Thu Aug 25 09:34:56 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.732962	94.206802	0.000000
0.903017	99.599887	0.005005
0.693478	90.780675	0.010010
0.738292	81.336318	0.015014
0.279096	73.850213	0.020019
0.024900	63.902218	0.025024
0.210104	62.842002	0.030029
-0.254513	50.304223	0.035034
-0.470755	39.211342	0.040038
-0.832341	40.384992	0.045043
-1.126356	32.094739	0.050048
-1.166860	15.836391	0.055053
-1.953764	23.151096	0.060058
-2.210051	10.302293	0.065062
-2.698482	13.394071	0.070067
-2.474083	8.268617	0.075072
-3.453900	12.367530	0.080077
-4.322840	17.496275	0.085082
-3.704598	16.966161	0.090086
-3.840201	19.689446	0.095091
-3.875677	12.064212	0.100096
-4.307355	14.441579	0.105101
-5.022469	17.625823	0.110106
-5.237036	8.778966	0.115110
-5.630857	9.565360	0.120115
-5.530190	13.010926	0.125120
-5.695587	21.402004	0.130125
-5.465148	12.352543	0.135130
-5.502996	7.755397	0.140134
-6.366445	15.885686	0.145139
-6.730266	9.735589	0.150144
-6.699626	16.390685	0.155149
-7.128088	19.223131	0.160154
-7.523231	6.763084	0.165158
-8.140439	14.158764	0.170163
-8.613416	12.793551	0.175168
-8.621209	15.541102	0.180173
-9.265642	11.874229	0.185178
-8.652350	16.701131	0.190182
-8.745496	15.934466	0.195187
-8.619263	17.224672	0.200192
-8.715707	10.808055	0.205197
-9.437330	18.447888	0.210202
-10.014652	18.048151	0.215206
-10.199400	20.896195	0.220211
-10.441177	23.946164	0.225216
-11.053188	16.240419	0.230221
-11.495362	8.922518	0.235226
-11.323744	8.588933	0.240230
-11.784082	18.911821	0.245235
-11.694767	14.335878	0.250240
-11.700971	8.964982	0.255245
-11.691143	18.359988	0.260250
-12.083664	17.646558	0.265254
-12.970765	11.913808	0.270259
-12.924425	12.087071	0.275264
-13.068698	10.679848	0.280269
-13.462175	14.243966	0.285274
-13.618604	-2.375850	0.290278
-14.130579	5.756312	0.295283
-14.256890	9.670874	0.300288
-14.375001	-0.665400	0.305293
-14.446755	5.626084	0.310298
-15.022818	7.893197	0.315302
-15.630966	11.823145	0.320307
-16.051222	8.380576	0.325312
-15.715265	10.175759	0.330317
-15.964849	12.958031	0.335322
-15.869591	12.389637	0.340326
-16.145934	8.111434	0.345331
-16.548652	4.178900	0.350336
-16.908384	-2.591928	0.355341
-17.322945	7.068883	0.360346
-17.354149	1.217852	0.365350
-17.459645	6.685720	0.370355
-18.100872	8.906095	0.375360
-18.592488	6.847778	0.380365
-18.922176	16.254850	0.385370
-19.074970	21.587764	0.390374
-18.714860	18.889792	0.395379
-19.017916	9.832174	0.400384
-18.842970	9.273441	0.405389
-19.945412	16.909666	0.410394
-20.288727	15.125505	0.415398
-20.332271	20.422318	0.420403
-20.355289	11.086704	0.425408
-20.429105	23.010004	0.430413
-21.044822	23.207906	0.435418
-21.287360	17.712686	0.440422
-22.068387	28.686939	0.445427
-21.735308	21.826532	0.450432
-21.449574	11.917358	0.455437
-22.068835	21.787420	0.460442
-22.626604	13.933973	0.465446
-23.053243	23.071501	0.470451
-23.435821	24.855883	0.475456
-23.242806	21.877207	0.480461
-23.274396	28.184552	0.485466
-23.217176	22.057067	0.490470
-23.621499	23.297526	0.495475
-24.497417	19.578337	0.500480
-24.734086	21.254435	0.505485
-25.105005	19.920688	0.510490
-25.037292	17.078705	0.515494
-25.021688	24.372074	0.520499
-25.485507	24.751821	0.525504
-25.311408	22.010227	0.530509
-26.264790	24.589563	0.535514
-26.402126	20.068115	0.540518
-26.135172	19.137460	0.545523
-26.685168	18.100692	0.550528
-27.104022	23.070333	0.555533
-27.621660	23.910930	0.560538
-27.508510	19.122444	0.565542
-27.291847	22.970616	0.570547
-27.411123	25.934952	0.575552
-28.219051	20.949099	0.580557
-28.752582	23.940378	0.585562
-28.692718	22.403092	0.590566
-28.961186	24.751726	0.595571
-29.491887	24.879361	0.600576
-29.599676	24.848982	0.605581
-30.136006	23.778435	0.610586
-29.921503	18.838027	0.615590
-30.148109	21.237048	0.620595
-30.312865	23.661181	0.625600
-30.176493	19.682142	0.630605
-31.187967	21.429020	0.635610
-31.367896	15.538013	0.640614
-31.933338	15.778659	0.645619
-31.858863	24.970548	0.650624
-31.771512	14.209768	0.655629
-32.578561	17.383108	0.660634
-32.380021	6.130348	0.665638
-32.859206	12.574257	0.670643
-33.623178	9.720220	0.675648
-33.723661	14.630483	0.680653
-34.070778	12.764661	0.685658
-33.689709	11.695904	0.690662
-33.477898	12.561412	0.695667
-33.941793	13.561267	0.700672
-33.919976	12.722806	0.705677
-34.677877	18.786446	0.710682
-34.681523	20.331119	0.715686
-35.324889	13.196604	0.720691
-35.918406	18.275869	0.725696
-36.011079	14.655422	0.730701
-36.470952	18.793094	0.735706
-36.380854	14.349907	0.740710
-36.591854	13.690295	0.745715
-36.699824	20.259541	0.750720
-36.751841	14.370638	0.755725
-36.935065	14.649473	0.760730
-37.619054	17.037902	0.765734
-38.079836	14.408441	0.770739
-38.094183	9.861398	0.775744
-37.962323	10.600228	0.780749
-37.958657	3.320043	0.785754
-38.709051	5.355044	0.790758
-38.818322	7.653421	0.795763
-39.310377	8.081886	0.800768
-39.134658	10.237533	0.805773
-40.209996	12.864451	0.810778
-40.393322	2.829461	0.815782
-41.188911	11.936208	0.820787
-40.975461	20.460912	0.825792
-40.818638	18.522456	0.830797
-41.224053	26.100092	0.835802
-41.518354	20.654111	0.840806
-41.259181	16.772891	0.845811
-41.388409	16.676269	0.850816
-41.702212	18.446711	0.855821
-42.827761	20.790432	0.860826
-42.980937	17.258559	0.865830
-42.786564	18.829154	0.870835
-42.975310	20.928014	0.875840
-42.754077	19.251549	0.880845
-43.130133	21.386085	0.885850
-43.860572	13.834943	0.890854
-44.011676	21.195559	0.895859
-44.301088	18.222872	0.900864
-44.018520	7.279649	0.905869
-45.237512	15.260003	0.910874
-45.521564	5.652083	0.915878
-45.638249	15.269388	0.920883
-45.672819	21.314605	0.925888
-45.620244	16.519792	0.930893
-45.903532	17.197120	0.935898
-45.679847	16.624422	0.940902
-46.494517	9.595845	0.945907
-47.376392	16.707130	0.950912
-47.015239	12.677054	0.955917
-47.369975	15.358743	0.960922
-47.243570	17.544264	0.965926
-47.433955	18.849277	0.970931
-48.359890	20.231578	0.975936
-48.250010	12.295669	0.980941
-48.605201	32.428714	0.985946
-48.510120	18.866795	0.990950
-48.700755	12.512395	0.995955
-49.666855	19.279374	1.000960
-49.591565	17.806111	1.005965
-49.955172	15.686608	1.010970
-49.885906	18.529652	1.015974
-49.987858	20.165659	1.020979
-50.902457	22.954056	1.025984
-50.708797	20.994009	1.030989
-51.410317	20.310015	1.035994
-51.691429	19.873360	1.040998
-51.397080	18.852991	1.046003
-51.987271	24.036141	1.051008
-51.612384	13.353696	1.056013
-52.192098	15.839682	1.061018
-52.528667	10.343381	1.066022
-52.703688	11.212552	1.071027
-52.725377	20.922543	1.076032
-52.840631	22.747296	1.081037
-53.940747	15.804572	1.086042
-54.227560	14.321608	1.091046
-54.075681	20.530598	1.096051
-54.780948	13.405785	1.101056
-54.370635	8.535939	1.106061
-54.753793	13.749921	1.111066
-55.213932	12.923702	1.116070
-55.648390	11.853014	1.121075
-55.915141	20.291608	1.126080
-55.946461	12.108904	1.131085
-56.256577	25.021518	1.136090
-56.262426	21.308373	1.141094
-56.232118	13.793056	1.146099
-56.907203	12.896113	1.151104
-56.774181	10.426713	1.156109
-57.208900	17.616631	1.161114
-57.533107	12.539172	1.166118
-57.444092	27.638677	1.171123
-58.211186	12.538230	1.176128
-58.128494	9.140244	1.181133
-58.332028	24.738003	1.186138
-58.697226	18.961448	1.191142
-58.889792	18.207198	1.196147
-59.621574	14.965305	1.201152
-59.717667	12.193282	1.206157
-60.266411	17.648346	1.211162
-60.183923	28.186739	1.216166
-60.408935	22.100315	1.221171
-60.273065	24.667168	1.226176
-60.503977	22.435125	1.231181
-61.471342	20.248873	1.236186
-61.930554	21.681431	1.241190
-62.304378	15.131108	1.246195
-62.594020	19.115557	1.251200
-62.110124	9.649900	1.256205
-61.619321	20.519779	1.261210
-62.015848	19.642464	1.266214
-62.351463	12.915312	1.271219
-62.988499	19.077073	1.276224
-63.574606	20.456748	1.281229
-63.856873	30.527111	1.286234
-63.880838	19.448415	1.291238
-63.914595	22.586012	1.296243
-64.422988	22.741791	1.301248
-65.014069	23.340797	1.306253
-65.244896	30.827803	1.311258
-64.963214	20.954062	1.316262
-65.167994	19.942299	1.321267
-65.427947	17.819211	1.326272
-64.965690	9.739505	1.331277
-65.848236	17.284330	1.336282
-66.244840	15.290222	1.341286
-66.642894	5.459722	1.346291
-67.440043	23.912450	1.351296
-67.585237	7.676851	1.356301
-67.609395	16.314712	1.361306
-67.435274	3.360518	1.366310
-67.809466	14.963878	1.371315
-68.203868	12.437915	1.376320
-68.059881	9.713696	1.381325
-68.704344	17.021900	1.386330
-69.269717	10.900226	1.391334
-69.475298	17.728373	1.396339
-69.678817	21.291203	1.401344
-69.848819	8.289687	1.406349
-69.728091	13.639850	1.411354
-69.756463	21.256481	1.416358
-69.688200	17.284951	1.421363
-70.602538	15.226435	1.426368
-70.414758	17.256805	1.431373
-70.758029	13.201064	1.436378
-71.119813	13.099753	1.441382
-71.721567	17.044521	1.446387
-72.100334	17.626079	1.451392
-72.117126	13.250262	1.456397
-72.246728	15.662557	1.461402
-72.247822	8.882992	1.466406
-72.926423	9.116061	1.471411
-73.770364	20.701281	1.476416
-73.523365	6.292994	1.481421
-73.829709	19.233484	1.486426
-73.845803	10.026505	1.491430
-73.285568	12.327545	1.496435
-74.272806	13.937752	1.501440
-74.508217	5.489639	1.506445
-74.802923	14.913373	1.511450
-75.150101	11.383428	1.516454
-75.185548	16.830829	1.521459
-75.796629	24.209735	1.526464
-76.158768	10.877656	1.531469
-76.579459	18.445026	1.536474
-76.766483	19.528051	1.541478
-76.025491	11.195861	1.546483
-76.503126	21.410727	1.551488
-76.759815	13.434181	1.556493
-77.562062	18.970096	1.561498
-77.680183	11.955766	1.566502
-77.981140	14.350619	1.571507
-78.152767	19.430217	1.576512
-78.016450	10.771996	1.581517
-78.635131	20.053507	1.586522
-79.074056	22.008071	1.591526
-79.357458	12.273499	1.596531
-79.548645	19.969424	1.601536
-79.285517	21.823473	1.606541
-79.577411	27.355353	1.611546
-80.191218	20.026384	1.616550
-80.777118	12.721519	1.621555
-81.048043	19.699111	1.626560
-80.896329	12.667811	1.631565
-81.130836	20.250301	1.636570
-81.430141	16.988100	1.641574
-81.371525	15.125144	1.646579
-82.026647	17.211660	1.651584
-82.126981	15.215422	1.656589
-82.470167	10.814820	1.661594
-82.729869	12.314192	1.666598
-82.809793	12.662263	1.671603
-83.203853	13.594231	1.676608
-83.632506	4.474045	1.681613
-84.153557	13.730765	1.686618
-84.334014	12.645588	1.691622
-83.817377	8.239973	1.696627
-83.985820	19.203655	1.701632
-84.212627	8.602840	1.706637
-84.881913	18.635762	1.711642
-85.369810	16.991318	1.716646
-85.366975	20.607235	1.721651
-85.558539	18.546199	1.726656
-85.682063	18.268350	1.731661
-86.464208	8.798592	1.736666
-86.666956	11.285623	1.741670
-87.157486	12.985680	1.746675
-87.374923	21.445019	1.751680
-86.927079	19.970327	1.756685
-87.452153	15.816523	1.761690
-87.275448	18.275736	1.766694
-87.237606	10.714949	1.771699
-88.303247	14.447667	1.776704
-88.711808	13.053384	1.781709
-89.022006	15.924247	1.786714
-88.837812	11.134125	1.791718
-88.488679	12.525443	1.796723
-89.302931	18.762429	1.801728
-89.820216	6.989086	1.806733
-90.164187	14.493813	1.811738
-90.537584	18.149700	1.816742
-90.496672	14.324826	1.821747
-90.616852	14.451415	1.826752
-90.103382	13.770033	1.831757
-91.019899	16.476475	1.836762
-91.310232	8.185665	1.841766
-91.605439	12.863847	1.846771
-92.133684	11.855313	1.851776
-92.192908	7.315304	1.856781
-93.152244	16.229413	1.861786
-93.486353	16.474943	1.866790
-92.539014	13.188247	1.871795
-92.970717	11.285062	1.876800
-93.089088	18.102707	1.881805
-93.342714	18.215404	1.886810
-94.001138	17.967587	1.891814
-94.464636	13.952832	1.896819
-94.715780	17.909102	1.901824
-94.581443	15.980497	1.906829
-94.829012	19.227526	1.911834
-94.658073	18.818116	1.916838
-94.971279	9.043925	1.921843
-95.656943	20.772023	1.926848
-95.937023	18.829260	1.931853
-96.170936	18.173240	1.936858
-96.407490	27.739727	1.941862
-97.074486	26.835192	1.946867
-97.703286	23.621457	1.951872
-97.724941	21.676166	1.956877
-97.790393	14.349864	1.961882
-97.567340	13.204624	1.966886
-97.734421	13.306924	1.971891
-97.953374	18.166147	1.976896
-98.018375	19.600211	1.981901
-98.584276	21.362700	1.986906
-99.280886	16.786522	1.991910
-99.313146	20.591436	1.996915
-99.612479	17.925179	2.006912
-99.245317	17.909207	2.016909
-98.304209	18.310149	2.026906
-98.246126	21.345687	2.036902
-98.028983	17.364954	2.046899
-97.026469	25.254473	2.056896
-96.796260	29.115181	2.066893
-96.447402	23.792832	2.076890
-95.493928	15.613418	2.086886
-95.419221	15.931542	2.096883
-94.730859	15.529452	2.106880
-94.272026	17.954165	2.116877
-93.965004	12.245566	2.126874
-92.985257	8.522309	2.136870
-92.778256	11.506001	2.146867
-92.068486	19.260824	2.156864
-91.420444	11.800846	2.166861
-91.277036	15.763852	2.176858
-90.995004	15.970294	2.186854
-90.033888	17.714420	2.196851
-89.943912	16.740854	2.206848
-89.058336	17.780892	2.216845
-88.587184	16.877479	2.226842
-88.417722	17.760464	2.236838
-87.701452	14.914791	2.246835
-87.285194	15.011503	2.256832
-86.461298	18.383208	2.266829
-85.738981	15.926228	2.276826
-85.457090	17.935174	2.286822
-85.340564	24.069173	2.296819
-85.208613	16.123024	2.306816
-84.123254	13.910100	2.316813
-83.987721	14.928281	2.326810
-82.686588	14.008858	2.336806
-83.124356	11.081087	2.346803
-82.063597	19.604543	2.356800
-81.459946	9.823185	2.366797
-81.322198	18.456423	2.376794
-80.648154	14.964799	2.386790
-80.184567	16.976953	2.396787
-79.811341	18.021246	2.406784
-78.559742	14.949142	2.416781
-78.562750	15.681754	2.426778
-78.414968	12.206067	2.436774
-78.002989	10.364753	2.446771
-77.023353	14.329778	2.456768
-77.130537	17.207479	2.466765
-75.839894	22.089954	2.476762
-75.810195	13.529434	2.486758
-74.978299	18.198687	2.496755
-74.094731	16.723804	2.506752
-74.127842	14.873035	2.516749
-73.799979	13.561253	2.526746
-73.509047	13.002860	2.536742
-72.515378	20.127158	2.546739
-72.338883	22.881215	2.556736
-71.252317	17.965964	2.566733
-70.865573	19.103174	2.576730
-71.059748	16.406495	2.586726
-70.601787	18.964394	2.596723
-69.584681	28.055400	2.606720
-68.675687	21.146910	2.616717
-68.421572	18.332471	2.626714
-68.332251	19.332552	2.636710
-67.943905	18.134837	2.646707
-67.017382	10.374632	2.656704
-66.854339	19.615296	2.666701
-66.043613	24.984787	2.676698
-65.649975	13.642925	2.686694
-65.469394	22.861836	2.696691
-64.428353	20.263049	2.706688
-64.153976	17.790727	2.716685
-63.672853	18.998680	2.726682
-62.573486	21.262842	2.736678
-62.503782	19.139371	2.746675
-62.343714	18.854907	2.756672
-61.356948	25.920103	2.766669
-60.759275	15.319215	2.776666
-60.671316	5.501453	2.786662
-60.580773	11.161182	2.796659
-59.552123	17.697124	2.806656
-59.464393	11.135900	2.816653
-58.494206	13.109858	2.826650
-58.135837	17.929338	2.836646
-57.650172	11.587696	2.846643
-56.598279	12.956472	2.856640
-56.653570	24.708574	2.866637
-56.144707	8.321350	2.876634
-55.702120	14.169841	2.886630
-55.067767	14.539658	2.896627
-54.853243	7.933226	2.906624
-54.128946	12.071310	2.916621
-53.610852	13.362168	2.926618
-53.053166	13.104101	2.936614
-52.069380	19.770619	2.946611
-51.899174	11.701267	2.956608
-51.853250	11.339655	2.966605
-50.964724	15.423497	2.976602
-50.502935	18.589016	2.986598
-50.307330	14.991795	2.996595
-49.692265	24.510095	3.006592
-48.932983	14.412909	3.016589
-48.737696	13.391164	3.026586
-48.170736	10.312298	3.036582
-47.529640	12.512051	3.046579
-47.280279	15.172328	3.056576
-46.234209	13.459742	3.066573
-45.788932	11.176054	3.076570
-45.886375	15.183136	3.086566
-44.716635	17.331736	3.096563
-44.655809	11.471644	3.106560
-44.235487	14.158987	3.116557
-43.856388	17.571881	3.126554
-43.192060	12.906525	3.136550
-42.389580	9.800259	3.146547
-41.750341	16.612630	3.156544
-41.560740	16.652992	3.166541
-41.391663	14.944772	3.176538
-40.681563	7.142453	3.186534
-40.224805	8.807221	3.196531
-39.352865	12.187242	3.206528
-39.042601	15.433524	3.216525
-38.815749	9.151443	3.226522
-37.560562	11.251809	3.236518
-37.068383	18.220272	3.246515
-36.994489	18.272427	3.256512
-37.224347	15.901287	3.266509
-36.240099	9.760293	3.276506
-35.874203	15.522600	3.286502
-34.526484	10.455561	3.296499
-34.254163	12.608560	3.306496
-34.036461	14.744774	3.316493
-33.641856	16.004299	3.326490
-32.547617	14.664304	3.336486
-32.533032	11.177809	3.346483
-32.390252	15.837833	3.356480
-31.617073	15.501654	3.366477
-31.126822	16.033436	3.376474
-30.416087	15.637349	3.386470
-29.679414	16.494817	3.396467
-29.682468	15.165194	3.406464
-29.335096	15.415254	3.416461
-28.397578	7.748363	3.426458
-27.888639	13.288686	3.436454
-27.833110	10.074543	3.446451
-26.841582	11.617507	3.456448
-26.441933	10.345164	3.466445
-26.284014	10.114891	3.476442
-25.065318	10.079540	3.486438
-24.990443	16.996179	3.496435
-24.917979	12.388715	3.506432
-23.972446	15.402413	3.516429
-23.985063	14.701515	3.526426
-22.845285	15.090344	3.536422
-22.187454	19.473265	3.546419
-22.283324	13.213238	3.556416
-21.580516	19.917451	3.566413
-21.006819	13.628539	3.576410
-20.599660	6.608619	3.586406
-19.438408	13.342368	3.596403
-18.968412	18.093675	3.606400
-19.101718	22.176070	3.616397
-19.110265	13.764089	3.626394
-18.235735	8.495595	3.636390
-17.509758	19.003881	3.646387
-16.517811	21.104316	3.656384
-16.602127	20.981689	3.666381
-16.312856	16.169192	3.676378
-15.284463	20.025217	3.686374
-14.688241	19.482348	3.696371
-14.476268	11.181535	3.706368
-14.325064	20.097775	3.716365
-13.611214	15.960020	3.726362
-13.081227	8.733953	3.736358
-12.279936	14.915885	3.746355
-12.105821	10.495233	3.756352
-11.413206	10.770394	3.766349
-10.409798	17.110728	3.776346
-10.377800	11.065083	3.786342
-10.380620	12.276005	3.796339
-9.634259	13.911238	3.806336
-9.040726	13.619047	3.816333
-8.664382	14.289054	3.826330
-7.695009	12.151332	3.836326
-7.236199	12.013298	3.846323
-7.337940	18.339890	3.856320
-6.453612	14.872342	3.866317
-6.008882	16.228552	3.876314
-5.562068	14.923477	3.886310
-4.768744	16.237739	3.896307
-4.801624	13.040615	3.906304
-4.312372	26.456032	3.916301
-3.906387	38.414642	3.926298
-2.953312	49.131288	3.936294
-2.833462	50.437033	3.946291
-2.269065	62.424691	3.956288
-2.195494	83.799482	3.966285
-1.343890	93.125542	3.976282
-0.710949	98.602116	3.986278
-0.478918	115.390453	3.996275
0.000000	135.864499	4.001280
0.068511	127.147238	4.006285
0.227833	134.883210	4.011290
0.488550	143.489158	4.016294
0.735207	155.295896	4.021299
0.614806	148.876654	4.026304
0.668256	149.229140	4.031309
0.627199	155.772134	4.036314
0.300230	148.939165	4.041318
0.870961	150.431821	4.046323
0.511342	156.265422	4.051328
1.052421	149.391358	4.056333
1.083816	163.348399	4.061338
0.782114	152.597870	4.066342
0.853028	149.815476	4.071347
0.699253	157.511929	4.076352
1.136696	167.570849	4.081357
0.850144	165.404450	4.086362
0.869013	164.667685	4.091366
0.801275	172.369647	4.096371
1.071778	174.510465	4.101376
1.324912	178.520638	4.106381
1.226441	164.761137	4.111386
0.962568	157.627211	4.116390
0.992732	154.923967	4.121395
0.595685	155.695054	4.126400
0.922431	165.654256	4.131405
0.951440	168.054376	4.136410
0.809981	172.816078	4.141414
1.588088	171.609174	4.146419
1.273901	182.390152	4.151424
1.525382	172.090781	4.156429
0.982975	171.837431	4.161434
0.886555	173.311232	4.166438
1.130946	175.471960	4.171443
1.382616	174.891710	4.176448
0.845592	175.257618	4.181453
0.857940	183.051441	4.186458
1.391063	185.647827	4.191462
1.146156	171.946066	4.196467
1.400028	179.850743	4.201472
1.216502	168.417294	4.206477
1.256540	173.682075	4.211482
1.294106	174.435686	4.216486
1.429922	181.061710	4.221491
0.987517	177.806076	4.226496
1.096065	184.186434	4.231501
1.020167	181.354271	4.236506
1.080635	185.071927	4.241510
1.158913	187.113149	4.246515
1.201270	187.309184	4.251520
1.381335	194.162399	4.256525
1.266541	194.360910	4.261530
1.211912	183.577979	4.266534
1.509486	177.767125	4.271539
1.039735	182.798568	4.276544
1.590112	193.852220	4.281549
1.312367	194.696365	4.286554
1.601304	190.905357	4.291558
1.534855	187.005516	4.296563
1.509673	185.861196	4.301568
1.342291	176.298174	4.306573
1.707781	186.972662	4.311578
1.744276	187.720114	4.316582
1.725507	182.341642	4.321587
1.945828	188.603247	4.326592
1.871390	182.420404	4.331597
1.552955	186.874478	4.336602
1.538829	179.514748	4.341606
1.599620	175.066621	4.346611
1.837903	177.414970	4.351616
1.719895	179.097800	4.356621
1.770175	178.916103	4.361626
1.416010	185.008288	4.366630
1.891540	179.049327	4.371635
1.776748	175.375364	4.376640
1.487493	169.805156	4.381645
1.506925	180.619283	4.386650
1.374097	182.725219	4.391654
1.679267	185.354157	4.396659
1.592635	192.603503	4.401664
1.752517	182.464012	4.406669
1.842300	178.251790	4.411674
1.535736	180.017948	4.416678
1.669316	182.952184	4.421683
1.518508	184.282646	4.426688
1.480775	186.541363	4.431693
2.071600	198.768773	4.436698
2.147428	196.257688	4.441702
1.800227	191.000276	4.446707
1.752628	191.722939	4.451712
2.018028	188.818317	4.456717
1.865704	186.305015	4.461722
1.788835	184.339881	4.466726
2.035016	200.968336	4.471731
2.030752	197.302361	4.476736
1.599065	187.859839	4.481741
2.069172	206.497021	4.486746
2.173159	208.679752	4.491750
2.053160	195.869573	4.496755
1.674888	201.408714	4.501760
2.009762	194.472029	4.506765
2.254694	211.663844	4.511770
2.227232	195.099565	4.516774
1.913700	194.041553	4.521779
1.858796	194.550223	4.526784
2.040431	199.770680	4.531789
1.891776	204.742328	4.536794
2.280217	208.187136	4.541798
2.400961	209.724992	4.546803
1.911840	202.578883	4.551808
2.028171	194.252734	4.556813
2.360465	196.988157	4.561818
2.197655	193.533688	4.566822
2.352217	185.872276	4.571827
1.780573	190.378678	4.576832
2.183585	198.623832	4.581837
2.478122	208.556468	4.586842
1.756255	192.119976	4.591846
1.746350	204.460496	4.596851
1.859874	218.505952	4.601856
2.064364	211.959853	4.606861
2.405510	211.384565	4.611866
2.331309	204.942246	4.616870
2.239374	206.253994	4.621875
2.217671	220.064372	4.626880
2.405051	213.365927	4.631885
2.650962	216.570474	4.636890
2.260713	208.466061	4.641894
2.577340	208.590648	4.646899
2.105040	218.931344	4.651904
2.299020	205.046895	4.656909
2.314911	203.177958	4.661914
1.957814	209.976136	4.666918
2.341250	212.902868	4.671923
1.961282	212.380453	4.676928
1.913574	207.949318	4.681933
2.385851	220.312377	4.686938
2.570904	230.942395	4.691942
2.533473	232.811924	4.696947
2.640695	228.097078	4.701952
2.690256	224.198034	4.706957
2.467470	217.595491	4.711962
2.339885	213.297094	4.716966
2.658776	202.664437	4.721971
2.495279	220.992779	4.726976
2.909351	224.952436	4.731981
2.870432	215.188929	4.736986
2.682151	219.708041	4.741990
2.686538	204.755462	4.746995
2.499509	206.986953	4.752000
2.671874	209.693652	4.757005
2.547338	210.254362	4.762010
2.166256	219.906878	4.767014
2.348148	218.597232	4.772019
2.426554	226.399707	4.777024
2.755586	229.429879	4.782029
2.752419	230.873255	4.787034
2.580044	235.162084	4.792038
2.879383	230.334877	4.797043
2.774144	241.497609	4.802048
2.616020	228.671234	4.807053
2.933536	231.102090	4.812058
2.917559	230.668178	4.817062
2.582305	235.241960	4.822067
2.575744	231.870570	4.827072
2.879582	225.780305	4.832077
2.634403	234.316863	4.837082
2.874904	241.897792	4.842086
2.681922	235.841073	4.847091
2.981981	241.391005	4.852096
2.679618	234.104889	4.857101
2.985598	231.035712	4.862106
2.173722	231.770556	4.867110
2.149285	227.845140	4.872115
2.318438	245.140610	4.877120
3.158165	253.257252	4.882125
3.038932	255.240842	4.887130
2.728790	253.201518	4.892134
3.233932	255.267616	4.897139
3.283156	262.998748	4.902144
3.320962	249.524718	4.907149
3.073888	237.787965	4.912154
2.621613	232.996263	4.917158
2.920201	236.762043	4.922163
2.697475	256.463298	4.927168
3.261681	261.351744	4.932173
3.266158	261.686594	4.937178
3.069666	262.647727	4.942182
2.991884	253.269945	4.947187
2.895204	262.783010	4.952192
3.116844	243.851099	4.957197
3.305864	246.118589	4.962202
3.151881	259.383404	4.967206
3.166939	257.245669	4.972211
3.094801	264.723730	4.977216
3.220032	256.215821	4.982221
3.178744	258.924365	4.987226
3.097262	256.086737	4.992230
3.460577	248.129995	4.997235
2.958825	252.919696	5.002240
3.528072	256.105226	5.007245
3.246693	253.684903	5.012250
3.173276	253.193551	5.017254
3.572434	252.609172	5.022259
3.098146	268.638720	5.027264
3.180062	255.670310	5.032269
3.170252	252.783487	5.037274
3.108093	261.142683	5.042278
3.187670	252.208489	5.047283
2.925304	247.209855	5.052288
3.055670	256.146333	5.057293
3.799686	253.530546	5.062298
3.052292	267.084499	5.067302
3.208223	254.537934	5.072307
3.189126	263.564274	5.077312
3.473741	259.615739	5.082317
3.285582	270.335893	5.087322
3.028878	278.719252	5.092326
3.451263	276.150692	5.097331
3.482389	281.407410	5.102336
3.324663	281.748693	5.107341
3.625717	279.294057	5.112346
3.535008	291.903566	5.117350
3.411662	276.977268	5.122355
3.528357	287.260520	5.127360
4.090838	279.275722	5.132365
3.790242	278.335903	5.137370
3.437324	285.794690	5.142374
3.605144	277.827436	5.147379
3.739914	282.039679	5.152384
3.794947	288.678399	5.157389
4.096325	279.133626	5.162394
3.493108	277.386995	5.167398
3.564733	262.873092	5.172403
3.226616	266.510845	5.177408
3.617211	277.681334	5.182413
3.675349	279.399850	5.187418
4.034414	283.595934	5.192422
4.224569	281.661719	5.197427
3.640121	270.949092	5.202432
3.227776	265.138708	5.207437
3.595338	272.750363	5.212442
3.651673	289.889544	5.217446
3.851835	282.980259	5.222451
3.484172	284.265610	5.227456
3.631177	287.637529	5.232461
3.810999	287.464008	5.237466
3.753818	297.037343	5.242470
3.871865	282.917954	5.247475
3.465485	284.728235	5.252480
3.738342	277.010284	5.257485
3.808821	286.057402	5.262490
3.601838	286.301996	5.267494
3.972264	281.526914	5.272499
3.668317	282.992110	5.277504
3.744080	275.026626	5.282509
3.921834	291.877862	5.287514
3.978549	306.754878	5.292518
4.400582	300.383473	5.297523
3.946125	294.364539	5.302528
3.711915	289.124196	5.307533
3.934653	292.702552	5.312538
4.124686	303.474204	5.317542
4.176664	299.682335	5.322547
4.053148	292.399811	5.327552
3.970913	283.763041	5.332557
4.202432	292.338833	5.337562
4.045261	297.799068	5.342566
4.132287	289.221198	5.347571
3.888530	290.828827	5.352576
4.220845	309.424430	5.357581
4.113454	298.035917	5.362586
4.309333	305.063871	5.367590
4.153335	299.583476	5.372595
4.234869	300.054953	5.377600
4.164357	292.893839	5.382605
4.208860	295.028953	5.387610
4.053628	303.915289	5.392614
4.510801	307.181665	5.397619
4.579501	304.320499	5.402624
4.206145	282.185084	5.407629
4.202393	292.104391	5.412634
3.764761	285.519666	5.417638
4.421759	304.197271	5.422643
4.292454	315.797262	5.427648
4.245774	310.170020	5.432653
4.660395	308.096227	5.437658
4.363944	305.523230	5.442662
4.663332	304.685559	5.447667
4.296097	301.032140	5.452672
4.196851	287.101820	5.457677
4.321482	289.891941	5.462682
4.347641	301.002485	5.467686
4.438193	309.647830	5.472691
4.522737	317.205770	5.477696
4.352004	309.829394	5.482701
4.299599	316.940547	5.487706
4.629208	312.377500	5.492710
4.893428	309.691346	5.497715
4.130370	295.915647	5.502720
4.517797	301.610099	5.507725
4.642698	307.728507	5.512730
4.466472	300.596609	5.517734
4.535392	300.086118	5.522739
4.476607	298.902762	5.527744
4.729075	308.120697	5.532749
4.919797	304.408330	5.537754
4.466336	295.320345	5.542758
4.204952	287.281128	5.547763
4.180375	305.980103	5.552768
4.544481	311.266917	5.557773
4.765909	309.305653	5.562778
4.513653	321.893037	5.567782
4.494949	312.088344	5.572787
4.865678	311.220512	5.577792
4.680943	308.645830	5.582797
4.964572	310.537831	5.587802
4.618223	303.565467	5.592806
4.703393	310.946133	5.597811
4.786599	316.454134	5.602816
4.660323	311.253822	5.607821
4.602415	313.686562	5.612826
5.088575	318.922617	5.617830
4.750675	314.815337	5.622835
4.732260	321.190327	5.627840
4.431999	318.934307	5.632845
4.524513	312.699950	5.637850
4.762197	315.178127	5.642854
5.068117	311.159803	5.647859
4.769453	319.458004	5.652864
4.797272	311.993570	5.657869
4.910636	320.562578	5.662874
5.003746	320.655748	5.667878
4.971143	316.519617	5.672883
4.712216	315.810552	5.677888
4.742616	315.644624	5.682893
4.820357	316.828553	5.687898
4.720538	321.017448	5.692902
4.873900	312.106465	5.697907
5.075924	318.016636	5.702912
5.165853	326.405818	5.707917
5.767690	303.310811	5.712922
4.878141	318.007063	5.717926
5.065594	312.884147	5.722931
4.983866	317.627038	5.727936
5.243536	311.796769	5.732941
5.036963	315.300023	5.737946
4.812269	307.998544	5.742950
4.970167	306.986885	5.747955
4.783409	312.540346	5.752960
4.842366	311.762492	5.757965
5.463807	324.434453	5.762970
5.342893	324.836408	5.767974
5.211588	315.729575	5.772979
5.199428	317.541369	5.777984
4.773977	317.098845	5.782989
5.043867	323.482448	5.787994
5.137286	334.130049	5.792998
5.445237	334.860286	5.798003
5.008073	340.440335	5.803008
4.885682	337.352834	5.808013
5.524475	335.731142	5.813018
5.304830	340.242543	5.818022
5.528947	335.480878	5.823027
5.459296	334.546000	5.828032
5.362425	334.339900	5.833037
5.274999	328.136895	5.838042
5.025054	341.473754	5.843046
5.312990	339.264780	5.848051
5.174719	342.371353	5.853056
5.018450	343.016134	5.858061
5.183401	336.064889	5.863066
4.835071	351.530599	5.868070
5.032726	344.264172	5.873075
5.327042	341.756799	5.878080
5.490907	344.066209	5.883085
5.590389	340.225759	5.888090
5.109614	344.300339	5.893094
5.707330	355.011309	5.898099
5.517219	362.327558	5.903104
5.316524	359.445316	5.908109
5.484913	353.135780	5.913114
5.606100	364.104921	5.918118
5.595634	361.670609	5.923123
5.624067	369.522106	5.928128
5.625819	366.927689	5.933133
5.730038	356.619647	5.938138
5.442970	350.318198	5.943142
5.543047	353.665844	5.948147
5.768831	355.453016	5.953152
5.613433	358.869165	5.958157
5.674195	357.059622	5.963162
5.416982	359.580545	5.968166
5.996021	359.524811	5.973171
5.795688	353.769766	5.978176
5.530321	350.040264	5.983181
5.637610	352.712887	5.988186
5.891740	356.460348	5.993190
5.578483	350.972939	5.998195
5.554541	353.362397	6.003200
5.849477	357.780521	6.008205
6.132920	358.115958	6.013210
5.578118	358.997193	6.018214
5.556106	345.494497	6.023219
5.729065	358.189294	6.028224
5.729547	363.077506	6.033229
5.976171	365.079717	6.038234
5.522857	361.923837	6.043238
5.882077	359.801770	6.048243
5.599516	365.107661	6.053248
5.842567	364.158589	6.058253
5.854027	357.832510	6.063258
5.427536	358.393078	6.068262
5.673089	359.313430	6.073267
5.714354	362.983510	6.078272
5.601986	362.621647	6.083277
6.059552	362.531161	6.088282
5.377245	370.715486	6.093286
5.592115	358.453849	6.098291
5.728611	365.873953	6.103296
5.519801	373.851210	6.108301
6.229647	364.400584	6.113306
5.662696	369.168892	6.118310
6.028706	367.431746	6.123315
5.618969	371.219949	6.128320
5.629431	370.326302	6.133325
5.918289	360.046278	6.138330
5.633420	372.547057	6.143334
6.058448	366.637077	6.148339
6.040399	369.484368	6.153344
5.476702	353.782260	6.158349
5.982980	354.019506	6.163354
5.182040	351.762834	6.168358
5.522886	354.161577	6.173363
5.348307	365.003049	6.178368
5.764981	364.197620	6.183373
6.044763	369.491335	6.188378
5.735735	375.525892	6.193382
5.743907	369.545180	6.198387
5.675948	371.242333	6.203392
5.477920	371.833546	6.208397
5.997061	366.323280	6.213402
5.586114	367.805248	6.218406
5.702357	369.112865	6.223411
6.084415	364.067013	6.228416
5.707953	370.697440	6.233421
6.184716	361.862313	6.238426
5.903469	368.408217	6.243430
5.618836	366.257312	6.248435
5.838242	363.616137	6.253440
5.717926	361.961518	6.258445
5.807161	346.818352	6.263450
5.573418	353.745956	6.268454
6.022135	353.951092	6.273459
5.796546	352.518615	6.278464
5.291236	352.382838	6.283469
5.900733	351.347876	6.288474
5.740895	370.517374	6.293478
5.850187	360.376218	6.298483
5.689724	362.964241	6.303488
5.692457	355.187338	6.308493
5.976130	361.505518	6.313498
5.459045	352.908373	6.318502
5.833886	357.139968	6.323507
5.848323	355.600279	6.328512
5.666215	352.711962	6.333517
6.089343	348.880913	6.338522
5.648127	350.532141	6.343526
5.773449	343.780094	6.348531
5.754172	334.905640	6.353536
5.575168	343.210414	6.358541
5.981861	338.306246	6.363546
5.688266	349.783301	6.368550
5.743041	336.531177	6.373555
5.575764	345.656707	6.378560
5.751621	340.956387	6.383565
6.249540	337.072493	6.388570
5.341767	345.890094	6.393574
5.423105	342.672594	6.398579
5.939050	353.222366	6.403584
5.719893	352.459611	6.408589
5.655118	337.046348	6.413594
5.407436	346.715998	6.418598
6.015531	353.211139	6.423603
5.551842	349.968300	6.428608
5.858910	359.123921	6.433613
5.747521	349.498248	6.438618
5.599321	350.549898	6.443622
5.842385	359.886394	6.448627
5.811372	350.206997	6.453632
5.618653	354.144696	6.458637
5.883894	341.900488	6.463642
5.676340	351.877070	6.468646
5.699030	341.350853	6.473651
5.913964	339.273541	6.478656
5.705807	336.920829	6.483661
5.905636	334.333347	6.488666
5.742729	346.106304	6.493670
5.326379	337.126381	6.498675
5.489115	345.991392	6.503680
5.361827	357.638552	6.508685
6.072698	358.596731	6.513690
5.992046	366.126789	6.518694
6.037815	359.285959	6.523699
5.805300	350.865695	6.528704
5.675837	345.808244	6.533709
5.573580	338.114238	6.538714
5.840212	358.321074	6.543718
5.494941	357.353447	6.548723
6.012854	359.240384	6.553728
5.620780	355.416835	6.558733
5.864455	347.633822	6.563738
5.597429	355.386070	6.568742
5.880602	359.698468	6.573747
6.056244	353.707342	6.578752
5.464237	340.486950	6.583757
6.085014	335.153762	6.588762
5.568291	342.805920	6.593766
5.570846	347.627364	6.598771
5.656399	341.352958	6.603776
5.545649	345.274647	6.608781
5.991370	351.899635	6.613786
5.713662	346.428804	6.618790
5.505452	340.099184	6.623795
5.866085	354.055409	6.628800
6.014540	360.546638	6.633805
6.086562	335.573034	6.638810
5.798596	343.527879	6.643814
5.724167	342.694991	6.648819
5.795735	342.260015	6.653824
5.254870	334.175979	6.658829
5.516188	338.798687	6.663834
5.474818	349.404139	6.668838
5.953167	354.151036	6.673843
5.809765	365.585586	6.678848
6.251287	362.564754	6.683853
5.901730	348.255981	6.688858
5.698929	347.867158	6.693862
5.754818	349.573379	6.698867
6.175257	348.757868	6.703872
5.954097	347.919496	6.708877
5.660337	341.036956	6.713882
5.470209	348.388003	6.718886
5.473575	339.772596	6.723891
5.825602	346.019949	6.728896
6.047905	350.474762	6.733901
6.510828	343.752079	6.738906
5.680885	348.368595	6.743910
5.617942	347.552890	6.748915
5.701300	348.460689	6.753920
5.937474	349.233811	6.758925
6.122174	336.084720	6.763930
5.899347	346.098494	6.768934
6.000809	345.386746	6.773939
6.058862	346.633875	6.778944
5.707397	340.222293	6.783949
5.774373	327.060016	6.788954
5.672174	331.065785	6.793958
5.525651	322.530820	6.798963
5.948912	335.407849	6.803968
5.277925	330.191636	6.808973
5.572561	328.763075	6.813978
5.811297	340.953998	6.818982
5.549405	342.520180	6.823987
5.788817	341.758344	6.828992
5.988048	353.471402	6.833997
6.169245	344.964173	6.839002
5.859544	334.300211	6.844006
5.669313	321.662300	6.849011
5.312938	323.354017	6.854016
5.652195	340.531178	6.859021
5.785048	342.348728	6.864026
5.827983	354.064128	6.869030
5.644817	349.638362	6.874035
5.659608	346.962809	6.879040
5.340583	350.221093	6.884045
5.403892	347.398730	6.889050
5.397873	356.910296	6.894054
5.651705	353.732207	6.899059
5.573933	357.009641	6.904064
5.969849	359.263712	6.909069
5.641710	347.235862	6.914074
5.814951	358.937176	6.919078
5.854186	354.207638	6.924083
5.890585	346.555180	6.929088
5.482587	353.956185	6.934093
5.808949	341.711893	6.939098
5.578880	346.876674	6.944102
5.824315	351.470235	6.949107
5.866367	346.262522	6.954112
5.742398	345.899313	6.959117
5.927367	351.331267	6.964122
5.435761	350.857978	6.969126
5.685247	352.075112	6.974131
6.010594	350.670212	6.979136
5.421076	349.443456	6.984141
5.535517	344.256039	6.989146
5.699709	352.358346	6.994150
5.542806	356.205010	6.999155
5.887292	358.843634	7.004160
5.684900	351.190622	7.009165
5.447531	351.835455	7.014170
5.643170	353.760230	7.019174
5.564642	342.648745	7.024179
6.087787	343.095325	7.029184
5.942187	344.959667	7.034189
5.775344	343.979904	7.039194
5.665316	350.109825	7.044198
5.817908	359.283322	7.049203
6.021360	347.513873	7.054208
5.840699	345.169507	7.059213
6.132511	345.307476	7.064218
6.092014	347.291395	7.069222
5.816828	346.442504	7.074227
5.716954	339.997831	7.079232
5.593994	346.427175	7.084237
5.437543	353.238264	7.089242
5.849650	357.913281	7.094246
5.402810	347.827630	7.099251
5.812002	351.028765	7.104256
5.639571	356.070620	7.109261
5.827197	346.306348	7.114266
5.651835	348.399985	7.119270
5.770482	351.988335	7.124275
5.856167	346.308704	7.129280
5.766767	355.652996	7.134285
6.066161	348.361135	7.139290
6.124157	354.018633	7.144294
6.104569	351.136490	7.149299
6.073221	345.351807	7.154304
5.949566	345.864926	7.159309
5.547268	326.182785	7.164314
5.205850	329.112374	7.169318
5.574602	345.734414	7.174323
5.580081	349.865689	7.179328
5.582945	359.657443	7.184333
5.628580	348.355655	7.189338
5.912986	355.141963	7.194342
5.672226	348.390325	7.199347
5.841012	348.591863	7.204352
5.682923	358.677760	7.209357
5.932787	350.976034	7.214362
5.681899	352.879021	7.219366
5.661335	351.949106	7.224371
5.884014	344.264298	7.229376
5.700939	359.207404	7.234381
5.682642	347.083549	7.239386
5.795296	361.799984	7.244390
5.660201	356.189744	7.249395
6.081630	356.402319	7.254400
5.861720	368.317103	7.259405
5.899065	357.054574	7.264410
5.810414	355.879058	7.269414
5.650582	354.841247	7.274419
5.859806	352.369352	7.279424
5.444830	342.360970	7.284429
6.012047	349.618667	7.289434
5.853237	358.568866	7.294438
5.626184	346.316366	7.299443
5.550608	340.472174	7.304448
5.814667	352.719251	7.309453
5.701407	353.711641	7.314458
5.742408	359.412933	7.319462
5.370257	353.558257	7.324467
5.987613	360.222796	7.329472
5.753878	357.250816	7.334477
5.422636	358.732950	7.339482
5.803922	357.806513	7.344486
5.715868	359.089189	7.349491
5.911186	361.225991	7.354496
5.663528	353.874305	7.359501
6.059442	348.184032	7.364506
6.087467	344.389579	7.369510
5.445030	340.725486	7.374515
5.597699	342.653829	7.379520
5.400049	350.439499	7.384525
5.688483	345.731031	7.389530
5.682420	355.546329	7.394534
5.572426	354.946807	7.399539
5.619969	352.076293	7.404544
5.543462	357.118938	7.409549
5.602964	358.903689	7.414554
5.667439	362.987757	7.419558
5.705459	362.406174	7.424563
5.795936	349.290820	7.429568
6.015473	359.706700	7.434573
5.797450	357.105588	7.439578
5.686491	354.785102	7.444582
5.540994	354.940968	7.449587
5.582583	348.081814	7.454592
5.313977	357.277011	7.459597
5.639231	351.113744	7.464602
5.627660	353.466462	7.469606
5.647322	350.071959	7.474611
5.820773	354.047199	7.479616
5.244551	355.235517	7.484621
5.725956	350.000093	7.489626
5.808372	364.822510	7.494630
5.454180	361.290424	7.499635
5.950606	364.041287	7.504640
5.888432	365.123752	7.509645
5.843798	353.469101	7.514650
5.565026	357.860054	7.519654
5.476988	358.250531	7.524659
6.060538	368.720116	7.529664
5.962410	368.020656	7.534669
5.642162	363.629020	7.539674
5.914139	359.824815	7.544678
5.543995	357.902449	7.549683
5.858383	349.839431	7.554688
5.626575	352.682245	7.559693
5.544018	358.652838	7.564698
5.840573	361.336937	7.569702
5.793029	349.271449	7.574707
5.841205	351.580003	7.579712
5.419473	354.655060	7.584717
5.825843	347.387568	7.589722
5.814598	349.518767	7.594726
5.453354	351.711133	7.599731
5.991028	355.107277	7.604736
5.955437	361.029382	7.609741
5.793614	348.507226	7.614746
5.820531	353.160336	7.619750
5.673726	364.310674	7.624755
5.971026	359.056637	7.629760
5.813196	358.958166	7.634765
6.039643	353.405178	7.639770
5.867328	359.288591	7.644774
5.433038	353.105122	7.649779
5.564085	349.939945	7.654784
5.415149	362.773767	7.659789
5.755220	354.475764	7.664794
5.869429	355.125624	7.669798
5.552942	357.390073	7.674803
5.977759	351.040360	7.679808
5.771716	348.111500	7.684813
5.489358	350.437041	7.689818
5.627208	352.785330	7.694822
5.633059	347.580125	7.699827
5.853932	349.092813	7.704832
5.705401	348.657521	7.709837
5.631006	352.912044	7.714842
5.563729	352.384926	7.719846
5.841699	367.100774	7.724851
6.366593	365.123594	7.729856
6.095783	348.863062	7.734861
5.886698	358.463393	7.739866
5.949931	350.639046	7.744870
5.727568	348.984598	7.749875
6.028783	344.925873	7.754880
5.601956	347.448059	7.759885
6.000950	346.553650	7.764890
5.697971	348.012372	7.769894
5.767969	352.222125	7.774899
5.959884	349.563113	7.779904
5.651426	353.170925	7.784909
5.833711	353.016001	7.789914
5.959203	354.300021	7.794918
5.765240	356.431375	7.799923
6.318741	341.924166	7.804928
5.857771	345.916548	7.809933
5.596637	324.054570	7.814938
5.455740	328.332162	7.819942
5.407638	341.229265	7.824947
5.928217	341.005517	7.829952
5.718909	349.334025	7.834957
5.790460	338.192701	7.839962
5.876233	351.885100	7.844966
6.022916	348.600412	7.849971
5.980566	333.022285	7.854976
5.602647	330.322842	7.859981
5.820334	326.175967	7.864986
5.818569	329.112451	7.869990
5.800852	328.504800	7.874995
5.490740	325.753604	7.880000
5.536750	335.832820	7.885005
5.728568	339.596368	7.890010
5.597111	333.802064	7.895014
