Thu Aug 25 09:37:55 2022

Number of Points = 9926

Depth (nm)	Load (N)	Time (s)
1.557851	99.953416	0.000000
1.323624	97.867399	0.005005
1.385798	92.767322	0.010010
1.163751	92.514384	0.015014
0.866518	95.563551	0.020019
1.204806	87.015994	0.025024
0.764736	84.816697	0.030029
0.726593	72.518947	0.035034
0.158066	63.366834	0.040038
0.176029	53.078790	0.045043
-0.384828	51.132541	0.050048
-0.738904	46.565933	0.055053
-0.799639	31.361089	0.060058
-0.513126	29.955955	0.065062
-1.326861	24.717890	0.070067
-1.197966	16.497405	0.075072
-2.214718	8.725346	0.080077
-2.032111	-3.220961	0.085082
-1.979754	-7.367181	0.090086
-2.967343	-4.966001	0.095091
-3.190982	-11.043160	0.100096
-3.812796	-5.057810	0.105101
-3.597929	-12.823516	0.110106
-3.694450	-5.835303	0.115110
-3.986286	-6.697400	0.120115
-4.262204	-11.266747	0.125120
-4.971599	-8.311207	0.130125
-5.249237	-14.161604	0.135130
-5.345721	-2.952949	0.140134
-5.391652	-4.824848	0.145139
-5.744341	-8.926586	0.150144
-6.252132	-13.484911	0.155149
-6.386108	-9.948814	0.160154
-6.423448	-5.171846	0.165158
-6.555855	-11.212679	0.170163
-6.616842	-11.740786	0.175168
-7.432544	-9.344392	0.180173
-7.778678	-10.232783	0.185178
-7.881051	-6.135324	0.190182
-8.136224	-3.235133	0.195187
-7.821409	-9.738344	0.200192
-8.199487	-6.635398	0.205197
-9.069504	0.277858	0.210202
-9.426083	-8.910589	0.215206
-9.973674	-9.637700	0.220211
-9.369114	-6.739338	0.225216
-9.857052	1.183402	0.230221
-9.917355	0.148986	0.235226
-9.603842	-13.203549	0.240230
-10.317789	-3.894477	0.245235
-10.900469	-7.646967	0.250240
-10.876676	-2.332248	0.255245
-11.164134	-4.197941	0.260250
-11.278936	-8.087015	0.265254
-11.924606	-4.575147	0.270259
-12.010232	-9.708984	0.275264
-12.420132	-8.426539	0.280269
-12.400285	1.561665	0.285274
-12.067101	-8.203092	0.290278
-13.505372	-16.326708	0.295283
-13.586486	-13.950500	0.300288
-14.002359	-15.957423	0.305293
-13.938100	-14.287363	0.310298
-13.903129	-9.645114	0.315302
-14.229734	3.459889	0.320307
-14.246162	-11.685421	0.325312
-14.649882	-8.154515	0.330317
-15.632128	-4.504488	0.335322
-15.559031	-7.632065	0.340326
-15.715128	2.804487	0.345331
-16.008954	-7.564382	0.350336
-16.208777	-5.852944	0.355341
-16.106631	-9.972163	0.360346
-16.068208	-8.797928	0.365350
-16.629693	4.989283	0.370355
-16.536921	-17.949642	0.375360
-17.008154	-7.764277	0.380365
-17.483945	-5.848247	0.385370
-18.225039	-15.824328	0.390374
-18.166165	-4.889954	0.395379
-18.412770	-5.145369	0.400384
-18.513681	-5.034470	0.405389
-18.312247	-9.150263	0.410394
-18.586390	-8.426926	0.415398
-19.319922	-15.487211	0.420403
-19.212218	-12.691335	0.425408
-19.475095	-8.306137	0.430413
-20.163696	-5.610118	0.435418
-20.386112	-12.804271	0.440422
-20.976338	3.749399	0.445427
-20.576367	-2.007855	0.450432
-21.164766	-4.136443	0.455437
-21.095163	4.660722	0.460442
-21.450707	-13.854634	0.465446
-22.340123	-4.518069	0.470451
-22.443384	-5.286325	0.475456
-22.792689	0.007759	0.480461
-22.859781	-1.826023	0.485466
-22.794165	-8.027596	0.490470
-22.942186	-0.635844	0.495475
-22.627207	-8.588080	0.500480
-23.327756	-14.818301	0.505485
-24.207160	-19.264613	0.510490
-23.974612	-4.687499	0.515494
-23.969930	-4.732350	0.520499
-23.932722	-7.572729	0.525504
-25.072359	-9.769968	0.530509
-25.312518	-10.877442	0.535514
-25.449173	-5.176917	0.540518
-25.789015	-2.912029	0.545523
-25.717733	-11.860628	0.550528
-25.863479	-12.451385	0.555533
-26.193793	-6.486399	0.560538
-26.740687	-14.737023	0.565542
-27.260628	-8.840403	0.570547
-26.745184	-7.927571	0.575552
-27.028300	-11.989588	0.580557
-27.105850	-16.302112	0.585562
-27.965028	-9.858793	0.590566
-28.334542	-3.197965	0.595571
-28.319201	0.770319	0.600576
-28.783463	-6.578931	0.605581
-28.763967	0.027272	0.610586
-28.545839	-10.020012	0.615590
-29.354091	-1.730710	0.620595
-29.928931	-6.237401	0.625600
-30.284895	-1.122607	0.630605
-30.307456	-2.495131	0.635610
-29.674643	-10.076387	0.640614
-30.434727	-3.230976	0.645619
-31.157104	-8.037252	0.650624
-31.533695	-6.101965	0.655629
-31.422161	-6.470442	0.660634
-31.667478	-14.420306	0.665638
-31.926478	-6.593552	0.670643
-31.746020	-19.017236	0.675648
-32.087004	-9.295206	0.680653
-32.374491	-10.395264	0.685658
-32.489551	-15.030941	0.690662
-33.362814	-2.052262	0.695667
-33.285346	-10.283658	0.700672
-33.473806	-9.368102	0.705677
-33.979089	-12.572732	0.710682
-34.266189	-10.148430	0.715686
-34.957427	-7.439342	0.720691
-35.142458	-7.365882	0.725696
-35.245938	-1.028312	0.730701
-35.196461	-3.079675	0.735706
-34.754053	-9.621860	0.740710
-35.248351	-3.662816	0.745715
-35.608619	-0.654409	0.750720
-35.903454	-8.729394	0.755725
-36.546202	-1.883385	0.760730
-36.548261	-8.839982	0.765734
-36.621838	-2.200214	0.770739
-36.607510	-9.086613	0.775744
-37.267929	-13.045217	0.780749
-37.800843	-0.037607	0.785754
-37.871841	-12.937587	0.790758
-38.339957	-5.233091	0.795763
-38.199197	-12.113989	0.800768
-38.808629	-4.912533	0.805773
-39.239488	-12.042387	0.810778
-39.270645	-12.964310	0.815782
-39.206269	-6.393615	0.820787
-39.007475	-17.292079	0.825792
-39.189602	-6.921059	0.830797
-40.414940	-10.550703	0.835802
-40.413299	-8.592422	0.840806
-41.190101	-13.950152	0.845811
-40.725390	-7.166938	0.850816
-40.640837	-5.961966	0.855821
-41.537678	-12.082335	0.860826
-41.684073	-16.931400	0.865830
-42.237769	-9.343211	0.870835
-42.214132	-10.593258	0.875840
-42.163312	-12.758725	0.880845
-42.676671	-14.361229	0.885850
-42.212018	-14.554082	0.890854
-43.175648	-4.497207	0.895859
-43.399304	-19.676475	0.900864
-43.696786	-7.192977	0.905869
-44.020555	-5.670926	0.910874
-43.885144	-4.439121	0.915878
-44.538843	-8.050766	0.920883
-45.076902	-4.460845	0.925888
-45.302871	-13.935505	0.930893
-45.487176	-5.206131	0.935898
-44.842346	-5.151969	0.940902
-45.609355	-8.163729	0.945907
-45.544271	-13.529985	0.950912
-45.765226	-14.786000	0.955917
-46.487178	-14.963769	0.960922
-46.347632	-15.349290	0.965926
-46.790504	-5.718861	0.970931
-46.704504	-20.722020	0.975936
-47.384721	-9.485183	0.980941
-47.942797	-7.271522	0.985946
-47.811891	-7.339315	0.990950
-48.227351	-10.453614	0.995955
-47.799088	-7.008777	1.000960
-48.344981	-11.557965	1.005965
-49.239487	-4.890808	1.010970
-49.252742	-12.421452	1.015974
-49.748494	-5.842086	1.020979
-49.782000	-12.366647	1.025984
-49.873507	-10.425409	1.030989
-49.697760	-5.732452	1.035994
-50.078558	-15.056300	1.040998
-51.007019	-0.778161	1.046003
-51.039175	-5.923539	1.051008
-51.090220	-11.281090	1.056013
-51.275049	-9.866231	1.061018
-51.048731	-4.788892	1.066022
-52.085231	-13.108331	1.071027
-52.427130	-14.364377	1.076032
-52.501646	-12.919347	1.081037
-52.548464	-15.569388	1.086042
-52.567345	-13.133329	1.091046
-53.169077	-4.284765	1.096051
-53.525260	-21.828733	1.101056
-53.865044	-12.929469	1.106061
-54.125427	-13.438987	1.111066
-53.878821	-25.980596	1.116070
-54.331396	-7.426871	1.121075
-54.293196	-4.319548	1.126080
-54.938418	-7.644619	1.131085
-55.413590	-3.776649	1.136090
-55.352029	-16.270288	1.141094
-55.716362	-5.699877	1.146099
-55.674243	-14.295889	1.151104
-56.047786	-10.633671	1.156109
-56.807026	-8.704864	1.161114
-56.818142	-18.795316	1.166118
-57.498719	-9.773049	1.171123
-57.293188	-17.227241	1.176128
-57.239620	-18.671802	1.181133
-57.598180	-11.272377	1.186138
-57.192818	-19.589946	1.191142
-57.858380	-12.262639	1.196147
-58.156531	-10.203601	1.201152
-58.721944	-10.209744	1.206157
-58.616904	-9.213626	1.211162
-59.018637	-7.970424	1.216166
-59.898702	-2.400188	1.221171
-59.731274	-7.057982	1.226176
-60.547903	-10.302410	1.231181
-60.195135	-7.026078	1.236186
-60.111119	-3.261546	1.241190
-60.405989	-9.042801	1.246195
-60.527084	-11.019980	1.251200
-61.132208	-4.565844	1.256205
-61.831797	-6.211934	1.261210
-61.875122	-8.976418	1.266214
-61.869444	-7.578754	1.271219
-61.981031	-20.197118	1.276224
-62.121435	-14.461209	1.281229
-63.121966	0.052850	1.286234
-62.812506	-15.232098	1.291238
-63.081955	-10.035951	1.296243
-63.330342	-15.194900	1.301248
-63.255114	-8.451902	1.306253
-64.252824	-7.295650	1.311258
-64.280652	-14.007760	1.316262
-64.880230	-5.744829	1.321267
-64.583980	-16.509865	1.326272
-64.611276	-3.037319	1.331277
-64.889542	2.628449	1.336282
-65.363547	1.206440	1.341286
-65.454434	-9.668783	1.346291
-65.663100	-3.906356	1.351296
-65.661240	-4.532895	1.356301
-66.287594	1.057700	1.361306
-66.872318	-2.131317	1.366310
-67.136140	4.699613	1.371315
-67.316636	-7.670681	1.376320
-67.203318	1.657466	1.381325
-67.646920	8.121098	1.386330
-68.412921	1.771420	1.391334
-68.928251	4.677575	1.396339
-68.314026	5.049743	1.401344
-68.800617	-7.240952	1.406349
-68.842769	-0.542833	1.411354
-68.620343	-2.747845	1.416358
-68.821734	-0.368609	1.421363
-69.711886	4.431255	1.426368
-70.042531	-4.245558	1.431373
-70.421154	-0.455991	1.436378
-70.293924	-2.858058	1.441382
-70.588855	-5.697013	1.446387
-70.667143	-8.497147	1.451392
-71.418418	-6.288014	1.456397
-71.610006	5.036783	1.461402
-71.502176	-13.298069	1.466406
-72.112407	-4.932228	1.471411
-72.414648	-6.238781	1.476416
-72.323252	-13.380860	1.481421
-73.026623	-3.089518	1.486426
-73.126240	2.646334	1.491430
-73.550547	1.880927	1.496435
-73.562969	8.140955	1.501440
-73.556197	-4.454836	1.506445
-73.615014	0.164144	1.511450
-73.925816	-3.760656	1.516454
-74.324170	-1.913705	1.521459
-74.500642	-9.871191	1.526464
-75.267575	-4.002305	1.531469
-75.619949	6.116986	1.536474
-75.400978	-5.075710	1.541478
-75.540235	-0.969309	1.546483
-75.527549	-9.298120	1.551488
-76.087994	-3.686216	1.556493
-76.354805	2.066342	1.561498
-76.015627	2.848602	1.566502
-77.388301	1.406056	1.571507
-77.458650	-3.961127	1.576512
-77.528449	-5.705898	1.581517
-77.650973	-6.733726	1.586522
-78.001548	-12.866918	1.591526
-77.961258	-13.306490	1.596531
-78.023714	-5.054954	1.601536
-78.707131	-0.508947	1.606541
-79.275787	-2.279955	1.611546
-79.041205	-14.440036	1.616550
-79.447334	-7.324221	1.621555
-79.489339	-6.067782	1.626560
-80.052990	-8.614693	1.631565
-80.938133	-4.071879	1.636570
-80.837612	-22.820027	1.641574
-81.211447	0.410043	1.646579
-81.228051	-0.846354	1.651584
-81.305213	-2.026823	1.656589
-81.304785	-4.079991	1.661594
-80.970537	-12.126992	1.666598
-81.455624	-1.822396	1.671603
-82.091814	-0.494999	1.676608
-82.239944	-3.312663	1.681613
-82.485930	-1.208013	1.686618
-82.738685	-5.736692	1.691622
-83.391461	3.018633	1.696627
-83.613885	-2.723354	1.701632
-83.658517	-1.789205	1.706637
-84.045804	-5.512194	1.711642
-83.871285	-4.220080	1.716646
-84.752655	-7.403741	1.721651
-85.245731	-4.279611	1.726656
-85.224137	-9.177144	1.731661
-85.269728	-3.320047	1.736666
-84.938980	-8.028741	1.741670
-84.939423	-5.551279	1.746675
-85.975503	-6.192351	1.751680
-86.514260	2.029417	1.756685
-86.735412	1.260651	1.761690
-87.128079	-4.350255	1.766694
-87.015898	-0.498388	1.771699
-87.200917	-9.150559	1.776704
-86.940613	-9.893524	1.781709
-88.085896	-3.063684	1.786714
-88.230934	-9.909289	1.791718
-88.495996	-7.194210	1.796723
-88.598481	-4.934876	1.801728
-88.413577	-1.458236	1.806733
-88.535839	-3.637711	1.811738
-89.280011	-12.063060	1.816742
-89.762566	-11.288083	1.821747
-89.708892	-10.815428	1.826752
-89.839190	-2.717777	1.831757
-89.927599	-4.788662	1.836762
-90.269108	-8.192956	1.841766
-91.015829	-4.209669	1.846771
-91.464446	-10.355972	1.851776
-91.628656	-13.832339	1.856781
-91.717638	-3.811274	1.861786
-91.014254	-5.930297	1.866790
-91.916973	-0.900674	1.871795
-92.044521	0.843733	1.876800
-92.332340	-7.140597	1.881805
-93.198866	-6.457314	1.886810
-92.644613	-4.753303	1.891814
-93.258286	2.901237	1.896819
-92.924437	-7.176833	1.901824
-93.783959	-10.623343	1.906829
-94.705562	-10.719204	1.911834
-94.345905	-8.684145	1.916838
-94.464754	-9.529051	1.921843
-94.540493	-0.025751	1.926848
-94.415628	-7.600183	1.931853
-95.318784	0.909637	1.936858
-95.612715	-3.853035	1.941862
-96.015176	-0.999367	1.946867
-95.907058	-3.838201	1.951872
-96.016956	-10.350790	1.956877
-96.612348	1.106879	1.961882
-96.735708	2.205223	1.966886
-97.345777	0.747590	1.971891
-97.609061	-2.855624	1.976896
-97.544542	-8.626751	1.981901
-97.714159	-8.147582	1.986906
-97.739481	-5.697858	1.991910
-97.967553	-16.633835	1.996915
-98.561440	-11.034548	2.006912
-98.254105	-2.636994	2.016909
-97.890406	-8.126416	2.026906
-97.576556	-8.888000	2.036902
-96.369638	-10.866575	2.046899
-96.371976	-6.022289	2.056896
-95.995733	-0.065235	2.066893
-95.307483	-8.101741	2.076890
-94.889435	-5.388734	2.086886
-94.287809	-10.779221	2.096883
-93.806642	-4.946315	2.106880
-93.084626	-9.161405	2.116877
-92.410509	-1.591098	2.126874
-92.101669	-3.489138	2.136870
-91.996622	-3.483074	2.146867
-91.103196	-2.406281	2.156864
-90.517685	1.249835	2.166861
-90.381885	0.560499	2.176858
-89.738037	-8.666480	2.186854
-89.152525	-7.151799	2.196851
-88.966019	-9.119369	2.206848
-88.377397	-0.712035	2.216845
-87.915101	-11.687703	2.226842
-87.393777	-8.566393	2.236838
-86.559440	-9.818179	2.246835
-86.279518	-9.516401	2.256832
-85.552801	-12.119815	2.266829
-85.276836	-8.842850	2.276826
-85.156792	-7.451638	2.286822
-83.929371	-12.892664	2.296819
-83.576141	-18.665545	2.306816
-83.689166	-11.199983	2.316813
-82.614403	-8.707086	2.326810
-82.074502	-19.289431	2.336806
-81.891414	-8.173441	2.346803
-81.181551	-16.362218	2.356800
-80.831987	-9.849788	2.366797
-80.011206	-6.712042	2.376794
-79.503769	-7.792230	2.386790
-79.137239	0.893827	2.396787
-79.084929	-7.717776	2.406784
-78.241679	-3.088347	2.416781
-78.090812	-5.528671	2.426778
-77.042708	-10.041945	2.436774
-76.325757	-2.500521	2.446771
-76.309931	-5.835181	2.456768
-75.626838	-3.851116	2.466765
-75.237510	-1.849530	2.476762
-74.954817	3.688197	2.486758
-74.182846	0.485311	2.496755
-73.488208	-2.984223	2.506752
-73.396820	-9.378150	2.516749
-72.680115	-7.551406	2.526746
-72.278398	-6.033268	2.536742
-71.762419	-6.750496	2.546739
-70.701315	-5.604940	2.556736
-70.521786	-8.841706	2.566733
-70.777585	-5.953419	2.576730
-69.873835	-3.414717	2.586726
-69.217259	-4.439077	2.596723
-68.343851	-8.893299	2.606720
-67.836584	-2.697013	2.616717
-67.573765	-6.817977	2.626714
-67.648728	-6.511275	2.636710
-67.310838	-6.690582	2.646707
-66.283088	-9.062397	2.656704
-65.466667	-7.827817	2.666701
-65.173081	-5.351898	2.676698
-64.988791	-1.981370	2.686694
-64.075031	-4.148424	2.696691
-63.534615	-5.560063	2.706688
-62.625202	-1.169080	2.716685
-62.744336	-6.867950	2.726682
-62.272660	-8.116763	2.736678
-61.944436	-4.632573	2.746675
-60.997118	-10.489041	2.756672
-60.445415	-3.295524	2.766669
-60.489043	-9.357850	2.776666
-59.541962	-8.495369	2.786662
-59.301096	-10.810411	2.796659
-58.569798	-8.621655	2.806656
-58.107028	-14.389526	2.816653
-57.831598	-12.544323	2.826650
-57.331170	-8.304669	2.836646
-56.340662	-14.101379	2.846643
-56.164888	-5.287231	2.856640
-56.040009	-7.942061	2.866637
-55.239098	-2.254285	2.876634
-54.501453	-2.198454	2.886630
-53.441242	-4.239568	2.896627
-53.654717	-8.244720	2.906624
-53.441946	-4.862816	2.916621
-52.755841	0.928482	2.926618
-51.887073	-0.331865	2.936614
-51.770373	-3.818548	2.946611
-51.351625	-9.627040	2.956608
-50.747355	-9.936783	2.966605
-50.077463	-5.444914	2.976602
-49.150848	-3.093524	2.986598
-49.019431	-10.865382	2.996595
-48.804557	-4.585267	3.006592
-48.410116	-5.182081	3.016589
-47.779095	-1.162458	3.026586
-47.239956	-2.291961	3.036582
-45.872571	-0.263057	3.046579
-46.107547	-0.830941	3.056576
-45.955278	-3.448882	3.066573
-45.323589	-3.328932	3.076570
-44.271868	-6.128987	3.086566
-44.253251	-6.014346	3.096563
-43.818069	-3.823539	3.106560
-43.283700	-2.484574	3.116557
-42.708387	-0.284045	3.126554
-41.396093	-2.782807	3.136550
-41.631377	-2.099358	3.146547
-41.503496	-5.153803	3.156544
-40.847841	-1.353450	3.166541
-40.145167	-1.745135	3.176538
-39.476313	-6.065935	3.186534
-38.462552	-4.025972	3.196531
-38.378247	-7.187630	3.206528
-38.429541	-4.375736	3.216525
-38.198002	-9.480152	3.226522
-37.166044	-6.207597	3.236518
-36.609484	-12.246757	3.246515
-35.844304	-5.650556	3.256512
-35.549812	-7.692066	3.266509
-35.225074	-10.257835	3.276506
-34.303357	-5.494977	3.286502
-33.926283	-6.763811	3.296499
-34.078214	-6.657293	3.306496
-33.008887	-10.591011	3.316493
-32.644693	-6.729152	3.326490
-32.271029	-8.263547	3.336486
-31.683295	-0.749387	3.346483
-31.267530	-8.673506	3.356480
-30.300601	-6.816273	3.366477
-29.744634	-5.825982	3.376474
-29.793567	-3.445279	3.386470
-29.134240	-8.413985	3.396467
-28.368325	-6.024742	3.406464
-28.091196	-0.831432	3.416461
-27.732304	-6.335941	3.426458
-26.814239	-11.180461	3.436454
-26.416380	-11.860171	3.446451
-25.930290	-7.802000	3.456448
-25.816646	-0.847117	3.466445
-25.119967	-1.393084	3.476442
-24.727334	-0.212474	3.486438
-24.065735	-5.824602	3.496435
-23.418641	-5.206550	3.506432
-23.156668	-4.509149	3.516429
-22.144673	2.304977	3.526426
-21.955263	0.029674	3.536422
-21.816688	-4.179528	3.546419
-21.223289	-7.287906	3.556416
-20.434834	-0.261358	3.566413
-20.389857	-6.001784	3.576410
-19.315757	-1.490880	3.586406
-19.186845	-3.138981	3.596403
-18.982992	-5.489406	3.606400
-18.132610	-1.063825	3.616397
-17.468735	-4.734444	3.626394
-16.571819	-7.595772	3.636390
-16.061813	-8.543311	3.646387
-16.016993	-3.006324	3.656384
-16.200600	-4.279174	3.666381
-15.387428	0.000182	3.676378
-14.418301	-1.522975	3.686374
-13.695270	-0.524013	3.696371
-13.252255	-1.825353	3.706368
-13.042515	2.763963	3.716365
-13.117071	6.083186	3.726362
-12.237735	-2.420420	3.736358
-11.499188	-2.127142	3.746355
-10.396152	3.510137	3.756352
-10.380366	-1.671351	3.766349
-10.507790	0.759665	3.776346
-9.603530	-3.613857	3.786342
-9.062895	1.715565	3.796339
-8.568561	1.410379	3.806336
-7.653741	-6.436714	3.816333
-7.347463	-1.656616	3.826330
-7.291331	-0.683042	3.836326
-6.883241	-3.474114	3.846323
-5.869132	-0.506033	3.856320
-5.567462	4.683435	3.866317
-5.060862	3.939169	3.876314
-4.426206	3.548641	3.886310
-4.339519	5.325220	3.896307
-3.930012	11.964489	3.906304
-3.187733	23.344518	3.916301
-2.807366	33.666190	3.926298
-2.347620	45.600520	3.936294
-2.154889	56.499637	3.946291
-1.538633	70.782156	3.956288
-1.053262	85.861310	3.966285
-0.715561	106.497806	3.976282
0.000000	118.553824	3.981286
-0.245923	119.468897	3.986291
0.338324	128.694857	3.991296
0.110807	146.042886	3.996301
0.403983	140.330793	4.001306
0.474048	140.917945	4.006310
0.338439	145.349678	4.011315
0.564807	153.451634	4.016320
0.462847	164.227814	4.021325
1.153834	172.105119	4.026330
1.156434	164.632024	4.031334
0.673091	160.310270	4.036339
1.014042	159.959628	4.041344
0.866958	157.284141	4.046349
0.784091	161.865805	4.051354
0.932177	149.187643	4.056358
0.587295	158.220672	4.061363
0.902652	165.688588	4.066368
0.845786	173.445785	4.071373
0.922204	169.700719	4.076378
1.542264	168.069305	4.081382
0.928290	163.932535	4.086387
0.850699	144.433816	4.091392
0.725357	151.091245	4.096397
0.839679	160.425652	4.101402
1.266192	162.858389	4.106406
1.002408	159.128664	4.111411
1.358449	148.350992	4.116416
0.807966	152.493388	4.121421
0.764857	161.077335	4.126426
1.160100	166.150405	4.131430
1.298420	165.489823	4.136435
0.925682	156.591726	4.141440
0.877914	168.912836	4.146445
1.200951	168.963638	4.151450
1.248905	168.257103	4.156454
1.037570	169.771042	4.161459
1.160665	166.281258	4.166464
1.140126	175.456467	4.171469
1.334872	176.166455	4.176474
1.325559	169.116009	4.181478
0.973177	164.808536	4.186483
1.165899	170.425873	4.191488
1.090254	168.077716	4.196493
0.991286	170.937641	4.201498
1.545436	171.660920	4.206502
1.267933	169.173546	4.211507
1.709489	173.084580	4.216512
1.047803	171.619192	4.221517
1.233397	163.364445	4.226522
1.406929	167.213067	4.231526
1.441517	168.976379	4.236531
1.157815	152.050466	4.241536
1.235872	170.147914	4.246541
1.239547	167.179882	4.251546
1.547862	179.929266	4.256550
1.389506	174.461918	4.261555
1.559592	181.981077	4.266560
1.251138	182.782563	4.271565
1.376612	181.190676	4.276570
1.428905	173.953403	4.281574
1.526953	177.617701	4.286579
1.564841	173.426249	4.291584
1.410737	181.353710	4.296589
1.204614	180.601562	4.301594
1.335581	178.331764	4.306598
1.321330	173.642275	4.311603
1.440387	168.352929	4.316608
1.044942	186.834633	4.321613
1.199869	186.883301	4.326618
1.400551	180.445361	4.331622
1.201600	186.389829	4.336627
1.248556	172.863782	4.341632
0.894389	177.064010	4.346637
1.429206	192.407022	4.351642
2.037503	202.711268	4.356646
1.981586	205.564454	4.361651
2.173902	205.123203	4.366656
1.665974	198.438775	4.371661
1.749973	186.833662	4.376666
1.530146	181.711305	4.381670
1.353384	187.937038	4.386675
1.703371	187.335040	4.391680
1.631680	187.384414	4.396685
1.782570	200.231246	4.401690
1.908176	208.684376	4.406694
1.818291	199.602732	4.411699
1.323776	178.976551	4.416704
1.675305	195.689730	4.421709
1.882004	201.048619	4.426714
1.746665	201.718577	4.431718
1.844602	205.392388	4.436723
2.111215	204.287756	4.441728
1.889652	206.717637	4.446733
1.959280	212.474497	4.451738
1.884689	210.164135	4.456742
1.698318	211.987382	4.461747
2.007559	203.994821	4.466752
1.908621	209.585100	4.471757
1.950353	197.489887	4.476762
2.029132	203.409828	4.481766
1.878752	216.341841	4.486771
2.095806	202.279749	4.491776
1.676858	200.776326	4.496781
1.463330	206.245351	4.501786
1.844521	203.784482	4.506790
1.552336	211.765230	4.511795
1.827696	206.906968	4.516800
1.695691	208.854576	4.521805
1.807887	206.122637	4.526810
1.874613	208.665539	4.531814
1.912654	218.552936	4.536819
2.296261	212.763376	4.541824
1.731900	216.961745	4.546829
2.255227	225.444317	4.551834
2.385955	222.579757	4.556838
2.063576	207.643551	4.561843
2.497565	200.713463	4.566848
2.307539	213.496660	4.571853
2.170192	205.729096	4.576858
2.250823	214.385431	4.581862
2.290131	214.009283	4.586867
2.288970	206.112813	4.591872
2.050251	211.294718	4.596877
2.554057	211.801257	4.601882
2.460982	206.738128	4.606886
2.134845	212.414627	4.611891
1.998219	199.771548	4.616896
2.054231	211.503780	4.621901
2.104057	211.992864	4.626906
2.117730	212.430664	4.631910
2.048530	216.943761	4.636915
2.446091	214.809360	4.641920
2.316096	229.266301	4.646925
2.298114	233.113307	4.651930
2.627903	229.755642	4.656934
2.453714	228.470134	4.661939
2.625481	216.098267	4.666944
2.254991	219.231699	4.671949
2.362139	211.568196	4.676954
2.380735	206.240794	4.681958
1.762671	218.436155	4.686963
2.668837	218.069720	4.691968
2.480803	227.726787	4.696973
2.695072	221.599919	4.701978
2.865729	229.909957	4.706982
2.141202	221.433947	4.711987
2.252786	225.937703	4.716992
2.479967	228.553544	4.721997
2.603568	230.923019	4.727002
2.629319	231.039384	4.732006
2.402975	239.164854	4.737011
2.512911	231.937509	4.742016
2.599968	229.459446	4.747021
2.674472	228.255197	4.752026
2.808002	224.295524	4.757030
2.590613	235.551747	4.762035
2.681869	222.958369	4.767040
2.413382	235.715909	4.772045
2.809425	229.532084	4.777050
2.905869	228.890716	4.782054
2.880345	234.080354	4.787059
2.989167	228.438247	4.792064
2.638720	227.768822	4.797069
2.501214	229.122500	4.802074
2.447723	236.142031	4.807078
2.459642	241.806701	4.812083
2.989466	221.839398	4.817088
2.676047	229.991162	4.822093
2.161363	235.099253	4.827098
2.685359	232.584367	4.832102
2.503799	237.238461	4.837107
2.997803	226.647937	4.842112
2.529167	234.127987	4.847117
2.450768	231.919460	4.852122
2.496603	229.223227	4.857126
2.908220	244.708975	4.862131
3.221526	242.973756	4.867136
3.229669	245.456238	4.872141
2.836119	238.668451	4.877146
3.033344	236.571764	4.882150
2.562745	247.117848	4.887155
3.017172	245.044137	4.892160
3.231027	256.061959	4.897165
3.179964	241.478689	4.902170
3.104313	234.416465	4.907174
2.876384	231.541659	4.912179
3.421773	223.603839	4.917184
3.153195	226.018942	4.922189
2.766337	233.761430	4.927194
2.876494	228.454477	4.932198
2.998329	239.939130	4.937203
3.236718	227.439756	4.942208
3.298934	230.843919	4.947213
2.961425	235.215560	4.952218
2.725995	224.799438	4.957222
2.841071	240.141818	4.962227
3.216066	246.641794	4.967232
3.196274	256.683809	4.972237
3.553282	250.635808	4.977242
3.310347	241.271235	4.982246
3.134893	242.944076	4.987251
3.262769	228.823168	4.992256
2.800132	235.251899	4.997261
3.000410	245.297392	5.002266
3.541437	248.231063	5.007270
3.379666	265.050043	5.012275
3.380273	255.979502	5.017280
3.022155	242.096085	5.022285
2.860685	251.011836	5.027290
3.518761	253.446271	5.032294
3.268079	266.659795	5.037299
3.559987	261.346502	5.042304
3.510137	257.216234	5.047309
3.312203	256.399523	5.052314
3.577594	250.014696	5.057318
3.262093	253.952615	5.062323
3.703159	250.049157	5.067328
3.475520	251.315717	5.072333
3.045137	244.337544	5.077338
3.332064	248.124123	5.082342
3.082365	250.786212	5.087347
3.186321	255.949241	5.092352
3.097676	259.845290	5.097357
3.292713	265.345233	5.102362
3.381506	257.247981	5.107366
3.430607	261.549561	5.112371
3.338183	262.911997	5.117376
3.421997	267.565650	5.122381
3.217458	274.162766	5.127386
3.388421	275.420659	5.132390
3.384301	268.720542	5.137395
3.625422	288.330169	5.142400
3.707109	288.219467	5.147405
3.469513	282.992295	5.152410
3.988074	282.550547	5.157414
3.743648	280.032664	5.162419
3.954717	266.566255	5.167424
3.633462	263.332738	5.172429
3.412157	261.592694	5.177434
3.466219	258.547149	5.182438
3.438430	265.046964	5.187443
3.600084	278.053520	5.192448
3.761454	291.414476	5.197453
3.621949	283.881338	5.202458
3.764972	285.842811	5.207462
4.095812	288.977103	5.212467
3.901447	287.675769	5.217472
3.926127	283.062411	5.222477
3.852254	278.243029	5.227482
3.494868	263.536891	5.232486
3.534693	278.229859	5.237491
3.683242	283.309978	5.242496
3.598304	285.588747	5.247501
3.750079	288.725785	5.252506
4.240837	286.137004	5.257510
3.840330	287.892568	5.262515
3.878347	283.444802	5.267520
3.676093	283.967057	5.272525
3.876110	288.953690	5.277530
4.230453	283.728686	5.282534
3.831310	284.044504	5.287539
4.142704	279.266000	5.292544
3.921963	292.500162	5.297549
3.775385	281.291789	5.302554
3.928197	283.428901	5.307558
3.879947	294.994024	5.312563
3.813648	290.483505	5.317568
3.757899	290.853089	5.322573
4.020991	286.490282	5.327578
3.812176	288.753659	5.332582
4.005245	296.686888	5.337587
3.959020	277.793723	5.342592
3.990165	287.302583	5.347597
3.657258	291.056573	5.352602
3.836798	292.768712	5.357606
3.929547	311.971334	5.362611
4.012414	315.299510	5.367616
4.110174	319.112581	5.372621
4.403413	314.359058	5.377626
4.244462	312.438394	5.382630
4.019928	314.365709	5.387635
3.866516	315.538385	5.392640
4.100905	310.180304	5.397645
4.232587	314.427829	5.402650
4.172515	306.695571	5.407654
4.262577	312.379658	5.412659
4.160132	308.235473	5.417664
3.901641	316.239462	5.422669
4.257266	314.677942	5.427674
4.136427	312.324192	5.432678
3.910102	318.690616	5.437683
4.280209	323.805636	5.442688
4.299193	334.664211	5.447693
4.519731	346.060700	5.452698
4.508533	329.038137	5.457702
4.424381	327.384167	5.462707
4.274857	319.922188	5.467712
4.433732	315.300451	5.472717
4.406375	324.584375	5.477722
4.349260	316.092334	5.482726
3.923276	328.007733	5.487731
4.330520	334.423592	5.492736
4.357205	335.248506	5.497741
4.516635	344.332328	5.502746
4.631117	338.964552	5.507750
4.375594	340.602490	5.512755
4.431801	335.629832	5.517760
4.438083	341.402987	5.522765
4.489913	341.319109	5.527770
4.536849	336.854114	5.532774
4.498415	344.029518	5.537779
4.573690	341.714641	5.542784
4.796864	342.685942	5.547789
4.681947	337.936252	5.552794
4.833785	339.659063	5.557798
4.568768	336.881801	5.562803
4.484191	342.305354	5.567808
4.616687	340.630093	5.572813
4.481927	334.769849	5.577818
4.734057	337.732981	5.582822
4.846710	342.464393	5.587827
4.838333	340.842843	5.592832
4.777362	341.349291	5.597837
4.666833	351.225238	5.602842
4.512476	338.613313	5.607846
4.510853	343.451218	5.612851
4.576621	340.182357	5.617856
5.008172	341.573435	5.622861
4.454427	345.779662	5.627866
4.799969	335.614140	5.632870
4.728259	341.067314	5.637875
4.870311	333.591282	5.642880
4.641628	340.594010	5.647885
4.127680	337.779820	5.652890
4.624893	348.474887	5.657894
4.707446	359.516510	5.662899
5.065095	365.288404	5.667904
5.234330	364.638791	5.672909
4.773008	370.361831	5.677914
5.195315	365.980386	5.682918
5.063186	367.741365	5.687923
5.170115	362.665837	5.692928
5.396632	365.326096	5.697933
5.128671	349.112552	5.702938
4.963974	341.077127	5.707942
4.667877	350.219669	5.712947
4.594947	338.787745	5.717952
4.845166	357.595577	5.722957
4.877354	360.941194	5.727962
5.489137	368.157103	5.732966
5.438949	364.703921	5.737971
5.053926	362.325117	5.742976
5.120009	357.138929	5.747981
5.135425	360.319492	5.752986
5.030984	354.369068	5.757990
4.613958	373.487110	5.762995
5.039391	370.794655	5.768000
5.353244	365.395633	5.773005
5.092699	372.567884	5.778010
5.344629	362.834639	5.783014
5.125784	370.126908	5.788019
5.001010	359.111227	5.793024
5.092038	369.518764	5.798029
5.340765	373.491694	5.803034
5.384272	360.855079	5.808038
5.069964	367.769991	5.813043
5.429989	361.920801	5.818048
5.395820	364.647216	5.823053
5.534645	368.349457	5.828058
5.609561	362.674655	5.833062
5.576631	361.632765	5.838067
5.268590	359.450712	5.843072
5.281378	367.241372	5.848077
5.333256	361.908709	5.853082
5.858633	363.519211	5.858086
5.326125	356.810100	5.863091
4.791629	356.868710	5.868096
5.297510	361.184168	5.873101
5.199147	369.270661	5.878106
5.569624	365.492136	5.883110
5.411631	368.952975	5.888115
5.516072	379.159096	5.893120
5.455942	379.057958	5.898125
5.005855	373.690043	5.903130
5.521187	369.838199	5.908134
5.403374	370.878748	5.913139
5.215323	371.547479	5.918144
5.248180	378.493424	5.923149
5.189448	374.092433	5.928154
5.523116	366.636986	5.933158
5.483078	364.137688	5.938163
5.151718	371.020471	5.943168
5.759596	380.894607	5.948173
5.728347	387.442467	5.953178
5.776674	385.562086	5.958182
5.871684	382.639820	5.963187
5.703284	366.765009	5.968192
5.323871	376.354063	5.973197
5.741566	380.983906	5.978202
6.024947	369.970708	5.983206
5.854159	368.747933	5.988211
5.455273	362.533586	5.993216
5.697354	366.058293	5.998221
5.824196	372.900923	6.003226
5.813111	374.332883	6.008230
5.622592	366.624201	6.013235
5.604648	367.604809	6.018240
5.456855	372.136586	6.023245
5.521533	374.483674	6.028250
5.619507	370.570670	6.033254
5.579520	380.853206	6.038259
5.896804	385.986012	6.043264
5.762442	381.046363	6.048269
5.475986	389.583125	6.053274
5.746356	374.746899	6.058278
5.911874	377.239543	6.063283
5.264214	374.531720	6.068288
5.788119	382.735861	6.073293
5.856803	382.010251	6.078298
5.920107	375.511506	6.083302
5.643757	377.576663	6.088307
5.665206	375.991566	6.093312
5.816086	365.030770	6.098317
5.660999	366.330264	6.103322
5.495175	362.480741	6.108326
5.408904	376.658861	6.113331
5.691684	375.864904	6.118336
5.766305	383.016283	6.123341
5.726416	394.820611	6.128346
5.702946	381.087137	6.133350
5.818298	373.551995	6.138355
5.611764	370.392234	6.143360
5.639768	373.301901	6.148365
5.394423	374.979378	6.153370
5.819574	381.658210	6.158374
6.134216	389.711640	6.163379
5.580200	374.915993	6.168384
5.854963	374.268828	6.173389
5.511752	373.718488	6.178394
5.620045	363.767296	6.183398
5.464071	374.571049	6.188403
6.176087	375.206326	6.193408
5.991222	375.083603	6.198413
5.815596	374.949941	6.203418
6.219283	368.090976	6.208422
6.195047	367.911447	6.213427
6.082041	362.772300	6.218432
5.921958	370.628014	6.223437
5.813518	367.522488	6.228442
5.817844	347.150153	6.233446
5.447957	351.213676	6.238451
5.488721	346.423772	6.243456
5.850730	357.003984	6.248461
5.737714	362.191548	6.253466
5.695686	351.219856	6.258470
5.825759	349.026108	6.263475
5.747861	344.523721	6.268480
5.678526	338.140686	6.273485
5.252887	345.281845	6.278490
5.551399	353.388407	6.283494
5.795469	369.251700	6.288499
6.052914	367.813129	6.293504
5.918159	365.164153	6.298509
5.845310	356.791620	6.303514
5.478759	350.103966	6.308518
5.702559	346.174416	6.313523
5.336098	342.527179	6.318528
5.812545	345.379234	6.323533
5.633402	356.572592	6.328538
5.712384	344.268959	6.333542
5.574022	350.979123	6.338547
5.764207	361.893150	6.343552
5.609903	347.455686	6.348557
5.265422	358.035859	6.353562
5.686953	361.861486	6.358566
5.694589	369.437815	6.363571
5.659644	367.703364	6.368576
5.805548	369.272081	6.373581
5.630542	371.334013	6.378586
5.972789	360.463461	6.383590
5.396971	367.156750	6.388595
5.713004	364.269461	6.393600
5.618003	366.062589	6.398605
5.606551	376.815224	6.403610
5.536425	367.720907	6.408614
5.654011	374.824422	6.413619
5.426554	376.154239	6.418624
5.777686	372.846988	6.423629
5.607960	376.800060	6.428634
6.070981	376.446108	6.433638
5.769154	368.273964	6.438643
5.564255	363.133397	6.443648
5.574412	363.090851	6.448653
5.708737	371.928678	6.453658
5.957576	366.017813	6.458662
5.549269	371.128257	6.463667
5.687143	379.310621	6.468672
6.013815	369.530859	6.473677
5.760288	378.767989	6.478682
5.991007	365.510402	6.483686
5.775900	353.303463	6.488691
5.549395	345.641558	6.493696
5.325882	344.879472	6.498701
5.707231	360.148597	6.503706
6.077720	350.978924	6.508710
5.541007	349.243997	6.513715
5.547563	348.028239	6.518720
5.796182	348.783578	6.523725
5.516255	350.703757	6.528730
5.967167	360.396828	6.533734
5.729005	349.639369	6.538739
5.606585	345.507796	6.543744
6.006969	340.101552	6.548749
5.679633	342.582826	6.553754
6.030476	349.516902	6.558758
5.638408	348.129479	6.563763
5.495308	348.000212	6.568768
5.558256	338.562350	6.573773
5.892115	349.191262	6.578778
5.809033	335.948062	6.583782
5.823789	344.741334	6.588787
5.527707	338.393827	6.593792
5.597906	345.156735	6.598797
5.682233	342.558859	6.603802
5.938430	343.616737	6.608806
5.933541	339.957142	6.613811
5.194117	344.075400	6.618816
5.337102	337.311079	6.623821
5.722698	347.093472	6.628826
5.909744	342.169915	6.633830
5.595132	349.692321	6.638835
5.523167	344.920079	6.643840
5.513675	341.447871	6.648845
5.801984	351.495450	6.653850
6.136342	351.035105	6.658854
5.544273	350.295963	6.663859
5.894721	348.785873	6.668864
5.852589	336.950483	6.673869
5.717929	348.924657	6.678874
5.826438	346.702650	6.683878
5.886064	356.792390	6.688883
5.720441	342.448455	6.693888
5.870854	344.016462	6.698893
5.794957	348.824876	6.703898
5.673877	345.234107	6.708902
5.846264	344.723208	6.713907
5.382390	347.820673	6.718912
5.826085	339.525405	6.723917
5.706395	351.190345	6.728922
5.708470	345.625039	6.733926
5.832859	344.276922	6.738931
5.398707	348.046787	6.743936
5.507124	347.080830	6.748941
5.380059	348.160793	6.753946
5.572815	345.128304	6.758950
5.877013	346.801933	6.763955
5.702571	346.446618	6.768960
5.783024	347.946493	6.773965
5.527689	350.495582	6.778970
5.531065	350.273761	6.783974
5.707984	348.427020	6.788979
5.469375	355.311084	6.793984
5.566921	352.040406	6.798989
5.734278	345.699379	6.803994
5.886620	341.692439	6.808998
5.748140	352.075814	6.814003
5.532809	348.904780	6.819008
5.539170	342.497228	6.824013
5.449546	339.977229	6.829018
5.393459	346.820036	6.834022
5.671946	338.936640	6.839027
5.616973	347.199826	6.844032
5.628326	352.494454	6.849037
5.649914	344.404528	6.854042
5.703233	348.857332	6.859046
5.670822	344.417422	6.864051
5.683086	345.099060	6.869056
5.632201	337.241960	6.874061
5.858481	345.100403	6.879066
5.949055	343.105837	6.884070
5.957649	348.979875	6.889075
5.897367	348.106790	6.894080
6.067259	338.845164	6.899085
5.780857	342.550749	6.904090
5.846771	338.775655	6.909094
5.718015	340.017237	6.914099
5.309386	345.773143	6.919104
5.537574	339.938289	6.924109
5.538552	344.298051	6.929114
5.710199	342.689423	6.934118
5.551055	346.305466	6.939123
5.683583	346.500016	6.944128
5.825036	345.377019	6.949133
5.664915	344.291783	6.954138
5.885761	344.124475	6.959142
5.734578	350.928399	6.964147
5.651450	351.305438	6.969152
6.017769	347.467455	6.974157
5.550148	355.697221	6.979162
5.716893	344.139154	6.984166
5.438681	346.280530	6.989171
5.474744	347.028044	6.994176
5.830315	341.714243	6.999181
5.422899	355.351031	7.004186
5.477432	349.859765	7.009190
5.513391	344.374574	7.014195
5.551780	346.267024	7.019200
5.258644	344.762858	7.024205
5.506302	342.715206	7.029210
6.102162	348.715533	7.034214
5.661248	351.192456	7.039219
5.782240	353.204846	7.044224
5.958049	343.916980	7.049229
5.617392	346.416161	7.054234
5.812736	345.294212	7.059238
5.887081	347.630291	7.064243
5.865538	350.870427	7.069248
6.058498	349.362866	7.074253
5.652065	350.296772	7.079258
5.917809	343.854907	7.084262
6.089646	340.363779	7.089267
5.737806	341.826979	7.094272
5.772892	345.602418	7.099277
5.330263	345.285960	7.104282
5.312537	340.460928	7.109286
5.563591	341.497465	7.114291
5.324542	345.828394	7.119296
5.587106	342.737511	7.124301
5.759011	349.202905	7.129306
5.564772	359.670951	7.134310
5.149486	350.187789	7.139315
5.210096	348.216901	7.144320
6.003961	351.332441	7.149325
5.792142	352.517434	7.154330
5.565631	349.376626	7.159334
5.657238	349.609226	7.164339
5.918152	350.463881	7.169344
5.649584	341.476601	7.174349
5.380006	349.966406	7.179354
5.423546	342.417219	7.184358
5.813617	352.480493	7.189363
5.818017	360.946359	7.194368
5.846124	349.049335	7.199373
5.915751	352.449197	7.204378
5.666740	339.988145	7.209382
5.770273	335.691456	7.214387
5.562575	337.008683	7.219392
5.920701	340.540513	7.224397
5.596766	345.023950	7.229402
5.243586	346.806907	7.234406
5.483078	349.281629	7.239411
5.613626	362.024195	7.244416
6.044172	365.857902	7.249421
5.567862	353.676069	7.254426
5.779687	350.507711	7.259430
5.697277	352.238751	7.264435
5.525848	348.864682	7.269440
5.823398	352.453463	7.274445
5.498748	341.836113	7.279450
5.704653	344.711574	7.284454
5.800026	346.430578	7.289459
5.645831	345.088143	7.294464
5.511537	346.884261	7.299469
5.436369	364.404788	7.304474
5.800711	369.030332	7.309478
5.995250	372.524524	7.314483
5.789075	370.579614	7.319488
5.792639	352.159471	7.324493
5.373611	353.380094	7.329498
5.350400	345.138997	7.334502
5.886229	363.418021	7.339507
5.618198	365.807746	7.344512
6.075161	368.121845	7.349517
5.310253	359.228143	7.354522
5.852338	353.185912	7.359526
5.794500	346.782090	7.364531
5.577139	350.461040	7.369536
5.762852	351.210416	7.374541
5.675352	349.164655	7.379546
5.460774	350.071665	7.384550
5.968236	350.795940	7.389555
5.664001	355.599002	7.394560
5.903446	344.213045	7.399565
5.315934	339.945534	7.404570
5.581499	349.961874	7.409574
5.721511	362.671320	7.414579
5.761067	372.106139	7.419584
5.722884	360.529549	7.424589
4.924776	359.208908	7.429594
5.410865	357.158698	7.434598
5.734796	368.532674	7.439603
5.518776	368.886241	7.444608
6.123075	371.749907	7.449613
5.904794	370.183389	7.454618
6.045823	375.062227	7.459622
5.794730	375.997106	7.464627
5.858201	371.096067	7.469632
5.817025	356.273868	7.474637
5.431611	357.039962	7.479642
5.618691	346.250679	7.484646
5.515048	342.998870	7.489651
5.827860	365.659924	7.494656
5.465649	355.231953	7.499661
5.914672	368.057504	7.504666
5.975930	353.842530	7.509670
5.651275	347.097692	7.514675
5.845384	344.365553	7.519680
5.533302	341.889900	7.524685
5.410899	345.455893	7.529690
5.623760	356.534045	7.534694
5.905545	361.163031	7.539699
5.567921	362.323443	7.544704
5.938613	352.315326	7.549709
5.610978	359.906216	7.554714
5.375598	352.818351	7.559718
5.634870	362.753425	7.564723
5.699491	370.153143	7.569728
5.858312	370.365721	7.574733
5.667024	358.398660	7.579738
5.773041	354.288242	7.584742
5.572560	352.551255	7.589747
5.346339	354.842677	7.594752
5.971238	362.236866	7.599757
6.319327	365.874680	7.604762
5.839093	350.589756	7.609766
5.909768	349.531634	7.614771
5.672558	354.264082	7.619776
5.885077	337.684195	7.624781
5.608024	347.814027	7.629786
5.685108	353.044571	7.634790
5.735269	349.214994	7.639795
5.421719	342.161528	7.644800
5.926952	339.399626	7.649805
5.931548	344.037236	7.654810
5.739615	347.531863	7.659814
6.122993	344.789053	7.664819
5.877124	346.226158	7.669824
6.277401	342.749858	7.674829
5.713594	324.349037	7.679834
5.396754	325.379637	7.684838
5.760974	334.972380	7.689843
5.329777	353.016923	7.694848
5.947147	357.216834	7.699853
5.535634	349.204257	7.704858
5.880879	345.432853	7.709862
5.848482	350.626765	7.714867
5.573489	349.765174	7.719872
5.669850	342.422851	7.724877
5.474057	343.118104	7.729882
5.731339	344.150502	7.734886
5.857257	344.896592	7.739891
5.614771	348.370666	7.744896
5.641740	340.469728	7.749901
5.603951	347.429894	7.754906
5.630111	345.223953	7.759910
5.735379	349.481952	7.764915
5.548342	357.784818	7.769920
5.680924	348.639767	7.774925
5.829392	354.526693	7.779930
5.815077	348.033792	7.784934
6.047665	339.626065	7.789939
5.642848	332.390745	7.794944
5.265005	321.879819	7.799949
5.314223	333.461334	7.804954
5.636125	337.084262	7.809958
5.812745	343.134455	7.814963
5.474962	348.692597	7.819968
5.641460	337.843267	7.824973
5.938324	351.176711	7.829978
5.697175	344.032804	7.834982
5.810065	340.133289	7.839987
5.731158	337.434437	7.844992
5.870477	339.076950	7.849997
5.762322	343.346241	7.855002
5.824400	338.223962	7.860006
5.852277	326.573767	7.865011
