Thu Aug 25 09:31:57 2022

Number of Points = 9924

Depth (nm)	Load (N)	Time (s)
2.269091	101.871463	0.000000
1.877960	94.836588	0.005005
1.748814	92.129838	0.010010
1.848717	101.564565	0.015014
2.086163	97.803787	0.020019
2.043439	93.621833	0.025024
1.892981	81.503037	0.030029
1.415656	70.330811	0.035034
1.039686	66.090344	0.040038
0.363866	48.757738	0.045043
0.385718	39.272701	0.050048
-0.275263	39.784577	0.055053
0.112962	41.286837	0.060058
-0.906103	37.030079	0.065062
-1.082990	30.901300	0.070067
-1.012251	22.547566	0.075072
-1.029156	35.531316	0.080077
-1.697452	20.798173	0.085082
-2.453247	31.847574	0.090086
-2.733722	30.572419	0.095091
-2.514689	30.085870	0.100096
-2.428354	34.400557	0.105101
-2.770945	32.005671	0.110106
-3.514824	21.811713	0.115110
-3.863677	25.280257	0.120115
-3.951244	29.941731	0.125120
-4.021810	34.787203	0.130125
-4.473945	24.436802	0.135130
-4.885235	39.042081	0.140134
-5.441834	30.353201	0.145139
-5.259334	28.534105	0.150144
-5.295968	30.020673	0.155149
-5.606615	26.529285	0.160154
-5.385299	32.006069	0.165158
-5.964915	24.203487	0.170163
-6.563727	13.730541	0.175168
-7.058139	30.107887	0.180173
-6.838859	27.397175	0.185178
-6.993384	27.513323	0.190182
-6.980449	28.549198	0.195187
-7.562696	17.203620	0.200192
-8.153461	26.980640	0.205197
-8.548154	18.298036	0.210202
-8.695986	19.004758	0.215206
-8.727484	23.334741	0.220211
-8.761512	10.365684	0.225216
-8.842153	22.679202	0.230221
-9.396495	28.419886	0.235226
-9.561888	21.466732	0.240230
-9.903968	26.889419	0.245235
-9.753471	24.781108	0.250240
-10.588763	22.238794	0.255245
-11.269270	26.401547	0.260250
-11.147460	22.111572	0.265254
-11.408024	39.733610	0.270259
-11.253559	20.442288	0.275264
-11.237977	25.644419	0.280269
-11.478366	23.774524	0.285274
-12.157630	20.296601	0.290278
-12.941366	18.723812	0.295283
-12.894450	18.662865	0.300288
-12.956771	27.449088	0.305293
-13.098704	16.366716	0.310298
-12.886550	18.864670	0.315302
-13.245587	26.609050	0.320307
-13.862177	24.646239	0.325312
-14.389200	30.600943	0.330317
-14.271102	27.494796	0.335322
-14.458989	19.741572	0.340326
-15.426410	29.735797	0.345331
-15.827762	26.230148	0.350336
-15.893248	25.440164	0.355341
-15.288903	13.241117	0.360346
-15.731302	13.570050	0.365350
-15.877105	16.250640	0.370355
-15.692678	24.533128	0.375360
-16.638618	26.620914	0.380365
-17.334816	22.864069	0.385370
-17.390865	22.120064	0.390374
-17.308946	20.848240	0.395379
-17.161195	16.481436	0.400384
-18.083166	21.169239	0.405389
-18.237464	21.063889	0.410394
-18.807703	22.532823	0.415398
-19.065922	27.531082	0.420403
-18.984119	23.266359	0.425408
-19.113681	20.129414	0.430413
-18.926779	11.630935	0.435418
-19.471859	14.168441	0.440422
-20.011250	26.186843	0.445427
-19.781782	16.615505	0.450432
-20.275691	31.192593	0.455437
-20.964593	22.973703	0.460442
-21.627194	17.841688	0.465446
-21.710399	25.833914	0.470451
-21.576307	19.969627	0.475456
-21.862730	22.045826	0.480461
-21.900145	20.368756	0.485466
-21.738362	17.815752	0.490470
-22.066899	28.659001	0.495475
-21.969509	23.746428	0.500480
-22.836544	27.175941	0.505485
-23.058087	26.555943	0.510490
-23.079153	19.485264	0.515494
-24.164153	21.139257	0.520499
-24.462673	21.834789	0.525504
-24.526834	30.222667	0.530509
-24.566605	28.530147	0.535514
-24.186306	18.916192	0.540518
-24.580118	24.014790	0.545523
-24.823600	15.893792	0.550528
-25.959613	24.784969	0.555533
-25.891265	20.335692	0.560538
-25.998437	22.304712	0.565542
-26.098514	29.432713	0.570547
-25.767609	28.520510	0.575552
-26.855296	26.118984	0.580557
-27.326165	24.104869	0.585562
-27.548362	23.725418	0.590566
-27.923405	33.006732	0.595571
-27.737845	23.091093	0.600576
-27.675735	34.556510	0.605581
-27.785227	28.913884	0.610586
-28.070807	28.246972	0.615590
-28.900217	28.715638	0.620595
-28.857332	27.035477	0.625600
-29.252225	26.145247	0.630605
-29.078782	24.552197	0.635610
-29.602957	24.893943	0.640614
-30.872841	20.815700	0.645619
-30.521537	21.010780	0.650624
-30.717433	25.224153	0.655629
-30.390114	20.933616	0.660634
-30.840912	27.379413	0.665638
-30.762487	35.020451	0.670643
-31.056695	30.121778	0.675648
-31.519580	26.777632	0.680653
-31.792675	32.537525	0.685658
-31.809748	30.382703	0.690662
-32.893574	23.981580	0.695667
-32.922164	24.438665	0.700672
-33.441560	25.561111	0.705677
-33.770037	28.153266	0.710682
-33.233484	25.452954	0.715686
-33.721121	25.402997	0.720691
-33.462980	22.303382	0.725696
-34.020428	28.591883	0.730701
-34.618126	31.754570	0.735706
-34.804446	31.442265	0.740710
-34.886237	29.522210	0.745715
-34.932697	23.800108	0.750720
-35.301996	29.359938	0.755725
-35.864781	26.768601	0.760730
-36.190858	23.925040	0.765734
-36.523762	26.350209	0.770739
-36.292825	21.328127	0.775744
-36.299750	23.170708	0.780749
-36.763031	25.157560	0.785754
-37.488564	22.816351	0.790758
-37.848586	25.739315	0.795763
-37.790177	21.383345	0.800768
-38.403851	25.997536	0.805773
-38.404463	19.942384	0.810778
-38.454490	23.076204	0.815782
-38.369421	30.751000	0.820787
-38.890703	19.550897	0.825792
-39.537637	27.489083	0.830797
-39.421212	15.445580	0.835802
-39.442180	14.417668	0.840806
-39.879863	23.481001	0.845811
-40.347724	24.756724	0.850816
-40.931581	32.523677	0.855821
-41.486314	22.673413	0.860826
-41.452285	27.521477	0.865830
-41.576438	18.325086	0.870835
-41.061703	19.665150	0.875840
-41.438732	26.735304	0.880845
-41.456909	28.940317	0.885850
-41.665963	21.225212	0.890854
-42.713049	24.644973	0.895859
-42.909544	24.274151	0.900864
-42.952847	19.336168	0.905869
-42.640929	23.881261	0.910874
-43.463842	22.656299	0.915878
-43.997000	35.452015	0.920883
-43.795346	19.759993	0.925888
-44.135216	20.452513	0.930893
-44.434582	26.982151	0.935898
-45.505678	25.356313	0.940902
-44.999518	26.628118	0.945907
-45.403038	26.720006	0.950912
-45.707250	30.909222	0.955917
-45.971572	28.192026	0.960922
-45.636410	26.222460	0.965926
-45.553332	24.115221	0.970931
-46.311484	23.661561	0.975936
-46.690307	27.890941	0.980941
-47.156466	24.075909	0.985946
-47.111734	26.217280	0.990950
-47.326422	27.203399	0.995955
-47.593390	24.192389	1.000960
-48.171435	35.641049	1.005965
-48.617006	29.779000	1.010970
-48.445588	33.707029	1.015974
-48.702821	37.885722	1.020979
-48.695408	17.930914	1.025984
-49.410098	31.179014	1.030989
-49.759393	30.534740	1.035994
-49.549571	29.018248	1.040998
-50.093551	31.890943	1.046003
-50.147805	33.380272	1.051008
-50.176016	32.869187	1.056013
-51.058888	25.016051	1.061018
-51.354706	21.677368	1.066022
-51.631044	28.174924	1.071027
-51.727159	28.908345	1.076032
-52.138911	29.156547	1.081037
-51.728205	29.987726	1.086042
-51.927985	23.308883	1.091046
-52.568066	26.440245	1.096051
-52.964365	25.448996	1.101056
-53.388933	29.407133	1.106061
-53.530986	31.520824	1.111066
-53.204999	30.467021	1.116070
-53.321514	43.627731	1.121075
-53.583075	22.939941	1.126080
-54.407124	29.453714	1.131085
-54.356870	27.212413	1.136090
-54.620375	33.416894	1.141094
-54.964179	36.425904	1.146099
-55.558436	30.685230	1.151104
-56.021268	31.004711	1.156109
-56.183033	20.529728	1.161114
-56.189876	25.004543	1.166118
-56.680758	30.267048	1.171123
-56.294217	25.027595	1.176128
-56.371265	26.324341	1.181133
-56.485333	29.006288	1.186138
-57.202535	18.960022	1.191142
-57.644492	23.107544	1.196147
-57.637230	21.942331	1.201152
-57.970357	26.392341	1.206157
-58.028195	23.231504	1.211162
-58.440639	22.524360	1.216166
-59.225946	29.835658	1.221171
-59.063180	29.338942	1.226176
-59.137307	29.094480	1.231181
-59.343689	32.410988	1.236186
-59.224356	26.564832	1.241190
-60.055994	31.754180	1.246195
-60.311211	32.145534	1.251200
-60.035416	30.210580	1.256205
-60.954411	31.927152	1.261210
-61.472527	29.132665	1.266214
-62.067487	28.707219	1.271219
-61.672497	26.968724	1.276224
-61.854133	29.161384	1.281229
-61.950544	28.562908	1.286234
-62.139580	27.070948	1.291238
-62.483450	28.947342	1.296243
-62.617007	25.045394	1.301248
-63.355476	23.402242	1.306253
-63.483420	20.097367	1.311258
-63.425583	24.824639	1.316262
-63.641279	30.012388	1.321267
-63.615544	25.860854	1.326272
-64.199985	21.820748	1.331277
-65.111985	29.145570	1.336282
-65.208014	26.281783	1.341286
-65.199668	27.675881	1.346291
-65.137708	23.082073	1.351296
-65.566290	30.821532	1.356301
-65.472085	21.059416	1.361306
-65.394924	28.621553	1.366310
-66.805113	31.781835	1.371315
-66.981303	22.017795	1.376320
-66.727977	26.958046	1.381325
-66.940127	32.581839	1.386330
-66.758951	23.625508	1.391334
-67.502832	29.614192	1.396339
-67.588496	21.712076	1.401344
-68.115706	27.685792	1.406349
-68.162854	25.073774	1.411354
-68.138855	25.253700	1.416358
-69.407447	34.997726	1.421363
-69.503923	24.218282	1.426368
-69.761704	36.426682	1.431373
-69.937229	32.645205	1.436378
-69.944829	33.690625	1.441382
-70.129433	36.674690	1.446387
-69.981071	21.335871	1.451392
-69.753493	28.972515	1.456397
-70.574421	36.472895	1.461402
-70.929772	29.960796	1.466406
-71.113000	36.643082	1.471411
-71.371845	23.687103	1.476416
-72.195667	24.306758	1.481421
-72.477385	25.072425	1.486426
-72.340588	24.478537	1.491430
-72.661871	28.502748	1.496435
-72.519488	26.193228	1.501440
-72.579245	33.757838	1.506445
-73.239109	38.974057	1.511450
-73.634498	29.367746	1.516454
-74.175478	26.804633	1.521459
-74.040626	21.930485	1.526464
-74.076829	26.232730	1.531469
-74.240534	23.107465	1.536474
-74.743262	33.452824	1.541478
-75.391904	31.286232	1.546483
-75.099121	27.358610	1.551488
-75.417946	18.309786	1.556493
-75.799412	25.143352	1.561498
-76.245127	25.498117	1.566502
-76.784557	31.669902	1.571507
-77.012126	26.457070	1.576512
-77.165212	32.618939	1.581517
-76.867675	29.924438	1.586522
-76.920321	17.464502	1.591526
-77.203742	24.874328	1.596531
-77.832384	29.794587	1.601536
-78.264789	26.322282	1.606541
-78.901948	30.228309	1.611546
-78.415501	26.264015	1.616550
-78.960270	26.574190	1.621555
-78.514724	26.178698	1.626560
-79.240519	27.893473	1.631565
-79.759415	28.474841	1.636570
-79.876054	25.579482	1.641574
-79.891107	24.338672	1.646579
-80.006974	19.038737	1.651584
-80.525280	31.126603	1.656589
-81.422355	32.608789	1.661594
-81.429838	28.693414	1.666598
-81.771140	27.222149	1.671603
-81.532870	19.035161	1.676608
-81.614190	25.884972	1.681613
-81.955541	17.633781	1.686618
-81.634741	24.066243	1.691622
-82.781156	32.921091	1.696627
-82.961628	21.648610	1.701632
-83.045248	31.380968	1.706637
-83.303749	29.159572	1.711642
-83.051765	27.285296	1.716646
-83.953174	27.572259	1.721651
-84.070299	30.596371	1.726656
-84.514262	36.297617	1.731661
-84.881624	29.787401	1.736666
-84.609655	23.401637	1.741670
-85.228416	24.080911	1.746675
-85.608522	26.940584	1.751680
-85.926626	29.809526	1.756685
-86.413603	36.438166	1.761690
-86.113134	27.637149	1.766694
-86.355153	27.706897	1.771699
-85.954070	18.412392	1.776704
-86.631841	21.707848	1.781709
-87.313974	18.473992	1.786714
-87.531261	26.249943	1.791718
-87.809839	27.227090	1.796723
-87.491738	22.058473	1.801728
-87.717554	27.121257	1.806733
-88.279381	24.634178	1.811738
-88.959116	24.136597	1.816742
-89.309856	29.962439	1.821747
-89.094768	18.260984	1.826752
-89.491202	23.704842	1.831757
-89.272936	27.353444	1.836762
-89.324090	20.515274	1.841766
-90.154888	26.856098	1.846771
-90.433959	24.100088	1.851776
-90.534388	30.060715	1.856781
-90.731536	23.356152	1.861786
-90.887999	21.463619	1.866790
-91.581000	20.651741	1.871795
-92.165579	19.633049	1.876800
-92.042630	22.208253	1.881805
-92.174556	24.326684	1.886810
-92.413183	24.933739	1.891814
-92.764538	25.336995	1.896819
-92.100943	21.617026	1.901824
-93.055210	23.687142	1.906829
-93.931679	27.054863	1.911834
-93.933278	25.340544	1.916838
-93.739031	19.422541	1.921843
-93.658509	16.584877	1.926848
-93.963189	24.868066	1.931853
-94.693038	27.497804	1.936858
-94.957030	22.319156	1.941862
-95.411364	33.337140	1.946867
-95.519712	20.325947	1.951872
-95.658815	20.256182	1.956877
-95.741800	21.205845	1.961882
-96.088040	27.727008	1.966886
-96.464995	27.121873	1.971891
-96.392294	20.368700	1.976896
-96.467050	25.493235	1.981901
-96.842091	16.763270	1.986906
-97.641878	17.451927	1.991910
-98.135309	21.787850	1.996915
-98.133587	22.687045	2.006912
-97.287934	22.985734	2.016909
-97.110962	26.081838	2.026906
-96.920714	32.321499	2.036902
-96.129421	22.136920	2.046899
-95.913573	24.520512	2.056896
-95.469791	28.303405	2.066893
-94.755844	21.761257	2.076890
-93.959204	26.939717	2.086886
-93.197094	24.359287	2.096883
-93.101583	25.551631	2.106880
-92.918267	20.917288	2.116877
-92.087522	20.087406	2.126874
-91.414152	17.901018	2.136870
-91.484564	15.460543	2.146867
-90.492149	19.683325	2.156864
-90.102934	13.841464	2.166861
-89.953074	14.147809	2.176858
-89.072782	20.339529	2.186854
-88.596488	21.320153	2.196851
-88.272228	20.582304	2.206848
-87.361529	18.913096	2.216845
-87.286564	21.391622	2.226842
-86.740487	20.539822	2.236838
-85.941210	26.316585	2.246835
-85.682067	18.740137	2.256832
-85.246437	24.241260	2.266829
-84.802702	25.154126	2.276826
-84.217522	19.706043	2.286822
-83.049957	24.693335	2.296819
-82.979185	25.230652	2.306816
-82.974108	17.063620	2.316813
-82.139020	22.695387	2.326810
-81.625796	26.461065	2.336806
-81.079114	27.443332	2.346803
-80.095166	27.400404	2.356800
-80.086555	23.141894	2.366797
-80.094727	24.901683	2.376794
-78.761823	22.279334	2.386790
-78.580708	23.794053	2.396787
-78.359593	19.768341	2.406784
-77.421389	18.056811	2.416781
-77.169793	18.065280	2.426778
-76.762923	30.980418	2.436774
-75.426280	24.796864	2.446771
-75.452655	25.517296	2.456768
-75.511112	29.283854	2.466765
-74.603838	23.604736	2.476762
-73.856820	26.823764	2.486758
-73.764905	24.680968	2.496755
-73.135707	19.498420	2.506752
-72.850018	19.983054	2.516749
-72.319739	24.766095	2.526746
-71.693012	24.750631	2.536742
-71.150184	22.948997	2.546739
-70.258658	19.321921	2.556736
-69.897018	19.208610	2.566733
-69.928838	19.194964	2.576730
-68.916672	26.959435	2.586726
-68.790806	26.002416	2.596723
-68.000759	23.484134	2.606720
-67.508081	20.635478	2.616717
-67.388097	22.191454	2.626714
-66.031129	30.148989	2.636710
-65.991804	21.925903	2.646707
-65.514741	26.213601	2.656704
-65.367864	26.282828	2.666701
-64.244592	26.240247	2.676698
-63.774217	22.606300	2.686694
-63.792297	22.013960	2.696691
-63.460092	23.973841	2.706688
-62.737760	23.705812	2.716685
-62.063780	32.765058	2.726682
-61.415786	31.602682	2.736678
-61.260971	25.056277	2.746675
-60.638323	25.519793	2.756672
-59.961791	25.401491	2.766669
-59.450698	26.224610	2.776666
-58.687841	31.671297	2.786662
-58.707325	29.796213	2.796659
-58.549049	28.599698	2.806656
-57.338485	28.169638	2.816653
-57.065760	26.863323	2.826650
-56.732831	26.966755	2.836646
-55.634891	22.157421	2.846643
-55.407276	20.034545	2.856640
-55.348554	15.204314	2.866637
-54.665837	21.908505	2.876634
-54.023226	24.025657	2.886630
-53.079480	24.587748	2.896627
-53.061309	27.252572	2.906624
-52.692902	23.137257	2.916621
-51.967786	27.924618	2.926618
-51.144772	34.720872	2.936614
-50.879001	28.828656	2.946611
-50.766964	30.154628	2.956608
-50.229606	25.848114	2.966605
-49.322024	29.469641	2.976602
-49.274987	24.552539	2.986598
-48.592372	23.321384	2.996595
-47.870080	26.468262	3.006592
-47.529445	29.488041	3.016589
-46.666707	28.760855	3.026586
-46.445996	27.335978	3.036582
-46.361148	27.728538	3.046579
-45.540051	26.567551	3.056576
-45.114905	20.279732	3.066573
-44.560723	28.416910	3.076570
-43.788386	27.931971	3.086566
-43.707989	27.758191	3.096563
-43.374331	28.387365	3.106560
-42.357129	28.073135	3.116557
-42.052468	30.306598	3.126554
-41.169992	33.200297	3.136550
-40.740147	29.803951	3.146547
-40.614628	28.713938	3.156544
-40.373452	30.713427	3.166541
-39.379433	35.468161	3.176538
-39.023578	29.815254	3.186534
-38.313635	34.915442	3.196531
-37.736323	37.080843	3.206528
-37.452001	32.221593	3.216525
-37.273563	37.658486	3.226522
-36.355240	24.219666	3.236518
-36.025827	32.933761	3.246515
-35.541140	31.372488	3.256512
-34.624147	33.956670	3.266509
-34.624483	31.663601	3.276506
-34.278472	31.296148	3.286502
-33.208859	31.081413	3.296499
-32.814680	26.293650	3.306496
-32.966362	24.261882	3.316493
-31.779618	22.704650	3.326490
-31.531712	24.826628	3.336486
-31.205074	24.683957	3.346483
-30.368392	23.042190	3.356480
-29.941447	20.324212	3.366477
-29.488110	23.804671	3.376474
-28.676623	26.288174	3.386470
-28.487880	31.580900	3.396467
-28.039077	27.345281	3.406464
-27.147180	24.868065	3.416461
-27.020898	26.790521	3.426458
-26.845172	27.336737	3.436454
-25.953555	24.355882	3.446451
-25.757463	31.313725	3.456448
-24.967847	25.260235	3.466445
-24.255622	20.729919	3.476442
-23.877939	23.138842	3.486438
-23.606580	28.744906	3.496435
-22.792335	29.203747	3.506432
-22.519465	27.485595	3.516429
-21.629848	31.772014	3.526426
-21.415119	31.602529	3.536422
-21.272526	29.109668	3.546419
-20.390048	30.891466	3.556416
-19.818990	23.712803	3.566413
-19.330299	27.786441	3.576410
-18.916759	25.878354	3.586406
-18.247130	28.868761	3.596403
-18.236728	24.904574	3.606400
-17.502022	26.047453	3.616397
-16.922993	22.963522	3.626394
-16.740316	26.847521	3.636390
-15.732939	19.115821	3.646387
-15.588833	19.632144	3.656384
-14.840195	24.146559	3.666381
-13.911267	17.472529	3.676378
-13.801441	18.526416	3.686374
-13.552225	21.516169	3.696371
-13.305649	20.530735	3.706368
-12.211086	20.369113	3.716365
-12.120412	16.028052	3.726362
-11.349447	18.106090	3.736358
-10.581842	23.897329	3.746355
-10.331184	20.351663	3.756352
-10.132960	18.556509	3.766349
-9.123773	11.363057	3.776346
-9.096343	21.565818	3.786342
-8.783425	18.580603	3.796339
-7.831874	26.351414	3.806336
-7.627645	17.288361	3.816333
-6.733536	21.333322	3.826330
-6.385559	21.434398	3.836326
-6.095389	24.341708	3.846323
-5.086432	25.612680	3.856320
-4.546953	26.136748	3.866317
-4.800330	27.668862	3.876314
-4.349594	31.514031	3.886310
-3.436990	39.287783	3.896307
-3.250921	43.947370	3.906304
-3.125302	51.961643	3.916301
-2.214199	62.748235	3.926298
-1.868756	77.405840	3.936294
-1.746455	89.044638	3.946291
-0.809413	100.495599	3.956288
0.000000	116.058863	3.961293
-0.143278	119.903343	3.966298
-0.278020	123.876201	3.971302
0.053468	126.611740	3.976307
-0.192965	131.212709	3.981312
0.229586	139.530709	3.986317
0.314400	144.737847	3.991322
0.432218	147.797935	3.996326
0.720880	151.258366	4.001331
0.655188	154.094105	4.006336
0.746200	150.346769	4.011341
0.555456	135.810791	4.016346
0.076304	134.108009	4.021350
0.416179	129.100465	4.026355
0.283133	141.937973	4.031360
0.562987	146.456486	4.036365
0.768202	147.595120	4.041370
0.615952	138.418885	4.046374
0.709508	129.798932	4.051379
0.515801	130.218615	4.056384
0.314573	134.069014	4.061389
0.326790	130.735827	4.066394
0.365690	145.637656	4.071398
0.814058	138.015645	4.076403
0.594699	149.316430	4.081408
0.710126	153.718338	4.086413
1.150467	153.336318	4.091418
0.624007	140.460139	4.096422
0.558845	127.185823	4.101427
0.526934	132.338480	4.106432
0.777277	125.570085	4.111437
0.693367	137.536180	4.116442
0.382038	136.253195	4.121446
0.654408	140.475484	4.126451
0.904500	142.594186	4.131456
0.867609	147.817231	4.136461
0.418454	144.818924	4.141466
0.577663	150.672475	4.146470
1.098782	146.123751	4.151475
1.448451	152.925070	4.156480
0.895433	133.174993	4.161485
0.654130	136.114175	4.166490
0.384672	137.741636	4.171494
0.817215	131.666033	4.176499
0.820753	139.458058	4.181504
0.849574	133.233737	4.186509
0.526476	141.083268	4.191514
0.760515	155.312282	4.196518
1.032950	149.299725	4.201523
1.173365	159.199538	4.206528
0.988179	149.886088	4.211533
0.939226	148.486062	4.216538
1.047042	145.318229	4.221542
1.074921	136.249815	4.226547
0.237793	142.240488	4.231552
1.115696	144.207040	4.236557
1.169940	153.791318	4.241562
0.927853	151.848908	4.246566
0.914196	152.531449	4.251571
1.089409	159.920094	4.256576
1.255233	153.835653	4.261581
1.175373	148.454103	4.266586
0.782848	155.827295	4.271590
1.260168	153.946175	4.276595
1.041819	152.689750	4.281600
0.886276	150.961573	4.286605
0.648766	153.840051	4.291610
1.156081	164.429034	4.296614
1.413955	162.382978	4.301619
1.258920	159.420843	4.306624
1.173039	151.892026	4.311629
1.341594	154.105763	4.316634
1.158757	168.691173	4.321638
1.303729	155.931247	4.326643
1.276760	154.211398	4.331648
1.260520	157.264018	4.336653
1.476035	158.015057	4.341658
0.915407	159.504641	4.346662
1.372222	152.191352	4.351667
1.145116	158.557855	4.356672
1.053201	163.096657	4.361677
0.998728	151.234861	4.366682
1.220626	148.893883	4.371686
1.437107	160.828747	4.376691
1.433913	160.152385	4.381696
1.003568	156.727182	4.386701
1.182902	157.379485	4.391706
1.278385	162.322363	4.396710
1.105254	146.961032	4.401715
0.888931	158.422699	4.406720
1.133222	163.975019	4.411725
1.339758	179.458058	4.416730
1.649992	178.694621	4.421734
1.623074	177.085494	4.426739
1.316354	177.978471	4.431744
1.534615	182.054222	4.436749
1.575476	188.733095	4.441754
1.428168	193.755152	4.446758
1.502099	180.092003	4.451763
1.750726	181.489596	4.456768
1.549101	180.325462	4.461773
1.500891	184.964991	4.466778
1.496852	184.902535	4.471782
2.057880	179.021923	4.476787
1.082785	175.615629	4.481792
1.358141	177.091291	4.486797
1.758866	178.968095	4.491802
1.828201	175.572166	4.496806
1.745438	173.848402	4.501811
1.452161	188.277123	4.506816
1.650336	181.994613	4.511821
1.728182	186.304340	4.516826
1.425879	176.857363	4.521830
1.883898	173.590362	4.526835
1.762678	183.844397	4.531840
1.624247	173.476394	4.536845
1.680452	176.558796	4.541850
1.461488	179.326804	4.546854
2.070318	174.599814	4.551859
1.655456	175.038330	4.556864
1.632906	167.490092	4.561869
1.868475	177.371842	4.566874
1.686008	186.702158	4.571878
1.595491	175.111752	4.576883
1.843588	187.674437	4.581888
1.737093	180.949276	4.586893
2.023688	175.431206	4.591898
1.927805	182.099864	4.596902
2.092868	177.537316	4.601907
1.776073	180.516808	4.606912
1.958446	178.533200	4.611917
1.894219	182.308359	4.616922
1.717615	178.191655	4.621926
2.135369	181.704632	4.626931
2.157604	185.428280	4.631936
1.864923	186.407643	4.636941
1.878268	183.615278	4.641946
1.682257	176.600420	4.646950
1.986527	180.669022	4.651955
1.837147	181.448761	4.656960
1.996965	179.206092	4.661965
1.974238	175.881536	4.666970
1.926792	177.702008	4.671974
2.084613	182.249142	4.676979
1.992173	183.105381	4.681984
1.715946	188.590566	4.686989
1.966495	190.658582	4.691994
2.373924	210.523659	4.696998
2.755987	195.328401	4.702003
2.200433	192.039869	4.707008
2.207656	192.244571	4.712013
2.257688	176.066794	4.717018
2.261415	179.394703	4.722022
2.056531	172.276832	4.727027
2.187532	181.656108	4.732032
2.367238	184.146515	4.737037
2.340562	182.268427	4.742042
2.086299	174.357854	4.747046
2.186726	170.919089	4.752051
2.331855	180.852977	4.757056
2.394505	172.981336	4.762061
1.964943	172.719795	4.767066
2.099849	180.953167	4.772070
2.211117	188.728334	4.777075
2.642812	205.428978	4.782080
2.702209	197.829922	4.787085
2.847245	182.149787	4.792090
2.428128	188.945023	4.797094
2.802557	184.934971	4.802099
2.371205	188.894205	4.807104
2.522737	181.078237	4.812109
2.828729	188.370473	4.817114
2.579301	183.043954	4.822118
2.512934	177.122437	4.827123
2.417749	185.834794	4.832128
2.638642	172.392237	4.837133
2.536159	182.583224	4.842138
2.292834	185.908713	4.847142
2.268552	179.243438	4.852147
2.361951	186.205147	4.857152
2.370835	184.808711	4.862157
2.029875	184.084029	4.867162
2.124910	180.462607	4.872166
2.785882	184.554417	4.877171
2.420662	192.568759	4.882176
2.239842	200.538394	4.887181
2.696579	201.558528	4.892186
2.425006	211.709585	4.897190
2.726623	204.531325	4.902195
2.742229	207.968110	4.907200
2.577196	211.025070	4.912205
2.906304	203.478666	4.917210
2.926345	215.245026	4.922214
3.156926	207.584342	4.927219
2.721276	193.475836	4.932224
2.461256	188.907122	4.937229
2.595043	186.478703	4.942234
2.415499	199.206478	4.947238
3.057341	197.910188	4.952243
2.820223	210.966534	4.957248
2.472251	200.397226	4.962253
2.666480	201.148438	4.967258
2.614196	214.795931	4.972262
3.357945	202.125655	4.977267
3.037416	203.324520	4.982272
3.208053	206.752834	4.987277
2.938965	200.322063	4.992282
2.530313	190.489940	4.997286
2.805064	196.619635	5.002291
2.831236	208.812142	5.007296
2.845976	207.743822	5.012301
3.065863	207.494420	5.017306
2.725973	210.433241	5.022310
3.117405	196.498869	5.027315
2.919345	210.564672	5.032320
2.952173	210.518587	5.037325
3.000943	207.831400	5.042330
2.631997	210.613421	5.047334
3.152099	197.573224	5.052339
2.905648	207.362834	5.057344
2.835912	199.793501	5.062349
2.761560	208.122949	5.067354
2.764919	209.606430	5.072358
3.044920	205.668117	5.077363
2.964045	208.550536	5.082368
2.978013	209.456544	5.087373
2.865055	200.821457	5.092378
3.380373	209.390714	5.097382
3.097388	204.091593	5.102387
2.666493	206.706147	5.107392
3.452666	223.794199	5.112397
3.325920	224.456496	5.117402
3.070027	216.577797	5.122406
3.020096	218.635947	5.127411
3.191233	227.730545	5.132416
3.297559	238.727254	5.137421
3.375336	242.100520	5.142426
3.487126	237.008459	5.147430
3.277928	218.950833	5.152435
3.068726	224.552080	5.157440
2.910899	228.677276	5.162445
3.088526	237.691767	5.167450
3.375357	237.726109	5.172454
3.364971	232.725959	5.177459
3.124994	235.804156	5.182464
3.657354	235.018570	5.187469
3.766702	237.175154	5.192474
3.507625	246.413099	5.197478
3.606408	231.426713	5.202483
3.001888	227.589018	5.207488
3.174244	240.049711	5.212493
3.317000	238.603822	5.217498
3.323232	246.382816	5.222502
3.482024	237.164123	5.227507
3.403457	241.881190	5.232512
3.456409	232.764505	5.237517
3.774137	231.639219	5.242522
3.113729	241.313371	5.247526
3.519849	231.546558	5.252531
3.199424	233.612289	5.257536
3.333419	232.917593	5.262541
3.557910	234.856817	5.267546
3.271420	237.641742	5.272550
3.496939	239.245443	5.277555
3.456475	240.647206	5.282560
3.391783	245.998023	5.287565
3.313388	239.834757	5.292570
3.502253	248.736760	5.297574
3.695686	261.402977	5.302579
3.450214	263.858771	5.307584
3.249914	261.115686	5.312589
3.708709	261.249637	5.317594
3.499442	260.744766	5.322598
4.064694	253.952293	5.327603
3.555815	261.590536	5.332608
3.815579	252.972956	5.337613
4.354399	250.667732	5.342618
3.893156	258.928106	5.347622
4.055888	256.020573	5.352627
3.680953	268.196872	5.357632
3.799532	257.911939	5.362637
4.005705	257.569771	5.367642
4.073154	256.442568	5.372646
3.933683	242.347730	5.377651
3.815987	230.714088	5.382656
3.748477	240.194102	5.387661
3.722975	236.828839	5.392666
3.885734	263.755945	5.397670
4.183195	249.842582	5.402675
3.987295	253.780758	5.407680
3.947123	244.491994	5.412685
3.749295	241.106274	5.417690
3.702971	244.767908	5.422694
4.221038	241.823686	5.427699
4.034824	241.226617	5.432704
3.802206	255.386457	5.437709
4.286388	251.621790	5.442714
4.035283	243.194992	5.447718
4.055784	239.420719	5.452723
3.642398	243.782116	5.457728
4.418498	244.470636	5.462733
4.313532	235.112933	5.467738
3.846533	232.095260	5.472742
3.988279	239.552458	5.477747
3.832751	242.089071	5.482752
4.154885	255.374205	5.487757
4.219345	259.151364	5.492762
4.284734	259.350118	5.497766
3.940365	259.632056	5.502771
4.159296	264.305680	5.507776
4.085714	259.052828	5.512781
4.233652	259.501243	5.517786
3.986678	261.735806	5.522790
4.659695	254.648033	5.527795
4.558188	256.435854	5.532800
3.867073	247.960934	5.537805
4.345870	247.440007	5.542810
4.566824	250.221358	5.547814
4.356368	241.342095	5.552819
3.861900	236.066609	5.557824
4.000325	245.650403	5.562829
4.325201	254.958211	5.567834
3.847827	262.370052	5.572838
4.423242	258.258890	5.577843
4.391994	261.440432	5.582848
4.049939	262.898941	5.587853
4.352145	259.922098	5.592858
4.178068	263.002630	5.597862
4.034946	252.768195	5.602867
3.914834	259.513445	5.607872
4.116971	258.213277	5.612877
4.408271	270.383268	5.617882
4.432538	268.323181	5.622886
4.594262	276.248670	5.627891
4.527117	273.816921	5.632896
4.379837	273.618718	5.637901
4.859252	272.724365	5.642906
4.116531	270.056775	5.647910
4.570632	268.400748	5.652915
4.718291	279.944671	5.657920
4.412345	278.635522	5.662925
4.581411	283.057532	5.667930
4.483557	282.914861	5.672934
4.911423	280.190413	5.677939
4.450293	277.902652	5.682944
4.139763	282.750988	5.687949
4.313384	276.987992	5.692954
4.504296	288.031590	5.697958
4.768971	285.291581	5.702963
4.984637	294.562736	5.707968
4.705586	288.487841	5.712973
4.805168	278.569711	5.717978
4.709716	290.180207	5.722982
4.775531	282.431410	5.727987
4.495604	285.417797	5.732992
4.635630	292.660148	5.737997
5.046445	286.625863	5.743002
4.757132	286.237939	5.748006
5.150738	278.497898	5.753011
4.702645	279.593366	5.758016
4.456810	285.352234	5.763021
5.001523	279.863294	5.768026
4.897682	282.448762	5.773030
5.073486	279.630927	5.778035
4.982064	284.900522	5.783040
4.709593	284.801029	5.788045
5.130464	277.575581	5.793050
4.791172	280.818045	5.798054
5.053395	282.336904	5.803059
4.962569	281.253482	5.808064
4.320889	276.039015	5.813069
4.694315	271.889894	5.818074
4.549102	282.179383	5.823078
4.845219	275.900477	5.828083
4.750246	277.304455	5.833088
4.714010	286.162651	5.838093
4.931067	278.459763	5.843098
4.868868	285.917296	5.848102
4.954805	282.863601	5.853107
4.964234	290.699062	5.858112
4.831971	285.623079	5.863117
5.107135	288.351649	5.868122
4.802303	298.789545	5.873126
5.123248	304.136907	5.878131
5.117623	308.535672	5.883136
4.744911	303.791592	5.888141
5.430023	303.481952	5.893146
5.410269	303.241621	5.898150
5.504258	303.866173	5.903155
5.320569	292.840791	5.908160
5.020845	282.956748	5.913165
5.307472	277.381693	5.918170
5.017463	291.499933	5.923174
4.888180	288.634984	5.928179
5.127458	301.426926	5.933184
5.097861	313.776942	5.938189
5.317840	298.081800	5.943194
5.194970	310.342021	5.948198
5.321319	301.935150	5.953203
5.399779	307.814060	5.958208
5.333457	311.693980	5.963213
5.516896	305.647858	5.968218
5.717841	296.413038	5.973222
5.470429	284.897764	5.978227
5.462503	274.762358	5.983232
5.181371	271.342228	5.988237
5.728793	277.210926	5.993242
5.108071	288.346890	5.998246
5.430299	273.066028	6.003251
5.181534	278.018582	6.008256
5.266068	277.125987	6.013261
5.358061	276.580241	6.018266
5.028630	275.151384	6.023270
4.768895	269.361375	6.028275
5.362419	279.997032	6.033280
4.985077	281.717340	6.038285
5.831106	291.778758	6.043290
5.376402	285.234668	6.048294
5.359108	278.356286	6.053299
5.174860	292.530723	6.058304
5.317860	275.335362	6.063309
5.246828	279.171720	6.068314
5.055517	285.757290	6.073318
5.396002	284.707531	6.078323
4.766950	287.992233	6.083328
5.293484	300.372165	6.088333
5.287095	307.159727	6.093338
5.360524	308.265235	6.098342
5.353598	296.345271	6.103347
5.598233	304.014170	6.108352
5.434091	304.210921	6.113357
5.026955	284.883916	6.118362
5.245367	299.846334	6.123366
5.240523	306.339419	6.128371
5.453887	308.818243	6.133376
5.596646	305.651235	6.138381
5.176415	275.961650	6.143386
5.080727	287.183032	6.148390
5.650695	296.983981	6.153395
5.409503	291.520096	6.158400
5.038751	285.649398	6.163405
5.048553	280.266415	6.168410
5.039584	285.763540	6.173414
5.517307	304.598963	6.178419
5.438146	313.941633	6.183424
5.582841	297.872302	6.188429
5.202106	282.938857	6.193434
4.770065	288.268149	6.198438
5.329860	299.491243	6.203443
5.145295	301.184512	6.208448
5.167080	302.582855	6.213453
5.711458	304.864279	6.218458
5.504671	302.191808	6.223462
5.648937	290.634144	6.228467
5.362887	297.051061	6.233472
5.199757	289.202089	6.238477
5.397299	278.601047	6.243482
5.052972	285.675671	6.248486
5.348027	276.577979	6.253491
5.165423	280.798820	6.258496
5.019329	282.096912	6.263501
5.497328	286.834357	6.268506
5.470585	298.206298	6.273510
5.202747	285.830503	6.278515
4.975992	283.746468	6.283520
5.382627	298.328212	6.288525
5.863087	291.049128	6.293530
5.468115	288.893371	6.298534
5.191989	278.040672	6.303539
5.143317	279.516491	6.308544
4.985074	281.246764	6.313549
5.517576	284.485516	6.318554
5.097377	285.051422	6.323558
5.271127	287.416225	6.328563
5.504797	294.007979	6.333568
5.632928	286.768281	6.338573
5.199033	282.688701	6.343578
5.012408	283.126260	6.348582
4.938992	270.014485	6.353587
5.540778	290.788850	6.358592
5.429649	290.749501	6.363597
5.647411	286.583637	6.368602
5.143321	286.140778	6.373606
5.106231	279.933060	6.378611
4.911809	284.355074	6.383616
5.407380	300.606030	6.388621
5.715186	311.590198	6.393626
5.175132	293.840604	6.398630
5.395246	283.466981	6.403635
5.580898	289.765695	6.408640
5.161840	280.738760	6.413645
5.226110	277.799193	6.418650
5.063514	280.710248	6.423654
4.916756	274.519715	6.428659
5.427500	301.063319	6.433664
5.630343	304.802987	6.438669
5.371617	287.749652	6.443674
5.160596	291.611110	6.448678
5.027158	284.152964	6.453683
5.208292	298.627668	6.458688
5.204614	303.219120	6.463693
5.698725	305.188875	6.468698
5.629413	311.176361	6.473702
5.184941	291.697008	6.478707
5.368761	292.845331	6.483712
5.419830	284.269926	6.488717
5.322506	286.291216	6.493722
5.149324	287.796037	6.498726
5.310355	280.981464	6.503731
5.549940	278.969898	6.508736
5.126087	288.347579	6.513741
5.348802	280.941201	6.518746
5.245894	281.875017	6.523750
5.090568	282.500664	6.528755
5.510024	277.246489	6.533760
5.416230	288.980112	6.538765
5.244270	282.663810	6.543770
4.937970	285.072189	6.548774
5.379953	295.184260	6.553779
5.363355	278.956716	6.558784
5.102037	293.317239	6.563789
5.470012	285.021216	6.568794
5.217900	284.412325	6.573798
5.239900	289.037716	6.578803
5.370096	291.213187	6.583808
5.448379	296.370772	6.588813
5.813841	288.157401	6.593818
5.263606	284.966096	6.598822
5.383188	281.492670	6.603827
5.333676	290.454190	6.608832
5.398738	284.211483	6.613837
5.348385	284.963055	6.618842
5.308174	288.225100	6.623846
5.612084	290.658096	6.628851
5.604202	283.876316	6.633856
5.281453	285.853831	6.638861
5.453948	279.977113	6.643866
5.377811	290.154542	6.648870
5.498859	281.384673	6.653875
5.520042	290.224383	6.658880
5.082908	285.955481	6.663885
5.275124	281.493059	6.668890
4.976193	288.297975	6.673894
5.625601	289.515721	6.678899
5.534381	289.865564	6.683904
5.444733	293.521341	6.688909
5.410149	289.183039	6.693914
5.304139	290.300842	6.698918
5.111866	293.434851	6.703923
5.348153	285.975724	6.708928
5.144795	286.767087	6.713933
5.027582	288.142914	6.718938
4.978046	295.649088	6.723942
5.180124	289.736094	6.728947
5.075078	294.302297	6.733952
5.100464	288.929525	6.738957
5.188145	287.976323	6.743962
4.926583	291.431242	6.748966
4.909924	291.668161	6.753971
5.086105	292.396895	6.758976
5.084214	299.433690	6.763981
5.316814	302.573899	6.768986
5.645168	311.811588	6.773990
5.360384	297.631904	6.778995
4.795967	284.748912	6.784000
5.192010	309.548260	6.789005
5.642228	308.997007	6.794010
5.142998	311.736181	6.799014
5.146225	315.203401	6.804019
5.572597	313.317592	6.809024
5.241172	322.326462	6.814029
5.539937	307.526982	6.819034
5.362269	304.887914	6.824038
5.225446	290.868554	6.829043
5.222486	289.293629	6.834048
5.256926	289.680733	6.839053
5.274075	297.340977	6.844058
5.314537	294.715192	6.849062
5.320605	303.035248	6.854067
5.620495	301.254680	6.859072
5.172513	301.264946	6.864077
5.650690	283.498196	6.869082
5.201562	285.156985	6.874086
5.308763	288.598417	6.879091
5.516014	288.037777	6.884096
5.200277	287.818511	6.889101
5.137360	289.831247	6.894106
5.110146	287.095841	6.899110
5.156743	286.604665	6.904115
5.088874	291.642777	6.909120
5.384929	297.528720	6.914125
5.542952	287.914645	6.919130
5.115641	293.458336	6.924134
5.274303	289.662405	6.929139
5.342915	288.791287	6.934144
5.158710	296.214156	6.939149
5.322661	292.376266	6.944154
5.268482	295.621519	6.949158
5.584881	299.093453	6.954163
5.541063	299.891458	6.959168
4.951314	288.002705	6.964173
5.418537	284.617182	6.969178
5.259029	289.520952	6.974182
4.960453	286.372476	6.979187
5.061489	291.178476	6.984192
5.181443	304.808542	6.989197
6.009681	313.683168	6.994202
5.451185	314.542831	6.999206
5.646002	300.145629	7.004211
5.507451	293.238783	7.009216
5.416910	303.412149	7.014221
5.233927	290.545321	7.019226
5.165656	289.075543	7.024230
5.425769	288.364248	7.029235
5.359539	295.929987	7.034240
4.871979	292.102427	7.039245
5.182587	290.383457	7.044250
5.446104	290.820092	7.049254
5.216496	293.153180	7.054259
5.514951	289.724494	7.059264
5.182794	292.241331	7.064269
5.474061	284.052242	7.069274
5.324372	289.530287	7.074278
5.306205	279.019991	7.079283
5.258484	284.614937	7.084288
4.938487	293.561890	7.089293
5.085747	288.916681	7.094298
5.122933	284.886680	7.099302
5.194828	289.703573	7.104307
5.260650	284.520622	7.109312
5.563956	304.288221	7.114317
5.505856	299.678350	7.119322
5.331694	302.069191	7.124326
5.469343	288.693375	7.129331
5.440102	290.441402	7.134336
5.455620	297.494451	7.139341
5.787802	290.903000	7.144346
5.584022	290.387777	7.149350
5.994408	295.749597	7.154355
5.478453	293.448277	7.159360
5.231501	293.053715	7.164365
5.554514	283.730173	7.169370
5.329965	280.459366	7.174374
5.048130	269.199435	7.179379
5.040935	274.588710	7.184384
5.136782	285.903470	7.189389
5.264998	287.952699	7.194394
5.342813	289.747228	7.199398
5.350306	288.983764	7.204403
5.509889	291.945583	7.209408
5.265883	291.465137	7.214413
5.606943	287.975992	7.219418
5.318077	279.596222	7.224422
5.156980	279.292615	7.229427
5.175413	283.311112	7.234432
4.808213	293.774596	7.239437
5.398208	293.407092	7.244442
5.368960	288.501632	7.249446
5.125998	287.869160	7.254451
5.204431	291.223350	7.259456
5.214961	294.490102	7.264461
5.211181	286.600345	7.269466
5.017369	297.327735	7.274470
5.420121	287.207072	7.279475
5.476549	283.180384	7.284480
5.079131	286.779976	7.289485
5.270435	281.343244	7.294490
4.951706	295.279322	7.299494
5.375858	288.157761	7.304499
5.471289	292.993114	7.309504
4.904698	296.498989	7.314509
5.401637	290.875159	7.319514
5.517307	295.441582	7.324518
5.458535	285.080016	7.329523
5.363072	288.110269	7.334528
5.333765	293.215107	7.339533
5.604389	282.877863	7.344538
5.347761	283.775651	7.349542
5.321508	294.597011	7.354547
5.499349	292.867205	7.359552
5.677304	299.723959	7.364557
5.536618	287.625639	7.369562
4.967398	294.238785	7.374566
5.104230	287.443821	7.379571
5.499430	291.352667	7.384576
5.338239	297.256467	7.389581
5.433633	287.974913	7.394586
5.184851	294.037971	7.399590
5.528002	288.944447	7.404595
5.446942	280.155624	7.409600
5.038191	280.403356	7.414605
4.885265	274.508024	7.419610
5.217336	289.209012	7.424614
5.323621	286.743760	7.429619
5.154871	290.994071	7.434624
5.183820	295.267192	7.439629
5.448853	288.157906	7.444634
5.357353	291.216013	7.449638
5.402358	291.114235	7.454643
5.477958	293.253967	7.459648
5.481232	292.756924	7.464653
5.200020	293.367494	7.469658
5.280319	295.784906	7.474662
5.444848	291.649527	7.479667
5.412766	285.532774	7.484672
5.031887	286.586074	7.489677
5.385050	292.861707	7.494682
5.083190	298.645176	7.499686
5.116598	292.926290	7.504691
5.416964	300.080246	7.509696
5.033288	301.997704	7.514701
5.519036	296.609748	7.519706
5.234261	294.455708	7.524710
5.165459	294.049053	7.529715
5.136060	289.232203	7.534720
5.226714	295.020611	7.539725
5.494714	289.717395	7.544730
5.281507	288.273490	7.549734
5.419475	289.742214	7.554739
5.592108	292.407754	7.559744
5.305381	298.457776	7.564749
5.325025	285.432651	7.569754
5.020767	289.992100	7.574758
5.131772	295.071790	7.579763
5.486421	291.495092	7.584768
5.211769	300.058450	7.589773
5.501696	292.397923	7.594778
5.427530	295.409022	7.599782
5.491817	288.995589	7.604787
5.429855	291.463764	7.609792
5.136690	277.279082	7.614797
5.343412	277.560097	7.619802
5.112202	295.351797	7.624806
5.007903	292.403838	7.629811
5.205240	290.598210	7.634816
5.474781	303.284170	7.639821
5.507403	293.329066	7.644826
5.680952	299.322790	7.649830
5.224905	284.287247	7.654835
5.255175	279.467379	7.659840
5.344946	288.312160	7.664845
5.311365	278.528791	7.669850
5.358727	285.538881	7.674854
5.024328	272.543927	7.679859
5.163999	277.055964	7.684864
5.062387	291.954620	7.689869
5.585648	284.001269	7.694874
5.349499	290.815333	7.699878
5.083452	291.198896	7.704883
5.324346	293.448774	7.709888
5.145852	297.191240	7.714893
5.661343	292.953415	7.719898
5.298986	296.095090	7.724902
5.463776	286.707750	7.729907
5.823518	291.868692	7.734912
4.975260	277.726689	7.739917
5.309735	262.678038	7.744922
5.066735	269.433054	7.749926
4.943009	285.556398	7.754931
5.258508	283.301980	7.759936
5.239874	298.668539	7.764941
5.456256	297.046591	7.769946
5.741300	300.014065	7.774950
5.357442	294.983827	7.779955
5.157573	279.765778	7.784960
5.050908	281.332943	7.789965
5.163584	289.737531	7.794970
5.400161	296.964756	7.799974
5.398314	289.077859	7.804979
5.495500	282.877576	7.809984
5.274779	286.788010	7.814989
5.396177	285.057557	7.819994
5.053713	288.408090	7.824998
5.448246	295.154977	7.830003
5.172727	281.369330	7.835008
4.796239	285.038410	7.840013
5.205433	287.834566	7.845018
5.376506	296.628648	7.850022
5.360765	291.588191	7.855027
5.765115	285.798532	7.860032
