Thu Aug 25 13:21:41 2022

Number of Points = 9925

Depth (nm)	Load (N)	Time (s)
1.118666	99.671150	0.000000
1.199318	109.618025	0.005005
1.462350	106.314854	0.010010
1.321149	109.067234	0.015014
1.793780	101.909368	0.020019
1.657673	106.682609	0.025024
1.656643	100.060871	0.030029
0.903071	87.096595	0.035034
0.971048	82.337011	0.040038
0.900222	76.074233	0.045043
0.405410	57.969418	0.050048
0.613935	53.792103	0.055053
0.575958	48.663149	0.060058
-0.103486	45.317831	0.065062
-0.323912	32.589602	0.070067
-0.842263	26.226117	0.075072
-0.927278	14.928857	0.080077
-1.527311	8.068809	0.085082
-1.902475	13.933017	0.090086
-1.905411	5.982828	0.095091
-2.493178	6.941701	0.100096
-2.658212	2.743833	0.105101
-2.859766	1.114341	0.110106
-3.321642	5.195112	0.115110
-3.196831	-5.923038	0.120115
-4.053955	-3.023702	0.125120
-4.078565	-8.752686	0.130125
-3.906428	-6.565112	0.135130
-4.192271	4.021259	0.140134
-4.352273	-14.949028	0.145139
-5.068342	-4.557846	0.150144
-5.472079	-8.575941	0.155149
-5.423048	-8.862127	0.160154
-5.649070	-4.603176	0.165158
-5.430864	-7.165309	0.170163
-6.291769	-0.326488	0.175168
-6.742318	-6.248165	0.180173
-6.661702	-10.158651	0.185178
-6.905562	6.217166	0.190182
-6.898112	-2.582536	0.195187
-7.756501	2.449380	0.200192
-8.087420	-2.399542	0.205197
-8.262902	-6.896328	0.210202
-8.755012	-0.798665	0.215206
-8.542676	-8.548458	0.220211
-8.666113	-1.040571	0.225216
-8.935644	-3.573741	0.230221
-9.350896	7.314484	0.235226
-9.980441	-2.584481	0.240230
-10.071726	-0.475856	0.245235
-10.293971	2.665694	0.250240
-9.997641	-1.936656	0.255245
-10.176175	-12.320735	0.260250
-10.588442	-5.469951	0.265254
-10.854117	-8.854778	0.270259
-11.126898	-6.379193	0.275264
-11.264965	-0.881171	0.280269
-11.792782	-5.389192	0.285274
-12.395005	0.981990	0.290278
-12.653670	-4.637556	0.295283
-12.539704	-4.142975	0.300288
-12.776322	1.620428	0.305293
-12.929167	-9.159985	0.310298
-13.155840	-5.938648	0.315302
-13.398080	-10.133907	0.320307
-14.394544	-9.908268	0.325312
-14.671112	-5.204798	0.330317
-14.564736	-13.735255	0.335322
-14.499510	-8.933478	0.340326
-14.545778	-5.398721	0.345331
-14.954999	-3.977439	0.350336
-14.880398	-4.647285	0.355341
-15.082345	-9.320258	0.360346
-15.868677	-9.108560	0.365350
-15.656215	-13.270658	0.370355
-16.211236	-5.324991	0.375360
-16.976855	-11.618080	0.380365
-17.213381	-15.238427	0.385370
-17.604241	-5.122827	0.390374
-17.455689	-11.049785	0.395379
-17.260602	-8.308985	0.400384
-17.644882	-4.711775	0.405389
-17.434251	-15.498514	0.410394
-18.405201	-6.285447	0.415398
-18.584952	-5.437960	0.420403
-18.915742	-5.152105	0.425408
-18.902082	4.039573	0.430413
-19.065115	-9.485394	0.435418
-19.972546	-2.000202	0.440422
-20.062544	0.541657	0.445427
-20.441882	4.115948	0.450432
-20.797609	-0.118479	0.455437
-20.559211	-3.047609	0.460442
-20.583059	1.486551	0.465446
-20.572049	-5.867864	0.470451
-20.892210	2.294109	0.475456
-21.316100	8.235553	0.480461
-21.509267	-4.345057	0.485466
-22.186493	14.588553	0.490470
-22.574309	3.430496	0.495475
-23.090517	4.466743	0.500480
-23.369964	4.886924	0.505485
-23.190341	9.202543	0.510490
-23.236570	4.524150	0.515494
-23.186209	-4.642943	0.520499
-23.369180	4.152435	0.525504
-24.146914	9.510240	0.530509
-24.250448	-0.281316	0.535514
-24.746585	6.456062	0.540518
-24.515998	-0.777734	0.545523
-24.964799	8.524371	0.550528
-25.253108	5.256985	0.555533
-25.820998	-0.412187	0.560538
-25.950299	1.708722	0.565542
-26.093666	-2.090740	0.570547
-26.259739	1.614651	0.575552
-26.576829	7.722859	0.580557
-26.630424	-5.993264	0.585562
-27.719159	0.719903	0.590566
-27.404871	-9.010563	0.595571
-27.924216	2.824115	0.600576
-28.376661	8.722577	0.605581
-28.152421	8.605091	0.610586
-28.203125	-0.185499	0.615590
-27.975047	-1.338138	0.620595
-28.286999	5.209028	0.625600
-28.766860	6.400933	0.630605
-29.105597	3.340766	0.635610
-29.252733	3.015713	0.640614
-29.508792	-2.844688	0.645619
-29.566442	-0.953306	0.650624
-30.496483	6.019738	0.655629
-30.255087	2.210609	0.660634
-31.167907	3.017933	0.665638
-31.198452	3.171324	0.670643
-31.566579	9.853844	0.675648
-31.623763	9.957624	0.680653
-31.694827	-0.300929	0.685658
-31.961506	9.089701	0.690662
-32.476383	9.657502	0.695667
-32.924380	-3.171082	0.700672
-32.988090	6.557905	0.705677
-32.499557	-2.374122	0.710682
-32.882466	-8.097585	0.715686
-33.284365	-3.466227	0.720691
-34.119863	-1.149246	0.725696
-34.425633	2.049684	0.730701
-34.306974	-1.512421	0.735706
-34.662712	6.104632	0.740710
-34.674232	4.831346	0.745715
-35.348429	8.587879	0.750720
-35.718750	-1.525706	0.755725
-35.855627	-7.797086	0.760730
-36.049293	3.565783	0.765734
-36.228955	1.698743	0.770739
-36.258062	1.117914	0.775744
-36.324903	-2.804270	0.780749
-36.431156	3.349996	0.785754
-37.145810	13.291712	0.790758
-37.557528	-5.683432	0.795763
-37.833566	-13.109926	0.800768
-37.587520	-6.106026	0.805773
-37.729980	-7.846016	0.810778
-38.820466	-0.502984	0.815782
-38.716895	-6.875314	0.820787
-39.136066	-5.582187	0.825792
-39.319451	-1.497596	0.830797
-39.131162	-10.477488	0.835802
-39.233568	-8.588586	0.840806
-39.993350	-11.165160	0.845811
-40.774805	-8.938905	0.850816
-41.158804	-6.667358	0.855821
-40.741538	-7.596539	0.860826
-40.959135	-3.829292	0.865830
-40.626791	-3.884622	0.870835
-40.817470	-1.485176	0.875840
-41.072346	3.170604	0.880845
-41.303519	-5.101321	0.885850
-41.713115	-0.674401	0.890854
-42.420695	-4.841039	0.895859
-43.118363	0.298574	0.900864
-43.517309	-0.078774	0.905869
-43.512194	-6.138282	0.910874
-43.606085	-8.211750	0.915878
-43.592654	-10.773434	0.920883
-43.770831	-4.889477	0.925888
-43.621011	-1.828371	0.930893
-43.690504	-2.798343	0.935898
-44.471338	3.142079	0.940902
-44.772794	-2.682733	0.945907
-44.806189	-8.818464	0.950912
-45.676869	-10.561411	0.955917
-45.579744	-9.402964	0.960922
-46.399366	6.885892	0.965926
-46.519095	-5.184198	0.970931
-46.795003	-10.487825	0.975936
-47.007720	-11.327788	0.980941
-46.606366	-8.299768	0.985946
-46.731078	-2.262835	0.990950
-46.432357	-4.907186	0.995955
-47.039367	-5.878358	1.000960
-47.674045	-7.405181	1.005965
-48.514972	-8.450433	1.010970
-49.315969	3.589728	1.015974
-49.043461	0.041482	1.020979
-48.562685	-5.877421	1.025984
-48.853330	-7.186065	1.030989
-48.994378	-7.236824	1.035994
-49.316876	-8.224101	1.040998
-50.166787	-10.561925	1.046003
-50.567181	-3.516849	1.051008
-51.031200	4.648683	1.056013
-50.777846	-13.918127	1.061018
-50.753067	-2.557853	1.066022
-50.645994	-10.379735	1.071027
-50.822522	-5.853293	1.076032
-51.852984	-2.983741	1.081037
-52.153972	-4.369859	1.086042
-52.024075	-5.589373	1.091046
-52.177076	-17.062617	1.096051
-52.337744	-8.492204	1.101056
-53.097686	-1.223111	1.106061
-53.319776	-7.500120	1.111066
-53.572247	-1.411531	1.116070
-53.456128	-6.558285	1.121075
-53.547305	-4.411712	1.126080
-54.027536	-3.852502	1.131085
-54.449202	-4.998248	1.136090
-55.167843	1.701225	1.141094
-55.188941	-2.041463	1.146099
-54.962299	3.038745	1.151104
-55.186269	-5.898699	1.156109
-54.942419	-8.468013	1.161114
-56.164230	3.040132	1.166118
-56.203897	-1.468442	1.171123
-56.720183	2.902430	1.176128
-56.893231	6.476036	1.181133
-57.136969	1.104091	1.186138
-57.174636	3.944636	1.191142
-57.286965	0.646515	1.196147
-57.970320	-0.891664	1.201152
-58.238686	-2.187980	1.206157
-58.438914	-6.351854	1.211162
-58.246717	2.941560	1.216166
-57.941262	8.850983	1.221171
-58.342491	7.961463	1.226176
-59.548099	6.378564	1.231181
-59.297100	-4.287953	1.236186
-59.702327	6.892929	1.241190
-59.983886	0.081067	1.246195
-60.031298	3.998821	1.251200
-60.924765	8.568000	1.256205
-61.060100	2.676029	1.261210
-61.131457	5.445923	1.266214
-61.417613	-4.373960	1.271219
-61.479555	-4.373838	1.276224
-61.418558	-0.998258	1.281229
-61.343174	5.295227	1.286234
-62.217651	5.944685	1.291238
-62.650415	-1.020655	1.296243
-62.836167	3.345883	1.301248
-62.737806	-2.696599	1.306253
-63.147157	-2.952091	1.311258
-63.310933	6.071233	1.316262
-63.544503	-7.844475	1.321267
-63.839860	-8.247544	1.326272
-64.486607	-6.295496	1.331277
-64.087159	-8.307057	1.336282
-64.325777	-4.628266	1.341286
-64.816796	-8.135969	1.346291
-65.324933	-5.455827	1.351296
-65.452228	2.343730	1.356301
-65.152127	-6.542950	1.361306
-65.897642	-5.758675	1.366310
-66.476014	-3.712935	1.371315
-66.921741	-11.283682	1.376320
-67.543465	-2.185443	1.381325
-67.192407	-5.499222	1.386330
-66.992183	-10.567404	1.391334
-67.175011	-6.900518	1.396339
-67.096311	-2.746262	1.401344
-67.804668	-4.957568	1.406349
-68.112581	-6.788691	1.411354
-68.667526	-4.047430	1.416358
-68.806035	-2.295240	1.421363
-68.790857	-5.357073	1.426368
-68.665694	8.221095	1.431373
-69.430929	6.505921	1.436378
-70.057483	-1.482588	1.441382
-70.309031	-9.830410	1.446387
-69.880505	-8.784002	1.451392
-70.511796	-4.727307	1.456397
-70.305624	0.144133	1.461402
-71.053792	-1.646481	1.466406
-71.533919	-5.918358	1.471411
-71.402932	0.505618	1.476416
-71.872451	1.784489	1.481421
-71.501054	-11.390773	1.486426
-72.126233	4.434177	1.491430
-72.843945	4.268131	1.496435
-73.286935	10.095509	1.501440
-73.334162	8.723413	1.506445
-73.023553	0.208408	1.511450
-73.192355	-1.897615	1.516454
-73.564697	3.953493	1.521459
-73.114860	0.263565	1.526464
-74.243376	4.202019	1.531469
-74.316996	-6.692043	1.536474
-74.714321	-5.041668	1.541478
-74.813631	-3.096302	1.546483
-75.446817	0.713917	1.551488
-76.027992	4.354636	1.556493
-75.907998	-2.570763	1.561498
-76.313959	8.221091	1.566502
-76.389713	1.383310	1.571507
-76.410279	-3.419322	1.576512
-76.502023	1.593712	1.581517
-76.312780	-0.799367	1.586522
-76.764519	3.270325	1.591526
-77.161847	0.867915	1.596531
-77.582929	4.008984	1.601536
-78.188516	9.380946	1.606541
-78.450117	-4.960643	1.611546
-78.993095	3.024269	1.616550
-79.231522	-3.063517	1.621555
-79.438848	3.587477	1.626560
-79.446542	-1.906874	1.631565
-79.022113	1.082728	1.636570
-79.158753	7.890327	1.641574
-79.465007	5.777368	1.646579
-80.070479	4.720535	1.651584
-80.873065	6.927960	1.656589
-80.480798	-5.200205	1.661594
-80.744797	-8.101234	1.666598
-81.180994	-7.261020	1.671603
-81.903859	-0.690600	1.676608
-82.430862	-2.155198	1.681613
-82.012379	5.650590	1.686618
-82.128913	-4.841277	1.691622
-82.247752	-4.082427	1.696627
-82.339109	1.019131	1.701632
-83.214437	1.633923	1.706637
-83.154926	4.756635	1.711642
-83.591308	1.695954	1.716646
-83.763765	0.495342	1.721651
-84.177013	3.413719	1.726656
-84.156932	2.318980	1.731661
-83.977992	1.889051	1.736666
-85.154759	2.253682	1.741670
-85.239741	4.029123	1.746675
-85.618269	-2.963694	1.751680
-85.602474	16.076458	1.756685
-85.438622	-6.424715	1.761690
-85.654109	0.717940	1.766694
-85.870769	1.855951	1.771699
-86.543379	1.300023	1.776704
-86.898119	10.967042	1.781709
-86.799624	6.987314	1.786714
-86.997763	2.772492	1.791718
-87.489227	5.196923	1.796723
-87.948454	1.386844	1.801728
-88.571580	2.079178	1.806733
-88.109732	0.203371	1.811738
-88.782293	3.418645	1.816742
-88.108641	5.929433	1.821747
-88.414064	7.964044	1.826752
-89.426795	7.888518	1.831757
-89.241664	2.344970	1.836762
-89.901096	-0.563701	1.841766
-89.831170	2.278967	1.846771
-90.629655	-0.424417	1.851776
-91.240135	8.393654	1.856781
-90.911309	2.353025	1.861786
-90.990953	7.158519	1.866790
-91.296233	6.987961	1.871795
-91.100036	1.790694	1.876800
-91.674033	12.365269	1.881805
-91.654713	1.659122	1.886810
-92.576458	4.416731	1.891814
-92.803108	4.031371	1.896819
-92.691718	-3.905083	1.901824
-92.958072	3.289836	1.906829
-92.832305	-0.539139	1.911834
-93.079361	11.094688	1.916838
-93.710716	1.300422	1.921843
-93.717250	-1.267626	1.926848
-94.324297	2.845385	1.931853
-94.244347	-2.374795	1.936858
-95.233357	1.124183	1.941862
-95.541868	-2.418443	1.946867
-95.998230	3.066177	1.951872
-95.968419	4.776175	1.956877
-95.656001	-0.043832	1.961882
-95.788187	-3.405278	1.966886
-95.852109	-0.279045	1.971891
-95.603458	-3.988068	1.976896
-96.623689	11.870315	1.981901
-96.791719	-1.052749	1.986906
-97.461416	5.917469	1.991910
-97.538759	0.775718	1.996915
-97.769070	-2.111176	2.006912
-97.793139	-0.498339	2.016909
-97.425535	2.250561	2.026906
-96.523951	1.811329	2.036902
-96.146042	3.997912	2.046899
-95.321923	5.439831	2.056896
-94.765460	-3.910246	2.066893
-94.644362	-0.121691	2.076890
-94.568901	0.617073	2.086886
-93.623116	6.341825	2.096883
-92.632018	3.449348	2.106880
-92.113035	-0.918216	2.116877
-91.881619	3.578485	2.126874
-92.019607	6.219707	2.136870
-91.067500	-2.387739	2.146867
-90.658895	-2.832087	2.156864
-90.134429	-0.684309	2.166861
-89.472722	3.317314	2.176858
-89.221008	-2.117107	2.186854
-88.337870	-1.495396	2.196851
-87.956366	-0.462463	2.206848
-87.609953	2.793442	2.216845
-86.710531	-0.195543	2.226842
-86.535517	5.212824	2.236838
-86.276357	5.045318	2.246835
-85.382330	4.927221	2.256832
-85.198371	4.666960	2.266829
-84.442669	3.154523	2.276826
-83.480632	3.595977	2.286822
-83.459152	4.362206	2.296819
-83.350998	0.502511	2.306816
-82.476190	4.334527	2.316813
-81.915876	2.792517	2.326810
-81.720563	1.485098	2.336806
-80.675644	12.845709	2.346803
-80.432692	2.017864	2.356800
-80.199797	5.728715	2.366797
-79.502517	7.903270	2.376794
-79.193452	7.420666	2.386790
-78.444319	7.087687	2.396787
-78.349205	3.584830	2.406784
-77.549629	0.348561	2.416781
-76.702405	4.517522	2.426778
-76.303815	2.940664	2.436774
-76.448750	2.516526	2.446771
-75.671392	6.427170	2.456768
-75.048338	2.936624	2.466765
-74.008712	6.733314	2.476762
-73.620535	7.768371	2.486758
-73.730122	0.106564	2.496755
-73.604635	3.827910	2.506752
-72.739114	5.310861	2.516749
-71.581998	8.059601	2.526746
-71.218465	3.079663	2.536742
-71.523218	6.047958	2.546739
-70.366019	3.500091	2.556736
-69.923079	1.795908	2.566733
-69.405706	2.164486	2.576730
-68.575394	-1.149458	2.586726
-68.379547	-2.640694	2.596723
-68.145307	-2.446332	2.606720
-67.427239	6.051100	2.616717
-66.957684	4.516976	2.626714
-66.817277	6.493685	2.636710
-65.627182	1.032606	2.646707
-65.347893	-1.171793	2.656704
-65.257469	-2.570483	2.666701
-64.563453	3.453484	2.676698
-64.012909	-1.812349	2.686694
-63.114625	1.984313	2.696691
-62.675497	7.509690	2.706688
-62.488500	3.577452	2.716685
-62.232704	3.340781	2.726682
-61.341736	-2.440893	2.736678
-61.067684	3.053327	2.746675
-60.612511	4.157083	2.756672
-59.695885	5.394442	2.766669
-59.514452	6.807186	2.776666
-59.007882	11.042198	2.786662
-58.192849	4.927128	2.796659
-57.985931	6.402403	2.806656
-57.633211	5.089326	2.816653
-56.535081	1.204393	2.826650
-56.526513	-0.286009	2.836646
-56.136620	1.464706	2.846643
-55.416566	-0.137177	2.856640
-54.987628	-0.141215	2.866637
-54.484418	-2.025904	2.876634
-53.915947	-1.491101	2.886630
-53.382355	1.263472	2.896627
-52.370885	-4.647956	2.906624
-52.385552	-6.410318	2.916621
-52.272803	1.158755	2.926618
-51.779638	-2.064347	2.936614
-51.012106	1.974551	2.946611
-50.076080	0.741141	2.956608
-49.384605	-0.906949	2.966605
-49.293883	-7.602278	2.976602
-49.395703	-4.025882	2.986598
-48.811962	0.307910	2.996595
-47.909164	4.227413	3.006592
-46.931607	-3.059871	3.016589
-46.397897	-2.003267	3.026586
-46.486852	1.358870	3.036582
-46.156367	5.960429	3.046579
-45.688527	5.817248	3.056576
-44.811755	2.850821	3.066573
-44.598285	0.257590	3.076570
-43.780302	0.373160	3.086566
-43.455298	9.299652	3.096563
-43.051330	4.180330	3.106560
-42.195425	6.520104	3.116557
-42.036917	5.782323	3.126554
-41.737555	3.384709	3.136550
-40.846521	7.312392	3.146547
-40.232981	3.348166	3.156544
-39.353742	1.287350	3.166541
-39.054731	2.174821	3.176538
-39.042976	8.464084	3.186534
-38.759562	1.732224	3.196531
-37.912519	-0.038444	3.206528
-37.623709	2.168438	3.216525
-36.393798	-0.431999	3.226522
-36.031927	-6.672466	3.236518
-36.158438	0.382896	3.246515
-35.764853	-2.165696	3.256512
-34.501148	-5.423998	3.266509
-34.142459	-2.721214	3.276506
-34.217660	-0.717059	3.286502
-33.185227	-3.318231	3.296499
-32.948003	-6.216126	3.306496
-32.495144	5.224587	3.316493
-32.041917	3.065795	3.326490
-31.583709	-2.619561	3.336486
-30.758338	3.418675	3.346483
-30.581586	9.530031	3.356480
-29.335499	-3.672465	3.366477
-29.093428	2.615556	3.376474
-29.002680	-0.253053	3.386470
-28.590178	6.356725	3.396467
-27.987419	6.021342	3.406464
-27.518885	5.649970	3.416461
-26.665591	2.199379	3.426458
-26.375204	-3.215759	3.436454
-25.871147	1.504324	3.446451
-25.346228	8.682537	3.456448
-24.854862	-1.956150	3.466445
-24.532854	-0.052244	3.476442
-23.322728	5.561409	3.486438
-23.246888	10.209205	3.496435
-23.242990	4.338438	3.506432
-22.367738	6.333058	3.516429
-21.626466	7.585226	3.526426
-21.424559	7.154259	3.536422
-20.930184	2.743035	3.546419
-20.151771	6.070642	3.556416
-19.982507	6.376557	3.566413
-19.380638	0.583160	3.576410
-18.797262	0.469395	3.586406
-18.442596	2.485393	3.596403
-17.311577	2.973238	3.606400
-16.954566	3.522169	3.616397
-16.715613	-1.292528	3.626394
-16.979883	1.387487	3.636390
-16.126764	6.100397	3.646387
-15.194251	10.734345	3.656384
-14.640412	6.668599	3.666381
-14.179596	7.001693	3.676378
-14.135403	3.107667	3.686374
-13.061995	2.201196	3.696371
-12.558247	-3.326568	3.706368
-12.572244	3.429231	3.716365
-11.704464	4.167398	3.726362
-11.113866	8.100977	3.736358
-11.130796	3.994781	3.746355
-10.341184	-0.412016	3.756352
-9.451526	3.344824	3.766349
-9.130817	0.389498	3.776346
-9.054947	2.417502	3.786342
-8.781200	6.315194	3.796339
-7.889612	8.370613	3.806336
-7.092563	9.278254	3.816333
-6.808231	3.807041	3.826330
-6.515590	-0.480707	3.836326
-5.974916	5.963272	3.846323
-5.382060	4.770963	3.856320
-4.549744	11.517709	3.866317
-4.409659	8.869451	3.876314
-4.030404	14.736839	3.886310
-3.384008	18.433595	3.896307
-2.897179	21.486942	3.906304
-2.640121	38.834674	3.916301
-2.171872	40.874063	3.926298
-1.406317	55.272088	3.936294
-1.118255	63.593010	3.946291
-1.093628	74.600351	3.956288
-0.486022	101.849723	3.966285
0.000000	109.716609	3.971290
0.211196	120.759853	3.976294
0.120831	123.801666	3.981299
0.693987	132.795017	3.986304
0.394337	149.989639	3.991309
0.721259	143.142491	3.996314
0.949964	150.873682	4.001318
1.200672	158.509679	4.006323
0.991486	157.140799	4.011328
0.693692	148.986805	4.016333
0.890359	149.034994	4.021338
0.784896	143.929241	4.026342
0.796985	150.055525	4.031347
1.048249	146.083466	4.036352
0.908603	148.509738	4.041357
0.939757	146.065478	4.046362
1.156502	164.220092	4.051366
1.353531	165.900743	4.056371
1.319142	155.095342	4.061376
1.008130	155.384428	4.066381
1.306332	142.789999	4.071386
1.023680	148.263265	4.076390
1.156066	147.707748	4.081395
1.373705	146.724417	4.086400
1.024701	147.595266	4.091405
1.547408	142.678996	4.096410
1.201605	147.428156	4.101414
0.934871	146.555518	4.106419
1.221942	142.514574	4.111424
1.079790	152.309718	4.116429
1.462302	160.668556	4.121434
1.388538	169.491199	4.126438
1.416562	156.600566	4.131443
1.451077	150.004878	4.136448
1.492738	144.113598	4.141453
1.346724	144.709030	4.146458
1.138091	157.656241	4.151462
1.533035	148.647052	4.156467
1.203090	151.242347	4.161472
1.383244	156.684232	4.166477
1.412365	154.021987	4.171482
1.296172	160.737858	4.176486
1.339581	167.628044	4.181491
1.687266	170.455697	4.186496
1.190259	167.230470	4.191501
1.468313	165.801067	4.196506
1.627385	172.280822	4.201510
1.416865	177.647881	4.206515
1.854873	169.694971	4.211520
1.210106	173.026140	4.216525
2.071432	167.120324	4.221530
1.255308	164.008373	4.226534
1.207894	162.759681	4.231539
1.395225	155.988185	4.236544
1.485235	173.567872	4.241549
2.068520	169.594407	4.246554
1.605037	175.361773	4.251558
1.433602	171.962146	4.256563
1.546377	185.994823	4.261568
1.398967	179.744008	4.266573
1.879984	176.596499	4.271578
1.615751	172.217977	4.276582
1.770568	176.069283	4.281587
1.773549	174.493150	4.286592
1.691110	175.818951	4.291597
1.968984	165.967543	4.296602
2.114048	177.758349	4.301606
1.667497	167.226329	4.306611
1.603720	155.220125	4.311616
1.762162	175.810519	4.316621
2.086410	165.749361	4.321626
1.621275	160.041887	4.326630
1.648430	161.739663	4.331635
2.314548	169.035327	4.336640
1.592338	157.385389	4.341645
1.988295	158.348328	4.346650
1.876676	161.912341	4.351654
1.824090	167.365384	4.356659
1.874973	165.949429	4.361664
1.531329	173.662736	4.366669
1.735643	163.987372	4.371674
1.987551	172.224308	4.376678
1.850624	178.851684	4.381683
1.879786	180.390957	4.386688
1.551764	180.423276	4.391693
1.718606	177.574932	4.396698
1.725757	180.940003	4.401702
1.750627	174.355309	4.406707
2.213918	175.386793	4.411712
1.989255	175.409246	4.416717
2.117034	174.215362	4.421722
2.137234	176.543826	4.426726
1.900287	179.285907	4.431731
2.204972	173.435666	4.436736
1.978790	175.853354	4.441741
2.237760	167.827255	4.446746
1.712729	182.516690	4.451750
1.770198	176.069258	4.456755
1.790228	178.094023	4.461760
2.037600	197.974472	4.466765
2.339302	201.733166	4.471770
2.156668	201.236497	4.476774
2.206165	197.666205	4.481779
2.785353	201.463680	4.486784
2.360957	187.745389	4.491789
1.916046	177.788919	4.496794
2.106405	175.674056	4.501798
1.925341	176.537576	4.506803
2.315321	194.810613	4.511808
2.164384	203.964909	4.516813
2.458687	198.103632	4.521818
2.399190	197.242815	4.526822
2.424778	202.076170	4.531827
2.494179	187.400973	4.536832
2.150575	186.249308	4.541837
2.435401	184.989689	4.546842
1.627873	188.245121	4.551846
2.546197	193.014530	4.556851
2.621339	199.845972	4.561856
2.300840	200.895858	4.566861
2.357482	201.241236	4.571866
1.846813	209.056660	4.576870
2.472551	201.792506	4.581875
2.546182	197.936855	4.586880
2.546932	205.963218	4.591885
2.649247	198.932938	4.596890
2.683453	209.665441	4.601894
2.596386	209.963733	4.606899
2.789488	202.365562	4.611904
2.642387	201.705135	4.616909
2.916669	200.111803	4.621914
2.454859	191.176717	4.626918
2.495283	190.328719	4.631923
2.355396	187.237362	4.636928
2.416795	202.704978	4.641933
2.336953	210.402279	4.646938
2.582249	203.805183	4.651942
2.226338	204.348081	4.656947
2.456579	203.653842	4.661952
2.621416	208.459054	4.666957
2.455504	209.649237	4.671962
2.483960	209.173279	4.676966
2.576784	199.062939	4.681971
3.013379	206.793220	4.686976
2.591474	208.656274	4.691981
2.722678	200.827352	4.696986
2.609472	194.498405	4.701990
1.985262	192.267555	4.706995
2.734247	196.630056	4.712000
2.508513	196.864651	4.717005
2.882285	209.214440	4.722010
2.535900	214.052295	4.727014
2.597196	222.227369	4.732019
2.869182	218.372272	4.737024
2.223558	227.265561	4.742029
2.509307	228.014813	4.747034
2.543886	229.860131	4.752038
2.640585	231.493232	4.757043
2.680255	226.583019	4.762048
2.634988	235.606877	4.767053
2.894229	234.749903	4.772058
2.825596	244.878434	4.777062
2.892123	243.662505	4.782067
3.275296	249.420628	4.787072
2.938387	249.014569	4.792077
2.842663	242.423434	4.797082
3.385672	254.961877	4.802086
2.740650	242.727139	4.807091
2.882575	235.519793	4.812096
3.086460	244.055358	4.817101
3.115199	243.658449	4.822106
3.107131	257.324131	4.827110
3.120053	248.931579	4.832115
3.015704	233.669788	4.837120
2.501627	245.513293	4.842125
3.135794	246.242757	4.847130
3.197339	250.279539	4.852134
3.124312	252.701714	4.857139
3.239141	252.775380	4.862144
3.147464	255.010649	4.867149
3.169129	248.625749	4.872154
2.987003	249.470456	4.877158
3.170474	254.279088	4.882163
3.009622	244.062934	4.887168
2.921795	247.809901	4.892173
3.303897	243.500940	4.897178
3.449695	246.113459	4.902182
3.120069	257.488302	4.907187
3.378780	245.055016	4.912192
3.133555	251.496903	4.917197
3.066982	247.008299	4.922202
2.885927	262.203900	4.927206
3.183926	257.518963	4.932211
3.377357	255.903492	4.937216
3.033634	256.058496	4.942221
3.000735	259.195735	4.947226
3.018926	256.117564	4.952230
3.572173	272.172577	4.957235
3.706492	274.394586	4.962240
3.391450	264.955567	4.967245
3.417356	254.371617	4.972250
3.364930	248.365329	4.977254
3.312712	256.295608	4.982259
3.535493	258.529064	4.987264
3.175351	269.244295	4.992269
3.330008	274.702866	4.997274
3.548440	276.851584	5.002278
3.614376	277.676408	5.007283
3.770091	273.950250	5.012288
3.511394	277.774617	5.017293
3.610335	270.425293	5.022298
3.544894	272.453968	5.027302
3.371776	273.275118	5.032307
3.603919	271.349854	5.037312
3.441368	269.457957	5.042317
3.634216	266.010727	5.047322
3.869318	274.234524	5.052326
3.497118	281.645462	5.057331
3.523353	265.692454	5.062336
3.611374	279.754394	5.067341
3.940753	266.721550	5.072346
3.706588	267.963561	5.077350
3.493852	268.120189	5.082355
3.349942	270.929966	5.087360
3.340612	274.054023	5.092365
3.387938	267.114592	5.097370
3.395842	268.973585	5.102374
3.625994	281.099148	5.107379
3.893669	265.304468	5.112384
3.823716	278.929242	5.117389
3.884730	273.104492	5.122394
3.860857	274.895696	5.127398
3.604128	275.426220	5.132403
3.914254	276.051430	5.137408
3.660303	282.807913	5.142413
3.922174	285.263044	5.147418
3.604764	272.416959	5.152422
3.880726	276.464444	5.157427
3.767815	273.185344	5.162432
3.753737	277.237144	5.167437
3.794742	281.868785	5.172442
3.726281	283.727089	5.177446
3.616916	292.419327	5.182451
4.244516	296.652173	5.187456
3.717104	294.244788	5.192461
3.915683	291.116201	5.197466
3.921795	289.061831	5.202470
3.988467	293.341433	5.207475
4.442176	294.054880	5.212480
4.064239	296.230600	5.217485
4.085548	296.125926	5.222490
4.350148	297.837133	5.227494
4.139208	292.042331	5.232499
4.018314	288.878377	5.237504
3.945729	293.198780	5.242509
3.987512	294.346936	5.247514
4.073061	295.573657	5.252518
4.132694	296.579808	5.257523
4.330687	286.057463	5.262528
4.126704	293.983063	5.267533
4.004575	290.502920	5.272538
4.151866	296.984566	5.277542
3.920843	303.939950	5.282547
4.541383	292.519311	5.287552
4.103281	299.564087	5.292557
4.558689	296.452208	5.297562
4.151483	295.044739	5.302566
4.170502	299.521639	5.307571
4.049015	295.399138	5.312576
3.856264	303.781736	5.317581
3.963584	296.168491	5.322586
4.390160	292.883956	5.327590
4.325196	298.886320	5.332595
4.148649	291.782635	5.337600
4.029313	295.996466	5.342605
4.053956	298.865263	5.347610
3.689195	305.319571	5.352614
4.244175	314.486709	5.357619
5.108510	305.590562	5.362624
4.737348	310.277298	5.367629
4.784072	296.617988	5.372634
4.347148	295.949182	5.377638
4.188672	292.974617	5.382643
4.498746	288.135917	5.387648
4.337794	296.111725	5.392653
4.763155	298.686777	5.397658
4.493822	293.790158	5.402662
4.605650	293.013227	5.407667
4.353092	295.267380	5.412672
4.527806	296.173240	5.417677
4.537892	292.381309	5.422682
4.833469	296.615556	5.427686
4.488777	297.419295	5.432691
4.639986	295.209310	5.437696
4.825293	310.701899	5.442701
4.918401	292.099760	5.447706
4.692804	292.483034	5.452710
4.402983	300.716321	5.457715
4.648871	295.511181	5.462720
4.551298	306.324503	5.467725
4.196398	289.200463	5.472730
4.596766	298.274756	5.477734
4.388746	298.851433	5.482739
4.529648	299.474683	5.487744
4.126633	308.535648	5.492749
4.759169	315.966352	5.497754
4.959893	321.189924	5.502758
4.851848	320.172188	5.507763
5.213211	319.004974	5.512768
5.157278	316.156711	5.517773
4.930792	302.467435	5.522778
5.031407	307.621265	5.527782
4.664268	302.334999	5.532787
4.813468	302.216614	5.537792
4.882709	302.430304	5.542797
4.807765	299.044008	5.547802
4.725535	302.948301	5.552806
4.781170	305.097219	5.557811
4.480627	303.499027	5.562816
4.931378	310.559569	5.567821
5.091269	317.978905	5.572826
4.668481	308.316294	5.577830
4.652949	319.559704	5.582835
5.070694	310.164039	5.587840
4.644640	322.886002	5.592845
4.700017	319.552051	5.597850
4.937198	318.907342	5.602854
4.848627	324.783697	5.607859
5.063837	321.598713	5.612864
4.966213	324.587913	5.617869
4.990892	323.100119	5.622874
4.849380	320.040632	5.627878
4.687082	319.996364	5.632883
4.997795	317.951214	5.637888
4.710016	325.314141	5.642893
4.779194	315.583936	5.647898
4.989843	336.087239	5.652902
4.919669	347.367703	5.657907
5.340048	348.127505	5.662912
5.304866	351.331558	5.667917
5.253928	358.628915	5.672922
5.525874	350.363414	5.677926
5.153437	339.819680	5.682931
5.209454	322.137668	5.687936
5.015712	330.786196	5.692941
5.191255	333.033391	5.697946
5.345850	332.407949	5.702950
5.276998	336.759417	5.707955
5.357553	325.698615	5.712960
5.123524	339.304849	5.717965
5.140760	340.491656	5.722970
5.516273	343.371925	5.727974
4.995956	338.976537	5.732979
5.518512	345.737934	5.737984
5.328111	349.845851	5.742989
5.269795	359.688086	5.747994
5.238444	359.085449	5.752998
5.400043	358.373485	5.758003
5.571929	348.228527	5.763008
5.739378	348.885586	5.768013
5.416510	352.305561	5.773018
5.286742	340.967648	5.778022
5.490551	352.660779	5.783027
5.326208	347.921705	5.788032
5.398143	350.887507	5.793037
5.087330	347.335673	5.798042
5.323522	350.598449	5.803046
5.376551	350.890612	5.808051
5.485409	344.700829	5.813056
5.699580	344.024922	5.818061
5.476035	356.797440	5.823066
5.403839	364.838467	5.828070
5.341775	358.827324	5.833075
5.591816	348.746052	5.838080
5.174380	352.797791	5.843085
5.334835	358.445309	5.848090
5.479099	353.632571	5.853094
5.177144	357.856047	5.858099
5.677197	363.782561	5.863104
5.695376	369.939605	5.868109
5.820973	376.114623	5.873114
5.617008	372.005027	5.878118
5.627700	373.426985	5.883123
5.843304	370.956958	5.888128
5.697673	374.849054	5.893133
5.870947	367.712675	5.898138
5.771865	362.476142	5.903142
5.590230	363.833318	5.908147
5.661967	365.479835	5.913152
5.503905	367.244616	5.918157
5.859542	372.605287	5.923162
5.870874	368.680263	5.928166
6.200705	369.960467	5.933171
5.888385	380.772678	5.938176
5.442228	366.649524	5.943181
5.536928	374.423954	5.948186
5.921601	372.696250	5.953190
5.736266	379.736256	5.958195
5.932925	369.315314	5.963200
6.343887	372.848112	5.968205
6.248662	370.180007	5.973210
6.077562	368.030004	5.978214
5.985370	369.793957	5.983219
5.800075	362.830823	5.988224
5.897430	360.154692	5.993229
6.060123	360.685944	5.998234
5.878276	344.040950	6.003238
5.866942	345.817542	6.008243
5.884902	345.773505	6.013248
5.657308	353.361137	6.018253
6.081789	362.200725	6.023258
5.980486	361.194586	6.028262
5.896054	358.790554	6.033267
5.958930	344.100432	6.038272
5.336789	349.918022	6.043277
5.772228	357.404935	6.048282
5.892140	361.454744	6.053286
5.890496	374.910696	6.058291
5.767723	362.005576	6.063296
5.498752	377.803523	6.068301
5.914385	367.066692	6.073306
6.044349	369.219791	6.078310
5.979298	370.039832	6.083315
6.229256	372.335486	6.088320
5.775202	374.004271	6.093325
5.683069	365.153549	6.098330
5.934594	373.096402	6.103334
5.856708	372.595971	6.108339
5.791099	367.892044	6.113344
5.717421	366.043161	6.118349
5.957678	364.391869	6.123354
6.007413	367.845219	6.128358
5.729514	371.723235	6.133363
5.965393	375.185386	6.138368
6.025468	378.523220	6.143373
5.445253	369.464223	6.148378
5.696983	378.710546	6.153382
5.697989	372.300365	6.158387
5.468160	374.721814	6.163392
5.741529	376.463292	6.168397
5.486923	386.880476	6.173402
5.898925	391.972887	6.178406
5.947804	396.280612	6.183411
6.160665	395.440389	6.188416
6.156623	393.343305	6.193421
6.058671	402.770982	6.198426
6.323810	384.559420	6.203430
5.920603	387.352894	6.208435
5.939955	368.243363	6.213440
5.798095	374.447630	6.218445
5.909259	364.932288	6.223450
5.777452	368.167303	6.228454
5.471361	371.236631	6.233459
5.845016	375.050528	6.238464
6.022247	391.060157	6.243469
5.994697	404.703693	6.248474
6.314385	396.066850	6.253478
5.652359	390.184500	6.258483
5.826144	389.736388	6.263488
6.045033	394.406628	6.268493
5.800559	381.558528	6.273498
5.824353	374.986583	6.278502
6.089238	393.697051	6.283507
5.984582	387.828617	6.288512
5.718854	378.932319	6.293517
6.102304	386.933603	6.298522
6.101317	379.799213	6.303526
5.609892	376.952732	6.308531
5.887254	377.564096	6.313536
5.833319	391.496502	6.318541
5.977514	390.891670	6.323546
6.062090	396.209395	6.328550
6.019958	383.108121	6.333555
5.676218	372.148572	6.338560
5.770721	379.888234	6.343565
5.557728	391.263871	6.348570
6.191896	395.441927	6.353574
5.994798	397.519720	6.358579
6.275172	389.322485	6.363584
5.804022	391.765927	6.368589
5.929273	375.927024	6.373594
5.971901	380.526798	6.378598
5.663293	382.416411	6.383603
5.770267	392.204291	6.388608
5.832106	396.940268	6.393613
5.920754	395.613292	6.398618
6.267562	401.497389	6.403622
5.814572	395.468387	6.408627
5.910456	400.876093	6.413632
6.002211	407.686028	6.418637
5.869809	399.044085	6.423642
6.115986	399.476833	6.428646
5.932713	391.896422	6.433651
5.573787	374.250898	6.438656
5.813493	389.124411	6.443661
6.140026	392.287616	6.448666
6.283294	388.183725	6.453670
5.887678	383.294212	6.458675
5.670714	366.623061	6.463680
5.581822	378.067832	6.468685
6.220434	392.850373	6.473690
6.053060	391.601477	6.478694
5.649101	378.980853	6.483699
5.935817	385.089500	6.488704
5.672646	390.999560	6.493709
6.160805	386.231011	6.498714
6.162184	395.997471	6.503718
5.733473	384.253941	6.508723
6.004388	384.477163	6.513728
5.785693	388.406020	6.518733
6.016495	396.453373	6.523738
6.160308	383.332457	6.528742
5.854501	386.474511	6.533747
5.705594	383.210522	6.538752
5.625257	385.469341	6.543757
5.708362	382.589791	6.548762
6.169862	403.076015	6.553766
6.161492	408.136215	6.558771
6.125826	392.170646	6.563776
5.964901	385.308091	6.568781
5.614052	382.139020	6.573786
5.602413	385.383684	6.578790
5.857116	395.325594	6.583795
5.602588	393.160185	6.588800
5.751709	397.914125	6.593805
5.721331	410.359014	6.598810
6.050874	412.215085	6.603814
5.568551	410.658020	6.608819
5.509736	397.935847	6.613824
5.572673	412.685212	6.618829
5.644178	407.298548	6.623834
5.774531	402.462666	6.628838
5.682087	400.872990	6.633843
5.684886	407.586129	6.638848
6.135883	419.518992	6.643853
6.276375	412.612365	6.648858
6.272445	413.932210	6.653862
6.001880	401.426715	6.658867
6.273128	405.057342	6.663872
6.047540	407.348413	6.668877
6.361429	407.523773	6.673882
6.420901	411.209729	6.678886
6.073338	402.111100	6.683891
6.216572	391.647895	6.688896
6.018584	394.861645	6.693901
5.641716	380.752934	6.698906
5.847695	389.392646	6.703910
5.953529	392.894160	6.708915
6.129988	395.666417	6.713920
5.985696	387.456624	6.718925
5.907343	385.532539	6.723930
6.103781	382.407435	6.728934
5.945316	382.406860	6.733939
6.052747	370.076286	6.738944
6.140552	372.362544	6.743949
6.077843	380.493843	6.748954
5.985683	373.838824	6.753958
5.889116	374.926401	6.758963
6.079105	371.204345	6.763968
5.806391	372.208787	6.768973
5.632093	370.673069	6.773978
5.910686	377.390443	6.778982
5.578255	374.231142	6.783987
5.887292	372.755740	6.788992
5.962263	379.289877	6.793997
6.205234	376.065732	6.799002
5.969335	379.057623	6.804006
5.889608	376.241553	6.809011
6.074874	366.755729	6.814016
5.911356	376.861235	6.819021
5.968424	374.858985	6.824026
5.871503	375.155659	6.829030
5.588727	373.149706	6.834035
5.959870	367.206730	6.839040
6.286898	370.667254	6.844045
5.883388	361.643852	6.849050
6.195202	365.113087	6.854054
6.163644	373.492609	6.859059
6.010240	369.580741	6.864064
5.622994	369.587537	6.869069
5.903848	371.783435	6.874074
5.711984	373.461762	6.879078
5.602890	373.684412	6.884083
5.693098	371.164427	6.889088
5.755300	370.888827	6.894093
5.792172	373.505776	6.899098
5.632583	375.324583	6.904102
6.068797	384.475563	6.909107
6.242699	380.366874	6.914112
5.731466	381.149253	6.919117
5.731957	377.482197	6.924122
5.844993	368.507576	6.929126
5.744427	382.520049	6.934131
5.831160	388.878336	6.939136
5.531840	396.613269	6.944141
5.868791	401.859814	6.949146
6.333475	391.131103	6.954150
5.890197	405.735144	6.959155
6.415578	392.927770	6.964160
6.262478	388.193252	6.969165
5.911639	387.574231	6.974170
6.203373	372.294556	6.979174
5.840656	380.222918	6.984179
5.708302	371.486065	6.989184
5.495633	369.788676	6.994189
5.511466	371.640110	6.999194
5.798554	381.504170	7.004198
5.979107	395.798483	7.009203
6.065572	398.192525	7.014208
6.172972	395.135155	7.019213
5.713776	397.019889	7.024218
6.121975	394.510191	7.029222
5.735166	391.928899	7.034227
5.832409	392.261592	7.039232
5.877971	390.137753	7.044237
5.840093	401.517597	7.049242
6.224838	393.648866	7.054246
6.317706	387.736828	7.059251
6.108602	380.195271	7.064256
5.947482	377.148338	7.069261
5.742679	373.858306	7.074266
5.834784	370.971020	7.079270
5.382205	373.974713	7.084275
5.833476	372.932617	7.089280
5.992787	398.863687	7.094285
5.902681	409.736014	7.099290
6.266642	394.381727	7.104294
5.844111	379.916330	7.109299
5.745488	375.904126	7.114304
5.647850	383.205646	7.119309
5.704895	389.388246	7.124314
6.079219	392.936280	7.129318
5.865744	395.206469	7.134323
5.952162	399.625375	7.139328
6.036451	397.375241	7.144333
5.993030	393.493593	7.149338
5.986544	395.000504	7.154342
5.744434	396.917666	7.159347
5.946803	396.496713	7.164352
6.059020	400.512934	7.169357
5.810947	393.793748	7.174362
6.186874	393.706281	7.179366
5.626733	395.480277	7.184371
5.821501	392.481987	7.189376
5.810581	398.570832	7.194381
5.807192	402.023020	7.199386
6.041260	391.972701	7.204390
6.249870	395.350542	7.209395
5.723283	388.709798	7.214400
5.782626	400.150341	7.219405
5.938227	397.727678	7.224410
6.297002	399.386173	7.229414
5.960538	391.437448	7.234419
5.891051	382.921700	7.239424
5.597647	381.180010	7.244429
5.804520	401.310647	7.249434
6.176845	397.718209	7.254438
5.964138	395.669637	7.259443
6.032846	380.453374	7.264448
5.811254	377.751282	7.269453
5.805985	389.676517	7.274458
6.113291	393.592565	7.279462
5.815488	384.153945	7.284467
6.078750	382.119387	7.289472
5.843699	387.056907	7.294477
5.703133	387.673639	7.299482
6.003102	389.341347	7.304486
6.035518	391.658433	7.309491
5.998215	382.609281	7.314496
5.788372	383.186247	7.319501
5.754630	386.080024	7.324506
6.142666	391.122405	7.329510
5.622828	392.406019	7.334515
6.147509	389.564852	7.339520
5.961357	394.599118	7.344525
5.722398	382.930265	7.349530
6.147635	387.903539	7.354534
6.111243	382.815370	7.359539
5.549707	376.240219	7.364544
5.566423	385.324046	7.369549
5.762899	393.689996	7.374554
6.137090	397.288673	7.379558
5.793810	399.974680	7.384563
5.760615	398.347247	7.389568
5.924463	392.069736	7.394573
5.506791	401.946151	7.399578
6.011385	395.365307	7.404582
5.919633	392.608067	7.409587
5.989988	388.664300	7.414592
5.935366	404.185070	7.419597
5.690359	396.475121	7.424602
5.743816	399.124278	7.429606
5.591623	398.360235	7.434611
5.741627	397.707035	7.439616
5.840456	403.221850	7.444621
5.898697	405.727886	7.449626
6.259849	394.493361	7.454630
5.869924	401.141476	7.459635
5.853734	392.493982	7.464640
5.919315	394.672991	7.469645
5.406648	401.321354	7.474650
5.815782	395.657162	7.479654
5.527106	394.525351	7.484659
6.410274	397.889253	7.489664
6.620669	401.339583	7.494669
6.330247	398.344544	7.499674
6.597100	391.699708	7.504678
6.319189	402.240778	7.509683
6.215274	388.677769	7.514688
5.979439	382.757120	7.519693
5.878870	384.351540	7.524698
6.065704	377.728738	7.529702
5.562679	368.948720	7.534707
5.603338	369.774346	7.539712
5.862594	374.681871	7.544717
5.961524	381.708977	7.549722
6.482936	378.339963	7.554726
5.693567	388.081614	7.559731
5.751632	383.870847	7.564736
5.800551	379.101515	7.569741
5.741102	376.000686	7.574746
6.112759	378.242471	7.579750
5.938078	390.751085	7.584755
6.143281	379.306880	7.589760
6.045193	379.366449	7.594765
6.069772	380.650187	7.599770
5.884020	372.886670	7.604774
5.610616	375.916075	7.609779
5.518601	375.825993	7.614784
6.000042	382.777348	7.619789
5.953590	387.527126	7.624794
5.930540	381.889522	7.629798
5.408771	385.321684	7.634803
5.696029	392.274994	7.639808
6.100736	391.180080	7.644813
6.113368	394.721507	7.649818
6.336020	403.861665	7.654822
5.933850	387.444146	7.659827
5.962817	385.522229	7.664832
5.600019	381.402714	7.669837
5.563796	385.831341	7.674842
5.673468	395.150552	7.679846
5.661369	406.168847	7.684851
6.127247	400.334406	7.689856
6.105216	391.801726	7.694861
5.866162	400.460551	7.699866
6.162527	399.268714	7.704870
5.860790	401.767873	7.709875
6.015913	403.727204	7.714880
6.208023	396.834642	7.719885
5.937356	405.742038	7.724890
5.966710	387.621201	7.729894
5.734543	391.074430	7.734899
6.153696	391.505386	7.739904
5.815890	395.237766	7.744909
5.792809	384.949324	7.749914
6.017959	390.593043	7.754918
5.909418	394.207241	7.759923
6.059053	400.932174	7.764928
5.982800	380.027893	7.769933
5.485300	383.975121	7.774938
5.663886	390.420259	7.779942
5.532325	396.591283	7.784947
5.941289	403.905188	7.789952
6.266815	396.444378	7.794957
6.119328	400.621516	7.799962
6.210994	397.541300	7.804966
5.787603	401.075113	7.809971
6.044796	390.616200	7.814976
6.145224	372.582321	7.819981
5.820808	381.880951	7.824986
5.898426	373.481367	7.829990
5.701826	386.344599	7.834995
6.086769	385.790634	7.840000
6.217037	378.983701	7.845005
5.821091	377.966777	7.850010
6.065544	379.918436	7.855014
5.855842	382.997975	7.860019
5.429946	378.904166	7.865024
5.707121	383.745610	7.870029
5.520256	396.632634	7.875034
6.059187	402.992843	7.880038
5.950042	396.033584	7.885043
6.014863	407.444799	7.890048
6.005581	403.402772	7.895053
5.768297	408.951268	7.900058
6.181390	403.938204	7.905062
5.900008	414.780390	7.910067
5.888523	404.648312	7.915072
6.229358	403.629845	7.920077
6.054228	388.973813	7.925082
5.741099	378.484040	7.930086
5.812234	382.620592	7.935091
5.718369	387.517007	7.940096
6.085150	402.509830	7.945101