5.562326	316.121841	7.870016
5.589979	311.574450	7.875021
5.621375	316.074973	7.880026
5.398251	339.440073	7.885030
5.620663	334.207251	7.890035
5.571995	349.398207	7.895040
5.695719	338.859305	7.900045
5.556134	340.074110	7.905050
5.229241	346.396188	7.910054
5.499379	338.463478	7.915059
5.584837	341.332500	7.920064
5.717331	340.090683	7.925069
5.700290	339.694887	7.930074
5.528664	338.646256	7.935078
5.978196	344.656852	7.940083
5.867155	344.819961	7.945088
5.737649	337.683875	7.950093
5.467552	349.790003	7.955098
5.509435	343.835639	7.960102
5.828918	340.058781	7.965107
5.293028	341.617259	7.970112
5.634500	335.514715	7.975117
5.872301	337.078522	7.980122
5.820123	338.617191	7.985139
5.676727	335.537737	7.990157
5.992386	346.151718	7.995174
6.095555	334.797136	8.000192
5.738323	345.421875	8.005210
5.722053	344.440007	8.010227
5.751464	335.615266	8.015245
5.929841	338.960984	8.020262
6.675292	319.430228	8.025280
5.834568	317.261594	8.030298
5.815148	314.011244	8.035315
5.610800	309.265646	8.040333
5.300930	315.114624	8.045350
5.138850	313.212037	8.050368
5.762821	328.902624	8.055386
5.626658	335.128326	8.060403
5.872223	327.238536	8.065421
5.857067	342.445462	8.070438
6.030851	339.770738	8.075456
6.068494	339.755549	8.080474
5.603409	326.871110	8.085491
5.473131	328.823012	8.090509
5.446881	339.875561	8.095526
5.524840	338.680118	8.100544
5.639154	336.087295	8.105562
5.713891	337.909248	8.110579
6.020974	333.335971	8.115597
5.933956	343.426075	8.120614
5.754719	336.218210	8.125632
5.991670	337.632902	8.130650
5.839727	343.081610	8.135667
5.665581	326.333135	8.140685
5.669035	338.583367	8.145702
5.944698	343.955610	8.150720
5.644574	337.164310	8.155738
6.089573	333.023852	8.160755
5.858153	328.026876	8.165773
5.651309	341.124241	8.170790
5.825241	335.584078	8.175808
5.819313	340.473432	8.180826
5.835697	347.208558	8.185843
5.722968	339.548466	8.190861
5.811139	343.413238	8.195878
5.599563	341.988609	8.200896
5.839669	345.444575	8.205914
5.747162	345.954697	8.210931
5.815171	344.312696	8.215949
5.731359	347.134618	8.220966
5.999340	356.519023	8.225984
6.226638	350.042704	8.231002
6.139746	344.032174	8.236019
6.018088	347.589003	8.241037
5.997610	340.031220	8.246054
5.537604	344.401595	8.251072
5.921608	333.328054	8.256090
5.731445	338.334634	8.261107
6.348605	342.593040	8.266125
5.714683	348.928295	8.271142
5.912058	349.399309	8.276160
6.370645	355.134207	8.281178
6.006067	349.612144	8.286195
5.765355	345.424490	8.291213
6.142720	360.693005	8.296230
6.074744	356.042791	8.301248
6.142431	354.830021	8.306266
6.082117	347.704502	8.311283
6.384510	339.878385	8.316301
6.123172	351.456916	8.321318
5.850984	339.763518	8.326336
5.843057	338.584687	8.331354
5.829773	340.622399	8.336371
5.809025	332.534497	8.341389
5.886825	353.927906	8.346406
6.076813	359.108454	8.351424
6.089343	367.343172	8.356442
6.027115	369.827206	8.361459
6.125621	360.303674	8.366477
6.154661	367.213546	8.371494
6.294177	366.686942	8.376512
6.636114	353.016487	8.381530
5.953063	352.454665	8.386547
5.970736	342.265322	8.391565
5.914701	349.497781	8.396582
6.032155	341.697483	8.401600
5.853264	351.357026	8.406618
5.864057	371.202015	8.411635
6.201491	358.396937	8.416653
6.384646	365.465695	8.421670
6.332607	370.488511	8.426688
6.523575	364.500710	8.431706
5.831174	355.871103	8.436723
5.892148	348.168013	8.441741
6.122346	364.374757	8.446758
6.385558	362.310856	8.451776
6.429750	354.550434	8.456794
6.054705	360.965049	8.461811
6.331587	355.976784	8.466829
6.096621	348.219079	8.471846
5.951616	353.070267	8.476864
6.544069	358.771570	8.481882
6.304036	356.865413	8.486899
6.595138	348.491960	8.491917
6.240976	351.261569	8.496934
6.146690	346.334618	8.501952
6.414374	350.531020	8.506970
5.822078	348.355016	8.511987
6.094367	341.414068	8.517005
5.964099	352.340914	8.522022
6.143963	373.058803	8.527040
6.096486	367.029467	8.532058
5.814668	367.528226	8.537075
6.368018	365.128537	8.542093
6.189006	374.172740	8.547110
6.209534	376.047371	8.552128
6.237860	367.894960	8.557146
6.043142	364.236573	8.562163
5.975797	356.395797	8.567181
5.853938	360.142005	8.572199
5.957070	369.634295	8.577216
6.306030	369.327334	8.582234
6.617484	382.570736	8.587251
6.425149	365.578925	8.592269
6.230618	367.326308	8.597287
6.539193	368.553059	8.602304
6.562542	367.356702	8.607322
6.338100	365.107281	8.612339
6.238754	369.869270	8.617357
6.199678	362.885582	8.622375
6.209530	364.269588	8.627392
6.477588	365.363834	8.632410
6.369415	368.505151	8.637427
6.526023	362.065149	8.642445
6.075908	364.426924	8.647463
6.348539	373.293066	8.652480
6.544834	392.843932	8.657498
6.627722	386.715270	8.662515
6.393717	374.037583	8.667533
6.354460	376.625314	8.672551
6.058092	370.243660	8.677568
6.263441	377.684480	8.682586
6.660254	390.251806	8.687603
6.790495	401.207291	8.692621
6.937020	380.454360	8.697639
6.430667	383.071097	8.702656
6.684987	375.018970	8.707674
6.374197	383.348535	8.712691
6.337651	380.085077	8.717709
6.604242	370.834999	8.722727
6.513566	372.177953	8.727744
6.397415	367.292291	8.732762
6.439896	377.302164	8.737779
6.349923	373.598962	8.742797
6.567646	372.138625	8.747815
6.492691	379.730659	8.752832
6.603459	369.883314	8.757850
6.365468	373.745549	8.762867
6.538091	371.680062	8.767885
6.554285	375.584520	8.772903
6.527152	375.125052	8.777920
6.407493	372.329046	8.782938
6.344987	373.228937	8.787955
6.412421	380.233783	8.792973
6.797845	389.236892	8.797991
6.620676	382.603032	8.803008
6.585457	376.899969	8.808026
6.479624	380.930844	8.813043
6.489188	375.179741	8.818061
6.424401	386.209955	8.823079
6.904637	391.266142	8.828096
6.529493	376.676090	8.833114
6.605101	384.465439	8.838131
6.682998	385.750424	8.843149
6.615044	380.841428	8.848167
6.043849	386.147559	8.853184
6.867295	392.661578	8.858202
6.833539	399.666507	8.863219
6.892550	394.175890	8.868237
6.745795	394.173813	8.873255
6.670111	382.452755	8.878272
7.015216	375.724443	8.883290
6.645368	378.597497	8.888307
6.552449	372.647861	8.893325
6.721791	369.222761	8.898343
6.579890	378.999597	8.903360
6.721705	371.735103	8.908378
6.386293	369.556716	8.913395
7.156773	386.275263	8.918413
6.894933	382.150870	8.923431
6.700986	381.660735	8.928448
6.747570	373.183573	8.933466
6.759228	376.094681	8.938483
6.742841	383.270449	8.943501
7.184404	371.443108	8.948519
6.677448	378.477991	8.953536
6.744596	364.639145	8.958554
6.573987	376.579011	8.963571
6.745544	370.221870	8.968589
6.631579	363.533933	8.973607
6.620334	377.342279	8.978624
7.004089	371.267465	8.983642
6.864443	370.967634	8.988659
6.853380	374.775379	8.993677
6.922965	373.622270	8.998695
6.653690	373.661480	9.003712
6.662828	376.686590	9.008730
6.759925	381.332598	9.013747
6.642411	376.387187	9.018765
6.579737	366.699561	9.023783
7.021416	388.692395	9.028800
6.836207	386.143338	9.033818
6.886569	398.809133	9.038835
7.214767	384.563303	9.043853
6.967925	387.922007	9.048871
6.411634	385.475273	9.053888
6.702106	384.574728	9.058906
7.222150	393.537813	9.063923
6.898867	395.797669	9.068941
7.109972	388.727436	9.073959
6.885292	380.100272	9.078976
6.751505	380.074074	9.083994
6.830239	388.036501	9.089011
6.984431	384.714755	9.094029
6.895115	385.694585	9.099047
6.704877	396.845446	9.104064
6.979451	401.611972	9.109082
6.939374	404.767872	9.114099
7.094198	406.394251	9.119117
7.185480	398.254051	9.124135
7.041923	398.494467	9.129152
6.598656	388.014407	9.134170
7.185383	393.820757	9.139187
6.830525	393.911246	9.144205
6.876684	392.496723	9.149223
6.988042	408.024704	9.154240
6.949400	404.884644	9.159258
7.240126	407.117725	9.164275
6.902647	412.068513	9.169293
7.146071	403.538406	9.174311
6.960767	404.820450	9.179328
6.903986	400.695482	9.184346
7.003334	405.764015	9.189363
6.779432	406.717597	9.194381
7.220072	412.155529	9.199399
7.012643	417.426764	9.204416
7.149416	421.959271	9.209434
7.171017	411.194924	9.214451
7.210016	408.894754	9.219469
7.188391	402.987585	9.224487
7.458628	405.293302	9.229504
7.363072	395.408843	9.234522
6.920566	390.473325	9.239539
6.912428	391.856996	9.244557
6.928206	392.952902	9.249575
7.090799	404.525004	9.254592
7.241348	401.421573	9.259610
7.211082	401.660016	9.264627
6.785354	409.856125	9.269645
7.289334	410.471603	9.274663
6.931981	406.987010	9.279680
7.194389	409.101453	9.284698
7.112940	405.696705	9.289715
7.073688	403.348836	9.294733
7.171848	405.653113	9.299751
6.870361	405.867781	9.304768
7.470241	401.860828	9.309786
7.535972	404.776091	9.314803
7.529246	397.982978	9.319821
7.370671	399.346040	9.324839
6.818859	405.501193	9.329856
7.112658	410.368850	9.334874
7.063500	399.776541	9.339891
7.368557	406.113015	9.344909
7.249885	406.267481	9.349927
7.067154	409.256388	9.354944
7.419083	404.515123	9.359962
7.369225	396.179292	9.364979
7.245376	402.191653	9.369997
7.504066	400.393540	9.375015
7.328741	408.058117	9.380032
7.402109	399.983839	9.385050
7.280763	402.915790	9.390067
7.184340	400.333886	9.395085
7.560950	405.551478	9.400103
7.153750	406.887225	9.405120
7.376037	406.151994	9.410138
7.073205	406.057609	9.415155
7.115394	411.510634	9.420173
7.291496	412.126992	9.425191
7.363641	407.997601	9.430208
7.110483	404.285246	9.435226
7.382441	398.436220	9.440243
7.061480	406.117303	9.445261
7.345631	398.798939	9.450279
7.030538	412.090039	9.455296
7.350047	408.370008	9.460314
7.470026	406.012968	9.465331
7.054824	411.146345	9.470349
7.214375	410.812257	9.475367
7.216713	422.939648	9.480384
7.617661	423.814263	9.485402
7.560882	432.318643	9.490419
7.907750	422.282799	9.495437
7.600707	420.756359	9.500455
7.705473	408.779795	9.505472
7.675599	405.663607	9.510490
7.367160	406.504205	9.515507
7.160068	412.169855	9.520525
7.205599	407.085283	9.525543
7.177503	409.194751	9.530560
7.284754	413.662454	9.535578
7.531294	429.740466	9.540595
7.855637	433.057020	9.545613
7.821055	434.646806	9.550631
7.541969	417.255133	9.555648
7.274084	415.798296	9.560666
7.527701	410.438126	9.565683
7.428946	425.156456	9.570701
7.716121	422.498667	9.575719
7.463701	418.593693	9.580736
7.613336	420.959333	9.585754
7.846598	417.549454	9.590771
7.393975	418.283257	9.595789
7.094183	411.681222	9.600807
7.704217	429.769302	9.605824
7.556492	425.279886	9.610842
7.786257	432.720059	9.615859
7.916344	435.420119	9.620877
7.786718	430.710118	9.625895
7.727251	414.609457	9.630912
7.396619	409.078900	9.635930
7.650223	408.029498	9.640947
7.615895	427.313584	9.645965
7.722375	422.831676	9.650983
7.553759	420.933257	9.656000
7.462479	426.482937	9.661018
7.812135	422.218544	9.666035
7.612194	435.213913	9.671053
7.803965	441.113719	9.676071
7.987312	434.735773	9.681088
7.847924	422.781676	9.686106
7.605021	409.265926	9.691123
7.489845	417.634284	9.696141
7.783570	419.652305	9.701159
7.936263	427.252872	9.706176
7.532774	423.305296	9.711194
7.411456	427.467993	9.716211
7.611152	431.009201	9.721229
7.481251	434.775619	9.726247
7.945309	429.789564	9.731264
7.864951	428.057195	9.736282
7.889492	434.112587	9.741299
7.708250	443.974516	9.746317
7.788859	429.126823	9.751335
7.961772	426.057753	9.756352
7.529425	438.922283	9.761370
7.931163	430.935395	9.766387
7.396273	434.298215	9.771405
7.740624	429.293047	9.776423
7.626958	432.072323	9.781440
7.959453	431.291422	9.786458
7.544174	425.010429	9.791475
7.529952	438.349081	9.796493
7.418164	433.301773	9.801511
7.847837	425.127477	9.806528
8.167134	437.252552	9.811546
8.138849	435.884402	9.816563
8.059660	437.594785	9.821581
7.642688	434.700188	9.826599
7.776506	431.009246	9.831616
7.949444	438.167995	9.836634
7.833669	429.315464	9.841651
7.870253	438.912891	9.846669
7.765882	426.527276	9.851687
8.087393	438.721432	9.856704
7.915208	452.741243	9.861722
7.994709	443.107037	9.866739
8.101256	445.558326	9.871757
8.254554	442.527039	9.876775
7.757790	429.814745	9.881792
7.825895	434.408505	9.886810
8.250885	436.456453	9.891827
8.194378	436.923068	9.896845
7.755320	433.867832	9.901863
8.141081	435.991353	9.906880
7.853742	432.751401	9.911898
7.805859	443.381376	9.916915
8.142218	454.361402	9.921933
8.124784	449.924148	9.926951
8.091323	448.840828	9.931968
8.049673	461.353828	9.936986
7.953839	458.020751	9.942003
8.339697	462.094524	9.947021
8.194943	455.304080	9.952039
8.133870	441.343256	9.957056
8.260310	445.126316	9.962074
7.808765	428.496946	9.967091
7.853928	441.709532	9.972109
8.171933	448.066083	9.977127
8.342719	445.609561	9.982144
8.101239	460.514382	9.987162
8.171998	454.658992	9.992179
8.167099	457.702093	9.997197
7.799683	458.921158	10.002215
8.119546	452.351405	10.007232
8.165344	459.154547	10.012250
8.303679	459.066777	10.017267
8.275682	460.762830	10.022285
7.995632	460.718523	10.027303
8.016445	444.248655	10.032320
8.038014	450.894647	10.037338
8.228935	452.499595	10.042355
8.091553	450.025085	10.047373
7.928647	449.340738	10.052391
8.553444	448.188994	10.057408
8.050938	455.740755	10.062426
8.082870	454.082306	10.067443
7.946887	457.376317	10.072461
7.965149	446.435750	10.077479
8.219867	451.300074	10.082496
8.090771	460.308097	10.087514
8.565228	457.655673	10.092531
8.250802	457.616751	10.097549
7.976264	448.047481	10.102567
8.479126	454.760074	10.107584
8.176598	470.116275	10.112602
8.263361	476.370213	10.117619
8.328776	479.276071	10.122637
8.763896	481.199362	10.127655
8.678337	468.451013	10.132672
8.183170	464.322134	10.137690
8.438094	440.932861	10.142707
8.432016	445.478288	10.147725
7.898312	454.817943	10.152743
8.843876	464.680057	10.157760
8.573438	460.187769	10.162778
8.645400	452.997302	10.167795
8.205250	446.985282	10.172813
8.055472	449.385216	10.177831
8.514759	455.656517	10.182848
8.524817	473.974346	10.187866
8.866920	461.692320	10.192883
8.447901	454.749192	10.197901
8.278752	454.558122	10.202919
8.411191	447.629577	10.207936
8.142799	458.748541	10.212954
8.609023	464.851503	10.217971
8.611537	465.921090	10.222989
8.620289	461.366123	10.228007
8.675863	452.685546	10.233024
8.601864	451.299312	10.238042
8.361529	442.283256	10.243059
8.300688	444.347367	10.248077
8.361491	458.832444	10.253095
8.625008	459.804332	10.258112
8.596780	469.030082	10.263130
8.540396	468.392160	10.268147
8.810628	465.787512	10.273165
8.661485	475.483485	10.278183
8.901448	465.098299	10.283200
8.594422	461.608965	10.288218
8.316901	454.791987	10.293235
8.521858	454.879969	10.298253
8.120597	463.179565	10.303271
8.063650	460.455769	10.308288
8.206110	475.032205	10.313306
8.255923	474.232478	10.318323
8.575130	471.547573	10.323341
8.539260	481.923227	10.328359
8.934309	473.826916	10.333376
9.133150	479.937064	10.338394
8.897427	475.616055	10.343411
8.890587	466.695945	10.348429
8.920240	477.518917	10.353447
9.242199	466.761124	10.358464
9.066830	472.371331	10.363482
8.280794	473.242581	10.368499
9.342015	466.597690	10.373517
8.807264	482.097583	10.378535
8.960660	474.159054	10.383552
8.678386	469.993662	10.388570
8.749940	471.759324	10.393587
8.792572	473.756733	10.398605
8.640954	471.271828	10.403623
8.619913	471.477269	10.408640
8.698789	474.873317	10.413658
8.659634	471.259961	10.418675
8.896414	465.312284	10.423693
8.406741	479.747929	10.428711
8.895320	464.700587	10.433728
8.468236	473.032636	10.438746
8.641242	468.278363	10.443763
8.539932	472.254901	10.448781
8.631123	474.364621	10.453799
8.827357	475.410168	10.458816
8.963970	475.767631	10.463834
9.037052	481.329445	10.468851
8.687656	472.418824	10.473869
8.936861	482.954937	10.478887
9.321083	474.027200	10.483904
9.064582	479.994099	10.488922
8.889262	481.650122	10.493939
9.066606	478.712890	10.498957
9.123248	481.604344	10.503975
9.006034	471.773729	10.508992
9.145800	475.034005	10.514010
8.858810	465.952665	10.519027
8.841774	464.358691	10.524045
8.976432	470.340039	10.529063
9.189476	467.962098	10.534080
9.249215	479.007572	10.539098
8.700696	475.997881	10.544115
9.187962	477.499595	10.549133
9.125771	486.333049	10.554151
8.980756	473.852785	10.559168
8.847304	479.794093	10.564186
8.688293	482.668843	10.569203
9.396741	476.767180	10.574221
9.142949	477.744384	10.579239
9.052925	473.927561	10.584256
8.932710	477.380049	10.589274
9.099367	485.966209	10.594291
9.366512	474.330229	10.599309
9.039219	475.609280	10.604327
9.277034	475.944575	10.609344
9.070734	476.598760	10.614362
9.123442	482.432008	10.619379
8.745843	480.241282	10.624397
8.833127	493.163288	10.629415
9.435869	497.575468	10.634432
9.334660	500.494812	10.639450
9.178155	492.576429	10.644467
9.372381	477.720361	10.649485
9.201601	483.146818	10.654503
9.254445	470.932197	10.659520
9.274880	479.418190	10.664538
9.164736	483.288818	10.669555
9.176512	469.045162	10.674573
9.284454	479.843245	10.679591
9.131002	478.453679	10.684608
9.086847	485.482362	10.689626
9.018560	501.155335	10.694643
9.439679	494.459250	10.699661
9.529976	513.777550	10.704679
9.076754	504.353010	10.709696
9.540593	505.807905	10.714714
9.577976	502.457103	10.719731
9.470741	492.154702	10.724749
9.233522	485.899437	10.729767
9.397677	475.718625	10.734784
9.425865	478.766013	10.739802
9.028249	484.698220	10.744819
9.530539	479.280133	10.749837
9.312350	492.145859	10.754855
9.316548	497.983557	10.759872
9.403824	493.148037	10.764890
9.486654	505.127173	10.769907
9.495246	493.825178	10.774925
9.388162	499.711869	10.779943
9.279324	508.038251	10.784960
9.537741	506.148654	10.789978
9.187944	500.393856	10.794995
9.536965	501.260832	10.800013
9.331383	503.688451	10.805031
9.579275	496.934300	10.810048
9.322088	496.349929	10.815066
9.476467	498.011099	10.820083
9.629863	504.851048	10.825101
9.611812	496.936216	10.830119
9.123487	497.536762	10.835136
9.217585	494.902902	10.840154
9.211213	504.320904	10.845171
9.615356	505.236048	10.850189
9.655519	501.894277	10.855207
9.477193	496.283026	10.860224
9.656196	503.737495	10.865242
9.472710	499.237884	10.870259
9.476750	494.039868	10.875277
9.539035	495.283126	10.880295
9.584393	509.606565	10.885312
9.742230	497.283958	10.890330
9.543030	505.794909	10.895347
9.708691	506.523359	10.900365
9.736450	500.576862	10.905383
9.656794	498.509864	10.910400
9.608615	495.595342	10.915418
9.364557	503.018267	10.920435
9.490293	490.435610	10.925453
9.717415	499.094353	10.930471
9.763346	508.415801	10.935488
9.739446	498.491655	10.940506
9.772597	505.318887	10.945523
9.970131	502.053444	10.950541
9.824127	505.254361	10.955559
9.652212	511.021827	10.960576
9.945075	505.560806	10.965594
9.535460	507.218827	10.970611
9.794989	506.960591	10.975629
9.935138	504.745544	10.980647
9.889596	502.338688	10.985664
10.254163	497.387138	10.990682
9.447714	506.952589	10.995699
9.895560	505.487743	11.000717
9.933064	506.390906	11.005735
9.674411	504.882122	11.010752
9.923533	500.166408	11.015770
9.773930	504.999423	11.020787
9.813429	500.843567	11.025805
10.067002	500.933399	11.030823
9.931166	503.501567	11.035840
9.904063	503.411316	11.040858
9.640132	505.390490	11.045875
9.326898	502.536431	11.050893
9.375599	508.887862	11.055911
9.627786	521.812453	11.060928
10.326840	525.496344	11.065946
9.940302	524.903838	11.070963
10.126484	525.067344	11.075981
10.408403	531.429579	11.080999
10.172292	521.671213	11.086016
9.752548	503.323203	11.091034
9.758558	516.889115	11.096051
10.429234	518.220086	11.101069
10.221297	499.870452	11.106087
9.709583	500.774460	11.111104
9.897608	507.530090	11.116122
10.195151	515.625548	11.121139
9.846043	518.555334	11.126157
10.152209	516.042878	11.131175
10.027355	521.919738	11.136192
9.944629	515.498246	11.141210
9.688936	528.199463	11.146227
10.086743	528.083661	11.151245
9.995157	535.956076	11.156263
10.063747	532.726610	11.161280
10.565320	531.319615	11.166298
10.525315	533.901175	11.171315
9.967182	527.626749	11.176333
10.150504	524.729599	11.181351
9.984617	534.503967	11.186368
10.391090	523.909622	11.191386
10.409284	532.594805	11.196403
10.457998	518.575694	11.201421
10.506438	504.676555	11.206439
9.834878	508.095516	11.211456
10.230283	505.073622	11.216474
10.120914	530.094152	11.221491
10.326399	528.058212	11.226509
10.523204	524.111231	11.231527
10.282065	515.840028	11.236544
10.138321	502.314983	11.241562
10.139573	512.545984	11.246579
10.151720	518.120513	11.251597
10.473930	531.065698	11.256615
10.035053	527.852627	11.261632
10.393119	525.625525	11.266650
10.163613	521.287752	11.271667
10.123474	521.783362	11.276685
10.414921	529.005630	11.281703
10.043450	524.191487	11.286720
10.345177	520.063967	11.291738
10.216320	527.093314	11.296755
10.236280	519.181984	11.301773
10.653436	524.273339	11.306791
10.324531	521.276567	11.311808
10.323858	524.221188	11.316826
10.379610	527.608246	11.321843
10.296520	518.274027	11.326861
10.183623	520.794422	11.331879
10.109345	522.321009	11.336896
10.350043	522.889381	11.341914
10.176781	529.638511	11.346931
10.218582	534.368961	11.351949
10.708008	534.768976	11.356967
10.126401	541.174995	11.361984
10.362920	538.537749	11.367002
10.150847	540.455153	11.372019
10.556070	534.503152	11.377037
10.600264	539.160646	11.382055
10.491831	547.960350	11.387072
10.738314	544.242265	11.392090
10.692377	538.556609	11.397107
10.770366	538.588747	11.402125
10.749687	542.353853	11.407143
10.936963	538.831236	11.412160
10.912117	542.363468	11.417178
10.592735	540.879975	11.422195
10.561495	534.497746	11.427213
11.034715	539.040683	11.432231
10.717812	535.382470	11.437248
10.493077	518.720634	11.442266
10.816893	523.741408	11.447283
10.397482	527.856161	11.452301
10.427474	535.431818	11.457319
10.481123	541.312274	11.462336
10.680766	539.182575	11.467354
10.935038	535.520075	11.472371
10.365659	540.598751	11.477389
10.806398	532.362712	11.482407
10.710654	540.412505	11.487424
10.595867	544.145020	11.492442
10.631393	535.726318	11.497459
10.595446	545.398282	11.502477
10.684417	536.103366	11.507495
10.717018	539.961109	11.512512
10.373284	543.063626	11.517530
10.400798	542.532475	11.522547
10.409040	546.706458	11.527565
11.025497	548.970571	11.532583
11.025438	567.176472	11.537600
10.958095	559.973075	11.542618
10.942161	554.248000	11.547635
11.171131	551.290045	11.552653
11.349436	548.362120	11.557671
11.333436	536.773618	11.562688
11.049917	538.089996	11.567706
10.886819	543.354322	11.572723
10.353123	542.601836	11.577741
11.191134	543.360640	11.582759
10.867137	548.965756	11.587776
11.129302	542.581734	11.592794
10.885174	529.151292	11.597811
10.888342	530.410127	11.602829
10.941811	528.726206	11.607847
11.000080	536.073373	11.612864
11.038738	535.957040	11.617882
10.878157	534.688506	11.622899
10.773427	524.944267	11.627917
10.755540	528.907746	11.632935
10.923840	543.420231	11.637952
10.983560	551.720223	11.642970
11.211018	554.143115	11.647987
10.934793	559.718658	11.653005
11.500877	550.295332	11.658023
11.430700	557.110371	11.663040
11.413943	544.464796	11.668058
11.226803	538.059656	11.673075
11.255283	535.382424	11.678093
11.103216	532.935450	11.683111
10.941840	530.685593	11.688128
10.945365	538.726143	11.693146
11.081753	535.681712	11.698163
11.293255	547.101078	11.703181
11.441108	542.114043	11.708199
11.213675	546.694179	11.713216
11.379474	542.436474	11.718234
11.056074	534.638894	11.723251
10.901311	535.225047	11.728269
11.174010	552.747574	11.733287
11.195164	564.723791	11.738304
11.576990	561.022366	11.743322
11.772626	561.556775	11.748339
11.626487	558.600787	11.753357
11.563075	540.963763	11.758375
11.204345	539.148768	11.763392
11.031761	535.758274	11.768410
11.174776	528.667096	11.773427
11.193183	538.854400	11.778445
11.280257	539.778199	11.783463
11.505695	549.024206	11.788480
11.185324	562.152144	11.793498
11.681388	546.923680	11.798515
11.578326	544.551077	11.803533
11.529230	535.760629	11.808551
11.211778	538.767509	11.813568
11.002239	544.181122	11.818586
11.450149	548.589172	11.823603
11.392401	566.311810	11.828621
11.478088	558.658405	11.833639
11.573465	564.178883	11.838656
11.564214	566.932353	11.843674
11.883547	560.577237	11.848691
11.611594	560.178212	11.853709
11.397929	539.576204	11.858727
11.475642	557.722574	11.863744
11.403098	552.994130	11.868762
11.778159	548.905606	11.873779
11.323536	553.836918	11.878797
11.623444	547.996086	11.883815
11.548263	559.892720	11.888832
11.477681	559.380095	11.893850
11.656217	554.706983	11.898867
11.676625	563.675855	11.903885
11.403393	555.984014	11.908903
11.450665	554.272660	11.913920
11.396899	559.317891	11.918938
11.474147	554.622780	11.923955
11.544264	560.333405	11.928973
11.825793	555.486368	11.933991
11.813820	554.901443	11.939008
11.654100	561.332885	11.944026
11.686760	555.436095	11.949043
11.525742	554.612594	11.954061
11.633289	555.280723	11.959079
11.642899	553.079813	11.964096
11.454750	560.686504	11.969114
11.714281	562.785638	11.974131
11.769593	570.906450	11.979149
12.217236	580.351186	11.984167
11.906283	559.862227	11.989184
11.650842	561.347775	11.994202
11.831989	557.021390	11.999219
11.371170	565.349299	12.004237
12.057963	578.145877	12.009255
12.410518	579.236364	12.014272
12.044510	576.980694	12.019290
12.076712	563.434347	12.024307
11.565105	563.255908	12.029325
11.842966	567.031047	12.034343
11.547530	560.485078	12.039360
12.067214	579.827691	12.044378
11.717528	575.985259	12.049395
11.662676	585.344627	12.054413
11.793065	585.731470	12.059431
12.075468	585.135136	12.064448
12.211166	582.614665	12.069466
12.404116	586.807054	12.074483
11.933993	584.185846	12.079501
11.969115	585.786815	12.084519
11.931552	589.267399	12.089536
11.752925	585.110986	12.094554
12.057794	583.270907	12.099571
11.950450	587.320999	12.104589
12.178747	574.359298	12.109607
12.336603	586.632845	12.114624
12.276316	586.730829	12.119642
12.418507	582.148611	12.124659
12.165412	583.223541	12.129677
11.978928	585.787033	12.134695
12.295369	576.863552	12.139712
11.994352	588.331689	12.144730
12.287372	580.636323	12.149747
12.153457	587.070042	12.154765
12.004540	580.034052	12.159783
12.145594	582.006585	12.164800
11.824501	583.511888	12.169818
12.069009	576.679343	12.174835
11.853577	571.389460	12.179853
12.394720	583.369423	12.184871
12.243654	580.202767	12.189888
11.942611	584.226403	12.194906
12.516591	581.930750	12.199923
12.298071	583.246414	12.204941
12.264129	592.119675	12.209959
12.174542	579.286671	12.214976
12.246400	586.442383	12.219994
12.424669	579.733823	12.225011
12.444813	583.877548	12.230029
12.230869	580.537707	12.235047
12.387506	586.468313	12.240064
12.094249	589.698628	12.245082
12.292486	588.670514	12.250099
12.741063	592.608259	12.255117
12.463088	586.687546	12.260135
12.534715	582.097450	12.265152
12.652758	574.625160	12.270170
12.537552	571.910475	12.275187
12.471222	576.171888	12.280205
12.346593	577.097302	12.285223
12.108174	580.088650	12.290240
12.094420	595.488075	12.295258
12.684611	601.893553	12.300275
12.912386	605.184245	12.305293
12.867783	595.544155	12.310311
12.939502	587.129225	12.315328
12.813500	583.305393	12.320346
12.818388	577.056343	12.325363
12.240138	578.879647	12.330381
12.278332	576.690033	12.335399
12.685229	578.106519	12.340416
12.768575	578.563849	12.345434
12.595509	582.772559	12.350451
12.681852	579.376202	12.355469
12.538627	576.160980	12.360487
12.528100	577.182124	12.365504
12.702410	598.311399	12.370522
13.126607	596.825005	12.375539
12.870824	587.855477	12.380557
12.576998	582.154998	12.385575
12.279816	573.744227	12.390592
12.513507	592.188083	12.395610
12.689093	590.418752	12.400627
12.502916	603.074416	12.405645
12.462082	601.316902	12.410663
12.949921	600.189764	12.415680
12.690118	610.395452	12.420698
13.186798	594.156998	12.425715
12.980620	605.480899	12.430733
13.255754	605.930269	12.435751
13.040073	600.280657	12.440768
12.708276	608.629396	12.445786
13.040540	604.042639	12.450803
13.109229	605.329083	12.455821
12.879190	608.906100	12.460839
13.078451	604.119276	12.465856
12.836873	598.006665	12.470874
12.945445	598.340122	12.475891
12.890015	605.856611	12.480909
12.827742	609.928048	12.485927
13.205949	597.409900	12.490944
12.569296	616.021705	12.495962
12.876667	605.966701	12.500979
12.944499	601.042681	12.505997
12.976446	609.848823	12.511015
13.018819	598.232201	12.516032
13.173030	601.307201	12.521050
13.185550	606.562965	12.526067
12.861050	599.245209	12.531085
12.711495	607.404449	12.536103
12.969832	596.902699	12.541120
12.611327	607.909642	12.546138
12.811408	605.338056	12.551155
13.372982	619.293524	12.556173
13.278756	615.950698	12.561191
13.159125	607.950746	12.566208
13.157055	601.696466	12.571226
12.929148	605.935866	12.576243
13.386157	619.996080	12.581261
13.012638	632.974607	12.586279
13.311231	621.415655	12.591296
13.225491	633.869412	12.596314
13.672324	619.024141	12.601331
13.659356	625.142279	12.606349
13.210124	609.219276	12.611367
13.277846	608.369400	12.616384
13.223407	605.553671	12.621402
13.136050	601.966775	12.626419
13.378265	610.001517	12.631437
13.033667	614.609494	12.636455
13.529486	620.654225	12.641472
13.352746	632.639403	12.646490
13.402666	622.419601	12.651507
13.550241	626.988337	12.656525
13.452098	632.337186	12.661543
14.027508	623.335237	12.666560
13.138616	612.934332	12.671578
13.320976	620.104302	12.676595
13.496433	620.736548	12.681613
13.500326	628.897001	12.686631
13.704322	625.564251	12.691648
13.612938	629.602385	12.696666
13.349087	616.850307	12.701683
13.935591	616.285219	12.706701
13.348583	617.627062	12.711719
13.447429	610.429164	12.716736
13.297516	610.522256	12.721754
13.176013	615.688568	12.726771
13.441617	622.350036	12.731789
13.574370	638.357702	12.736807
13.528160	627.862625	12.741824
13.309214	632.170054	12.746842
13.137020	633.563669	12.751859
13.141791	631.401376	12.756877
13.656108	642.855409	12.761895
14.051026	639.536924	12.766912
13.616082	638.510185	12.771930
13.465813	636.318535	12.776947
13.548772	637.334503	12.781965
13.857744	651.064487	12.786983
13.867428	657.068634	12.792000
13.984140	652.045423	12.797018
13.357507	635.834611	12.802035
13.932278	635.605875	12.807053
13.899346	655.524304	12.812071
14.093073	652.811696	12.817088
13.670990	638.913592	12.822106
13.709093	640.548812	12.827123
14.188696	642.834380	12.832141
13.627891	636.743371	12.837159
14.184471	637.132866	12.842176
14.002601	628.751338	12.847194
14.141313	624.917579	12.852211
13.905024	624.929530	12.857229
13.570777	634.105483	12.862247
13.830909	626.011308	12.867264
13.954987	647.375728	12.872282
14.204045	656.719075	12.877299
14.170977	639.001461	12.882317
14.098427	632.357427	12.887335
13.840718	623.167277	12.892352
14.225784	626.490133	12.897370
14.024624	626.275675	12.902387
14.086413	624.871307	12.907405
13.894185	632.923636	12.912423
13.826117	637.018078	12.917440
14.292965	650.035361	12.922458
14.071765	655.422432	12.927475
14.892463	646.290522	12.932493
14.270085	636.769338	12.937511
14.163867	635.353424	12.942528
14.265111	628.284531	12.947546
14.010452	630.341160	12.952563
13.973150	624.089237	12.957581
13.811828	631.152114	12.962599
14.181746	637.784620	12.967616
14.631626	646.405378	12.972634
14.102148	641.909448	12.977651
14.354891	642.169825	12.982669
13.924587	660.130808	12.987687
14.166512	654.400013	12.992704
14.217060	662.199721	12.997722
13.919753	654.035084	13.002739
14.198144	645.404709	13.007757
14.209485	651.519048	13.012775
14.525157	657.207009	13.017792
14.832691	657.111663	13.022810
14.136561	651.603584	13.027827
14.360447	644.900476	13.032845
14.332006	658.620216	13.037863
14.343715	654.361381	13.042880
14.601293	653.519625	13.047898
14.312544	652.009233	13.052915
14.750949	636.250086	13.057933
14.274896	649.976836	13.062951
14.777884	652.183002	13.067968
14.637857	646.423692	13.072986
14.434606	653.818194	13.078003
14.562894	647.701264	13.083021
14.508301	653.330473	13.088039
14.605371	651.396713	13.093056
14.542830	658.573511	13.098074
14.479104	656.339897	13.103091
14.595390	650.240625	13.108109
14.513872	661.747000	13.113127
14.635147	655.735307	13.118144
14.646979	655.086690	13.123162
14.451606	655.934829	13.128179
14.884401	652.250646	13.133197
15.048831	650.524082	13.138215
14.794683	638.922335	13.143232
14.671092	650.832926	13.148250
14.512391	650.296234	13.153267
14.731884	644.240754	13.158285
14.666766	649.931572	13.163303
14.660530	645.369438	13.168320
14.724575	651.017928	13.173338
14.676636	653.619682	13.178355
14.883049	647.809247	13.183373
14.583279	650.993256	13.188391
14.709788	647.366531	13.193408
15.023590	640.731387	13.198426
14.728598	645.495701	13.203443
14.734426	640.363635	13.208461
14.946515	657.469729	13.213479
15.109254	666.406885	13.218496
14.894226	655.591104	13.223514
14.606166	658.271507	13.228531
15.057080	674.462885	13.233549
15.039796	683.002222	13.238567
15.228638	679.782290	13.243584
15.096335	671.209939	13.248602
14.753422	655.951889	13.253619
15.437401	660.692209	13.258637
14.954654	663.387338	13.263655
15.061037	649.040352	13.268672
15.058092	655.885921	13.273690
15.288577	677.748101	13.278707
15.353757	654.571314	13.283725
15.119008	655.141601	13.288743
14.744017	650.712982	13.293760
15.257362	657.906847	13.298778
15.348536	661.342029	13.303795
15.126639	648.416097	13.308813
15.087445	662.651921	13.313831
15.097210	669.350336	13.318848
15.530634	669.124812	13.323866
15.177375	662.777212	13.328883
15.373006	652.405175	13.333901
15.407931	651.188051	13.338919
15.102109	661.334707	13.343936
15.232352	652.165808	13.348954
14.832278	667.490125	13.353971
15.522959	665.466512	13.358989
15.567111	675.564653	13.364007
15.502654	677.575708	13.369024
15.203751	673.242459	13.374042
15.369061	668.041215	13.379059
15.552561	666.725072	13.384077
15.624519	676.894597	13.389095
15.781424	671.158183	13.394112
15.317105	652.416216	13.399130
15.409363	660.537592	13.404147
15.382209	654.119966	13.409165
15.437471	655.919757	13.414183
15.380615	673.355183	13.419200
15.677341	669.821704	13.424218
15.576464	675.925231	13.429235
15.709281	673.174826	13.434253
15.590625	666.648456	13.439271
15.552842	675.279363	13.444288
15.770083	667.520094	13.449306
15.390748	662.779728	13.454323
15.553421	667.352420	13.459341
15.262645	664.324403	13.464359
15.552761	672.083424	13.469376
15.895933	663.464981	13.474394
15.613818	676.097859	13.479411
15.517081	668.996854	13.484429
15.345703	670.895272	13.489447
15.391900	679.260559	13.494464
15.732798	674.120165	13.499482
15.329372	674.944099	13.504499
15.866062	672.717394	13.509517
15.772663	671.574023	13.514535
15.413109	675.247086	13.519552
15.821937	671.099595	13.524570
15.780033	676.193493	13.529587
15.846153	678.764757	13.534605
15.868978	669.192957	13.539623
15.752673	676.169904	13.544640
16.028927	680.813166	13.549658
15.620837	686.037025	13.554675
15.890652	684.925107	13.559693
16.166191	700.206712	13.564711
16.288209	688.643825	13.569728
15.845224	679.488986	13.574746
16.037406	670.446073	13.579763
15.956987	668.830454	13.584781
15.707651	675.657830	13.589799
16.098029	686.781016	13.594816
16.572893	688.489820	13.599834
16.017597	687.216847	13.604851
15.896981	671.759852	13.609869
16.264881	680.295641	13.614887
16.129016	681.629919	13.619904
16.176367	667.554099	13.624922
16.083286	673.056801	13.629939
16.023703	679.027628	13.634957
16.393137	688.992760	13.639975
16.092669	687.357968	13.644992
16.399494	685.899424	13.650010
16.238359	683.804145	13.655027
16.002366	681.076810	13.660045
16.506481	685.106860	13.665063
16.128424	687.662513	13.670080
16.586854	681.118303	13.675098
16.393915	676.878904	13.680115
16.102966	663.916443	13.685133
16.087267	674.210153	13.690151
16.143051	683.747899	13.695168
16.404158	686.774608	13.700186
16.226083	692.000298	13.705203
16.270670	691.378106	13.710221
16.324850	693.629350	13.715239
16.523602	688.795247	13.720256
16.733464	677.590988	13.725274
16.461728	693.021451	13.730291
16.289670	696.494727	13.735309
16.250192	692.022996	13.740327
16.238400	698.358726	13.745344
16.704113	686.031933	13.750362
16.188228	697.170887	13.755379
16.138409	693.679077	13.760397
16.185849	699.557402	13.765415
16.227527	697.900560	13.770432
16.427748	703.193214	13.775450
16.590864	712.449071	13.780467
16.346146	721.175539	13.785485
16.933723	712.913255	13.790503
16.886469	712.857718	13.795520
16.795085	718.391727	13.800538
16.786018	719.276950	13.805555
16.684041	718.371606	13.810573
17.158965	713.538406	13.815591
16.858033	704.689502	13.820608
17.167278	693.684257	13.825626
16.520810	685.640584	13.830643
16.650466	690.070132	13.835661
16.715202	682.988003	13.840679
16.414201	692.054635	13.845696
16.737499	703.484987	13.850714
16.631970	712.038164	13.855731
16.825282	716.157943	13.860749
16.879433	715.467979	13.865767
16.625771	719.594675	13.870784
16.808313	708.202173	13.875802
16.831731	712.010899	13.880819
17.076721	719.429872	13.885837
17.073281	717.628618	13.890855
17.002579	722.064320	13.895872
17.073292	712.664875	13.900890
17.224048	710.233547	13.905907
17.036329	711.402382	13.910925
17.062814	707.791316	13.915943
16.627060	713.511823	13.920960
16.805888	703.338050	13.925978
16.885877	721.004546	13.930995
16.969287	714.055178	13.936013
17.444341	708.533992	13.941031
17.276856	718.920938	13.946048
17.189432	708.397557	13.951066
16.816835	706.240733	13.956083
17.268225	707.353613	13.961101
17.248381	711.588839	13.966119
17.557490	715.848266	13.971136
17.167734	705.388036	13.976154
17.512908	715.044559	13.981171
17.412208	718.866421	13.986189
17.393322	708.120863	13.991207
17.160564	715.841907	13.996224
17.500796	707.968675	14.001242
17.015126	716.287924	14.006259
17.087900	712.189921	14.011277
17.408136	712.613294	14.016295
17.292214	721.821357	14.021312
17.060540	712.380928	14.026330
17.246293	730.977606	14.031347
17.062619	738.832981	14.036365
17.730293	737.434661	14.041383
17.391644	740.195586	14.046400
17.490045	733.890804	14.051418
17.451774	735.143522	14.056435
17.313130	739.037607	14.061453
17.339395	730.724406	14.066471
17.574988	734.452555	14.071488
17.768231	729.931729	14.076506
17.900622	736.816084	14.081523
17.504668	733.182839	14.086541
17.969029	726.561944	14.091559
17.473516	735.715879	14.096576
17.716124	724.130918	14.101594
17.691617	729.338870	14.106611
17.660391	736.848466	14.111629
17.961833	729.028640	14.116647
17.618506	742.857741	14.121664
17.575759	732.504072	14.126682
17.720634	733.267346	14.131699
17.504821	742.863457	14.136717
17.843072	735.956203	14.141735
18.030312	735.516786	14.146752
17.654774	735.812487	14.151770
17.594838	728.566836	14.156787
17.384470	733.911208	14.161805
17.579929	724.530081	14.166823
18.004873	741.060106	14.171840
18.002403	751.881965	14.176858
18.415419	744.937747	14.181875
17.875609	742.879701	14.186893
18.008454	733.224357	14.191911
17.913799	737.162042	14.196928
17.749379	737.778116	14.201946
17.840912	741.995899	14.206963
18.522837	757.718812	14.211981
18.652505	742.635953	14.216999
18.090336	745.889494	14.222016
17.910889	730.725688	14.227034
18.051884	723.615815	14.232051
18.245701	741.507495	14.237069
18.164217	728.524791	14.242087
18.148454	734.450900	14.247104
17.899121	739.766665	14.252122
17.999136	743.298307	14.257139
18.137540	749.509536	14.262157
18.653625	748.456860	14.267175
18.365632	745.636676	14.272192
17.882375	740.559120	14.277210
18.410716	748.618522	14.282227
18.292062	753.222692	14.287245
18.496825	746.222740	14.292263
18.520378	757.255121	14.297280
18.238420	750.934188	14.302298
18.356946	749.568258	14.307315
18.734047	762.198897	14.312333
18.392497	742.487697	14.317351
18.350458	740.784007	14.322368
18.082245	749.163875	14.327386
18.575415	753.034708	14.332403
18.857585	755.919273	14.337421
18.620141	744.952315	14.342439
18.264191	750.186957	14.347456
18.421644	752.781792	14.352474
18.807357	751.399246	14.357491
18.823442	757.238321	14.362509
18.461284	755.827784	14.367527
18.335066	758.211444	14.372544
18.265382	757.610309	14.377562
18.590764	745.816704	14.382579
18.623523	755.572692	14.387597
18.588478	754.871455	14.392615
18.751793	752.810539	14.397632
18.314673	763.182952	14.402650
18.666359	754.039266	14.407667
18.504095	762.121672	14.412685
18.641933	750.616226	14.417703
18.706403	754.989732	14.422720
18.470257	758.346828	14.427738
19.079085	755.569166	14.432755
18.753297	767.729267	14.437773
18.674342	762.541021	14.442791
18.996690	767.524224	14.447808
19.013413	771.229870	14.452826
19.138111	770.585655	14.457843
18.913951	764.747969	14.462861
18.945624	773.462716	14.467879
19.205634	764.768892	14.472896
18.941671	765.290110	14.477914
18.845674	757.775540	14.482931
18.315564	770.157005	14.487949
19.009513	771.471728	14.492967
19.182586	780.520931	14.497984
18.900028	779.681748	14.503002
19.340101	775.381014	14.508019
19.393703	783.287595	14.513037
19.438321	772.538360	14.518055
19.362818	778.862010	14.523072
19.226828	782.585273	14.528090
19.210368	772.770263	14.533107
18.980570	776.921636	14.538125
19.169456	769.337179	14.543143
19.351741	777.526554	14.548160
19.149703	779.057401	14.553178
19.268759	767.425498	14.558195
19.114125	787.445194	14.563213
19.082600	784.202966	14.568231
19.518742	775.557279	14.573248
19.383753	776.635806	14.578266
19.418764	775.033650	14.583283
19.593445	778.297979	14.588301
19.625884	774.130542	14.593319
19.161781	773.572269	14.598336
19.350068	766.543332	14.603354
