621521	10.012327
8.088850	478.236281	10.017344
8.259625	471.834753	10.022362
8.239565	475.536382	10.027379
8.256489	477.275631	10.032397
7.799344	485.741549	10.037415
8.052809	479.336529	10.042432
8.372135	473.041113	10.047450
8.292155	476.502823	10.052467
8.472769	476.490212	10.057485
8.695526	476.590918	10.062503
8.202382	478.848739	10.067520
8.154746	478.303849	10.072538
7.798713	478.766637	10.077555
8.105753	484.865905	10.082573
8.560305	476.485418	10.087591
8.492115	478.159108	10.092608
8.326516	480.217287	10.097626
8.124551	487.273614	10.102643
8.166398	475.704177	10.107661
8.104172	473.571059	10.112679
7.826381	483.997018	10.117696
8.348442	493.795891	10.122714
8.641354	507.212493	10.127731
8.681929	496.476369	10.132749
8.661690	487.504396	10.137767
8.460781	486.036786	10.142784
8.743397	476.884824	10.147802
8.445971	486.196713	10.152819
8.445414	469.054499	10.157837
8.882816	472.753878	10.162855
8.534125	475.408784	10.167872
8.782770	475.227725	10.172890
8.812093	482.083712	10.177907
8.856362	472.079165	10.182925
8.694402	473.909558	10.187943
8.420248	478.127521	10.192960
8.665811	469.366374	10.197978
8.585282	469.009673	10.202995
8.773996	474.379557	10.208013
8.435913	473.340536	10.213031
8.118747	472.560168	10.218048
9.187248	477.688067	10.223066
8.337045	480.629832	10.228083
8.759420	477.417248	10.233101
8.509749	472.839366	10.238119
8.565247	492.298607	10.243136
8.971533	482.379345	10.248154
8.138390	477.268035	10.253171
8.291409	469.414474	10.258189
8.779281	481.784349	10.263207
8.227474	470.604572	10.268224
8.435458	479.310254	10.273242
8.395327	474.011581	10.278259
8.622055	482.622810	10.283277
8.869920	472.889320	10.288295
8.748443	464.476015	10.293312
8.797576	474.017619	10.298330
8.674204	474.522848	10.303347
8.918697	470.252547	10.308365
8.893030	476.621689	10.313383
8.503029	478.355268	10.318400
8.705787	480.633442	10.323418
8.572695	479.212011	10.328435
8.594236	474.067775	10.333453
8.927673	478.654441	10.338471
8.380353	468.969804	10.343488
8.723916	472.961595	10.348506
8.885713	476.398046	10.353523
8.486820	475.829297	10.358541
8.936718	471.630954	10.363559
8.616099	468.780934	10.368576
8.913455	476.516411	10.373594
8.433928	474.186746	10.378611
8.844632	475.943192	10.383629
8.953594	481.634840	10.388647
8.911070	484.112390	10.393664
8.820137	473.797669	10.398682
9.002134	477.429770	10.403699
8.856298	470.512964	10.408717
8.799454	471.717820	10.413735
8.850416	469.055732	10.418752
8.883127	480.244075	10.423770
8.875055	479.200685	10.428787
8.570568	476.991916	10.433805
8.889370	492.260049	10.438823
8.944662	510.636909	10.443840
9.153557	492.095399	10.448858
9.292314	497.170161	10.453875
9.000207	487.934673	10.458893
9.019236	481.190846	10.463911
8.781874	483.187686	10.468928
8.738402	479.016150	10.473946
8.684095	491.385773	10.478963
9.150756	493.830882	10.483981
8.991367	505.046182	10.488999
8.548340	502.792845	10.494016
9.232658	498.753425	10.499034
9.192897	506.816288	10.504051
9.218156	511.116734	10.509069
9.334814	499.279941	10.514087
9.180330	490.215392	10.519104
8.845790	483.798359	10.524122
9.046388	492.107577	10.529139
9.091997	492.030912	10.534157
8.984804	493.082714	10.539175
8.905224	501.085541	10.544192
9.025338	497.718341	10.549210
9.081504	503.023795	10.554227
8.839897	503.254062	10.559245
9.220373	507.565123	10.564263
9.028868	507.159538	10.569280
9.445118	500.817368	10.574298
9.349198	501.330920	10.579315
8.918656	507.009276	10.584333
9.296562	492.102000	10.589351
8.922705	500.431799	10.594368
9.175500	497.078525	10.599386
8.928518	506.136369	10.604403
9.030189	506.966099	10.609421
9.117650	499.252185	10.614439
9.254194	506.186054	10.619456
8.976268	498.289549	10.624474
9.245286	497.960131	10.629491
9.064015	500.591966	10.634509
9.381465	499.548064	10.639527
9.288006	504.968479	10.644544
9.307127	503.381186	10.649562
9.359442	495.663312	10.654579
9.166625	504.292950	10.659597
9.272271	500.804941	10.664615
8.790070	503.395563	10.669632
8.962332	496.798134	10.674650
9.268115	510.540923	10.679667
9.134196	517.397253	10.684685
9.337070	522.651324	10.689703
9.437794	532.424717	10.694720
9.630254	519.834422	10.699738
9.499889	516.162483	10.704755
8.813852	509.131486	10.709773
9.125731	512.392951	10.714791
9.429526	523.702949	10.719808
9.683277	519.080893	10.724826
9.530706	520.291283	10.729843
9.689488	534.031876	10.734861
9.642070	517.026345	10.739879
9.303723	507.110130	10.744896
9.364886	501.565204	10.749914
9.294436	504.769808	10.754931
9.195633	514.252562	10.759949
9.631556	513.221655	10.764967
9.380486	525.114048	10.769984
9.341862	527.269103	10.775002
9.343865	521.673481	10.780019
9.429606	526.586145	10.785037
9.385649	519.110562	10.790055
9.059686	527.802097	10.795072
9.190916	525.067465	10.800090
9.293711	525.571973	10.805107
9.228786	530.116927	10.810125
9.752510	528.693567	10.815143
9.356725	528.528270	10.820160
9.218536	523.197609	10.825178
9.516773	533.018950	10.830195
9.605086	546.890514	10.835213
9.770482	545.479115	10.840231
9.404845	540.357653	10.845248
9.700886	543.675255	10.850266
9.595103	552.587924	10.855283
9.563471	549.093012	10.860301
9.875073	541.586957	10.865319
9.636124	546.970220	10.870336
9.557070	547.724127	10.875354
9.493742	538.392807	10.880371
9.860462	546.713891	10.885389
10.032206	545.213135	10.890407
9.364772	536.228932	10.895424
9.777362	533.361852	10.900442
9.795611	534.801099	10.905459
9.815720	547.051805	10.910477
9.619802	538.593324	10.915495
9.636941	546.953402	10.920512
9.403191	542.792728	10.925530
9.532078	551.583422	10.930547
9.719491	539.685024	10.935565
10.055506	538.477265	10.940583
9.806902	540.734648	10.945600
9.616380	540.287883	10.950618
9.720161	546.084505	10.955635
9.165656	549.696316	10.960653
9.568025	539.067583	10.965671
9.934799	540.657350	10.970688
10.087137	534.381764	10.975706
9.759605	543.004125	10.980723
10.086089	542.271229	10.985741
10.118212	539.466916	10.990759
9.665489	537.795760	10.995776
9.804309	542.529699	11.000794
10.110028	546.148741	11.005811
9.859728	540.901912	11.010829
10.019390	540.062610	11.015847
9.930833	539.950162	11.020864
10.174968	537.254642	11.025882
9.929978	538.053482	11.030899
9.913196	548.659489	11.035917
9.794991	541.179750	11.040935
9.936750	545.591339	11.045952
9.794556	552.329059	11.050970
10.009035	543.563279	11.055987
9.862111	552.068985	11.061005
10.084351	547.010047	11.066023
9.996604	544.423329	11.071040
9.827929	544.724220	11.076058
9.923707	536.399918	11.081075
9.993398	555.039654	11.086093
9.802028	546.671975	11.091111
9.953248	543.486084	11.096128
9.694819	541.248000	11.101146
9.982455	555.820485	11.106163
9.979583	570.444811	11.111181
10.152795	571.137103	11.116199
10.233284	581.639526	11.121216
10.227368	569.020319	11.126234
10.229064	574.078708	11.131251
10.280341	580.830307	11.136269
10.413558	569.634656	11.141287
9.997637	562.091102	11.146304
10.124240	570.535026	11.151322
10.604904	563.144484	11.156339
10.542331	561.276497	11.161357
10.244906	554.339228	11.166375
9.908953	550.317642	11.171392
9.699329	552.603633	11.176410
10.079708	559.461450	11.181427
9.793604	571.977899	11.186445
10.219433	570.197491	11.191463
10.584086	569.408120	11.196480
10.575793	575.645188	11.201498
10.690609	567.280019	11.206515
10.536630	565.322212	11.211533
10.306115	551.911387	11.216551
10.465897	546.773873	11.221568
10.272470	552.774853	11.226586
10.193192	538.807013	11.231603
10.072155	554.510186	11.236621
10.321713	556.140411	11.241639
10.637438	569.234749	11.246656
10.041531	560.561217	11.251674
10.727551	556.335326	11.256691
10.224415	553.141505	11.261709
10.514987	551.372823	11.266727
10.491013	550.082612	11.271744
10.335073	543.927907	11.276762
10.394022	540.674424	11.281779
10.417214	546.332194	11.286797
10.150797	542.549022	11.291815
10.798127	559.081706	11.296832
10.741989	558.872660	11.301850
10.577005	539.824792	11.306867
10.122108	548.053702	11.311885
10.094507	541.837865	11.316903
10.613582	553.562274	11.321920
10.362516	568.222329	11.326938
10.555212	564.774317	11.331955
10.408278	564.112439	11.336973
10.399500	569.822563	11.341991
10.644110	565.751036	11.347008
10.499480	567.957417	11.352026
10.992350	572.907291	11.357043
10.721634	571.952383	11.362061
10.535371	570.889569	11.367079
10.658817	572.186105	11.372096
10.531023	565.294838	11.377114
10.797433	561.425023	11.382131
11.025688	568.697997	11.387149
10.323409	560.378802	11.392167
10.429176	561.349904	11.397184
10.683712	565.844814	11.402202
11.107542	565.718357	11.407219
11.077867	564.930810	11.412237
10.360101	551.691002	11.417255
10.607530	534.074371	11.422272
10.264497	550.620205	11.427290
11.056690	548.788708	11.432307
10.905760	564.663831	11.437325
10.648985	546.296211	11.442343
11.034599	551.234482	11.447360
10.065887	553.790885	11.452378
10.605941	552.828867	11.457395
10.570750	564.144666	11.462413
10.329319	562.737046	11.467431
10.688684	565.258937	11.472448
10.527362	580.981068	11.477466
10.852600	559.666245	11.482483
10.740879	564.429978	11.487501
10.749581	565.520430	11.492519
10.996463	563.742813	11.497536
10.866066	571.242394	11.502554
10.812911	575.324769	11.507571
10.737063	572.657288	11.512589
10.418873	567.080261	11.517607
10.760324	563.552138	11.522624
10.518994	577.112457	11.527642
10.765777	584.505610	11.532659
11.145158	594.005003	11.537677
10.856825	590.891129	11.542695
11.189194	585.871730	11.547712
11.077031	594.936899	11.552730
11.135594	587.969087	11.557747
10.931607	581.970220	11.562765
10.870467	589.843966	11.567783
11.374183	595.966105	11.572800
11.072233	580.341610	11.577818
11.191990	565.941778	11.582835
10.744343	572.061490	11.587853
10.619742	569.253326	11.592871
11.290661	587.969309	11.597888
11.061571	594.569181	11.602906
11.296157	588.539466	11.607923
10.932558	590.234204	11.612941
11.221422	596.797106	11.617959
11.234522	589.306242	11.622976
10.920609	587.139961	11.627994
11.229275	588.072963	11.633011
11.270286	596.552400	11.638029
10.672852	588.579683	11.643047
10.896415	588.995843	11.648064
10.783432	597.565681	11.653082
10.911236	590.359801	11.658099
10.819956	601.248911	11.663117
11.221816	598.055299	11.668135
11.420335	596.212672	11.673152
11.470535	592.723865	11.678170
11.085853	599.190327	11.683187
11.284141	596.527227	11.688205
10.768778	598.125825	11.693223
11.379662	588.625728	11.698240
11.260304	599.475054	11.703258
11.341771	593.279979	11.708275
11.317741	587.401238	11.713293
11.272069	593.609454	11.718311
11.441897	587.397382	11.723328
11.127642	602.793199	11.728346
11.224683	594.509698	11.733363
11.339795	604.142020	11.738381
11.322302	601.427522	11.743399
11.626520	584.123835	11.748416
11.353100	594.555485	11.753434
11.162107	598.892990	11.758451
11.344997	601.171137	11.763469
11.201367	598.599479	11.768487
11.315832	593.715204	11.773504
11.275705	612.552087	11.778522
11.605894	616.593343	11.783539
11.840900	619.554449	11.788557
11.500284	616.518190	11.793575
11.357391	597.728731	11.798592
11.252885	596.608924	11.803610
11.491431	614.496431	11.808627
11.377753	605.438053	11.813645
11.554182	614.016202	11.818663
11.982490	618.184097	11.823680
11.466990	612.360259	11.828698
11.603549	597.260336	11.833715
11.593878	602.405721	11.838733
11.134139	600.656762	11.843751
11.560363	611.341719	11.848768
11.299762	619.855800	11.853786
11.843643	619.366551	11.858803
11.862792	617.725595	11.863821
11.844766	633.598891	11.868839
11.654442	610.528104	11.873856
11.726592	620.403852	11.878874
11.793142	603.872687	11.883891
11.699634	595.499120	11.888909
11.308255	592.710660	11.893927
11.441172	603.911782	11.898944
11.525252	615.354092	11.903962
11.647470	620.390455	11.908979
11.656545	614.967266	11.913997
11.392929	620.534296	11.919015
11.598818	614.635301	11.924032
11.544134	615.577896	11.929050
11.598873	619.678090	11.934067
11.719804	622.373046	11.939085
11.436733	623.263063	11.944103
11.783483	614.908869	11.949120
11.852165	625.952812	11.954138
11.914000	616.074821	11.959155
11.831768	615.917201	11.964173
11.951331	618.571345	11.969191
11.863717	612.513209	11.974208
12.199354	612.283805	11.979226
12.078942	617.762126	11.984243
12.201450	610.894740	11.989261
11.732264	619.488839	11.994279
12.308850	609.148349	11.999296
12.236365	610.223121	12.004314
11.958911	613.125662	12.009331
11.831527	611.394057	12.014349
11.725031	615.961324	12.019367
12.250725	606.338866	12.024384
12.050516	608.806425	12.029402
11.860225	622.847932	12.034419
12.055324	616.095402	12.039437
11.587076	619.397067	12.044455
11.608231	610.323873	12.049472
11.557960	618.678767	12.054490
11.647653	614.836629	12.059507
12.320388	623.090868	12.064525
12.147629	640.743042	12.069543
12.335246	631.217722	12.074560
12.096149	627.275617	12.079578
12.035063	619.228318	12.084595
12.059023	617.580297	12.089613
12.184422	619.245759	12.094631
12.204669	616.478009	12.099648
12.108801	615.814440	12.104666
12.066102	621.204846	12.109683
12.242142	630.988583	12.114701
12.436207	635.919019	12.119719
12.260751	626.059267	12.124736
12.024162	615.606339	12.129754
12.146671	625.190176	12.134771
12.664043	627.084560	12.139789
12.038281	619.135202	12.144807
12.059469	614.483287	12.149824
12.226608	620.702351	12.154842
12.038675	636.652763	12.159859
12.573519	628.174419	12.164877
12.527793	636.415000	12.169895
12.273681	631.519036	12.174912
12.178719	628.829294	12.179930
12.417504	628.933802	12.184947
12.510527	626.123089	12.189965
12.523384	625.742287	12.194983
12.379304	626.847212	12.200000
12.268714	620.798985	12.205018
12.175629	628.460002	12.210035
12.456699	619.207224	12.215053
12.459157	645.179064	12.220071
12.388190	633.387358	12.225088
12.561281	630.908083	12.230106
12.182853	634.905734	12.235123
12.331138	638.022442	12.240141
12.592017	642.655233	12.245159
12.431443	638.287411	12.250176
12.527052	642.911382	12.255194
12.748437	636.577606	12.260211
12.630923	627.712322	12.265229
12.609734	641.149835	12.270247
12.667843	641.929592	12.275264
12.645027	649.219846	12.280282
12.357446	645.878626	12.285299
12.489683	637.075193	12.290317
12.566427	642.036636	12.295335
12.581228	632.210187	12.300352
12.895131	636.992459	12.305370
12.473638	633.744807	12.310387
12.754336	619.894072	12.315405
12.724344	631.707716	12.320423
12.518611	625.349345	12.325440
12.831524	636.812621	12.330458
12.701955	633.039547	12.335475
12.527618	630.128712	12.340493
12.455283	626.630694	12.345511
12.472551	640.930029	12.350528
12.953459	631.781634	12.355546
12.779234	638.262473	12.360563
12.655039	629.937878	12.365581
12.750539	648.027712	12.370599
12.664541	634.461639	12.375616
12.463471	634.164847	12.380634
12.380171	643.834589	12.385651
12.928252	635.808604	12.390669
12.640803	634.979391	12.395687
12.590628	627.971796	12.400704
12.798665	645.128810	12.405722
12.560147	658.830762	12.410739
13.001681	647.877090	12.415757
13.188512	656.166451	12.420775
12.917250	656.723259	12.425792
13.036429	657.796406	12.430810
12.882733	652.919417	12.435827
12.953491	647.417125	12.440845
12.752947	665.938370	12.445863
12.876022	659.433796	12.450880
13.055303	652.052568	12.455898
12.952215	658.777889	12.460915
13.078638	655.406515	12.465933
13.014695	658.414467	12.470951
13.135230	659.553674	12.475968
12.950706	663.341070	12.480986
13.160276	671.450149	12.486003
13.349202	649.910422	12.491021
12.973288	652.295064	12.496039
13.147807	661.918109	12.501056
13.220412	651.012772	12.506074
13.202764	655.446208	12.511091
13.324090	650.302066	12.516109
13.219224	640.926708	12.521127
12.868084	641.840014	12.526144
13.230752	640.757462	12.531162
13.115436	653.562791	12.536179
13.366324	653.608598	12.541197
13.362240	651.425324	12.546215
13.233974	650.388132	12.551232
13.500006	635.744418	12.556250
13.373665	636.411063	12.561267
13.326355	635.424304	12.566285
13.153356	624.282908	12.571303
13.362919	629.842076	12.576320
13.232870	619.763774	12.581338
13.221060	624.272027	12.586355
13.040716	622.690730	12.591373
13.406265	641.489329	12.596391
13.421406	649.572056	12.601408
13.480033	645.043656	12.606426
13.347933	647.614159	12.611443
13.394649	642.547981	12.616461
13.619742	635.850705	12.621479
13.146349	638.537797	12.626496
13.471336	635.255237	12.631514
13.668583	648.781608	12.636531
13.438131	638.229875	12.641549
13.172646	634.282435	12.646567
13.361274	639.406229	12.651584
13.550418	657.172131	12.656602
13.241990	645.736359	12.661619
13.460570	647.791169	12.666637
13.568954	653.363042	12.671655
13.563240	653.799348	12.676672
13.307678	633.638946	12.681690
13.176805	653.411587	12.686707
13.320512	642.823319	12.691725
13.316513	644.101958	12.696743
13.024585	658.853696	12.701760
13.636142	659.988554	12.706778
13.396409	673.555007	12.711795
13.950671	678.599434	12.716813
13.767921	673.282021	12.721831
13.460618	664.509572	12.726848
13.847368	670.820477	12.731866
13.998878	669.625840	12.736883
13.877388	655.677145	12.741901
13.790695	656.107205	12.746919
13.480169	658.481602	12.751936
13.595742	646.042121	12.756954
13.487967	658.294005	12.761971
13.976278	668.959801	12.766989
14.151306	673.934256	12.772007
13.726628	662.734440	12.777024
14.019904	651.295909	12.782042
13.508904	656.545104	12.787059
13.598003	650.686485	12.792077
13.535263	666.030327	12.797095
13.710139	682.419398	12.802112
13.850147	677.733071	12.807130
14.057016	679.922264	12.812147
14.136673	675.854466	12.817165
13.901340	678.693613	12.822183
14.122198	675.342154	12.827200
14.551324	668.698105	12.832218
14.034377	669.384925	12.837235
13.695079	658.790274	12.842253
14.097574	653.911347	12.847271
13.659058	653.935781	12.852288
14.233482	665.023586	12.857306
14.100179	671.494869	12.862323
14.096392	664.871313	12.867341
14.199584	648.135550	12.872359
13.613679	663.450905	12.877376
14.023573	672.620510	12.882394
14.094038	673.688668	12.887411
14.011933	673.275406	12.892429
14.132931	678.618091	12.897447
13.975622	683.316414	12.902464
14.391649	682.998675	12.907482
14.530649	677.977989	12.912499
14.144318	674.055786	12.917517
14.331996	676.595125	12.922535
14.209001	680.183535	12.927552
14.260334	685.754889	12.932570
14.137619	683.871066	12.937587
14.116146	681.636864	12.942605
14.476487	676.666705	12.947623
14.406265	689.452372	12.952640
14.252743	670.336296	12.957658
13.997675	675.040466	12.962675
14.352885	673.280580	12.967693
14.475000	676.817962	12.972711
14.101431	688.609736	12.977728
14.410333	675.407794	12.982746
14.776572	675.523891	12.987763
14.123714	676.452913	12.992781
14.167096	681.687839	12.997799
14.386405	676.944906	13.002816
14.517786	679.470975	13.007834
14.451503	679.680086	13.012851
14.443773	680.728938	13.017869
14.375979	674.983257	13.022887
14.450576	679.111911	13.027904
14.401278	672.059980	13.032922
14.209809	675.845310	13.037939
14.082465	676.168130	13.042957
14.100301	672.880038	13.047975
13.877320	672.596146	13.052992
14.376896	689.581293	13.058010
14.371386	700.292921	13.063027
14.101123	701.840502	13.068045
14.288818	693.874112	13.073063
14.497680	704.470104	13.078080
14.817819	689.095185	13.083098
14.677486	704.283959	13.088115
14.773312	702.066090	13.093133
14.735521	704.262060	13.098151
14.854504	702.311964	13.103168
15.011906	699.377543	13.108186
15.039126	698.262338	13.113203
14.959225	703.055836	13.118221
14.844689	693.571511	13.123239
14.631681	697.486454	13.128256
14.773850	695.103534	13.133274
15.012018	695.381709	13.138291
14.632429	696.135372	13.143309
14.844436	697.023564	13.148327
14.624883	696.934795	13.153344
14.606504	704.110767	13.158362
15.042402	694.824224	13.163379
14.558797	695.490042	13.168397
14.905343	689.266026	13.173415
14.685632	696.116931	13.178432
14.609992	691.748412	13.183450
14.535116	690.551373	13.188467
14.560561	694.908640	13.193485
14.440033	687.795279	13.198503
14.869763	698.107352	13.203520
14.854686	699.106863	13.208538
15.203547	715.604405	13.213555
15.059957	718.501768	13.218573
15.356823	713.563636	13.223591
14.914013	718.322479	13.228608
14.958133	718.021984	13.233626
15.648973	712.312064	13.238643
15.139068	699.550821	13.243661
15.324383	693.355220	13.248679
14.640661	688.274085	13.253696
14.736738	698.587942	13.258714
15.163593	706.104412	13.263731
15.253726	718.265369	13.268749
15.236096	710.268025	13.273767
15.221845	716.026390	13.278784
15.236629	719.482767	13.283802
15.442598	711.295754	13.288819
15.266448	718.843591	13.293837
15.497040	702.008922	13.298855
15.230939	703.562162	13.303872
14.857064	694.594999	13.308890
15.245502	708.220849	13.313907
15.256002	710.204125	13.318925
15.691261	706.897963	13.323943
15.485055	722.848159	13.328960
15.018099	706.454139	13.333978
15.423061	708.826894	13.338995
15.369051	708.844732	13.344013
15.564181	709.729257	13.349031
15.044293	715.011420	13.354048
15.521064	709.877843	13.359066
15.570006	713.180543	13.364083
15.250234	714.382429	13.369101
15.254960	703.768563	13.374119
15.612825	714.224450	13.379136
15.383590	710.208197	13.384154
15.654109	709.032781	13.389171
15.635052	707.520880	13.394189
15.722049	711.638132	13.399207
15.664883	719.678571	13.404224
16.057231	710.957424	13.409242
15.698673	706.611138	13.414259
15.186748	694.468756	13.419277
15.503730	697.161409	13.424295
15.644354	710.049755	13.429312
15.689177	712.403198	13.434330
15.389706	707.192425	13.439347
15.283189	712.438223	13.444365
15.285921	708.376159	13.449383
15.196977	712.451548	13.454400
15.232106	714.749705	13.459418
15.448058	709.672772	13.464435
15.537929	726.630627	13.469453
15.860804	730.786666	13.474471
15.667272	739.337633	13.479488
15.960872	734.093891	13.484506
16.174440	739.983829	13.489523
15.829469	730.898509	13.494541
15.519404	711.617567	13.499559
15.827647	722.601944	13.504576
16.037539	727.081799	13.509594
16.310605	730.857475	13.514611
15.904441	728.345866	13.519629
15.928095	709.148340	13.524647
15.883407	720.222727	13.529664
15.616929	718.468723	13.534682
15.882761	715.129144	13.539699
15.564576	736.019984	13.544717
16.043057	735.162279	13.549735
16.114707	732.364366	13.554752
16.053428	734.529307	13.559770
16.301108	731.170479	13.564787
15.942522	734.142555	13.569805
16.133333	734.478644	13.574823
15.977862	732.505273	13.579840
16.363353	734.294099	13.584858
16.193763	734.917030	13.589875
15.996080	734.032722	13.594893
15.889536	744.034366	13.599911
16.065184	741.576766	13.604928
15.965370	738.117746	13.609946
16.183308	733.558051	13.614963
15.984137	738.856243	13.619981
16.260429	728.272398	13.624999
16.572841	730.280958	13.630016
16.243634	734.109972	13.635034
16.600951	730.923316	13.640051
16.551989	738.580623	13.645069
16.557835	732.350011	13.650087
16.222496	730.281745	13.655104
16.218621	736.013244	13.660122
16.286820	728.153924	13.665139
16.113270	732.637053	13.670157
16.392188	727.698573	13.675175
16.461290	728.931051	13.680192
16.193452	730.964252	13.685210
16.556110	732.693538	13.690227
16.523126	738.309677	13.695245
16.305197	734.755554	13.700263
16.732931	725.135757	13.705280
16.663403	736.532785	13.710298
16.679201	721.508482	13.715315
16.400491	723.704332	13.720333
16.555437	728.890234	13.725351
16.565406	725.950506	13.730368
16.640082	735.052744	13.735386
16.735424	729.104759	13.740403
16.416792	728.021649	13.745421
16.759122	732.588053	13.750439
16.704051	734.086141	13.755456
16.412844	734.352584	13.760474
16.783798	724.618606	13.765491
16.618650	734.518973	13.770509
16.469650	736.268465	13.775527
16.694816	738.836654	13.780544
16.562616	735.619396	13.785562
16.354745	728.614378	13.790579
16.497433	734.812067	13.795597
16.732560	733.055210	13.800615
16.582491	729.250613	13.805632
16.568652	735.466515	13.810650
16.837777	733.237269	13.815667
16.592197	755.710449	13.820685
17.100522	759.483984	13.825703
17.047837	748.519322	13.830720
16.685823	747.449320	13.835738
16.939201	751.499486	13.840755
16.899022	758.044573	13.845773
16.759267	754.765379	13.850791
17.051426	758.818938	13.855808
17.111837	759.270133	13.860826
17.116796	763.573821	13.865843
16.935805	756.226907	13.870861
16.733270	761.841216	13.875879
17.132333	755.078768	13.880896
16.685103	755.849344	13.885914
16.995693	759.792717	13.890931
16.800481	757.598350	13.895949
16.700819	744.005931	13.900967
16.853242	751.246680	13.905984
16.658147	750.740665	13.911002
16.868352	750.111187	13.916019
17.154326	773.157518	13.921037
17.179114	772.418234	13.926055
17.590756	762.936639	13.931072
17.294762	771.065014	13.936090
17.195367	760.356974	13.941107
16.882396	752.011406	13.946125
17.493506	758.552281	13.951143
17.529570	767.313443	13.956160
16.820909	765.511949	13.961178
17.239025	778.123336	13.966195
17.219091	784.564274	13.971213
17.225440	780.318588	13.976231
17.184639	777.636117	13.981248
17.424664	783.181093	13.986266
17.332514	777.426572	13.991283
17.205473	781.624712	13.996301
17.327807	778.531670	14.001319
17.562919	777.876198	14.006336
17.568816	785.218814	14.011354
17.374761	779.212012	14.016371
17.368698	781.841682	14.021389
17.492404	781.560274	14.026407
17.499913	774.139637	14.031424
17.235222	774.790094	14.036442
17.108041	771.789795	14.041459
17.087141	782.513352	14.046477
17.659781	799.970000	14.051495
17.884853	793.966953	14.056512
17.673757	801.529768	14.061530
18.027397	792.880919	14.066547
17.705094	785.676056	14.071565
17.525033	773.904506	14.076583
17.885842	773.781611	14.081600
17.441485	775.425903	14.086618
17.714168	797.063689	14.091635
17.448956	797.259787	14.096653
17.744112	803.013884	14.101671
18.118846	796.409869	14.106688
17.742769	803.588276	14.111706
17.785836	797.487510	14.116723
17.528409	801.772357	14.121741
17.626519	812.297402	14.126759
18.028966	797.275573	14.131776
17.987236	804.998048	14.136794
17.817666	804.510123	14.141811
17.961602	802.657093	14.146829
17.685614	804.319189	14.151847
17.705576	797.635058	14.156864
17.663164	806.720963	14.161882
18.058233	803.465263	14.166899
18.191405	797.713301	14.171917
18.477540	804.204123	14.176935
18.325090	804.944293	14.181952
18.086493	798.704620	14.186970
18.434432	799.322208	14.191987
18.115420	804.976871	14.197005
18.210397	802.752811	14.202023
18.355793	799.476268	14.207040
18.372797	801.912977	14.212058
18.309374	797.252181	14.217075
18.321052	790.042325	14.222093
18.259968	784.762621	14.227111
18.401626	774.218778	14.232128
18.174976	780.837271	14.237146
18.334153	770.940788	14.242163
18.307525	773.460069	14.247181
17.974457	774.320056	14.252199
18.772564	781.882534	14.257216
18.550730	779.080103	14.262234
18.376402	767.380243	14.267251
18.644507	772.324364	14.272269
18.230976	773.209581	14.277287
18.139331	770.292079	14.282304
17.980113	783.072821	14.287322
17.977759	778.926330	14.292339
18.226141	792.331188	14.297357
18.107225	784.766251	14.302375
18.798126	785.797167	14.307392
18.619091	788.210940	14.312410
18.672056	783.042757	14.317427
18.922183	789.753812	14.322445
18.407559	792.608333	14.327463
18.837049	792.307418	14.332480
18.458836	784.738926	14.337498
18.390705	793.125102	14.342515
18.517061	787.759225	14.347533
18.484438	792.226599	14.352551
18.302843	792.709401	14.357568
18.267219	785.655283	14.362586
18.311216	789.877120	14.367603
18.754622	795.933039	14.372621
18.503247	792.384145	14.377639
18.843093	802.779790	14.382656
19.114640	808.960471	14.387674
18.874936	805.144655	14.392691
18.804217	799.263691	14.397709
18.473655	800.025456	14.402727
18.831761	800.183854	14.407744
18.707853	810.506996	14.412762
18.810293	806.606014	14.417779
18.969105	808.335688	14.422797
19.110714	816.695326	14.427815
19.184032	810.138531	14.432832
19.311537	814.227369	14.437850
19.116293	809.527261	14.442867
19.078635	795.218180	14.447885
19.176738	797.424429	14.452903
18.729218	791.927556	14.457920
18.850559	795.521888	14.462938
19.167816	799.173889	14.467955
19.156025	797.446245	14.472973
18.868212	791.129078	14.477991
19.204154	796.513861	14.483008
19.166874	805.166612	14.488026
19.140800	813.842858	14.493043
19.129079	805.137637	14.498061
19.022050	818.670785	14.503079
18.954202	813.243808	14.508096
19.208574	813.816096	14.513114
19.157280	815.667053	14.518131
19.310011	818.022537	14.523149
19.405263	816.315991	14.528167
19.017104	813.252432	14.533184
19.138150	823.205839	14.538202
19.041430	816.760891	14.543219
19.441746	809.212422	14.548237
19.146167	816.719052	14.553255
19.242847	811.941647	14.558272
19.184197	818.675845	14.563290
19.197645	816.900064	14.568307
19.249541	820.707256	14.573325
19.574049	832.721114	14.578343
19.724214	833.798885	14.583360
19.656735	832.120989	14.588378
19.291902	819.583086	14.593395
19.454468	828.337081	14.598413
19.599715	831.773039	14.603431
19.585257	833.028084	14.608448
19.702093	837.301637	14.613466
19.539395	845.289239	14.618483
19.741438	837.270044	14.623501
19.818886	838.479131	14.628519
19.838954	836.071141	14.633536
19.646597	847.818848	14.638554
19.510133	843.295717	14.643571
19.914219	833.124138	14.648589
19.785827	835.962334	14.653607
19.815359	852.232321	14.658624
19.681717	838.859751	14.663642
19.561570	832.686715	14.668659
19.909250	831.477110	14.673677
19.847373	834.835066	14.678695
20.061211	831.860223	14.683712
20.132712	841.117649	14.688730
19.921427	836.019255	14.693747
20.326460	833.143846	14.698765
20.179910	840.245279	14.703783
19.769939	824.602779	14.708800
20.011382	827.316755	14.713818
19.857536	835.975161	14.718835
20.147779	832.972568	14.723853
20.054873	835.779956	14.728871
20.103657	832.991922	14.733888
20.110752	831.741004	14.738906
20.010579	825.792062	14.743923
20.433176	827.104863	14.748941
20.331734	838.863566	14.753959
20.174808	827.612226	14.758976
20.277766	823.957315	14.763994
20.139094	836.457162	14.769011
20.377236	831.884809	14.774029
20.248303	828.326191	14.779047
20.289055	831.772209	14.784064
20.298005	827.879559	14.789082
20.405744	825.988016	14.794099
20.422319	825.436211	14.799117
20.105160	827.593916	14.804135
20.118575	829.302191	14.809152
20.524568	835.405011	14.814170
20.053632	836.346563	14.819187
20.603517	827.749002	14.824205
20.713017	846.480637	14.829223
20.481943	835.231442	14.834240
20.493754	836.302488	14.839258
20.397069	840.896678	14.844275
20.525254	835.934448	14.849293
20.314610	838.100712	14.854311
20.333050	835.314276	14.859328
20.284816	835.103988	14.864346
20.315320	836.610768	14.869363
20.399604	835.900030	14.874381
19.821586	842.242234	14.879399
20.069584	842.316897	14.884416
20.299064	856.778818	14.889434
20.295098	864.615325	14.894451
20.715894	864.404135	14.899469
20.446837	865.443448	14.904487
20.298036	862.301353	14.909504
20.754479	866.654250	14.914522
20.610182	865.401803	14.919539
20.484685	867.576821	14.924557
20.769964	878.350295	14.929575
20.817757	878.825561	14.934592
21.078543	876.190499	14.939610
21.346748	881.156726	14.944627
21.092703	876.102891	14.949645
21.121458	868.284404	14.954663
20.997967	861.319763	14.959680
21.370600	853.160222	14.964698
20.696166	868.133011	14.969715
21.062156	858.516505	14.974733
21.317574	858.283888	14.979751
21.416573	850.154598	14.984768
21.322883	862.221376	14.989786
21.066264	852.058629	14.994803
21.374403	848.097007	14.999821
20.946321	849.868145	15.004839
20.997581	850.033595	15.009856
21.086747	846.399775	15.014874
21.016586	852.861231	15.019891
20.942278	847.959126	15.024909
21.224604	863.359528	15.029927
21.445906	867.042356	15.034944
21.605918	867.231792	15.039962
20.615388	867.797157	15.044979
21.393152	861.578102	15.049997
21.542268	876.295632	15.055015
21.471289	884.821155	15.060032
21.706652	872.350125	15.065050
21.606345	868.162155	15.070067
21.489912	854.771098	15.075085
21.167084	849.885839	15.080103
21.401296	869.415323	15.085120
21.900108	871.088577	15.090138
21.290811	869.249412	15.095155
21.528642	865.301958	15.100173
21.619861	873.802063	15.105191
21.705376	872.554635	15.110208
22.061726	873.246649	15.115226
21.334730	856.795400	15.120243
21.514015	862.031177	15.125261
21.375636	866.464646	15.130279
21.244809	874.169553	15.135296
21.250138	869.614732	15.140314
21.386962	875.153815	15.145331
21.521075	865.816636	15.150349
21.198391	876.025791	15.155367
21.177499	879.680295	15.160384
21.783801	884.969097	15.165402
21.853524	889.237421	15.170419
22.096721	899.133862	15.175437
22.205078	902.417820	15.180455
21.854828	897.243350	15.185472
22.233614	897.508965	15.190490
21.980042	896.207364	15.195507
21.953367	890.701327	15.200525
22.076674	887.589178	15.205543
21.711890	882.208704	15.210560
21.765036	886.296585	15.215578
21.653399	889.170034	15.220595
21.955504	886.594769	15.225613
22.187095	885.728403	15.230631
22.253374	885.771577	15.235648
22.550192	890.780661	15.240666
22.469866	894.494974	15.245683
22.423297	887.108010	15.250701
22.310735	883.496322	15.255719
22.377338	891.227108	15.260736
22.281890	863.858632	15.265754
22.001095	868.923495	15.270771
22.103205	890.471354	15.275789
22.413569	877.149112	15.280807
22.191502	885.916062	15.285824
21.844653	882.915447	15.290842
21.881974	882.966314	15.295859
22.327564	880.826168	15.300877
22.204605	885.828436	15.305895
22.470523	886.395761	15.310912
22.422987	886.712392	15.315930
22.278018	891.503512	15.320947
22.189443	883.722337	15.325965
22.424533	883.549710	15.330983
22.436714	905.891173	15.336000
22.705249	897.378687	15.341018
22.395115	916.674768	15.346035
22.843344	906.695051	15.351053
23.117564	897.070812	15.356071
22.732224	900.103913	15.361088
22.787779	886.979379	15.366106
22.537798	885.759268	15.371123
22.574374	877.687084	15.376141
22.638959	888.599285	15.381159
22.606658	903.316858	15.386176
22.880659	907.165010	15.391194
23.027507	908.685126	15.396211
22.915949	902.210913	15.401229
23.046429	905.270496	15.406247
22.540486	910.184451	15.411264
23.004738	901.707571	15.416282
23.246310	904.812865	15.421299
23.333850	903.577741	15.426317
23.128656	892.059364	15.431335
22.557084	880.361707	15.436352
23.078547	886.528506	15.441370
23.160875	901.912939	15.446387
23.194422	899.042073	15.451405
23.258111	882.258630	15.456423
22.991657	878.939303	15.461440
22.968296	875.777551	15.466458
22.914919	890.340623	15.471475
23.334892	889.009233	15.476493
23.627006	899.156790	15.481511
23.296980	895.623353	15.486528
23.167768	877.446847	15.491546
22.900559	889.739649	15.496563
23.329665	889.801716	15.501581
23.333798	906.015770	15.506599
23.245891	915.061521	15.511616
23.428539	906.736059	15.516634
23.391852	905.226904	15.521651
23.422340	907.620489	15.526669
23.532445	902.923009	15.531687
23.491410	908.613048	15.536704
23.478390	898.232224	15.541722
23.286892	907.186902	15.546739
23.361241	906.263119	15.551757
23.180890	892.923074	15.556775