5.537654	298.027676	7.865037
5.517564	278.462861	7.870042
4.961060	272.760479	7.875046
5.156233	265.393225	7.880051
5.657838	277.745409	7.885056
5.062976	275.652611	7.890061
5.274981	271.389574	7.895066
5.327939	280.752656	7.900070
5.157094	283.820030	7.905075
5.339767	290.486212	7.910080
5.425226	288.172922	7.915085
5.858388	281.094245	7.920090
5.687564	272.075878	7.925094
5.281625	271.646115	7.930099
5.312643	266.190208	7.935104
5.011548	274.745042	7.940109
5.372507	264.997941	7.945114
5.161335	271.956783	7.950118
5.201999	268.280586	7.955123
5.232708	264.517363	7.960128
4.840034	273.854495	7.965146
5.141946	265.438374	7.970163
5.371749	281.783972	7.975181
5.595083	281.042283	7.980198
5.480112	271.249306	7.985216
5.321784	269.674345	7.990234
5.326471	261.415246	7.995251
5.123185	269.544895	8.000269
5.235007	265.560807	8.005286
5.038209	268.649734	8.010304
4.889872	287.629664	8.015322
5.313617	281.116290	8.020339
5.254659	292.483211	8.025357
5.305985	282.954500	8.030374
5.578098	284.811807	8.035392
5.448663	292.794199	8.040410
5.639650	280.179386	8.045427
5.506127	288.616843	8.050445
5.442065	291.962682	8.055462
5.786820	288.156682	8.060480
5.079787	278.614254	8.065498
5.349289	281.617500	8.070515
5.749410	293.830812	8.075533
5.421242	284.494101	8.080550
5.502274	273.673201	8.085568
5.031362	277.234258	8.090586
5.440275	285.804470	8.095603
5.361314	286.776373	8.100621
5.227663	290.751640	8.105638
5.526624	288.454946	8.110656
5.378744	302.016420	8.115674
5.436433	291.555765	8.120691
5.640843	290.914868	8.125709
5.588551	287.663374	8.130726
5.833932	284.649256	8.135744
5.305187	291.491876	8.140762
5.383091	286.714696	8.145779
5.701396	292.484190	8.150797
5.546424	290.416406	8.155814
5.582505	283.282132	8.160832
5.233656	282.708987	8.165850
5.779629	288.890924	8.170867
5.338323	290.288822	8.175885
5.388493	283.928651	8.180902
5.543326	291.721340	8.185920
5.273061	289.898833	8.190938
5.479658	291.747470	8.195955
5.899241	290.987655	8.200973
5.376271	287.996095	8.205990
5.761417	289.838848	8.211008
5.229939	295.501652	8.216026
4.991989	285.027363	8.221043
5.379617	289.195504	8.226061
5.451844	299.418433	8.231078
5.819126	294.523328	8.236096
5.602189	299.713982	8.241114
5.522981	293.888465	8.246131
5.518198	294.274403	8.251149
5.628534	299.483206	8.256166
5.556450	296.351573	8.261184
5.241860	306.186998	8.266202
5.252071	293.527918	8.271219
5.274257	297.668114	8.276237
5.418192	306.238828	8.281254
5.710356	308.528487	8.286272
5.505505	316.140861	8.291290
5.790476	310.513894	8.296307
6.261976	310.796805	8.301325
5.685171	300.517607	8.306342
5.908743	290.507478	8.311360
5.223869	299.056572	8.316378
5.415264	299.995584	8.321395
5.818968	296.678953	8.326413
5.585845	295.207224	8.331430
5.454614	292.842236	8.336448
5.358212	304.675769	8.341466
5.625241	308.764983	8.346483
6.047803	312.987615	8.351501
5.824948	318.002480	8.356518
5.747745	298.730036	8.361536
5.506777	312.091513	8.366554
5.865703	318.548914	8.371571
6.124109	316.507875	8.376589
5.447504	304.871563	8.381606
5.381321	306.024499	8.386624
5.507725	314.698947	8.391642
5.754150	322.464675	8.396659
5.906474	318.117630	8.401677
5.846914	324.896217	8.406694
6.167065	321.829354	8.411712
5.948488	309.925619	8.416730
5.842017	294.712892	8.421747
5.591731	291.751189	8.426765
5.503689	299.948000	8.431782
5.934012	304.945726	8.436800
5.928667	314.821063	8.441818
6.177624	303.797112	8.446835
5.569277	302.772330	8.451853
5.571729	301.986355	8.456870
5.744515	310.975419	8.461888
5.421259	317.123148	8.466906
5.754227	322.091952	8.471923
6.008186	322.295341	8.476941
6.065858	329.456342	8.481958
6.329836	315.416296	8.486976
5.984860	316.101683	8.491994
5.777036	295.559010	8.497011
5.878348	298.011112	8.502029
5.444800	302.121730	8.507046
6.109450	302.579502	8.512064
5.991988	308.922197	8.517082
5.705322	295.290327	8.522099
5.966551	302.189054	8.527117
5.666900	313.240258	8.532134
5.773874	315.091884	8.537152
5.792240	315.505752	8.542170
6.103942	317.110711	8.547187
6.105154	312.156195	8.552205
5.894165	307.594683	8.557223
6.235002	318.703325	8.562240
6.012565	303.366752	8.567258
5.726694	291.577712	8.572275
5.781607	304.899135	8.577293
5.844974	309.250628	8.582311
5.937927	316.838432	8.587328
6.107626	312.056330	8.592346
6.370853	316.032534	8.597363
6.153208	306.766855	8.602381
6.021057	297.661351	8.607399
6.215846	288.810733	8.612416
5.649285	301.368011	8.617434
5.621675	292.934081	8.622451
6.347914	300.397408	8.627469
5.983556	305.746859	8.632487
5.898031	304.192045	8.637504
6.261078	303.478957	8.642522
6.016158	297.505837	8.647539
6.090998	293.492823	8.652557
5.919674	294.532846	8.657575
6.122042	288.110959	8.662592
6.089571	290.255825	8.667610
5.895705	284.905857	8.672627
6.120371	288.149655	8.677645
5.525939	294.680683	8.682663
6.292700	310.105905	8.687680
6.237887	316.186327	8.692698
6.534773	315.682416	8.697715
6.192390	295.526892	8.702733
5.869558	291.601433	8.707751
5.764972	288.061492	8.712768
5.735659	301.263569	8.717786
5.902967	306.624390	8.722803
6.131294	312.840325	8.727821
5.959094	326.355136	8.732839
5.997965	324.578862	8.737856
5.937498	321.375978	8.742874
5.647439	315.176400	8.747891
5.747698	315.444896	8.752909
6.336229	320.155911	8.757927
6.221095	319.268441	8.762944
6.257437	320.190723	8.767962
6.146870	315.528270	8.772979
6.221682	313.932554	8.777997
6.009883	319.570524	8.783015
5.960155	314.620834	8.788032
6.153088	322.779943	8.793050
5.826014	314.042637	8.798067
6.127054	323.459728	8.803085
6.354271	337.259097	8.808103
6.450972	339.497337	8.813120
6.530137	327.477513	8.818138
6.148764	320.531706	8.823155
5.932169	319.675911	8.828173
5.833601	327.691351	8.833191
5.937743	328.988011	8.838208
6.643612	330.868878	8.843226
6.546453	342.715178	8.848243
6.792600	332.379602	8.853261
6.155126	332.340818	8.858279
5.993241	318.790363	8.863296
6.176536	321.775566	8.868314
6.562764	333.681819	8.873331
6.270501	316.232360	8.878349
6.652158	322.051897	8.883367
6.198629	326.017331	8.888384
6.131453	311.997615	8.893402
6.148557	313.219551	8.898419
6.419626	323.386093	8.903437
6.701391	325.674228	8.908455
6.567355	315.833722	8.913472
6.437308	316.245598	8.918490
6.140418	317.914355	8.923507
6.411175	309.831292	8.928525
6.433774	306.713223	8.933543
6.581913	307.949341	8.938560
6.362915	314.901226	8.943578
6.262252	318.956536	8.948595
6.250789	310.611584	8.953613
6.156650	317.061078	8.958631
6.165352	315.999574	8.963648
6.558504	325.638914	8.968666
6.167601	332.390527	8.973683
6.766603	325.600374	8.978701
6.482190	323.546555	8.983719
6.296417	326.245609	8.988736
6.481039	323.575514	8.993754
6.172142	331.671246	8.998771
6.859729	330.654848	9.003789
6.785320	329.385463	9.008807
6.431654	315.281246	9.013824
6.444479	309.188845	9.018842
6.022599	315.699157	9.023859
6.309489	316.528535	9.028877
6.442940	327.622340	9.033895
6.584453	340.822926	9.038912
6.706149	330.390088	9.043930
6.389902	333.668153	9.048947
6.765482	327.623048	9.053965
6.667149	325.947165	9.058983
6.391589	320.770929	9.064000
6.381245	316.193756	9.069018
6.361184	326.762514	9.074035
6.663397	329.546053	9.079053
6.559611	333.412510	9.084071
6.662127	335.173320	9.089088
6.836269	332.444906	9.094106
6.290690	321.908344	9.099123
6.299622	326.820624	9.104141
6.466961	336.624737	9.109159
6.579455	334.085859	9.114176
7.180624	336.904608	9.119194
6.352106	334.405874	9.124211
6.739510	337.311764	9.129229
6.688340	336.105007	9.134247
6.548724	335.710512	9.139264
6.526282	325.303417	9.144282
6.864214	332.786574	9.149299
6.555671	332.453260	9.154317
6.596272	324.213751	9.159335
6.778753	334.832828	9.164352
6.755633	316.129392	9.169370
6.213098	324.813984	9.174387
6.990131	325.920010	9.179405
6.848562	329.644066	9.184423
6.480440	325.362785	9.189440
6.910148	325.803720	9.194458
6.315550	337.166234	9.199475
6.803945	330.257712	9.204493
6.987082	341.280625	9.209511
6.847853	336.250280	9.214528
6.623151	322.223679	9.219546
6.307465	332.318061	9.224563
6.722508	328.415835	9.229581
6.903603	337.946400	9.234599
6.672851	337.092822	9.239616
6.684483	338.107338	9.244634
6.927125	342.074150	9.249651
7.089344	336.813539	9.254669
6.734524	331.447751	9.259687
6.469795	335.708648	9.264704
6.695085	329.769140	9.269722
6.649428	337.268219	9.274739
6.805535	333.292956	9.279757
6.594704	335.491018	9.284775
6.667708	342.659089	9.289792
6.896717	334.213334	9.294810
7.056976	339.521622	9.299827
7.161160	336.229823	9.304845
6.950033	332.157467	9.309863
6.662953	336.724817	9.314880
6.899932	339.578538	9.319898
7.008247	346.040502	9.324915
6.942374	333.061962	9.329933
7.179893	339.983354	9.334951
6.784727	331.881545	9.339968
6.786175	326.239036	9.344986
6.816843	342.369742	9.350003
6.911681	341.686053	9.355021
7.177828	344.112334	9.360039
6.751447	336.671809	9.365056
6.861627	335.758502	9.370074
6.604068	340.049834	9.375091
6.872935	339.821707	9.380109
6.845645	341.041133	9.385127
7.050575	348.586160	9.390144
7.296689	346.468150	9.395162
7.111710	343.073335	9.400179
7.251679	335.342106	9.405197
6.897077	327.824067	9.410215
6.981843	330.127290	9.415232
7.233434	323.274809	9.420250
7.046885	321.947256	9.425267
6.703183	323.301462	9.430285
6.863295	326.542758	9.435303
6.608777	331.613080	9.440320
7.069353	331.228686	9.445338
7.120060	341.167838	9.450355
7.038767	334.578944	9.455373
7.147491	341.296458	9.460391
6.882756	355.005666	9.465408
7.128569	333.757567	9.470426
7.280712	342.427996	9.475443
7.069095	341.265313	9.480461
7.027873	336.677194	9.485479
6.945353	340.906388	9.490496
7.671677	338.129325	9.495514
7.202750	334.065804	9.500531
6.817162	324.823273	9.505549
7.113066	325.856363	9.510567
7.191634	331.332079	9.515584
7.084406	326.855289	9.520602
7.297402	334.566301	9.525619
6.915209	320.677984	9.530637
7.123677	331.441308	9.535655
6.994057	343.008677	9.540672
7.227162	332.378504	9.545690
7.491211	342.217960	9.550707
6.897302	320.890010	9.555725
7.310146	323.103959	9.560743
6.869478	333.085383	9.565760
7.262238	326.352790	9.570778
7.167235	337.318296	9.575795
7.204349	333.693030	9.580813
7.189840	329.081793	9.585831
7.234517	340.571360	9.590848
7.180844	324.640292	9.595866
7.222056	330.620469	9.600883
6.962208	333.482606	9.605901
7.096699	328.128514	9.610919
6.532428	339.319023	9.615936
7.011353	333.548052	9.620954
6.976110	334.803437	9.625971
7.152843	343.406899	9.630989
7.433219	334.747972	9.636007
7.125449	335.440154	9.641024
7.389851	337.923511	9.646042
7.448870	336.172481	9.651059
6.891785	341.138737	9.656077
7.294281	344.316813	9.661095
7.165637	353.075421	9.666112
7.342133	347.354987	9.671130
7.795393	358.174645	9.676147
7.395920	344.743445	9.681165
7.288666	332.169013	9.686183
7.137885	329.437861	9.691200
7.041659	337.273061	9.696218
7.592323	351.024919	9.701235
7.791316	349.854704	9.706253
7.487297	340.684590	9.711271
7.106240	342.754693	9.716288
7.105941	338.677704	9.721306
7.662989	349.099249	9.726323
7.586025	358.086444	9.731341
7.161950	338.098303	9.736359
7.267774	352.759289	9.741376
7.752186	353.819648	9.746394
7.537423	348.867404	9.751411
7.259041	337.967081	9.756429
7.218197	346.992791	9.761447
7.300742	366.820239	9.766464
7.407247	365.749719	9.771482
7.631890	361.321906	9.776499
7.599848	371.185679	9.781517
7.757153	359.882569	9.786535
7.756372	362.773546	9.791552
7.431336	345.666857	9.796570
7.405258	348.321959	9.801587
7.613482	364.506915	9.806605
7.520380	359.014907	9.811623
7.337850	367.665203	9.816640
7.396471	361.991635	9.821658
7.625244	367.532189	9.826675
7.586265	360.602146	9.831693
7.453944	360.629378	9.836711
7.507342	362.183296	9.841728
7.324459	359.315160	9.846746
7.730816	360.779062	9.851763
7.668204	369.801884	9.856781
7.888408	360.309786	9.861799
7.625422	370.519007	9.866816
7.600029	364.085442	9.871834
7.546564	362.749658	9.876851
7.570564	367.766885	9.881869
7.796611	364.818898	9.886887
7.775420	370.783619	9.891904
7.724179	362.425941	9.896922
7.720621	365.080673	9.901939
7.534729	365.226749	9.906957
7.666436	368.229510	9.911975
7.575637	367.783185	9.916992
7.678448	360.805680	9.922010
7.829789	365.717749	9.927027
7.555850	365.877621	9.932045
7.965510	371.244671	9.937063
7.652948	373.155725	9.942080
7.804582	366.546102	9.947098
7.883627	365.063326	9.952115
7.583547	374.609342	9.957133
8.082794	369.163374	9.962151
7.949519	366.808163	9.967168
8.002579	361.962273	9.972186
7.659648	351.905173	9.977203
7.717262	341.166794	9.982221
8.010175	341.749082	9.987239
7.333923	346.768723	9.992256
7.502044	352.653285	9.997274
7.750931	364.719931	10.002291
7.578998	374.697141	10.007309
8.066107	364.787688	10.012327
7.906878	374.447332	10.017344
7.844873	363.383706	10.022362
7.902463	361.487732	10.027379
7.561508	374.287419	10.032397
7.875358	372.029406	10.037415
7.803143	374.521330	10.042432
7.660708	369.254796	10.047450
7.757874	366.273354	10.052467
7.617539	374.178597	10.057485
7.656231	366.753551	10.062503
7.466024	370.384253	10.067520
7.489981	365.192633	10.072538
7.887276	371.697690	10.077555
7.841139	388.089776	10.082573
8.081401	382.021674	10.087591
8.037121	387.194769	10.092608
7.780144	375.091883	10.097626
7.968021	384.356326	10.102643
8.191076	381.175280	10.107661
8.339343	371.647112	10.112679
8.211588	375.410038	10.117696
7.870520	371.705165	10.122714
7.827163	370.743331	10.127731
8.137949	369.467237	10.132749
8.137047	366.381243	10.137767
7.494569	377.416774	10.142784
7.576529	372.676804	10.147802
8.138621	379.660963	10.152819
8.119088	395.821674	10.157837
8.088288	396.767103	10.162855
8.204593	388.108611	10.167872
8.491823	386.334442	10.172890
8.276098	373.224720	10.177907
7.933816	376.882406	10.182925
8.114395	362.568216	10.187943
7.701275	363.560922	10.192960
7.828331	379.297870	10.197978
7.891603	385.984653	10.202995
8.048021	392.110899	10.208013
8.213325	384.754370	10.213031
8.073284	384.350473	10.218048
8.042992	386.854764	10.223066
8.316988	382.807371	10.228083
8.229225	398.379181	10.233101
8.427113	389.338682	10.238119
8.091647	393.733750	10.243136
8.073464	387.248556	10.248154
8.825942	382.999963	10.253171
8.232375	391.219219	10.258189
8.337227	394.314553	10.263207
8.225590	398.011844	10.268224
8.228828	398.440707	10.273242
8.369701	394.051258	10.278259
8.233343	382.204018	10.283277
8.135336	377.514335	10.288295
8.044947	388.043656	10.293312
8.633949	396.115497	10.298330
8.385241	380.984941	10.303347
8.060869	382.064728	10.308365
8.189977	392.625931	10.313383
8.139995	396.976270	10.318400
8.328652	392.030232	10.323418
8.133649	389.378582	10.328435
8.146021	398.777827	10.333453
8.248326	398.604198	10.338471
8.305331	395.733184	10.343488
8.371454	389.853307	10.348506
8.406889	391.731929	10.353523
8.304253	400.376034	10.358541
8.255227	394.236491	10.363559
8.425539	392.092483	10.368576
8.071431	396.881786	10.373594
8.427511	385.446532	10.378611
8.080518	396.378974	10.383629
8.012785	394.411116	10.388647
8.332250	395.080762	10.393664
8.261503	394.423015	10.398682
8.713102	385.402726	10.403699
8.005647	392.342811	10.408717
8.368846	399.913555	10.413735
8.665847	407.762913	10.418752
8.699136	404.068805	10.423770
8.781127	392.834278	10.428787
8.742323	397.350120	10.433805
8.869011	397.952143	10.438823
8.586107	398.236494	10.443840
8.268457	397.882515	10.448858
8.779458	389.307346	10.453875
8.822972	394.760172	10.458893
8.635221	395.619741	10.463911
8.714265	393.281753	10.468928
8.703873	395.663009	10.473946
8.865673	386.738617	10.478963
8.587260	389.837198	10.483981
8.430936	389.827166	10.488999
8.513666	385.263794	10.494016
8.433852	385.582596	10.499034
8.550835	381.787018	10.504051
8.499867	389.397403	10.509069
8.659359	398.385439	10.514087
8.542535	393.581936	10.519104
8.540858	388.400638	10.524122
8.378859	383.869299	10.529139
8.458828	381.180879	10.534157
8.419608	384.169399	10.539175
8.515361	384.444914	10.544192
8.521139	389.660658	10.549210
8.597590	380.282591	10.554227
8.618705	382.491654	10.559245
8.545808	386.132380	10.564263
8.555221	387.724749	10.569280
8.738294	411.531681	10.574298
8.534173	408.029402	10.579315
8.715091	412.555003	10.584333
8.826444	410.155147	10.589351
8.389569	409.327549	10.594368
9.070214	413.844280	10.599386
9.338107	399.055639	10.604403
8.902847	401.430882	10.609421
8.358598	396.161025	10.614439
8.663190	398.051124	10.619456
8.848641	415.817573	10.624474
9.003448	404.363349	10.629491
8.958115	401.776608	10.634509
9.118821	404.260443	10.639527
8.806867	399.377061	10.644544
8.555351	388.358890	10.649562
8.937009	403.194447	10.654579
8.538435	417.129797	10.659597
8.766023	412.818273	10.664615
9.252123	409.220472	10.669632
8.792891	411.713080	10.674650
8.955072	403.527068	10.679667
8.343373	415.195262	10.684685
8.903473	413.728627	10.689703
9.300535	415.771494	10.694720
8.991802	413.453236	10.699738
9.207891	405.116767	10.704755
8.944983	410.876381	10.709773
8.567243	415.101356	10.714791
8.966109	411.820175	10.719808
9.082815	412.654132	10.724826
9.266509	408.412602	10.729843
9.272674	416.070850	10.734861
8.958029	410.992229	10.739879
8.967685	408.021336	10.744896
8.934799	418.289204	10.749914
8.962077	400.448774	10.754931
8.881179	408.297382	10.759949
9.122861	408.398557	10.764967
9.330305	402.982520	10.769984
9.011763	411.916076	10.775002
9.029536	409.227929	10.780019
9.219977	413.152444	10.785037
9.216745	406.147355	10.790055
9.322248	411.801910	10.795072
8.905112	408.168907	10.800090
9.073638	413.889327	10.805107
9.309836	409.945678	10.810125
9.161474	401.729429	10.815143
9.316396	398.839917	10.820160
9.076492	395.052917	10.825178
9.061225	388.311649	10.830195
9.120981	389.590022	10.835213
9.062553	399.896595	10.840231
9.299526	408.342330	10.845248
9.070441	412.301019	10.850266
9.344094	391.998372	10.855283
9.766310	409.150214	10.860301
9.099120	406.114960	10.865319
8.955547	393.255845	10.870336
8.877050	402.091826	10.875354
9.190393	404.068916	10.880371
9.185830	406.373521	10.885389
9.237056	407.555404	10.890407
9.594993	411.497856	10.895424
9.365715	419.701072	10.900442
9.356598	404.091152	10.905459
9.477265	412.018632	10.910477
9.478860	406.082589	10.915495
9.361987	394.942334	10.920512
8.791295	398.373884	10.925530
9.064535	404.633307	10.930547
9.659386	401.870523	10.935565
9.413505	413.683368	10.940583
9.276752	409.918073	10.945600
9.352882	411.263309	10.950618
9.263804	412.306231	10.955635
9.385137	411.179737	10.960653
9.242378	412.562425	10.965671
9.474079	408.177675	10.970688
9.398780	411.474806	10.975706
9.411677	408.885251	10.980723
9.687804	409.801526	10.985741
9.316684	407.003901	10.990759
9.469879	407.137874	10.995776
9.692089	408.438132	11.000794
9.638882	413.448533	11.005811
9.152727	409.946263	11.010829
9.539315	414.064104	11.015847
9.495493	405.667374	11.020864
9.380692	407.541135	11.025882
9.326460	406.451617	11.030899
9.633284	407.741773	11.035917
9.452228	405.075312	11.040935
9.790793	403.365681	11.045952
9.706144	403.701019	11.050970
9.800254	405.762950	11.055987
9.869099	398.087019	11.061005
9.556267	403.106538	11.066023
9.675060	405.559072	11.071040
9.510923	411.520957	11.076058
9.698711	412.602550	11.081075
9.519244	414.909315	11.086093
9.433886	402.722717	11.091111
9.647337	411.244720	11.096128
9.612932	414.039990	11.101146
9.399336	413.183720	11.106163
9.737093	409.874246	11.111181
9.653532	410.607039	11.116199
9.808543	409.254366	11.121216
9.418973	413.544308	11.126234
9.417341	414.491480	11.131251
9.585197	411.255962	11.136269
9.155656	415.703644	11.141287
9.717146	407.385639	11.146304
9.822947	412.872893	11.151322
9.502438	417.376075	11.156339
9.821865	419.626763	11.161357
9.928855	433.031640	11.166375
10.013618	430.408732	11.171392
9.676393	421.373166	11.176410
9.755569	411.265674	11.181427
9.928128	421.144754	11.186445
9.961771	430.468101	11.191463
9.886810	412.069329	11.196480
9.685204	417.260771	11.201498
9.911779	419.481827	11.206515
9.942653	415.683955	11.211533
9.783764	412.221924	11.216551
9.977315	415.934517	11.221568
9.695728	414.012786	11.226586
9.711951	424.932518	11.231603
10.446735	424.770243	11.236621
9.774684	426.949063	11.241639
9.953770	422.916532	11.246656
9.933996	424.974218	11.251674
10.104748	433.963664	11.256691
9.795847	418.252380	11.261709
10.102777	426.838639	11.266727
10.026733	419.399991	11.271744
9.828994	428.008518	11.276762
9.788121	432.373218	11.281779
10.304733	430.383227	11.286797
9.885355	430.802569	11.291815
10.221943	426.398225	11.296832
9.966500	428.593821	11.301850
9.878179	429.194819	11.306867
9.961402	426.865639	11.311885
9.893293	427.791669	11.316903
10.208068	431.841873	11.321920
10.098688	430.379146	11.326938
10.079811	429.571261	11.331955
10.065693	433.827629	11.336973
10.186165	434.853498	11.341991
10.471541	426.067513	11.347008
10.009757	429.368398	11.352026
10.054845	427.812043	11.357043
10.371783	427.749950	11.362061
10.397896	428.970482	11.367079
10.493396	423.963293	11.372096
10.045284	423.512991	11.377114
9.700218	426.296978	11.382131
9.866549	424.396583	11.387149
9.812517	436.848406	11.392167
9.959396	434.389332	11.397184
10.226042	431.532802	11.402202
9.920354	439.422956	11.407219
10.351312	427.938073	11.412237
10.080579	431.761282	11.417255
10.231874	426.903139	11.422272
10.313010	433.464066	11.427290
10.343678	428.792077	11.432307
10.200094	423.459436	11.437325
10.111283	430.188999	11.442343
10.267598	432.664059	11.447360
10.374850	422.167159	11.452378
10.264591	428.253151	11.457395
10.545861	428.322877	11.462413
10.290727	423.036115	11.467431
10.204102	421.961139	11.472448
10.396677	432.345166	11.477466
10.467305	440.621322	11.482483
10.915370	434.602693	11.487501
10.758032	421.389114	11.492519
10.426481	415.372724	11.497536
10.553435	424.668824	11.502554
10.210626	436.234943	11.507571
10.777966	425.230460	11.512589
10.404477	426.523069	11.517607
10.544761	425.456720	11.522624
10.592686	421.444740	11.527642
10.363190	427.722980	11.532659
10.351159	410.005462	11.537677
10.486380	424.213783	11.542695
10.434253	426.207112	11.547712
10.588749	418.164307	11.552730
10.320588	424.347620	11.557747
10.576969	412.211611	11.562765
10.376064	425.437509	11.567783
10.601502	433.578954	11.572800
10.512507	435.098385	11.577818
10.551951	435.180754	11.582835
11.408009	442.983559	11.587853
10.817176	434.782974	11.592871
10.475924	420.285414	11.597888
10.894541	422.763556	11.602906
10.448947	427.570357	11.607923
10.698937	418.351269	11.612941
10.492648	415.534128	11.617959
10.606748	423.942318	11.622976
10.465413	422.904315	11.627994
10.324218	429.092983	11.633011
11.040178	440.632069	11.638029
10.967760	452.534525	11.643047
10.781467	431.174135	11.648064
10.857386	432.513094	11.653082
10.697501	435.545774	11.658099
10.695152	419.268914	11.663117
10.566204	418.336266	11.668135
10.822376	432.355232	11.673152
10.770272	440.735823	11.678170
11.154364	442.559822	11.683187
10.952526	426.765485	11.688205
10.548203	426.453487	11.693223
10.884299	435.262395	11.698240
10.895519	444.179013	11.703258
10.974227	444.229985	11.708275
10.908917	441.703171	11.713293
10.575301	442.389939	11.718311
10.863394	447.473106	11.723328
10.992171	433.820218	11.728346
10.903295	449.471141	11.733363
10.943457	451.762434	11.738381
10.713003	448.589316	11.743399
11.230233	444.080927	11.748416
11.283182	443.318591	11.753434
10.925414	447.269048	11.758451
10.982772	431.468809	11.763469
10.819375	433.804617	11.768487
11.055431	441.944402	11.773504
11.097821	440.423181	11.778522
10.716358	444.364727	11.783539
11.128916	443.732238	11.788557
10.998803	446.630869	11.793575
10.967851	444.019778	11.798592
11.137763	436.889721	11.803610
10.656854	450.986318	11.808627
10.938026	445.675481	11.813645
10.927039	452.250849	11.818663
11.058813	452.763715	11.823680
11.123085	447.584689	11.828698
10.947155	447.962732	11.833715
11.180529	444.095257	11.838733
11.185837	442.743946	11.843751
10.985675	445.044491	11.848768
11.247925	445.192935	11.853786
11.051737	449.411562	11.858803
11.139880	443.032763	11.863821
11.115406	445.267911	11.868839
11.254285	440.793556	11.873856
11.333997	445.915683	11.878874
10.999330	456.423358	11.883891
11.368738	450.511722	11.888909
11.478515	454.698190	11.893927
10.996030	453.713637	11.898944
11.196872	449.494656	11.903962
11.274984	437.225617	11.908979
11.232816	447.397128	11.913997
11.215550	442.508587	11.919015
11.189714	447.252781	11.924032
11.532531	448.196478	11.929050
11.276775	458.735971	11.934067
11.557454	461.705940	11.939085
11.307754	449.409361	11.944103
11.185699	446.916684	11.949120
11.575175	449.768620	11.954138
11.763459	459.086687	11.959155
11.786759	446.845164	11.964173
11.688267	444.837939	11.969191
10.979540	447.439069	11.974208
11.292940	433.867707	11.979226
11.230567	439.191972	11.984243
11.463043	450.204067	11.989261
11.582883	451.851723	11.994279
11.552360	461.895186	11.999296
11.563600	460.047490	12.004314
11.575872	455.277392	12.009331
11.528673	455.991867	12.014349
11.374773	454.990544	12.019367
11.779725	462.065628	12.024384
11.724144	456.381522	12.029402
11.264102	448.902042	12.034419
11.616522	449.512879	12.039437
11.814136	453.038653	12.044455
11.519437	452.242425	12.049472
11.713578	449.630779	12.054490
11.766304	455.318863	12.059507
11.596827	448.794235	12.064525
11.596802	447.172364	12.069543
11.646662	453.444713	12.074560
11.521863	463.300980	12.079578
11.628944	460.441044	12.084595
11.926039	455.673657	12.089613
11.927894	460.798519	12.094631
11.407174	458.642855	12.099648
11.989930	459.921340	12.104666
11.687703	451.230564	12.109683
11.478269	446.122825	12.114701
11.800970	459.418186	12.119719
11.600707	462.779086	12.124736
11.800289	458.935837	12.129754
11.755789	463.903863	12.134771
12.053462	468.919264	12.139789
11.872155	461.818980	12.144807
11.489410	471.968128	12.149824
11.625794	469.267699	12.154842
11.814611	474.729342	12.159859
11.743241	467.378303	12.164877
12.055271	463.410138	12.169895
11.992126	469.637084	12.174912
12.102326	463.112812	12.179930
11.949115	468.665910	12.184947
12.087239	465.703281	12.189965
11.978931	462.309054	12.194983
11.950678	467.599580	12.200000
11.900617	457.736371	12.205018
12.113705	458.410064	12.210035
11.900031	460.709572	12.215053
11.916530	457.996371	12.220071
11.953423	464.681006	12.225088
12.069579	459.755776	12.230106
11.989383	459.762218	12.235123
12.035255	466.719998	12.240141
12.324744	465.153748	12.245159
12.059404	473.627724	12.250176
12.191809	465.588359	12.255194
11.879187	462.030486	12.260211
11.959767	469.705500	12.265229
12.142867	464.511007	12.270247
11.855416	463.587413	12.275264
12.365026	467.676524	12.280282
12.316612	461.596822	12.285299
11.956066	457.374281	12.290317
12.302738	459.832142	12.295335
11.973836	470.604007	12.300352
11.914048	455.532149	12.305370
12.138291	458.561452	12.310387
12.010984	457.991458	12.315405
12.314814	463.346716	12.320423
12.201274	466.125990	12.325440
12.229970	460.251955	12.330458
12.033423	460.039944	12.335475
11.847850	469.407125	12.340493
12.431305	474.008526	12.345511
12.411021	477.514796	12.350528
12.746251	477.336230	12.355546
12.432511	477.085777	12.360563
11.720871	465.776737	12.365581
12.671449	479.507061	12.370599
12.543366	486.280668	12.375616
12.248661	471.337121	12.380634
12.350232	479.497994	12.385651
11.934774	482.791630	12.390669
12.665300	485.154640	12.395687
12.399147	486.244245	12.400704
12.894374	486.715945	12.405722
12.778850	479.523296	12.410739
11.955080	473.063306	12.415757
12.257500	476.733607	12.420775
12.389492	487.752002	12.425792
12.350103	487.000976	12.430810
12.470169	484.981593	12.435827
12.558847	487.612424	12.440845
12.569386	484.808635	12.445863
12.632444	485.919242	12.450880
12.587882	486.721667	12.455898
12.489801	492.042076	12.460915
12.567200	481.843306	12.465933
12.637523	480.649061	12.470951
12.524930	490.759048	12.475968
12.773131	490.269073	12.480986
12.660085	479.620465	12.486003
12.619455	492.076539	12.491021
12.559351	489.002954	12.496039
12.700373	492.042146	12.501056
12.733238	481.689409	12.506074
12.925428	487.699632	12.511091
12.930832	486.799578	12.516109
12.764529	480.359647	12.521127
12.861804	487.031674	12.526144
13.023059	477.914820	12.531162
12.910262	481.353536	12.536179
12.533805	487.288754	12.541197
12.835998	476.186929	12.546215
12.834112	483.003877	12.551232
12.903160	480.714780	12.556250
13.026037	476.504853	12.561267
12.602443	485.344453	12.566285
12.705970	487.234507	12.571303
12.688426	486.975514	12.576320
12.841841	477.667387	12.581338
12.881741	481.770137	12.586355
12.888487	482.046976	12.591373
12.848955	486.086434	12.596391
12.696935	479.177211	12.601408
12.914392	488.487567	12.606426
12.941690	478.331362	12.611443
12.980156	478.439131	12.616461
13.060062	479.957348	12.621479
12.954457	479.734244	12.626496
12.814610	483.439128	12.631514
12.961639	479.395828	12.636531
13.030576	485.693601	12.641549
12.996218	481.744991	12.646567
13.143773	479.651875	12.651584
13.149221	482.526117	12.656602
13.208317	492.634450	12.661619
13.192568	485.568176	12.666637
13.354090	477.420103	12.671655
13.251509	487.020440	12.676672
13.004876	487.460054	12.681690
13.264028	483.515948	12.686707
13.046800	483.269308	12.691725
13.113320	478.743166	12.696743
13.216311	483.849034	12.701760
13.135780	483.666182	12.706778
13.200934	482.087743	12.711795
13.067487	486.504829	12.716813
13.103968	481.143958	12.721831
13.182858	491.129270	12.726848
13.114694	477.794381	12.731866
13.242039	480.090952	12.736883
12.997029	495.728510	12.741901
13.357610	495.681669	12.746919
13.557849	509.403349	12.751936
13.429804	496.579597	12.756954
13.502015	499.118336	12.761971
13.381558	492.352485	12.766989
13.565230	481.941406	12.772007
13.266813	480.211651	12.777024
13.015242	474.226890	12.782042
13.287361	473.303983	12.787059
13.292085	500.357863	12.792077
13.538312	502.746262	12.797095
13.025714	504.713918	12.802112
13.586452	506.497624	12.807130
13.571189	501.678180	12.812147
13.646814	511.544096	12.817165
13.572788	501.567853	12.822183
13.702171	503.649516	12.827200
13.309890	508.842457	12.832218
13.730609	500.262446	12.837235
13.365352	502.238574	12.842253
13.354041	497.879254	12.847271
13.452039	502.676643	12.852288
13.315858	504.411754	12.857306
13.631843	504.763217	12.862323
13.391219	511.630205	12.867341
13.509187	510.374845	12.872359
13.518835	517.502421	12.877376
13.509140	505.619475	12.882394
13.621910	500.177218	12.887411
13.456518	511.431568	12.892429
13.688316	507.075181	12.897447
13.524862	515.526901	12.902464
13.731831	506.993001	12.907482
13.899069	503.713382	12.912499
13.599801	514.622639	12.917517
13.838312	496.625941	12.922535
13.799492	498.812851	12.927552
13.531089	502.897640	12.932570
14.114542	508.155451	12.937587
13.647472	505.928260	12.942605
13.733280	506.580872	12.947623
14.021890	504.847501	12.952640
14.260950	511.276417	12.957658
14.347228	509.915571	12.962675
14.188307	502.221633	12.967693
14.348046	501.073337	12.972711
14.372752	496.957681	12.977728
14.312895	494.890749	12.982746
14.611676	498.769906	12.987763
14.388689	483.657323	12.992781
13.918097	485.040889	12.997799
14.242479	477.179720	13.002816
13.957806	473.910953	13.007834
13.857123	471.351808	13.012851
13.652817	483.006708	13.017869
13.841501	476.085131	13.022887
13.999158	483.817501	13.027904
13.832560	492.121382	13.032922
14.079922	491.167639	13.037939
14.167491	505.670667	13.042957
14.308925	504.670405	13.047975
14.584328	500.184112	13.052992
13.767745	486.843404	13.058010
13.464392	480.614292	13.063027
13.893033	493.296639	13.068045
13.990986	494.752070	13.073063
14.229041	498.688079	13.078080
14.215627	508.186095	13.083098
14.156475	505.137605	13.088115
14.345778	506.414624	13.093133
14.221991	497.086803	13.098151
14.232113	500.907047	13.103168
14.160442	507.668668	13.108186
14.687836	506.440677	13.113203
14.276236	512.734856	13.118221
14.214859	509.418473	13.123239
14.025198	505.509969	13.128256
14.076977	507.089400	13.133274
13.991909	499.036756	13.138291
14.009677	505.364644	13.143309
14.156425	513.682555	13.148327
14.617288	528.411134	13.153344
14.359830	529.480445	13.158362
14.888136	527.501234	13.163379
14.771185	516.512392	13.168397
14.271242	504.744128	13.173415
14.416292	501.445896	13.178432
14.197889	502.474373	13.183450
14.646371	504.644893	13.188467
14.548049	529.319729	13.193485
14.776485	526.970939	13.198503
14.496684	521.249359	13.203520
14.719168	514.076321	13.208538
14.185737	513.734057	13.213555
14.614513	517.356168	13.218573
14.648462	526.499637	13.223591
14.935076	512.888230	13.228608
14.659185	520.152063	13.233626
15.030778	510.740307	13.238643
14.811249	506.940624	13.243661
14.573002	502.402267	13.248679
14.722808	487.445864	13.253696
13.979348	488.717551	13.258714
14.704083	499.886076	13.263731
14.592737	518.866767	13.268749
14.724927	518.123570	13.273767
14.772033	519.612217	13.278784
14.903340	522.993760	13.283802
15.138876	518.671498	13.288819
15.194523	520.234545	13.293837
14.796115	510.438509	13.298855
14.731910	506.128500	13.303872
14.735235	511.530855	13.308890
15.350809	517.970208	13.313907
14.763023	505.799144	13.318925
14.610999	504.257887	13.323943
15.156419	518.455662	13.328960
14.822754	525.233092	13.333978
14.731006	517.670632	13.338995
14.870635	520.280862	13.344013
14.722790	524.750705	13.349031
14.830688	520.044502	13.354048
14.881109	528.629975	13.359066
14.875016	523.484042	13.364083
14.962711	519.077648	13.369101
14.756328	515.367420	13.374119
15.173980	516.573949	13.379136
14.976272	525.327684	13.384154
15.169441	514.798334	13.389171
15.010964	519.083651	13.394189
15.313338	518.566252	13.399207
15.510076	514.843356	13.404224
14.810808	520.807073	13.409242
15.158387	521.892038	13.414259
15.235194	520.598946	13.419277
15.163401	525.460814	13.424295
15.252312	510.469752	13.429312
15.040759	521.605110	13.434330
15.204343	518.771026	13.439347
15.140855	523.536919	13.444365
14.941371	522.971920	13.449383
15.154472	517.621234	13.454400
14.909764	524.930675	13.459418
15.123333	536.229806	13.464435
15.489144	549.322821	13.469453
15.398130	545.869064	13.474471
15.785244	538.449317	13.479488
15.696962	531.889846	13.484506
15.323678	523.746651	13.489523
15.184495	514.752590	13.494541
15.119577	533.101177	13.499559
15.688928	544.480268	13.504576
15.501222	550.600526	13.509594
15.704821	538.731476	13.514611
15.302375	525.641429	13.519629
15.486296	532.536580	13.524647
15.629952	530.526119	13.529664
15.302935	532.584620	13.534682
15.459807	541.888717	13.539699
15.837512	544.493206	13.544717
15.723653	536.539730	13.549735
15.608615	520.435067	13.554752
15.185975	533.149836	13.559770
15.180255	534.337494	13.564787
15.315374	539.103831	13.569805
15.416857	547.870659	13.574823
15.842983	537.708736	13.579840
15.798492	546.731963	13.584858
15.767260	542.322106	13.589875
15.687973	532.785324	13.594893
15.449455	540.153762	13.599911
15.903709	534.004743	13.604928
15.635207	540.642582	13.609946
15.631366	539.144376	13.614963
15.953845	546.248196	13.619981
15.577313	537.950869	13.624999
16.002861	532.377546	13.630016
15.232654	535.013567	13.635034
15.778890	540.933621	13.640051
15.921574	546.443539	13.645069
15.860384	542.966176	13.650087
15.742183	542.839718	13.655104
15.831173	547.209344	13.660122
16.040495	556.066577	13.665139
15.982583	562.119167	13.670157
15.694471	550.068376	13.675175
16.149121	562.431119	13.680192
16.231560	563.816403	13.685210
16.236713	561.704564	13.690227
16.017638	541.766124	13.695245
15.945375	538.129551	13.700263
15.765305	535.412424	13.705280
16.016059	557.277609	13.710298
15.876022	555.567213	13.715315
16.041594	553.906763	13.720333
16.322405	554.266894	13.725351
16.251974	555.114400	13.730368
16.389954	556.948570	13.735386
16.276168	560.002451	13.740403
16.307168	561.531494	13.745421
16.166483	557.470139	13.750439
16.244699	546.283443	13.755456
16.020257	554.883593	13.760474
16.150245	561.976552	13.765491
16.313924	563.674154	13.770509
16.304363	568.469479	13.775527
16.573114	556.915255	13.780544
16.531062	562.561419	13.785562
16.428230	545.637471	13.790579
16.168088	547.350983	13.795597
15.956329	556.106935	13.800615
16.159569	549.460757	13.805632
16.290000	557.169024	13.810650
16.526013	557.258465	13.815667
16.579949	556.240351	13.820685
16.378398	562.167124	13.825703
16.712570	566.476250	13.830720
16.602272	570.703538	13.835738
16.578293	560.365974	13.840755
16.554244	561.963601	13.845773
16.272774	558.931000	13.850791
16.868083	558.938900	13.855808
16.453480	565.224101	13.860826
16.470709	568.557255	13.865843
16.683317	557.974341	13.870861
16.472548	562.820125	13.875879
16.914459	558.626463	13.880896
16.627903	557.185175	13.885914
16.497287	560.440507	13.890931
16.686152	561.739689	13.895949
16.954072	558.068747	13.900967
16.833147	562.745820	13.905984
16.318497	560.008528	13.911002
16.792597	565.217219	13.916019
16.609566	558.338070	13.921037
16.439029	559.718810	13.926055
17.048415	555.378989	13.931072
16.707345	556.369884	13.936090
17.138645	556.883161	13.941107
16.763851	554.329082	13.946125
16.809508	561.933869	13.951143
16.760455	554.342614	13.956160
16.749252	557.273125	13.961178
16.767717	557.276732	13.966195
17.090351	543.268341	13.971213
16.651233	552.684758	13.976231
16.665464	555.794320	13.981248
16.934786	551.678193	13.986266
16.857610	554.865192	13.991283
16.853692	549.444358	13.996301
16.620439	558.935821	14.001319
16.810203	550.073238	14.006336
16.887894	572.536754	14.011354
16.864757	580.247001	14.016371
17.403543	575.337572	14.021389
17.042008	577.578211	14.026407
17.192850	578.570929	14.031424
17.541909	574.985100	14.036442
17.413001	575.466230	14.041459
17.049122	566.737720	14.046477
16.711486	562.792429	14.051495
17.185712	572.040508	14.056512
17.214384	579.083077	14.061530
17.081671	580.953351	14.066547
17.125450	569.150346	14.071565
17.235926	578.165088	14.076583
17.105101	574.973182	14.081600
17.286118	572.451936	14.086618
17.030568	578.062129	14.091635
17.356147	582.615601	14.096653
17.478523	580.699986	14.101671
17.512665	572.297273	14.106688
17.587555	577.417038	14.111706
17.335537	584.326864	14.116723
17.207134	571.787134	14.121741
17.096739	587.788687	14.126759
17.633180	575.346757	14.131776
17.324479	583.663478	14.136794
17.144158	570.292444	14.141811
17.311050	577.789880	14.146829
17.448026	581.849041	14.151847
17.590681	575.408005	14.156864
17.372867	573.107038	14.161882
17.111460	586.140563	14.166899
17.557276	594.301202	14.171917
17.866133	596.695580	14.176935
17.649001	596.246953	14.181952
17.685638	603.231480	14.186970
17.675660	592.774938	14.191987
18.246800	599.732522	14.197005
17.639332	586.371597	14.202023
17.447277	581.239005	14.207040
17.433588	587.855872	14.212058
17.416429	599.696120	14.217075
17.816185	598.740585	14.222093
17.604973	602.109538	14.227111
17.893002	600.691828	14.232128
18.047572	599.162486	14.237146
17.979163	602.827799	14.242163
18.378591	596.740999	14.247181
18.005741	601.018898	14.252199
18.096675	594.210420	14.257216
17.914129	581.426703	14.262234
17.773131	578.419426	14.267251
18.297818	579.407219	14.272269
17.674308	582.045508	14.277287
18.056466	592.693414	14.282304
17.965690	586.402556	14.287322
17.906476	592.483762	14.292339
18.570221	586.033661	14.297357
18.033990	585.268959	14.302375
18.024251	577.333864	14.307392
18.067399	571.725769	14.312410
18.123813	580.124137	14.317427
18.022886	575.472728	14.322445
18.094345	586.809935	14.327463
18.212790	593.399790	14.332480
18.321554	594.471685	14.337498
18.392371	596.799219	14.342515
18.473720	584.924046	14.347533
18.248890	583.141726	14.352551
18.184314	579.784805	14.357568
18.075726	571.369742	14.362586
18.180101	582.935319	14.367603
18.409897	591.814608	14.372621
18.441980	595.252737	14.377639
18.211046	593.452438	14.382656
18.308334	594.740724	14.387674
18.129707	603.504131	14.392691
18.172336	596.573833	14.397709
18.258998	597.024344	14.402727
18.815489	595.103827	14.407744
18.506550	601.748024	14.412762
18.029126	608.626904	14.417779
18.100213	600.117405	14.422797
18.555910	593.882934	14.427815
17.908029	599.147506	14.432832
18.103751	599.388427	14.437850
17.917263	602.639898	14.442867
18.375351	611.783229	14.447885
18.405424	626.320609	14.452903
18.483301	628.681755	14.457920
18.460610	618.984581	14.462938
18.553053	626.531572	14.467955
19.121099	622.308666	14.472973
18.742663	616.949647	14.477991
18.693425	618.522824	14.483008
18.916383	617.058504	14.488026
18.814540	622.603602	14.493043
19.163895	615.214985	14.498061
19.040123	620.864505	14.503079
18.940834	626.021041	14.508096
19.173276	617.170673	14.513114
18.869854	612.995948	14.518131
19.024322	595.798110	14.523149
18.797279	590.289147	14.528167
18.639270	589.559859	14.533184
18.607888	593.168876	14.538202
18.857158	609.000487	14.543219
19.108693	603.788920	14.548237
19.249368	615.251000	14.553255
18.880133	616.583981	14.558272
18.961422	609.764385	14.563290
19.084114	613.008440	14.568307
18.975232	612.470268	14.573325
18.784679	619.559825	14.578343
18.814239	617.321079	14.583360
18.919157	615.790047	14.588378
18.924033	617.020231	14.593395
