Thu Aug 25 13:24:40 2022

Number of Points = 9925

Depth (nm)	Load (N)	Time (s)
1.553528	101.302071	0.000000
1.833989	103.403084	0.005005
1.723512	105.185697	0.010010
1.575010	114.266792	0.015014
1.791402	103.146896	0.020019
1.571182	96.309575	0.025024
1.591229	90.636848	0.030029
1.247264	86.909935	0.035034
0.959038	74.726997	0.040038
0.818830	59.939235	0.045043
0.072942	59.451733	0.050048
0.118524	45.330904	0.055053
-0.163520	52.272034	0.060058
-0.379379	40.144221	0.065062
-0.450516	36.928231	0.070067
-0.688301	32.672161	0.075072
-0.962677	12.713712	0.080077
-1.124887	23.726807	0.085082
-1.432212	14.410116	0.090086
-1.822287	3.964275	0.095091
-2.421595	21.537904	0.100096
-2.751957	0.471431	0.105101
-3.407189	9.530629	0.110106
-4.159305	11.037278	0.115110
-3.850105	10.045940	0.120115
-3.924890	13.271957	0.125120
-4.223016	7.411826	0.130125
-4.421005	16.525936	0.135130
-4.359317	10.884675	0.140134
-4.279498	4.319919	0.145139
-4.672992	13.145118	0.150144
-5.391822	5.060339	0.155149
-5.539132	15.621839	0.160154
-5.599277	13.340606	0.165158
-5.607095	3.641634	0.170163
-6.433581	5.270667	0.175168
-7.396519	11.021323	0.180173
-7.279015	8.114304	0.185178
-7.406930	6.232834	0.190182
-7.489654	9.703703	0.195187
-7.604673	16.941354	0.200192
-7.460341	12.850045	0.205197
-7.525768	3.571389	0.210202
-8.129663	13.650769	0.215206
-8.468322	11.125272	0.220211
-8.746671	16.699062	0.225216
-8.976576	13.836985	0.230221
-9.117339	15.807832	0.235226
-10.112540	18.007471	0.240230
-10.234464	11.642002	0.245235
-10.320180	11.677490	0.250240
-10.164449	15.623529	0.255245
-10.457178	5.200401	0.260250
-10.712266	19.512035	0.265254
-10.500794	15.634834	0.270259
-11.344637	14.324284	0.275264
-11.545348	13.906389	0.280269
-11.804768	18.895080	0.285274
-11.863460	12.855063	0.290278
-12.466379	12.012968	0.295283
-13.181745	10.552574	0.300288
-13.316356	13.503225	0.305293
-12.850731	12.743642	0.310298
-13.139807	11.083577	0.315302
-13.080427	10.267424	0.320307
-13.495104	10.737271	0.325312
-13.998931	8.538212	0.330317
-14.019972	18.219385	0.335322
-14.547555	14.492784	0.340326
-14.431540	14.768748	0.345331
-15.616637	14.103292	0.350336
-15.642424	15.072193	0.355341
-15.663104	12.895509	0.360346
-15.989663	13.610978	0.365350
-15.971756	13.712488	0.370355
-16.039778	16.700163	0.375360
-16.440022	11.874766	0.380365
-17.221647	10.608253	0.385370
-17.626475	12.813465	0.390374
-17.090441	9.777593	0.395379
-17.328773	-0.410444	0.400384
-17.464098	13.825472	0.405389
-18.218977	10.688145	0.410394
-18.840225	17.631790	0.415398
-18.786632	15.108109	0.420403
-19.007431	13.332941	0.425408
-18.762224	11.570179	0.430413
-18.677592	15.283747	0.435418
-19.690900	16.103657	0.440422
-19.780525	12.615320	0.445427
-20.389721	7.670804	0.450432
-20.333092	7.212587	0.455437
-20.348370	12.007999	0.460442
-20.726945	7.549368	0.465446
-21.441973	2.260766	0.470451
-21.736524	14.791052	0.475456
-21.947602	17.351886	0.480461
-22.012109	15.669289	0.485466
-22.159966	19.852722	0.490470
-21.830502	9.971186	0.495475
-21.962712	17.341244	0.500480
-22.503162	19.260821	0.505485
-22.912492	12.930894	0.510490
-23.250061	15.989277	0.515494
-23.730544	16.409324	0.520499
-24.423749	16.751970	0.525504
-24.322019	8.965729	0.530509
-24.830835	11.234692	0.535514
-24.678639	16.016518	0.540518
-24.464994	4.121993	0.545523
-24.892038	15.454989	0.550528
-24.978697	5.610182	0.555533
-25.754515	10.145107	0.560538
-26.374180	7.976855	0.565542
-26.315676	9.331182	0.570547
-26.377319	17.984164	0.575552
-26.539939	16.794669	0.580557
-26.746660	14.507929	0.585562
-27.007311	8.293914	0.590566
-27.110454	6.149134	0.595571
-27.842004	7.826570	0.600576
-27.873560	7.701711	0.605581
-27.744388	13.983606	0.610586
-27.922063	12.283939	0.615590
-28.529803	4.694287	0.620595
-28.941075	15.338274	0.625600
-29.118845	13.189368	0.630605
-29.049551	10.093749	0.635610
-30.078345	14.370920	0.640614
-30.286685	7.405224	0.645619
-30.819736	18.985786	0.650624
-30.183542	15.355249	0.655629
-30.489169	5.734578	0.660634
-30.993714	12.985803	0.665638
-30.648548	7.217869	0.670643
-30.949360	13.022968	0.675648
-31.503936	8.553951	0.680653
-31.930091	6.361706	0.685658
-32.278362	13.509351	0.690662
-32.272226	11.239880	0.695667
-32.287880	17.215436	0.700672
-32.896644	15.985115	0.705677
-33.482041	4.642899	0.710682
-33.713340	22.832746	0.715686
-33.334526	14.215310	0.720691
-33.773945	18.643744	0.725696
-34.082205	15.800273	0.730701
-34.763568	3.454361	0.735706
-35.040550	10.438974	0.740710
-35.119238	7.787323	0.745715
-35.314604	15.572238	0.750720
-35.560785	14.490749	0.755725
-35.553299	6.307988	0.760730
-35.366009	12.194795	0.765734
-35.382997	11.631054	0.770739
-36.467055	17.077987	0.775744
-36.589967	13.367076	0.780749
-36.555464	11.966360	0.785754
-37.209808	14.340383	0.790758
-37.824962	4.935892	0.795763
-38.046571	14.888934	0.800768
-38.459724	21.625967	0.805773
-38.253099	19.030850	0.810778
-38.558648	20.416911	0.815782
-38.291132	17.454748	0.820787
-38.363716	12.663434	0.825792
-38.972863	17.805000	0.830797
-39.365402	12.655693	0.835802
-39.520884	12.629346	0.840806
-39.661871	15.736021	0.845811
-39.952291	15.132865	0.850816
-40.833638	22.708891	0.855821
-40.987202	19.278029	0.860826
-40.954582	18.643240	0.865830
-41.105348	16.471120	0.870835
-41.217394	15.444544	0.875840
-41.468590	1.923914	0.880845
-41.722373	11.135346	0.885850
-42.546823	14.355439	0.890854
-42.259051	4.274794	0.895859
-42.746048	9.039713	0.900864
-42.599447	12.778371	0.905869
-42.722309	5.119074	0.910874
-43.738840	16.493815	0.915878
-43.937501	5.619352	0.920883
-44.383220	11.561052	0.925888
-44.367070	4.038162	0.930893
-43.963363	10.903463	0.935898
-44.306374	12.713010	0.940902
-44.501909	12.072841	0.945907
-45.530302	9.503560	0.950912
-45.799711	19.144553	0.955917
-45.680947	15.598254	0.960922
-45.884025	15.272480	0.965926
-45.772270	9.256380	0.970931
-46.519882	12.366356	0.975936
-47.102120	9.777787	0.980941
-46.726803	10.886320	0.985946
-47.377309	20.213703	0.990950
-47.068680	17.014143	0.995955
-47.196739	10.548398	1.000960
-47.585590	16.898806	1.005965
-47.897703	16.023802	1.010970
-48.315191	25.691164	1.015974
-48.653600	20.454280	1.020979
-49.457004	14.616375	1.025984
-49.740781	16.603304	1.030989
-50.070562	12.529337	1.035994
-50.014903	22.771132	1.040998
-49.685640	9.127909	1.046003
-50.339169	21.309483	1.051008
-50.393919	13.193419	1.056013
-50.033722	8.555758	1.061018
-50.508508	10.563124	1.066022
-51.314052	14.802151	1.071027
-51.548875	24.235246	1.076032
-51.747189	16.106874	1.081037
-51.487087	13.803937	1.086042
-52.074599	16.015629	1.091046
-52.686987	13.166029	1.096051
-52.873207	19.608074	1.101056
-53.274985	12.865677	1.106061
-53.057356	16.922238	1.111066
-53.215297	12.416384	1.116070
-53.637814	12.251544	1.121075
-54.282735	8.100407	1.126080
-54.627088	20.125967	1.131085
-54.780735	17.096917	1.136090
-55.281742	27.033632	1.141094
-54.520350	24.864119	1.146099
-54.899306	14.451338	1.151104
-54.873334	21.970618	1.156109
-55.063522	21.152440	1.161114
-56.113320	26.603501	1.166118
-55.791950	17.378130	1.171123
-56.090092	25.843543	1.176128
-57.088863	17.255298	1.181133
-57.403378	13.080862	1.186138
-57.581633	16.876750	1.191142
-57.368249	21.921073	1.196147
-57.680582	25.586110	1.201152
-57.522549	6.651426	1.206157
-57.677900	14.101037	1.211162
-58.663446	24.471178	1.216166
-58.671605	23.384031	1.221171
-59.122719	18.130007	1.226176
-59.341908	20.935723	1.231181
-59.295527	17.397603	1.236186
-59.675882	13.657429	1.241190
-60.203381	19.219638	1.246195
-60.417870	17.981323	1.251200
-60.431437	27.496810	1.256205
-60.287397	24.981102	1.261210
-60.345455	25.841164	1.266214
-61.026113	10.347193	1.271219
-61.396230	22.965252	1.276224
-61.719751	14.334479	1.281229
-61.463703	8.336899	1.286234
-62.109278	29.312501	1.291238
-62.861226	25.804556	1.296243
-63.091399	24.252322	1.301248
-63.391065	10.309012	1.306253
-63.214274	13.372221	1.311258
-63.323937	23.665230	1.316262
-63.203902	15.626183	1.321267
-63.717538	25.814813	1.326272
-64.631617	17.282902	1.331277
-64.350797	12.904451	1.336282
-65.096138	24.249360	1.341286
-64.786912	17.012738	1.346291
-64.868455	17.313329	1.351296
-65.579126	19.914481	1.356301
-65.905002	8.512621	1.361306
-66.358444	22.722454	1.366310
-66.264138	16.038368	1.371315
-66.088180	22.474284	1.376320
-66.489670	22.277676	1.381325
-66.701290	9.320322	1.386330
-67.489621	24.661475	1.391334
-67.408462	14.723932	1.396339
-67.569751	17.792659	1.401344
-67.915872	19.055363	1.406349
-68.126232	24.134445	1.411354
-69.223454	20.310443	1.416358
-69.230563	16.480147	1.421363
-69.163972	18.121110	1.426368
-69.161266	18.642619	1.431373
-69.212106	17.489394	1.436378
-69.276418	20.587219	1.441382
-69.354629	15.512048	1.446387
-70.329256	15.082542	1.451392
-70.845761	23.980804	1.456397
-70.940599	5.487544	1.461402
-70.532043	21.811745	1.466406
-71.012150	23.000531	1.471411
-71.423996	18.702140	1.476416
-72.359683	23.913857	1.481421
-72.252221	12.320708	1.486426
-72.060763	17.719642	1.491430
-71.744995	16.005934	1.496435
-72.576394	21.498703	1.501440
-73.233125	20.006980	1.506445
-73.544994	16.050430	1.511450
-73.727506	19.185758	1.516454
-73.341877	19.691559	1.521459
-73.469244	16.373654	1.526464
-74.426126	21.604510	1.531469
-74.839872	11.377520	1.536474
-75.417959	23.569420	1.541478
-75.538900	17.143688	1.546483
-75.820432	20.712150	1.551488
-75.704557	15.840686	1.556493
-75.737369	16.317140	1.561498
-75.557388	9.230489	1.566502
-75.546002	17.653724	1.571507
-76.152798	25.072836	1.576512
-76.795704	24.964677	1.581517
-76.985922	17.505757	1.586522
-77.221058	23.987106	1.591526
-77.178679	11.850496	1.596531
-77.892267	20.804948	1.601536
-78.538292	25.768797	1.606541
-78.483507	9.374978	1.611546
-78.637307	13.113248	1.616550
-78.440922	7.574273	1.621555
-78.282482	10.273359	1.626560
-79.008688	12.465655	1.631565
-79.608937	9.487605	1.636570
-79.914098	16.008397	1.641574
-80.167408	13.991552	1.646579
-79.910528	2.213645	1.651584
-80.839032	20.867073	1.656589
-80.892591	13.276010	1.661594
-81.146121	17.589896	1.666598
-81.284562	19.731223	1.671603
-81.354952	19.685216	1.676608
-81.615251	21.481805	1.681613
-81.906982	11.852632	1.686618
-82.119176	17.419218	1.691622
-82.202185	19.276612	1.696627
-82.829764	14.888640	1.701632
-82.758212	16.873676	1.706637
-83.199199	26.589013	1.711642
-84.330827	24.526295	1.716646
-84.051852	22.925919	1.721651
-84.266296	12.231101	1.726656
-84.385384	22.769195	1.731661
-84.429804	21.523215	1.736666
-84.795604	26.452646	1.741670
-84.396870	25.858565	1.746675
-85.262042	18.081462	1.751680
-85.682152	18.061780	1.756685
-85.513612	16.390124	1.761690
-86.064026	16.011208	1.766694
-86.160703	20.692823	1.771699
-85.916924	14.763603	1.776704
-86.612415	15.631797	1.781709
-86.950259	6.617296	1.786714
-87.177684	23.069623	1.791718
-87.284306	11.677701	1.796723
-88.236282	19.650773	1.801728
-88.656179	18.039683	1.806733
-88.529235	13.599922	1.811738
-88.839950	28.473932	1.816742
-88.901446	21.241615	1.821747
-88.706692	11.238820	1.826752
-89.068008	20.916359	1.831757
-89.137100	1.580674	1.836762
-89.936129	15.164442	1.841766
-90.259238	17.366343	1.846771
-90.353320	20.503634	1.851776
-90.613051	11.767957	1.856781
-90.296929	7.251098	1.861786
-90.736663	14.280196	1.866790
-91.195266	18.056737	1.871795
-91.725218	13.713580	1.876800
-91.996686	19.355894	1.881805
-92.008624	17.373995	1.886810
-92.184193	17.575424	1.891814
-92.531756	12.925277	1.896819
-93.211559	23.035538	1.901824
-93.582021	18.161186	1.906829
-93.684382	16.237748	1.911834
-94.016349	15.296254	1.916838
-93.970998	14.336766	1.921843
-93.820409	20.615302	1.926848
-93.705933	19.056522	1.931853
-93.907635	14.582836	1.936858
-94.403118	9.927394	1.941862
-94.884242	22.904531	1.946867
-95.139773	13.703122	1.951872
-95.618309	17.011386	1.956877
-95.846201	17.398185	1.961882
-96.574617	16.863663	1.966886
-96.306960	10.139762	1.971891
-96.201525	8.892447	1.976896
-96.958206	3.986869	1.981901
-96.418566	15.557530	1.986906
-97.338118	19.355680	1.991910
-97.835464	11.593712	1.996915
-97.863821	20.303599	2.006912
-97.665632	15.416104	2.016909
-96.592961	13.416847	2.026906
-96.639847	16.506301	2.036902
-96.554907	19.163284	2.046899
-95.873553	21.299157	2.056896
-94.862721	14.174558	2.066893
-94.222555	20.568095	2.076890
-93.911710	12.333572	2.086886
-93.975549	17.497435	2.096883
-93.180116	16.669362	2.106880
-92.917986	13.805586	2.116877
-92.030812	15.668454	2.126874
-91.386445	16.466968	2.136870
-91.028170	13.591294	2.146867
-90.272279	11.597326	2.156864
-89.929011	14.733352	2.166861
-89.802350	17.443985	2.176858
-89.190781	14.937270	2.186854
-88.915389	20.820926	2.196851
-87.604593	25.832752	2.206848
-87.071136	19.223280	2.216845
-87.133335	20.997324	2.226842
-86.865289	12.104265	2.236838
-86.067817	17.117327	2.246835
-85.627602	21.334228	2.256832
-84.850085	14.715026	2.266829
-84.440912	13.820766	2.276826
-84.387585	17.227139	2.286822
-83.150523	12.854772	2.296819
-83.034030	19.190982	2.306816
-83.076974	11.927394	2.316813
-81.885794	11.553666	2.326810
-81.380377	9.288500	2.336806
-81.336167	15.604357	2.346803
-80.256276	14.570154	2.356800
-80.009345	17.379152	2.366797
-79.688068	24.126770	2.376794
-79.106704	15.856192	2.386790
-78.736089	16.751455	2.396787
-77.985577	13.393001	2.406784
-77.672846	20.411222	2.416781
-76.667659	14.801725	2.426778
-76.186729	13.303840	2.436774
-75.929317	20.137492	2.446771
-75.966977	14.520340	2.456768
-74.891940	11.893487	2.466765
-74.629389	13.274519	2.476762
-74.009620	11.507790	2.486758
-73.275569	13.454841	2.496755
-72.904571	16.820942	2.506752
-72.723561	11.400777	2.516749
-72.012898	10.611332	2.526746
-71.473354	11.210861	2.536742
-71.180905	10.043452	2.546739
-70.082267	4.216577	2.556736
-70.162251	9.712421	2.566733
-69.701155	14.581788	2.576730
-68.763984	21.926652	2.586726
-68.610031	19.605684	2.596723
-68.186298	17.742958	2.606720
-67.428859	17.978892	2.616717
-67.018768	19.824652	2.626714
-66.180821	16.408148	2.636710
-65.826402	12.766468	2.646707
-65.695101	14.161731	2.656704
-64.916466	22.833411	2.666701
-64.519720	24.583059	2.676698
-64.182238	16.445729	2.686694
-63.239052	18.676795	2.696691
-62.966824	17.135584	2.706688
-62.828445	15.957470	2.716685
-62.234335	11.882255	2.726682
-61.620840	20.921935	2.736678
-60.457520	22.833404	2.746675
-60.510982	22.230215	2.756672
-60.365156	12.377450	2.766669
-59.107075	16.447193	2.776666
-58.808998	12.101582	2.786662
-58.758127	20.222053	2.796659
-58.194606	15.175943	2.806656
-57.520000	15.862016	2.816653
-56.675532	17.281749	2.826650
-56.343695	18.103894	2.836646
-56.139903	22.034725	2.846643
-55.858564	24.803488	2.856640
-54.623374	15.112650	2.866637
-54.527093	17.314858	2.876634
-54.040578	17.732629	2.886630
-53.496877	16.551194	2.896627
-52.901471	13.799924	2.906624
-52.064855	13.598966	2.916621
-51.391745	19.249244	2.926618
-51.404649	18.566840	2.936614
-51.686458	15.626734	2.946611
-50.152380	19.250921	2.956608
-50.124346	20.307571	2.966605
-49.291291	21.893820	2.976602
-48.675508	15.936693	2.986598
-48.783036	19.045154	2.996595
-47.854570	23.210898	3.006592
-47.238413	26.804685	3.016589
-47.158924	17.789111	3.026586
-46.745094	19.105260	3.036582
-45.477670	21.177817	3.046579
-45.601909	18.897271	3.056576
-44.795278	19.983978	3.066573
-43.986571	13.280695	3.076570
-44.080649	17.356401	3.086566
-43.561143	21.526036	3.096563
-42.832501	21.018879	3.106560
-42.569293	19.567781	3.116557
-42.069433	15.009986	3.126554
-41.155918	20.198110	3.136550
-40.830560	15.807041	3.146547
-40.726279	20.463057	3.156544
-39.707233	18.079398	3.166541
-39.305757	13.046008	3.176538
-38.926771	14.830118	3.186534
-38.149297	14.679609	3.196531
-37.834992	16.109555	3.206528
-37.873580	8.259237	3.216525
-36.944421	8.357394	3.226522
-36.519291	11.347547	3.236518
-35.905851	7.798331	3.246515
-35.008752	10.499121	3.256512
-35.194362	14.734888	3.266509
-34.386908	18.979782	3.276506
-33.844313	17.979088	3.286502
-33.512850	14.911211	3.296499
-32.601407	16.177901	3.306496
-32.153867	14.463503	3.316493
-32.265912	11.363749	3.326490
-31.527064	10.044033	3.336486
-30.989546	13.422058	3.346483
-30.372188	15.152979	3.356480
-29.359294	18.535716	3.366477
-29.217747	17.502826	3.376474
-29.154936	13.339797	3.386470
-28.866239	11.767497	3.396467
-28.024384	12.877196	3.406464
-27.057363	17.543751	3.416461
-26.826309	13.972086	3.426458
-26.816286	15.034725	3.436454
-25.905910	12.497033	3.446451
-24.828768	15.014392	3.456448
-24.819510	14.176460	3.466445
-24.620999	20.803934	3.476442
-23.382473	17.280319	3.486438
-23.394547	12.147000	3.496435
-23.337718	16.949834	3.506432
-22.267869	12.853932	3.516429
-21.875902	16.834475	3.526426
-21.385448	13.399563	3.536422
-20.449376	15.058372	3.546419
-20.570691	22.550089	3.556416
-20.091326	13.851998	3.566413
-19.350436	16.260485	3.576410
-18.851529	10.514910	3.586406
-18.317888	14.428905	3.596403
-17.835096	19.903100	3.606400
-17.498046	18.798396	3.616397
-16.539559	15.549910	3.626394
-15.812568	14.475975	3.636390
-15.656270	19.130177	3.646387
-15.736381	17.118315	3.656384
-15.342000	23.157564	3.666381
-14.619314	13.119375	3.676378
-13.602756	6.770003	3.686374
-13.405905	13.309036	3.696371
-13.075055	12.610785	3.706368
-12.115420	19.119002	3.716365
-11.956459	19.952397	3.726362
-11.575599	22.173375	3.736358
-10.653494	17.764833	3.746355
-10.455949	16.704162	3.756352
-9.675066	18.545680	3.766349
-9.052886	15.489274	3.776346
-9.023278	18.557242	3.786342
-8.703027	22.989351	3.796339
-7.793610	13.105638	3.806336
-7.470094	10.580704	3.816333
-6.259264	12.921896	3.826330
-5.932389	13.763827	3.836326
-5.883375	10.832074	3.846323
-6.033493	18.011520	3.856320
-5.065242	25.373702	3.866317
-4.188151	22.489599	3.876314
-3.503142	32.560301	3.886310
-3.361165	24.700688	3.896307
-3.216342	30.880413	3.906304
-3.037742	40.488768	3.916301
-2.006015	51.531531	3.926298
-1.923501	58.804425	3.936294
-1.224771	75.119957	3.946291
-0.955565	96.530155	3.956288
-0.322073	110.366025	3.966285
0.000000	122.609127	3.971290
0.264232	133.821232	3.976294
0.626980	144.404132	3.981299
0.662993	139.570456	3.986304
0.316240	155.127276	3.991309
0.549829	146.023160	3.996314
0.495380	151.194911	4.001318
0.247851	154.213898	4.006323
0.874825	162.164263	4.011328
0.793831	174.376459	4.016333
0.716809	173.505740	4.021338
0.920588	174.758223	4.026342
0.810841	173.582579	4.031347
1.328215	167.278240	4.036352
1.063671	181.835099	4.041357
0.803797	169.492628	4.046362
0.991839	180.159872	4.051366
0.998614	171.901212	4.056371
1.252257	181.805195	4.061376
0.934351	174.793322	4.066381
1.089211	178.786991	4.071386
1.219181	182.873147	4.076390
1.031843	182.880265	4.081395
0.941155	180.853736	4.086400
1.050379	180.596085	4.091405
1.267940	177.205119	4.096410
1.163115	175.607918	4.101414
1.171388	180.203530	4.106419
1.175770	178.658822	4.111424
0.946694	189.964074	4.116429
1.637852	177.928174	4.121434
1.049728	185.746228	4.126438
1.368112	191.463859	4.131443
1.442451	186.655804	4.136448
1.276355	187.444215	4.141453
1.653730	182.272300	4.146458
1.406985	182.007147	4.151462
1.137262	176.724649	4.156467
1.457079	168.654227	4.161472
1.041154	180.121629	4.166477
1.253495	185.242097	4.171482
1.606062	192.204072	4.176486
1.388575	190.823842	4.181491
1.623574	180.615321	4.186496
1.761949	182.241890	4.191501
1.613324	178.288195	4.196506
1.215794	180.166412	4.201510
1.564994	179.725626	4.206515
1.413829	173.997440	4.211520
1.321887	174.264860	4.216525
1.415822	176.312849	4.221530
1.516262	174.132986	4.226534
1.374500	178.514821	4.231539
1.446892	177.598544	4.236544
0.979181	184.904178	4.241549
1.533858	192.451428	4.246554
1.831578	197.520556	4.251558
1.714912	197.972187	4.256563
1.262936	191.797574	4.261568
1.609493	200.285446	4.266573
1.776702	193.077332	4.271578
1.760600	206.155755	4.276582
1.746580	202.649207	4.281587
1.778181	200.426342	4.286592
1.980396	207.595382	4.291597
1.801348	184.382071	4.296602
1.278696	190.408651	4.301606
1.380990	185.805026	4.306611
1.421698	192.569089	4.311616
1.353308	194.351443	4.316621
1.686268	190.837989	4.321626
1.459205	193.831629	4.326630
1.547957	193.608824	4.331635
1.614433	189.105724	4.336640
1.691829	193.817061	4.341645
1.628788	192.827089	4.346650
1.790368	201.587557	4.351654
2.051380	208.750549	4.356659
2.104538	208.606088	4.361664
1.965983	202.932865	4.366669
2.075012	205.848537	4.371674
1.756835	199.589681	4.376678
1.649963	202.729009	4.381683
1.777143	201.044834	4.386688
1.519009	202.996127	4.391693
1.776910	214.022610	4.396698
1.831592	220.898391	4.401702
2.062161	226.190023	4.406707
2.259488	222.359287	4.411712
1.863556	223.607661	4.416717
2.148924	218.684273	4.421722
2.077438	216.376316	4.426726
1.504182	227.011008	4.431731
2.452571	224.625512	4.436736
2.037541	231.514781	4.441741
2.230272	228.523172	4.446746
2.428978	229.858713	4.451750
2.114128	226.582796	4.456755
2.024103	212.521048	4.461760
1.527233	220.312164	4.466765
2.201242	225.442566	4.471770
1.962750	228.162752	4.476774
1.985867	227.700289	4.481779
2.447454	232.737425	4.486784
2.424324	230.529459	4.491789
2.349901	225.529563	4.496794
2.029000	234.998405	4.501798
1.997790	226.033816	4.506803
2.150691	227.094955	4.511808
1.650120	226.866409	4.516813
1.626597	226.300520	4.521818
1.970335	231.859165	4.526822
1.928597	218.463737	4.531827
2.244079	234.271211	4.536832
2.272007	248.820264	4.541837
2.508152	254.098376	4.546842
2.600069	258.899206	4.551846
2.160339	243.863986	4.556851
2.329772	233.064585	4.561856
2.380363	245.980725	4.566861
2.546172	247.786502	4.571866
2.378632	235.609855	4.576870
1.961320	245.350077	4.581875
2.327191	250.981192	4.586880
2.194035	264.065342	4.591885
2.607766	252.155120	4.596890
2.601576	256.547370	4.601894
2.665368	251.199938	4.606899
2.728091	245.849511	4.611904
2.654008	252.163339	4.616909
2.475714	244.575896	4.621914
2.124948	241.808649	4.626918
2.585855	252.917246	4.631923
2.650682	258.994172	4.636928
2.664821	256.356413	4.641933
2.998486	252.722611	4.646938
2.592760	240.143512	4.651942
2.253679	234.352999	4.656947
2.634233	239.320574	4.661952
2.477173	252.449590	4.666957
2.865993	252.878971	4.671962
2.888887	244.083068	4.676966
2.198075	242.441632	4.681971
2.718638	239.620122	4.686976
2.474167	258.793058	4.691981
2.864885	255.640707	4.696986
3.048230	259.642586	4.701990
2.785715	252.789685	4.706995
2.831458	234.277313	4.712000
2.181957	245.756044	4.717005
2.291373	252.825745	4.722010
2.764682	258.408390	4.727014
2.887899	255.440323	4.732019
3.100569	253.268177	4.737024
2.956884	255.495777	4.742029
3.090375	251.684528	4.747034
2.685698	263.137565	4.752038
2.603100	257.139176	4.757043
3.019173	258.965854	4.762048
2.657912	260.265747	4.767053
2.764896	261.277134	4.772058
2.960039	256.459623	4.777062
2.631631	254.381746	4.782067
2.513833	254.741806	4.787072
2.929564	258.536428	4.792077
2.912748	250.768656	4.797082
3.023837	248.710504	4.802086
2.865921	257.340722	4.807091
3.204391	243.882538	4.812096
3.144277	257.812632	4.817101
3.333441	259.386957	4.822106
2.879718	264.409324	4.827110
2.929263	263.139111	4.832115
3.380328	251.741905	4.837120
2.800475	261.855622	4.842125
2.784806	252.436159	4.847130
2.872545	257.025668	4.852134
3.034268	255.864431	4.857139
3.328067	255.929043	4.862144
2.382812	256.839538	4.867149
2.965111	256.485616	4.872154
3.069617	261.382552	4.877158
2.898578	266.914296	4.882163
3.404825	262.740913	4.887168
2.883368	264.224097	4.892173
3.007147	275.768352	4.897178
3.271874	275.502154	4.902182
3.449069	281.953794	4.907187
3.463765	283.770597	4.912192
3.135720	273.466741	4.917197
3.167318	265.469910	4.922202
2.754506	272.415795	4.927206
3.084680	269.339368	4.932211
3.282650	278.575072	4.937216
3.344657	287.936489	4.942221
3.667082	273.585437	4.947226
3.447015	288.499252	4.952230
3.375780	286.118480	4.957235
3.739221	285.476140	4.962240
3.177765	284.067537	4.967245
3.621503	276.616741	4.972250
3.775727	282.746108	4.977254
3.416175	261.348535	4.982259
3.441518	262.859941	4.987264
2.855281	264.536776	4.992269
3.421734	271.889221	4.997274
3.280839	276.891052	5.002278
3.583426	280.583182	5.007283
3.526414	281.455748	5.012288
3.498844	289.625788	5.017293
3.211043	277.012366	5.022298
3.636940	282.754311	5.027302
3.552647	288.497100	5.032307
3.889300	285.530389	5.037312
3.341902	291.987995	5.042317
3.534453	282.504253	5.047322
3.731648	281.938583	5.052326
3.682631	287.811889	5.057331
3.705442	280.037894	5.062336
3.397133	287.021196	5.067341
3.374481	286.856975	5.072346
3.352386	282.791680	5.077350
3.432649	287.768353	5.082355
3.628794	284.377559	5.087360
3.186764	284.003795	5.092365
3.398037	284.625513	5.097370
3.542775	289.164970	5.102374
3.756123	290.776637	5.107379
3.646080	286.763088	5.112384
3.456616	294.445958	5.117389
3.591953	295.724994	5.122394
3.806048	306.767890	5.127398
4.276233	302.328060	5.132403
3.732633	292.833103	5.137408
3.659889	284.472953	5.142413
3.545249	290.938684	5.147418
4.098914	299.454266	5.152422
3.795472	305.057388	5.157427
3.884648	310.627469	5.162432
4.012914	308.914639	5.167437
4.079442	297.669404	5.172442
4.055216	280.946013	5.177446
3.546575	287.422855	5.182451
3.990616	282.794133	5.187456
3.855148	302.642913	5.192461
4.211368	301.881479	5.197466
4.385510	298.589045	5.202470
3.946163	290.703956	5.207475
3.931131	280.009361	5.212480
3.781525	290.865619	5.217485
3.844095	294.174571	5.222490
3.722802	288.457486	5.227494
3.511283	305.122730	5.232499
3.986955	307.272277	5.237504
4.324093	311.904982	5.242509
4.304345	310.857599	5.247514
4.147947	305.310528	5.252518
4.276698	310.551699	5.257523
4.609836	303.051781	5.262528
4.174556	294.957242	5.267533
3.969751	276.344875	5.272538
3.955294	283.993992	5.277542
4.117084	295.981566	5.282547
4.432756	298.352338	5.287552
4.053335	296.984816	5.292557
3.867344	296.862005	5.297562
4.315352	294.583377	5.302566
4.441092	304.134137	5.307571
4.328663	305.534253	5.312576
4.513378	312.582689	5.317581
4.392235	298.424506	5.322586
3.964160	294.982815	5.327590
3.715572	301.396769	5.332595
4.359841	301.124888	5.337600
4.430475	311.225300	5.342605
4.472232	306.254635	5.347610
4.271081	310.107958	5.352614
4.303521	307.922914	5.357619
3.972483	306.601595	5.362624
3.550453	311.846805	5.367629
3.975039	302.222291	5.372634
4.008932	312.337952	5.377638
3.866841	309.019132	5.382643
4.374730	332.196723	5.387648
4.170160	329.609041	5.392653
4.461101	338.390437	5.397658
4.702611	335.729697	5.402662
4.569972	333.424979	5.407667
4.957951	331.905577	5.412672
4.344927	329.957709	5.417677
4.534562	330.592310	5.422682
4.420764	328.303624	5.427686
4.248194	331.753832	5.432691
4.504736	329.657061	5.437696
4.654695	333.607240	5.442701
4.649553	323.053441	5.447706
4.914732	340.738711	5.452710
4.402946	328.869044	5.457715
4.634852	332.777908	5.462720
4.306572	331.079660	5.467725
4.680847	329.764891	5.472730
4.231700	337.194232	5.477734
4.285379	339.438376	5.482739
4.548523	337.631642	5.487744
4.409666	333.413785	5.492749
4.506568	339.811587	5.497754
4.456549	338.262733	5.502758
4.332261	333.394008	5.507763
5.122430	342.688822	5.512768
4.660546	350.958578	5.517773
4.729794	341.984518	5.522778
4.998458	344.131701	5.527782
4.391131	336.358336	5.532787
5.023964	341.615450	5.537792
4.633376	346.514050	5.542797
4.766540	358.781404	5.547802
5.162144	354.435507	5.552806
5.020046	359.054726	5.557811
4.967009	335.482944	5.562816
4.619862	330.608009	5.567821
4.475340	336.863299	5.572826
4.692161	348.453135	5.577830
4.645869	351.016672	5.582835
5.095432	343.704145	5.587840
5.111294	353.256329	5.592845
5.362046	358.029134	5.597850
5.304854	358.832128	5.602854
4.994453	342.792610	5.607859
4.739400	336.216924	5.612864
4.751495	344.092867	5.617869
4.684438	353.272056	5.622874
5.064906	360.134811	5.627878
5.042006	361.963840	5.632883
5.084205	360.609348	5.637888
4.937385	360.964465	5.642893
5.100894	358.806337	5.647898
5.382532	363.922326	5.652902
5.000815	364.358542	5.657907
5.024075	363.611308	5.662912
4.914775	360.037398	5.667917
4.960562	360.501546	5.672922
5.045224	365.249756	5.677926
5.094075	360.657624	5.682931
5.512478	356.763745	5.687936
5.294124	364.821340	5.692941
5.220516	357.331345	5.697946
5.404606	359.419014	5.702950
5.053902	364.656228	5.707955
5.558792	361.495461	5.712960
5.353968	360.483401	5.717965
5.273874	358.040730	5.722970
4.968839	362.755083	5.727974
4.914744	364.430809	5.732979
5.138480	354.695364	5.737984
5.485202	363.724303	5.742989
5.157730	370.046236	5.747994
5.137034	368.325102	5.752998
5.005398	368.940438	5.758003
5.369420	362.217123	5.763008
5.231763	362.023462	5.768013
5.185015	362.071828	5.773018
5.327698	355.731217	5.778022
5.254565	357.786420	5.783027
5.283940	361.087930	5.788032
5.123213	368.266444	5.793037
5.141942	368.443759	5.798042
5.506280	380.795133	5.803046
5.336682	387.079680	5.808051
5.351970	378.076091	5.813056
5.365003	385.360267	5.818061
5.667564	386.970621	5.823066
5.346380	383.714651	5.828070
5.185785	383.774526	5.833075
5.114008	383.118115	5.838080
5.298244	378.273806	5.843085
5.290828	384.048874	5.848090
5.272668	386.677613	5.853094
5.487735	403.921532	5.858099
5.698284	397.643041	5.863104
5.682327	415.571756	5.868109
5.981064	405.125324	5.873114
5.933926	397.814667	5.878118
5.723497	388.947680	5.883123
5.940690	384.161483	5.888128
5.518276	390.166095	5.893133
5.273700	376.343573	5.898138
5.592658	391.853243	5.903142
5.893574	405.106772	5.908147
5.893961	397.630477	5.913152
5.631774	394.612039	5.918157
5.756279	393.997642	5.923162
5.769655	385.816945	5.928166
5.516915	406.956076	5.933171
6.113269	410.213053	5.938176
5.979708	419.390041	5.943181
5.825866	398.232162	5.948186
5.679478	391.724854	5.953190
5.608778	407.763837	5.958195
5.851305	415.065853	5.963200
5.673140	417.922152	5.968205
5.739594	411.109398	5.973210
6.040048	403.655689	5.978214
5.964012	412.586372	5.983219
6.066899	411.301464	5.988224
5.702445	404.622668	5.993229
5.502099	403.435893	5.998234
5.911550	397.531208	6.003238
5.624291	409.956222	6.008243
5.885235	413.196148	6.013248
5.651395	410.669989	6.018253
5.856813	410.156811	6.023258
5.959032	412.349066	6.028262
6.110171	410.300440	6.033267
5.926280	417.969834	6.038272
5.690381	418.275633	6.043277
5.673323	421.701492	6.048282
5.831316	421.366592	6.053286
5.900355	422.662352	6.058291
6.247466	412.926528	6.063296
5.969401	416.814071	6.068301
5.787732	403.332858	6.073306
5.814328	408.552098	6.078310
5.792753	416.727585	6.083315
6.065565	408.012670	6.088320
5.839686	406.269895	6.093325
5.775459	412.575907	6.098330
6.090261	415.835870	6.103334
6.058527	423.766172	6.108339
5.994157	414.936401	6.113344
6.119763	414.476858	6.118349
5.895689	414.480240	6.123354
6.015232	418.220061	6.128358
6.190967	413.674476	6.133363
6.376799	404.356242	6.138368
5.923475	393.999177	6.143373
5.689399	392.374751	6.148378
5.714831	387.498372	6.153382
5.355413	395.381925	6.158387
6.079943	402.526155	6.163392
6.021289	408.821801	6.168397
5.875900	413.596578	6.173402
6.046090	407.716722	6.178406
5.942259	409.694481	6.183411
5.668373	385.521306	6.188416
5.981361	405.261968	6.193421
5.830388	404.924857	6.198426
6.157323	403.838968	6.203430
5.966836	391.501291	6.208435
5.708244	386.647268	6.213440
5.854200	386.181373	6.218445
5.403562	395.303623	6.223450
5.638543	401.632355	6.228454
5.777939	409.576967	6.233459
5.938337	401.860458	6.238464
5.954480	414.921326	6.243469
6.007731	408.382732	6.248474
5.942400	410.041239	6.253478
6.080464	411.224940	6.258483
6.464366	406.513859	6.263488
6.073383	405.986557	6.268493
5.888541	393.280988	6.273498
6.223521	387.672720	6.278502
5.680150	392.914819	6.283507
5.904767	386.131078	6.288512
6.146116	386.580404	6.293517
5.995255	387.518301	6.298522
6.131430	391.195398	6.303526
5.969684	391.843928	6.308531
6.264799	384.359425	6.313536
5.950111	388.670327	6.318541
6.072031	386.373175	6.323546
5.977058	395.695968	6.328550
5.973743	391.124657	6.333555
5.975500	389.691076	6.338560
5.895963	380.136016	6.343565
5.773560	385.631701	6.348570
5.928996	386.556409	6.353574
5.589412	389.896751	6.358579
5.940938	382.681828	6.363584
5.811951	394.275255	6.368589
5.298491	388.103879	6.373594
5.652185	390.902151	6.378598
5.401584	390.412967	6.383603
5.684462	386.195458	6.388608
5.668313	382.233616	6.393613
5.457858	391.413147	6.398618
5.864779	406.415488	6.403622
5.847848	412.799513	6.408627
5.997217	404.439308	6.413632
6.062861	411.455818	6.418637
5.852042	417.291241	6.423642
5.792182	414.003811	6.428646
5.716609	412.158390	6.433651
5.915627	415.234008	6.438656
5.741904	412.420011	6.443661
5.835022	413.749964	6.448666
5.837174	410.883100	6.453670
5.795408	412.319611	6.458675
5.967400	405.620040	6.463680
6.336981	410.488139	6.468685
6.058878	410.382924	6.473690
6.175679	405.473241	6.478694
6.053838	393.564580	6.483699
5.929422	384.880277	6.488704
5.471669	388.523879	6.493709
5.368012	390.583868	6.498714
6.024410	402.051080	6.503718
5.819560	411.799233	6.508723
5.775008	412.597084	6.513728
5.964349	414.250491	6.518733
5.896133	417.608433	6.523738
6.007187	406.628243	6.528742
5.578857	417.183391	6.533747
6.037935	408.622794	6.538752
5.703281	412.813440	6.543757
6.034507	417.067438	6.548762
6.330667	414.347502	6.553766
5.855282	400.134008	6.558771
6.009469	396.917450	6.563776
5.733719	392.749501	6.568781
5.565282	396.284497	6.573786
5.973525	416.785387	6.578790
5.823646	417.688329	6.583795
6.033269	410.906928	6.588800
6.127804	413.473719	6.593805
6.212267	413.694521	6.598810
5.840345	396.892617	6.603814
5.481465	397.916892	6.608819
5.627684	394.783843	6.613824
5.806277	411.081170	6.618829
6.031324	408.362885	6.623834
6.461726	408.750953	6.628838
5.430034	404.296474	6.633843
5.562400	398.242209	6.638848
5.460651	406.123361	6.643853
5.764649	410.001963	6.648858
5.841506	411.511638	6.653862
6.110277	412.162318	6.658867
5.891000	418.850140	6.663872
5.969212	415.509438	6.668877
5.817332	415.915971	6.673882
6.173575	405.264371	6.678886
5.947318	410.061308	6.683891
5.910419	412.686659	6.688896
5.952060	419.086820	6.693901
5.846029	413.471711	6.698906
6.144052	411.950578	6.703910
5.852929	413.897570	6.708915
5.993718	410.917233	6.713920
5.922482	406.821644	6.718925
5.623716	406.276729	6.723930
5.734829	414.241595	6.728934
5.784606	421.934492	6.733939
6.012230	413.849931	6.738944
6.063343	420.368834	6.743949
6.128538	418.858871	6.748954
5.839127	398.532175	6.753958
5.747525	411.179641	6.758963
6.225513	406.352575	6.763968
5.728051	398.169652	6.768973
5.900301	393.311398	6.773978
5.875201	384.117976	6.778982
5.563993	394.749674	6.783987
5.845882	398.081231	6.788992
5.738293	406.504314	6.793997
5.861163	408.946439	6.799002
5.893134	400.845082	6.804006
6.097452	413.455675	6.809011
5.970111	399.269908	6.814016
5.980430	408.769205	6.819021
5.944173	414.393774	6.824026
6.391975	396.046035	6.829030
5.625501	393.413502	6.834035
5.957315	385.353759	6.839040
5.801223	383.261523	6.844045
5.589315	385.063219	6.849050
5.896296	395.183596	6.854054
5.639587	407.553200	6.859059
5.992596	411.294406	6.864064
6.187987	409.416022	6.869069
6.251540	400.265650	6.874074
6.207314	387.987318	6.879078
5.586243	386.274827	6.884083
6.058698	395.511878	6.889088
5.938581	381.869173	6.894093
5.911487	387.802354	6.899098
5.999688	387.187317	6.904102
5.596962	396.226128	6.909107
5.703624	386.104039	6.914112
5.571251	382.837468	6.919117
5.766830	390.007621	6.924122
6.159432	383.960044	6.929126
6.070924	382.708290	6.934131
5.971429	380.727412	6.939136
6.016901	378.394781	6.944141
5.973619	379.863164	6.949146
5.888117	371.530284	6.954150
5.781971	387.135030	6.959155
5.824983	381.370025	6.964160
6.064365	379.111418	6.969165
5.954596	379.473386	6.974170
6.164292	381.114109	6.979174
5.677183	380.070345	6.984179
5.791549	377.242854	6.989184
5.888704	377.996354	6.994189
5.705729	383.191473	6.999194
6.059151	373.255360	7.004198
6.023975	377.361109	7.009203
5.931134	383.918374	7.014208
6.063395	386.213488	7.019213
5.910425	375.306324	7.024218
5.874859	377.621406	7.029222
5.893996	376.982388	7.034227
6.067509	386.304240	7.039232
6.043101	374.870719	7.044237
5.793503	390.580204	7.049242
5.993367	381.256620	7.054246
5.852188	382.107576	7.059251
6.138290	372.302237	7.064256
5.870683	377.336605	7.069261
5.655189	388.453188	7.074266
5.609841	382.702027	7.079270
5.822992	385.357800	7.084275
6.409365	379.235570	7.089280
5.976900	387.560847	7.094285
6.012245	381.923596	7.099290
5.623475	386.179664	7.104294
5.475107	382.134132	7.109299
5.662597	375.280280	7.114304
5.876223	386.196746	7.119309
5.792914	382.042941	7.124314
5.827925	379.642345	7.129318
5.839647	377.770595	7.134323
5.806630	383.767979	7.139328
5.758499	393.222640	7.144333
5.388468	388.490483	7.149338
5.735488	382.146321	7.154342
5.752591	397.140128	7.159347
5.912977	401.015919	7.164352
6.091159	406.568921	7.169357
5.962736	394.117111	7.174362
6.038804	381.785133	7.179366
5.579681	392.452661	7.184371
5.535959	392.016486	7.189376
5.751724	396.298062	7.194381
5.878092	408.022336	7.199386
5.967649	404.265395	7.204390
5.803401	415.057582	7.209395
6.183521	405.272296	7.214400
6.003522	407.299956	7.219405
5.673454	406.601753	7.224410
6.017170	405.152558	7.229414
5.938180	401.358750	7.234419
5.954783	405.573454	7.239424
5.880107	405.145293	7.244429
6.076232	407.797409	7.249434
5.916109	395.774518	7.254438
5.592641	385.517338	7.259443
5.967275	383.490646	7.264448
5.919830	402.923939	7.269453
5.600848	405.115747	7.274458
6.054338	404.519407	7.279462
5.899543	402.401654	7.284467
6.212794	403.839488	7.289472
5.990273	396.667045	7.294477
5.722526	381.633237	7.299482
5.667889	382.894586	7.304486
5.636907	390.606452	7.309491
5.901933	408.171586	7.314496
5.912962	405.328643	7.319501
5.775271	405.201428	7.324506
6.108362	407.870050	7.329510
5.940395	416.245648	7.334515
5.898398	408.934181	7.339520
6.146828	418.139904	7.344525
5.921865	398.502320	7.349530
6.426330	375.634094	7.354534
5.503109	382.561915	7.359539
5.830389	380.144000	7.364544
5.552734	381.500406	7.369549
5.674485	394.747197	7.374554
5.913098	402.597165	7.379558
5.916225	413.201771	7.384563
5.647933	414.895243	7.389568
5.715240	413.657038	7.394573
6.014052	414.413746	7.399578
5.483664	406.327730	7.404582
5.612680	410.186292	7.409587
5.719386	410.900330	7.414592
5.701925	411.276310	7.419597
5.975646	406.525544	7.424602
6.021988	407.378758	7.429606
5.688870	417.279892	7.434611
5.609999	414.318152	7.439616
5.487051	410.622981	7.444621
5.618633	414.275492	7.449626
5.776296	408.603249	7.454630
5.730491	417.260271	7.459635
5.762211	412.873296	7.464640
5.855830	417.056953	7.469645
6.103783	430.002415	7.474650
6.183033	420.087088	7.479654
6.074145	426.824057	7.484659
6.030479	419.209119	7.489664
6.064444	412.259081	7.494669
5.928246	421.784506	7.499674
5.987240	412.755067	7.504678
5.965516	418.658942	7.509683
5.844859	407.167714	7.514688
5.765685	401.599021	7.519693
6.044699	405.968769	7.524698
6.092787	403.759115	7.529702
5.778160	417.801979	7.534707
5.841396	406.500243	7.539712
5.990786	412.877191	7.544717
5.864057	417.813565	7.549722
6.089901	414.788262	7.554726
5.746440	413.032272	7.559731
5.796883	413.609590	7.564736
6.220514	409.974316	7.569741
5.906888	412.804380	7.574746
6.190949	409.864872	7.579750
6.178425	411.075332	7.584755
6.278453	409.509290	7.589760
6.029853	412.085551	7.594765
5.624340	405.919402	7.599770
6.356884	409.246791	7.604774
5.866056	398.933566	7.609779
5.624369	390.682097	7.614784
5.720581	396.747824	7.619789
5.829171	415.542899	7.624794
6.035872	405.822751	7.629798
5.952355	410.654273	7.634803
5.829277	406.576298	7.639808
5.936778	404.414284	7.644813
5.487823	414.023510	7.649818
6.076014	416.044707	7.654822
5.854564	420.651063	7.659827
5.974525	405.565979	7.664832
6.140420	409.134017	7.669837
6.036038	395.292678	7.674842
5.716178	387.458430	7.679846
5.974269	395.333817	7.684851
5.751549	384.703338	7.689856
5.867189	382.116098	7.694861
5.625288	389.285192	7.699866
5.922658	401.280069	7.704870
5.859830	407.570041	7.709875
5.810746	417.002718	7.714880
6.060676	412.284151	7.719885
6.025127	417.563752	7.724890
6.174940	402.318965	7.729894
5.857458	391.440731	7.734899
5.559299	384.327602	7.739904
5.815236	396.724447	7.744909
5.802762	416.256681	7.749914
5.943434	407.296708	7.754918
5.995011	419.956548	7.759923
5.890136	406.675278	7.764928
5.763784	401.433525	7.769933
5.640453	414.139749	7.774938
6.228559	409.048650	7.779942
5.961973	410.542532	7.784947
5.939054	400.415427	7.789952
5.780638	398.472253	7.794957
5.823435	407.058440	7.799962
6.087267	400.240074	7.804966
5.597406	395.915842	7.809971
5.817542	402.379782	7.814976
5.949125	408.386186	7.819981
6.067309	412.490061	7.824986
5.979974	398.611247	7.829990
5.766879	392.506705	7.834995
5.707306	406.639315	7.840000
6.155475	405.331946	7.845005
5.790406	401.598781	7.850010
5.971068	394.480229	7.855014
5.593983	391.002055	7.860019
5.788929	406.720998	7.865024
6.208738	410.945296	7.870029
6.110347	406.755883	7.875034
5.804009	389.867778	7.880038
5.732458	391.115959	7.885043
5.847510	391.844509	7.890048
5.950839	399.956124	7.895053
5.754124	402.214198	7.900058
5.805106	406.853798	7.905062
5.984043	415.181370	7.910067
6.032409	401.278127	7.915072
5.927645	392.698311	7.920077
5.790562	387.287397	7.925082