23.243396	907.139794	15.561792
23.329970	895.869195	15.566810
23.145131	905.823236	15.571827
23.341342	903.065741	15.576845
23.742735	902.570408	15.581863
22.904250	910.357802	15.586880
24.080288	916.194831	15.591898
24.019789	923.203918	15.596915
23.922999	925.014677	15.601933
23.869457	910.417653	15.606951
23.447285	910.398499	15.611968
23.625693	917.392243	15.616986
23.569357	924.624744	15.622003
23.415558	925.917407	15.627021
23.518025	925.598298	15.632039
23.449341	925.258668	15.637056
23.984401	927.314419	15.642074
23.929785	922.557534	15.647091
23.986940	930.381337	15.652109
24.298079	922.139880	15.657127
23.849816	921.522044	15.662144
24.058977	922.353888	15.667162
23.773773	921.274996	15.672179
23.807099	928.035850	15.677197
24.111452	925.031031	15.682215
24.046626	942.190057	15.687232
24.441746	943.131625	15.692250
24.356091	937.843102	15.697267
24.274752	934.608371	15.702285
24.352715	929.663451	15.707303
23.858935	934.818508	15.712320
24.026594	942.583977	15.717338
24.292243	944.334795	15.722355
24.754267	940.535239	15.727373
25.091605	932.251802	15.732391
24.392666	930.180518	15.737408
24.346781	921.209189	15.742426
24.762484	925.006741	15.747443
24.684004	926.735735	15.752461
24.344469	922.130790	15.757479
24.508986	929.770511	15.762496
24.511674	920.239296	15.767514
24.304174	914.398660	15.772531
24.187966	915.941056	15.777549
24.284976	924.613851	15.782567
24.090588	932.294026	15.787584
24.204389	935.378318	15.792602
24.385504	942.302219	15.797619
24.662242	940.040197	15.802637
24.897240	931.936899	15.807655
24.664720	934.466370	15.812672
24.598365	932.460079	15.817690
24.529200	940.988501	15.822707
24.491917	934.474237	15.827725
24.812408	931.034534	15.832743
24.580317	947.023700	15.837760
24.786438	953.296735	15.842778
24.901630	958.728779	15.847795
24.507306	965.190570	15.852813
25.092640	959.017412	15.857831
24.996638	968.225407	15.862848
24.813249	965.230727	15.867866
25.288489	959.576601	15.872883
25.083741	963.401943	15.877901
25.525001	963.525224	15.882919
25.425109	966.409468	15.887936
25.020198	948.102514	15.892954
25.218281	946.521857	15.897971
25.439885	958.583482	15.902989
25.475060	952.673253	15.908007
25.051822	933.838999	15.913024
25.163649	934.888068	15.918042
24.821411	933.764461	15.923059
24.940205	952.718818	15.928077
25.298137	950.472475	15.933095
25.556844	958.204751	15.938112
25.313218	966.277671	15.943130
25.315366	952.697544	15.948147
25.222743	959.635938	15.953165
25.121856	955.321803	15.958183
25.581541	961.974844	15.963200
25.233535	954.221661	15.968218
25.480358	956.874853	15.973235
25.502002	956.871371	15.978253
25.601114	950.443030	15.983271
25.487099	952.512115	15.988288
25.537574	955.959790	15.993306
25.590883	950.321281	15.998323
25.005539	958.460361	16.003341
25.537254	969.779115	16.008359
25.571066	979.840953	16.013376
25.662105	975.884915	16.018394
26.182700	977.819860	16.023411
25.802402	982.723616	16.028429
26.324961	973.252935	16.033447
25.993651	967.365406	16.038464
26.138388	964.565473	16.043482
26.053337	958.920235	16.048499
26.011314	944.577004	16.053517
25.778848	942.293774	16.058535
25.801150	951.871397	16.063552
26.134321	954.918166	16.068570
26.235176	945.431519	16.073587
25.987229	949.323588	16.078605
26.283966	939.547472	16.083623
26.131801	949.963486	16.088640
25.858081	945.569134	16.093658
25.891467	956.697708	16.098675
26.109375	959.273378	16.103693
26.381103	976.010470	16.108711
26.214243	976.711879	16.113728
25.984600	976.902405	16.118746
26.045515	970.154987	16.123763
26.288265	976.469629	16.128781
26.353403	960.635803	16.133799
26.080204	972.292114	16.138816
26.365274	970.893491	16.143834
26.241636	962.290937	16.148851
26.260551	975.012348	16.153869
26.047812	964.899467	16.158887
26.279849	968.706870	16.163904
26.210762	970.667930	16.168922
26.430082	970.418877	16.173939
26.303881	986.388332	16.178957
26.619117	986.414591	16.183975
26.534746	988.172917	16.188992
26.829043	992.680641	16.194010
26.891986	994.699915	16.199027
26.522866	993.056641	16.204045
26.711649	986.358612	16.209063
26.922398	990.219848	16.214080
26.553967	992.328800	16.219098
26.788584	993.112476	16.224115
26.532566	992.202580	16.229133
26.709857	986.692960	16.234151
26.586394	991.629062	16.239168
26.577671	992.526606	16.244186
26.860007	990.187959	16.249203
26.609390	997.280512	16.254221
26.718331	989.787088	16.259239
26.792913	987.758708	16.264256
27.228691	1002.488234	16.269274
27.119008	1003.370038	16.274291
26.424450	1007.051220	16.279309
27.027847	1009.209886	16.284327
27.346886	1011.034399	16.289344
27.069253	1020.018408	16.294362
27.244694	1016.285829	16.299379
27.466331	1015.039155	16.304397
27.360805	1014.872556	16.309415
27.129516	1027.112486	16.314432
27.304334	1020.779558	16.319450
27.473384	1022.564455	16.324467
27.290945	1015.315493	16.329485
27.273773	1015.374898	16.334503
27.453747	1023.091134	16.339520
27.319745	1010.640009	16.344538
27.500171	1011.470047	16.349555
27.184191	1007.397889	16.354573
27.411866	1016.084970	16.359591
27.523202	1015.982226	16.364608
27.500754	1009.071125	16.369626
27.642018	1011.295886	16.374643
27.359872	1012.637066	16.379661
27.301084	1007.887123	16.384679
27.248028	1003.855824	16.389696
27.428111	1029.730964	16.394714
27.841545	1028.889750	16.399731
28.139874	1041.154010	16.404749
28.091826	1038.002409	16.409767
27.945546	1018.480872	16.414784
27.450885	1014.054846	16.419802
27.641928	1024.634886	16.424819
28.120946	1038.789608	16.429837
28.052316	1034.066448	16.434855
28.191330	1023.911046	16.439872
27.710825	1031.342595	16.444890
27.976022	1026.317819	16.449907
27.976103	1032.257081	16.454925
28.120561	1035.787879	16.459943
27.983688	1025.445321	16.464960
27.947080	1043.862376	16.469978
27.973577	1035.009041	16.474995
27.827542	1034.656280	16.480013
27.943096	1030.819469	16.485031
28.361065	1035.654974	16.490048
28.218584	1044.649379	16.495066
28.211918	1025.620369	16.500083
28.209952	1030.313379	16.505101
28.063930	1029.935370	16.510119
28.479249	1027.676871	16.515136
28.197608	1036.125017	16.520154
28.539391	1033.496177	16.525171
28.473532	1045.666018	16.530189
28.452010	1031.133307	16.535207
28.527079	1026.422349	16.540224
28.161341	1035.533782	16.545242
28.734114	1033.133845	16.550259
28.303288	1038.222262	16.555277
28.628380	1046.963525	16.560295
28.536812	1050.932102	16.565312
28.590426	1063.490345	16.570330
29.075352	1059.210637	16.575347
28.803677	1060.547025	16.580365
28.560245	1061.598113	16.585383
28.810703	1055.067125	16.590400
28.705458	1062.884872	16.595418
28.832067	1060.229780	16.600435
29.010096	1066.923833	16.605453
28.932837	1056.164808	16.610471
29.052508	1043.026959	16.615488
29.088191	1062.811827	16.620506
29.232274	1050.212960	16.625523
28.736734	1038.989293	16.630541
28.896427	1048.592779	16.635559
29.089892	1043.004866	16.640576
28.781658	1058.908230	16.645594
29.083344	1059.545698	16.650611
29.278833	1060.382847	16.655629
29.079124	1054.547255	16.660647
29.258396	1055.765651	16.665664
28.789622	1066.013582	16.670682
29.232476	1051.641633	16.675699
29.465441	1069.413704	16.680717
29.094050	1065.037781	16.685735
28.937306	1054.262808	16.690752
28.780266	1062.457908	16.695770
29.086329	1064.596893	16.700787
29.564265	1070.881032	16.705805
29.629114	1081.484033	16.710823
29.703757	1080.405557	16.715840
29.521859	1079.976361	16.720858
29.613511	1080.353241	16.725875
29.366374	1078.769743	16.730893
29.731603	1080.751133	16.735911
29.607922	1073.511877	16.740928
29.533289	1084.638520	16.745946
29.582512	1086.104517	16.750963
29.474911	1081.109732	16.755981
29.779006	1075.009001	16.760999
29.750728	1074.628322	16.766016
29.641892	1072.530838	16.771034
29.560499	1071.107571	16.776051
29.904973	1081.477408	16.781069
29.883399	1069.611401	16.786087
30.125761	1072.438883	16.791104
29.933229	1079.386665	16.796122
30.110928	1081.615193	16.801139
29.715678	1074.308028	16.806157
29.890509	1077.998182	16.811175
30.134781	1081.491259	16.816192
30.098769	1080.123998	16.821210
30.073652	1074.491425	16.826227
30.059351	1073.723538	16.831245
29.974876	1071.410793	16.836263
29.908955	1083.918349	16.841280
30.025544	1096.605608	16.846298
30.129851	1106.075788	16.851315
30.130684	1096.194466	16.856333
30.324656	1098.571930	16.861351
30.373469	1103.209665	16.866368
30.305154	1101.487692	16.871386
30.418769	1088.710530	16.876403
30.541439	1098.209387	16.881421
30.255814	1095.388497	16.886439
30.441773	1097.978661	16.891456
30.590174	1100.678854	16.896474
30.376052	1093.535812	16.901491
30.621502	1088.905443	16.906509
30.341209	1104.267968	16.911527
30.417096	1096.855418	16.916544
30.322787	1099.252802	16.921562
30.867413	1115.978827	16.926579
30.713457	1114.797306	16.931597
30.867105	1124.313415	16.936615
31.119445	1120.647663	16.941632
30.950706	1107.147843	16.946650
30.967813	1094.209068	16.951667
31.158931	1093.320630	16.956685
30.773798	1097.830688	16.961703
30.647782	1087.779891	16.966720
31.011816	1106.045874	16.971738
30.765073	1112.860147	16.976755
30.936922	1120.804923	16.981773
31.197529	1120.479970	16.986791
31.141793	1120.737927	16.991808
31.341490	1118.718334	16.996826
31.147853	1118.044816	17.001843
31.549696	1112.623055	17.006861
31.121545	1122.391269	17.011879
31.573147	1105.919235	17.016896
31.719969	1113.703823	17.021914
31.373048	1102.261165	17.026931
31.498658	1083.018859	17.031949
31.265058	1083.203695	17.036967
31.294385	1091.555807	17.041984
31.409876	1098.319632	17.047002
31.288225	1109.882859	17.052019
31.486305	1099.345764	17.057037
31.447107	1107.127935	17.062055
31.379991	1106.210527	17.067072
31.208171	1100.581995	17.072090
31.680794	1103.398653	17.077107
31.878657	1104.409006	17.082125
31.454774	1113.545368	17.087143
31.542025	1100.074875	17.092160
31.400152	1103.786251	17.097178
31.682086	1096.070012	17.102195
31.965668	1094.886213	17.107213
31.681724	1106.433839	17.112231
32.027255	1104.227292	17.117248
31.749021	1121.451485	17.122266
31.866933	1122.518548	17.127283
32.201838	1127.673215	17.132301
32.104914	1133.163793	17.137319
32.307872	1139.367960	17.142336
32.389784	1129.524410	17.147354
32.305285	1115.291841	17.152371
32.203882	1105.805239	17.157389
31.749078	1107.331272	17.162407
32.077569	1125.956304	17.167424
32.323139	1129.209339	17.172442
31.775003	1137.257460	17.177459
32.302961	1126.211060	17.182477
32.407577	1128.656178	17.187495
32.392950	1127.042559	17.192512
32.439292	1127.436006	17.197530
32.272768	1132.154826	17.202547
32.410114	1131.536751	17.207565
32.122485	1138.060785	17.212583
32.303216	1136.792109	17.217600
32.442738	1130.114368	17.222618
32.272269	1134.603425	17.227635
32.397920	1132.374519	17.232653
32.334106	1141.520754	17.237671
32.527360	1153.246115	17.242688
32.676425	1154.620734	17.247706
32.593886	1163.820409	17.252723
32.746502	1157.453040	17.257741
32.541837	1162.591267	17.262759
33.139496	1152.546975	17.267776
32.823395	1158.740952	17.272794
32.535860	1153.534489	17.277811
32.885922	1149.105471	17.282829
32.342044	1155.900041	17.287847
32.569650	1153.197552	17.292864
32.800842	1156.361323	17.297882
32.987988	1171.754813	17.302899
33.406675	1168.981357	17.307917
33.002551	1175.561527	17.312935
33.378213	1168.445974	17.317952
33.528190	1167.144244	17.322970
33.171540	1170.879817	17.327987
33.360240	1151.539187	17.333005
32.943000	1166.187896	17.338023
33.245096	1167.087245	17.343040
33.644887	1172.616779	17.348058
33.380027	1180.396467	17.353075
33.471537	1168.452715	17.358093
33.667696	1178.429267	17.363111
33.450680	1177.923517	17.368128
33.438879	1168.094629	17.373146
33.390254	1176.351693	17.378163
33.587053	1164.962666	17.383181
33.233163	1168.306474	17.388199
33.504836	1181.114666	17.393216
33.631470	1167.732629	17.398234
33.782871	1174.910593	17.403251
33.771512	1171.248275	17.408269
33.347306	1179.314869	17.413287
33.492674	1173.980612	17.418304
33.960858	1168.807224	17.423322
33.942212	1170.530023	17.428339
33.757453	1170.473670	17.433357
33.752517	1187.730849	17.438375
34.074238	1196.608418	17.443392
34.220171	1193.779859	17.448410
34.025799	1190.509141	17.453427
34.543980	1196.465117	17.458445
34.449716	1198.341782	17.463463
34.252111	1174.397218	17.468480
33.932539	1167.655689	17.473498
34.112458	1180.623428	17.478515
34.389500	1175.647250	17.483533
34.150843	1191.281045	17.488551
34.075154	1186.565262	17.493568
34.296548	1186.249607	17.498586
33.984945	1188.359145	17.503603
34.306692	1183.723110	17.508621
34.431886	1181.128183	17.513639
34.418217	1181.660426	17.518656
34.438897	1185.295856	17.523674
34.110641	1194.212142	17.528691
34.192524	1186.135875	17.533709
34.327669	1194.411494	17.538727
34.233727	1206.970865	17.543744
34.636374	1206.150270	17.548762
34.643308	1217.191630	17.553779
34.901570	1211.094878	17.558797
34.746234	1210.743571	17.563815
34.836895	1210.543077	17.568832
34.978689	1203.170652	17.573850
34.619763	1214.231461	17.578867
35.063913	1210.330504	17.583885
35.217695	1207.832084	17.588903
35.001858	1202.614373	17.593920
34.926075	1210.266617	17.598938
35.232148	1207.491863	17.603955
35.121715	1203.879777	17.608973
35.340628	1210.879914	17.613991
35.238469	1206.319757	17.619008
35.198879	1195.437977	17.624026
35.105981	1208.044524	17.629043
35.418219	1203.839178	17.634061
35.563535	1206.946983	17.639079
35.189331	1200.479097	17.644096
35.295408	1206.417590	17.649114
35.070092	1213.531511	17.654131
35.199175	1204.015057	17.659149
35.470197	1208.302414	17.664167
35.321151	1210.970329	17.669184
35.571443	1203.079115	17.674202
35.445642	1229.990270	17.679219
35.357165	1226.273750	17.684237
35.503728	1234.367711	17.689255
35.641024	1238.770704	17.694272
35.627740	1229.557418	17.699290
35.476560	1233.500661	17.704307
35.686055	1225.571646	17.709325
35.825320	1227.746252	17.714343
35.910887	1228.758427	17.719360
36.241803	1226.307994	17.724378
35.521148	1231.896326	17.729395
35.925778	1221.131131	17.734413
35.820213	1222.955918	17.739431
35.612776	1238.761595	17.744448
36.658313	1237.354261	17.749466
36.220880	1243.652486	17.754483
35.819228	1238.653233	17.759501
36.541602	1239.268980	17.764519
35.904505	1236.518914	17.769536
36.560523	1243.336967	17.774554
36.049466	1245.799665	17.779571
36.103945	1252.143903	17.784589
36.367909	1241.485944	17.789607
36.164382	1254.599025	17.794624
36.653436	1243.385072	17.799642
36.705650	1255.328266	17.804659
36.343886	1246.841781	17.809677
36.210875	1247.354853	17.814695
36.438980	1255.420268	17.819712
36.811153	1245.035699	17.824730
36.565823	1256.059800	17.829747
36.846641	1251.231337	17.834765
36.351496	1248.578953	17.839783
36.223622	1242.236566	17.844800
36.919948	1254.564853	17.849818
36.787606	1267.628918	17.854835
36.903511	1264.596762	17.859853
36.738876	1260.829048	17.864871
37.177842	1271.793284	17.869888
37.369279	1263.655635	17.874906
36.862633	1256.435279	17.879923
37.079414	1265.136813	17.884941
37.281473	1270.801503	17.889959
37.258803	1258.133939	17.894976
37.124923	1238.373524	17.899994
37.279870	1249.363311	17.905011
37.251275	1253.886976	17.910029
37.087374	1249.932950	17.915047
36.846155	1266.624445	17.920064
37.519127	1253.860516	17.925082
37.210294	1262.600217	17.930099
37.434164	1264.818379	17.935117
37.270976	1268.198601	17.940135
37.464096	1274.432759	17.945152
37.574226	1266.923253	17.950170
37.251046	1273.156249	17.955187
37.318807	1265.760682	17.960205
37.305402	1259.138413	17.965223
37.410217	1263.754792	17.970240
37.779661	1274.007216	17.975258
37.649341	1284.309544	17.980275
37.909280	1290.681568	17.985293
38.126138	1285.342389	17.990311
37.840181	1293.204329	17.995328
37.886890	1287.522565	18.000346
37.817345	1289.322780	18.005363
37.889694	1288.563399	18.010381
38.139997	1271.469475	18.015399
37.830152	1284.580299	18.020416
38.393367	1282.765675	18.025434
38.227242	1286.676556	18.030451
37.931768	1289.638834	18.035469
38.059205	1278.289005	18.040487
38.120357	1285.607390	18.045504
38.137076	1285.197565	18.050522
38.334321	1276.557208	18.055539
37.981710	1285.234349	18.060557
38.218558	1284.149382	18.065575
37.845913	1284.169805	18.070592
38.109062	1284.122172	18.075610
38.097918	1300.332666	18.080627
38.346188	1309.101874	18.085645
38.746992	1307.284290	18.090663
38.495752	1308.112544	18.095680
38.371651	1309.394269	18.100698
38.554449	1311.697770	18.105715
38.747714	1311.446483	18.110733
38.781053	1300.237621	18.115751
38.731725	1310.965949	18.120768
38.805018	1304.260649	18.125786
39.089207	1309.151905	18.130803
38.871940	1319.392134	18.135821
39.253786	1313.821961	18.140839
39.064590	1315.148600	18.145856
38.751756	1312.650687	18.150874
39.210936	1322.945886	18.155891
39.209652	1324.564990	18.160909
39.194606	1321.865778	18.165927
39.461219	1326.649335	18.170944
39.244726	1322.946540	18.175962
39.502997	1328.599286	18.180979
38.922645	1333.506077	18.185997
39.482559	1328.040550	18.191015
39.508041	1337.460084	18.196032
39.472508	1328.720468	18.201050
39.577956	1331.859789	18.206067
39.843997	1332.446046	18.211085
39.752644	1319.946995	18.216103
39.238072	1309.332077	18.221120
39.928283	1317.243065	18.226138
39.712483	1321.982278	18.231155
39.733351	1309.216334	18.236173
39.616150	1315.076232	18.241191
39.670511	1319.735246	18.246208
39.552916	1321.252646	18.251226
39.647300	1318.526823	18.256243
39.415151	1323.483201	18.261261
39.885220	1320.124136	18.266279
39.571212	1326.169514	18.271296
40.046299	1326.880815	18.276314
39.896691	1321.902011	18.281331
39.404462	1324.513254	18.286349
39.946283	1336.433443	18.291367
39.923072	1348.353801	18.296384
40.067939	1340.614749	18.301402
40.229078	1337.300927	18.306419
39.865927	1344.824676	18.311437
39.961750	1343.278943	18.316455
40.062833	1353.011702	18.321472
40.111893	1352.246500	18.326490
40.181457	1355.565024	18.331507
40.598594	1374.088060	18.336525
41.005457	1370.634743	18.341543
40.699886	1374.333951	18.346560
40.695901	1369.815177	18.351578
40.784281	1373.111820	18.356595
40.828471	1379.309386	18.361613
41.215547	1372.902052	18.366631
40.940699	1362.170644	18.371648
40.576295	1348.477226	18.376666
40.997546	1354.498937	18.381683
40.652592	1366.229865	18.386701
41.053140	1363.651734	18.391719
41.111179	1366.085246	18.396736
40.953925	1370.199892	18.401754
40.758538	1366.168718	18.406771
41.362424	1374.494061	18.411789
41.311447	1372.065571	18.416807
41.114435	1373.847894	18.421824
41.215092	1370.543542	18.426842
41.345317	1370.718716	18.431859
41.117710	1370.432380	18.436877
41.434895	1369.603076	18.441895
41.194814	1371.827667	18.446912
41.239554	1364.956396	18.451930
41.218248	1364.091760	18.456947
41.217345	1365.161674	18.461965
41.355159	1362.981328	18.466983
41.191126	1370.609596	18.472000
41.290468	1374.851304	18.477018
41.807289	1389.338070	18.482035
41.756574	1400.704170	18.487053
41.984986	1391.497116	18.492071
41.827809	1382.849119	18.497088
42.052252	1387.137504	18.502106
42.177562	1387.313449	18.507123
41.887563	1397.905959	18.512141
42.651753	1385.888228	18.517159
42.408010	1380.472857	18.522176
41.995810	1367.907272	18.527194
42.217337	1359.862699	18.532211
41.954387	1356.533264	18.537229
41.998171	1360.124082	18.542247
42.294652	1354.971232	18.547264
41.717316	1360.025886	18.552282
41.912583	1370.949467	18.557299
41.939185	1386.036922	18.562317
42.208846	1384.732204	18.567335
42.273615	1387.811634	18.572352
41.900605	1383.202345	18.577370
42.050646	1378.795142	18.582387
41.959084	1404.751257	18.587405
42.228524	1397.475524	18.592423
41.873869	1407.873034	18.597440
42.181639	1405.359928	18.602458
42.568436	1408.707658	18.607475
42.992266	1431.165171	18.612493
42.696732	1414.358612	18.617511
42.719360	1422.219600	18.622528
42.807073	1421.511458	18.627546
42.637462	1429.607705	18.632563
42.687973	1434.917478	18.637581
43.178689	1435.159255	18.642599
43.490432	1430.688833	18.647616
43.295786	1424.741868	18.652634
43.432037	1425.903911	18.657651
43.409633	1432.364405	18.662669
42.914211	1425.530403	18.667687
43.535653	1432.950421	18.672704
43.336141	1428.187699	18.677722
43.808962	1422.764193	18.682739
43.562322	1426.772930	18.687757
43.317794	1426.558674	18.692775
43.527509	1428.892689	18.697792
43.174203	1432.312196	18.702810
43.728492	1417.180848	18.707827
43.631112	1430.621424	18.712845
43.787483	1429.798378	18.717863
44.127857	1419.358727	18.722880
43.809184	1427.453080	18.727898
43.882792	1422.685440	18.732915
43.425868	1432.029120	18.737933
43.810169	1422.636673	18.742951
43.816820	1430.610626	18.747968
43.442126	1424.874916	18.752986
43.827655	1413.667610	18.758003
43.666927	1418.527614	18.763021
43.865972	1422.753712	18.768039
43.938831	1430.171313	18.773056
43.948619	1441.701537	18.778074
44.266825	1438.625032	18.783091
44.156410	1447.576744	18.788109
44.229259	1443.471967	18.793127
44.424274	1448.494004	18.798144
44.383896	1442.390313	18.803162
44.415825	1437.635510	18.808179
44.394263	1447.112969	18.813197
44.589737	1438.393912	18.818215
44.892634	1439.438324	18.823232
44.534658	1445.784134	18.828250
44.756411	1444.133451	18.833267
44.519771	1443.312016	18.838285
44.551441	1444.632464	18.843303
44.656916	1439.815643	18.848320
44.218008	1441.332900	18.853338
44.647241	1447.009394	18.858355
44.814747	1460.462143	18.863373
44.973999	1466.701675	18.868391
45.185535	1472.876211	18.873408
45.458844	1474.114618	18.878426
45.124862	1459.396973	18.883443
45.056714	1478.485324	18.888461
45.343052	1476.745620	18.893479
45.563412	1467.625000	18.898496
45.150158	1454.160071	18.903514
45.364495	1450.888389	18.908531
45.002619	1463.534102	18.913549
45.067266	1469.210917	18.918567
45.151422	1463.008809	18.923584
45.124527	1465.200010	18.928602
45.283731	1465.979744	18.933619
45.168817	1475.165716	18.938637
45.076282	1470.367286	18.943655
45.479405	1480.611397	18.948672
45.856451	1487.230244	18.953690
46.068998	1480.272675	18.958707
46.003724	1491.903058	18.963725
45.730178	1487.101424	18.968743
45.965760	1485.792571	18.973760
45.964248	1491.072640	18.978778
46.100420	1482.994046	18.983795
46.116474	1488.403912	18.988813
45.976909	1477.862688	18.993831
46.170819	1482.960651	18.998848
46.144995	1477.454300	19.003866
46.404178	1474.036725	19.008883
46.008997	1477.421774	19.013901
46.187541	1478.630846	19.018919
45.952039	1477.455764	19.023936
45.786104	1481.612822	19.028954
46.047083	1479.517312	19.033971
46.134074	1491.370003	19.038989
46.194686	1498.704340	19.044007
46.367850	1497.638807	19.049024
46.272679	1503.239682	19.054042
46.168245	1492.746596	19.059059
46.220133	1505.561054	19.064077
46.498998	1521.978788	19.069095
46.991623	1517.353767	19.074112
46.683798	1526.396410	19.079130
46.926115	1522.091486	19.084147
47.008156	1525.890950	19.089165
46.927003	1518.843675	19.094183
47.361566	1522.420640	19.099200
46.963812	1526.888598	19.104218
47.235233	1521.862709	19.109235
47.481279	1523.351557	19.114253
47.222340	1526.516443	19.119271
47.556802	1511.457329	19.124288
47.422594	1516.912838	19.129306
47.045269	1517.707204	19.134323
47.229166	1523.813501	19.139341
47.488540	1519.802566	19.144359
47.392515	1518.990656	19.149376
47.441690	1513.084360	19.154394
47.707790	1512.717513	19.159411
47.551629	1517.841929	19.164429
47.713829	1525.027810	19.169447
48.219633	1534.444781	19.174464
47.719701	1532.544224	19.179482
47.896034	1515.524777	19.184499
47.856088	1517.957883	19.189517
47.776545	1536.969182	19.194535
47.813092	1534.946700	19.199552
47.895320	1537.518465	19.204570
47.921716	1533.146377	19.209587
47.836411	1541.453540	19.214605
47.869341	1540.040726	19.219623
48.265190	1539.625147	19.224640
48.142948	1548.076962	19.229658
48.225258	1542.149685	19.234675
48.324479	1546.426169	19.239693
48.115023	1544.016173	19.244711
48.297289	1542.273833	19.249728
48.377072	1554.866193	19.254746
48.372179	1557.719869	19.259763
48.596686	1560.827953	19.264781
48.481245	1560.804921	19.269799
48.467074	1563.622179	19.274816
48.537870	1567.259302	19.279834
48.765324	1552.292663	19.284851
48.537314	1557.283173	19.289869
48.467933	1560.885450	19.294887
48.905863	1562.864974	19.299904
48.820078	1564.437374	19.304922
48.819894	1571.976937	19.309939
48.960551	1583.142746	19.314957
48.610792	1590.989565	19.319975
48.888408	1582.342781	19.324992
48.753501	1587.912036	19.330010
48.847751	1579.691635	19.335027
49.274296	1595.467728	19.340045
49.261969	1612.546584	19.345063
49.632459	1606.220665	19.350080
49.191285	1602.843363	19.355098
49.546647	1597.495016	19.360115
49.871147	1595.313797	19.365133
49.751383	1600.943803	19.370151
49.904219	1596.943231	19.375168
49.628782	1611.298670	19.380186
49.808029	1593.798983	19.385203
49.945409	1599.552812	19.390221
49.951855	1598.746936	19.395239
50.051123	1588.613221	19.400256
49.940683	1593.332842	19.405274
50.026429	1591.009140	19.410291
50.062550	1596.677841	19.415309
49.877217	1595.813645	19.420327
50.027653	1591.270621	19.425344
50.082412	1595.140650	19.430362
50.154432	1606.377191	19.435379
50.206984	1592.861269	19.440397
49.861483	1607.574840	19.445415
50.198602	1606.445741	19.450432
50.114739	1623.835634	19.455450
50.167411	1620.551379	19.460467
50.520593	1626.833170	19.465485
50.448817	1629.025111	19.470503
50.853213	1611.528003	19.475520
50.501716	1620.066267	19.480538
50.543683	1615.111018	19.485555
51.089492	1621.043874	19.490573
50.915406	1630.166607	19.495591
50.760715	1620.590245	19.500608
51.126091	1640.529238	19.505626
51.314199	1641.212928	19.510643
51.256010	1622.428054	19.515661
51.074288	1625.666071	19.520679
51.051707	1625.426507	19.525696
51.085766	1637.357020	19.530714
51.393109	1642.781259	19.535731
51.552700	1638.950043	19.540749
51.354686	1647.202325	19.545767
51.853972	1641.036107	19.550784
51.707513	1645.341638	19.555802
51.463434	1642.712978	19.560819
51.615312	1638.706234	19.565837
51.280572	1643.861821	19.570855
51.505664	1636.829639	19.575872
51.522336	1638.868859	19.580890
51.492949	1635.783661	19.585907
51.652141	1632.110308	19.590925
51.188191	1644.140943	19.595943
51.595934	1632.134712	19.600960
51.321324	1652.098243	19.605978
51.777152	1661.251696	19.610995
52.045003	1656.115870	19.616013
51.909066	1661.817861	19.621031
51.940569	1665.824100	19.626048
51.993378	1673.809865	19.631066
51.900206	1668.140428	19.636083
52.265202	1679.012358	19.641101
52.392610	1681.416109	19.646119
52.428804	1693.352637	19.651136
52.117941	1694.777265	19.656154
52.516938	1691.931072	19.661171
52.832559	1692.771522	19.666189
52.621481	1685.687729	19.671207
52.805506	1683.427517	19.676224
52.612115	1686.064578	19.681242
52.741183	1687.502335	19.686259
52.602988	1688.742110	19.691277
52.875179	1680.698925	19.696295
53.364601	1686.359753	19.701312
53.362081	1682.329851	19.706330
53.162172	1682.398952	19.711347
53.201535	1682.654641	19.716365
52.950483	1685.846724	19.721383
53.485683	1678.601827	19.726400
53.495183	1680.878876	19.731418
52.925930	1683.805212	19.736435
52.637677	1677.620348	19.741453
53.053001	1698.971778	19.746471
53.044543	1699.765168	19.751488
53.172649	1708.468187	19.756506
53.216969	1711.847541	19.761523
53.594285	1715.181034	19.766541
53.310917	1728.076581	19.771559
53.584681	1730.567869	19.776576
53.897555	1730.708119	19.781594
54.025302	1729.659156	19.786611
53.736881	1728.296675	19.791629
53.719689	1737.581086	19.796647
54.063833	1734.809756	19.801664
54.000598	1728.037320	19.806682
54.004981	1727.512645	19.811699
54.094880	1730.992165	19.816717
54.081014	1733.623198	19.821735
54.363274	1737.075737	19.826752
54.728489	1741.320061	19.831770
54.188012	1746.100787	19.836787
54.449248	1744.797364	19.841805
54.489416	1748.571875	19.846823
54.417023	1754.986666	19.851840
54.676414	1744.123986	19.856858
54.540694	1747.250669	19.861875
54.903749	1743.633721	19.866893
54.814496	1740.169696	19.871911
54.832158	1738.945463	19.876928
54.912266	1745.124905	19.881946
54.879597	1741.762473	19.886963
55.034160	1737.736351	19.891981
54.483583	1743.266631	19.896999
54.630951	1745.506308	19.902016
55.092498	1757.985346	19.907034
55.298355	1763.573855	19.912051
55.432337	1761.384594	19.917069
55.345864	1774.372409	19.922087
55.168580	1776.634550	19.927104
55.342201	1762.701874	19.932122
55.763243	1772.416293	19.937139
55.859868	1767.360914	19.942157
55.617966	1762.074534	19.947175
56.038771	1766.493203	19.952192
55.756521	1766.461589	19.957210
55.667750	1764.597580	19.962227
55.369389	1768.362015	19.967245
55.505354	1770.754969	19.972263
55.489771	1770.410159	19.977280
55.766308	1772.916798	19.982298
55.333200	1765.347018	19.987315
55.584236	1774.400063	19.992333
55.892227	1782.390081	19.997351
55.640578	1786.768935	20.002368
56.201257	1790.133679	20.007386
56.017421	1789.253459	20.012403
56.459948	1786.990605	20.017421
56.223283	1797.518186	20.022439
56.357923	1807.479481	20.027456
56.598599	1806.479096	20.032474
56.424968	1820.026591	20.037491
56.927414	1812.909858	20.042509
56.537226	1809.044813	20.047527
56.553777	1811.112476	20.052544
57.066205	1807.541545	20.057562
56.551325	1813.476536	20.062579
56.885863	1806.417672	20.067597
57.021938	1812.654644	20.072615
57.044841	1803.514294	20.077632
56.866052	1810.065702	20.082650
56.926060	1820.111285	20.087667
57.226631	1830.122339	20.092685
57.071299	1831.863461	20.097703
56.790796	1834.103908	20.102720
57.357667	1833.639436	20.107738
57.010418	1829.597234	20.112755
57.137902	1828.863909	20.117773
57.847835	1841.490295	20.122791
57.683565	1842.939308	20.127808
57.464364	1840.764343	20.132826
57.618284	1845.934952	20.137843
57.881378	1858.022246	20.142861
57.892837	1863.221491	20.147879
57.596209	1857.315608	20.152896
57.880652	1853.846664	20.157914
57.780333	1850.712577	20.162931
58.198620	1858.252973	20.167949
57.823984	1854.909381	20.172967
58.211160	1851.578988	20.177984
58.340436	1857.094311	20.183002
58.188461	1856.606754	20.188019
58.180285	1849.996071	20.193037
58.452053	1860.339882	20.198055
58.587209	1873.760138	20.203072
58.609789	1880.011759	20.208090
58.564376	1876.064278	20.213107
58.836492	1888.491030	20.218125
58.745157	1882.133222	20.223143
59.061558	1879.511394	20.228160
59.014489	1880.370806	20.233178
58.980067	1879.233625	20.238195
59.151805	1873.349036	20.243213
59.203639	1880.722777	20.248231
58.753705	1882.424847	20.253248
59.062473	1871.986730	20.258266
58.839339	1877.459437	20.263283
58.938184	1870.317546	20.268301
59.228000	1869.145346	20.273319
58.900091	1874.075850	20.278336
59.116373	1872.927795	20.283354
59.015443	1871.441247	20.288371
59.399289	1885.248612	20.293389
59.408068	1886.616863	20.298407
59.563355	1889.912588	20.303424
59.453591	1891.346752	20.308442
59.592608	1891.915059	20.313459
59.439108	1887.637346	20.318477
60.054335	1884.302777	20.323495
59.758449	1887.164223	20.328512
59.701876	1889.934523	20.333530
59.754174	1909.632512	20.338547
60.570155	1914.077674	20.343565
60.203540	1914.772541	20.348583
60.181402	1911.080200	20.353600
60.360582	1907.839192	20.358618
60.196430	1914.817566	20.363635
60.590046	1905.884190	20.368653
60.516522	1900.662913	20.373671
60.401244	1906.712065	20.378688
60.454352	1898.289666	20.383706
60.424372	1904.723113	20.388723
60.474962	1906.892760	20.393741
60.718516	1915.962829	20.398759
61.109445	1927.152763	20.403776
60.973189	1914.243735	20.408794
60.636511	1917.471365	20.413811
60.803069	1927.080562	20.418829
61.133243	1931.115811	20.423847
60.833508	1931.626618	20.428864
61.595417	1924.112558	20.433882
61.385551	1933.392541	20.438899
61.215364	1935.341141	20.443917
61.400558	1932.256989	20.448935
61.141333	1935.314685	20.453952
61.169866	1924.746862	20.458970
61.092044	1931.970512	20.463987
61.468054	1948.420758	20.469005
61.222501	1954.910090	20.474023
61.502857	1959.413934	20.479040
61.583380	1954.294748	20.484058
61.595611	1942.135667	20.489075
61.801662	1950.129107	20.494093
61.975312	1962.224172	20.499111
62.077822	1975.327703	20.504128
62.141398	1981.875918	20.509146
61.977696	1982.393818	20.514163
61.894719	1980.263770	20.519181
62.214205	1978.534607	20.524199
62.027326	1979.883023	20.529216
62.340747	1975.753058	20.534234
61.883860	1975.101814	20.539251
62.214448	1980.023859	20.544269
62.701750	1991.684766	20.549287
62.620858	2000.770993	20.554304
62.992635	2008.807928	20.559322
62.722290	2003.753169	20.564339
62.658630	2005.306361	20.569357
62.863041	2007.177343	20.574375
62.576638	2010.728499	20.579392
62.910823	2006.961375	20.584410
63.236558	2022.662115	20.589427
63.341506	2021.058085	20.594445
63.357283	2017.836347	20.599463
63.415388	2027.633016	20.604480
63.482577	2011.352936	20.609498
63.308769	2017.120938	20.614515
63.095244	2021.531748	20.619533
63.326352	2017.458855	20.624551
63.602450	2023.430947	20.629568
63.667115	2022.458128	20.634586
63.852470	2023.117016	20.639603
63.973939	2015.188821	20.644621
63.893512	2024.628467	20.649639
63.628471	2023.281236	20.654656
63.890644	2016.069513	20.659674
64.155962	2023.940083	20.664691
63.887365	2013.889011	20.669709
64.108968	2018.780801	20.674727
63.904170	2026.469387	20.679744
64.431875	2030.214914	20.684762
64.491968	2043.517660	20.689779
64.571576	2059.894517	20.694797
64.522866	2048.429777	20.699815
64.622241	2054.341197	20.704832
64.512402	2039.247103	20.709850
64.531637	2047.490780	20.714867
64.653312	2057.318534	20.719885
65.038910	2044.561200	20.724903
64.750530	2045.007110	20.729920
65.135081	2048.449996	20.734938
65.218071	2046.095106	20.739955
64.858108	2039.665711	20.744973
65.321245	2045.381270	20.749991
65.017390	2050.914017	20.755008
65.037083	2045.204684	20.760026
64.969178	2059.307042	20.765043
65.127524	2056.706796	20.770061
65.062053	2061.451055	20.775079
65.334622	2066.366434	20.780096
65.498655	2066.498446	20.785114
65.503627	2061.375286	20.790131
65.553944	2074.995193	20.795149
65.931959	2085.101563	20.800167
65.475983	2090.733901	20.805184
65.896682	2090.065089	20.810202
65.795368	2088.269288	20.815219
65.951178	2086.041852	20.820237
66.175912	2085.959210	20.825255
65.792306	2092.615399	20.830272
65.760555	2089.552585	20.835290
66.032564	2099.435711	20.840307
66.103927	2115.419402	20.845325
66.192573	2116.071354	20.850343
66.361402	2118.796906	20.855360
66.652425	2123.141316	20.860378
66.535088	2110.431172	20.865395
66.349684	2118.653290	20.870413
66.416063	2128.360347	20.875431
66.506146	2138.751720	20.880448
66.613442	2135.875415	20.885466
67.212751	2122.317617	20.890483
67.313705	2137.469801	20.895501
67.392681	2135.235459	20.900519
67.712474	2136.545534	20.905536
67.561040	2126.838991	20.910554
67.567964	2133.415073	20.915571
67.224290	2137.360267	20.920589
67.719683	2126.880140	20.925607