19.405379	616.541060	14.598413
19.073787	618.944270	14.603431
19.019704	614.336004	14.608448
19.079534	609.252301	14.613466
18.802917	614.524980	14.618483
19.230426	615.335497	14.623501
19.308204	620.899789	14.628519
19.155568	618.645408	14.633536
19.327116	610.615623	14.638554
19.515037	617.024188	14.643571
19.354622	608.449971	14.648589
19.161225	612.649264	14.653607
19.089601	621.029842	14.658624
19.593539	616.334145	14.663642
19.502513	617.620381	14.668659
19.102071	619.595722	14.673677
19.371031	625.003829	14.678695
19.715162	635.787106	14.683712
19.645952	628.400949	14.688730
19.477747	623.179402	14.693747
19.444936	613.988744	14.698765
19.454297	624.265890	14.703783
19.337631	632.861814	14.708800
19.447774	634.823430	14.713818
19.546759	642.369403	14.718835
19.303872	630.371432	14.723853
19.662176	641.761561	14.728871
19.418538	646.063408	14.733888
19.486281	633.303554	14.738906
19.288772	643.366972	14.743923
19.357518	638.468056	14.748941
19.709387	642.569301	14.753959
19.553856	639.883026	14.758976
19.507149	633.818776	14.763994
19.728705	658.752941	14.769011
19.971807	662.044412	14.774029
20.008806	662.944519	14.779047
19.943746	662.270091	14.784064
20.347363	648.886402	14.789082
19.824643	639.321210	14.794099
19.688506	627.874559	14.799117
19.535147	634.573287	14.804135
19.978300	649.784422	14.809152
20.584180	649.260492	14.814170
20.133813	648.343478	14.819187
19.951432	640.160851	14.824205
19.985435	635.254756	14.829223
19.796820	635.249783	14.834240
20.130872	632.089171	14.839258
19.890178	637.365696	14.844275
20.207664	635.807669	14.849293
20.221713	639.065595	14.854311
20.140461	644.181441	14.859328
20.259323	635.355172	14.864346
20.077696	643.251223	14.869363
20.100713	636.939363	14.874381
19.959819	644.658621	14.879399
20.104745	660.916880	14.884416
20.555055	650.022114	14.889434
20.543000	660.233209	14.894451
20.552158	658.688775	14.899469
20.521537	647.478043	14.904487
20.212287	643.799685	14.909504
20.414194	635.967103	14.914522
20.038892	636.991768	14.919539
20.219899	640.072058	14.924557
20.277485	645.052542	14.929575
20.506441	650.899270	14.934592
20.731120	648.999177	14.939610
20.639202	654.425965	14.944627
20.574074	651.529865	14.949645
20.855352	652.467437	14.954663
20.644338	657.792966	14.959680
20.841702	641.244770	14.964698
20.342342	645.441516	14.969715
20.566848	639.811297	14.974733
20.639257	640.885735	14.979751
20.702121	653.972645	14.984768
20.780944	650.369181	14.989786
20.381043	648.898306	14.994803
20.118736	646.995620	14.999821
20.600886	655.854337	15.004839
20.723348	657.201800	15.009856
20.983548	658.470878	15.014874
20.644099	655.349515	15.019891
20.465553	658.369377	15.024909
20.792138	653.414280	15.029927
20.640416	658.124606	15.034944
20.989049	654.115951	15.039962
21.100743	649.759412	15.044979
20.683275	652.535842	15.049997
20.916944	645.095911	15.055015
20.752189	656.568003	15.060032
21.332938	653.330865	15.065050
21.232616	656.691921	15.070067
21.302645	651.158485	15.075085
21.300586	648.454474	15.080103
20.856669	654.154164	15.085120
20.890672	650.964822	15.090138
21.160249	653.428479	15.095155
20.903332	656.829849	15.100173
21.518233	652.211431	15.105191
21.180423	655.675969	15.110208
21.183010	650.329824	15.115226
21.318646	654.499665	15.120243
21.451337	664.987885	15.125261
21.349363	650.203339	15.130279
20.768000	663.975016	15.135296
21.159896	654.515823	15.140314
21.277108	659.284998	15.145331
20.654457	662.118824	15.150349
21.084058	662.613435	15.155367
20.893205	678.236355	15.160384
21.557563	672.079618	15.165402
21.200937	670.923853	15.170419
21.261880	673.480162	15.175437
21.455010	667.116391	15.180455
21.133279	680.891584	15.185472
21.586278	678.349800	15.190490
21.231608	675.211883	15.195507
21.069543	671.434718	15.200525
21.421723	663.124144	15.205543
21.717335	690.946935	15.210560
21.765199	682.557799	15.215578
21.758269	672.223810	15.220595
21.479469	672.845193	15.225613
21.440982	670.503493	15.230631
21.979247	687.893043	15.235648
21.946948	678.749608	15.240666
22.000852	666.215962	15.245683
21.525145	674.148636	15.250701
22.057755	667.031087	15.255719
21.957853	663.329391	15.260736
21.912224	665.832969	15.265754
21.715737	667.842632	15.270771
21.468688	671.883087	15.275789
21.362387	676.046658	15.280807
21.672874	691.922400	15.285824
22.238648	687.971235	15.290842
22.435805	690.285297	15.295859
21.820283	705.876948	15.300877
22.036796	688.353720	15.305895
21.612832	694.896053	15.310912
22.116660	693.649652	15.315930
22.376728	690.039874	15.320947
22.071387	696.986500	15.325965
22.467391	693.686783	15.330983
22.274250	694.793363	15.336000
22.431159	684.301152	15.341018
22.175530	672.254656	15.346035
21.928381	671.346826	15.351053
22.460617	679.777986	15.356071
22.386624	678.309695	15.361088
22.247304	669.366070	15.366106
22.315788	666.064024	15.371123
22.164277	683.432256	15.376141
22.317869	683.436782	15.381159
21.991727	690.159446	15.386176
22.457876	688.344592	15.391194
22.592084	692.584094	15.396211
22.206857	694.790589	15.401229
22.473108	688.680442	15.406247
22.322410	691.983126	15.411264
22.253372	689.611496	15.416282
22.021448	689.569126	15.421299
22.118003	694.470935	15.426317
22.337424	687.434007	15.431335
22.641509	685.445730	15.436352
22.501311	688.980297	15.441370
22.735903	688.921639	15.446387
22.239370	700.540416	15.451405
22.786892	695.345564	15.456423
22.618585	697.615902	15.461440
23.083967	707.850050	15.466458
22.724367	701.910541	15.471475
22.497339	702.583773	15.476493
23.100696	705.834587	15.481511
23.152114	705.350191	15.486528
23.324620	693.694193	15.491546
22.954573	690.845861	15.496563
22.821972	689.055391	15.501581
22.554719	686.957815	15.506599
22.883040	694.407917	15.511616
22.828040	686.912211	15.516634
22.618013	686.399352	15.521651
22.453577	695.299436	15.526669
23.134211	703.574813	15.531687
22.980643	710.683857	15.536704
22.791416	715.545241	15.541722
23.145117	718.996119	15.546739
23.109028	715.072975	15.551757
22.887736	709.635658	15.556775
23.127867	719.090905	15.561792
23.106969	713.742110	15.566810
23.476040	707.044645	15.571827
22.788024	714.903304	15.576845
23.327090	712.897142	15.581863
23.133707	718.775350	15.586880
23.022230	713.986702	15.591898
23.208940	715.532386	15.596915
23.097546	719.800907	15.601933
23.223185	715.868203	15.606951
23.201215	717.812658	15.611968
23.112673	713.481165	15.616986
23.489294	717.853105	15.622003
23.635378	735.875351	15.627021
23.681049	724.365438	15.632039
23.392302	723.429409	15.637056
23.403493	730.474777	15.642074
23.765455	725.984334	15.647091
23.430843	724.976595	15.652109
23.577542	725.682792	15.657127
23.294842	730.240088	15.662144
23.346095	733.306010	15.667162
23.676111	730.505776	15.672179
23.407167	743.584779	15.677197
23.887393	730.996914	15.682215
23.557256	735.195570	15.687232
23.901820	726.037246	15.692250
23.881536	729.325815	15.697267
23.699251	736.171124	15.702285
23.653161	732.088597	15.707303
24.020195	720.244312	15.712320
23.905196	731.935875	15.717338
24.089641	727.933994	15.722355
23.760366	725.259149	15.727373
24.225860	723.046762	15.732391
24.031792	724.718380	15.737408
24.012750	733.674598	15.742426
23.579225	726.298143	15.747443
23.587016	731.993356	15.752461
23.583776	730.580247	15.757479
23.981314	730.653849	15.762496
24.049663	741.136416	15.767514
24.612202	742.594816	15.772531
24.193630	741.559206	15.777549
24.499292	732.347013	15.782567
24.092368	728.393605	15.787584
23.898765	732.135365	15.792602
24.190909	726.794323	15.797619
23.864334	732.661846	15.802637
24.074917	744.160393	15.807655
24.556204	751.974719	15.812672
24.683615	751.364806	15.817690
24.566181	747.549075	15.822707
24.459732	733.989617	15.827725
24.157160	723.380026	15.832743
24.128121	738.816700	15.837760
24.033381	746.238434	15.842778
24.316905	740.977634	15.847795
24.507049	751.958679	15.852813
24.633563	745.207685	15.857831
24.867937	748.806654	15.862848
24.841221	754.879667	15.867866
24.808357	739.572976	15.872883
24.372818	757.670593	15.877901
24.681280	753.583003	15.882919
24.885579	753.844673	15.887936
24.728984	764.431926	15.892954
24.674899	748.456362	15.897971
24.733431	760.770853	15.902989
24.970695	749.366606	15.908007
24.893053	749.189610	15.913024
24.303053	751.043186	15.918042
25.065283	744.994166	15.923059
24.690252	754.037728	15.928077
25.066155	749.983754	15.933095
24.933805	746.186139	15.938112
24.827124	743.599492	15.943130
25.026024	742.861614	15.948147
24.679825	751.080145	15.953165
24.809707	752.391739	15.958183
24.736057	745.302875	15.963200
24.498311	747.461023	15.968218
25.096923	752.703910	15.973235
25.224379	769.807610	15.978253
25.367411	763.694653	15.983271
24.912761	752.663901	15.988288
24.960787	766.258149	15.993306
25.419953	767.698034	15.998323
25.343608	775.435636	16.003341
25.300502	779.112801	16.008359
25.496046	771.574649	16.013376
25.340487	777.087185	16.018394
25.574717	771.322856	16.023411
25.288969	774.678273	16.028429
25.303784	770.829192	16.033447
25.551937	772.826006	16.038464
25.584004	770.078760	16.043482
25.574029	766.047371	16.048499
25.528763	769.967870	16.053517
25.524833	776.583278	16.058535
25.741472	769.325846	16.063552
25.438555	765.835819	16.068570
25.302456	771.465226	16.073587
25.380857	777.288247	16.078605
25.290543	774.784238	16.083623
25.675046	764.685513	16.088640
25.522017	764.709678	16.093658
25.716869	762.631209	16.098675
26.055163	770.524752	16.103693
25.713741	773.475479	16.108711
25.888958	760.477788	16.113728
25.480935	774.588466	16.118746
26.142728	766.298763	16.123763
25.522745	776.848173	16.128781
25.376486	769.767520	16.133799
25.810664	773.139528	16.138816
25.770982	782.408275	16.143834
26.302721	788.636800	16.148851
26.005438	786.316697	16.153869
26.023886	787.642597	16.158887
26.252794	778.155227	16.163904
25.984336	781.460598	16.168922
26.211646	776.240154	16.173939
25.794499	772.992086	16.178957
26.111878	786.679848	16.183975
25.815585	800.400654	16.188992
25.967356	801.689887	16.194010
26.012523	802.127970	16.199027
26.126939	798.982807	16.204045
26.253487	798.171055	16.209063
26.116605	795.283017	16.214080
25.611939	805.347314	16.219098
25.879479	804.390394	16.224115
26.267953	815.094249	16.229133
26.504395	820.782068	16.234151
27.073646	814.835845	16.239168
26.988728	820.198471	16.244186
26.834691	802.932004	16.249203
26.789739	799.145931	16.254221
26.785123	802.413124	16.259239
27.093222	793.055350	16.264256
26.605693	790.932313	16.269274
26.990719	789.660339	16.274291
27.252235	796.679136	16.279309
26.807446	790.582529	16.284327
27.047612	789.465795	16.289344
26.467811	783.137879	16.294362
26.431788	781.654162	16.299379
26.595016	785.128585	16.304397
26.900597	790.669861	16.309415
26.936361	789.537816	16.314432
26.580425	791.487267	16.319450
27.113275	783.271408	16.324467
26.713798	784.789021	16.329485
26.623322	802.340310	16.334503
26.771899	786.856827	16.339520
26.685116	788.442213	16.344538
26.572344	789.457311	16.349555
27.087884	792.052865	16.354573
27.124578	806.649316	16.359591
27.057573	804.927453	16.364608
26.853402	815.001478	16.369626
26.577216	818.746728	16.374643
26.934748	814.765045	16.379661
26.935104	815.595161	16.384679
27.145364	817.238152	16.389696
27.372069	820.737350	16.394714
27.184323	818.980754	16.399731
27.283296	816.907834	16.404749
27.104362	815.544336	16.409767
27.192846	814.287263	16.414784
27.454530	834.913993	16.419802
27.691165	835.284207	16.424819
27.401841	825.622385	16.429837
27.703359	840.795915	16.434855
27.702640	819.323931	16.439872
27.458928	815.174517	16.444890
27.504859	822.236569	16.449907
27.733094	827.824690	16.454925
27.518375	839.045949	16.459943
28.041522	825.573971	16.464960
27.434012	823.179392	16.469978
27.909965	833.740163	16.474995
28.150599	823.755466	16.480013
27.553616	829.905230	16.485031
27.663042	814.004975	16.490048
27.694256	825.190849	16.495066
27.687369	830.856835	16.500083
27.932106	827.464028	16.505101
27.757546	837.299895	16.510119
28.150734	837.724477	16.515136
27.815811	831.960940	16.520154
27.908348	835.039346	16.525171
27.829311	834.644815	16.530189
27.828470	832.294039	16.535207
28.276630	836.670579	16.540224
27.951704	831.719681	16.545242
27.981526	831.961351	16.550259
28.197181	832.467398	16.555277
28.081463	832.078615	16.560295
28.333934	828.447908	16.565312
28.166729	837.301159	16.570330
28.239293	840.859227	16.575347
28.570791	835.111196	16.580365
28.339007	833.058538	16.585383
28.310639	844.364213	16.590400
28.361870	834.175653	16.595418
28.373261	831.169703	16.600435
28.484476	833.569834	16.605453
28.285927	830.467389	16.610471
28.118694	823.718207	16.615488
28.336873	834.833767	16.620506
28.182309	832.560726	16.625523
28.788034	833.251812	16.630541
28.636769	854.195731	16.635559
28.894902	853.827268	16.640576
28.756243	845.697656	16.645594
28.501425	844.238747	16.650611
29.147933	854.526654	16.655629
28.960520	841.162839	16.660647
28.394817	832.579429	16.665664
28.852014	843.550247	16.670682
28.698640	849.191853	16.675699
28.818289	852.098755	16.680717
28.681342	846.979543	16.685735
28.863541	847.692806	16.690752
28.615632	849.574844	16.695770
28.777295	854.466496	16.700787
29.233498	849.194389	16.705805
29.153950	854.325807	16.710823
29.089935	849.842114	16.715840
29.478201	851.106920	16.720858
29.496162	851.905877	16.725875
29.444017	841.484198	16.730893
28.873747	849.324467	16.735911
29.062204	851.677784	16.740928
29.058659	858.381526	16.745946
28.943220	858.292502	16.750963
29.085294	843.804077	16.755981
28.909766	853.214067	16.760999
29.352003	835.980378	16.766016
29.073769	851.967438	16.771034
29.242178	867.603664	16.776051
29.072813	863.186967	16.781069
29.147471	869.850057	16.786087
29.219229	869.444522	16.791104
29.870051	867.247263	16.796122
29.705341	875.825584	16.801139
29.869565	866.158951	16.806157
29.661292	876.066394	16.811175
29.612735	883.777599	16.816192
29.774321	866.089231	16.821210
29.483148	877.492907	16.826227
29.798506	872.498484	16.831245
29.510726	875.402952	16.836263
29.951143	868.460717	16.841280
29.875801	867.323984	16.846298
30.154597	869.820942	16.851315
29.870799	869.692024	16.856333
29.954068	864.923315	16.861351
29.687610	870.440633	16.866368
30.062967	873.932331	16.871386
29.875891	869.543654	16.876403
29.934544	869.821834	16.881421
30.007878	875.058694	16.886439
29.948950	859.755983	16.891456
29.999479	865.558153	16.896474
29.742976	862.963404	16.901491
29.872596	869.094014	16.906509
29.698526	893.175300	16.911527
30.264657	894.560567	16.916544
30.086229	881.454093	16.921562
30.088868	890.375434	16.926579
30.278899	888.723745	16.931597
30.150950	894.992550	16.936615
30.154028	883.732208	16.941632
30.374366	883.884069	16.946650
30.403629	883.958568	16.951667
30.569473	889.070484	16.956685
30.205828	884.330766	16.961703
30.724786	885.685553	16.966720
30.758692	884.623222	16.971738
30.439461	890.151970	16.976755
30.752127	880.679824	16.981773
30.598469	891.604367	16.986791
30.950751	885.909869	16.991808
30.734393	888.818929	16.996826
30.339528	886.031258	17.001843
30.789701	900.335782	17.006861
30.920038	905.462733	17.011879
30.983107	917.502063	17.016896
31.282465	908.476963	17.021914
30.940034	898.201720	17.026931
31.438481	885.670854	17.031949
30.878599	892.029424	17.036967
30.914357	891.768386	17.041984
31.125125	888.112643	17.047002
30.554514	887.618403	17.052019
30.926287	896.778561	17.057037
31.015550	906.835066	17.062055
30.908886	902.493743	17.067072
31.385145	909.027653	17.072090
31.292545	910.661299	17.077107
30.975678	894.300738	17.082125
31.239174	909.811647	17.087143
31.527833	908.027737	17.092160
31.423116	904.509785	17.097178
31.173121	905.196090	17.102195
31.308127	905.919906	17.107213
31.528224	905.699414	17.112231
31.200374	910.232271	17.117248
31.169246	905.607710	17.122266
31.676663	909.457425	17.127283
31.646173	908.704988	17.132301
31.543325	910.027810	17.137319
31.673684	900.742010	17.142336
31.797497	913.128431	17.147354
31.505299	901.911185	17.152371
31.755834	903.446886	17.157389
31.736792	912.403194	17.162407
32.107404	922.172626	17.167424
32.234479	907.658096	17.172442
32.016227	903.842348	17.177459
31.916543	894.763009	17.182477
31.815230	908.245063	17.187495
31.340855	910.036356	17.192512
31.903895	912.034343	17.197530
32.034752	932.640657	17.202547
32.088969	927.851237	17.207565
32.170992	929.867786	17.212583
32.408055	923.171988	17.217600
32.393102	912.151142	17.222618
31.674732	913.308469	17.227635
32.069606	911.877151	17.232653
32.037527	924.811875	17.237671
32.108506	926.609244	17.242688
32.424885	925.802459	17.247706
32.164769	922.917929	17.252723
32.155551	921.878132	17.257741
32.236631	923.636047	17.262759
32.339870	925.046504	17.267776
32.474298	921.781417	17.272794
32.222790	930.423857	17.277811
32.291628	925.991914	17.282829
32.258632	925.318765	17.287847
32.292722	926.462341	17.292864
32.683760	931.633661	17.297882
32.785993	950.073255	17.302899
32.683749	955.763689	17.307917
33.105895	948.912650	17.312935
32.759227	933.806439	17.317952
32.781561	929.719457	17.322970
32.978803	918.371866	17.327987
32.674657	921.821712	17.333005
32.730474	936.569910	17.338023
32.848694	947.272006	17.343040
32.924954	938.509067	17.348058
32.588998	944.876753	17.353075
33.226485	944.919074	17.358093
33.531363	948.885740	17.363111
33.119906	954.602529	17.368128
33.246754	944.834411	17.373146
33.045517	946.238924	17.378163
33.144550	949.414164	17.383181
33.332900	945.768234	17.388199
33.209024	943.888007	17.393216
33.186278	943.733966	17.398234
33.333828	944.468441	17.403251
33.448616	945.949675	17.408269
33.440897	939.551003	17.413287
33.385259	948.983285	17.418304
33.697401	935.418052	17.423322
33.625395	937.259915	17.428339
33.601029	937.342817	17.433357
33.701784	940.505162	17.438375
33.081457	945.263736	17.443392
33.737258	933.778017	17.448410
33.474268	944.574553	17.453427
33.690460	944.660791	17.458445
33.532521	944.625764	17.463463
33.635951	943.940706	17.468480
33.818326	942.378575	17.473498
33.468898	946.517185	17.478515
33.501547	943.466860	17.483533
33.659050	949.605752	17.488551
33.617034	962.466320	17.493568
33.975651	961.271056	17.498586
33.964350	974.477121	17.503603
34.290663	966.034758	17.508621
34.218661	967.652558	17.513639
34.156576	978.395547	17.518656
34.235742	966.394228	17.523674
34.173694	963.762685	17.528691
33.852729	964.384372	17.533709
34.154056	957.864688	17.538727
34.238495	968.565778	17.543744
34.602605	965.179489	17.548762
34.599452	966.808594	17.553779
34.248206	961.710301	17.558797
34.499779	959.461974	17.563815
34.312510	973.254194	17.568832
34.306885	958.378556	17.573850
34.288499	965.592756	17.578867
33.994770	968.583379	17.583885
34.474647	958.671577	17.588903
34.162056	963.135784	17.593920
34.360826	957.528432	17.598938
34.386505	965.843433	17.603955
34.380788	966.381012	17.608973
34.648128	968.633622	17.613991
34.429789	988.581489	17.619008
34.726662	988.184863	17.624026
34.714523	993.842256	17.629043
34.800466	984.803217	17.634061
34.546733	995.317462	17.639079
34.641806	990.111362	17.644096
34.619625	988.398237	17.649114
34.669895	996.652594	17.654131
34.895872	997.333757	17.659149
35.209999	1007.689610	17.664167
35.199191	1022.268433	17.669184
35.483259	1002.651440	17.674202
35.645399	998.877059	17.679219
34.889722	988.824303	17.684237
35.143367	989.084558	17.689255
35.113802	1001.709670	17.694272
35.464740	1000.648153	17.699290
35.382724	1005.347648	17.704307
35.381741	1003.924696	17.709325
35.700778	1003.818093	17.714343
35.285535	1009.806897	17.719360
35.561262	1004.727126	17.724378
35.630527	1002.232797	17.729395
35.570751	1002.349650	17.734413
35.746811	998.835025	17.739431
35.803235	1001.000762	17.744448
35.716331	1002.608277	17.749466
35.666599	1006.232877	17.754483
35.763164	1006.410443	17.759501
35.975935	1007.122079	17.764519
35.641651	1009.494202	17.769536
35.719005	1002.832865	17.774554
36.049943	1005.523648	17.779571
35.551374	1001.843318	17.784589
35.890246	1006.252803	17.789607
35.905753	1004.240277	17.794624
35.817713	1010.477622	17.799642
35.995845	996.598817	17.804659
35.788948	1003.526981	17.809677
35.457102	1008.530713	17.814695
35.928448	1013.544305	17.819712
36.005902	1026.417760	17.824730
36.526261	1024.357690	17.829747
36.069221	1026.420839	17.834765
36.513755	1025.644464	17.839783
36.520737	1030.383671	17.844800
36.377976	1021.008054	17.849818
36.624951	1029.891183	17.854835
36.295960	1029.182353	17.859853
36.934820	1015.348115	17.864871
36.844668	1020.875725	17.869888
36.794793	1020.924754	17.874906
36.558949	1014.101041	17.879923
36.509042	1016.788379	17.884941
36.714009	1014.020318	17.889959
36.592345	1020.367079	17.894976
36.877328	1022.089902	17.899994
36.887883	1020.756660	17.905011
36.663428	1010.245113	17.910029
36.797048	1006.885462	17.915047
36.837529	1020.989181	17.920064
36.878328	1020.301309	17.925082
36.808489	1018.665078	17.930099
36.637115	1016.107462	17.935117
37.199106	1012.510277	17.940135
36.690865	1024.737023	17.945152
36.864715	1018.136303	17.950170
36.973754	1014.603773	17.955187
36.638107	1022.700852	17.960205
36.918280	1028.037897	17.965223
37.105868	1037.075504	17.970240
37.108772	1038.817277	17.975258
37.464148	1026.955681	17.980275
37.466248	1036.098091	17.985293
37.448677	1027.952580	17.990311
37.081774	1036.783568	17.995328
37.597578	1036.759747	18.000346
37.612660	1033.879419	18.005363
37.321721	1029.563781	18.010381
37.253040	1027.756950	18.015399
37.132214	1034.999852	18.020416
37.347335	1040.883590	18.025434
37.760066	1055.026844	18.030451
37.653500	1056.271363	18.035469
37.403876	1051.052979	18.040487
37.757941	1056.185947	18.045504
37.700853	1059.505590	18.050522
37.667595	1054.635166	18.055539
37.739045	1053.563786	18.060557
37.876508	1045.091013	18.065575
37.914580	1045.997283	18.070592
37.733846	1066.018241	18.075610
38.474497	1072.122615	18.080627
38.552533	1069.033598	18.085645
38.445915	1051.506991	18.090663
37.982671	1043.661679	18.095680
38.217273	1053.054853	18.100698
38.244226	1063.114898	18.105715
38.432608	1070.782748	18.110733
38.908910	1065.684158	18.115751
38.511811	1064.973374	18.120768
38.377578	1050.764762	18.125786
38.279579	1043.455528	18.130803
38.268941	1056.194480	18.135821
38.816810	1067.981226	18.140839
38.875367	1070.601083	18.145856
38.682631	1067.649167	18.150874
38.604004	1051.626683	18.155891
38.944390	1068.034575	18.160909
39.289907	1057.020279	18.165927
38.932764	1046.324368	18.170944
38.461949	1046.111138	18.175962
38.724187	1046.139668	18.180979
38.472854	1060.850884	18.185997
39.090724	1063.484097	18.191015
38.885094	1069.373806	18.196032
38.742320	1070.532478	18.201050
39.003797	1070.794663	18.206067
38.848356	1069.616817	18.211085
39.035107	1078.402106	18.216103
38.885527	1072.795647	18.221120
38.877531	1062.875018	18.226138
39.392729	1060.853624	18.231155
38.854593	1071.295706	18.236173
39.358215	1069.260345	18.241191
39.516877	1068.374121	18.246208
39.094871	1062.990233	18.251226
39.650211	1072.708714	18.256243
39.518452	1085.084803	18.261261
39.617151	1091.936719	18.266279
39.640948	1090.288965	18.271296
40.045396	1084.542049	18.276314
39.733251	1063.857039	18.281331
39.326037	1067.928989	18.286349
39.544593	1072.739203	18.291367
39.613475	1079.592629	18.296384
39.847808	1083.737640	18.301402
40.097300	1082.449011	18.306419
39.767283	1089.999271	18.311437
39.710693	1083.314709	18.316455
39.894594	1087.934691	18.321472
39.958563	1089.600629	18.326490
39.992719	1077.315946	18.331507
39.918209	1085.447880	18.336525
40.120269	1076.488434	18.341543
39.973391	1086.711429	18.346560
39.798198	1089.427875	18.351578
40.167365	1084.743705	18.356595
39.886493	1090.102399	18.361613
40.230972	1089.963406	18.366631
40.385994	1106.223646	18.371648
40.509936	1109.568586	18.376666
40.292930	1109.893115	18.381683
40.247145	1103.045902	18.386701
40.468702	1101.427125	18.391719
40.672825	1103.143690	18.396736
40.255802	1109.883905	18.401754
40.653910	1102.231824	18.406771
40.389781	1113.574608	18.411789
40.587906	1103.905691	18.416807
40.756273	1098.839558	18.421824
40.580788	1103.638933	18.426842
40.487176	1104.714164	18.431859
40.618971	1125.386827	18.436877
40.704850	1124.631927	18.441895
40.701562	1131.250522	18.446912
40.593729	1129.020615	18.451930
40.460392	1127.605766	18.456947
40.856772	1130.059091	18.461965
41.055696	1137.457069	18.466983
41.455806	1151.330971	18.472000
41.422796	1154.542715	18.477018
41.536606	1140.613914	18.482035
41.194309	1124.885146	18.487053
41.288203	1125.047352	18.492071
41.578501	1126.665209	18.497088
41.612052	1132.750999	18.502106
41.429647	1116.855172	18.507123
41.734485	1125.000274	18.512141
41.621195	1118.024773	18.517159
41.867245	1128.340867	18.522176
41.477209	1120.357815	18.527194
41.759648	1113.882061	18.532211
41.645342	1115.803156	18.537229
41.666311	1113.376340	18.542247
41.714202	1116.524908	18.547264
41.759003	1132.931834	18.552282
41.868274	1142.022791	18.557299
42.012274	1125.630835	18.562317
41.899332	1135.977933	18.567335
42.452888	1138.125760	18.572352
42.123009	1138.531092	18.577370
42.145505	1124.897484	18.582387
41.894210	1123.223399	18.587405
42.054093	1137.488388	18.592423
42.398346	1132.445182	18.597440
42.058916	1139.081731	18.602458
42.454868	1139.180833	18.607475
42.211986	1131.405100	18.612493
42.334939	1138.660343	18.617511
42.632258	1135.675817	18.622528
42.310807	1140.674800	18.627546
42.080092	1145.889948	18.632563
42.046480	1132.287217	18.637581
42.044409	1133.038830	18.642599
42.481623	1137.918947	18.647616
42.139640	1152.234176	18.652634
42.351504	1159.709033	18.657651
42.618189	1166.083365	18.662669
42.711392	1166.984159	18.667687
43.079336	1165.613847	18.672704
42.915977	1166.106702	18.677722
43.042229	1165.048821	18.682739
43.134257	1167.013335	18.687757
43.096238	1158.792070	18.692775
42.974325	1154.904367	18.697792
42.985540	1161.687963	18.702810
43.255004	1161.434488	18.707827
43.155155	1161.466099	18.712845
42.947556	1156.269503	18.717863
42.973605	1153.551544	18.722880
43.225963	1166.486061	18.727898
43.640463	1167.891953	18.732915
43.198711	1167.446943	18.737933
43.425383	1169.977357	18.742951
43.672663	1169.257129	18.747968
43.230852	1189.309662	18.752986
43.723712	1183.507836	18.758003
43.816652	1189.656927	18.763021
43.652842	1178.179542	18.768039
43.541786	1169.736180	18.773056
43.934971	1181.168530	18.778074
43.779113	1174.594163	18.783091
43.795953	1180.212360	18.788109
43.652794	1177.413608	18.793127
44.138857	1178.129771	18.798144
44.257508	1175.971673	18.803162
43.956264	1173.371264	18.808179
44.173714	1179.759627	18.813197
44.083950	1180.856351	18.818215
44.089161	1172.621996	18.823232
44.057106	1172.851275	18.828250
44.114288	1175.865850	18.833267
43.711717	1178.570595	18.838285
44.484351	1178.670641	18.843303
44.263434	1169.862629	18.848320
43.744836	1187.108978	18.853338
44.373162	1185.379124	18.858355
44.477738	1190.778445	18.863373
44.556560	1202.424168	18.868391
44.862851	1205.958313	18.873408
44.506057	1199.263936	18.878426
44.448358	1197.367002	18.883443
44.714962	1201.118808	18.888461
44.455349	1199.985678	18.893479
44.743736	1196.854214	18.898496
44.663850	1191.066380	18.903514
44.729354	1195.455625	18.908531
44.854372	1195.795998	18.913549
44.623594	1192.335610	18.918567
45.246073	1204.022392	18.923584
45.093150	1204.232738	18.928602
45.222628	1198.440502	18.933619
45.072573	1199.780210	18.938637
45.125734	1210.622049	18.943655
45.523915	1213.141378	18.948672
45.414433	1221.925813	18.953690
45.550284	1203.603651	18.958707
45.510685	1200.043878	18.963725
45.014868	1194.460069	18.968743
45.540601	1202.075121	18.973760
45.239644	1218.630975	18.978778
45.595765	1211.099038	18.983795
45.657968	1207.289777	18.988813
45.613508	1215.811550	18.993831
45.705401	1206.465344	18.998848
45.840343	1219.992670	19.003866
45.625444	1209.656239	19.008883
45.756134	1210.879375	19.013901
45.917405	1206.928357	19.018919
46.114270	1208.371506	19.023936
45.833845	1217.968541	19.028954
45.662634	1211.851015	19.033971
46.016987	1209.573931	19.038989
45.883637	1205.602799	19.044007
46.228051	1199.821069	19.049024
45.905360	1215.654469	19.054042
46.300412	1227.007658	19.059059
46.589302	1233.599449	19.064077
46.579353	1240.670422	19.069095
46.527939	1222.983514	19.074112
46.590413	1232.362725	19.079130
46.413175	1231.434444	19.084147
46.246715	1226.326058	19.089165
46.490859	1236.819244	19.094183
46.872168	1226.108516	19.099200
46.887403	1228.072444	19.104218
46.712609	1229.977781	19.109235
46.777998	1223.873676	19.114253
46.469207	1235.286652	19.119271
46.607990	1232.339573	19.124288
46.856222	1228.008841	19.129306
46.998218	1222.924714	19.134323
47.103588	1227.383462	19.139341
46.667480	1228.506050	19.144359
46.829296	1222.607751	19.149376
46.877119	1234.046907	19.154394
47.272751	1248.748434	19.159411
47.502927	1250.713404	19.164429
47.124539	1253.947719	19.169447
47.280851	1256.700616	19.174464
47.093988	1250.995797	19.179482
47.540691	1245.286392	19.184499
47.506534	1245.213034	19.189517
47.270595	1253.569159	19.194535
47.368702	1246.812959	19.199552
47.480253	1246.416961	19.204570
47.499205	1255.320149	19.209587
47.839739	1246.793373	19.214605
47.587255	1244.908017	19.219623
47.854122	1239.346714	19.224640
47.620172	1253.380001	19.229658
47.907464	1257.595653	19.234675
48.373470	1245.031749	19.239693
48.093683	1250.557582	19.244711
48.182588	1249.120527	19.249728
47.953960	1241.781183	19.254746
48.149862	1241.293072	19.259763
48.145156	1246.027856	19.264781
48.066407	1248.258985	19.269799
48.076545	1253.767798	19.274816
48.247736	1266.661455	19.279834
48.139808	1271.264090	19.284851
48.665519	1260.063642	19.289869
48.748836	1253.713713	19.294887
48.728424	1262.616761	19.299904
48.782015	1268.740485	19.304922
48.591688	1265.671389	19.309939
48.341810	1266.079969	19.314957
48.491805	1272.671444	19.319975
48.623137	1264.250023	19.324992
48.788507	1257.682103	19.330010
48.671477	1253.888290	19.335027
49.077354	1260.120923	19.340045
48.832013	1256.817444	19.345063
49.254078	1253.841757	19.350080
49.024652	1257.106385	19.355098
49.234638	1255.050736	19.360115
48.940029	1261.689775	19.365133
48.752719	1267.172722	19.370151
49.167312	1267.126888	19.375168
49.061868	1284.564228	19.380186
49.085077	1294.606054	19.385203
49.373134	1277.560206	19.390221
49.535061	1288.820568	19.395239
49.466632	1285.000198	19.400256
49.788970	1281.980170	19.405274
49.484919	1287.121639	19.410291
49.574811	1286.072604	19.415309
49.488955	1289.431512	19.420327
49.833655	1282.447308	19.425344
49.554384	1287.581739	19.430362
49.404190	1287.476067	19.435379
49.727013	1290.780413	19.440397
49.693690	1308.130734	19.445415
50.018659	1310.576338	19.450432
50.184876	1317.761757	19.455450
50.215139	1307.689825	19.460467
50.411125	1298.242053	19.465485
50.154899	1308.769496	19.470503
50.251293	1304.153254	19.475520
50.276228	1302.590513	19.480538
50.314172	1312.551142	19.485555
49.990718	1301.152342	19.490573
50.233387	1313.747645	19.495591
50.163701	1315.014807	19.500608
50.051754	1315.423868	19.505626
50.148885	1327.353994	19.510643
50.539480	1322.969374	19.515661
50.404079	1328.886036	19.520679
50.798657	1331.765721	19.525696
50.605252	1327.769256	19.530714
50.723902	1327.766634	19.535731
50.928054	1321.937411	19.540749
50.801104	1326.397869	19.545767
50.965472	1332.778824	19.550784
51.236772	1339.812083	19.555802
51.135860	1345.824336	19.560819
51.301311	1335.882692	19.565837
51.284858	1345.447905	19.570855
51.643265	1333.364718	19.575872
51.687291	1324.511962	19.580890
51.306421	1322.611997	19.585907
51.360175	1318.116046	19.590925
51.368482	1323.637791	19.595943
51.190845	1308.911891	19.600960
51.473137	1321.207492	19.605978
51.346745	1330.770986	19.610995
52.127510	1340.624717	19.616013
51.815176	1341.945677	19.621031
52.014583	1335.741638	19.626048
52.054470	1338.383396	19.631066
51.888653	1330.693335	19.636083
52.175972	1331.219728	19.641101
51.874183	1324.750223	19.646119
51.875354	1334.034948	19.651136
51.869566	1334.926012	19.656154
52.144331	1330.313377	19.661171
52.348430	1339.825096	19.666189
51.897670	1333.331589	19.671207
52.257694	1335.822199	19.676224
52.399202	1341.162129	19.681242
51.955601	1342.661452	19.686259
52.215304	1338.568746	19.691277
52.042054	1335.446467	19.696295
52.236471	1345.871768	19.701312
52.501026	1347.736684	19.706330
52.376658	1360.973373	19.711347
52.766357	1357.747111	19.716365
52.697845	1355.375310	19.721383
52.707256	1359.120107	19.726400
52.734088	1355.695068	19.731418
52.311469	1352.984256	19.736435
52.781305	1353.160150	19.741453
52.682997	1364.259353	19.746471
52.864657	1370.596586	19.751488
53.208322	1377.706888	19.756506
52.829687	1377.766399	19.761523
53.351768	1372.991923	19.766541
53.485275	1375.884117	19.771559
53.363848	1371.440846	19.776576
53.745162	1372.542673	19.781594
53.500442	1378.069364	19.786611
53.565169	1369.431101	19.791629
53.821067	1374.241859	19.796647
53.543934	1387.530905	19.801664
54.003654	1372.332694	19.806682
53.597131	1376.253120	19.811699
53.814943	1373.142151	19.816717
53.761429	1368.233788	19.821735
54.004911	1375.564921	19.826752
53.967042	1372.187887	19.831770
53.657601	1364.927428	19.836787
53.884858	1369.957274	19.841805
54.215411	1370.259137	19.846823
54.377485	1378.231056	19.851840
54.137982	1375.037096	19.856858
54.443888	1387.950762	19.861875
54.139041	1384.587151	19.866893
54.350251	1394.467028	19.871911
54.373833	1386.816699	19.876928
54.224276	1385.215015	19.881946
54.099493	1381.690643	19.886963
54.555925	1386.801358	19.891981
54.587820	1394.702158	19.896999
54.532009	1386.878067	19.902016
54.614400	1380.884859	19.907034
54.700523	1384.800687	19.912051
54.583192	1392.756425	19.917069
54.880220	1403.263516	19.922087
54.786704	1410.783169	19.927104
54.913883	1414.105567	19.932122
54.955080	1415.418482	19.937139
55.249948	1416.514920	19.942157
55.155871	1410.568285	19.947175
55.205783	1412.469994	19.952192
55.204550	1410.901876	19.957210
55.842777	1414.327249	19.962227
55.317438	1402.306735	19.967245
55.479625	1400.400576	19.972263
55.327603	1412.735883	19.977280
55.805016	1399.059194	19.982298
55.494115	1401.793793	19.987315
55.634124	1393.831717	19.992333
55.854018	1395.571087	19.997351
55.727877	1404.411873	20.002368
55.884417	1406.508323	20.007386
55.681897	1401.853679	20.012403
55.422466	1395.607894	20.017421
55.846997	1406.820876	20.022439
55.915605	1423.243274	20.027456
56.301896	1422.554908	20.032474
56.038475	1426.863196	20.037491
56.328834	1423.037078	20.042509
56.413931	1420.641201	20.047527
56.209640	1428.323390	20.052544
56.303455	1429.085240	20.057562
56.513350	1424.867769	20.062579
56.396551	1424.892568	20.067597
56.672057	1424.174221	20.072615
56.819771	1423.327566	20.077632
56.716903	1421.232549	20.082650
56.388980	1414.460980	20.087667
56.398073	1423.776069	20.092685
56.768278	1431.876355	20.097703
56.891885	1440.845294	20.102720
56.962883	1447.985721	20.107738
57.063743	1451.605753	20.112755
57.334717	1450.512557	20.117773
57.241149	1446.550918	20.122791
57.188771	1452.454612	20.127808
57.546164	1440.488282	20.132826
57.295551	1441.057933	20.137843
56.956025	1439.899436	20.142861
57.683500	1439.675188	20.147879
57.435873	1440.279087	20.152896
57.650060	1436.490148	20.157914
57.626987	1432.050389	20.162931
57.424482	1436.371226	20.167949
57.354168	1440.390475	20.172967
56.938381	1444.160881	20.177984
57.301558	1446.799342	20.183002
57.666584	1458.397236	20.188019
57.819051	1463.063270	20.193037
57.849268	1458.233285	20.198055
57.846234	1463.485439	20.203072
58.022922	1467.333445	20.208090
58.234856	1485.642792	20.213107
58.070592	1484.488392	20.218125
58.321475	1485.396057	20.223143
58.337101	1484.219784	20.228160
58.478198	1486.741560	20.233178
58.459966	1484.204067	20.238195
58.589467	1489.110401	20.243213
58.319272	1474.780735	20.248231
58.191734	1483.195726	20.253248
58.304766	1475.345143	20.258266
58.634082	1480.065527	20.263283
58.709706	1493.614979	20.268301
58.792113	1506.683673	20.273319
58.613841	1509.732039	20.278336
58.650900	1503.231471	20.283354
59.072954	1495.815324	20.288371
59.090900	1504.800849	20.293389
59.374817	1486.837068	20.298407
59.339089	1499.769625	20.303424
59.265861	1491.809356	20.308442
59.501412	1498.712573	20.313459
59.314922	1494.169008	20.318477
59.460092	1487.903983	20.323495
59.465481	1493.255817	20.328512
59.559548	1490.514527	20.333530
59.710191	1487.676006	20.338547
59.814930	1486.116526	20.343565
59.211287	1483.090057	20.348583
59.891610	1500.814771	20.353600
59.813050	1499.227200	20.358618
59.984023	1512.149472	20.363635
60.395891	1513.095036	20.368653
60.356884	1508.559919	20.373671
60.319674	1514.372891	20.378688
60.444494	1501.612943	20.383706
60.429770	1495.489737	20.388723
60.058062	1486.818806	20.393741
60.226935	1492.571079	20.398759
60.488236	1506.328146	20.403776
60.695987	1506.835452	20.408794
60.401142	1501.254773	20.413811
60.842556	1507.683908	20.418829
60.588800	1499.944432	20.423847
60.897608	1505.356034	20.428864
60.979674	1501.089141	20.433882
61.139832	1502.822102	20.438899
60.867792	1500.756736	20.443917
61.021751	1500.511886	20.448935
60.687276	1508.975090	20.453952
61.120311	1502.128448	20.458970
60.988879	1504.812851	20.463987
60.686743	1506.091198	20.469005
61.322349	1516.507438	20.474023
61.135408	1523.590474	20.479040
61.177246	1531.559208	20.484058
61.005174	1530.355532	20.489075
61.026049	1532.410133	20.494093
61.259663	1527.317878	20.499111
61.414439	1530.803240	20.504128
61.756967	1546.223424	20.509146
61.825559	1564.615273	20.514163
62.116646	1559.564499	20.519181
62.144029	1551.821981	20.524199
61.888707	1550.000155	20.529216
62.095763	1554.045404	20.534234
62.141777	1563.316909	20.539251
62.210623	1550.950723	20.544269
62.409834	1541.726390	20.549287
62.461544	1544.325299	20.554304
62.469357	1546.120004	20.559322
62.245177	1538.861895	20.564339
62.331172	1550.121695	20.569357
62.137741	1536.928722	20.574375
62.432517	1543.595449	20.579392
62.542775	1541.725815	20.584410
62.757091	1539.618960	20.589427
62.348532	1543.498713	20.594445
62.791297	1543.372724	20.599463
62.621766	1568.192702	20.604480
62.728218	1561.062673	20.609498
62.853276	1559.200186	20.614515
62.984965	1567.243225	20.619533
63.405460	1565.107221	20.624551
63.398790	1566.045775	20.629568
63.382215	1565.556229	20.634586
63.530196	1560.969711	20.639603
63.260025	1562.239898	20.644621
63.716769	1550.892277	20.649639
63.283010	1554.968494	20.654656
63.696802	1554.010714	20.659674
63.666761	1552.993078	20.664691
63.745995	1557.825252	20.669709
64.133318	1550.597570	20.674727
64.162429	1556.561118	20.679744
64.053007	1556.840395	20.684762
64.045568	1556.958519	20.689779
64.192211	1559.337418	20.694797
64.170971	1539.859194	20.699815
64.099954	1542.489954	20.704832
64.537679	1556.528703	20.709850
64.349909	1545.525073	20.714867
63.908715	1543.445177	20.719885
64.242157	1543.793930	20.724903
64.209774	1545.743262	20.729920
64.239947	1552.801761	20.734938
64.387062	1563.461829	20.739955
64.471710	1564.332425	20.744973
64.652529	1561.646963	20.749991
64.758267	1579.117779	20.755008
64.915868	1573.311548	20.760026
65.061020	1570.950425	20.765043
64.583778	1573.171440	20.770061
64.702353	1572.906886	20.775079
64.747958	1576.560847	20.780096
65.218960	1578.109407	20.785114
65.403956	1584.234744	20.790131
65.293163	1589.828883	20.795149
65.053120	1583.182343	20.800167
65.278446	1590.383859	20.805184
65.157551	1586.363351	20.810202
65.199163	1591.996733	20.815219
65.081459	1604.547713	20.820237
65.647704	1599.895653	20.825255
65.598474	1614.730302	20.830272
65.425614	1614.022231	20.835290
66.016305	1611.323041	20.840307
66.023776	1605.218412	20.845325
65.994647	1603.664115	20.850343
65.967128	1608.115377	20.855360
66.200483	1625.219086	20.860378
66.681761	1628.962598	20.865395
66.181510	1625.276086	20.870413
66.188064	1621.863641	20.875431
66.346067	1626.197473	20.880448
66.450124	1636.949542	20.885466
66.873985	1628.952358	20.890483
66.217322	1636.885401	20.895501
66.213825	1633.408253	20.900519
66.603324	1632.779341	20.905536
66.727880	1629.136956	20.910554
66.439312	1635.226047	20.915571
66.752819	1653.999361	20.920589
67.349973	1652.113395	20.925607
67.171731	1657.446708	20.930624
67.422748	1650.814730	20.935642
67.509573	1653.767934	20.940659
67.567144	1651.297439	20.945677
67.936175	1643.555006	20.950695
67.724207	1638.033886	20.955712
67.479975	1621.740173	20.960730
67.505784	1613.070019	20.965747
67.243618	1630.500691	20.970765
67.738027	1634.589305	20.975783
67.503564	1651.532792	20.980800
67.548756	1649.793268	20.985818
67.725951	1645.565089	20.990835
67.569882	1656.537816	20.995853
67.524263	1634.974050	21.000871
67.744709	1660.951264	21.005888
67.665476	1671.429097	21.010906
67.790070	1670.500842	21.015923
67.952852	1677.292447	21.020941
68.228416	1675.630442	21.025959
68.278564	1688.221458	21.030976
68.016372	1701.625168	21.035994
68.594496	1698.760666	21.041011