6.069208	383.181287	7.930086
5.425922	393.985241	7.935091
5.808216	403.198457	7.940096
6.209799	406.175895	7.945101
5.740992	400.225315	7.950106
5.950868	402.362734	7.955110
5.644753	406.450828	7.960115
5.729420	410.547299	7.965120
6.195041	412.249168	7.970125
5.932321	410.950826	7.975142
5.862207	413.738798	7.980160
5.962750	414.262592	7.985178
5.859900	418.643045	7.990195
6.015668	409.984369	7.995213
5.595076	421.956893	8.000230
6.107774	410.865997	8.005248
5.973384	408.251900	8.010266
6.038324	406.916214	8.015283
6.133375	407.314637	8.020301
6.059282	400.329824	8.025318
5.774774	378.984548	8.030336
5.638989	395.396767	8.035354
5.852551	406.386305	8.040371
6.310466	404.023383	8.045389
5.760687	402.828194	8.050406
5.842225	408.246403	8.055424
6.172013	417.731371	8.060442
6.010623	409.725140	8.065459
5.982267	413.598465	8.070477
5.853627	416.790079	8.075494
5.783711	407.646063	8.080512
5.965490	413.193733	8.085530
6.035002	409.979649	8.090547
6.061778	414.469177	8.095565
5.520639	414.796869	8.100582
5.884354	409.621138	8.105600
5.975667	413.223251	8.110618
5.859530	403.373276	8.115635
6.019958	403.767767	8.120653
5.675224	407.589677	8.125670
5.669591	405.542378	8.130688
6.133825	410.196891	8.135706
6.034485	403.496895	8.140723
6.204976	408.762313	8.145741
5.932344	408.315797	8.150758
6.231233	401.405086	8.155776
6.266010	413.180025	8.160794
6.132056	407.558413	8.165811
5.990605	397.702940	8.170829
5.899993	407.089672	8.175846
5.958968	406.790012	8.180864
5.907145	403.118420	8.185882
5.795476	409.116005	8.190899
5.998948	412.296606	8.195917
5.989904	422.838200	8.200934
6.299050	423.827922	8.205952
6.007710	418.710643	8.210970
6.016687	427.393824	8.215987
6.255072	428.688120	8.221005
6.468645	431.324349	8.226022
5.987656	415.604997	8.231040
5.996221	427.888975	8.236058
6.224814	437.658050	8.241075
6.273805	433.184869	8.246093
6.325808	432.939949	8.251110
6.022865	416.204943	8.256128
6.003500	420.042147	8.261146
6.296683	431.167546	8.266163
6.241895	434.281320	8.271181
6.136659	437.879521	8.276198
6.463116	436.079984	8.281216
6.269884	425.314279	8.286234
5.965048	424.115424	8.291251
6.161119	417.956110	8.296269
6.446197	436.104369	8.301286
6.233231	427.206817	8.306304
6.328781	420.624600	8.311322
6.050247	415.319125	8.316339
6.189322	416.972958	8.321357
6.217307	432.718931	8.326374
6.189963	437.131739	8.331392
6.439966	440.828913	8.336410
6.157382	431.443655	8.341427
6.646702	429.296712	8.346445
6.300875	420.561990	8.351462
6.262828	411.984172	8.356480
6.461163	415.399106	8.361498
5.954158	412.190146	8.366515
6.183145	410.487933	8.371533
6.224209	430.627839	8.376550
6.501436	428.798148	8.381568
6.311200	417.381890	8.386586
6.153067	424.866815	8.391603
6.228968	433.656278	8.396621
6.005084	432.921260	8.401638
6.096143	428.911697	8.406656
6.352515	437.174273	8.411674
6.389026	431.169342	8.416691
6.210771	429.546715	8.421709
6.626407	442.309714	8.426726
6.291308	436.899488	8.431744
6.231261	434.936450	8.436762
6.264866	443.287580	8.441779
6.383927	434.123409	8.446797
6.135423	441.821315	8.451814
6.299498	445.819129	8.456832
6.496487	438.466782	8.461850
6.033924	443.578938	8.466867
6.232739	437.059429	8.471885
6.475560	436.746743	8.476902
6.062882	444.211599	8.481920
6.382009	430.153037	8.486938
6.273149	443.348508	8.491955
6.034825	437.310898	8.496973
6.331196	450.177796	8.501990
6.621134	460.315965	8.507008
6.543596	462.783219	8.512026
6.595822	456.965163	8.517043
6.402126	443.068992	8.522061
5.987775	455.160479	8.527078
6.433952	455.551225	8.532096
6.779810	458.106772	8.537114
6.561423	460.476175	8.542131
6.621280	459.908135	8.547149
6.540407	455.158652	8.552166
6.309790	458.060141	8.557184
6.761770	458.383707	8.562202
6.162588	463.482560	8.567219
6.678757	457.418245	8.572237
6.723321	461.371672	8.577255
6.642948	458.824842	8.582272
6.553854	445.735936	8.587290
6.177546	445.192056	8.592307
6.452292	450.248649	8.597325
6.054645	469.737821	8.602343
5.889886	462.700918	8.607360
6.526979	454.708412	8.612378
6.584805	462.686531	8.617395
6.639696	464.359871	8.622413
6.843403	458.953577	8.627431
6.701592	460.499948	8.632448
6.727025	456.352340	8.637466
6.397416	456.627955	8.642483
6.790483	459.624226	8.647501
6.786915	457.077985	8.652519
6.335670	466.685354	8.657536
6.471732	467.957815	8.662554
6.256493	474.072634	8.667571
6.752066	463.479847	8.672589
6.803116	465.570351	8.677607
6.657563	475.240280	8.682624
6.703029	473.330133	8.687642
6.801809	476.527150	8.692659
7.140498	463.939245	8.697677
6.796728	468.606765	8.702695
6.376073	471.727378	8.707712
6.667394	462.220624	8.712730
6.314318	467.129441	8.717747
6.642347	470.091722	8.722765
6.753897	467.830398	8.727783
6.811765	467.821242	8.732800
6.972080	476.562786	8.737818
6.627384	478.595378	8.742835
6.782091	470.350246	8.747853
6.628211	466.764058	8.752871
6.357420	470.965712	8.757888
6.617945	461.738337	8.762906
6.515133	467.324302	8.767923
6.836199	463.275538	8.772941
6.565950	462.547783	8.777959
6.535421	470.126343	8.782976
6.801722	464.088552	8.787994
6.681631	465.776685	8.793011
6.672789	467.368493	8.798029
6.770251	469.357052	8.803047
6.716801	471.716392	8.808064
6.816085	466.001413	8.813082
6.853270	460.996748	8.818099
7.138180	471.151490	8.823117
7.014712	467.629964	8.828135
6.738278	465.596686	8.833152
7.175852	469.311813	8.838170
6.713319	461.968120	8.843187
6.667589	468.545523	8.848205
6.605889	457.923290	8.853223
6.730713	468.210410	8.858240
6.928394	469.302804	8.863258
6.576665	471.516377	8.868275
6.719143	476.833541	8.873293
7.394290	477.339889	8.878311
6.968039	473.916295	8.883328
6.869758	468.730883	8.888346
6.738857	470.676329	8.893363
6.842865	463.202842	8.898381
6.607403	466.821452	8.903399
6.817440	491.270990	8.908416
7.028521	492.269769	8.913434
7.057489	493.871434	8.918451
7.015081	491.025163	8.923469
6.954915	477.549852	8.928487
6.808180	480.823206	8.933504
7.254705	477.105074	8.938522
7.011119	473.895854	8.943539
6.793941	475.128989	8.948557
6.782455	476.667564	8.953575
6.720366	489.256142	8.958592
7.203734	489.404378	8.963610
6.869319	495.443204	8.968627
7.028732	498.510805	8.973645
7.098575	498.051651	8.978663
6.845631	502.023300	8.983680
7.286331	490.299857	8.988698
7.065963	488.084224	8.993715
6.884768	475.675597	8.998733
6.778934	485.594926	9.003751
7.126961	484.883905	9.008768
6.862418	490.687721	9.013786
6.707523	501.738205	9.018803
7.243587	495.408830	9.023821
7.149785	492.589546	9.028839
6.927944	498.661227	9.033856
6.949680	497.849852	9.038874
6.962268	496.105799	9.043891
7.013451	500.708289	9.048909
6.720371	490.308481	9.053927
7.266012	503.281527	9.058944
7.130043	501.046357	9.063962
7.041246	506.163083	9.068979
7.178910	497.608187	9.073997
7.308966	498.073711	9.079015
6.623927	501.406166	9.084032
6.964109	499.077456	9.089050
6.966828	489.940953	9.094067
6.620483	495.271597	9.099085
7.053942	502.300948	9.104103
6.760922	508.443744	9.109120
7.264009	517.223119	9.114138
7.317676	532.453919	9.119155
7.174410	520.029851	9.124173
7.407600	512.703360	9.129191
7.368325	511.709040	9.134208
7.052395	495.092759	9.139226
7.111876	495.916477	9.144243
7.017557	510.154282	9.149261
7.379405	509.788231	9.154279
7.468571	508.284641	9.159296
7.491904	502.998114	9.164314
7.123720	500.518463	9.169331
7.281190	498.925277	9.174349
7.426549	493.139955	9.179367
7.042140	494.055313	9.184384
6.987467	498.860579	9.189402
7.324220	494.632627	9.194419
7.165023	504.670780	9.199437
7.422642	499.975546	9.204455
6.995128	508.477851	9.209472
6.838530	507.549251	9.214490
7.290460	525.280141	9.219507
7.401283	522.551867	9.224525
7.436803	520.024739	9.229543
7.207672	522.515753	9.234560
7.347142	525.517055	9.239578
7.427804	525.854620	9.244595
7.186426	520.366568	9.249613
7.381189	523.236131	9.254631
7.324686	528.710719	9.259648
7.279845	525.176862	9.264666
7.514967	527.232221	9.269683
7.376166	523.397507	9.274701
7.464976	524.743648	9.279719
7.087726	523.303668	9.284736
7.440335	526.886954	9.289754
7.456845	528.197086	9.294771
7.318908	526.265177	9.299789
7.178007	521.502991	9.304807
6.985591	522.991024	9.309824
7.144135	525.231949	9.314842
7.513980	517.846175	9.319859
7.430079	522.356228	9.324877
7.599975	518.343760	9.329895
7.644664	529.312497	9.334912
7.415771	524.917546	9.339930
7.355111	523.964446	9.344947
7.203428	527.948637	9.349965
7.251746	518.625094	9.354983
7.239637	520.129056	9.360000
7.455158	525.065563	9.365018
7.664003	524.341634	9.370035
7.348786	527.448893	9.375053
7.689889	520.077088	9.380071
7.648118	522.365178	9.385088
7.360346	516.089138	9.390106
7.131661	521.533897	9.395123
7.321120	522.621272	9.400141
7.788734	537.828243	9.405159
7.336531	536.100206	9.410176
7.753812	539.171591	9.415194
7.741770	529.857500	9.420211
7.680802	529.734420	9.425229
7.450293	519.813939	9.430247
7.245750	518.634076	9.435264
7.269576	532.872323	9.440282
7.757927	539.293488	9.445299
7.937411	551.784300	9.450317
7.782757	537.566359	9.455335
7.466497	539.982665	9.460352
7.377793	529.102690	9.465370
7.603213	526.419576	9.470387
7.573555	545.074848	9.475405
7.748932	551.466160	9.480423
7.834504	558.647871	9.485440
7.856022	557.205369	9.490458
7.466520	536.469644	9.495475
7.309952	542.745706	9.500493
7.703154	545.047697	9.505511
7.668356	550.054989	9.510528
7.701714	553.132882	9.515546
7.815820	548.539017	9.520563
7.767507	550.026564	9.525581
8.217901	550.110540	9.530599
7.751181	540.668868	9.535616
7.899955	530.190339	9.540634
7.694892	521.506094	9.545651
7.334911	528.041240	9.550669
7.706073	542.591144	9.555687
7.679615	555.701203	9.560704
7.557474	556.360878	9.565722
7.817634	555.770918	9.570739
7.747850	559.391990	9.575757
7.924398	550.837288	9.580775
7.784377	551.578658	9.585792
7.813615	549.863549	9.590810
7.629334	546.402028	9.595827
7.905948	550.719902	9.600845
8.093639	548.721191	9.605863
8.097310	552.419115	9.610880
7.898933	530.362732	9.615898
7.830048	526.845265	9.620915
7.834881	530.997436	9.625933
7.712548	523.281679	9.630951
8.025632	518.110693	9.635968
7.852834	522.022452	9.640986
8.338731	526.304374	9.646003
7.801302	521.758950	9.651021
8.292695	526.800556	9.656039
7.870401	534.472083	9.661056
7.628293	533.433804	9.666074
7.874624	523.754187	9.671091
7.890196	529.930690	9.676109
8.020582	521.405325	9.681127
7.911253	529.769424	9.686144
7.559933	530.733247	9.691162
8.110227	525.218982	9.696179
7.634282	531.235814	9.701197
7.710315	527.799781	9.706215
7.920902	542.605218	9.711232
7.876593	541.425494	9.716250
8.060702	543.599300	9.721267
7.970334	548.864607	9.726285
7.923966	550.733700	9.731303
8.331505	554.062233	9.736320
7.939685	546.294016	9.741338
8.077408	534.630639	9.746355
7.700763	538.388148	9.751373
8.146147	538.236225	9.756391
8.424458	541.297827	9.761408
8.112924	538.102398	9.766426
7.974296	527.725705	9.771443
7.958067	528.709609	9.776461
7.873693	526.261226	9.781479
7.785541	540.980925	9.786496
7.941375	545.226204	9.791514
8.206901	545.654724	9.796531
8.013167	551.270741	9.801549
8.097622	557.269204	9.806567
8.340284	544.674198	9.811584
7.877703	549.171007	9.816602
8.016367	537.122474	9.821619
8.066506	548.939276	9.826637
8.124152	547.453245	9.831655
8.030693	548.218877	9.836672
7.940342	554.519283	9.841690
8.415102	551.591971	9.846707
8.254492	561.248526	9.851725
8.155296	545.074765	9.856743
8.129042	557.348509	9.861760
7.944964	552.839232	9.866778
8.266668	554.571760	9.871795
8.275598	544.762071	9.876813
8.247484	546.230674	9.881831
7.947497	551.134351	9.886848
8.289435	556.196226	9.891866
8.454025	547.416181	9.896883
8.099496	555.436860	9.901901
8.138305	549.321076	9.906919
8.062097	554.041370	9.911936
8.159955	552.460675	9.916954
8.306005	549.354494	9.921971
8.059975	558.080850	9.926989
8.397567	548.547866	9.932007
8.115938	560.748016	9.937024
8.305947	555.394333	9.942042
8.122389	548.350874	9.947059
8.106241	553.017576	9.952077
8.225384	554.800777	9.957095
8.406615	550.126966	9.962112
8.236989	555.597196	9.967130
8.279591	557.493375	9.972147
8.184696	557.284093	9.977165
8.423708	563.526585	9.982183
8.363228	566.701234	9.987200
8.587438	560.673162	9.992218
8.417432	556.433077	9.997235
8.112796	555.893742	10.002253
8.455041	553.078710	10.007271
8.487813	553.909772	10.012288
8.410280	566.406150	10.017306
8.329068	552.504892	10.022323
8.348103	558.592501	10.027341
8.238897	557.523930	10.032359
8.758759	573.994530	10.037376
8.183248	568.912264	10.042394
8.561777	575.568400	10.047411
8.400431	584.562366	10.052429
8.376992	584.155696	10.057447
8.782770	582.463637	10.062464
8.374438	576.951233	10.067482
8.412982	573.076099	10.072499
8.544366	578.792662	10.077517
8.420022	580.651885	10.082535
8.482535	577.763915	10.087552
8.270477	581.356791	10.092570
8.393528	587.715289	10.097587
8.607647	592.683593	10.102605
8.419773	579.101983	10.107623
8.472398	575.906294	10.112640
8.528624	587.728480	10.117658
8.596516	582.412857	10.122675
8.627042	580.473481	10.127693
8.584864	593.832184	10.132711
8.731553	581.757117	10.137728
8.569311	575.448764	10.142746
8.797940	581.733914	10.147763
8.634411	584.624911	10.152781
8.528715	590.848838	10.157799
8.624647	587.352873	10.162816
8.714085	583.810588	10.167834
8.848838	575.527509	10.172851
8.882250	588.110661	10.177869
8.903326	580.501797	10.182887
8.557904	569.665177	10.187904
8.911022	571.383317	10.192922
8.571050	556.484343	10.197939
8.531030	571.294355	10.202957
8.464917	581.033945	10.207975
9.012009	571.461812	10.212992
8.658128	581.173907	10.218010
8.974619	575.816179	10.223027
8.672969	564.174288	10.228045
8.595189	561.570232	10.233063
8.601464	567.965955	10.238080
8.780190	575.139389	10.243098
8.959397	574.300181	10.248115
8.564010	579.218813	10.253133
8.642732	579.162209	10.258151
8.981103	581.532755	10.263168
8.887706	585.378438	10.268186
8.854541	578.147302	10.273203
8.747280	584.295733	10.278221
8.676659	588.522856	10.283239
8.703128	585.937177	10.288256
8.540909	588.130538	10.293274
8.855990	586.446378	10.298291
8.839314	589.178667	10.303309
8.458528	591.172745	10.308327
8.826368	580.965976	10.313344
8.551556	581.024724	10.318362
8.592304	582.996935	10.323379
8.400462	580.341321	10.328397
8.243234	591.139761	10.333415
8.772491	600.571484	10.338432
8.939569	607.327034	10.343450
8.891022	603.512875	10.348467
9.202629	611.981473	10.353485
9.289510	615.265585	10.358503
9.367053	605.391464	10.363520
8.856306	597.042256	10.368538
8.656995	581.764616	10.373555
8.943566	589.457643	10.378573
8.968829	601.676008	10.383591
8.838805	605.066687	10.388608
8.842015	606.057017	10.393626
9.084093	595.914125	10.398643
8.835081	603.337625	10.403661
8.753890	594.308889	10.408679
8.796386	601.115514	10.413696
9.043727	608.221406	10.418714
9.101924	607.341197	10.423731
9.322428	601.250576	10.428749
8.989875	603.344395	10.433767
9.039495	603.595308	10.438784
8.958012	614.164144	10.443802
9.079721	605.046807	10.448819
8.837415	611.664530	10.453837
8.621805	606.125077	10.458855
8.904519	602.732387	10.463872
8.638802	605.538413	10.468890
8.911579	607.064018	10.473907
9.328266	616.882615	10.478925
9.097965	619.787236	10.483943
9.437092	593.086422	10.488960
9.227174	608.636296	10.493978
9.136887	602.629084	10.498995
8.864332	609.283104	10.504013
8.969031	611.112755	10.509031
9.522183	608.438239	10.514048
9.192369	614.454293	10.519066
9.077208	609.482923	10.524083
9.484030	607.841191	10.529101
8.834806	617.293468	10.534119
9.426261	615.351408	10.539136
9.000616	625.876345	10.544154
9.457995	624.602231	10.549171
9.513322	622.198217	10.554189
8.993487	614.292238	10.559207
9.124029	611.652379	10.564224
9.448094	621.059458	10.569242
9.334684	626.473564	10.574259
9.533639	613.913760	10.579277
9.397224	618.122796	10.584295
9.276104	603.918482	10.589312
9.038758	614.076239	10.594330
9.107897	616.094498	10.599347
9.198083	615.117759	10.604365
9.482165	632.704641	10.609383
9.344699	624.060248	10.614400
9.472304	627.722990	10.619418
9.389844	628.067181	10.624435
9.662262	618.989340	10.629453
9.420016	629.116314	10.634471
9.602766	622.476180	10.639488
9.395082	619.242374	10.644506
9.517742	620.829371	10.649523
9.487624	618.186281	10.654541
9.012112	616.278852	10.659559
9.704555	620.881884	10.664576
9.850396	629.092440	10.669594
9.710382	620.202295	10.674611
9.378286	603.007778	10.679629
9.005787	611.283761	10.684647
9.134762	605.583021	10.689664
9.435357	613.431651	10.694682
9.414720	618.957451	10.699699
9.551594	617.970241	10.704717
9.699651	624.312211	10.709735
9.620389	623.172672	10.714752
9.982316	628.001062	10.719770
9.808149	619.476031	10.724787
9.484618	608.011108	10.729805
9.445702	611.639978	10.734823
9.461715	596.852450	10.739840
9.443891	614.486618	10.744858
9.893695	618.748971	10.749875
9.635885	608.943170	10.754893
9.253534	603.382506	10.759911
9.668156	608.360424	10.764928
9.821775	616.610781	10.769946
9.567108	618.039148	10.774963
9.857003	615.667810	10.779981
9.542885	613.577303	10.784999
9.555587	604.985130	10.790016
9.799160	623.260003	10.795034
9.450772	611.300356	10.800051
9.821095	618.137674	10.805069
9.649405	630.724589	10.810087
9.430717	623.219545	10.815104
9.777913	621.830152	10.820122
9.378969	624.669678	10.825139
9.618379	621.359508	10.830157
9.608305	626.486025	10.835175
9.985482	624.741639	10.840192
9.822722	615.836126	10.845210
9.588145	631.778047	10.850227
9.707990	620.622344	10.855245
9.532963	636.037387	10.860263
9.378663	627.944740	10.865280
9.744152	624.580102	10.870298
9.639561	635.215687	10.875315
9.700751	626.215119	10.880333
9.670577	623.467896	10.885351
9.893973	629.113254	10.890368
9.466988	626.077909	10.895386
9.703622	647.547569	10.900403
9.971458	648.490128	10.905421
9.777194	653.453007	10.910439
10.153670	637.943091	10.915456
9.860645	639.601532	10.920474
9.552345	651.938467	10.925491
9.642118	649.652129	10.930509
9.672402	639.864289	10.935527
9.936587	642.126547	10.940544
10.224069	640.096411	10.945562
10.095934	655.516747	10.950579
10.322097	648.364871	10.955597
10.273573	654.545149	10.960615
9.992565	646.696409	10.965632
9.664698	634.073967	10.970650
10.083624	645.615300	10.975667
10.475809	639.709206	10.980685
9.841329	642.525679	10.985703
9.772183	642.735240	10.990720
10.295839	647.995888	10.995738
10.069050	643.871977	11.000755
10.078635	630.189962	11.005773
9.769609	640.560936	11.010791
9.899664	637.400441	11.015808
10.048990	645.692509	11.020826
10.115758	654.590809	11.025843
9.995339	653.085331	11.030861
10.114315	653.921825	11.035879
10.168207	655.245045	11.040896
10.150743	644.811430	11.045914
9.990117	644.243216	11.050931
10.311456	648.206968	11.055949
10.220636	659.503130	11.060967
9.973572	660.037214	11.065984
10.238724	647.975099	11.071002
10.126690	660.890360	11.076019
10.100037	650.461338	11.081037
9.880654	646.910623	11.086055
9.887842	651.908210	11.091072
10.101842	651.136132	11.096090
9.735552	655.965019	11.101107
9.884533	654.477291	11.106125
9.871851	646.444498	11.111143
9.866957	660.438038	11.116160
10.194558	675.805920	11.121178
9.972825	684.219260	11.126195
10.258430	671.415465	11.131213
10.215366	682.057217	11.136231
10.492131	681.594040	11.141248
10.706447	674.636515	11.146266
10.217360	689.617972	11.151283
10.255033	676.802526	11.156301
10.483273	674.683839	11.161319
10.368472	680.741966	11.166336
10.681111	666.002580	11.171354
10.511081	678.043312	11.176371
10.743450	680.913321	11.181389
10.085659	668.393041	11.186407
10.119754	673.203380	11.191424
10.355783	681.570243	11.196442
9.991624	683.205119	11.201459
10.286768	683.370226	11.206477
10.488021	684.591463	11.211495
10.180887	687.331407	11.216512
10.528444	680.308822	11.221530
9.975524	678.959470	11.226547
10.284421	686.443913	11.231565
10.304277	679.993382	11.236583
10.532429	679.973325	11.241600
10.777020	676.987382	11.246618
10.124682	687.743535	11.251635
10.283119	676.316662	11.256653
10.551596	673.200744	11.261671
10.499624	682.218649	11.266688
10.374016	678.056785	11.271706
10.704633	700.641566	11.276723
10.495762	702.558227	11.281741
10.494307	701.980851	11.286759
10.790793	708.223855	11.291776
10.880701	707.165103	11.296794
10.601743	701.408326	11.301811
10.209027	691.361685	11.306829
10.275331	698.410771	11.311847
10.661873	703.579309	11.316864
10.987372	707.558201	11.321882
10.779243	709.698810	11.326899
10.840514	711.005098	11.331917
10.875570	701.074464	11.336935
11.144251	697.336815	11.341952
10.974665	683.708078	11.346970
10.296748	690.927416	11.351987
10.173701	682.927678	11.357005
10.565097	687.786181	11.362023
10.853413	700.114877	11.367040
10.593850	702.358219	11.372058
10.752600	707.612942	11.377075
10.474277	700.372831	11.382093
10.233513	701.552871	11.387111
10.595692	708.656589	11.392128
10.623212	703.757512	11.397146
10.784145	707.850552	11.402163
10.742932	706.244297	11.407181
10.963522	708.743768	11.412199
10.802183	709.813535	11.417216
10.803157	707.370689	11.422234
11.027475	708.825000	11.427251
10.782278	704.126444	11.432269
10.911994	706.132067	11.437287
10.756278	707.705883	11.442304
10.827058	704.308510	11.447322
10.872573	714.267369	11.452339
10.992930	704.866169	11.457357
10.768396	713.324144	11.462375
10.397938	722.000647	11.467392
10.880673	716.383299	11.472410
11.057228	722.563049	11.477427
11.135305	720.168081	11.482445
11.328966	720.336465	11.487463
11.230667	714.967947	11.492480
11.152213	708.794742	11.497498
11.084991	709.212286	11.502515
11.176941	713.256175	11.507533
11.087714	709.186435	11.512551
10.961516	711.118546	11.517568
11.041921	708.126765	11.522586
10.702648	703.998373	11.527603
10.964291	702.802260	11.532621
10.858708	704.737452	11.537639
10.649931	709.027275	11.542656
11.073282	719.416089	11.547674
11.244290	728.784089	11.552691
11.091794	729.044581	11.557709
11.186776	721.468258	11.562727
11.066107	722.812521	11.567744
11.258792	721.728197	11.572762
11.168568	719.438495	11.577779
11.327471	729.089261	11.582797
11.209588	711.185730	11.587815
11.004951	714.673327	11.592832
11.282535	711.931519	11.597850
11.419713	728.711532	11.602867
10.988486	718.557300	11.607885
11.344256	723.099501	11.612903
11.290972	730.467140	11.617920
11.410601	727.223055	11.622938
11.330470	722.053661	11.627955
11.070590	714.245762	11.632973
11.420528	715.711950	11.637991
11.053602	724.157526	11.643008
10.958865	730.038955	11.648026
10.987566	732.177174	11.653043
10.925861	734.809243	11.658061
11.409055	728.276631	11.663079
11.076570	739.841083	11.668096
11.467503	747.126504	11.673114
11.422962	735.725085	11.678131
11.227637	731.697210	11.683149
11.337820	730.253425	11.688167
11.257994	742.633520	11.693184
11.494366	729.808994	11.698202
11.007655	737.042573	11.703219
11.263299	739.511310	11.708237
10.968967	733.523401	11.713255
11.091966	752.167594	11.718272
11.541611	754.836312	11.723290
11.824200	762.170274	11.728307
11.705024	770.567586	11.733325
11.902992	761.697000	11.738343
12.107866	751.193773	11.743360
11.652947	739.064537	11.748378
11.639444	727.973842	11.753395
11.599906	740.536972	11.758413
11.619139	735.333070	11.763431
11.500054	732.864850	11.768448
11.638332	733.559468	11.773466
11.371953	735.971140	11.778483
11.186866	739.029642	11.783501
11.527506	733.453488	11.788519
11.310086	729.176610	11.793536
11.311803	725.247252	11.798554
11.389854	751.106387	11.803571
11.594023	761.024634	11.808589
11.485674	755.247421	11.813607
11.396799	761.582381	11.818624
11.914081	754.391162	11.823642
11.589281	759.769001	11.828659
11.572211	757.306885	11.833677
12.012061	754.356608	11.838695
11.718685	763.118885	11.843712
11.780973	754.487312	11.848730
11.448511	751.689602	11.853747
12.043743	750.330764	11.858765
11.954128	742.549825	11.863783
11.383933	753.520366	11.868800
11.799354	757.125416	11.873818
11.941610	757.554321	11.878835
11.623648	766.134257	11.883853
11.941750	751.368699	11.888871
11.661052	763.190141	11.893888
11.842538	759.936359	11.898906
11.791087	758.937622	11.903923
11.862154	765.862911	11.908941
11.995286	755.910569	11.913959
11.598604	759.772250	11.918976
11.926334	756.943683	11.923994
11.866173	751.357737	11.929011
11.780208	755.505252	11.934029
12.023430	751.200375	11.939047
12.075246	761.376025	11.944064
12.091426	759.713435	11.949082
12.158439	759.150576	11.954099
11.834739	751.220116	11.959117
12.301795	747.697529	11.964135
12.044004	754.084200	11.969152
12.199069	763.719806	11.974170
12.001175	751.155813	11.979187
11.577988	758.887536	11.984205
11.995420	746.719444	11.989223
11.884112	748.996367	11.994240
12.197369	754.176402	11.999258
12.085860	755.784322	12.004275
11.796378	761.459588	12.009293
11.992324	755.991305	12.014311
11.829277	758.339452	12.019328
11.907089	756.474700	12.024346
12.144609	762.291458	12.029363
11.996491	770.459774	12.034381
12.212050	769.778965	12.039399
12.387466	775.889483	12.044416
12.266356	772.556877	12.049434
12.221111	761.067188	12.054451
11.989972	772.691523	12.059469
12.084453	763.127088	12.064487
12.355509	780.709845	12.069504
12.150545	782.925706	12.074522
12.329649	785.718870	12.079539
12.332086	783.127460	12.084557
12.314935	761.812419	12.089575
12.158651	770.288130	12.094592
12.130701	774.417091	12.099610
12.674973	782.899809	12.104627
12.133556	788.440986	12.109645
12.132126	774.142044	12.114663
12.279898	775.715652	12.119680
12.418670	779.695415	12.124698
12.495421	784.227700	12.129715
12.394581	790.775986	12.134733
12.707948	785.270362	12.139751
12.301230	770.529990	12.144768
12.178790	765.370368	12.149786
12.444477	777.027315	12.154803
12.541062	793.381400	12.159821
12.599009	791.081096	12.164839
12.453264	786.171275	12.169856
12.301968	769.715136	12.174874
12.520459	768.298560	12.179891
12.338647	774.843748	12.184909
12.448706	780.914015	12.189927
12.598676	783.863223	12.194944
12.536294	779.300106	12.199962
12.822410	788.129391	12.204979
12.390962	787.597293	12.209997
12.652690	781.960904	12.215015
12.777718	785.226448	12.220032
12.095142	777.181790	12.225050
12.677843	779.308953	12.230067
12.347599	788.095953	12.235085
12.474090	782.666947	12.240103
12.672763	784.993136	12.245120
12.521723	793.023063	12.250138
12.901148	783.376102	12.255155
12.698000	787.087544	12.260173
12.505069	784.678225	12.265191
12.680117	785.329213	12.270208
12.620628	782.886363	12.275226
12.563872	779.250180	12.280243
12.347858	786.258327	12.285261
12.377178	786.518734	12.290279
12.143807	795.341053	12.295296
12.158429	801.921746	12.300314
12.576964	803.361414	12.305331
12.981222	816.050725	12.310349
12.937458	813.564381	12.315367
13.250825	808.058749	12.320384
12.802098	799.993221	12.325402
12.684315	801.756763	12.330419
12.360416	814.304539	12.335437
12.717417	816.176732	12.340455
12.863655	808.216797	12.345472
13.000807	806.677262	12.350490
13.088748	802.074807	12.355507
12.768589	818.251212	12.360525
13.224754	812.587504	12.365543
13.362323	813.847131	12.370560
12.900782	808.333524	12.375578
13.217712	804.676656	12.380595
13.093372	798.188715	12.385613
12.869732	786.692246	12.390631
12.871676	792.990898	12.395648
13.039829	805.508909	12.400666
13.309808	801.534347	12.405683
12.733837	798.197265	12.410701
12.805570	796.314526	12.415719
13.416519	805.405351	12.420736
13.111948	800.873864	12.425754
13.102053	787.267366	12.430771
12.917291	783.474511	12.435789
13.303372	795.557580	12.440807
13.277948	781.814662	12.445824
13.119945	790.524183	12.450842
13.024521	781.753205	12.455859
12.975727	784.626257	12.460877
12.910442	785.015097	12.465895
12.785301	800.214180	12.470912
13.071953	808.825638	12.475930
13.333423	797.941127	12.480947
13.323255	810.730081	12.485965
13.094368	807.165044	12.490983
13.084630	808.198440	12.496000
13.126968	807.633134	12.501018
12.763825	806.370803	12.506035
12.895357	811.371043	12.511053
13.139164	812.307907	12.516071
13.100289	812.648428	12.521088
13.051872	813.485911	12.526106
13.105943	811.886807	12.531123
13.096411	824.473698	12.536141
13.564740	834.865000	12.541159
13.708212	832.863719	12.546176
13.392635	831.754881	12.551194
13.313741	818.127611	12.556211
13.246584	827.387811	12.561229
13.194754	836.759225	12.566247
13.501195	829.298050	12.571264
13.177245	839.807179	12.576282
13.551244	833.752390	12.581299
13.562405	845.121054	12.586317
13.472337	839.953183	12.591335
13.393699	831.580342	12.596352
13.516086	830.942532	12.601370
13.396691	825.675117	12.606387
13.045789	835.181752	12.611405
13.202261	830.467566	12.616423
13.374668	829.777737	12.621440
13.507124	837.845318	12.626458
13.666412	825.149568	12.631475
13.626323	830.908858	12.636493
13.412105	830.907619	12.641511
13.375228	826.823338	12.646528
12.991735	837.202937	12.651546
13.355903	843.545839	12.656563
13.420428	852.018550	12.661581
13.423815	855.432555	12.666599
13.889642	853.096738	12.671616
13.568076	858.196386	12.676634
13.708770	850.641249	12.681651
13.920002	860.328069	12.686669
13.650785	857.299523	12.691687
13.765642	850.357513	12.696704
13.677906	859.112863	12.701722
14.019726	852.255213	12.706739
13.623934	857.530594	12.711757
13.804815	855.491891	12.716775
14.164726	857.745490	12.721792
13.727011	865.252313	12.726810
13.632971	858.415615	12.731827
13.981718	853.939544	12.736845
13.614192	868.917883	12.741863
13.790089	859.539459	12.746880
13.674526	854.085240	12.751898
14.038158	855.306294	12.756915
14.067185	858.716282	12.761933
14.022378	855.109770	12.766951
13.956865	854.886413	12.771968
13.798328	857.824010	12.776986
13.991111	858.686819	12.782003
13.885774	856.708740	12.787021
13.932172	870.457719	12.792039
14.306203	857.078195	12.797056
14.482380	859.745595	12.802074
14.062096	853.755289	12.807091
14.267545	857.917129	12.812109
13.929041	866.124785	12.817127
14.403740	861.430159	12.822144
14.144460	861.600084	12.827162
14.070313	848.091970	12.832179
14.065432	852.659154	12.837197
14.047189	860.661992	12.842215
14.338560	851.508480	12.847232
13.818899	854.335398	12.852250
14.191519	855.315199	12.857267
13.973771	864.292896	12.862285
14.248527	861.876561	12.867303
14.133081	862.169119	12.872320
14.243949	860.854606	12.877338
14.076616	857.882681	12.882355
14.269765	849.681845	12.887373
13.916048	867.378358	12.892391
14.312942	852.284786	12.897408
14.334939	861.209138	12.902426
14.227760	854.368189	12.907443
14.473832	851.849050	12.912461
14.187909	856.807412	12.917479
14.038066	853.466669	12.922496
13.893061	857.115366	12.927514
14.155213	851.702954	12.932531
14.192526	851.573941	12.937549
14.161921	850.758127	12.942567
14.615835	861.568275	12.947584
14.612563	862.275608	12.952602
13.994141	850.253966	12.957619
14.418092	868.216802	12.962637
14.882684	870.491871	12.967655
14.696293	859.270390	12.972672
14.507375	868.701170	12.977690
14.235303	861.980729	12.982707
14.327215	859.694029	12.987725
14.305163	877.023001	12.992743
14.711596	874.901617	12.997760
14.200090	886.841357	13.002778
14.333013	885.857907	13.007795
14.121957	878.888054	13.012813
14.365204	880.093258	13.017831
14.590725	888.764826	13.022848
14.526489	884.063116	13.027866
14.889723	869.205181	13.032883
14.629956	878.681781	13.037901
14.547558	892.144839	13.042919
14.815769	881.454885	13.047936
14.709946	878.523812	13.052954
14.435294	876.108349	13.057971
14.975202	870.257931	13.062989
14.846229	886.281363	13.068007
14.697160	872.204293	13.073024
14.517627	878.461980	13.078042
14.517209	881.794534	13.083059
14.815583	882.779659	13.088077
15.004359	884.179592	13.093095
14.650083	882.694957	13.098112
14.875168	890.956334	13.103130
14.722664	873.708170	13.108147
14.523218	873.000862	13.113165
14.818184	879.092684	13.118183
14.858947	876.337463	13.123200
14.605544	879.495057	13.128218
15.196969	893.676218	13.133235
15.334351	893.604110	13.138253
14.666841	887.668307	13.143271
14.625680	878.904558	13.148288
14.942707	896.211980	13.153306
15.188635	906.587676	13.158323
15.077837	906.983649	13.163341
15.087728	911.277129	13.168359
15.193181	889.387297	13.173376
14.757650	883.547694	13.178394
14.644564	899.417168	13.183411
15.216268	902.619059	13.188429
14.690350	907.485647	13.193447
15.015440	911.016518	13.198464
15.301616	920.802083	13.203482
15.177461	912.875000	13.208499
15.444758	905.082250	13.213517
15.338530	910.012471	13.218535
15.199663	918.902096	13.223552
15.316404	910.757386	13.228570
15.518122	910.204976	13.233587
15.404111	896.516875	13.238605
14.797761	886.838116	13.243623
15.151590	884.166388	13.248640
15.210104	892.700021	13.253658
15.255681	904.672411	13.258675
15.242345	910.339171	13.263693
15.296193	905.555836	13.268711
15.146069	901.921634	13.273728
15.445046	901.275088	13.278746
15.003488	901.934328	13.283763
15.502392	905.239146	13.288781
15.434178	900.799990	13.293799
15.266813	902.164206	13.298816
15.586156	908.217505	13.303834
15.359372	908.129870	13.308851
15.632663	900.528690	13.313869
15.204771	911.243497	13.318887
15.271705	898.237113	13.323904
15.413333	904.412930	13.328922
15.184449	905.322875	13.333939
15.402984	905.960742	13.338957
15.230408	910.907671	13.343975
15.115970	897.860275	13.348992
15.310686	896.996533	13.354010
15.322058	909.223596	13.359027
15.650520	913.277812	13.364045
15.365502	923.471615	13.369063
15.425717	924.329952	13.374080
15.797277	924.871260	13.379098
15.635759	929.709162	13.384115
15.643709	934.252264	13.389133
15.878772	931.747463	13.394151
15.686924	930.369920	13.399168
15.662515	923.143584	13.404186
15.277263	927.842968	13.409203
15.771904	923.224099	13.414221
15.831253	930.088170	13.419239
15.786873	932.676527	13.424256
16.334098	925.019793	13.429274
15.870808	931.962597	13.434291
16.220669	923.986487	13.439309
15.756669	920.171082	13.444327
15.902563	913.116886	13.449344
15.687579	902.676198	13.454362
15.418415	905.306083	13.459379
15.818728	919.488805	13.464397
15.743944	921.352921	13.469415
15.981806	923.505729	13.474432
15.948912	925.984986	13.479450
16.223760	933.004645	13.484467
16.019070	932.528534	13.489485
16.017466	930.966546	13.494503
15.840605	922.050466	13.499520
16.330895	926.776773	13.504538
15.999743	926.897999	13.509555
16.110148	918.605953	13.514573
15.649734	917.447218	13.519591
15.828161	921.174642	13.524608
16.066018	925.473434	13.529626
16.032850	915.468163	13.534643
15.801629	909.296734	13.539661
16.208729	925.078416	13.544679
15.995785	922.946772	13.549696
16.021763	925.618781	13.554714
15.777535	921.106211	13.559731
16.054148	917.973198	13.564749
15.954709	928.339902	13.569767
16.015797	919.332891	13.574784
16.152111	908.578378	13.579802
15.940104	916.324418	13.584819
16.651947	924.913495	13.589837
16.208962	925.856986	13.594855
16.096306	921.421633	13.599872
16.202861	934.290219	13.604890
16.267706	945.117195	13.609907
16.533015	935.749969	13.614925
16.633344	939.918831	13.619943
16.186120	925.411899	13.624960
16.721757	929.181189	13.629978
16.103682	926.065277	13.634995
16.298295	926.691114	13.640013
16.520676	936.947439	13.645031
16.614681	941.372917	13.650048
16.343528	933.235323	13.655066
16.242489	947.228372	13.660083
16.635036	934.003683	13.665101
16.472031	949.716918	13.670119
16.431426	955.012417	13.675136
16.806112	948.452545	13.680154
16.609202	950.361046	13.685171
16.558201	939.484382	13.690189
16.753981	935.641339	13.695207
16.527325	940.208578	13.700224
16.797330	939.825351	13.705242
16.003021	942.199844	13.710259
16.248447	940.763255	13.715277
16.725721	942.253693	13.720295
16.709116	954.030727	13.725312
16.888962	941.461064	13.730330
16.622467	949.644853	13.735347
16.629860	944.193432	13.740365
16.721990	945.318174	13.745383
16.058819	944.367934	13.750400
16.706606	937.064675	13.755418
16.316570	944.706075	13.760435
16.710939	947.279340	13.765453
16.623098	943.209329	13.770471
17.163047	955.877480	13.775488
16.995676	951.479094	13.780506
16.679893	957.395232	13.785523
16.823948	950.600090	13.790541
16.696537	950.036130	13.795559
16.944943	958.025636	13.800576
17.097422	955.322328	13.805594
16.880604	959.443054	13.810611
17.003435	953.007849	13.815629
17.136026	941.152504	13.820647
16.891979	946.530370	13.825664
16.895647	938.059375	13.830682
16.659049	952.042108	13.835699
16.963072	955.409028	13.840717
17.338429	961.182164	13.845735
17.212360	964.985710	13.850752
17.483898	964.100460	13.855770
17.362339	962.727681	13.860787
17.420999	945.544194	13.865805
17.335835	939.965262	13.870823
17.283054	936.710284	13.875840
17.481148	938.067735	13.880858
17.417577	945.708479	13.885875
17.168291	933.575294	13.890893
17.385481	935.412600	13.895911
17.323190	944.337577	13.900928
17.010053	938.977405	13.905946
16.821876	946.495658	13.910963
16.976159	929.928376	13.915981
17.314133	934.192549	13.920999
17.011304	938.768566	13.926016
17.130560	933.286999	13.931034
17.321088	958.324067	13.936051
17.177053	953.189864	13.941069
17.479245	955.521948	13.946087
17.593239	970.393368	13.951104
17.160158	958.572992	13.956122
17.393763	955.143748	13.961139
17.121299	959.453076	13.966157
17.113925	953.836706	13.971175
17.192600	965.207491	13.976192
17.312811	958.242510	13.981210
17.456842	966.027463	13.986227
17.109515	963.452958	13.991245
17.367783	961.332688	13.996263
17.381932	967.152953	14.001280
17.785979	977.936270	14.006298
17.938656	977.830207	14.011315
17.449759	965.043409	14.016333
17.596815	955.240256	14.021351
17.761933	960.591888	14.026368
17.957565	964.524913	14.031386
17.479861	966.957102	14.036403
17.828305	957.333837	14.041421
17.742676	967.853038	14.046439
17.353147	965.717499	14.051456
17.774247	971.877954	14.056474
17.643623	982.012886	14.061491
17.632937	977.678309	14.066509
17.441049	980.223512	14.071527
17.679562	984.282369	14.076544
18.310067	982.712857	14.081562
17.814972	993.217332	14.086579
17.678241	977.535063	14.091597
17.821825	986.853847	14.096615
17.702697	987.241660	14.101632
17.831669	981.985777	14.106650
18.192447	981.881823	14.111667
17.797507	977.531711	14.116685
18.007081	973.023767	14.121703
17.988088	980.815333	14.126720
18.004008	987.367489	14.131738
17.944906	985.640932	14.136755
18.152184	993.630586	14.141773
18.288886	984.879944	14.146791
18.003723	983.179340	14.151808
17.899113	987.219374	14.156826
18.024989	981.960821	14.161843
17.873882	984.133554	14.166861
18.099127	977.552903	14.171879
18.045509	981.098942	14.176896
18.234257	974.656558	14.181914
18.186834	979.912106	14.186931
18.137325	970.751981	14.191949
18.134147	976.612834	14.196967
18.170907	980.583379	14.201984
18.151777	977.966917	14.207002
18.485223	969.712486	14.212019
18.577236	991.798523	14.217037
18.417118	985.710602	14.222055
17.897029	984.457069	14.227072
18.150572	979.610868	14.232090
18.550893	992.935251	14.237107
18.079894	994.987690	14.242125
18.376499	1002.941261	14.247143
18.432647	1003.601420	14.252160
18.626179	999.556739	14.257178
18.565451	994.674566	14.262195
18.535526	1002.537284	14.267213
18.765497	992.490741	14.272231
18.709807	1003.383976	14.277248
18.293544	986.767177	14.282266
18.592683	989.225979	14.287283
18.590642	990.889352	14.292301
18.743313	988.873989	14.297319
18.012019	1002.798570	14.302336
18.771190	1001.568666	14.307354
18.876066	991.945674	14.312371
18.869023	995.067845	14.317389
19.047745	994.364397	14.322407
18.694983	994.536346	14.327424
18.445810	982.813373	14.332442
18.627640	991.491837	14.337459
18.733299	997.821649	14.342477
18.860919	996.125797	14.347495
18.628176	997.907371	14.352512
18.864043	995.083692	14.357530
18.818847	1004.432063	14.362547
18.679923	1007.663263	14.367565
18.947118	999.444446	14.372583
18.651196	1008.361878	14.377600
19.039700	1002.803388	14.382618
19.135586	1001.548018	14.387635
18.724364	1002.196196	14.392653
18.775205	995.737541	14.397671
18.661605	1002.802311	14.402688
18.739416	1012.696315	14.407706
18.660793	1002.581349	14.412723
18.525850	1005.755120	14.417741
19.117504	1000.701299	14.422759
18.797996	996.752782	14.427776
18.883576	1007.775368	14.432794
19.245930	1024.179544	14.437811
19.271497	1028.315958	14.442829
19.638821	1012.987038	14.447847
19.172817	1003.548162	14.452864
19.292699	999.382475	14.457882
19.021057	999.052554	14.462899
19.040752	1006.172182	14.467917
19.258796	1005.664549	14.472935
18.865079	1000.572609	14.477952
18.954852	1021.797481	14.482970
19.487673	1023.525381	14.487987
19.254392	1024.243512	14.493005
19.747288	1013.736030	14.498023
19.514186	1016.445489	14.503040
19.210729	1006.460425	14.508058
19.632596	995.711612	14.513075
19.294113	994.672626	14.518093
19.513250	992.621602	14.523111
19.288678	993.227911	14.528128
19.409227	984.094784	14.533146
19.443035	996.747591	14.538163
19.169995	1004.768325	14.543181
19.388820	1005.049537	14.548199
18.955881	1022.850136	14.553216
19.498544	1013.439413	14.558234
19.772714	1017.767252	14.563251
19.532000	1016.899143	14.568269
19.485396	1011.115327	14.573287
19.526363	1016.713651	14.578304
19.253733	1012.590525	14.583322
19.254367	1018.946267	14.588339
19.370652	1022.828620	14.593357
19.332176	1025.573859	14.598375
19.356813	1045.884293	14.603392
19.989994	1049.868705	14.608410
19.970463	1046.558002	14.613427
19.601871	1052.962140	14.618445
19.896014	1034.864336	14.623463
20.007687	1038.141486	14.628480
19.961463	1044.630814	14.633498
19.738270	1029.659497	14.638515
19.815412	1037.903096	14.643533
19.994102	1037.906568	14.648551
19.836644	1041.453110	14.653568
19.779404	1039.634736	14.658586
20.165334	1044.358491	14.663603
20.027459	1046.983605	14.668621
19.897756	1043.093703	14.673639
20.075101	1041.087092	14.678656
19.861665	1041.855764	14.683674