5.921022	350.089443	7.900019
5.943234	336.007174	7.905024
5.960397	336.321055	7.910029
6.137678	325.549159	7.915034
5.683064	325.424421	7.920038
5.535872	337.565077	7.925043
5.609356	321.911862	7.930048
5.303704	332.584023	7.935053
5.813423	329.802452	7.940058
5.794458	324.816281	7.945062
5.495561	331.216237	7.950067
5.721095	333.718467	7.955072
5.717215	354.420108	7.960077
5.741141	350.015679	7.965082
5.770631	356.180691	7.970086
5.690865	357.215291	7.975091
6.027301	347.165106	7.980096
5.760580	342.920115	7.985101
5.782767	325.882855	7.990106
5.661711	330.005476	7.995110
5.003228	335.019076	8.000115
5.456830	350.193562	8.005133
5.822178	353.926559	8.010150
5.950514	355.105824	8.015168
6.046705	353.289011	8.020186
6.027324	358.470817	8.025203
6.046146	348.533769	8.030221
5.700338	342.702677	8.035238
6.002930	325.589200	8.040256
5.629387	331.729031	8.045274
5.567456	340.366725	8.050291
6.024382	330.875430	8.055309
5.411252	341.754860	8.060326
5.601922	346.196865	8.065344
6.100842	348.290035	8.070362
5.787402	351.652868	8.075379
5.772407	337.561852	8.080397
5.767210	351.018950	8.085414
5.609137	353.723135	8.090432
5.663121	352.320027	8.095450
5.838505	358.620008	8.100467
5.932536	358.551817	8.105485
5.853277	361.130048	8.110502
5.828432	352.383245	8.115520
5.518647	353.151482	8.120538
5.594122	360.407530	8.125555
6.067219	355.647311	8.130573
5.881237	371.953987	8.135590
5.814734	359.736073	8.140608
6.223783	355.140519	8.145626
5.985013	368.593203	8.150643
6.175215	358.114910	8.155661
6.020698	365.921383	8.160678
5.724488	372.326817	8.165696
6.078069	359.093203	8.170714
5.674968	357.275726	8.175731
6.212413	353.035590	8.180749
5.900798	364.319063	8.185766
5.349994	362.833991	8.190784
6.208103	361.844523	8.195802
5.759418	363.764281	8.200819
5.945602	357.464829	8.205837
5.626549	366.054461	8.210854
5.774383	359.095155	8.215872
6.063091	365.677179	8.220890
5.594208	362.137503	8.225907
5.466869	356.732915	8.230925
5.761710	358.334208	8.235942
5.666219	360.378505	8.240960
6.223550	359.650754	8.245978
6.216822	364.811645	8.250995
6.174153	354.426645	8.256013
6.078339	365.685774	8.261030
6.167359	359.354209	8.266048
5.891543	348.756438	8.271066
5.834905	370.808396	8.276083
6.019240	351.491775	8.281101
5.853366	362.297985	8.286118
5.744953	359.541259	8.291136
5.976719	357.434965	8.296154
5.767989	365.451900	8.301171
6.044644	373.212909	8.306189
6.169250	386.353056	8.311206
5.976323	384.193382	8.316224
6.130503	380.186856	8.321242
6.285398	382.463319	8.326259
6.486775	372.993108	8.331277
6.026107	373.377894	8.336294
5.910530	364.806245	8.341312
6.068560	355.027259	8.346330
6.031575	350.201797	8.351347
6.107167	358.082664	8.356365
6.102419	369.355929	8.361382
6.144180	371.397656	8.366400
6.260446	371.433277	8.371418
5.904775	376.970731	8.376435
6.233465	371.519933	8.381453
6.315726	377.206518	8.386470
6.113970	368.275990	8.391488
6.066534	361.423016	8.396506
5.889544	363.817747	8.401523
6.218984	376.581816	8.406541
6.598864	385.753057	8.411558
6.371220	374.384031	8.416576
5.869871	362.915888	8.421594
6.145482	363.977407	8.426611
6.057970	356.919278	8.431629
6.273678	373.002076	8.436646
6.322035	377.709379	8.441664
6.174552	358.804496	8.446682
6.128743	362.841752	8.451699
5.972250	364.314950	8.456717
6.670373	375.367640	8.461734
5.953776	377.174745	8.466752
6.379743	361.029654	8.471770
6.217395	361.784258	8.476787
6.094795	367.256789	8.481805
6.380819	371.494515	8.486822
6.124937	375.028211	8.491840
6.303784	377.831087	8.496858
6.204312	383.549304	8.501875
6.362779	387.898536	8.506893
6.250798	387.348236	8.511910
6.363680	387.292870	8.516928
6.235552	375.535872	8.521946
6.460264	387.540044	8.526963
6.185269	370.368700	8.531981
6.255888	372.125045	8.536998
6.501100	380.414839	8.542016
6.239945	370.493244	8.547034
5.940927	369.656675	8.552051
6.422860	378.294379	8.557069
6.224148	387.704596	8.562087
6.268690	379.470763	8.567104
6.501793	385.619702	8.572122
6.233434	387.107272	8.577139
6.342796	385.521918	8.582157
6.395381	381.130530	8.587175
6.230083	376.211558	8.592192
6.237517	384.551232	8.597210
6.335261	392.270856	8.602227
6.498854	380.581755	8.607245
6.505260	381.546600	8.612263
6.237828	384.179563	8.617280
6.100429	366.964574	8.622298
6.263504	379.240325	8.627315
6.105830	381.146046	8.632333
6.781065	375.189678	8.637351
6.080653	387.269372	8.642368
6.587975	374.917359	8.647386
6.265702	378.802279	8.652403
6.424784	381.062307	8.657421
6.390770	378.224495	8.662439
6.367703	381.349336	8.667456
6.420070	377.822658	8.672474
6.564445	382.281393	8.677491
6.703933	382.802517	8.682509
6.626864	379.286652	8.687527
6.565181	384.642349	8.692544
6.540554	385.959190	8.697562
6.216853	382.841723	8.702579
6.029329	377.377132	8.707597
6.419358	378.250313	8.712615
6.392895	386.024108	8.717632
6.235358	377.370666	8.722650
6.301101	376.448543	8.727667
6.319647	385.919391	8.732685
6.619269	385.891570	8.737703
6.721539	391.202645	8.742720
6.593762	378.745013	8.747738
6.615731	385.656011	8.752755
6.467707	385.404843	8.757773
6.319009	373.430167	8.762791
6.507415	389.902259	8.767808
6.522981	402.548270	8.772826
6.737846	404.887922	8.777843
6.589973	404.762960	8.782861
6.792989	381.514466	8.787879
6.176771	386.994917	8.792896
6.833168	392.354869	8.797914
6.458851	387.825243	8.802931
6.948195	393.217681	8.807949
7.095610	391.812553	8.812967
6.600517	387.544844	8.817984
6.737598	381.092134	8.823002
6.663673	380.930339	8.828019
6.410398	381.178492	8.833037
6.802068	380.056982	8.838055
6.450064	378.045308	8.843072
6.620758	380.439213	8.848090
6.326161	376.973210	8.853107
6.680355	379.231069	8.858125
6.847895	374.004332	8.863143
6.720947	380.888169	8.868160
6.770921	377.434449	8.873178
6.540225	386.095452	8.878195
6.677090	376.004196	8.883213
6.742193	378.720754	8.888231
6.705935	378.868633	8.893248
6.578705	379.030766	8.898266
7.007582	379.569663	8.903283
6.773680	387.357026	8.908301
6.882881	373.877672	8.913319
6.854181	380.553615	8.918336
6.874607	373.194550	8.923354
6.836618	375.090986	8.928371
6.751230	385.212424	8.933389
6.789404	375.572125	8.938407
6.940322	381.090167	8.943424
6.878629	386.464800	8.948442
6.483341	387.019221	8.953459
6.529919	388.214454	8.958477
6.941293	368.470929	8.963495
6.868377	383.863669	8.968512
6.782889	379.184652	8.973530
6.556562	381.252606	8.978547
6.480267	383.259184	8.983565
6.984096	387.967709	8.988583
6.817614	397.631652	8.993600
7.142784	393.437390	8.998618
6.800372	384.882336	9.003635
6.925280	386.705914	9.008653
7.155105	386.127305	9.013671
6.475423	392.958897	9.018688
6.585562	381.246613	9.023706
6.591152	393.916271	9.028723
6.720589	402.110608	9.033741
7.101041	405.210098	9.038759
6.788917	410.652378	9.043776
7.151231	406.957213	9.048794
7.091101	414.136702	9.053811
6.486811	403.473601	9.058829
7.096014	400.793777	9.063847
7.129194	409.069469	9.068864
6.834539	408.289018	9.073882
7.353446	406.626871	9.078899
6.890343	399.450851	9.083917
7.199491	381.657806	9.088935
6.965965	386.762722	9.093952
6.850822	384.180613	9.098970
6.857222	384.085127	9.103987
6.830724	395.144069	9.109005
7.228266	379.921739	9.114023
6.910953	385.670932	9.119040
6.978162	383.748206	9.124058
7.254893	382.357531	9.129075
6.718112	387.964389	9.134093
7.142156	385.525014	9.139111
6.894088	386.930512	9.144128
7.055954	379.123257	9.149146
7.097339	383.632842	9.154163
6.828724	388.629649	9.159181
6.923717	390.710375	9.164199
7.201272	397.745431	9.169216
7.112660	402.313258	9.174234
7.299952	390.800315	9.179251
7.028892	399.615969	9.184269
7.144797	392.443905	9.189287
7.125922	383.326928	9.194304
6.739144	389.576148	9.199322
7.019260	390.845242	9.204339
7.400707	408.457889	9.209357
7.310123	398.755702	9.214375
7.082238	390.009136	9.219392
6.892742	385.914448	9.224410
7.273063	383.276799	9.229427
6.863260	390.788772	9.234445
6.963159	388.841989	9.239463
7.131675	397.951680	9.244480
7.328998	412.446894	9.249498
7.439179	400.437950	9.254515
6.989597	396.005320	9.259533
7.023201	393.362035	9.264551
7.190677	400.692046	9.269568
7.285449	403.429204	9.274586
7.407049	401.583160	9.279603
7.040934	401.647024	9.284621
6.874692	393.045430	9.289639
7.114621	401.187741	9.294656
7.186009	407.835388	9.299674
7.325999	403.922598	9.304691
7.152277	415.424335	9.309709
7.476027	406.783831	9.314727
7.306908	411.007673	9.319744
7.232064	411.612872	9.324762
7.040139	408.089751	9.329779
6.720087	414.603076	9.334797
7.170531	411.007709	9.339815
7.288784	408.783497	9.344832
7.297942	418.388375	9.349850
7.520064	411.357449	9.354867
7.195957	417.622106	9.359885
7.388922	412.334570	9.364903
7.702452	419.206211	9.369920
7.243536	417.369071	9.374938
7.297433	405.854928	9.379955
7.030184	414.120891	9.384973
6.716429	408.682380	9.389991
7.294517	408.017646	9.395008
7.047204	415.627245	9.400026
7.035638	417.393315	9.405043
6.964956	412.674099	9.410061
7.402982	419.772383	9.415079
7.853935	422.662017	9.420096
7.214438	410.836798	9.425114
7.507354	407.720542	9.430131
7.270852	404.207563	9.435149
7.162831	403.022334	9.440167
7.321678	408.753733	9.445184
7.291376	420.135174	9.450202
7.924910	426.442290	9.455219
7.188318	415.730484	9.460237
7.107246	416.361905	9.465255
7.781185	425.644881	9.470272
7.257250	424.628957	9.475290
7.584271	419.519228	9.480307
7.349825	424.965121	9.485325
7.660176	427.053133	9.490343
7.772941	422.519764	9.495360
7.656069	417.820407	9.500378
7.382623	406.550054	9.505395
7.588945	411.406182	9.510413
7.458068	411.146015	9.515431
7.625582	404.688529	9.520448
7.289305	406.363465	9.525466
7.362143	406.680441	9.530483
7.483320	408.252145	9.535501
7.693119	418.582968	9.540519
7.602262	420.569741	9.545536
7.119500	418.853100	9.550554
7.525588	418.041749	9.555571
7.810319	427.010172	9.560589
7.737464	424.923197	9.565607
7.524575	414.040977	9.570624
7.564794	418.096324	9.575642
7.620227	410.580283	9.580659
7.582832	416.219357	9.585677
7.494051	415.554969	9.590695
7.852604	415.953409	9.595712
7.615170	418.161961	9.600730
7.618882	408.441839	9.605747
7.747483	409.523238	9.610765
7.355284	404.753416	9.615783
7.571106	412.467171	9.620800
7.430238	424.689591	9.625818
7.828185	420.446050	9.630835
7.924036	416.953576	9.635853
8.013528	425.750621	9.640871
8.188987	408.331941	9.645888
7.292166	415.715106	9.650906
7.519844	395.429142	9.655923
7.562087	401.222988	9.660941
7.519382	408.478638	9.665959
7.743780	415.970148	9.670976
7.875807	427.556530	9.675994
7.840232	418.410594	9.681011
7.819336	414.406246	9.686029
7.539393	409.486293	9.691047
8.077193	412.687362	9.696064
7.506439	405.234721	9.701082
7.796275	408.708166	9.706099
8.150998	415.911017	9.711117
7.530521	394.116950	9.716135
7.929780	404.392834	9.721152
7.683833	403.910859	9.726170
7.545162	401.452353	9.731187
7.825350	411.150459	9.736205
8.239070	426.577441	9.741223
7.644301	409.080627	9.746240
7.659935	406.806224	9.751258
7.856791	412.165601	9.756275
7.701132	411.110910	9.761293
7.886448	420.905936	9.766311
8.162771	419.692045	9.771328
7.899401	421.055762	9.776346
7.941517	409.530840	9.781363
7.786876	415.869928	9.786381
7.708441	406.298375	9.791399
8.007689	409.593624	9.796416
8.009382	416.769738	9.801434
7.722311	399.963171	9.806451
7.724903	417.127110	9.811469
8.088667	430.677935	9.816487
8.143829	428.634017	9.821504
7.590317	422.481996	9.826522
7.806297	431.593736	9.831539
8.145710	425.917182	9.836557
7.909294	431.445435	9.841575
7.922612	431.443538	9.846592
7.886048	430.704697	9.851610
8.249319	431.313835	9.856627
8.232732	437.763841	9.861645
7.570003	425.898071	9.866663
7.947678	430.484364	9.871680
8.025412	440.725440	9.876698
8.391466	430.841237	9.881715
8.245775	434.278786	9.886733
7.739187	432.209276	9.891751
8.160666	430.190012	9.896768
7.875508	433.983924	9.901786
8.023839	432.891070	9.906803
8.204007	430.483587	9.911821
7.979000	426.479660	9.916839
8.101172	428.846461	9.921856
8.158876	440.147855	9.926874
7.922851	437.392176	9.931891
7.935967	428.153401	9.936909
7.781787	438.711675	9.941927
8.241883	431.031238	9.946944
8.004213	430.494318	9.951962
7.886987	424.362300	9.956979
8.149884	425.141796	9.961997
8.067803	435.934921	9.967015
7.964905	434.360730	9.972032
7.970035	439.806959	9.977050
7.991319	431.589369	9.982067
8.162919	428.529987	9.987085
8.131226	434.120837	9.992103
7.971129	427.799878	9.997120
7.746008	437.308931	10.002138
8.040769	429.648088	10.007155
8.245844	433.999497	10.012173
8.238075	454.529136	10.017191
8.506881	440.491401	10.022208
8.348855	435.599675	10.027226
7.997784	428.715354	10.032243
8.073352	427.431933	10.037261
8.354964	441.784578	10.042279
8.302105	451.777883	10.047296
8.214473	451.384709	10.052314
8.702117	443.254988	10.057331
8.445449	435.712098	10.062349
8.071505	433.432459	10.067367
8.633229	421.573656	10.072384
8.316156	426.196219	10.077402
8.217437	436.834163	10.082419
8.356388	429.002076	10.087437
8.467787	435.558259	10.092455
8.352615	431.316218	10.097472
8.230315	432.758817	10.102490
8.764749	418.051485	10.107507
8.368646	421.086460	10.112525
8.528512	424.567649	10.117543
8.277187	430.341231	10.122560
8.528899	434.205657	10.127578
8.288518	423.876840	10.132595
8.491396	423.406592	10.137613
8.188341	427.209618	10.142631
8.275393	418.814474	10.147648
8.346842	427.696396	10.152666
8.319600	417.955872	10.157683
8.404898	426.570540	10.162701
8.756385	428.033578	10.167719
8.374288	433.272237	10.172736
8.513685	428.832522	10.177754
8.248109	424.535154	10.182771
8.194201	416.698576	10.187789
8.003672	427.309875	10.192807
8.448251	438.235075	10.197824
8.580327	443.509939	10.202842
8.706215	446.160179	10.207859
8.712498	449.728551	10.212877
8.473411	447.525610	10.217895
8.544207	435.428140	10.222912
8.832505	434.266020	10.227930
8.542045	436.877352	10.232947
8.469532	426.392846	10.237965
7.880990	429.227604	10.242983
8.327357	445.148096	10.248000
8.611333	451.771919	10.253018
8.719410	451.900340	10.258035
8.977903	444.989933	10.263053
8.850234	451.813950	10.268071
9.016212	442.857326	10.273088
8.892127	437.155562	10.278106
8.590921	435.757607	10.283123
8.642071	423.950397	10.288141
8.626570	432.514590	10.293159
8.357576	435.267724	10.298176
8.715199	430.673898	10.303194
8.543930	424.193747	10.308211
8.783083	425.106349	10.313229
8.369174	431.394548	10.318247
8.696359	433.031805	10.323264
8.782137	437.685925	10.328282
8.942662	442.208415	10.333299
8.901514	431.135176	10.338317
8.639100	434.228101	10.343335
8.689339	429.385795	10.348352
8.402433	428.320110	10.353370
8.569469	436.319226	10.358387
8.871815	439.847520	10.363405
9.073022	455.364627	10.368423
8.645975	442.499411	10.373440
8.798531	437.028854	10.378458
8.474228	452.467352	10.383475
9.008207	444.027417	10.388493
8.699789	452.126281	10.393511
8.378884	442.554830	10.398528
8.744544	449.743358	10.403546
8.782450	448.996004	10.408563
9.035599	447.201926	10.413581
8.854123	458.566052	10.418599
8.630602	455.230907	10.423616
8.559992	448.652926	10.428634
8.881527	449.805083	10.433651
8.889007	453.979175	10.438669
8.802343	456.151486	10.443687
8.906078	455.750419	10.448704
8.930991	450.987814	10.453722
9.113773	452.139620	10.458739
8.987124	448.779831	10.463757
9.134950	446.983320	10.468775
9.031716	453.579451	10.473792
8.962139	455.865848	10.478810
8.600620	458.090691	10.483827
9.063519	448.879261	10.488845
8.877055	459.502565	10.493863
8.842326	459.807994	10.498880
9.249975	454.808697	10.503898
8.860181	457.867936	10.508915
9.094872	450.989658	10.513933
8.904178	456.573870	10.518951
9.299617	445.779351	10.523968
9.226482	450.893868	10.528986
8.801552	458.222048	10.534003
9.102655	458.881952	10.539021
9.026153	464.943730	10.544039
9.063750	462.028413	10.549056
9.227928	452.816449	10.554074
9.204091	468.195260	10.559091
9.343488	456.042847	10.564109
9.194808	458.171227	10.569127
9.206682	457.844513	10.574144
9.305953	454.155839	10.579162
8.813815	456.612583	10.584179
8.964659	451.565162	10.589197
8.906620	458.204706	10.594215
8.874096	454.956398	10.599232
9.318525	447.754929	10.604250
9.173520	455.607287	10.609267
9.005706	459.360728	10.614285
9.341581	464.834037	10.619303
8.966692	456.940437	10.624320
9.087376	453.926897	10.629338
8.961043	458.292368	10.634355
9.064119	455.351014	10.639373
9.084581	455.635172	10.644391
8.864763	458.178636	10.649408
9.240815	451.656901	10.654426
8.791146	466.464966	10.659443
9.140943	455.879561	10.664461
9.044738	467.918289	10.669479
9.510137	479.638662	10.674496
9.323034	468.824951	10.679514
9.062935	463.213916	10.684531
9.433194	463.137158	10.689549
9.572174	475.391504	10.694567
9.277501	466.497576	10.699584
9.071712	460.483562	10.704602
9.238101	475.349743	10.709619
9.196423	474.337150	10.714637
9.575080	473.536406	10.719655
9.283020	477.845798	10.724672
9.508616	473.086457	10.729690
9.507433	481.515888	10.734707
9.201912	469.887606	10.739725
9.519311	471.598983	10.744743
9.432635	473.367360	10.749760
9.421128	461.942323	10.754778
9.173461	458.683543	10.759795
9.376113	465.096053	10.764813
9.347034	475.101424	10.769831
9.548226	480.147721	10.774848
9.582657	470.280742	10.779866
9.400047	474.481467	10.784883
9.376756	479.124285	10.789901
9.674129	475.887400	10.794919
9.541218	480.121365	10.799936
9.637864	470.541280	10.804954
9.088602	459.096361	10.809971
9.403980	469.136119	10.814989
9.390708	469.169946	10.820007
9.155339	482.887267	10.825024
9.552493	475.948810	10.830042
9.518086	477.323994	10.835059
9.560284	468.850649	10.840077
9.322112	481.100976	10.845095
9.301885	474.044881	10.850112
9.763767	466.228452	10.855130
9.219821	475.651781	10.860147
9.469771	478.115332	10.865165
9.717329	474.646415	10.870183
9.577172	480.945387	10.875200
9.676960	474.937138	10.880218
9.622836	476.959188	10.885235
9.571973	475.888074	10.890253
9.923779	472.645817	10.895271
9.547279	477.186187	10.900288
9.563497	472.885680	10.905306
9.572033	472.591046	10.910323
9.445149	477.628786	10.915341
9.853293	476.785553	10.920359
9.626988	478.373838	10.925376
9.681465	477.055848	10.930394
9.272408	483.923966	10.935411
9.662165	487.066194	10.940429
9.849932	500.108167	10.945447
9.640500	497.307287	10.950464
10.234964	491.335134	10.955482
9.939652	480.718249	10.960499
9.874736	479.895487	10.965517
9.757308	473.735081	10.970535
9.506192	477.372191	10.975552
9.755686	473.890347	10.980570
10.469682	482.791541	10.985587
9.765724	484.369460	10.990605
10.054970	471.458264	10.995623
9.671834	470.839994	11.000640
9.813070	475.368671	11.005658
9.863845	482.956839	11.010675
9.315704	474.197294	11.015693
9.869999	474.202153	11.020711
9.612334	486.865788	11.025728
10.077123	495.092830	11.030746
9.932526	497.198484	11.035763
10.062286	496.607148	11.040781
10.203075	493.028725	11.045799
10.067948	479.622287	11.050816
9.882770	474.173078	11.055834
10.067003	477.139225	11.060851
9.857565	473.492604	11.065869
9.780391	474.899735	11.070887
9.708812	473.686702	11.075904
10.089428	480.326951	11.080922
10.287329	484.029408	11.085939
9.956812	489.177951	11.090957
10.257954	486.760974	11.095975
10.287388	478.314871	11.100992
10.307495	471.378689	11.106010
9.951838	474.517787	11.111027
9.908753	472.249419	11.116045
9.760048	464.355090	11.121063
9.820463	472.806424	11.126080
9.958454	477.824754	11.131098
9.968028	486.596480	11.136115
10.203559	494.969895	11.141133
10.290069	484.447815	11.146151
10.371209	495.164910	11.151168
10.082629	465.511378	11.156186
10.223511	472.889766	11.161203
9.911460	469.177174	11.166221
9.946719	478.011144	11.171239
9.974523	492.968480	11.176256
10.231471	493.007304	11.181274
10.386142	496.167433	11.186291
10.471394	492.660827	11.191309
10.323693	484.258253	11.196327
10.021977	484.520308	11.201344
10.313544	485.181707	11.206362
10.290760	483.882133	11.211379
10.458411	482.082513	11.216397
10.088994	473.099308	11.221415
10.072153	482.200215	11.226432
10.124254	491.848897	11.231450
10.501047	493.494166	11.236467
10.241907	498.820875	11.241485
10.152127	492.009199	11.246503
10.087406	499.366164	11.251520
10.152058	492.486110	11.256538
10.351679	491.249518	11.261555
10.187153	496.138529	11.266573
10.125179	492.860115	11.271591
10.077424	499.715811	11.276608
10.288366	497.265629	11.281626
10.003885	497.985726	11.286643
10.166877	492.646059	11.291661
10.741266	485.682986	11.296679
10.568880	491.507335	11.301696
10.731829	486.682067	11.306714
10.651152	492.094420	11.311731
10.376730	496.697695	11.316749
10.481465	493.011313	11.321767
10.443795	491.269108	11.326784
10.609604	491.009791	11.331802
10.457467	492.122559	11.336819
10.336326	502.603111	11.341837
10.620093	495.079661	11.346855
10.403659	492.996239	11.351872
10.365279	494.602418	11.356890
10.508634	494.034198	11.361907
10.118027	499.144823	11.366925
10.746817	489.238357	11.371943
10.482478	490.605387	11.376960
10.740358	490.710337	11.381978
10.719640	494.065201	11.386995
10.781466	497.123113	11.392013
10.362711	489.097518	11.397031
10.388300	496.484513	11.402048
10.024424	492.275113	11.407066
10.451411	486.534327	11.412083
10.616400	502.060305	11.417101
10.745000	510.431546	11.422119
10.713465	509.275352	11.427136
10.757902	492.896433	11.432154
10.785008	493.176395	11.437171
10.573127	497.631018	11.442189
10.672544	493.008205	11.447207
10.731559	494.403466	11.452224
10.474502	495.135045	11.457242
10.821836	502.553682	11.462259
11.023644	510.014057	11.467277
11.153377	491.475849	11.472295
10.771324	493.404115	11.477312
10.560249	493.674059	11.482330
11.066136	483.569105	11.487347
10.820424	493.539001	11.492365
10.759881	477.754050	11.497383
10.863553	487.337846	11.502400
10.807047	488.123208	11.507418
11.128032	480.095321	11.512435
10.578076	490.605184	11.517453
10.613151	491.019596	11.522471
10.898828	493.177753	11.527488
10.371211	489.653565	11.532506
10.734996	494.169467	11.537523
10.563586	507.898876	11.542541
10.764099	509.805294	11.547559
10.971373	508.049956	11.552576
10.898361	508.418187	11.557594
11.449060	511.121797	11.562611
10.939313	518.570588	11.567629
11.118161	505.092846	11.572647
10.966418	502.630062	11.577664
10.771244	490.814066	11.582682
11.210391	498.256185	11.587699
10.896397	497.999461	11.592717
10.981485	507.248511	11.597735
11.040945	507.539183	11.602752
11.208259	505.985763	11.607770
11.192313	494.867511	11.612787
10.857220	499.306725	11.617805
10.904648	493.445528	11.622823
11.083121	500.862219	11.627840
11.114656	516.715230	11.632858
11.088297	509.707419	11.637875
11.251824	509.085546	11.642893
10.982381	502.014840	11.647911
11.369167	498.675580	11.652928
11.113707	501.354021	11.657946
11.117043	482.958701	11.662963
11.174797	488.803794	11.667981
10.772139	490.369219	11.672999
11.374153	503.803877	11.678016
11.086761	512.060418	11.683034
11.468591	507.061996	11.688051
11.092675	496.713347	11.693069
11.309481	496.894160	11.698087
11.179096	497.788927	11.703104
11.158546	500.165477	11.708122
11.537210	494.429104	11.713139
11.035430	500.942531	11.718157
11.381139	494.040531	11.723175
11.156332	497.345322	11.728192
11.156677	499.504006	11.733210
11.336924	504.443139	11.738227
11.466818	514.941171	11.743245
11.232233	513.371826	11.748263
11.361390	503.701424	11.753280
11.199162	509.350619	11.758298
11.278338	501.925493	11.763315
11.355261	519.361904	11.768333
11.220372	514.049968	11.773351
11.010604	526.491534	11.778368
11.303687	517.265651	11.783386
11.702838	511.914223	11.788403
11.565967	516.994564	11.793421
11.348177	512.049065	11.798439
11.623320	519.204467	11.803456
11.414218	515.955413	11.808474
11.821747	513.562789	11.813491
11.434031	508.385142	11.818509
11.406900	504.422776	11.823527
11.555314	516.025582	11.828544
10.968093	504.630761	11.833562
11.575890	510.143530	11.838579
11.467197	513.941367	11.843597
11.450803	512.719685	11.848615
11.722553	509.089181	11.853632
11.384321	512.519044	11.858650
11.758018	512.643717	11.863667
11.577836	504.056876	11.868685
11.659372	507.553510	11.873703
11.718425	511.015798	11.878720
11.714956	516.302453	11.883738
11.799352	512.792821	11.888755
11.529260	516.877877	11.893773
11.644990	510.917610	11.898791
11.557336	505.210116	11.903808
11.440755	519.211807	11.908826
11.323439	510.040762	11.913843
11.739521	505.541898	11.918861
11.711422	513.801995	11.923879
11.715598	506.155090	11.928896
11.672758	513.038423	11.933914
11.856767	515.597517	11.938931
11.864012	514.028151	11.943949
11.937105	503.123158	11.948967
11.961099	517.986439	11.953984
11.742586	519.201125	11.959002
11.857066	525.169885	11.964019
11.678082	522.973296	11.969037
11.837775	518.448329	11.974055
11.715201	516.577414	11.979072
11.542424	518.895767	11.984090
11.649399	508.159030	11.989107
11.847255	517.955301	11.994125
11.745155	505.995325	11.999143
11.937658	496.065695	12.004160
11.581333	512.108859	12.009178
11.609800	521.884335	12.014195
11.528213	518.400708	12.019213
11.582851	506.261541	12.024231
11.768547	505.446848	12.029248
11.634164	515.837966	12.034266
11.691994	523.245167	12.039283
12.238296	530.676822	12.044301
12.401117	529.752104	12.049319
12.563481	517.958965	12.054336
12.108251	510.229406	12.059354
11.808966	506.265499	12.064371
11.866440	509.885823	12.069389
11.727374	502.854649	12.074407
12.009933	505.893757	12.079424
11.768587	511.201903	12.084442
12.163437	524.523869	12.089459
12.243700	530.782012	12.094477
12.182008	517.723798	12.099495
11.969209	506.866752	12.104512
11.845457	520.210011	12.109530
12.380680	524.727462	12.114547
12.050744	530.421876	12.119565
12.335388	526.076143	12.124583
12.225041	507.039053	12.129600
11.745557	514.603020	12.134618
12.109526	519.185172	12.139635
12.346574	527.100776	12.144653
12.320708	536.035869	12.149671
12.468126	526.703417	12.154688
11.975883	531.498619	12.159706
12.385791	521.134129	12.164723
12.081786	512.039670	12.169741
11.965894	525.520555	12.174759
12.135948	525.774965	12.179776
12.088956	536.461668	12.184794
12.005279	541.442164	12.189811
12.190134	533.309351	12.194829
12.210946	533.107466	12.199847
12.353161	529.894882	12.204864
11.997119	535.085307	12.209882
12.075505	533.952914	12.214899
12.468897	537.978199	12.219917
12.620023	542.016198	12.224935
12.664329	533.615074	12.229952
12.393454	537.119594	12.234970
12.587806	532.494519	12.239987
12.324117	543.912606	12.245005
11.895818	532.253028	12.250023
12.314126	526.305308	12.255040
12.514137	536.934376	12.260058
12.725418	536.595352	12.265075
12.580123	531.307132	12.270093
12.431970	529.377108	12.275111
12.648330	527.882274	12.280128
12.501930	527.804416	12.285146
12.190445	530.882956	12.290163
12.445809	535.595736	12.295181
12.617039	535.641680	12.300199
12.746247	522.228507	12.305216
12.473086	524.089223	12.310234
12.685631	526.580732	12.315251
12.454663	523.344570	12.320269
12.436214	533.089533	12.325287
12.574700	527.479143	12.330304
12.595898	539.789857	12.335322
12.663988	537.822795	12.340339
12.709467	536.503055	12.345357
12.230063	531.046280	12.350375
12.586840	535.443372	12.355392
12.493304	542.142156	12.360410
12.842227	551.958957	12.365427
13.181031	545.159004	12.370445
13.104748	541.567245	12.375463
12.774126	527.200487	12.380480
12.722687	524.494768	12.385498
12.411050	535.162976	12.390515
12.857828	526.279077	12.395533
12.527150	531.310894	12.400551
12.536309	530.842593	12.405568
12.637925	544.967906	12.410586
13.075467	558.201158	12.415603
13.068444	550.022663	12.420621
12.682165	540.038527	12.425639
12.853036	542.088447	12.430656
12.862332	550.560450	12.435674
13.314379	552.998659	12.440691
13.158922	536.316507	12.445709
12.767663	535.863607	12.450727
12.668329	530.157935	12.455744
12.706715	541.522380	12.460762
12.781465	544.448888	12.465779
12.919511	543.146202	12.470797
13.132833	556.941600	12.475815
13.159209	541.969789	12.480832
13.170350	546.323209	12.485850
12.955952	540.376788	12.490867
12.951357	525.842185	12.495885
12.741770	541.133399	12.500903
13.005312	547.277625	12.505920
13.176208	548.207240	12.510938
13.273101	548.208027	12.515955
13.422822	539.626284	12.520973
12.776337	544.960047	12.525991
13.150095	542.395987	12.531008
12.581493	543.469869	12.536026
13.119460	557.504733	12.541043
13.312208	553.302779	12.546061
12.849940	553.003015	12.551079
13.215036	546.334641	12.556096
13.224330	543.881333	12.561114
12.944894	557.864390	12.566131
13.122629	550.685730	12.571149
13.135466	554.432977	12.576167
13.217832	546.414045	12.581184
13.472223	545.575964	12.586202
13.363374	556.540613	12.591219
13.593841	543.976242	12.596237
13.411818	547.211224	12.601255
13.449693	558.099236	12.606272
13.175817	556.674898	12.611290
13.338762	548.220466	12.616307
13.629565	547.417705	12.621325
13.119904	546.756140	12.626343
13.253043	547.552817	12.631360
13.479682	546.286742	12.636378
13.271271	558.153765	12.641395
13.322932	549.827220	12.646413
13.312677	557.970933	12.651431
13.326702	553.127956	12.656448
13.644342	547.296987	12.661466
13.254251	544.505471	12.666483
13.451423	543.240857	12.671501
13.399460	544.369491	12.676519
13.274216	541.836278	12.681536
13.397303	541.309102	12.686554
13.522262	550.106962	12.691571
13.616642	545.062050	12.696589
13.334188	553.936369	12.701607
13.314379	549.256483	12.706624
13.187774	554.590845	12.711642
13.563749	550.808305	12.716659
13.414060	544.236367	12.721677
13.246313	552.991728	12.726695
13.550579	561.051449	12.731712
13.759979	559.977421	12.736730
13.445606	573.113902	12.741747
13.583887	564.698040	12.746765
13.384045	573.998079	12.751783
13.719907	567.725595	12.756800
13.843774	566.065369	12.761818
13.276330	572.964649	12.766835
13.685507	568.782429	12.771853
14.047323	569.748403	12.776871
13.606743	574.715401	12.781888
13.764371	576.893632	12.786906
13.759367	573.678860	12.791923
13.466917	573.399825	12.796941
13.568696	565.983754	12.801959
13.694265	565.421475	12.806976
13.708928	574.302900	12.811994
13.618971	581.341963	12.817011
14.288858	571.126057	12.822029
13.992317	573.239748	12.827047
13.796983	565.381082	12.832064
13.811872	578.096751	12.837082
13.600729	564.351867	12.842099
13.859000	562.399186	12.847117
13.909060	572.060854	12.852135
13.640183	571.781282	12.857152
13.688570	564.430381	12.862170
13.883678	576.511901	12.867187
14.238271	562.779364	12.872205
14.184143	575.092437	12.877223
14.121344	570.034275	12.882240
13.966030	566.994533	12.887258
13.968729	573.444723	12.892275
13.811725	568.215131	12.897293
13.822450	572.972563	12.902311
14.074198	569.064317	12.907328
14.240837	571.222200	12.912346
14.015278	567.022668	12.917363
13.933117	565.328452	12.922381
14.298108	589.517356	12.927399
14.165739	581.090243	12.932416
14.095162	574.871969	12.937434
14.231267	572.310427	12.942451
14.363301	578.532073	12.947469
13.935528	576.955122	12.952487
14.238871	580.647390	12.957504
14.613184	583.410205	12.962522
13.946107	571.844817	12.967539
14.083106	574.136732	12.972557
14.404690	591.064667	12.977575
14.429241	591.313473	12.982592
14.461985	568.318631	12.987610
14.257334	568.805318	12.992627
14.306871	563.227788	12.997645
14.480153	562.815822	13.002663
14.112790	571.782348	13.007680
14.603559	572.642912	13.012698
14.282977	569.480742	13.017715
14.132701	573.294574	13.022733
14.404235	576.531080	13.027751
14.344323	590.126319	13.032768
14.597620	586.334590	13.037786
14.927773	587.198230	13.042803
14.727090	573.319157	13.047821
14.585078	570.248928	13.052839
14.564306	578.211262	13.057856
14.617328	568.663206	13.062874
14.291759	571.403135	13.067891
14.275626	575.016070	13.072909
14.350443	572.880694	13.077927
14.279758	575.662738	13.082944
14.657630	571.305543	13.087962
14.349320	581.742884	13.092979
14.784469	579.838227	13.097997
14.611495	574.188260	13.103015
14.487547	586.206169	13.108032
14.914822	586.764259	13.113050
14.642302	590.338473	13.118067
14.673791	580.569724	13.123085
14.580279	574.146762	13.128103
14.608341	585.588591	13.133120
14.826665	585.955359	13.138138
14.746098	586.428916	13.143155
14.748863	579.889883	13.148173
15.028585	574.680224	13.153191
14.796362	578.879280	13.158208
14.573532	572.435555	13.163226
14.617530	577.721103	13.168243
15.123705	577.774528	13.173261
14.869580	566.415839	13.178279
14.317770	571.185671	13.183296
14.977391	577.431950	13.188314
14.773801	594.653611	13.193331
14.837987	589.566081	13.198349
14.844207	598.404660	13.203367
14.807088	595.772425	13.208384
14.971269	589.561546	13.213402
14.895298	595.415003	13.218419
14.781568	593.211336	13.223437
14.867964	592.992863	13.228455
14.775635	600.704489	13.233472
15.272022	594.403688	13.238490
14.900210	599.407254	13.243507
15.054164	600.150179	13.248525
14.917811	595.617929	13.253543
14.851081	589.417982	13.258560
15.214156	588.726972	13.263578
15.597269	601.751035	13.268595
14.955413	590.954852	13.273613
15.108757	593.774381	13.278631
15.139625	601.962163	13.283648
15.133053	590.952834	13.288666
14.969985	598.921694	13.293683
14.863293	595.713383	13.298701
15.173972	591.808522	13.303719
15.052946	598.625243	13.308736
15.012052	585.970817	13.313754
15.253292	596.009641	13.318771
15.124010	597.049406	13.323789
15.170348	594.012778	13.328807
15.048667	604.925818	13.333824
15.167856	590.122461	13.338842
15.124485	588.422164	13.343859
14.703450	597.368711	13.348877
15.410433	608.114048	13.353895
15.571750	612.989907	13.358912
15.326379	591.837410	13.363930
15.503953	590.556930	13.368947
15.233893	588.137918	13.373965
15.160677	592.125872	13.378983
15.397588	603.964177	13.384000
15.614891	606.587495	13.389018
15.803637	609.537179	13.394035
15.626268	600.889891	13.399053
15.504940	596.737136	13.404071
15.514776	597.272269	13.409088
15.801536	586.346371	13.414106
15.474004	583.579761	13.419123
15.158523	588.855364	13.424141
15.564779	579.592782	13.429159
15.057129	579.615706	13.434176
15.441012	601.384335	13.439194
15.925234	605.057735	13.444211
15.469836	601.506429	13.449229
15.405493	600.819270	13.454247
15.258472	609.694488	13.459264
15.637372	608.000611	13.464282
15.663625	612.345368	13.469299
15.362782	608.703574	13.474317
15.478344	614.012633	13.479335
15.441476	610.449399	13.484352
15.606313	606.999728	13.489370
15.706845	614.939917	13.494387
15.667730	613.513506	13.499405
15.608220	615.375469	13.504423
15.544779	618.456185	13.509440
15.477088	605.392535	13.514458
15.804740	605.903119	13.519475
15.334701	609.561933	13.524493
15.881325	622.367890	13.529511
15.733302	637.318182	13.534528
16.137859	637.027768	13.539546
16.143150	644.080334	13.544563
16.347681	628.319990	13.549581
15.918577	614.823812	13.554599
16.299643	610.942632	13.559616
15.766811	612.036159	13.564634
15.981795	615.442478	13.569651
15.929825	607.365672	13.574669
16.317597	611.931496	13.579687
16.064725	622.066686	13.584704
15.946893	608.777361	13.589722
15.967897	604.977843	13.594739
15.583053	609.043029	13.599757
16.090060	607.007190	13.604775
15.694133	614.378227	13.609792
16.349121	615.541265	13.614810
16.189469	611.959399	13.619827
15.755906	609.313539	13.624845
16.214910	628.921337	13.629863
16.140402	627.348991	13.634880
16.298889	630.385470	13.639898
16.482751	632.389184	13.644915
16.241037	619.778822	13.649933
16.311452	605.661589	13.654951
16.048840	608.274894	13.659968
15.923503	624.569144	13.664986
16.350854	624.552869	13.670003
16.172967	638.797788	13.675021
16.481978	633.517251	13.680039
16.410141	632.818643	13.685056
16.278712	630.223270	13.690074
16.221320	631.062426	13.695091
16.195125	646.656355	13.700109
16.400542	633.622477	13.705127
16.497286	641.853605	13.710144
16.514370	637.963176	13.715162
16.408267	632.290090	13.720179
16.165217	629.425029	13.725197
16.302800	634.408753	13.730215
16.285954	636.447071	13.735232
16.269563	630.933498	13.740250
16.650597	630.760378	13.745267
16.522932	636.066528	13.750285
16.780006	630.298670	13.755303
16.812575	632.726875	13.760320
16.987872	626.359607	13.765338
16.469713	621.675733	13.770355
16.454423	637.103844	13.775373
16.604594	627.843491	13.780391
16.739910	637.577043	13.785408
16.634749	636.448155	13.790426
16.523843	625.808601	13.795443
16.521856	632.202743	13.800461
16.815513	631.702488	13.805479
16.478296	636.299858	13.810496
16.634070	629.547485	13.815514
16.597753	627.669355	13.820531
16.462721	632.279228	13.825549
16.651493	622.536305	13.830567
16.493893	627.493693	13.835584
16.600226	623.403092	13.840602
16.551153	622.606243	13.845619
16.562724	647.958284	13.850637
16.596445	643.367816	13.855655
16.808884	649.936650	13.860672
16.961241	661.377988	13.865690
17.062050	655.476816	13.870707
16.906017	659.657641	13.875725
16.902229	664.297451	13.880743
17.054193	658.520807	13.885760
16.716453	658.592848	13.890778
16.791499	653.001826	13.895795
16.732864	660.613524	13.900813
17.238638	656.763288	13.905831
16.862518	656.017679	13.910848
16.974509	652.399555	13.915866
17.269251	650.157128	13.920883
17.306367	662.351824	13.925901
17.011668	661.202139	13.930919
17.496584	660.924380	13.935936
17.205687	654.314566	13.940954
17.059502	653.801174	13.945971
17.083228	652.484834	13.950989
17.065043	654.630660	13.956007
16.926152	656.028540	13.961024
17.097088	648.955048	13.966042
17.280315	647.945076	13.971059
17.069077	651.528636	13.976077
16.944810	660.324574	13.981095
16.891377	649.174229	13.986112
16.848748	659.491094	13.991130
17.148446	662.767385	13.996147
17.227645	675.870678	14.001165
17.422491	674.767366	14.006183
17.784764	679.974675	14.011200
17.485515	668.638770	14.016218
17.721939	657.670223	14.021235
17.289153	657.318500	14.026253
17.131904	655.572924	14.031271
17.592314	662.304881	14.036288
17.687158	660.835387	14.041306
17.787861	658.576024	14.046323
17.600497	656.841478	14.051341
17.482646	655.591501	14.056359
17.513230	654.062647	14.061376
17.040404	648.286069	14.066394
17.641292	659.294212	14.071411
17.801874	675.288091	14.076429
17.724412	668.477572	14.081447
17.882536	653.813229	14.086464
17.272173	656.307458	14.091482
17.342762	650.414178	14.096499
17.579961	672.183784	14.101517
17.785197	677.516683	14.106535
18.100103	667.738193	14.111552
17.829313	664.842759	14.116570
17.679554	647.903990	14.121587
17.649939	649.335241	14.126605
17.665329	659.977530	14.131623
17.885738	660.467049	14.136640
17.603719	669.316110	14.141658
17.669764	667.797479	14.146675
17.860629	666.511754	14.151693
17.985467	659.915695	14.156711
18.230428	661.875126	14.161728
17.659361	667.209732	14.166746
18.062012	657.666809	14.171763
17.857684	663.287935	14.176781
17.755697	661.596816	14.181799
18.384571	662.924895	14.186816
18.131238	661.762417	14.191834
18.175740	649.754128	14.196851
17.760172	652.896333	14.201869
17.640327	647.919671	14.206887
18.250139	658.655017	14.211904
18.105528	665.920427	14.216922
18.081447	661.427374	14.221939
17.981192	671.702782	14.226957
18.079438	670.286402	14.231975
18.299307	670.356284	14.236992
17.973531	673.067857	14.242010
18.207278	666.596743	14.247027
18.296357	671.086305	14.252045
18.194876	664.525704	14.257063
18.394178	669.297797	14.262080
18.247864	669.040045	14.267098
18.308687	664.678854	14.272115
18.233249	666.249829	14.277133
18.353001	658.897175	14.282151
18.446848	649.992774	14.287168
17.737401	651.779849	14.292186
18.264235	656.819356	14.297203
18.232657	664.748709	14.302221
18.219538	657.618844	14.307239
18.615648	672.089436	14.312256
18.297208	666.986094	14.317274
18.469403	665.539193	14.322291
18.722017	659.052502	14.327309
18.351008	666.081986	14.332327
18.309522	665.324971	14.337344
18.327526	664.953111	14.342362
18.466484	663.120099	14.347379
18.337737	664.159785	14.352397
18.081617	665.355126	14.357415
18.558929	661.645048	14.362432
18.562443	673.109714	14.367450
18.255036	661.371149	14.372467
18.154656	672.110480	14.377485
18.321714	689.081655	14.382503
18.806719	678.130952	14.387520
19.115552	688.430636	14.392538
19.000135	686.167262	14.397555
18.480500	678.211035	14.402573
18.465341	690.161476	14.407591
19.062556	699.737485	14.412608
18.448039	699.603583	14.417626
18.579269	691.794681	14.422643
18.651839	694.371261	14.427661
18.458480	698.838810	14.432679
18.990534	687.442073	14.437696
18.652315	702.393817	14.442714
18.820251	690.179969	14.447731
18.607898	692.775944	14.452749
18.147437	689.695629	14.457767
18.909810	694.906526	14.462784
18.761014	709.898025	14.467802
19.125800	712.226852	14.472819
19.339314	713.007787	14.477837
19.147468	696.447951	14.482855
19.055379	690.387642	14.487872
18.811236	693.345205	14.492890
18.698821	692.151178	14.497907
19.477480	702.295207	14.502925
19.055708	691.909448	14.507943
19.208501	692.624156	14.512960
19.039856	694.809341	14.517978
19.017619	697.129376	14.522995
19.398498	699.847000	14.528013
19.318637	697.833674	14.533031
19.115323	688.350963	14.538048
19.123362	692.480843	14.543066
19.301725	695.201794	14.548083
19.499737	699.554375	14.553101
19.144189	695.589774	14.558119
19.306176	690.344880	14.563136
19.137889	698.456613	14.568154
19.404482	701.302596	14.573171
19.408873	709.084321	14.578189
19.309483	714.625905	14.583207
19.717387	705.514480	14.588224
19.416683	701.582310	14.593242
19.280652	696.185292	14.598259
19.430028	701.375470	14.603277
19.377619	711.106917	14.608295
19.748026	707.126401	14.613312
19.651618	709.275023	14.618330
19.449174	695.481337	14.623347