5.849532	402.154337	7.950106
6.084554	397.048950	7.955110
5.848797	392.688059	7.960115
5.689003	390.631197	7.965120
5.852875	395.015820	7.970125
5.473191	401.359699	7.975142
5.987995	402.137316	7.980160
6.030781	412.169025	7.985178
6.149536	389.059562	7.990195
6.446724	397.101139	7.995213
6.430225	396.220015	8.000230
5.690972	379.594405	8.005248
5.654565	387.123363	8.010266
5.757872	379.312342	8.015283
5.816549	386.832713	8.020301
5.858036	400.743056	8.025318
6.252076	396.054868	8.030336
5.912331	410.072287	8.035354
6.222468	410.803077	8.040371
5.757825	389.804714	8.045389
5.958591	406.082178	8.050406
6.309183	402.180270	8.055424
5.949892	398.670452	8.060442
5.871249	390.247313	8.065459
6.197175	391.878178	8.070477
5.996046	396.813661	8.075494
6.239938	381.965340	8.080512
5.744623	385.772969	8.085530
5.692126	385.310892	8.090547
6.290125	402.169889	8.095565
5.957211	401.243669	8.100582
6.360651	394.635301	8.105600
6.008331	390.856151	8.110618
5.823047	380.556265	8.115635
5.906935	388.934211	8.120653
5.901457	394.429168	8.125670
6.259826	396.768153	8.130688
5.771411	405.365162	8.135706
5.927710	409.512509	8.140723
6.064283	405.678847	8.145741
5.810738	397.718604	8.150758
6.332610	405.942729	8.155776
5.732067	407.182274	8.160794
5.855366	404.041806	8.165811
5.980861	411.255076	8.170829
5.934958	414.269625	8.175846
6.210322	400.363089	8.180864
6.179891	402.134995	8.185882
5.883046	402.787319	8.190899
5.942560	397.308954	8.195917
5.919279	410.206983	8.200934
6.127684	402.874941	8.205952
6.242969	402.515962	8.210970
6.119071	406.830284	8.215987
6.004449	400.495586	8.221005
5.923868	406.204282	8.226022
6.353039	418.428676	8.231040
6.274371	415.184152	8.236058
6.216358	419.557581	8.241075
6.303426	415.381383	8.246093
6.144233	419.133199	8.251110
6.416740	414.785936	8.256128
5.962547	407.071720	8.261146
6.409923	416.004947	8.266163
6.290722	418.188390	8.271181
6.346664	409.813581	8.276198
6.477119	403.901226	8.281216
6.441239	409.306277	8.286234
6.291621	403.308417	8.291251
6.184802	398.035991	8.296269
5.933187	408.861742	8.301286
6.440602	398.352328	8.306304
6.191888	404.447125	8.311322
6.326662	401.434246	8.316339
6.464350	395.583875	8.321357
5.901047	407.594537	8.326374
6.542744	399.449846	8.331392
6.310959	400.956658	8.336410
5.883851	406.375669	8.341427
6.223576	406.903010	8.346445
6.651983	408.050766	8.351462
6.408381	401.569020	8.356480
6.386566	395.295520	8.361498
6.073377	397.439928	8.366515
6.255256	400.639690	8.371533
5.923711	398.899067	8.376550
6.172258	400.807141	8.381568
6.439998	413.258793	8.386586
6.384765	414.210929	8.391603
6.473271	418.053323	8.396621
6.401522	417.423850	8.401638
6.346449	412.285322	8.406656
6.476213	411.813622	8.411674
6.298633	410.888309	8.416691
6.324057	398.595665	8.421709
6.026474	420.379146	8.426726
6.252483	410.529192	8.431744
6.191013	419.681001	8.436762
6.365977	426.883371	8.441779
6.797738	426.664152	8.446797
6.345629	420.975609	8.451814
6.497907	422.270771	8.456832
6.097003	417.372617	8.461850
6.384091	419.760643	8.466867
6.480260	412.338886	8.471885
6.341080	421.575454	8.476902
6.711600	423.117285	8.481920
6.612110	428.396610	8.486938
6.298457	437.023056	8.491955
6.660935	425.163573	8.496973
6.505371	431.486779	8.501990
6.719768	430.118202	8.507008
6.552148	427.007532	8.512026
6.872819	429.106278	8.517043
6.402633	412.993896	8.522061
6.360708	411.472978	8.527078
6.212935	416.100309	8.532096
6.718631	422.278880	8.537114
6.502056	424.133602	8.542131
7.081883	429.480059	8.547149
6.496370	417.747022	8.552166
6.296127	405.098415	8.557184
6.373655	410.387870	8.562202
6.232359	421.505609	8.567219
6.693099	418.454277	8.572237
6.639120	422.451539	8.577255
6.653935	422.616380	8.582272
6.715298	421.988141	8.587290
6.396302	432.540444	8.592307
6.901299	424.518145	8.597325
6.893936	419.255376	8.602343
6.382293	410.846422	8.607360
6.556271	403.781702	8.612378
6.245026	409.728510	8.617395
6.525862	409.662325	8.622413
6.500762	420.856531	8.627431
6.684883	421.496614	8.632448
7.024223	419.805507	8.637466
6.457031	417.795693	8.642483
6.625315	423.402287	8.647501
6.673259	433.373240	8.652519
6.274802	429.563442	8.657536
6.610627	432.123713	8.662554
6.384117	438.464349	8.667571
6.806570	430.366618	8.672589
6.558490	429.849978	8.677607
6.654737	421.844386	8.682624
6.751269	425.234248	8.687642
6.538772	421.922329	8.692659
6.919163	412.912867	8.697677
6.563181	422.009836	8.702695
6.797221	428.363515	8.707712
7.037604	420.108125	8.712730
6.699943	427.605406	8.717747
6.753249	427.066791	8.722765
6.464045	431.022015	8.727783
6.485807	424.344050	8.732800
6.479632	425.891254	8.737818
6.452319	427.410212	8.742835
6.732969	428.360215	8.747853
6.590818	430.932260	8.752871
6.530784	423.749565	8.757888
7.067046	424.135660	8.762906
6.706934	425.470078	8.767923
6.457506	429.144517	8.772941
6.425136	430.733694	8.777959
6.497172	426.922763	8.782976
6.740747	433.221301	8.787994
6.548387	440.702133	8.793011
6.691966	450.421428	8.798029
7.259721	450.853083	8.803047
7.079219	446.797694	8.808064
6.969641	428.025282	8.813082
6.561480	429.733298	8.818099
6.756788	432.785796	8.823117
6.869290	431.370068	8.828135
6.773482	440.397881	8.833152
7.116346	442.767704	8.838170
6.778630	440.333772	8.843187
6.833680	435.237944	8.848205
7.082342	430.509409	8.853223
6.488763	432.984928	8.858240
6.738503	441.270642	8.863258
7.374304	455.390865	8.868275
7.004943	438.044532	8.873293
6.713627	420.370410	8.878311
6.617205	424.642562	8.883328
6.955587	436.190078	8.888346
6.790674	440.485589	8.893363
7.280424	446.294285	8.898381
7.171307	445.613862	8.903399
6.518591	434.961151	8.908416
7.039943	450.850758	8.913434
7.076581	451.384563	8.918451
6.838750	453.659180	8.923469
6.899423	455.265339	8.928487
6.725110	456.778930	8.933504
6.719699	454.876750	8.938522
6.978053	458.967093	8.943539
6.944441	457.911924	8.948557
6.749222	460.855203	8.953575
7.023013	461.421277	8.958592
7.099861	453.967816	8.963610
6.854797	455.751266	8.968627
6.844294	451.211653	8.973645
6.519172	446.879125	8.978663
6.760464	455.607978	8.983680
7.208066	449.563866	8.988698
6.732294	448.893554	8.993715
6.741095	458.094332	8.998733
7.115669	460.077340	9.003751
6.985405	464.301156	9.008768
7.330944	458.544429	9.013786
6.722973	469.719538	9.018803
6.977629	472.658604	9.023821
7.333716	481.703996	9.028839
6.983377	478.445222	9.033856
7.517245	467.811703	9.038874
6.931504	474.054003	9.043891
6.727838	463.122636	9.048909
6.982076	473.736626	9.053927
7.157467	485.000445	9.058944
7.511358	477.711849	9.063962
7.211464	485.095939	9.068979
7.224635	469.532618	9.073997
7.288418	458.938044	9.079015
6.808817	459.729457	9.084032
7.132981	475.997118	9.089050
6.872287	485.107592	9.094067
7.109792	485.385865	9.099085
7.302020	481.565557	9.104103
7.353720	485.735621	9.109120
7.591050	471.194365	9.114138
6.974577	467.106295	9.119155
6.996808	476.156657	9.124173
7.562020	471.208102	9.129191
7.485902	472.690530	9.134208
7.219143	454.829491	9.139226
7.123667	458.492438	9.144243
6.816848	457.934507	9.149261
6.935351	469.516496	9.154279
7.370674	480.338801	9.159296
7.502302	476.142984	9.164314
7.591420	485.814027	9.169331
7.263642	467.987781	9.174349
7.178239	464.750615	9.179367
7.179665	463.702580	9.184384
7.366438	460.321785	9.189402
6.936429	477.095771	9.194419
7.350470	481.979074	9.199437
7.400235	477.625670	9.204455
7.306465	487.704063	9.209472
7.508655	478.274367	9.214490
7.613696	480.031367	9.219507
7.454896	466.969126	9.224525
7.185530	457.102088	9.229543
7.121230	450.974081	9.234560
7.583515	469.195611	9.239578
7.150834	469.089743	9.244595
7.235156	477.029009	9.249613
7.374583	467.274639	9.254631
7.372174	479.238493	9.259648
7.657886	476.691099	9.264666
7.578721	481.702170	9.269683
7.705269	473.136390	9.274701
7.533805	454.850169	9.279719
7.553664	450.693960	9.284736
7.287682	440.895828	9.289754
7.500627	456.322525	9.294771
7.219222	451.301498	9.299789
7.306316	454.765427	9.304807
7.133267	450.759363	9.309824
7.572019	457.074666	9.314842
7.461927	469.241576	9.319859
7.793385	466.223116	9.324877
7.414339	459.484862	9.329895
7.025223	458.570600	9.334912
7.463263	466.094681	9.339930
7.718040	472.000161	9.344947
7.493433	480.514848	9.349965
7.778035	471.640284	9.354983
7.404964	462.351220	9.360000
7.270483	451.077665	9.365018
7.553255	465.306857	9.370035
7.538669	477.906930	9.375053
8.284642	469.547055	9.380071
7.716377	460.061360	9.385088
7.667495	453.864664	9.390106
7.712600	455.198710	9.395123
7.666767	453.586883	9.400141
7.815855	443.102028	9.405159
7.513885	453.998812	9.410176
7.626402	449.563000	9.415194
7.453524	452.906716	9.420211
7.340130	447.534321	9.425229
7.505177	444.658702	9.430247
7.464959	454.252163	9.435264
7.422129	444.712553	9.440282
7.092445	449.500937	9.445299
7.696559	462.900302	9.450317
7.812206	469.938415	9.455335
7.511850	468.205521	9.460352
8.136577	457.687160	9.465370
7.704611	460.635974	9.470387
7.393529	461.767054	9.475405
7.508590	450.533295	9.480423
7.555536	449.894691	9.485440
7.965541	462.213635	9.490458
7.391026	462.451879	9.495475
7.678415	470.864250	9.500493
7.876787	464.158599	9.505511
7.522616	464.075143	9.510528
7.919450	465.770644	9.515546
7.475221	464.615710	9.520563
7.243235	471.862925	9.525581
7.529645	467.276788	9.530599
7.502600	474.668617	9.535616
7.777276	476.458997	9.540634
7.636938	480.103731	9.545651
7.999018	476.310460	9.550669
8.157161	475.919519	9.555687
8.081608	479.049177	9.560704
7.918076	481.861262	9.565722
7.855584	475.108118	9.570739
7.623148	486.887113	9.575757
7.916691	468.464905	9.580775
7.976942	480.317957	9.585792
7.959379	477.931688	9.590810
8.002254	477.744997	9.595827
7.968737	474.364001	9.600845
7.539876	458.709002	9.605863
7.660096	467.071825	9.610880
7.638019	471.367054	9.615898
7.777332	481.285848	9.620915
7.675459	487.057867	9.625933
7.604763	472.353434	9.630951
8.005069	486.763042	9.635968
7.879613	489.275675	9.640986
7.750483	485.246943	9.646003
7.886734	476.076886	9.651021
8.180291	483.481603	9.656039
7.972299	481.412346	9.661056
7.759091	478.880007	9.666074
8.119587	478.255390	9.671091
8.144205	478.043158	9.676109
8.226815	472.529594	9.681127
8.002971	482.293851	9.686144
8.474123	482.358792	9.691162
8.141523	471.182536	9.696179
7.812054	469.129158	9.701197
7.794274	466.963829	9.706215
7.860935	473.261699	9.711232
7.821849	476.745402	9.716250
8.051414	479.871435	9.721267
7.951320	482.512637	9.726285
8.009303	474.329981	9.731303
7.976005	490.382265	9.736320
7.915642	482.574752	9.741338
7.845215	468.615045	9.746355
8.170362	485.059284	9.751373
8.202581	477.338252	9.756391
7.875780	487.468935	9.761408
8.060286	484.776452	9.766426
8.335128	483.672953	9.771443
7.993082	484.124081	9.776461
8.083246	476.747418	9.781479
8.094143	475.988230	9.786496
8.322712	485.167212	9.791514
8.127748	468.793908	9.796531
7.983776	485.049719	9.801549
8.122133	477.009102	9.806567
8.179599	477.981454	9.811584
8.167218	484.462124	9.816602
8.312845	480.686988	9.821619
8.207660	481.542813	9.826637
8.264880	481.937695	9.831655
8.169504	488.175752	9.836672
7.978515	489.707737	9.841690
8.426186	486.308150	9.846707
8.318108	485.258335	9.851725
8.446823	483.685430	9.856743
7.916892	477.226428	9.861760
8.102109	484.865868	9.866778
8.268411	478.199951	9.871795
7.949333	486.559029	9.876813
8.387557	476.628452	9.881831
8.286826	476.909227	9.886848
7.952800	478.842316	9.891866
8.064592	468.379069	9.896883
7.906253	480.462028	9.901901
8.271607	476.317953	9.906919
7.968874	473.995299	9.911936
7.792608	476.421218	9.916954
8.275061	470.336926	9.921971
8.223943	479.080047	9.926989
8.117893	485.300841	9.932007
8.213234	481.887030	9.937024
8.447503	495.050879	9.942042
8.330118	488.470431	9.947059
8.027041	484.058701	9.952077
8.509878	492.588782	9.957095
8.838357	499.593561	9.962112
8.315788	485.887717	9.967130
8.493590	471.605094	9.972147
8.291118	477.727384	9.977165
8.491798	469.825328	9.982183
8.482512	488.704585	9.987200
8.157077	481.787509	9.992218
8.124668	479.823286	9.997235
7.667677	495.001534	10.002253
8.302025	487.037835	10.007271
8.377079	492.573852	10.012288
8.477409	497.130773	10.017306
8.254962	498.118581	10.022323
8.581259	505.852690	10.027341
8.599996	500.737286	10.032359
8.337658	501.595645	10.037376
8.191489	507.286248	10.042394
8.117896	499.016900	10.047411
8.133765	503.056884	10.052429
7.914580	499.017012	10.057447
8.181325	504.917472	10.062464
8.139027	512.261214	10.067482
8.474382	524.528782	10.072499
8.564522	528.525577	10.077517
8.457184	533.474804	10.082535
8.831131	528.811820	10.087552
8.308808	528.931435	10.092570
8.404968	528.578605	10.097587
8.614286	524.553640	10.102605
8.292458	529.438644	10.107623
8.322593	532.722165	10.112640
8.181659	533.072356	10.117658
8.695944	528.920713	10.122675
8.579047	530.766139	10.127693
8.684890	527.928184	10.132711
8.660919	530.453325	10.137728
8.454296	533.553036	10.142746
8.648607	526.851154	10.147763
8.696545	529.784748	10.152781
8.532703	527.232044	10.157799
8.611311	530.362803	10.162816
8.384104	533.604594	10.167834
8.780722	534.239789	10.172851
8.719323	534.915188	10.177869
8.355679	535.827291	10.182887
8.833584	529.866767	10.187904
8.452343	536.058111	10.192922
8.783597	541.784375	10.197939
8.815165	541.990775	10.202957
9.071532	542.796267	10.207975
8.850656	543.203164	10.212992
8.626010	539.400824	10.218010
8.702056	531.202689	10.223027
8.645369	532.281291	10.228045
8.720059	530.000481	10.233063
8.957122	526.681222	10.238080
8.671542	528.082864	10.243098
8.638656	527.071758	10.248115
8.950758	531.147385	10.253133
8.819988	532.534239	10.258151
8.823459	530.387664	10.263168
8.591620	531.354854	10.268186
9.100655	538.561731	10.273203
8.713448	535.958816	10.278221
8.829866	533.766142	10.283239
9.017227	545.236405	10.288256
8.797513	546.312149	10.293274
8.773540	539.653931	10.298291
9.021231	540.719557	10.303309
8.785559	537.600596	10.308327
8.969014	537.013184	10.313344
8.748226	545.792389	10.318362
9.221925	542.262482	10.323379
9.090567	532.859771	10.328397
8.766784	539.515483	10.333415
8.797772	530.838416	10.338432
8.933123	540.991393	10.343450
8.737374	547.980497	10.348467
8.999093	551.117284	10.353485
8.937225	552.730029	10.358503
9.040297	550.520508	10.363520
8.920372	561.840113	10.368538
9.270621	559.279440	10.373555
9.003548	554.432863	10.378573
9.117656	546.818891	10.383591
8.940199	531.967035	10.388608
8.882017	536.463595	10.393626
9.053499	538.241748	10.398643
9.005240	547.038103	10.403661
9.019751	551.015195	10.408679
9.375412	561.774292	10.413696
9.012673	558.523757	10.418714
9.010476	544.209319	10.423731
9.171273	561.162215	10.428749
8.810682	551.265237	10.433767
9.232030	553.723764	10.438784
8.947440	556.990328	10.443802
9.010963	553.966497	10.448819
9.554183	542.589857	10.453837
9.117414	544.668438	10.458855
9.253302	544.987880	10.463872
8.726627	538.850236	10.468890
9.121134	543.708214	10.473907
9.319648	544.200880	10.478925
9.232048	549.415263	10.483943
9.442821	558.079520	10.488960
8.688785	544.498260	10.493978
8.917663	549.429528	10.498995
9.037550	552.478084	10.504013
9.100568	554.951729	10.509031
9.065459	559.668742	10.514048
9.095975	558.130150	10.519066
9.216107	549.792556	10.524083
9.465937	558.119335	10.529101
9.169399	561.349903	10.534119
9.065047	546.650682	10.539136
8.922647	557.623513	10.544154
8.912025	561.655037	10.549171
9.033541	561.872590	10.554189
9.268568	552.797470	10.559207
9.228687	552.529072	10.564224
9.282115	564.780879	10.569242
9.363215	574.251255	10.574259
9.534991	563.904786	10.579277
9.245362	556.095293	10.584295
9.467133	555.157895	10.589312
9.704581	554.915472	10.594330
9.509229	553.203987	10.599347
9.509341	553.929709	10.604365
9.709055	555.867542	10.609383
9.625813	552.579529	10.614400
9.195986	554.874773	10.619418
9.461180	554.479680	10.624435
9.365571	558.619194	10.629453
9.302829	558.988692	10.634471
9.532686	556.835045	10.639488
9.315261	556.323066	10.644506
9.433505	553.896573	10.649523
9.293984	551.844982	10.654541
8.993330	560.532567	10.659559
9.217381	551.399208	10.664576
9.661770	564.186205	10.669594
9.501621	566.211980	10.674611
9.645494	554.408754	10.679629
9.580850	553.453116	10.684647
9.489542	552.621575	10.689664
9.300725	568.395339	10.694682
9.442756	576.300361	10.699699
9.842504	582.006440	10.704717
9.970032	571.054673	10.709735
9.742842	565.072068	10.714752
9.663727	567.419662	10.719770
9.702516	566.002850	10.724787
9.874653	560.276415	10.729805
9.795184	554.570469	10.734823
9.847817	547.900245	10.739840
9.657110	565.744505	10.744858
9.781082	563.828353	10.749875
10.056546	564.690815	10.754893
9.614251	569.698845	10.759911
9.814244	571.933281	10.764928
9.315768	564.948612	10.769946
9.310429	565.037717	10.774963
9.901757	560.220746	10.779981
9.567950	561.708842	10.784999
9.695927	559.902516	10.790016
9.633766	559.751217	10.795034
9.723190	564.540237	10.800051
9.784529	560.756199	10.805069
9.415224	559.526403	10.810087
9.917245	560.252382	10.815104
9.327018	565.192071	10.820122
9.444615	557.009505	10.825139
9.872452	555.894654	10.830157
9.464560	566.025463	10.835175
9.802831	558.363742	10.840192
9.691658	554.101807	10.845210
9.510184	548.992512	10.850227
9.539401	550.480532	10.855245
9.586815	580.958023	10.860263
10.115515	577.043951	10.865280
10.091825	583.920904	10.870298
9.771665	576.062537	10.875315
9.771228	566.989589	10.880333
9.512458	579.937261	10.885351
10.231299	576.927515	10.890368
10.089755	580.417824	10.895386
9.883339	579.039429	10.900403
9.655154	568.850297	10.905421
9.636620	581.867627	10.910439
9.894911	574.556101	10.915456
9.748202	577.690613	10.920474
9.983726	578.947497	10.925491
10.234261	579.457259	10.930509
10.122393	578.505863	10.935527
10.290669	579.006423	10.940544
10.392428	576.434188	10.945562
9.979788	568.069607	10.950579
9.926139	553.457110	10.955597
9.255051	561.577887	10.960615
10.025618	568.358793	10.965632
9.731393	577.859574	10.970650
9.898296	572.771428	10.975667
10.031636	580.964991	10.980685
10.212030	586.929501	10.985703
10.282920	577.293108	10.990720
10.152053	581.864184	10.995738
10.057061	586.476977	11.000755
10.170171	577.654476	11.005773
10.253531	582.179364	11.010791
10.347428	582.937731	11.015808
10.140829	574.872223	11.020826
9.983747	578.241890	11.025843
10.367682	577.970203	11.030861
9.539633	572.239528	11.035879
10.081919	580.040815	11.040896
10.197166	572.713832	11.045914
10.102925	583.303592	11.050931
10.300818	578.841748	11.055949
10.121820	583.309913	11.060967
10.309751	577.833462	11.065984
10.026272	571.395772	11.071002
10.148705	580.465200	11.076019
9.936107	575.423890	11.081037
10.006805	580.272653	11.086055
9.827743	578.246189	11.091072
10.002703	579.266409	11.096090
10.107942	576.570553	11.101107
10.338631	578.737064	11.106125
9.758458	583.438498	11.111143
10.478159	577.216012	11.116160
10.002776	577.672253	11.121178
9.937664	590.472826	11.126195
10.375092	597.741439	11.131213
10.060548	602.366546	11.136231
10.021575	597.077119	11.141248
10.441465	592.627827	11.146266
10.232638	603.762572	11.151283
10.898494	591.132766	11.156301
10.570953	604.015491	11.161319
10.465122	602.744412	11.166336
10.595579	598.542438	11.171354
10.123069	598.808882	11.176371
10.681315	602.255824	11.181389
10.463723	607.844040	11.186407
10.305349	593.926417	11.191424
10.306880	599.720140	11.196442
10.355805	604.313545	11.201459
10.691027	601.042008	11.206477
10.247092	605.267666	11.211495
10.265501	610.850465	11.216512
10.405727	607.836697	11.221530
10.243156	613.637201	11.226547
10.538714	605.508781	11.231565
10.146139	607.867623	11.236583
10.208654	609.852205	11.241600
10.395556	610.921048	11.246618
10.514946	602.570922	11.251635
10.650096	600.309033	11.256653
10.924285	600.518444	11.261671
10.784964	603.194212	11.266688
10.513002	597.224923	11.271706
10.221448	608.217997	11.276723
10.454714	601.172313	11.281741
10.357447	607.129841	11.286759
10.257463	612.753281	11.291776
10.508457	612.985261	11.296794
10.490239	624.730783	11.301811
10.705690	625.110344	11.306829
10.788453	633.393907	11.311847
10.629723	618.264490	11.316864
10.822547	622.447189	11.321882
10.600543	611.644837	11.326899
11.075305	621.810953	11.331917
10.750517	620.640450	11.336935
10.436966	617.082396	11.341952
10.840600	609.038026	11.346970
10.670263	619.043283	11.351987
10.880197	615.715635	11.357005
10.644697	607.547343	11.362023
10.495975	615.775648	11.367040
10.969770	621.893016	11.372058
10.717458	625.126133	11.377075
10.944343	625.929937	11.382093
10.678294	626.937206	11.387111
10.861416	630.225178	11.392128
10.939868	628.540214	11.397146
10.674852	632.397017	11.402163
10.882754	629.713470	11.407181
10.525548	635.475049	11.412199
10.507573	634.341680	11.417216
10.850885	624.293348	11.422234
10.458522	629.643867	11.427251
11.029705	626.237525	11.432269
10.782186	629.072261	11.437287
10.709799	630.569896	11.442304
11.029860	622.794235	11.447322
11.056736	635.801334	11.452339
10.796288	626.462981	11.457357
10.678260	627.361851	11.462375
10.728152	632.371678	11.467392
11.063415	626.029528	11.472410
10.806212	629.430671	11.477427
10.808891	632.500761	11.482445
10.705554	626.239953	11.487463
10.770679	640.740072	11.492480
11.153002	648.181443	11.497498
10.889255	650.993477	11.502515
11.002396	648.735030	11.507533
10.914357	661.876918	11.512551
11.500531	657.549880	11.517568
11.480915	645.810078	11.522586
10.834141	639.691216	11.527603
11.181907	639.753400	11.532621
11.305479	648.469234	11.537639
10.992778	637.652674	11.542656
11.135669	642.559571	11.547674
11.184214	648.980262	11.552691
11.374982	636.762533	11.557709
11.176596	630.005376	11.562727
10.970276	640.183540	11.567744
11.158306	638.784364	11.572762
11.248812	653.163752	11.577779
10.628557	653.194568	11.582797
11.480606	652.578137	11.587815
11.218163	658.763533	11.592832
11.618941	656.860807	11.597850
11.261394	656.891487	11.602867
11.263211	654.849298	11.607885
11.607428	649.190548	11.612903
10.755759	631.503027	11.617920
11.698327	636.382459	11.622938
11.443551	635.355620	11.627955
11.212228	635.284473	11.632973
11.295040	621.246988	11.637991
11.256311	628.716451	11.643008
11.198382	632.278876	11.648026
11.114209	645.167681	11.653043
11.551005	653.064423	11.658061
11.589823	646.248003	11.663079
11.607088	653.052294	11.668096
11.448194	626.495697	11.673114
11.357240	626.879085	11.678131
11.081524	622.005441	11.683149
11.901844	633.569094	11.688167
11.464369	646.235543	11.693184
11.375549	622.265207	11.698202
11.611101	624.964294	11.703219
11.069231	623.562715	11.708237
11.213003	628.415821	11.713255
11.454851	648.439327	11.718272
11.818021	642.266368	11.723290
11.507013	641.952086	11.728307
11.235650	649.953469	11.733325
11.533143	655.694527	11.738343
11.700917	651.644484	11.743360
11.782919	639.229201	11.748378
11.797870	629.721464	11.753395
11.468525	622.277926	11.758413
11.232416	620.882090	11.763431
11.191655	630.706105	11.768448
11.448528	640.335169	11.773466
11.512654	649.142368	11.778483
11.290278	645.705723	11.783501
11.528516	646.880135	11.788519
11.366968	652.983450	11.793536
11.395641	656.841581	11.798554
11.252015	645.903851	11.803571
11.059221	645.697279	11.808589
11.652931	654.718152	11.813607
11.609145	668.026681	11.818624
11.885046	669.517086	11.823642
11.779210	672.099255	11.828659
11.926872	679.003046	11.833677
12.001498	666.595211	11.838695
11.631815	661.196634	11.843712
11.601167	659.768603	11.848730
11.986258	670.437948	11.853747
12.049116	673.448124	11.858765
11.852687	658.927339	11.863783
11.415387	654.363027	11.868800
11.867963	651.215106	11.873818
11.908996	662.190818	11.878835
11.782134	662.595611	11.883853
12.023304	659.831107	11.888871
11.611811	663.480493	11.893888
11.699111	668.244627	11.898906
11.825039	668.830721	11.903923
12.078719	670.318296	11.908941
12.181197	673.789325	11.913959
11.992588	669.482691	11.918976
11.646203	653.385407	11.923994
11.916627	663.690860	11.929011
11.960860	670.617165	11.934029
11.835477	668.705358	11.939047
12.038654	675.474217	11.944064
12.322139	679.958306	11.949082
12.018527	674.038131	11.954099
11.938480	676.751960	11.959117
11.960728	670.597693	11.964135
11.530320	684.727362	11.969152
11.910862	677.999401	11.974170
12.148350	681.102137	11.979187
12.012268	677.083918	11.984205
12.130317	678.684264	11.989223
12.115314	677.588297	11.994240
12.324692	679.862302	11.999258
12.265524	677.782328	12.004275
12.039209	668.549058	12.009293
12.250277	674.919048	12.014311
11.743798	680.082333	12.019328
12.065524	676.459446	12.024346
12.375415	678.345316	12.029363
12.096702	675.403487	12.034381
12.214811	673.677592	12.039399
12.570676	668.872237	12.044416
11.955059	679.064059	12.049434
12.211652	664.469135	12.054451
12.118208	665.771256	12.059469
12.178666	669.094232	12.064487
11.972583	673.027018	12.069504
12.313033	662.726648	12.074522
12.281626	674.354348	12.079539
11.994213	674.923152	12.084557
12.118716	677.077910	12.089575
12.222739	685.575918	12.094592
12.134844	675.781312	12.099610
12.154033	673.180975	12.104627
12.355861	668.974114	12.109645
12.483957	670.566573	12.114663
12.194307	675.396081	12.119680
12.584123	670.635900	12.124698
12.237336	673.072783	12.129715
12.353329	678.144851	12.134733
12.323561	672.819246	12.139751
12.229311	680.007094	12.144768
12.428504	686.410506	12.149786
12.710238	692.475939	12.154803
12.519561	688.245364	12.159821
12.433858	677.484733	12.164839
12.191352	679.690683	12.169856
12.200264	682.901817	12.174874
12.556446	687.718503	12.179891
12.893655	691.165380	12.184909
12.557235	687.399455	12.189927
12.398897	687.720818	12.194944
12.328675	690.654016	12.199962
12.828967	683.957784	12.204979
12.443526	692.336823	12.209997
12.870439	684.964118	12.215015
12.862101	695.111294	12.220032
12.551464	681.230082	12.225050
12.536994	680.137187	12.230067
12.814596	690.621413	12.235085
12.795387	672.509930	12.240103
12.402061	673.581325	12.245120
12.587790	679.993156	12.250138
12.872163	691.249497	12.255155
12.557583	698.503432	12.260173
12.548322	682.504781	12.265191
12.927054	693.717937	12.270208
12.731657	685.038395	12.275226
12.913158	694.777129	12.280243
12.648908	689.617646	12.285261
12.795329	679.559106	12.290279
12.619443	689.334897	12.295296
12.802604	693.831553	12.300314
12.687186	688.225871	12.305331
12.687662	700.404017	12.310349
12.524160	687.336041	12.315367
12.499623	689.709813	12.320384
12.758034	683.875147	12.325402
12.737599	697.489309	12.330419
12.457371	696.936672	12.335437
12.829016	689.844025	12.340455
12.658071	698.072694	12.345472
12.639370	698.176518	12.350490
12.802542	691.154404	12.355507
12.730668	707.433834	12.360525
13.283430	708.833527	12.365543
13.063040	706.763031	12.370560
12.846991	708.617698	12.375578
13.005885	697.547331	12.380595
12.936208	697.040600	12.385613
13.015172	703.308221	12.390631
13.218586	710.888103	12.395648
12.992845	692.597518	12.400666
13.054701	694.620083	12.405683
12.462542	696.994428	12.410701
12.658802	705.632628	12.415719
12.700976	706.635791	12.420736
12.846021	710.440986	12.425754
13.101891	703.063515	12.430771
13.228925	715.969772	12.435789
13.141374	717.021663	12.440807
13.094028	714.160343	12.445824
12.807894	709.607046	12.450842
13.103379	706.546845	12.455859
12.803366	709.449778	12.460877
13.091580	717.941033	12.465895
13.176148	712.146219	12.470912
13.328541	707.025594	12.475930
13.140439	705.123609	12.480947
13.141948	723.354478	12.485965
13.297784	713.483794	12.490983
13.288718	712.693009	12.496000
13.350846	738.958595	12.501018
13.669620	718.168461	12.506035
13.025104	716.066584	12.511053
13.243739	712.434596	12.516071
13.658420	711.580574	12.521088
13.441229	721.274491	12.526106
13.460693	712.141547	12.531123
13.193549	717.469316	12.536141
13.274987	715.370463	12.541159
13.453441	714.752271	12.546176
13.305843	711.966620	12.551194
13.574849	706.953957	12.556211
13.462187	710.578622	12.561229
13.684652	703.133800	12.566247
13.775021	710.737705	12.571264
13.606669	709.719412	12.576282
13.440354	709.966285	12.581299
13.423827	711.278448	12.586317
13.324557	704.145969	12.591335
13.445250	708.579832	12.596352
13.434634	706.829921	12.601370
13.380975	700.141579	12.606387
13.203186	705.603669	12.611405
13.508027	727.207928	12.616423
13.691568	725.389724	12.621440
13.241994	728.697949	12.626458
13.631470	726.333079	12.631475
13.982899	718.009660	12.636493
13.687684	722.000604	12.641511
13.549748	733.865941	12.646528
13.728685	733.777851	12.651546
14.080641	729.743115	12.656563
13.548680	721.542325	12.661581
13.682789	711.324749	12.666599
13.887080	716.083190	12.671616
13.602631	714.780127	12.676634
13.630344	708.808028	12.681651
13.902262	712.927863	12.686669
13.595961	711.738678	12.691687
13.616856	719.615406	12.696704
13.681695	730.417016	12.701722
14.097714	728.385661	12.706739
13.881954	729.018980	12.711757
13.841836	717.897730	12.716775
14.043863	721.416287	12.721792
13.867935	716.744734	12.726810
13.998637	705.221184	12.731827
13.790858	709.763317	12.736845
13.631207	716.128290	12.741863
14.003538	717.070257	12.746880
14.035497	729.316073	12.751898
14.048137	712.465046	12.756915
13.979435	713.425621	12.761933
14.110713	715.279519	12.766951
14.045987	702.732545	12.771968
13.937143	713.466682	12.776986
14.100607	707.571145	12.782003
13.681868	716.087957	12.787021
13.559476	713.746483	12.792039
14.003568	724.371903	12.797056
13.928098	741.005380	12.802074
14.123189	732.968383	12.807091
13.700187	747.232641	12.812109
13.977029	735.522071	12.817127
14.115852	738.526667	12.822144
14.046251	735.088158	12.827162
13.966649	737.764057	12.832179
14.213474	741.856272	12.837197
14.351725	744.081468	12.842215
14.344677	731.563307	12.847232
14.098620	744.073601	12.852250
14.303287	733.551466	12.857267
14.093349	735.146401	12.862285
14.136333	739.018086	12.867303
14.127708	730.934113	12.872320
13.839852	740.718007	12.877338
14.139321	734.394050	12.882355
13.985923	735.090183	12.887373
13.832142	735.483416	12.892391
14.382221	734.990035	12.897408
14.255299	741.706497	12.902426
14.387819	741.291162	12.907443
14.156140	740.001920	12.912461
14.127124	738.728263	12.917479
14.562606	739.224832	12.922496
14.284710	758.146459	12.927514
14.737231	750.848611	12.932531
14.380849	749.818749	12.937549
14.483037	740.836933	12.942567
14.782433	735.942577	12.947584
14.249336	735.139222	12.952602
14.530229	734.344031	12.957619
14.427013	734.461097	12.962637
14.110632	738.259698	12.967655
14.588569	736.325940	12.972672
14.334076	749.894762	12.977690
14.304570	759.855941	12.982707
14.215686	759.942359	12.987725
14.230430	761.745092	12.992743
14.512951	769.874343	12.997760
14.488715	760.962817	13.002778
14.543019	762.065069	13.007795
14.713106	761.943652	13.012813
14.230264	764.048411	13.017831
14.914850	766.339491	13.022848
14.553701	761.807401	13.027866
14.739182	770.213791	13.032883
14.897324	768.128160	13.037901
14.345591	765.279587	13.042919
14.780794	759.070056	13.047936
14.549816	762.789009	13.052954
14.644844	752.956233	13.057971
14.854088	761.059091	13.062989
14.497836	753.572376	13.068007
14.556499	753.862896	13.073024
14.415012	757.444750	13.078042
14.884941	766.825904	13.083059
14.877161	783.764398	13.088077
14.733988	785.803318	13.093095
15.157309	780.283613	13.098112
14.858246	777.862513	13.103130
14.939606	762.673265	13.108147
14.844957	762.962559	13.113165
14.769002	753.001936	13.118183
15.294257	752.376744	13.123200
14.947495	756.464134	13.128218
14.816774	756.033238	13.133235
15.077736	757.068397	13.138253
14.650913	763.159663	13.143271
14.961206	755.704214	13.148288
14.714807	767.826411	13.153306
15.137000	775.245809	13.158323
15.195357	772.516243	13.163341
14.981735	781.051442	13.168359
15.239654	768.943024	13.173376
15.138698	773.727215	13.178394
15.119008	768.115977	13.183411
14.885080	765.766725	13.188429
15.113307	776.930931	13.193447
15.217326	780.739414	13.198464
15.427382	773.331221	13.203482
15.186054	765.697106	13.208499
15.273340	760.236369	13.213517
14.809695	757.064724	13.218535
15.413200	761.050566	13.223552
15.293394	771.268898	13.228570
15.385675	762.443259	13.233587
15.250921	757.686348	13.238605
15.117516	754.718584	13.243623
15.141564	748.598722	13.248640
15.496894	764.318961	13.253658
15.357953	761.311037	13.258675
15.265852	753.085497	13.263693
14.970540	754.274084	13.268711
15.477109	767.729989	13.273728
15.468583	778.893421	13.278746
15.525889	767.583304	13.283763
15.782365	757.292880	13.288781
14.949480	760.544402	13.293799
15.316634	760.947535	13.298816
15.556261	774.312724	13.303834
15.507397	774.058353	13.308851
15.660837	770.480749	13.313869
15.383054	760.113084	13.318887
15.168894	765.236904	13.323904
15.336310	780.286004	13.328922
15.382146	776.744193	13.333939
15.383332	772.117460	13.338957
15.503890	775.756091	13.343975
15.745228	774.799837	13.348992
15.425041	787.274439	13.354010
15.672553	781.665513	13.359027
15.523295	777.709297	13.364045
15.637064	779.969892	13.369063
15.686227	772.978232	13.374080
15.581704	774.212668	13.379098
15.363044	773.164383	13.384115
15.513434	779.531294	13.389133
15.393901	775.314798	13.394151
15.449912	778.559596	13.399168
15.497263	778.182851	13.404186
15.068548	778.868473	13.409203
15.454684	780.625642	13.414221
15.665616	799.243502	13.419239
15.754104	792.876841	13.424256
15.926864	800.871823	13.429274
15.969794	797.800684	13.434291
16.024570	797.318633	13.439309
15.883633	806.208532	13.444327
16.037094	795.751188	13.449344
15.941576	799.915990	13.454362
15.631280	798.377126	13.459379
16.195263	798.291825	13.464397
16.176754	797.155374	13.469415
16.304244	801.461962	13.474432
15.990753	789.430435	13.479450
15.832542	774.748932	13.484467
15.806672	764.830949	13.489485
15.475140	774.568056	13.494503
15.911627	779.899209	13.499520
15.714616	788.756860	13.504538
15.547955	789.265722	13.509555
16.241032	787.831587	13.514573
16.308613	794.861580	13.519591
16.422731	794.499621	13.524608
16.070982	793.172382	13.529626
15.845141	793.450673	13.534643
16.396593	796.633628	13.539661
15.798248	795.973038	13.544679
15.617257	800.141764	13.549696
15.614265	794.682538	13.554714
15.764124	804.034964	13.559731
16.110226	813.000039	13.564749
16.271571	825.023675	13.569767
16.305715	819.650142	13.574784
16.549189	827.675083	13.579802
16.470783	812.144747	13.584819
16.303052	807.954730	13.589837
16.315973	801.438957	13.594855
16.127269	798.382019	13.599872
16.169026	804.920596	13.604890
16.303808	812.164132	13.609907
16.789837	821.836286	13.614925
16.098163	816.589099	13.619943
16.334816	819.878185	13.624960
16.671778	824.047816	13.629978
16.604959	822.950491	13.634995
16.751453	796.727650	13.640013
16.231857	801.388090	13.645031
16.586744	798.340657	13.650048
16.467932	797.595467	13.655066
16.463980	800.893845	13.660083
16.772255	797.907365	13.665101
16.432835	789.868882	13.670119
16.535129	784.096514	13.675136
16.646393	794.142955	13.680154
16.103020	797.428018	13.685171
16.759487	801.481311	13.690189
16.979696	806.890541	13.695207
16.896525	799.821773	13.700224
16.729433	797.345280	13.705242
16.618098	793.184300	13.710259
16.808894	789.042256	13.715277
16.659029	793.991907	13.720295
16.915721	797.375681	13.725312
16.676131	789.892763	13.730330
16.686342	783.241721	13.735347
16.825780	790.787479	13.740365
16.776839	799.233768	13.745383
16.589234	796.542735	13.750400
16.780188	791.229849	13.755418
16.569630	795.128649	13.760435
17.018949	788.049040	13.765453
16.919313	791.261422	13.770471
16.803161	794.596314	13.775488
16.578995	798.146948	13.780506
16.943749	799.298392	13.785523
16.878932	799.538831	13.790541
16.396592	822.636175	13.795559
16.816134	821.263830	13.800576
16.714303	817.966056	13.805594
16.521551	820.656539	13.810611
16.802568	817.270379	13.815629
17.088870	818.913804	13.820647
16.586685	817.382913	13.825664
16.862216	810.440979	13.830682
16.535713	814.174910	13.835699
16.908001	823.975341	13.840717
16.854278	836.430318	13.845735
16.648689	836.159475	13.850752
17.312047	840.325308	13.855770
16.943016	842.147153	13.860787
17.226175	840.035616	13.865805
17.138645	835.700480	13.870823
17.040015	842.027534	13.875840
17.290976	846.617749	13.880858
17.412891	851.177690	13.885875
17.608909	832.319101	13.890893
17.360929	844.391104	13.895911
17.039076	845.448154	13.900928
17.244340	841.644663	13.905946
17.005704	844.859898	13.910963
17.223898	845.112801	13.915981
17.251094	845.304109	13.920999
16.954584	848.452672	13.926016
17.402133	840.000526	13.931034
17.262944	835.992225	13.936051
17.120314	837.153740	13.941069
17.392230	840.219552	13.946087
17.212604	843.150982	13.951104
17.387767	845.275733	13.956122
17.287758	865.258369	13.961139
17.492626	874.640084	13.966157
17.390127	871.825250	13.971175
17.363652	873.801713	13.976192
17.853298	867.697225	13.981210
17.487053	861.594294	13.986227
17.456252	863.460979	13.991245
18.034558	864.443267	13.996263
17.892697	861.502056	14.001280
17.854580	847.230873	14.006298
17.506793	849.298702	14.011315
17.772796	837.697063	14.016333
17.607032	833.629810	14.021351
17.578757	837.922941	14.026368
17.863823	842.895981	14.031386
17.731372	839.085442	14.036403
17.945842	829.906105	14.041421
17.766800	832.951052	14.046439
17.529735	839.432340	14.051456
17.873432	840.820619	14.056474
17.683508	846.612861	14.061491
17.661545	855.802885	14.066509
17.894215	849.969042	14.071527
17.428906	855.880174	14.076544
17.815978	868.168279	14.081562
17.533137	857.226985	14.086579
17.888429	858.714435	14.091597
18.076817	862.809522	14.096615
17.554622	864.756355	14.101632
17.851971	859.051233	14.106650
17.557632	858.497645	14.111667
18.139393	853.426472	14.116685
18.297699	855.717969	14.121703
17.969551	867.225027	14.126720
18.175285	852.653698	14.131738
17.881676	857.477563	14.136755
18.153898	855.446634	14.141773
18.020427	855.811440	14.146791
17.901418	865.288077	14.151808
17.955632	857.172110	14.156826
18.038349	865.553620	14.161843
17.728053	860.802094	14.166861
18.148041	865.807650	14.171879
17.913892	872.654572	14.176896
18.145249	873.505025	14.181914
18.421397	886.915070	14.186931
18.201548	883.963985	14.191949
18.066157	872.996422	14.196967
18.028532	886.802773	14.201984
18.231906	878.234230	14.207002
18.203726	895.586287	14.212019
18.071620	888.948036	14.217037
18.258442	875.875527	14.222055
18.259281	878.352647	14.227072
18.211390	881.064624	14.232090
18.480493	880.145041	14.237107
18.746591	874.337512	14.242125
18.451718	879.123711	14.247143
17.936145	884.061257	14.252160
18.392076	882.354997	14.257178
18.289004	875.342967	14.262195
18.524542	884.072932	14.267213
18.273702	897.161604	14.272231
18.618479	906.436207	14.277248
18.749585	896.461997	14.282266
18.787283	904.923163	14.287283
18.614456	890.193362	14.292301
18.882822	876.432722	14.297319
18.686135	878.439010	14.302336
19.012491	877.974367	14.307354
18.710665	882.562838	14.312371
18.626863	879.530475	14.317389
18.767581	878.324890	14.322407
18.580762	881.964364	14.327424
18.878346	877.928647	14.332442
18.687612	882.988869	14.337459
18.745730	882.234889	14.342477
18.826705	875.724206	14.347495
18.665378	882.013759	14.352512
18.689189	871.668204	14.357530
18.733540	887.550886	14.362547
19.090389	896.186110	14.367565
19.157408	883.826653	14.372583
18.782882	879.965669	14.377600
18.746761	879.437897	14.382618
19.223265	884.238940	14.387635
18.893783	883.239570	14.392653
19.155791	877.066602	14.397671
18.732072	876.075686	14.402688
19.328243	883.644599	14.407706
19.017588	883.024138	14.412723
18.941847	872.205023	14.417741
18.880394	888.792259	14.422759
18.913179	899.387551	14.427776
19.434927	897.039806	14.432794
19.346950	911.759796	14.437811
19.124809	891.808461	14.442829
19.261070	887.337262	14.447847
19.019324	883.303993	14.452864
19.362301	893.617148	14.457882
19.197541	895.659461	14.462899
19.040015	887.936423	14.467917
19.250928	894.634725	14.472935
19.099929	897.574302	14.477952
19.613428	892.706320	14.482970
19.218297	900.137061	14.487987
19.238528	902.292405	14.493005
19.181959	901.206093	14.498023
18.879728	908.527606	14.503040
19.335521	898.767616	14.508058
19.402280	908.937861	14.513075
19.509490	907.866914	14.518093
19.628511	897.276049	14.523111
18.896759	916.180588	14.528128
19.449681	901.911434	14.533146
19.385625	905.755744	14.538163
19.552343	905.117294	14.543181
19.343295	897.014153	14.548199
19.441484	908.429193	14.553216
19.482101	906.352493	14.558234
19.728255	903.896446	14.563251
19.381446	914.898365	14.568269
19.787273	898.446314	14.573287
19.304548	907.127879	14.578304
19.438588	901.757605	14.583322
19.544103	911.981741	14.588339
19.825749	921.663882	14.593357
19.776657	930.410062	14.598375
19.450707	926.831797	14.603392
19.871078	933.431023	14.608410
19.996899	922.488777	14.613427
19.869915	913.511221	14.618445
20.096755	905.238795	14.623463
19.626491	905.022043	14.628480
19.919259	902.931084	14.633498
19.944421	896.078838	14.638515
19.809938	915.773437	14.643533
20.091501	913.444387	14.648551
20.320396	908.327497	14.653568
19.788887	901.108024	14.658586
20.150361	907.337766	14.663603
19.545714	912.418665	14.668621
20.015580	904.218618	14.673639
19.984326	916.392415	14.678656
20.171216	920.923259	14.683674
20.162265	918.406191	14.688691
19.831995	918.767119	14.693709
