Thu Aug 25 09:28:58 2022

Number of Points = 9924

Depth (nm)	Load (N)	Time (s)
1.910604	106.841792	0.000000
2.053343	98.410057	0.005005
1.810913	102.747616	0.010010
1.960107	93.909908	0.015014
1.973942	92.775088	0.020019
1.681601	86.123138	0.025024
1.455265	78.537023	0.030029
1.073424	68.070922	0.035034
0.988795	65.094391	0.040038
0.808768	52.850270	0.045043
0.274100	51.396429	0.050048
0.416799	54.253096	0.055053
-0.168341	36.035966	0.060058
-0.354462	38.570825	0.065062
-0.384188	28.837359	0.070067
-1.354704	22.525809	0.075072
-1.460332	15.414358	0.080077
-1.509251	15.611834	0.085082
-1.773875	9.588325	0.090086
-2.186103	3.856865	0.095091
-2.676054	9.565132	0.100096
-2.712018	2.822423	0.105101
-2.833371	1.294337	0.110106
-3.149584	4.457018	0.115110
-3.666970	-3.513732	0.120115
-4.252037	0.567438	0.125120
-3.829323	-4.728524	0.130125
-3.933523	-9.087708	0.135130
-4.241275	1.733137	0.140134
-4.711320	-5.197822	0.145139
-5.336720	15.743087	0.150144
-4.964778	3.766860	0.155149
-5.463384	8.258430	0.160154
-6.224779	3.698491	0.165158
-6.420442	2.906551	0.170163
-6.789949	10.918156	0.175168
-6.592454	2.044451	0.180173
-6.698840	5.509617	0.185178
-6.538234	4.876993	0.190182
-6.395099	-6.512881	0.195187
-7.613375	5.899635	0.200192
-7.810421	9.170197	0.205197
-8.250445	3.006493	0.210202
-8.257035	6.933752	0.215206
-8.387424	4.945170	0.220211
-9.363871	4.104722	0.225216
-9.620216	6.979611	0.230221
-9.488186	1.843089	0.235226
-9.930377	3.468933	0.240230
-9.524755	3.876766	0.245235
-9.828481	10.542952	0.250240
-9.813159	8.588487	0.255245
-10.494079	6.515320	0.260250
-11.099318	11.314666	0.265254
-10.985719	2.941327	0.270259
-11.149260	1.293300	0.275264
-11.368417	0.505042	0.280269
-12.110216	2.497370	0.285274
-12.478557	-3.443444	0.290278
-12.737550	-2.592954	0.295283
-12.797251	6.670417	0.300288
-12.863084	7.503298	0.305293
-12.506285	3.366111	0.310298
-12.931450	13.205607	0.315302
-13.618174	8.532727	0.320307
-13.967401	10.931786	0.325312
-14.562431	7.835917	0.330317
-14.656085	9.559013	0.335322
-14.748784	9.801314	0.340326
-14.566227	-1.547282	0.345331
-14.405434	5.194817	0.350336
-14.909935	6.865226	0.355341
-15.431842	2.391152	0.360346
-15.761907	5.274428	0.365350
-15.934276	-1.560802	0.370355
-16.914992	10.089993	0.375360
-17.258058	8.802290	0.380365
-17.125953	3.504403	0.385370
-17.177849	5.350670	0.390374
-17.193113	-3.983244	0.395379
-17.688507	-1.112029	0.400384
-17.460682	1.762929	0.405389
-17.854178	5.624258	0.410394
-18.517564	19.841778	0.415398
-18.455832	2.668619	0.420403
-18.890885	15.062829	0.425408
-18.788776	-0.949220	0.430413
-19.097080	-1.483063	0.435418
-20.216997	7.506662	0.440422
-20.334145	1.039269	0.445427
-20.737121	8.780868	0.450432
-20.135452	-2.263234	0.455437
-20.545105	-0.136285	0.460442
-20.760624	5.184131	0.465446
-20.569589	0.582533	0.470451
-21.254865	0.395658	0.475456
-21.937350	1.097366	0.480461
-21.701301	3.898269	0.485466
-21.950873	4.899144	0.490470
-21.904379	0.956111	0.495475
-22.145152	6.777196	0.500480
-23.006858	-1.816651	0.505485
-23.217358	-8.253595	0.510490
-23.249789	-2.221546	0.515494
-23.241555	-4.228683	0.520499
-24.379135	6.937321	0.525504
-24.264507	-4.372156	0.530509
-24.369615	4.316195	0.535514
-24.653985	8.527424	0.540518
-24.472032	5.268688	0.545523
-24.820501	0.583941	0.550528
-25.056213	-2.846635	0.555533
-25.408476	-6.407646	0.560538
-25.944671	12.573560	0.565542
-25.931101	3.342694	0.570547
-26.736994	6.452386	0.575552
-27.035617	11.586507	0.580557
-26.930282	0.322776	0.585562
-27.661566	2.525431	0.590566
-27.278182	4.657839	0.595571
-27.562154	8.944936	0.600576
-27.450026	7.373940	0.605581
-27.573808	6.422041	0.610586
-28.328197	12.159087	0.615590
-28.500946	12.572118	0.620595
-28.998191	8.853486	0.625600
-29.125608	4.826970	0.630605
-29.015205	6.704755	0.635610
-29.673661	14.151027	0.640614
-29.824459	1.706211	0.645619
-30.216638	5.137061	0.650624
-29.933828	8.376729	0.655629
-30.414748	1.760689	0.660634
-31.371108	15.277459	0.665638
-31.492065	0.056504	0.670643
-31.616084	10.791616	0.675648
-31.532364	9.560431	0.680653
-31.676043	9.174801	0.685658
-31.862018	15.354300	0.690662
-31.982505	9.112056	0.695667
-32.822493	8.465365	0.700672
-32.883142	1.530373	0.705677
-32.968174	1.113408	0.710682
-33.213859	6.868823	0.715686
-33.583557	-1.023824	0.720691
-34.279679	17.552172	0.725696
-34.416074	4.760247	0.730701
-34.536339	-4.079484	0.735706
-34.474513	7.433269	0.740710
-34.438771	-3.031775	0.745715
-35.125057	-1.535365	0.750720
-35.582181	5.926814	0.755725
-35.569560	5.057947	0.760730
-36.462825	3.223700	0.765734
-36.116513	0.578294	0.770739
-36.317607	8.984291	0.775744
-36.276816	3.937995	0.780749
-36.502287	-3.135686	0.785754
-37.213062	3.812575	0.790758
-37.289617	8.861280	0.795763
-37.543902	11.568168	0.800768
-38.040230	-6.874798	0.805773
-38.660798	-5.309590	0.810778
-38.951504	6.872169	0.815782
-38.838493	-5.528553	0.820787
-39.317759	-5.064331	0.825792
-39.054192	0.854900	0.830797
-38.974928	2.493954	0.835802
-39.669092	5.981612	0.840806
-39.020854	3.421776	0.845811
-40.443641	10.114605	0.850816
-40.486006	-1.053214	0.855821
-40.628470	1.750047	0.860826
-40.829632	2.971129	0.865830
-40.709707	9.501331	0.870835
-41.524090	6.430343	0.875840
-41.721805	6.363230	0.880845
-41.754284	2.150996	0.885850
-42.047075	9.027440	0.890854
-41.973238	0.394578	0.895859
-42.961865	-3.351463	0.900864
-43.395347	0.402235	0.905869
-43.877403	7.760753	0.910874
-44.039186	15.151349	0.915878
-43.719058	-2.831085	0.920883
-43.844560	-2.479240	0.925888
-43.406022	-5.101130	0.930893
-43.898377	1.733813	0.935898
-44.835963	7.572329	0.940902
-45.041528	0.796087	0.945907
-45.108333	5.748349	0.950912
-45.005068	3.349834	0.955917
-45.377777	1.092336	0.960922
-46.523422	13.116990	0.965926
-46.517050	4.915478	0.970931
-46.822156	9.278653	0.975936
-47.101547	8.768754	0.980941
-46.650885	3.006501	0.985946
-47.068980	9.624167	0.990950
-46.674795	4.737636	0.995955
-47.071190	8.906306	1.000960
-47.725883	0.754592	1.005965
-47.876560	-3.284096	1.010970
-48.967928	12.291294	1.015974
-49.184433	3.694432	1.020979
-49.246922	2.172943	1.025984
-49.716032	-3.831173	1.030989
-49.638698	1.658492	1.035994
-49.486194	9.404804	1.040998
-49.519319	0.019905	1.046003
-50.087971	-3.462907	1.051008
-50.178032	-1.566368	1.056013
-50.594517	-5.914585	1.061018
-51.421090	3.835939	1.066022
-50.696519	-9.644536	1.071027
-51.039090	-0.172333	1.076032
-51.446204	6.054467	1.081037
-52.198994	0.578857	1.086042
-52.805228	2.875815	1.091046
-53.025804	-1.019043	1.096051
-52.928018	-0.657891	1.101056
-52.859166	0.239307	1.106061
-52.766254	-1.720985	1.111066
-53.274059	3.297212	1.116070
-53.324130	-1.934162	1.121075
-53.817579	4.980048	1.126080
-54.484875	-4.216896	1.131085
-54.405969	-7.048194	1.136090
-54.412725	-3.215826	1.141094
-54.577603	-2.120653	1.146099
-55.646656	6.829467	1.151104
-55.704424	4.490984	1.156109
-55.706045	1.931732	1.161114
-56.002283	7.122425	1.166118
-55.824448	1.697152	1.171123
-56.409497	2.162131	1.176128
-56.900505	2.485824	1.181133
-57.227231	-1.174100	1.186138
-57.490399	4.261349	1.191142
-57.096832	9.622371	1.196147
-57.306437	11.812890	1.201152
-57.815201	3.255495	1.206157
-58.407031	-4.687764	1.211162
-59.052596	4.752822	1.216166
-58.930318	-2.495568	1.221171
-58.847743	3.281178	1.226176
-59.270486	11.484621	1.231181
-59.104313	12.999326	1.236186
-59.168833	14.252782	1.241190
-59.886477	1.906280	1.246195
-60.361883	7.251598	1.251200
-60.751910	3.047931	1.256205
-60.311395	4.155815	1.261210
-61.062719	10.471351	1.266214
-61.377452	1.804461	1.271219
-61.768267	-3.405160	1.276224
-62.045525	5.221577	1.281229
-61.662821	-0.036479	1.286234
-62.124999	12.479036	1.291238
-61.947196	2.798494	1.296243
-62.943329	7.795130	1.301248
-63.238436	5.139494	1.306253
-63.117818	7.670579	1.311258
-63.117793	10.872296	1.316262
-63.062236	-0.870851	1.321267
-63.937429	11.393000	1.326272
-64.446176	6.714387	1.331277
-64.545828	5.391711	1.336282
-65.024265	3.887939	1.341286
-65.018758	4.314170	1.346291
-64.902018	15.030540	1.351296
-65.213323	10.295679	1.356301
-65.517023	-1.891052	1.361306
-66.067027	3.108447	1.366310
-66.319484	9.127516	1.371315
-66.326650	1.279307	1.376320
-66.447403	3.367318	1.381325
-67.113179	9.318272	1.386330
-68.024646	-0.659830	1.391334
-67.713649	-2.610001	1.396339
-67.830061	3.729437	1.401344
-68.213290	6.216081	1.406349
-67.939854	-2.505001	1.411354
-68.479147	3.498899	1.416358
-68.117721	-5.346701	1.421363
-68.571987	7.322595	1.426368
-69.150680	0.753517	1.431373
-69.312749	-1.587604	1.436378
-70.001945	8.549523	1.441382
-70.254422	0.825174	1.446387
-70.796338	5.620925	1.451392
-71.032312	2.823146	1.456397
-70.998757	-3.712149	1.461402
-70.700972	7.393467	1.466406
-70.790939	9.549421	1.471411
-70.848547	1.297826	1.476416
-71.612657	6.109411	1.481421
-71.959149	5.391727	1.486426
-72.593288	10.170292	1.491430
-72.328201	0.893693	1.496435
-72.301980	2.993476	1.501440
-73.061700	3.343455	1.506445
-73.555918	3.272181	1.511450
-74.100948	13.883434	1.516454
-74.066510	1.273558	1.521459
-74.009289	-0.874132	1.526464
-74.535892	2.194964	1.531469
-74.390491	8.591457	1.536474
-74.344151	7.951427	1.541478
-74.586614	4.344738	1.546483
-74.990524	5.550133	1.551488
-75.396220	9.897432	1.556493
-75.487826	1.977032	1.561498
-75.885340	12.805617	1.566502
-76.452215	1.175817	1.571507
-76.869865	13.057928	1.576512
-77.352698	15.664585	1.581517
-76.904673	12.455906	1.586522
-76.971158	14.203219	1.591526
-76.883140	9.940467	1.596531
-77.524741	5.969210	1.601536
-78.091578	14.097156	1.606541
-77.908101	2.954063	1.611546
-78.368720	-0.504546	1.616550
-78.439149	-8.108718	1.621555
-79.164979	-0.927143	1.626560
-79.718285	6.439374	1.631565
-79.541124	11.372393	1.636570
-79.612266	9.073971	1.641574
-79.813552	6.742158	1.646579
-80.420460	0.205977	1.651584
-81.308848	1.512594	1.656589
-80.723746	3.850674	1.661594
-81.255545	2.260352	1.666598
-81.385437	-3.214778	1.671603
-81.147807	1.455661	1.676608
-81.042006	-3.034503	1.681613
-81.371746	5.015159	1.686618
-82.250623	3.684866	1.691622
-82.445087	1.073573	1.696627
-82.589804	3.269743	1.701632
-83.211890	4.695986	1.706637
-83.774687	0.465609	1.711642
-84.317594	5.163439	1.716646
-83.901219	3.161954	1.721651
-83.747939	4.561618	1.726656
-84.037292	6.407127	1.731661
-84.032101	3.584215	1.736666
-84.572352	2.969658	1.741670
-85.246164	-4.628556	1.746675
-85.529928	0.696223	1.751680
-85.870645	3.562186	1.756685
-85.744381	-0.485093	1.761690
-86.015547	-3.546277	1.766694
-85.905418	-3.769193	1.771699
-86.374036	4.928655	1.776704
-87.123151	7.017049	1.781709
-87.242321	0.363315	1.786714
-87.461265	1.036687	1.791718
-86.933368	0.520518	1.796723
-87.253851	3.867368	1.801728
-88.237951	9.611935	1.806733
-88.365941	-2.244819	1.811738
-88.942658	5.017798	1.816742
-88.813751	-3.456008	1.821747
-88.768472	1.466034	1.826752
-89.199955	10.034680	1.831757
-89.297778	2.061472	1.836762
-89.875666	7.793009	1.841766
-89.888874	-4.777758	1.846771
-89.869848	3.087539	1.851776
-90.671299	1.700822	1.856781
-91.118793	1.786744	1.861786
-91.466140	7.156289	1.866790
-91.689446	3.204913	1.871795
-91.869814	-6.030356	1.876800
-91.757740	-4.978579	1.881805
-91.458811	-5.705645	1.886810
-91.660209	-3.911884	1.891814
-92.406745	1.678398	1.896819
-92.818112	1.923175	1.901824
-93.164743	-1.461544	1.906829
-93.112708	-2.725729	1.911834
-93.213506	7.752636	1.916838
-93.611246	4.448692	1.921843
-94.512291	7.051276	1.926848
-94.729512	1.279779	1.931853
-94.531432	-1.174721	1.936858
-94.620382	3.277970	1.941862
-94.813351	-4.452535	1.946867
-95.293923	3.196815	1.951872
-96.009651	9.256836	1.956877
-95.833277	1.082476	1.961882
-96.222529	6.670560	1.966886
-96.385154	-6.582314	1.971891
-95.734482	6.745917	1.976896
-96.737731	0.879284	1.981901
-97.183463	-3.391580	1.986906
-97.658598	5.892588	1.991910
-97.611343	9.014137	1.996915
-97.698553	1.970084	2.006912
-97.975740	-1.132159	2.016909
-97.071141	1.193798	2.026906
-96.540779	0.736861	2.036902
-96.064160	-1.837262	2.046899
-95.490652	-2.278785	2.056896
-95.177530	-3.648861	2.066893
-94.670821	-1.669206	2.076890
-94.116177	-7.527912	2.086886
-93.896548	-11.344733	2.096883
-92.679909	-7.353880	2.106880
-92.161253	-3.795356	2.116877
-92.189342	1.499274	2.126874
-91.808292	2.801699	2.136870
-91.151592	2.138065	2.146867
-90.782956	-1.071710	2.156864
-89.656096	-1.748826	2.166861
-89.469954	0.572499	2.176858
-89.431069	4.830262	2.186854
-88.550801	-1.066797	2.196851
-88.341726	1.130558	2.206848
-87.281224	10.642050	2.216845
-86.846182	5.822119	2.226842
-86.358241	7.836395	2.236838
-86.401948	5.527535	2.246835
-85.475186	-0.981864	2.256832
-85.176421	6.542384	2.266829
-84.880327	6.030288	2.276826
-84.006246	9.526789	2.286822
-83.436233	5.354120	2.296819
-82.533860	4.927591	2.306816
-82.493221	1.363730	2.316813
-82.482818	4.330317	2.326810
-81.820862	3.140001	2.336806
-81.118209	-1.329050	2.346803
-80.196395	7.285506	2.356800
-79.460678	2.294918	2.366797
-79.303497	3.002025	2.376794
-79.290059	-4.849971	2.386790
-79.205843	0.670984	2.396787
-78.323927	-0.664670	2.406784
-77.440687	2.263355	2.416781
-76.946242	3.399125	2.426778
-76.521629	7.396877	2.436774
-75.830139	4.142849	2.446771
-75.634437	8.515426	2.456768
-75.397514	8.126644	2.466765
-74.326438	6.121450	2.476762
-74.106132	10.917828	2.486758
-73.444667	4.291607	2.496755
-72.742687	14.603719	2.506752
-72.460482	8.676823	2.516749
-72.321962	5.718516	2.526746
-71.487817	5.039750	2.536742
-71.071664	1.813027	2.546739
-70.449165	7.971905	2.556736
-69.858856	13.777866	2.566733
-69.469993	7.739222	2.576730
-69.204381	8.679598	2.586726
-68.429343	15.758589	2.596723
-67.920703	2.788990	2.606720
-67.832539	8.192120	2.616717
-66.889530	2.589341	2.626714
-66.535760	10.643503	2.636710
-65.772189	7.875530	2.646707
-65.497051	10.059367	2.656704
-65.140290	13.861845	2.666701
-64.123364	4.598150	2.676698
-63.859630	8.016057	2.686694
-64.146969	7.430653	2.696691
-63.028093	14.816901	2.706688
-62.236752	10.916830	2.716685
-62.192177	10.279418	2.726682
-61.325454	1.929419	2.736678
-60.489453	-0.643993	2.746675
-60.608738	4.902515	2.756672
-60.352467	10.307817	2.766669
-59.443624	4.051483	2.776666
-58.943297	-0.015230	2.786662
-57.975120	-1.057120	2.796659
-58.123640	8.577292	2.806656
-57.711560	13.118708	2.816653
-57.142842	4.780556	2.826650
-56.427169	4.652549	2.836646
-55.949722	4.064521	2.846643
-55.033632	1.050904	2.856640
-54.966834	0.856672	2.866637
-54.640169	-4.168022	2.876634
-54.152288	-3.604598	2.886630
-53.639772	-0.947936	2.896627
-53.067905	0.406956	2.906624
-52.321678	6.533778	2.916621
-52.006695	3.300732	2.926618
-51.381031	1.520554	2.936614
-50.758882	4.616205	2.946611
-50.650071	-0.184286	2.956608
-50.023303	2.308755	2.966605
-49.250588	0.369320	2.976602
-49.070108	0.277654	2.986598
-48.506709	3.917873	2.996595
-47.550402	2.545222	3.006592
-47.306103	0.850142	3.016589
-47.151515	-1.407425	3.026586
-46.461950	2.843422	3.036582
-45.977120	6.527630	3.046579
-45.515245	8.213371	3.056576
-44.722816	2.703879	3.066573
-44.295351	5.449897	3.076570
-44.301717	1.386547	3.086566
-43.650362	-0.796801	3.096563
-42.898574	3.339759	3.106560
-42.351324	-1.690989	3.116557
-41.914135	4.062936	3.126554
-41.421309	2.566502	3.136550
-40.806686	6.100493	3.146547
-40.235579	-0.879036	3.156544
-39.953278	9.061678	3.166541
-39.733727	6.378946	3.176538
-38.552813	-0.832347	3.186534
-38.389116	8.056226	3.196531
-38.246140	8.749721	3.206528
-37.460903	5.164224	3.216525
-36.836712	8.145516	3.226522
-36.480290	2.799375	3.236518
-35.375408	1.793088	3.246515
-35.401998	8.392630	3.256512
-35.061166	1.427007	3.266509
-34.635393	-0.603786	3.276506
-33.972010	3.435753	3.286502
-33.642553	1.527757	3.296499
-32.532471	6.986182	3.306496
-32.266699	-3.518809	3.316493
-32.406357	-1.285818	3.326490
-31.572795	4.279290	3.336486
-31.336121	3.196794	3.346483
-30.066620	5.383223	3.356480
-29.975097	4.963370	3.366477
-29.383205	2.662627	3.376474
-28.680123	5.036007	3.386470
-28.420253	4.187464	3.396467
-27.994142	-1.511720	3.406464
-27.248843	2.337586	3.416461
-26.529324	-4.405434	3.426458
-26.807103	1.682263	3.436454
-25.742023	-0.337825	3.446451
-25.090751	2.081687	3.456448
-24.916777	1.230763	3.466445
-24.684616	-0.738015	3.476442
-23.952910	1.833621	3.486438
-23.561335	5.652820	3.496435
-22.638457	1.874696	3.506432
-22.317315	4.114684	3.516429
-22.369521	1.940202	3.526426
-21.495141	1.061900	3.536422
-20.767756	-0.651850	3.546419
-19.883081	1.636057	3.556416
-19.872360	0.088449	3.566413
-19.553073	-4.314196	3.576410
-18.892393	1.344524	3.586406
-18.157199	1.729817	3.596403
-18.035775	4.115138	3.606400
-17.552289	5.011875	3.616397
-16.663179	4.501901	3.626394
-16.497900	2.492916	3.636390
-15.930561	4.478917	3.646387
-15.103099	9.861250	3.656384
-14.824398	6.351952	3.666381
-14.475947	4.507505	3.676378
-13.756696	2.706330	3.686374
-13.388667	-2.461062	3.696371
-13.281660	1.133458	3.706368
-12.136470	-3.395424	3.716365
-11.799931	1.756548	3.726362
-11.430284	-0.164080	3.736358
-10.744658	3.574201	3.746355
-10.582232	1.236210	3.756352
-9.398790	3.984159	3.766349
-9.006978	3.070594	3.776346
-8.921502	-1.206719	3.786342
-8.822599	3.491474	3.796339
-7.789533	3.956810	3.806336
-7.450476	5.379860	3.816333
-7.330188	5.300794	3.826330
-6.210655	2.939554	3.836326
-5.787314	11.074690	3.846323
-5.285211	15.807915	3.856320
-4.963936	15.678351	3.866317
-4.604747	25.632373	3.876314
-3.923598	30.600479	3.886310
-3.562456	32.333687	3.896307
-3.189215	37.502094	3.906304
-2.477660	51.604632	3.916301
-2.198415	56.109856	3.926298
-1.771435	66.050112	3.936294
-1.721039	79.698725	3.946291
-0.973969	103.945493	3.956288
0.000000	102.851451	3.961293
-0.184182	119.616752	3.966298
-0.269235	113.175925	3.971302
-0.169467	128.596426	3.976307
-0.000686	137.495033	3.981312
0.329733	141.322062	3.986317
0.351076	138.537725	3.991322
0.476805	139.115968	3.996326
0.073353	144.709483	4.001331
0.168061	148.690505	4.006336
0.571759	137.035085	4.011341
0.481084	136.666457	4.016346
0.869003	125.956327	4.021350
0.233631	137.920095	4.026355
0.263205	138.937352	4.031360
0.545234	133.907005	4.036365
0.652531	152.379410	4.041370
0.518843	152.232660	4.046374
0.572998	148.930645	4.051379
0.560024	153.121531	4.056384
0.859571	145.826320	4.061389
0.802107	151.470033	4.066394
0.356723	147.797027	4.071398
0.672902	154.233260	4.076403
0.878019	167.210654	4.081408
0.944963	143.936732	4.086413
0.681686	147.714412	4.091418
0.651092	138.423953	4.096422
0.764251	139.997598	4.101427
0.647856	149.674893	4.106432
0.832841	141.258666	4.111437
0.521389	145.236886	4.116442
0.755757	152.745809	4.121446
0.770416	153.411058	4.126451
0.813885	161.133395	4.131456
0.626282	157.144747	4.136461
0.627517	161.374538	4.141466
0.801937	159.860209	4.146470
0.952357	170.558748	4.151475
0.862422	171.727611	4.156480
1.287051	173.401156	4.161485
0.986528	174.492281	4.166490
1.111686	159.397142	4.171494
0.946826	153.468686	4.176499
0.802301	145.676732	4.181504
0.874356	144.516968	4.186509
0.903564	146.698561	4.191514
1.043576	163.985755	4.196518
0.857654	160.512543	4.201523
0.854050	156.745006	4.206528
1.179935	166.191660	4.211533
1.336019	170.305442	4.216538
0.983114	159.312726	4.221542
1.170843	148.858579	4.226547
0.704413	141.139210	4.231552
1.201228	151.074773	4.236557
0.922637	158.749492	4.241562
1.297159	161.468613	4.246566
1.060201	155.725461	4.251571
0.938318	155.250990	4.256576
1.066045	165.200097	4.261581
1.273136	165.177126	4.266586
1.398696	161.781662	4.271590
1.000075	158.572733	4.276595
1.187045	166.452925	4.281600
1.382447	161.780998	4.286605
0.949961	157.315019	4.291610
1.164983	163.849363	4.296614
1.395926	170.017378	4.301619
1.041996	173.578310	4.306624
1.196593	164.711245	4.311629
1.311152	170.384960	4.316634
1.585770	168.968827	4.321638
1.523603	169.791649	4.326643
1.088745	153.252978	4.331648
0.912863	158.589376	4.336653
1.164165	177.504322	4.341658
1.299115	175.594372	4.346662
1.524474	174.391604	4.351667
1.271822	169.422875	4.356672
1.730248	166.456154	4.361677
1.444304	172.448888	4.366682
1.565535	168.658626	4.371686
1.384534	166.554568	4.376691
1.599399	161.762530	4.381696
1.398521	163.192388	4.386701
1.678378	169.839965	4.391706
1.253782	159.510225	4.396710
1.375875	161.756361	4.401715
1.189934	166.515361	4.406720
1.413605	166.530922	4.411725
1.387454	166.895677	4.416730
1.249871	172.381104	4.421734
1.478292	172.813542	4.426739
1.638638	173.579354	4.431744
1.665337	165.687797	4.436749
1.781076	165.119146	4.441754
1.630144	168.847591	4.446758
1.329681	167.660769	4.451763
1.494379	168.343640	4.456768
1.778354	160.718664	4.461773
1.723868	169.462441	4.466778
1.608943	164.557556	4.471782
1.717635	166.441956	4.476787
1.936230	168.850145	4.481792
2.073645	166.753146	4.486797
1.530645	181.524580	4.491802
1.591014	169.676155	4.496806
1.983146	175.553158	4.501811
2.081277	180.451154	4.506816
2.123048	165.698109	4.511821
1.544115	154.028956	4.516826
1.390880	146.409212	4.521830
1.435684	157.497619	4.526835
1.565904	172.378705	4.531840
2.065403	166.602420	4.536845
1.800666	174.591355	4.541850
1.637213	159.380081	4.546854
1.694640	170.662674	4.551859
1.820809	169.500758	4.556864
1.604695	170.790633	4.561869
1.424047	166.686996	4.566874
1.670692	166.028231	4.571878
1.913661	177.895535	4.576883
1.798813	181.029861	4.581888
2.134706	179.948981	4.586893
1.785116	185.606838	4.591898
2.028774	165.484824	4.596902
1.840066	171.032045	4.601907
1.893740	177.746701	4.606912
2.116021	171.058381	4.611917
1.575215	178.423010	4.616922
2.288456	192.722375	4.621926
2.048542	192.456224	4.626931
2.076511	200.997268	4.631936
2.380263	191.331688	4.636941
1.955443	188.345161	4.641946
1.635411	175.417364	4.646950
2.223959	193.333510	4.651955
2.096822	189.999781	4.656960
2.383554	193.248362	4.661965
2.470251	200.318526	4.666970
2.330073	178.655750	4.671974
1.927188	171.897700	4.676979
1.868490	168.800028	4.681984
2.070270	181.123048	4.686989
2.101986	192.086975	4.691994
1.865882	191.532321	4.696998
2.183772	192.827116	4.702003
1.540675	196.949059	4.707008
2.292750	197.824643	4.712013
2.144753	203.011150	4.717018
2.193792	199.592866	4.722022
2.437705	195.777049	4.727027
2.109083	195.284347	4.732032
2.730346	196.927086	4.737037
2.329967	194.642257	4.742042
2.381422	192.859284	4.747046
2.349014	199.271055	4.752051
2.153765	196.340308	4.757056
2.230711	191.436992	4.762061
2.147034	195.610493	4.767066
2.131782	196.166533	4.772070
2.478645	195.137718	4.777075
2.202478	200.977067	4.782080
2.536092	193.246222	4.787085
2.254435	215.671116	4.792090
2.781326	212.462702	4.797094
2.405492	206.791914	4.802099
2.025070	209.436336	4.807104
2.676360	212.681586	4.812109
2.644695	224.936807	4.817114
2.802873	206.324623	4.822118
2.726553	206.130918	4.827123
2.484493	211.018948	4.832128
2.559804	196.880729	4.837133
2.104355	202.118571	4.842138
2.623756	213.888804	4.847142
2.990581	216.485750	4.852147
2.427979	217.852063	4.857152
2.572520	209.698410	4.862157
2.755830	223.175979	4.867162
2.948156	207.412202	4.872166
2.476282	208.416280	4.877171
2.706862	217.900041	4.882176
2.747486	208.892621	4.887181
2.480409	209.918396	4.892186
2.336308	213.348381	4.897190
2.604214	224.066511	4.902195
2.862051	224.741118	4.907200
2.946445	215.720510	4.912205
2.249429	221.606822	4.917210
2.246738	222.480440	4.922214
2.580491	225.250252	4.927219
2.724624	228.261749	4.932224
2.849259	218.956419	4.937229
2.831150	220.914476	4.942234
3.014915	222.704860	4.947238
2.928757	222.784784	4.952243
3.280461	228.029048	4.957248
3.023603	215.515274	4.962253
2.824588	223.996979	4.967258
2.860261	219.717065	4.972262
2.898051	218.100749	4.977267
2.947740	234.079691	4.982272
2.988792	222.490526	4.987277
2.997051	225.178456	4.992282
2.807837	226.131920	4.997286
2.776794	224.637122	5.002291
2.578865	222.323733	5.007296
2.982441	216.957938	5.012301
3.063271	216.359953	5.017306
2.755901	213.029148	5.022310
2.975287	210.840204	5.027315
2.923415	222.544923	5.032320
2.930145	217.079952	5.037325
2.978272	234.027264	5.042330
3.036996	239.266815	5.047334
3.625531	243.420427	5.052339
3.203662	239.269145	5.057344
3.248947	219.646396	5.062349
2.817324	218.619329	5.067354
2.817646	212.604860	5.072358
3.312780	235.398461	5.077363
3.183298	245.378421	5.082368
3.244262	249.155941	5.087373
3.307306	251.360719	5.092378
3.264859	240.335130	5.097382
3.427005	220.687742	5.102387
3.180959	227.939768	5.107392
3.159776	225.696764	5.112397
3.419524	241.092297	5.117402
3.498414	235.752058	5.122406
3.090239	229.652887	5.127411
2.954751	226.203398	5.132416
3.357192	235.182505	5.137421
3.279325	248.862370	5.142426
3.628884	243.739153	5.147430
3.454074	240.890619	5.152435
3.107165	235.575964	5.157440
3.479644	239.804557	5.162445
3.303307	252.082464	5.167450
2.975675	256.075898	5.172454
3.437257	244.648625	5.177459
3.395520	246.433213	5.182464
3.723354	236.469601	5.187469
3.677385	251.460616	5.192474
3.608011	247.292069	5.197478
3.979753	241.782555	5.202483
3.137559	240.506598	5.207488
3.152606	224.014431	5.212493
3.639582	232.512047	5.217498
3.432846	244.794712	5.222502
3.888047	243.976715	5.227507
3.414354	250.337420	5.232512
3.491591	245.285344	5.237517
3.712985	247.272319	5.242522
3.529637	246.408834	5.247526
3.705080	244.147677	5.252531
3.443003	249.829807	5.257536
3.667921	248.218971	5.262541
3.813551	262.464954	5.267546
3.777105	257.547748	5.272550
3.657522	251.609001	5.277555
3.526869	254.011810	5.282560
3.801420	254.892613	5.287565
3.342519	253.661005	5.292570
3.461482	256.995997	5.297574
3.771400	251.818876	5.302579
3.361390	258.875137	5.307584
3.402452	253.303533	5.312589
3.526182	247.965756	5.317594
3.384468	254.812297	5.322598
3.578300	250.267145	5.327603
3.263730	265.214834	5.332608
3.934644	268.026741	5.337613
3.928359	268.758552	5.342618
4.074836	275.275203	5.347622
3.834293	272.383178	5.352627
3.814538	269.007298	5.357632
3.888471	266.682947	5.362637
3.835680	281.520030	5.367642
3.898519	267.750713	5.372646
4.317844	272.715471	5.377651
3.765073	263.468796	5.382656
3.957790	258.996585	5.387661
4.002859	260.501813	5.392666
3.708290	269.077606	5.397670
3.979977	271.376250	5.402675
3.651834	274.664236	5.407680
4.176581	272.731168	5.412685
3.930031	280.559109	5.417690
3.833203	270.934103	5.422694
3.431399	278.394055	5.427699
3.767971	277.686394	5.432704
3.786439	275.908581	5.437709
3.667435	282.609202	5.442714
3.819445	271.591092	5.447718
4.208661	283.309000	5.452723
3.903828	289.130722	5.457728
4.278482	289.442173	5.462733
4.160777	303.460523	5.467738
4.247874	301.108794	5.472742
4.365195	289.618370	5.477747
3.965878	285.634390	5.482752
4.349419	284.125250	5.487757
4.235062	290.154416	5.492762
3.955189	280.118313	5.497766
4.264866	290.946999	5.502771
4.261357	290.438158	5.507776
4.542306	300.515197	5.512781
4.427207	297.679445	5.517786
4.224802	289.222603	5.522790
4.376471	279.751650	5.527795
4.099803	283.999702	5.532800
4.317055	281.769955	5.537805
4.137349	289.574772	5.542810
4.493697	292.435969	5.547814
4.582058	300.923306	5.552819
4.410607	296.960570	5.557824
3.993818	278.333991	5.562829
4.433880	290.550149	5.567834
4.166179	293.249689	5.572838
4.647988	298.290087	5.577843
4.109855	303.313118	5.582848
4.412321	303.126504	5.587853
4.227708	301.342542	5.592858
4.255819	300.113721	5.597862
4.768744	304.149478	5.602867
4.440903	306.399687	5.607872
4.663626	295.383138	5.612877
4.273764	304.824948	5.617882
4.221139	305.532383	5.622886
3.964313	307.179831	5.627891
4.442755	301.707366	5.632896
4.462984	309.775102	5.637901
4.397857	299.699013	5.642906
4.257466	300.878954	5.647910
4.847298	302.014088	5.652915
4.673324	317.325778	5.657920
4.537836	304.821400	5.662925
4.836411	310.260678	5.667930
4.673767	300.756702	5.672934
4.769360	299.953916	5.677939
4.668837	305.477871	5.682944
4.676025	309.877612	5.687949
4.627606	303.896060	5.692954
4.913795	308.669711	5.697958
4.926915	311.983331	5.702963
4.469031	313.886913	5.707968
4.728849	305.430410	5.712973
4.666081	312.194999	5.717978
4.765325	315.732412	5.722982
4.736694	321.055278	5.727987
4.834982	320.036929	5.732992
4.754777	324.592739	5.737997
4.952300	323.448107	5.743002
4.584004	310.885286	5.748006
4.692450	311.539010	5.753011
4.608471	315.883433	5.758016
4.971913	329.136702	5.763021
4.625166	324.353519	5.768026
5.031396	324.900475	5.773030
5.021739	320.732045	5.778035
4.777480	321.820692	5.783040
4.746926	313.311602	5.788045
4.751920	319.078462	5.793050
4.990080	318.152096	5.798054
4.990480	311.549109	5.803059
5.012808	322.748711	5.808064
5.214780	308.824682	5.813069
5.119962	324.067027	5.818074
4.982427	315.223513	5.823078
4.914382	322.624862	5.828083
4.732712	322.283143	5.833088
4.913697	320.581105	5.838093
4.976297	318.068693	5.843098
5.022108	317.659693	5.848102
4.884086	315.827300	5.853107
4.757599	320.675105	5.858112
5.276942	331.281135	5.863117
5.544841	341.591202	5.868122
5.137673	333.900430	5.873126
5.227498	330.406127	5.878131
4.602460	323.398081	5.883136
5.102827	338.322552	5.888141
5.560590	345.325144	5.893146
5.133133	344.148716	5.898150
5.644844	336.389905	5.903155
5.109669	327.728912	5.908160
5.113508	319.423243	5.913165
5.320629	338.750254	5.918170
5.014104	344.502655	5.923174
5.531006	341.881093	5.928179
5.493778	345.857521	5.933184
5.227144	348.145603	5.938189
5.110919	334.195478	5.943194
5.050657	344.139337	5.948198
5.337278	346.755197	5.953203
5.373332	347.319023	5.958208
5.537127	347.660349	5.963213
5.383752	350.231250	5.968218
5.389900	346.360903	5.973222
5.743009	349.668717	5.978227
5.531471	354.732342	5.983232
5.301168	340.410934	5.988237
5.544010	327.534043	5.993242
5.155697	344.223967	5.998246
5.570370	337.802841	6.003251
5.465242	339.600535	6.008256
5.485314	330.735483	6.013261
5.250336	326.197385	6.018266
5.321622	326.148235	6.023270
5.387757	321.740134	6.028275
5.250575	324.694482	6.033280
5.594455	329.212322	6.038285
5.337753	324.139777	6.043290
5.241243	321.206194	6.048294
5.457033	330.094368	6.053299
5.331787	326.855231	6.058304
5.182889	342.893859	6.063309
5.506593	344.213065	6.068314
5.443299	344.700706	6.073318
5.399156	352.158435	6.078323
5.687956	354.729662	6.083328
5.471143	334.986496	6.088333
5.114257	332.372124	6.093338
5.288431	327.045403	6.098342
5.437040	319.381455	6.103347
5.176600	332.998240	6.108352
5.397524	341.964711	6.113357
5.436658	344.992680	6.118362
5.307864	341.519972	6.123366
5.549089	339.207366	6.128371
5.212542	353.260043	6.133376
5.632910	343.642551	6.138381
5.490165	325.814564	6.143386
5.160786	323.376222	6.148390
5.466862	318.990641	6.153395
5.384699	332.206160	6.158400
5.481226	325.654547	6.163405
5.529892	318.673828	6.168410
5.277251	329.625444	6.173414
5.315392	326.015850	6.178419
5.156731	322.342177	6.183424
5.440151	327.480108	6.188429
5.422944	337.550098	6.193434
5.212455	346.985973	6.198438
5.414034	339.883208	6.203443
5.233508	354.069632	6.208448
5.518906	354.388741	6.213453
5.725064	349.341747	6.218458
5.358743	339.724126	6.223462
5.620977	329.887802	6.228467
4.974350	331.991804	6.233472
5.330506	326.617588	6.238477
5.430171	340.522813	6.243482
5.338204	334.541746	6.248486
5.351730	339.630217	6.253491
5.473668	347.365650	6.258496
5.388198	333.562570	6.263501
5.399038	339.711345	6.268506
5.473399	329.632368	6.273510
5.294190	328.249363	6.278515
5.185466	337.239006	6.283520
5.443234	343.665477	6.288525
5.432545	354.496940	6.293530
5.599620	349.139686	6.298534
5.049938	332.843471	6.303539
5.194796	342.169882	6.308544
5.045773	347.245856	6.313549
5.476780	345.238881	6.318554
5.369515	348.723233	6.323558
5.456497	350.484500	6.328563
5.320366	350.474175	6.333568
5.378004	347.968864	6.338573
5.426832	355.323441	6.343578
5.561773	360.335945	6.348582
5.562153	353.774076	6.353587
5.464593	355.096009	6.358592
5.655382	350.171649	6.363597
5.552540	334.893780	6.368602
5.397392	330.662720	6.373606
5.061327	324.349734	6.378611
4.968587	333.710203	6.383616
5.223139	341.393218	6.388621
5.703233	345.557517	6.393626
5.594549	348.001191	6.398630
6.016092	342.069381	6.403635
5.424979	334.470706	6.408640
5.274668	327.033929	6.413645
5.290194	325.534989	6.418650
5.134594	321.345132	6.423654
5.506099	328.389707	6.428659
5.451361	328.148325	6.433664
5.337552	326.182420	6.438669
5.244299	319.322015	6.443674
5.050398	325.332016	6.448678
5.468247	334.979492	6.453683
5.311336	342.897822	6.458688
5.195570	342.257868	6.463693
5.631417	343.505718	6.468698
5.460699	353.166324	6.473702
5.450346	336.592609	6.478707
5.260623	330.797707	6.483712
5.258738	329.197089	6.488717
5.607635	341.357961	6.493722
5.147495	338.715472	6.498726
5.542986	331.851253	6.503731
5.506078	333.464247	6.508736
5.172272	327.375537	6.513741
5.240812	334.973795	6.518746
5.232566	340.919912	6.523750
5.299744	343.911848	6.528755
5.479642	342.228962	6.533760
5.543369	343.500314	6.538765
5.712101	347.333738	6.543770
5.026780	341.451963	6.548774
5.492300	345.874816	6.553779
5.509022	338.104972	6.558784
5.344050	337.567642	6.563789
5.380954	334.704904	6.568794
5.268168	357.426228	6.573798
5.241376	352.602398	6.578803
5.181397	358.101034	6.583808
5.269486	352.471410	6.588813
5.400384	339.700637	6.593818
5.613870	350.610871	6.598822
5.605044	349.523880	6.603827
5.505516	351.763634	6.608832
5.475137	342.473035	6.613837
5.367403	336.548223	6.618842
4.969835	334.667906	6.623846
5.389939	340.667134	6.628851
5.445200	351.108601	6.633856
5.257848	347.901338	6.638861
5.345243	346.679045	6.643866
5.254328	350.667050	6.648870
5.541706	347.458174	6.653875
5.690789	353.506198	6.658880
5.800251	342.646574	6.663885
5.398483	329.759945	6.668890
5.102574	331.957697	6.673894
5.175364	331.487521	6.678899
5.592892	344.365324	6.683904
5.499072	345.968252	6.688909
5.045345	336.968619	6.693914
4.888442	344.007403	6.698918
5.874562	348.962473	6.703923
5.441491	357.287920	6.708928
5.504742	350.887048	6.713933
5.357301	348.920082	6.718938
5.133946	353.473017	6.723942
5.602604	349.463762	6.728947
5.589665	351.430515	6.733952
5.488681	340.629176	6.738957
5.329859	331.241646	6.743962
5.249596	330.738501	6.748966
5.082914	319.393798	6.753971
5.109965	337.530947	6.758976
4.942707	350.190322	6.763981
5.418644	351.887484	6.768986
5.622080	348.834132	6.773990
5.409752	348.579475	6.778995
5.612001	357.817807	6.784000
5.423310	358.581365	6.789005
5.763371	358.664114	6.794010
5.474713	340.754568	6.799014
5.708683	327.081782	6.804019
5.165592	334.253838	6.809024
5.190350	320.759373	6.814029
5.469039	325.872734	6.819034
5.012853	331.275247	6.824038
5.567359	337.528670	6.829043
5.387380	350.620320	6.834048
5.250578	343.760400	6.839053
5.524925	350.658851	6.844058
5.487899	350.781699	6.849062
5.396073	341.067283	6.854067
5.230156	341.988628	6.859072
5.581909	337.659163	6.864077
5.519461	333.866006	6.869082
5.138594	324.022876	6.874086
5.448406	322.942911	6.879091
5.367157	329.587013	6.884096
5.470281	333.557266	6.889101
5.700636	325.390115	6.894106
5.270882	333.550511	6.899110
5.359043	320.447918	6.904115
5.136624	328.734019	6.909120
5.259872	330.401015	6.914125
5.535400	336.663345	6.919130
5.271719	334.338097	6.924134
5.190510	336.160517	6.929139
5.591945	349.316098	6.934144
5.916924	344.206195	6.939149
5.627253	335.652269	6.944154
5.346144	331.962977	6.949158
5.703713	332.387840	6.954163
5.571755	328.342977	6.959168
5.451055	331.965476	6.964173
5.562206	325.917785	6.969178
5.328969	328.675207	6.974182
5.273335	327.639844	6.979187
4.806762	329.671342	6.984192
5.215504	332.524337	6.989197
5.349699	325.663094	6.994202
5.140134	334.975429	6.999206
5.507737	325.245987	7.004211
5.332416	333.334881	7.009216
5.010209	335.093818	7.014221
5.465750	321.528692	7.019226
5.143806	333.111279	7.024230
5.279399	333.801881	7.029235
5.853522	346.095151	7.034240
5.514900	340.583009	7.039245
5.541566	328.015242	7.044250
5.191308	338.014026	7.049254
5.496231	329.898465	7.054259
5.280220	333.991489	7.059264
5.377243	326.449520	7.064269
5.273049	332.416994	7.069274
5.399434	328.239903	7.074278
5.244281	325.312344	7.079283
5.469090	325.216993	7.084288
5.191527	323.922166	7.089293
5.129380	331.601012	7.094298
5.423151	341.476744	7.099302
5.768400	337.651347	7.104307
5.420074	333.437899	7.109312
5.452886	329.705750	7.114317
5.733167	325.169181	7.119322
5.155547	325.079329	7.124326
5.323548	321.319672	7.129331
5.052057	325.560596	7.134336
5.261552	328.498593	7.139341
5.367116	342.247868	7.144346
5.542233	334.174791	7.149350
5.588939	334.562936	7.154355
5.376120	330.546562	7.159360
5.112311	329.341331	7.164365
5.329132	333.148234	7.169370
5.483675	341.644204	7.174374
5.426468	343.323655	7.179379
5.137622	338.294109	7.184384
5.397334	349.023089	7.189389
5.707648	337.024657	7.194394
5.344974	335.635594	7.199398
5.617972	326.262669	7.204403
5.293507	326.500157	7.209408
4.961343	320.145430	7.214413
5.411360	329.702439	7.219418
5.663434	351.398457	7.224422
5.438073	336.247353	7.229427
5.304051	333.313318	7.234432
5.181077	333.721721	7.239437
5.678809	332.362369	7.244442
5.280008	339.413742	7.249446
5.427603	333.777964	7.254451
5.562819	328.754746	7.259456
5.170273	325.883365	7.264461
5.523824	332.187254	7.269466
5.447790	333.575418	7.274470
5.193386	325.632918	7.279475
5.222717	337.056064	7.284480
5.055645	329.508014	7.289485
5.329917	349.061801	7.294490
5.307310	356.133334	7.299494
5.629871	353.703576	7.304499
5.584247	361.968319	7.309504
5.420205	353.964191	7.314509
5.528717	343.709008	7.319514
5.155784	329.207471	7.324518
5.231882	346.267569	7.329523
5.434505	355.619738	7.334528
5.337755	350.579074	7.339533
5.753875	346.869124	7.344538
4.973308	345.210170	7.349542
5.056979	335.914361	7.354547
5.426818	349.309016	7.359552
5.316044	356.362724	7.364557
5.737955	353.575706	7.369562
5.934323	353.016563	7.374566
5.424304	342.766540	7.379571
5.035310	332.791798	7.384576
5.175508	334.620657	7.389581
5.296889	343.039564	7.394586
5.436034	363.791485	7.399590
5.311203	349.804730	7.404595
5.216736	355.289785	7.409600
5.371001	348.387424	7.414605
5.588771	346.417022	7.419610
5.518680	365.240151	7.424614
5.980912	349.076447	7.429619
5.578336	350.310126	7.434624
5.219825	333.265767	7.439629
5.353090	327.401277	7.444634
5.194865	335.791220	7.449638
5.469296	328.724502	7.454643
5.600481	326.160214	7.459648
5.229660	332.441553	7.464653
5.467269	323.994848	7.469658
5.370455	330.723649	7.474662
5.046310	327.303698	7.479667
5.086065	331.676195	7.484672
5.255659	349.306956	7.489677
5.444278	353.896586	7.494682
5.603491	353.915918	7.499686
5.730979	352.276045	7.504691
5.720138	338.834600	7.509696
5.601406	335.502690	7.514701
5.498591	332.244219	7.519706
5.188001	341.382555	7.524710
5.403128	331.762423	7.529715
5.303313	333.284030	7.534720
5.085922	327.632672	7.539725
5.549577	321.124782	7.544730
5.414608	337.332070	7.549734
5.541406	328.880578	7.554739
5.402209	327.671642	7.559744
5.129221	332.751216	7.564749
5.302329	326.969071	7.569754
4.846811	331.900069	7.574758
5.119484	342.146112	7.579763
5.374572	344.013920	7.584768
5.555897	349.825931	7.589773
5.533937	353.879065	7.594778
5.331854	350.813318	7.599782
5.315412	338.657268	7.604787
5.749022	337.481973	7.609792
5.593229	337.126707	7.614797
5.363718	329.414430	7.619802
5.272467	333.209489	7.624806
5.509499	329.366247	7.629811
5.627793	334.903384	7.634816
5.212215	332.389959	7.639821
5.746735	323.425324	7.644826
4.979790	339.794908	7.649830
5.368714	324.506438	7.654835
5.319472	325.346225	7.659840
5.104636	335.282660	7.664845
5.463206	325.510340	7.669850
5.239651	320.546501	7.674854
5.356002	324.796261	7.679859
5.909493	334.375026	7.684864
5.393502	331.757109	7.689869
5.620888	329.525768	7.694874
5.121952	336.349213	7.699878
5.369786	330.735697	7.704883
5.348515	334.273013	7.709888
5.206024	329.305962	7.714893
5.114724	331.474820	7.719898
5.337639	332.148576	7.724902
5.609935	332.371659	7.729907
5.512328	328.182206	7.734912
5.277071	324.631268	7.739917
5.460345	319.214536	7.744922
5.282687	329.388757	7.749926
5.169329	317.896491	7.754931
5.385200	337.832749	7.759936
5.386193	327.888657	7.764941
5.724814	323.089842	7.769946
5.155176	331.613848	7.774950
5.428793	323.588619	7.779955
5.305385	327.021711	7.784960
5.254031	334.673557	7.789965
5.365796	339.471382	7.794970
5.244611	335.870930	7.799974
5.530174	338.015544	7.804979
5.812233	337.253146	7.809984
5.347236	334.839214	7.814989
5.444074	324.215703	7.819994
5.237207	330.287851	7.824998
5.246816	326.394819	7.830003
5.307182	327.489522	7.835008
4.962024	333.757349	7.840013
5.630383	337.379608	7.845018
5.660321	345.863465	7.850022
5.798627	338.973099	7.855027
5.377936	332.888509	7.860032
5.377320	331.765430	7.865037
5.635860	331.905245	7.870042
5.544685	338.136443	7.875046
5.535379	331.111017	7.880051
5.417169	317.680083	7.885056
5.466277	329.217186	7.890061
5.619120	323.435053	7.895066
5.557452	332.309752	7.900070
5.452724	326.409782	7.905075
5.878239	335.818770	7.910080
5.311139	334.955295	7.915085
5.490357	329.026655	7.920090
5.403203	334.975641	7.925094