19.455976	762.572671	14.608371
19.528241	777.699999	14.613389
19.377252	768.158536	14.618407
19.556210	772.504640	14.623424
19.662669	776.215162	14.628442
19.558024	768.004506	14.633459
19.112678	772.767165	14.638477
19.490350	766.481732	14.643495
19.823308	756.675100	14.648512
19.420150	762.942784	14.653530
19.437441	760.800604	14.658547
19.747884	764.539123	14.663565
19.784591	764.470431	14.668583
19.891900	763.481801	14.673600
19.544657	763.078789	14.678618
19.693064	756.781943	14.683635
19.611986	769.544335	14.688653
19.563504	782.866521	14.693671
19.932019	777.333605	14.698688
19.784561	785.356896	14.703706
19.859318	778.153237	14.708723
20.033583	781.821577	14.713741
19.994023	784.153793	14.718759
20.178578	789.729797	14.723776
19.859910	782.505727	14.728794
20.141197	777.952159	14.733811
19.583341	783.707598	14.738829
19.927277	790.281117	14.743847
20.075243	788.935818	14.748864
19.995584	790.936644	14.753882
19.774574	784.363151	14.758899
19.887366	780.120007	14.763917
19.916182	779.557087	14.768935
19.821095	785.855406	14.773952
19.899819	786.780527	14.778970
19.957603	787.393346	14.783987
20.001696	784.975563	14.789005
19.953364	794.570707	14.794023
20.445770	796.551331	14.799040
20.221491	803.797710	14.804058
20.474266	794.798889	14.809075
20.176203	790.484415	14.814093
19.957374	792.399749	14.819111
20.609514	807.739206	14.824128
20.345846	808.522313	14.829146
20.786871	805.966596	14.834163
20.645442	795.719871	14.839181
20.295650	783.492382	14.844199
20.368871	783.430592	14.849216
20.722090	788.573067	14.854234
20.451345	791.304426	14.859251
20.437255	784.673266	14.864269
20.307822	791.128447	14.869287
20.521269	792.894000	14.874304
20.099621	790.306191	14.879322
20.563436	799.139436	14.884339
20.572958	796.256850	14.889357
20.514542	813.812579	14.894375
20.876830	798.248254	14.899392
20.648594	792.206069	14.904410
20.924827	779.984639	14.909427
20.861116	779.429905	14.914445
20.388920	783.915905	14.919463
20.475287	780.904516	14.924480
20.475251	803.778119	14.929498
20.809772	809.267515	14.934515
21.081405	809.244066	14.939533
20.532389	816.377228	14.944551
20.911977	807.762477	14.949568
20.828001	817.110752	14.954586
20.973530	814.645514	14.959603
20.737479	804.312622	14.964621
20.583770	811.131379	14.969639
20.893674	807.813560	14.974656
20.521475	817.910744	14.979674
20.694172	810.581273	14.984691
20.714251	812.500202	14.989709
20.885176	817.068484	14.994727
20.790318	807.486647	14.999744
20.945239	818.577379	15.004762
21.030615	808.553888	15.009779
21.275156	811.955601	15.014797
20.650530	814.603554	15.019815
20.898096	815.167704	15.024832
20.627562	827.754692	15.029850
21.036550	828.662784	15.034867
21.266364	834.105476	15.039885
21.588094	835.623692	15.044903
21.467354	836.469613	15.049920
21.412758	839.959227	15.054938
21.595233	829.781655	15.059955
21.561552	831.705853	15.064973
21.367853	818.696484	15.069991
21.139012	810.650436	15.075008
21.192509	826.048990	15.080026
21.074792	828.989910	15.085043
21.573647	835.210966	15.090061
21.147098	839.210141	15.095079
21.527689	840.157397	15.100096
21.326099	839.933535	15.105114
21.403622	837.264352	15.110131
21.547006	834.161970	15.115149
21.328459	837.652024	15.120167
21.663607	832.894342	15.125184
21.449785	829.503941	15.130202
21.341330	834.696675	15.135219
21.064058	830.988008	15.140237
21.031595	833.902948	15.145255
21.447907	831.515203	15.150272
21.506220	855.702023	15.155290
21.662518	859.755051	15.160307
21.491616	863.048295	15.165325
21.832290	860.088568	15.170343
21.991719	858.094522	15.175360
22.007579	872.735301	15.180378
21.851030	856.747283	15.185395
21.868468	848.741526	15.190413
21.899116	846.657205	15.195431
22.075170	839.683805	15.200448
22.125648	832.635408	15.205466
22.264207	826.333769	15.210483
22.145774	833.702433	15.215501
21.838925	832.605119	15.220519
22.093262	826.269560	15.225536
22.119582	834.982020	15.230554
21.863590	834.974967	15.235571
22.263975	826.322235	15.240589
21.975480	830.921477	15.245607
21.964152	831.617711	15.250624
21.863526	832.286910	15.255642
21.806133	830.232163	15.260659
22.150333	830.288864	15.265677
21.860892	838.924566	15.270695
22.273184	835.369792	15.275712
22.009504	832.533162	15.280730
22.240984	843.425719	15.285747
22.230986	838.892528	15.290765
22.207820	860.693689	15.295783
22.306452	857.784508	15.300800
22.532063	850.004913	15.305818
22.075145	852.197400	15.310835
22.068951	846.265576	15.315853
21.817904	847.504302	15.320871
22.119821	846.242177	15.325888
22.812336	861.373382	15.330906
22.447482	862.771954	15.335923
22.558451	854.893553	15.340941
22.361901	858.294957	15.345959
22.231194	853.802766	15.350976
22.204228	847.435534	15.355994
22.307919	851.544141	15.361011
22.528338	849.221800	15.366029
22.499643	855.736961	15.371047
22.432142	853.765847	15.376064
22.653251	846.851658	15.381082
22.639471	855.876527	15.386099
22.690004	852.144898	15.391117
22.649533	862.938065	15.396135
22.862751	862.595561	15.401152
22.734633	860.848541	15.406170
22.465759	862.617087	15.411187
23.208881	871.630671	15.416205
22.936780	860.145202	15.421223
23.059675	854.117410	15.426240
22.894005	851.227550	15.431258
22.545374	854.662250	15.436275
22.999941	848.162766	15.441293
22.787372	858.755674	15.446311
22.847389	860.258092	15.451328
23.203558	858.867544	15.456346
23.052019	865.840617	15.461363
22.929059	864.701866	15.466381
23.309854	877.669682	15.471399
23.096583	861.823092	15.476416
23.026433	853.584901	15.481434
22.726312	854.664058	15.486451
23.113972	857.541579	15.491469
22.877817	874.399373	15.496487
23.197427	860.886665	15.501504
23.194629	865.725178	15.506522
23.196611	865.071785	15.511539
23.422306	859.482324	15.516557
23.254093	866.817775	15.521575
23.260163	864.844601	15.526592
23.628042	865.951642	15.531610
23.340049	869.544103	15.536627
23.673164	860.933453	15.541645
23.269201	866.226144	15.546663
23.406865	856.147097	15.551680
23.425401	861.367278	15.556698
23.563226	870.456765	15.561715
23.235639	857.714500	15.566733
23.300402	863.646970	15.571751
23.148775	863.727707	15.576768
23.464199	858.373500	15.581786
23.302094	866.771511	15.586803
23.567439	863.482755	15.591821
23.303930	861.157339	15.596839
23.391861	859.518481	15.601856
23.658999	857.141482	15.606874
23.388743	870.880338	15.611891
23.553402	858.641622	15.616909
23.385584	869.899718	15.621927
23.595408	867.781009	15.626944
23.735631	875.715085	15.631962
23.641059	889.975546	15.636979
24.004303	886.005564	15.641997
23.979100	890.033387	15.647015
23.596009	887.635184	15.652032
23.649635	884.786700	15.657050
23.852842	892.259630	15.662067
23.681567	887.944202	15.667085
23.676170	891.340909	15.672103
23.929285	887.025260	15.677120
24.128456	885.652997	15.682138
23.804736	890.661721	15.687155
24.270006	879.253215	15.692173
24.166346	897.339984	15.697191
24.572420	884.814113	15.702208
24.452463	884.091461	15.707226
24.372408	889.664773	15.712243
24.436728	887.489963	15.717261
24.196326	879.212163	15.722279
24.408790	889.590171	15.727296
24.247144	873.726014	15.732314
24.243030	876.485038	15.737331
24.302084	881.840890	15.742349
24.274569	878.714782	15.747367
24.168691	874.894045	15.752384
24.419099	873.851430	15.757402
24.222609	882.696654	15.762419
24.392365	878.043769	15.767437
24.324109	878.865690	15.772455
24.396982	873.076105	15.777472
24.489502	881.323774	15.782490
24.483377	878.465718	15.787507
24.412863	876.308879	15.792525
24.177868	885.062306	15.797543
24.302302	888.593308	15.802560
24.744180	876.210158	15.807578
24.412263	884.117226	15.812595
24.663807	878.877163	15.817613
24.508599	881.618836	15.822631
24.458703	880.418142	15.827648
24.675961	880.138122	15.832666
24.252002	886.011471	15.837683
24.357865	894.130822	15.842701
24.537790	900.622781	15.847719
24.508481	903.439406	15.852736
24.913497	903.739045	15.857754
24.497672	906.622542	15.862771
25.216515	906.380700	15.867789
24.733871	903.471067	15.872807
24.941575	910.735014	15.877824
25.033467	909.957077	15.882842
24.912607	911.683502	15.887859
24.903905	909.482260	15.892877
24.855149	900.218202	15.897895
25.039772	911.238065	15.902912
25.143246	894.578103	15.907930
25.299650	899.281227	15.912947
25.195437	908.194058	15.917965
25.180206	902.771721	15.922983
25.098934	901.784228	15.928000
25.360508	897.902758	15.933018
24.815183	901.055855	15.938035
25.174579	900.715695	15.943053
25.360350	895.517491	15.948071
25.055286	900.905152	15.953088
25.519476	903.871677	15.958106
25.393910	901.729772	15.963123
25.590744	898.180342	15.968141
25.635069	900.868663	15.973159
25.091806	905.037621	15.978176
25.332270	902.469133	15.983194
25.146873	906.689318	15.988211
25.275196	903.513543	15.993229
25.692801	909.482265	15.998247
25.240644	904.709061	16.003264
25.559079	913.255869	16.008282
25.368389	932.987883	16.013299
25.703700	933.913835	16.018317
25.874924	926.969561	16.023335
25.658181	928.556374	16.028352
26.017983	928.263487	16.033370
25.667290	927.671660	16.038387
25.972499	930.546332	16.043405
25.883542	931.220018	16.048423
25.638208	917.382366	16.053440
25.892748	910.863707	16.058458
25.919426	912.008431	16.063475
25.935966	901.730582	16.068493
25.714283	909.128078	16.073511
25.811765	924.371501	16.078528
26.088985	921.970823	16.083546
26.131752	933.558888	16.088563
26.034761	924.384427	16.093581
26.132225	930.453809	16.098599
26.064876	926.892115	16.103616
26.134610	923.526697	16.108634
25.821864	924.358524	16.113651
26.005759	926.340163	16.118669
26.352563	929.555461	16.123687
25.913746	923.158056	16.128704
26.062725	917.438584	16.133722
25.686006	921.780269	16.138739
25.622998	926.883857	16.143757
26.018623	915.344226	16.148775
25.894206	920.968681	16.153792
26.216547	932.844305	16.158810
26.391914	942.672727	16.163827
26.615488	949.470294	16.168845
26.668678	940.212332	16.173863
26.377801	929.218918	16.178880
26.425824	923.868717	16.183898
26.171448	918.262936	16.188915
26.248396	939.878091	16.193933
26.884824	939.346200	16.198951
26.803100	945.686663	16.203968
26.769773	933.620929	16.208986
26.529582	929.628717	16.214003
26.440607	916.842712	16.219021
26.734552	935.179652	16.224039
26.667228	936.493742	16.229056
27.044677	938.391407	16.234074
26.663260	930.492288	16.239091
26.705729	926.613583	16.244109
26.923909	919.781876	16.249127
26.790515	920.658187	16.254144
26.384616	920.816634	16.259162
26.688746	934.418206	16.264179
26.917895	939.917841	16.269197
27.209651	937.789443	16.274215
26.895470	935.061695	16.279232
27.015658	944.520061	16.284250
26.945367	941.915049	16.289267
26.737554	940.202599	16.294285
26.986827	942.508516	16.299303
27.018774	938.470508	16.304320
26.871677	939.336343	16.309338
26.832713	939.187986	16.314355
26.842386	945.214323	16.319373
26.858312	936.164177	16.324391
26.535895	941.343127	16.329408
27.253995	950.313334	16.334426
27.441710	962.648736	16.339443
27.436746	965.180685	16.344461
27.863839	958.391972	16.349479
27.365662	953.550225	16.354496
27.237582	941.657125	16.359514
27.602127	952.443693	16.364531
27.073142	952.249035	16.369549
27.229598	956.636580	16.374567
27.413398	965.236066	16.379584
27.367661	957.644108	16.384602
27.566878	965.395410	16.389619
27.511893	973.300153	16.394637
27.913540	955.719244	16.399655
27.630594	964.199351	16.404672
27.724370	958.371749	16.409690
27.414276	956.463880	16.414707
27.243391	960.785948	16.419725
27.522775	955.986477	16.424743
27.615910	957.865573	16.429760
27.777836	957.739391	16.434778
27.931196	961.682447	16.439795
27.888609	961.711386	16.444813
28.038764	955.998030	16.449831
27.776356	962.167989	16.454848
27.961181	955.653925	16.459866
28.145970	962.918328	16.464883
27.972173	960.212764	16.469901
27.914828	964.911525	16.474919
27.531128	964.359583	16.479936
27.844965	971.830992	16.484954
28.139469	968.064270	16.489971
28.287266	982.703403	16.494989
28.375150	963.600028	16.500007
27.913235	963.767252	16.505024
27.937045	966.364123	16.510042
28.728429	976.133916	16.515059
28.284956	969.184948	16.520077
28.612999	960.240525	16.525095
28.424225	957.928633	16.530112
28.138257	960.671870	16.535130
28.299610	961.691352	16.540147
27.935696	963.973424	16.545165
28.245364	963.505352	16.550183
28.407048	984.640219	16.555200
28.454110	980.356832	16.560218
28.702701	991.742270	16.565235
28.392195	988.086116	16.570253
28.682461	984.443132	16.575271
28.837871	991.996178	16.580288
28.547731	993.657613	16.585306
28.511460	982.125648	16.590323
28.459564	988.777039	16.595341
28.836462	989.428231	16.600359
28.099274	980.054240	16.605376
28.224833	992.263698	16.610394
28.619440	990.052906	16.615411
28.520228	982.317835	16.620429
28.907403	981.263253	16.625447
28.881857	991.546066	16.630464
28.623953	979.922593	16.635482
29.008436	971.830870	16.640499
28.800622	980.826242	16.645517
29.054187	974.124673	16.650535
29.083498	980.069048	16.655552
28.921456	969.273177	16.660570
29.067170	980.583207	16.665587
28.863242	995.514148	16.670605
29.180512	998.907659	16.675623
29.412193	1004.274371	16.680640
29.222956	1008.886509	16.685658
29.398490	992.256192	16.690675
29.308476	991.399453	16.695693
29.165420	973.256919	16.700711
29.152523	983.515654	16.705728
29.326492	995.073735	16.710746
29.352619	999.677375	16.715763
29.399265	1003.722369	16.720781
29.564717	1001.474894	16.725799
29.766978	1002.071396	16.730816
29.624553	998.729738	16.735834
29.262237	979.819962	16.740851
29.297238	984.239168	16.745869
29.748994	994.100054	16.750887
29.701287	994.944007	16.755904
29.316352	1005.636593	16.760922
29.863091	995.379763	16.765939
29.662696	1000.886756	16.770957
29.489753	1005.035585	16.775975
29.439066	998.776159	16.780992
29.691218	1004.111261	16.786010
29.787529	999.854868	16.791027
29.460345	1005.776210	16.796045
29.837494	1002.716069	16.801063
29.876673	1002.419767	16.806080
29.988463	1005.545666	16.811098
30.073822	999.634161	16.816115
29.809547	1005.034398	16.821133
29.596553	1003.183895	16.826151
29.952312	995.570041	16.831168
29.636966	991.094120	16.836186
29.782112	994.760756	16.841203
29.643025	1014.087136	16.846221
30.235732	1020.056863	16.851239
30.145686	1027.402224	16.856256
30.336662	1022.297844	16.861274
30.239988	1024.692690	16.866291
30.130436	1022.646094	16.871309
30.596208	1022.683748	16.876327
30.481926	1031.165863	16.881344
30.668523	1027.324515	16.886362
30.382471	1021.231350	16.891379
30.302661	1011.104236	16.896397
30.717958	1019.137292	16.901415
30.194812	1009.818113	16.906432
30.018264	1008.539423	16.911450
30.293827	1017.815690	16.916467
30.076205	1028.649337	16.921485
30.221002	1016.735522	16.926503
30.253448	1017.910908	16.931520
30.034872	1030.221649	16.936538
30.804753	1025.613558	16.941555
30.629901	1046.214234	16.946573
30.701754	1042.684357	16.951591
31.337069	1039.908815	16.956608
30.809024	1031.388827	16.961626
30.425831	1023.600401	16.966643
30.537224	1037.585707	16.971661
30.946209	1042.823663	16.976679
31.213753	1044.580765	16.981696
30.902327	1047.040820	16.986714
30.970515	1047.412172	16.991731
31.058640	1051.176117	16.996749
31.069826	1042.183466	17.001767
31.027141	1051.831513	17.006784
30.959999	1054.489984	17.011802
31.386329	1048.386182	17.016819
31.063786	1041.165769	17.021837
31.201506	1038.480813	17.026855
31.281684	1040.576547	17.031872
31.220123	1043.426650	17.036890
31.416053	1039.552279	17.041907
31.141435	1035.006848	17.046925
30.914205	1043.206859	17.051943
31.174476	1038.091618	17.056960
31.110856	1037.776707	17.061978
31.141506	1036.762202	17.066995
31.138216	1040.228037	17.072013
31.344552	1046.813743	17.077031
31.773028	1052.054960	17.082048
31.788554	1049.802567	17.087066
31.799350	1035.164128	17.092083
31.896364	1033.785768	17.097101
31.492226	1029.115463	17.102119
31.677462	1029.926076	17.107136
31.373540	1039.649762	17.112154
31.767897	1034.308382	17.117171
31.647881	1054.900477	17.122189
31.983687	1052.288627	17.127207
31.861671	1053.746997	17.132224
32.203057	1062.463854	17.137242
32.070247	1036.676127	17.142259
31.977109	1028.785446	17.147277
32.069504	1020.155630	17.152295
32.257408	1022.483797	17.157312
31.984400	1027.566666	17.162330
31.962603	1020.927158	17.167347
31.974054	1023.825780	17.172365
32.033940	1017.672102	17.177383
32.138053	1029.297956	17.182400
32.300320	1045.632731	17.187418
32.375391	1030.526624	17.192435
32.366608	1032.983441	17.197453
32.862991	1016.577390	17.202471
32.563009	1014.563787	17.207488
32.281234	1023.043739	17.212506
32.537433	1011.295514	17.217523
32.221141	1019.200194	17.222541
32.117747	1020.684046	17.227559
31.704344	1007.125126	17.232576
32.205684	1030.062478	17.237594
32.433482	1028.212339	17.242611
32.796787	1042.997641	17.247629
32.878261	1045.714879	17.252647
33.055664	1045.485283	17.257664
32.563092	1036.906085	17.262682
32.883500	1017.327555	17.267699
32.542051	1017.071954	17.272717
32.681374	1032.817009	17.277735
32.741003	1041.098309	17.282752
32.607686	1037.742593	17.287770
32.670328	1031.859883	17.292787
32.794900	1033.197564	17.297805
32.550339	1042.214503	17.302823
32.990809	1045.105872	17.307840
32.336609	1053.281264	17.312858
33.023055	1048.493732	17.317875
32.909193	1051.206861	17.322893
32.902282	1045.423408	17.327911
33.016433	1041.473485	17.332928
32.818823	1045.689305	17.337946
33.007046	1051.021814	17.342963
33.022344	1064.861249	17.347981
33.091261	1069.988389	17.352999
33.194094	1066.400003	17.358016
33.228287	1074.148805	17.363034
33.207801	1071.741102	17.368051
33.256541	1069.243656	17.373069
33.047213	1079.545847	17.378087
33.433982	1058.543042	17.383104
33.154238	1068.957248	17.388122
33.323177	1059.311852	17.393139
33.294236	1062.889010	17.398157
33.426851	1081.983541	17.403175
33.733555	1078.893398	17.408192
33.509652	1093.499340	17.413210
34.027178	1088.785601	17.418227
33.993176	1090.062922	17.423245
33.861875	1082.029871	17.428263
33.690676	1054.626013	17.433280
33.630961	1081.627735	17.438298
34.302443	1068.864488	17.443315
33.892268	1068.761668	17.448333
33.912246	1068.957533	17.453351
34.171108	1065.597171	17.458368
33.586654	1062.785515	17.463386
34.069796	1070.296713	17.468403
34.101094	1068.199640	17.473421
34.221043	1086.497725	17.478439
34.133045	1077.533219	17.483456
33.967835	1079.061476	17.488474
33.764061	1089.391205	17.493491
34.039844	1081.960263	17.498509
34.441607	1076.810218	17.503527
34.091232	1084.761293	17.508544
33.988653	1079.472512	17.513562
34.239580	1083.842132	17.518579
34.075198	1069.578258	17.523597
33.975220	1080.077916	17.528615
34.079710	1082.599044	17.533632
34.303488	1094.146230	17.538650
34.890872	1099.652904	17.543667
35.040565	1107.083815	17.548685
34.724927	1103.819770	17.553703
34.743282	1080.274218	17.558720
34.575739	1082.825345	17.563738
34.531200	1071.761687	17.568755
34.594386	1074.002101	17.573773
34.320134	1077.068575	17.578791
34.668976	1080.305673	17.583808
34.252690	1089.639882	17.588826
34.841843	1097.604708	17.593843
34.702638	1100.239762	17.598861
35.066109	1100.779451	17.603879
35.111154	1099.677479	17.608896
34.823121	1098.391002	17.613914
34.729589	1099.210581	17.618931
34.866124	1094.401896	17.623949
34.733800	1097.411421	17.628967
35.198353	1097.982610	17.633984
35.010873	1098.210980	17.639002
35.014135	1091.359232	17.644019
35.143830	1094.876827	17.649037
35.125967	1104.142308	17.654055
35.481633	1110.228103	17.659072
35.483125	1121.907966	17.664090
35.541782	1111.358303	17.669107
35.400521	1106.110289	17.674125
35.186318	1106.024103	17.679143
35.637206	1119.574420	17.684160
35.655795	1130.260662	17.689178
35.549325	1116.044484	17.694195
35.810801	1115.814339	17.699213
35.511054	1115.463837	17.704231
35.372037	1098.229437	17.709248
35.595810	1120.285721	17.714266
35.933348	1117.648343	17.719283
35.829895	1125.027404	17.724301
35.394233	1126.414998	17.729319
35.836584	1119.346117	17.734336
35.735721	1120.261522	17.739354
35.871690	1123.869660	17.744371
36.055664	1127.852140	17.749389
36.045843	1121.892389	17.754407
35.982204	1112.614772	17.759424
36.021548	1126.128587	17.764442
35.824978	1121.189044	17.769459
36.371119	1126.727436	17.774477
36.050509	1118.837641	17.779495
36.141915	1116.901562	17.784512
35.969327	1120.971465	17.789530
35.938012	1125.012922	17.794547
36.464711	1117.173414	17.799565
36.214030	1121.287111	17.804583
36.420481	1118.013848	17.809600
36.465647	1116.242808	17.814618
36.232257	1117.472475	17.819635
36.208942	1115.794218	17.824653
36.224474	1121.027570	17.829671
36.552638	1136.926171	17.834688
36.302726	1138.859034	17.839706
36.628191	1140.878478	17.844723
36.612499	1137.876708	17.849741
36.805378	1148.254780	17.854759
36.685331	1142.558451	17.859776
36.692598	1142.046235	17.864794
36.711560	1130.350881	17.869811
37.028383	1132.093960	17.874829
36.835424	1142.207425	17.879847
36.802699	1136.216543	17.884864
37.251321	1140.599385	17.889882
37.051141	1147.375056	17.894899
37.109721	1142.550169	17.899917
36.772696	1140.286728	17.904935
36.821634	1130.969372	17.909952
36.969420	1144.144310	17.914970
36.959658	1138.279221	17.919987
37.051267	1140.007093	17.925005
36.939645	1142.091863	17.930023
37.009951	1137.590196	17.935040
37.113884	1147.439391	17.940058
37.071059	1146.228104	17.945075
37.107317	1144.493172	17.950093
36.995555	1149.642332	17.955111
37.220380	1152.248761	17.960128
37.327303	1152.263743	17.965146
37.116874	1157.904904	17.970163
37.311871	1148.198572	17.975181
37.465162	1150.150316	17.980199
37.328080	1140.609630	17.985216
37.311258	1155.290477	17.990234
37.423065	1166.100995	17.995251
37.625205	1165.883301	18.000269
37.674644	1180.411772	18.005287
37.935528	1173.873089	18.010304
38.120422	1170.237110	18.015322
37.960418	1174.412354	18.020339
38.046954	1167.437072	18.025357
38.058017	1178.825131	18.030375
38.155410	1175.411150	18.035392
38.670910	1171.347822	18.040410
38.047073	1169.094599	18.045427
38.389994	1163.410936	18.050445
38.141315	1157.731601	18.055463
38.265709	1165.216994	18.060480
38.234129	1160.147445	18.065498
38.356257	1161.668561	18.070515
38.565664	1162.342846	18.075533
38.378583	1147.631174	18.080551
38.559012	1142.859781	18.085568
38.526821	1131.731033	18.090586
38.316745	1136.021413	18.095603
38.189620	1131.411822	18.100621
38.427417	1146.415695	18.105639
38.587791	1160.977264	18.110656
38.790281	1170.987760	18.115674
38.654222	1169.466021	18.120691
38.691362	1163.827112	18.125709
38.296956	1169.437139	18.130727
38.349483	1168.580150	18.135744
38.736891	1167.310921	18.140762
38.482140	1166.278007	18.145779
38.882241	1167.468384	18.150797
38.488662	1167.782697	18.155815
38.501373	1168.591945	18.160832
38.805077	1177.513583	18.165850
38.653742	1192.193445	18.170867
39.215208	1191.515498	18.175885
39.045258	1187.736291	18.180903
38.735489	1187.927016	18.185920
39.066356	1182.365160	18.190938
38.908400	1192.937085	18.195955
39.212019	1189.822160	18.200973
39.157537	1193.501178	18.205991
39.358696	1192.680863	18.211008
39.310093	1187.601349	18.216026
39.224430	1199.667314	18.221043
39.413468	1205.094419	18.226061
39.575122	1209.815738	18.231079
39.855220	1211.548800	18.236096
39.870166	1197.177829	18.241114
39.611005	1190.395562	18.246131
39.669348	1177.693589	18.251149
39.919312	1179.933155	18.256167
39.627941	1187.022939	18.261184
40.021875	1178.917019	18.266202
39.456329	1195.874063	18.271219
39.085094	1187.269469	18.276237
39.646052	1193.392557	18.281255
39.741231	1207.260613	18.286272
39.983186	1206.026794	18.291290
40.059823	1212.213148	18.296307
40.354167	1211.371919	18.301325
40.116158	1215.833957	18.306343
39.816519	1215.253055	18.311360
40.081630	1204.551067	18.316378
39.716956	1204.882942	18.321395
40.148678	1197.670524	18.326413
40.241875	1214.644299	18.331431
40.272867	1201.381688	18.336448
40.279408	1202.535897	18.341466
40.195174	1206.601443	18.346483
40.287006	1210.456363	18.351501
40.320555	1221.638948	18.356519
40.642403	1231.548724	18.361536
40.725978	1231.996567	18.366554
40.597661	1224.843481	18.371571
40.592240	1224.860286	18.376589
40.791166	1226.151617	18.381607
40.542577	1235.065139	18.386624
40.674491	1224.728001	18.391642
40.817169	1224.134604	18.396659
41.039507	1222.941728	18.401677
41.099642	1220.363578	18.406695
41.031326	1224.079485	18.411712
41.336386	1221.302010	18.416730
40.793450	1234.585235	18.421747
41.280622	1221.645624	18.426765
41.327415	1226.902512	18.431783
41.022544	1229.715024	18.436800
41.177429	1223.559015	18.441818
41.116061	1223.445726	18.446835
41.054092	1219.608567	18.451853
41.162292	1222.214344	18.456871
41.077295	1218.809995	18.461888
41.249371	1217.896402	18.466906
41.174878	1224.327352	18.471923
41.109297	1215.078390	18.476941
41.337701	1215.888561	18.481959
41.176158	1222.279498	18.486976
41.090921	1227.923158	18.491994
41.292836	1242.942202	18.497011
41.180699	1243.695273	18.502029
41.210210	1242.605193	18.507047
41.195984	1251.450445	18.512064
41.872477	1246.923205	18.517082
41.788697	1255.435363	18.522099
41.877286	1251.855484	18.527117
41.883803	1246.631614	18.532135
42.074359	1266.165403	18.537152
42.209736	1258.970988	18.542170
42.118554	1260.651769	18.547187
41.999614	1257.659844	18.552205
42.222340	1257.407366	18.557223
41.989902	1261.433027	18.562240
42.549258	1259.638217	18.567258
41.986308	1248.898678	18.572275
42.394918	1260.716823	18.577293
42.438133	1257.279756	18.582311
42.108387	1262.715575	18.587328
42.224228	1253.895774	18.592346
42.376330	1263.374557	18.597363
42.534518	1259.395595	18.602381
42.908655	1261.123395	18.607399
42.594267	1262.829680	18.612416
42.587291	1258.674618	18.617434
42.755480	1262.754278	18.622451
42.439930	1254.147239	18.627469
42.655174	1259.649152	18.632487
42.738106	1258.815798	18.637504
43.004984	1251.010628	18.642522
42.663827	1253.134530	18.647539
42.891702	1253.294669	18.652557
42.935311	1258.495259	18.657575
42.582064	1255.454835	18.662592
42.898758	1260.685225	18.667610
42.773327	1260.821822	18.672627
42.571112	1257.091838	18.677645
42.541566	1261.877843	18.682663
42.505110	1280.481508	18.687680
42.977172	1285.135278	18.692698
42.967719	1281.220447	18.697715
43.042627	1282.083074	18.702733
43.370307	1276.483817	18.707751
43.131363	1284.307064	18.712768
43.591024	1289.344643	18.717786
43.289123	1301.204707	18.722803
43.745795	1290.374820	18.727821
43.914065	1301.148170	18.732839
43.578337	1302.264491	18.737856
44.030417	1294.834242	18.742874
43.954710	1286.555694	18.747891
43.562021	1276.288096	18.752909
43.772172	1268.201463	18.757927
43.752963	1289.582792	18.762944
44.371689	1289.009484	18.767962
43.886592	1275.489995	18.772979
43.639254	1280.395338	18.777997
44.203920	1290.481704	18.783015
44.111362	1291.058134	18.788032
44.229680	1291.210191	18.793050
44.136834	1292.146441	18.798067
44.004267	1290.703043	18.803085
44.433307	1291.443911	18.808103
44.265157	1285.982299	18.813120
44.140714	1287.352703	18.818138
44.530472	1291.687999	18.823155
44.514448	1292.561717	18.828173
44.715101	1285.480145	18.833191
44.387645	1293.184715	18.838208
44.414757	1278.900138	18.843226
44.077254	1281.635718	18.848243
44.381992	1280.581412	18.853261
44.371502	1274.672210	18.858279
44.293908	1288.374888	18.863296
44.422281	1295.834466	18.868314
44.902678	1299.675864	18.873331
44.970533	1304.364566	18.878349
44.915953	1308.879941	18.883367
44.852572	1311.720905	18.888384
44.901621	1313.966720	18.893402
45.020265	1319.894057	18.898419
44.696387	1314.655658	18.903437
44.782694	1310.287145	18.908455
44.727352	1311.185960	18.913472
44.894720	1307.486426	18.918490
45.199536	1307.565080	18.923507
45.018095	1316.474435	18.928525
45.366415	1320.364934	18.933543
45.308211	1337.911677	18.938560
45.665801	1333.759441	18.943578
45.714433	1331.056840	18.948595
45.581278	1331.428185	18.953613
45.874276	1310.162057	18.958631
45.337390	1310.249506	18.963648
45.277379	1313.632760	18.968666
45.641290	1331.539410	18.973683
45.795074	1337.016262	18.978701
45.883745	1329.633469	18.983719
45.691178	1340.229840	18.988736
45.915766	1328.334876	18.993754
45.863861	1331.142485	18.998771
45.816105	1326.078579	19.003789
45.936245	1336.726943	19.008807
46.124261	1330.502588	19.013824
45.755096	1327.584571	19.018842
45.994807	1334.711129	19.023859
45.807527	1332.376862	19.028877
46.127148	1323.196883	19.033895
45.603074	1338.998810	19.038912
46.442066	1352.867209	19.043930
46.716552	1356.204374	19.048947
46.591879	1358.676237	19.053965
46.650197	1358.234914	19.058983
46.639457	1361.607301	19.064000
46.583562	1360.612649	19.069018
46.564036	1348.569720	19.074035
46.388114	1353.508076	19.079053
46.628852	1350.440846	19.084071
46.867895	1351.407153	19.089088
46.914507	1350.175527	19.094106
46.816807	1343.254290	19.099123
46.574490	1349.462262	19.104141
46.777046	1352.072209	19.109159
46.727034	1351.736225	19.114176
46.833992	1345.265779	19.119194
47.148146	1346.592716	19.124211
46.978030	1346.344980	19.129229
47.049302	1343.130727	19.134247
47.130432	1353.614793	19.139264
46.912383	1369.763290	19.144282
47.061692	1367.698187	19.149299
46.926276	1372.377728	19.154317
47.221518	1372.546249	19.159335
47.067782	1374.022238	19.164352
47.196531	1384.590384	19.169370
47.392725	1381.719483	19.174387
47.430081	1400.927115	19.179405
47.911929	1397.812633	19.184423
48.074510	1401.549207	19.189440
47.658201	1389.880854	19.194458
47.964320	1385.648304	19.199475
47.862048	1395.365835	19.204493
48.147078	1385.329675	19.209511
47.600770	1382.401532	19.214528
47.869861	1380.036783	19.219546
48.059681	1382.418348	19.224563
47.653564	1389.138010	19.229581
48.184994	1381.537497	19.234599
47.854979	1389.419241	19.239616
47.626412	1387.189269	19.244634
47.964817	1384.144603	19.249651
48.098832	1385.035845	19.254669
48.184332	1374.573343	19.259687
48.152454	1399.229486	19.264704
48.386888	1415.414431	19.269722
48.733389	1400.893516	19.274739
48.692539	1412.646478	19.279757
48.809779	1399.752074	19.284775
48.315284	1404.150199	19.289792
48.530280	1399.663668	19.294810
48.918424	1401.247271	19.299827
48.643052	1404.585385	19.304845
48.944838	1405.595516	19.309863
48.926335	1410.354583	19.314880
48.680559	1405.268029	19.319898
48.533767	1403.994115	19.324915
48.946129	1398.053335	19.329933
49.110277	1400.372651	19.334951
49.238456	1407.582987	19.339968
49.087627	1395.532194	19.344986
48.990508	1392.587322	19.350003
49.077302	1391.317839	19.355021
49.362667	1393.681279	19.360039
49.207950	1395.403587	19.365056
48.966339	1393.554370	19.370074
49.599624	1405.451024	19.375091
49.619166	1425.156955	19.380109
49.713872	1414.491008	19.385127
49.877128	1420.951053	19.390144
49.483794	1425.658394	19.395162
49.828929	1418.371088	19.400179
49.464815	1424.187896	19.405197
50.029382	1412.226986	19.410215
50.038471	1425.849913	19.415232
49.616734	1423.959484	19.420250
49.991573	1419.596234	19.425267
50.115780	1418.901578	19.430285
50.258290	1417.159441	19.435303
50.014583	1415.856527	19.440320
50.046216	1422.734843	19.445338
50.508406	1414.394052	19.450355
50.105738	1414.204841	19.455373
50.464427	1408.726923	19.460391
50.450799	1409.950580	19.465408
50.558601	1408.649400	19.470426
50.690160	1397.750461	19.475443
50.354188	1409.612779	19.480461
50.634036	1403.736943	19.485479
50.828004	1412.821066	19.490496
50.693928	1408.603828	19.495514
50.915400	1398.025331	19.500531
50.859793	1411.872987	19.505549
50.771458	1409.567391	19.510567
51.278099	1402.936469	19.515584
51.056837	1406.436526	19.520602
51.447176	1400.855817	19.525619
51.261138	1399.455503	19.530637
51.013449	1393.690726	19.535655
51.205627	1397.144941	19.540672
51.087804	1398.549031	19.545690
51.386576	1400.238159	19.550707
51.061852	1398.171580	19.555725
51.160588	1398.080544	19.560743
51.157597	1405.447136	19.565760
51.157319	1400.533567	19.570778
51.284851	1396.616184	19.575795
51.219859	1405.030792	19.580813
51.476032	1401.307857	19.585831
51.425457	1405.522816	19.590848
51.453149	1407.216545	19.595866
51.528476	1394.609590	19.600883
51.399007	1407.310589	19.605901
51.483159	1410.683898	19.610919
51.813791	1419.128049	19.615936
51.807943	1425.352648	19.620954
51.802124	1419.524720	19.625971
51.838149	1427.901420	19.630989
51.607674	1416.838276	19.636007
51.604419	1423.662096	19.641024
51.571439	1424.816200	19.646042
51.579381	1447.802992	19.651059
51.888737	1437.964971	19.656077
52.104623	1439.632374	19.661095
52.031836	1439.643954	19.666112
52.219795	1457.751875	19.671130
52.452286	1459.839575	19.676147
52.316122	1478.645268	19.681165
52.914547	1475.670305	19.686183
52.902888	1469.313077	19.691200
52.770984	1468.674327	19.696218
53.126024	1467.719431	19.701235
52.942165	1479.308643	19.706253
52.765907	1465.200954	19.711271
53.071707	1466.548145	19.716288
52.726370	1465.002363	19.721306
53.118657	1460.456480	19.726323
53.059807	1472.865582	19.731341
53.375988	1474.444688	19.736359
52.730671	1471.147016	19.741376
52.907934	1469.948563	19.746394
52.987451	1463.744317	19.751411
53.002368	1468.924216	19.756429
52.961728	1470.189981	19.761447
53.300645	1472.778582	19.766464
53.735596	1488.941647	19.771482
53.720374	1481.997966	19.776499
53.348609	1474.826115	19.781517
53.146074	1480.497699	19.786535
53.623105	1484.901424	19.791552
53.507131	1494.813669	19.796570
53.661070	1496.566526	19.801587
53.818742	1492.565501	19.806605
53.774279	1493.980197	19.811623
54.002858	1492.543318	19.816640
54.010658	1502.960062	19.821658
54.089745	1493.331667	19.826675
54.191555	1489.882218	19.831693
54.006797	1496.841806	19.836711
54.339876	1491.402590	19.841728
53.805776	1497.867776	19.846746
54.232825	1502.203594	19.851763
54.529615	1508.295595	19.856781
54.398822	1515.284606	19.861799
54.566940	1511.815297	19.866816
54.476445	1515.537895	19.871834
54.465443	1519.219636	19.876851
54.469235	1514.090794	19.881869
54.640432	1513.887413	19.886887
54.736726	1495.978258	19.891904
54.602459	1507.774322	19.896922
54.570334	1505.289485	19.901939
54.373606	1508.555334	19.906957
54.746734	1528.625721	19.911975
54.948450	1528.007285	19.916992
54.674054	1539.446611	19.922010
54.838083	1529.801731	19.927027
55.266959	1528.346091	19.932045
54.841027	1534.608142	19.937063
55.298279	1522.026470	19.942080
55.385051	1527.447604	19.947098
55.257816	1532.675041	19.952115
55.660568	1528.203245	19.957133
55.653645	1536.151203	19.962151
55.722189	1526.830569	19.967168
55.863358	1538.274215	19.972186
55.391710	1523.720432	19.977203
55.918985	1528.753798	19.982221
55.669013	1531.185353	19.987239
56.291725	1539.852056	19.992256
55.724114	1536.854637	19.997274
56.111895	1523.340217	20.002291
55.985377	1523.063555	20.007309
56.049259	1539.562528	20.012327
56.405571	1542.716486	20.017344
55.743400	1547.832070	20.022362
56.094961	1549.348832	20.027379
56.268211	1548.684360	20.032397
56.005786	1544.102172	20.037415
56.310392	1536.922159	20.042432
55.923785	1548.502153	20.047450
56.154652	1544.420218	20.052467
56.372825	1553.090346	20.057485
56.339252	1571.924248	20.062503
56.708688	1571.752926	20.067520
56.516473	1567.273347	20.072538
56.896714	1566.270315	20.077555
56.968908	1570.002151	20.082573
57.034789	1567.293656	20.087591
57.189131	1563.103780	20.092608
57.176751	1569.540902	20.097626
57.392569	1569.213760	20.102643
57.621009	1556.279730	20.107661
57.299655	1559.662948	20.112679
57.230822	1561.617980	20.117696
57.117489	1561.317160	20.122714
57.278490	1555.377841	20.127731
57.244998	1564.194707	20.132749
57.290078	1553.391277	20.137767
57.627322	1549.488344	20.142784
57.554906	1554.965988	20.147802
57.182065	1558.928502	20.152819
57.234378	1563.436662	20.157837
57.016390	1574.728309	20.162855
57.480234	1587.317542	20.167872
57.444205	1588.569969	20.172890
57.500463	1600.181600	20.177907
57.896975	1606.270635	20.182925
57.509939	1612.488746	20.187943
58.191114	1606.205965	20.192960
57.882445	1607.778835	20.197978
58.212454	1609.349474	20.202995
58.259703	1598.280577	20.208013
58.210091	1598.850288	20.213031
58.355063	1597.978794	20.218048
58.425776	1602.746026	20.223066
58.544267	1610.279871	20.228083
59.042194	1614.904429	20.233101
58.793781	1615.495820	20.238119
59.033763	1608.616253	20.243136
58.477700	1591.718130	20.248154
59.153091	1597.653009	20.253171
59.161347	1595.591044	20.258189
58.660313	1589.452466	20.263207
58.694907	1591.053608	20.268224
59.207599	1611.777600	20.273242
58.983415	1612.106405	20.278259
59.720926	1620.834061	20.283277
59.044731	1604.920475	20.288295
59.478844	1605.433333	20.293312
59.040113	1601.500479	20.298330
59.180127	1614.402413	20.303347
59.165440	1611.744407	20.308365
59.279166	1611.029295	20.313383
59.935034	1611.886126	20.318400
59.836882	1618.279897	20.323418
59.384170	1623.886576	20.328435
59.539001	1614.009550	20.333453
59.584628	1612.610794	20.338471
59.594687	1617.441185	20.343488
59.754778	1608.825727	20.348506
59.686279	1617.607076	20.353523
60.099437	1623.617765	20.358541
60.204837	1633.343916	20.363559
60.278438	1634.263572	20.368576
60.248303	1637.437068	20.373594
60.315468	1635.375337	20.378611
60.385689	1628.061587	20.383629
60.228002	1646.416369	20.388647
60.506337	1629.882968	20.393664
60.664315	1633.850699	20.398682
60.542929	1639.585363	20.403699
60.685985	1635.264687	20.408717
60.771457	1639.007081	20.413735
60.825291	1637.474486	20.418752
60.763943	1639.665052	20.423770
60.817361	1635.323705	20.428787
60.942684	1626.625318	20.433805
61.024096	1634.632067	20.438823
60.911938	1622.979027	20.443840
61.134186	1622.224820	20.448858
60.967025	1628.465295	20.453875
61.393881	1640.716360	20.458893
61.343463	1642.255083	20.463911
61.433993	1647.233829	20.468928
61.044684	1656.485205	20.473946
61.281761	1658.417567	20.478963
61.687599	1657.438924	20.483981
61.338196	1664.850429	20.488999
61.553045	1655.759284	20.494016
61.534729	1651.145134	20.499034
61.218245	1658.914417	20.504051
61.418548	1657.706029	20.509069
61.454310	1675.396181	20.514087
61.569626	1673.431048	20.519104
61.373938	1683.387447	20.524122
61.626122	1685.740346	20.529139
61.787749	1701.690792	20.534157
61.975079	1705.865392	20.539175
61.985133	1707.921695	20.544192
62.528415	1704.112687	20.549210
62.270959	1707.785741	20.554227
62.748131	1697.170161	20.559245
62.645202	1705.404651	20.564263
62.582265	1701.561228	20.569280
62.471017	1703.295690	20.574298
62.723510	1697.537659	20.579315
62.918038	1689.888810	20.584333
62.970511	1699.863145	20.589351
63.098879	1699.003716	20.594368
63.037899	1697.457545	20.599386
62.731513	1699.162616	20.604403
63.235948	1718.856019	20.609421
63.048472	1723.950930	20.614439
63.424990	1717.993570	20.619456
63.635028	1714.031633	20.624474
63.705183	1717.347228	20.629491
63.774948	1695.522293	20.634509
63.574678	1687.215735	20.639527
63.526225	1688.678411	20.644544
63.525079	1683.786992	20.649562
63.356096	1686.597220	20.654579
63.305006	1697.190571	20.659597
63.522268	1702.556598	20.664615
63.937106	1703.508007	20.669632
63.982534	1714.935207	20.674650
63.560379	1714.032635	20.679667
63.972781	1707.861362	20.684685
63.760133	1712.527843	20.689703
63.959783	1712.417839	20.694720
64.116904	1717.676522	20.699738
63.782963	1728.216372	20.704755
63.938809	1727.027570	20.709773
64.251279	1724.495024	20.714791
64.102018	1733.491067	20.719808
64.275132	1725.400564	20.724826
64.193657	1734.853073	20.729843
64.742936	1738.772144	20.734861
64.794330	1748.762455	20.739879
64.828199	1751.600875	20.744896
65.192622	1747.349638	20.749914
64.895776	1757.173594	20.754931
64.712091	1747.614636	20.759949
65.102007	1749.358950	20.764967
65.323830	1747.320315	20.769984
64.973538	1736.575564	20.775002
64.642374	1745.843124	20.780019
65.160411	1738.342397	20.785037
65.102524	1745.604114	20.790055
65.300474	1764.534495	20.795072
65.388576	1772.660186	20.800090
65.415718	1769.673691	20.805107
65.936114	1764.312349	20.810125
65.707440	1766.538614	20.815143
65.426304	1765.292034	20.820160
66.112055	1758.910648	20.825178
65.796279	1770.602771	20.830195
66.120159	1758.322714	20.835213
66.392164	1758.965124	20.840231
66.435791	1754.284435	20.845248
66.273437	1755.187414	20.850266
66.390412	1758.909118	20.855283
66.473151	1750.125819	20.860301
66.408456	1759.222241	20.865319
66.475300	1754.165507	20.870336
66.385316	1746.359226	20.875354
66.357742	1761.547215	20.880371
66.500855	1749.838317	20.885389
66.571215	1761.315292	20.890407
66.750072	1773.876720	20.895424
66.599239	1778.514598	20.900442
66.963189	1776.286424	20.905459
67.082520	1781.936079	20.910477
67.149247	1777.971332	20.915495
66.773621	1775.900059	20.920512
67.004167	1770.988096	20.925530
67.022996	1777.344659	20.930547
67.321252	1776.042018	20.935565
67.297524	1776.468815	20.940583
67.283995	1783.701505	20.945600
67.513710	1787.736931	20.950618
67.571052	1803.826892	20.955635
67.736536	1796.435028	20.960653
68.145448	1800.044725	20.965671
67.618680	1787.702251	20.970688
67.902990	1793.300814	20.975706
67.612540	1790.966870	20.980723
68.131914	1805.229706	20.985741
67.782253	1792.569128	20.990759
67.716395	1801.848802	20.995776
68.044558	1786.150104	21.000794
68.045513	1803.618603	21.005811
68.199485	1796.758752	21.010829
67.777247	1791.292609	21.015847
67.965685	1810.615875	21.020864
68.378984	1816.377283	21.025882