20.155179	909.690630	14.698727
20.227430	920.844650	14.703744
20.459506	922.187307	14.708762
20.195939	907.733644	14.713779
19.742877	907.088157	14.718797
20.224355	914.555130	14.723815
20.114070	932.863690	14.728832
20.071879	926.097726	14.733850
20.494134	931.923470	14.738867
20.378214	918.551218	14.743885
20.244671	930.595881	14.748903
20.286492	927.606946	14.753920
20.284268	925.738931	14.758938
19.975256	928.883154	14.763955
20.066810	921.730157	14.768973
20.169005	920.218174	14.773991
19.923082	925.820396	14.779008
19.989693	929.877773	14.784026
20.062310	927.691913	14.789043
20.304768	940.536067	14.794061
20.456432	948.423965	14.799079
20.658361	951.939428	14.804096
20.775192	957.481668	14.809114
20.973143	952.072963	14.814131
20.486312	930.070717	14.819149
20.338614	924.056600	14.824167
20.566595	929.956964	14.829184
20.503539	944.834026	14.834202
20.641463	950.928391	14.839219
20.547464	953.546616	14.844237
20.652479	951.522938	14.849255
20.815156	951.917088	14.854272
20.746215	953.991733	14.859290
21.086881	952.051056	14.864307
20.927886	963.074073	14.869325
20.653916	954.040630	14.874343
20.525450	951.229852	14.879360
20.508490	945.927406	14.884378
20.629671	951.532080	14.889395
20.607096	954.252725	14.894413
20.638477	944.366698	14.899431
20.768672	948.609781	14.904448
20.525281	944.658808	14.909466
20.878882	946.335883	14.914483
20.747929	948.499141	14.919501
21.256846	947.248485	14.924519
20.627226	945.857472	14.929536
20.693021	957.741531	14.934554
21.151677	967.266572	14.939571
20.853922	976.099073	14.944589
20.832043	974.224665	14.949607
20.971594	971.722194	14.954624
20.915307	971.566814	14.959642
21.201411	968.918302	14.964659
20.916928	968.514648	14.969677
21.004771	969.854660	14.974695
20.819643	978.013095	14.979712
20.903707	978.362756	14.984730
21.297561	964.708623	14.989747
20.808852	975.306770	14.994765
21.242138	984.715872	14.999783
21.392563	990.382249	15.004800
21.249896	989.902725	15.009818
21.534698	991.568493	15.014835
21.549238	1000.405726	15.019853
21.577807	989.519703	15.024871
21.453927	986.509382	15.029888
21.373770	991.571244	15.034906
21.910555	993.992812	15.039923
21.335957	988.111834	15.044941
21.358659	977.845288	15.049959
21.451167	977.761272	15.054976
21.637061	986.852523	15.059994
21.674385	981.746693	15.065011
21.527034	992.985659	15.070029
21.621257	992.462707	15.075047
21.740221	989.894029	15.080064
21.724343	987.983965	15.085082
21.498703	977.374469	15.090099
21.704015	983.742315	15.095117
21.874061	986.921946	15.100135
21.843460	984.540808	15.105152
21.604344	991.054031	15.110170
21.717632	985.522878	15.115187
21.624474	983.678572	15.120205
21.793927	988.470947	15.125223
22.037625	982.812063	15.130240
21.649090	987.297378	15.135258
22.136319	987.546001	15.140275
21.853646	995.486193	15.145293
21.974999	992.200757	15.150311
22.153078	983.588788	15.155328
21.741171	989.516844	15.160346
21.809285	981.379707	15.165363
21.850482	987.546046	15.170381
22.009555	981.900421	15.175399
22.130455	981.231276	15.180416
22.078889	984.025897	15.185434
22.298345	979.415406	15.190451
21.913478	986.393285	15.195469
21.865251	986.571165	15.200487
22.142726	983.447466	15.205504
22.079747	988.983174	15.210522
22.404442	978.817637	15.215539
22.034186	993.111697	15.220557
22.231006	990.180518	15.225575
22.164598	988.685479	15.230592
22.050004	989.754246	15.235610
22.321375	983.453539	15.240627
22.258785	990.990010	15.245645
22.231606	996.507487	15.250663
22.756594	982.782299	15.255680
22.424015	988.391806	15.260698
22.146702	993.304675	15.265715
21.941009	986.819931	15.270733
22.112914	1003.588467	15.275751
22.406305	993.421515	15.280768
22.362279	996.309633	15.285786
22.318200	1006.781329	15.290803
22.372341	1020.393520	15.295821
22.520340	1020.016781	15.300839
22.425133	1015.004291	15.305856
22.320844	1019.823784	15.310874
22.669313	1014.890106	15.315891
22.531453	1016.975557	15.320909
22.597013	1018.221231	15.325927
22.833631	1010.272280	15.330944
22.597686	1020.483705	15.335962
22.832131	1018.591223	15.340979
22.374004	1021.651525	15.345997
22.339759	1020.362888	15.351015
22.814608	1015.030703	15.356032
22.480896	1019.914545	15.361050
22.917372	1005.000819	15.366067
22.635978	1018.286875	15.371085
22.918817	1031.790657	15.376103
23.281918	1026.015219	15.381120
22.959269	1022.019841	15.386138
23.129270	1014.179158	15.391155
23.478184	1004.726197	15.396173
22.986002	1007.088073	15.401191
22.880392	1004.504085	15.406208
22.702452	1005.762663	15.411226
22.638159	998.753976	15.416243
22.921309	1021.251948	15.421261
22.654457	1028.104052	15.426279
22.902337	1030.110132	15.431296
22.955839	1022.565416	15.436314
23.537539	1031.323270	15.441331
23.398999	1030.066752	15.446349
23.164097	1032.423035	15.451367
23.504804	1026.562741	15.456384
23.219331	1030.056752	15.461402
23.647177	1024.072350	15.466419
23.316817	1027.377730	15.471437
23.284768	1028.105354	15.476455
23.643155	1026.632120	15.481472
23.196512	1028.516637	15.486490
23.512365	1026.636646	15.491507
23.252355	1025.787333	15.496525
23.454245	1032.805845	15.501543
23.689320	1023.670519	15.506560
23.556698	1037.501338	15.511578
23.509104	1027.223686	15.516595
23.462100	1031.365161	15.521613
23.459477	1025.381930	15.526631
23.612703	1026.945237	15.531648
23.419439	1032.567645	15.536666
23.425478	1024.216147	15.541683
23.631009	1031.218308	15.546701
23.291290	1027.812597	15.551719
23.286392	1029.583720	15.556736
23.105560	1020.813367	15.561754
23.284108	1027.718767	15.566771
23.801362	1044.638365	15.571789
23.688335	1047.486808	15.576807
24.101515	1045.408525	15.581824
23.779454	1050.918570	15.586842
23.744541	1052.246263	15.591859
23.929804	1053.627824	15.596877
23.750776	1048.300245	15.601895
23.828771	1051.601610	15.606912
23.612687	1055.637034	15.611930
23.835991	1055.728190	15.616947
23.908593	1052.292587	15.621965
23.866081	1046.381873	15.626983
24.123974	1044.820238	15.632000
23.608293	1044.386532	15.637018
23.758835	1039.780511	15.642035
24.455421	1045.493881	15.647053
23.730360	1048.627570	15.652071
23.907789	1038.967924	15.657088
23.663958	1057.041908	15.662106
24.155424	1059.726212	15.667123
24.206744	1069.794824	15.672141
24.053694	1059.947098	15.677159
24.201693	1061.710048	15.682176
24.002161	1068.968198	15.687194
24.482005	1070.963186	15.692211
24.217042	1066.340205	15.697229
24.356232	1065.207432	15.702247
24.725509	1067.387005	15.707264
24.607901	1062.728315	15.712282
24.780161	1065.970731	15.717299
24.799139	1068.924731	15.722317
24.600627	1060.466406	15.727335
24.747578	1053.427756	15.732352
24.554214	1065.444012	15.737370
24.654027	1063.787220	15.742387
24.640149	1063.003485	15.747405
24.584113	1049.094719	15.752423
24.802530	1055.542592	15.757440
24.605831	1061.408549	15.762458
24.810842	1057.273684	15.767475
24.753665	1051.630360	15.772493
24.809505	1053.941093	15.777511
24.552414	1049.171713	15.782528
24.701506	1052.594486	15.787546
24.584658	1052.398101	15.792563
24.493864	1052.876148	15.797581
24.928484	1057.283004	15.802599
24.857266	1052.156289	15.807616
24.764589	1065.586386	15.812634
24.769841	1059.238983	15.817651
24.686455	1059.857885	15.822669
24.652638	1053.437708	15.827687
24.755504	1050.161470	15.832704
24.706369	1060.274219	15.837722
24.604281	1058.551228	15.842739
24.896399	1058.417001	15.847757
25.117697	1072.138746	15.852775
25.098707	1085.424764	15.857792
24.782338	1077.410942	15.862810
25.209104	1077.227216	15.867827
25.235659	1069.513128	15.872845
25.343933	1073.800702	15.877863
25.595639	1066.666737	15.882880
25.364016	1080.408956	15.887898
25.542726	1075.454521	15.892915
25.473569	1055.094015	15.897933
24.926300	1062.485542	15.902951
25.359540	1067.517483	15.907968
25.415789	1082.259198	15.912986
25.656016	1082.483406	15.918003
25.525067	1064.972871	15.923021
25.106676	1064.621754	15.928039
25.284652	1060.708880	15.933056
25.401830	1074.753061	15.938074
25.231715	1085.998807	15.943091
25.772383	1084.736857	15.948109
25.457621	1076.924760	15.953127
25.559176	1074.775374	15.958144
25.665565	1077.917657	15.963162
25.561283	1077.589911	15.968179
25.495790	1072.765258	15.973197
25.138380	1072.467704	15.978215
25.325711	1064.374969	15.983232
25.309500	1080.866930	15.988250
25.140359	1100.207391	15.993267
25.792383	1091.416969	15.998285
25.564706	1100.898133	16.003303
25.810546	1096.308726	16.008320
25.665774	1096.400745	16.013338
25.929699	1101.585459	16.018355
25.492448	1099.419501	16.023373
25.741185	1099.506672	16.028391
26.017292	1099.557996	16.033408
26.026453	1095.220272	16.038426
25.936979	1103.953929	16.043443
26.164677	1095.476148	16.048461
26.029839	1094.503075	16.053479
25.798832	1099.746398	16.058496
25.826481	1105.659273	16.063514
26.185824	1111.472842	16.068531
26.238394	1108.785158	16.073549
26.237424	1123.640017	16.078567
26.465100	1113.710518	16.083584
26.716014	1114.147653	16.088602
26.655194	1107.242524	16.093619
26.524983	1095.305154	16.098637
26.213430	1088.978974	16.103655
26.091380	1080.593868	16.108672
26.116699	1086.466075	16.113690
26.063850	1095.244484	16.118707
26.661238	1100.212844	16.123725
26.749862	1105.336660	16.128743
26.660419	1099.048262	16.133760
26.749945	1097.882242	16.138778
26.228530	1088.814913	16.143795
26.568986	1084.324297	16.148813
26.448100	1096.903590	16.153831
26.727369	1103.881604	16.158848
26.748388	1115.573962	16.163866
26.741135	1109.660858	16.168883
26.503970	1102.644501	16.173901
26.451510	1105.729624	16.178919
26.507599	1114.169072	16.183936
26.880234	1117.547366	16.188954
26.566274	1112.613305	16.193971
26.939601	1108.840232	16.198989
26.643367	1116.747886	16.204007
26.730449	1111.706808	16.209024
26.786366	1103.180196	16.214042
26.670890	1112.631163	16.219059
26.978049	1117.894317	16.224077
26.904558	1118.593724	16.229095
26.769480	1111.476160	16.234112
26.800470	1104.938510	16.239130
26.756042	1117.815117	16.244147
27.364387	1109.848907	16.249165
27.050817	1110.118856	16.254183
27.142162	1115.355861	16.259200
27.028833	1108.332723	16.264218
27.128636	1109.049160	16.269235
27.381967	1107.431429	16.274253
26.751741	1117.038789	16.279271
27.061124	1128.326204	16.284288
27.207892	1127.425776	16.289306
27.408650	1144.410837	16.294323
27.352457	1136.798050	16.299341
27.592844	1138.417140	16.304359
27.597467	1146.148279	16.309376
27.313604	1139.142379	16.314394
27.277924	1140.508070	16.319411
27.648729	1131.736442	16.324429
27.613092	1131.947066	16.329447
27.701046	1139.478947	16.334464
27.491032	1138.205216	16.339482
27.536055	1132.448021	16.344499
27.816597	1142.654335	16.349517
27.573165	1141.543635	16.354535
27.686435	1141.825605	16.359552
27.693420	1143.121493	16.364570
27.824960	1145.754903	16.369587
27.965306	1138.682540	16.374605
27.701240	1136.741915	16.379623
27.740914	1134.845223	16.384640
27.991387	1134.244136	16.389658
27.773850	1137.759083	16.394675
27.777015	1132.377686	16.399693
27.677437	1133.324185	16.404711
27.750784	1138.873295	16.409728
28.050707	1127.199880	16.414746
27.813430	1129.591263	16.419763
27.796858	1130.351182	16.424781
28.017522	1132.311043	16.429799
27.786233	1130.422090	16.434816
28.113561	1131.891855	16.439834
27.846101	1133.748309	16.444851
27.946554	1134.234265	16.449869
27.720509	1139.164388	16.454887
28.081913	1151.974278	16.459904
28.193679	1159.111105	16.464922
28.107612	1167.651749	16.469939
28.343692	1164.853252	16.474957
28.430950	1163.308874	16.479975
28.452483	1160.938479	16.484992
28.322383	1154.760577	16.490010
28.241128	1158.165810	16.495027
28.722452	1163.420625	16.500045
28.585270	1158.799691	16.505063
28.520750	1151.598470	16.510080
28.904883	1156.565544	16.515098
28.166039	1165.006485	16.520115
28.516702	1159.125653	16.525133
28.609218	1160.528065	16.530151
28.212994	1162.414164	16.535168
28.643669	1155.709729	16.540186
28.625846	1160.465219	16.545203
28.477782	1153.034082	16.550221
28.575229	1159.532504	16.555239
28.386655	1164.311592	16.560256
28.842269	1153.888752	16.565274
28.457105	1161.431651	16.570291
28.802248	1160.610597	16.575309
29.031542	1159.204917	16.580327
28.448715	1167.384722	16.585344
28.705959	1159.227339	16.590362
28.294634	1174.433722	16.595379
28.735994	1177.987458	16.600397
28.875001	1187.483802	16.605415
28.645008	1184.922432	16.610432
29.055662	1185.353476	16.615450
29.024560	1186.964613	16.620467
29.263750	1187.135334	16.625485
29.118409	1177.248464	16.630503
29.142042	1194.185582	16.635520
29.528880	1193.102365	16.640538
29.116156	1193.365759	16.645555
29.381827	1180.321700	16.650573
29.438307	1185.415860	16.655591
29.218678	1187.981216	16.660608
29.437353	1180.035002	16.665626
29.269268	1178.025684	16.670643
29.300235	1185.850545	16.675661
29.468510	1180.190792	16.680679
29.387998	1185.527330	16.685696
29.603543	1181.062571	16.690714
29.616781	1180.965727	16.695731
29.285123	1171.246912	16.700749
29.339538	1174.485720	16.705767
29.345736	1184.836031	16.710784
29.499196	1183.379112	16.715802
29.491512	1201.832823	16.720819
29.209407	1196.006937	16.725837
29.795177	1200.513228	16.730855
29.681395	1209.563180	16.735872
29.824428	1201.180668	16.740890
29.820083	1206.331702	16.745907
29.928926	1204.357891	16.750925
29.847997	1196.853099	16.755943
30.163958	1201.616265	16.760960
30.318489	1200.582069	16.765978
30.602410	1202.330049	16.770995
30.317179	1197.195797	16.776013
30.262338	1183.671760	16.781031
29.896243	1175.296443	16.786048
29.823562	1183.134386	16.791066
29.834278	1190.432229	16.796083
30.164792	1200.283596	16.801101
30.240696	1196.872695	16.806119
30.212416	1196.258475	16.811136
30.561000	1196.894911	16.816154
30.595391	1200.651275	16.821171
30.330564	1193.601345	16.826189
30.225819	1182.013388	16.831207
30.233704	1187.067824	16.836224
30.402706	1202.820800	16.841242
30.298554	1198.380879	16.846259
30.126044	1198.382568	16.851277
30.253546	1194.348181	16.856295
30.050054	1194.982749	16.861312
30.252764	1187.982649	16.866330
30.125525	1194.030277	16.871347
30.610739	1204.977757	16.876365
30.432842	1193.101443	16.881383
30.290902	1196.923304	16.886400
30.397114	1196.792957	16.891418
30.406836	1197.959028	16.896435
30.403071	1216.481570	16.901453
30.652280	1220.766033	16.906471
30.936524	1220.585701	16.911488
31.208552	1212.356549	16.916506
30.677198	1218.442253	16.921523
30.761700	1220.275131	16.926541
31.083570	1219.849054	16.931559
30.968242	1220.665477	16.936576
30.870292	1219.421520	16.941594
30.944147	1220.110469	16.946611
30.856394	1217.062889	16.951629
30.873882	1215.090766	16.956647
30.701397	1215.468004	16.961664
31.077985	1212.666420	16.966682
30.907453	1216.830447	16.971699
30.922619	1218.434338	16.976717
30.989034	1217.975699	16.981735
30.545030	1220.958080	16.986752
31.151305	1238.952706	16.991770
31.230135	1239.735553	16.996787
31.087058	1236.002336	17.001805
31.427784	1236.330725	17.006823
31.371397	1244.276599	17.011840
31.246458	1237.387778	17.016858
31.279785	1242.416151	17.021875
31.459502	1239.948376	17.026893
31.374299	1238.639303	17.031911
31.477705	1242.839315	17.036928
31.109254	1237.888509	17.041946
31.446935	1244.734345	17.046963
31.395424	1258.312776	17.051981
31.863157	1261.489998	17.056999
31.506707	1266.087124	17.062016
31.926419	1263.373454	17.067034
31.836093	1262.052558	17.072051
31.992249	1269.311867	17.077069
31.996701	1262.639457	17.082087
32.091584	1265.079805	17.087104
31.907231	1248.161304	17.092122
32.178777	1234.273655	17.097139
31.538625	1243.828987	17.102157
31.957563	1249.074667	17.107175
31.485448	1262.330823	17.112192
32.066019	1257.587940	17.117210
32.386195	1261.836047	17.122227
32.054887	1260.808537	17.127245
32.210217	1261.812938	17.132263
32.252345	1256.933503	17.137280
32.486841	1258.379952	17.142298
32.546482	1263.565161	17.147315
32.188528	1257.063147	17.152333
32.360974	1249.263005	17.157351
32.056221	1259.876681	17.162368
32.239954	1256.641385	17.167386
32.202705	1255.160690	17.172403
32.185393	1258.252956	17.177421
32.506215	1257.363122	17.182439
32.288572	1254.241209	17.187456
32.699147	1252.709285	17.192474
32.804081	1252.572826	17.197491
32.639894	1261.779030	17.202509
32.845382	1255.425433	17.207527
32.777256	1251.374345	17.212544
32.906285	1256.898987	17.217562
33.175055	1253.483106	17.222579
32.855801	1249.499767	17.227597
32.548754	1234.995844	17.232615
32.464307	1238.370034	17.237632
32.459152	1245.569397	17.242650
32.771938	1247.931419	17.247667
32.335693	1247.781918	17.252685
32.322074	1251.608933	17.257703
32.489277	1261.776266	17.262720
32.000328	1266.599286	17.267738
32.560135	1272.615038	17.272755
32.359989	1278.734081	17.277773
32.817025	1277.024456	17.282791
33.175168	1277.144982	17.287808
32.771008	1282.702676	17.292826
33.194755	1292.227050	17.297843
33.372450	1305.772762	17.302861
33.280528	1296.956784	17.307879
33.508060	1306.565559	17.312896
33.530694	1301.995290	17.317914
33.851331	1283.530128	17.322931
33.310412	1279.240673	17.327949
33.373947	1273.218591	17.332967
33.099392	1274.504948	17.337984
33.337679	1273.287206	17.343002
33.693788	1283.674272	17.348019
33.404363	1296.750345	17.353037
33.665301	1291.902892	17.358055
33.618782	1290.581442	17.363072
33.812610	1293.659569	17.368090
33.729138	1289.740269	17.373107
33.515404	1298.884825	17.378125
33.499071	1291.470862	17.383143
33.558398	1296.214300	17.388160
33.809692	1293.987777	17.393178
33.956353	1295.021942	17.398195
33.711155	1308.327788	17.403213
33.530141	1297.976207	17.408231
33.444820	1302.884326	17.413248
34.074368	1291.875556	17.418266
34.333016	1287.123141	17.423283
33.763458	1296.942006	17.428301
34.244696	1295.559961	17.433319
34.237408	1294.630011	17.438336
33.973493	1291.729943	17.443354
34.129103	1287.047323	17.448371
33.983264	1287.764383	17.453389
34.219482	1289.832283	17.458407
34.164453	1290.787590	17.463424
34.252376	1310.782306	17.468442
34.599673	1311.444195	17.473459
33.911250	1309.178703	17.478477
34.457432	1312.753915	17.483495
34.500232	1318.282619	17.488512
34.564284	1315.075532	17.493530
34.734272	1308.777973	17.498547
34.308986	1320.679252	17.503565
34.589621	1318.965702	17.508583
34.843219	1309.568542	17.513600
34.884397	1317.060488	17.518618
34.876942	1315.824438	17.523635
35.025874	1299.712083	17.528653
34.640281	1292.488523	17.533671
34.631584	1288.608003	17.538688
34.398251	1288.865383	17.543706
34.878519	1296.051831	17.548723
34.881652	1312.960714	17.553741
35.122159	1318.846621	17.558759
34.926654	1315.677045	17.563776
34.740000	1323.870591	17.568794
35.139666	1312.967256	17.573811
35.185759	1320.246986	17.578829
35.130819	1317.815965	17.583847
35.071887	1312.898698	17.588864
35.247651	1313.641114	17.593882
35.289118	1321.625341	17.598899
35.080183	1321.809469	17.603917
35.030428	1310.077108	17.608935
34.975215	1309.047365	17.613952
34.695289	1312.736229	17.618970
34.980671	1308.582402	17.623987
34.808731	1318.332670	17.629005
34.915593	1322.677332	17.634023
34.874548	1326.006866	17.639040
34.941372	1331.358234	17.644058
35.281278	1335.691634	17.649075
35.000624	1326.946238	17.654093
35.083974	1344.764115	17.659111
35.125974	1357.024569	17.664128
34.959661	1357.015818	17.669146
35.319388	1357.609487	17.674163
35.745650	1359.123734	17.679181
36.028646	1355.257461	17.684199
36.030192	1358.671851	17.689216
35.727584	1350.876664	17.694234
36.073191	1347.445570	17.699251
35.754673	1361.640294	17.704269
36.089452	1351.870616	17.709287
36.098580	1353.797370	17.714304
35.866467	1354.389089	17.719322
36.116270	1354.722258	17.724339
36.070689	1354.729307	17.729357
35.942976	1349.750219	17.734375
35.918545	1355.967994	17.739392
36.252426	1363.164781	17.744410
36.401932	1365.138973	17.749427
36.589109	1365.923786	17.754445
36.221919	1368.903624	17.759463
36.624349	1367.224638	17.764480
36.404071	1369.790122	17.769498
36.314297	1350.051074	17.774515
36.220777	1356.181841	17.779533
36.232086	1367.209982	17.784551
36.538701	1370.813273	17.789568
36.607804	1374.813554	17.794586
37.026675	1366.327784	17.799603
37.055054	1370.782588	17.804621
36.658410	1360.650955	17.809639
37.012197	1360.308241	17.814656
36.407809	1350.016651	17.819674
36.576213	1352.019440	17.824691
36.430024	1361.980301	17.829709
36.809626	1367.705570	17.834727
37.032746	1367.982957	17.839744
36.620256	1372.446873	17.844762
36.910393	1366.054726	17.849779
36.545720	1368.485036	17.854797
36.629861	1363.778878	17.859815
36.707251	1365.950570	17.864832
36.965633	1377.123051	17.869850
37.052383	1386.005968	17.874867
37.098399	1388.952629	17.879885
37.299752	1392.588196	17.884903
37.230246	1391.507036	17.889920
37.354662	1398.143337	17.894938
37.262635	1394.449427	17.899955
37.590345	1395.186976	17.904973
37.168411	1386.053413	17.909991
37.464299	1387.180972	17.915008
37.087469	1392.980582	17.920026
37.176323	1388.680796	17.925043
37.168542	1398.140287	17.930061
37.596219	1395.977640	17.935079
37.558494	1392.881164	17.940096
37.570128	1393.642987	17.945114
37.744541	1388.117913	17.950131
37.449199	1390.789838	17.955149
37.648996	1397.322806	17.960167
37.930734	1383.584931	17.965184
37.672139	1385.206481	17.970202
37.753312	1387.933029	17.975219
37.372061	1392.316312	17.980237
37.455293	1406.527025	17.985255
38.078127	1414.742114	17.990272
37.935138	1424.071318	17.995290
38.405634	1417.269026	18.000307
38.034533	1412.889812	18.005325
37.856030	1422.297166	18.010343
38.301330	1416.092140	18.015360
38.010468	1421.341778	18.020378
37.756091	1412.604847	18.025395
38.198972	1416.366686	18.030413
38.167496	1418.082049	18.035431
38.092319	1413.811112	18.040448
38.021450	1420.156112	18.045466
38.244158	1416.558059	18.050483
38.639073	1428.207821	18.055501
38.591183	1443.303838	18.060519
39.022689	1434.986478	18.065536
38.388937	1421.862246	18.070554
38.489039	1413.659938	18.075571
38.818067	1419.033370	18.080589
38.543915	1424.198336	18.085607
38.824074	1427.083070	18.090624
38.630955	1436.016173	18.095642
38.744386	1423.380816	18.100659
38.812101	1428.877247	18.105677
38.886720	1425.693733	18.110695
38.846394	1425.232878	18.115712
38.597504	1421.118550	18.120730
38.983270	1417.090988	18.125747
38.870540	1420.608505	18.130765
38.987536	1427.555263	18.135783
38.851084	1421.457162	18.140800
38.876819	1425.858743	18.145818
38.834865	1420.320219	18.150835
39.107371	1422.271991	18.155853
39.380240	1440.379021	18.160871
39.362728	1440.236498	18.165888
39.562990	1446.059322	18.170906
39.416790	1449.200218	18.175923
39.495806	1427.178133	18.180941
39.182766	1441.305787	18.185959
39.321751	1444.023285	18.190976
39.385544	1448.601954	18.195994
39.758690	1446.308983	18.201011
39.625336	1442.776179	18.206029
39.352938	1447.637906	18.211047
39.924106	1449.142081	18.216064
39.998681	1455.022472	18.221082
39.814578	1447.631574	18.226099
39.848625	1445.880904	18.231117
39.740389	1450.881021	18.236135
40.042683	1446.042827	18.241152
40.067212	1453.284962	18.246170
40.243721	1448.914621	18.251187
40.294205	1446.132535	18.256205
39.801848	1441.702881	18.261223
39.807088	1443.071650	18.266240
39.622043	1447.821856	18.271258
39.692416	1445.011407	18.276275
39.724445	1438.748040	18.281293
39.839892	1444.306429	18.286311
39.712704	1448.315389	18.291328
40.119753	1468.828354	18.296346
39.908263	1472.187776	18.301363
40.180061	1474.275371	18.306381
40.209837	1473.159715	18.311399
40.446265	1470.550474	18.316416
40.448276	1465.128130	18.321434
40.380280	1474.060584	18.326451
40.537961	1466.956972	18.331469
40.311738	1475.844785	18.336487
40.452567	1469.962013	18.341504
40.526502	1482.466870	18.346522
40.690563	1486.752115	18.351539
41.033014	1488.153266	18.356557
40.935002	1486.167650	18.361575
40.829543	1490.741288	18.366592
40.824558	1499.310414	18.371610
40.481957	1491.133248	18.376627
40.648664	1490.980798	18.381645
41.008646	1491.299863	18.386663
41.147059	1494.951624	18.391680
41.137634	1496.799246	18.396698
40.820867	1490.593666	18.401715
41.211799	1483.295705	18.406733
40.973109	1488.694986	18.411751
40.939656	1489.659547	18.416768
41.202347	1500.133963	18.421786
41.305044	1510.036975	18.426803
41.724361	1509.226377	18.431821
41.474493	1512.831674	18.436839
41.731582	1510.790419	18.441856
41.656032	1514.100147	18.446874
41.560142	1499.749127	18.451891
41.599405	1489.703766	18.456909
41.847192	1494.938463	18.461927
41.624156	1503.863663	18.466944
41.684903	1498.293245	18.471962
41.698910	1511.833199	18.476979
41.738359	1508.468979	18.481997
41.569492	1510.565656	18.487015
42.002801	1505.066259	18.492032
42.276764	1500.693260	18.497050
41.815973	1509.201254	18.502067
42.060857	1501.222388	18.507085
42.060211	1503.037075	18.512103
42.235391	1496.198967	18.517120
42.141902	1501.408237	18.522138
42.024380	1498.478887	18.527155
41.966561	1498.595155	18.532173
41.830520	1501.289478	18.537191
42.090972	1500.428028	18.542208
41.983424	1496.143207	18.547226
41.965641	1503.167919	18.552243
42.531028	1504.281665	18.557261
42.273369	1521.970101	18.562279
42.525409	1524.045018	18.567296
42.631476	1525.713593	18.572314
42.274653	1518.406535	18.577331
42.771584	1524.148188	18.582349
42.688293	1524.347346	18.587367
42.872840	1521.430629	18.592384
42.720168	1532.165812	18.597402
42.537849	1532.528817	18.602419
42.459312	1527.065423	18.607437
42.289736	1521.389065	18.612455
42.402582	1527.023630	18.617472
42.882855	1519.067839	18.622490
42.904750	1528.800475	18.627507
43.207926	1530.756922	18.632525
42.893229	1540.065749	18.637543
43.165761	1547.960224	18.642560
43.185413	1548.073823	18.647578
43.230945	1540.877294	18.652595
43.403367	1545.543116	18.657613
43.137130	1558.158130	18.662631
43.341024	1550.100452	18.667648
43.478883	1546.528292	18.672666
43.401132	1549.538554	18.677683
43.623451	1552.287196	18.682701
43.474472	1539.181604	18.687719
43.190085	1547.065499	18.692736
43.633725	1545.701950	18.697754
43.429813	1547.788343	18.702771
43.594454	1537.455054	18.707789
43.550654	1543.300369	18.712807
43.894957	1545.711145	18.717824
43.673181	1534.157076	18.722842
43.432980	1551.334694	18.727859
43.700769	1544.352663	18.732877
43.641865	1568.224113	18.737895
43.928328	1567.920348	18.742912
43.747548	1571.612667	18.747930
43.808705	1569.497956	18.752947
44.150177	1563.466946	18.757965
44.040695	1572.450132	18.762983
43.751434	1567.641469	18.768000
44.123738	1563.417158	18.773018
44.019716	1574.943205	18.778035
44.172261	1569.995889	18.783053
44.188860	1591.602174	18.788071
44.425543	1604.734905	18.793088
44.524304	1592.168004	18.798106
44.166518	1604.731119	18.803123
44.488793	1586.016066	18.808141
44.245277	1594.007194	18.813159
44.759836	1595.065791	18.818176
44.649486	1594.243496	18.823194
44.610558	1591.626883	18.828211
44.558432	1589.545699	18.833229
44.730380	1597.298156	18.838247
44.874178	1589.757990	18.843264
44.795061	1583.316316	18.848282
45.010895	1598.825606	18.853299
45.095975	1609.987514	18.858317
44.840539	1598.432365	18.863335
44.953524	1606.143568	18.868352
45.289671	1609.483490	18.873370
45.367367	1620.239440	18.878387
45.589913	1608.221210	18.883405
45.399053	1599.158637	18.888423
45.490063	1587.347233	18.893440
45.532605	1585.920284	18.898458
45.030923	1585.793654	18.903475
45.214582	1583.801768	18.908493
45.278328	1590.614913	18.913511
44.936415	1598.785570	18.918528
45.395257	1605.921849	18.923546
45.388989	1606.370888	18.928563
45.656732	1606.966354	18.933581
45.466957	1607.702934	18.938599
45.583703	1607.892845	18.943616
45.850217	1597.909654	18.948634
45.463402	1603.130195	18.953651
45.377630	1608.502397	18.958669
45.267540	1618.060090	18.963687
45.466792	1635.317268	18.968704
46.047537	1631.382195	18.973722
45.732860	1636.367368	18.978739
45.977800	1623.158968	18.983757
46.268387	1624.445173	18.988775
46.091971	1635.218853	18.993792
46.244527	1632.177735	18.998810
46.142695	1641.244968	19.003827
46.412341	1632.908693	19.008845
46.454923	1651.916759	19.013863
46.440821	1656.280454	19.018880
46.739100	1652.654735	19.023898
46.369601	1652.305411	19.028915
46.830900	1644.062187	19.033933
46.629109	1644.892175	19.038951
46.777101	1642.858530	19.043968
46.652779	1639.845011	19.048986
46.805792	1648.711365	19.054003
47.019246	1639.493902	19.059021
47.216001	1635.249738	19.064039
46.907593	1626.196101	19.069056
46.930677	1618.163566	19.074074
47.031525	1628.780186	19.079091
47.301593	1629.432097	19.084109
47.176504	1628.807781	19.089127
47.177820	1623.278195	19.094144
46.984592	1614.032939	19.099162
46.708804	1620.523730	19.104179
47.077244	1626.389696	19.109197
47.335506	1636.978502	19.114215
47.343356	1637.614689	19.119232
47.315230	1643.097797	19.124250
47.136817	1640.127469	19.129267
47.356171	1634.923501	19.134285
47.679438	1636.037319	19.139303
47.303141	1643.294991	19.144320
47.465705	1637.121563	19.149338
47.317340	1647.142887	19.154355
47.211006	1662.222997	19.159373
47.725040	1663.493132	19.164391
47.268293	1669.655666	19.169408
47.605892	1666.039563	19.174426
47.702050	1670.647934	19.179443
47.365045	1666.642035	19.184461
47.576654	1676.073612	19.189479
47.944022	1694.345986	19.194496
48.304434	1697.038299	19.199514
48.144688	1686.010933	19.204531
48.142137	1689.284008	19.209549
48.238505	1684.926166	19.214567
48.482044	1691.408205	19.219584
48.481467	1673.851399	19.224602
48.397609	1690.780580	19.229619
48.455155	1684.137567	19.234637
48.629556	1681.859925	19.239655
48.698223	1686.314807	19.244672
48.847578	1683.053262	19.249690
48.859947	1686.835271	19.254707
48.554428	1679.905139	19.259725
48.418272	1681.750543	19.264743
48.755741	1683.313447	19.269760
48.540095	1686.203316	19.274778
48.386936	1687.432810	19.279795
48.245232	1684.131655	19.284813
48.883089	1682.037036	19.289831
48.984353	1706.997643	19.294848
49.201081	1700.638971	19.299866
49.343038	1713.884460	19.304883
48.760318	1707.193420	19.309901
49.356492	1706.187838	19.314919
48.870590	1709.744942	19.319936
49.301672	1704.245833	19.324954
49.440885	1702.248273	19.329971
49.265019	1704.222986	19.334989
49.462507	1706.211791	19.340007
49.357043	1715.487927	19.345024
49.731700	1701.877270	19.350042
49.537257	1702.324233	19.355059
49.143189	1706.435028	19.360077
49.729463	1701.508090	19.365095
49.357639	1708.361119	19.370112
49.726425	1710.553475	19.375130
49.638390	1710.617671	19.380147
49.726559	1722.015865	19.385165
49.943181	1727.413313	19.390183
49.904065	1730.512233	19.395200
50.052167	1732.537182	19.400218
49.567899	1731.754529	19.405235
49.626981	1727.595034	19.410253
49.926655	1733.585425	19.415271
50.044430	1735.782395	19.420288
50.249337	1737.896282	19.425306
50.005140	1742.958809	19.430323
50.271695	1754.278579	19.435341
50.699677	1741.521128	19.440359
50.773332	1757.586196	19.445376
50.929759	1751.085467	19.450394
50.877150	1758.942609	19.455411
50.826178	1738.095607	19.460429
50.988466	1720.724691	19.465447
50.393019	1724.945941	19.470464
50.280765	1725.146483	19.475482
50.625553	1745.846258	19.480499
50.566644	1752.839639	19.485517
51.179792	1749.527509	19.490535
50.811974	1754.773521	19.495552
50.968187	1746.562270	19.500570
50.723527	1743.788507	19.505587
50.834864	1741.978359	19.510605
50.909757	1739.324955	19.515623
51.155246	1750.250367	19.520640
51.402951	1760.591576	19.525658
51.341191	1772.433042	19.530675
51.306074	1766.464122	19.535693
51.760100	1767.450158	19.540711
51.887103	1770.428377	19.545728
51.587935	1761.044998	19.550746
51.655236	1762.890094	19.555763
51.806824	1765.425775	19.560781
51.611159	1754.634383	19.565799
51.866897	1752.116756	19.570816
51.729153	1756.064318	19.575834
51.600964	1763.983800	19.580851
51.327647	1767.655940	19.585869
51.642462	1759.612351	19.590887
51.525398	1769.218557	19.595904
51.403514	1766.665412	19.600922
51.732346	1772.903728	19.605939
51.745307	1783.622579	19.610957
52.108453	1780.434825	19.615975
51.601059	1786.996679	19.620992
51.867922	1786.806443	19.626010
51.798672	1782.209420	19.631027
52.076048	1798.394095	19.636045
52.286803	1801.210865	19.641063
52.534413	1804.264874	19.646080
52.602482	1798.163005	19.651098
52.709338	1803.394625	19.656115
52.597311	1802.070777	19.661133
52.704717	1806.630081	19.666151
52.819616	1806.034435	19.671168
52.608993	1806.562836	19.676186
52.860155	1805.503998	19.681203
53.187214	1806.532021	19.686221
53.157825	1804.068527	19.691239
52.894027	1807.505639	19.696256
52.999390	1810.379951	19.701274
53.200964	1806.128681	19.706291
53.032671	1804.917796	19.711309
53.004820	1800.661444	19.716327
53.272999	1811.734827	19.721344
53.208444	1811.852153	19.726362
53.176450	1809.682576	19.731379
53.326995	1822.642759	19.736397
53.638325	1821.148431	19.741415
53.868820	1827.446359	19.746432
53.655662	1827.912037	19.751450
53.867423	1832.139395	19.756467
53.649473	1832.574264	19.761485
54.206297	1817.543174	19.766503
53.744061	1825.890586	19.771520
53.536367	1822.697580	19.776538
54.028494	1831.697100	19.781555
53.718661	1827.393396	19.786573
53.774379	1832.102826	19.791591
53.743702	1825.590355	19.796608
53.737876	1830.284178	19.801626
53.764604	1829.071141	19.806643
54.056727	1836.498740	19.811661
54.224743	1839.309588	19.816679
54.462478	1849.081170	19.821696
54.356137	1855.403477	19.826714
54.466277	1850.008260	19.831731
54.715410	1850.237397	19.836749
54.303474	1839.621858	19.841767
54.467853	1843.724090	19.846784
54.538107	1851.420002	19.851802
54.501693	1848.045511	19.856819
54.533242	1848.517035	19.861837
54.950581	1848.729286	19.866855
54.570683	1844.354499	19.871872
54.547501	1846.358957	19.876890
54.875376	1860.721063	19.881907
54.834909	1880.411461	19.886925
55.173667	1872.367226	19.891943
55.145702	1874.107330	19.896960
55.049698	1877.707528	19.901978
55.266886	1862.107875	19.906995
54.959616	1874.262448	19.912013
55.352882	1866.414817	19.917031
55.148465	1869.271396	19.922048
55.329614	1870.824092	19.927066
55.671516	1877.865186	19.932083
55.644886	1881.637565	19.937101
55.619335	1874.701365	19.942119
55.917053	1885.050591	19.947136
55.642586	1882.890591	19.952154
56.295354	1887.143548	19.957171
55.789122	1886.228619	19.962189
55.856858	1874.382800	19.967207
55.927814	1882.599360	19.972224
55.813400	1890.106455	19.977242
55.979910	1889.947721	19.982259
55.902337	1894.513937	19.987277
56.254064	1892.808132	19.992295
56.200281	1900.873818	19.997312
56.118955	1897.560007	20.002330
56.393890	1888.717820	20.007347
56.430697	1896.627290	20.012365
56.082456	1894.330513	20.017383
56.027567	1887.938586	20.022400
55.885193	1891.735414	20.027418
56.494173	1904.702732	20.032435
56.491972	1919.672062	20.037453
56.293552	1922.287851	20.042471
56.406883	1913.291077	20.047488
56.529939	1913.057094	20.052506
56.775566	1920.943326	20.057523
56.984880	1933.705019	20.062541
57.095367	1930.610477	20.067559
57.333960	1940.811196	20.072576
57.168004	1940.477316	20.077594
57.173839	1926.766472	20.082611
56.949858	1939.040593	20.087629
57.315482	1931.557054	20.092647
57.461987	1929.949676	20.097664
57.510049	1929.026801	20.102682
57.268852	1925.722253	20.107699
57.430600	1935.303801	20.112717
57.620026	1925.222045	20.117735
57.669084	1925.299479	20.122752
57.825004	1930.081605	20.127770
58.035923	1927.668813	20.132787
57.788727	1932.725551	20.137805
57.867735	1927.404622	20.142823
57.541455	1927.130577	20.147840
57.552936	1943.375979	20.152858
58.060471	1958.341223	20.157875
57.805051	1957.831996	20.162893
58.094100	1958.168498	20.167911
58.389303	1955.389021	20.172928
58.229942	1946.778962	20.177946
58.288546	1948.284588	20.182963
58.487268	1962.143108	20.187981
58.184651	1954.294005	20.192999
58.527362	1953.744719	20.198016
58.508890	1964.923073	20.203034
58.567863	1962.483586	20.208051
58.389557	1968.040820	20.213069
58.613017	1971.963398	20.218087
58.701995	1974.701437	20.223104
58.819705	1980.673080	20.228122
59.118695	1970.962327	20.233139
59.015080	1983.798332	20.238157
58.931987	1972.045513	20.243175
59.075242	1970.527010	20.248192
59.093828	1977.691387	20.253210
59.318384	1974.080310	20.258227
59.292849	1973.951664	20.263245
59.423693	1970.541477	20.268263
59.253080	1967.336324	20.273280
58.935070	1969.538478	20.278298
59.372835	1971.877862	20.283315
59.353998	1983.999943	20.288333
59.358375	1988.805826	20.293351
59.447639	1996.530383	20.298368
59.636751	2001.398852	20.303386
59.733589	1989.699888	20.308403
59.186003	1997.738834	20.313421
59.824908	1993.624145	20.318439
60.012333	1996.312047	20.323456
59.598838	2001.615783	20.328474
60.177562	1997.535770	20.333491
60.053580	2014.982823	20.338509
60.100229	2020.309154	20.343527
60.193787	2022.863431	20.348544
60.257314	2024.996347	20.353562
60.497137	2017.144288	20.358579
60.358880	2020.394500	20.363597
60.482472	2017.597715	20.368615
60.462777	2017.969966	20.373632
60.372014	2010.655736	20.378650
60.809013	2001.497746	20.383667
60.914065	2006.499317	20.388685
60.861425	2004.582279	20.393703
60.468383	2007.234885	20.398720
60.301056	2017.972653	20.403738
60.762991	2022.205046	20.408755
60.703113	2027.497572	20.413773
60.891161	2032.574516	20.418791
61.053597	2035.872302	20.423808
60.588898	2022.181453	20.428826
61.137956	2037.045577	20.433843
61.239702	2048.874232	20.438861
61.504991	2051.644625	20.443879
61.562496	2053.639621	20.448896
61.718497	2053.990658	20.453914
62.094928	2048.850330	20.458931
61.767661	2057.375535	20.463949
61.768977	2055.266987	20.468967
61.417129	2057.171471	20.473984
61.309937	2062.622910	20.479002
62.086698	2055.100155	20.484019
61.806823	2045.571580	20.489037
61.909252	2053.256226	20.494055
61.986619	2049.936460	20.499072
62.071275	2058.756918	20.504090
62.265732	2056.577081	20.509107
62.678640	2075.088883	20.514125
62.146461	2069.181959	20.519143
62.064356	2070.198358	20.524160
62.049559	2073.599664	20.529178
62.081643	2076.851603	20.534195
62.238034	2071.079814	20.539213
62.226368	2076.554164	20.544231
62.710087	2073.562082	20.549248
62.552828	2096.433391	20.554266
63.025767	2101.112240	20.559283
62.711745	2107.293589	20.564301
62.894788	2100.157350	20.569319
63.287207	2096.387395	20.574336
62.979660	2103.940618	20.579354
62.924812	2104.087985	20.584371
63.029283	2094.865272	20.589389
62.729583	2094.845856	20.594407
63.022188	2097.062821	20.599424
63.235417	2119.109189	20.604442
63.689296	2122.796867	20.609459
63.695436	2123.862565	20.614477
63.639105	2125.051669	20.619495
63.763507	2130.470000	20.624512
63.416855	2126.250895	20.629530
63.776626	2118.957560	20.634547
63.869254	2121.666645	20.639565
63.684641	2127.430061	20.644583
64.161729	2127.235290	20.649600
63.717842	2124.483213	20.654618
63.987665	2123.964279	20.659635
64.051428	2119.002318	20.664653
63.630314	2117.726872	20.669671
64.070781	2114.470137	20.674688
63.971121	2118.320285	20.679706
63.979742	2140.073660	20.684723
64.069956	2145.260646	20.689741
64.273033	2144.651174	20.694759
64.346809	2145.526380	20.699776
64.035753	2139.360707	20.704794
64.154230	2152.995241	20.709811
64.622319	2163.961776	20.714829
64.587668	2170.307678	20.719847
65.141821	2171.584191	20.724864
64.722958	2176.702610	20.729882
64.666202	2176.604102	20.734899
64.860618	2169.806910	20.739917
65.079878	2187.702171	20.744935
65.551261	2192.299230	20.749952
65.801080	2198.023009	20.754970
65.528761	2182.774351	20.759987
65.541307	2171.883808	20.765005
65.183687	2176.983163	20.770023
65.950638	2185.479016	20.775040
65.993872	2192.080991	20.780058
65.671310	2179.639654	20.785075
65.788851	2176.982661	20.790093
65.258837	2188.528502	20.795111
65.576838	2178.862000	20.800128
65.357415	2186.275208	20.805146
65.723211	2186.388233	20.810163
66.048863	2189.420613	20.815181
65.863426	2195.758587	20.820199
66.448609	2202.310373	20.825216
66.408178	2205.681004	20.830234
66.274666	2203.921795	20.835251
66.363979	2211.554910	20.840269
66.234031	2214.636583	20.845287
66.741512	2213.300858	20.850304
66.132620	2206.907244	20.855322
66.854970	2212.493874	20.860339
66.753688	2197.997959	20.865357
66.388009	2204.676628	20.870375
66.555251	2210.126145	20.875392
66.978423	2222.024487	20.880410
67.177792	2236.104043	20.885427
67.132927	2234.450875	20.890445
67.255378	2241.210885	20.895463
67.409862	2233.492034	20.900480
67.239576	2240.304220	20.905498
67.176464	2227.695957	20.910515
67.382802	2233.183541	20.915533
66.939419	2233.896757	20.920551
67.371282	2232.689654	20.925568
67.383661	2228.972901	20.930586
67.033911	2225.590621	20.935603
67.507968	2239.810198	20.940621
67.527498	2257.058260	20.945639
67.876803	2243.141870	20.950656
67.774184	2253.547719	20.955674
67.490947	2244.739155	20.960691
67.459936	2252.567880	20.965709
67.838030	2257.589865	20.970727
68.339020	2262.617845	20.975744
68.188094	2270.462209	20.980762
68.048597	2271.266684	20.985779
68.409023	2274.224197	20.990797
68.545649	2284.267502	20.995815
68.565335	2277.052635	21.000832
68.458064	2279.449048	21.005850
68.607791	2272.696692	21.010867
68.568866	2277.329540	21.015885
68.416627	2271.129471	21.020903
68.685614	2264.816067	21.025920
69.182373	2284.081879	21.030938
68.820482	2291.511139	21.035955
69.048664	2282.594026	21.040973
69.186976	2291.406192	21.045991
69.020566	2288.967255	21.051008
68.896849	2292.193145	21.056026
69.227811	2290.386406	21.061043
69.312573	2285.537885	21.066061
69.166217	2300.271317	21.071079
69.426082	2285.699813	21.076096
69.091908	2298.180808	21.081114
69.111575	2301.690378	21.086131
69.647718	2312.296014	21.091149
69.678414	2320.250813	21.096167