5.604720	325.411431	7.930099
5.326414	329.485740	7.935104
5.024940	331.171824	7.940109
5.460519	329.936108	7.945114
5.259951	330.309211	7.950118
5.411306	325.777023	7.955123
5.621055	328.639049	7.960128
5.481302	333.547289	7.965146
5.613609	336.675992	7.970163
5.302910	322.217631	7.975181
5.272149	329.780478	7.980198
5.583187	323.382342	7.985216
5.130467	331.907537	7.990234
5.708722	323.081779	7.995251
5.312999	329.433193	8.000269
5.392335	318.940473	8.005286
5.578865	322.003875	8.010304
5.190052	317.116551	8.015322
5.512499	330.907171	8.020339
5.516400	332.367661	8.025357
5.470238	321.705257	8.030374
5.428156	314.494618	8.035392
5.087197	337.761785	8.040410
5.587940	325.262243	8.045427
5.578717	333.616967	8.050445
5.483308	334.572317	8.055462
5.404019	329.090547	8.060480
5.266529	333.782598	8.065498
5.676595	324.153227	8.070515
5.300337	330.713027	8.075533
5.581404	333.076818	8.080550
5.564109	326.610206	8.085568
5.545349	324.795413	8.090586
5.665198	325.313098	8.095603
5.391869	338.474401	8.100621
5.171573	329.865275	8.105638
5.578134	324.234800	8.110656
5.366166	336.386113	8.115674
5.520172	333.963589	8.120691
5.340119	329.163472	8.125709
5.441677	327.557042	8.130726
5.504500	325.145651	8.135744
5.311745	336.287266	8.140762
5.582984	325.190127	8.145779
5.691117	325.056406	8.150797
5.613352	334.592657	8.155814
6.006168	320.756206	8.160832
5.554352	327.902192	8.165850
5.807279	332.785532	8.170867
5.623220	335.998517	8.175885
5.721964	340.019249	8.180902
5.748961	323.674479	8.185920
5.267342	332.365146	8.190938
5.729059	334.697478	8.195955
5.490345	337.117463	8.200973
5.848045	325.561815	8.205990
5.420065	335.354906	8.211008
5.237949	329.520023	8.216026
5.926412	318.761454	8.221043
5.700616	325.023127	8.226061
5.636461	325.399231	8.231078
5.684136	332.640525	8.236096
5.701462	334.777400	8.241114
5.507207	329.136920	8.246131
5.490988	324.819212	8.251149
5.591118	330.370267	8.256166
5.604459	322.412493	8.261184
5.557821	325.174762	8.266202
5.577434	328.327433	8.271219
5.327001	330.963845	8.276237
5.435761	330.435556	8.281254
5.477368	333.038835	8.286272
5.707312	349.052994	8.291290
5.602014	348.280536	8.296307
5.750591	352.416537	8.301325
6.044130	350.909411	8.306342
6.087677	340.602165	8.311360
5.503397	341.725629	8.316378
5.374611	333.739626	8.321395
5.469278	345.053960	8.326413
6.006809	354.459104	8.331430
6.190162	353.553058	8.336448
5.634298	347.303363	8.341466
6.076329	353.741274	8.346483
5.927554	330.250989	8.351501
5.656469	332.041738	8.356518
5.874251	327.220313	8.361536
5.752155	329.079235	8.366554
5.723056	322.567137	8.371571
5.262432	323.245198	8.376589
5.693560	341.594648	8.381606
6.014104	343.280078	8.386624
5.749894	359.276998	8.391642
6.040686	355.523398	8.396659
6.039161	355.795017	8.401677
6.213058	348.427450	8.406694
5.968781	343.479603	8.411712
6.053498	334.267271	8.416730
5.339630	327.486925	8.421747
5.963271	325.950171	8.426765
5.658094	334.853032	8.431782
5.899748	332.606122	8.436800
5.875409	347.110643	8.441818
5.772964	344.504240	8.446835
5.890845	351.538885	8.451853
6.030071	352.012510	8.456870
5.881429	352.341893	8.461888
6.016654	349.635136	8.466906
6.271397	348.307656	8.471923
6.117435	331.751394	8.476941
5.702520	334.337839	8.481958
5.900551	322.999711	8.486976
5.834763	329.223692	8.491994
5.720413	327.632156	8.497011
6.004556	347.068132	8.502029
5.951155	337.120055	8.507046
6.000024	335.092696	8.512064
5.848499	345.489409	8.517082
5.842692	357.766223	8.522099
6.045751	347.553899	8.527117
5.639700	346.604504	8.532134
5.987024	351.501461	8.537152
6.209345	353.085519	8.542170
6.149338	354.628607	8.547187
6.367837	355.257067	8.552205
5.773253	347.738510	8.557223
6.062320	339.264163	8.562240
5.694767	346.905032	8.567258
6.075007	348.760988	8.572275
6.099703	347.340166	8.577293
6.016103	350.480610	8.582311
6.027480	353.763961	8.587328
6.077330	357.085466	8.592346
5.912521	357.493121	8.597363
6.292032	360.377972	8.602381
5.742281	353.511942	8.607399
6.134089	355.886788	8.612416
5.818217	361.234792	8.617434
5.802271	357.232610	8.622451
5.726698	352.059515	8.627469
5.756205	360.370315	8.632487
6.056372	347.760174	8.637504
5.878138	359.533836	8.642522
5.857285	350.723039	8.647539
6.187414	359.043541	8.652557
5.930744	356.947288	8.657575
6.199107	351.174358	8.662592
6.193853	354.602325	8.667610
6.188146	353.347210	8.672627
6.062520	357.103302	8.677645
6.020762	357.845122	8.682663
6.411769	355.802024	8.687680
6.033875	354.447434	8.692698
6.089082	357.376785	8.697715
5.999480	357.040519	8.702733
6.106618	364.057917	8.707751
6.277657	378.749599	8.712768
6.320593	384.287542	8.717786
6.017598	387.534950	8.722803
6.241398	382.289694	8.727821
6.477369	386.251066	8.732839
6.410950	370.943359	8.737856
5.923130	358.917414	8.742874
6.072909	368.389629	8.747891
6.273089	375.117902	8.752909
6.280007	376.568456	8.757927
6.416204	378.797163	8.762944
6.244253	370.694832	8.767962
6.204016	368.394256	8.772979
6.479327	366.359816	8.777997
5.935495	370.449676	8.783015
6.142309	370.792793	8.788032
5.941728	379.092315	8.793050
6.017575	382.027903	8.798067
6.496294	371.863893	8.803085
6.319332	373.781908	8.808103
6.277836	373.999830	8.813120
6.213040	379.529405	8.818138
6.095012	376.262728	8.823155
6.367800	378.842415	8.828173
6.139567	388.686289	8.833191
5.954014	376.821253	8.838208
6.129026	386.576699	8.843226
6.343477	386.268532	8.848243
6.324391	372.632276	8.853261
6.296356	372.163288	8.858279
6.195594	373.501327	8.863296
6.220603	379.196709	8.868314
6.003361	375.229217	8.873331
6.397079	384.536990	8.878349
6.628220	398.588118	8.883367
6.313648	388.002443	8.888384
6.387181	379.653364	8.893402
6.631017	390.679272	8.898419
6.356561	378.995420	8.903437
6.298874	380.200479	8.908455
6.572241	386.784747	8.913472
6.367088	384.443736	8.918490
6.457560	378.774408	8.923507
6.322847	378.770253	8.928525
6.505166	387.675654	8.933543
6.539891	387.272571	8.938560
6.552000	390.811432	8.943578
5.914837	379.853431	8.948595
6.337232	393.309707	8.953613
6.833630	392.515556	8.958631
7.156671	407.274964	8.963648
6.787276	391.929503	8.968666
6.687689	389.196415	8.973683
6.329722	387.554682	8.978701
6.227853	382.505617	8.983719
6.436946	376.139214	8.988736
6.703967	390.254141	8.993754
6.518839	387.001131	8.998771
6.649150	386.381102	9.003789
6.365788	383.048811	9.008807
6.552107	381.372291	9.013824
6.645946	384.024198	9.018842
6.221784	376.715609	9.023859
6.598763	377.783138	9.028877
6.489241	383.739439	9.033895
6.646279	389.445696	9.038912
6.813189	392.183983	9.043930
6.699189	384.728966	9.048947
6.636831	374.201611	9.053965
6.196790	384.889701	9.058983
6.066007	381.757564	9.064000
6.401911	397.881396	9.069018
6.460916	407.838065	9.074035
6.938937	403.802658	9.079053
7.135300	411.285772	9.084071
6.905950	397.985396	9.089088
6.665765	388.722956	9.094106
6.684613	380.934705	9.099123
6.337992	391.437751	9.104141
6.700699	394.385200	9.109159
6.687020	406.922054	9.114176
6.763884	408.257510	9.119194
6.761477	405.992027	9.124211
6.786999	396.037863	9.129229
6.521760	385.274048	9.134247
6.515200	393.464284	9.139264
6.869564	397.615389	9.144282
6.766361	402.545080	9.149299
6.855188	401.025844	9.154317
6.906745	394.052963	9.159335
6.268199	389.731761	9.164352
6.935559	400.110654	9.169370
6.720910	398.698927	9.174387
7.154797	393.903584	9.179405
7.165973	386.836048	9.184423
6.669559	379.952185	9.189440
6.690179	375.502462	9.194458
6.357732	377.009343	9.199475
6.815778	373.355764	9.204493
7.096792	385.291016	9.209511
6.853732	380.917318	9.214528
6.885313	380.779812	9.219546
6.663306	379.460756	9.224563
6.676057	377.413805	9.229581
6.358534	383.481589	9.234599
6.348136	392.896864	9.239616
6.898798	399.699619	9.244634
6.785162	402.699613	9.249651
7.104981	405.407633	9.254669
7.039961	399.342944	9.259687
6.990951	410.288515	9.264704
7.041654	404.593852	9.269722
6.802849	402.030896	9.274739
7.056304	405.001776	9.279757
7.303854	403.441892	9.284775
6.666660	387.810193	9.289792
6.735323	384.902423	9.294810
6.652952	395.906861	9.299827
6.924992	396.113528	9.304845
7.096498	407.292788	9.309863
6.795271	411.732806	9.314880
7.057699	395.467847	9.319898
6.880114	415.834611	9.324915
7.223169	409.917417	9.329933
7.084147	412.511140	9.334951
6.927396	400.240792	9.339968
6.967406	394.857073	9.344986
6.681042	400.967318	9.350003
7.004871	404.258528	9.355021
6.853887	406.690023	9.360039
6.650702	414.604966	9.365056
7.065698	405.874174	9.370074
6.835167	406.547744	9.375091
6.807349	402.635774	9.380109
6.729742	391.208247	9.385127
6.899648	409.027500	9.390144
7.278450	400.431769	9.395162
6.865555	418.326566	9.400179
7.019195	403.735426	9.405197
7.446067	401.358503	9.410215
7.447605	398.514896	9.415232
7.404193	400.415145	9.420250
7.284598	409.311057	9.425267
6.914673	405.348546	9.430285
7.343461	403.870718	9.435303
6.719281	408.661133	9.440320
6.877267	400.431355	9.445338
6.692776	410.094820	9.450355
7.034241	403.057578	9.455373
6.976419	397.651318	9.460391
6.851615	406.213532	9.465408
7.201214	399.683096	9.470426
7.102677	409.471947	9.475443
7.280141	400.134597	9.480461
7.527515	395.052900	9.485479
6.849424	402.294328	9.490496
7.326421	397.296572	9.495514
7.151121	397.611198	9.500531
7.168356	405.090818	9.505549
7.427845	407.606322	9.510567
7.275963	408.393800	9.515584
7.353888	402.445567	9.520602
7.257533	410.451065	9.525619
7.201067	401.901441	9.530637
7.430778	399.460736	9.535655
7.155201	400.769362	9.540672
7.283583	395.406511	9.545690
6.990635	405.651849	9.550707
7.370005	404.951772	9.555725
7.472621	404.241409	9.560743
7.171738	402.401384	9.565760
7.144749	401.130665	9.570778
6.983643	409.613363	9.575795
7.035993	409.226452	9.580813
7.112087	408.229913	9.585831
6.660888	415.426329	9.590848
7.028039	408.195714	9.595866
7.383591	423.735829	9.600883
7.338742	431.089488	9.605901
7.603741	421.725789	9.610919
7.668372	427.743180	9.615936
7.670339	422.321232	9.620954
7.445208	411.333369	9.625971
6.904490	407.899385	9.630989
7.025842	407.135594	9.636007
7.049038	419.035524	9.641024
7.427412	419.897711	9.646042
7.437423	429.353989	9.651059
7.591252	427.717269	9.656077
7.452043	430.254219	9.661095
7.317095	430.287970	9.666112
7.516708	423.531720	9.671130
7.398003	424.197237	9.676147
7.726277	434.083329	9.681165
7.337815	426.333629	9.686183
7.371184	431.222996	9.691200
7.520389	420.769762	9.696218
7.359677	422.874583	9.701235
7.410864	430.402541	9.706253
7.357769	422.852760	9.711271
7.691057	440.343492	9.716288
7.308363	428.370456	9.721306
7.308074	436.061115	9.726323
7.291883	437.710953	9.731341
7.821929	431.988514	9.736359
7.144735	439.583263	9.741376
7.605795	426.894210	9.746394
7.557137	441.434175	9.751411
7.799557	436.372177	9.756429
7.832316	434.738648	9.761447
7.404100	428.651959	9.766464
7.551459	430.493919	9.771482
7.565802	434.297524	9.776499
7.684851	439.858272	9.781517
7.603658	434.742838	9.786535
7.600782	439.868258	9.791552
7.815554	432.469005	9.796570
7.883072	431.852502	9.801587
7.544697	407.795379	9.806605
7.470052	413.238145	9.811623
7.422976	425.477291	9.816640
7.759930	421.012706	9.821658
7.588737	437.626277	9.826675
7.781155	434.077421	9.831693
7.894755	428.174082	9.836711
7.348105	415.096975	9.841728
7.504456	414.008967	9.846746
7.917996	422.815042	9.851763
7.409818	424.403108	9.856781
7.702835	426.957543	9.861799
7.304059	434.675923	9.866816
7.351624	436.546143	9.871834
7.822304	429.132043	9.876851
7.626979	436.809080	9.881869
7.679563	428.210799	9.886887
7.641740	433.556285	9.891904
7.418482	433.875269	9.896922
7.793426	438.588044	9.901939
7.149534	434.201397	9.906957
7.102912	426.177233	9.911975
7.736480	444.365684	9.916992
7.980602	446.220888	9.922010
7.983935	451.828172	9.927027
7.472163	451.141486	9.932045
8.060690	442.001639	9.937063
7.881740	455.205044	9.942080
8.212599	446.159215	9.947098
8.037259	444.400500	9.952115
7.495422	433.739953	9.957133
7.978795	429.757350	9.962151
7.600109	435.140464	9.967168
7.678592	433.237841	9.972186
8.096749	434.961634	9.977203
7.994742	436.637541	9.982221
8.058388	438.603070	9.987239
7.781896	434.859442	9.992256
7.603571	431.759990	9.997274
7.860484	433.837248	10.002291
7.921811	443.452749	10.007309
7.859756	442.209612	10.012327
7.687440	445.584877	10.017344
8.215279	449.011387	10.022362
8.297924	449.534906	10.027379
7.838042	443.557314	10.032397
7.925961	427.512171	10.037415
7.717677	427.989753	10.042432
7.892555	441.027259	10.047450
8.038498	449.143133	10.052467
7.681844	448.741410	10.057485
8.178662	457.007438	10.062503
8.375061	462.701240	10.067520
7.789030	447.957715	10.072538
7.922344	446.494620	10.077555
7.917129	451.995947	10.082573
7.818866	459.515776	10.087591
7.949747	459.908662	10.092608
8.217663	462.776301	10.097626
8.071312	457.229260	10.102643
7.936555	456.451945	10.107661
7.912930	459.204317	10.112679
7.922872	452.455683	10.117696
8.029346	456.503632	10.122714
8.042118	456.135544	10.127731
7.958739	457.972634	10.132749
8.250221	452.416955	10.137767
8.081704	465.827015	10.142784
8.024041	454.080745	10.147802
7.825430	454.995466	10.152819
7.858427	458.477420	10.157837
8.351132	460.347325	10.162855
8.248210	453.098825	10.167872
8.003133	453.616887	10.172890
8.279790	455.347075	10.177907
8.397534	454.918359	10.182925
8.228219	460.893521	10.187943
8.415074	463.309961	10.192960
8.343953	466.435847	10.197978
8.460907	457.265737	10.202995
8.285477	459.988246	10.208013
8.504036	455.769419	10.213031
8.357174	463.287397	10.218048
7.973265	460.191750	10.223066
8.681377	465.205779	10.228083
7.924719	465.709322	10.233101
8.259421	465.751539	10.238119
8.196391	456.136262	10.243136
8.238843	468.235178	10.248154
8.652263	457.500686	10.253171
8.431833	463.345003	10.258189
8.426566	453.897401	10.263207
8.069876	446.253166	10.268224
8.335342	460.043347	10.273242
8.701791	454.223458	10.278259
8.335803	444.961765	10.283277
8.145016	436.679320	10.288295
7.967552	447.342086	10.293312
8.430075	460.975161	10.298330
8.466398	459.094920	10.303347
8.374406	462.675352	10.308365
8.295823	461.800874	10.313383
8.062327	462.812579	10.318400
8.373386	463.691627	10.323418
8.357205	451.986196	10.328435
8.382838	465.034479	10.333453
8.491711	461.274647	10.338471
8.112336	456.852861	10.343488
8.477176	456.830396	10.348506
8.257573	448.978490	10.353523
8.304076	461.146194	10.358541
8.544864	454.187822	10.363559
8.366529	457.128534	10.368576
8.225808	454.086303	10.373594
8.309162	457.494095	10.378611
8.168883	465.178299	10.383629
8.224659	461.379449	10.388647
8.472089	463.073191	10.393664
8.287349	472.370657	10.398682
8.547111	476.924765	10.403699
8.602821	485.300945	10.408717
8.651321	483.582894	10.413735
8.645709	476.114013	10.418752
8.561655	473.280649	10.423770
8.525812	466.491845	10.428787
8.574373	471.962663	10.433805
8.877240	469.873401	10.438823
8.469554	462.719985	10.443840
8.299577	460.988831	10.448858
8.877204	473.221648	10.453875
8.664239	469.297646	10.458893
8.615935	467.216070	10.463911
8.308572	471.451937	10.468928
8.604540	480.579417	10.473946
8.666632	483.072212	10.478963
8.749961	483.090698	10.483981
8.827528	491.192059	10.488999
8.861651	471.346269	10.494016
8.409707	470.994189	10.499034
8.497266	474.593828	10.504051
8.700351	477.238099	10.509069
8.527064	483.415861	10.514087
8.786133	488.926284	10.519104
8.828109	498.964566	10.524122
8.736002	486.860755	10.529139
8.803545	492.214996	10.534157
8.452384	492.437257	10.539175
8.883752	483.227339	10.544192
8.889085	489.566464	10.549210
8.926307	476.855420	10.554227
8.813268	487.261964	10.559245
8.520133	481.965130	10.564263
8.513490	480.429287	10.569280
8.720566	482.403907	10.574298
8.915983	479.741348	10.579315
8.770963	481.423998	10.584333
8.655655	490.776867	10.589351
8.849056	479.243706	10.594368
8.932386	488.290898	10.599386
8.768811	477.624707	10.604403
8.630760	481.281786	10.609421
8.747822	487.379344	10.614439
8.821205	483.205348	10.619456
8.910154	491.336483	10.624474
8.895419	487.921058	10.629491
8.743264	493.552717	10.634509
9.046405	487.045308	10.639527
8.786604	488.622867	10.644544
8.853593	493.364972	10.649562
8.875950	485.011240	10.654579
8.990195	490.721078	10.659597
8.570321	490.739512	10.664615
8.797315	487.715400	10.669632
8.684256	495.581543	10.674650
9.257264	503.292860	10.679667
9.315470	499.796578	10.684685
9.214258	493.428259	10.689703
9.182084	481.883103	10.694720
8.629268	492.743560	10.699738
8.872686	494.718799	10.704755
9.261710	484.609803	10.709773
9.068854	490.787478	10.714791
9.338980	474.183572	10.719808
9.111891	478.722443	10.724826
9.043364	484.830143	10.729843
9.123038	493.019536	10.734861
9.167767	486.369579	10.739879
9.055907	479.794652	10.744896
8.954392	482.634970	10.749914
8.945158	476.391101	10.754931
9.078980	485.525054	10.759949
9.099406	489.204642	10.764967
9.335783	476.446616	10.769984
9.027118	481.133967	10.775002
9.043467	480.923108	10.780019
9.133481	486.494731	10.785037
8.965476	490.279582	10.790055
8.909702	496.259056	10.795072
9.083269	505.468843	10.800090
9.317218	516.922409	10.805107
9.222046	513.096706	10.810125
9.427716	514.014359	10.815143
9.489796	508.791250	10.820160
9.716167	510.024394	10.825178
9.327746	495.735859	10.830195
9.260425	486.099148	10.835213
9.095240	485.964068	10.840231
9.515287	491.225209	10.845248
8.990726	488.583937	10.850266
9.144610	485.120003	10.855283
9.333093	482.562671	10.860301
9.053941	488.435131	10.865319
9.314640	494.557524	10.870336
9.367971	505.540767	10.875354
9.557487	511.241975	10.880371
9.564155	498.996448	10.885389
8.902065	494.865099	10.890407
9.435472	495.762960	10.895424
9.061194	503.509090	10.900442
9.177621	501.843510	10.905459
9.779601	504.945992	10.910477
9.278585	514.564432	10.915495
9.642615	504.554015	10.920512
9.623650	510.029112	10.925530
9.379790	509.401433	10.930547
9.680430	501.445902	10.935565
9.444157	504.566113	10.940583
9.502234	486.275514	10.945600
9.333022	489.031766	10.950618
9.315356	491.909441	10.955635
9.537489	505.059510	10.960653
9.487566	510.088179	10.965671
9.802518	510.067219	10.970688
9.662504	509.476917	10.975706
9.375239	502.759051	10.980723
9.608165	502.066137	10.985741
9.432581	501.651821	10.990759
9.682896	502.739203	10.995776
9.624642	506.364851	11.000794
9.461875	494.941133	11.005811
9.520674	496.279426	11.010829
9.778659	502.241301	11.015847
9.634121	492.206432	11.020864
9.169614	493.749793	11.025882
9.336256	499.609214	11.030899
9.599403	499.545878	11.035917
9.761140	513.923551	11.040935
9.870492	500.604744	11.045952
9.759716	510.354543	11.050970
9.547074	514.383076	11.055987
9.713503	497.441947	11.061005
9.728459	508.191365	11.066023
9.776160	500.329114	11.071040
9.825194	500.984131	11.076058
9.704618	504.957212	11.081075
9.741695	497.699383	11.086093
9.514324	505.381470	11.091111
9.791684	501.838227	11.096128
9.553662	498.132738	11.101146
9.978618	507.773351	11.106163
9.978634	502.812430	11.111181
9.707831	508.326985	11.116199
9.843016	502.694793	11.121216
9.815037	499.963092	11.126234
9.783277	509.523785	11.131251
9.743710	510.612406	11.136269
9.792448	509.708509	11.141287
9.482239	505.869163	11.146304
9.934533	502.550974	11.151322
9.741466	508.286877	11.156339
9.895311	501.462029	11.161357
9.779753	508.302938	11.166375
9.754558	506.883608	11.171392
9.545890	505.114330	11.176410
9.650277	509.897917	11.181427
9.612767	503.002065	11.186445
9.548289	519.936662	11.191463
9.560901	505.266550	11.196480
9.735194	510.446281	11.201498
9.465291	524.055306	11.206515
10.061432	531.955515	11.211533
9.835515	524.685232	11.216551
10.093075	525.045648	11.221568
10.002748	536.906639	11.226586
10.004116	538.272869	11.231603
10.140868	526.496090	11.236621
9.919790	534.492783	11.241639
9.995378	526.768162	11.246656
9.802219	531.828747	11.251674
9.905772	538.278732	11.256691
10.170799	531.016732	11.261709
10.117721	535.903893	11.266727
9.808256	530.145700	11.271744
9.889399	533.244585	11.276762
9.499833	535.868113	11.281779
9.896387	528.765386	11.286797
9.733994	529.065369	11.291815
9.924052	539.272976	11.296832
10.251058	536.220563	11.301850
10.228900	540.339177	11.306867
10.251288	534.503743	11.311885
10.095085	544.358507	11.316903
10.147341	540.288794	11.321920
10.201635	539.885797	11.326938
10.238289	539.924219	11.331955
10.225624	528.499052	11.336973
10.032812	531.574589	11.341991
10.155682	539.820351	11.347008
10.331511	550.099621	11.352026
10.158113	564.668699	11.357043
10.437337	558.688874	11.362061
10.188169	551.040371	11.367079
10.170039	546.243227	11.372096
10.571147	545.088460	11.377114
10.278394	543.322885	11.382131
10.012197	543.497121	11.387149
10.225225	544.322105	11.392167
10.170310	564.925439	11.397184
10.574703	554.189148	11.402202
10.339165	561.430727	11.407219
10.876273	553.643251	11.412237
10.432841	550.449616	11.417255
10.462599	540.194908	11.422272
10.516609	539.930810	11.427290
10.462790	535.117171	11.432307
10.617493	530.876774	11.437325
10.425789	533.885865	11.442343
10.060888	529.755282	11.447360
10.450411	525.534899	11.452378
10.155822	533.031871	11.457395
10.283598	531.036308	11.462413
9.944525	539.332356	11.467431
10.170515	551.651880	11.472448
10.196110	551.875072	11.477466
10.230557	553.747360	11.482483
10.468527	545.549165	11.487501
10.516117	544.790613	11.492519
10.423979	553.391961	11.497536
10.508984	553.069358	11.502554
10.182612	560.908992	11.507571
10.378668	554.389934	11.512589
10.709543	563.385756	11.517607
10.781575	554.601330	11.522624
10.930302	554.142512	11.527642
10.704002	560.540045	11.532659
10.811123	551.683852	11.537677
10.405928	552.012409	11.542695
10.414077	557.880903	11.547712
10.454076	554.242296	11.552730
10.612341	557.931859	11.557747
10.874952	552.061937	11.562765
10.744928	561.600185	11.567783
10.828354	551.532721	11.572800
10.951649	557.638794	11.577818
10.755161	559.032869	11.582835
10.689193	550.131213	11.587853
10.676560	550.253097	11.592871
10.733568	556.464229	11.597888
10.793511	554.226828	11.602906
10.668481	556.354476	11.607923
10.628676	550.178487	11.612941
10.812766	548.669559	11.617959
10.593032	552.686589	11.622976
10.767806	546.584278	11.627994
10.363509	555.439662	11.633011
10.780063	553.499836	11.638029
10.873037	551.433985	11.643047
10.578740	559.205476	11.648064
10.708244	546.442054	11.653082
10.288782	552.080899	11.658099
10.981269	563.415315	11.663117
11.393800	582.427490	11.668135
11.010783	565.925833	11.673152
11.189949	553.189339	11.678170
11.179864	551.657186	11.683187
11.079212	547.179084	11.688205
10.909110	555.584365	11.693223
10.877450	549.889937	11.698240
11.129591	556.790018	11.703258
11.085327	549.210397	11.708275
10.941267	555.421474	11.713293
11.327860	549.753033	11.718311
10.903850	557.172463	11.723328
11.082832	552.546405	11.728346
10.763771	561.246427	11.733363
10.797731	553.771312	11.738381
11.027997	553.668947	11.743399
10.743212	557.901297	11.748416
10.840428	554.231634	11.753434
10.710512	553.229495	11.758451
10.578518	558.103780	11.763469
11.257028	572.451025	11.768487
11.074174	568.509659	11.773504
11.192510	579.804656	11.778522
10.795709	576.676293	11.783539
11.255275	574.732882	11.788557
11.607454	582.412562	11.793575
10.980799	564.169206	11.798592
11.084726	559.551750	11.803610
10.983483	566.576631	11.808627
11.253616	569.750053	11.813645
11.307713	575.762832	11.818663
11.253160	575.856571	11.823680
10.921898	568.959381	11.828698
10.954625	573.842575	11.833715
11.121249	575.867725	11.838733
11.660360	582.142185	11.843751
11.400005	588.693387	11.848768
11.668123	584.283729	11.853786
11.087803	561.110063	11.858803
11.223485	571.259936	11.863821
11.372182	563.119902	11.868839
10.926453	580.000681	11.873856
11.215400	572.211053	11.878874
11.364458	592.596268	11.883891
11.480039	583.164377	11.888909
11.575523	586.399879	11.893927
11.186442	582.456109	11.898944
11.537079	577.304533	11.903962
11.545321	586.426656	11.908979
11.474527	579.864192	11.913997
11.442685	576.255770	11.919015
11.171107	582.458434	11.924032
11.480218	574.769787	11.929050
11.279255	575.220980	11.934067
11.555099	579.015202	11.939085
11.545650	583.523155	11.944103
11.502605	582.964995	11.949120
11.434918	578.361800	11.954138
11.606854	575.784956	11.959155
11.324203	583.059172	11.964173
11.499869	576.032061	11.969191
11.053500	588.602122	11.974208
11.321821	569.593687	11.979226
11.256998	588.939437	11.984243
11.124235	577.286903	11.989261
11.348299	583.569700	11.994279
11.289519	592.547692	11.999296
11.034979	590.479480	12.004314
11.479912	601.029041	12.009331
11.467538	609.236065	12.014349
11.829467	609.027864	12.019367
11.634610	610.598413	12.024384
11.758031	611.292273	12.029402
11.975545	613.902746	12.034419
11.624694	613.493797	12.039437
12.105607	606.709183	12.044455
11.603102	615.851383	12.049472
11.887163	607.084205	12.054490
11.798035	600.631903	12.059507
11.568729	579.921550	12.064525
11.880498	588.854106	12.069543
11.736386	578.393088	12.074560
11.887813	569.526789	12.079578
11.657165	575.154993	12.084595
11.509573	576.815963	12.089613
12.059594	583.208636	12.094631
11.719733	597.806977	12.099648
12.106807	594.618911	12.104666
11.957710	582.946841	12.109683
11.909988	574.540931	12.114701
11.715151	578.651896	12.119719
11.558948	582.053064	12.124736
11.998911	585.341891	12.129754
12.423119	598.207903	12.134771
11.863537	589.894807	12.139789
11.835352	566.069736	12.144807
11.924915	571.685638	12.149824
12.054439	574.799041	12.154842
12.172011	576.437401	12.159859
11.604498	582.699055	12.164877
11.602975	579.524539	12.169895
11.476209	590.715933	12.174912
11.604861	592.560842	12.179930
12.038202	597.911450	12.184947
11.883572	608.488683	12.189965
12.170167	606.695446	12.194983
12.207918	604.972756	12.200000
12.136289	603.090479	12.205018
12.337087	610.746552	12.210035
12.304738	603.849851	12.215053
12.180981	598.700013	12.220071
12.221919	605.226105	12.225088
12.237447	606.659550	12.230106
12.505895	604.604068	12.235123
12.066765	594.949814	12.240141
12.174262	582.331825	12.245159
12.050936	588.362940	12.250176
12.058959	591.902481	12.255194
12.123069	594.663219	12.260211
12.269416	596.817780	12.265229
12.363413	600.877184	12.270247
11.910514	593.386816	12.275264
11.787068	599.657795	12.280282
12.352265	605.375910	12.285299
12.123916	609.845583	12.290317
12.255557	597.110193	12.295335
12.274877	604.292924	12.300352
12.135412	601.313586	12.305370
12.331171	605.284464	12.310387
11.961296	601.201980	12.315405
12.202875	602.562137	12.320423
12.236442	604.046403	12.325440
12.183831	598.105934	12.330458
12.334876	596.883046	12.335475
12.163410	595.972621	12.340493
12.316062	603.579430	12.345511
12.332720	613.504979	12.350528
12.112931	606.015951	12.355546
12.572208	606.376322	12.360563
12.132454	615.603365	12.365581
12.497940	616.025769	12.370599
12.479015	623.571106	12.375616
12.466732	616.541868	12.380634
12.953630	616.714875	12.385651
12.835047	614.549619	12.390669
12.672401	600.298209	12.395687
12.542928	600.129130	12.400704
12.212251	600.228262	12.405722
12.314601	593.603952	12.410739
12.239985	615.759932	12.415757
12.852173	619.539334	12.420775
12.722110	621.409002	12.425792
12.340657	607.794628	12.430810
12.325588	614.509380	12.435827
12.309782	616.676726	12.440845
12.879957	607.280895	12.445863
12.944369	616.318492	12.450880
12.486233	616.718461	12.455898
12.841192	627.013892	12.460915
12.502690	624.267707	12.465933
12.451132	620.952701	12.470951
12.468868	626.570406	12.475968
12.588156	624.348944	12.480986
12.531855	618.907664	12.486003
12.393430	622.448066	12.491021
12.697426	617.682484	12.496039
12.791438	621.713488	12.501056
12.795132	621.009148	12.506074
12.804254	619.341435	12.511091
12.806161	623.929670	12.516109
13.035759	618.718151	12.521127
12.657520	619.749387	12.526144
12.709141	616.951548	12.531162
13.029487	618.624413	12.536179
12.670617	618.336642	12.541197
12.980695	622.482116	12.546215
13.049754	624.377390	12.551232
12.705620	615.260507	12.556250
12.949402	627.700373	12.561267
12.718116	624.280981	12.566285
12.632673	619.920399	12.571303
12.859876	626.808635	12.576320
13.019526	641.496007	12.581338
13.589619	640.008644	12.586355
13.004707	627.297138	12.591373
12.783996	628.963258	12.596391
12.834652	620.784910	12.601408
12.697434	620.620201	12.606426
13.212794	639.568989	12.611443
12.859223	650.616074	12.616461
13.079541	649.341304	12.621479
13.415113	645.078853	12.626496
13.036243	657.692036	12.631514
13.482883	642.474124	12.636531
13.166008	638.190823	12.641549
13.200573	623.914807	12.646567
13.147985	614.916348	12.651584
12.671481	616.783491	12.656602
12.970590	626.955127	12.661619
13.360138	636.027000	12.666637
13.318518	633.480452	12.671655
13.394332	646.811341	12.676672
13.009981	640.711395	12.681690
13.388528	625.336908	12.686707
13.145650	651.120076	12.691725
13.225601	646.714639	12.696743
13.260465	642.593978	12.701760
12.756748	644.263415	12.706778
13.203707	638.298309	12.711795
13.376438	647.467274	12.716813
13.138729	639.258359	12.721831
13.509384	636.227492	12.726848
13.315730	646.571020	12.731866
13.405461	641.962079	12.736883
13.338553	641.388721	12.741901
13.480279	638.163349	12.746919
13.540663	639.343614	12.751936
13.200016	647.337001	12.756954
13.319922	641.300059	12.761971
13.254109	641.117851	12.766989
13.260245	638.970920	12.772007
13.298829	639.883201	12.777024
13.397655	644.607735	12.782042
13.428275	646.824616	12.787059
13.150557	639.496130	12.792077
13.265911	640.841353	12.797095
13.624674	650.413519	12.802112
13.345523	657.560984	12.807130
13.576753	650.376815	12.812147
13.709798	666.232871	12.817165
13.600284	658.401495	12.822183
13.791494	658.570337	12.827200
13.747319	665.864027	12.832218
13.931440	644.943655	12.837235
13.850657	636.852165	12.842253
13.734151	640.423850	12.847271
13.795634	631.666286	12.852288
13.729120	637.186742	12.857306
13.628361	634.210802	12.862323
13.365416	645.934809	12.867341
13.430946	637.684695	12.872359
13.745402	648.990032	12.877376
13.706131	651.637588	12.882394
14.151278	650.160333	12.887411
13.567384	646.161864	12.892429
13.953875	638.555741	12.897447
14.082694	625.016040	12.902464
13.664655	636.827457	12.907482
13.888204	638.124170	12.912499
14.029637	638.064125	12.917517
13.542198	646.314041	12.922535
13.588672	637.467307	12.927552
13.676511	652.983295	12.932570
14.049394	655.821897	12.937587
13.910054	669.363238	12.942605
13.703117	668.423653	12.947623
14.075394	662.580694	12.952640
13.539687	660.701694	12.957658
13.914271	663.577900	12.962675
14.148419	666.902145	12.967693
13.793998	670.182907	12.972711
14.188946	667.170320	12.977728
14.378654	671.634468	12.982746
14.558644	664.139584	12.987763
14.174626	660.807231	12.992781
13.998111	648.915352	12.997799
14.264756	642.729186	13.002816
13.844551	644.679029	13.007834
14.024067	657.914783	13.012851
13.628998	668.084753	13.017869
13.793292	668.324085	13.022887
14.175577	668.702832	13.027904
13.933989	673.840473	13.032922
14.186922	665.400037	13.037939
14.253013	666.352191	13.042957
14.208126	674.207732	13.047975
14.423353	664.624485	13.052992
13.798221	675.575278	13.058010
13.872092	663.546328	13.063027
14.085341	667.378779	13.068045
13.953430	663.479904	13.073063
14.542054	660.635790	13.078080
14.229035	668.422885	13.083098
14.133417	663.334892	13.088115
14.250906	668.154339	13.093133
14.466533	674.113440	13.098151
14.741531	656.814321	13.103168
14.380456	673.401057	13.108186
14.065298	661.811759	13.113203
14.448870	660.905887	13.118221
14.061180	666.640776	13.123239
14.351409	673.500221	13.128256
14.560457	689.177132	13.133274
14.556028	689.234615	13.138291
14.390003	678.726478	13.143309
14.487176	690.201586	13.148327
14.555270	682.844147	13.153344
14.426627	692.625247	13.158362
14.590075	688.967270	13.163379
14.588269	685.928480	13.168397
14.421151	694.380696	13.173415
14.616461	693.232918	13.178432
14.361694	694.191164	13.183450
14.726105	697.630706	13.188467
14.521332	691.073414	13.193485
14.251083	694.609237	13.198503
14.594606	698.534893	13.203520
14.933862	692.072245	13.208538
14.698208	688.350566	13.213555
14.906073	687.039874	13.218573
14.538678	694.330568	13.223591
14.697914	691.354909	13.228608
14.715889	691.765490	13.233626
15.288702	683.558951	13.238643
14.980304	685.970965	13.243661
14.311742	679.265436	13.248679
14.456744	674.218635	13.253696
14.892656	683.472617	13.258714
14.907515	679.361394	13.263731
14.910091	687.774396	13.268749
14.714960	690.749336	13.273767
15.144603	677.272917	13.278784
14.961339	689.199064	13.283802
14.664720	685.259718	13.288819
15.176259	686.053718	13.293837
14.991883	683.860891	13.298855
15.249231	684.656848	13.303872
15.071486	676.514259	13.308890
14.717667	668.266717	13.313907
15.138762	664.574689	13.318925
14.480230	686.838024	13.323943
14.825201	675.826946	13.328960
14.861448	677.541174	13.333978
14.871061	695.966500	13.338995
15.172263	689.913760	13.344013
14.798783	686.150560	13.349031
14.998271	689.549668	13.354048
14.780167	682.555808	13.359066
15.107186	684.224479	13.364083
15.287042	683.448354	13.369101
14.817558	683.307300	13.374119
14.820945	678.917007	13.379136
14.817823	685.393226	13.384154
15.096129	696.745284	13.389171
15.573271	706.122207	13.394189
15.275212	693.876953	13.399207
15.313696	685.097720	13.404224
15.099561	680.056693	13.409242
15.261452	682.095220	13.414259
15.263438	678.784437	13.419277
15.175660	692.425015	13.424295
15.219786	685.693027	13.429312
15.332237	694.139310	13.434330
15.263433	695.636468	13.439347
15.332176	701.605970	13.444365
15.166713	711.048864	13.449383
15.578115	705.669978	13.454400
15.473944	700.482328	13.459418
15.297373	702.034241	13.464435
15.727679	710.029941	13.469453
15.268123	702.935047	13.474471
15.289089	690.911212	13.479488
15.602282	696.577323	13.484506
15.454610	706.134192	13.489523
15.715421	694.416760	13.494541
15.498104	698.319834	13.499559
15.331740	684.618053	13.504576
15.462600	706.136034	13.509594
15.616917	701.816761	13.514611
15.856183	699.210416	13.519629
15.569473	699.965383	13.524647
15.430225	686.224638	13.529664
15.437653	687.514190	13.534682
15.548329	695.638858	13.539699
15.795429	703.170951	13.544717
15.670621	703.988914	13.549735
15.794698	704.666895	13.554752
15.715793	702.710008	13.559770
15.338609	707.212492	13.564787
15.850564	699.006013	13.569805
15.636382	702.659286	13.574823
15.819124	708.585683	13.579840
15.999201	703.498664	13.584858
15.595054	712.464556	13.589875
15.707942	705.412516	13.594893
15.645619	711.153246	13.599911
15.698667	705.073109	13.604928
16.007401	707.183306	13.609946
15.723645	702.891644	13.614963
16.066395	701.058042	13.619981
16.190421	703.556943	13.624999
16.276531	704.900440	13.630016
16.326178	700.032675	13.635034
15.618026	698.947555	13.640051
15.739686	688.975009	13.645069
15.953504	703.287870	13.650087
16.208784	689.299114	13.655104
16.338713	698.487435	13.660122
15.711312	697.620038	13.665139
16.086329	696.627141	13.670157
15.701009	706.218089	13.675175
15.820836	705.072670	13.680192
16.215145	697.323284	13.685210
15.955556	704.909519	13.690227
16.156061	698.538035	13.695245
15.805382	696.478561	13.700263
15.776145	690.670099	13.705280
15.840001	699.101908	13.710298
16.060911	703.100425	13.715315
16.028445	696.437238	13.720333
15.811887	707.425022	13.725351
16.023337	712.709445	13.730368
16.094518	727.136192	13.735386
15.755077	727.116775	13.740403
16.291189	723.072197	13.745421
16.315499	730.598182	13.750439
16.371212	729.939336	13.755456
16.564743	726.762636	13.760474
16.144503	731.783117	13.765491
16.428786	725.594159	13.770509
16.334057	728.619647	13.775527
16.310999	719.483963	13.780544
16.482185	720.997171	13.785562
16.467042	719.257510	13.790579
16.744471	719.466494	13.795597
16.842876	727.189153	13.800615
16.342205	727.479023	13.805632
16.323809	721.062933	13.810650
16.478518	726.283666	13.815667
16.538643	717.661973	13.820685
16.384434	731.691689	13.825703
16.467798	721.753528	13.830720
16.699913	724.418535	13.835738
16.234003	730.885228	13.840755
16.555334	727.590674	13.845773
16.482002	732.121297	13.850791
16.396950	729.556294	13.855808
16.411789	723.766162	13.860826
16.327573	731.141892	13.865843
16.204952	720.702670	13.870861
16.573611	725.116703	13.875879
16.606357	742.437068	13.880896
16.676582	741.141626	13.885914
16.494096	751.079518	13.890931
16.906664	746.385254	13.895949
17.092079	743.528562	13.900967
17.071222	747.624929	13.905984
17.009484	739.290565	13.911002
16.542470	732.480853	13.916019
16.810674	730.065631	13.921037
16.795793	740.273905	13.926055
17.032330	745.279850	13.931072
17.105750	733.724298	13.936090
16.664216	723.265612	13.941107
16.465418	731.849043	13.946125
16.897835	736.489777	13.951143
16.956397	743.467598	13.956160
17.119155	744.202637	13.961178
16.815162	756.725262	13.966195
17.066535	744.961939	13.971213
17.019280	755.402513	13.976231
17.113375	750.240590	13.981248
17.152453	745.863622	13.986266
16.933355	746.014700	13.991283
17.126984	751.674315	13.996301
17.180346	756.150380	14.001319
17.160281	749.630399	14.006336
16.955134	743.814766	14.011354
17.212297	748.858506	14.016371
17.213012	739.488711	14.021389
17.085043	738.025505	14.026407
17.023100	749.885346	14.031424
17.252398	742.272249	14.036442
17.018865	751.508077	14.041459
17.138373	750.570989	14.046477
16.985814	744.526209	14.051495
17.180436	753.360437	14.056512
17.058400	740.891910	14.061530
17.123888	753.372422	14.066547
17.113583	753.140489	14.071565
17.322966	759.981076	14.076583
17.414290	777.134505	14.081600
17.827261	773.787714	14.086618
17.422984	767.091237	14.091635
17.222352	756.976644	14.096653
17.544143	755.345137	14.101671
17.418198	764.886010	14.106688
17.741519	757.185592	14.111706
17.302856	760.337556	14.116723
17.647212	752.715896	14.121741
17.812501	754.842262	14.126759
17.626874	749.553750	14.131776
17.506390	748.603770	14.136794
17.635360	745.948427	14.141811
17.500715	743.214466	14.146829
17.790657	742.055014	14.151847
17.542789	748.992485	14.156864
17.829028	746.637551	14.161882
17.864100	738.231215	14.166899
17.458623	749.848233	14.171917
17.818083	749.009251	14.176935
17.387366	749.600588	14.181952
17.685391	742.598422	14.186970
17.433010	747.810359	14.191987
17.727767	759.387100	14.197005
18.239387	769.926313	14.202023
17.634626	764.627726	14.207040
17.741934	761.855853	14.212058
17.724547	770.196282	14.217075
17.711944	768.105921	14.222093
17.983927	770.177702	14.227111
17.683919	781.610956	14.232128
17.879622	772.371541	14.237146
17.880241	772.655454	14.242163
17.736897	770.973745	14.247181
17.900141	769.878324	14.252199
17.470721	774.758242	14.257216
17.829243	767.623510	14.262234
17.843263	775.943242	14.267251
17.736411	772.674740	14.272269
17.762736	778.751900	14.277287
17.734191	784.462115	14.282304
18.030701	792.532464	14.287322
18.191378	790.550653	14.292339
18.228175	799.340202	14.297357
18.294792	797.521452	14.302375
18.154236	797.575017	14.307392
18.424806	794.301027	14.312410
18.358991	796.271101	14.317427
18.120220	785.442935	14.322445
18.059654	776.054320	14.327463
18.028770	792.892393	14.332480
18.304750	796.863368	14.337498
18.102095	792.082446	14.342515
18.540730	790.745057	14.347533
18.606918	791.504697	14.352551
18.277496	796.384732	14.357568
18.389694	796.307176	14.362586
18.351082	793.334096	14.367603
18.258676	794.292155	14.372621
18.655320	793.065489	14.377639
18.120214	795.550908	14.382656
18.166859	790.664654	14.387674
18.454955	794.059367	14.392691
18.316129	796.675204	14.397709
18.513809	792.945570	14.402727
18.076750	792.455448	14.407744
18.364158	795.077088	14.412762
18.344949	795.016965	14.417779
18.265326	783.311789	14.422797
18.894666	785.942971	14.427815
18.489684	795.275112	14.432832
18.641163	791.044626	14.437850
18.588450	797.777968	14.442867
18.564079	795.140332	14.447885
18.577987	785.620121	14.452903
18.783995	810.395904	14.457920
18.793415	790.929175	14.462938
18.803444	795.187974	14.467955
18.792376	794.331303	14.472973
18.684625	789.418746	14.477991
18.822279	787.891827	14.483008
18.952884	797.452483	14.488026
18.788689	795.751948	14.493043
18.728444	795.613047	14.498061
19.002150	794.670732	14.503079
18.959607	788.375168	14.508096
18.983782	788.860520	14.513114
19.031620	785.460481	14.518131
18.672727	786.485539	14.523149
18.901779	780.658670	14.528167
18.810564	800.308588	14.533184
19.101443	809.323425	14.538202
19.001332	822.249658	14.543219
19.060109	813.315701	14.548237
18.931844	811.581133	14.553255
19.276987	814.004379	14.558272
19.369117	807.182772	14.563290
19.085236	801.840210	14.568307
18.882615	792.688440	14.573325
19.203947	798.861399	14.578343
19.145831	812.958175	14.583360
19.569250	808.079156	14.588378
19.324384	790.081866	14.593395
19.052421	786.280648	14.598413
19.188656	791.034074	14.603431
19.002021	803.674045	14.608448
19.250200	809.915274	14.613466
19.554008	812.859399	14.618483
19.181587	814.700787	14.623501
19.608452	802.499670	14.628519
19.263969	814.274433	14.633536
19.274844	818.561507	14.638554
19.342023	810.888574	14.643571
19.170602	812.884663	14.648589
19.302482	808.714050	14.653607