67.278662	2132.516460	20.930624
67.698844	2128.401294	20.935642
67.744802	2129.151460	20.940659
67.633576	2126.233647	20.945677
67.938531	2117.680162	20.950695
67.655268	2138.873301	20.955712
67.571760	2128.821571	20.960730
67.645578	2123.012208	20.965747
67.719957	2138.522036	20.970765
68.082290	2146.232281	20.975783
67.881668	2156.886980	20.980800
67.731333	2149.897636	20.985818
68.403723	2151.556447	20.990835
68.140106	2151.837520	20.995853
68.589960	2145.022412	21.000871
68.099204	2154.371765	21.005888
68.402230	2168.700140	21.010906
68.788798	2172.398377	21.015923
68.380466	2177.840224	21.020941
68.539824	2171.512470	21.025959
68.345754	2171.627999	21.030976
68.395964	2173.706211	21.035994
69.098734	2181.937541	21.041011
68.932353	2191.434925	21.046029
69.341420	2190.963609	21.051047
69.058324	2200.703367	21.056064
69.242321	2195.968724	21.061082
69.455611	2194.202525	21.066099
69.291302	2199.555650	21.071117
69.544009	2198.038918	21.076135
69.207228	2196.740787	21.081152
69.291049	2193.795560	21.086170
69.428718	2193.442511	21.091187
69.740124	2220.296121	21.096205
70.158052	2221.341495	21.101223
70.030635	2223.444387	21.106240
70.122259	2216.006817	21.111258
70.332370	2213.761389	21.116275
70.428326	2220.746471	21.121293
70.239705	2217.654559	21.126311
70.470359	2225.192946	21.131328
70.295722	2232.390856	21.136346
70.677933	2231.134724	21.141363
70.570507	2224.031322	21.146381
70.627267	2221.775202	21.151399
70.547275	2225.208845	21.156416
70.550346	2217.690466	21.161434
70.606043	2210.504703	21.166451
70.677320	2217.260099	21.171469
70.853907	2211.743903	21.176487
70.568340	2210.178947	21.181504
70.824781	2213.809210	21.186522
70.728140	2225.104125	21.191539
70.793549	2239.747521	21.196557
70.870744	2243.216507	21.201575
70.627756	2235.575710	21.206592
70.657594	2250.401430	21.211610
71.235423	2257.172161	21.216627
71.231682	2269.904353	21.221645
71.482669	2259.007963	21.226663
71.426324	2260.673651	21.231680
71.206402	2269.952226	21.236698
71.758746	2276.827952	21.241715
71.614627	2282.408333	21.246733
71.638973	2288.767128	21.251751
71.546197	2288.699514	21.256768
71.528823	2289.582697	21.261786
72.290583	2303.182840	21.266803
72.167617	2303.647025	21.271821
72.524649	2303.808768	21.276839
72.362746	2311.184612	21.281856
72.714683	2304.438439	21.286874
72.725598	2307.094078	21.291891
72.656801	2310.365022	21.296909
72.495067	2300.944048	21.301927
72.329154	2304.157617	21.306944
72.594190	2312.830009	21.311962
72.821322	2301.343983	21.316979
73.039810	2302.228087	21.321997
72.502389	2297.158278	21.327015
72.954472	2300.013066	21.332032
72.849135	2311.814374	21.337050
73.471747	2322.438031	21.342067
73.237074	2330.222954	21.347085
73.460056	2335.584875	21.352103
73.785116	2323.603763	21.357120
73.491881	2332.663461	21.362138
73.765738	2321.346844	21.367155
73.675700	2324.564309	21.372173
73.917029	2320.379283	21.377191
73.587355	2322.804235	21.382208
73.390586	2327.881590	21.387226
73.848879	2324.517876	21.392243
73.778153	2318.822623	21.397261
73.496505	2330.569507	21.402279
73.917575	2344.371395	21.407296
74.263340	2351.257423	21.412314
74.340281	2345.617929	21.417331
73.980975	2354.725863	21.422349
74.309266	2347.610957	21.427367
74.577512	2357.138174	21.432384
74.607727	2370.354315	21.437402
74.850766	2363.394785	21.442419
74.723323	2370.670570	21.447437
74.816811	2368.702197	21.452455
75.036303	2367.370554	21.457472
74.645336	2369.047647	21.462490
75.104993	2360.826451	21.467507
74.934503	2369.128406	21.472525
75.001949	2358.967681	21.477543
75.239990	2370.339652	21.482560
75.068068	2387.703051	21.487578
75.332578	2381.832168	21.492595
75.390141	2389.088444	21.497613
75.440461	2384.538813	21.502631
75.384643	2380.659130	21.507648
75.288443	2391.281826	21.512666
75.550781	2394.885953	21.517683
75.514396	2409.636963	21.522701
75.612765	2415.435040	21.527719
75.761671	2411.854668	21.532736
75.502987	2423.623264	21.537754
75.987786	2432.450651	21.542771
75.877372	2432.815033	21.547789
75.903902	2435.020074	21.552807
76.274162	2444.222055	21.557824
76.323419	2453.127157	21.562842
77.060318	2458.777866	21.567859
76.918677	2465.380502	21.572877
77.040631	2463.123606	21.577895
77.120753	2452.834598	21.582912
77.022774	2447.563339	21.587930
76.856617	2441.425360	21.592947
77.181035	2460.020859	21.597965
77.331497	2453.546063	21.602983
77.541232	2451.641527	21.608000
77.485756	2461.396261	21.613018
77.564053	2441.932670	21.618035
77.342401	2446.963458	21.623053
77.115648	2442.103737	21.628071
77.087566	2450.295045	21.633088
77.346331	2445.233010	21.638106
77.349121	2437.421064	21.643123
77.011638	2452.673765	21.648141
77.611018	2465.759775	21.653159
77.736977	2470.029135	21.658176
77.703613	2480.660976	21.663194
77.849470	2478.479237	21.668211
78.016047	2479.958524	21.673229
78.080410	2487.721913	21.678247
78.479360	2492.560798	21.683264
78.200556	2497.111353	21.688282
78.368402	2501.610868	21.693299
78.445604	2505.925749	21.698317
78.676565	2500.688155	21.703335
78.809396	2506.818569	21.708352
78.542693	2509.394644	21.713370
78.891862	2498.160801	21.718387
78.614559	2497.999007	21.723405
78.943778	2514.693815	21.728423
78.928866	2518.773796	21.733440
78.736546	2526.056652	21.738458
78.909415	2519.013372	21.743475
79.095307	2520.552759	21.748493
79.451425	2543.729255	21.753511
79.386193	2538.796859	21.758528
79.502985	2549.219003	21.763546
79.633538	2543.447958	21.768563
79.979412	2548.853813	21.773581
80.007742	2550.881842	21.778599
80.107820	2550.058098	21.783616
80.054703	2549.110016	21.788634
80.328001	2537.007471	21.793651
80.128544	2549.581155	21.798669
80.054513	2548.566915	21.803687
80.642679	2544.554740	21.808704
80.145526	2555.732710	21.813722
80.340904	2542.364130	21.818739
80.406846	2559.583119	21.823757
80.338303	2571.959564	21.828775
80.700961	2568.380390	21.833792
80.426015	2576.323222	21.838810
80.619720	2575.920357	21.843827
80.669752	2567.674872	21.848845
80.887672	2594.935052	21.853863
81.208534	2585.176359	21.858880
81.149191	2595.610345	21.863898
81.325962	2587.395493	21.868915
81.527256	2595.326843	21.873933
81.349618	2602.951451	21.878951
81.543310	2581.200355	21.883968
81.511856	2585.873143	21.888986
81.299156	2585.174148	21.894003
81.404893	2609.160057	21.899021
81.519633	2614.283372	21.904039
81.765805	2609.198015	21.909056
81.736038	2622.038687	21.914074
82.014855	2609.376589	21.919091
82.256649	2618.605098	21.924109
81.863562	2642.233653	21.929127
82.213071	2640.165171	21.934144
82.224125	2642.543096	21.939162
82.522375	2640.820354	21.944179
82.349700	2644.072916	21.949197
82.499158	2642.392423	21.954215
82.775922	2643.242165	21.959232
82.697409	2641.142901	21.964250
82.605297	2647.857778	21.969267
82.618393	2655.130597	21.974285
82.702231	2660.927874	21.979303
83.071290	2653.746494	21.984320
82.792006	2660.740037	21.989338
83.194748	2665.710935	21.994355
83.357178	2676.561554	21.999373
83.148573	2678.569908	22.004391
83.267215	2677.175139	22.009408
83.291745	2679.749795	22.014426
83.408069	2684.273209	22.019443
83.878763	2681.166294	22.024461
83.469646	2686.403264	22.029479
83.916189	2695.902727	22.034496
83.826346	2695.086639	22.039514
83.526405	2695.938364	22.044531
84.117697	2700.873419	22.049549
83.986943	2705.568108	22.054567
84.171996	2710.292224	22.059584
84.433139	2720.158458	22.064602
84.619282	2724.841377	22.069619
84.875102	2726.331953	22.074637
84.489976	2720.988823	22.079655
84.985194	2730.401775	22.084672
84.862172	2727.113282	22.089690
84.733662	2721.976129	22.094707
84.953054	2734.547444	22.099725
85.182338	2744.434464	22.104743
85.650997	2743.057444	22.109760
85.351414	2747.889061	22.114778
85.269616	2741.242242	22.119795
85.677649	2748.039763	22.124813
85.285266	2749.511960	22.129831
85.744947	2735.095006	22.134848
85.898022	2753.117980	22.139866
85.701270	2747.445492	22.144883
85.564764	2740.557905	22.149901
85.873162	2762.369221	22.154919
86.427853	2756.301256	22.159936
86.073768	2767.318070	22.164954
86.024506	2763.787613	22.169971
86.263822	2765.583771	22.174989
86.115714	2763.088249	22.180007
86.265654	2762.373462	22.185024
86.573660	2777.275969	22.190042
86.555867	2786.475799	22.195059
86.762020	2789.403915	22.200077
86.498836	2791.332459	22.205095
86.829845	2794.004300	22.210112
86.894400	2787.495500	22.215130
86.628267	2805.154962	22.220147
87.192340	2807.689293	22.225165
86.957977	2815.887836	22.230183
87.516955	2808.092745	22.235200
87.695549	2809.068343	22.240218
87.340852	2809.975994	22.245235
87.306708	2804.208576	22.250253
87.617314	2819.899760	22.255271
87.628133	2832.797347	22.260288
87.772844	2827.150241	22.265306
87.934092	2831.183756	22.270323
88.033723	2834.469438	22.275341
88.197742	2833.600945	22.280359
87.893702	2837.505362	22.285376
88.310318	2847.883862	22.290394
88.224701	2856.567267	22.295411
88.650465	2851.643078	22.300429
88.688724	2859.038285	22.305447
88.881479	2843.021840	22.310464
88.660827	2852.865787	22.315482
88.590944	2849.534229	22.320499
89.058866	2852.639122	22.325517
89.097306	2855.823927	22.330535
88.659214	2851.227608	22.335552
89.283081	2856.454286	22.340570
89.620401	2877.080790	22.345587
89.689991	2870.552234	22.350605
89.509056	2872.783520	22.355623
89.733668	2874.926020	22.360640
89.885655	2877.603829	22.365658
89.781530	2878.197636	22.370675
90.294736	2870.687436	22.375693
90.155003	2870.033809	22.380711
90.348069	2871.354325	22.385728
90.496860	2872.943743	22.390746
90.184076	2875.946864	22.395763
90.306664	2873.295292	22.400781
89.841868	2879.989739	22.405799
90.248313	2869.248530	22.410816
90.201543	2879.112593	22.415834
90.148263	2891.524740	22.420851
90.690450	2895.312372	22.425869
90.427583	2903.651137	22.430887
90.634184	2896.286804	22.435904
90.883231	2910.911445	22.440922
91.023166	2926.793584	22.445939
91.281329	2921.690480	22.450957
91.144392	2926.345164	22.455975
91.192887	2929.086538	22.460992
90.936356	2926.888882	22.466010
91.183801	2931.679031	22.471027
91.333730	2942.538081	22.476045
91.313893	2948.556848	22.481063
91.320629	2947.387901	22.486080
92.014525	2956.653065	22.491098
91.739987	2968.449748	22.496115
92.069567	2962.025613	22.501133
92.014212	2978.585419	22.506151
92.233956	2976.789728	22.511168
92.143099	2967.947514	22.516186
92.284258	2970.907936	22.521203
92.611312	2977.446797	22.526221
92.776626	2993.662734	22.531239
93.077969	2998.400270	22.536256
93.042037	2996.420542	22.541274
92.339481	2996.372709	22.546291
92.363394	2986.928603	22.551309
92.499107	3006.340132	22.556327
92.694693	3016.308330	22.561344
92.885498	3009.972201	22.566362
93.162770	3023.090146	22.571379
93.154152	3029.971989	22.576397
93.284398	3040.010405	22.581415
93.557648	3041.722370	22.586432
94.163525	3034.437457	22.591450
94.008605	3041.064477	22.596467
93.977243	3035.290236	22.601485
93.961872	3036.012174	22.606503
93.928933	3051.347073	22.611520
94.546163	3055.347074	22.616538
94.193255	3053.720000	22.621555
94.521151	3057.727457	22.626573
94.579972	3054.997475	22.631591
94.285508	3054.693175	22.636608
94.754861	3056.248168	22.641626
94.793641	3061.320386	22.646643
94.802946	3052.664437	22.651661
95.034678	3048.060968	22.656679
95.139883	3064.576760	22.661696
95.583491	3070.595553	22.666714
95.201963	3076.611060	22.671731
95.621681	3077.182772	22.676749
95.538071	3081.418829	22.681767
95.683985	3085.776741	22.686784
95.647501	3079.984351	22.691802
95.261665	3084.141509	22.696819
95.606481	3074.192582	22.701837
95.603160	3080.312961	22.706855
96.119240	3090.814893	22.711872
96.225372	3098.209033	22.716890
95.632757	3105.273930	22.721907
96.125605	3100.247634	22.726925
95.864989	3106.847049	22.731943
95.803426	3109.741412	22.736960
96.056416	3127.184138	22.741978
96.082686	3130.342492	22.746995
96.435948	3132.578493	22.752013
96.834915	3155.632283	22.757031
96.512507	3163.538620	22.762048
97.094584	3166.250090	22.767066
96.880930	3167.852131	22.772083
96.942557	3170.200108	22.777101
97.230965	3181.365858	22.782119
97.372310	3187.810796	22.787136
97.514699	3186.396487	22.792154
97.224325	3181.110968	22.797171
97.916625	3187.624245	22.802189
98.433579	3200.237642	22.807207
98.434350	3209.718842	22.812224
98.511615	3184.424996	22.817242
98.459771	3176.858008	22.822259
98.283081	3184.905651	22.827277
98.078742	3188.182208	22.832295
98.040386	3197.890470	22.837312
98.385354	3198.549647	22.842330
98.439722	3213.492254	22.847347
98.903687	3202.328366	22.852365
99.020592	3205.283159	22.857383
98.802955	3209.928464	22.862400
99.161305	3216.320478	22.867418
99.202897	3218.977758	22.872435
99.233933	3221.797661	22.877453
99.397837	3216.690305	22.882471
99.497539	3215.358432	22.887488
99.651607	3211.111122	22.892506
99.387921	3219.137690	22.897523
99.835589	3216.416201	22.902541
99.959702	3234.882915	22.907559
99.767035	3239.183439	22.912576
100.132799	3237.803568	22.917594
100.036966	3245.532411	22.922611
100.041712	3245.351669	22.927629
100.082680	3246.692887	22.932647
100.139574	3255.729753	22.937664
100.440110	3267.875257	22.942682
100.845406	3270.166248	22.947699
100.683281	3267.464537	22.952717
100.479724	3266.391641	22.957735
100.325924	3276.755600	22.962752
100.598615	3280.673911	22.967770
100.385800	3295.125034	22.972787
100.915021	3289.846798	22.977805
101.211244	3302.283378	22.982823
101.980121	3306.597400	22.987840
101.897892	3312.768095	22.992858
101.929898	3317.282785	22.997875
101.589584	3322.506001	23.002893
101.595967	3323.114072	23.007911
101.550237	3310.799021	23.012928
102.231944	3309.458022	23.017946
101.796166	3317.060247	23.022963
102.326163	3313.015989	23.027981
102.210156	3321.969507	23.032999
102.211029	3337.444540	23.038016
102.370524	3337.097519	23.043034
102.284821	3341.665376	23.048051
102.482894	3337.701521	23.053069
102.768123	3338.568909	23.058087
102.522385	3362.639292	23.063104
103.045179	3362.102790	23.068122
103.086953	3366.963154	23.073139
103.122621	3361.803253	23.078157
103.352917	3363.727137	23.083175
103.013990	3365.102631	23.088192
103.556728	3374.063440	23.093210
103.559532	3381.827389	23.098227
103.527925	3384.878073	23.103245
103.690507	3384.558975	23.108263
103.714872	3385.972243	23.113280
104.199880	3401.582953	23.118298
104.067973	3412.192906	23.123315
104.190586	3414.638675	23.128333
104.427082	3410.151151	23.133351
104.439707	3410.246927	23.138368
104.534957	3407.561685	23.143386
104.798718	3418.450533	23.148403
104.653545	3424.593252	23.153421
104.728286	3431.073963	23.158439
104.536850	3436.961961	23.163456
104.600455	3439.849391	23.168474
105.222071	3448.829443	23.173491
105.223297	3459.323876	23.178509
105.472043	3456.848146	23.183527
105.621685	3466.164123	23.188544
105.428830	3457.789000	23.193562
105.863326	3466.047176	23.198579
105.883316	3473.003613	23.203597
106.353205	3475.467578	23.208615
105.882763	3481.190985	23.213632
105.912836	3486.794947	23.218650
106.391793	3481.811755	23.223667
105.873019	3484.149701	23.228685
106.413840	3489.692584	23.233703
106.401022	3503.474964	23.238720
106.846499	3497.900470	23.243738
106.900305	3503.497562	23.248755
106.888640	3513.479567	23.253773
107.076911	3500.269209	23.258791
106.762305	3512.205088	23.263808
107.064037	3516.421909	23.268826
107.426109	3527.800431	23.273843
107.362023	3529.962990	23.278861
107.947790	3517.024914	23.283879
107.592760	3532.631624	23.288896
107.661662	3526.421728	23.293914
107.424350	3539.399726	23.298931
108.030118	3546.318076	23.303949
108.158735	3554.933533	23.308967
107.868520	3562.765561	23.313984
107.874072	3554.132054	23.319002
108.215420	3554.157392	23.324019
108.020248	3575.849738	23.329037
108.289741	3568.443716	23.334055
108.408058	3580.769483	23.339072
108.751056	3595.241081	23.344090
108.927522	3596.665256	23.349107
108.977951	3608.591354	23.354125
109.164413	3603.704455	23.359143
109.190350	3604.328410	23.364160
109.060572	3608.533948	23.369178
109.464734	3595.813648	23.374195
109.556415	3616.091253	23.379213
109.705251	3617.620760	23.384231
109.486280	3625.766756	23.389248
109.586771	3622.866031	23.394266
109.644800	3631.776654	23.399283
110.073665	3642.980655	23.404301
110.219761	3646.571684	23.409319
110.113283	3654.842103	23.414336
110.132492	3650.963017	23.419354
110.388478	3659.031460	23.424371
110.491935	3668.799822	23.429389
110.810815	3667.594551	23.434407
110.576217	3674.496261	23.439424
111.116121	3677.195480	23.444442
111.067566	3667.746590	23.449459
111.224145	3678.592417	23.454477
111.008445	3690.026840	23.459495
110.950544	3697.772028	23.464512
111.273685	3697.238390	23.469530
111.510266	3701.364458	23.474547
111.645869	3708.198713	23.479565
111.638219	3709.935813	23.484583
111.594872	3719.787172	23.489600
111.856044	3739.722727	23.494618
112.126460	3739.459326	23.499635
112.111315	3740.793589	23.504653
112.289860	3734.004613	23.509671
112.577535	3756.947197	23.514688
112.643488	3759.417671	23.519706
112.614940	3767.890566	23.524723
112.674000	3768.540901	23.529741
113.151366	3767.629587	23.534759
112.755978	3777.349906	23.539776
112.812792	3786.768970	23.544794
113.379896	3781.260556	23.549811
113.214694	3789.180412	23.554829
113.503603	3800.677885	23.559847
113.778658	3809.314711	23.564864
113.824527	3810.693079	23.569882
114.141209	3807.480694	23.574899
114.035350	3814.296004	23.579917
114.335517	3805.205893	23.584935
114.388703	3811.406044	23.589952
114.745571	3815.263940	23.594970
114.927800	3828.476271	23.599987
114.915386	3837.388562	23.605005
115.209497	3828.867535	23.610023
115.115470	3828.907426	23.615040
115.038077	3829.244566	23.620058
114.976016	3827.136273	23.625075
114.799091	3836.692986	23.630093
115.003261	3824.622508	23.635111
114.837556	3840.600680	23.640128
115.125060	3851.066272	23.645146
115.404890	3854.005115	23.650163
115.035526	3872.597137	23.655181
115.825136	3877.034307	23.660199
115.974803	3895.084206	23.665216
115.916065	3883.765064	23.670234
116.380446	3880.406427	23.675251
116.187630	3895.445137	23.680269
116.679565	3900.689638	23.685287
116.582501	3906.588254	23.690304
116.594448	3903.123737	23.695322
116.818291	3900.241519	23.700339
116.699049	3903.675317	23.705357
116.678368	3911.165410	23.710375
117.136899	3928.917599	23.715392
117.252992	3931.806354	23.720410
117.382442	3935.349546	23.725427
117.258531	3936.789243	23.730445
117.395044	3931.550253	23.735463
117.587671	3941.074375	23.740480
117.836603	3958.354408	23.745498
118.002620	3960.812390	23.750515
117.733989	3960.933294	23.755533
118.094015	3959.557426	23.760551
118.257569	3974.208948	23.765568
118.247485	3984.235155	23.770586
118.574533	3976.980927	23.775603
118.561140	3971.819070	23.780621
118.783544	3975.240389	23.785639
118.731434	3997.696768	23.790656
119.067547	4004.597570	23.795674
119.194195	4001.345483	23.800691
119.428964	4008.473643	23.805709
119.299543	4000.621762	23.810727
119.230136	4010.423703	23.815744
119.635045	4025.542479	23.820762
120.080209	4027.710537	23.825779
119.794541	4038.597457	23.830797
119.942546	4034.322498	23.835815
119.737245	4036.911261	23.840832
120.115965	4043.691773	23.845850
120.273331	4055.544596	23.850867
119.969142	4063.066543	23.855885
120.436296	4063.801306	23.860903
120.527440	4071.911542	23.865920
121.074957	4084.243007	23.870938
120.760198	4082.328938	23.875955
120.547624	4079.792828	23.880973
120.877959	4092.698072	23.885991
121.187461	4116.483612	23.891008
120.950337	4118.575500	23.896026
121.522645	4108.909167	23.901043
121.472750	4128.003773	23.906061
121.840517	4125.054782	23.911079
121.937362	4131.813203	23.916096
121.952607	4132.015891	23.921114
122.243486	4135.966262	23.926131
122.107712	4144.879092	23.931149
122.531490	4153.486470	23.936167
122.796974	4165.041504	23.941184
122.354934	4172.244198	23.946202
122.655748	4155.685698	23.951219
122.717405	4162.051932	23.956237
123.106110	4178.808406	23.961255
123.278216	4180.425852	23.966272
123.111044	4190.558850	23.971290
123.475338	4183.873176	23.976307
123.545828	4184.120869	23.981325
123.722434	4188.499491	23.986343
123.878659	4203.922517	23.991360
124.074815	4206.189581	23.996378
124.159560	4209.569383	24.001395
124.421482	4208.584482	24.006413
124.117554	4205.308279	24.011431
124.372915	4206.754863	24.016448
124.506109	4205.597587	24.021466
124.769844	4197.567239	24.026483
124.654770	4205.482578	24.031501
124.667029	4216.790082	24.036519
124.714468	4216.744682	24.041536
124.780573	4228.327837	24.046554
125.104770	4221.667370	24.051571
125.014346	4239.720505	24.056589
125.221728	4252.462051	24.061607
125.505180	4252.250261	24.066624
125.248871	4261.488207	24.071642
125.605640	4272.211490	24.076659
125.498280	4284.582561	24.081677
125.600308	4283.543795	24.086695
125.891909	4307.442866	24.091712
125.889379	4315.829872	24.096730
126.153243	4306.688383	24.101747
126.153159	4328.357376	24.106765
126.379272	4343.406579	24.111783
126.609020	4339.642714	24.116800
126.767613	4349.052438	24.121818
127.234140	4362.836129	24.126835
127.267516	4369.109017	24.131853
127.348835	4361.384943	24.136871
127.584027	4362.342292	24.141888
127.568625	4380.011350	24.146906
127.932564	4369.563156	24.151923
128.437497	4386.074347	24.156941
128.124919	4387.897161	24.161959
128.341686	4376.105270	24.166976
128.466983	4384.974160	24.171994
128.560363	4374.937657	24.177011
128.498732	4371.105803	24.182029
128.587629	4388.206148	24.187047
129.355885	4400.402240	24.192064
128.887587	4404.714656	24.197082
128.906653	4415.664536	24.202099
128.732707	4398.283756	24.207117
128.907056	4414.029238	24.212135
129.549227	4434.230984	24.217152
129.295616	4439.343083	24.222170
129.622235	4424.434291	24.227187
130.052256	4445.177479	24.232205
130.016776	4450.833043	24.237223
130.084998	4457.116284	24.242240
129.881270	4461.027425	24.247258
130.289443	4452.986961	24.252275
130.200886	4462.811085	24.257293
130.315826	4469.093325	24.262311
130.654490	4466.871673	24.267328
130.648596	4482.841155	24.272346
130.959876	4494.979488	24.277363
130.926360	4499.059673	24.282381
131.106092	4502.118469	24.287399
131.228646	4502.152838	24.292416
131.369034	4521.682051	24.297434
131.541781	4521.392907	24.302451
131.813821	4528.843709	24.307469
131.672945	4524.213019	24.312487
131.997383	4521.797887	24.317504
131.642498	4543.440652	24.322522
132.241534	4547.516443	24.327539
132.395806	4559.805678	24.332557
132.290796	4573.240316	24.337575
132.597305	4575.041915	24.342592
132.369793	4575.629855	24.347610
132.804949	4571.789572	24.352627
133.214640	4590.446508	24.357645
133.310738	4603.414065	24.362663
133.235212	4604.918833	24.367680
133.232150	4607.955781	24.372698
133.507493	4601.321769	24.377715
133.451505	4611.216626	24.382733
133.460387	4619.444159	24.387751
134.029023	4623.395314	24.392768
134.006717	4630.283065	24.397786
133.935758	4627.784665	24.402803
134.149908	4640.055104	24.407821
134.242961	4648.850261	24.412839
134.519109	4656.644532	24.417856
134.652818	4663.880323	24.422874
134.845636	4675.623832	24.427891
135.229905	4677.356442	24.432909
134.800433	4681.388222	24.437927
135.177630	4682.509575	24.442944
135.203199	4697.773569	24.447962
135.649920	4697.116379	24.452979
135.916772	4698.703247	24.457997
135.486151	4710.803285	24.463015
135.971993	4705.670329	24.468032
136.120764	4728.111921	24.473050
136.093357	4710.777328	24.478067
136.435728	4724.255623	24.483085
136.394319	4749.463745	24.488103
136.743114	4749.238557	24.493120
136.820698	4746.211825	24.498138
137.033627	4749.596898	24.503155
137.382942	4757.957395	24.508173
137.333962	4768.586712	24.513191
137.838102	4761.506448	24.518208
137.518460	4775.716646	24.523226
137.361878	4770.416012	24.528243
137.524470	4779.329756	24.533261
137.783861	4791.997246	24.538279
137.923003	4788.799879	24.543296
138.097869	4800.533656	24.548314
138.123165	4812.496048	24.553331
138.485418	4819.358346	24.558349
138.345590	4832.719717	24.563367
138.853232	4832.539087	24.568384
138.641288	4833.405528	24.573402
138.908899	4842.678479	24.578419
139.020273	4852.468334	24.583437
138.919427	4859.280093	24.588455
139.411756	4863.855627	24.593472
139.562767	4865.145003	24.598490
139.821641	4869.229968	24.603507
140.059798	4875.193171	24.608525
140.029447	4896.460387	24.613543
140.312444	4901.479077	24.618560
140.133483	4904.155375	24.623578
140.024132	4905.311932	24.628595
140.417086	4915.565914	24.633613
140.320179	4934.169994	24.638631
140.685489	4935.353201	24.643648
140.880697	4942.759392	24.648666
141.149614	4949.639518	24.653683
141.172768	4952.631381	24.658701
141.169035	4958.720891	24.663719
141.383546	4969.643642	24.668736
141.704905	4980.047765	24.673754
141.722801	4967.895233	24.678771
142.036745	4977.094707	24.683789
141.980808	4993.725886	24.688807
142.151628	4998.380232	24.693824
142.039082	5000.578966	24.698842
142.307330	4998.109444	24.703859
142.621189	5007.908696	24.708877
142.817503	5022.514897	24.713895
142.745270	5008.659279	24.718912
143.132281	5021.190143	24.723930
143.465788	5020.774796	24.728947
143.729789	5028.088174	24.733965
143.186906	5043.372068	24.738983
143.752033	5050.338404	24.744000
143.723175	5048.732976	24.749018
143.850238	5054.947231	24.754035
144.051594	5064.388505	24.759053
143.804878	5077.056568	24.764071
143.997233	5074.138065	24.769088
144.276176	5081.502785	24.774106
144.462409	5098.313925	24.779123
144.661691	5103.137451	24.784141
144.662067	5116.619111	24.789159
144.995391	5118.713285	24.794176
145.149023	5135.725275	24.799194
145.165366	5137.799665	24.804211
145.364567	5151.553236	24.809229
145.585461	5168.750429	24.814247
145.594224	5158.401622	24.819264
146.082332	5167.390824	24.824282
145.989483	5184.930749	24.829299
146.133477	5175.675028	24.834317
146.403385	5191.279948	24.839335
146.630401	5194.738656	24.844352
146.905108	5204.597811	24.849370
146.912577	5201.540952	24.854387
146.980720	5200.510600	24.859405
146.972589	5204.492267	24.864423
147.454095	5210.442711	24.869440
147.923626	5223.453217	24.874458
147.404777	5233.196806	24.879475
147.752056	5230.484439	24.884493
147.652809	5249.913084	24.889511
147.761895	5243.762596	24.894528
147.958625	5253.911776	24.899546
147.909132	5264.494112	24.904563
148.405583	5271.351341	24.909581
148.260351	5272.412531	24.914599
148.726450	5289.726098	24.919616
149.295403	5299.125688	24.924634
149.187559	5299.395022	24.929651
149.537610	5301.196187	24.934669
149.413637	5306.566001	24.939687
149.675984	5322.121712	24.944704
149.720536	5330.643857	24.949722
149.767178	5328.357371	24.954739
149.972627	5323.852148	24.959757
150.182171	5344.302615	24.964775
150.214430	5346.191450	24.969792
150.411562	5344.209676	24.974810
150.360789	5353.501202	24.979827
150.641795	5364.457965	24.984845
150.709354	5377.430544	24.989863
150.930040	5379.233044	24.994880
151.304530	5385.620144	24.999898
151.234049	5397.762070	25.004915
151.402086	5392.817604	25.009933
151.301983	5408.180796	25.014951
151.754914	5416.563244	25.019968
151.811477	5419.881398	25.024986
152.142223	5426.729922	25.030003
152.188848	5430.466312	25.035021
151.887708	5429.648476	25.040039
152.265629	5440.937334	25.045056
152.591564	5446.934325	25.050074
152.231088	5459.582594	25.055091
152.624577	5466.680150	25.060109
152.595204	5478.503181	25.065127
152.695037	5484.235723	25.070144
153.117920	5506.105011	25.075162
153.071064	5507.775821	25.080179
152.916784	5522.437348	25.085197
153.395309	5534.594369	25.090215
153.506425	5542.351742	25.095232
153.879621	5551.766348	25.100250
154.276626	5567.875687	25.105267
154.857062	5579.360184	25.110285
154.399394	5587.519194	25.115303
154.533279	5575.187097	25.120320
155.026740	5588.913838	25.125338
154.991893	5604.200681	25.130355
155.635953	5602.843332	25.135373
155.589492	5609.495329	25.140391
155.515251	5607.985349	25.145408
155.638159	5626.375766	25.150426
156.054169	5637.201060	25.155443
156.205213	5626.905458	25.160461
156.139057	5640.015968	25.165479
156.028261	5652.170692	25.170496
156.539352	5650.531129	25.175514
156.500669	5668.785913	25.180531
156.992501	5666.963121	25.185549
157.239524	5680.472847	25.190567
157.520891	5674.049003	25.195584
157.414641	5672.616636	25.200602
157.383027	5682.719754	25.205619
157.787419	5693.265955	25.210637
157.657609	5706.878930	25.215655
158.018062	5699.028488	25.220672
158.376346	5711.981012	25.225690
158.206889	5721.704845	25.230707
158.204931	5732.797705	25.235725
158.365612	5730.600631	25.240743
158.338173	5745.826454	25.245760
158.786244	5753.698434	25.250778
158.945739	5761.145277	25.255795
158.965544	5778.964853	25.260813
158.896099	5786.678013	25.265831
159.510289	5799.754657	25.270848
159.777243	5802.916808	25.275866
159.948617	5801.150520	25.280883
159.908690	5803.928278	25.285901
159.886964	5820.984163	25.290919
160.124251	5834.085155	25.295936
160.231330	5839.873495	25.300954
160.565549	5858.840288	25.305971
160.718294	5860.331495	25.310989
160.507585	5865.093185	25.316007
160.658043	5888.479801	25.321024
161.618183	5891.394475	25.326042
161.670385	5898.308912	25.331059
161.895983	5902.714997	25.336077
161.760839	5916.085895	25.341095
161.903079	5919.128707	25.346112
162.089653	5917.546275	25.351130
162.088906	5928.995774	25.356147
162.560637	5939.607331	25.361165
162.745085	5947.407052	25.366183
162.470545	5938.263866	25.371200
162.919933	5942.881126	25.376218
162.728569	5960.058419	25.381235
163.442498	5965.925349	25.386253
163.282302	5969.735287	25.391271
163.286974	5976.335212	25.396288
163.709985	5991.156057	25.401306
163.515215	5990.122656	25.406323
163.912956	5994.965837	25.411341
163.742519	6014.766315	25.416359
164.072210	6014.572520	25.421376
164.657549	6024.866437	25.426394
164.866159	6036.740934	25.431411
164.731432	6039.221061	25.436429
164.795221	6049.479899	25.441447
164.796677	6066.147256	25.446464
165.122155	6061.553600	25.451482
165.019696	6077.552231	25.456499
165.371051	6085.357431	25.461517
165.411912	6093.785807	25.466535
165.742258	6097.847226	25.471552
166.422790	6110.869507	25.476570
166.202171	6115.980059	25.481587
166.453691	6131.424513	25.486605
166.450662	6136.747210	25.491623
166.481411	6148.078268	25.496640
166.934442	6157.404919	25.501658
167.007029	6167.176301	25.506675
167.144603	6163.521209	25.511693
167.672234	6193.872952	25.516711
167.889801	6191.048184	25.521728
167.907470	6196.462359	25.526746
168.021936	6206.732287	25.531763
168.264841	6210.971583	25.536781
168.248548	6217.161341	25.541799
168.700933	6222.226467	25.546816
168.929240	6217.171322	25.551834
169.176133	6239.097470	25.556851
169.642248	6237.878443	25.561869
169.737343	6239.419751	25.566887
169.369298	6248.751964	25.571904
169.940239	6238.901637	25.576922
169.500438	6241.622148	25.581939
170.058686	6257.372216	25.586957
169.973626	6275.565421	25.591975
169.646936	6283.448518	25.596992
170.320154	6287.604634	25.602010
170.214857	6305.636885	25.607027
170.489035	6315.768209	25.612045
170.682565	6320.390925	25.617063
170.945490	6331.644685	25.622080
171.063674	6346.245244	25.627098
170.931930	6345.318750	25.632115
171.549168	6360.504068	25.637133
171.690935	6372.635486	25.642151
171.851187	6386.077251	25.647168
172.155957	6385.069743	25.652186
172.325611	6400.025315	25.657203
172.184154	6407.828937	25.662221
172.511602	6410.868072	25.667239
172.662372	6424.241900	25.672256
172.907549	6430.150849	25.677274
173.150710	6445.865207	25.682292
173.400323	6458.727954	25.687309
173.879834	6455.761091	25.692327
173.668156	6459.010966	25.697344
174.034290	6469.797217	25.702362
174.027383	6477.743945	25.707380
174.273305	6484.517766	25.712397
174.621341	6484.027509	25.717415
174.743103	6487.199898	25.722432
174.921429	6477.543539	25.727450
175.015796	6488.031438	25.732468
175.132808	6510.114002	25.737485
175.613717	6507.781435	25.742503
175.477049	6500.441018	25.747520
175.663411	6499.736169	25.752538
175.713736	6522.387955	25.757556
175.554733	6527.855161	25.762573
176.084180	6532.810440	25.767591
175.905161	6548.366890	25.772608
176.298251	6551.657783	25.777626
176.257685	6562.337332	25.782644
176.343440	6586.843028	25.787661
176.768523	6592.446043	25.792679
177.021109	6612.202991	25.797696
177.298324	6612.004786	25.802714
177.194659	6615.645001	25.807732
177.397354	6637.026101	25.812749
177.733950	6639.110471	25.817767
177.809484	6647.700983	25.822784
177.831715	6651.905502	25.827802
178.324768	6675.769804	25.832820
178.380973	6684.953696	25.837837
178.670538	6689.997108	25.842855
178.934436	6698.472900	25.847872
179.342198	6705.151998	25.852890
179.121014	6723.553226	25.857908
179.400511	6725.851747	25.862925
179.530930	6726.045892	25.867943
179.695475	6742.678843	25.872960
179.864882	6742.529095	25.877978
180.161513	6763.387369	25.882996
180.300301	6779.992820	25.888013
180.339020	6780.734844	25.893031
180.570595	6790.128081	25.898048
180.792362	6796.470152	25.903066
180.825331	6803.151177	25.908084
181.268002	6821.505328	25.913101
181.756582	6826.530228	25.918119
181.668199	6833.609102	25.923136
181.788702	6846.151403	25.928154
181.836703	6861.265313	25.933172
181.814211	6860.602640	25.938189
182.473286	6876.877276	25.943207
182.623378	6884.780644	25.948224
182.448066	6881.149171	25.953242
182.714920	6899.549885	25.958260
182.808120	6903.610753	25.963277
183.003224	6909.174129	25.968295
183.356993	6923.555140	25.973312
183.848306	6928.472306	25.978330
183.966899	6943.556283	25.983348
183.947898	6952.805757	25.988365
184.393354	6942.933676	25.993383
184.496465	6971.872624	25.998400
184.848022	6972.290995	26.003418
184.500999	6974.807662	26.008436
184.647576	6985.038269	26.013453
184.904601	6994.872749	26.018471
185.236731	7012.332058	26.023488
185.211302	7016.686188	26.028506
185.583396	7024.794763	26.033524
185.869689	7030.845841	26.038541
186.053306	7041.638923	26.043559
185.764015	7063.425914	26.048576
186.330255	7068.637602	26.053594
186.485621	7089.310019	26.058612
186.762914	7079.145360	26.063629
186.623942	7077.253939	26.068647
186.960570	7102.617589	26.073664
186.994212	7108.597780	26.078682
187.313661	7119.559045	26.083700
187.467890	7137.804009	26.088717
187.441279	7139.175043	26.093735
187.329207	7151.065774	26.098752
187.993879	7162.601214	26.103770
187.955659	7176.497681	26.108788
188.098897	7197.260514	26.113805
188.751326	7202.704981	26.118823
188.815657	7224.515687	26.123840
188.822511	7228.893222	26.128858
189.547011	7239.911069	26.133876
189.611847	7250.448226	26.138893
190.515143	7245.009245	26.143911
190.077124	7253.052258	26.148928
190.199196	7258.832384	26.153946
190.212458	7270.713028	26.158964
190.578587	7274.731222	26.163981