68.498544	1700.843059	21.046029
68.917476	1697.135603	21.051047
68.712177	1699.727461	21.056064
68.794993	1701.475714	21.061082
68.948176	1684.561070	21.066099
68.926804	1688.301292	21.071117
69.074923	1686.877017	21.076135
69.568778	1685.218683	21.081152
68.991206	1695.209685	21.086170
69.294073	1695.796775	21.091187
69.559753	1706.826539	21.096205
69.718779	1704.400105	21.101223
69.597191	1703.261096	21.106240
69.579528	1713.956539	21.111258
70.116548	1708.996587	21.116275
69.543045	1704.624062	21.121293
69.769804	1710.686091	21.126311
70.123677	1713.742641	21.131328
69.846215	1706.407600	21.136346
69.870044	1700.625443	21.141363
70.006290	1704.069558	21.146381
69.877266	1707.719347	21.151399
69.984073	1698.386328	21.156416
70.071702	1707.244266	21.161434
70.415071	1705.136109	21.166451
69.948254	1709.435303	21.171469
70.698769	1715.143860	21.176487
70.987101	1717.560545	21.181504
70.494723	1721.062125	21.186522
70.245565	1719.119388	21.191539
70.201111	1731.264482	21.196557
70.881517	1723.369082	21.201575
70.770623	1725.725233	21.206592
70.601313	1729.709561	21.211610
70.906625	1726.698439	21.216627
71.218550	1745.001854	21.221645
71.079338	1741.779491	21.226663
71.337348	1748.202732	21.231680
71.380876	1751.080680	21.236698
71.687826	1750.158566	21.241715
71.205147	1755.927794	21.246733
71.531207	1752.398990	21.251751
71.909774	1743.834460	21.256768
71.635946	1750.249503	21.261786
71.918570	1749.495313	21.266803
71.493977	1744.644984	21.271821
71.781874	1754.367871	21.276839
71.590302	1752.886351	21.281856
71.563125	1749.141475	21.286874
72.112099	1764.479007	21.291891
72.081138	1767.015157	21.296909
72.228615	1770.526957	21.301927
72.297567	1771.472610	21.306944
72.021107	1768.562098	21.311962
72.733548	1761.185558	21.316979
72.302215	1767.237096	21.321997
72.233116	1774.822508	21.327015
72.709158	1761.821143	21.332032
72.481234	1763.958935	21.337050
72.606960	1768.064315	21.342067
72.631992	1789.912727	21.347085
72.942378	1788.131641	21.352103
73.236007	1784.680499	21.357120
73.379858	1795.874582	21.362138
73.238400	1788.988443	21.367155
73.182163	1788.441986	21.372173
73.315171	1788.282471	21.377191
73.180959	1780.634603	21.382208
73.369848	1783.707546	21.387226
73.148271	1782.161293	21.392243
73.130451	1790.167893	21.397261
73.520488	1805.438839	21.402279
73.965274	1806.467630	21.407296
73.838188	1805.591424	21.412314
73.840098	1803.315833	21.417331
73.439853	1805.969809	21.422349
73.884943	1803.388084	21.427367
73.909251	1812.953472	21.432384
74.201079	1816.540502	21.437402
74.724866	1827.772915	21.442419
74.606561	1832.503560	21.447437
74.679480	1824.229892	21.452455
74.875525	1830.157910	21.457472
74.629387	1823.234506	21.462490
74.908087	1821.755046	21.467507
74.813365	1827.378301	21.472525
74.921935	1823.321788	21.477543
75.137692	1819.860749	21.482560
75.063872	1827.446922	21.487578
75.117381	1827.527095	21.492595
75.249628	1831.038138	21.497613
74.824767	1830.571525	21.502631
75.202619	1825.592296	21.507648
74.876283	1826.312686	21.512666
75.042909	1814.701064	21.517683
75.440717	1820.872040	21.522701
75.440005	1837.141567	21.527719
75.499140	1839.701483	21.532736
75.537053	1846.945090	21.537754
75.878368	1847.248433	21.542771
75.926082	1843.043649	21.547789
75.600535	1846.042557	21.552807
75.736147	1833.814048	21.557824
75.885752	1842.946384	21.562842
75.751429	1856.541628	21.567859
76.053437	1868.092854	21.572877
76.279391	1860.975543	21.577895
76.701172	1859.539939	21.582912
76.277246	1870.068736	21.587930
76.471090	1865.812649	21.592947
76.724524	1859.088691	21.597965
76.378149	1860.834771	21.602983
76.564466	1862.620476	21.608000
76.557189	1885.155766	21.613018
76.769458	1881.808878	21.618035
76.894890	1889.941411	21.623053
77.070582	1891.526799	21.628071
77.284047	1879.352338	21.633088
77.146044	1876.278094	21.638106
77.243063	1883.739689	21.643123
77.528434	1878.793870	21.648141
77.562969	1882.496969	21.653159
77.969357	1878.384316	21.658176
77.857425	1881.952561	21.663194
77.493551	1881.359619	21.668211
77.532434	1875.508770	21.673229
77.722044	1878.436440	21.678247
78.200502	1880.365738	21.683264
77.708365	1882.276678	21.688282
78.088759	1893.250712	21.693299
78.140452	1901.255939	21.698317
78.038223	1897.431266	21.703335
78.307797	1882.032026	21.708352
77.969409	1896.975332	21.713370
78.407119	1888.578205	21.718387
78.622140	1899.041630	21.723405
78.609396	1894.319251	21.728423
78.812316	1898.949090	21.733440
78.910721	1919.946664	21.738458
78.842613	1920.396210	21.743475
78.577007	1912.923517	21.748493
78.792748	1917.226282	21.753511
79.026827	1908.883141	21.758528
79.051145	1915.428269	21.763546
78.990509	1912.518634	21.768563
79.433825	1915.655888	21.773581
79.314145	1932.142969	21.778599
79.650829	1931.850550	21.783616
79.592508	1942.763953	21.788634
79.821457	1946.398733	21.793651
79.542046	1935.639611	21.798669
79.473998	1939.829041	21.803687
80.232441	1934.045332	21.808704
79.928293	1932.852853	21.813722
79.781724	1940.469408	21.818739
79.850227	1932.448864	21.823757
80.160579	1951.781603	21.828775
80.629519	1956.884212	21.833792
80.055956	1962.869730	21.838810
80.247511	1961.053592	21.843827
80.175876	1959.973016	21.848845
80.281989	1967.272264	21.853863
80.581553	1960.553665	21.858880
80.776612	1983.483442	21.863898
81.025522	1984.530309	21.868915
80.957529	1982.603344	21.873933
80.797107	1982.309906	21.878951
81.103492	1976.540199	21.883968
81.276484	1989.538246	21.888986
81.200956	1986.375294	21.894003
81.496549	1982.882779	21.899021
81.274794	1978.669686	21.904039
81.515643	1968.378183	21.909056
81.632377	1980.182588	21.914074
81.759053	2001.279977	21.919091
81.771921	2004.980184	21.924109
81.826492	2002.939332	21.929127
81.830284	2004.624252	21.934144
82.208903	2006.291475	21.939162
81.996017	2000.644145	21.944179
82.122537	2003.174590	21.949197
81.951259	2007.427551	21.954215
82.182823	2006.267909	21.959232
82.076890	2006.843313	21.964250
82.505101	2011.453665	21.969267
82.549765	2015.496056	21.974285
82.675002	2025.314009	21.979303
82.738759	2026.358327	21.984320
82.932112	2023.954877	21.989338
82.884383	2021.832214	21.994355
82.971152	2030.062394	21.999373
83.104007	2030.650884	22.004391
82.989141	2010.902772	22.009408
82.889378	2018.445750	22.014426
83.036045	2021.449604	22.019443
83.627610	2031.052477	22.024461
83.167342	2045.579467	22.029479
83.091953	2045.998597	22.034496
83.440628	2055.636381	22.039514
83.390528	2046.242551	22.044531
83.815237	2036.837457	22.049549
83.617657	2043.912896	22.054567
83.563710	2050.366185	22.059584
83.867625	2071.000353	22.064602
83.843531	2068.381637	22.069619
84.531358	2059.683292	22.074637
84.111577	2057.596823	22.079655
84.446605	2058.488180	22.084672
84.529486	2058.617405	22.089690
84.778161	2071.729896	22.094707
84.724965	2071.959342	22.099725
84.949070	2080.145936	22.104743
85.020704	2075.735364	22.109760
85.286344	2064.789775	22.114778
85.053180	2079.953451	22.119795
85.476631	2073.928668	22.124813
85.382575	2069.626113	22.129831
85.559982	2066.079510	22.134848
85.655238	2075.359346	22.139866
85.350959	2067.545481	22.144883
85.718831	2065.831107	22.149901
85.569840	2065.838858	22.154919
85.627813	2063.434521	22.159936
85.389906	2056.329842	22.164954
85.556188	2059.153891	22.169971
85.757480	2052.892501	22.174989
85.912682	2072.729398	22.180007
85.936369	2087.404679	22.185024
86.149687	2090.562218	22.190042
85.832811	2094.639178	22.195059
86.421405	2093.464623	22.200077
86.401312	2093.142885	22.205095
86.206290	2101.963245	22.210112
86.614699	2104.143404	22.215130
86.254243	2113.848136	22.220147
86.864890	2117.060203	22.225165
86.640243	2115.615395	22.230183
86.631211	2112.479875	22.235200
87.184795	2124.689342	22.240218
87.456129	2130.252185	22.245235
87.490927	2136.435961	22.250253
87.801367	2136.308610	22.255271
87.570836	2123.887939	22.260288
87.769926	2119.031318	22.265306
87.787007	2118.596450	22.270323
87.975212	2114.483210	22.275341
88.205968	2113.664543	22.280359
87.673121	2108.550184	22.285376
88.027782	2119.105478	22.290394
88.013417	2115.478448	22.295411
88.142693	2126.665553	22.300429
88.390255	2127.854664	22.305447
88.307693	2118.156587	22.310464
88.790348	2118.178995	22.315482
88.550560	2131.563734	22.320499
88.342683	2121.465533	22.325517
88.150852	2123.042246	22.330535
88.127396	2120.432890	22.335552
88.079368	2127.920468	22.340570
88.599070	2139.671313	22.345587
89.070525	2146.219060	22.350605
89.137516	2151.955948	22.355623
88.945864	2146.308401	22.360640
89.428860	2148.656775	22.365658
89.130738	2152.976984	22.370675
89.170415	2147.258477	22.375693
89.323170	2178.003238	22.380711
89.166715	2177.485094	22.385728
89.459048	2175.384880	22.390746
89.261537	2178.452152	22.395763
89.608533	2178.596808	22.400781
89.637178	2199.233223	22.405799
90.054773	2202.365089	22.410816
90.349718	2202.767230	22.415834
90.041654	2203.797222	22.420851
90.462861	2193.269034	22.425869
90.442650	2193.610088	22.430887
90.325879	2205.555376	22.435904
90.610220	2209.143659	22.440922
90.570149	2212.729116	22.445939
90.803017	2210.698180	22.450957
90.958207	2217.693169	22.455975
90.823199	2209.038454	22.460992
90.905068	2202.612670	22.466010
90.816071	2204.495198	22.471027
91.351924	2217.430248	22.476045
91.424779	2226.890413	22.481063
91.299882	2232.771009	22.486080
91.648202	2229.844592	22.491098
91.519055	2230.493074	22.496115
91.664216	2221.930170	22.501133
91.896548	2226.552330	22.506151
91.897370	2227.739075	22.511168
92.011442	2225.568946	22.516186
92.011875	2223.243036	22.521203
92.311015	2237.575457	22.526221
92.311806	2250.840534	22.531239
92.355313	2241.324630	22.536256
92.663359	2246.430438	22.541274
92.510826	2253.082298	22.546291
92.865283	2250.331658	22.551309
92.759096	2241.962771	22.556327
92.453408	2255.398956	22.561344
93.000987	2238.453560	22.566362
92.931907	2249.419332	22.571379
93.292658	2241.807340	22.576397
93.298670	2251.495760	22.581415
93.563759	2263.128773	22.586432
93.368460	2269.058283	22.591450
93.202073	2270.804607	22.596467
93.541404	2273.847753	22.601485
93.777200	2265.538895	22.606503
93.741820	2278.194224	22.611520
94.094267	2262.301950	22.616538
93.434893	2268.184236	22.621555
93.740951	2266.110267	22.626573
94.062607	2279.615455	22.631591
94.059718	2282.645941	22.636608
94.243738	2283.482067	22.641626
93.926692	2281.865512	22.646643
94.048139	2283.828697	22.651661
94.008175	2291.062592	22.656679
94.378747	2311.014346	22.661696
94.609679	2308.144182	22.666714
94.630348	2311.262509	22.671731
95.028366	2302.502146	22.676749
94.839924	2307.587918	22.681767
94.814404	2319.834595	22.686784
95.505539	2323.905173	22.691802
95.376715	2336.777172	22.696819
95.230780	2334.521521	22.701837
95.519978	2321.113486	22.706855
95.744327	2329.694669	22.711872
95.652346	2340.114923	22.716890
95.708280	2323.341158	22.721907
95.707274	2334.192165	22.726925
95.849614	2337.285122	22.731943
96.049213	2353.312275	22.736960
96.452134	2347.625165	22.741978
96.625167	2350.271461	22.746995
96.378196	2346.677671	22.752013
96.730842	2353.139958	22.757031
96.241786	2347.081307	22.762048
96.416733	2353.192702	22.767066
96.266616	2354.579845	22.772083
96.506856	2361.848771	22.777101
96.748844	2366.908153	22.782119
96.791841	2371.288590	22.787136
96.997665	2364.139517	22.792154
96.978120	2373.446962	22.797171
97.316713	2391.712145	22.802189
97.344635	2392.768411	22.807207
97.483617	2397.859720	22.812224
97.633212	2387.733769	22.817242
97.669593	2393.330349	22.822259
97.922212	2393.439296	22.827277
98.019682	2403.451172	22.832295
97.939128	2420.197685	22.837312
98.500260	2413.510529	22.842330
98.660711	2417.721081	22.847347
98.277100	2421.338310	22.852365
98.542903	2417.825130	22.857383
98.681114	2421.884519	22.862400
98.739596	2411.173167	22.867418
98.766638	2413.990682	22.872435
98.846008	2414.287734	22.877453
98.674660	2407.494411	22.882471
98.686635	2415.985819	22.887488
99.175198	2426.987422	22.892506
99.125561	2432.108292	22.897523
99.093880	2427.063660	22.902541
99.506069	2429.031808	22.907559
99.219307	2438.924004	22.912576
99.476905	2450.536220	22.917594
99.682494	2450.728282	22.922611
99.571054	2456.291231	22.927629
99.581876	2449.065368	22.932647
99.482529	2463.914882	22.937664
100.342072	2472.368211	22.942682
100.459217	2477.365125	22.947699
100.264573	2472.958300	22.952717
100.174724	2484.262018	22.957735
100.185551	2488.183573	22.962752
100.190840	2489.448538	22.967770
100.826462	2497.296268	22.972787
100.908434	2491.962385	22.977805
100.747949	2498.628206	22.982823
100.969382	2506.187345	22.987840
101.323303	2491.235165	22.992858
100.995979	2495.560030	22.997875
101.247765	2493.911147	23.002893
101.454800	2499.796636	23.007911
101.689686	2495.470848	23.012928
101.875299	2495.280993	23.017946
101.980916	2497.587544	23.022963
101.515162	2497.682795	23.027981
101.620307	2508.226913	23.032999
101.774174	2523.036805	23.038016
102.115365	2520.244017	23.043034
101.973518	2512.805337	23.048051
102.072238	2513.456002	23.053069
102.711445	2522.300518	23.058087
102.675158	2535.909321	23.063104
102.798026	2536.758196	23.068122
102.981029	2533.207468	23.073139
102.973649	2531.914798	23.078157
103.265065	2530.830962	23.083175
103.034334	2532.076098	23.088192
103.383591	2528.177399	23.093210
103.481563	2534.616529	23.098227
103.242334	2537.835580	23.103245
103.472499	2523.215220	23.108263
103.392144	2522.824012	23.113280
103.737566	2542.044586	23.118298
103.756979	2545.100027	23.123315
103.696062	2549.174862	23.128333
103.872298	2545.855590	23.133351
103.932249	2552.808821	23.138368
103.973875	2550.492196	23.143386
103.968044	2559.406228	23.148403
104.165450	2576.832093	23.153421
104.583606	2577.186535	23.158439
104.537502	2578.671021	23.163456
104.193956	2577.664569	23.168474
104.775838	2588.307631	23.173491
104.579342	2597.036935	23.178509
104.933355	2601.226675	23.183527
104.964133	2604.728518	23.188544
105.077030	2601.059359	23.193562
105.598804	2606.182284	23.198579
105.731133	2612.575029	23.203597
105.840736	2615.496419	23.208615
105.709153	2610.697786	23.213632
106.116965	2607.285411	23.218650
106.132269	2613.412438	23.223667
105.508606	2613.879605	23.228685
105.972840	2604.909885	23.233703
106.264397	2612.994627	23.238720
106.452045	2619.041001	23.243738
106.658626	2623.702016	23.248755
106.763896	2631.427747	23.253773
106.754377	2629.264307	23.258791
106.694738	2637.647106	23.263808
106.569204	2623.325416	23.268826
107.213611	2625.661192	23.273843
107.173199	2637.219221	23.278861
106.854376	2627.097087	23.283879
106.974957	2633.384371	23.288896
107.486690	2646.582316	23.293914
107.451460	2648.633211	23.298931
107.185924	2649.097925	23.303949
107.664632	2645.949021	23.308967
107.800809	2654.518924	23.313984
107.724711	2655.907118	23.319002
107.733568	2670.206460	23.324019
107.857437	2681.075986	23.329037
108.379662	2670.721064	23.334055
108.365851	2681.003022	23.339072
108.426112	2679.614528	23.344090
108.811857	2670.133150	23.349107
108.387697	2682.281564	23.354125
108.454247	2685.481140	23.359143
108.719648	2699.105924	23.364160
108.874698	2701.688811	23.369178
109.038162	2705.469722	23.374195
108.926389	2703.104518	23.379213
109.285773	2702.145739	23.384231
109.342189	2713.597119	23.389248
109.274357	2717.764603	23.394266
109.509017	2715.626021	23.399283
109.380111	2720.061880	23.404301
109.718354	2724.478207	23.409319
110.094135	2743.943578	23.414336
110.475553	2746.128047	23.419354
110.547086	2744.942933	23.424371
110.154397	2751.219143	23.429389
110.574521	2743.799633	23.434407
110.512331	2743.121520	23.439424
110.710224	2749.715505	23.444442
111.025691	2743.038312	23.449459
110.716636	2740.407332	23.454477
111.355812	2737.353206	23.459495
111.283551	2733.640437	23.464512
111.062512	2730.932545	23.469530
111.554945	2750.136622	23.474547
111.467121	2759.953640	23.479565
111.581663	2756.006448	23.484583
111.785777	2760.033495	23.489600
111.650476	2769.529714	23.494618
111.791447	2764.653621	23.499635
111.825575	2765.749967	23.504653
111.851687	2776.009944	23.509671
112.246385	2782.541546	23.514688
112.308065	2786.900220	23.519706
112.445618	2791.436379	23.524723
112.250871	2786.783310	23.529741
112.688990	2782.867479	23.534759
112.988250	2800.886747	23.539776
112.834744	2805.162359	23.544794
113.484913	2797.732036	23.549811
113.219104	2806.020967	23.554829
113.293856	2793.249009	23.559847
113.529775	2802.762835	23.564864
113.573872	2792.075604	23.569882
113.998146	2799.975517	23.574899
113.346942	2802.687889	23.579917
113.795588	2795.317545	23.584935
113.904566	2812.801681	23.589952
113.888502	2820.294007	23.594970
114.221983	2820.516537	23.599987
114.159444	2821.820558	23.605005
114.397556	2821.373138	23.610023
114.772651	2816.050047	23.615040
114.464336	2814.072269	23.620058
114.710524	2824.080018	23.625075
114.464423	2843.592428	23.630093
114.931473	2847.916013	23.635111
114.923424	2847.961649	23.640128
114.876484	2846.820339	23.645146
115.430331	2844.928417	23.650163
115.463495	2862.973655	23.655181
115.789071	2857.983398	23.660199
115.697295	2861.968452	23.665216
115.540038	2855.715615	23.670234
116.124084	2862.526889	23.675251
115.836748	2861.505302	23.680269
115.966283	2853.755687	23.685287
115.962050	2857.329345	23.690304
116.134504	2858.590240	23.695322
116.370879	2864.196664	23.700339
116.116824	2885.449427	23.705357
116.345230	2873.947379	23.710375
116.406493	2872.703898	23.715392
116.727711	2895.315238	23.720410
117.134896	2897.063290	23.725427
117.008112	2915.269355	23.730445
117.010389	2904.534954	23.735463
117.412076	2897.538045	23.740480
117.016117	2895.734955	23.745498
117.246870	2910.870834	23.750515
117.699053	2920.047845	23.755533
117.717089	2931.871496	23.760551
117.637065	2926.941609	23.765568
117.841517	2933.736632	23.770586
118.158060	2945.532462	23.775603
118.135306	2961.254123	23.780621
118.315109	2958.120434	23.785639
118.576909	2944.640480	23.790656
118.715466	2950.612595	23.795674
118.449204	2954.643943	23.800691
118.902204	2972.064867	23.805709
119.270221	2976.621778	23.810727
119.349625	2986.308564	23.815744
119.523347	2977.314738	23.820762
119.533953	2971.379589	23.825779
119.167393	2977.295132	23.830797
119.523231	2991.619273	23.835815
119.806803	2994.683905	23.840832
119.783195	3003.957594	23.845850
120.242786	3000.047821	23.850867
120.153437	2997.458131	23.855885
120.312632	3001.211367	23.860903
120.461649	3000.856806	23.865920
120.485109	3005.265708	23.870938
120.765526	3012.926288	23.875955
120.672838	3019.158746	23.880973
120.727823	3022.748408	23.885991
120.724319	3013.274179	23.891008
120.552354	3018.834158	23.896026
120.713226	3036.831157	23.901043
120.916850	3041.855711	23.906061
121.070563	3044.984883	23.911079
121.348279	3061.483332	23.916096
121.133015	3064.370473	23.921114
121.463149	3073.456216	23.926131
121.860643	3077.440414	23.931149
122.024735	3089.856750	23.936167
122.441144	3087.342466	23.941184
122.414260	3093.725608	23.946202
122.701930	3092.036331	23.951219
122.797346	3094.164651	23.956237
122.665618	3088.346450	23.961255
122.755651	3084.933273	23.966272
122.628781	3094.721871	23.971290
123.517729	3091.776900	23.976307
123.536846	3100.150732	23.981325
123.467359	3105.902994	23.986343
123.854389	3102.064536	23.991360
123.600249	3105.014586	23.996378
123.792291	3103.166698	24.001395
123.990025	3106.670888	24.006413
123.743293	3102.530879	24.011431
123.878669	3097.273668	24.016448
123.858875	3108.790895	24.021466
123.978079	3101.544634	24.026483
124.168096	3112.328308	24.031501
124.441152	3121.845954	24.036519
124.564750	3119.974067	24.041536
124.405962	3130.935493	24.046554
124.581547	3126.378972	24.051571
124.803266	3144.148765	24.056589
124.919741	3145.364795	24.061607
124.872270	3153.865864	24.066624
124.854417	3158.925149	24.071642
125.255212	3166.191343	24.076659
125.464517	3166.300770	24.081677
125.570959	3168.269560	24.086695
125.875095	3171.854937	24.091712
125.935425	3175.058731	24.096730
125.952658	3185.913707	24.101747
126.378919	3189.893423	24.106765
126.522914	3193.153550	24.111783
126.747585	3184.423077	24.116800
126.643204	3195.151923	24.121818
126.853693	3182.165894	24.126835
127.149263	3184.004055	24.131853
127.112087	3183.501912	24.136871
127.381459	3188.377331	24.141888
127.242084	3204.714007	24.146906
127.510675	3203.857803	24.151923
127.533717	3204.810725	24.156941
127.137538	3205.125482	24.161959
127.798331	3212.164742	24.166976
127.994637	3232.267917	24.171994
128.186221	3229.627867	24.177011
128.428728	3233.298662	24.182029
128.325131	3232.156735	24.187047
128.326605	3229.035156	24.192064
128.501565	3237.324667	24.197082
128.523258	3240.976401	24.202099
128.853195	3254.345308	24.207117
128.604558	3257.436553	24.212135
128.966545	3245.332590	24.217152
128.819025	3255.638980	24.222170
129.070114	3266.182772	24.227187
129.115100	3279.047150	24.232205
129.352726	3273.597119	24.237223
129.842549	3286.953626	24.242240
129.542686	3304.934699	24.247258
129.764214	3304.644524	24.252275
129.720526	3299.996062	24.257293
129.933233	3314.342885	24.262311
130.331851	3314.823501	24.267328
130.129695	3330.103306	24.272346
130.521678	3323.682195	24.277363
131.020243	3329.430752	24.282381
131.089027	3340.624935	24.287399
131.940694	3334.630494	24.292416
131.462633	3344.177557	24.297434
131.824099	3344.714495	24.302451
131.714766	3344.741281	24.307469
131.642778	3342.183540	24.312487
132.076167	3333.218294	24.317504
131.653304	3341.386886	24.322522
132.103402	3338.491693	24.327539
132.325677	3331.131348	24.332557
132.289311	3334.587040	24.337575
132.654885	3332.061749	24.342592
132.520338	3330.580630	24.347610
132.275703	3329.091509	24.352627
132.490372	3345.956755	24.357645
132.747526	3356.827903	24.362663
132.947369	3350.124413	24.367680
132.883958	3356.166180	24.372698
133.106386	3360.089493	24.377715
133.338653	3364.080704	24.382733
133.290578	3375.072276	24.387751
133.262119	3378.166921	24.392768
133.274385	3386.081142	24.397786
133.379770	3391.029652	24.402803
133.608771	3398.550107	24.407821
133.655683	3420.008849	24.412839
134.119291	3427.015961	24.417856
133.861007	3437.368214	24.422874
134.122776	3431.715506	24.427891
134.295404	3441.675154	24.432909
134.333419	3462.901775	24.437927
134.882525	3460.300369	24.442944
135.165801	3476.447979	24.447962
135.628052	3475.015383	24.452979
136.043662	3473.296559	24.457997
135.486934	3485.639876	24.463015
135.723042	3479.808108	24.468032
136.354269	3481.224428	24.473050
136.127619	3479.808227	24.478067
136.309167	3484.378700	24.483085
136.018883	3486.188738	24.488103
136.344400	3488.678749	24.493120
136.418563	3500.276194	24.498138
136.799070	3504.386246	24.503155
137.105594	3491.211353	24.508173
136.553433	3507.720285	24.513191
137.049313	3495.693025	24.518208
137.030510	3518.532014	24.523226
137.355186	3520.990599	24.528243
137.527446	3521.819159	24.533261
137.375334	3517.260222	24.538279
137.616583	3536.775936	24.543296
137.724696	3547.433825	24.548314
137.775736	3553.773358	24.553331
138.115201	3546.400878	24.558349
137.737226	3555.332673	24.563367
138.391249	3555.808002	24.568384
138.326139	3563.955365	24.573402
138.328340	3575.261126	24.578419
138.686081	3577.266342	24.583437
138.674746	3583.451530	24.588455
139.173409	3589.904014	24.593472
138.944903	3590.050473	24.598490
139.339912	3604.223776	24.603507
139.644522	3611.195899	24.608525
139.532834	3621.932456	24.613543
139.715564	3616.847587	24.618560
139.503532	3622.243587	24.623578
139.879775	3631.458111	24.628595
140.509552	3625.498339	24.633613
140.339696	3635.821070	24.638631
140.401536	3630.862452	24.643648
140.828113	3648.007258	24.648666
140.771622	3655.225351	24.653683
141.187076	3651.694802	24.658701
141.254645	3657.599366	24.663719
141.549602	3649.116477	24.668736
141.505386	3655.392061	24.673754
141.965448	3650.210077	24.678771
142.125027	3649.797036	24.683789
141.632695	3656.073386	24.688807
141.532105	3663.067978	24.693824
142.056944	3668.692589	24.698842
141.775159	3674.090062	24.703859
142.461140	3662.184413	24.708877
142.025490	3676.996078	24.713895
142.479008	3688.338520	24.718912
142.459133	3687.997781	24.723930
142.719873	3694.298198	24.728947
142.779927	3698.063956	24.733965
143.230478	3714.914687	24.738983
143.693411	3718.165976	24.744000
143.654183	3715.322134	24.749018
143.487640	3720.729974	24.754035
143.903499	3716.830058	24.759053
144.029042	3725.686208	24.764071
144.039686	3729.118828	24.769088
143.994717	3738.617185	24.774106
144.142530	3739.418022	24.779123
144.686532	3738.064133	24.784141
144.680273	3739.678194	24.789159
144.218299	3748.752652	24.794176
144.536853	3755.321792	24.799194
144.848471	3756.021214	24.804211
145.237850	3768.601573	24.809229
145.205875	3794.176372	24.814247
145.434370	3792.433176	24.819264
145.538147	3797.176887	24.824282
145.501626	3799.221801	24.829299
145.782306	3807.286693	24.834317
145.837622	3815.809846	24.839335
145.891481	3816.944198	24.844352
145.950265	3830.548551	24.849370
146.280328	3845.871665	24.854387
146.643056	3832.349989	24.859405
146.914429	3854.310662	24.864423
147.053212	3862.874419	24.869440
147.018240	3873.409725	24.874458
146.978915	3870.329147	24.879475
147.458290	3865.608062	24.884493
147.799019	3881.923791	24.889511
147.673713	3881.684788	24.894528
148.114385	3892.991494	24.899546
148.054989	3888.847204	24.904563
148.051965	3876.692690	24.909581
148.267048	3897.058798	24.914599
148.411825	3909.090491	24.919616
149.159409	3905.372137	24.924634
148.996679	3913.875839	24.929651
148.911051	3905.963788	24.934669
149.263193	3908.901049	24.939687
149.547082	3909.699514	24.944704
149.868786	3920.718708	24.949722
149.705003	3924.888876	24.954739
150.091502	3915.776029	24.959757
149.656527	3922.337026	24.964775
149.696060	3921.649244	24.969792
150.156566	3921.198522	24.974810
150.278136	3937.580199	24.979827
150.685340	3935.565951	24.984845
150.581669	3940.556833	24.989863
150.582959	3942.955667	24.994880
150.766289	3943.987678	24.999898
150.942589	3949.206149	25.004915
151.348472	3960.998119	25.009933
151.366354	3966.266665	25.014951
151.014053	3968.013868	25.019968
151.547922	3965.929270	25.024986
151.726073	3988.911598	25.030003
151.930878	3987.345696	25.035021
152.037593	3995.235917	25.040039
152.259941	3993.354784	25.045056
152.344472	3984.229239	25.050074
152.393948	3996.279077	25.055091
152.643756	4012.880617	25.060109
152.560234	4019.639100	25.065127
152.625978	4024.480365	25.070144
153.009633	4021.497628	25.075162
152.795222	4039.349254	25.080179
153.232806	4032.387320	25.085197
153.359791	4047.385748	25.090215
153.298162	4047.704918	25.095232
153.934864	4054.164353	25.100250
153.611297	4067.544710	25.105267
154.111166	4067.798008	25.110285
154.158040	4086.770302	25.115303
154.370963	4094.729151	25.120320
154.637891	4091.259664	25.125338
154.499952	4089.665383	25.130355
154.655167	4104.009216	25.135373
154.919919	4112.190370	25.140391
155.070793	4120.193671	25.145408
155.474884	4126.569630	25.150426
155.628601	4134.897602	25.155443
156.090817	4132.341281	25.160461
155.694045	4141.882338	25.165479
155.834034	4136.027543	25.170496
156.031394	4154.941612	25.175514
155.938019	4167.238049	25.180531
156.318127	4160.199848	25.185549
156.530332	4187.198368	25.190567
156.553416	4184.212121	25.195584
156.876989	4189.369713	25.200602
157.116402	4202.305293	25.205619
157.606346	4201.392272	25.210637
157.932726	4199.652642	25.215655
157.942986	4206.001949	25.220672
158.209724	4203.782415	25.225690
158.366037	4194.471915	25.230707
158.670547	4195.693280	25.235725
158.471064	4197.845837	25.240743
158.274560	4197.472788	25.245760
159.051050	4207.704400	25.250778
158.906660	4220.722218	25.255795
159.106313	4220.889982	25.260813
158.927438	4220.886629	25.265831
159.092947	4224.093070	25.270848
159.068426	4236.044185	25.275866
159.388288	4240.047120	25.280883
159.633600	4251.921251	25.285901
159.793019	4259.153105	25.290919
159.746260	4271.366555	25.295936
160.346725	4270.928620	25.300954
160.125897	4273.267603	25.305971
160.647461	4274.808489	25.310989
161.022103	4280.867161	25.316007
160.794120	4289.359166	25.321024
160.867917	4288.830136	25.326042
160.763877	4290.686828	25.331059
161.537740	4300.612731	25.336077
161.520458	4307.957511	25.341095
161.595629	4310.692028	25.346112
161.922528	4323.809690	25.351130
162.029970	4328.540340	25.356147
162.176231	4329.467705	25.361165
162.530645	4317.607263	25.366183
162.337516	4332.798117	25.371200
162.676173	4330.557832	25.376218
162.681159	4341.876261	25.381235
163.000795	4342.479759	25.386253
162.759829	4353.751503	25.391271
162.999265	4350.343091	25.396288
163.397370	4346.401633	25.401306
163.315051	4368.345743	25.406323
163.491687	4366.907324	25.411341
163.790294	4372.223546	25.416359
163.439808	4378.452668	25.421376
163.896679	4386.622787	25.426394
164.314004	4398.334339	25.431411
164.357519	4405.142505	25.436429
164.931710	4405.336820	25.441447
164.715180	4426.115196	25.446464
164.922412	4416.717694	25.451482
165.078869	4416.573426	25.456499
165.520840	4433.088431	25.461517
165.950510	4432.996054	25.466535
165.651967	4439.217059	25.471552
165.953618	4437.591756	25.476570
165.698460	4450.197812	25.481587
166.117165	4458.727467	25.486605
166.519220	4459.778902	25.491623
166.763286	4471.587087	25.496640
166.679308	4472.376923	25.501658
166.802761	4485.015226	25.506675
166.961792	4490.886794	25.511693
167.179204	4491.613632	25.516711
167.173794	4507.838955	25.521728
167.510576	4508.938497	25.526746
167.317915	4516.313993	25.531763
167.749984	4516.154954	25.536781
167.827977	4533.424654	25.541799
167.629708	4539.140729	25.546816
168.330018	4540.394805	25.551834
168.607353	4556.073995	25.556851
168.533321	4567.449135	25.561869
168.969324	4566.295186	25.566887
168.575652	4571.303265	25.571904
169.246157	4581.087691	25.576922
169.581233	4582.601005	25.581939
169.600186	4579.722661	25.586957
170.019048	4599.546284	25.591975
170.432702	4603.171609	25.596992
170.600415	4599.843830	25.602010
170.704130	4602.163576	25.607027
170.627307	4600.231399	25.612045
171.134219	4592.494521	25.617063
171.128731	4595.140709	25.622080
171.563138	4591.607013	25.627098
171.263970	4595.198811	25.632115
171.409169	4611.571083	25.637133
171.731567	4616.122935	25.642151
171.476330	4620.285494	25.647168
171.882305	4615.664100	25.652186
171.936813	4627.533648	25.657203
171.993347	4621.616015	25.662221
172.503524	4633.543598	25.667239
172.089186	4641.660929	25.672256
172.574128	4647.822392	25.677274
172.760324	4656.899921	25.682292
173.043016	4659.302112	25.687309
173.065983	4667.284659	25.692327
173.324387	4678.768770	25.697344
173.707843	4679.267586	25.702362
173.887866	4688.674375	25.707380
173.761381	4686.895168	25.712397
174.069634	4691.411377	25.717415
173.765493	4709.662812	25.722432
174.412106	4710.600193	25.727450
174.288132	4714.960009	25.732468
174.423576	4738.398202	25.737485
174.854822	4738.627543	25.742503
174.657732	4744.545514	25.747520
174.768907	4752.126028	25.752538
174.943752	4763.304474	25.757556
175.181900	4769.368911	25.762573
175.738400	4781.825944	25.767591
175.875421	4796.529862	25.772608
175.620124	4795.651496	25.777626
175.930523	4810.476620	25.782644
176.342920	4814.493595	25.787661
176.410822	4823.192016	25.792679
176.546978	4847.356241	25.797696
176.765869	4845.573416	25.802714
176.866481	4848.954275	25.807732
176.874831	4865.995306	25.812749
177.392646	4866.536210	25.817767
177.257863	4882.207645	25.822784
177.820346	4893.871525	25.827802
178.176729	4891.865137	25.832820
177.867374	4898.207940	25.837837
178.634844	4910.751959	25.842855
178.386924	4920.869846	25.847872
178.713705	4915.818866	25.852890
179.371615	4924.248138	25.857908
179.296067	4935.642684	25.862925
180.181074	4926.062981	25.867943
179.599441	4930.440884	25.872960
180.050105	4928.776413	25.877978
179.954383	4937.588906	25.882996
180.404871	4949.586023	25.888013
180.390330	4951.447699	25.893031
180.454347	4960.620278	25.898048
180.723216	4953.340363	25.903066
180.838329	4955.197511	25.908084
180.821391	4985.036137	25.913101
181.590698	4983.195479	25.918119
181.365547	4981.254933	25.923136
181.357491	4989.463441	25.928154
181.432362	5006.980292	25.933172
181.599147	5009.391219	25.938189
182.146208	5016.720476	25.943207
181.839417	5028.656357	25.948224
182.167077	5035.167720	25.953242
182.572624	5043.036834	25.958260
182.252289	5050.719795	25.963277
182.745023	5062.382085	25.968295
182.853498	5077.090702	25.973312
183.258783	5081.194079	25.978330
183.255215	5091.589437	25.983348
183.555914	5104.803310	25.988365
184.055391	5097.405140	25.993383
183.960357	5117.287740	25.998400
184.364824	5125.179156	26.003418
184.591235	5128.552986	26.008436
184.675535	5135.370819	26.013453
184.894759	5137.233772	26.018471
184.791916	5151.268479	26.023488
184.986493	5158.204778	26.028506
185.453630	5165.691820	26.033524
185.362444	5182.171083	26.038541
185.828053	5179.838207	26.043559
185.619938	5182.023795	26.048576
185.756777	5191.955291	26.053594
186.102949	5199.666476	26.058612
186.092434	5200.343823	26.063629
186.706922	5200.784367	26.068647
186.952534	5217.709642	26.073664
187.082294	5229.349988	26.078682
187.317813	5225.676874	26.083700
187.721392	5223.764068	26.088717
188.046721	5221.648873	26.093735
188.254849	5237.124844	26.098752
188.343953	5239.920451	26.103770
188.484238	5241.246533	26.108788
188.625381	5241.284585	26.113805
188.860921	5238.432182	26.118823
188.933764	5235.538979	26.123840
188.735201	5233.641589	26.128858
189.360244	5241.754185	26.133876
189.440270	5252.401694	26.138893
189.771532	5255.598135	26.143911
189.382873	5261.659922	26.148928
189.777960	5270.730286	26.153946
190.020460	5281.008288	26.158964
190.095747	5286.965835	26.163981
190.171403	5297.339430	26.168999
190.320260	5312.007188	26.174016
190.713836	5310.793553	26.179034
191.203905	5330.834097	26.184052
191.086557	5341.241109	26.189069
191.213071	5336.196136	26.194087
191.456003	5351.622560	26.199104
191.502521	5373.045792	26.204122
191.627523	5364.585578	26.209140
191.888785	5390.151405	26.214157
192.154675	5395.299440	26.219175
192.172626	5404.731990	26.224192
192.412247	5424.208955	26.229210
193.010877	5426.350260	26.234228
192.719346	5445.512722	26.239245
193.278206	5440.898738	26.244263
193.100900	5445.424914	26.249280
193.023986	5472.852591	26.254298
193.318131	5484.606240	26.259316
193.150085	5497.660241	26.264333
194.294278	5513.807376	26.269351
194.847494	5523.926356	26.274368
194.696865	5526.185052	26.279386
195.095967	5528.105096	26.284404
194.933706	5536.884108	26.289421
195.104277	5539.903748	26.294439
195.507491	5545.623764	26.299456
195.696391	5561.788019	26.304474
196.157920	5559.506242	26.309492
196.331157	5565.779985	26.314509
196.274805	5561.956815	26.319527
197.021457	5575.492593	26.324544
196.899774	5579.965896	26.329562
197.059993	5582.652558	26.334580
196.894479	5592.783159	26.339597
197.267603	5598.151203	26.344615
197.601362	5606.255932	26.349632
197.541772	5608.478280	26.354650
197.811359	5604.531437	26.359668
198.032996	5630.362655	26.364685
198.146066	5629.887413	26.369703
198.366406	5636.418961	26.374720
198.608046	5650.583172	26.379738
199.354521	5640.876440	26.384756
199.602559	5649.976344	26.389773
199.484056	5645.938769	26.394791
199.497529	5636.422631	26.399808
199.693130	5649.069380	26.404826
200.541372	5654.808100	26.409844
200.529242	5666.013236	26.414861
200.455706	5666.498446	26.419879
200.906213	5670.396003	26.424896
200.890471	5679.379412	26.429914
200.791905	5666.809360	26.434932
200.691333	5667.270395	26.439949
201.256123	5677.030943	26.444967
201.386680	5677.222176	26.449984
201.488532	5688.453663	26.455002
201.887155	5697.798318	26.460020
201.870851	5710.481464	26.465037
202.134365	5720.838496	26.470055
202.519598	5733.351425	26.475072
202.700203	5739.930273	26.480090
202.734505	5740.707947	26.485108
202.974443	5761.293221	26.490125
202.983232	5768.445104	26.495143
203.169749	5770.928803	26.500160
203.219025	5778.683589	26.505178
203.484709	5784.703016	26.510196
203.517186	5794.714324	26.515213
203.679702	5811.280678	26.520231
204.328812	5818.584805	26.525248
204.161887	5843.975281	26.530266
204.554139	5841.600152	26.535284
204.548585	5866.703374	26.540301
205.041369	5873.227051	26.545319
205.316255	5890.902820	26.550336
205.173025	5898.100665	26.555354
205.520564	5913.021886	26.560372
205.778872	5932.512250	26.565389
206.214792	5932.545162	26.570407
206.746829	5940.862047	26.575424
206.701207	5949.064244	26.580442
207.035867	5951.104915	26.585460
207.195032	5972.233411	26.590477
207.311765	5977.322903	26.595495
207.372202	5973.064663	26.600512
207.654219	5984.643759	26.605530
208.191032	5984.275744	26.610548
208.371605	5998.658137	26.615565
208.270326	6012.974209	26.620583
208.636989	6018.857938	26.625600
208.514848	6031.961949	26.630618
208.890261	6037.089852	26.635636
208.986943	6051.368628	26.640653
209.395089	6060.592022	26.645671
209.820721	6069.193959	26.650688
209.858276	6076.780243	26.655706
210.167534	6086.268525	26.660724
210.353962	6094.096662	26.665741
210.402433	6097.454355	26.670759
211.023349	6107.089542	26.675776
210.784441	6131.304754	26.680794
211.548117	6116.054969	26.685812
211.477099	6129.533008	26.690829
211.550053	6138.884714	26.695847
212.165934	6143.138435	26.700864
211.984264	6151.204198	26.705882
212.358268	6151.865537	26.710900
212.875950	6149.423368	26.715917
213.211092	6167.696064	26.720935
213.303937	6162.602473	26.725952
212.984684	6170.598251	26.730970
213.560857	6154.658066	26.735988
213.706964	6178.727793	26.741005
213.775920	6187.919155	26.746023
214.034357	6183.986562	26.751040
214.143117	6190.002296	26.756058
214.294425	6192.078032	26.761076
214.168893	6193.493178	26.766093
213.943129	6207.301723	26.771111
214.864906	6211.226586	26.776128
214.899944	6233.722772	26.781146
215.217558	6236.391188	26.786164
215.316578	6263.606238	26.791181
215.649158	6262.108520	26.796199
215.995145	6278.883314	26.801216
216.065030	6287.506360	26.806234
216.080818	6277.654907	26.811252
216.439400	6301.445280	26.816269
216.582117	6310.401017	26.821287
216.979659	6329.270202	26.826304
217.041061	6348.848679	26.831322
217.433628	6343.749123	26.836340
217.916110	6362.781817	26.841357
217.830260	6367.271795	26.846375
218.277338	6370.807010	26.851392
218.148989	6390.734095	26.856410
218.484276	6388.983398	26.861428
218.792482	6401.032176	26.866445
218.698890	6412.847166	26.871463
219.023935	6424.713384	26.876480
219.611287	6437.119370	26.881498
219.734566	6443.732707	26.886516
219.941776	6442.219889	26.891533
220.223119	6463.342439	26.896551
220.443979	6467.165657	26.901568
220.622101	6494.201347	26.906586
220.970778	6488.006897	26.911604
221.053078	6488.123622	26.916621
221.176639	6504.908213	26.921639
221.381850	6512.979819	26.926656
221.748008	6529.795879	26.931674
222.188969	6534.418033	26.936692
222.515939	6540.728009	26.941709
222.371617	6544.930448	26.946727
222.976319	6555.720657	26.951744
222.928770	6565.192477	26.956762
223.222958	6565.358087	26.961780
223.299014	6567.657162	26.966797
223.425191	6577.925707	26.971815
223.912483	6582.215462	26.976832
224.007649	6597.823930	26.981850
224.346584	6605.546317	26.986868
224.486620	6597.544078	26.991885
224.527659	6607.614469	26.996903
224.870894	6622.625336	27.001920
225.214583	6628.569685	27.006938
225.346849	6637.397789	27.011956
225.838666	6646.816725	27.016973
225.666898	6655.667211	27.021991
226.026773	6661.448037	27.027008
226.335110	6672.830878	27.032026
226.252068	6675.991457	27.037044
226.545736	6694.814155	27.042061
226.816879	6701.142402	27.047079
227.248943	6714.134825	27.052096
227.486088	6733.496770	27.057114
227.748939	6734.513330	27.062132
228.186636	6745.689697	27.067149
227.770013	6757.287180	27.072167
228.162932	6743.796511	27.077184
228.262884	6764.865747	27.082202
228.222329	6778.813020	27.087220
228.325009	6787.557439	27.092237
228.716075	6806.544936	27.097255
229.124269	6814.464915	27.102272
229.361449	6839.774522	27.107290
229.536910	6848.103487	27.112308
229.712324	6854.377333	27.117325
230.060273	6868.137537	27.122343
230.383738	6874.612335	27.127360
230.799054	6885.473448	27.132378
230.832631	6878.264359	27.137396
231.529945	6892.828525	27.142413
231.709610	6907.353834	27.147431
232.024852	6907.089969	27.152448
232.072740	6909.049399	27.157466
232.350324	6920.977041	27.162484
232.122168	6933.088095	27.167501
232.394744	6942.579412	27.172519
233.420660	6944.953874	27.177536
233.212108	6956.503102	27.182554
233.627843	6960.097011	27.187572
234.210806	6967.626635	27.192589
233.636846	6975.665819	27.197607
234.112893	6976.301735	27.202624
234.475628	6987.559445	27.207642
234.436498	6999.082159	27.212660
234.778229	7002.965477	27.217677
234.663138	7007.090833	27.222695
235.288028	7020.523646	27.227712
235.330451	7027.831754	27.232730
235.387512	7051.383057	27.237748
235.859583	7055.255439	27.242765
235.780533	7070.178137	27.247783
236.818637	7086.002350	27.252800