19.300301	809.437064	14.658624
19.260081	810.538428	14.663642
19.739581	806.616312	14.668659
19.498251	814.666796	14.673677
19.298400	811.586430	14.678695
19.482156	817.642093	14.683712
19.188959	808.135273	14.688730
19.418398	805.836570	14.693747
19.292601	821.102151	14.698765
19.538197	811.435171	14.703783
19.636580	828.237245	14.708800
19.662920	823.530890	14.713818
20.094428	823.551630	14.718835
19.617282	822.796385	14.723853
19.713410	817.441617	14.728871
19.694482	809.078423	14.733888
19.532135	813.140168	14.738906
19.699458	830.988651	14.743923
19.993370	839.100455	14.748941
19.987522	826.512677	14.753959
19.603672	834.437175	14.758976
19.753809	833.321713	14.763994
19.968699	827.433931	14.769011
19.494903	831.594972	14.774029
19.667312	835.828339	14.779047
19.781874	836.185920	14.784064
19.868339	838.542400	14.789082
20.234403	826.224560	14.794099
20.240473	832.380652	14.799117
20.266505	830.442023	14.804135
20.082357	832.945045	14.809152
20.099883	834.684311	14.814170
20.424779	832.872428	14.819187
20.318509	831.449996	14.824205
20.171043	836.718106	14.829223
20.071675	830.952144	14.834240
19.726577	833.631864	14.839258
20.106102	818.477968	14.844275
20.053916	829.316995	14.849293
20.060109	827.914813	14.854311
20.264460	834.074554	14.859328
19.879169	830.256368	14.864346
19.988519	831.574143	14.869363
19.675605	839.995622	14.874381
19.854194	827.568296	14.879399
20.183550	846.944085	14.884416
20.086000	853.457252	14.889434
20.193767	850.631643	14.894451
20.286389	857.878732	14.899469
20.681600	852.215157	14.904487
20.730239	854.956268	14.909504
20.424420	857.784474	14.914522
20.852137	851.197454	14.919539
20.549467	859.771973	14.924557
20.485307	856.708210	14.929575
20.697505	858.357017	14.934592
20.480092	852.978778	14.939610
20.685182	849.058620	14.944627
20.933167	851.822147	14.949645
20.958935	832.346500	14.954663
20.830445	820.737319	14.959680
20.142487	825.686160	14.964698
20.488918	820.374226	14.969715
20.574526	833.908850	14.974733
20.583384	837.501959	14.979751
20.888364	845.845564	14.984768
20.749479	848.145833	14.989786
21.230852	850.377324	14.994803
20.622630	850.690358	14.999821
20.871236	834.578647	15.004839
20.724876	844.946438	15.009856
20.598712	845.029306	15.014874
20.897999	844.114540	15.019891
20.769812	846.952783	15.024909
20.730908	849.723389	15.029927
20.702647	848.411811	15.034944
20.906037	847.890772	15.039962
21.190183	836.399969	15.044979
21.202875	850.387849	15.049997
20.875284	842.565312	15.055015
21.194548	842.988652	15.060032
21.168885	844.223439	15.065050
21.182242	848.279755	15.070067
20.998313	851.202473	15.075085
20.805386	851.046490	15.080103
21.224739	854.736234	15.085120
20.655454	856.747328	15.090138
20.920360	852.767303	15.095155
20.845424	851.040154	15.100173
21.347539	854.369788	15.105191
21.270065	845.245722	15.110208
20.754677	861.184612	15.115226
21.066000	871.468086	15.120243
21.382480	873.589714	15.125261
21.381624	872.523153	15.130279
21.221686	860.152001	15.135296
21.175722	873.170774	15.140314
21.244759	857.052463	15.145331
21.591158	871.593999	15.150349
21.651639	863.985209	15.155367
21.827059	860.479959	15.160384
21.495143	870.769538	15.165402
21.916108	859.623363	15.170419
21.885210	851.972090	15.175437
21.658204	841.691165	15.180455
21.663693	837.398334	15.185472
21.890970	835.986759	15.190490
21.551543	832.050932	15.195507
21.602756	831.793580	15.200525
21.707186	828.331017	15.205543
21.761804	824.705843	15.210560
21.155814	839.907819	15.215578
21.613955	839.141736	15.220595
21.636824	850.410835	15.225613
21.713902	852.188111	15.230631
22.002344	858.773349	15.235648
21.868367	862.439335	15.240666
22.065809	853.600399	15.245683
21.697628	849.104176	15.250701
21.352451	852.367743	15.255719
21.738879	847.068469	15.260736
21.827071	851.564348	15.265754
21.946183	850.996552	15.270771
21.454028	852.294961	15.275789
21.634003	852.153136	15.280807
21.817697	851.026104	15.285824
22.212300	857.335928	15.290842
22.070547	850.746612	15.295859
22.291028	856.477793	15.300877
22.001346	856.277008	15.305895
22.004596	854.310388	15.310912
21.729447	855.151913	15.315930
21.803327	853.433006	15.320947
22.178142	864.050515	15.325965
21.775522	874.237564	15.330983
22.440219	882.736269	15.336000
21.894132	889.098815	15.341018
22.162423	897.706974	15.346035
22.412296	891.106777	15.351053
22.445267	889.482640	15.356071
22.360309	893.175667	15.361088
22.348729	881.728013	15.366106
22.560605	882.303881	15.371123
22.427647	885.650971	15.376141
22.381700	876.698677	15.381159
22.632199	876.589985	15.386176
22.259710	884.149802	15.391194
22.369250	876.489139	15.396211
22.532595	877.779523	15.401229
22.755522	864.856067	15.406247
22.493679	863.170824	15.411264
22.231635	882.102816	15.416282
22.502702	877.418065	15.421299
22.522619	880.397213	15.426317
22.366206	873.447262	15.431335
23.022912	867.395568	15.436352
22.710233	865.872927	15.441370
22.629015	873.699534	15.446387
22.835826	864.190083	15.451405
22.697776	879.871051	15.456423
22.773164	871.695025	15.461440
22.766234	882.776306	15.466458
22.953614	873.418221	15.471475
22.903349	880.845499	15.476493
22.841723	880.025148	15.481511
22.755381	875.301720	15.486528
22.669074	876.962584	15.491546
22.982855	876.742990	15.496563
23.061164	877.781605	15.501581
22.690890	870.155095	15.506599
22.862853	880.447785	15.511616
22.656840	874.203050	15.516634
22.911730	894.130208	15.521651
23.134764	899.917810	15.526669
23.167484	906.969172	15.531687
23.178415	908.135113	15.536704
23.049101	911.074530	15.541722
23.254345	904.269879	15.546739
23.399690	901.132256	15.551757
23.126351	901.790460	15.556775
23.270246	893.379624	15.561792
22.928086	897.914538	15.566810
23.205137	905.350504	15.571827
23.082919	904.419723	15.576845
22.910138	913.002320	15.581863
23.424852	908.348816	15.586880
23.394504	908.198918	15.591898
23.329718	905.955767	15.596915
23.545775	902.472544	15.601933
23.158783	907.206993	15.606951
23.320798	897.824466	15.611968
23.249053	908.641359	15.616986
23.239219	900.153618	15.622003
23.390478	906.261741	15.627021
23.421371	912.666441	15.632039
23.577297	913.314194	15.637056
23.445101	909.973897	15.642074
23.723997	919.741762	15.647091
24.291546	920.823650	15.652109
23.747740	903.258098	15.657127
24.164623	893.403289	15.662144
23.725899	889.337837	15.667162
23.501329	896.117077	15.672179
23.338101	896.344611	15.677197
23.323018	899.215635	15.682215
23.711465	912.251583	15.687232
23.804455	916.617335	15.692250
23.714406	923.609043	15.697267
24.079670	908.602475	15.702285
24.046114	910.567508	15.707303
24.395501	921.296335	15.712320
24.353531	918.153343	15.717338
24.341712	906.753048	15.722355
24.166216	893.664774	15.727373
23.878467	893.892882	15.732391
24.041284	897.963662	15.737408
24.030048	888.838663	15.742426
23.690903	892.502086	15.747443
24.223611	902.189149	15.752461
23.767143	904.362455	15.757479
24.346815	912.596781	15.762496
24.336703	921.870276	15.767514
24.289620	924.222445	15.772531
24.295123	922.050332	15.777549
24.635334	913.709716	15.782567
24.266270	888.605849	15.787584
24.518378	890.873266	15.792602
24.136219	893.249527	15.797619
24.497546	883.968326	15.802637
24.186898	896.015556	15.807655
24.230767	877.758341	15.812672
24.280425	897.818647	15.817690
24.476451	912.462673	15.822707
24.612297	916.711256	15.827725
24.463792	909.425530	15.832743
24.655784	915.795523	15.837760
24.786955	913.048290	15.842778
24.677771	907.984443	15.847795
24.165559	895.617966	15.852813
24.307722	909.598230	15.857831
24.581450	916.801188	15.862848
24.698085	911.727206	15.867866
24.708226	923.506440	15.872883
24.824604	911.634768	15.877901
24.603314	914.863157	15.882919
24.894926	912.535763	15.887936
24.570594	920.548806	15.892954
24.464692	920.966178	15.897971
24.973270	905.795144	15.902989
24.784866	919.382233	15.908007
24.898055	910.878368	15.913024
24.539887	910.432687	15.918042
24.777535	919.686298	15.923059
24.899538	911.619716	15.928077
24.907866	911.110302	15.933095
24.588016	923.493514	15.938112
24.840059	919.442906	15.943130
24.666064	943.782942	15.948147
25.097654	930.324963	15.953165
24.953916	940.604034	15.958183
25.603884	938.151062	15.963200
25.219040	939.442131	15.968218
25.454481	938.486870	15.973235
25.274928	936.520478	15.978253
25.282903	937.147231	15.983271
25.326937	935.335160	15.988288
25.363370	934.963356	15.993306
25.038678	931.653215	15.998323
25.485349	936.209716	16.003341
25.627416	938.768941	16.008359
25.450246	936.338264	16.013376
25.602736	933.107996	16.018394
25.067669	930.746018	16.023411
25.041957	925.195708	16.028429
25.110067	931.149607	16.033447
25.421294	939.056768	16.038464
25.648020	936.606991	16.043482
25.272998	942.339983	16.048499
25.246962	929.695333	16.053517
25.093946	933.582071	16.058535
25.332195	940.774819	16.063552
25.814727	954.474568	16.068570
25.517709	959.472649	16.073587
26.013982	955.153389	16.078605
25.586010	962.264330	16.083623
25.818017	962.155379	16.088640
25.624914	957.180407	16.093658
25.775722	972.368065	16.098675
25.944812	952.712038	16.103693
25.631824	953.089271	16.108711
25.754552	955.187615	16.113728
26.021032	954.953340	16.118746
25.935887	958.157250	16.123763
26.422095	946.442209	16.128781
26.273621	950.706944	16.133799
25.907408	949.571388	16.138816
26.093400	956.759705	16.143834
26.041328	959.627067	16.148851
25.759951	951.838267	16.153869
26.071880	949.312022	16.158887
25.830962	948.778541	16.163904
26.294805	947.383542	16.168922
25.698096	952.169795	16.173939
25.931358	950.842482	16.178957
25.850403	950.397550	16.183975
26.072782	953.199819	16.188992
26.604555	958.317360	16.194010
26.192829	963.904627	16.199027
26.449437	964.060071	16.204045
26.398829	965.718506	16.209063
26.261944	960.999818	16.214080
26.785913	959.358708	16.219098
26.496015	958.716133	16.224115
26.442499	949.417842	16.229133
26.216664	950.548297	16.234151
26.304339	959.093264	16.239168
26.949372	973.831096	16.244186
26.689523	971.157742	16.249203
26.633181	958.476794	16.254221
26.960035	971.696009	16.259239
26.565809	954.753924	16.264256
26.741583	944.958954	16.269274
26.627397	949.896828	16.274291
26.946504	963.555916	16.279309
26.737001	960.839961	16.284327
26.574141	962.907311	16.289344
27.002060	964.544421	16.294362
26.829273	970.548699	16.299379
27.106308	967.273665	16.304397
27.221858	969.104887	16.309415
27.151844	964.842790	16.314432
26.814655	948.668119	16.319450
26.546348	952.588705	16.324467
26.842057	970.461395	16.329485
27.161538	964.446725	16.334503
26.881479	969.934468	16.339520
27.178372	967.805060	16.344538
27.128446	973.259903	16.349555
27.159009	964.412345	16.354573
27.085511	971.849612	16.359591
26.919164	977.448932	16.364608
27.315496	976.449526	16.369626
27.191242	969.264120	16.374643
27.293824	962.620701	16.379661
27.183768	972.632576	16.384679
27.033483	972.776030	16.389696
27.046204	975.955142	16.394714
27.130798	975.178151	16.399731
27.116504	971.308118	16.404749
27.268252	991.500860	16.409767
27.365874	997.787836	16.414784
27.525900	991.962246	16.419802
27.367192	1001.208570	16.424819
27.539916	990.202196	16.429837
27.739394	988.914888	16.434855
28.019917	994.150702	16.439872
28.046862	986.947911	16.444890
27.762186	990.482897	16.449907
27.898492	986.071702	16.454925
27.765288	984.741842	16.459943
27.876848	987.671935	16.464960
27.972172	964.145725	16.469978
27.825164	962.464572	16.474995
27.616059	955.939419	16.480013
28.249354	967.494813	16.485031
27.541514	961.401256	16.490048
27.797189	969.878880	16.495066
27.809627	990.828767	16.500083
28.032212	985.911737	16.505101
28.107012	993.111179	16.510119
28.069372	993.350596	16.515136
28.499028	985.497716	16.520154
27.872670	968.273245	16.525171
28.046691	966.286168	16.530189
28.007327	975.135075	16.535207
27.881425	985.868980	16.540224
28.103662	982.940207	16.545242
28.264946	988.361963	16.550259
28.539888	990.998209	16.555277
28.688175	983.703823	16.560295
28.049919	984.251942	16.565312
28.243993	985.603793	16.570330
28.290497	987.026103	16.575347
28.079740	986.383751	16.580365
28.298470	982.726520	16.585383
28.246509	981.068344	16.590400
28.101829	984.625577	16.595418
27.900625	979.503542	16.600435
28.310173	987.347982	16.605453
28.446771	981.494507	16.610471
28.553640	998.967614	16.615488
28.699627	997.133252	16.620506
28.412420	997.556941	16.625523
28.385750	1008.975916	16.630541
28.665089	1007.117504	16.635559
28.433814	1001.488922	16.640576
28.839640	999.143623	16.645594
28.797297	1007.068340	16.650611
28.633943	1004.098990	16.655629
28.684895	1000.496446	16.660647
28.337178	1007.093046	16.665664
28.412761	1009.716348	16.670682
28.824121	1016.948276	16.675699
29.097672	1027.098900	16.680717
28.993315	1027.001623	16.685735
28.921545	1033.132110	16.690752
29.678641	1021.620738	16.695770
28.987360	1009.067637	16.700787
28.758461	996.104422	16.705805
29.436704	1004.657870	16.710823
28.899833	1006.313598	16.715840
29.180291	1003.940602	16.720858
29.202200	1005.518249	16.725875
29.071081	1014.211135	16.730893
29.309792	1014.896415	16.735911
29.355392	1026.730123	16.740928
29.223137	1014.468138	16.745946
29.597627	1017.590576	16.750963
29.426720	1015.531301	16.755981
29.766025	1009.450392	16.760999
29.506691	1011.330887	16.766016
29.683113	1007.986400	16.771034
29.511963	1004.260860	16.776051
29.627667	1016.970380	16.781069
29.879913	1009.943724	16.786087
29.395952	998.686773	16.791104
29.232179	1008.167430	16.796122
29.771002	1006.943720	16.801139
29.551636	1007.602939	16.806157
29.714109	998.176105	16.811175
29.699450	1000.627348	16.816192
29.673208	994.846720	16.821210
29.763638	995.302762	16.826227
29.826555	1000.891415	16.831245
29.989852	994.980103	16.836263
29.544737	1001.519377	16.841280
29.806023	999.209347	16.846298
29.799120	1005.074035	16.851315
29.927540	1004.826676	16.856333
29.797394	994.795580	16.861351
29.886557	998.218345	16.866368
30.189871	998.309666	16.871386
30.184103	1001.046700	16.876403
29.640896	1007.197392	16.881421
30.203629	1000.740646	16.886439
30.104998	1014.137012	16.891456
30.132022	1014.517779	16.896474
30.346629	1023.412128	16.901491
30.264190	1022.920088	16.906509
30.506476	1009.576918	16.911527
30.154556	1011.670739	16.916544
30.200062	1028.424480	16.921562
30.279857	1021.333318	16.926579
30.457172	1027.386907	16.931597
30.436727	1019.904342	16.936615
30.536752	1032.142947	16.941632
30.291726	1023.471085	16.946650
30.262546	1017.542583	16.951667
30.673050	1021.334738	16.956685
30.704009	1017.287188	16.961703
30.648232	1024.551284	16.966720
30.598431	1033.196723	16.971738
30.760096	1023.665859	16.976755
30.429940	1015.351329	16.981773
30.654272	1018.560412	16.986791
30.521567	1024.400634	16.991808
30.576069	1030.905822	16.996826
30.761027	1025.114185	17.001843
30.492498	1027.747222	17.006861
30.821631	1029.109474	17.011879
30.695639	1043.030869	17.016896
30.645129	1057.827253	17.021914
30.847821	1046.248090	17.026931
31.033810	1046.140037	17.031949
30.995249	1032.304351	17.036967
30.803611	1048.047513	17.041984
30.482482	1047.056369	17.047002
31.432447	1051.136403	17.052019
31.136895	1046.303693	17.057037
31.053117	1038.597508	17.062055
31.032216	1048.800590	17.067072
31.701483	1061.555958	17.072090
31.871431	1046.646150	17.077107
31.431034	1052.774437	17.082125
31.983437	1045.479828	17.087143
31.659986	1044.826727	17.092160
31.482474	1039.628377	17.097178
31.888597	1029.819361	17.102195
31.629565	1039.693665	17.107213
31.887704	1029.058902	17.112231
31.462338	1038.246036	17.117248
31.424091	1042.708123	17.122266
31.611730	1045.752542	17.127283
31.585342	1044.563736	17.132301
31.875464	1042.656292	17.137319
31.990887	1040.874052	17.142336
31.743068	1032.193156	17.147354
31.488617	1029.894497	17.152371
31.097295	1037.665617	17.157389
31.571185	1039.428079	17.162407
31.807989	1038.343208	17.167424
31.516085	1039.547137	17.172442
31.847830	1048.593563	17.177459
32.014336	1054.762467	17.182477
31.987712	1056.196240	17.187495
32.008561	1061.614774	17.192512
32.400781	1062.837753	17.197530
32.537440	1062.030510	17.202547
32.206886	1047.622007	17.207565
32.184495	1039.729474	17.212583
31.770757	1034.691216	17.217600
31.802017	1041.225296	17.222618
32.046001	1057.610288	17.227635
32.105997	1068.182569	17.232653
32.045394	1067.030681	17.237671
31.958905	1060.874453	17.242688
31.825900	1062.151320	17.247706
31.703006	1054.820495	17.252723
31.974808	1075.789807	17.257741
32.503968	1079.711711	17.262759
32.618740	1081.385271	17.267776
32.602693	1087.043130	17.272794
32.700135	1079.501044	17.277811
32.807759	1086.865799	17.282829
32.991214	1077.205256	17.287847
32.953316	1080.108287	17.292864
32.674709	1086.545762	17.297882
32.781100	1079.172691	17.302899
33.222688	1079.305466	17.307917
33.030916	1061.331142	17.312935
33.116265	1049.587319	17.317952
32.723685	1053.846142	17.322970
33.091061	1049.701693	17.327987
32.735759	1052.528214	17.333005
32.579027	1050.072228	17.338023
32.833207	1058.973018	17.343040
32.984895	1078.433702	17.348058
33.159894	1073.208515	17.353075
33.039086	1076.329668	17.358093
33.370378	1074.242197	17.363111
33.362811	1078.424923	17.368128
33.188025	1078.524878	17.373146
33.215445	1078.975015	17.378163
33.029348	1084.921455	17.383181
33.256455	1080.865250	17.388199
33.386830	1068.969189	17.393216
33.407576	1078.035954	17.398234
33.403736	1077.774601	17.403251
33.462129	1079.939846	17.408269
33.589366	1073.888987	17.413287
33.424842	1072.390453	17.418304
33.468391	1074.135134	17.423322
33.790276	1071.506323	17.428339
33.555201	1078.195757	17.433357
33.428413	1074.349640	17.438375
33.601195	1067.969745	17.443392
33.394641	1078.268205	17.448410
33.440610	1079.902051	17.453427
33.251505	1077.239689	17.458445
33.612682	1081.194224	17.463463
33.577151	1093.129052	17.468480
33.772425	1105.425370	17.473498
34.061913	1100.920717	17.478515
34.001373	1108.674756	17.483533
34.178891	1103.146200	17.488551
34.359755	1092.217385	17.493568
34.234151	1101.057776	17.498586
33.736282	1094.795571	17.503603
34.027355	1100.026608	17.508621
34.141858	1091.913782	17.513639
34.295419	1094.726856	17.518656
33.963896	1099.888177	17.523674
34.370680	1088.766172	17.528691
33.664793	1094.639416	17.533709
33.697978	1095.603061	17.538727
33.968632	1093.064327	17.543744
33.900126	1091.803220	17.548762
34.556566	1097.971118	17.553779
34.486794	1116.017985	17.558797
34.454846	1119.494464	17.563815
34.734921	1120.914904	17.568832
34.755696	1120.460340	17.573850
34.955468	1095.803560	17.578867
34.711097	1095.702972	17.583885
34.320609	1090.610561	17.588903
34.562704	1090.992349	17.593920
34.215298	1100.820571	17.598938
34.380445	1106.699363	17.603955
34.543704	1118.076027	17.608973
34.868053	1116.545077	17.613991
34.875694	1113.539449	17.619008
34.625346	1127.975870	17.624026
35.110570	1111.817369	17.629043
35.186997	1117.059950	17.634061
34.775013	1116.243987	17.639079
34.976638	1110.247734	17.644096
35.083100	1126.392397	17.649114
35.129256	1119.050839	17.654131
35.142747	1109.937632	17.659149
34.671150	1116.509498	17.664167
35.247021	1115.204236	17.669184
34.700675	1113.412061	17.674202
35.292625	1120.382202	17.679219
35.237512	1131.048297	17.684237
35.119563	1142.642610	17.689255
35.481506	1136.469747	17.694272
35.570498	1143.250447	17.699290
35.734560	1142.268488	17.704307
35.707983	1144.898348	17.709325
35.478788	1146.275501	17.714343
35.979144	1135.990902	17.719360
35.585132	1124.606166	17.724378
35.544179	1108.239764	17.729395
35.822384	1112.971034	17.734413
35.439600	1120.425262	17.739431
35.825694	1117.139426	17.744448
35.877697	1134.236242	17.749466
35.508019	1125.372414	17.754483
35.736019	1125.128387	17.759501
35.621239	1132.105116	17.764519
36.014508	1127.372751	17.769536
35.649150	1133.094821	17.774554
36.134560	1126.034744	17.779571
35.999697	1124.569430	17.784589
35.908927	1130.841787	17.789607
35.900910	1128.611805	17.794624
35.545211	1125.341200	17.799642
35.635152	1118.178981	17.804659
35.932274	1125.510906	17.809677
36.076997	1141.270880	17.814695
36.583457	1136.416633	17.819712
36.256206	1145.929288	17.824730
36.614132	1143.493642	17.829747
36.499364	1144.852867	17.834765
36.853694	1150.900855	17.839783
36.780379	1132.156794	17.844800
36.259524	1127.981074	17.849818
36.485236	1132.313462	17.854835
36.753958	1141.388745	17.859853
36.517336	1139.121994	17.864871
37.076552	1133.713511	17.869888
36.583914	1127.302148	17.874906
36.520177	1117.790769	17.879923
36.572081	1119.600419	17.884941
36.794693	1138.737624	17.889959
36.963309	1138.114724	17.894976
36.342051	1153.650727	17.899994
36.624409	1140.616772	17.905011
36.838136	1139.671214	17.910029
36.405712	1149.187725	17.915047
36.659984	1140.705828	17.920064
36.834135	1135.894179	17.925082
36.529043	1135.070936	17.930099
36.973686	1151.907429	17.935117
37.074730	1160.393592	17.940135
36.991212	1162.915608	17.945152
37.581891	1167.279188	17.950170
37.389252	1163.935689	17.955187
37.614980	1175.551920	17.960205
37.088205	1164.285792	17.965223
37.335018	1154.807791	17.970240
37.444412	1162.509983	17.975258
37.384783	1164.999853	17.980275
37.805493	1163.034066	17.985293
37.268878	1162.843561	17.990311
37.283501	1168.241012	17.995328
37.331032	1169.334961	18.000346
37.586701	1155.481485	18.005363
37.761726	1162.687384	18.010381
37.436042	1164.761332	18.015399
37.412308	1156.111539	18.020416
37.519193	1168.832017	18.025434
37.759813	1160.989744	18.030451
37.734560	1148.496299	18.035469
37.386230	1168.332078	18.040487
37.877152	1173.484487	18.045504
37.986867	1185.705899	18.050522
37.873234	1188.235792	18.055539
38.006446	1186.586456	18.060557
37.829550	1193.049059	18.065575
38.053800	1181.813580	18.070592
37.723066	1189.256526	18.075610
37.904073	1185.359004	18.080627
37.936666	1178.473998	18.085645
37.967534	1189.237113	18.090663
38.363855	1195.187015	18.095680
38.456876	1203.803848	18.100698
38.645512	1202.717047	18.105715
38.807783	1190.266779	18.110733
38.345096	1194.918484	18.115751
38.696359	1183.448502	18.120768
38.783646	1188.048752	18.125786
38.633734	1175.814669	18.130803
38.681404	1163.726369	18.135821
38.553626	1173.037366	18.140839
38.709111	1168.137111	18.145856
38.854536	1164.860571	18.150874
38.455948	1175.091340	18.155891
39.095551	1177.541089	18.160909
38.886084	1185.050243	18.165927
38.830254	1171.769439	18.170944
38.993924	1180.179526	18.175962
38.568869	1186.564239	18.180979
38.580565	1184.911850	18.185997
38.606336	1200.273932	18.191015
38.843800	1193.154843	18.196032
38.988004	1200.491823	18.201050
38.986609	1200.933854	18.206067
39.447273	1195.203111	18.211085
39.087462	1195.410954	18.216103
39.259996	1197.709814	18.221120
39.297914	1197.381954	18.226138
39.336402	1194.623953	18.231155
39.423404	1200.657035	18.236173
38.954395	1196.870821	18.241191
39.103438	1194.101810	18.246208
39.529921	1208.987693	18.251226
39.210540	1212.215724	18.256243
39.601284	1224.162751	18.261261
39.478276	1221.351150	18.266279
39.594285	1222.708938	18.271296
39.725812	1217.118122	18.276314
39.721612	1220.157912	18.281331
40.026760	1217.471741	18.286349
39.753024	1220.171895	18.291367
40.178548	1218.479913	18.296384
40.025038	1214.300269	18.301402
39.865401	1221.514442	18.306419
39.724658	1219.759696	18.311437
40.100473	1212.959763	18.316455
40.138406	1213.894267	18.321472
40.486588	1218.914413	18.326490
39.713310	1221.017467	18.331507
40.273409	1209.558932	18.336525
39.928888	1217.467969	18.341543
40.025111	1211.510288	18.346560
39.982358	1216.380237	18.351578
40.348546	1218.080694	18.356595
40.811641	1213.517254	18.361613
40.486351	1216.945034	18.366631
40.749675	1213.167157	18.371648
40.638337	1212.824811	18.376666
40.398096	1220.367205	18.381683
40.807531	1209.992663	18.386701
40.435367	1211.243892	18.391719
40.135488	1216.327702	18.396736
40.276276	1210.713346	18.401754
40.567474	1230.338538	18.406771
40.927190	1236.811760	18.411789
40.708418	1242.709721	18.416807
40.666019	1232.245006	18.421824
41.114975	1237.034766	18.426842
41.011203	1245.218531	18.431859
41.320237	1246.808021	18.436877
41.036354	1246.568450	18.441895
41.046417	1243.881169	18.446912
41.152920	1247.045636	18.451930
40.918487	1235.657917	18.456947
41.215639	1235.633437	18.461965
41.163774	1232.056423	18.466983
41.208395	1234.239624	18.472000
40.725142	1230.114795	18.477018
41.412216	1238.291419	18.482035
41.310236	1232.566764	18.487053
41.080614	1234.786621	18.492071
41.029082	1243.448213	18.497088
41.505178	1253.321070	18.502106
41.622731	1258.904401	18.507123
41.568813	1261.153539	18.512141
41.842688	1269.830434	18.517159
41.722975	1261.287151	18.522176
41.920784	1259.065932	18.527194
41.760214	1265.131513	18.532211
41.662052	1262.524304	18.537229
42.036297	1259.732623	18.542247
41.687408	1266.477830	18.547264
42.042855	1257.834854	18.552282
41.924847	1258.784325	18.557299
42.243914	1258.810062	18.562317
42.142550	1260.454384	18.567335
42.003144	1252.583246	18.572352
42.168905	1252.516233	18.577370
42.014474	1256.627333	18.582387
42.398667	1257.166749	18.587405
42.337423	1259.442282	18.592423
42.195186	1254.651768	18.597440
42.634037	1252.986099	18.602458
42.434160	1255.504266	18.607475
42.339325	1247.963831	18.612493
42.416356	1261.036203	18.617511
42.036463	1253.218522	18.622528
42.454869	1245.556648	18.627546
42.144647	1251.535215	18.632563
42.496313	1245.723700	18.637581
42.233635	1245.657538	18.642599
42.333101	1255.153889	18.647616
42.372313	1261.702583	18.652634
42.273381	1271.820184	18.657651
42.634608	1270.116180	18.662669
42.555091	1273.663260	18.667687
42.515378	1281.054336	18.672704
42.631276	1274.894728	18.677722
42.740241	1292.064824	18.682739
43.046050	1283.764142	18.687757
43.225279	1292.036139	18.692775
43.263313	1292.339445	18.697792
43.081827	1295.927753	18.702810
42.859879	1293.548225	18.707827
42.978053	1297.461983	18.712845
43.395758	1293.356933	18.717863
43.152703	1293.615913	18.722880
43.262219	1291.187609	18.727898
43.528195	1291.578284	18.732915
43.657747	1289.942135	18.737933
43.428090	1293.086692	18.742951
43.403680	1290.089212	18.747968
43.601358	1290.285452	18.752986
43.548139	1309.200957	18.758003
43.668680	1313.543555	18.763021
43.338289	1313.828843	18.768039
43.865665	1319.660420	18.773056
43.878638	1313.302321	18.778074
43.876513	1316.064081	18.783091
43.783723	1313.894697	18.788109
44.060295	1310.300925	18.793127
43.742814	1311.865498	18.798144
44.125483	1315.892462	18.803162
44.091093	1313.496169	18.808179
43.925933	1310.672222	18.813197
43.714426	1313.649831	18.818215
43.917971	1319.746748	18.823232
44.517036	1325.017963	18.828250
44.599498	1331.531504	18.833267
44.401676	1326.923256	18.838285
44.397083	1319.135112	18.843303
44.494684	1330.645281	18.848320
44.926525	1329.245801	18.853338
44.764673	1316.792577	18.858355
44.675671	1308.335981	18.863373
44.829615	1305.237968	18.868391
44.475755	1308.149512	18.873408
44.700785	1289.345919	18.878426
44.779787	1308.802464	18.883443
44.898719	1313.782813	18.888461
44.974581	1296.072445	18.893479
44.697182	1305.653115	18.898496
45.134725	1310.918074	18.903514
44.944391	1316.284562	18.908531
44.877131	1323.276012	18.913549
45.051577	1330.794508	18.918567
44.843089	1325.149628	18.923584
45.089916	1323.406736	18.928602
45.002426	1321.391162	18.933619
44.893588	1330.667713	18.938637
44.987527	1329.283304	18.943655
44.857297	1329.726587	18.948672
45.256484	1329.540948	18.953690
45.577460	1339.523367	18.958707
45.287011	1339.928635	18.963725
45.480033	1345.137235	18.968743
45.481160	1353.440321	18.973760
45.543544	1347.629914	18.978778
45.351144	1351.535537	18.983795
45.301771	1357.596351	18.988813
45.519109	1352.459127	18.993831
45.606799	1356.690113	18.998848
45.639152	1344.266405	19.003866
45.420606	1351.423586	19.008883
45.590021	1373.305577	19.013901
45.951973	1364.140800	19.018919
45.843180	1378.921334	19.023936
46.343003	1367.172328	19.028954
46.148431	1363.374639	19.033971
46.254465	1366.192047	19.038989
46.538034	1356.783923	19.044007
46.481325	1365.042425	19.049024
46.390724	1366.666135	19.054042
46.662188	1368.135284	19.059059
46.524055	1369.324610	19.064077
46.347219	1367.910034	19.069095
46.258510	1362.738703	19.074112
46.031661	1368.003626	19.079130
46.520389	1365.970355	19.084147
46.469982	1368.076939	19.089165
47.353475	1350.823831	19.094183
46.932294	1360.177738	19.099200
46.943929	1353.056096	19.104218
46.907386	1354.106422	19.109235
46.610144	1356.478906	19.114253
47.129785	1345.963937	19.119271
46.765929	1355.955828	19.124288
46.954384	1350.943057	19.129306
47.049013	1352.913301	19.134323
46.931980	1355.349073	19.139341
47.300896	1353.770094	19.144359
46.882546	1357.894163	19.149376
47.269232	1352.607326	19.154394
47.113543	1348.472174	19.159411
46.946351	1363.902501	19.164429
47.387963	1377.384917	19.169447
47.433224	1380.871442	19.174464
47.563111	1388.037165	19.179482
47.566993	1383.946435	19.184499
47.341914	1382.656187	19.189517
47.820248	1373.886600	19.194535
47.456425	1383.379862	19.199552
47.419093	1374.823616	19.204570
47.962987	1379.901512	19.209587
47.657269	1382.016539	19.214605
48.150145	1375.996657	19.219623
47.774568	1378.024795	19.224640
47.874877	1378.959003	19.229658
48.041233	1372.119240	19.234675
47.893095	1370.087914	19.239693
47.863520	1368.385167	19.244711
47.638724	1375.133064	19.249728
47.706830	1379.818424	19.254746
47.952242	1389.086843	19.259763
47.677834	1393.967887	19.264781
48.167011	1399.647679	19.269799
48.214209	1401.413912	19.274816
48.418240	1397.515893	19.279834
48.483706	1393.715327	19.284851
48.391317	1392.461096	19.289869
48.640473	1397.683009	19.294887
48.804178	1403.461135	19.299904
48.594586	1393.132978	19.304922
48.739547	1397.250854	19.309939
48.707813	1398.145788	19.314957
48.564411	1398.256607	19.319975
48.659839	1413.686858	19.324992
48.988931	1417.340369	19.330010
48.935425	1417.042610	19.335027
49.136741	1421.587183	19.340045
49.505372	1413.702652	19.345063
49.352888	1421.221912	19.350080
49.436780	1419.286778	19.355098
49.596549	1409.276301	19.360115
49.108502	1407.386593	19.365133
49.187314	1391.521900	19.370151
49.112217	1402.140792	19.375168
49.363450	1404.932301	19.380186
49.065575	1411.574891	19.385203
49.104422	1414.986684	19.390221
49.236850	1417.929359	19.395239
48.985265	1424.050281	19.400256
48.962165	1417.571559	19.405274
49.428227	1441.957166	19.410291
49.423813	1447.146234	19.415309
49.614924	1447.150992	19.420327
49.638257	1449.328087	19.425344
49.681738	1449.062471	19.430362
49.809250	1437.750466	19.435379
49.850908	1451.456555	19.440397
50.055653	1451.295066	19.445415
50.072668	1469.549610	19.450432
50.196615	1469.669037	19.455450
50.273931	1474.864244	19.460467
50.142750	1469.027317	19.465485
50.446864	1466.290776	19.470503
50.781207	1463.322271	19.475520
50.744070	1460.825397	19.480538
50.582915	1447.829147	19.485555
50.259505	1451.767941	19.490573
50.840778	1452.652046	19.495591
50.575362	1460.621383	19.500608
50.558259	1473.980072	19.505626
51.220517	1463.890837	19.510643
50.740246	1460.204164	19.515661
50.571488	1452.520582	19.520679
50.794417	1456.430587	19.525696
50.663870	1457.498803	19.530714
51.106284	1458.208994	19.535731
50.826878	1457.160793	19.540749
51.057497	1456.446114	19.545767
51.083022	1456.388448	19.550784
51.054680	1452.649906	19.555802
50.994452	1455.038919	19.560819
50.665981	1456.191797	19.565837
51.211387	1440.197149	19.570855
50.992566	1447.461714	19.575872
51.336527	1463.544224	19.580890
51.600993	1474.719058	19.585907
51.660695	1477.288110	19.590925
51.781277	1483.710523	19.595943
51.355767	1483.205945	19.600960
51.161475	1476.258536	19.605978
51.191634	1472.955815	19.610995
51.442549	1487.572779	19.616013
51.344467	1480.493525	19.621031
51.530146	1482.332748	19.626048
51.551085	1499.191771	19.631066
52.079948	1497.360491	19.636083
52.133634	1510.241034	19.641101
52.043775	1500.481066	19.646119
51.886036	1509.042655	19.651136
51.960220	1506.736629	19.656154
52.328732	1506.846143	19.661171
52.354425	1503.872337	19.666189
52.094294	1499.974431	19.671207
52.438670	1497.594513	19.676224
52.147786	1498.848807	19.681242
52.398252	1494.148188	19.686259
52.440553	1505.708162	19.691277
52.503000	1500.206980	19.696295
52.447995	1505.486047	19.701312
52.615291	1521.293315	19.706330
53.235577	1514.716911	19.711347
53.074963	1524.724393	19.716365
52.941554	1508.283743	19.721383
52.768962	1505.252636	19.726400
52.648568	1505.801686	19.731418
52.971828	1505.646877	19.736435
52.904918	1524.839324	19.741453
53.134398	1527.268168	19.746471
53.108010	1519.619058	19.751488
52.838000	1525.155891	19.756506
53.208469	1519.631692	19.761523
52.953144	1519.886285	19.766541
53.227694	1519.502410	19.771559
53.341346	1519.995855	19.776576
53.609369	1553.315635	19.781594
53.560869	1543.861606	19.786611
53.585337	1545.489396	19.791629
53.773571	1536.200262	19.796647
53.728133	1547.294301	19.801664
53.332688	1544.298103	19.806682
53.754086	1539.731646	19.811699
53.243340	1550.955397	19.816717
53.689953	1544.999516	19.821735
53.776723	1545.055337	19.826752
53.601288	1538.243813	19.831770
54.431487	1557.949028	19.836787
54.136126	1568.583592	19.841805
54.276786	1557.222112	19.846823
54.703967	1559.591582	19.851840
54.614347	1564.838218	19.856858
54.497015	1539.902287	19.861875
54.523870	1542.779468	19.866893
54.364073	1536.524101	19.871911
54.504688	1544.180538	19.876928
54.539041	1555.722854	19.881946
54.633870	1558.589387	19.886963
54.576920	1560.012172	19.891981
54.668121	1567.124065	19.896999
54.920906	1559.513255	19.902016
54.654505	1560.836304	19.907034
54.935440	1564.033462	19.912051
54.988208	1558.962991	19.917069
54.818223	1555.016234	19.922087
55.083770	1564.467792	19.927104
55.111548	1565.069373	19.932122
54.944941	1561.248324	19.937139
54.967047	1566.310189	19.942157
54.890704	1559.628306	19.947175
55.289192	1563.892702	19.952192
55.188251	1562.958552	19.957210
55.344996	1567.607982	19.962227
55.507161	1571.745295	19.967245
55.365549	1579.019908	19.972263
55.528804	1577.533096	19.977280
55.144857	1584.227106	19.982298
55.708912	1574.408830	19.987315
55.691373	1584.337121	19.992333
55.407865	1578.574519	19.997351
55.656194	1578.586093	20.002368
55.422208	1590.359831	20.007386
56.202552	1589.767314	20.012403
56.014661	1591.087533	20.017421
56.142667	1599.443442	20.022439
56.254841	1593.865009	20.027456
56.270916	1604.536012	20.032474
56.097498	1601.858488	20.037491
56.509273	1604.075734	20.042509
56.213372	1593.413826	20.047527
56.188644	1595.781516	20.052544
56.247209	1600.197014	20.057562
56.422620	1587.305730	20.062579
56.409216	1594.986320	20.067597
56.475579	1599.293292	20.072615
56.566552	1604.281259	20.077632
56.580767	1615.662657	20.082650
56.934935	1618.232933	20.087667
57.155347	1616.004974	20.092685
57.043112	1618.298009	20.097703
57.352269	1611.088623	20.102720
56.976731	1611.712366	20.107738
57.608064	1611.461950	20.112755
57.585200	1598.055737	20.117773
57.570349	1600.027382	20.122791
57.097262	1580.221955	20.127808
56.945594	1589.540067	20.132826
56.971474	1594.797020	20.137843
57.182451	1602.836956	20.142861
57.143336	1597.411620	20.147879
57.665006	1587.192856	20.152896
57.419424	1588.171800	20.157914
57.433188	1601.743511	20.162931
57.518564	1613.625028	20.167949
57.941583	1624.333277	20.172967
58.074016	1617.385120	20.177984
57.937915	1626.539857	20.183002
58.195566	1623.400293	20.188019
58.281606	1618.037399	20.193037
58.014365	1614.150049	20.198055
58.251916	1618.515417	20.203072
58.128253	1625.165507	20.208090
58.150435	1616.309471	20.213107
58.163403	1611.683903	20.218125
57.830767	1621.573215	20.223143
57.970745	1614.163102	20.228160
58.423067	1617.888872	20.233178
58.583654	1640.242815	20.238195
58.346737	1642.384965	20.243213
58.520544	1652.065550	20.248231
58.731959	1634.709174	20.253248
58.561074	1640.299943	20.258266
58.580111	1639.025080	20.263283
58.678512	1640.344632	20.268301
58.844662	1639.526431	20.273319
59.088341	1633.788519	20.278336
58.822317	1636.067779	20.283354
59.002901	1642.518720	20.288371
58.965211	1647.580509	20.293389
59.093589	1672.833585	20.298407
59.593607	1672.805725	20.303424
59.564688	1666.346760	20.308442
59.141998	1670.064457	20.313459
59.285351	1662.357132	20.318477
59.579402	1665.577502	20.323495
59.777169	1659.174547	20.328512
59.581284	1667.439213	20.333530
59.534892	1674.847278	20.338547
59.827703	1658.607972	20.343565
59.644922	1662.606835	20.348583
59.517419	1663.598843	20.353600
59.386610	1671.632395	20.358618
59.556916	1680.571885	20.363635
59.739949	1692.021563	20.368653
59.875584	1686.414177	20.373671
60.028108	1686.608029	20.378688
59.955036	1691.880513	20.383706
60.264193	1709.199538	20.388723
60.260874	1717.790685	20.393741
60.152604	1711.290485	20.398759
60.619559	1703.829107	20.403776
60.519609	1709.512932	20.408794
61.119935	1712.360256	20.413811
61.022056	1710.027509	20.418829
61.214192	1699.831907	20.423847
61.164050	1704.412794	20.428864
61.140798	1700.815423	20.433882
61.241825	1704.198594	20.438899
61.506060	1705.107136	20.443917
61.137458	1695.715802	20.448935
61.117079	1670.025994	20.453952
60.910733	1689.316208	20.458970
61.194440	1696.451644	20.463987
61.234528	1696.524248	20.469005
61.353145	1703.016479	20.474023
61.400628	1690.880512	20.479040
61.204305	1696.579432	20.484058
61.306942	1701.474074	20.489075
61.519248	1696.110310	20.494093
61.660174	1699.714460	20.499111
61.555700	1702.826851	20.504128
61.646503	1706.009639	20.509146
61.574641	1713.162918	20.514163
62.186610	1720.262714	20.519181
61.961048	1731.091579	20.524199
61.796994	1726.026628	20.529216
61.871675	1732.629902	20.534234
62.163453	1729.216713	20.539251
62.197943	1724.139591	20.544269
62.041972	1731.299743	20.549287
62.427663	1725.050371	20.554304
62.029801	1725.131626	20.559322
62.337161	1734.867077	20.564339
62.706332	1747.032444	20.569357
62.642856	1753.758364	20.574375
62.760171	1750.811190	20.579392
62.740699	1748.687074	20.584410
62.798044	1755.545554	20.589427
63.078984	1738.967186	20.594445
62.488960	1745.652515	20.599463
62.979184	1744.149178	20.604480
62.839445	1745.947889	20.609498
62.990776	1746.811003	20.614515
63.357018	1739.453758	20.619533
63.040159	1739.282465	20.624551
63.243023	1739.468431	20.629568
63.251365	1745.816998	20.634586
63.167833	1743.614552	20.639603
63.276967	1739.819695	20.644621
63.368020	1750.677867	20.649639
63.666475	1761.879116	20.654656
63.722625	1767.257618	20.659674
63.730244	1758.274397	20.664691
64.055464	1760.259056	20.669709
64.045220	1762.050104	20.674727
64.045780	1758.581543	20.679744
63.863576	1753.674072	20.684762
64.080421	1753.864160	20.689779
63.978918	1742.859260	20.694797
64.354482	1754.288280	20.699815
64.047056	1747.724588	20.704832
64.113460	1754.105090	20.709850
64.309098	1761.001869	20.714867
64.833736	1750.908788	20.719885
64.387602	1745.566113	20.724903
64.450155	1748.895356	20.729920
64.403524	1749.464416	20.734938
64.105708	1748.201316	20.739955
64.672319	1764.293398	20.744973
64.383146	1779.730570	20.749991
64.578305	1773.820323	20.755008
65.039279	1773.609220	20.760026
64.639148	1776.928902	20.765043
64.893711	1774.818657	20.770061
65.323516	1790.054825	20.775079
65.142389	1792.456513	20.780096
65.504774	1800.135123	20.785114
65.224901	1807.724999	20.790131
65.846659	1798.711815	20.795149
65.639192	1800.445398	20.800167
65.464771	1798.039419	20.805184
65.521215	1791.213561	20.810202
65.371423	1793.326298	20.815219
65.732481	1792.903616	20.820237
65.637244	1784.422523	20.825255
65.714116	1787.506516	20.830272
65.706300	1782.290830	20.835290
65.523397	1791.254154	20.840307
65.686578	1804.559596	20.845325
65.913329	1803.870759	20.850343
65.661330	1815.079383	20.855360
65.968867	1816.729124	20.860378
66.081625	1815.584743	20.865395
66.188156	1828.185817	20.870413
66.421547	1843.042520	20.875431
66.349803	1845.221935	20.880448
66.644703	1837.301430	20.885466
66.519627	1837.302075	20.890483
67.024812	1825.255265	20.895501
67.091820	1833.011727	20.900519
67.061763	1829.686814	20.905536
67.188842	1834.748089	20.910554
66.808915	1835.079016	20.915571
67.120873	1831.331264	20.920589
67.076801	1840.118216	20.925607
66.627114	1847.034077	20.930624
67.254309	1843.072819	20.935642
66.797771	1837.018484	20.940659
67.163129	1840.477040	20.945677
67.464760	1853.082281	20.950695
67.173683	1871.028872	20.955712
67.540903	1860.439649	20.960730
67.401032	1856.901546	20.965747
67.512084	1849.707322	20.970765
67.759018	1851.246633	20.975783
67.401397	1854.717470	20.980800
68.176897	1861.324609	20.985818
67.744804	1872.198541	20.990835
68.183138	1866.515271	20.995853
67.997226	1871.167968	21.000871
68.017481	1886.389483	21.005888
68.357259	1879.061576	21.010906
68.034860	1878.768064	21.015923
68.350284	1868.092270	21.020941
68.232744	1868.937550	21.025959
68.268910	1872.554992	21.030976
68.275624	1878.288436	21.035994
68.474068	1889.047810	21.041011
68.983101	1886.092895	21.046029
68.827682	1899.883857	21.051047
68.730815	1901.543313	21.056064
68.818154	1899.184678	21.061082
68.881003	1899.771307	21.066099
