Thu Aug 25 09:40:54 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
1.337254	107.103732	0.000000
1.053745	109.802719	0.005005
1.014886	108.223917	0.010010
1.450194	104.324543	0.015014
0.737546	99.984935	0.020019
0.346429	83.329013	0.025024
0.157278	79.948268	0.030029
-0.155995	69.639338	0.035034
-0.040780	57.795290	0.040038
-0.616012	54.835711	0.045043
-0.759383	41.450308	0.050048
-0.453229	39.390347	0.055053
-0.904028	27.717262	0.060058
-1.197878	16.551105	0.065062
-1.985888	15.089691	0.070067
-2.278747	6.451226	0.075072
-2.188275	1.169559	0.080077
-2.728553	4.930655	0.085082
-2.770124	-5.170866	0.090086
-3.418352	-8.913100	0.095091
-4.046960	-17.337594	0.100096
-4.297715	-7.379783	0.105101
-5.010255	0.552819	0.110106
-5.061071	-6.510048	0.115110
-4.936746	0.332813	0.120115
-5.153537	-18.577609	0.125120
-5.396035	-18.264207	0.130125
-5.111864	-15.859828	0.135130
-5.067180	-8.972854	0.140134
-5.973793	-9.691183	0.145139
-6.060921	-6.149788	0.150144
-6.087111	-16.538450	0.155149
-7.448841	-10.278999	0.160154
-7.399446	-13.029552	0.165158
-7.770193	0.427192	0.170163
-7.943670	-7.030908	0.175168
-8.060176	-5.677389	0.180173
-7.879340	-4.560285	0.185178
-7.694313	-9.679594	0.190182
-8.057783	-7.341418	0.195187
-8.272806	-14.112798	0.200192
-8.793575	-5.985620	0.205197
-9.130513	-7.350029	0.210202
-9.863705	-15.590458	0.215206
-10.099806	-7.457264	0.220211
-10.297297	-13.449944	0.225216
-10.592692	-10.337825	0.230221
-10.596669	-16.006484	0.235226
-10.403319	-14.815411	0.240230
-10.619020	-12.500389	0.245235
-11.300220	-14.623941	0.250240
-11.706509	-21.915842	0.255245
-12.311795	-9.548653	0.260250
-11.567782	-21.886638	0.265254
-12.076227	-11.350616	0.270259
-12.447992	-12.149583	0.275264
-12.771963	-15.183320	0.280269
-13.732629	-4.937105	0.285274
-13.269444	-9.290076	0.290278
-13.376188	-6.852921	0.295283
-13.619063	-10.057552	0.300288
-14.243791	-5.574546	0.305293
-14.831123	-2.489450	0.310298
-14.833401	-13.916406	0.315302
-15.287900	-3.743172	0.320307
-14.838831	-16.139352	0.325312
-15.006146	-11.658415	0.330317
-15.551395	-0.673695	0.335322
-15.392446	-13.951399	0.340326
-15.905485	-9.014494	0.345331
-16.034280	-21.914913	0.350336
-15.952841	-7.643177	0.355341
-17.170291	-12.337094	0.360346
-17.114144	-9.928625	0.365350
-17.491789	-19.977478	0.370355
-17.750515	-12.068531	0.375360
-17.188102	-12.751278	0.380365
-18.062926	-6.333999	0.385370
-18.478257	-17.617140	0.390374
-19.346848	-19.148181	0.395379
-19.180120	-19.234256	0.400384
-19.159186	-9.059588	0.405389
-19.352539	-10.221867	0.410394
-19.372424	-13.043822	0.415398
-19.253454	-17.184670	0.420403
-20.371207	-9.432190	0.425408
-20.678073	-11.244235	0.430413
-21.004064	-1.840945	0.435418
-20.687473	-14.539071	0.440422
-20.964194	-18.485042	0.445427
-20.982950	-21.633039	0.450432
-21.754887	-14.953473	0.455437
-22.234704	-7.544556	0.460442
-22.104887	-16.644703	0.465446
-22.283542	-8.355996	0.470451
-22.486626	-13.224667	0.475456
-22.313229	-20.645361	0.480461
-23.269972	-14.288014	0.485466
-23.546422	-13.191010	0.490470
-23.869536	-16.829156	0.495475
-23.808566	-14.627087	0.500480
-23.744169	-12.843170	0.505485
-24.439771	-11.819695	0.510490
-24.450963	-14.431040	0.515494
-25.322039	-8.792631	0.520499
-25.623767	-15.284668	0.525504
-25.169832	-16.216174	0.530509