20.158334	1040.925547	14.688691
20.192409	1040.651869	14.693709
20.334145	1031.023081	14.698727
20.017178	1027.544385	14.703744
20.089088	1037.278377	14.708762
20.249729	1026.374811	14.713779
20.120534	1030.229355	14.718797
20.120004	1024.810709	14.723815
20.124347	1040.201152	14.728832
20.197064	1045.115996	14.733850
20.318267	1043.222325	14.738867
20.281420	1047.409549	14.743885
20.536754	1040.909370	14.748903
20.320448	1028.401715	14.753920
19.936700	1033.706819	14.758938
20.043187	1034.109777	14.763955
20.235063	1042.568937	14.768973
20.413360	1042.291598	14.773991
20.605048	1042.154175	14.779008
19.993730	1044.298033	14.784026
20.143771	1035.579991	14.789043
20.020499	1048.525695	14.794061
20.211716	1041.852521	14.799079
20.271493	1036.964078	14.804096
20.124346	1042.538234	14.809114
20.624194	1041.203789	14.814131
20.439221	1044.016166	14.819149
20.476392	1061.266608	14.824167
20.438694	1066.514347	14.829184
20.579646	1072.128581	14.834202
20.706603	1060.649589	14.839219
20.778252	1066.205251	14.844237
20.662085	1058.103278	14.849255
21.251930	1058.392633	14.854272
20.731197	1039.608283	14.859290
21.110411	1033.836640	14.864307
20.593190	1034.738118	14.869325
20.509187	1036.019853	14.874343
20.823852	1036.920381	14.879360
20.658516	1037.204979	14.884378
20.529516	1031.696005	14.889395
20.617573	1045.457527	14.894413
20.955614	1045.969376	14.899431
20.911551	1052.622474	14.904448
21.000255	1058.895002	14.909466
21.004766	1054.718975	14.914483
21.226264	1054.359126	14.919501
20.931656	1041.412439	14.924519
20.610603	1043.753821	14.929536
20.909306	1051.151651	14.934554
21.047290	1051.805301	14.939571
20.958847	1059.191207	14.944589
20.988342	1058.675244	14.949607
20.908387	1058.059662	14.954624
20.835186	1065.301168	14.959642
21.217226	1057.723910	14.964659
21.119039	1061.949151	14.969677
21.185457	1056.602060	14.974695
21.183582	1054.942271	14.979712
21.236720	1059.273193	14.984730
21.246272	1060.827457	14.989747
20.989920	1050.850767	14.994765
20.944741	1055.676787	14.999783
21.221158	1058.505240	15.004800
20.791208	1058.140161	15.009818
21.374530	1054.170098	15.014835
20.777757	1062.686560	15.019853
21.054199	1078.712918	15.024871
21.600300	1081.666383	15.029888
21.440788	1086.756483	15.034906
21.644981	1086.181589	15.039923
21.395362	1078.760096	15.044941
21.224990	1081.639622	15.049959
21.255680	1077.238576	15.054976
21.324466	1085.316244	15.059994
21.757083	1077.008355	15.065011
21.698707	1074.256014	15.070029
21.464154	1086.701616	15.075047
21.556543	1080.476268	15.080064
21.383555	1082.390503	15.085082
21.627220	1071.028921	15.090099
21.632070	1078.567480	15.095117
22.076079	1077.175508	15.100135
22.095840	1073.053893	15.105152
21.500917	1086.840404	15.110170
21.760575	1074.261299	15.115187
21.860054	1077.571926	15.120205
21.777537	1074.813899	15.125223
21.531828	1080.299365	15.130240
21.477561	1078.944436	15.135258
21.790241	1069.074244	15.140275
21.820762	1077.189463	15.145293
21.680107	1074.689860	15.150311
21.907390	1067.250457	15.155328
21.406387	1071.390488	15.160346
21.636446	1075.277117	15.165363
21.858597	1087.499681	15.170381
22.088509	1091.468390	15.175399
22.034244	1093.313529	15.180416
22.196150	1091.208343	15.185434
22.130519	1100.187571	15.190451
22.524210	1093.031361	15.195469
22.041470	1083.503545	15.200487
22.056825	1069.605689	15.205504
21.975398	1084.110181	15.210522
21.836127	1076.920715	15.215539
22.014290	1092.937237	15.220557
22.016118	1091.564051	15.225575
22.396113	1097.055631	15.230592
22.303557	1106.897482	15.235610
22.119877	1098.146489	15.240627
22.175977	1098.049245	15.245645
22.008979	1100.161364	15.250663
22.642449	1084.358326	15.255680
22.342517	1094.447263	15.260698
22.550504	1095.045764	15.265715
22.507021	1092.846522	15.270733
22.452554	1085.694259	15.275751
22.770635	1087.888169	15.280768
22.243480	1090.485917	15.285786
22.437099	1085.421852	15.290803
22.379812	1091.600498	15.295821
21.993563	1089.934656	15.300839
22.273115	1097.821513	15.305856
22.294957	1094.024624	15.310874
22.389099	1095.190087	15.315891
22.376676	1090.909404	15.320909
22.320263	1099.615782	15.325927
22.883751	1112.245642	15.330944
22.793804	1129.475040	15.335962
22.746091	1125.906799	15.340979
22.896405	1103.400588	15.345997
22.747322	1103.225036	15.351015
22.886843	1086.066615	15.356032
23.006838	1083.172713	15.361050
23.052676	1087.577371	15.366067
22.669367	1082.165032	15.371085
22.617174	1082.643348	15.376103
22.709822	1084.235089	15.381120
22.871722	1096.457631	15.386138
23.130095	1108.885979	15.391155
22.986957	1109.640484	15.396173
23.098276	1107.861966	15.401191
22.776380	1097.993352	15.406208
22.967657	1107.228985	15.411226
23.114342	1112.277429	15.416243
23.633323	1111.154582	15.421261
22.739131	1102.994604	15.426279
23.137085	1100.347490	15.431296
23.246924	1101.955475	15.436314
23.078834	1102.404611	15.441331
23.075295	1091.892812	15.446349
23.008861	1103.974406	15.451367
23.319426	1106.885882	15.456384
23.174312	1110.095979	15.461402
22.885652	1108.323325	15.466419
23.520062	1110.729613	15.471437
23.155283	1113.551238	15.476455
23.311752	1106.511089	15.481472
23.088658	1115.477125	15.486490
23.462006	1116.321125	15.491507
23.450446	1107.751447	15.496525
23.155055	1113.456152	15.501543
23.477061	1104.168320	15.506560
23.445663	1110.702687	15.511578
23.386284	1108.247151	15.516595
23.749602	1100.306725	15.521613
23.331404	1106.125346	15.526631
23.398902	1102.892518	15.531648
23.338421	1113.748700	15.536666
23.561831	1115.553492	15.541683
23.288489	1102.587650	15.546701
23.425574	1107.179993	15.551719
23.472946	1105.310507	15.556736
23.540288	1118.841795	15.561754
23.781229	1126.393877	15.566771
24.101398	1126.125868	15.571789
23.537680	1127.700528	15.576807
23.692994	1118.482988	15.581824
23.397366	1134.277127	15.586842
23.904138	1136.207942	15.591859
24.228747	1131.972277	15.596877
23.681073	1136.927543	15.601895
23.559518	1132.973228	15.606912
23.878222	1134.138224	15.611930
23.594835	1138.269420	15.616947
23.852788	1137.010739	15.621965
23.688751	1134.265476	15.626983
23.855422	1125.623681	15.632000
23.984883	1127.089734	15.637018
23.668613	1132.674637	15.642035
23.677549	1132.253414	15.647053
23.782697	1150.083443	15.652071
24.108411	1151.329395	15.657088
24.393867	1153.610478	15.662106
24.561070	1153.950275	15.667123
24.734316	1145.834476	15.672141
24.390194	1133.832782	15.677159
24.611621	1124.008416	15.682176
24.587862	1124.879921	15.687194
24.443966	1120.525154	15.692211
24.253012	1122.896656	15.697229
24.111875	1129.476627	15.702247
24.318425	1125.688662	15.707264
24.196312	1124.562117	15.712282
24.254203	1123.877596	15.717299
24.631801	1121.138992	15.722317
24.189755	1128.712877	15.727335
24.490997	1134.248367	15.732352
24.400164	1133.590304	15.737370
24.354772	1127.304474	15.742387
24.277343	1125.265186	15.747405
24.459624	1161.469385	15.752423
24.583251	1142.981610	15.757440
24.836117	1152.968188	15.762458
24.605881	1159.334906	15.767475
24.860325	1146.936453	15.772493
24.520954	1158.549592	15.777511
24.608837	1148.518912	15.782528
24.599563	1152.256859	15.787546
24.576825	1151.086338	15.792563
24.802991	1141.400080	15.797581
24.788832	1155.761543	15.802599
24.802637	1150.731945	15.807616
24.852170	1148.388731	15.812634
24.634080	1155.675066	15.817651
24.855737	1155.435115	15.822669
24.552507	1154.377971	15.827687
24.906904	1152.532961	15.832704
24.528596	1143.092894	15.837722
24.559629	1156.169139	15.842739
24.847544	1159.731132	15.847757
25.173002	1174.099360	15.852775
24.953771	1187.940697	15.857792
25.264143	1176.502323	15.862810
25.014482	1174.710928	15.867827
24.990952	1175.980043	15.872845
25.305262	1180.169085	15.877863
25.290714	1166.035991	15.882880
25.431036	1166.080190	15.887898
25.326206	1179.742645	15.892915
25.358069	1165.731672	15.897933
25.219083	1163.307537	15.902951
25.880725	1157.845064	15.907968
25.493044	1150.268442	15.912986
25.289507	1150.669484	15.918003
25.251405	1146.039351	15.923021
25.621514	1147.814850	15.928039
25.409058	1153.661212	15.933056
25.145907	1154.705930	15.938074
25.348098	1157.501847	15.943091
25.665079	1171.732542	15.948109
25.645967	1166.300986	15.953127
25.623534	1167.939168	15.958144
25.573419	1168.319327	15.963162
25.612883	1175.003566	15.968179
25.696959	1166.819676	15.973197
26.047677	1169.131562	15.978215
25.457494	1158.456011	15.983232
25.348317	1152.820813	15.988250
25.484927	1171.400194	15.993267
25.779328	1159.427831	15.998285
25.696797	1175.923943	16.003303
25.885322	1159.048117	16.008320
25.918388	1168.059254	16.013338
25.732468	1167.198331	16.018355
26.095451	1161.858392	16.023373
25.633374	1169.104064	16.028391
25.586159	1171.162708	16.033408
25.896709	1168.131635	16.038426
25.536981	1165.328663	16.043443
26.027565	1165.674600	16.048461
26.161177	1161.831781	16.053479
26.024403	1175.281481	16.058496
26.345230	1165.798135	16.063514
25.797800	1165.978495	16.068531
26.052213	1168.387523	16.073549
26.196139	1187.079387	16.078567
26.334069	1182.506873	16.083584
26.499175	1179.779462	16.088602
26.101583	1174.713326	16.093619
26.217387	1182.345001	16.098637
26.519431	1181.369753	16.103655
26.351356	1171.953537	16.108672
25.954900	1167.821372	16.113690
26.295807	1192.961445	16.118707
26.079549	1193.803151	16.123725
26.023451	1194.184248	16.128743
26.188876	1193.807935	16.133760
26.478033	1197.240349	16.138778
26.457104	1189.461076	16.143795
26.618897	1191.007278	16.148813
26.725840	1186.234485	16.153831
26.523092	1193.600485	16.158848
26.522605	1189.377872	16.163866
26.560864	1184.798883	16.168883
26.347779	1183.140616	16.173901
26.703667	1190.927188	16.178919
26.783417	1195.026749	16.183936
26.820763	1192.486616	16.188954
26.581226	1191.170175	16.193971
26.857994	1181.990379	16.198989
26.666122	1186.407059	16.204007
26.647087	1187.230487	16.209024
26.439059	1189.134443	16.214042
26.227790	1206.064177	16.219059
26.458092	1215.887063	16.224077
26.827523	1220.304171	16.229095
26.872362	1213.461357	16.234112
26.988382	1214.891652	16.239130
27.024960	1212.178062	16.244147
26.934100	1212.640348	16.249165
27.145107	1209.773193	16.254183
27.255043	1215.894122	16.259200
27.194329	1215.250272	16.264218
27.241835	1212.475008	16.269235
27.391914	1204.760456	16.274253
27.473796	1200.111510	16.279271
27.178060	1215.041019	16.284288
27.260268	1219.140200	16.289306
27.415520	1214.113670	16.294323
27.485353	1209.845318	16.299341
27.522179	1206.636213	16.304359
27.455200	1215.315899	16.309376
27.557715	1207.861271	16.314394
27.180891	1210.400767	16.319411
27.150657	1208.622326	16.324429
27.510585	1207.477056	16.329447
27.484010	1205.218345	16.334464
27.545832	1205.221193	16.339482
27.387399	1201.944848	16.344499
27.688141	1203.791183	16.349517
27.362628	1213.959937	16.354535
27.551162	1209.887590	16.359552
27.709885	1201.338526	16.364570
27.759567	1209.381373	16.369587
27.997065	1201.182895	16.374605
27.771443	1203.443071	16.379623
27.803802	1196.346590	16.384640
27.814214	1200.027813	16.389658
27.812259	1201.306172	16.394675
28.060567	1193.494181	16.399693
27.771002	1194.584066	16.404711
27.677451	1202.138095	16.409728
27.772168	1195.748235	16.414746
27.700745	1195.582605	16.419763
27.755738	1191.509094	16.424781
27.802410	1212.624178	16.429799
27.711753	1228.490430	16.434816
28.302080	1217.816080	16.439834
28.038946	1223.092874	16.444851
27.914371	1221.329214	16.449869
28.100292	1221.202161	16.454887
27.782152	1217.477450	16.459904
28.138255	1211.163399	16.464922
27.851440	1209.103257	16.469939
28.055514	1214.764454	16.474957
28.019552	1215.041407	16.479975
27.698550	1226.869470	16.484992
28.116985	1231.998451	16.490010
28.154850	1245.941567	16.495027
28.305986	1237.182228	16.500045
28.321547	1237.829819	16.505063
28.335745	1243.766936	16.510080
28.679296	1239.269492	16.515098
28.821764	1244.855140	16.520115
28.926704	1239.817550	16.525133
29.054539	1230.654753	16.530151
28.763236	1236.497716	16.535168
28.895477	1209.976726	16.540186
28.868010	1217.621396	16.545203
28.301129	1207.544943	16.550221
28.741815	1205.995687	16.555239
28.671643	1205.249175	16.560256
28.592089	1208.739361	16.565274
28.565115	1221.808963	16.570291
28.677484	1232.253114	16.575309
28.422299	1225.047034	16.580327
28.324885	1227.719485	16.585344
28.814104	1223.117169	16.590362
28.481249	1235.360519	16.595379
28.740490	1240.940493	16.600397
28.861389	1226.846092	16.605415
28.930561	1236.934084	16.610432
29.109996	1235.466785	16.615450
29.141366	1237.399511	16.620467
29.003954	1233.958916	16.625485
29.162745	1241.514451	16.630503
29.365526	1243.780096	16.635520
29.111797	1236.226633	16.640538
28.894448	1234.969830	16.645555
29.167608	1245.193129	16.650573
29.265331	1252.452113	16.655591
29.243219	1257.934160	16.660608
29.405401	1258.921709	16.665626
29.641369	1254.213892	16.670643
29.552328	1263.001203	16.675661
29.923764	1246.967669	16.680679
29.214398	1246.434917	16.685696
29.265230	1248.333036	16.690714
29.445817	1258.236321	16.695731
29.606415	1261.322804	16.700749
29.701731	1256.731701	16.705767
29.787421	1267.757586	16.710784
29.583982	1252.142334	16.715802
29.591556	1246.753911	16.720819
29.507080	1251.968006	16.725837
29.475674	1253.175242	16.730855
29.738149	1255.494653	16.735872
29.910363	1259.923736	16.740890
29.896978	1264.403992	16.745907
29.986607	1256.228658	16.750925
29.643891	1253.574489	16.755943
29.886847	1250.702321	16.760960
29.664678	1259.513645	16.765978
29.608053	1263.722954	16.770995
29.426042	1256.104595	16.776013
29.675310	1252.148959	16.781031
29.968920	1259.077443	16.786048
29.476251	1251.848599	16.791066
29.620090	1265.592083	16.796083
29.773189	1279.618159	16.801101
30.340746	1270.055074	16.806119
30.299044	1277.323290	16.811136
30.389914	1281.623107	16.816154
30.373146	1271.930659	16.821171
30.414462	1278.545216	16.826189
30.389537	1283.671092	16.831207
30.537008	1279.466302	16.836224
30.454780	1280.823519	16.841242
30.606907	1277.779379	16.846259
30.149746	1260.641692	16.851277
30.385576	1261.339982	16.856295
30.339453	1278.947680	16.861312
30.579884	1274.504256	16.866330
30.861080	1270.366881	16.871347
30.356320	1268.299853	16.876365
30.297646	1258.872763	16.881383
30.481963	1278.625094	16.886400
30.472622	1270.531534	16.891418
30.535314	1271.787146	16.896435
30.259519	1278.874282	16.901453
30.450906	1280.213876	16.906471
30.704667	1275.392809	16.911488
30.764810	1271.703494	16.916506
30.570372	1275.902839	16.921523
30.642790	1272.236849	16.926541
30.608387	1267.044352	16.931559
30.309160	1276.552592	16.936576
30.421690	1290.736518	16.941594
30.604187	1289.770526	16.946611
30.381593	1295.154602	16.951629
30.684285	1292.042686	16.956647
31.014054	1302.083573	16.961664
31.033971	1306.839498	16.966682
31.194990	1308.660398	16.971699
31.300425	1316.524137	16.976717
31.675776	1303.778416	16.981735
31.127725	1297.691207	16.986752
31.147670	1293.629476	16.991770
31.115735	1288.843700	16.996787
30.787339	1298.356521	17.001805
31.596622	1300.426157	17.006823
31.541515	1320.402247	17.011840
31.213441	1307.047184	17.016858
31.261781	1309.015130	17.021875
31.337729	1317.091781	17.026893
31.722899	1305.862521	17.031911
31.641758	1324.703405	17.036928
31.566637	1312.485867	17.041946
31.773024	1309.467935	17.046963
31.644731	1310.860775	17.051981
31.880757	1310.959410	17.056999
32.010752	1319.488360	17.062016
31.901358	1301.671272	17.067034
31.837232	1294.173287	17.072051
31.659629	1293.547749	17.077069
31.597324	1287.535922	17.082087
31.455659	1290.672924	17.087104
31.891905	1315.324843	17.092122
31.779698	1307.622939	17.097139
32.003298	1316.118285	17.102157
32.138983	1313.695277	17.107175
31.744737	1316.231205	17.112192
31.952254	1306.894932	17.117210
31.868594	1308.549032	17.122227
31.773914	1312.161533	17.127245
31.978718	1303.122344	17.132263
32.180813	1305.482781	17.137280
31.689988	1314.213144	17.142298
32.139963	1304.356027	17.147315
32.080732	1300.956819	17.152333
32.149998	1296.117314	17.157351
32.276434	1311.122774	17.162368
32.047776	1328.418279	17.167386
32.310546	1329.942361	17.172403
32.318784	1337.543617	17.177421
32.565460	1334.077538	17.182439
32.792397	1331.201556	17.187456
32.600304	1325.579295	17.192474
32.650730	1322.093472	17.197491
32.253997	1322.764637	17.202509
32.836664	1322.524927	17.207527
32.860479	1326.750051	17.212544
32.517124	1308.909650	17.217562
32.447978	1308.674233	17.222579
32.328872	1322.673562	17.227597
32.546328	1329.143772	17.232615
32.643689	1328.797055	17.237632
32.920119	1333.986187	17.242650
32.888278	1328.796426	17.247667
32.909084	1330.064917	17.252685
32.854883	1332.418176	17.257703
33.069735	1335.335219	17.262720
32.765542	1331.904956	17.267738
33.017186	1320.213750	17.272755
32.771245	1325.920242	17.277773
32.691246	1323.884490	17.282791
32.945447	1317.548496	17.287808
32.736002	1320.775022	17.292826
32.996775	1322.662347	17.297843
32.930491	1321.189357	17.302861
33.054584	1325.499759	17.307879
33.517163	1346.638203	17.312896
33.324194	1359.004893	17.317914
33.461640	1354.344046	17.322931
33.240267	1351.083847	17.327949
33.562530	1353.068843	17.332967
33.890239	1352.496680	17.337984
33.452864	1344.915137	17.343002
33.346071	1323.177953	17.348019
33.222818	1323.891479	17.353037
33.379323	1339.229936	17.358055
33.495672	1341.935186	17.363072
33.578582	1352.756423	17.368090
33.473131	1349.487530	17.373107
33.354899	1357.465230	17.378125
33.432030	1349.717863	17.383143
33.618496	1350.007308	17.388160
33.897659	1345.459964	17.393178
33.970165	1340.335905	17.398195
33.846893	1344.290577	17.403213
33.894109	1350.219399	17.408231
33.897613	1343.783815	17.413248
33.711275	1348.016623	17.418266
33.810884	1336.551207	17.423283
33.671587	1345.848226	17.428301
34.021742	1344.401509	17.433319
34.059302	1350.196139	17.438336
33.918041	1369.403110	17.443354
34.231182	1366.557799	17.448371
34.068239	1377.417571	17.453389
34.171368	1377.931522	17.458407
34.512698	1374.905060	17.463424
34.026046	1366.302393	17.468442
34.131215	1366.793932	17.473459
34.122696	1372.867200	17.478477
34.133655	1372.676038	17.483495
34.146239	1376.072922	17.488512
33.962557	1369.865480	17.493530
34.366663	1372.270019	17.498547
34.354302	1372.565368	17.503565
34.504632	1370.556642	17.508583
34.285172	1375.006093	17.513600
34.312226	1391.128613	17.518618
34.335501	1388.956747	17.523635
34.761769	1398.534425	17.528653
34.562055	1395.971444	17.533671
34.765932	1398.192753	17.538688
34.607454	1396.491195	17.543706
35.205206	1386.181671	17.548723
34.805864	1382.655848	17.553741
35.003684	1401.266905	17.558759
35.136818	1378.949240	17.563776
35.193942	1388.139763	17.568794
35.308192	1378.590838	17.573811
35.255320	1386.829721	17.578829
35.137982	1374.855450	17.583847
35.271069	1366.307168	17.588864
34.739874	1370.931699	17.593882
35.239883	1380.466255	17.598899
35.344207	1391.410398	17.603917
35.349990	1391.743933	17.608935
35.636995	1377.285702	17.613952
34.893463	1370.468514	17.618970
35.263712	1374.352180	17.623987
35.113933	1371.061825	17.629005
35.117248	1376.117028	17.634023
35.499165	1380.809943	17.639040
35.340447	1390.911637	17.644058
34.973736	1383.663003	17.649075
35.068345	1387.539364	17.654093
35.150099	1373.965398	17.659111
35.349383	1386.870277	17.664128
35.412399	1396.242926	17.669146
35.430217	1402.419379	17.674163
35.374155	1408.919848	17.679181
35.355253	1410.970928	17.684199
35.794231	1413.297422	17.689216
35.354679	1413.694420	17.694234
36.085381	1402.022781	17.699251
35.846753	1403.991517	17.704269
35.742617	1403.433362	17.709287
36.260428	1403.225905	17.714304
35.679263	1403.509385	17.719322
35.783931	1403.723281	17.724339
36.260733	1411.812912	17.729357
36.097425	1412.504314	17.734375
36.137230	1409.323109	17.739392
36.096223	1423.319748	17.744410
36.436338	1432.560634	17.749427
36.649401	1411.928304	17.754445
36.195191	1413.217574	17.759463
36.281444	1410.303659	17.764480
35.865647	1414.682892	17.769498
36.344067	1425.950313	17.774515
36.632688	1434.545986	17.779533
36.552084	1426.880107	17.784551
36.928320	1430.974295	17.789568
36.302441	1409.996864	17.794586
36.596186	1415.823964	17.799603
36.819611	1421.690486	17.804621
36.483175	1434.657245	17.809639
36.976734	1433.169116	17.814656
36.698921	1428.462854	17.819674
36.827838	1418.854802	17.824691
37.184233	1400.667978	17.829709
36.451297	1403.414780	17.834727
36.774684	1399.744157	17.839744
36.946832	1421.625658	17.844762
36.953459	1423.903124	17.849779
36.950744	1426.488181	17.854797
36.959134	1428.658068	17.859815
37.005990	1418.425373	17.864832
36.939691	1434.073386	17.869850
36.779528	1425.694104	17.874867
36.846467	1423.587979	17.879885
36.838171	1419.385470	17.884903
36.789555	1422.318560	17.889920
36.651837	1429.519827	17.894938
37.211244	1426.254052	17.899955
37.648535	1439.014376	17.904973
36.962070	1433.220218	17.909991
37.264572	1434.996872	17.915008
37.408138	1449.510591	17.920026
37.415926	1455.022729	17.925043
37.409017	1453.174335	17.930061
37.165960	1450.536081	17.935079
37.290907	1452.716114	17.940096
37.710528	1451.028120	17.945114
37.736630	1452.175863	17.950131
37.594899	1450.736775	17.955149
37.605239	1452.212051	17.960167
37.672907	1453.135522	17.965184
37.483577	1451.804882	17.970202
37.203549	1456.229128	17.975219
37.505338	1451.097517	17.980237
37.491029	1471.528152	17.985255
37.877573	1469.327763	17.990272
37.809999	1483.038263	17.995290
38.035969	1479.973051	18.000307
38.229532	1477.402091	18.005325
37.886922	1474.719468	18.010343
38.155533	1465.218899	18.015360
38.102173	1483.834681	18.020378
38.204787	1469.569376	18.025395
38.218275	1469.876457	18.030413
38.179482	1474.316562	18.035431
38.275020	1458.177738	18.040448
37.809742	1473.474868	18.045466
38.215725	1472.142476	18.050483
38.370623	1482.157212	18.055501
38.563042	1498.970322	18.060519
38.534459	1493.461252	18.065536
38.465136	1507.676998	18.070554
38.496748	1494.599971	18.075571
38.598220	1490.525421	18.080589
38.646024	1499.553352	18.085607
38.966138	1494.103262	18.090624
38.760624	1492.872990	18.095642
38.693695	1494.609696	18.100659
39.162200	1491.317125	18.105677
39.255614	1493.315901	18.110695
39.115576	1488.913100	18.115712
38.643702	1487.910762	18.120730
38.736813	1491.156189	18.125747
39.007887	1487.844056	18.130765
38.229874	1487.994269	18.135783
39.030442	1487.685703	18.140800
39.100442	1489.501945	18.145818
38.909401	1489.667495	18.150835
39.170195	1484.479179	18.155853
39.071350	1494.489494	18.160871
38.849837	1486.580566	18.165888
38.925056	1502.746135	18.170906
39.091918	1516.186389	18.175923
39.231195	1512.358388	18.180941
39.220337	1520.117356	18.185959
39.449409	1511.920058	18.190976
39.598758	1511.025523	18.195994
39.409035	1508.341033	18.201011
39.741226	1500.323253	18.206029
39.471265	1505.544392	18.211047
39.256124	1509.892209	18.216064
39.259851	1510.276564	18.221082
39.445757	1510.629218	18.226099
39.759959	1518.289916	18.231117
39.535689	1532.987574	18.236135
40.112095	1526.298053	18.241152
40.102585	1523.241325	18.246170
40.026273	1533.699435	18.251187
40.111854	1521.235658	18.256205
39.822142	1518.948703	18.261223
40.123658	1528.047356	18.266240
40.162993	1532.860262	18.271258
40.295165	1529.995940	18.276275
40.226928	1502.079432	18.281293
39.801662	1511.490772	18.286311
40.219424	1506.482994	18.291328
40.196490	1527.710347	18.296346
40.456963	1532.141449	18.301363
40.290548	1519.164862	18.306381
39.973108	1518.485481	18.311399
40.226912	1519.588085	18.316416
40.302246	1519.711900	18.321434
39.948730	1529.004705	18.326451
40.622560	1520.425278	18.331469
40.271554	1526.618534	18.336487
40.385118	1525.284615	18.341504
40.589906	1545.570547	18.346522
40.525092	1554.827601	18.351539
40.974956	1551.219187	18.356557
40.596481	1554.440677	18.361575
40.799053	1550.953064	18.366592
40.642625	1562.234827	18.371610
40.831116	1563.189868	18.376627
41.024295	1552.419747	18.381645
40.972629	1554.826290	18.386663
40.941928	1546.713860	18.391680
40.966077	1549.203202	18.396698
40.636863	1546.641552	18.401715
41.119013	1540.216115	18.406733
40.991164	1552.247670	18.411751
41.055996	1568.888322	18.416768
41.320220	1570.948712	18.421786
41.622155	1577.292161	18.426803
41.772859	1558.948045	18.431821
41.212074	1557.543045	18.436839
41.176249	1559.249637	18.441856
41.807136	1570.537445	18.446874
41.569609	1562.810882	18.451891
41.606716	1557.976344	18.456909
41.566572	1570.672704	18.461927
41.474435	1567.051372	18.466944
41.583155	1568.997263	18.471962
41.912701	1573.540636	18.476979
41.928440	1569.346950	18.481997
41.454931	1571.813277	18.487015
41.583069	1562.274702	18.492032
41.601392	1562.527376	18.497050
41.298358	1565.298368	18.502067
41.918119	1561.016359	18.507085
41.707912	1568.951756	18.512103
41.835306	1573.722473	18.517120
42.168869	1582.841380	18.522138
42.285083	1590.312211	18.527155
42.520724	1580.308635	18.532173
42.471612	1586.580849	18.537191
42.323616	1582.277107	18.542208
42.398472	1588.914928	18.547226
41.967382	1585.605489	18.552243
42.363681	1584.855306	18.557261
42.592937	1583.774670	18.562279
42.465332	1583.564188	18.567296
42.816364	1579.968097	18.572314
42.379940	1585.186936	18.577331
42.907400	1581.957699	18.582349
42.562028	1589.481914	18.587367
42.575542	1581.192119	18.592384
42.637432	1577.862249	18.597402
42.871171	1582.988711	18.602419
42.770054	1578.093770	18.607437
42.796034	1581.624300	18.612455
42.574402	1582.277507	18.617472
42.758081	1577.476808	18.622490
42.538604	1577.239692	18.627507
42.850286	1575.846325	18.632525
42.772786	1578.421029	18.637543
42.607673	1584.632518	18.642560
43.019022	1592.035017	18.647578
42.614800	1604.005761	18.652595
43.177789	1592.969380	18.657613
43.105283	1606.712308	18.662631
42.943144	1593.084865	18.667648
42.728453	1596.523712	18.672666
43.132559	1608.156361	18.677683
43.558015	1617.049438	18.682701
43.179206	1619.860715	18.687719
42.962690	1628.018046	18.692736
43.386141	1620.405659	18.697754
43.244546	1620.822253	18.702771
43.245616	1624.811156	18.707789
43.119830	1627.156734	18.712807
43.265312	1638.277627	18.717824
43.912270	1646.283898	18.722842
43.824716	1654.648265	18.727859
44.274503	1645.441125	18.732877
44.508341	1646.739381	18.737895
44.086247	1649.147166	18.742912
44.541810	1620.267885	18.747930
44.052603	1618.431920	18.752947
43.939091	1611.613763	18.757965
43.942243	1615.712798	18.762983
44.141383	1628.712554	18.768000
44.329328	1637.604982	18.773018
44.395540	1640.163490	18.778035
44.444476	1638.811285	18.783053
44.144213	1639.236958	18.788071
44.367099	1642.780834	18.793088
44.636013	1629.701244	18.798106
44.607699	1637.112684	18.803123
44.656010	1637.010346	18.808141
44.792600	1638.563692	18.813159
44.365553	1642.329326	18.818176
44.820121	1637.022238	18.823194
44.670941	1644.272727	18.828211
44.379980	1635.923307	18.833229
44.374613	1632.698644	18.838247
44.227453	1636.123761	18.843264
44.662751	1634.739426	18.848282
44.495693	1643.128869	18.853299
44.653665	1646.152711	18.858317
45.345995	1653.173521	18.863335
44.817398	1657.245419	18.868352
44.882799	1670.187259	18.873370
45.048958	1668.378003	18.878387
44.752367	1659.319356	18.883405
45.300141	1659.709997	18.888423
44.739835	1663.521762	18.893440
44.959495	1660.697364	18.898458
45.141979	1663.417549	18.903475
44.996132	1680.668859	18.908493
45.284864	1685.010361	18.913511
45.475554	1689.483996	18.918528
45.567505	1685.013239	18.923546
45.578099	1682.347833	18.928563
45.739159	1686.463171	18.933581
45.803473	1678.073848	18.938599
45.877772	1690.957501	18.943616
45.843173	1680.810006	18.948634
45.302204	1678.423534	18.953651
45.893359	1685.649568	18.958669
46.076349	1680.949941	18.963687
46.054708	1685.914462	18.968704
46.005331	1674.125014	18.973722
46.032440	1682.234730	18.978739
45.838118	1689.590145	18.983757
45.868042	1677.542103	18.988775
45.982628	1688.061917	18.993792
46.065793	1687.913090	18.998810
45.993393	1687.977997	19.003827
46.280622	1688.276909	19.008845
46.545219	1699.435985	19.013863
46.108502	1701.590432	19.018880
46.480091	1697.069547	19.023898
46.625045	1707.114371	19.028915
46.315455	1702.252059	19.033933
46.575406	1708.813585	19.038951
46.431409	1709.113784	19.043968
46.729183	1711.187870	19.048986
46.717368	1710.176558	19.054003
46.627506	1703.067465	19.059021
46.873437	1691.727229	19.064039
46.964293	1701.414431	19.069056
46.906299	1699.163736	19.074074
46.807198	1704.121462	19.079091
46.270647	1691.613021	19.084109
46.599668	1696.582568	19.089127
46.986755	1723.464573	19.094144
47.252705	1724.653655	19.099162
47.497469	1720.562915	19.104179
47.396718	1725.615585	19.109197
47.693452	1723.148354	19.114215
47.168283	1717.786450	19.119232
47.239670	1720.041182	19.124250
47.408129	1731.799201	19.129267
47.133319	1727.464797	19.134285
47.655978	1726.385523	19.139303
47.296747	1727.634685	19.144320
47.565693	1724.755215	19.149338
47.493128	1725.577587	19.154355
47.168856	1719.947507	19.159373
47.612133	1720.354522	19.164391
47.379880	1725.572972	19.169408
47.388689	1723.699995	19.174426
47.382657	1741.892038	19.179443
47.623118	1753.673506	19.184461
47.837953	1748.113595	19.189479
47.741499	1745.427079	19.194496
48.243007	1743.486374	19.199514
48.212929	1738.826426	19.204531
48.042846	1741.718635	19.209549
48.056058	1749.846339	19.214567
48.131228	1756.073893	19.219584
48.395039	1764.108688	19.224602
48.424341	1766.553069	19.229619
48.199953	1774.844252	19.234637
48.653735	1761.726133	19.239655
48.981106	1764.660334	19.244672
48.662216	1749.116388	19.249690
48.569134	1745.668748	19.254707
48.016412	1746.045610	19.259725
48.327993	1740.596783	19.264743
48.484819	1765.365691	19.269760
48.782079	1758.644076	19.274778
48.662993	1768.739773	19.279795
48.763676	1760.698185	19.284813
48.769862	1761.934281	19.289831
48.665255	1771.491189	19.294848
48.924321	1769.358078	19.299866
49.183415	1765.675363	19.304883
49.070285	1766.422036	19.309901
49.188222	1757.421477	19.314919
49.050610	1757.982626	19.319936
49.326424	1770.222498	19.324954
49.371331	1786.973779	19.329971
49.322026	1786.148229	19.334989
49.680698	1788.881857	19.340007
49.377207	1789.977113	19.345024
49.352354	1788.115716	19.350042
49.325441	1783.748770	19.355059
49.430405	1792.789985	19.360077
49.762780	1789.992091	19.365095
49.631111	1790.419757	19.370112
49.684935	1779.081160	19.375130
49.664687	1781.258734	19.380147
49.804686	1793.096996	19.385165
49.808113	1789.167137	19.390183
49.817168	1790.222893	19.395200
49.960882	1789.717417	19.400218
49.952250	1789.605064	19.405235
49.981230	1790.556706	19.410253
50.178734	1797.011276	19.415271
50.298834	1811.465846	19.420288
50.100499	1810.811976	19.425306
49.963265	1813.822135	19.430323
50.037732	1816.969549	19.435341
50.375236	1813.107271	19.440359
50.626163	1819.777556	19.445376
50.419158	1818.083559	19.450394
50.244417	1812.338497	19.455411
50.261198	1815.251936	19.460429
50.549817	1806.158334	19.465447
50.396015	1818.156262	19.470464
50.530695	1835.505789	19.475482
50.891751	1829.629434	19.480499
50.663354	1841.443391	19.485517
51.139604	1831.269424	19.490535
51.051135	1825.431940	19.495552
51.104799	1833.644869	19.500570
51.418028	1831.964043	19.505587
50.939359	1836.154398	19.510605
51.262280	1830.687988	19.515623
51.007962	1837.715169	19.520640
50.969043	1830.433931	19.525658
51.606218	1825.151831	19.530675
51.256049	1831.127294	19.535693
51.825404	1826.430215	19.540711
51.093925	1821.447765	19.545728
51.362553	1822.207216	19.550746
51.553600	1826.835475	19.555763
50.963765	1826.627979	19.560781
51.155541	1825.947703	19.565799
51.518414	1841.443618	19.570816
51.564883	1850.156333	19.575834
51.936636	1850.457785	19.580851
51.681837	1854.171227	19.585869
51.976733	1850.050510	19.590887
51.908682	1859.791099	19.595904
51.919166	1860.123906	19.600922
51.695472	1849.494666	19.605939
51.608754	1848.914832	19.610957
52.039860	1852.744885	19.615975
52.147350	1851.392958	19.620992
52.015107	1858.735559	19.626010
52.083552	1867.946647	19.631027
52.515536	1876.646314	19.636045
52.641103	1869.484466	19.641063
52.564868	1875.720003	19.646080
52.416678	1864.308855	19.651098
52.634310	1864.918497	19.656115
52.244907	1874.564265	19.661133
52.498477	1871.466259	19.666151
52.779631	1865.555070	19.671168
52.582789	1855.713782	19.676186
52.872849	1862.336923	19.681203
52.633294	1871.460561	19.686221
52.477936	1866.050138	19.691239
53.063791	1881.785727	19.696256
52.950820	1877.937205	19.701274
53.137445	1888.846666	19.706291
52.880700	1892.601449	19.711309
52.920091	1891.963982	19.716327
53.372138	1901.998674	19.721344
53.459010	1896.581851	19.726362
53.298727	1889.909782	19.731379
53.294115	1894.578182	19.736397
53.508964	1889.002445	19.741415
53.391010	1887.638496	19.746432
53.340224	1895.116683	19.751450
53.503110	1886.402528	19.756467
53.088201	1890.854324	19.761485
53.376105	1903.288068	19.766503
54.014375	1921.047962	19.771520
53.796259	1925.115459	19.776538
53.779493	1911.992054	19.781555
53.668745	1925.921112	19.786573
53.974479	1915.303565	19.791591
53.864343	1914.758958	19.796608
53.759164	1912.847012	19.801626
53.902325	1919.010317	19.806643
53.712085	1926.090614	19.811661
53.976419	1930.959901	19.816679
54.308443	1932.088148	19.821696
54.187079	1931.557924	19.826714
54.488542	1927.562403	19.831731
54.227185	1935.622749	19.836749
54.276451	1937.246612	19.841767
54.413903	1932.604550	19.846784
54.684851	1925.101143	19.851802
54.550150	1930.089757	19.856819
54.460659	1943.816668	19.861837
54.804555	1947.272213	19.866855
54.995295	1953.589033	19.871872
54.951445	1952.109320	19.876890
55.145832	1945.788790	19.881907
54.756985	1953.029612	19.886925
54.835261	1950.700727	19.891943
54.989358	1954.227038	19.896960
54.963546	1956.632740	19.901978
55.247655	1954.009653	19.906995
55.287250	1967.710045	19.912013
55.616089	1952.774547	19.917031
55.392714	1954.747264	19.922048
54.995970	1958.120022	19.927066
55.258466	1948.503382	19.932083
55.045156	1958.983204	19.937101
55.400416	1976.897957	19.942119
55.629415	1975.081981	19.947136
55.541479	1975.225067	19.952154
55.517589	1969.083906	19.957171
55.805539	1976.303912	19.962189
56.011513	1970.533866	19.967207
55.629233	1981.305282	19.972224
55.758952	1978.453898	19.977242
56.244964	1967.372541	19.982259
55.925489	1971.992456	19.987277
56.295240	1968.405980	19.992295
56.056281	1975.260382	19.997312
56.110342	1989.094234	20.002330
56.547787	1985.822221	20.007347
56.417625	1986.432706	20.012365
56.659525	1995.787110	20.017383
56.788136	2005.623207	20.022400
56.538377	1993.258983	20.027418
56.604951	1992.112287	20.032435
56.521762	1998.146969	20.037453
56.319361	1998.131251	20.042471
56.522204	1992.424809	20.047488
56.125916	2005.994692	20.052506
56.531635	1990.097148	20.057523
56.615169	1998.409621	20.062541
56.562832	2007.920593	20.067559
56.984107	2013.696348	20.072576
56.896783	2022.016666	20.077594
57.080904	2019.563882	20.082611
57.092894	2025.220715	20.087629
57.167318	2024.401016	20.092647
56.935968	2025.437643	20.097664
57.182444	2027.137921	20.102682
57.361008	2034.091045	20.107699
57.576340	2047.858645	20.112717
57.340324	2044.764728	20.117735
57.493316	2038.109797	20.122752
57.291341	2042.581922	20.127770
57.675984	2035.076436	20.132787
57.311981	2033.864644	20.137805
57.230951	2048.616026	20.142823
57.739822	2056.148618	20.147840
57.892197	2056.071002	20.152858
58.065044	2061.850979	20.157875
57.737637	2062.025273	20.162893
58.493265	2055.812447	20.167911
58.601004	2057.389287	20.172928
58.188992	2061.793331	20.177946
58.535218	2042.865777	20.182963
58.450896	2060.994664	20.187981
58.528960	2048.408613	20.192999
58.631822	2045.422559	20.198016
58.349444	2050.847788	20.203034
58.924604	2056.170223	20.208051
58.908826	2046.840146	20.213069
58.836553	2050.487157	20.218087
59.071033	2051.608603	20.223104
58.798699	2052.547503	20.228122
58.817391	2051.424085	20.233139
58.747521	2042.146671	20.238157
58.936976	2047.835671	20.243175
59.115677	2048.318865	20.248192
59.148689	2049.759078	20.253210
58.979689	2047.260622	20.258227
59.227184	2049.064893	20.263245
59.190675	2053.201802	20.268263
59.283168	2051.078976	20.273280
59.160023	2069.920912	20.278298
59.257906	2070.694502	20.283315
59.608227	2074.783433	20.288333
59.644583	2075.090098	20.293351
59.929226	2065.002830	20.298368
59.624175	2070.892401	20.303386
59.824974	2070.138114	20.308403
59.774546	2067.065612	20.313421
59.598745	2060.645239	20.318439
59.887854	2061.925397	20.323456
59.736697	2064.344440	20.328474
59.977449	2064.249822	20.333491
59.504527	2068.016417	20.338509
59.683976	2078.759847	20.343527
60.280927	2088.803502	20.348544
59.702920	2092.454013	20.353562
59.619265	2093.432786	20.358579
59.906419	2091.358358	20.363597
60.083991	2110.986423	20.368615
60.299664	2112.325432	20.373632
60.521037	2123.422112	20.378650
60.259607	2112.378871	20.383667
60.445413	2120.880522	20.388685
60.466334	2123.635560	20.393703
60.716568	2134.926558	20.398720
60.615303	2148.257804	20.403738
60.612933	2152.717619	20.408755
60.883058	2148.802705	20.413773
60.978847	2145.644159	20.418791
61.320015	2140.048553	20.423808
61.012208	2136.489300	20.428826
61.112308	2142.233359	20.433843
61.338696	2135.396466	20.438861
61.374912	2138.335317	20.443879
61.447694	2152.983785	20.448896
61.550095	2163.316423	20.453914
61.930886	2174.003116	20.458931
61.987074	2164.352408	20.463949
62.021667	2151.091383	20.468967
61.837686	2129.611487	20.473984
61.864296	2133.596502	20.479002
61.604460	2134.962673	20.484019
61.693767	2154.172232	20.489037
61.657494	2165.104160	20.494055
61.935494	2154.844298	20.499072
62.159301	2164.709753	20.504090
61.735108	2161.405436	20.509107
61.903228	2155.489770	20.514125
61.609524	2171.590657	20.519143
62.460974	2175.717872	20.524160
62.147617	2185.389764	20.529178
62.155465	2188.219449	20.534195
62.422479	2186.896157	20.539213
62.301477	2192.472884	20.544231
62.598017	2182.961249	20.549248
62.561242	2186.347084	20.554266
62.647688	2196.322448	20.559283
62.655957	2205.574698	20.564301
62.471764	2218.070002	20.569319
63.130674	2200.169519	20.574336
63.244401	2218.838787	20.579354
63.286843	2209.114462	20.584371
63.572595	2202.375549	20.589389
63.208786	2214.214122	20.594407
63.324767	2206.365616	20.599424
63.386801	2201.265045	20.604442
63.076566	2198.921252	20.609459
63.263756	2195.685256	20.614477
63.341998	2203.903971	20.619495
63.757354	2198.041082	20.624512
63.396749	2197.914438	20.629530
63.511973	2210.173461	20.634547
63.880627	2210.093520	20.639565
63.789329	2217.167898	20.644583
64.150851	2225.370645	20.649600
63.778973	2233.255918	20.654618
64.043185	2227.284144	20.659635
64.373469	2230.858653	20.664653
64.130193	2226.023680	20.669671
64.181306	2219.687629	20.674688
64.166947	2223.761141	20.679706
63.873474	2224.861165	20.684723
64.088547	2222.280417	20.689741
64.088009	2231.837045	20.694759
64.347386	2234.680983	20.699776
64.601071	2239.293223	20.704794
64.455822	2248.695792	20.709811
64.478244	2250.585845	20.714829
64.454427	2254.127466	20.719847
64.762968	2249.045070	20.724864
64.556805	2254.613067	20.729882
64.737909	2254.789749	20.734899
64.831621	2265.193241	20.739917
65.006399	2272.039743	20.744935
65.427569	2273.791578	20.749952
65.279877	2273.331746	20.754970
65.227108	2273.655535	20.759987
65.421805	2271.652382	20.765005
65.357202	2275.557036	20.770023
65.655263	2267.500079	20.775040
65.698859	2264.870445	20.780058
65.170382	2264.101010	20.785075
65.939388	2264.100368	20.790093
65.592548	2266.783647	20.795111
65.387620	2261.759603	20.800128
66.089859	2276.899740	20.805146
65.979835	2287.442473	20.810163
66.135427	2289.706178	20.815181
66.194039	2291.025624	20.820199
66.336566	2286.934993	20.825216
66.386387	2298.355333	20.830234
66.137545	2296.099747	20.835251
66.374069	2284.602806	20.840269
66.098634	2288.300633	20.845287
65.807163	2291.376065	20.850304
66.182832	2289.458175	20.855322
66.260228	2305.781933	20.860339
66.795835	2311.823921	20.865357
66.584749	2313.128813	20.870375
66.468924	2305.995144	20.875392
66.805476	2305.803457	20.880410
66.439476	2312.396999	20.885427
67.176777	2315.336500	20.890445
66.963459	2330.935739	20.895463
67.329920	2332.263765	20.900480
67.574119	2334.485188	20.905498
67.534022	2331.903374	20.910515
67.596779	2327.285539	20.915533
67.541057	2336.932927	20.920551
67.649831	2329.612567	20.925568
67.664615	2322.202784	20.930586
67.324972	2326.728108	20.935603
67.629798	2313.910665	20.940621
67.592574	2327.809577	20.945639
67.459943	2325.434785	20.950656
67.544422	2334.432141	20.955674
67.473925	2333.666695	20.960691
67.893906	2335.456596	20.965709
67.703916	2348.208543	20.970727
67.683497	2343.243939	20.975744
68.301920	2348.651211	20.980762
68.116777	2357.264747	20.985779
68.211736	2351.073274	20.990797
68.358697	2351.795002	20.995815
68.392010	2344.729478	21.000832
68.355792	2343.365313	21.005850
68.048242	2351.448862	21.010867
68.112150	2365.044752	21.015885
68.547016	2377.673572	21.020903
68.432146	2377.173877	21.025920
68.918217	2367.537767	21.030938
68.593577	2366.629083	21.035955
69.164830	2383.459417	21.040973
68.903822	2391.636687	21.045991
68.948482	2392.437567	21.051008
69.205350	2391.762854	21.056026
69.222541	2400.698195	21.061043
69.163951	2396.421278	21.066061
69.426457	2397.080719	21.071079
69.570584	2404.755820	21.076096