68.777900	1895.832931	21.071117
68.944626	1896.892471	21.076135
69.114687	1899.024540	21.081152
69.362951	1903.501917	21.086170
69.129688	1915.089549	21.091187
69.831120	1914.108571	21.096205
69.695869	1916.815535	21.101223
69.958868	1919.359112	21.106240
70.184786	1911.310517	21.111258
69.713399	1891.917918	21.116275
69.730430	1885.622100	21.121293
69.790680	1899.581258	21.126311
69.529178	1905.694429	21.131328
70.094889	1906.839793	21.136346
69.992353	1912.953308	21.141363
69.882752	1902.650219	21.146381
70.515914	1903.125404	21.151399
70.236236	1906.868082	21.156416
70.473383	1902.175756	21.161434
70.496268	1909.124907	21.166451
70.669328	1899.670693	21.171469
71.125735	1905.179045	21.176487
70.454016	1904.410047	21.181504
70.845672	1898.308015	21.186522
70.751642	1903.757427	21.191539
70.943465	1901.518132	21.196557
70.649355	1897.556029	21.201575
70.841075	1905.419225	21.206592
71.233757	1910.603022	21.211610
71.049209	1923.278172	21.216627
70.922923	1924.402557	21.221645
71.323577	1922.247314	21.226663
71.462480	1926.899634	21.231680
71.460553	1921.951248	21.236698
71.164163	1924.699239	21.241715
71.362976	1923.108991	21.246733
71.639585	1915.645788	21.251751
71.503092	1917.822732	21.256768
71.833035	1916.839992	21.261786
71.563953	1927.353877	21.266803
71.770685	1932.727773	21.271821
71.904567	1929.351908	21.276839
71.839189	1942.030493	21.281856
71.945754	1936.500173	21.286874
72.293285	1939.062069	21.291891
72.080942	1938.489362	21.296909
72.552877	1936.180928	21.301927
72.289292	1939.999993	21.306944
72.603918	1928.352227	21.311962
72.703869	1937.340742	21.316979
72.644768	1929.718674	21.321997
72.378863	1929.574112	21.327015
72.314916	1942.400807	21.332032
72.670745	1941.275144	21.337050
72.549155	1952.365584	21.342067
72.840202	1951.306879	21.347085
73.121436	1950.514819	21.352103
73.200827	1961.905162	21.357120
73.234029	1952.952552	21.362138
73.033601	1952.639929	21.367155
73.042237	1948.936518	21.372173
73.296506	1956.041954	21.377191
73.177557	1973.466181	21.382208
73.355638	1972.472514	21.387226
73.738368	1991.118451	21.392243
73.477808	1983.720443	21.397261
73.966180	1976.511238	21.402279
73.774476	1979.829862	21.407296
74.239131	1977.891822	21.412314
73.991362	1971.586964	21.417331
74.080324	1971.579323	21.422349
74.127612	1971.455125	21.427367
73.788893	1971.946868	21.432384
73.909912	1986.556188	21.437402
74.236795	1996.004678	21.442419
74.296563	1999.744691	21.447437
74.401468	1996.676335	21.452455
74.183819	1994.665296	21.457472
74.568553	1992.525164	21.462490
74.671582	1997.082129	21.467507
74.533756	2007.944755	21.472525
74.560588	2022.489959	21.477543
74.298409	2031.235431	21.482560
74.427740	2018.897056	21.487578
74.845370	2035.722838	21.492595
75.260836	2045.261626	21.497613
75.429185	2040.933522	21.502631
75.423560	2046.391219	21.507648
75.561713	2043.945703	21.512666
75.784652	2035.414642	21.517683
75.590206	2040.772522	21.522701
75.667287	2032.690382	21.527719
75.650150	2042.672517	21.532736
75.748537	2036.723691	21.537754
75.730589	2039.724746	21.542771
75.676522	2046.985832	21.547789
76.311612	2040.627844	21.552807
76.049125	2054.719745	21.557824
76.221092	2046.597484	21.562842
76.707612	2054.720697	21.567859
76.392058	2058.352254	21.572877
76.683987	2054.680183	21.577895
76.854319	2064.026994	21.582912
76.828487	2055.260321	21.587930
76.602596	2039.180840	21.592947
76.503156	2042.967897	21.597965
76.780911	2048.283360	21.602983
76.559460	2053.440330	21.608000
76.516632	2055.002964	21.613018
76.552204	2052.497773	21.618035
76.723522	2062.024324	21.623053
76.855570	2066.627257	21.628071
76.957743	2074.618175	21.633088
77.221337	2078.140062	21.638106
77.594874	2076.036392	21.643123
77.090151	2076.383718	21.648141
77.487740	2073.929112	21.653159
77.244241	2075.425350	21.658176
77.662854	2085.992544	21.663194
77.695183	2085.242632	21.668211
77.701967	2101.593156	21.673229
77.972448	2095.645754	21.678247
77.914042	2100.398465	21.683264
78.033875	2099.316078	21.688282
78.199180	2095.916324	21.693299
77.762607	2108.823610	21.698317
78.306642	2106.472298	21.703335
78.041496	2099.630429	21.708352
77.945162	2110.540270	21.713370
78.136362	2116.876101	21.718387
78.286260	2121.488876	21.723405
78.666055	2121.069565	21.728423
78.401600	2124.891961	21.733440
79.054729	2143.568283	21.738458
79.061918	2148.351758	21.743475
79.033370	2156.634617	21.748493
79.055561	2151.205820	21.753511
79.288338	2147.959601	21.758528
79.166474	2145.393849	21.763546
79.221393	2146.789685	21.768563
79.563705	2151.640588	21.773581
79.882697	2144.189587	21.778599
79.549476	2143.130837	21.783616
79.379321	2148.516504	21.788634
79.775498	2140.722023	21.793651
79.610764	2157.206777	21.798669
79.771575	2158.497654	21.803687
79.638422	2165.171522	21.808704
80.116785	2156.925462	21.813722
79.917776	2164.518600	21.818739
79.630811	2163.449447	21.823757
79.985408	2166.104951	21.828775
80.349152	2187.897528	21.833792
80.597049	2180.659640	21.838810
80.843064	2176.325648	21.843827
80.429665	2177.293041	21.848845
80.768439	2178.038439	21.853863
80.584671	2174.936378	21.858880
80.774077	2180.133165	21.863898
80.612922	2174.401698	21.868915
81.074616	2192.615715	21.873933
81.186994	2203.003719	21.878951
81.336987	2200.546858	21.883968
81.127515	2204.969783	21.888986
81.362027	2200.839577	21.894003
81.512362	2205.445992	21.899021
81.217331	2196.841358	21.904039
81.358567	2194.688855	21.909056
81.435462	2193.007221	21.914074
81.563912	2205.242176	21.919091
81.448911	2224.225136	21.924109
81.810667	2220.744082	21.929127
81.498375	2226.439246	21.934144
81.658264	2228.285744	21.939162
81.917290	2233.642069	21.944179
82.075908	2247.497716	21.949197
82.322214	2257.643842	21.954215
82.351396	2256.733454	21.959232
82.525926	2255.115421	21.964250
82.892004	2246.864819	21.969267
82.763430	2254.702604	21.974285
83.188211	2242.633396	21.979303
83.345880	2248.491644	21.984320
83.249650	2250.154189	21.989338
83.404341	2240.456498	21.994355
83.100199	2248.776264	21.999373
82.855596	2249.455259	22.004391
83.005025	2244.688217	22.009408
82.997516	2251.762194	22.014426
83.109418	2242.023865	22.019443
82.806578	2246.451959	22.024461
83.527185	2261.425199	22.029479
83.429814	2264.078939	22.034496
83.412506	2269.671090	22.039514
83.649273	2267.490987	22.044531
83.468233	2273.556959	22.049549
83.558521	2290.266993	22.054567
83.749637	2299.793724	22.059584
83.780722	2301.531010	22.064602
83.923482	2296.335769	22.069619
83.977465	2314.664284	22.074637
84.676270	2321.192086	22.079655
84.697850	2325.162233	22.084672
84.581785	2321.746553	22.089690
84.641667	2318.382210	22.094707
84.586632	2327.145869	22.099725
84.789210	2316.762071	22.104743
84.787520	2313.489435	22.109760
84.807316	2307.688545	22.114778
85.183173	2313.878740	22.119795
84.725606	2320.985381	22.124813
85.206589	2336.352867	22.129831
85.230160	2335.478071	22.134848
85.075494	2347.309311	22.139866
85.455761	2340.808088	22.144883
85.427838	2349.128811	22.149901
85.338426	2348.770382	22.154919
85.714706	2355.837925	22.159936
85.721896	2367.504951	22.164954
85.930508	2362.693888	22.169971
85.991609	2363.347085	22.174989
85.847133	2362.972034	22.180007
85.892278	2362.835544	22.185024
86.120478	2372.201855	22.190042
86.401238	2379.710449	22.195059
86.260090	2390.318180	22.200077
86.702329	2383.791453	22.205095
86.637612	2385.240768	22.210112
86.723633	2385.962652	22.215130
86.743175	2382.393157	22.220147
86.741652	2374.913373	22.225165
86.988238	2391.397022	22.230183
87.142325	2394.099757	22.235200
87.520246	2417.253836	22.240218
87.457243	2403.228397	22.245235
87.411479	2411.087993	22.250253
87.414777	2404.724710	22.255271
87.667228	2403.454254	22.260288
87.616764	2408.237363	22.265306
87.659042	2405.232404	22.270323
87.606984	2399.433274	22.275341
87.643685	2402.419515	22.280359
87.913226	2395.367518	22.285376
87.615193	2396.619835	22.290394
88.001469	2400.053131	22.295411
88.137896	2423.879436	22.300429
88.067000	2425.639023	22.305447
88.204150	2420.053265	22.310464
88.090668	2420.503418	22.315482
88.128738	2421.182318	22.320499
88.262225	2436.689548	22.325517
88.621798	2439.319065	22.330535
88.798455	2440.339209	22.335552
88.595429	2451.215473	22.340570
88.672060	2451.358103	22.345587
88.854170	2453.952303	22.350605
88.874798	2460.687403	22.355623
89.306766	2474.282626	22.360640
89.007351	2472.271718	22.365658
89.383076	2471.426960	22.370675
89.507190	2479.436714	22.375693
89.276364	2477.929510	22.380711
89.633222	2471.365630	22.385728
89.575338	2476.787459	22.390746
89.974170	2486.957161	22.395763
89.883136	2495.000630	22.400781
90.244893	2491.547930	22.405799
90.402347	2492.684706	22.410816
90.254972	2497.239999	22.415834
90.408695	2486.046317	22.420851
90.528010	2483.862497	22.425869
90.537403	2488.973956	22.430887
90.846636	2486.877158	22.435904
90.747482	2487.924735	22.440922
90.741534	2484.564362	22.445939
90.819220	2486.471109	22.450957
90.675115	2495.242492	22.455975
91.030309	2502.764725	22.460992
91.145622	2510.308763	22.466010
91.369104	2503.737361	22.471027
91.649315	2506.764372	22.476045
91.088628	2510.541732	22.481063
91.321672	2497.754388	22.486080
91.420283	2499.976627	22.491098
91.458308	2520.539245	22.496115
91.630640	2520.748941	22.501133
91.800563	2530.080279	22.506151
92.163211	2520.981087	22.511168
91.958035	2532.277505	22.516186
92.100252	2531.620822	22.521203
92.428135	2525.790532	22.526221
91.994504	2535.333208	22.531239
92.392655	2534.825797	22.536256
92.491925	2555.524043	22.541274
92.546426	2552.169968	22.546291
92.492593	2562.827244	22.551309
92.773395	2559.942698	22.556327
92.678164	2554.434335	22.561344
92.880181	2561.967967	22.566362
93.016000	2573.248861	22.571379
93.072414	2579.407135	22.576397
93.109905	2582.106072	22.581415
93.378124	2573.839092	22.586432
93.153370	2582.124480	22.591450
93.591986	2581.582323	22.596467
93.293815	2580.082505	22.601485
93.458243	2590.080684	22.606503
93.666591	2598.291913	22.611520
93.584072	2588.874224	22.616538
93.495842	2596.039887	22.621555
93.761257	2607.581396	22.626573
93.881057	2621.213013	22.631591
94.288220	2616.888387	22.636608
94.196196	2625.616956	22.641626
94.421763	2623.489065	22.646643
93.986886	2620.025434	22.651661
94.420535	2637.164889	22.656679
94.847151	2638.256349	22.661696
94.850200	2647.879009	22.666714
95.288253	2641.586402	22.671731
95.263442	2639.377800	22.676749
95.404941	2641.883706	22.681767
95.895717	2636.854775	22.686784
95.509073	2638.894252	22.691802
95.681167	2632.703282	22.696819
95.518379	2628.060802	22.701837
95.648860	2637.543559	22.706855
95.658294	2630.093514	22.711872
96.027320	2637.080245	22.716890
96.170095	2632.301519	22.721907
96.039091	2631.643452	22.726925
95.749897	2632.834433	22.731943
96.101595	2625.425453	22.736960
96.484585	2641.057890	22.741978
96.523624	2650.987374	22.746995
96.747541	2650.873374	22.752013
96.905840	2653.341931	22.757031
96.790816	2643.957711	22.762048
96.850789	2653.328431	22.767066
97.000794	2646.998890	22.772083
96.909092	2643.894948	22.777101
96.988141	2651.255356	22.782119
97.263088	2638.578126	22.787136
97.152884	2649.244285	22.792154
97.225497	2644.949973	22.797171
97.256772	2646.744073	22.802189
97.274558	2665.189083	22.807207
97.533974	2669.377694	22.812224
97.318874	2678.996675	22.817242
97.420954	2676.869187	22.822259
97.728679	2688.135845	22.827277
97.598937	2690.116141	22.832295
97.970104	2692.825941	22.837312
97.670197	2696.076431	22.842330
97.878681	2700.582334	22.847347
98.297321	2709.464496	22.852365
98.266494	2716.274033	22.857383
98.461985	2710.625391	22.862400
98.838586	2708.063523	22.867418
98.976994	2700.407029	22.872435
99.296061	2702.332792	22.877453
99.232711	2701.900837	22.882471
99.437237	2700.988205	22.887488
99.544369	2705.970791	22.892506
99.648727	2717.360858	22.897523
99.809027	2704.644732	22.902541
99.677848	2702.181356	22.907559
100.186632	2695.580968	22.912576
99.685278	2697.682608	22.917594
99.792037	2702.119233	22.922611
100.426845	2709.386283	22.927629
99.962412	2720.259477	22.932647
100.059879	2724.779624	22.937664
100.291034	2719.232701	22.942682
100.217181	2719.152727	22.947699
100.629934	2712.709406	22.952717
100.247569	2720.372533	22.957735
100.373636	2708.999988	22.962752
100.438528	2716.277424	22.967770
100.579850	2740.658870	22.972787
100.457295	2734.283626	22.977805
100.733837	2749.408909	22.982823
100.773707	2743.478487	22.987840
100.870160	2756.050230	22.992858
100.857851	2764.980998	22.997875
101.370623	2764.610278	23.002893
101.170187	2762.536487	23.007911
101.461919	2774.389600	23.012928
101.568752	2773.946761	23.017946
101.834257	2781.028672	23.022963
102.148980	2779.603250	23.027981
101.984954	2796.359910	23.032999
102.292633	2788.370708	23.038016
102.346104	2792.244432	23.043034
102.594410	2791.987738	23.048051
102.461875	2780.614631	23.053069
102.698312	2786.883645	23.058087
102.581138	2773.617578	23.063104
102.695241	2784.024585	23.068122
102.734692	2781.515529	23.073139
102.891201	2796.609157	23.078157
102.929598	2808.688198	23.083175
103.243837	2808.664200	23.088192
103.138889	2803.217252	23.093210
103.186894	2810.708837	23.098227
103.702454	2797.028003	23.103245
103.401780	2809.971309	23.108263
103.533844	2815.006830	23.113280
103.861886	2829.978927	23.118298
103.933226	2830.387510	23.123315
104.113709	2831.959411	23.128333
103.576770	2838.516886	23.133351
104.163385	2835.912630	23.138368
104.264113	2830.471324	23.143386
104.326788	2835.732345	23.148403
104.652639	2838.307238	23.153421
104.499300	2850.466845	23.158439
104.569127	2843.575367	23.163456
104.496992	2848.232584	23.168474
104.458098	2844.927805	23.173491
104.870367	2854.530651	23.178509
104.985945	2874.036819	23.183527
104.599247	2874.428789	23.188544
105.123001	2874.056346	23.193562
105.046135	2891.616897	23.198579
104.971410	2889.835861	23.203597
105.370103	2896.041618	23.208615
105.920568	2906.796952	23.213632
106.390194	2912.707543	23.218650
105.913171	2919.473438	23.223667
106.068450	2910.356040	23.228685
106.157499	2918.377796	23.233703
106.134669	2907.470323	23.238720
106.458129	2910.960904	23.243738
106.409338	2911.097937	23.248755
106.482467	2894.592096	23.253773
106.737482	2918.362603	23.258791
106.589252	2928.046989	23.263808
106.889774	2929.221347	23.268826
106.847502	2933.962281	23.273843
107.215825	2928.624208	23.278861
106.986339	2920.094174	23.283879
107.441234	2931.375803	23.288896
107.783844	2944.764448	23.293914
108.052125	2955.346242	23.298931
107.908950	2958.360756	23.303949
107.786883	2952.291512	23.308967
108.079984	2948.518080	23.313984
108.098793	2948.139527	23.319002
108.084737	2952.386831	23.324019
108.141610	2946.018120	23.329037
108.528683	2953.099991	23.334055
108.433373	2947.304304	23.339072
108.695106	2940.433223	23.344090
108.227311	2946.803155	23.349107
108.768540	2960.555223	23.354125
108.689854	2971.428101	23.359143
108.721071	2980.655155	23.364160
108.955954	2977.998673	23.369178
109.173404	2967.179769	23.374195
108.915569	2974.034437	23.379213
109.160001	2981.971910	23.384231
108.892989	3009.330889	23.389248
109.547245	3000.996923	23.394266
109.506528	3006.069036	23.399283
109.554403	3008.229851	23.404301
109.957500	3020.706394	23.409319
109.799692	3026.305012	23.414336
110.110418	3022.572990	23.419354
109.940850	3022.861508	23.424371
110.131091	3032.896920	23.429389
110.296784	3042.544810	23.434407
110.472439	3046.039637	23.439424
110.613488	3048.176390	23.444442
110.531874	3046.828822	23.449459
110.820510	3059.307543	23.454477
111.039635	3076.986027	23.459495
110.622689	3074.163371	23.464512
110.911955	3070.753482	23.469530
110.979778	3078.201043	23.474547
111.610645	3092.131699	23.479565
111.433056	3099.422029	23.484583
111.657718	3097.420474	23.489600
111.864225	3097.735293	23.494618
111.918592	3104.986129	23.499635
112.218444	3110.958103	23.504653
112.258160	3116.961364	23.509671
112.405436	3116.111338	23.514688
112.883884	3121.622929	23.519706
112.685589	3124.279981	23.524723
112.804556	3117.655294	23.529741
113.036537	3119.522153	23.534759
112.576342	3118.849360	23.539776
112.989656	3104.878157	23.544794
113.358748	3110.075471	23.549811
113.239728	3111.246133	23.554829
113.122991	3111.292812	23.559847
113.512017	3137.725425	23.564864
113.811953	3128.474785	23.569882
113.870528	3129.462968	23.574899
113.265490	3131.883901	23.579917
113.918741	3126.018225	23.584935
114.077179	3132.110205	23.589952
114.203354	3132.585954	23.594970
114.532485	3152.731248	23.599987
114.614073	3153.737922	23.605005
114.623487	3151.492333	23.610023
114.350067	3152.927062	23.615040
114.611207	3151.560507	23.620058
114.771005	3153.640679	23.625075
114.980441	3151.546817	23.630093
114.836014	3155.764093	23.635111
115.029989	3165.227712	23.640128
115.074202	3168.689498	23.645146
115.303854	3179.952916	23.650163
115.183449	3167.539255	23.655181
115.401496	3170.601369	23.660199
115.592543	3184.629409	23.665216
115.524696	3186.297060	23.670234
115.590326	3192.971728	23.675251
116.095272	3195.846867	23.680269
116.134012	3187.451434	23.685287
116.064104	3189.798005	23.690304
116.567139	3193.917011	23.695322
116.639432	3216.955878	23.700339
116.636533	3211.798976	23.705357
116.885363	3212.249198	23.710375
116.808518	3207.384790	23.715392
116.965853	3205.359053	23.720410
117.107426	3212.479488	23.725427
116.933897	3202.605452	23.730445
117.350162	3206.848524	23.735463
117.265003	3228.078283	23.740480
117.567805	3236.344445	23.745498
117.514776	3234.193848	23.750515
117.766799	3237.727247	23.755533
117.937767	3230.813464	23.760551
117.810023	3239.528988	23.765568
118.320122	3246.743202	23.770586
118.462329	3257.332301	23.775603
118.525852	3266.500783	23.780621
118.539783	3259.526371	23.785639
118.434953	3258.990431	23.790656
118.691884	3259.597199	23.795674
118.413109	3265.274811	23.800691
118.578146	3278.830401	23.805709
119.140203	3277.662883	23.810727
118.820688	3294.245518	23.815744
119.128213	3296.943289	23.820762
119.055178	3309.844975	23.825779
118.888742	3309.448092	23.830797
118.983870	3315.221799	23.835815
119.394247	3332.971572	23.840832
119.468856	3342.346670	23.845850
119.631709	3351.234505	23.850867
120.079401	3356.754144	23.855885
120.478617	3356.811524	23.860903
120.394785	3364.194585	23.865920
120.634772	3356.521900	23.870938
120.913867	3367.888159	23.875955
120.901493	3379.098086	23.880973
121.193265	3386.627472	23.885991
120.946080	3386.782965	23.891008
121.406658	3375.142966	23.896026
121.333094	3383.076778	23.901043
121.447555	3385.473398	23.906061
121.680618	3383.906065	23.911079
121.821764	3383.281084	23.916096
121.654442	3382.931683	23.921114
121.818406	3388.309560	23.926131
121.767401	3395.880027	23.931149
122.151708	3401.232857	23.936167
122.047254	3404.673791	23.941184
122.365722	3406.580789	23.946202
122.532509	3425.681837	23.951219
122.541793	3434.025637	23.956237
123.065050	3426.134946	23.961255
123.015450	3433.045540	23.966272
123.105951	3421.397208	23.971290
122.935146	3423.276702	23.976307
122.725841	3430.291223	23.981325
123.353351	3434.226656	23.986343
122.944710	3448.740234	23.991360
123.541434	3450.559455	23.996378
123.196258	3452.179046	24.001395
123.501074	3474.509519	24.006413
123.570766	3471.342273	24.011431
123.385474	3472.933661	24.016448
123.828655	3479.315718	24.021466
124.067245	3492.948322	24.026483
124.152989	3500.712038	24.031501
124.538140	3490.614596	24.036519
124.924405	3499.808385	24.041536
125.219494	3498.133479	24.046554
125.281527	3494.793831	24.051571
125.217625	3502.334799	24.056589
125.234095	3506.637421	24.061607
125.713678	3516.394206	24.066624
125.574700	3511.848769	24.071642
125.937142	3515.330205	24.076659
125.879963	3515.020359	24.081677
126.001201	3506.880141	24.086695
125.891685	3520.873466	24.091712
126.395544	3513.926360	24.096730
126.484038	3506.725542	24.101747
126.143672	3515.929020	24.106765
126.532379	3509.486029	24.111783
126.257830	3529.066650	24.116800
126.707263	3531.136210	24.121818
126.895377	3535.560296	24.126835
126.559006	3543.229188	24.131853
126.877734	3534.732916	24.136871
126.876629	3547.503562	24.141888
126.761799	3554.048818	24.146906
127.237689	3555.707070	24.151923
126.945071	3569.681774	24.156941
127.247728	3574.823349	24.161959
127.212140	3590.717882	24.166976
127.524073	3607.432289	24.171994
128.186962	3607.773465	24.177011
127.678377	3617.741931	24.182029
128.005040	3625.224918	24.187047
128.342163	3627.280521	24.192064
128.371618	3628.850905	24.197082
128.924518	3641.749454	24.202099
129.040857	3659.334140	24.207117
129.226696	3637.330550	24.212135
129.761308	3657.545220	24.217152
129.947473	3652.964590	24.222170
130.260087	3655.415423	24.227187
129.697789	3654.023175	24.232205
129.689612	3651.243702	24.237223
129.873879	3656.053493	24.242240
130.141509	3650.784644	24.247258
130.065998	3641.087548	24.252275
130.044417	3650.484189	24.257293
130.068383	3644.959975	24.262311
130.054321	3662.126361	24.267328
130.179300	3673.621118	24.272346
130.393060	3665.062321	24.277363
130.449772	3680.544773	24.282381
130.937830	3690.590709	24.287399
131.061605	3692.875438	24.292416
131.161282	3686.982682	24.297434
131.697326	3708.216686	24.302451
131.868016	3712.211124	24.307469
131.779930	3705.716507	24.312487
131.948261	3720.452389	24.317504
131.666871	3722.286112	24.322522
132.319457	3713.996273	24.327539
132.020790	3713.373901	24.332557
132.634476	3711.447057	24.337575
132.578921	3710.467806	24.342592
132.653769	3715.070654	24.347610
132.796888	3725.577820	24.352627
132.735238	3730.763888	24.357645
132.770799	3730.881399	24.362663
132.709827	3739.015402	24.367680
132.690046	3744.381140	24.372698
132.965352	3743.561529	24.377715
133.021980	3755.341649	24.382733
133.439354	3766.042598	24.387751
133.652310	3766.413234	24.392768
133.626302	3776.486096	24.397786
133.729385	3781.857848	24.402803
133.294257	3794.649319	24.407821
133.848183	3798.204972	24.412839
134.122594	3812.952718	24.417856
134.118430	3810.753364	24.422874
134.618221	3817.578034	24.427891
134.565538	3834.523375	24.432909
134.830757	3834.087262	24.437927
135.105298	3830.932049	24.442944
135.132187	3829.889374	24.447962
135.557789	3829.737459	24.452979
135.491014	3848.184299	24.457997
135.989185	3852.660891	24.463015
135.679155	3854.956788	24.468032
135.631325	3855.308311	24.473050
135.911374	3845.874197	24.478067
136.004723	3856.083066	24.483085
136.377190	3864.941471	24.488103
136.435317	3872.864336	24.493120
136.673976	3871.327650	24.498138
137.074233	3867.647715	24.503155
137.238576	3873.155090	24.508173
137.085931	3865.373257	24.513191
137.123254	3863.691356	24.518208
137.229281	3892.442005	24.523226
137.365088	3891.757872	24.528243
137.594012	3901.948684	24.533261
137.601853	3888.649586	24.538279
137.762763	3885.531104	24.543296
137.665915	3912.908978	24.548314
137.803543	3902.559699	24.553331
137.615870	3923.086676	24.558349
137.849641	3928.318054	24.563367
138.231029	3936.127175	24.568384
138.447239	3947.216420	24.573402
138.781740	3954.549966	24.578419
138.876423	3965.967589	24.583437
139.111824	3968.370590	24.588455
139.624134	3964.815119	24.593472
139.487224	3963.002685	24.598490
139.792222	3958.337078	24.603507
139.385460	3969.025223	24.608525
139.631179	3977.477427	24.613543
139.845786	3974.129570	24.618560
139.729844	3986.328270	24.623578
140.027468	3992.537617	24.628595
140.386283	4004.614605	24.633613
140.619843	4007.260943	24.638631
140.803492	4007.301598	24.643648
140.747981	4011.823939	24.648666
140.726098	4002.455984	24.653683
140.898254	4027.203635	24.658701
140.852258	4031.632955	24.663719
141.375141	4033.192356	24.668736
141.380872	4032.291866	24.673754
141.609408	4040.254391	24.678771
141.835663	4058.803889	24.683789
141.776223	4059.564412	24.688807
142.004725	4062.000071	24.693824
141.856165	4066.268709	24.698842
141.953353	4054.603140	24.703859
141.916320	4080.699862	24.708877
142.421775	4080.109320	24.713895
142.569672	4083.226770	24.718912
142.400043	4089.607202	24.723930
142.763660	4095.964067	24.728947
142.731097	4110.539198	24.733965
142.671181	4102.780613	24.738983
143.095083	4117.681947	24.744000
143.316592	4125.067985	24.749018
143.579782	4130.436852	24.754035
144.052518	4139.772087	24.759053
144.095257	4148.780138	24.764071
144.452166	4153.064300	24.769088
144.466021	4158.295477	24.774106
144.660779	4148.176997	24.779123
144.339091	4159.558966	24.784141
144.450988	4158.932228	24.789159
144.979244	4165.689444	24.794176
144.899667	4185.202349	24.799194
145.025342	4178.109072	24.804211
144.953270	4180.891698	24.809229
145.069361	4194.689220	24.814247
145.633247	4200.771701	24.819264
145.482785	4200.230255	24.824282
145.600046	4198.346414	24.829299
145.960823	4216.849747	24.834317
146.091517	4224.253210	24.839335
146.647686	4223.825167	24.844352
146.634517	4225.863120	24.849370
146.529282	4219.222653	24.854387
146.630552	4233.827419	24.859405
146.886902	4239.112166	24.864423
147.454506	4233.894004	24.869440
147.258622	4243.712815	24.874458
147.885824	4244.974968	24.879475
147.830122	4244.712225	24.884493
147.934972	4236.233351	24.889511
147.823228	4238.734964	24.894528
148.066650	4260.410017	24.899546
148.069829	4256.006257	24.904563
148.205351	4256.338533	24.909581
148.055268	4259.338561	24.914599
148.424985	4265.997550	24.919616
148.666544	4277.196659	24.924634
148.757740	4271.926863	24.929651
148.610191	4288.795953	24.934669
149.076678	4310.224637	24.939687
148.688552	4306.415610	24.944704
148.778600	4315.921365	24.949722
149.134337	4329.454181	24.954739
149.557076	4328.630387	24.959757
149.481020	4355.301779	24.964775
150.054938	4362.433848	24.969792
149.836109	4374.667865	24.974810
150.160718	4374.711689	24.979827
150.660698	4380.378120	24.984845
150.550382	4389.059901	24.989863
150.921902	4378.348592	24.994880
150.777168	4390.015473	24.999898
151.044165	4390.800624	25.004915
151.178781	4402.417436	25.009933
151.102783	4402.716566	25.014951
151.718916	4402.039234	25.019968
151.584120	4420.513093	25.024986
151.732489	4422.270087	25.030003
151.914388	4421.957492	25.035021
152.089578	4438.075421	25.040039
152.552254	4426.686942	25.045056
152.078474	4429.759805	25.050074
152.684694	4428.686309	25.055091
153.154430	4441.052391	25.060109
152.860843	4455.169967	25.065127
153.129550	4446.946252	25.070144
153.299113	4451.079916	25.075162
153.452624	4444.708165	25.080179
153.768935	4441.129649	25.085197
153.484576	4446.259274	25.090215
153.989783	4456.552314	25.095232
153.715123	4467.245306	25.100250
154.006522	4473.465264	25.105267
154.109494	4466.596386	25.110285
154.004746	4493.405048	25.115303
154.386827	4495.157000	25.120320
154.500236	4497.973746	25.125338
154.723567	4518.099261	25.130355
154.803038	4521.650478	25.135373
154.446915	4517.511272	25.140391
155.293240	4536.368149	25.145408
155.196569	4546.591394	25.150426
155.441561	4547.496790	25.155443
155.311278	4553.498753	25.160461
155.340049	4578.825164	25.165479
155.767579	4577.915383	25.170496
156.037245	4594.896159	25.175514
156.137933	4594.750953	25.180531
156.716373	4592.447605	25.185549
156.845372	4621.331540	25.190567
157.397974	4620.780945	25.195584
157.218669	4621.096263	25.200602
157.514708	4619.768325	25.205619
157.588100	4624.289564	25.210637
157.494045	4629.708234	25.215655
157.899761	4633.268336	25.220672
157.815795	4638.739089	25.225690
158.368485	4638.018028	25.230707
158.722242	4637.467019	25.235725
158.377187	4640.876437	25.240743
158.738954	4629.472076	25.245760
158.869059	4647.538510	25.250778
158.941224	4656.236021	25.255795
158.732060	4664.185323	25.260813
158.743264	4658.366087	25.265831
159.078326	4666.369018	25.270848
159.624812	4679.783830	25.275866
159.157190	4685.573536	25.280883
159.871983	4680.019694	25.285901
159.228534	4711.641543	25.290919
159.670465	4710.353874	25.295936
160.009089	4732.756361	25.300954
160.109723	4745.635015	25.305971
160.321485	4739.844308	25.310989
160.637028	4760.205011	25.316007
160.633088	4762.292084	25.321024
160.977046	4770.587225	25.326042
161.081263	4770.706613	25.331059
161.219198	4793.345790	25.336077
161.224275	4804.083538	25.341095
161.524600	4807.537081	25.346112
161.772271	4809.988778	25.351130
161.902255	4820.984745	25.356147
162.524706	4823.232529	25.361165
162.400219	4827.961585	25.366183
162.444799	4822.964084	25.371200
162.346312	4837.243940	25.376218
162.503781	4846.212267	25.381235
163.204375	4840.240780	25.386253
162.888111	4845.451272	25.391271
163.177250	4857.078889	25.396288
163.339037	4869.894390	25.401306
163.119151	4870.010893	25.406323
162.921843	4874.470436	25.411341
163.097688	4891.879696	25.416359
163.775299	4903.042444	25.421376
164.032939	4914.397255	25.426394
164.337089	4920.110320	25.431411
164.502843	4932.742163	25.436429
164.667289	4941.532676	25.441447
164.924320	4938.184311	25.446464
165.630573	4933.824914	25.451482
165.611354	4929.882202	25.456499
165.936138	4937.804792	25.461517
166.112785	4946.299836	25.466535
166.388359	4931.695403	25.471552
166.510720	4944.599205	25.476570
166.439304	4945.623636	25.481587
166.787267	4944.637920	25.486605
166.599487	4948.111139	25.491623
166.703734	4936.983673	25.496640
166.871431	4946.165094	25.501658
166.941862	4948.436244	25.506675
167.285569	4952.949938	25.511693
167.379870	4966.022292	25.516711
167.408049	4960.686413	25.521728
167.795886	4957.001895	25.526746
167.820177	4965.899605	25.531763
168.163164	4975.299792	25.536781
168.225063	4982.584923	25.541799
168.624071	4983.680861	25.546816
168.567429	4986.145535	25.551834
168.534772	4996.166452	25.556851
168.963011	5010.250289	25.561869
168.986516	5015.985254	25.566887
168.831146	5009.731142	25.571904
168.988010	5017.336006	25.576922
169.221805	5034.644784	25.581939
169.573947	5025.741699	25.586957
169.424935	5042.494922	25.591975
169.917109	5044.068696	25.596992
169.994911	5053.554661	25.602010
169.863647	5064.942083	25.607027
170.126919	5072.366158	25.612045
170.324383	5079.696378	25.617063
170.662952	5104.829784	25.622080
171.000496	5115.657679	25.627098
170.788836	5113.509613	25.632115
171.035562	5122.606140	25.637133
171.281826	5131.769034	25.642151
171.506722	5142.775578	25.647168
171.699735	5149.541492	25.652186
171.628140	5162.109667	25.657203
171.853260	5162.339538	25.662221
171.993190	5184.448579	25.667239
172.222523	5193.039653	25.672256
172.450277	5204.790748	25.677274
172.959133	5215.200443	25.682292
173.090770	5206.117166	25.687309
172.972014	5233.377350	25.692327
173.372421	5237.718089	25.697344
173.578340	5232.448984	25.702362
173.471941	5250.489935	25.707380
173.677513	5248.497453	25.712397
174.203912	5254.387299	25.717415
174.165485	5261.312620	25.722432
174.753216	5279.270110	25.727450
174.754913	5289.882409	25.732468
174.942815	5287.075124	25.737485
175.320807	5288.474254	25.742503
175.320519	5280.674258	25.747520
175.477601	5285.703394	25.752538
175.368565	5289.214847	25.757556
175.289047	5303.422650	25.762573
175.861030	5308.547781	25.767591
175.799016	5310.561942	25.772608
176.602830	5326.380154	25.777626
176.240501	5337.159991	25.782644
176.635230	5327.473556	25.787661
176.400115	5334.344489	25.792679
176.593920	5350.725468	25.797696
176.935769	5350.810790	25.802714
176.982412	5359.774637	25.807732
177.414199	5378.422706	25.812749
177.545191	5391.297062	25.817767
177.166572	5395.911401	25.822784
178.112207	5404.879639	25.827802
177.792056	5412.221637	25.832820
178.325813	5418.482869	25.837837
178.107757	5425.237524	25.842855
178.380073	5441.716768	25.847872
178.761305	5444.397005	25.852890
178.807645	5463.866300	25.857908
179.156751	5473.982348	25.862925
179.003797	5469.766901	25.867943
179.569536	5492.134743	25.872960
179.684537	5495.671115	25.877978
179.669602	5501.238638	25.882996
179.931429	5518.897031	25.888013
180.171564	5521.400513	25.893031
180.132390	5524.651690	25.898048
180.564829	5537.273741	25.903066
180.662919	5541.488298	25.908084
181.042317	5553.872449	25.913101
181.341546	5564.744493	25.918119
181.371648	5570.633276	25.923136
181.447468	5571.176958	25.928154
181.678068	5591.460355	25.933172
182.102672	5591.349628	25.938189
182.039487	5598.285268	25.943207
182.174311	5612.541806	25.948224
182.942882	5616.679754	25.953242
182.772481	5621.094225	25.958260
182.937349	5622.615157	25.963277
183.057043	5637.432818	25.968295
183.220792	5640.330243	25.973312
183.600498	5646.082208	25.978330
183.523697	5644.519036	25.983348
183.922937	5651.237045	25.988365
184.238420	5663.615501	25.993383
184.266719	5660.198668	25.998400
184.543237	5655.805412	26.003418
184.168674	5663.904170	26.008436
184.908446	5684.332029	26.013453
185.190511	5684.344646	26.018471
184.992990	5687.895291	26.023488
185.436406	5697.955653	26.028506
185.408780	5708.241335	26.033524
185.677221	5711.397003	26.038541
185.671972	5717.821697	26.043559
186.318536	5730.965918	26.048576
186.523530	5733.598046	26.053594
186.414178	5735.149321	26.058612
186.734869	5741.425104	26.063629
186.659226	5726.351046	26.068647
186.936458	5730.007257	26.073664
186.824425	5748.542028	26.078682
187.012419	5759.778853	26.083700
187.222586	5762.397548	26.088717
187.435730	5768.535510	26.093735
187.536760	5778.068720	26.098752
188.299276	5782.305513	26.103770
188.015415	5802.268837	26.108788
187.999992	5798.909335	26.113805
188.630507	5815.323332	26.118823
188.909885	5821.151048	26.123840
189.157850	5827.817060	26.128858
189.041242	5829.669367	26.133876
189.237934	5823.514500	26.138893
189.399596	5837.915376	26.143911
189.361661	5848.155401	26.148928
189.850761	5858.559091	26.153946
189.933919	5867.249145	26.158964
189.757027	5871.718357	26.163981
190.252494	5891.774348	26.168999
190.501799	5891.889957	26.174016
190.634763	5908.587171	26.179034
191.009636	5930.060530	26.184052
190.791221	5931.909855	26.189069
191.139567	5936.268390	26.194087
190.965583	5951.277523	26.199104
191.746996	5968.542436	26.204122
191.725516	5979.449187	26.209140
192.005618	5990.725389	26.214157
192.327051	6008.879999	26.219175
192.369763	6014.950041	26.224192
192.598860	6021.047708	26.229210
193.045453	6035.981789	26.234228
193.029320	6038.778031	26.239245
193.207894	6044.328031	26.244263
193.359617	6066.559405	26.249280
193.676767	6071.330082	26.254298
193.670775	6081.394768	26.259316
193.696686	6097.821660	26.264333
194.234746	6099.006374	26.269351
194.248937	6122.945076	26.274368
194.639415	6121.832684	26.279386
194.816080	6143.258425	26.284404
194.945519	6153.235641	26.289421
195.185017	6143.273202	26.294439
195.263288	6166.475865	26.299456
195.781882	6168.288675	26.304474
196.143947	6167.613210	26.309492
196.007658	6201.932986	26.314509
196.079820	6203.345376	26.319527
196.259233	6208.516481	26.324544
196.673699	6217.120073	26.329562
197.204865	6220.916539	26.334580
197.014816	6222.414203	26.339597
197.489686	6238.931885	26.344615
197.852061	6243.237787	26.349632
197.764240	6243.040024	26.354650
198.010810	6248.213247	26.359668
198.513078	6262.889405	26.364685
198.476353	6264.678732	26.369703
198.484273	6266.290599	26.374720
198.988199	6273.349158	26.379738
198.683374	6288.287516	26.384756
198.803533	6288.417046	26.389773
199.078783	6285.308658	26.394791
199.528436	6309.220424	26.399808
199.776080	6314.832293	26.404826
199.656940	6316.571400	26.409844
199.651655	6321.777785	26.414861
199.996726	6327.121850	26.419879
200.305879	6344.031778	26.424896
200.600200	6351.432570	26.429914
200.784156	6365.606235	26.434932
200.881440	6371.882510	26.439949
201.324956	6376.649255	26.444967
201.304245	6385.586274	26.449984
201.389942	6388.777003	26.455002
201.497248	6390.509054	26.460020
201.805762	6410.424434	26.465037
202.474165	6416.156671	26.470055
202.383965	6437.504603	26.475072
202.038469	6444.229086	26.480090
202.642492	6446.558890	26.485108
202.700049	6471.160500	26.490125
203.157668	6467.963532	26.495143
203.545799	6487.935974	26.500160
203.726177	6499.370171	26.505178
203.750141	6499.461107	26.510196
204.073081	6514.209756	26.515213
204.274712	6514.995775	26.520231
204.170841	6518.478241	26.525248
204.418006	6544.432942	26.530266
204.806023	6552.156921	26.535284
204.765660	6568.537794	26.540301
205.320925	6563.355639	26.545319
205.299043	6588.841142	26.550336
205.769516	6596.539595	26.555354
205.785954	6602.642359	26.560372
206.028008	6621.173050	26.565389
206.482311	6622.039452	26.570407
206.252704	6632.461470	26.575424
206.566774	6653.335929	26.580442
207.299903	6655.358260	26.585460
207.438765	6654.686177	26.590477
207.602983	6664.866577	26.595495
207.733278	6679.178322	26.600512
207.811263	6676.703734	26.605530
208.032422	6684.936908	26.610548
208.120252	6693.768681	26.615565
208.807119	6698.349016	26.620583
208.640527	6706.725023	26.625600
208.986394	6730.741990	26.630618
209.134894	6718.978292	26.635636
209.355370	6730.302175	26.640653
209.820773	6751.604472	26.645671
209.885192	6743.973658	26.650688
209.851223	6743.691688	26.655706
209.860313	6750.714305	26.660724
210.117159	6772.390241	26.665741
210.851090	6784.028331	26.670759
210.803047	6804.574549	26.675776
210.769081	6803.856927	26.680794
211.069090	6809.814317	26.685812
211.236170	6830.206902	26.690829
211.764747	6827.633293	26.695847
211.881923	6849.245964	26.700864
211.938111	6855.064778	26.705882
211.983573	6854.782990	26.710900
212.219165	6880.225405	26.715917
212.590167	6884.552207	26.720935
213.090826	6893.909745	26.725952
212.923926	6908.492366	26.730970
213.347621	6909.041573	26.735988
213.462606	6916.524357	26.741005
214.151133	6929.445044	26.746023
214.217670	6936.525027	26.751040
214.091565	6951.315962	26.756058
214.193364	6945.131390	26.761076
214.104824	6964.440307	26.766093
214.643466	6955.961671	26.771111
214.948392	6961.567923	26.776128
215.035433	6977.152600	26.781146
215.143550	6978.998229	26.786164
215.072566	7008.400271	26.791181
215.271405	7015.222789	26.796199
215.576691	7026.138953	26.801216
215.952991	7050.018980	26.806234
216.281775	7055.274260	26.811252
216.431165	7068.431037	26.816269
216.600344	7083.343137	26.821287
216.999396	7092.293665	26.826304
217.092408	7103.255756	26.831322
217.815844	7113.977032	26.836340
217.765486	7132.263608	26.841357
218.219320	7123.788711	26.846375
218.318589	7149.792692	26.851392
218.362728	7159.048250	26.856410
218.862798	7148.084737	26.861428
218.789043	7163.653721	26.866445
219.431243	7164.212904	26.871463
220.075647	7163.382683	26.876480
219.955293	7164.942114	26.881498
220.521574	7167.088508	26.886516
220.144922	7193.441762	26.891533
220.670735	7181.375575	26.896551
220.848477	7182.181151	26.901568
220.556899	7183.476967	26.906586
221.354084	7197.416303	26.911604
221.587447	7210.979903	26.916621
221.607482	7210.752605	26.921639
221.665184	7221.729769	26.926656
221.561683	7240.817176	26.931674
221.938412	7247.501419	26.936692
222.029245	7262.397525	26.941709
221.954501	7273.051359	26.946727
222.161284	7278.638356	26.951744
222.432031	7300.101220	26.956762
222.830519	7314.936545	26.961780
222.850274	7328.186426	26.966797
223.223789	7344.749398	26.971815
223.258536	7361.166564	26.976832
223.612383	7381.760963	26.981850
224.310250	7375.211369	26.986868
224.186375	7396.294186	26.991885
224.685155	7400.856811	26.996903
225.294528	7409.414649	27.001920
225.425176	7417.877007	27.006938
225.834963	7407.975606	27.011956
226.351937	7415.338794	27.016973
226.336349	7436.843516	27.021991
226.475383	7435.855679	27.027008
226.875815	7437.778685	27.032026
226.952441	7432.870164	27.037044
227.123548	7439.207850	27.042061
227.210112	7446.714244	27.047079
227.500172	7455.397893	27.052096
227.359720	7460.117497	27.057114
227.614996	7466.034754	27.062132
227.512704	7487.865662	27.067149
227.934330	7487.446012	27.072167
228.045758	7505.073055	27.077184
227.938364	7511.274445	27.082202
228.396266	7521.403000	27.087220
228.575684	7550.302599	27.092237
228.521535	7554.636179	27.097255
229.068846	7568.078250	27.102272
229.015781	7586.605634	27.107290
229.306308	7601.679095	27.112308
229.464219	7629.246765	27.117325
229.693637	7626.176904	27.122343
230.103815	7653.398860	27.127360
230.213311	7673.602507	27.132378
230.516267	7683.196628	27.137396
230.871978	7699.229168	27.142413
231.019180	7715.925796	27.147431
231.223421	7730.059451	27.152448
231.679726	7752.440888	27.157466
231.769423	7757.560187	27.162484
232.115083	7782.074218	27.167501
232.589920	7788.061366	27.172519
232.645687	7799.471694	27.177536
232.961465	7819.598987	27.182554
233.089520	7822.922241	27.187572
233.478922	7839.612609	27.192589
233.561570	7857.111901	27.197607
233.976422	7859.932458	27.202624
233.971316	7885.016177	27.207642
234.466473	7888.262992	27.212660
234.611664	7908.556017	27.217677
234.984451	7916.286116	27.222695
235.673454	7922.375513	27.227712
235.536588	7933.689817	27.232730
236.036094	7938.148280	27.237748
236.102368	7943.618579	27.242765
236.465491	7964.221647	27.247783
236.864026	7961.368335	27.252800
236.770191	7966.705868	27.257818
237.063626	7981.154081	27.262836
237.262500	7988.381063	27.267853
237.657767	7997.664120	27.272871
237.987541	8005.745118	27.277888