236.645937	7087.677506	27.257818
236.676631	7102.983968	27.262836
237.584255	7109.231590	27.267853
237.396567	7129.288734	27.272871
237.372967	7144.534283	27.277888
237.943224	7140.139082	27.282906
238.065612	7159.292155	27.287924
238.137110	7155.688550	27.292941
238.145494	7172.242397	27.297959
238.642715	7185.947887	27.302976
238.670203	7202.514553	27.307994
239.051923	7210.173668	27.313012
239.432676	7224.923439	27.318029
239.868214	7236.605557	27.323047
240.280041	7248.041996	27.328064
240.575215	7264.753044	27.333082
240.823705	7264.464906	27.338100
240.993791	7252.644076	27.343117
241.328562	7270.469644	27.348135
241.630204	7282.835726	27.353152
241.539550	7282.742779	27.358170
241.920167	7289.183516	27.363188
242.242464	7302.758648	27.368205
241.999177	7310.752489	27.373223
242.342477	7320.542305	27.378240
242.788322	7330.518107	27.383258
243.188255	7328.394147	27.388276
243.681221	7341.617404	27.393293
243.758769	7352.544336	27.398311
243.816758	7362.221021	27.403328
244.233576	7354.673896	27.408346
244.284733	7365.131424	27.413364
244.777011	7357.405157	27.418381
244.540929	7369.880791	27.423399
245.094124	7369.585958	27.428416
245.096939	7374.087547	27.433434
244.909200	7392.515987	27.438452
245.395085	7389.848183	27.443469
245.381597	7406.342527	27.448487
245.716814	7411.694948	27.453504
246.205892	7427.984304	27.458522
246.005690	7439.983974	27.463540
246.164103	7451.946415	27.468557
246.679248	7474.940324	27.473575
246.762446	7492.606627	27.478592
247.202601	7501.099628	27.483610
247.422504	7521.068090	27.488628
247.571859	7531.822872	27.493645
247.786331	7560.079352	27.498663
248.180448	7562.306628	27.503680
248.932325	7584.253347	27.508698
248.340497	7585.425944	27.513716
248.895949	7595.672009	27.518733
249.372304	7612.942194	27.523751
249.425926	7628.349683	27.528768
249.892309	7637.653148	27.533786
250.150318	7664.302360	27.538804
250.631617	7665.679381	27.543821
250.649239	7688.240057	27.548839
251.287823	7693.283004	27.553856
251.498590	7696.748161	27.558874
251.926950	7704.801121	27.563892
252.316099	7712.686590	27.568909
252.005934	7725.142498	27.573927
252.434944	7736.194550	27.578944
253.011067	7742.484854	27.583962
252.869478	7747.189105	27.588980
253.021817	7754.133009	27.593997
253.572123	7768.683019	27.599015
253.653120	7771.432928	27.604032
253.789157	7781.347013	27.609050
253.952505	7798.053940	27.614068
254.053313	7804.986993	27.619085
254.371085	7819.062028	27.624103
254.449126	7839.747610	27.629120
254.813684	7853.019766	27.634138
254.942603	7871.588501	27.639156
255.335227	7873.822363	27.644173
255.819102	7897.989811	27.649191
256.237789	7908.658423	27.654208
256.624965	7928.238060	27.659226
256.160073	7933.179273	27.664244
257.067174	7952.248127	27.669261
257.127339	7957.151293	27.674279
257.525376	7967.895786	27.679296
257.872712	7985.559068	27.684314
257.724968	7987.536631	27.689332
258.347803	8011.240468	27.694349
258.441537	8008.703465	27.699367
258.785001	8014.357851	27.704384
259.003651	8026.551167	27.709402
259.114181	8041.962714	27.714420
259.435951	8052.782347	27.719437
259.435151	8059.791397	27.724455
259.804642	8073.950081	27.729472
260.165747	8099.301992	27.734490
260.396278	8116.942655	27.739508
260.864207	8111.609815	27.744525
261.197017	8129.989015	27.749543
261.228517	8144.551139	27.754560
261.755415	8141.542153	27.759578
261.756196	8163.856637	27.764596
261.797184	8169.321671	27.769613
262.577674	8179.245514	27.774631
262.553053	8181.497421	27.779648
263.070042	8184.567417	27.784666
262.698590	8201.023833	27.789684
263.192546	8211.077821	27.794701
263.138026	8225.025218	27.799719
263.339726	8232.046811	27.804736
263.867950	8256.889719	27.809754
263.952106	8270.938554	27.814772
264.349351	8278.999798	27.819789
265.077335	8296.029151	27.824807
264.779436	8314.838836	27.829824
265.548339	8320.900240	27.834842
265.130208	8341.799866	27.839860
265.608967	8349.188530	27.844877
266.100447	8372.799752	27.849895
266.184419	8378.198129	27.854912
266.759230	8397.502614	27.859930
266.732025	8413.940020	27.864948
267.100367	8425.702879	27.869965
267.503946	8444.301778	27.874983
267.718448	8461.806366	27.880000
268.278236	8465.207522	27.885018
268.226266	8487.795861	27.890036
268.283687	8492.611199	27.895053
268.910835	8503.891562	27.900071
269.139917	8531.323218	27.905088
269.433706	8539.725972	27.910106
269.658040	8547.877564	27.915124
270.477693	8563.292118	27.920141
270.772761	8573.004914	27.925159
270.711651	8588.961581	27.930176
271.421505	8591.616259	27.935194
271.091268	8598.200385	27.940212
271.608641	8609.138091	27.945229
271.935765	8628.191157	27.950247
272.179307	8626.280983	27.955264
272.390563	8641.696194	27.960282
272.062356	8645.504850	27.965300
272.498478	8660.029253	27.970317
273.173509	8677.367187	27.975335
273.581900	8684.220815	27.980352
273.808714	8693.865437	27.985370
274.079975	8708.251528	27.990388
274.615712	8703.952932	27.995405
275.099185	8721.718723	28.000423
274.840938	8732.923235	28.005440
275.423750	8722.959552	28.010458
275.211271	8747.429786	28.015476
275.979745	8750.997209	28.020493
276.095504	8760.264612	28.025511
276.392668	8783.843655	28.030528
276.677464	8784.481188	28.035546
276.324120	8803.328467	28.040564
276.852607	8816.550379	28.045581
276.828596	8826.168060	28.050599
277.025514	8844.929182	28.055616
277.332332	8860.800032	28.060634
277.885207	8878.940284	28.065652
278.209521	8899.339050	28.070669
278.518019	8901.974559	28.075687
278.730057	8917.986594	28.080704
279.372166	8937.211644	28.085722
279.427536	8949.140681	28.090740
279.924932	8963.137936	28.095757
280.119106	8970.211505	28.100775
280.487131	8975.786566	28.105792
281.239677	8972.590554	28.110810
280.888920	8988.397188	28.115828
281.445532	9007.673591	28.120845
281.441149	9002.089290	28.125863
281.673659	9008.951647	28.130880
282.294352	9014.329278	28.135898
282.609323	9019.922135	28.140916
282.523899	9032.526833	28.145933
282.847291	9041.038839	28.150951
282.809347	9047.596279	28.155968
282.832977	9054.712382	28.160986
283.183893	9079.479983	28.166004
283.531476	9101.895975	28.171021
283.741489	9111.660265	28.176039
283.907536	9134.619369	28.181056
284.328857	9151.738597	28.186074
285.010206	9166.401791	28.191092
284.975781	9180.523565	28.196109
285.512029	9200.175917	28.201127
285.662768	9216.813484	28.206144
285.909019	9237.868937	28.211162
286.235112	9251.299674	28.216180
286.504450	9269.137424	28.221197
286.746290	9277.539179	28.226215
286.924501	9310.110564	28.231232
287.411136	9314.738901	28.236250
287.774029	9331.463314	28.241268
287.730140	9350.767838	28.246285
288.416247	9361.521694	28.251303
288.330372	9387.049579	28.256320
288.553917	9395.965739	28.261338
289.177014	9409.893124	28.266356
289.454122	9435.395788	28.271373
289.851505	9449.298572	28.276391
290.199865	9462.451287	28.281408
290.416983	9476.063439	28.286426
290.997758	9490.884725	28.291444
291.244129	9498.828058	28.296461
291.754128	9512.593269	28.301479
291.939220	9536.137150	28.306496
292.023910	9549.141790	28.311514
292.240791	9561.942605	28.316532
292.596662	9568.675339	28.321549
293.016014	9582.038032	28.326567
293.345328	9596.781972	28.331584
293.759676	9611.136878	28.336602
294.215348	9618.018179	28.341620
293.835566	9633.836220	28.346637
294.438323	9635.213315	28.351655
294.523568	9661.715653	28.356672
295.060233	9677.150211	28.361690
295.182914	9689.779587	28.366708
295.223151	9705.351923	28.371725
295.830239	9727.715390	28.376743
296.040549	9739.920614	28.381760
296.210498	9762.829364	28.386778
296.767757	9768.015082	28.391796
297.168603	9782.754279	28.396813
297.542548	9801.466534	28.401831
297.671231	9821.855913	28.406848
297.816125	9830.443605	28.411866
298.036029	9848.381218	28.416884
298.528664	9865.549924	28.421901
298.917885	9875.194980	28.426919
299.242051	9881.784396	28.431936
299.474080	9908.122008	28.436954
299.645363	9910.327649	28.441972
299.997530	9921.487772	28.446989
299.921944	9928.575547	28.452007
300.162918	9944.328184	28.457024
300.677167	9947.493634	28.462042
301.075614	9970.054261	28.467060
301.205454	9987.273596	28.472077
301.607526	9997.431361	28.477095
301.969828	10018.400056	28.482112
302.310223	10041.512940	28.487130
302.665855	10038.877803	28.492148
302.511430	10059.305475	28.497165
303.217664	10075.872579	28.502183
303.229739	10097.082512	28.507200
303.417958	10102.367181	28.512218
303.927670	10127.509140	28.517236
304.065148	10145.782010	28.522253
304.829254	10157.881813	28.527271
305.226591	10167.642574	28.532288
305.360674	10177.242502	28.537306
306.009282	10198.681215	28.542324
305.772579	10213.542726	28.547341
306.367758	10217.690144	28.552359
306.631189	10241.383674	28.557376
307.173837	10251.361684	28.562394
307.223480	10268.748558	28.567412
307.646080	10276.967734	28.572429
308.110398	10294.974845	28.577447
308.204981	10318.710710	28.582464
308.380775	10325.655062	28.587482
309.186669	10337.552673	28.592500
309.286817	10359.611099	28.597517
309.338270	10367.364313	28.602535
309.731252	10388.432816	28.607552
309.667923	10390.760517	28.612570
310.331358	10407.489339	28.617588
310.675797	10426.841501	28.622605
311.492688	10444.686172	28.627623
311.797183	10462.304848	28.632640
311.908615	10475.545915	28.637658
312.314241	10482.075422	28.642676
312.232818	10489.660052	28.647693
312.604299	10502.620432	28.652711
312.862896	10526.978158	28.657728
313.347338	10545.143391	28.662746
313.672183	10549.993150	28.667764
314.079935	10573.329799	28.672781
314.256093	10581.275121	28.677799
314.613197	10591.206598	28.682816
314.551505	10607.013522	28.687834
315.277326	10628.743758	28.692852
315.205899	10644.688012	28.697869
315.739569	10657.206299	28.702887
316.301704	10673.799668	28.707904
316.249943	10685.209817	28.712922
316.453398	10700.429032	28.717940
317.350004	10720.427552	28.722957
317.677643	10736.887203	28.727975
317.940461	10755.393639	28.732992
318.244928	10751.178173	28.738010
318.974353	10748.544378	28.743028
319.675006	10749.328398	28.748045
319.878753	10745.068717	28.753063
319.963579	10756.539611	28.758080
320.406724	10758.952214	28.763098
320.770152	10768.286019	28.768116
320.930946	10770.884943	28.773133
321.206519	10774.201596	28.778151
321.203508	10780.476307	28.783168
321.257895	10784.086529	28.788186
321.913514	10793.756641	28.793204
322.056122	10807.381438	28.798221
322.517247	10806.494744	28.803239
322.244002	10819.647907	28.808256
322.601953	10841.660204	28.813274
322.796953	10854.901079	28.818292
323.045583	10870.435428	28.823309
323.714211	10887.609086	28.828327
323.572556	10907.382065	28.833344
323.824150	10924.725283	28.838362
323.923305	10947.495013	28.843380
324.029939	10977.649185	28.848397
324.636251	10987.996529	28.853415
325.124697	11019.695014	28.858432
325.476193	11049.902516	28.863450
326.027193	11071.638550	28.868468
325.957490	11093.149764	28.873485
325.990147	11103.703864	28.878503
326.310914	11136.944464	28.883520
327.084733	11176.618843	28.888538
327.444960	11190.231933	28.893556
327.529404	11209.777198	28.898573
328.287280	11226.356185	28.903591
328.460109	11252.584975	28.908608
329.075022	11269.388483	28.913626
329.644865	11287.828406	28.918644
329.802954	11309.601003	28.923661
330.169406	11322.802721	28.928679
330.468847	11338.560007	28.933696
331.018217	11352.411986	28.938714
331.589575	11361.391438	28.943732
331.560040	11384.194486	28.948749
332.035659	11404.632290	28.953767
332.468332	11408.710704	28.958784
332.551247	11441.629129	28.963802
333.000406	11452.692877	28.968820
333.095712	11462.119552	28.973837
333.909320	11480.704626	28.978855
334.136211	11494.203044	28.983872
334.327321	11509.661676	28.988890
334.980943	11524.271083	28.993908
335.032540	11544.210235	28.998925
335.582827	11549.811205	29.003943
335.993602	11569.343619	29.008960
336.010396	11581.551941	29.013978
336.588068	11592.538803	29.018996
336.365013	11612.255804	29.024013
337.085433	11628.626294	29.029031
337.537045	11642.108563	29.034048
337.686263	11659.724271	29.039066
338.063037	11671.645751	29.044084
338.584141	11692.664077	29.049101
339.012833	11705.591069	29.054119
339.089631	11722.394018	29.059136
339.511122	11742.850143	29.064154
340.074863	11753.791917	29.069172
340.194472	11767.038931	29.074189
340.220680	11779.754299	29.079207
340.875574	11801.743313	29.084224
340.936338	11818.820425	29.089242
340.959955	11835.000260	29.094260
341.705973	11863.366314	29.099277
341.936984	11875.519167	29.104295
342.250382	11891.325255	29.109312
342.725982	11917.870686	29.114330
343.228016	11933.656734	29.119348
343.688924	11955.215284	29.124365
343.391723	11971.966520	29.129383
343.950185	11972.434993	29.134400
344.695401	11983.954763	29.139418
345.057667	11988.827457	29.144436
345.545095	12004.619011	29.149453
345.802675	12012.624815	29.154471
346.131694	12019.116340	29.159488
346.325424	12036.232818	29.164506
346.791384	12042.548169	29.169524
346.703987	12060.333943	29.174541
347.384105	12071.876595	29.179559
347.419532	12087.211674	29.184576
347.418974	12107.488001	29.189594
348.160053	12118.711672	29.194612
348.616567	12143.498373	29.199629
349.040565	12163.278799	29.204647
349.113792	12180.786903	29.209664
349.280327	12205.464377	29.214682
350.076296	12222.938253	29.219700
350.507396	12230.241202	29.224717
350.683996	12248.971032	29.229735
350.659424	12270.009166	29.234752
350.841624	12297.305282	29.239770
351.443048	12322.318986	29.244788
351.548206	12350.303017	29.249805
351.842629	12378.740589	29.254823
352.271949	12397.345718	29.259840
352.773666	12425.845624	29.264858
353.331938	12439.207552	29.269876
353.719087	12461.378223	29.274893
354.173443	12484.921526	29.279911
354.675055	12500.319703	29.284928
354.787394	12530.273368	29.289946
355.256066	12541.947325	29.294964
355.284912	12555.408055	29.299981
355.623099	12579.260194	29.304999
356.368303	12596.047642	29.310016
356.373693	12636.653886	29.315034
357.196652	12651.341858	29.320052
357.695897	12671.489974	29.325069
357.838396	12688.394019	29.330087
358.336302	12707.358182	29.335104
358.280806	12729.225876	29.340122
358.821712	12742.976001	29.345140
358.987057	12770.480702	29.350157
359.441049	12784.032893	29.355175
359.989753	12802.818669	29.360192
360.109718	12824.403200	29.365210
360.931889	12846.711445	29.370228
361.057774	12873.644583	29.375245
361.446193	12886.433433	29.380263
361.806519	12904.273026	29.385280
361.984724	12921.102212	29.390298
362.655057	12942.439613	29.395316
362.864711	12956.532310	29.400333
363.026417	12987.454761	29.405351
363.556748	13002.615165	29.410368
363.620405	13022.516095	29.415386
363.996285	13047.929253	29.420404
364.620863	13065.392865	29.425421
364.836640	13093.029085	29.430439
365.415117	13117.185322	29.435456
365.503355	13132.187708	29.440474
366.173453	13158.745474	29.445492
366.591574	13174.886767	29.450509
366.668563	13195.199482	29.455527
367.350310	13205.343605	29.460544
367.739040	13229.134962	29.465562
367.979178	13247.161078	29.470580
368.021207	13257.894919	29.475597
368.334820	13276.364300	29.480615
369.058802	13288.854539	29.485632
369.406608	13298.672065	29.490650
369.927598	13320.086973	29.495668
370.515505	13340.885091	29.500685
370.587462	13363.529363	29.505703
370.778511	13380.041147	29.510720
371.256462	13407.611494	29.515738
371.782936	13412.910432	29.520756
372.031113	13432.486038	29.525773
372.263260	13445.877659	29.530791
372.641733	13469.576186	29.535808
372.840436	13490.122791	29.540826
373.401823	13504.675555	29.545844
373.547660	13525.243112	29.550861
373.759349	13553.338554	29.555879
374.217829	13566.577961	29.560896
374.888785	13598.356413	29.565914
375.202859	13627.099112	29.570932
375.760175	13639.925178	29.575949
375.591873	13677.683893	29.580967
376.248545	13698.503214	29.585984
376.562922	13717.190810	29.591002
377.025429	13742.588174	29.596020
377.586139	13770.120821	29.601037
377.976535	13797.500177	29.606055
378.314154	13816.121069	29.611072
378.649822	13834.780181	29.616090
378.951193	13854.562639	29.621108
379.628259	13875.442121	29.626125
380.140472	13901.574058	29.631143
380.607411	13912.105915	29.636160
380.638159	13936.813231	29.641178
381.211315	13960.535564	29.646196
381.514148	13979.121009	29.651213
382.006344	13995.444043	29.656231
382.418683	14012.044879	29.661248
382.547599	14023.921405	29.666266
383.149605	14049.259431	29.671284
383.735721	14071.571362	29.676301
383.860474	14096.504176	29.681319
384.468800	14102.763185	29.686336
384.765935	14124.160379	29.691354
384.766044	14140.525878	29.696372
385.232890	14159.003698	29.701389
385.987580	14175.525787	29.706407
386.666713	14193.180859	29.711424
386.692745	14211.421441	29.716442
387.274637	14223.722963	29.721460
387.911254	14241.754241	29.726477
388.448259	14259.172670	29.731495
389.059762	14259.967667	29.736512
388.994715	14272.986392	29.741530
389.531341	14281.284213	29.746548
390.061941	14296.909860	29.751565
390.367429	14311.932837	29.756583
390.911872	14322.654904	29.761600
390.926758	14328.375314	29.766618
391.611773	14348.483487	29.771636
391.936544	14355.459681	29.776653
392.198556	14367.615598	29.781671
392.456411	14382.500816	29.786688
392.583298	14401.028965	29.791706
392.859295	14410.144573	29.796724
393.512959	14431.937885	29.801741
393.330256	14457.213040	29.806759
393.853408	14458.530349	29.811776
394.302305	14479.427289	29.816794
394.680206	14501.349146	29.821812
395.149771	14519.163675	29.826829
394.805412	14544.982208	29.831847
395.301289	14563.035837	29.836864
395.687448	14592.943548	29.841882
396.153158	14621.051310	29.846900
396.926601	14640.552202	29.851917
396.950056	14672.114897	29.856935
397.555554	14694.427683	29.861952
397.389473	14721.693410	29.866970
398.008999	14744.749395	29.871988
398.356055	14774.650883	29.877005
398.865315	14808.506372	29.882023
399.454797	14825.471792	29.887040
400.125915	14853.661418	29.892058
400.329736	14890.249390	29.897076
400.869431	14912.241124	29.902093
401.292025	14935.489256	29.907111
401.560893	14958.458304	29.912128
402.120848	14977.759272	29.917146
402.260408	14999.750617	29.922164
402.679100	15023.072107	29.927181
403.316635	15048.825950	29.932199
403.962910	15075.153263	29.937216
404.576739	15094.600665	29.942234
405.096780	15118.531735	29.947252
405.788571	15118.739391	29.952269
405.922531	15145.058616	29.957287
406.551116	15156.497538	29.962304
407.242289	15180.300815	29.967322
407.119984	15187.050464	29.972340
407.599070	15200.925759	29.977357
407.743195	15235.284517	29.982375
408.284385	15244.873788	29.987392
408.759216	15272.851592	29.992410
408.802460	15288.052222	29.997428
409.502893	15298.510378	30.002445
409.837030	15327.214600	30.007463
410.281112	15332.887034	30.012480
410.703764	15351.331877	30.017498
411.139811	15370.497894	30.022516
411.453205	15386.107926	30.027533
411.809352	15414.211910	30.032551
412.417400	15435.385011	30.037568
412.932101	15455.423124	30.042586
413.149922	15480.371593	30.047604
414.053392	15501.283727	30.052621
413.880736	15513.306325	30.057639
414.282219	15533.703355	30.062656
414.725036	15556.968027	30.067674
415.099189	15580.878311	30.072692
415.717575	15598.158886	30.077709
415.846974	15616.852054	30.082727
416.036984	15639.831115	30.087744
416.777207	15674.779497	30.092762
416.980934	15706.432519	30.097780
417.525430	15715.478272	30.102797
417.643402	15753.158345	30.107815
418.373185	15766.445226	30.112832
418.341239	15796.631923	30.117850
418.956414	15820.356310	30.122868
419.530495	15844.601980	30.127885
419.718055	15877.217968	30.132903
420.109678	15895.437634	30.137920
420.638664	15919.185118	30.142938
421.043852	15957.989215	30.147956
421.398485	15960.789060	30.152973
421.797886	15997.844383	30.157991
422.170057	16015.432368	30.163008
422.793355	16036.689023	30.168026
423.041450	16065.587859	30.173044
423.735165	16076.688657	30.178061
423.990058	16099.301202	30.183079
424.217897	16111.545702	30.188096
425.335078	16132.406103	30.193114
425.524695	16173.385824	30.198132
426.120522	16180.399193	30.203149
426.176920	16201.969077	30.208167
426.928951	16214.668474	30.213184
427.022176	16234.798689	30.218202
427.451008	16258.581232	30.223220
428.156426	16277.257464	30.228237
428.488322	16304.062105	30.233255
428.679148	16327.585117	30.238272
429.494910	16349.105712	30.243290
429.964727	16383.349182	30.248308
430.591243	16401.229322	30.253325
430.925847	16422.196826	30.258343
431.123022	16439.904206	30.263360
431.791819	16469.517901	30.268378
431.785396	16492.933037	30.273396
432.328819	16510.652577	30.278413
432.629710	16535.001923	30.283431
433.142462	16565.066606	30.288448
434.030379	16588.468116	30.293466
434.134854	16619.206426	30.298484
434.284736	16642.954175	30.303501
435.045671	16664.129956	30.308519
435.226188	16682.490825	30.313536
436.005763	16712.820323	30.318554
436.126194	16748.186753	30.323572
436.884457	16768.273371	30.328589
437.382590	16791.486657	30.333607
437.661329	16816.740016	30.338624
438.213596	16841.309377	30.343642
438.319879	16880.471692	30.348660
438.991419	16892.612448	30.353677
439.253653	16925.518580	30.358695
439.521282	16952.362617	30.363712
440.039603	16976.482633	30.368730
440.380045	17008.160604	30.373748
441.163134	17027.204431	30.378765
441.893875	17058.524443	30.383783
442.462599	17084.165459	30.388800
442.937960	17096.637138	30.393818
442.990980	17126.263013	30.398836
443.988717	17145.488121	30.403853
444.206931	17163.704566	30.408871
444.653056	17186.079966	30.413888
444.998890	17201.831691	30.418906
444.950891	17239.616474	30.423924
445.688122	17255.408013	30.428941
445.875016	17291.128269	30.433959
446.138682	17304.852472	30.438976
446.618283	17336.806097	30.443994
447.129115	17369.923580	30.449012
447.695117	17399.747485	30.454029
448.521326	17425.898229	30.459047
448.993835	17439.804607	30.464064
449.277726	17464.675809	30.469082
449.628739	17496.308703	30.474100
450.565974	17512.795620	30.479117
451.120213	17525.754292	30.484135
451.086920	17556.910506	30.489152
452.019660	17563.915836	30.494170
452.260461	17592.432746	30.499188
452.465545	17609.843045	30.504205
452.956321	17616.898668	30.509223
453.309353	17633.761474	30.514240
453.745116	17647.667440	30.519258
454.048525	17677.368652	30.524276
454.626074	17700.905416	30.529293
455.050727	17718.982654	30.534311
455.462044	17747.826858	30.539328
455.909016	17771.137781	30.544346
455.905069	17800.350343	30.549364
456.523723	17834.550967	30.554381
457.332266	17863.004619	30.559399
457.441963	17888.484855	30.564416
458.041410	17907.798382	30.569434
458.425733	17940.342817	30.574452
458.718255	17972.484731	30.579469
459.113549	18002.866973	30.584487
459.566414	18035.906232	30.589504
460.297779	18063.967948	30.594522
460.613254	18090.622863	30.599540
460.887176	18116.981082	30.604557
461.915508	18142.267226	30.609575
462.207060	18187.537495	30.614592
462.644096	18210.117667	30.619610
462.827351	18235.094067	30.624628
463.368654	18271.847240	30.629645
463.827392	18293.590189	30.634663
463.791828	18335.304697	30.639680
465.234118	18363.337624	30.644698
465.597083	18393.915071	30.649716
465.985523	18422.555381	30.654733
467.032709	18439.423883	30.659751
467.476959	18466.514014	30.664768
468.471079	18489.354726	30.669786
468.646015	18514.642353	30.674804
468.962714	18531.138891	30.679821
469.819432	18540.734096	30.684839
469.832052	18569.919949	30.689856
470.378295	18586.942854	30.694874
470.852396	18608.949093	30.699892
470.941256	18626.245838	30.704909
471.664432	18663.034443	30.709927
471.867918	18689.271799	30.714944
472.882746	18704.705162	30.719962
472.905915	18738.589999	30.724980
473.367867	18769.860119	30.729997
473.931251	18790.026753	30.735015
474.083145	18818.843688	30.740032
474.910341	18838.943781	30.745050
474.952453	18874.070486	30.750068
475.572037	18901.803446	30.755085
476.099157	18933.025715	30.760103
476.602744	18967.031553	30.765120
476.788531	18996.001386	30.770138
477.276178	19014.164733	30.775156
477.798944	19046.367127	30.780173
478.730447	19068.997208	30.785191
478.736016	19104.976642	30.790208
479.222929	19132.357958	30.795226
479.710309	19162.247432	30.800244
480.452792	19194.453565	30.805261
481.154768	19215.666655	30.810279
481.357370	19243.692857	30.815296
482.298680	19269.101509	30.820314
482.538781	19294.367306	30.825332
482.879664	19316.717426	30.830349
483.962882	19331.357157	30.835367
484.195024	19348.467834	30.840384
484.591596	19372.527772	30.845402
485.062805	19388.350089	30.850420
485.351929	19408.452917	30.855437
486.131154	19423.544680	30.860455
486.174431	19458.065729	30.865472
486.817420	19470.449508	30.870490
487.083822	19497.733198	30.875508
487.519136	19513.548603	30.880525
488.076323	19534.582544	30.885543
488.607385	19573.898567	30.890560
488.976678	19595.777025	30.895578
489.439960	19624.464243	30.900596
489.667519	19653.763365	30.905613
490.607147	19683.905025	30.910631
490.976819	19717.073894	30.915648
491.697477	19735.397278	30.920666
491.939078	19758.976520	30.925684
492.352204	19798.981183	30.930701
492.976918	19825.166727	30.935719
492.898117	19853.591692	30.940736
493.928669	19886.385659	30.945754
494.533844	19922.417998	30.950772
494.796898	19948.249676	30.955789
495.373697	19978.259076	30.960807
495.479562	20010.591541	30.965824
496.236123	20046.581444	30.970842
496.812931	20072.711641	30.975860
497.336361	20109.711172	30.980877
497.607512	20132.686010	30.985895
498.182316	20177.884941	30.990912
498.616398	20213.413886	30.995930
499.456451	20243.698371	31.000948
499.672994	20276.563624	31.005965
500.451905	20310.459179	31.010983
500.919510	20351.195669	31.016000
501.367843	20377.586490	31.021018
502.133346	20400.901220	31.026036
502.362782	20444.107740	31.031053
503.063344	20466.586070	31.036071
503.698442	20502.602154	31.041088
504.428901	20533.239122	31.046106
504.768529	20563.337112	31.051124
505.427209	20595.634503	31.056141
506.215304	20618.086660	31.061159
506.548307	20639.081083	31.066176
507.313433	20668.348071	31.071194
507.810042	20685.942919	31.076212
507.850495	20712.796132	31.081229
508.614642	20740.161553	31.086247
508.943932	20779.770652	31.091264
509.161186	20796.613236	31.096282
509.870219	20824.992032	31.101300
510.646606	20847.244098	31.106317
511.111024	20874.625059	31.111335
511.427538	20907.109240	31.116352
512.147247	20926.192103	31.121370
512.404715	20960.233637	31.126388
512.337566	20987.274675	31.131405
513.063964	21022.228549	31.136423
513.665528	21038.082334	31.141440
514.732384	21069.444625	31.146458
515.458484	21091.679571	31.151476
516.148569	21106.824513	31.156493
516.456520	21128.069803	31.161511
517.103502	21144.276715	31.166528
517.522490	21162.775058	31.171546
517.920089	21179.330665	31.176564
518.089335	21195.018503	31.181581
518.796050	21217.774747	31.186599
518.943011	21237.181404	31.191616
519.419229	21265.944822	31.196634
519.759689	21289.270315	31.201652
520.515594	21322.463545	31.206669
521.551811	21339.058273	31.211687
521.753209	21366.139911	31.216704
522.213528	21391.879405	31.221722
522.526108	21412.486101	31.226740
523.154900	21447.481294	31.231757
523.852094	21466.523979	31.236775
524.217176	21498.679281	31.241792
524.330029	21533.414229	31.246810
525.429809	21556.671660	31.251828
525.455785	21590.984330	31.256845
526.312299	21618.684035	31.261863
526.470193	21654.941257	31.266880
527.019741	21680.724021	31.271898
527.387589	21724.132824	31.276916
527.878206	21765.424683	31.281933
528.385185	21793.779657	31.286951
529.075264	21828.810158	31.291968
529.880229	21865.452962	31.296986
530.245781	21896.692622	31.302004
530.846600	21941.664056	31.307021
531.394113	21964.660937	31.312039
531.734047	22001.983430	31.317056
532.233152	22037.505484	31.322074
533.163258	22067.317407	31.327092
533.329620	22108.155264	31.332109
534.094542	22132.021879	31.337127
534.603046	22167.681709	31.342144
534.593926	22213.267434	31.347162
535.837165	22248.635407	31.352180
536.673994	22280.528529	31.357197
537.001603	22311.123941	31.362215
537.328125	22347.337063	31.367232
537.832894	22379.301309	31.372250
538.440439	22411.729746	31.377268
538.907502	22451.156329	31.382285
539.230043	22483.294618	31.387303
539.873080	22512.703531	31.392320
540.063494	22560.502027	31.397338
541.185428	22601.134365	31.402356
541.400606	22637.687724	31.407373
542.041821	22663.444775	31.412391
542.979612	22713.679457	31.417408
543.239187	22748.753738	31.422426
544.438387	22776.395078	31.427444
544.949765	22813.673290	31.432461
545.375851	22839.603283	31.437479
545.979200	22865.417080	31.442496
546.480253	22898.406431	31.447514
547.473484	22925.979135	31.452532
547.856126	22949.773910	31.457549
548.409237	22974.142329	31.462567
548.696462	23000.384958	31.467584
549.312674	23023.719861	31.472602
550.013231	23043.104775	31.477620
550.478201	23086.343371	31.482637
550.883120	23106.457115	31.487655
551.478722	23139.198251	31.492672
551.979422	23172.061729	31.497690
552.595122	23186.550094	31.502708
553.195455	23213.710797	31.507725
554.001233	23248.927904	31.512743
554.421823	23265.671235	31.517760
554.504904	23293.317486	31.522778
555.231937	23310.543672	31.527796
555.488524	23333.992137	31.532813
556.258024	23364.791690	31.537831
556.777384	23389.178543	31.542848
556.882564	23419.083789	31.547866
557.709283	23452.882471	31.552884
557.977123	23480.070336	31.557901
558.510809	23515.387403	31.562919
559.162506	23543.090288	31.567936
559.581191	23585.604182	31.572954
560.385644	23613.201090	31.577972
560.506258	23655.685985	31.582989
561.081561	23695.963829	31.588007
562.164609	23739.764250	31.593024
562.655701	23770.393178	31.598042
563.303081	23805.035741	31.603060
563.829998	23841.447694	31.608077
563.984583	23871.484906	31.613095
565.142906	23912.739850	31.618112
565.315063	23941.617967	31.623130
566.301089	23976.909243	31.628148
566.583173	24012.626803	31.633165
567.073349	24043.389001	31.638183
567.896277	24083.135929	31.643200
568.271707	24123.584966	31.648218
569.156819	24150.816097	31.653236
569.659809	24186.505689	31.658253
570.079616	24214.776662	31.663271
571.058004	24256.357514	31.668288
571.677850	24288.054024	31.673306
572.298043	24316.477023	31.678324
572.915246	24344.862612	31.683341
573.666840	24375.047220	31.688359
574.331612	24407.672174	31.693376
574.746146	24440.488043	31.698394
575.102647	24465.053388	31.703412
575.656938	24500.552239	31.708429
576.014122	24540.531009	31.713447
577.345182	24562.529761	31.718464
577.465442	24594.993837	31.723482
578.204819	24628.138313	31.728500
578.676446	24660.351557	31.733517
578.800225	24694.812244	31.738535
579.707142	24722.407279	31.743552
580.053042	24753.566025	31.748570
580.766765	24776.521171	31.753588
581.217106	24826.799607	31.758605
581.791626	24869.626767	31.763623
582.452768	24887.629321	31.768640
583.062576	24930.868185	31.773658
583.569563	24961.648121	31.778676
584.164444	25004.636693	31.783693
584.600885	25034.549347	31.788711
585.516309	25072.716460	31.793728
586.058457	25108.900823	31.798746
586.776481	25141.796704	31.803764
587.250564	25178.175125	31.808781
587.869232	25213.191172	31.813799
588.949042	25243.976625	31.818816
588.866590	25285.662563	31.823834
589.247104	25306.995751	31.828852
590.337313	25348.403364	31.833869
590.910645	25383.768080	31.838887
591.858490	25406.194333	31.843904
591.767887	25438.800233	31.848922
592.626670	25462.112639	31.853940
593.048737	25505.755015	31.858957
593.624172	25527.032630	31.863975
594.332540	25553.914161	31.868992
594.730520	25592.390818	31.874010
595.277376	25617.060479	31.879028
595.775896	25651.072278	31.884045
596.248189	25689.354204	31.889063
597.033590	25719.219545	31.894080
597.405858	25756.645111	31.899098
598.023722	25792.041489	31.904116
598.645145	25822.905942	31.909133
599.419802	25857.500521	31.914151
600.423075	25891.768635	31.919168
600.674397	25921.566241	31.924186
601.486505	25947.098527	31.929204
601.915456	25989.489508	31.934221
602.271127	26027.000335	31.939239
602.997587	26058.632385	31.944256
603.548620	26094.785529	31.949274
604.465610	26123.114044	31.954292
605.694604	26149.137463	31.959309
606.255907	26183.266730	31.964327
606.910740	26213.191174	31.969344
607.447624	26235.499434	31.974362
607.786451	26259.823256	31.979380
608.324868	26285.095469	31.984397
608.957897	26328.523302	31.989415
609.710716	26362.559677	31.994432
609.971665	26398.082538	31.999450
610.624004	26427.856007	32.004468
611.259843	26457.505701	32.009485
611.700115	26497.089812	32.014503
612.243872	26531.064409	32.019520
613.143651	26571.954507	32.024538
613.407634	26610.024314	32.029556
613.995282	26649.591963	32.034573
614.486960	26698.244289	32.039591
615.175013	26733.207868	32.044608
616.101913	26778.828020	32.049626
616.766411	26816.595319	32.054644
617.212416	26856.785983	32.059661
617.873405	26886.950633	32.064679
618.862738	26924.762065	32.069696
619.027983	26966.273623	32.074714
619.751344	26997.345119	32.079732
620.669343	27041.880157	32.084749
620.928759	27082.220577	32.089767
621.519486	27116.536421	32.094784
622.373118	27156.866093	32.099802
622.969524	27193.172104	32.104820
623.954265	27232.906237	32.109837
623.990556	27267.283885	32.114855
625.015135	27312.548638	32.119872
625.360910	27345.841396	32.124890
626.020506	27387.453366	32.129908
626.863453	27422.084173	32.134925
627.205008	27461.243191	32.139943
628.040771	27494.762840	32.144960
628.576738	27532.361986	32.149978
629.628208	27567.782052	32.154996
629.800998	27607.132115	32.160013
629.906672	27649.476067	32.165031
631.127094	27685.647307	32.170048
631.470619	27725.185758	32.175066
632.049851	27765.774514	32.180084
632.993273	27818.530364	32.185101
633.414439	27860.281772	32.190119
634.232789	27886.940603	32.195136
634.846620	27930.640338	32.200154
635.170949	27957.376630	32.205172
635.908696	27991.639324	32.210189
636.310722	28023.489590	32.215207
637.228544	28056.485340	32.220224
637.757111	28102.480563	32.225242
638.562976	28137.364903	32.230260
639.118543	28175.410936	32.235277
639.480585	28212.368580	32.240295
640.519517	28244.580859	32.245312
640.970851	28289.716337	32.250330
641.591795	28317.512780	32.255348
642.526717	28367.136285	32.260365
642.936109	28401.925151	32.265383
643.683998	28435.757189	32.270400
644.672761	28467.655318	32.275418
644.915748	28506.066961	32.280436
645.885416	28552.069966	32.285453
646.657804	28589.425448	32.290471
647.367412	28625.400242	32.295488
647.957929	28662.449335	32.300506
648.296728	28696.870506	32.305524
649.266075	28724.183120	32.310541
649.600064	28770.810804	32.315559
650.491334	28803.243040	32.320576
651.382920	28838.494410	32.325594
651.801898	28884.274681	32.330612
652.812554	28907.327082	32.335629
653.319215	28944.288683	32.340647
653.974793	28974.760682	32.345664
654.779659	29011.776839	32.350682
655.545903	29040.404842	32.355700
656.006587	29067.342467	32.360717
656.471578	29114.500343	32.365735
656.939205	29142.619007	32.370752
657.619862	29193.535899	32.375770
658.167953	29229.429593	32.380788
659.100776	29267.058277	32.385805
659.520083	29313.932997	32.390823
660.195388	29348.460588	32.395840
660.671567	29395.642642	32.400858
661.481763	29441.849613	32.405876
662.194400	29478.331120	32.410893
662.922544	29522.534686	32.415911
663.596010	29563.346134	32.420928
664.472355	29604.669510	32.425946
664.715668	29651.085831	32.430964
665.664106	29690.255212	32.435981
666.070481	29731.178354	32.440999
666.728556	29774.818207	32.446016
667.918801	29815.852643	32.451034
668.210469	29864.126633	32.456052
668.918591	29900.217679	32.461069
669.575709	29941.917413	32.466087
670.683281	29975.752559	32.471104
670.993897	30018.416976	32.476122
671.358933	30057.684742	32.481140
672.630834	30103.315191	32.486157
672.896875	30140.019523	32.491175
673.631108	30185.468860	32.496192
674.679389	30224.307556	32.501210
675.002218	30261.926129	32.506228
675.773013	30291.509692	32.511245
676.422758	30337.674267	32.516263
677.309026	30376.051876	32.521280
677.933264	30419.009360	32.526298
678.721494	30453.773979	32.531316
679.498492	30481.308704	32.536333
679.827627	30518.383114	32.541351
680.641126	30546.955247	32.546368
681.298172	30576.828856	32.551386
681.681309	30622.112887	32.556404
682.024750	30647.800327	32.561421
682.723999	30702.169565	32.566439
683.246024	30739.979064	32.571456
684.047183	30776.904158	32.576474
684.690371	30816.439562	32.581492
685.197319	30862.033448	32.586509
686.114229	30909.364876	32.591527
686.625411	30947.359779	32.596544
687.540818	30995.127827	32.601562
687.943943	31046.086437	32.606580
689.137000	31081.326051	32.611597
689.870088	31123.161670	32.616615
690.368672	31163.991029	32.621632
691.085687	31201.827731	32.626650
691.987612	31254.219612	32.631668
692.704325	31290.950234	32.636685
693.546553	31339.217305	32.641703
693.820220	31365.896423	32.646720
694.850171	31410.189524	32.651738
695.775500	31461.434034	32.656756
696.374531	31501.552938	32.661773
697.082542	31541.515773	32.666791
697.553554	31580.706616	32.671808
698.205171	31621.120959	32.676826
699.193986	31666.811841	32.681844
699.918624	31711.418913	32.686861
700.484372	31761.740597	32.691879
701.344995	31800.403025	32.696896
702.192287	31844.213590	32.701914
702.690987	31887.889182	32.706932
703.187068	31934.650347	32.711949
703.904523	31978.589000	32.716967
704.686835	32017.219842	32.721984
705.352857	32040.494101	32.727002
706.119955	32096.651787	32.732020
707.287910	32138.408708	32.737037
707.654999	32177.155447	32.742055
708.625984	32221.149738	32.747072
709.520030	32261.483107	32.752090
709.546389	32308.021537	32.757108
711.014131	32358.494220	32.762125
711.456433	32394.909413	32.767143
712.085173	32437.263459	32.772160
713.312931	32469.256805	32.777178
713.758342	32512.809289	32.782196
714.419181	32550.385396	32.787213
715.134082	32596.070638	32.792231
715.528373	32628.226362	32.797248
716.366879	32672.944104	32.802266
716.697341	32721.699139	32.807284
717.512309	32756.248480	32.812301
718.002777	32806.995413	32.817319
718.740844	32861.048110	32.822336
719.754555	32898.910980	32.827354
720.045233	32955.354214	32.832372
721.067224	32999.917478	32.837389
721.577820	33043.144749	32.842407
722.748509	33103.724382	32.847424
723.233801	33147.202397	32.852442
724.059519	33193.453235	32.857460
724.926105	33231.592638	32.862477
725.242178	33280.743208	32.867495
726.030650	33321.000324	32.872512
727.066364	33351.096802	32.877530
727.353349	33407.630343	32.882548
728.416316	33436.616272	32.887565
729.432362	33469.908774	32.892583
729.809130	33510.477298	32.897600
730.781630	33540.900066	32.902618
730.874240	33597.015669	32.907636
731.988310	33623.281558	32.912653
732.774305	33668.117131	32.917671
733.404660	33713.407095	32.922688
734.620382	33761.987983	32.927706
734.899846	33793.980127	32.932724
735.561727	33843.823907	32.937741
736.492373	33881.379119	32.942759
737.245938	33927.826228	32.947776
737.577127	33960.992827	32.952794
738.520962	34017.393533	32.957812
738.961051	34055.348324	32.962829
739.857602	34099.990474	32.967847
740.655429	34150.072914	32.972864
741.380436	34191.669371	32.977882
742.029308	34250.355075	32.982900
742.673204	34303.066880	32.987917
743.435143	34356.923691	32.992935
744.124155	34405.519000	32.997952
745.130356	34450.486144	33.002970
745.922080	34503.775951	33.007988
746.897286	34560.805464	33.013005
747.400542	34596.892476	33.018023
747.857953	34647.174827	33.023040
749.134681	34698.783215	33.028058
749.415872	34761.808385	33.033076
750.532981	34802.010550	33.038093
751.762843	34849.649650	33.043111
752.306625	34894.266530	33.048128
753.301799	34949.314943	33.053146
753.853229	34996.295558	33.058164
754.718253	35036.531324	33.063181
755.790475	35078.732729	33.068199
755.910988	35124.712554	33.073216
756.923367	35172.942849	33.078234
757.764032	35213.701240	33.083252
758.333761	35254.679177	33.088269
759.331352	35303.234551	33.093287
759.993756	35350.476781	33.098304
760.648014	35385.169425	33.103322
761.586754	35436.914742	33.108340
762.654814	35481.058738	33.113357
763.436463	35530.097377	33.118375
764.322318	35573.106675	33.123392
765.036745	35610.205636	33.128410
765.589176	35646.640824	33.133428
766.174614	35696.292287	33.138445
767.305394	35730.442973	33.143463
768.235842	35782.904933	33.148480
768.853940	35815.909375	33.153498
769.392599	35865.701343	33.158516
770.006483	35902.835529	33.163533
770.903962	35940.311077	33.168551
771.033549	36007.347219	33.173568
772.315643	36047.665026	33.178586
772.746614	36105.732390	33.183604
773.561229	36151.359140	33.188621
774.621720	36188.809600	33.193639
775.492184	36243.324466	33.198656
776.007001	36283.566854	33.203674
776.372999	36339.830280	33.208692
777.318069	36391.987941	33.213709
777.981678	36432.207310	33.218727
778.596222	36490.038307	33.223744
779.760411	36534.593097	33.228762
780.427725	36576.462526	33.233780
781.039531	36621.268402	33.238797
781.696055	36667.072772	33.243815
782.252345	36716.124142	33.248832
783.575211	36764.182965	33.253850
784.064564	36808.458282	33.258868
784.572535	36865.883322	33.263885
785.572450	36915.226110	33.268903