19.429262	696.365117	14.628365
19.388279	711.103039	14.633383
19.696160	715.593045	14.638400
19.203967	718.753578	14.643418
19.386108	716.061725	14.648435
19.559196	709.615879	14.653453
19.822779	718.054431	14.658471
19.809523	706.055154	14.663488
19.801914	711.049026	14.668506
19.755529	711.731826	14.673523
20.062385	713.343893	14.678541
19.721652	716.392333	14.683559
19.946624	711.831842	14.688576
19.781272	711.501333	14.693594
19.395161	718.085077	14.698611
19.565340	721.529995	14.703629
19.850698	720.491394	14.708647
19.934104	715.754268	14.713664
19.690939	712.680928	14.718682
19.821932	705.777774	14.723699
20.170591	711.006160	14.728717
19.717571	714.466668	14.733735
20.334019	710.229850	14.738752
20.008305	707.668063	14.743770
19.965905	716.239763	14.748787
19.831730	713.345006	14.753805
20.044900	712.245133	14.758823
19.933068	709.668769	14.763840
19.985483	711.409065	14.768858
19.512784	713.512502	14.773875
19.867771	711.011320	14.778893
20.388339	727.734639	14.783911
20.545298	710.476354	14.788928
20.572834	712.684452	14.793946
19.903144	711.236910	14.798963
20.278944	706.542336	14.803981
20.231678	712.631175	14.808999
20.325985	702.593740	14.814016
20.064198	713.191127	14.819034
20.102484	706.971530	14.824051
20.214243	709.819683	14.829069
20.080795	725.402083	14.834087
20.499205	731.926053	14.839104
20.290547	724.984589	14.844122
20.505136	737.549163	14.849139
20.701297	724.819626	14.854157
20.422757	730.988889	14.859175
20.298739	716.138326	14.864192
20.220163	717.555163	14.869210
20.452480	731.521289	14.874227
20.742710	726.956882	14.879245
20.750593	737.398422	14.884263
20.760836	726.619905	14.889280
20.456234	718.693084	14.894298
19.880254	716.268338	14.899315
20.240675	724.331958	14.904333
20.085772	738.892092	14.909351
20.524078	732.625590	14.914368
20.327886	734.613123	14.919386
20.448646	733.388871	14.924403
20.603773	732.222351	14.929421
20.392729	746.983793	14.934439
20.920802	751.272049	14.939456
20.713084	754.880325	14.944474
20.918072	752.784492	14.949491
20.974472	749.771508	14.954509
20.771118	750.437878	14.959527
20.729590	753.193291	14.964544
20.923467	753.604918	14.969562
21.013145	751.539776	14.974579
21.107848	749.284498	14.979597
20.984823	746.589961	14.984615
21.196677	739.765644	14.989632
21.244000	735.188800	14.994650
20.906783	732.915990	14.999667
21.232514	728.926690	15.004685
20.596907	733.886418	15.009703
20.843087	728.271715	15.014720
21.098402	735.032679	15.019738
21.246491	741.299204	15.024755
21.071718	742.664842	15.029773
20.990658	753.764113	15.034791
20.973152	753.050676	15.039808
21.276759	756.664044	15.044826
21.154597	743.886539	15.049843
21.131345	749.949537	15.054861
21.079197	754.013122	15.059879
21.299801	758.835550	15.064896
21.284203	748.733258	15.069914
21.453651	754.286382	15.074931
21.829934	741.989362	15.079949
21.628304	747.562754	15.084967
21.445856	743.918160	15.089984
21.449592	738.224675	15.095002
21.049112	737.965719	15.100019
21.013761	734.367508	15.105037
21.184063	742.069603	15.110055
20.979036	743.080219	15.115072
21.847200	749.962919	15.120090
21.541902	750.711534	15.125107
21.442360	747.984915	15.130125
21.564498	753.649594	15.135143
21.320879	756.408268	15.140160
21.549319	745.128492	15.145178
21.517006	747.241829	15.150195
21.835032	754.163389	15.155213
21.547182	746.590538	15.160231
21.794950	752.803579	15.165248
21.747272	747.929191	15.170266
21.626015	759.056855	15.175283
21.801737	751.846872	15.180301
21.877886	751.125072	15.185319
21.641989	745.727907	15.190336
21.956519	743.356136	15.195354
21.742432	753.056133	15.200371
22.032748	751.966260	15.205389
21.702384	751.626890	15.210407
21.881043	762.761214	15.215424
21.772636	753.762218	15.220442
21.516667	756.576476	15.225459
21.608377	747.233702	15.230477
21.981557	765.359242	15.235495
22.004319	783.331419	15.240512
22.063674	777.193703	15.245530
21.931525	781.175153	15.250547
21.978398	781.142752	15.255565
22.031457	777.738965	15.260583
22.178905	780.789822	15.265600
22.481435	774.131166	15.270618
22.396587	788.734014	15.275635
22.380744	769.905900	15.280653
21.728103	755.564164	15.285671
22.212653	762.683699	15.290688
22.286983	775.885659	15.295706
21.932847	785.588682	15.300723
22.463727	778.269393	15.305741
22.372017	773.805842	15.310759
22.034850	779.574051	15.315776
22.268715	770.089072	15.320794
22.282233	779.119102	15.325811
22.585288	774.410661	15.330829
22.386817	771.952005	15.335847
22.199745	782.484077	15.340864
22.371690	770.398935	15.345882
22.509705	782.243387	15.350899
22.352570	771.904480	15.355917
22.460911	784.163839	15.360935
22.355159	778.209783	15.365952
22.487184	776.532481	15.370970
22.342050	776.050479	15.375987
22.426889	772.521792	15.381005
22.492249	775.806418	15.386023
22.494511	780.344324	15.391040
22.446914	769.735790	15.396058
22.398251	786.974388	15.401075
22.599808	800.102784	15.406093
22.689885	801.527916	15.411111
22.441608	800.314143	15.416128
22.685025	805.587449	15.421146
22.741884	803.584248	15.426163
22.771405	791.966377	15.431181
23.013700	792.840637	15.436199
22.877329	794.335963	15.441216
23.196138	794.125255	15.446234
23.129251	793.593122	15.451251
22.668222	797.414665	15.456269
23.049680	786.344419	15.461287
23.080467	796.410018	15.466304
22.999928	789.107627	15.471322
22.955069	793.166923	15.476339
23.026948	787.055644	15.481357
22.858691	790.171746	15.486375
22.942848	800.222674	15.491392
23.347095	790.294419	15.496410
23.179174	796.383257	15.501427
23.120497	788.430496	15.506445
22.987752	789.101584	15.511463
22.948161	795.268145	15.516480
22.968134	792.245081	15.521498
23.070186	793.081354	15.526515
23.094752	789.016150	15.531533
23.109829	798.999004	15.536551
23.252140	795.824228	15.541568
23.623963	801.882149	15.546586
23.249721	795.001316	15.551603
23.347551	801.708084	15.556621
23.175375	792.946279	15.561639
23.333250	804.503610	15.566656
23.420596	801.962297	15.571674
23.468004	811.362577	15.576691
23.307149	812.104342	15.581709
23.793677	812.274457	15.586727
23.497787	815.420030	15.591744
23.497411	808.303888	15.596762
23.361986	811.121358	15.601779
23.544916	809.215170	15.606797
23.906131	805.201358	15.611815
23.546767	814.425529	15.616832
23.767250	817.991973	15.621850
23.776508	806.396203	15.626867
23.837522	813.443262	15.631885
23.856037	811.193601	15.636903
23.659899	815.639525	15.641920
23.774114	815.293613	15.646938
23.999650	816.255707	15.651955
23.931352	818.759702	15.656973
23.968965	809.602098	15.661991
23.815622	816.322979	15.667008
23.633179	809.235363	15.672026
23.771085	811.012767	15.677043
23.777320	809.105860	15.682061
23.642935	809.199690	15.687079
23.890126	806.283036	15.692096
23.656685	810.327700	15.697114
23.742238	811.586284	15.702131
23.443344	823.524465	15.707149
24.350478	820.422357	15.712167
23.926305	838.606628	15.717184
24.000860	838.289020	15.722202
24.102795	832.286627	15.727219
24.133407	837.773166	15.732237
24.419324	838.631127	15.737255
24.328728	840.939801	15.742272
24.311890	834.817159	15.747290
24.242721	837.561136	15.752307
24.314920	836.382356	15.757325
24.308654	835.903841	15.762343
24.294842	843.874670	15.767360
24.670385	834.569433	15.772378
24.677745	840.056460	15.777395
24.077575	828.553005	15.782413
24.230910	827.762303	15.787431
24.403654	835.514550	15.792448
24.356063	832.606208	15.797466
24.459513	832.574410	15.802483
24.499702	836.696130	15.807501
24.367131	831.446853	15.812519
24.161798	832.848844	15.817536
24.273858	830.171111	15.822554
24.258624	833.269558	15.827571
24.704438	858.509679	15.832589
24.797303	854.146578	15.837607
24.921860	853.906344	15.842624
25.039665	854.525554	15.847642
25.116060	858.029375	15.852659
24.795480	838.327430	15.857677
24.918387	833.243253	15.862695
24.775614	823.321792	15.867712
24.469510	824.603871	15.872730
25.017728	836.197895	15.877747
24.634895	849.493628	15.882765
25.133766	842.128836	15.887783
24.713928	854.426817	15.892800
24.650904	849.810428	15.897818
24.985441	857.366920	15.902835
25.275944	852.698295	15.907853
25.325913	846.688260	15.912871
25.220560	849.150727	15.917888
25.191154	845.447420	15.922906
25.312726	842.818688	15.927923
25.266425	843.331065	15.932941
25.330015	828.510974	15.937959
24.911666	828.614580	15.942976
25.128717	826.406396	15.947994
25.409885	844.906197	15.953011
25.076034	844.030880	15.958029
25.121972	849.085829	15.963047
25.103811	848.823774	15.968064
25.245335	851.509495	15.973082
25.425596	840.802101	15.978099
25.284129	849.698659	15.983117
25.485017	838.240102	15.988135
25.208878	854.381463	15.993152
25.317399	846.566583	15.998170
25.044546	847.565741	16.003187
25.253805	854.939887	16.008205
25.577018	843.998653	16.013223
25.611485	856.351688	16.018240
25.715829	842.102719	16.023258
25.678848	845.835741	16.028275
25.450224	844.098173	16.033293
25.579157	842.178350	16.038311
25.280686	855.192625	16.043328
25.676500	856.995897	16.048346
26.089733	860.611046	16.053363
25.945543	871.095426	16.058381
25.684257	862.243405	16.063399
26.124321	863.844083	16.068416
25.661921	851.107186	16.073434
25.871997	851.920225	16.078451
25.495396	867.963727	16.083469
25.675143	861.283251	16.088487
25.608128	864.219401	16.093504
25.871203	865.974043	16.098522
26.138712	871.076334	16.103539
26.124145	870.056314	16.108557
26.169485	866.448590	16.113575
26.332269	870.977148	16.118592
26.416790	868.089127	16.123610
26.456566	866.820749	16.128627
25.894158	877.080322	16.133645
26.218643	877.957488	16.138663
26.448172	874.368241	16.143680
26.112565	878.286916	16.148698
26.248340	868.255514	16.153715
25.793629	881.287975	16.158733
26.311000	875.933697	16.163751
26.316236	882.882223	16.168768
26.068017	873.185541	16.173786
26.393345	876.662985	16.178803
26.383444	859.452791	16.183821
26.301139	865.537705	16.188839
26.392564	874.984771	16.193856
26.324100	873.745975	16.198874
26.633649	869.778114	16.203891
26.257024	871.080713	16.208909
26.443993	867.958888	16.213927
26.213379	869.986543	16.218944
26.615855	887.186112	16.223962
26.683256	889.176545	16.228979
26.881014	898.767911	16.233997
27.098201	880.859389	16.239015
26.768690	868.511917	16.244032
26.199349	876.348893	16.249050
26.802650	880.227759	16.254067
26.719758	886.413758	16.259085
26.821301	896.200081	16.264103
27.083096	897.087070	16.269120
26.870292	893.923734	16.274138
27.175993	892.724145	16.279155
26.985161	885.265423	16.284173
26.634436	872.056573	16.289191
26.871755	896.392132	16.294208
26.820340	892.345120	16.299226
27.003383	876.931911	16.304243
26.892967	884.589687	16.309261
26.822286	884.354795	16.314279
27.003027	890.048206	16.319296
26.980169	892.321026	16.324314
27.019135	887.960050	16.329331
27.132926	888.895475	16.334349
27.010649	898.628503	16.339367
27.247128	892.500867	16.344384
27.015819	892.486804	16.349402
27.392315	887.713178	16.354419
27.165219	892.987645	16.359437
27.226150	884.343908	16.364455
27.637989	894.823235	16.369472
27.118850	902.333616	16.374490
27.138154	903.006132	16.379507
27.592223	907.678411	16.384525
27.577064	908.911755	16.389543
27.785390	915.800073	16.394560
27.411963	917.774369	16.399578
27.619265	912.351895	16.404595
27.414198	910.001551	16.409613
27.767438	915.093578	16.414631
27.922174	907.432380	16.419648
27.525264	912.010770	16.424666
27.840651	898.085301	16.429683
27.716368	904.757480	16.434701
27.715740	910.362547	16.439719
28.089450	903.875730	16.444736
28.002593	912.634373	16.449754
27.940816	893.305234	16.454771
28.104948	893.213434	16.459789
27.723385	879.311969	16.464807
27.947488	886.365063	16.469824
27.794325	895.932513	16.474842
27.833416	902.250887	16.479859
28.094779	898.221141	16.484877
28.113238	903.583371	16.489895
28.211555	905.250221	16.494912
27.822278	908.918532	16.499930
28.395819	909.106574	16.504947
28.343305	908.540628	16.509965
28.095555	904.117272	16.514983
28.280299	901.163049	16.520000
27.739386	908.496961	16.525018
28.287861	903.522814	16.530035
28.326273	901.557207	16.535053
28.305840	899.408313	16.540071
28.595517	905.614842	16.545088
28.287913	911.384772	16.550106
28.273624	897.163814	16.555123
28.384119	899.977482	16.560141
28.234828	902.014490	16.565159
28.522954	902.537588	16.570176
28.565115	913.860653	16.575194
28.373834	907.724291	16.580211
28.355354	913.458390	16.585229
28.128799	914.649116	16.590247
28.314434	913.127505	16.595264
28.051172	919.796218	16.600282
28.469194	915.555729	16.605299
28.745116	924.412174	16.610317
28.676684	942.824839	16.615335
29.001120	934.594234	16.620352
28.844770	931.889111	16.625370
28.633810	928.248947	16.630387
28.525710	934.700848	16.635405
28.768780	935.540280	16.640423
29.031819	937.373831	16.645440
28.706984	932.599622	16.650458
28.529289	938.939351	16.655475
29.171274	932.328439	16.660493
29.100592	937.666776	16.665511
29.279986	933.198578	16.670528
28.976501	935.442788	16.675546
28.866138	932.919811	16.680563
28.966185	935.198628	16.685581
29.213182	938.041408	16.690599
29.093346	934.961330	16.695616
28.698660	941.944136	16.700634
28.908219	934.580454	16.705651
28.964567	937.462573	16.710669
29.072434	948.746962	16.715687
29.361553	947.499474	16.720704
29.506548	953.536181	16.725722
29.338266	956.693342	16.730739
29.381650	960.000380	16.735757
29.522787	959.394624	16.740775
30.044865	961.146566	16.745792
29.437323	944.424408	16.750810
29.153681	936.986518	16.755827
29.470657	945.176969	16.760845
29.465656	951.596944	16.765863
29.788348	939.355523	16.770880
29.703839	951.345407	16.775898
29.833948	944.934612	16.780915
29.886281	944.487939	16.785933
29.829012	945.718416	16.790951
29.747091	937.314788	16.795968
29.550739	943.676377	16.800986
29.829305	939.533472	16.806003
29.783630	942.220134	16.811021
29.851335	945.318229	16.816039
30.255527	942.171824	16.821056
29.872446	943.084114	16.826074
29.939537	950.840341	16.831091
29.877404	945.081370	16.836109
29.660603	945.191268	16.841127
29.917066	944.321287	16.846144
29.524846	951.726595	16.851162
29.905556	948.391361	16.856179
29.960754	953.145082	16.861197
29.636033	951.353131	16.866215
30.171552	958.799281	16.871232
30.243311	972.863338	16.876250
30.626861	973.068525	16.881267
30.568156	956.165690	16.886285
30.469870	951.131915	16.891303
30.590410	941.143885	16.896320
30.217811	947.239596	16.901338
30.373890	940.111511	16.906355
30.341130	938.400051	16.911373
30.017179	950.496879	16.916391
30.408816	948.242391	16.921408
30.322759	962.684622	16.926426
30.662146	972.348513	16.931443
30.880309	964.282871	16.936461
30.335324	967.319172	16.941479
30.549036	975.440607	16.946496
30.702137	975.984864	16.951514
30.612164	970.612104	16.956531
30.651987	970.110585	16.961549
30.421712	966.735375	16.966567
30.782350	966.899970	16.971584
30.665911	973.312166	16.976602
30.290713	980.960975	16.981619
30.565840	976.196897	16.986637
30.405804	972.075366	16.991655
30.741850	978.991035	16.996672
31.045508	993.245996	17.001690
30.630285	996.719571	17.006707
31.245159	983.693869	17.011725
31.030337	991.415388	17.016743
31.480004	995.479300	17.021760
31.427391	991.467168	17.026778
31.344181	984.354466	17.031795
31.277151	977.030947	17.036813
31.145979	975.186577	17.041831
31.198076	973.925729	17.046848
31.329107	983.035282	17.051866
31.419879	984.362489	17.056883
31.328310	976.395863	17.061901
31.537860	980.844538	17.066919
31.373943	974.410371	17.071936
31.001618	970.738675	17.076954
31.321745	976.703768	17.081971
31.727394	980.291728	17.086989
31.694045	979.972089	17.092007
31.830055	986.622451	17.097024
31.333346	988.685500	17.102042
31.174494	984.336559	17.107059
31.542268	980.520500	17.112077
31.588740	988.368338	17.117095
31.883799	981.676062	17.122112
31.736386	982.526182	17.127130
31.308110	995.813365	17.132147
31.889579	982.306896	17.137165
31.790538	986.923844	17.142183
31.923340	991.204662	17.147200
31.762405	991.450976	17.152218
31.617305	987.674246	17.157235
32.036714	976.175053	17.162253
31.919080	989.902718	17.167271
31.663216	986.481019	17.172288
32.114543	996.442971	17.177306
32.156122	1004.430441	17.182323
32.335650	997.772039	17.187341
32.213010	995.579186	17.192359
31.976363	990.586013	17.197376
32.196564	991.949748	17.202394
31.811239	1002.273166	17.207411
32.265007	1005.424394	17.212429
32.363475	1016.650338	17.217447
32.190928	1018.687847	17.222464
32.306173	1014.791424	17.227482
32.258658	1010.014770	17.232499
32.662911	1013.827021	17.237517
32.364162	1007.230928	17.242535
32.396346	1004.862335	17.247552
32.337499	1010.747959	17.252570
32.372345	1007.984466	17.257587
32.932546	1005.514208	17.262605
32.305482	1008.102620	17.267623
32.098424	1011.010242	17.272640
32.111490	1009.373648	17.277658
32.453386	1027.311848	17.282675
33.010455	1026.606208	17.287693
32.912231	1025.517234	17.292711
32.983257	1025.190709	17.297728
32.918500	1013.104618	17.302746
32.792076	1016.766482	17.307763
32.518391	1013.622130	17.312781
32.825138	1023.420554	17.317799
33.002208	1026.179629	17.322816
33.431994	1024.364131	17.327834
33.090868	1031.366984	17.332851
33.152303	1025.790601	17.337869
33.339652	1030.066037	17.342887
33.111559	1017.819339	17.347904
32.996830	1014.378678	17.352922
33.071039	1025.261283	17.357939
33.338741	1021.852222	17.362957
32.927201	1023.734669	17.367975
32.752115	1026.135501	17.372992
33.457475	1032.106529	17.378010
33.316459	1027.660107	17.383027
32.912730	1018.637818	17.388045
33.006497	1025.550438	17.393063
33.307184	1024.752421	17.398080
33.227920	1030.107910	17.403098
33.481989	1049.893452	17.408115
33.985563	1046.668341	17.413133
33.803505	1051.437170	17.418151
33.740467	1036.340095	17.423168
33.610366	1024.851226	17.428186
33.446276	1029.689820	17.433203
33.815114	1033.611767	17.438221
33.595951	1042.725725	17.443239
33.554443	1038.361541	17.448256
33.558925	1041.677846	17.453274
33.579836	1044.496105	17.458291
33.933040	1032.107826	17.463309
33.856748	1039.233293	17.468327
33.800519	1040.094376	17.473344
33.932430	1035.229642	17.478362
33.896373	1037.324665	17.483379
34.116963	1042.200823	17.488397
33.947086	1039.968027	17.493415
34.103676	1041.467966	17.498432
34.261189	1036.621312	17.503450
33.802355	1041.790117	17.508467
34.376656	1041.990665	17.513485
34.440946	1042.706632	17.518503
34.132467	1045.279848	17.523520
34.346220	1048.399260	17.528538
34.220702	1065.249373	17.533555
34.486776	1062.957738	17.538573
34.803913	1072.126542	17.543591
34.531405	1055.692621	17.548608
34.505964	1042.770357	17.553626
34.397713	1046.517744	17.558643
34.499016	1049.077250	17.563661
34.679002	1055.436720	17.568679
34.823054	1057.367824	17.573696
34.682384	1034.866619	17.578714
34.325784	1042.168551	17.583731
34.591681	1056.517844	17.588749
34.825869	1061.202524	17.593767
34.591614	1058.490653	17.598784
35.136222	1049.928847	17.603802
34.558820	1068.695947	17.608819
34.782937	1060.518873	17.613837
34.949909	1057.116120	17.618855
35.017330	1063.142928	17.623872
35.131915	1067.215175	17.628890
34.983893	1071.634687	17.633907
35.013626	1057.450885	17.638925
35.131772	1054.828971	17.643943
35.086885	1063.653697	17.648960
35.276891	1056.832682	17.653978
35.213728	1059.130774	17.658995
35.288153	1052.864368	17.664013
35.161774	1057.933751	17.669031
34.877294	1058.369840	17.674048
35.231216	1060.839275	17.679066
34.907809	1054.259651	17.684083
34.904316	1067.095316	17.689101
35.051327	1074.466682	17.694119
35.424217	1078.220744	17.699136
35.637697	1081.674727	17.704154
35.454357	1080.217225	17.709171
35.258036	1086.077075	17.714189
35.612678	1084.535283	17.719207
35.639767	1083.357243	17.724224
35.924764	1082.656357	17.729242
35.617351	1093.595640	17.734259
35.790248	1079.843837	17.739277
35.897412	1073.038951	17.744295
35.470786	1081.936119	17.749312
35.948556	1075.249896	17.754330
35.749400	1070.490673	17.759347
35.615218	1078.947537	17.764365
35.779359	1086.994738	17.769383
35.670305	1095.132084	17.774400
36.172971	1095.018802	17.779418
36.197923	1099.616352	17.784435
36.085766	1105.387281	17.789453
35.905024	1101.303679	17.794471
35.987368	1104.276428	17.799488
36.640669	1097.584785	17.804506
36.275045	1095.922307	17.809523
36.406614	1085.743116	17.814541
36.478001	1083.412553	17.819559
36.396368	1097.358727	17.824576
36.654715	1084.164746	17.829594
36.744962	1093.192381	17.834611
36.559560	1086.856216	17.839629
36.482331	1086.423527	17.844647
36.475764	1092.976345	17.849664
36.469511	1089.042136	17.854682
36.480116	1086.755810	17.859699
36.107316	1086.157987	17.864717
36.313729	1079.530057	17.869735
36.268875	1079.284804	17.874752
36.616079	1087.480053	17.879770
36.821046	1101.532808	17.884787
36.824971	1110.034321	17.889805
36.918729	1100.037776	17.894823
36.927389	1106.354678	17.899840
37.171721	1110.690635	17.904858
37.133210	1108.049075	17.909875
37.184901	1107.602499	17.914893
37.038535	1099.918965	17.919911
36.991650	1105.023244	17.924928
37.178951	1104.044168	17.929946
37.169055	1101.824169	17.934963
37.339000	1102.766587	17.939981
37.047874	1101.272321	17.944999
37.002240	1102.374750	17.950016
37.182191	1098.092622	17.955034
37.178697	1109.214676	17.960051
37.331709	1103.945820	17.965069
37.420584	1101.356888	17.970087
37.322328	1103.543717	17.975104
37.362037	1105.630033	17.980122
36.731896	1108.985819	17.985139
37.210677	1103.710105	17.990157
37.387929	1114.043276	17.995175
37.444627	1125.872295	18.000192
37.567249	1136.589588	18.005210
37.707014	1128.239502	18.010227
37.774061	1136.301938	18.015245
37.631496	1130.019008	18.020263
38.103836	1124.984144	18.025280
37.861864	1129.983294	18.030298
37.896605	1123.574754	18.035315
38.256323	1122.606533	18.040333
38.234531	1129.818174	18.045351
38.100181	1130.678878	18.050368
38.356177	1122.834460	18.055386
37.687251	1120.597791	18.060403
37.550787	1129.544198	18.065421
38.070765	1125.464414	18.070439
37.882776	1125.370978	18.075456
37.998470	1122.083547	18.080474
38.119546	1123.677423	18.085491
37.574431	1135.076861	18.090509
38.205529	1141.725454	18.095527
37.913332	1151.800831	18.100544
38.154425	1145.255808	18.105562
38.485398	1148.842879	18.110579
38.610544	1154.513526	18.115597
38.621264	1151.352992	18.120615
38.552056	1161.238799	18.125632
38.508229	1159.582702	18.130650
38.827678	1147.852901	18.135667
38.442337	1155.825274	18.140685
38.536925	1141.814286	18.145703
38.544159	1147.124699	18.150720
38.697461	1164.638139	18.155738
39.207144	1167.010599	18.160755
39.236457	1162.455403	18.165773
39.035210	1154.155578	18.170791
38.786778	1145.282467	18.175808
39.097721	1148.850584	18.180826
39.136898	1165.719170	18.185843
39.186898	1159.226174	18.190861
39.155866	1139.910885	18.195879
39.121633	1160.215104	18.200896
39.486712	1152.602897	18.205914
39.528333	1152.151586	18.210931
39.132327	1143.945398	18.215949
39.367931	1136.593331	18.220967
39.041855	1133.195228	18.225984
39.329954	1144.732377	18.231002
39.742541	1153.551745	18.236019
39.511712	1156.191708	18.241037
39.674910	1150.271130	18.246055
39.550035	1149.754384	18.251072
39.388384	1141.347373	18.256090
39.604738	1153.422801	18.261107
39.367551	1154.204942	18.266125
39.826192	1157.503761	18.271143
39.670499	1164.613315	18.276160
39.677624	1161.140910	18.281178
39.593187	1158.834751	18.286195
39.511741	1159.759753	18.291213
39.998870	1158.377082	18.296231
39.885402	1151.549929	18.301248
40.009820	1157.820310	18.306266
39.752012	1158.694047	18.311283
39.720656	1157.600900	18.316301
39.879467	1162.382626	18.321319
39.852620	1159.559345	18.326336
39.909985	1162.769554	18.331354
40.162285	1177.966853	18.336371
39.489620	1193.911863	18.341389
40.188869	1186.218883	18.346407
40.307744	1187.074630	18.351424
40.242466	1191.670561	18.356442
40.434057	1182.974648	18.361459
40.292853	1190.681562	18.366477
40.437486	1185.672779	18.371495
40.789476	1187.309378	18.376512
40.383220	1184.166832	18.381530
40.306780	1182.367515	18.386547
40.583712	1188.595076	18.391565
40.474151	1199.456085	18.396583
40.609298	1210.632222	18.401600
40.802547	1212.123276	18.406618
41.238851	1199.232698	18.411635
40.932229	1212.216950	18.416653
40.887354	1205.154960	18.421671
40.878202	1204.661108	18.426688
40.934126	1209.253833	18.431706
41.032704	1210.409416	18.436723
40.676823	1202.105393	18.441741
41.190883	1205.376603	18.446759
41.517792	1197.596784	18.451776
41.191662	1201.801230	18.456794
41.575385	1191.197452	18.461811
41.230445	1205.803521	18.466829
41.305171	1198.725951	18.471847
40.996959	1206.957670	18.476864
41.152061	1204.800172	18.481882
41.395724	1191.624192	18.486899
41.031579	1207.347301	18.491917
41.711141	1195.318043	18.496935
41.211001	1194.976860	18.501952
41.415956	1196.204139	18.506970
41.835589	1190.297021	18.511987
41.329005	1201.128715	18.517005
41.627016	1199.706243	18.522023
41.758384	1207.727074	18.527040
41.687861	1225.812146	18.532058
42.221007	1213.420796	18.537075
41.938320	1221.396050	18.542093
42.225575	1209.339883	18.547111
42.284611	1197.420470	18.552128
41.507462	1195.992877	18.557146
42.011879	1189.621182	18.562163
41.876670	1213.412765	18.567181
42.049472	1209.721883	18.572199
41.935292	1211.816543	18.577216
41.859161	1227.829070	18.582234
41.939369	1213.002901	18.587251
42.018386	1221.562132	18.592269
42.305839	1215.325410	18.597287
42.356337	1224.125803	18.602304
42.412825	1208.732136	18.607322
42.388864	1203.778165	18.612339
42.274637	1217.110984	18.617357
42.112519	1215.205164	18.622375
42.458097	1222.813732	18.627392
42.430085	1226.176188	18.632410
42.489752	1229.714262	18.637427
42.814672	1246.276215	18.642445
42.579257	1234.292454	18.647463
42.864022	1231.502393	18.652480
42.672472	1235.950857	18.657498
42.783455	1229.659726	18.662515
42.515998	1242.536874	18.667533
42.532249	1227.458774	18.672551
42.723816	1234.674898	18.677568
42.698428	1240.504862	18.682586
43.619370	1247.253254	18.687603
43.310445	1244.474155	18.692621
43.388515	1235.638208	18.697639
43.465984	1238.507599	18.702656
43.463059	1240.348138	18.707674
43.353158	1229.597609	18.712691
43.548731	1225.372965	18.717709
43.512200	1226.698044	18.722727
43.239569	1229.133122	18.727744
43.386629	1233.847278	18.732762
43.772882	1231.694588	18.737779
43.793501	1230.170403	18.742797
43.421479	1226.703738	18.747815
43.433891	1234.733752	18.752832
43.256606	1238.299485	18.757850
43.214635	1233.786998	18.762867
43.512970	1255.513025	18.767885
43.466354	1255.788771	18.772903
43.833250	1255.488471	18.777920
44.103135	1253.742187	18.782938
44.112201	1252.390229	18.787955
44.221975	1262.235425	18.792973
44.013032	1245.740875	18.797991
43.802928	1249.144489	18.803008
43.903893	1243.173669	18.808026
44.095656	1254.287312	18.813043
43.909039	1260.868401	18.818061
43.854026	1253.934217	18.823079
44.400534	1268.413290	18.828096
44.573465	1273.682000	18.833114
44.598583	1268.947547	18.838131
44.511891	1271.789013	18.843149
44.293033	1264.836313	18.848167
44.798050	1261.778201	18.853184
44.686975	1276.950465	18.858202
45.065609	1267.322616	18.863219
44.582060	1253.714556	18.868237
44.792095	1257.434209	18.873255
44.775368	1257.515918	18.878272
44.456019	1259.936227	18.883290
44.677746	1264.275764	18.888307
44.762324	1272.218746	18.893325
44.738862	1272.695998	18.898343
44.771167	1266.660186	18.903360
44.709602	1268.326873	18.908378
44.987273	1264.086201	18.913395
45.130638	1264.404766	18.918413
44.854130	1266.445968	18.923431
45.139891	1271.100532	18.928448
45.119793	1275.995529	18.933466
44.961746	1267.871925	18.938483
45.089875	1270.585056	18.943501
45.060551	1269.927100	18.948519
45.368704	1275.023140	18.953536
45.149654	1291.386331	18.958554
45.658680	1296.176340	18.963571
45.707321	1292.833109	18.968589
45.766424	1293.641420	18.973607
45.927318	1283.552200	18.978624
45.299313	1289.012676	18.983642
45.793284	1279.546637	18.988659
45.821589	1285.582805	18.993677
45.640398	1281.095275	18.998695
45.440586	1278.699876	19.003712
45.772333	1289.334002	19.008730
45.778601	1289.506784	19.013747
46.088741	1284.200634	19.018765
45.617658	1281.020888	19.023783
45.867641	1273.003772	19.028800
46.070533	1279.653233	19.033818
46.404937	1284.975544	19.038835
46.381604	1278.121597	19.043853
45.916084	1279.245640	19.048871
46.544405	1274.353560	19.053888
46.467654	1277.673168	19.058906
46.050641	1284.233557	19.063923
46.369729	1283.751393	19.068941
46.742833	1301.479847	19.073959
46.582442	1296.540914	19.078976
46.288986	1297.107807	19.083994
46.481599	1303.739953	19.089011
46.914226	1298.228408	19.094029
46.392141	1307.888596	19.099047
46.432391	1296.464383	19.104064
46.947028	1303.112348	19.109082
46.750648	1299.851688	19.114099
47.047535	1300.266125	19.119117
47.295439	1299.195490	19.124135
46.848136	1296.460155	19.129152
46.702630	1301.403211	19.134170
46.598408	1306.724822	19.139187
47.123343	1296.206159	19.144205
46.802207	1302.622141	19.149223
47.029590	1309.801126	19.154240
47.056210	1324.137629	19.159258
47.450733	1328.607905	19.164275
47.417119	1321.954374	19.169293
47.392790	1317.735758	19.174311
47.524922	1323.806166	19.179328
47.549060	1315.458329	19.184346
47.428059	1319.614883	19.189363
47.311591	1318.134260	19.194381
47.210330	1323.534310	19.199399
47.485100	1313.099015	19.204416
47.299175	1323.006355	19.209434
47.782727	1335.245177	19.214451
48.044658	1344.489047	19.219469
48.054224	1345.137857	19.224487
48.235638	1344.166003	19.229504
48.267347	1330.963166	19.234522
48.172664	1321.920705	19.239539
48.056543	1310.101246	19.244557
48.017774	1313.755748	19.249575
48.046042	1307.007318	19.254592
48.185423	1326.659653	19.259610
48.164808	1340.088354	19.264627
48.605590	1333.919090	19.269645
48.247080	1349.493113	19.274663
48.356643	1339.402435	19.279680
48.495998	1342.388383	19.284698
48.635642	1335.578309	19.289715
48.807382	1337.022250	19.294733
48.760733	1328.360438	19.299751
48.412581	1312.070680	19.304768
48.563410	1327.473361	19.309786
48.615259	1331.647019	19.314803
48.278847	1328.742821	19.319821
48.396946	1335.446615	19.324839
48.431559	1326.510131	19.329856
48.362322	1330.232528	19.334874
48.395844	1343.838949	19.339891
48.737615	1357.368681	19.344909
48.563833	1359.277029	19.349927
48.965746	1354.761240	19.354944
49.047598	1360.012686	19.359962
48.857025	1358.638348	19.364979
48.997629	1361.696690	19.369997
49.155970	1375.151029	19.375015
49.414939	1378.534825	19.380032
49.714368	1381.587222	19.385050
49.439241	1379.566541	19.390067
49.901212	1369.392229	19.395085
49.699214	1376.932016	19.400103
49.603033	1375.170488	19.405120
49.816374	1378.290024	19.410138
49.702275	1382.571748	19.415155
50.001736	1375.701904	19.420173
49.862889	1367.108169	19.425191
50.082342	1364.006416	19.430208
50.107504	1356.396886	19.435226
49.768945	1357.352714	19.440243
49.825613	1357.034745	19.445261
49.741195	1363.252708	19.450279
49.800740	1367.680799	19.455296
49.958337	1371.907329	19.460314
49.999607	1369.161708	19.465331
50.471100	1365.667003	19.470349
50.339332	1373.135822	19.475367
50.069839	1367.560687	19.480384
49.959585	1361.578737	19.485402
49.922160	1368.761364	19.490419
50.406746	1372.087719	19.495437
50.363895	1380.905970	19.500455
50.588596	1376.310640	19.505472
50.865453	1375.642579	19.510490
50.631056	1377.462591	19.515507
50.950770	1370.599044	19.520525
50.858889	1385.528542	19.525543
50.779057	1377.645107	19.530560
50.815897	1385.261091	19.535578
51.077487	1380.189746	19.540595
51.171952	1376.507947	19.545613
51.216709	1384.580300	19.550631
51.126694	1378.200682	19.555648
51.220319	1387.130104	19.560666
51.128867	1377.837790	19.565683
51.291363	1373.981224	19.570701
51.045604	1375.591570	19.575719
51.354153	1384.414730	19.580736
51.220383	1373.809870	19.585754
51.162323	1381.538555	19.590771
51.320509	1388.876742	19.595789
51.462474	1399.291350	19.600807
51.637677	1403.672925	19.605824
51.642275	1402.255381	19.610842
51.432368	1407.606204	19.615859
51.652938	1390.271021	19.620877
51.331694	1407.818024	19.625895
51.125294	1398.868770	19.630912
51.685686	1401.908687	19.635930
51.586083	1421.778458	19.640947
51.954953	1423.560765	19.645965
51.962955	1432.052325	19.650983
52.290374	1431.218543	19.656000
52.122568	1425.024674	19.661018
52.149559	1434.763011	19.666035
52.422971	1429.844440	19.671053
52.588279	1431.942676	19.676071
52.498246	1430.098124	19.681088
52.761645	1415.198903	19.686106
52.740837	1426.869844	19.691123
52.519689	1430.909565	19.696141
52.698845	1434.245914	19.701159
52.523844	1430.013007	19.706176
52.944095	1420.129238	19.711194
52.566232	1430.880940	19.716211
52.731657	1422.242662	19.721229
52.583884	1421.423370	19.726247
52.489986	1425.594638	19.731264
52.975680	1422.214466	19.736282
52.914071	1426.753076	19.741299
53.144568	1429.860464	19.746317
53.165011	1425.903063	19.751335
52.754229	1424.260251	19.756352
53.061538	1420.352584	19.761370
53.027841	1443.655179	19.766387
53.558674	1452.023806	19.771405
53.348821	1451.046974	19.776423
53.369186	1451.318540	19.781440
53.335757	1444.936345	19.786458
53.555356	1445.407079	19.791475
53.755292	1447.910162	19.796493
53.517490	1452.246000	19.801511
53.411267	1438.843779	19.806528
53.693045	1443.988183	19.811546
53.293109	1451.300227	19.816563
53.871065	1437.872866	19.821581
53.813094	1443.493397	19.826599
53.811108	1459.529230	19.831616
53.985008	1464.807312	19.836634
54.011154	1476.022785	19.841651
54.248694	1471.049861	19.846669
53.911555	1468.723291	19.851687
54.136217	1462.499478	19.856704
54.337168	1460.830249	19.861722
53.886016	1462.759973	19.866739
54.495115	1468.711518	19.871757
54.475687	1461.976814	19.876775
54.570667	1462.839474	19.881792
54.582889	1467.180326	19.886810
54.135515	1465.410693	19.891827
54.536796	1465.180747	19.896845
54.750311	1475.678868	19.901863
54.918200	1486.335629	19.906880
54.929047	1470.705879	19.911898
54.638904	1484.555630	19.916915
55.030238	1488.360541	19.921933
55.062342	1484.660088	19.926951
55.158111	1492.304755	19.931968
55.591644	1485.233975	19.936986
55.770732	1481.210678	19.942003
55.036575	1460.351490	19.947021
54.660701	1459.189221	19.952039
55.054904	1477.832924	19.957056
55.282509	1474.726719	19.962074
55.300573	1477.242523	19.967091
55.377285	1475.848389	19.972109
55.624903	1489.090003	19.977127
55.088806	1483.215759	19.982144
55.474906	1482.701000	19.987162
55.192540	1484.424393	19.992179
55.287932	1481.679744	19.997197
55.826093	1492.553063	20.002215
55.489715	1504.131479	20.007232
55.847453	1496.040574	20.012250
55.734648	1505.444230	20.017267
55.903153	1504.152483	20.022285
56.204183	1506.380948	20.027303
55.706920	1499.998818	20.032320
56.033665	1495.166553	20.037338
56.274086	1502.226803	20.042355
56.044737	1497.153445	20.047373
56.147466	1511.885292	20.052391
55.875909	1527.998137	20.057408
56.207089	1525.226007	20.062426
55.881027	1526.460765	20.067443
56.241882	1530.355671	20.072461
56.732275	1531.099576	20.077479
56.732381	1543.597333	20.082496
56.756702	1535.097879	20.087514
56.518773	1536.037949	20.092531
56.849784	1549.039313	20.097549
57.003981	1545.717368	20.102567
56.935748	1542.493393	20.107584
56.903690	1548.157236	20.112602
57.388268	1544.887675	20.117619
57.249806	1544.944274	20.122637
57.598473	1538.710473	20.127655
57.274408	1546.878556	20.132672
57.826969	1537.750358	20.137690
57.314931	1540.333444	20.142707
57.309161	1539.719127	20.147725
57.667495	1533.442786	20.152743
57.580520	1545.840573	20.157760
57.773949	1540.145515	20.162778
57.513449	1536.926417	20.167795
57.704127	1540.592356	20.172813
57.834832	1532.382363	20.177831
57.396703	1541.903283	20.182848
57.724506	1532.602009	20.187866
57.404754	1529.998138	20.192883
57.512356	1539.916416	20.197901
58.274213	1550.527494	20.202919
58.070314	1563.353887	20.207936
58.204379	1567.072885	20.212954
58.234452	1567.005243	20.217971
58.022692	1579.694017	20.222989
58.285572	1572.277536	20.228007
57.766339	1561.597251	20.233024
58.175063	1565.787638	20.238042
58.233089	1568.972568	20.243059
58.147627	1583.487794	20.248077
58.384761	1591.126136	20.253095
58.565671	1601.253879	20.258112
58.760521	1592.503607	20.263130
58.713124	1594.120764	20.268147
58.682194	1591.310679	20.273165
59.011409	1592.051436	20.278183
58.604015	1593.251602	20.283200
58.690914	1589.062835	20.288218
58.791109	1597.505313	20.293235
58.999522	1607.713962	20.298253
59.562777	1603.144430	20.303271
59.421468	1611.249192	20.308288
59.606448	1606.379145	20.313306
59.481102	1603.350309	20.318323
59.755033	1605.557785	20.323341
59.752762	1609.519070	20.328359
59.346155	1599.070438	20.333376
59.360091	1606.841591	20.338394
59.688613	1596.536573	20.343411
59.581106	1599.627517	20.348429
59.794868	1609.428210	20.353447
59.618094	1613.012872	20.358464
59.659792	1600.199612	20.363482
59.693065	1597.590916	20.368499
59.787352	1599.201656	20.373517
59.691970	1594.116748	20.378535
59.610233	1618.973521	20.383552
60.077334	1618.733261	20.388570
60.296010	1615.063513	20.393587
60.079668	1625.979383	20.398605
60.356586	1624.358201	20.403623
60.299523	1628.801470	20.408640
60.631267	1621.273189	20.413658
60.555619	1622.588646	20.418675
60.585071	1626.551277	20.423693
60.678187	1618.930988	20.428711
60.641063	1630.651958	20.433728
60.972948	1632.487421	20.438746
61.154530	1641.062343	20.443763
61.320840	1639.455333	20.448781
61.367364	1626.849592	20.453799
61.205487	1625.931508	20.458816
61.211261	1626.662979	20.463834
60.925408	1608.766267	20.468851
60.965327	1620.086975	20.473869
61.196250	1626.006301	20.478887
61.196337	1637.468968	20.483904
61.281724	1643.164936	20.488922
61.617941	1643.626872	20.493939
61.388736	1644.682352	20.498957
61.542545	1641.928526	20.503975
61.510774	1634.798038	20.508992
61.426078	1635.562619	20.514010
61.609713	1637.029968	20.519027
61.413906	1657.672508	20.524045
61.911784	1661.476544	20.529063
61.761329	1661.292011	20.534080
62.348042	1664.264732	20.539098
62.516759	1659.346723	20.544115
62.029801	1666.618835	20.549133
62.453822	1658.880410	20.554151
62.222464	1659.740558	20.559168
62.389063	1655.413049	20.564186
62.395944	1658.647037	20.569203
61.971832	1659.404833	20.574221
62.287134	1651.756032	20.579239
62.439705	1669.696139	20.584256
62.522818	1666.009748	20.589274
62.329671	1667.397270	20.594291
62.415654	1675.974563	20.599309
62.634499	1679.901220	20.604327
62.411352	1672.699710	20.609344
62.476895	1669.855561	20.614362
62.891356	1681.237553	20.619379
62.682217	1691.461175	20.624397
62.868859	1688.632766	20.629415
63.159052	1697.335874	20.634432
62.866286	1689.829665	20.639450
63.091048	1693.928978	20.644467
62.957711	1690.156567	20.649485
63.498301	1704.573804	20.654503
63.282144	1713.826494	20.659520
63.533051	1721.153447	20.664538
63.823855	1715.777612	20.669555
63.527250	1717.875664	20.674573
63.856936	1716.400850	20.679591
63.788465	1715.578587	20.684608
63.858254	1709.817635	20.689626
64.089345	1711.763577	20.694643
63.952759	1713.846026	20.699661
64.301415	1710.446244	20.704679
64.541357	1711.838503	20.709696
64.210879	1712.016709	20.714714
64.194164	1714.856750	20.719731
64.072470	1712.449052	20.724749
64.516303	1699.818883	20.729767
64.230866	1708.302897	20.734784
64.186068	1715.007108	20.739802
64.490845	1711.696256	20.744819
64.599051	1724.271882	20.749837
64.703128	1731.602908	20.754855
64.681103	1725.556517	20.759872
64.835783	1727.710104	20.764890
65.075747	1735.704691	20.769907
64.789615	1734.215899	20.774925
64.889441	1726.468274	20.779943
65.091519	1727.926430	20.784960
65.336991	1728.336311	20.789978
65.168160	1720.741240	20.794995
64.843504	1725.134935	20.800013
65.519649	1731.246488	20.805031
65.649539	1734.966175	20.810048
65.661759	1742.311597	20.815066
65.727991	1733.805482	20.820083
65.564633	1731.341190	20.825101
65.996612	1736.853490	20.830119
65.912565	1746.388474	20.835136
65.822820	1746.958179	20.840154
66.105783	1743.338296	20.845171
66.032160	1749.816649	20.850189
66.066063	1747.021629	20.855207
66.323691	1741.770912	20.860224
66.248349	1737.326647	20.865242
66.275796	1739.727401	20.870259
66.117278	1741.084255	20.875277
65.946792	1744.301863	20.880295
66.219433	1736.246275	20.885312
66.313577	1741.366512	20.890330
66.660958	1735.593620	20.895347
66.460293	1742.792504	20.900365
66.161888	1742.694271	20.905383
66.740964	1752.179015	20.910400
66.761658	1760.154315	20.915418
66.965675	1765.667624	20.920435
66.947146	1768.062962	20.925453
66.895862	1764.375515	20.930471
67.281815	1763.343189	20.935488
67.107670	1763.799878	20.940506
66.845658	1759.722545	20.945523
67.188248	1760.104586	20.950541
67.196289	1760.589539	20.955559
67.331197	1766.277788	20.960576
67.192577	1776.282113	20.965594
67.659288	1778.573023	20.970611
67.474751	1792.526394	20.975629
67.540033	1792.137635	20.980647
67.959278	1792.687560	20.985664
68.023147	1787.836438	20.990682
68.051222	1779.121673	20.995699
67.896003	1786.954122	21.000717
67.530998	1793.156231	21.005735
68.076701	1784.082635	21.010752
67.804484	1790.551089	21.015770
68.041409	1784.483044	21.020787
68.050480	1783.336184	21.025805
68.147573	1797.349582	21.030823
68.456288	1801.394738	21.035840
68.535369	1804.273436	21.040858
68.608146	1796.397466	21.045875
68.580843	1810.982665	21.050893
68.670612	1812.849768	21.055911