70.119295	2308.074822	21.101184
69.604142	2313.385107	21.106202
69.806257	2310.651721	21.111219
69.820711	2322.235432	21.116237
69.935377	2330.675745	21.121255
70.261294	2329.131750	21.126272
70.191702	2326.914347	21.131290
70.409239	2329.887944	21.136307
70.246849	2330.093191	21.141325
70.114542	2333.613953	21.146343
70.614362	2330.521467	21.151360
70.881659	2347.257381	21.156378
70.424689	2354.395420	21.161395
70.870931	2352.873601	21.166413
70.450804	2356.218532	21.171431
70.814769	2353.816423	21.176448
71.049081	2352.308871	21.181466
70.852340	2356.025943	21.186483
71.253224	2344.976613	21.191501
71.126957	2347.530661	21.196519
71.181645	2351.318803	21.201536
71.369386	2364.939490	21.206554
71.079820	2374.762413	21.211571
71.370832	2372.497976	21.216589
71.343955	2379.751695	21.221607
71.306302	2375.001232	21.226624
71.717939	2374.936647	21.231642
71.463078	2379.470795	21.236659
71.995492	2388.571593	21.241677
71.808298	2400.764517	21.246695
72.031147	2397.819566	21.251712
71.999555	2394.412656	21.256730
72.121227	2393.759120	21.261747
72.418221	2400.053143	21.266765
72.391256	2395.086384	21.271783
72.336881	2390.007144	21.276800
72.177879	2388.990443	21.281818
72.209924	2396.171816	21.286835
72.256590	2393.775228	21.291853
72.163058	2402.674270	21.296871
72.552396	2411.731217	21.301888
72.914914	2414.795734	21.306906
72.801687	2423.754683	21.311923
73.043066	2413.677139	21.316941
72.897734	2421.227173	21.321959
72.758995	2413.882422	21.326976
73.290064	2407.941360	21.331994
73.165750	2412.997916	21.337011
73.281515	2407.702648	21.342029
73.367640	2410.816779	21.347047
73.264749	2405.088663	21.352064
73.144743	2413.714119	21.357082
73.516876	2433.245796	21.362099
73.565115	2439.032796	21.367117
73.841692	2443.843497	21.372135
73.818759	2436.796205	21.377152
73.794554	2436.995585	21.382170
73.873704	2442.518941	21.387187
73.783643	2435.283331	21.392205
73.780267	2440.207327	21.397223
73.855181	2437.957802	21.402240
73.868913	2443.077954	21.407258
74.004242	2455.510748	21.412275
74.171670	2466.587697	21.417293
74.262950	2460.889108	21.422311
74.360565	2460.261432	21.427328
74.415974	2463.677062	21.432346
74.695032	2475.711772	21.437363
75.139936	2481.588134	21.442381
74.874010	2492.426848	21.447399
75.369581	2487.384509	21.452416
75.125066	2480.835868	21.457434
75.280916	2479.375316	21.462451
75.221710	2479.040480	21.467469
75.092765	2476.043324	21.472487
75.398288	2485.807790	21.477504
75.572437	2476.605526	21.482522
75.183606	2487.659174	21.487539
75.615994	2477.103498	21.492557
75.218224	2479.744287	21.497575
75.337620	2478.090610	21.502592
75.590938	2476.630568	21.507610
75.449247	2484.804973	21.512627
75.762777	2487.318541	21.517645
76.084856	2504.585719	21.522663
76.101941	2505.564509	21.527680
76.168737	2506.728035	21.532698
75.848484	2506.948548	21.537715
76.154517	2497.952853	21.542733
76.274976	2502.724906	21.547751
76.127834	2502.776272	21.552768
76.264826	2507.185936	21.557786
76.150796	2524.587738	21.562803
76.414022	2517.845914	21.567821
76.555370	2522.734634	21.572839
76.673891	2529.886730	21.577856
76.892023	2518.859615	21.582874
76.600274	2533.887445	21.587891
76.710391	2538.610630	21.592909
77.324053	2538.075689	21.597927
77.018652	2541.503676	21.602944
77.327723	2541.398350	21.607962
76.951170	2543.707585	21.612979
77.270459	2544.755807	21.617997
76.956630	2549.223489	21.623015
77.186965	2541.792456	21.628032
77.452714	2552.453223	21.633050
77.325192	2565.416478	21.638067
77.491017	2570.512838	21.643085
77.777127	2568.239677	21.648103
78.052639	2571.986957	21.653120
77.971069	2572.346820	21.658138
77.621992	2575.488135	21.663155
77.774453	2573.542059	21.668173
77.924684	2583.750676	21.673191
77.846240	2578.713028	21.678208
78.377346	2581.918437	21.683226
77.902258	2599.178041	21.688243
78.261590	2589.612154	21.693261
78.852089	2612.755173	21.698279
78.730043	2613.695799	21.703296
78.886236	2613.478710	21.708314
78.647111	2617.944172	21.713331
79.114392	2614.140289	21.718349
79.242258	2610.941911	21.723367
79.073704	2617.261607	21.728384
79.067888	2612.102105	21.733402
78.994610	2613.189743	21.738419
79.231630	2613.341885	21.743437
79.588532	2603.082016	21.748455
79.470361	2616.151152	21.753472
79.221323	2603.890527	21.758490
79.417072	2623.740412	21.763507
79.652631	2625.960068	21.768525
79.620714	2632.390921	21.773543
79.777220	2638.817505	21.778560
80.029396	2633.879538	21.783578
79.807318	2637.379705	21.788595
80.002340	2636.241245	21.793613
80.011914	2647.541875	21.798631
80.100847	2663.428615	21.803648
80.588661	2658.324321	21.808666
80.531022	2662.761361	21.813683
80.358071	2660.345491	21.818701
80.500929	2660.294610	21.823719
80.752381	2662.151978	21.828736
80.593130	2649.009310	21.833754
80.416332	2653.859537	21.838771
81.050270	2659.819964	21.843789
81.077169	2666.396266	21.848807
81.049850	2673.034720	21.853824
81.218703	2672.083415	21.858842
81.384581	2676.226634	21.863859
81.155490	2680.068774	21.868877
81.444616	2682.674567	21.873895
81.494114	2680.391120	21.878912
81.750957	2683.652142	21.883930
81.284817	2678.940325	21.888947
81.200799	2681.200588	21.893965
81.675980	2691.961186	21.898983
81.909228	2704.366187	21.904000
81.854050	2693.833117	21.909018
81.748141	2703.109831	21.914035
81.907868	2698.394639	21.919053
82.285375	2695.671591	21.924071
81.797083	2708.969214	21.929088
81.946267	2714.652115	21.934106
82.498751	2727.493168	21.939123
82.332079	2725.126804	21.944141
82.571599	2725.628892	21.949159
82.429287	2730.546329	21.954176
82.721387	2727.208577	21.959194
83.024253	2744.450590	21.964211
82.768807	2752.261040	21.969229
82.921138	2759.133342	21.974247
82.880170	2747.540694	21.979264
83.175535	2750.928252	21.984282
83.094278	2762.413619	21.989299
83.140337	2743.068375	21.994317
83.423014	2744.684146	21.999335
83.234670	2746.329526	22.004352
83.574388	2747.582869	22.009370
83.859799	2764.038589	22.014387
83.985901	2768.222779	22.019405
84.054717	2769.840497	22.024423
83.912341	2766.545559	22.029440
84.021796	2764.050711	22.034458
84.019821	2764.890473	22.039475
84.087219	2765.709898	22.044493
84.214744	2756.574763	22.049511
83.680103	2761.026593	22.054528
83.985812	2772.583899	22.059546
84.166856	2779.319151	22.064563
84.394239	2784.008248	22.069581
84.413498	2786.413310	22.074599
84.082117	2785.133223	22.079616
84.487133	2808.627486	22.084634
84.605321	2817.310503	22.089651
84.626509	2813.292411	22.094669
85.112916	2813.377078	22.099687
84.824713	2809.745173	22.104704
84.857345	2822.383682	22.109722
85.334451	2826.749608	22.114739
85.258681	2844.786432	22.119757
85.495946	2833.348978	22.124775
85.311854	2835.463974	22.129792
85.440366	2839.531023	22.134810
85.792124	2853.050635	22.139827
85.882878	2853.118385	22.144845
86.452239	2858.306258	22.149863
86.141514	2859.955041	22.154880
86.338348	2854.138792	22.159898
86.526000	2850.012551	22.164915
86.389918	2857.854844	22.169933
86.412474	2846.611987	22.174951
86.306402	2857.492155	22.179968
86.557241	2857.383326	22.184986
86.961664	2855.142093	22.190003
86.762422	2855.062748	22.195021
86.626991	2853.051280	22.200039
86.762411	2851.215155	22.205056
86.683899	2853.146333	22.210074
87.197916	2871.766209	22.215091
86.877280	2877.203991	22.220109
86.917565	2877.102901	22.225127
87.006517	2875.002620	22.230144
87.186200	2869.930762	22.235162
87.409347	2886.519441	22.240179
87.310919	2901.776098	22.245197
87.710266	2894.510971	22.250215
87.708727	2900.463728	22.255232
87.707489	2896.837345	22.260250
87.710978	2887.390176	22.265267
87.729643	2901.883623	22.270285
87.782045	2911.110391	22.275303
87.950256	2922.354778	22.280320
87.756988	2922.081968	22.285338
88.195265	2928.663352	22.290355
88.155407	2936.651571	22.295373
88.411117	2939.846537	22.300391
88.496833	2950.207500	22.305408
88.507440	2938.707647	22.310426
88.805583	2950.878559	22.315443
88.725600	2949.549605	22.320461
88.847873	2943.656635	22.325479
88.751478	2946.509083	22.330496
89.452784	2959.087114	22.335514
89.248874	2967.697574	22.340531
89.443698	2966.335033	22.345549
89.869413	2973.038338	22.350567
89.748072	2974.051465	22.355584
89.555506	2965.316715	22.360602
89.824472	2965.517512	22.365619
89.729801	2964.279232	22.370637
89.914470	2965.272822	22.375655
90.061546	2967.275980	22.380672
89.648962	2967.634055	22.385690
90.076614	2955.500733	22.390707
89.916694	2966.335748	22.395725
90.264561	2964.996573	22.400743
89.989992	2985.810596	22.405760
90.093220	2991.074694	22.410778
90.202669	2987.102704	22.415795
90.565926	2988.330282	22.420813
90.626327	2989.681059	22.425831
90.676414	3001.827745	22.430848
90.637087	3012.814330	22.435866
90.903822	3007.220642	22.440883
90.539971	3015.493217	22.445901
90.882586	3005.421577	22.450919
90.827462	3022.136041	22.455936
90.843017	3030.453336	22.460954
91.301085	3033.165274	22.465971
91.346166	3043.141284	22.470989
91.730794	3043.955208	22.476007
91.963018	3060.571033	22.481024
92.351996	3052.688844	22.486042
91.951755	3047.591012	22.491059
91.711429	3049.080439	22.496077
92.157615	3049.266097	22.501095
92.206898	3043.141500	22.506112
92.281983	3044.625699	22.511130
92.435570	3045.583132	22.516147
92.710861	3057.296887	22.521165
92.715472	3068.263997	22.526183
92.669653	3069.789234	22.531200
92.733154	3069.858098	22.536218
92.951012	3073.096893	22.541235
92.533657	3068.876015	22.546253
92.827451	3067.740991	22.551271
93.183397	3073.552580	22.556288
93.086520	3087.840185	22.561306
93.455052	3100.760826	22.566323
93.214891	3103.411729	22.571341
93.565954	3103.388198	22.576359
93.457945	3098.039411	22.581376
93.481531	3101.838897	22.586394
93.504733	3092.940875	22.591411
93.662716	3109.902938	22.596429
93.713612	3124.495670	22.601447
93.932994	3128.535923	22.606464
93.729463	3130.392030	22.611482
93.909143	3130.682567	22.616499
94.077670	3144.941262	22.621517
94.626094	3142.033558	22.626535
94.358972	3157.133797	22.631552
94.333264	3144.086626	22.636570
94.766710	3144.757188	22.641587
94.669648	3151.501432	22.646605
94.772801	3153.287399	22.651623
94.959529	3163.424346	22.656640
94.945322	3164.786825	22.661658
95.317801	3160.413775	22.666675
95.533121	3164.887080	22.671693
95.721705	3172.596582	22.676711
95.473289	3165.031987	22.681728
95.524918	3170.035940	22.686746
95.640297	3161.906193	22.691763
95.202359	3174.255704	22.696781
95.645826	3170.919407	22.701799
95.931672	3178.206516	22.706816
95.747737	3192.814001	22.711834
95.979862	3190.186252	22.716851
96.146189	3195.380555	22.721869
96.136286	3195.830202	22.726887
96.332554	3200.357001	22.731904
96.229075	3207.323210	22.736922
96.598385	3221.266445	22.741939
96.454458	3223.192129	22.746957
96.665120	3214.110020	22.751975
96.861793	3207.996994	22.756992
96.330241	3216.886155	22.762010
96.946025	3218.648628	22.767027
97.393337	3235.420291	22.772045
97.157408	3239.645529	22.777063
97.361419	3240.661355	22.782080
97.350414	3237.326810	22.787098
97.377804	3241.002635	22.792115
97.339933	3251.427322	22.797133
97.155968	3260.533487	22.802151
97.589797	3262.371814	22.807168
97.981261	3259.375058	22.812186
98.199687	3261.490165	22.817203
98.808719	3273.988187	22.822221
98.625203	3263.168733	22.827239
98.580540	3258.744231	22.832256
98.203379	3264.535018	22.837274
98.858744	3265.173973	22.842291
99.002338	3278.429829	22.847309
99.082703	3277.697514	22.852327
99.368713	3282.102961	22.857344
99.234623	3285.942970	22.862362
99.352676	3276.316678	22.867379
98.699061	3280.702052	22.872397
98.682046	3271.646116	22.877415
98.889791	3283.582071	22.882432
98.988321	3291.624517	22.887450
99.030575	3289.086469	22.892467
98.936571	3301.255931	22.897485
99.351453	3308.077842	22.902503
99.536583	3323.984811	22.907520
99.357503	3334.220198	22.912538
99.957132	3331.970419	22.917555
100.160635	3339.137929	22.922573
100.460457	3344.140922	22.927591
100.581714	3347.562184	22.932608
100.537991	3358.571762	22.937626
100.568842	3348.271023	22.942643
100.511786	3361.151214	22.947661
100.672204	3357.436286	22.952679
101.109118	3352.052552	22.957696
100.559413	3357.037141	22.962714
100.899385	3354.209407	22.967731
101.189061	3372.025376	22.972749
101.243666	3372.790020	22.977767
101.429473	3364.475553	22.982784
101.348905	3373.284665	22.987802
101.545335	3368.307889	22.992819
101.529879	3371.952578	22.997837
101.576569	3365.032893	23.002855
101.758855	3368.248908	23.007872
101.651219	3389.081429	23.012890
101.840939	3391.753401	23.017907
101.703710	3402.935470	23.022925
101.259408	3393.996917	23.027943
101.934882	3401.895365	23.032960
101.694854	3419.866964	23.037978
102.271560	3415.376637	23.042995
102.319954	3424.503295	23.048013
102.340033	3445.154900	23.053031
102.796597	3440.882237	23.058048
102.411999	3443.360127	23.063066
102.806552	3444.466053	23.068083
103.209896	3454.070530	23.073101
103.515234	3465.795625	23.078119
103.846240	3469.367116	23.083136
103.609884	3478.920326	23.088154
104.067787	3471.762578	23.093171
104.027147	3471.260687	23.098189
103.775876	3464.040451	23.103207
104.020907	3467.044650	23.108224
103.851590	3465.653901	23.113242
103.739458	3459.134663	23.118259
104.166002	3457.404371	23.123277
103.721323	3460.750191	23.128295
103.991408	3466.234479	23.133312
104.234371	3485.774911	23.138330
104.327106	3487.884487	23.143347
104.568526	3486.994367	23.148365
104.413668	3507.351506	23.153383
104.826397	3509.309950	23.158400
104.726579	3523.481576	23.163418
104.804153	3517.005191	23.168435
104.906335	3528.654841	23.173453
104.920921	3538.913658	23.178471
105.283039	3539.911044	23.183488
105.391344	3549.574422	23.188506
105.786933	3554.392027	23.193523
105.621673	3567.330349	23.198541
105.540701	3564.120334	23.203559
105.704217	3566.190423	23.208576
105.888484	3574.431036	23.213594
105.819293	3571.171828	23.218611
106.402752	3579.283620	23.223629
106.385956	3595.869512	23.228647
106.275770	3588.661842	23.233664
106.521171	3590.504475	23.238682
106.862429	3597.098149	23.243699
106.906208	3601.134457	23.248717
106.938673	3611.766119	23.253735
107.282287	3614.290917	23.258752
107.533193	3616.883897	23.263770
107.280006	3610.705493	23.268787
107.141566	3608.697567	23.273805
107.354314	3618.556093	23.278823
107.475112	3612.000307	23.283840
107.523913	3609.413844	23.288858
107.550947	3629.196579	23.293875
107.589064	3636.645782	23.298893
107.444475	3645.865912	23.303911
107.809885	3630.241512	23.308928
108.026263	3647.592630	23.313946
108.178629	3657.643705	23.318963
108.159584	3663.119692	23.323981
108.457778	3659.218988	23.328999
108.742800	3654.512325	23.334016
108.399315	3658.113773	23.339034
108.588230	3671.388067	23.344051
109.187577	3673.181569	23.349069
108.896205	3688.213453	23.354087
108.947732	3683.808497	23.359104
109.339978	3686.777044	23.364122
109.118797	3689.267241	23.369139
109.448143	3693.186234	23.374157
109.354344	3708.357624	23.379175
109.840546	3706.627431	23.384192
109.608474	3712.086307	23.389210
109.439029	3714.363239	23.394227
109.826322	3711.846828	23.399245
109.896749	3729.287174	23.404263
109.968355	3728.338425	23.409280
110.110787	3733.034767	23.414298
110.383849	3720.612676	23.419315
110.373508	3729.631904	23.424333
110.355316	3743.235395	23.429351
110.873817	3746.607124	23.434368
110.906224	3753.293431	23.439386
110.764018	3756.888615	23.444403
111.137440	3753.257021	23.449421
111.124776	3750.462379	23.454439
111.235211	3767.416727	23.459456
111.104353	3767.553921	23.464474
111.372437	3766.160906	23.469491
111.635326	3775.156288	23.474509
111.211439	3785.199867	23.479527
111.997455	3796.777274	23.484544
111.707821	3806.828240	23.489562
112.139922	3798.935817	23.494579
112.643581	3796.726270	23.499597
112.155930	3805.807690	23.504615
112.378802	3812.318987	23.509632
112.635279	3829.010628	23.514650
112.693079	3823.392609	23.519667
112.880164	3826.440667	23.524685
113.044590	3836.537298	23.529703
113.087847	3826.868774	23.534720
112.997316	3827.589891	23.539738
113.051920	3846.535261	23.544755
113.516790	3853.283264	23.549773
113.337384	3850.675705	23.554791
113.720143	3848.049514	23.559808
113.420717	3849.885995	23.564826
113.593285	3852.466033	23.569843
113.649963	3874.106651	23.574861
113.542297	3883.014948	23.579879
113.604545	3878.762928	23.584896
113.945578	3891.177111	23.589914
113.817879	3905.732169	23.594931
114.110134	3908.381842	23.599949
114.047174	3926.433519	23.604967
114.609664	3925.439418	23.609984
114.630566	3929.697175	23.615002
114.990655	3933.077975	23.620019
114.994278	3938.970295	23.625037
115.331168	3954.330082	23.630055
115.240495	3953.195268	23.635072
115.660612	3947.908683	23.640090
115.725107	3948.785432	23.645107
115.812886	3947.777324	23.650125
115.612331	3952.401202	23.655143
115.822258	3960.009848	23.660160
116.071970	3961.381542	23.665178
115.716813	3968.845149	23.670195
115.909689	3965.876235	23.675213
116.078018	3976.082806	23.680231
116.480468	3975.561985	23.685248
116.767923	3984.184324	23.690266
116.486677	3994.975833	23.695283
116.533550	3999.242162	23.700301
116.874589	3999.684195	23.705319
117.076630	3999.336808	23.710336
117.037870	3995.283657	23.715354
116.682118	4000.301160	23.720371
117.565100	4010.619892	23.725389
117.224563	4027.963934	23.730407
117.530397	4028.051652	23.735424
117.335375	4026.952119	23.740442
117.525968	4025.343964	23.745459
118.050644	4033.080089	23.750477
117.970604	4046.166377	23.755495
118.134349	4051.007814	23.760512
118.099113	4051.663462	23.765530
118.121393	4058.938561	23.770547
118.385894	4074.136189	23.775565
118.548786	4066.146946	23.780583
118.801518	4075.166164	23.785600
118.889498	4074.827177	23.790618
119.001551	4080.219624	23.795635
119.249745	4086.345126	23.800653
119.258051	4103.180063	23.805671
119.065998	4100.198835	23.810688
119.047193	4099.422053	23.815706
119.111696	4107.340779	23.820723
119.596541	4115.430386	23.825741
119.486709	4125.671150	23.830759
119.562529	4123.784264	23.835776
119.989808	4133.268567	23.840794
120.176658	4145.994316	23.845811
120.321528	4147.325633	23.850829
120.431511	4148.735015	23.855847
120.545719	4149.603985	23.860864
120.501491	4152.423198	23.865882
120.520656	4163.148802	23.870899
121.079597	4169.932690	23.875917
120.931531	4171.761272	23.880935
121.164674	4170.793506	23.885952
121.335453	4179.743549	23.890970
121.428645	4191.218273	23.895987
121.723901	4191.310806	23.901005
121.520938	4204.586914	23.906023
121.397694	4202.952156	23.911040
121.838009	4204.331885	23.916058
121.479543	4215.400762	23.921075
121.982940	4220.820320	23.926093
122.037626	4227.635883	23.931111
122.255079	4237.525574	23.936128
122.655851	4245.091816	23.941146
122.460577	4255.816350	23.946163
122.746557	4247.097543	23.951181
122.775540	4252.297886	23.956199
122.987332	4253.628197	23.961216
123.297328	4269.784734	23.966234
123.236707	4282.511471	23.971251
123.512718	4270.644078	23.976269
123.555562	4271.211747	23.981287
123.411100	4272.244349	23.986304
123.599606	4268.622686	23.991322
123.384461	4281.884976	23.996339
123.641374	4292.819613	24.001357
123.724570	4295.637824	24.006375
123.911298	4313.960100	24.011392
124.397184	4315.503147	24.016410
124.494853	4330.212625	24.021427
124.430292	4326.873644	24.026445
124.753835	4331.977359	24.031463
124.414546	4327.343081	24.036480
124.929661	4341.412693	24.041498
124.477977	4353.967168	24.046515
124.611449	4338.122825	24.051533
124.663353	4348.792907	24.056551
125.175989	4361.622434	24.061568
125.478334	4371.707225	24.066586
125.410673	4378.630393	24.071603
125.582179	4389.556374	24.076621
125.705592	4392.974341	24.081639
126.076802	4406.015444	24.086656
126.179280	4396.570918	24.091674
126.070624	4405.735300	24.096691
126.445741	4411.175013	24.101709
126.247586	4422.736561	24.106727
126.400992	4418.763686	24.111744
126.870381	4416.325857	24.116762
126.516107	4439.088950	24.121779
126.767795	4443.591597	24.126797
126.702352	4449.712699	24.131815
127.068649	4455.264284	24.136832
127.462680	4458.800847	24.141850
127.136588	4468.599057	24.146867
127.540802	4462.674051	24.151885
127.861572	4481.884563	24.156903
127.785570	4492.659993	24.161920
128.023328	4491.031782	24.166938
127.812355	4498.078455	24.171955
128.180691	4508.108794	24.176973
128.448680	4521.491269	24.181991
128.499212	4527.426934	24.187008
129.040900	4518.304941	24.192026
129.104921	4523.133720	24.197043
129.068792	4513.171088	24.202061
129.187604	4529.645050	24.207079
129.182031	4535.968286	24.212096
129.350804	4534.407696	24.217114
129.208571	4547.008519	24.222131
129.453160	4543.052896	24.227149
129.210185	4554.447942	24.232167
129.446864	4571.872521	24.237184
129.793575	4567.430575	24.242202
129.969549	4591.237657	24.247219
130.027896	4580.474218	24.252237
130.230102	4583.460062	24.257255
130.127150	4592.544732	24.262272
130.607216	4606.187600	24.267290
130.444354	4606.806445	24.272307
130.771705	4608.588997	24.277325
130.947018	4633.933457	24.282343
130.634440	4640.424774	24.287360
131.147695	4639.435197	24.292378
131.305609	4652.967588	24.297395
131.370189	4653.257246	24.302413
131.470173	4665.056326	24.307431
131.524547	4670.363289	24.312448
131.838424	4671.945942	24.317466
132.079678	4690.061195	24.322483
132.053650	4687.476833	24.327501
132.351359	4696.167349	24.332519
132.611836	4707.268974	24.337536
132.894541	4706.628008	24.342554
133.132559	4714.112623	24.347571
132.544997	4710.382030	24.352589
133.117253	4718.189909	24.357607
133.001506	4725.919344	24.362624
133.717791	4709.942336	24.367642
133.305974	4721.404973	24.372659
133.606249	4730.953679	24.377677
133.812050	4731.034980	24.382695
133.976413	4742.792459	24.387712
134.449443	4735.676042	24.392730
134.275366	4740.116048	24.397747
134.399099	4744.616721	24.402765
134.256415	4738.654202	24.407783
134.324364	4742.043046	24.412800
134.455013	4750.030602	24.417818
134.346807	4763.844664	24.422835
134.725133	4766.963931	24.427853
134.900495	4767.842290	24.432871
134.984577	4783.226605	24.437888
135.260327	4796.930035	24.442906
135.201928	4796.655002	24.447923
135.337393	4799.714469	24.452941
135.830636	4806.701440	24.457959
135.738907	4819.632288	24.462976
135.526529	4813.222963	24.467994
135.955663	4821.422626	24.473011
135.767062	4841.224680	24.478029
136.127903	4842.755798	24.483047
135.970884	4857.549795	24.488064
136.446041	4861.799736	24.493082
136.586920	4871.351392	24.498099
136.796043	4868.215646	24.503117
136.641184	4880.613501	24.508135
136.961881	4894.657184	24.513152
137.216818	4894.828640	24.518170
137.322256	4902.141554	24.523187
137.525243	4920.900657	24.528205
137.918166	4924.772082	24.533223
138.040868	4929.629654	24.538240
137.739223	4934.544238	24.543258
138.185931	4937.753830	24.548275
138.262977	4945.831942	24.553293
138.324659	4946.576604	24.558311
138.256315	4954.001992	24.563328
138.611033	4953.678019	24.568346
138.844997	4963.941151	24.573363
138.746454	4963.555612	24.578381
139.319686	4972.442996	24.583399
139.083069	4980.718621	24.588416
139.562272	4980.952798	24.593434
139.301340	4994.027071	24.598451
139.416798	4995.413565	24.603469
139.775090	4998.207726	24.608487
139.672907	5022.207308	24.613504
140.064292	5029.806916	24.618522
140.276462	5025.288084	24.623539
139.955373	5032.734160	24.628557
140.098829	5042.699015	24.633575
140.359028	5050.316027	24.638592
140.177666	5057.768632	24.643610
140.498792	5075.243595	24.648627
140.981881	5082.039711	24.653645
141.346026	5089.384772	24.658663
140.855190	5099.556353	24.663680
141.185228	5108.617637	24.668698
141.677332	5111.712825	24.673715
141.549709	5116.458148	24.678733
142.109313	5129.312427	24.683751
141.854881	5127.881220	24.688768
141.999479	5124.446193	24.693786
142.401598	5137.312524	24.698803
142.745186	5147.290275	24.703821
142.647434	5149.382539	24.708839
142.408883	5160.448983	24.713856
142.485113	5151.345936	24.718874
142.629865	5160.218468	24.723891
142.859398	5178.285538	24.728909
143.259277	5178.317496	24.733927
143.097410	5182.054930	24.738944
143.096146	5183.396593	24.743962
143.119790	5201.205533	24.748979
143.460781	5204.406483	24.753997
143.724414	5214.785060	24.759015
144.129843	5228.310669	24.764032
144.363400	5234.912346	24.769050
144.382875	5253.148133	24.774067
144.600435	5261.166491	24.779085
144.659767	5260.415297	24.784103
144.699938	5263.347724	24.789120
145.038040	5271.902767	24.794138
145.421345	5273.446188	24.799155
145.190404	5280.193254	24.804173
145.355643	5287.010834	24.809191
145.222590	5294.272883	24.814208
145.718194	5305.142326	24.819226
145.991808	5307.754091	24.824243
146.138063	5304.647061	24.829261
146.550993	5312.161340	24.834279
146.153751	5329.913235	24.839296
146.448856	5334.447182	24.844314
146.674423	5340.996487	24.849331
146.563032	5338.075019	24.854349
147.061954	5339.537200	24.859367
146.778663	5352.403737	24.864384
147.095630	5354.914018	24.869402
147.114500	5366.022331	24.874419
147.361550	5382.208659	24.879437
147.915439	5375.521257	24.884455
148.020539	5371.760925	24.889472
147.880432	5384.788138	24.894490
148.266247	5402.490029	24.899507
148.377387	5411.882483	24.904525
148.299177	5403.109700	24.909543
148.248367	5409.244614	24.914560
148.563458	5424.918414	24.919578
148.602708	5430.335294	24.924595
148.440603	5445.660881	24.929613
148.931372	5446.972829	24.934631
149.403708	5455.645822	24.939648
149.260916	5464.203691	24.944666
149.552296	5472.349470	24.949683
149.543460	5485.413009	24.954701
150.133040	5482.413269	24.959719
150.127530	5493.313981	24.964736
150.467905	5517.873057	24.969754
150.469253	5513.134600	24.974771
150.297867	5516.226478	24.979789
150.790520	5516.559570	24.984807
150.933554	5506.858740	24.989824
150.709334	5524.738394	24.994842
150.694641	5538.396341	24.999859
150.893026	5541.799623	25.004877
151.248741	5548.297047	25.009895
151.472554	5565.850860	25.014912
151.413685	5571.636700	25.019930
151.449897	5571.583584	25.024947
151.864611	5590.736357	25.029965
152.070334	5585.025175	25.034983
151.941357	5602.728993	25.040000
152.211395	5606.736614	25.045018
152.644201	5615.583180	25.050035
152.624071	5609.323387	25.055053
152.801600	5610.394007	25.060071
152.764675	5634.942901	25.065088
153.004535	5643.500884	25.070106
153.142430	5645.149075	25.075123
153.174768	5654.983308	25.080141
153.842371	5659.114902	25.085159
153.499955	5674.099595	25.090176
153.690003	5683.063143	25.095194
154.107871	5688.862721	25.100211
154.082010	5698.339919	25.105229
154.420189	5693.946390	25.110247
154.394160	5698.202443	25.115264
154.576722	5715.510327	25.120282
154.894738	5722.364112	25.125299
154.672493	5721.530745	25.130317
155.277975	5728.670951	25.135335
155.152760	5742.478947	25.140352
155.206063	5747.805331	25.145370
155.129688	5750.967594	25.150387
155.405322	5769.454182	25.155405
156.158925	5767.325205	25.160423
155.722074	5775.297946	25.165440
156.013603	5791.291424	25.170458
156.009056	5794.922261	25.175475
156.119166	5814.081952	25.180493
156.232081	5816.939937	25.185511
156.463871	5833.305832	25.190528
156.627750	5841.582237	25.195546
156.886997	5854.783973	25.200563
156.827825	5878.708492	25.205581
157.225899	5870.435393	25.210599
157.526322	5881.263155	25.215616
157.797242	5903.623921	25.220634
158.226728	5904.595108	25.225651
158.156614	5911.055201	25.230669
158.568384	5920.943777	25.235687
158.934206	5923.935778	25.240704
158.308987	5927.998492	25.245722
158.806295	5920.562143	25.250739
159.063037	5937.284090	25.255757
159.324290	5947.549815	25.260775
159.446069	5952.142639	25.265792
159.239586	5949.071820	25.270810
159.441229	5961.373518	25.275827
159.642959	5983.338001	25.280845
160.023334	5973.053626	25.285863
159.960474	5984.677040	25.290880
159.949287	6004.367325	25.295898
160.522778	6008.804165	25.300915
160.572112	6013.518840	25.305933
160.678165	6021.337186	25.310951
161.124207	6029.196974	25.315968
160.859320	6038.576054	25.320986
161.110544	6037.469621	25.326003
160.770712	6049.401634	25.331021
161.368338	6058.604563	25.336039
161.425548	6067.241868	25.341056
161.353860	6092.671244	25.346074
161.676948	6094.322030	25.351091
161.708968	6106.293685	25.356109
162.159248	6114.234922	25.361127
162.414750	6120.189503	25.366144
162.470416	6142.391720	25.371162
162.802781	6140.887443	25.376179
162.934823	6159.175947	25.381197
162.966551	6152.270176	25.386215
163.244878	6155.771536	25.391232
163.074546	6169.990989	25.396250
163.238085	6169.763242	25.401267
163.267078	6184.368173	25.406285
163.593995	6191.839470	25.411303
163.941491	6198.783520	25.416320
163.988616	6218.610112	25.421338
164.170137	6213.000387	25.426355
164.288325	6221.359884	25.431373
165.111868	6232.964548	25.436391
165.262894	6248.999378	25.441408
165.664949	6249.693928	25.446426
165.496799	6241.367313	25.451443
165.209022	6248.824445	25.456461
165.411847	6245.304325	25.461479
165.320309	6262.103229	25.466496
165.375894	6266.719129	25.471514
165.586622	6284.174664	25.476531
165.740081	6297.270178	25.481549
166.077527	6306.573973	25.486567
166.323934	6320.033758	25.491584
166.153380	6331.055530	25.496602
166.530971	6336.201853	25.501619
166.991677	6353.255260	25.506637
167.240933	6357.171599	25.511655
167.488215	6371.237392	25.516672
167.352877	6380.684741	25.521690
168.105896	6387.091812	25.526707
167.653133	6391.976791	25.531725
167.889011	6408.749789	25.536743
168.211846	6406.865010	25.541760
168.406710	6420.983249	25.546778
168.325203	6430.763127	25.551795
168.675921	6438.338128	25.556813
168.612206	6449.529485	25.561831
169.388373	6449.426738	25.566848
169.141987	6458.133886	25.571866
169.724664	6463.289155	25.576883
169.597733	6475.806829	25.581901
169.954190	6482.815877	25.586919
169.871885	6493.119947	25.591936
169.631005	6500.866576	25.596954
170.299651	6507.520513	25.601971
170.180495	6513.041450	25.606989
170.312142	6529.991888	25.612007
170.867088	6535.227286	25.617024
170.737886	6548.651378	25.622042
171.221300	6551.104183	25.627059
171.463324	6572.703181	25.632077
171.378686	6575.055570	25.637095
171.919141	6575.917862	25.642112
171.726253	6583.909555	25.647130
172.145327	6596.998398	25.652147
172.189901	6599.690428	25.657165
172.394327	6604.317821	25.662183
172.885887	6608.237294	25.667200
172.845916	6621.338088	25.672218
173.151035	6613.843178	25.677236
172.883494	6626.143061	25.682253
172.898000	6640.640135	25.687271
173.240140	6642.935144	25.692288
173.047963	6653.562732	25.697306
173.923094	6668.142825	25.702324
173.277723	6675.413071	25.707341
173.586544	6688.743388	25.712359
174.327737	6700.673782	25.717376
174.349375	6705.610798	25.722394
174.298011	6712.841668	25.727412
174.549962	6724.646682	25.732429
174.461241	6728.745481	25.737447
174.599599	6727.574611	25.742464
174.855208	6757.941492	25.747482
174.883609	6752.560788	25.752500
175.461644	6771.098877	25.757517
175.767707	6779.473392	25.762535
175.606859	6778.980770	25.767552
175.613820	6798.302864	25.772570
176.154852	6811.293832	25.777588
176.054853	6818.914346	25.782605
175.926631	6834.434666	25.787623
176.524932	6839.180357	25.792640
176.694124	6863.386071	25.797658
176.598832	6868.647668	25.802676
177.226938	6884.788257	25.807693
177.226359	6894.596743	25.812711
177.400371	6893.123529	25.817728
177.724315	6914.290227	25.822746
177.977285	6921.928096	25.827764
178.358911	6929.744698	25.832781
178.338231	6943.827655	25.837799
178.685771	6946.248133	25.842816
178.530540	6951.197138	25.847834
178.589518	6952.671554	25.852852
179.213388	6977.724850	25.857869
179.005125	6984.585792	25.862887
179.464040	6986.464780	25.867904
179.659058	7008.639899	25.872922
179.756904	7003.169320	25.877940
180.126801	7024.398399	25.882957
179.794011	7020.251734	25.887975
180.328619	7040.129119	25.892992
180.795759	7054.006304	25.898010
180.951302	7047.775324	25.903028
180.626953	7055.828856	25.908045
180.837883	7065.645338	25.913063
181.015423	7072.306967	25.918080
181.234011	7096.963006	25.923098
181.649413	7101.828970	25.928116
181.901180	7104.611736	25.933133
181.925370	7130.538951	25.938151
182.385781	7133.929894	25.943168
182.232180	7140.959120	25.948186
182.372641	7148.854637	25.953204
182.645607	7153.512472	25.958221
182.708064	7167.279508	25.963239
182.827380	7183.032839	25.968256
183.061595	7194.402119	25.973274
183.425260	7211.001141	25.978292
183.342950	7220.020738	25.983309
184.030689	7236.067057	25.988327
184.336247	7245.906695	25.993344
184.396757	7258.651249	25.998362
184.414089	7253.597300	26.003380
184.921008	7256.163328	26.008397
184.564567	7282.620773	26.013415
184.916706	7274.155355	26.018432
185.069642	7274.213385	26.023450
185.064688	7286.785110	26.028468
185.147553	7300.801606	26.033485
185.215832	7316.187367	26.038503
185.770251	7319.784607	26.043520
185.486299	7337.710105	26.048538
185.487014	7351.133370	26.053556
186.398119	7367.024847	26.058573
186.461666	7391.020503	26.063591
186.690205	7388.515844	26.068608
186.831914	7398.627477	26.073626
187.439238	7406.781450	26.078644
187.184823	7413.536129	26.083661
187.155954	7414.051991	26.088679
187.363363	7430.069548	26.093696
187.426580	7440.395548	26.098714
188.107090	7448.045583	26.103732
188.329676	7467.716597	26.108749
188.237255	7473.855561	26.113767
188.319713	7479.493581	26.118784
188.775872	7496.340402	26.123802
188.838723	7495.635922	26.128820
189.049489	7509.863002	26.133837
188.992276	7526.215700	26.138855
189.396511	7535.484400	26.143872
189.651056	7548.988010	26.148890
189.472739	7554.963665	26.153908
189.823421	7568.679534	26.158925
190.155541	7584.873424	26.163943
190.364456	7596.388981	26.168960
190.542749	7622.523208	26.173978
190.830484	7624.615345	26.178996
190.913755	7628.627415	26.184013
191.029955	7641.426650	26.189031
191.604864	7654.981175	26.194048
191.888872	7659.826831	26.199066
191.495494	7669.662537	26.204084
192.111601	7677.177534	26.209101
191.713012	7689.950110	26.214119
192.230545	7701.269004	26.219136
192.784154	7724.493773	26.224154
192.783577	7718.043933	26.229172
192.918159	7735.361237	26.234189
192.730916	7752.552180	26.239207
193.083077	7767.385560	26.244224
193.241015	7774.991316	26.249242
193.300109	7788.648846	26.254260
193.802403	7798.587399	26.259277
193.620108	7813.580312	26.264295
194.169317	7827.435755	26.269312
194.312113	7844.152033	26.274330
194.507557	7860.588571	26.279348
195.190115	7869.112970	26.284365
195.010547	7880.146548	26.289383
195.467872	7888.491560	26.294400
195.760931	7895.135391	26.299418
195.938846	7920.111452	26.304436
196.243438	7911.605837	26.309453
196.307999	7914.118133	26.314471
196.407517	7928.634472	26.319488
196.776945	7930.979042	26.324506
196.734038	7936.040153	26.329524
196.963031	7945.914260	26.334541
197.038569	7968.608070	26.339559
197.360322	7972.623897	26.344576
197.439476	7981.669084	26.349594
197.806740	7989.201094	26.354612
197.801886	7998.578315	26.359629
197.843298	8026.856121	26.364647
198.351380	8022.249160	26.369664
198.310881	8040.033014	26.374682
198.235896	8053.427605	26.379700
198.597095	8057.478314	26.384717
198.944315	8073.663953	26.389735
199.095627	8087.471426	26.394752
199.378900	8106.855789	26.399770
199.380317	8108.396143	26.404788
199.861449	8113.422564	26.409805
199.780961	8138.035291	26.414823
200.316403	8134.330108	26.419840
200.100603	8151.513266	26.424858
200.385958	8163.313971	26.429876
200.637907	8164.073159	26.434893
200.539163	8195.893367	26.439911
200.996138	8198.334755	26.444928
201.318118	8209.397300	26.449946
201.073862	8225.527347	26.454964
201.368091	8238.191763	26.459981
201.917067	8250.203797	26.464999
202.094435	8264.951303	26.470016
202.344409	8281.856401	26.475034
202.511357	8291.348927	26.480052
202.502155	8302.577067	26.485069
202.424458	8305.563173	26.490087
203.105525	8320.550687	26.495104
203.258031	8331.122082	26.500122
203.287994	8362.410955	26.505140
204.088840	8364.141809	26.510157
204.289913	8369.556304	26.515175
204.245119	8390.154190	26.520192
204.280136	8401.280747	26.525210
204.267104	8412.468510	26.530228
204.835552	8428.547189	26.535245
205.034348	8438.517848	26.540263
205.080990	8441.793899	26.545280
205.280772	8458.135574	26.550298
205.330326	8473.127428	26.555316
206.038166	8493.837997	26.560333
205.783695	8504.504820	26.565351
205.890256	8515.853869	26.570368
206.300161	8532.677312	26.575386
206.311838	8549.632614	26.580404
206.750890	8548.591328	26.585421
207.315944	8565.485212	26.590439
207.416742	8588.147409	26.595456
207.644847	8591.480304	26.600474
207.201703	8608.380622	26.605492
207.902983	8613.991504	26.610509
208.242074	8634.062258	26.615527
208.345544	8640.044632	26.620544
208.710387	8650.109366	26.625562
208.677549	8668.397774	26.630580
208.910448	8679.686089	26.635597
209.181220	8699.290877	26.640615
209.653890	8706.105768	26.645632
209.788120	8707.467505	26.650650
209.906032	8721.144924	26.655668
210.059437	8738.485476	26.660685
210.107000	8747.198163	26.665703
210.327530	8759.271453	26.670720
210.731093	8774.681676	26.675738
210.720830	8782.898284	26.680756
211.139425	8799.262811	26.685773
211.222751	8812.169037	26.690791
211.558355	8820.618786	26.695808
212.084226	8827.138080	26.700826
211.686228	8838.642143	26.705844
211.934257	8850.266015	26.710861
212.173789	8872.682663	26.715879
212.357434	8880.243803	26.720896
212.772825	8889.975553	26.725914
213.051162	8913.071292	26.730932
212.934760	8913.673525	26.735949
213.177937	8937.785121	26.740967
213.236018	8947.708638	26.745984
213.786542	8959.048397	26.751002
213.625696	8974.742954	26.756020
214.299615	8980.364550	26.761037
214.244182	8997.422334	26.766055
214.341622	9011.409428	26.771072
214.903954	9013.471338	26.776090
214.810000	9028.214597	26.781108
215.052889	9046.917986	26.786125
215.266575	9058.572627	26.791143
215.243814	9074.245637	26.796160
215.748774	9084.746462	26.801178
215.882948	9105.266587	26.806196
216.342873	9120.706156	26.811213
216.548959	9130.025645	26.816231
216.291946	9147.029898	26.821248
216.596936	9158.970241	26.826266
216.975826	9181.188622	26.831284
217.226173	9194.608846	26.836301
217.546285	9214.383258	26.841319
217.944767	9218.384181	26.846336
218.274921	9232.407602	26.851354
217.663683	9239.130436	26.856372
218.531023	9269.285634	26.861389
218.881531	9275.545244	26.866407
219.012996	9299.134910	26.871424
219.372694	9296.644182	26.876442
219.443755	9312.056424	26.881460
219.435490	9322.906155	26.886477
219.620189	9332.437479	26.891495
220.097823	9350.555027	26.896512
220.135887	9371.210480	26.901530
220.463054	9387.580378	26.906548
220.753162	9402.775255	26.911565
220.838393	9412.521114	26.916583
220.620260	9422.346075	26.921600
221.316103	9430.588118	26.926618
221.686607	9455.908642	26.931636
221.662614	9465.700056	26.936653
222.209386	9480.958981	26.941671
221.929496	9505.841556	26.946688
222.596241	9511.966457	26.951706
222.739961	9529.662888	26.956724
222.735010	9552.923780	26.961741
223.113358	9561.490308	26.966759
223.420304	9579.167530	26.971776
223.824956	9587.966753	26.976794
223.872510	9604.832147	26.981812
224.132816	9619.744550	26.986829
224.649955	9630.108010	26.991847
224.270971	9649.310411	26.996864
224.865348	9653.015522	27.001882
225.025343	9678.593500	27.006900
225.527102	9679.935623	27.011917
225.914577	9700.208337	27.016935
225.675711	9713.197234	27.021952
225.897888	9709.177722	27.026970
225.977236	9729.628190	27.031988
226.378009	9747.691861	27.037005
226.317956	9760.081292	27.042023
226.160078	9776.237037	27.047040
227.056518	9784.848803	27.052058
227.037484	9800.553413	27.057076
227.416324	9814.999054	27.062093
227.635156	9835.645647	27.067111
227.799957	9847.125312	27.072128
228.459701	9865.369547	27.077146
228.176285	9882.738549	27.082164
228.451839	9890.484620	27.087181
228.870460	9899.177607	27.092199
228.989644	9906.913449	27.097216
229.459886	9913.337649	27.102234
229.400712	9933.377474	27.107252
229.333615	9944.877740	27.112269
229.858266	9961.640300	27.117287
229.813152	9976.663983	27.122304
230.046499	9990.532641	27.127322
230.224377	10015.653610	27.132340
230.552352	10026.593162	27.137357
230.909236	10042.823211	27.142375
230.786805	10056.959201	27.147392
231.314004	10078.047159	27.152410
231.798081	10093.177482	27.157428
231.846351	10115.461401	27.162445
232.191836	10121.336876	27.167463
232.563956	10139.831672	27.172480
232.616226	10145.345777	27.177498
232.744443	10163.045237	27.182516
232.915026	10176.235539	27.187533
233.464842	10198.093668	27.192551
233.681564	10209.495958	27.197568
233.835309	10221.921667	27.202586
233.992985	10241.886805	27.207604
234.120052	10241.137431	27.212621
234.828450	10263.946452	27.217639
234.968454	10278.613001	27.222656
235.041260	10296.750684	27.227674
235.535167	10308.501140	27.232692
235.503781	10315.963936	27.237709
236.015703	10325.700264	27.242727
236.013358	10342.681496	27.247744
236.248219	10360.598091	27.252762
236.582159	10368.827783	27.257780
236.939937	10389.712137	27.262797
237.361885	10394.997900	27.267815
237.147141	10414.693184	27.272832
237.411473	10426.296542	27.277850
237.532218	10440.764155	27.282868
237.566097	10465.305203	27.287885
238.293703	10475.184643	27.292903
238.370449	10490.366468	27.297920
238.500253	10507.895500	27.302938
238.883073	10519.562451	27.307956
238.624409	10541.096108	27.312973
239.106966	10550.748744	27.317991
239.239189	10569.003684	27.323008
239.667184	10598.787811	27.328026
240.154367	10610.533195	27.333044