786.969874	36962.350496	33.273920
787.815173	37013.475620	33.278938
788.412503	37046.801390	33.283956
789.260647	37095.264116	33.288973
790.090151	37129.337761	33.293991
790.489722	37186.552993	33.299008
791.443737	37232.583898	33.304026
792.380438	37278.370999	33.309044
793.274806	37327.870384	33.314061
793.890178	37366.916577	33.319079
794.916831	37422.307930	33.324096
795.727428	37465.389746	33.329114
796.487692	37521.291010	33.334132
797.151922	37568.152133	33.339149
798.349544	37616.257782	33.344167
799.086683	37665.460067	33.349184
800.023495	37713.682659	33.354202
800.479021	37752.912675	33.359220
801.379336	37794.899769	33.364237
802.644465	37840.257224	33.369255
803.230710	37893.688875	33.374272
804.281983	37927.071405	33.379290
805.422879	37968.989548	33.384308
806.031272	38006.134574	33.389325
807.292987	38045.030200	33.394343
808.126812	38086.547677	33.399360
808.680917	38123.758321	33.404378
809.271076	38165.522788	33.409396
809.825790	38209.272216	33.414413
810.784164	38243.327455	33.419431
811.107680	38292.956400	33.424448
812.407194	38339.871498	33.429466
813.291858	38386.997107	33.434484
813.643882	38439.916621	33.439501
814.505769	38472.311524	33.444519
815.488962	38528.699052	33.449536
816.481634	38581.645071	33.454554
817.077272	38614.221004	33.459572
817.758443	38664.812940	33.464589
819.094399	38706.980230	33.469607
819.889603	38755.638386	33.474624
820.448558	38798.287988	33.479642
821.500329	38850.238883	33.484660
822.162047	38902.295249	33.489677
823.097243	38945.354197	33.494695
823.669538	38991.062884	33.499712
824.404878	39034.146981	33.504730
825.505441	39084.174633	33.509748
826.207324	39136.901941	33.514765
827.153684	39178.346984	33.519783
827.646634	39239.771170	33.524800
828.315466	39278.932617	33.529818
829.228741	39324.544346	33.534836
829.692841	39377.777456	33.539853
830.534046	39422.818863	33.544871
831.344914	39495.374987	33.549888
832.180338	39539.500545	33.554906
833.232259	39587.399424	33.559924
833.613564	39641.272234	33.564941
834.486341	39676.614296	33.569959
835.194495	39742.711387	33.574976
836.347100	39788.273968	33.579994
836.945952	39845.989955	33.585012
837.630636	39896.154172	33.590029
838.580735	39934.109101	33.595047
839.228495	39994.385466	33.600064
839.580405	40056.245122	33.605082
840.782245	40115.815281	33.610100
841.425515	40173.885667	33.615117
842.764614	40222.582113	33.620135
843.503997	40292.185983	33.625152
844.406062	40345.713371	33.630170
845.423034	40397.736669	33.635188
846.153857	40468.114015	33.640205
847.332527	40522.844431	33.645223
848.031525	40577.194736	33.650240
848.966456	40631.369095	33.655258
849.877514	40688.070786	33.660276
850.842673	40749.007876	33.665293
851.892170	40783.862381	33.670311
852.603997	40848.773249	33.675328
853.291334	40899.774196	33.680346
854.508405	40951.021189	33.685364
855.373046	41012.297305	33.690381
855.901285	41048.954134	33.695399
856.861247	41106.559992	33.700416
857.789085	41159.497154	33.705434
858.909009	41218.994613	33.710452
859.878536	41279.040727	33.715469
861.208575	41320.259012	33.720487
861.546624	41369.861081	33.725504
862.849341	41420.943974	33.730522
863.355813	41468.432753	33.735540
864.216959	41527.301154	33.740557
864.978691	41567.451474	33.745575
865.857540	41627.544366	33.750592
866.648440	41688.207772	33.755610
867.712105	41732.808013	33.760628
868.311474	41792.268369	33.765645
869.512794	41839.016669	33.770663
870.315698	41895.086970	33.775680
871.192450	41948.223783	33.780698
872.387464	41991.678165	33.785716
873.050330	42057.296010	33.790733
874.290731	42104.348675	33.795751
875.354814	42153.794554	33.800768
875.914709	42200.055847	33.805786
876.701911	42246.224721	33.810804
877.574046	42291.849099	33.815821
878.523129	42348.593409	33.820839
879.464525	42403.055761	33.825856
880.201743	42446.683926	33.830874
881.299853	42486.732656	33.835892
882.112284	42526.434042	33.840909
883.281999	42574.087006	33.845927
883.904240	42626.677085	33.850944
884.488890	42673.024045	33.855962
885.769420	42726.131138	33.860980
886.489822	42777.156569	33.865997
887.596739	42819.481548	33.871015
888.203859	42873.042317	33.876032
888.946217	42923.691470	33.881050
890.039750	42967.391375	33.886068
890.761179	43019.840357	33.891085
891.695729	43062.262368	33.896103
892.382321	43105.121771	33.901120
893.324732	43147.776746	33.906138
894.530111	43178.094486	33.911156
895.091851	43225.945260	33.916173
896.064037	43269.399107	33.921191
896.670989	43313.441546	33.926208
897.321894	43357.907306	33.931226
898.806021	43397.802371	33.936244
899.419471	43453.855699	33.941261
900.546512	43503.041739	33.946279
901.150320	43559.862202	33.951296
901.705873	43604.185254	33.956314
902.652641	43653.728771	33.961332
903.639478	43698.977556	33.966349
904.536571	43753.956202	33.971367
905.302220	43818.038775	33.976384
905.910680	43876.358429	33.981402
906.667241	43926.311860	33.986420
907.922199	43995.947924	33.991437
908.878915	44053.233075	33.996455
909.608095	44107.125612	34.001472
910.570861	44178.180620	34.006490
911.913256	44232.426551	34.011508
912.724159	44299.134822	34.016525
913.837373	44347.255890	34.021543
914.576704	44409.756587	34.026560
915.692212	44481.319989	34.031578
916.683417	44529.599718	34.036596
917.323717	44589.377458	34.041613
918.279596	44649.289387	34.046631
919.584086	44705.332550	34.051648
920.240689	44771.307320	34.056666
921.275099	44818.543508	34.061684
921.886008	44881.546382	34.066701
923.136158	44949.358067	34.071719
924.250824	44999.865098	34.076736
925.237124	45067.952507	34.081754
926.283379	45128.180507	34.086772
927.066941	45174.280140	34.091789
928.320101	45223.209859	34.096807
928.942695	45274.091869	34.101824
929.709904	45339.557587	34.106842
930.886143	45391.966251	34.111860
931.893775	45460.551253	34.116877
932.848075	45516.436206	34.121895
933.614259	45566.315892	34.126912
934.499040	45631.542648	34.131930
935.651221	45679.116463	34.136948
936.444244	45746.015301	34.141965
937.356913	45784.365725	34.146983
938.419577	45847.243647	34.152000
938.984425	45912.407447	34.157018
940.303648	45962.530369	34.162036
940.945614	46023.444022	34.167053
942.298271	46086.884503	34.172071
943.431517	46143.546401	34.177088
943.979156	46203.077261	34.182106
945.172802	46249.715867	34.187124
946.206399	46308.323227	34.192141
946.924989	46369.023383	34.197159
948.032397	46412.335663	34.202176
948.712115	46480.544948	34.207194
949.798427	46531.161088	34.212212
950.334974	46592.225633	34.217229
951.640070	46641.877823	34.222247
952.651054	46702.678598	34.227264
953.315064	46766.133926	34.232282
954.083750	46815.048083	34.237300
955.092688	46866.607042	34.242317
956.525312	46917.277371	34.247335
957.279939	46956.837546	34.252352
957.952590	47015.541216	34.257370
959.007847	47058.546592	34.262388
959.932978	47115.711664	34.267405
960.874910	47167.730970	34.272423
961.652529	47221.250153	34.277440
962.693391	47283.604086	34.282458
963.526545	47326.062724	34.287476
964.353020	47384.041041	34.292493
965.337842	47434.801626	34.297511
966.710008	47481.541358	34.302528
967.454340	47560.302523	34.307546
968.666374	47606.656370	34.312564
969.791661	47662.728646	34.317581
970.408642	47726.826674	34.322599
972.104701	47781.013162	34.327616
972.769128	47844.629608	34.332634
973.599142	47893.454249	34.337652
974.573200	47946.438267	34.342669
975.333368	48000.917326	34.347687
976.294766	48064.582788	34.352704
977.068388	48130.530086	34.357722
978.182890	48178.526301	34.362740
979.210117	48248.065689	34.367757
980.040466	48323.861508	34.372775
981.323649	48381.524125	34.377792
982.307304	48446.857403	34.382810
983.815565	48496.222461	34.387828
984.786176	48561.804851	34.392845
985.352259	48626.065219	34.397863
986.538406	48682.598659	34.402880
987.032096	48749.407723	34.407898
988.530817	48808.872429	34.412916
989.544243	48876.808900	34.417933
990.060698	48939.053350	34.422951
991.420282	48999.229958	34.427968
992.625742	49063.764729	34.432986
993.792803	49121.055135	34.438004
994.621130	49176.880275	34.443021
995.564001	49237.268272	34.448039
996.707118	49296.353371	34.453056
997.706915	49364.476904	34.458074
999.432593	49411.620795	34.463092
1000.147262	49475.815996	34.468109
1001.049155	49529.839955	34.473127
1002.444427	49581.730528	34.478144
1003.436611	49632.804880	34.483162
1004.357181	49680.543578	34.488180
1005.814400	49734.898655	34.493197
1006.407185	49786.402850	34.498215
1007.186848	49834.473955	34.503232
1008.280969	49898.136398	34.508250
1009.599907	49938.543478	34.513268
1010.571650	49995.221291	34.518285
1011.158817	50050.662402	34.523303
1011.783770	50098.650722	34.528320
1012.979184	50157.660254	34.533338
1013.785924	50211.985437	34.538356
1014.721671	50269.991935	34.543373
1015.725641	50338.143011	34.548391
1016.976204	50403.737457	34.553408
1018.110686	50466.977561	34.558426
1019.048482	50518.340795	34.563444
1020.114818	50579.934145	34.568461
1021.005606	50636.088395	34.573479
1022.267258	50687.761954	34.578496
1022.900608	50736.705705	34.583514
1023.647432	50796.691911	34.588532
1024.624029	50836.901078	34.593549
1025.125916	50904.759127	34.598567
1026.412897	50955.410619	34.603584
1027.389414	51021.676136	34.608602
1028.559914	51072.497980	34.613620
1029.424841	51141.217350	34.618637
1030.400564	51197.891169	34.623655
1031.536525	51257.463308	34.628672
1032.506112	51318.238554	34.633690
1033.483707	51380.252888	34.638708
1034.296647	51443.906673	34.643725
1035.463621	51507.467238	34.648743
1036.611683	51573.941594	34.653760
1037.719393	51656.456424	34.658778
1038.613746	51711.245977	34.663796
1039.575226	51784.855988	34.668813
1040.504397	51847.638460	34.673831
1041.931462	51913.677795	34.678848
1043.007030	51990.687502	34.683866
1044.220103	52063.480705	34.688884
1045.140778	52119.152969	34.693901
1046.198149	52194.647560	34.698919
1047.656317	52256.342211	34.703936
1048.947236	52319.676779	34.708954
1049.772784	52385.836942	34.713972
1050.924908	52446.510627	34.718989
1051.952022	52509.709836	34.724007
1053.411518	52578.751671	34.729024
1053.983595	52643.933477	34.734042
1054.880774	52701.844525	34.739060
1056.367525	52767.731399	34.744077
1056.992525	52841.789753	34.749095
1058.517405	52891.389440	34.754112
1059.417727	52969.790308	34.759130
1060.819290	53027.597882	34.764148
1061.947449	53095.364260	34.769165
1062.752865	53154.898089	34.774183
1064.500306	53216.132345	34.779200
1065.352175	53278.943427	34.784218
1066.582355	53336.772270	34.789236
1067.764834	53376.175256	34.794253
1068.728644	53439.374233	34.799271
1069.785809	53498.717649	34.804288
1070.640388	53551.410514	34.809306
1071.843988	53617.185911	34.814324
1073.073523	53669.484949	34.819341
1074.353363	53732.021412	34.824359
1075.552510	53779.579384	34.829376
1076.668637	53823.707952	34.834394
1077.635161	53872.511202	34.839412
1078.794183	53923.594190	34.844429
1079.539331	53986.930125	34.849447
1080.790394	54040.258111	34.854464
1081.769905	54092.451688	34.859482
1082.583258	54147.917765	34.864500
1083.887841	54205.509286	34.869517
1084.722747	54268.344652	34.874535
1085.840710	54326.155532	34.879552
1087.081574	54384.004268	34.884570
1088.144343	54441.824074	34.889588
1088.806960	54501.231790	34.894605
1089.719012	54566.802355	34.899623
1090.998997	54618.912086	34.904640
1092.291695	54682.271744	34.909658
1093.131597	54748.126228	34.914676
1094.184704	54812.827390	34.919693
1095.014658	54867.969812	34.924711
1096.218181	54921.256607	34.929728
1097.257526	54972.974462	34.934746
1097.746582	55026.335381	34.939764
1099.192091	55083.913311	34.944781
1099.784938	55151.389708	34.949799
1101.134570	55207.097064	34.954816
1102.239695	55270.930660	34.959834
1103.297434	55336.815960	34.964852
1104.494757	55405.622361	34.969869
1105.989659	55471.047222	34.974887
1106.917201	55534.263816	34.979904
1107.923028	55588.861437	34.984922
1109.036062	55666.282347	34.989940
1110.200297	55730.164881	34.994957
1111.261354	55783.463262	34.999975
1112.374795	55851.480350	35.004992
1113.679727	55919.980276	35.010010
1114.574797	55999.904579	35.015028
1116.024241	56055.035045	35.020045
1117.148490	56126.506705	35.025063
1118.198937	56187.294544	35.030080
1119.648866	56253.152626	35.035098
1120.601317	56324.050541	35.040116
1121.642536	56387.802208	35.045133
1122.985968	56466.556669	35.050151
1124.206008	56526.401142	35.055168
1125.375435	56584.393005	35.060186
1126.415404	56667.087882	35.065204
1127.600236	56723.628359	35.070221
1128.545059	56787.427828	35.075239
1129.888918	56846.443618	35.080256
1131.176683	56918.018624	35.085274
1132.512805	56995.130445	35.090292
1133.447610	57054.425973	35.095309
1134.458306	57122.418463	35.100327
1135.332613	57191.432482	35.105344
1136.769378	57258.415631	35.110362
1137.886835	57337.239979	35.115380
1139.052650	57393.557169	35.120397
1140.314706	57470.080850	35.125415
1141.313161	57535.880234	35.130432
1142.612929	57596.107303	35.135450
1143.842510	57669.035433	35.140468
1144.923554	57738.366759	35.145485
1145.874556	57812.408564	35.150503
1147.303294	57865.831241	35.155520
1148.657042	57926.462084	35.160538
1149.842483	57998.442412	35.165556
1150.878547	58054.692855	35.170573
1152.034105	58123.912358	35.175591
1153.563915	58190.124025	35.180608
1154.461055	58248.156208	35.185626
1155.886787	58310.302107	35.190644
1157.331553	58362.444857	35.195661
1158.070635	58434.629282	35.200679
1159.495951	58495.933922	35.205696
1160.735811	58557.141165	35.210714
1161.500844	58615.846838	35.215732
1162.851317	58689.689547	35.220749
1163.804556	58738.289640	35.225767
1164.579267	58809.159412	35.230784
1166.364302	58857.389005	35.235802
1166.773358	58938.215661	35.240820
1168.177525	58995.777833	35.245837
1169.640734	59065.141751	35.250855
1170.792083	59125.307260	35.255872
1171.967607	59181.146061	35.260890
1172.767045	59238.866778	35.265908
1173.806121	59281.998452	35.270925
1174.556180	59352.202736	35.275943
1175.826663	59404.558576	35.280960
1177.004465	59467.980533	35.285978
1177.808964	59535.037335	35.290996
1179.132705	59598.278544	35.296013
1180.517236	59668.966740	35.301031
1181.604991	59735.201201	35.306048
1182.753216	59786.652871	35.311066
1183.767268	59855.772878	35.316084
1184.785514	59924.284771	35.321101
1186.341589	59997.580232	35.326119
1187.467925	60051.441191	35.331136
1188.889628	60125.137858	35.336154
1189.730577	60193.608635	35.341172
1190.856931	60271.637253	35.346189
1191.826488	60346.120638	35.351207
1193.312932	60411.648877	35.356224
1195.003712	60486.652768	35.361242
1195.993829	60566.229153	35.366260
1197.539051	60632.495709	35.371277
1198.507085	60695.852418	35.376295
1199.642844	60770.273095	35.381312
1201.168960	60834.245418	35.386330
1202.421029	60915.136538	35.391348
1203.951685	60975.684000	35.396365
1205.028445	61041.727491	35.401383
1206.142937	61109.993424	35.406400
1207.271101	61167.325412	35.411418
1208.670642	61240.750384	35.416436
1210.137223	61304.828206	35.421453
1211.299854	61377.853900	35.426471
1212.493171	61443.031989	35.431488
1214.307304	61502.529884	35.436506
1215.165115	61570.723337	35.441524
1216.620546	61631.303183	35.446541
1217.633734	61697.320405	35.451559
1218.776273	61770.483341	35.456576
1220.226755	61826.772567	35.461594
1221.570736	61888.503602	35.466612
1222.730070	61947.541691	35.471629
1224.205233	62012.354321	35.476647
1225.457643	62069.118226	35.481664
1226.896866	62122.991725	35.486682
1227.803461	62191.261548	35.491700
1229.509244	62238.567022	35.496717
1230.417720	62288.858714	35.501735
1231.729303	62351.216351	35.506752
1233.316001	62406.725935	35.511770
1234.524939	62457.755899	35.516788
1235.846256	62513.649108	35.521805
1236.856537	62564.096343	35.526823
1237.976001	62615.438169	35.531840
1239.419746	62662.601896	35.536858
1240.453639	62729.739120	35.541876
1241.551972	62790.580288	35.546893
1242.784181	62847.393456	35.551911
1243.603524	62906.879549	35.556928
1244.728755	62975.680720	35.561946
1245.747487	63042.118475	35.566964
1247.120788	63109.431492	35.571981
1248.520999	63180.779376	35.576999
1249.475174	63258.971010	35.582016
1251.062186	63308.088679	35.587034
1251.780623	63384.722301	35.592052
1253.471086	63443.649157	35.597069
1254.860708	63512.093891	35.602087
1255.589539	63570.557512	35.607104
1256.547184	63619.432464	35.612122
1257.384489	63686.704335	35.617140
1258.613228	63752.376748	35.622157
1259.997959	63821.177615	35.627175
1261.201179	63882.239268	35.632192
1262.574329	63943.160516	35.637210
1263.583956	64021.516787	35.642228
1264.851521	64096.376312	35.647245
1266.190463	64163.172096	35.652263
1267.163483	64244.421645	35.657280
1268.682836	64310.429880	35.662298
1270.203225	64392.518525	35.667316
1271.004240	64465.578251	35.672333
1272.530845	64546.925715	35.677351
1274.033817	64625.922038	35.682368
1275.217875	64687.488797	35.687386
1276.405338	64782.406677	35.692404
1277.224633	64854.787259	35.697421
1278.886706	64926.459997	35.702439
1280.234924	65018.061480	35.707456
1281.738163	65086.277476	35.712474
1282.874080	65165.218993	35.717492
1284.415999	65236.841783	35.722509
1286.007313	65314.167695	35.727527
1286.854735	65395.130396	35.732544
1288.539517	65484.572625	35.737562
1289.774619	65558.194349	35.742580
1291.068490	65639.486808	35.747597
1292.367383	65705.140683	35.752615
1293.771336	65783.453373	35.757632
1295.145657	65863.632327	35.762650
1296.700914	65946.758902	35.767668
1297.756645	66014.851191	35.772685
1299.061484	66101.942865	35.777703
1300.216080	66178.263464	35.782720
1301.768184	66253.097517	35.787738
1303.587155	66323.090853	35.792756
1304.508628	66405.482405	35.797773
1305.990470	66483.614119	35.802791
1307.162898	66551.550290	35.807808
1308.492559	66625.388243	35.812826
1310.198563	66702.542157	35.817844
1311.203342	66782.446295	35.822861
1312.767511	66852.316358	35.827879
1313.755098	66933.388653	35.832896
1315.406484	66995.090483	35.837914
1316.344733	67072.536652	35.842932
1317.657886	67157.060033	35.847949
1319.388276	67221.434625	35.852967
1320.899895	67302.407066	35.857984
1321.930376	67375.489913	35.863002
1323.482035	67455.867733	35.868020
1324.591760	67531.971473	35.873037
1326.076804	67592.770036	35.878055
1327.388897	67673.065738	35.883072
1328.562163	67746.488199	35.888090
1329.688937	67821.798669	35.893108
1330.939344	67890.365700	35.898125
1332.509894	67955.552299	35.903143
1333.824435	68044.421976	35.908160
1335.284593	68116.268297	35.913178
1336.750328	68195.978056	35.918196
1337.947163	68270.734340	35.923213
1339.338453	68330.105672	35.928231
1340.712274	68411.913666	35.933248
1342.035285	68477.906497	35.938266
1343.326424	68548.501444	35.943284
1344.296151	68610.757109	35.948301
1345.830026	68666.162115	35.953319
1346.959036	68727.266045	35.958336
1348.325925	68788.928088	35.963354
1349.669456	68858.027672	35.968372
1350.411005	68924.574900	35.973389
1351.591797	68996.169805	35.978407
1352.957892	69072.003688	35.983424
1354.240936	69148.566315	35.988442
1355.689162	69234.208823	35.993460
1356.700859	69302.468718	35.998477
1357.908767	69387.706105	36.003495
1359.691278	69472.036984	36.008512
1360.928579	69555.528989	36.013530
1362.431224	69642.120481	36.018548
1363.831609	69720.781375	36.023565
1365.634799	69790.204093	36.028583
1366.856634	69889.587093	36.033600
1368.254408	69971.370943	36.038618
1369.643751	70057.082376	36.043636
1370.851091	70137.566781	36.048653
1372.520599	70204.124010	36.053671
1373.850235	70294.860756	36.058688
1375.142770	70370.849262	36.063706
1376.636068	70460.801085	36.068724
1377.828801	70548.989205	36.073741
1379.207489	70635.413434	36.078759
1380.546608	70726.707449	36.083776
1382.276502	70811.291541	36.088794
1383.577490	70901.148335	36.093812
1385.055876	70993.409346	36.098829
1386.249731	71076.001143	36.103847
1387.615938	71163.315623	36.108864
1388.910857	71249.830984	36.113882
1390.361168	71342.604224	36.118900
1391.978566	71431.640734	36.123917
1393.427769	71511.990190	36.128935
1395.263278	71600.233218	36.133952
1396.720145	71688.624468	36.138970
1398.596528	71762.562499	36.143988
1399.977520	71847.255210	36.149005
1401.349546	71919.233500	36.154023
1403.023973	72006.261893	36.159040
1404.371334	72078.801762	36.164058
1405.678610	72149.891567	36.169076
1406.894942	72228.379831	36.174093
1408.809203	72306.227127	36.179111
1410.038744	72385.549722	36.184128
1411.558714	72455.074512	36.189146
1413.204523	72525.643710	36.194164
1414.330787	72602.070004	36.199181
1415.998972	72667.240465	36.204199
1417.194150	72747.557457	36.209216
1418.433025	72816.088599	36.214234
1420.173238	72894.509506	36.219252
1421.337044	72958.999681	36.224269
1423.257200	73034.403677	36.229287
1424.385132	73101.990312	36.234304
1425.584317	73186.487785	36.239322
1427.289978	73255.947618	36.244340
1428.621457	73328.176748	36.249357
1430.060392	73403.669785	36.254375
1431.434954	73477.032528	36.259392
1432.679291	73561.600124	36.264410
1433.903069	73634.594251	36.269428
1435.141452	73705.179698	36.274445
1436.571802	73782.815756	36.279463
1437.782805	73861.968338	36.284480
1439.439370	73930.462309	36.289498
1440.566245	73991.705508	36.294516
1442.044711	74064.774946	36.299533
1443.395673	74133.659267	36.304551
1444.856731	74203.134527	36.309568
1446.217712	74275.348941	36.314586
1447.339474	74346.461000	36.319604
1449.052367	74434.656665	36.324621
1450.345063	74502.221061	36.329639
1451.562268	74585.985480	36.334656
1452.617467	74667.584173	36.339674
1454.539358	74750.048132	36.344692
1455.572537	74836.400826	36.349709
1457.193748	74922.750425	36.354727
1459.229516	75007.401384	36.359744
1460.267716	75102.772981	36.364762
1462.015739	75188.330901	36.369780
1463.251033	75282.722261	36.374797
1464.773063	75366.644074	36.379815
1466.361982	75459.828001	36.384832
1467.725268	75540.684428	36.389850
1469.382444	75613.198092	36.394868
1470.991593	75725.190540	36.399885
1472.646574	75806.901482	36.404903
1474.244493	75902.948333	36.409920
1475.661037	75989.308051	36.414938
1477.401142	76067.636940	36.419956
1478.697432	76151.710533	36.424973
1480.338900	76236.807093	36.429991
1481.973076	76323.982535	36.435008
1483.370777	76400.174500	36.440026
1485.302114	76489.824806	36.445044
1486.855902	76578.837782	36.450061
1488.299482	76654.947276	36.455079
1490.074972	76733.158543	36.460096
1491.050301	76818.475201	36.465114
1492.911786	76898.459635	36.470132
1493.843642	76992.537081	36.475149
1495.582693	77070.691682	36.480167
1497.401322	77155.662049	36.485184
1498.335363	77244.546183	36.490202
1500.573633	77324.320879	36.495220
1501.652917	77414.880342	36.500237
1503.286929	77499.272611	36.505255
1505.005439	77586.692259	36.510272
1506.142258	77668.540574	36.515290
1507.915529	77748.477969	36.520308
1509.163046	77835.414731	36.525325
1510.405356	77924.138807	36.530343
1511.972985	78007.466231	36.535360
1513.425358	78107.407467	36.540378
1515.198468	78190.817303	36.545396
1516.623926	78290.611397	36.550413
1518.303786	78376.038001	36.555431
1519.894500	78453.079609	36.560448
1521.497680	78549.299646	36.565466
1522.783499	78631.545571	36.570484
1524.131765	78725.487772	36.575501
1525.767805	78812.670860	36.580519
1527.472321	78909.877119	36.585536
1528.924526	78987.904723	36.590554
1530.677953	79075.944413	36.595572
1532.071798	79159.226512	36.600589
1533.230966	79241.633434	36.605607
1535.058057	79347.094812	36.610624
1536.350501	79435.283810	36.615642
1537.649127	79520.634269	36.620660
1539.546692	79608.843129	36.625677
1540.899257	79686.634918	36.630695
1542.987455	79762.766158	36.635712
1543.639391	79844.443439	36.640730
1544.974431	79921.896563	36.645748
1546.655880	79993.809921	36.650765
1547.634169	80085.432830	36.655783
1549.480472	80171.751116	36.660800
1550.675253	80259.210527	36.665818
1552.793557	80350.111097	36.670836
1554.004213	80442.167576	36.675853
1555.387309	80536.465200	36.680871
1557.047919	80635.964875	36.685888
1558.492403	80726.832771	36.690906
1559.829631	80826.472425	36.695924
1561.473460	80917.246390	36.700941
1563.092029	81022.252635	36.705959
1565.218072	81116.524620	36.710976
1566.407941	81221.776084	36.715994
1568.263529	81314.938119	36.721012
1570.006169	81414.427721	36.726029
1571.634250	81516.976378	36.731047
1573.249640	81618.564481	36.736064
1574.864578	81716.326688	36.741082
1576.318463	81806.803839	36.746100
1577.983327	81910.678525	36.751117
1579.497121	82004.593192	36.756135
1581.063183	82109.421662	36.761152
1582.446538	82210.490726	36.766170
1584.371459	82306.217240	36.771188
1585.745129	82422.378839	36.776205
1587.410045	82519.388456	36.781223
1589.313694	82622.303451	36.786240
1590.884948	82725.980387	36.791258
1592.585804	82825.988321	36.796276
1594.508819	82936.529051	36.801293
1595.999770	83038.331788	36.806311
1597.455836	83129.509706	36.811328
1599.183383	83225.536299	36.816346
1600.722661	83327.167787	36.821364
1602.717035	83430.907779	36.826381
1604.227955	83540.020202	36.831399
1605.861782	83634.225576	36.836416
1607.437093	83733.939578	36.841434
1609.186340	83831.269915	36.846452
1610.759467	83922.862861	36.851469
1612.563016	84019.741858	36.856487
1614.204502	84124.274516	36.861504
1615.687142	84227.425926	36.866522
1617.438702	84316.812777	36.871540
1619.604293	84409.226876	36.876557
1620.783540	84501.782971	36.881575
1622.607326	84593.389515	36.886592
1623.980559	84700.576535	36.891610
1625.427414	84796.310206	36.896628
1627.446332	84888.634760	36.901645
1629.127927	84982.811747	36.906663
1630.749428	85068.774666	36.911680
1632.455316	85168.904048	36.916698
1633.807982	85250.766001	36.921716
1635.282859	85353.732589	36.926733
1636.738124	85448.377351	36.931751
1638.597146	85547.204242	36.936768
1640.014268	85640.778511	36.941786
1642.056597	85724.624703	36.946804
1643.563547	85822.810690	36.951821
1645.060172	85930.426473	36.956839
1646.874497	86013.713609	36.961856
1648.291492	86114.575756	36.966874
1650.374030	86201.635703	36.971892
1651.944104	86273.595068	36.976909
1653.396789	86353.315589	36.981927
1655.009379	86421.593781	36.986944
1656.518312	86502.167606	36.991962
1658.029487	86585.199695	36.996980
1659.628661	86670.005023	37.001997
1660.839840	86759.281245	37.007015
1663.058836	86842.684835	37.012032
1664.541452	86934.060718	37.017050
1665.879590	87025.079329	37.022068
1667.597176	87112.351184	37.027085
1669.007292	87212.559242	37.032103
1671.009658	87303.386058	37.037120
1672.634763	87401.406801	37.042138
1674.492704	87493.105865	37.047156
1676.528001	87579.594384	37.052173
1678.313492	87667.478220	37.057191
1679.800497	87764.140476	37.062208
1681.858003	87867.734427	37.067226
1683.715237	87952.363683	37.072244
1685.640823	88031.812005	37.077261
1686.913854	88124.428306	37.082279
1688.931998	88205.243944	37.087296
1690.257804	88306.976992	37.092314
1691.926840	88401.357080	37.097332
1693.592855	88505.267999	37.102349
1695.025698	88607.099385	37.107367
1696.692362	88704.573022	37.112384
1698.476603	88802.231349	37.117402
1700.071766	88913.429135	37.122420
1701.878554	89016.229927	37.127437
1703.261687	89125.028439	37.132455
1705.503534	89235.454545	37.137472
1706.905620	89331.919768	37.142490
1708.566746	89436.772539	37.147508
1710.037844	89546.661407	37.152525
1711.604871	89662.403470	37.157543
1713.828617	89765.090902	37.162560
1715.435019	89882.171044	37.167578
1717.146703	89989.869391	37.172596
1718.991940	90100.867715	37.177613
1720.763355	90216.782715	37.182631
1722.266426	90322.601181	37.187648
1724.329808	90431.310669	37.192666
1725.956262	90540.900052	37.197684
1728.067858	90649.729523	37.202701
1729.869241	90758.645958	37.207719
1731.991949	90861.771203	37.212736
1733.785204	90964.086529	37.217754
1735.258657	91060.115233	37.222772
1737.357587	91157.693989	37.227789
1738.545830	91268.685377	37.232807
1740.653348	91380.737356	37.237824
1742.152043	91467.916842	37.242842
1743.698692	91582.516137	37.247860
1745.577551	91695.542961	37.252877
1747.193332	91789.612543	37.257895
1748.852275	91902.953391	37.262912
1750.580926	92005.840025	37.267930
1752.189394	92111.153965	37.272948
1754.105618	92213.644390	37.277965
1755.515703	92334.161542	37.282983
1757.435239	92447.831202	37.288000
1759.143563	92564.690330	37.293018
1760.615706	92677.987249	37.298036
1762.288134	92791.405343	37.303053
1763.984745	92907.976097	37.308071
1765.745026	93002.812651	37.313088
1767.385031	93098.948485	37.318106
1768.998616	93208.574870	37.323124
1770.686424	93303.056124	37.328141
1772.030926	93409.581946	37.333159
1773.996108	93514.920952	37.338176
1776.015766	93627.311822	37.343194
1777.512232	93736.780970	37.348212
1779.232881	93854.428945	37.353229
1780.869236	93961.544766	37.358247
1782.445167	94073.563071	37.363264
1784.637715	94200.378797	37.368282
1785.948464	94313.149289	37.373300
1788.284381	94430.690501	37.378317
1790.031841	94549.857981	37.383335
1791.506558	94670.576988	37.388352
1793.520262	94793.493721	37.393370
1795.560092	94909.638071	37.398388
1797.782066	95034.576617	37.403405
1799.559116	95148.392632	37.408423
1801.888821	95268.283000	37.413440
1803.614783	95378.748775	37.418458
1805.741492	95500.940776	37.423476
1807.694171	95594.284782	37.428493
1809.512403	95716.361114	37.433511
1810.736081	95827.452144	37.438528
1812.911655	95948.142481	37.443546
1815.036525	96067.282059	37.448564
1816.749837	96175.572343	37.453581
1818.325606	96297.131131	37.458599
1820.291106	96413.546234	37.463616
1821.896194	96528.458985	37.468634
1823.557361	96658.486235	37.473652
1825.621802	96781.846521	37.478669
1827.305041	96904.582417	37.483687
1829.135426	97023.480144	37.488704
1831.001315	97141.523437	37.493722
1832.332893	97270.375160	37.498740
1834.379446	97391.598287	37.503757
1836.300889	97520.257308	37.508775
1837.989875	97642.931785	37.513792
1839.930686	97780.538595	37.518810
1841.835175	97907.718657	37.523828
1844.051718	98028.080944	37.528845
1845.822358	98166.780913	37.533863
1847.640820	98286.052869	37.538880
1849.962685	98400.213718	37.543898
1851.430175	98533.232705	37.548916
1853.451917	98651.219184	37.553933
1855.491028	98787.319057	37.558951
1857.350733	98905.661438	37.563968
1859.373171	99021.506724	37.568986
1860.540328	99151.012960	37.574004
1862.599987	99273.863889	37.579021
1864.248198	99412.727862	37.584039
1865.833990	99543.120972	37.589056
1867.621046	99675.346710	37.594074
1869.410967	99814.862147	37.599092
1871.304366	99945.728529	37.604109
1873.513267	100092.405850	37.609127
1874.952376	100230.583430	37.614144
1877.050093	100354.674936	37.619162
1878.516288	100499.340450	37.624180
1880.968067	100640.112401	37.629197
1882.718364	100778.585921	37.634215
1884.682142	100909.216972	37.639232
1886.605879	101038.574328	37.644250
1888.078943	101171.375096	37.649268
1889.889953	101290.722712	37.654285
1891.802439	101418.435174	37.659303
1893.602663	101540.371742	37.664320
1895.676858	101653.872863	37.669338
1897.249190	101769.253233	37.674356
1899.086471	101905.499205	37.679373
1900.795363	102022.317109	37.684391
1902.665935	102161.322830	37.689408
1904.295421	102291.529922	37.694426
1905.862385	102437.696976	37.699444
1908.066334	102572.519043	37.704461
1909.658259	102713.852850	37.709479
1911.403746	102864.177825	37.714496
1913.603479	102998.026022	37.719514
1915.072781	103158.665384	37.724532
1917.182563	103309.683427	37.729549
1918.923570	103469.964803	37.734567
1920.757691	103626.783679	37.739584
1923.173014	103778.263198	37.744602
1924.838643	103937.848587	37.749620
1926.987878	104101.099436	37.754637
1928.613517	104266.246149	37.759655
1930.495563	104421.793325	37.764672
1932.546012	104589.601216	37.769690
1934.823095	104764.944127	37.774708
1936.628204	104922.914760	37.779725
1938.554927	105087.130824	37.784743
1940.390280	105252.236879	37.789760
1942.917230	105420.849243	37.794778
1944.378197	105583.872626	37.799796
1946.737540	105750.002258	37.804813
1948.694640	105912.556512	37.809831
1950.558772	106088.719015	37.814848
1952.874369	106248.074144	37.819866
1954.936767	106423.624073	37.824884
1956.903114	106579.104568	37.829901
1959.254208	106749.031730	37.834919
1961.028649	106908.144930	37.839936
1963.154945	107068.674730	37.844954
1965.133364	107232.220993	37.849972
1967.379839	107390.691950	37.854989
1969.332501	107548.664350	37.860007
1971.260710	107710.534234	37.865024
1973.550506	107872.589230	37.870042
1975.233762	108034.143901	37.875060
1977.046630	108192.052351	37.880077
1979.410800	108349.291940	37.885095
1980.977135	108505.693336	37.890112
1983.332122	108664.064385	37.895130
1985.226927	108838.435466	37.900148
1987.316066	108990.623237	37.905165
1989.223778	109154.849054	37.910183
1991.039636	109320.890739	37.915200
1993.193232	109480.298815	37.920218
1995.041824	109653.717421	37.925236
1997.076405	109804.332108	37.930253
1999.252564	109968.126609	37.935271
2001.001963	110132.115463	37.940288
2002.943581	110296.366677	37.945306
2005.120405	110467.620121	37.950324
2007.189006	110621.441412	37.955341
2009.346753	110783.289608	37.960359
2011.094708	110952.076164	37.965376
2013.497502	111109.106488	37.970394
2015.582870	111274.620606	37.975412
2017.466161	111432.773557	37.980429
2019.777023	111585.800204	37.985447
2021.257330	111751.132203	37.990464
2023.256370	111894.507216	37.995482
2025.071702	112033.624990	38.000500
2026.601002	112175.565454	38.005517
2029.094423	112321.540760	38.010535
2030.585362	112463.145943	38.015552
2032.965961	112617.370900	38.020570
2034.857804	112764.811825	38.025588
2036.531453	112913.682559	38.030605
2038.990811	113076.901686	38.035623
2040.956354	113239.095435	38.040640
2043.045095	113388.029998	38.045658
2044.828650	113545.129821	38.050676
2046.600067	113707.470181	38.055693
2048.704145	113876.975709	38.060711
2050.595304	114048.608006	38.065728
2052.755880	114209.190211	38.070746
2054.200764	114389.530980	38.075764
2056.244929	114575.029634	38.080781
2058.640791	114749.592123	38.085799
2060.299562	114937.283663	38.090816
2062.171490	115123.332042	38.095834
2064.103332	115316.981942	38.100852
2066.198865	115510.011129	38.105869
2068.315875	115699.993947	38.110887
2069.954245	115901.784830	38.115904
2072.391026	116106.635454	38.120922
2074.517368	116310.153264	38.125940
2076.630674	116505.987920	38.130957
2078.505413	116709.255548	38.135975
2080.752952	116921.851969	38.140992
2083.161821	117116.920599	38.146010
2085.518294	117318.898506	38.151028
2087.568347	117519.263834	38.156045
2089.973598	117711.330001	38.161063
2092.149998	117915.647781	38.166080
2094.691736	118109.609922	38.171098
2096.504183	118304.321376	38.176116
2098.940462	118492.619422	38.181133
2101.301890	118689.390607	38.186151
2103.248789	118888.358655	38.191168
2105.501517	119076.396561	38.196186
2107.914001	119268.291881	38.201204
2109.786396	119474.238474	38.206221
2112.074681	119651.986381	38.211239
2113.758252	119850.784982	38.216256
2115.959360	120043.478331	38.221274
2118.023927	120238.845151	38.226292
2120.284405	120445.522675	38.231309
2122.516702	120634.928680	38.236327
2124.513688	120835.560687	38.241344
2126.422285	121031.831174	38.246362
2128.605738	121237.573571	38.251380
2130.629941	121441.109354	38.256397
2132.913116	121639.087542	38.261415
2134.791372	121845.921086	38.266432
2137.013715	122045.154011	38.271450
2139.209820	122237.960470	38.276468
2141.023095	122444.832696	38.281485
2143.182493	122651.322023	38.286503
2145.115627	122863.898934	38.291520
2147.611345	123069.741588	38.296538
2149.914083	123285.332896	38.301556
2151.827138	123493.983687	38.306573
2154.036757	123686.097336	38.311591
2156.075151	123895.580575	38.316608
2158.309973	124107.609465	38.321626
2160.815554	124315.727814	38.326644
2162.414529	124520.677962	38.331661
2164.453606	124707.291955	38.336679
2166.383251	124895.179885	38.341696
2168.609993	125079.381191	38.346714
2170.656500	125270.335385	38.351732
2172.305719	125467.733983	38.356749
2174.566283	125663.325192	38.361767
2176.739482	125864.614650	38.366784
2178.643543	126070.958478	38.371802
2181.160951	126266.334772	38.376820
2182.912255	126479.986795	38.381837
2185.073385	126687.384573	38.386855
2187.273791	126916.865356	38.391872
2189.073206	127127.189200	38.396890
2191.493536	127334.879536	38.401908
2193.291949	127572.432436	38.406925
2195.549206	127802.860764	38.411943
2197.208976	128042.011253	38.416960
2199.278709	128285.958258	38.421978
2201.524652	128520.071664	38.426996
2203.838287	128768.880694	38.432013
2206.270595	129008.474071	38.437031
2208.050752	129257.661261	38.442048
2210.466368	129503.857676	38.447066
2212.869213	129764.382137	38.452084
2214.807039	130016.632263	38.457101
2217.083941	130274.172492	38.462119
2219.281395	130535.418940	38.467136
2221.823550	130789.862931	38.472154
2223.961995	131046.947303	38.477172
2226.385583	131311.411273	38.482189
2228.381514	131569.142771	38.487207
2230.704177	131834.348958	38.492224
2233.066401	132098.548173	38.497242
2235.505084	132359.932832	38.502260
2237.747258	132626.691746	38.507277
2240.053361	132881.870093	38.512295
2241.908728	133140.850963	38.517312
2244.250254	133413.753200	38.522330
2247.125747	133680.457469	38.527348
2249.660896	133942.686576	38.532365
2252.451784	134197.466739	38.537383
2254.792075	134449.666797	38.542400
2257.209930	134695.993676	38.547418
2259.572488	134951.479602	38.552436
2261.570708	135207.912238	38.557453
2264.238451	135449.077599	38.562471
2266.395763	135698.838815	38.567488
2268.352906	135950.815341	38.572506
2270.745311	136204.996627	38.577524
2272.963634	136460.399402	38.582541
2275.487629	136708.294133	38.587559
2277.684174	136968.322255	38.592576
2279.569452	137224.580843	38.597594
2282.105815	137474.800033	38.602612
2284.272425	137735.852359	38.607629
2286.565843	137988.853398	38.612647
2288.571694	138241.850036	38.617664
2290.920232	138502.700526	38.622682
2293.467591	138758.978187	38.627700
2295.577161	139030.249764	38.632717
2297.909900	139281.221136	38.637735
2300.423636	139540.719015	38.642752
2302.277380	139804.090703	38.647770
2304.795045	140061.915636	38.652788
2307.289926	140336.738573	38.657805
2309.366335	140584.393833	38.662823
2312.016854	140843.928152	38.667840
2314.226022	141090.803788	38.672858
2316.440854	141330.737756	38.677876
2318.492603	141581.917425	38.682893
2320.326343	141810.148657	38.687911
2322.934749	142050.075366	38.692928
2324.887095	142285.003958	38.697946
2327.218253	142535.484865	38.702964
2329.737739	142777.281989	38.707981
2332.165684	143038.220788	38.712999
2334.455222	143292.278372	38.718016
2336.278808	143555.865453	38.723034
2338.784647	143806.960046	38.728052
2340.743373	144062.418632	38.733069
2343.020276	144325.456563	38.738087
2344.816647	144598.508837	38.743104
2347.139494	144879.095438	38.748122
2349.779668	145155.115566	38.753140
2351.865457	145439.575360	38.758157
2354.075176	145715.742017	38.763175
2356.582315	146011.549391	38.768192
2358.259175	146291.292885	38.773210
2361.065959	146582.398562	38.778228
2363.370487	146884.385776	38.783245
2365.410137	147183.306496	38.788263
2367.778493	147488.790382	38.793280
2370.253726	147789.740715	38.798298
2372.508891	148105.615861	38.803316
2375.156756	148417.268197	38.808333
2377.371809	148720.612717	38.813351
2379.759774	149031.433497	38.818368
2382.441604	149340.445771	38.823386
2384.858098	149656.825295	38.828404
2387.756035	149970.351538	38.833421
2390.409619	150270.107486	38.838439
2392.748698	150573.988866	38.843456
2395.199474	150887.158774	38.848474
2397.963626	151194.264711	38.853492
2400.182846	151499.337776	38.858509
2403.276345	151799.782196	38.863527
2405.957502	152099.493042	38.868544
2408.402215	152392.997133	38.873562
2411.073237	152685.337606	38.878580
2413.229360	152990.162131	38.883597
2415.821951	153278.900182	38.888615
2418.225424	153568.316687	38.893632
2420.429961	153878.038328	38.898650
2422.763039	154176.405610	38.903668
2425.103635	154482.364445	38.908685
2427.812744	154783.189520	38.913703
2430.555696	155083.249201	38.918720
2432.781089	155381.055611	38.923738
2435.365789	155676.535011	38.928756
2438.157975	155980.780805	38.933773
2440.829351	156267.134894	38.938791
2443.109912	156557.283756	38.943808
2445.545543	156847.295526	38.948826
2448.231244	157146.003646	38.953844
2449.746999	157442.192252	38.958861
2452.321070	157742.875822	38.963879
2455.259388	158030.567665	38.968896
2457.473912	158341.986983	38.973914
2460.158088	158628.439205	38.978932
2462.329119	158926.233701	38.983949
2464.977178	159222.533147	38.988967
2467.462722	159519.189515	38.993984
2469.586973	159817.795434	38.999002
2472.144539	160122.479606	39.004020
2474.711011	160415.496678	39.009037
2476.447085	160709.978046	39.014055
2479.073458	160986.636489	39.019072
2480.905323	161275.443245	39.024090
2483.490804	161556.719103	39.029108
2485.937318	161847.666751	39.034125
2488.082905	162141.341617	39.039143
2490.328299	162432.577282	39.044160
2492.456773	162734.522562	39.049178
2494.592720	163033.725724	39.054196
2496.759999	163347.602045	39.059213
2499.131125	163668.075372	39.064231