-25.636747	-4.338898	0.535514
-25.399478	-5.394642	0.540518
-26.299246	-2.877523	0.545523
-26.808711	-6.961035	0.550528
-26.599595	-11.153975	0.555533
-26.804077	-6.135702	0.560538
-26.993470	-7.906042	0.565542
-27.375603	-1.429917	0.570547
-27.521573	-7.215535	0.575552
-27.486496	-2.155703	0.580557
-28.106584	-1.713535	0.585562
-27.721647	-5.209525	0.590566
-28.430999	-0.264005	0.595571
-29.074209	-10.435767	0.600576
-29.523706	-13.633332	0.605581
-29.830040	-6.178831	0.610586
-29.731994	-6.893222	0.615590
-29.832794	-9.031783	0.620595
-29.829960	-8.364516	0.625600
-29.780219	-13.965662	0.630605
-30.944222	-11.011673	0.635610
-30.921939	-16.627498	0.640614
-31.250109	-6.480388	0.645619
-31.708899	-7.819375	0.650624
-31.481901	-17.102427	0.655629
-31.842349	-8.702978	0.660634
-31.840228	-4.893993	0.665638
-32.586803	-11.300511	0.670643
-32.855768	-12.700878	0.675648
-32.954062	-10.834522	0.680653
-32.725114	-5.137517	0.685658
-33.145808	-6.058530	0.690662
-33.760212	-10.511576	0.695667
-34.170775	-10.447087	0.700672
-34.087296	-8.210579	0.705677
-34.338622	-9.480833	0.710682
-34.407474	-24.225616	0.715686
-34.697284	-9.465444	0.720691
-35.273744	-8.473291	0.725696
-35.182853	-8.186816	0.730701
-35.504786	-6.851730	0.735706
-35.787645	-10.281049	0.740710
-36.113969	-10.463876	0.745715
-36.827381	-9.779294	0.750720
-36.644627	-16.413681	0.755725
-37.271987	-10.810296	0.760730
-36.922849	-18.274345	0.765734
-37.129439	-16.099956	0.770739
-37.476768	-17.181160	0.775744
-38.098898	-13.448371	0.780749
-38.128466	-12.564056	0.785754
-38.478973	-13.078451	0.790758
-38.617885	-8.073617	0.795763
-38.775888	-5.226633	0.800768
-38.767097	-5.531570	0.805773
-39.828090	-9.800746	0.810778
-40.004373	-2.360294	0.815782
-39.893761	-12.124985	0.820787
-39.843071	-9.114548	0.825792
-40.086573	-13.571925	0.830797
-40.543041	-10.070736	0.835802
-40.937906	-17.557414	0.840806
-41.841010	-8.437024	0.845811
-41.369458	-5.840544	0.850816
-41.273509	-12.673303	0.855821
-41.543333	-14.690466	0.860826
-41.937924	-22.291080	0.865830
-42.456869	-17.631662	0.870835
-43.087557	-10.914115	0.875840
-43.093896	-13.143406	0.880845
-43.333383	-15.753781	0.885850
-43.013207	-13.162057	0.890854
-43.095661	-7.992063	0.895859
-43.919889	-8.985888	0.900864
-44.212855	-11.701779	0.905869
-44.831620	-13.154903	0.910874
-44.724526	-17.603938	0.915878
-44.837901	-3.159308	0.920883
-45.635631	-5.853056	0.925888
-45.648944	-12.801572	0.930893
-45.681801	-6.193515	0.935898
-45.764197	-9.505547	0.940902
-46.434417	-8.024140	0.945907
-46.563477	-6.406063	0.950912
-46.281755	-14.672634	0.955917
-46.723516	-0.005706	0.960922
-47.355467	-4.895764	0.965926
-47.486620	-0.591333	0.970931
-47.719225	-6.012199	0.975936
-47.225840	-7.845229	0.980941
-48.265338	-7.593606	0.985946
-48.859393	-9.737137	0.990950
-49.175791	-8.485176	0.995955
-49.566358	-9.512148	1.000960
-49.537623	-8.725553	1.005965
-49.104778	-7.065807	1.010970
-49.159841	-9.686096	1.015974
-49.309080	-14.050674	1.020979
-49.771460	-7.909991	1.025984
-50.172690	-14.642699	1.030989
-50.612307	-8.752355	1.035994
-50.703406	-11.174009	1.040998
-51.787675	-7.808567	1.046003
-52.221761	-10.397942	1.051008
-51.560719	-13.937193	1.056013
-51.728227	-4.501790	1.061018
-51.607247	-14.631935	1.066022
-52.083701	-7.150779	1.071027