190.944316	7291.314210	26.168999
190.566457	7297.734607	26.174016
190.911710	7304.581566	26.179034
191.427385	7315.565877	26.184052
191.044689	7342.567364	26.189069
191.596079	7335.163020	26.194087
191.480701	7348.528704	26.199104
191.944843	7356.285209	26.204122
191.856401	7363.900982	26.209140
191.786698	7382.800038	26.214157
192.185082	7390.756279	26.219175
192.382458	7417.247122	26.224192
192.865567	7429.208956	26.229210
193.192544	7443.742951	26.234228
193.436093	7456.383201	26.239245
193.599897	7458.696783	26.244263
193.954445	7464.715213	26.249280
193.869824	7473.669000	26.254298
194.447643	7477.802455	26.259316
194.223182	7492.883798	26.264333
194.757263	7494.024956	26.269351
194.680561	7511.094178	26.274368
195.050116	7519.613781	26.279386
195.403111	7530.241707	26.284404
195.296261	7538.523408	26.289421
195.272332	7549.286162	26.294439
195.852090	7562.811448	26.299456
195.980067	7566.200885	26.304474
196.099383	7572.155177	26.309492
196.057437	7595.851925	26.314509
196.378574	7594.914402	26.319527
196.709392	7615.894569	26.324544
197.259180	7622.851671	26.329562
197.441433	7629.550651	26.334580
197.256649	7639.704095	26.339597
197.270554	7650.726171	26.344615
197.599596	7656.653949	26.349632
197.437191	7673.380002	26.354650
197.991407	7672.339664	26.359668
198.069750	7691.585216	26.364685
198.605774	7701.695229	26.369703
198.722524	7721.768254	26.374720
198.948455	7734.796614	26.379738
198.938479	7725.137532	26.384756
199.286011	7751.627432	26.389773
199.464122	7758.488117	26.394791
199.750977	7760.248920	26.399808
199.992804	7769.719978	26.404826
199.836865	7782.707170	26.409844
200.086353	7778.781663	26.414861
200.356600	7787.882061	26.419879
200.476675	7790.183593	26.424896
200.930959	7800.379078	26.429914
201.035055	7810.897777	26.434932
201.079052	7838.309858	26.439949
201.684313	7830.808482	26.444967
201.677415	7854.137009	26.449984
201.677908	7860.327845	26.455002
202.050711	7869.437474	26.460020
202.328860	7883.913167	26.465037
202.499500	7886.686666	26.470055
202.475084	7894.999811	26.475072
202.770038	7913.510790	26.480090
203.270557	7915.945321	26.485108
203.349987	7925.536613	26.490125
203.303636	7943.712770	26.495143
203.018770	7954.030447	26.500160
203.586379	7973.079676	26.505178
203.686616	7988.539920	26.510196
203.912759	8004.580300	26.515213
204.214596	8011.039688	26.520231
204.106740	8029.238193	26.525248
204.560479	8045.887001	26.530266
205.174691	8059.220987	26.535284
205.056215	8065.932509	26.540301
205.100782	8073.597193	26.545319
205.540606	8090.917528	26.550336
205.893602	8103.294822	26.555354
206.266999	8108.881145	26.560372
206.296194	8139.803539	26.565389
206.274021	8146.196920	26.570407
206.765764	8149.305323	26.575424
207.039428	8169.130097	26.580442
207.486687	8170.303844	26.585460
207.354110	8186.605791	26.590477
207.383686	8181.047691	26.595495
207.659675	8193.228739	26.600512
207.825524	8216.287562	26.605530
208.089316	8222.705628	26.610548
208.271109	8240.401181	26.615565
208.578380	8252.905710	26.620583
208.848846	8269.504503	26.625600
208.710524	8275.477283	26.630618
209.619409	8285.996462	26.635636
209.494156	8298.341466	26.640653
209.831809	8296.716223	26.645671
210.071019	8321.073897	26.650688
210.041286	8325.261681	26.655706
210.309054	8330.577318	26.660724
210.808061	8351.904517	26.665741
210.983335	8346.923401	26.670759
211.040705	8355.722770	26.675776
211.043362	8377.266669	26.680794
211.400651	8383.218672	26.685812
211.424630	8393.560824	26.690829
211.887025	8405.340266	26.695847
211.902813	8433.348036	26.700864
212.386332	8449.083280	26.705882
212.407400	8448.565271	26.710900
212.460340	8461.090840	26.715917
212.465648	8472.840901	26.720935
213.072987	8489.920681	26.725952
213.132760	8516.374671	26.730970
213.498536	8513.488447	26.735988
213.648365	8522.181853	26.741005
213.884449	8526.492213	26.746023
214.200090	8529.975559	26.751040
214.196234	8550.857673	26.756058
214.467422	8552.980926	26.761076
214.590371	8566.666915	26.766093
214.637500	8567.502410	26.771111
214.909214	8583.548782	26.776128
215.115993	8604.120125	26.781146
215.470592	8614.183289	26.786164
215.681817	8632.922795	26.791181
215.931291	8649.600991	26.796199
216.238336	8652.744729	26.801216
215.885879	8673.501630	26.806234
216.678354	8679.688646	26.811252
216.679868	8692.825454	26.816269
216.666648	8697.566403	26.821287
217.113864	8712.350925	26.826304
217.088700	8734.777302	26.831322
217.325018	8737.985808	26.836340
217.663837	8762.079038	26.841357
217.580586	8777.256119	26.846375
218.341966	8808.428008	26.851392
218.354410	8814.891970	26.856410
218.992411	8832.503992	26.861428
219.024300	8839.864728	26.866445
219.117805	8851.266546	26.871463
219.556238	8862.664851	26.876480
219.486471	8879.535340	26.881498
220.033570	8887.083749	26.886516
220.119686	8907.917440	26.891533
220.248434	8920.494588	26.896551
220.655610	8925.321286	26.901568
220.790100	8943.312230	26.906586
220.912550	8944.101213	26.911604
221.053187	8969.479187	26.916621
221.345283	8974.301825	26.921639
221.566905	8993.864111	26.926656
221.529878	9005.791633	26.931674
221.987816	9019.261300	26.936692
222.376386	9039.915152	26.941709
222.412618	9065.543251	26.946727
222.704325	9068.152727	26.951744
222.631132	9090.590215	26.956762
222.902206	9103.877679	26.961780
223.492308	9125.336734	26.966797
223.382909	9132.053532	26.971815
223.856693	9146.998419	26.976832
223.911875	9164.247410	26.981850
224.555241	9167.531145	26.986868
224.579594	9185.258578	26.991885
224.527222	9196.001485	26.996903
225.037911	9206.236271	27.001920
225.150942	9233.996374	27.006938
225.544995	9238.777850	27.011956
225.593401	9249.899663	27.016973
225.932504	9271.742354	27.021991
226.690632	9281.253284	27.027008
226.400982	9296.576786	27.032026
226.583752	9300.804117	27.037044
226.759631	9318.814200	27.042061
226.824690	9336.844817	27.047079
227.576778	9335.767084	27.052096
227.268410	9359.005806	27.057114
227.728122	9368.528799	27.062132
227.656054	9385.718997	27.067149
228.035870	9405.721061	27.072167
228.429879	9413.811471	27.077184
228.252704	9432.644202	27.082202
228.750927	9437.242073	27.087220
229.129957	9458.819828	27.092237
229.169270	9469.520113	27.097255
229.933376	9479.506968	27.102272
229.823659	9497.334634	27.107290
230.268155	9496.229302	27.112308
230.390328	9511.062224	27.117325
230.482726	9530.894749	27.122343
230.753531	9525.061656	27.127360
231.022459	9541.807068	27.132378
230.827914	9543.394028	27.137396
231.423724	9573.169174	27.142413
231.307902	9575.823620	27.147431
231.676002	9589.967664	27.152448
231.734366	9605.562108	27.157466
232.106543	9623.961664	27.162484
232.180686	9638.375967	27.167501
232.526070	9663.725971	27.172519
232.700879	9678.752852	27.177536
232.924791	9703.392585	27.182554
233.583013	9711.466995	27.187572
233.525361	9719.931402	27.192589
233.613349	9739.174409	27.197607
234.055268	9745.593517	27.202624
233.973882	9776.494909	27.207642
234.286212	9790.092141	27.212660
234.484382	9795.624334	27.217677
234.432096	9819.666537	27.222695
234.950280	9846.199003	27.227712
235.155011	9866.847842	27.232730
235.297824	9891.961510	27.237748
236.155691	9902.091776	27.242765
236.056726	9924.935295	27.247783
236.371757	9931.854273	27.252800
236.580030	9952.269003	27.257818
237.102909	9973.272271	27.262836
237.710874	9978.137255	27.267853
237.359651	9988.646422	27.272871
237.801879	10002.381332	27.277888
238.238916	10009.814831	27.282906
238.647892	10028.875241	27.287924
238.744257	10028.588515	27.292941
238.470314	10046.477163	27.297959
239.059099	10060.615411	27.302976
239.053186	10084.328631	27.307994
239.305702	10087.073848	27.313012
239.755729	10106.614152	27.318029
240.143318	10124.598163	27.323047
240.144017	10143.217456	27.328064
240.297109	10150.348173	27.333082
240.516578	10164.424371	27.338100
241.208577	10176.667852	27.343117
241.031380	10214.562963	27.348135
241.447539	10210.497171	27.353152
241.567433	10223.913315	27.358170
241.568815	10247.155136	27.363188
241.866500	10262.684222	27.368205
241.931484	10274.460803	27.373223
242.350480	10301.094707	27.378240
242.787174	10312.658366	27.383258
243.048806	10331.840049	27.388276
242.932654	10346.692025	27.393293
243.470046	10354.324651	27.398311
243.651502	10375.975466	27.403328
243.854982	10392.728737	27.408346
244.209384	10413.136867	27.413364
244.190677	10411.949329	27.418381
244.754051	10432.233177	27.423399
244.968285	10442.028832	27.428416
245.381059	10460.369177	27.433434
245.775658	10474.626570	27.438452
246.006118	10484.703881	27.443469
245.572339	10492.352928	27.448487
246.173744	10494.775163	27.453504
246.297817	10506.899433	27.458522
246.289022	10533.809079	27.463540
246.694001	10551.913921	27.468557
247.302607	10560.479576	27.473575
247.077367	10571.648201	27.478592
247.294634	10596.561700	27.483610
247.605949	10619.294432	27.488628
248.056632	10625.797726	27.493645
248.209411	10650.042529	27.498663
248.775776	10659.233725	27.503680
248.663506	10678.082801	27.508698
248.813478	10697.032905	27.513716
249.181814	10716.122486	27.518733
249.275723	10738.302115	27.523751
249.330637	10753.108669	27.528768
249.977514	10765.804822	27.533786
249.991119	10796.907732	27.538804
250.297176	10804.279972	27.543821
250.374369	10828.442119	27.548839
250.644898	10847.821865	27.553856
251.102834	10869.357315	27.558874
251.561274	10892.026282	27.563892
251.750601	10911.643002	27.568909
251.703518	10935.755289	27.573927
252.282319	10948.124369	27.578944
252.434009	10967.279720	27.583962
252.594077	10988.723035	27.588980
253.097478	11000.421921	27.593997
253.102180	11019.594037	27.599015
253.319755	11037.488728	27.604032
253.885143	11060.220086	27.609050
253.778819	11078.724453	27.614068
254.380701	11087.092475	27.619085
254.922086	11115.473471	27.624103
255.199268	11121.132616	27.629120
255.333077	11140.755115	27.634138
255.278476	11160.647129	27.639156
255.739779	11172.690584	27.644173
255.939902	11188.267298	27.649191
256.190094	11216.245679	27.654208
256.384493	11226.370089	27.659226
256.589408	11250.339101	27.664244
256.963896	11263.574014	27.669261
257.225437	11283.618723	27.674279
257.852629	11297.016162	27.679296
258.035599	11308.607555	27.684314
258.396543	11327.755755	27.689332
258.551052	11329.944975	27.694349
258.561395	11346.820926	27.699367
259.281582	11366.152872	27.704384
259.542391	11370.981036	27.709402
259.387319	11385.347334	27.714420
259.856435	11405.533328	27.719437
259.619996	11417.676769	27.724455
260.141627	11428.899418	27.729472
260.095930	11443.390722	27.734490
260.189719	11467.961589	27.739508
260.559557	11489.442084	27.744525
261.055848	11511.126990	27.749543
260.764066	11522.909720	27.754560
261.667759	11539.614324	27.759578
261.484029	11557.806046	27.764596
262.073562	11569.311807	27.769613
262.406590	11601.515410	27.774631
262.514674	11608.840039	27.779648
262.612757	11627.391867	27.784666
263.013105	11642.849177	27.789684
263.430608	11662.939329	27.794701
263.596518	11678.493390	27.799719
263.794359	11691.806800	27.804736
264.369154	11709.908265	27.809754
264.387157	11725.375014	27.814772
264.665219	11740.213702	27.819789
264.540657	11770.149403	27.824807
264.664654	11784.162831	27.829824
265.082926	11801.865768	27.834842
265.291086	11825.140304	27.839860
265.695929	11845.955756	27.844877
266.224611	11876.487156	27.849895
266.168073	11898.751718	27.854912
266.638873	11904.693388	27.859930
266.876769	11936.325125	27.864948
267.429566	11956.504918	27.869965
267.547122	11975.275082	27.874983
268.021877	11993.638796	27.880000
268.252444	12005.055801	27.885018
268.385816	12035.842009	27.890036
268.558178	12051.982713	27.895053
268.969354	12063.781972	27.900071
269.025633	12084.857546	27.905088
269.707935	12101.303660	27.910106
269.786259	12112.738264	27.915124
270.385680	12136.829758	27.920141
270.133446	12160.852595	27.925159
270.563133	12179.286707	27.930176
270.947360	12202.199401	27.935194
271.290586	12218.534528	27.940212
271.473321	12226.343478	27.945229
272.004738	12239.886066	27.950247
272.035553	12263.751013	27.955264
272.502920	12272.308005	27.960282
272.190254	12294.799467	27.965300
272.841560	12316.129449	27.970317
273.044001	12340.374967	27.975335
273.210250	12354.628510	27.980352
273.582782	12374.410684	27.985370
273.841070	12404.006370	27.990388
274.081885	12419.119843	27.995405
274.388387	12438.091390	28.000423
274.732179	12462.081242	28.005440
275.326263	12469.061656	28.010458
274.879889	12489.142755	28.015476
275.523738	12505.292093	28.020493
275.620764	12536.886905	28.025511
275.888241	12550.250013	28.030528
276.594078	12565.893909	28.035546
276.970706	12594.830310	28.040564
276.700646	12603.348234	28.045581
277.134278	12619.271656	28.050599
277.125124	12648.612779	28.055616
277.776872	12665.885221	28.060634
277.855936	12692.752608	28.065652
278.182317	12703.646609	28.070669
278.355434	12721.717234	28.075687
278.907251	12749.063275	28.080704
278.921440	12772.160943	28.085722
279.011279	12800.801532	28.090740
279.498109	12812.194672	28.095757
280.079058	12831.139412	28.100775
280.174302	12852.822372	28.105792
280.725569	12866.943357	28.110810
280.525786	12888.959944	28.115828
281.029233	12895.585240	28.120845
281.458244	12914.781235	28.125863
281.377286	12933.665553	28.130880
281.793256	12953.267844	28.135898
281.958961	12975.044117	28.140916
282.391948	12990.784793	28.145933
282.601273	13007.492110	28.150951
282.419538	13035.133476	28.155968
283.186126	13052.577760	28.160986
283.114232	13071.309213	28.166004
283.671362	13108.599311	28.171021
283.968884	13129.300357	28.176039
284.170587	13150.126965	28.181056
284.744101	13162.359387	28.186074
284.910311	13188.907504	28.191092
285.021211	13217.374893	28.196109
285.475122	13228.088163	28.201127
285.721122	13262.392491	28.206144
286.074286	13274.100541	28.211162
286.230520	13303.271503	28.216180
286.510542	13321.319638	28.221197
286.941750	13342.138927	28.226215
287.269318	13364.386096	28.231232
287.292266	13381.309259	28.236250
287.853969	13404.344036	28.241268
287.913778	13420.513013	28.246285
288.545711	13446.249564	28.251303
288.550148	13471.092829	28.256320
289.340810	13482.593523	28.261338
289.358122	13502.230409	28.266356
289.700280	13525.906064	28.271373
290.317702	13552.001887	28.276391
290.503085	13570.601949	28.281408
290.667448	13582.668200	28.286426
290.784484	13602.507472	28.291444
291.228355	13628.621113	28.296461
291.553627	13652.479579	28.301479
291.356714	13669.803771	28.306496
292.044120	13681.769204	28.311514
292.152442	13724.603711	28.316532
292.363645	13738.645981	28.321549
292.565418	13748.224246	28.326567
293.356612	13788.011776	28.331584
293.589396	13802.764435	28.336602
293.767079	13833.132914	28.341620
293.996731	13849.869369	28.346637
294.372970	13870.884176	28.351655
294.315192	13887.482520	28.356672
294.922221	13911.925633	28.361690
295.251300	13936.314417	28.366708
295.672509	13954.918968	28.371725
296.011152	13969.383578	28.376743
295.752337	13999.441728	28.381760
296.100450	14006.094908	28.386778
296.613181	14042.386362	28.391796
296.401883	14059.795272	28.396813
297.293476	14086.922641	28.401831
297.520753	14105.421919	28.406848
297.959638	14126.774589	28.411866
298.589936	14149.859531	28.416884
298.480679	14170.116975	28.421901
298.794151	14183.148743	28.426919
299.291798	14217.307999	28.431936
299.485473	14222.554813	28.436954
299.846473	14241.968085	28.441972
299.979170	14254.039722	28.446989
300.459035	14277.331556	28.452007
300.628039	14303.672354	28.457024
301.157706	14319.171603	28.462042
301.313015	14334.811619	28.467060
301.384081	14350.948042	28.472077
302.048064	14362.323842	28.477095
301.936480	14374.607520	28.482112
302.290094	14395.749620	28.487130
302.538605	14417.805126	28.492148
302.598482	14437.916350	28.497165
302.909171	14460.593800	28.502183
302.982989	14488.560433	28.507200
303.436029	14512.017823	28.512218
303.947174	14546.813509	28.517236
304.246116	14560.034145	28.522253
304.392039	14585.677829	28.527271
304.510607	14624.729236	28.532288
304.950638	14638.044678	28.537306
305.407573	14673.196488	28.542324
305.741169	14698.220341	28.547341
306.205732	14721.758297	28.552359
306.411961	14749.420331	28.557376
306.585697	14763.099713	28.562394
306.875408	14789.652824	28.567412
306.733214	14821.418390	28.572429
307.721748	14844.590180	28.577447
307.830959	14873.041358	28.582464
308.273093	14892.868946	28.587482
308.845311	14920.897102	28.592500
309.203045	14952.445611	28.597517
309.786733	14961.604621	28.602535
309.914707	14993.195505	28.607552
310.054786	15019.194412	28.612570
310.602090	15031.789033	28.617588
310.633871	15051.169426	28.622605
311.448024	15064.672908	28.627623
311.102529	15098.766845	28.632640
311.216358	15113.277015	28.637658
311.792459	15141.263829	28.642676
311.944806	15166.484075	28.647693
312.417301	15183.392108	28.652711
312.846909	15224.654195	28.657728
313.269391	15227.310380	28.662746
313.459767	15257.587547	28.667764
313.728562	15282.123302	28.672781
314.141393	15296.807856	28.677799
314.526597	15323.087767	28.682816
315.265220	15344.079017	28.687834
315.416547	15361.716555	28.692852
315.628994	15384.881082	28.697869
315.973964	15400.893368	28.702887
316.287541	15425.760234	28.707904
316.027473	15451.206533	28.712922
316.367859	15464.617120	28.717940
316.905410	15487.765587	28.722957
317.174017	15514.613578	28.727975
317.167003	15541.176312	28.732992
317.752282	15562.400273	28.738010
318.406941	15592.327305	28.743028
318.258714	15610.890020	28.748045
319.015624	15643.921581	28.753063
319.054833	15662.789772	28.758080
319.625557	15688.952691	28.763098
319.842249	15714.552059	28.768116
319.813522	15729.966215	28.773133
320.514342	15749.343581	28.778151
320.655439	15777.175220	28.783168
321.056662	15794.774012	28.788186
321.383708	15811.768553	28.793204
321.826742	15842.701912	28.798221
322.241836	15859.745871	28.803239
322.543020	15874.533635	28.808256
322.958174	15886.110405	28.813274
323.166068	15917.115461	28.818292
323.002904	15935.794532	28.823309
323.659814	15956.764512	28.828327
323.884091	15984.968750	28.833344
323.905951	15995.732310	28.838362
324.092855	16026.342868	28.843380
324.336791	16059.534459	28.848397
324.684656	16083.701951	28.853415
324.982167	16115.902972	28.858432
325.334188	16149.737903	28.863450
325.936974	16170.672377	28.868468
326.428035	16204.242424	28.873485
326.905300	16235.227906	28.878503
326.627214	16267.146645	28.883520
327.376685	16285.161949	28.888538
327.662704	16315.741648	28.893556
327.768401	16340.332731	28.898573
328.302158	16374.989223	28.903591
328.694456	16391.421319	28.908608
328.904598	16410.882533	28.913626
329.026325	16442.581009	28.918644
329.386296	16478.512518	28.923661
330.389673	16489.147874	28.928679
330.635577	16526.982970	28.933696
331.100650	16554.550206	28.938714
331.120233	16577.361041	28.943732
331.539329	16603.138350	28.948749
331.798988	16615.820134	28.953767
332.015734	16641.341764	28.958784
332.546609	16672.370089	28.963802
332.987404	16702.913525	28.968820
333.056668	16729.529120	28.973837
333.324160	16740.677865	28.978855
333.667790	16785.548043	28.983872
333.969654	16809.928958	28.988890
334.161971	16836.800220	28.993908
334.485409	16868.120356	28.998925
334.959396	16886.226755	29.003943
335.531603	16916.585699	29.008960
336.018354	16938.707860	29.013978
336.247758	16969.960768	29.018996
336.493237	17002.240909	29.024013
337.116437	17016.666410	29.029031
337.640399	17045.712822	29.034048
337.480262	17063.451246	29.039066
337.921958	17094.784812	29.044084
337.975640	17122.388873	29.049101
338.726403	17138.980243	29.054119
339.079950	17174.099131	29.059136
339.095850	17198.500062	29.064154
339.627254	17224.873382	29.069172
340.023259	17254.704540	29.074189
340.611851	17268.592366	29.079207
340.867729	17305.344013	29.084224
340.876566	17327.175078	29.089242
341.655099	17346.257607	29.094260
341.578923	17376.295578	29.099277
342.179266	17407.788003	29.104295
342.280712	17427.412566	29.109312
342.753193	17439.796229	29.114330
343.061680	17453.532227	29.119348
343.014116	17494.412760	29.124365
343.605032	17511.162154	29.129383
343.911602	17533.016305	29.134400
344.219366	17559.545144	29.139418
344.594629	17583.789191	29.144436
344.907109	17622.080329	29.149453
345.274445	17637.778264	29.154471
345.688761	17662.477462	29.159488
345.856422	17685.812864	29.164506
346.180416	17713.710248	29.169524
346.283200	17742.008734	29.174541
346.727928	17765.180800	29.179559
347.124481	17796.301463	29.184576
347.503554	17818.289880	29.189594
347.770083	17854.093282	29.194612
348.035663	17882.808695	29.199629
348.746415	17909.293840	29.204647
349.080268	17938.459817	29.209664
349.026016	17975.804618	29.214682
349.972928	17999.403702	29.219700
350.003961	18033.784978	29.224717
350.421434	18061.396567	29.229735
350.768839	18086.795397	29.234752
351.129059	18113.967484	29.239770
351.381759	18140.410979	29.244788
351.609418	18183.328326	29.249805
351.871797	18203.471776	29.254823
352.250919	18233.300768	29.259840
352.383574	18264.583553	29.264858
352.899213	18302.869481	29.269876
352.875435	18342.200257	29.274893
353.700469	18377.980316	29.279911
354.041511	18406.059236	29.284928
354.283476	18439.852237	29.289946
354.964500	18468.471852	29.294964
355.229772	18499.108793	29.299981
355.633194	18537.507526	29.304999
356.134417	18566.111225	29.310016
356.242757	18600.007565	29.315034
357.067334	18623.247510	29.320052
356.971597	18650.441226	29.325069
357.734311	18683.957231	29.330087
358.228799	18717.054114	29.335104
358.454595	18753.655270	29.340122
359.020560	18772.456617	29.345140
359.198432	18796.802594	29.350157
359.160677	18828.763707	29.355175
359.953390	18857.315858	29.360192
360.374521	18883.437044	29.365210
360.639218	18899.398472	29.370228
360.881434	18940.198743	29.375245
361.412262	18958.645659	29.380263
362.176545	18994.840710	29.385280
361.914370	19019.672871	29.390298
362.505052	19039.152931	29.395316
362.845440	19070.499238	29.400333
363.438722	19097.629874	29.405351
363.665256	19126.346920	29.410368
363.773158	19155.562749	29.415386
364.052893	19181.062058	29.420404
364.567899	19210.833356	29.425421
365.051020	19238.442650	29.430439
365.094507	19269.545159	29.435456
365.742156	19306.125497	29.440474
365.833852	19324.300376	29.445492
366.167644	19377.628326	29.450509
366.287802	19401.175398	29.455527
366.997935	19419.834748	29.460544
367.147740	19451.950722	29.465562
368.122434	19470.695040	29.470580
367.997208	19503.978781	29.475597
368.580007	19528.988813	29.480615
369.081556	19548.236942	29.485632
369.334037	19573.241909	29.490650
369.757110	19591.453582	29.495668
369.714528	19634.138457	29.500685
370.238154	19658.690389	29.505703
370.679022	19687.987537	29.510720
370.834777	19718.270780	29.515738
371.068685	19751.953589	29.520756
371.559902	19787.169355	29.525773
371.575883	19814.416687	29.530791
372.050983	19846.545536	29.535808
372.323250	19886.148950	29.540826
372.937921	19919.159547	29.545844
373.274936	19951.512378	29.550861
373.953661	19982.946150	29.555879
374.286354	20013.669678	29.560896
374.727272	20056.374508	29.565914
375.113864	20075.641164	29.570932
375.316185	20114.706315	29.575949
375.799322	20151.332958	29.580967
376.142208	20176.450898	29.585984
376.066848	20209.544795	29.591002
376.636109	20256.330485	29.596020
377.309007	20279.103344	29.601037
377.514935	20320.809366	29.606055
377.892868	20350.768144	29.611072
378.131026	20392.241812	29.616090
378.768237	20428.383603	29.621108
378.994732	20451.649912	29.626125
379.069797	20484.903941	29.631143
379.933385	20524.738255	29.636160
379.931170	20564.828315	29.641178
380.413504	20606.940250	29.646196
381.073170	20642.503949	29.651213
381.032183	20673.217538	29.656231
381.801020	20712.030861	29.661248
382.132105	20743.646674	29.666266
382.555684	20792.806902	29.671284
382.886647	20822.527338	29.676301
383.358782	20854.222330	29.681319
383.927686	20885.497835	29.686336
384.137859	20923.223852	29.691354
385.108215	20961.740728	29.696372
385.247259	21002.138111	29.701389
385.586301	21025.343239	29.706407
386.044973	21057.217585	29.711424
386.444593	21078.309228	29.716442
386.541728	21118.599681	29.721460
387.535424	21143.648509	29.726477
387.562412	21183.141310	29.731495
388.179629	21210.094205	29.736512
388.370849	21245.056285	29.741530
388.271481	21269.423482	29.746548
388.695973	21306.295248	29.751565
389.035966	21333.822496	29.756583
389.625451	21361.651907	29.761600
389.882928	21411.623200	29.766618
390.408214	21445.389640	29.771636
390.953638	21484.700740	29.776653
390.869731	21514.967419	29.781671
391.332306	21540.346372	29.786688
391.973656	21593.139301	29.791706
392.406438	21613.234292	29.796724
393.002429	21649.056211	29.801741
392.880282	21675.727477	29.806759
393.662908	21696.696603	29.811776
394.059732	21738.615832	29.816794
394.614085	21761.377385	29.821812
394.748832	21797.107533	29.826829
394.405214	21826.511789	29.831847
395.073083	21859.902754	29.836864
395.692163	21907.588142	29.841882
395.935794	21930.670267	29.846900
396.673909	21967.677388	29.851917
397.026359	22011.215435	29.856935
397.718738	22037.784879	29.861952
397.886772	22069.895947	29.866970
398.002198	22097.813288	29.871988
398.420284	22143.262267	29.877005
398.822792	22176.404665	29.882023
399.354656	22202.847821	29.887040
399.726822	22243.792559	29.892058
399.788313	22281.304337	29.897076
400.055358	22325.444108	29.902093
400.350707	22367.361605	29.907111
401.076104	22406.501012	29.912128
401.251354	22458.017003	29.917146
402.046937	22491.471176	29.922164
402.506552	22539.100915	29.927181
402.681209	22575.319091	29.932199
403.408971	22608.461817	29.937216
403.534304	22657.256341	29.942234
404.177795	22682.728483	29.947252
404.579684	22724.415199	29.952269
404.816375	22772.320537	29.957287
405.371343	22800.555479	29.962304
405.742382	22842.493717	29.967322
406.120545	22886.459352	29.972340
406.841077	22925.739564	29.977357
407.283538	22960.380956	29.982375
408.242449	22996.767738	29.987392
408.352048	23021.363435	29.992410
408.793018	23051.499687	29.997428
409.008599	23087.251089	30.002445
409.539470	23127.945300	30.007463
410.158160	23151.241821	30.012480
409.929933	23188.560560	30.017498
410.580198	23225.154084	30.022516
411.097541	23258.867984	30.027533
411.398402	23297.721769	30.032551
411.885552	23333.367883	30.037568
412.335397	23360.330965	30.042586
412.868964	23392.014078	30.047604
413.404145	23423.254642	30.052621
413.055374	23466.539193	30.057639
413.866975	23497.180481	30.062656
414.182032	23548.765864	30.067674
414.614725	23574.069950	30.072692
415.304157	23613.090980	30.077709
415.536223	23654.218546	30.082727
416.033280	23674.141256	30.087744
416.384135	23723.730896	30.092762
416.477693	23756.652586	30.097780
417.020377	23791.109101	30.102797
417.471252	23823.747437	30.107815
417.984606	23866.120532	30.112832
418.613618	23906.946307	30.117850
418.706152	23938.705687	30.122868
419.185591	23979.536080	30.127885
419.446926	24016.312043	30.132903
420.010918	24059.992060	30.137920
420.572140	24092.942163	30.142938
420.960521	24131.309900	30.147956
421.095571	24163.480063	30.152973
421.630272	24196.801021	30.157991
421.680314	24226.178745	30.163008
422.520008	24269.449504	30.168026
422.842867	24302.677429	30.173044
423.491755	24336.764356	30.178061
423.580831	24377.587189	30.183079
424.205588	24404.265183	30.188096
424.547489	24440.530061	30.193114
424.689147	24480.049354	30.198132
425.292128	24516.450424	30.203149
425.284208	24559.822976	30.208167
425.860852	24600.721564	30.213184
426.395126	24638.776718	30.218202
427.000281	24687.545278	30.223220
427.461215	24727.526941	30.228237
427.745357	24764.540851	30.233255
428.283241	24802.026980	30.238272
428.774127	24847.211607	30.243290
429.060238	24893.995698	30.248308
429.704270	24929.487370	30.253325
429.685958	24961.095097	30.258343
430.074623	25007.073422	30.263360
430.753864	25055.243533	30.268378
431.070143	25097.593221	30.273396
431.879043	25144.289689	30.278413
432.170642	25186.321120	30.283431
432.560394	25230.991587	30.288448
433.269145	25272.629229	30.293466
433.644259	25310.818023	30.298484
434.006381	25357.433289	30.303501
434.308226	25394.824777	30.308519
434.954662	25427.687887	30.313536
435.544443	25471.069900	30.318554
435.759446	25507.615694	30.323572
436.011724	25561.484926	30.328589
436.346372	25599.453087	30.333607
436.995285	25639.154321	30.338624
437.420889	25692.238360	30.343642
437.619022	25736.187884	30.348660
438.362914	25775.470031	30.353677
438.485124	25818.572108	30.358695
438.844371	25857.036181	30.363712
439.660310	25903.859708	30.368730
439.908939	25950.690042	30.373748
440.812084	25990.371106	30.378765
441.109482	26049.745659	30.383783
441.221086	26090.720113	30.388800
441.748372	26138.132923	30.393818
442.041636	26184.147832	30.398836
442.917340	26217.267044	30.403853
443.099193	26267.445594	30.408871
443.694691	26307.801163	30.413888
444.584462	26349.210430	30.418906
444.995444	26388.956724	30.423924
445.850087	26427.603416	30.428941
445.668366	26470.773446	30.433959
446.193928	26510.950768	30.438976
446.713950	26539.082686	30.443994
447.052943	26579.965631	30.449012
447.026607	26618.839158	30.454029
447.926092	26666.125384	30.459047
448.020218	26713.152326	30.464064
448.566394	26743.599974	30.469082
448.830647	26796.686901	30.474100
449.397644	26835.398385	30.479117
449.965208	26886.687312	30.484135
450.444739	26924.502539	30.489152
450.869739	26956.157711	30.494170
451.159982	27001.391223	30.499188
451.901055	27031.644448	30.504205
452.176743	27070.439931	30.509223
452.608765	27105.621013	30.514240
452.957365	27149.587955	30.519258
453.275361	27184.085467	30.524276
453.792138	27229.884447	30.529293
453.927868	27275.313421	30.534311
454.531084	27320.435417	30.539328
455.027982	27351.169796	30.544346
455.115263	27412.110798	30.549364
455.629667	27456.242047	30.554381
456.226415	27505.315785	30.559399
456.636531	27562.268984	30.564416
457.663810	27603.153630	30.569434
457.878994	27652.028342	30.574452
458.491613	27697.649027	30.579469
459.029638	27750.885178	30.584487
459.145460	27789.447924	30.589504
459.837743	27831.030201	30.594522
460.021258	27888.632903	30.599540
460.751101	27921.499637	30.604557
461.156580	27973.183286	30.609575
461.649131	28016.288901	30.614592
462.099866	28067.637024	30.619610
462.630245	28108.771173	30.624628
463.211853	28142.337797	30.629645
463.234602	28190.776205	30.634663
463.921347	28239.395161	30.639680
464.256338	28290.705086	30.644698
464.380543	28343.994956	30.649716
464.871193	28395.204913	30.654733
465.638649	28457.407788	30.659751
466.040607	28496.236770	30.664768
466.832109	28555.338970	30.669786
467.396176	28599.167831	30.674804
467.797686	28642.112040	30.679821
468.372032	28699.017399	30.684839
468.769415	28739.724863	30.689856
469.313505	28784.322079	30.694874
469.421381	28844.360227	30.699892
470.164492	28884.394376	30.704909
470.655662	28933.311092	30.709927
470.907574	28985.659765	30.714944
471.474251	29033.717882	30.719962
471.685131	29095.093322	30.724980
472.894682	29121.173935	30.729997
473.273006	29181.385623	30.735015
473.652431	29226.117047	30.740032
473.847291	29260.845942	30.745050
474.803435	29314.817124	30.750068
475.436511	29356.481305	30.755085
475.954311	29404.004330	30.760103
476.111749	29458.960659	30.765120
476.691806	29489.716833	30.770138
476.732502	29533.541166	30.775156
477.495383	29579.079295	30.780173
477.854083	29624.149851	30.785191
478.498989	29673.448804	30.790208
478.967054	29717.212912	30.795226
479.170604	29758.780831	30.800244
479.503257	29804.329952	30.805261
480.214047	29854.466064	30.810279
480.871843	29894.066735	30.815296
481.475745	29945.281781	30.820314
481.538684	29994.533584	30.825332
482.277180	30033.401256	30.830349
482.485349	30078.591202	30.835367
482.889822	30127.246195	30.840384
483.322759	30162.887521	30.845402
483.736979	30209.189642	30.850420
484.182194	30249.627104	30.855437
484.840162	30302.193660	30.860455
484.930768	30348.812278	30.865472
485.593130	30388.526968	30.870490
486.483690	30439.477093	30.875508
486.806484	30487.848620	30.880525
487.392564	30541.331011	30.885543
487.372243	30591.305277	30.890560
487.870813	30631.943738	30.895578
488.156685	30696.327539	30.900596
488.644104	30744.705490	30.905613
489.435797	30802.126264	30.910631
489.930429	30857.292678	30.915648
490.724357	30913.038198	30.920666
491.338773	30961.927776	30.925684
491.777418	31008.689335	30.930701
492.462627	31055.671567	30.935719
492.802523	31113.992098	30.940736
493.103512	31149.870725	30.945754
493.446459	31211.731172	30.950772
494.142170	31260.216777	30.955789
494.663072	31305.714430	30.960807
494.916361	31366.521014	30.965824
495.576326	31414.102252	30.970842
496.062831	31470.776139	30.975860
496.545846	31510.653826	30.980877
496.975118	31562.260560	30.985895
497.674282	31620.576816	30.990912
497.977558	31675.465605	30.995930
498.605234	31729.804307	31.000948
499.251270	31783.419586	31.005965
499.662368	31827.898797	31.010983
500.116486	31876.961037	31.016000
500.792586	31937.298466	31.021018
500.772120	31992.706615	31.026036
501.069182	32046.750220	31.031053
501.984658	32104.793718	31.036071
502.250134	32173.383045	31.041088
502.934033	32209.355251	31.046106
503.454684	32274.687065	31.051124
503.983122	32332.374564	31.056141
504.768600	32386.721872	31.061159
505.281221	32446.700734	31.066176
506.040787	32490.538830	31.071194
506.456661	32550.564753	31.076212
507.116413	32604.654148	31.081229
507.296265	32648.052315	31.086247
507.710208	32700.163708	31.091264
508.602114	32754.210807	31.096282
508.871523	32809.171099	31.101300
509.226220	32855.949948	31.106317
510.061373	32914.469793	31.111335
510.202956	32966.927971	31.116352
511.001894	33019.687945	31.121370
511.426998	33072.203136	31.126388
512.176049	33135.194251	31.131405
512.703321	33175.769954	31.136423
512.947714	33229.571970	31.141440
513.424643	33283.641173	31.146458
513.936855	33336.775611	31.151476
514.463958	33385.627642	31.156493
514.779987	33440.563318	31.161511
515.206383	33492.870720	31.166528
516.122946	33543.312253	31.171546
516.649232	33590.596942	31.176564
516.540380	33648.166591	31.181581
517.249423	33687.949804	31.186599
517.704395	33747.176401	31.191616
518.037498	33800.327417	31.196634
518.426775	33849.973450	31.201652
519.754228	33906.749828	31.206669
520.148411	33958.159318	31.211687
520.082097	34016.564200	31.216704
520.811083	34067.908875	31.221722
521.159629	34119.540872	31.226740