69.856423	2396.580788	21.081114
69.430424	2398.989281	21.086131
69.961008	2396.930334	21.091149
69.841011	2403.693669	21.096167
69.663186	2405.362622	21.101184
69.560230	2413.092220	21.106202
69.600518	2429.475558	21.111219
70.280229	2418.107932	21.116237
70.129853	2425.788154	21.121255
70.196062	2414.052701	21.126272
70.804978	2422.033724	21.131290
70.169766	2427.612185	21.136307
70.399558	2411.208448	21.141325
70.547339	2417.989801	21.146343
70.174730	2413.635834	21.151360
70.702134	2417.940122	21.156378
70.137009	2435.298876	21.161395
70.417729	2436.722403	21.166413
70.732557	2439.172639	21.171431
70.789010	2447.164483	21.176448
70.827575	2438.996611	21.181466
70.615460	2434.869984	21.186483
70.971577	2448.994570	21.191501
71.048861	2461.698410	21.196519
71.267042	2467.237862	21.201536
71.358638	2463.502346	21.206554
71.614755	2468.183699	21.211571
71.991877	2462.528708	21.216589
71.457141	2457.142828	21.221607
71.481738	2457.037889	21.226624
71.860670	2463.789356	21.231642
71.433901	2469.653941	21.236659
71.965471	2455.588918	21.241677
71.844294	2451.031430	21.246695
71.766996	2466.214959	21.251712
72.036130	2459.825728	21.256730
71.908390	2482.071122	21.261747
72.057483	2480.245523	21.266765
72.675655	2490.030433	21.271783
71.949462	2487.777020	21.276800
72.149356	2482.231849	21.281818
72.286324	2489.055953	21.286835
72.372860	2486.463745	21.291853
72.539184	2488.432273	21.296871
72.213229	2485.866819	21.301888
72.512773	2495.597501	21.306906
72.661633	2507.062423	21.311923
72.713444	2506.385116	21.316941
72.919941	2512.854316	21.321959
72.961400	2508.091433	21.326976
73.139170	2511.961321	21.331994
72.770188	2509.958084	21.337011
73.141254	2511.291715	21.342029
73.056383	2509.562736	21.347047
73.157758	2523.670482	21.352064
73.011932	2527.587917	21.357082
73.096705	2532.583341	21.362099
73.644998	2531.673596	21.367117
73.277092	2533.075665	21.372135
73.570633	2542.633725	21.377152
73.712324	2553.689501	21.382170
73.647234	2563.477349	21.387187
73.759873	2568.310610	21.392205
74.070332	2563.909554	21.397223
73.740757	2563.449805	21.402240
73.992689	2561.548118	21.407258
73.821101	2569.755645	21.412275
74.401074	2583.498089	21.417293
74.350375	2585.661594	21.422311
74.363157	2588.455852	21.427328
74.747582	2579.318446	21.432346
74.785957	2586.281123	21.437363
75.050857	2577.680053	21.442381
74.882325	2581.058199	21.447399
74.533139	2592.033099	21.452416
74.996289	2585.095818	21.457434
74.852389	2583.663290	21.462451
74.935643	2576.523572	21.467469
74.909190	2593.457217	21.472487
74.899823	2593.957268	21.477504
75.307937	2596.004703	21.482522
75.471055	2599.046838	21.487539
75.539168	2599.108669	21.492557
75.767282	2595.692601	21.497575
75.876033	2603.174492	21.502592
75.938544	2594.990174	21.507610
75.994759	2606.024657	21.512627
75.624794	2604.696980	21.517645
75.767294	2597.254449	21.522663
75.707707	2602.660718	21.527680
75.767483	2618.542502	21.532698
75.713373	2621.328308	21.537715
75.983183	2619.581622	21.542733
75.964646	2613.417310	21.547751
75.775023	2622.426193	21.552768
76.394837	2629.379851	21.557786
76.381435	2639.017614	21.562803
76.108205	2637.636906	21.567821
76.722822	2638.316937	21.572839
76.526146	2646.683082	21.577856
76.922576	2636.413860	21.582874
76.528810	2645.281151	21.587891
76.880740	2651.986421	21.592909
76.961701	2653.068836	21.597927
76.904918	2662.483009	21.602944
77.219789	2647.987832	21.607962
77.221105	2650.417781	21.612979
77.136470	2651.204212	21.617997
77.524504	2647.898794	21.623015
77.396122	2659.451436	21.628032
77.596299	2646.299818	21.633050
77.570674	2656.233029	21.638067
77.556168	2674.919706	21.643085
77.967783	2675.319084	21.648103
77.693925	2676.472872	21.653120
78.532818	2682.991393	21.658138
78.025650	2690.396230	21.663155
77.819860	2683.008232	21.668173
78.572946	2670.925128	21.673191
78.326576	2686.346795	21.678208
78.199737	2676.860203	21.683226
78.443289	2687.029000	21.688243
78.257205	2677.415975	21.693261
78.609894	2678.121265	21.698279
78.441316	2682.010736	21.703296
78.728955	2689.496198	21.708314
78.474338	2700.254352	21.713331
78.626367	2698.977444	21.718349
78.669706	2707.555350	21.723367
78.899274	2710.000045	21.728384
78.776711	2699.442829	21.733402
79.081298	2711.290629	21.738419
78.979212	2730.306701	21.743437
79.160825	2730.562214	21.748455
79.127889	2727.761445	21.753472
79.557256	2729.852910	21.758490
79.195898	2732.667934	21.763507
79.516158	2731.765501	21.768525
79.760852	2748.416940	21.773543
79.404089	2752.086572	21.778560
79.903715	2742.539669	21.783578
79.683756	2751.300875	21.788595
80.028415	2756.530232	21.793613
80.103443	2751.743088	21.798631
80.217250	2754.032336	21.803648
80.518312	2761.607254	21.808666
80.391408	2773.620540	21.813683
80.492894	2773.838109	21.818701
81.040335	2775.958422	21.823719
80.529242	2788.634741	21.828736
80.732957	2772.474633	21.833754
81.004316	2765.721985	21.838771
80.677070	2769.128189	21.843789
80.778493	2764.554683	21.848807
80.675149	2774.118237	21.853824
80.827821	2780.750620	21.858842
81.347729	2789.421177	21.863859
81.045264	2802.039569	21.868877
81.415453	2795.113617	21.873895
81.445729	2805.451613	21.878912
81.273490	2800.201362	21.883930
81.448845	2800.580948	21.888947
81.320209	2804.088601	21.893965
81.771564	2815.433734	21.898983
82.039321	2820.375320	21.904000
81.829545	2819.666392	21.909018
82.042490	2814.756626	21.914035
81.973499	2816.739965	21.919053
82.233571	2814.609731	21.924071
82.228970	2815.623500	21.929088
81.907291	2807.464560	21.934106
82.218439	2815.176793	21.939123
82.300617	2837.553858	21.944141
82.782765	2845.450778	21.949159
82.737053	2844.690896	21.954176
82.797905	2838.119543	21.959194
82.803630	2835.151735	21.964211
82.785778	2841.507862	21.969229
82.815835	2833.476862	21.974247
82.969248	2835.210737	21.979264
82.612657	2838.523709	21.984282
82.855352	2839.517672	21.989299
82.839578	2857.961710	21.994317
83.003413	2861.934855	21.999335
83.150040	2869.761261	22.004352
83.391507	2867.441408	22.009370
83.813031	2862.154924	22.014387
83.978776	2889.240635	22.019405
83.942275	2881.384164	22.024423
83.845015	2892.240870	22.029440
83.760054	2896.666466	22.034458
83.867288	2889.024187	22.039475
83.592469	2886.097168	22.044493
83.987105	2892.909461	22.049511
84.134387	2893.871033	22.054528
84.244591	2900.806797	22.059546
84.681023	2911.447339	22.064563
84.656866	2911.817155	22.069581
84.763222	2906.359102	22.074599
84.733074	2914.222692	22.079616
84.809113	2910.836704	22.084634
84.663284	2902.558639	22.089651
84.626088	2914.046659	22.094669
84.833801	2905.501736	22.099687
84.785611	2938.763017	22.104704
84.740644	2943.349638	22.109722
85.371815	2931.067684	22.114739
85.214912	2940.021100	22.119757
85.304422	2934.912861	22.124775
85.300131	2945.565661	22.129792
85.340368	2959.067866	22.134810
85.486094	2956.942906	22.139827
85.494152	2952.087296	22.144845
85.924819	2958.234320	22.149863
85.698393	2965.169195	22.154880
85.608421	2977.905916	22.159898
85.974520	2972.123089	22.164915
86.212569	2974.724302	22.169933
86.420357	2981.206095	22.174951
86.281700	2981.881067	22.179968
86.285738	2987.201732	22.184986
86.598386	2996.419326	22.190003
86.777484	3008.558418	22.195021
87.038011	3004.891010	22.200039
86.702621	3012.382688	22.205056
86.836897	3010.931792	22.210074
87.124072	3000.991948	22.215091
87.202760	3007.269885	22.220109
87.569356	3002.635835	22.225127
87.609176	3003.080848	22.230144
87.302084	3012.537576	22.235162
87.683569	2992.874416	22.240179
87.070906	3004.111780	22.245197
87.610506	3023.021314	22.250215
87.544302	3022.630756	22.255232
87.606536	3020.566213	22.260250
88.123071	3017.212191	22.265267
87.877342	3026.627750	22.270285
88.252818	3028.175354	22.275303
88.046184	3018.177150	22.280320
87.999548	3028.236950	22.285338
88.375221	3026.401048	22.290355
88.110233	3041.415624	22.295373
88.088110	3050.969756	22.300391
88.432585	3045.483823	22.305408
88.370774	3046.781161	22.310426
88.451659	3059.352296	22.315443
88.847991	3066.855606	22.320461
89.045489	3077.893492	22.325479
89.040676	3075.697417	22.330496
89.097421	3073.924101	22.335514
89.547193	3077.786215	22.340531
89.216353	3073.602291	22.345549
89.083020	3077.943979	22.350567
89.627500	3064.021650	22.355584
89.085388	3076.494718	22.360602
89.461679	3074.065341	22.365619
89.547625	3097.250134	22.370637
89.590218	3093.645259	22.375655
89.695725	3094.165201	22.380672
89.789387	3092.726974	22.385690
89.914947	3100.591500	22.390707
90.336171	3116.451812	22.395725
90.059218	3121.835479	22.400743
90.504103	3121.582626	22.405760
90.287958	3123.974116	22.410778
90.291220	3125.078201	22.415795
90.339350	3122.368826	22.420813
90.222092	3121.061486	22.425831
90.699910	3139.157042	22.430848
90.661976	3144.209736	22.435866
90.687677	3139.550155	22.440883
90.525599	3154.570796	22.445901
90.743624	3154.482892	22.450919
91.249241	3172.340563	22.455936
91.109645	3171.465970	22.460954
91.267183	3169.452760	22.465971
91.349016	3175.856512	22.470989
91.322662	3177.413429	22.476007
91.398856	3182.912222	22.481024
91.462650	3196.325695	22.486042
91.858282	3188.783293	22.491059
91.629614	3187.790091	22.496077
92.092829	3212.014301	22.501095
92.403719	3212.369506	22.506112
92.201099	3217.845711	22.511130
92.389375	3212.494669	22.516147
92.864398	3212.038250	22.521165
92.801760	3210.283625	22.526183
92.986617	3210.491294	22.531200
93.029338	3214.966401	22.536218
92.896728	3209.949697	22.541235
93.112567	3217.658098	22.546253
93.318737	3211.789783	22.551271
93.662094	3197.444360	22.556288
92.971773	3206.645605	22.561306
93.150917	3196.261766	22.566323
93.378160	3210.018924	22.571341
93.317990	3206.534283	22.576359
93.077972	3215.841733	22.581376
93.509236	3230.447538	22.586394
93.601571	3232.522429	22.591411
93.717947	3242.301152	22.596429
93.618836	3239.109825	22.601447
93.637057	3249.197463	22.606464
94.028054	3255.849495	22.611482
94.102931	3251.160087	22.616499
93.858567	3254.408206	22.621517
93.998125	3265.916101	22.626535
94.363040	3272.581695	22.631552
94.264559	3287.365230	22.636570
94.609233	3280.862876	22.641587
94.898739	3282.313502	22.646605
94.799159	3282.196451	22.651623
94.931315	3271.958807	22.656640
94.526978	3290.994417	22.661658
95.151133	3299.863516	22.666675
95.439690	3303.855095	22.671693
95.146177	3300.877279	22.676711
95.397444	3305.493330	22.681728
95.463278	3308.203637	22.686746
95.574631	3297.678860	22.691763
95.838169	3304.044721	22.696781
95.615427	3301.450352	22.701799
95.897706	3302.182482	22.706816
95.775627	3321.199152	22.711834
95.878791	3317.007144	22.716851
95.968659	3320.171347	22.721869
96.161118	3326.554665	22.726887
96.098754	3318.907213	22.731904
96.404751	3336.969919	22.736922
96.593240	3341.248624	22.741939
96.454010	3339.846865	22.746957
96.391711	3339.335750	22.751975
96.686265	3339.886050	22.756992
96.579063	3361.636929	22.762010
97.004455	3361.071500	22.767027
96.904332	3369.091440	22.772045
97.290988	3374.393306	22.777063
97.402541	3370.525068	22.782080
97.084718	3381.748035	22.787098
97.320530	3385.643738	22.792115
97.632196	3394.511341	22.797133
97.600405	3392.404674	22.802151
97.803559	3389.585751	22.807168
97.826495	3390.456362	22.812186
97.585918	3396.809704	22.817203
97.796107	3408.776911	22.822221
97.982002	3418.459617	22.827239
97.900253	3425.425657	22.832256
98.388761	3423.890823	22.837274
98.781146	3433.345496	22.842291
98.977457	3440.795080	22.847309
98.669944	3441.225082	22.852327
98.820701	3440.601677	22.857344
98.868103	3446.619538	22.862362
99.031400	3444.643271	22.867379
99.231776	3446.742292	22.872397
99.006051	3438.350247	22.877415
98.968839	3436.825182	22.882432
99.090348	3459.430423	22.887450
99.393221	3460.452869	22.892467
99.391107	3460.339484	22.897485
99.221822	3466.246111	22.902503
99.563815	3469.613876	22.907520
99.758404	3486.706262	22.912538
99.698326	3487.308971	22.917555
99.759784	3484.881522	22.922573
99.999281	3492.529521	22.927591
100.384262	3500.126323	22.932608
100.124694	3516.238840	22.937626
100.322274	3511.962555	22.942643
100.619174	3515.315299	22.947661
100.569339	3512.958939	22.952679
101.009257	3516.917383	22.957696
100.876093	3513.636654	22.962714
100.957058	3525.633653	22.967731
101.125086	3524.672970	22.972749
101.126408	3535.000137	22.977767
101.461686	3527.864748	22.982784
101.328215	3539.305121	22.987802
101.317800	3528.859257	22.992819
101.452956	3528.449767	22.997837
101.414212	3535.974092	23.002855
101.752490	3544.427279	23.007872
101.641082	3557.057295	23.012890
101.292076	3563.298274	23.017907
101.689455	3564.059727	23.022925
101.696961	3574.417511	23.027943
101.998589	3581.358266	23.032960
102.535977	3580.838411	23.037978
102.121788	3584.914902	23.042995
102.546519	3579.498300	23.048013
102.297861	3593.450250	23.053031
102.815998	3602.149886	23.058048
102.932437	3613.311272	23.063066
103.061719	3613.537122	23.068083
103.237151	3603.971121	23.073101
102.680227	3604.948371	23.078119
103.247523	3606.819483	23.083136
103.292135	3628.894094	23.088154
103.385907	3628.958222	23.093171
103.443168	3621.033081	23.098189
103.558934	3630.976239	23.103207
103.548141	3628.553777	23.108224
104.183854	3655.194560	23.113242
104.286208	3659.044948	23.118259
104.191048	3659.482717	23.123277
104.137279	3661.144973	23.128295
104.221900	3655.358685	23.133312
104.279584	3658.985660	23.138330
104.310106	3650.029417	23.143347
104.822175	3664.891203	23.148365
105.029895	3678.607588	23.153383
104.714964	3677.394303	23.158400
105.221722	3681.717916	23.163418
104.970331	3672.913145	23.168435
105.099258	3672.782385	23.173453
104.891230	3679.642054	23.178471
105.538631	3689.113722	23.183488
105.324206	3701.712633	23.188506
105.432945	3698.779045	23.193523
106.149645	3697.912304	23.198541
106.070071	3709.928264	23.203559
106.141623	3700.141762	23.208576
105.971980	3706.967020	23.213594
105.747207	3713.112833	23.218611
106.367500	3714.177098	23.223629
106.357089	3725.099606	23.228647
106.495321	3726.880136	23.233664
106.288904	3725.170081	23.238682
105.986011	3722.963813	23.243699
106.325078	3737.764387	23.248717
106.772409	3758.346234	23.253735
106.744454	3752.198790	23.258752
106.811455	3754.508124	23.263770
107.088171	3768.324240	23.268787
107.269841	3781.558705	23.273805
107.242560	3780.262470	23.278823
107.361414	3782.112325	23.283840
107.593143	3793.558769	23.288858
107.330405	3786.494876	23.293875
107.987720	3795.608378	23.298893
107.917812	3798.122237	23.303911
108.145535	3798.986034	23.308928
108.482150	3793.690490	23.313946
108.473129	3793.281487	23.318963
108.609792	3798.632115	23.323981
108.241850	3799.112624	23.328999
108.374219	3797.232700	23.334016
108.822566	3820.923476	23.339034
108.689920	3822.582323	23.344051
108.999555	3829.562952	23.349069
108.630834	3826.685209	23.354087
108.863423	3823.375528	23.359104
108.764545	3823.978015	23.364122
109.191257	3836.858493	23.369139
109.552085	3852.612131	23.374157
109.732872	3846.027936	23.379175
109.681546	3845.152104	23.384192
109.708293	3843.108810	23.389210
109.645622	3856.157508	23.394227
109.805493	3844.592679	23.399245
109.742276	3862.369711	23.404263
110.131716	3863.653223	23.409280
110.091003	3867.415597	23.414298
110.280862	3865.135269	23.419315
109.910624	3872.124583	23.424333
110.176733	3889.635412	23.429351
110.484929	3898.431211	23.434368
110.743500	3909.002363	23.439386
110.553563	3918.359141	23.444403
110.884151	3923.414287	23.449421
111.132821	3925.357448	23.454439
111.013121	3928.267361	23.459456
110.845444	3933.504734	23.464474
110.927388	3946.331988	23.469491
111.448153	3945.975705	23.474509
111.397842	3962.093708	23.479527
111.442438	3972.234431	23.484544
111.854982	3970.496821	23.489562
111.799778	3974.169952	23.494579
112.394832	3975.089838	23.499597
112.385554	3990.800577	23.504615
112.281600	4000.907774	23.509632
112.700873	3995.763355	23.514650
112.634763	3998.374494	23.519667
112.646640	3997.640260	23.524685
112.621367	4002.587049	23.529703
113.192987	4011.688836	23.534720
112.854542	4016.861452	23.539738
112.974858	4019.212970	23.544755
113.365240	4019.694620	23.549773
112.845183	4024.261255	23.554791
113.491625	4033.783758	23.559808
113.618029	4041.916856	23.564826
113.584875	4036.546605	23.569843
113.844959	4034.479358	23.574861
114.083831	4046.622409	23.579879
114.109958	4063.347183	23.584896
114.401957	4060.514238	23.589914
114.418822	4066.477118	23.594931
114.748142	4066.387558	23.599949
114.347059	4070.064395	23.604967
114.670352	4062.362521	23.609984
114.765082	4069.500013	23.615002
115.113949	4085.470364	23.620019
115.340853	4098.464400	23.625037
114.994090	4088.411802	23.630055
115.360054	4093.915977	23.635072
115.498844	4089.251060	23.640090
115.120573	4100.316649	23.645107
115.662026	4088.322583	23.650125
115.750638	4089.526986	23.655143
115.822992	4097.595980	23.660160
115.669808	4107.613100	23.665178
115.704380	4111.512082	23.670195
115.891131	4107.335204	23.675213
116.054907	4124.309920	23.680231
115.968352	4132.110278	23.685248
116.378856	4135.113916	23.690266
116.457405	4135.925347	23.695283
116.619759	4136.079738	23.700301
116.692826	4152.557352	23.705319
116.689850	4157.585913	23.710336
117.011562	4160.748662	23.715354
116.751846	4161.935045	23.720371
117.144919	4177.573440	23.725389
117.158060	4178.799143	23.730407
117.177259	4181.592641	23.735424
117.130617	4184.598467	23.740442
117.236448	4202.885941	23.745459
117.675614	4217.191447	23.750477
117.744861	4215.229832	23.755495
117.956102	4229.842511	23.760512
118.074186	4236.023165	23.765530
118.102562	4242.053741	23.770547
118.614593	4232.911298	23.775565
118.468288	4237.504653	23.780583
118.561635	4250.832209	23.785600
118.524044	4264.382302	23.790618
118.764586	4269.132853	23.795635
119.342388	4267.192564	23.800653
119.285206	4265.623212	23.805671
119.121611	4262.896335	23.810688
119.655479	4271.650647	23.815706
119.677121	4284.736947	23.820723
119.800739	4287.974944	23.825741
119.884314	4292.844786	23.830759
119.959079	4290.538246	23.835776
120.375187	4292.613038	23.840794
119.968747	4298.430831	23.845811
120.191926	4310.977387	23.850829
120.169979	4310.766098	23.855847
120.106728	4320.052731	23.860864
120.377278	4318.665606	23.865882
120.444980	4345.661539	23.870899
120.460180	4345.337110	23.875917
120.838263	4349.283331	23.880935
120.489083	4356.872415	23.885952
120.773106	4362.102272	23.890970
120.772983	4378.313789	23.895987
121.353338	4377.477851	23.901005
121.418626	4391.346505	23.906023
121.739386	4397.283979	23.911040
121.654737	4391.432438	23.916058
121.845854	4417.443264	23.921075
122.389384	4416.938210	23.926093
122.365133	4416.632586	23.931111
122.265878	4423.103029	23.936128
122.690274	4417.591539	23.941146
122.702833	4425.114508	23.946163
122.682541	4417.103320	23.951181
122.846257	4429.722403	23.956199
123.048903	4435.242801	23.961216
123.040416	4441.888418	23.966234
123.161096	4448.015078	23.971251
123.170050	4446.501635	23.976269
123.058090	4456.790258	23.981287
123.269005	4465.440595	23.986304
123.581234	4464.716103	23.991322
123.529405	4482.583495	23.996339
123.558351	4489.185387	24.001357
124.150799	4489.619612	24.006375
124.078791	4497.818721	24.011392
124.308693	4497.356489	24.016410
124.254144	4500.139495	24.021427
124.444501	4514.635729	24.026445
124.741489	4511.476815	24.031463
124.577301	4514.627371	24.036480
124.917039	4517.894680	24.041498
124.746213	4518.502148	24.046515
125.012246	4526.373695	24.051533
125.004538	4537.233137	24.056551
125.290661	4548.965092	24.061568
125.417269	4549.011454	24.066586
125.161983	4551.361913	24.071603
125.582973	4565.073965	24.076621
125.712152	4575.369067	24.081639
125.968912	4573.999867	24.086656
126.053522	4577.019916	24.091674
126.050856	4582.926052	24.096691
126.155928	4592.053880	24.101709
126.563118	4592.965356	24.106727
126.500595	4598.868249	24.111744
126.726730	4600.174245	24.116762
126.853160	4613.831474	24.121779
126.947316	4613.794538	24.126797
127.313197	4621.221199	24.131815
126.920264	4622.014979	24.136832
126.890121	4624.298610	24.141850
127.019804	4635.726853	24.146867
127.181175	4645.133129	24.151885
127.636668	4664.032309	24.156903
127.584693	4673.636163	24.161920
127.834691	4672.968761	24.166938
127.935618	4689.534036	24.171955
128.183136	4694.681327	24.176973
128.001736	4698.472227	24.181991
128.049258	4703.625601	24.187008
128.506962	4718.105365	24.192026
128.319243	4730.258890	24.197043
128.524958	4728.585179	24.202061
128.939708	4741.537620	24.207079
129.134120	4753.063118	24.212096
129.427555	4752.963396	24.217114
129.410706	4760.298563	24.222131
129.621080	4768.548249	24.227149
130.020754	4769.328338	24.232167
130.042401	4778.131580	24.237184
129.680177	4777.995692	24.242202
130.263599	4785.404121	24.247219
130.007057	4791.324847	24.252237
130.350421	4795.267137	24.257255
130.265874	4806.735364	24.262272
130.565345	4800.125918	24.267290
130.449020	4806.523414	24.272307
130.621137	4822.664150	24.277325
131.004331	4826.906391	24.282343
130.719565	4841.382626	24.287360
130.805323	4845.317937	24.292378
131.410551	4857.224212	24.297395
131.135210	4862.683894	24.302413
131.948033	4869.444048	24.307431
131.351173	4887.911743	24.312448
131.940798	4876.297871	24.317466
131.974232	4891.671258	24.322483
132.088188	4895.438022	24.327501
132.355418	4899.013476	24.332519
132.195731	4913.246057	24.337536
132.421434	4909.656326	24.342554
132.660496	4912.488092	24.347571
132.906595	4924.548529	24.352589
133.268088	4921.748757	24.357607
133.403647	4932.551268	24.362624
133.138225	4932.277106	24.367642
133.246325	4930.438747	24.372659
133.429747	4921.195929	24.377677
133.549192	4918.904406	24.382695
133.701410	4942.567286	24.387712
133.811030	4947.950899	24.392730
133.789389	4944.560897	24.397747
133.651928	4946.192190	24.402765
133.934073	4965.052554	24.407783
133.925089	4976.325968	24.412800
134.047420	4982.585126	24.417818
134.576758	4987.659939	24.422835
134.304562	5005.205675	24.427853
134.504584	5003.813767	24.432871
134.646364	5013.292748	24.437888
134.990067	5025.981901	24.442906
134.996666	5040.295852	24.447923
135.133169	5046.862156	24.452941
135.213820	5061.227654	24.457959
135.737237	5063.614009	24.462976
135.878441	5073.604478	24.467994
135.933331	5078.564252	24.473011
136.129470	5094.988716	24.478029
136.271994	5084.382265	24.483047
136.418549	5091.155345	24.488064
136.299553	5110.157619	24.493082
136.580533	5114.251799	24.498099
136.959935	5116.910095	24.503117
136.840019	5120.221117	24.508135
137.056820	5139.792663	24.513152
137.235087	5138.299985	24.518170
137.565848	5140.325116	24.523187
137.215072	5139.499292	24.528205
137.517154	5161.683788	24.533223
137.542994	5161.673337	24.538240
137.909849	5164.415677	24.543258
138.545119	5182.987355	24.548275
138.207091	5193.434919	24.553293
138.483335	5196.958514	24.558311
138.616327	5191.950155	24.563328
138.833490	5200.539888	24.568346
138.738782	5193.625889	24.573363
138.487398	5209.943798	24.578381
138.806763	5209.536979	24.583399
139.029114	5212.882781	24.588416
139.189429	5222.071715	24.593434
139.326171	5234.364140	24.598451
139.386760	5242.252401	24.603469
139.670787	5245.607487	24.608487
139.969328	5257.776723	24.613504
139.980170	5258.261054	24.618522
140.083477	5264.734783	24.623539
140.148472	5277.278379	24.628557
140.687362	5291.291328	24.633575
140.055766	5297.933866	24.638592
140.664659	5295.515110	24.643610
141.248076	5305.354353	24.648627
141.004204	5326.096776	24.653645
141.320865	5321.485751	24.658663
141.346480	5319.148902	24.663680
141.327562	5317.365127	24.668698
141.444626	5324.761613	24.673715
141.336243	5340.277548	24.678733
141.698940	5333.818993	24.683751
141.823418	5347.126693	24.688768
142.035611	5360.745793	24.693786
142.331250	5362.691223	24.698803
141.947726	5373.038690	24.703821
142.248074	5372.622220	24.708839
142.524467	5392.108941	24.713856
142.659550	5393.400851	24.718874
142.954740	5398.171547	24.723891
142.695137	5399.702063	24.728909
143.031672	5414.785344	24.733927
143.112542	5424.873844	24.738944
143.396723	5423.228815	24.743962
143.528762	5435.954572	24.748979
143.209323	5446.620332	24.753997
143.739291	5443.645725	24.759015
143.916221	5459.593716	24.764032
143.517888	5470.477033	24.769050
144.058427	5479.073054	24.774067
143.938022	5498.745163	24.779085
144.367184	5502.399538	24.784103
144.745559	5523.606584	24.789120
145.010213	5534.509180	24.794138
144.895881	5522.579038	24.799155
144.787837	5532.280514	24.804173
145.195567	5549.297257	24.809191
145.542597	5557.939415	24.814208
145.192553	5561.605394	24.819226
145.928650	5573.990392	24.824243
145.595949	5583.806008	24.829261
145.893157	5580.059738	24.834279
146.195574	5603.311673	24.839296
146.233810	5610.155579	24.844314
146.563190	5609.630386	24.849331
146.686307	5610.914716	24.854349
146.843559	5624.103843	24.859367
147.054529	5633.553366	24.864384
147.064682	5630.499177	24.869402
147.682132	5642.868087	24.874419
147.393544	5661.518701	24.879437
147.975340	5663.952813	24.884455
147.691379	5664.155045	24.889472
148.121925	5671.685647	24.894490
148.281897	5666.398300	24.899507
148.124744	5682.591384	24.904525
148.552961	5691.148283	24.909543
148.584092	5685.906369	24.914560
148.238964	5689.991442	24.919578
148.685929	5704.028581	24.924595
148.879731	5712.325486	24.929613
149.184546	5711.763102	24.934631
149.294129	5729.855805	24.939648
149.034051	5743.224040	24.944666
149.530325	5736.258286	24.949683
149.927016	5741.379347	24.954701
150.021517	5758.420104	24.959719
149.849232	5762.970561	24.964736
149.786562	5767.655367	24.969754
149.915282	5769.282911	24.974771
149.996326	5785.015769	24.979789
150.528530	5788.297351	24.984807
150.621039	5798.633614	24.989824
150.676870	5809.843723	24.994842
151.239951	5811.456886	24.999859
150.953201	5821.076027	25.004877
151.056435	5830.700367	25.009895
151.420049	5845.536696	25.014912
151.245026	5847.006646	25.019930
151.716863	5850.869063	25.024947
151.823294	5874.199398	25.029965
151.982628	5876.178865	25.034983
152.328339	5872.090325	25.040000
152.190058	5887.523020	25.045018
152.410388	5889.167790	25.050035
152.662907	5899.561116	25.055053
152.461863	5903.895142	25.060071
153.194128	5912.881178	25.065088
152.754151	5926.407155	25.070106
153.217809	5926.107143	25.075123
153.340983	5932.417002	25.080141
153.511898	5954.427294	25.085159
153.627689	5953.695642	25.090176
153.513288	5956.431425	25.095194
154.111393	5963.061482	25.100211
154.020362	5981.488910	25.105229
154.646476	5984.487493	25.110247
154.730241	5980.885067	25.115264
154.342602	5984.446533	25.120282
154.978553	5994.072733	25.125299
154.931610	6005.573700	25.130317
154.863198	5995.012396	25.135335
155.175643	6020.261509	25.140352
155.247721	6035.544572	25.145370
155.372596	6036.317264	25.150387
155.230123	6044.947953	25.155405
155.785209	6058.087693	25.160423
155.665318	6064.104219	25.165440
155.857770	6080.249196	25.170458
156.293521	6082.753597	25.175475
156.434662	6094.613435	25.180493
156.557861	6109.430821	25.185511
157.036956	6115.053631	25.190528
156.796518	6111.142100	25.195546
157.026903	6121.769465	25.200563
157.095135	6135.550594	25.205581
157.419304	6135.862747	25.210599
157.677941	6135.528560	25.215616
157.804651	6162.997764	25.220634
158.140194	6165.366351	25.225651
157.949245	6156.127897	25.230669
158.307779	6186.281954	25.235687
158.724961	6188.732457	25.240704
158.862893	6181.570134	25.245722
158.971199	6184.482564	25.250739
158.852006	6191.449212	25.255757
158.777722	6194.128237	25.260775
159.155534	6193.213471	25.265792
159.131132	6210.304844	25.270810
159.404409	6217.045863	25.275827
159.434375	6214.992329	25.280845
159.693574	6234.921436	25.285863
160.214859	6242.990497	25.290880
159.984054	6255.940979	25.295898
160.276191	6255.541563	25.300915
160.689231	6270.774563	25.305933
160.443746	6285.286820	25.310951
160.892507	6287.451435	25.315968
161.015121	6290.188017	25.320986
161.199012	6303.367146	25.326003
161.147802	6309.073097	25.331021
161.129575	6321.084321	25.336039
161.570129	6325.340027	25.341056
161.797461	6336.952917	25.346074
161.712046	6334.949013	25.351091
161.951748	6349.189587	25.356109
162.258296	6367.441471	25.361127
162.670244	6362.202840	25.366144
162.742747	6375.573096	25.371162
162.996653	6366.968811	25.376179
163.039596	6384.504376	25.381197
162.909947	6399.765681	25.386215
163.168840	6391.665693	25.391232
163.348464	6392.426666	25.396250
163.349986	6398.938841	25.401267
163.343956	6412.854929	25.406285
163.297260	6427.493995	25.411303
164.278860	6436.747442	25.416320
163.695328	6447.600368	25.421338
164.104226	6449.537644	25.426355
164.589782	6464.727876	25.431373
164.805670	6477.425438	25.436391
164.723506	6475.117955	25.441408
164.657091	6486.215043	25.446426
164.829711	6495.001774	25.451443
165.118822	6505.585436	25.456461
165.505615	6516.242192	25.461479
165.711523	6521.746929	25.466496
165.847182	6522.562148	25.471514
165.735791	6525.250191	25.476531
166.190944	6536.038307	25.481549
166.050209	6557.643563	25.486567
166.162181	6559.646309	25.491584
166.534960	6571.179737	25.496602
166.828087	6568.178923	25.501619
166.791760	6583.460485	25.506637
166.780770	6600.240749	25.511655
166.774111	6598.739044	25.516672
166.889277	6620.013853	25.521690
167.448754	6627.006930	25.526707
167.334386	6628.164382	25.531725
167.564056	6660.132498	25.536743
167.923555	6667.226370	25.541760
168.011787	6677.368074	25.546778
168.310400	6693.121293	25.551795
168.568608	6706.292226	25.556813
168.893822	6712.892703	25.561831
169.261463	6711.193448	25.566848
168.968189	6729.100858	25.571866
169.375419	6736.749203	25.576883
169.768601	6729.941287	25.581901
169.847767	6739.614071	25.586919
170.377111	6750.011866	25.591936
170.377014	6749.282555	25.596954
170.414234	6757.314033	25.601971
170.411700	6756.329396	25.606989
170.301924	6766.473758	25.612007
170.362595	6776.569323	25.617024
170.501959	6787.302884	25.622042
170.617409	6805.449396	25.627059
171.032697	6806.609117	25.632077
171.365205	6832.203463	25.637095
171.792795	6846.184535	25.642112
171.699637	6842.764346	25.647130
172.148219	6853.894624	25.652147
172.294474	6865.387960	25.657165
172.177766	6866.514224	25.662183
172.359269	6870.378149	25.667200
172.622623	6886.099175	25.672218
172.574486	6895.062742	25.677236
173.017165	6901.322881	25.682253
173.068191	6903.126858	25.687271
173.168248	6916.780469	25.692288
173.306160	6918.873898	25.697306
173.548728	6935.327467	25.702324
174.026464	6942.257706	25.707341
173.676988	6951.098036	25.712359
174.015397	6961.478510	25.717376
174.324038	6974.300789	25.722394
174.528825	6972.658593	25.727412
174.766480	6972.210874	25.732429
174.818582	6997.524218	25.737447
175.082338	7006.461076	25.742464
175.373492	7009.569133	25.747482
175.089960	7005.196937	25.752500
175.168799	7018.519315	25.757517
175.563282	7028.594292	25.762535
175.969134	7022.775557	25.767552
175.896078	7037.738088	25.772570
176.011519	7045.858459	25.777588
176.402761	7054.507030	25.782605
176.385759	7061.713707	25.787623
176.773980	7075.549590	25.792640
176.895674	7087.204760	25.797658
176.585265	7094.668931	25.802676
176.960831	7104.519615	25.807693
176.952721	7121.527202	25.812711
177.486025	7128.537201	25.817728
177.976215	7132.605376	25.822746
177.561362	7146.447161	25.827764
178.147231	7165.514768	25.832781
177.647087	7176.086716	25.837799
178.218306	7184.893412	25.842816
178.667162	7194.009721	25.847834
178.548244	7207.675755	25.852852
179.003363	7215.815597	25.857869
178.981402	7228.020572	25.862887
179.445378	7246.033994	25.867904
179.485223	7251.173504	25.872922
179.573083	7259.718166	25.877940
179.895311	7267.837809	25.882957
179.983251	7286.487906	25.887975
180.528358	7287.444218	25.892992
180.537280	7296.048617	25.898010
180.618365	7302.106672	25.903028
181.228752	7313.215037	25.908045
181.253953	7335.666532	25.913063
181.186479	7326.202941	25.918080
181.730895	7329.830161	25.923098
181.695384	7346.255052	25.928116
181.704361	7352.611704	25.933133
181.752742	7370.832421	25.938151
182.073247	7372.783646	25.943168
182.625849	7375.869749	25.948186
182.458925	7381.183752	25.953204
182.855544	7399.207877	25.958221
182.777910	7411.560603	25.963239
182.958619	7403.346142	25.968256
183.341899	7427.307516	25.973274
183.214665	7435.144064	25.978292
183.402996	7440.771797	25.983309
183.518093	7459.427285	25.988327
183.791410	7453.329265	25.993344
184.010116	7466.210175	25.998362
183.805161	7487.280420	26.003380
184.337381	7496.497473	26.008397
184.479945	7512.184288	26.013415
184.510018	7517.622162	26.018432
184.462060	7535.630829	26.023450
184.799954	7553.282308	26.028468
185.105984	7563.238842	26.033485
185.427719	7586.906992	26.038503
185.462187	7593.392328	26.043520
186.182589	7593.860271	26.048538
186.078817	7606.734973	26.053556
185.983715	7618.522310	26.058573
186.393936	7636.086768	26.063591
186.584514	7635.516972	26.068608
187.000953	7643.640965	26.073626
187.038170	7660.455683	26.078644
187.197139	7658.520688	26.083661
187.369773	7670.742826	26.088679
187.785194	7668.290942	26.093696
188.011266	7675.646044	26.098714
188.191750	7696.334127	26.103732
188.434492	7700.074980	26.108749
188.262932	7704.815221	26.113767
188.445723	7717.042113	26.118784
188.631624	7729.893619	26.123802
188.530996	7738.401734	26.128820
188.955298	7744.283040	26.133837
189.536277	7754.382870	26.138855
189.295231	7763.793810	26.143872
189.585709	7773.860235	26.148890
189.450424	7788.807866	26.153908
189.930593	7808.063180	26.158925
190.200595	7816.955256	26.163943
190.212015	7822.061493	26.168960
190.755918	7848.154520	26.173978
190.579847	7853.144913	26.178996
191.429311	7857.712611	26.184013
191.188960	7874.283716	26.189031
191.037189	7883.709144	26.194048
191.749102	7902.479948	26.199066
191.782347	7909.704342	26.204084
192.601949	7904.505599	26.209101
192.595456	7906.732261	26.214119
192.477938	7929.768795	26.219136
192.651502	7931.373723	26.224154
192.769738	7936.065467	26.229172
193.220936	7947.410680	26.234189
193.286535	7954.939416	26.239207
193.089514	7961.833682	26.244224
193.220935	7972.875414	26.249242
193.519915	7993.965159	26.254260
194.008415	8004.493193	26.259277
193.737766	8017.495350	26.264295
194.074057	8034.323540	26.269312
194.161387	8040.093564	26.274330
194.460582	8051.560524	26.279348
194.907611	8064.194557	26.284365
194.693471	8080.944852	26.289383
195.359197	8094.384433	26.294400
195.329623	8111.977201	26.299418
195.462476	8119.517568	26.304436
195.764833	8126.374705	26.309453
195.788846	8137.307078	26.314471
196.239702	8150.208925	26.319488
196.686925	8152.411894	26.324506
196.646737	8181.823466	26.329524
196.560757	8186.048441	26.334541
197.116454	8189.872966	26.339559
197.253221	8210.331689	26.344576
197.750660	8204.712924	26.349594
197.786784	8220.508572	26.354612
198.072269	8230.534987	26.359629
197.901636	8234.047096	26.364647
197.773969	8243.585744	26.369664
198.315903	8256.978538	26.374682
198.414341	8265.345210	26.379700
198.619113	8285.171407	26.384717
199.203113	8293.780894	26.389735
199.048118	8310.711558	26.394752
199.373369	8318.414451	26.399770
199.562613	8330.590223	26.404788
199.541594	8341.337186	26.409805
199.769586	8345.093110	26.414823
200.035930	8357.266293	26.419840
200.113855	8357.898054	26.424858
200.352856	8375.139597	26.429876
200.595145	8393.293059	26.434893
200.849668	8399.810504	26.439911
200.951688	8416.625229	26.444928
201.234740	8416.344011	26.449946
201.090619	8437.187962	26.454964
201.557274	8447.173483	26.459981
201.742980	8456.805220	26.464999
201.931794	8469.631527	26.470016
202.241665	8480.516163	26.475034
202.595308	8490.689900	26.480052
202.779601	8496.946865	26.485069
203.183194	8518.645940	26.490087
203.197162	8529.567489	26.495104
203.476472	8535.279177	26.500122
203.487269	8548.906936	26.505140
203.835256	8564.622450	26.510157
203.869424	8567.651061	26.515175
203.983712	8581.107928	26.520192
204.377028	8602.407749	26.525210
204.256022	8617.009676	26.530228
204.513439	8611.974585	26.535245
204.828720	8628.730836	26.540263
204.857484	8649.412181	26.545280
205.403161	8665.412531	26.550298
205.480539	8682.329231	26.555316
205.527331	8691.976538	26.560333
205.794519	8700.339070	26.565351
206.394778	8726.307693	26.570368
206.620909	8722.682431	26.575386
206.488536	8739.698344	26.580404
206.849747	8748.011439	26.585421
207.276912	8760.655377	26.590439
207.424057	8784.541845	26.595456
207.586843	8786.555818	26.600474
207.653794	8799.303570	26.605492
207.893098	8804.412265	26.610509
208.370858	8813.395406	26.615527
208.645551	8834.988756	26.620544
208.753222	8832.597564	26.625562
208.854766	8839.896865	26.630580
209.004336	8861.929760	26.635597
209.399072	8863.515908	26.640615
209.611844	8876.562907	26.645632
209.673858	8892.342443	26.650650
209.693048	8899.023222	26.655668
210.061538	8908.190860	26.660685
210.237335	8920.760626	26.665703
210.207840	8937.122839	26.670720
210.710720	8953.840524	26.675738
210.214402	8957.444834	26.680756
210.797028	8980.423504	26.685773
211.692150	8987.753248	26.690791
211.859387	9014.453135	26.695808
212.118783	9006.762374	26.700826
211.935189	9019.915770	26.705844
212.078025	9031.253128	26.710861
212.224841	9040.834431	26.715879
212.409111	9057.210621	26.720896
212.472613	9069.160311	26.725914
212.904316	9081.522760	26.730932
213.157155	9094.222651	26.735949
213.424251	9104.287150	26.740967
213.721939	9122.467377	26.745984
213.496588	9126.092415	26.751002
213.549275	9142.350374	26.756020
213.441517	9157.607364	26.761037
214.167837	9173.403047	26.766055
214.202632	9188.871370	26.771072
214.659422	9207.746617	26.776090
214.516060	9222.346207	26.781108
215.184062	9233.730867	26.786125
215.215330	9240.210966	26.791143
215.393886	9270.158306	26.796160
216.015965	9274.367324	26.801178
216.095729	9282.671076	26.806196
216.310470	9305.913007	26.811213
216.362769	9308.616853	26.816231
216.359171	9316.602163	26.821248
217.165148	9341.219665	26.826266
217.339759	9350.402109	26.831284
217.119866	9354.010550	26.836301
217.376356	9360.490139	26.841319
217.639820	9382.322683	26.846336
218.015540	9400.588835	26.851354
217.972617	9408.084645	26.856372
218.502429	9437.071074	26.861389
218.918032	9439.954824	26.866407
218.643312	9461.243463	26.871424
219.059694	9462.996770	26.876442
219.411793	9478.674527	26.881460
219.606804	9490.051351	26.886477
220.376150	9504.542911	26.891495
219.984501	9524.836433	26.896512
219.978234	9529.604918	26.901530
220.455150	9547.182846	26.906548
220.673360	9558.151937	26.911565
220.909226	9568.884625	26.916583
220.944810	9585.344562	26.921600
221.196514	9600.763460	26.926618
221.608272	9608.781705	26.931636
221.947393	9638.019336	26.936653
221.952453	9634.463262	26.941671
222.425369	9657.914620	26.946688
222.510542	9656.047813	26.951706
222.618560	9675.009747	26.956724
222.634502	9691.611780	26.961741
223.160915	9711.382799	26.966759
223.122651	9724.103465	26.971776
223.410019	9745.844284	26.976794
223.954857	9743.526573	26.981812
223.803604	9771.328848	26.986829
224.374075	9780.417917	26.991847
224.367734	9806.508340	26.996864
224.389197	9811.856670	27.001882
225.072735	9834.160694	27.006900
224.875234	9850.291121	27.011917
225.612281	9856.701916	27.016935
225.594413	9881.035577	27.021952
226.118098	9885.743234	27.026970
226.095818	9900.292811	27.031988
226.205211	9924.423462	27.037005
226.506872	9929.137495	27.042023
226.656701	9945.336732	27.047040
227.006640	9951.246183	27.052058
227.457109	9966.571098	27.057076
227.257788	9990.399722	27.062093
227.687889	10006.463541	27.067111
227.680822	10015.826331	27.072128
228.275098	10026.310532	27.077146
228.492912	10043.436961	27.082164
228.460396	10052.787969	27.087181
228.879454	10057.575210	27.092199
229.013125	10081.282321	27.097216
228.842629	10080.399599	27.102234
229.930355	10103.325792	27.107252
229.319374	10111.776013	27.112269
230.085421	10127.812568	27.117287
229.896953	10130.358489	27.122304
230.056551	10152.265041	27.127322
230.529923	10155.379821	27.132340
230.630346	10172.859449	27.137357
230.755036	10182.874220	27.142375
230.680177	10210.387324	27.147392
231.012303	10226.056210	27.152410
231.462120	10243.989521	27.157428
231.442313	10273.268589	27.162445
231.697115	10282.735733	27.167463
232.408877	10307.255607	27.172480
232.545952	10315.389810	27.177498
232.901977	10329.684694	27.182516
232.911435	10348.776421	27.187533
233.275679	10363.960455	27.192551
233.521158	10391.010010	27.197568
233.442289	10402.585014	27.202586
234.075051	10414.209575	27.207604
234.088805	10426.635238	27.212621
234.426091	10443.976973	27.217639
234.878253	10450.817820	27.222656
235.339795	10471.199734	27.227674
235.245647	10481.460500	27.232692
235.603491	10497.690780	27.237709
235.798073	10505.039309	27.242727
236.107455	10522.151833	27.247744
236.182921	10536.929721	27.252762
236.680599	10540.662790	27.257780
236.504414	10561.198384	27.262797
236.990800	10583.666807	27.267815
237.519104	10589.040159	27.272832
237.630323	10607.611005	27.277850
238.070258	10616.888283	27.282868
237.830003	10626.521566	27.287885
238.406762	10635.954241	27.292903
238.044226	10655.063508	27.297920
238.214472	10674.297728	27.302938
238.949677	10677.867314	27.307956
238.968969	10710.020616	27.312973
239.480403	10715.134571	27.317991
239.710621	10741.918633	27.323008