240.034199	10638.316127	27.338061
240.553504	10642.724702	27.343079
240.882158	10667.106165	27.348096
240.810533	10668.613967	27.353114
241.278564	10685.082925	27.358132
241.155871	10706.147100	27.363149
241.357222	10713.226264	27.368167
242.013511	10737.408090	27.373184
242.395519	10749.643671	27.378202
242.029730	10771.696425	27.383220
242.441933	10796.494397	27.388237
243.009886	10797.538898	27.393255
242.938296	10822.510577	27.398272
243.151286	10840.544730	27.403290
243.743208	10855.481954	27.408308
243.621659	10862.918043	27.413325
244.124803	10889.400667	27.418343
244.311297	10902.238498	27.423360
244.278913	10925.385405	27.428378
244.889352	10940.521882	27.433396
244.591606	10956.766863	27.438413
245.332023	10967.392908	27.443431
245.198713	10989.791567	27.448448
245.782303	10993.167094	27.453466
246.009427	11017.170219	27.458484
245.907630	11033.450880	27.463501
246.351175	11047.142144	27.468519
246.783040	11075.211843	27.473536
246.649871	11083.635014	27.478554
247.140962	11109.636723	27.483572
247.442473	11123.716577	27.488589
247.877943	11131.529684	27.493607
247.686177	11151.885241	27.498624
248.401276	11175.518467	27.503642
248.427611	11180.067547	27.508660
248.486779	11204.956098	27.513677
249.059831	11221.083840	27.518695
249.181241	11233.808947	27.523712
249.452646	11244.994898	27.528730
249.786366	11260.130775	27.533748
249.650336	11287.964517	27.538765
250.372141	11295.846513	27.543783
250.461289	11311.481762	27.548800
250.753004	11330.615547	27.553818
251.009881	11344.547834	27.558836
250.997282	11374.547465	27.563853
251.499726	11387.067733	27.568871
251.589343	11406.043794	27.573888
251.789614	11422.792172	27.578906
252.398540	11446.568679	27.583924
252.023503	11463.972440	27.588941
252.591175	11478.475045	27.593959
252.780325	11504.202518	27.598976
253.245764	11524.417632	27.603994
253.668339	11540.291346	27.609012
253.694945	11551.787389	27.614029
254.189465	11576.532449	27.619047
253.755434	11595.316011	27.624064
254.407924	11611.564269	27.629082
255.020453	11623.660108	27.634100
254.839402	11645.249180	27.639117
255.463250	11666.374314	27.644135
255.595080	11685.224050	27.649152
255.560497	11702.284188	27.654170
256.001018	11714.795429	27.659188
256.289599	11740.217139	27.664205
256.456638	11750.481897	27.669223
256.837696	11777.089105	27.674240
257.262678	11795.438317	27.679258
257.660568	11802.506052	27.684276
257.537095	11825.538868	27.689293
257.436146	11838.614990	27.694311
257.779635	11863.554604	27.699328
258.010841	11890.763313	27.704346
258.670707	11908.336928	27.709364
258.694217	11930.307946	27.714381
259.082156	11942.732844	27.719399
259.207993	11966.086761	27.724416
259.798988	11986.620585	27.729434
259.960346	11997.770542	27.734452
260.098925	12015.113297	27.739469
260.450823	12042.713830	27.744487
260.610349	12063.520583	27.749504
260.962628	12080.520461	27.754522
261.340164	12090.869268	27.759540
261.370090	12113.272111	27.764557
261.784666	12125.282445	27.769575
261.862591	12140.695937	27.774592
262.095329	12163.995459	27.779610
262.203849	12178.554743	27.784628
262.435535	12197.755654	27.789645
262.904670	12216.619397	27.794663
263.272810	12231.216997	27.799680
263.538299	12250.425297	27.804698
264.308972	12265.092495	27.809716
264.391059	12281.383321	27.814733
264.519000	12285.133614	27.819751
265.036473	12307.463470	27.824768
265.129311	12317.017021	27.829786
265.588609	12330.106770	27.834804
265.595313	12340.330652	27.839821
265.564465	12353.554040	27.844839
265.828213	12370.047007	27.849856
265.981384	12402.074892	27.854874
266.417779	12414.972502	27.859892
266.423379	12434.253280	27.864909
266.731346	12454.314066	27.869927
266.985638	12482.874727	27.874944
267.312916	12499.190489	27.879962
267.758090	12514.221497	27.884980
267.663382	12540.907470	27.889997
268.146690	12563.546136	27.895015
268.271448	12590.355692	27.900032
268.513217	12612.299629	27.905050
268.744421	12619.213786	27.910068
268.790632	12648.634655	27.915085
269.433669	12666.780033	27.920103
269.539108	12693.501183	27.925120
269.708360	12726.111306	27.930138
270.350799	12733.905293	27.935156
270.782836	12754.682750	27.940173
270.928058	12780.579897	27.945191
271.267778	12802.410816	27.950208
271.464771	12822.764115	27.955226
272.254356	12843.536187	27.960244
272.180273	12862.776199	27.965261
272.314068	12887.352118	27.970279
272.731387	12902.912014	27.975296
273.043681	12932.528486	27.980314
273.391377	12942.692962	27.985332
273.278331	12968.820299	27.990349
273.599624	12989.425887	27.995367
274.151111	13006.689081	28.000384
274.546856	13036.090535	28.005402
274.585659	13040.533899	28.010420
274.868654	13066.274063	28.015437
275.114066	13076.243051	28.020455
275.504638	13096.310526	28.025472
275.511173	13111.581253	28.030490
275.867670	13135.607862	28.035508
276.212719	13162.418457	28.040525
276.343426	13194.245934	28.045543
276.844965	13212.565585	28.050560
277.085684	13223.365931	28.055578
277.790555	13245.430694	28.060596
277.804939	13262.977211	28.065613
277.791865	13286.654526	28.070631
278.027391	13305.063307	28.075648
278.474364	13330.241286	28.080666
278.821937	13346.665130	28.085684
278.725547	13376.491583	28.090701
279.323628	13390.040343	28.095719
279.958299	13412.365780	28.100736
280.089236	13428.119396	28.105754
280.171372	13440.476339	28.110772
280.330761	13466.299570	28.115789
280.547824	13487.190457	28.120807
280.953033	13494.911393	28.125824
280.979519	13516.072175	28.130842
281.674731	13534.374432	28.135860
281.970149	13552.196153	28.140877
281.642461	13573.216682	28.145895
282.041068	13593.719233	28.150912
282.045653	13612.890837	28.155930
282.559129	13635.184992	28.160948
282.614358	13657.920449	28.165965
283.008639	13678.518510	28.170983
283.770388	13697.287367	28.176000
283.523456	13726.477918	28.181018
283.999602	13750.259184	28.186036
284.475629	13781.768274	28.191053
284.740147	13799.342422	28.196071
285.030932	13822.802270	28.201088
285.176226	13857.353985	28.206106
285.688347	13865.042535	28.211124
285.784275	13892.616385	28.216141
286.112270	13925.541615	28.221159
286.438400	13941.656683	28.226176
287.121391	13966.037435	28.231194
287.711144	13981.959652	28.236212
287.602544	14001.105163	28.241229
287.884403	14018.244139	28.246247
288.346363	14033.826395	28.251264
288.455524	14064.256504	28.256282
288.677376	14069.167258	28.261300
289.230475	14095.921316	28.266317
289.293786	14111.913476	28.271335
289.498537	14128.347737	28.276352
289.629011	14158.522009	28.281370
290.043699	14170.435726	28.286388
290.336778	14197.884391	28.291405
290.409472	14227.208811	28.296423
290.997384	14248.759340	28.301440
291.009861	14276.542622	28.306458
291.431884	14289.415340	28.311476
291.853811	14306.760021	28.316493
292.230630	14337.928702	28.321511
292.517691	14354.094454	28.326528
292.324521	14380.596308	28.331546
292.767075	14402.270842	28.336564
293.502829	14417.687356	28.341581
293.527897	14450.676738	28.346599
293.837278	14465.433701	28.351616
294.317229	14486.151862	28.356634
294.294272	14515.684357	28.361652
294.528665	14541.538353	28.366669
294.808148	14566.662094	28.371687
295.421906	14584.911803	28.376704
295.724748	14601.410061	28.381722
296.264153	14622.854918	28.386740
296.300737	14651.645594	28.391757
296.617723	14677.524734	28.396775
296.822629	14688.956850	28.401792
296.961750	14712.975289	28.406810
297.487469	14733.550746	28.411828
297.766746	14750.321273	28.416845
297.969208	14783.122372	28.421863
298.195813	14801.663486	28.426880
298.624391	14825.425123	28.431898
298.951391	14849.474310	28.436916
299.383018	14874.631472	28.441933
299.849133	14891.164411	28.446951
300.116249	14908.297022	28.451968
300.295702	14916.928737	28.456986
300.537890	14940.902894	28.462004
300.897846	14951.262338	28.467021
301.177062	14972.018788	28.472039
301.407897	14984.890344	28.477056
301.643579	15004.330337	28.482074
301.670984	15028.584593	28.487092
302.335106	15048.017525	28.492109
302.618742	15067.427962	28.497127
302.988527	15075.900446	28.502144
303.105107	15107.348020	28.507162
303.499496	15114.550195	28.512180
303.662492	15141.979537	28.517197
303.545059	15169.569703	28.522215
303.878601	15190.611601	28.527232
304.125439	15221.347291	28.532250
304.487914	15246.370494	28.537268
304.987807	15274.770543	28.542285
305.061348	15298.989489	28.547303
305.228291	15320.026044	28.552320
305.607755	15345.959468	28.557338
305.955205	15385.845109	28.562356
306.528561	15407.073921	28.567373
306.183751	15444.920460	28.572391
306.796961	15474.828532	28.577408
307.113893	15506.415926	28.582426
307.628837	15531.693552	28.587444
307.894878	15564.053334	28.592461
308.488504	15592.265462	28.597479
308.810365	15612.930651	28.602496
308.980510	15630.135949	28.607514
309.640627	15662.554185	28.612532
309.711530	15690.128229	28.617549
309.868332	15708.128440	28.622567
310.154392	15728.278229	28.627584
310.610866	15767.999142	28.632602
310.861084	15789.424282	28.637620
311.351771	15817.223325	28.642637
311.789499	15844.579052	28.647655
311.894309	15856.131772	28.652672
312.245650	15892.114068	28.657690
312.701140	15916.905646	28.662708
313.092809	15932.800515	28.667725
313.120612	15959.260459	28.672743
313.137804	15986.824392	28.677760
313.788225	16010.628553	28.682778
314.009911	16031.985789	28.687796
314.619184	16059.975064	28.692813
314.865345	16088.242350	28.697831
315.411010	16116.112174	28.702848
315.413838	16133.025128	28.707866
315.936996	16155.832384	28.712884
316.622886	16190.900577	28.717901
316.477254	16216.449980	28.722919
317.040918	16226.095978	28.727936
317.241899	16260.191646	28.732954
317.502013	16273.400596	28.737972
318.083087	16287.825827	28.742989
317.728171	16324.870265	28.748007
317.997511	16344.243174	28.753024
318.355080	16378.065001	28.758042
318.883825	16397.419439	28.763060
319.223713	16428.082473	28.768077
319.382043	16460.163737	28.773095
320.022936	16490.226981	28.778112
320.102996	16514.692800	28.783130
320.521505	16538.578163	28.788148
320.811740	16567.534122	28.793165
321.197537	16588.787306	28.798183
321.435859	16596.794644	28.803200
321.610284	16621.302671	28.808218
322.053162	16641.618364	28.813236
322.377376	16660.408143	28.818253
322.452306	16689.571731	28.823271
322.978745	16712.704463	28.828288
323.188128	16744.992985	28.833306
323.142801	16767.255146	28.838324
323.553309	16789.392234	28.843341
323.698759	16824.982121	28.848359
324.230841	16852.889885	28.853376
324.451655	16890.998100	28.858394
324.775585	16924.491346	28.863412
325.440831	16946.124400	28.868429
325.445734	16977.936809	28.873447
326.062773	17000.531370	28.878464
326.647056	17031.280265	28.883482
327.074311	17062.104344	28.888500
327.531064	17084.446153	28.893517
327.612609	17105.949717	28.898535
328.109547	17132.037715	28.903552
328.245026	17159.325787	28.908570
328.876843	17189.195709	28.913588
329.249201	17202.687783	28.918605
329.306296	17228.573168	28.923623
329.735603	17250.382502	28.928640
330.169414	17280.094063	28.933658
330.194280	17305.801398	28.938676
330.941294	17318.900051	28.943693
331.034249	17357.825192	28.948711
331.275070	17377.554217	28.953728
331.639474	17397.118605	28.958746
331.501685	17430.931429	28.963764
332.341924	17457.288274	28.968781
332.609941	17493.261341	28.973799
332.913507	17518.710512	28.978816
333.100677	17541.297234	28.983834
333.455639	17577.610610	28.988852
334.189998	17607.484069	28.993869
334.323506	17632.088229	28.998887
334.826742	17645.831760	29.003904
335.049479	17673.485932	29.008922
334.915837	17701.783486	29.013940
335.684653	17734.886260	29.018957
335.822241	17763.533098	29.023975
336.096384	17790.048564	29.028992
336.851123	17820.708840	29.034010
337.104745	17851.239185	29.039028
337.525110	17875.343863	29.044045
337.199661	17903.684391	29.049063
337.825470	17924.869862	29.054080
338.246055	17962.879401	29.059098
338.281343	17994.713989	29.064116
339.129000	18014.860325	29.069133
339.286112	18044.490051	29.074151
339.605883	18064.738081	29.079168
339.901626	18107.568782	29.084186
340.081084	18138.957747	29.089204
340.462465	18159.278352	29.094221
341.060215	18185.876337	29.099239
341.684433	18213.481025	29.104256
341.941024	18240.656883	29.109274
342.005216	18266.485681	29.114292
342.704907	18289.346777	29.119309
342.562672	18324.545405	29.124327
342.851486	18339.934009	29.129344
343.189506	18370.571984	29.134362
343.223137	18402.085298	29.139380
344.311980	18425.372055	29.144397
344.653773	18449.325495	29.149415
344.518514	18472.924089	29.154432
344.927603	18506.558354	29.159450
345.027567	18529.128296	29.164468
345.561198	18550.853258	29.169485
346.051514	18582.150021	29.174503
346.453044	18607.149354	29.179520
346.865379	18634.086564	29.184538
347.445600	18661.104915	29.189556
347.606200	18680.993138	29.194573
347.940723	18712.864158	29.199591
348.370247	18743.103004	29.204608
348.613944	18762.264388	29.209626
348.305268	18782.068278	29.214644
348.873781	18817.529212	29.219661
349.155743	18860.982872	29.224679
349.551404	18881.036648	29.229696
350.027774	18920.555592	29.234714
350.328019	18960.196971	29.239732
350.695203	18988.190501	29.244749
351.286358	19009.635299	29.249767
351.428655	19055.006619	29.254784
352.013191	19080.060024	29.259802
352.298739	19113.784185	29.264820
353.037995	19138.724980	29.269837
353.274611	19165.425099	29.274855
353.533331	19194.156154	29.279872
353.702121	19221.435584	29.284890
353.879618	19258.487502	29.289908
354.190403	19277.063953	29.294925
354.327291	19312.492310	29.299943
354.876987	19353.302138	29.304960
355.403380	19383.564712	29.309978
355.715993	19418.826741	29.314996
356.251994	19451.286568	29.320013
356.727483	19481.683627	29.325031
356.901549	19520.038083	29.330048
357.217144	19549.342007	29.335066
357.724018	19585.047758	29.340084
358.714174	19614.075530	29.345101
358.452528	19641.896821	29.350119
358.625083	19670.433577	29.355136
358.913104	19699.445097	29.360154
359.321362	19727.742838	29.365172
360.122736	19766.151149	29.370189
360.464128	19795.249222	29.375207
360.610600	19818.369359	29.380224
361.471658	19845.313771	29.385242
361.184963	19889.402146	29.390260
361.646248	19908.416846	29.395277
362.213931	19937.271186	29.400295
362.360685	19966.254683	29.405312
362.845887	20007.872066	29.410330
363.329169	20042.198669	29.415348
363.739779	20068.809585	29.420365
364.112878	20094.447093	29.425383
364.167131	20135.677340	29.430400
365.074656	20153.636741	29.435418
365.289037	20182.666829	29.440436
365.656723	20210.788395	29.445453
365.802834	20244.700619	29.450471
366.079821	20269.045536	29.455488
366.771156	20292.106158	29.460506
366.808727	20321.530605	29.465524
367.207148	20346.418922	29.470541
367.428124	20371.897391	29.475559
367.912672	20409.282484	29.480576
368.250221	20425.328518	29.485594
368.290507	20458.745906	29.490612
368.433821	20489.480884	29.495629
369.396080	20513.617672	29.500647
369.389254	20554.555085	29.505664
370.399473	20571.626855	29.510682
370.070143	20615.755127	29.515700
370.454800	20641.852779	29.520717
371.031253	20673.347904	29.525735
371.127057	20711.976000	29.530752
371.653221	20739.795491	29.535770
371.624303	20767.329183	29.540788
372.507374	20805.581411	29.545805
372.814468	20843.165722	29.550823
373.136220	20881.404927	29.555840
373.462956	20912.674175	29.560858
373.747573	20937.840124	29.565876
374.120105	20980.709314	29.570893
374.684444	21025.324047	29.575911
374.702472	21054.019704	29.580928
375.298348	21094.863833	29.585946
375.502159	21129.217156	29.590964
375.940941	21166.762501	29.595981
376.368551	21203.532487	29.600999
377.085326	21238.304815	29.606016
377.471259	21272.155968	29.611034
377.655040	21306.967674	29.616052
378.022055	21342.047714	29.621069
378.615747	21379.575518	29.626087
378.912616	21417.718562	29.631104
379.665967	21441.232079	29.636122
379.972066	21482.969097	29.641140
380.496712	21508.736358	29.646157
380.596145	21544.402073	29.651175
381.000647	21581.378579	29.656192
381.666895	21608.052633	29.661210
381.981769	21643.166649	29.666228
382.195221	21668.957589	29.671245
382.842651	21695.167125	29.676263
383.074106	21733.339980	29.681280
383.548021	21770.880971	29.686298
383.382360	21799.353734	29.691316
383.891726	21822.514162	29.696333
384.513106	21865.510581	29.701351
384.581379	21901.409295	29.706368
385.347048	21934.159505	29.711386
385.222799	21969.513490	29.716404
385.785726	22006.744003	29.721421
386.224150	22041.416014	29.726439
386.493530	22083.608685	29.731456
387.015302	22112.378624	29.736474
387.327739	22145.535075	29.741492
387.887019	22184.933857	29.746509
388.317121	22218.703886	29.751527
388.593545	22262.229114	29.756544
389.355152	22288.149841	29.761562
389.915974	22328.332209	29.766580
389.982550	22350.930722	29.771597
390.590418	22391.017384	29.776615
390.754811	22429.518029	29.781632
390.939152	22454.246651	29.786650
391.607877	22485.458501	29.791668
392.240811	22518.457952	29.796685
392.790705	22544.544875	29.801703
392.810503	22577.842671	29.806720
393.169295	22607.593024	29.811738
393.546744	22639.640614	29.816756
393.928671	22666.373269	29.821773
394.567597	22692.970919	29.826791
394.723332	22723.960184	29.831808
395.256423	22752.621856	29.836826
395.643110	22776.693600	29.841844
396.051838	22805.716057	29.846861
395.843592	22825.343970	29.851879
395.869265	22868.303172	29.856896
396.377534	22896.084269	29.861914
396.981146	22930.807789	29.866932
397.246329	22981.426373	29.871949
397.553139	23010.029074	29.876967
398.044515	23056.403888	29.881984
398.053354	23095.991803	29.887002
398.945382	23133.716328	29.892020
399.192132	23172.388766	29.897037
399.754380	23204.642129	29.902055
399.898917	23254.825325	29.907072
400.380848	23292.481683	29.912090
400.751394	23340.721294	29.917108
400.905481	23384.009049	29.922125
401.252389	23415.291725	29.927143
401.961397	23468.148550	29.932160
402.598100	23503.961119	29.937178
402.740604	23550.720330	29.942196
403.408718	23594.161840	29.947213
404.003239	23629.128135	29.952231
404.092982	23670.284343	29.957248
404.479663	23710.465182	29.962266
405.164492	23756.034043	29.967284
405.481261	23798.147092	29.972301
405.974145	23820.566748	29.977319
406.055262	23864.416759	29.982336
406.917524	23910.147761	29.987354
407.308729	23941.506475	29.992372
407.420164	23983.392980	29.997389
408.086129	24020.459457	30.002407
408.499931	24068.725647	30.007424
408.960653	24097.027741	30.012442
409.308126	24134.921610	30.017460
409.784464	24177.604494	30.022477
410.307410	24213.366639	30.027495
410.589069	24255.915876	30.032512
411.276560	24293.206989	30.037530
411.564202	24338.352787	30.042548
411.626407	24367.785686	30.047565
412.155394	24398.971867	30.052583
412.496716	24449.392654	30.057600
413.135978	24479.733824	30.062618
413.642933	24516.876684	30.067636
414.137763	24555.576134	30.072653
414.660558	24584.172535	30.077671
414.838004	24632.590856	30.082688
415.342435	24662.372016	30.087706
416.084090	24708.932649	30.092724
416.353180	24737.878671	30.097741
416.846463	24764.268070	30.102759
417.108955	24803.200300	30.107776
417.455279	24841.923563	30.112794
417.946262	24876.560672	30.117812
418.453455	24914.753302	30.122829
418.736257	24944.335765	30.127847
419.278248	24988.741696	30.132864
419.490209	25018.891502	30.137882
420.124067	25053.449659	30.142900
420.323498	25084.675885	30.147917
421.049984	25110.435155	30.152935
421.223981	25152.061506	30.157952
421.370682	25182.537768	30.162970
421.710377	25210.550721	30.167988
422.237229	25251.420510	30.173005
422.610028	25287.321843	30.178023
422.804649	25324.534077	30.183040
423.337593	25359.007449	30.188058
423.849841	25393.117569	30.193076
423.805416	25436.238608	30.198093
424.133226	25466.832290	30.203111
424.843082	25518.601049	30.208128
425.374565	25574.853425	30.213146
426.110524	25596.484924	30.218164
426.213796	25636.947847	30.223181
426.868652	25675.599108	30.228199
427.312538	25718.821223	30.233216
427.631944	25757.455663	30.238234
428.304191	25795.813711	30.243252
428.426622	25838.865234	30.248269
429.012931	25869.431677	30.253287
429.480491	25918.641888	30.258304
429.263769	25962.644240	30.263322
430.333467	25994.828932	30.268340
430.536307	26045.174283	30.273357
431.134515	26088.790143	30.278375
431.581109	26135.185408	30.283392
432.262567	26160.074581	30.288410
432.647585	26201.777485	30.293428
432.574579	26246.807083	30.298445
433.364021	26286.380132	30.303463
433.606755	26326.759389	30.308480
433.866824	26365.233639	30.313498
434.252018	26407.019100	30.318516
435.131749	26468.193400	30.323533
435.643317	26508.227540	30.328551
435.930109	26545.945842	30.333568
436.263196	26597.510929	30.338586
436.821903	26638.359575	30.343604
437.218961	26676.775038	30.348621
437.728278	26720.254495	30.353639
438.150750	26763.311548	30.358656
438.922434	26809.967133	30.363674
439.315641	26837.247123	30.368692
439.302855	26880.265153	30.373709
440.418760	26913.954632	30.378727
440.456861	26957.780180	30.383744
440.760861	27001.361922	30.388762
441.586157	27042.327634	30.393780
441.947547	27092.777158	30.398797
442.218437	27129.980763	30.403815
442.663607	27179.064812	30.408832
443.185761	27214.674392	30.413850
443.952888	27243.501752	30.418868
443.773928	27292.905047	30.423885
444.027349	27321.149331	30.428903
444.686771	27376.925276	30.433920
445.212024	27421.768963	30.438938
445.638973	27454.625497	30.443956
446.183364	27501.463643	30.448973
446.439516	27544.169168	30.453991
447.111756	27585.893132	30.459008
447.666979	27636.775044	30.464026
448.043338	27675.303085	30.469044
448.372499	27718.060745	30.474061
448.932877	27752.002963	30.479079
449.218109	27800.380370	30.484096
449.446051	27832.263706	30.489114
450.155114	27878.109869	30.494132
450.302775	27925.990828	30.499149
451.075706	27968.970256	30.504167
451.321262	28002.684093	30.509184
451.573267	28046.845075	30.514202
452.551234	28080.058761	30.519220
452.523337	28126.741471	30.524237
452.952769	28157.449706	30.529255
454.031132	28214.129394	30.534272
454.198946	28255.124679	30.539290
454.763873	28302.492390	30.544308
454.775866	28331.294189	30.549325
455.199137	28373.905744	30.554343
455.954501	28408.583330	30.559360
456.151723	28466.798627	30.564378
456.741883	28508.050629	30.569396
457.085027	28556.073106	30.574413
457.125612	28591.943823	30.579431
457.723552	28643.984590	30.584448
457.948771	28709.610579	30.589466
458.917464	28749.444786	30.594484
458.904852	28793.187397	30.599501
460.028422	28847.339711	30.604519
460.453789	28902.492782	30.609536
460.510740	28943.329820	30.614554
461.187239	28985.207677	30.619572
461.563490	29040.501551	30.624589
462.200529	29087.410991	30.629607
462.769939	29132.934184	30.634624
463.095652	29190.568836	30.639642
463.990124	29230.466172	30.644660
464.076186	29291.905993	30.649677
464.764649	29328.947057	30.654695
465.579937	29374.937961	30.659712
465.703187	29408.698550	30.664730
466.106516	29458.262381	30.669748
466.693057	29506.602940	30.674765
467.160208	29545.689180	30.679783
467.576122	29599.221063	30.684800
468.138673	29644.999311	30.689818
468.842159	29683.296575	30.694836
468.925562	29729.712644	30.699853
469.238493	29781.876787	30.704871
469.983130	29833.410855	30.709888
470.316005	29876.962587	30.714906
471.089693	29922.025684	30.719924
471.425311	29965.665672	30.724941
471.984441	30012.956058	30.729959
472.452563	30049.274374	30.734976
473.005524	30102.267750	30.739994
473.507334	30144.042580	30.745012
473.965243	30198.435463	30.750029
474.484989	30237.331457	30.755047
475.059489	30278.747499	30.760064
475.321826	30318.594241	30.765082
475.668227	30367.031322	30.770100
475.986506	30420.947269	30.775117
476.611883	30465.579641	30.780135
477.251828	30507.428391	30.785152
477.751740	30558.591705	30.790170
478.301274	30600.480090	30.795188
478.595049	30647.933599	30.800205
478.931665	30692.605366	30.805223
479.751778	30724.577438	30.810240
480.133902	30779.344044	30.815258
480.755510	30821.474449	30.820276
480.984797	30873.243544	30.825293
481.460164	30919.322740	30.830311
481.834057	30954.999961	30.835328
482.091993	31000.455948	30.840346
482.907464	31036.171614	30.845364
483.228309	31090.550378	30.850381
483.837072	31128.403679	30.855399
484.318464	31172.731402	30.860416
484.532069	31213.674820	30.865434
484.976956	31255.397590	30.870452
485.378135	31304.637455	30.875469
485.705470	31354.401060	30.880487
486.275853	31401.338839	30.885504
486.714935	31457.893681	30.890522
487.291203	31499.495216	30.895540
487.102125	31553.853910	30.900557
487.281009	31611.549909	30.905575
488.229170	31667.481912	30.910592
488.590370	31722.146809	30.915610
489.479754	31775.041192	30.920628
489.701166	31836.802414	30.925645
490.120301	31904.348970	30.930663
490.614587	31945.629177	30.935680
491.313444	32010.066151	30.940698
491.876614	32071.894657	30.945716
492.190961	32135.020383	30.950733
493.268546	32192.223201	30.955751
493.774465	32238.104551	30.960768
493.837836	32293.335991	30.965786
494.688895	32348.810883	30.970804
495.332798	32406.651194	30.975821
495.550534	32458.855934	30.980839
496.078569	32508.717298	30.985856
496.475021	32571.104445	30.990874
497.161234	32626.814522	30.995892
498.119118	32694.253961	31.000909
498.402736	32743.237460	31.005927
499.418115	32787.175195	31.010944
499.581284	32842.266009	31.015962
500.208147	32882.161717	31.020980
500.650392	32930.532847	31.025997
500.791721	32982.175539	31.031015
501.643669	33026.512384	31.036032
502.291294	33086.598375	31.041050
502.978533	33127.446072	31.046068
503.027912	33180.892848	31.051085
503.321346	33235.755657	31.056103
504.193741	33282.283669	31.061120
504.303210	33331.023957	31.066138
504.825377	33381.533191	31.071156
505.650452	33438.949670	31.076173
505.925216	33491.527386	31.081191
506.744874	33538.361376	31.086208
506.906465	33598.550244	31.091226
507.442334	33651.024240	31.096244
508.258357	33701.500863	31.101261
508.611623	33751.335652	31.106279
509.195261	33795.475892	31.111296
509.486180	33856.245872	31.116314
509.878700	33912.846248	31.121332
510.617739	33967.129052	31.126349
510.901683	34023.215640	31.131367
511.583530	34065.058638	31.136384
512.092088	34128.261098	31.141402
512.478303	34177.130706	31.146420
513.329515	34227.976111	31.151437
513.629263	34283.314851	31.156455
514.241556	34335.095741	31.161472
514.759716	34386.606984	31.166490
515.339459	34443.078296	31.171508
515.773276	34493.597711	31.176525
516.207033	34529.884944	31.181543
516.884193	34585.639564	31.186560
516.934814	34639.614621	31.191578
517.520597	34679.090228	31.196596
518.291542	34735.184625	31.201613
518.507603	34782.014751	31.206631
519.218968	34827.869576	31.211648
519.520481	34890.411239	31.216666
520.005682	34943.168261	31.221684
520.380812	34995.601222	31.226701
520.772622	35049.599759	31.231719
521.961252	35107.020742	31.236736
521.846565	35163.160139	31.241754
522.709281	35214.227414	31.246772
523.334841	35265.888369	31.251789
523.909673	35326.023752	31.256807
524.518810	35376.258573	31.261824
524.672292	35429.776924	31.266842
525.152630	35485.431957	31.271860
526.073899	35536.193658	31.276877
526.107214	35606.790626	31.281895
526.921251	35651.979885	31.286912
527.416930	35710.389929	31.291930
528.081608	35768.697788	31.296948
528.372239	35830.965709	31.301965
528.958189	35893.965296	31.306983
529.745699	35960.310029	31.312000
530.051990	36008.620973	31.317018
530.241886	36067.313841	31.322036
531.179092	36129.323290	31.327053
531.739829	36197.771943	31.332071
532.625114	36249.217560	31.337088
533.072607	36303.969338	31.342106
533.564853	36355.565293	31.347124
534.357828	36404.806299	31.352141
534.936235	36458.077306	31.357159
535.270405	36509.786917	31.362176
535.865276	36574.918052	31.367194
536.423501	36629.349804	31.372212
536.988240	36680.827695	31.377229
537.490463	36733.491637	31.382247
538.021948	36791.488016	31.387264
538.820683	36848.532134	31.392282
539.113352	36901.406363	31.397300
540.014096	36942.790762	31.402317
540.794340	36998.478650	31.407335
541.410109	37049.279155	31.412352
541.693815	37104.444362	31.417370
541.831618	37150.356079	31.422388
542.247430	37212.159452	31.427405
542.667960	37264.957640	31.432423
543.489014	37316.833235	31.437440
543.953416	37383.890633	31.442458
544.689126	37433.541356	31.447476
544.836708	37487.540044	31.452493
545.505862	37550.740156	31.457511
545.823295	37603.820913	31.462528
546.451616	37657.194585	31.467546
546.851467	37729.941751	31.472564
547.658485	37788.713417	31.477581
548.200327	37841.057691	31.482599
548.881061	37908.120783	31.487616
549.204808	37970.016636	31.492634
549.525547	38024.855895	31.497652
550.101376	38072.237633	31.502669
550.966335	38137.729602	31.507687
551.618280	38186.535157	31.512704
552.095857	38251.930050	31.517722
552.731748	38306.493012	31.522740
553.124327	38354.384677	31.527757
553.408252	38410.008507	31.532775
554.241241	38460.613907	31.537792
554.918966	38512.097460	31.542810
555.503815	38567.832662	31.547828
555.907536	38618.309623	31.552845
556.157536	38685.006243	31.557863
556.762815	38734.604506	31.562880
557.659916	38776.163753	31.567898
557.967803	38840.024995	31.572916
558.285615	38888.321636	31.577933
558.587438	38960.455905	31.582951
559.371570	39022.459739	31.587968
559.903193	39086.311962	31.592986
560.195965	39144.193962	31.598004
560.866196	39202.997225	31.603021
561.456647	39274.568763	31.608039
561.987067	39341.697789	31.613056
562.438876	39401.895476	31.618074
562.959741	39463.707812	31.623092
563.959930	39537.031064	31.628109
564.453249	39603.584889	31.633127
565.141476	39664.574741	31.638144
565.421774	39734.564734	31.643162
565.874877	39800.549958	31.648180
567.086842	39861.395094	31.653197
567.295148	39933.717993	31.658215
567.941690	39988.947569	31.663232
568.725538	40059.530113	31.668250
568.944829	40126.602775	31.673268
569.905000	40190.233015	31.678285
570.354586	40252.988431	31.683303
571.344405	40315.842825	31.688320
572.012924	40374.510388	31.693338
572.358381	40426.720904	31.698356
573.099279	40490.228251	31.703373
573.467259	40553.547535	31.708391
574.269622	40611.796335	31.713408
574.845251	40670.023879	31.718426
575.246472	40741.022723	31.723444
575.846436	40799.879250	31.728461
576.379134	40861.681046	31.733479
577.022951	40925.426221	31.738496
578.128083	40979.764292	31.743514
578.195106	41044.491908	31.748532
578.782900	41094.275376	31.753549
579.587956	41163.258045	31.758567
579.892770	41218.341861	31.763584
580.563078	41279.282109	31.768602
581.210767	41341.313910	31.773620
582.152585	41400.200731	31.778637
582.389370	41458.255750	31.783655
582.788561	41520.061337	31.788672
583.849633	41575.571533	31.793690
583.931945	41641.234572	31.798708
585.195535	41697.016946	31.803725
585.547958	41760.424372	31.808743
586.336285	41803.556004	31.813760
586.867339	41865.708748	31.818778
586.934834	41933.360968	31.823796
587.982936	41977.565426	31.828813
588.164409	42040.595642	31.833831
589.006049	42101.865530	31.838848
589.740254	42160.679382	31.843866
589.992820	42225.988604	31.848884
590.365396	42281.045492	31.853901
591.095704	42339.948981	31.858919
591.385901	42391.515029	31.863936
591.709155	42449.198593	31.868954
592.693705	42513.394681	31.873972
593.271542	42565.396786	31.878989
593.544078	42627.642765	31.884007
593.992406	42690.892368	31.889024
594.554687	42760.512619	31.894042
594.861060	42825.821511	31.899060
595.784638	42886.606363	31.904077
596.370154	42959.278623	31.909095
597.301600	43030.492763	31.914112
597.749676	43097.481725	31.919130
598.033425	43165.824913	31.924148
598.651823	43223.976612	31.929165
599.305681	43301.882878	31.934183
600.073082	43369.195838	31.939200
600.572881	43435.209958	31.944218
601.150443	43506.462074	31.949236
601.669923	43573.846108	31.954253
602.068728	43631.369109	31.959271
602.890851	43721.300213	31.964288
603.400223	43781.045454	31.969306
604.247079	43854.533637	31.974324
604.962082	43921.223938	31.979341
605.381783	43998.916302	31.984359
605.498260	44076.871490	31.989376
606.574412	44145.359255	31.994394
607.068938	44215.741081	31.999412
607.802467	44285.699843	32.004429
608.693607	44363.692849	32.009447
609.306936	44441.274197	32.014464
610.139832	44502.868367	32.019482
610.584469	44580.660059	32.024500
611.221467	44643.714878	32.029517
611.813177	44715.892180	32.034535
612.283966	44793.908240	32.039552
612.998334	44862.575053	32.044570
613.253704	44927.278178	32.049588
614.049159	45003.770240	32.054605
614.675474	45077.069261	32.059623
615.369476	45162.693118	32.064640
616.694730	45216.058262	32.069658
616.810991	45298.964482	32.074676
617.310536	45357.437668	32.079693
618.251746	45431.207246	32.084711
619.199214	45499.757269	32.089728
619.744033	45567.162322	32.094746
620.512211	45636.740328	32.099764
620.685843	45698.377774	32.104781
621.599696	45771.374669	32.109799
622.144731	45835.788335	32.114816
623.013990	45892.731071	32.119834
623.344527	45961.265252	32.124852
623.885933	46031.234246	32.129869
624.556819	46091.776409	32.134887
624.875238	46166.759312	32.139904
625.677341	46237.776196	32.144922
626.108340	46308.838769	32.149940
627.051359	46377.151772	32.154957
627.777505	46452.609487	32.159975
628.404784	46518.290096	32.164992
628.896829	46591.184900	32.170010
629.705516	46660.215672	32.175028
629.935113	46719.063628	32.180045
630.583471	46795.338094	32.185063
631.105888	46865.812416	32.190080
631.828892	46927.006583	32.195098
632.485900	47004.861960	32.200116
633.379896	47068.598192	32.205133
633.813772	47130.300006	32.210151
634.504098	47190.411879	32.215168
635.188223	47256.073074	32.220186
635.576896	47315.789677	32.225204
636.299876	47380.711291	32.230221
636.669593	47457.765481	32.235239
637.449787	47523.608521	32.240256
638.168660	47587.114254	32.245274
638.635506	47652.576544	32.250292
639.625882	47722.784122	32.255309
640.449732	47789.456189	32.260327
640.645235	47859.921529	32.265344
641.719360	47924.732766	32.270362
641.969648	47997.973620	32.275380
642.431279	48065.525671	32.280397
642.738097	48132.906043	32.285415
643.629693	48213.120263	32.290432
644.469778	48279.949388	32.295450
645.107583	48357.711176	32.300468
645.451532	48435.955789	32.305485
646.244843	48509.733254	32.310503
646.846031	48594.707670	32.315520
647.485653	48659.633329	32.320538
647.960504	48746.013643	32.325556
648.927995	48820.498736	32.330573
649.609274	48895.819742	32.335591
649.868096	48986.321895	32.340608
651.072437	49047.667818	32.345626
651.481426	49137.147411	32.350644
652.330978	49219.421644	32.355661
653.177169	49295.559611	32.360679
653.548089	49366.849921	32.365696
654.478026	49442.747492	32.370714
654.738690	49521.002522	32.375732
655.529963	49592.721206	32.380749
656.462860	49661.216474	32.385767
656.878998	49743.073279	32.390784
657.896330	49815.744271	32.395802
658.599615	49894.937253	32.400820
658.991778	49979.082718	32.405837
659.652651	50046.406934	32.410855
660.217335	50129.437669	32.415872
661.170410	50203.296791	32.420890
661.952020	50278.530687	32.425908
662.495352	50352.176058	32.430925
663.400372	50427.182316	32.435943
663.789354	50505.490188	32.440960
664.655984	50582.242948	32.445978
664.858341	50659.859262	32.450996
665.886740	50732.784500	32.456013
666.011632	50795.512643	32.461031
667.170234	50874.574405	32.466048
668.169975	50960.241759	32.471066
668.660538	51028.177621	32.476084
669.031277	51099.897242	32.481101
669.934903	51178.829133	32.486119
670.467248	51261.204613	32.491136
670.820648	51331.586249	32.496154
671.786233	51407.984564	32.501172
671.984294	51494.424837	32.506189
672.996902	51565.564486	32.511207
673.162849	51652.978486	32.516224
674.200297	51730.847251	32.521242
675.182659	51808.680611	32.526260
675.614417	51888.979636	32.531277
676.435870	51968.496560	32.536295
677.004808	52040.339902	32.541312
677.703173	52113.871666	32.546330
678.393132	52187.923848	32.551348
678.871159	52262.762450	32.556365
679.959727	52321.869881	32.561383
680.297188	52407.228646	32.566400
680.769898	52479.202307	32.571418
681.126631	52554.541747	32.576436
681.929356	52636.183684	32.581453
682.656115	52712.364233	32.586471
683.234454	52796.111065	32.591488
684.240580	52872.406582	32.596506
684.720262	52958.548722	32.601524
685.555367	53038.510099	32.606541
686.592082	53110.909936	32.611559
686.709251	53199.197947	32.616576
687.432741	53276.380656	32.621594
687.977024	53359.647577	32.626612
688.447009	53449.551867	32.631629
689.216483	53542.649559	32.636647
690.203312	53627.797164	32.641664
691.030143	53715.349496	32.646682
691.446007	53803.713229	32.651700
692.307054	53884.609981	32.656717
693.232585	53962.642911	32.661735
693.876343	54059.306102	32.666752
694.521938	54146.723883	32.671770
695.432441	54233.176582	32.676788
695.717663	54317.778413	32.681805
696.274257	54401.996323	32.686823
697.259504	54482.666840	32.691840
698.190377	54579.875726	32.696858
698.681590	54667.484144	32.701876
699.247435	54755.093855	32.706893
700.144696	54841.057234	32.711911
700.818282	54935.377823	32.716928
701.902316	55028.052399	32.721946
702.535994	55108.052329	32.726964
703.177863	55196.980742	32.731981
704.054141	55281.841517	32.736999
704.357642	55370.235015	32.742016
705.301836	55456.750183	32.747034
706.233561	55544.191591	32.752052
706.894746	55621.537264	32.757069
707.436105	55707.129163	32.762087
708.223869	55799.201291	32.767104
708.660831	55886.202483	32.772122
709.812312	55972.332656	32.777140
710.243307	56057.120363	32.782157
711.090340	56138.988957	32.787175
711.710069	56232.367473	32.792192
712.454321	56313.271800	32.797210
713.526413	56410.883748	32.802228
714.373390	56496.538203	32.807245
714.807127	56570.289814	32.812263
715.512396	56655.834125	32.817280
716.135591	56736.309488	32.822298
717.335819	56827.776697	32.827316
718.053166	56922.857753	32.832333
718.667640	56999.556984	32.837351
719.144078	57075.866692	32.842368
719.859110	57159.721428	32.847386
720.828701	57235.283540	32.852404
721.111669	57325.984906	32.857421
722.200271	57396.471976	32.862439
722.732044	57480.312224	32.867456
723.427160	57573.785414	32.872474
724.564776	57650.512391	32.877492
724.800015	57728.153079	32.882509
725.637700	57808.047800	32.887527
726.339382	57889.913477	32.892544
726.899991	57978.953542	32.897562
727.564914	58045.546764	32.902580
728.431261	58135.710438	32.907597
729.195626	58216.852199	32.912615
729.527230	58292.675761	32.917632
730.437017	58369.978692	32.922650
730.976722	58450.232333	32.927668
731.709289	58539.652610	32.932685
732.507343	58625.088103	32.937703
733.236145	58713.041190	32.942720
733.585334	58791.249745	32.947738
734.542602	58886.243990	32.952756
734.912759	58979.792481	32.957773
736.009837	59068.885457	32.962791
736.768042	59162.842268	32.967808
737.329803	59251.361469	32.972826
738.572363	59350.040956	32.977844
739.236983	59449.931687	32.982861
740.027551	59531.959879	32.987879
740.459389	59626.798767	32.992896
741.405901	59717.208939	32.997914
742.266636	59797.923124	33.002932
743.176110	59904.081746	33.007949
743.695304	59978.887414	33.012967
744.422671	60082.676355	33.017984
745.241095	60170.601673	33.023002
746.324556	60258.738996	33.028020
746.489282	60360.129602	33.033037
747.500454	60445.702672	33.038055
748.258449	60539.107776	33.043072
748.747718	60632.390738	33.048090
749.745453	60723.841040	33.053108
750.706075	60824.957010	33.058125
751.267496	60910.171690	33.063143
751.981384	61006.870738	33.068160
752.676304	61098.179949	33.073178
753.473947	61188.916369	33.078196
753.896188	61285.643190	33.083213
755.280273	61383.599733	33.088231
755.710247	61480.313446	33.093248
756.368846	61584.442326	33.098266
757.287768	61671.635632	33.103284
757.697114	61771.430178	33.108301
758.846967	61863.804086	33.113319
759.610868	61960.081239	33.118336
760.007584	62067.127091	33.123354
761.107765	62154.825458	33.128372
761.688122	62245.998589	33.133389
762.796002	62347.927004	33.138407
763.415652	62433.036525	33.143424
764.152786	62538.049693	33.148442
764.877930	62637.443767	33.153460
765.701873	62734.474169	33.158477
766.562954	62820.952570	33.163495
767.484669	62917.683505	33.168512
768.069848	63024.355787	33.173530
769.017344	63113.948950	33.178548
769.821186	63209.813200	33.183565
770.476068	63305.390944	33.188583
771.388062	63404.227044	33.193600
771.674980	63499.863152	33.198618
772.552358	63582.125432	33.203636
773.232888	63686.930724	33.208653
773.931638	63784.909093	33.213671
774.769150	63882.131749	33.218688
775.527682	63975.125539	33.223706
776.523768	64076.179550	33.228724
777.395146	64173.492994	33.233741
777.908866	64257.947920	33.238759
778.976722	64349.799426	33.243776
779.683253	64433.547348	33.248794
780.894149	64519.115838	33.253812
781.135971	64611.002684	33.258829
782.027922	64698.970502	33.263847
782.734775	64784.245296	33.268864
783.303216	64878.582702	33.273882
784.247451	64964.561660	33.278900
784.802607	65064.023626	33.283917
785.450968	65170.182312	33.288935
786.451014	65269.005623	33.293952
787.317735	65369.724207	33.298970
788.392408	65460.496071	33.303988
788.782699	65559.289375	33.309005
789.754316	65659.650803	33.314023
790.725559	65760.341910	33.319040
791.402830	65857.217398	33.324058
792.230609	65947.466187	33.329076
792.735331	66054.296855	33.334093
793.602604	66145.388554	33.339111