2501.455395	163983.314036	39.069248
2503.763404	164318.972368	39.074266
2506.159645	164643.229952	39.079284
2508.184555	164984.166788	39.084301
2510.541420	165336.911926	39.089319
2513.084400	165671.829222	39.094336
2515.601811	166029.288633	39.099354
2518.570131	166384.774865	39.104372
2520.700981	166755.541130	39.109389
2523.192117	167115.371843	39.114407
2525.991806	167480.907818	39.119424
2528.177984	167848.014496	39.124442
2530.465926	168217.494188	39.129460
2533.161420	168599.672591	39.134477
2535.831710	168975.876613	39.139495
2538.701793	169342.566523	39.144512
2541.109216	169735.652079	39.149530
2543.754725	170109.516821	39.154548
2546.351647	170504.189390	39.159565
2548.832916	170874.858533	39.164583
2551.518808	171250.690786	39.169600
2553.853074	171647.949956	39.174618
2556.587489	172042.405911	39.179636
2559.456066	172437.909517	39.184653
2562.001977	172821.224949	39.189671
2564.772756	173213.547964	39.194688
2567.231749	173607.521645	39.199706
2569.757737	174010.908709	39.204724
2572.169686	174394.849556	39.209741
2574.781332	174799.928736	39.214759
2577.597301	175196.063871	39.219776
2579.958555	175596.449771	39.224794
2582.588023	175992.160791	39.229812
2585.652894	176404.173766	39.234829
2588.239026	176808.517623	39.239847
2590.877723	177197.286872	39.244864
2594.033373	177594.815215	39.249882
2597.112516	177982.985813	39.254900
2600.270924	178356.948675	39.259917
2602.650906	178738.679515	39.264935
2605.756425	179117.809575	39.269952
2608.589585	179504.780925	39.274970
2611.179759	179864.286232	39.279988
2613.713002	180245.618604	39.285005
2616.282042	180613.638467	39.290023
2619.220360	180988.713496	39.295040
2621.501164	181368.540750	39.300058
2623.638230	181738.715310	39.305076
2626.398933	182119.918253	39.310093
2628.977524	182543.033240	39.315111
2631.477861	182950.669219	39.320128
2633.821720	183349.797443	39.325146
2636.299142	183730.390716	39.330164
2638.869012	184106.907183	39.335181
2641.085060	184505.475910	39.340199
2643.809135	184899.598122	39.345216
2646.246118	185301.361118	39.350234
2648.667467	185692.739843	39.355252
2651.377616	186060.174099	39.360269
2653.359252	186438.569152	39.365287
2656.009860	186813.101801	39.370304
2658.234085	187193.976163	39.375322
2661.176157	187582.791302	39.380340
2663.949462	187965.055685	39.385357
2666.602823	188356.966715	39.390375
2668.955907	188732.416119	39.395392
2671.272161	189141.603813	39.400410
2673.667849	189535.388072	39.405428
2676.655506	189941.273208	39.410445
2678.864709	190360.489692	39.415463
2681.544678	190771.734514	39.420480
2684.088176	191184.805543	39.425498
2686.562866	191620.825488	39.430516
2689.107793	192040.731978	39.435533
2691.299977	192482.107918	39.440551
2693.916276	192921.945834	39.445568
2696.483338	193369.057650	39.450586
2698.924444	193831.710758	39.455604
2701.949529	194292.165878	39.460621
2704.720362	194744.864195	39.465639
2707.001784	195218.495055	39.470656
2709.835898	195690.821850	39.475674
2712.603608	196151.729977	39.480692
2715.717903	196631.534971	39.485709
2718.554719	197102.189578	39.490727
2721.530054	197579.301483	39.495744
2724.104966	198063.615462	39.500762
2726.434879	198543.320771	39.505780
2729.373649	199019.909520	39.510797
2732.366031	199502.384612	39.515815
2735.426783	199994.274662	39.520832
2737.719153	200474.575968	39.525850
2740.226456	200969.349749	39.530868
2743.312344	201461.646668	39.535885
2745.448970	201968.445827	39.540903
2748.170359	202463.901683	39.545920
2750.880180	202972.138201	39.550938
2753.331551	203492.177962	39.555956
2756.334102	204002.886370	39.560973
2759.075486	204523.010598	39.565991
2762.036731	205033.905982	39.571008
2764.659947	205559.233560	39.576026
2767.551188	206082.488306	39.581044
2770.397461	206603.592109	39.586061
2772.839677	207129.409103	39.591079
2775.455219	207659.950597	39.596096
2778.608306	208192.035030	39.601114
2780.733541	208721.563247	39.606132
2784.133120	209250.436028	39.611149
2786.863931	209786.425819	39.616167
2790.100391	210311.287128	39.621184
2792.416491	210843.736594	39.626202
2795.490041	211382.394061	39.631220
2798.713570	211909.927702	39.636237
2801.220359	212454.315307	39.641255
2804.035978	212976.859220	39.646272
2806.816031	213514.956555	39.651290
2809.254794	214064.285723	39.656308
2812.233841	214595.062691	39.661325
2814.869804	215151.958320	39.666343
2817.560303	215688.573939	39.671360
2820.285471	216229.859110	39.676378
2823.019669	216785.344274	39.681396
2826.097893	217334.780947	39.686413
2828.857358	217885.131784	39.691431
2831.664020	218418.582153	39.696448
2834.482404	218933.892725	39.701466
2836.945361	219461.656435	39.706484
2839.981730	219970.862144	39.711501
2842.308953	220504.058868	39.716519
2845.022039	221026.729106	39.721536
2847.978707	221561.631682	39.726554
2850.531891	222095.454430	39.731572
2853.565842	222619.497849	39.736589
2855.959958	223168.004013	39.741607
2858.691734	223706.753156	39.746624
2861.148148	224258.679380	39.751642
2863.733338	224826.285258	39.756660
2866.824554	225397.165364	39.761677
2869.310497	225965.066216	39.766695
2872.192795	226545.937312	39.771712
2875.110747	227137.370814	39.776730
2877.723843	227714.803373	39.781748
2880.567411	228313.361259	39.786765
2882.830932	228898.418418	39.791783
2886.104865	229514.284759	39.796800
2888.884683	230119.659900	39.801818
2891.282354	230744.630029	39.806836
2894.324196	231350.776157	39.811853
2897.420847	231978.785953	39.816871
2899.872100	232608.191623	39.821888
2903.367398	233230.904495	39.826906
2906.048799	233867.436561	39.831924
2909.772434	234502.712407	39.836941
2912.500695	235140.556352	39.841959
2915.214210	235776.648750	39.846976
2918.689504	236405.126875	39.851994
2920.913553	237039.617024	39.857012
2924.511786	237690.454248	39.862029
2927.636051	238332.981122	39.867047
2930.586696	238979.979427	39.872064
2933.602795	239617.998666	39.877082
2936.062876	240265.528070	39.882100
2938.737352	240906.417532	39.887117
2942.150359	241562.863723	39.892135
2945.316403	242224.249618	39.897152
2948.411902	242863.213769	39.902170
2951.600474	243523.271521	39.907188
2954.502037	244174.328743	39.912205
2957.381041	244825.336712	39.917223
2960.520928	245480.366292	39.922240
2963.608476	246141.828809	39.927258
2966.245865	246805.467893	39.932276
2969.389341	247451.878784	39.937293
2972.589874	248111.360734	39.942311
2975.435262	248767.491861	39.947328
2978.765486	249425.449850	39.952346
2981.837061	250090.736132	39.957364
2984.995777	250742.009553	39.962381
2987.896130	251395.657699	39.967399
2991.129664	252040.258746	39.972416
2994.667374	252692.938044	39.977434
2997.667090	253343.158438	39.982452
3001.289453	253986.953570	39.987469
3004.065293	254635.933030	39.992487
3007.079753	255268.285106	39.997504
3009.890736	255903.739592	40.002522
3012.580962	256555.314171	40.007540
3015.725631	257192.183504	40.012557
3019.086497	257850.352491	40.017575
3021.648612	258485.909349	40.022592
3024.936301	259133.059079	40.027610
3027.273587	259783.986195	40.032628
3030.380833	260409.998699	40.037645
3033.398255	261036.402866	40.042663
3036.415840	261652.999180	40.047680
3039.161681	262272.479368	40.052698
3041.756594	262903.079319	40.057716
3044.493271	263519.277303	40.062733
3047.598390	264144.888067	40.067751
3050.300201	264783.968941	40.072768
3052.874250	265423.523013	40.077786
3055.286373	266077.880523	40.082804
3058.542206	266724.609186	40.087821
3061.788092	267388.733148	40.092839
3064.377603	268049.932782	40.097856
3067.240249	268725.739866	40.102874
3069.772575	269412.641859	40.107892
3073.038668	270112.503867	40.112909
3075.913137	270803.253183	40.117927
3078.694223	271515.396385	40.122944
3081.912708	272224.570151	40.127962
3085.043061	272935.072542	40.132980
3088.273901	273639.788242	40.137997
3091.490457	274360.119163	40.143015
3094.535083	275088.241993	40.148032
3097.520756	275805.472625	40.153050
3100.699377	276541.027926	40.158068
3103.983430	277277.474171	40.163085
3107.535551	278003.103922	40.168103
3110.841176	278734.098383	40.173120
3114.248862	279460.549574	40.178138
3117.542967	280191.303202	40.183156
3120.703777	280924.838464	40.188173
3123.932657	281664.323356	40.193191
3127.384461	282399.702795	40.198208
3130.804360	283121.494038	40.203226
3133.593689	283865.849619	40.208244
3136.729744	284598.919263	40.213261
3140.151792	285328.076648	40.218279
3143.629613	286068.644120	40.223296
3147.031841	286799.363024	40.228314
3150.553632	287543.716054	40.233332
3153.727708	288267.522313	40.238349
3157.330208	288985.743540	40.243367
3160.650674	289711.465788	40.248384
3164.027535	290443.874065	40.253402
3166.910262	291164.493640	40.258420
3170.453752	291876.648104	40.263437
3173.808275	292589.610907	40.268455
3177.380230	293312.179374	40.273472
3180.630978	294022.957909	40.278490
3183.483526	294735.618189	40.283508
3186.951032	295452.235845	40.288525
3190.622066	296160.993195	40.293543
3193.818047	296866.744119	40.298560
3197.189108	297573.601359	40.303578
3200.255734	298265.544113	40.308596
3203.547177	298968.918122	40.313613
3207.002622	299680.762116	40.318631
3210.476510	300375.889656	40.323648
3213.791950	301064.737287	40.328666
3216.716779	301765.441575	40.333684
3219.936212	302453.930918	40.338701
3223.686499	303156.213960	40.343719
3226.321249	303850.005763	40.348736
3229.671540	304532.456451	40.353754
3233.204526	305233.095324	40.358772
3236.545368	305925.098723	40.363789
3240.165833	306605.296373	40.368807
3243.491648	307290.988217	40.373824
3247.018924	307947.778884	40.378842
3250.374518	308597.683610	40.383860
3253.580725	309211.788895	40.388877
3257.108520	309840.887520	40.393895
3259.998513	310467.920221	40.398912
3263.470469	311093.000877	40.403930
3266.517860	311712.251333	40.408948
3269.524585	312358.885504	40.413965
3273.225599	312982.077867	40.418983
3276.066531	313610.091590	40.424000
3279.361687	314255.486761	40.429018
3282.502844	314901.277587	40.434036
3285.402261	315544.229235	40.439053
3288.594939	316190.044366	40.444071
3291.581818	316852.657174	40.449088
3295.072295	317507.212809	40.454106
3298.321780	318170.500783	40.459124
3301.552427	318834.086179	40.464141
3304.828444	319502.069850	40.469159
3308.166520	320188.151949	40.474176
3311.388601	320850.895653	40.479194
3314.930535	321527.053262	40.484212
3318.112765	322222.642630	40.489229
3321.323330	322908.751401	40.494247
3323.818874	323606.455065	40.499264
3328.058079	324310.598321	40.504282
3330.890046	325007.007753	40.509300
3334.277868	325736.632650	40.514317
3337.767611	326434.310273	40.519335
3340.667483	327150.411779	40.524352
3344.170869	327868.993953	40.529370
3347.753083	328600.083953	40.534388
3350.714141	329319.688620	40.539405
3354.376222	330048.252848	40.544423
3357.669900	330784.750876	40.549440
3360.949177	331517.025847	40.554458
3364.754949	332256.840382	40.559476
3367.834394	332987.875306	40.564493
3371.602123	333732.537604	40.569511
3374.680062	334474.654797	40.574528
3378.437919	335207.062397	40.579546
3382.028958	335968.880642	40.584564
3384.904473	336718.492756	40.589581
3388.722825	337457.643933	40.594599
3391.959967	338219.445147	40.599616
3395.752461	338960.877750	40.604634
3399.120654	339711.137001	40.609652
3402.563500	340469.205814	40.614669
3406.150263	341215.188808	40.619687
3410.028864	341976.859872	40.624704
3413.746460	342706.559126	40.629722
3416.965161	343454.631307	40.634740
3420.637180	344207.713700	40.639757
3424.037536	344952.098322	40.644775
3427.509807	345699.320935	40.649792
3430.898915	346435.914869	40.654810
3434.502430	347178.240672	40.659828
3437.790236	347924.022518	40.664845
3441.765964	348663.695863	40.669863
3444.924470	349416.209086	40.674880
3448.061979	350163.713264	40.679898
3452.026631	350899.788030	40.684916
3455.202045	351642.384063	40.689933
3458.902368	352383.942790	40.694951
3462.184300	353135.336020	40.699968
3465.261097	353873.965879	40.704986
3468.646789	354619.603359	40.710004
3472.292381	355373.421677	40.715021
3476.248047	356098.307280	40.720026
3479.349809	356800.707240	40.725031
3482.110328	357459.635082	40.730036
3485.477177	358058.070532	40.735040
3489.186520	358602.360865	40.740045
3492.656043	359087.542769	40.745050
3495.459925	359531.525346	40.750055
3498.178294	359910.408292	40.755060
3501.097808	360232.636878	40.760064
3503.531135	360501.115674	40.765069
3505.934110	360707.871813	40.770074
3508.312728	360879.409913	40.775079
3510.507102	361005.667223	40.780084
3512.256385	361065.898570	40.785088
3513.764034	361107.236101	40.790093
3515.787642	361089.563948	40.795098
3517.181490	361057.581969	40.800103
3518.129121	360974.897603	40.805108
3519.870512	360858.545638	40.810112
3520.930358	360716.811841	40.815117
3521.935876	360549.877326	40.820122
3523.192500	360354.949426	40.825127
3523.834997	360139.761115	40.830132
3524.613666	359900.713161	40.835136
3525.091517	359641.227785	40.840141
3525.886753	359363.799927	40.845146
3526.168672	359071.837257	40.850151
3526.528328	358761.765329	40.855156
3527.120179	358440.522782	40.860160
3527.660637	358117.073883	40.865165
3527.959121	357773.607621	40.870170
3528.225133	357416.342538	40.875175
3528.266837	357050.975651	40.880180
3528.720555	356681.397367	40.885184
3528.452823	356314.570658	40.890189
3528.853705	355931.674035	40.895194
3528.451810	355553.193509	40.900199
3528.974643	355160.000278	40.905204
3529.457195	354763.377162	40.910208
3528.928038	354362.942159	40.915213
3529.180728	353960.575206	40.920218
3529.236594	353553.760401	40.925223
3529.147079	353152.478796	40.930228
3529.242945	352741.783809	40.935232
3529.004448	352343.616331	40.940237
3528.798782	351931.407535	40.945242
3529.008265	351516.586620	40.950247
3528.855776	351110.891735	40.955252
3528.939427	350693.131239	40.960256
3528.338366	350285.157504	40.965261
3528.863501	349868.105403	40.970266
3528.418843	349458.800423	40.975271
3527.968712	349043.822262	40.980276
3527.953731	348631.719723	40.985280
3527.907774	348229.073783	40.990285
3527.722382	347819.199442	40.995290
3527.487239	347420.462836	41.000295
3527.253457	347010.255594	41.005300
3527.413210	346611.778080	41.010304
3526.973288	346221.016578	41.015309
3526.682230	345810.752766	41.020314
3526.529674	345416.581087	41.025319
3526.146495	345017.330605	41.030324
3526.424481	344630.862299	41.035328
3525.968397	344243.563655	41.040333
3526.211947	343851.600154	41.045338
3525.833523	343470.840305	41.050343
3525.780925	343083.236653	41.055348
3525.626594	342698.746521	41.060352
3525.343151	342309.136209	41.065357
3525.100830	341923.023960	41.070362
3524.656257	341550.338974	41.075367
3524.499578	341175.799689	41.080372
3524.614877	340795.365601	41.085376
3524.494116	340429.483470	41.090381
3524.347781	340057.880280	41.095386
3523.685615	339696.067381	41.100391
3522.933800	339332.459400	41.105396
3523.147673	338976.223616	41.110400
3522.832663	338630.518241	41.115405
3522.746267	338279.026813	41.120410
3522.488820	337931.932549	41.125415
3522.124800	337587.140275	41.130420
3522.115352	337241.856980	41.135424
3521.912330	336912.774207	41.140429
3521.669563	336574.819495	41.145434
3521.294077	336238.967713	41.150439
3521.239334	335913.413041	41.155444
3520.839762	335594.241717	41.160448
3520.472550	335263.720245	41.165453
3520.855210	334947.854261	41.170458
3520.359800	334633.140130	41.175463
3519.922681	334312.081687	41.180468
3520.043373	333999.605620	41.185472
3519.660158	333694.097878	41.190477
3519.510875	333393.154361	41.195482
3519.550110	333086.990692	41.200487
3519.292631	332794.223208	41.205492
3518.949017	332484.757372	41.210496
3518.898907	332195.437180	41.215501
3518.467151	331903.910873	41.220506
3518.139451	331615.112910	41.225511
3517.513663	331332.845010	41.230516
3517.923026	331051.049053	41.235520
3517.473930	330781.084998	41.240525
3517.597756	330506.959976	41.245530
3517.342219	330235.690127	41.250535
3517.018921	329960.842669	41.255540
3516.700518	329695.454309	41.260544
3516.054027	329441.484936	41.265549
3516.098809	329181.097888	41.270554
3516.191032	328929.934764	41.275559
3515.676881	328674.617085	41.280564
3516.006466	328423.769719	41.285568
3515.174725	328190.373321	41.290573
3515.255476	327943.784175	41.295578
3515.155668	327700.503000	41.300583
3515.141482	327469.696222	41.305588
3515.284612	327227.824052	41.310592
3515.203702	326999.237963	41.315597
3514.652422	326749.077348	41.320602
3514.988003	326517.727093	41.325607
3514.769338	326289.082183	41.330612
3514.428642	326049.924015	41.335616
3514.383731	325835.952127	41.340621
3513.854450	325606.537916	41.345626
3513.984785	325385.006727	41.350631
3513.828488	325165.477858	41.355636
3513.697234	324937.854610	41.360640
3513.663211	324728.352279	41.365645
3513.239980	324512.550160	41.370650
3513.252593	324304.259406	41.375655
3512.891098	324097.959410	41.380660
3513.063572	323891.880166	41.385664
3512.780886	323683.683319	41.390669
3512.746400	323480.356326	41.395674
3512.671159	323279.807562	41.400679
3512.530078	323084.966489	41.405684
3512.572128	322885.160658	41.410688
3512.482434	322696.898504	41.415693
3512.195308	322496.709808	41.420698
3512.134042	322289.209113	41.425703
3511.968858	322095.333901	41.430708
3512.105507	321898.790302	41.435712
3511.731877	321719.395781	41.440717
3511.675214	321524.559697	41.445722
3511.482558	321349.765409	41.450727
3511.463915	321154.998002	41.455732
3511.365972	320970.112980	41.460736
3510.943852	320803.722213	41.465741
3510.778005	320623.425594	41.470746
3510.552173	320446.750175	41.475751
3510.310903	320279.082493	41.480756
3510.441318	320105.504634	41.485760
3510.411411	319954.262915	41.490765
3510.176253	319775.245615	41.495770
3510.068816	319614.601607	41.500775
3509.966751	319452.836744	41.505780
3510.350318	319284.711325	41.510784
3510.032807	319134.809211	41.515789
3509.362148	318973.869255	41.520794
3509.442714	318816.881927	41.525799
3508.963904	318661.533434	41.530804
3508.917827	318514.639759	41.535808
3509.005520	318380.140346	41.540813
3509.310900	318231.918677	41.545818
3508.799713	318088.836265	41.550823
3508.734852	317946.268778	41.555828
3508.943202	317796.152643	41.560832
3508.676660	317665.039356	41.565837
3508.852366	317516.352144	41.570842
3508.600765	317378.976830	41.575847
3508.383334	317245.870104	41.580852
3508.543209	317105.223844	41.585856
3508.116042	316971.691115	41.590861
3508.580983	316842.013039	41.595866
3508.501963	316706.771302	41.600871
3508.149933	316573.429174	41.605876
3508.130311	316440.111008	41.610880
3507.485873	316324.725760	41.615885
3507.377605	316188.494743	41.620890
3507.614980	316063.429758	41.625895
3507.519425	315948.135831	41.630900
3507.790211	315822.734189	41.635904
3507.759328	315713.688628	41.640909
3507.772391	315592.855575	41.645914
3507.094419	315471.061603	41.650919
3507.081070	315352.318411	41.655924
3507.457964	315235.142296	41.660928
3507.220572	315115.721085	41.665933
3506.985722	314999.963080	41.670938
3506.927424	314893.260661	41.675943
3507.144326	314785.522652	41.680948
3507.005917	314656.212488	41.685952
3506.897536	314547.328899	41.690957
3506.580276	314434.559301	41.695962
3506.761267	314321.660640	41.700967
3506.221013	314225.362371	41.705972
3506.672372	314121.962561	41.710976
3506.412285	314022.566741	41.715981
3506.475932	313909.914411	41.720986
3506.593835	313813.843159	41.725991
3506.198880	313705.129593	41.730996
3506.626423	313601.248889	41.736000
3506.441217	313509.549981	41.741005
3506.308054	313409.115204	41.746010
3506.123351	313298.917459	41.751015
3505.773020	313198.058169	41.756020
3506.187936	313107.180656	41.761024
3506.110473	313002.944997	41.766029
3505.829560	312901.463529	41.771034
3505.874120	312814.739995	41.776039
3505.862857	312730.315089	41.781044
3505.798824	312628.086654	41.786048
3505.726194	312548.302035	41.791053
3505.809998	312441.698945	41.796058
3505.889162	312349.625627	41.801063
3505.257667	312249.495261	41.806068
3505.186849	312166.961605	41.811072
3505.295043	312087.682284	41.816077
3504.897272	312001.229958	41.821082
3505.509403	311915.688299	41.826087
3505.101962	311837.201645	41.831092
3505.197828	311757.211217	41.836096
3505.083773	311665.802906	41.841101
3505.344969	311597.186033	41.846106
3505.080371	311513.816371	41.851111
3505.073576	311434.452144	41.856116
3505.065798	311344.807804	41.861120
3504.890908	311272.721661	41.866125
3504.608350	311193.781831	41.871130
3504.791668	311110.341432	41.876135
3504.526520	311034.197675	41.881140
3504.794460	310959.090082	41.886144
3504.493340	310880.534325	41.891149
3504.770054	310805.374225	41.896154
3504.755732	310741.939315	41.901159
3504.347500	310675.537801	41.906164
3504.576573	310593.310761	41.911168
3504.342861	310525.151407	41.916173
3504.250560	310461.092156	41.921178
3504.652832	310377.997938	41.926183
3504.495210	310317.740220	41.931188
3504.557161	310241.722185	41.936192
3504.204097	310184.828342	41.941197
3504.087876	310108.252681	41.946202
3504.190054	310036.630282	41.951207
3504.139084	309966.889323	41.956212
3504.093185	309904.501551	41.961216
3504.071674	309841.448271	41.966221
3504.121193	309776.297174	41.971226
3504.217070	309719.027232	41.976231
3504.053462	309646.249809	41.981236
3503.707550	309579.429885	41.986240
3503.617116	309517.761086	41.991245
3503.657715	309456.453426	41.996250
3503.848022	309392.272228	42.001255
3503.559474	309343.688446	42.006260
3503.858672	309286.538887	42.011264
3503.358804	309226.715015	42.016269
3503.278629	309175.146635	42.021274
3503.668108	309112.384409	42.026279
3502.908624	309061.812758	42.031284
3503.042950	309003.747100	42.036288
3503.046464	308964.125556	42.041293
3503.025924	308911.377004	42.046298
3503.100294	308856.883148	42.051303
3503.053631	308814.393794	42.056308
3503.364905	308763.705325	42.061312
3503.046514	308717.950227	42.066317
3502.778910	308657.224136	42.071322
3503.018000	308602.195296	42.076327
3503.048635	308565.190264	42.081332
3502.941642	308521.768535	42.086336
3502.558463	308473.504047	42.091341
3503.099505	308422.524829	42.096346
3503.250065	308382.727141	42.101351
3502.802020	308346.102148	42.106356
3502.771464	308287.145307	42.111360
3502.915035	308249.079032	42.116365
3502.849428	308193.741105	42.121370
3502.775821	308159.653083	42.126375
3502.639337	308110.484452	42.131380
3502.866509	308066.170307	42.136384
3502.589455	308025.217696	42.141389
3502.732931	307983.843039	42.146394
3503.035948	307931.297323	42.151399
3502.710021	307899.742441	42.156404
3502.598436	307851.511223	42.161408
3502.699149	307805.562512	42.166413
3502.553415	307770.518483	42.171418
3502.797430	307726.634011	42.176423
3502.556413	307690.586910	42.181428
3502.552024	307650.151211	42.186432
3502.204030	307608.496806	42.191437
3502.065181	307573.680590	42.196442
3502.565541	307527.083840	42.201447
3502.507059	307510.857417	42.206452
3502.361690	307460.213549	42.211456
3502.286889	307424.140267	42.216461
3502.272993	307386.097945	42.221466
3502.353959	307347.277324	42.226471
3502.243466	307322.228521	42.231476
3502.579748	307285.378327	42.236480
3502.533611	307254.084666	42.241485
3502.628849	307206.838407	42.246490
3502.428493	307167.323633	42.251495
3502.504509	307131.404697	42.256500
3502.426888	307087.849873	42.261504
3502.363150	307051.520111	42.266509
3502.110087	307016.823154	42.271514
3502.373961	306976.955722	42.276519
3502.279287	306957.884582	42.281524
3502.457181	306908.029402	42.286528
3502.428590	306874.009802	42.291533
3502.464218	306841.888756	42.296538
3502.222738	306796.272540	42.301543
3502.006084	306770.985575	42.306548
3502.026786	306740.724521	42.311552
3502.005171	306704.998679	42.316557
3502.158520	306671.866636	42.321562
3502.441999	306643.523962	42.326567
3502.272073	306600.008592	42.331572
3502.642745	306563.483317	42.336576
3502.106154	306531.629671	42.341581
3502.133683	306498.211802	42.346586
3502.473512	306463.014594	42.351591
3502.237725	306434.880226	42.356596
3502.398340	306401.212450	42.361600
3502.206881	306367.523350	42.366605
3501.985517	306328.036645	42.371610
3502.373955	306289.218028	42.376615
3501.923455	306259.259388	42.381620
3502.256255	306223.248758	42.386624
3501.974621	306195.833983	42.391629
3501.929213	306168.331364	42.396634
3502.317830	306145.774248	42.401639
3502.077923	306110.133008	42.406644
3502.089464	306070.202510	42.411648
3501.991399	306044.794844	42.416653
3501.810876	306013.725007	42.421658
3502.169260	305981.654746	42.426663
3501.908261	305954.083921	42.431668
3501.740020	305929.068898	42.436672
3501.898984	305896.953414	42.441677
3501.364742	305868.280069	42.446682
3502.254085	305850.225308	42.451687
3501.706428	305822.139355	42.456692
3502.259220	305791.387364	42.461696
3502.287555	305757.230863	42.466701
3501.392653	305720.342964	42.471706
3501.950084	305693.432957	42.476711
3501.811683	305667.344289	42.481716
3502.069871	305637.096341	42.486720
3501.978176	305612.069194	42.491725
3501.810113	305579.699250	42.496730
3501.783659	305545.780213	42.501735
3501.633531	305530.025556	42.506740
3501.433752	305494.606648	42.511744
3501.664651	305477.825347	42.516749
3501.516669	305456.904200	42.521754
3502.115965	305432.863240	42.526759
3501.609359	305416.273566	42.531764
3501.714344	305384.522482	42.536768
3502.106563	305350.385166	42.541773
3501.763778	305335.933018	42.546778
3501.959057	305308.163262	42.551783
3501.606570	305281.624335	42.556788
3501.659731	305246.801935	42.561792
3501.836862	305236.085832	42.566797
3501.570899	305199.201020	42.571802
3501.754216	305178.736945	42.576807
3501.353937	305152.434464	42.581812
3501.920075	305136.974890	42.586816
3501.795111	305102.383833	42.591821
3501.578523	305079.590022	42.596826
3501.584791	305049.330212	42.601831
3501.188473	305041.350431	42.606836
3501.500822	305001.626556	42.611840
3501.138103	304985.930416	42.616845
3501.157958	304974.857109	42.621850
3501.370599	304941.231128	42.626855
3501.252552	304943.540198	42.631860
3501.666144	304910.391765	42.636864
3501.365076	304890.359591	42.641869
3501.313051	304876.090899	42.646874
3501.608120	304835.936960	42.651879
3501.352688	304835.722589	42.656884
3501.364290	304804.418381	42.661888
3501.220103	304795.152129	42.666893
3501.532896	304775.532926	42.671898
3501.370911	304751.127127	42.676903
3501.696393	304746.368311	42.681908
3501.669958	304708.911263	42.686912
3501.767915	304692.964866	42.691917
3501.662197	304674.988911	42.696922
3501.629085	304642.139186	42.701927
3501.586773	304620.692189	42.706932
3501.774619	304605.164350	42.711936
3501.792086	304576.124079	42.716941
3501.970142	304548.687446	42.721946
3501.813843	304517.282065	42.726951
3501.643876	304486.973127	42.731956
3501.646252	304467.122393	42.736960
3501.768715	304441.526753	42.741965
3501.591316	304419.082813	42.746970
3501.776340	304390.830624	42.751975
3501.616341	304379.072721	42.756980
3501.511409	304344.656167	42.761984
3501.753217	304327.923683	42.766989
3501.414861	304311.612739	42.771994
3501.826665	304285.539145	42.776999
3501.510464	304262.531498	42.782004
3501.760605	304233.505556	42.787009
3501.658925	304212.703909	42.792013
3501.609026	304180.187358	42.797018
3501.806584	304164.479721	42.802023
3501.500802	304143.379111	42.807028
3501.702882	304119.501436	42.812033
3501.910786	304097.098917	42.817037
3501.528981	304077.588041	42.822042
3501.781834	304045.762111	42.827047
3501.414539	304033.094901	42.832052
3501.402774	303998.663551	42.837057
3501.633831	303992.061602	42.842061
3501.706328	303966.677135	42.847066
3501.452583	303942.972441	42.852071
3501.679784	303923.086348	42.857076
3501.577740	303896.889295	42.862081
3501.569586	303870.982947	42.867085
3501.217636	303852.994301	42.872090
3501.518335	303835.692557	42.877095
3501.574197	303814.713422	42.882100
3501.582776	303792.952727	42.887105
3501.754201	303778.776045	42.892109
3501.636679	303754.668221	42.897114
3501.540594	303728.800998	42.902119
3501.093487	303697.313335	42.907124
3501.254845	303679.651576	42.912129
3501.689576	303668.080480	42.917133
3501.438525	303647.734605	42.922138
3501.504429	303625.913979	42.927143
3501.327624	303608.406863	42.932148
3501.299745	303584.335845	42.937153
3501.465886	303568.480241	42.942157
3501.249058	303553.168053	42.947162
3501.317237	303528.547544	42.952167
3501.518803	303511.821088	42.957172
3501.328009	303493.425374	42.962177
3501.382773	303476.391009	42.967181
3501.232005	303454.044287	42.972186
3501.247538	303442.869527	42.977191
3501.432769	303422.073607	42.982196
3501.667123	303397.503406	42.987201
3501.523413	303381.161738	42.992205
3501.219459	303355.530428	42.997210
3501.637195	303336.835922	43.002215
3501.182972	303314.332982	43.007220
3501.269575	303301.849131	43.012225
3501.547270	303277.195747	43.017229
3500.732720	303266.812425	43.022234
3501.007629	303250.354369	43.027239
3501.000445	303237.376165	43.032244
3500.796406	303217.480873	43.037249
3500.954070	303208.956096	43.042253
3500.795802	303207.733975	43.047258
3501.247663	303204.762213	43.052263
3501.018647	303174.461739	43.057268
3501.210128	303167.407772	43.062273
3500.903142	303146.968646	43.067277
3500.775661	303127.035901	43.072282
3501.163557	303121.656376	43.077287
3500.671928	303109.237430	43.082292
3500.888972	303100.041650	43.087297
3500.963687	303099.088503	43.092301
3500.817734	303081.983588	43.097306
3501.263436	303060.714151	43.102311
3500.769164	303054.454533	43.107316
3501.080943	303040.357508	43.112321
3500.959080	303019.685790	43.117325
3500.696441	303013.771705	43.122330
3500.949846	303007.955093	43.127335
3500.691865	302992.725524	43.132340
3500.863780	302967.070527	43.137345
3500.958966	302954.916103	43.142349
3501.029346	302956.508648	43.147354
3501.030752	302940.347756	43.152359
3500.963419	302912.083317	43.157364
3501.031754	302916.017600	43.162369
3501.256164	302910.460012	43.167373
3500.880208	302889.751616	43.172378
3500.952656	302867.089793	43.177383
3501.248297	302866.025752	43.182388
3500.874392	302850.839716	43.187393
3501.174241	302826.488059	43.192397
3500.979353	302821.530470	43.197402
3501.327237	302808.700250	43.202407
3501.105668	302803.746830	43.207412
3501.279936	302770.761698	43.212417
3501.177190	302757.340210	43.217421
3500.882387	302744.025096	43.222426
3501.275249	302717.342873	43.227431
3501.377773	302720.253814	43.232436
3501.299531	302691.940061	43.237441
3500.994270	302681.171596	43.242445
3501.020834	302675.924868	43.247450
3501.251738	302648.631672	43.252455
3500.855657	302634.059848	43.257460
3500.838986	302626.936551	43.262465
3501.439267	302619.284142	43.267469
3501.118393	302604.751453	43.272474
3500.841133	302590.466444	43.277479
3500.971070	302588.410289	43.282484
3501.189734	302560.228200	43.287489
3501.027248	302547.325006	43.292493
3501.035686	302546.840317	43.297498
3501.353025	302518.999084	43.302503
3501.209387	302501.639115	43.307508
3501.130900	302499.182885	43.312513
3501.130576	302489.104767	43.317517
3500.466197	302468.797603	43.322522
3500.832615	302453.012152	43.327527
3501.165074	302451.789644	43.332532
3501.062470	302440.709492	43.337537
3501.342971	302423.563142	43.342541
3501.232052	302411.618969	43.347546
3501.358821	302378.284711	43.352551
3500.887014	302369.960012	43.357556
3500.862154	302368.717013	43.362561
3501.211030	302351.279996	43.367565
3500.927973	302338.090194	43.372570
3501.433086	302319.585271	43.377575
3500.952788	302308.996797	43.382580
3500.672884	302281.630569	43.387585
3500.765675	302269.018253	43.392589
3500.683505	302273.052466	43.397594
3501.013432	302262.897224	43.402599
3501.004250	302260.913707	43.407604
3500.856817	302238.896802	43.412609
3501.041957	302222.656065	43.417613
3500.374122	302219.757499	43.422618
3501.015079	302212.098673	43.427623
3500.681918	302199.400231	43.432628
3500.550127	302186.339446	43.437633
3500.923747	302170.145577	43.442637
3500.821741	302164.867997	43.447642
3501.244741	302163.631327	43.452647
3501.045103	302146.305447	43.457652
3501.171600	302126.638023	43.462657
3500.759943	302119.601859	43.467661
3501.374891	302112.354294	43.472666
3501.315951	302094.421037	43.477671
3501.143449	302084.929674	43.482676
3501.448544	302062.332936	43.487681
3501.494021	302045.503164	43.492685
3501.332832	302030.003679	43.497690
3501.083897	302008.053448	43.502695
3501.037674	302000.552927	43.507700
3500.831448	301987.656434	43.512705
3501.178846	301956.552525	43.517709
3500.800468	301953.812296	43.522714
3501.104224	301945.264476	43.527719
3500.725813	301929.468062	43.532724
3500.625542	301911.973866	43.537729
3500.831734	301899.114678	43.542733
3501.005029	301897.815238	43.547738
3500.997495	301889.036118	43.552743
3501.143976	301877.509695	43.557748
3500.888105	301859.810752	43.562753
3501.119194	301854.888277	43.567757
3500.992454	301838.721632	43.572762
3500.936707	301818.777176	43.577767
3500.896078	301822.830379	43.582772
3500.946925	301818.877756	43.587777
3501.058483	301794.096950	43.592781
3500.749749	301780.656517	43.597786
3501.003879	301766.390011	43.602791
3501.073817	301767.117336	43.607796
3501.114384	301755.734698	43.612801
3501.225002	301735.458793	43.617805
3501.138241	301730.306041	43.622810
3501.178099	301721.214075	43.627815
3500.986436	301694.062805	43.632820
3501.116768	301684.218616	43.637825
3501.223259	301673.945489	43.642829
3500.590423	301650.909844	43.647834
3500.927089	301633.398148	43.652839
3501.098989	301628.764864	43.657844
3500.698762	301625.111805	43.662849
3501.242882	301614.312133	43.667853
3501.106454	301602.651724	43.672858
3501.054442	301585.735246	43.677863
3500.765951	301573.793194	43.682868
3501.016294	301544.358522	43.687873
3501.170968	301534.815910	43.692877
3500.913944	301520.298391	43.697882
3501.086650	301514.926897	43.702887
3501.133090	301504.917634	43.707892
3500.998967	301498.270663	43.712897
3500.823511	301492.062817	43.717901
3500.770270	301471.481569	43.722906
3501.035403	301448.330899	43.727911
3500.879922	301448.533550	43.732916
3500.809506	301442.182023	43.737921
3500.930904	301416.966838	43.742925
3500.865269	301409.800130	43.747930
3501.118235	301394.362965	43.752935
3500.997090	301396.749027	43.757940
3501.288465	301377.971782	43.762945
3501.194562	301365.235735	43.767949
3501.328638	301360.150225	43.772954
3501.251459	301333.209931	43.777959
3501.026679	301319.807158	43.782964
3500.926596	301320.306560	43.787969
3501.003349	301287.284851	43.792973
3501.085758	301270.067296	43.797978
3501.137135	301264.180275	43.802983
3500.973004	301263.315338	43.807988
3501.069091	301244.110460	43.812993
3501.168879	301231.496804	43.817997
3500.876883	301230.066484	43.823002
3500.967897	301207.884620	43.828007
3500.867976	301193.189744	43.833012
3500.757538	301182.034201	43.838017
3500.834555	301166.853537	43.843021
3500.815798	301166.525794	43.848026
3500.963799	301148.458061	43.853031
3501.196320	301144.171573	43.858036
3500.999251	301133.080466	43.863041
3501.040273	301108.539429	43.868045
3500.675988	301092.486048	43.873050
3500.838926	301083.909204	43.878055
3500.940593	301073.662167	43.883060
3500.540662	301074.666569	43.888065
3501.000595	301052.045198	43.893069
3500.904279	301045.010493	43.898074
3501.144349	301030.873245	43.903079
3501.239918	301030.196763	43.908084
3501.121864	301007.156713	43.913089
3501.063494	300996.832877	43.918093
3501.324658	300993.865356	43.923098
3501.352532	300966.755748	43.928103
3501.452484	300958.188731	43.933108
3501.072662	300945.217322	43.938113
3501.233254	300916.839834	43.943117
3501.053885	300921.958293	43.948122
3501.272373	300899.374604	43.953127
3501.306195	300877.863275	43.958132
3501.069831	300872.759280	43.963137
3501.060791	300849.498510	43.968141
3500.918467	300841.758338	43.973146
3501.307377	300829.099388	43.978151
3501.279303	300821.163193	43.983156
3501.084553	300794.062852	43.988161
3500.750051	300773.550759	43.993165
3501.053965	300777.804687	43.998170
3500.998027	300748.621073	44.003175
3500.925375	300744.993093	44.008180
3501.080765	300741.889389	44.013185
3501.419161	300720.915758	44.018189
3501.238069	300702.364850	44.023194
3501.144977	300689.755772	44.028199
3501.494013	300664.122876	44.033204
3501.223052	300658.235281	44.038209
3501.291278	300649.265955	44.043213
3501.052943	300627.109890	44.048218
3501.382800	300606.595673	44.053223
3501.227864	300590.840280	44.058228
3501.150842	300571.458616	44.063233
3501.349785	300559.974610	44.068237
3501.223278	300548.592386	44.073242
3501.132815	300520.228488	44.078247
3501.198327	300511.437723	44.083252
3500.988725	300504.420659	44.088257
3501.210794	300475.549753	44.093261
3501.268248	300477.627969	44.098266
3501.035492	300452.187735	44.103271
3501.449205	300430.158711	44.108276
3501.347998	300425.033543	44.113281
3501.243531	300390.563436	44.118285
3501.231126	300387.155076	44.123290
3501.162794	300371.386079	44.128295
3501.533660	300357.202756	44.133300
3501.324752	300347.920387	44.138305
3501.112178	300326.727326	44.143309
3501.108677	300314.256862	44.148314
3501.147875	300299.489090	44.153319
3501.416933	300278.984255	44.158324
3501.384491	300257.915713	44.163329
3501.642851	300243.062760	44.168333
3501.232113	300220.195389	44.173338
3501.364116	300207.881876	44.178343
3501.554423	300190.927075	44.183348
3501.561350	300175.095353	44.188353
3501.185566	300152.298843	44.193357
3501.607065	300140.067313	44.198362
3501.045835	300114.652823	44.203367
3501.492556	300099.210449	44.208372
3501.161621	300086.434802	44.213377
3501.541950	300059.447798	44.218381
3501.123783	300049.689063	44.223386
3501.181160	300035.300150	44.228391
3501.236390	300016.457546	44.233396
3500.791850	300001.714418	44.238401
3501.238343	299989.351688	44.243405
3501.249481	299969.472446	44.248410
3501.486617	299957.702375	44.253415
3501.042192	299942.730149	44.258420
3501.059424	299917.657808	44.263425
3501.448301	299898.941162	44.268429
3501.153500	299892.624532	44.273434
3501.338332	299874.372456	44.278439
3501.337403	299859.381773	44.283444
3500.953835	299843.407391	44.288449
3501.120458	299826.583438	44.293453
3500.853443	299819.804326	44.298458
3500.727672	299801.702591	44.303463
3500.932480	299792.482706	44.308468
3500.968373	299778.198891	44.313473
3501.129624	299776.494058	44.318477
3500.880504	299769.788497	44.323482
3500.985419	299751.294356	44.328487
3501.042252	299736.243707	44.333492
3501.009565	299734.034706	44.338497
3501.224938	299713.308987	44.343501
3501.022938	299698.960537	44.348506
3501.195497	299680.761218	44.353511
3501.285636	299672.577309	44.358516
3500.825241	299651.931763	44.363521
3501.226407	299627.002879	44.368525
3501.438364	299628.853358	44.373530
3501.013080	299608.838601	44.378535
3501.244817	299602.617781	44.383540
3501.259929	299589.660658	44.388545
3501.033718	299572.999849	44.393549
3501.085832	299563.014792	44.398554
3501.108276	299557.259368	44.403559
3501.045839	299532.326565	44.408564
3500.678411	299519.938267	44.413569
3500.786201	299509.689979	44.418573
3500.774461	299503.201791	44.423578
3500.972689	299490.521438	44.428583
3500.903871	299467.854814	44.433588
3500.948282	299468.026221	44.438593
3500.797535	299456.138521	44.443597
3500.998527	299450.177009	44.448602
3501.194476	299429.810545	44.453607
3500.940057	299416.208319	44.458612
3500.868187	299414.514469	44.463617
3500.845317	299393.545905	44.468621
3500.591228	299376.660328	44.473626
3500.929118	299364.568956	44.478631
3501.226235	299365.795286	44.483636
3500.938239	299354.616222	44.488641
3501.001977	299329.256371	44.493645
3501.194978	299325.281341	44.498650
3501.134924	299310.452464	44.503655
3501.222595	299293.208008	44.508660
3501.087479	299278.925348	44.513665
3501.502742	299267.789030	44.518669
3501.135912	299254.204339	44.523674
3501.169464	299237.604625	44.528679
3501.335780	299225.769114	44.533684
3500.982398	299210.655193	44.538689
3501.164066	299192.607000	44.543693
3501.230467	299186.411982	44.548698
3501.189981	299162.188234	44.553703
3501.156439	299146.820676	44.558708
3500.871056	299145.287458	44.563713
3501.269198	299103.662313	44.568717
3501.006763	299108.717572	44.573722
3501.019888	299097.109598	44.578727
3501.289393	299080.956536	44.583732
3501.209401	299073.639052	44.588737
3501.179011	299060.714371	44.593741
3501.209817	299038.235611	44.598746
3501.142375	299025.062193	44.603751
3501.313799	299010.884251	44.608756
3501.182872	298993.470260	44.613761
3501.067174	298975.341227	44.618765
3501.023234	298973.770256	44.623770
3501.140903	298949.012648	44.628775
3501.099708	298941.078231	44.633780
3501.158688	298930.481137	44.638785
3501.416271	298910.181201	44.643789
3500.781106	298907.557317	44.648794
3501.282272	298895.185795	44.653799
3501.286614	298872.278420	44.658804
3501.042468	298859.997960	44.663809
3501.055176	298847.473724	44.668813
3501.171603	298819.076599	44.673818
3501.259141	298808.220496	44.678823
3501.223313	298798.299954	44.683828
3500.893639	298790.003382	44.688833
3501.239535	298764.522802	44.693837
3501.030286	298755.927425	44.698842