68.612030	1819.320216	21.030899
68.487888	1820.274020	21.035917
68.565769	1821.423404	21.040935
68.641260	1824.138542	21.045952
68.663253	1813.884562	21.050970
68.599716	1829.232887	21.055987
68.602579	1831.959406	21.061005
68.782402	1839.594199	21.066023
69.471842	1840.638300	21.071040
69.505241	1839.919984	21.076058
69.225497	1844.877898	21.081075
69.333324	1855.544281	21.086093
69.761033	1832.492216	21.091111
69.483796	1836.932149	21.096128
69.853098	1832.793744	21.101146
69.474021	1843.397541	21.106163
69.793356	1831.436903	21.111181
69.756275	1842.286938	21.116199
69.429806	1828.009980	21.121216
69.504517	1823.075078	21.126234
69.567421	1834.041995	21.131251
69.745775	1852.113950	21.136269
70.441598	1858.607487	21.141287
70.040836	1867.163286	21.146304
70.104404	1855.593022	21.151322
69.813627	1862.263228	21.156339
70.171364	1864.760571	21.161357
69.912620	1860.064108	21.166375
70.014644	1875.266604	21.171392
70.454660	1880.089667	21.176410
70.490301	1892.026632	21.181427
70.718851	1880.187490	21.186445
70.270643	1880.377818	21.191463
70.343942	1883.194301	21.196480
70.894622	1896.555996	21.201498
70.809507	1916.496630	21.206515
70.696935	1911.875089	21.211533
71.302458	1914.952197	21.216551
71.177856	1906.753611	21.221568
71.578667	1901.944333	21.226586
71.223017	1908.103976	21.231603
71.183229	1908.728966	21.236621
71.612835	1904.385424	21.241639
71.558617	1909.876104	21.246656
71.354848	1907.052005	21.251674
71.766816	1922.774065	21.256691
71.989737	1925.838531	21.261709
72.337024	1925.891601	21.266727
72.182291	1919.042197	21.271744
72.104923	1903.564733	21.276762
72.093213	1907.587516	21.281779
72.187070	1918.562259	21.286797
72.481937	1923.840450	21.291815
72.468018	1914.930194	21.296832
72.247182	1898.250675	21.301850
72.387095	1911.373761	21.306867
72.293719	1922.128515	21.311885
72.396923	1927.048545	21.316903
72.548421	1930.499769	21.321920
72.700707	1919.092302	21.326938
72.572716	1920.024622	21.331955
71.954509	1928.365192	21.336973
72.221325	1926.761332	21.341991
72.448352	1931.040226	21.347008
72.898432	1940.595768	21.352026
72.812736	1956.342177	21.357043
73.055286	1946.501722	21.362061
73.018978	1945.093685	21.367079
73.230201	1962.131735	21.372096
73.630681	1966.774810	21.377114
73.713240	1972.496563	21.382131
73.290183	1974.213626	21.387149
73.604542	1964.933153	21.392167
73.767605	1966.463705	21.397184
73.712387	1962.170859	21.402202
73.721948	1965.855783	21.407219
73.819294	1961.071942	21.412237
73.921660	1959.957781	21.417255
73.628805	1970.557611	21.422272
73.819265	1969.994577	21.427290
74.100332	1985.525747	21.432307
74.328680	1989.308950	21.437325
74.200815	1983.563081	21.442343
74.132826	1990.242613	21.447360
74.516840	1978.764086	21.452378
74.556669	1976.542485	21.457395
74.487874	1990.619890	21.462413
75.104694	1996.191669	21.467431
75.232280	2005.052948	21.472448
74.978887	2000.352453	21.477466
74.991621	1992.548907	21.482483
75.192811	2002.235003	21.487501
75.406270	2001.737797	21.492519
75.575525	1995.601365	21.497536
75.750035	1998.020128	21.502554
75.378325	1979.943955	21.507571
75.494814	1978.007011	21.512589
75.530840	1964.752513	21.517607
75.504861	1984.245269	21.522624
75.884538	1980.373468	21.527642
75.847418	1987.657278	21.532659
75.592562	2000.662385	21.537677
75.709672	1988.487156	21.542695
75.425101	1996.867011	21.547712
75.649134	2001.787066	21.552730
76.012447	2006.221364	21.557747
76.036237	2016.153028	21.562765
76.082717	2022.483253	21.567783
76.189845	2027.913975	21.572800
76.546634	2026.759947	21.577818
76.322811	2025.043586	21.582835
76.217123	2017.571032	21.587853
76.226621	2021.167607	21.592871
76.510252	2028.363308	21.597888
76.883827	2040.342108	21.602906
77.129030	2035.916963	21.607923
77.086980	2039.777258	21.612941
77.375616	2033.110830	21.617959
77.200787	2042.448730	21.622976
77.163028	2043.082874	21.627994
77.268688	2028.315142	21.633011
77.019111	2034.401400	21.638029
77.173947	2021.327077	21.643047
77.119933	2029.405718	21.648064
77.561483	2028.620292	21.653082
77.597013	2019.572838	21.658099
77.273431	2034.630696	21.663117
77.764089	2043.176315	21.668135
77.852560	2054.644328	21.673152
77.888871	2057.532912	21.678170
77.901516	2051.622984	21.683187
77.914224	2055.654598	21.688205
77.770788	2052.552758	21.693223
77.809044	2056.690831	21.698240
78.205617	2054.170313	21.703258
78.318236	2056.977507	21.708275
78.328162	2079.428271	21.713293
78.684883	2079.274720	21.718311
78.528909	2073.608971	21.723328
78.362808	2076.630263	21.728346
78.729842	2070.633245	21.733363
78.661333	2071.496288	21.738381
78.919027	2069.729730	21.743399
78.830941	2075.039560	21.748416
78.915992	2087.994632	21.753434
79.143188	2095.164484	21.758451
79.081990	2107.757445	21.763469
79.500335	2105.615391	21.768487
79.202394	2101.092276	21.773504
79.482391	2101.638765	21.778522
79.548393	2090.348858	21.783539
79.606689	2090.829089	21.788557
79.729223	2096.516214	21.793575
79.300038	2093.111971	21.798592
79.247173	2109.175287	21.803610
79.725759	2124.306373	21.808627
79.555834	2127.047384	21.813645
79.832697	2133.862304	21.818663
80.003395	2136.628850	21.823680
80.149548	2137.499293	21.828698
81.044003	2136.286270	21.833715
80.652215	2147.419299	21.838733
80.755517	2141.012261	21.843751
80.722024	2142.753519	21.848768
80.858165	2138.796754	21.853786
80.895794	2136.906864	21.858803
80.863756	2143.022197	21.863821
80.919961	2132.260861	21.868839
81.169487	2135.267543	21.873856
81.275188	2125.132825	21.878874
81.578526	2135.992824	21.883891
81.356956	2136.185517	21.888909
81.570545	2143.366989	21.893927
81.524017	2129.831790	21.898944
81.364015	2128.146448	21.903962
81.618439	2125.001198	21.908979
81.380635	2124.240148	21.913997
81.774472	2133.848791	21.919015
81.702560	2148.797882	21.924032
81.880614	2157.424092	21.929050
82.029730	2143.586809	21.934067
81.869930	2165.278412	21.939085
82.003937	2150.165283	21.944103
82.145495	2149.729836	21.949120
82.005917	2150.686075	21.954138
82.502261	2158.167264	21.959155
82.769240	2170.191256	21.964173
82.797985	2167.646293	21.969191
83.087471	2158.435895	21.974208
82.715291	2151.554192	21.979226
82.790551	2144.031143	21.984243
82.472492	2139.457517	21.989261
82.539071	2151.437149	21.994279
83.096264	2163.838582	21.999296
82.924360	2170.316693	22.004314
83.268773	2166.731268	22.009331
83.199593	2169.147206	22.014349
83.558798	2160.828518	22.019367
83.119115	2164.691173	22.024384
82.939440	2163.573847	22.029402
83.436882	2180.646164	22.034419
83.343298	2190.949794	22.039437
83.350799	2185.043785	22.044455
84.050036	2181.806742	22.049472
83.855699	2191.371857	22.054490
83.868109	2190.218122	22.059507
84.357873	2207.440003	22.064525
84.473831	2207.646092	22.069543
84.883696	2215.633202	22.074560
84.435960	2202.173431	22.079578
85.042323	2193.159543	22.084595
84.782715	2191.650761	22.089613
84.785190	2185.085919	22.094631
84.430047	2180.757954	22.099648
84.382073	2191.108091	22.104666
85.039625	2199.905372	22.109683
84.900473	2197.863276	22.114701
85.080330	2212.529957	22.119719
85.169961	2202.618638	22.124736
84.802788	2217.421525	22.129754
85.138332	2205.656932	22.134771
84.941895	2216.421698	22.139789
85.090518	2222.212082	22.144807
85.070365	2230.481184	22.149824
84.870766	2234.713373	22.154842
85.120917	2253.834928	22.159859
85.652380	2254.723911	22.164877
85.686697	2260.958287	22.169895
85.930575	2249.350052	22.174912
85.805675	2256.082785	22.179930
85.965551	2269.149351	22.184947
86.424532	2274.891128	22.189965
86.412764	2283.742817	22.194983
86.564857	2276.169802	22.200000
86.509126	2277.823030	22.205018
86.754900	2271.207415	22.210035
86.955631	2279.050578	22.215053
86.796558	2272.501547	22.220071
86.946468	2268.864517	22.225088
86.863413	2278.888812	22.230106
86.635517	2262.585635	22.235123
86.610789	2274.005246	22.240141
86.737216	2297.624719	22.245159
86.969754	2290.487259	22.250176
86.792393	2294.804349	22.255194
87.241673	2298.313141	22.260211
87.695891	2318.513737	22.265229
87.703354	2316.969413	22.270247
87.724637	2320.993431	22.275264
87.615664	2325.006296	22.280282
88.392179	2319.573104	22.285299
87.990256	2313.882691	22.290317
88.196747	2315.564274	22.295335
88.094828	2310.824184	22.300352
88.177923	2317.202431	22.305370
88.319466	2315.305710	22.310387
88.285077	2315.409113	22.315405
88.204768	2333.007635	22.320423
88.886754	2326.172164	22.325440
88.843757	2338.992830	22.330458
88.565856	2346.207201	22.335475
89.035216	2338.915843	22.340493
89.227414	2335.120682	22.345511
88.978698	2332.385615	22.350528
88.862203	2339.442139	22.355546
88.865320	2338.021583	22.360563
89.133986	2332.118792	22.365581
89.208246	2338.384811	22.370599
89.397386	2334.492290	22.375616
89.523825	2343.095116	22.380634
89.568315	2346.553718	22.385651
89.716675	2346.880977	22.390669
89.666247	2341.138641	22.395687
89.794508	2346.739734	22.400704
89.753261	2353.917031	22.405722
89.984580	2351.368709	22.410739
89.900328	2357.785814	22.415757
89.908348	2363.055423	22.420775
90.091187	2371.980817	22.425792
90.002513	2375.886362	22.430810
90.348479	2369.646370	22.435827
89.941778	2383.786492	22.440845
90.268982	2398.360804	22.445863
91.065355	2396.080588	22.450880
90.705846	2405.605416	22.455898
91.043472	2398.909085	22.460915
90.910580	2405.763057	22.465933
90.946615	2422.920521	22.470951
91.564680	2419.036527	22.475968
91.612847	2419.856058	22.480986
91.468157	2423.738828	22.486003
91.505988	2410.950823	22.491021
91.270204	2417.268601	22.496039
91.527430	2410.471242	22.501056
91.914879	2414.684090	22.506074
91.680421	2422.418756	22.511091
92.032778	2428.041574	22.516109
92.080458	2442.047430	22.521127
92.289714	2440.351548	22.526144
92.548603	2437.088769	22.531162
92.502748	2436.982508	22.536179
92.344354	2440.633877	22.541197
92.458361	2436.611080	22.546215
92.603284	2437.601663	22.551232
92.531252	2439.074406	22.556250
92.501432	2446.534000	22.561267
93.148615	2453.843344	22.566285
93.042519	2453.380412	22.571303
93.112251	2455.206523	22.576320
93.097351	2460.681744	22.581338
93.212944	2456.914339	22.586355
93.155976	2453.540081	22.591373
93.049232	2467.658522	22.596391
93.644925	2472.750876	22.601408
93.455698	2484.291078	22.606426
93.732994	2479.567278	22.611443
93.697688	2471.004114	22.616461
93.708457	2478.703540	22.621479
93.802205	2483.489490	22.626496
93.778084	2493.694039	22.631514
94.590222	2496.549514	22.636531
94.691923	2497.000862	22.641549
94.543651	2501.401815	22.646567
94.635623	2491.316384	22.651584
94.630797	2497.209802	22.656602
94.771448	2493.249096	22.661619
95.129061	2493.300552	22.666637
94.746977	2496.324192	22.671655
94.908851	2493.625768	22.676672
94.800172	2490.830863	22.681690
95.348289	2497.029009	22.686707
95.046381	2484.963278	22.691725
95.190809	2497.874626	22.696743
95.274468	2507.415290	22.701760
95.562899	2514.493658	22.706778
95.681212	2514.289086	22.711795
95.581117	2511.679045	22.716813
95.419650	2516.757480	22.721831
95.598676	2508.896096	22.726848
95.775915	2526.246152	22.731866
95.907883	2537.726597	22.736883
96.221463	2539.931122	22.741901
96.180367	2542.945532	22.746919
96.456681	2542.766703	22.751936
96.343005	2546.319558	22.756954
96.548710	2544.021401	22.761971
96.715169	2552.510749	22.766989
96.518985	2568.745269	22.772007
96.819776	2566.318591	22.777024
96.940218	2561.856054	22.782042
97.092510	2558.187032	22.787059
97.182025	2557.087472	22.792077
97.179209	2567.531747	22.797095
97.196274	2561.781923	22.802112
97.291147	2573.747935	22.807130
97.396117	2574.091465	22.812147
97.826187	2576.647012	22.817165
97.641455	2584.544389	22.822183
97.809748	2580.582490	22.827200
97.895307	2577.753983	22.832218
98.200797	2575.361285	22.837235
98.071502	2580.797654	22.842253
98.206930	2594.146028	22.847271
98.565809	2596.176188	22.852288
98.622718	2600.084222	22.857306
98.154021	2603.414970	22.862323
98.731871	2602.873284	22.867341
98.376353	2602.458894	22.872359
98.760092	2599.763568	22.877376
99.237600	2622.504710	22.882394
99.233149	2626.791632	22.887411
99.360464	2630.013226	22.892429
99.291357	2634.414433	22.897447
99.466622	2627.651927	22.902464
99.527050	2621.737482	22.907482
99.691240	2622.343163	22.912499
99.554211	2624.605672	22.917517
99.334304	2623.573523	22.922535
99.418967	2623.610932	22.927552
99.788769	2639.150861	22.932570
100.089278	2647.369916	22.937587
99.961471	2648.327492	22.942605
99.724722	2653.127395	22.947623
100.009586	2642.926442	22.952640
100.187081	2651.631882	22.957658
100.453304	2676.359854	22.962675
100.541523	2673.783408	22.967693
100.322143	2672.981573	22.972711
100.871008	2678.144446	22.977728
100.814585	2684.386874	22.982746
100.989714	2686.471082	22.987763
101.084948	2686.150190	22.992781
101.128776	2691.796181	22.997799
101.442053	2691.409566	23.002816
101.546830	2688.928365	23.007834
101.578299	2700.651903	23.012851
101.841773	2689.100282	23.017869
101.654659	2697.253729	23.022887
102.113249	2687.353774	23.027904
101.742586	2682.292732	23.032922
101.799296	2689.170762	23.037939
101.860039	2686.055760	23.042957
101.812492	2711.397891	23.047975
102.149551	2704.587915	23.052992
102.238706	2709.570328	23.058010
102.252413	2712.251095	23.063027
102.607847	2710.901557	23.068045
102.561148	2726.405818	23.073063
102.623338	2732.610742	23.078080
102.728349	2732.663901	23.083098
103.196869	2733.761611	23.088115
103.130416	2734.138313	23.093133
102.832843	2742.946633	23.098151
102.967469	2740.119882	23.103168
103.186981	2761.001607	23.108186
103.031564	2756.967295	23.113203
103.124051	2754.001961	23.118221
103.510847	2774.778589	23.123239
103.828169	2776.165109	23.128256
103.835134	2780.118881	23.133274
104.085685	2776.418639	23.138291
104.091445	2779.782395	23.143309
103.971846	2780.388357	23.148327
103.852860	2793.697834	23.153344
104.568663	2799.254360	23.158362
104.600639	2800.966487	23.163379
104.919005	2792.341447	23.168397
105.046363	2799.126390	23.173415
105.080921	2794.386884	23.178432
105.205574	2791.583781	23.183450
104.991117	2792.709593	23.188467
105.066345	2810.763953	23.193485
105.655774	2816.460219	23.198503
105.559294	2814.537614	23.203520
105.915557	2807.257476	23.208538
105.398638	2817.006020	23.213555
105.619964	2807.266263	23.218573
105.633610	2816.284666	23.223591
106.166479	2809.115730	23.228608
106.191765	2813.921964	23.233626
106.021473	2828.277889	23.238643
106.673175	2821.708942	23.243661
106.622007	2826.224163	23.248679
106.924155	2833.114294	23.253696
106.835209	2819.121262	23.258714
106.352574	2831.862817	23.263731
107.151882	2825.557956	23.268749
106.985471	2821.866219	23.273767
107.102970	2822.444505	23.278784
107.331162	2812.261804	23.283802
107.083209	2830.666654	23.288819
107.335989	2839.016366	23.293837
107.371588	2849.767249	23.298855
107.248758	2854.473608	23.303872
107.517679	2850.685256	23.308890
107.664320	2856.832806	23.313907
107.567105	2846.091923	23.318925
107.999254	2861.032069	23.323943
108.108725	2872.525722	23.328960
108.214124	2877.808631	23.333978
108.088631	2874.770117	23.338995
108.306005	2869.941981	23.344013
108.538266	2866.837951	23.349031
108.489913	2870.863533	23.354048
108.962400	2868.340479	23.359066
109.059724	2888.061080	23.364083
109.194898	2890.359881	23.369101
109.483306	2895.383721	23.374119
109.277312	2886.859725	23.379136
109.379956	2889.081561	23.384154
108.932405	2887.352824	23.389171
109.483610	2891.098263	23.394189
109.458166	2891.301265	23.399207
109.446572	2890.804578	23.404224
109.575995	2892.179515	23.409242
109.635658	2909.226430	23.414259
109.858025	2922.485678	23.419277
109.884470	2919.833659	23.424295
109.763390	2918.037989	23.429312
110.034916	2922.329087	23.434330
110.120526	2926.052792	23.439347
110.427206	2935.031657	23.444365
110.304084	2936.891188	23.449383
110.296397	2951.076550	23.454400
110.538174	2961.728917	23.459418
110.932884	2963.494698	23.464435
111.026032	2951.928563	23.469453
110.847146	2964.821464	23.474471
111.403043	2984.691260	23.479488
111.608246	2983.428364	23.484506
111.610480	2991.915243	23.489523
111.702941	2987.507485	23.494541
111.847645	2983.179918	23.499559
111.737067	2978.163262	23.504576
112.076744	2992.076455	23.509594
112.407511	3001.313546	23.514611
112.370494	2996.380046	23.519629
112.359335	3002.082092	23.524647
112.503779	3005.774502	23.529664
112.931425	2999.530967	23.534682
112.573961	3005.956387	23.539699
112.654517	3001.146496	23.544717
112.811250	3006.831708	23.549735
112.544197	3031.066129	23.554752
113.346081	3022.018043	23.559770
113.199722	3027.491938	23.564787
113.375376	3019.548799	23.569805
113.809257	3011.337959	23.574823
113.566685	3020.462886	23.579840
113.754924	3035.561328	23.584858
113.709614	3038.213515	23.589875
113.987720	3039.426295	23.594893
114.200561	3036.606182	23.599911
113.748892	3041.162111	23.604928
114.162370	3040.974414	23.609946
114.457468	3053.202905	23.614963
114.386734	3059.561329	23.619981
114.603031	3059.900051	23.624999
114.509701	3065.381431	23.630016
115.068972	3063.526499	23.635034
114.769822	3076.952786	23.640051
115.160837	3077.339885	23.645069
115.342540	3081.515689	23.650087
115.379434	3086.036116	23.655104
115.619052	3072.947749	23.660122
115.645306	3085.464567	23.665139
115.594250	3084.607935	23.670157
116.189268	3085.616413	23.675175
115.506488	3081.835086	23.680192
115.843782	3079.958117	23.685210
115.909037	3102.325740	23.690227
116.036033	3115.420168	23.695245
116.217008	3106.696567	23.700263
115.853809	3107.223923	23.705280
116.366833	3110.659767	23.710298
117.013034	3127.160498	23.715315
116.592233	3116.893085	23.720333
116.793682	3119.721249	23.725351
116.999031	3125.032759	23.730368
117.050859	3119.615027	23.735386
117.195670	3131.150651	23.740403
117.485297	3133.759847	23.745421
117.531576	3148.653375	23.750439
117.613004	3144.461932	23.755456
117.851365	3140.107028	23.760474
118.016572	3141.495316	23.765491
118.173999	3137.014219	23.770509
118.079752	3140.684084	23.775527
117.920970	3140.355637	23.780544
118.406000	3156.720678	23.785562
118.657449	3152.976032	23.790579
118.695425	3158.976585	23.795597
118.987879	3158.722630	23.800615
118.899259	3157.136475	23.805632
118.825823	3156.254939	23.810650
119.121391	3157.698554	23.815667
119.045854	3154.803666	23.820685
118.893856	3162.336354	23.825703
119.284214	3178.410091	23.830720
119.534254	3177.272720	23.835738
119.649429	3179.085473	23.840755
119.527869	3170.526021	23.845773
120.173874	3180.581782	23.850791
119.755818	3203.596531	23.855808
119.964804	3201.427184	23.860826
120.144499	3204.271394	23.865843
120.570125	3201.670419	23.870861
120.401857	3201.024676	23.875879
120.495903	3218.956559	23.880896
120.702892	3223.781779	23.885914
120.866394	3232.442350	23.890931
120.875566	3228.767208	23.895949
120.683915	3225.174030	23.900967
120.924029	3230.606375	23.905984
120.908142	3241.264558	23.911002
120.959411	3253.465104	23.916019
121.061771	3254.983185	23.921037
121.440127	3264.642206	23.926055
121.672711	3282.779699	23.931072
121.948752	3277.216323	23.936090
122.097107	3280.387394	23.941107
122.432666	3292.931649	23.946125
122.672729	3289.898918	23.951143
122.515942	3295.002088	23.956160
122.706162	3299.085077	23.961178
123.045381	3292.312417	23.966195
122.903829	3294.373717	23.971213
123.009657	3290.456169	23.976231
123.087950	3289.538230	23.981248
123.436512	3287.009286	23.986266
123.510633	3294.007913	23.991283
123.233440	3294.136735	23.996301
123.536641	3305.186842	24.001319
123.344541	3318.129408	24.006336
123.638868	3320.570612	24.011354
123.825110	3316.968712	24.016371
123.866617	3321.911416	24.021389
124.123112	3331.873630	24.026407
123.876072	3343.268780	24.031424
124.291406	3335.982332	24.036442
124.335161	3343.070955	24.041459
124.503426	3342.852236	24.046477
125.128506	3337.578192	24.051495
124.776719	3336.677131	24.056512
124.780219	3349.061977	24.061530
124.863656	3350.500968	24.066547
124.687707	3359.637722	24.071565
125.328618	3350.775664	24.076583
124.800807	3370.850390	24.081600
125.031453	3377.657245	24.086618
125.239459	3383.886893	24.091635
125.548317	3401.201391	24.096653
126.176136	3405.455723	24.101671
126.142924	3413.048813	24.106688
125.717487	3414.801098	24.111706
125.992760	3415.499874	24.116723
126.356994	3429.422185	24.121741
126.529837	3432.478976	24.126759
126.897307	3440.788906	24.131776
126.700665	3433.667735	24.136794
127.055136	3453.402324	24.141811
127.076985	3453.519016	24.146829
127.621531	3443.040207	24.151847
127.664910	3457.524127	24.156864
127.982275	3444.331778	24.161882
128.072930	3451.053278	24.166899
127.788676	3448.790738	24.171917
128.248515	3440.799735	24.176935
128.177711	3442.360742	24.181952
128.495713	3436.680274	24.186970
128.600525	3438.658804	24.191987
128.130392	3433.789884	24.197005
128.915972	3443.975430	24.202023
128.915434	3466.792537	24.207040
129.042701	3471.005366	24.212058
129.276461	3463.665251	24.217075
129.089617	3459.443170	24.222093
129.222869	3463.257367	24.227111
129.242701	3473.408240	24.232128
129.498089	3459.455453	24.237146
129.810423	3476.261316	24.242163
129.497357	3487.474366	24.247181
129.773117	3478.852519	24.252199
129.704350	3485.766293	24.257216
129.848529	3488.515111	24.262234
130.223195	3498.944974	24.267251
130.430653	3504.783369	24.272269
130.463225	3506.167215	24.277287
130.429362	3512.703086	24.282304
130.398883	3514.614445	24.287322
130.519540	3517.477423	24.292339
130.242355	3524.000919	24.297357
131.039780	3531.085167	24.302375
131.096136	3542.546536	24.307392
131.342803	3546.043133	24.312410
131.697341	3554.304641	24.317427
131.729264	3552.058835	24.322445
132.024048	3546.325156	24.327463
131.687419	3562.014435	24.332480
132.189814	3569.217515	24.337498
132.255294	3567.790248	24.342515
132.386757	3569.187012	24.347533
132.808094	3564.288862	24.352551
132.975642	3570.019903	24.357568
133.228071	3572.066855	24.362586
133.268963	3575.671448	24.367603
133.068102	3569.687157	24.372621
133.391944	3556.629433	24.377639
133.011369	3561.628860	24.382656
133.173147	3569.043120	24.387674
133.206226	3578.200894	24.392691
133.430178	3588.985834	24.397709
133.554236	3587.836613	24.402727
133.552326	3594.755735	24.407744
134.087858	3608.127399	24.412762
133.902748	3614.355589	24.417779
134.041319	3618.468837	24.422797
134.301639	3625.309012	24.427815
134.106756	3626.012016	24.432832
134.140423	3640.421852	24.437850
134.348704	3636.907970	24.442867
134.723686	3657.867380	24.447885
134.875674	3658.077313	24.452903
135.404168	3663.672927	24.457920
135.123017	3674.900030	24.462938
135.442176	3675.500409	24.467955
135.507942	3686.146061	24.472973
135.580031	3689.932013	24.477991
135.508990	3686.389285	24.483008
135.558130	3693.855963	24.488026
136.111016	3703.175401	24.493043
136.131697	3714.629843	24.498061
136.313801	3707.540760	24.503079
136.353107	3712.389225	24.508096
136.516918	3732.671630	24.513114
136.808550	3730.470335	24.518131
136.813793	3738.941312	24.523149
137.232875	3737.285034	24.528167
137.508429	3752.670250	24.533184
137.411046	3755.093974	24.538202
137.928143	3751.781039	24.543219
137.693303	3748.598535	24.548237
137.826315	3742.833325	24.553255
137.949575	3747.141537	24.558272
137.859842	3757.836844	24.563290
138.185328	3765.294977	24.568307
138.232372	3780.384599	24.573325
138.318683	3766.656916	24.578343
138.576177	3782.376403	24.583360
138.661989	3787.220759	24.588378
139.140817	3792.732661	24.593395
139.103495	3791.611865	24.598413
139.425848	3791.839298	24.603431
139.686294	3806.156923	24.608448
139.373735	3814.611441	24.613466
139.604997	3816.365039	24.618483
139.754422	3822.992250	24.623501
140.112263	3817.823064	24.628519
139.996659	3816.395740	24.633536
140.233627	3832.667692	24.638554
140.547184	3838.918839	24.643571
140.803829	3838.339069	24.648589
140.576894	3840.126577	24.653607
140.622373	3838.418350	24.658624
141.005218	3839.176043	24.663642
141.046903	3842.909976	24.668659
140.966669	3865.465468	24.673677
141.294184	3871.875413	24.678695
141.548975	3872.435381	24.683712
141.338088	3871.913075	24.688730
141.603916	3886.188887	24.693747
141.680070	3897.921984	24.698765
142.010220	3891.349375	24.703783
141.992558	3894.410840	24.708800
142.065569	3906.643141	24.713818
142.354804	3908.182503	24.718835
141.993516	3919.147707	24.723853
142.292299	3920.448845	24.728871
142.495400	3926.881458	24.733888
142.718327	3945.740784	24.738906
143.251170	3937.324642	24.743923
143.058988	3941.821201	24.748941
143.398451	3951.130015	24.753959
143.647162	3963.000252	24.758976
143.452245	3967.393085	24.763994
144.066559	3966.413231	24.769011
143.744393	3968.351396	24.774029
143.747098	3979.540529	24.779047
144.460088	3987.158992	24.784064
144.481031	3994.447140	24.789082
144.849696	3984.361717	24.794099
144.904977	3984.053376	24.799117
144.997787	3986.693532	24.804135
145.130457	3989.551547	24.809152
144.758947	4007.879101	24.814170
145.371978	4001.328419	24.819187
145.327800	4008.345857	24.824205
145.317405	4014.660442	24.829223
145.785159	4022.210023	24.834240
145.656704	4029.761477	24.839258
146.197630	4027.912484	24.844275
145.938116	4026.693915	24.849293
146.097510	4043.398011	24.854311
146.475371	4045.788352	24.859328
146.710250	4053.396524	24.864346
146.883512	4055.436996	24.869363
147.070759	4061.442871	24.874381
146.932032	4067.891210	24.879399
147.247859	4074.981686	24.884416
147.407953	4075.499681	24.889434
147.506887	4078.754389	24.894451
147.450784	4073.829898	24.899469
147.772204	4087.093424	24.904487
147.823933	4086.602566	24.909504
147.878419	4089.384466	24.914522
148.466780	4105.191280	24.919539
148.389005	4124.965915	24.924557
148.402713	4115.864014	24.929575
148.558000	4120.640760	24.934592
148.627982	4130.793614	24.939610
148.530082	4126.951992	24.944627
149.083999	4142.426499	24.949645
148.942184	4144.547907	24.954663
149.561733	4150.707034	24.959680
149.453825	4159.379006	24.964698
149.714404	4160.815561	24.969715
150.031271	4158.332497	24.974733
149.518292	4175.400879	24.979751
150.395616	4181.866838	24.984768
150.545741	4183.254414	24.989786
150.715437	4181.289962	24.994803
150.795495	4187.151694	24.999821
150.755405	4187.704211	25.004839
151.172055	4200.618321	25.009856
151.264863	4207.983676	25.014874
151.458879	4211.602283	25.019891
151.365653	4215.127010	25.024909
151.176190	4214.812817	25.029927
151.944586	4222.905634	25.034944
151.880407	4229.629586	25.039962
151.927203	4228.505055	25.044979
152.064001	4228.474329	25.049997
152.096401	4229.567866	25.055015
152.564394	4229.598885	25.060032
152.618126	4249.536126	25.065050
152.676943	4253.516817	25.070067
152.826033	4250.977959	25.075085
152.822407	4263.042591	25.080103
153.077095	4244.121085	25.085120
152.744959	4268.540959	25.090138
153.093569	4281.879279	25.095155
153.219929	4283.652515	25.100173
153.614556	4295.828380	25.105191
154.075306	4306.709223	25.110208
153.881016	4309.186079	25.115226
154.046951	4305.322025	25.120243
154.389926	4327.148936	25.125261
154.308915	4330.886409	25.130279
154.692772	4326.887203	25.135296
154.740564	4331.702940	25.140314
154.745745	4351.657369	25.145331
154.766294	4345.805425	25.150349
154.449324	4363.676577	25.155367
155.234133	4375.617763	25.160384
155.666406	4382.592266	25.165402
155.737855	4393.246913	25.170419
156.195975	4399.753375	25.175437
156.224287	4411.380667	25.180455
156.448002	4407.264491	25.185472
156.405295	4415.190916	25.190490
156.568576	4403.136243	25.195507
157.012494	4413.404277	25.200525
156.798373	4425.745042	25.205543
157.220616	4420.212074	25.210560
157.403921	4430.906036	25.215578
157.467315	4421.663626	25.220595
157.749083	4430.893346	25.225613
157.978419	4442.542824	25.230631
158.329308	4435.054553	25.235648
158.317503	4441.830352	25.240666
158.423001	4435.396906	25.245683
158.609741	4432.792151	25.250701
158.509903	4435.389956	25.255719
158.391260	4439.161755	25.260736
158.792747	4454.142750	25.265754
158.714496	4465.215450	25.270771
159.066314	4457.158860	25.275789
159.082345	4478.345907	25.280807
159.239258	4480.316390	25.285824
159.548421	4484.699818	25.290842
159.330651	4492.331742	25.295859
159.727813	4504.822999	25.300877
159.587042	4509.983973	25.305895
160.085463	4522.923380	25.310912
160.128509	4525.015871	25.315930
160.449396	4531.029373	25.320947
160.609570	4539.555364	25.325965
160.786931	4562.143964	25.330983
161.359275	4554.980789	25.336000
161.215431	4558.784970	25.341018
161.363699	4561.545937	25.346035
161.858340	4567.693212	25.351053
161.587048	4584.203291	25.356071
161.932055	4578.417231	25.361088
162.287862	4575.252523	25.366106
162.146359	4576.730008	25.371123
162.662590	4585.140266	25.376141
162.479609	4605.916731	25.381159
162.567192	4597.809936	25.386176
162.770113	4597.573149	25.391194
162.776485	4607.003929	25.396211
162.845233	4610.632772	25.401229
162.929784	4623.807541	25.406247
163.193499	4623.292928	25.411264
163.021899	4638.670038	25.416282
163.259650	4639.930288	25.421299
163.602421	4643.124802	25.426317
164.310693	4671.899175	25.431335
164.124317	4684.889164	25.436352
164.012576	4675.279500	25.441370
164.314211	4675.443906	25.446387
164.801671	4692.753757	25.451405
164.644301	4698.741233	25.456423
165.297746	4696.792479	25.461440
165.140688	4702.798847	25.466458
165.197793	4718.569480	25.471475
165.567681	4714.045242	25.476493
165.532583	4719.183406	25.481511
165.509727	4729.199626	25.486528
165.537562	4742.212915	25.491546
165.717256	4753.501058	25.496563
166.358473	4763.154426	25.501581
166.600464	4781.020487	25.506599
166.877117	4764.070985	25.511616
166.886992	4771.853596	25.516634
166.988915	4791.654465	25.521651
167.363895	4790.027101	25.526669
167.805174	4800.478848	25.531687
167.753741	4795.846986	25.536704
168.100808	4798.823055	25.541722
168.176099	4826.450010	25.546739
168.190368	4825.014884	25.551757
168.094906	4819.922747	25.556775
168.581865	4805.888459	25.561792
168.762107	4823.587471	25.566810
168.911092	4837.143710	25.571827
169.410849	4829.025901	25.576845
169.197304	4847.263265	25.581863
169.083056	4827.013233	25.586880
169.752866	4839.944957	25.591898
169.731634	4853.572067	25.596915
170.077645	4860.809637	25.601933
170.208858	4866.401582	25.606951
170.274448	4860.706556	25.611968
170.096204	4869.639252	25.616986
170.170986	4875.779809	25.622003
170.807049	4886.125333	25.627021
170.907552	4883.906497	25.632039
170.910213	4898.401103	25.637056
171.023819	4907.486958	25.642074
171.102177	4906.692034	25.647091
171.215634	4904.499575	25.652109
171.360406	4925.414450	25.657127
171.833276	4933.572826	25.662144
171.681364	4944.067083	25.667162
171.692232	4961.865364	25.672180
172.354359	4953.958805	25.677197
172.383448	4974.541482	25.682215
172.503360	4979.374502	25.687232
173.127355	4978.077428	25.692250
172.781086	4988.472740	25.697268
173.372401	4992.092393	25.702285
173.551922	5003.955213	25.707303
173.351198	5008.544912	25.712320
173.662032	5005.772277	25.717338
173.575697	5023.358574	25.722356
174.144270	5018.023463	25.727373
174.173252	5041.608127	25.732391
174.293130	5033.865398	25.737408
174.754754	5048.455519	25.742426
175.093049	5054.210787	25.747444
175.042877	5044.480802	25.752461
174.931956	5055.723121	25.757479
175.293365	5049.546085	25.762496
175.394263	5058.330975	25.767514
175.568707	5070.491352	25.772532
175.776400	5071.027173	25.777549
175.827063	5072.682926	25.782567
176.460147	5085.380680	25.787584
176.164970	5099.035108	25.792602
176.357302	5105.643440	25.797620
176.766786	5090.560460	25.802637
176.576969	5109.122652	25.807655
176.784981	5124.027188	25.812672
177.232511	5117.732470	25.817690
177.242180	5126.569564	25.822708
177.227854	5142.673727	25.827725
177.476499	5154.977209	25.832743
177.229357	5151.436530	25.837760
177.741006	5170.378162	25.842778
177.818822	5180.530375	25.847796
177.947805	5188.449178	25.852813
178.127680	5194.469211	25.857831
178.981820	5205.977104	25.862848
179.157177	5209.889242	25.867866
178.820434	5215.999686	25.872884
179.373871	5229.180352	25.877901
179.719964	5237.361884	25.882919
179.485678	5240.470139	25.887936
179.907439	5235.568324	25.892954
180.085346	5258.817434	25.897972
180.287915	5254.821176	25.902989
180.549442	5263.659916	25.908007
180.439555	5265.539706	25.913024
180.845188	5277.250486	25.918042
180.628967	5288.168531	25.923060
181.302290	5288.795556	25.928077
181.592080	5296.414589	25.933095
181.724029	5305.478829	25.938112
181.999570	5302.156115	25.943130
181.754581	5304.372735	25.948148
182.547611	5308.023985	25.953165
182.563778	5321.658212	25.958183
182.838630	5339.649096	25.963200
183.025985	5330.288951	25.968218
182.807683	5327.573911	25.973236
183.209230	5331.176014	25.978253
183.291269	5341.463390	25.983271
183.302842	5344.564711	25.988288
183.720104	5345.247637	25.993306
183.565272	5357.491357	25.998324
183.710536	5372.295445	26.003341
183.715795	5369.807375	26.008359
183.871220	5379.938071	26.013376
184.421166	5391.553715	26.018394
184.552704	5404.017759	26.023412
184.640383	5413.742412	26.028429
184.922016	5423.537697	26.033447
184.790516	5432.198187	26.038464
185.299336	5445.262891	26.043482
185.675435	5448.970017	26.048500
185.523536	5463.059983	26.053517
185.875018	5466.701523	26.058535
185.853392	5472.967867	26.063552
186.313383	5472.015276	26.068570
186.173710	5481.160037	26.073588
186.733638	5494.475615	26.078605
186.864935	5500.992640	26.083623
186.944184	5504.001313	26.088640
187.259285	5500.454557	26.093658
187.072665	5523.322338	26.098676
187.329238	5527.941538	26.103693
187.383921	5534.423228	26.108711
187.711083	5552.200944	26.113728
188.233490	5553.539775	26.118746
188.208278	5553.900603	26.123764
188.406965	5563.042902	26.128781
188.584858	5560.398338	26.133799
188.946648	5584.376654	26.138816
189.224453	5579.333154	26.143834
189.439889	5590.991861	26.148852
189.646390	5598.870289	26.153869
189.593878	5595.740965	26.158887
189.582109	5603.514696	26.163904
190.046051	5621.687733	26.168922
190.293325	5624.546993	26.173940
190.327295	5624.655487	26.178957
190.481870	5643.786132	26.183975
190.361706	5652.703798	26.188992
190.520969	5654.954986	26.194010
190.953536	5673.076168	26.199028
191.015456	5672.804639	26.204045
191.366488	5690.869166	26.209063
191.694454	5706.623474	26.214080
192.087053	5709.081179	26.219098
192.389112	5722.203728	26.224116
192.042193	5729.114578	26.229133
192.391525	5733.005887	26.234151
192.588637	5747.451765	26.239168
192.973988	5751.975087	26.244186
192.888027	5758.721955	26.249204
192.895441	5771.215166	26.254221
193.471396	5780.383703	26.259239
193.554885	5789.493656	26.264256
193.835478	5791.318639	26.269274
194.047647	5803.091635	26.274292
194.339368	5819.318910	26.279309
194.584932	5825.180496	26.284327
194.554238	5828.787281	26.289344
194.946420	5831.876409	26.294362
195.182789	5843.481491	26.299380
195.279773	5856.901427	26.304397
195.546140	5851.171482	26.309415
195.500214	5863.161725	26.314432
195.996888	5873.993690	26.319450
196.074351	5868.362781	26.324468
195.794071	5869.956811	26.329485
196.300385	5892.164072	26.334503
196.603123	5891.722231	26.339520
197.153222	5908.894004	26.344538
196.972250	5929.450689	26.349556
197.063201	5926.428259	26.354573
197.500392	5933.614093	26.359591
197.523975	5944.210856	26.364608
198.070185	5948.371258	26.369626
197.897694	5960.968544	26.374644
198.182564	5971.830591	26.379661
198.532584	5974.796923	26.384679
198.411920	5978.275779	26.389696
198.761076	5986.829664	26.394714
199.033162	6005.683427	26.399732
198.933554	6000.919909	26.404749
199.617507	6008.281774	26.409767
199.509907	6030.219197	26.414784
199.831165	6021.472227	26.419802
199.833517	6023.725946	26.424820
199.817609	6033.558702	26.429837
200.155856	6047.644935	26.434855
200.592532	6056.090440	26.439872
201.043076	6060.167996	26.444890
200.689689	6067.979658	26.449908
200.975010	6073.661475	26.454925
201.657867	6065.650179	26.459943
201.285945	6072.587172	26.464960
201.714162	6085.093593	26.469978
201.850624	6092.664375	26.474996
202.129834	6101.781704	26.480013
202.372065	6109.399058	26.485031
202.330892	6124.100379	26.490048
202.776490	6135.290901	26.495066
202.812690	6159.671380	26.500084
202.785834	6151.739663	26.505101
203.051028	6164.669430	26.510119
203.438057	6170.379538	26.515136
203.745872	6178.457005	26.520154
203.912344	6197.182299	26.525172
204.025892	6198.490530	26.530189
203.934764	6212.776741	26.535207
204.277464	6232.547766	26.540224
205.053826	6230.273396	26.545242
204.790911	6241.486589	26.550260
205.519726	6242.130215	26.555277
205.967205	6252.790177	26.560295
205.985215	6269.174376	26.565312
205.907210	6270.503150	26.570330
206.244384	6275.608686	26.575348
206.343768	6269.661698	26.580365
206.939091	6290.766411	26.585383
206.929674	6298.764200	26.590400
206.999732	6302.162730	26.595418
207.247306	6292.246537	26.600436
207.257527	6299.341566	26.605453
207.960876	6299.913422	26.610471
208.108399	6300.805955	26.615488
208.014156	6305.881224	26.620506
208.310745	6317.559250	26.625524
208.367019	6323.873661	26.630541
208.896560	6322.417675	26.635559
208.526619	6335.226087	26.640576
209.270932	6353.349617	26.645594
209.563210	6344.070379	26.650612
209.846834	6352.098047	26.655629
209.776749	6358.593261	26.660647
210.358070	6364.203544	26.665664
210.231837	6377.305270	26.670682
210.260816	6370.681097	26.675700
210.026017	6384.175495	26.680717
210.954631	6382.934785	26.685735
211.148246	6392.835927	26.690752
211.430476	6403.013619	26.695770
211.240791	6419.320002	26.700788
211.022277	6420.822325	26.705805
211.585593	6426.435448	26.710823
212.158805	6447.632197	26.715840
212.538104	6441.398228	26.720858
212.585178	6446.606082	26.725876
212.318781	6464.979607	26.730893
212.853882	6461.215109	26.735911
212.651451	6486.286867	26.740928
213.341779	6491.286630	26.745946
213.645550	6487.760402	26.750964
213.401231	6489.629808	26.755981
214.045401	6506.342296	26.760999
213.891418	6512.765474	26.766016
214.052799	6523.896585	26.771034
214.353045	6527.637916	26.776052
214.496536	6549.252510	26.781069
214.794324	6544.619162	26.786087
214.799399	6565.437840	26.791104
214.852633	6573.119722	26.796122
215.299735	6578.359650	26.801140
215.180693	6602.796607	26.806157
215.870533	6600.643082	26.811175
216.193008	6615.243632	26.816192
216.241763	6616.448397	26.821210
216.793069	6628.746498	26.826228
216.279598	6638.518625	26.831245
217.025434	6644.867179	26.836263
217.249085	6660.525006	26.841280
217.534471	6670.626588	26.846298
217.818683	6670.427554	26.851316
217.703569	6679.076594	26.856333
218.100317	6690.063601	26.861351
217.884830	6701.146526	26.866368
218.370712	6721.242904	26.871386
218.383033	6721.995639	26.876404
218.592809	6746.539117	26.881421
219.229258	6747.857020	26.886439
219.386775	6756.005641	26.891456
219.794209	6773.497325	26.896474
219.978070	6778.270294	26.901492
219.777785	6786.386589	26.906509
220.402853	6798.682720	26.911527
220.459244	6798.980278	26.916544
220.466041	6812.497122	26.921562
220.768134	6822.425700	26.926580
220.780653	6836.718257	26.931597
221.329223	6843.151451	26.936615
221.661888	6862.258628	26.941632
221.844732	6869.282638	26.946650
222.039307	6879.430131	26.951668
222.060036	6896.168035	26.956685
222.540304	6903.716862	26.961703
222.499861	6914.163213	26.966720
223.329776	6928.634009	26.971738
223.794456	6930.701764	26.976756
223.168146	6931.781850	26.981773
223.635149	6946.783048	26.986791
224.012630	6952.592762	26.991808
223.976028	6960.503548	26.996826
224.095300	6977.829057	27.001844
224.557977	6989.481494	27.006861
225.031357	7003.099014	27.011879
225.014161	7009.715606	27.016896
225.033368	7018.779416	27.021914
225.508785	7026.610019	27.026932
225.867415	7036.896058	27.031949
226.121186	7047.864639	27.036967
226.481734	7056.676109	27.041984
226.627121	7058.866508	27.047002
227.208082	7051.148561	27.052020
226.732719	7059.260715	27.057037
226.982224	7070.829793	27.062055
227.569527	7076.587735	27.067072
227.965127	7093.769043	27.072090
228.295489	7091.349773	27.077108
228.326647	7100.525401	27.082125
228.466032	7107.862533	27.087143
228.554140	7105.623274	27.092160
228.278361	7116.561204	27.097178
229.015823	7120.237321	27.102196
229.066413	7126.783354	27.107213
228.962403	7132.292881	27.112231
229.662530	7145.038399	27.117248
229.545532	7153.795293	27.122266
229.992722	7155.067110	27.127284
230.062206	7177.855789	27.132301
230.587705	7170.878892	27.137319
230.562296	7193.278368	27.142336
230.566508	7196.529533	27.147354
231.025889	7202.796881	27.152372
231.104336	7220.952977	27.157389
231.378431	7234.595575	27.162407
231.813514	7241.008806	27.167424
231.804353	7254.711578	27.172442
231.861292	7264.211571	27.177460
232.107436	7274.155473	27.182477
232.723452	7281.048643	27.187495
232.997870	7292.550819	27.192512
233.365109	7303.012448	27.197530
233.382949	7313.099473	27.202548
233.507720	7333.590888	27.207565
233.728906	7340.710095	27.212583
234.137720	7337.921767	27.217600
234.436115	7358.076627	27.222618
234.669531	7364.966627	27.227636
235.014977	7378.926479	27.232653
234.661526	7383.957414	27.237671
235.057231	7390.452633	27.242688
235.625125	7406.988477	27.247706