-52.554498	-15.274129	1.076032
-53.212068	-11.368107	1.081037
-53.815298	-6.287355	1.086042
-53.527892	-13.067854	1.091046
-53.539156	0.775484	1.096051
-53.505999	-7.069329	1.101056
-53.484750	-18.344941	1.106061
-54.396485	-23.387307	1.111066
-55.039326	-21.248967	1.116070
-55.301078	-15.342201	1.121075
-55.392226	-12.084916	1.126080
-55.342657	-14.778546	1.131085
-55.403095	-9.861939	1.136090
-56.176074	-16.700912	1.141094
-56.592137	-10.045468	1.146099
-56.729218	-16.401949	1.151104
-56.827707	-13.694006	1.156109
-57.475943	-12.978506	1.161114
-56.757263	-8.250417	1.166118
-56.592770	-13.157699	1.171123
-57.330961	-15.114129	1.176128
-57.362528	-17.950070	1.181133
-58.119655	-13.996811	1.186138
-58.882671	-8.343694	1.191142
-59.150387	-15.170088	1.196147
-59.637889	-8.943211	1.201152
-59.367623	-19.650400	1.206157
-59.376751	-13.511135	1.211162
-59.440121	-16.674287	1.216166
-59.578566	-13.004631	1.221171
-59.939367	-6.797605	1.226176
-60.417479	-14.410444	1.231181
-61.161416	-7.422050	1.236186
-60.801383	-14.232911	1.241190
-61.115645	-16.568977	1.246195
-61.475198	-11.567537	1.251200
-60.773643	-15.312452	1.256205
-62.179839	-3.240545	1.261210
-62.294886	-8.815871	1.266214
-62.436631	-11.628221	1.271219
-62.423381	-11.626973	1.276224
-62.527255	-18.738466	1.281229
-63.266636	-15.911119	1.286234
-63.592947	-18.814771	1.291238
-63.739671	-13.596744	1.296243
-64.173972	-6.691668	1.301248
-63.605762	-12.586023	1.306253
-64.895533	-9.988810	1.311258
-64.841769	-10.563385	1.316262
-65.290798	-7.237367	1.321267
-65.651163	-4.026481	1.326272
-65.186880	-8.461883	1.331277
-65.681819	-10.285585	1.336282
-65.569484	-18.588887	1.341286
-66.072909	-7.727785	1.346291
-66.430030	-15.508277	1.351296
-66.721239	-13.516781	1.356301
-66.964113	-15.085750	1.361306
-67.545195	-18.174108	1.366310
-67.677635	-12.341388	1.371315
-68.165497	-22.085062	1.376320
-68.322381	-16.707256	1.381325
-68.768209	-4.747865	1.386330
-68.385292	0.355538	1.391334
-69.238383	-12.849005	1.396339
-68.999257	-13.221672	1.401344
-68.306439	-11.346398	1.406349
-68.828597	-11.919317	1.411354
-69.395856	-13.035662	1.416358
-69.584749	-7.355446	1.421363
-69.956248	-3.313912	1.426368
-70.919553	-11.252522	1.431373
-71.396193	-12.101492	1.436378
-71.855858	-16.863515	1.441382
-71.144999	-14.620911	1.446387
-71.526700	-10.122201	1.451392
-71.153962	-21.142837	1.456397
-71.894062	-5.654050	1.461402
-71.760989	-15.324180	1.466406
-72.402695	-19.845707	1.471411
-73.091347	-23.363297	1.476416
-73.012136	-17.987685	1.481421
-73.134826	-7.619674	1.486426
-73.108848	-18.060796	1.491430
-73.920195	-15.383523	1.496435
-74.377099	-22.436532	1.501440
-74.407656	-15.056885	1.506445
-74.767216	-10.634411	1.511450
-74.582561	-11.058653	1.516454
-74.882078	-8.945633	1.521459
-75.041201	-8.518743	1.526464
-75.020230	-19.670922	1.531469
-75.842756	-1.056087	1.536474
-76.054302	-12.912155	1.541478
-75.999928	-13.211580	1.546483
-76.077399	-7.254594	1.551488
-76.743848	-13.104185	1.556493
-77.561588	-10.482857	1.561498
-77.410302	-16.254935	1.566502
-77.597668	-14.469535	1.571507
-77.808610	-9.940634	1.576512
-77.665312	-12.392687	1.581517
-78.191423	-11.231251	1.586522
-78.929959	-29.923852	1.591526
-78.928802	-15.607914	1.596531
-78.872062	-5.195252	1.601536
-78.950716	-16.176799	1.606541