237.886545	8010.764919	27.282906
237.763244	8030.683402	27.287924
238.098811	8040.528326	27.292941
238.249551	8059.201054	27.297959
238.582710	8065.251530	27.302976
238.681388	8083.850354	27.307994
238.692358	8103.047003	27.313012
239.079424	8121.417575	27.318029
239.468369	8137.322163	27.323047
240.143050	8154.002855	27.328064
240.183988	8165.365218	27.333082
240.807960	8178.836769	27.338100
241.055483	8181.781461	27.343117
240.795466	8190.081217	27.348135
241.250137	8203.285695	27.353152
241.396727	8209.166546	27.358170
241.866412	8227.224354	27.363188
241.799769	8236.302065	27.368205
242.134103	8250.778810	27.373223
242.197806	8263.116379	27.378240
242.609187	8277.221162	27.383258
242.790492	8287.734440	27.388276
242.926996	8296.565670	27.393293
243.212788	8321.149781	27.398311
243.609709	8321.551688	27.403328
243.918629	8342.510956	27.408346
243.862161	8344.155191	27.413364
244.017306	8347.569010	27.418381
244.227147	8372.922805	27.423399
244.499016	8376.270987	27.428416
244.751964	8386.028009	27.433434
245.363156	8399.681683	27.438452
245.578469	8415.815769	27.443469
245.214788	8413.981584	27.448487
245.938840	8430.137017	27.453504
246.442753	8436.167181	27.458522
247.086439	8443.406747	27.463540
247.504484	8445.065058	27.468557
247.805339	8451.164923	27.473575
247.874258	8440.154533	27.478592
248.218343	8445.054214	27.483610
248.335233	8442.740625	27.488628
248.679478	8456.363544	27.493645
248.469284	8463.174904	27.498663
248.559091	8467.230415	27.503680
248.841913	8468.060632	27.508698
249.328882	8489.049004	27.513716
249.682744	8487.317094	27.518733
249.693851	8503.660049	27.523751
249.931709	8509.160466	27.528768
249.931775	8517.012349	27.533786
249.964966	8535.261967	27.538804
250.390499	8552.098866	27.543821
250.626390	8573.593929	27.548839
250.888680	8586.642545	27.553856
250.690327	8604.647513	27.558874
250.917753	8614.651758	27.563892
251.436502	8629.361959	27.568909
251.430814	8654.749902	27.573927
251.782009	8676.444869	27.578944
252.068113	8691.390468	27.583962
252.726415	8715.938850	27.588980
252.731516	8721.472635	27.593997
252.868673	8738.484324	27.599015
253.535168	8746.651817	27.604032
253.473383	8759.356668	27.609050
253.918905	8782.306187	27.614068
254.477448	8797.537545	27.619085
254.404857	8815.058902	27.624103
255.030585	8831.567915	27.629120
255.168325	8843.540662	27.634138
255.032234	8855.862565	27.639156
255.305087	8866.314473	27.644173
255.798836	8889.708055	27.649191
255.749868	8894.862020	27.654208
256.200695	8915.824965	27.659226
256.604831	8931.989910	27.664244
256.950571	8949.543737	27.669261
257.226467	8959.512161	27.674279
257.122599	8973.271960	27.679296
257.808251	8979.327507	27.684314
257.867052	9010.521509	27.689332
258.178471	9013.611031	27.694349
258.187064	9032.398569	27.699367
258.590481	9042.258657	27.704384
258.983698	9063.047672	27.709402
259.413778	9073.411921	27.714420
259.940833	9079.735457	27.719437
259.825296	9099.173962	27.724455
259.714401	9094.256490	27.729472
259.834110	9105.266103	27.734490
260.601432	9137.905867	27.739508
261.069761	9138.959639	27.744525
261.060175	9157.071334	27.749543
261.294099	9167.024343	27.754560
261.672063	9185.170074	27.759578
261.713293	9193.375726	27.764596
262.217968	9193.656585	27.769613
262.169411	9203.584404	27.774631
262.404189	9223.028150	27.779648
262.527148	9230.984218	27.784666
262.595020	9250.930893	27.789684
262.970070	9262.854106	27.794701
263.521314	9280.246605	27.799719
263.937874	9282.789274	27.804736
264.203782	9311.463376	27.809754
264.016291	9326.666800	27.814772
264.381560	9331.885446	27.819789
264.891043	9356.154887	27.824807
265.208670	9370.104695	27.829824
265.047603	9393.607805	27.834842
265.487603	9392.342235	27.839860
266.114651	9398.097683	27.844877
266.196472	9415.557530	27.849895
266.261175	9416.867144	27.854912
266.830449	9433.530775	27.859930
266.850383	9444.710929	27.864948
267.367880	9460.716497	27.869965
267.321824	9485.019457	27.874983
267.520650	9501.447547	27.880000
268.083441	9519.024744	27.885018
267.905424	9533.361738	27.890036
268.390040	9542.353731	27.895053
268.714171	9571.729517	27.900071
269.040865	9577.462611	27.905088
269.161160	9599.368482	27.910106
269.503705	9628.523616	27.915124
270.468346	9629.209193	27.920141
270.377114	9640.075354	27.925159
270.589696	9665.604140	27.930176
271.225737	9667.616774	27.935194
271.291886	9681.972466	27.940212
271.858533	9696.167675	27.945229
272.066318	9693.394503	27.950247
271.996504	9703.629026	27.955264
272.206577	9721.258511	27.960282
272.414875	9740.716419	27.965300
273.212322	9744.213010	27.970317
273.094191	9767.533051	27.975335
273.255086	9770.257921	27.980352
273.822689	9782.552295	27.985370
273.861358	9803.205077	27.990388
274.315878	9814.712050	27.995405
274.630507	9828.659515	28.000423
275.004068	9836.282947	28.005440
275.224550	9846.882538	28.010458
275.082218	9866.922791	28.015476
275.643164	9865.410911	28.020493
275.464908	9881.933138	28.025511
275.780197	9902.315364	28.030528
276.108561	9922.818703	28.035546
275.791657	9942.305418	28.040564
276.784059	9957.296109	28.045581
277.167862	9990.957309	28.050599
277.250628	10002.228992	28.055616
277.502553	10015.409691	28.060634
277.261426	10031.487227	28.065652
278.249521	10052.522008	28.070669
278.332326	10068.886680	28.075687
278.740570	10080.802062	28.080704
279.421367	10100.161069	28.085722
279.376954	10115.576373	28.090740
279.772773	10126.076035	28.095757
280.108875	10139.729884	28.100775
280.426516	10140.349491	28.105792
280.489355	10147.551264	28.110810
280.520123	10168.505646	28.115828
280.975389	10176.397434	28.120845
281.323032	10195.398258	28.125863
281.507278	10215.605591	28.130880
281.651011	10229.412782	28.135898
282.037340	10240.813874	28.140916
282.302237	10249.594346	28.145933
282.596265	10267.732180	28.150951
282.820428	10287.352362	28.155968
283.078133	10304.488685	28.160986
283.223933	10320.625842	28.166004
283.600187	10329.786752	28.171021
283.762767	10358.876494	28.176039
284.166522	10371.610557	28.181056
284.687062	10381.620359	28.186074
284.591654	10404.703980	28.191092
285.268239	10420.467587	28.196109
285.596526	10433.835542	28.201127
285.410767	10456.305036	28.206144
285.771485	10473.719025	28.211162
286.137589	10495.439040	28.216180
286.678494	10506.074065	28.221197
286.575866	10530.245157	28.226215
286.763539	10547.054818	28.231232
287.375648	10568.610080	28.236250
287.487830	10589.968974	28.241268
288.097402	10603.251941	28.246285
288.242899	10621.293399	28.251303
288.208931	10643.379379	28.256320
288.769551	10662.833578	28.261338
289.051186	10678.210900	28.266356
289.504450	10707.372478	28.271373
289.900904	10723.104443	28.276391
290.002079	10725.134674	28.281408
290.581062	10741.466414	28.286426
290.611552	10763.412979	28.291444
291.386734	10784.450366	28.296461
291.653206	10787.092540	28.301479
291.677720	10809.791595	28.306496
291.891568	10819.483398	28.311514
292.230443	10849.600915	28.316532
292.640609	10854.715074	28.321549
293.095965	10868.082381	28.326567
293.466696	10881.867125	28.331584
293.652282	10900.278324	28.336602
294.097966	10907.152023	28.341620
294.270771	10915.378870	28.346637
294.750164	10927.624668	28.351655
295.035650	10944.362528	28.356672
295.073894	10967.599572	28.361690
295.140853	10973.462197	28.366708
295.529970	10984.939091	28.371725
295.876382	11006.883816	28.376743
296.000926	11013.867855	28.381760
296.180220	11029.362541	28.386778
296.496984	11062.799352	28.391796
296.577288	11081.167226	28.396813
297.230370	11098.794925	28.401831
297.075336	11120.092080	28.406848
297.661277	11137.193537	28.411866
297.606170	11166.236534	28.416884
298.128702	11192.145132	28.421901
298.563914	11210.937498	28.426919
298.295656	11232.988247	28.431936
298.829229	11245.434171	28.436954
299.406399	11275.350847	28.441972
299.574149	11282.069291	28.446989
299.919473	11296.729831	28.452007
300.170921	11325.996612	28.457024
300.898883	11331.285315	28.462042
300.796707	11349.802027	28.467060
301.071924	11371.158376	28.472077
301.597073	11370.318259	28.477095
301.564784	11401.101074	28.482112
301.931017	11428.651209	28.487130
302.498575	11443.352836	28.492148
302.956265	11460.711505	28.497165
302.845314	11474.379520	28.502183
303.087880	11494.282275	28.507200
304.161912	11510.821333	28.512218
303.759490	11530.263092	28.517236
304.289290	11551.144004	28.522253
304.490016	11566.004237	28.527271
304.853296	11592.579347	28.532288
305.321505	11600.109734	28.537306
305.492007	11625.022559	28.542324
305.982554	11632.675768	28.547341
306.546339	11660.978410	28.552359
306.522995	11678.608410	28.557376
306.982483	11691.097814	28.562394
306.932907	11713.812724	28.567412
307.127275	11737.086260	28.572429
307.470210	11743.629014	28.577447
307.722701	11763.937846	28.582464
308.274090	11783.874633	28.587482
308.469216	11799.604304	28.592500
309.224376	11818.615569	28.597517
309.397751	11843.389292	28.602535
309.979416	11860.072100	28.607552
310.294200	11869.085508	28.612570
310.376599	11886.288631	28.617588
310.564387	11905.499381	28.622605
311.481279	11909.470292	28.627623
311.712047	11922.838799	28.632640
312.091510	11923.107749	28.637658
312.587750	11931.467527	28.642676
312.960365	11942.849703	28.647693
313.438136	11945.076854	28.652711
314.041702	11949.425263	28.657728
314.627949	11931.125775	28.662746
315.173449	11945.218647	28.667764
314.990004	11957.837361	28.672781
315.479336	11955.907088	28.677799
315.631583	11949.289818	28.682816
315.854564	11940.337360	28.687834
316.075925	11956.164101	28.692852
315.911546	11951.756337	28.697869
316.087576	11964.770306	28.702887
316.379102	11982.843880	28.707904
316.686848	12002.939061	28.712922
316.943201	12014.686848	28.717940
316.942534	12035.206149	28.722957
317.252390	12046.775055	28.727975
317.376399	12075.099843	28.732992
317.718139	12089.237373	28.738010
317.736405	12108.073846	28.743028
317.878966	12142.370364	28.748045
318.178846	12164.847926	28.753063
318.313107	12191.623962	28.758080
318.487247	12220.054796	28.763098
319.086292	12254.150541	28.768116
319.090536	12278.632391	28.773133
319.792002	12309.914368	28.778151
320.105961	12333.962521	28.783168
320.372046	12353.824607	28.788186
320.967694	12375.343477	28.793204
320.822247	12404.999364	28.798221
321.479851	12422.359185	28.803239
321.811149	12453.086764	28.808256
322.114219	12474.367372	28.813274
322.831913	12494.323072	28.818292
322.651044	12518.145817	28.823309
323.173240	12540.983735	28.828327
323.160220	12559.932926	28.833344
323.735824	12587.524591	28.838362
324.153847	12605.916839	28.843380
324.161881	12637.036405	28.848397
324.827359	12649.007867	28.853415
325.073002	12684.782897	28.858432
325.730886	12696.872421	28.863450
326.023904	12717.160143	28.868468
326.249220	12744.914277	28.873485
326.674415	12763.618187	28.878503
326.925220	12793.812612	28.883520
327.502042	12801.329629	28.888538
327.972834	12814.569591	28.893556
328.276990	12840.157824	28.898573
328.731930	12837.721271	28.903591
328.984328	12869.472417	28.908608
329.284858	12887.668606	28.913626
329.522862	12893.931355	28.918644
329.889499	12919.487803	28.923661
330.672118	12924.237872	28.928679
330.460443	12957.103973	28.933696
330.739528	12968.656160	28.938714
331.052550	12991.167384	28.943732
331.453465	13008.482691	28.948749
331.565481	13037.120276	28.953767
331.618477	13054.995395	28.958784
332.040876	13086.638169	28.963802
332.319235	13116.017199	28.968820
332.436083	13144.038387	28.973837
333.396811	13171.681108	28.978855
333.485760	13196.052979	28.983872
333.953671	13215.514873	28.988890
334.127992	13242.750344	28.993908
334.752824	13258.110755	28.998925
335.109276	13270.885777	29.003943
335.497395	13307.347054	29.008960
335.697109	13317.402369	29.013978
336.518106	13340.646041	29.018996
336.533470	13367.016035	29.024013
337.385613	13374.499629	29.029031
337.710021	13399.245418	29.034048
337.923727	13403.292067	29.039066
338.290791	13418.547718	29.044084
338.526136	13438.766297	29.049101
339.168560	13463.342351	29.054119
339.095593	13475.960558	29.059136
339.485358	13491.484301	29.064154
340.039698	13499.235655	29.069172
340.223140	13516.857082	29.074189
340.341583	13537.390932	29.079207
340.860839	13548.110030	29.084224
341.127599	13572.710332	29.089242
341.477877	13586.225514	29.094260
342.181959	13605.543443	29.099277
342.357513	13618.264928	29.104295
342.450703	13633.734186	29.109312
342.787979	13653.441216	29.114330
343.101240	13667.328587	29.119348
343.620631	13696.746555	29.124365
343.762690	13699.778123	29.129383
344.253361	13725.897312	29.134400
344.210788	13736.745578	29.139418
344.704693	13751.659506	29.144436
344.823130	13761.010909	29.149453
345.092595	13775.041016	29.154471
345.248070	13797.770519	29.159488
345.772478	13833.538790	29.164506
346.058050	13848.100143	29.169524
346.122603	13879.058145	29.174541
346.527361	13898.656958	29.179559
347.086453	13923.654055	29.184576
347.135937	13948.993133	29.189594
347.786465	13983.696601	29.194612
348.068654	14000.721919	29.199629
348.290982	14027.180418	29.204647
348.614304	14058.012908	29.209664
348.661030	14086.283328	29.214682
349.784943	14112.982852	29.219700
349.572483	14132.302771	29.224717
350.187030	14163.159293	29.229735
350.337571	14187.579633	29.234752
350.667338	14216.301737	29.239770
351.810657	14238.674908	29.244788
351.761511	14279.470036	29.249805
352.536319	14291.396995	29.254823
352.915264	14316.119644	29.259840
352.645005	14339.447050	29.264858
353.263390	14356.615831	29.269876
353.307933	14383.225840	29.274893
353.891903	14404.603574	29.279911
354.415532	14429.051053	29.284928
354.859442	14453.530000	29.289946
355.589035	14474.483913	29.294964
355.698884	14491.975653	29.299981
356.214598	14510.720799	29.304999
356.770893	14524.564412	29.310016
357.038802	14543.465259	29.315034
357.505784	14555.418495	29.320052
357.755757	14572.708343	29.325069
358.069508	14578.770294	29.330087
358.683746	14613.313212	29.335104
358.651338	14617.183915	29.340122
359.318975	14648.765612	29.345140
359.458794	14661.900801	29.350157
359.651676	14674.036008	29.355175
360.219951	14697.974684	29.360192
360.400265	14708.535931	29.365210
360.942633	14725.698004	29.370228
361.258133	14754.552641	29.375245
361.337891	14772.346225	29.380263
361.635273	14787.029618	29.385280
361.740304	14812.443255	29.390298
362.359328	14840.884124	29.395316
362.698126	14870.111117	29.400333
362.856113	14889.569585	29.405351
363.425141	14910.729151	29.410368
363.655349	14937.835120	29.415386
364.274534	14965.966641	29.420404
364.303019	14988.938533	29.425421
364.837317	15005.028311	29.430439
365.512066	15034.923019	29.435456
365.751066	15056.083909	29.440474
366.026933	15075.034568	29.445492
366.408665	15099.836754	29.450509
366.991377	15114.330425	29.455527
367.667823	15129.643212	29.460544
367.633714	15151.993447	29.465562
367.982192	15157.999611	29.470580
368.199167	15171.514693	29.475597
368.492899	15199.119568	29.480615
369.043754	15218.311543	29.485632
369.307448	15231.456144	29.490650
369.455095	15245.323235	29.495668
369.976456	15265.341037	29.500685
370.206986	15283.203071	29.505703
371.101126	15312.542727	29.510720
370.916379	15338.438300	29.515738
371.299536	15353.086585	29.520756
371.631657	15387.081329	29.525773
372.104422	15423.299680	29.530791
372.063678	15443.405716	29.535808
372.903637	15460.051243	29.540826
373.194335	15493.307295	29.545844
373.501834	15514.938032	29.550861
374.325703	15546.108265	29.555879
374.385893	15557.377319	29.560896
375.008446	15589.182403	29.565914
375.737351	15605.627526	29.570932
375.890600	15625.535972	29.575949
376.126198	15642.323701	29.580967
376.748458	15653.182616	29.585984
376.823862	15675.819511	29.591002
377.314238	15700.539132	29.596020
377.501372	15726.790727	29.601037
377.803850	15739.519013	29.606055
378.167793	15769.353010	29.611072
378.456451	15793.349491	29.616090
379.173813	15817.825255	29.621108
379.435577	15846.490977	29.626125
379.931239	15877.457328	29.631143
380.348003	15890.850030	29.636160
380.560679	15923.762148	29.641178
381.205889	15942.178892	29.646196
381.352497	15965.897789	29.651213
381.796685	15986.496951	29.656231
382.048111	16003.099327	29.661248
382.343372	16027.259306	29.666266
382.865550	16055.189692	29.671284
383.354753	16082.717844	29.676301
383.820901	16104.649716	29.681319
384.128753	16125.608337	29.686336
384.529712	16141.761020	29.691354
385.098377	16164.201206	29.696372
385.014275	16186.134082	29.701389
385.296498	16221.297275	29.706407
385.976287	16238.237041	29.711424
385.878411	16277.805931	29.716442
386.465045	16305.252813	29.721460
387.103188	16337.410446	29.726477
387.172613	16357.364365	29.731495
387.758040	16389.817766	29.736512
387.927768	16428.495413	29.741530
388.521390	16451.026780	29.746548
389.102926	16477.482936	29.751565
389.372045	16498.792308	29.756583
390.043362	16515.035615	29.761600
390.585289	16546.602234	29.766618
390.979806	16572.216062	29.771636
391.493375	16594.573784	29.776653
392.104071	16602.800838	29.781671
392.147778	16610.851391	29.786688
392.527633	16630.892786	29.791706
393.157082	16652.468058	29.796724
393.176456	16679.451584	29.801741
393.574683	16705.845170	29.806759
394.323310	16712.285039	29.811776
394.052872	16727.677937	29.816794
394.204224	16754.855677	29.821812
394.759783	16784.174817	29.826829
395.239961	16804.387033	29.831847
395.545571	16834.174965	29.836864
395.577167	16865.155584	29.841882
395.706672	16894.232087	29.846900
396.236557	16926.644555	29.851917
396.466046	16955.269604	29.856935
397.049215	16991.002987	29.861952
397.415142	17024.698422	29.866970
397.690010	17051.768792	29.871988
398.579956	17087.593280	29.877005
398.979833	17112.862699	29.882023
399.050424	17141.266540	29.887040
399.976917	17176.403208	29.892058
400.438066	17197.209480	29.897076
400.911014	17226.308494	29.902093
400.996263	17261.166461	29.907111
401.941883	17276.167164	29.912128
402.060249	17300.811292	29.917146
402.365600	17328.123649	29.922164
403.015829	17349.140525	29.927181
403.544002	17381.137083	29.932199
404.062916	17398.472635	29.937216
404.147405	17430.545089	29.942234
404.929699	17446.436982	29.947252
405.068338	17472.341620	29.952269
405.252036	17492.161941	29.957287
405.938492	17520.899454	29.962304
406.374676	17549.000252	29.967322
406.947877	17579.303347	29.972340
407.182326	17596.310909	29.977357
407.593081	17620.113654	29.982375
407.860063	17638.853441	29.987392
408.383603	17666.353208	29.992410
408.617105	17695.168245	29.997428
409.265780	17720.197331	30.002445
409.772449	17746.107863	30.007463
410.264781	17768.375512	30.012480
410.259106	17799.350828	30.017498
410.712681	17825.440354	30.022516
410.972124	17847.630857	30.027533
411.546439	17882.628132	30.032551
411.790265	17900.285192	30.037568
412.631152	17931.355548	30.042586
413.069066	17961.629893	30.047604
413.287794	17984.667158	30.052621
413.443270	18016.988480	30.057639
413.914099	18037.029720	30.062656
414.463221	18061.234609	30.067674
414.655325	18084.945823	30.072692
415.443163	18113.535668	30.077709
415.744725	18145.019357	30.082727
416.050808	18167.032346	30.087744
416.337750	18197.160131	30.092762
417.122731	18232.339838	30.097780
417.388460	18256.627265	30.102797
417.404556	18291.036729	30.107815
417.904278	18311.490690	30.112832
418.553312	18339.742506	30.117850
418.659914	18371.560345	30.122868
419.338382	18399.990850	30.127885
419.741181	18435.015987	30.132903
420.032948	18460.676840	30.137920
420.519085	18495.815386	30.142938
421.034676	18525.920502	30.147956
421.858337	18547.562239	30.152973
422.020972	18563.425759	30.157991
422.485727	18571.521736	30.163008
422.853690	18596.071553	30.168026
423.042900	18619.986040	30.173044
423.699627	18649.260572	30.178061
424.088832	18679.600525	30.183079
424.653958	18700.297361	30.188096
424.638110	18729.209848	30.193114
424.941984	18754.806016	30.198132
425.537027	18773.426018	30.203149
425.615107	18801.098252	30.208167
426.128536	18838.141110	30.213184
427.032562	18871.919734	30.218202
427.239081	18910.356494	30.223220
427.451687	18935.329095	30.228237
428.135982	18960.354203	30.233255
428.479893	18990.360572	30.238272
428.753259	19025.697665	30.243290
428.933762	19059.280366	30.248308
429.766049	19079.683046	30.253325
430.157345	19114.483763	30.258343
430.292625	19158.782526	30.263360
431.279083	19181.170254	30.268378
431.690728	19218.811026	30.273396
432.566328	19250.446670	30.278413
432.956001	19275.145573	30.283431
433.026973	19297.645239	30.288448
433.766844	19321.461699	30.293466
433.917706	19355.289634	30.298484
434.910916	19367.226623	30.303501
435.222664	19397.794637	30.308519
435.565865	19429.248607	30.313536
435.962154	19451.501639	30.318554
436.151925	19475.612943	30.323572
436.782405	19492.819172	30.328589
437.396942	19525.968248	30.333607
437.719627	19543.721854	30.338624
438.123997	19558.442667	30.343642
438.444905	19585.787350	30.348660
439.319860	19607.997176	30.353677
439.588809	19646.596192	30.358695
439.784351	19672.103125	30.363712
440.578755	19693.365321	30.368730
440.818891	19713.305426	30.373748
441.486518	19747.621724	30.378765
441.638100	19768.384470	30.383783
442.271584	19792.117080	30.388800
442.478156	19821.432292	30.393818
442.750552	19844.956163	30.398836
443.274228	19880.129232	30.403853
443.887315	19910.183307	30.408871
444.064219	19937.633172	30.413888
444.730324	19965.101224	30.418906
444.786345	20010.185142	30.423924
445.316832	20033.902587	30.428941
446.028634	20061.363617	30.433959
446.514945	20082.061630	30.438976
446.755345	20114.417350	30.443994
447.017127	20151.855935	30.449012
447.480972	20175.249124	30.454029
447.971450	20214.774930	30.459047
448.051283	20244.995179	30.464064
448.839570	20278.990235	30.469082
449.007675	20312.406435	30.474100
449.772061	20342.917664	30.479117
450.297037	20382.855411	30.484135
450.494618	20409.481320	30.489152
450.878966	20436.280197	30.494170
451.314853	20472.504282	30.499188
451.963932	20491.401787	30.504205
452.657130	20528.103775	30.509223
452.734808	20551.431531	30.514240
453.114144	20580.935641	30.519258
453.536737	20607.981496	30.524276
454.110785	20635.142671	30.529293
454.236112	20667.056084	30.534311
455.023247	20696.938781	30.539328
455.956861	20735.170460	30.544346
456.263683	20770.486505	30.549364
456.734610	20792.261808	30.554381
456.994657	20823.282431	30.559399
457.531530	20851.966151	30.564416
457.992483	20880.762900	30.569434
457.937728	20915.933648	30.574452
458.642332	20942.796787	30.579469
458.977655	20988.363632	30.584487
458.934872	21017.694411	30.589504
459.728422	21053.320155	30.594522
460.274484	21092.952754	30.599540
461.288459	21133.023946	30.604557
461.378475	21174.358319	30.609575
462.169995	21199.407411	30.614592
462.831843	21220.856314	30.619610
463.018765	21252.445098	30.624628
463.732494	21285.234092	30.629645
464.166627	21320.714421	30.634663
464.714645	21347.406763	30.639680
465.419888	21378.213202	30.644698
466.034592	21405.173196	30.649716
466.364578	21431.697606	30.654733
466.740033	21456.085552	30.659751
467.113081	21481.409063	30.664768
467.705120	21508.878240	30.669786
468.213709	21545.908019	30.674804
468.127130	21571.872315	30.679821
468.654732	21590.707763	30.684839
469.336744	21638.692411	30.689856
470.046503	21664.810124	30.694874
470.293299	21692.624292	30.699892
470.796457	21728.461028	30.704909
471.038606	21755.656777	30.709927
471.635231	21795.099625	30.714944
471.802587	21818.850826	30.719962
472.516978	21865.466104	30.724980
472.970883	21897.652298	30.729997
473.354732	21937.179306	30.735015
473.741750	21964.763373	30.740032
474.029552	22005.847347	30.745050
474.826707	22042.144108	30.750068
475.189619	22074.837710	30.755085
475.905763	22107.627693	30.760103
476.514402	22141.609874	30.765120
476.968454	22178.263929	30.770138
477.743307	22201.421249	30.775156
478.297104	22228.271849	30.780173
478.764580	22250.586408	30.785191
479.073854	22274.606597	30.790208
479.848728	22297.738751	30.795226
480.326982	22317.043902	30.800244
480.629138	22350.562614	30.805261
481.482977	22366.662167	30.810279
481.917313	22405.695646	30.815296
482.517919	22424.741619	30.820314
482.855909	22441.781404	30.825332
483.537040	22467.051605	30.830349
483.926746	22477.663267	30.835367
483.899646	22492.864592	30.840384
484.395372	22509.576420	30.845402
484.839763	22534.548882	30.850420
484.935340	22554.008985	30.855437
485.457339	22585.433674	30.860455
485.539389	22623.328468	30.865472
486.255505	22645.901524	30.870490
486.788266	22684.262957	30.875508
486.921266	22709.928952	30.880525
487.642412	22747.888180	30.885543
488.062764	22786.033611	30.890560
488.560469	22825.967935	30.895578
488.873605	22864.281967	30.900596
489.328475	22902.807680	30.905613
490.071262	22930.267859	30.910631
490.484694	22983.555323	30.915648
490.937198	23010.005786	30.920666
491.421148	23042.113303	30.925684
491.809178	23080.681425	30.930701
492.587538	23115.479140	30.935719
492.590778	23160.104566	30.940736
493.770812	23195.616768	30.945754
493.943535	23236.696034	30.950772
494.370224	23282.456059	30.955789
494.882825	23317.207282	30.960807
495.504799	23359.992141	30.965824
495.871211	23394.387241	30.970842
495.849043	23430.764317	30.975860
496.513712	23479.564999	30.980877
497.132058	23520.992128	30.985895
497.462547	23567.311331	30.990912
498.177279	23610.846835	30.995930
498.578564	23658.286319	31.000948
499.134795	23697.202130	31.005965
500.044191	23741.604777	31.010983
500.487697	23789.113791	31.016000
501.004004	23821.659852	31.021018
501.556731	23871.907207	31.026036
501.915587	23896.863178	31.031053
502.852416	23940.320380	31.036071
503.878813	23977.975048	31.041088
504.548744	23985.693563	31.046106
505.192974	24015.932271	31.051124
505.943282	24034.507662	31.056141
506.597076	24059.423963	31.061159
506.544103	24082.820568	31.066176
507.548312	24093.747614	31.071194
508.104475	24113.017031	31.076212
508.306428	24139.640943	31.081229
509.138738	24160.232163	31.086247
509.351047	24198.052669	31.091264
509.542747	24218.023859	31.096282
509.926251	24246.313107	31.101300
510.416039	24269.858744	31.106317
510.840368	24306.616166	31.111335
511.134214	24337.017670	31.116352
511.929139	24367.726233	31.121370
512.286822	24392.910512	31.126388
512.782549	24428.734319	31.131405
513.210351	24465.023839	31.136423
513.406737	24505.811304	31.141440
514.205942	24532.291640	31.146458
514.681866	24571.512432	31.151476
514.771297	24602.003231	31.156493
515.522505	24636.959525	31.161511
515.710324	24674.620454	31.166528
516.287574	24704.365122	31.171546
516.950590	24749.712310	31.176564
517.168842	24786.875749	31.181581
517.651605	24813.728322	31.186599
518.212374	24851.438606	31.191616
518.707356	24887.920599	31.196634
518.955711	24929.990009	31.201652
519.428725	24971.607217	31.206669
520.437858	25008.602959	31.211687
521.251729	25048.062462	31.216704
521.656880	25083.124292	31.221722
522.014572	25126.434624	31.226740
522.091924	25159.531914	31.231757
522.864276	25201.842133	31.236775
523.386406	25246.144459	31.241792
524.443441	25277.495906	31.246810
524.924068	25313.399495	31.251828
524.930223	25355.653084	31.256845
525.948103	25388.578165	31.261863
526.009425	25431.316223	31.266880
527.102279	25466.087735	31.271898
527.732988	25503.251096	31.276916
527.953251	25541.161361	31.281933
528.696464	25572.372823	31.286951
529.269744	25615.738921	31.291968
529.618072	25645.034200	31.296986
530.333052	25685.723874	31.302004
530.709946	25726.453942	31.307021
531.277264	25751.139411	31.312039
531.864012	25799.926346	31.317056
531.966783	25844.289347	31.322074
532.762376	25877.281643	31.327092
533.098188	25915.667476	31.332109
534.186494	25951.849910	31.337127
534.732575	25992.294894	31.342144
535.514117	26018.912680	31.347162
536.302335	26061.076859	31.352180
536.472866	26090.236308	31.357197
537.224483	26114.621594	31.362215
537.396465	26150.366450	31.367232
537.970098	26177.554217	31.372250
538.688596	26215.147550	31.377268
538.956910	26254.871827	31.382285
539.565271	26284.626599	31.387303
540.251573	26327.546754	31.392320
540.391424	26364.169203	31.397338
541.220530	26395.317926	31.402356
541.607239	26448.372283	31.407373
542.250535	26474.683672	31.412391
542.761155	26513.650003	31.417408
543.139372	26550.488264	31.422426
543.848949	26585.694633	31.427444
544.297861	26620.006491	31.432461
545.010529	26650.333249	31.437479
545.599895	26694.830471	31.442496
546.011490	26731.335179	31.447514
546.661150	26772.549217	31.452532
546.851111	26810.302278	31.457549
547.869065	26851.066935	31.462567
548.287919	26889.884032	31.467584
548.349588	26927.202338	31.472602
549.285520	26969.446402	31.477620
549.448335	27012.766014	31.482637
550.123902	27046.606989	31.487655
550.363713	27094.206262	31.492672
551.288883	27139.018450	31.497690
551.940041	27174.683742	31.502708
552.251394	27215.047841	31.507725
553.235986	27244.966316	31.512743
553.724203	27289.120417	31.517760
554.337828	27316.202323	31.522778
554.772852	27352.464300	31.527796
555.394440	27386.914742	31.532813
556.007823	27408.453734	31.537831
556.506160	27443.593549	31.542848
557.031777	27474.203656	31.547866
557.657981	27509.355161	31.552884
558.251760	27542.084716	31.557901
558.912325	27576.662107	31.562919
559.155257	27599.498150	31.567936
559.407043	27636.971277	31.572954
560.194298	27673.058569	31.577972
560.831478	27714.744197	31.582989
561.384821	27755.046185	31.588007
561.991757	27789.948369	31.593024
562.306645	27835.350681	31.598042
562.752179	27874.348777	31.603060
563.034381	27916.122015	31.608077
563.518182	27961.826828	31.613095
564.074356	28004.246291	31.618112
564.739655	28054.840383	31.623130
565.407180	28103.575960	31.628148
565.897100	28150.424287	31.633165
566.677153	28203.124540	31.638183
567.018998	28256.734222	31.643200
567.571691	28295.785868	31.648218
568.250750	28346.056166	31.653236
568.628621	28397.922357	31.658253
569.326403	28449.138097	31.663271
570.092485	28489.698975	31.668288
570.464212	28537.900397	31.673306
571.561812	28583.510469	31.678324
571.917575	28629.142013	31.683341
572.651209	28662.591005	31.688359
573.714590	28704.205582	31.693376
574.093784	28752.583325	31.698394
574.601208	28789.481249	31.703412
574.897755	28828.479214	31.708429
575.638618	28870.783057	31.713447
576.364185	28917.374999	31.718464
577.092572	28962.645520	31.723482
577.628965	29002.004474	31.728500
577.850712	29038.359734	31.733517
578.549329	29078.053725	31.738535
579.621822	29122.208775	31.743552
580.072060	29172.150317	31.748570
580.472678	29213.073276	31.753588
581.087594	29251.111950	31.758605
581.511061	29285.590302	31.763623
582.196481	29318.061827	31.768640
582.954574	29372.974592	31.773658
583.693675	29400.747577	31.778676
584.066169	29453.938393	31.783693
584.911828	29484.697343	31.788711
585.491371	29524.929180	31.793728
585.673541	29558.503929	31.798746
586.381607	29604.373237	31.803764
586.909463	29644.897857	31.808781
587.077991	29689.802537	31.813799
587.772022	29726.224113	31.818816
588.318544	29767.384494	31.823834
588.919338	29816.893142	31.828852
589.286817	29860.294184	31.833869
590.143562	29902.569361	31.838887
590.484458	29956.006629	31.843904
590.815206	30000.842331	31.848922
591.301408	30040.590410	31.853940
591.897555	30097.256188	31.858957
592.504899	30142.314374	31.863975
593.286274	30189.134348	31.868992
593.909166	30231.573251	31.874010
594.743921	30275.597336	31.879028
595.260148	30313.116111	31.884045
595.659170	30357.726967	31.889063
596.668790	30404.448469	31.894080
597.077645	30445.789799	31.899098
597.752454	30487.513097	31.904116
598.280913	30537.679590	31.909133
599.119622	30577.714855	31.914151
599.572449	30622.570715	31.919168
600.281917	30666.166429	31.924186
600.702228	30704.453194	31.929204
601.483936	30752.829487	31.934221
602.092725	30794.626959	31.939239
603.194943	30837.390296	31.944256
603.216203	30883.964237	31.949274
604.047051	30925.961095	31.954292
604.390929	30960.113345	31.959309
604.843343	31007.113123	31.964327
605.627842	31056.842513	31.969344
606.121085	31117.522467	31.974362
607.026847	31155.089230	31.979380
607.669201	31200.536181	31.984397
608.139188	31246.484352	31.989415
608.832862	31281.612782	31.994432
609.415842	31334.092725	31.999450
609.861241	31366.244727	32.004468
610.651716	31419.160197	32.009485
611.180524	31469.992673	32.014503
611.965682	31518.022514	32.019520
612.063735	31562.430226	32.024538
612.614679	31613.430274	32.029556
614.057966	31660.080372	32.034573
614.077531	31703.577693	32.039591
615.147896	31758.416278	32.044608
615.381870	31807.936559	32.049626
616.382251	31852.633461	32.054644
617.152295	31892.106730	32.059661
617.528675	31943.267683	32.064679
618.375608	31981.256079	32.069696
618.709663	32029.496831	32.074714
619.506480	32077.134178	32.079732
620.255100	32123.672842	32.084749
620.523044	32166.095429	32.089767
621.176360	32219.906845	32.094784
621.926458	32262.209863	32.099802
622.590369	32309.938099	32.104820
623.681622	32355.879930	32.109837
624.107414	32397.974810	32.114855
624.593981	32440.610274	32.119872
625.113157	32485.763220	32.124890
625.793785	32526.395986	32.129908
626.087516	32569.460203	32.134925
626.872016	32619.357702	32.139943
627.574242	32665.987028	32.144960
627.723365	32718.285517	32.149978
628.704387	32760.407971	32.154996
629.725106	32815.901972	32.160013
630.415311	32863.728509	32.165031
631.046626	32899.482686	32.170048
631.458885	32947.106378	32.175066
631.997753	32980.953224	32.180084
632.869565	33027.980387	32.185101
633.329641	33072.302998	32.190119
634.259463	33108.592429	32.195136
634.428968	33143.003162	32.200154
635.482747	33174.285036	32.205172
636.096025	33211.199544	32.210189
636.836741	33253.828475	32.215207
637.909504	33277.369051	32.220224
638.183058	33308.621581	32.225242
638.847404	33338.333534	32.230260
639.969154	33371.779935	32.235277
640.249158	33406.534168	32.240295
640.736711	33428.295152	32.245312
641.099931	33467.038495	32.250330
641.738873	33505.296164	32.255348
642.364817	33540.647645	32.260365
642.953740	33583.168248	32.265383
643.781510	33624.753750	32.270400
643.889627	33672.799741	32.275418
644.519355	33720.011784	32.280436
645.375166	33765.930361	32.285453
645.965217	33816.569277	32.290471
646.811813	33858.063778	32.295488
647.346365	33901.921259	32.300506
647.677011	33942.415584	32.305524
648.685788	33988.765912	32.310541
648.997596	34038.462624	32.315559
649.815408	34075.852423	32.320576
650.420827	34136.340212	32.325594
651.146247	34195.431061	32.330612
651.775247	34245.438973	32.335629
652.169905	34293.403567	32.340647
653.157297	34323.028387	32.345664
653.677622	34385.452290	32.350682
654.529368	34441.305827	32.355700
655.117485	34484.220378	32.360717
655.407092	34531.740411	32.365735
656.343564	34578.236136	32.370752
656.577740	34643.424368	32.375770
657.440613	34699.055549	32.380788
658.291467	34754.568627	32.385805
658.464131	34815.499173	32.390823
659.314647	34867.383339	32.395840
660.347154	34909.110028	32.400858
661.014957	34963.988431	32.405876
661.860997	35015.785142	32.410893
662.272268	35064.653045	32.415911
663.082092	35112.086589	32.420928
663.948375	35166.997663	32.425946
664.462903	35217.771898	32.430964
665.165901	35263.129637	32.435981
665.972566	35319.062104	32.440999
666.757560	35364.407219	32.446016
667.229561	35416.541695	32.451034
668.029866	35463.636077	32.456052
668.989978	35507.847559	32.461069
669.489607	35555.223182	32.466087
670.148016	35603.490878	32.471104
670.724719	35647.320085	32.476122
671.569617	35694.148753	32.481140
671.866744	35734.879383	32.486157
672.531959	35785.087596	32.491175
673.580172	35843.006990	32.496192
673.908031	35887.438414	32.501210
674.441551	35936.099485	32.506228
675.332419	35986.386650	32.511245
675.655516	36029.990791	32.516263
676.485661	36078.321194	32.521280
677.297308	36136.898102	32.526298
677.777540	36179.093170	32.531316
678.541965	36221.224846	32.536333
679.075467	36269.083637	32.541351
680.018625	36314.083527	32.546368
680.516905	36360.329300	32.551386
681.129272	36398.052566	32.556404
682.044013	36441.217116	32.561421
682.572518	36493.048186	32.566439
683.205635	36532.437779	32.571456
683.805138	36587.274158	32.576474
684.506801	36624.218722	32.581492
685.221957	36675.180007	32.586509
685.731618	36723.720145	32.591527
686.454798	36784.102184	32.596544
687.235766	36824.284872	32.601562
687.393591	36879.564246	32.606580
688.452520	36927.860746	32.611597
689.199142	36991.439331	32.616615
689.659978	37041.846916	32.621632
690.325132	37092.298504	32.626650
691.044574	37157.601812	32.631668
691.895675	37209.029984	32.636685
692.804420	37259.538671	32.641703
693.581404	37318.528950	32.646720
693.806538	37367.374367	32.651738
694.294681	37439.575766	32.656756
695.421745	37488.482567	32.661773
695.767140	37556.179053	32.666791
696.828779	37616.409257	32.671808
697.470342	37679.133677	32.676826
698.250001	37733.242855	32.681844
699.274719	37787.933508	32.686861
699.704830	37836.400091	32.691879
700.501257	37899.284288	32.696896
700.990410	37961.299853	32.701914
701.614750	38023.111039	32.706932
702.540997	38071.936792	32.711949
703.106893	38140.593408	32.716967
704.020341	38192.589632	32.721984
704.705507	38242.389440	32.727002
705.725681	38293.287830	32.732020
707.010841	38341.621648	32.737037
707.522178	38404.621527	32.742055
707.448158	38457.512915	32.747072
708.807649	38504.810999	32.752090
709.275311	38573.168182	32.757108
710.029390	38611.201989	32.762125
710.706979	38664.545330	32.767143
711.412986	38715.867025	32.772160
712.523763	38776.826354	32.777178
712.625458	38833.491822	32.782196
713.263499	38878.766214	32.787213
714.360595	38948.980118	32.792231
714.620980	38996.862459	32.797248
715.524644	39054.724631	32.802266
716.170004	39121.632818	32.807284
717.098957	39175.975196	32.812301
717.774385	39235.846695	32.817319
718.381419	39292.238180	32.822336
719.169528	39342.561949	32.827354
719.654976	39404.316621	32.832372
720.119197	39465.796532	32.837389
720.716483	39531.771217	32.842407
721.144551	39592.188366	32.847424
722.324129	39655.068263	32.852442
723.359108	39714.954344	32.857460
724.357810	39776.187004	32.862477
724.916337	39837.697468	32.867495
725.516347	39894.369882	32.872512
726.462767	39937.606054	32.877530
726.943280	39993.728256	32.882548
727.951809	40030.162612	32.887565
728.478195	40090.369695	32.892583
729.279543	40141.490105	32.897600
730.167349	40186.310706	32.902618
730.527372	40240.852357	32.907636
731.111907	40290.957228	32.912653
731.747383	40347.094020	32.917671
732.619135	40396.420527	32.922688
733.347077	40452.808736	32.927706
733.954433	40510.379668	32.932724
735.363165	40573.080873	32.937741
735.366790	40632.106424	32.942759
736.131014	40692.783881	32.947776
736.992140	40745.705148	32.952794
737.716444	40810.266100	32.957812
738.270351	40865.986931	32.962829
739.152389	40935.374466	32.967847
739.690982	41006.624831	32.972864
740.325265	41057.432021	32.977882
740.963800	41124.777500	32.982900
742.056370	41178.024072	32.987917
742.642400	41253.264971	32.992935
743.426605	41320.227734	32.997952
744.283325	41387.634723	33.002970
744.580950	41461.700835	33.007988
745.670004	41522.019813	33.013005
746.162217	41590.667228	33.018023
747.002418	41654.877306	33.023040
748.049055	41719.333535	33.028058
748.722412	41802.557158	33.033076
749.550549	41866.744446	33.038093
750.129913	41935.075696	33.043111
751.056494	41997.938709	33.048128
752.261688	42059.588171	33.053146
752.792276	42130.950957	33.058164
753.722968	42194.680399	33.063181
754.639855	42264.446172	33.068199
755.035039	42319.986823	33.073216
755.996163	42378.993621	33.078234
756.624421	42456.205409	33.083252
757.257875	42513.530832	33.088269
758.653488	42580.787513	33.093287
759.035240	42643.351858	33.098304
760.057841	42703.773032	33.103322
760.497984	42765.689749	33.108340
761.453237	42835.198314	33.113357
762.433991	42892.565212	33.118375
762.826750	42951.264061	33.123392
764.058698	43006.605829	33.128410
764.657860	43088.530288	33.133428
765.493638	43139.298079	33.138445
765.806068	43202.387198	33.143463
766.726781	43267.202906	33.148480
767.805426	43319.229748	33.153498
768.379035	43388.388673	33.158516
769.337063	43438.176567	33.163533
770.455734	43509.907130	33.168551
770.738976	43570.516028	33.173568
771.727776	43624.404645	33.178586
772.204184	43688.101998	33.183604
773.220454	43749.665579	33.188621
774.091737	43806.343546	33.193639
774.373021	43870.015046	33.198656
775.507497	43930.485302	33.203674
776.222008	43991.173296	33.208692
777.036065	44047.057509	33.213709
777.912349	44109.308178	33.218727
778.091137	44153.482510	33.223744
779.148252	44202.927677	33.228762
779.680142	44263.632360	33.233780
780.582217	44325.272346	33.238797
781.568176	44382.351307	33.243815
782.147723	44439.285312	33.248832
782.763365	44494.841162	33.253850
783.246282	44558.527332	33.258868
784.104540	44628.822094	33.263885
785.325121	44683.417077	33.268903
786.033219	44743.621050	33.273920
787.050112	44795.445946	33.278938