3500.652186	298742.140751	44.703847
3500.745252	298721.102902	44.708852
3500.942125	298724.253831	44.713857
3501.226392	298718.813717	44.718861
3500.733157	298700.870878	44.723866
3500.776989	298689.079853	44.728871
3501.098235	298665.664709	44.733876
3501.058289	298660.478893	44.738881
3501.260650	298648.281293	44.743885
3500.816604	298634.301285	44.748890
3500.854191	298616.631761	44.753895
3500.882717	298619.707207	44.758900
3501.064801	298619.195335	44.763905
3501.454679	298593.224209	44.768909
3500.871524	298578.426012	44.773914
3500.668494	298573.138424	44.778919
3501.107484	298558.282229	44.783924
3501.206802	298529.989440	44.788929
3500.968288	298526.565410	44.793933
3501.216964	298519.705514	44.798938
3501.016730	298503.574818	44.803943
3501.601309	298483.579936	44.808948
3501.213472	298472.645373	44.813953
3501.276716	298446.521626	44.818957
3501.331723	298438.623002	44.823962
3501.062347	298413.823856	44.828967
3501.487887	298404.874658	44.833972
3501.113173	298384.317051	44.838977
3501.014182	298360.763859	44.843981
3501.256020	298359.708144	44.848986
3501.088893	298344.717582	44.853991
3501.405947	298319.190403	44.858996
3501.333554	298315.918554	44.864001
3501.134940	298301.798283	44.869005
3500.782144	298275.892213	44.874010
3501.084897	298263.220691	44.879015
3501.206970	298248.897555	44.884020
3501.396401	298238.941696	44.889025
3501.318656	298214.010692	44.894029
3501.320278	298214.036078	44.899034
3501.165180	298203.854100	44.904039
3501.502857	298190.438982	44.909044
3501.105332	298164.768925	44.914049
3501.280154	298146.416034	44.919053
3501.202911	298133.600271	44.924058
3501.039605	298106.595496	44.929063
3501.315784	298094.589853	44.934068
3501.026665	298094.406169	44.939073
3501.269718	298061.178347	44.944077
3501.166312	298056.078755	44.949082
3501.207543	298048.614921	44.954087
3500.907136	298030.768981	44.959092
3501.300014	298017.167024	44.964097
3501.243225	297999.308439	44.969101
3500.830586	297990.744741	44.974106
3501.045770	297968.643963	44.979111
3501.084842	297966.372769	44.984116
3500.923526	297962.503942	44.989121
3501.240268	297924.479446	44.994125
3500.935166	297925.647244	44.999130
3501.259666	297914.092154	45.004135
3501.367159	297896.564188	45.009140
3501.170506	297888.144875	45.014145
3501.145861	297867.226917	45.019149
3501.000106	297857.603372	45.024154
3500.862832	297838.891932	45.029159
3501.027904	297830.416058	45.034164
3500.815846	297816.068692	45.039169
3501.303023	297786.187735	45.044173
3500.949658	297785.912283	45.049178
3501.030777	297780.020239	45.054183
3501.246281	297769.525716	45.059188
3501.108112	297744.731213	45.064193
3500.992785	297738.106298	45.069197
3500.842150	297718.124276	45.074202
3501.290060	297699.423112	45.079207
3501.085406	297691.259547	45.084212
3501.180800	297679.562059	45.089217
3501.024946	297660.395317	45.094221
3500.676849	297653.959499	45.099226
3500.614938	297652.467659	45.104231
3501.451125	297645.337636	45.109236
3500.988139	297618.506741	45.114241
3501.215530	297600.858128	45.119245
3501.002335	297590.532405	45.124250
3500.860196	297576.301310	45.129255
3501.376169	297564.054444	45.134260
3500.868314	297563.981313	45.139265
3501.294809	297546.123386	45.144269
3501.089968	297519.964761	45.149274
3500.957760	297519.985617	45.154279
3501.069369	297495.101048	45.159284
3500.902754	297474.714195	45.164289
3500.744968	297462.038134	45.169293
3500.801979	297463.251140	45.174298
3501.140244	297456.529825	45.179303
3501.131248	297434.056642	45.184308
3501.014444	297430.384441	45.189313
3500.965652	297414.026132	45.194317
3500.759995	297393.874428	45.199322
3500.575060	297380.388105	45.204327
3501.082825	297380.181645	45.209332
3500.969517	297385.264649	45.214337
3500.564981	297366.620288	45.219341
3500.605105	297344.750257	45.224346
3500.749895	297341.851642	45.229351
3500.850365	297326.997141	45.234356
3500.870738	297330.633894	45.239361
3500.950850	297321.509453	45.244365
3500.937370	297309.752551	45.249370
3500.807389	297295.697655	45.254375
3500.776965	297290.713846	45.259380
3500.765856	297282.087264	45.264385
3500.675260	297281.108955	45.269389
3500.601916	297268.368744	45.274394
3500.707131	297245.775819	45.279399
3500.912366	297234.824652	45.284404
3500.499145	297239.674576	45.289409
3500.564624	297231.825051	45.294413
3501.011371	297233.817074	45.299418
3500.578039	297223.780229	45.304423
3500.616643	297201.452229	45.309428
3500.621404	297194.324871	45.314433
3500.718821	297185.579496	45.319437
3500.410863	297188.962155	45.324442
3500.484158	297187.347353	45.329447
3501.005762	297186.578765	45.334452
3500.366558	297185.915300	45.339457
3500.396497	297169.544612	45.344461
3500.643480	297159.070507	45.349466
3500.648450	297152.401263	45.354471
3500.843831	297136.666476	45.359476
3500.620676	297130.516499	45.364481
3500.988710	297126.361233	45.369485
3500.471457	297129.343917	45.374490
3500.704632	297132.489261	45.379495
3501.079828	297096.516752	45.384500
3500.771564	297090.889136	45.389505
3500.788410	297089.334062	45.394509
3500.671234	297088.156282	45.399514
3500.714587	297078.197603	45.404519
3501.127309	297059.018124	45.409524
3501.003271	297056.696035	45.414529
3501.067848	297039.276324	45.419533
3500.664515	297028.725695	45.424538
3500.131174	297008.777801	45.429543
3500.872614	296995.197463	45.434548
3500.380935	297000.390562	45.439553
3500.632711	296996.075291	45.444557
3500.639804	296989.532961	45.449562
3500.362415	296998.255972	45.454567
3500.677832	296989.120143	45.459572
3500.824092	296989.402900	45.464577
3500.749077	296972.132257	45.469581
3500.711736	296960.862619	45.474586
3500.784698	296954.666329	45.479591
3501.107827	296946.725577	45.484596
3500.723548	296946.174971	45.489601
3501.001361	296934.397904	45.494605
3500.754484	296916.212353	45.499610
3500.746135	296906.439898	45.504615
3500.876439	296894.024106	45.509620
3500.693408	296902.096055	45.514625
3500.824394	296877.819057	45.519629
3501.015221	296866.819165	45.524634
3501.118999	296849.724157	45.529639
3501.034477	296844.468784	45.534644
3500.928894	296831.478985	45.539649
3501.020066	296819.476543	45.544653
3501.048863	296813.261688	45.549658
3500.932214	296802.284402	45.554663
3500.709158	296771.444920	45.559668
3500.862863	296773.457321	45.564673
3500.828277	296757.554757	45.569677
3500.821658	296770.562489	45.574682
3500.905649	296765.051686	45.579687
3501.022312	296742.304053	45.584692
3500.714160	296738.203568	45.589697
3500.903515	296724.022245	45.594701
3500.836602	296722.912958	45.599706
3500.840825	296708.989653	45.604711
3501.234319	296690.653009	45.609716
3500.994477	296679.389521	45.614721
3501.296746	296667.684935	45.619725
3500.763213	296648.118740	45.624730
3501.184129	296643.166125	45.629735
3501.293467	296628.946383	45.634740
3501.118678	296617.036385	45.639745
3500.572961	296604.344422	45.644749
3500.850051	296592.261960	45.649754
3500.933163	296588.507543	45.654759
3501.162577	296566.811244	45.659764
3500.825038	296562.002652	45.664769
3501.081683	296554.072240	45.669773
3501.034817	296541.734977	45.674778
3500.865707	296533.336608	45.679783
3501.044197	296512.895455	45.684788
3500.875169	296505.209759	45.689793
3500.729379	296491.284400	45.694797
3501.057244	296459.875009	45.699802
3501.017642	296461.001328	45.704807
3501.273751	296451.518341	45.709812
3500.948114	296435.152126	45.714817
3500.987988	296414.656250	45.719821
3500.766025	296412.247631	45.724826
3500.887686	296388.251868	45.729831
3501.203199	296322.940632	45.734836
3500.765668	296220.712519	45.739841
3500.695213	296065.738396	45.744845
3500.767190	295871.696009	45.749850
3500.540193	295616.942091	45.754855
3500.599311	295318.285624	45.759860
3499.766219	294982.019079	45.764865
3499.470438	294573.555409	45.769869
3499.518059	294140.446456	45.774874
3498.997277	293651.041697	45.779879
3498.772357	293106.986472	45.784884
3497.929917	292527.029657	45.789889
3497.574416	291885.516982	45.794893
3496.683478	291198.770616	45.799898
3496.053259	290481.301699	45.804903
3495.611402	289705.500762	45.809908
3494.918730	288888.159265	45.814913
3494.372561	288021.856632	45.819917
3493.572275	287097.005450	45.824922
3492.436475	286130.341703	45.829927
3491.519046	285120.555213	45.834932
3490.622937	284059.401185	45.839937
3489.705931	282956.965748	45.844941
3489.027689	281800.349870	45.849946
3487.620786	280598.435141	45.854951
3486.574803	279359.552995	45.859956
3485.618330	278068.493761	45.864961
3484.493519	276728.427302	45.869965
3483.285237	275335.799311	45.874970
3481.824614	273908.253568	45.879975
3480.553537	272427.005261	45.884980
3479.025716	270913.536135	45.889985
3477.450231	269356.379817	45.894989
3476.157896	267755.967067	45.899994
3474.638024	266120.906904	45.904999
3473.328948	264429.867491	45.910004
3471.567283	262711.776926	45.915009
3469.732778	260940.906991	45.920013
3468.449962	259132.769206	45.925018
3466.539317	257296.537142	45.930023
3464.982329	255418.560524	45.935028
3463.013155	253507.999536	45.940033
3461.372749	251540.748898	45.945037
3459.204785	249546.942470	45.950042
3457.099197	247529.035716	45.955047
3455.319330	245458.770354	45.960052
3453.173532	243385.026245	45.965057
3450.765951	241250.816725	45.970061
3448.919176	239088.995575	45.975066
3446.647336	236901.221392	45.980071
3444.509540	234682.416903	45.985076
3442.011468	232428.790251	45.990081
3439.828195	230147.242169	45.995085
3437.536766	227834.657769	46.000090
3435.039680	225502.439783	46.005095
3432.846053	223122.113667	46.010100
3430.121769	220748.775304	46.015105
3427.437378	218321.136901	46.020109
3424.861778	215878.006169	46.025114
3422.301697	213415.326493	46.030119
3419.396913	210917.418718	46.035124
3416.391873	208402.484499	46.040129
3413.616369	205864.873705	46.045133
3410.733725	203304.771065	46.050138
3407.790081	200731.317065	46.055143
3405.005613	198137.758794	46.060148
3401.680319	195534.168285	46.065153
3398.406572	192901.969582	46.070157
3395.621042	190262.924331	46.075162
3392.119625	187607.396358	46.080167
3388.534481	184940.334459	46.085172
3385.152908	182266.664593	46.090177
3381.576528	179571.991491	46.095181
3378.423093	176878.580685	46.100186
3374.398206	174174.965353	46.105191
3371.131002	171464.753842	46.110196
3366.857659	168769.956907	46.115201
3363.408541	166039.438702	46.120205
3359.878713	163310.606411	46.125210
3355.360701	160598.142153	46.130215
3351.433005	157867.628633	46.135220
3347.074318	155164.782553	46.140225
3342.672442	152452.472589	46.145229
3338.259914	149743.400148	46.150234
3333.324977	147065.810208	46.155239
3329.058748	144394.156789	46.160244
3323.859364	141744.560587	46.165249
3318.797879	139066.802852	46.170253
3313.592863	136409.103580	46.175258
3308.135948	133828.333578	46.180263
3302.242556	131276.949619	46.185268
3296.267796	128772.550674	46.190273
3289.887401	126302.362012	46.195277
3283.110418	123891.168417	46.200282
3275.410134	121540.724026	46.205287
3267.881626	119255.339234	46.210292
3259.765029	117060.175582	46.215297
3250.764380	114945.488084	46.220301
3241.768842	112933.250412	46.225306
3232.261202	111018.570042	46.230311
3222.896188	109193.372085	46.235316
3213.536253	107476.824196	46.240321
3204.651411	105869.372030	46.245325
3195.868691	104354.508844	46.250330
3187.421272	102942.597190	46.255335
3178.587488	101621.344595	46.260340
3170.459732	100397.547944	46.265345
3162.447291	99260.714542	46.270349
3155.166779	98209.442842	46.275354
3147.830457	97245.004453	46.280359
3140.997203	96351.354914	46.285364
3133.999145	95534.616621	46.290369
3127.936395	94766.450616	46.295373
3122.191751	94060.763291	46.300378
3116.856927	93411.271336	46.305383
3111.211950	92812.378305	46.310388
3106.013633	92249.184676	46.315393
3101.336404	91727.255177	46.320397
3097.266884	91230.385956	46.325402
3092.377379	90765.088745	46.330407
3088.557176	90321.537010	46.335412
3084.100609	89897.569680	46.340417
3080.228456	89501.495280	46.345421
3076.634374	89099.245780	46.350426
3072.460854	88745.030339	46.355431
3069.248189	88386.590424	46.360436
3065.782601	88024.446340	46.365441
3062.211741	87673.122480	46.370445
3058.757953	87322.521381	46.375450
3055.385927	86985.658262	46.380455
3052.197096	86648.147831	46.385460
3049.024906	86315.847533	46.390465
3045.474771	85982.987603	46.395469
3042.420449	85643.778052	46.400474
3038.727183	85316.436348	46.405479
3035.886583	84976.667592	46.410484
3032.272502	84643.883822	46.415489
3029.329416	84305.091767	46.420493
3026.045740	83975.719426	46.425498
3022.336697	83638.630234	46.430503
3019.212706	83295.483015	46.435508
3015.854853	82955.120341	46.440513
3012.812561	82613.670742	46.445517
3009.164858	82278.264794	46.450522
3006.090352	81934.262440	46.455527
3002.314399	81590.373960	46.460532
2998.944469	81252.904329	46.465537
2995.071715	80911.821057	46.470541
2991.566641	80566.581689	46.475546
2988.254769	80240.712024	46.480551
2984.744934	79906.100260	46.485556
2981.280733	79575.422840	46.490561
2977.516486	79243.043481	46.495565
2974.394487	78898.145878	46.500570
2970.213485	78575.200485	46.505575
2967.018213	78227.033124	46.510580
2963.408006	77903.726898	46.515585
2959.920415	77572.569024	46.520589
2956.149992	77246.336346	46.525594
2952.174221	76912.265485	46.530599
2948.882745	76598.323015	46.535604
2945.473271	76282.370611	46.540609
2941.695945	75967.850987	46.545613
2938.091855	75640.163721	46.550618
2934.094066	75334.245521	46.555623
2930.860389	75020.401145	46.560628
2926.970310	74718.244803	46.565633
2923.414390	74410.718660	46.570637
2920.040968	74107.218468	46.575642
2916.444714	73808.213851	46.580647
2913.169273	73498.216130	46.585652
2908.830595	73204.413854	46.590657
2904.754730	72913.621337	46.595661
2901.014181	72635.147680	46.600666
2897.236192	72337.508607	46.605671
2894.214525	72062.077677	46.610676
2890.034593	71795.122474	46.615681
2887.083476	71520.930542	46.620685
2883.710884	71249.207228	46.625690
2880.065015	70973.948769	46.630695
2876.829131	70697.587895	46.635700
2872.398340	70418.610728	46.640705
2869.002124	70157.987083	46.645709
2865.832834	69886.538134	46.650714
2862.030222	69628.078340	46.655719
2858.142899	69357.832780	46.660724
2854.384985	69101.796300	46.665729
2851.079381	68854.947321	46.670733
2847.669002	68587.593470	46.675738
2844.214557	68334.380141	46.680743
2840.422384	68077.616433	46.685748
2836.639353	67816.651499	46.690753
2833.172080	67571.147772	46.695757
2829.921210	67318.363304	46.700762
2826.871003	67080.168899	46.705767
2823.113291	66821.355686	46.710772
2819.463635	66574.950572	46.715777
2815.999862	66318.654593	46.720781
2812.213683	66070.092140	46.725786
2808.781982	65819.623214	46.730791
2805.458647	65565.217110	46.735796
2801.754045	65326.462285	46.740801
2798.226320	65075.755488	46.745805
2795.087710	64829.636492	46.750810
2791.388457	64591.877943	46.755815
2788.067644	64332.977363	46.760820
2784.911399	64083.212488	46.765825
2780.984229	63831.882376	46.770829
2777.517936	63572.307879	46.775834
2774.030941	63335.949740	46.780839
2770.731275	63089.339857	46.785844
2766.942855	62840.784251	46.790849
2763.448269	62579.872646	46.795853
2759.813096	62339.682015	46.800858
2756.823668	62090.901046	46.805863
2753.362977	61838.350318	46.810868
2749.631608	61591.346838	46.815873
2746.058980	61345.926624	46.820877
2742.846414	61085.462624	46.825882
2739.264276	60849.707873	46.830887
2735.815569	60591.196246	46.835892
2732.423779	60337.469731	46.840897
2728.748355	60083.879048	46.845901
2725.003032	59833.417789	46.850906
2721.970489	59589.961354	46.855911
2718.324128	59337.858803	46.860916
2714.778413	59089.341165	46.865921
2711.114383	58837.106956	46.870925
2707.685895	58583.518634	46.875930
2704.137516	58328.492235	46.880935
2700.484362	58088.853706	46.885940
2696.882177	57829.297605	46.890945
2693.584914	57586.410297	46.895949
2690.265802	57344.639281	46.900954
2686.677550	57087.189285	46.905959
2683.047397	56842.229552	46.910964
2679.715684	56593.761211	46.915969
2675.956826	56342.500643	46.920973
2672.696393	56087.592533	46.925978
2669.097415	55840.874266	46.930983
2665.449239	55597.725702	46.935988
2662.062498	55342.280619	46.940993
2658.446455	55096.955888	46.945997
2654.930582	54849.143611	46.951002
2651.241452	54605.649959	46.956007
2648.179163	54359.377035	46.961012
2644.555127	54113.968563	46.966017
2640.973655	53867.172908	46.971021
2637.303621	53612.108016	46.976026
2633.149478	53373.439014	46.981031
2630.299892	53130.793592	46.986036
2627.120062	52887.682114	46.991041
2623.140014	52644.362091	46.996045
2620.010075	52394.003026	47.001050
2616.581629	52151.160124	47.006055
2613.176348	51896.066149	47.011060
2609.747479	51644.715142	47.016065
2606.068935	51401.671763	47.021069
2602.637024	51149.673181	47.026074
2599.087514	50908.314881	47.031079
2595.455055	50642.270437	47.036084
2592.141134	50400.201828	47.041089
2588.308160	50153.161277	47.046093
2585.155155	49897.738997	47.051098
2581.196811	49657.884957	47.056103
2577.715490	49405.392983	47.061108
2574.141044	49158.157751	47.066113
2571.041480	48909.474465	47.071117
2567.617258	48657.184772	47.076122
2563.927667	48417.694931	47.081127
2560.490523	48165.361946	47.086132
2556.966524	47913.597159	47.091137
2553.333129	47671.791257	47.096141
2549.997504	47421.366128	47.101146
2546.235745	47167.515673	47.106151
2543.087149	46920.225406	47.111156
2539.464627	46676.310026	47.116161
2535.976434	46431.995726	47.121165
2532.403607	46171.638676	47.126170
2529.113639	45923.721832	47.131175
2525.334394	45675.129539	47.136180
2521.750907	45412.956397	47.141185
2518.123915	45168.277974	47.146189
2514.992596	44919.497567	47.151194
2511.332537	44673.294979	47.156199
2507.615062	44425.410830	47.161204
2504.509278	44178.105970	47.166209
2500.717985	43923.167949	47.171213
2497.421508	43667.514946	47.176218
2494.036646	43419.881669	47.181223
2490.486855	43174.084260	47.186228
2486.825476	42923.551019	47.191233
2483.293907	42678.111379	47.196237
2480.171430	42424.018133	47.201242
2476.225271	42179.441540	47.206247
2472.360632	41920.796771	47.211252
2469.259697	41684.000767	47.216257
2465.765126	41433.914904	47.221261
2462.534563	41175.477738	47.226266
2458.822903	40940.338800	47.231271
2455.422852	40685.186751	47.236276
2452.077942	40428.640455	47.241281
2448.260713	40167.447344	47.246285
2444.768472	39922.983442	47.251290
2441.222536	39684.218036	47.256295
2437.744810	39431.844546	47.261300
2434.224331	39173.730053	47.266305
2430.381305	38929.985249	47.271309
2426.918544	38681.111605	47.276314
2423.552420	38440.074691	47.281319
2419.686535	38200.678284	47.286324
2416.580291	37954.331276	47.291329
2412.640591	37704.472063	47.296333
2409.342032	37470.586761	47.301338
2405.687058	37218.812083	47.306343
2402.302733	36985.287830	47.311348
2399.076577	36728.728805	47.316353
2395.491551	36486.188520	47.321357
2391.986519	36229.070527	47.326362
2388.400332	35991.708995	47.331367
2385.075073	35743.272639	47.336372
2381.616625	35493.382989	47.341377
2377.959295	35246.430703	47.346381
2374.846447	34994.546751	47.351386
2371.046471	34750.411733	47.356391
2367.692240	34508.288954	47.361396
2364.606441	34245.240566	47.366401
2360.784485	34004.559577	47.371405
2357.486465	33742.552176	47.376410
2353.800227	33495.124122	47.381415
2350.303714	33240.652570	47.386420
2346.669307	32995.935169	47.391425
2343.168677	32741.242134	47.396429
2340.017386	32488.151837	47.401434
2336.146650	32242.440738	47.406439
2332.618978	31991.747795	47.411444
2329.628774	31729.907540	47.416449
2325.685517	31480.908298	47.421453
2322.464137	31218.945848	47.426458
2319.036392	30976.723264	47.431463
2315.314530	30715.821484	47.436468
2312.452887	30453.913815	47.441473
2308.437936	30199.383046	47.446477
2305.165946	29947.876248	47.451482
2301.501266	29688.771997	47.456487
2298.075715	29419.379764	47.461492
2294.743906	29151.319892	47.466497
2291.048312	28894.416835	47.471501
2287.488236	28644.865848	47.476506
2284.021061	28383.541840	47.481511
2280.484204	28119.969781	47.486516
2277.338043	27853.336323	47.491521
2273.737994	27589.432467	47.496525
2270.222975	27329.491836	47.501530
2266.872106	27077.855164	47.506535
2262.932723	26811.340430	47.511540
2259.876179	26542.511335	47.516545
2256.122688	26289.635776	47.521549
2252.719024	26020.595447	47.526554
2249.298095	25759.247220	47.531559
2245.853388	25488.192811	47.536564
2242.262280	25214.472133	47.541569
2239.036020	24948.389943	47.546573
2235.661642	24676.118955	47.551578
2232.006573	24414.191227	47.556583
2228.589782	24135.699790	47.561588
2225.235274	23869.240148	47.566593
2221.357604	23606.078021	47.571597
2217.901553	23322.149159	47.576602
2214.697744	23060.618373	47.581607
2211.014825	22789.080218	47.586612
2207.789329	22507.686342	47.591617
2204.382907	22236.220178	47.596621
2200.998627	21955.353109	47.601626
2197.320910	21691.291799	47.606631
2193.618492	21403.754641	47.611636
2190.534684	21127.229685	47.616641
2186.897627	20852.625879	47.621645
2183.389625	20564.266036	47.626650
2180.114556	20270.787396	47.631655
2176.187132	19998.477011	47.636660
2172.856163	19717.088727	47.641665
2169.346746	19444.213899	47.646669
2165.991547	19149.808107	47.651674
2162.423048	18864.111388	47.656679
2158.951084	18582.736153	47.661684
2155.752836	18294.570291	47.666689
2152.390400	18014.224882	47.671693
2149.017213	17731.161732	47.676698
2145.557317	17440.015664	47.681703
2142.079943	17140.497543	47.686708
2138.864474	16845.604431	47.691713
2134.888433	16552.212304	47.696717
2131.781009	16250.864112	47.701722
2128.314967	15967.391659	47.706727
2124.546331	15671.453605	47.711732
2121.091473	15365.860881	47.716737
2117.552555	15077.327673	47.721741
2114.486896	14775.527460	47.726746
2110.639410	14474.468596	47.731751
2106.991315	14172.686709	47.736756
2103.768765	13867.018260	47.741761
2100.091037	13571.757046	47.746765
2096.781681	13267.907003	47.751770
2092.887205	12972.891640	47.756775
2089.435682	12684.308177	47.761780
2086.227337	12372.513207	47.766785
2082.562099	12071.156819	47.771789
2079.117766	11769.416104	47.776794
2075.759006	11476.464556	47.781799
2071.927970	11176.126650	47.786804
2068.505332	10879.139090	47.791809
2064.175739	10586.825004	47.796813
2060.210320	10315.088664	47.801818
2055.887844	10044.504255	47.806823
2051.373279	9787.400884	47.811828
2047.356476	9538.152656	47.816833
2042.865752	9301.488500	47.821837
2039.216655	9064.961559	47.826842
2035.008698	8851.964446	47.831847
2031.354593	8633.549572	47.836852
2027.882860	8407.464608	47.841857
2023.609206	8209.083399	47.846861
2020.002143	8011.625543	47.851866
2016.203099	7823.093965	47.856871
2012.321104	7640.815783	47.861876
2008.917414	7452.969935	47.866881
2004.840044	7274.416467	47.871885
2001.679047	7089.454555	47.876890
1998.248758	6920.425011	47.881895
1994.513618	6743.820274	47.886900
1991.451619	6577.394849	47.891905
1987.614972	6407.810118	47.896909
1983.945069	6234.833416	47.901914
1980.793456	6066.477078	47.906919
1977.038397	5901.688545	47.911924
1973.721877	5723.869813	47.916929
1970.327567	5561.952181	47.921933
1966.887622	5388.096186	47.926938
1963.627673	5223.353402	47.931943
1960.294094	5057.512821	47.936948
1957.031113	4880.811070	47.941953
1953.150889	4724.125831	47.946957
1950.126903	4545.412043	47.951962
1946.763501	4369.332253	47.956967
1942.586493	4200.647279	47.961972
1939.711704	4024.219066	47.966977
1936.012050	3859.491001	47.971981
1932.762197	3687.687945	47.976986
1928.976903	3515.666521	47.981991
1925.346299	3353.849862	47.986996
1922.258140	3179.301790	47.992001
1918.219046	3007.470487	47.997005
1914.762327	2828.107243	48.002010
1911.330321	2661.060443	48.007015
1907.610850	2503.132077	48.012020
1904.119080	2333.468181	48.017025
1900.784895	2172.501736	48.022029
1897.420364	2010.709308	48.027034
1893.870852	1840.138339	48.032039
1890.131909	1680.992573	48.037044
1886.976911	1509.261909	48.042049
1883.134993	1349.758678	48.047053
1879.520523	1175.078295	48.052058
1876.147274	1019.266689	48.057063
1872.164616	870.879543	48.062068
1868.636209	712.775711	48.067073
1864.955292	561.284402	48.072077
1861.599380	406.421449	48.077082
1857.866535	265.315150	48.082087
1853.660497	130.076996	48.087092
1848.982153	25.450875	48.092097
1838.228349	71.496956	48.097101
1831.204096	79.338478	48.102106
1827.295583	71.132746	48.107111
1824.990666	78.302176	48.112116
1822.601981	77.796631	48.117121
1819.323800	79.872756	48.122125
1817.173026	81.291550	48.127130
1814.295626	79.296396	48.132135
1810.471846	87.469167	48.137140
1807.564789	80.334282	48.142145
1803.896137	79.098885	48.147149
1800.421186	75.346414	48.152154
1797.000101	78.919249	48.157159
1793.619753	81.375209	48.162164
1790.198782	79.734053	48.167169
1786.604520	80.821920	48.172173
1783.238024	83.225095	48.177178
1779.860498	80.036363	48.182183
1775.914447	84.583558	48.187188
1773.131288	81.276501	48.192193
1769.817959	86.196088	48.197197
1766.240335	89.388463	48.202202
1763.251535	86.034495	48.207207
1758.947438	90.827559	48.212212
1755.993178	82.782570	48.217217
1752.193522	83.377398	48.222221
1748.969584	80.594920	48.227226
1746.182968	75.795090	48.232231
1742.227333	88.171085	48.237236
1738.618448	75.881465	48.242241
1734.868554	82.508242	48.247245
1731.461607	88.081583	48.252250
1728.299527	81.454881	48.257255
1724.479521	89.041781	48.262260
1721.499272	82.326512	48.267265
1717.913764	82.517671	48.272269
1714.358001	89.246955	48.277274
1711.097475	76.225771	48.282279
1707.146617	90.315818	48.287284
1703.601345	85.523997	48.292289
1699.913580	93.988735	48.297293
1697.075409	86.052150	48.302298
1693.744509	84.241903	48.307303
1690.279472	86.340983	48.312308
1687.042224	81.693955	48.317313
1682.842577	87.445156	48.322317
1679.563744	83.823389	48.327322
1675.918314	92.113825	48.332327
1672.233251	87.024348	48.337332
1668.788364	80.299558	48.342337
1665.544498	76.536280	48.347341
1662.009548	81.091941	48.352346
1658.857467	84.265206	48.357351
1655.006898	88.699421	48.362356
1651.686504	90.595538	48.367361
1648.236224	82.318164	48.372365
1644.517972	92.546771	48.377370
1641.384143	88.772605	48.382375
1638.132834	90.759156	48.387380
1634.593508	79.834955	48.392385
1630.793444	81.224009	48.397389
1627.011148	81.018884	48.402394
1623.848456	81.308419	48.407399
1620.391688	78.239716	48.412404
1616.788708	77.762916	48.417409
1613.140422	77.438744	48.422413
1609.530626	85.204753	48.427418
1606.483817	82.204771	48.432423
1602.557542	76.994888	48.437428
1599.700773	75.044026	48.442433
1595.959184	81.634743	48.447437
1592.359640	75.544807	48.452442
1589.072826	74.199105	48.457447
1584.943330	85.203948	48.462452
1581.461859	84.704979	48.467457
1578.103345	81.500687	48.472461
1575.052709	83.155286	48.477466
1571.869342	79.974205	48.482471
1568.179281	85.879811	48.487476
1564.674768	78.284854	48.492481
1560.742129	82.580082	48.497485
1557.217507	83.818482	48.502490
1553.624381	77.471288	48.507495
1550.013286	90.283801	48.512500
1547.000863	75.676751	48.517505
1543.285853	83.816757	48.522509
1540.061221	77.468841	48.527514
1536.714820	79.508271	48.532519
1533.077584	84.959522	48.537524
1529.401016	79.954199	48.542529
1526.154971	80.462458	48.547533
1522.214621	82.544238	48.552538
1518.834964	74.546938	48.557543
1515.463973	87.448429	48.562548
1512.041659	79.211030	48.567553
1508.357971	83.543241	48.572557
1504.863295	77.310374	48.577562
1501.632838	77.718123	48.582567
1497.734313	84.124624	48.587572
1494.656186	81.563023	48.592577
1490.957138	84.299920	48.597581
1487.394269	77.723386	48.602586
1484.038640	86.019134	48.607591
1480.212964	89.006813	48.612596
1476.995554	88.757619	48.617601
1473.165482	89.097878	48.622605
1469.929087	91.952194	48.627610
1466.767347	79.855304	48.632615
1463.253423	82.310128	48.637620
1459.715323	87.328262	48.642625
1456.267456	82.628862	48.647629
1451.973353	83.285376	48.652634
1448.755682	88.750076	48.657639
1445.092066	97.578111	48.662644
1442.189699	90.597641	48.667649
1438.794931	83.767018	48.672653
1435.202204	84.535220	48.677658
1431.523244	87.281648	48.682663
1427.868996	90.093814	48.687668
1424.673813	85.089113	48.692673
1420.964202	89.748121	48.697677
1417.473053	81.948648	48.702682
1414.201430	76.427562	48.707687
1410.171627	87.524425	48.712692
1407.099692	79.456854	48.717697
1403.276183	87.819534	48.722701
1399.852128	81.502886	48.727706
1396.388993	72.493630	48.732711
1392.867559	88.411661	48.737716
1389.749058	73.539706	48.742721
1386.224704	76.470758	48.747725
1382.298161	76.927395	48.752730
1378.749763	68.886965	48.757735
1375.494562	76.746231	48.762740
1372.391605	71.129157	48.767745
1368.607484	80.327252	48.772749
1365.049522	79.321468	48.777754
1361.483089	76.763582	48.782759
1357.735120	87.639170	48.787764
1354.519025	77.237148	48.792769
1350.944794	76.347814	48.797773
1347.208785	77.961066	48.802778
1344.106241	80.142721	48.807783
1340.314942	85.235329	48.812788
1337.083276	74.047966	48.817793
1333.563293	75.624242	48.822797
1330.128311	87.801790	48.827802
1326.646584	69.797606	48.832807
1323.123854	75.053822	48.837812
1319.467543	77.094377	48.842817
1316.107860	76.326497	48.847821
1312.093953	84.912002	48.852826
1309.254350	74.216942	48.857831
1305.450346	69.190535	48.862836
1302.388995	77.202974	48.867841
1298.555183	78.379130	48.872845
1294.512015	80.379013	48.877850
1291.278360	81.505515	48.882855
1287.836322	84.075696	48.887860
1284.612545	73.437623	48.892865
1281.297406	82.059284	48.897869
1277.330870	83.771926	48.902874
1274.284726	79.930377	48.907879
1270.389920	79.939157	48.912884
1266.628496	77.266297	48.917889
1263.368166	74.189123	48.922893
1259.576940	77.288548	48.927898
1256.685818	76.301801	48.932903
1252.510114	81.932350	48.937908
1249.713664	75.672540	48.942913
1246.046926	80.789972	48.947917
1242.204887	84.039730	48.952922
1239.175342	81.768007	48.957927
1235.344983	81.377563	48.962932
1231.965498	81.808729	48.967937
1228.336975	79.469425	48.972941
1224.891470	89.310595	48.977946
1221.426633	80.393427	48.982951
1217.619037	84.441409	48.987956
1214.414073	70.351874	48.992961
1210.819162	77.530364	48.997965
1207.222394	85.949359	49.002970
1204.382869	76.646400	49.007975
1200.031545	84.807032	49.012980
1197.054770	73.374178	49.017985
1193.490637	77.551733	49.022989
1189.915567	80.367403	49.027994
1186.591246	77.474283	49.032999
1182.513368	78.821573	49.038004
1179.454466	77.307451	49.043009
1176.107372	80.071616	49.048013
1172.139182	79.563568	49.053018
1168.875695	85.744209	49.058023
1165.218587	80.489214	49.063028
1161.722036	81.625278	49.068033
1158.247975	82.874882	49.073037
1154.493822	80.504654	49.078042
1151.614235	78.813769	49.083047
1147.932844	89.432219	49.088052
1144.624609	75.596166	49.093057
1140.738665	72.654947	49.098061
1137.249769	81.787911	49.103066
1133.924100	72.893291	49.108071
1130.386675	69.479891	49.113076
1127.450855	69.797340	49.118081
1123.580561	80.299832	49.123085
1119.984266	80.397980	49.128090
1116.225352	87.200376	49.133095
1112.669086	86.618369	49.138100
1108.949228	76.532606	49.143105
1105.867795	77.274662	49.148109
1102.402074	84.024831	49.153114
1098.817933	69.194273	49.158119
1095.240354	78.543615	49.163124
1091.785657	79.163778	49.168129
1088.363822	78.158932	49.173133
1084.838925	75.449115	49.178138
1081.637141	66.440210	49.183143
1078.049775	73.041746	49.188148
1074.012039	80.055488	49.193153
1070.450288	75.459495	49.198157
1067.319666	73.703535	49.203162
1064.114288	78.040103	49.208167
1060.674529	81.375643	49.213172
1056.777222	77.496590	49.218177
1053.352692	76.982567	49.223181
1049.310811	79.846063	49.228186
1046.198712	73.233943	49.233191
1042.930578	80.551149	49.238196
1039.503892	84.805315	49.243201
1035.576071	77.488835	49.248205
1032.371042	78.648904	49.253210
1029.178090	73.909763	49.258215
1025.354488	81.551230	49.263220
1021.459784	77.251000	49.268225
1018.166932	74.280248	49.273229
1014.375641	77.344971	49.278234
1011.318592	71.882196	49.283239
1007.635285	81.352524	49.288244
1004.234522	71.226344	49.293249
1000.960567	68.606987	49.298253
997.103661	75.620916	49.303258
994.025590	67.339333	49.308263
989.985048	79.342851	49.313268
986.701135	66.841357	49.318273
983.313219	74.487385	49.323277
979.613516	73.671621	49.328282
976.559572	71.236126	49.333287
972.822114	77.905491	49.338292
969.026104	79.104329	49.343297
965.869048	71.062916	49.348301
962.116258	74.216543	49.353306
958.961668	71.391847	49.358311
955.154283	82.890630	49.363316
951.621472	76.344419	49.368321
948.596932	75.979779	49.373325
944.677889	81.342465	49.378330
941.187755	80.955816	49.383335
937.506107	82.256985	49.388340
934.269520	76.132641	49.393345
930.815042	80.815141	49.398349
927.151648	72.761275	49.403354
923.713155	79.839432	49.408359
919.900602	77.915050	49.413364
916.561277	81.279204	49.418369
913.110427	71.955020	49.423373
909.536939	82.116873	49.428378
906.054373	77.717359	49.433383
902.480733	84.107995	49.438388
899.071194	73.834537	49.443393
895.758380	79.703435	49.448397
892.230581	84.172801	49.453402
888.780814	61.405500	49.458407
885.376303	73.489792	49.463412
882.058230	78.223716	49.468417
878.102749	81.681200	49.473421
874.368037	75.191949	49.478426
871.000014	78.690327	49.483431
867.827066	76.934736	49.488436
864.080463	73.006861	49.493441
860.447030	65.704484	49.498445
856.936594	74.657398	49.503450
853.650653	76.931196	49.508455
849.786239	75.527499	49.513460
846.775869	76.581217	49.518465
843.396073	74.304361	49.523469
839.441350	81.618406	49.528474
836.022686	81.755286	49.533479
832.451471	82.700675	49.538484
829.204058	77.783473	49.543489
825.648872	71.952676	49.548493
822.065015	72.637455	49.553498
818.891925	70.518068	49.558503
814.884814	78.204160	49.563508
811.464769	81.919515	49.568513
807.766086	83.071538	49.573517
804.255779	83.203798	49.578522
801.579188	75.106194	49.583527
797.537534	75.277369	49.588532
793.868033	67.351076	49.593537
790.704597	67.514444	49.598541
786.860490	71.033617	49.603546
784.087787	73.445368	49.608551
780.134247	76.358414	49.613556
776.726775	69.900223	49.618561
773.098961	67.402804	49.623565
769.540135	79.859311	49.628570
766.149699	69.896140	49.633575
762.538862	73.097215	49.638580
758.952740	80.518084	49.643585
755.722243	69.131475	49.648589
751.509260	77.976139	49.653594
748.701891	72.123181	49.658599
745.012716	72.492283	49.663604
741.491304	70.224989	49.668609
737.940764	69.797256	49.673613
734.506472	76.090192	49.678618
731.156998	72.109676	49.683623
727.395932	68.437230	49.688628
723.991188	78.129779	49.693633
720.950050	64.144538	49.698637
717.024775	66.474208	49.703642
713.288684	70.334002	49.708647
709.633006	69.283659	49.713652
706.273527	69.730861	49.718657
703.270906	71.583849	49.723661
699.476253	79.584728	49.728666
696.232059	64.678997	49.733671
692.560162	69.063424	49.738676
688.900203	67.823934	49.743681
685.299350	80.103547	49.748685
681.860864	71.957625	49.753690
678.447980	66.655107	49.758695
675.211273	74.549632	49.763700
671.445215	67.391499	49.768705
668.438010	72.532390	49.773709
664.402703	80.368488	49.778714
660.508710	70.626596	49.783719
657.202159	77.276041	49.788724
653.514380	75.136078	49.793729
650.110823	72.837708	49.798733
646.634028	78.650105	49.803738
643.823465	72.149108	49.808743
640.426748	72.023192	49.813748
636.722194	69.964959	49.818753
633.213688	68.913745	49.823757
629.425649	74.486987	49.828762
625.914883	72.167451	49.833767
622.169813	61.519565	49.838772
618.716092	68.290145	49.843777
615.489532	69.001303	49.848781
611.697589	83.041458	49.853786
608.409159	66.677862	49.858791
604.666247	77.372542	49.863796
601.104291	77.797708	49.868801
598.035331	67.493198	49.873805
594.028666	80.348928	49.878810
590.802388	70.065894	49.883815
586.985639	78.573314	49.888820
583.853331	72.483402	49.893825
580.585973	74.390545	49.898829
577.007987	74.944783	49.903834
573.435057	64.219338	49.908839
569.699642	75.868317	49.913844
566.237939	71.494153	49.918849
562.669976	73.204772	49.923853
559.171576	74.765290	49.928858
555.783421	71.553375	49.933863
552.593539	70.759178	49.938868
549.346903	80.088490	49.943873
545.307503	69.353856	49.948877
541.621778	74.926925	49.953882
538.274645	73.040545	49.958887
534.836268	72.668091	49.963892
531.122125	75.527924	49.968897
528.068747	74.551002	49.973901
524.413115	74.022752	49.978906
521.048708	63.710768	49.983911
517.404669	70.428931	49.988916
513.672363	69.298921	49.993921
510.252468	62.975672	49.998925
506.315094	73.485702	50.003930
503.581457	65.311724	50.008935
499.802541	70.402689	50.013940
495.989047	64.612497	50.018945
492.618012	63.758109	50.023949
489.043766	65.972781	50.028954
485.761315	66.635790	50.033959
482.511742	66.306552	50.038964
478.847232	68.370849	50.043969
475.431906	67.447473	50.048973
471.545364	70.315349	50.053978
468.350806	67.734377	50.058983
465.252000	55.634415	50.063988
460.933565	67.153277	50.068993
457.674228	61.722399	50.073997
453.450838	66.642552	50.079002
450.741095	70.724503	50.084007
447.252366	70.166979	50.089012
443.658939	79.594932	50.094017
440.628638	68.284679	50.099021
436.507678	87.976316	50.104026
433.505870	76.778657	50.109031
429.767072	74.925194	50.114036
426.138392	76.620065	50.119041
422.608675	67.105980	50.124045
418.896552	76.077964	50.129050
415.431244	67.699082	50.134055
412.203506	76.807170	50.139060
408.586892	72.669310	50.144065
405.400487	61.807475	50.149069
401.893330	70.807468	50.154074
398.487513	64.241615	50.159079
394.537652	73.054691	50.164084
391.137063	77.393570	50.169089
387.597370	67.947503	50.174093
383.817262	81.052555	50.179098
380.322522	68.122455	50.184103
376.703157	73.216949	50.189108
373.566058	70.301143	50.194113
370.190295	68.776821	50.199117
366.757072	81.479526	50.204122
363.533450	68.835999	50.209127
359.798771	64.786260	50.214132
356.198820	74.006451	50.219137
352.537971	64.721751	50.224141
348.984781	74.152920	50.229146
345.773544	67.031422	50.234151
342.312995	73.192554	50.239156
338.457518	75.486139	50.244161
335.411304	71.176703	50.249165
331.326727	81.402971	50.254170
328.026446	74.191020	50.259175
324.721082	65.192337	50.264180
321.218420	69.733891	50.269185
317.710284	65.534788	50.274189
314.140271	77.540755	50.279194
310.682863	76.785388	50.284199
307.144001	81.864135	50.289204
303.677965	65.012822	50.294209
300.445325	59.944826	50.299213
296.307751	65.620400	50.304218
292.761952	60.535024	50.309223
289.548009	73.975356	50.314228
285.812720	68.733002	50.319233
282.557949	65.009919	50.324237
278.715629	72.135717	50.329242
275.366016	73.603432	50.334247
272.337039	65.586540	50.339252
268.220691	76.472707	50.344257
265.384457	65.106822	50.349261
261.169438	83.310447	50.354266
257.869593	76.243992	50.359271
254.531686	80.399092	50.364276
251.113376	74.543943	50.369281
247.830723	69.591368	50.374285
243.840934	69.033325	50.379290
240.568807	66.945486	50.384295
237.026928	71.493214	50.389300
233.235164	80.420791	50.394305
230.324258	70.009421	50.399309
226.411455	73.305458	50.404314
223.585820	68.189550	50.409319
219.336390	72.167916	50.414324
215.529483	75.463188	50.419329
212.603605	72.697852	50.424333
208.720740	82.240829	50.429338
205.579978	68.663737	50.434343
202.375687	70.760451	50.439348
198.272276	71.991941	50.444353
195.192473	64.663255	50.449357
191.233528	72.952643	50.454362
187.739154	75.053677	50.459367
184.376323	62.533290	50.464372
180.734146	69.102583	50.469377
176.917316	65.739681	50.474381
173.631361	77.147529	50.479386
170.521422	64.574873	50.484391
167.420518	60.713837	50.489396
163.807706	77.598764	50.494401
160.578048	65.497288	50.499405
156.556366	71.531256	50.504410
152.624984	74.855545	50.509415
149.152578	75.684480	50.514420
145.847976	71.510511	50.519425
142.653602	69.030876	50.524429
138.797051	70.834327	50.529434
135.435801	71.867317	50.534439
131.798296	66.578078	50.539444
128.259469	80.066191	50.544449
124.722226	71.578489	50.549453
121.646916	66.574502	50.554458
118.116224	64.153896	50.559463
114.455846	61.358139	50.564468
110.878359	63.291888	50.569473
107.502930	65.228784	50.574477
104.051141	71.141850	50.579482
100.082060	65.891920	50.584487
96.761406	60.606842	50.589492
93.005759	62.856414	50.594497
90.056332	60.025212	50.599501
86.543251	67.384237	50.604506
82.944410	64.635800	50.609511
78.989356	73.687089	50.614516
75.886173	69.709385	50.619521
72.213544	56.193551	50.624525
68.711994	66.929680	50.629530
65.470913	60.550140	50.634535
62.116170	59.218802	50.639540
58.550715	60.264832	50.644545
55.053880	59.901726	50.649549
51.296420	59.399121	50.654554
47.599716	56.235761	50.659559
44.045089	62.383258	50.664564
40.813824	75.456207	50.669569
37.550896	64.223713	50.674573
33.561081	58.806224	50.679578
30.437596	50.620749	50.684583
27.048440	61.029229	50.689588
23.306149	57.483879	50.694593
19.835498	46.419993	50.699597
15.862225	56.366335	50.704602
12.556110	60.516534	50.709607
9.517646	60.768166	50.714612
5.662129	53.849007	50.719617
2.669849	48.591618	50.724621