68.780642	1805.277247	21.060928
68.620824	1810.945409	21.065946
68.852989	1806.254120	21.070963
68.879688	1790.643699	21.075981
68.798405	1798.508754	21.080999
68.965118	1800.824577	21.086016
68.698910	1802.132031	21.091034
69.143750	1810.659478	21.096051
69.041855	1816.233355	21.101069
69.120672	1820.286130	21.106087
69.321293	1822.950116	21.111104
69.308780	1822.314753	21.116122
69.357020	1809.497162	21.121139
69.451421	1821.607931	21.126157
69.604616	1844.528294	21.131175
69.685786	1843.875096	21.136192
69.972444	1845.521995	21.141210
69.932832	1848.283587	21.146227
70.063126	1847.985634	21.151245
70.108334	1846.375488	21.156263
70.130025	1837.567014	21.161280
70.102667	1842.614792	21.166298
70.532768	1830.895613	21.171315
70.055531	1836.692415	21.176333
70.343650	1825.986471	21.181351
70.352665	1835.456426	21.186368
70.692279	1853.591490	21.191386
71.056472	1848.721704	21.196403
70.970801	1853.570324	21.201421
70.734920	1851.451915	21.206439
70.885265	1850.708979	21.211456
70.662452	1859.539881	21.216474
71.185108	1854.348601	21.221491
71.175706	1848.991357	21.226509
70.822782	1856.955805	21.231527
71.458714	1861.864952	21.236544
71.123965	1854.270571	21.241562
71.234138	1859.489322	21.246579
71.759975	1857.586108	21.251597
71.557778	1852.189637	21.256615
71.689137	1850.193583	21.261632
71.607963	1856.979291	21.266650
71.641362	1849.835350	21.271667
71.664923	1854.651077	21.276685
71.467555	1858.674544	21.281703
71.604712	1857.943142	21.286720
71.522456	1877.826481	21.291738
72.047418	1878.744880	21.296755
71.963128	1880.402560	21.301773
71.824803	1877.164257	21.306791
71.739725	1882.754456	21.311808
71.880381	1896.675894	21.316826
72.074411	1894.950902	21.321843
72.350951	1899.263071	21.326861
72.664158	1909.771077	21.331879
72.461684	1905.356156	21.336896
72.738644	1908.402697	21.341914
72.777130	1892.155981	21.346931
72.579495	1904.429333	21.351949
72.738576	1905.938424	21.356967
73.065333	1894.061815	21.361984
72.964590	1902.258190	21.367002
72.895898	1918.377474	21.372019
73.520607	1918.734255	21.377037
73.194636	1920.802214	21.382055
73.599485	1914.799340	21.387072
73.132880	1921.610743	21.392090
73.319362	1911.188934	21.397107
73.254766	1921.689862	21.402125
73.043057	1914.521178	21.407143
73.595328	1907.775636	21.412160
73.996318	1925.998994	21.417178
74.157578	1926.794485	21.422195
74.283945	1919.351909	21.427213
73.835340	1915.026044	21.432231
74.369933	1910.628195	21.437248
74.064082	1916.824234	21.442266
74.219534	1924.522857	21.447283
74.353452	1933.272657	21.452301
74.323211	1926.937131	21.457319
74.460549	1933.991610	21.462336
74.463638	1932.378587	21.467354
74.444611	1932.552183	21.472371
74.681339	1922.819977	21.477389
74.425518	1924.561344	21.482407
74.663419	1925.344827	21.487424
74.740521	1933.901543	21.492442
74.840258	1948.208155	21.497459
75.090361	1949.668274	21.502477
75.257519	1953.035005	21.507495
75.600630	1954.332218	21.512512
75.294704	1951.243246	21.517530
75.675093	1950.653625	21.522547
75.546466	1943.446664	21.527565
75.540006	1951.284283	21.532583
75.615544	1954.397106	21.537600
75.615334	1958.736869	21.542618
75.645771	1953.231331	21.547635
75.858224	1956.253270	21.552653
75.887483	1953.960755	21.557671
76.211895	1939.496539	21.562688
75.804968	1942.694418	21.567706
75.833762	1945.189670	21.572723
76.198598	1942.267027	21.577741
75.942049	1942.458900	21.582759
76.013695	1943.495666	21.587776
76.391629	1953.605365	21.592794
76.448992	1970.560230	21.597811
76.512822	1962.149065	21.602829
76.349295	1959.359696	21.607847
76.825911	1962.677945	21.612864
76.804382	1956.707142	21.617882
76.905848	1954.696825	21.622899
76.906285	1946.380811	21.627917
76.762468	1959.049740	21.632935
77.162810	1965.719019	21.637952
77.178501	1975.557258	21.642970
77.195304	1975.883042	21.647987
77.220627	1976.317953	21.653005
77.149221	1977.497062	21.658023
77.668922	1979.322072	21.663040
77.135208	1982.924858	21.668058
77.200121	1981.778706	21.673075
77.546133	1974.708823	21.678093
77.418268	1974.337697	21.683111
77.620115	1992.787999	21.688128
77.934692	1999.069911	21.693146
77.751542	1998.227729	21.698163
77.797159	1999.230703	21.703181
77.672022	2006.477825	21.708199
77.935068	1997.066527	21.713216
78.082904	1998.993985	21.718234
78.121373	2016.652495	21.723251
78.426720	2018.889818	21.728269
78.548270	2030.302145	21.733287
78.491675	2031.655676	21.738304
78.630744	2034.398770	21.743322
78.567781	2029.838875	21.748339
78.838789	2028.512095	21.753357
78.661517	2032.204224	21.758375
78.838383	2026.233876	21.763392
79.024305	2040.738514	21.768410
78.944200	2053.956148	21.773427
79.449664	2049.108359	21.778445
79.180116	2044.849090	21.783463
79.756378	2046.747303	21.788480
79.442249	2044.401270	21.793498
79.457626	2046.721899	21.798515
79.792043	2038.198872	21.803533
79.619893	2045.791071	21.808551
79.769790	2029.021808	21.813568
80.082545	2030.809814	21.818586
79.638541	2039.549218	21.823603
79.929418	2042.006578	21.828621
80.287744	2054.047750	21.833639
80.228483	2060.946875	21.838656
80.379874	2051.695064	21.843674
80.162962	2063.921048	21.848691
80.468925	2058.501708	21.853709
80.173472	2063.604176	21.858727
80.462507	2062.886843	21.863744
80.573417	2058.069308	21.868762
80.372215	2064.170100	21.873779
80.469547	2073.216057	21.878797
80.616596	2084.867440	21.883815
80.550131	2078.307144	21.888832
81.251033	2086.460064	21.893850
80.986351	2089.828202	21.898867
81.592055	2086.444887	21.903885
81.364627	2077.899405	21.908903
81.423865	2093.680042	21.913920
81.804127	2109.230502	21.918938
81.865814	2110.253057	21.923955
81.912900	2106.177713	21.928973
81.698260	2103.352145	21.933991
82.039202	2106.009970	21.939008
82.024786	2110.894837	21.944026
82.069018	2101.808124	21.949043
82.403866	2102.292381	21.954061
82.381617	2103.334399	21.959079
82.191810	2100.577530	21.964096
82.377338	2098.083773	21.969114
82.495496	2107.281132	21.974131
82.363146	2091.862638	21.979149
82.480701	2098.409002	21.984167
82.426635	2105.206336	21.989184
82.510594	2107.775025	21.994202
82.344180	2101.104138	21.999219
82.609525	2094.179401	22.004237
82.506072	2108.214994	22.009255
82.437932	2117.864457	22.014272
82.816564	2115.457219	22.019290
82.631315	2128.448364	22.024307
82.837676	2130.808516	22.029325
83.155722	2149.250241	22.034343
82.913323	2142.130458	22.039360
83.052641	2144.166573	22.044378
83.087687	2146.594596	22.049395
83.509450	2154.608229	22.054413
84.057484	2172.900328	22.059431
83.970557	2167.817088	22.064448
83.800791	2165.704063	22.069466
83.884978	2163.529157	22.074483
84.196177	2163.297539	22.079501
84.071395	2165.753761	22.084519
84.159657	2174.293064	22.089536
84.314031	2166.798656	22.094554
84.276251	2177.680573	22.099571
84.567492	2182.852115	22.104589
84.620708	2187.527574	22.109607
84.468438	2196.511705	22.114624
84.850540	2192.958259	22.119642
84.983672	2193.650862	22.124659
84.773260	2189.865172	22.129677
84.642404	2184.318556	22.134695
85.185140	2190.059818	22.139712
84.814985	2187.204949	22.144730
84.965828	2194.920190	22.149747
85.348748	2202.166693	22.154765
85.447096	2211.973175	22.159783
85.561766	2212.075330	22.164800
85.886403	2208.123750	22.169818
85.696690	2208.601825	22.174835
85.751157	2216.133343	22.179853
85.955118	2204.648184	22.184871
86.073034	2203.616800	22.189888
85.915957	2211.708524	22.194906
85.792748	2221.306705	22.199923
86.233916	2221.177810	22.204941
86.425451	2227.472768	22.209959
86.223337	2223.808858	22.214976
86.704556	2231.901581	22.219994
86.679622	2228.238315	22.225011
86.639097	2228.102830	22.230029
86.683409	2224.861099	22.235047
86.590408	2234.710196	22.240064
86.811742	2227.069562	22.245082
86.806157	2254.165567	22.250099
87.225386	2250.969242	22.255117
87.333497	2256.472481	22.260135
86.992759	2261.231774	22.265152
87.343757	2262.016489	22.270170
87.611240	2252.329785	22.275187
87.551073	2255.034694	22.280205
87.502642	2254.202954	22.285223
87.104348	2254.666368	22.290240
87.713103	2265.156684	22.295258
87.978379	2273.819792	22.300275
87.919914	2270.117586	22.305293
88.203106	2281.750924	22.310311
88.466092	2285.134265	22.315328
88.248521	2285.799759	22.320346
87.964618	2271.853499	22.325363
88.205987	2267.447852	22.330381
88.018836	2268.155921	22.335399
88.174590	2290.492578	22.340416
88.673014	2275.546354	22.345434
88.817121	2291.165532	22.350451
88.916561	2284.427676	22.355469
89.020210	2285.566754	22.360487
88.935365	2287.032037	22.365504
89.174021	2273.906546	22.370522
89.234159	2281.247837	22.375539
89.256301	2271.754208	22.380557
89.407442	2273.734832	22.385575
89.212716	2277.799007	22.390592
89.491675	2274.321671	22.395610
89.275975	2286.247788	22.400627
89.612328	2295.108073	22.405645
89.684146	2306.099140	22.410663
89.594694	2312.277191	22.415680
89.693058	2306.836648	22.420698
90.037930	2305.091141	22.425715
89.938137	2309.225664	22.430733
89.804370	2313.138273	22.435751
89.890736	2322.687892	22.440768
90.141469	2328.929427	22.445786
90.027358	2334.047744	22.450803
90.195164	2344.073811	22.455821
90.483692	2342.898914	22.460839
90.720823	2356.193311	22.465856
90.685480	2345.477771	22.470874
90.938054	2353.612684	22.475891
91.044837	2347.842576	22.480909
91.223583	2362.572682	22.485927
91.423367	2369.529179	22.490944
91.570981	2375.136729	22.495962
91.926713	2370.757324	22.500979
91.810141	2369.645893	22.505997
92.030575	2360.815493	22.511015
91.685033	2361.873459	22.516032
91.591418	2352.580977	22.521050
92.288681	2363.802324	22.526067
92.059035	2368.885099	22.531085
92.171566	2366.197596	22.536103
91.855171	2375.418989	22.541120
92.083954	2371.756973	22.546138
92.435723	2363.085893	22.551155
92.235492	2361.217480	22.556173
92.413201	2363.661054	22.561191
92.441569	2375.160791	22.566208
92.541422	2386.895512	22.571226
92.578787	2393.691255	22.576243
92.408737	2399.206556	22.581261
92.950565	2401.233292	22.586279
92.911039	2402.098136	22.591296
93.420649	2411.540463	22.596314
93.693115	2419.558670	22.601331
93.467759	2412.843247	22.606349
93.623772	2410.230984	22.611367
93.401872	2420.829439	22.616384
93.569209	2416.148149	22.621402
93.650996	2417.710424	22.626419
93.436584	2410.759735	22.631437
93.711308	2415.978118	22.636455
93.578700	2431.716518	22.641472
93.844817	2434.638605	22.646490
93.907374	2436.929801	22.651507
93.790964	2438.709340	22.656525
94.586990	2437.647449	22.661543
94.520004	2458.914573	22.666560
94.287731	2456.385230	22.671578
94.723325	2449.862916	22.676595
94.653885	2465.534639	22.681613
94.973013	2456.553016	22.686631
94.711229	2462.234203	22.691648
94.649219	2460.902757	22.696666
94.861784	2458.597239	22.701683
94.934401	2459.848499	22.706701
95.462094	2472.150624	22.711719
94.814176	2481.323015	22.716736
95.346838	2474.255256	22.721754
95.647013	2468.880887	22.726771
95.659116	2485.467751	22.731789
95.687638	2487.227745	22.736807
95.631018	2496.768298	22.741824
96.159918	2487.794824	22.746842
96.169591	2496.595926	22.751859
96.538569	2497.469364	22.756877
96.625015	2496.790068	22.761895
96.264812	2501.000151	22.766912
96.240310	2496.683445	22.771930
96.957374	2492.348397	22.776947
96.905893	2495.683207	22.781965
96.747068	2487.316148	22.786983
96.827051	2496.775333	22.792000
96.581667	2490.233449	22.797018
96.862904	2486.291765	22.802035
96.607915	2503.248729	22.807053
96.801044	2506.589403	22.812071
96.990442	2511.388793	22.817088
97.221911	2512.226965	22.822106
97.438440	2511.861837	22.827123
97.442255	2535.592363	22.832141
97.477910	2532.519207	22.837159
97.482080	2536.675368	22.842176
97.876501	2531.260965	22.847194
97.714740	2533.050775	22.852211
97.842929	2556.294735	22.857229
98.234264	2548.264376	22.862247
98.073019	2552.238151	22.867264
98.049621	2564.364721	22.872282
98.171779	2557.222374	22.877299
98.486508	2567.768403	22.882317
99.095005	2577.129046	22.887335
99.195594	2579.253339	22.892352
99.181928	2575.774448	22.897370
99.271136	2569.574632	22.902387
99.522633	2580.313631	22.907405
99.624483	2568.339257	22.912423
99.142370	2567.881592	22.917440
99.554291	2564.777886	22.922458
99.817683	2574.239939	22.927475
99.683398	2569.956195	22.932493
100.048849	2572.323043	22.937511
99.814565	2571.656119	22.942528
99.508256	2560.253836	22.947546
100.191206	2565.856477	22.952563
99.790114	2564.574992	22.957581
100.151787	2570.423649	22.962599
100.614007	2582.067008	22.967616
100.688971	2578.627886	22.972634
101.189211	2576.621302	22.977651
100.753760	2581.666945	22.982669
101.040611	2569.512091	22.987687
100.849111	2574.604727	22.992704
101.281020	2563.045755	22.997722
101.127414	2569.959856	23.002739
100.888488	2582.006584	23.007757
101.167581	2579.580163	23.012775
101.285528	2574.215375	23.017792
101.476726	2575.425972	23.022810
101.643354	2568.317683	23.027827
101.352321	2564.304678	23.032845
101.516681	2574.167294	23.037863
101.546318	2573.484271	23.042880
101.461726	2581.293376	23.047898
101.734478	2583.617938	23.052915
101.948096	2592.084145	23.057933
102.165908	2594.521469	23.062951
102.262106	2592.565560	23.067968
102.172558	2597.853692	23.072986
102.153225	2588.129683	23.078003
101.726784	2611.810941	23.083021
102.225815	2606.866173	23.088039
102.108840	2627.131362	23.093056
102.343888	2630.901041	23.098074
102.574668	2635.059595	23.103091
102.864392	2648.036667	23.108109
103.115536	2644.055477	23.113127
103.179935	2661.319196	23.118144
102.951026	2669.621216	23.123162
103.338203	2669.068386	23.128179
103.293715	2671.704622	23.133197
103.534138	2685.522670	23.138215
103.870986	2689.582559	23.143232
103.790466	2688.818949	23.148250
104.097220	2694.108143	23.153267
103.955473	2697.453976	23.158285
104.104685	2692.595553	23.163303
104.284491	2693.438672	23.168320
104.203752	2706.189772	23.173338
104.259079	2710.726166	23.178355
104.456775	2714.811018	23.183373
104.336451	2703.180667	23.188391
104.881406	2724.102895	23.193408
105.149730	2731.863085	23.198426
105.515712	2729.328347	23.203443
105.379251	2736.463913	23.208461
105.448005	2742.876131	23.213479
105.703452	2734.582923	23.218496
105.447823	2723.425089	23.223514
105.796525	2724.364839	23.228531
105.757814	2732.599215	23.233549
105.750533	2732.644732	23.238567
105.947948	2723.571580	23.243584
106.096794	2727.380033	23.248602
106.538667	2714.354943	23.253619
106.245993	2733.331658	23.258637
106.322707	2747.623578	23.263655
106.150958	2748.578589	23.268672
106.426674	2755.065696	23.273690
106.660562	2748.514910	23.278707
106.621227	2758.210702	23.283725
106.482666	2760.325140	23.288743
106.726992	2768.060701	23.293760
106.844240	2777.823501	23.298778
107.025348	2779.499650	23.303795
107.063168	2774.671281	23.308813
106.982533	2785.926396	23.313831
107.195237	2799.019798	23.318848
107.430651	2797.995221	23.323866
107.920450	2802.324698	23.328883
107.676158	2805.790770	23.333901
107.747735	2819.849995	23.338919
107.972198	2823.577186	23.343936
108.121762	2824.668076	23.348954
108.219864	2821.054849	23.353971
108.340081	2821.020423	23.358989
108.446726	2825.192157	23.364007
108.969715	2815.888049	23.369024
108.772286	2821.461423	23.374042
108.690028	2813.233713	23.379059
108.911485	2821.474712	23.384077
108.620454	2834.157851	23.389095
109.133575	2845.020142	23.394112
109.089988	2842.208687	23.399130
109.063991	2833.590254	23.404147
109.133219	2840.772541	23.409165
109.319922	2846.699202	23.414183
109.830579	2850.700335	23.419200
109.674110	2859.682298	23.424218
109.965446	2860.880382	23.429235
109.917562	2868.377709	23.434253
109.935006	2863.353669	23.439271
110.353726	2861.059989	23.444288
110.351421	2864.658595	23.449306
110.341607	2863.552500	23.454323
110.371596	2875.030209	23.459341
110.438370	2885.836205	23.464359
110.571551	2883.675631	23.469376
110.295028	2881.702337	23.474394
110.879499	2886.660865	23.479411
110.966702	2907.421464	23.484429
111.224718	2909.227606	23.489447
111.187903	2903.590284	23.494464
111.238852	2906.167416	23.499482
111.234555	2909.248727	23.504499
111.607144	2917.535528	23.509517
111.806427	2936.040857	23.514535
112.122540	2931.001568	23.519552
112.075676	2928.525170	23.524570
112.050108	2927.194293	23.529587
112.177272	2928.279230	23.534605
112.352393	2931.004190	23.539623
112.599636	2936.350122	23.544640
112.153369	2948.612639	23.549658
112.443883	2934.096126	23.554675
112.873926	2947.758420	23.559693
113.110124	2941.535448	23.564711
113.145234	2932.910550	23.569728
113.309946	2943.376149	23.574746
113.377138	2933.622617	23.579763
113.188712	2941.119900	23.584781
113.132728	2958.598448	23.589799
113.801144	2959.273500	23.594816
113.822319	2965.226133	23.599834
114.242574	2961.808590	23.604851
114.018394	2953.978638	23.609869
114.059472	2955.288530	23.614887
114.127381	2957.821981	23.619904
114.127698	2964.538527	23.624922
114.451366	2969.695749	23.629939
114.406819	2982.952680	23.634957
114.266879	2983.953219	23.639975
114.961236	2971.775282	23.644992
114.722769	2991.018366	23.650010
114.791751	2974.039966	23.655027
115.126127	2988.657830	23.660045
115.224111	3005.225406	23.665063
115.580282	3005.198200	23.670080
115.387141	3001.109791	23.675098
115.450208	3003.252637	23.680115
115.730720	3005.102607	23.685133
115.653822	3002.873933	23.690151
115.821628	3002.011436	23.695168
116.084207	3006.281875	23.700186
115.877483	3014.350174	23.705203
116.234478	3026.827767	23.710221
116.099630	3025.362505	23.715239
116.484170	3018.986860	23.720256
116.118781	3023.418811	23.725274
116.100287	3021.231483	23.730291
116.342013	3031.618787	23.735309
116.517473	3040.533056	23.740327
116.611732	3045.685210	23.745344
116.789318	3055.495519	23.750362
116.848524	3066.002969	23.755379
117.083563	3066.180958	23.760397
117.298041	3069.531018	23.765415
117.639473	3068.543474	23.770432
117.583301	3073.744453	23.775450
117.824200	3076.998845	23.780467
118.316188	3093.081840	23.785485
118.183843	3090.038066	23.790503
118.294217	3089.976776	23.795520
118.485116	3090.101713	23.800538
118.459705	3088.240553	23.805555
118.603142	3091.308218	23.810573
118.270844	3094.731320	23.815591
118.264457	3089.341672	23.820608
118.863179	3107.011321	23.825626
118.900337	3111.661131	23.830643
119.042756	3113.333905	23.835661
119.010928	3121.090789	23.840679
119.189041	3109.268232	23.845696
119.394449	3137.838035	23.850714
119.622311	3137.581589	23.855731
119.769606	3135.077900	23.860749
119.728428	3134.734199	23.865767
119.673339	3130.478945	23.870784
120.230908	3140.838922	23.875802
119.950506	3148.527450	23.880819
120.441408	3149.640633	23.885837
120.794428	3166.869087	23.890855
120.920459	3150.506519	23.895872
120.676482	3150.737463	23.900890
120.518479	3150.336314	23.905907
121.051062	3150.208877	23.910925
120.942673	3165.716875	23.915943
121.275316	3160.880088	23.920960
121.235366	3174.158533	23.925978
121.035629	3179.176880	23.930995
121.403987	3174.738494	23.936013
121.266591	3181.148446	23.941031
121.874998	3180.538850	23.946048
122.031135	3192.947027	23.951066
121.986542	3195.785356	23.956083
122.127351	3197.682484	23.961101
122.328903	3206.097216	23.966119
122.143336	3202.285324	23.971136
122.319650	3211.433105	23.976154
122.732417	3222.383941	23.981171
123.026183	3216.830449	23.986189
122.867164	3225.532087	23.991207
122.893970	3211.006167	23.996224
122.891824	3220.503850	24.001242
123.380449	3241.195632	24.006259
123.660728	3242.464913	24.011277
123.415577	3252.540403	24.016295
123.464809	3248.050995	24.021312
123.758686	3240.562694	24.026330
123.694632	3243.943799	24.031347
123.770009	3238.194108	24.036365
123.993628	3264.659193	24.041383
124.086880	3261.327546	24.046400
123.868229	3265.572440	24.051418
124.254546	3270.467433	24.056435
124.419380	3259.909362	24.061453
124.774066	3273.820431	24.066471
124.777805	3280.984747	24.071488
124.630336	3285.666684	24.076506
124.878528	3285.501739	24.081523
125.090272	3282.757526	24.086541
125.131854	3288.852256	24.091559
125.359468	3295.107219	24.096576
125.472179	3303.889417	24.101594
125.294699	3304.053131	24.106611
125.706909	3304.339086	24.111629
125.680983	3308.651641	24.116647
125.969596	3327.563161	24.121664
126.176535	3336.576801	24.126682
126.080543	3324.711828	24.131699
126.077705	3323.159578	24.136717
126.481125	3345.531338	24.141735
126.624994	3348.176039	24.146752
126.701422	3349.975956	24.151770
126.645513	3351.645105	24.156787
127.467099	3353.975316	24.161805
127.073816	3355.618414	24.166823
127.191347	3373.846623	24.171840
127.656007	3368.301031	24.176858
127.392485	3372.439353	24.181875
127.777690	3363.491118	24.186893
127.634863	3366.389052	24.191911
127.640356	3374.332731	24.196928
127.726481	3383.971328	24.201946
127.819153	3394.666259	24.206963
128.252815	3404.805925	24.211981
128.294912	3416.518803	24.216999
128.624917	3415.908629	24.222016
128.820700	3422.367469	24.227034
128.707777	3427.208156	24.232051
129.133166	3414.873217	24.237069
129.086372	3428.544301	24.242087
129.248086	3438.385712	24.247104
129.641061	3439.848823	24.252122
129.687137	3444.247974	24.257139
130.021119	3435.260385	24.262157
130.010355	3441.410712	24.267175
129.951919	3432.263662	24.272192
129.885967	3444.154457	24.277210
129.688898	3446.821023	24.282227
130.307608	3456.748663	24.287245
130.234769	3451.751228	24.292263
130.264737	3448.697746	24.297280
130.607607	3462.462466	24.302298
130.648297	3479.348771	24.307315
131.160535	3479.013049	24.312333
131.146514	3478.384176	24.317351
131.302618	3481.651926	24.322368
131.573852	3464.581410	24.327386
131.545900	3479.161749	24.332403
131.526437	3490.919039	24.337421
132.125084	3492.308900	24.342439
132.083879	3493.944195	24.347456
132.299772	3496.426132	24.352474
132.220788	3505.430995	24.357491
132.435194	3491.803411	24.362509
132.324636	3496.198708	24.367527
132.418269	3491.468718	24.372544
132.708632	3497.896986	24.377562
132.548842	3518.845332	24.382579
132.700371	3511.540192	24.387597
132.592510	3517.188123	24.392615
133.015324	3511.948892	24.397632
133.301217	3527.745778	24.402650
133.158182	3542.202164	24.407667
133.391597	3543.737626	24.412685
133.457797	3553.133243	24.417703
133.642696	3554.351208	24.422720
133.973375	3559.273935	24.427738
134.020482	3567.615187	24.432755
134.277844	3559.854720	24.437773
134.471301	3571.619737	24.442791
134.174229	3569.507550	24.447808
134.378659	3569.617746	24.452826
134.394531	3585.539051	24.457843
134.599595	3579.879405	24.462861
135.033371	3591.534189	24.467879
134.916050	3601.735037	24.472896
135.549248	3605.663488	24.477914
135.235533	3621.608052	24.482931
135.678266	3620.500450	24.487949
135.728001	3613.511068	24.492967
135.532898	3618.023798	24.497984
136.106394	3618.063549	24.503002
136.142128	3631.141093	24.508019
136.287275	3637.033493	24.513037
136.453434	3629.634480	24.518055
136.393333	3628.962320	24.523072
136.115701	3629.776148	24.528090
136.355303	3648.320080	24.533107
136.606094	3645.345596	24.538125
137.321344	3658.225170	24.543143
137.014163	3667.316365	24.548160
137.334511	3675.756894	24.553178
137.568556	3673.896057	24.558195
137.601968	3673.392312	24.563213
137.896205	3672.730920	24.568231
137.804875	3692.914379	24.573248
138.086336	3698.293055	24.578266
138.209482	3702.516065	24.583283
138.461648	3706.444263	24.588301
138.912551	3694.799531	24.593319
138.674019	3701.036131	24.598336
138.663512	3686.301045	24.603354
139.016185	3708.365574	24.608371
139.431892	3702.142625	24.613389
139.726369	3709.798139	24.618407
139.524535	3714.469765	24.623424
139.479541	3707.810820	24.628442
139.571274	3704.100569	24.633459
139.872882	3713.576173	24.638477
140.096949	3717.953819	24.643495
139.705698	3709.051307	24.648512
139.957238	3719.166026	24.653530
140.395737	3735.554672	24.658547
140.338193	3728.263262	24.663565
140.353023	3724.609243	24.668583
140.227869	3748.752956	24.673600
140.825657	3740.336217	24.678618
140.795146	3753.815615	24.683635
140.883958	3754.875048	24.688653
140.987126	3765.391799	24.693671
141.348843	3778.169028	24.698688
141.691078	3767.295642	24.703706
141.619266	3774.386768	24.708723
141.894656	3792.773738	24.713741
141.945602	3804.807429	24.718759
141.585846	3813.749116	24.723776
142.263200	3802.100402	24.728794
142.396646	3806.530143	24.733811
141.896519	3809.083267	24.738829
142.520497	3818.202256	24.743847
142.552582	3841.368239	24.748864
142.769524	3826.764691	24.753882
142.786103	3830.979177	24.758899
142.861678	3842.860686	24.763917
142.983317	3850.533869	24.768935
143.069590	3862.034952	24.773952
143.566049	3869.305378	24.778970
143.416714	3874.044572	24.783987
143.352493	3876.245340	24.789005
144.096898	3896.481163	24.794023
144.510608	3903.496276	24.799040
144.327497	3905.879805	24.804058
144.795640	3902.454587	24.809075
144.961203	3905.269572	24.814093
144.947341	3897.886027	24.819111
144.772439	3901.865393	24.824128
144.976178	3903.809551	24.829146
145.021109	3918.438797	24.834163
145.307691	3918.741290	24.839181
145.618849	3919.857433	24.844199
145.402999	3928.104324	24.849216
145.828212	3933.346920	24.854234
145.854773	3948.692409	24.859251
145.731823	3951.480005	24.864269
146.109234	3946.610746	24.869287
146.539546	3966.532872	24.874304
146.524170	3964.108214	24.879322
146.595494	3978.704966	24.884339
146.858863	3973.114973	24.889357
146.939666	3971.113983	24.894375
146.891534	3973.084983	24.899392
147.253407	3981.711690	24.904410
147.682084	3986.038407	24.909427
147.558538	3981.010894	24.914445
147.918627	3987.630423	24.919463
147.912261	4007.501064	24.924480
148.039107	4004.552253	24.929498
148.305694	4006.467638	24.934515
148.472958	4022.397173	24.939533
148.598722	4007.460562	24.944551
148.427536	4017.079837	24.949568
148.973151	4023.850228	24.954586
149.113933	4023.695794	24.959603
149.136122	4031.274160	24.964621
149.479990	4022.950731	24.969639
149.231990	4025.366536	24.974656
149.363084	4042.229734	24.979674
149.790552	4048.340019	24.984691
149.708808	4050.628777	24.989709
149.791277	4045.082885	24.994727
150.063705	4059.124234	24.999744
150.149561	4066.105551	25.004762
150.344666	4069.888105	25.009779
150.070470	4073.870438	25.014797
150.692086	4087.121662	25.019815
150.774996	4095.062998	25.024832
150.969152	4096.670944	25.029850
151.116979	4091.862866	25.034867
151.133257	4098.397418	25.039885
151.586918	4105.311658	25.044903
151.842634	4119.759693	25.049920
151.896283	4116.099514	25.054938
151.835779	4123.084844	25.059955
152.126020	4126.167564	25.064973
152.204667	4125.265325	25.069991
152.278218	4138.416222	25.075008
152.426922	4138.932861	25.080026
152.465165	4137.134218	25.085043
152.412563	4137.322564	25.090061
152.635753	4152.489069	25.095079
152.955504	4167.965570	25.100096
153.238266	4171.642876	25.105114
153.391447	4171.571721	25.110131
153.335585	4178.707853	25.115149
153.801133	4186.949115	25.120167
153.486925	4192.459137	25.125184
153.813400	4191.915778	25.130202
153.875887	4195.457151	25.135219
154.148690	4211.335598	25.140237
154.336225	4215.469731	25.145255
154.137251	4220.396708	25.150272
154.533607	4229.778830	25.155290
154.935734	4235.984685	25.160307
154.548439	4251.489960	25.165325
155.213224	4257.133863	25.170343
155.391844	4270.309428	25.175360
155.357795	4262.124007	25.180378
155.673217	4269.539746	25.185395
155.477589	4268.629966	25.190413
155.692125	4275.379723	25.195431
156.105923	4286.769792	25.200448
156.543421	4308.020029	25.205466
156.666892	4310.974242	25.210483
156.621004	4326.896404	25.215501
156.874407	4304.165233	25.220519
156.637078	4316.528506	25.225536
156.922593	4324.147809	25.230554
157.146250	4327.026357	25.235571
157.761294	4328.161204	25.240589
157.673593	4321.126795	25.245607
157.845755	4344.217816	25.250624
157.921538	4353.337736	25.255642
158.246266	4340.433998	25.260659
158.399377	4344.586180	25.265677
158.753342	4346.339560	25.270695
158.465575	4346.558437	25.275712
158.324056	4362.236784	25.280730
159.217365	4372.361802	25.285747
159.075022	4367.595955	25.290765
158.939881	4374.378436	25.295783
158.938472	4378.971484	25.300800
158.855793	4398.564116	25.305818
159.144118	4398.424441	25.310835
159.612460	4419.761515	25.315853
159.985052	4417.291797	25.320871
159.908193	4420.738256	25.325888
160.210876	4443.139786	25.330906
160.400680	4442.961886	25.335923
160.596604	4455.206874	25.340941
161.013999	4455.350000	25.345959
161.095297	4468.023295	25.350976
161.173569	4479.889017	25.355994
161.562185	4463.604073	25.361011
161.396341	4468.308131	25.366029
161.444791	4473.979218	25.371047
162.197407	4489.514439	25.376064
162.115193	4495.947774	25.381082
162.099678	4481.575820	25.386099
162.360124	4487.232638	25.391117
162.537654	4486.302264	25.396135
162.188980	4496.593519	25.401152
162.312873	4512.006304	25.406170
162.842448	4512.974635	25.411187
162.721599	4521.835049	25.416205
163.137932	4529.901103	25.421223
163.201445	4533.325592	25.426240
163.547076	4542.112936	25.431258
163.808072	4534.452493	25.436275
163.879429	4541.919206	25.441293
164.185425	4560.280066	25.446311
164.070271	4553.458195	25.451328
164.349118	4560.494693	25.456346
164.726811	4557.490712	25.461363
164.706571	4558.785074	25.466381
164.828339	4576.736061	25.471399
165.468534	4582.734290	25.476416
165.411826	4582.333020	25.481434
165.417195	4583.664407	25.486451
165.454410	4586.502763	25.491469
165.363015	4581.915110	25.496487
165.500969	4595.375054	25.501504
165.879322	4605.208414	25.506522
166.162835	4599.914941	25.511539
166.161987	4612.610676	25.516557
166.388650	4624.724704	25.521575
166.560513	4627.841839	25.526592
166.603243	4625.654196	25.531610
166.825973	4641.345161	25.536627
166.850365	4643.450070	25.541645
167.454609	4647.373821	25.546663
167.648221	4657.608618	25.551680
167.831960	4663.571063	25.556698
167.723994	4669.604462	25.561715
168.074424	4661.948893	25.566733
168.499310	4667.728362	25.571751
168.803409	4658.372384	25.576768
168.674369	4671.167156	25.581786
169.191723	4674.738371	25.586803
169.125125	4682.747578	25.591821
169.064293	4679.869095	25.596839
169.643241	4674.778681	25.601856
169.370346	4675.033109	25.606874
169.986114	4673.295448	25.611891
169.832266	4682.088511	25.616909
169.939150	4690.995400	25.621927
170.136058	4688.853038	25.626944
169.862925	4693.870673	25.631962
170.272488	4695.561717	25.636979
170.326707	4710.717284	25.641997
170.560773	4711.252132	25.647015
170.543355	4723.202448	25.652032
170.659908	4736.362824	25.657050
171.152973	4735.761787	25.662067
171.368728	4746.113113	25.667085
171.521942	4764.662254	25.672103
172.046227	4763.822743	25.677120
171.895932	4770.440449	25.682138
172.367211	4770.739277	25.687156
172.482459	4785.869562	25.692173
172.556903	4783.522262	25.697191
172.714971	4785.502080	25.702208
172.541180	4796.432132	25.707226
172.813157	4794.928242	25.712244
172.892481	4815.850092	25.717261
173.004921	4818.367360	25.722279
173.664385	4815.477021	25.727296
173.603974	4835.988341	25.732314
173.940801	4832.608777	25.737332
173.765309	4839.861763	25.742349
173.638712	4844.117853	25.747367
174.503837	4853.486836	25.752384
174.138056	4866.637643	25.757402
174.337090	4867.114854	25.762420
174.649644	4878.827342	25.767437
174.486512	4877.442115	25.772455
174.779698	4890.789576	25.777472
174.774840	4908.501892	25.782490
175.195735	4913.499242	25.787508
175.093045	4928.490178	25.792525
175.497688	4940.043077	25.797543
176.025618	4938.369659	25.802560
176.193468	4936.875757	25.807578
176.425947	4956.684766	25.812596
176.579151	4966.468368	25.817613
176.975104	4967.097812	25.822631
176.889626	4957.742740	25.827648
177.005899	4965.897032	25.832666
177.186103	4974.227550	25.837684
177.541913	4989.730671	25.842701
177.427156	4986.601749	25.847719
178.009295	4993.407821	25.852736
178.147442	5010.573844	25.857754
178.524300	5006.932296	25.862772
178.854043	5005.943329	25.867789
178.706207	5007.418697	25.872807
178.872065	5004.551997	25.877824
178.843608	5021.204358	25.882842
179.207596	5023.789570	25.887860
179.502460	5030.362883	25.892877
179.455718	5026.964461	25.897895
179.947302	5025.296729	25.902912
179.769449	5041.549534	25.907930
180.013149	5044.286169	25.912948
180.508811	5032.961857	25.917965
180.448900	5053.542788	25.922983
180.534371	5050.597134	25.928000
180.631149	5063.640895	25.933018
181.074584	5072.700424	25.938036
181.006084	5064.775721	25.943053
180.880835	5077.907937	25.948071
181.352886	5084.642907	25.953088
181.428748	5086.973391	25.958106
181.537073	5101.590502	25.963124
181.623522	5111.059512	25.968141
181.615641	5120.663256	25.973159
182.253388	5128.019382	25.978176
182.454920	5145.393406	25.983194
182.085397	5151.628926	25.988212
182.683785	5157.921148	25.993229
182.840086	5174.390032	25.998247
183.070672	5182.772728	26.003264
183.634759	5199.764876	26.008282
183.418651	5197.292585	26.013300
183.862355	5205.610338	26.018317
183.714618	5222.751903	26.023335
184.175344	5219.763217	26.028352
184.467383	5217.416495	26.033370
184.356673	5244.148341	26.038388
184.502958	5238.399536	26.043405
184.654049	5248.777063	26.048423
185.179313	5263.635176	26.053440
185.412018	5268.643167	26.058458
185.514851	5267.440363	26.063476
185.724528	5270.460143	26.068493
185.819303	5279.580710	26.073511
186.566613	5285.540299	26.078528
186.470678	5285.937468	26.083546
186.367389	5287.532144	26.088564
186.735515	5280.580626	26.093581
186.631895	5289.700713	26.098599
187.135036	5302.703081	26.103616
187.098756	5304.113647	26.108634
186.973182	5305.235167	26.113652
187.542290	5312.422196	26.118669
187.327529	5326.979621	26.123687
187.813023	5322.945355	26.128704
188.085708	5330.361912	26.133722
187.961017	5346.231022	26.138740
188.189721	5349.595063	26.143757
187.632683	5359.569060	26.148775
188.375133	5381.479865	26.153792
189.002239	5382.496101	26.158810
189.200046	5400.256061	26.163828
189.283120	5404.255313	26.168845
189.138213	5416.585912	26.173863
189.826419	5416.377274	26.178880
190.008852	5429.281613	26.183898
189.968625	5437.728949	26.188916
190.398444	5435.884617	26.193933
190.637927	5447.296412	26.198951
190.885312	5449.767374	26.203968
190.861594	5457.369310	26.208986
190.700524	5465.775614	26.214004
191.022545	5472.764667	26.219021
190.976649	5472.172285	26.224039
191.427203	5482.913394	26.229056
191.889620	5492.449969	26.234074
192.104205	5503.900424	26.239092
192.460567	5499.693794	26.244109
192.638017	5516.778377	26.249127
192.924928	5512.058621	26.254144
193.083356	5515.496836	26.259162
193.270483	5527.598720	26.264180
193.551672	5514.805145	26.269197
193.490519	5528.855699	26.274215
193.989735	5540.091127	26.279232
194.006241	5547.248024	26.284250
194.140841	5541.289459	26.289268
194.162505	5551.431745	26.294285
194.116832	5552.752259	26.299303
194.576153	5558.198328	26.304320
194.719693	5572.753480	26.309338
194.560066	5585.989303	26.314356
195.270317	5589.558894	26.319373
195.037118	5598.292224	26.324391
195.078415	5621.717879	26.329408
195.607037	5627.986472	26.334426
195.882317	5642.246411	26.339444
195.864794	5645.393392	26.344461
196.219711	5653.529547	26.349479
196.475293	5651.633573	26.354496
196.875425	5667.578576	26.359514
196.574136	5666.631613	26.364532
196.942538	5682.761531	26.369549
196.823468	5698.102900	26.374567
197.451174	5703.118578	26.379584
197.788577	5716.687000	26.384602
197.401193	5730.703586	26.389620
197.671185	5733.451990	26.394637
198.011157	5750.249326	26.399655
198.243829	5749.133477	26.404672
198.597943	5763.387475	26.409690
198.711592	5773.597548	26.414708
199.396517	5785.163897	26.419725
199.757784	5792.838243	26.424743
199.542038	5790.249015	26.429760
199.794919	5793.334719	26.434778
199.587751	5796.754501	26.439796
200.354060	5801.069803	26.444813
200.234391	5812.459174	26.449831
200.306146	5815.295468	26.454848
200.504020	5816.000170	26.459866
200.588607	5825.135233	26.464884
201.178643	5827.868237	26.469901
201.114429	5835.593473	26.474919
200.858970	5843.572798	26.479936
201.610953	5849.525530	26.484954
201.696377	5864.708735	26.489972
201.709357	5866.907118	26.494989
201.962833	5882.108204	26.500007
202.634756	5883.452062	26.505024
202.531053	5895.508207	26.510042
202.493022	5904.706713	26.515060
202.687470	5911.195062	26.520077
203.103356	5924.830262	26.525095
203.260748	5937.006525	26.530112
203.881458	5936.107667	26.535130
204.170694	5958.301669	26.540148
204.294972	5947.688419	26.545165
204.413322	5957.512738	26.550183
204.392137	5952.108775	26.555200
204.631724	5965.064517	26.560218
204.756135	5988.291374	26.565236
205.031323	5984.959139	26.570253
205.192062	6006.317856	26.575271
205.371680	6008.578539	26.580288
205.447901	6015.789400	26.585306
205.778426	6027.910189	26.590324
206.264180	6034.602330	26.595341
206.464482	6044.833703	26.600359
206.572085	6053.630660	26.605376
206.802027	6059.927255	26.610394
206.831522	6077.360686	26.615412
207.301644	6085.289582	26.620429
207.316370	6084.643488	26.625447
207.087200	6102.663583	26.630464
207.975808	6104.188172	26.635482
208.005796	6121.065979	26.640500
207.924914	6136.812111	26.645517
208.427959	6144.540156	26.650535
208.451778	6147.586043	26.655552
208.682976	6161.026223	26.660570
208.758543	6172.549385	26.665588
209.671631	6177.469980	26.670605
209.274475	6186.958488	26.675623
209.542994	6196.118587	26.680640
209.815488	6204.836120	26.685658
210.127264	6221.221613	26.690676
210.264545	6226.655199	26.695693
210.555926	6234.280701	26.700711
211.182784	6240.439415	26.705728
211.338030	6235.468618	26.710746
211.049071	6244.997028	26.715764
211.159906	6262.780922	26.720781
211.718636	6258.902290	26.725799
211.748698	6267.051731	26.730816
212.083052	6278.831155	26.735834
212.268289	6292.821598	26.740852
212.684192	6288.873789	26.745869
212.979519	6296.552364	26.750887
212.966168	6312.376457	26.755904
213.255464	6309.809053	26.760922
213.200685	6313.457600	26.765940
213.827922	6333.247301	26.770957
214.006128	6338.564022	26.775975
214.024745	6336.354697	26.780992
214.331062	6336.644676	26.786010
214.227419	6336.342266	26.791028
214.477158	6350.471019	26.796045
214.963772	6345.400929	26.801063
215.206029	6357.977717	26.806080
215.212651	6343.506125	26.811098
215.396461	6373.012497	26.816116
215.645564	6374.469985	26.821133
215.641218	6380.219386	26.826151
215.648663	6400.140979	26.831168
215.962947	6407.027430	26.836186
216.300778	6414.440539	26.841204
216.129083	6420.673905	26.846221
216.408445	6428.115119	26.851239
216.725305	6455.163725	26.856256
216.835915	6457.959307	26.861274
217.593022	6479.313541	26.866292
217.718269	6492.306511	26.871309
217.751458	6496.777870	26.876327
217.958339	6505.461630	26.881344
218.270635	6503.029497	26.886362
218.872763	6520.727206	26.891380
218.922337	6540.696018	26.896397
218.965045	6538.145115	26.901415
219.078386	6551.139992	26.906432
219.670600	6555.848944	26.911450
219.672998	6565.915889	26.916468
219.593097	6581.835875	26.921485
220.085535	6579.732233	26.926503
220.246291	6596.577365	26.931520
220.799586	6607.697649	26.936538
220.904772	6620.485501	26.941556
220.704476	6623.418205	26.946573
220.914340	6637.723895	26.951591
221.366226	6650.874159	26.956608
221.724872	6654.647418	26.961626
221.600578	6663.676721	26.966644
222.141274	6671.897875	26.971661
222.144675	6678.672132	26.976679
222.436805	6707.145566	26.981696
222.651636	6702.727230	26.986714
223.504626	6717.279486	26.991732
223.270214	6732.447220	26.996749
223.640691	6734.876978	27.001767
223.886744	6746.960968	27.006784
224.128637	6756.210754	27.011802
224.447142	6756.183146	27.016820
224.491460	6757.063472	27.021837
224.804446	6767.432284	27.026855
224.891396	6783.231599	27.031872
224.820520	6781.954890	27.036890
225.151667	6801.696777	27.041908
225.243843	6810.477573	27.046925
225.536043	6822.731169	27.051943
225.787903	6842.513934	27.056960
226.219735	6847.096557	27.061978
226.411183	6857.058281	27.066996
226.421596	6860.321054	27.072013
226.913406	6871.305915	27.077031
227.097375	6889.577748	27.082048
227.540315	6891.686800	27.087066
227.862467	6908.832094	27.092084
228.059262	6910.032642	27.097101
228.158933	6908.975444	27.102119
228.561264	6923.443776	27.107136
228.643843	6935.332518	27.112154
228.935638	6929.958159	27.117172
228.882911	6930.995755	27.122189
229.043091	6943.216447	27.127207
229.333597	6964.877956	27.132224
229.561783	6953.929000	27.137242
229.823290	6964.511187	27.142260
229.822778	6974.392555	27.147277
230.072505	6977.857784	27.152295
230.188048	6996.329856	27.157312
230.586917	7006.145519	27.162330
230.823752	7018.019620	27.167348
231.297235	7027.280617	27.172365
231.137763	7034.569841	27.177383
231.106426	7050.321621	27.182400
231.514273	7061.708051	27.187418
232.197187	7062.939791	27.192436
232.124831	7084.569892	27.197453
232.579995	7085.209084	27.202471
232.356359	7108.195132	27.207488
232.693907	7123.955483	27.212506
233.422145	7135.165490	27.217524
233.287558	7137.090392	27.222541
233.850942	7142.908939	27.227559
233.734698	7157.275592	27.232576
234.383318	7169.186304	27.237594
234.694125	7178.365527	27.242612
234.652246	7179.587697	27.247629
234.884553	7187.655352	27.252647
235.060122	7202.361473	27.257664
234.990070	7208.225605	27.262682
235.571296	7215.484103	27.267700
235.928096	7235.017237	27.272717