521.761758	34178.644472	31.231757
522.363965	34235.883067	31.236775
522.808959	34297.951607	31.241792
523.530650	34352.339284	31.246810
524.044177	34403.117873	31.251828
524.513022	34471.271872	31.256845
525.232997	34518.819149	31.261863
525.773290	34587.423887	31.266880
526.037741	34639.285295	31.271898
526.681813	34688.457127	31.276916
526.842946	34753.479908	31.281933
527.721572	34808.564970	31.286951
527.960643	34876.269409	31.291968
528.754543	34927.264577	31.296986
529.743366	34985.234996	31.302004
530.158077	35047.057564	31.307021
530.883909	35095.793909	31.312039
531.052529	35165.135271	31.317056
531.571413	35213.385824	31.322074
532.130166	35266.321819	31.327092
532.621505	35329.170159	31.332109
533.356390	35389.388146	31.337127
533.630694	35454.351088	31.342144
534.541590	35499.600731	31.347162
534.964482	35561.796570	31.352180
535.273118	35617.453550	31.357197
536.072608	35679.831025	31.362215
536.306437	35725.901691	31.367232
537.052083	35786.055886	31.372250
537.689159	35840.941185	31.377268
538.053928	35917.190663	31.382285
538.588214	35970.246057	31.387303
539.460935	36027.826506	31.392320
539.626865	36077.285103	31.397338
540.248994	36135.297123	31.402356
540.467634	36201.687443	31.407373
541.348704	36262.517321	31.412391
541.426339	36330.858694	31.417408
542.345063	36384.101512	31.422426
542.783412	36440.277797	31.427444
543.251159	36507.515304	31.432461
544.155011	36566.521385	31.437479
544.448025	36631.383808	31.442496
545.225149	36689.720839	31.447514
546.103312	36747.409873	31.452532
546.240719	36814.712730	31.457549
546.950042	36865.953430	31.462567
547.401342	36935.249947	31.467584
547.961184	36992.964204	31.472602
548.307251	37040.234215	31.477620
549.079111	37106.559667	31.482637
549.945258	37161.532628	31.487655
549.937306	37227.702355	31.492672
550.386382	37280.464496	31.497690
551.473576	37342.074566	31.502708
551.600414	37390.239678	31.507725
551.970795	37445.253070	31.512743
552.462746	37509.777139	31.517760
553.239805	37562.741547	31.522778
553.940988	37629.674099	31.527796
554.314832	37682.486951	31.532813
555.073378	37726.418250	31.537831
555.245769	37795.773872	31.542848
556.191934	37846.347458	31.547866
556.948250	37905.683867	31.552884
557.185120	37964.159566	31.557901
558.030244	38020.111863	31.562919
558.272800	38073.863172	31.567936
558.871732	38128.684423	31.572954
559.342514	38186.080674	31.577972
560.081319	38246.179613	31.582989
560.694810	38305.539492	31.588007
560.852103	38376.385431	31.593024
561.503964	38432.729523	31.598042
562.637985	38487.183310	31.603060
563.004330	38543.458579	31.608077
563.168760	38597.248721	31.613095
563.589939	38673.511797	31.618112
564.028939	38730.851234	31.623130
564.706638	38789.974727	31.628148
565.165819	38865.461009	31.633165
565.916775	38927.450797	31.638183
566.401547	38988.837406	31.643200
567.231255	39061.350988	31.648218
567.689660	39131.545134	31.653236
568.069717	39192.777971	31.658253
568.967257	39261.227893	31.663271
569.200619	39326.967838	31.668288
569.673543	39401.353443	31.673306
570.455554	39472.851367	31.678324
571.022791	39529.850303	31.683341
571.391878	39598.251244	31.688359
572.184660	39673.726035	31.693376
572.688956	39736.604204	31.698394
573.543336	39799.693344	31.703412
573.907971	39881.079479	31.708429
574.791625	39948.426999	31.713447
575.275022	40018.828796	31.718464
576.058352	40076.592179	31.723482
576.905084	40138.292155	31.728500
577.202232	40203.145676	31.733517
578.199390	40256.550209	31.738535
578.529147	40327.343876	31.743552
579.355312	40392.481921	31.748570
580.168287	40443.499845	31.753588
580.402026	40505.303186	31.758605
580.960841	40565.923718	31.763623
581.596870	40632.218005	31.768640
581.948245	40694.724446	31.773658
582.336250	40757.484632	31.778676
583.080656	40823.073156	31.783693
583.706727	40877.150803	31.788711
584.107469	40950.022459	31.793728
584.813568	41012.082129	31.798746
585.836626	41075.711427	31.803764
586.065645	41135.398552	31.808781
586.665494	41198.645441	31.813799
587.511416	41259.064812	31.818816
587.696744	41327.050894	31.823834
588.769578	41378.605845	31.828852
589.108249	41457.332900	31.833869
589.869452	41515.533630	31.838887
589.930076	41573.161163	31.843904
590.656057	41633.012149	31.848922
591.346116	41689.908937	31.853940
592.071461	41752.758282	31.858957
592.700551	41808.362022	31.863975
593.052957	41864.135731	31.868992
593.410805	41921.673354	31.874010
594.193295	41973.344747	31.879028
594.337904	42039.834096	31.884045
595.193056	42102.227696	31.889063
595.581736	42170.342656	31.894080
595.917495	42241.419849	31.899098
596.643977	42305.459678	31.904116
597.015291	42377.448855	31.909133
597.906186	42442.329851	31.914151
598.574513	42508.023867	31.919168
598.851388	42586.707708	31.924186
599.841635	42653.313142	31.929204
600.277878	42735.210968	31.934221
600.861902	42797.623695	31.939239
601.549738	42876.408655	31.944256
601.693714	42940.535226	31.949274
602.672925	43010.812032	31.954292
603.324517	43091.791931	31.959309
604.023395	43168.659679	31.964327
604.568202	43232.793897	31.969344
605.119718	43299.805222	31.974362
606.421110	43360.880096	31.979380
606.670801	43450.444337	31.984397
607.436673	43517.890820	31.989415
608.213266	43579.118062	31.994432
608.518577	43649.407553	31.999450
609.245933	43714.374815	32.004468
609.802335	43788.363693	32.009485
610.264655	43859.312395	32.014503
610.900757	43927.172616	32.019520
611.458302	43996.955621	32.024538
612.302934	44064.903787	32.029556
612.772425	44146.390454	32.034573
613.668136	44211.870466	32.039591
614.083470	44273.491445	32.044608
614.643829	44344.527545	32.049626
615.325465	44418.669691	32.054644
616.194548	44492.415845	32.059661
616.269289	44563.636228	32.064679
617.154673	44636.943841	32.069696
617.712181	44702.124024	32.074714
618.344001	44783.745733	32.079732
618.830627	44864.865449	32.084749
619.534783	44933.230448	32.089767
620.434759	44991.962580	32.094784
621.015216	45080.937550	32.099802
621.616705	45141.355182	32.104820
621.942658	45214.568853	32.109837
622.847775	45300.343620	32.114855
623.805894	45367.158308	32.119872
623.982882	45444.621693	32.124890
625.130967	45506.453927	32.129908
625.394887	45586.054970	32.134925
625.969220	45650.223136	32.139943
626.700955	45713.221846	32.144960
627.470372	45780.181181	32.149978
628.547690	45851.963467	32.154996
628.775241	45921.778844	32.160013
629.102441	45984.810039	32.165031
629.911940	46059.519574	32.170048
630.613693	46126.775206	32.175066
631.139464	46199.347164	32.180084
631.390898	46269.855742	32.185101
631.943195	46339.760728	32.190119
632.757848	46396.042725	32.195136
633.367753	46483.013254	32.200154
634.035295	46543.898765	32.205172
634.498673	46608.789236	32.210189
635.016104	46678.985408	32.215207
635.248965	46743.773190	32.220224
636.241939	46823.549100	32.225242
637.335366	46887.658469	32.230260
637.420380	46965.584311	32.235277
638.257262	47032.985961	32.240295
638.897254	47111.059461	32.245312
639.296100	47188.626932	32.250330
639.988419	47256.602275	32.255348
640.762305	47340.678263	32.260365
641.208483	47419.422138	32.265383
642.085531	47489.925105	32.270400
642.404538	47570.891006	32.275418
643.672676	47645.407421	32.280436
644.202634	47716.332381	32.285453
644.677571	47794.819994	32.290471
645.203870	47875.425537	32.295488
645.689802	47952.083610	32.300506
646.318085	48035.406805	32.305524
647.311473	48117.692509	32.310541
647.821298	48190.956603	32.315559
649.062465	48267.605014	32.320576
649.336623	48347.391293	32.325594
650.261690	48434.281974	32.330612
650.357472	48506.770477	32.335629
651.206567	48587.384922	32.340647
652.328079	48662.187021	32.345664
652.650494	48744.953340	32.350682
653.121579	48807.394096	32.355700
653.934888	48895.499789	32.360717
654.745318	48982.081510	32.365735
655.254991	49052.691128	32.370752
655.992990	49140.708328	32.375770
656.583315	49218.973972	32.380788
656.827168	49299.147922	32.385805
657.698662	49378.122975	32.390823
658.416474	49461.722053	32.395840
659.411789	49548.865364	32.400858
660.181118	49619.069095	32.405876
660.571897	49703.650333	32.410893
661.058350	49785.141963	32.415911
662.191260	49865.570931	32.420928
662.501782	49942.788276	32.425946
663.615858	50015.020832	32.430964
664.428614	50095.323582	32.435981
664.963466	50173.310110	32.440999
665.614717	50253.075586	32.446016
666.190634	50333.207457	32.451034
666.849860	50402.608285	32.456052
667.636643	50480.638651	32.461069
668.102288	50561.971773	32.466087
669.064450	50626.542439	32.471104
669.441172	50706.472689	32.476122
670.256744	50787.201329	32.481140
670.833461	50858.685474	32.486157
671.331203	50954.966415	32.491175
672.266487	51025.939354	32.496192
673.052479	51106.028346	32.501210
673.618789	51183.336319	32.506228
674.143974	51255.411878	32.511245
674.871738	51341.755976	32.516263
675.484131	51417.399719	32.521280
675.986187	51500.147781	32.526298
676.577188	51572.049499	32.531316
677.289490	51654.815807	32.536333
677.799390	51730.463963	32.541351
678.681109	51811.280717	32.546368
679.422081	51884.969604	32.551386
679.847666	51949.564704	32.556404
680.830405	52028.860420	32.561421
681.103732	52105.483331	32.566439
681.984132	52187.041931	32.571456
682.560614	52272.369101	32.576474
683.324976	52353.136506	32.581492
683.726487	52424.722502	32.586509
684.233519	52504.214556	32.591527
685.223877	52592.768520	32.596544
685.798140	52670.118143	32.601562
686.450544	52759.099001	32.606580
687.158036	52843.199118	32.611597
687.615329	52928.262588	32.616615
688.760413	53021.350018	32.621632
689.178982	53099.377213	32.626650
690.152246	53186.360442	32.631668
690.914830	53271.605154	32.636685
691.934473	53355.917671	32.641703
692.266210	53435.636499	32.646720
693.122499	53529.498890	32.651738
693.733437	53613.325794	32.656756
694.397336	53683.665876	32.661773
695.147523	53775.084237	32.666791
695.916549	53854.780300	32.671808
696.284994	53945.379491	32.676826
697.027711	54031.167955	32.681844
697.505228	54124.731325	32.686861
698.131436	54222.657243	32.691879
699.023693	54300.829395	32.696896
699.694763	54396.325286	32.701914
700.881926	54492.481154	32.706932
701.451479	54580.640201	32.711949
702.046545	54668.390567	32.716967
702.836230	54746.504313	32.721984
703.467760	54843.261215	32.727002
704.394598	54933.390709	32.732020
705.050398	55020.006405	32.737037
705.623994	55103.325503	32.742055
706.322445	55188.935238	32.747072
707.192583	55285.903388	32.752090
707.539179	55367.278134	32.757108
708.669787	55468.338770	32.762125
709.429785	55550.124044	32.767143
709.828431	55630.567565	32.772160
710.734985	55722.082860	32.777178
711.375264	55810.836612	32.782196
712.238500	55897.638190	32.787213
712.847082	55995.105848	32.792231
713.784678	56076.257559	32.797248
714.487352	56180.938643	32.802266
715.218665	56257.300765	32.807284
716.041496	56338.945998	32.812301
716.427816	56442.785407	32.817319
717.286516	56520.691639	32.822336
718.018901	56614.667900	32.827354
718.660361	56692.532763	32.832372
719.256128	56782.214775	32.837389
719.828174	56879.666438	32.842407
720.877634	56970.948946	32.847424
721.532872	57056.882256	32.852442
722.220597	57150.772674	32.857460
723.185349	57232.405051	32.862477
723.607739	57332.559162	32.867495
724.336120	57405.210241	32.872512
725.017688	57492.989074	32.877530
725.457274	57585.571946	32.882548
726.102728	57663.654517	32.887565
727.149089	57757.991140	32.892583
727.754024	57835.618583	32.897600
728.496335	57931.490856	32.902618
729.112442	58014.237455	32.907636
729.840394	58094.226255	32.912653
730.542521	58190.694469	32.917671
731.858616	58268.768913	32.922688
732.370434	58366.641087	32.927706
732.660623	58453.256806	32.932724
733.776149	58535.895333	32.937741
734.361630	58644.966406	32.942759
735.125935	58719.001944	32.947776
736.011085	58803.177529	32.952794
736.472710	58897.857009	32.957812
737.250467	58984.043818	32.962829
737.823134	59082.947383	32.967847
738.949845	59169.447316	32.972864
739.585436	59275.506841	32.977882
740.387794	59360.355592	32.982900
741.391691	59459.990686	32.987917
741.778003	59548.949864	32.992935
742.472288	59651.115437	32.997952
743.415229	59739.905860	33.002970
743.476237	59841.747309	33.007988
744.513784	59920.453011	33.013005
744.985202	60037.422354	33.018023
746.437699	60124.773481	33.023040
747.175541	60231.030022	33.028058
747.624090	60324.678990	33.033076
748.501130	60419.406918	33.038093
749.045951	60520.662705	33.043111
750.131999	60604.325637	33.048128
750.800552	60714.260133	33.053146
751.403306	60820.008661	33.058164
752.364819	60912.294558	33.063181
752.705309	61012.717158	33.068199
753.591789	61106.420794	33.073216
754.523812	61209.657050	33.078234
755.270434	61316.657522	33.083252
756.300477	61409.434626	33.088269
756.710106	61514.899870	33.093287
757.804684	61605.192520	33.098304
758.572794	61709.576973	33.103322
759.544196	61816.272210	33.108340
760.261532	61904.656331	33.113357
761.018575	62012.531754	33.118375
761.639716	62098.310900	33.123392
762.578073	62196.042935	33.128410
763.140932	62291.776796	33.133428
763.848329	62386.981963	33.138445
764.960974	62479.845098	33.143463
765.504738	62581.388026	33.148480
766.386428	62679.649930	33.153498
767.024266	62778.627766	33.158516
767.840918	62877.615978	33.163533
768.940756	62973.186077	33.168551
769.401602	63071.964895	33.173568
770.649286	63155.484532	33.178586
770.946400	63257.777859	33.183604
772.096175	63344.478751	33.188621
772.909209	63444.742229	33.193639
773.480394	63538.263853	33.198656
774.089647	63633.748705	33.203674
774.837196	63737.131970	33.208692
775.645193	63817.886519	33.213709
776.135919	63915.727041	33.218727
776.699536	63998.660231	33.223744
777.940915	64091.458557	33.228762
778.484334	64183.904371	33.233780
779.291906	64277.986832	33.238797
779.732341	64362.288981	33.243815
780.510424	64458.719153	33.248832
781.181027	64565.004757	33.253850
781.772292	64663.047693	33.258868
782.671735	64744.632914	33.263885
783.372907	64864.032732	33.268903
784.269250	64958.698947	33.273920
785.080184	65063.704806	33.278938
786.229540	65172.450413	33.283956
786.886353	65270.314504	33.288973
787.380969	65372.883063	33.293991
788.520587	65467.665037	33.299008
789.080874	65574.503975	33.304026
789.462449	65687.746856	33.309044
790.801539	65789.564407	33.314061
791.701302	65908.361911	33.319079
792.273604	66007.071471	33.324096
793.360670	66097.159893	33.329114
793.619847	66216.192101	33.334132
794.406580	66313.470049	33.339149
795.208197	66426.903699	33.344167
796.132548	66530.473307	33.349184
797.128994	66641.351175	33.354202
798.143577	66754.588316	33.359220
798.878867	66856.517348	33.364237
799.496585	66967.436941	33.369255
800.211403	67066.976708	33.374272
801.386162	67177.898628	33.379290
802.146646	67294.698297	33.384308
802.890915	67392.005996	33.389325
803.415903	67507.311259	33.394343
804.478667	67617.385183	33.399360
805.790881	67721.677671	33.404378
806.407358	67835.988671	33.409396
807.114008	67938.616645	33.414413
807.856686	68046.874665	33.419431
808.958549	68147.472405	33.424448
809.963158	68248.604976	33.429466
810.813429	68359.291544	33.434484
811.601076	68458.755645	33.439501
812.499414	68553.580511	33.444519
813.150754	68656.580921	33.449536
814.102031	68757.559208	33.454554
814.951790	68866.304119	33.459572
815.985103	68966.320578	33.464589
816.337973	69069.717628	33.469607
816.901533	69171.910669	33.474624
818.060953	69279.823653	33.479642
818.579459	69388.014743	33.484660
819.654980	69483.486470	33.489677
820.167602	69592.724134	33.494695
821.222485	69704.169593	33.499712
822.486116	69803.722625	33.504730
823.176559	69917.436002	33.509748
823.776891	70016.948071	33.514765
824.554921	70121.599833	33.519783
825.416886	70224.491156	33.524800
826.418058	70325.815998	33.529818
827.007774	70434.994457	33.534836
828.011052	70538.992050	33.539853
828.881691	70643.454093	33.544871
829.542091	70743.909383	33.549888
830.249804	70845.028890	33.554906
831.153311	70953.311824	33.559924
831.662435	71048.156059	33.564941
833.023105	71141.778103	33.569959
833.664105	71239.857299	33.574976
834.310484	71335.770279	33.579994
834.929100	71439.996321	33.585012
835.981719	71535.111835	33.590029
836.744317	71642.406451	33.595047
837.299948	71745.997636	33.600064
838.155951	71851.923287	33.605082
838.827705	71958.498820	33.610100
839.937769	72060.674551	33.615117
840.713608	72171.996872	33.620135
841.219174	72285.173163	33.625152
842.131082	72396.082486	33.630170
842.660001	72514.930312	33.635188
843.606843	72631.104084	33.640205
844.756479	72745.625384	33.645223
845.628268	72866.840269	33.650240
846.592524	72974.830662	33.655258
847.169366	73089.721786	33.660276
848.228624	73201.751339	33.665293
849.414701	73312.988874	33.670311
850.046498	73433.889268	33.675328
851.107823	73542.677397	33.680346
851.612009	73656.100392	33.685364
852.734300	73782.916700	33.690381
853.635070	73890.464754	33.695399
854.321437	74010.003907	33.700416
855.551974	74116.969246	33.705434
856.366012	74239.605384	33.710452
856.968574	74358.069890	33.715469
858.095406	74468.574179	33.720487
858.718861	74585.617754	33.725504
859.890063	74699.700720	33.730522
860.507131	74818.798321	33.735540
861.076013	74924.375796	33.740557
862.310557	75044.885065	33.745575
863.433968	75170.884403	33.750592
864.157913	75274.158913	33.755610
864.799286	75392.330547	33.760628
865.368145	75508.284638	33.765645
866.647354	75629.676221	33.770663
867.296960	75761.022044	33.775680
868.700039	75875.542358	33.780698
869.065084	75993.886557	33.785716
869.984745	76106.748114	33.790733
871.184570	76228.560165	33.795751
871.840992	76348.025686	33.800768
872.701562	76469.195223	33.805786
873.620898	76591.762203	33.810804
874.371250	76706.704914	33.815821
875.417012	76822.437925	33.820839
876.457792	76949.864576	33.825856
877.102126	77063.064564	33.830874
878.176578	77192.716615	33.835892
879.061283	77307.324117	33.840909
880.060302	77419.570618	33.845927
880.560978	77550.061614	33.850944
881.732176	77654.136548	33.855962
882.522667	77786.331488	33.860980
883.286194	77909.346813	33.865997
884.460599	78024.215985	33.871015
885.150833	78142.277859	33.876032
886.087475	78253.118677	33.881050
886.467713	78376.791519	33.886068
887.706157	78505.739990	33.891085
888.277617	78626.090194	33.896103
888.990927	78735.815079	33.901120
890.410534	78836.080336	33.906138
891.343911	78959.947886	33.911156
892.010913	79066.995567	33.916173
892.958450	79181.879738	33.921191
893.383162	79310.237247	33.926208
894.679129	79422.990164	33.931226
895.150542	79535.239197	33.936244
895.659968	79657.769984	33.941261
896.921895	79782.387906	33.946279
898.063318	79907.582697	33.951296
898.790878	80030.106304	33.956314
899.714012	80152.650503	33.961332
900.718423	80278.818606	33.966349
901.651376	80395.914529	33.971367
902.389179	80527.611336	33.976384
903.225317	80653.718791	33.981402
903.857306	80781.075054	33.986420
904.628605	80917.506856	33.991437
905.874223	81054.688580	33.996455
906.944875	81184.993370	34.001472
907.848798	81312.980959	34.006490
908.917075	81435.178619	34.011508
909.381847	81572.814546	34.016525
911.085961	81696.104750	34.021543
911.679957	81832.087284	34.026560
912.978042	81967.491434	34.031578
913.526260	82106.586622	34.036596
914.595664	82224.023546	34.041613
915.535998	82334.233789	34.046631
916.288982	82481.204982	34.051648
917.361326	82609.539506	34.056666
918.205886	82740.849811	34.061684
919.195185	82873.835904	34.066701
920.394468	82999.542192	34.071719
920.974348	83139.347024	34.076736
921.818965	83264.565177	34.081754
922.894303	83396.856021	34.086772
923.890462	83517.033951	34.091789
924.851477	83655.121759	34.096807
926.203718	83785.470421	34.101824
927.106253	83908.274854	34.106842
927.952723	84041.871607	34.111860
928.319325	84179.700222	34.116877
929.824333	84306.897582	34.121895
930.475730	84440.298649	34.126912
931.713010	84579.488050	34.131930
932.729122	84709.247298	34.136948
933.732603	84838.084099	34.141965
934.833647	84958.619103	34.146983
935.526310	85088.544741	34.152000
936.482390	85214.298805	34.157018
937.087052	85331.707192	34.162036
937.977459	85464.708088	34.167053
939.148124	85601.948739	34.172071
940.111616	85737.397747	34.177088
940.835114	85864.534249	34.182106
942.082497	85993.540745	34.187124
942.747053	86132.928657	34.192141
944.080863	86261.758074	34.197159
944.898254	86395.268861	34.202176
945.825220	86515.786893	34.207194
946.977090	86643.049797	34.212212
947.712769	86781.960799	34.217229
948.798875	86902.480851	34.222247
949.427685	87041.688606	34.227264
950.791081	87165.131640	34.232282
951.549318	87288.593910	34.237300
952.636700	87415.198625	34.242317
953.883889	87537.026668	34.247335
954.097513	87652.363945	34.252352
955.271810	87774.825341	34.257370
956.347780	87889.508948	34.262388
957.216487	88014.135519	34.267405
957.971085	88130.327742	34.272423
958.746309	88259.823657	34.277440
959.717348	88392.419680	34.282458
960.693167	88517.614552	34.287476
961.547452	88647.074432	34.292493
962.636772	88775.509580	34.297511
963.525087	88903.076964	34.302528
964.141007	89031.663377	34.307546
965.193578	89167.481748	34.312564
965.915569	89311.159231	34.317581
967.102532	89440.228294	34.322599
967.940804	89584.167698	34.327616
969.045933	89726.164995	34.332634
970.113386	89864.924446	34.337652
971.093805	90015.826772	34.342669
972.469593	90153.043799	34.347687
973.035056	90289.399778	34.352704
973.702232	90428.085093	34.357722
975.265155	90569.507753	34.362740
975.673632	90717.448761	34.367757
976.798770	90855.608081	34.372775
977.903238	90997.750899	34.377792
978.921351	91140.364173	34.382810
979.845077	91288.341369	34.387828
980.930072	91427.371425	34.392845
981.866702	91571.038764	34.397863
982.801583	91729.814808	34.402880
983.775748	91874.466300	34.407898
985.174749	92023.019055	34.412916
986.208022	92160.311493	34.417933
987.197543	92310.374649	34.422951
987.839536	92457.438378	34.427968
988.765500	92604.471028	34.432986
990.218683	92736.668476	34.438004
991.291132	92885.023057	34.443021
992.388273	93028.253860	34.448039
993.055188	93184.797950	34.453056
993.983345	93324.063998	34.458074
995.554673	93471.798282	34.463092
996.316215	93606.655442	34.468109
997.064119	93762.353233	34.473127
998.280468	93900.943009	34.478144
999.085263	94051.994234	34.483162
1000.109660	94198.182521	34.488180
1001.103927	94350.511094	34.493197
1002.034547	94487.944074	34.498215
1003.398813	94640.951318	34.503232
1003.952653	94787.013244	34.508250
1005.295643	94930.619989	34.513268
1005.877899	95079.150579	34.518285
1007.157572	95230.843022	34.523303
1008.085493	95387.915106	34.528320
1008.695701	95535.125205	34.533338
1010.048964	95684.463295	34.538356
1011.048101	95843.922265	34.543373
1012.309651	95990.690274	34.548391
1013.232876	96145.180978	34.553408
1014.438905	96300.338027	34.558426
1015.592327	96430.544606	34.563444
1016.410992	96581.086164	34.568461
1017.546786	96725.950497	34.573479
1018.535485	96874.147063	34.578496
1019.600869	97002.176767	34.583514
1020.099395	97142.541234	34.588532
1021.012739	97280.356772	34.593549
1021.989739	97413.320478	34.598567
1022.754835	97559.780532	34.603584
1023.752130	97720.491575	34.608602
1024.918221	97859.854645	34.613620
1026.399235	98017.753270	34.618637
1027.293315	98157.210935	34.623655
1028.212662	98314.032687	34.628672
1028.975396	98459.254897	34.633690
1030.438405	98611.125011	34.638708
1031.264280	98755.552699	34.643725
1032.417329	98903.910453	34.648743
1033.361052	99059.299510	34.653760
1034.257828	99209.765190	34.658778
1035.501427	99358.820794	34.663796
1036.384717	99519.520674	34.668813
1037.424233	99678.878435	34.673831
1038.407877	99829.675696	34.678848
1039.244516	99987.456688	34.683866
1040.483754	100137.999848	34.688884
1041.392159	100297.938997	34.693901
1042.233682	100465.318599	34.698919
1043.445011	100625.744401	34.703936
1044.633126	100795.657722	34.708954
1045.745682	100942.243565	34.713972
1046.505311	101107.585448	34.718989
1047.704283	101278.171515	34.724007
1049.281631	101435.437849	34.729024
1050.017590	101607.327902	34.734042
1051.381990	101762.524554	34.739060
1052.159300	101935.956605	34.744077
1053.568515	102085.784811	34.749095
1054.472363	102242.082780	34.754112
1055.557830	102406.873043	34.759130
1057.008600	102565.178876	34.764148
1057.894468	102732.119338	34.769165
1058.798107	102894.468152	34.774183
1060.092250	103055.374632	34.779200
1061.366319	103213.901407	34.784218
1062.366732	103364.953180	34.789236
1063.384061	103534.184650	34.794253
1064.102922	103693.979778	34.799271
1065.577072	103849.929764	34.804288
1066.649826	104017.506720	34.809306
1067.479135	104170.883852	34.814324
1068.274196	104329.161251	34.819341
1069.663078	104500.570989	34.824359
1071.178193	104659.776921	34.829376
1072.139830	104823.596829	34.834394
1073.237736	104982.210269	34.839412
1074.201736	105140.896136	34.844429
1075.090947	105292.303657	34.849447
1076.009572	105464.831646	34.854464
1077.153080	105631.568685	34.859482
1078.504456	105791.312770	34.864500
1079.577122	105957.504587	34.869517
1080.999429	106110.379242	34.874535
1081.773759	106271.991116	34.879552
1082.754835	106437.882612	34.884570
1084.120228	106597.615600	34.889588
1085.046558	106758.267645	34.894605
1085.801415	106909.437099	34.899623
1087.231942	107066.169534	34.904640
1087.939981	107237.927907	34.909658
1089.098248	107404.100661	34.914676
1090.147050	107561.846147	34.919693
1091.192917	107713.011609	34.924711
1092.340253	107872.721253	34.929728
1092.971989	108026.920183	34.934746
1094.229546	108184.990886	34.939764
1095.228595	108339.577525	34.944781
1096.067669	108491.324029	34.949799
1097.410945	108659.819796	34.954816
1098.580443	108833.745669	34.959834
1099.674885	108991.021307	34.964852
1100.234993	109159.578691	34.969869
1101.418749	109326.948672	34.974887
1102.967864	109492.626379	34.979904
1103.809667	109669.511699	34.984922
1104.964568	109828.011708	34.989940
1106.098933	110001.378215	34.994957
1106.964084	110178.021486	34.999975
1108.389544	110357.266400	35.004992
1109.290750	110528.021559	35.010010
1110.830251	110694.150272	35.015028
1111.722412	110875.713266	35.020045
1112.848844	111046.980974	35.025063
1114.202705	111223.362716	35.030080
1114.955003	111401.830562	35.035098
1115.939605	111556.319441	35.040116
1116.821219	111754.730166	35.045133
1118.009831	111933.246494	35.050151
1119.375022	112109.402556	35.055168
1120.598739	112304.148356	35.060186
1121.680734	112484.015742	35.065204
1122.724805	112664.942595	35.070221
1124.077591	112847.496098	35.075239
1125.122038	113027.701812	35.080256
1125.999504	113222.468723	35.085274
1127.425229	113398.482089	35.090292
1128.512093	113588.043688	35.095309
1129.037178	113766.660265	35.100327
1130.905840	113955.353102	35.105344
1131.941149	114141.450568	35.110362
1133.181458	114328.125666	35.115380
1134.251385	114521.537677	35.120397
1135.410401	114706.172784	35.125415
1136.594331	114890.437109	35.130432
1137.725739	115077.868683	35.135450
1138.753621	115262.565157	35.140468
1140.109239	115447.870777	35.145485
1140.978361	115650.883343	35.150503
1142.192740	115831.507468	35.155520
1143.372709	116025.075006	35.160538
1144.282721	116218.571660	35.165556
1145.867739	116408.640539	35.170573
1146.847725	116601.088165	35.175591
1148.141605	116782.300581	35.180608
1149.165158	116987.389060	35.185626
1150.344669	117174.658768	35.190644
1151.895989	117361.718994	35.195661
1153.081369	117551.906964	35.200679
1154.356592	117739.139125	35.205696
1155.144507	117933.158402	35.210714
1156.081908	118113.710031	35.215732
1157.583397	118300.351438	35.220749
1158.372797	118487.561875	35.225767
1159.592132	118682.164336	35.230784
1160.664860	118881.483982	35.235802
1162.316953	119064.541227	35.240820
1163.414731	119252.493574	35.245837
1164.458901	119445.338814	35.250855
1165.709693	119623.121320	35.255872
1166.945959	119819.654977	35.260890
1168.093605	119985.328682	35.265908
1169.217355	120162.689596	35.270925
1170.228114	120348.897715	35.275943
1171.289384	120526.117854	35.280960
1172.125728	120696.968069	35.285978
1173.421135	120881.091888	35.290996
1174.803426	121060.890023	35.296013
1175.594530	121253.454064	35.301031
1177.071901	121425.881568	35.306048
1178.003826	121617.194882	35.311066
1178.952016	121817.272191	35.316084
1180.484507	122009.381375	35.321101
1181.334978	122197.221759	35.326119
1182.283490	122383.360506	35.331136
1183.401488	122587.461838	35.336154
1184.560700	122793.435255	35.341172
1186.069190	122990.639934	35.346189
1187.080967	123193.505118	35.351207
1188.397345	123389.232230	35.356224
1189.276345	123598.793044	35.361242
1190.781350	123801.330383	35.366260
1191.823510	124004.550133	35.371277
1192.939558	124219.126145	35.376295
1194.462088	124421.080300	35.381312
1195.543014	124625.514992	35.386330
1196.834988	124830.184093	35.391348
1198.062777	125040.674655	35.396365
1199.169541	125250.246455	35.401383
1200.454067	125452.661664	35.406400
1201.328817	125663.109220	35.411418
1202.700237	125876.271178	35.416436
1204.082289	126083.241449	35.421453
1205.004036	126304.671667	35.426471
1206.438733	126510.468662	35.431488
1207.486870	126727.732759	35.436506
1208.965153	126943.598526	35.441524
1210.539503	127148.425314	35.446541
1211.396383	127365.900319	35.451559
1213.313609	127576.181760	35.456576
1214.264357	127778.419585	35.461594
1215.968145	127988.114840	35.466612
1217.090570	128203.586107	35.471629
1217.953783	128402.440429	35.476647
1219.613795	128615.888477	35.481664
1220.936232	128825.368488	35.486682
1221.917218	129036.463570	35.491700
1223.503230	129236.261750	35.496717
1224.578814	129442.713037	35.501735
1225.771292	129637.334664	35.506752
1226.719395	129837.260906	35.511770
1228.210843	130046.048028	35.516788
1229.472219	130260.353405	35.521805
1230.577186	130470.053193	35.526823
1231.846276	130668.105985	35.531840
1232.881009	130875.928215	35.536858
1234.272022	131084.812240	35.541876
1235.729748	131285.896209	35.546893
1236.675625	131498.988304	35.551911
1238.456073	131705.060982	35.556928
1239.345283	131911.502543	35.561946
1240.461434	132123.911241	35.566964
1241.839616	132321.586539	35.571981
1242.958326	132537.943004	35.576999
1244.560095	132741.878779	35.582016
1245.715662	132962.418845	35.587034
1246.690912	133159.463102	35.592052
1248.012929	133361.161540	35.597069
1249.036804	133567.665930	35.602087
1250.489461	133758.915395	35.607104
1251.542431	133954.149175	35.612122
1252.540888	134151.308402	35.617140
1253.708085	134357.730572	35.622157
1254.567135	134558.834378	35.627175
1255.962519	134755.451937	35.632192
1257.223375	134963.029646	35.637210
1258.585049	135173.333443	35.642228
1259.943607	135383.867118	35.647245
1261.230074	135588.893106	35.652263
1262.542604	135790.426301	35.657280
1263.579236	136004.287161	35.662298
1264.854290	136221.867857	35.667316
1266.309539	136431.426823	35.672333
1267.344930	136656.419859	35.677351
1268.219352	136861.338400	35.682368
1269.637028	137081.565723	35.687386
1270.624970	137307.280001	35.692404
1272.384809	137516.961196	35.697421
1273.713378	137752.839831	35.702439
1274.712926	137975.179963	35.707456
1275.881422	138199.956617	35.712474
1277.209585	138419.062166	35.717492
1278.937594	138643.918341	35.722509
1279.867228	138872.771150	35.727527
1281.326631	139100.945688	35.732544
1283.151948	139317.997880	35.737562
1284.216545	139555.779713	35.742580
1285.682860	139766.760585	35.747597
1286.492333	140002.807892	35.752615
1288.098711	140227.144919	35.757632
1289.607416	140452.805444	35.762650
1290.742442	140674.159847	35.767668
1292.255836	140901.674619	35.772685
1293.824161	141131.225122	35.777703
1294.908856	141351.321404	35.782720
1295.946069	141576.033005	35.787738
1297.443147	141799.264933	35.792756
1299.164296	142024.468029	35.797773
1300.324708	142250.254899	35.802791
1301.115946	142467.406995	35.807808
1302.687175	142702.929387	35.812826
1303.883450	142931.048991	35.817844
1305.214618	143151.888959	35.822861
1306.810041	143385.570538	35.827879
1307.748296	143616.855822	35.832896
1309.471647	143842.587220	35.837914
1310.861855	144079.692868	35.842932
1312.143842	144295.722713	35.847949
1313.346637	144523.417054	35.852967
1314.690890	144754.377498	35.857984
1316.286039	144980.603674	35.863002
1317.502070	145211.573580	35.868020
1318.935087	145424.297354	35.873037
1320.100331	145657.472970	35.878055
1321.648004	145886.223653	35.883072
1323.243629	146112.911695	35.888090
1324.427976	146332.900087	35.893108
1325.786946	146553.534780	35.898125
1327.092594	146775.828781	35.903143
1328.461631	146999.179983	35.908160
1329.771927	147219.533197	35.913178
1330.839086	147446.322485	35.918196
1332.732067	147668.934523	35.923213
1333.689406	147897.202609	35.928231
1335.184957	148124.993961	35.933248
1336.490810	148339.272723	35.938266
1337.661900	148558.840997	35.943284
1339.425714	148770.511237	35.948301
1340.276399	148981.906381	35.953319
1341.357241	149171.992790	35.958336
1343.040888	149380.948994	35.963354
1344.268472	149599.522642	35.968372
1345.895995	149812.322638	35.973389
1346.751143	150031.210196	35.978407
1348.290324	150242.553296	35.983424
1350.127230	150445.549171	35.988442
1350.983241	150664.045650	35.993460
1352.091968	150881.995708	35.998477
1353.572890	151099.329859	36.003495
1354.865601	151327.255360	36.008512
1356.117622	151537.150573	36.013530
1357.257243	151763.108942	36.018548
1358.487552	151989.345991	36.023565
1359.662559	152216.874686	36.028583
1361.144959	152454.625479	36.033600
1362.621357	152682.883216	36.038618
1363.775075	152930.233253	36.043636
1365.077301	153155.638654	36.048653
1366.344102	153391.218404	36.053671
1367.710584	153634.933120	36.058688
1369.089625	153877.656773	36.063706
1370.359724	154129.944531	36.068724
1371.825078	154359.784824	36.073741
1373.168002	154602.060207	36.078759
1374.319248	154855.359905	36.083776
1376.076243	155108.083509	36.088794
1377.483328	155362.437094	36.093812
1378.799068	155597.180386	36.098829
1380.318204	155854.768368	36.103847
1381.739537	156092.746923	36.108864
1383.082289	156348.435095	36.113882
1384.361264	156599.538867	36.118900
1386.166109	156845.877020	36.123917
1387.444033	157093.530066	36.128935
1389.071107	157352.364450	36.133952
1390.397042	157597.460393	36.138970
1391.731698	157852.254933	36.143988
1393.305006	158095.574967	36.149005
1394.751316	158350.112918	36.154023
1396.125430	158600.968948	36.159040
1397.683103	158841.196794	36.164058