-79.149389	-8.293081	1.611546
-79.475341	-14.006200	1.616550
-80.238580	-17.822150	1.621555
-80.398492	-14.092183	1.626560
-80.292781	-12.381180	1.631565
-80.902591	-8.558569	1.636570
-80.698924	-16.771779	1.641574
-81.537200	-17.450188	1.646579
-82.024011	-19.354254	1.651584
-82.212363	-17.306110	1.656589
-82.299252	-13.745772	1.661594
-82.212506	-21.301581	1.666598
-81.972746	-21.256732	1.671603
-82.434293	-13.838027	1.676608
-82.828134	-23.628068	1.681613
-83.284405	-13.454564	1.686618
-83.661964	-21.054679	1.691622
-83.648243	-17.494289	1.696627
-83.649791	-12.783063	1.701632
-84.366795	-14.863033	1.706637
-84.812513	-20.854774	1.711642
-85.074954	-13.062307	1.716646
-85.197216	-9.759017	1.721651
-85.237709	-9.961320	1.726656
-85.092651	-14.229641	1.731661
-85.656722	-5.108589	1.736666
-86.233910	-14.585168	1.741670
-86.418855	-14.407332	1.746675
-86.670266	-9.577860	1.751680
-86.296703	-10.936536	1.756685
-86.644502	-3.820388	1.761690
-87.173841	-7.951400	1.766694
-87.736326	-1.991181	1.771699
-87.735768	-6.641822	1.776704
-87.841378	-11.111311	1.781709
-88.278466	-5.173906	1.786714
-88.364772	-12.642491	1.791718
-88.742919	-17.328702	1.796723
-89.231377	-6.893888	1.801728
-89.485539	-18.006119	1.806733
-89.516804	0.446767	1.811738
-89.552445	-4.312098	1.816742
-89.559469	-13.318034	1.821747
-90.710222	-3.753875	1.826752
-90.783888	-19.124323	1.831757
-91.252192	-8.015625	1.836762
-91.062335	-10.294641	1.841766
-91.551497	-6.161905	1.846771
-91.466788	0.000624	1.851776
-91.137241	-11.161946	1.856781
-92.076919	-2.646425	1.861786
-92.234598	-4.222415	1.866790
-92.453750	-8.123621	1.871795
-92.387819	-5.375002	1.876800
-92.904148	-12.542087	1.881805
-93.833996	-15.091740	1.886810
-93.866582	-10.726828	1.891814
-94.173985	-15.734171	1.896819
-94.418740	-3.388672	1.901824
-93.995991	-7.694180	1.906829
-94.300617	-8.601740	1.911834
-93.954581	-3.843737	1.916838
-94.898946	-11.668251	1.921843
-95.881159	-2.133664	1.926848
-95.940709	-17.844846	1.931853
-95.588086	-3.315054	1.936858
-95.670422	-4.558001	1.941862
-95.944238	-7.878003	1.946867
-97.198915	-4.463708	1.951872
-97.280766	-13.325041	1.956877
-97.435756	-8.042443	1.961882
-97.294367	-0.484091	1.966886
-97.143815	-15.114556	1.971891
-97.418172	2.816439	1.976896
-97.455065	-6.728985	1.981901
-98.219118	-12.848016	1.986906
-98.148889	-10.764459	1.991910
-98.291449	-12.535806	1.996915
-99.489044	-12.260375	2.006912
-99.128903	-7.891070	2.016909
-98.600751	-9.642940	2.026906
-97.585397	-12.427827	2.036902
-97.280377	-8.417350	2.046899
-97.113176	-12.922500	2.056896
-96.410321	-5.819231	2.066893
-95.890675	0.004446	2.076890
-94.922035	-6.618834	2.086886
-94.739308	-11.028215	2.096883
-94.538228	-7.467117	2.106880
-93.629030	-9.886912	2.116877
-93.433417	-3.980784	2.126874
-93.029699	-7.702536	2.136870
-91.992730	-10.915295	2.146867
-91.858508	-8.088154	2.156864
-91.488084	-8.145877	2.166861
-90.487074	-3.861152	2.176858
-90.160414	-11.321504	2.186854
-90.344260	-13.063178	2.196851
-89.371126	-14.656691	2.206848
-88.658474	-16.998170	2.216845
-87.996013	-17.323399	2.226842
-87.674125	-15.232085	2.236838
-87.635231	-21.925084	2.246835
-86.798924	-16.179540	2.256832
-86.535161	-18.114895	2.266829
-85.797433	-14.311603	2.276826
-85.035172	-14.677813	2.286822
-84.981701	-22.817613	2.296819