239.796304	10749.956877	27.328026
239.964547	10758.013766	27.333044
240.104911	10776.264458	27.338061
240.365719	10796.845525	27.343079
240.593082	10804.741610	27.348096
240.925262	10822.264477	27.353114
241.273264	10837.877711	27.358132
241.227204	10862.763323	27.363149
242.092404	10866.483091	27.368167
241.972982	10881.935926	27.373184
241.917900	10905.398941	27.378202
242.402432	10925.187282	27.383220
242.534465	10938.071549	27.388237
243.029737	10946.437254	27.393255
243.110412	10960.216863	27.398272
243.376519	10980.475227	27.403290
243.956152	10988.047810	27.408308
243.831170	11011.408235	27.413325
244.212472	11024.607163	27.418343
244.197975	11037.492350	27.423360
244.733855	11060.269353	27.428378
244.880796	11064.947918	27.433396
244.920897	11070.031607	27.438413
245.325073	11079.415761	27.443431
245.514157	11099.493706	27.448448
245.518321	11115.271552	27.453466
246.051896	11127.480469	27.458484
245.969997	11145.532676	27.463501
246.419415	11171.395722	27.468519
246.663591	11181.619658	27.473536
246.555335	11203.613608	27.478554
247.116924	11206.433719	27.483572
247.181895	11233.869581	27.488589
247.840569	11257.300164	27.493607
248.035025	11263.215444	27.498624
247.705193	11289.184937	27.503642
248.396969	11304.384736	27.508660
248.666498	11328.940496	27.513677
248.721297	11341.638207	27.518695
248.995547	11354.399437	27.523712
249.160670	11383.900722	27.528730
249.690966	11392.848465	27.533748
249.876655	11417.158546	27.538765
250.057654	11424.323263	27.543783
250.422063	11443.309977	27.548800
250.515539	11465.721019	27.553818
250.754273	11479.567821	27.558836
251.430398	11505.556855	27.563853
251.551812	11517.230634	27.568871
252.083688	11541.429806	27.573888
251.876354	11548.933281	27.578906
252.288672	11562.812948	27.583924
252.189842	11582.636532	27.588941
252.762661	11593.620737	27.593959
253.054419	11608.387689	27.598976
253.103859	11628.383871	27.603994
253.489943	11640.186781	27.609012
254.085258	11665.231912	27.614029
254.052718	11684.893649	27.619047
254.445119	11696.259841	27.624064
254.786698	11711.079066	27.629082
254.991609	11730.542609	27.634100
255.304338	11741.665535	27.639117
255.185414	11757.605299	27.644135
255.470473	11768.448380	27.649152
255.721823	11800.074589	27.654170
256.127123	11804.261311	27.659188
256.156693	11830.841528	27.664205
256.826161	11852.856500	27.669223
257.155411	11852.122762	27.674240
257.464549	11873.003738	27.679258
257.370398	11884.105228	27.684276
257.617575	11903.117087	27.689293
258.152976	11919.873390	27.694311
258.625670	11931.760806	27.699328
258.373601	11949.780443	27.704346
258.950622	11967.376547	27.709364
258.837600	11981.559863	27.714381
258.603809	12000.890313	27.719399
259.113275	12015.181394	27.724416
259.464062	12032.355123	27.729434
259.972272	12053.656675	27.734452
260.309493	12065.660132	27.739469
260.476063	12095.070729	27.744487
260.807875	12104.416209	27.749504
260.643769	12121.073858	27.754522
261.472233	12144.962092	27.759540
261.527304	12162.687511	27.764557
261.662282	12179.765712	27.769575
261.893413	12190.446964	27.774592
262.078272	12203.393294	27.779610
262.591034	12216.461946	27.784628
262.559750	12236.818776	27.789645
262.804763	12253.753494	27.794663
263.166466	12262.800695	27.799680
263.402848	12292.080667	27.804698
263.764159	12301.699512	27.809716
263.966975	12319.382985	27.814733
264.198317	12339.705101	27.819751
264.629544	12366.096839	27.824768
264.877030	12378.307179	27.829786
264.905535	12392.045484	27.834804
265.153014	12401.274852	27.839821
265.566205	12432.295728	27.844839
265.859367	12446.005244	27.849856
266.082601	12470.566587	27.854874
266.394598	12489.824669	27.859892
266.800817	12500.137622	27.864909
266.858694	12521.238674	27.869927
267.127744	12539.104606	27.874944
267.243662	12559.653458	27.879962
267.645736	12572.910222	27.884980
268.065447	12599.673560	27.889997
268.481330	12618.050244	27.895015
268.913598	12632.325468	27.900032
269.134668	12651.809536	27.905050
269.336794	12663.610328	27.910068
269.510357	12690.393407	27.915085
269.466603	12699.103283	27.920103
269.968655	12704.964517	27.925120
270.191178	12739.944169	27.930138
270.725084	12752.274094	27.935156
270.733113	12769.097978	27.940173
270.800188	12788.492627	27.945191
271.446695	12802.194418	27.950208
272.097535	12823.922919	27.955226
272.176288	12834.726302	27.960244
272.518491	12858.420037	27.965261
272.726003	12865.019043	27.970279
273.056888	12875.407161	27.975296
273.159881	12898.494206	27.980314
273.709337	12920.819756	27.985332
274.003347	12927.724183	27.990349
273.700927	12943.068423	27.995367
274.456164	12953.494320	28.000384
274.553363	12976.617105	28.005402
274.486865	12992.729698	28.010420
275.066584	13008.453702	28.015437
274.893824	13028.274592	28.020455
275.057505	13035.464741	28.025472
275.408263	13069.016474	28.030490
275.780897	13090.267804	28.035508
276.293735	13105.399198	28.040525
276.257433	13144.774952	28.045543
276.734884	13157.297147	28.050560
276.553387	13171.697347	28.055578
276.998003	13198.328155	28.060596
277.693430	13218.641676	28.065613
277.659100	13246.585501	28.070631
278.075027	13270.906114	28.075648
278.394549	13284.141571	28.080666
278.690505	13305.143041	28.085684
279.143338	13328.403182	28.090701
279.241344	13344.139767	28.095719
279.581702	13366.201748	28.100736
279.697439	13384.133550	28.105754
280.311127	13402.770547	28.110772
280.580682	13413.247518	28.115789
280.795437	13434.479754	28.120807
280.834919	13443.385360	28.125824
280.703466	13465.095036	28.130842
281.487773	13475.633516	28.135860
282.254348	13485.483175	28.140877
282.119229	13519.231822	28.145895
282.266738	13520.692893	28.150912
282.725377	13549.475765	28.155930
282.718802	13565.339447	28.160948
283.075422	13583.988470	28.165965
283.199353	13609.927956	28.170983
283.674041	13631.009162	28.176000
283.727209	13647.634114	28.181018
283.514242	13673.181178	28.186036
284.456563	13698.714677	28.191053
284.506950	13732.668337	28.196071
285.088913	13749.103169	28.201088
285.248349	13765.443142	28.206106
285.528685	13785.825454	28.211124
285.774730	13815.737879	28.216141
285.798501	13837.666834	28.221159
286.482421	13849.181302	28.226176
286.657306	13888.544461	28.231194
286.871960	13910.206742	28.236212
287.413080	13925.321731	28.241229
287.633402	13950.412848	28.246247
287.963357	13969.347497	28.251264
288.659910	13992.841869	28.256282
288.887839	14010.851430	28.261300
289.328340	14025.233791	28.266317
289.439023	14053.500318	28.271335
289.856989	14062.672210	28.276352
289.813359	14080.752799	28.281370
290.192351	14104.754982	28.286388
290.827307	14113.021268	28.291405
290.800200	14139.780981	28.296423
290.848832	14158.421969	28.301440
291.469816	14178.590276	28.306458
291.644883	14195.774547	28.311476
292.075364	14208.598503	28.316493
292.080518	14236.310211	28.321511
292.497235	14259.119220	28.326528
292.842439	14281.165715	28.331546
292.857520	14298.438303	28.336564
293.222448	14319.982766	28.341581
293.421138	14350.692987	28.346599
293.910453	14363.327816	28.351616
294.557057	14382.345916	28.356634
294.787413	14405.787503	28.361652
295.455067	14413.309789	28.366669
295.492010	14446.985752	28.371687
295.796729	14442.813361	28.376704
295.732365	14473.902911	28.381722
296.085999	14491.514254	28.386740
296.138483	14508.016895	28.391757
296.489998	14528.155147	28.396775
296.827598	14552.587574	28.401792
297.037274	14572.460697	28.406810
297.349637	14594.945372	28.411828
297.476216	14611.758631	28.416845
297.640411	14643.210585	28.421863
298.013744	14663.797185	28.426880
298.297617	14700.255190	28.431898
299.005207	14722.937077	28.436916
298.852654	14747.238093	28.441933
299.003543	14772.994920	28.446951
299.528008	14790.892444	28.451968
299.838899	14815.045151	28.456986
300.046003	14830.655336	28.462004
300.603243	14857.046592	28.467021
300.661786	14888.825007	28.472039
301.033151	14908.009920	28.477056
301.242021	14924.797931	28.482074
301.563570	14953.531762	28.487092
302.103956	14972.983981	28.492109
302.131301	15011.096631	28.497127
302.293266	15030.968230	28.502144
303.059141	15046.241558	28.507162
302.959135	15071.791745	28.512180
303.508069	15086.994866	28.517197
303.405640	15118.890470	28.522215
303.915513	15131.974224	28.527232
304.252304	15174.100275	28.532250
304.207066	15203.738359	28.537268
305.005308	15223.838949	28.542285
305.313304	15254.015537	28.547303
305.862647	15275.904871	28.552320
306.163722	15298.098419	28.557338
306.294418	15323.167480	28.562356
306.704350	15336.500745	28.567373
307.080172	15369.266184	28.572391
307.550383	15391.079613	28.577408
307.669133	15406.874658	28.582426
307.790469	15428.196389	28.587444
308.263038	15456.853627	28.592461
308.508248	15475.016621	28.597479
308.880611	15496.520189	28.602496
309.259118	15521.569640	28.607514
309.582202	15545.765577	28.612532
309.720925	15568.054353	28.617549
310.079979	15591.998362	28.622567
310.613726	15613.650491	28.627584
310.903609	15644.121100	28.632602
310.857307	15673.959054	28.637620
311.435737	15690.993050	28.642637
311.644511	15712.917283	28.647655
311.697867	15727.045737	28.652672
312.189580	15761.729780	28.657690
312.248898	15793.465355	28.662708
312.526469	15815.824262	28.667725
312.802143	15849.468451	28.672743
313.258328	15871.758385	28.677760
314.239225	15902.187485	28.682778
314.425943	15930.568051	28.687796
314.503867	15950.131609	28.692813
314.836159	15964.702940	28.697831
314.928087	15990.710679	28.702848
315.601661	16020.992287	28.707866
315.644642	16046.884591	28.712884
316.092486	16068.964445	28.717901
316.467372	16096.579865	28.722919
316.725007	16121.374249	28.727936
317.152059	16142.670993	28.732954
317.302002	16169.709016	28.737972
317.940351	16192.561417	28.742989
317.990342	16212.995035	28.748007
318.234856	16235.144833	28.753024
318.933837	16261.503189	28.758042
318.898354	16287.035407	28.763060
319.407284	16308.082623	28.768077
319.496792	16328.235386	28.773095
319.828067	16361.337977	28.778112
320.121471	16382.229527	28.783130
320.456269	16404.864419	28.788148
321.015445	16430.076264	28.793165
321.422102	16435.473513	28.798183
321.440607	16454.680505	28.803200
321.684383	16476.176887	28.808218
321.961931	16503.533349	28.813236
322.309685	16518.668052	28.818253
322.546113	16557.215316	28.823271
322.809157	16587.047286	28.828288
323.360303	16593.236844	28.833306
323.487965	16626.968748	28.838324
323.367496	16643.348707	28.843341
324.059991	16672.658710	28.848359
324.098388	16711.790047	28.853376
324.615906	16747.792096	28.858394
325.022401	16778.138844	28.863412
325.679046	16796.769275	28.868429
326.056241	16829.435914	28.873447
326.260176	16857.650903	28.878464
326.421177	16872.859358	28.883482
326.786071	16902.953817	28.888500
327.368730	16926.608617	28.893517
327.547515	16941.564813	28.898535
327.669928	16967.395372	28.903552
328.260569	16992.640929	28.908570
328.396766	17027.073400	28.913588
328.716593	17051.218045	28.918605
329.160905	17076.360290	28.923623
329.636149	17113.260369	28.928640
330.300435	17136.757345	28.933658
330.016305	17164.780754	28.938676
330.557730	17190.242747	28.943693
330.630501	17211.779370	28.948711
331.268326	17249.469166	28.953728
331.588125	17269.185691	28.958746
331.714764	17298.768486	28.963764
332.245736	17325.028271	28.968781
332.399254	17357.784538	28.973799
332.771779	17377.562405	28.978816
333.435160	17402.891864	28.983834
333.319219	17439.310296	28.988852
334.223360	17459.314520	28.993869
334.526199	17487.492825	28.998887
334.305708	17523.700368	29.003904
334.823602	17541.459350	29.008922
335.219124	17567.260563	29.013940
335.495645	17595.430513	29.018957
335.923149	17625.756350	29.023975
336.331607	17660.147299	29.028992
336.685860	17680.743281	29.034010
337.025157	17709.636382	29.039028
337.372105	17736.285644	29.044045
337.743557	17761.654986	29.049063
337.924038	17787.578621	29.054080
338.350645	17807.297916	29.059098
338.695880	17840.587220	29.064116
339.091047	17868.612633	29.069133
339.193331	17893.626310	29.074151
339.489761	17921.155551	29.079168
340.230724	17947.395923	29.084186
340.542282	17968.428488	29.089204
340.831148	17993.969007	29.094221
341.135098	18018.022583	29.099239
341.392780	18050.498368	29.104256
341.844201	18065.551711	29.109274
342.079142	18106.698796	29.114292
342.316902	18126.372187	29.119309
342.416361	18144.626860	29.124327
342.802259	18174.726324	29.129344
343.194208	18196.150866	29.134362
343.379359	18231.152706	29.139380
343.838737	18261.120759	29.144397
344.386573	18281.118473	29.149415
344.504835	18319.984683	29.154432
344.960853	18339.984205	29.159450
345.184375	18365.668118	29.164468
345.707813	18391.450391	29.169485
346.080357	18419.164262	29.174503
346.124278	18447.902566	29.179520
346.917423	18458.442427	29.184538
347.365707	18493.491968	29.189556
347.690038	18518.970764	29.194573
347.774228	18541.227286	29.199591
347.949698	18574.841372	29.204608
348.862315	18589.380641	29.209626
348.926505	18630.877784	29.214644
349.034263	18658.867228	29.219661
349.594803	18679.172930	29.224679
350.043452	18715.221014	29.229696
350.151875	18729.039783	29.234714
350.493006	18763.733849	29.239732
350.582499	18788.017820	29.244749
351.066454	18823.447751	29.249767
351.340461	18854.980974	29.254784
352.226250	18886.822756	29.259802
352.217285	18919.455480	29.264820
352.906997	18944.492212	29.269837
353.045221	18975.124499	29.274855
353.399261	19002.848417	29.279872
353.584668	19030.295533	29.284890
353.747266	19065.264496	29.289908
354.514608	19082.954228	29.294925
355.037320	19128.007051	29.299943
355.075197	19158.352086	29.304960
355.524536	19176.135940	29.309978
356.042616	19209.482644	29.314996
356.352715	19237.769754	29.320013
357.191233	19258.891754	29.325031
357.363516	19298.471692	29.330048
357.773812	19311.731836	29.335066
357.900449	19345.854015	29.340084
358.113853	19373.398315	29.345101
358.311923	19404.855870	29.350119
359.161532	19436.135602	29.355136
359.308831	19461.472774	29.360154
359.773869	19486.836024	29.365172
359.520043	19516.026890	29.370189
360.630906	19539.381012	29.375207
360.730187	19580.489276	29.380224
361.153549	19603.805852	29.385242
361.510156	19630.923729	29.390260
362.130292	19660.969843	29.395277
362.498700	19682.469208	29.400295
362.756028	19709.937602	29.405312
362.812030	19735.074616	29.410330
363.455399	19764.043178	29.415348
363.641298	19796.950109	29.420365
364.044264	19817.408043	29.425383
364.370551	19856.585901	29.430400
364.704764	19887.403732	29.435418
365.014788	19915.015794	29.440436
365.507680	19947.205169	29.445453
365.494644	19972.782934	29.450471
366.187066	20011.120300	29.455488
366.742438	20024.528794	29.460506
367.077077	20058.783905	29.465524
366.984407	20079.022795	29.470541
367.576970	20109.882644	29.475559
367.920213	20148.982612	29.480576
368.093030	20176.382762	29.485594
368.620539	20192.228245	29.490612
368.528924	20221.912844	29.495629
369.435753	20258.504872	29.500647
369.354585	20292.983479	29.505664
370.005548	20316.442163	29.510682
370.502179	20347.816556	29.515700
370.169028	20381.507097	29.520717
370.963813	20414.016409	29.525735
371.198052	20444.661226	29.530752
371.538889	20473.817230	29.535770
372.044496	20512.721896	29.540788
372.040245	20544.490976	29.545805
372.821221	20567.601043	29.550823
373.169410	20607.105521	29.555840
373.706255	20633.204573	29.560858
374.358624	20668.440869	29.565876
373.983539	20704.640603	29.570893
374.766685	20727.068133	29.575911
374.796129	20769.579869	29.580928
375.253894	20808.928583	29.585946
375.566461	20841.337222	29.590964
376.066888	20883.130949	29.595981
376.988188	20915.046297	29.600999
376.995748	20953.164221	29.606016
377.433936	20974.521384	29.611034
377.739410	21014.488300	29.616052
378.001364	21047.947755	29.621069
378.602445	21079.825070	29.626087
378.841649	21117.685880	29.631104
379.217018	21148.663523	29.636122
379.971617	21187.340965	29.641140
379.862632	21221.572811	29.646157
380.696957	21256.434140	29.651175
381.131142	21290.524158	29.656192
380.826731	21318.076471	29.661210
381.496227	21354.644532	29.666228
381.507808	21390.500617	29.671245
382.403084	21426.995535	29.676263
382.599282	21472.528232	29.681280
383.160742	21508.323673	29.686298
383.505238	21544.121570	29.691316
383.849537	21571.111361	29.696333
384.159729	21606.801010	29.701351
384.725438	21650.165803	29.706368
385.137809	21678.238209	29.711386
385.624763	21708.497878	29.716404
385.892569	21748.687015	29.721421
386.775319	21780.306507	29.726439
386.818377	21815.507604	29.731456
387.150211	21843.675003	29.736474
387.469286	21880.235740	29.741492
387.905944	21915.836631	29.746509
388.395130	21943.360286	29.751527
388.633384	21980.793221	29.756544
389.071237	22023.856602	29.761562
389.510712	22054.256932	29.766580
389.523020	22092.515320	29.771597
390.102869	22127.114745	29.776615
390.502035	22164.067865	29.781632
390.764887	22194.913121	29.786650
391.758550	22235.962653	29.791668
391.799131	22269.484125	29.796685
391.868906	22297.282491	29.801703
392.689241	22331.117932	29.806720
392.779523	22367.570071	29.811738
393.524465	22396.343352	29.816756
393.527725	22429.150583	29.821773
393.820381	22455.416674	29.826791
394.141486	22497.791651	29.831808
394.643918	22529.042224	29.836826
395.067437	22565.050753	29.841844
395.736881	22604.824851	29.846861
395.747920	22640.272546	29.851879
396.143133	22668.241620	29.856896
396.655665	22703.711980	29.861914
397.000887	22738.753640	29.866932
397.456931	22781.442994	29.871949
397.680994	22804.036292	29.876967
398.494652	22846.353817	29.881984
398.683103	22889.647713	29.887002
399.233649	22923.608573	29.892020
399.567187	22951.840470	29.897037
400.177300	22981.855305	29.902055
400.551693	23026.649596	29.907072
400.533140	23061.976295	29.912090
401.201750	23086.117977	29.917108
401.257892	23137.338373	29.922125
401.632169	23168.452048	29.927143
402.296245	23203.811094	29.932160
402.352228	23239.935286	29.937178
403.271563	23270.477167	29.942196
403.611615	23324.876363	29.947213
403.710628	23349.233968	29.952231
404.882071	23387.913609	29.957248
404.636996	23433.741092	29.962266
405.340028	23462.933235	29.967284
405.289699	23510.000559	29.972301
405.881202	23549.226339	29.977319
406.473233	23584.831161	29.982336
407.024517	23618.647746	29.987354
407.013290	23656.236658	29.992372
407.531816	23702.261114	29.997389
408.179287	23744.966782	30.002407
408.362570	23773.141226	30.007424
408.666312	23813.682790	30.012442
409.419941	23848.548681	30.017460
409.872638	23894.356394	30.022477
409.834092	23937.555412	30.027495
410.561292	23968.336999	30.032512
410.723414	24017.855768	30.037530
411.184988	24042.277497	30.042548
411.657217	24092.493570	30.047565
412.141350	24133.462526	30.052583
412.598954	24166.688045	30.057600
412.598393	24209.281348	30.062618
413.585287	24239.055794	30.067636
413.768366	24278.997889	30.072653
414.510509	24323.175048	30.077671
414.809155	24359.370683	30.082688
415.437326	24389.770301	30.087706
415.569245	24428.621107	30.092724
416.043967	24467.664756	30.097741
416.347726	24507.556806	30.102759
416.858734	24545.975605	30.107776
417.299423	24582.863508	30.112794
417.470352	24623.345358	30.117812
417.975095	24673.229173	30.122829
418.440588	24715.756869	30.127847
419.066340	24739.243704	30.132864
419.214734	24781.549463	30.137882
419.811739	24820.568325	30.142900
420.119532	24858.185355	30.147917
420.441810	24900.021748	30.152935
421.160154	24933.827028	30.157952
421.740741	24966.724943	30.162970
421.762286	24993.801524	30.167988
422.258361	25029.999042	30.173005
422.634562	25055.212707	30.178023
423.003280	25097.535178	30.183040
423.229744	25139.159565	30.188058
423.788140	25169.773528	30.193076
423.884127	25205.345171	30.198093
424.406962	25253.982593	30.203111
425.170298	25287.553908	30.208128
425.422358	25322.955957	30.213146
425.859433	25365.401000	30.218164
425.818472	25401.221955	30.223181
426.872436	25449.884094	30.228199
427.338671	25469.775480	30.233216
427.380257	25529.359149	30.238234
428.151966	25571.474136	30.243252
428.714855	25604.268427	30.248269
428.824969	25643.068112	30.253287
429.677257	25686.131348	30.258304
429.457423	25728.528372	30.263322
429.950640	25772.197871	30.268340
430.736379	25814.753567	30.273357
430.833614	25855.331595	30.278375
431.364277	25898.205501	30.283392
431.626405	25944.110934	30.288410
432.017157	25977.950320	30.293428
433.111312	26028.099091	30.298445
433.059417	26063.088683	30.303463
433.774293	26110.566797	30.308480
433.782538	26154.825013	30.313498
434.304186	26194.547231	30.318516
434.883005	26235.347633	30.323533
434.971377	26290.230363	30.328551
435.623865	26331.664075	30.333568
436.040165	26374.809711	30.338586
436.639669	26422.433031	30.343604
437.456898	26463.525200	30.348621
437.522759	26509.898751	30.353639
438.208049	26550.417663	30.358656
438.670495	26586.509477	30.363674
439.239364	26630.965330	30.368692
439.512271	26672.895292	30.373709
439.672207	26717.851485	30.378727
440.018763	26749.322660	30.383744
440.715309	26805.249174	30.388762
441.427329	26846.295396	30.393780
442.056225	26884.422091	30.398797
442.025072	26932.316039	30.403815
442.655971	26966.226907	30.408832
443.386682	27013.805784	30.413850
443.908886	27049.901702	30.418868
443.964923	27087.233653	30.423885
444.574166	27130.635092	30.428903
444.979380	27163.873755	30.433920
445.659306	27216.890297	30.438938
445.993427	27254.836322	30.443956
446.581084	27296.237917	30.448973
446.419751	27338.521688	30.453991
447.082811	27363.604814	30.459008
447.165078	27410.154821	30.464026
447.722446	27466.743324	30.469044
448.321776	27505.583712	30.474061
448.980279	27554.786897	30.479079
449.247697	27595.948516	30.484096
449.758714	27621.687831	30.489114
449.853583	27663.167357	30.494132
450.743815	27704.851060	30.499149
450.922666	27754.401640	30.504167
451.037640	27786.081348	30.509184
451.629917	27830.055791	30.514202
452.146603	27873.808305	30.519220
452.810959	27906.407130	30.524237
453.028197	27957.140470	30.529255
453.651044	27995.668396	30.534272
453.623553	28039.234711	30.539290
454.257415	28085.074111	30.544308
455.269811	28128.540945	30.549325
455.244085	28169.648504	30.554343
455.574660	28210.441188	30.559360
456.030582	28255.815825	30.564378
456.455293	28308.148292	30.569396
457.061729	28355.749769	30.574413
457.291507	28399.402969	30.579431
457.822175	28446.921713	30.584448
458.011231	28499.847812	30.589466
458.762348	28555.138498	30.594484
459.448569	28603.594009	30.599501
459.466469	28653.178295	30.604519
460.168238	28686.177041	30.609536
460.840158	28734.116789	30.614554
461.136309	28790.452790	30.619572
461.842198	28840.707242	30.624589
462.128941	28890.161499	30.629607
462.952240	28935.834073	30.634624
463.050327	28978.605235	30.639642
463.502788	29024.942905	30.644660
464.432578	29061.534787	30.649677
464.958768	29117.835655	30.654695
465.518101	29151.546451	30.659712
465.532836	29202.965657	30.664730
465.862817	29244.342026	30.669748
467.073060	29281.819570	30.674765
466.981702	29330.828423	30.679783
467.785078	29378.053767	30.684800
467.905809	29431.011929	30.689818
468.570292	29472.254190	30.694836
469.297142	29509.131503	30.699853
469.588519	29569.901502	30.704871
470.536342	29605.827810	30.709888
470.647770	29653.408691	30.714906
470.513408	29698.897937	30.719924
471.553499	29741.339823	30.724941
471.632542	29781.087777	30.729959
472.081154	29823.603512	30.734976
472.760940	29870.893593	30.739994
473.121434	29930.516005	30.745012
473.638912	29981.377991	30.750029
473.979290	30027.906149	30.755047
474.545823	30064.619928	30.760064
475.468205	30130.273933	30.765082
475.525552	30176.151409	30.770100
476.196708	30220.807646	30.775117
476.675436	30252.162363	30.780135
477.068901	30300.048233	30.785152
477.638516	30354.177444	30.790170
477.949226	30398.587095	30.795188
478.776039	30449.370176	30.800205
479.409151	30490.891210	30.805223
479.708377	30528.930933	30.810240
479.731470	30575.636447	30.815258
480.274573	30622.191083	30.820276
481.206163	30673.558844	30.825293
481.418811	30720.051670	30.830311
481.681146	30760.771594	30.835328
482.124477	30810.901295	30.840346
482.533610	30852.533994	30.845364
483.363934	30901.048199	30.850381
483.817251	30940.853546	30.855399
483.884236	30990.808729	30.860416
484.336870	31030.696535	30.865434
484.469480	31069.774804	30.870452
485.227545	31122.744939	30.875469
485.771032	31171.993762	30.880487
486.333131	31214.222748	30.885504
486.636683	31267.409839	30.890522
486.928474	31318.202989	30.895540
487.740376	31371.045213	30.900557
487.844428	31428.904094	30.905575
488.859943	31466.934495	30.910592
489.218883	31527.592186	30.915610
489.479680	31585.332125	30.920628
490.183680	31629.094884	30.925645
490.510195	31683.708164	30.930663
490.810846	31731.573943	30.935680
491.394576	31792.690298	30.940698
491.979138	31852.788885	30.945716
492.582204	31901.372631	30.950733
492.893280	31965.882787	30.955751
493.669445	32015.280497	30.960768
494.195335	32058.433544	30.965786
494.668167	32112.171571	30.970804
495.358481	32172.848778	30.975821
495.736350	32214.097137	30.980839
496.302944	32274.174464	30.985856
496.757671	32321.935279	30.990874
497.233172	32384.486445	30.995892
497.816513	32427.359409	31.000909
498.481072	32489.660008	31.005927
498.820900	32543.596994	31.010944
499.393357	32585.542645	31.015962
499.356153	32638.464175	31.020980
500.393883	32686.387392	31.025997
500.923491	32745.706893	31.031015
501.117278	32803.625068	31.036032
501.961370	32857.762056	31.041050
502.220038	32908.020555	31.046068
503.165190	32964.405327	31.051085
503.430654	33015.642958	31.056103
504.080153	33064.835389	31.061120
504.659107	33115.240208	31.066138
504.812868	33164.105894	31.071156
505.450600	33221.418298	31.076173
506.411189	33269.886004	31.081191
506.727801	33316.090148	31.086208
507.465997	33363.783650	31.091226
507.556180	33420.278267	31.096244
507.986027	33464.087809	31.101261
508.413856	33524.146196	31.106279
509.463739	33578.284425	31.111296
509.949859	33628.022199	31.116314
510.330792	33683.770200	31.121332
510.833422	33724.483553	31.126349
511.287094	33772.930657	31.131367
511.850563	33818.148876	31.136384
512.210850	33865.068143	31.141402
512.733668	33920.687067	31.146420
513.338134	33967.897087	31.151437
514.025324	34031.324119	31.156455
513.991194	34074.670187	31.161472
514.581861	34132.776438	31.166490
515.224227	34182.389888	31.171508
515.541305	34234.336849	31.176525
516.194395	34286.718149	31.181543
516.891705	34334.211609	31.186560
517.190121	34377.000405	31.191578
517.451098	34425.042928	31.196596
518.313520	34466.023815	31.201613
518.459990	34510.859923	31.206631
518.955441	34571.119348	31.211648
519.487255	34617.140893	31.216666
519.662892	34674.339944	31.221684
520.615572	34732.991802	31.226701
521.092708	34785.547319	31.231719
521.502043	34846.238315	31.236736
521.942352	34901.114013	31.241754
522.402499	34951.876938	31.246772
523.097611	35007.244116	31.251789
523.634295	35064.330766	31.256807
524.078029	35110.651706	31.261824
525.068664	35180.420714	31.266842
525.277611	35227.998992	31.271860
526.016396	35284.093505	31.276877
526.785664	35335.574002	31.281895
527.154413	35389.197591	31.286912
527.653261	35448.067937	31.291930
528.299698	35498.632274	31.296948
528.992079	35544.510549	31.301965
529.201332	35609.269109	31.306983
529.671510	35660.360952	31.312000
530.225143	35712.084794	31.317018
530.595917	35775.598222	31.322036
531.431056	35826.064231	31.327053
531.810887	35879.396460	31.332071
532.188491	35936.541983	31.337088
533.222719	35994.628128	31.342106
534.015941	36049.894134	31.347124
534.286592	36102.422017	31.352141
534.930835	36148.852923	31.357159
535.225896	36208.054475	31.362176
536.259202	36243.808082	31.367194
536.274609	36310.198892	31.372212
537.088632	36359.885398	31.377229
537.461809	36419.479985	31.382247
537.625100	36470.558603	31.387264
538.770155	36522.805136	31.392282
538.869496	36585.446616	31.397300
539.752129	36638.057019	31.402317
540.368446	36681.673275	31.407335
540.484610	36746.879849	31.412352
541.153123	36790.880199	31.417370
541.594746	36852.438150	31.422388
542.319681	36904.871561	31.427405
542.675567	36969.073792	31.432423
543.138543	37026.929724	31.437440
544.255084	37082.065559	31.442458
544.578276	37141.815424	31.447476
545.068462	37189.183292	31.452493
545.727199	37248.912520	31.457511
545.877596	37307.798302	31.462528
547.067174	37360.235937	31.467546
547.206774	37405.793762	31.472564
547.875686	37460.399946	31.477581
548.463053	37521.045372	31.482599
548.951843	37574.870644	31.487616
549.893712	37624.381975	31.492634
549.713494	37681.353931	31.497652
550.591210	37742.618484	31.502669
551.076186	37801.940135	31.507687
551.872706	37851.626521	31.512704
552.439572	37896.732725	31.517722
552.596837	37962.037727	31.522740
552.988245	37998.735852	31.527757
553.672723	38048.395975	31.532775
553.914510	38100.218693	31.537792
554.502357	38156.730130	31.542810
555.168129	38218.528807	31.547828
555.635840	38274.692591	31.552845
556.150294	38335.939842	31.557863
556.394757	38398.487987	31.562880
557.273958	38448.491638	31.567898
557.890624	38504.386062	31.572916
558.188775	38573.129979	31.577933
558.725659	38629.815056	31.582951
559.046895	38698.245886	31.587968
559.781720	38754.824403	31.592986
560.006807	38828.709259	31.598004
560.612425	38889.361998	31.603021
561.794647	38950.702447	31.608039
562.105812	39010.788219	31.613056
562.604004	39069.883619	31.618074
562.945401	39143.650148	31.623092
563.736327	39208.271535	31.628109
564.487719	39272.039235	31.633127
564.702557	39338.148849	31.638144
565.816962	39409.822106	31.643162
566.323861	39473.382050	31.648180
566.947653	39538.656683	31.653197
567.624054	39590.433871	31.658215
567.978209	39671.276911	31.663232
568.597469	39713.912274	31.668250
569.239368	39781.777716	31.673268
569.895602	39847.547808	31.678285
570.645577	39907.130962	31.683303
570.734870	39960.126695	31.688320
571.778738	40040.730276	31.693338
572.125468	40105.366981	31.698356
572.435953	40168.137557	31.703373
573.083135	40230.178879	31.708391
573.423818	40301.128791	31.713408
574.579285	40363.002344	31.718426
574.905013	40419.510133	31.723444
575.265125	40497.041323	31.728461
575.953375	40550.684638	31.733479
576.712908	40634.490832	31.738496
577.420121	40687.505393	31.743514
578.363114	40748.565838	31.748532
578.850326	40820.285047	31.753549
579.145430	40886.197046	31.758567
579.486338	40944.721335	31.763584
580.554999	41007.343956	31.768602
580.878534	41073.188819	31.773620
581.640705	41135.474008	31.778637
581.978977	41202.923399	31.783655
582.529418	41266.070643	31.788672
583.016178	41328.431137	31.793690
583.604515	41391.870067	31.798708
584.315320	41455.542986	31.803725
584.897306	41519.906684	31.808743
585.430455	41594.511618	31.813760
586.140463	41651.221712	31.818778
586.726625	41722.890425	31.823796
587.258432	41783.474222	31.828813
588.061779	41855.185249	31.833831
588.408743	41922.850530	31.838848
589.275955	41979.783518	31.843866
589.622451	42036.817180	31.848884
590.300276	42111.635228	31.853901
590.745145	42164.808293	31.858919
591.309906	42237.089220	31.863936
591.716238	42290.401446	31.868954
592.520232	42356.358325	31.873972
592.795822	42409.482592	31.878989
594.131388	42472.314262	31.884007
594.430899	42522.607791	31.889024
594.582714	42590.539707	31.894042
595.180970	42657.149556	31.899060
595.868315	42715.542071	31.904077
596.731203	42776.481547	31.909095
597.036544	42855.414814	31.914112
597.438269	42906.395292	31.919130
598.028377	42976.890991	31.924148
598.518162	43046.789087	31.929165
599.430614	43117.930516	31.934183
599.792508	43192.858629	31.939200
600.776974	43262.724208	31.944218
601.330898	43323.738880	31.949236
601.896063	43411.140851	31.954253
602.324171	43470.031372	31.959271
602.889552	43534.504744	31.964288
603.622984	43611.589928	31.969306
604.026831	43690.934534	31.974324
604.427428	43761.348548	31.979341
605.331122	43829.704154	31.984359
606.256634	43903.515358	31.989376
606.793518	43966.065203	31.994394
607.544683	44047.153097	31.999412
607.457841	44114.893009	32.004429
608.546820	44189.078061	32.009447
609.052999	44264.398339	32.014464
609.771659	44337.642456	32.019482
610.527092	44398.217356	32.024500
611.229212	44469.187307	32.029517
611.877052	44543.910717	32.034535
612.364886	44612.858877	32.039552
612.982672	44683.184855	32.044570
613.894418	44755.242516	32.049588
614.017553	44824.843054	32.054605
614.917027	44892.519410	32.059623
615.355773	44971.995941	32.064640
615.653187	45046.276181	32.069658
616.718113	45121.081689	32.074676
617.209458	45199.968823	32.079693
617.711343	45270.852486	32.084711
618.112455	45345.661493	32.089728
619.029106	45423.179691	32.094746
620.064275	45497.523006	32.099764
620.574945	45566.071993	32.104781
621.185671	45638.571840	32.109799
621.790719	45710.212489	32.114816
622.165274	45782.851002	32.119834
623.205358	45856.403996	32.124852
623.977443	45928.373432	32.129869
624.278464	45999.328805	32.134887
625.010646	46071.374532	32.139904
625.559074	46144.391844	32.144922
626.161568	46200.807745	32.149940
626.565571	46278.232047	32.154957
627.319074	46342.595478	32.159975
628.287636	46428.921226	32.164992
628.591614	46495.050885	32.170010
629.448217	46561.157452	32.175028
630.164897	46641.741379	32.180045
630.812929	46708.077151	32.185063
631.398576	46773.999033	32.190080
631.835405	46846.675499	32.195098
632.672459	46919.757660	32.200116
632.941447	46982.142767	32.205133
633.700007	47042.445948	32.210151
634.075263	47119.523360	32.215168
634.755608	47187.070121	32.220186
635.596815	47242.654122	32.225204
636.579971	47315.746311	32.230221
636.790400	47380.147133	32.235239
637.102980	47439.395123	32.240256
637.697071	47507.335928	32.245274
638.945283	47580.684800	32.250292
639.250747	47655.029295	32.255309
639.795485	47719.650759	32.260327
640.023528	47795.994345	32.265344
640.812689	47871.472151	32.270362
641.597011	47956.206660	32.275380
642.018797	48034.152943	32.280397
642.535081	48101.677502	32.285415
643.413083	48181.286318	32.290432
643.895004	48266.094643	32.295450
644.893562	48338.915663	32.300468
645.513855	48437.254586	32.305485
645.865424	48511.164437	32.310503
646.850798	48587.436351	32.315520
647.287065	48660.030120	32.320538
648.247814	48735.831883	32.325556
648.577228	48809.259008	32.330573
649.075564	48897.711314	32.335591
649.665098	48989.211852	32.340608
650.134939	49069.703839	32.345626
651.247423	49141.345437	32.350644
651.736486	49225.207169	32.355661
652.741820	49310.930711	32.360679
653.513313	49399.133384	32.365696
654.139317	49469.605791	32.370714
655.106459	49550.059543	32.375732
655.087482	49632.540797	32.380749
655.953743	49709.170427	32.385767
656.947252	49789.222285	32.390784
657.280815	49873.680166	32.395802
658.199056	49955.066741	32.400820
659.133204	50033.376146	32.405837
659.518111	50109.272623	32.410855
660.610353	50189.139577	32.415872
660.783132	50272.731972	32.420890
661.332330	50345.933438	32.425908
661.790281	50427.115367	32.430925
663.065208	50502.253687	32.435943
663.700614	50573.499918	32.440960
664.207909	50657.844875	32.445978
664.749911	50740.742084	32.450996
665.327554	50824.829869	32.456013
666.024484	50907.899559	32.461031
666.418276	50987.499013	32.466048
667.376599	51073.717347	32.471066
668.159763	51147.068199	32.476084
668.520561	51241.422852	32.481101
669.312878	51326.921488	32.486119
669.862447	51413.799878	32.491136
670.576026	51496.413490	32.496154
671.599678	51571.873040	32.501172
671.935177	51655.305726	32.506189
672.812212	51740.995099	32.511207
673.369033	51825.184677	32.516224
673.801038	51903.863783	32.521242
674.841165	51988.648989	32.526260
675.490306	52072.603536	32.531277
676.024550	52166.371610	32.536295
676.695776	52240.686262	32.541312
677.321641	52318.248042	32.546330
678.249027	52388.840320	32.551348
678.983415	52475.573495	32.556365
679.541391	52536.479331	32.561383
679.707787	52620.233022	32.566400
680.436027	52704.050893	32.571418
681.118810	52780.371367	32.576436
681.816249	52871.984230	32.581453
682.440452	52948.187867	32.586471
683.336840	53033.872621	32.591488
683.452815	53124.989037	32.596506
684.694100	53198.458102	32.601524
685.300875	53288.954088	32.606541
685.612634	53384.116062	32.611559
686.325548	53460.680820	32.616576
687.200224	53553.375988	32.621594
688.240246	53630.807640	32.626612
688.718049	53726.679050	32.631629
689.151820	53807.693003	32.636647
690.177219	53904.745005	32.641664
690.326960	53992.239789	32.646682
691.563405	54081.273327	32.651700
692.333213	54170.399261	32.656717
692.728333	54260.115781	32.661735
693.732931	54347.775436	32.666752
694.032666	54442.785353	32.671770
694.908715	54531.952967	32.676788
695.555219	54622.618708	32.681805
696.014914	54720.224616	32.686823
697.031390	54806.466557	32.691840
697.729357	54908.086086	32.696858
698.356992	54991.478526	32.701876
699.003614	55095.657256	32.706893
699.927101	55182.421402	32.711911
700.389556	55282.465652	32.716928
700.947399	55372.293791	32.721946
701.904631	55465.356901	32.726964
702.864136	55569.108992	32.731981
703.479636	55658.796283	32.736999
704.364345	55746.606449	32.742016
704.747016	55844.121441	32.747034
705.763711	55937.531488	32.752052
706.523034	56032.096056	32.757069
707.271984	56121.466737	32.762087
707.978072	56201.566515	32.767104
708.687398	56304.576216	32.772122
709.531426	56385.446105	32.777140
710.001083	56485.506924	32.782157
710.547732	56581.917014	32.787175
711.506102	56667.231788	32.792192
712.233029	56760.373981	32.797210
712.857278	56849.570710	32.802228
713.783239	56937.106641	32.807245
714.312176	57022.857008	32.812263
715.077335	57120.621085	32.817280
715.306339	57222.709964	32.822298
716.275982	57314.265684	32.827316
717.062572	57421.084487	32.832333
717.813308	57505.472733	32.837351
718.641609	57593.007357	32.842368
719.271090	57689.801319	32.847386
719.736452	57783.279571	32.852404
720.763453	57880.910790	32.857421
721.607269	57973.045684	32.862439
722.723968	58059.872270	32.867456
722.990036	58158.199731	32.872474
723.864387	58239.039453	32.877492
724.049940	58328.329337	32.882509
724.689194	58427.491882	32.887527
725.794429	58505.973473	32.892544
726.415140	58606.202984	32.897562
726.792450	58687.735988	32.902580
727.798705	58777.183825	32.907597
728.354752	58870.139384	32.912615
729.269000	58955.741322	32.917632
729.745507	59048.861927	32.922650
730.653986	59144.086267	32.927668
731.448168	59236.923651	32.932685
731.814334	59333.474247	32.937703
733.303045	59423.855311	32.942720
733.696834	59514.927202	32.947738
734.253800	59604.796567	32.952756
735.026243	59700.392513	32.957773
735.587902	59798.471430	32.962791
736.558117	59887.175753	32.967808
737.374119	59990.475603	32.972826
738.075762	60082.925591	32.977844
738.933411	60175.870540	32.982861
739.422574	60270.114189	32.987879
740.242905	60369.287921	32.992896
740.969371	60467.451315	32.997914
741.590977	60566.429088	33.002932
742.658224	60666.400899	33.007949
743.159844	60766.208495	33.012967
743.630178	60861.887928	33.017984
744.958451	60966.402977	33.023002
745.063276	61066.843627	33.028020
745.818255	61176.874170	33.033037
746.624191	61279.801213	33.038055
747.194157	61384.721637	33.043072
747.885609	61484.761948	33.048090
748.828260	61594.410475	33.053108
750.170125	61703.351295	33.058125
750.729692	61806.357093	33.063143
751.381435	61905.620378	33.068160
752.057201	62002.747003	33.073178
752.862454	62113.963930	33.078196
753.719132	62211.139004	33.083213
754.297391	62325.475286	33.088231
755.432551	62426.412127	33.093248
756.086364	62537.015297	33.098266
756.753787	62628.555940	33.103284
757.757466	62733.363510	33.108301
757.913258	62843.647212	33.113319
758.998762	62944.410347	33.118336
759.832864	63056.981698	33.123354
760.412740	63168.770397	33.128372
761.112964	63274.324120	33.133389
761.617932	63385.137946	33.138407
763.030503	63483.497055	33.143424
763.511062	63593.157119	33.148442
764.427994	63705.072691	33.153460
765.045885	63813.154863	33.158477
765.710873	63927.010093	33.163495
766.362242	64025.205647	33.168512
767.389846	64135.257224	33.173530
768.207230	64240.157258	33.178548
768.642634	64355.208921	33.183565
769.471173	64468.059709	33.188583
770.476146	64580.934021	33.193600
771.215686	64684.094434	33.198618
772.138445	64788.727015	33.203636
773.246957	64907.790920	33.208653
773.446752	65018.488797	33.213671
774.253844	65124.508382	33.218688
775.211744	65228.827063	33.223706
775.900528	65328.421002	33.228724
777.106815	65421.672817	33.233741
777.442410	65524.007226	33.238759
778.232743	65608.233344	33.243776
779.222175	65709.814006	33.248794
779.775067	65817.351466	33.253812
780.716856	65912.761134	33.258829
781.588883	66023.275823	33.263847
782.057377	66114.480427	33.268864
782.834704	66221.756525	33.273882
783.448965	66329.508135	33.278900
784.791854	66424.907566	33.283917
784.949422	66536.207486	33.288935
786.000233	66637.820232	33.293952
787.053028	66739.983907	33.298970
787.416367	66848.872343	33.303988
788.109307	66954.626189	33.309005
788.973616	67061.341355	33.314023
789.768288	67174.323445	33.319040
790.635458	67286.490569	33.324058
791.424292	67398.290554	33.329076
792.234988	67503.705315	33.334093
792.611078	67615.437915	33.339111