788.036764	44861.135237	33.283956
788.399826	44917.591981	33.288973
789.289229	44976.591613	33.293991
790.063794	45042.485442	33.299008
790.835050	45101.617768	33.304026
791.454823	45170.553590	33.309044
792.312449	45231.823492	33.314061
793.133096	45297.976539	33.319079
793.802511	45366.519317	33.324096
794.589917	45424.036882	33.329114
795.552465	45492.673311	33.334132
796.499312	45567.246073	33.339149
797.343694	45626.981943	33.344167
798.370101	45702.643401	33.349184
799.165955	45753.663782	33.354202
800.005917	45825.717445	33.359220
800.651987	45882.707960	33.364237
801.555707	45940.385761	33.369255
802.034427	46008.675688	33.374272
803.080023	46069.323798	33.379290
803.995744	46140.158337	33.384308
804.673643	46201.307203	33.389325
805.974781	46263.010226	33.394343
806.036080	46328.045301	33.399360
807.044916	46390.578879	33.404378
807.970905	46467.251829	33.409396
808.863197	46535.763267	33.414413
809.810601	46601.147486	33.419431
810.000599	46671.325541	33.424448
811.621205	46719.852973	33.429466
812.561632	46784.536609	33.434484
813.243192	46855.264557	33.439501
814.141882	46912.755846	33.444519
814.770269	46985.339790	33.449536
815.371157	47032.610488	33.454554
816.274073	47103.260264	33.459572
817.017681	47167.805005	33.464589
817.983162	47224.748891	33.469607
818.733931	47289.235919	33.474624
819.489185	47365.052958	33.479642
820.485181	47421.448492	33.484660
821.366543	47494.228528	33.489677
822.240191	47552.649018	33.494695
823.054743	47615.267016	33.499712
823.868596	47673.241676	33.504730
824.868022	47731.889664	33.509748
825.506500	47801.203850	33.514765
826.590057	47859.592261	33.519783
827.029420	47916.468430	33.524800
828.043890	47981.333681	33.529818
828.759395	48043.013059	33.534836
829.537271	48112.097587	33.539853
830.346583	48177.482669	33.544871
831.234637	48243.013773	33.549888
832.038299	48313.233664	33.554906
832.895973	48365.262515	33.559924
833.622862	48419.754056	33.564941
834.514307	48468.601870	33.569959
835.129676	48525.034436	33.574976
836.065100	48586.560640	33.579994
836.867881	48642.603527	33.585012
837.334810	48696.649278	33.590029
838.412386	48752.877169	33.595047
839.247760	48822.353429	33.600064
839.628120	48887.598929	33.605082
840.447787	48951.358619	33.610100
841.258411	49034.505315	33.615117
842.255822	49092.176458	33.620135
842.927850	49165.766483	33.625152
843.922649	49234.725534	33.630170
844.268708	49307.696406	33.635188
845.255581	49382.155226	33.640205
846.312242	49449.637389	33.645223
846.732482	49536.643202	33.650240
847.755909	49614.463001	33.655258
848.727419	49694.201952	33.660276
849.309284	49771.952232	33.665293
850.315106	49847.434573	33.670311
850.913808	49933.414265	33.675328
852.156045	50024.557662	33.680346
853.253331	50097.242573	33.685364
854.181286	50175.174125	33.690381
855.062775	50251.461825	33.695399
855.700313	50331.495708	33.700416
856.565022	50402.484350	33.705434
857.441796	50490.814262	33.710452
858.148142	50574.482699	33.715469
859.428726	50655.536939	33.720487
860.077217	50729.243207	33.725504
861.092726	50807.922459	33.730522
862.065791	50886.412477	33.735540
862.683168	50965.350752	33.740557
863.718433	51049.032675	33.745575
864.545330	51124.882559	33.750592
865.410612	51209.490169	33.755610
866.448113	51287.433624	33.760628
867.097799	51364.413015	33.765645
868.326742	51446.066562	33.770663
869.320534	51525.504622	33.775680
869.940336	51606.982032	33.780698
870.834846	51676.375369	33.785716
871.702363	51767.369166	33.790733
872.636485	51839.623182	33.795751
873.451933	51922.032855	33.800768
874.440359	51995.841776	33.805786
875.248945	52078.601097	33.810804
876.073908	52149.778481	33.815821
877.206372	52224.078113	33.820839
877.817147	52297.744636	33.825856
878.919702	52379.617407	33.830874
879.882378	52453.577346	33.835892
880.423755	52540.790598	33.840909
881.462059	52607.784943	33.845927
882.182350	52685.770089	33.850944
883.423799	52757.719384	33.855962
884.341802	52835.110891	33.860980
885.011275	52921.881538	33.865997
886.371655	52990.130092	33.871015
887.059279	53072.146191	33.876032
888.044730	53145.130247	33.881050
889.106659	53212.470660	33.886068
889.769969	53283.955236	33.891085
890.635841	53348.169069	33.896103
891.661085	53403.808963	33.901120
892.683545	53466.321675	33.906138
893.591442	53523.404035	33.911156
894.368452	53589.125862	33.916173
895.984355	53638.491301	33.921191
896.703999	53694.983403	33.926208
897.276416	53760.389699	33.931226
898.108435	53818.073171	33.936244
898.810231	53883.060876	33.941261
899.570255	53938.730908	33.946279
900.852695	54004.083659	33.951296
901.564615	54070.443511	33.956314
902.436333	54142.942217	33.961332
902.894493	54204.045457	33.966349
903.883528	54273.475984	33.971367
905.344105	54345.497084	33.976384
905.953709	54400.084310	33.981402
906.917435	54464.001090	33.986420
907.727249	54547.167600	33.991437
908.613233	54612.356293	33.996455
909.327166	54701.531303	34.001472
910.087837	54769.815638	34.006490
911.416625	54843.270122	34.011508
911.779056	54918.312697	34.016525
912.595022	54990.942970	34.021543
914.097979	55080.723634	34.026560
914.456617	55158.178708	34.031578
915.515610	55232.106978	34.036596
916.175443	55320.229593	34.041613
917.350136	55406.012623	34.046631
918.209287	55484.776346	34.051648
919.306908	55569.192402	34.056666
920.201749	55644.856380	34.061684
921.044348	55730.825480	34.066701
921.753554	55817.018293	34.071719
922.990195	55893.895278	34.076736
923.673472	55985.301269	34.081754
924.463927	56074.488428	34.086772
925.495744	56167.017686	34.091789
926.548450	56248.456004	34.096807
927.339060	56337.789683	34.101824
928.831679	56429.893395	34.106842
929.878910	56505.896984	34.111860
930.529936	56592.291567	34.116877
931.981141	56665.302142	34.121895
932.899918	56752.402188	34.126912
933.627248	56841.753983	34.131930
934.670608	56900.924464	34.136948
935.918224	56978.480415	34.141965
936.572851	57055.553526	34.146983
937.466822	57131.386896	34.152000
938.255356	57218.914084	34.157018
939.559901	57288.949559	34.162036
940.503452	57376.263176	34.167053
941.228644	57440.997432	34.172071
942.295550	57522.722663	34.177088
942.983905	57612.317600	34.182106
944.001444	57688.228314	34.187124
944.637578	57767.774971	34.192141
945.725783	57842.801680	34.197159
946.821935	57935.650468	34.202176
947.794705	58011.695793	34.207194
948.854359	58093.303837	34.212212
949.394264	58163.980578	34.217229
950.510755	58258.105935	34.222247
951.709076	58338.958896	34.227264
952.250897	58420.079481	34.232282
953.156571	58499.440767	34.237300
954.213697	58567.581907	34.242317
955.236742	58641.671888	34.247335
955.893772	58714.502884	34.252352
956.293808	58801.799148	34.257370
957.505959	58875.803271	34.262388
958.699728	58956.336201	34.267405
959.280001	59030.597968	34.272423
960.522019	59113.611362	34.277440
960.963324	59209.137348	34.282458
962.168506	59293.245806	34.287476
963.214320	59375.898382	34.292493
964.708072	59452.448975	34.297511
965.669720	59539.678940	34.302528
966.543595	59623.992326	34.307546
967.859472	59704.147821	34.312564
968.659013	59775.959588	34.317581
969.551820	59854.846251	34.322599
970.561009	59934.335262	34.327616
971.232248	60017.744932	34.332634
972.365438	60093.847611	34.337652
973.387315	60178.241012	34.342669
974.451645	60262.874921	34.347687
975.468445	60361.765061	34.352704
976.318117	60446.604119	34.357722
977.390303	60528.952631	34.362740
978.194508	60617.875853	34.367757
979.500314	60707.524765	34.372775
980.354814	60790.952679	34.377792
981.211891	60880.469921	34.382810
982.252040	60957.368436	34.387828
983.247928	61044.142636	34.392845
984.539243	61138.637862	34.397863
985.609641	61226.382197	34.402880
986.524788	61309.580821	34.407898
987.700668	61392.966787	34.412916
988.937674	61474.260848	34.417933
989.629796	61564.869866	34.422951
990.589516	61653.177441	34.427968
991.472658	61734.306206	34.432986
992.263070	61823.273918	34.438004
993.547003	61914.931000	34.443021
994.461126	61998.955038	34.448039
995.874530	62082.375775	34.453056
996.588229	62176.990731	34.458074
997.638838	62259.063535	34.463092
998.424512	62343.292431	34.468109
999.656965	62428.641773	34.473127
1000.598452	62517.208498	34.478144
1001.690157	62603.574352	34.483162
1002.641756	62688.360839	34.488180
1003.717283	62780.306967	34.493197
1004.582061	62861.113107	34.498215
1005.795003	62953.576452	34.503232
1006.963889	63043.400872	34.508250
1007.769204	63121.273466	34.513268
1008.813549	63187.897427	34.518285
1009.817369	63285.877025	34.523303
1011.283450	63359.253471	34.528320
1012.194548	63446.467175	34.533338
1013.341832	63520.786630	34.538356
1014.312977	63599.445076	34.543373
1015.369987	63684.895830	34.548391
1016.412919	63755.725113	34.553408
1017.300621	63835.315320	34.558426
1018.480784	63909.637114	34.563444
1019.437508	63992.116500	34.568461
1020.175661	64069.553076	34.573479
1021.128623	64144.012430	34.578496
1022.223995	64217.652023	34.583514
1023.256551	64286.395256	34.588532
1024.135014	64353.402820	34.593549
1025.162048	64428.022353	34.598567
1026.400748	64491.700816	34.603584
1026.658430	64568.340491	34.608602
1027.754053	64656.669079	34.613620
1028.685135	64730.437192	34.618637
1029.479077	64818.699624	34.623655
1030.322601	64900.743883	34.628672
1031.454503	64991.771306	34.633690
1032.411346	65077.597016	34.638708
1033.741765	65162.395875	34.643725
1034.451400	65254.180443	34.648743
1035.561557	65345.085923	34.653760
1036.414959	65442.008525	34.658778
1037.666842	65537.387618	34.663796
1038.728492	65630.669573	34.668813
1039.116274	65729.432576	34.673831
1040.596650	65829.550731	34.678848
1041.675523	65928.624170	34.683866
1042.664255	66022.533116	34.688884
1043.757972	66118.743231	34.693901
1045.077547	66219.331290	34.698919
1046.003727	66314.738972	34.703936
1047.088296	66421.069179	34.708954
1048.112077	66511.080638	34.713972
1049.413465	66613.946080	34.718989
1050.521913	66725.731515	34.724007
1051.289504	66817.158091	34.729024
1052.700411	66912.865678	34.734042
1053.373384	67011.538347	34.739060
1054.398903	67107.218358	34.744077
1055.462299	67205.406434	34.749095
1056.755685	67304.920174	34.754112
1057.784655	67410.161502	34.759130
1059.202246	67512.480509	34.764148
1060.394060	67606.800372	34.769165
1061.181002	67705.432541	34.774183
1061.853587	67804.076661	34.779200
1063.289958	67904.349143	34.784218
1064.593953	67999.608979	34.789236
1065.775583	68098.364484	34.794253
1067.067982	68188.314455	34.799271
1068.094576	68278.097404	34.804288
1069.304467	68385.226615	34.809306
1070.171366	68480.531336	34.814324
1071.745754	68563.872296	34.819341
1072.367699	68656.645260	34.824359
1073.812366	68750.853744	34.829376
1074.722064	68843.613987	34.834394
1075.989018	68935.280181	34.839412
1077.042344	69027.898290	34.844429
1077.930562	69118.250378	34.849447
1079.174562	69214.790502	34.854464
1080.227086	69305.155510	34.859482
1081.098232	69394.225816	34.864500
1082.125602	69482.170178	34.869517
1082.912286	69565.928968	34.874535
1084.224145	69659.123074	34.879552
1085.643634	69760.621181	34.884570
1086.420210	69857.274866	34.889588
1087.512240	69937.890590	34.894605
1088.933880	70044.645235	34.899623
1089.669894	70138.564438	34.904640
1091.021672	70235.895682	34.909658
1092.166628	70327.459242	34.914676
1093.436986	70407.351941	34.919693
1094.118260	70485.817338	34.924711
1095.549880	70567.952274	34.929728
1096.570829	70643.376072	34.934746
1097.297405	70717.744330	34.939764
1098.519802	70801.951802	34.944781
1099.713775	70872.105896	34.949799
1100.589803	70956.773371	34.954816
1101.659093	71044.539125	34.959834
1102.763857	71120.609757	34.964852
1103.911992	71207.679799	34.969869
1105.042142	71297.437959	34.974887
1106.189605	71385.445917	34.979904
1107.665960	71472.984727	34.984922
1108.481981	71561.412455	34.989940
1109.568201	71638.323399	34.994957
1110.438347	71724.463444	34.999975
1111.519787	71818.739876	35.004992
1112.671293	71912.575050	35.010010
1113.622607	72016.738948	35.015028
1114.973415	72099.904568	35.020045
1115.958531	72192.272252	35.025063
1116.848381	72295.281637	35.030080
1117.897079	72400.622370	35.035098
1118.772057	72489.715257	35.040116
1120.618319	72597.465055	35.045133
1121.209322	72704.005903	35.050151
1122.729852	72786.019851	35.055168
1123.889722	72885.746795	35.060186
1124.823348	72995.122999	35.065204
1126.430050	73088.650423	35.070221
1127.259988	73192.647952	35.075239
1128.512755	73286.978782	35.080256
1129.882602	73396.275676	35.085274
1130.821386	73489.339098	35.090292
1131.959912	73589.034020	35.095309
1132.919614	73691.746555	35.100327
1134.081712	73797.518387	35.105344
1135.280734	73891.302449	35.110362
1136.121805	73990.842775	35.115380
1137.420539	74091.097144	35.120397
1138.544497	74199.675831	35.125415
1139.807319	74317.289829	35.130432
1141.178791	74413.113375	35.135450
1142.070444	74533.940423	35.140468
1143.304279	74626.100270	35.145485
1144.448126	74739.086049	35.150503
1145.192014	74847.954859	35.155520
1146.540060	74951.346098	35.160538
1148.083516	75057.962545	35.165556
1149.278435	75154.500389	35.170573
1150.505122	75248.500198	35.175591
1151.514143	75345.321168	35.180608
1153.029048	75451.588964	35.185626
1154.364653	75555.313811	35.190644
1155.853558	75644.853107	35.195661
1156.875921	75739.266629	35.200679
1157.811328	75833.719427	35.205696
1159.060615	75919.826305	35.210714
1160.265550	76029.337067	35.215732
1161.706835	76115.148493	35.220749
1162.494528	76205.749477	35.225767
1163.724648	76302.564591	35.230784
1164.901740	76388.228227	35.235802
1166.171462	76493.246401	35.240820
1167.392911	76582.792662	35.245837
1168.420384	76680.514914	35.250855
1169.734727	76763.384019	35.255872
1171.058645	76854.371922	35.260890
1171.781581	76948.684506	35.265908
1172.943766	77012.348443	35.270925
1173.978535	77096.402435	35.275943
1175.114428	77181.961006	35.280960
1176.203886	77258.748213	35.285978
1177.328029	77344.473815	35.290996
1178.698094	77428.489005	35.296013
1179.701291	77518.642567	35.301031
1180.712868	77606.324828	35.306048
1182.211216	77698.998433	35.311066
1183.269829	77784.342957	35.316084
1184.566170	77868.801758	35.321101
1185.689752	77956.176234	35.326119
1186.796066	78048.684363	35.331136
1188.250611	78139.504069	35.336154
1189.258095	78233.295128	35.341172
1190.794303	78316.564929	35.346189
1191.661442	78418.093676	35.351207
1193.137598	78506.428184	35.356224
1194.351472	78595.880864	35.361242
1195.579418	78684.026763	35.366260
1196.891786	78775.960326	35.371277
1197.818242	78876.581997	35.376295
1199.331868	78973.134126	35.381312
1200.013433	79058.680979	35.386330
1201.137857	79160.121498	35.391348
1202.999915	79248.613338	35.396365
1204.291637	79345.594239	35.401383
1205.020159	79442.828343	35.406400
1206.682100	79542.678508	35.411418
1207.744498	79644.510578	35.416436
1209.013698	79729.055333	35.421453
1209.816301	79831.752249	35.426471
1210.974112	79929.262916	35.431488
1212.516691	80025.649475	35.436506
1213.389899	80127.348227	35.441524
1214.868259	80228.901938	35.446541
1215.894573	80335.493178	35.451559
1216.759809	80437.156297	35.456576
1218.404877	80543.689475	35.461594
1219.510296	80640.514007	35.466612
1220.853866	80747.373888	35.471629
1221.982258	80847.172883	35.476647
1223.119709	80954.395230	35.481664
1224.313870	81052.917697	35.486682
1225.549039	81162.900206	35.491700
1227.154573	81267.301137	35.496717
1228.372418	81371.725137	35.501735
1229.398403	81482.577851	35.506752
1230.779406	81580.908210	35.511770
1232.154117	81687.082613	35.516788
1233.638057	81776.021754	35.521805
1234.988256	81879.768077	35.526823
1235.972493	81975.095765	35.531840
1237.318096	82080.275265	35.536858
1238.574818	82185.823835	35.541876
1239.730611	82280.783602	35.546893
1241.478097	82376.284576	35.551911
1242.589324	82469.972254	35.556928
1243.735715	82562.146963	35.561946
1244.913372	82662.337448	35.566964
1246.409546	82759.019391	35.571981
1247.353962	82846.690617	35.576999
1248.998381	82948.101433	35.582016
1250.578363	83036.041196	35.587034
1251.520147	83124.258524	35.592052
1252.694895	83204.393789	35.597069
1254.240387	83298.624409	35.602087
1255.093100	83373.742283	35.607104
1256.282219	83450.277502	35.612122
1257.069459	83534.757076	35.617140
1258.374119	83614.784461	35.622157
1259.785654	83703.082093	35.627175
1260.766312	83797.592843	35.632192
1262.240695	83877.505700	35.637210
1263.135610	83967.823677	35.642228
1264.491985	84062.213129	35.647245
1265.927964	84153.207254	35.652263
1266.924092	84244.967434	35.657280
1268.156880	84333.409030	35.662298
1269.338158	84441.359936	35.667316
1270.094335	84536.136338	35.672333
1271.722832	84628.647724	35.677351
1272.966727	84735.183417	35.682368
1274.502503	84839.202894	35.687386
1275.566329	84948.428551	35.692404
1276.824439	85048.652808	35.697421
1278.104791	85151.585633	35.702439
1279.477374	85256.607867	35.707456
1280.865910	85369.991245	35.712474
1281.876748	85487.881944	35.717492
1283.158004	85579.981884	35.722509
1284.374999	85692.417655	35.727527
1286.007994	85806.461419	35.732544
1287.442704	85913.719216	35.737562
1288.604188	86029.459661	35.742580
1289.900266	86135.282708	35.747597
1291.568713	86242.568489	35.752615
1292.496926	86345.332575	35.757632
1294.527436	86449.191680	35.762650
1295.443058	86552.059841	35.767668
1296.970120	86657.405102	35.772685
1298.253679	86765.868207	35.777703
1299.796309	86863.925252	35.782720
1301.297842	86971.480613	35.787738
1302.497237	87064.801930	35.792756
1303.669729	87171.256348	35.797773
1305.088187	87274.910058	35.802791
1306.588315	87368.476731	35.807808
1307.842591	87475.895232	35.812826
1309.375326	87566.618788	35.817844
1310.519974	87673.434215	35.822861
1312.392933	87759.885133	35.827879
1313.074260	87860.982369	35.832896
1314.609263	87957.637593	35.837914
1315.975957	88058.488821	35.842932
1317.471767	88155.657740	35.847949
1318.859670	88249.624965	35.852967
1319.874974	88345.120869	35.857984
1321.413365	88442.030607	35.863002
1322.470399	88544.997656	35.868020
1323.958903	88639.558675	35.873037
1325.010180	88749.738285	35.878055
1326.201583	88850.670344	35.883072
1327.998723	88947.921426	35.888090
1328.873920	89050.132955	35.893108
1330.211142	89159.040022	35.898125
1331.499533	89246.144412	35.903143
1332.086458	89367.348709	35.908160
1334.276885	89462.562872	35.913178
1335.251730	89569.867953	35.918196
1336.368268	89682.119236	35.923213
1337.886173	89789.948426	35.928231
1339.041249	89903.943452	35.933248
1340.604907	90000.828964	35.938266
1341.771333	90106.876642	35.943284
1342.863202	90216.586387	35.948301
1344.515149	90301.469744	35.953319
1345.224859	90401.443199	35.958336
1346.960820	90491.510187	35.963354
1347.971864	90597.545898	35.968372
1349.389441	90696.661772	35.973389
1350.838601	90797.572727	35.978407
1352.279884	90904.733523	35.983424
1353.319544	91008.142687	35.988442
1354.614809	91112.969711	35.993460
1355.840513	91227.047414	35.998477
1357.190071	91332.424361	36.003495
1358.454401	91440.286486	36.008512
1360.110960	91559.494422	36.013530
1361.752491	91662.025805	36.018548
1363.017329	91770.662157	36.023565
1364.518834	91871.860014	36.028583
1365.823753	91993.025853	36.033600
1367.210935	92098.627713	36.038618
1368.937317	92206.496281	36.043636
1370.200074	92323.715586	36.048653
1371.968151	92430.513758	36.053671
1373.276257	92541.072628	36.058688
1374.828268	92648.792611	36.063706
1376.130854	92762.635896	36.068724
1377.394637	92866.637362	36.073741
1378.986202	92964.592677	36.078759
1380.931639	93073.621456	36.083776
1381.971464	93174.401579	36.088794
1383.653272	93266.880845	36.093812
1385.000214	93389.123012	36.098829
1386.255550	93488.476181	36.103847
1387.318572	93592.283380	36.108864
1388.930988	93698.058305	36.113882
1390.055406	93802.946666	36.118900
1391.259355	93921.131919	36.123917
1392.514651	94040.564440	36.128935
1394.164709	94146.487115	36.133952
1395.428999	94269.620306	36.138970
1396.888981	94381.594339	36.143988
1397.986619	94495.095847	36.149005
1399.614008	94613.534351	36.154023
1400.547624	94734.655040	36.159040
1401.818418	94863.049926	36.164058
1403.707327	94984.237544	36.169076
1404.748417	95112.175061	36.174093
1406.185615	95235.208960	36.179111
1407.483324	95364.412948	36.184128
1408.595799	95497.728093	36.189146
1410.293828	95617.972010	36.194164
1411.521731	95744.792747	36.199181
1413.101896	95870.418018	36.204199
1414.545949	96017.107381	36.209216
1416.005159	96137.834338	36.214234
1417.862269	96271.784112	36.219252
1419.002265	96404.743871	36.224269
1420.571311	96523.274803	36.229287
1422.110498	96653.042085	36.234304
1423.590719	96776.899259	36.239322
1425.015034	96888.723060	36.244340
1426.703845	97020.750191	36.249357
1428.116040	97126.542726	36.254375
1429.501277	97256.818293	36.259392
1430.765975	97368.326506	36.264410
1433.010784	97494.627491	36.269428
1434.388858	97604.648295	36.274445
1436.154499	97711.376243	36.279463
1437.357632	97827.421307	36.284480
1439.066197	97921.013051	36.289498
1440.359559	98010.828966	36.294516
1441.770174	98106.977914	36.299533
1442.828707	98190.036265	36.304551
1444.293547	98285.188462	36.309568
1445.576974	98375.881672	36.314586
1447.106003	98466.574729	36.319604
1448.461804	98573.686642	36.324621
1450.057790	98665.650170	36.329639
1451.386092	98773.223432	36.334656
1452.491916	98870.956324	36.339674
1454.395915	98978.503552	36.344692
1455.577436	99099.006332	36.349709
1457.192073	99193.630691	36.354727
1458.227995	99297.815913	36.359744
1459.851715	99403.773052	36.364762
1461.292507	99523.007127	36.369780
1462.788788	99640.445428	36.374797
1464.200501	99747.704632	36.379815
1465.720975	99862.718541	36.384832
1467.026158	99978.615958	36.389850
1468.839319	100103.498836	36.394868
1470.015454	100222.814949	36.399885
1471.698490	100333.355196	36.404903
1472.927230	100458.394302	36.409920
1474.087176	100583.279844	36.414938
1475.894784	100712.463738	36.419956
1477.051957	100840.330014	36.424973
1478.941860	100953.134705	36.429991
1480.218631	101082.707424	36.435008
1481.602662	101226.514090	36.440026
1483.503815	101339.432458	36.445044
1484.885234	101477.243855	36.450061
1486.310747	101599.670174	36.455079
1487.624397	101724.028885	36.460096
1489.678143	101850.731833	36.465114
1491.095508	101973.059392	36.470132
1492.723922	102099.614338	36.475149
1494.199848	102218.370992	36.480167
1496.054319	102342.571322	36.485184
1497.314034	102470.947722	36.490202
1499.260793	102583.064473	36.495220
1500.271576	102700.703870	36.500237
1502.108873	102817.770565	36.505255
1503.647863	102935.315444	36.510272
1505.182449	103065.159902	36.515290
1506.878367	103177.381321	36.520308
1508.304787	103300.904189	36.525325
1509.856440	103418.347364	36.530343
1511.911061	103529.017708	36.535360
1512.742184	103651.684124	36.540378
1514.437563	103772.909773	36.545396
1515.797832	103888.457333	36.550413
1516.884976	104011.262505	36.555431
1518.298257	104123.074893	36.560448
1519.625492	104256.215007	36.565466
1521.463773	104384.660383	36.570484
1522.918964	104517.578637	36.575501
1524.958475	104642.265762	36.580519
1526.546532	104761.685946	36.585536
1527.802310	104879.256631	36.590554
1529.716724	105002.912271	36.595572
1531.164747	105131.218705	36.600589
1532.801080	105239.982146	36.605607
1534.246825	105356.421629	36.610624
1535.851273	105475.271186	36.615642
1537.561812	105586.496679	36.620660
1539.183574	105701.971497	36.625677
1540.449274	105804.188566	36.630695
1542.180181	105892.955829	36.635712
1543.223636	105993.356985	36.640730
1545.084151	106093.364279	36.645748
1546.352880	106192.196486	36.650765
1547.533945	106298.232292	36.655783
1549.189395	106397.625891	36.660800
1550.470726	106509.441464	36.665818
1552.073543	106624.009406	36.670836
1553.599532	106737.981105	36.675853
1555.098299	106847.481312	36.680871
1556.919530	106959.530862	36.685888
1558.306435	107087.385064	36.690906
1559.686449	107206.504028	36.695924
1561.096149	107323.475766	36.700941
1562.690218	107439.239761	36.705959
1564.484407	107568.236651	36.710976
1565.874752	107692.782946	36.715994
1567.501544	107823.785160	36.721012
1568.847301	107944.801449	36.726029
1570.798943	108077.985581	36.731047
1572.176195	108210.600724	36.736064
1573.636362	108344.699731	36.741082
1575.178168	108467.234219	36.746100
1576.504024	108597.817267	36.751117
1578.237129	108732.204755	36.756135
1580.108805	108870.337331	36.761152
1581.804717	109008.092170	36.766170
1583.401884	109148.323140	36.771188
1584.737445	109276.941639	36.776205
1586.319930	109410.175963	36.781223
1588.035046	109544.303086	36.786240
1589.828023	109690.909611	36.791258
1591.515465	109820.629030	36.796276
1592.806291	109949.535984	36.801293
1594.544538	110091.257728	36.806311
1596.370832	110224.228714	36.811328
1598.069741	110371.867316	36.816346
1599.957735	110489.865431	36.821364
1601.286185	110632.059291	36.826381
1603.195380	110769.267702	36.831399
1604.873056	110894.465234	36.836416
1606.212743	111023.786954	36.841434
1607.915208	111154.941959	36.846452
1609.603506	111291.920642	36.851469
1611.130069	111430.751361	36.856487
1613.029388	111569.689147	36.861504
1614.644213	111701.975894	36.866522
1616.116269	111827.652757	36.871540
1618.169881	111958.945992	36.876557
1619.621359	112099.820197	36.881575
1621.484531	112217.574281	36.886592
1622.644275	112354.994857	36.891610
1624.253502	112480.424258	36.896628
1625.848774	112611.246273	36.901645
1627.709485	112746.174358	36.906663
1629.291339	112875.274627	36.911680
1630.763707	113021.348961	36.916698
1632.779789	113145.626307	36.921716
1634.361749	113280.663427	36.926733
1635.736482	113408.783407	36.931751
1637.657320	113537.224217	36.936768
1639.268511	113666.766607	36.941786
1640.929422	113795.743636	36.946804
1642.793061	113916.420213	36.951821
1644.328421	114045.963137	36.956839
1646.148896	114163.717553	36.961856
1647.960513	114294.017143	36.966874
1649.464427	114393.748685	36.971892
1651.149688	114499.337025	36.976909
1652.680834	114599.280476	36.981927
1654.828604	114708.614629	36.986944
1656.175491	114814.662692	36.991962
1657.662941	114918.824641	36.996980
1659.444686	115024.957453	37.001997
1660.877618	115128.938282	37.007015
1662.431152	115223.273949	37.012032
1663.805735	115349.472893	37.017050
1665.682224	115456.137501	37.022068
1667.291543	115569.921543	37.027085
1668.667451	115688.333855	37.032103
1670.363229	115805.288623	37.037120
1671.950320	115932.382188	37.042138
1673.466848	116047.995958	37.047156
1675.405940	116180.527250	37.052173
1676.923831	116307.341204	37.057191
1678.584740	116439.536445	37.062208
1680.224295	116575.439137	37.067226
1681.884414	116703.196139	37.072244
1684.047388	116826.093095	37.077261
1685.298155	116959.115386	37.082279
1687.311706	117091.257743	37.087296
1688.879328	117234.137530	37.092314
1690.700097	117359.030427	37.097332
1692.474178	117490.602834	37.102349
1693.922877	117632.031398	37.107367
1695.751775	117765.042166	37.112384
1697.377510	117895.903524	37.117402
1699.130003	118039.543848	37.122420
1701.014845	118163.972750	37.127437
1702.624578	118307.839379	37.132455
1704.509755	118440.336341	37.137472
1706.245243	118571.271643	37.142490
1707.741802	118704.781671	37.147508
1709.614418	118845.146346	37.152525
1711.144675	118991.108246	37.157543
1713.006162	119123.433707	37.162560
1715.036873	119265.170485	37.167578
1716.344400	119407.363447	37.172596
1718.049284	119534.653661	37.177613
1719.919552	119682.505741	37.182631
1721.747147	119806.441566	37.187648
1723.552832	119944.740437	37.192666
1725.070652	120086.294126	37.197684
1727.467515	120231.554299	37.202701
1729.216733	120367.516812	37.207719
1731.137197	120502.793382	37.212736
1733.291089	120628.405942	37.217754
1734.812133	120759.318832	37.222772
1736.836838	120881.400602	37.227789
1738.617602	121008.214444	37.232807
1740.249958	121116.975499	37.237824
1742.103444	121235.469891	37.242842
1743.641522	121368.881157	37.247860
1745.873438	121493.989575	37.252877
1747.519414	121607.722515	37.257895
1749.102061	121718.877873	37.262912
1750.994342	121837.152365	37.267930
1752.928059	121963.678976	37.272948
1754.841077	122077.853538	37.277965
1756.324437	122200.303224	37.282983
1758.147787	122305.612589	37.288000
1759.826353	122426.370617	37.293018
1761.752748	122538.210264	37.298036
1763.453254	122640.304902	37.303053
1764.992602	122769.762784	37.308071
1766.821340	122869.656000	37.313088
1768.334041	122964.829063	37.318106
1770.432078	123060.633848	37.323124
1771.818657	123148.684967	37.328141
1773.551002	123249.735952	37.333159
1775.105583	123356.688597	37.338176
1776.853977	123460.401651	37.343194
1778.240886	123570.438424	37.348212
1780.545255	123678.061129	37.353229
1781.835073	123794.913425	37.358247
1783.799193	123904.594384	37.363264
1785.424257	124024.312691	37.368282
1786.969322	124144.399086	37.373300
1788.982492	124242.846031	37.378317
1790.387468	124381.121708	37.383335
1791.932061	124501.361479	37.388352
1794.042841	124619.876471	37.393370
1795.605741	124753.016121	37.398388
1797.660200	124886.193464	37.403405
1799.443755	125028.433706	37.408423
1800.824051	125156.338380	37.413440
1802.981085	125289.259953	37.418458
1804.730753	125419.530782	37.423476
1806.956376	125544.652902	37.428493
1808.875738	125687.051810	37.433511
1810.533757	125806.338887	37.438528
1812.880377	125935.173160	37.443546
1814.781694	126070.382851	37.448564
1816.615455	126199.285524	37.453581
1818.505141	126319.641598	37.458599
1820.363061	126445.420299	37.463616
1822.328124	126564.357051	37.468634
1824.388637	126685.956160	37.473652
1826.107968	126812.176339	37.478669
1827.804059	126944.985117	37.483687
1829.762933	127062.554074	37.488704
1831.866972	127181.432797	37.493722
1833.490348	127318.301342	37.498740
1835.614583	127432.445315	37.503757
1837.395765	127547.975444	37.508775
1839.426269	127679.554334	37.513792
1841.177419	127802.270863	37.518810
1843.078171	127925.243466	37.523828
1844.939098	128034.165047	37.528845
1846.569111	128151.890047	37.533863
1848.627065	128281.690303	37.538880
1850.637211	128411.676068	37.543898
1852.495115	128535.456481	37.548916
1854.054759	128649.958572	37.553933
1855.989633	128776.962982	37.558951
1857.806258	128892.262902	37.563968
1859.718203	129020.058266	37.568986
1861.469974	129150.556188	37.574004
1863.872751	129271.512957	37.579021
1865.748965	129384.952487	37.584039
1867.673524	129510.235178	37.589056
1869.501479	129632.589773	37.594074
1870.958911	129759.938291	37.599092
1872.967618	129871.531332	37.604109
1874.778855	129995.297947	37.609127
1876.542371	130118.184228	37.614144
1878.366774	130228.703189	37.619162
1879.747755	130371.925541	37.624180
1881.901711	130494.409230	37.629197
1883.568502	130627.703675	37.634215
1885.200288	130752.908946	37.639232
1887.081723	130875.385613	37.644250
1889.079418	131009.314626	37.649268
1890.769528	131123.866397	37.654285
1892.566784	131241.180451	37.659303
1894.280555	131341.454726	37.664320
1896.204663	131461.223759	37.669338
1898.026955	131581.516592	37.674356
1900.271536	131699.358249	37.679373
1901.958886	131821.347740	37.684391
1903.393058	131944.455715	37.689408
1905.752427	132067.241626	37.694426
1907.012724	132195.224552	37.699444
1909.071800	132323.108240	37.704461
1911.148862	132451.522412	37.709479
1912.674952	132590.605569	37.714496
1914.567833	132723.680744	37.719514
1916.334802	132855.963940	37.724532
1918.160299	133008.400945	37.729549
1919.955938	133156.338594	37.734567
1921.480789	133307.580165	37.739584
1923.577467	133448.238997	37.744602
1925.514584	133604.175436	37.749620
1927.848194	133759.009879	37.754637
1929.952496	133912.332672	37.759655
1931.768240	134070.624535	37.764672
1933.953661	134211.132316	37.769690
1935.689360	134371.556865	37.774708
1937.366711	134522.804082	37.779725
1939.523173	134682.275656	37.784743
1941.435406	134841.392641	37.789760
1943.967873	135006.110685	37.794778
1946.040758	135158.338682	37.799796
1947.326841	135310.791822	37.804813
1949.917937	135464.335609	37.809831
1951.786621	135617.827991	37.814848
1953.979775	135771.079777	37.819866
1955.722377	135923.247819	37.824884
1957.869215	136075.429256	37.829901
1960.170133	136232.980237	37.834919
1962.041140	136395.040460	37.839936
1964.608976	136537.284900	37.844954
1966.305779	136683.967943	37.849972
1968.340723	136828.288979	37.854989
1970.860451	136975.719794	37.860007
1972.976917	137119.483321	37.865024
1975.417341	137253.679078	37.870042
1977.264934	137398.576888	37.875060
1979.383289	137530.006646	37.880077
1981.782339	137655.910714	37.885095
1983.795845	137787.827145	37.890112
1986.238035	137910.057691	37.895130
1987.961979	138029.735990	37.900148
1989.984692	138146.829793	37.905165
1992.043302	138279.019745	37.910183
1993.755564	138409.132285	37.915200
1996.198666	138525.425220	37.920218
1997.834137	138656.324575	37.925236
1999.590809	138776.748400	37.930253
2001.689119	138891.395672	37.935271
2003.618388	139024.534369	37.940288
2006.035709	139143.980118	37.945306
2007.860757	139273.709379	37.950324
2009.524908	139389.123775	37.955341
2011.863025	139524.661890	37.960359
2013.529577	139642.284700	37.965376
2015.747377	139768.387782	37.970394
2017.681245	139895.195543	37.975412
2019.729877	140019.219094	37.980429
2021.812703	140137.437917	37.985447
2023.558062	140259.174436	37.990464
2025.681570	140362.120367	37.995482
2027.521698	140461.163989	38.000500
2029.401891	140553.944923	38.005517
2031.059147	140661.774310	38.010535
2033.227073	140775.932983	38.015552
2034.894804	140881.984489	38.020570
2036.899502	141004.735675	38.025588
2038.653130	141118.871147	38.030605
2040.831693	141238.841763	38.035623
2042.713340	141368.910513	38.040640
2044.853655	141496.832406	38.045658
2046.494972	141622.015263	38.050676
2048.575368	141745.619487	38.055693
2050.288944	141887.061885	38.060711
2052.169985	142032.412797	38.065728
2054.063210	142180.363961	38.070746
2055.761360	142326.683522	38.075764
2058.061926	142486.222567	38.080781
2059.912587	142629.054408	38.085799
2062.014343	142799.692533	38.090816
2064.114208	142942.879729	38.095834
2066.084208	143105.175797	38.100852
2068.174505	143277.137288	38.105869
2070.352250	143432.370762	38.110887
2072.292716	143602.592679	38.115904
2074.387251	143766.204052	38.120922
2076.777567	143923.030341	38.125940
2078.426153	144102.818475	38.130957
2080.955716	144261.020138	38.135975
2083.138244	144440.840169	38.140992
2085.026507	144603.623497	38.146010
2087.227614	144774.176677	38.151028
2089.420583	144948.018947	38.156045
2091.626501	145110.779591	38.161063
2093.635482	145290.350569	38.166080
2095.726237	145463.690218	38.171098
2098.049145	145633.300698	38.176116
2100.201809	145793.266874	38.181133
2102.558082	145957.072845	38.186151
2104.884640	146138.653268	38.191168
2106.965471	146299.914189	38.196186
2109.280322	146472.854109	38.201204
2111.791043	146628.641824	38.206221
2113.936075	146791.988494	38.211239
2116.201449	146967.577850	38.216256
2118.370527	147117.683456	38.221274
2120.126122	147280.521425	38.226292
2122.237143	147437.326048	38.231309
2124.703682	147595.750955	38.236327
2126.459607	147753.690962	38.241344
2128.878318	147908.798801	38.246362
2131.132570	148081.753540	38.251380
2132.964511	148238.121891	38.256397
2135.106695	148397.171137	38.261415
2137.263037	148561.841615	38.266432
2139.926531	148716.938915	38.271450
2142.112925	148882.443421	38.276468
2144.367513	149047.188882	38.281485
2146.518746	149205.756796	38.286503
2148.261458	149356.595517	38.291520
2150.826283	149516.356262	38.296538
2152.839362	149658.458719	38.301556
2154.902544	149822.944566	38.306573
2157.300287	149971.968945	38.311591
2159.296527	150132.226657	38.316608
2161.489393	150285.193490	38.321626
2163.795415	150438.752333	38.326644
2165.611472	150581.395773	38.331661
2167.915497	150710.355877	38.336679
2169.926737	150845.163007	38.341696
2171.910602	150967.827075	38.346714
2174.072061	151103.030224	38.351732
2176.067505	151237.383824	38.356749
2178.195386	151362.463407	38.361767
2180.237611	151513.730919	38.366784
2182.125031	151656.492927	38.371802
2184.611477	151792.154671	38.376820
2186.620211	151938.376498	38.381837
2188.695202	152077.302129	38.386855
2190.945819	152231.864762	38.391872
2193.262108	152385.528982	38.396890
2195.049392	152541.891322	38.401908
2197.426991	152687.778140	38.406925
2199.507422	152847.332411	38.411943
2201.453530	153003.468086	38.416960
2203.573077	153163.981876	38.421978
2205.760283	153337.014549	38.426996
2207.973093	153504.090224	38.432013
2210.524535	153672.941365	38.437031
2212.521530	153846.614666	38.442048
2214.681866	154010.107593	38.447066
2217.509731	154182.699866	38.452084
2219.226525	154350.046034	38.457101
2221.581385	154522.827579	38.462119
2223.489093	154698.789711	38.467136
2225.781869	154873.244978	38.472154
2227.935737	155060.378833	38.477172
2230.291760	155239.725353	38.482189
2232.606995	155414.623040	38.487207
2234.877378	155605.371045	38.492224
2237.307223	155782.435363	38.497242
2239.521905	155963.824656	38.502260
2241.874562	156151.032463	38.507277
2244.631650	156331.132040	38.512295
2246.434504	156515.494543	38.517312
2248.927223	156701.857025	38.522330
2251.267113	156876.552082	38.527348
2253.850768	157055.068750	38.532365
2256.028388	157227.454370	38.537383
2258.213390	157415.555642	38.542400
2260.514638	157588.608485	38.547418
2262.665764	157773.250452	38.552436
2265.040858	157956.106031	38.557453
2267.430669	158132.193386	38.562471
2269.651976	158313.144450	38.567488
2271.911831	158490.967015	38.572506
2274.275304	158664.229013	38.577524
2276.417263	158853.572913	38.582541
2278.953053	159034.515000	38.587559
2281.462942	159210.789803	38.592576
2283.698798	159393.379474	38.597594
2286.011702	159560.202679	38.602612
2288.037734	159755.521609	38.607629
2290.356615	159926.140788	38.612647
2292.942513	160096.782139	38.617664
2295.036828	160277.428749	38.622682
2297.801668	160454.720923	38.627700
2300.135808	160635.915041	38.632717
2302.434804	160791.774725	38.637735
2304.706037	160971.900522	38.642752
2306.683306	161145.077495	38.647770
2309.295717	161312.671027	38.652788
2311.503200	161495.195075	38.657805
2314.131510	161653.722248	38.662823
2316.346883	161824.045351	38.667840
2318.649195	161983.195649	38.672858
2321.281985	162127.719770	38.677876
2323.193487	162264.866467	38.682893
2325.517620	162400.526959	38.687911
2328.249035	162548.908854	38.692928
2330.145584	162682.161113	38.697946
2332.165372	162826.452595	38.702964
2334.831897	162974.299684	38.707981
2337.262482	163113.042845	38.712999
2339.073218	163265.848977	38.718016
2341.215866	163423.821650	38.723034
2343.580905	163574.624670	38.728052
2345.590469	163747.448055	38.733069
2347.752689	163915.994774	38.738087
2349.871276	164085.729499	38.743104
2352.122711	164261.233382	38.748122
2354.523126	164438.961669	38.753140
2356.400975	164619.654249	38.758157
2358.417944	164806.622963	38.763175
2360.952199	164998.691416	38.768192
2362.900812	165194.572094	38.773210
2365.347035	165395.771508	38.778228
2367.346469	165604.062597	38.783245
2369.376296	165809.899125	38.788263
2371.836208	166030.854148	38.793280
2374.214790	166249.219787	38.798298
2376.853960	166464.142635	38.803316
2378.957555	166692.291058	38.808333
2381.712826	166902.219975	38.813351
2384.171054	167130.314354	38.818368
2386.217802	167353.103069	38.823386
2389.049178	167567.631033	38.828404
2391.221582	167795.886550	38.833421
2393.858757	168025.669915	38.838439
2396.384525	168251.230642	38.843456
2398.432603	168475.952617	38.848474
2401.413561	168701.418160	38.853492
2403.644573	168931.928214	38.858509
2406.105638	169152.257966	38.863527
2408.779503	169376.910243	38.868544
2410.745702	169603.781656	38.873562
2413.940268	169833.128050	38.878580
2416.567177	170053.561546	38.883597
2418.933158	170270.303488	38.888615
2421.513012	170494.465987	38.893632
2423.588066	170717.946278	38.898650
2426.332138	170944.484258	38.903668
2428.972706	171165.756941	38.908685
2431.550600	171394.087224	38.913703
2434.206338	171607.778383	38.918720
2436.412254	171827.394117	38.923738
2439.309168	172034.039652	38.928756
2441.462660	172250.693546	38.933773
2444.228515	172465.461878	38.938791
2446.719101	172682.534071	38.943808
2448.945458	172907.660522	38.948826
2451.753382	173106.374014	38.953844
2454.062286	173320.568598	38.958861
2456.876251	173534.316520	38.963879
2459.401507	173738.053410	38.968896
2461.845527	173948.520762	38.973914
2464.794161	174149.906845	38.978932
2467.185157	174349.044226	38.983949
2469.506994	174546.415189	38.988967
2471.923128	174747.606714	38.993984
2474.308138	174953.654296	38.999002
2476.779016	175149.924078	39.004020
2479.198373	175353.541952	39.009037
2481.739679	175537.027260	39.014055
2483.945296	175718.203612	39.019072
2486.082854	175907.581402	39.024090
2488.747771	176086.007379	39.029108
2490.504131	176275.318655	39.034125
2492.938049	176458.835505	39.039143
2495.161031	176649.039713	39.044160