235.981457	7249.139563	27.277735
236.271298	7254.988371	27.282752
236.479105	7273.872456	27.287770
236.958791	7281.052179	27.292788
236.886072	7289.461259	27.297805
237.200993	7298.788274	27.302823
237.675498	7308.611193	27.307840
237.827478	7316.435775	27.312858
238.143756	7325.626841	27.317876
238.412402	7333.966681	27.322893
238.686103	7353.655022	27.327911
238.821715	7364.181395	27.332928
238.990737	7373.108270	27.337946
239.218592	7381.508189	27.342964
239.680297	7394.629037	27.347981
239.804172	7385.722943	27.352999
240.215920	7406.936633	27.358016
240.215125	7409.658260	27.363034
240.879008	7422.624333	27.368052
241.004625	7427.829644	27.373069
240.990358	7438.616312	27.378087
241.105980	7438.494208	27.383104
241.071127	7454.840398	27.388122
241.641122	7458.208192	27.393140
241.970296	7488.817471	27.398157
242.101112	7484.914071	27.403175
242.026612	7499.454399	27.408192
242.127527	7509.010780	27.413210
242.740325	7516.886380	27.418228
243.186250	7535.837614	27.423245
243.436072	7539.362918	27.428263
243.731087	7564.493969	27.433280
243.793106	7564.737003	27.438298
244.159480	7576.307042	27.443316
244.354284	7593.324546	27.448333
244.870303	7596.104148	27.453351
245.092405	7592.423200	27.458368
244.874448	7602.522075	27.463386
245.621688	7603.709051	27.468404
245.673574	7621.216207	27.473421
245.572578	7615.802158	27.478439
246.010067	7631.471521	27.483456
246.116819	7643.088587	27.488474
246.450803	7648.217120	27.493492
246.320759	7660.562679	27.498509
246.993257	7670.929353	27.503527
246.958512	7688.772160	27.508544
247.283639	7695.313284	27.513562
247.377957	7700.476220	27.518580
247.560949	7724.816840	27.523597
248.103573	7733.189710	27.528615
248.373778	7748.740154	27.533632
248.659406	7754.899172	27.538650
248.648854	7770.698824	27.543668
248.977435	7783.638754	27.548685
249.522435	7791.559822	27.553703
249.574851	7800.284178	27.558720
249.797486	7818.291999	27.563738
250.207193	7817.883888	27.568756
250.285484	7838.367365	27.573773
250.499326	7849.074340	27.578791
251.089479	7863.245642	27.583808
251.377544	7875.696327	27.588826
251.462499	7881.564804	27.593844
251.363821	7900.686968	27.598861
251.567951	7903.786983	27.603879
252.102381	7909.259879	27.608896
252.278351	7929.204083	27.613914
252.726051	7941.216229	27.618932
252.749129	7950.690321	27.623949
252.882696	7968.759597	27.628967
253.349923	7977.766334	27.633984
253.707975	7995.718386	27.639002
254.236571	8009.438511	27.644020
254.370826	8026.563770	27.649037
254.610357	8041.257383	27.654055
254.568523	8043.240461	27.659072
254.565704	8061.167025	27.664090
254.840128	8063.577282	27.669108
255.175378	8076.933109	27.674125
255.576624	8100.333949	27.679143
256.199026	8104.107235	27.684160
256.474431	8119.578251	27.689178
256.984582	8124.717206	27.694196
257.228119	8142.134849	27.699213
257.338535	8137.423132	27.704231
257.518874	8150.784338	27.709248
257.871347	8151.588044	27.714266
258.302417	8150.112637	27.719284
258.548882	8172.404416	27.724301
258.896785	8178.061312	27.729319
259.332517	8168.982861	27.734336
259.326558	8176.024331	27.739354
259.509543	8184.526360	27.744372
259.597769	8199.739469	27.749389
259.668082	8203.144638	27.754407
260.094687	8220.476848	27.759424
260.830316	8224.832274	27.764442
260.713356	8216.999042	27.769460
261.185536	8234.589324	27.774477
261.261923	8245.589574	27.779495
261.548605	8245.816366	27.784512
261.766023	8253.687924	27.789530
262.017430	8261.813044	27.794548
262.106681	8271.545289	27.799565
262.035964	8267.348112	27.804583
262.381308	8281.996928	27.809600
262.616662	8290.904386	27.814618
262.896239	8299.767035	27.819636
263.066352	8320.716546	27.824653
262.802130	8322.889190	27.829671
263.157246	8342.884706	27.834688
263.282191	8364.052870	27.839706
263.911427	8375.234949	27.844724
264.014143	8392.368645	27.849741
264.547586	8420.911113	27.854759
265.065432	8426.149977	27.859776
264.994948	8445.947075	27.864794
265.607982	8449.633501	27.869812
265.752146	8461.977682	27.874829
265.689331	8471.156093	27.879847
266.675443	8491.273924	27.884864
266.712119	8512.178254	27.889882
267.155179	8515.941835	27.894900
267.092942	8528.255250	27.899917
267.584229	8533.842437	27.904935
268.168056	8559.052729	27.909952
267.856835	8555.647726	27.914970
268.344292	8567.609853	27.919988
268.364068	8582.834000	27.925005
268.603223	8610.330479	27.930023
269.106881	8622.511107	27.935040
269.205620	8630.009926	27.940058
269.529894	8640.475901	27.945076
269.914469	8665.524964	27.950093
269.910403	8673.500854	27.955111
270.383117	8673.332277	27.960128
270.548944	8698.576668	27.965146
271.268089	8709.372317	27.970164
271.257080	8717.930239	27.975181
271.522602	8740.336534	27.980199
272.189931	8742.334883	27.985216
272.260578	8751.947164	27.990234
272.655407	8762.506344	27.995252
272.997116	8763.434895	28.000269
272.930147	8786.496358	28.005287
273.446632	8796.218782	28.010304
273.668896	8803.436272	28.015322
273.953394	8814.505290	28.020340
274.078431	8836.791634	28.025357
274.211929	8843.442117	28.030375
274.939357	8851.862323	28.035392
274.926680	8874.915391	28.040410
275.647619	8878.720762	28.045428
275.716029	8876.073951	28.050445
275.663264	8903.341916	28.055463
276.462224	8918.485322	28.060480
276.213534	8932.043747	28.065498
276.555306	8929.426723	28.070516
276.850962	8947.370532	28.075533
276.935171	8959.475014	28.080551
277.096903	8971.033787	28.085568
277.413240	8984.525839	28.090586
277.555594	8999.219651	28.095604
278.085663	9013.555957	28.100621
277.940244	9034.723038	28.105639
278.834577	9044.970496	28.110656
278.698343	9069.653360	28.115674
278.859118	9077.120541	28.120692
279.522767	9087.385215	28.125709
279.180194	9111.456376	28.130727
279.690216	9104.954792	28.135744
280.425371	9120.705083	28.140762
280.662405	9130.158890	28.145780
281.154049	9154.841385	28.150797
281.498211	9156.044256	28.155815
281.949997	9145.428383	28.160832
282.123147	9166.346801	28.165850
282.641328	9174.443163	28.170868
282.679389	9177.992484	28.175885
282.463044	9183.498127	28.180903
283.269605	9193.794147	28.185920
283.440582	9194.597918	28.190938
283.421814	9211.808233	28.195956
283.688210	9218.336999	28.200973
283.582205	9232.769959	28.205991
284.167202	9254.021779	28.211008
284.336367	9274.760979	28.216026
284.935128	9290.804308	28.221044
285.179027	9299.843521	28.226061
285.169172	9314.248854	28.231079
285.902255	9326.460311	28.236096
286.013245	9341.664476	28.241114
286.056089	9354.533449	28.246132
286.774585	9365.882116	28.251149
286.711802	9389.148895	28.256167
287.354855	9398.599225	28.261184
287.354313	9411.115100	28.266202
287.607330	9431.108841	28.271220
288.111093	9438.026739	28.276237
287.934048	9458.482544	28.281255
288.274521	9473.953972	28.286272
288.825495	9490.317536	28.291290
288.806774	9493.269605	28.296308
289.434143	9510.066403	28.301325
289.754659	9540.563612	28.306343
290.265927	9546.646838	28.311360
290.522037	9556.599892	28.316378
290.791106	9571.965766	28.321396
290.899419	9579.223510	28.326413
291.446353	9600.677446	28.331431
291.662057	9606.036599	28.336448
291.848524	9623.944492	28.341466
291.995254	9631.625640	28.346484
292.580136	9650.153136	28.351501
293.013347	9663.431618	28.356519
293.449912	9668.288902	28.361536
294.057729	9679.582480	28.366554
293.492962	9691.754370	28.371572
294.018418	9710.253347	28.376589
294.153408	9715.236819	28.381607
294.473905	9729.906460	28.386624
295.119564	9747.931984	28.391642
295.333449	9757.793881	28.396660
295.684542	9761.063789	28.401677
295.904942	9779.358032	28.406695
295.877242	9799.838177	28.411712
296.125076	9807.471985	28.416730
296.431439	9820.372620	28.421748
296.943081	9835.186059	28.426765
297.199556	9857.730887	28.431783
297.520678	9865.154323	28.436800
297.822005	9875.684583	28.441818
297.925697	9899.487937	28.446836
298.086599	9903.299163	28.451853
298.796977	9918.097323	28.456871
298.876505	9933.145872	28.461888
299.147811	9949.212651	28.466906
299.534840	9966.896855	28.471924
299.817601	9984.092223	28.476941
299.648451	9993.029134	28.481959
300.190001	10004.699552	28.486976
300.684676	10011.830637	28.491994
301.032342	10031.848087	28.497012
301.137738	10043.233220	28.502029
301.413951	10059.795042	28.507047
302.011726	10069.761155	28.512064
302.013376	10080.900497	28.517082
302.336848	10103.381452	28.522100
302.465404	10111.371916	28.527117
302.917897	10124.331964	28.532135
303.469120	10158.737687	28.537152
303.464967	10161.738098	28.542170
303.747681	10179.467262	28.547188
304.537711	10186.949987	28.552205
304.903955	10196.005203	28.557223
305.037620	10214.812336	28.562240
305.142101	10220.738487	28.567258
305.430000	10246.559458	28.572276
305.597261	10253.546163	28.577293
305.732763	10275.119005	28.582311
306.370050	10285.925246	28.587328
306.879142	10313.615612	28.592346
307.032544	10319.995121	28.597364
307.818631	10328.520487	28.602381
307.642239	10343.773645	28.607399
308.233527	10352.159032	28.612416
308.649337	10368.547702	28.617434
308.519653	10374.943157	28.622452
309.009120	10383.947588	28.627469
309.219680	10399.203325	28.632487
309.632515	10426.267968	28.637504
310.170345	10434.702815	28.642522
310.015688	10450.691508	28.647540
310.720959	10456.476259	28.652557
310.935491	10466.366848	28.657575
311.453617	10475.584701	28.662592
311.830932	10497.293582	28.667610
311.831422	10506.459922	28.672628
312.227645	10514.822262	28.677645
312.156248	10533.409239	28.682663
312.781819	10545.799378	28.687680
313.012004	10566.025255	28.692698
313.205858	10589.376471	28.697716
313.867914	10594.905961	28.702733
314.329236	10621.597021	28.707751
314.332574	10628.502189	28.712768
314.786791	10641.932799	28.717786
314.811824	10659.961701	28.722804
315.158839	10661.154756	28.727821
315.575699	10687.492916	28.732839
315.696781	10701.863020	28.737856
316.230231	10724.671791	28.742874
316.163389	10747.454636	28.747892
317.200077	10744.198040	28.752909
317.364122	10770.086501	28.757927
317.396723	10784.997839	28.762944
317.852657	10796.296947	28.767962
318.085036	10808.284693	28.772980
318.383329	10824.518507	28.777997
318.674638	10836.263381	28.783015
318.930893	10856.731779	28.788032
319.556270	10864.831036	28.793050
319.402449	10892.872395	28.798068
320.099988	10900.881425	28.803085
320.166947	10917.906217	28.808103
320.617552	10931.719668	28.813120
321.270814	10944.156257	28.818138
321.082730	10966.888894	28.823156
321.772621	10962.303567	28.828173
321.936265	10964.532634	28.833191
322.330791	10979.333755	28.838208
322.450742	11001.127743	28.843226
322.465452	11021.346817	28.848244
323.169246	11034.037631	28.853261
323.381124	11045.400380	28.858279
323.504964	11055.125505	28.863296
324.159417	11071.638448	28.868314
324.304654	11093.084404	28.873332
324.890412	11094.173780	28.878349
325.233306	11119.100057	28.883367
325.462361	11136.465937	28.888384
326.249854	11146.620788	28.893402
326.230137	11155.850605	28.898420
326.651698	11165.964901	28.903437
327.060553	11183.893135	28.908455
326.887621	11192.193370	28.913472
327.438419	11205.694514	28.918490
327.765947	11224.443876	28.923508
327.677141	11235.771744	28.928525
327.766258	11254.419547	28.933543
328.581508	11273.042037	28.938560
329.404617	11285.824849	28.943578
329.443513	11313.909274	28.948596
329.986032	11329.388486	28.953613
330.309358	11329.934822	28.958631
330.178554	11346.697321	28.963648
331.189824	11361.799998	28.968666
331.203562	11375.379077	28.973684
331.552768	11384.699626	28.978701
331.826269	11409.776096	28.983719
332.158705	11424.735706	28.988736
332.808466	11431.372555	28.993754
332.944194	11445.665152	28.998772
333.398831	11448.470754	29.003789
333.387808	11476.800067	29.008807
333.675392	11496.897967	29.013824
334.283652	11507.128456	29.018842
334.613943	11526.815517	29.023860
334.569782	11535.133624	29.028877
335.334179	11557.212546	29.033895
335.426154	11570.151132	29.038912
335.839263	11576.604065	29.043930
336.138809	11598.114842	29.048948
336.651882	11602.976441	29.053965
337.093995	11620.543065	29.058983
337.072672	11634.699365	29.064000
337.668866	11649.766250	29.069018
337.959968	11659.834938	29.074036
338.496261	11678.368907	29.079053
338.507471	11692.712775	29.084071
338.766801	11710.519681	29.089088
339.176927	11730.680736	29.094106
339.434711	11744.714456	29.099124
339.907418	11759.920766	29.104141
339.950948	11771.013502	29.109159
340.309900	11799.938993	29.114176
341.021507	11807.437820	29.119194
341.279173	11832.015257	29.124212
341.760786	11842.297347	29.129229
341.884836	11860.210844	29.134247
342.108047	11881.146565	29.139264
342.497644	11892.579879	29.144282
342.582603	11912.261566	29.149300
343.108398	11926.487112	29.154317
343.649882	11944.970008	29.159335
343.713194	11962.008948	29.164352
344.147672	11972.554270	29.169370
344.424551	11995.635296	29.174388
344.609931	12011.957296	29.179405
345.191162	12023.938542	29.184423
344.984945	12047.259509	29.189440
345.454585	12057.894104	29.194458
346.034247	12073.017601	29.199476
346.229871	12101.486003	29.204493
346.665066	12118.334205	29.209511
347.067393	12136.097010	29.214528
347.309309	12156.985899	29.219546
347.540627	12180.181652	29.224564
347.704422	12197.609262	29.229581
348.647746	12201.958375	29.234599
348.908171	12230.053674	29.239616
349.088410	12245.505132	29.244634
349.696112	12268.540987	29.249652
349.902949	12285.750363	29.254669
350.306943	12304.915131	29.259687
350.682824	12322.776989	29.264704
351.226376	12340.599969	29.269722
351.601796	12359.387173	29.274740
351.784775	12375.375137	29.279757
352.779709	12387.740222	29.284775
353.132494	12406.294182	29.289792
353.075701	12407.241141	29.294810
353.563529	12428.764427	29.299828
353.654198	12440.898571	29.304845
354.616366	12453.985660	29.309863
354.778057	12472.196994	29.314880
355.015355	12480.875632	29.319898
355.256117	12500.230375	29.324916
355.442278	12516.300064	29.329933
355.831595	12532.211629	29.334951
355.871969	12554.777765	29.339968
356.632151	12561.410354	29.344986
356.673540	12586.240545	29.350004
357.110478	12609.098306	29.355021
357.735667	12616.528893	29.360039
357.571449	12653.716496	29.365056
358.168169	12671.720933	29.370074
358.882625	12688.677481	29.375092
358.796676	12717.020392	29.380109
359.345556	12730.674515	29.385127
359.411381	12751.285331	29.390144
360.079463	12769.979734	29.395162
360.892089	12772.224202	29.400180
360.889291	12791.832132	29.405197
361.725839	12809.783345	29.410215
361.996273	12819.615894	29.415232
362.431558	12835.498410	29.420250
362.832858	12839.064159	29.425268
363.291445	12848.276725	29.430285
363.522896	12862.659614	29.435303
363.842854	12878.639179	29.440320
364.066939	12883.710593	29.445338
364.268907	12896.092859	29.450356
364.724084	12920.290250	29.455373
364.725725	12932.309180	29.460391
364.986959	12951.102229	29.465408
365.586865	12970.079090	29.470426
365.931794	12982.066385	29.475444
366.230064	13010.087444	29.480461
366.706357	13032.421654	29.485479
366.862750	13047.081707	29.490496
367.320693	13064.040878	29.495514
367.883618	13076.275142	29.500532
367.873133	13101.812038	29.505549
368.542011	13117.253986	29.510567
368.651574	13133.263565	29.515584
369.182557	13149.276621	29.520602
369.620924	13163.750488	29.525620
369.824862	13188.091789	29.530637
370.243616	13195.851790	29.535655
370.365526	13218.942798	29.540672
371.146162	13226.428228	29.545690
371.396238	13247.806530	29.550708
371.772794	13264.829158	29.555725
372.302600	13272.909698	29.560743
372.164315	13304.580709	29.565760
372.750343	13309.709230	29.570778
373.169356	13331.563281	29.575796
372.838505	13358.922329	29.580813
373.798221	13377.104273	29.585831
374.287622	13393.439848	29.590848
374.458752	13418.999251	29.595866
375.294652	13443.516634	29.600884
375.368116	13463.890180	29.605901
375.678547	13474.920002	29.610919
376.187722	13499.807594	29.615936
376.448459	13517.909681	29.620954
377.124856	13541.987950	29.625972
377.433963	13558.677185	29.630989
377.871349	13575.580034	29.636007
378.156059	13596.406967	29.641024
378.714666	13607.893802	29.646042
378.848825	13624.531548	29.651060
379.193077	13647.796680	29.656077
379.620723	13673.881532	29.661095
379.898846	13686.849255	29.666112
380.292326	13716.432304	29.671130
380.819522	13731.066384	29.676148
381.301053	13762.318950	29.681165
381.704960	13768.906720	29.686183
382.181899	13787.878401	29.691200
381.984168	13814.336156	29.696218
382.860009	13829.885224	29.701236
383.219062	13848.897538	29.706253
383.721064	13860.690252	29.711271
383.876807	13882.260897	29.716288
384.629130	13906.975141	29.721306
384.840144	13922.780011	29.726324
385.116199	13944.192925	29.731341
385.465620	13964.012173	29.736359
385.579582	13987.130625	29.741376
385.762657	14012.868967	29.746394
386.449097	14031.097505	29.751412
386.883959	14053.947864	29.756429
387.225055	14072.388442	29.761447
387.624869	14099.210918	29.766464
388.321582	14118.805390	29.771482
388.987959	14132.950581	29.776500
389.133507	14152.160863	29.781517
389.666190	14166.175431	29.786535
389.899530	14187.579520	29.791552
390.103059	14204.194275	29.796570
390.964995	14225.727329	29.801588
391.127249	14253.610466	29.806605
391.544215	14263.322912	29.811623
391.685894	14280.399034	29.816640
392.251701	14297.313993	29.821658
392.541074	14314.442807	29.826676
392.734466	14331.154004	29.831693
393.271272	14342.954200	29.836711
393.793387	14363.526876	29.841728
394.050784	14390.075205	29.846746
394.309880	14390.896985	29.851764
394.887651	14416.965660	29.856781
395.512509	14434.319950	29.861799
395.838290	14439.619031	29.866816
396.287027	14456.233496	29.871834
396.714029	14466.936137	29.876852
396.655732	14487.612495	29.881869
396.738512	14505.689709	29.886887
397.272269	14523.611031	29.891904
397.596524	14551.292370	29.896922
397.911630	14567.643628	29.901940
397.969183	14602.251651	29.906957
398.613920	14631.828351	29.911975
399.244157	14650.044182	29.916992
399.312318	14678.466939	29.922010
400.173481	14704.633738	29.927028
400.269568	14729.597123	29.932045
400.879604	14751.722918	29.937063
401.329136	14769.348160	29.942080
401.702509	14794.141867	29.947098
402.314281	14811.517501	29.952116
402.774558	14842.873077	29.957133
403.363708	14862.125129	29.962151
403.730076	14873.023832	29.967168
403.897282	14897.467822	29.972186
404.444882	14915.655794	29.977204
404.791588	14944.411147	29.982221
405.195471	14962.738531	29.987239
405.917020	14972.728931	29.992256
405.953293	14997.079860	29.997274
406.610294	15013.779045	30.002292
406.678676	15040.048376	30.007309
407.283879	15064.578728	30.012327
407.500131	15084.988490	30.017344
408.122201	15109.718387	30.022362
408.442176	15137.837089	30.027380
408.875197	15151.157384	30.032397
409.224016	15178.709455	30.037415
409.560092	15196.103358	30.042432
410.046806	15224.436100	30.047450
410.209624	15241.778226	30.052468
410.791261	15268.371737	30.057485
411.327817	15294.084865	30.062503
411.966737	15313.913864	30.067520
412.018980	15340.685147	30.072538
412.352981	15362.239019	30.077556
412.608971	15390.794488	30.082573
413.217191	15418.347331	30.087591
413.918231	15441.498761	30.092608
414.059377	15458.816053	30.097626
415.024760	15478.095072	30.102644
415.265641	15509.388198	30.107661
415.388935	15533.208211	30.112679
416.015612	15543.621199	30.117696
416.388610	15567.506367	30.122714
416.705388	15586.157511	30.127732
417.031100	15612.279936	30.132749
417.615364	15631.085045	30.137767
417.946493	15649.812962	30.142784
418.484117	15682.879107	30.147802
419.377951	15703.142337	30.152820
419.385751	15721.314562	30.157837
419.797555	15744.047384	30.162855
420.572595	15758.397853	30.167872
420.737056	15784.498395	30.172890
421.270584	15799.142553	30.177908
421.739458	15817.691140	30.182925
422.112065	15829.066330	30.187943
422.715551	15841.668719	30.192960
422.674018	15860.584709	30.197978
423.065511	15875.851268	30.202996
423.372348	15886.920955	30.208013
423.914925	15910.110408	30.213031
424.374393	15930.732490	30.218048
424.488859	15957.188522	30.223066
424.937446	15978.962021	30.228084
425.238674	15994.811329	30.233101
425.672304	16027.603784	30.238119
426.176309	16041.624227	30.243136
426.248827	16078.105518	30.248154
426.963009	16106.419729	30.253172
427.615446	16116.497361	30.258189
427.789774	16151.222545	30.263207
428.507133	16156.015433	30.268224
428.995661	16196.278770	30.273242
429.433206	16216.105505	30.278260
429.561573	16239.246532	30.283277
430.090729	16261.825773	30.288295
431.108656	16280.115093	30.293312
431.215883	16291.851130	30.298330
431.683391	16320.482240	30.303348
431.542859	16349.701354	30.308365
432.159417	16393.340410	30.313383
432.921648	16403.340986	30.318400
433.087246	16429.337995	30.323418
433.449876	16458.134186	30.328436
434.053602	16483.639406	30.333453
434.341178	16515.656471	30.338471
435.217987	16527.594278	30.343488
435.357778	16555.386371	30.348506
435.894887	16568.962983	30.353524
436.557558	16596.430030	30.358541
436.659516	16616.132866	30.363559
437.424234	16637.946035	30.368576
438.089697	16664.133541	30.373594
438.762576	16678.500705	30.378612
439.014342	16704.838345	30.383629
439.168148	16725.221732	30.388647
439.900578	16734.317491	30.393664
440.131780	16758.403230	30.398682
440.499052	16776.652805	30.403700
441.077236	16810.336773	30.408717
441.113600	16840.106936	30.413735
441.672348	16854.248901	30.418752
442.346485	16875.574318	30.423770
442.388259	16905.694335	30.428788
443.066383	16924.204901	30.433805
443.292584	16954.005518	30.438823
443.936785	16975.939023	30.443840
444.346620	17004.434890	30.448858
444.795691	17033.063631	30.453876
445.046152	17059.878907	30.458893
445.418996	17079.031253	30.463911
446.127469	17099.577685	30.468928
446.223467	17123.909318	30.473946
446.775074	17158.378232	30.478964
447.630619	17189.761016	30.483981
447.906479	17213.894025	30.488999
448.421688	17228.387374	30.494016
448.891223	17277.102092	30.499034
448.948075	17284.800426	30.504052
449.423042	17312.345275	30.509069
450.017069	17339.738852	30.514087
450.539059	17355.286219	30.519104
450.848727	17389.989277	30.524122
451.263157	17410.184109	30.529140
452.022938	17423.944395	30.534157
452.379724	17460.206890	30.539175
453.014463	17473.203450	30.544192
453.173719	17485.718571	30.549210
453.478804	17519.715040	30.554228
453.968702	17523.864791	30.559245
454.108161	17551.917381	30.564263
455.055791	17572.306830	30.569280
455.414203	17605.328543	30.574298
455.377555	17625.202576	30.579316
456.116340	17650.918772	30.584333
456.534539	17685.074701	30.589351
457.170189	17716.037934	30.594368
457.268941	17747.331689	30.599386
457.760575	17780.673974	30.604404
458.860372	17809.056642	30.609421
459.092101	17829.558495	30.614439
459.492232	17863.351158	30.619456
459.835663	17881.245419	30.624474
460.115483	17908.663748	30.629492
461.316932	17936.525285	30.634509
461.704527	17970.913941	30.639527
462.089609	17991.859440	30.644544
462.453524	18002.302291	30.649562
462.755345	18042.428153	30.654580
463.233549	18059.271717	30.659597
463.609499	18084.312490	30.664615
464.228094	18116.353012	30.669632
464.776353	18143.445340	30.674650
464.896391	18175.993641	30.679668
465.453130	18198.586626	30.684685
465.922022	18229.343050	30.689703
466.363707	18259.099290	30.694720
466.961283	18289.810384	30.699738
467.236030	18320.521550	30.704756
468.189413	18344.568801	30.709773
468.471854	18373.642588	30.714791
468.785876	18400.557164	30.719808
469.204409	18432.383157	30.724826
469.579835	18461.928969	30.729844
470.154449	18499.492311	30.734861
470.710221	18530.065026	30.739879
471.612805	18551.782958	30.744896
472.111315	18577.462210	30.749914
472.572350	18601.624803	30.754932
473.371513	18627.863527	30.759949
473.708402	18653.738771	30.764967
473.986659	18670.146674	30.769984
474.303978	18687.906780	30.775002
474.888841	18711.014010	30.780020
475.460668	18732.272215	30.785037
475.861885	18763.532868	30.790055
476.486778	18784.776502	30.795072
477.103422	18807.057562	30.800090
477.301380	18831.564899	30.805108
477.838060	18853.106723	30.810125
478.678885	18881.556801	30.815143
478.862455	18900.904859	30.820160
479.349016	18921.734382	30.825178
479.694473	18945.100511	30.830196
480.385278	18955.265237	30.835213
480.809659	18982.321279	30.840231
481.172345	19007.321095	30.845248
481.604691	19033.055537	30.850266
481.919553	19054.897677	30.855284
482.366762	19080.124426	30.860301
482.840187	19103.616012	30.865319
483.103631	19122.181002	30.870336
483.909895	19141.179053	30.875354
484.479098	19170.316519	30.880372
484.912987	19184.817756	30.885389
485.097867	19206.282398	30.890407
485.817706	19225.868996	30.895424
486.151226	19245.206545	30.900442
486.423878	19270.283980	30.905460
487.109295	19286.116881	30.910477
487.805952	19316.851987	30.915495
488.339252	19341.345349	30.920512
489.083542	19367.473628	30.925530
489.207194	19393.686515	30.930548
489.607990	19402.645948	30.935565
490.005774	19430.951414	30.940583
490.543819	19455.418904	30.945600
491.092844	19479.840479	30.950618
491.394979	19518.143442	30.955636
491.864692	19533.207946	30.960653
492.423489	19568.166501	30.965671
492.606592	19600.934753	30.970688
493.404311	19622.493407	30.975706
493.628471	19659.077723	30.980724
494.171018	19687.449339	30.985741
494.442096	19723.862159	30.990759
495.105627	19753.446940	30.995776
495.946903	19787.161214	31.000794
496.237432	19819.906688	31.005812
496.832031	19847.733347	31.010829
497.125784	19878.330265	31.015847
497.519827	19908.993659	31.020864
498.375576	19940.848408	31.025882
498.871845	19972.866921	31.030900
499.520470	19998.783578	31.035917
500.049635	20031.612075	31.040935
500.836291	20063.755845	31.045952
501.342724	20085.341680	31.050970
501.583449	20112.017372	31.055988
502.085422	20147.251227	31.061005
502.525171	20166.010731	31.066023
503.526861	20201.204324	31.071040
504.028403	20223.132260	31.076058
504.060758	20257.517408	31.081076
504.873196	20278.088840	31.086093
505.061199	20302.372125	31.091111
505.704527	20334.197604	31.096128
506.444400	20355.115350	31.101146
506.969265	20394.004329	31.106164
507.335037	20411.215045	31.111181
507.676382	20438.178699	31.116199
508.458150	20474.146466	31.121216
508.998815	20501.641316	31.126234
509.126249	20521.176682	31.131252
509.696856	20551.093140	31.136269
510.030424	20577.723333	31.141287
510.469950	20612.001100	31.146304
511.198341	20637.874519	31.151322
511.220052	20672.925487	31.156340
511.989376	20708.459668	31.161357
512.556367	20741.327657	31.166375
513.388899	20772.056409	31.171392
514.262769	20799.177251	31.176410
514.422998	20824.027867	31.181428
514.799646	20840.567506	31.186445
515.285833	20873.069268	31.191463
515.976901	20910.031395	31.196480
516.576395	20929.050940	31.201498
517.217154	20958.356781	31.206516
517.791545	20981.184011	31.211533
518.291595	20996.718776	31.216551
518.516212	21008.385567	31.221568
519.305755	21028.462217	31.226586
519.464958	21063.536575	31.231604
520.095236	21082.027014	31.236621
520.455016	21095.372358	31.241639
520.644914	21136.520423	31.246656
521.329387	21162.647836	31.251674
522.090680	21185.534490	31.256692
522.242283	21217.766981	31.261709
522.785811	21249.066182	31.266727
523.624321	21283.396364	31.271744
523.694249	21305.810136	31.276762
523.983834	21331.506774	31.281780
524.666675	21368.654291	31.286797
525.510524	21397.480359	31.291815
525.847308	21443.945263	31.296832
526.042033	21471.154448	31.301850
526.615575	21507.763308	31.306868
527.321054	21543.915586	31.311885
527.947279	21577.868820	31.316903
528.794093	21611.105149	31.321920
529.315852	21640.860313	31.326938
529.849424	21673.633996	31.331956
530.367422	21704.900008	31.336973
531.224924	21731.822505	31.341991
531.503963	21768.749679	31.347008
532.096303	21797.015448	31.352026
532.711609	21821.467473	31.357044
533.276117	21842.667022	31.362061
534.105884	21874.377334	31.367079
534.398954	21898.721955	31.372096
535.035366	21923.518332	31.377114
535.792491	21959.574822	31.382132
536.119715	21989.531587	31.387149
536.734585	22016.599894	31.392167
537.192423	22028.989016	31.397184
537.923603	22057.650453	31.402202
538.415147	22092.447110	31.407220
538.594215	22123.495160	31.412237
539.398394	22140.676639	31.417255
539.451616	22184.912921	31.422272
540.330305	22208.218379	31.427290
540.576517	22238.200846	31.432308
540.988939	22273.111314	31.437325
541.429578	22297.572329	31.442343
542.152615	22343.839837	31.447360
542.828426	22377.559200	31.452378
543.466422	22414.286024	31.457396
543.734342	22445.984149	31.462413
544.585671	22479.353931	31.467431
544.956170	22518.625139	31.472448
545.273223	22544.028380	31.477466
546.050263	22588.468144	31.482484
546.329200	22622.635540	31.487501
546.812612	22646.237225	31.492519
547.546064	22696.642859	31.497536
548.497111	22721.422554	31.502554
549.056635	22756.980650	31.507572
549.363522	22784.249901	31.512589
550.019738	22806.927411	31.517607
550.686740	22838.551020	31.522624
551.477194	22871.678237	31.527642
551.678067	22900.828372	31.532660
552.042122	22931.956138	31.537677
552.533939	22958.975498	31.542695
553.212985	23000.480523	31.547712
553.767274	23013.872531	31.552730
554.559030	23048.288934	31.557748
555.193700	23069.826362	31.562765
555.793309	23098.314022	31.567783
556.376688	23125.312948	31.572800
557.036530	23139.067658	31.577818
557.166398	23171.420475	31.582836
557.734719	23199.748883	31.587853
558.237608	23227.430385	31.592871
558.785089	23253.607298	31.597888
559.183385	23284.616508	31.602906
560.263747	23313.477844	31.607924
559.937689	23345.687498	31.612941
560.704885	23369.965988	31.617959
561.520376	23413.270438	31.622976
562.437144	23445.715312	31.627994
562.764071	23473.778593	31.633012
563.065520	23508.961384	31.638029
563.695047	23528.806556	31.643047
563.792592	23566.504853	31.648064
564.696392	23608.576278	31.653082
565.221897	23640.488735	31.658100
565.847369	23682.212111	31.663117
566.734132	23710.668313	31.668135
566.958113	23748.220765	31.673152
567.910010	23780.085623	31.678170
568.540537	23811.286778	31.683188
569.060229	23848.831021	31.688205
569.843418	23878.586516	31.693223
570.617104	23909.304089	31.698240
571.243538	23942.692597	31.703258
571.740665	23967.785081	31.708276
572.030976	23993.466096	31.713293
572.853093	24013.730267	31.718311
573.288003	24051.515669	31.723328
573.815005	24083.921517	31.728346
574.708697	24111.486167	31.733364
575.322896	24149.597564	31.738381
575.767181	24169.503985	31.743399
575.876332	24203.346793	31.748416
576.603592	24235.411869	31.753434
577.340457	24268.044246	31.758452
577.524151	24303.240559	31.763469
578.486091	24334.466462	31.768487
579.259484	24374.866299	31.773504
579.690420	24391.830132	31.778522
580.597234	24425.440956	31.783540
580.714552	24459.718967	31.788557
581.322974	24496.959832	31.793575
581.984754	24528.498471	31.798592
582.148004	24554.730950	31.803610
582.854200	24597.164027	31.808628
583.566604	24641.372033	31.813645
584.353495	24666.849747	31.818663
585.027310	24704.858071	31.823680
585.381671	24720.254268	31.828698
586.166974	24748.064281	31.833716
586.295091	24790.841091	31.838733
587.111318	24826.444830	31.843751
587.973216	24857.971605	31.848768
588.410883	24885.153728	31.853786
588.762936	24915.496507	31.858804
589.489891	24952.997722	31.863821
590.010212	24978.220556	31.868839
590.430016	25012.768123	31.873856
591.187057	25051.579315	31.878874
591.785023	25084.866753	31.883892
592.211917	25115.988082	31.888909
592.801434	25154.143175	31.893927
593.384792	25188.715987	31.898944
594.065962	25207.347663	31.903962
594.798100	25231.943583	31.908980
595.149126	25270.382720	31.913997
595.778080	25296.309399	31.919015
596.347110	25320.438026	31.924032
596.623663	25363.824790	31.929050
597.249016	25393.525102	31.934068
598.029303	25426.304244	31.939085
598.108425	25463.061012	31.944103
598.833711	25499.672409	31.949120
599.447871	25550.053369	31.954138
600.119970	25578.703851	31.959156
600.311103	25626.579052	31.964173
601.112203	25660.745699	31.969191
602.259842	25702.966620	31.974208
602.498199	25750.973759	31.979226
603.300919	25782.776695	31.984244
603.924700	25827.272950	31.989261
604.501541	25860.760900	31.994279
605.391961	25901.600523	31.999296
605.777832	25939.169638	32.004314
606.638794	25968.005977	32.009332
607.240324	26011.886761	32.014349
608.129795	26043.904045	32.019367
608.826253	26077.202981	32.024384
609.159751	26124.955946	32.029402
609.661668	26144.962744	32.034420
610.640341	26194.630938	32.039437
611.455336	26211.839527	32.044455
612.114022	26242.894695	32.049472
612.588800	26278.074153	32.054490
613.364249	26293.140163	32.059508
613.904085	26335.350159	32.064525
614.904242	26371.325999	32.069543
615.725400	26386.991656	32.074560
615.858261	26413.446200	32.079578
616.758530	26433.403538	32.084596
617.221417	26466.594333	32.089613
617.964767	26497.314304	32.094631
618.479379	26517.344764	32.099648
618.840690	26540.028459	32.104666
619.490835	26576.609340	32.109684
619.779288	26621.197782	32.114701
620.386332	26648.975143	32.119719
621.502285	26682.139857	32.124736
621.854502	26707.978970	32.129754
622.754850	26739.439473	32.134772
623.290746	26770.666370	32.139789
623.420708	26802.070655	32.144807
624.274872	26833.481655	32.149824
624.847958	26872.881353	32.154842
625.734601	26909.425798	32.159860
625.825263	26953.224305	32.164877
626.798406	26977.569723	32.169895
627.517261	27018.229904	32.174912
628.148006	27051.964203	32.179930
628.551210	27091.074912	32.184948
629.040809	27125.501397	32.189965
629.598471	27158.804892	32.194983
630.276307	27188.227851	32.200000
630.948568	27236.973251	32.205018
631.622373	27274.468149	32.210036
631.851495	27313.505422	32.215053
632.372520	27354.747138	32.220071
633.440211	27390.417155	32.225088
633.856203	27432.781562	32.230106
634.711969	27455.489972	32.235124
635.274603	27497.799946	32.240141
635.835519	27528.499490	32.245159
636.533729	27561.503531	32.250176
636.988626	27592.282980	32.255194
638.093186	27632.087598	32.260212
638.604984	27661.290746	32.265229
638.825420	27684.610877	32.270247
639.515248	27726.661226	32.275264
640.021450	27770.933663	32.280282
640.775830	27804.276935	32.285300
641.248583	27842.790381	32.290317
642.168204	27878.452843	32.295335
642.711992	27912.063135	32.300352
643.199026	27955.131734	32.305370
644.001775	27992.803703	32.310388
644.465506	28032.178530	32.315405
645.295917	28083.764454	32.320423
646.133687	28127.947817	32.325440
646.776952	28160.841342	32.330458
647.196758	28192.196058	32.335476
648.039375	28239.172660	32.340493
648.511843	28280.872629	32.345511
649.463714	28318.749394	32.350528
649.778818	28366.030128	32.355546
650.524211	28398.073700	32.360564
651.009392	28437.578686	32.365581
651.962847	28488.653342	32.370599
652.887051	28514.822346	32.375616
653.337728	28564.439972	32.380634
654.276193	28598.217135	32.385652
655.201707	28636.408339	32.390669
655.461326	28676.859316	32.395687
656.551127	28693.072532	32.400704
657.017103	28739.199065	32.405722
657.995198	28784.480670	32.410740
658.214423	28820.159654	32.415757
658.864919	28852.433712	32.420775
659.487154	28883.182582	32.425792
659.549533	28924.246462	32.430810
660.208166	28971.215635	32.435828
661.387090	29016.927734	32.440845
661.963490	29061.963134	32.445863
662.841375	29102.602569	32.450880
663.452926	29147.866530	32.455898
664.061324	29184.389106	32.460916
664.924016	29229.203049	32.465933
665.287888	29270.163515	32.470951
666.433289	29301.709707	32.475968
666.970085	29343.420729	32.480986
667.630085	29367.925513	32.486004
668.276230	29413.696651	32.491021
668.713123	29459.993707	32.496039
669.501622	29487.676992	32.501056
670.076326	29547.764312	32.506074
670.587048	29567.248446	32.511092
671.360371	29614.978632	32.516109
671.973919	29661.033556	32.521127
673.024660	29695.344890	32.526144
673.474561	29739.731542	32.531162
674.032710	29788.658929	32.536180
675.085730	29822.736235	32.541197
675.798369	29862.429587	32.546215
676.890673	29894.933194	32.551232
677.495475	29937.873736	32.556250
677.627087	29966.918470	32.561268
678.679578	29996.071882	32.566285
678.993757	30039.709240	32.571303
679.550764	30068.162831	32.576320
680.171325	30107.555011	32.581338
680.710816	30138.792818	32.586356
681.717039	30183.965646	32.591373
682.011947	30204.230100	32.596391
682.541470	30253.694067	32.601408
683.036036	30286.633256	32.606426
683.458408	30324.628261	32.611444
684.439289	30368.907828	32.616461
684.994154	30424.898231	32.621479
685.772663	30456.781801	32.626496
686.542935	30509.875100	32.631514
687.242033	30548.781716	32.636532
687.872578	30592.339090	32.641549
687.928152	30638.862867	32.646567
689.066733	30689.907687	32.651584
689.571773	30731.177666	32.656602
690.712336	30777.847916	32.661620
691.408917	30825.687747	32.666637
691.823440	30885.007533	32.671655
692.683121	30915.020565	32.676672
693.270062	30970.988458	32.681690
694.240306	31016.857795	32.686708
695.289290	31068.258946	32.691725
695.561078	31115.881500	32.696743
696.653384	31157.205757	32.701760
697.239991	31206.555595	32.706778
697.838503	31251.023366	32.711796
698.636419	31286.774032	32.716813
699.271372	31331.052940	32.721831
700.116046	31372.220434	32.726848
700.956226	31424.533885	32.731866
701.782413	31470.433108	32.736884
702.232492	31519.330941	32.741901
702.838873	31556.262624	32.746919
703.571545	31596.095248	32.751936
704.604129	31636.095922	32.756954
705.469817	31687.325017	32.761972
706.153247	31724.156427	32.766989
706.858964	31762.868312	32.772007
707.883750	31800.436627	32.777024
708.494189	31840.042310	32.782042
709.196238	31872.774519	32.787060
710.371936	31903.599267	32.792077
710.720046	31951.312932	32.797095
711.518011	31985.351569	32.802112
711.899294	32029.519965	32.807130
712.713631	32063.082023	32.812148
713.612153	32098.179821	32.817165
714.378323	32133.032883	32.822183
715.197759	32171.904736	32.827200
715.903628	32206.078273	32.832218
716.311164	32244.641771	32.837236
717.341755	32281.451412	32.842253
717.857107	32322.893633	32.847271
718.492723	32352.210486	32.852288
719.193946	32390.108706	32.857306
719.829033	32435.116975	32.862324
720.425119	32469.952983	32.867341
721.027981	32513.177333	32.872359
721.999193	32553.948030	32.877376
722.737191	32595.747893	32.882394
722.980747	32633.244071	32.887412
723.964658	32681.327672	32.892429
724.417429	32729.247998	32.897447
725.446820	32766.823661	32.902464
726.133390	32808.271643	32.907482
726.420908	32849.042508	32.912500
727.259803	32888.241400	32.917517
727.750611	32934.088895	32.922535
728.843783	32973.184906	32.927552
729.421266	33020.763939	32.932570
730.275797	33064.847770	32.937588
731.105261	33099.281592	32.942605
731.460349	33125.804789	32.947623
732.139771	33165.674042	32.952640
732.689902	33221.950892	32.957658
733.179214	33265.656103	32.962676
734.117691	33306.635710	32.967693
734.966424	33367.519386	32.972711
735.611931	33413.299448	32.977728
736.554160	33450.668710	32.982746
737.299104	33508.369954	32.987764
738.183225	33542.814915	32.992781
739.140271	33591.872136	32.997799
739.980906	33621.247178	33.002816
740.855769	33674.231010	33.007834
741.311254	33714.654812	33.012852
742.106610	33749.000209	33.017869
743.109516	33799.726174	33.022887
743.746213	33840.810985	33.027904
744.591509	33880.693558	33.032922
745.400399	33928.004479	33.037940
746.234790	33962.179729	33.042957
746.814554	34007.882868	33.047975
747.609506	34045.231995	33.052992
747.956834	34086.476407	33.058010
748.643959	34148.481449	33.063028
749.519859	34183.554681	33.068045
750.255835	34238.211868	33.073063
751.173175	34287.213705	33.078080
752.160156	34320.840869	33.083098
752.666890	34371.532107	33.088116
753.238229	34411.325812	33.093133
754.340145	34467.633394	33.098151
755.152051	34508.995558	33.103168
755.857654	34554.319786	33.108186
756.500452	34600.494860	33.113204
757.758322	34640.921242	33.118221
758.009780	34696.262468	33.123239
758.991079	34741.752573	33.128256
759.737858	34781.329822	33.133274
760.331778	34824.187289	33.138292
761.529791	34865.205166	33.143309
762.295059	34913.859232	33.148327
762.802451	34960.277594	33.153344
763.644686	34995.692557	33.158362
764.175488	35046.065505	33.163380
765.301458	35085.368968	33.168397
765.806007	35138.351244	33.173415
766.429288	35179.314308	33.178432
767.187937	35219.731456	33.183450
768.149514	35272.490751	33.188468
769.247577	35314.302866	33.193485
769.697123	35362.438345	33.198503
770.329279	35403.318255	33.203520
771.595918	35444.452970	33.208538
772.354708	35494.525719	33.213556
773.403093	35523.877208	33.218573
773.707799	35574.735747	33.223591
774.434804	35616.973298	33.228608
775.550528	35656.665129	33.233626
776.026425	35705.910106	33.238644
777.197373	35745.315244	33.243661
777.564052	35783.246676	33.248679
778.479999	35826.258080	33.253696
779.783067	35850.144980	33.258714
779.879425	35871.539900	33.263732
780.484845	35910.452184	33.268749
781.125306	35953.721970	33.273767
781.884468	35991.510114	33.278784
782.811386	36027.678636	33.283802
783.142411	36074.550701	33.288820