235.819587	7412.672318	27.252724
236.095153	7422.314935	27.257741
236.494566	7430.621695	27.262759
236.763560	7448.265146	27.267776
237.045085	7450.708923	27.272794
237.269366	7462.582112	27.277812
237.572733	7473.230636	27.282829
237.767452	7474.759860	27.287847
237.839633	7489.801255	27.292864
237.999003	7495.989424	27.297882
238.287011	7499.622377	27.302900
238.060759	7506.249798	27.307917
238.236581	7519.844864	27.312935
238.833806	7543.346885	27.317952
238.961968	7553.205239	27.322970
239.287280	7564.137666	27.327988
239.451944	7576.680082	27.333005
240.052365	7585.864641	27.338023
240.198033	7596.948352	27.343040
240.516506	7599.477914	27.348058
240.544877	7611.874383	27.353076
240.581559	7634.880287	27.358093
240.681488	7639.455109	27.363111
241.274491	7653.404803	27.368128
241.443461	7665.700357	27.373146
241.746341	7675.408283	27.378164
242.131860	7695.871881	27.383181
242.197105	7699.274581	27.388199
242.444513	7707.359031	27.393216
242.907753	7718.617215	27.398234
242.788035	7728.937537	27.403252
242.680033	7737.270256	27.408269
243.177805	7753.438553	27.413287
243.647837	7771.698014	27.418304
243.504707	7774.811353	27.423322
244.014734	7803.138695	27.428340
244.374495	7812.518921	27.433357
244.514934	7813.696774	27.438375
244.857655	7832.070949	27.443392
245.308616	7840.237223	27.448410
245.358291	7845.192502	27.453428
245.563045	7855.613603	27.458445
245.929477	7855.944693	27.463463
246.579561	7862.333933	27.468480
246.603543	7882.867004	27.473498
247.206738	7875.397800	27.478516
247.299026	7888.614748	27.483533
247.164985	7887.265758	27.488551
247.606018	7894.072920	27.493568
247.352322	7903.246215	27.498586
247.988185	7914.499577	27.503604
248.190489	7931.970830	27.508621
248.219958	7941.743827	27.513639
249.024592	7938.167277	27.518656
249.022249	7952.384101	27.523674
248.792400	7956.316108	27.528692
249.258834	7959.501312	27.533709
249.310472	7986.691588	27.538727
249.922803	7998.491705	27.543744
249.454316	8015.256750	27.548762
250.324998	8027.976167	27.553780
250.627404	8039.944831	27.558797
250.426674	8057.252029	27.563815
250.959739	8062.914599	27.568832
251.140394	8088.951418	27.573850
251.688126	8095.088422	27.578868
251.586509	8109.295661	27.583885
251.865609	8111.702022	27.588903
252.214691	8136.250787	27.593920
252.216689	8152.077206	27.598938
252.658952	8170.385612	27.603956
252.996255	8183.971656	27.608973
253.066371	8203.585451	27.613991
253.512388	8213.315437	27.619008
254.002627	8221.447315	27.624026
254.258189	8227.191293	27.629044
254.600281	8246.645714	27.634061
254.512645	8254.331422	27.639079
255.089040	8263.201217	27.644096
255.151986	8277.856374	27.649114
255.441691	8284.150675	27.654132
255.974888	8299.224695	27.659149
255.841942	8310.898665	27.664167
256.559253	8323.566542	27.669184
256.865976	8331.638818	27.674202
256.524493	8344.605174	27.679220
257.041318	8350.614505	27.684237
256.864490	8361.704996	27.689255
257.794221	8374.759532	27.694272
257.550565	8391.489695	27.699290
257.873605	8402.527162	27.704308
258.075766	8411.727168	27.709325
258.296018	8422.916506	27.714343
258.957698	8426.781566	27.719360
258.863846	8449.897332	27.724378
259.288108	8456.416871	27.729396
259.689403	8464.272332	27.734413
259.666019	8482.186733	27.739431
260.299702	8489.304910	27.744448
260.576395	8507.914261	27.749466
260.678287	8503.222714	27.754484
261.149410	8517.672047	27.759501
261.178668	8533.876539	27.764519
261.871661	8534.320660	27.769536
261.620380	8557.069732	27.774554
262.130406	8560.406072	27.779572
262.227140	8561.745522	27.784589
262.482196	8577.744193	27.789607
262.964936	8589.555520	27.794624
262.814841	8604.853645	27.799642
262.792492	8617.053517	27.804660
263.187575	8626.409682	27.809677
263.523613	8638.060905	27.814695
264.082258	8644.098511	27.819712
264.115027	8660.359393	27.824730
264.360926	8668.087738	27.829748
264.440455	8680.034903	27.834765
264.878654	8687.868892	27.839783
265.235681	8711.157456	27.844800
265.180515	8727.447958	27.849818
265.508074	8743.624847	27.854836
265.959826	8744.302512	27.859853
266.038525	8770.990861	27.864871
266.522844	8771.941260	27.869888
266.992361	8791.133188	27.874906
266.947188	8796.656092	27.879924
267.290029	8808.438960	27.884941
267.292432	8829.462672	27.889959
268.261243	8840.800206	27.894976
268.199370	8859.778670	27.899994
268.444458	8868.710130	27.905012
268.989959	8879.621473	27.910029
269.336681	8889.439989	27.915047
269.254207	8908.232296	27.920064
269.638905	8919.942376	27.925082
269.739450	8927.390505	27.930100
270.226985	8935.008494	27.935117
270.510504	8954.577025	27.940135
271.006945	8963.257620	27.945152
270.925634	8972.218160	27.950170
271.284570	8985.706688	27.955188
271.615332	8994.429038	27.960205
272.013478	9014.851077	27.965223
272.445536	9022.992424	27.970240
272.281795	9031.043987	27.975258
272.737912	9038.461719	27.980276
272.985977	9050.887882	27.985293
272.812476	9073.094981	27.990311
273.288537	9082.659701	27.995328
273.397611	9105.005694	28.000346
273.868230	9114.950155	28.005364
274.498946	9116.515408	28.010381
274.869466	9136.872449	28.015399
274.565483	9146.616228	28.020416
275.413541	9153.770543	28.025434
275.489445	9172.547779	28.030452
275.844684	9171.358843	28.035469
275.945948	9196.247778	28.040487
276.307454	9194.107517	28.045504
276.677548	9205.674831	28.050522
276.826953	9219.205825	28.055540
277.093890	9225.851317	28.060557
277.446174	9251.809211	28.065575
277.831395	9248.351796	28.070592
278.045755	9272.657962	28.075610
277.883988	9284.899056	28.080628
278.466346	9288.202099	28.085645
278.221031	9299.834303	28.090663
279.027569	9316.072424	28.095680
279.187346	9331.167896	28.100698
279.380154	9342.819899	28.105716
280.207587	9360.384012	28.110733
280.315096	9380.722533	28.115751
280.586546	9382.211482	28.120768
280.504481	9387.096249	28.125786
280.460058	9393.471687	28.130804
280.886352	9405.245019	28.135821
281.137848	9431.632562	28.140839
281.410954	9437.532036	28.145856
281.586645	9454.901546	28.150874
281.885588	9473.896733	28.155892
282.511504	9478.891631	28.160909
282.582711	9507.713410	28.165927
282.916962	9519.788551	28.170944
283.246659	9534.112439	28.175962
283.531544	9545.197611	28.180980
284.052314	9554.828191	28.185997
283.955543	9571.965803	28.191015
284.404737	9579.987890	28.196032
284.987110	9592.949313	28.201050
285.076098	9609.372716	28.206068
285.662340	9626.826469	28.211085
285.692602	9636.957016	28.216103
286.124195	9642.658073	28.221120
286.433703	9650.831525	28.226138
286.510465	9666.186548	28.231156
287.188545	9670.472393	28.236173
286.983540	9682.745780	28.241191
287.323496	9696.938735	28.246208
287.959661	9713.857469	28.251226
288.036404	9727.321281	28.256244
288.422971	9740.086150	28.261261
288.606112	9752.863950	28.266279
288.902833	9759.167129	28.271296
289.483940	9775.759863	28.276314
289.509007	9784.271568	28.281332
290.000922	9795.024507	28.286349
290.086962	9813.273518	28.291367
290.524324	9824.615979	28.296384
290.614561	9833.613208	28.301402
290.602702	9853.781501	28.306420
291.311388	9862.296662	28.311437
291.330874	9875.965309	28.316455
292.166984	9889.360802	28.321472
292.375713	9906.731873	28.326490
292.214706	9918.717514	28.331508
292.633871	9934.505361	28.336525
292.888178	9949.940157	28.341543
293.269479	9961.676688	28.346560
293.310550	9972.711901	28.351578
293.821553	9989.704171	28.356596
294.165263	10004.562987	28.361613
294.570054	10033.879557	28.366631
294.663961	10036.829844	28.371648
295.012944	10045.862420	28.376666
295.448595	10061.505709	28.381684
295.834693	10066.876180	28.386701
296.022093	10084.231813	28.391719
296.035385	10094.848355	28.396736
296.524159	10113.631327	28.401754
296.582701	10119.539370	28.406772
296.746474	10143.185220	28.411789
297.318041	10150.809493	28.416807
297.260877	10178.585202	28.421824
298.010747	10186.067891	28.426842
298.340538	10204.544328	28.431860
298.882433	10214.042487	28.436877
299.150085	10222.750043	28.441895
299.204127	10246.236395	28.446912
299.816350	10248.919231	28.451930
299.833288	10256.747256	28.456948
300.406728	10280.805884	28.461965
300.344946	10282.640752	28.466983
300.843174	10290.046076	28.472000
301.424456	10301.214726	28.477018
301.000468	10320.320866	28.482036
301.426184	10323.474975	28.487053
301.708608	10329.884785	28.492071
301.930944	10337.649094	28.497088
302.662340	10357.878320	28.502106
302.789972	10382.824702	28.507124
302.890816	10387.993667	28.512141
303.175481	10409.230702	28.517159
303.771449	10422.998894	28.522176
303.903346	10430.193273	28.527194
304.219877	10453.117781	28.532212
304.367949	10456.059649	28.537229
304.569927	10483.526829	28.542247
304.216973	10499.751857	28.547264
305.032585	10511.572262	28.552282
305.182520	10533.739904	28.557300
305.830475	10558.080865	28.562317
306.267374	10572.136159	28.567335
306.346776	10594.024431	28.572352
306.812495	10598.485849	28.577370
306.866744	10626.926795	28.582388
307.774446	10646.771918	28.587405
307.803284	10656.110701	28.592423
308.342550	10679.499485	28.597440
308.930301	10690.645253	28.602458
308.874896	10711.894855	28.607476
309.279108	10710.903396	28.612493
309.572031	10738.808233	28.617511
309.838278	10741.990553	28.622528
310.156740	10761.716546	28.627546
310.277325	10774.814285	28.632564
310.590863	10786.587212	28.637581
311.089420	10802.824362	28.642599
311.583300	10818.765448	28.647616
312.102840	10828.649489	28.652634
312.253383	10839.102862	28.657652
312.420810	10853.753153	28.662669
312.761265	10872.613804	28.667687
313.066348	10887.791975	28.672704
313.609152	10903.706525	28.677722
313.808159	10914.828069	28.682740
313.933937	10924.622279	28.687757
314.443134	10936.756190	28.692775
314.823277	10951.752146	28.697792
314.676562	10962.788942	28.702810
314.980661	10981.655397	28.707828
315.334137	10998.723786	28.712845
315.867090	11011.829719	28.717863
315.866282	11031.558646	28.722880
316.557208	11050.254060	28.727898
316.968394	11060.871972	28.732916
317.394287	11080.900390	28.737933
317.515848	11091.412124	28.742951
317.864526	11103.713381	28.747968
318.221058	11116.395486	28.752986
318.217945	11132.155769	28.758004
318.846330	11145.745750	28.763021
318.850309	11152.900451	28.768039
319.274055	11162.859670	28.773056
319.687235	11185.160516	28.778074
319.621465	11206.756482	28.783092
320.093138	11217.822864	28.788109
320.773124	11238.048470	28.793127
320.794390	11248.594948	28.798144
321.485311	11261.973129	28.803162
321.793735	11268.565490	28.808180
322.140384	11281.078743	28.813197
322.449518	11302.985536	28.818215
322.731831	11296.379919	28.823232
323.139557	11309.439368	28.828250
323.216625	11318.853025	28.833268
323.716521	11333.978938	28.838285
323.741814	11333.040489	28.843303
324.320054	11346.354284	28.848320
324.469076	11359.867945	28.853338
324.952801	11366.158165	28.858356
325.206378	11377.561939	28.863373
325.474523	11388.789768	28.868391
325.456992	11397.564649	28.873408
326.035674	11408.718585	28.878426
326.037988	11444.084172	28.883444
326.618411	11462.699422	28.888461
327.052221	11474.873912	28.893479
327.026075	11497.660761	28.898496
327.319631	11511.698168	28.903514
327.493965	11531.008632	28.908532
327.925699	11542.191981	28.913549
328.221294	11568.888246	28.918567
328.685831	11591.263631	28.923584
329.401971	11613.249126	28.928602
329.437037	11624.513607	28.933620
329.734928	11649.195019	28.938637
330.771039	11665.130833	28.943655
330.621275	11687.820441	28.948672
330.896038	11691.832067	28.953690
331.398572	11708.157797	28.958708
331.554453	11720.192836	28.963725
332.379822	11747.482118	28.968743
332.025487	11762.079069	28.973760
332.449178	11774.782678	28.978778
332.853944	11788.225008	28.983796
333.742670	11809.154283	28.988813
333.989432	11817.265889	28.993831
334.190799	11849.667532	28.998848
334.733600	11851.332063	29.003866
334.949410	11863.000983	29.008884
335.300559	11870.853114	29.013901
335.757168	11885.092616	29.018919
335.947927	11898.170674	29.023936
335.897752	11915.382071	29.028954
336.510600	11936.566272	29.033972
336.686217	11953.972851	29.038989
337.003752	11959.338823	29.044007
337.031060	11977.542303	29.049024
337.510130	12005.003042	29.054042
337.520961	12017.973585	29.059060
337.882888	12043.535971	29.064077
338.548922	12062.188931	29.069095
338.787963	12085.326514	29.074112
339.369700	12106.752613	29.079130
339.625986	12117.925896	29.084148
340.134963	12143.294864	29.089165
340.665436	12166.431104	29.094183
340.616008	12174.639785	29.099200
341.049739	12190.897769	29.104218
341.215066	12203.578984	29.109236
341.669439	12228.110332	29.114253
342.102300	12254.479762	29.119271
342.524513	12263.318791	29.124288
343.003554	12274.990942	29.129306
343.305934	12292.883226	29.134324
343.411947	12310.067359	29.139341
343.969558	12317.776814	29.144359
344.173688	12343.815893	29.149376
344.198426	12349.783617	29.154394
344.525691	12366.607889	29.159412
344.942823	12393.769432	29.164429
345.630966	12388.849297	29.169447
345.623810	12425.996062	29.174464
345.745002	12429.987693	29.179482
345.987532	12448.524222	29.184500
346.226025	12488.436784	29.189517
346.900821	12494.773244	29.194535
347.112701	12522.481851	29.199552
347.722323	12550.832395	29.204570
348.068301	12571.219128	29.209588
348.293292	12593.945858	29.214605
348.844703	12595.849107	29.219623
349.023827	12629.862923	29.224640
349.301744	12638.775257	29.229658
349.929686	12660.750534	29.234676
350.427138	12686.482035	29.239693
350.605545	12698.548908	29.244711
350.705836	12718.390079	29.249728
351.294511	12740.816860	29.254746
351.647931	12758.559486	29.259764
352.297754	12774.547284	29.264781
352.454236	12795.068152	29.269799
352.843647	12808.842040	29.274816
353.368330	12833.975794	29.279834
353.543733	12851.841129	29.284852
353.928734	12875.297870	29.289869
354.350997	12883.016128	29.294887
354.766093	12911.505055	29.299904
354.685560	12925.921064	29.304922
355.174245	12935.100525	29.309940
355.196331	12964.396360	29.314957
355.828831	12982.013374	29.319975
356.436055	13003.847032	29.324992
357.205477	13021.382635	29.330010
357.386642	13041.034633	29.335028
357.623261	13056.190543	29.340045
358.034381	13070.333857	29.345063
358.227299	13087.505084	29.350080
358.172599	13101.743494	29.355098
358.952092	13116.744942	29.360116
359.357657	13155.735886	29.365133
359.836308	13155.398975	29.370151
360.127651	13181.258175	29.375168
360.409756	13196.416547	29.380186
361.016659	13206.048159	29.385204
361.280333	13231.895972	29.390221
361.473371	13242.827193	29.395239
361.803713	13267.072999	29.400256
362.374791	13285.713626	29.405274
362.795930	13304.298809	29.410292
362.809716	13325.739469	29.415309
363.098743	13341.651629	29.420327
363.453282	13357.414590	29.425344
363.863573	13378.818465	29.430362
364.635610	13391.613869	29.435380
364.918799	13417.919946	29.440397
365.134912	13438.062686	29.445415
365.582692	13453.154258	29.450432
365.930692	13467.415129	29.455450
366.305995	13481.997007	29.460468
366.547997	13511.726624	29.465485
366.807446	13523.298154	29.470503
367.227050	13539.392139	29.475520
367.427738	13568.935679	29.480538
367.968978	13582.490551	29.485556
368.051530	13602.856500	29.490573
368.756191	13620.418596	29.495591
369.365712	13633.018559	29.500608
369.661973	13642.635893	29.505626
369.626193	13661.081411	29.510644
369.412751	13680.833780	29.515661
369.810518	13703.711628	29.520679
370.528392	13734.766064	29.525696
370.946005	13755.717618	29.530714
371.535891	13767.265959	29.535732
371.773347	13787.648897	29.540749
371.935229	13814.138743	29.545767
372.571339	13834.516131	29.550784
372.619388	13868.107414	29.555802
374.191238	13865.233864	29.560820
374.306454	13889.795232	29.565837
375.005258	13903.237228	29.570855
375.432399	13909.016088	29.575872
375.424005	13921.179320	29.580890
375.741317	13927.761750	29.585908
375.736252	13946.998569	29.590925
376.361973	13973.589677	29.595943
376.686912	13991.097906	29.600960
377.070983	14003.206031	29.605978
377.771144	14021.678735	29.610996
377.773321	14041.880892	29.616013
378.379423	14051.506746	29.621031
378.737198	14074.587108	29.626048
378.872284	14086.450059	29.631066
379.371761	14103.776305	29.636084
379.568912	14124.541733	29.641101
379.910085	14142.208622	29.646119
380.223026	14168.277378	29.651136
380.506993	14189.212448	29.656154
381.206183	14205.790612	29.661172
381.523847	14225.422455	29.666189
381.777700	14252.517499	29.671207
381.850836	14278.425006	29.676224
382.334214	14301.359644	29.681242
382.871537	14322.833114	29.686260
383.145027	14355.717261	29.691277
383.519760	14365.499527	29.696295
384.073524	14386.711526	29.701312
384.101407	14427.599129	29.706330
384.686111	14447.015673	29.711348
385.287605	14467.187566	29.716365
385.575400	14486.489592	29.721383
386.076215	14513.192608	29.726400
386.094498	14539.377507	29.731418
387.253057	14550.919364	29.736436
387.232603	14576.901942	29.741453
387.752009	14597.759526	29.746471
388.322343	14614.610887	29.751488
388.336918	14644.778989	29.756506
389.004655	14659.518091	29.761524
389.256171	14687.444725	29.766541
389.617120	14700.785458	29.771559
390.103024	14716.990070	29.776576
390.461917	14741.741758	29.781594
390.959013	14760.888107	29.786612
391.392410	14781.689884	29.791629
391.784969	14804.345640	29.796647
392.033411	14823.837348	29.801664
392.126443	14844.294572	29.806682
392.685173	14855.627383	29.811700
393.358607	14881.748029	29.816717
393.781005	14905.675158	29.821735
394.129001	14900.735031	29.826752
394.481386	14924.354168	29.831770
395.090476	14920.383776	29.836788
395.307797	14943.329280	29.841805
395.861133	14954.309272	29.846823
396.535477	14969.189702	29.851840
396.603389	14978.091818	29.856858
397.056681	14995.179770	29.861876
397.082837	15008.197328	29.866893
397.664283	15040.645952	29.871911
397.626904	15040.822529	29.876928
397.950766	15073.864253	29.881946
398.585367	15078.976165	29.886964
398.752521	15106.130217	29.891981
398.938618	15142.607730	29.896999
399.751521	15169.228040	29.902016
399.806601	15187.487095	29.907034
400.567375	15208.503355	29.912052
400.773312	15234.489265	29.917069
401.271790	15247.919380	29.922087
401.602980	15280.909781	29.927104
402.112461	15301.523343	29.932122
402.668879	15318.822829	29.937140
402.982890	15340.682999	29.942157
403.306419	15358.527488	29.947175
403.964050	15373.410853	29.952192
404.690055	15400.477786	29.957210
405.108830	15418.825377	29.962228
405.107245	15445.267294	29.967245
405.363955	15459.847159	29.972263
406.141067	15478.704019	29.977280
406.365778	15506.209674	29.982298
406.859658	15526.289005	29.987316
407.121373	15547.172201	29.992333
407.350214	15573.717169	29.997351
407.903094	15591.257491	30.002368
408.274270	15621.554459	30.007386
408.650600	15632.530986	30.012404
409.150625	15661.364466	30.017421
409.714434	15695.683558	30.022439
410.215426	15707.995542	30.027456
410.790511	15738.655553	30.032474
410.981423	15757.370789	30.037492
411.333693	15775.703872	30.042509
411.994946	15805.715659	30.047527
412.407961	15822.741176	30.052544
412.651991	15843.813810	30.057562
413.384052	15857.119332	30.062580
413.326337	15879.076243	30.067597
413.728326	15890.690054	30.072615
414.596029	15907.413863	30.077632
414.531491	15946.019868	30.082650
415.319394	15960.968564	30.087668
415.607075	15983.594770	30.092685
415.904165	15993.841688	30.097703
416.363597	16010.759033	30.102720
416.778030	16043.421866	30.107738
417.481251	16063.791132	30.112756
417.784193	16077.363004	30.117773
418.299271	16098.456631	30.122791
419.106118	16109.883981	30.127808
419.336862	16128.789164	30.132826
419.465433	16146.014286	30.137844
420.259759	16162.320264	30.142861
420.335396	16183.258567	30.147879
420.655057	16197.311148	30.152896
420.854846	16228.340256	30.157914
421.708331	16235.790199	30.162932
421.778806	16251.173659	30.167949
422.081785	16272.840797	30.172967
422.635663	16278.167822	30.177984
422.923831	16305.851033	30.183002
423.019217	16318.628068	30.188020
423.450332	16352.725919	30.193037
424.212850	16368.294813	30.198055
424.653995	16387.915855	30.203072
424.695866	16405.998105	30.208090
425.171015	16424.574716	30.213108
425.855756	16454.921799	30.218125
425.833528	16487.454799	30.223143
426.318108	16497.906349	30.228160
426.751374	16532.436897	30.233178
427.190952	16556.063340	30.238196
427.595104	16582.724376	30.243213
428.241071	16614.660201	30.248231
428.653243	16636.446461	30.253248
428.718551	16669.894663	30.258266
429.399076	16690.672442	30.263284
430.014661	16714.277829	30.268301
430.395151	16746.208076	30.273319
431.223950	16764.483257	30.278336
431.590354	16795.401900	30.283354
431.876482	16806.159496	30.288372
432.225117	16835.703860	30.293389
432.775605	16866.754870	30.298407
433.436902	16886.954698	30.303424
433.858773	16909.968430	30.308442
434.374479	16920.020515	30.313460
434.559751	16930.320193	30.318477
435.193157	16976.696417	30.323495
435.521410	16991.642111	30.328512
435.952189	17013.590131	30.333530
436.549261	17032.195611	30.338548
436.933923	17060.101686	30.343565
437.277528	17078.260489	30.348583
437.868628	17099.804464	30.353600
438.040484	17130.504588	30.358618
438.605212	17152.855038	30.363636
439.524689	17173.570644	30.368653
439.653428	17192.205415	30.373671
440.274508	17201.451489	30.378688
440.542048	17229.237175	30.383706
440.777121	17248.120669	30.388724
441.337595	17265.689763	30.393741
441.558820	17289.521874	30.398759
442.710798	17311.452028	30.403776
442.496732	17331.441985	30.408794
443.301944	17355.782848	30.413812
443.662406	17372.448410	30.418829
444.091270	17405.559822	30.423847
444.101326	17427.612116	30.428864
444.728971	17445.650968	30.433882
444.759202	17472.425500	30.438900
445.383393	17499.953558	30.443917
445.833614	17528.993478	30.448935
446.509365	17553.430676	30.453952
446.962393	17589.741513	30.458970
447.001006	17617.784721	30.463988
448.000233	17640.061363	30.469005
448.447143	17659.853367	30.474023
448.869624	17673.559260	30.479040
449.152957	17688.240883	30.484058
449.577418	17730.614834	30.489076
450.336461	17743.465750	30.494093
450.379756	17772.449743	30.499111
450.888752	17796.869147	30.504128
451.483149	17823.922209	30.509146
452.054744	17840.776216	30.514164
452.367200	17855.175436	30.519181
452.641796	17865.448988	30.524199
453.225729	17897.557750	30.529216
453.779831	17921.932342	30.534234
453.817615	17939.185919	30.539252
454.821742	17953.881195	30.544269
455.064335	17986.094108	30.549287
455.735021	18006.129386	30.554304
456.002320	18025.425546	30.559322
456.076032	18047.241144	30.564340
456.798811	18064.412811	30.569357
457.099914	18095.523812	30.574375
457.678662	18104.543205	30.579392
458.023890	18130.694413	30.584410
458.393919	18156.614340	30.589428
459.258678	18178.337771	30.594445
459.383988	18202.571400	30.599463
459.992703	18229.376402	30.604480
460.084895	18266.180937	30.609498
461.022898	18284.822673	30.614516
461.630570	18312.007008	30.619533
461.762682	18344.534747	30.624551
462.245015	18357.941141	30.629568
462.746005	18391.567304	30.634586
463.233438	18419.250761	30.639604
464.036179	18438.836206	30.644621
464.282463	18477.859766	30.649639
464.516263	18493.339463	30.654656
465.233795	18519.350752	30.659674
465.329440	18538.522685	30.664692
465.730817	18573.902123	30.669709
466.397107	18605.380026	30.674727
467.297098	18621.538873	30.679744
467.861056	18655.907437	30.684762
468.512052	18681.063838	30.689780
468.954544	18698.627446	30.694797
469.275832	18725.901441	30.699815
469.712586	18741.633846	30.704832
469.973341	18768.045535	30.709850
470.340293	18802.312541	30.714868
471.268769	18825.940998	30.719885
471.353511	18839.447907	30.724903
472.019292	18871.551780	30.729920
472.582671	18893.797053	30.734938
472.928607	18919.873399	30.739956
473.879990	18936.352986	30.744973
473.612783	18964.237550	30.749991
474.095863	18989.092126	30.755008
474.500034	19022.355477	30.760026
474.606720	19055.520168	30.765044
475.653493	19071.005665	30.770061
475.875805	19099.186501	30.775079
476.318492	19117.679180	30.780096
477.188833	19154.161341	30.785114
477.415852	19179.372160	30.790132
477.984399	19199.898512	30.795149
479.016520	19232.274131	30.800167
478.903756	19261.253195	30.805184
479.626228	19289.084296	30.810202
479.811848	19313.802658	30.815220
480.503626	19329.609318	30.820237
480.782287	19360.599498	30.825255
481.033290	19382.932165	30.830272
481.952868	19421.883748	30.835290
482.482714	19441.266550	30.840308
482.907374	19463.211986	30.845325
483.035791	19497.151133	30.850343
483.283501	19508.472233	30.855360
484.156405	19535.597783	30.860378
484.631654	19563.284777	30.865396
485.121798	19582.225360	30.870413
485.155073	19612.376172	30.875431
485.702478	19637.019324	30.880448
486.400231	19667.969623	30.885466
486.983695	19697.787988	30.890484
487.305570	19721.803177	30.895501
487.988565	19748.788182	30.900519
488.096262	19776.943722	30.905536
489.160996	19798.302790	30.910554
489.177726	19833.637354	30.915572
489.786038	19861.436609	30.920589
490.191372	19886.430869	30.925607
490.534747	19923.275003	30.930624
491.148004	19957.941410	30.935642
491.443722	19995.210141	30.940660
492.034377	20020.125000	30.945677
492.672089	20047.540826	30.950695
493.368455	20077.879131	30.955712
494.041171	20107.001781	30.960730
494.331275	20141.769674	30.965748
494.753095	20161.719793	30.970765
495.390286	20196.205965	30.975783
496.081899	20222.331000	30.980800
496.426579	20249.717188	30.985818
497.054095	20274.367551	30.990836
497.839171	20299.505044	30.995853
498.291645	20323.431015	31.000871
498.719156	20349.622858	31.005888
499.359966	20373.462528	31.010906
499.495285	20392.762749	31.015924
500.387633	20422.799208	31.020941
500.919667	20453.795663	31.025959
501.256701	20473.734108	31.030976
501.980102	20493.864790	31.035994
501.985568	20511.365796	31.041012
502.978789	20541.070723	31.046029
503.208257	20565.739570	31.051047
503.860943	20596.774218	31.056064
504.726756	20612.933762	31.061082
505.017259	20643.071143	31.066100
505.608662	20669.578935	31.071117
506.112139	20693.307819	31.076135
506.124145	20724.784208	31.081152
506.557312	20740.986348	31.086170
506.604555	20770.694465	31.091188
507.597180	20802.067935	31.096205
508.257490	20838.068031	31.101223
508.336956	20866.027365	31.106240
509.175386	20891.473183	31.111258
509.495257	20919.142201	31.116276
510.614217	20953.383651	31.121293
511.040945	20985.490530	31.126311
511.411974	21004.034129	31.131328
511.725164	21031.331563	31.136346
512.040031	21050.553761	31.141364
512.421315	21082.945929	31.146381
513.088340	21114.996427	31.151399
513.451893	21145.925586	31.156416
513.844055	21181.045806	31.161434
514.856684	21213.282438	31.166452
515.503316	21239.757076	31.171469
516.275417	21267.804371	31.176487
516.645328	21305.784281	31.181504
517.425446	21320.814175	31.186522
517.141688	21344.755606	31.191540
517.756905	21366.654373	31.196557
518.582193	21377.241596	31.201575
518.936872	21412.197498	31.206592
519.583951	21434.369368	31.211610
519.401734	21456.633240	31.216628
519.825391	21481.607705	31.221645
520.535269	21506.164575	31.226663
521.144878	21541.447258	31.231680
521.774980	21570.534525	31.236698
521.944991	21602.935364	31.241716
522.339920	21643.294137	31.246733
523.203564	21669.969155	31.251751
523.629554	21706.614132	31.256768
524.289956	21743.829058	31.261786
524.804995	21768.581058	31.266804
525.533239	21803.681342	31.271821
526.164298	21836.894974	31.276839
526.210399	21860.311460	31.281856
527.170578	21891.502191	31.286874
527.629234	21931.548272	31.291892
528.009662	21947.677524	31.296909
528.348543	21983.344612	31.301927
528.817091	22018.214245	31.306944
529.542846	22048.443573	31.311962
530.039311	22083.744946	31.316980
530.643827	22122.833386	31.321997
531.259291	22149.048738	31.327015
531.700730	22186.614734	31.332032
532.387386	22207.884002	31.337050
533.182696	22242.905056	31.342068
533.751984	22276.881046	31.347085
534.417875	22315.214628	31.352103
534.963617	22348.189727	31.357120
535.682918	22366.894903	31.362138
536.116146	22393.417153	31.367156
536.434673	22420.431321	31.372173
537.367173	22451.677825	31.377191
537.623706	22480.711202	31.382208
538.277472	22509.391735	31.387226
538.266251	22533.216086	31.392244
538.768775	22563.746561	31.397261
539.674086	22587.547489	31.402279
540.266970	22623.763612	31.407296
541.043946	22648.703173	31.412314
541.786348	22691.688912	31.417332
541.964513	22712.975175	31.422349
542.499556	22736.038079	31.427367
542.999115	22769.513996	31.432384
543.344494	22787.083840	31.437402
543.952802	22821.250543	31.442420
544.679456	22857.957984	31.447437
545.288616	22886.134206	31.452455
545.618177	22916.022493	31.457472
546.627080	22934.139410	31.462490
546.967633	22968.676895	31.467508
547.679257	23000.679236	31.472525
548.113630	23024.535493	31.477543
548.659579	23055.028328	31.482560
549.122108	23078.842325	31.487578
549.521476	23107.001165	31.492596
550.004876	23141.478662	31.497613
550.725857	23167.242816	31.502631
551.032348	23199.479547	31.507648
551.761912	23225.697412	31.512666
552.628470	23260.980832	31.517684
552.876799	23288.424241	31.522701
553.680638	23311.281417	31.527719
554.108633	23345.344560	31.532736
554.244206	23361.209991	31.537754
554.892127	23383.225938	31.542772
555.428917	23411.028767	31.547789
556.191242	23434.037929	31.552807
556.192729	23460.363816	31.557824
557.003454	23488.806329	31.562842
557.586031	23522.548559	31.567860
557.907523	23556.590828	31.572877
558.671047	23572.497101	31.577895
558.825947	23616.290934	31.582912
559.548009	23644.684363	31.587930
560.184894	23676.351937	31.592948
560.784154	23711.968711	31.597965
561.487804	23748.852023	31.602983
561.960289	23773.006536	31.608000
562.678858	23808.408896	31.613018
563.175112	23841.299435	31.618036
563.677795	23873.361183	31.623053
564.405946	23902.069995	31.628071
564.804841	23941.118387	31.633088
565.582916	23973.080289	31.638106
566.035794	23997.377172	31.643124
566.341042	24035.157573	31.648141
567.116642	24072.510492	31.653159
567.726596	24111.267063	31.658176
568.195779	24136.471562	31.663194
568.894258	24164.850468	31.668212
569.269370	24212.396477	31.673229
570.068571	24233.498625	31.678247
570.274011	24276.748832	31.683264
571.233551	24296.770579	31.688282
572.197901	24326.081279	31.693300
572.788081	24365.757771	31.698317
573.081857	24388.702391	31.703335
574.003424	24420.693094	31.708352
574.637767	24445.941631	31.713370
575.543449	24477.498864	31.718388
576.004350	24515.868793	31.723405
576.523375	24532.926375	31.728423
576.788221	24557.897986	31.733440
577.373559	24593.114059	31.738458
578.067687	24621.241512	31.743476
578.412813	24654.479358	31.748493
579.130539	24680.953779	31.753511
579.758313	24717.225121	31.758528
580.128037	24751.103878	31.763546
580.797562	24773.901616	31.768564
581.266578	24808.953016	31.773581
581.932117	24835.006077	31.778599
582.126086	24870.296571	31.783616
582.986971	24900.875617	31.788634
583.410406	24936.029173	31.793652
583.825862	24978.552834	31.798669
584.639970	25011.199604	31.803687
584.974928	25039.023671	31.808704
585.624634	25077.864365	31.813722
586.263426	25114.482286	31.818740
586.747047	25149.993337	31.823757
587.425406	25184.810374	31.828775
587.880629	25232.017623	31.833792
588.765333	25265.273091	31.838810
589.445782	25298.503726	31.843828
589.900650	25339.985527	31.848845
590.751546	25372.570246	31.853863
591.093899	25403.237589	31.858880
591.811625	25428.518546	31.863898
592.274660	25460.551126	31.868916
592.591656	25504.993601	31.873933
593.446389	25523.914376	31.878951
593.770835	25553.889566	31.883968
594.548186	25581.088947	31.888986
595.224569	25614.756815	31.894004
595.272447	25655.708935	31.899021
595.961411	25682.694779	31.904039
596.478352	25712.191340	31.909056
597.033025	25755.585952	31.914074
598.036863	25786.516839	31.919092
598.428034	25823.541391	31.924109
599.156291	25849.724987	31.929127
599.813188	25891.467003	31.934144
600.395208	25924.436007	31.939162
601.264874	25966.403977	31.944180
601.626372	25995.337535	31.949197
602.235989	26024.680999	31.954215
602.786999	26061.257512	31.959232
603.414796	26094.630429	31.964250
604.018837	26137.714768	31.969268
604.530645	26177.091107	31.974285
605.415073	26216.636688	31.979303
605.726242	26249.579122	31.984320
606.668516	26290.303971	31.989338
607.645406	26312.505469	31.994356
607.785805	26351.447344	31.999373
608.559585	26378.168031	32.004391
609.168762	26409.294409	32.009408
609.722095	26446.850882	32.014426
610.697489	26486.250022	32.019444
611.062534	26522.736412	32.024461
611.835845	26556.434914	32.029479
612.432177	26582.336753	32.034496
613.164097	26613.330458	32.039514
613.681901	26649.357056	32.044532
614.464851	26674.970657	32.049549
615.258349	26706.131827	32.054567
615.672954	26748.349659	32.059584
616.207270	26778.862623	32.064602
616.958416	26798.072595	32.069620
617.163070	26842.573528	32.074637
617.736607	26867.265804	32.079655
618.431835	26902.936410	32.084672
619.130210	26940.053942	32.089690
619.864397	26975.585847	32.094708
620.347678	27020.542840	32.099725
620.987148	27047.013671	32.104743
621.437968	27086.432933	32.109760
622.244698	27122.983958	32.114778
622.604342	27159.143678	32.119796
623.311963	27201.000542	32.124813
623.992589	27234.120570	32.129831
624.930178	27277.951472	32.134848
625.378079	27311.626350	32.139866
625.843799	27337.164064	32.144884
626.585802	27380.317927	32.149901
627.263183	27410.069940	32.154919
627.984591	27448.019098	32.159936
628.601478	27482.325126	32.164954
629.226257	27515.460680	32.169972
629.820223	27558.233593	32.174989
630.419829	27589.300078	32.180007
631.382317	27622.926484	32.185024
631.472017	27665.765956	32.190042
632.428593	27690.601505	32.195060
632.969553	27724.249852	32.200077
633.488642	27761.251591	32.205095
634.124271	27795.062205	32.210112
634.524379	27834.560386	32.215130
635.199105	27861.943248	32.220148
635.806129	27885.942573	32.225165
636.531577	27913.728402	32.230183
637.249162	27948.221705	32.235200
637.443292	27985.028238	32.240218
638.552100	28007.109810	32.245236
638.712278	28046.506922	32.250253
639.812636	28086.793462	32.255271
640.455976	28121.981322	32.260288
641.221739	28151.676335	32.265306
641.788699	28178.494995	32.270324
642.057466	28219.872783	32.275341
642.536600	28256.047342	32.280359
643.670339	28292.353314	32.285376
644.095674	28324.838780	32.290394
644.484543	28368.808535	32.295412
645.121633	28408.365525	32.300429
645.964747	28447.549003	32.305447
646.928361	28475.639623	32.310464
647.506698	28523.138654	32.315482
648.166088	28558.078240	32.320500
648.662728	28602.246528	32.325517
649.495466	28642.873159	32.330535
650.259401	28672.000339	32.335552
650.768117	28710.933290	32.340570
651.560404	28749.543787	32.345588
651.965490	28790.762320	32.350605
652.372108	28821.614392	32.355623
653.217276	28861.910824	32.360640
653.405271	28907.152096	32.365658
654.848114	28941.192166	32.370676
655.264150	28987.169058	32.375693
655.751834	29024.361312	32.380711
656.785131	29071.328932	32.385728
657.428755	29114.230069	32.390746
658.286048	29147.508850	32.395764
658.728843	29188.115459	32.400781
659.555539	29226.304279	32.405799
660.523394	29264.957784	32.410816
660.387292	29308.196354	32.415834
661.599125	29344.093741	32.420852
662.056509	29378.743989	32.425869
662.860080	29416.797721	32.430887
663.771898	29451.522310	32.435904
664.331344	29490.493045	32.440922
664.745028	29526.174407	32.445940
664.915025	29569.618434	32.450957
665.763300	29611.116871	32.455975
666.560786	29662.661369	32.460992
667.397036	29709.313645	32.466010
667.916800	29736.129097	32.471028
668.662709	29779.104101	32.476045
669.592095	29811.841689	32.481063
670.227807	29856.471309	32.486080
670.607454	29892.778118	32.491098
671.519495	29933.578205	32.496116
672.671595	29979.916139	32.501133
673.093141	30015.812042	32.506151
673.366593	30047.053444	32.511168
673.897281	30094.171652	32.516186
674.816196	30125.122449	32.521204
675.327641	30171.624359	32.526221
676.027750	30206.547734	32.531239
676.736126	30249.870952	32.536256
677.564943	30285.690901	32.541274
678.112488	30327.484413	32.546292
678.825379	30356.634624	32.551309
679.298779	30400.595489	32.556327
680.521501	30432.143953	32.561344
680.789181	30479.677193	32.566362
681.335893	30501.236318	32.571380
681.885802	30526.290721	32.576397
682.724960	30562.533069	32.581415
683.588483	30600.339387	32.586432
684.102512	30645.160450	32.591450
684.987066	30673.152681	32.596468
685.766110	30711.023004	32.601485
686.520142	30749.927719	32.606503
687.004317	30786.561092	32.611520
687.614495	30811.024822	32.616538
688.390880	30843.490901	32.621556
688.929144	30891.874050	32.626573
689.496763	30931.408847	32.631591
690.585324	30966.639326	32.636608
690.892904	31008.762588	32.641626
691.842898	31043.907433	32.646644
692.137708	31080.627877	32.651661
692.787391	31121.964487	32.656679
694.168928	31166.157737	32.661696
694.223112	31202.732752	32.666714
695.130642	31248.049801	32.671732
695.792975	31295.915052	32.676749
696.312968	31343.056745	32.681767
697.592130	31378.852318	32.686784
697.632799	31426.556035	32.691802
698.422483	31463.022648	32.696820
699.740363	31507.808196	32.701837
700.549484	31553.988438	32.706855
701.193016	31590.920686	32.711872
701.921407	31633.516665	32.716890
702.543155	31676.628854	32.721908
703.649405	31700.269978	32.726925
704.024999	31738.799612	32.731943
705.062033	31777.952742	32.736960
705.623435	31809.385616	32.741978
706.225181	31851.262221	32.746996
706.925878	31877.925681	32.752013
707.859144	31924.333858	32.757031
708.813856	31954.510526	32.762048
708.901272	31995.557617	32.767066
709.465475	32037.743927	32.772084
710.347840	32076.365515	32.777101
710.885966	32122.570494	32.782119
711.926646	32161.382393	32.787136
712.397064	32212.763196	32.792154
713.160315	32248.053123	32.797172
714.370803	32283.431121	32.802189
714.958067	32316.927996	32.807207
715.538382	32345.842570	32.812224
716.217882	32398.202607	32.817242
717.129571	32435.410462	32.822260
718.018497	32479.032488	32.827277
718.716048	32506.057603	32.832295
719.205361	32541.175977	32.837312
720.064487	32588.103008	32.842330
720.849641	32611.890289	32.847348
721.712334	32651.698253	32.852365
722.066031	32690.245719	32.857383
722.644432	32730.768497	32.862400
723.454543	32771.293000	32.867418
724.024691	32798.237291	32.872436
725.001974	32834.158517	32.877453
725.197932	32876.094405	32.882471
726.143453	32914.935256	32.887488
726.578570	32956.599933	32.892506
727.177526	32997.309674	32.897524
727.834894	33033.401462	32.902541
728.179637	33079.992886	32.907559
729.307029	33108.070500	32.912576
729.875857	33157.895595	32.917594
730.587805	33194.902161	32.922612
731.919558	33236.882184	32.927629
732.317546	33275.019166	32.932647
733.328582	33313.161369	32.937664
733.842683	33349.080148	32.942682
734.646382	33397.364325	32.947700
735.216667	33434.418789	32.952717
736.199490	33484.736192	32.957735
736.852495	33516.719981	32.962752
737.148328	33563.143111	32.967770
737.932361	33612.094710	32.972788
739.175059	33649.139089	32.977805
739.885862	33705.701881	32.982823
740.478606	33745.592136	32.987840
741.147666	33781.177589	32.992858
741.803716	33824.731409	32.997876
742.705534	33866.015008	33.002893
743.543177	33906.676491	33.007911
744.236747	33953.455480	33.012928
744.987372	33997.051749	33.017946
745.843001	34048.193378	33.022964
746.465630	34091.980596	33.027981
747.143181	34136.853101	33.032999
748.114696	34190.992777	33.038016
748.918577	34232.583270	33.043034
749.461951	34280.119922	33.048052
750.505856	34310.747578	33.053069
751.585639	34360.780026	33.058087
751.955228	34401.193310	33.063104
752.740999	34449.368904	33.068122
753.367002	34492.473582	33.073140
754.405885	34535.766598	33.078157
754.809777	34587.125698	33.083175
755.865937	34634.146583	33.088192
756.661769	34677.281948	33.093210
757.206547	34717.756921	33.098228
758.292601	34761.770126	33.103245
758.742920	34813.596709	33.108263
759.710299	34846.026462	33.113280
760.654289	34897.295415	33.118298
761.387468	34940.656104	33.123316
762.182086	34972.936069	33.128333
762.944868	35023.316901	33.133351
763.624304	35063.246657	33.138368
764.597127	35106.336214	33.143386
764.799143	35155.161241	33.148404
766.082006	35187.896195	33.153421
766.738238	35229.537066	33.158439
767.481435	35280.857361	33.163456
768.390627	35316.230762	33.168474
768.742842	35366.948590	33.173492
769.801673	35404.050148	33.178509
770.435974	35457.759015	33.183527
771.341507	35496.180940	33.188544
772.056800	35549.592825	33.193562
772.786088	35598.241458	33.198580
773.334415	35636.441364	33.203597
773.954479	35681.667593	33.208615
774.791665	35729.534549	33.213632
776.000520	35773.246095	33.218650
776.278381	35817.900223	33.223668
777.226153	35851.017477	33.228685
778.098137	35905.430052	33.233703
779.183443	35937.843015	33.238720
779.875274	35972.018551	33.243738
780.432015	35998.589655	33.248756
781.486472	36032.525134	33.253773
781.954929	36079.578033	33.258791
782.587935	36117.898330	33.263808