2497.226236	176853.643653	39.049178
2499.638442	177050.269971	39.054196
2501.905116	177269.014882	39.059213
2503.956478	177484.898771	39.064231
2506.484958	177705.076877	39.069248
2508.784170	177922.446925	39.074266
2511.220977	178141.523011	39.079284
2513.653882	178382.391150	39.084301
2515.788272	178628.335329	39.089319
2518.145508	178860.454525	39.094336
2520.557912	179112.883717	39.099354
2522.935212	179365.928661	39.104372
2525.709077	179626.887161	39.109389
2528.061838	179870.794215	39.114407
2530.647386	180128.913686	39.119424
2532.679867	180396.187446	39.124442
2535.182819	180664.632899	39.129460
2537.500128	180943.089602	39.134477
2539.770638	181253.378301	39.139495
2542.835339	181573.957074	39.144512
2545.361306	181856.701570	39.149530
2548.020815	182132.771657	39.154548
2550.609821	182421.044822	39.159565
2553.142346	182703.054260	39.164583
2555.878408	182997.757379	39.169600
2558.492224	183287.984954	39.174618
2561.001573	183563.422272	39.179636
2563.787599	183855.935880	39.184653
2566.219468	184144.518126	39.189671
2568.745012	184433.035759	39.194688
2571.749024	184726.940173	39.199706
2574.407422	185021.585278	39.204724
2577.145301	185298.413984	39.209741
2579.913484	185597.437637	39.214759
2582.965388	185872.517023	39.219776
2585.850373	186157.554404	39.224794
2588.825607	186421.547704	39.229812
2592.005590	186692.418306	39.234829
2594.377018	186961.460302	39.239847
2597.423974	187225.952377	39.244864
2600.246650	187493.172552	39.249882
2603.073918	187746.930796	39.254900
2605.915872	188002.744717	39.259917
2608.542245	188264.765125	39.264935
2611.637086	188512.285716	39.269952
2613.740463	188763.924333	39.274970
2616.642284	188999.589000	39.279988
2619.826453	189238.537410	39.285005
2622.480356	189496.365376	39.290023
2625.273996	189729.127460	39.295040
2627.429825	189971.083068	39.300058
2630.413154	190200.895404	39.305076
2633.357954	190446.005237	39.310093
2635.372879	190687.704964	39.315111
2637.933170	190915.375029	39.320128
2640.104348	191166.093855	39.325146
2642.920971	191416.077236	39.330164
2645.490382	191660.537064	39.335181
2647.622739	191916.750050	39.340199
2650.186231	192153.998000	39.345216
2652.576912	192421.576555	39.350234
2655.593169	192655.935162	39.355252
2657.873081	192884.694181	39.360269
2660.136191	193127.071132	39.365287
2662.800242	193354.297662	39.370304
2665.080692	193576.910807	39.375322
2667.070715	193817.629908	39.380340
2669.845657	194070.673226	39.385357
2672.071901	194318.214598	39.390375
2674.484892	194576.522734	39.395392
2677.009888	194852.213707	39.400410
2679.306092	195122.911570	39.405428
2681.325531	195386.972704	39.410445
2683.641877	195678.472225	39.415463
2686.146480	195974.261161	39.420480
2688.341634	196277.363954	39.425498
2691.037294	196585.850451	39.430516
2693.499481	196896.076039	39.435533
2695.881702	197216.424666	39.440551
2698.898405	197545.235142	39.445568
2701.393256	197874.839219	39.450586
2704.147635	198214.360954	39.455604
2706.836695	198548.660872	39.460621
2709.280487	198893.440083	39.465639
2712.205136	199233.343869	39.470656
2714.776862	199585.547383	39.475674
2717.388156	199940.590522	39.480692
2720.325624	200289.944140	39.485709
2722.901377	200651.725961	39.490727
2725.870529	201004.098995	39.495744
2728.838587	201371.815948	39.500762
2731.578524	201730.500710	39.505780
2734.264765	202082.488360	39.510797
2737.674393	202451.865892	39.515815
2740.461319	202804.829916	39.520832
2743.362264	203159.910605	39.525850
2746.289158	203507.621147	39.530868
2749.735406	203859.061505	39.535885
2752.469997	204215.922981	39.540903
2755.853441	204554.596848	39.545920
2758.656445	204905.530026	39.550938
2761.978497	205238.194181	39.555956
2765.116193	205570.989320	39.560973
2767.549539	205916.266384	39.565991
2770.984199	206239.286804	39.571008
2773.526209	206568.721863	39.576026
2776.725218	206896.911524	39.581044
2779.723105	207215.149702	39.586061
2782.703718	207547.972425	39.591079
2785.799268	207864.570426	39.596096
2788.548575	208185.109692	39.601114
2791.326662	208500.462622	39.606132
2794.443253	208798.768230	39.611149
2797.066409	209114.679640	39.616167
2800.083432	209413.535016	39.621184
2803.287303	209716.248226	39.626202
2806.130049	210017.748091	39.631220
2809.241586	210323.982096	39.636237
2811.982958	210620.036745	39.641255
2815.536273	210905.092039	39.646272
2818.283435	211180.137701	39.651290
2821.155395	211467.205369	39.656308
2824.293240	211744.807018	39.661325
2827.321307	212024.966443	39.666343
2830.391869	212290.842661	39.671360
2833.141740	212558.242664	39.676378
2835.832569	212825.220258	39.681396
2839.072701	213089.622604	39.686413
2841.933225	213353.042973	39.691431
2844.482062	213604.293116	39.696448
2847.474714	213835.532126	39.701466
2850.228231	214062.947317	39.706484
2853.148439	214290.133350	39.711501
2855.321306	214518.427144	39.716519
2858.114837	214754.956439	39.721536
2861.034025	214985.267704	39.726554
2863.258066	215229.964744	39.731572
2866.116250	215464.706080	39.736589
2868.147753	215705.673746	39.741607
2870.973491	215967.069035	39.746624
2873.894188	216229.592800	39.751642
2876.361366	216488.834331	39.756660
2879.311411	216760.829445	39.761677
2881.409112	217043.195775	39.766695
2884.647771	217322.386168	39.771712
2887.173231	217603.974598	39.776730
2889.998135	217905.915700	39.781748
2892.092052	218195.193096	39.786765
2894.822298	218501.696617	39.791783
2897.826927	218817.658463	39.796800
2900.249468	219127.487519	39.801818
2903.381839	219454.124764	39.806836
2906.263337	219775.009277	39.811853
2908.801148	220103.060796	39.816871
2911.569680	220435.471260	39.821888
2914.639904	220775.100223	39.826906
2916.872293	221121.109726	39.831924
2920.149612	221461.875124	39.836941
2922.899969	221816.110971	39.841959
2926.324461	222168.869675	39.846976
2929.304088	222523.527130	39.851994
2932.015874	222877.515236	39.857012
2935.416962	223230.277835	39.862029
2938.577565	223590.470685	39.867047
2941.577676	223937.656386	39.872064
2944.823966	224292.399443	39.877082
2947.546060	224650.603245	39.882100
2951.008460	224989.409584	39.887117
2953.983256	225351.816365	39.892135
2956.704689	225700.239703	39.897152
2960.190111	226053.497344	39.902170
2963.068250	226400.981580	39.907188
2966.064092	226753.045508	39.912205
2969.342558	227108.748779	39.917223
2972.401495	227459.557928	39.922240
2975.695328	227812.642042	39.927258
2978.293113	228166.393809	39.932276
2981.590794	228508.477188	39.937293
2984.658486	228857.836586	39.942311
2987.381554	229209.028046	39.947328
2990.489663	229564.096792	39.952346
2993.474327	229921.852126	39.957364
2996.463950	230275.008406	39.962381
2999.478942	230632.479239	39.967399
3002.336617	230980.092351	39.972416
3005.621020	231329.416834	39.977434
3008.816973	231692.574711	39.982452
3012.153212	232040.518883	39.987469
3014.431832	232393.912251	39.992487
3017.636024	232738.243886	39.997504
3020.927330	233090.817939	40.002522
3023.582986	233445.142400	40.007540
3026.509519	233797.061686	40.012557
3029.406182	234154.701240	40.017575
3032.509331	234509.590012	40.022592
3035.519575	234873.231924	40.027610
3038.223619	235228.893810	40.032628
3041.365664	235564.722775	40.037645
3044.273570	235909.885826	40.042663
3047.124985	236238.951449	40.047680
3050.138027	236569.490318	40.052698
3052.628372	236902.600173	40.057716
3055.730969	237235.715580	40.062733
3058.278955	237574.988843	40.067751
3061.266262	237921.534688	40.072768
3063.928340	238273.643580	40.077786
3066.437599	238652.170219	40.082804
3069.526223	239008.403141	40.087821
3071.928181	239390.451296	40.092839
3075.088695	239768.900053	40.097856
3077.890927	240160.512463	40.102874
3080.254704	240569.365525	40.107892
3083.691990	240973.223459	40.112909
3086.621668	241386.000465	40.117927
3089.235387	241797.073375	40.122944
3092.406971	242213.266007	40.127962
3095.529985	242641.150945	40.132980
3099.213177	243071.335388	40.137997
3102.289211	243498.235352	40.143015
3105.246688	243929.268313	40.148032
3108.516949	244366.830864	40.153050
3111.266515	244814.050813	40.158068
3114.384253	245253.057918	40.163085
3117.371543	245692.033661	40.168103
3120.477154	246155.478135	40.173120
3123.928838	246607.817235	40.178138
3126.789950	247072.440838	40.183156
3129.927387	247534.505220	40.188173
3132.872585	247990.019250	40.193191
3136.032160	248458.631626	40.198208
3139.544309	248931.124970	40.203226
3142.134591	249420.983876	40.208244
3145.573864	249901.487610	40.213261
3148.767020	250374.052165	40.218279
3152.011421	250860.349812	40.223296
3155.613966	251330.713750	40.228314
3158.551572	251824.854771	40.233332
3161.731630	252297.822000	40.238349
3165.327473	252786.293962	40.243367
3168.166549	253267.338354	40.248384
3171.909313	253743.362749	40.253402
3175.082078	254236.569847	40.258420
3178.235875	254716.290054	40.263437
3181.600280	255194.045160	40.268455
3185.109921	255686.203736	40.273472
3188.776136	256168.353387	40.278490
3191.777143	256643.188192	40.283508
3195.384558	257121.787367	40.288525
3198.735019	257595.674971	40.293543
3201.846453	258063.908402	40.298560
3205.460704	258527.438529	40.303578
3208.304876	259007.267423	40.308596
3211.584550	259488.651930	40.313613
3214.678973	259945.882365	40.318631
3217.680855	260416.231983	40.323648
3220.969713	260897.888654	40.328666
3224.235755	261376.371855	40.333684
3227.058503	261856.776522	40.338701
3230.917455	262344.484616	40.343719
3233.531125	262812.624320	40.348736
3236.622178	263306.950475	40.353754
3240.273924	263785.794621	40.358772
3242.940230	264262.453935	40.363789
3246.374234	264751.614426	40.368807
3249.636631	265241.688387	40.373824
3252.992242	265708.784763	40.378842
3256.131788	266159.124122	40.383860
3259.401699	266608.272712	40.388877
3262.227716	267061.273044	40.393895
3265.339754	267506.632395	40.398912
3268.393984	267955.884670	40.403930
3271.313862	268430.198490	40.408948
3274.001334	268893.294895	40.413965
3277.500379	269365.227588	40.418983
3280.127802	269849.866077	40.424000
3283.314427	270337.919437	40.429018
3286.019930	270830.794723	40.434036
3289.534194	271333.852184	40.439053
3292.844764	271842.526023	40.444071
3295.431998	272362.510122	40.449088
3298.916752	272877.728506	40.454106
3301.890210	273401.277685	40.459124
3304.955912	273946.624918	40.464141
3307.888587	274489.881477	40.469159
3311.156065	275030.288517	40.474176
3314.264547	275589.967115	40.479194
3317.602981	276154.685072	40.484212
3320.932238	276724.758977	40.489229
3324.163981	277295.986813	40.494247
3327.215800	277874.146153	40.499264
3330.625050	278454.073734	40.504282
3334.300994	279040.761079	40.509300
3337.537119	279636.857926	40.514317
3341.031229	280229.176673	40.519335
3343.982171	280818.223536	40.524352
3347.578308	281426.058066	40.529370
3350.569029	282030.122259	40.534388
3353.944733	282643.846976	40.539405
3358.007072	283259.109600	40.544423
3361.105986	283879.570722	40.549440
3364.428217	284481.733738	40.554458
3367.924385	285104.077002	40.559476
3371.518935	285726.424573	40.564493
3376.057210	286341.432781	40.569511
3379.318082	286963.668650	40.574528
3383.181145	287553.709093	40.579546
3386.291474	288170.472385	40.584564
3390.205283	288785.149026	40.589581
3394.115765	289379.532704	40.594599
3397.141999	289989.131292	40.599616
3401.030706	290584.497266	40.604634
3404.716548	291188.014212	40.609652
3407.978108	291788.824048	40.614669
3411.323375	292370.927860	40.619687
3414.327740	292977.580471	40.624704
3418.017644	293567.337325	40.629722
3421.609528	294176.678750	40.634740
3425.137015	294775.944529	40.639757
3428.496959	295372.970765	40.644775
3431.867341	295982.454943	40.649792
3435.663870	296576.404637	40.654810
3439.142159	297185.376755	40.659828
3442.262408	297786.655062	40.664845
3445.794816	298376.793592	40.669863
3449.175484	298975.022673	40.674880
3452.724466	299587.334012	40.679898
3456.695450	300180.253374	40.684916
3460.131388	300765.354780	40.689933
3464.125589	301352.342652	40.694951
3467.725972	301942.812709	40.699968
3471.281289	302512.492579	40.704986
3475.006367	303097.776983	40.710004
3478.461774	303662.916026	40.715021
3482.154082	304213.950822	40.720026
3485.485054	304738.730714	40.725031
3489.095021	305216.737237	40.730036
3492.238223	305642.107801	40.735040
3495.272727	306014.940424	40.740045
3498.187408	306317.144148	40.745050
3500.479949	306602.087566	40.750055
3503.760879	306821.600244	40.755060
3506.112617	306983.006512	40.760064
3508.321157	307099.442496	40.765069
3510.652805	307180.129956	40.770074
3512.489643	307211.500098	40.775079
3514.498673	307201.006795	40.780084
3515.980310	307158.989502	40.785088
3517.765411	307073.841167	40.790093
3518.820656	306953.484795	40.795098
3520.203919	306813.659877	40.800103
3521.640543	306638.147733	40.805108
3522.016571	306431.270229	40.810112
3522.921480	306213.544471	40.815117
3523.908367	305968.651273	40.820122
3524.442918	305703.392249	40.825127
3525.806108	305415.250969	40.830132
3526.232047	305125.218658	40.835136
3526.824024	304807.368207	40.840141
3527.606901	304478.619054	40.845146
3527.948508	304124.894434	40.850151
3528.263142	303761.984255	40.855156
3528.392574	303399.456789	40.860160
3528.885620	303028.700477	40.865165
3529.332437	302644.307421	40.870170
3529.392183	302256.307204	40.875175
3529.508126	301854.119340	40.880180
3529.624387	301453.048220	40.885184
3529.608074	301050.569557	40.890189
3529.771792	300641.391509	40.895194
3529.593964	300244.531342	40.900199
3530.105548	299814.778818	40.905204
3530.061535	299387.909472	40.910208
3530.402786	298970.012040	40.915213
3530.186489	298538.734394	40.920218
3530.086136	298114.943732	40.925223
3529.808817	297682.956332	40.930228
3529.629947	297253.113707	40.935232
3529.530507	296823.993532	40.940237
3529.762478	296390.542173	40.945242
3529.228813	295967.083134	40.950247
3529.099249	295535.081769	40.955252
3529.319481	295111.956760	40.960256
3528.935689	294695.642945	40.965261
3529.349033	294266.830855	40.970266
3528.678995	293848.697642	40.975271
3528.643850	293419.007712	40.980276
3528.764889	293002.246691	40.985280
3528.025281	292578.591797	40.990285
3528.239261	292160.079493	40.995290
3527.761906	291761.680158	41.000295
3527.478008	291337.614455	41.005300
3527.649939	290936.562722	41.010304
3527.073838	290519.970096	41.015309
3526.862353	290109.783468	41.020314
3526.524065	289710.330964	41.025319
3526.489448	289311.159387	41.030324
3525.835469	288919.693573	41.035328
3525.645608	288525.887175	41.040333
3525.557916	288139.928494	41.045338
3525.151955	287764.480006	41.050343
3524.681178	287383.642616	41.055348
3525.106163	287006.939760	41.060352
3524.618317	286632.184922	41.065357
3524.683389	286246.700343	41.070362
3524.006866	285879.302481	41.075367
3524.101140	285512.571289	41.080372
3524.077405	285142.496127	41.085376
3523.327620	284784.854093	41.090381
3523.378416	284420.033143	41.095386
3523.242032	284061.324029	41.100391
3522.850542	283708.686560	41.105396
3522.878699	283361.964432	41.110400
3522.329909	283015.305326	41.115405
3522.296607	282667.876539	41.120410
3521.755277	282333.484010	41.125415
3521.315622	281994.771456	41.130420
3521.339057	281668.892643	41.135424
3521.143970	281345.185091	41.140429
3520.954067	281023.384730	41.145434
3520.556625	280701.080747	41.150439
3520.274123	280380.361326	41.155444
3520.190695	280058.667383	41.160448
3520.022895	279758.422320	41.165453
3519.869466	279446.971481	41.170458
3519.613713	279146.406735	41.175463
3519.235860	278833.155327	41.180468
3519.216125	278534.002471	41.185472
3518.823359	278239.184080	41.190477
3518.526225	277949.492590	41.195482
3518.693845	277664.030165	41.200487
3518.299650	277379.087351	41.205492
3518.376119	277095.317483	41.210496
3517.959394	276805.462206	41.215501
3517.658941	276518.031920	41.220506
3517.351565	276242.695593	41.225511
3517.081106	275973.310409	41.230516
3516.745806	275700.344448	41.235520
3516.665217	275443.123644	41.240525
3516.735828	275176.330430	41.245530
3516.203202	274921.902996	41.250535
3516.006500	274660.191223	41.255540
3515.974241	274413.271473	41.260544
3515.618381	274160.392658	41.265549
3515.558873	273912.737294	41.270554
3515.270880	273670.540254	41.275559
3514.921092	273423.056132	41.280564
3514.802903	273197.203088	41.285568
3514.660973	272968.857888	41.290573
3514.632312	272737.540782	41.295578
3514.482311	272513.065843	41.300583
3514.367838	272277.152284	41.305588
3514.144537	272052.865841	41.310592
3513.509450	271837.682287	41.315597
3513.601323	271608.151131	41.320602
3513.397789	271403.949673	41.325607
3513.468749	271190.818447	41.330612
3513.409075	270970.679488	41.335616
3513.102399	270767.613036	41.340621
3513.004396	270553.997448	41.345626
3512.832904	270351.469093	41.350631
3512.789803	270149.913257	41.355636
3512.415341	269950.038392	41.360640
3512.412935	269760.901156	41.365645
3512.730397	269549.229805	41.370650
3512.072593	269361.085407	41.375655
3512.075839	269162.397456	41.380660
3511.815302	268971.389227	41.385664
3511.487973	268792.104067	41.390669
3511.732101	268607.865763	41.395674
3511.347332	268422.477722	41.400679
3511.169490	268240.545427	41.405684
3510.844410	268063.779385	41.410688
3510.743898	267892.885395	41.415693
3510.804977	267717.051406	41.420698
3510.590458	267547.982522	41.425703
3510.214503	267383.547466	41.430708
3510.384665	267218.364699	41.435712
3510.158240	267056.452059	41.440717
3510.232046	266892.862542	41.445722
3510.189581	266727.737647	41.450727
3509.745147	266573.140886	41.455732
3509.701404	266409.696258	41.460736
3509.915850	266268.160750	41.465741
3509.871536	266110.241350	41.470746
3509.265071	265959.717704	41.475751
3509.214293	265805.083664	41.480756
3509.063775	265655.303122	41.485760
3508.957567	265516.846884	41.490765
3508.889874	265376.754740	41.495770
3508.920882	265228.625806	41.500775
3508.749094	265079.306087	41.505780
3508.815078	264955.031102	41.510784
3508.297762	264816.459933	41.515789
3508.698689	264675.427781	41.520794
3508.574547	264543.033492	41.525799
3508.580768	264404.150741	41.530804
3508.447217	264278.301889	41.535808
3507.978893	264139.060081	41.540813
3508.403476	264007.699751	41.545818
3508.139542	263883.118557	41.550823
3507.959173	263752.718274	41.555828
3507.859775	263616.422891	41.560832
3507.413481	263502.386559	41.565837
3507.663855	263378.411904	41.570842
3507.675072	263262.852313	41.575847
3507.252860	263133.966019	41.580852
3507.422859	263022.582992	41.585856
3507.285544	262900.756488	41.590861
3507.456655	262783.643509	41.595866
3507.138140	262668.287617	41.600871
3507.189373	262555.980485	41.605876
3507.083527	262445.734970	41.610880
3507.017431	262337.520306	41.615885
3506.825619	262209.844662	41.620890
3506.584789	262115.331663	41.625895
3506.504717	262007.016999	41.630900
3506.698852	261895.578117	41.635904
3506.467632	261791.488567	41.640909
3506.232157	261687.144936	41.645914
3506.056127	261584.014229	41.650919
3506.115220	261489.301017	41.655924
3506.001006	261387.026270	41.660928
3506.059288	261296.565666	41.665933
3505.856329	261198.200760	41.670938
3506.122754	261100.857379	41.675943
3505.772536	261019.984327	41.680948
3505.776870	260920.822821	41.685952
3505.635954	260824.612419	41.690957
3505.792434	260736.758917	41.695962
3505.474101	260651.729810	41.700967
3505.589265	260558.840541	41.705972
3505.400579	260470.506031	41.710976
3505.315018	260387.197431	41.715981
3505.496621	260296.436637	41.720986
3505.448916	260215.439326	41.725991
3505.037343	260126.655560	41.730996
3505.384539	260055.375041	41.736000
3504.522151	259975.778192	41.741005
3504.887729	259889.648458	41.746010
3505.090718	259827.124930	41.751015
3504.514122	259735.259902	41.756020
3504.489084	259660.650452	41.761024
3504.758094	259587.064528	41.766029
3505.019013	259516.510200	41.771034
3504.656648	259438.897506	41.776039
3504.464068	259362.735210	41.781044
3504.932284	259302.767408	41.786048
3504.314405	259235.609873	41.791053
3504.561036	259152.426720	41.796058
3504.185288	259084.925661	41.801063
3504.154003	259007.031736	41.806068
3504.156767	258939.063971	41.811072
3504.251352	258882.948727	41.816077
3504.362513	258807.706279	41.821082
3504.256248	258743.015033	41.826087
3504.139829	258685.481151	41.831092
3504.291533	258607.176377	41.836096
3503.699729	258552.747154	41.841101
3503.989644	258480.303232	41.846106
3503.753767	258424.112113	41.851111
3503.615512	258379.568944	41.856116
3503.873843	258315.940956	41.861120
3503.727451	258252.605399	41.866125
3504.106298	258196.037948	41.871130
3503.699435	258133.787142	41.876135
3503.608157	258069.806234	41.881140
3503.719215	258019.315927	41.886144
3503.942100	257957.323097	41.891149
3503.991155	257887.946899	41.896154
3503.689074	257842.308658	41.901159
3503.611217	257780.413689	41.906164
3503.881511	257722.666105	41.911168
3503.413678	257672.775474	41.916173
3503.498500	257620.404642	41.921178
3503.647665	257569.093291	41.926183
3503.251009	257503.962944	41.931188
3503.477210	257448.488580	41.936192
3503.455099	257400.463556	41.941197
3503.562963	257337.953621	41.946202
3503.534561	257279.717748	41.951207
3503.468724	257230.604466	41.956212
3503.452454	257174.403915	41.961216
3503.146611	257131.032463	41.966221
3503.287043	257083.160168	41.971226
3503.262265	257022.937275	41.976231
3502.782838	256980.458749	41.981236
3503.007011	256924.653417	41.986240
3502.917075	256889.550005	41.991245
3503.281545	256837.186061	41.996250
3502.985196	256792.361454	42.001255
3502.759483	256750.912754	42.006260
3503.350449	256695.279171	42.011264
3502.863477	256656.494277	42.016269
3502.825533	256604.193152	42.021274
3502.822459	256559.297147	42.026279
3502.943106	256524.695498	42.031284
3502.965506	256481.450771	42.036288
3502.831034	256441.617530	42.041293
3502.796860	256381.777796	42.046298
3502.713376	256353.931037	42.051303
3502.713329	256318.762485	42.056308
3502.721405	256273.482648	42.061312
3502.699264	256230.779588	42.066317
3502.653216	256187.672794	42.071322
3502.799745	256141.632751	42.076327
3502.599057	256100.103534	42.081332
3502.755817	256057.270583	42.086336
3502.326991	256034.570957	42.091341
3502.594632	255990.014424	42.096346
3502.790751	255944.730541	42.101351
3502.284748	255905.439077	42.106356
3502.602681	255864.618153	42.111360
3502.726189	255833.937652	42.116365
3502.405684	255791.841350	42.121370
3502.341147	255756.784594	42.126375
3502.274211	255719.512653	42.131380
3502.825106	255676.516096	42.136384
3502.165053	255650.771152	42.141389
3502.406863	255611.413621	42.146394
3502.247099	255572.195258	42.151399
3502.098630	255539.316190	42.156404
3502.128212	255510.636659	42.161408
3502.081672	255477.283250	42.166413
3502.358153	255452.741558	42.171418
3502.038750	255419.838251	42.176423
3502.134063	255389.442185	42.181428
3502.278547	255342.230740	42.186432
3501.798188	255323.537241	42.191437
3502.059360	255285.780957	42.196442
3502.103968	255262.115866	42.201447
3502.008235	255229.839666	42.206452
3502.621426	255192.868707	42.211456
3502.362749	255168.257832	42.216461
3502.561916	255123.889979	42.221466
3502.282788	255094.596501	42.226471
3502.243434	255060.019486	42.231476
3502.460863	255024.714727	42.236480
3502.056388	254997.147064	42.241485
3502.077045	254945.116252	42.246490
3501.809276	254915.897359	42.251495
3502.001978	254893.227701	42.256500
3501.833878	254854.901753	42.261504
3501.863905	254843.742812	42.266509
3501.765591	254819.259600	42.271514
3501.956339	254793.483344	42.276519
3501.665916	254763.987831	42.281524
3501.956049	254739.316545	42.286528
3501.524173	254713.077356	42.291533
3501.718522	254694.125488	42.296538
3501.858352	254667.618646	42.301543
3501.858262	254642.177793	42.306548
3502.040259	254612.863053	42.311552
3502.084758	254584.155529	42.316557
3502.132561	254549.717556	42.321562
3501.829719	254525.775595	42.326567
3501.866817	254496.967345	42.331572
3502.247794	254458.046116	42.336576
3502.067258	254434.950874	42.341581
3501.892688	254405.182509	42.346586
3501.664319	254377.816386	42.351591
3501.712767	254351.731232	42.356596
3502.054707	254327.764831	42.361600
3501.879181	254301.663751	42.366605
3502.191793	254280.248565	42.371610
3502.071946	254247.110047	42.376615
3501.475732	254215.548514	42.381620
3501.648883	254194.282450	42.386624
3501.680678	254175.203128	42.391629
3501.852811	254149.837125	42.396634
3501.802425	254124.174843	42.401639
3501.743915	254108.623994	42.406644
3501.767388	254084.274411	42.411648
3501.660741	254069.444144	42.416653
3501.938530	254021.243681	42.421658
3502.007030	254004.144978	42.426663
3501.513906	253978.551887	42.431668
3501.634617	253948.202465	42.436672
3501.721985	253931.941196	42.441677
3501.912089	253902.192110	42.446682
3501.520530	253882.109343	42.451687
3501.295798	253852.730699	42.456692
3501.738350	253828.290087	42.461696
3501.599203	253811.835020	42.466701
3501.633924	253784.274852	42.471706
3501.551455	253770.179301	42.476711
3501.398390	253742.113686	42.481716
3501.530519	253715.225871	42.486720
3501.431407	253717.762533	42.491725
3501.298968	253685.262514	42.496730
3501.382017	253679.392220	42.501735
3501.280167	253652.337241	42.506740
3501.581231	253623.334744	42.511744
3501.336315	253611.531093	42.516749
3501.218522	253576.915040	42.521754
3501.310290	253573.768296	42.526759
3501.176489	253560.648477	42.531764
3501.470229	253535.772683	42.536768
3501.483711	253532.281646	42.541773
3501.349455	253499.909201	42.546778
3501.630206	253484.356178	42.551783
3501.338294	253457.840206	42.556788
3501.291683	253431.642412	42.561792
3501.236443	253429.715575	42.566797
3501.446750	253410.404509	42.571802
3501.546075	253393.020781	42.576807
3501.069576	253380.642120	42.581812
3501.629858	253346.913196	42.586816
3501.377835	253344.940724	42.591821
3501.532964	253322.022021	42.596826
3501.544024	253302.334626	42.601831
3501.360428	253295.003477	42.606836
3501.273548	253255.543866	42.611840
3501.106537	253250.985978	42.616845
3501.035513	253240.301106	42.621850
3501.165694	253217.309887	42.626855
3501.214758	253203.142784	42.631860
3501.442795	253184.312780	42.636864
3501.392986	253160.127296	42.641869
3501.360408	253151.448267	42.646874
3501.605203	253128.031650	42.651879
3501.517364	253110.651684	42.656884
3501.178163	253094.558876	42.661888
3500.979727	253070.447547	42.666893
3501.046583	253058.391375	42.671898
3501.476765	253039.402417	42.676903
3501.186502	253033.259395	42.681908
3501.316618	253006.015229	42.686912
3501.330635	252995.317044	42.691917
3501.400248	252976.868314	42.696922
3501.495904	252968.576692	42.701927
3501.266514	252946.762178	42.706932
3501.140595	252917.877227	42.711936
3501.216076	252907.857025	42.716941
3500.967044	252885.001440	42.721946
3501.166966	252875.063647	42.726951
3501.232483	252861.301404	42.731956
3501.513365	252858.634412	42.736960
3501.081623	252840.900713	42.741965
3501.356262	252819.160179	42.746970
3501.539002	252812.026399	42.751975
3501.286135	252781.938869	42.756980
3501.305956	252767.521629	42.761984
3501.487205	252758.987414	42.766989
3501.447816	252716.591566	42.771994
3501.672574	252715.716012	42.776999
3501.505090	252697.202448	42.782004
3501.661825	252675.454860	42.787009
3501.244731	252647.710445	42.792013
3501.373409	252627.724436	42.797018
3501.605682	252616.202634	42.802023
3501.173004	252595.081983	42.807028
3501.422267	252587.275659	42.812033
3501.337651	252561.694850	42.817037
3501.072360	252540.675355	42.822042
3501.219528	252541.569132	42.827047
3500.779208	252531.349411	42.832052
3501.184505	252499.885592	42.837057
3501.129343	252502.186204	42.842061
3501.004881	252489.676029	42.847066
3501.308346	252465.511600	42.852071
3501.319335	252446.842769	42.857076
3501.148579	252439.254902	42.862081
3501.145768	252421.887028	42.867085
3501.318411	252406.019724	42.872090
3501.406578	252389.910958	42.877095
3501.355671	252381.947817	42.882100
3501.290326	252355.523559	42.887105
3501.249181	252349.952763	42.892109
3501.033204	252314.460424	42.897114
3501.276745	252304.948708	42.902119
3501.107086	252299.550803	42.907124
3501.277472	252273.293409	42.912129
3501.231458	252264.310828	42.917133
3501.145838	252257.397244	42.922138
3501.216507	252226.316751	42.927143
3501.172547	252215.856774	42.932148
3501.498640	252198.157318	42.937153
3501.541494	252180.629476	42.942157
3501.420987	252169.850395	42.947162
3501.618892	252140.277998	42.952167
3500.858078	252131.101559	42.957172
3501.283677	252107.249045	42.962177
3501.263900	252104.527178	42.967181
3501.024509	252079.046884	42.972186
3501.212577	252062.132994	42.977191
3501.403632	252056.780553	42.982196
3501.597321	252035.638297	42.987201
3500.946348	252027.692552	42.992205
3500.854116	252002.443906	42.997210
3501.171505	251990.755948	43.002215
3500.879381	251979.570749	43.007220
3501.289711	251969.600001	43.012225
3501.502284	251951.892798	43.017229
3501.242977	251931.177883	43.022234
3501.398293	251917.528848	43.027239
3501.279560	251899.695167	43.032244
3501.517603	251881.016235	43.037249
3501.214425	251875.282653	43.042253
3501.372765	251860.843669	43.047258
3501.469154	251850.208924	43.052263
3501.166541	251833.702791	43.057268
3501.415558	251807.101954	43.062273
3501.438371	251809.492253	43.067277
3501.264004	251776.692766	43.072282
3501.550842	251759.483266	43.077287
3501.596983	251756.420017	43.082292
3501.572168	251725.201548	43.087297
3501.332422	251704.814613	43.092301
3501.114689	251683.354627	43.097306
3501.372948	251668.950937	43.102311
3500.872440	251659.886575	43.107316
3501.583108	251641.846795	43.112321
3501.164320	251629.764566	43.117325
3501.243836	251607.290357	43.122330
3501.203793	251581.982549	43.127335
3501.487605	251577.837999	43.132340
3501.745679	251558.544691	43.137345
3501.236357	251539.931626	43.142349
3501.500020	251521.732515	43.147354
3501.260325	251501.243678	43.152359
3501.413121	251490.880225	43.157364
3501.411781	251475.829497	43.162369
3501.565169	251452.885313	43.167373
3501.262356	251439.409726	43.172378
3501.005311	251413.295410	43.177383
3501.156015	251398.348238	43.182388
3501.455082	251392.622351	43.187393
3501.442949	251360.586884	43.192397
3501.266367	251353.254543	43.197402
3501.344174	251348.225385	43.202407
3501.294401	251325.720415	43.207412
3501.811958	251302.923009	43.212417
3501.233496	251291.094920	43.217421
3501.053857	251268.839446	43.222426
3501.383501	251262.446634	43.227431
3500.963320	251235.619251	43.232436
3501.444125	251230.221482	43.237441
3501.154231	251212.821951	43.242445
3501.134829	251193.571979	43.247450
3501.342432	251177.036941	43.252455
3501.006449	251176.427314	43.257460
3501.102378	251150.054033	43.262465
3501.132168	251146.382123	43.267469
3501.181955	251132.520314	43.272474
3501.343405	251126.764998	43.277479
3501.178892	251098.802543	43.282484
3501.259178	251086.183842	43.287489
3501.000581	251073.694522	43.292493
3501.038865	251057.415145	43.297498
3501.080757	251042.688687	43.302503
3500.922024	251050.506373	43.307508
3501.463613	251021.720438	43.312513
3501.055216	251007.268110	43.317517
3501.265001	250993.381275	43.322522
3501.348584	250986.441181	43.327527
3501.029339	250965.506305	43.332532
3501.354856	250950.710029	43.337537
3501.149252	250934.799840	43.342541
3500.787662	250910.891942	43.347546
3501.367384	250896.132320	43.352551
3500.980256	250899.630869	43.357556
3501.295279	250889.165612	43.362561
3500.787022	250863.166879	43.367565
3500.872839	250846.498045	43.372570
3500.965311	250844.573549	43.377575
3500.914138	250841.525497	43.382580
3501.124203	250816.560467	43.387585
3500.874640	250803.534906	43.392589
3501.073018	250798.435947	43.397594
3501.161125	250791.215000	43.402599
3500.958595	250776.170192	43.407604
3500.883728	250748.626598	43.412609
3501.279023	250752.945105	43.417613
3501.116936	250737.664767	43.422618
3501.196906	250717.787993	43.427623
3500.932996	250707.158565	43.432628
3501.251387	250701.353230	43.437633
3500.847553	250686.543621	43.442637
3501.009621	250672.536883	43.447642
3501.347820	250656.923654	43.452647
3501.098889	250652.276627	43.457652
3501.086535	250630.325980	43.462657
3500.968794	250618.400344	43.467661
3500.762836	250611.963906	43.472666
3501.025645	250618.264090	43.477671
3500.846951	250592.366590	43.482676
3501.098080	250573.812790	43.487681
3500.959415	250576.559425	43.492685
3501.043946	250562.462931	43.497690
3501.038792	250533.125710	43.502695
3500.635618	250529.266804	43.507700
3501.441648	250510.728112	43.512705
3501.248264	250508.950171	43.517709
3501.188836	250496.989942	43.522714
3501.299127	250472.575265	43.527719
3501.085084	250476.174098	43.532724
3501.230015	250442.967873	43.537729
3501.163542	250436.331352	43.542733
3500.793557	250426.584368	43.547738
3501.130902	250423.195430	43.552743
3501.118585	250413.443462	43.557748
3501.194456	250395.630119	43.562753
3501.367939	250388.599542	43.567757
3501.302487	250355.375257	43.572762
3501.413244	250351.945340	43.577767
3501.079696	250338.576333	43.582772
3501.096558	250300.271222	43.587777
3500.784689	250302.280928	43.592781
3500.897649	250294.444864	43.597786
3501.145423	250281.723513	43.602791
3500.970265	250268.915479	43.607796
3500.958710	250259.392586	43.612801
3501.393237	250255.377241	43.617805
3501.096735	250240.678146	43.622810
3501.246830	250219.058586	43.627815
3500.807239	250217.904876	43.632820
3501.130921	250202.395740	43.637825
3501.113528	250180.878761	43.642829
3501.023423	250168.031955	43.647834
3501.324712	250163.120623	43.652839
3501.097943	250156.229013	43.657844
3501.212652	250135.251651	43.662849
3501.269610	250128.086478	43.667853
3501.364542	250119.489212	43.672858
3501.183612	250092.802501	43.677863
3500.835033	250085.828064	43.682868
3501.235072	250073.643167	43.687873
3501.328111	250059.188760	43.692877
3501.222941	250037.023340	43.697882
3501.136952	250030.848262	43.702887
3501.120664	250015.010252	43.707892
3501.384356	249999.383140	43.712897
3501.315221	249987.551726	43.717901
3501.123894	249970.263986	43.722906
3501.422950	249950.531134	43.727911
3501.160177	249950.775938	43.732916
3500.966787	249920.958691	43.737921
3501.444912	249907.768357	43.742925
3500.859907	249902.893712	43.747930
3501.098085	249881.311270	43.752935
3501.170979	249872.080757	43.757940
3501.073237	249854.345432	43.762945
3501.228660	249851.876273	43.767949
3501.517992	249835.812195	43.772954
3501.068676	249811.153835	43.777959
3501.143576	249813.688823	43.782964
3500.909070	249789.837292	43.787969
3500.828634	249760.282496	43.792973
3501.158211	249755.774204	43.797978
3501.256757	249741.700915	43.802983
3500.803911	249738.129895	43.807988
3501.023799	249704.911801	43.812993
3501.036256	249702.592326	43.817997
3500.976039	249698.348710	43.823002
3500.984044	249689.153799	43.828007
3500.845811	249680.516561	43.833012
3501.146267	249664.119654	43.838017
3501.290281	249672.195681	43.843021
3501.019092	249660.344899	43.848026
3501.293122	249642.449559	43.853031
3501.032739	249630.902691	43.858036
3501.095698	249609.984287	43.863041
3500.917383	249597.354964	43.868045
3500.567737	249590.762680	43.873050
3501.163295	249587.282421	43.878055
3501.206895	249577.903669	43.883060
3500.955897	249559.861199	43.888065
3501.112915	249534.038381	43.893069
3500.877371	249546.452241	43.898074
3501.031787	249535.477196	43.903079
3500.967968	249501.615802	43.908084
3501.010644	249501.099771	43.913089
3500.925794	249493.523799	43.918093
3500.683462	249496.719601	43.923098
3500.816428	249482.182499	43.928103
3500.555741	249465.109287	43.933108
3500.905194	249445.393964	43.938113
3501.062680	249438.798790	43.943117
3500.698738	249445.018735	43.948122
3500.997051	249440.795461	43.953127
3500.796403	249425.495562	43.958132
3500.930471	249397.358796	43.963137
3500.630996	249393.865659	43.968141
3500.864170	249398.948097	43.973146
3500.891060	249391.431053	43.978151
3500.371618	249393.065746	43.983156
3500.983036	249385.915726	43.988161
3501.161996	249361.795754	43.993165
3500.731733	249353.382425	43.998170
3501.117966	249347.770174	44.003175
3500.732256	249340.546838	44.008180
3501.135241	249329.481984	44.013185
3501.164755	249316.718280	44.018189
3500.550619	249304.360809	44.023194
3500.974694	249294.948025	44.028199
3500.693725	249302.657569	44.033204
3500.969338	249278.089532	44.038209
3501.081731	249259.990216	44.043213
3500.960699	249259.907254	44.048218
3501.183254	249245.025052	44.053223
3501.032903	249222.051635	44.058228
3500.990043	249205.886629	44.063233
3501.032318	249211.431861	44.068237
3500.605308	249203.527360	44.073242
3501.318928	249194.476779	44.078247
3500.965116	249175.176979	44.083252
3500.867759	249165.438232	44.088257
3501.052331	249160.774323	44.093261
3500.722966	249152.192407	44.098266
3501.130903	249143.495219	44.103271
3500.975205	249125.081262	44.108276
3501.076872	249109.148323	44.113281
3501.211612	249110.349670	44.118285
3500.873222	249099.655380	44.123290
3501.058181	249078.437696	44.128295
3501.063003	249069.472454	44.133300
3501.136202	249059.630635	44.138305
3501.047515	249040.442174	44.143309
3501.225054	249030.558573	44.148314
3500.954524	249027.035436	44.153319
3501.002362	249017.070243	44.158324
3501.044507	248997.453846	44.163329
3501.081447	248990.877502	44.168333
3500.969027	248986.718430	44.173338
3501.152842	248966.035724	44.178343
3500.948811	248964.514103	44.183348
3501.147477	248951.825795	44.188353
3501.108501	248938.410621	44.193357
3501.123291	248929.673019	44.198362
3500.928614	248914.703214	44.203367
3501.092022	248900.645182	44.208372
3500.929980	248896.672137	44.213377
3501.177464	248870.504000	44.218381
3500.825303	248857.545260	44.223386
3500.945427	248851.159643	44.228391
3501.134744	248858.923019	44.233396
3500.825876	248841.780874	44.238401
3500.852012	248827.005745	44.243405
3500.717086	248821.398553	44.248410
3501.106159	248803.969017	44.253415
3500.743556	248801.377093	44.258420
3500.990732	248788.095441	44.263425
3500.893356	248773.135879	44.268429
3500.798290	248771.087875	44.273434
3500.959174	248759.449619	44.278439
3500.880982	248756.966033	44.283444
3500.838693	248741.412108	44.288449
3500.906447	248720.543779	44.293453
3500.724916	248721.361630	44.298458
3500.946522	248713.635843	44.303463
3500.659485	248717.704537	44.308468
3500.852924	248702.317493	44.313473
3501.101630	248679.841896	44.318477
3500.902086	248676.358588	44.323482
3501.082252	248663.851423	44.328487
3501.362241	248656.829590	44.333492
3501.043653	248639.841748	44.338497
3501.322171	248630.502618	44.343501
3501.089918	248624.936103	44.348506
3501.063749	248595.550890	44.353511
3500.726317	248591.707128	44.358516
3501.254948	248581.819547	44.363521
3501.237676	248571.457030	44.368525
3501.245646	248554.443593	44.373530
3501.450869	248534.776181	44.378535
3501.019419	248526.108323	44.383540
3500.909088	248501.116634	44.388545
3501.175495	248493.205561	44.393549
3500.933913	248496.655938	44.398554
3501.324365	248479.098817	44.403559
3501.416183	248465.332082	44.408564
3501.392549	248435.258828	44.413569
3501.146617	248425.492332	44.418573
3500.283303	248414.447121	44.423578
3500.916059	248397.055849	44.428583
3501.064576	248405.767916	44.433588
3500.869598	248398.412852	44.438593
3501.069267	248385.469672	44.443597
3500.963135	248372.243225	44.448602
3501.054936	248362.016447	44.453607
3500.961803	248353.473960	44.458612
3500.914180	248340.696775	44.463617
3500.966633	248328.515160	44.468621
3501.052419	248317.168756	44.473626
3501.037855	248311.033383	44.478631
3501.208716	248296.974136	44.483636
3500.884730	248284.647632	44.488641
3500.871581	248273.927910	44.493645
3500.938878	248270.632082	44.498650
3501.010610	248254.958419	44.503655
3500.731158	248247.361881	44.508660
3500.881363	248241.302614	44.513665
3500.878098	248231.854713	44.518669
3500.724915	248236.462774	44.523674
3501.008676	248230.662768	44.528679
3500.656742	248214.622391	44.533684
3500.593805	248193.901768	44.538689
3500.560392	248193.906976	44.543693
3500.889001	248195.714705	44.548698
3500.984152	248183.169861	44.553703
3500.716898	248181.861857	44.558708
3500.621815	248172.835785	44.563713
3500.479709	248157.042740	44.568717
3500.498151	248148.890277	44.573722
3500.757360	248140.470966	44.578727
3500.880361	248140.604525	44.583732
3500.761005	248130.156072	44.588737
3500.680315	248123.903693	44.593741
3500.822054	248131.267062	44.598746
3500.857432	248118.171276	44.603751
3500.795152	248101.397985	44.608756
3500.852250	248087.814920	44.613761
3501.031402	248078.211155	44.618765
3500.868473	248089.162125	44.623770
3501.067590	248076.448216	44.628775
3500.812443	248058.813714	44.633780
3500.943067	248042.825216	44.638785
3500.843016	248039.351808	44.643789
3500.672372	248041.186657	44.648794
3501.406774	248023.881326	44.653799
3501.144076	248015.212528	44.658804
3501.000778	248008.817129	44.663809
3501.299422	247993.413575	44.668813
3500.620283	247983.078098	44.673818