-84.285424	-16.432406	2.306816
-83.415756	-13.368879	2.316813
-83.489316	-11.022364	2.326810
-83.150212	-15.209159	2.336806
-82.168600	-16.075406	2.346803
-81.900425	-23.387207	2.356800
-81.044608	-19.234955	2.366797
-80.701759	-11.787007	2.376794
-80.671082	-11.712299	2.386790
-79.734006	-12.622252	2.396787
-79.313126	-15.168268	2.406784
-78.373120	-12.904544	2.416781
-78.007854	-10.756669	2.426778
-77.668431	-14.275109	2.436774
-77.836697	-18.201837	2.446771
-76.829671	-24.305270	2.456768
-76.177418	-17.881486	2.466765
-75.570464	-16.873877	2.476762
-74.998495	-16.776280	2.486758
-74.747452	-17.299970	2.496755
-74.525292	-14.401078	2.506752
-73.790248	-9.219371	2.516749
-73.676011	-16.662276	2.526746
-72.515006	-16.203980	2.536742
-72.189171	-18.088872	2.546739
-71.760515	-12.957359	2.556736
-70.712216	-8.746565	2.566733
-70.481251	-11.421214	2.576730
-70.545986	-12.985148	2.586726
-70.107436	-13.240446	2.596723
-69.073668	-13.889949	2.606720
-69.060343	-14.550620	2.616717
-67.890920	-15.192870	2.626714
-67.358401	-8.972067	2.636710
-67.348779	-10.816915	2.646707
-67.127514	-17.281901	2.656704
-66.079612	-13.086885	2.666701
-65.732134	-19.140825	2.676698
-65.251971	-12.379629	2.686694
-64.639523	-23.366171	2.696691
-64.621240	-15.037403	2.706688
-63.918973	-12.967675	2.716685
-63.413788	-13.708583	2.726682
-62.340293	-15.333658	2.736678
-61.942806	-5.607114	2.746675
-61.916777	-9.760693	2.756672
-61.309439	-15.446707	2.766669
-60.429739	-13.984488	2.776666
-60.220117	-18.629331	2.786662
-59.844699	-19.533639	2.796659
-58.985630	-16.322729	2.806656
-58.674396	-17.961413	2.816653
-58.582191	-10.325301	2.826650
-57.685236	-21.220209	2.836646
-57.479441	-15.629290	2.846643
-56.435582	-10.762063	2.856640
-55.853946	-19.146183	2.866637
-55.648435	-11.692551	2.876634
-55.630139	-21.863738	2.886630
-54.252351	-13.507235	2.896627
-54.013063	-13.667954	2.906624
-54.075966	-20.196118	2.916621
-53.267214	-12.973224	2.926618
-52.613018	-9.204356	2.936614
-52.583026	-20.853572	2.946611
-51.689633	-18.341789	2.956608
-50.938444	-13.054904	2.966605
-50.450410	-14.442523	2.976602
-49.626152	-12.851240	2.986598
-49.497484	-14.755922	2.996595
-49.239972	-16.550914	3.006592
-49.357151	-18.293531	3.016589
-48.270323	-6.042555	3.026586
-47.980643	-9.654570	3.036582
-46.967028	-17.241566	3.046579
-46.523352	-17.332940	3.056576
-46.193253	-10.903022	3.066573
-45.190332	-7.610112	3.076570
-45.000095	-15.131451	3.086566
-45.103067	-11.779302	3.096563
-44.559305	-14.170343	3.106560
-43.937573	-12.015135	3.116557
-42.807720	-8.624904	3.126554
-42.556886	-16.811473	3.136550
-42.332108	-16.497915	3.146547
-41.603064	-14.758664	3.156544
-41.153383	-17.382052	3.166541
-40.853157	-15.854377	3.176538
-40.187519	-20.922298	3.186534
-39.933462	-17.071727	3.196531
-38.588409	-15.425829	3.206528
-38.672440	-19.454457	3.216525
-38.107454	-16.777173	3.226522
-37.612471	-19.109885	3.236518
-37.240675	-12.683332	3.246515
-36.356445	-19.204680	3.256512
-36.538739	-10.831808	3.266509
-35.934302	-9.484846	3.276506
-34.916544	-16.426260	3.286502
-34.809343	-20.494354	3.296499
-34.082143	-12.431882	3.306496
-33.829537	-12.753077	3.316493
-32.849578	-11.537814	3.326490
-32.290208	-16.500387	3.336486
-32.307516	-21.420118	3.346483
-31.959645	-11.597101	3.356480
-31.015141	-26.037890	3.366477