783.730993	36114.028751	33.293837
784.690510	36161.175652	33.298855
785.684357	36211.959415	33.303872
786.121094	36249.646751	33.308890
786.703827	36309.878692	33.313908
787.717101	36350.226506	33.318925
788.315476	36396.393479	33.323943
788.997906	36464.640711	33.328960
790.008824	36503.269268	33.333978
791.088546	36560.926416	33.338996
791.783199	36611.201536	33.344013
792.690785	36660.311564	33.349031
793.297755	36719.440615	33.354048
794.302708	36765.740741	33.359066
795.216817	36812.156368	33.364084
796.080292	36863.891628	33.369101
796.385364	36916.675605	33.374119
796.894632	36968.131445	33.379136
797.985177	37021.861332	33.384154
798.768833	37082.652063	33.389172
799.595315	37136.543733	33.394189
800.892668	37184.190132	33.399207
801.598324	37243.943845	33.404224
802.794448	37293.547640	33.409242
803.412949	37344.310669	33.414260
804.124613	37394.218204	33.419277
805.188164	37437.039012	33.424295
805.967714	37490.610100	33.429312
806.975832	37533.294339	33.434330
807.383136	37583.901301	33.439348
808.278533	37634.299156	33.444365
809.055018	37682.837646	33.449383
809.788586	37739.325403	33.454400
810.707666	37787.563563	33.459418
811.618561	37845.294876	33.464436
812.493510	37878.964196	33.469453
813.154796	37937.601182	33.474471
814.080729	37990.239988	33.479488
815.055315	38028.206684	33.484506
815.785678	38083.835827	33.489524
816.489491	38134.473538	33.494541
817.310767	38181.716105	33.499559
818.430265	38229.411652	33.504576
819.397986	38275.986473	33.509594
820.060870	38320.718323	33.514612
821.215523	38360.535568	33.519629
822.109739	38400.943839	33.524647
823.119051	38453.456895	33.529664
823.628749	38488.272060	33.534682
824.458555	38534.869038	33.539700
825.075918	38575.567618	33.544717
826.317564	38618.767623	33.549735
827.172468	38658.657654	33.554752
827.929079	38702.338506	33.559770
828.746796	38743.885051	33.564788
829.504264	38788.444963	33.569805
830.217924	38823.361533	33.574823
830.661742	38874.636144	33.579840
831.922141	38921.716714	33.584858
832.598743	38959.326983	33.589876
833.131058	39005.769195	33.594893
833.962339	39049.495973	33.599911
834.482454	39095.813809	33.604928
835.444862	39128.212916	33.609946
836.125995	39158.505951	33.614964
836.915306	39213.464757	33.619981
837.723451	39253.571903	33.624999
838.362478	39318.167049	33.630016
839.409830	39353.734195	33.635034
839.735220	39400.456295	33.640052
840.673201	39462.393212	33.645069
841.629132	39510.819183	33.650087
842.640150	39565.718870	33.655104
843.437167	39616.939932	33.660122
844.200850	39667.692022	33.665140
845.028553	39723.405008	33.670157
845.804495	39769.020186	33.675175
846.751559	39828.774882	33.680192
847.922848	39882.549862	33.685210
848.920443	39941.550699	33.690228
849.295650	39991.972275	33.695245
850.226120	40043.198742	33.700263
851.187859	40102.053847	33.705280
852.215486	40141.913243	33.710298
853.199752	40200.929519	33.715316
853.587972	40258.053449	33.720333
854.919402	40306.700669	33.725351
855.318799	40371.178359	33.730368
856.386041	40419.658496	33.735386
857.364386	40484.532844	33.740404
857.935157	40533.830930	33.745421
859.471178	40585.280074	33.750439
860.457682	40649.793144	33.755456
860.980286	40696.012810	33.760474
862.402954	40738.334901	33.765492
863.278351	40791.361579	33.770509
863.939405	40843.928638	33.775527
864.926446	40896.223420	33.780544
866.170813	40934.918243	33.785562
866.771580	40987.121939	33.790580
867.376424	41041.077024	33.795597
868.363890	41080.501710	33.800615
868.841811	41133.483939	33.805632
870.104677	41196.355230	33.810650
870.925020	41240.322140	33.815668
871.653869	41281.754640	33.820685
872.633572	41330.724858	33.825703
873.153108	41394.769329	33.830720
874.178061	41437.623079	33.835738
875.289931	41500.367096	33.840756
876.059405	41547.106477	33.845773
877.334918	41599.414694	33.850791
878.064002	41645.591386	33.855808
878.790759	41690.402394	33.860826
879.855781	41731.093708	33.865844
880.575909	41789.175299	33.870861
881.267548	41830.627314	33.875879
882.538643	41894.422740	33.880896
883.179109	41938.792382	33.885914
883.689095	41984.542382	33.890932
884.671411	42046.916109	33.895949
885.441642	42093.941155	33.900967
886.683873	42150.512531	33.905984
887.882811	42199.406087	33.911002
888.906313	42242.305914	33.916020
889.507973	42300.616128	33.921037
890.431562	42348.338746	33.926055
891.281603	42394.643546	33.931072
892.382451	42443.464456	33.936090
893.412482	42461.727980	33.941108
894.090306	42510.235778	33.946125
894.904411	42546.217834	33.951143
895.488190	42590.388942	33.956160
896.387942	42634.611862	33.961178
897.318235	42671.145181	33.966196
898.215171	42721.877171	33.971213
899.162913	42751.943701	33.976231
899.877690	42800.205999	33.981248
900.636241	42847.462187	33.986266
901.811382	42893.318651	33.991284
902.335470	42944.976072	33.996301
903.536918	42998.513640	34.001319
903.971062	43052.260035	34.006336
904.819962	43106.561481	34.011354
906.271896	43146.954479	34.016372
907.029841	43213.123787	34.021389
908.131849	43255.064518	34.026407
908.463003	43312.888446	34.031424
909.418252	43373.246097	34.036442
910.720258	43419.501255	34.041460
911.660062	43474.175210	34.046477
912.784667	43523.070694	34.051495
913.616857	43589.343355	34.056512
914.464013	43637.744885	34.061530
915.611909	43687.453049	34.066548
915.998269	43738.223039	34.071565
916.913445	43794.413395	34.076583
917.687997	43856.299762	34.081600
918.710924	43917.881745	34.086618
919.901762	43973.466432	34.091636
920.803281	44029.450783	34.096653
921.930577	44082.110700	34.101671
922.917554	44148.038194	34.106688
923.898338	44191.916292	34.111706
924.695779	44244.248714	34.116724
925.575330	44311.060103	34.121741
926.720142	44365.343600	34.126759
927.617479	44406.072433	34.131776
928.069838	44465.695804	34.136794
929.368543	44522.245432	34.141812
930.170612	44583.882818	34.146829
931.511807	44640.736048	34.151847
932.363818	44699.823049	34.156864
933.270822	44752.702489	34.161882
934.688560	44796.026288	34.166900
935.295723	44856.537355	34.171917
936.782980	44903.380190	34.176935
937.364357	44947.872650	34.181952
937.776534	44995.326809	34.186970
939.093112	45042.955744	34.191988
939.979833	45105.890737	34.197005
941.002482	45158.790986	34.202023
942.000302	45208.393208	34.207040
943.019131	45275.413403	34.212058
943.941147	45312.578622	34.217076
945.097759	45365.009254	34.222093
945.854630	45415.978080	34.227111
946.954431	45457.170545	34.232128
947.765001	45511.426931	34.237146
948.479915	45561.498064	34.242164
949.414068	45619.227228	34.247181
950.255901	45670.404735	34.252199
951.302512	45725.440719	34.257216
951.930129	45780.460205	34.262234
953.397474	45835.512819	34.267252
953.981472	45889.071787	34.272269
954.932356	45940.523829	34.277287
955.817121	45984.692502	34.282304
956.917760	46032.502854	34.287322
957.748279	46079.242229	34.292340
958.407282	46119.334621	34.297357
959.122795	46169.147649	34.302375
959.845081	46225.658994	34.307392
960.959965	46283.355242	34.312410
961.748672	46328.052041	34.317428
963.222828	46400.204325	34.322445
964.131480	46448.785775	34.327463
964.863331	46491.802734	34.332480
965.944922	46562.739131	34.337498
966.757946	46613.537402	34.342516
967.847391	46672.662013	34.347533
968.693887	46732.330912	34.352551
969.987336	46791.746528	34.357568
970.865802	46856.832297	34.362586
972.036979	46917.488348	34.367604
972.895691	46974.296519	34.372621
973.777269	47030.171294	34.377639
974.750652	47084.190887	34.382656
975.722699	47152.520886	34.387674
976.995866	47208.663756	34.392692
978.232577	47267.102603	34.397709
978.370357	47325.163273	34.402727
980.110942	47387.572397	34.407744
980.861056	47437.686472	34.412762
981.902624	47501.843888	34.417780
983.105851	47555.385771	34.422797
984.137444	47617.982456	34.427815
985.211739	47662.377798	34.432832
986.235716	47734.199939	34.437850
987.453004	47791.112178	34.442868
988.058872	47842.489721	34.447885
989.334936	47902.474035	34.452903
990.589298	47954.623352	34.457920
990.935838	48012.551867	34.462938
991.973000	48060.218292	34.467956
993.198393	48125.544407	34.472973
994.182524	48190.136641	34.477991
995.554537	48247.392741	34.483008
996.188669	48303.454908	34.488026
997.409833	48355.325646	34.493044
998.457244	48410.127635	34.498061
999.401871	48478.832864	34.503079
1000.247242	48538.443425	34.508096
1001.071279	48590.762805	34.513114
1002.081490	48641.180452	34.518132
1002.917832	48705.518912	34.523149
1003.662941	48770.985344	34.528167
1005.312303	48825.896541	34.533184
1006.483960	48887.298012	34.538202
1007.767111	48925.595746	34.543220
1008.562342	48979.160577	34.548237
1009.875573	49042.185267	34.553255
1010.807543	49086.776498	34.558272
1011.976666	49142.111624	34.563290
1013.063733	49189.266451	34.568308
1014.262231	49246.185271	34.573325
1014.915826	49298.336826	34.578343
1016.249466	49344.751084	34.583360
1017.016842	49400.681197	34.588378
1018.142519	49448.210128	34.593396
1018.786089	49500.623116	34.598413
1019.673220	49559.160547	34.603431
1020.940664	49597.594735	34.608448
1021.676746	49650.670568	34.613466
1022.583554	49701.758424	34.618484
1023.524457	49755.314917	34.623501
1023.975364	49801.071105	34.628519
1025.228962	49843.126932	34.633536
1025.934795	49906.761592	34.638554
1026.831667	49954.928468	34.643572
1028.114344	50018.561701	34.648589
1028.915163	50071.027296	34.653607
1029.901874	50126.943819	34.658624
1030.852525	50187.352059	34.663642
1031.968424	50242.533670	34.668660
1032.985443	50304.640156	34.673677
1034.069343	50371.715829	34.678695
1035.439168	50436.057872	34.683712
1036.295866	50495.298443	34.688730
1037.261594	50552.326547	34.693748
1038.336388	50620.859634	34.698765
1039.251277	50688.683998	34.703783
1040.935638	50741.829005	34.708800
1042.067534	50803.475939	34.713818
1042.923981	50865.862169	34.718836
1043.687409	50913.957034	34.723853
1044.165926	50985.153455	34.728871
1045.935296	51042.854193	34.733888
1046.869800	51106.848657	34.738906
1048.169038	51177.259124	34.743924
1049.019568	51243.779093	34.748941
1050.300551	51303.765218	34.753959
1051.695884	51367.295951	34.758976
1052.304814	51433.632830	34.763994
1053.338621	51490.810777	34.769012
1054.425362	51554.586490	34.774029
1055.367256	51614.221548	34.779047
1057.017378	51687.432342	34.784064
1057.803923	51749.294053	34.789082
1058.866641	51806.012667	34.794100
1060.438089	51850.926752	34.799117
1061.209142	51931.305894	34.804135
1062.714907	51980.514304	34.809152
1063.589694	52047.336503	34.814170
1064.498391	52100.637715	34.819188
1065.801835	52157.268875	34.824205
1066.398874	52216.022975	34.829223
1067.995196	52273.785514	34.834240
1068.650951	52336.631075	34.839258
1069.664926	52389.694996	34.844276
1071.110828	52451.037711	34.849293
1071.808225	52519.382384	34.854311
1073.145110	52574.724789	34.859328
1074.191587	52642.116624	34.864346
1075.330944	52699.135477	34.869364
1076.686485	52751.254523	34.874381
1077.861227	52815.956435	34.879399
1079.114681	52860.707113	34.884416
1080.112978	52918.950881	34.889434
1081.079914	52976.149275	34.894452
1082.327179	53026.425489	34.899469
1083.444058	53086.264724	34.904487
1084.649642	53130.732331	34.909504
1085.295225	53191.196151	34.914522
1086.560666	53249.557117	34.919540
1087.506822	53299.254591	34.924557
1088.617777	53356.779406	34.929575
1090.009752	53418.088811	34.934592
1090.827967	53469.021653	34.939610
1091.868230	53522.742147	34.944628
1093.223322	53578.571338	34.949645
1093.974659	53637.020087	34.954663
1095.049464	53685.040284	34.959680
1096.366193	53734.895820	34.964698
1097.235008	53785.954318	34.969716
1098.221891	53818.079697	34.974733
1099.077015	53870.678256	34.979751
1100.171884	53913.101713	34.984768
1101.081336	53968.678868	34.989786
1102.059451	54023.118990	34.994804
1103.241009	54072.768592	34.999821
1104.075256	54139.584126	35.004839
1105.163489	54188.438573	35.009856
1106.053206	54250.778019	35.014874
1106.993377	54322.545150	35.019892
1108.581156	54384.256744	35.024909
1109.297273	54447.756648	35.029927
1110.433405	54509.475996	35.034944
1111.828084	54570.857597	35.039962
1112.727837	54639.474189	35.044980
1113.858111	54710.364740	35.049997
1114.713965	54792.240227	35.055015
1116.097637	54844.663283	35.060032
1117.166904	54926.410896	35.065050
1118.445848	55000.411605	35.070068
1119.742010	55060.683441	35.075085
1121.130528	55130.205846	35.080103
1122.146621	55190.350991	35.085120
1123.310541	55262.585895	35.090138
1124.119535	55331.376913	35.095156
1125.439198	55397.733966	35.100173
1126.761866	55474.475895	35.105191
1128.066044	55532.614953	35.110208
1129.478278	55602.236286	35.115226
1130.396461	55667.346929	35.120244
1131.635088	55727.762370	35.125261
1132.778860	55790.407840	35.130279
1133.767507	55851.685456	35.135296
1135.087105	55910.974843	35.140314
1135.922338	55976.523339	35.145332
1137.476360	56043.712536	35.150349
1138.648508	56110.018728	35.155367
1139.789518	56171.374574	35.160384
1140.993985	56229.537277	35.165402
1141.892614	56307.569730	35.170420
1143.282289	56365.178479	35.175437
1144.383272	56429.914504	35.180455
1145.714425	56491.235075	35.185472
1147.064690	56555.299531	35.190490
1148.221263	56608.470869	35.195508
1149.284303	56665.523911	35.200525
1150.770375	56730.453618	35.205543
1152.094826	56781.554829	35.210560
1153.211662	56837.530275	35.215578
1153.871336	56900.013949	35.220596
1154.921999	56948.690095	35.225613
1156.116877	57019.317926	35.230631
1157.365581	57074.988479	35.235648
1158.478949	57130.199345	35.240666
1159.230487	57196.941484	35.245684
1160.843534	57251.200999	35.250701
1161.838801	57321.506544	35.255719
1162.841329	57383.766918	35.260736
1164.159962	57450.977939	35.265754
1164.822445	57511.367839	35.270772
1166.358297	57572.671794	35.275789
1167.959264	57639.136610	35.280807
1168.856911	57704.724370	35.285824
1170.621864	57761.841023	35.290842
1171.327715	57815.724849	35.295860
1172.819642	57866.688231	35.300877
1173.926604	57919.363911	35.305895
1174.772754	57966.428547	35.310912
1176.235899	58009.909278	35.315930
1176.949201	58052.811262	35.320948
1178.301856	58103.898219	35.325965
1179.335628	58162.472094	35.330983
1180.473015	58201.795209	35.336000
1181.715830	58266.532974	35.341018
1182.347314	58318.764962	35.346036
1183.702049	58367.060927	35.351053
1184.728866	58428.389791	35.356071
1185.638671	58474.128951	35.361088
1187.033256	58547.103509	35.366106
1188.363029	58609.600643	35.371124
1189.430649	58671.721238	35.376141
1190.663713	58739.259391	35.381159
1191.771495	58796.532016	35.386176
1192.909974	58866.148725	35.391194
1193.978964	58944.549158	35.396212
1195.593298	59002.831638	35.401229
1196.848462	59075.399211	35.406247
1197.463002	59136.610855	35.411264
1198.824317	59200.408457	35.416282
1200.114668	59271.629246	35.421300
1201.450346	59338.013683	35.426317
1203.025349	59403.936752	35.431335
1203.970510	59479.161853	35.436352
1205.800509	59541.766640	35.441370
1206.689689	59624.204068	35.446388
1208.030119	59678.587683	35.451405
1209.141924	59737.494952	35.456423
1210.287681	59807.417043	35.461440
1211.585241	59879.461344	35.466458
1212.656447	59944.578588	35.471476
1214.342701	59997.737779	35.476493
1215.192172	60074.726707	35.481511
1216.794443	60142.388195	35.486528
1218.006107	60199.166799	35.491546
1218.887134	60262.232161	35.496564
1220.705385	60325.752298	35.501581
1221.610391	60399.961092	35.506599
1222.734421	60468.635169	35.511616
1224.122767	60523.133436	35.516634
1225.288864	60590.497314	35.521652
1226.699751	60652.556569	35.526669
1228.010933	60708.352301	35.531687
1229.332948	60779.585197	35.536704
1230.854250	60840.367984	35.541722
1232.033262	60911.737590	35.546740
1233.204429	60966.467073	35.551757
1234.467968	61023.625600	35.556775
1235.421917	61085.459974	35.561792
1237.059798	61145.187143	35.566810
1237.882370	61200.706004	35.571828
1239.275466	61256.262279	35.576845
1240.504737	61324.244960	35.581863
1241.449104	61392.797829	35.586880
1243.198869	61450.090126	35.591898
1244.092151	61516.473776	35.596916
1245.234560	61577.108808	35.601933
1246.717940	61638.076752	35.606951
1247.538800	61699.256175	35.611968
1249.008935	61765.183040	35.616986
1250.018497	61833.239503	35.622004
1251.266302	61899.220522	35.627021
1252.524604	61963.199715	35.632039
1253.749882	62041.490649	35.637056
1255.042423	62096.108691	35.642074
1256.146527	62160.593636	35.647092
1257.396565	62213.560053	35.652109
1258.457692	62266.986618	35.657127
1259.668000	62320.947016	35.662144
1260.731595	62378.519810	35.667162
1262.219835	62441.210836	35.672180
1263.144650	62496.457061	35.677197
1264.522931	62566.040416	35.682215
1265.527885	62633.118588	35.687232
1266.818977	62688.630756	35.692250
1267.786811	62773.041521	35.697268
1269.369851	62851.975362	35.702285
1270.684471	62918.708297	35.707303
1271.747113	62989.519723	35.712320
1273.364150	63062.631173	35.717338
1274.476025	63133.346673	35.722356
1275.801618	63206.668765	35.727373
1277.053637	63275.761098	35.732391
1278.088285	63348.280854	35.737408
1279.485943	63433.664792	35.742426
1280.939136	63510.658558	35.747444
1282.172822	63586.287846	35.752461
1283.537445	63655.844737	35.757479
1284.847957	63730.550819	35.762496
1286.402291	63808.074109	35.767514
1287.803989	63885.064429	35.772532
1289.049204	63957.996145	35.777549
1290.587366	64030.831569	35.782567
1291.369745	64103.772855	35.787584
1293.050494	64168.837472	35.792602
1294.406140	64253.477422	35.797620
1295.609735	64323.890718	35.802637
1297.459806	64388.144375	35.807655
1298.228734	64467.337387	35.812672
1299.581086	64534.480245	35.817690
1301.371310	64614.108951	35.822708
1302.435343	64685.918921	35.827725
1304.189105	64755.696514	35.832743
1305.403477	64823.222609	35.837760
1306.807265	64899.753558	35.842778
1308.300386	64968.901460	35.847796
1309.462758	65030.041931	35.852813
1310.923962	65092.743855	35.857831
1312.114565	65166.909525	35.862848
1313.514408	65225.107340	35.867866
1314.666307	65299.057870	35.872884
1316.034277	65369.701608	35.877901
1317.629487	65434.985495	35.882919
1318.754404	65501.254855	35.887936
1319.613790	65561.481710	35.892954
1321.335726	65646.892062	35.897972
1322.127791	65716.670914	35.902989
1323.679698	65782.374006	35.908007
1324.733984	65858.816959	35.913024
1326.482520	65930.377703	35.918042
1327.864211	65999.628181	35.923060
1329.359261	66076.882842	35.928077
1330.579450	66143.006012	35.933095
1331.806268	66214.870825	35.938112
1333.144251	66281.438104	35.943130
1334.533210	66346.167816	35.948148
1336.049793	66412.384582	35.953165
1337.920380	66475.184141	35.958183
1338.924851	66546.134989	35.963200
1340.207012	66609.242257	35.968218
1341.567601	66671.267393	35.973236
1342.898092	66729.650477	35.978253
1344.080747	66781.263177	35.983271
1345.023093	66849.673017	35.988288
1346.679158	66899.420043	35.993306
1347.776518	66964.608525	35.998324
1349.256587	67009.558708	36.003341
1350.386156	67065.587032	36.008359
1351.399623	67132.049049	36.013376
1352.685461	67189.256178	36.018394
1354.131868	67254.568047	36.023412
1355.142688	67323.342003	36.028429
1356.887803	67400.118330	36.033447
1357.656864	67466.999373	36.038464
1359.294561	67538.157779	36.043482
1360.471231	67611.857900	36.048500
1361.543540	67681.990835	36.053517
1363.011770	67752.980084	36.058535
1364.308966	67845.011288	36.063552
1365.820093	67923.022509	36.068570
1367.239929	68001.535802	36.073588
1368.374529	68084.817496	36.078605
1369.799879	68166.148074	36.083623
1371.117872	68252.060959	36.088640
1372.340997	68324.907392	36.093658
1373.791789	68418.847820	36.098676
1375.537853	68501.819867	36.103693
1377.290229	68577.376531	36.108711
1378.435852	68666.344432	36.113728
1380.083567	68744.995287	36.118746
1381.777227	68826.292285	36.123764
1382.942402	68903.828749	36.128781
1384.799578	68978.357068	36.133799
1386.006118	69061.668650	36.138816
1387.700621	69123.254872	36.143834
1389.290699	69195.197832	36.148852
1390.761953	69270.471266	36.153869
1392.232649	69341.705133	36.158887
1393.781374	69409.248026	36.163904
1395.310303	69478.427883	36.168922
1396.910298	69542.740049	36.173940
1398.052010	69609.549326	36.178957
1399.240590	69681.467835	36.183975
1400.467563	69749.986480	36.188992
1401.869079	69813.412218	36.194010
1403.363351	69898.942053	36.199028
1404.830916	69971.875179	36.204045
1406.482536	70031.064024	36.209063
1407.963057	70111.796860	36.214080
1409.114419	70189.212687	36.219098
1410.796293	70246.231641	36.224116
1411.982604	70318.956473	36.229133
1413.233453	70380.881090	36.234151
1414.812643	70450.834551	36.239168
1416.291200	70520.943265	36.244186
1417.630698	70586.907218	36.249204
1418.890174	70678.264174	36.254221
1420.446825	70745.473686	36.259239
1421.465387	70811.526437	36.264256
1423.234578	70899.144226	36.269274
1425.079163	70965.498680	36.274292
1426.049836	71044.933728	36.279309
1427.297444	71105.315441	36.284327
1428.893701	71171.139360	36.289344
1429.985950	71251.341239	36.294362
1431.533601	71317.730399	36.299380
1433.036151	71404.416402	36.304397
1434.459367	71478.855175	36.309415
1435.701109	71559.275234	36.314432
1437.112910	71628.523464	36.319450
1439.096112	71701.937986	36.324468
1440.114507	71762.471079	36.329485
1441.412396	71819.160948	36.334503
1442.415690	71892.222767	36.339520
1443.948781	71957.703917	36.344538
1445.317176	72017.182241	36.349556
1446.864100	72093.895845	36.354573
1448.183170	72157.954459	36.359591
1449.304939	72227.680292	36.364608
1450.986134	72298.382657	36.369626
1452.399189	72371.381667	36.374644
1453.922935	72453.115541	36.379661
1455.363965	72520.715004	36.384679
1457.059378	72603.663714	36.389696
1458.166160	72683.171062	36.394714
1459.776396	72750.883953	36.399732
1461.207873	72832.924757	36.404749
1462.661617	72911.466541	36.409767
1464.057018	72987.991139	36.414784
1465.796343	73068.312583	36.419802
1467.393080	73148.466598	36.424820
1468.834849	73222.983386	36.429837
1470.184661	73301.403266	36.434855
1472.390692	73382.273250	36.439872
1473.511567	73457.512228	36.444890
1475.006037	73536.378807	36.449908
1476.329665	73624.075397	36.454925
1477.911608	73704.626060	36.459943
1479.531004	73776.786003	36.464960
1480.742395	73859.751069	36.469978
1482.712167	73928.499998	36.474996
1484.299315	74007.809458	36.480013
1485.303111	74088.502439	36.485031
1486.737156	74170.090975	36.490048
1488.344679	74257.935211	36.495066
1490.076452	74327.875078	36.500084
1491.419018	74419.776621	36.505101
1492.774507	74503.987795	36.510119
1494.639788	74583.331429	36.515136
1496.433576	74669.247857	36.520154
1498.027297	74749.445159	36.525172
1499.745611	74822.289118	36.530189
1501.032648	74903.611562	36.535207
1503.090151	74970.880090	36.540224
1504.497790	75048.105361	36.545242
1506.098467	75111.493667	36.550260
1507.473362	75187.749110	36.555277
1508.816991	75265.669042	36.560295
1510.735358	75329.388149	36.565312
1511.936273	75412.093652	36.570330
1514.001318	75466.226478	36.575348
1515.131758	75549.146107	36.580365
1516.409097	75609.470077	36.585383
1517.949123	75688.551208	36.590400
1519.534602	75762.685228	36.595418
1520.493595	75843.086476	36.600436
1522.068922	75933.246676	36.605453
1523.530531	76005.145965	36.610471
1525.405171	76080.591008	36.615488
1526.534278	76159.395812	36.620506
1528.281490	76237.546733	36.625524
1529.463686	76322.056731	36.630541
1531.149458	76406.969542	36.635559
1532.640559	76489.113550	36.640576
1533.964775	76563.442667	36.645594
1535.663280	76648.012213	36.650612
1537.390866	76738.366611	36.655629
1538.827206	76816.542522	36.660647
1540.335640	76888.753519	36.665664
1541.731551	76965.340046	36.670682
1543.117691	77025.206768	36.675700
1544.828790	77089.925225	36.680717
1545.978277	77151.944800	36.685735
1547.754006	77221.771285	36.690752
1549.029807	77307.612494	36.695770
1550.277869	77378.548074	36.700788
1551.715525	77450.822312	36.705805
1552.897963	77537.717636	36.710823
1555.231955	77611.093480	36.715840
1556.257791	77700.256086	36.720858
1557.770842	77774.292919	36.725876
1559.698135	77869.028335	36.730893
1561.278081	77950.567435	36.735911
1562.909642	78029.539703	36.740928
1564.084601	78122.455495	36.745946
1566.081864	78208.249951	36.750964
1567.349577	78301.430536	36.755981
1569.138031	78387.650955	36.760999
1570.741696	78475.028064	36.766016
1572.189633	78568.498058	36.771034
1574.214275	78654.986395	36.776052
1575.537581	78738.594976	36.781069
1577.351324	78823.191218	36.786087
1579.311258	78911.337415	36.791104
1580.786024	78988.854740	36.796122
1582.502113	79074.898607	36.801140
1583.936066	79157.629662	36.806157
1585.037485	79264.825906	36.811175
1587.398070	79346.665036	36.816192
1588.657889	79432.578725	36.821210
1590.431516	79514.269507	36.826228
1592.070829	79608.017120	36.831245
1593.495550	79700.709097	36.836263
1595.295649	79786.133912	36.841280
1596.655939	79879.862768	36.846298
1598.280759	79964.682108	36.851316
1599.975706	80051.403783	36.856333
1601.980899	80144.513160	36.861351
1603.697897	80234.285249	36.866368
1605.316511	80325.149919	36.871386
1607.113464	80403.684999	36.876404
1608.751616	80484.905733	36.881421
1610.334856	80560.193323	36.886439
1612.534008	80630.659001	36.891456
1614.223780	80721.057724	36.896474
1615.651233	80799.094289	36.901492
1617.561221	80877.701701	36.906509
1619.050655	80949.774276	36.911527
1620.459746	81022.695808	36.916544
1622.167911	81097.179775	36.921562
1623.723332	81175.172022	36.926580
1625.104190	81264.442563	36.931597
1626.500432	81335.061021	36.936615
1628.259725	81418.432044	36.941632
1629.936514	81501.790889	36.946650
1631.330715	81591.250428	36.951668
1633.021731	81674.290809	36.956685
1634.827420	81754.424730	36.961703
1636.673146	81825.810295	36.966720
1637.820272	81908.290318	36.971738
1639.577045	81992.144900	36.976756
1641.227466	82071.391777	36.981773
1642.881695	82168.110451	36.986791
1644.373600	82247.712057	36.991808
1645.870174	82343.923858	36.996826
1647.444736	82420.294768	37.001844
1649.132871	82497.268956	37.006861
1650.327530	82581.187921	37.011879
1652.311961	82650.703994	37.016896
1653.947756	82719.653950	37.021914
1655.183198	82794.229062	37.026932
1656.541652	82871.699331	37.031949
1658.140630	82959.471320	37.036967
1660.416517	83039.547972	37.041984
1661.284766	83121.733070	37.047002
1663.102868	83201.311645	37.052020
1664.707719	83284.788375	37.057037
1665.986510	83377.375939	37.062055
1667.741039	83464.048132	37.067072
1669.505178	83570.422175	37.072090
1671.602930	83650.059606	37.077108
1673.310107	83741.643669	37.082125
1675.094105	83835.192665	37.087143
1677.070631	83923.592770	37.092160
1678.668780	84020.693986	37.097178
1680.047510	84115.840518	37.102196
1682.068334	84203.474292	37.107213
1683.391128	84298.604842	37.112231
1684.899482	84387.396427	37.117248
1686.455758	84490.144456	37.122266
1688.022130	84587.417290	37.127284
1689.893964	84690.965625	37.132301
1691.916496	84796.125352	37.137319
1694.134511	84890.268778	37.142336
1695.531529	84987.949613	37.147354
1697.083328	85094.628643	37.152372
1698.790185	85186.850942	37.157389
1700.503065	85292.124298	37.162407
1702.408649	85381.135556	37.167424
1703.935829	85494.801969	37.172442
1705.529303	85596.927209	37.177460
1707.410267	85688.160812	37.182477
1709.309141	85805.850574	37.187495
1710.967972	85902.695202	37.192512
1712.845332	85994.754004	37.197530
1714.574802	86108.150397	37.202548
1716.826823	86201.342380	37.207565
1718.281193	86306.102310	37.212583
1720.314004	86405.969386	37.217600
1721.832868	86503.686948	37.222618
1723.437574	86600.491683	37.227636
1725.226218	86693.846468	37.232653
1726.752018	86799.813521	37.237671
1728.880869	86889.326697	37.242688
1730.347711	86998.712535	37.247706
1732.091168	87103.024570	37.252724
1734.182486	87199.412983	37.257741
1735.797026	87294.469689	37.262759
1737.732455	87389.299070	37.267776
1739.569949	87488.959640	37.272794
1741.231449	87577.939783	37.277812
1743.176130	87673.389590	37.282829
1744.645487	87757.635453	37.287847
1747.017201	87856.364600	37.292864
1748.340462	87947.527804	37.297882
1749.814866	88050.719423	37.302900
1751.878667	88138.092228	37.307917
1753.593310	88232.528008	37.312935
1755.284967	88329.730374	37.317952
1757.055813	88422.928699	37.322970
1758.432646	88522.081904	37.327988
1760.156180	88610.954076	37.333005
1761.765916	88711.275400	37.338023
1763.916939	88810.789991	37.343040
1765.392474	88895.950598	37.348058
1766.816943	88985.985931	37.353076
1768.985124	89067.287383	37.358093
1770.286622	89151.677548	37.363111
1771.902342	89231.114229	37.368128
1773.432575	89318.979567	37.373146
1774.744116	89420.528571	37.378164
1776.574038	89513.087412	37.383181
1778.287538	89621.037618	37.388199
1779.842481	89713.627441	37.393216
1781.778597	89817.868218	37.398234
1783.603737	89925.307788	37.403252
1785.358091	90029.932609	37.408269
1787.117891	90142.287865	37.413287
1788.954774	90253.579564	37.418304
1790.824983	90357.059440	37.423322
1792.481856	90468.240695	37.428340
1794.426129	90579.326691	37.433357
1795.924479	90689.354905	37.438375
1797.697995	90802.572311	37.443392
1799.977696	90910.565298	37.448410
1801.703885	91037.643643	37.453428
1803.893106	91145.930463	37.458445
1805.478581	91267.366489	37.463463
1807.417398	91384.425818	37.468480
1809.300518	91490.100200	37.473498
1811.574526	91606.715036	37.478516
1813.592871	91699.327179	37.483533
1815.472791	91818.868894	37.488551
1817.623207	91915.111242	37.493568
1819.548806	92020.349899	37.498586
1820.835121	92137.057966	37.503604
1822.934355	92234.145852	37.508621
1824.699473	92346.901394	37.513639
1826.693152	92452.346361	37.518656
1828.840285	92561.012390	37.523674
1830.494215	92671.353000	37.528692
1832.609288	92770.696216	37.533709
1834.452322	92874.404427	37.538727
1835.881534	92978.418570	37.543744
1838.234782	93081.604024	37.548762
1839.770963	93194.474572	37.553780
1841.899077	93287.822194	37.558797
1843.819962	93393.433901	37.563815
1845.425285	93495.267489	37.568832
1847.015183	93601.590809	37.573850
1848.732754	93706.487578	37.578868
1850.871021	93815.184799	37.583885
1852.737939	93924.660029	37.588903
1854.812008	94028.614844	37.593920
1857.117435	94134.447777	37.598938
1858.902942	94221.729680	37.603956
1861.246981	94318.773196	37.608973
1863.365211	94416.334019	37.613991
1865.394741	94510.093717	37.619008
1866.863976	94601.545709	37.624026
1868.638308	94699.668260	37.629044
1870.882539	94779.832361	37.634061
1872.538902	94886.859539	37.639079
1874.159652	94980.786036	37.644096
1875.843985	95068.263619	37.649114
1877.565762	95167.397253	37.654132
1879.570837	95275.309205	37.659149
1881.029524	95366.866508	37.664167
1882.606985	95475.264369	37.669184
1884.766330	95579.718081	37.674202
1886.163482	95692.758937	37.679220
1888.162575	95792.472286	37.684237
1890.007753	95894.631157	37.689255
1891.594881	95995.081446	37.694272
1893.385606	96086.373407	37.699290
1894.717648	96194.343149	37.704308
1896.779044	96277.341146	37.709325
1898.532480	96386.627312	37.714343
1899.887002	96497.294612	37.719360
1901.812877	96593.586701	37.724378
1903.471949	96715.603108	37.729396
1905.214009	96831.750506	37.734413
1906.841895	96948.702138	37.739431
1908.870131	97077.063780	37.744448
1910.764125	97194.025386	37.749466
1912.596439	97324.484967	37.754484
1914.482958	97454.733778	37.759501
1916.405896	97587.031050	37.764519
1918.471070	97714.831724	37.769536
1920.333649	97848.939631	37.774554
1922.273800	97988.892673	37.779572
1924.063982	98115.559040	37.784589
1926.254413	98254.776857	37.789607
1928.322878	98390.908497	37.794624
1930.714268	98529.411508	37.799642
1932.318017	98660.001070	37.804660
1934.638698	98794.193393	37.809677
1936.543817	98920.540715	37.814695
1938.626315	99052.616263	37.819712
1940.495661	99178.754686	37.824730
1942.314967	99325.819114	37.829748
1944.768401	99453.071569	37.834765
1947.048943	99583.013854	37.839783
1948.623652	99723.044331	37.844800
1951.108607	99856.213860	37.849818
1952.676890	99990.985303	37.854836
1954.638784	100118.368009	37.859853
1956.531394	100254.966101	37.864871
1958.032952	100391.283658	37.869888
1960.200682	100534.229489	37.874906
1962.085292	100673.949350	37.879924
1964.637253	100814.516234	37.884941
1966.469780	100952.888899	37.889959
1968.152673	101094.543830	37.894976
1970.633656	101224.017596	37.899994
1972.670614	101374.733914	37.905012
1974.536319	101513.978559	37.910029
1976.484907	101646.757577	37.915047
1978.442563	101781.779780	37.920064
1980.329357	101917.472903	37.925082
1982.179141	102072.253444	37.930100
1984.528188	102202.360286	37.935117
1986.500852	102336.089210	37.940135
1988.134034	102494.835980	37.945152
1990.669115	102629.999526	37.950170
1992.660147	102764.766964	37.955188
1994.900185	102903.210867	37.960205
1996.996381	103028.136876	37.965223
1999.037172	103165.662142	37.970240
2000.853499	103297.238648	37.975258
2002.785431	103437.000882	37.980276
2005.119448	103576.865615	37.985293
2007.000979	103702.372947	37.990311
2008.856287	103834.477998	37.995328
2010.430703	103970.875047	38.000346
2012.643370	104103.419734	38.005364
2014.538424	104245.308555	38.010381
2016.713042	104376.123214	38.015399
2018.717823	104522.864903	38.020416
2020.620630	104661.482990	38.025434
2022.464642	104788.724668	38.030452
2024.294640	104916.324047	38.035469
2026.873773	105033.980020	38.040487
2028.157697	105155.110406	38.045504
2029.999986	105272.083687	38.050522
2031.770844	105404.677276	38.055540
2033.852567	105535.498296	38.060557
2035.730586	105664.234167	38.065575
2037.302828	105800.207852	38.070592
2039.468111	105940.654059	38.075610
2041.635001	106089.190416	38.080628
2043.316460	106231.945204	38.085645
2045.480018	106378.568661	38.090663
2047.345939	106535.180544	38.095680
2049.268538	106678.913882	38.100698
2051.633298	106844.084339	38.105716
2053.528759	106992.819260	38.110733
2055.410451	107147.478709	38.115751
2057.449283	107306.552415	38.120768
2059.845597	107470.288061	38.125786
2061.724776	107637.021924	38.130804
2063.897655	107796.571460	38.135821
2066.181812	107948.369121	38.140839
2068.455435	108114.358816	38.145856
2070.605050	108269.488604	38.150874
2072.513132	108431.441123	38.155892
2074.296484	108594.352298	38.160909
2076.796660	108756.873098	38.165927
2079.062972	108927.331518	38.170944
2081.556635	109076.146655	38.175962
2083.519853	109249.279052	38.180980
2085.293149	109405.652127	38.185997
2087.800886	109572.373013	38.191015
2089.496562	109743.761658	38.196032
2091.658433	109904.273670	38.201050
2093.866071	110078.094752	38.206068
2096.120228	110248.130328	38.211085
2098.264014	110403.384628	38.216103
2100.256375	110569.658250	38.221120
2102.503464	110734.053958	38.226138
2105.177080	110902.898387	38.231156
2107.521421	111061.713123	38.236173
2109.895771	111224.658152	38.241191
2111.424506	111385.580311	38.246208
2113.624952	111546.499556	38.251226
2115.537871	111706.526043	38.256244
2117.857090	111862.989428	38.261261
2119.850221	112022.916007	38.266279
2122.089923	112198.188205	38.271296
2124.021453	112359.267318	38.276314
2126.153789	112511.159118	38.281332
2128.219682	112684.241478	38.286349
2130.555421	112852.133390	38.291367
2132.267785	113023.788849	38.296384
2134.447013	113184.287546	38.301402
2136.487742	113358.493134	38.306420
2138.513702	113542.353367	38.311437
2141.213084	113697.864768	38.316455
2143.231371	113878.975757	38.321472
2145.140808	114047.396478	38.326490
2147.400352	114212.135895	38.331508
2149.084964	114387.606996	38.336525
2151.082868	114568.927519	38.341543
2153.119506	114754.250728	38.346560
2155.108551	114927.381143	38.351578
2157.393187	115113.200051	38.356596
2159.506449	115300.479917	38.361613
2161.793886	115480.795704	38.366631
2163.412297	115655.496837	38.371648
2165.191820	115822.487422	38.376666
2167.800995	115985.848310	38.381684
2169.595215	116172.040982	38.386701
2171.365981	116344.527262	38.391719
2173.233716	116518.914403	38.396736
2175.286786	116699.551810	38.401754
2177.703004	116874.793395	38.406772
2179.402170	117066.725788	38.411789
2182.315850	117246.140372	38.416807
2184.177204	117428.295302	38.421824
2185.847096	117617.368504	38.426842
2188.158687	117810.629484	38.431860
2190.515236	118011.938871	38.436877
2192.441108	118202.979050	38.441895
2194.634274	118405.356195	38.446912
2196.846694	118613.464742	38.451930
2198.744503	118819.162865	38.456948
2200.976056	119028.957717	38.461965
2203.211985	119238.714981	38.466983
2205.531576	119461.436707	38.472000
2208.071792	119679.698236	38.477018
2210.462304	119880.276445	38.482036
2212.290972	120093.666516	38.487053
2214.963982	120303.018707	38.492071
2216.979752	120513.185217	38.497088
2219.801564	120723.163333	38.502106
2222.742881	120929.927233	38.507124
2225.074896	121135.189221	38.512141
2227.266021	121342.364436	38.517159
2229.462873	121546.799818	38.522176
2232.049439	121749.234431	38.527194
2234.579182	121953.581797	38.532212
2236.720305	122161.301950	38.537229
2239.097956	122360.550267	38.542247
2241.310879	122542.636289	38.547264
2243.020169	122750.947213	38.552282
2245.395895	122951.594237	38.557300
2247.756761	123166.414700	38.562317
2250.430623	123362.868881	38.567335
2252.639316	123574.467755	38.572352
2254.988244	123777.799876	38.577370
2257.726755	123962.157085	38.582388
2259.873257	124169.151087	38.587405
2262.126654	124364.356602	38.592423
2264.025914	124562.333334	38.597440
2266.016928	124780.531431	38.602458
2268.410438	124971.290419	38.607476
2270.568524	125190.885468	38.612493
2273.047315	125394.953928	38.617511
2275.088975	125596.123128	38.622528
2277.129153	125816.767615	38.627546
2279.421455	126021.236296	38.632564
2280.996901	126233.506357	38.637581
2283.402986	126456.685155	38.642599
2285.770977	126678.957662	38.647616
2288.059366	126899.251957	38.652634
2290.563954	127112.840194	38.657652
2292.776936	127334.087446	38.662669
2295.335479	127555.180317	38.667687
2297.988823	127775.726666	38.672704
2300.231175	128009.482581	38.677722
2302.598863	128220.623886	38.682740
2304.297072	128436.552673	38.687757
2306.986862	128648.597303	38.692775
2309.085711	128868.728649	38.697792
2311.200344	129095.481646	38.702810
2313.648504	129300.259245	38.707828
2315.699996	129518.142960	38.712845
2318.053960	129722.417133	38.717863
2320.102964	129919.355616	38.722880
2322.267696	130125.044307	38.727898
2324.461729	130325.933319	38.732916
2326.190005	130539.330489	38.737933
2328.261939	130755.605925	38.742951
2330.462787	130979.411787	38.747968
2332.438442	131207.986778	38.752986
2334.659538	131433.009899	38.758004
2336.583255	131671.898427	38.763021
2338.937949	131909.020584	38.768039
2340.995694	132154.806035	38.773056
2343.125227	132406.202715	38.778074
2345.628037	132659.407684	38.783092
2347.246093	132916.724119	38.788109
2349.929211	133190.954677	38.793127
2352.265442	133447.108674	38.798144
2354.441332	133727.436472	38.803162
2356.827498	134003.494974	38.808180
2359.334362	134277.556788	38.813197
2361.464530	134550.626000	38.818215
2363.757657	134823.887099	38.823232
2366.298108	135107.262709	38.828250
2368.812788	135385.009986	38.833268
2371.628462	135667.889231	38.838285
2374.095166	135949.796966	38.843303
2376.818241	136218.557835	38.848320
2379.314536	136505.591028	38.853338
2381.860549	136767.834873	38.858356
2384.390147	137062.975179	38.863373
2387.181922	137335.982979	38.868391
2389.703285	137601.763252	38.873408
2391.891208	137878.802649	38.878426
2394.515823	138147.222137	38.883444
2397.000887	138424.205597	38.888461
2399.462079	138699.557363	38.893479
2402.014979	138977.167993	38.898496
2404.117389	139258.975162	38.903514
2406.886835	139526.021969	38.908532
2409.506849	139800.568484	38.913549
2412.173423	140083.548670	38.918567
2414.543180	140359.127427	38.923584
2417.077580	140639.428421	38.928602
2419.213146	140904.691140	38.933620
2421.746956	141190.630237	38.938637
2423.835377	141464.406423	38.943655
2426.173936	141741.939696	38.948672
2429.102788	142008.277327	38.953690
2431.778181	142279.351861	38.958708
2434.147404	142548.660913	38.963725
2436.188869	142824.660363	38.968743
2438.741430	143101.292131	38.973760
2441.538492	143391.276880	38.978778
2443.453505	143662.681015	38.983796
2445.924513	143949.052108	38.988813
2447.776718	144225.571219	38.993831
2450.524598	144516.141317	38.998848
2452.554283	144800.428666	39.003866
2454.783385	145087.605591	39.008884
2457.302352	145397.203899	39.013901
2459.552267	145687.109761	39.018919
2462.073377	145983.866758	39.023936
2464.234997	146290.835598	39.028954
2466.593245	146582.874575	39.033972
2469.489897	146890.506235	39.038989
2471.486344	147190.474588	39.044007
2473.792330	147493.505945	39.049024
2475.895540	147799.553567	39.054042
2478.262284	148074.883227	39.059060
2480.481532	148378.885211	39.064077
2483.132046	148666.396802	39.069095
2485.224370	148954.504982	39.074112
2487.269199	149259.554720	39.079130
2489.388642	149562.931717	39.084148
2491.777229	149872.995733	39.089165
2494.174204	150190.638117	39.094183
2497.391596	150501.464615	39.099200