793.809076	67720.343369	33.344128
794.376087	67837.283341	33.349146
794.979044	67959.144315	33.354164
796.196671	68071.595571	33.359181
796.827964	68185.715752	33.364199
797.984003	68299.931559	33.369216
798.824226	68414.153002	33.374234
799.374792	68531.833195	33.379252
800.267676	68648.022975	33.384269
801.107968	68755.261814	33.389287
802.176465	68875.547211	33.394304
802.811163	68991.911936	33.399322
803.539131	69104.545678	33.404340
804.609561	69215.416628	33.409357
805.327317	69328.318886	33.414375
806.185996	69436.165542	33.419392
807.184175	69551.678013	33.424410
807.935564	69660.416234	33.429428
808.717582	69765.838379	33.434445
809.402566	69883.383340	33.439463
810.323409	69993.964422	33.444480
811.253753	70106.152883	33.449498
811.916434	70213.824485	33.454516
812.909845	70335.502501	33.459533
813.380552	70450.778602	33.464551
814.612631	70564.618853	33.469568
815.540982	70670.110387	33.474586
816.337454	70775.015084	33.479604
817.071577	70891.758996	33.484621
817.757770	70999.658116	33.489639
818.487334	71113.085503	33.494656
819.388132	71220.508649	33.499674
820.135209	71324.245422	33.504692
821.196064	71439.876736	33.509709
822.137584	71559.010185	33.514727
822.567434	71674.513362	33.519744
823.850487	71783.094815	33.524762
824.428518	71900.513575	33.529780
825.283758	72005.983919	33.534797
826.282620	72119.487458	33.539815
827.031195	72231.016851	33.544832
827.582243	72331.609222	33.549850
828.517368	72448.151231	33.554868
829.504376	72557.073531	33.559885
830.344960	72672.592742	33.564903
830.995045	72762.683982	33.569920
831.909197	72869.706434	33.574938
832.865347	72985.018919	33.579956
833.938447	73083.607173	33.584973
834.528937	73179.180855	33.589991
835.011254	73277.799007	33.595008
836.026448	73390.507460	33.600026
836.397327	73504.279910	33.605044
836.912406	73600.474885	33.610061
837.982373	73718.255297	33.615079
839.073456	73827.723814	33.620096
839.906804	73943.642323	33.625114
840.197803	74057.530963	33.630132
841.455430	74170.863399	33.635149
841.995600	74297.595859	33.640167
842.481250	74407.617543	33.645184
843.592330	74525.648398	33.650202
844.141662	74650.810424	33.655220
845.336685	74782.103975	33.660237
846.294361	74901.376511	33.665255
846.929405	75027.248873	33.670272
848.050967	75147.978862	33.675290
848.544910	75275.787186	33.680308
849.457003	75397.412447	33.685325
850.767564	75520.039898	33.690343
851.409923	75651.918238	33.695360
852.194321	75775.718614	33.700378
853.220992	75910.312158	33.705396
854.283058	76026.064466	33.710413
854.877765	76145.107971	33.715431
856.124415	76271.587055	33.720448
856.829716	76398.240167	33.725466
857.516681	76517.359527	33.730484
858.204303	76641.178998	33.735501
859.430718	76770.830479	33.740519
860.474301	76895.722793	33.745536
861.241080	77004.621572	33.750554
862.128301	77143.930137	33.755572
862.831966	77265.317692	33.760589
863.754762	77390.155169	33.765607
864.524939	77513.319595	33.770624
865.703329	77630.935367	33.775642
866.480936	77763.296790	33.780660
867.289101	77885.202788	33.785677
868.146017	78016.070828	33.790695
869.334984	78138.767096	33.795712
870.202862	78262.755690	33.800730
870.604219	78392.569364	33.805748
871.829718	78515.210913	33.810765
872.785976	78646.623805	33.815783
873.480379	78778.040317	33.820800
874.827735	78892.252494	33.825818
875.430803	79019.187073	33.830836
876.152231	79146.800482	33.835853
877.295713	79263.554534	33.840871
877.836049	79384.609594	33.845888
879.248806	79503.742253	33.850906
879.783980	79637.708890	33.855924
880.803536	79757.233597	33.860941
881.439554	79885.281848	33.865959
882.913777	80004.749093	33.870976
883.747225	80125.609446	33.875994
884.233790	80252.073788	33.881012
885.284778	80366.743845	33.886029
886.107855	80496.349274	33.891047
886.940016	80606.937024	33.896064
888.372983	80730.011955	33.901082
888.895606	80856.942153	33.906100
890.010532	80962.710603	33.911117
890.690071	81076.770238	33.916135
891.420623	81190.556283	33.921152
892.365054	81296.035941	33.926170
892.890609	81413.263151	33.931188
893.790217	81515.241110	33.936205
894.437904	81647.096533	33.941223
895.254641	81759.845117	33.946240
896.531071	81877.564841	33.951258
897.350827	82010.915422	33.956276
898.315102	82135.159510	33.961293
899.271970	82255.768957	33.966311
899.885799	82372.948312	33.971328
901.034905	82499.369678	33.976346
901.567963	82629.549802	33.981364
902.810672	82747.823247	33.986381
903.511567	82881.525959	33.991399
904.847067	83004.017879	33.996416
905.649800	83131.991413	34.001434
906.345089	83264.049621	34.006452
907.578803	83384.062994	34.011469
908.243648	83506.180593	34.016487
908.920102	83635.569938	34.021504
910.359060	83759.037220	34.026522
911.149026	83896.709386	34.031540
911.712563	84026.967129	34.036557
912.553691	84153.355345	34.041575
913.549459	84275.323034	34.046592
914.344301	84413.148963	34.051610
915.394084	84546.044547	34.056628
916.349711	84686.925714	34.061645
917.366079	84824.845638	34.066663
918.003248	84950.863804	34.071680
919.520940	85075.452162	34.076698
920.245440	85220.908497	34.081716
921.262920	85355.789618	34.086733
921.899194	85485.345617	34.091751
922.931321	85624.014506	34.096768
924.039192	85755.056483	34.101786
924.764622	85894.826439	34.106804
925.840185	86027.813489	34.111821
926.806520	86168.434068	34.116839
927.818641	86296.933749	34.121856
928.685922	86432.147506	34.126874
929.414315	86566.889423	34.131892
930.449356	86706.259969	34.136909
931.607371	86844.889608	34.141927
932.541510	86973.962051	34.146944
933.070377	87111.867765	34.151962
933.781073	87257.995378	34.156980
934.864253	87391.747776	34.161997
936.141623	87533.061207	34.167015
937.323572	87659.968880	34.172032
938.199438	87793.565475	34.177050
939.053154	87938.406808	34.182068
940.329282	88068.951226	34.187085
941.436773	88186.799147	34.192103
942.123559	88336.154730	34.197120
943.260758	88465.037160	34.202138
944.051829	88603.808563	34.207156
944.934398	88729.221599	34.212173
946.098860	88858.583044	34.217191
946.805765	88997.369462	34.222208
947.777091	89123.517978	34.227226
948.545369	89269.697196	34.232244
949.672929	89396.037847	34.237261
951.094780	89521.306413	34.242279
951.900147	89663.337564	34.247296
952.670316	89780.433515	34.252314
953.376507	89908.249061	34.257332
954.450706	90027.136033	34.262349
955.325632	90148.183844	34.267367
955.986174	90268.112407	34.272384
956.903153	90397.405197	34.277402
957.871945	90533.458229	34.282420
958.588079	90664.621312	34.287437
959.893735	90793.081841	34.292455
960.971433	90926.952362	34.297472
962.044890	91055.146188	34.302490
962.930603	91187.336932	34.307508
963.408770	91316.030639	34.312525
964.558292	91447.598205	34.317543
965.141647	91582.816443	34.322560
966.463274	91725.815765	34.327578
967.274819	91866.373432	34.332596
968.321717	92003.523508	34.337613
969.061479	92130.468662	34.342631
970.091330	92280.259080	34.347648
971.044289	92417.628520	34.352666
972.029993	92569.835438	34.357684
972.756106	92712.514367	34.362701
974.188643	92857.580280	34.367719
975.271050	93009.698195	34.372736
976.145093	93143.458251	34.377754
977.169859	93297.918794	34.382772
977.975327	93447.724701	34.387789
979.046060	93586.728686	34.392807
979.971774	93732.296359	34.397824
981.221477	93872.896026	34.402842
982.015763	94026.204838	34.407860
983.234950	94170.309000	34.412877
984.715635	94308.161970	34.417895
985.417020	94451.866851	34.422912
986.663591	94590.645011	34.427930
987.662842	94733.974999	34.432948
988.442426	94875.083788	34.437965
989.223740	95014.025412	34.442983
990.189563	95167.972136	34.448000
991.443900	95309.756426	34.453018
992.523296	95459.947461	34.458036
993.290682	95601.010738	34.463053
994.762757	95740.785457	34.468071
995.050940	95895.678471	34.473088
996.117033	96042.020879	34.478106
997.260606	96180.327864	34.483124
998.338474	96331.068382	34.488141
999.629083	96482.042514	34.493159
1000.475070	96631.781326	34.498176
1001.443118	96759.064615	34.503194
1002.547096	96922.074565	34.508212
1003.296925	97076.863073	34.513229
1004.252570	97213.518040	34.518247
1005.382309	97365.852614	34.523264
1006.128345	97517.081745	34.528282
1007.249065	97662.992102	34.533300
1008.025475	97820.505561	34.538317
1009.271346	97970.454295	34.543335
1010.279746	98118.945043	34.548352
1011.004056	98265.985082	34.553370
1011.989980	98425.509710	34.558388
1013.186137	98581.718857	34.563405
1014.602995	98723.138044	34.568423
1015.203842	98879.999644	34.573440
1016.505408	99036.371982	34.578458
1017.666308	99187.975084	34.583476
1018.162219	99337.350381	34.588493
1019.574349	99479.280729	34.593511
1020.448293	99616.694042	34.598528
1021.474812	99761.297561	34.603546
1022.316650	99889.906184	34.608564
1023.086643	100038.481153	34.613581
1024.418711	100180.363724	34.618599
1025.390221	100323.330264	34.623616
1026.139055	100470.858271	34.628634
1027.338772	100619.710919	34.633652
1028.224573	100773.443681	34.638669
1029.525783	100917.400799	34.643687
1030.216866	101070.480836	34.648704
1031.290020	101230.626858	34.653722
1032.495109	101380.407632	34.658740
1033.207405	101528.034880	34.663757
1034.410125	101684.727040	34.668775
1035.393480	101845.359219	34.673792
1036.126377	101995.204047	34.678810
1037.220211	102162.185026	34.683828
1038.257288	102325.397537	34.688845
1039.735626	102474.012120	34.693863
1040.555306	102647.973658	34.698880
1041.441817	102800.422564	34.703898
1042.586848	102963.900253	34.708916
1043.422420	103134.032865	34.713933
1044.668653	103296.646864	34.718951
1045.794173	103463.096921	34.723968
1046.507611	103631.755079	34.728986
1047.717068	103802.225613	34.734004
1048.819502	103973.208258	34.739021
1049.525591	104129.520591	34.744039
1050.785514	104304.372783	34.749056
1051.982762	104473.111581	34.754074
1053.120554	104643.470817	34.759092
1054.263754	104823.225550	34.764109
1055.059803	104983.572515	34.769127
1056.357672	105160.388537	34.774144
1057.532218	105336.793683	34.779162
1058.829609	105499.562495	34.784180
1059.680813	105670.390206	34.789197
1060.903596	105841.033801	34.794215
1062.221396	106005.145904	34.799232
1063.006682	106175.491954	34.804250
1064.166673	106338.983692	34.809268
1065.039932	106510.015039	34.814285
1066.547029	106679.768751	34.819303
1067.668981	106848.049296	34.824320
1068.429283	107018.137166	34.829338
1069.552166	107181.144202	34.834356
1070.670656	107355.958152	34.839373
1071.886020	107524.404909	34.844391
1073.176096	107692.561818	34.849408
1074.227180	107859.133848	34.854426
1075.659515	108019.560278	34.859444
1076.215262	108178.539602	34.864461
1077.722820	108345.410243	34.869479
1078.654778	108508.339299	34.874496
1079.287200	108682.880982	34.879514
1080.643728	108829.120424	34.884532
1081.362281	109010.193627	34.889549
1082.712984	109183.154360	34.894567
1083.697167	109346.979509	34.899584
1084.363855	109522.648638	34.904602
1085.994674	109682.087871	34.909620
1086.951832	109870.774956	34.914637
1088.130082	110034.598289	34.919655
1089.002661	110196.491935	34.924672
1090.150099	110363.086170	34.929690
1091.169818	110523.829625	34.934708
1092.014442	110685.362119	34.939725
1093.305035	110839.888656	34.944743
1094.494894	110994.761361	34.949760
1095.334069	111162.498240	34.954778
1096.641684	111319.560553	34.959796
1097.450363	111495.014328	34.964813
1098.661995	111652.816002	34.969831
1099.695190	111823.239548	34.974848
1100.642101	111998.192231	34.979866
1101.803388	112162.598714	34.984884
1102.517097	112326.036080	34.989901
1103.699968	112507.904145	34.994919
1104.872589	112684.930086	34.999936
1105.778111	112859.335412	35.004954
1107.165948	113035.771353	35.009972
1107.941871	113215.804325	35.014989
1108.940586	113397.274487	35.020007
1110.462013	113576.938884	35.025024
1111.277751	113760.760428	35.030042
1112.375362	113940.049072	35.035060
1113.462593	114134.521559	35.040077
1114.880319	114315.347282	35.045095
1115.738648	114505.583443	35.050112
1116.985970	114684.243511	35.055130
1118.127505	114864.303465	35.060148
1119.325240	115064.369497	35.065165
1120.463402	115247.336290	35.070183
1121.537681	115435.577547	35.075200
1122.092250	115632.043827	35.080218
1123.901785	115819.030423	35.085236
1125.236621	116016.644924	35.090253
1126.357925	116201.166444	35.095271
1127.236783	116388.720163	35.100288
1128.494853	116583.876386	35.105306
1129.566155	116773.875223	35.110324
1130.605670	116970.716562	35.115341
1131.751841	117162.747737	35.120359
1132.777621	117353.986969	35.125376
1134.173480	117555.214952	35.130394
1135.455824	117739.325621	35.135412
1136.507703	117926.986766	35.140429
1137.666191	118133.582317	35.145447
1138.669511	118323.383968	35.150464
1140.026256	118527.705512	35.155482
1141.283517	118705.749009	35.160500
1142.306320	118902.628377	35.165517
1143.598921	119100.303697	35.170535
1144.676638	119279.811324	35.175552
1145.809721	119487.458314	35.180570
1147.374941	119669.593269	35.185588
1148.298330	119873.203381	35.190605
1149.268188	120061.268383	35.195623
1150.601596	120258.258282	35.200640
1151.933181	120447.308691	35.205658
1153.321723	120637.251740	35.210676
1154.340571	120826.276843	35.215693
1155.339442	121020.443470	35.220711
1156.619913	121218.499389	35.225728
1157.379619	121403.051924	35.230746
1158.711522	121589.418547	35.235764
1159.736482	121783.052090	35.240781
1161.426831	121975.719808	35.245799
1162.578210	122167.204296	35.250816
1163.558313	122362.458768	35.255834
1164.746666	122544.945232	35.260852
1165.787012	122734.965633	35.265869
1166.966222	122918.140274	35.270887
1168.382986	123095.734874	35.275904
1169.449870	123275.287919	35.280922
1170.478959	123442.732641	35.285940
1171.510753	123623.269560	35.290957
1172.482905	123810.020097	35.295975
1173.993479	123986.259251	35.300992
1175.063672	124169.583556	35.306010
1176.412823	124359.132009	35.311028
1177.612956	124530.702881	35.316045
1178.104262	124712.623301	35.321063
1179.063705	124908.959088	35.326080
1180.669383	125099.346212	35.331098
1181.912935	125284.323041	35.336116
1182.788688	125477.376189	35.341133
1183.942631	125671.756854	35.346151
1185.317460	125876.735296	35.351168
1186.070105	126075.240436	35.356186
1187.177372	126269.707367	35.361204
1188.492638	126471.742084	35.366221
1189.792866	126675.492880	35.371239
1190.763589	126884.231502	35.376256
1191.871107	127085.997259	35.381274
1193.590835	127291.905654	35.386292
1194.657836	127494.326782	35.391309
1195.543977	127700.278885	35.396327
1197.192122	127905.795531	35.401344
1197.955174	128126.169086	35.406362
1199.333362	128333.252577	35.411380
1200.488627	128537.682240	35.416397
1201.939586	128751.493456	35.421415
1202.955130	128953.726689	35.426432
1204.294753	129171.363745	35.431450
1205.441726	129379.973030	35.436468
1206.577067	129593.368463	35.441485
1207.653953	129804.997816	35.446503
1209.118666	130024.535526	35.451520
1210.327740	130241.893985	35.456538
1211.481675	130455.582641	35.461556
1212.854957	130673.983380	35.466573
1213.809762	130883.429438	35.471591
1215.338977	131097.925331	35.476608
1216.675553	131315.396135	35.481626
1218.075889	131529.229173	35.486644
1219.373754	131744.170512	35.491661
1220.537177	131957.928551	35.496679
1222.003201	132161.299090	35.501696
1222.918493	132380.630253	35.506714
1224.431051	132584.731415	35.511732
1225.469442	132798.741529	35.516749
1226.382879	133018.380694	35.521767
1228.252777	133224.827070	35.526784
1229.431611	133445.302344	35.531802
1230.758065	133648.397069	35.536820
1231.905482	133857.763759	35.541837
1232.734783	134077.573610	35.546855
1234.328886	134284.347245	35.551872
1235.466020	134510.024185	35.556890
1237.029655	134709.825478	35.561908
1238.108505	134925.222618	35.566925
1239.230126	135126.922223	35.571943
1240.684477	135346.208995	35.576960
1241.841177	135565.530735	35.581978
1243.212978	135771.889175	35.586996
1244.497881	135979.581876	35.592013
1245.315581	136187.881628	35.597031
1246.774627	136392.719145	35.602048
1248.252522	136611.500735	35.607066
1249.702411	136816.633445	35.612084
1250.728026	137011.770373	35.617101
1251.946442	137207.588584	35.622119
1253.432183	137393.987842	35.627136
1254.298192	137598.669756	35.632154
1255.639558	137790.816439	35.637172
1257.192650	137984.529737	35.642189
1258.116488	138193.177242	35.647207
1259.400942	138377.898768	35.652224
1260.025382	138588.295401	35.657242
1261.482307	138796.329147	35.662260
1262.823293	138998.810845	35.667277
1263.866613	139206.873076	35.672295
1265.072952	139414.555367	35.677312
1266.280683	139618.608828	35.682330
1267.704266	139839.228797	35.687348
1268.911751	140042.091187	35.692365
1269.782708	140274.462471	35.697383
1271.101187	140485.088829	35.702400
1272.234001	140707.852312	35.707418
1273.759865	140929.641547	35.712436
1274.979179	141152.380851	35.717453
1276.309996	141387.883661	35.722471
1277.760028	141600.080677	35.727488
1278.572855	141838.243058	35.732506
1280.306292	142067.467434	35.737524
1281.336852	142286.637152	35.742541
1282.427724	142530.178573	35.747559
1283.656419	142755.791979	35.752576
1285.108711	142988.973630	35.757594
1286.512314	143226.199923	35.762612
1287.562952	143463.799891	35.767629
1288.862668	143698.887123	35.772647
1290.005607	143940.790092	35.777664
1291.415191	144180.761408	35.782682
1292.914335	144415.884246	35.787700
1294.373178	144659.784618	35.792717
1295.754192	144893.290913	35.797735
1297.126408	145127.205807	35.802752
1298.360643	145370.776690	35.807770
1299.622208	145606.602232	35.812788
1300.918825	145839.034549	35.817805
1302.505386	146090.524431	35.822823
1303.916203	146328.665311	35.827840
1305.254279	146557.413602	35.832858
1306.539561	146800.983276	35.837876
1307.894753	147030.822529	35.842893
1308.972351	147270.276455	35.847911
1310.286036	147500.555823	35.852928
1311.588681	147743.467162	35.857946
1312.915237	147982.466513	35.862964
1314.476869	148219.919706	35.867981
1315.986797	148467.866368	35.872999
1317.256959	148708.274043	35.878016
1318.278592	148936.282583	35.883034
1320.056526	149170.672545	35.888052
1321.657730	149416.464210	35.893069
1322.587442	149647.206488	35.898087
1323.842815	149875.118965	35.903104
1325.443592	150115.379650	35.908122
1326.615736	150357.028599	35.913140
1327.801183	150586.287810	35.918157
1329.448131	150827.229854	35.923175
1330.513042	151058.337766	35.928192
1332.036875	151306.295294	35.933210
1333.302381	151535.596717	35.938228
1335.096967	151766.250654	35.943245
1335.891713	152010.161952	35.948263
1337.528303	152233.670624	35.953280
1338.783248	152448.455824	35.958298
1339.861976	152669.692518	35.963316
1341.505871	152885.979855	35.968333
1342.301395	153119.791526	35.973351
1343.806182	153331.164401	35.978368
1345.152598	153550.737818	35.983386
1346.404701	153780.355182	35.988404
1347.665407	154006.557399	35.993421
1349.028502	154231.563923	35.998439
1350.457978	154461.549777	36.003456
1351.941847	154688.646432	36.008474
1353.427614	154924.883613	36.013492
1354.664130	155153.087134	36.018509
1355.768579	155394.095535	36.023527
1357.276037	155626.612699	36.028544
1358.469555	155854.787613	36.033562
1359.781717	156099.625549	36.038580
1361.196571	156326.752080	36.043597
1362.406049	156576.432034	36.048615
1363.517717	156813.865214	36.053632
1364.803021	157056.972129	36.058650
1366.276921	157317.594810	36.063668
1367.629693	157560.959804	36.068685
1368.695998	157813.003198	36.073703
1370.240649	158060.884972	36.078720
1371.587622	158321.074837	36.083738
1372.723292	158586.808574	36.088756
1374.574132	158830.151478	36.093773
1375.542606	159095.012233	36.098791
1377.211797	159352.198053	36.103808
1378.678433	159619.382490	36.108826
1380.052608	159879.968250	36.113844
1381.420333	160128.508129	36.118861
1382.562440	160390.541537	36.123879
1384.618262	160655.441863	36.128896
1385.886177	160915.566126	36.133914
1387.202975	161175.658415	36.138932
1388.905668	161432.784048	36.143949
1390.257076	161690.854405	36.148967
1391.432796	161955.517033	36.153984
1392.974890	162206.767357	36.159002
1394.156707	162475.201833	36.164020
1396.072074	162729.417384	36.169037
1397.511570	163001.266999	36.174055
1399.030919	163269.271031	36.179072
1400.404673	163534.467711	36.184090
1401.665596	163785.996649	36.189108
1403.451834	164034.308351	36.194125
1404.504621	164304.801887	36.199143
1405.889258	164568.553615	36.204160
1407.595607	164818.734398	36.209178
1408.826047	165077.090909	36.214196
1410.284180	165333.406726	36.219213
1411.498739	165596.871677	36.224231
1413.018720	165855.249305	36.229248
1414.798195	166116.025037	36.234266
1415.815718	166368.934827	36.239284
1417.694938	166626.598893	36.244301
1419.049915	166883.152476	36.249319
1420.321105	167144.557594	36.254336
1421.882942	167390.847048	36.259354
1422.733463	167657.093925	36.264372
1424.496302	167915.606241	36.269389
1426.028153	168177.164835	36.274407
1427.573666	168440.702984	36.279424
1429.358467	168685.095562	36.284442
1430.476359	168951.000682	36.289460
1432.053261	169195.757654	36.294477
1433.259791	169442.008205	36.299495
1434.522749	169684.784407	36.304512
1436.286241	169913.808098	36.309530
1437.275398	170157.403251	36.314548
1438.787730	170392.346598	36.319565
1440.377112	170640.712480	36.324583
1441.654022	170891.426334	36.329600
1443.139725	171135.784998	36.334618
1444.354292	171390.230638	36.339636
1445.649105	171633.617686	36.344653
1447.191730	171885.626496	36.349671
1448.566674	172139.313079	36.354688
1450.013588	172387.732389	36.359706
1451.419517	172653.986539	36.364724
1452.400544	172912.727532	36.369741
1453.799412	173179.365520	36.374759
1455.337498	173450.503067	36.379776
1456.780868	173709.999691	36.384794
1458.394159	173987.527059	36.389812
1459.825553	174252.081117	36.394829
1461.190729	174523.350979	36.399847
1462.834452	174801.244653	36.404864
1464.458841	175064.869615	36.409882
1465.482950	175339.230451	36.414900
1467.086495	175607.990493	36.419917
1468.821631	175887.486237	36.424935
1470.075969	176168.696261	36.429952
1472.168325	176438.360268	36.434970
1473.429052	176719.761627	36.439988
1475.227000	176992.622696	36.445005
1476.429318	177270.301701	36.450023
1477.527769	177548.582001	36.455040
1479.269315	177818.051351	36.460058
1480.809498	178106.981895	36.465076
1482.189980	178382.858816	36.470093
1484.056034	178663.105144	36.475111
1485.802474	178948.755344	36.480128
1487.355399	179213.179056	36.485146
1488.175235	179496.258524	36.490164
1490.004797	179780.272951	36.495181
1491.756934	180054.649258	36.500199
1493.219092	180337.478461	36.505216
1495.283980	180609.648689	36.510234
1495.956554	180891.434891	36.515252
1497.623563	181156.151219	36.520269
1499.143834	181446.898939	36.525287
1500.529713	181726.061627	36.530304
1502.510103	182009.322811	36.535322
1503.914973	182289.322343	36.540340
1505.386411	182576.627026	36.545357
1506.768514	182844.059535	36.550375
1508.214050	183133.681205	36.555392
1509.822187	183415.582503	36.560410
1511.422439	183691.745743	36.565428
1513.099132	183977.015959	36.570445
1514.501433	184271.803719	36.575463
1516.071268	184611.039677	36.580480
1517.857287	184885.805623	36.585498
1519.255524	185177.167814	36.590516
1520.856191	185441.906239	36.595533
1522.385868	185725.883670	36.600551
1523.786939	186009.501022	36.605568
1525.414130	186283.736793	36.610586
1527.049391	186560.384965	36.615604
1528.343465	186834.064723	36.620621
1529.902340	187105.443182	36.625639
1531.337378	187388.881133	36.630656
1533.049564	187660.846593	36.635674
1534.674410	187931.759615	36.640692
1536.126636	188189.517823	36.645709
1537.912475	188451.694799	36.650727
1539.084271	188713.765300	36.655744
1540.528299	188969.469211	36.660762
1542.164445	189235.583056	36.665780
1543.482079	189493.822543	36.670797
1545.118873	189759.988315	36.675815
1546.443308	190029.658022	36.680832
1548.307192	190296.653099	36.685850
1549.929518	190565.134414	36.690868
1551.188514	190842.106139	36.695885
1552.369846	191109.413091	36.700903
1554.228903	191396.528578	36.705920
1555.953894	191666.164733	36.710938
1557.147000	191938.856606	36.715956
1558.570393	192226.651856	36.720973
1560.343479	192498.847789	36.725991
1561.638940	192793.954393	36.731008
1563.398912	193068.744501	36.736026
1565.016187	193353.209888	36.741044
1566.489104	193644.632967	36.746061
1568.177837	193939.198058	36.751079
1569.847015	194225.511521	36.756096
1571.551211	194502.574111	36.761114
1573.351991	194798.927074	36.766132
1574.572853	195088.309906	36.771149
1576.240744	195365.684779	36.776167
1577.863299	195669.129108	36.781184
1579.717936	195950.971980	36.786202
1581.139008	196245.075983	36.791220
1582.646529	196541.681822	36.796237
1584.337949	196826.447768	36.801255
1585.850404	197133.494110	36.806272
1587.422125	197419.854862	36.811290
1589.040461	197722.034154	36.816308
1590.657081	198019.921431	36.821325
1592.375624	198318.682412	36.826343
1593.645332	198619.673388	36.831360
1595.639734	198909.323886	36.836378
1596.891662	199217.482157	36.841396
1598.327596	199517.051754	36.846413
1600.187814	199817.038154	36.851431
1601.875669	200131.251877	36.856448
1603.505579	200427.795367	36.861466
1605.174612	200733.605078	36.866484
1606.855832	201024.984960	36.871501
1608.668750	201330.112785	36.876519
1610.100538	201638.603110	36.881536
1611.920615	201929.048322	36.886554
1613.319640	202231.575265	36.891572
1614.784014	202546.514311	36.896589
1616.808534	202844.930811	36.901607
1618.102852	203156.976244	36.906624
1619.701213	203458.737371	36.911642
1621.488003	203755.617589	36.916660
1623.009099	204058.966733	36.921677
1624.951720	204365.349520	36.926695
1626.255584	204674.373031	36.931712
1628.425706	204978.384115	36.936730
1629.814499	205276.218032	36.941748
1631.030050	205582.640267	36.946765
1633.435313	205880.265175	36.951783
1634.614888	206196.194632	36.956800
1636.475094	206494.820211	36.961818
1637.970533	206797.161322	36.966836
1639.099359	207103.015039	36.971853
1641.241830	207396.263020	36.976871
1642.413824	207701.602728	36.981888
1644.173319	207983.276761	36.986906
1645.765402	208269.626114	36.991924
1647.449832	208551.490391	36.996941
1648.820539	208840.542402	37.001959
1650.478730	209147.357458	37.006976
1652.252717	209432.968404	37.011994
1653.854858	209739.869154	37.017012
1655.368145	210030.957871	37.022029
1657.375662	210333.705926	37.027047
1658.690863	210632.625132	37.032064
1660.434958	210931.198100	37.037082
1662.115806	211233.871239	37.042100
1663.808027	211542.284105	37.047117
1665.626385	211846.765408	37.052135
1666.953439	212148.402495	37.057152
1668.468625	212455.751641	37.062170
1670.494135	212768.940260	37.067188
1671.790689	213088.111495	37.072205
1673.238802	213391.305825	37.077223
1675.009509	213716.703553	37.082240
1676.624785	214032.675732	37.087258
1678.105446	214358.805335	37.092276
1680.195957	214684.915996	37.097293
1681.934472	214996.373241	37.102311
1683.856600	215329.090364	37.107328
1685.753793	215644.892729	37.112346
1687.310126	215972.027967	37.117364
1688.868813	216292.329448	37.122381
1690.725472	216615.150314	37.127399
1692.743930	216944.678107	37.132416
1694.209798	217260.574499	37.137434
1695.884068	217582.662430	37.142452
1697.581763	217922.605846	37.147469
1699.412036	218242.332595	37.152487
1700.822745	218568.196722	37.157504
1702.311385	218898.621542	37.162522
1704.401119	219237.208757	37.167540
1705.999636	219568.277222	37.172557
1708.154266	219886.683834	37.177575
1709.836936	220228.891782	37.182592
1711.973364	220559.215996	37.187610
1713.454749	220882.783759	37.192628
1714.803307	221213.307723	37.197645
1717.033843	221545.700693	37.202663
1718.681726	221877.448227	37.207680
1720.068076	222204.486221	37.212698
1722.159567	222527.908187	37.217716
1723.713291	222864.802324	37.222733
1725.676736	223192.131287	37.227751
1727.197543	223523.340186	37.232768
1729.352059	223862.757096	37.237786
1731.270960	224183.996191	37.242804
1733.117303	224518.431388	37.247821
1734.864231	224832.228642	37.252839
1736.679885	225154.373096	37.257856
1738.390520	225483.037434	37.262874
1739.822689	225801.990175	37.267892
1741.574075	226131.588069	37.272909
1743.664008	226452.597189	37.277927
1745.259499	226786.131654	37.282944
1747.327460	227114.079457	37.287962
1749.057128	227423.865431	37.292980
1750.763031	227746.280896	37.297997
1752.398518	228068.529489	37.303015
1754.351057	228394.157944	37.308032
1755.777851	228716.362832	37.313050
1757.797549	229027.220859	37.318068
1759.272108	229333.743803	37.323085
1760.989842	229624.071638	37.328103
1762.801565	229930.033551	37.333120
1764.337993	230232.380261	37.338138
1766.413449	230537.589374	37.343156
1767.724867	230839.285157	37.348173
1769.608492	231149.960496	37.353191
1771.331628	231462.464491	37.358208
1772.705514	231770.856743	37.363226
1774.777868	232080.739992	37.368244
1776.459606	232414.030418	37.373261
1778.103931	232725.555350	37.378279
1779.590367	233047.063142	37.383296
1781.212987	233381.784849	37.388314
1783.232061	233694.038085	37.393332
1784.621972	234036.137482	37.398349
1786.394515	234369.183797	37.403367
1788.577445	234698.939362	37.408384
1789.845605	235037.881572	37.413402
1792.003133	235376.252473	37.418420
1793.432812	235710.138908	37.423437
1795.275101	236054.426828	37.428455
1797.130361	236403.437493	37.433472
1798.971356	236749.960499	37.438490
1801.123934	237085.510839	37.443508
1802.834070	237450.522086	37.448525
1804.437860	237791.416158	37.453543
1806.516440	238143.514763	37.458560
1808.514858	238496.362225	37.463578
1810.175603	238836.484156	37.468596
1811.457093	239190.078090	37.473613
1813.689917	239541.465052	37.478631
1815.388885	239907.491282	37.483648
1817.150804	240265.860762	37.488666
1819.188140	240617.912044	37.493684
1821.090257	240969.501358	37.498701
1823.082415	241336.927757	37.503719
1824.873374	241695.189133	37.508736
1827.174300	242053.954467	37.513754
1829.380991	242400.616704	37.518772
1830.995343	242753.239251	37.523789
1832.696735	243107.422638	37.528807
1834.683422	243461.891075	37.533824
1836.298662	243816.721912	37.538842
1838.262867	244162.301694	37.543860
1840.265970	244535.411619	37.548877
1842.433875	244879.713625	37.553895
1844.647065	245229.291768	37.558912
1846.059185	245581.484140	37.563930
1848.136843	245926.484382	37.568948
1849.600092	246280.902961	37.573965
1852.006098	246627.781196	37.578983
1853.703600	246980.231232	37.584000
1855.116928	247327.568351	37.589018
1857.343083	247687.783724	37.594036
1859.269291	248040.780211	37.599053
1861.361743	248381.099582	37.604071
1862.546220	248741.780666	37.609088
1864.787898	249084.082110	37.614106
1866.760671	249443.800103	37.619124
1868.513741	249795.880238	37.624141
1870.262184	250147.325299	37.629159
1872.306326	250495.624281	37.634176
1874.079267	250849.934432	37.639194
1876.003951	251195.989806	37.644212
1877.802157	251545.163248	37.649229
1879.968446	251890.163204	37.654247
1882.039563	252238.250897	37.659264
1883.511772	252571.012630	37.664282
1885.387526	252899.036563	37.669300
1887.330177	253225.804619	37.674317
1889.066643	253556.693865	37.679335
1891.156144	253877.290289	37.684352
1892.914648	254214.245540	37.689370
1895.000219	254544.950861	37.694388
1896.756058	254878.247128	37.699405
1898.660660	255203.670311	37.704423
1900.824466	255538.171204	37.709440
1902.492264	255885.805084	37.714458
1904.729085	256208.608340	37.719476
1905.800925	256549.577036	37.724493
1907.511104	256885.923585	37.729511
1909.517720	257242.797613	37.734528
1911.271419	257593.614017	37.739546
1913.372556	257942.825635	37.744564
1915.270948	258301.313855	37.749581
1916.820906	258661.735202	37.754599
1918.797883	259007.737361	37.759616
1920.436271	259376.550334	37.764634
1922.944415	259739.053785	37.769652
1924.477530	260109.989192	37.774669
1926.584018	260478.166686	37.779687
1928.708677	260840.269530	37.784704
1930.168388	261218.248721	37.789722
1931.987720	261579.812793	37.794740
1933.974669	261967.511377	37.799757
1935.786205	262346.473121	37.804775
1937.704883	262727.474175	37.809792
1940.039799	263108.815163	37.814810
1942.239760	263482.962447	37.819828
1943.865487	263879.270399	37.824845
1945.921010	264265.222876	37.829863
1947.665039	264644.745855	37.834880
1950.010198	265037.812744	37.839898
1951.715448	265421.148811	37.844916
1953.538973	265808.020784	37.849933
1955.803315	266204.423074	37.854951
1957.918772	266586.928553	37.859968
1959.290723	266984.203924	37.864986
1961.423978	267375.669283	37.870004
1963.736584	267774.191173	37.875021
1965.780587	268172.423258	37.880039
1967.505127	268554.194791	37.885056
1969.857071	268963.576001	37.890074
1971.708214	269351.724815	37.895092
1973.749494	269749.112501	37.900109
1975.505310	270137.577698	37.905127
1977.932262	270530.584010	37.910144
1979.452378	270944.480341	37.915162
1981.549472	271336.214062	37.920180
1983.602849	271730.797397	37.925197
1985.786479	272133.942855	37.930215
1987.673414	272524.688269	37.935232
1989.644927	272926.821947	37.940250
1991.659967	273325.721520	37.945268
1993.773242	273720.362585	37.950285
1995.565257	274120.182194	37.955303
1997.506099	274524.243224	37.960320
1999.280816	274927.642573	37.965338
2001.294804	275331.027902	37.970356
2003.445090	275730.910634	37.975373
2005.212874	276150.025249	37.980391
2007.457566	276539.121276	37.985408
2009.265395	276954.238249	37.990426
2011.324906	277359.663313	37.995444
2013.609135	277755.350030	38.000461
2015.889393	278146.514975	38.005479
2017.758476	278527.838115	38.010496
2019.219311	278923.241350	38.015514
2021.252400	279300.979649	38.020532
2023.584732	279690.554044	38.025549
2025.063379	280076.780901	38.030567
2027.482787	280466.363021	38.035584
2029.245679	280855.588706	38.040602
2031.325250	281247.276820	38.045620
2033.305002	281643.422433	38.050637
2035.082062	282042.873427	38.055655
2037.276304	282433.851538	38.060672
2039.075452	282840.608078	38.065690
2041.147499	283242.824912	38.070708
2042.772603	283648.308957	38.075725
2044.676216	284069.567125	38.080743
2047.108540	284484.391720	38.085760
2048.562983	284906.045181	38.090778
2050.463898	285334.558445	38.095796
2052.772858	285760.415108	38.100813
2054.687648	286194.532546	38.105831
2057.032547	286616.873987	38.110848
2058.626681	287055.225739	38.115866
2060.865379	287494.819515	38.120884
2063.173090	287933.383870	38.125901
2064.952238	288383.708153	38.130919
2067.230563	288818.081494	38.135936
2069.217398	289262.654044	38.140954
2071.361741	289713.241952	38.145972
2073.834009	290160.804600	38.150989
2075.979647	290617.987500	38.156007
2077.944527	291056.126972	38.161024
2079.916867	291499.264100	38.166042
2082.006414	291951.697929	38.171060
2084.312177	292404.221535	38.176077
2086.342167	292855.769321	38.181095
2088.786588	293308.899220	38.186112
2090.818905	293754.168643	38.191130
2092.937954	294216.990571	38.196148
2095.205677	294662.495634	38.201165
2097.231076	295116.134297	38.206183
2099.549633	295565.940652	38.211200
2101.256461	296028.152659	38.216218
2103.465066	296483.224505	38.221236
2105.462847	296930.074580	38.226253
2108.186299	297388.257565	38.231271
2110.461724	297844.679016	38.236288
2112.514798	298305.548973	38.241306
2114.534382	298744.866551	38.246324
2116.722843	299200.376585	38.251341
2118.849644	299666.478833	38.256359
2121.059156	300115.428179	38.261376
2123.168830	300581.322211	38.266394
2125.447172	301039.214569	38.271412
2127.587404	301479.100561	38.276429
2129.531255	301938.433808	38.281447
2131.999879	302391.029963	38.286464
2134.171589	302841.155543	38.291482
2136.167585	303299.631090	38.296500
2138.431766	303734.757285	38.301517
2140.372162	304190.872890	38.306535
2142.421333	304648.160521	38.311552
2144.598181	305101.667235	38.316570
2146.473550	305552.704067	38.321588
2148.351758	306012.366947	38.326605
2151.075418	306477.071625	38.331623
2153.518172	306924.529886	38.336640
2155.539195	307375.756051	38.341658
2157.470917	307804.223626	38.346676
2159.739976	308232.304734	38.351693
2161.667643	308661.628497	38.356711
2163.921086	309076.099676	38.361728
2165.839420	309519.859839	38.366746
2167.905124	309944.683445	38.371764
2170.629653	310385.339852	38.376781
2172.665788	310818.409358	38.381799
2174.831727	311258.612089	38.386816
2176.870309	311695.531144	38.391834
2178.743274	312145.162371	38.396852
2181.178523	312572.518872	38.401869
2182.865402	313025.698625	38.406887
2185.375602	313467.958698	38.411904
2187.253744	313919.526232	38.416922
2189.509777	314364.482327	38.421940
2191.706562	314820.356397	38.426957
2193.847306	315279.863848	38.431975
2195.956279	315741.579547	38.436992
2198.083312	316204.404336	38.442010
2199.878111	316676.818488	38.447028
2202.303768	317142.530704	38.452045
2204.118184	317625.082846	38.457063
2206.676736	318103.097649	38.462080
2208.761339	318577.552478	38.467098
2211.124305	319063.403510	38.472116
2213.515577	319539.830018	38.477133
2215.336823	320029.713688	38.482151
2217.861088	320517.832364	38.487168
2220.098416	321014.389674	38.492186
2222.073382	321497.888587	38.497204
2224.808869	321994.813248	38.502221
2226.680603	322488.593835	38.507239
2228.931873	322989.490182	38.512256
2231.324528	323475.311560	38.517274
2233.301416	323978.573332	38.522292
2235.845901	324474.762468	38.527309
2238.065983	324979.902337	38.532327
2240.271374	325488.971050	38.537344
2242.937330	325986.721304	38.542362
2245.035132	326490.136199	38.547380
2247.382523	326988.228396	38.552397
2249.824899	327498.782355	38.557415
2252.178509	327990.188356	38.562432
2254.675879	328490.775430	38.567450
2256.842752	328993.412132	38.572468
2259.094605	329493.060781	38.577485
2261.287637	329992.788351	38.582503
2263.486126	330488.145066	38.587520
2266.220386	330983.614580	38.592538
2268.010030	331489.398458	38.597556
2270.635587	331996.998282	38.602573
2272.779577	332495.635564	38.607591
2274.907151	332995.156745	38.612608
2277.357022	333494.950685	38.617626
2279.877275	334002.819144	38.622644
2282.317576	334499.836160	38.627661
2284.637155	335008.711646	38.632679
2286.622355	335513.015797	38.637696
2289.477172	336007.258943	38.642714
2291.402938	336504.684647	38.647732
2293.853708	337002.275114	38.652749
2296.084137	337502.480472	38.657767
2298.715962	337998.380259	38.662784
2301.113643	338489.896488	38.667802
2302.779308	338980.100132	38.672820
2305.243679	339478.922530	38.677837
2307.824718	339970.694099	38.682855
2310.496910	340448.495047	38.687872
2312.772024	340912.960260	38.692890
2315.238947	341377.972666	38.697908
2317.624444	341822.068142	38.702925
2319.483284	342296.521968	38.707943
2321.837269	342758.769242	38.712960
2323.965911	343221.020234	38.717978
2325.978523	343688.710320	38.722996
2328.408271	344157.064229	38.728013
2330.848488	344639.155077	38.733031
2332.963630	345104.831706	38.738048
2335.424214	345588.275320	38.743066
2337.450462	346069.624476	38.748084
2340.092746	346551.022534	38.753101
2342.243223	347037.967931	38.758119
2344.767653	347514.679341	38.763136
2347.294940	348015.599611	38.768154
2349.269379	348507.825328	38.773172
2351.826909	348994.247289	38.778189
2354.398680	349486.441009	38.783207
2356.605509	349977.847676	38.788224
2359.260124	350468.897982	38.793242
2361.490643	350961.072110	38.798260
2364.212357	351459.120229	38.803277
2366.442784	351959.823621	38.808295
2368.856337	352450.425118	38.813312
2371.028300	352931.016943	38.818330
2373.182276	353445.906901	38.823348
2375.626945	353947.154061	38.828365
2377.837723	354461.486210	38.833383
2380.437476	354977.219507	38.838400
2383.137758	355475.005209	38.843418
2385.406271	355993.055188	38.848436
2387.810463	356500.301357	38.853453
2390.277866	357010.140386	38.858471
2392.596597	357528.765224	38.863488
2395.370598	358042.189551	38.868506
2397.315437	358554.467525	38.873524
2400.347054	359063.879969	38.878541
2402.417068	359586.868690	38.883559
2404.630135	360097.735238	38.888576
2407.138759	360609.560777	38.893594
2409.434028	361133.577348	38.898612
2412.065193	361654.059768	38.903629
2414.338918	362188.402433	38.908647
2416.904848	362708.369684	38.913664
2419.340311	363217.120426	38.918682
2421.776322	363754.704223	38.923700
2424.410545	364280.259484	38.928717
2427.067905	364811.985480	38.933735
2429.438727	365331.708650	38.938752
2432.085142	365855.611606	38.943770
2434.324774	366387.678159	38.948788
2436.908999	366909.290907	38.953805
2438.933748	367420.237019	38.958823
2441.546860	367946.970594	38.963840
2444.188095	368471.206677	38.968858
2446.547956	369008.552401	38.973876
2449.110562	369525.711453	38.978893
2451.255004	370055.975908	38.983911
2453.557445	370585.420135	38.988928
2456.098376	371115.830538	38.993946
2458.565156	371650.904511	38.998964
2461.062530	372179.401119	39.003981
2463.698382	372720.179449	39.008999
2465.894820	373240.316451	39.014016
2468.702897	373766.656443	39.019034
2470.546553	374292.047747	39.024052
2473.227850	374803.693292	39.029069
2475.404509	375312.545383	39.034087
2477.577980	375826.961773	39.039104
2480.032124	376320.374025	39.044122
2482.186105	376845.312539	39.049140
2484.842577	377351.543100	39.054157
2487.148881	377876.741514	39.059175
2489.471091	378407.423907	39.064192
2492.087574	378923.712544	39.069210
2494.500570	379459.121780	39.074228
2496.516133	379985.894252	39.079245
2498.943586	380523.685833	39.084263
2501.475491	381077.786888	39.089280