794.268376	66252.410099	33.344128
794.928166	66347.795997	33.349146
795.881423	66448.897854	33.354164
796.755048	66565.081329	33.359181
797.083256	66667.491227	33.364199
798.377230	66760.512710	33.369216
799.073050	66872.704952	33.374234
799.926040	66977.832434	33.379252
800.573653	67087.747493	33.384269
801.388359	67196.072961	33.389287
802.149307	67310.643924	33.394304
802.898108	67414.751133	33.399322
803.641553	67514.129866	33.404340
803.938698	67629.338393	33.409357
804.918487	67745.282658	33.414375
806.175795	67856.384540	33.419392
807.220998	67976.283266	33.424410
807.916029	68073.816538	33.429428
808.745720	68203.311056	33.434445
809.670941	68302.696030	33.439463
810.471465	68410.288010	33.444480
811.343936	68522.915688	33.449498
812.119505	68627.644134	33.454516
812.732075	68733.918195	33.459533
814.054790	68841.784791	33.464551
814.795339	68941.897657	33.469568
815.462267	69054.496514	33.474586
816.449261	69164.310298	33.479604
817.470076	69265.292341	33.484621
818.384700	69367.076585	33.489639
818.927399	69473.218978	33.494656
819.564133	69576.706573	33.499674
821.083652	69674.768983	33.504692
821.308996	69795.874652	33.509709
821.814687	69897.079119	33.514727
823.399775	70004.390219	33.519744
824.169719	70111.462130	33.524762
824.951354	70208.464290	33.529780
825.724337	70321.058351	33.534797
826.245600	70424.624382	33.539815
827.210601	70533.047929	33.544832
827.966874	70636.590664	33.549850
829.336232	70733.376093	33.554868
830.179832	70830.966106	33.559885
830.848060	70940.653642	33.564903
831.395678	71033.174112	33.569920
832.153812	71136.465228	33.574938
833.319287	71223.013037	33.579956
833.906022	71321.873609	33.584973
834.652757	71418.797056	33.589991
835.528900	71507.582184	33.595008
836.241150	71607.386731	33.600026
836.606881	71712.172727	33.605044
837.569592	71813.699316	33.610061
838.404259	71927.088519	33.615079
839.181347	72023.008864	33.620096
839.877423	72123.856464	33.625114
841.028486	72232.460529	33.630132
841.737345	72342.096870	33.635149
842.298856	72459.698118	33.640167
843.091940	72570.449461	33.645184
843.559940	72692.220743	33.650202
845.093769	72795.118235	33.655220
845.846368	72916.466006	33.660237
846.722677	73029.068116	33.665255
847.811169	73144.854643	33.670272
848.136213	73262.813120	33.675290
849.624935	73369.291729	33.680308
850.388857	73492.071619	33.685325
851.793615	73595.663726	33.690343
852.599731	73698.893986	33.695360
853.068298	73817.440420	33.700378
854.088299	73919.181412	33.705396
854.540739	74033.500758	33.710413
855.413517	74148.958090	33.715431
856.056775	74264.135193	33.720448
857.244643	74377.466859	33.725466
858.235311	74490.272548	33.730484
858.739556	74609.184225	33.735501
859.699380	74732.179789	33.740519
861.053246	74854.848211	33.745536
861.855294	74961.149332	33.750554
862.681729	75070.626451	33.755572
863.770837	75199.114011	33.760589
864.526193	75306.095153	33.765607
865.667874	75411.027495	33.770624
866.415421	75534.072620	33.775642
867.364418	75633.297784	33.780660
868.096421	75752.672854	33.785677
869.161570	75867.752742	33.790695
869.899668	75974.093193	33.795712
870.388546	76088.174857	33.800730
871.430169	76200.536350	33.805748
872.626602	76321.411962	33.810765
873.125112	76434.708186	33.815783
874.120830	76541.453882	33.820800
874.621962	76663.681309	33.825818
875.686665	76781.881379	33.830836
876.468496	76887.103789	33.835853
877.214680	77009.104375	33.840871
878.252719	77127.854834	33.845888
879.069161	77254.038578	33.850906
879.692993	77367.458394	33.855924
880.918977	77489.880046	33.860941
881.739838	77612.403684	33.865959
883.105275	77731.156166	33.870976
883.240614	77859.007522	33.875994
884.458433	77980.203822	33.881012
885.536677	78080.025721	33.886029
886.117141	78207.669646	33.891047
887.300073	78317.103976	33.896064
887.991451	78435.889033	33.901082
889.036879	78552.009445	33.906100
890.197381	78661.689357	33.911117
890.759273	78774.985313	33.916135
891.653942	78871.494300	33.921152
892.697177	78993.330483	33.926170
893.379297	79093.750158	33.931188
893.995254	79206.710025	33.936205
894.923413	79323.004059	33.941223
895.966593	79423.520418	33.946240
896.956637	79541.870714	33.951258
897.720102	79653.960481	33.956276
898.719372	79770.194574	33.961293
899.554178	79881.741985	33.966311
900.667136	79996.046180	33.971328
901.531374	80114.013191	33.976346
902.216154	80233.655807	33.981364
902.937337	80345.336884	33.986381
903.612978	80469.099475	33.991399
904.483842	80587.156129	33.996416
905.265127	80722.926616	34.001434
906.221116	80851.093998	34.006452
907.226467	80968.573738	34.011469
907.910553	81105.539569	34.016487
909.268782	81234.380560	34.021504
910.408301	81354.514222	34.026522
911.459762	81484.595352	34.031540
912.457253	81602.826492	34.036557
912.924354	81725.499642	34.041575
914.040562	81843.776552	34.046592
914.833739	81977.321299	34.051610
915.658247	82108.758526	34.056628
916.647622	82237.256404	34.061645
917.469603	82362.170052	34.066663
918.662602	82485.379017	34.071680
919.472472	82618.645422	34.076698
920.587888	82739.878392	34.081716
921.411342	82862.741401	34.086733
922.104437	82998.980092	34.091751
923.362555	83126.426267	34.096768
924.428718	83252.167189	34.101786
925.175417	83381.709212	34.106804
926.118894	83511.068963	34.111821
926.950558	83650.203339	34.116839
928.015471	83764.314894	34.121856
929.356547	83893.842196	34.126874
929.997637	84028.510066	34.131892
930.938999	84156.998764	34.136909
931.546311	84287.086215	34.141927
932.782069	84412.146774	34.146944
933.849197	84540.364069	34.151962
934.295838	84671.010602	34.156980
935.604840	84805.944996	34.161997
936.445056	84943.525714	34.167015
937.615460	85061.503342	34.172032
938.659815	85197.532732	34.177050
939.090138	85325.625132	34.182068
940.095850	85447.051439	34.187085
941.283611	85579.322042	34.192103
942.202183	85711.850814	34.197120
942.949171	85844.407056	34.202138
944.334787	85975.698099	34.207156
945.049621	86095.702726	34.212173
946.141334	86232.020998	34.217191
946.961352	86362.857450	34.222208
947.869112	86492.160101	34.227226
948.586477	86622.164757	34.232244
949.763217	86751.249029	34.237261
950.845868	86883.846139	34.242279
951.634432	87005.908531	34.247296
952.525020	87136.534634	34.252314
953.434998	87250.291319	34.257332
954.514245	87372.132308	34.262349
955.409858	87497.031280	34.267367
956.467879	87622.260185	34.272384
957.405463	87752.146653	34.277402
958.100120	87872.668613	34.282420
958.737007	87995.772670	34.287437
959.741696	88120.327712	34.292455
960.473701	88256.800408	34.297472
961.627529	88386.338984	34.302490
962.296373	88525.876972	34.307508
963.936920	88656.164263	34.312525
964.546294	88793.533065	34.317543
965.310794	88929.915055	34.322560
966.625968	89062.840388	34.327578
967.167514	89198.003871	34.332596
968.135240	89332.581634	34.337613
969.415464	89475.741621	34.342631
970.266531	89611.707628	34.347648
971.163774	89748.541491	34.352666
972.151076	89901.140412	34.357684
973.263923	90028.601412	34.362701
974.132787	90179.699464	34.367719
975.126543	90323.288563	34.372736
975.993672	90454.249761	34.377754
976.918796	90607.977297	34.382772
977.980939	90741.114454	34.387789
978.990565	90893.816307	34.392807
979.931704	91044.324377	34.397824
980.815557	91189.138836	34.402842
982.019254	91336.045837	34.407860
983.348423	91487.192432	34.412877
984.181729	91633.043535	34.417895
985.117308	91772.821005	34.422912
986.548833	91920.341553	34.427930
987.225504	92062.036696	34.432948
988.593367	92205.893011	34.437965
989.342073	92352.597322	34.442983
990.093464	92489.643866	34.448000
991.502915	92633.280216	34.453018
992.270221	92784.052252	34.458036
993.483348	92919.989102	34.463053
994.618643	93068.119264	34.468071
995.561084	93213.187659	34.473088
996.703144	93355.120118	34.478106
997.566760	93498.047454	34.483124
998.716841	93632.983327	34.488141
999.743965	93775.417371	34.493159
1000.620798	93919.865608	34.498176
1001.782671	94066.488062	34.503194
1002.634037	94207.329181	34.508212
1003.585841	94342.780859	34.513229
1004.693601	94489.832076	34.518247
1005.539494	94636.063056	34.523264
1006.691068	94778.000556	34.528282
1007.369610	94925.133709	34.533300
1008.951315	95069.527641	34.538317
1009.484714	95205.365475	34.543335
1010.728940	95353.236002	34.548352
1011.866637	95495.495836	34.553370
1012.721851	95650.222922	34.558388
1013.623404	95785.321135	34.563405
1014.451199	95942.056755	34.568423
1015.430094	96082.315953	34.573440
1016.472650	96238.334919	34.578458
1017.376883	96388.304415	34.583476
1018.374699	96524.696382	34.588493
1019.356384	96667.581734	34.593511
1020.179792	96813.813721	34.598528
1021.767316	96947.224974	34.603546
1022.814189	97092.966914	34.608564
1023.442797	97221.940572	34.613581
1024.502269	97362.699904	34.618599
1025.355234	97497.559522	34.623616
1026.809969	97637.979303	34.628634
1027.510536	97786.770347	34.633652
1028.589430	97932.130820	34.638669
1029.540546	98078.690910	34.643687
1030.244819	98216.226316	34.648704
1031.451739	98374.118916	34.653722
1032.399109	98529.923187	34.658740
1033.730059	98672.674123	34.663757
1034.845867	98828.073158	34.668775
1035.260456	98978.258294	34.673792
1036.910905	99124.016428	34.678810
1037.316597	99276.967997	34.683828
1038.539987	99431.237495	34.688845
1039.846120	99594.495777	34.693863
1040.502054	99749.299347	34.698880
1041.582554	99905.786694	34.703898
1042.694672	100070.814584	34.708916
1044.172727	100220.737573	34.713933
1044.548830	100383.917241	34.718951
1046.017376	100549.880628	34.723968
1047.316147	100701.760936	34.728986
1048.164749	100853.306736	34.734004
1049.595299	101022.270476	34.739021
1050.551559	101181.978272	34.744039
1051.837401	101337.007723	34.749056
1052.620659	101482.202237	34.754074
1053.550459	101650.601028	34.759092
1055.028312	101807.124031	34.764109
1056.127668	101967.764121	34.769127
1056.790522	102127.763340	34.774144
1058.201575	102285.579598	34.779162
1059.063277	102446.271904	34.784180
1060.223974	102604.179593	34.789197
1061.444675	102768.012271	34.794215
1062.591853	102919.901202	34.799232
1063.852758	103081.573746	34.804250
1064.385847	103242.879225	34.809268
1065.836318	103395.039815	34.814285
1066.647780	103560.880347	34.819303
1067.868334	103728.534155	34.824320
1068.850487	103886.082831	34.829338
1069.525365	104045.341327	34.834356
1070.794888	104207.068688	34.839373
1072.006155	104364.989480	34.844391
1072.741037	104527.182465	34.849408
1074.321828	104681.864373	34.854426
1075.323573	104858.319562	34.859444
1076.242982	105018.951806	34.864461
1077.640020	105183.618229	34.869479
1078.518154	105339.148573	34.874496
1079.673834	105492.734220	34.879514
1080.492231	105669.336459	34.884532
1081.734911	105829.465461	34.889549
1083.039753	105989.927842	34.894567
1083.791398	106156.082134	34.899584
1084.987596	106315.523299	34.904602
1086.203636	106488.593201	34.909620
1087.597515	106642.970948	34.914637
1088.509068	106805.261273	34.919655
1089.495456	106968.326826	34.924672
1090.570371	107119.827513	34.929690
1091.655461	107277.642105	34.934708
1092.721217	107428.574968	34.939725
1094.017057	107565.511246	34.944743
1094.656422	107727.227185	34.949760
1095.941747	107878.774348	34.954778
1096.537244	108037.975166	34.959796
1097.997381	108192.387525	34.964813
1099.047783	108346.598422	34.969831
1099.857395	108499.262596	34.974848
1101.308334	108671.266842	34.979866
1102.008214	108822.047474	34.984884
1103.095148	108982.760795	34.989901
1104.172098	109149.702822	34.994919
1104.983797	109325.323021	34.999936
1106.398865	109486.621341	35.004954
1107.269080	109663.869947	35.009972
1108.356727	109833.540022	35.014989
1109.489865	110000.794331	35.020007
1110.307897	110184.863626	35.025024
1111.901637	110352.567432	35.030042
1112.782026	110533.597902	35.035060
1113.964071	110710.561993	35.040077
1115.294419	110893.996777	35.045095
1116.282339	111071.069146	35.050112
1117.428233	111255.041939	35.055130
1118.794437	111436.888678	35.060148
1119.536417	111598.619043	35.065165
1120.896101	111791.387763	35.070183
1121.960839	111975.237465	35.075200
1123.405164	112140.626898	35.080218
1124.315615	112325.276156	35.085236
1125.234515	112502.493230	35.090253
1126.615637	112678.700321	35.095271
1127.646751	112859.363855	35.100288
1129.053183	113042.594802	35.105306
1130.258588	113219.060318	35.110324
1131.007280	113404.869157	35.115341
1132.633487	113582.386628	35.120359
1133.526236	113762.125119	35.125376
1134.905900	113948.256479	35.130394
1136.009107	114126.277007	35.135412
1136.949896	114301.115056	35.140429
1138.369006	114484.934685	35.145447
1139.164965	114673.875266	35.150464
1140.685970	114852.569526	35.155482
1141.507384	115040.924584	35.160500
1142.658745	115221.175111	35.165517
1143.917842	115400.940370	35.170535
1145.154953	115589.867309	35.175552
1146.276788	115766.878183	35.180570
1147.643234	115946.109260	35.185588
1148.657478	116133.247437	35.190605
1150.227223	116308.782897	35.195623
1151.165751	116500.767214	35.200640
1152.209081	116672.771958	35.205658
1153.297627	116862.274005	35.210676
1154.898719	117042.272686	35.215693
1156.230935	117226.893206	35.220711
1157.220845	117399.594571	35.225728
1158.318523	117570.897300	35.230746
1159.357679	117760.792122	35.235764
1160.719829	117938.498621	35.240781
1162.112569	118109.224863	35.245799
1163.094394	118288.273643	35.250816
1164.185401	118461.382604	35.255834
1165.299298	118640.323574	35.260852
1166.158564	118828.032128	35.265869
1167.261993	118995.255995	35.270887
1168.059377	119169.581104	35.275904
1169.239302	119343.365105	35.280922
1170.469133	119520.122973	35.285940
1171.508122	119698.890344	35.290957
1172.849825	119852.749014	35.295975
1174.302259	120045.748998	35.300992
1175.239088	120208.716750	35.306010
1176.250933	120385.068734	35.311028
1177.105270	120562.105797	35.316045
1178.737680	120735.368566	35.321063
1179.578357	120924.701232	35.326080
1181.067142	121103.594944	35.331098
1182.188287	121295.346425	35.336116
1183.204753	121472.856964	35.341133
1184.414739	121656.388924	35.346151
1185.498262	121847.743065	35.351168
1186.734356	122037.146060	35.356186
1187.841266	122221.318379	35.361204
1189.079926	122422.824821	35.366221
1190.227748	122605.191170	35.371239
1191.302748	122805.494671	35.376256
1192.725862	122997.232529	35.381274
1193.776180	123196.184484	35.386292
1194.967481	123393.580368	35.391309
1196.220971	123576.708467	35.396327
1197.211945	123783.436447	35.401344
1198.436854	123979.891194	35.406362
1199.820859	124180.724092	35.411380
1200.912006	124372.076489	35.416397
1202.277794	124568.093409	35.421415
1203.370154	124783.716417	35.426432
1204.568239	124982.298865	35.431450
1205.700025	125184.901586	35.436468
1207.088612	125381.844984	35.441485
1208.648134	125590.040955	35.446503
1209.900994	125796.129261	35.451520
1210.835060	125991.675101	35.456538
1212.305839	126198.073858	35.461556
1213.278642	126393.590174	35.466573
1214.802245	126596.316164	35.471591
1215.801353	126803.337330	35.476608
1217.101113	127002.180080	35.481626
1218.579453	127203.025765	35.486644
1219.710714	127412.452521	35.491661
1221.293963	127603.095933	35.496679
1221.820466	127809.574426	35.501696
1223.371277	128016.527957	35.506714
1224.692872	128214.827526	35.511732
1225.949340	128407.479622	35.516749
1227.439579	128613.494022	35.521767
1228.317464	128823.094374	35.526784
1229.555443	129023.529670	35.531802
1231.069055	129228.883659	35.536820
1232.306531	129435.093886	35.541837
1233.456859	129633.236613	35.546855
1234.458707	129835.856952	35.551872
1235.919482	130038.139966	35.556890
1237.119188	130238.231716	35.561908
1238.194827	130440.424664	35.566925
1239.765223	130647.641740	35.571943
1240.973163	130858.418493	35.576960
1242.010411	131056.141415	35.581978
1243.463967	131257.073654	35.586996
1244.519291	131463.410966	35.592013
1246.116998	131655.694402	35.597031
1247.380585	131861.950251	35.602048
1248.410323	132062.724169	35.607066
1249.678283	132256.394171	35.612084
1250.924215	132451.121636	35.617101
1252.098071	132643.323507	35.622119
1253.273638	132835.132600	35.627136
1254.271927	133022.732214	35.632154
1255.725101	133213.446325	35.637172
1257.086565	133403.477723	35.642189
1258.365387	133596.200247	35.647207
1259.521668	133789.666065	35.652224
1260.446540	133986.937607	35.657242
1261.746491	134184.773076	35.662260
1262.424213	134398.834800	35.667277
1263.805278	134593.220601	35.672295
1265.455719	134803.426724	35.677312
1266.482569	135007.183725	35.682330
1267.716331	135207.990687	35.687348
1268.942210	135422.428288	35.692365
1270.229375	135630.905911	35.697383
1271.616465	135852.515285	35.702400
1273.083021	136064.507216	35.707418
1274.502930	136275.593773	35.712436
1275.572353	136487.675212	35.717453
1276.840618	136706.084119	35.722471
1278.241979	136916.465897	35.727488
1279.343911	137128.113743	35.732506
1280.840321	137343.774306	35.737524
1281.712978	137567.401366	35.742541
1283.382250	137779.001447	35.747559
1284.664252	138000.599541	35.752576
1285.967123	138210.596519	35.757594
1287.271991	138433.398661	35.762612
1288.809886	138654.858274	35.767629
1290.105673	138861.445563	35.772647
1291.307216	139069.368322	35.777664
1292.948650	139298.530573	35.782682
1294.482330	139509.157123	35.787700
1295.533028	139718.921102	35.792717
1296.731996	139929.056208	35.797735
1298.416945	140150.893209	35.802752
1299.265555	140366.859389	35.807770
1300.719192	140589.661061	35.812788
1301.617332	140801.687263	35.817805
1303.486265	141021.836973	35.822823
1304.797365	141240.184036	35.827840
1305.671168	141465.212611	35.832858
1307.439424	141688.858479	35.837876
1308.555875	141908.419293	35.842893
1309.751733	142114.198606	35.847911
1311.420380	142343.929505	35.852928
1312.499874	142565.593121	35.857946
1314.032711	142780.396837	35.862964
1315.152593	143005.660485	35.867981
1316.579985	143217.525480	35.872999
1317.834495	143442.528899	35.878016
1318.886615	143654.898707	35.883034
1320.501589	143878.540425	35.888052
1321.888009	144109.605549	35.893069
1322.966007	144331.378804	35.898087
1324.575409	144555.049793	35.903104
1325.745698	144785.504562	35.908122
1327.136613	144989.589885	35.913140
1328.158301	145224.207510	35.918157
1330.051556	145443.611525	35.923175
1331.059260	145664.056245	35.928192
1332.180348	145894.879119	35.933210
1333.464578	146121.780956	35.938228
1334.977349	146340.499522	35.943245
1336.478820	146570.656651	35.948263
1337.978089	146794.913147	35.953280
1338.893655	147013.372648	35.958298
1340.693611	147210.003018	35.963316
1341.239531	147424.498556	35.968333
1342.949329	147631.489116	35.973351
1343.844558	147839.026856	35.978368
1345.295363	148072.968279	35.983386
1346.688105	148275.860463	35.988404
1348.295408	148500.716603	35.993421
1349.487026	148716.385613	35.998439
1350.758429	148946.386084	36.003456
1352.353805	149165.471589	36.008474
1353.875432	149373.691554	36.013492
1355.156706	149596.496291	36.018509
1356.294258	149815.795737	36.023527
1357.684833	150040.413018	36.028544
1358.439619	150259.545698	36.033562
1360.166407	150491.855134	36.038580
1361.262615	150730.636356	36.043597
1363.016327	150953.918532	36.048615
1364.184752	151173.561339	36.053632
1365.216600	151404.663301	36.058650
1366.870222	151640.098979	36.063668
1368.213234	151892.860368	36.068685
1369.539754	152124.820462	36.073703
1371.076191	152372.158918	36.078720
1371.849092	152613.296448	36.083738
1373.427457	152843.112925	36.088756
1374.876148	153081.772928	36.093773
1376.567398	153342.432760	36.098791
1377.806675	153573.803179	36.103808
1378.568141	153823.668481	36.108826
1380.730768	154070.192794	36.113844
1382.028678	154318.668793	36.118861
1383.472748	154555.952027	36.123879
1384.872778	154806.864144	36.128896
1386.259276	155057.741384	36.133914
1387.942157	155297.046768	36.138932
1389.651940	155552.750205	36.143949
1390.849292	155793.682350	36.148967
1392.287838	156033.117854	36.153984
1393.314270	156278.839214	36.159002
1395.181216	156524.265004	36.164020
1396.580280	156774.284376	36.169037
1397.847506	157013.331733	36.174055
1399.075590	157263.951187	36.179072
1400.684949	157513.636061	36.184090
1402.020560	157754.605295	36.189108
1403.664605	158005.150034	36.194125
1404.880322	158252.601780	36.199143
1406.479092	158499.893014	36.204160
1407.730319	158746.973051	36.209178
1409.311604	158990.968264	36.214196
1410.571299	159242.682724	36.219213
1411.920499	159495.374435	36.224231
1413.626050	159740.635387	36.229248
1414.924514	159998.402540	36.234266
1416.293471	160237.053033	36.239284
1417.852322	160483.444370	36.244301
1419.115304	160736.459289	36.249319
1420.544267	160969.694854	36.254336
1422.130221	161220.083943	36.259354
1423.857258	161480.697381	36.264372
1425.028991	161719.523985	36.269389
1426.706636	161975.208512	36.274407
1428.193303	162224.918801	36.279424
1429.776024	162465.981796	36.284442
1430.912485	162713.425428	36.289460
1432.193518	162951.630068	36.294477
1433.864512	163180.277888	36.299495
1435.048761	163407.555335	36.304512
1436.666148	163645.290872	36.309530
1438.045641	163869.670022	36.314548
1438.995964	164101.519004	36.319565
1440.783221	164334.177321	36.324583
1442.134749	164555.985813	36.329600
1443.653015	164793.575909	36.334618
1444.655629	165031.577657	36.339636
1446.033856	165273.685887	36.344653
1447.638392	165519.670079	36.349671
1449.065679	165768.780857	36.354688
1450.559338	166024.268537	36.359706
1451.668440	166254.360601	36.364724
1453.410986	166497.457256	36.369741
1454.817827	166759.131825	36.374759
1456.223745	166997.699399	36.379776
1457.354927	167261.653628	36.384794
1458.695192	167508.828961	36.389812
1460.365717	167765.615813	36.394829
1461.617779	168020.424881	36.399847
1462.820989	168286.822170	36.404864
1464.345558	168547.050175	36.409882
1466.185495	168816.549427	36.414900
1467.477156	169074.504920	36.419917
1468.750717	169348.868924	36.424935
1470.756401	169616.872333	36.429952
1471.801095	169879.999010	36.434970
1473.641317	170155.547070	36.439988
1475.207436	170420.295502	36.445005
1476.299537	170694.185023	36.450023
1478.477326	170962.712358	36.455040
1479.457371	171232.913727	36.460058
1480.910850	171497.785177	36.465076
1482.562316	171771.146650	36.470093
1483.906604	172043.833416	36.475111
1485.395674	172315.990584	36.480128
1486.985648	172593.110432	36.485146
1488.536867	172871.100786	36.490164
1490.393627	173142.352558	36.495181
1491.749281	173415.258236	36.500199
1492.896003	173688.667383	36.505216
1494.845856	173968.948348	36.510234
1496.094346	174234.419925	36.515252
1497.999041	174513.770221	36.520269
1499.284111	174786.247219	36.525287
1500.989321	175054.989620	36.530304
1502.649022	175328.628827	36.535322
1504.353658	175600.738133	36.540340
1505.769269	175877.147491	36.545357
1507.195526	176150.813275	36.550375
1509.195057	176419.501377	36.555392
1510.183429	176694.088269	36.560410
1512.081609	176965.663820	36.565428
1513.699343	177229.969824	36.570445
1514.704292	177501.178954	36.575463
1516.665792	177768.556658	36.580480
1517.935600	178042.113372	36.585498
1519.812979	178313.239315	36.590516
1521.071580	178577.808852	36.595533
1522.386956	178857.227780	36.600551
1524.404791	179122.391260	36.605568
1525.454119	179402.336106	36.610586
1526.765230	179670.532553	36.615604
1528.402651	179933.218227	36.620621
1529.926108	180222.666367	36.625639
1531.652164	180483.485731	36.630656
1532.992099	180763.922681	36.635674
1534.465063	181025.189569	36.640692
1535.629164	181281.222737	36.645709
1537.126162	181544.874751	36.650727
1538.825167	181805.651292	36.655744
1540.232469	182068.226695	36.660762
1541.450506	182335.810527	36.665780
1543.098784	182607.645510	36.670797
1544.691249	182882.994995	36.675815
1546.435016	183150.905203	36.680832
1547.845157	183421.281238	36.685850
1549.474511	183691.014144	36.690868
1550.724871	183966.039258	36.695885
1552.575585	184247.244696	36.700903
1554.111739	184518.619976	36.705920
1555.395573	184798.290155	36.710938
1557.086338	185067.712396	36.715956
1558.479996	185389.758075	36.720973
1560.076801	185717.894187	36.725991
1561.695882	186003.661815	36.731008
1562.862299	186289.475675	36.736026
1564.781274	186584.798922	36.741044
1566.446410	186866.878779	36.746061
1567.528858	187158.245226	36.751079
1569.477335	187445.082788	36.756096
1571.078366	187740.839989	36.761114
1572.587302	188037.247403	36.766132
1574.547147	188329.038475	36.771149
1575.879654	188631.037667	36.776167
1577.577503	188929.780101	36.781184
1578.859398	189228.334428	36.786202
1580.566933	189528.448535	36.791220
1582.299360	189823.631898	36.796237
1583.653567	190134.064562	36.801255
1585.328236	190427.175684	36.806272
1587.203301	190734.531192	36.811290
1588.418213	191030.586014	36.816308
1590.412590	191329.516842	36.821325
1591.925321	191632.460881	36.826343
1593.778035	191935.530273	36.831360
1595.083950	192241.022854	36.836378
1596.599161	192539.091814	36.841396
1598.672529	192837.531347	36.846413
1599.819097	193153.211429	36.851431
1601.612399	193456.751030	36.856448
1603.670136	193763.729903	36.861466
1604.962066	194068.467055	36.866484
1606.924121	194367.765804	36.871501
1608.864239	194668.745143	36.876519
1610.194089	194972.284588	36.881536
1611.878351	195265.253116	36.886554
1613.463061	195567.712557	36.891572
1615.050702	195869.511768	36.896589
1616.812350	196172.021046	36.901607
1618.232877	196468.894422	36.906624
1620.202578	196773.887179	36.911642
1621.607986	197080.797815	36.916660
1623.258388	197375.757375	36.921677
1624.606416	197678.944205	36.926695
1626.750414	197986.350791	36.931712
1628.169346	198285.717495	36.936730
1630.020754	198583.543799	36.941748
1631.374694	198884.064936	36.946765
1632.961509	199197.327405	36.951783
1634.781836	199500.088321	36.956800
1636.727587	199793.863255	36.961818
1638.312061	200098.973808	36.966836
1639.718751	200396.720727	36.971853
1641.199116	200684.651401	36.976871
1642.934478	200964.388545	36.981888
1644.715066	201253.289306	36.986906
1645.824529	201533.023733	36.991924
1647.785270	201816.892992	36.996941
1649.248619	202109.248756	37.001959
1651.010123	202397.214523	37.006976
1652.588282	202674.260968	37.011994
1654.026926	202973.861729	37.017012
1655.979360	203259.004709	37.022029
1657.291239	203556.543242	37.027047
1658.581181	203849.259172	37.032064
1660.360041	204146.242900	37.037082
1661.794575	204447.726450	37.042100
1663.780637	204746.406054	37.047117
1665.160925	205060.295585	37.052135
1666.809907	205370.129902	37.057152
1668.472414	205675.364646	37.062170
1670.004905	205990.603537	37.067188
1672.350044	206298.653695	37.072205
1673.449265	206619.931018	37.077223
1675.216394	206928.174137	37.082240
1677.335585	207247.184300	37.087258
1678.694682	207568.320708	37.092276
1680.542798	207881.125010	37.097293
1681.792212	208194.455276	37.102311
1683.548072	208505.572827	37.107328
1685.227295	208834.180203	37.112346
1686.644394	209164.912104	37.117364
1688.616213	209492.636244	37.122381
1690.280941	209832.653271	37.127399
1692.246883	210154.536391	37.132416
1694.009357	210476.350121	37.137434
1695.532607	210811.817906	37.142452
1697.106738	211139.123614	37.147469
1699.003616	211479.411178	37.152487
1700.962979	211806.454118	37.157504
1702.706234	212131.524349	37.162522
1704.132644	212465.916810	37.167540
1706.250600	212793.698077	37.172557
1707.982870	213122.302138	37.177575
1709.508006	213457.264444	37.182592
1711.326676	213785.626990	37.187610
1713.239018	214125.051194	37.192628
1715.392978	214454.784487	37.197645
1716.912321	214788.097691	37.202663
1718.608418	215115.947114	37.207680
1720.344632	215439.065422	37.212698
1721.894843	215771.536285	37.217716
1723.938153	216102.837876	37.222733
1725.810881	216435.944677	37.227751
1727.295790	216762.837653	37.232768
1729.131642	217090.844510	37.237786
1730.418856	217426.761839	37.242804
1732.882824	217754.924870	37.247821
1734.344337	218082.584469	37.252839
1736.060069	218421.102766	37.257856
1738.072575	218753.960539	37.262874
1739.029421	219088.711156	37.267892
1741.131312	219419.268928	37.272909
1742.949858	219759.321482	37.277927
1744.690832	220078.580451	37.282944
1746.682597	220422.924874	37.287962
1748.189502	220757.513954	37.292980
1750.496805	221082.476797	37.297997
1752.249712	221407.348676	37.303015
1753.798397	221737.409634	37.308032
1755.370113	222063.275413	37.313050
1756.965438	222394.574050	37.318068
1759.010251	222695.215928	37.323085
1760.348294	223004.123169	37.328103
1761.971838	223325.662421	37.333120
1763.826259	223634.082491	37.338138
1765.311623	223960.724270	37.343156
1766.955619	224276.392098	37.348173
1768.887000	224599.229740	37.353191
1770.313627	224918.335772	37.358208
1772.264187	225227.909505	37.363226
1773.866839	225577.650734	37.368244
1775.615430	225896.528555	37.373261
1777.533679	226227.700794	37.378279
1778.915018	226565.917742	37.383296
1781.081447	226900.353613	37.388314
1782.187957	227240.417174	37.393332
1784.521474	227583.718223	37.398349
1785.995666	227923.571702	37.403367
1787.957290	228273.916918	37.408384
1789.595192	228616.437445	37.413402
1791.303111	228973.401821	37.418420
1793.053614	229319.003812	37.423437
1795.132456	229672.785211	37.428455
1796.701856	230028.195838	37.433472
1798.312423	230387.156436	37.438490
1800.276707	230744.105414	37.443508
1802.112717	231096.628597	37.448525
1803.974501	231463.221367	37.453543
1805.643166	231830.809503	37.458560
1807.832480	232182.692528	37.463578
1809.968346	232550.054695	37.468596
1811.631286	232909.793241	37.473613
1813.242725	233279.802775	37.478631
1814.756107	233637.989180	37.483648
1817.125591	234008.158996	37.488666
1818.872561	234383.786137	37.493684
1820.588145	234740.237999	37.498701
1822.226630	235103.789288	37.503719
1824.411081	235468.397994	37.508736
1826.520505	235845.897803	37.513754
1827.945065	236223.606025	37.518772
1829.690803	236594.150574	37.523789
1831.745211	236963.147625	37.528807
1833.958753	237339.715071	37.533824
1835.953902	237701.328145	37.538842
1837.498706	238073.020298	37.543860
1839.575619	238451.132063	37.548877
1841.434852	238813.273213	37.553895
1843.337814	239194.586715	37.558912
1845.260769	239557.529898	37.563930
1847.277990	239933.083368	37.568948
1849.311242	240305.534609	37.573965
1851.324568	240665.235977	37.578983
1852.491547	241030.734229	37.584000
1854.688475	241395.308704	37.589018
1856.459554	241775.267442	37.594036
1858.281457	242141.652334	37.599053
1860.036205	242502.128243	37.604071
1861.917590	242884.278054	37.609088
1864.003278	243256.208631	37.614106
1865.865565	243628.732422	37.619124
1867.261270	243991.014981	37.624141
1869.432598	244365.292780	37.629159
1871.633139	244737.736344	37.634176
1873.591446	245111.741321	37.639194
1875.243619	245478.274286	37.644212
1876.834756	245852.106731	37.649229
1878.690570	246223.178966	37.654247
1880.370382	246587.190687	37.659264
1882.587444	246940.245328	37.664282
1884.345655	247300.763255	37.669300
1885.829602	247652.610327	37.674317
1887.735807	248010.284025	37.679335
1889.472044	248365.214739	37.684352
1891.551137	248718.185916	37.689370
1893.151316	249092.797884	37.694388
1895.075339	249449.094131	37.699405
1896.944746	249823.586156	37.704423
1898.492732	250183.114957	37.709440
1900.614821	250550.021355	37.714458
1902.828835	250928.241844	37.719476
1904.681492	251293.232742	37.724493
1906.559752	251671.808810	37.729511
1908.263937	252054.526289	37.734528
1910.021217	252430.376015	37.739546
1912.011735	252797.373907	37.744564
1913.908244	253193.140282	37.749581
1915.975018	253572.190098	37.754599
1917.456574	253968.654325	37.759616
1919.823904	254360.127174	37.764634
1921.577622	254741.610593	37.769652
1923.589908	255140.884223	37.774669
1925.772761	255530.629935	37.779687
1927.356490	255935.327945	37.784704
1929.115149	256321.759375	37.789722
1931.328116	256734.738840	37.794740
1932.789163	257142.271839	37.799757
1934.993316	257535.411994	37.804775
1937.102746	257941.469337	37.809792
1939.021050	258347.301258	37.814810
1941.036262	258757.104575	37.819828
1942.921744	259161.745107	37.824845
1945.053155	259570.663873	37.829863
1946.915276	259982.392005	37.834880
1948.789903	260387.715875	37.839898
1950.924258	260798.661928	37.844916
1953.011864	261209.029624	37.849933
1955.076343	261620.796454	37.854951
1956.910597	262032.775596	37.859968
1959.461590	262432.347565	37.864986
1961.095166	262846.793448	37.870004
1963.064575	263257.603859	37.875021
1965.498998	263662.929848	37.880039
1967.298463	264079.503976	37.885056
1969.564334	264483.938811	37.890074
1971.758139	264895.672920	37.895092
1973.386262	265299.239184	37.900109
1975.720041	265693.676795	37.905127
1977.444955	266113.607030	37.910144
1979.639980	266510.145853	37.915162
1981.469792	266919.007797	37.920180
1983.448852	267325.228629	37.925197
1985.696824	267731.761264	37.930215
1987.576103	268138.553053	37.935232
1989.460193	268543.970844	37.940250
1991.568118	268950.901158	37.945268
1993.578839	269359.673566	37.950285
1995.745504	269767.556240	37.955303
1997.464442	270177.818352	37.960320
1999.510702	270579.569966	37.965338
2001.787696	270980.724939	37.970356
2003.519299	271388.668373	37.975373
2006.052140	271787.011351	37.980391
2007.686082	272202.915666	37.985408
2009.473734	272605.130295	37.990426
2011.289178	273013.560963	37.995444
2013.536438	273419.636398	38.000461
2015.759278	273794.704269	38.005479
2017.476427	274183.893930	38.010496
2019.976004	274564.934056	38.015514
2021.448383	274944.863321	38.020532
2023.419069	275331.163522	38.025549
2025.361001	275718.431445	38.030567
2027.121169	276111.186101	38.035584
2029.456914	276506.997876	38.040602
2031.208662	276895.508877	38.045620
2032.923408	277291.109150	38.050637
2035.504314	277687.029028	38.055655
2037.549693	278098.775831	38.060672
2039.588931	278500.820407	38.065690
2041.338655	278899.200479	38.070708
2043.059623	279310.635996	38.075725
2045.185104	279711.822641	38.080743
2046.976192	280129.108924	38.085760
2049.228224	280546.422325	38.090778
2051.403550	280969.459115	38.095796
2052.939091	281385.178427	38.100813
2055.318630	281801.652109	38.105831
2057.211965	282237.143375	38.110848
2059.287034	282663.893473	38.115866
2061.739886	283088.575801	38.120884
2063.495480	283525.350409	38.125901
2065.582510	283950.795780	38.130919
2067.189490	284391.524189	38.135936
2069.580570	284815.545444	38.140954
2071.611160	285265.445046	38.145972
2073.624772	285714.785687	38.150989
2076.118090	286159.604587	38.156007
2078.017401	286599.155675	38.161024
2080.012879	287046.890498	38.166042
2081.897879	287495.274370	38.171060
2084.154377	287948.624642	38.176077
2086.566219	288391.206767	38.181095
2088.830876	288845.209677	38.186112
2090.793646	289292.502510	38.191130
2092.718846	289741.956329	38.196148
2094.879495	290196.727613	38.201165
2097.099198	290651.841836	38.206183
2099.410558	291106.913008	38.211200
2101.565664	291561.700597	38.216218
2103.962814	292010.378692	38.221236
2106.083240	292460.747137	38.226253
2108.337234	292916.270873	38.231271
2110.398274	293375.756752	38.236288
2112.642936	293812.893036	38.241306
2114.697743	294259.018227	38.246324
2116.680115	294715.230850	38.251341
2118.912134	295165.282150	38.256359
2121.383606	295617.475942	38.261376
2123.095597	296057.547772	38.266394
2125.901378	296513.262028	38.271412
2127.655447	296959.159671	38.276429
2129.827408	297406.003957	38.281447
2131.930682	297863.213634	38.286464
2134.233889	298323.409421	38.291482
2136.623457	298764.801316	38.296500
2138.829564	299205.380627	38.301517
2140.806782	299648.251659	38.306535
2142.995829	300100.149012	38.311552
2144.748603	300548.556767	38.316570
2147.415149	300984.327819	38.321588
2149.345448	301430.034924	38.326605
2151.536329	301868.970306	38.331623
2153.702307	302324.051216	38.336640
2155.680486	302769.663454	38.341658
2157.809687	303193.366256	38.346676
2160.108671	303612.545921	38.351693
2162.032005	304029.674039	38.356711
2164.418972	304454.976251	38.361728
2166.373730	304880.241027	38.366746
2168.711660	305297.395548	38.371764
2170.293432	305723.498562	38.376781
2172.761704	306151.540771	38.381799
2174.777270	306582.899256	38.386816
2176.519857	307019.043410	38.391834
2178.692734	307451.004376	38.396852
2180.824101	307900.329940	38.401869
2182.996297	308332.029488	38.406887
2185.314348	308779.871003	38.411904
2187.357578	309228.817451	38.416922
2190.059615	309678.316611	38.421940
2191.879346	310131.680721	38.426957
2194.246226	310580.234007	38.431975
2196.200193	311036.284368	38.436992
2198.376370	311494.123018	38.442010
2200.913196	311949.692690	38.447028
2202.729389	312415.116778	38.452045
2205.140479	312876.712278	38.457063
2207.330556	313341.561026	38.462080
2209.019268	313804.833856	38.467098
2211.694290	314269.242075	38.472116
2214.038840	314737.478780	38.477133
2216.259029	315205.019514	38.482151
2218.691468	315679.196804	38.487168
2220.712873	316157.443190	38.492186
2223.266991	316631.819798	38.497204
2225.397867	317106.993526	38.502221
2227.595972	317577.050756	38.507239
2229.780424	318049.820486	38.512256
2231.744607	318535.967897	38.517274
2233.981490	319028.081523	38.522292
2236.429909	319507.112988	38.527309
2238.782915	319993.690790	38.532327
2240.946532	320485.926159	38.537344
2243.426063	320963.033344	38.542362
2245.707165	321450.037214	38.547380
2247.879635	321937.280853	38.552397
2250.518319	322421.477081	38.557415
2252.911070	322902.026898	38.562432
2254.973951	323390.235019	38.567450
2257.781074	323869.896860	38.572468
2260.280161	324349.880425	38.577485
2262.423114	324828.620061	38.582503
2264.709172	325300.151162	38.587520
2266.843130	325789.639057	38.592538
2269.132179	326262.224169	38.597556
2271.577957	326749.241287	38.602573
2273.806059	327220.581442	38.607591
2276.065950	327695.869004	38.612608
2278.493431	328187.235333	38.617626
2280.813626	328670.924985	38.622644
2283.025805	329153.585402	38.627661
2285.026678	329623.359501	38.632679
2287.285021	330104.630965	38.637696
2289.569505	330597.257939	38.642714
2291.943026	331077.103978	38.647732
2294.160247	331560.342548	38.652749
2296.687787	332050.629685	38.657767
2299.327674	332524.352822	38.662784
2301.361423	333006.612395	38.667802
2303.693716	333479.255511	38.672820
2305.452208	333961.038580	38.677837
2308.036348	334430.586238	38.682855
2310.136806	334902.486645	38.687872
2312.161630	335363.485350	38.692890
2314.903032	335824.112550	38.697908
2317.004804	336281.003816	38.702925
2319.269141	336742.023885	38.707943
2321.762270	337207.973898	38.712960
2323.438631	337675.288577	38.717978
2326.200191	338146.993065	38.722996
2328.061715	338606.606674	38.728013
2330.486543	339080.482178	38.733031
2332.571821	339564.245526	38.738048
2335.128543	340053.939602	38.743066
2337.399778	340521.529903	38.748084
2339.530976	341020.914994	38.753101
2341.856290	341506.795389	38.758119
2344.082827	342004.680560	38.763136
2345.841444	342498.295030	38.768154
2348.487361	342987.376238	38.773172
2350.961494	343502.953840	38.778189
2353.237255	344010.794526	38.783207
2355.803152	344521.245080	38.788224
2357.794167	345031.017135	38.793242
2360.071118	345535.791795	38.798260
2362.450562	346050.255262	38.803277
2364.875766	346574.517366	38.808295
2367.405599	347096.421978	38.813312
2369.817094	347627.034558	38.818330
2372.294562	348146.065517	38.823348
2374.737220	348672.472575	38.828365
2377.106323	349206.717815	38.833383
2379.701812	349726.618238	38.838400
2381.911355	350251.236162	38.843418
2384.199509	350790.488544	38.848436
2386.682319	351321.309121	38.853453
2388.891074	351858.933401	38.858471
2391.709491	352389.455673	38.863488
2394.252653	352937.404596	38.868506
2396.456672	353458.294869	38.873524
2399.138919	353998.699266	38.878541
2401.589512	354544.606692	38.883559
2404.318881	355071.421963	38.888576
2406.321973	355623.515710	38.893594
2408.945647	356156.286748	38.898612
2411.787701	356692.538176	38.903629
2414.100262	357237.431381	38.908647
2416.517360	357773.274200	38.913664
2419.095414	358314.050878	38.918682
2421.979165	358843.844946	38.923700
2424.226217	359374.160294	38.928717
2426.283952	359907.030737	38.933735
2429.141971	360440.907216	38.938752
2431.629353	360981.168869	38.943770
2434.282531	361509.355351	38.948788
2436.570767	362052.416873	38.953805
2438.905927	362582.205495	38.958823
2441.667982	363112.754238	38.963840
2443.671123	363641.815433	38.968858
2446.354354	364170.862091	38.973876
2448.967987	364708.450836	38.978893
2450.909815	365247.756696	38.983911
2453.753505	365765.192850	38.988928
2455.938589	366318.531212	38.993946
2458.497560	366837.589216	38.998964
2461.215850	367379.217261	39.003981
2463.476121	367926.101526	39.008999
2465.931327	368444.234304	39.014016
2468.487376	368987.605595	39.019034
2470.797762	369502.852911	39.024052
2473.499709	370013.468558	39.029069
2475.814964	370520.841401	39.034087
2478.316171	371023.513769	39.039104
2480.217172	371529.970214	39.044122
2482.675013	372038.103909	39.049140
2485.235703	372555.358667	39.054157
2487.912044	373070.862773	39.059175
2490.088140	373579.822860	39.064192
2492.408023	374105.218804	39.069210
2494.808175	374624.283753	39.074228
2497.189777	375155.400727	39.079245