783.497789	36157.250275	33.268826
784.334177	36189.165136	33.273844
785.608769	36222.788230	33.278861
786.130370	36270.218941	33.283879
786.929680	36298.908635	33.288896
787.707105	36338.262684	33.293914
788.209288	36371.216570	33.298932
789.031179	36418.404568	33.303949
790.158642	36450.482907	33.308967
790.768711	36493.448715	33.313984
791.509383	36543.552073	33.319002
792.051663	36587.932448	33.324020
792.977739	36626.321586	33.329037
793.890741	36676.246511	33.334055
794.593383	36719.868548	33.339072
795.178169	36761.390820	33.344090
795.718739	36819.101487	33.349108
796.657973	36863.034551	33.354125
797.374514	36912.851680	33.359143
798.382823	36966.158001	33.364160
799.258530	37005.573773	33.369178
800.064593	37046.239908	33.374196
800.972938	37093.934381	33.379213
801.676472	37143.134390	33.384231
802.393527	37187.229381	33.389248
804.004744	37232.929716	33.394266
804.593434	37292.505866	33.399284
805.541929	37328.325429	33.404301
805.986507	37374.657721	33.409319
806.897095	37410.179830	33.414336
807.948947	37455.203089	33.419354
808.512111	37508.656352	33.424372
809.542580	37552.165516	33.429389
810.481751	37594.209353	33.434407
810.922858	37640.624969	33.439424
812.170728	37677.719865	33.444442
812.922234	37718.364203	33.449460
813.499011	37766.554747	33.454477
814.418646	37809.430459	33.459495
814.930903	37853.343887	33.464512
816.030406	37902.072597	33.469530
816.504746	37943.121211	33.474548
817.727609	37982.130295	33.479565
818.411354	38034.041979	33.484583
819.413860	38076.810393	33.489600
820.161177	38110.835219	33.494618
821.034848	38162.262165	33.499636
821.532487	38195.447226	33.504653
822.490557	38250.990565	33.509671
823.111996	38298.517638	33.514688
824.569302	38338.831298	33.519706
825.142160	38384.178142	33.524724
826.133564	38424.704042	33.529741
826.883953	38465.109664	33.534759
827.401526	38515.663615	33.539776
828.657066	38558.703234	33.544794
829.021777	38605.303637	33.549812
830.220198	38660.234926	33.554829
830.904225	38693.606579	33.559847
831.450028	38742.778036	33.564864
832.501400	38777.413990	33.569882
833.168205	38823.739900	33.574900
833.972262	38860.526903	33.579917
834.569821	38897.390572	33.584935
835.472149	38936.369372	33.589952
836.268111	38968.718415	33.594970
837.002588	39010.917232	33.599988
837.771603	39054.160505	33.605005
838.714016	39108.918010	33.610023
839.225631	39149.084046	33.615040
840.199677	39191.776920	33.620058
841.288783	39245.240671	33.625076
841.904733	39287.521829	33.630093
842.936783	39337.257227	33.635111
843.243983	39395.700670	33.640128
844.506392	39429.937831	33.645146
845.457517	39481.962907	33.650164
846.092337	39527.827349	33.655181
846.970663	39582.222964	33.660199
847.505019	39631.581633	33.665216
848.472534	39679.247276	33.670234
849.170991	39744.542707	33.675252
850.275241	39794.059150	33.680269
851.190482	39846.501794	33.685287
851.807829	39904.980257	33.690304
852.789679	39954.990551	33.695322
853.674015	40011.625084	33.700340
854.276266	40076.221935	33.705357
855.155316	40132.686855	33.710375
855.804793	40195.758833	33.715392
857.019442	40252.981028	33.720410
857.970377	40303.357452	33.725428
859.261333	40357.696720	33.730445
860.049793	40412.557515	33.735463
860.699614	40464.221040	33.740480
861.913956	40515.663479	33.745498
862.953404	40570.605534	33.750516
863.642839	40628.239827	33.755533
864.503089	40679.801344	33.760551
865.286741	40739.590467	33.765568
866.621369	40778.523860	33.770586
867.652067	40836.819934	33.775604
868.409747	40884.476805	33.780621
869.591017	40930.745626	33.785639
870.280743	40977.091514	33.790656
871.182487	41014.126180	33.795674
871.895930	41063.384156	33.800692
872.813036	41107.999733	33.805709
873.456540	41153.455142	33.810727
874.652292	41199.646371	33.815744
875.642592	41247.185389	33.820762
876.207453	41302.810765	33.825780
876.975467	41348.367250	33.830797
878.301317	41393.830158	33.835815
878.744935	41453.181153	33.840832
879.601768	41485.897571	33.845850
880.503677	41545.063209	33.850868
881.128198	41587.233644	33.855885
882.844349	41633.888231	33.860903
883.468728	41693.135673	33.865920
884.327234	41726.851501	33.870938
885.065906	41782.109340	33.875956
885.880929	41836.975875	33.880973
886.916041	41866.856741	33.885991
887.712022	41917.659614	33.891008
888.719480	41965.437848	33.896026
889.636581	42017.967641	33.901044
890.157395	42062.811663	33.906061
891.204850	42113.657836	33.911079
891.845328	42163.138430	33.916096
892.980051	42201.675573	33.921114
894.214978	42242.037640	33.926132
894.492472	42280.468803	33.931149
895.220224	42326.236021	33.936167
895.974640	42384.079804	33.941184
896.977561	42427.248868	33.946202
897.700339	42471.796451	33.951220
898.391396	42525.147146	33.956237
899.683684	42572.192677	33.961255
900.107356	42619.045417	33.966272
900.725379	42673.046732	33.971290
901.820066	42731.521250	33.976308
902.520301	42786.338551	33.981325
903.690749	42847.350513	33.986343
904.336504	42915.617463	33.991360
905.669950	42966.914184	33.996378
906.508734	43023.057627	34.001396
907.322749	43078.831907	34.006413
908.394010	43136.900033	34.011431
908.931557	43189.688130	34.016448
910.438441	43255.620130	34.021466
911.578266	43315.151759	34.026484
912.322514	43365.921795	34.031501
913.501293	43417.275407	34.036519
914.153826	43464.309160	34.041536
915.548161	43511.435596	34.046554
916.631440	43568.794544	34.051572
917.552672	43622.794978	34.056589
918.387448	43656.504827	34.061607
919.561808	43709.023666	34.066624
920.556901	43756.042352	34.071642
921.503211	43801.664550	34.076660
922.549233	43857.436090	34.081677
923.537786	43896.049687	34.086695
924.366270	43939.811981	34.091712
925.601516	43985.098346	34.096730
926.414106	44035.277277	34.101748
926.994797	44089.237287	34.106765
928.071467	44126.376313	34.111783
928.747258	44177.772494	34.116800
929.830908	44224.639148	34.121818
931.106519	44278.345321	34.126836
932.004823	44326.696074	34.131853
932.784122	44369.062654	34.136871
933.666339	44429.807832	34.141888
934.961739	44467.653268	34.146906
935.656222	44518.724707	34.151924
935.992791	44567.802820	34.156941
937.100253	44613.173731	34.161959
938.405543	44662.271162	34.166976
938.818253	44717.018067	34.171994
939.777160	44761.723049	34.177012
940.674890	44820.341453	34.182029
942.289238	44870.662406	34.187047
942.672340	44917.937517	34.192064
943.528304	44959.837768	34.197082
944.764079	45020.231888	34.202100
945.642244	45074.989023	34.207117
946.617691	45130.578708	34.212135
947.441155	45184.149114	34.217152
948.181972	45234.740505	34.222170
949.047614	45279.714158	34.227188
949.965466	45344.656557	34.232205
951.545157	45397.305691	34.237223
951.915075	45453.769064	34.242240
953.401934	45504.035499	34.247258
953.890439	45554.882198	34.252276
954.818659	45598.701717	34.257293
956.047252	45652.083291	34.262311
956.716432	45696.671036	34.267328
957.397808	45743.123101	34.272346
958.804330	45778.543198	34.277364
959.228967	45828.894445	34.282381
960.584610	45883.458604	34.287399
961.323323	45933.628064	34.292416
962.480053	45984.478650	34.297434
963.384235	46041.593660	34.302452
964.138542	46092.444240	34.307469
965.134188	46145.268819	34.312487
966.287466	46200.485383	34.317504
967.041489	46245.472126	34.322522
968.437695	46294.773994	34.327540
969.043074	46351.696188	34.332557
970.060220	46393.852232	34.337575
970.800053	46454.764370	34.342592
971.813673	46517.335530	34.347610
972.835841	46571.428507	34.352628
973.653700	46631.696293	34.357645
974.982416	46687.803876	34.362663
976.020553	46742.274333	34.367680
976.743005	46809.155738	34.372698
978.338492	46859.053936	34.377716
979.043906	46910.957843	34.382733
980.318813	46966.283767	34.387751
981.059053	47028.184283	34.392768
981.790130	47073.549520	34.397786
983.161015	47126.355605	34.402804
984.017344	47186.821290	34.407821
985.437480	47235.855769	34.412839
985.823268	47300.317749	34.417856
986.972372	47345.618080	34.422874
987.895391	47394.559927	34.427892
988.917282	47460.567621	34.432909
990.303125	47513.258393	34.437927
991.512580	47570.063767	34.442944
992.172783	47635.002498	34.447962
993.145683	47684.101648	34.452980
994.182649	47744.122993	34.457997
995.478299	47789.154536	34.463015
996.750069	47850.967750	34.468032
997.157528	47893.658583	34.473050
998.352471	47945.133930	34.478068
999.226161	48014.494186	34.483085
1000.227180	48069.846712	34.488103
1001.659849	48122.461979	34.493120
1002.915492	48183.032289	34.498138
1003.758010	48224.371329	34.503156
1003.959466	48286.486167	34.508173
1005.818730	48348.689575	34.513191
1006.315774	48397.795180	34.518208
1007.069997	48450.871724	34.523226
1008.599760	48508.723808	34.528244
1009.229615	48558.707353	34.533261
1010.029136	48614.630521	34.538279
1011.378416	48666.697028	34.543296
1012.344784	48740.676141	34.548314
1013.537871	48788.300706	34.553332
1014.376615	48843.307241	34.558349
1015.582953	48897.174476	34.563367
1016.817904	48949.797306	34.568384
1017.275782	49007.546430	34.573402
1018.595149	49057.113096	34.578420
1019.636440	49114.783799	34.583437
1020.684174	49160.438945	34.588455
1021.821967	49225.756637	34.593472
1023.013644	49272.439730	34.598490
1023.542739	49307.907846	34.603508
1024.595331	49370.151767	34.608525
1025.590148	49402.434273	34.613543
1026.221882	49437.576500	34.618560
1027.602510	49493.904337	34.623578
1028.746804	49538.982023	34.628596
1029.509275	49592.528121	34.633613
1030.382096	49644.102029	34.638631
1031.498827	49692.670502	34.643648
1032.026675	49744.456822	34.648666
1033.120144	49794.788063	34.653684
1034.197760	49851.436283	34.658701
1035.743330	49910.820591	34.663719
1036.641101	49965.510554	34.668736
1037.309822	50021.906861	34.673754
1038.776890	50079.892957	34.678772
1039.551578	50135.349193	34.683789
1040.847060	50198.107792	34.688807
1041.956279	50244.596982	34.693824
1042.750564	50318.152573	34.698842
1044.088653	50363.770983	34.703860
1044.827219	50434.678253	34.708877
1046.205352	50483.340343	34.713895
1047.231169	50542.972169	34.718912
1048.033454	50598.418872	34.723930
1049.214785	50656.640976	34.728948
1050.387364	50715.155653	34.733965
1051.576423	50775.173793	34.738983
1052.743805	50828.178497	34.744000
1053.721270	50895.019282	34.749018
1054.981666	50953.210774	34.754036
1056.150715	50999.046730	34.759053
1056.800377	51064.414434	34.764071
1057.952889	51125.692028	34.769088
1058.810260	51178.708109	34.774106
1059.936613	51240.654481	34.779124
1061.137643	51303.975035	34.784141
1062.267198	51367.294299	34.789159
1063.643396	51420.932052	34.794176
1064.617332	51478.144664	34.799194
1066.041557	51525.764030	34.804212
1066.716950	51587.104890	34.809229
1068.033787	51645.839782	34.814247
1069.134406	51693.902467	34.819264
1069.971162	51751.213161	34.824282
1071.303728	51810.831867	34.829300
1072.127117	51867.765287	34.834317
1073.105631	51919.783319	34.839335
1073.967044	51977.767765	34.844352
1075.140123	52045.486091	34.849370
1076.340005	52096.216987	34.854388
1077.115891	52161.637622	34.859405
1078.612657	52219.390316	34.864423
1079.843069	52268.104603	34.869440
1080.534986	52333.962824	34.874458
1081.751425	52397.296604	34.879476
1082.891853	52447.290901	34.884493
1084.020184	52505.987876	34.889511
1085.311448	52562.267588	34.894528
1086.241912	52616.199361	34.899546
1087.446940	52671.847404	34.904564
1088.559862	52732.989898	34.909581
1090.097132	52781.834397	34.914599
1090.960366	52835.467139	34.919616
1091.965100	52892.513883	34.924634
1092.948227	52941.964361	34.929652
1094.338524	52998.843427	34.934669
1095.428092	53044.752819	34.939687
1096.274496	53089.023471	34.944704
1097.303992	53135.796717	34.949722
1098.640701	53171.131655	34.954740
1099.337758	53214.786805	34.959757
1100.379603	53264.456579	34.964775
1101.575713	53307.103558	34.969792
1102.311395	53357.947844	34.974810
1103.050840	53411.177311	34.979828
1104.193177	53461.477227	34.984845
1105.256345	53512.916036	34.989863
1106.307450	53573.418617	34.994880
1107.329997	53639.791946	34.999898
1108.541111	53689.126044	35.004916
1109.309390	53749.774607	35.009933
1110.990703	53817.102094	35.014951
1112.143364	53875.703775	35.019968
1112.690652	53933.419516	35.024986
1114.195427	54003.262138	35.030004
1115.360029	54067.741297	35.035021
1116.545193	54129.875979	35.040039
1117.876282	54190.064201	35.045056
1118.863034	54245.446402	35.050074
1120.047094	54305.955365	35.055092
1121.167959	54358.045130	35.060109
1122.466497	54436.445498	35.065127
1123.642914	54484.717219	35.070144
1124.306161	54556.541093	35.075162
1125.727587	54615.355671	35.080180
1127.110625	54666.538090	35.085197
1128.071740	54734.088536	35.090215
1129.487911	54788.392245	35.095232
1130.532460	54847.620794	35.100250
1132.204307	54904.947686	35.105268
1133.214445	54965.827305	35.110285
1134.035407	55019.952608	35.115303
1135.366497	55074.776571	35.120320
1136.674648	55147.925178	35.125338
1138.133223	55206.286091	35.130356
1139.149743	55251.875820	35.135373
1140.148273	55309.334420	35.140391
1141.475704	55359.065159	35.145408
1142.586141	55424.499454	35.150426
1143.750365	55471.977704	35.155444
1144.730672	55531.895178	35.160461
1145.816342	55586.587877	35.165479
1147.041195	55642.087960	35.170496
1148.078103	55699.554154	35.175514
1149.397975	55758.476074	35.180532
1150.574826	55807.060530	35.185549
1151.363722	55867.736613	35.190567
1153.014225	55915.114306	35.195584
1154.384501	55971.522708	35.200602
1155.600661	56023.405031	35.205620
1157.021029	56078.324927	35.210637
1158.040497	56129.415540	35.215655
1158.907758	56179.903546	35.220672
1159.987271	56236.294809	35.225690
1161.118755	56287.849212	35.230708
1161.895538	56345.262758	35.235725
1163.170783	56391.947025	35.240743
1164.315800	56453.954856	35.245760
1165.456296	56514.248441	35.250778
1166.441197	56580.705525	35.255796
1167.779803	56630.411861	35.260813
1169.256354	56690.760872	35.265831
1170.200053	56754.781941	35.270848
1171.498229	56800.090047	35.275866
1172.407419	56858.610644	35.280884
1173.562535	56896.220038	35.285901
1174.409968	56949.016508	35.290919
1175.309271	56990.286259	35.295936
1176.213137	57050.010660	35.300954
1177.313361	57109.552574	35.305972
1178.587175	57163.605525	35.310989
1179.440035	57228.857252	35.316007
1180.577705	57287.222875	35.321024
1181.854479	57355.218674	35.326042
1182.989649	57413.439428	35.331060
1184.670083	57477.745822	35.336077
1185.832111	57548.639870	35.341095
1186.890695	57601.942695	35.346112
1188.077553	57668.016745	35.351130
1189.714050	57737.121873	35.356148
1190.921442	57789.737257	35.361165
1192.085925	57856.226724	35.366183
1192.990264	57914.731667	35.371200
1194.775994	57972.003814	35.376218
1195.804047	58033.894800	35.381236
1196.853075	58090.042030	35.386253
1197.711445	58159.517028	35.391271
1198.794766	58222.077076	35.396288
1200.056336	58289.261419	35.401306
1201.219799	58357.467669	35.406324
1203.154328	58426.692682	35.411341
1204.045495	58501.733350	35.416359
1205.566306	58562.877638	35.421376
1206.914704	58619.384313	35.426394
1207.932163	58687.506752	35.431412
1209.270724	58737.432660	35.436429
1210.457072	58809.535527	35.441447
1212.002109	58877.487296	35.446464
1212.881845	58934.530127	35.451482
1214.309172	58996.177516	35.456500
1215.640892	59054.700596	35.461517
1216.987323	59116.139422	35.466535
1217.918177	59180.023368	35.471552
1219.238127	59250.929338	35.476570
1220.267583	59307.253355	35.481588
1221.820050	59364.375439	35.486605
1222.992573	59435.406301	35.491623
1224.287637	59494.094420	35.496640
1225.357540	59544.133675	35.501658
1226.655068	59615.594898	35.506676
1228.320659	59673.263339	35.511693
1229.049462	59742.269441	35.516711
1230.182069	59802.711740	35.521728
1231.871817	59864.275946	35.526746
1232.870398	59918.694640	35.531764
1234.233589	59982.190194	35.536781
1235.307428	60046.016050	35.541799
1236.505087	60115.209330	35.546816
1237.880143	60167.955551	35.551834
1239.092822	60234.722508	35.556852
1240.726075	60284.004134	35.561869
1241.830551	60359.466558	35.566887
1243.029760	60408.398614	35.571904
1244.211397	60461.884693	35.576922
1245.426206	60532.658937	35.581940
1246.975176	60580.359226	35.586957
1247.777825	60644.912730	35.591975
1249.366258	60706.393644	35.596992
1250.912527	60764.729001	35.602010
1251.581594	60828.810165	35.607028
1253.002221	60876.828632	35.612045
1253.906961	60936.385232	35.617063
1255.029003	60996.262439	35.622080
1256.762225	61043.282798	35.627098
1257.482448	61098.197123	35.632116
1258.957364	61143.757894	35.637133
1259.683934	61206.685304	35.642151
1260.686131	61255.016889	35.647168
1262.252874	61316.977487	35.652186
1262.943143	61370.631093	35.657204
1263.989327	61431.458091	35.662221
1265.397159	61501.793457	35.667239
1266.691533	61568.449976	35.672256
1268.369468	61631.413115	35.677274
1269.566609	61701.611120	35.682292
1271.043789	61765.239048	35.687309
1272.231715	61821.138913	35.692327
1273.554603	61893.792895	35.697344
1275.080238	61965.750676	35.702362
1275.851141	62031.091406	35.707380
1277.654607	62098.347003	35.712397
1278.493933	62171.704198	35.717415
1279.996031	62238.652857	35.722432
1281.649225	62293.556732	35.727450
1282.694280	62368.047087	35.732468
1283.923427	62425.277573	35.737485
1285.191388	62497.150630	35.742503
1286.607558	62567.063591	35.747520
1288.260363	62636.218038	35.752538
1289.208142	62702.279840	35.757556
1290.926851	62766.847426	35.762573
1291.804869	62839.675114	35.767591
1293.520162	62898.185313	35.772608
1294.612107	62967.403159	35.777626
1295.861149	63039.312402	35.782644
1297.231739	63108.278114	35.787661
1298.367853	63178.008736	35.792679
1299.907573	63244.169233	35.797696
1301.720354	63307.026905	35.802714
1302.881240	63377.279648	35.807732
1304.414708	63432.299750	35.812749
1305.212699	63502.331105	35.817767
1306.627111	63567.423207	35.822784
1308.332167	63625.968378	35.827802
1309.837610	63699.611980	35.832820
1310.971085	63760.108165	35.837837
1312.329237	63813.630853	35.842855
1313.784718	63877.311915	35.847872
1315.164719	63935.465545	35.852890
1316.579119	64000.723380	35.857908
1317.739441	64063.653444	35.862925
1318.721105	64128.631160	35.867943
1319.913575	64180.756140	35.872960
1321.402733	64252.219790	35.877978
1322.775642	64321.644315	35.882996
1324.059641	64383.068073	35.888013
1325.642184	64444.609850	35.893031
1326.667659	64510.005866	35.898048
1327.948279	64573.924994	35.903066
1329.124821	64646.806183	35.908084
1330.637002	64702.978318	35.913101
1332.256988	64769.079644	35.918119
1333.412866	64835.475379	35.923136
1334.785775	64892.992916	35.928154
1336.126914	64951.541181	35.933172
1337.616503	65018.075091	35.938189
1338.929905	65082.978024	35.943207
1340.546155	65151.512062	35.948224
1341.813658	65205.191199	35.953242
1342.830060	65265.183863	35.958260
1344.087605	65323.714425	35.963277
1345.308921	65376.666749	35.968295
1346.055403	65429.307315	35.973312
1347.285866	65480.808597	35.978330
1348.762690	65545.870745	35.983348
1350.055192	65604.421811	35.988365
1351.294378	65667.419521	35.993383
1352.110747	65729.970747	35.998400
1353.638961	65787.630629	36.003418
1355.129874	65871.615428	36.008436
1356.432455	65934.673525	36.013453
1357.911502	66006.207054	36.018471
1359.069764	66068.135782	36.023488
1360.598804	66144.087446	36.028506
1361.851907	66213.884163	36.033524
1363.618287	66286.570127	36.038541
1364.746112	66359.413237	36.043559
1366.152374	66426.989585	36.048576
1367.955473	66493.592273	36.053594
1369.092001	66560.723681	36.058612
1370.380015	66624.203647	36.063629
1371.856299	66701.038973	36.068647
1373.395403	66779.055013	36.073664
1374.756763	66846.417904	36.078682
1376.205763	66923.112547	36.083700
1377.623117	66987.212654	36.088717
1378.867799	67051.206990	36.093735
1380.341183	67135.262028	36.098752
1381.927589	67200.754479	36.103770
1383.597109	67272.996222	36.108788
1384.843029	67342.353949	36.113805
1386.376461	67411.210983	36.118823
1387.774666	67485.287645	36.123840
1389.269356	67551.016959	36.128858
1390.865491	67624.797115	36.133876
1392.116367	67681.314355	36.138893
1393.662646	67749.606770	36.143911
1394.769798	67822.299002	36.148928
1396.394013	67879.689005	36.153946
1397.741237	67951.482909	36.158964
1399.022466	68025.022250	36.163981
1400.575735	68089.363451	36.168999
1402.208163	68155.440002	36.174016
1404.085375	68220.262698	36.179034
1405.132738	68281.087096	36.184052
1406.682296	68343.453984	36.189069
1408.282169	68399.253336	36.194087
1409.357745	68468.400165	36.199104
1410.895595	68533.112143	36.204122
1412.297594	68599.080271	36.209140
1413.379628	68661.825045	36.214157
1414.960627	68732.615756	36.219175
1416.024420	68795.205411	36.224192
1417.577955	68862.727154	36.229210
1418.630398	68940.711982	36.234228
1419.783083	69007.600328	36.239245
1421.761900	69071.864716	36.244263
1423.197672	69153.266468	36.249280
1425.033616	69222.074678	36.254298
1426.580372	69289.060373	36.259316
1427.804186	69357.869778	36.264333
1429.221992	69424.819020	36.269351
1430.565209	69491.267208	36.274368
1431.803829	69544.320453	36.279386
1433.281951	69634.784724	36.284404
1434.690452	69698.418075	36.289421
1436.239415	69760.275578	36.294439
1437.014732	69839.629920	36.299456
1439.010700	69907.465073	36.304474
1440.135901	69954.489630	36.309492
1441.405939	70026.364713	36.314509
1442.762615	70078.571047	36.319527
1444.323486	70149.527095	36.324544
1445.466603	70203.058894	36.329562
1446.662997	70264.814479	36.334580
1447.850200	70341.515962	36.339597
1449.526292	70401.715019	36.344615
1451.039177	70482.026039	36.349632
1452.114038	70561.266037	36.354650
1453.713558	70615.905072	36.359668
1455.027481	70690.789345	36.364685
1456.451485	70774.636005	36.369703
1457.651943	70849.107885	36.374720
1459.429613	70926.795184	36.379738
1461.178346	71008.020778	36.384756
1462.293379	71093.753247	36.389773
1464.101313	71163.634851	36.394791
1465.418074	71260.164929	36.399808
1467.226089	71337.709383	36.404826
1468.627717	71405.210852	36.409844
1470.236591	71487.143745	36.414861
1472.071118	71565.685277	36.419879
1473.363706	71646.376315	36.424896
1475.165997	71710.915504	36.429914
1476.557644	71794.175220	36.434932
1477.916601	71872.931429	36.439949
1479.619126	71944.199477	36.444967
1480.993645	72028.121218	36.449984
1482.457134	72097.666594	36.455002
1484.275337	72177.580388	36.460020
1485.479748	72257.425843	36.465037
1487.272657	72332.315822	36.470055
1488.434009	72420.641821	36.475072
1490.121392	72493.889573	36.480090
1491.655554	72569.808653	36.485108
1493.181866	72642.461407	36.490125
1494.767357	72717.182292	36.495143
1495.875549	72807.481105	36.500160
1497.973836	72868.202376	36.505178
1499.744113	72959.664667	36.510196
1500.905036	73036.048814	36.515213
1502.587011	73099.609626	36.520231
1503.833876	73182.377073	36.525248
1505.729336	73255.759026	36.530266
1506.984410	73321.717748	36.535284
1508.671088	73403.163100	36.540301
1510.222189	73476.992214	36.545319
1511.981355	73553.778195	36.550336
1513.745375	73626.928423	36.555354
1515.149114	73691.724832	36.560372
1516.189011	73767.788035	36.565389
1518.164750	73824.135469	36.570407
1519.750146	73900.734322	36.575424
1520.969120	73973.033500	36.580442
1522.891004	74043.956211	36.585460
1524.105581	74111.709198	36.590477
1525.819860	74174.494872	36.595495
1527.453546	74250.884509	36.600512
1528.721397	74326.090299	36.605530
1530.668183	74393.108734	36.610548
1531.651023	74463.026874	36.615565
1533.125234	74522.658948	36.620583
1534.610091	74596.843533	36.625600
1536.478558	74672.564292	36.630618
1538.336869	74733.238724	36.635636
1539.922322	74804.862120	36.640653
1541.366550	74855.518864	36.645671
1542.544793	74917.604839	36.650688
1543.644708	74965.858311	36.655706
1545.155447	75027.284490	36.660724
1546.412167	75086.559186	36.665741
1547.977950	75155.349202	36.670759
1549.236255	75220.121412	36.675776
1550.675623	75287.968861	36.680794
1552.218625	75353.608859	36.685812
1553.469570	75425.818284	36.690829
1554.949903	75488.200308	36.695847
1556.520266	75579.474854	36.700864
1557.943959	75662.804989	36.705882
1559.438956	75739.524585	36.710900
1560.723198	75826.385878	36.715917
1562.642073	75907.105806	36.720935
1563.412567	75993.224667	36.725952
1565.521323	76083.187915	36.730970
1567.366019	76175.510934	36.735988
1569.125377	76268.886359	36.741005
1570.569616	76352.747438	36.746023
1572.341278	76444.018731	36.751040
1573.893604	76523.290426	36.756058
1575.618393	76608.641168	36.761076
1577.309120	76698.253853	36.766093
1579.086610	76781.874085	36.771111
1580.587164	76866.361323	36.776128
1581.918806	76958.855981	36.781146
1583.878040	77032.656320	36.786164
1585.509826	77119.834725	36.791181
1587.430818	77202.838400	36.796199
1588.907506	77285.531828	36.801216
1590.708613	77365.299095	36.806234
1592.578114	77448.628278	36.811252
1594.071558	77525.517849	36.816269
1595.706966	77599.142382	36.821287
1597.062330	77681.526626	36.826304
1598.669056	77772.840855	36.831322
1600.178120	77853.554697	36.836340
1601.652749	77941.419069	36.841357
1603.884138	78017.915826	36.846375
1605.043675	78111.239422	36.851392
1606.725742	78199.236842	36.856410
1608.746435	78270.205859	36.861428
1609.919892	78361.653201	36.866445
1611.507377	78442.001784	36.871463
1613.458666	78530.540880	36.876480
1615.006613	78620.068194	36.881498
1616.472433	78696.407954	36.886516
1618.065371	78785.384013	36.891533
1620.070053	78857.079167	36.896551
1621.848997	78939.844295	36.901568
1623.340536	79027.025376	36.906586
1625.268811	79107.411246	36.911604
1626.546809	79198.110208	36.916621
1628.117999	79266.833751	36.921639
1629.934932	79353.217471	36.926656
1631.319579	79428.457095	36.931674
1632.913587	79508.186984	36.936692
1634.670267	79599.863872	36.941709
1636.179321	79681.140507	36.946727
1637.668828	79765.689068	36.951744
1639.378378	79841.588433	36.956762
1641.322768	79928.486103	36.961780
1642.452104	80015.714314	36.966797
1644.256941	80093.297130	36.971815
1645.860576	80176.004705	36.976832
1647.764462	80268.889683	36.981850
1649.559259	80335.984545	36.986868
1650.919880	80412.472192	36.991885
1652.629288	80478.516532	36.996903
1653.921877	80549.884087	37.001920
1655.537622	80620.187690	37.006938
1657.226519	80685.868316	37.011956
1658.548333	80758.878869	37.016973
1660.212823	80826.780819	37.021991
1661.582469	80916.026707	37.027008
1663.152396	80992.141105	37.032026
1664.863465	81080.117795	37.037044
1666.118644	81161.679205	37.042061
1668.037258	81247.951535	37.047079
1669.492360	81331.382616	37.052096
1671.209002	81438.123552	37.057114
1673.149826	81528.447625	37.062132
1674.758890	81614.579480	37.067149
1676.238229	81717.012825	37.072167
1677.974695	81803.226678	37.077184
1679.459904	81902.175522	37.082202
1681.532670	81990.960022	37.087220
1683.055422	82098.671394	37.092237
1684.869549	82189.068096	37.097255
1686.904543	82285.689617	37.102272
1688.296282	82380.790344	37.107290
1690.432388	82476.547786	37.112308
1692.209830	82562.263403	37.117325
1693.637106	82662.389648	37.122343
1695.682121	82747.354408	37.127360
1697.744732	82844.252266	37.132378
1699.375746	82931.803798	37.137396
1701.220624	83028.812384	37.142413
1702.972605	83117.688638	37.147431
1704.850326	83197.891441	37.152448
1706.760876	83294.979354	37.157466
1708.067491	83380.897836	37.162484
1709.882518	83469.942715	37.167501
1711.580774	83563.605649	37.172519
1713.556009	83656.300571	37.177536
1714.918674	83742.958953	37.182554
1716.935627	83830.909003	37.187572
1718.311653	83927.613899	37.192589
1720.436617	84018.208526	37.197607
1722.597147	84104.248970	37.202624
1723.508760	84194.958018	37.207642
1726.002450	84282.657456	37.212660
1727.895011	84381.994670	37.217677
1729.541833	84455.698823	37.222695
1731.232458	84546.375766	37.227712
1732.832194	84634.811733	37.232730
1734.576326	84709.692410	37.237748
1736.251199	84806.036716	37.242765
1737.852243	84893.662307	37.247783
1739.887537	84980.383892	37.252800
1741.226210	85073.043634	37.257818
1743.039755	85158.305225	37.262836
1745.144873	85245.903688	37.267853
1746.715333	85328.732873	37.272871
1748.847866	85421.636974	37.277888
1750.090443	85521.244571	37.282906
1752.270817	85600.633768	37.287924
1753.576515	85680.768308	37.292941
1755.344079	85766.178279	37.297959
1757.220601	85853.206114	37.302976
1758.760612	85940.084123	37.307994
1760.535797	86030.651125	37.313012
1762.609652	86118.916065	37.318029
1763.859628	86218.157412	37.323047
1765.785982	86292.101295	37.328064
1767.090675	86373.124944	37.333082
1769.352452	86441.745150	37.338100
1770.679563	86517.734884	37.343117
1772.127374	86593.034304	37.348135
1774.130573	86677.218900	37.353152
1775.367526	86765.920907	37.358170
1777.414005	86845.283776	37.363188
1778.804004	86941.667091	37.368205
1780.403126	87012.204480	37.373223
1782.332669	87108.605289	37.378240
1783.680519	87209.406061	37.383258
1785.624004	87300.888431	37.388276
1787.133468	87408.672457	37.393293
1788.924388	87507.161887	37.398311
1791.253025	87616.706690	37.403328
1792.540801	87721.954025	37.408346
1794.329499	87815.477169	37.413364
1796.082955	87925.493314	37.418381
1797.802618	88035.705249	37.423399
1800.095299	88145.194284	37.428416
1801.653067	88260.311423	37.433434
1803.607467	88365.317332	37.438452
1805.971972	88468.295133	37.443469
1807.950064	88580.458312	37.448487
1810.026916	88680.985290	37.453504
1811.923045	88790.754217	37.458522
1813.719924	88882.087019	37.463540
1815.461405	88978.789517	37.468557
1817.198434	89089.180084	37.473575
1819.260477	89195.743572	37.478592
1820.643709	89310.562599	37.483610
1822.620133	89407.331112	37.488628
1824.349004	89514.277386	37.493645
1826.028044	89624.096036	37.498663
1828.144230	89718.511778	37.503680
1830.273896	89833.558195	37.508698
1832.051389	89941.081372	37.513716
1833.848512	90050.439537	37.518733
1835.773329	90163.364765	37.523751
1838.004848	90254.253550	37.528768
1839.595069	90364.709832	37.533786
1841.624197	90467.100676	37.538804
1843.676658	90577.333320	37.543821
1845.187240	90676.840348	37.548839
1847.375820	90782.920764	37.553856
1849.390161	90889.535778	37.558874
1851.099557	90987.910089	37.563892
1852.988144	91084.571031	37.568909
1854.468166	91193.894264	37.573927
1856.769455	91287.449494	37.578944
1858.549941	91401.124383	37.583962
1860.525331	91508.913708	37.588980
1862.120199	91603.949279	37.593997
1863.705932	91704.740712	37.599015
1865.894458	91800.520507	37.604032
1867.747501	91913.640970	37.609050
1869.607010	92020.347576	37.614068
1871.809094	92117.672533	37.619085
1873.697523	92234.489602	37.624103
1875.602559	92319.858916	37.629120
1877.750091	92419.195957	37.634138
1879.272804	92523.054548	37.639156
1881.141581	92617.923684	37.644173
1882.809361	92722.241890	37.649191
1884.963684	92810.742255	37.654208
1886.985186	92924.537226	37.659226
1888.734390	93014.838026	37.664244
1890.463796	93113.634366	37.669261
1892.193130	93194.876261	37.674279
1893.887901	93280.851541	37.679296
1895.391572	93364.233241	37.684314
1897.054634	93452.279987	37.689332
1899.012979	93541.294785	37.694349
1900.703923	93651.899368	37.699367
1902.416805	93742.005192	37.704384
1904.558297	93849.662726	37.709402
1906.266939	93951.773239	37.714420
1907.925707	94050.748426	37.719437
1909.612486	94155.562868	37.724455
1911.579555	94255.910106	37.729472
1913.215302	94386.312204	37.734490
1914.812911	94494.855647	37.739508
1917.162868	94608.326594	37.744525
1919.159975	94730.041577	37.749543
1921.101927	94842.322345	37.754560
1923.303503	94970.749697	37.759578
1924.823624	95081.779071	37.764596
1927.007074	95198.104911	37.769613
1928.995644	95321.953074	37.774631
1931.075059	95444.050923	37.779648
1933.312852	95559.076672	37.784666
1934.887725	95680.113565	37.789684
1937.120530	95800.008544	37.794701
1938.894497	95938.089841	37.799719
1940.924887	96061.566787	37.804736
1942.779280	96179.418201	37.809754
1944.680417	96309.343152	37.814772
1946.991102	96433.715743	37.819789
1948.673038	96556.222385	37.824807
1950.551273	96674.971943	37.829824
1952.772271	96808.879984	37.834842
1954.581078	96942.434769	37.839860
1956.802028	97071.336735	37.844877
1958.687008	97203.131346	37.849895
1960.932624	97326.478164	37.854912
1962.781492	97454.451139	37.859930
1964.605346	97579.284723	37.864948
1967.167655	97716.439143	37.869965
1968.929678	97837.417007	37.874983
1970.590184	97962.493162	37.880000
1973.001874	98093.068137	37.885018
1975.120283	98234.109999	37.890036
1976.990227	98347.441384	37.895053
1979.488910	98470.283996	37.900071
1981.384473	98589.988793	37.905088
1983.319735	98707.760900	37.910106
1984.949817	98834.227041	37.915124
1987.197202	98956.781238	37.920141
1989.260320	99087.148597	37.925159
1991.397712	99197.487334	37.930176
1993.679080	99322.294177	37.935194
1995.353035	99448.134679	37.940212
1997.618608	99560.495674	37.945229
1999.236238	99685.712043	37.950247
2001.335145	99806.175563	37.955264
2003.143812	99937.422900	37.960282
2004.845779	100058.012858	37.965300
2007.169622	100183.830604	37.970317
2008.559368	100324.564613	37.975335
2010.600907	100443.150492	37.980352
2012.690701	100575.155127	37.985370
2014.434609	100710.662816	37.990388
2016.390589	100852.527593	37.995405
2018.476574	100988.375931	38.000423
2020.633791	101122.844456	38.005440
2022.429884	101236.755381	38.010458
2024.641110	101355.013756	38.015476
2026.237714	101463.010617	38.020493
2027.607383	101593.978335	38.025511
2029.905313	101709.840911	38.030528
2031.676886	101826.661061	38.035546
2033.660192	101956.608691	38.040564
2035.788559	102094.584963	38.045581
2037.915251	102222.977115	38.050599
2039.618226	102367.233564	38.055616
2041.682629	102490.045253	38.060634
2043.436305	102632.481885	38.065652
2045.583202	102773.412228	38.070669
2047.096560	102928.376285	38.075687
2049.147724	103077.386610	38.080704
2051.517546	103224.331801	38.085722
2053.158858	103383.538071	38.090740
2055.358220	103528.355853	38.095757
2057.576961	103690.719071	38.100775
2059.678224	103848.790553	38.105792
2061.742155	103995.457350	38.110810
2063.870579	104159.878330	38.115828
2066.265177	104317.335564	38.120845
2068.135417	104472.441142	38.125863
2070.634648	104628.450696	38.130880
2072.819887	104787.185476	38.135898
2074.839078	104949.167590	38.140916
2076.970991	105086.115980	38.145933
2079.091219	105248.641627	38.150951
2081.123280	105414.440539	38.155968
2083.414410	105568.483607	38.160986
2085.880236	105725.036009	38.166004
2087.958997	105872.875207	38.171021
2090.420868	106032.688382	38.176039
2092.443230	106186.953828	38.181056
2094.655169	106326.950594	38.186074
2096.670897	106488.509482	38.191092
2098.795350	106643.001940	38.196109
2101.011837	106788.325564	38.201127
2102.961286	106952.293576	38.206144
2105.146363	107108.591932	38.211162
2107.186397	107270.657920	38.216180
2109.382102	107418.777158	38.221197
2111.235820	107572.238319	38.226215
2113.595303	107728.334676	38.231232
2116.039264	107885.204721	38.236250
2117.998350	108050.102140	38.241268
2120.420178	108203.730834	38.246285
2122.224432	108354.603653	38.251303
2124.380980	108498.688468	38.256320
2126.609086	108658.994262	38.261338
2128.291873	108823.494751	38.266356
2130.731199	108978.734620	38.271373
2132.750462	109150.830675	38.276391
2134.584514	109305.532642	38.281408
2136.780380	109463.881598	38.286426
2139.032986	109636.932668	38.291444
2140.832276	109792.009978	38.296461
2143.228636	109956.429508	38.301479
2145.376818	110123.754644	38.306496
2147.498075	110280.039193	38.311514
2149.744323	110452.194880	38.316532
2151.718242	110613.196135	38.321549
2153.738578	110784.437662	38.326567
2155.543599	110954.293348	38.331584
2158.052471	111121.756997	38.336602
2159.938105	111284.588609	38.341620
2162.122684	111457.405596	38.346637
2164.329225	111615.787886	38.351655
2166.277396	111774.021070	38.356672
2168.163891	111928.358520	38.361690
2170.338044	112081.510235	38.366708
2172.428079	112234.092384	38.371725
2174.469179	112395.395548	38.376743
2176.456544	112553.372393	38.381760
2178.650412	112707.107077	38.386778
2180.469731	112873.063460	38.391796
2182.320552	113040.131735	38.396813
2184.424419	113220.718830	38.401831
2186.579997	113392.319449	38.406848
2189.203173	113568.362750	38.411866
2191.090954	113758.663206	38.416884
2193.234982	113937.053466	38.421901
2195.423839	114118.494153	38.426919
2197.350074	114312.545607	38.431936
2199.552380	114496.624114	38.436954
2201.752163	114693.589924	38.441972
2204.068808	114888.116030	38.446989
2206.448362	115082.455757	38.452007
2208.519358	115276.464285	38.457024
2210.679351	115470.066725	38.462042
2212.931769	115678.064052	38.467060
2215.093199	115872.353273	38.472077
2217.952986	116074.791229	38.477095
2219.863316	116272.508329	38.482112
2222.575828	116459.560852	38.487130
2225.108476	116659.960365	38.492148
2227.426825	116842.091765	38.497165
2229.609923	117033.200011	38.502183
2232.166321	117233.915975	38.507200
2234.616935	117431.453196	38.512218
2236.736148	117613.632175	38.517236
2239.291626	117810.305143	38.522253
2241.652315	118004.231774	38.527271
2243.792517	118200.020423	38.532288
2246.484009	118367.387093	38.537306
2248.502913	118567.661489	38.542324
2250.491309	118760.559370	38.547341
2252.865098	118958.002405	38.552359
2255.058667	119137.386471	38.557376
2257.409826	119329.088858	38.562394
2259.472221	119527.496838	38.567412
2261.645099	119720.687810	38.572429
2263.835351	119919.027067	38.577447
2265.901383	120131.086450	38.582464
2268.211199	120330.360480	38.587482
2270.147820	120536.239389	38.592500
2271.998228	120742.183616	38.597517
2274.453233	120960.503852	38.602535
2276.331000	121173.321433	38.607552
2278.685677	121381.879416	38.612570
2280.785938	121611.561384	38.617588
2283.431976	121823.171363	38.622605
2285.839286	122041.860284	38.627623
2288.079636	122267.896116	38.632640
2290.300376	122476.886802	38.637658
2292.856649	122692.397297	38.642676
2295.030218	122922.189600	38.647693
2297.388361	123136.388810	38.652711
2299.448769	123347.400841	38.657728
2301.880659	123566.703253	38.662746
2303.845707	123792.638595	38.667764
2306.223661	124010.746701	38.672781
2308.514691	124232.929174	38.677799
2310.475854	124462.433713	38.682816
2313.150882	124688.770468	38.687834
2315.062604	124906.334728	38.692852
2316.998682	125122.018746	38.697869
2319.658608	125324.142933	38.702887
2321.605693	125527.432630	38.707904
2324.017062	125743.261258	38.712922
2326.097588	125953.585991	38.717940
2328.410692	126175.407724	38.722957
2330.451721	126387.694631	38.727975
2332.211679	126609.288068	38.732992
2334.534396	126835.425415	38.738010
2336.671926	127072.351612	38.743028
2339.014343	127305.123787	38.748045
2341.403556	127551.820518	38.753063
2343.879503	127792.364488	38.758080
2345.954686	128032.858353	38.763098
2348.130922	128287.953731	38.768116
2350.414140	128535.396032	38.773133
2352.662247	128795.913510	38.778151
2354.879896	129053.265441	38.783168
2357.358084	129315.665969	38.788186
2359.584177	129589.171353	38.793204
2361.657222	129855.076996	38.798221
2364.394868	130124.826295	38.803239
2366.844012	130400.484320	38.808256
2369.296065	130669.520441	38.813274
2371.505815	130946.513610	38.818292
2373.900161	131221.868262	38.823309
2376.486437	131486.130355	38.828327
2379.020573	131771.528530	38.833344
2381.680877	132055.157817	38.838362
2384.094528	132326.824073	38.843380
2386.280635	132602.029697	38.848397
2389.065922	132882.066566	38.853415
2391.486239	133159.649911	38.858432
2394.079338	133429.797615	38.863450
2397.045979	133701.017856	38.868468
2399.060001	133978.276523	38.873485
2401.898569	134250.065775	38.878503
2404.426813	134534.899038	38.883520
2407.105952	134791.946206	38.888538
2409.817684	135068.835998	38.893556
2412.028351	135337.976451	38.898573
2414.450908	135596.908318	38.903591
2416.609707	135871.059738	38.908608
2418.723874	136146.095381	38.913626
2421.596572	136422.143411	38.918644
2423.692394	136694.964505	38.923661
2426.032628	136965.375963	38.928679
2428.903637	137235.477555	38.933696
2431.553493	137506.668598	38.938714
2434.156443	137776.371123	38.943732
2436.389922	138048.988313	38.948749
2439.632391	138310.840151	38.953767
2442.327982	138577.550589	38.958784
2444.900250	138849.941778	38.963802
2447.412131	139106.176249	38.968820
2449.594592	139366.676919	38.973837
2451.495489	139623.288957	38.978855
2453.761530	139890.137448	38.983872
2456.365631	140158.990460	38.988890
2458.396964	140425.396404	38.993908
2460.337251	140710.054969	38.998925
2463.016422	140997.163220	39.003943
2465.122036	141265.161256	39.008960
2467.401188	141545.126784	39.013978
2470.087301	141835.018276	39.018996
2472.199638	142126.143462	39.024013
2474.676480	142403.722401	39.029031
2476.905594	142686.862447	39.034048
2478.937914	142948.256218	39.039066
2481.245188	143232.135961	39.044084
2483.403707	143495.315082	39.049101
2485.876096	143773.410063	39.054119
2487.689389	144059.377084	39.059136
2490.239990	144342.463567	39.064154
2492.517584	144640.875471	39.069172
2494.728019	144934.895503	39.074189
2497.328120	145235.380032	39.079207