1398.851461	159105.378957	36.169076
1399.962029	159346.960980	36.174093
1401.212630	159603.400968	36.179111
1402.455538	159846.830440	36.184128
1404.012672	160105.471603	36.189146
1405.520254	160374.125643	36.194164
1406.796042	160622.466144	36.199181
1408.213554	160881.868699	36.204199
1410.184990	161153.297269	36.209216
1411.759274	161403.181067	36.214234
1412.727919	161672.166187	36.219252
1414.664445	161918.364311	36.224269
1416.030760	162176.523255	36.229287
1417.393395	162448.954008	36.234304
1418.744948	162695.779884	36.239322
1420.081785	162954.403589	36.244340
1421.796655	163212.207383	36.249357
1423.609278	163459.255981	36.254375
1424.789268	163713.450890	36.259392
1426.540652	163961.183846	36.264410
1427.539107	164212.488953	36.269428
1429.160988	164456.193914	36.274445
1430.041786	164710.325187	36.279463
1431.709788	164956.564014	36.284480
1433.123979	165192.445082	36.289498
1434.256097	165436.585742	36.294516
1435.956263	165669.389245	36.299533
1437.535901	165903.431275	36.304551
1438.813777	166147.208849	36.309568
1440.242361	166378.101984	36.314586
1441.230137	166616.911442	36.319604
1442.393779	166864.429553	36.324621
1444.108825	167119.734245	36.329639
1445.573824	167375.637665	36.334656
1447.040305	167620.419314	36.339674
1448.422629	167879.372054	36.344692
1449.904076	168132.596585	36.349709
1451.541296	168379.195185	36.354727
1452.588828	168632.984587	36.359744
1454.552620	168898.731813	36.364762
1455.744056	169158.023778	36.369780
1457.168757	169415.908860	36.374797
1458.937937	169666.592389	36.379815
1460.121845	169926.789765	36.384832
1461.265028	170187.921339	36.389850
1462.789340	170451.673326	36.394868
1464.106391	170719.547257	36.399885
1465.510316	170985.961039	36.404903
1467.175776	171252.169764	36.409920
1468.615299	171517.208522	36.414938
1469.812585	171794.285351	36.419956
1471.408337	172073.370537	36.424973
1473.102349	172350.206565	36.429991
1474.536703	172629.128564	36.435008
1476.008317	172894.281338	36.440026
1477.515880	173174.565197	36.445044
1478.849131	173450.318805	36.450061
1480.772085	173730.704707	36.455079
1482.284868	174000.629190	36.460096
1484.130256	174279.010194	36.465114
1485.077482	174577.036947	36.470132
1486.750182	174841.631452	36.475149
1488.704185	175115.655604	36.480167
1490.108123	175389.766772	36.485184
1491.481641	175667.883560	36.490202
1492.959224	175954.124588	36.495220
1494.676693	176226.246637	36.500237
1496.395935	176497.010575	36.505255
1497.763021	176775.170177	36.510272
1499.439553	177048.279083	36.515290
1500.796407	177331.445302	36.520308
1502.239615	177596.135306	36.525325
1503.923501	177879.175966	36.530343
1505.611725	178161.327976	36.535360
1506.609744	178432.541117	36.540378
1507.759184	178703.325044	36.545396
1509.635329	178983.189939	36.550413
1511.015382	179257.596710	36.555431
1512.573418	179547.824571	36.560448
1514.295891	179824.109713	36.565466
1515.957835	180102.589387	36.570484
1517.348549	180383.347378	36.575501
1519.009842	180657.587421	36.580519
1520.362605	180936.752987	36.585536
1522.039608	181226.586635	36.590554
1523.849193	181509.771524	36.595572
1525.425426	181786.237870	36.600589
1527.117012	182053.035627	36.605607
1528.647242	182335.403189	36.610624
1530.103358	182601.883768	36.615642
1531.548863	182871.516166	36.620660
1532.981558	183138.357480	36.625677
1534.901411	183402.431029	36.630695
1536.110375	183656.228481	36.635712
1537.609617	183908.101650	36.640730
1538.981806	184166.370455	36.645748
1540.315229	184423.782437	36.650765
1541.799915	184679.850661	36.655783
1543.058229	184951.803965	36.660800
1544.588503	185273.573894	36.665818
1546.236065	185563.729883	36.670836
1547.493592	185843.356242	36.675853
1549.297101	186110.782428	36.680871
1550.388280	186394.398599	36.685888
1552.187173	186656.467631	36.690906
1553.719521	186937.196878	36.695924
1555.260398	187218.992313	36.700941
1556.492722	187506.500903	36.705959
1557.975537	187790.288094	36.710976
1559.632412	188079.306539	36.715994
1561.516895	188367.731327	36.721012
1562.978371	188661.963453	36.726029
1564.811829	188933.582948	36.731047
1566.112296	189232.312170	36.736064
1567.698949	189525.333163	36.741082
1569.206385	189819.103911	36.746100
1571.007830	190122.989495	36.751117
1572.599239	190406.156688	36.756135
1573.893890	190711.037531	36.761152
1575.151445	191020.319244	36.766170
1577.092990	191310.012521	36.771188
1578.262174	191603.027846	36.776205
1580.048717	191906.310716	36.781223
1581.798334	192216.255100	36.786240
1583.369295	192509.489123	36.791258
1585.203951	192817.923056	36.796276
1586.739094	193124.245546	36.801293
1588.804809	193430.028521	36.806311
1590.260737	193743.146945	36.811328
1592.082135	194031.265088	36.816346
1593.638679	194330.678010	36.821364
1595.025960	194636.366790	36.826381
1597.049307	194938.298948	36.831399
1598.204548	195251.290199	36.836416
1599.911886	195551.342683	36.841434
1601.418352	195846.753402	36.846452
1603.306272	196156.355268	36.851469
1605.158763	196454.964508	36.856487
1606.719381	196763.704478	36.861504
1608.574486	197070.519305	36.866522
1609.977674	197371.359910	36.871540
1611.360549	197674.058638	36.876557
1613.163882	197988.834233	36.881575
1614.575827	198291.199443	36.886592
1615.977689	198584.447562	36.891610
1618.283362	198898.485984	36.896628
1619.380464	199197.879429	36.901645
1620.977215	199505.730332	36.906663
1622.548327	199819.631539	36.911680
1624.357840	200127.450345	36.916698
1626.182570	200437.629756	36.921716
1627.834287	200740.851217	36.926733
1629.550291	201040.100416	36.931751
1631.085972	201346.999061	36.936768
1632.824603	201659.251795	36.941786
1634.600141	201963.675378	36.946804
1635.784157	202269.208159	36.951821
1637.618387	202580.888721	36.956839
1639.113624	202877.864004	36.961856
1640.660284	203180.648911	36.966874
1642.582966	203465.110989	36.971892
1644.035105	203766.031849	36.976909
1646.148228	204046.883227	36.981927
1647.739832	204340.517996	36.986944
1649.276086	204623.314888	36.991962
1650.776446	204917.574465	36.996980
1652.386318	205206.228711	37.001997
1653.920875	205489.484341	37.007015
1655.094163	205788.724521	37.012032
1656.602007	206078.462875	37.017050
1658.328990	206380.462371	37.022068
1659.807741	206691.798640	37.027085
1661.789129	206987.738650	37.032103
1663.100135	207303.522161	37.037120
1664.630209	207614.902491	37.042138
1666.776940	207924.738756	37.047156
1668.011787	208233.829022	37.052173
1670.004031	208547.043496	37.057191
1671.496567	208870.243842	37.062208
1672.737267	209196.583219	37.067226
1674.588947	209511.218084	37.072244
1676.325331	209838.319015	37.077261
1678.277004	210157.841855	37.082279
1680.023361	210492.664652	37.087296
1681.414465	210811.513879	37.092314
1683.106638	211144.821731	37.097332
1684.484811	211472.336302	37.102349
1686.586880	211804.285181	37.107367
1688.131651	212139.293852	37.112384
1689.693957	212483.674061	37.117402
1691.716691	212800.216446	37.122420
1693.291205	213144.392219	37.127437
1695.324174	213480.646868	37.132455
1697.044144	213814.689899	37.137472
1698.717456	214146.352595	37.142490
1700.683066	214477.309352	37.147508
1702.194421	214821.623647	37.152525
1704.154701	215156.849652	37.157543
1705.755716	215494.393096	37.162560
1707.430442	215828.140108	37.167578
1709.396400	216163.340629	37.172596
1710.784675	216512.908766	37.177613
1712.895544	216841.685337	37.182631
1714.792051	217178.345477	37.187648
1716.584592	217509.509464	37.192666
1718.151072	217839.591264	37.197684
1720.225142	218184.353513	37.202701
1721.768733	218514.998177	37.207719
1723.609091	218848.568844	37.212736
1725.395326	219186.060367	37.217754
1726.879406	219515.495473	37.222772
1728.552210	219859.965768	37.227789
1730.380710	220202.303322	37.232807
1732.247788	220533.508025	37.237824
1734.192612	220864.522861	37.242842
1735.962078	221188.756974	37.247860
1737.636727	221524.107597	37.252877
1739.370039	221860.770154	37.257895
1741.114393	222198.244007	37.262912
1742.773470	222539.389475	37.267930
1744.524162	222859.511519	37.272948
1746.330879	223204.343021	37.277965
1748.110553	223531.268938	37.282983
1749.523349	223865.644901	37.288000
1751.214441	224205.896503	37.293018
1753.438894	224540.526582	37.298036
1754.898392	224883.380288	37.303053
1757.043805	225206.667139	37.308071
1758.826645	225514.107770	37.313088
1760.157535	225839.935465	37.318106
1762.148755	226141.322699	37.323124
1763.433403	226458.748843	37.328141
1765.314643	226781.314839	37.333159
1767.029340	227096.234827	37.338176
1768.514847	227423.968884	37.343194
1770.184286	227745.780358	37.348212
1772.140724	228071.662316	37.353229
1773.660075	228403.836592	37.358247
1775.379230	228742.787802	37.363264
1776.898351	229084.539257	37.368282
1778.975828	229408.344194	37.373300
1780.603417	229756.251631	37.378317
1782.165565	230093.575702	37.383335
1783.411838	230440.602589	37.388352
1785.536955	230783.173120	37.393370
1787.453836	231129.840714	37.398388
1789.069164	231491.645280	37.403405
1790.910273	231844.980203	37.408423
1792.812781	232199.804150	37.413440
1794.961201	232557.688680	37.418458
1796.894183	232914.641345	37.423476
1798.703276	233277.811706	37.428493
1800.536024	233630.384694	37.433511
1801.794017	233984.876442	37.438528
1803.914399	234344.262932	37.443546
1806.058970	234702.349756	37.448564
1807.798776	235072.261575	37.453581
1809.730774	235425.859178	37.458599
1811.264067	235779.569667	37.463616
1813.075466	236151.806433	37.468634
1815.127780	236515.139243	37.473652
1817.000699	236880.481246	37.478669
1818.614735	237241.112899	37.483687
1820.458018	237610.574159	37.488704
1822.517088	237991.636081	37.493722
1824.338257	238350.176422	37.498740
1825.955428	238725.819440	37.503757
1827.830559	239094.308650	37.508775
1830.082794	239468.073117	37.513792
1831.543958	239837.388268	37.518810
1833.599045	240193.882895	37.523828
1835.859359	240578.390253	37.528845
1837.910670	240950.736166	37.533863
1839.424377	241312.623305	37.538880
1840.973090	241681.337927	37.543898
1843.382737	242056.064862	37.548916
1845.036143	242422.602717	37.553933
1846.695291	242785.023801	37.558951
1848.623554	243157.309417	37.563968
1850.555745	243535.588930	37.568986
1852.407776	243904.201801	37.574004
1854.559858	244275.637636	37.579021
1856.388311	244634.523620	37.584039
1858.137872	245010.111027	37.589056
1859.716701	245388.417167	37.594074
1861.958867	245752.494859	37.599092
1863.828524	246128.391641	37.604109
1865.965869	246500.664035	37.609127
1867.708309	246866.087984	37.614144
1869.576494	247240.306248	37.619162
1871.422550	247604.442414	37.624180
1873.381028	247968.636472	37.629197
1874.888210	248343.340806	37.634215
1876.774884	248713.539551	37.639232
1878.830836	249075.404461	37.644250
1880.499240	249443.705218	37.649268
1882.223141	249810.243735	37.654285
1884.123004	250156.381380	37.659303
1886.257294	250497.274182	37.664320
1887.884929	250861.361409	37.669338
1889.802185	251205.207903	37.674356
1891.763324	251566.218489	37.679373
1893.290586	251918.354663	37.684391
1895.155108	252270.665873	37.689408
1896.689507	252646.143515	37.694426
1898.595329	253006.575097	37.699444
1900.840142	253368.070425	37.704461
1902.461021	253746.376710	37.709479
1904.581629	254111.191813	37.714496
1905.974325	254482.317822	37.719514
1908.165369	254857.864772	37.724532
1910.203116	255236.584445	37.729549
1911.979874	255617.579210	37.734567
1913.803022	256005.119133	37.739584
1915.406721	256386.087983	37.744602
1917.462065	256769.067939	37.749620
1919.398008	257151.735235	37.754637
1921.528916	257546.004468	37.759655
1923.581159	257933.172565	37.764672
1925.232238	258343.466055	37.769690
1927.178251	258728.616240	37.774708
1929.349740	259131.281688	37.779725
1931.014631	259526.582730	37.784743
1933.333834	259922.313489	37.789760
1934.996492	260327.772346	37.794778
1936.946795	260718.376482	37.799796
1939.338007	261127.401569	37.804813
1941.076174	261536.095565	37.809831
1943.313701	261928.784205	37.814848
1945.123029	262329.945797	37.819866
1947.531894	262726.338571	37.824884
1949.453525	263125.777895	37.829901
1951.325824	263529.363582	37.834919
1953.232219	263920.928473	37.839936
1955.449279	264332.838975	37.844954
1957.166964	264734.463097	37.849972
1959.365850	265135.324592	37.854989
1961.182008	265540.003458	37.860007
1963.434074	265934.351332	37.865024
1965.741865	266346.417328	37.870042
1967.498459	266735.201020	37.875060
1969.189025	267143.804443	37.880077
1971.221446	267550.142993	37.885095
1973.585154	267949.037058	37.890112
1975.191911	268351.349674	37.895130
1977.225904	268750.368163	37.900148
1979.203778	269154.143180	37.905165
1981.273628	269565.750029	37.910183
1983.347720	269974.535213	37.915200
1984.923225	270382.533051	37.920218
1987.529872	270792.551912	37.925236
1989.577835	271195.875171	37.930253
1991.713384	271600.274983	37.935271
1993.610268	271998.360957	37.940288
1995.902131	272402.046888	37.945306
1997.601577	272808.998258	37.950324
1999.984259	273205.199482	37.955341
2001.595836	273596.643321	37.960359
2003.614814	273999.094563	37.965376
2005.747110	274399.545209	37.970394
2007.633725	274801.632340	37.975412
2010.115764	275189.427798	37.980429
2011.871346	275597.550460	37.985447
2013.958273	275979.664428	37.990464
2015.749959	276364.895687	37.995482
2017.850488	276740.629512	38.000500
2019.365034	277120.008640	38.005517
2021.192352	277497.584706	38.010535
2023.546845	277867.000704	38.015552
2025.365152	278257.932512	38.020570
2027.313326	278642.721768	38.025588
2029.468637	279038.752101	38.030605
2031.148824	279434.778518	38.035623
2033.394313	279811.668285	38.040640
2034.935806	280207.407588	38.045658
2037.197782	280611.463050	38.050676
2039.399467	281000.085922	38.055693
2041.207600	281413.426156	38.060711
2043.281642	281814.228519	38.065728
2045.537234	282212.257698	38.070746
2047.359056	282626.426842	38.075764
2049.370150	283031.447621	38.080781
2051.487821	283450.593614	38.085799
2053.398108	283851.257755	38.090816
2055.441251	284269.648693	38.095834
2057.041481	284684.830684	38.100852
2059.213465	285117.797347	38.105869
2061.207292	285548.986245	38.110887
2063.571607	285969.805025	38.115904
2065.558535	286402.360747	38.120922
2067.815570	286830.910207	38.125940
2069.912882	287264.433349	38.130957
2071.417764	287701.220318	38.135975
2074.058136	288125.816398	38.140992
2075.848619	288562.222815	38.146010
2077.822121	289013.705555	38.151028
2080.168816	289441.258927	38.156045
2082.258006	289884.846103	38.161063
2084.415825	290327.759261	38.166080
2086.687001	290771.717966	38.171098
2088.498095	291223.337262	38.176116
2090.819209	291661.289617	38.181133
2092.888458	292113.471370	38.186151
2094.998707	292562.342658	38.191168
2097.699874	292995.681163	38.196186
2099.794169	293443.735922	38.201204
2101.993995	293883.874699	38.206221
2103.673118	294344.377690	38.211239
2106.253394	294780.362614	38.216256
2108.372289	295221.773532	38.221274
2110.488682	295663.917769	38.226292
2112.489690	296110.011898	38.231309
2114.782428	296553.061111	38.236327
2116.684290	296998.326031	38.241344
2119.101528	297438.378481	38.246362
2121.129058	297886.079390	38.251380
2123.497244	298327.554277	38.256397
2125.361205	298779.234079	38.261415
2127.202683	299223.627632	38.266432
2129.617480	299679.656639	38.271450
2131.338558	300121.624629	38.276468
2134.026464	300576.968751	38.281485
2135.981646	301027.524132	38.286503
2138.111307	301477.515338	38.291520
2139.958618	301924.348320	38.296538
2142.154418	302381.328035	38.301556
2144.706770	302832.358613	38.306573
2146.795001	303286.326451	38.311591
2149.099014	303734.519592	38.316608
2151.077046	304182.074477	38.321626
2153.104632	304642.081516	38.326644
2155.685646	305082.350434	38.331661
2157.305252	305514.693834	38.336679
2159.343337	305936.560712	38.341696
2161.830085	306364.547482	38.346714
2163.613511	306791.396850	38.351732
2165.852168	307212.967801	38.356749
2167.585754	307647.508746	38.361767
2169.974457	308079.455876	38.366784
2172.417718	308513.878166	38.371802
2174.334404	308943.734018	38.376820
2176.488090	309392.001768	38.381837
2178.194077	309830.081147	38.386855
2180.367657	310271.509910	38.391872
2182.529575	310719.890928	38.396890
2184.208489	311180.678520	38.401908
2186.745449	311642.088828	38.406925
2188.838207	312097.092054	38.411943
2191.117021	312555.716536	38.416960
2193.365879	313025.026233	38.421978
2195.380682	313491.702916	38.426996
2197.552200	313966.649500	38.432013
2200.075723	314443.642590	38.437031
2202.175907	314901.840268	38.442048
2204.176013	315374.337264	38.447066
2206.353850	315854.592736	38.452084
2209.022902	316339.968781	38.457101
2210.689464	316822.958588	38.462119
2213.074490	317297.582994	38.467136
2215.793031	317779.737996	38.472154
2217.719920	318278.785876	38.477172
2220.012999	318755.895908	38.482189
2222.275292	319242.750150	38.487207
2224.485661	319727.145543	38.492224
2226.636258	320222.177404	38.497242
2228.728871	320713.888402	38.502260
2231.123761	321206.028581	38.507277
2233.532436	321719.095394	38.512295
2235.701063	322201.210844	38.517312
2238.200557	322702.274543	38.522330
2240.433893	323199.085624	38.527348
2242.844067	323699.466206	38.532365
2245.402191	324197.204106	38.537383
2247.716631	324685.941204	38.542400
2250.347245	325182.412526	38.547418
2252.276670	325665.057870	38.552436
2254.769168	326145.554219	38.557453
2256.890781	326659.086609	38.562471
2259.130091	327144.862663	38.567488
2261.930032	327636.887979	38.572506
2264.069287	328133.044577	38.577524
2266.359927	328620.570557	38.582541
2268.375044	329115.998468	38.587559
2271.255524	329603.369242	38.592576
2273.990094	330088.118282	38.597594
2275.525044	330578.275065	38.602612
2277.824656	331067.621045	38.607629
2280.133527	331558.405383	38.612647
2282.585553	332047.537445	38.617664
2285.173031	332526.646938	38.622682
2286.986854	333020.686295	38.627700
2289.608370	333507.109393	38.632717
2291.785854	333994.965492	38.637735
2293.908411	334478.105570	38.642752
2296.738023	334964.654740	38.647770
2298.794870	335457.355593	38.652788
2301.061882	335941.138910	38.657805
2303.242731	336420.820107	38.662823
2304.992633	336915.046019	38.667840
2307.590393	337385.061254	38.672858
2309.919225	337857.471381	38.677876
2311.847107	338315.556490	38.682893
2314.059815	338794.947688	38.687911
2316.195025	339266.735504	38.692928
2318.497391	339732.175473	38.697946
2320.379818	340216.037827	38.702964
2322.808849	340684.793391	38.707981
2325.127856	341174.230190	38.712999
2327.711925	341665.292587	38.718016
2330.064668	342151.413403	38.723034
2332.230194	342639.534889	38.728052
2334.783625	343133.675424	38.733069
2336.855400	343620.352163	38.738087
2339.156824	344118.068463	38.743104
2341.466213	344610.729686	38.748122
2343.635172	345121.689869	38.753140
2345.764963	345617.154137	38.758157
2348.169190	346118.476773	38.763175
2350.319550	346636.948466	38.768192
2353.293624	347144.430127	38.773210
2355.198637	347666.956125	38.778228
2357.468552	348171.489384	38.783245
2359.612826	348692.415015	38.788263
2361.961086	349219.943842	38.793280
2364.836705	349738.659278	38.798298
2366.858025	350289.752234	38.803316
2369.195256	350815.735686	38.808333
2371.798680	351349.427465	38.813351
2374.094235	351880.572440	38.818368
2376.442235	352415.503491	38.823386
2378.794681	352966.270727	38.828404
2381.566815	353498.201645	38.833421
2383.779901	354039.185858	38.838439
2386.265190	354579.788644	38.843456
2388.890085	355122.109555	38.848474
2391.261116	355672.395687	38.853492
2393.656869	356211.387174	38.858509
2396.487907	356748.881598	38.863527
2398.284496	357303.994508	38.868544
2400.947199	357840.735739	38.873562
2403.306584	358398.630663	38.878580
2405.873198	358942.034358	38.883597
2408.415056	359497.371117	38.888615
2410.768985	360051.231578	38.893632
2413.748653	360592.386493	38.898650
2415.621600	361151.396696	38.903668
2417.933536	361697.249180	38.908685
2420.574876	362253.938769	38.913703
2423.052885	362807.551342	38.918720
2425.847471	363346.606839	38.923738
2428.142759	363910.010346	38.928756
2430.640274	364455.123882	38.933773
2433.312649	365008.994003	38.938791
2435.551317	365561.172754	38.943808
2438.335246	366108.516671	38.948826
2440.455840	366664.088683	38.953844
2442.422489	367214.200299	38.958861
2445.214398	367766.579634	38.963879
2447.643412	368322.780737	38.968896
2450.766359	368873.845103	38.973914
2452.984030	369427.776977	38.978932
2455.398120	369975.079126	38.983949
2458.133126	370523.055215	38.988967
2460.355032	371076.497784	38.993984
2462.951087	371621.129433	38.999002
2465.029710	372176.396800	39.004020
2467.628199	372724.958903	39.009037
2470.301178	373264.022804	39.014055
2472.691170	373791.592772	39.019072
2474.968736	374312.887084	39.024090
2477.394311	374836.960385	39.029108
2479.431132	375354.953559	39.034125
2482.308739	375873.919970	39.039143
2484.286822	376403.859582	39.044160
2487.123135	376935.427768	39.049178
2489.486491	377466.502063	39.054196
2492.013024	377999.490774	39.059213
2494.298913	378537.547283	39.064231
2496.106276	379080.125853	39.069248
2498.738253	379609.392745	39.074266
2500.821099	380178.729927	39.079284
2503.413533	380739.591195	39.084301
2506.082181	381292.728694	39.089319
2508.627187	381855.067722	39.094336
2511.072530	382413.281800	39.099354
2513.346570	382997.191774	39.104372
2516.029298	383562.308633	39.109389
2518.645358	384142.188198	39.114407
2521.032588	384712.112373	39.119424
2524.197146	385288.182625	39.124442
2526.228854	385875.534085	39.129460
2528.503885	386459.592462	39.134477
2531.015054	387041.751795	39.139495
2533.533704	387631.543667	39.144512
2535.855457	388226.290068	39.149530
2539.003659	388827.805549	39.154548
2541.427026	389429.090635	39.159565
2544.008735	390022.993652	39.164583
2546.255560	390630.151174	39.169600
2549.537988	391225.181455	39.174618
2552.020946	391833.183642	39.179636
2554.521502	392440.712175	39.184653
2556.665366	393036.635733	39.189671
2559.444543	393647.533412	39.194688
2562.101954	394260.358573	39.199706
2564.563075	394871.679900	39.204724
2567.112289	395486.211971	39.209741
2570.209855	396096.541676	39.214759
2572.833633	396720.649142	39.219776
2575.444680	397326.112605	39.224794
2578.261058	397944.639569	39.229812
2580.625640	398554.564688	39.234829
2583.509219	399166.215025	39.239847
2585.857933	399782.893548	39.244864
2588.709684	400395.123941	39.249882
2591.403115	401011.310904	39.254900
2594.103674	401618.521533	39.259917
2596.987335	402237.379060	39.264935
2598.950598	402854.187497	39.269952
2601.909103	403464.750359	39.274970
2604.686564	404077.045823	39.279988
2607.076181	404686.146501	39.285005
2610.155529	405303.978930	39.290023
2612.724910	405915.902774	39.295040
2615.388214	406528.959089	39.300058
2618.044010	407152.777957	39.305076
2620.743110	407762.859812	39.310093
2623.591851	408371.838889	39.315111
2626.094326	408981.917889	39.320128
2628.959032	409579.071852	39.325146
2631.563376	410187.482374	39.330164
2634.072222	410793.715385	39.335181
2636.886485	411398.416596	39.340199
2639.059016	412004.061385	39.345216
2641.866294	412609.893501	39.350234
2644.487271	413200.156660	39.355252
2646.754185	413790.560172	39.360269
2649.532284	414354.462002	39.365287
2652.359405	414938.271340	39.370304
2654.677815	415522.093664	39.375322
2657.193909	416091.959226	39.380340
2659.546638	416688.743418	39.385357
2662.110198	417261.756554	39.390375
2664.481844	417863.309479	39.395392
2667.357450	418437.303872	39.400410
2670.048411	419046.106339	39.405428
2672.331068	419655.966338	39.410445
2674.965892	420254.981733	39.415463
2677.819234	420865.172084	39.420480
2680.359685	421468.465512	39.425498
2682.723311	422083.955469	39.430516
2685.090660	422713.736298	39.435533
2688.428553	423324.283512	39.440551
2690.804777	423967.676434	39.445568
2693.349622	424595.500595	39.450586
2695.954168	425232.295428	39.455604
2698.878680	425865.531693	39.460621
2701.652493	426502.917160	39.465639
2704.372638	427159.299058	39.470656
2706.888049	427798.705859	39.475674
2709.964728	428440.936311	39.480692
2712.417217	429089.309502	39.485709
2715.138920	429744.645446	39.490727
2718.011586	430404.181859	39.495744
2720.552350	431062.636098	39.500762
2723.732942	431717.733459	39.505780
2726.344331	432377.294906	39.510797
2729.238915	433034.111174	39.515815
2731.727647	433706.786819	39.520832
2734.871987	434383.632059	39.525850
2737.665345	435041.154070	39.530868
2740.627798	435714.342561	39.535885
2743.051775	436369.451311	39.540903
2745.426424	437046.979903	39.545920
2748.583824	437713.801928	39.550938
2751.441178	438388.579834	39.555956
2754.390509	439067.664260	39.560973
2757.029478	439733.687790	39.565991
2760.268868	440413.840277	39.571008
2763.308257	441090.008463	39.576026
2765.981408	441752.974329	39.581044
2768.822841	442427.205379	39.586061
2771.536362	443097.188924	39.591079
2774.384419	443772.228695	39.596096
2777.398933	444437.924181	39.601114
2780.173061	445098.835028	39.606132
2782.852404	445770.746889	39.611149
2786.144936	446437.487858	39.616167
2788.698870	447116.692659	39.621184
2791.641893	447775.813555	39.626202
2794.428786	448452.406917	39.631220
2797.277443	449127.854350	39.636237
2800.196228	449786.299638	39.641255
2802.973916	450445.146745	39.646272
2805.282296	451117.220793	39.651290
2808.273847	451777.853385	39.656308
2810.899424	452448.868272	39.661325
2813.971136	453124.583960	39.666343
2816.908719	453792.823414	39.671360
2819.718001	454461.007090	39.676378
2822.780793	455127.106556	39.681396
2825.560014	455800.947898	39.686413
2828.559304	456458.930311	39.691431
2831.028286	457113.235800	39.696448
2834.038737	457747.344611	39.701466
2836.933453	458385.738126	39.706484
2839.502960	459014.469209	39.711501
2842.083428	459632.628381	39.716519
2844.512231	460275.717876	39.721536
2847.711139	460909.882486	39.726554
2850.495296	461554.684875	39.731572
2852.921192	462184.734767	39.736589
2855.982204	462837.316562	39.741607
2858.610075	463487.821856	39.746624
2861.405772	464135.046907	39.751642
2864.091027	464791.547099	39.756660
2867.057827	465469.821480	39.761677
2869.590572	466133.910523	39.766695
2872.075810	466808.926852	39.771712
2874.842858	467484.376133	39.776730
2877.789886	468166.982622	39.781748
2880.627432	468853.461739	39.786765
2883.447568	469546.219418	39.791783
2886.405095	470237.615151	39.796800
2889.127499	470935.120652	39.801818
2892.331662	471634.992065	39.806836
2894.895274	472349.153930	39.811853
2897.982236	473044.999295	39.816871
2900.750418	473763.252154	39.821888
2903.397774	474473.323903	39.826906
2907.029668	475188.655516	39.831924
2910.027227	475924.876089	39.836941
2913.024066	476637.469483	39.841959
2916.221274	477360.787690	39.846976
2918.843871	478073.980293	39.851994
2921.970151	478797.899470	39.857012
2924.591264	479523.779865	39.862029
2927.775305	480248.681993	39.867047
2930.449796	480986.885447	39.872064
2933.212540	481719.647851	39.877082
2936.483775	482453.606653	39.882100
2939.353520	483198.226452	39.887117
2942.889212	483923.407077	39.892135
2945.733539	484667.859531	39.897152
2948.862835	485404.925698	39.902170
2951.814843	486146.871434	39.907188
2954.770171	486878.805498	39.912205
2957.851185	487618.140846	39.917223
2960.698356	488359.995721	39.922240
2964.078352	489099.665829	39.927258
2967.062372	489831.050657	39.932276
2969.892056	490576.930281	39.937293
2972.971816	491308.883388	39.942311
2976.120336	492051.870025	39.947328
2978.902218	492798.150633	39.952346
2982.131210	493536.669658	39.957364
2985.045894	494280.589313	39.962381
2988.192992	495019.903633	39.967399
2991.498778	495752.761748	39.972416
2994.295689	496499.861276	39.977434
2997.789310	497234.076584	39.982452
3000.690479	497970.814671	39.987469
3003.754294	498697.522879	39.992487
3006.328579	499434.439796	39.997504
3009.497005	500174.397703	40.002522
3012.618452	500902.497058	40.007540
3015.349982	501644.713324	40.012557
3018.649709	502365.513982	40.017575
3021.756868	503104.274845	40.022592
3024.367489	503847.201851	40.027610
3027.802294	504577.784038	40.032628
3030.679344	505314.252936	40.037645
3033.304051	506006.697650	40.042663
3036.559326	506711.990705	40.047680
3039.507448	507407.335322	40.052698
3042.253037	508100.564515	40.057716
3045.519216	508800.871893	40.062733
3048.065674	509505.230870	40.067751
3051.411152	510214.761387	40.072768
3054.182741	510933.650719	40.077786
3057.598204	511642.393687	40.082804
3060.079419	512354.264212	40.087821
3062.910904	513073.486387	40.092839
3065.967916	513801.184784	40.097856
3069.046691	514532.361375	40.102874
3071.676329	515264.725890	40.107892
3074.988544	515993.022899	40.112909
3078.064323	516740.925985	40.117927
3080.812725	517488.789084	40.122944
3083.741185	518246.637191	40.127962
3086.728081	518990.208084	40.132980
3089.570563	519761.255895	40.137997
3092.779989	520539.440165	40.143015
3096.245789	521311.407809	40.148032
3098.848004	522090.753379	40.153050
3102.235102	522870.081726	40.158068
3105.387866	523650.858584	40.163085
3108.252771	524441.081332	40.168103
3111.643083	525232.581854	40.173120
3114.447772	526030.507420	40.178138
3117.545665	526815.477933	40.183156
3121.345609	527623.802266	40.188173
3124.334044	528426.376845	40.193191
3127.450632	529237.722686	40.198208
3130.624428	530041.626006	40.203226
3133.558510	530841.147857	40.208244
3136.850633	531662.309924	40.213261
3139.951575	532468.033317	40.218279
3143.627630	533284.412591	40.223296
3146.641601	534096.626035	40.228314
3150.538837	534904.482894	40.233332
3153.428230	535719.324454	40.238349
3156.494862	536539.508140	40.243367
3160.059581	537340.285251	40.248384
3163.404196	538153.896236	40.253402
3166.166036	538954.897920	40.258420
3169.709880	539774.346520	40.263437
3173.032907	540582.836103	40.268455
3176.105694	541403.557247	40.273472
3179.479212	542219.059511	40.278490
3182.856083	543025.376226	40.283508
3186.417849	543836.578992	40.288525
3189.508040	544634.257064	40.293543
3193.136473	545436.665809	40.298560
3196.096016	546246.450844	40.303578
3199.298190	547041.247632	40.308596
3202.736575	547848.695789	40.313613
3205.152412	548643.311416	40.318631
3208.934437	549454.662527	40.323648
3211.894537	550259.519169	40.328666
3215.530668	551062.211280	40.333684
3219.033636	551863.667871	40.338701
3221.736888	552668.004141	40.343719
3225.315064	553471.398154	40.348736
3228.918020	554275.787500	40.353754
3232.092258	555070.265159	40.358772
3235.438925	555851.180270	40.363789
3238.567989	556659.744357	40.368807
3241.913732	557435.794773	40.373824
3244.677348	558211.384509	40.378842
3248.460488	558969.125661	40.383860
3251.528392	559717.911029	40.388877
3254.117509	560473.337464	40.393895
3257.575058	561217.607847	40.398912
3260.220254	561969.723175	40.403930
3263.775564	562720.395694	40.408948
3266.933648	563484.957241	40.413965
3269.467963	564255.676904	40.418983
3272.710727	565016.268183	40.424000
3275.753758	565797.373933	40.429018
3279.241885	566579.559347	40.434036
3282.056164	567379.323005	40.439053
3285.475082	568173.228730	40.444071
3288.482652	568970.047887	40.449088
3291.532723	569773.263275	40.454106
3294.811375	570581.993297	40.459124
3298.120244	571406.929584	40.464141
3301.226287	572232.438508	40.469159
3304.518799	573053.804397	40.474176
3307.522215	573885.665475	40.479194
3311.030581	574719.037810	40.484212
3314.437102	575557.968733	40.489229
3317.683133	576403.216522	40.494247
3320.854155	577255.116433	40.499264
3324.009444	578112.506910	40.504282
3327.609204	578966.360547	40.509300
3331.102279	579831.969792	40.514317
3334.052464	580698.146624	40.519335
3337.655168	581556.952185	40.524352
3341.375010	582439.926013	40.529370
3344.784988	583313.977042	40.534388
3348.157096	584187.364510	40.539405
3351.141136	585058.593297	40.544423
3354.902676	585933.530421	40.549440
3358.079671	586813.087528	40.554458
3361.625097	587699.563499	40.559476
3365.188254	588594.210746	40.564493
3368.535259	589472.476142	40.569511
3372.459873	590352.528621	40.574528
3375.407898	591247.901563	40.579546
3378.845569	592133.980218	40.584564
3382.635889	593012.536624	40.589581
3385.709505	593904.120834	40.594599
3389.178497	594783.630625	40.599616
3392.797043	595679.076785	40.604634
3396.174760	596568.292199	40.609652
3399.759128	597465.390455	40.614669
3402.862517	598355.447024	40.619687
3406.422590	599244.857584	40.624704
3410.016021	600139.030180	40.629722
3413.341175	601023.533684	40.634740
3416.727286	601914.142270	40.639757
3419.862603	602814.895838	40.644775
3423.497234	603713.347186	40.649792
3426.902454	604620.938582	40.654810
3430.316550	605531.792037	40.659828
3434.018465	606422.262920	40.664845
3437.343905	607326.235631	40.669863
3440.521246	608219.376502	40.674880
3444.237966	609128.516495	40.679898
3447.507028	610024.677476	40.684916
3450.985490	610932.895585	40.689933
3454.232949	611838.575105	40.694951
3457.822117	612742.325068	40.699968
3461.131983	613657.455426	40.704986
3464.622844	614568.386255	40.710004
3467.977175	615479.255788	40.715021
3471.451074	616369.437965	40.720026
3474.859902	617221.603940	40.725031
3478.078428	618041.799607	40.730036
3481.182295	618805.240482	40.735040
3484.372126	619512.907294	40.740045
3487.013254	620169.806551	40.745050
3490.012136	620756.975192	40.750055
3492.644072	621315.496211	40.755060
3494.956793	621799.617071	40.760064
3497.672627	622235.855558	40.765069
3499.782355	622629.569664	40.770074
3502.331175	622956.680090	40.775079
3504.508985	623254.474080	40.780084
3505.948867	623496.695008	40.785088
3507.969695	623692.279077	40.790093
3509.403643	623853.046493	40.795098
3510.662684	623976.188184	40.800103
3512.080078	624051.417018	40.805108
3513.362886	624103.497106	40.810112
3514.483239	624129.686829	40.815117
3515.459300	624114.604010	40.820122
3516.334768	624072.073316	40.825127
3517.552091	624016.056724	40.830132
3518.037525	623933.289474	40.835136
3518.833869	623817.765458	40.840141
3519.442666	623694.229744	40.845146
3519.926216	623529.714184	40.850151
3520.350155	623370.099054	40.855156
3520.830725	623194.092721	40.860160
3521.631958	623005.098841	40.865165
3521.801972	622804.414101	40.870170
3521.928130	622580.609260	40.875175
3522.267488	622348.425584	40.880180
3522.457245	622116.109984	40.885184
3522.828927	621865.530532	40.890189
3522.926080	621613.339394	40.895194
3523.277912	621341.372662	40.900199
3523.179077	621084.953093	40.905204
3523.250123	620813.415299	40.910208