2504.023226	381621.083964	39.094298
2506.502165	382173.017073	39.099316
2508.682729	382719.919692	39.104333
2511.084262	383276.982653	39.109351
2513.962373	383843.076262	39.114368
2516.450430	384408.230664	39.119386
2518.908752	384982.696653	39.124404
2520.803838	385549.210010	39.129421
2523.635347	386123.085297	39.134439
2526.266619	386710.399984	39.139456
2528.729966	387291.548554	39.144474
2531.084009	387873.992132	39.149492
2533.859481	388458.938944	39.154509
2537.094644	389043.521554	39.159527
2539.035312	389647.460015	39.164544
2542.093062	390218.952151	39.169562
2544.236277	390818.931015	39.174580
2547.002323	391416.215315	39.179597
2549.696854	392013.698713	39.184615
2552.454203	392608.625910	39.189632
2555.021563	393195.568273	39.194650
2557.176001	393801.142607	39.199668
2559.981045	394391.866613	39.204685
2563.053277	394995.748353	39.209703
2565.634016	395596.957804	39.214720
2568.586214	396189.892523	39.219738
2570.906715	396781.594960	39.224756
2573.540486	397381.788965	39.229773
2576.413493	397974.843120	39.234791
2579.119096	398569.275226	39.239808
2581.981184	399165.287567	39.244826
2584.781457	399768.937703	39.249844
2587.354193	400347.805325	39.254861
2590.412021	400938.123007	39.259879
2592.478382	401531.010138	39.264896
2595.329210	402113.586004	39.269914
2598.000112	402699.161292	39.274932
2600.479329	403293.912062	39.279949
2603.293743	403877.663228	39.284967
2605.826292	404459.469726	39.289984
2608.693886	405041.866722	39.295002
2611.381218	405636.573964	39.300020
2614.473658	406214.806353	39.305037
2617.379591	406790.117995	39.310055
2620.078567	407390.393682	39.315072
2622.817144	407947.940447	39.320090
2625.644276	408523.421926	39.325108
2628.526535	409084.054695	39.330125
2630.840075	409647.949693	39.335143
2633.580428	410212.674154	39.340160
2636.567779	410761.813139	39.345178
2638.880905	411324.147174	39.350196
2641.331511	411901.015389	39.355213
2644.389462	412442.663974	39.360231
2647.215069	412988.078864	39.365248
2649.605435	413514.071921	39.370266
2652.204057	414030.054075	39.375284
2654.688395	414558.890215	39.380301
2657.389114	415073.617186	39.385319
2659.671018	415611.412180	39.390336
2662.229419	416124.062108	39.395354
2664.692156	416659.981310	39.400372
2667.129879	417190.529500	39.405389
2669.606933	417729.150531	39.410407
2671.692489	418276.012277	39.415424
2674.626755	418824.244243	39.420442
2677.064905	419381.946026	39.425460
2679.524167	419936.494108	39.430477
2682.060310	420509.827583	39.435495
2684.493420	421076.081613	39.440512
2687.232933	421645.862490	39.445530
2689.681307	422219.870120	39.450548
2692.294622	422810.775119	39.455565
2694.813201	423397.936168	39.460583
2697.407798	423990.023484	39.465600
2700.118182	424584.654025	39.470618
2702.483513	425196.814469	39.475636
2705.343807	425801.244787	39.480653
2708.056953	426416.600040	39.485671
2710.621024	427034.588565	39.490688
2713.480425	427643.665087	39.495706
2716.348185	428268.190367	39.500724
2719.006454	428887.876034	39.505741
2721.631667	429517.404359	39.510759
2724.570182	430149.795321	39.515776
2727.317106	430778.809444	39.520794
2729.715168	431409.475359	39.525812
2732.901759	432051.420011	39.530829
2735.783904	432681.615377	39.535847
2738.715875	433320.626714	39.540864
2741.478710	433951.203845	39.545882
2744.470551	434596.379700	39.550900
2746.831922	435235.871773	39.555917
2749.857576	435872.560504	39.560935
2752.255134	436523.929399	39.565952
2755.153681	437164.435249	39.570970
2758.443724	437810.214106	39.575988
2760.656869	438463.869659	39.581005
2763.644172	439105.761294	39.586023
2766.586614	439762.036615	39.591040
2769.574658	440394.840888	39.596058
2772.702053	441043.868691	39.601076
2775.467320	441702.730658	39.606093
2778.263369	442339.136226	39.611111
2781.104495	442986.070021	39.616128
2784.090732	443631.645234	39.621146
2786.679148	444269.936285	39.626164
2789.323579	444923.752622	39.631181
2792.759733	445559.542956	39.636199
2794.944299	446207.930787	39.641216
2798.172929	446857.445331	39.646234
2801.358540	447506.387888	39.651252
2803.963117	448144.086483	39.656269
2806.652913	448779.678895	39.661287
2809.435722	449420.132312	39.666304
2812.323314	450071.402451	39.671322
2815.232197	450714.011627	39.676340
2818.048284	451353.229416	39.681357
2820.888230	451992.521498	39.686375
2823.307888	452641.549497	39.691392
2826.250585	453276.740357	39.696410
2829.163538	453935.084155	39.701428
2831.802929	454557.756790	39.706445
2834.459691	455179.596964	39.711463
2837.088585	455795.665087	39.716480
2839.891586	456406.232973	39.721498
2842.295414	457018.053209	39.726516
2845.569568	457644.150502	39.731533
2848.365723	458255.663810	39.736551
2850.597767	458889.449345	39.741568
2853.162393	459511.350595	39.746586
2855.966374	460153.427838	39.751604
2858.425639	460797.957070	39.756621
2861.196528	461439.587481	39.761639
2864.054787	462088.748739	39.766656
2866.938861	462757.508518	39.771674
2869.766465	463416.109447	39.776692
2872.113815	464088.785437	39.781709
2874.892031	464757.835663	39.786727
2877.869105	465440.499510	39.791744
2880.724157	466127.846045	39.796762
2883.639705	466811.421954	39.801780
2886.205914	467499.665033	39.806797
2889.331095	468197.980936	39.811815
2891.694162	468903.094699	39.816832
2895.034319	469610.698579	39.821850
2897.897961	470311.790199	39.826868
2900.542710	471034.268760	39.831885
2903.535446	471744.608502	39.836903
2906.460714	472458.961931	39.841920
2909.273421	473187.672442	39.846938
2912.763523	473916.244224	39.851956
2915.637746	474652.291108	39.856973
2918.715774	475372.189318	39.861991
2921.780310	476107.030611	39.867008
2924.709174	476842.565135	39.872026
2927.763106	477565.846848	39.877044
2930.537017	478299.069845	39.882061
2933.914202	479030.400387	39.887079
2936.421024	479763.395688	39.892096
2939.598059	480505.576294	39.897114
2942.784639	481235.725442	39.902132
2945.387622	481983.217758	39.907149
2948.558078	482724.991832	39.912167
2951.695012	483470.565557	39.917184
2954.487962	484216.812313	39.922202
2957.635131	484956.014333	39.927220
2960.787513	485703.997365	39.932237
2963.762101	486444.867992	39.937255
2967.150857	487187.300586	39.942272
2970.063490	487935.111534	39.947290
2973.478166	488670.213687	39.952308
2975.866841	489418.436706	39.957325
2979.248341	490156.746233	39.962343
2982.315288	490896.680620	39.967360
2984.872072	491640.536524	39.972378
2988.267449	492377.475958	39.977396
2990.944531	493118.772027	39.982413
2994.423867	493863.380510	39.987431
2997.876198	494611.782938	39.992448
3000.686715	495351.285346	39.997466
3003.909664	496082.076568	40.002484
3006.918599	496817.345981	40.007501
3009.921301	497546.085212	40.012519
3012.742769	498272.752596	40.017536
3015.897925	499010.205096	40.022554
3018.839909	499736.529207	40.027572
3021.580773	500484.039365	40.032589
3024.854169	501216.277884	40.037607
3027.839731	501953.859296	40.042624
3030.764010	502673.445953	40.047642
3033.850012	503370.979626	40.052660
3036.629676	504064.803503	40.057677
3039.410579	504762.317232	40.062695
3042.511584	505471.822953	40.067712
3045.235789	506166.559798	40.072730
3048.446538	506870.393724	40.077748
3051.116801	507592.438963	40.082765
3054.314058	508290.469121	40.087783
3057.295432	509002.684353	40.092800
3059.795574	509729.174211	40.097818
3063.414267	510435.683929	40.102836
3066.045508	511166.756589	40.107853
3069.262645	511895.033758	40.112871
3072.283965	512627.729083	40.117888
3075.535428	513368.345661	40.122906
3078.413053	514108.126207	40.127924
3081.446716	514849.451785	40.132941
3084.279417	515586.344179	40.137959
3087.696548	516343.468212	40.142976
3090.390671	517105.841771	40.147994
3093.846880	517864.082111	40.153012
3096.403030	518626.392260	40.158029
3099.642769	519402.627408	40.163047
3103.033138	520159.141392	40.168064
3105.574338	520942.936947	40.173082
3109.071764	521720.958763	40.178100
3112.154290	522507.191964	40.183117
3115.134423	523291.585962	40.188135
3118.156116	524072.007982	40.193152
3121.479074	524878.917400	40.198170
3124.820536	525667.184978	40.203188
3127.961145	526452.472892	40.208205
3131.279343	527255.369833	40.213223
3134.395468	528042.074080	40.218240
3137.479171	528855.509430	40.223258
3140.794309	529653.588824	40.228276
3143.817256	530458.445509	40.233293
3146.924063	531256.409219	40.238311
3150.415943	532058.431869	40.243328
3153.400520	532875.197335	40.248346
3156.327440	533668.370616	40.253364
3159.862788	534492.429253	40.258381
3163.088845	535299.212550	40.263399
3166.771487	536112.199225	40.268416
3169.568909	536923.264601	40.273434
3172.944285	537734.137811	40.278452
3176.725410	538545.197006	40.283469
3180.069729	539357.627722	40.288487
3183.451078	540154.342146	40.293504
3185.920238	540955.113351	40.298522
3189.544171	541761.323408	40.303540
3192.823991	542571.148185	40.308557
3195.841839	543371.478601	40.313575
3199.446798	544171.716038	40.318592
3202.526080	544977.151431	40.323610
3206.322301	545777.506342	40.328628
3209.365552	546582.241046	40.333645
3212.915002	547376.712265	40.338663
3216.385522	548167.533407	40.343680
3219.823882	548961.969671	40.348698
3223.321289	549740.999842	40.353716
3226.785466	550524.047245	40.358733
3229.759994	551289.621410	40.363751
3233.496360	552062.198043	40.368768
3236.581578	552854.329857	40.373786
3239.913177	553610.125777	40.378804
3242.771792	554377.628323	40.383821
3246.203522	555138.526079	40.388839
3249.390295	555875.756001	40.393856
3252.431437	556607.951328	40.398874
3255.758608	557317.554701	40.403892
3258.975889	558044.522413	40.408909
3262.281998	558773.887194	40.413927
3265.458273	559490.951094	40.418944
3268.006007	560214.282757	40.423962
3271.356144	560945.460869	40.428980
3274.533776	561697.511481	40.433997
3277.804887	562443.538052	40.439015
3280.991599	563180.263368	40.444032
3283.773488	563936.490018	40.449050
3287.023190	564688.287187	40.454068
3290.060843	565453.941672	40.459085
3293.089617	566226.157450	40.464103
3296.289786	566991.284412	40.469120
3299.605084	567781.879426	40.474138
3303.191924	568549.446375	40.479156
3306.084610	569333.441938	40.484173
3309.310631	570140.360199	40.489191
3312.708451	570937.683660	40.494208
3316.065340	571749.173344	40.499226
3319.321814	572552.062167	40.504244
3322.551344	573362.005198	40.509261
3325.682547	574174.808254	40.514279
3329.212292	574986.289586	40.519296
3332.466927	575812.466298	40.524314
3335.745660	576633.174988	40.529332
3338.838892	577465.859668	40.534349
3342.286070	578302.979374	40.539367
3345.690290	579141.793768	40.544384
3348.942831	579991.022426	40.549402
3352.497363	580824.284441	40.554420
3356.158571	581666.969060	40.559437
3359.506881	582525.940441	40.564455
3363.120075	583364.052362	40.569472
3366.689391	584212.656985	40.574490
3370.345665	585065.781860	40.579508
3373.389980	585917.486107	40.584525
3376.815330	586774.362922	40.589543
3380.373187	587612.507803	40.594560
3383.694802	588468.367550	40.599578
3387.135352	589319.593283	40.604596
3390.792607	590175.065545	40.609613
3393.955194	591032.745757	40.614631
3397.646092	591885.578346	40.619648
3401.201891	592735.616409	40.624666
3404.473044	593590.527013	40.629684
3407.948535	594456.176598	40.634701
3411.367362	595318.717797	40.639719
3414.960675	596170.823322	40.644736
3418.324243	597030.187290	40.649754
3421.492849	597883.769227	40.654772
3425.177749	598746.238809	40.659789
3428.805743	599604.352736	40.664807
3432.009139	600460.066454	40.669824
3435.693895	601330.211181	40.674842
3439.294472	602182.676541	40.679860
3442.913859	603036.815956	40.684877
3445.591064	603894.376076	40.689895
3449.263405	604755.102946	40.694912
3452.618753	605623.491927	40.699930
3455.965209	606473.248500	40.704948
3459.732677	607336.439020	40.709965
3462.962774	608203.382257	40.714983
3466.309842	609074.922544	40.720000
3469.404545	609944.881609	40.725018
3472.959128	610788.133805	40.730023
3476.496156	611605.706714	40.735028
3479.369730	612379.723784	40.740032
3482.943727	613097.434418	40.745037
3485.883279	613763.257981	40.750042
3488.640167	614376.584253	40.755047
3491.382578	614922.102591	40.760052
3494.041984	615449.612365	40.765056
3496.266717	615908.596627	40.770061
3498.248566	616306.330881	40.775066
3500.652746	616667.404311	40.780071
3502.929903	616979.814066	40.785076
3504.406264	617250.865498	40.790080
3506.360424	617474.665830	40.795085
3507.988103	617654.291989	40.800090
3509.615704	617802.686422	40.805095
3511.134583	617897.183341	40.810100
3512.088533	617970.632576	40.815104
3513.208640	618007.581176	40.820109
3514.213678	618028.608955	40.825114
3515.449643	618008.379855	40.830119
3516.030439	617972.164481	40.835124
3516.904043	617907.922768	40.840128
3517.869288	617823.580184	40.845133
3518.508789	617721.449942	40.850138
3519.165054	617589.286077	40.855143
3519.635603	617446.356532	40.860148
3520.212229	617284.120631	40.865152
3520.157399	617102.942575	40.870157
3520.893153	616930.482339	40.875162
3521.341091	616721.085596	40.880167
3521.682316	616512.200872	40.885172
3521.296666	616292.831100	40.890176
3521.984227	616069.290798	40.895181
3522.241680	615828.121423	40.900186
3522.055254	615589.014702	40.905191
3522.453394	615332.618476	40.910196
3522.269411	615078.155933	40.915200
3522.477463	614811.880219	40.920205
3522.675439	614550.047414	40.925210
3522.477980	614271.925089	40.930215
3522.613819	613998.241588	40.935220
3522.206255	613729.334279	40.940224
3522.626648	613440.645328	40.945229
3522.358413	613167.952204	40.950234
3522.136212	612882.597007	40.955239
3522.103251	612604.452940	40.960244
3521.919018	612330.424285	40.965248
3521.874280	612046.167564	40.970253
3521.652674	611767.480033	40.975258
3521.371969	611487.444153	40.980263
3521.241970	611204.427067	40.985268
3520.861737	610927.991184	40.990272
3520.933620	610643.476903	40.995277
3521.308152	610381.058482	41.000282
3520.663312	610089.340368	41.005287
3520.356416	609810.212412	41.010292
3520.346135	609543.432086	41.015296
3520.051423	609266.987700	41.020301
3519.632972	608999.806888	41.025306
3519.598863	608735.309581	41.030311
3519.746217	608472.627499	41.035316
3519.152790	608211.604882	41.040320
3518.994286	607948.957166	41.045325
3518.757835	607693.867267	41.050330
3518.376301	607440.994442	41.055335
3518.622132	607184.666088	41.060340
3518.132889	606936.049195	41.065344
3518.182452	606675.237062	41.070349
3517.856086	606428.083029	41.075354
3517.749244	606188.642306	41.080359
3517.283163	605941.698519	41.085364
3517.194213	605711.848551	41.090368
3517.113233	605473.037475	41.095373
3516.740543	605236.517714	41.100378
3516.599694	605005.759624	41.105383
3516.447229	604767.693830	41.110388
3515.785472	604552.616363	41.115392
3515.500423	604322.315827	41.120397
3515.510894	604116.129957	41.125402
3515.231098	603900.628987	41.130407
3515.047932	603690.812430	41.135412
3515.017268	603486.621865	41.140416
3514.986604	603276.322755	41.145421
3514.735093	603074.060005	41.150426
3514.274560	602875.378761	41.155431
3514.226990	602663.118351	41.160436
3513.875330	602470.066861	41.165440
3513.916966	602274.848543	41.170445
3513.805924	602077.848888	41.175450
3513.491837	601888.183643	41.180455
3513.467012	601691.513509	41.185460
3512.989582	601518.782178	41.190464
3512.972020	601333.764769	41.195469
3512.987684	601153.843713	41.200474
3512.766656	600969.151932	41.205479
3512.694570	600798.947825	41.210484
3512.339538	600627.483882	41.215488
3512.417700	600453.446873	41.220493
3512.216373	600283.454781	41.225498
3511.877958	600108.426076	41.230503
3512.016006	599942.880106	41.235508
3511.890337	599786.482553	41.240512
3511.401192	599611.018615	41.245517
3511.252337	599455.620843	41.250522
3510.892819	599303.607465	41.255527
3510.997194	599149.567146	41.260532
3511.049572	599003.541914	41.265536
3510.837433	598835.980864	41.270541
3510.458019	598693.222556	41.275546
3510.375791	598543.307364	41.280551
3510.198784	598401.464589	41.285556
3510.122495	598262.357517	41.290560
3510.224639	598124.121825	41.295565
3510.102479	597984.267325	41.300570
3509.722569	597856.466398	41.305575
3509.631697	597718.606002	41.310580
3509.625127	597582.282619	41.315584
3509.341482	597441.695200	41.320589
3509.036112	597318.381947	41.325594
3508.695032	597200.179584	41.330599
3508.843769	597072.586912	41.335604
3508.701190	596955.251978	41.340608
3509.064760	596827.272290	41.345613
3508.799788	596707.800822	41.350618
3508.732751	596591.201066	41.355623
3508.799718	596469.221628	41.360628
3507.882100	596357.609018	41.365632
3507.990273	596232.616203	41.370637
3508.027698	596122.604288	41.375642
3508.037680	596016.000402	41.380647
3507.839319	595913.383721	41.385652
3507.912518	595805.115447	41.390656
3507.696152	595699.244779	41.395661
3507.943402	595604.967755	41.400666
3507.533011	595488.409537	41.405671
3507.840950	595391.417119	41.410676
3507.370856	595300.904990	41.415680
3507.188268	595186.811602	41.420685
3507.198826	595093.017717	41.425690
3507.314927	594994.048618	41.430695
3507.374429	594898.342453	41.435700
3506.707222	594808.558018	41.440704
3506.982635	594708.559808	41.445709
3506.803908	594619.899286	41.450714
3506.934536	594531.139586	41.455719
3506.799614	594425.543963	41.460724
3506.764688	594343.318879	41.465728
3506.819515	594249.109995	41.470733
3506.404389	594169.947813	41.475738
3506.698970	594083.963262	41.480743
3506.648400	593979.802378	41.485748
3506.244651	593903.190583	41.490752
3506.097251	593805.103015	41.495757
3506.066341	593734.040920	41.500762
3505.933847	593654.129567	41.505767
3505.991732	593570.381525	41.510772
3505.598986	593497.070586	41.515776
3505.805121	593418.707208	41.520781
3505.665668	593346.607738	41.525786
3505.568583	593280.511316	41.530791
3505.813363	593201.639459	41.535796
3505.715259	593134.089825	41.540800
3505.393128	593051.298656	41.545805
3505.556546	592984.208049	41.550810
3505.535469	592915.292668	41.555815
3505.652394	592836.488191	41.560820
3505.133128	592779.770796	41.565824
3505.407675	592706.800898	41.570829
3505.122020	592645.287972	41.575834
3504.913354	592577.251228	41.580839
3505.197675	592503.927805	41.585844
3505.169314	592453.943940	41.590848
3505.018410	592381.188600	41.595853
3504.826526	592306.635961	41.600858
3504.989674	592248.807283	41.605863
3505.122832	592185.523201	41.610868
3504.937825	592133.859279	41.615872
3504.896968	592054.773177	41.620877
3504.542790	592011.650471	41.625882
3504.529330	591954.549084	41.630887
3504.584419	591891.225378	41.635892
3504.191059	591833.982374	41.640896
3504.692698	591777.100066	41.645901
3504.633576	591721.457235	41.650906
3504.305062	591674.121436	41.655911
3504.436109	591608.079209	41.660916
3504.528755	591566.487819	41.665920
3504.582958	591504.063635	41.670925
3504.683958	591450.999203	41.675930
3504.699165	591395.894090	41.680935
3504.705430	591327.264785	41.685940
3504.382809	591270.759122	41.690944
3504.344188	591212.505559	41.695949
3504.261819	591157.113909	41.700954
3503.921396	591107.423028	41.705959
3504.504172	591055.784173	41.710964
3504.470780	591015.863493	41.715968
3504.253810	590946.114461	41.720973
3504.482347	590896.233468	41.725978
3504.309786	590844.110530	41.730983
3504.325807	590788.250735	41.735988
3504.223176	590735.865859	41.740992
3504.579805	590675.844319	41.745997
3504.146376	590638.539712	41.751002
3503.921901	590580.311779	41.756007
3504.459235	590531.432865	41.761012
3504.000434	590486.416683	41.766016
3504.080587	590426.186485	41.771021
3503.932609	590384.227357	41.776026
3504.166069	590340.204502	41.781031
3504.422580	590290.216134	41.786036
3504.369225	590237.871231	41.791040
3504.130012	590176.837886	41.796045
3504.263888	590127.819819	41.801050
3504.390381	590085.716423	41.806055
3504.089976	590019.681799	41.811060
3504.177868	589981.491818	41.816064
3503.990892	589927.663297	41.821069
3503.933880	589882.631879	41.826074
3503.611547	589838.643764	41.831079
3504.109681	589788.765602	41.836084
3503.753231	589750.193358	41.841088
3503.982983	589698.753502	41.846093
3504.294442	589642.691281	41.851098
3503.816925	589611.552502	41.856103
3503.809113	589551.882293	41.861108
3503.703153	589516.626890	41.866112
3503.692437	589467.127406	41.871117
3503.972749	589420.137433	41.876122
3503.591511	589379.663839	41.881127
3504.042889	589329.941180	41.886132
3503.770553	589296.765293	41.891136
3503.909397	589240.427352	41.896141
3503.714179	589198.721516	41.901146
3503.487719	589154.064275	41.906151
3503.706437	589108.986527	41.911156
3503.166057	589074.448945	41.916160
3503.218318	589028.996052	41.921165
3503.606466	588996.667975	41.926170
3503.499256	588953.444296	41.931175
3503.746505	588914.123326	41.936180
3503.245336	588881.432881	41.941184
3503.627873	588835.025649	41.946189
3503.748660	588787.757238	41.951194
3503.314525	588750.997368	41.956199
3503.284167	588711.117791	41.961204
3503.138238	588679.022576	41.966208
3503.524134	588640.731166	41.971213
3503.360157	588608.087394	41.976218
3503.222649	588563.514022	41.981223
3503.124350	588531.260603	41.986228
3503.212855	588492.714521	41.991232
3503.320983	588442.841024	41.996237
3503.678219	588415.626976	42.001242
3503.386905	588381.148457	42.006247
3503.152113	588339.194956	42.011252
3503.016731	588306.946667	42.016256
3503.275468	588264.715294	42.021261
3503.151203	588228.556610	42.026266
3503.051358	588191.542147	42.031271
3502.906617	588153.582514	42.036276
3502.972450	588124.609386	42.041280
3503.371958	588095.734344	42.046285
3503.260859	588068.141662	42.051290
3502.784666	588033.490502	42.056295
3503.268933	587995.632421	42.061300
3503.237313	587972.236243	42.066304
3503.052773	587924.009611	42.071309
3503.147779	587888.166281	42.076314
3503.149003	587860.154632	42.081319
3503.295707	587812.527150	42.086324
3503.216669	587789.739313	42.091328
3502.969474	587753.397822	42.096333
3503.114561	587714.238806	42.101338
3503.416776	587672.298996	42.106343
3503.482032	587640.117580	42.111348
3503.058935	587607.461191	42.116352
3503.567334	587570.199189	42.121357
3503.074629	587538.906477	42.126362
3503.111321	587504.524226	42.131367
3503.135420	587466.535796	42.136372
3502.851215	587436.162315	42.141376
3502.988235	587402.666069	42.146381
3503.119074	587373.680777	42.151386
3502.680377	587339.071647	42.156391
3502.695524	587297.175268	42.161396
3503.021279	587277.079258	42.166400
3502.789303	587246.947645	42.171405
3502.713768	587214.536415	42.176410
3502.581236	587180.079367	42.181415
3502.591834	587152.515446	42.186420
3502.915941	587138.332783	42.191424
3502.763430	587102.826237	42.196429
3502.925206	587079.147336	42.201434
3502.776480	587055.266356	42.206439
3502.650119	587015.445670	42.211444
3502.119300	586994.079861	42.216448
3502.116694	586967.620040	42.221453
3502.587864	586948.102059	42.226458
3502.746920	586920.263770	42.231463
3502.734460	586887.340564	42.236468
3502.571874	586863.260872	42.241472
3502.663015	586828.166369	42.246477
3502.881265	586801.471160	42.251482
3503.094139	586775.929367	42.256487
3503.218111	586756.314976	42.261492
3503.173502	586723.997681	42.266496
3503.174158	586684.907655	42.271501
3503.034912	586649.046747	42.276506
3502.802955	586631.091467	42.281511
3503.275163	586591.175654	42.286516
3502.932953	586568.626862	42.291520
3502.945590	586529.133478	42.296525
3502.930294	586488.792342	42.301530
3503.239968	586465.088987	42.306535
3503.180593	586421.296469	42.311540
3502.747949	586399.012045	42.316544
3502.539187	586367.821919	42.321549
3502.539048	586332.940559	42.326554
3502.689064	586306.605624	42.331559
3502.665538	586277.491196	42.336564
3502.732313	586256.230982	42.341568
3502.476413	586223.343826	42.346573
3502.514814	586198.629835	42.351578
3502.512524	586166.304270	42.356583
3502.679150	586142.522343	42.361588
3502.623879	586126.292729	42.366592
3502.572601	586089.864933	42.371597
3502.805210	586068.478193	42.376602
3502.777558	586044.125006	42.381607
3502.774043	586003.780235	42.386612
3502.513775	585987.482225	42.391616
3502.349660	585957.737382	42.396621
3502.766120	585938.576983	42.401626
3502.472102	585915.618354	42.406631
3502.284601	585876.805440	42.411636
3502.275662	585861.269855	42.416640
3502.346176	585835.146688	42.421645
3502.662087	585809.436170	42.426650
3502.517316	585794.222440	42.431655
3502.514780	585756.282330	42.436660
3502.257620	585733.768631	42.441664
3501.997421	585705.992788	42.446669
3502.455478	585690.885153	42.451674
3502.324557	585670.657102	42.456679
3502.316268	585649.457562	42.461684
3502.338177	585625.446532	42.466688
3502.771064	585602.223247	42.471693
3503.052205	585583.233742	42.476698
3502.608915	585552.579152	42.481703
3502.736099	585520.431916	42.486708
3502.940584	585490.728419	42.491712
3502.646538	585473.933715	42.496717
3502.512229	585438.669506	42.501722
3502.270255	585419.811617	42.506727
3502.404524	585385.708156	42.511732
3502.124806	585371.667721	42.516736
3502.329908	585344.219188	42.521741
3502.724294	585324.710317	42.526746
3502.301528	585306.231346	42.531751
3502.693235	585281.610414	42.536756
3502.529397	585255.672864	42.541760
3501.960161	585221.277895	42.546765
3502.243023	585211.058819	42.551770
3502.600756	585188.949092	42.556775
3503.028161	585155.751410	42.561780
3502.620524	585138.422601	42.566784
3502.673988	585102.777098	42.571789
3502.974796	585080.224948	42.576794
3502.628350	585053.062398	42.581799
3502.525683	585011.225782	42.586804
3502.788465	584991.436155	42.591808
3502.242499	584962.851004	42.596813
3502.726651	584940.921507	42.601818
3502.182907	584915.744267	42.606823
3502.599164	584888.261581	42.611828
3502.266956	584860.544969	42.616832
3502.325248	584842.290750	42.621837
3502.357348	584824.942823	42.626842
3502.635556	584807.456148	42.631847
3502.435816	584792.249616	42.636852
3501.994049	584762.043683	42.641856
3502.008317	584742.843823	42.646861
3502.439549	584718.566319	42.651866
3502.247271	584700.651781	42.656871
3502.837711	584673.792946	42.661876
3502.506071	584652.792397	42.666880
3502.383113	584620.130254	42.671885
3502.426160	584601.827893	42.676890
3502.092435	584582.381404	42.681895
3502.693783	584559.881452	42.686900
3502.898529	584530.526186	42.691904
3502.559802	584498.398662	42.696909
3502.658626	584476.728978	42.701914
3502.523544	584451.737410	42.706919
3502.476216	584425.729553	42.711924
3502.413405	584405.388263	42.716928
3502.392420	584378.173158	42.721933
3502.512639	584340.760336	42.726938
3502.350034	584329.808066	42.731943
3502.491300	584299.158828	42.736948
3502.597167	584291.322500	42.741952
3502.835135	584256.597800	42.746957
3502.907161	584225.708550	42.751962
3502.301839	584205.902838	42.756967
3502.632705	584186.050990	42.761972
3502.085788	584155.007666	42.766976
3502.207102	584127.619314	42.771981
3502.373455	584117.467564	42.776986
3502.182962	584098.599349	42.781991
3502.509668	584063.509276	42.786996
3502.356491	584051.151690	42.792001
3502.135769	584023.816549	42.797005
3502.627674	584006.445575	42.802010
3502.451358	583990.632737	42.807015
3502.584701	583954.018588	42.812020
3502.231348	583924.097288	42.817025
3502.405191	583900.710390	42.822029
3502.476977	583879.895932	42.827034
3502.343311	583861.670091	42.832039
3502.405939	583834.741337	42.837044
3502.114193	583816.840904	42.842049
3502.340071	583786.227136	42.847053
3502.334855	583777.204722	42.852058
3502.145606	583754.977105	42.857063
3502.531837	583731.707032	42.862068
3502.333260	583701.961445	42.867073
3502.085447	583681.697864	42.872077
3502.238429	583660.770039	42.877082
3502.095813	583647.357635	42.882087
3502.313787	583608.122386	42.887092
3502.178603	583602.528942	42.892097
3501.824845	583570.802084	42.897101
3502.209739	583562.420321	42.902106
3502.197624	583564.577697	42.907111
3502.359446	583533.822853	42.912116
3502.215519	583511.687918	42.917121
3502.278129	583491.776496	42.922125
3502.578647	583475.036163	42.927130
3502.232165	583444.460792	42.932135
3502.190316	583421.457506	42.937140
3502.068820	583405.936036	42.942145
3502.198866	583385.512577	42.947149
3502.327273	583367.495598	42.952154
3502.221794	583347.860844	42.957159
3502.033695	583333.803471	42.962164
3501.955604	583299.526203	42.967169
3502.078792	583289.330308	42.972173
3502.442697	583261.851745	42.977178
3501.990781	583247.584849	42.982183
3501.880398	583225.544356	42.987188
3502.122485	583207.008031	42.992193
3501.822641	583187.854558	42.997197
3502.324284	583173.689153	43.002202
3501.871249	583158.169031	43.007207
3502.126784	583126.696560	43.012212
3501.913904	583117.706068	43.017217
3502.066842	583099.484290	43.022221
3502.146537	583081.173667	43.027226
3502.014276	583060.138898	43.032231
3502.263344	583045.962682	43.037236
3502.066158	583027.394464	43.042241
3502.306846	583001.187814	43.047245
3502.196287	582979.497780	43.052250
3502.232867	582961.043302	43.057255
3502.509043	582938.891672	43.062260
3502.133169	582926.968693	43.067265
3502.134546	582909.121221	43.072269
3501.934347	582885.239183	43.077274
3502.201759	582877.125931	43.082279
3502.299946	582842.769552	43.087284
3501.971841	582825.173982	43.092289
3501.956505	582815.450501	43.097293
3502.008170	582813.938346	43.102298
3501.927158	582786.377754	43.107303
3502.318052	582762.503311	43.112308
3501.824817	582743.629962	43.117313
3501.983331	582723.852559	43.122317
3502.073743	582715.516193	43.127322
3501.915020	582694.184060	43.132327
3502.165627	582677.801257	43.137332
3502.077850	582657.661169	43.142337
3501.824928	582637.145791	43.147341
3502.111967	582622.060687	43.152346
3501.946580	582612.310350	43.157351
3502.197338	582591.264942	43.162356
3502.192733	582573.167191	43.167361
3502.092259	582547.012796	43.172365
3502.331759	582526.670904	43.177370
3502.257948	582509.135343	43.182375
3502.304060	582487.319580	43.187380
3502.287852	582464.510824	43.192385
3502.245051	582452.134184	43.197389
3502.081800	582427.643762	43.202394
3501.805009	582406.881013	43.207399
3502.154228	582389.579940	43.212404
3502.139864	582362.208408	43.217409
3502.282624	582351.256561	43.222413
3502.015390	582318.359457	43.227418
3501.669775	582313.099063	43.232423
3502.351038	582284.315074	43.237428
3501.878058	582274.662659	43.242433
3501.673678	582257.397787	43.247437
3501.777048	582242.340879	43.252442
3501.518542	582239.974695	43.257447
3502.170430	582231.550188	43.262452
3501.759119	582211.108913	43.267457
3501.863326	582195.249638	43.272461
3501.973519	582164.799861	43.277466
3501.534884	582153.637892	43.282471
3501.596518	582148.764978	43.287476
3501.547951	582134.834667	43.292481
3501.805859	582115.191045	43.297485
3502.314612	582094.655857	43.302490
3501.926749	582086.644465	43.307495
3501.937780	582071.300941	43.312500
3501.751393	582060.801353	43.317505
3501.657781	582041.864326	43.322509
3502.017611	582032.131641	43.327514
3501.972850	582016.696491	43.332519
3502.220749	581983.918405	43.337524
3502.395912	581974.465222	43.342529
3501.709938	581950.205867	43.347533
3501.962340	581933.721407	43.352538
3501.849858	581927.221095	43.357543
3502.142969	581898.246099	43.362548
3502.081168	581882.863562	43.367553
3501.817276	581858.989258	43.372557
3501.733492	581846.568207	43.377562
3501.947574	581840.417892	43.382567
3501.840145	581814.212710	43.387572
3501.622323	581808.129895	43.392577
3501.912088	581784.971078	43.397581
3501.933846	581776.093222	43.402586
3501.626077	581770.174861	43.407591
3502.065628	581739.722563	43.412596
3501.821177	581730.184356	43.417601
3502.331078	581713.458762	43.422605
3502.376084	581699.964517	43.427610
3502.076668	581684.318021	43.432615
3502.053665	581657.648027	43.437620
3501.985406	581634.244036	43.442625
3502.041764	581612.876189	43.447629
3501.983710	581603.960533	43.452634
3501.622306	581602.362373	43.457639
3501.952986	581582.004490	43.462644
3501.940148	581566.413304	43.467649
3502.062678	581546.188172	43.472653
3501.740081	581534.155075	43.477658
3501.778056	581512.037826	43.482663
3502.101836	581494.137665	43.487668
3501.873848	581490.061822	43.492673
3501.802310	581467.109240	43.497677
3501.417628	581458.846197	43.502682
3501.846739	581448.400223	43.507687
3501.817403	581435.268250	43.512692
3501.880978	581418.662126	43.517697
3501.998198	581402.950099	43.522701
3502.245887	581387.167515	43.527706
3501.736121	581374.311133	43.532711
3501.912498	581350.216483	43.537716
3501.475434	581339.404419	43.542721
3501.222089	581341.549801	43.547725
3501.661669	581326.739925	43.552730
3501.751460	581313.539045	43.557735
3502.080008	581293.080686	43.562740
3502.054158	581277.340707	43.567745
3501.755536	581259.236627	43.572749
3501.843130	581251.300718	43.577754
3501.705951	581228.759024	43.582759
3501.906057	581219.150878	43.587764
3501.478230	581203.824617	43.592769
3501.721877	581184.783257	43.597773
3502.074085	581168.482619	43.602778
3501.501924	581167.870010	43.607783
3501.744859	581136.293562	43.612788
3501.859777	581123.439512	43.617793
3501.723562	581126.017890	43.622797
3502.227625	581097.408947	43.627802
3502.082870	581091.765580	43.632807
3501.805359	581066.337328	43.637812
3501.982217	581043.896586	43.642817
3501.778691	581029.287133	43.647821
3501.800876	581015.193928	43.652826
3501.822027	581004.911596	43.657831
3502.400322	580992.737073	43.662836
3501.897627	580970.101569	43.667841
3501.692105	580969.080641	43.672845
3501.898544	580941.570792	43.677850
3501.691258	580934.483018	43.682855
3501.917865	580932.943259	43.687860
3501.928266	580911.882094	43.692865
3501.781745	580887.084792	43.697869
3502.171908	580870.777783	43.702874
3501.771155	580855.396664	43.707879
3502.020955	580842.370777	43.712884
3502.090417	580824.459152	43.717889
3501.695651	580811.935130	43.722893
3501.921928	580790.990413	43.727898
3501.638972	580782.560533	43.732903
3501.585913	580766.272518	43.737908
3501.649588	580758.189569	43.742913
3501.615384	580730.365820	43.747917
3501.979150	580717.121400	43.752922
3501.836401	580707.466124	43.757927
3502.091547	580686.366270	43.762932
3501.712336	580678.502926	43.767937
3501.851821	580666.246218	43.772941
3501.825199	580650.304899	43.777946
3501.851290	580643.230597	43.782951
3501.761264	580621.482580	43.787956
3501.967041	580611.873022	43.792961
3501.903989	580594.633601	43.797965
3502.016676	580573.154658	43.802970
3501.563185	580562.043539	43.807975
3501.841007	580548.812355	43.812980
3501.890837	580539.628260	43.817985
3501.869515	580527.045534	43.822989
3502.108850	580499.178443	43.827994
3501.858664	580486.280445	43.832999
3502.008419	580474.423068	43.838004
3501.841696	580457.751220	43.843009
3501.997664	580443.937236	43.848013
3501.970786	580421.527087	43.853018
3501.955758	580409.444682	43.858023
3502.070587	580397.642827	43.863028
3501.876850	580381.777391	43.868033
3501.922994	580362.514778	43.873037
3502.091088	580341.026724	43.878042
3501.939383	580324.853770	43.883047
3502.096795	580307.278572	43.888052
3501.988290	580305.038951	43.893057
3501.611322	580293.564589	43.898061
3501.795106	580277.339119	43.903066
3501.720896	580256.239792	43.908071
3501.576899	580247.336479	43.913076
3501.548813	580237.813302	43.918081
3501.699656	580215.926546	43.923085
3501.616866	580209.370437	43.928090
3502.065313	580197.766939	43.933095
3501.699076	580173.553983	43.938100
3501.943906	580167.849241	43.943105
3501.746845	580150.780514	43.948109
3501.620168	580135.154967	43.953114
3501.522831	580128.901954	43.958119
3501.930209	580116.552616	43.963124
3501.720631	580095.724871	43.968129
3501.743508	580083.736477	43.973133
3501.515217	580068.929046	43.978138
3501.669134	580053.109082	43.983143
3501.620001	580049.907363	43.988148
3502.037283	580035.199548	43.993153
3501.803526	580009.511301	43.998157
3501.769136	579998.634972	44.003162
3501.126087	579999.337160	44.008167
3501.904444	579989.236388	44.013172
3501.836929	579972.197281	44.018177
3501.619610	579956.385068	44.023181
3501.731479	579950.500417	44.028186
3501.767896	579933.244419	44.033191
3501.876963	579913.770608	44.038196
3501.263951	579902.382887	44.043201
3501.644661	579887.530156	44.048205
3501.742234	579872.721667	44.053210
3501.969805	579870.128542	44.058215
3502.063097	579849.052402	44.063220
3502.061758	579835.763719	44.068225
3501.803901	579820.759994	44.073229
3501.720631	579799.460629	44.078234
3501.867361	579798.885989	44.083239
3502.056832	579777.393505	44.088244
3501.936108	579768.185289	44.093249
3502.058143	579747.204756	44.098253
3502.210812	579727.773950	44.103258
3501.520114	579713.840685	44.108263
3501.983414	579699.576556	44.113268
3502.015478	579683.173351	44.118273
3501.583897	579669.249669	44.123277
3501.792267	579646.600591	44.128282
3501.768248	579649.011329	44.133287
3501.714503	579624.497585	44.138292
3501.692496	579603.689742	44.143297
3501.761486	579598.062347	44.148301
3501.311276	579595.224082	44.153306
3501.411663	579577.405908	44.158311
3501.498176	579551.566240	44.163316
3501.586507	579547.390079	44.168321
3501.315798	579541.514873	44.173325
3501.443644	579541.193912	44.178330
3501.425723	579525.299766	44.183335
3501.278698	579507.620454	44.188340
3501.506684	579503.322149	44.193345
3501.244238	579506.221521	44.198349
3501.408344	579505.794594	44.203354
3501.235408	579499.803786	44.208359
3501.347825	579477.119216	44.213364
3501.461079	579475.446536	44.218369
3501.396999	579468.987361	44.223373
3501.646246	579465.788976	44.228378
3501.454552	579451.075297	44.233383
3501.590076	579424.926783	44.238388
3501.548887	579425.033430	44.243393
3501.347423	579422.005789	44.248397
3501.381397	579417.487039	44.253402
3501.136584	579396.462898	44.258407
3501.281786	579381.495866	44.263412
3501.566100	579381.451331	44.268417
3501.333968	579380.434413	44.273421
3501.258344	579378.741097	44.278426
3501.480498	579369.529096	44.283431
3501.533934	579359.240195	44.288436
3501.659659	579355.308860	44.293441
3501.489200	579350.471002	44.298445
3501.768390	579333.627459	44.303450
3501.725162	579315.129235	44.308455
3501.742653	579303.441734	44.313460
3501.821267	579289.036625	44.318465
3501.882104	579279.649174	44.323469
3502.086960	579257.050004	44.328474
3501.678908	579244.927476	44.333479
3501.610586	579226.884371	44.338484
3501.623886	579212.238627	44.343489
3501.693414	579202.047363	44.348493
3501.718562	579189.004514	44.353498
3501.759667	579179.820661	44.358503
3501.965967	579166.548869	44.363508
3501.622522	579149.100291	44.368513
3501.891859	579143.240748	44.373517
3502.083511	579126.109679	44.378522
3501.713861	579106.107498	44.383527
3501.436743	579105.197886	44.388532
3501.554286	579077.496727	44.393537
3501.481527	579059.604493	44.398541
3501.750145	579056.051914	44.403546
3501.237545	579059.341558	44.408551
3501.782225	579041.102021	44.413556
3501.961897	579028.736929	44.418561
3501.755313	579024.606677	44.423565
3501.959567	579003.210689	44.428570
3501.816814	578995.309182	44.433575
3501.829648	578982.468617	44.438580
3501.903799	578968.264393	44.443585
3501.738938	578950.486683	44.448589
3501.824467	578941.446140	44.453594
3501.827332	578923.240963	44.458599
3501.923336	578912.443489	44.463604
3501.928206	578898.952115	44.468609
3501.597199	578874.078859	44.473613
3501.606116	578862.091332	44.478618
3501.771446	578860.962079	44.483623
3501.827461	578834.172649	44.488628
3501.800133	578821.388328	44.493633
3501.550129	578815.108292	44.498637
3501.764242	578785.335117	44.503642
3501.791206	578782.622649	44.508647
3501.872908	578777.745120	44.513652
3501.993174	578756.813152	44.518657
3501.478417	578751.326737	44.523661
3501.609363	578743.933929	44.528666
3501.719780	578723.504951	44.533671
3501.591169	578709.131489	44.538676
3501.547478	578703.772015	44.543681
3501.841059	578693.043745	44.548685
3501.806160	578677.953470	44.553690
3502.010128	578664.982357	44.558695
3501.969503	578638.658931	44.563700
3501.668612	578625.967304	44.568705
3501.719380	578615.778438	44.573709
3501.773676	578584.575306	44.578714
3501.545495	578579.144310	44.583719
3501.805745	578573.135433	44.588724
3501.585378	578555.566379	44.593729
3501.449992	578547.763706	44.598733
3501.702324	578542.759097	44.603738
3501.520868	578547.702297	44.608743
3501.729220	578514.619252	44.613748
3501.757608	578510.803142	44.618753
3501.647650	578498.382436	44.623757
3502.001151	578487.343687	44.628762
3501.870103	578470.863892	44.633767
3501.826995	578458.232080	44.638772
3501.938281	578422.104623	44.643777
3501.751671	578420.779581	44.648781
3501.742119	578411.703321	44.653786
3501.432232	578406.535777	44.658791
3501.879731	578386.354405	44.663796
3501.562678	578385.049751	44.668801
3501.631074	578361.416889	44.673805
3501.738402	578344.548570	44.678810
3501.725534	578348.211674	44.683815
3501.954490	578323.650875	44.688820
3501.935341	578310.212698	44.693825
3501.766101	578310.790753	44.698829
3501.783364	578288.218950	44.703834
3501.389320	578269.021532	44.708839
3501.799555	578255.315549	44.713844
3501.655804	578247.664435	44.718849
3501.602538	578226.557987	44.723853
3501.687184	578216.664383	44.728858
3501.636398	578212.409165	44.733863
3501.739269	578185.259777	44.738868
3501.764362	578182.798225	44.743873
3501.734751	578183.304305	44.748877
3501.793926	578154.556749	44.753882
3501.734460	578147.594546	44.758887
3501.172464	578138.002578	44.763892