3501.065397	247957.006263	44.678823
3500.859568	247956.452676	44.683828
3500.889918	247945.522394	44.688833
3500.858480	247945.960240	44.693837
3500.695922	247927.241619	44.698842
3501.137033	247912.681677	44.703847
3501.220630	247910.096382	44.708852
3500.876241	247896.499670	44.713857
3501.026835	247882.647298	44.718861
3501.455839	247861.620519	44.723866
3501.278987	247853.956988	44.728871
3500.892532	247842.964526	44.733876
3500.889604	247827.582639	44.738881
3500.607685	247823.169897	44.743885
3500.228747	247812.048921	44.748890
3500.882125	247808.635989	44.753895
3500.773455	247810.130075	44.758900
3500.805874	247806.457680	44.763905
3500.786250	247780.636749	44.768909
3500.674785	247776.324695	44.773914
3501.033202	247771.990114	44.778919
3500.779078	247765.459228	44.783924
3500.856186	247760.073527	44.788929
3500.954157	247759.421509	44.793933
3501.095203	247740.120586	44.798938
3500.844949	247727.604244	44.803943
3500.859301	247729.384706	44.808948
3501.011613	247724.369258	44.813953
3501.107185	247704.846234	44.818957
3500.774477	247697.690945	44.823962
3501.000585	247692.358349	44.828967
3500.835088	247682.146291	44.833972
3500.961024	247671.150113	44.838977
3501.082045	247651.572169	44.843981
3500.751792	247636.878126	44.848986
3501.085591	247633.566089	44.853991
3500.844843	247630.089203	44.858996
3500.727233	247616.151405	44.864001
3500.961852	247594.671102	44.869005
3500.809107	247588.761047	44.874010
3500.746849	247579.831683	44.879015
3500.891818	247579.859939	44.884020
3501.092731	247567.935204	44.889025
3501.034227	247548.869198	44.894029
3500.715490	247540.947694	44.899034
3500.980390	247539.556488	44.904039
3500.781748	247548.297405	44.909044
3500.817179	247533.342442	44.914049
3501.051005	247516.955750	44.919053
3501.103556	247518.602905	44.924058
3500.977674	247515.948484	44.929063
3500.776207	247495.274905	44.934068
3500.395872	247493.959107	44.939073
3500.791017	247470.518165	44.944077
3500.772507	247466.140636	44.949082
3500.678579	247452.173655	44.954087
3500.581535	247469.863247	44.959092
3500.743078	247464.795414	44.964097
3500.853748	247447.511140	44.969101
3500.822447	247455.563744	44.974106
3501.099469	247431.682850	44.979111
3500.437987	247420.224010	44.984116
3500.764536	247412.125214	44.989121
3500.771097	247404.942340	44.994125
3500.631052	247403.436169	44.999130
3501.212021	247394.941052	45.004135
3501.075592	247381.821137	45.009140
3500.595161	247364.170854	45.014145
3500.820205	247355.705912	45.019149
3501.023682	247362.321103	45.024154
3500.966800	247347.024012	45.029159
3501.086312	247331.342798	45.034164
3500.963798	247327.210733	45.039169
3501.204556	247320.627928	45.044173
3500.786624	247314.733856	45.049178
3501.416496	247285.576939	45.054183
3500.942043	247277.883508	45.059188
3501.153804	247268.809419	45.064193
3500.882246	247253.316676	45.069197
3500.746666	247242.004812	45.074202
3500.848531	247230.935969	45.079207
3500.647868	247223.556277	45.084212
3500.778403	247228.782162	45.089217
3501.230449	247218.651804	45.094221
3501.030513	247203.682677	45.099226
3501.070865	247190.280436	45.104231
3501.161703	247182.855169	45.109236
3500.953552	247173.795789	45.114241
3501.454647	247160.245111	45.119245
3501.015063	247143.301510	45.124250
3501.309531	247134.494627	45.129255
3500.984077	247118.093467	45.134260
3501.140171	247105.513553	45.139265
3500.882927	247094.704585	45.144269
3500.755196	247080.844730	45.149274
3500.948091	247058.657798	45.154279
3500.889190	247058.794328	45.159284
3501.036720	247051.945947	45.164289
3501.387880	247049.853627	45.169293
3500.884089	247032.461639	45.174298
3501.199797	247010.102695	45.179303
3501.043570	247010.279909	45.184308
3501.251613	247002.505233	45.189313
3501.423926	246973.266996	45.194317
3501.106714	246976.321745	45.199322
3501.515836	246959.118103	45.204327
3501.189492	246942.742535	45.209332
3500.679891	246934.341493	45.214337
3500.779673	246922.177852	45.219341
3500.770973	246915.710436	45.224346
3500.850058	246892.344301	45.229351
3501.013073	246893.974191	45.234356
3500.888770	246888.161537	45.239361
3501.183652	246877.648250	45.244365
3500.917840	246865.567229	45.249370
3500.867977	246844.997213	45.254375
3500.937202	246838.721352	45.259380
3501.095880	246833.246469	45.264385
3501.092408	246821.582847	45.269389
3500.912148	246811.092905	45.274394
3500.993203	246797.811610	45.279399
3500.880190	246791.335030	45.284404
3500.786625	246794.176544	45.289409
3500.836489	246774.023878	45.294413
3500.876688	246760.927240	45.299418
3501.012052	246754.742907	45.304423
3500.982463	246749.730403	45.309428
3500.754716	246738.662127	45.314433
3500.847989	246712.339511	45.319437
3500.781130	246705.601037	45.324442
3500.790735	246702.849020	45.329447
3500.919190	246699.085186	45.334452
3500.698329	246700.545885	45.339457
3500.982531	246685.093545	45.344461
3500.747840	246674.764910	45.349466
3500.822856	246664.795337	45.354471
3501.043870	246657.375165	45.359476
3501.041435	246650.652085	45.364481
3500.697688	246642.785388	45.369485
3500.917419	246623.904996	45.374490
3501.021983	246624.092373	45.379495
3500.729079	246625.869948	45.384500
3500.740051	246616.878153	45.389505
3501.300577	246613.326911	45.394509
3501.041279	246593.477236	45.399514
3500.917713	246581.806908	45.404519
3500.977029	246578.690570	45.409524
3500.885668	246554.332337	45.414529
3500.918628	246527.662578	45.419533
3500.522260	246531.239061	45.424538
3500.826551	246520.316802	45.429543
3501.000661	246531.317043	45.434548
3500.857744	246519.777074	45.439553
3501.131302	246490.548401	45.444557
3501.011500	246487.128987	45.449562
3500.853064	246486.466116	45.454567
3500.802638	246474.911684	45.459572
3500.866326	246465.682433	45.464577
3501.317080	246440.602739	45.469581
3500.927765	246448.482151	45.474586
3501.006803	246432.221433	45.479591
3501.295734	246426.598836	45.484596
3500.974657	246398.812898	45.489601
3501.321283	246399.650058	45.494605
3501.018279	246390.070650	45.499610
3500.996332	246374.156794	45.504615
3501.003461	246358.824148	45.509620
3500.887216	246344.784170	45.514625
3500.972076	246337.920093	45.519629
3500.753760	246323.768733	45.524634
3500.935619	246301.736242	45.529639
3500.911659	246295.984285	45.534644
3501.005672	246301.496050	45.539649
3500.972871	246294.141014	45.544653
3500.828101	246274.910091	45.549658
3500.697713	246268.996498	45.554663
3501.075036	246263.665689	45.559668
3500.841138	246254.381081	45.564673
3500.916957	246253.325038	45.569677
3500.480092	246237.959925	45.574682
3500.772609	246234.807124	45.579687
3501.332093	246219.311708	45.584692
3500.753823	246212.373026	45.589697
3501.041682	246210.647142	45.594701
3500.957129	246192.832985	45.599706
3500.804449	246180.657830	45.604711
3501.115263	246165.455964	45.609716
3500.727981	246168.394342	45.614721
3501.105607	246159.829089	45.619725
3500.797692	246144.291003	45.624730
3500.943366	246133.266181	45.629735
3501.016431	246128.950707	45.634740
3500.871423	246118.964568	45.639745
3500.814044	246104.660693	45.644749
3500.700550	246101.775107	45.649754
3500.850535	246087.387876	45.654759
3501.037444	246087.689719	45.659764
3500.505202	246074.606127	45.664769
3501.082491	246071.714414	45.669773
3500.754313	246065.144110	45.674778
3500.950485	246043.414964	45.679783
3501.285258	246037.275835	45.684788
3500.890589	246027.812610	45.689793
3500.760830	246032.035049	45.694797
3500.865653	246005.404918	45.699802
3501.003108	245993.286263	45.704807
3500.883950	245993.839698	45.709812
3500.739762	245993.607548	45.714817
3500.927011	245986.218097	45.719821
3500.968054	245974.063578	45.724826
3501.210192	245944.559590	45.729831
3500.998003	245883.088264	45.734836
3500.449047	245781.583393	45.739841
3500.410733	245629.215984	45.744845
3500.307159	245435.549963	45.749850
3500.098112	245195.981828	45.754855
3499.586903	244910.287491	45.759860
3499.504645	244583.700713	45.764865
3499.467363	244187.324327	45.769869
3498.724211	243759.782903	45.774874
3498.295243	243278.937901	45.779879
3498.140233	242753.352564	45.784884
3497.129375	242184.502126	45.789889
3496.947589	241558.191786	45.794893
3496.208572	240897.126380	45.799898
3495.744921	240187.626380	45.804903
3494.992124	239422.648582	45.809908
3493.772802	238618.596599	45.814913
3493.504780	237758.923230	45.819917
3492.379734	236865.406400	45.824922
3491.361914	235924.880758	45.829927
3490.764387	234931.821411	45.834932
3489.686653	233905.164968	45.839937
3488.657155	232802.219421	45.844941
3487.550730	231682.219392	45.849946
3486.326099	230508.521738	45.854951
3485.543312	229296.142130	45.859956
3483.678506	228042.466548	45.864961
3482.525456	226730.074218	45.869965
3481.506304	225390.077219	45.874970
3480.084758	223998.542631	45.879975
3478.802686	222563.001656	45.884980
3477.127466	221091.637514	45.889985
3475.580260	219563.255849	45.894989
3473.837609	218022.631809	45.899994
3472.426847	216419.535792	45.904999
3470.585200	214782.511740	45.910004
3468.888496	213121.225566	45.915009
3466.957803	211411.746641	45.920013
3465.204142	209670.796327	45.925018
3463.250382	207891.890138	45.930023
3461.414895	206085.091256	45.935028
3459.512901	204244.853245	45.940033
3457.744383	202368.218497	45.945037
3455.349253	200457.473261	45.950042
3453.359224	198506.066883	45.955047
3451.029692	196537.038965	45.960052
3448.429819	194529.524463	45.965057
3446.269110	192492.074462	45.970061
3443.717963	190442.520561	45.975066
3440.980272	188343.782184	45.980071
3438.776811	186225.621325	45.985076
3435.940891	184100.115476	45.990081
3433.660744	181929.599693	45.995085
3430.791344	179756.501114	46.000090
3428.015092	177549.702949	46.005095
3425.369139	175325.143381	46.010100
3422.161948	173077.104136	46.015105
3419.723829	170812.141594	46.020109
3416.479013	168536.247492	46.025114
3413.330897	166242.347104	46.030119
3410.315895	163934.703567	46.035124
3406.944326	161616.656290	46.040129
3403.342917	159268.716071	46.045133
3399.897746	156930.016474	46.050138
3396.610158	154565.433348	46.055143
3392.975245	152207.084053	46.060148
3389.194259	149855.486790	46.065153
3385.499145	147476.020577	46.070157
3381.348724	145105.958330	46.075162
3377.409620	142744.485274	46.080167
3373.119380	140384.731687	46.085172
3369.059462	138022.703765	46.090177
3364.554005	135661.169684	46.095181
3360.125422	133323.967270	46.100186
3355.207940	130996.975238	46.105191
3350.581656	128609.909151	46.110196
3345.351455	126320.400631	46.115201
3340.102449	124048.700792	46.120205
3334.411069	121810.824107	46.125210
3328.599924	119600.930894	46.130215
3322.455570	117439.589634	46.135220
3315.290024	115317.454352	46.140225
3308.570285	113261.387268	46.145229
3300.776044	111284.802005	46.150234
3292.784103	109372.408348	46.155239
3284.043853	107543.251636	46.160244
3274.610305	105813.558202	46.165249
3265.039788	104175.714705	46.170253
3255.257242	102651.177212	46.175258
3245.637673	101223.577427	46.180263
3236.495793	99891.087606	46.185268
3227.643691	98657.373767	46.190273
3219.793481	97506.516184	46.195277
3211.650419	96453.552615	46.200282
3204.261975	95471.825541	46.205287
3197.277944	94566.657124	46.210292
3190.768386	93736.123796	46.215297
3184.446856	92952.651392	46.220301
3178.552821	92229.986165	46.225306
3173.095806	91564.755127	46.230311
3167.822316	90944.935736	46.235316
3162.677185	90350.445268	46.240321
3157.560984	89794.601052	46.245325
3153.495047	89278.867632	46.250330
3148.861883	88791.692374	46.255335
3144.802423	88314.968158	46.260340
3140.204044	87874.977720	46.265345
3136.752268	87433.582139	46.270349
3132.573709	87014.400548	46.275354
3128.657180	86609.425905	46.280359
3125.203227	86212.134272	46.285364
3121.200409	85837.395142	46.290369
3117.932843	85434.164724	46.295373
3114.480460	85069.957385	46.300378
3111.164301	84698.504829	46.305383
3107.800579	84332.171364	46.310388
3104.283296	83970.363614	46.315393
3100.800016	83611.527688	46.320397
3097.718205	83243.347423	46.325402
3094.407261	82873.365784	46.330407
3091.152547	82504.752059	46.335412
3087.522076	82148.548909	46.340417
3084.533082	81781.452741	46.345421
3080.743605	81418.945047	46.350426
3077.946273	81057.988957	46.355431
3074.610810	80691.304094	46.360436
3070.680633	80316.638608	46.365441
3067.529026	79941.106978	46.370445
3063.956135	79574.638975	46.375450
3060.794814	79208.238442	46.380455
3057.204588	78829.437205	46.385460
3053.915910	78459.052884	46.390465
3050.732659	78089.584198	46.395469
3047.184527	77714.398695	46.400474
3043.277354	77343.719641	46.405479
3039.978876	76972.378888	46.410484
3035.912607	76610.548684	46.415489
3032.768246	76234.685275	46.420493
3029.312308	75873.366306	46.425498
3025.273478	75508.663581	46.430503
3021.660820	75144.445197	46.435508
3017.957772	74798.469420	46.440513
3014.484827	74431.419546	46.445517
3011.424270	74084.476218	46.450522
3007.334713	73725.710576	46.455527
3003.569429	73370.035604	46.460532
3000.160877	73025.954116	46.465537
2996.409041	72670.743509	46.470541
2992.588508	72332.386176	46.475546
2989.204055	71992.923726	46.480551
2985.413717	71646.024669	46.485556
2981.796073	71324.612832	46.490561
2978.388549	70990.537999	46.495565
2974.854951	70663.902398	46.500570
2971.295703	70323.980883	46.505575
2967.632176	70001.259208	46.510580
2963.638536	69670.035434	46.515585
2960.204130	69349.215923	46.520589
2956.285479	69034.405406	46.525594
2952.897602	68716.931977	46.530599
2949.077415	68401.294830	46.535604
2945.508628	68083.933637	46.540609
2942.061609	67773.184603	46.545613
2938.099532	67475.076039	46.550618
2934.223160	67177.046403	46.555623
2930.607437	66875.373939	46.560628
2926.838213	66590.601203	46.565633
2923.216730	66294.579595	46.570637
2919.287843	66011.203037	46.575642
2916.081702	65725.660022	46.580647
2912.718756	65446.136693	46.585652
2908.907643	65166.223180	46.590657
2905.281722	64869.190610	46.595661
2901.688149	64596.739156	46.600666
2898.199493	64328.717228	46.605671
2894.790644	64050.657317	46.610676
2891.531930	63773.103803	46.615681
2888.412376	63490.022470	46.620685
2884.823348	63218.657878	46.625690
2881.140294	62931.824799	46.630695
2878.067839	62654.483047	46.635700
2874.362705	62376.208828	46.640705
2870.576475	62080.218113	46.645709
2867.207610	61802.595851	46.650714
2863.738552	61525.335076	46.655719
2860.215728	61241.238110	46.660724
2856.713373	60963.506525	46.665729
2853.262579	60678.021292	46.670733
2849.888645	60404.089998	46.675738
2846.171234	60120.753505	46.680743
2843.105751	59837.464284	46.685748
2839.232815	59559.571730	46.690753
2836.139630	59280.329294	46.695757
2832.554884	58996.902578	46.700762
2828.637688	58712.668142	46.705767
2825.305745	58427.177904	46.710772
2821.632081	58152.436710	46.715777
2818.339311	57870.950934	46.720781
2814.764372	57589.474492	46.725786
2811.231496	57309.612812	46.730791
2807.688106	57029.927347	46.735796
2804.287043	56754.899270	46.740801
2800.631118	56475.104613	46.745805
2797.234862	56201.167143	46.750810
2793.715516	55915.793064	46.755815
2790.082163	55638.390361	46.760820
2786.484718	55363.554916	46.765825
2783.074614	55085.438492	46.770829
2779.568198	54805.246646	46.775834
2776.217415	54525.769738	46.780839
2772.808390	54251.939161	46.785844
2768.922420	53980.806604	46.790849
2765.697440	53699.016752	46.795853
2761.981103	53424.311213	46.800858
2758.001570	53144.155954	46.805863
2754.484011	52887.068875	46.810868
2750.693221	52617.529517	46.815873
2747.369336	52344.557914	46.820877
2743.675533	52082.190963	46.825882
2740.358485	51818.473885	46.830887
2737.033934	51558.510142	46.835892
2733.397765	51286.912916	46.840897
2730.169167	51018.674339	46.845901
2726.432202	50757.629514	46.850906
2722.888356	50484.282761	46.855911
2719.475499	50212.828118	46.860916
2716.042624	49950.951906	46.865921
2712.404875	49668.380894	46.870925
2709.277031	49410.611611	46.875930
2705.532362	49141.251312	46.880935
2702.377502	48871.345222	46.885940
2698.494773	48604.137747	46.890945
2695.779030	48313.751507	46.895949
2691.948280	48051.109252	46.900954
2688.186981	47773.699580	46.905959
2684.660709	47498.780911	46.910964
2681.360299	47231.561861	46.915969
2678.097794	46955.872761	46.920973
2674.166426	46681.166887	46.925978
2670.489028	46405.974318	46.930983
2667.430120	46127.694800	46.935988
2663.732365	45868.126687	46.940993
2659.916282	45590.390818	46.945997
2656.451405	45321.964327	46.951002
2652.911814	45052.905847	46.956007
2649.741910	44773.614009	46.961012
2646.080361	44507.726737	46.966017
2643.118284	44234.674846	46.971021
2639.324857	43960.380186	46.976026
2635.796907	43684.322462	46.981031
2632.779759	43408.207290	46.986036
2628.728342	43131.699277	46.991041
2625.315049	42848.417446	46.996045
2621.977448	42570.124326	47.001050
2618.327822	42291.820101	47.006055
2615.043989	42022.314374	47.011060
2611.438250	41755.988428	47.016065
2607.821484	41468.190574	47.021069
2604.514161	41194.488255	47.026074
2600.710160	40916.529927	47.031079
2597.259583	40626.669033	47.036084
2593.568145	40358.642435	47.041089
2590.132662	40074.613550	47.046093
2587.104914	39821.003289	47.051098
2582.637137	39542.785843	47.056103
2579.723435	39255.059315	47.061108
2576.052113	38984.941492	47.066113
2572.500514	38701.551025	47.071117
2569.048840	38434.005181	47.076122
2565.517626	38160.699346	47.081127
2562.147007	37881.380625	47.086132
2558.502149	37609.557734	47.091137
2555.016213	37325.465001	47.096141
2551.797022	37054.305277	47.101146
2548.025371	36777.238139	47.106151
2544.662107	36498.601898	47.111156
2541.455595	36223.342703	47.116161
2537.591310	35950.402380	47.121165
2534.700223	35668.438342	47.126170
2530.807654	35395.591961	47.131175
2527.319064	35106.375377	47.136180
2523.679284	34836.938762	47.141185
2520.098793	34554.628254	47.146189
2516.579120	34281.687161	47.151194
2513.032126	34007.663598	47.156199
2510.025197	33721.604346	47.161204
2506.280330	33444.804673	47.166209
2502.643571	33153.470185	47.171213
2499.291949	32887.024188	47.176218
2495.958934	32601.791786	47.181223
2492.625647	32325.062923	47.186228
2488.577405	32041.426855	47.191233
2485.098799	31761.559096	47.196237
2482.135652	31483.832763	47.201242
2478.189089	31208.361820	47.206247
2474.736607	30921.079558	47.211252
2471.025946	30639.057627	47.216257
2467.910178	30352.047458	47.221261
2464.284883	30067.896831	47.226266
2460.802164	29799.672945	47.231271
2456.927279	29509.871631	47.236276
2453.734078	29220.259272	47.241281
2450.515613	28942.892136	47.246285
2447.156962	28670.354231	47.251290
2443.344651	28385.875839	47.256295
2439.786119	28096.393511	47.261300
2436.145876	27813.448716	47.266305
2432.596740	27521.989606	47.271309
2429.090564	27252.883849	47.276314
2425.702955	26962.193228	47.281319
2422.369619	26678.195984	47.286324
2418.491917	26395.441103	47.291329
2415.338716	26114.217944	47.296333
2411.828494	25833.719849	47.301338
2408.442224	25544.398962	47.306343
2404.993214	25254.211319	47.311348
2401.366199	24969.561681	47.316353
2398.019033	24677.370574	47.321357
2394.329678	24386.833870	47.326362
2390.988317	24106.802252	47.331367
2387.560254	23805.817154	47.336372
2384.110805	23522.427387	47.341377
2380.751464	23223.746434	47.346381
2377.450112	22946.100600	47.351386
2373.845905	22647.308202	47.356391
2370.201373	22350.813596	47.361396
2366.680874	22053.144693	47.366401
2363.234207	21758.775567	47.371405
2359.719540	21467.987995	47.376410
2356.309709	21170.802824	47.381415
2352.968505	20869.006061	47.386420
2349.048426	20578.529393	47.391425
2345.823014	20277.300026	47.396429
2342.582592	19981.778591	47.401434
2338.931378	19684.045514	47.406439
2335.639020	19371.426078	47.411444
2332.267265	19076.470907	47.416449
2328.764117	18767.175178	47.421453
2324.912499	18466.223636	47.426458
2321.479475	18167.744787	47.431463
2317.742898	17859.279047	47.436468
2314.412601	17564.802632	47.441473
2310.688142	17263.735808	47.446477
2307.821216	16957.181423	47.451482
2304.213599	16657.157103	47.456487
2300.904859	16351.384442	47.461492
2297.233252	16039.238934	47.466497
2293.757855	15730.538291	47.471501
2290.204482	15417.523079	47.476506
2286.820678	15123.735072	47.481511
2283.562062	14808.919983	47.486516
2279.918884	14491.083080	47.491521
2276.512531	14173.872995	47.496525
2272.838448	13871.030821	47.501530
2269.370884	13556.199412	47.506535
2266.143901	13237.935178	47.511540
2262.260876	12921.931827	47.516545
2258.623222	12614.712659	47.521549
2255.273387	12294.108981	47.526554
2251.756223	11998.889396	47.531559
2248.016040	11680.098449	47.536564
2244.311379	11372.317954	47.541569
2240.428435	11063.066658	47.546573
2236.844222	10774.347528	47.551578
2232.426955	10487.447296	47.556583
2228.665286	10208.837717	47.561588
2224.188337	9944.047859	47.566593
2220.611948	9677.705881	47.571597
2216.112370	9421.917013	47.576602
2212.100922	9182.512311	47.581607
2208.354496	8938.621868	47.586612
2204.344708	8707.516323	47.591617
2200.689100	8472.208535	47.596621
2196.982351	8256.536362	47.601626
2193.323456	8045.480448	47.606631
2189.541652	7822.478585	47.611636
2185.672146	7633.005795	47.616641
2181.672069	7433.866936	47.621645
2178.228415	7234.554551	47.626650
2174.488532	7044.118012	47.631655
2171.115059	6856.262583	47.636660
2167.119536	6678.178618	47.641665
2163.622870	6482.566732	47.646669
2159.861087	6310.308112	47.651674
2155.865599	6133.444768	47.656679
2152.685814	5956.895428	47.661684
2149.264519	5784.363781	47.666689
2145.693330	5614.692885	47.671693
2142.384573	5447.267479	47.676698
2139.036281	5282.362609	47.681703
2135.542254	5110.269626	47.686708
2132.209035	4942.434939	47.691713
2128.783820	4767.945081	47.696717
2125.474675	4599.207865	47.701722
2121.626218	4427.442625	47.706727
2118.825910	4256.799834	47.711732
2114.920883	4080.834677	47.716737
2111.313527	3910.615717	47.721741
2108.036874	3734.916358	47.726746
2104.406555	3569.052206	47.731751
2101.335666	3393.102458	47.736756
2097.449109	3222.639367	47.741761
2093.780989	3044.780231	47.746765
2090.639916	2871.909646	47.751770
2087.068474	2708.189611	47.756775
2083.740183	2534.626929	47.761780
2080.204297	2371.432828	47.766785
2076.803989	2201.048879	47.771789
2073.057138	2025.493532	47.776794
2069.499170	1866.759481	47.781799
2066.308628	1679.476378	47.786804
2062.802705	1510.048930	47.791809
2059.038238	1338.869515	47.796813
2055.554696	1173.678433	47.801818
2051.675563	1014.413681	47.806823
2048.121245	842.997309	47.811828
2044.227037	692.384943	47.816833
2040.485011	543.148495	47.821837
2036.957819	375.317101	47.826842
2033.273891	240.732429	47.831847
2029.169108	100.880383	47.836852
2023.423278	21.224915	47.841857
2013.854917	54.006081	47.846861
2007.356129	61.236727	47.851866
2002.901274	72.342810	47.856871
2000.275456	62.471187	47.861876
1998.035936	63.501824	47.866881
1995.039181	66.160100	47.871885
1993.056732	63.249499	47.876890
1989.636219	71.827186	47.881895
1986.052725	67.869935	47.886900
1982.762759	68.862457	47.891905
1979.309390	72.092073	47.896909
1976.093949	73.942993	47.901914
1972.343122	79.563563	47.906919
1969.444853	78.292765	47.911924
1965.850231	72.002347	47.916929
1961.978480	66.543093	47.921933
1958.835737	58.400733	47.926938
1955.751192	73.202911	47.931943
1951.827114	68.315012	47.936948
1948.613224	81.783316	47.941953
1944.965072	74.441395	47.946957
1941.482589	69.193326	47.951962
1937.988244	71.242927	47.956967
1934.995249	77.570684	47.961972
1931.485121	67.008532	47.966977
1928.050644	65.375552	47.971981
1924.596435	62.413686	47.976986
1920.575933	73.958042	47.981991
1917.321004	73.818776	47.986996
1913.947528	81.145737	47.992001
1910.364741	80.826816	47.997005
1907.302884	76.829094	48.002010
1903.560954	81.768068	48.007015
1900.320126	72.198361	48.012020
1896.692436	78.596972	48.017025
1893.091504	80.321572	48.022029
1889.988629	70.961242	48.027034
1886.582376	73.329277	48.032039
1882.888056	74.233241	48.037044
1879.063995	78.084058	48.042049
1875.463543	68.111882	48.047053
1872.583848	73.115258	48.052058
1868.927255	74.718858	48.057063
1865.627428	66.715008	48.062068
1862.142393	70.803850	48.067073
1858.286943	79.864098	48.072077
1855.086044	70.924092	48.077082
1851.169344	77.462857	48.082087
1848.309217	70.927829	48.087092
1844.375306	70.372805	48.092097
1841.108219	75.041331	48.097101
1837.559777	68.408372	48.102106
1833.647945	77.138918	48.107111
1830.720917	58.727840	48.112116
1827.158289	72.975251	48.117121
1823.600613	79.169933	48.122125
1820.198791	77.329392	48.127130
1816.932185	69.573468	48.132135
1813.397044	80.605294	48.137140
1809.647955	69.115618	48.142145
1805.772188	69.323484	48.147149
1802.290775	69.795514	48.152154
1798.902121	75.324657	48.157159
1796.079371	74.532485	48.162164
1792.487114	71.750459	48.167169
1788.930751	70.348577	48.172173
1785.418164	70.214871	48.177178
1781.703633	67.091308	48.182183
1778.009689	67.267567	48.187188
1774.432478	63.679580	48.192193
1771.230868	73.381029	48.197197
1768.270670	75.144606	48.202202
1764.202812	77.508646	48.207207
1761.091507	75.591023	48.212212
1757.219340	70.305929	48.217217
1753.573311	69.383175	48.222221
1750.119756	66.218782	48.227226
1746.887818	73.808379	48.232231
1743.616026	80.338004	48.237236
1739.532344	74.396301	48.242241
1735.939233	66.473202	48.247245
1732.724561	63.420131	48.252250
1729.207676	63.242823	48.257255
1725.874757	63.878305	48.262260
1722.498645	65.798735	48.267265
1718.438017	71.913965	48.272269
1715.477208	66.755188	48.277274
1711.585082	76.915902	48.282279
1708.601410	63.768865	48.287284
1705.025657	65.606647	48.292289
1701.396123	62.112301	48.297293
1697.834778	62.318457	48.302298
1694.156003	57.575781	48.307303
1690.694861	61.021839	48.312308
1687.106651	66.626534	48.317313
1683.669587	62.994502	48.322317
1680.614524	69.088414	48.327322
1677.146514	65.834559	48.332327
1673.733208	68.020260	48.337332
1670.147768	69.508385	48.342337
1665.978592	67.797484	48.347341
1663.190126	58.346911	48.352346
1659.160610	70.484386	48.357351
1655.638740	61.775034	48.362356
1652.334068	66.379888	48.367361
1648.778743	65.699247	48.372365
1645.188068	61.961554	48.377370
1641.794368	77.204487	48.382375
1638.652954	64.234029	48.387380
1634.944507	66.940509	48.392385
1631.305341	65.042266	48.397389
1627.928504	68.715601	48.402394
1624.303273	67.859243	48.407399
1621.525435	66.022356	48.412404
1617.520610	64.200331	48.417409
1613.549964	54.994913	48.422413
1610.229448	56.931987	48.427418
1606.659122	69.374103	48.432423
1602.992793	58.441066	48.437428
1600.062267	56.662886	48.442433
1596.514095	60.752195	48.447437
1593.399382	59.110414	48.452442
1589.475092	59.730926	48.457447
1585.803276	56.876008	48.462452
1582.082188	53.639654	48.467457
1578.752775	70.849923	48.472461
1575.284901	62.736445	48.477466
1571.438756	70.181764	48.482471
1568.673524	56.639924	48.487476
1564.857689	66.250884	48.492481
1561.083298	71.296287	48.497485
1557.405256	69.685737	48.502490
1553.897480	74.293936	48.507495
1550.434789	67.027560	48.512500
1546.935468	67.110163	48.517505
1543.399225	69.916274	48.522509
1540.536701	65.773580	48.527514
1536.606239	67.606823	48.532519
1533.610771	68.066160	48.537524
1530.290993	60.533813	48.542529
1526.474388	71.290213	48.547533
1522.980425	64.031908	48.552538
1519.550927	65.195112	48.557543
1516.246179	67.117093	48.562548
1512.194914	58.680493	48.567553
1508.588852	62.415052	48.572557
1505.449801	60.716995	48.577562
1501.501909	65.672511	48.582567
1498.347085	61.853999	48.587572
1494.958109	66.994125	48.592577
1490.998035	65.427744	48.597581
1487.614870	64.384848	48.602586
1484.366856	62.368488	48.607591
1481.169723	67.241303	48.612596
1477.663600	61.443445	48.617601
1473.955164	64.387264	48.622605
1470.458187	57.031377	48.627610
1466.952133	66.204728	48.632615
1462.903755	69.461194	48.637620
1459.610300	54.863101	48.642625
1456.312620	60.969731	48.647629
1452.919184	61.576807	48.652634
1449.465937	68.163381	48.657639
1446.038068	59.705167	48.662644
1442.422751	62.435100	48.667649
1438.387083	62.025878	48.672653
1435.491428	58.318685	48.677658
1431.572512	71.245689	48.682663
1427.954301	59.409837	48.687668
1424.883819	55.742669	48.692673
1421.285445	64.360994	48.697677
1418.164875	59.480432	48.702682
1414.268125	65.165144	48.707687
1410.729510	57.929696	48.712692
1407.212686	58.448531	48.717697
1403.642125	65.853929	48.722701
1400.340592	55.322639	48.727706
1396.645288	62.424854	48.732711
1393.404911	53.067265	48.737716
1389.915178	58.128276	48.742721
1386.015114	66.246495	48.747725
1382.930687	58.674203	48.752730
1379.256316	65.301738	48.757735
1375.605630	59.403161	48.762740
1372.095029	49.486757	48.767745
1368.578622	60.844787	48.772749
1365.570428	61.878817	48.777754
1361.791649	63.523864	48.782759
1358.650827	60.937099	48.787764
1354.754089	67.871539	48.792769
1351.047387	64.607712	48.797773
1347.931999	56.163902	48.802778
1344.065695	62.498782	48.807783
1340.419301	57.453781	48.812788
1337.142073	64.901867	48.817793
1333.693888	63.752141	48.822797
1330.228176	60.884042	48.827802
1326.859190	64.274659	48.832807
1323.401155	60.155652	48.837812
1319.961605	65.170864	48.842817
1316.168320	65.748827	48.847821
1313.013260	55.653400	48.852826
1308.703071	65.031768	48.857831
1305.309613	53.391754	48.862836
1302.330356	59.489709	48.867841
1298.804358	58.023141	48.872845
1295.623852	54.642165	48.877850
1291.576969	63.485763	48.882855
1288.460591	62.211345	48.887860
1284.565987	66.108208	48.892865
1281.181705	63.341277	48.897869
1277.885785	59.215893	48.902874
1273.998399	59.036631	48.907879
1270.481245	59.463816	48.912884
1267.119177	63.897427	48.917889
1263.495705	60.725013	48.922893
1260.466595	56.203521	48.927898
1256.643511	63.385895	48.932903
1253.116408	66.060954	48.937908
1249.796057	61.341443	48.942913
1246.043252	59.337748	48.947917
1242.902034	60.484390	48.952922
1239.205163	62.227393	48.957927
1235.725904	66.505350	48.962932
1232.225517	54.167085	48.967937
1228.876144	52.622272	48.972941
1225.174268	51.414223	48.977946
1221.652350	75.108882	48.982951
1218.214664	67.066757	48.987956
1214.917812	67.605008	48.992961
1210.674545	69.797399	48.997965
1207.606075	65.690217	49.002970
1204.190693	59.027199	49.007975
1200.746954	66.688054	49.012980
1197.352578	61.163887	49.017985
1193.332335	68.557487	49.022989
1189.825053	60.551583	49.027994
1186.365842	65.361102	49.032999
1183.120807	55.172245	49.038004
1179.802716	56.773711	49.043009
1176.218536	60.783369	49.048013
1172.652343	64.062535	49.053018
1169.064888	57.518221	49.058023
1165.499583	64.027506	49.063028
1162.088937	60.942038	49.068033
1158.662458	67.951622	49.073037
1155.100465	66.449611	49.078042
1151.331163	64.768082	49.083047
1147.706527	70.435597	49.088052
1144.628022	61.321689	49.093057
1140.991649	66.845507	49.098061
1137.466784	60.174345	49.103066
1133.981411	58.736279	49.108071
1130.513201	64.705181	49.113076
1127.088731	68.708836	49.118081
1123.549351	64.213492	49.123085
1120.460657	55.366952	49.128090
1116.671489	60.826111	49.133095
1113.189989	58.390846	49.138100
1109.468561	60.403501	49.143105
1105.812973	68.708168	49.148109
1102.624677	66.688918	49.153114
1099.042413	62.083237	49.158119
1095.455438	61.819048	49.163124
1092.453556	66.107736	49.168129
1088.824079	65.249079	49.173133
1085.420016	65.747211	49.178138
1081.366930	67.182203	49.183143
1077.776374	64.703912	49.188148
1074.587610	60.558663	49.193153
1070.937217	74.402367	49.198157
1067.230085	64.029631	49.203162
1063.551487	63.026812	49.208167
1060.517552	60.379122	49.213172
1057.388320	55.129882	49.218177
1053.206556	65.370938	49.223181
1049.755093	63.867481	49.228186
1046.223263	65.907424	49.233191
1043.016644	52.915803	49.238196
1039.648832	59.074659	49.243201
1036.238373	54.435780	49.248205
1032.523717	58.589303	49.253210
1029.328120	62.965286	49.258215
1025.406947	60.089519	49.263220
1021.716613	51.504901	49.268225
1018.248078	63.504110	49.273229
1015.065550	67.735680	49.278234
1011.402150	60.668639	49.283239
1008.012825	61.461888	49.288244
1004.424929	46.172946	49.293249
1001.055216	54.755588	49.298253
997.978139	57.423548	49.303258
994.070328	57.140027	49.308263
989.772380	57.458605	49.313268
986.949462	52.942892	49.318273
983.551831	58.562259	49.323277
979.943155	51.439210	49.328282
976.349498	65.084220	49.333287
972.756317	55.373913	49.338292
969.421697	63.217069	49.343297
965.902948	55.190914	49.348301
963.034380	55.108525	49.353306
959.178835	58.138835	49.358311
955.135919	63.099934	49.363316
951.839375	55.984971	49.368321
948.178154	60.604729	49.373325
944.837359	46.052261	49.378330
941.179704	55.477284	49.383335
937.578845	48.454273	49.388340
934.775564	48.500878	49.393345
930.864046	60.123373	49.398349
927.520547	52.392504	49.403354
924.053439	49.452014	49.408359
920.333194	53.546338	49.413364
916.675254	49.227838	49.418369
913.197669	62.399099	49.423373
909.689716	55.004040	49.428378
906.617021	60.218206	49.433383
903.134310	63.617273	49.438388
899.853603	64.558071	49.443393
895.994266	58.850561	49.448397
892.075342	56.838221	49.453402
888.363467	61.769656	49.458407
885.274996	60.184114	49.463412
881.905756	53.415928	49.468417
877.967953	60.239898	49.473421
874.873945	58.342009	49.478426
871.416385	60.977834	49.483431
868.001909	69.785832	49.488436
864.314551	60.735737	49.493441
860.523679	61.408413	49.498445
857.013982	57.519147	49.503450
853.572249	55.928820	49.508455
850.016619	54.951124	49.513460
846.915245	59.511726	49.518465
843.408980	61.766040	49.523469
840.155168	53.628851	49.528474
836.090240	61.703463	49.533479
832.594313	54.898186	49.538484
829.282611	57.248591	49.543489
825.691314	61.322759	49.548493
822.864745	48.575453	49.553498
818.795760	48.114761	49.558503
815.036892	50.914848	49.563508
811.396695	40.297648	49.568513
807.939897	52.579810	49.573517
805.034469	40.901576	49.578522
801.536364	56.363504	49.583527
797.802481	49.630308	49.588532
794.467155	37.994090	49.593537
790.742278	52.020360	49.598541
787.231314	41.303839	49.603546
783.565667	48.357308	49.608551
779.837891	39.136420	49.613556
776.563146	47.565043	49.618561
773.239353	52.056089	49.623565
770.132035	52.153518	49.628570
766.580719	47.527315	49.633575
762.871956	51.948934	49.638580
759.506342	40.545267	49.643585
755.394679	45.235626	49.648589
751.896945	48.621276	49.653594
748.375687	46.809322	49.658599
744.769512	50.079077	49.663604
741.615521	46.137322	49.668609
738.324345	49.674131	49.673613
734.975267	50.122647	49.678618
731.553868	52.961668	49.683623
727.778512	44.691066	49.688628
724.226206	43.909055	49.693633
720.493475	60.119603	49.698637
716.873376	49.360088	49.703642
713.324286	53.332771	49.708647
709.867693	49.821235	49.713652
706.585131	48.373719	49.718657
703.233778	57.848927	49.723661
700.099992	41.134926	49.728666
696.387957	53.583640	49.733671
692.679048	48.662604	49.738676
689.466553	45.191946	49.743681
685.650140	49.171699	49.748685
682.037243	52.467840	49.753690
678.141023	49.784477	49.758695
674.788820	47.158291	49.763700
672.088155	45.353901	49.768705
667.973851	51.395653	49.773709
664.793336	53.934378	49.778714
660.898155	52.842251	49.783719
657.230587	58.197106	49.788724
653.989201	45.688846	49.793729
650.599455	57.935241	49.798733
647.602003	49.979454	49.803738
643.595997	47.566404	49.808743
640.194190	53.563024	49.813748
636.617356	44.258451	49.818753
632.821069	54.891705	49.823757
629.966611	47.334317	49.828762
625.988911	55.154894	49.833767
622.747668	57.601902	49.838772
619.100381	42.328793	49.843777
615.261194	50.311179	49.848781
611.811521	50.471769	49.853786
608.397073	53.379349	49.858791
605.002131	57.169738	49.863796
601.861858	54.219318	49.868801
598.292717	58.951330	49.873805
594.365746	55.165490	49.878810
591.199739	46.492632	49.883815
587.476773	53.096395	49.888820
583.655179	46.946521	49.893825
579.813306	57.280044	49.898829
576.947455	48.019173	49.903834
574.070203	50.396535	49.908839
570.393188	53.481293	49.913844
566.831976	51.213753	49.918849
562.881060	52.835444	49.923853
559.545786	43.398163	49.928858
555.988747	47.856205	49.933863
552.353072	48.014311	49.938868
549.291388	34.734470	49.943873
545.038280	58.644980	49.948877
541.607504	45.815253	49.953882
538.491971	46.739797	49.958887
535.176224	58.256452	49.963892
531.962854	45.389516	49.968897
528.154882	52.506492	49.973901
524.842451	50.804291	49.978906
520.813612	46.037847	49.983911
516.752558	53.121699	49.988916
513.859191	46.168407	49.993921
510.539453	50.459583	49.998925
507.400513	51.583959	50.003930
503.471629	48.136989	50.008935
499.692289	44.416659	50.013940
496.519400	41.155010	50.018945
493.034016	47.085671	50.023949
489.678488	44.096242	50.028954
486.130832	43.411675	50.033959
482.387309	50.373038	50.038964
479.081817	41.870776	50.043969
475.010164	47.149777	50.048973
471.544979	40.197479	50.053978
468.454183	43.016448	50.058983
464.612260	38.685834	50.063988
461.708725	42.718844	50.068993
457.384495	54.289070	50.073997
454.426877	46.991519	50.079002
451.153594	38.917665	50.084007
447.321396	36.088338	50.089012
444.080991	35.510689	50.094017
440.397542	48.714309	50.099021
436.681853	38.384369	50.104026
433.250246	42.038186	50.109031
429.684033	34.168416	50.114036
426.536597	35.721261	50.119041
422.588926	39.645742	50.124045
419.458163	42.198900	50.129050
416.383652	39.491355	50.134055
412.619572	45.582756	50.139060
409.067770	42.870879	50.144065
404.913878	47.321221	50.149069
401.524935	41.869304	50.154074
398.048827	39.784662	50.159079
394.996255	37.469163	50.164084
391.574219	38.049456	50.169089
388.009014	50.339218	50.174093
384.218674	45.184302	50.179098
380.541141	43.071105	50.184103
377.039395	43.724001	50.189108
373.902983	51.178772	50.194113
370.146007	57.566475	50.199117
366.716205	46.859586	50.204122
363.087432	54.967294	50.209127
359.804979	49.555661	50.214132
356.429255	42.902616	50.219137
352.183684	50.129331	50.224141
349.519091	45.892764	50.229146
345.865680	42.551417	50.234151
342.455966	45.167279	50.239156
339.460721	42.564406	50.244161
335.170987	50.278941	50.249165
331.646309	40.896743	50.254170
327.962309	48.408828	50.259175
324.771635	49.709051	50.264180
321.205237	42.937191	50.269185
317.901340	44.176057	50.274189
314.382995	41.721574	50.279194
310.857625	44.798494	50.284199
307.089515	44.227627	50.289204
303.852311	46.395696	50.294209
300.178521	44.845101	50.299213
296.713857	43.151016	50.304218
293.086526	42.634033	50.309223
289.332824	51.030257	50.314228
285.724221	39.655386	50.319233
282.630797	56.310074	50.324237
279.586843	46.219835	50.329242
275.866762	47.447980	50.334247
272.250393	46.467376	50.339252
269.060019	48.463604	50.344257
265.042058	45.296459	50.349261
261.673336	47.178258	50.354266
258.203981	47.098455	50.359271
254.430694	48.018565	50.364276
251.164243	42.129904	50.369281
247.699096	51.256067	50.374285
244.051335	46.275037	50.379290
240.590918	43.159769	50.384295
237.390184	44.414142	50.389300
233.941201	34.627827	50.394305
229.932110	44.880089	50.399309
226.864377	33.841306	50.404314
222.955324	51.481159	50.409319
219.639259	49.137397	50.414324
215.965238	43.290452	50.419329
212.627251	46.603813	50.424333
209.112865	40.700227	50.429338
205.840946	41.149506	50.434343
202.208485	50.649910	50.439348
198.598345	45.416232	50.444353
194.751852	54.678085	50.449357
191.447034	46.720014	50.454362
188.031137	42.224712	50.459367
184.146307	54.327326	50.464372
181.451769	43.995728	50.469377
177.898895	53.565933	50.474381
174.543692	44.647645	50.479386
170.972227	45.896845	50.484391
166.874243	52.999275	50.489396
163.619168	33.191384	50.494401
160.058984	47.211014	50.499405
156.852563	48.115126	50.504410
153.137896	47.282850	50.509415
149.240157	50.282126	50.514420
145.743298	36.959913	50.519425
142.171471	48.567408	50.524429
139.231990	36.499323	50.529434
135.929024	44.325106	50.534439
132.089412	45.628985	50.539444
128.844465	42.486336	50.544449
124.975386	48.198821	50.549453
121.516791	40.290187	50.554458
118.146111	44.336373	50.559463
114.255025	42.266240	50.564468
110.872623	44.542546	50.569473
107.069051	51.497635	50.574477
103.715013	49.916012	50.579482
100.870411	40.300828	50.584487
97.051436	37.453771	50.589492
93.867209	36.497289	50.594497
90.329782	47.979186	50.599501
86.601035	35.886082	50.604506
82.986405	32.937414	50.609511
79.371031	52.309344	50.614516
76.102511	41.919019	50.619521
72.256429	38.142905	50.624525
68.810493	42.074347	50.629530
65.492860	41.401369	50.634535
61.776144	46.700863	50.639540
58.530137	44.036139	50.644545
54.934924	39.046965	50.649549
51.270201	42.958908	50.654554
47.858765	45.878871	50.659559
44.499266	42.073990	50.664564
41.037000	42.948625	50.669569
37.434289	47.967673	50.674573
34.204345	44.142498	50.679578
30.497071	40.755947	50.684583
26.620226	43.739344	50.689588
23.530400	39.452456	50.694593
20.337702	43.939030	50.699597
16.637345	41.022804	50.704602
12.894040	41.780131	50.709607
9.409839	44.050278	50.714612
5.905170	39.515180	50.719617
2.502974	42.724779	50.724621