2499.490134	145543.093256	39.084224
2501.858686	145848.872184	39.089242
2504.371785	146162.233035	39.094260
2506.743777	146495.075349	39.099277
2509.570594	146806.461787	39.104295
2512.097270	147105.877171	39.109312
2515.246275	147434.821574	39.114330
2517.850973	147749.205773	39.119348
2520.297817	148067.982869	39.124365
2522.806788	148393.542863	39.129383
2525.470321	148717.963698	39.134400
2527.420071	149045.760271	39.139418
2530.103723	149371.705095	39.144436
2532.940001	149701.270969	39.149453
2535.520664	150031.234251	39.154471
2538.028969	150374.132691	39.159488
2540.413689	150704.029162	39.164506
2542.982515	151039.648981	39.169524
2545.595906	151388.566756	39.174541
2548.349235	151718.792467	39.179559
2550.780839	152067.082885	39.184576
2552.842194	152415.953841	39.189594
2555.432489	152773.160287	39.194612
2558.059971	153130.667838	39.199629
2560.547781	153486.511187	39.204647
2562.695069	153851.118209	39.209664
2565.423712	154203.437474	39.214682
2568.323721	154574.875100	39.219700
2570.623668	154951.004344	39.224717
2573.229054	155314.076423	39.229735
2575.744611	155688.564511	39.234752
2578.019743	156059.842773	39.239770
2580.343442	156439.024577	39.244788
2582.796176	156829.156917	39.249805
2585.482929	157199.882833	39.254823
2587.855457	157592.647840	39.259840
2590.531621	157987.297556	39.264858
2593.253653	158372.713316	39.269876
2596.077801	158776.967902	39.274893
2598.428315	159169.771921	39.279911
2601.123528	159564.796990	39.284928
2603.599877	159966.371564	39.289946
2606.700568	160354.101812	39.294964
2609.429793	160758.561874	39.299981
2611.836127	161153.731006	39.304999
2614.154996	161557.282774	39.310016
2617.184506	161948.868016	39.315034
2620.067867	162337.799658	39.320052
2622.576490	162730.854963	39.325069
2625.415667	163134.551018	39.330087
2628.262458	163520.499153	39.335104
2631.035291	163899.973344	39.340122
2633.890027	164277.138860	39.345140
2636.780250	164662.388531	39.350157
2640.117415	165026.913408	39.355175
2642.421872	165410.506858	39.360192
2645.067416	165793.274622	39.365210
2647.689554	166166.513006	39.370228
2650.449000	166534.259649	39.375245
2652.825409	166880.953420	39.380263
2655.429372	167230.863705	39.385280
2657.674653	167581.288921	39.390298
2660.757305	167919.154577	39.395316
2663.154409	168278.523537	39.400333
2665.613501	168624.209847	39.405351
2667.910309	168986.391388	39.410368
2670.086120	169360.605220	39.415386
2672.356124	169716.611045	39.420404
2674.732241	170100.015538	39.425421
2677.419911	170490.560014	39.430439
2679.408794	170878.612851	39.435456
2682.039937	171277.309349	39.440474
2684.184467	171675.347598	39.445492
2687.025306	172085.341799	39.450509
2689.885983	172488.732262	39.455527
2692.390214	172896.739089	39.460544
2695.088864	173323.980308	39.465562
2698.233089	173740.411699	39.470580
2700.990000	174160.677163	39.475597
2703.473371	174590.727041	39.480615
2706.255489	175015.424662	39.485632
2708.850410	175443.023574	39.490650
2711.378192	175877.352601	39.495668
2713.984821	176324.217533	39.500685
2716.542249	176759.295730	39.505703
2719.357557	177211.758144	39.510720
2722.128719	177657.093289	39.515738
2725.015294	178100.025353	39.520756
2727.671320	178559.605602	39.525773
2730.324098	179013.601325	39.530791
2733.435799	179458.892417	39.535808
2736.474458	179905.365450	39.540826
2739.854397	180350.111059	39.545844
2742.894055	180799.128126	39.550861
2745.489769	181250.451853	39.555879
2748.665472	181695.870867	39.560896
2751.407279	182146.058550	39.565914
2753.772257	182596.256510	39.570932
2756.091358	183126.113742	39.575949
2758.709668	183575.159108	39.580967
2761.134336	184046.841780	39.585984
2763.977199	184514.981628	39.591002
2766.851036	184964.679086	39.596020
2769.629039	185437.659180	39.601037
2772.529391	185912.654260	39.606055
2774.988129	186384.291657	39.611072
2777.888755	186873.667129	39.616090
2780.619830	187344.428022	39.621108
2783.221475	187836.166014	39.626125
2785.490731	188314.470867	39.631143
2788.346004	188794.997531	39.636160
2790.487034	189306.676874	39.641178
2793.130368	189790.873131	39.646196
2796.021023	190307.697542	39.651213
2798.104548	190812.102657	39.656231
2801.062197	191327.981243	39.661248
2803.183368	191853.619702	39.666266
2806.343940	192366.829291	39.671284
2809.151331	192898.588055	39.676301
2811.219302	193430.058281	39.681319
2814.411657	193972.912337	39.686336
2817.717159	194493.702731	39.691354
2821.440136	194999.646333	39.696372
2824.895456	195506.827553	39.701389
2828.213762	196020.611046	39.706407
2831.456778	196522.647283	39.711424
2834.054594	197007.817905	39.716442
2836.724032	197485.333033	39.721460
2839.486259	197957.170594	39.726477
2841.931114	198430.532583	39.731495
2844.705911	198893.886872	39.736512
2846.952681	199380.440966	39.741530
2849.656411	199857.500908	39.746548
2852.239539	200347.358416	39.751565
2854.793776	200850.761302	39.756583
2857.268199	201348.792885	39.761600
2860.034272	201855.239301	39.766618
2862.857922	202356.953316	39.771636
2865.240636	202878.754902	39.776653
2868.171440	203401.767790	39.781671
2870.721514	203920.015167	39.786688
2873.225098	204460.066777	39.791706
2876.046928	205010.129615	39.796724
2879.147499	205551.056114	39.801741
2882.732575	206086.675236	39.806759
2886.206315	206628.740076	39.811776
2889.149625	207170.838396	39.816794
2891.560089	207716.018914	39.821812
2894.522618	208264.162747	39.826829
2897.396727	208814.582541	39.831847
2899.815173	209369.215547	39.836864
2902.739811	209955.169146	39.841882
2905.074553	210513.983802	39.846900
2907.968080	211092.806339	39.851917
2910.370874	211679.022988	39.856935
2912.794701	212282.334087	39.861952
2915.716018	212885.771759	39.866970
2918.601401	213489.038318	39.871988
2921.274977	214116.243931	39.877005
2924.016890	214725.047602	39.882023
2927.215966	215338.226388	39.887040
2930.293731	215967.302441	39.892058
2933.325666	216598.622089	39.897076
2936.168544	217215.314091	39.902093
2939.454642	217852.159041	39.907111
2942.305917	218471.366161	39.912128
2945.140795	219113.897322	39.917146
2948.035377	219753.574507	39.922164
2951.167588	220391.792446	39.927181
2954.045144	221030.076087	39.932199
2957.319805	221669.568239	39.937216
2960.552983	222311.302785	39.942234
2963.362812	222944.517245	39.947252
2966.781167	223589.017785	39.952269
2969.471511	224235.385214	39.957287
2973.102877	224867.861965	39.962304
2975.759500	225522.745157	39.967322
2978.588583	226163.121010	39.972340
2981.578373	226809.035123	39.977357
2984.270724	227466.605241	39.982375
2987.130559	228122.243617	39.987392
2990.079692	228768.900086	39.992410
2993.426758	229416.992792	39.997428
2996.519315	230076.937726	40.002445
2999.300778	230738.429618	40.007463
3002.203057	231386.158471	40.012480
3005.340181	232049.422573	40.017498
3008.483544	232703.793587	40.022516
3011.815611	233363.418306	40.027533
3014.545528	234015.438948	40.032551
3017.501904	234672.834264	40.037568
3020.257405	235332.114459	40.042586
3023.308062	235991.550643	40.047604
3026.565397	236647.269819	40.052621
3029.645772	237301.389625	40.057639
3032.224579	237928.353954	40.062656
3035.105699	238562.052520	40.067674
3038.430364	239193.089252	40.072692
3042.314257	239802.317239	40.077709
3045.489708	240409.419183	40.082727
3048.504738	241010.498848	40.087744
3051.414277	241644.389192	40.092762
3054.289525	242264.336932	40.097780
3056.982831	242890.840111	40.102797
3059.495103	243529.893591	40.107815
3062.542001	244165.965692	40.112832
3065.420617	244816.922912	40.117850
3068.007414	245471.530922	40.122868
3071.085080	246127.228565	40.127885
3073.618846	246805.439574	40.132903
3076.739742	247465.317309	40.137920
3079.748426	248147.945399	40.142938
3082.629848	248833.842264	40.147956
3085.421512	249517.565843	40.152973
3088.402648	250228.615102	40.157991
3091.389149	250937.729863	40.163008
3094.433516	251645.155874	40.168026
3097.780796	252367.899350	40.173044
3101.510368	253073.357237	40.178061
3104.662829	253781.518321	40.183079
3108.010436	254496.148135	40.188096
3111.463114	255200.825947	40.193114
3114.654644	255919.917987	40.198132
3117.741344	256623.477107	40.203149
3120.649936	257349.311420	40.208167
3124.163982	258056.123368	40.213184
3127.187903	258774.209581	40.218202
3130.472639	259503.172945	40.223220
3133.784969	260221.434011	40.228237
3136.856149	260948.846991	40.233255
3139.902580	261681.491588	40.238272
3143.358144	262401.596119	40.243290
3146.123445	263133.817864	40.248308
3149.464424	263869.297328	40.253325
3151.960031	264609.501113	40.258343
3155.232107	265356.842320	40.263360
3158.421294	266092.583701	40.268378
3161.437046	266848.157746	40.273396
3165.333496	267593.936824	40.278413
3168.235231	268348.932845	40.283431
3171.162457	269086.978327	40.288448
3174.187793	269850.781451	40.293466
3177.166795	270618.598261	40.298484
3180.733388	271377.351330	40.303501
3183.439668	272147.838929	40.308519
3186.569461	272914.596306	40.313536
3189.465591	273684.100792	40.318554
3192.732996	274459.533764	40.323572
3196.193477	275228.351643	40.328589
3199.682772	276000.586230	40.333607
3203.246483	276759.011828	40.338624
3206.749418	277539.914723	40.343642
3209.762298	278308.061789	40.348660
3213.528748	279071.309071	40.353677
3216.510959	279854.022106	40.358695
3219.480242	280610.471018	40.363712
3222.579421	281385.734382	40.368730
3225.823239	282158.173510	40.373748
3228.991201	282934.476006	40.378765
3231.671167	283716.407431	40.383783
3234.735516	284492.988207	40.388800
3238.273791	285284.493281	40.393818
3241.321577	286056.996011	40.398836
3244.185111	286815.984567	40.403853
3247.415525	287574.221470	40.408871
3250.294416	288327.934038	40.413888
3253.487649	289081.537876	40.418906
3256.600108	289850.557826	40.423924
3259.441996	290614.151690	40.428941
3262.539064	291386.303659	40.433959
3265.479963	292166.214354	40.438976
3268.784165	292952.608819	40.443994
3271.967988	293743.962771	40.449012
3275.729994	294516.021614	40.454029
3278.685094	295319.323130	40.459047
3281.882344	296116.380910	40.464064
3285.687548	296914.754311	40.469082
3288.901972	297720.368201	40.474100
3292.588288	298527.826198	40.479117
3295.963358	299334.534132	40.484135
3299.355829	300134.423898	40.489152
3302.465255	300945.033755	40.494170
3306.455209	301769.176689	40.499188
3309.675053	302565.554053	40.504205
3313.227753	303384.206185	40.509223
3317.016915	304191.563082	40.514240
3320.848812	304985.878535	40.519258
3324.198227	305790.943674	40.524276
3327.151702	306599.078532	40.529293
3330.541540	307410.609595	40.534311
3333.641193	308226.157811	40.539328
3336.966577	309043.180113	40.544346
3340.295204	309873.868942	40.549364
3343.490067	310706.594849	40.554381
3346.848689	311535.879561	40.559399
3350.500852	312373.022496	40.564416
3353.812092	313209.366197	40.569434
3356.667212	314054.065199	40.574452
3360.090466	314893.051044	40.579469
3363.769981	315742.208884	40.584487
3366.846002	316595.708566	40.589504
3370.450074	317443.602406	40.594522
3373.320184	318297.177678	40.599540
3376.451904	319162.419384	40.604557
3379.521480	320037.956225	40.609575
3382.709291	320915.791282	40.614592
3385.764184	321801.749019	40.619610
3389.571313	322690.260224	40.624628
3392.782280	323574.405292	40.629645
3396.447318	324467.772522	40.634663
3399.516402	325359.792588	40.639680
3403.039893	326256.897984	40.644698
3406.273948	327162.426692	40.649716
3409.734750	328051.890224	40.654733
3412.914854	328954.925536	40.659751
3416.034265	329869.695854	40.664768
3419.827504	330775.054114	40.669786
3423.239888	331699.147443	40.674804
3426.936875	332618.709137	40.679821
3430.375485	333531.566509	40.684839
3433.677185	334439.578021	40.689856
3437.257572	335359.268429	40.694874
3441.141626	336273.815329	40.699892
3444.746938	337185.770375	40.704909
3448.313557	338100.321113	40.709927
3451.773764	339006.520602	40.714944
3455.769751	339913.906874	40.719962
3458.813554	340828.900714	40.724980
3462.826954	341719.194314	40.729997
3466.636460	342622.710241	40.735015
3469.956647	343498.414790	40.740020
3474.614280	344321.280788	40.745024
3478.255845	345114.666657	40.750029
3481.611676	345829.646840	40.755034
3485.254975	346496.644363	40.760039
3487.939369	347107.899572	40.765044
3491.390816	347661.696570	40.770048
3494.405731	348157.285734	40.775053
3496.935891	348580.110655	40.780058
3499.693720	348952.204639	40.785063
3501.798599	349268.089029	40.790068
3504.245385	349543.294534	40.795072
3505.840302	349779.991612	40.800077
3507.790958	349961.443594	40.805082
3509.689194	350101.848924	40.810087
3511.167270	350201.824872	40.815092
3512.840428	350258.555662	40.820096
3513.961794	350279.453884	40.825101
3515.081259	350262.222081	40.830106
3516.665196	350228.318238	40.835111
3517.243643	350163.304605	40.840116
3518.718498	350059.232124	40.845120
3519.547091	349938.711624	40.850125
3520.305518	349792.501446	40.855130
3521.269161	349625.591497	40.860135
3521.191529	349446.666900	40.865140
3522.239043	349235.229904	40.870144
3522.924193	349031.982976	40.875149
3523.171202	348791.866073	40.880154
3523.444086	348541.066322	40.885159
3523.988094	348295.916751	40.890164
3524.091919	348017.099260	40.895168
3524.270040	347752.224577	40.900173
3524.722934	347460.357110	40.905178
3525.177354	347169.808822	40.910183
3524.919047	346868.996917	40.915188
3525.361010	346556.174833	40.920192
3525.492275	346243.449253	40.925197
3525.452836	345919.103468	40.930202
3525.288140	345600.596194	40.935207
3525.609736	345275.094557	40.940212
3525.443737	344950.454177	40.945216
3525.415942	344613.305647	40.950221
3525.529591	344278.140228	40.955226
3525.398873	343938.865448	40.960231
3524.946959	343604.086948	40.965236
3525.384560	343264.157295	40.970240
3525.184567	342929.739663	40.975245
3525.188487	342587.709962	40.980250
3524.714488	342252.540420	40.985255
3524.967743	341917.787908	40.990260
3524.711008	341562.287389	40.995264
3524.499763	341229.406201	41.000269
3524.385042	340895.718520	41.005274
3524.651858	340553.068400	41.010279
3524.355554	340219.911258	41.015284
3524.188254	339879.534692	41.020288
3523.897676	339544.539493	41.025293
3523.885880	339201.614731	41.030298
3523.593548	338869.258024	41.035303
3523.160509	338543.938620	41.040308
3522.962991	338215.070222	41.045312
3522.720511	337891.368021	41.050317
3522.796846	337567.918233	41.055322
3522.679280	337248.666369	41.060327
3522.081799	336923.688671	41.065332
3522.404019	336595.182060	41.070336
3521.786389	336293.902945	41.075341
3521.204875	335968.456506	41.080346
3521.652419	335666.293652	41.085351
3521.558989	335366.934032	41.090356
3521.502397	335054.189328	41.095360
3520.869306	334745.397716	41.100365
3520.458139	334441.019407	41.105370
3520.791523	334144.355267	41.110375
3520.238053	333845.843710	41.115380
3519.942219	333546.729985	41.120384
3520.075070	333257.923361	41.125389
3519.687259	332972.375023	41.130394
3519.787314	332687.994471	41.135399
3519.473432	332401.387513	41.140404
3519.384736	332114.412555	41.145408
3519.454433	331838.321666	41.150413
3519.012395	331561.622074	41.155418
3519.043717	331274.901817	41.160423
3518.586809	331006.975249	41.165428
3518.503293	330726.245867	41.170432
3518.403427	330469.476262	41.175437
3518.113302	330199.152607	41.180442
3518.218407	329927.391800	41.185447
3517.885744	329666.125877	41.190452
3517.865902	329403.969937	41.195456
3517.833205	329145.680418	41.200461
3517.212339	328883.258860	41.205466
3517.108970	328630.878034	41.210471
3517.068098	328386.320050	41.215476
3516.857473	328130.010236	41.220480
3516.410116	327876.203077	41.225485
3516.494193	327631.646333	41.230490
3516.319336	327392.928076	41.235495
3516.027080	327152.217252	41.240500
3516.112124	326915.337815	41.245504
3515.927677	326670.461048	41.250509
3515.798070	326436.486711	41.255514
3515.646125	326201.751390	41.260519
3515.396171	325979.545199	41.265524
3515.593855	325750.679496	41.270528
3515.124861	325529.675204	41.275533
3515.170684	325306.579640	41.280538
3514.918087	325087.039938	41.285543
3514.771857	324865.345631	41.290548
3514.489210	324649.115217	41.295552
3514.368633	324435.529347	41.300557
3514.067385	324227.668821	41.305562
3514.088186	324005.689368	41.310567
3514.034351	323803.664332	41.315572
3513.773837	323599.966219	41.320576
3513.458789	323389.127285	41.325581
3513.295203	323184.674248	41.330586
3513.462870	322980.015782	41.335591
3512.847379	322797.763593	41.340596
3513.027196	322596.764609	41.345600
3512.937202	322404.151016	41.350605
3512.761187	322223.684705	41.355610
3512.827037	322027.814182	41.360615
3512.270923	321843.894976	41.365620
3512.464972	321656.372407	41.370624
3512.210600	321470.979760	41.375629
3511.744394	321285.492219	41.380634
3511.708200	321104.108853	41.385639
3511.449385	320941.585441	41.390644
3511.919302	320769.381840	41.395648
3511.480269	320597.701257	41.400653
3511.377822	320418.640429	41.405658
3511.414430	320250.674762	41.410663
3511.447886	320079.401607	41.415668
3511.152050	319906.169408	41.420672
3511.369713	319755.295320	41.425677
3511.100123	319588.112728	41.430682
3511.117559	319414.804136	41.435687
3510.894224	319259.087082	41.440692
3510.360664	319092.986943	41.445696
3510.604930	318935.211181	41.450701
3510.325178	318783.113948	41.455706
3510.107645	318633.270776	41.460711
3509.966318	318482.168523	41.465716
3510.316413	318328.546490	41.470720
3510.015391	318183.167172	41.475725
3510.392595	318026.003394	41.480730
3510.205430	317881.826500	41.485735
3509.829356	317731.903261	41.490740
3509.747229	317572.494423	41.495744
3509.705053	317441.523471	41.500749
3509.599132	317295.627311	41.505754
3509.501291	317151.917475	41.510759
3509.315484	317019.008644	41.515764
3509.246216	316874.072189	41.520768
3508.939500	316737.466768	41.525773
3509.030129	316601.256780	41.530778
3509.186712	316466.817078	41.535783
3508.871154	316340.032834	41.540788
3508.802449	316207.077830	41.545792
3508.908731	316076.257751	41.550797
3508.696594	315947.955076	41.555802
3508.464789	315810.062942	41.560807
3508.264174	315688.423899	41.565812
3508.071852	315559.811697	41.570816
3507.776133	315447.524657	41.575821
3507.827360	315333.325707	41.580826
3508.113470	315224.661929	41.585831
3507.829458	315109.929620	41.590836
3507.605314	314989.920779	41.595840
3507.570572	314879.906923	41.600845
3507.612188	314763.087314	41.605850
3507.764279	314647.242453	41.610855
3507.499005	314545.711260	41.615860
3507.496882	314423.757906	41.620864
3507.515472	314322.410835	41.625869
3507.345407	314219.184712	41.630874
3507.307566	314111.001476	41.635879
3507.322529	314003.802063	41.640884
3507.242892	313893.589295	41.645888
3507.185150	313796.375002	41.650893
3506.843898	313689.535880	41.655898
3506.971215	313581.300133	41.660903
3506.591030	313487.672407	41.665908
3506.715285	313381.192354	41.670912
3506.877837	313286.359799	41.675917
3506.877795	313189.949443	41.680922
3506.915932	313080.963120	41.685927
3506.598826	312981.752067	41.690932
3506.570904	312883.437058	41.695936
3506.130237	312794.575609	41.700941
3505.741433	312705.960334	41.705946
3505.873366	312613.828378	41.710951
3506.162586	312536.506224	41.715956
3505.851946	312447.954573	41.720960
3505.963006	312354.756668	41.725965
3505.951374	312273.664313	41.730970
3506.169234	312184.418850	41.735975
3505.896031	312102.247494	41.740980
3505.887984	312020.976024	41.745984
3505.666783	311930.908128	41.750989
3505.586528	311850.767257	41.755994
3505.639758	311764.014956	41.760999
3505.724946	311690.234806	41.766004
3505.638815	311599.127330	41.771008
3505.557927	311515.881608	41.776013
3505.275303	311450.810153	41.781018
3505.328097	311361.436261	41.786023
3505.162103	311303.369429	41.791028
3505.425801	311215.056461	41.796032
3505.321543	311145.350984	41.801037
3505.413683	311066.403237	41.806042
3505.125328	310990.950065	41.811047
3505.162107	310923.995834	41.816052
3505.414845	310841.002121	41.821056
3505.125757	310767.889755	41.826061
3504.753175	310697.513077	41.831066
3505.168598	310619.404665	41.836071
3505.111376	310550.861491	41.841076
3505.150517	310478.308078	41.846080
3504.949532	310403.730939	41.851085
3505.029740	310339.033825	41.856090
3504.643327	310264.867155	41.861095
3504.588468	310201.208830	41.866100
3504.741245	310125.049161	41.871104
3504.723016	310068.509961	41.876109
3504.706365	310003.573072	41.881114
3504.744608	309936.311870	41.886119
3504.447952	309883.582083	41.891124
3504.485189	309818.331160	41.896128
3504.420053	309749.889865	41.901133
3504.501272	309689.288642	41.906138
3504.317000	309626.718553	41.911143
3504.403164	309565.836488	41.916148
3504.502282	309500.015629	41.921152
3504.221587	309442.447961	41.926157
3504.170639	309392.809191	41.931162
3504.306888	309328.738132	41.936167
3504.264542	309275.000937	41.941172
3503.935999	309207.414359	41.946176
3504.223454	309158.078701	41.951181
3504.053366	309092.477506	41.956186
3504.154639	309038.946620	41.961191
3504.180790	308984.511323	41.966196
3503.954138	308926.323862	41.971200
3503.944448	308876.296406	41.976205
3503.918403	308818.789975	41.981210
3504.053548	308755.176383	41.986215
3503.943941	308707.530969	41.991220
3503.907992	308650.611175	41.996224
3503.958210	308606.579641	42.001229
3503.600398	308554.723178	42.006234
3503.691945	308498.801169	42.011239
3503.719542	308453.704243	42.016244
3503.747055	308401.787377	42.021248
3503.767264	308356.615175	42.026253
3503.748621	308309.642234	42.031258
3503.889692	308249.029860	42.036263
3503.482552	308194.483291	42.041268
3503.788329	308142.573543	42.046272
3503.536437	308096.425738	42.051277
3503.263036	308047.863730	42.056282
3503.553408	307998.806371	42.061287
3503.450134	307969.074387	42.066292
3503.012796	307919.011021	42.071296
3503.393414	307881.670818	42.076301
3503.409182	307832.274509	42.081306
3503.463599	307787.707182	42.086311
3503.420381	307744.452915	42.091316
3503.623535	307698.589865	42.096320
3503.531599	307646.181921	42.101325
3502.968169	307601.049376	42.106330
3503.127165	307553.513537	42.111335
3503.097821	307512.216384	42.116340
3503.127221	307470.502846	42.121344
3502.840563	307435.353357	42.126349
3502.931664	307398.668803	42.131354
3502.797186	307362.324864	42.136359
3502.783133	307331.509733	42.141364
3502.980726	307283.662226	42.146368
3503.152102	307253.301569	42.151373
3502.834370	307222.635639	42.156378
3502.714492	307176.313648	42.161383
3502.564927	307142.185889	42.166388
3502.468835	307117.312855	42.171392
3502.763545	307085.787649	42.176397
3502.515132	307049.283157	42.181402
3503.095668	307008.755474	42.186407
3502.788663	306974.983040	42.191412
3502.625776	306941.289844	42.196416
3502.880582	306903.077889	42.201421
3502.542081	306873.763746	42.206426
3502.868411	306839.281448	42.211431
3502.610973	306806.849907	42.216436
3502.612685	306773.334451	42.221440
3502.758803	306733.205289	42.226445
3502.505424	306700.518562	42.231450
3502.737296	306667.984984	42.236455
3502.818286	306644.534584	42.241460
3502.556751	306604.570844	42.246464
3502.690136	306569.813144	42.251469
3502.407949	306542.322286	42.256474
3502.790042	306509.892363	42.261479
3502.469075	306482.203947	42.266484
3502.357315	306451.098167	42.271488
3502.700098	306412.541253	42.276493
3502.733290	306394.696868	42.281498
3502.763471	306360.158746	42.286503
3502.395976	306326.802507	42.291508
3502.524666	306290.951063	42.296512
3502.550516	306256.337201	42.301517
3502.720200	306226.739642	42.306522
3502.576387	306191.592393	42.311527
3502.696988	306162.307852	42.316532
3502.394311	306132.987675	42.321536
3502.235590	306097.079232	42.326541
3502.066414	306067.229173	42.331546
3502.308202	306039.325289	42.336551
3502.273077	306016.579862	42.341556
3502.244951	305987.700202	42.346560
3502.088139	305966.322556	42.351565
3501.925422	305946.269157	42.356570
3502.331494	305920.044585	42.361575
3501.983579	305891.214865	42.366580
3501.827539	305862.176990	42.371584
3502.105429	305841.571139	42.376589
3501.975096	305827.518532	42.381594
3502.239228	305796.862556	42.386599
3502.296639	305781.253659	42.391604
3501.950878	305751.609162	42.396608
3502.264898	305730.386846	42.401613
3501.923311	305700.258139	42.406618
3502.095386	305684.224104	42.411623
3502.270688	305666.102756	42.416628
3502.104261	305635.997524	42.421632
3502.182973	305611.859880	42.426637
3502.193741	305582.948459	42.431642
3502.091796	305554.054643	42.436647
3502.123979	305534.734076	42.441652
3502.171249	305505.333375	42.446656
3502.063884	305479.417887	42.451661
3502.069948	305466.030977	42.456666
3502.212974	305426.842869	42.461671
3501.961454	305408.788158	42.466676
3501.628838	305389.550018	42.471680
3502.172630	305353.480319	42.476685
3502.017319	305336.962930	42.481690
3502.170833	305319.608334	42.486695
3502.251628	305290.431309	42.491700
3502.408387	305266.586687	42.496704
3501.973806	305240.722234	42.501709
3501.939106	305220.623084	42.506714
3502.169662	305197.708508	42.511719
3502.284608	305178.858399	42.516724
3502.332315	305157.321193	42.521728
3502.114554	305129.412308	42.526733
3501.976018	305116.913182	42.531738
3502.334382	305080.388747	42.536743
3501.642876	305055.531434	42.541748
3502.292135	305030.439044	42.546752
3502.094728	305008.125723	42.551757
3501.995638	304992.744645	42.556762
3502.155032	304950.525161	42.561767
3501.558924	304940.184362	42.566772
3501.669845	304923.268927	42.571776
3501.782637	304905.233429	42.576781
3501.834127	304887.487449	42.581786
3502.266364	304864.846584	42.586791
3502.012580	304843.458177	42.591796
3502.054463	304823.957680	42.596800
3502.118118	304794.986645	42.601805
3501.792496	304784.476281	42.606810
3501.570629	304760.410676	42.611815
3502.064897	304742.137335	42.616820
3501.750270	304714.879600	42.621824
3502.117336	304692.401543	42.626829
3501.818856	304677.407833	42.631834
3502.042231	304649.633313	42.636839
3502.091986	304634.483350	42.641844
3501.742346	304604.736994	42.646848
3501.896942	304577.354928	42.651853
3501.669612	304565.963873	42.656858
3501.976381	304547.007194	42.661863
3502.165417	304536.365418	42.666868
3502.010209	304501.295130	42.671872
3502.103325	304490.286600	42.676877
3502.090268	304468.834951	42.681882
3502.277985	304448.598928	42.686887
3502.326252	304431.184138	42.691892
3502.299462	304404.873766	42.696896
3502.231459	304364.012722	42.701901
3501.949902	304351.866613	42.706906
3501.933160	304328.175928	42.711911
3501.763943	304302.778503	42.716916
3502.261383	304281.654158	42.721920
3502.068638	304258.754443	42.726925
3501.820754	304243.040109	42.731930
3502.230261	304217.806660	42.736935
3501.965051	304195.681732	42.741940
3501.921206	304179.019295	42.746944
3502.210595	304142.403178	42.751949
3501.829275	304137.576647	42.756954
3501.892638	304106.569303	42.761959
3501.927921	304085.415333	42.766964
3501.954307	304057.594943	42.771968
3502.442394	304036.828256	42.776973
3501.976984	304014.963597	42.781978
3501.907792	303996.574487	42.786983
3502.336665	303971.923232	42.791988
3501.574278	303953.413434	42.796993
3502.037035	303926.517289	42.801997
3501.786950	303909.963357	42.807002
3502.016051	303886.463082	42.812007
3501.697908	303875.849563	42.817012
3501.798802	303852.776511	42.822017
3501.702025	303824.033611	42.827021
3501.760636	303817.382238	42.832026
3501.577792	303782.544830	42.837031
3501.950142	303773.961119	42.842036
3501.401053	303766.564905	42.847041
3501.918893	303736.962373	42.852045
3501.517406	303733.156948	42.857050
3501.720688	303716.735674	42.862055
3501.847459	303706.561559	42.867060
3502.001194	303676.532371	42.872065
3501.954279	303649.410366	42.877069
3501.607888	303642.873189	42.882074
3501.899002	303612.415289	42.887079
3501.630345	303594.566218	42.892084
3501.434682	303584.493387	42.897089
3501.781970	303558.760348	42.902093
3501.740445	303551.437450	42.907098
3501.310906	303523.357204	42.912103
3501.782395	303506.079535	42.917108
3501.766857	303497.454621	42.922113
3501.640768	303470.548501	42.927117
3501.531180	303465.679424	42.932122
3501.594720	303450.043410	42.937127
3501.601607	303436.757644	42.942132
3501.535266	303415.288440	42.947137
3501.912387	303402.402881	42.952141
3501.794237	303383.206809	42.957146
3501.704181	303373.346477	42.962151
3501.727717	303340.741554	42.967156
3501.490836	303333.601867	42.972161
3501.721903	303323.640421	42.977165
3501.400042	303301.244019	42.982170
3501.503994	303288.655639	42.987175
3501.427498	303282.254371	42.992180
3501.336116	303258.447616	42.997185
3501.853090	303241.060948	43.002189
3501.567781	303231.180215	43.007194
3501.563856	303214.180376	43.012199
3501.291018	303192.463414	43.017204
3501.396720	303193.846816	43.022209
3502.027420	303173.541040	43.027213
3501.639989	303164.337962	43.032218
3501.916593	303151.544406	43.037223
3501.784204	303129.372809	43.042228
3501.442934	303116.090491	43.047233
3501.770881	303087.102631	43.052237
3501.415393	303077.792743	43.057242
3501.596183	303054.808648	43.062247
3501.717406	303045.246074	43.067252
3501.624788	303034.393524	43.072257
3501.905957	303008.975953	43.077261
3501.414293	302999.432839	43.082266
3501.845998	302978.725446	43.087271
3501.498547	302968.192674	43.092276
3501.336855	302957.452707	43.097281
3501.560381	302937.235947	43.102285
3501.533395	302931.412250	43.107290
3501.535444	302900.719176	43.112295
3501.572605	302898.524824	43.117300
3501.337545	302887.745413	43.122305
3501.361491	302868.297885	43.127309
3501.204960	302862.087229	43.132314
3501.334809	302853.617631	43.137319
3501.082283	302841.950183	43.142324
3501.228386	302822.814394	43.147329
3501.423732	302812.654834	43.152333
3501.414725	302812.809118	43.157338
3502.077820	302787.993436	43.162343
3501.665379	302774.645808	43.167348
3501.435398	302778.168623	43.172353
3501.401874	302748.728084	43.177357
3501.613405	302740.271148	43.182362
3501.655419	302724.002026	43.187367
3501.485202	302701.479857	43.192372
3501.516223	302686.230454	43.197377
3501.642764	302679.135662	43.202381
3501.391497	302664.948397	43.207386
3501.567308	302640.565133	43.212391
3501.667361	302640.142460	43.217396
3501.092682	302620.152171	43.222401
3501.721557	302589.513620	43.227405
3501.624194	302588.154697	43.232410
3501.579297	302579.712375	43.237415
3501.630634	302559.649642	43.242420
3501.847789	302550.428286	43.247425
3501.528949	302528.107431	43.252429
3501.279734	302518.551775	43.257434
3501.624226	302496.661660	43.262439
3501.670116	302492.735300	43.267444
3501.303946	302474.213930	43.272449
3501.385664	302458.040321	43.277453
3501.582587	302452.588771	43.282458
3501.484801	302427.611921	43.287463
3501.299166	302413.210725	43.292468
3501.195852	302411.521873	43.297473
3501.627406	302405.091970	43.302477
3501.142166	302384.451348	43.307482
3501.382810	302375.429892	43.312487
3501.406077	302366.951428	43.317492
3501.052362	302365.454425	43.322497
3501.289016	302336.454975	43.327501
3501.262909	302334.117788	43.332506
3501.338099	302328.379851	43.337511
3501.223965	302321.246286	43.342516
3501.169068	302303.974167	43.347521
3501.618776	302278.708048	43.352525
3501.541821	302288.951353	43.357530
3501.745396	302269.322818	43.362535
3501.667867	302243.146541	43.367540
3501.318092	302251.243761	43.372545
3501.126940	302222.540186	43.377549
3501.568589	302207.277349	43.382554
3501.587559	302197.781508	43.387559
3501.717133	302195.979888	43.392564
3501.588575	302174.010893	43.397569
3501.592481	302155.329752	43.402573
3501.490859	302152.877110	43.407578
3501.423862	302120.489189	43.412583
3501.751938	302110.461447	43.417588
3501.499547	302100.269947	43.422593
3501.758002	302080.963620	43.427597
3501.664965	302063.086571	43.432602
3501.536395	302046.385799	43.437607
3501.413252	302038.922746	43.442612
3501.235087	302022.687832	43.447617
3501.362599	302017.145286	43.452621
3501.529006	302001.085550	43.457626
3501.419258	301986.926880	43.462631
3501.423083	301978.018733	43.467636
3501.353776	301975.586481	43.472641
3501.632577	301944.416923	43.477645
3501.588647	301936.661514	43.482650
3501.609493	301919.046569	43.487655
3501.459139	301898.735161	43.492660
3501.561135	301890.931482	43.497665
3501.743617	301875.047349	43.502669
3501.551862	301859.781635	43.507674
3501.599806	301844.758400	43.512679
3501.367587	301834.410991	43.517684
3501.558123	301818.143822	43.522689
3501.817590	301811.664400	43.527693
3501.393109	301797.936645	43.532698
3501.465848	301782.247797	43.537703
3501.637717	301777.105504	43.542708
3501.478417	301764.201607	43.547713
3501.556497	301742.200128	43.552717
3501.241809	301728.175232	43.557722
3501.241278	301719.242271	43.562727
3501.569571	301698.296038	43.567732
3501.336296	301690.061181	43.572737
3501.489766	301677.159266	43.577741
3501.787342	301667.848831	43.582746
3501.609804	301653.853375	43.587751
3501.452680	301641.839886	43.592756
3501.545439	301631.543434	43.597761
3501.869266	301609.045365	43.602765
3501.546853	301610.470290	43.607770
3501.519208	301579.755641	43.612775
3501.207196	301566.493809	43.617780
3501.331760	301565.100164	43.622785
3501.721358	301549.972530	43.627789
3501.793093	301525.808632	43.632794
3501.651827	301519.646333	43.637799
3501.444965	301494.406138	43.642804
3501.622344	301483.485607	43.647809
3501.539546	301470.467875	43.652813
3501.430796	301460.431952	43.657818
3501.436186	301443.150128	43.662823
3501.385005	301421.066921	43.667828
3501.604097	301419.327632	43.672833
3501.518093	301399.616795	43.677837
3501.473095	301386.135017	43.682842
3501.389737	301382.101526	43.687847
3501.673012	301356.835540	43.692852
3501.264730	301339.542003	43.697857
3501.560766	301330.689868	43.702861
3501.375708	301318.629771	43.707866
3501.109942	301297.623551	43.712871
3501.599275	301293.576873	43.717876
3501.053748	301291.295395	43.722881
3501.487923	301274.379147	43.727885
3501.598851	301264.436097	43.732890
3501.558337	301250.724525	43.737895
3501.774584	301237.201866	43.742900
3501.412672	301222.395239	43.747905
3501.486239	301210.294685	43.752909
3501.650970	301195.838382	43.757914
3501.427388	301177.828739	43.762919
3501.589265	301160.344202	43.767924
3501.532543	301151.089068	43.772929
3501.639282	301127.683048	43.777933
3501.295493	301127.304303	43.782938
3501.481605	301112.895538	43.787943
3501.719162	301095.195539	43.792948
3501.526415	301079.293480	43.797953
3501.506394	301068.276471	43.802957
3501.348745	301051.198167	43.807962
3501.058691	301045.568097	43.812967
3501.185168	301035.978889	43.817972
3501.445533	301037.312717	43.822977
3501.315742	301007.326341	43.827981
3501.287366	301003.411482	43.832986
3501.239675	300988.326605	43.837991
3501.115840	300997.101322	43.842996
3501.527831	300989.605362	43.848001
3501.435462	300963.405325	43.853005
3501.325693	300963.269955	43.858010
3501.272678	300955.337666	43.863015
3501.591475	300928.920625	43.868020
3501.379611	300918.926172	43.873025
3501.218769	300902.993622	43.878029
3501.096363	300915.025877	43.883034
3501.260145	300884.993535	43.888039
3501.576841	300868.019172	43.893044
3501.173919	300874.954155	43.898049
3501.343124	300858.537322	43.903053
3501.339498	300839.195168	43.908058
3501.139747	300836.426942	43.913063
3501.523805	300823.641479	43.918068
3501.364594	300821.045072	43.923073
3501.463410	300796.011271	43.928077
3501.357747	300784.167703	43.933082
3501.322156	300784.198893	43.938087
3501.655579	300772.210322	43.943092
3501.314964	300761.116115	43.948097
3501.221268	300734.076284	43.953101
3500.708452	300738.890562	43.958106
3501.179750	300730.723562	43.963111
3501.302163	300723.145582	43.968116
3500.969795	300708.665060	43.973121
3501.247041	300691.085979	43.978125
3501.095413	300696.912745	43.983130
3501.078896	300690.247274	43.988135
3501.165367	300689.903064	43.993140
3501.197664	300678.216062	43.998145
3501.531279	300657.981227	44.003149
3501.122365	300655.932877	44.008154
3501.487772	300652.490905	44.013159
3501.608511	300636.030679	44.018164
3501.550177	300630.873364	44.023169
3501.758672	300608.392908	44.028173
3501.522290	300595.017206	44.033178
3501.139435	300580.162773	44.038183
3501.641039	300568.173315	44.043188
3501.037512	300563.075778	44.048193
3501.528815	300528.003575	44.053197
3501.115872	300519.160343	44.058202
3501.260127	300524.686355	44.063207
3501.539906	300512.527954	44.068212
3501.187132	300497.796053	44.073217
3501.569344	300486.079756	44.078221
3501.411613	300478.774601	44.083226
3501.597287	300472.230201	44.088231
3501.389514	300449.687501	44.093236
3501.303145	300449.930241	44.098241
3501.194645	300435.898223	44.103245
3501.461869	300426.134194	44.108250
3501.468036	300404.677889	44.113255
3501.335856	300396.070708	44.118260
3501.295416	300392.692170	44.123265
3501.645178	300374.236302	44.128269
3501.611208	300364.035775	44.133274
3501.451700	300361.159426	44.138279
3501.619766	300334.791112	44.143284
3501.301890	300317.534015	44.148289
3501.566360	300315.024053	44.153293
3501.761030	300308.834547	44.158298
3501.707309	300284.842414	44.163303
3501.749425	300276.233416	44.168308
3501.387010	300258.067011	44.173313
3501.628350	300236.293906	44.178317
3501.580594	300231.822089	44.183322
3501.635262	300204.224318	44.188327
3501.625740	300190.558534	44.193332
3501.280036	300176.538081	44.198337
3501.601982	300161.293378	44.203341
3501.490831	300149.068756	44.208346
3501.381224	300145.115632	44.213351
3501.718639	300121.647662	44.218356
3501.472595	300110.996663	44.223361
3501.666744	300103.229221	44.228365
3501.311353	300084.119952	44.233370
3501.139525	300076.180659	44.238375
3501.298487	300059.281607	44.243380
3501.146071	300061.443540	44.248385
3501.282201	300050.020137	44.253389
3501.204003	300033.921702	44.258394
3501.303064	300017.133808	44.263399
3501.064429	300016.127776	44.268404
3501.003249	300017.537352	44.273409
3501.434580	300008.053011	44.278413
3501.056121	299993.146827	44.283418
3501.131264	299983.132782	44.288423
3501.576460	299976.496846	44.293428
3501.343367	299981.878295	44.298433
3501.209883	299961.029035	44.303437
3501.652946	299949.048593	44.308442
3501.454400	299942.996875	44.313447
3501.628696	299924.262869	44.318452
3501.284307	299908.485980	44.323457
3501.325571	299898.960797	44.328461
3501.334146	299886.666495	44.333466
3501.481067	299874.630530	44.338471
3501.426573	299858.299271	44.343476
3500.895880	299864.796228	44.348481
3501.424004	299845.192425	44.353485
3501.420750	299836.463192	44.358490
3501.417408	299812.183006	44.363495
3501.348349	299802.267827	44.368500
3501.177483	299796.771703	44.373505
3501.316032	299783.133571	44.378509
3501.261940	299770.365458	44.383514
3501.082295	299771.946271	44.388519
3501.450450	299757.763202	44.393524
3501.201653	299756.987820	44.398529
3501.079892	299734.533184	44.403533
3500.934704	299724.858958	44.408538
3501.032814	299721.331459	44.413543
3501.246080	299726.872215	44.418548
3501.171664	299717.186924	44.423553
3501.306887	299704.083778	44.428557
3501.305495	299692.503639	44.433562
3501.024303	299683.130638	44.438567
3501.065477	299676.405119	44.443572
3500.655818	299671.480801	44.448577
3501.271219	299669.526788	44.453581
3501.063360	299663.756464	44.458586
3500.978792	299642.924887	44.463591
3501.073975	299634.765622	44.468596
3500.387609	299636.349304	44.473601
3500.736028	299627.565058	44.478605
3500.992417	299625.489008	44.483610
3501.035913	299634.212333	44.488615
3501.436338	299615.773741	44.493620
3501.194156	299627.977716	44.498625
3501.402110	299610.943607	44.503629
3501.274898	299595.896227	44.508634
3501.071917	299591.728595	44.513639
3501.233452	299586.282288	44.518644
3501.024647	299586.773239	44.523649
3501.046347	299562.209059	44.528653
3501.032719	299547.143908	44.533658
3501.359914	299544.115069	44.538663
3501.368209	299537.623741	44.543668
3500.979852	299543.385832	44.548673
3501.105625	299531.709423	44.553677
3501.049007	299511.764238	44.558682
3501.046609	299510.059517	44.563687
3501.490748	299500.293116	44.568692
3501.193409	299497.005590	44.573697
3501.079094	299489.362641	44.578701
3501.378492	299479.898835	44.583706
3501.303381	299459.371131	44.588711
3501.063624	299451.875048	44.593716
3500.958549	299458.076445	44.598721
3501.333650	299456.210896	44.603725
3501.413308	299436.295282	44.608730
3501.009431	299418.058724	44.613735
3501.190112	299418.005199	44.618740
3500.757807	299422.552485	44.623745
3501.147232	299409.511335	44.628749
3500.959218	299418.219984	44.633754
3500.652299	299400.019165	44.638759
3500.965978	299383.833820	44.643764
3500.890977	299375.319345	44.648769
3501.201837	299377.001647	44.653773
3501.061158	299367.046683	44.658778
3501.126695	299360.520932	44.663783
3501.357508	299362.419364	44.668788
3501.075591	299357.118720	44.673793
3501.125644	299334.382539	44.678797
3501.286963	299331.990468	44.683802
3500.891766	299331.339775	44.688807
3501.256969	299323.061893	44.693812
3501.209993	299328.388857	44.698817
3501.082654	299305.731302	44.703821
3501.079214	299295.627610	44.708826
3501.299950	299288.848519	44.713831
3501.065964	299289.903352	44.718836
3500.810696	299287.220081	44.723841