2499.533492	375693.074613	39.084263
2501.848339	376223.598360	39.089280
2504.531411	376767.708315	39.094298
2506.818576	377310.425210	39.099316
2509.148984	377849.856530	39.104333
2511.522868	378400.263783	39.109351
2514.178276	378948.031854	39.114368
2516.326511	379504.708051	39.119386
2519.344113	380067.872802	39.124404
2521.647268	380625.767467	39.129421
2524.284710	381195.046341	39.134439
2526.542688	381762.877768	39.139456
2528.688675	382337.350007	39.144474
2531.298504	382917.030190	39.149492
2533.759357	383503.710611	39.154509
2536.184412	384092.763798	39.159527
2538.868585	384671.227698	39.164544
2541.626662	385269.141301	39.169562
2544.423408	385860.830431	39.174580
2546.977763	386453.176682	39.179597
2548.988023	387056.204229	39.184615
2552.307295	387653.821530	39.189632
2554.985272	388249.499116	39.194650
2557.985743	388838.705849	39.199668
2560.595469	389438.518174	39.204685
2563.219673	390029.375876	39.209703
2565.944697	390626.583976	39.214720
2568.513626	391225.928671	39.219738
2571.045298	391810.630875	39.224756
2573.937697	392405.136256	39.229773
2576.368555	392999.294181	39.234791
2579.520252	393588.261586	39.239808
2581.602929	394192.773404	39.244826
2584.083732	394777.361118	39.249844
2587.114972	395374.454775	39.254861
2589.775580	395966.073127	39.259879
2592.140367	396552.457963	39.264896
2594.451123	397156.858870	39.269914
2597.141458	397756.831351	39.274932
2600.046552	398347.592426	39.279949
2602.405741	398954.116215	39.284967
2605.311698	399551.123605	39.289984
2607.967026	400149.521523	39.295002
2610.607639	400746.235939	39.300020
2613.313169	401344.038296	39.305037
2616.005255	401953.215269	39.310055
2618.575285	402536.228592	39.315072
2621.302878	403140.408385	39.320090
2623.932809	403733.756950	39.325108
2626.469529	404322.094345	39.330125
2629.043654	404929.286978	39.335143
2631.925817	405514.958284	39.340160
2634.946590	406125.945378	39.345178
2637.565731	406720.482054	39.350196
2640.267074	407314.484005	39.355213
2642.393411	407916.352439	39.360231
2644.874109	408489.004161	39.365248
2647.718474	409070.185738	39.370266
2650.376149	409621.832953	39.375284
2652.697951	410185.762814	39.380301
2655.166851	410740.700048	39.385319
2657.871576	411314.609011	39.390336
2660.417393	411874.463363	39.395354
2663.038483	412452.857907	39.400372
2665.352501	413027.490862	39.405389
2668.079003	413613.628394	39.410407
2670.451140	414190.902274	39.415424
2673.320957	414774.001102	39.420442
2675.908757	415360.415981	39.425460
2678.886015	415949.839245	39.430477
2680.813331	416549.374589	39.435495
2683.786482	417151.511182	39.440512
2686.103230	417743.769522	39.445530
2689.083858	418352.799611	39.450548
2691.230516	418968.112455	39.455565
2693.878188	419575.742891	39.460583
2696.719741	420206.588003	39.465600
2699.280218	420835.333946	39.470618
2701.854516	421459.052348	39.475636
2705.152225	422088.099909	39.480653
2707.656987	422717.555585	39.485671
2710.458795	423352.911924	39.490688
2713.386865	423983.779272	39.495706
2716.042024	424624.781773	39.500724
2718.784662	425250.431024	39.505741
2721.331376	425894.342650	39.510759
2724.219394	426541.516959	39.515776
2727.037221	427191.310163	39.520794
2729.990197	427842.274363	39.525812
2732.720155	428486.781704	39.530829
2735.465581	429139.454633	39.535847
2738.127766	429780.948124	39.540864
2740.651079	430433.208691	39.545882
2743.625902	431092.958600	39.550900
2746.750496	431746.345110	39.555917
2749.488360	432403.308084	39.560935
2752.292335	433048.665175	39.565952
2755.437186	433712.999995	39.570970
2758.231316	434360.892324	39.575988
2760.899515	435017.929182	39.581005
2764.151170	435671.011916	39.586023
2767.066321	436323.417596	39.591040
2769.585979	436964.746574	39.596058
2772.540269	437617.101888	39.601076
2775.605986	438263.505928	39.606093
2778.509707	438909.660606	39.611111
2781.507788	439554.515359	39.616128
2784.524363	440197.172755	39.621146
2787.382470	440832.507773	39.626164
2790.110564	441469.508574	39.631181
2792.749197	442117.261232	39.636199
2795.523927	442759.161039	39.641216
2798.612396	443399.878293	39.646234
2801.506222	444035.350775	39.651252
2804.558205	444665.978357	39.656269
2807.021578	445312.535203	39.661287
2809.719497	445946.305481	39.666304
2812.570005	446578.565317	39.671322
2815.324627	447213.595718	39.676340
2818.811654	447837.682584	39.681357
2821.436232	448484.909498	39.686375
2824.286288	449113.243162	39.691392
2826.688649	449744.452528	39.696410
2829.672998	450377.618831	39.701428
2832.663025	451002.128027	39.706445
2835.428727	451613.018583	39.711463
2837.986916	452197.465608	39.716480
2840.963280	452797.528805	39.721498
2843.593855	453390.911441	39.726516
2846.683156	453988.240902	39.731533
2849.778939	454588.325452	39.736551
2852.082705	455181.446392	39.741568
2855.159069	455779.776907	39.746586
2857.787523	456399.507714	39.751604
2860.797918	456994.626925	39.756621
2863.137639	457608.959157	39.761639
2866.224091	458203.974472	39.766656
2868.746698	458816.216425	39.771674
2871.521194	459451.409586	39.776692
2874.576483	460064.785415	39.781709
2876.908504	460696.620556	39.786727
2879.845103	461336.714161	39.791744
2882.608715	461967.122768	39.796762
2885.670491	462606.947142	39.801780
2888.329125	463243.581293	39.806797
2891.354387	463903.695437	39.811815
2894.336323	464546.435491	39.816832
2897.378715	465207.202083	39.821850
2899.893488	465865.502775	39.826868
2902.997351	466515.462923	39.831885
2905.982086	467184.231420	39.836903
2909.075761	467841.758133	39.841920
2912.172703	468513.683646	39.846938
2914.702115	469178.710319	39.851956
2917.669816	469842.885073	39.856973
2920.964599	470522.111529	39.861991
2923.785538	471189.280617	39.867008
2926.619286	471866.506082	39.872026
2929.591172	472551.346539	39.877044
2932.465992	473229.063491	39.882061
2935.623198	473910.590390	39.887079
2938.639362	474590.497127	39.892096
2941.682977	475289.378274	39.897114
2943.947571	475971.058318	39.902132
2947.093611	476670.115301	39.907149
2950.190260	477363.906629	39.912167
2953.188023	478058.540111	39.917184
2956.237214	478751.975781	39.922202
2959.354807	479451.066051	39.927220
2961.905189	480142.351293	39.932237
2965.042001	480847.475238	39.937255
2967.671738	481552.092397	39.942272
2970.888910	482249.480207	39.947290
2973.772844	482975.411426	39.952308
2976.676782	483689.211858	39.957325
2979.658951	484403.773412	39.962343
2982.221690	485121.289918	39.967360
2985.037581	485833.493542	39.972378
2988.150531	486562.848150	39.977396
2991.169032	487286.741894	39.982413
2993.767542	488020.742337	39.987431
2996.944556	488755.977074	39.992448
3000.393978	489480.454842	39.997466
3003.195660	490219.052275	40.002484
3006.135287	490946.662438	40.007501
3009.469869	491686.716428	40.012519
3012.074612	492414.005798	40.017536
3015.226237	493148.577185	40.022554
3017.654359	493888.915909	40.027572
3021.082920	494626.392621	40.032589
3024.388913	495370.347268	40.037607
3027.383875	496114.766315	40.042624
3030.380174	496840.116506	40.047642
3033.221435	497542.196068	40.052660
3036.351241	498245.606525	40.057677
3039.218861	498947.262303	40.062695
3041.932469	499641.810903	40.067712
3045.328336	500342.259893	40.072730
3047.880283	501058.108117	40.077748
3050.426741	501763.302229	40.082765
3053.694662	502487.221910	40.087783
3056.787566	503209.572519	40.092800
3059.927480	503933.540108	40.097818
3062.683638	504673.029622	40.102836
3065.562757	505405.517891	40.107853
3068.872102	506149.624542	40.112871
3071.795553	506888.318892	40.117888
3074.769811	507630.589077	40.122906
3077.818697	508380.907988	40.127924
3080.786691	509130.696577	40.132941
3083.799080	509889.945171	40.137959
3087.036434	510664.056115	40.142976
3090.120032	511424.417519	40.147994
3093.019592	512190.751089	40.153012
3096.130857	512970.688233	40.158029
3099.605176	513755.151159	40.163047
3102.621320	514528.377493	40.168064
3105.726386	515299.334163	40.173082
3108.276445	516088.485009	40.178100
3111.500836	516878.993272	40.183117
3115.241545	517673.346644	40.188135
3117.898665	518479.737117	40.193152
3121.532261	519277.482222	40.198170
3124.757871	520079.064215	40.203188
3127.723998	520869.782844	40.208205
3130.853022	521680.583092	40.213223
3133.507601	522494.273132	40.218240
3136.824130	523296.905589	40.223258
3139.876171	524111.691417	40.228276
3143.110349	524926.348689	40.233293
3146.315473	525752.315396	40.238311
3149.281151	526570.732097	40.243328
3152.492541	527401.769491	40.248346
3156.148674	528227.962978	40.253364
3159.496777	529059.527255	40.258381
3162.703704	529887.695588	40.263399
3165.538467	530699.998871	40.268416
3169.158038	531525.989661	40.273434
3172.239085	532365.570780	40.278452
3175.264646	533193.707521	40.283469
3178.735240	534021.721552	40.288487
3181.890222	534863.237516	40.293504
3185.186633	535689.665092	40.298522
3188.286483	536526.963677	40.303540
3191.485492	537355.507605	40.308557
3194.981494	538192.434033	40.313575
3197.954450	539024.016579	40.318592
3201.557427	539854.090904	40.323610
3205.083760	540697.672450	40.328628
3208.276490	541523.736341	40.333645
3211.570215	542350.432555	40.338663
3214.522972	543177.779736	40.343680
3217.970549	543989.040215	40.348698
3220.834905	544826.526728	40.353716
3224.640893	545661.752764	40.358733
3227.267030	546483.061737	40.363751
3230.592458	547313.987541	40.368768
3234.109105	548132.890573	40.373786
3237.650046	548981.575127	40.378804
3240.001643	549793.427929	40.383821
3243.592126	550602.375415	40.388839
3247.204188	551406.552513	40.393856
3250.285700	552197.522914	40.398874
3253.290577	552988.002443	40.403892
3256.287638	553766.399959	40.408909
3259.561548	554557.135695	40.413927
3262.516359	555344.611197	40.418944
3265.426689	556138.557738	40.423962
3268.682268	556945.428318	40.428980
3271.819080	557740.435819	40.433997
3274.895536	558549.330604	40.439015
3278.114310	559360.603302	40.444032
3281.394490	560193.506023	40.449050
3284.390444	561022.887365	40.454068
3287.116376	561855.959719	40.459085
3290.776130	562685.620996	40.464103
3293.976640	563533.127409	40.469120
3297.314432	564371.385046	40.474138
3300.721289	565218.586506	40.479156
3303.856560	566076.936330	40.484173
3307.020350	566936.620244	40.489191
3310.211366	567817.616589	40.494208
3313.510044	568683.408276	40.499226
3316.961488	569562.928568	40.504244
3319.794264	570442.478108	40.509261
3323.923132	571315.300092	40.514279
3327.072743	572209.280457	40.519296
3330.195213	573085.477592	40.524314
3333.621641	574000.894617	40.529332
3336.985739	574887.173708	40.534349
3340.814402	575779.364961	40.539367
3343.816453	576682.071494	40.544384
3347.516576	577571.588796	40.549402
3351.206013	578483.498098	40.554420
3354.327417	579386.167852	40.559437
3358.442977	580286.308184	40.564455
3361.521310	581185.787434	40.569472
3365.105197	582073.662603	40.574490
3368.446322	582981.856052	40.579508
3371.867504	583881.411999	40.584525
3375.537413	584775.105769	40.589543
3378.782690	585676.191769	40.594560
3382.475468	586579.232920	40.599578
3385.759076	587484.812294	40.604596
3388.972746	588387.728134	40.609613
3392.932480	589282.705862	40.614631
3396.352227	590197.382494	40.619648
3399.590014	591086.376815	40.624666
3403.269441	591988.268840	40.629684
3406.371188	592889.475823	40.634701
3409.697810	593796.915861	40.639719
3413.257843	594706.589797	40.644736
3416.691835	595617.054656	40.649754
3420.404101	596522.703299	40.654772
3423.682872	597431.538110	40.659789
3427.470711	598321.190516	40.664807
3430.332555	599229.735579	40.669824
3434.137222	600129.517486	40.674842
3437.842130	601026.242379	40.679860
3440.807497	601931.691183	40.684877
3444.575222	602836.187119	40.689895
3448.031261	603749.885785	40.694912
3451.350173	604648.205107	40.699930
3454.925071	605556.785142	40.704948
3458.401808	606462.556203	40.709965
3462.009597	607357.849874	40.714983
3464.973803	608260.349410	40.720000
3468.678420	609164.149948	40.725018
3471.768776	610055.499055	40.730023
3474.878207	610898.246103	40.735028
3478.425745	611699.008136	40.740032
3481.851340	612466.331167	40.745037
3484.973289	613172.707372	40.750042
3487.697330	613816.414696	40.755047
3490.851478	614407.981924	40.760052
3493.515666	614939.465280	40.765056
3495.734196	615424.311291	40.770061
3498.209789	615852.321835	40.775066
3500.605849	616223.057055	40.780071
3502.312216	616548.262138	40.785076
3504.482782	616829.060376	40.790080
3506.531465	617082.286812	40.795085
3508.008169	617270.038121	40.800090
3509.709799	617417.227174	40.805095
3510.879313	617539.613757	40.810100
3512.475872	617609.017663	40.815104
3513.851504	617655.171353	40.820109
3514.667762	617664.687149	40.825114
3516.044512	617654.528547	40.830119
3516.521664	617620.576657	40.835124
3517.530078	617535.525536	40.840128
3518.219177	617446.826027	40.845133
3518.819339	617339.651538	40.850138
3519.724830	617216.987919	40.855143
3520.221872	617063.855481	40.860148
3520.870579	616894.506687	40.865152
3521.143452	616718.467697	40.870157
3521.596244	616523.807932	40.875162
3521.819295	616315.637622	40.880167
3521.718732	616107.163752	40.885172
3522.153204	615865.368419	40.890176
3522.177582	615638.274448	40.895181
3522.609182	615394.369194	40.900186
3522.670380	615146.867461	40.905191
3522.747578	614888.311524	40.910196
3522.894416	614625.739533	40.915200
3522.976869	614356.672991	40.920205
3522.958546	614089.314465	40.925210
3523.201328	613800.664199	40.930215
3522.947389	613527.179359	40.935220
3523.103350	613241.125956	40.940224
3523.240201	612955.767287	40.945229
3523.559908	612672.971507	40.950234
3523.330656	612380.655067	40.955239
3522.491303	612082.426269	40.960244
3522.717073	611792.021447	40.965248
3522.831385	611491.526349	40.970253
3522.386480	611193.309697	40.975258
3522.486878	610899.699018	40.980263
3522.347545	610609.067403	40.985268
3522.312826	610315.160946	40.990272
3521.824949	610028.717453	40.995277
3521.858945	609737.883836	41.000282
3521.675910	609435.174174	41.005287
3521.207813	609164.155440	41.010292
3521.039664	608860.476234	41.015296
3520.959390	608592.232249	41.020301
3520.559672	608300.525263	41.025306
3520.872467	608028.053985	41.030311
3520.242538	607748.220536	41.035316
3520.279620	607466.924719	41.040320
3519.487550	607186.751165	41.045325
3519.665038	606920.473833	41.050330
3519.499126	606653.342910	41.055335
3519.275368	606394.567746	41.060340
3518.959181	606119.943166	41.065344
3518.513248	605861.339389	41.070349
3518.091737	605614.981600	41.075354
3518.252978	605355.019554	41.080359
3517.434038	605101.557767	41.085364
3517.737412	604849.665334	41.090368
3517.219192	604612.604189	41.095373
3516.880687	604378.261252	41.100378
3516.918718	604132.596754	41.105383
3516.511181	603902.806830	41.110388
3516.338497	603678.028635	41.115392
3516.318620	603457.424712	41.120397
3515.901718	603227.170943	41.125402
3515.788242	603007.022410	41.130407
3515.771446	602789.856457	41.135412
3515.488272	602568.774417	41.140416
3514.818868	602362.710442	41.145421
3514.739669	602152.546725	41.150426
3514.721705	601945.571972	41.155431
3514.146397	601748.538977	41.160436
3514.616331	601537.876660	41.165440
3514.067279	601342.433334	41.170445
3513.730338	601144.250635	41.175450
3513.787591	600941.298017	41.180455
3513.117723	600757.123459	41.185460
3513.581365	600561.657351	41.190464
3513.124306	600381.196653	41.195469
3513.176506	600204.056749	41.200474
3513.148528	600023.222490	41.205479
3512.594615	599831.405502	41.210484
3512.477823	599651.930163	41.215488
3512.194551	599478.184073	41.220493
3512.519405	599303.739366	41.225498
3512.295151	599138.487951	41.230503
3511.854190	598971.215449	41.235508
3512.040302	598797.635006	41.240512
3511.843678	598626.864790	41.245517
3511.463736	598471.939434	41.250522
3511.121410	598315.954640	41.255527
3511.258622	598147.677555	41.260532
3511.027996	597995.174854	41.265536
3510.832879	597847.570567	41.270541
3510.712524	597695.296602	41.275546
3510.987334	597534.547835	41.280551
3510.485636	597387.535743	41.285556
3510.512448	597250.702479	41.290560
3510.091824	597110.833267	41.295565
3510.024504	596960.693268	41.300570
3510.009527	596819.304833	41.305575
3509.996010	596689.830582	41.310580
3509.699246	596544.827529	41.315584
3509.913344	596411.258683	41.320589
3509.521350	596277.832972	41.325594
3509.631337	596139.570355	41.330599
3509.216931	596017.811424	41.335604
3509.181657	595886.478097	41.340608
3509.107893	595757.953242	41.345613
3508.742181	595638.285398	41.350618
3508.663977	595511.661042	41.355623
3508.619596	595390.688320	41.360628
3508.666004	595278.363030	41.365632
3508.523951	595162.510641	41.370637
3508.624795	595047.770770	41.375642
3508.380903	594920.063584	41.380647
3508.183280	594814.131291	41.385652
3508.150320	594688.641830	41.390656
3508.337018	594588.055618	41.395661
3507.802755	594473.909624	41.400666
3507.760604	594362.439844	41.405671
3507.461992	594256.918424	41.410676
3507.824900	594159.055011	41.415680
3507.689123	594066.426986	41.420685
3507.586946	593967.682985	41.425690
3507.228994	593851.699829	41.430695
3507.204513	593767.715967	41.435700
3507.924587	593664.934207	41.440704
3507.197161	593562.778409	41.445709
3507.188519	593454.098552	41.450714
3506.896577	593362.290163	41.455719
3506.433887	593269.055224	41.460724
3506.642047	593178.769784	41.465728
3506.271094	593098.390854	41.470733
3506.672134	593014.134201	41.475738
3506.752253	592918.156797	41.480743
3506.748039	592843.378360	41.485748
3507.002778	592746.320298	41.490752
3506.855148	592661.695860	41.495757
3506.477878	592564.284161	41.500762
3506.658751	592479.707106	41.505767
3506.381804	592402.413720	41.510772
3506.280570	592314.874145	41.515776
3506.023368	592227.758952	41.520781
3505.762108	592154.869199	41.525786
3506.227501	592071.045877	41.530791
3506.103757	592004.094331	41.535796
3506.050477	591902.668813	41.540800
3506.096214	591830.079496	41.545805
3505.518573	591751.225496	41.550810
3505.943788	591672.715062	41.555815
3505.811649	591603.357908	41.560820
3505.990997	591521.829172	41.565824
3505.788501	591445.719474	41.570829
3505.660319	591374.556872	41.575834
3505.282989	591296.469709	41.580839
3505.155945	591234.372975	41.585844
3505.263263	591164.274234	41.590848
3505.063001	591098.531267	41.595853
3505.346413	591030.508105	41.600858
3505.345565	590963.831429	41.605863
3505.284777	590898.366007	41.610868
3505.303280	590835.743261	41.615872
3504.992623	590763.052160	41.620877
3505.319822	590703.436260	41.625882
3505.171019	590629.015668	41.630887
3505.080946	590569.764841	41.635892
3505.193505	590508.377916	41.640896
3504.728496	590433.754918	41.645901
3505.003348	590374.997047	41.650906
3504.752423	590311.110818	41.655911
3504.741924	590246.284848	41.660916
3504.771830	590186.161476	41.665920
3504.362336	590132.268666	41.670925
3504.411835	590079.205624	41.675930
3504.901404	590026.424223	41.680935
3504.244007	589972.719668	41.685940
3504.260400	589907.336356	41.690944
3504.271493	589853.426502	41.695949
3504.623877	589808.881967	41.700954
3504.747845	589742.128118	41.705959
3504.320384	589690.139745	41.710964
3504.337384	589632.269862	41.715968
3504.185535	589587.502630	41.720973
3504.134020	589534.903619	41.725978
3504.081712	589480.400589	41.730983
3504.169806	589443.511404	41.735988
3504.240707	589392.145121	41.740992
3504.040436	589333.405754	41.745997
3504.004402	589287.366600	41.751002
3504.507111	589234.479073	41.756007
3503.981103	589189.367855	41.761012
3503.880860	589131.263099	41.766016
3503.662480	589081.694198	41.771021
3503.822559	589037.827904	41.776026
3504.093126	588993.743741	41.781031
3503.998617	588961.691490	41.786036
3503.888720	588901.081773	41.791040
3504.430501	588857.305391	41.796045
3504.110667	588814.314897	41.801050
3504.265126	588759.876124	41.806055
3504.200855	588719.701320	41.811060
3504.110463	588650.619272	41.816064
3504.199259	588607.964926	41.821069
3503.551320	588548.439471	41.826074
3503.772002	588502.908019	41.831079
3504.127972	588470.383036	41.836084
3503.664889	588418.093468	41.841088
3503.538668	588380.532663	41.846093
3503.940734	588339.582045	41.851098
3504.182563	588287.532402	41.856103
3503.532576	588245.192552	41.861108
3503.442496	588197.303215	41.866112
3503.739136	588161.279007	41.871117
3503.670080	588115.841333	41.876122
3503.672373	588068.187529	41.881127
3503.541171	588038.844157	41.886132
3503.890144	587988.029051	41.891136
3503.878972	587941.128430	41.896141
3503.403227	587898.459328	41.901146
3503.423995	587860.973964	41.906151
3503.424437	587821.387031	41.911156
3503.494148	587783.743419	41.916160
3503.322562	587747.039383	41.921165
3503.180058	587706.271730	41.926170
3503.639732	587664.407574	41.931175
3502.948777	587625.479228	41.936180
3503.195590	587584.399702	41.941184
3503.434553	587552.040596	41.946189
3503.673890	587514.569979	41.951194
3503.666117	587474.832733	41.956199
3503.790100	587444.696189	41.961204
3503.737014	587384.770677	41.966208
3503.402700	587336.715276	41.971213
3503.430704	587307.445263	41.976218
3503.547046	587256.813443	41.981223
3503.547665	587231.706846	41.986228
3503.351663	587183.629146	41.991232
3503.750137	587153.348659	41.996237
3503.681346	587112.617368	42.001242
3503.404017	587058.788810	42.006247
3503.628844	587026.781147	42.011252
3503.207436	586986.254847	42.016256
3503.699254	586947.289508	42.021261
3503.223004	586913.486779	42.026266
3503.452488	586878.270647	42.031271
3503.373470	586834.432828	42.036276
3503.203029	586794.568183	42.041280
3503.143270	586751.478739	42.046285
3503.385461	586724.879877	42.051290
3503.477642	586690.285982	42.056295
3503.212325	586649.082527	42.061300
3503.151430	586611.755969	42.066304
3503.333362	586579.152311	42.071309
3503.386115	586544.012843	42.076314
3503.269027	586495.168027	42.081319
3503.172388	586469.122671	42.086324
3503.001183	586436.022512	42.091328
3502.933727	586395.238212	42.096333
3503.024983	586366.857879	42.101338
3503.396783	586340.187702	42.106343
3502.984215	586300.308983	42.111348
3503.113592	586261.999260	42.116352
3503.052882	586235.647027	42.121357
3502.677315	586209.895241	42.126362
3502.844332	586179.197178	42.131367
3502.677465	586141.785342	42.136372
3503.077061	586106.640362	42.141376
3502.864689	586079.960636	42.146381
3502.918098	586056.597207	42.151386
3503.000721	586021.050440	42.156391
3502.829276	585989.302154	42.161396
3503.107932	585947.359468	42.166400
3502.743811	585906.569600	42.171405
3502.885302	585893.767101	42.176410
3503.094956	585852.837216	42.181415
3502.801392	585831.482187	42.186420
3503.025629	585805.886275	42.191424
3502.659625	585774.969687	42.196429
3502.676062	585746.148363	42.201434
3503.227007	585706.718281	42.206439
3502.867452	585693.442560	42.211444
3503.333848	585651.218791	42.216448
3503.310164	585624.107494	42.221453
3502.928276	585589.183259	42.226458
3503.369684	585554.180328	42.231463
3503.026667	585513.937016	42.236468
3502.961788	585480.215889	42.241472
3503.150106	585451.417038	42.246477
3502.886204	585418.729250	42.251482
3502.966451	585381.827510	42.256487
3502.702944	585360.567102	42.261492
3502.714807	585331.294308	42.266496
3502.736329	585302.771748	42.271501
3502.473969	585276.599088	42.276506
3502.961966	585240.034100	42.281511
3502.520829	585214.540822	42.286516
3502.708013	585181.029977	42.291520
3503.148316	585163.067459	42.296525
3502.812641	585137.808127	42.301530
3503.212154	585087.121973	42.306535
3502.960622	585062.851763	42.311540
3502.846105	585028.936513	42.316544
3502.540469	584995.953248	42.321549
3502.467644	584973.760065	42.326554
3502.590422	584947.777025	42.331559
3502.173670	584922.379499	42.336564
3502.647961	584911.478634	42.341568
3502.639705	584886.668769	42.346573
3502.436237	584855.273057	42.351578
3502.869837	584826.283848	42.356583
3502.923413	584806.075513	42.361588
3502.770530	584770.361003	42.366592
3502.644355	584742.311188	42.371597
3503.001591	584712.481508	42.376602
3503.216829	584696.157386	42.381607
3502.895300	584662.674358	42.386612
3502.566815	584624.781349	42.391616
3502.140149	584600.888364	42.396621
3502.312325	584576.450588	42.401626
3502.777194	584546.002131	42.406631
3502.442859	584518.936659	42.411636
3502.412287	584495.131898	42.416640
3502.542624	584476.715464	42.421645
3502.635275	584444.670779	42.426650
3502.817052	584424.592077	42.431655
3502.712293	584406.061899	42.436660
3502.682771	584367.068624	42.441664
3502.732119	584343.100662	42.446669
3502.529892	584318.821094	42.451674
3503.052043	584288.112338	42.456679
3502.681715	584257.994152	42.461684
3502.600088	584227.229235	42.466688
3502.429962	584198.082116	42.471693
3502.280154	584183.267969	42.476698
3502.310573	584147.422521	42.481703
3502.117239	584126.299123	42.486708
3502.251430	584097.555306	42.491712
3502.718550	584087.907923	42.496717
3502.457226	584062.283595	42.501722
3502.239976	584024.421247	42.506727
3502.345275	584013.326542	42.511732
3502.842231	583987.633626	42.516736
3502.221336	583977.003301	42.521741
3502.393110	583944.644022	42.526746
3502.478888	583923.727240	42.531751
3502.114657	583903.231663	42.536756
3502.462815	583874.102917	42.541760
3502.522780	583847.224786	42.546765
3502.361593	583827.248735	42.551770
3502.453870	583804.676477	42.556775
3502.075757	583782.277966	42.561780
3502.289590	583768.759881	42.566784
3502.289049	583745.099184	42.571789
3502.315509	583721.534472	42.576794
3502.248067	583696.430395	42.581799
3502.337011	583680.525540	42.586804
3502.601024	583656.522522	42.591808
3502.382344	583636.354595	42.596813
3502.385013	583614.999056	42.601818
3502.922000	583593.008524	42.606823
3502.490216	583572.372501	42.611828
3502.793822	583543.350103	42.616832
3502.757504	583519.694514	42.621837
3502.449000	583502.046865	42.626842
3502.697599	583461.753655	42.631847
3502.905539	583438.210096	42.636852
3502.601205	583408.730951	42.641856
3502.928107	583381.108129	42.646861
3502.607335	583359.201093	42.651866
3502.978689	583327.310103	42.656871
3502.516314	583306.778623	42.661876
3502.634197	583274.876975	42.666880
3502.986710	583244.893661	42.671885
3502.845516	583211.979583	42.676890
3502.755451	583181.513842	42.681895
3502.443971	583144.515423	42.686900
3502.457925	583131.128065	42.691904
3502.310377	583096.961350	42.696909
3502.386883	583071.031238	42.701914
3502.538640	583051.656567	42.706919
3502.739314	583036.535423	42.711924
3502.420223	583011.268595	42.716928
3502.929818	582986.473747	42.721933
3503.165757	582958.412897	42.726938
3502.800326	582929.844399	42.731943
3502.710160	582890.855368	42.736948
3502.678999	582873.464148	42.741952
3503.233955	582845.202741	42.746957
3502.719832	582806.881282	42.751962
3502.702951	582773.144331	42.756967
3502.628820	582742.223686	42.761972
3502.388602	582721.505982	42.766976
3502.492454	582692.362173	42.771981
3502.688790	582672.829467	42.776986
3502.445736	582635.969042	42.781991
3502.499095	582627.538146	42.786996
3502.507521	582593.796690	42.792001
3502.541565	582573.386770	42.797005
3502.393388	582555.311464	42.802010
3502.842716	582519.294957	42.807015
3502.587387	582494.768988	42.812020
3502.359301	582473.347040	42.817025
3502.537300	582435.517702	42.822029
3502.119120	582423.450404	42.827034
3502.775850	582398.430697	42.832039
3502.147082	582373.010275	42.837044
3502.384647	582352.167051	42.842049
3502.511157	582324.823587	42.847053
3502.231112	582317.447277	42.852058
3502.937691	582284.347761	42.857063
3502.380613	582259.517493	42.862068
3502.437276	582241.860869	42.867073
3502.401059	582213.640131	42.872077
3501.996440	582198.010837	42.877082
3502.378853	582174.537578	42.882087
3502.882948	582164.230978	42.887092
3502.181065	582126.237316	42.892097
3502.209889	582104.924897	42.897101
3502.263572	582082.756236	42.902106
3502.584822	582061.197474	42.907111
3502.117831	582042.920486	42.912116
3502.509868	582015.033383	42.917121
3502.227565	581994.721983	42.922125
3502.643103	581974.802821	42.927130
3502.723304	581933.627895	42.932135
3502.382731	581910.317236	42.937140
3502.314464	581882.501757	42.942145
3502.022472	581858.882573	42.947149
3501.750151	581853.510231	42.952154
3502.089645	581829.491441	42.957159
3502.203766	581824.309360	42.962164
3502.796781	581804.562697	42.967169
3502.614061	581777.918009	42.972173
3502.768020	581751.521450	42.977178
3502.594432	581722.318177	42.982183
3502.051348	581704.403488	42.987188
3501.778915	581672.207259	42.992193
3501.976671	581666.410374	42.997197
3501.839655	581652.192475	43.002202
3502.360978	581627.493026	43.007207
3502.362611	581607.337079	43.012212
3502.404891	581580.055080	43.017217
3502.145036	581561.093111	43.022221
3501.995738	581547.879769	43.027226
3502.471390	581526.396107	43.032231
3501.981116	581511.932420	43.037236
3501.773352	581490.003996	43.042241
3501.575287	581450.425077	43.047245
3501.606430	581451.523176	43.052250
3501.931988	581444.903970	43.057255
3501.696898	581427.893326	43.062260
3501.738987	581406.226512	43.067265
3501.817512	581407.668183	43.072269
3501.902475	581389.253685	43.077274
3502.277812	581364.225497	43.082279
3502.148665	581362.189876	43.087284
3502.103753	581332.163225	43.092289
3502.400059	581315.119474	43.097293
3502.219602	581290.930102	43.102298
3502.128482	581268.682166	43.107303
3501.632256	581256.525508	43.112308
3501.746472	581239.810947	43.117313
3502.050506	581231.740920	43.122317
3501.917206	581212.708429	43.127322
3502.003688	581190.382432	43.132327
3501.816918	581181.436430	43.137332
3501.918771	581158.907405	43.142337
3501.905135	581151.839648	43.147341
3501.956592	581128.014788	43.152346
3502.091495	581117.915356	43.157351
3502.126253	581096.951052	43.162356
3501.853647	581086.915297	43.167361
3502.292809	581065.987996	43.172365
3501.938749	581052.204383	43.177370
3502.322215	581035.347140	43.182375
3502.219080	581012.699441	43.187380
3502.410789	581012.017546	43.192385
3502.349629	580979.585708	43.197389
3502.078235	580954.908405	43.202394
3502.068931	580927.833428	43.207399
3502.046764	580922.120676	43.212404
3502.047901	580901.211399	43.217409
3502.031004	580874.488470	43.222413
3501.991004	580858.198575	43.227418
3501.895632	580827.877595	43.232423
3502.064984	580833.517059	43.237428
3502.256740	580793.473716	43.242433
3501.851287	580787.369535	43.247437
3501.882233	580769.664441	43.252442
3502.118791	580761.303769	43.257447
3501.716095	580740.958742	43.262452
3501.700883	580717.845414	43.267457
3501.896333	580712.299104	43.272461
3501.938694	580696.196666	43.277466
3501.959625	580675.835437	43.282471
3501.988341	580666.955617	43.287476
3502.115169	580646.828493	43.292481
3502.226747	580628.408571	43.297485
3501.901714	580612.413588	43.302490
3502.160226	580581.083896	43.307495
3502.286408	580573.592769	43.312500
3502.292240	580554.637683	43.317505
3502.241708	580533.234358	43.322509
3502.346200	580521.133409	43.327514
3502.255407	580493.869539	43.332519
3501.950645	580477.470044	43.337524
3502.042072	580447.870975	43.342529
3502.159483	580434.363891	43.347533
3501.927067	580419.858461	43.352538
3502.321667	580393.822201	43.357543
3502.166276	580379.705827	43.362548
3502.178833	580358.643311	43.367553
3502.165538	580345.657992	43.372557
3502.156801	580325.300758	43.377562
3502.111159	580302.843197	43.382567
3501.954003	580282.659520	43.387572
3502.221007	580268.376684	43.392577
3502.304541	580252.818754	43.397581
3501.753914	580232.546063	43.402586
3502.202735	580221.092983	43.407591
3502.168056	580201.140734	43.412596
3502.135288	580179.984674	43.417601
3502.385185	580153.669605	43.422605
3502.464793	580142.474743	43.427610
3502.296900	580106.246018	43.432615
3502.275821	580094.866268	43.437620
3502.438989	580065.756417	43.442625
3502.123816	580045.747447	43.447629
3502.315765	580043.711531	43.452634
3502.467769	580012.497178	43.457639
3501.969473	579992.266011	43.462644
3502.367694	579968.585036	43.467649
3502.438210	579950.270702	43.472653
3502.207203	579931.201138	43.477658
3502.174957	579910.746528	43.482663
3501.985435	579879.384607	43.487668
3502.036131	579856.209037	43.492673
3502.462988	579840.697153	43.497677
3502.030268	579818.449563	43.502682
3502.091792	579797.177741	43.507687
3502.345872	579777.330030	43.512692
3502.602254	579767.711848	43.517697
3502.321504	579741.679346	43.522701
3502.133266	579719.092457	43.527706
3502.297061	579701.816216	43.532711
3502.314904	579685.014087	43.537716
3502.394838	579660.078391	43.542721
3502.782478	579635.746451	43.547725
3502.338339	579626.739131	43.552730
3502.802573	579592.315509	43.557735
3502.091080	579565.698015	43.562740
3502.221059	579538.397287	43.567745
3502.482285	579517.344450	43.572749
3502.004487	579496.256660	43.577754
3502.263240	579476.658422	43.582759
3502.073653	579468.112659	43.587764
3501.993509	579444.856390	43.592769
3502.288777	579420.287680	43.597773
3502.138854	579408.325590	43.602778
3501.860317	579376.123644	43.607783
3502.049302	579377.397867	43.612788
3501.882488	579356.461790	43.617793
3502.075716	579334.416267	43.622797
3501.769988	579316.460599	43.627802
3501.880102	579287.005965	43.632807
3502.072116	579288.329874	43.637812
3502.240430	579260.270239	43.642817
3501.887941	579251.198137	43.647821
3501.925258	579233.840644	43.652826
3501.901613	579213.634153	43.657831
3501.926908	579206.358474	43.662836
3501.746967	579168.924998	43.667841
3501.769193	579166.915456	43.672845
3502.092258	579164.407540	43.677850
3502.322773	579133.228599	43.682855
3502.405205	579124.238851	43.687860
3502.599035	579100.989183	43.692865
3502.306350	579077.013127	43.697869
3501.906646	579062.030575	43.702874
3502.016194	579038.944404	43.707879
3502.435799	579022.228919	43.712884
3502.192567	578997.944061	43.717889
3502.264478	578980.330016	43.722893
3502.158697	578963.847027	43.727898
3502.165343	578935.410645	43.732903
3501.824986	578929.997363	43.737908
3501.840895	578905.721944	43.742913
3502.087823	578888.832652	43.747917
3501.610371	578890.612319	43.752922
3501.960273	578858.862291	43.757927
3501.933995	578848.284491	43.762932
3501.821088	578834.711172	43.767937
3501.352690	578809.658689	43.772941
3501.574242	578799.894666	43.777946
3501.446757	578788.429912	43.782951
3501.782042	578788.527859	43.787956
3501.505749	578752.712880	43.792961
3501.679813	578757.650548	43.797965
3501.353950	578753.789602	43.802970
3501.814070	578740.678251	43.807975
3501.777717	578722.328453	43.812980
3501.918111	578718.695514	43.817985
3502.111480	578699.858405	43.822989
3501.636642	578685.940272	43.827994
3501.936814	578672.502785	43.832999
3502.343716	578651.525846	43.838004
3501.900924	578634.593538	43.843009
3501.502595	578614.243926	43.848013
3501.574194	578600.741782	43.853018
3502.042684	578585.723169	43.858023
3501.980343	578579.213061	43.863028
3501.806581	578552.107858	43.868033
3501.724591	578546.503542	43.873037
3501.799626	578530.493167	43.878042
3501.656379	578507.796481	43.883047
3501.843613	578506.463158	43.888052
3501.371485	578491.491159	43.893057
3501.684054	578462.855291	43.898061
3501.810281	578461.381042	43.903066
3501.827493	578451.949576	43.908071
3501.482544	578431.290370	43.913076
3501.691919	578424.938306	43.918081
3502.168448	578410.419729	43.923085
3502.072697	578408.779563	43.928090
3501.969686	578383.267778	43.933095
3501.777246	578383.047005	43.938100
3501.906895	578353.787466	43.943105
3502.113162	578344.928191	43.948109
3501.567769	578326.406554	43.953114
3502.109222	578306.812224	43.958119
3502.212786	578305.291344	43.963124
3501.988107	578276.187300	43.968129
3501.967506	578268.216038	43.973133
3501.718865	578253.008166	43.978138
3501.827933	578219.538600	43.983143
3501.725246	578219.554560	43.988148
3501.754660	578202.297006	43.993153
3502.014492	578176.176335	43.998157
3501.860392	578177.805255	44.003162
3501.948060	578155.723754	44.008167
3501.882350	578141.991752	44.013172
3501.636426	578130.946069	44.018177
3501.709963	578103.098959	44.023181
3501.690114	578093.622830	44.028186
3502.031794	578089.657295	44.033191
3501.967653	578080.639467	44.038196
3501.880309	578060.440845	44.043201
3501.567967	578053.969513	44.048205
3501.376874	578032.733818	44.053210
3501.929284	578013.036953	44.058215
3501.830478	578015.760652	44.063220
3501.803930	577999.614934	44.068225
3502.101997	577977.299572	44.073229
3502.126310	577969.371230	44.078234
3501.923125	577943.523017	44.083239
3501.982730	577926.962487	44.088244
3501.786635	577914.855546	44.093249
3501.806195	577895.492549	44.098253
3501.216977	577893.076813	44.103258
3501.506947	577893.934182	44.108263
3501.780665	577872.324588	44.113268
3501.590670	577855.000488	44.118273
3501.944346	577849.728957	44.123277
3501.318168	577833.977670	44.128282
3501.488854	577817.750700	44.133287
3501.821001	577808.419925	44.138292
3501.536316	577803.348476	44.143297
3502.103782	577784.952901	44.148301
3501.592782	577775.302504	44.153306
3501.502625	577758.113113	44.158311
3501.834845	577766.085995	44.163316
3501.766142	577744.379218	44.168321
3501.762301	577734.298412	44.173325
3501.990267	577726.538685	44.178330
3501.935215	577700.215350	44.183335
3502.373194	577692.121832	44.188340
3501.629229	577679.849504	44.193345
3501.735358	577649.638835	44.198349
3501.677661	577649.547450	44.203354
3501.952814	577623.322782	44.208359
3501.588428	577612.746511	44.213364
3501.502297	577604.082831	44.218369
3501.936113	577586.861421	44.223373
3501.251230	577576.836783	44.228378
3501.814687	577564.711036	44.233383
3501.905349	577554.966392	44.238388
3501.855647	577536.265637	44.243393
3502.113061	577527.197095	44.248397
3501.798911	577504.274303	44.253402
3501.906383	577487.956425	44.258407
3501.538360	577484.653351	44.263412
3501.683795	577470.937673	44.268417
3501.779733	577455.875476	44.273421
3501.172859	577442.528156	44.278426
3501.227116	577442.770367	44.283431
3501.220365	577442.871644	44.288436
3501.272787	577435.440101	44.293441
3501.456187	577406.871884	44.298445
3501.718865	577413.451486	44.303450
3501.732716	577410.740737	44.308455
3501.077865	577396.498031	44.313460
3501.447379	577376.126438	44.318465
3501.827349	577361.019712	44.323469
3501.656558	577366.363010	44.328474
3501.872730	577350.780301	44.333479
3501.990615	577320.617066	44.338484
3501.322365	577330.552337	44.343489
3501.367126	577308.776819	44.348493
3501.190369	577304.240006	44.353498
3501.250711	577287.076521	44.358503
3501.404104	577284.494401	44.363508
3501.760351	577286.294456	44.368513
3501.687058	577273.766360	44.373517
3501.396251	577269.598467	44.378522
3501.675195	577255.861655	44.383527
3501.402607	577249.283324	44.388532
3501.161620	577238.837881	44.393537
3501.419860	577232.477505	44.398541
3501.363586	577244.373663	44.403546
3501.618896	577213.335969	44.408551
3501.501522	577201.717531	44.413556
3501.617452	577204.257383	44.418561
3501.345248	577182.079746	44.423565
3501.402847	577165.167295	44.428570
3501.429792	577160.698896	44.433575
3501.919779	577155.907316	44.438580
3501.381298	577153.232691	44.443585
3501.657393	577137.339368	44.448589
3501.142169	577119.563385	44.453594
3501.285838	577112.869742	44.458599
3501.363239	577106.086138	44.463604
3501.463422	577113.945285	44.468609
3501.821727	577102.904443	44.473613
3501.621210	577094.408726	44.478618
3501.540600	577086.044733	44.483623
3501.759256	577089.922837	44.488628
3501.812467	577077.424904	44.493633
3502.027616	577053.415270	44.498637
3501.746153	577042.775336	44.503642
3501.538285	577024.549883	44.508647
3501.483036	577014.325989	44.513652
3500.991663	577003.819151	44.518657
3501.601556	576999.159238	44.523661
3501.556461	577003.530036	44.528666
3501.467088	576974.301132	44.533671
3501.406314	576961.168820	44.538676
3501.520037	576963.759231	44.543681
3501.701781	576951.592179	44.548685
3501.312892	576943.777866	44.553690
3501.628591	576923.714823	44.558695
3501.964001	576923.561978	44.563700
3501.637067	576911.374084	44.568705
3501.640550	576891.008675	44.573709
3501.578135	576880.284183	44.578714
3501.463896	576871.122733	44.583719
3501.501422	576876.032421	44.588724
3501.058052	576857.642873	44.593729
3501.491200	576846.991358	44.598733
3501.508643	576839.715369	44.603738
3501.581230	576833.835229	44.608743
3501.657533	576827.503066	44.613748
3501.177802	576796.328328	44.618753
3501.516321	576794.319075	44.623757
3501.087318	576786.460762	44.628762
3501.274350	576785.528551	44.633767
3501.691649	576789.124906	44.638772
3501.725697	576773.068267	44.643777
3502.043547	576759.174286	44.648781
3501.917872	576759.795762	44.653786
3501.888392	576736.425614	44.658791
3501.791356	576710.307158	44.663796
3501.762336	576704.342514	44.668801
3501.930034	576682.747205	44.673805
3502.025901	576670.442793	44.678810
3501.881060	576660.533546	44.683815
3501.945060	576637.800667	44.688820
3501.590620	576619.547308	44.693825
3501.579477	576617.091078	44.698829
3501.667387	576598.016119	44.703834
3501.603303	576582.777123	44.708839
3501.661610	576591.495919	44.713844
3501.227788	576581.932744	44.718849
3501.538452	576561.468555	44.723853
3501.395994	576551.157550	44.728858
3501.370909	576546.044945	44.733863
3501.564877	576547.820330	44.738868
3501.987354	576533.207459	44.743873