2499.780453	150819.860851	39.104218
2501.722843	151130.509565	39.109236
2504.486433	151452.773153	39.114253
2506.975102	151773.913808	39.119271
2510.005902	152104.276034	39.124288
2512.329089	152429.356033	39.129306
2514.616209	152758.937199	39.134324
2517.283976	153109.190008	39.139341
2519.778344	153440.951492	39.144359
2521.971938	153776.379787	39.149376
2524.592881	154116.338506	39.154394
2527.300688	154448.402510	39.159412
2529.664276	154804.184534	39.164429
2531.923234	155151.441761	39.169447
2535.182741	155499.902865	39.174464
2537.244280	155850.698817	39.179482
2539.996973	156194.889089	39.184500
2542.849688	156555.226108	39.189517
2544.702154	156910.326482	39.194535
2547.998700	157242.415781	39.199552
2551.549718	157586.451144	39.204570
2554.318428	157932.857860	39.209588
2556.805020	158277.647627	39.214605
2559.367740	158623.011416	39.219623
2562.183516	158952.760521	39.224640
2564.945700	159305.574441	39.229658
2566.874715	159656.438656	39.234676
2569.539239	160007.659533	39.239693
2571.917809	160358.812851	39.244711
2574.784976	160710.272572	39.249728
2576.740324	161061.622959	39.254746
2578.935934	161424.693951	39.259764
2581.700701	161790.179050	39.264781
2584.122467	162148.127746	39.269799
2587.273925	162516.476528	39.274816
2590.220725	162879.273162	39.279834
2593.235913	163232.132773	39.284852
2596.055539	163587.272086	39.289869
2598.621398	163935.203457	39.294887
2601.554329	164294.823294	39.299904
2604.403221	164640.289080	39.304922
2606.658771	164991.765976	39.309940
2609.718119	165336.681853	39.314957
2612.093086	165685.604364	39.319975
2614.866536	166025.108922	39.324992
2617.478057	166380.320872	39.330010
2619.447727	166729.946897	39.335028
2622.011627	167083.278071	39.340045
2624.385893	167441.719433	39.345063
2627.869103	167771.281405	39.350080
2630.570828	168126.170661	39.355098
2633.084216	168474.882281	39.360116
2635.495050	168822.976776	39.365133
2638.088917	169182.789203	39.370151
2640.730941	169526.241837	39.375168
2643.119825	169888.032476	39.380186
2645.355976	170251.423252	39.385204
2647.648242	170610.312143	39.390221
2649.945447	170974.141304	39.395239
2652.779183	171307.033282	39.400256
2655.491530	171641.367843	39.405274
2657.834267	171987.265753	39.410292
2660.580008	172325.293099	39.415309
2663.053676	172669.980016	39.420327
2666.027071	173012.253903	39.425344
2668.219094	173368.898518	39.430362
2670.681278	173708.957087	39.435380
2673.142937	174062.286594	39.440397
2675.364582	174436.276830	39.445415
2677.784341	174803.177673	39.450432
2680.313602	175185.630998	39.455450
2682.384790	175564.538768	39.460468
2685.153566	175955.326353	39.465485
2687.327316	176372.405531	39.470503
2689.904620	176770.198282	39.475520
2692.392190	177187.714966	39.480538
2694.888055	177600.864108	39.485556
2697.897795	178022.544512	39.490573
2699.663962	178463.799621	39.495591
2702.890876	178880.370757	39.500608
2705.583268	179313.332695	39.505626
2708.827098	179754.464738	39.510644
2711.926338	180177.385940	39.515661
2714.572005	180610.234450	39.520679
2717.231969	181057.127888	39.525696
2719.972113	181492.276991	39.530714
2723.151532	181941.963430	39.535732
2725.610382	182429.074977	39.540749
2728.380210	182882.411110	39.545767
2731.393550	183317.043277	39.550784
2733.807126	183758.527259	39.555802
2736.264879	184209.886472	39.560820
2739.496156	184664.987395	39.565837
2742.137380	185128.335774	39.570855
2745.038161	185576.533127	39.575872
2747.427459	186029.562101	39.580890
2750.519145	186488.807649	39.585908
2753.922179	186938.837263	39.590925
2756.413425	187391.500548	39.595943
2759.390245	187845.308972	39.600960
2762.655681	188286.729806	39.605978
2765.488624	188741.758226	39.610996
2768.360058	189184.184040	39.616013
2770.996267	189640.110458	39.621031
2773.875404	190080.328727	39.626048
2776.886853	190539.273436	39.631066
2779.477898	190990.182937	39.636084
2782.523604	191436.400129	39.641101
2784.617781	191897.550965	39.646119
2787.532686	192350.929548	39.651136
2790.248519	192811.503954	39.656154
2792.656555	193275.989123	39.661172
2795.820951	193734.642453	39.666189
2798.203680	194209.041339	39.671207
2801.316181	194669.992165	39.676224
2803.837084	195131.494326	39.681242
2806.591661	195602.817242	39.686260
2809.738480	196066.663194	39.691277
2812.638834	196525.570525	39.696295
2815.100884	196999.052210	39.701312
2817.814339	197463.427714	39.706330
2820.105121	197958.886369	39.711348
2823.183433	198432.428686	39.716365
2825.939936	198916.971042	39.721383
2828.554131	199392.443238	39.726400
2831.392768	199871.057022	39.731418
2833.961616	200357.411278	39.736436
2836.765195	200808.954581	39.741453
2839.387047	201262.458097	39.746471
2842.152309	201723.865933	39.751488
2844.851024	202189.807034	39.756506
2847.125422	202661.328064	39.761524
2849.807809	203124.429062	39.766541
2852.557791	203606.267799	39.771559
2855.319725	204083.406392	39.776576
2858.127775	204569.226695	39.781594
2860.448548	205076.970834	39.786612
2863.380698	205572.046191	39.791629
2865.893254	206076.231799	39.796647
2868.733459	206585.854404	39.801664
2871.145050	207114.775352	39.806682
2873.674010	207638.522344	39.811700
2876.150690	208163.447235	39.816717
2878.919113	208715.229687	39.821735
2881.733160	209267.996959	39.826752
2884.966376	209811.884900	39.831770
2887.499052	210367.696096	39.836788
2890.284318	210920.903159	39.841805
2893.169337	211494.647127	39.846823
2896.073625	212062.978225	39.851840
2899.222607	212635.844740	39.856858
2902.359394	213217.554638	39.861876
2905.280751	213781.592845	39.866893
2908.075347	214374.053130	39.871911
2910.919646	214961.095566	39.876928
2914.240567	215532.288564	39.881946
2917.018291	216125.719424	39.886964
2920.261514	216711.660336	39.891981
2923.323062	217298.468698	39.896999
2926.547768	217886.878058	39.902016
2929.728836	218477.454195	39.907034
2932.600561	219060.737531	39.912052
2935.707296	219654.095412	39.917069
2938.317487	220249.309702	39.922087
2941.233172	220855.374971	39.927104
2944.455128	221433.372068	39.932122
2947.633950	222030.784916	39.937140
2951.082234	222613.777195	39.942157
2954.291417	223208.086487	39.947175
2957.213008	223793.270048	39.952192
2960.174880	224384.950871	39.957210
2963.296986	224971.957754	39.962228
2966.549676	225559.680950	39.967245
2969.608440	226142.252004	39.972263
2972.451838	226725.136102	39.977280
2975.637107	227312.336107	39.982298
2978.401847	227901.379977	39.987316
2981.525415	228473.016531	39.992333
2985.189962	229053.510443	39.997351
2988.342494	229619.629213	40.002368
2991.714925	230195.747827	40.007386
2994.094902	230782.386061	40.012404
2997.301963	231355.430377	40.017421
3000.109595	231925.437377	40.022439
3002.731776	232515.008453	40.027456
3005.979322	233088.273425	40.032474
3008.638162	233677.761273	40.037492
3011.302023	234258.153039	40.042509
3014.268156	234854.323350	40.047527
3017.126639	235444.057096	40.052544
3019.906936	236035.402628	40.057562
3022.240896	236652.169895	40.062580
3025.404272	237250.033105	40.067597
3028.524808	237860.603748	40.072615
3031.005602	238464.058668	40.077632
3033.568760	239048.142065	40.082650
3036.222714	239654.285687	40.087668
3039.081079	240237.101141	40.092685
3041.742951	240844.968341	40.097703
3044.254153	241448.869370	40.102720
3047.282576	242057.235236	40.107738
3050.545019	242681.414531	40.112756
3053.098688	243299.809477	40.117773
3056.000662	243925.565932	40.122791
3059.091884	244566.202506	40.127808
3061.915635	245198.064169	40.132826
3065.625894	245845.103109	40.137844
3068.402739	246490.050454	40.142861
3071.655940	247147.368402	40.147879
3074.281245	247800.590799	40.152896
3076.853213	248454.403425	40.157914
3080.206687	249126.406465	40.162932
3082.781524	249812.067984	40.167949
3085.789147	250494.610738	40.172967
3088.546296	251195.225175	40.177984
3091.763806	251889.820457	40.183002
3094.913022	252586.226784	40.188020
3098.423541	253274.622646	40.193037
3101.699883	253981.569560	40.198055
3104.627299	254703.300304	40.203072
3107.736304	255405.719343	40.208090
3111.196704	256133.912704	40.213108
3114.076437	256850.355991	40.218125
3117.613965	257552.467973	40.223143
3120.539176	258277.379999	40.228160
3123.799343	258990.474941	40.233178
3127.102099	259721.212270	40.238196
3130.486852	260454.319876	40.243213
3133.461949	261179.968477	40.248231
3136.450025	261908.480590	40.253248
3139.848183	262632.529650	40.258266
3143.183177	263366.388001	40.263284
3146.653428	264097.959617	40.268301
3149.890978	264824.127086	40.273319
3153.011485	265563.388224	40.278336
3156.641325	266277.343275	40.283354
3159.888233	267008.649545	40.288372
3163.665429	267731.104947	40.293389
3166.646084	268451.063435	40.298407
3170.224839	269164.116223	40.303424
3173.422460	269880.423255	40.308442
3176.497517	270603.423416	40.313460
3179.704357	271329.368655	40.318477
3183.004368	272055.394951	40.323495
3186.360450	272775.615900	40.328512
3189.682290	273489.563134	40.333530
3192.713616	274204.794192	40.338548
3196.271480	274914.476548	40.343565
3200.040687	275617.796070	40.348583
3203.421680	276317.538556	40.353600
3207.069588	277015.582446	40.358618
3209.833463	277721.199253	40.363636
3212.887382	278433.697202	40.368653
3216.365675	279138.706821	40.373671
3219.352045	279843.710597	40.378688
3222.476220	280546.629207	40.383706
3225.455536	281254.617227	40.388724
3228.353258	281968.273988	40.393741
3231.697772	282684.520147	40.398759
3234.329427	283414.100568	40.403776
3237.167869	284129.903298	40.408794
3240.431952	284866.251191	40.413812
3243.370000	285590.301261	40.418829
3246.403004	286283.908548	40.423847
3248.947432	286995.029462	40.428864
3251.782219	287694.213893	40.433882
3255.095884	288413.781623	40.438900
3258.020719	289133.376730	40.443917
3261.080676	289861.524771	40.448935
3264.176537	290597.225239	40.453952
3267.139807	291329.078405	40.458970
3270.215815	292068.979329	40.463988
3273.383240	292829.092691	40.469005
3276.355637	293594.381035	40.474023
3279.116315	294366.852411	40.479040
3282.400493	295140.272754	40.484058
3285.483433	295928.668134	40.489076
3289.018859	296708.527722	40.494093
3292.034082	297504.528463	40.499111
3295.173807	298316.441815	40.504128
3298.533983	299116.148466	40.509146
3302.015852	299925.217573	40.514164
3305.427897	300752.106792	40.519181
3308.994623	301566.824678	40.524199
3312.263320	302381.855965	40.529216
3315.623745	303197.368032	40.534234
3319.311392	304030.255529	40.539252
3322.573763	304860.048442	40.544269
3325.923071	305694.688016	40.549287
3329.245174	306528.099674	40.554304
3332.773213	307367.963338	40.559322
3336.242072	308199.115785	40.564340
3339.772855	309045.956064	40.569357
3343.299239	309889.533407	40.574375
3346.708928	310729.636964	40.579392
3350.126213	311565.130580	40.584410
3353.554296	312419.236931	40.589428
3356.702930	313268.599928	40.594445
3359.875029	314118.197456	40.599463
3363.318651	314980.806961	40.604480
3367.080659	315827.209552	40.609498
3370.908434	316673.814323	40.614516
3374.404314	317540.376261	40.619533
3377.966528	318385.949363	40.624551
3381.607236	319248.090099	40.629568
3384.782779	320096.025060	40.634586
3388.404530	320943.188365	40.639604
3391.414491	321793.094827	40.644621
3395.080671	322657.116666	40.649639
3398.542031	323511.713535	40.654656
3402.329127	324355.559610	40.659674
3406.091902	325216.823360	40.664692
3408.617086	326065.931388	40.669709
3412.563379	326927.358452	40.674727
3416.347287	327781.637647	40.679744
3419.200987	328639.925612	40.684762
3422.925502	329493.847258	40.689780
3426.074037	330370.216309	40.694797
3429.686953	331213.132568	40.699815
3433.042631	332078.166527	40.704832
3436.415264	332938.180701	40.709850
3440.655737	333791.241161	40.714868
3443.924805	334650.319164	40.719885
3447.358065	335491.468473	40.724903
3450.990329	336351.439518	40.729920
3454.565446	337188.976608	40.734938
3458.803473	338045.997465	40.739956
3462.149916	338887.842941	40.744973
3465.638679	339730.255082	40.749991
3469.062857	340565.961602	40.755008
3472.923984	341375.860352	40.760013
3476.130313	342148.837796	40.765018
3479.787722	342899.988477	40.770023
3483.048923	343578.315902	40.775028
3486.227408	344206.276280	40.780032
3489.342990	344778.326697	40.785037
3492.265769	345302.498797	40.790042
3495.055103	345762.336365	40.795047
3497.513915	346156.855879	40.800052
3499.677825	346524.061613	40.805056
3501.948425	346835.290955	40.810061
3504.409134	347086.312250	40.815066
3506.226854	347304.179548	40.820071
3508.172119	347465.435290	40.825076
3509.359483	347591.649725	40.830080
3510.685182	347687.742160	40.835085
3512.710245	347727.948748	40.840090
3514.054211	347756.948905	40.845095
3514.966162	347744.273393	40.850100
3516.337290	347693.621591	40.855104
3517.154582	347629.862146	40.860109
3518.209595	347524.296533	40.865114
3518.876560	347404.503848	40.870119
3519.682146	347273.248922	40.875124
3520.523383	347116.158502	40.880128
3520.727837	346936.972808	40.885133
3521.332812	346743.588389	40.890138
3521.875353	346539.560341	40.895143
3522.666010	346309.662237	40.900148
3523.097973	346075.878006	40.905152
3523.001367	345825.624008	40.910157
3523.303293	345566.026155	40.915162
3523.686220	345300.922057	40.920167
3523.853336	345021.561210	40.925172
3524.232430	344746.639628	40.930176
3524.151762	344469.753733	40.935181
3524.407504	344157.396163	40.940186
3524.248139	343863.050762	40.945191
3524.561635	343554.085627	40.950196
3524.592539	343247.272219	40.955200
3524.446750	342933.644170	40.960205
3524.750796	342617.349498	40.965210
3524.699857	342300.242946	40.970215
3524.910424	341967.201068	40.975220
3524.967173	341652.411019	40.980224
3524.952943	341311.719163	40.985229
3524.830775	340991.942036	40.990234
3524.728754	340651.104934	40.995239
3524.994105	340316.030045	41.000244
3524.691063	339988.186090	41.005248
3524.527782	339650.095135	41.010253
3524.641241	339309.313148	41.015258
3524.379283	338983.233498	41.020263
3524.256909	338642.888885	41.025268
3524.333860	338302.560742	41.030272
3524.297421	337969.570764	41.035277
3524.453723	337629.656164	41.040282
3523.763233	337289.006146	41.045287
3523.330925	336960.925883	41.050292
3523.472828	336629.701259	41.055296
3522.992385	336308.717707	41.060301
3523.394520	335982.456355	41.065306
3522.662191	335659.929803	41.070311
3522.599627	335333.735352	41.075316
3522.746588	335015.999359	41.080320
3522.092346	334694.672886	41.085325
3521.912126	334372.989777	41.090330
3521.717802	334060.283619	41.095335
3521.867908	333747.622728	41.100340
3521.758068	333426.810612	41.105344
3521.507710	333124.761629	41.110349
3521.623994	332812.428883	41.115354
3521.036809	332523.983492	41.120359
3521.216448	332209.957293	41.125364
3521.009184	331915.267592	41.130368
3521.080096	331600.134295	41.135373
3520.598506	331295.461819	41.140378
3520.475503	331000.980812	41.145383
3520.153755	330707.088179	41.150388
3520.277846	330409.740820	41.155392
3519.981149	330120.824976	41.160397
3519.955108	329830.872707	41.165402
3519.712322	329546.039179	41.170407
3519.413858	329252.793208	41.175412
3519.221604	328972.678559	41.180416
3518.964286	328693.309717	41.185421
3518.822022	328403.263303	41.190426
3518.393641	328145.181645	41.195431
3518.218839	327869.507722	41.200436
3518.558877	327602.730417	41.205440
3517.759893	327340.148360	41.210445
3518.114854	327065.378067	41.215450
3517.831834	326817.312548	41.220455
3517.792156	326546.772033	41.225460
3517.683852	326291.095725	41.230464
3517.782978	326043.677929	41.235469
3517.370496	325777.413125	41.240474
3517.010000	325526.070336	41.245479
3516.692976	325260.346842	41.250484
3516.763173	325012.215020	41.255488
3516.510187	324774.027638	41.260493
3516.747997	324527.240325	41.265498
3516.160180	324294.317342	41.270503
3516.470498	324048.507916	41.275508
3515.844237	323807.676800	41.280512
3515.856334	323577.835816	41.285517
3515.824842	323330.269398	41.290522
3515.588169	323111.912269	41.295527
3515.312313	322877.507945	41.300532
3515.158659	322649.595687	41.305536
3514.727671	322416.866592	41.310541
3514.644878	322199.345579	41.315546
3514.372139	321986.686700	41.320551
3514.210851	321760.933193	41.325556
3514.293260	321558.316287	41.330560
3514.070930	321347.121828	41.335565
3513.989538	321121.555939	41.340570
3513.892803	320933.668562	41.345575
3513.590866	320729.581360	41.350580
3513.806643	320522.486565	41.355584
3513.523834	320315.112544	41.360589
3513.308566	320123.016958	41.365594
3512.957242	319932.035747	41.370599
3512.946943	319731.256412	41.375604
3512.886913	319539.897187	41.380608
3512.713731	319355.423977	41.385613
3512.917367	319156.872809	41.390618
3512.618275	318981.195004	41.395623
3512.238850	318782.606072	41.400628
3512.437119	318607.027092	41.405632
3512.093157	318425.807746	41.410637
3512.039292	318242.227070	41.415642
3512.203934	318079.702989	41.420647
3511.740456	317888.374138	41.425652
3511.510544	317718.583041	41.430656
3511.600412	317543.881791	41.435661
3511.162310	317368.244691	41.440666
3511.283833	317210.659996	41.445671
3511.006808	317034.563864	41.450676
3510.873391	316872.845218	41.455680
3510.547095	316714.870803	41.460685
3510.611991	316553.399865	41.465690
3510.412383	316402.554020	41.470695
3510.004607	316244.946882	41.475700
3510.319403	316092.442093	41.480704
3510.279660	315945.309873	41.485709
3510.126865	315796.999004	41.490714
3509.857876	315646.797549	41.495719
3510.103929	315489.289089	41.500724
3510.257603	315347.824045	41.505728
3509.615767	315207.271684	41.510733
3509.738215	315053.953810	41.515738
3509.775347	314917.416304	41.520743
3509.396318	314778.373606	41.525748
3509.399912	314632.858756	41.530752
3509.435156	314496.600168	41.535757
3509.440204	314343.807138	41.540762
3509.248594	314221.552084	41.545767
3508.675175	314081.418103	41.550772
3509.077902	313949.731314	41.555776
3508.837392	313813.386582	41.560781
3508.955724	313693.651563	41.565786
3508.743927	313568.064682	41.570791
3508.948834	313423.786756	41.575796
3508.675587	313298.717644	41.580800
3508.175003	313168.518422	41.585805
3508.570987	313035.456054	41.590810
3508.197745	312922.437027	41.595815
3508.335242	312801.958800	41.600820
3508.398965	312677.802246	41.605824
3508.153839	312562.930264	41.610829
3508.194507	312433.305940	41.615834
3508.108152	312322.581573	41.620839
3508.003771	312201.579813	41.625844
3507.618681	312081.664891	41.630848
3507.570541	311981.926193	41.635853
3507.544835	311857.425207	41.640858
3507.642267	311748.019368	41.645863
3507.569794	311634.008715	41.650868
3507.566890	311523.345755	41.655872
3507.221681	311420.700601	41.660877
3507.318533	311313.329513	41.665882
3507.340878	311209.863061	41.670887
3507.159143	311101.084626	41.675892
3507.057116	310997.230018	41.680896
3506.738032	310889.541307	41.685901
3507.220125	310795.798835	41.690906
3506.338504	310694.279264	41.695911
3506.541347	310600.452835	41.700916
3506.916403	310507.489919	41.705920
3506.627819	310407.861838	41.710925
3506.591116	310299.237023	41.715930
3506.365061	310206.545625	41.720935
3506.256072	310115.744237	41.725940
3506.561228	310020.093971	41.730944
3506.324344	309943.816807	41.735949
3506.332078	309851.215406	41.740954
3506.170929	309777.318126	41.745959
3506.009080	309669.856556	41.750964
3506.393848	309573.200532	41.755968
3505.706508	309487.857659	41.760973
3505.965694	309402.850147	41.765978
3505.979739	309324.726043	41.770983
3505.627999	309243.020079	41.775988
3505.656122	309155.096405	41.780992
3505.693532	309073.074845	41.785997
3505.627264	308992.112688	41.791002
3505.444646	308910.456066	41.796007
3505.072301	308831.500925	41.801012
3505.421624	308749.786318	41.806016
3505.274319	308687.540055	41.811021
3505.326084	308614.396582	41.816026
3505.206510	308544.766077	41.821031
3505.161776	308466.191732	41.826036
3505.083051	308390.040084	41.831040
3505.236945	308317.185570	41.836045
3505.204718	308240.695602	41.841050
3505.030223	308176.009978	41.846055
3505.142799	308093.135253	41.851060
3505.031152	308022.510310	41.856064
3504.959717	307961.498198	41.861069
3504.931493	307885.745035	41.866074
3504.552203	307820.683798	41.871079
3504.911621	307754.616313	41.876084
3504.725903	307692.273003	41.881088
3504.640809	307632.356876	41.886093
3504.796988	307551.433907	41.891098
3504.984108	307499.542038	41.896103
3504.919104	307429.163433	41.901108
3504.842358	307355.172951	41.906112
3504.844179	307294.504836	41.911117
3504.958270	307213.842377	41.916122
3504.578892	307151.579559	41.921127
3504.451304	307080.497698	41.926132
3504.706140	307032.157491	41.931136
3504.481487	306968.139780	41.936141
3504.762596	306901.345407	41.941146
3504.412856	306832.257435	41.946151
3504.515388	306773.837834	41.951156
3504.405325	306713.161054	41.956160
3504.217405	306662.217637	41.961165
3504.454560	306588.049699	41.966170
3504.145703	306534.223944	41.971175
3504.382317	306484.740879	41.976180
3504.257115	306420.248847	41.981184
3503.847922	306366.922120	41.986189
3503.863366	306307.853930	41.991194
3503.967744	306248.364590	41.996199
3504.094678	306190.093186	42.001204
3504.080629	306135.813736	42.006208
3503.783269	306094.837255	42.011213
3504.323399	306036.221138	42.016218
3504.084971	305980.526028	42.021223
3503.671667	305927.555759	42.026228
3504.116661	305878.268558	42.031232
3503.893495	305833.132121	42.036237
3504.230414	305774.471125	42.041242
3504.037369	305724.163779	42.046247
3503.788844	305662.438529	42.051252
3503.958796	305622.152069	42.056256
3503.637702	305565.705960	42.061261
3503.932900	305506.567648	42.066266
3503.684525	305463.776123	42.071271
3503.644156	305403.570400	42.076276
3503.541260	305353.910266	42.081280
3503.640821	305310.173500	42.086285
3503.611112	305262.741348	42.091290
3503.561694	305215.388580	42.096295
3503.594332	305164.765457	42.101300
3503.365956	305118.687582	42.106304
3503.361234	305075.475901	42.111309
3503.560952	305023.732204	42.116314
3503.372931	304982.610483	42.121319
3503.141077	304939.994079	42.126324
3503.279383	304900.933558	42.131328
3503.506186	304858.830713	42.136333
3503.346047	304804.776274	42.141338
3503.235061	304764.304015	42.146343
3502.759807	304731.218074	42.151348
3503.085473	304689.812213	42.156352
3502.832636	304651.576133	42.161357
3503.101314	304607.888676	42.166362
3502.931726	304576.230909	42.171367
3503.173912	304535.703255	42.176372
3503.260021	304493.520309	42.181376
3503.467908	304465.646322	42.186381
3503.309565	304413.245404	42.191386
3503.096175	304386.149822	42.196391
3502.957613	304343.136594	42.201396
3503.129490	304299.871201	42.206400
3503.033571	304266.852903	42.211405
3502.949559	304211.767958	42.216410
3502.646826	304175.422592	42.221415
3502.962428	304144.528541	42.226420
3503.119624	304108.772913	42.231424
3502.908224	304061.088109	42.236429
3503.213132	304025.360229	42.241434
3502.735108	303990.823614	42.246439
3502.534442	303947.896115	42.251444
3502.676706	303923.645952	42.256448
3502.227826	303899.004652	42.261453
3502.672164	303858.012216	42.266458
3502.607044	303839.444277	42.271463
3502.813554	303801.212101	42.276468
3503.099162	303767.370343	42.281472
3502.741292	303731.160534	42.286477
3502.953134	303699.747995	42.291482
3502.736209	303670.107608	42.296487
3502.709492	303624.556765	42.301492
3503.155405	303602.269517	42.306496
3502.664641	303562.619186	42.311501
3502.913043	303518.399531	42.316506
3502.605700	303490.401972	42.321511
3502.569337	303461.522185	42.326516
3502.775758	303423.467895	42.331520
3502.451731	303386.005507	42.336525
3502.687278	303359.628150	42.341530
3502.545440	303329.288681	42.346535
3502.810560	303298.834670	42.351540
3502.946104	303260.053292	42.356544
3502.631173	303231.496879	42.361549
3502.756700	303179.533885	42.366554
3502.756735	303153.905846	42.371559
3502.464172	303122.571818	42.376564
3502.431632	303092.164223	42.381568
3502.324699	303067.189117	42.386573
3502.607835	303047.904746	42.391578
3502.646604	303014.737344	42.396583
3502.619030	302987.510180	42.401588
3502.395780	302942.549371	42.406592
3502.233802	302930.638748	42.411597
3502.381585	302899.719296	42.416602
3502.749527	302867.289294	42.421607
3502.489063	302835.568323	42.426612
3502.700175	302807.362091	42.431616
3502.447319	302772.662214	42.436621
3502.685360	302741.295904	42.441626
3502.501045	302718.114249	42.446631
3502.529171	302682.632325	42.451636
3502.711606	302660.207717	42.456640
3502.465155	302631.054914	42.461645
3502.298770	302589.495256	42.466650
3502.334139	302570.122194	42.471655
3502.149378	302539.967131	42.476660
3502.442538	302507.624951	42.481664
3502.225010	302487.935091	42.486669
3502.572297	302451.359647	42.491674
3502.223846	302441.768603	42.496679
3502.610319	302402.871011	42.501684
3502.582623	302382.006163	42.506688
3502.024247	302350.840484	42.511693
3502.059127	302331.569213	42.516698
3502.100317	302304.050990	42.521703
3501.955434	302284.171543	42.526708
3502.223253	302258.806608	42.531712
3502.060657	302234.145216	42.536717
3502.284902	302202.398985	42.541722
3502.016383	302184.167664	42.546727
3501.824801	302167.654947	42.551732
3502.298721	302132.179309	42.556736
3501.972553	302118.232674	42.561741
3502.101486	302083.930765	42.566746
3502.346451	302071.930875	42.571751
3502.015177	302047.219414	42.576756
3502.237408	302026.493508	42.581760
3502.138754	301998.946088	42.586765
3502.335825	301977.842336	42.591770
3502.310572	301952.090413	42.596775
3502.028701	301922.102884	42.601780
3502.310754	301899.738732	42.606784
3501.784729	301874.675878	42.611789
3502.140178	301855.863330	42.616794
3502.204750	301825.287119	42.621799
3502.013290	301805.033014	42.626804
3502.092943	301777.508504	42.631808
3502.004010	301765.484395	42.636813
3502.213477	301727.453856	42.641818
3502.078403	301712.433757	42.646823
3501.808051	301690.003175	42.651828
3502.210409	301670.903270	42.656832
3501.755967	301653.897021	42.661837
3501.816598	301637.319257	42.666842
3501.964463	301612.354530	42.671847
3502.005778	301599.444692	42.676852
3501.888122	301571.441907	42.681856
3501.957372	301555.982607	42.686861
3501.979403	301532.691821	42.691866
3502.035705	301511.660794	42.696871
3501.646168	301491.590242	42.701876
3502.502609	301462.035312	42.706880
3501.974749	301452.879351	42.711885
3501.779525	301422.674387	42.716890
3501.987123	301404.113854	42.721895
3502.047813	301383.921971	42.726900
3501.992080	301360.566914	42.731904
3501.529501	301348.473872	42.736909
3502.068268	301329.276166	42.741914
3502.035098	301308.869870	42.746919
3501.617817	301288.345461	42.751924
3501.963585	301259.175670	42.756928
3501.666764	301246.853081	42.761933
3501.734928	301232.691859	42.766938
3501.883115	301205.334497	42.771943
3501.674145	301197.375737	42.776948
3501.894445	301181.383694	42.781952
3501.866105	301162.681806	42.786957
3502.056045	301140.102678	42.791962
3502.116862	301117.034707	42.796967
3501.839069	301102.494869	42.801972
3502.169016	301071.749483	42.806977
3501.974465	301057.680189	42.811981
3501.766956	301033.686990	42.816986
3501.834453	301017.362472	42.821991
3501.817999	300992.372244	42.826996
3501.936389	300973.036524	42.832001
3501.607448	300959.395432	42.837005
3501.619366	300937.098563	42.842010
3501.800911	300932.183749	42.847015
3502.146286	300914.288688	42.852020
3502.198871	300895.446799	42.857025
3501.821160	300864.837382	42.862029
3501.877904	300847.292836	42.867034
3501.734674	300831.103011	42.872039
3502.029437	300818.280617	42.877044
3501.903295	300797.634151	42.882049
3501.630495	300771.360434	42.887053
3501.707762	300759.971847	42.892058
3501.785257	300742.882145	42.897063
3501.917066	300728.176364	42.902068
3502.030443	300701.384116	42.907073
3502.057107	300671.449455	42.912077
3501.825195	300659.549255	42.917082
3502.279082	300638.786595	42.922087
3502.201895	300623.375372	42.927092
3502.197301	300597.390507	42.932097
3501.760016	300576.665343	42.937101
3501.798512	300550.164692	42.942106
3501.841073	300532.138687	42.947111
3501.486551	300508.473654	42.952116
3501.771497	300486.439330	42.957121
3501.429721	300481.860805	42.962125
3501.580226	300462.978006	42.967130
3501.981316	300457.774312	42.972135
3501.751819	300442.794072	42.977140
3502.018682	300414.094285	42.982145
3501.809372	300402.445009	42.987149
3501.586777	300374.534361	42.992154
3501.896133	300359.622562	42.997159
3501.718043	300346.721274	43.002164
3501.757532	300326.099635	43.007169
3501.544774	300321.348218	43.012173
3501.606142	300298.050748	43.017178
3501.666732	300291.169574	43.022183
3501.390935	300279.632472	43.027188
3501.723815	300257.005177	43.032193
3501.972548	300250.578162	43.037197
3501.804246	300220.724635	43.042202
3501.692092	300205.318760	43.047207
3501.597212	300206.937226	43.052212
3501.667652	300177.733541	43.057217
3501.642182	300164.655640	43.062221
3501.638044	300147.374902	43.067226
3501.649383	300137.599936	43.072231
3501.605960	300107.981339	43.077236
3501.500660	300095.475836	43.082241
3501.416923	300088.795362	43.087245
3501.377346	300069.840337	43.092250
3501.301005	300056.235881	43.097255
3501.394802	300059.860977	43.102260
3501.791629	300040.455942	43.107265
3501.649362	300021.466052	43.112269
3501.817386	300009.503184	43.117274
3501.779316	299991.031477	43.122279
3501.721740	299979.231130	43.127284
3501.783509	299966.495865	43.132289
3501.386992	299938.535829	43.137293
3501.510914	299932.611870	43.142298
3501.919084	299919.364308	43.147303
3501.638939	299892.047798	43.152308
3501.819057	299882.119141	43.157313
3501.625157	299871.994440	43.162317
3501.741830	299838.609277	43.167322
3501.832088	299838.824420	43.172327
3501.683719	299815.432275	43.177332
3502.012806	299795.146935	43.182337
3501.774797	299782.331236	43.187341
3501.971174	299756.492711	43.192346
3501.616961	299755.810178	43.197351
3501.588939	299731.228404	43.202356
3501.657612	299710.805584	43.207361
3501.560142	299700.996648	43.212365
3501.677849	299683.900327	43.217370
3501.525955	299670.180328	43.222375
3501.436679	299658.842999	43.227380
3501.676748	299640.022268	43.232385
3501.553967	299638.005512	43.237389
3501.392029	299628.639321	43.242394
3501.752734	299607.178188	43.247399
3501.697209	299581.658932	43.252404
3501.715394	299575.675110	43.257409
3501.663935	299556.009115	43.262413
3502.026331	299540.783379	43.267418
3502.160733	299530.505481	43.272423
3501.566153	299505.324983	43.277428
3501.603687	299492.109812	43.282433
3501.692866	299479.624667	43.287437
3501.609333	299452.429909	43.292442
3501.733767	299438.488488	43.297447
3501.707537	299425.181462	43.302452
3501.952427	299403.712904	43.307457
3501.914995	299391.832926	43.312461
3502.101533	299375.183881	43.317466
3501.925139	299349.276184	43.322471
3501.863164	299329.662656	43.327476
3502.047347	299312.479471	43.332481
3501.957302	299291.317752	43.337485
3501.574619	299286.389194	43.342490
3501.944268	299256.654654	43.347495
3501.881043	299238.670212	43.352500
3502.053097	299223.016012	43.357505
3501.904133	299196.442203	43.362509
3501.891542	299177.711719	43.367514
3502.133071	299155.098251	43.372519
3501.719285	299133.707113	43.377524
3501.717271	299104.310568	43.382529
3501.829968	299098.108302	43.387533
3501.908775	299083.639433	43.392538
3501.804946	299062.072548	43.397543
3501.868515	299049.234981	43.402548
3501.691052	299025.465268	43.407553
3501.769681	299013.974296	43.412557
3501.852039	298995.025289	43.417562
3501.982930	298976.908605	43.422567
3501.508704	298959.268301	43.427572
3501.620613	298931.915471	43.432577
3501.670869	298917.730994	43.437581
3501.580953	298906.800843	43.442586
3501.349917	298894.900122	43.447591
3501.245667	298889.037175	43.452596
3501.484176	298879.455538	43.457601
3501.250786	298869.642251	43.462605
3501.336292	298847.892970	43.467610
3501.558761	298844.167821	43.472615
3501.317245	298839.242605	43.477620
3501.679075	298824.271282	43.482625
3501.671224	298807.423388	43.487629
3501.449984	298805.651064	43.492634
3501.663589	298777.696859	43.497639
3501.533487	298769.343631	43.502644
3501.687816	298756.797232	43.507649
3501.412895	298753.124387	43.512653
3501.403507	298729.735505	43.517658
3501.762850	298716.240767	43.522663
3501.197433	298709.660883	43.527668
3501.465062	298682.919889	43.532673
3501.311850	298672.712249	43.537677
3501.352143	298668.837404	43.542682
3501.452264	298672.054369	43.547687
3501.547648	298646.282017	43.552692
3501.533673	298623.326495	43.557697
3501.500860	298627.556882	43.562701
3501.406983	298603.570302	43.567706
3501.527439	298586.218689	43.572711
3501.429895	298589.670180	43.577716
3501.462344	298562.151424	43.582721
3501.647680	298547.029454	43.587725
3501.415261	298533.525378	43.592730
3501.627999	298522.166051	43.597735
3501.670694	298515.236549	43.602740
3501.704887	298489.473691	43.607745
3501.861933	298488.100356	43.612749
3501.607310	298458.692057	43.617754
3501.228192	298444.014637	43.622759
3501.201573	298440.226595	43.627764
3501.123768	298424.305804	43.632769
3501.340108	298413.607652	43.637773
3501.680131	298405.537202	43.642778
3501.586404	298398.730822	43.647783
3501.503184	298379.654778	43.652788
3501.732342	298359.053654	43.657793
3501.402204	298352.182420	43.662797
3501.740831	298342.534134	43.667802
3501.816446	298324.833117	43.672807
3501.613024	298318.018425	43.677812
3501.783761	298293.634009	43.682817
3501.432665	298288.471353	43.687821
3501.324586	298275.405918	43.692826
3501.408807	298256.227296	43.697831
3501.291424	298253.904217	43.702836
3501.544380	298231.161325	43.707841
3501.490153	298233.638874	43.712845
3501.208143	298208.307107	43.717850
3501.629275	298183.119925	43.722855
3501.408689	298180.914787	43.727860
3501.579832	298181.066386	43.732865
3501.300946	298158.228445	43.737869
3501.329697	298152.090103	43.742874
3501.761754	298149.630215	43.747879
3501.399709	298140.142342	43.752884
3501.453824	298111.245545	43.757889
3501.355723	298100.952827	43.762893
3501.497760	298103.374246	43.767898
3501.458837	298081.364141	43.772903
3501.588477	298064.876314	43.777908
3501.319557	298057.944568	43.782913
3501.322737	298059.242336	43.787917
3500.888963	298042.868039	43.792922
3501.221409	298023.726888	43.797927
3501.202909	298023.806326	43.802932
3501.364508	298017.698105	43.807937
3501.470624	298019.412473	43.812941
3501.048268	298001.178347	43.817946
3501.163722	297983.343731	43.822951
3500.990773	297975.022535	43.827956
3501.155478	297965.325018	43.832961
3501.062300	297965.288869	43.837965
3501.336081	297957.712309	43.842970
3501.514625	297959.669880	43.847975
3501.168611	297942.594616	43.852980
3501.424125	297914.735237	43.857985
3501.298455	297918.496596	43.862989
3501.423597	297904.885563	43.867994
3501.295739	297890.295978	43.872999
3501.291010	297893.427569	43.878004
3501.349792	297879.674189	43.883009
3501.484898	297874.104598	43.888013
3501.403944	297858.362306	43.893018
3501.177801	297834.930579	43.898023
3501.346755	297839.460364	43.903028
3501.695807	297824.694392	43.908033
3501.322508	297811.492145	43.913037
3501.569282	297801.985390	43.918042
3501.439320	297790.730397	43.923047
3501.286084	297788.438357	43.928052
3501.466724	297757.358125	43.933057
3501.522040	297754.906215	43.938061
3501.362824	297747.091890	43.943066
3501.472204	297723.047703	43.948071
3501.442763	297715.289442	43.953076
3501.286037	297706.863859	43.958081
3501.600505	297699.204546	43.963085
3501.573324	297675.563477	43.968090
3501.602884	297661.687349	43.973095
3501.454302	297651.835136	43.978100
3501.565354	297633.186612	43.983105
3501.228860	297625.043648	43.988109
3501.308491	297621.162581	43.993114
3501.271887	297607.627668	43.998119
3501.308064	297605.865966	44.003124
3501.477402	297586.902883	44.008129
3501.694238	297572.590211	44.013133
3501.232467	297574.622450	44.018138
3501.542388	297552.455790	44.023143
3501.580283	297539.392815	44.028148
3501.493480	297516.117339	44.033153
3501.508751	297518.584054	44.038157
3501.394930	297498.647101	44.043162
3501.546555	297482.766532	44.048167
3501.353629	297482.058753	44.053172
3501.592200	297467.106338	44.058177
3501.322915	297456.534832	44.063181
3501.284100	297445.672764	44.068186
3501.249008	297446.594738	44.073191
3501.192049	297444.923950	44.078196
3501.689928	297425.324035	44.083201
3501.642595	297400.031573	44.088205
3501.373591	297402.008228	44.093210
3501.742887	297373.850813	44.098215
3501.057180	297369.223986	44.103220
3501.467806	297361.549594	44.108225
3501.598831	297357.151418	44.113229
3501.191443	297342.198148	44.118234
3501.761709	297322.052371	44.123239
3501.368539	297314.503638	44.128244
3501.592338	297301.996958	44.133249
3501.374816	297292.791781	44.138253
3501.350861	297279.305717	44.143258
3501.332466	297272.181989	44.148263
3501.324212	297257.013579	44.153268
3501.449443	297240.602559	44.158273
3501.538727	297231.400311	44.163277
3501.511006	297230.692154	44.168282
3501.330651	297203.969588	44.173287
3501.135679	297200.360499	44.178292
3500.919450	297185.071867	44.183297
3501.170588	297186.941758	44.188301
3500.876568	297178.639372	44.193306
3501.174453	297186.661549	44.198311
3501.191361	297184.979205	44.203316
3501.180661	297148.481639	44.208321
3501.180314	297143.722192	44.213325
3501.151893	297144.414052	44.218330
3501.215304	297133.637754	44.223335
3501.070819	297140.940058	44.228340
3501.397825	297126.559144	44.233345
3501.605529	297116.523871	44.238349
3501.688525	297106.788075	44.243354
3501.782438	297090.076473	44.248359
3501.406521	297077.739862	44.253364
3501.421458	297059.895217	44.258369
3501.471584	297060.829327	44.263373
3501.417779	297034.494143	44.268378
3501.588586	297021.333910	44.273383
3501.322339	297014.299805	44.278388
3501.336232	296998.542445	44.283393
3501.396273	296977.025496	44.288397
3501.467378	296967.469706	44.293402
3501.627313	296957.696403	44.298407
3501.069572	296955.874816	44.303412
3501.087062	296932.048282	44.308417
3501.316566	296931.732608	44.313421
3501.458199	296925.347407	44.318426
3501.254295	296916.878176	44.323431
3501.124314	296919.647609	44.328436
3501.360002	296899.095837	44.333441
3501.636892	296883.551858	44.338445
3501.489440	296886.298571	44.343450
3501.378438	296866.844562	44.348455
3501.514196	296847.733763	44.353460
3501.593078	296830.489921	44.358465
3501.224239	296839.838129	44.363469
3501.231686	296822.987248	44.368474
3501.286727	296796.609484	44.373479
3501.576138	296801.476864	44.378484
3501.425705	296786.585086	44.383489
3501.506544	296769.799075	44.388493
3501.328737	296758.958606	44.393498
3501.602267	296755.378055	44.398503
3501.587143	296744.333978	44.403508
3501.319347	296725.540760	44.408513
3501.621435	296710.298232	44.413517
3501.465266	296707.752075	44.418522
3501.290733	296678.126699	44.423527
3501.104037	296678.945122	44.428532
3501.291516	296668.276605	44.433537
3501.005407	296668.626961	44.438541
3501.449765	296668.659491	44.443546
3501.745169	296648.429183	44.448551
3501.606707	296639.313351	44.453556
3501.606080	296627.248861	44.458561
3501.524218	296612.448130	44.463565
3501.582569	296582.073608	44.468570
3501.194348	296579.487364	44.473575
3501.205819	296575.565975	44.478580
3501.341752	296560.476650	44.483585
3501.059440	296551.485106	44.488589
3500.936205	296543.385005	44.493594
3501.326032	296530.979465	44.498599
3501.002270	296531.462974	44.503604
3501.106158	296532.388688	44.508609
3501.298327	296534.191461	44.513613
3501.209073	296516.693826	44.518618
3501.410423	296495.765480	44.523623
3500.973245	296492.321478	44.528628
3501.116766	296488.277626	44.533633
3501.177310	296484.984889	44.538637
3500.919636	296480.036538	44.543642
3501.519193	296458.995016	44.548647
3501.249711	296457.561051	44.553652
3501.131445	296448.263859	44.558657
3501.327420	296442.455532	44.563661
3501.107684	296442.922779	44.568666
3501.538140	296411.319144	44.573671
3501.166542	296413.948203	44.578676
3501.443076	296406.981883	44.583681
3501.687304	296399.944254	44.588685
3501.327202	296377.830981	44.593690
3501.455454	296364.117279	44.598695
3501.229429	296361.429308	44.603700
3501.477056	296352.838494	44.608705
3501.324616	296334.968883	44.613709
3501.206750	296333.613023	44.618714
3501.499863	296325.829598	44.623719
3501.199475	296321.524243	44.628724
3501.493447	296295.414332	44.633729
3501.381159	296275.909416	44.638733
3500.952995	296275.416572	44.643738
3501.134703	296272.792118	44.648743
3500.917390	296269.288275	44.653748
3501.108960	296259.179015	44.658753
3501.247303	296245.387347	44.663757
3501.119030	296229.881081	44.668762
3501.451170	296219.215317	44.673767
3501.340703	296234.530208	44.678772
3501.329861	296221.041844	44.683777
3501.260381	296196.337735	44.688781
3501.300563	296188.313848	44.693786
3501.442093	296176.888823	44.698791
3501.307093	296186.200579	44.703796
3501.490842	296172.503608	44.708801
3501.340235	296153.590068	44.713805
3501.227185	296151.342584	44.718810
3501.451735	296134.712093	44.723815
3501.408584	296130.773760	44.728820
3501.306973	296112.641600	44.733825