-30.843611	-19.535610	3.376474
-29.924904	-16.749024	3.386470
-29.165487	-17.865552	3.396467
-29.159233	-13.402780	3.406464
-29.116182	-10.558184	3.416461
-28.371995	-15.799971	3.426458
-27.789419	-12.792823	3.436454
-26.732083	-14.795499	3.446451
-26.423262	-16.018821	3.456448
-26.160990	-12.663713	3.466445
-25.696353	-15.048690	3.476442
-24.606359	-16.169498	3.486438
-24.386216	-20.511881	3.496435
-24.436116	-21.482593	3.506432
-23.860534	-9.404933	3.516429
-23.105381	-19.349456	3.526426
-22.964200	-12.728378	3.536422
-21.930124	-14.784429	3.546419
-21.322439	-17.695500	3.556416
-21.397319	-17.480709	3.566413
-20.028261	-16.320075	3.576410
-19.827190	-16.671208	3.586406
-19.710417	-16.233021	3.596403
-19.671610	-20.366427	3.606400
-18.555262	-19.121848	3.616397
-18.279296	-17.780439	3.626394
-17.184192	-17.866175	3.636390
-16.989775	-21.447423	3.646387
-16.914525	-19.393487	3.656384
-16.255286	-15.584226	3.666381
-15.958263	-8.864019	3.676378
-15.123863	-11.579364	3.686374
-14.293523	-16.052203	3.696371
-14.208515	-14.389436	3.706368
-13.455138	-11.041583	3.716365
-12.773481	-15.085647	3.726362
-12.566602	-16.723817	3.736358
-12.455697	-19.366982	3.746355
-11.481530	-18.816048	3.756352
-11.256816	-10.782545	3.766349
-10.596978	-18.231745	3.776346
-10.041929	-16.145281	3.786342
-9.903817	-15.399993	3.796339
-8.485071	-16.759209	3.806336
-8.410576	-19.422012	3.816333
-8.247146	-17.309033	3.826330
-7.800807	-14.815896	3.836326
-6.568446	-13.180845	3.846323
-6.570419	-18.261371	3.856320
-6.473979	-15.821115	3.866317
-5.867207	-15.519892	3.876314
-5.204967	-10.760757	3.886310
-4.572206	-1.403686	3.896307
-4.295398	0.441274	3.906304
-3.424797	13.739851	3.916301
-3.364005	16.569001	3.926298
-2.973413	18.196563	3.936294
-2.675970	33.786586	3.946291
-2.112846	45.552626	3.956288
-1.618399	65.961733	3.966285
-1.049860	81.303414	3.976282
-0.522979	97.662171	3.986278
-0.379941	116.289059	3.996275
0.000000	131.628252	4.001280
0.534856	138.729550	4.006285
0.406971	140.939082	4.011290
0.732255	159.855141	4.016294
0.977532	161.300685	4.021299
0.929420	164.924587	4.026304
1.102976	163.233404	4.031309
0.873538	178.189920	4.036314
0.989497	171.724117	4.041318
1.222657	169.935008	4.046323
1.034841	184.056097	4.051328
1.394281	174.151073	4.056333
1.218462	182.306547	4.061338
1.236707	172.967516	4.066342
1.287950	183.264098	4.071347
1.030125	170.222402	4.076352
1.617323	180.381222	4.081357
1.357771	180.020248	4.086362
1.687230	175.995073	4.091366
1.332365	178.474294	4.096371
1.231384	176.879909	4.101376
1.423651	172.534541	4.106381
1.489286	176.153279	4.111386
1.573863	179.228042	4.116390
1.283431	178.175874	4.121395
1.596620	178.576220	4.126400
1.485036	172.864248	4.131405
1.315338	173.928719	4.136410
1.501503	171.055467	4.141414
1.272848	181.655333	4.146419
1.212392	180.779105	4.151424
1.688627	179.151229	4.156429
1.407491	179.464360	4.161434
1.337132	181.009980	4.166438
1.789593	198.387536	4.171443
1.559822	188.255282	4.176448
1.830028	183.625614	4.181453
1.403326	187.277201	4.186458
1.079624	179.583130	4.191462
1.601872	192.805188	4.196467
1.401446	195.019765	4.201472
1.818763	205.208381	4.206477
1.777391	207.584703	4.211482
1.755102	203.557686	4.216486
1.765777	201.417451	4.221491
2.140592	204.975096	4.226496
1.528401	204.675702	4.231501