3523.432319	620519.424299	40.915213
3523.388707	620244.192350	40.920218
3523.329152	619955.467470	40.925223
3523.069854	619663.917893	40.930228
3522.745600	619374.867774	40.935232
3523.053953	619084.261520	40.940237
3522.677070	618794.003684	40.945242
3522.984278	618496.086153	40.950247
3522.490668	618204.530329	40.955252
3522.649273	617913.213755	40.960256
3522.641017	617603.926802	40.965261
3522.245627	617317.526167	40.970266
3522.759572	617021.530928	40.975271
3522.122353	616721.359399	40.980276
3521.831861	616419.775387	40.985280
3521.748864	616129.943694	40.990285
3521.389139	615836.798516	40.995290
3521.022153	615541.596838	41.000295
3520.810855	615259.656354	41.005300
3520.730748	614977.137659	41.010304
3521.018784	614690.504995	41.015309
3520.181057	614420.484380	41.020314
3520.308871	614129.662244	41.025319
3520.064567	613859.633768	41.030324
3519.930601	613582.732640	41.035328
3519.628496	613289.554094	41.040333
3519.483235	613029.135571	41.045338
3519.062824	612754.406018	41.050343
3518.641943	612499.815848	41.055348
3518.835211	612241.273777	41.060352
3518.653757	611973.834656	41.065357
3518.535733	611712.178075	41.070362
3517.916464	611454.692859	41.075367
3517.960073	611205.747194	41.080372
3517.648341	610953.650996	41.085376
3517.360983	610704.294773	41.090381
3516.858293	610462.366392	41.095386
3516.939434	610228.241486	41.100391
3516.462656	609988.597926	41.105396
3516.501121	609749.068198	41.110400
3516.418830	609518.052851	41.115405
3516.015079	609291.183159	41.120410
3515.919555	609058.709249	41.125415
3515.749581	608834.643366	41.130420
3515.621680	608614.566877	41.135424
3514.915101	608386.874237	41.140429
3514.999878	608179.508235	41.145434
3515.093720	607964.484437	41.150439
3514.960823	607750.041739	41.155444
3514.540599	607533.438748	41.160448
3514.166432	607332.929575	41.165453
3514.213959	607139.853304	41.170458
3513.971092	606937.665276	41.175463
3513.891411	606742.450588	41.180468
3513.252063	606536.515105	41.185472
3513.297708	606340.222739	41.190477
3513.141339	606158.765044	41.195482
3513.565082	605967.208669	41.200487
3513.151460	605784.533993	41.205492
3512.396737	605597.307028	41.210496
3512.781343	605409.848525	41.215501
3512.225660	605231.188381	41.220506
3511.950634	605047.078196	41.225511
3511.819600	604880.402443	41.230516
3511.811780	604712.504017	41.235520
3511.812581	604542.200033	41.240525
3511.497958	604385.801330	41.245530
3511.444832	604221.254129	41.250535
3511.204622	604053.031098	41.255540
3510.946646	603894.164477	41.260544
3511.156077	603729.818592	41.265549
3510.963959	603582.344828	41.270554
3510.777104	603426.962412	41.275559
3510.516517	603274.191121	41.280564
3510.162712	603117.629281	41.285568
3510.215480	602973.411069	41.290573
3509.769468	602833.722313	41.295578
3509.545535	602690.544212	41.300583
3509.527737	602557.440094	41.305588
3509.619344	602419.313057	41.310592
3509.765042	602283.827947	41.315597
3509.258817	602153.747483	41.320602
3509.280396	602018.678663	41.325607
3509.282843	601888.715541	41.330612
3509.339288	601756.340228	41.335616
3509.500998	601620.243452	41.340621
3508.733729	601494.799701	41.345626
3508.809367	601353.708341	41.350631
3508.720988	601236.112701	41.355636
3508.592041	601119.372882	41.360640
3508.627684	600993.697491	41.365645
3508.755409	600887.174784	41.370650
3508.372675	600766.667011	41.375655
3508.133638	600643.232503	41.380660
3508.213877	600524.351248	41.385664
3507.913606	600407.329955	41.390669
3507.534061	600297.026624	41.395674
3507.460290	600191.229046	41.400679
3507.555868	600077.445601	41.405684
3507.633547	599988.990461	41.410688
3507.328888	599867.659278	41.415693
3507.111120	599767.135529	41.420698
3506.947190	599669.755821	41.425703
3507.156580	599574.419149	41.430708
3507.142610	599478.165479	41.435712
3507.114164	599369.849761	41.440717
3507.414421	599283.005710	41.445722
3507.281020	599174.303933	41.450727
3507.123595	599073.513819	41.455732
3507.006131	598982.677957	41.460736
3507.011386	598880.258714	41.465741
3506.724347	598785.643242	41.470746
3506.760841	598697.534066	41.475751
3506.510406	598596.904097	41.480756
3506.533792	598505.341258	41.485760
3506.987035	598409.204996	41.490765
3506.535229	598327.376531	41.495770
3506.225376	598234.762097	41.500775
3506.534460	598149.459203	41.505780
3506.146964	598064.665009	41.510784
3506.283272	597968.023586	41.515789
3505.904297	597887.131498	41.520794
3505.723676	597800.450512	41.525799
3505.853984	597724.533944	41.530804
3505.641648	597644.565151	41.535808
3505.575357	597570.931090	41.540813
3505.805542	597497.700748	41.545818
3505.724176	597407.095969	41.550823
3505.861288	597339.386238	41.555828
3505.694307	597253.349474	41.560832
3505.767494	597172.130885	41.565837
3505.467348	597097.628888	41.570842
3505.408687	597018.332257	41.575847
3505.223897	596954.825936	41.580852
3505.168648	596877.430269	41.585856
3505.304439	596810.618572	41.590861
3505.380671	596746.869925	41.595866
3505.384899	596676.172625	41.600871
3505.399486	596594.357936	41.605876
3505.167266	596528.853713	41.610880
3505.237476	596459.696797	41.615885
3504.946944	596398.256516	41.620890
3505.125657	596319.768726	41.625895
3505.113910	596258.334121	41.630900
3504.879439	596197.334543	41.635904
3505.193051	596112.565277	41.640909
3504.831124	596051.684928	41.645914
3504.865815	595990.742225	41.650919
3504.734750	595919.259872	41.655924
3504.659444	595861.037514	41.660928
3505.026663	595799.941587	41.665933
3504.767499	595732.483814	41.670938
3504.674648	595670.958336	41.675943
3504.830151	595610.094707	41.680948
3504.276155	595550.293046	41.685952
3504.308606	595482.487652	41.690957
3504.394997	595432.449827	41.695962
3504.297921	595371.524166	41.700967
3504.690460	595321.738408	41.705972
3504.307982	595265.313422	41.710976
3504.450287	595191.580121	41.715981
3503.847177	595154.968866	41.720986
3504.414674	595102.550793	41.725991
3504.325306	595034.060516	41.730996
3504.297954	594990.748614	41.736000
3504.178408	594926.769247	41.741005
3504.387517	594889.579413	41.746010
3503.930593	594821.495763	41.751015
3504.281643	594772.665391	41.756020
3503.791283	594711.246571	41.761024
3504.030593	594652.918328	41.766029
3503.861376	594621.094975	41.771034
3503.980786	594551.266915	41.776039
3504.054371	594509.389552	41.781044
3503.789995	594468.065646	41.786048
3504.093463	594407.071841	41.791053
3504.010213	594363.866283	41.796058
3503.770203	594302.606284	41.801063
3503.772277	594251.925050	41.806068
3503.632721	594207.024938	41.811072
3504.040815	594159.284601	41.816077
3503.936429	594119.086179	41.821082
3503.898968	594059.345616	41.826087
3504.061178	594011.242408	41.831092
3503.558352	593968.651731	41.836096
3503.611310	593925.272857	41.841101
3503.879343	593867.086067	41.846106
3503.759142	593814.017939	41.851111
3504.094084	593772.096822	41.856116
3503.898835	593725.150014	41.861120
3504.053929	593676.445421	41.866125
3503.546963	593629.046093	41.871130
3503.533772	593570.500986	41.876135
3503.895090	593529.927042	41.881140
3503.773651	593484.570304	41.886144
3503.705126	593430.240099	41.891149
3503.515673	593395.260964	41.896154
3503.582349	593344.515235	41.901159
3503.497329	593296.998385	41.906164
3503.308429	593254.806538	41.911168
3503.451803	593212.963259	41.916173
3503.213025	593182.398604	41.921178
3503.426285	593134.283466	41.926183
3503.593230	593099.397903	41.931188
3503.147492	593061.302358	41.936192
3503.536814	593012.708379	41.941197
3503.646613	592972.572326	41.946202
3503.390823	592923.678104	41.951207
3503.196765	592885.692847	41.956212
3503.169762	592839.066446	41.961216
3503.752906	592808.572579	41.966221
3503.244147	592767.380458	41.971226
3503.225309	592721.002700	41.976231
3503.662661	592679.311727	41.981236
3503.336267	592645.102854	41.986240
3503.334596	592598.421356	41.991245
3503.587444	592553.152418	41.996250
3503.094247	592510.504323	42.001255
3503.258576	592469.506361	42.006260
3503.230404	592438.305593	42.011264
3503.416483	592387.837191	42.016269
3502.984848	592354.695703	42.021274
3503.041575	592327.338183	42.026279
3503.252520	592278.618494	42.031284
3502.883096	592232.744231	42.036288
3502.957158	592191.659138	42.041293
3502.961349	592160.302233	42.046298
3503.236271	592127.600575	42.051303
3503.207379	592089.987392	42.056308
3502.762647	592049.884479	42.061312
3503.287523	592008.527849	42.066317
3503.060935	591979.761108	42.071322
3502.932739	591941.812295	42.076327
3502.898811	591909.909618	42.081332
3502.996938	591882.644673	42.086336
3503.572158	591833.966201	42.091341
3503.617560	591803.954277	42.096346
3503.691476	591761.414907	42.101351
3503.346518	591718.089289	42.106356
3503.323109	591681.726114	42.111360
3503.175009	591636.465894	42.116365
3502.867795	591590.078232	42.121370
3502.957108	591557.754502	42.126375
3503.471194	591519.653696	42.131380
3502.868367	591490.343345	42.136384
3503.156577	591442.409268	42.141389
3502.821843	591410.051198	42.146394
3502.768771	591376.296475	42.151399
3503.096482	591340.979312	42.156404
3502.848823	591314.217823	42.161408
3503.494118	591264.123193	42.166413
3503.141248	591230.515067	42.171418
3503.032266	591191.658903	42.176423
3503.001825	591151.037014	42.181428
3502.905219	591129.310993	42.186432
3503.269774	591090.981573	42.191437
3502.881820	591049.012533	42.196442
3502.902960	590999.465099	42.201447
3503.330550	590979.911114	42.206452
3502.969313	590931.625430	42.211456
3503.000389	590903.216286	42.216461
3502.877099	590852.839129	42.221466
3502.975136	590832.735245	42.226471
3503.042636	590794.300919	42.231476
3502.828693	590764.677309	42.236480
3503.259677	590722.629068	42.241485
3502.934468	590690.417629	42.246490
3502.642277	590644.524500	42.251495
3503.079311	590616.552106	42.256500
3502.845935	590586.530267	42.261504
3503.320678	590548.582470	42.266509
3503.187311	590515.739350	42.271514
3503.025487	590476.989060	42.276519
3503.018829	590448.133736	42.281524
3503.090432	590409.346711	42.286528
3502.967993	590373.846258	42.291533
3502.892087	590334.280453	42.296538
3502.764489	590302.988830	42.301543
3502.983170	590273.697024	42.306548
3502.520357	590248.820164	42.311552
3502.842555	590209.692653	42.316557
3502.769321	590178.742862	42.321562
3502.866695	590144.259370	42.326567
3502.678713	590107.215210	42.331572
3502.581781	590071.308978	42.336576
3502.706496	590035.367977	42.341581
3502.347524	590016.586506	42.346586
3502.240037	589994.809796	42.351591
3502.404058	589964.022698	42.356596
3502.561192	589940.901911	42.361600
3502.608584	589892.948487	42.366605
3502.261689	589875.317189	42.371610
3502.190946	589850.728819	42.376615
3502.220080	589827.076693	42.381620
3502.012791	589810.325276	42.386624
3502.222622	589785.642795	42.391629
3502.176196	589768.264955	42.396634
3502.279353	589734.430561	42.401639
3502.748181	589703.945780	42.406644
3502.256000	589678.470977	42.411648
3502.412170	589652.043033	42.416653
3502.404822	589635.911408	42.421658
3502.295608	589607.119967	42.426663
3502.160886	589578.733251	42.431668
3502.199558	589564.798805	42.436672
3502.393560	589534.256305	42.441677
3502.313743	589514.728890	42.446682
3502.239435	589490.290563	42.451687
3502.379082	589455.898468	42.456692
3502.079673	589432.296837	42.461696
3502.570652	589402.008153	42.466701
3502.413328	589384.797340	42.471706
3502.098747	589356.638568	42.476711
3502.588695	589330.157659	42.481716
3502.532541	589314.784728	42.486720
3502.455291	589280.526188	42.491725
3502.326034	589245.574223	42.496730
3502.270227	589220.781670	42.501735
3502.577305	589181.352181	42.506740
3502.590880	589173.984729	42.511744
3502.249130	589153.044601	42.516749
3502.189213	589132.110478	42.521754
3502.225000	589104.748043	42.526759
3502.000072	589072.666402	42.531764
3502.087960	589053.663082	42.536768
3502.371272	589037.334812	42.541773
3502.612685	589015.802210	42.546778
3502.388471	588987.528140	42.551783
3502.235349	588954.933879	42.556788
3502.437396	588927.494900	42.561792
3502.682348	588901.502187	42.566797
3502.705891	588865.472903	42.571802
3502.459811	588847.774058	42.576807
3502.291171	588824.401181	42.581812
3502.274669	588789.931169	42.586816
3502.459628	588756.531877	42.591821
3502.144911	588738.242315	42.596826
3502.240367	588708.464476	42.601831
3502.274867	588693.276914	42.606836
3502.305926	588667.517501	42.611840
3502.335185	588639.253001	42.616845
3502.196529	588624.844004	42.621850
3502.159967	588591.228301	42.626855
3502.634247	588559.436683	42.631860
3502.118702	588541.428716	42.636864
3502.404337	588517.833841	42.641869
3502.584427	588497.662678	42.646874
3502.313182	588468.342359	42.651879
3502.176196	588439.251508	42.656884
3502.597087	588426.107664	42.661888
3502.627675	588384.714214	42.666893
3502.499283	588353.266743	42.671898
3502.380907	588334.945806	42.676903
3502.250147	588298.638112	42.681908
3502.349621	588282.638093	42.686912
3502.327362	588247.465746	42.691917
3502.429234	588230.162467	42.696922
3502.496564	588206.901692	42.701927
3502.561644	588175.924543	42.706932
3502.536677	588152.277213	42.711936
3502.597971	588120.148004	42.716941
3502.467725	588092.408099	42.721946
3502.671682	588069.877302	42.726951
3502.682862	588042.866793	42.731956
3502.661948	588008.495203	42.736960
3502.701668	587979.375494	42.741965
3502.726772	587957.674171	42.746970
3502.789155	587913.768487	42.751975
3502.875339	587883.338409	42.756980
3502.601665	587858.877456	42.761984
3502.711833	587833.705013	42.766989
3502.409515	587802.834344	42.771994
3502.727079	587768.609521	42.776999
3502.708392	587735.890356	42.782004
3502.484639	587713.676235	42.787009
3502.684484	587680.171083	42.792013
3502.600323	587653.625505	42.797018
3502.342498	587632.368648	42.802023
3502.474640	587599.024161	42.807028
3502.067629	587569.872968	42.812033
3502.439498	587543.957388	42.817037
3502.804607	587529.818960	42.822042
3502.795001	587490.282499	42.827047
3502.525343	587464.767687	42.832052
3502.415930	587432.011678	42.837057
3502.521464	587390.803168	42.842061
3502.359858	587367.325825	42.847066
3502.623186	587341.226282	42.852071
3502.636450	587303.940615	42.857076
3502.425762	587281.773679	42.862081
3502.439030	587257.567187	42.867085
3502.308553	587238.143812	42.872090
3502.284958	587219.605723	42.877095
3502.516824	587197.970786	42.882100
3502.703618	587173.987545	42.887105
3502.752510	587136.996413	42.892109
3502.516303	587110.022259	42.897114
3502.353827	587080.430617	42.902119
3502.592742	587036.844588	42.907124
3502.444369	587025.291455	42.912129
3502.430189	586995.776628	42.917133
3502.227447	586966.441539	42.922138
3501.957217	586946.438124	42.927143
3502.109652	586918.751258	42.932148
3502.156214	586905.613987	42.937153
3502.579620	586869.114654	42.942157
3502.107014	586855.106310	42.947162
3502.179097	586825.828109	42.952167
3502.544720	586805.424345	42.957172
3502.092057	586787.303397	42.962177
3502.224167	586761.874471	42.967181
3502.260699	586732.150542	42.972186
3502.137038	586709.567915	42.977191
3502.115094	586679.001026	42.982196
3501.982994	586661.080330	42.987201
3502.131173	586635.798944	42.992205
3502.092231	586613.052527	42.997210
3501.834994	586591.492846	43.002215
3501.992636	586565.608430	43.007220
3501.946743	586560.253130	43.012225
3501.712092	586545.004409	43.017229
3502.192516	586533.202108	43.022234
3502.205897	586514.005530	43.027239
3502.206922	586481.129161	43.032244
3501.851777	586459.935339	43.037249
3502.049762	586442.363611	43.042253
3501.992056	586425.733921	43.047258
3501.811218	586401.455637	43.052263
3501.754637	586373.850179	43.057268
3501.865588	586364.561168	43.062273
3501.593123	586346.411313	43.067277
3501.581154	586329.924678	43.072282
3501.608165	586323.605645	43.077287
3501.847740	586290.039889	43.082292
3501.384004	586279.236902	43.087297
3501.897159	586263.921000	43.092301
3501.913758	586253.995123	43.097306
3501.616621	586245.922501	43.102311
3501.566520	586219.317982	43.107316
3501.979400	586203.867321	43.112321
3502.158539	586185.596483	43.117325
3501.598988	586170.097322	43.122330
3501.833156	586149.963473	43.127335
3502.033331	586124.522421	43.132340
3501.831910	586110.871664	43.137345
3501.853597	586095.131179	43.142349
3501.935170	586065.197919	43.147354
3501.900511	586059.189083	43.152359
3502.303465	586035.670728	43.157364
3501.989468	586010.710735	43.162369
3502.206032	585986.519756	43.167373
3502.102543	585968.092264	43.172378
3501.877048	585945.874803	43.177383
3501.933779	585924.615550	43.182388
3502.186571	585914.351728	43.187393
3502.151228	585883.534111	43.192397
3502.426617	585869.958870	43.197402
3501.997636	585848.975876	43.202407
3502.335374	585823.262023	43.207412
3502.328109	585805.220166	43.212417
3502.268073	585778.415648	43.217421
3502.830008	585749.308577	43.222426
3502.222008	585721.637312	43.227431
3502.599866	585694.212818	43.232436
3502.237713	585679.183295	43.237441
3502.234225	585646.605836	43.242445
3501.908334	585622.749453	43.247450
3501.666665	585597.977689	43.252455
3501.945211	585578.086450	43.257460
3501.750508	585570.197794	43.262465
3502.075176	585546.189423	43.267469
3501.870982	585530.232834	43.272474
3501.651446	585512.674762	43.277479
3502.432756	585478.470500	43.282484
3502.087847	585471.707909	43.287489
3502.119986	585435.064469	43.292493
3502.060921	585418.533699	43.297498
3502.113181	585405.343611	43.302503
3502.429084	585382.288551	43.307508
3502.471031	585360.930271	43.312513
3501.958087	585328.130778	43.317517
3501.708285	585305.665206	43.322522
3501.986095	585290.735589	43.327527
3502.118209	585274.024349	43.332532
3501.954563	585245.029367	43.337537
3501.821367	585227.557583	43.342541
3502.057885	585219.300529	43.347546
3502.237471	585201.880051	43.352551
3502.370687	585182.963132	43.357556
3501.695353	585153.847412	43.362561
3501.737978	585135.495917	43.367565
3502.187127	585118.183533	43.372570
3501.930510	585098.876309	43.377575
3502.004470	585086.785139	43.382580
3501.472142	585063.962256	43.387585
3501.722246	585032.897127	43.392589
3501.936569	585031.510217	43.397594
3501.767626	585016.599944	43.402599
3501.752342	584995.400266	43.407604
3501.696747	584972.803404	43.412609
3501.798887	584958.452150	43.417613
3501.580480	584938.637439	43.422618
3501.403697	584937.662521	43.427623
3501.790147	584922.715420	43.432628
3501.954230	584898.780858	43.437633
3501.828097	584888.124203	43.442637
3501.866304	584871.627523	43.447642
3501.762284	584847.283650	43.452647
3501.751913	584839.816761	43.457652
3501.384343	584813.809809	43.462657
3501.727053	584798.217768	43.467661
3501.618708	584787.758730	43.472666
3501.731216	584764.884540	43.477671
3501.962140	584746.001716	43.482676
3501.483541	584732.643186	43.487681
3501.330543	584703.294235	43.492685
3501.415341	584713.155363	43.497690
3501.535274	584701.607948	43.502695
3501.780641	584680.016042	43.507700
3501.580448	584678.744013	43.512705
3501.904000	584662.202411	43.517709
3501.684322	584632.713321	43.522714
3501.617349	584632.874074	43.527719
3501.764085	584611.347577	43.532724
3501.942589	584597.836033	43.537729
3501.880384	584576.241881	43.542733
3501.378465	584561.533416	43.547738
3501.454597	584548.589189	43.552743
3501.593161	584534.682811	43.557748
3501.363272	584520.382890	43.562753
3501.168578	584504.623818	43.567757
3501.416341	584505.286747	43.572762
3501.153285	584503.222523	43.577767
3501.509643	584478.655484	43.582772
3501.361478	584464.944218	43.587777
3501.805467	584456.203030	43.592781
3501.635155	584436.179389	43.597786
3501.599402	584424.505644	43.602791
3501.636633	584414.324244	43.607796
3501.424205	584392.151706	43.612801
3501.415292	584380.022586	43.617805
3501.338741	584381.889115	43.622810
3501.402170	584373.407856	43.627815
3501.614193	584355.680210	43.632820
3501.107185	584342.425894	43.637825
3501.635426	584335.325594	43.642829
3501.568071	584333.631751	43.647834
3501.753982	584300.068284	43.652839
3501.534299	584287.169993	43.657844
3501.527293	584279.952828	43.662849
3501.629422	584260.387537	43.667853
3501.707810	584247.292224	43.672858
3501.564420	584233.630048	43.677863
3501.536680	584213.784218	43.682868
3501.498388	584215.043276	43.687873
3501.570201	584199.392481	43.692877
3501.382399	584189.045546	43.697882
3501.334169	584177.022601	43.702887
3501.499455	584174.239705	43.707892
3501.639879	584159.229774	43.712897
3501.280502	584142.142503	43.717901
3501.619301	584134.369914	43.722906
3501.855030	584118.091857	43.727911
3501.462948	584089.630796	43.732916
3501.516240	584091.827965	43.737921
3501.683177	584072.653225	43.742925
3501.436106	584055.197371	43.747930
3500.992057	584039.927757	43.752935
3501.046707	584037.663394	43.757940
3501.208302	584035.282059	43.762945
3501.278310	584018.879380	43.767949
3501.516319	583998.039195	43.772954
3501.336458	583997.114799	43.777959
3501.442215	583991.233258	43.782964
3501.235396	583978.783741	43.787969
3501.050406	583961.067394	43.792973
3501.611856	583953.861404	43.797978
3501.380731	583954.248338	43.802983
3501.804323	583941.800483	43.807988
3501.565277	583925.746746	43.812993
3501.726358	583914.793604	43.817997
3501.454482	583887.616552	43.823002
3501.539596	583876.775504	43.828007
3501.578464	583874.663960	43.833012
3501.883993	583866.244719	43.838017
3501.584206	583853.007543	43.843021
3501.881618	583831.155193	43.848026
3501.579810	583818.469702	43.853031
3501.617470	583792.597488	43.858036
3501.640040	583801.266083	43.863041
3501.604601	583775.004228	43.868045
3501.499792	583761.836718	43.873050
3501.538001	583749.699536	43.878055
3501.675856	583721.505575	43.883060
3501.487418	583715.920522	43.888065
3501.714576	583701.949113	43.893069
3501.717571	583693.927937	43.898074
3501.330819	583681.857113	43.903079
3501.516809	583665.586162	43.908084
3501.362884	583661.649943	43.913089
3501.451278	583645.995768	43.918093
3501.585415	583641.813993	43.923098
3501.751090	583628.654168	43.928103
3501.864482	583602.268376	43.933108
3501.441903	583590.303311	43.938113
3501.614483	583572.931474	43.943117
3501.224861	583557.000994	43.948122
3501.398517	583556.672979	43.953127
3501.676003	583546.753994	43.958132
3501.436671	583530.398945	43.963137
3501.751085	583513.806916	43.968141
3501.643774	583499.536630	43.973146
3501.517233	583473.990115	43.978151
3501.880265	583470.975609	43.983156
3501.938277	583451.516035	43.988161
3501.784416	583433.493191	43.993165
3501.440506	583417.755883	43.998170
3501.006258	583406.444132	44.003175
3501.593558	583391.162774	44.008180
3501.315743	583384.588918	44.013185
3501.582246	583379.183224	44.018189
3501.598409	583364.893460	44.023194
3501.485621	583351.977358	44.028199
3501.941815	583333.658459	44.033204
3501.290522	583327.142954	44.038209
3501.856815	583308.506019	44.043213
3501.746191	583306.969173	44.048218
3501.577178	583281.729634	44.053223
3501.967891	583262.618762	44.058228
3502.006581	583247.773885	44.063233
3501.642897	583233.192415	44.068237
3501.594093	583231.044321	44.073242
3501.617563	583220.462919	44.078247
3501.871039	583192.249529	44.083252
3501.657750	583175.288305	44.088257
3501.636138	583148.421218	44.093261
3501.615568	583142.157922	44.098266
3501.447766	583130.202655	44.103271
3501.886862	583105.068173	44.108276
3501.539284	583104.520840	44.113281
3501.339088	583077.079917	44.118285
3501.385226	583064.790345	44.123290
3501.319568	583071.919223	44.128295
3501.567760	583061.252406	44.133300
3501.434241	583048.790374	44.138305
3501.481279	583021.611455	44.143309
3501.677809	583026.142646	44.148314
3501.625266	583005.295873	44.153319
3501.692280	582985.282617	44.158324
3501.627508	582982.786046	44.163329
3501.500576	582954.531251	44.168333
3501.538892	582949.161020	44.173338
3501.774086	582941.804849	44.178343
3501.734104	582908.924172	44.183348
3501.597988	582902.528405	44.188353
3501.314921	582883.772870	44.193357
3501.587772	582872.650824	44.198362
3501.209698	582869.401083	44.203367
3501.523399	582844.636539	44.208372
3501.500528	582849.954093	44.213377
3501.605871	582822.214107	44.218381
3501.806055	582812.456947	44.223386
3501.922980	582802.562394	44.228391
3502.091428	582778.622536	44.233396
3501.656688	582773.526703	44.238401
3501.946864	582745.206166	44.243405
3501.775973	582732.448818	44.248410
3501.038850	582718.727175	44.253415
3501.375460	582699.623787	44.258420
3501.476142	582689.932207	44.263425
3501.688980	582693.257784	44.268429
3501.792899	582666.620565	44.273434
3501.482207	582662.106890	44.278439
3501.862258	582644.249955	44.283444
3501.621396	582622.228689	44.288449
3501.413986	582607.471555	44.293453
3501.555004	582603.488847	44.298458
3501.343808	582591.940850	44.303463
3501.637165	582580.815304	44.308468
3501.784417	582576.580942	44.313473
3501.379099	582548.418759	44.318477
3501.556284	582538.414281	44.323482
3501.323520	582541.207955	44.328487
3501.275516	582515.646938	44.333492
3501.125894	582502.234254	44.338497
3501.640302	582497.491256	44.343501
3501.999442	582486.555869	44.348506
3501.443665	582474.861079	44.353511
3501.478756	582463.725656	44.358516
3501.572166	582455.488906	44.363521
3501.465712	582437.757826	44.368525
3501.119292	582420.064231	44.373530
3501.050503	582422.982705	44.378535
3501.233610	582403.752399	44.383540
3501.253071	582409.915838	44.388545
3501.101603	582396.703853	44.393549
3501.415290	582377.202413	44.398554
3501.113695	582369.328159	44.403559
3501.082598	582360.559318	44.408564
3501.008609	582368.642517	44.413569
3501.193171	582355.227546	44.418573
3500.664116	582337.211424	44.423578
3500.665200	582330.392795	44.428583
3501.285173	582328.290382	44.433588
3500.931769	582329.799456	44.438593
3500.751548	582324.362814	44.443597
3501.298051	582320.868102	44.448602
3500.943886	582327.390806	44.453607
3501.168889	582322.091355	44.458612
3501.163996	582321.991759	44.463617
3501.312284	582303.468613	44.468621
3501.182300	582283.936097	44.473626
3500.961984	582284.521936	44.478631
3501.222894	582281.573211	44.483636
3501.190199	582282.982020	44.488641
3501.273213	582278.958127	44.493645
3501.353231	582253.877843	44.498650
3501.293284	582255.691999	44.503655
3501.145498	582245.587653	44.508660
3501.285994	582240.902999	44.513665
3501.800267	582231.196496	44.518669
3501.679391	582217.879243	44.523674
3501.329657	582212.920266	44.528679
3501.841431	582191.632786	44.533684
3501.518531	582179.249511	44.538689
3501.532714	582168.919231	44.543693
3501.627729	582153.111495	44.548698
3501.554303	582128.656545	44.553703
3501.638220	582122.827559	44.558708
3501.678692	582113.144885	44.563713
3501.563963	582085.788405	44.568717
3501.433866	582084.805928	44.573722
3501.406120	582081.551322	44.578727
3501.577997	582048.133597	44.583732
3501.568821	582046.129486	44.588737
3501.416848	582035.674647	44.593741
3501.409907	582014.367644	44.598746
3501.447826	582003.682543	44.603751
3501.447420	581994.607795	44.608756
3501.348927	581988.005068	44.613761
3501.378685	581962.230066	44.618765
3501.282129	581963.097394	44.623770
3501.441045	581959.963982	44.628775
3501.732767	581949.489836	44.633780
3501.705687	581939.667160	44.638785
3501.402317	581929.235888	44.643789
3501.326836	581904.530078	44.648794
3501.074117	581893.138250	44.653799
3501.522206	581879.681506	44.658804
3501.543255	581874.814823	44.663809
3501.416612	581864.305724	44.668813
3501.608095	581850.137002	44.673818
3501.225794	581847.489263	44.678823
3501.464949	581827.848096	44.683828
3501.487187	581825.839034	44.688833
3501.225145	581809.535114	44.693837
3501.383393	581804.245852	44.698842
3501.322237	581801.497761	44.703847
3501.473705	581782.722558	44.708852
3501.344986	581774.620302	44.713857
3501.299456	581760.689067	44.718861
3501.437199	581759.764965	44.723866
3501.149390	581743.515113	44.728871
3501.457345	581718.899360	44.733876
3501.062548	581722.921876	44.738881
3501.160777	581716.388509	44.743885
3501.176867	581715.333008	44.748890
3501.279896	581713.160882	44.753895
3501.025551	581685.825237	44.758900
3501.208829	581676.721512	44.763905
3500.938444	581675.359825	44.768909
3501.423479	581676.136257	44.773914
3501.024058	581679.808546	44.778919
3501.354851	581663.612285	44.783924
3501.327064	581652.586150	44.788929
3501.364100	581632.324437	44.793933
3501.301546	581643.715501	44.798938
3500.761144	581636.178882	44.803943
3501.228585	581629.387193	44.808948
3501.305656	581615.436609	44.813953
3500.908286	581603.665988	44.818957
3501.053982	581593.815995	44.823962
3501.022936	581598.032384	44.828967
3501.241219	581593.084605	44.833972
3501.174807	581584.270530	44.838977
3501.395718	581580.174689	44.843981
3501.162206	581560.907770	44.848986
3501.152885	581557.449575	44.853991
3501.443043	581557.955649	44.858996
3501.558670	581553.274593	44.864001
3501.635680	581529.847711	44.869005
3501.617877	581510.196011	44.874010
3501.326995	581509.689867	44.879015
3501.666018	581488.377905	44.884020
3501.365055	581486.218752	44.889025
3501.114017	581475.829008	44.894029
3501.479871	581470.657549	44.899034
3501.257571	581440.307947	44.904039
3501.461627	581436.766218	44.909044
3501.145028	581431.851846	44.914049
3500.862356	581428.887595	44.919053
3501.291750	581427.516760	44.924058
3501.087375	581406.690702	44.929063
3501.024929	581392.561091	44.934068
3501.063587	581394.359973	44.939073
3501.158381	581390.333917	44.944077
3501.200959	581385.162816	44.949082
3500.907726	581378.891004	44.954087
3501.005178	581378.274006	44.959092
3500.874394	581364.706576	44.964097
3501.048504	581352.996767	44.969101
3501.136538	581341.551099	44.974106
3500.958123	581354.314342	44.979111
3501.417636	581343.311999	44.984116
3501.222897	581349.459375	44.989121
3501.145738	581345.560463	44.994125
3501.347792	581326.826719	44.999130
3501.254233	581312.100194	45.004135
3501.543864	581304.934986	45.009140
3501.345915	581313.138613	45.014145
3501.018529	581296.643592	45.019149
3501.297025	581272.482710	45.024154
3501.148238	581281.831892	45.029159
3501.324792	581274.834762	45.034164
3501.580863	581272.839185	45.039169
3501.092521	581251.054429	45.044173
3501.314605	581241.994422	45.049178
3501.043081	581237.674596	45.054183
3500.866184	581229.078070	45.059188
3500.430913	581237.268713	45.064193
3500.761721	581228.893659	45.069197
3500.983214	581230.613845	45.074202
3501.123334	581231.043110	45.079207
3501.024636	581230.958169	45.084212
3500.739792	581228.846584	45.089217
3500.936675	581209.110648	45.094221
3501.335873	581200.073059	45.099226
3501.140948	581196.994747	45.104231
3500.988354	581186.037798	45.109236
3501.494978	581187.262155	45.114241
3501.234527	581190.461616	45.119245
3501.247000	581167.846301	45.124250
3500.988785	581151.741372	45.129255
3501.410134	581147.263054	45.134260
3501.232094	581146.187707	45.139265
3500.973088	581141.264200	45.144269
3501.259133	581132.545088	45.149274
3501.085731	581122.193015	45.154279
3500.934767	581112.338830	45.159284
3500.959062	581114.942252	45.164289
3501.220569	581116.906904	45.169293
3501.542797	581109.987178	45.174298
3501.137885	581098.467900	45.179303
3501.324021	581079.284960	45.184308
3501.371228	581068.346801	45.189313
3500.687780	581057.222007	45.194317
3500.889779	581053.429774	45.199322
3500.608592	581063.200965	45.204327
3501.103570	581056.304341	45.209332
3500.946749	581059.036372	45.214337
3500.896130	581064.008137	45.219341
3501.166368	581051.129743	45.224346
3501.116921	581038.050605	45.229351
3501.152248	581022.952559	45.234356
3501.262393	581025.743146	45.239361
3501.487517	581021.947287	45.244365
3501.125413	581014.683213	45.249370
3501.229625	580999.674649	45.254375
3501.114588	580989.513892	45.259380
3501.182587	580983.235525	45.264385
3501.036653	580988.623353	45.269389
3501.279515	580980.763272	45.274394
3500.895260	580982.026640	45.279399
3501.244718	580964.272065	45.284404
3501.458087	580960.427881	45.289409
3501.179833	580955.607584	45.294413
3501.513561	580950.992462	45.299418
3501.159033	580935.554111	45.304423
3501.295226	580918.534782	45.309428
3501.328712	580906.244788	45.314433
3501.513155	580908.773081	45.319437
3501.196506	580903.958763	45.324442
3501.079132	580891.491770	45.329447
3500.963954	580869.397217	45.334452
3501.077640	580863.362348	45.339457
3501.062155	580866.122473	45.344461
3501.505104	580854.219686	45.349466
3501.182257	580859.183957	45.354471
3501.155433	580847.103892	45.359476
3501.386449	580844.610739	45.364481
3501.345955	580835.441023	45.369485
3501.535462	580836.564570	45.374490
3501.370099	580809.262989	45.379495
3501.478313	580789.740737	45.384500
3501.241032	580790.229018	45.389505
3501.186441	580789.184478	45.394509
3501.099873	580770.946195	45.399514
3500.851323	580758.198705	45.404519
3501.364486	580748.089947	45.409524
3501.156792	580746.116635	45.414529
3501.166398	580745.814189	45.419533
3501.399741	580744.774775	45.424538
3501.134922	580736.642891	45.429543
3501.027824	580727.182644	45.434548
3501.240430	580715.265575	45.439553
3501.350319	580702.863126	45.444557
3501.413033	580701.048103	45.449562
3501.289606	580695.451350	45.454567
3501.501886	580671.098942	45.459572
3501.763157	580668.300164	45.464577
3501.565002	580661.210798	45.469581
3501.572691	580642.054999	45.474586
3501.172182	580638.306671	45.479591
3501.569374	580624.555511	45.484596
3501.836258	580612.278847	45.489601
3501.152959	580600.852710	45.494605
3501.428001	580586.218025	45.499610
3501.159998	580588.817123	45.504615
3501.163149	580570.012910	45.509620
3501.081156	580552.224839	45.514625
3501.075460	580540.642568	45.519629
3501.169558	580553.715132	45.524634
3501.010881	580551.433262	45.529639
3501.144687	580540.932333	45.534644
3501.456729	580521.227316	45.539649
3501.459073	580505.782720	45.544653
3501.644142	580489.607529	45.549658
3501.408610	580501.427955	45.554663
3500.914051	580478.990785	45.559668
3500.959032	580466.397645	45.564673
3501.030095	580469.695917	45.569677
3501.280981	580463.238236	45.574682
3501.254393	580469.008806	45.579687
3501.343144	580455.255511	45.584692
3501.238744	580439.526648	45.589697
3500.910085	580432.557824	45.594701
3501.306474	580420.411134	45.599706
3501.012604	580423.265032	45.604711
3501.353990	580412.932107	45.609716
3501.351118	580416.643103	45.614721
3501.007389	580391.825420	45.619725
3501.164584	580388.641692	45.624730
3501.078238	580393.519054	45.629735
3500.878063	580382.618892	45.634740
3501.440914	580390.052394	45.639745
3501.147304	580375.807192	45.644749
3501.232645	580360.148842	45.649754