3501.405410	296098.245255	44.738829
3501.220831	296095.703512	44.743834
3501.814394	296091.894713	44.748839
3501.258642	296076.480691	44.753844
3501.553608	296056.250243	44.758849
3501.546600	296056.073354	44.763853
3501.208086	296039.734490	44.768858
3501.682007	296031.337330	44.773863
3501.319723	296027.576151	44.778868
3501.710244	296007.661641	44.783873
3501.539069	295988.802169	44.788877
3501.349992	295983.893957	44.793882
3501.393925	295970.116983	44.798887
3501.545660	295947.898070	44.803892
3501.329989	295943.732162	44.808897
3501.362346	295931.255114	44.813901
3501.245533	295929.542732	44.818906
3501.469021	295906.294448	44.823911
3501.081267	295899.279201	44.828916
3501.094584	295889.045023	44.833921
3501.521079	295885.465958	44.838925
3501.231779	295882.584229	44.843930
3501.406191	295860.463551	44.848935
3501.403442	295850.893668	44.853940
3501.745206	295839.335458	44.858945
3501.603203	295833.808991	44.863949
3501.410259	295821.774398	44.868954
3501.318273	295810.614890	44.873959
3501.571764	295802.532147	44.878964
3501.481737	295774.343942	44.883969
3501.285840	295757.728167	44.888973
3501.482015	295761.133909	44.893978
3501.830566	295754.359879	44.898983
3501.859829	295742.825053	44.903988
3501.576290	295722.303129	44.908993
3501.619666	295697.402988	44.913997
3501.160253	295692.104306	44.919002
3501.638547	295676.706688	44.924007
3501.608772	295679.231433	44.929012
3501.493623	295645.345499	44.934017
3501.343892	295636.918516	44.939021
3501.569530	295642.585025	44.944026
3501.462631	295618.421043	44.949031
3501.350535	295606.399219	44.954036
3501.221690	295599.903436	44.959041
3501.505039	295593.292303	44.964045
3501.394412	295589.695379	44.969050
3501.414611	295567.445978	44.974055
3501.358720	295561.015146	44.979060
3501.448048	295557.845124	44.984065
3501.502061	295518.663775	44.989069
3501.482949	295509.478197	44.994074
3501.438239	295492.049648	44.999079
3501.430146	295508.901397	45.004084
3501.130104	295478.556870	45.009089
3501.743007	295471.028778	45.014093
3501.279817	295471.534093	45.019098
3501.626851	295452.058903	45.024103
3501.293062	295447.249631	45.029108
3501.402654	295419.284581	45.034113
3501.449959	295426.735294	45.039117
3501.193044	295408.907183	45.044122
3501.442563	295393.036185	45.049127
3501.324000	295386.080605	45.054132
3501.214099	295381.032695	45.059137
3501.462265	295377.481479	45.064141
3501.287424	295360.709576	45.069146
3501.414788	295341.777765	45.074151
3501.354905	295333.718497	45.079156
3501.581857	295327.141605	45.084161
3501.243798	295311.642436	45.089165
3500.968422	295303.642307	45.094170
3501.099946	295301.738359	45.099175
3501.334961	295298.265555	45.104180
3501.294135	295286.181615	45.109185
3501.066518	295270.945160	45.114189
3501.136851	295258.563844	45.119194
3501.418874	295246.734865	45.124199
3501.153370	295256.576248	45.129204
3501.134802	295253.295809	45.134209
3501.319433	295241.329334	45.139213
3501.241892	295231.872856	45.144218
3501.359038	295213.273500	45.149223
3501.609619	295214.507200	45.154228
3501.650400	295210.530229	45.159233
3501.864870	295178.221529	45.164237
3501.331709	295176.192410	45.169242
3501.560842	295166.127994	45.174247
3501.343379	295145.442813	45.179252
3501.126545	295129.619198	45.184257
3501.241893	295129.474084	45.189261
3501.090135	295132.094284	45.194266
3501.296756	295118.978926	45.199271
3501.144639	295098.716226	45.204276
3501.116595	295089.913786	45.209281
3501.148787	295088.254445	45.214285
3500.987875	295082.959946	45.219290
3501.159904	295080.464221	45.224295
3501.223642	295073.403742	45.229300
3501.253453	295058.152438	45.234305
3501.368911	295046.425822	45.239309
3501.122118	295034.577660	45.244314
3501.709816	295040.747608	45.249319
3501.400507	295028.934673	45.254324
3501.267678	295014.676031	45.259329
3501.537437	294997.656338	45.264333
3501.542523	294996.892117	45.269338
3501.541962	294972.456703	45.274343
3501.471385	294964.806317	45.279348
3501.257947	294964.916236	45.284353
3501.482912	294946.579931	45.289357
3501.380524	294924.756710	45.294362
3501.178632	294909.643409	45.299367
3501.008127	294916.542800	45.304372
3501.209439	294914.042490	45.309377
3501.268086	294911.920838	45.314381
3501.257172	294894.206833	45.319386
3501.469585	294877.374248	45.324391
3501.350696	294871.945891	45.329396
3501.136978	294867.372338	45.334401
3501.488238	294855.176101	45.339405
3501.459629	294838.762995	45.344410
3501.648033	294830.613931	45.349415
3501.512951	294831.347948	45.354420
3501.458091	294812.368094	45.359425
3501.392453	294797.462546	45.364429
3501.300493	294794.117193	45.369434
3501.506184	294777.616531	45.374439
3501.288089	294753.825930	45.379444
3501.244309	294734.538871	45.384449
3501.462377	294745.730159	45.389453
3501.345147	294740.479708	45.394458
3501.534123	294720.698083	45.399463
3501.398938	294711.148718	45.404468
3501.550047	294707.663543	45.409473
3501.474101	294688.025141	45.414477
3501.365634	294684.478732	45.419482
3501.367446	294664.039092	45.424487
3501.358486	294672.135048	45.429492
3501.218221	294649.146763	45.434497
3501.443703	294628.901229	45.439501
3501.492875	294629.122816	45.444506
3501.495490	294622.810004	45.449511
3501.425489	294607.014200	45.454516
3501.455008	294592.348264	45.459521
3501.446907	294576.873676	45.464525
3501.075319	294575.990160	45.469530
3501.241478	294566.877285	45.474535
3501.454645	294546.786372	45.479540
3501.222626	294548.222806	45.484545
3501.482392	294538.077131	45.489549
3501.469955	294524.283174	45.494554
3501.335644	294504.246571	45.499559
3501.229410	294502.354315	45.504564
3501.342882	294497.220498	45.509569
3501.255590	294491.532626	45.514573
3501.051534	294472.881435	45.519578
3501.084552	294451.215048	45.524583
3501.125835	294452.354216	45.529588
3500.888752	294446.435216	45.534593
3501.062783	294443.430070	45.539597
3500.800020	294446.042201	45.544602
3501.456065	294438.761773	45.549607
3501.102536	294432.351896	45.554612
3500.825654	294418.624711	45.559617
3501.365073	294398.100930	45.564621
3501.036680	294397.363383	45.569626
3500.985760	294400.222391	45.574631
3501.093330	294397.278541	45.579636
3500.755033	294403.236970	45.584641
3501.077258	294384.427110	45.589645
3501.087916	294395.243626	45.594650
3501.267564	294374.012460	45.599655
3501.431843	294359.045401	45.604660
3501.634454	294353.948545	45.609665
3501.504906	294355.852592	45.614669
3501.524014	294334.035611	45.619674
3501.592288	294313.534551	45.624679
3501.621240	294321.853715	45.629684
3501.583697	294300.580116	45.634689
3501.623730	294277.996219	45.639693
3501.352466	294274.882502	45.644698
3501.428035	294263.391053	45.649703
3501.379591	294247.311787	45.654708
3501.407302	294238.882314	45.659713
3501.275373	294227.194211	45.664717
3500.811829	294223.168748	45.669722
3501.245315	294222.210270	45.674727
3501.237274	294200.499301	45.679732
3501.196189	294185.437035	45.684737
3501.578813	294185.682854	45.689741
3501.072775	294185.354890	45.694746
3501.372565	294176.450151	45.699751
3501.340824	294161.055513	45.704756
3501.001639	294151.308862	45.709761
3501.365731	294134.426897	45.714765
3501.148131	294142.860994	45.719770
3501.427685	294135.970295	45.724775
3501.575770	294116.678491	45.729780
3501.105082	294098.094321	45.734785
3501.281266	294101.274198	45.739789
3501.324848	294102.183925	45.744794
3501.423437	294079.616252	45.749799
3501.301785	294069.224677	45.754804
3501.392495	294059.792615	45.759809
3501.553078	294051.342342	45.764813
3501.180033	294031.521082	45.769818
3501.249999	293961.307453	45.774823
3501.237810	293868.350422	45.779828
3500.769759	293718.624888	45.784833
3501.379515	293516.345184	45.789837
3500.656861	293272.705789	45.794842
3500.424510	292985.486679	45.799847
3500.135484	292636.801629	45.804852
3499.915587	292253.001312	45.809857
3499.259756	291818.916380	45.814861
3499.106479	291321.111340	45.819866
3498.879812	290789.152329	45.824871
3498.273418	290219.497123	45.829876
3497.780194	289593.077426	45.834881
3497.455003	288917.290835	45.839885
3496.583510	288204.823123	45.844890
3495.844151	287432.630378	45.849895
3495.014886	286619.125456	45.854900
3494.217724	285751.915494	45.859905
3493.628358	284848.460701	45.864909
3493.055518	283910.215380	45.869914
3492.375792	282906.061687	45.874919
3491.156604	281859.461512	45.879924
3490.426655	280761.748996	45.884929
3489.377016	279625.192946	45.889933
3488.251070	278441.122877	45.894938
3487.312915	277203.130530	45.899943
3486.501142	275926.525458	45.904948
3485.125551	274603.801254	45.909953
3484.178150	273225.303873	45.914957
3482.580717	271815.821789	45.919962
3481.316764	270349.457633	45.924967
3479.819010	268861.309815	45.929972
3478.295023	267322.546411	45.934977
3477.291817	265732.443735	45.939981
3475.500553	264117.433174	45.944986
3474.276330	262454.690055	45.949991
3472.807009	260750.833856	45.954996
3470.823894	259006.695350	45.960001
3469.477156	257210.710986	45.965005
3467.988408	255398.170450	45.970010
3466.511863	253528.940607	45.975015
3464.227605	251641.043659	45.980020
3462.224076	249705.608865	45.985025
3460.612872	247725.751325	45.990029
3458.507531	245727.561631	45.995034
3456.476903	243683.141177	46.000039
3454.543920	241602.547053	46.005044
3452.676212	239512.934882	46.010049
3450.586828	237359.950639	46.015053
3448.112080	235205.357255	46.020058
3446.024462	232987.860156	46.025063
3443.789895	230758.533452	46.030068
3441.047685	228506.586307	46.035073
3438.896455	226216.517206	46.040077
3436.370814	223914.356437	46.045082
3434.153259	221565.795376	46.050087
3431.782039	219192.660059	46.055092
3428.886046	216796.310887	46.060097
3426.973994	214372.618917	46.065101
3423.991126	211929.244282	46.070106
3421.177601	209456.599272	46.075111
3418.525662	206960.572675	46.080116
3415.592823	204446.408150	46.085121
3412.981956	201902.581113	46.090125
3409.923994	199334.081242	46.095130
3406.758325	196761.896142	46.100135
3403.369492	194161.880896	46.105140
3400.413785	191544.863495	46.110145
3397.443189	188925.459930	46.115149
3393.739180	186300.349411	46.120154
3390.554481	183648.307888	46.125159
3387.595358	180988.128722	46.130164
3383.589220	178325.032240	46.135169
3380.485983	175627.655491	46.140173
3377.036018	172943.533164	46.145178
3372.904222	170234.607895	46.150183
3369.218320	167536.327672	46.155188
3365.303173	164844.372033	46.160193
3361.200576	162140.676944	46.165197
3357.261116	159437.578054	46.170202
3353.240131	156730.103845	46.175207
3349.348923	154029.668019	46.180212
3344.874810	151350.473628	46.185217
3340.494847	148659.661238	46.190221
3335.560047	145983.831845	46.195226
3330.665134	143325.490622	46.200231
3325.668329	140691.405039	46.205236
3320.146222	138053.550093	46.210241
3315.040502	135404.901099	46.215245
3308.973893	132851.075560	46.220250
3302.747044	130336.207467	46.225255
3296.277689	127872.085431	46.230260
3288.768448	125457.722455	46.235265
3282.433934	123095.145402	46.240269
3274.980286	120798.658305	46.245274
3267.534397	118578.949394	46.250279
3259.482210	116422.942978	46.255284
3250.897551	114349.832155	46.260289
3242.547303	112359.421792	46.265293
3233.836441	110469.618465	46.270298
3225.535107	108656.958409	46.275303
3216.887877	106927.715025	46.280308
3207.913605	105302.722163	46.285313
3199.221077	103777.370956	46.290317
3190.158996	102351.458278	46.295322
3182.100808	101014.372831	46.300327
3173.437681	99783.273060	46.305332
3165.094554	98646.653127	46.310337
3157.071501	97583.342605	46.315341
3149.422418	96620.688119	46.320346
3142.742106	95709.164560	46.325351
3135.880131	94872.673590	46.330356
3129.226011	94110.297020	46.335361
3123.836485	93399.359273	46.340365
3117.798798	92750.791944	46.345370
3112.570866	92140.308863	46.350375
3107.616273	91574.777086	46.355380
3102.227869	91058.993448	46.360385
3097.636120	90561.950195	46.365389
3093.445527	90101.814499	46.370394
3088.480563	89660.865846	46.375399
3084.509002	89245.319619	46.380404
3080.253877	88858.970149	46.385409
3076.424683	88476.446950	46.390413
3073.097518	88120.798067	46.395418
3068.893843	87765.442986	46.400423
3065.766928	87421.142297	46.405428
3062.527470	87093.608208	46.410433
3058.985302	86754.208099	46.415437
3055.672904	86430.631270	46.420442
3052.237689	86106.022761	46.425447
3048.943609	85784.394001	46.430452
3045.816728	85461.561164	46.435457
3042.525893	85138.008018	46.440461
3039.400273	84820.695648	46.445466
3036.016240	84499.768503	46.450471
3033.123667	84168.211407	46.455476
3029.580764	83846.986086	46.460481
3026.513763	83517.458211	46.465485
3022.965088	83191.439300	46.470490
3019.455632	82858.596471	46.475495
3016.031049	82523.521259	46.480500
3012.609184	82201.431722	46.485505
3009.175599	81881.100626	46.490509
3005.845169	81554.215286	46.495514
3002.175437	81225.176598	46.500519
2998.898515	80897.858619	46.505524
2995.248561	80579.202018	46.510529
2991.918326	80244.532854	46.515533
2988.112234	79921.957885	46.520538
2984.235088	79612.620043	46.525543
2980.875810	79284.089072	46.530548
2977.487214	78975.952045	46.535553
2973.815809	78649.522296	46.540557
2970.168372	78343.274446	46.545562
2966.268215	78030.071374	46.550567
2963.011384	77718.625552	46.555572
2959.386096	77421.630568	46.560577
2955.654388	77107.497230	46.565581
2951.820322	76809.080996	46.570586
2948.592995	76504.451688	46.575591
2945.098968	76213.875548	46.580596
2941.107192	75913.156997	46.585601
2937.936600	75617.405926	46.590605
2934.196730	75328.211182	46.595610
2930.385629	75031.715812	46.600615
2926.903066	74738.867809	46.605620
2923.087529	74468.069971	46.610625
2919.472347	74173.166208	46.615629
2915.962272	73898.237270	46.620634
2912.074626	73618.684369	46.625639
2908.677567	73352.378513	46.630644
2904.921110	73076.493373	46.635649
2901.322535	72804.776859	46.640653
2897.694429	72546.934206	46.645658
2894.054814	72278.251679	46.650663
2890.435403	72017.212901	46.655668
2886.970027	71761.904739	46.660673
2883.721462	71493.930898	46.665677
2880.274440	71235.247372	46.670682
2876.555081	70976.799445	46.675687
2872.980051	70726.927601	46.680692
2868.924682	70469.895840	46.685697
2865.564265	70224.934448	46.690701
2861.954743	69972.980179	46.695706
2858.252013	69727.226298	46.700711
2854.622147	69475.267330	46.705716
2850.890375	69239.070564	46.710721
2847.856252	68998.957883	46.715725
2843.867489	68754.292716	46.720730
2840.689938	68512.023204	46.725735
2836.933251	68266.044042	46.730740
2833.205975	68030.194066	46.735745
2829.997890	67794.436447	46.740749
2826.647842	67552.634597	46.745754
2823.377543	67314.332910	46.750759
2819.570561	67064.164501	46.755764
2816.212493	66830.026152	46.760769
2813.137873	66588.298244	46.765773
2809.168123	66351.346378	46.770778
2806.131020	66117.538880	46.775783
2802.591482	65874.862155	46.780788
2798.748375	65631.505276	46.785793
2795.663570	65388.019439	46.790797
2792.093602	65144.719729	46.795802
2788.612795	64896.533735	46.800807
2784.893499	64656.892706	46.805812
2781.271435	64418.869960	46.810817
2777.995560	64180.947651	46.815821
2774.720834	63940.831354	46.820826
2770.891454	63696.297779	46.825831
2767.374091	63451.394102	46.830836
2763.692335	63210.574152	46.835841
2760.532402	62976.440552	46.840845
2757.013465	62743.742535	46.845850
2753.442297	62496.324319	46.850855
2749.841474	62249.128989	46.855860
2746.308142	62018.585158	46.860865
2743.127113	61770.573706	46.865869
2738.936409	61531.493368	46.870874
2735.915240	61287.891534	46.875879
2732.296174	61051.664787	46.880884
2728.860677	60815.855829	46.885889
2725.525364	60576.562123	46.890893
2722.106144	60335.411778	46.895898
2718.646077	60097.709736	46.900903
2715.088969	59847.866329	46.905908
2711.079592	59610.299365	46.910913
2707.966361	59377.512568	46.915917
2704.700804	59133.450001	46.920922
2700.811419	58893.091816	46.925927
2697.582709	58653.038795	46.930932
2693.839529	58410.428855	46.935937
2690.396423	58164.119392	46.940941
2686.830545	57933.650857	46.945946
2683.195446	57685.053869	46.950951
2680.205959	57438.909282	46.955956
2676.230361	57205.631013	46.960961
2672.973467	56963.517939	46.965965
2669.285971	56736.639542	46.970970
2665.854905	56498.397215	46.975975
2662.633991	56241.228938	46.980980
2658.601675	56014.995057	46.985985
2655.651125	55750.873771	46.990989
2651.639249	55526.678033	46.995994
2647.866004	55290.144593	47.000999
2644.738114	55052.021561	47.006004
2641.051418	54810.612979	47.011009
2637.647352	54565.432043	47.016013
2634.319113	54328.844928	47.021018
2630.902420	54093.473116	47.026023
2627.519975	53848.898951	47.031028
2624.111901	53613.048412	47.036033
2620.138109	53372.200641	47.041037
2616.780057	53135.757050	47.046042
2613.199539	52883.135080	47.051047
2610.164882	52637.986208	47.056052
2606.438221	52403.770979	47.061057
2602.839958	52154.801093	47.066061
2599.430797	51921.936696	47.071066
2595.912494	51678.618103	47.076071
2592.451771	51438.598128	47.081076
2588.980975	51190.126115	47.086081
2585.691159	50945.256984	47.091085
2581.919482	50704.500294	47.096090
2578.100053	50454.105185	47.101095
2574.758007	50219.204787	47.106100
2571.147004	49983.765266	47.111105
2567.844243	49740.122506	47.116109
2564.426914	49508.216120	47.121114
2560.558669	49260.397930	47.126119
2557.142553	49012.384833	47.131124
2553.755165	48772.279633	47.136129
2550.347581	48526.566625	47.141133
2546.605810	48296.010874	47.146138
2543.382816	48053.686538	47.151143
2539.773060	47811.628245	47.156148
2536.019781	47579.242161	47.161153
2532.732543	47329.165834	47.166157
2529.196086	47081.801447	47.171162
2525.702723	46838.834681	47.176167
2522.057904	46600.543185	47.181172
2518.585220	46363.432316	47.186177
2515.253165	46113.084689	47.191181
2512.061202	45877.526921	47.196186
2508.348053	45643.296201	47.201191
2505.157521	45389.433637	47.206196
2501.369668	45140.474598	47.211201
2497.855150	44899.884935	47.216205
2494.455763	44656.153323	47.221210
2490.757273	44416.720143	47.226215
2487.231923	44164.236596	47.231220
2483.609817	43914.922833	47.236225
2480.138838	43680.046977	47.241229
2476.735403	43441.516678	47.246234
2473.215293	43192.949697	47.251239
2469.695474	42946.528834	47.256244
2466.664020	42707.910192	47.261249
2462.816744	42460.943542	47.266253
2459.201503	42214.412603	47.271258
2455.541080	41967.935876	47.276263
2452.516637	41726.149878	47.281268
2448.237045	41498.271985	47.286273
2444.646525	41252.375714	47.291277
2440.835815	41013.092052	47.296282
2437.129466	40786.951693	47.301287
2433.774259	40549.903527	47.306292
2430.540714	40312.223863	47.311297
2427.244533	40087.757564	47.316301
2423.682525	39855.124264	47.321306
2420.219928	39608.110575	47.326311
2416.709904	39369.996239	47.331316
2413.466559	39131.589189	47.336321
2410.171385	38891.747307	47.341325
2406.657093	38652.950438	47.346330
2402.879303	38411.826255	47.351335
2399.649832	38158.281412	47.356340
2396.405029	37923.330516	47.361345
2393.187054	37666.993760	47.366349
2389.697222	37418.107412	47.371354
2386.009226	37171.879575	47.376359
2382.687708	36916.937339	47.381364
2379.053460	36685.160981	47.386369
2375.113460	36430.467106	47.391373
2371.653322	36178.439813	47.396378
2368.468205	35928.445427	47.401383
2364.944853	35675.299236	47.406388
2361.160463	35433.265066	47.411393
2357.685056	35175.743304	47.416397
2354.248160	34933.451283	47.421402
2351.079698	34689.801538	47.426407
2347.856852	34418.563704	47.431412
2343.890752	34182.505427	47.436417
2340.771120	33915.390796	47.441421
2337.167221	33674.812754	47.446426
2333.479345	33417.199875	47.451431
2330.204716	33164.051180	47.456436
2326.682377	32920.629374	47.461441
2323.452364	32654.942477	47.466445
2320.234862	32393.883914	47.471450
2316.413233	32131.522387	47.476455
2312.968839	31869.117819	47.481460
2309.407399	31612.382032	47.486465
2305.722025	31356.853995	47.491469
2302.204269	31095.554442	47.496474
2298.725178	30830.905784	47.501479
2295.274402	30566.224385	47.506484
2291.960753	30308.065334	47.511489
2288.546057	30053.132106	47.516493
2285.383429	29787.699451	47.521498
2281.672361	29525.347254	47.526503
2278.138782	29243.527827	47.531508
2274.160137	28985.736523	47.536513
2270.708663	28734.583340	47.541517
2267.399352	28450.306254	47.546522
2264.045519	28202.186101	47.551527
2260.553187	27925.365527	47.556532
2256.942398	27667.520600	47.561537
2253.587884	27402.864886	47.566541
2250.042898	27140.498253	47.571546
2246.145960	26864.598162	47.576551
2242.987562	26598.116320	47.581556
2239.604315	26333.187551	47.586561
2236.202321	26065.908077	47.591565
2232.767313	25805.702184	47.596570
2229.077914	25525.390530	47.601575
2225.681521	25253.343487	47.606580
2221.886909	24985.670876	47.611585
2218.451829	24705.248479	47.616589
2215.020874	24442.753300	47.621594
2211.377693	24170.537770	47.626599
2208.455679	23896.192045	47.631604
2204.853244	23632.182090	47.636609
2201.625875	23347.735800	47.641613
2197.985945	23068.635465	47.646618
2194.366286	22804.708845	47.651623
2190.893288	22517.690031	47.656628
2187.354007	22236.558365	47.661633
2184.125718	21960.595734	47.666637
2181.172070	21678.233720	47.671642
2177.735038	21401.373974	47.676647
2174.277555	21096.927205	47.681652
2170.607052	20810.489821	47.686657
2167.219116	20521.769964	47.691661
2163.411042	20231.118392	47.696666
2160.030258	19938.757335	47.701671
2156.925080	19649.302946	47.706676
2153.264753	19368.332470	47.711681
2150.007763	19057.095709	47.716685
2146.161653	18765.889099	47.721690
2142.859360	18474.291393	47.726695
2139.509743	18158.497730	47.731700
2136.128512	17863.501284	47.736705
2132.445653	17563.236299	47.741709
2129.173886	17267.478091	47.746714
2125.799542	16952.980945	47.751719
2122.318312	16645.738252	47.756724
2118.521370	16351.026229	47.761729
2115.158260	16036.127439	47.766733
2111.676375	15738.379948	47.771738
2108.073633	15435.918978	47.776743
2104.842017	15121.429405	47.781748
2101.392670	14818.001098	47.786753
2097.697939	14505.433750	47.791757
2094.227066	14196.692973	47.796762
2090.822400	13892.813267	47.801767
2087.385551	13577.896787	47.806772
2083.295016	13275.356389	47.811777
2080.109613	12955.186843	47.816781
2077.000012	12653.645814	47.821786
2073.198517	12340.253787	47.826791
2069.939833	12021.149926	47.831796
2066.359602	11716.841856	47.836801
2062.802625	11400.004925	47.841805
2059.196577	11101.586517	47.846810
2055.321353	10790.520621	47.851815
2051.515154	10492.136890	47.856820
2047.510397	10193.089391	47.861825
2043.587131	9896.547348	47.866829
2040.262657	9606.291581	47.871834
2036.325209	9332.757883	47.876839
2032.687664	9037.976419	47.881844
2028.710444	8756.635776	47.886849
2025.346840	8480.486236	47.891853
2021.496034	8209.111082	47.896858
2017.879210	7944.584413	47.901863
2014.279469	7667.717965	47.906868
2010.710016	7411.971612	47.911873
2006.954838	7141.666974	47.916877
2003.777192	6884.369564	47.921882
1999.770665	6625.910979	47.926887
1996.284260	6367.273368	47.931892
1992.586447	6104.684740	47.936897
1989.164572	5853.456411	47.941901
1985.486604	5597.859889	47.946906
1981.650184	5365.179161	47.951911
1978.149292	5121.397749	47.956916
1973.674371	4907.136926	47.961921
1969.772997	4683.785512	47.966925
1965.750492	4451.693050	47.971930
1961.672878	4242.789335	47.976935
1958.074209	4036.063052	47.981940
1954.163020	3851.159660	47.986945
1950.741257	3651.761176	47.991949
1947.078033	3464.364159	47.996954
1943.220915	3281.904221	48.001959
1939.492281	3085.939560	48.006964
1935.697612	2911.583826	48.011969
1932.186757	2728.784184	48.016973
1928.654728	2550.289934	48.021978
1924.750569	2380.206077	48.026983
1921.609283	2209.782961	48.031988
1918.292114	2056.424863	48.036993
1914.875667	1876.223228	48.041997
1911.255826	1710.461411	48.047002
1907.749200	1546.933072	48.052007
1903.753376	1371.472046	48.057012
1899.982722	1211.987445	48.062017
1896.912475	1042.481879	48.067021
1893.360500	886.452683	48.072026
1889.629115	747.243941	48.077031
1886.595728	584.979208	48.082036
1883.104237	427.580919	48.087041
1879.112930	259.223553	48.092045
1875.337786	125.667673	48.097050
1870.732043	10.621329	48.102055
1860.730560	37.667961	48.107060
1853.368568	57.635425	48.112065
1848.395205	64.039159	48.117069
1845.877550	58.950442	48.122074
1843.188865	73.440879	48.127079
1840.909096	56.131077	48.132084
1837.846976	67.209244	48.137089
1835.045592	63.667742	48.142093
1831.991468	66.290943	48.147098
1828.500941	66.587429	48.152103
1825.602974	71.793179	48.157108
1821.879008	64.083776	48.162113
1818.383719	62.963621	48.167117
1815.524175	60.086138	48.172122
1811.357289	70.786696	48.177127
1808.555559	63.866301	48.182132
1804.719959	65.466503	48.187137
1801.231703	62.545042	48.192141
1797.683892	68.757346	48.197146
1794.133490	69.433380	48.202151
1790.832452	64.293263	48.207156
1787.546531	64.127463	48.212161
1784.223860	59.117288	48.217165
1780.902033	59.890435	48.222170
1777.456643	63.460750	48.227175
1774.203959	60.075318	48.232180
1770.414904	66.461427	48.237185
1766.953278	72.508391	48.242189
1763.796160	55.554224	48.247194
1759.848859	68.957131	48.252199
1756.473249	59.753705	48.257204
1752.972172	66.721187	48.262209
1749.513464	65.766176	48.267213
1746.451155	64.676363	48.272218
1742.386312	73.313986	48.277223
1739.470665	64.222081	48.282228
1736.085272	69.599049	48.287233
1732.440437	66.645168	48.292237
1728.705520	68.932007	48.297242
1725.095171	72.218101	48.302247
1721.973277	70.115708	48.307252
1718.403364	68.146708	48.312257
1714.765937	66.147146	48.317261
1711.357245	64.750878	48.322266
1708.143298	72.562470	48.327271
1704.465607	63.928368	48.332276
1700.975813	61.738025	48.337281
1697.566894	61.673763	48.342285
1694.439729	64.858935	48.347290
1690.599412	63.976323	48.352295
1687.054086	65.005946	48.357300
1683.445438	69.335845	48.362305
1679.953079	70.803278	48.367309
1676.492633	58.806859	48.372314
1672.975590	66.985438	48.377319
1669.568493	51.614382	48.382324
1666.301298	65.825211	48.387329
1662.893963	61.540188	48.392333
1659.206703	54.989396	48.397338
1655.405925	65.964901	48.402343
1652.413641	55.312613	48.407348
1648.814069	61.729215	48.412353
1645.157190	61.175422	48.417357
1642.138087	54.643453	48.422362
1638.491384	65.585357	48.427367
1634.896584	53.401177	48.432372
1631.339538	64.575827	48.437377
1627.344195	62.480453	48.442381
1624.392939	58.481574	48.447386
1620.803833	61.375227	48.452391
1617.599530	60.000788	48.457396
1613.825662	61.521793	48.462401
1610.422552	58.270694	48.467405
1606.609533	66.030535	48.472410
1603.070694	58.197339	48.477415
1600.003922	59.436833	48.482420
1596.528443	60.205613	48.487425
1593.192257	61.797329	48.492429
1589.834804	57.529838	48.497434
1585.636846	59.980949	48.502439
1582.010882	54.338100	48.507444
1578.983235	49.379906	48.512449
1575.238622	67.806901	48.517453
1572.342312	54.089710	48.522458
1568.480175	58.415025	48.527463
1565.084805	63.227279	48.532468
1561.662024	57.163488	48.537473
1557.934589	60.898239	48.542477
1554.565207	53.038542	48.547482
1550.900240	57.203286	48.552487
1547.236155	57.564997	48.557492
1543.892675	56.686937	48.562497
1540.349817	57.697240	48.567501
1537.232515	59.223076	48.572506
1533.386467	62.090534	48.577511
1530.055306	68.613862	48.582516
1526.684162	64.737683	48.587521
1522.908088	61.367819	48.592525
1519.516200	57.219640	48.597530
1515.662587	52.491989	48.602535
1512.226895	59.572691	48.607540
1508.930452	53.166439	48.612545
1505.218321	48.932349	48.617549
1502.316359	48.016834	48.622554
1498.171515	60.254807	48.627559
1494.992393	49.037032	48.632564
1491.446987	64.579110	48.637569
1487.741487	61.119119	48.642573
1484.436407	64.098076	48.647578
1480.826628	62.894718	48.652583
1477.702262	57.806159	48.657588
1474.164291	60.793098	48.662593
1470.521205	64.672866	48.667597
1467.086383	55.475665	48.672602
1463.385292	61.367203	48.677607
1460.075017	57.759938	48.682612
1456.806872	60.005446	48.687617
1453.000961	63.429808	48.692621
1449.555395	61.150374	48.697626
1446.055322	71.936501	48.702631
1442.796424	63.047133	48.707636
1439.125207	54.611458	48.712641
1435.364844	58.879759	48.717645
1431.833836	53.260075	48.722650
1428.191502	62.730180	48.727655
1424.463044	63.718954	48.732660
1421.549760	56.094806	48.737665
1418.282022	60.890288	48.742669
1414.893355	62.768691	48.747674
1410.919281	68.313830	48.752679
1407.607725	61.138011	48.757684
1404.129889	57.401969	48.762689
1400.469675	58.601535	48.767693
1396.998893	57.433399	48.772698
1393.396613	56.355452	48.777703
1390.085480	58.838668	48.782708
1386.566098	64.803029	48.787713
1382.728068	60.180563	48.792717
1379.602591	58.078844	48.797722
1375.810523	59.979276	48.802727
1372.964742	53.230445	48.807732
1368.957846	58.100516	48.812737
1365.391976	64.755542	48.817741
1362.195595	56.188624	48.822746
1358.449722	62.783242	48.827751
1354.766760	56.579924	48.832756
1351.187396	53.078098	48.837761
1347.674426	60.503142	48.842765
1344.509782	53.446725	48.847770
1340.802946	58.288819	48.852775
1337.895159	54.545826	48.857780
1334.477082	59.029503	48.862785
1330.294825	62.769089	48.867789
1326.848650	58.828800	48.872794
1323.162908	58.868111	48.877799
1319.918962	63.694700	48.882804
1316.706730	57.085510	48.887809
1313.005465	59.123613	48.892813
1309.557471	61.988952	48.897818
1306.255698	56.191062	48.902823
1302.672213	65.193241	48.907828
1298.959570	61.946418	48.912833
1295.051798	55.607473	48.917837
1291.973748	55.539011	48.922842
1288.407347	45.562048	48.927847
1284.719745	58.895949	48.932852
1281.556750	53.481311	48.937857
1278.163883	55.221208	48.942861
1274.512486	48.389718	48.947866
1270.970337	53.199725	48.952871
1267.536456	47.387732	48.957876
1263.987892	53.157376	48.962881
1260.192141	52.793147	48.967885
1257.117531	49.898885	48.972890
1253.394072	50.890103	48.977895
1250.170949	50.391941	48.982900
1246.598115	59.041284	48.987905
1242.878009	56.725811	48.992909
1239.656797	57.489710	48.997914
1236.049165	62.607378	49.002919
1232.185791	52.401678	49.007924
1228.908439	52.522625	49.012929
1225.036433	63.737195	49.017933
1221.820092	56.176382	49.022938
1218.651487	64.759290	49.027943
1215.190241	65.699981	49.032948
1211.433472	61.333790	49.037953
1208.052553	54.001231	49.042957
1204.541912	58.569043	49.047962
1200.839422	60.563086	49.052967
1197.383390	55.991631	49.057972
1193.662988	60.788441	49.062977
1190.335406	61.024835	49.067981
1187.388735	61.033915	49.072986
1183.095475	61.051328	49.077991
1179.676148	50.212980	49.082996
1176.011098	57.731486	49.088001
1172.799754	60.711683	49.093005
1169.165134	52.555143	49.098010
1165.691324	64.719806	49.103015
1162.292244	54.150380	49.108020
1158.860854	55.165512	49.113025
1155.317409	59.162664	49.118029
1152.186649	54.147993	49.123034
1148.352173	63.594476	49.128039
1144.579845	58.205680	49.133044
1141.169988	54.329382	49.138049
1138.054193	55.244490	49.143053
1134.682596	49.378505	49.148058
1130.932062	59.659747	49.153063
1127.103187	65.603039	49.158068
1123.907081	54.315309	49.163073
1120.305792	55.524734	49.168077
1117.133675	51.335975	49.173082
1113.344660	55.833502	49.178087
1109.755767	49.470030	49.183092
1106.399382	56.873792	49.188097
1102.465509	65.067171	49.193101
1099.479484	58.593494	49.198106
1095.799849	60.969980	49.203111
1092.523357	58.936294	49.208116
1088.726798	55.234456	49.213121
1085.339462	67.341309	49.218125
1081.712042	62.980232	49.223130
1078.042771	59.948176	49.228135
1075.044863	58.943407	49.233140
1071.224170	61.392607	49.238145
1067.369488	59.398835	49.243149
1064.608289	56.506189	49.248154
1060.826626	66.798657	49.253159
1057.163877	57.080490	49.258164
1053.801152	52.529286	49.263169
1050.389081	60.400535	49.268173
1047.070786	48.834576	49.273178
1043.289618	51.008675	49.278183
1040.061105	55.741177	49.283188
1036.480893	53.568402	49.288193
1032.921822	59.333439	49.293197
1028.953822	55.237684	49.298202
1025.525748	54.050343	49.303207
1022.220994	53.773850	49.308212
1018.930779	50.002256	49.313217
1015.508361	50.361127	49.318221
1012.108608	55.591854	49.323226
1008.332901	58.489620	49.328231
1004.457405	51.253568	49.333236
1001.140602	46.391472	49.338241
997.585850	46.467346	49.343245
994.171280	50.406407	49.348250
990.643145	58.798887	49.353255
987.441991	42.415146	49.358260
983.940194	54.059042	49.363265
980.239451	55.287254	49.368269
976.612132	55.725679	49.373274
972.829907	52.239949	49.378279
969.731596	53.927502	49.383284
966.192022	54.089597	49.388289
962.544456	54.075611	49.393293
959.209427	45.578027	49.398298
955.814270	61.609232	49.403303
952.302792	45.773974	49.408308
948.843421	46.284190	49.413313
945.162384	59.006542	49.418317
941.959500	44.916840	49.423322
937.978850	63.162628	49.428327
934.604467	45.252613	49.433332
931.480853	52.945847	49.438337
927.287507	58.886164	49.443341
924.305372	46.701307	49.448346
920.855618	50.070091	49.453351
917.290610	48.837793	49.458356
913.716138	44.215397	49.463361
910.064174	48.390976	49.468365
906.725345	46.613896	49.473370
903.284497	56.068421	49.478375
899.668850	54.011982	49.483380
896.424768	53.400162	49.488385
892.383178	63.233502	49.493389
889.171098	57.108516	49.498394
885.607806	65.199648	49.503399
882.281376	61.430610	49.508404
878.703550	59.127808	49.513409
874.893666	59.775195	49.518413
871.553580	53.894890	49.523418
867.777716	64.869887	49.528423
864.431813	59.635907	49.533428
861.417867	55.953990	49.538433
857.620708	61.999977	49.543437
854.316046	57.458742	49.548442
850.871472	57.574366	49.553447
847.188688	59.188963	49.558452
843.443645	53.862469	49.563457
840.063051	57.543159	49.568461
836.278598	52.346228	49.573466
833.018117	64.974286	49.578471
829.736322	59.502488	49.583476
826.051244	60.427747	49.588481
822.337546	63.939140	49.593485
819.459899	55.075757	49.598490
815.741225	58.856852	49.603495
812.039775	55.070638	49.608500
808.630502	58.483743	49.613505
804.802444	61.427749	49.618509
801.917517	56.406350	49.623514
798.167086	62.657016	49.628519
794.551482	51.729355	49.633524
790.966729	52.990097	49.638529
787.285426	55.961748	49.643533
783.782229	47.053972	49.648538
780.516587	64.779708	49.653543
777.196568	58.519807	49.658548
774.127042	52.556044	49.663553
770.014089	68.060616	49.668557
766.582188	63.362167	49.673562
763.095906	45.488746	49.678567
759.234062	64.241166	49.683572
755.618767	56.670251	49.688577
752.539405	67.150230	49.693581
749.118743	54.363393	49.698586
745.596903	68.101763	49.703591
741.852067	54.887963	49.708596
738.926399	58.101971	49.713601
735.043178	63.171215	49.718605
731.651212	53.954971	49.723610
727.712835	62.244097	49.728615
724.110553	62.109216	49.733620
720.926153	62.418265	49.738625
717.458995	60.041249	49.743629
714.205114	53.353399	49.748634
710.216503	51.545272	49.753639
706.660253	53.529252	49.758644
703.160321	48.205567	49.763649
699.786370	58.348871	49.768653
697.058788	47.731448	49.773658
693.404295	52.223879	49.778663
689.476656	55.610635	49.783668
686.191982	43.720037	49.788673
681.996818	50.878789	49.793677
679.176098	59.318767	49.798682
675.422523	49.225866	49.803687
672.255618	58.321178	49.808692
668.451875	51.830194	49.813697
664.385708	51.749003	49.818701
661.385554	50.124621	49.823706
657.702332	56.459721	49.828711
654.482041	51.756656	49.833716
650.680223	49.409933	49.838721
647.237324	51.784310	49.843725
643.993242	54.478732	49.848730
640.425869	53.449395	49.853735
637.320283	53.062752	49.858740
633.601337	42.075430	49.863745
629.979725	52.485330	49.868749
626.296586	47.731377	49.873754
622.694416	44.945272	49.878759
619.460993	47.365946	49.883764
616.163000	50.600335	49.888769
612.843392	63.126973	49.893773
608.750822	49.569071	49.898778
605.446639	56.053636	49.903783
601.410616	58.119123	49.908788
598.368218	52.787100	49.913793
594.286232	53.983421	49.918797
591.275477	51.943104	49.923802
587.321195	49.237470	49.928807
584.482941	48.413504	49.933812
581.159295	45.064935	49.938817
577.335796	50.925319	49.943821
574.437089	42.887919	49.948826
570.425305	48.129219	49.953831
566.615891	50.355383	49.958836
563.456270	50.872578	49.963841
559.672997	48.902644	49.968845
556.607529	44.441128	49.973850
553.072408	53.084772	49.978855
549.483820	56.772825	49.983860
545.735241	57.455037	49.988865
541.951729	54.906176	49.993869
538.500577	49.922937	49.998874
534.869125	52.405981	50.003879
531.751271	56.975774	50.008884
528.401269	64.571700	50.013889
524.809394	67.956556	50.018893
521.403297	55.727537	50.023898
517.776508	50.363688	50.028903
514.127796	51.071400	50.033908
510.951925	56.877832	50.038913
507.461270	66.061865	50.043917
503.909006	64.198142	50.048922
500.427989	58.226167	50.053927
496.617034	58.430947	50.058932
493.768210	55.463624	50.063937
489.694378	56.652387	50.068941
485.964729	50.130902	50.073946
482.525509	54.216366	50.078951
479.387428	52.626304	50.083956
475.693921	53.015179	50.088961
471.999734	56.624887	50.093965
468.904810	53.028563	50.098970
464.746771	52.243675	50.103975
461.717301	49.738096	50.108980
458.795123	53.653997	50.113985
454.836108	56.580687	50.118989
451.440345	51.468585	50.123994
447.843807	61.336777	50.128999
443.918275	53.276758	50.134004
440.560908	58.722496	50.139009
436.771094	52.504688	50.144013
433.442290	54.022871	50.149018
430.146636	51.356515	50.154023
426.516722	54.680924	50.159028
423.548204	49.830946	50.164033
419.824151	57.400071	50.169037
416.292399	60.671144	50.174042
412.765907	50.963586	50.179047
409.124092	56.763938	50.184052
405.780192	57.537845	50.189057
401.904561	57.664210	50.194061
398.772066	55.608228	50.199066
394.971834	57.171795	50.204071
391.461080	56.775936	50.209076
388.041060	53.255875	50.214081
384.240087	54.556969	50.219085
381.260303	54.985946	50.224090
377.816713	58.059724	50.229095
374.228396	54.126267	50.234100
370.828098	50.922666	50.239105
367.031674	62.290184	50.244109
363.933763	55.432515	50.249114
360.205283	55.134049	50.254119
356.416332	54.541335	50.259124
353.089155	55.913759	50.264129
349.648501	54.946947	50.269133
346.249965	53.790042	50.274138
342.405156	54.835426	50.279143
338.890980	49.792542	50.284148
335.817285	46.161307	50.289153
332.310804	54.794209	50.294157
328.679924	52.844797	50.299162
325.208398	57.229608	50.304167
321.434979	54.445145	50.309172
318.351756	49.752380	50.314177
314.568625	49.867458	50.319181
311.041916	48.066252	50.324186
307.564949	45.874440	50.329191
303.814544	50.657285	50.334196
300.639890	40.043619	50.339201
297.013021	47.578577	50.344205
293.670941	40.294117	50.349210
290.148308	46.999660	50.354215
286.617434	38.042671	50.359220
283.283417	40.365321	50.364225
279.223331	57.918210	50.369229
275.957044	48.078210	50.374234
272.340810	47.287632	50.379239
268.829604	51.685005	50.384244
265.626379	48.137363	50.389249
262.077644	47.380509	50.394253
258.590412	50.654155	50.399258
255.147006	44.692222	50.404263
251.616057	47.023588	50.409268
248.667546	46.517562	50.414273
244.303785	56.613574	50.419277
240.620535	41.311806	50.424282
237.397656	44.215015	50.429287
233.805765	47.546195	50.434292
230.612446	34.996097	50.439297
226.590024	47.974613	50.444301
223.674065	48.270258	50.449306
220.205177	47.602153	50.454311
216.597122	56.785682	50.459316
213.093394	53.788175	50.464321
209.075468	59.989208	50.469325
205.621633	47.359702	50.474330
202.555072	51.216040	50.479335
199.124257	59.435334	50.484340
195.601754	54.393817	50.489345
191.664704	53.726299	50.494349
188.438958	47.398099	50.499354
185.086223	50.245740	50.504359
181.161916	56.546013	50.509364
177.982867	45.752752	50.514369
174.150240	58.612975	50.519373
171.180366	47.448423	50.524378
167.403394	53.323820	50.529383
164.123929	46.649705	50.534388
160.601585	41.892921	50.539393
156.603013	57.737268	50.544397
153.298122	50.893132	50.549402
150.105270	48.609417	50.554407
146.522042	57.339825	50.559412
142.951918	50.312620	50.564417
139.371102	55.337881	50.569421
135.928190	46.731013	50.574426
132.211273	52.929209	50.579431
128.689329	55.604064	50.584436
125.754313	46.382952	50.589441
121.956531	55.846174	50.594445
118.186074	49.065503	50.599450
114.664579	54.780672	50.604455
111.258134	54.488807	50.609460
108.137290	43.882614	50.614465
104.925721	58.999400	50.619469
101.063866	54.694465	50.624474
97.373951	50.327794	50.629479
93.610072	54.328219	50.634484
90.524232	53.793143	50.639489
86.936644	51.697847	50.644493
83.346069	44.746643	50.649498
79.623890	40.454641	50.654503
75.954623	52.327513	50.659508
72.903590	44.836198	50.664513
69.193776	55.320208	50.669517
65.941021	55.867989	50.674522
62.682280	58.612364	50.679527
58.646931	60.428045	50.684532
55.075693	58.811093	50.689537
51.775309	62.042889	50.694541
48.462112	47.822200	50.699546
45.008430	47.389066	50.704551
41.135783	57.778375	50.709556
37.861638	54.336847	50.714561
34.005680	58.057493	50.719565
30.620747	50.833646	50.724570
27.515859	62.437778	50.729575
23.720763	53.335645	50.734580
20.310053	59.134731	50.739585
16.958116	60.507995	50.744589
13.473442	56.137678	50.749594
10.183133	52.860047	50.754599
6.228667	59.620697	50.759604
3.189438	54.962292	50.764609