1.625460	214.120391	4.236506
1.895897	200.230265	4.241510
1.956717	195.880177	4.246515
1.500694	191.642708	4.251520
1.937259	192.738740	4.256525
1.582332	193.626587	4.261530
1.886302	193.579120	4.266534
1.758485	201.445504	4.271539
2.016297	194.565157	4.276544
1.835301	189.680313	4.281549
1.301969	192.408964	4.286554
2.156011	191.462217	4.291558
1.627297	200.618963	4.296563
2.127297	206.403285	4.301568
2.147712	203.242784	4.306573
1.631510	195.101135	4.311578
2.025115	201.424151	4.316582
1.837474	215.839469	4.321587
1.809232	206.333697	4.326592
2.017941	207.307241	4.331597
1.752828	207.766560	4.336602
1.619974	204.247254	4.341606
1.558559	206.360958	4.346611
1.749764	202.639016	4.351616
1.706462	203.294538	4.356621
1.635435	204.672584	4.361626
2.253665	198.912694	4.366630
2.108680	201.197680	4.371635
1.709115	214.099109	4.376640
2.244934	203.615933	4.381645
1.636274	210.203559	4.386650
2.254647	214.457044	4.391654
2.519325	220.458578	4.396659
2.097323	219.427022	4.401664
2.222839	206.081624	4.406669
1.940540	210.653401	4.411674
2.239458	202.039180	4.416678
2.313093	205.109335	4.421683
2.374801	207.782721	4.426688
2.438932	206.039075	4.431693
1.730293	212.993547	4.436698
2.180867	207.104898	4.441702
2.101121	213.903885	4.446707
2.029568	218.480609	4.451712
2.350845	215.798155	4.456717
2.218239	231.097052	4.461722
2.236621	225.779157	4.466726
2.273715	236.258322	4.471731
2.706705	234.637216	4.476736
2.432476	230.792038	4.481741
2.482448	227.104875	4.486746
2.296147	217.592224	4.491750
1.878784	216.942761	4.496755
2.320384	227.716050	4.501760
2.403769	226.307912	4.506765
2.244353	229.341818	4.511770
2.577923	230.188231	4.516774
2.353849	233.124700	4.521779
2.364859	234.179843	4.526784
2.570863	230.047447	4.531789
2.468160	238.764136	4.536794
2.813973	232.724212	4.541798
2.791450	238.606233	4.546803
2.714068	235.312351	4.551808
2.341872	224.591779	4.556813
2.378357	230.496190	4.561818
2.598341	229.737373	4.566822
2.240397	237.083002	4.571827
2.373992	236.767997	4.576832
2.468158	235.475229	4.581837
2.057339	240.193702	4.586842
2.362384	235.852795	4.591846
2.098843	241.535296	4.596851
2.103543	244.265077	4.601856
2.996433	257.482894	4.606861
2.214654	251.901215	4.611866
2.988327	243.228408	4.616870
2.476294	257.004878	4.621875
2.778897	265.060118	4.626880
3.203319	259.972827	4.631885
2.276575	247.725591	4.636890
2.438623	258.106095	4.641894
2.336617	265.000340	4.646899
2.641184	271.916307	4.651904
2.704283	261.292027	4.656909
2.740630	270.477335	4.661914
3.242563	268.323397	4.666918
3.165765	272.230230	4.671923
3.339991	270.918588	4.676928
3.138132	248.740499	4.681933
2.399516	251.260874	4.686938
2.740450	240.384263	4.691942
2.996513	253.312710	4.696947
2.969763	252.412215	4.701952
3.085612	246.813283	4.706957
2.835327	244.226707	4.711962
2.830290	237.457131	4.716966
2.966265	246.547721	4.721971
2.952972	246.417084	4.726976
3.196182	243.417823	4.731981
3.115137	247.663843	4.736986
2.919021	240.395850	4.741990
2.858725	243.490160	4.746995
3.059993	245.398192	4.752000
3.023852	249.330288	4.757005
2.833607	253.283367	4.762010
3.171397	243.115938	4.767014
2.919986	242.136747	4.772019
2.800534	249.584220	4.777024
3.404314	268.437777	4.782029
3.264637	257.744029	4.787034
2.966443	250.321181	4.792038
3.206227	255.032633	4.797043
3.050525	252.782417	4.802048