3501.036206	580354.864195	45.654759
3501.389793	580345.431892	45.659764
3501.405000	580347.886483	45.664769
3501.185566	580331.874586	45.669773
3501.529173	580311.863398	45.674778
3501.102828	580315.289620	45.679783
3500.993353	580308.838039	45.684788
3500.980953	580301.067528	45.689793
3501.412151	580304.810992	45.694797
3501.496038	580287.698585	45.699802
3501.239203	580277.559341	45.704807
3501.282117	580268.225684	45.709812
3501.370633	580262.796157	45.714817
3501.227558	580253.742286	45.719821
3501.445409	580233.951195	45.724826
3501.319380	580210.001675	45.729831
3501.328694	580150.077074	45.734836
3501.245091	580050.000281	45.739841
3500.179978	579900.882833	45.744845
3500.482483	579703.057572	45.749850
3499.765199	579465.570745	45.754855
3499.613890	579178.944434	45.759860
3499.084169	578844.676565	45.764865
3498.588384	578464.353430	45.769869
3498.302152	578041.854928	45.774874
3496.836577	577579.499997	45.779879
3496.323243	577071.132054	45.784884
3495.249795	576537.396933	45.789889
3494.317226	575958.366791	45.794893
3493.659103	575321.672830	45.799898
3492.810524	574664.553699	45.804903
3491.689566	573941.461968	45.809908
3490.452054	573191.498101	45.814913
3489.024578	572394.847442	45.819917
3487.788714	571575.327867	45.824922
3486.288914	570718.351238	45.829927
3484.788435	569821.760112	45.834932
3483.216402	568887.714848	45.839937
3481.464555	567916.374048	45.844941
3479.512913	566907.581034	45.849946
3478.247687	565885.237388	45.854951
3476.006550	564804.709678	45.859956
3474.381416	563701.387543	45.864961
3472.431048	562585.556952	45.869965
3470.894403	561419.629749	45.874970
3468.474875	560237.248889	45.879975
3466.330814	559008.237036	45.884980
3464.375977	557754.147830	45.889985
3461.542014	556477.050332	45.894989
3459.875349	555171.893926	45.899994
3457.334619	553861.555589	45.904999
3454.625840	552511.442304	45.910004
3451.899444	551142.581187	45.915009
3449.578855	549747.258437	45.920013
3447.171247	548338.515516	45.925018
3444.263253	546909.222035	45.930023
3441.641266	545457.538682	45.935028
3438.954893	543982.959906	45.940033
3436.467562	542492.429727	45.945037
3433.618405	540986.886327	45.950042
3430.847656	539453.727275	45.955047
3427.581521	537912.810486	45.960052
3424.652451	536354.642579	45.965057
3421.689345	534791.407312	45.970061
3418.976121	533197.737279	45.975066
3416.021510	531612.517894	45.980071
3412.585310	529985.939679	45.985076
3409.632080	528372.932578	45.990081
3406.479118	526738.302073	45.995085
3403.038611	525090.265903	46.000090
3400.230111	523440.213475	46.005095
3396.829598	521776.143229	46.010100
3393.732902	520120.234881	46.015105
3390.214058	518422.812492	46.020109
3387.388067	516725.422705	46.025114
3383.700379	515038.140075	46.030119
3380.421218	513323.966419	46.035124
3377.614648	511605.573681	46.040129
3373.908713	509877.679331	46.045133
3370.308725	508138.610926	46.050138
3366.902339	506397.885605	46.055143
3363.435818	504656.401466	46.060148
3359.954121	502907.946707	46.065153
3356.476393	501160.439524	46.070157
3353.155414	499403.865395	46.075162
3349.104238	497638.865879	46.080167
3345.618018	495856.554497	46.085172
3342.158420	494092.653023	46.090177
3338.645924	492314.413370	46.095181
3335.309909	490546.892974	46.100186
3331.398074	488763.953295	46.105191
3327.962153	486978.659195	46.110196
3324.176118	485198.162037	46.115201
3320.655489	483413.527670	46.120205
3316.894483	481628.675234	46.125210
3313.004829	479838.080695	46.130215
3309.522618	478056.467290	46.135220
3305.901013	476273.159352	46.140225
3301.932467	474487.533106	46.145229
3298.294287	472690.686883	46.150234
3294.708787	470902.835350	46.155239
3290.859695	469111.593299	46.160244
3287.098822	467319.282940	46.165249
3283.318646	465536.138684	46.170253
3279.746665	463747.258336	46.175258
3275.855415	461967.040198	46.180263
3272.518346	460174.912557	46.185268
3268.613589	458383.748616	46.190273
3264.581828	456597.580080	46.195277
3260.908480	454815.423127	46.200282
3257.111762	453046.668622	46.205287
3253.757348	451258.736687	46.210292
3249.915554	449489.887752	46.215297
3246.139533	447704.703888	46.220301
3242.319036	445920.667439	46.225306
3238.283109	444155.580927	46.230311
3234.999364	442363.974482	46.235316
3231.131165	440597.509169	46.240321
3227.025925	438825.291796	46.245325
3223.339994	437051.018837	46.250330
3219.507536	435285.114695	46.255335
3215.478107	433523.942983	46.260340
3212.086648	431759.775163	46.265345
3208.356168	429998.693677	46.270349
3204.597925	428249.774523	46.275354
3200.567284	426490.962017	46.280359
3196.842577	424738.080894	46.285364
3193.472844	422980.987723	46.290369
3189.415254	421238.350573	46.295373
3185.486644	419487.078699	46.300378
3181.528879	417750.774454	46.305383
3178.107977	415999.181667	46.310388
3174.700184	414240.697025	46.315393
3170.638724	412512.043445	46.320397
3167.041732	410773.490810	46.325402
3162.679202	409032.535083	46.330407
3158.771089	407312.220976	46.335412
3155.342482	405574.499657	46.340417
3151.312466	403855.409654	46.345421
3147.979753	402142.220050	46.350426
3143.499977	400428.726345	46.355431
3139.779257	398707.323668	46.360436
3136.410406	397006.852581	46.365441
3132.257164	395295.773257	46.370445
3128.881297	393597.495035	46.375450
3124.749941	391896.169245	46.380455
3121.046195	390193.134513	46.385460
3116.921406	388491.291484	46.390465
3112.988572	386802.782548	46.395469
3109.830123	385118.939019	46.400474
3105.931196	383437.867099	46.405479
3102.151164	381752.527371	46.410484
3098.723923	380078.297875	46.415489
3094.825569	378404.492187	46.420493
3091.073427	376730.100718	46.425498
3087.495582	375052.910443	46.430503
3083.726852	373390.302253	46.435508
3080.119832	371716.975245	46.440513
3076.426545	370045.745400	46.445517
3072.715325	368374.876033	46.450522
3068.715997	366705.909606	46.455527
3064.869998	365055.166731	46.460532
3061.385832	363401.656298	46.465537
3057.735731	361745.080343	46.470541
3053.833962	360074.144438	46.475546
3050.295096	358428.726902	46.480551
3046.052496	356777.510636	46.485556
3042.542766	355131.632274	46.490561
3038.616887	353501.872630	46.495565
3035.419503	351858.265271	46.500570
3031.031185	350226.046599	46.505575
3027.528276	348594.217678	46.510580
3024.020092	346959.181798	46.515585
3020.397394	345341.880603	46.520589
3016.953315	343704.286622	46.525594
3013.108675	342080.458284	46.530599
3009.342179	340462.390325	46.535604
3005.496428	338830.732512	46.540609
3001.607696	337210.399674	46.545613
2997.716615	335585.391933	46.550618
2994.274119	333983.105906	46.555623
2990.334421	332363.483586	46.560628
2986.629031	330766.163167	46.565633
2982.861595	329157.391276	46.570637
2979.612002	327556.281288	46.575642
2975.493531	325960.889834	46.580647
2971.987517	324352.696762	46.585652
2968.244427	322765.567018	46.590657
2964.320142	321171.281984	46.595661
2960.531096	319577.272092	46.600666
2956.768812	318010.829345	46.605671
2953.098025	316422.511677	46.610676
2950.010361	314846.819208	46.615681
2945.855659	313274.165136	46.620685
2942.647022	311681.512901	46.625690
2938.867748	310110.805554	46.630695
2934.972538	308543.398536	46.635700
2931.566397	306973.090940	46.640705
2927.567357	305403.233773	46.645709
2923.785596	303833.904923	46.650714
2919.973973	302270.565000	46.655719
2916.557164	300703.146726	46.660724
2913.331572	299148.302681	46.665729
2909.031058	297590.095865	46.670733
2905.667241	296028.517771	46.675738
2901.619585	294491.160163	46.680743
2898.190069	292933.480119	46.685748
2894.711190	291378.160292	46.690753
2890.638039	289831.498267	46.695757
2887.203208	288289.306143	46.700762
2883.356739	286751.418407	46.705767
2879.832854	285222.456580	46.710772
2876.515193	283672.501308	46.715777
2872.406253	282133.175330	46.720781
2868.970513	280597.122553	46.725786
2864.539197	279076.927688	46.730791
2860.986115	277535.076280	46.735796
2857.615644	276006.380056	46.740801
2853.547928	274493.422554	46.745805
2850.131299	272962.614055	46.750810
2845.841787	271454.601587	46.755815
2842.672618	269943.892752	46.760820
2839.874254	268434.144873	46.765825
2835.898572	266923.232838	46.770829
2832.132886	265407.197258	46.775834
2828.495893	263902.577850	46.780839
2824.906740	262393.727783	46.785844
2821.156045	260888.243594	46.790849
2817.284552	259395.058237	46.795853
2814.018222	257880.852177	46.800858
2810.423246	256386.950074	46.805863
2806.764669	254882.217657	46.810868
2803.183033	253373.280191	46.815873
2799.100570	251877.928187	46.820877
2795.412390	250386.014326	46.825882
2791.641813	248909.583698	46.830887
2788.388816	247419.383374	46.835892
2784.307080	245932.051049	46.840897
2780.617667	244450.274496	46.845901
2777.134132	242970.594670	46.850906
2773.293607	241498.525166	46.855911
2769.989246	240019.741340	46.860916
2766.464829	238538.895533	46.865921
2762.631854	237079.204256	46.870925
2758.834680	235602.844595	46.875930
2755.091761	234146.769488	46.880935
2751.604740	232674.375052	46.885940
2747.985620	231212.617810	46.890945
2744.504767	229758.629260	46.895949
2741.082503	228284.941578	46.900954
2737.187523	226831.497626	46.905959
2733.332394	225377.613573	46.910964
2730.031430	223925.960389	46.915969
2726.008206	222484.557449	46.920973
2722.638267	221019.138266	46.925978
2718.950766	219572.159485	46.930983
2715.196965	218125.041092	46.935988
2711.523417	216680.053103	46.940993
2708.042741	215243.902377	46.945997
2704.844025	213799.970050	46.951002
2700.484270	212361.446130	46.956007
2696.846422	210928.291464	46.961012
2693.592746	209492.256851	46.966017
2689.516559	208063.999203	46.971021
2686.551666	206633.564273	46.976026
2682.688395	205207.201141	46.981031
2678.978979	203779.932480	46.986036
2675.718615	202349.369844	46.991041
2671.839894	200926.657353	46.996045
2668.236251	199484.660743	47.001050
2664.692849	198067.395989	47.006055
2660.951969	196646.610090	47.011060
2657.656282	195225.819546	47.016065
2653.837760	193812.154151	47.021069
2650.226160	192389.533219	47.026074
2646.454927	190978.056384	47.031079
2642.653515	189562.857529	47.036084
2639.243038	188157.087855	47.041089
2635.302069	186758.243500	47.046093
2632.009765	185349.181321	47.051098
2628.424016	183942.756194	47.056103
2625.079263	182538.172126	47.061108
2621.630441	181130.874876	47.066113
2617.549610	179734.799506	47.071117
2614.450174	178332.379489	47.076122
2610.419792	176924.347757	47.081127
2606.677544	175523.716338	47.086132
2603.201493	174139.591260	47.091137
2599.482358	172741.703037	47.096141
2596.038868	171349.219739	47.101146
2592.416763	169956.433459	47.106151
2588.352629	168561.489377	47.111156
2584.979267	167176.838570	47.116161
2581.270005	165798.288335	47.121165
2578.165250	164413.230370	47.126170
2573.922384	163040.547405	47.131175
2570.413119	161660.981439	47.136180
2566.575984	160296.693544	47.141185
2563.129428	158927.461201	47.146189
2559.592017	157558.680730	47.151194
2555.495303	156184.609706	47.156199
2552.087551	154822.464199	47.161204
2548.418146	153454.321001	47.166209
2544.842288	152093.679046	47.171213
2541.253269	150734.357580	47.176218
2537.582086	149386.344787	47.181223
2534.033314	148035.394292	47.186228
2530.342064	146678.825218	47.191233
2526.814212	145293.750092	47.196237
2523.085354	143900.791261	47.201242
2519.641807	142554.853990	47.206247
2516.221819	141210.552850	47.211252
2512.612623	139864.728063	47.216257
2508.768281	138522.934707	47.221261
2505.414474	137183.431050	47.226266
2502.027629	135854.619646	47.231271
2498.126133	134511.386422	47.236276
2494.429310	133172.028555	47.241281
2490.921732	131843.519798	47.246285
2487.313046	130503.504201	47.251290
2483.431244	129171.077897	47.256295
2479.742251	127847.999535	47.261300
2476.495782	126528.060836	47.266305
2472.744309	125214.017676	47.271309
2469.245624	123888.670475	47.276314
2465.560888	122574.676993	47.281319
2461.731014	121253.996534	47.286324
2458.049909	119928.759023	47.291329
2454.545597	118624.878077	47.296333
2450.975218	117309.721553	47.301338
2447.275306	116004.829266	47.306343
2443.614977	114704.223375	47.311348
2440.050192	113393.565316	47.316353
2436.592063	112091.825205	47.321357
2433.175883	110790.481541	47.326362
2429.371556	109498.806829	47.331367
2425.505459	108199.446784	47.336372
2422.097577	106903.686669	47.341377
2418.352257	105618.566555	47.346381
2414.682691	104315.686549	47.351386
2410.844801	103043.034450	47.356391
2407.425374	101755.836994	47.361396
2403.817493	100484.047873	47.366401
2399.827955	99210.817384	47.371405
2396.463708	97931.260830	47.376410
2392.846322	96653.841159	47.381415
2389.424759	95384.728181	47.386420
2386.011205	94112.323156	47.391425
2381.812313	92854.604808	47.396429
2378.444072	91589.031432	47.401434
2374.676168	90327.334191	47.406439
2371.162539	89074.937782	47.411444
2367.484839	87812.239406	47.416449
2364.021739	86571.400508	47.421453
2360.368002	85312.705758	47.426458
2356.697635	84063.163804	47.431463
2353.212184	82815.920930	47.436468
2349.810663	81562.241161	47.441473
2346.171261	80324.531417	47.446477
2342.448370	79075.369257	47.451482
2338.740294	77837.069164	47.456487
2334.763139	76615.630936	47.461492
2331.621362	75366.037819	47.466497
2327.870290	74135.785735	47.471501
2324.643168	72907.628579	47.476506
2320.774457	71668.962161	47.481511
2317.187004	70439.667571	47.486516
2313.748228	69207.912404	47.491521
2309.803790	67989.479423	47.496525
2305.988660	66763.999639	47.501530
2302.589518	65557.485769	47.506535
2298.747300	64340.593983	47.511540
2295.550039	63117.211627	47.516545
2291.554472	61916.569327	47.521549
2287.983955	60709.350227	47.526554
2284.574287	59507.343258	47.531559
2280.872985	58305.472631	47.536564
2277.447920	57109.874615	47.541569
2273.822195	55907.552757	47.546573
2269.830440	54708.178187	47.551578
2266.216168	53521.430171	47.556583
2262.523317	52328.651165	47.561588
2258.929943	51143.339318	47.566593
2255.125072	49962.199630	47.571597
2251.330093	48792.218958	47.576602
2247.876670	47610.871998	47.581607
2243.929305	46447.929435	47.586612
2240.191665	45269.951408	47.591617
2236.496897	44116.881394	47.596621
2232.939602	42960.241060	47.601626
2229.040163	41814.386408	47.606631
2225.228544	40671.563943	47.611636
2221.652674	39525.289577	47.616641
2217.796268	38390.518754	47.621645
2214.211619	37250.439469	47.626650
2210.319406	36133.493283	47.631655
2206.358050	35018.137564	47.636660
2203.129566	33906.516204	47.641665
2199.186959	32789.968912	47.646669
2195.505272	31691.902835	47.651674
2191.755553	30585.837156	47.656679
2188.026487	29486.715840	47.661684
2184.310871	28390.318773	47.666689
2180.226159	27312.889670	47.671693
2176.479031	26225.738230	47.676698
2172.979507	25152.868640	47.681703
2168.938028	24088.282181	47.686708
2165.245862	23027.714092	47.691713
2161.481486	21983.545295	47.696717
2157.770015	20937.243916	47.701722
2154.030489	19903.480984	47.706727
2149.987170	18861.262608	47.711732
2146.317355	17835.230230	47.716737
2141.942923	16826.867592	47.721741
2138.080368	15812.986596	47.726746
2134.382847	14816.050934	47.731751
2130.042747	13834.037903	47.736756
2126.023408	12863.229785	47.741761
2121.341450	11912.000736	47.746765
2116.564543	10986.397559	47.751770
2110.937540	10103.043296	47.756775
2105.679133	9241.786653	47.761780
2100.644393	8406.259000	47.766785
2095.063580	7602.515278	47.771789
2090.086059	6817.211544	47.776794
2085.117423	6071.985088	47.781799
2079.605117	5357.704992	47.786804
2074.990232	4670.426977	47.791809
2070.056768	4025.357192	47.796813
2064.695752	3402.854049	47.801818
2058.766817	2857.774983	47.806823
2052.377784	2349.002180	47.811828
2046.743544	1871.862081	47.816833
2040.478042	1451.369125	47.821837
2034.480340	1066.948646	47.826842
2029.270171	718.602444	47.831847
2024.085529	407.763836	47.836852
2019.005479	146.362039	47.841857
2006.653154	114.966769	47.846861
1994.960964	137.282107	47.851866
1988.959688	139.170217	47.856871
1986.124985	147.880825	47.861876
1985.086663	157.740410	47.866881
1984.339248	142.221520	47.871885
1983.415447	141.125753	47.876890
1981.949723	140.032522	47.881895
1979.384053	149.539456	47.886900
1976.668755	139.491900	47.891905
1973.343493	144.058696	47.896909
1970.533639	139.834767	47.901914
1967.578672	140.366664	47.906919
1963.899036	140.550033	47.911924
1960.979005	133.264925	47.916929
1957.086640	142.087250	47.921933
1954.294715	146.570597	47.926938
1951.335516	135.691159	47.931943
1947.985746	146.383843	47.936948
1945.030022	133.925104	47.941953
1941.741287	134.790818	47.946957
1938.064845	123.004868	47.951962
1934.911397	130.363771	47.956967
1931.157827	138.544270	47.961972
1928.096635	131.597647	47.966977
1924.637253	139.921945	47.971981
1921.578907	138.720423	47.976986
1918.388850	141.937261	47.981991
1915.059999	138.228009	47.986996
1912.038657	131.638998	47.992001
1908.287523	130.144082	47.997005
1904.523530	132.444630	48.002010
1901.428625	130.989400	48.007015
1897.502843	140.955956	48.012020
1894.331246	133.071139	48.017025
1890.594236	135.968600	48.022029
1887.493183	135.545750	48.027034
1884.005303	133.876766	48.032039
1880.691940	132.724655	48.037044
1877.125650	126.363307	48.042049
1873.871386	143.020726	48.047053
1870.743313	140.052049	48.052058
1866.884236	146.626027	48.057063
1863.504909	141.728757	48.062068
1860.423229	133.200276	48.067073
1856.312009	145.435867	48.072077
1853.246334	132.785556	48.077082
1850.242118	134.378752	48.082087
1846.217613	140.921673	48.087092
1843.206883	139.314079	48.092097
1839.234676	140.979661	48.097101
1835.862604	131.980926	48.102106
1832.766736	131.028920	48.107111
1829.103627	132.304440	48.112116
1825.974968	134.875761	48.117121
1821.952600	139.811122	48.122125
1818.908325	135.522682	48.127130
1815.716541	135.386143	48.132135
1811.869285	136.348791	48.137140
1808.574051	124.576011	48.142145
1804.631673	125.831965	48.147149
1801.473843	132.147519	48.152154
1797.925901	136.761864	48.157159
1794.323275	143.226126	48.162164
1791.375752	130.395996	48.167169
1787.198803	143.670140	48.172173
1783.929594	138.983464	48.177178
1780.551000	137.474588	48.182183
1776.914063	134.060379	48.187188
1774.071420	141.054301	48.192193
1770.423115	130.346053	48.197197
1766.719945	129.220180	48.202202
1762.854179	127.091506	48.207207
1759.375632	140.753081	48.212212
1756.546071	136.756935	48.217217
1753.123546	143.610651	48.222221
1749.375376	144.500866	48.227226
1746.014871	125.224200	48.232231
1742.534404	137.240881	48.237236
1739.065276	137.929238	48.242241
1735.349544	139.276302	48.247245
1731.548701	131.635558	48.252250
1728.346311	129.893475	48.257255
1724.772619	140.105543	48.262260
1721.510306	129.643802	48.267265
1718.293094	129.337262	48.272269
1714.406076	130.897805	48.277274
1711.029381	136.494641	48.282279
1707.591524	136.190996	48.287284
1704.236721	126.746677	48.292289
1700.576620	127.398493	48.297293
1696.640886	129.836723	48.302298
1693.634079	131.199407	48.307303
1690.069070	134.743913	48.312308
1686.882995	131.467992	48.317313
1683.225869	129.809746	48.322317
1679.612608	132.574011	48.327322
1676.187889	131.664027	48.332327
1672.424286	133.800073	48.337332
1669.279563	126.129442	48.342337
1665.625319	130.127695	48.347341
1661.921294	128.840639	48.352346
1658.622265	125.538112	48.357351
1654.950506	124.768042	48.362356
1651.847282	119.732729	48.367361
1648.142828	128.867425	48.372365
1644.826861	130.506304	48.377370
1641.329115	129.933637	48.382375
1637.503726	129.915300	48.387380
1634.444819	121.864247	48.392385
1630.669970	134.623069	48.397389
1627.371031	123.932979	48.402394
1623.954718	124.787118	48.407399
1619.989866	129.634449	48.412404
1616.714487	138.249575	48.417409
1613.435286	134.744637	48.422413
1609.800881	129.975974	48.427418
1606.496017	130.508948	48.432423
1602.873609	130.496821	48.437428
1599.289547	132.522533	48.442433
1595.808227	136.053971	48.447437
1592.345834	127.762353	48.452442
1588.796509	113.798938	48.457447
1585.432322	122.231806	48.462452
1582.311489	128.165126	48.467457
1578.504494	128.957038	48.472461
1574.703492	126.109602	48.477466
1570.935430	114.521668	48.482471
1567.453491	122.840090	48.487476
1564.585400	123.000988	48.492481
1560.951463	124.635875	48.497485
1557.669893	122.029859	48.502490
1553.792919	119.045624	48.507495
1550.133922	125.844649	48.512500
1547.142924	108.921108	48.517505
1543.598769	119.856271	48.522509
1539.664608	125.132270	48.527514
1536.427623	119.089687	48.532519
1533.029984	124.468380	48.537524
1529.315467	122.161097	48.542529
1525.829272	124.858067	48.547533
1522.338202	115.403518	48.552538
1519.438987	113.019252	48.557543
1515.410825	119.429967	48.562548
1511.587572	112.476224	48.567553
1508.258549	119.154009	48.572557
1504.998981	115.668187	48.577562
1501.624869	114.313735	48.582567
1497.996310	121.231400	48.587572
1494.438466	112.891494	48.592577
1491.034676	115.126311	48.597581
1487.387024	112.691519	48.602586
1484.140788	110.399547	48.607591
1480.378881	118.745993	48.612596
1476.883195	113.167881	48.617601
1473.329547	123.066812	48.622605
1470.036468	117.362074	48.627610
1466.686927	112.469790	48.632615
1463.013022	112.911874	48.637620
1459.613773	104.518688	48.642625
1455.766490	114.476236	48.647629
1452.153892	105.334982	48.652634
1448.753162	113.640720	48.657639
1445.026654	116.789792	48.662644
1441.871225	108.140143	48.667649
1438.535796	101.840924	48.672653
1435.086768	115.279627	48.677658
1431.880119	102.357342	48.682663
1428.065756	117.422492	48.687668
1424.471737	112.663406	48.692673
1420.991648	109.300721	48.697677
1417.401179	115.813803	48.702682
1413.881949	108.559411	48.707687
1410.256113	115.293172	48.712692
1406.840886	113.426320	48.717697
1403.207652	106.730792	48.722701
1399.835267	109.590324	48.727706
1396.590471	112.372936	48.732711
1392.951630	119.412467	48.737716
1389.881946	102.238722	48.742721
1385.904174	105.287934	48.747725
1382.662992	104.305031	48.752730
1379.268898	108.550559	48.757735
1375.213116	112.295374	48.762740
1371.969612	112.844130	48.767745
1368.318253	115.598641	48.772749
1364.995542	114.736075	48.777754
1361.357692	117.899772	48.782759
1357.883728	111.770966	48.787764
1354.531388	102.782009	48.792769
1350.972567	105.705542	48.797773
1347.528909	113.081535	48.802778
1344.287262	104.758641	48.807783
1340.654723	120.035804	48.812788
1336.742867	110.492179	48.817793
1333.286298	116.133258	48.822797
1329.963576	117.298719	48.827802
1326.815343	105.579078	48.832807
1322.767093	111.009052	48.837812
1319.544199	104.353733	48.842817
1316.146974	113.082911	48.847821
1312.362403	112.124980	48.852826
1308.704288	110.688500	48.857831
1305.098205	116.153671	48.862836
1301.833070	106.996056	48.867841
1298.299415	114.041295	48.872845
1294.804213	115.885515	48.877850
1291.632364	111.522315	48.882855
1288.029865	117.755740	48.887860
1284.599822	100.027839	48.892865
1281.090992	113.646785	48.897869
1277.423458	107.162328	48.902874
1274.349757	104.103086	48.907879
1270.532178	114.233213	48.912884
1267.260525	114.912962	48.917889
1263.302544	105.155128	48.922893
1259.665827	104.942882	48.927898
1256.116690	103.888005	48.932903
1252.616049	105.559080	48.937908
1249.407456	106.159359	48.942913
1245.855022	112.055921	48.947917
1242.047791	111.614104	48.952922
1238.964087	113.248389	48.957927
1235.536723	109.501025	48.962932
1231.938996	106.454227	48.967937
1228.543014	106.568145	48.972941
1224.724218	105.334027	48.977946
1221.561961	99.928455	48.982951
1218.023387	103.652473	48.987956
1214.337407	87.201741	48.992961
1210.647857	100.010573	48.997965
1207.398031	100.348396	49.002970
1203.842278	111.769522	49.007975
1200.174646	105.259804	49.012980
1196.939691	98.606423	49.017985
1193.603092	98.366200	49.022989
1189.949214	101.358452	49.027994
1186.924640	111.310672	49.032999
1182.983050	111.133527	49.038004
1179.103282	109.867842	49.043009
1175.541474	106.809116	49.048013
1171.973078	108.430713	49.053018
1168.785284	100.583526	49.058023
1165.402140	120.238379	49.063028
1161.941025	108.048923	49.068033
1158.530898	106.912207	49.073037
1155.047479	108.539490	49.078042
1151.924004	99.283832	49.083047
1147.824774	107.642055	49.088052
1144.397683	96.956430	49.093057
1140.791823	102.212803	49.098061
1136.899409	97.696711	49.103066
1133.780221	99.820646	49.108071
1130.441991	106.651836	49.113076
1127.090150	96.432175	49.118081
1123.312150	97.150114	49.123085
1119.577316	103.021485	49.128090
1116.234687	105.762550	49.133095
1112.633060	105.712547	49.138100
1109.561659	102.197412	49.143105
1106.101514	111.528130	49.148109
1102.434757	101.221737	49.153114
1099.152082	103.529469	49.158119
1094.892761	108.517999	49.163124
1092.019090	90.051352	49.168129
1088.047405	106.384590	49.173133
1084.688775	103.401660	49.178138
1081.761722	106.697782	49.183143
1077.830421	108.142107	49.188148
1074.159339	104.499404	49.193153
1070.523763	102.777910	49.198157
1066.857216	101.962953	49.203162
1063.576366	108.241002	49.208167
1060.635248	104.098032	49.213172
1057.342751	102.430398	49.218177
1053.311354	113.350220	49.223181
1049.843726	104.259217	49.228186
1046.364284	99.536135	49.233191
1042.451468	108.893450	49.238196
1039.509276	98.903924	49.243201
1036.072308	100.463862	49.248205
1032.536293	102.985291	49.253210
1029.015450	94.668277	49.258215
1025.062367	104.702629	49.263220
1021.809967	100.231917	49.268225
1018.472400	105.999992	49.273229
1014.945984	109.320370	49.278234
1011.542487	105.930032	49.283239
1007.546046	109.491687	49.288244
1004.083500	97.416433	49.293249
1000.896793	94.438256	49.298253
997.126231	106.547977	49.303258
993.785941	97.051079	49.308263
990.231749	98.233911	49.313268
986.953788	96.497587	49.318273
983.258421	95.231586	49.323277
979.734170	90.724362	49.328282
976.173632	93.471115	49.333287
972.547335	99.989941	49.338292
969.267046	96.169035	49.343297
965.871568	92.929324	49.348301
961.794350	99.708585	49.353306
958.660103	103.799660	49.358311
955.170136	102.194620	49.363316
951.657473	85.830788	49.368321
948.313914	98.167893	49.373325
944.638123	89.742300	49.378330
941.359057	94.292660	49.383335
937.681123	92.128590	49.388340
934.298168	91.174367	49.393345
930.636990	97.081724	49.398349
927.270193	96.764064	49.403354
923.864411	93.174800	49.408359
920.080901	103.514834	49.413364
916.815376	106.753265	49.418369
913.145204	108.906593	49.423373
909.649537	109.960066	49.428378
906.340588	95.798003	49.433383
902.665994	90.827124	49.438388
899.089462	90.428417	49.443393
895.810569	101.720846	49.448397
892.500886	98.954956	49.453402
888.926681	89.102423	49.458407
884.963528	97.686206	49.463412
881.508483	98.957958	49.468417
877.706505	97.487227	49.473421
874.065082	99.525333	49.478426
871.188759	93.141799	49.483431
867.670050	99.577372	49.488436
864.137618	97.865120	49.493441
860.727997	104.970162	49.498445
857.001321	103.860977	49.503450
854.171270	101.814114	49.508455
850.217625	97.064125	49.513460
846.642259	93.204048	49.518465
843.130347	102.400571	49.523469
839.589748	95.950220	49.528474
836.498960	93.108946	49.533479
832.909800	101.409555	49.538484
829.054304	94.385247	49.543489
825.554928	98.919520	49.548493
821.964869	93.492505	49.553498
818.673685	90.600359	49.558503
815.067130	96.043613	49.563508
811.573513	93.853896	49.568513
808.190759	91.181740	49.573517
804.315872	92.924231	49.578522
800.575755	96.290800	49.583527
797.106888	89.848219	49.588532
794.264367	95.086414	49.593537
790.794846	91.247752	49.598541
787.199233	87.001724	49.603546
784.174052	88.782010	49.608551
779.818406	97.436782	49.613556
776.444112	94.839245	49.618561
772.864085	88.543798	49.623565
769.531030	86.502965	49.628570
766.183311	92.826369	49.633575
762.667091	105.089321	49.638580
758.993676	105.430351	49.643585
755.476702	98.166401	49.648589
752.118725	98.385270	49.653594
748.809529	92.974416	49.658599
744.912329	102.310399	49.663604
741.274447	96.748535	49.668609
738.072151	93.136970	49.673613
734.542987	96.590753	49.678618
731.029515	95.017956	49.683623
727.949791	96.648610	49.688628
724.538632	91.070234	49.693633
720.900349	90.285791	49.698637
716.902304	92.354492	49.703642
713.748532	89.444031	49.708647
709.797244	96.108750	49.713652
706.341545	96.175258	49.718657
702.808386	98.430595	49.723661
699.418183	100.821738	49.728666
696.164178	82.883088	49.733671
692.406675	93.712669	49.738676
689.108757	96.763252	49.743681
685.543810	89.260072	49.748685
681.915337	90.495780	49.753690
678.912065	83.913898	49.758695
674.704074	90.992158	49.763700
671.282663	91.632285	49.768705
668.152882	86.474948	49.773709
664.812285	79.398562	49.778714
660.790296	94.651440	49.783719
657.313824	97.783781	49.788724
654.077027	91.311245	49.793729
650.628728	89.272686	49.798733
647.071594	92.680258	49.803738
643.117183	90.198935	49.808743
639.568213	99.470925	49.813748
636.222482	92.670601	49.818753
633.275479	88.196508	49.823757
629.535682	101.674606	49.828762
625.990828	90.523604	49.833767
622.471207	86.626418	49.838772
619.054142	102.303440	49.843777
615.609137	97.049952	49.848781
612.072042	92.586022	49.853786
608.327252	87.199153	49.858791
604.768421	97.459803	49.863796
601.278366	89.122344	49.868801
597.807522	92.763196	49.873805
594.268896	89.207525	49.878810
591.112577	89.293629	49.883815
587.231525	91.236492	49.888820
584.035539	88.592122	49.893825
580.222445	86.601232	49.898829
576.799073	93.581958	49.903834
573.454860	86.091718	49.908839
569.893191	86.744357	49.913844
566.673363	79.500401	49.918849
563.484513	86.669029	49.923853
559.524428	86.646906	49.928858
555.733692	98.247377	49.933863
552.087919	89.235128	49.938868
549.046130	90.821933	49.943873
545.726426	92.186506	49.948877
541.624102	83.714013	49.953882
538.456133	85.162393	49.958887
534.716993	91.686380	49.963892
531.203135	81.030455	49.968897
527.593246	88.369443	49.973901
523.975383	89.448523	49.978906
520.863112	90.682539	49.983911
517.433790	88.432249	49.988916
513.743162	86.362095	49.993921
510.355251	97.111702	49.998925
506.641415	98.553839	50.003930
503.778470	84.695453	50.008935
499.896025	87.502287	50.013940
496.201370	90.064571	50.018945
492.637464	87.041258	50.023949
489.503155	93.616064	50.028954
485.488909	91.299211	50.033959
482.042004	90.450088	50.038964
479.041963	89.091208	50.043969
475.785180	84.010786	50.048973
471.878445	100.216960	50.053978
468.435834	94.479099	50.058983
464.480683	87.565493	50.063988
461.194012	94.648233	50.068993
457.912201	88.901012	50.073997
454.385733	95.916909	50.079002
450.776983	92.207763	50.084007
447.180397	92.429315	50.089012
443.849441	91.834133	50.094017
440.159767	93.202908	50.099021
436.553866	95.700694	50.104026
433.526256	91.834092	50.109031
429.883322	98.010851	50.114036
426.160464	88.131202	50.119041
422.638234	93.396865	50.124045
418.853221	98.621432	50.129050
416.085426	89.807091	50.134055
412.330281	94.153774	50.139060
408.447838	89.421317	50.144065
405.152599	80.531411	50.149069
401.409881	91.782716	50.154074
397.925709	78.277955	50.159079
394.862828	83.689977	50.164084
391.503919	85.405599	50.169089
388.127579	82.390916	50.174093
384.213692	85.060351	50.179098
381.013353	85.941209	50.184103
377.027816	93.117624	50.189108
373.298286	86.795154	50.194113
370.262718	82.781126	50.199117
366.896948	85.760186	50.204122
363.349620	82.623598	50.209127
359.956945	91.792094	50.214132
355.769286	91.176112	50.219137
352.560263	80.956586	50.224141
348.697543	83.795193	50.229146
345.753435	83.035047	50.234151
342.214314	80.349605	50.239156
338.911419	89.013655	50.244161
335.048398	85.698736	50.249165
331.519625	96.394527	50.254170
327.771411	82.193995	50.259175
324.537284	95.213315	50.264180
321.453902	90.934706	50.269185
317.969328	83.457074	50.274189
314.125905	82.973854	50.279194
310.660750	84.766261	50.284199
306.969257	97.816101	50.289204
303.378369	83.148006	50.294209
299.917685	86.894940	50.299213
297.059270	90.215335	50.304218
293.136133	82.221112	50.309223
289.825155	90.051202	50.314228
286.241410	90.479618	50.319233
282.671489	84.413767	50.324237
279.165739	87.860881	50.329242
275.816303	80.627859	50.334247
271.809499	84.447697	50.339252
268.508898	83.189757	50.344257
264.849350	76.419777	50.349261
261.278613	95.082260	50.354266
258.477513	78.860437	50.359271
254.989757	83.655679	50.364276
251.243563	81.885412	50.369281
247.479883	84.132736	50.374285
243.803947	87.555902	50.379290
240.494493	78.576548	50.384295
236.925601	86.937443	50.389300
233.687625	83.008959	50.394305
230.279791	79.619620	50.399309
226.276495	83.021307	50.404314
222.955573	83.639532	50.409319
219.216105	90.673055	50.414324
215.992860	87.681915	50.419329
212.932565	75.205520	50.424333
208.982038	84.654440	50.429338
206.068023	85.841685	50.434343
202.085452	87.180510	50.439348
198.558618	88.103088	50.444353
194.944572	86.464005	50.449357
191.471869	86.596650	50.454362
187.857895	82.932734	50.459367
184.717914	83.203085	50.464372
180.982648	85.882588	50.469377
177.763458	83.988663	50.474381
173.813889	93.383666	50.479386
170.467710	80.711626	50.484391
166.712237	90.266050	50.489396
163.335339	89.754103	50.494401
159.830481	78.796391	50.499405
156.210748	88.478251	50.504410
153.098722	81.888304	50.509415
149.373361	90.631251	50.514420
145.978018	83.883209	50.519425
142.514708	78.351222	50.524429
138.799892	85.064531	50.529434
135.560627	80.139696	50.534439
131.822083	87.846991	50.539444
128.497187	88.725305	50.544449
125.050141	84.731541	50.549453
121.701943	91.722783	50.554458
118.416446	85.315052	50.559463
114.640465	86.039413	50.564468
110.918205	82.778478	50.569473
107.438559	83.959458	50.574477
103.852963	89.269961	50.579482
100.295552	78.636892	50.584487
96.607635	82.254983	50.589492
93.560289	85.820174	50.594497
89.880896	91.721188	50.599501
86.225907	88.174474	50.604506
83.025340	82.414685	50.609511
79.639170	86.874532	50.614516
75.914904	85.123054	50.619521
72.535800	84.272963	50.624525
68.828134	81.952570	50.629530
65.604951	88.791364	50.634535
61.836624	79.064563	50.639540
58.397660	75.866838	50.644545
55.001466	78.958344	50.649549
51.378635	82.699134	50.654554
47.896456	79.742303	50.659559
44.306330	93.333166	50.664564
40.796484	77.833099	50.669569
37.121368	75.912585	50.674573
34.032435	81.407891	50.679578
30.440415	76.165043	50.684583
27.200593	80.288763	50.689588
23.280781	81.538739	50.694593
19.553613	81.777762	50.699597
16.220572	82.258757	50.704602
12.841854	82.095171	50.709607
9.518093	80.103800	50.714612
5.975269	73.141650	50.719617
2.556445	79.005030	50.724621