3501.508081	578133.937694	44.768897
3501.338116	578118.516699	44.773901
3501.531107	578103.941718	44.778906
3501.461615	578106.560513	44.783911
3501.833459	578097.223757	44.788916
3502.026616	578077.081589	44.793921
3501.695088	578060.231294	44.798925
3501.765327	578053.850609	44.803930
3501.877455	578028.254181	44.808935
3501.671815	578021.364905	44.813940
3501.654743	578009.882072	44.818945
3501.415788	577989.355906	44.823949
3501.783580	577980.270460	44.828954
3501.342613	577979.887915	44.833959
3501.427676	577963.925289	44.838964
3501.186115	577944.252081	44.843969
3501.259820	577933.557458	44.848973
3501.480252	577941.748328	44.853978
3501.551268	577938.176134	44.858983
3502.068321	577934.183124	44.863988
3501.830461	577910.597187	44.868993
3501.853634	577899.759966	44.873997
3501.607675	577874.921339	44.879002
3501.550872	577865.250159	44.884007
3501.741304	577860.154612	44.889012
3501.836586	577853.418810	44.894017
3501.494364	577828.294197	44.899021
3501.639436	577815.331307	44.904026
3502.164102	577808.327731	44.909031
3501.854302	577786.407911	44.914036
3501.817579	577768.859065	44.919041
3501.559377	577761.526443	44.924045
3501.917703	577737.345380	44.929050
3501.762128	577736.767742	44.934055
3501.899408	577720.194736	44.939060
3501.950557	577711.860757	44.944065
3501.676794	577714.712202	44.949069
3502.049950	577683.557020	44.954074
3501.762990	577672.667749	44.959079
3501.999026	577660.994522	44.964084
3501.758316	577643.978931	44.969089
3501.129448	577625.920554	44.974093
3501.711831	577612.537971	44.979098
3501.523459	577625.206749	44.984103
3501.352434	577593.584668	44.989108
3501.540068	577586.232390	44.994113
3501.411702	577581.838590	44.999117
3501.626876	577572.626204	45.004122
3501.287511	577563.600815	45.009127
3501.741387	577544.620691	45.014132
3501.723767	577541.212698	45.019137
3501.598198	577543.439137	45.024141
3501.771435	577507.299041	45.029146
3502.000423	577509.720844	45.034151
3501.482557	577490.390972	45.039156
3501.483017	577468.271554	45.044161
3501.226996	577469.665731	45.049165
3501.175212	577461.297500	45.054170
3501.687025	577450.333298	45.059175
3501.741096	577452.732301	45.064180
3501.723008	577426.703441	45.069185
3501.336075	577418.588201	45.074189
3501.822710	577407.377107	45.079194
3501.566174	577397.586274	45.084199
3501.689445	577372.387865	45.089204
3501.727044	577372.833317	45.094209
3501.484978	577371.617132	45.099213
3501.627088	577353.237157	45.104218
3501.603322	577337.691913	45.109223
3501.943384	577322.992611	45.114228
3501.613181	577305.238129	45.119233
3501.170330	577297.282016	45.124237
3501.552877	577301.435383	45.129242
3501.214167	577298.077511	45.134247
3501.624762	577288.884501	45.139252
3502.052043	577264.641482	45.144257
3501.546972	577259.855023	45.149261
3501.798633	577245.721178	45.154266
3501.384211	577226.274360	45.159271
3501.452320	577215.429452	45.164276
3501.642100	577211.637828	45.169281
3501.590297	577201.564026	45.174285
3501.857691	577174.286151	45.179290
3501.555466	577174.734577	45.184295
3501.616981	577163.990967	45.189300
3501.903911	577139.518827	45.194305
3501.462635	577134.521707	45.199309
3501.781525	577117.668626	45.204314
3501.309274	577117.040143	45.209319
3501.574825	577101.298867	45.214324
3501.470957	577087.170242	45.219329
3501.444991	577089.983106	45.224333
3501.521961	577079.738587	45.229338
3501.144812	577067.759331	45.234343
3501.146498	577060.636414	45.239348
3501.480680	577061.185990	45.244353
3501.338790	577056.794098	45.249357
3501.503735	577042.472917	45.254362
3501.231992	577053.500126	45.259367
3501.545719	577029.525147	45.264372
3501.464281	577013.286242	45.269377
3501.383154	577001.661912	45.274381
3501.045598	576995.996444	45.279386
3501.425071	576998.444993	45.284391
3501.440642	576991.470340	45.289396
3501.550229	576965.721405	45.294401
3501.425828	576969.101440	45.299405
3501.716547	576957.117976	45.304410
3501.347366	576944.033836	45.309415
3501.693767	576922.762130	45.314420
3501.479988	576924.300248	45.319425
3501.501205	576921.738706	45.324429
3501.754486	576907.854980	45.329434
3501.486615	576883.218216	45.334439
3501.456264	576877.354184	45.339444
3501.594945	576875.426345	45.344449
3501.358407	576868.390708	45.349453
3501.504334	576844.993325	45.354458
3501.788422	576841.036353	45.359463
3501.747624	576839.487686	45.364468
3501.873095	576824.720959	45.369473
3501.399845	576799.915479	45.374477
3501.592614	576792.762520	45.379482
3501.481909	576793.181019	45.384487
3501.245558	576777.919033	45.389492
3501.540353	576765.633768	45.394497
3501.409221	576757.177096	45.399501
3501.375333	576754.022207	45.404506
3501.468017	576753.355545	45.409511
3501.689139	576739.225837	45.414516
3501.308221	576720.826271	45.419521
3500.977521	576715.410391	45.424525
3501.476154	576709.864860	45.429530
3501.567662	576718.528227	45.434535
3501.218698	576689.439433	45.439540
3501.336441	576678.786890	45.444545
3501.053840	576669.651581	45.449549
3501.321195	576663.389773	45.454554
3501.085187	576666.636863	45.459559
3501.220473	576666.264501	45.464564
3501.461088	576668.985634	45.469569
3501.680452	576651.395004	45.474573
3501.599075	576631.543963	45.479578
3501.373348	576627.315490	45.484583
3501.270540	576629.388068	45.489588
3501.136083	576619.727951	45.494593
3501.321600	576595.671768	45.499597
3501.699184	576583.574006	45.504602
3501.359943	576583.025018	45.509607
3501.212026	576581.091772	45.514612
3501.380892	576592.953451	45.519617
3501.567063	576578.929328	45.524621
3501.700081	576566.518653	45.529626
3501.362056	576551.322414	45.534631
3501.339691	576550.422920	45.539636
3501.505251	576547.086310	45.544641
3501.168722	576528.027391	45.549645
3501.037486	576508.434733	45.554650
3501.108429	576520.713088	45.559655
3501.165793	576506.056912	45.564660
3501.480567	576510.522140	45.569665
3501.461798	576512.029827	45.574669
3501.447863	576509.975301	45.579674
3501.309577	576488.778546	45.584679
3501.287296	576472.880742	45.589684
3501.038005	576474.775602	45.594689
3500.957487	576475.891654	45.599693
3501.117822	576469.044530	45.604698
3501.008410	576470.365746	45.609703
3501.361979	576465.294227	45.614708
3501.312226	576461.589959	45.619713
3501.017121	576445.182988	45.624717
3501.168663	576428.003905	45.629722
3501.358131	576428.325329	45.634727
3501.500522	576432.065111	45.639732
3501.730694	576426.009630	45.644737
3501.214458	576416.509345	45.649741
3501.646846	576401.242627	45.654746
3501.210844	576408.383519	45.659751
3501.156109	576391.086141	45.664756
3501.331471	576394.319162	45.669761
3501.259307	576394.430678	45.674765
3501.631319	576390.861100	45.679770
3501.484484	576369.314323	45.684775
3501.304279	576360.413564	45.689780
3501.572156	576350.489671	45.694785
3501.295571	576351.134766	45.699789
3501.420151	576330.297915	45.704794
3501.478698	576315.892118	45.709799
3501.286628	576315.019135	45.714804
3501.305032	576311.103513	45.719809
3500.979400	576315.618772	45.724813
3501.337337	576304.426702	45.729818
3501.519614	576304.297794	45.734823
3501.506854	576272.847894	45.739828
3501.482848	576209.797196	45.744833
3501.285230	576103.984162	45.749837
3501.242663	575944.570972	45.754842
3500.840295	575752.705054	45.759847
3500.339138	575503.662363	45.764852
3500.250835	575207.141731	45.769857
3499.485984	574880.015900	45.774861
3498.748694	574491.668592	45.779866
3498.107869	574077.905746	45.784871
3497.557144	573606.965310	45.789876
3496.864839	573096.388027	45.794881
3495.774239	572552.731977	45.799885
3494.986179	571958.871344	45.804890
3493.930247	571331.950191	45.809895
3492.736561	570656.886607	45.814900
3491.786450	569956.198211	45.819905
3490.627816	569202.344595	45.824909
3489.302617	568408.259701	45.829914
3487.710666	567591.119640	45.834919
3486.179948	566737.915651	45.839924
3485.001408	565821.582373	45.844929
3482.860403	564904.021692	45.849933
3481.552527	563941.967573	45.854938
3479.676165	562946.224980	45.859943
3478.082027	561918.209544	45.864948
3476.600616	560844.478034	45.869953
3474.514200	559749.946302	45.874957
3472.518335	558619.177227	45.879962
3470.367422	557466.217334	45.884967
3468.087318	556277.740555	45.889972
3466.412119	555071.060164	45.894977
3463.757562	553826.516187	45.899981
3461.301377	552565.627541	45.904986
3459.232293	551284.238040	45.909991
3457.210893	549969.474111	45.914996
3455.105518	548629.089403	45.920001
3451.994455	547270.511769	45.925005
3449.435066	545869.301898	45.930010
3447.077194	544468.103039	45.935015
3444.412374	543034.600039	45.940020
3442.058351	541595.349912	45.945025
3439.270650	540129.587129	45.950029
3436.650183	538641.687893	45.955034
3433.853747	537148.256537	45.960039
3430.610135	535625.728267	45.965044
3428.113074	534078.840219	45.970049
3425.169890	532533.900206	45.975053
3422.022446	530961.567753	45.980058
3419.313296	529388.322134	45.985063
3416.246171	527782.056057	45.990068
3412.917737	526170.094071	45.995073
3409.851203	524552.454161	46.000077
3406.885961	522919.839879	46.005082
3403.796531	521288.960586	46.010087
3400.604153	519633.912196	46.015092
3397.609428	517966.484119	46.020097
3393.896379	516297.149589	46.025101
3390.749173	514617.591917	46.030106
3387.835433	512922.012044	46.035111
3383.939476	511210.948430	46.040116
3380.606024	509494.543977	46.045121
3377.699818	507790.421873	46.050125
3374.310438	506058.879993	46.055130
3371.074613	504326.397051	46.060135
3367.363503	502595.242004	46.065140
3363.773069	500846.097603	46.070145
3360.141514	499102.653457	46.075149
3357.062597	497351.646530	46.080154
3353.202328	495590.002938	46.085159
3349.379925	493811.230978	46.090164
3346.341764	492047.170666	46.095169
3342.429096	490285.413108	46.100173
3338.990927	488516.254922	46.105178
3336.085776	486744.635788	46.110183
3332.220455	484961.949614	46.115188
3328.808123	483172.115790	46.120193
3324.999408	481383.805228	46.125197
3321.495950	479582.205209	46.130202
3317.779628	477802.972822	46.135207
3313.748385	476005.343969	46.140212
3310.742716	474209.223180	46.145217
3306.704541	472408.412659	46.150221
3303.124052	470612.740966	46.155226
3299.587373	468812.415577	46.160231
3295.804508	467017.495086	46.165236
3291.797855	465210.226565	46.170241
3287.882186	463420.756300	46.175245
3284.598461	461612.836339	46.180250
3280.563375	459815.112232	46.185255
3276.788988	458023.382530	46.190260
3273.152800	456226.435665	46.195265
3269.382154	454435.448197	46.200269
3265.372597	452638.899691	46.205274
3261.933682	450852.254170	46.210279
3257.986302	449056.346274	46.215284
3254.059419	447278.026921	46.220289
3250.129751	445490.672668	46.225293
3246.702622	443702.963946	46.230298
3242.932594	441920.807783	46.235303
3239.294536	440133.648609	46.240308
3235.736448	438350.510996	46.245313
3231.519030	436577.744154	46.250317
3227.467812	434789.030366	46.255322
3224.126071	433025.880169	46.260327
3220.306614	431250.533870	46.265332
3216.559607	429473.343035	46.270337
3212.758550	427717.337870	46.275341
3208.866923	425943.198679	46.280346
3205.257851	424190.351698	46.285351
3201.224344	422417.293888	46.290356
3197.676447	420647.859878	46.295361
3193.863506	418892.208715	46.300365
3189.833299	417133.198553	46.305370
3186.285379	415375.690323	46.310375
3182.584839	413628.356112	46.315380
3178.791128	411882.923064	46.320385
3174.991170	410130.147566	46.325389
3171.629726	408385.330377	46.330394
3167.517222	406630.143440	46.335399
3163.691191	404901.359477	46.340404
3159.958089	403165.426189	46.345409
3155.936618	401424.737108	46.350413
3152.329499	399682.785694	46.355418
3148.381247	397956.286936	46.360423
3144.460842	396228.286329	46.365428
3140.585930	394510.507425	46.370433
3136.745437	392796.356306	46.375437
3133.696830	391085.005852	46.380442
3129.688147	389357.591692	46.385447
3125.842421	387651.863756	46.390452
3122.358180	385932.049929	46.395457
3117.956703	384230.797084	46.400461
3114.093097	382523.125683	46.405466
3110.653707	380829.952276	46.410471
3106.606467	379120.815875	46.415476
3102.938464	377428.195018	46.420481
3099.159798	375748.157769	46.425485
3095.586507	374046.673251	46.430490
3092.041334	372371.825924	46.435495
3088.393539	370694.352690	46.440500
3084.368826	369010.130809	46.445505
3080.545041	367321.178592	46.450509
3076.908378	365642.895499	46.455514
3072.939927	363980.803237	46.460519
3068.994669	362309.084110	46.465524
3065.572236	360640.695768	46.470529
3061.522707	358987.306516	46.475533
3058.481285	357323.122608	46.480538
3054.340946	355659.401784	46.485543
3050.909261	354009.333740	46.490548
3046.832153	352346.621925	46.495553
3042.858337	350701.194730	46.500557
3039.616243	349057.120262	46.505562
3035.733749	347404.343744	46.510567
3031.805486	345758.026215	46.515572
3028.149007	344111.331624	46.520577
3024.528589	342478.841639	46.525581
3020.892819	340851.998397	46.530586
3016.950358	339213.100236	46.535591
3013.511412	337584.525109	46.540596
3009.402581	335952.472068	46.545601
3005.685997	334333.993009	46.550605
3002.310976	332704.250677	46.555610
2998.857771	331073.560257	46.560615
2994.682617	329460.107752	46.565620
2991.314866	327835.473908	46.570625
2987.450364	326236.212128	46.575629
2983.999753	324609.730491	46.580634
2980.109709	322996.684918	46.585639
2976.242440	321387.872710	46.590644
2972.625235	319786.287334	46.595649
2968.770781	318181.804559	46.600653
2965.392152	316579.249509	46.605658
2961.629227	314986.060324	46.610663
2957.567066	313385.254019	46.615668
2954.258896	311783.205635	46.620673
2950.552446	310202.005708	46.625677
2946.898076	308611.635349	46.630682
2943.265983	307028.207995	46.635687
2939.305862	305433.914903	46.640692
2935.455979	303855.918734	46.645697
2931.628783	302278.838094	46.650701
2928.409704	300699.808293	46.655706
2924.495263	299118.423128	46.660711
2920.790510	297546.606416	46.665716
2917.171074	295979.135969	46.670721
2913.510352	294413.538390	46.675725
2909.913660	292836.587277	46.680730
2906.073313	291285.368463	46.685735
2902.513817	289721.338704	46.690740
2899.066302	288163.082313	46.695745
2895.166450	286605.342866	46.700749
2891.455969	285042.954850	46.705754
2887.931084	283492.136504	46.710759
2884.051199	281939.378961	46.715764
2880.450360	280381.706922	46.720769
2876.631218	278839.134021	46.725773
2872.768646	277289.713182	46.730778
2869.395370	275745.200995	46.735783
2865.377629	274204.808422	46.740788
2862.013792	272659.141747	46.745793
2858.199252	271133.505797	46.750797
2854.759611	269600.680854	46.755802
2850.998985	268065.818005	46.760807
2847.344413	266537.228810	46.765812
2843.452070	265014.942750	46.770817
2839.667558	263492.769988	46.775821
2835.865731	261972.386179	46.780826
2832.352174	260460.645528	46.785831
2828.684032	258950.539083	46.790836
2825.640890	257439.653903	46.795841
2821.265426	255930.359674	46.800845
2818.041508	254409.331902	46.805850
2814.217997	252900.376120	46.810855
2810.685903	251400.654707	46.815860
2807.157199	249894.322311	46.820865
2803.264249	248400.512141	46.825869
2799.452687	246895.343457	46.830874
2795.949312	245393.629058	46.835879
2792.300232	243898.446059	46.840884
2788.890523	242407.876021	46.845889
2784.789403	240923.771792	46.850893
2781.415358	239429.128749	46.855898
2777.900964	237947.692544	46.860903
2774.452790	236465.194879	46.865908
2771.068694	234972.009684	46.870913
2767.048819	233494.072510	46.875917
2763.200180	232004.923227	46.880922
2759.616920	230526.527547	46.885927
2755.685285	229045.611091	46.890932
2752.258501	227570.878953	46.895937
2748.244209	226107.953163	46.900941
2744.842071	224644.217981	46.905946
2741.047699	223169.287072	46.910951
2737.488427	221715.205031	46.915956
2734.034896	220247.889808	46.920961
2730.254038	218795.120168	46.925965
2726.478356	217333.922786	46.930970
2723.220040	215876.290590	46.935975
2719.533534	214419.519696	46.940980
2716.118620	212960.929077	46.945985
2712.344332	211510.678248	46.950989
2708.520341	210047.962700	46.955994
2704.575254	208614.817106	46.960999
2700.988286	207165.731724	46.966004
2697.766865	205718.814096	46.971009
2694.071923	204281.887403	46.976013
2690.338154	202835.070443	46.981018
2686.879035	201401.948818	46.986023
2683.084534	199976.200620	46.991028
2679.636663	198530.470157	46.996033
2676.342996	197102.173803	47.001037
2672.416628	195666.248616	47.006042
2668.608130	194233.604978	47.011047
2664.643660	192811.747818	47.016052
2661.534668	191383.839370	47.021057
2657.633170	189958.847412	47.026061
2654.347125	188535.380951	47.031066
2650.350055	187123.884861	47.036071
2646.790596	185697.034851	47.041076
2643.654186	184270.876763	47.046081
2639.451590	182863.748757	47.051085
2635.949515	181445.073254	47.056090
2632.478213	180029.266275	47.061095
2628.714494	178630.612376	47.066100
2625.460044	177214.688824	47.071105
2621.616982	175811.840741	47.076109
2618.298619	174398.164316	47.081114
2614.322767	172996.454721	47.086119
2610.751400	171589.907693	47.091124
2607.051197	170191.171940	47.096129
2603.805329	168787.681483	47.101133
2599.744943	167393.447071	47.106138
2596.280369	165994.500825	47.111143
2592.562439	164603.272562	47.116148
2588.913873	163209.783719	47.121153
2585.263076	161825.272651	47.126157
2581.578984	160438.950941	47.131162
2578.361684	159056.684989	47.136167
2574.281357	157678.492267	47.141172
2570.814501	156291.351411	47.146177
2566.889471	154914.559777	47.151181
2563.453602	153530.011939	47.156186
2559.840607	152150.094143	47.161191
2556.208059	150781.246818	47.166196
2552.790193	149412.819984	47.171201
2548.843131	148045.859539	47.176205
2545.807948	146650.949570	47.181210
2542.006561	145234.259661	47.186215
2537.947493	143875.773686	47.191220
2534.643668	142513.529115	47.196225
2530.999212	141160.587244	47.201229
2527.558011	139809.597896	47.206234
2523.749315	138444.009328	47.211239
2520.068234	137094.114492	47.216244
2516.722193	135738.125413	47.221249
2512.716265	134392.253664	47.226253
2509.198587	133041.028325	47.231258
2505.677668	131690.811507	47.236263
2502.043069	130354.672271	47.241268
2498.572331	129008.105657	47.246273
2494.650147	127674.842766	47.251277
2491.276302	126334.375609	47.256282
2487.753011	125000.576483	47.261287
2483.595450	123665.355891	47.266292
2480.090407	122335.317453	47.271297
2476.488004	121018.412591	47.276301
2472.546534	119681.893390	47.281306
2469.256757	118364.253736	47.286311
2465.307042	117056.300046	47.291316
2462.361234	115731.564166	47.296321
2458.689173	114419.920597	47.301325
2455.285250	113103.043265	47.306330
2451.885961	111790.497685	47.311335
2447.800462	110470.491667	47.316340
2444.395121	109160.840723	47.321345
2440.561167	107846.843368	47.326349
2436.945611	106545.955569	47.331354
2433.485793	105240.795991	47.336359
2429.661905	103930.620730	47.341364
2425.934334	102618.371458	47.346369
2422.264172	101328.078171	47.351373
2418.593129	100034.950457	47.356378
2415.413900	98745.724480	47.361383
2411.123462	97456.787490	47.366388
2407.879256	96162.109055	47.371393
2404.117901	94885.089093	47.376397
2400.395780	93602.625533	47.381402
2396.601962	92333.225667	47.386407
2392.926823	91055.575199	47.391412
2389.722245	89774.334552	47.396417
2385.746056	88505.580803	47.401421
2382.017618	87239.230905	47.406426
2378.806843	85979.079537	47.411431
2374.644163	84713.630687	47.416436
2371.305612	83450.966459	47.421441
2367.413874	82197.615669	47.426445
2364.023583	80947.277487	47.431450
2360.694206	79693.606626	47.436455
2356.818240	78459.522723	47.441460
2352.984780	77205.636407	47.446465
2349.398326	75975.047490	47.451469
2345.966961	74733.098680	47.456474
2342.072052	73493.844630	47.461479
2338.313698	72267.743682	47.466484
2335.081944	71020.183575	47.471489
2331.403556	69803.955021	47.476493
2327.849384	68572.642330	47.481498
2324.190732	67354.119196	47.486503
2320.733189	66134.441672	47.491508
2317.123146	64905.712599	47.496513
2313.627275	63701.467325	47.501517
2309.618134	62468.229009	47.506522
2305.828847	61263.512238	47.511527
2302.374558	60058.509770	47.516532
2298.290355	58856.793368	47.521537
2294.510658	57658.572157	47.526541
2290.864162	56469.723002	47.531546
2287.430373	55273.349100	47.536551
2283.609459	54088.319038	47.541556
2280.006230	52900.535449	47.546561
2276.460280	51730.946122	47.551565
2272.381595	50548.113915	47.556570
2268.838324	49385.638804	47.561575
2265.209227	48218.205859	47.566580
2261.660450	47051.904435	47.571585
2257.952849	45897.103604	47.576589
2254.409610	44736.082990	47.581594
2250.291801	43582.365568	47.586599
2246.367526	42437.751831	47.591604
2242.906538	41299.028101	47.596609
2239.377719	40164.856639	47.601613
2235.052011	39033.062352	47.606618
2231.159853	37912.892868	47.611623
2227.787155	36800.111135	47.616628
2224.165019	35689.074263	47.621633
2220.000625	34581.983383	47.626637
2216.072755	33487.615775	47.631642
2212.325925	32402.124810	47.636647
2208.362591	31327.080065	47.641652
2204.472428	30265.705141	47.646657
2200.494988	29191.964409	47.651661
2196.449479	28146.711486	47.656666
2191.843990	27115.489352	47.661671
2187.732251	26086.181003	47.666676
2183.124781	25087.111126	47.671681
2177.901449	24120.860272	47.676685
2172.672845	23164.159834	47.681690
2167.660718	22247.262148	47.686695
2162.778047	21353.635281	47.691700
2157.916773	20482.868768	47.696705
2153.283027	19648.774247	47.701709
2148.485441	18823.481733	47.706714
2144.186037	18024.798544	47.711719
2139.643151	17249.569490	47.716724
2135.427030	16488.674608	47.721729
2130.859621	15754.276470	47.726733
2126.596460	15046.747718	47.731738
2122.520297	14354.201779	47.736743
2118.630409	13681.528950	47.741748
2114.816030	13001.734917	47.746753
2110.856090	12355.645117	47.751757
2107.048765	11720.950493	47.756762
2103.024691	11094.380569	47.761767
2098.993231	10484.923894	47.766772
2095.530098	9886.119734	47.771777
2091.301343	9286.764456	47.776781
2087.640002	8715.875103	47.781786
2084.037170	8138.059073	47.786791
2079.845461	7588.503909	47.791796
2076.046955	7043.958122	47.796801
2071.626061	6528.099009	47.801805
2067.198449	6023.288146	47.806810
2062.632865	5538.840177	47.811815
2057.353554	5087.163828	47.816820
2052.762653	4637.808712	47.821825
2048.082768	4225.124182	47.826829
2043.599311	3830.072975	47.831834
2039.356538	3451.963518	47.836839
2035.004158	3100.250905	47.841844
2030.817982	2746.936970	47.846849
2026.723257	2422.074855	47.851853
2022.706163	2109.584763	47.856858
2019.175121	1813.474400	47.861863
2015.238729	1525.092599	47.866868
2011.621474	1247.638385	47.871873
2007.747178	980.318660	47.876877
2003.657821	720.978086	47.881882
1999.875942	482.879913	47.886887
1995.755903	257.537585	47.891892
1987.974286	133.276624	47.896897
1975.844176	165.234332	47.901901
1968.189544	170.488082	47.906906
1964.062026	171.633750	47.911911
1961.199686	169.347990	47.916916
1959.410225	163.126204	47.921921
1957.475905	163.742018	47.926925
1955.288709	161.429712	47.931930
1953.137241	172.925181	47.936935
1950.447299	175.228506	47.941940
1947.762965	168.979066	47.946945
1944.892724	163.476914	47.951949
1940.780616	168.027644	47.956954
1937.448377	160.205920	47.961959
1933.628718	170.994294	47.966964
1930.735618	163.587922	47.971969
1927.155585	167.248615	47.976973
1924.137387	174.064339	47.981978
1921.435709	169.010393	47.986983
1918.004648	170.445740	47.991988
1914.681699	166.827323	47.996993
1911.222064	161.192780	48.001997
1907.196196	168.011161	48.007002
1904.659622	163.598957	48.012007
1900.656113	164.440497	48.017012
1897.422545	159.922224	48.022017
1894.568915	162.368237	48.027021
1890.926910	167.098528	48.032026
1888.040219	158.004840	48.037031
1884.116801	166.221435	48.042036
1880.873162	157.708805	48.047041
1877.022650	162.648904	48.052045
1872.878254	159.636789	48.057050
1870.479051	159.354066	48.062055
1866.762310	163.058317	48.067060
1863.271235	160.924763	48.072065
1860.048328	165.646428	48.077069
1856.839747	161.703242	48.082074
1853.616790	157.208635	48.087079
1849.807770	154.969812	48.092084
1846.935913	155.393829	48.097089
1843.034906	155.785903	48.102093
1839.351367	161.509828	48.107098
1836.374147	149.434168	48.112103
1832.527020	160.919743	48.117108
1829.029607	160.935443	48.122113
1825.229069	157.761967	48.127117
1821.831631	162.555249	48.132122
1819.076377	164.849841	48.137127
1815.572848	156.801863	48.142132
1812.435216	156.283525	48.147137
1808.558434	165.714088	48.152141
1804.527080	156.774251	48.157146
1801.150747	160.232257	48.162151
1797.881565	149.198913	48.167156
1794.791169	145.512511	48.172161
1791.558815	152.659173	48.177165
1787.704843	157.878259	48.182170
1784.163989	150.763144	48.187175
1780.288339	159.848676	48.192180
1777.322907	155.278992	48.197185
1773.375989	149.401215	48.202189
1769.962416	156.174436	48.207194
1767.433701	154.083304	48.212199
1763.681398	160.415979	48.217204
1760.000891	160.292672	48.222209
1756.270672	152.545959	48.227213
1752.655676	158.224380	48.232218
1749.233387	155.453660	48.237223
1746.173722	164.354555	48.242228
1742.460122	157.143099	48.247233
1739.020991	154.685075	48.252237
1735.371604	152.829450	48.257242
1732.047541	153.814663	48.262247
1728.279474	151.904845	48.267252
1725.034234	156.645860	48.272257
1721.573018	160.047569	48.277261
1718.034243	152.761306	48.282266
1715.035696	153.553208	48.287271
1711.321678	156.070643	48.292276
1708.118990	152.281616	48.297281
1704.219409	145.963015	48.302285
1700.287361	151.150053	48.307290
1696.944742	140.688249	48.312295
1693.880195	151.823583	48.317300
1690.355399	152.090395	48.322305
1686.876675	154.080617	48.327309
1683.073143	163.831955	48.332314
1679.671857	146.842841	48.337319
1676.158288	150.195807	48.342324
1672.769248	152.573806	48.347329
1669.203420	147.500160	48.352333
1665.915122	152.947136	48.357338
1662.335717	150.640812	48.362343
1658.651578	154.472908	48.367348
1655.397571	159.924014	48.372353
1652.304766	148.461319	48.377357
1648.279476	155.937768	48.382362
1645.132217	147.773991	48.387367
1641.163854	156.136900	48.392372
1638.082075	151.556997	48.397377
1633.858359	149.149039	48.402381
1630.630885	150.688657	48.407386
1628.073023	150.693421	48.412391
1623.855107	152.210881	48.417396
1620.549926	148.817587	48.422401
1617.337947	148.285635	48.427405
1613.005880	156.132822	48.432410
1609.932601	147.486068	48.437415
1605.960392	150.211631	48.442420
1602.641018	143.821249	48.447425
1599.645339	149.133856	48.452429
1596.089951	151.186728	48.457434
1592.782565	143.161934	48.462439
1588.965579	143.556772	48.467444
1585.795710	144.426146	48.472449
1582.208844	148.163946	48.477453
1578.345635	151.150877	48.482458
1574.991892	144.440009	48.487463
1571.419744	148.912682	48.492468
1568.132983	142.311560	48.497473
1564.344864	141.585055	48.502477
1560.998286	146.905136	48.507482
1557.524325	135.960900	48.512487
1553.626696	143.955247	48.517492
1550.682020	141.941934	48.522497
1547.107148	139.755171	48.527501
1543.538741	149.801943	48.532506
1540.433460	130.823986	48.537511
1536.745905	145.843968	48.542516
1532.777348	141.067536	48.547521
1529.352324	148.035606	48.552525
1525.961506	145.415070	48.557530
1522.893429	136.739066	48.562535
1519.206709	139.926188	48.567540
1515.449480	146.993716	48.572545
1511.816016	143.648681	48.577549
1508.372545	142.453791	48.582554
1505.276508	141.881581	48.587559
1501.439802	149.572174	48.592564
1498.238260	140.951869	48.597569
1494.891349	138.732608	48.602573
1491.527801	143.568133	48.607578
1487.617384	136.912797	48.612583
1483.961106	140.474826	48.617588
1480.560761	146.755658	48.622593
1477.109294	137.139910	48.627597
1473.540440	146.626771	48.632602
1470.440161	137.895714	48.637607
1466.831083	144.342103	48.642612
1462.881028	147.560972	48.647617
1459.713945	140.276754	48.652621
1456.009241	141.138133	48.657626
1452.556849	139.381498	48.662631
1449.071548	147.890319	48.667636
1445.756119	141.274748	48.672641
1442.046676	138.742084	48.677645
1438.676740	146.438728	48.682650
1435.321948	138.196787	48.687655
1431.244525	149.696367	48.692660
1428.046716	145.732665	48.697665
1424.432981	148.747040	48.702669
1421.204822	149.606606	48.707674
1417.702003	137.698816	48.712679
1414.162865	145.048620	48.717684
1410.473636	142.496984	48.722689
1407.034730	136.014657	48.727693
1403.555018	143.956289	48.732698
1400.327036	136.061517	48.737703
1396.582703	142.835990	48.742708
1393.138846	134.212531	48.747713
1389.703014	145.893272	48.752717
1385.996053	136.551681	48.757722
1382.653880	143.196766	48.762727
1379.059442	149.773772	48.767732
1375.722525	149.153885	48.772737
1372.021265	141.428122	48.777741
1368.675908	148.861505	48.782746
1365.200473	133.165515	48.787751
1361.233061	143.970833	48.792756
1358.117151	138.858523	48.797761
1355.024984	134.666336	48.802765
1351.277091	139.008396	48.807770
1347.603395	133.977078	48.812775
1344.025706	137.618602	48.817780
1340.966940	135.196099	48.822785
1336.922085	140.097190	48.827789
1333.711804	139.454331	48.832794
1330.027020	142.138166	48.837799
1326.545518	136.447168	48.842804
1323.360030	137.002685	48.847809
1319.583367	138.381590	48.852813
1316.111877	143.645363	48.857818
1312.677954	138.576523	48.862823
1309.009145	137.239805	48.867828
1305.602588	132.011658	48.872833
1302.272513	137.797474	48.877837
1298.665367	135.539925	48.882842
1295.163427	135.581829	48.887847
1291.524434	135.180106	48.892852
1288.039091	130.729946	48.897857
1284.670787	123.863289	48.902861
1281.093822	121.373230	48.907866
1277.978095	127.837354	48.912871
1274.024483	127.807600	48.917876
1270.592640	134.232628	48.922881
1266.715483	139.376418	48.927885
1263.368418	142.475654	48.932890
1260.348043	128.211299	48.937895
1256.302829	133.590212	48.942900
1252.957538	138.226792	48.947905
1249.811608	143.882554	48.952909
1245.905211	145.360892	48.957914
1242.286308	134.135762	48.962919
1239.041445	136.244547	48.967924
1235.562148	134.008138	48.972929
1232.266125	140.801067	48.977933
1228.599272	141.045986	48.982938
1224.908132	130.512396	48.987943
1221.158250	135.873563	48.992948
1218.199150	131.787146	48.997953
1214.636168	136.432506	49.002957
1211.183771	139.855139	49.007962
1208.044248	134.854151	49.012967
1203.768296	140.038248	49.017972
1200.704094	138.923301	49.022977
1197.074258	126.184437	49.027981
1193.623376	143.552968	49.032986
1190.247195	137.481697	49.037991
1186.379724	147.012223	49.042996
1183.375020	137.753776	49.048001
1179.640327	138.407975	49.053005
1175.715602	142.189310	49.058010
1172.680658	128.658117	49.063015
1168.915729	135.451704	49.068020
1165.527809	136.016817	49.073025
1162.137824	135.221811	49.078029
1158.213817	129.628635	49.083034
1155.382203	127.505998	49.088039
1151.422410	135.146363	49.093044
1147.820429	127.503242	49.098049
1144.291017	129.536380	49.103053
1140.914867	128.068487	49.108058
1137.622639	122.167600	49.113063
1134.295550	136.115651	49.118068
1130.876150	131.867205	49.123073
1127.247830	123.782120	49.128077
1123.250085	138.205340	49.133082
1120.120266	129.456902	49.138087
1116.453894	134.102661	49.143092
1113.093306	130.446141	49.148097
1109.341514	126.974260	49.153101
1105.644292	126.939236	49.158106
1102.939452	125.185917	49.163111
1099.261299	132.048199	49.168116
1095.494113	117.233283	49.173121
1091.638647	125.768510	49.178125
1088.195750	129.471274	49.183130
1085.144508	130.499406	49.188135
1081.268869	131.533221	49.193140
1078.161656	121.522066	49.198145
1074.805012	130.210161	49.203149
1071.083632	130.226390	49.208154
1067.700162	120.441993	49.213159
1064.018422	128.013542	49.218164
1060.280905	123.663069	49.223169
1056.866216	132.749409	49.228173
1053.250428	129.404956	49.233178
1050.047018	121.867160	49.238183
1046.246309	124.265517	49.243188
1042.699391	127.402440	49.248193
1039.790717	117.277958	49.253197
1036.223859	118.750673	49.258202
1032.679858	119.422529	49.263207
1028.995915	129.667859	49.268212
1025.568663	124.034934	49.273217
1022.116769	124.309551	49.278221
1018.340514	123.211238	49.283226
1014.997413	120.586587	49.288231
1011.380403	120.763672	49.293236
1007.979063	125.051588	49.298241
1004.242041	124.383744	49.303245
1000.826741	126.263021	49.308250
997.635051	128.822310	49.313255
993.715015	120.415959	49.318260
990.215531	118.372635	49.323265
986.875644	121.885292	49.328269
983.187602	130.384852	49.333274
980.256836	117.093709	49.338279
976.677933	122.817334	49.343284
973.152585	113.687960	49.348289
969.521217	124.719190	49.353293
965.621471	127.202689	49.358298
962.346520	120.046297	49.363303
958.923062	131.060798	49.368308
955.294965	119.277258	49.373313
951.798897	117.771262	49.378317
948.259793	122.827428	49.383322
944.898403	122.534234	49.388327
941.194839	117.134440	49.393332
937.794552	112.661616	49.398337
934.647567	119.500890	49.403341
931.011043	118.997677	49.408346
927.378373	116.943593	49.413351
924.119902	118.969186	49.418356
920.496971	120.501344	49.423361
916.875080	105.448641	49.428365
913.285079	121.864541	49.433370
910.142864	112.618256	49.438375
906.047711	115.739826	49.443380
902.617105	112.420227	49.448385
899.714905	115.804265	49.453389
895.727237	123.857211	49.458394
892.380444	115.933801	49.463399
889.122900	117.247402	49.468404
885.156433	121.620683	49.473409
881.751554	124.798696	49.478413
878.068523	122.847432	49.483418
875.147737	121.517145	49.488423
871.425389	120.132035	49.493428
867.973207	119.419644	49.498433
864.477149	119.663268	49.503437
860.578882	129.312610	49.508442
856.997653	118.157705	49.513447
853.826341	125.858205	49.518452
850.433503	114.629513	49.523457
847.232360	124.119074	49.528461
843.133076	126.469348	49.533466
839.816956	117.047838	49.538471
835.862603	126.259872	49.543476
832.790313	136.203837	49.548481
829.412688	128.392845	49.553485
825.900475	134.767316	49.558490
822.617567	115.422064	49.563495
818.485110	124.263353	49.568500
815.099816	118.510050	49.573505
811.807569	117.554332	49.578509
807.643579	126.678979	49.583514
804.844489	116.088170	49.588519
801.307490	122.362121	49.593524
798.129615	118.079154	49.598529
794.581872	114.464723	49.603533
790.520022	123.045024	49.608538
787.182274	116.271869	49.613543
783.640950	120.641890	49.618548
780.230118	119.628822	49.623553
776.856218	115.832149	49.628557
773.163058	126.199222	49.633562
769.837448	120.249926	49.638567
766.410656	125.180995	49.643572
762.641775	123.097687	49.648577
759.513084	125.112503	49.653581
755.703792	124.554154	49.658586
752.418986	115.633989	49.663591
748.894340	119.925478	49.668596
745.418590	127.173801	49.673601
741.898035	125.896351	49.678605
737.970529	120.139404	49.683610
734.731337	117.327742	49.688615
731.547769	128.500892	49.693620
727.913969	117.933260	49.698625
724.264449	114.429711	49.703629
720.264382	120.776206	49.708634
717.212221	120.478962	49.713639
713.605400	124.843446	49.718644
710.438901	121.257931	49.723649
706.569411	122.389012	49.728653
702.878524	116.854459	49.733658
699.801938	121.876241	49.738663
695.838701	117.887150	49.743668
692.712658	117.145896	49.748673
689.247539	107.039100	49.753677
685.710520	120.485435	49.758682
682.546626	110.005594	49.763687
678.506446	118.307288	49.768692
674.942510	117.837102	49.773697
671.581190	118.907597	49.778701
668.351061	117.125942	49.783706
664.933190	109.447885	49.788711
661.193628	117.281721	49.793716
657.742807	119.014817	49.798721
654.317290	116.251349	49.803725
650.267081	117.182962	49.808730
647.266114	113.581040	49.813735
643.320049	120.767006	49.818740
639.986212	114.581769	49.823745
636.868349	118.803262	49.828749
633.269131	116.696603	49.833754
629.716092	110.893720	49.838759
626.212573	123.287608	49.843764
622.332463	118.231986	49.848769
619.275171	120.264138	49.853773
615.519845	119.887225	49.858778
611.961378	112.474823	49.863783
608.385030	119.036577	49.868788
605.000171	109.939156	49.873793
601.824665	122.053885	49.878797
597.762805	123.522028	49.883802
594.485118	116.151080	49.888807
590.754929	112.850052	49.893812
587.722383	119.437377	49.898817
584.383117	111.383207	49.903821
580.506977	115.290036	49.908826
577.422693	106.224649	49.913831
573.589452	122.352856	49.918836
570.114141	114.481352	49.923841
566.753111	120.911320	49.928845
563.089107	122.911961	49.933850
559.440329	116.080046	49.938855
556.051926	120.052867	49.943860
552.323762	119.317381	49.948865
549.250575	112.999608	49.953869
545.540428	120.091712	49.958874
542.016482	115.761804	49.963879
538.448980	111.040082	49.968884
534.854372	120.281297	49.973889
531.371679	115.875329	49.978893
528.052122	119.290039	49.983898
524.354854	115.167622	49.988903
520.658943	118.780487	49.993908
517.326935	127.056751	49.998913
514.080634	117.583320	50.003917
510.752182	111.884519	50.008922
507.341824	109.479411	50.013927
503.522249	110.238921	50.018932
500.071664	118.533758	50.023937
496.770435	111.261455	50.028941
492.969314	118.041954	50.033946
489.067363	112.762024	50.038951
485.699449	110.824845	50.043956
482.285672	108.613274	50.048961
478.871185	104.506701	50.053965
475.341158	117.100934	50.058970
472.101644	108.543966	50.063975
468.503255	109.098001	50.068980
465.119236	114.743814	50.073985
461.629147	108.931146	50.078989
458.111112	112.544647	50.083994
454.733592	107.056041	50.088999
450.874554	115.800852	50.094004
447.367162	118.052258	50.099009
444.137044	111.382617	50.104013
440.557832	113.683239	50.109018
436.950510	109.220903	50.114023
433.210496	116.108912	50.119028
429.870623	112.607611	50.124033
426.436438	109.586162	50.129037
423.006312	115.096840	50.134042
419.439355	112.336639	50.139047
415.993943	109.383393	50.144052
412.290056	116.512527	50.149057
409.166137	110.455862	50.154061
404.866131	122.281699	50.159066
401.798697	105.873736	50.164071
398.625643	112.786846	50.169076
395.055130	107.942271	50.174081
391.335084	104.614434	50.179085
387.597587	105.854687	50.184090
384.616441	99.408672	50.189095
380.852762	113.352503	50.194100
377.280928	104.505943	50.199105
374.137628	109.364259	50.204109
370.326654	113.577342	50.209114
366.905452	111.582118	50.214119
363.243468	120.672588	50.219124
359.778252	112.748978	50.224129
356.526613	108.892196	50.229133
352.690222	118.924325	50.234138
349.373594	113.533792	50.239143
345.348635	112.825902	50.244148
341.892851	115.857048	50.249153
338.475992	108.106212	50.254157
335.582534	111.881352	50.259162
332.478731	105.603266	50.264167
328.573144	117.231302	50.269172
324.586924	116.713508	50.274177
321.488482	108.431904	50.279181
317.762224	106.395900	50.284186
314.590965	109.236950	50.289191
311.372162	114.376037	50.294196
307.465568	109.343699	50.299201
304.217658	105.571777	50.304205
300.139213	115.240037	50.309210
296.475355	107.850619	50.314215
293.056088	106.513191	50.319220
289.701375	106.611506	50.324225
286.088303	104.010449	50.329229
282.535610	119.354462	50.334234
279.366434	103.092215	50.339239
275.839575	114.844439	50.344244
272.232120	106.459094	50.349249
268.964397	109.176065	50.354253
265.316376	116.976714	50.359258
262.078374	108.096894	50.364263
257.947083	109.196408	50.369268
254.707435	116.082028	50.374273
251.435203	101.598174	50.379277
247.806119	104.352777	50.384282
244.492651	104.163070	50.389287
240.640732	108.496514	50.394292
236.765523	104.449562	50.399297
233.422246	103.780469	50.404301
230.025913	102.116767	50.409306
226.905357	102.703613	50.414311
223.012700	106.869437	50.419316
219.927381	107.112239	50.424321
216.560979	106.529033	50.429325
212.954211	114.633289	50.434330
209.755880	105.573271	50.439335
205.589778	106.912383	50.444340
201.910901	100.335297	50.449345
198.649515	105.398830	50.454349
194.915874	102.269366	50.459354
191.951544	107.134503	50.464359
188.205841	107.376367	50.469364
184.667553	99.423163	50.474369
181.198195	100.169073	50.479373
177.241733	103.436904	50.484378
173.871208	112.374204	50.489383
170.827506	106.627777	50.494388
167.244366	106.695484	50.499393
163.873991	101.746894	50.504397
160.060848	105.052391	50.509402
156.593141	97.591187	50.514407
153.110900	109.032730	50.519412
149.625476	112.176158	50.524417
146.107893	98.740047	50.529421
142.252209	112.593959	50.534426
139.260528	94.468986	50.539431
135.880919	103.822173	50.544436
132.220563	107.445435	50.549441
128.580946	104.661942	50.554445
125.280005	113.085313	50.559450
121.937911	114.766773	50.564455
118.113944	112.657578	50.569460
114.231095	101.164326	50.574465
111.065367	104.324120	50.579469
107.540961	107.230059	50.584474
103.972115	103.565448	50.589479
100.769686	103.959518	50.594484
97.019924	99.576602	50.599489
93.451581	97.224890	50.604493
90.421931	107.915329	50.609498
87.026918	105.647195	50.614503
83.024445	96.377864	50.619508
79.517476	100.147958	50.624513
76.219143	102.034551	50.629517
72.470676	105.016737	50.634522
69.329778	92.246160	50.639527
65.332877	105.780529	50.644532
62.044944	109.851675	50.649537
58.790690	101.524996	50.654541
54.728565	113.111210	50.659546
51.232268	104.496584	50.664551
47.777312	105.237127	50.669556
44.943026	105.624159	50.674561
41.359794	97.494566	50.679565
37.908366	100.961742	50.684570
34.307002	101.294954	50.689575
30.601243	106.184555	50.694580
26.920635	111.472019	50.699585
23.586531	100.380063	50.704589
19.842158	94.015812	50.709594
16.133950	101.579198	50.714599
12.723043	103.736556	50.719604
9.299340	105.475136	50.724609
6.327941	104.058160	50.729613
2.390154	101.153762	50.734618