3501.266288	299292.112150	44.728845
3501.397942	299263.432889	44.733850
3501.543560	299253.127721	44.738855
3501.588522	299245.816164	44.743860
3501.689055	299230.453107	44.748865
3501.669134	299202.637425	44.753869
3501.329898	299205.388542	44.758874
3501.171495	299186.324519	44.763879
3501.135902	299161.896376	44.768884
3501.047795	299156.005469	44.773889
3501.235091	299158.445202	44.778893
3501.552556	299157.403118	44.783898
3501.155529	299142.066921	44.788903
3501.668563	299115.949511	44.793908
3500.963728	299124.764459	44.798913
3501.103290	299108.224475	44.803917
3501.213182	299107.342101	44.808922
3501.251939	299092.344992	44.813927
3501.444722	299078.570946	44.818932
3501.061707	299078.020153	44.823937
3501.077955	299068.727805	44.828941
3501.140648	299069.634451	44.833946
3501.172556	299054.358429	44.838951
3501.489900	299030.842227	44.843956
3501.305009	299023.693836	44.848961
3501.290910	299009.570336	44.853965
3501.089804	299002.526285	44.858970
3501.316233	298990.477696	44.863975
3501.244918	298984.202365	44.868980
3500.716509	298981.765398	44.873985
3501.238726	298973.971958	44.878989
3501.110885	298972.414092	44.883994
3501.105422	298958.492846	44.888999
3501.154066	298944.690397	44.894004
3500.993155	298941.126987	44.899009
3501.557596	298931.010802	44.904013
3501.061250	298945.698063	44.909018
3500.933127	298920.240745	44.914023
3500.996608	298900.352919	44.919028
3501.360298	298906.455639	44.924033
3501.085813	298891.532899	44.929037
3501.040759	298898.259469	44.934042
3501.449939	298892.010815	44.939047
3501.292716	298877.578781	44.944052
3500.826266	298867.420136	44.949057
3501.166517	298851.383194	44.954061
3501.218484	298852.775110	44.959066
3501.055447	298856.084096	44.964071
3501.255995	298845.999333	44.969076
3501.091731	298831.670196	44.974081
3501.475888	298823.923772	44.979085
3501.347547	298812.006965	44.984090
3501.149718	298818.502908	44.989095
3501.215680	298798.894631	44.994100
3501.017969	298781.567358	44.999105
3500.982396	298771.952184	45.004109
3501.201422	298772.961655	45.009114
3501.081282	298780.463542	45.014119
3501.091902	298771.070216	45.019124
3501.168252	298774.367233	45.024129
3501.195882	298745.805774	45.029133
3501.659888	298728.629553	45.034138
3501.370233	298738.804974	45.039143
3501.485590	298712.138695	45.044148
3501.221521	298704.340884	45.049153
3501.424661	298696.062794	45.054157
3501.474640	298690.073892	45.059162
3501.369862	298666.852600	45.064167
3501.380282	298650.867165	45.069172
3501.290050	298649.227054	45.074177
3501.498291	298641.228132	45.079181
3501.523167	298619.920918	45.084186
3501.152030	298609.594611	45.089191
3501.484449	298608.346561	45.094196
3501.173343	298601.141491	45.099201
3501.686130	298582.506822	45.104205
3501.472940	298571.672223	45.109210
3501.175580	298571.922505	45.114215
3501.423541	298540.399486	45.119220
3501.482954	298524.279095	45.124225
3501.427739	298512.885289	45.129229
3501.335958	298509.972802	45.134234
3501.361449	298488.309109	45.139239
3501.632242	298483.634633	45.144244
3501.270252	298478.600946	45.149249
3501.610971	298450.270362	45.154253
3501.969875	298444.105875	45.159258
3501.282547	298438.003146	45.164263
3501.617333	298404.939339	45.169268
3501.465375	298406.184982	45.174273
3501.467227	298398.600078	45.179277
3501.736410	298379.672546	45.184282
3501.311424	298364.340504	45.189287
3501.547108	298350.381405	45.194292
3501.347026	298334.301527	45.199297
3501.425787	298323.166712	45.204301
3501.882488	298325.844340	45.209306
3501.562433	298309.452332	45.214311
3501.775278	298291.373506	45.219316
3501.449901	298276.891248	45.224321
3501.516007	298263.111352	45.229325
3501.398907	298242.691571	45.234330
3501.247522	298245.413366	45.239335
3501.467342	298235.223671	45.244340
3501.397208	298212.607630	45.249345
3501.285608	298200.408098	45.254349
3501.354572	298190.521956	45.259354
3501.445068	298190.864317	45.264359
3501.543614	298160.255278	45.269364
3501.203132	298157.636179	45.274369
3500.910437	298160.787309	45.279373
3501.634807	298142.704821	45.284378
3500.986519	298126.669504	45.289383
3501.542790	298117.165308	45.294388
3501.055036	298112.049439	45.299393
3501.233812	298108.814655	45.304397
3500.974352	298083.937441	45.309402
3500.966533	298085.211461	45.314407
3501.392187	298068.728250	45.319412
3501.333912	298073.064455	45.324417
3501.333085	298058.607757	45.329421
3501.400272	298042.664178	45.334426
3500.955913	298032.883714	45.339431
3501.582730	298022.070395	45.344436
3501.458456	298019.493845	45.349441
3501.434852	298011.276556	45.354445
3501.418811	297991.426290	45.359450
3501.047326	297986.164970	45.364455
3501.208080	297984.027454	45.369460
3500.938326	297964.013224	45.374465
3501.040996	297949.616675	45.379469
3501.266712	297941.614921	45.384474
3501.128068	297940.695028	45.389479
3501.121806	297939.728986	45.394484
3501.223630	297941.876706	45.399489
3501.164408	297922.771290	45.404493
3501.364299	297907.010546	45.409498
3501.368324	297896.829075	45.414503
3501.473092	297896.583797	45.419508
3501.262466	297881.498087	45.424513
3501.320169	297867.923029	45.429517
3501.238780	297861.700051	45.434522
3501.245335	297864.804413	45.439527
3501.276077	297839.627194	45.444532
3500.914764	297828.001126	45.449537
3500.780753	297820.437383	45.454541
3501.033190	297803.548482	45.459546
3500.708457	297802.632227	45.464551
3500.706343	297801.232840	45.469556
3500.999571	297804.979607	45.474561
3500.833236	297798.286303	45.479565
3501.060652	297796.494695	45.484570
3500.780584	297801.476458	45.489575
3500.733405	297799.345991	45.494580
3500.897450	297800.236812	45.499585
3500.962287	297792.489263	45.504589
3501.184284	297770.081897	45.509594
3501.210313	297761.322307	45.514599
3501.554599	297756.432660	45.519604
3501.055057	297763.535853	45.524609
3501.220411	297747.831369	45.529613
3501.535354	297722.126066	45.534618
3501.037692	297727.218212	45.539623
3501.040656	297710.419190	45.544628
3500.958362	297719.111577	45.549633
3501.125626	297721.427243	45.554637
3501.359863	297708.613578	45.559642
3500.825996	297687.393362	45.564647
3501.008514	297676.674892	45.569652
3500.696852	297681.941584	45.574657
3500.876599	297677.637613	45.579661
3501.023364	297679.014738	45.584666
3500.982197	297670.978313	45.589671
3501.134837	297667.594874	45.594676
3500.962808	297652.197637	45.599681
3501.053691	297642.155255	45.604685
3501.178696	297631.140336	45.609690
3501.158399	297629.412903	45.614695
3501.229923	297625.762164	45.619700
3501.137557	297624.020545	45.624705
3501.000166	297616.228230	45.629709
3501.471933	297594.010819	45.634714
3501.038719	297590.769874	45.639719
3501.011790	297580.465921	45.644724
3501.318560	297586.832212	45.649729
3501.331406	297583.470624	45.654733
3501.175999	297561.911213	45.659738
3501.288987	297560.951973	45.664743
3501.190149	297557.302412	45.669748
3500.941239	297548.891204	45.674753
3501.256091	297544.337027	45.679757
3501.728753	297523.824780	45.684762
3500.914750	297517.716301	45.689767
3501.024719	297506.194654	45.694772
3500.983978	297509.535504	45.699777
3500.700812	297505.863852	45.704781
3500.958892	297500.402248	45.709786
3501.030885	297484.457760	45.714791
3501.277202	297466.704321	45.719796
3501.252079	297460.650671	45.724801
3501.162304	297460.715787	45.729805
3501.287513	297449.293557	45.734810
3500.960621	297445.705095	45.739815
3501.230313	297423.137418	45.744820
3501.493714	297409.657355	45.749825
3501.356575	297352.435671	45.754829
3501.180888	297246.503244	45.759834
3500.847934	297100.405084	45.764839
3500.731845	296892.752780	45.769844
3500.562124	296660.444054	45.774849
3500.321972	296372.428301	45.779853
3500.443316	296032.378804	45.784858
3500.079885	295652.822837	45.789863
3499.630685	295207.174457	45.794868
3499.127683	294721.492022	45.799873
3498.850257	294187.407366	45.804877
3498.286576	293614.290099	45.809882
3497.612427	292991.293409	45.814887
3497.187245	292321.159651	45.819892
3496.212807	291603.350292	45.824897
3495.873730	290838.773125	45.829901
3495.610507	290028.201313	45.834906
3494.584629	289170.440564	45.839911
3493.703703	288254.299040	45.844916
3493.067308	287306.005038	45.849921
3492.020866	286310.334359	45.854925
3491.344964	285259.372988	45.859930
3490.573316	284168.415520	45.864935
3489.830729	283026.340902	45.869940
3488.608783	281839.260269	45.874945
3487.649331	280605.935581	45.879949
3486.758447	279317.611604	45.884954
3485.006250	277996.963794	45.889959
3484.115579	276623.531278	45.894964
3482.541176	275215.554601	45.899969
3481.391965	273764.380518	45.904973
3480.093138	272270.046451	45.909978
3478.537871	270739.187919	45.914983
3477.045031	269152.529469	45.919988
3475.961993	267539.450606	45.924993
3474.348472	265882.400622	45.929997
3473.209701	264170.347987	45.935002
3471.133561	262423.654542	45.940007
3469.837540	260648.850559	45.945012
3468.315214	258813.981414	45.950017
3466.491617	256970.294923	45.955021
3464.412525	255052.464125	45.960026
3462.520334	253131.241011	45.965031
3461.003080	251153.702949	45.970036
3459.044104	249157.439640	45.975041
3456.709139	247115.828478	45.980045
3454.882043	245030.641876	45.985050
3452.777593	242940.409269	45.990055
3450.619187	240800.095351	45.995060
3448.412654	238626.000121	46.000065
3446.317885	236440.691007	46.005069
3444.461220	234205.438006	46.010074
3442.029038	231944.081778	46.015079
3439.707229	229646.355438	46.020084
3437.152562	227330.652975	46.025089
3434.490204	224987.687013	46.030093
3432.220615	222604.189437	46.035098
3429.632778	220204.113784	46.040103
3427.100351	217785.902456	46.045108
3424.547839	215332.888867	46.050113
3421.791685	212847.194282	46.055117
3419.143846	210358.062982	46.060122
3416.247796	207853.813750	46.065127
3413.083298	205304.223701	46.070132
3410.448789	202749.565092	46.075137
3407.317062	200157.455802	46.080141
3404.501723	197548.275268	46.085146
3400.985905	194937.161821	46.090151
3398.042957	192306.756944	46.095156
3394.800234	189666.675734	46.100161
3391.102681	187003.171257	46.105165
3388.553555	184332.932642	46.110170
3385.100894	181654.070589	46.115175
3381.229544	178957.271856	46.120180
3377.908565	176260.761905	46.125185
3373.972168	173553.092192	46.130189
3370.374124	170832.375576	46.135194
3366.232277	168121.452963	46.140199
3362.371954	165397.656080	46.145204
3358.492911	162694.081438	46.150209
3354.744692	159969.125883	46.155213
3350.844530	157251.528809	46.160218
3346.895660	154532.089292	46.165223
3342.445935	151814.408378	46.170228
3338.051932	149108.635076	46.175233
3333.684668	146399.418073	46.180237
3329.146803	143697.443821	46.185242
3324.070559	141027.927956	46.190247
3318.732436	138389.478062	46.195252
3313.775723	135677.977038	46.200257
3307.788738	133077.092148	46.205261
3301.866235	130529.203819	46.210266
3295.722986	128015.780474	46.215271
3288.815322	125543.150032	46.220276
3282.250923	123111.351976	46.225281
3275.214497	120747.318626	46.230285
3267.962209	118427.373211	46.235290
3260.388028	116197.864791	46.240295
3252.726599	114032.727889	46.245300
3244.952057	111938.340516	46.250305
3236.942194	109934.087789	46.255309
3228.541583	107997.669211	46.260314
3219.698769	106167.538713	46.265319
3211.057005	104418.461728	46.270324
3202.229258	102770.037452	46.275329
3193.345362	101224.265560	46.280333
3184.195542	99777.746383	46.285338
3175.361913	98430.465444	46.290343
3166.553640	97166.684499	46.295348
3158.333490	96007.478617	46.300353
3150.554335	94931.319412	46.305357
3142.932062	93930.872594	46.310362
3135.284670	93029.197997	46.315367
3128.537824	92189.253951	46.320372
3122.268699	91421.317819	46.325377
3115.995562	90708.001022	46.330381
3110.378752	90064.164339	46.335386
3105.026688	89470.856638	46.340391
3099.847359	88891.509865	46.345396
3095.023288	88356.803626	46.350401
3090.356184	87871.886751	46.355405
3085.808917	87414.236681	46.360410
3081.507857	86991.722095	46.365415
3076.817041	86575.766599	46.370420
3072.630836	86185.401092	46.375425
3068.874942	85817.510922	46.380429
3065.414679	85465.116331	46.385434
3061.463914	85121.174648	46.390439
3057.930444	84785.581736	46.395444
3054.615638	84453.782340	46.400449
3051.092385	84132.855490	46.405453
3047.892891	83814.676343	46.410458
3044.694257	83510.563118	46.415463
3041.146624	83196.904123	46.420468
3038.323780	82889.143749	46.425473
3035.141932	82571.801361	46.430477
3031.890217	82258.347771	46.435482
3028.498280	81948.323863	46.440487
3025.097567	81632.436193	46.445492
3021.841717	81304.043038	46.450497
3018.635199	81001.698114	46.455501
3015.356503	80676.504093	46.460506
3011.759438	80368.612767	46.465511
3008.327677	80044.796409	46.470516
3004.973540	79727.043020	46.475521
3001.350931	79413.094865	46.480525
2998.131956	79099.709494	46.485530
2994.530889	78796.065697	46.490535
2991.264598	78480.814950	46.495540
2987.776317	78154.844879	46.500545
2984.063657	77844.738847	46.505549
2980.678265	77520.589095	46.510554
2977.001366	77218.498601	46.515559
2973.308808	76910.393950	46.520564
2969.883848	76600.396701	46.525569
2966.030096	76297.823336	46.530573
2962.415433	75987.646826	46.535578
2958.964368	75694.503999	46.540583
2955.852009	75391.354896	46.545588
2951.811274	75093.916734	46.550593
2948.013187	74802.641164	46.555597
2944.594455	74508.033031	46.560602
2940.966325	74215.086350	46.565607
2937.319491	73928.317454	46.570612
2933.730995	73637.364614	46.575617
2930.364148	73350.951781	46.580621
2926.360470	73068.362274	46.585626
2922.686621	72793.457483	46.590631
2918.788607	72512.355767	46.595636
2915.594483	72246.790994	46.600641
2911.998034	71977.723678	46.605645
2908.367760	71705.883565	46.610650
2904.714208	71433.694359	46.615655
2901.255703	71175.647957	46.620660
2897.442502	70913.837629	46.625665
2893.750798	70647.795400	46.630669
2890.409731	70400.823019	46.635674
2886.473588	70147.546709	46.640679
2882.934265	69881.056750	46.645684
2879.208237	69635.408818	46.650689
2875.438347	69395.762916	46.655693
2872.069229	69148.876620	46.660698
2868.134719	68910.441732	46.665703
2864.374892	68673.708427	46.670708
2861.149147	68428.653899	46.675713
2857.703752	68193.723121	46.680717
2854.464307	67965.827607	46.685722
2850.456779	67726.938978	46.690727
2847.011032	67495.677398	46.695732
2844.068396	67270.915575	46.700737
2840.326094	67035.692694	46.705741
2836.897846	66792.405691	46.710746
2832.934481	66567.727171	46.715751
2829.487075	66344.715528	46.720756
2826.139818	66111.311931	46.725761
2822.272690	65886.097532	46.730765
2819.157021	65648.548792	46.735770
2815.482139	65423.892395	46.740775
2812.122444	65201.016727	46.745780
2808.609057	64958.306476	46.750785
2805.026694	64754.428850	46.755789
2801.801318	64517.441064	46.760794
2798.133508	64290.565805	46.765799
2794.509309	64058.424083	46.770804
2791.026395	63841.539587	46.775809
2787.191813	63616.943338	46.780813
2783.845946	63382.117685	46.785818
2780.775334	63170.505888	46.790823
2777.526077	62931.550283	46.795828
2773.759923	62700.281148	46.800833
2770.026355	62489.273870	46.805837
2766.890355	62246.956102	46.810842
2763.456408	62021.835584	46.815847
2759.633692	61802.369150	46.820852
2756.332359	61562.044996	46.825857
2752.594178	61333.906668	46.830861
2749.289614	61108.101525	46.835866
2746.125143	60886.801399	46.840871
2742.710983	60651.510942	46.845876
2739.180839	60419.420277	46.850881
2735.461324	60186.764901	46.855885
2731.925829	59949.088663	46.860890
2728.330184	59716.964134	46.865895
2725.005321	59490.758226	46.870900
2721.565089	59256.094465	46.875905
2718.038074	59029.778501	46.880909
2714.843851	58798.450266	46.885914
2710.860644	58570.217392	46.890919
2707.190130	58327.584093	46.895924
2703.947106	58095.001089	46.900929
2700.259894	57875.567755	46.905933
2696.602060	57647.102337	46.910938
2693.433859	57421.817652	46.915943
2689.574353	57180.177245	46.920948
2686.355802	56958.362942	46.925953
2682.603077	56734.851254	46.930957
2679.354896	56503.781880	46.935962
2675.813383	56272.221289	46.940967
2672.211237	56059.390065	46.945972
2668.837959	55816.107467	46.950977
2665.038969	55590.932314	46.955981
2661.901041	55358.264222	46.960986
2658.478914	55128.631221	46.965991
2654.672089	54899.498395	46.970996
2651.636646	54668.343748	46.976001
2647.912628	54447.824644	46.981005
2644.445575	54213.690226	46.986010
2641.036608	53981.801310	46.991015
2637.253914	53752.016011	46.996020
2634.096144	53518.125617	47.001025
2630.352596	53290.324465	47.006029
2626.878750	53059.057490	47.011034
2623.428510	52826.793078	47.016039
2619.940571	52596.979320	47.021044
2616.504781	52364.748953	47.026049
2613.068925	52136.244781	47.031053
2609.650958	51888.600656	47.036058
2605.611908	51658.666651	47.041063
2602.110354	51434.943818	47.046068
2599.000140	51194.858720	47.051073
2595.546498	50965.981861	47.056077
2591.819180	50734.073459	47.061082
2588.914625	50508.242598	47.066087
2584.926914	50271.228673	47.071092
2581.760939	50033.612896	47.076097
2577.800781	49798.293195	47.081101
2574.714838	49562.579084	47.086106
2571.066061	49328.255774	47.091111
2567.403242	49092.579634	47.096116
2563.728264	48863.961255	47.101121
2560.280982	48632.239553	47.106125
2557.069833	48383.129124	47.111130
2553.469192	48160.106926	47.116135
2549.477704	47927.665624	47.121140
2546.680539	47696.061048	47.126145
2542.598496	47460.663960	47.131149
2539.182219	47226.763498	47.136154
2535.855934	46994.703381	47.141159
2532.240478	46756.843153	47.146164
2528.927166	46528.622957	47.151169
2525.075728	46290.886999	47.156173
2521.579272	46060.569173	47.161178
2517.962513	45824.076219	47.166183
2514.657556	45599.599663	47.171188
2511.141594	45366.920043	47.176193
2508.022644	45135.766226	47.181197
2504.415437	44897.163324	47.186202
2501.061773	44665.353468	47.191207
2497.507912	44439.392745	47.196212
2494.073654	44185.581829	47.201217
2490.035380	43954.260615	47.206221
2486.892755	43721.552410	47.211226
2483.358864	43491.780551	47.216231
2479.888271	43247.663166	47.221236
2476.374400	43008.514192	47.226241
2472.703908	42771.561027	47.231245
2469.505020	42547.612263	47.236250
2465.973489	42310.242810	47.241255
2462.380540	42079.366129	47.246260
2458.996480	41847.146597	47.251265
2454.859539	41607.685424	47.256269
2451.701559	41368.530267	47.261274
2448.343972	41126.301932	47.266279
2444.734686	40897.431253	47.271284
2441.506821	40655.834587	47.276289
2437.960517	40430.725316	47.281293
2434.314359	40185.585128	47.286298
2430.865147	39950.770909	47.291303
2427.133617	39713.257985	47.296308
2424.047427	39466.072770	47.301313
2420.037181	39223.149766	47.306317
2417.034417	38989.201780	47.311322
2413.622364	38759.726748	47.316327
2409.816150	38519.277742	47.321332
2406.648652	38283.175837	47.326337
2402.959352	38037.679944	47.331341
2399.509920	37795.674287	47.336346
2395.898020	37552.029404	47.341351
2392.242200	37321.631491	47.346356
2389.144791	37079.699283	47.351361
2385.593124	36842.804761	47.356365
2381.937350	36603.127084	47.361370
2378.744166	36355.842136	47.366375
2374.750642	36112.526911	47.371380
2371.428719	35868.399399	47.376385
2367.740742	35644.116666	47.381389
2364.414024	35390.695743	47.386394
2360.756716	35155.712886	47.391399
2357.304130	34913.626272	47.396404
2353.995546	34671.190272	47.401409
2350.398367	34432.725956	47.406413
2347.049007	34185.199123	47.411418
2343.592340	33937.844110	47.416423
2340.075609	33697.809853	47.421428
2336.459240	33441.757341	47.426433
2332.887559	33211.111979	47.431437
2329.151096	32971.405628	47.436442
2325.864952	32729.305394	47.441447
2322.533761	32492.285630	47.446452
2318.996200	32250.344359	47.451457
2315.538220	32007.436384	47.456461
2312.177972	31758.520144	47.461466
2308.789483	31513.217608	47.466471
2305.300877	31269.378672	47.471476
2301.456221	31021.269559	47.476481
2297.972062	30780.078552	47.481485
2294.688308	30529.865823	47.486490
2291.017218	30280.661020	47.491495
2287.341223	30033.583064	47.496500
2284.553623	29785.728994	47.501505
2280.377852	29545.002825	47.506509
2277.010324	29290.971428	47.511514
2273.891191	29049.122483	47.516519
2270.159328	28798.912145	47.521524
2266.650811	28553.676210	47.526529
2263.177380	28299.173027	47.531533
2259.779746	28049.489885	47.536538
2256.086386	27811.357438	47.541543
2252.236714	27568.195481	47.546548
2249.047451	27316.296189	47.551553
2245.510202	27061.533277	47.556557
2242.016306	26815.694957	47.561562
2238.526538	26573.008191	47.566567
2235.128103	26317.941416	47.571572
2231.828205	26065.599720	47.576577
2227.874319	25816.480915	47.581581
2224.588542	25569.991537	47.586586
2221.044271	25308.427751	47.591591
2217.114461	25080.159951	47.596596
2214.268790	24822.788980	47.601601
2210.738837	24573.752277	47.606605
2207.097754	24324.001103	47.611610
2203.335061	24073.676516	47.616615
2200.311637	23824.113710	47.621620
2197.002345	23569.131189	47.626625
2193.629910	23313.813354	47.631629
2189.754072	23048.105205	47.636634
2186.474885	22805.304295	47.641639
2182.804538	22547.255376	47.646644
2179.389202	22293.154699	47.651649
2175.474704	22043.690264	47.656653
2172.221267	21787.176098	47.661658
2168.732569	21525.235073	47.666663
2165.197252	21274.200647	47.671668
2161.940162	21013.611154	47.676673
2158.300640	20761.199592	47.681677
2154.633154	20504.532496	47.686682
2151.423863	20240.246387	47.691687
2147.652310	19998.000418	47.696692
2144.593058	19741.070774	47.701697
2140.843360	19490.517065	47.706701
2137.410742	19226.849641	47.711706
2133.882791	18973.468181	47.716711
2130.249982	18716.021010	47.721716
2126.894174	18460.497405	47.726721
2122.736329	18211.664460	47.731725
2118.851447	17957.661683	47.736730
2115.352688	17718.131182	47.741735
2111.406566	17480.168359	47.746740
2107.354120	17247.633895	47.751745
2103.615413	17032.014023	47.756749
2100.186330	16796.385419	47.761754
2096.454582	16579.692845	47.766759
2092.193077	16365.039391	47.771764
2088.572316	16151.371044	47.776769
2084.439460	15959.973077	47.781773
2080.398449	15766.371433	47.786778
2076.988163	15578.087719	47.791783
2072.901633	15400.345084	47.796788
2069.521892	15196.332645	47.801793
2065.797752	15021.500588	47.806797
2062.338708	14835.796578	47.811802
2058.702077	14665.773269	47.816807
2055.025664	14499.541420	47.821812
2051.791888	14318.205185	47.826817
2048.208403	14149.390851	47.831821
2044.868406	13965.161667	47.836826
2041.708210	13798.323254	47.841831
2038.058942	13623.948252	47.846836
2034.355802	13449.459805	47.851841
2030.789754	13278.475371	47.856845
2027.447492	13107.587275	47.861850
2024.190433	12932.495565	47.866855
2020.346003	12761.815811	47.871860
2017.389844	12588.355023	47.876865
2013.802225	12418.606978	47.881869
2010.427345	12247.598798	47.886874
2007.144835	12074.519891	47.891879
2003.257951	11900.932467	47.896884
1999.900847	11723.775005	47.901889
1995.952511	11556.294602	47.906893
1992.788880	11386.568674	47.911898
1989.696066	11207.554411	47.916903
1986.175473	11035.668330	47.921908
1982.716115	10851.997907	47.926913
1979.010791	10690.388053	47.931917
1975.505089	10516.405586	47.936922
1972.257588	10336.866705	47.941927
1968.253450	10167.169398	47.946932
1965.279835	9989.382713	47.951937
1961.336911	9819.352946	47.956941
1957.661875	9647.364536	47.961946
1954.283656	9467.987431	47.966951
1950.805528	9300.833543	47.971956
1947.524300	9138.819432	47.976961
1943.709482	8972.056723	47.981965
1940.599924	8794.214108	47.986970
1937.396695	8618.280709	47.991975
1933.720182	8448.376920	47.996980
1930.351911	8264.638657	48.001985
1926.445343	8089.997812	48.006989
1922.936538	7924.032285	48.011994
1919.657534	7742.864871	48.016999
1916.151184	7584.792743	48.022004
1912.765225	7401.907762	48.027009
1909.174797	7226.291932	48.032013
1905.535411	7052.499005	48.037018
1902.661428	6870.593147	48.042023
1898.563135	6696.473446	48.047028
1895.536840	6516.883204	48.052033
1891.321232	6355.353098	48.057037
1887.797526	6180.531230	48.062042
1884.794334	6007.927265	48.067047
1881.370206	5826.155840	48.072052
1877.812595	5648.853645	48.077057
1874.252728	5477.487458	48.082061
1870.632523	5303.420146	48.087066
1867.178912	5118.261463	48.092071
1863.881342	4950.900507	48.097076
1860.493899	4765.798347	48.102081
1856.498423	4596.166897	48.107085
1852.898597	4416.206053	48.112090
1850.041796	4245.203482	48.117095
1846.317154	4073.762387	48.122100
1842.789501	3890.634109	48.127105
1839.241165	3717.801737	48.132109
1835.562540	3537.909416	48.137114
1832.070480	3354.160772	48.142119
1828.504089	3189.218790	48.147124
1824.883342	3013.537573	48.152129
1821.124173	2842.322415	48.157133
1817.964428	2664.218217	48.162138
1814.363579	2489.409175	48.167143
1810.577088	2322.541417	48.172148
1807.344091	2151.345421	48.177153
1803.872386	1982.014130	48.182157
1800.072625	1807.423212	48.187162
1796.655450	1636.276774	48.192167
1792.803015	1480.235724	48.197172
1789.712430	1305.915237	48.202177
1785.825936	1150.249427	48.207181
1781.987451	984.478038	48.212186
1778.696315	836.916498	48.217191
1774.798178	674.637674	48.222196
1771.267906	517.871215	48.227201
1767.376769	377.826716	48.232205
1763.553078	228.641907	48.237210
1759.610852	93.619176	48.242215
1753.849690	20.946456	48.247220
1744.644076	37.225573	48.252225
1737.756362	46.216371	48.257229
1733.708655	57.312747	48.262234
1730.839467	49.994791	48.267239
1728.252525	60.277253	48.272244
1726.113829	45.843458	48.277249
1723.442593	50.314530	48.282253
1719.938515	49.043909	48.287258
1716.372459	60.125024	48.292263
1712.617350	53.657581	48.297268
1709.825142	49.269931	48.302273
1706.151748	49.775402	48.307277
1702.917229	56.397442	48.312282
1700.131993	44.817360	48.317287
1696.071518	46.085780	48.322292
1692.563785	50.434670	48.327297
1689.476898	49.266449	48.332301
1685.840352	55.147804	48.337306
1682.490706	48.461892	48.342311
1679.140872	53.513751	48.347316
1675.428329	48.096377	48.352321
1672.410770	50.340554	48.357325
1668.562530	52.904570	48.362330
1665.508239	52.183680	48.367335
1661.727185	60.887634	48.372340
1658.267607	57.082183	48.377345
1654.792217	54.278973	48.382349
1651.138467	53.341855	48.387354
1648.325418	53.304562	48.392359
1644.319482	56.573487	48.397364
1641.313893	52.219254	48.402369
1637.794824	53.358668	48.407373
1634.256779	50.147650	48.412378
1630.600590	44.844864	48.417383
1626.846816	55.211883	48.422388
1623.767321	49.840986	48.427393
1620.112691	48.711024	48.432397
1616.940479	49.353225	48.437402
1613.511709	39.506426	48.442407
1609.644315	54.396495	48.447412
1606.240058	48.994174	48.452417
1602.563995	52.388657	48.457421
1599.240416	46.423210	48.462426
1595.957876	45.038864	48.467431
1592.416658	56.505269	48.472436
1589.252701	49.261972	48.477441
1585.728169	52.683365	48.482445
1581.847346	55.208218	48.487450
1578.582718	47.104308	48.492455
1574.587865	51.633882	48.497460
1571.558199	49.827144	48.502465
1567.950976	54.792768	48.507469
1564.505718	54.424173	48.512474
1560.959109	49.607308	48.517479
1557.610757	51.669171	48.522484
1554.228502	55.441634	48.527489
1550.363870	50.978275	48.532493
1547.168809	60.049295	48.537498
1543.971288	46.448851	48.542503
1540.181788	54.347389	48.547508
1536.501569	45.868775	48.552513
1533.299421	50.502083	48.557517
1529.505307	48.112646	48.562522
1526.194850	43.309454	48.567527
1522.569358	45.705776	48.572532
1519.008727	44.396622	48.577537
1515.798306	46.209114	48.582541
1511.675594	51.451597	48.587546
1508.635193	48.276631	48.592551
1505.289952	48.382791	48.597556
1501.930276	43.726520	48.602561
1498.138061	41.703800	48.607565
1494.476405	49.053984	48.612570
1491.526913	46.668401	48.617575
1487.824641	58.489078	48.622580
1484.368752	60.390623	48.627585
1480.725232	54.443659	48.632589
1477.296935	53.300470	48.637594
1473.911609	48.075575	48.642599
1470.338483	48.758427	48.647604
1466.746496	44.467567	48.652609
1463.112698	54.724102	48.657613
1460.085161	51.021947	48.662618
1456.342835	55.401303	48.667623
1452.721137	47.441921	48.672628
1449.229532	50.146346	48.677633
1445.708199	43.664575	48.682637
1442.094018	52.608229	48.687642
1438.569769	38.359779	48.692647
1435.384238	49.080834	48.697652
1431.923971	54.988459	48.702657
1428.835632	48.824899	48.707661
1424.386464	53.995127	48.712666
1421.389847	50.547576	48.717671
1417.776021	51.407663	48.722676
1414.380663	49.585450	48.727681
1411.040868	43.549847	48.732685
1407.286596	43.745377	48.737690
1403.893472	40.824979	48.742695
1400.229517	50.023212	48.747700
1396.450818	48.444512	48.752705
1393.168481	51.720485	48.757709
1390.069714	43.783681	48.762714
1386.453221	50.199834	48.767719
1382.827023	46.752770	48.772724
1379.385291	35.493883	48.777729
1376.056448	51.476640	48.782733
1372.417278	54.017527	48.787738
1368.667555	51.697135	48.792743
1365.073069	55.047290	48.797748
1361.972782	50.556114	48.802753
1358.535086	53.097104	48.807757
1355.029054	54.095366	48.812762
1351.382089	44.864972	48.817767
1348.008716	53.976605	48.822772
1343.952883	50.957484	48.827777
1340.981398	52.299187	48.832781
1337.218530	54.925888	48.837786
1333.744141	44.361837	48.842791
1330.351347	44.045222	48.847796
1326.993742	49.101562	48.852801
1323.828607	44.914785	48.857805
1319.784405	50.698713	48.862810
1316.132782	50.296069	48.867815
1312.293544	50.976342	48.872820
1309.279113	45.766217	48.877825
1306.026581	46.205949	48.882829
1302.502296	56.961086	48.887834
1298.826043	44.628447	48.892839
1295.606833	50.058606	48.897844
1291.941446	51.673467	48.902849
1288.314791	49.419265	48.907853
1284.623149	48.921655	48.912858
1281.578722	40.122162	48.917863
1277.845383	50.663251	48.922868
1274.289520	58.123496	48.927873
1270.976958	53.548520	48.932877
1267.079338	50.817882	48.937882
1263.385881	50.387005	48.942887
1260.467080	43.295286	48.947892
1257.276181	45.142767	48.952897
1253.657842	40.865611	48.957901
1249.787392	49.254643	48.962906
1246.318460	42.809044	48.967911
1243.044793	48.614744	48.972916
1239.290634	49.044441	48.977921
1236.067096	44.677010	48.982925
1232.206937	50.422667	48.987930
1228.806721	46.244252	48.992935
1225.077325	49.938281	48.997940
1221.824939	47.549582	49.002945
1218.324011	50.742768	49.007949
1214.527117	55.896389	49.012954
1211.417290	49.938757	49.017959
1207.846638	43.901409	49.022964
1204.582722	42.223212	49.027969
1201.100370	46.859351	49.032973
1197.248826	38.410877	49.037978
1193.872512	44.596496	49.042983
1190.109933	48.105905	49.047988
1186.622490	52.613130	49.052993
1183.191391	46.917781	49.057997
1179.937666	56.301797	49.063002
1176.574030	48.495126	49.068007
1172.448218	52.222761	49.073012
1168.942812	51.360677	49.078017
1165.487984	41.021434	49.083021
1162.222131	54.922089	49.088026
1159.212344	49.986540	49.093031
1155.096338	54.661787	49.098036
1151.507846	53.436225	49.103041
1148.700216	53.024897	49.108045
1144.603521	47.136371	49.113050
1141.427939	43.523944	49.118055
1137.744591	50.690969	49.123060
1134.377938	50.731004	49.128065
1130.938560	48.653190	49.133069
1127.317690	47.825018	49.138074
1123.682686	46.030939	49.143079
1120.527831	48.676424	49.148084
1116.381614	53.144440	49.153089
1113.326371	42.881867	49.158093
1109.808877	48.782727	49.163098
1106.731202	55.516413	49.168103
1102.654597	54.294523	49.173108
1099.186405	52.623034	49.178113
1095.808246	41.534654	49.183117
1091.822990	51.893774	49.188122
1089.045017	46.899810	49.193127
1085.234190	48.420456	49.198132
1081.844897	51.428529	49.203137
1078.575374	53.304196	49.208141
1074.541812	39.638706	49.213146
1071.144819	41.562805	49.218151
1067.804479	37.349770	49.223156
1064.003644	49.027799	49.228161
1060.703679	48.902392	49.233165
1057.257948	52.934888	49.238170
1053.996633	43.062111	49.243175
1050.087643	45.816200	49.248180
1046.514924	47.359692	49.253185
1043.292465	46.443863	49.258189
1039.644235	51.634380	49.263194
1036.145154	44.813933	49.268199
1032.717365	52.200411	49.273204
1029.049630	49.734441	49.278209
1025.697137	39.262179	49.283213
1022.186020	50.084929	49.288218
1019.038742	41.991347	49.293223
1015.209450	48.950306	49.298228
1011.705260	48.869547	49.303233
1008.083663	45.073898	49.308237
1004.762568	44.992948	49.313242
1001.317508	41.365817	49.318247
997.786536	51.308985	49.323252
994.230022	47.727779	49.328257
990.729590	48.184285	49.333261
987.048313	54.892287	49.338266
983.927887	49.407805	49.343271
980.372352	52.119234	49.348276
976.769637	51.367371	49.353281
973.181872	45.437207	49.358285
969.375593	49.076926	49.363290
965.908054	43.710078	49.368295
962.319785	51.251420	49.373300
959.179807	48.955947	49.378305
955.832767	52.738902	49.383309
952.036662	54.798303	49.388314
948.810262	50.073919	49.393319
945.087945	51.498502	49.398324
941.448059	56.447298	49.403329
938.318039	46.525537	49.408333
934.687718	47.685780	49.413338
931.221730	46.434794	49.418343
927.570508	51.255654	49.423348
924.016523	48.949088	49.428353
920.339814	37.277944	49.433357
916.581634	48.060312	49.438362
913.522164	40.149180	49.443367
910.094672	49.759791	49.448372
906.573514	48.833832	49.453377
903.401921	45.492952	49.458381
899.476346	53.966665	49.463386
896.094538	42.983350	49.468391
892.623312	52.230652	49.473396
889.032348	39.704527	49.478401
885.705488	31.310090	49.483405
882.398555	42.686202	49.488410
878.965534	42.407686	49.493415
875.333015	42.745710	49.498420
871.439433	47.829167	49.503425
868.150460	45.313446	49.508429
864.511587	45.810659	49.513434
860.658981	42.234745	49.518439
857.303290	42.839478	49.523444
853.868134	47.246874	49.528449
850.556697	46.243804	49.533453
847.072562	53.107645	49.538458
843.434241	44.632277	49.543463
840.209988	42.077958	49.548468
836.345349	48.830540	49.553473
833.084058	33.481345	49.558477
829.449211	43.567375	49.563482
825.918734	38.204116	49.568487
822.738619	45.804973	49.573492
819.112110	40.877538	49.578497
815.810144	37.588745	49.583501
811.954869	41.201392	49.588506
808.784682	47.490892	49.593511
805.028324	40.210956	49.598516
801.291539	47.813569	49.603521
798.326580	31.111346	49.608525
794.275430	43.031132	49.613530
790.479650	39.262852	49.618535
787.341972	38.539483	49.623540
783.628644	41.693310	49.628545
781.044445	33.014939	49.633549
777.237332	44.649741	49.638554
773.531212	38.931191	49.643559
769.991762	48.723890	49.648564
766.256305	39.444351	49.653569
762.862745	26.241973	49.658573
759.508245	40.204046	49.663578
756.220482	44.072695	49.668583
752.463022	42.674432	49.673588
748.753431	43.081522	49.678593
745.637258	39.001189	49.683597
741.550352	37.913953	49.688602
738.294015	38.556954	49.693607
734.852492	40.769720	49.698612
731.423484	43.062786	49.703617
728.167247	38.662705	49.708621
724.479399	39.572605	49.713626
721.116492	50.071669	49.718631
717.513236	38.484036	49.723636
713.588830	45.777535	49.728641
710.544493	43.897449	49.733645
706.372140	51.811919	49.738650
703.728853	41.342632	49.743655
700.226076	43.141056	49.748660
696.356468	54.833133	49.753665
693.149360	38.191021	49.758669
689.302744	41.656825	49.763674
685.781418	44.862878	49.768679
682.499505	42.447363	49.773684
678.980147	45.403173	49.778689
675.678545	30.886117	49.783693
671.508007	44.795678	49.788698
668.251190	41.768792	49.793703
664.778547	44.416731	49.798708
661.395212	40.893965	49.803713
658.166818	38.213812	49.808717
654.372083	53.845739	49.813722
650.744352	40.180201	49.818727
647.159540	42.902661	49.823732
644.026474	44.301516	49.828737
640.732215	38.648239	49.833741
636.661676	46.986554	49.838746
633.343592	48.733932	49.843751
630.267743	41.233605	49.848756
626.119181	44.946042	49.853761
622.985504	27.548985	49.858765
619.020162	39.417424	49.863770
615.604282	33.182089	49.868775
612.298157	32.811031	49.873780
608.972153	37.419712	49.878785
605.470881	42.090647	49.883789
601.862614	42.947003	49.888794
598.639008	44.233503	49.893799
594.772565	42.298713	49.898804
590.835329	41.273526	49.903809
587.777246	41.749488	49.908813
584.247906	40.419973	49.913818
580.846280	32.698608	49.918823
577.183194	35.129630	49.923828
573.790582	41.485670	49.928833
570.461748	33.651667	49.933837
567.110321	48.293524	49.938842
563.453504	43.855005	49.943847
560.202503	31.408683	49.948852
556.005652	35.989258	49.953857
552.816979	31.316073	49.958861
549.035490	46.819398	49.963866
544.959133	42.522527	49.968871
542.438211	37.425217	49.973876
538.955943	48.173981	49.978881
535.346684	42.646014	49.983885
531.628274	47.600923	49.988890
527.860654	45.204592	49.993895
524.451634	30.938554	49.998900
521.271477	35.641480	50.003905
517.936689	29.409306	50.008909
514.038487	41.159697	50.013914
510.996347	38.352350	50.018919
507.361193	45.587966	50.023924
503.688656	39.475134	50.028929
500.534089	44.882747	50.033933
496.586663	39.964588	50.038938
493.278951	41.960328	50.043943
489.396595	42.777400	50.048948
485.716239	41.772137	50.053953
482.553193	34.573435	50.058957
479.209678	37.621996	50.063962
475.672631	40.903354	50.068967
472.275528	45.045488	50.073972
468.608929	39.539188	50.078977
465.405098	30.957985	50.083981
461.713095	43.802401	50.088986
458.136587	37.538507	50.093991
454.908679	36.993904	50.098996
451.257116	43.368397	50.104001
447.552146	32.318857	50.109005
444.080539	43.983471	50.114010
440.876024	45.735273	50.119015
437.702939	35.080155	50.124020
433.757251	52.409424	50.129025
430.307763	39.250761	50.134029
426.693965	38.984912	50.139034
422.907954	32.149571	50.144039
419.532474	29.698195	50.149044
416.021862	36.012655	50.154049
412.505388	39.974189	50.159053
409.141410	41.118225	50.164058
405.684241	37.290751	50.169063
402.282759	36.226022	50.174068
398.554485	41.340713	50.179073
395.203474	40.255426	50.184077
391.626445	35.272974	50.189082
387.976505	40.720249	50.194087
384.419313	35.902373	50.199092
381.002471	40.044465	50.204097
377.798835	34.756756	50.209101
374.102859	46.314167	50.214106
370.660899	44.692639	50.219111
367.114384	38.930292	50.224116
363.110064	37.156410	50.229121
359.934513	28.327214	50.234125
356.825452	37.173087	50.239130
353.064031	35.655393	50.244135
349.746323	29.718010	50.249140
346.132172	28.784694	50.254145
342.968243	35.750394	50.259149
339.130146	38.000113	50.264154
335.306141	35.438694	50.269159
332.161354	38.443522	50.274164
328.468799	46.577211	50.279169
325.292969	36.188330	50.284173
321.480848	31.467364	50.289178
317.742624	37.365094	50.294183
314.418572	29.815196	50.299188
310.949838	44.032561	50.304193
307.405018	30.566195	50.309197
304.006760	37.818552	50.314202
300.664165	35.994825	50.319207
297.374927	39.591772	50.324212
293.397648	42.242966	50.329217
290.274327	26.650969	50.334221
286.318749	40.365632	50.339226
282.083007	39.662594	50.344231
279.333200	42.994709	50.349236
275.667528	39.962422	50.354241
273.082406	30.778177	50.359245
269.464874	32.309999	50.364250
265.996573	30.464850	50.369255
262.175053	30.272738	50.374260
258.447594	33.432143	50.379265
254.837039	31.220140	50.384269
250.894466	34.096870	50.389274
247.698885	30.234813	50.394279
244.557871	30.840942	50.399284
240.791396	29.725888	50.404289
237.258265	29.577195	50.409293
234.242097	25.861046	50.414298
230.638442	38.460733	50.419303
226.868043	29.174287	50.424308
223.454162	40.776135	50.429313
220.231939	33.058465	50.434317
216.256409	44.770452	50.439322
212.705996	38.799977	50.444327
209.441986	33.123161	50.449332
205.612800	34.979233	50.454337
202.331045	31.285719	50.459341
198.743792	32.876101	50.464346
195.155870	40.019001	50.469351
191.587212	37.129742	50.474356
188.489306	36.900230	50.479361
185.017281	30.522019	50.484365
181.457308	44.152597	50.489370
178.237464	42.936114	50.494375
174.622834	36.551772	50.499380
170.902936	43.582480	50.504385
167.412196	30.129862	50.509389
163.874130	35.607148	50.514394
160.058484	33.854424	50.519399
156.923950	32.672041	50.524404
153.193637	38.426224	50.529409
149.640297	33.709090	50.534413
146.685190	39.034941	50.539418
143.197455	36.117206	50.544423
139.621120	26.404932	50.549428
135.644826	45.472820	50.554433
132.233785	27.698685	50.559437
128.702867	29.166373	50.564442
125.226134	31.954355	50.569447
121.752003	33.096773	50.574452
117.951509	34.682630	50.579457
115.054627	37.503158	50.584461
111.571616	42.589023	50.589466
107.891367	30.700553	50.594471
104.322801	31.655292	50.599476
100.916096	40.237820	50.604481
97.648650	31.612961	50.609485
94.235809	40.886154	50.614490
90.333638	33.822402	50.619495
86.635127	34.772197	50.624500
83.049569	41.917931	50.629505
79.505747	47.124068	50.634509
76.386181	43.275478	50.639514
72.578707	41.894837	50.644519
68.954542	42.149618	50.649524
65.255868	43.159560	50.654529
62.143178	38.253201	50.659533
58.696978	41.175631	50.664538
55.372444	33.888516	50.669543
52.047040	33.179004	50.674548
47.965877	46.489483	50.679553
45.214722	39.941441	50.684557
41.483621	44.427122	50.689562
38.005236	40.296244	50.694567
34.490979	39.749206	50.699572
30.823149	46.075781	50.704577
27.212609	41.025976	50.709581
23.860764	36.397551	50.714586
20.065783	29.465739	50.719591
16.555448	36.533269	50.724596
12.969845	30.875288	50.729601
9.540352	37.968120	50.734605
5.984811	40.072468	50.739610
2.692533	42.417143	50.744615