3502.131005	576516.079934	44.748877
3502.076910	576507.912010	44.753882
3502.354628	576474.812160	44.758887
3502.043843	576460.865600	44.763892
3501.542018	576452.065367	44.768897
3501.822405	576443.293330	44.773901
3501.545836	576438.571122	44.778906
3501.631405	576410.216309	44.783911
3501.605119	576394.419370	44.788916
3501.517432	576397.593178	44.793921
3501.647966	576393.609897	44.798925
3501.448419	576377.940344	44.803930
3501.493520	576363.336085	44.808935
3501.985568	576361.403080	44.813940
3502.033187	576346.999054	44.818945
3502.066696	576319.805879	44.823949
3501.709201	576310.280701	44.828954
3501.599578	576287.524094	44.833959
3501.787811	576277.211303	44.838964
3501.686434	576272.862936	44.843969
3501.775059	576264.572199	44.848973
3501.564239	576246.145292	44.853978
3501.519588	576226.939939	44.858983
3501.551131	576231.600032	44.863988
3501.157531	576215.759937	44.868993
3502.116043	576185.713053	44.873997
3501.917722	576185.041685	44.879002
3501.387248	576168.972108	44.884007
3501.465659	576154.061393	44.889012
3501.534595	576147.629674	44.894017
3501.585417	576141.652250	44.899021
3501.363436	576141.185230	44.904026
3501.734528	576135.107572	44.909031
3501.582958	576120.333091	44.914036
3501.255162	576113.361416	44.919041
3501.000610	576108.234322	44.924045
3501.759852	576104.152654	44.929050
3501.914239	576094.346618	44.934055
3501.669739	576070.858210	44.939060
3501.617774	576071.518364	44.944065
3501.461717	576052.631109	44.949069
3501.840247	576043.893582	44.954074
3501.375811	576021.392557	44.959079
3501.541539	576024.677345	44.964084
3501.261792	576015.842050	44.969089
3501.498395	575996.040537	44.974093
3501.849848	575996.085829	44.979098
3501.480280	575972.315785	44.984103
3501.656561	575969.328477	44.989108
3501.663163	575952.321846	44.994113
3501.664424	575941.636667	44.999117
3501.837555	575941.459018	45.004122
3502.081965	575928.729263	45.009127
3501.533121	575915.371043	45.014132
3501.420101	575907.262057	45.019137
3501.362904	575886.101689	45.024141
3501.236240	575867.761333	45.029146
3501.729962	575864.222731	45.034151
3501.584950	575861.636770	45.039156
3501.458532	575864.616127	45.044161
3501.416432	575835.075883	45.049165
3501.471769	575824.432304	45.054170
3501.477816	575825.986361	45.059175
3501.645155	575824.304685	45.064180
3501.737741	575821.179929	45.069185
3501.615847	575795.916027	45.074189
3501.247189	575793.013862	45.079194
3501.534419	575796.731203	45.084199
3501.654569	575784.723013	45.089204
3500.984321	575763.758580	45.094209
3501.323368	575751.966959	45.099213
3501.353357	575751.009050	45.104218
3501.630635	575744.093049	45.109223
3501.683980	575736.559909	45.114228
3501.505205	575719.481576	45.119233
3501.434489	575696.567196	45.124237
3501.548137	575694.944060	45.129242
3501.239707	575702.466754	45.134247
3500.924769	575702.064411	45.139252
3501.185078	575703.779396	45.144257
3501.349648	575677.968798	45.149261
3501.479081	575667.463982	45.154266
3501.183688	575655.018965	45.159271
3501.209590	575653.509870	45.164276
3501.055435	575656.995268	45.169281
3501.016837	575648.372811	45.174285
3501.209856	575650.298984	45.179290
3501.383563	575653.331808	45.184295
3501.440988	575656.834295	45.189300
3501.222495	575640.665023	45.194305
3501.620174	575618.931391	45.199309
3501.606282	575618.481982	45.204314
3501.595505	575618.784566	45.209319
3501.926870	575604.034241	45.214324
3501.351549	575582.552976	45.219329
3501.736800	575569.098483	45.224333
3501.914849	575574.789419	45.229338
3501.475104	575545.661738	45.234343
3501.301288	575537.862984	45.239348
3500.978893	575534.050537	45.244353
3501.496465	575529.053300	45.249357
3501.642053	575535.100491	45.254362
3501.460041	575508.791864	45.259367
3501.738042	575493.447748	45.264372
3501.495420	575488.017508	45.269377
3501.655256	575485.634634	45.274381
3501.510698	575473.416665	45.279386
3501.319491	575457.644191	45.284391
3501.198883	575452.495856	45.289396
3501.191624	575464.085239	45.294401
3501.336215	575457.290137	45.299405
3501.517547	575449.435802	45.304410
3501.793825	575422.704168	45.309415
3501.340806	575417.507450	45.314420
3501.145577	575408.909295	45.319425
3501.430429	575411.272649	45.324429
3501.111376	575403.396174	45.329434
3501.094064	575380.121638	45.334439
3501.236162	575377.440516	45.339444
3501.201169	575372.078094	45.344449
3501.431039	575364.868275	45.349453
3501.585680	575365.897502	45.354458
3501.511819	575368.467441	45.359463
3501.657060	575349.030239	45.364468
3501.566444	575331.887370	45.369473
3501.590528	575317.435540	45.374477
3501.055158	575321.632802	45.379482
3501.435245	575316.757298	45.384487
3501.895319	575301.986458	45.389492
3501.209944	575295.571840	45.394497
3501.276503	575287.785501	45.399501
3501.701615	575283.605279	45.404506
3501.451302	575269.998952	45.409511
3501.701479	575258.822712	45.414516
3501.554338	575247.407571	45.419521
3501.901710	575236.416782	45.424525
3501.927324	575223.268933	45.429530
3501.533709	575212.694961	45.434535
3501.624407	575195.021868	45.439540
3501.320264	575182.627862	45.444545
3501.162466	575170.712637	45.449549
3501.085864	575164.804782	45.454554
3501.680751	575163.106339	45.459559
3501.561377	575153.743621	45.464564
3501.443730	575162.741869	45.469569
3501.458352	575144.528749	45.474573
3501.323604	575128.395816	45.479578
3501.307046	575123.682572	45.484583
3501.862219	575125.502054	45.489588
3501.493316	575116.980993	45.494593
3501.266120	575093.788844	45.499597
3501.387453	575082.030560	45.504602
3501.502194	575086.076109	45.509607
3501.239006	575079.896372	45.514612
3500.981824	575087.010122	45.519617
3501.533199	575071.121020	45.524621
3501.682341	575056.097461	45.529626
3501.230172	575042.221408	45.534631
3501.038663	575035.779602	45.539636
3501.232560	575035.949870	45.544641
3501.220630	575034.195767	45.549645
3501.449054	575039.477758	45.554650
3501.703268	575028.952841	45.559655
3502.004490	575006.430424	45.564660
3501.319611	575000.768078	45.569665
3501.854547	574988.092182	45.574669
3501.430181	574972.706655	45.579674
3501.742799	574965.784655	45.584679
3501.942081	574949.950425	45.589684
3501.551491	574932.452497	45.594689
3501.563832	574914.440036	45.599693
3501.330406	574914.175424	45.604698
3501.762006	574916.214933	45.609703
3502.115603	574899.754489	45.614708
3501.839518	574887.957794	45.619713
3501.864095	574871.649081	45.624717
3501.680527	574852.814282	45.629722
3501.165737	574841.155191	45.634727
3501.630353	574828.640617	45.639732
3501.671019	574825.523702	45.644737
3501.513465	574803.524120	45.649741
3501.482237	574801.973674	45.654746
3501.568411	574792.478185	45.659751
3501.430093	574793.954614	45.664756
3501.713120	574778.157222	45.669761
3501.507937	574763.289002	45.674765
3501.589481	574755.198940	45.679770
3501.668894	574747.008866	45.684775
3501.459486	574724.013852	45.689780
3501.457131	574713.578921	45.694785
3501.943621	574710.542788	45.699789
3501.614345	574710.895187	45.704794
3501.630404	574683.700791	45.709799
3501.534518	574681.458064	45.714804
3501.229376	574678.043983	45.719809
3501.618179	574672.313961	45.724813
3501.296987	574654.754582	45.729818
3501.160788	574648.504586	45.734823
3501.231007	574626.418881	45.739828
3501.344669	574568.053539	45.744833
3501.126145	574462.078043	45.749837
3500.793015	574319.193645	45.754842
3500.581245	574126.417717	45.759847
3500.445283	573881.497048	45.764852
3499.992644	573598.086841	45.769857
3499.607819	573256.706105	45.774861
3499.388552	572880.867564	45.779866
3498.563022	572462.007462	45.784871
3498.077846	571985.420485	45.789876
3496.517213	571473.251009	45.794881
3495.805594	570925.193400	45.799885
3494.904478	570337.339628	45.804890
3493.675129	569688.775482	45.809895
3492.756922	569026.071600	45.814900
3491.529843	568320.659857	45.819905
3490.522086	567569.237070	45.824909
3488.695311	566785.963644	45.829914
3487.711538	565969.167573	45.834919
3486.163813	565100.734756	45.839924
3484.819613	564213.525233	45.844929
3483.297252	563283.087639	45.849933
3481.742510	562312.754038	45.854938
3479.916858	561315.460567	45.859943
3478.254314	560274.656674	45.864948
3475.928468	559218.743558	45.869953
3474.191798	558122.149900	45.874957
3472.143901	556992.894195	45.879962
3470.307284	555850.282658	45.884967
3468.341042	554664.262044	45.889972
3466.083266	553446.354976	45.894977
3464.155421	552204.598202	45.899981
3461.471023	550938.953686	45.904986
3459.300155	549654.746341	45.909991
3457.311132	548338.396382	45.914996
3454.874970	546996.982358	45.920001
3452.354339	545628.327710	45.925005
3449.789467	544233.977051	45.930010
3446.980247	542827.737116	45.935015
3444.566409	541399.291699	45.940020
3442.083800	539967.172462	45.945025
3439.403383	538482.436293	45.950029
3436.212639	536991.868747	45.955034
3433.898709	535483.473768	45.960039
3431.009562	533962.104254	45.965044
3428.061680	532437.090361	45.970049
3425.320529	530870.274286	45.975053
3422.600463	529292.791948	45.980058
3419.369649	527701.701871	45.985063
3416.984274	526104.796933	45.990068
3413.236789	524496.426571	45.995073
3410.361421	522866.363513	46.000077
3407.266564	521219.306621	46.005082
3403.974284	519568.702664	46.010087
3400.854632	517906.984024	46.015092
3397.157124	516243.943260	46.020097
3394.193984	514553.766272	46.025101
3390.647291	512868.464810	46.030106
3387.841942	511176.892542	46.035111
3384.703331	509463.986300	46.040116
3381.415238	507756.341785	46.045121
3377.661608	506021.677399	46.050125
3374.148725	504303.563566	46.055130
3370.746487	502566.608134	46.060135
3367.244323	500833.495918	46.065140
3363.538340	499090.569167	46.070145
3360.498434	497331.279580	46.075149
3356.955368	495575.846045	46.080154
3352.997378	493816.987598	46.085159
3349.897585	492045.416884	46.090164
3345.909412	490281.047578	46.095169
3342.255013	488498.794279	46.100173
3338.927256	486737.293080	46.105178
3335.155941	484955.604159	46.110183
3331.888980	483175.702023	46.115188
3327.788796	481412.299122	46.120193
3324.311409	479622.980178	46.125197
3320.733234	477842.772968	46.130202
3317.461846	476068.029706	46.135207
3313.942147	474281.906416	46.140212
3309.837525	472490.014469	46.145217
3306.241329	470696.884625	46.150221
3302.320924	468911.750094	46.155226
3298.631518	467130.229565	46.160231
3295.083899	465332.007685	46.165236
3291.308055	463552.040309	46.170241
3287.759350	461750.248623	46.175245
3284.283440	459954.679920	46.180250
3280.405705	458170.775302	46.185255
3276.637226	456382.064404	46.190260
3272.767783	454588.074008	46.195265
3269.319392	452792.214724	46.200269
3265.626106	451010.536606	46.205274
3261.599176	449226.252082	46.210279
3258.069621	447426.827781	46.215284
3253.970952	445638.301461	46.220289
3250.656430	443843.097039	46.225293
3246.814686	442059.549627	46.230298
3242.537735	440279.697804	46.235303
3239.195205	438491.375694	46.240308
3235.514760	436709.928150	46.245313
3231.794514	434923.760781	46.250317
3227.667832	433153.502112	46.255322
3223.704822	431368.006721	46.260327
3220.786141	429594.449016	46.265332
3216.364770	427820.054789	46.270337
3212.496391	426052.360074	46.275341
3208.706422	424290.073645	46.280346
3204.987451	422523.618197	46.285351
3201.474160	420756.268432	46.290356
3197.195268	419009.878402	46.295361
3193.829000	417248.494270	46.300365
3190.246530	415498.102454	46.305370
3186.291072	413738.698792	46.310375
3182.863308	411977.140965	46.315380
3178.755219	410222.038940	46.320385
3175.172118	408470.163477	46.325389
3171.502066	406716.437736	46.330394
3167.829681	404976.273190	46.335399
3163.736068	403232.234537	46.340404
3159.874190	401490.867562	46.345409
3155.973236	399744.249175	46.350413
3152.567100	398002.700111	46.355418
3148.658363	396280.742539	46.360423
3145.174942	394533.010780	46.365428
3141.042480	392804.339611	46.370433
3136.843346	391082.104123	46.375437
3133.168394	389363.599944	46.380442
3129.509368	387641.292639	46.385447
3125.875568	385925.311206	46.390452
3121.903846	384213.175990	46.395457
3118.277695	382504.909108	46.400461
3114.553101	380807.387461	46.405466
3110.694949	379100.303827	46.410471
3106.987202	377397.327404	46.415476
3103.118090	375702.979079	46.420481
3099.459681	374009.659759	46.425485
3095.474986	372318.775701	46.430490
3092.107309	370637.217687	46.435495
3088.113236	368949.813317	46.440500
3084.173505	367267.101404	46.445505
3080.690297	365581.220982	46.450509
3076.710737	363908.049859	46.455514
3073.040568	362240.426710	46.460519
3069.616072	360565.606867	46.465524
3065.660038	358898.197379	46.470529
3061.831829	357226.889663	46.475533
3057.984893	355565.380969	46.480538
3054.444623	353903.481621	46.485543
3050.775598	352242.506307	46.490548
3046.760712	350593.700464	46.495553
3043.304205	348938.876590	46.500557
3039.711703	347292.507214	46.505562
3035.580440	345642.937332	46.510567
3032.075519	343992.349913	46.515572
3028.193434	342355.675484	46.520577
3024.597628	340712.293461	46.525581
3021.048187	339076.430667	46.530586
3017.257353	337438.826948	46.535591
3012.890332	335797.323019	46.540596
3009.762021	334172.515298	46.545601
3006.249156	332539.914523	46.550605
3002.020921	330919.919815	46.555610
2998.208729	329300.758433	46.560615
2994.828608	327676.426075	46.565620
2991.061782	326059.998791	46.570625
2987.603466	324444.476083	46.575629
2984.117277	322831.794215	46.580634
2980.024794	321220.798435	46.585639
2976.342341	319605.148812	46.590644
2972.404191	317999.095820	46.595649
2968.586191	316404.363780	46.600653
2965.314710	314804.222437	46.605658
2961.205553	313205.835144	46.610663
2957.808318	311607.866586	46.615668
2954.021214	310023.416991	46.620673
2950.539172	308419.680073	46.625677
2946.679158	306837.020893	46.630682
2942.476731	305255.688433	46.635687
2939.119936	303659.464608	46.640692
2935.342061	302088.809990	46.645697
2931.721747	300518.084193	46.650701
2928.359353	298938.771483	46.655706
2924.629920	297370.924810	46.660711
2920.937819	295806.006835	46.665716
2916.950365	294228.391001	46.670721
2913.713790	292662.503009	46.675725
2909.987033	291095.251048	46.680730
2906.030082	289531.126487	46.685735
2902.550903	287965.666681	46.690740
2898.700134	286396.535943	46.695745
2894.879413	284834.466314	46.700749
2891.146512	283288.258833	46.705754
2887.247940	281748.357047	46.710759
2884.040206	280195.660910	46.715764
2880.075833	278659.905188	46.720769
2876.218458	277094.694772	46.725773
2872.724209	275559.898822	46.730778
2868.957739	274022.799342	46.735783
2865.281284	272484.970014	46.740788
2861.811380	270953.293807	46.745793
2858.148735	269416.885306	46.750797
2854.312953	267889.594159	46.755802
2850.203713	266372.124894	46.760807
2847.086637	264850.122837	46.765812
2843.301433	263336.122196	46.770817
2839.708173	261812.240652	46.775821
2836.205941	260295.989034	46.780826
2832.208744	258781.424818	46.785831
2828.785808	257272.965549	46.790836
2825.082827	255764.073772	46.795841
2821.388581	254252.667838	46.800845
2817.925513	252745.869856	46.805850
2814.152000	251236.889445	46.810855
2810.648225	249731.876099	46.815860
2806.500143	248237.060422	46.820865
2803.015427	246732.527062	46.825869
2799.534555	245240.460342	46.830874
2795.568749	243753.679426	46.835879
2792.160088	242247.903925	46.840884
2788.268174	240770.158679	46.845889
2784.557978	239285.500163	46.850893
2781.453974	237809.678654	46.855898
2777.940129	236323.727003	46.860903
2774.132298	234840.183861	46.865908
2770.429740	233366.144358	46.870913
2766.615573	231869.577923	46.875917
2763.372472	230397.241334	46.880922
2759.277457	228923.099526	46.885927
2756.127100	227446.337444	46.890932
2751.944220	225981.476830	46.895937
2748.339353	224505.166150	46.900941
2745.066802	223039.526279	46.905946
2741.188116	221572.479617	46.910951
2738.108451	220109.766914	46.915956
2733.963652	218647.045126	46.920961
2730.467681	217185.778836	46.925965
2726.890967	215721.956959	46.930970
2723.280793	214264.410528	46.935975
2719.193764	212793.802514	46.940980
2715.581254	211347.372778	46.945985
2712.157771	209903.569221	46.950989
2707.986575	208449.855886	46.955994
2704.857862	207008.441982	46.960999
2701.313405	205562.976498	46.966004
2697.592031	204124.042930	46.971009
2693.835390	202683.724788	46.976013
2690.505973	201245.617790	46.981018
2686.479651	199810.815242	46.986023
2683.145305	198367.258477	46.991028
2679.412987	196936.332613	46.996033
2675.835940	195510.337039	47.001037
2672.429118	194076.715207	47.006042
2668.686098	192647.745397	47.011047
2665.253847	191212.325890	47.016052
2661.375551	189789.369307	47.021057
2657.986550	188365.920785	47.026061
2654.094729	186944.326172	47.031066
2650.445231	185512.450460	47.036071
2647.034476	184093.925774	47.041076
2643.350513	182684.427149	47.046081
2639.569799	181253.244271	47.051085
2636.292410	179849.835360	47.056090
2632.401546	178443.055878	47.061095
2629.238789	177019.965904	47.066100
2625.245604	175608.920135	47.071105
2621.389895	174204.458652	47.076109
2618.029299	172798.072951	47.081114
2614.346076	171400.648602	47.086119
2610.739363	169991.908431	47.091124
2607.168277	168586.753737	47.096129
2603.760802	167191.415065	47.101133
2600.110569	165787.740791	47.106138
2596.107160	164398.648464	47.111143
2592.554411	162994.838339	47.116148
2588.771831	161608.099076	47.121153
2585.379438	160216.415683	47.126157
2581.762288	158827.318300	47.131162
2577.993265	157449.590652	47.136167
2574.578317	156058.361063	47.141172
2570.426926	154681.826135	47.146177
2567.020718	153297.762331	47.151181
2563.401068	151924.951927	47.156186
2559.728437	150555.848644	47.161191
2556.511844	149185.372079	47.166196
2552.507500	147822.968754	47.171201
2549.275706	146359.953132	47.176205
2546.047345	144995.237040	47.181210
2541.565913	143629.799194	47.186215
2538.468393	142260.632157	47.191220
2534.829606	140903.586087	47.196225
2531.344247	139541.006738	47.201229
2527.644214	138169.670307	47.206234
2523.620982	136820.065287	47.211239
2520.492120	135460.958223	47.216244
2516.489221	134117.917786	47.221249
2512.640029	132755.773510	47.226253
2509.242436	131407.415454	47.231258
2505.380884	130059.069978	47.236263
2502.301688	128715.936042	47.241268
2498.461025	127376.054733	47.246273
2494.588294	126038.892514	47.251277
2491.519174	124702.080480	47.256282
2487.892566	123362.385397	47.261287
2484.381896	122017.006604	47.266292
2480.528522	120689.989587	47.271297
2476.896932	119358.608308	47.276301
2473.524466	118023.201308	47.281306
2469.610306	116699.001727	47.286311
2465.856265	115369.686585	47.291316
2462.454294	114045.195783	47.296321
2458.968285	112721.935714	47.301325
2455.236962	111400.186335	47.306330
2451.149352	110081.147812	47.311335
2447.812833	108746.988231	47.316340
2444.444478	107451.493719	47.321345
2440.499560	106137.793781	47.326349
2437.247330	104826.794414	47.331354
2433.144889	103518.838901	47.336359
2429.653918	102209.872800	47.341364
2426.389393	100913.086941	47.346369
2422.561197	99613.618947	47.351373
2419.226774	98309.054701	47.356378
2415.568910	97017.938478	47.361383
2412.208625	95714.234119	47.366388
2408.161732	94426.588807	47.371393
2404.837538	93126.481301	47.376397
2400.865780	91832.908766	47.381402
2396.878398	90545.632301	47.386407
2393.322714	89257.174204	47.391412
2389.604848	87985.821920	47.396417
2386.325926	86702.640136	47.401421
2382.793168	85424.750086	47.406426
2378.904105	84158.976739	47.411431
2375.058760	82888.336051	47.416436
2371.638213	81620.225890	47.421441
2368.193989	80356.266203	47.426445
2364.500436	79093.418527	47.431450
2360.700023	77831.165607	47.436455
2357.356295	76570.892921	47.441460
2353.178797	75326.187882	47.446465
2349.701086	74083.208362	47.451469
2346.525234	72816.251854	47.456474
2342.661622	71579.404448	47.461479
2339.163226	70333.187239	47.466484
2335.117040	69099.900370	47.471489
2331.540778	67860.212373	47.476493
2328.025016	66620.187236	47.481498
2324.453987	65399.831461	47.486503
2321.091676	64165.734861	47.491508
2316.958289	62938.737249	47.496513
2313.332358	61714.703258	47.501517
2309.998362	60496.839684	47.506522
2306.089583	59287.540765	47.511527
2302.715380	58068.490357	47.516532
2298.854772	56864.621674	47.521537
2295.004917	55645.932742	47.526541
2291.486269	54440.634706	47.531546
2287.453509	53242.729698	47.536551
2283.772044	52046.625904	47.541556
2279.916748	50869.019447	47.546561
2276.555558	49671.445791	47.551565
2273.003311	48496.475147	47.556570
2269.570676	47315.133603	47.561575
2265.902470	46135.380593	47.566580
2261.808395	44963.473846	47.571585
2258.349973	43803.431949	47.576589
2254.889217	42640.844400	47.581594
2250.927019	41476.538311	47.586599
2247.333806	40318.367360	47.591604
2243.512172	39157.953817	47.596609
2239.832650	38008.972777	47.601613
2236.132495	36872.399209	47.606618
2232.296343	35735.057552	47.611623
2228.157759	34593.228038	47.616628
2224.637079	33468.635920	47.621633
2220.404654	32355.459142	47.626637
2216.584585	31244.311393	47.631642
2212.807230	30150.150185	47.636647
2209.000745	29045.981372	47.641652
2205.093349	27959.719550	47.646657
2201.341422	26878.908737	47.651661
2197.226406	25813.659795	47.656666
2193.409560	24743.503506	47.661671
2189.520986	23683.577500	47.666676
2185.751614	22640.540618	47.671681
2181.063630	21610.213457	47.676685
2177.393994	20585.937699	47.681690
2172.073832	19608.213498	47.686695
2166.401867	18653.186283	47.691700
2161.382018	17724.654441	47.696705
2156.285564	16824.033072	47.701709
2151.549033	15937.858868	47.706714
2146.237058	15094.270523	47.711719
2141.485209	14269.144768	47.716724
2136.221773	13473.693681	47.721729
2131.666776	12708.308520	47.726733
2127.195702	11955.433666	47.731738
2122.841879	11239.321749	47.736743
2118.817346	10529.013473	47.741748
2114.518360	9860.797378	47.746753
2110.178054	9200.091487	47.751757
2106.338764	8551.507541	47.756762
2102.028201	7936.476124	47.761767
2098.328654	7312.231863	47.766772
2094.148994	6721.063027	47.771777
2090.466724	6136.180937	47.776781
2086.792488	5570.447390	47.781786
2082.862747	5016.316104	47.786791
2078.969608	4465.335170	47.791796
2074.932553	3930.940636	47.796801
2071.044120	3412.006246	47.801805
2067.110001	2896.305640	47.806810
2062.846684	2415.433658	47.811815
2058.991456	1925.818662	47.816820
2055.126906	1454.142944	47.821825
2051.189327	1013.985502	47.826829
2045.515705	612.596552	47.831834
2038.301705	270.517572	47.836839
2025.608010	123.131482	47.841844
2009.803585	147.355806	47.846849
1999.966011	160.060265	47.851853
1995.559734	143.288342	47.856858
1993.958269	149.518515	47.861863
1993.687459	146.048923	47.866868
1993.178346	147.542735	47.871873
1991.926606	149.272975	47.876877
1990.178970	153.235394	47.881882
1987.286316	147.521582	47.886887
1984.422768	145.982665	47.891892
1981.431253	155.559398	47.896897
1977.957235	155.856124	47.901901
1974.691034	150.365287	47.906906
1971.690256	150.622767	47.911911
1968.345424	152.892507	47.916916
1965.182229	145.031652	47.921921
1961.858160	140.160501	47.926925
1958.899008	139.734407	47.931930
1955.334597	143.756480	47.936935
1952.145799	143.366322	47.941940
1948.879686	137.207913	47.946945
1945.369865	140.107771	47.951949
1942.496002	132.223803	47.956954
1939.027722	146.127354	47.961959
1936.011639	144.707235	47.966964
1931.911269	137.828300	47.971969
1928.778714	143.757045	47.976973
1925.402796	130.842030	47.981978
1922.289272	129.614340	47.986983
1918.558431	136.411847	47.991988
1915.070092	144.079435	47.996993
1912.249680	136.962254	48.001997
1909.168738	134.976473	48.007002
1905.178474	140.333901	48.012007
1901.606832	128.208849	48.017012
1897.867462	135.501257	48.022017
1894.447164	137.523391	48.027021
1891.405985	129.194211	48.032026
1888.171305	129.102327	48.037031
1885.027412	133.068106	48.042036
1881.325359	137.674903	48.047041
1877.953153	128.385098	48.052045
1874.519607	122.094729	48.057050
1871.061148	140.663422	48.062055
1867.749689	128.700157	48.067060
1864.041132	126.603790	48.072065
1860.914403	133.290959	48.077069
1856.786722	122.578595	48.082074
1853.484475	131.561706	48.087079
1850.082718	132.549540	48.092084
1847.014078	134.602082	48.097089
1843.076365	133.221809	48.102093
1839.901125	128.599505	48.107098
1836.400121	138.278134	48.112103
1832.794099	128.521886	48.117108
1829.857094	137.175758	48.122113
1826.064933	130.261298	48.127117
1822.399260	126.025806	48.132122
1819.159399	135.407300	48.137127
1815.847476	133.805717	48.142132
1812.538692	128.195056	48.147137
1808.686098	140.317414	48.152141
1805.241489	132.930946	48.157146
1801.339055	129.577258	48.162151
1798.080878	124.369982	48.167156
1794.963028	135.162445	48.172161
1791.590980	132.244629	48.177165
1788.387017	124.823675	48.182170
1784.233280	134.949322	48.187175
1780.889660	120.479041	48.192180
1777.132636	127.638198	48.197185
1773.816030	122.908324	48.202189
1770.254413	129.818600	48.207194
1766.336333	140.919806	48.212199
1763.318994	115.885026	48.217204
1760.213974	131.446555	48.222209
1756.689060	130.681940	48.227213
1753.544515	127.813959	48.232218
1749.509449	131.485793	48.237223
1746.203188	131.152047	48.242228
1742.499128	135.629484	48.247233
1738.755453	138.221144	48.252237
1735.925229	127.846803	48.257242
1732.318013	127.857563	48.262247
1728.879416	134.315153	48.267252
1725.250357	131.152836	48.272257
1721.457606	133.559188	48.277261
1718.140388	121.464011	48.282266
1714.367211	129.922890	48.287271
1711.595268	120.324074	48.292276
1708.301385	120.640154	48.297281
1704.596308	128.506232	48.302285
1701.071184	114.494679	48.307290
1697.296024	122.355904	48.312295
1693.944339	122.070415	48.317300
1690.330406	123.148454	48.322305
1686.382929	126.063100	48.327309
1683.279308	116.930667	48.332314
1679.894220	122.554131	48.337319
1676.788474	120.458408	48.342324
1673.073207	118.723841	48.347329
1669.576816	128.680203	48.352333
1665.965276	120.206249	48.357338
1662.554925	125.944407	48.362343
1658.707019	116.539316	48.367348
1655.174657	127.210010	48.372353
1651.839593	128.310858	48.377357
1648.701208	114.577333	48.382362
1644.899598	120.228028	48.387367
1641.718252	122.649451	48.392372
1638.311130	122.296725	48.397377
1634.290001	120.723940	48.402381
1631.014321	112.149983	48.407386
1627.360149	118.587550	48.412391
1623.664080	122.563885	48.417396
1620.482731	114.414940	48.422401
1617.015727	125.252588	48.427405
1613.838741	122.405550	48.432410
1609.738595	129.517218	48.437415
1606.820603	115.521420	48.442420
1603.014902	120.960792	48.447425
1599.381682	122.763235	48.452429
1595.994995	114.032654	48.457434
1592.379211	119.647954	48.462439
1589.073360	116.605954	48.467444
1585.414986	107.886264	48.472449
1582.063847	118.775387	48.477453
1579.070846	116.098887	48.482458
1575.005851	114.748134	48.487463
1571.431403	117.019126	48.492468
1568.324300	113.560039	48.497473
1564.661189	122.394047	48.502477
1561.519508	110.572035	48.507482
1557.631427	125.269037	48.512487
1554.097975	118.690702	48.517492
1550.855173	113.838627	48.522497
1546.699247	124.913836	48.527501
1543.588429	113.226207	48.532506
1540.171849	122.512030	48.537511
1536.747066	118.957138	48.542516
1533.028324	117.558535	48.547521
1529.475837	118.813677	48.552525
1526.153598	119.051995	48.557530
1522.650890	120.280366	48.562535
1519.157202	116.540108	48.567540
1516.426716	122.959689	48.572545
1512.419492	127.693462	48.577549
1509.052379	109.012764	48.582554
1504.907185	112.831637	48.587559
1501.239040	111.542189	48.592564
1498.174863	111.120012	48.597569
1494.278974	122.243122	48.602573
1491.284405	116.194251	48.607578
1487.921026	110.598589	48.612583
1484.089270	111.248873	48.617588
1480.678964	106.941911	48.622593
1476.978543	109.779994	48.627597
1473.797428	110.885276	48.632602
1469.922551	108.100069	48.637607
1466.942603	112.366169	48.642612
1463.129674	121.033826	48.647617
1459.507195	118.813406	48.652621
1456.993512	111.417418	48.657626
1452.500403	123.513565	48.662631
1448.655968	117.616717	48.667636
1445.689258	108.972327	48.672641
1442.248097	118.024733	48.677645
1438.730391	117.591304	48.682650
1435.139157	108.981396	48.687655
1431.831511	114.592806	48.692660
1428.322965	109.573560	48.697665
1424.217307	115.256098	48.702669
1421.087135	105.868495	48.707674
1418.146746	110.969994	48.712679
1414.189345	110.940765	48.717684
1410.971348	110.093430	48.722689
1407.123982	112.483129	48.727693
1403.794455	107.100505	48.732698
1399.970730	119.863863	48.737703
1396.391100	105.804043	48.742708
1392.918371	106.736693	48.747713
1389.412223	109.908236	48.752717
1386.001808	105.955676	48.757722
1382.443792	111.713860	48.762727
1379.183757	105.776190	48.767732
1376.210446	111.920589	48.772737
1372.670274	116.413617	48.777741
1368.815835	105.057608	48.782746
1364.775187	109.508753	48.787751
1361.628404	119.204815	48.792756
1358.257026	120.067826	48.797761
1354.629272	114.861619	48.802765
1351.351354	106.756373	48.807770
1347.648150	117.251398	48.812775
1343.957723	107.932541	48.817780
1340.502710	120.075037	48.822785
1337.322906	114.608887	48.827789
1333.745107	107.284598	48.832794
1329.946998	116.725111	48.837799
1326.535159	113.728270	48.842804
1323.431910	106.975121	48.847809
1319.861306	113.352241	48.852813
1316.451054	103.208076	48.857818
1312.453321	120.940592	48.862823
1308.851652	115.654388	48.867828
1305.689521	108.606735	48.872833
1302.335621	114.747454	48.877837
1298.655918	108.052914	48.882842
1294.834682	114.598994	48.887847
1291.698709	106.126695	48.892852
1288.127745	100.538298	48.897857
1284.792917	110.940869	48.902861
1281.728057	104.146925	48.907866
1277.836957	107.467353	48.912871
1274.220035	111.061245	48.917876
1270.559079	101.952951	48.922881
1266.995917	106.512886	48.927885
1263.578266	102.162865	48.932890
1259.909235	103.553406	48.937895
1256.503517	107.050963	48.942900
1253.359764	101.095140	48.947905
1249.662919	106.745380	48.952909
1246.458897	99.960581	48.957914
1242.536244	109.534511	48.962919
1239.123489	107.857162	48.967924
1235.869102	109.875677	48.972929
1231.857059	115.420242	48.977933
1228.477578	101.439908	48.982938
1224.721361	121.554961	48.987943
1221.136837	113.975501	48.992948
1218.139290	108.974421	48.997953
1214.399631	113.166527	49.002957
1211.278225	109.516809	49.007962
1207.972987	112.403854	49.012967
1204.212563	111.084672	49.017972
1201.002667	113.175329	49.022977
1197.159568	108.933065	49.027981
1193.723630	102.564251	49.032986
1190.045413	106.322794	49.037991
1186.241997	102.434999	49.042996
1182.996686	104.379343	49.048001
1179.243964	106.687868	49.053005
1176.604002	107.078923	49.058010
1172.503519	110.406859	49.063015
1169.093164	106.289853	49.068020
1165.742944	107.428033	49.073025
1162.268642	109.901789	49.078029
1158.559267	101.702815	49.083034
1154.934958	111.397749	49.088039
1151.573957	97.506312	49.093044
1147.761772	98.818063	49.098049
1144.359215	113.983330	49.103053
1141.016851	110.570714	49.108058
1137.734531	111.714091	49.113063
1133.989538	111.879517	49.118068
1130.435284	104.285870	49.123073
1127.233325	112.664982	49.128077
1123.328505	109.716924	49.133082
1119.822432	112.562671	49.138087
1116.533862	111.384791	49.143092
1113.311776	110.047803	49.148097
1109.429944	107.333439	49.153101
1106.148414	108.786758	49.158106
1102.620839	109.563575	49.163111
1098.860466	107.326920	49.168116
1095.846723	110.345537	49.173121
1092.122753	110.517179	49.178125
1088.750101	99.623731	49.183130
1085.136591	110.041508	49.188135
1081.614728	117.363382	49.193140
1078.086601	114.074786	49.198145
1074.442330	106.704068	49.203149
1071.157472	101.305090	49.208154
1067.247530	108.191005	49.213159
1064.137480	108.779078	49.218164
1060.552145	105.942383	49.223169
1056.988273	108.550422	49.228173
1053.801130	106.856801	49.233178
1049.965934	110.507090	49.238183
1046.272782	109.746926	49.243188
1042.547362	106.036809	49.248193
1039.121363	105.734704	49.253197
1036.145749	111.376501	49.258202
1032.452636	105.016379	49.263207
1029.124098	104.800261	49.268212
1025.719515	100.454614	49.273217
1021.942124	107.566568	49.278221
1018.110666	100.649137	49.283226
1014.895099	113.542010	49.288231
1011.531776	107.256815	49.293236
1008.223421	100.956689	49.298241
1004.571549	102.281360	49.303245
1001.081253	95.794587	49.308250
997.680679	99.022496	49.313255
993.957560	104.142250	49.318260
990.752576	101.809190	49.323265
986.785842	99.674496	49.328269
983.202891	94.831602	49.333274
979.893852	111.504055	49.338279
976.779301	104.423772	49.343284
973.170164	100.644858	49.348289
969.182206	105.059427	49.353293
965.744302	94.907096	49.358298
962.438449	105.349502	49.363303
959.009804	105.756534	49.368308
955.881021	89.905237	49.373313
951.837161	109.948313	49.378317
948.278317	98.179231	49.383322
945.147830	105.443026	49.388327
941.364441	101.754685	49.393332
937.780717	94.918729	49.398337
934.765253	107.071590	49.403341
931.142337	103.525809	49.408346
927.228010	97.943871	49.413351
923.659704	101.672640	49.418356
920.358722	100.319600	49.423361
916.393068	102.259759	49.428365
913.409242	97.835620	49.433370
910.089995	103.221200	49.438375
906.600388	104.248413	49.443380
903.093383	95.002289	49.448385
899.137873	104.454920	49.453389
896.042749	103.215190	49.458394
892.048967	113.743189	49.463399
888.784422	105.117174	49.468404
885.737137	100.187280	49.473409
882.058580	110.719706	49.478413
878.630555	96.288391	49.483418
874.694453	100.169683	49.488423
871.209389	101.525233	49.493428
868.000657	101.154368	49.498433
864.075166	107.039860	49.503437
860.877024	104.651990	49.508442
857.245749	102.002908	49.513447
853.417013	103.700185	49.518452
850.234753	109.909073	49.523457
846.783598	107.981613	49.528461
843.685732	100.082508	49.533466
839.934195	105.811053	49.538471
836.205233	113.428026	49.543476
833.279220	106.353077	49.548481
829.314402	104.487076	49.553485
825.424743	103.476191	49.558490
821.967863	104.824182	49.563495
818.865214	97.799048	49.568500
815.688579	104.617679	49.573505
812.153443	102.349037	49.578509
808.610160	102.305831	49.583514
804.939268	96.049904	49.588519
801.001446	101.333061	49.593524
797.760640	93.813871	49.598529
794.304431	96.718360	49.603533
790.730211	103.263892	49.608538
787.015521	102.029469	49.613543
783.613836	103.580806	49.618548
780.627177	95.468157	49.623553
776.923319	100.047122	49.628557
773.286494	92.852553	49.633562
769.768834	95.852096	49.638567
766.014741	102.596649	49.643572
762.857477	99.240616	49.648577
759.164124	97.449197	49.653581
755.840978	95.125235	49.658586
752.288298	99.111049	49.663591
748.529951	96.747672	49.668596
745.305793	100.008152	49.673601
741.654874	100.874021	49.678605
738.236308	97.530443	49.683610
735.017923	100.761548	49.688615
731.695337	104.793597	49.693620
727.932101	89.766275	49.698625
724.061146	96.598745	49.703629
720.776378	90.937299	49.708634
717.282652	97.596800	49.713639
713.401604	93.211998	49.718644
710.609635	89.552004	49.723649
706.641886	93.935033	49.728653
703.476889	102.991847	49.733658
699.741385	100.650223	49.738663
695.923402	97.014865	49.743668
692.520700	96.199866	49.748673
688.735608	91.980386	49.753677
685.773590	93.124376	49.758682
682.383301	92.554214	49.763687
678.864266	97.230822	49.768692
675.176262	95.182332	49.773697
671.878294	103.143154	49.778701
668.370989	90.967503	49.783706
664.706367	85.321276	49.788711
661.010958	94.742741	49.793716
657.451666	96.654167	49.798721
653.847744	100.046918	49.803725
650.888523	96.425791	49.808730
647.126147	96.730175	49.813735
643.595513	97.703797	49.818740
640.451877	87.761802	49.823745
636.566674	96.640351	49.828749
633.447835	92.345028	49.833754
629.433078	96.058396	49.838759
625.970077	94.563156	49.843764
622.435375	93.901737	49.848769
618.651258	99.875910	49.853773
615.950686	90.592210	49.858778
612.240703	89.081872	49.863783
608.878590	90.124028	49.868788
605.514291	85.769082	49.873793
601.513362	92.615622	49.878797
598.120062	87.853926	49.883802
594.599480	92.179621	49.888807
591.141331	92.948918	49.893812
587.992040	88.686857	49.898817
583.976016	96.140055	49.903821
580.587153	91.488403	49.908826
577.009408	91.099502	49.913831
572.949335	93.855030	49.918836
570.032561	91.344107	49.923841
566.593883	96.786463	49.928845
563.087162	98.794097	49.933850
559.635259	96.126538	49.938855
556.202814	94.408238	49.943860
552.623703	87.109820	49.948865
548.874684	89.800822	49.953869
545.821294	95.296737	49.958874
541.858968	98.248945	49.963879
538.452467	104.119713	49.968884
535.022426	85.658210	49.973889
531.905768	95.900247	49.978893
528.158101	90.232285	49.983898
524.973096	97.558515	49.988903
521.051773	92.158202	49.993908
517.503006	87.525294	49.998913
513.607680	94.649562	50.003917
510.064793	93.132079	50.008922
507.015527	97.168848	50.013927
503.459766	99.086107	50.018932
499.816431	102.108595	50.023937
496.332310	100.600895	50.028941
493.073937	104.721043	50.033946
490.147072	89.328732	50.038951
485.913032	97.651358	50.043956
482.472499	95.788819	50.048961
478.508153	107.701254	50.053965
475.510038	97.815627	50.058970
471.749311	98.736766	50.063975
468.673645	94.064578	50.068980
465.162616	92.295347	50.073985
461.574033	94.812556	50.078989
457.856896	98.624914	50.083994
454.346441	96.096285	50.088999
451.096755	99.911360	50.094004
447.823184	94.707021	50.099009
443.628089	97.603978	50.104013
440.079924	89.421227	50.109018
436.994941	85.272540	50.114023
433.465205	93.930964	50.119028
430.119055	94.069002	50.124033
426.174509	91.899448	50.129037
423.090178	91.822470	50.134042
419.693741	93.926779	50.139047
416.147291	94.130998	50.144052
412.880642	89.564679	50.149057
409.038277	98.392306	50.154061
405.425093	98.717714	50.159066
402.030059	93.048360	50.164071
398.399771	89.206566	50.169076
394.870764	84.706661	50.174081
391.203733	87.647477	50.179085
387.680531	91.543380	50.184090
384.351368	86.107330	50.189095
380.682940	89.877284	50.194100
377.506134	86.454856	50.199105
373.739096	95.397247	50.204109
370.572892	89.885055	50.209114
367.273191	92.426653	50.214119
363.586149	92.001173	50.219124
359.972646	83.705308	50.224129
356.396067	101.270853	50.229133
353.046982	85.887798	50.234138
349.640133	88.506298	50.239143
345.702640	92.008360	50.244148
342.710783	89.996501	50.249153
338.715746	89.986277	50.254157
335.367157	87.093817	50.259162
331.772000	86.714070	50.264167
327.952838	94.383304	50.269172
324.772571	79.005463	50.274177
321.131649	93.088261	50.279181
318.129984	83.342472	50.284186
314.391439	88.227598	50.289191
310.956784	92.884787	50.294196
307.486304	83.705992	50.299201
303.693177	85.742767	50.304205
300.704560	88.843106	50.309210
296.895472	87.667971	50.314215
293.616835	94.986787	50.319220
289.916259	84.945526	50.324225
285.855955	79.911957	50.329229
282.911309	84.002007	50.334234
279.651374	90.855983	50.339239
275.643432	92.217731	50.344244
272.276380	81.447183	50.349249
268.702657	77.213770	50.354253
265.148927	77.741896	50.359258
261.619852	83.144727	50.364263
258.169844	88.626924	50.369268
254.605319	82.174258	50.374273
251.290558	88.097184	50.379277
247.764752	81.246145	50.384282
244.453803	85.140487	50.389287
240.582609	85.772138	50.394292
237.514609	84.436642	50.399297
233.636436	90.295974	50.404301
230.249406	81.480635	50.409306
226.685237	81.564317	50.414311
223.294971	84.183428	50.419316
219.948670	80.268754	50.424321
216.013764	81.277397	50.429325
212.676163	77.585993	50.434330
209.272978	81.656148	50.439335
205.765108	85.711067	50.444340
202.583946	84.070604	50.449345
198.765890	88.604395	50.454349
195.434754	79.008352	50.459354
191.702122	83.443340	50.464359
187.990809	77.760355	50.469364
184.683990	78.866771	50.474369
181.319227	83.408650	50.479373
177.895475	78.901843	50.484378
174.332341	81.203200	50.489383
170.519632	79.158647	50.494388
167.294403	75.478132	50.499393
163.674717	82.363190	50.504397
159.970878	71.598006	50.509402
156.747541	84.210705	50.514407
153.036904	90.524717	50.519412
149.640359	82.770775	50.524417
145.678255	83.157280	50.529421
142.756184	82.586740	50.534426
139.134768	81.629049	50.539431
135.989587	82.033110	50.544436
132.216467	93.640446	50.549441
128.640250	80.707066	50.554445
125.017115	83.074791	50.559450
121.653775	85.778307	50.564455
117.852162	86.772438	50.569460
114.764420	82.947015	50.574465
111.262358	88.459565	50.579469
108.175736	81.318319	50.584474
104.240603	77.476963	50.589479
100.483397	82.716274	50.594484
96.952069	77.198126	50.599489
93.769918	77.051167	50.604493
90.247170	76.906951	50.609498
86.527817	76.850486	50.614503
83.341976	82.712139	50.619508
79.906639	77.640873	50.624513
76.132540	80.756775	50.629517
72.489549	88.382681	50.634522
69.128377	83.654142	50.639527
65.193867	78.876226	50.644532
62.277430	91.333302	50.649537
58.837561	93.292687	50.654541
54.830295	81.458274	50.659546
51.331633	72.065722	50.664551
48.083367	81.170553	50.669556
44.935582	80.755634	50.674561
40.986087	87.869583	50.679565
37.475040	84.898294	50.684570
34.317064	81.431922	50.689575
30.264983	82.911428	50.694580
27.227679	76.787558	50.699585
23.859342	86.474364	50.704589
20.472678	90.086415	50.709594
16.509551	89.906821	50.714599
12.697000	89.940921	50.719604
9.893375	86.801857	50.724609
6.274251	91.617771	50.729613
2.621128	84.024321	50.734618