3.223318	256.055346	4.807053
2.782151	257.510374	4.812058
3.406083	259.238287	4.817062
3.175404	261.005189	4.822067
3.054945	270.680144	4.827072
3.614856	268.893614	4.832077
3.407866	264.272254	4.837082
3.156239	251.492123	4.842086
2.793746	247.546874	4.847091
2.831787	257.206480	4.852096
3.129675	262.029054	4.857101
3.210697	275.007089	4.862106
3.385502	263.954011	4.867110
3.524873	266.681677	4.872115
3.322276	264.005367	4.877120
3.391562	261.824303	4.882125
3.108703	275.666122	4.887130
3.125129	266.532975	4.892134
3.446431	268.096332	4.897139
3.408621	270.215836	4.902144
3.582106	272.748330	4.907149
2.972999	274.640966	4.912154
3.225313	267.384960	4.917158
2.979329	265.209001	4.922163
3.177689	274.005088	4.927168
3.720419	272.885648	4.932173
3.325817	271.992167	4.937178
3.286061	267.271836	4.942182
3.620693	272.006398	4.947187
3.321288	272.369850	4.952192
3.514434	260.690630	4.957197
3.120432	277.697846	4.962202
3.818358	281.454822	4.967206
3.859257	280.676605	4.972211
3.876173	282.581889	4.977216
3.967857	277.885254	4.982221
3.481314	277.376343	4.987226
3.603143	273.124246	4.992230
3.400893	275.332791	4.997235
3.111468	270.974286	5.002240
3.796660	268.437289	5.007245
3.613276	273.904758	5.012250
3.680252	279.348821	5.017254
3.900085	288.122568	5.022259
3.655512	278.615851	5.027264
3.485155	269.192424	5.032269
3.559706	284.379814	5.037274
4.170082	294.338912	5.042278
3.560605	292.033238	5.047283
3.674456	281.631951	5.052288
4.212958	281.674290	5.057293
3.635236	276.165036	5.062298
3.345725	283.351263	5.067302
3.535165	282.302996	5.072307
4.238358	292.054558	5.077312
4.224401	287.671870	5.082317
3.820367	281.173605	5.087322
3.808912	279.729701	5.092326
3.761811	267.594567	5.097331
3.752596	281.842775	5.102336
3.763520	291.440207	5.107341
3.549767	290.901210	5.112346
3.912181	289.433529	5.117350
4.113542	294.590781	5.122355
4.084149	293.181325	5.127360
3.807575	282.863357	5.132365
3.669716	294.072332	5.137370
3.812046	288.307884	5.142374
3.327609	289.168571	5.147379
3.794477	293.407848	5.152384
4.003429	285.098754	5.157389
3.881713	292.565583	5.162394
4.006965	288.550231	5.167398
4.054697	293.851779	5.172403
3.976383	288.770482	5.177408
3.707417	282.981892	5.182413
4.021449	300.159771	5.187418
4.159862	302.871774	5.192422
4.398709	310.320082	5.197427
4.126147	307.426933	5.202432
4.338329	292.875136	5.207437
4.129506	302.219098	5.212442
4.408557	297.290617	5.217446
4.085127	289.042790	5.222451
3.915133	292.625703	5.227456
4.478060	304.341826	5.232461
4.376911	298.789533	5.237466
4.033658	301.213166	5.242470
4.591824	294.981758	5.247475
4.011341	298.211366	5.252480
4.329737	291.210757	5.257485
3.918521	308.302958	5.262490
4.439833	300.878238	5.267494
4.505436	310.356381	5.272499
4.196174	308.753488	5.277504
4.527954	302.026029	5.282509
3.825062	306.701695	5.287514
3.919643	319.174592	5.292518
4.170893	318.768384	5.297523
4.186489	317.304420	5.302528
4.425184	319.260381	5.307533
4.487686	324.638718	5.312538
4.932093	324.442695	5.317542
4.788553	328.771294	5.322547
4.377057	315.304307	5.327552
4.772959	321.335935	5.332557
4.418759	321.831362	5.337562
4.157629	320.113358	5.342566
4.155412	322.296895	5.347571
4.374755	315.957213	5.352576
4.560953	317.317112	5.357581
4.299839	315.137189	5.362586
4.700710	312.303042	5.367590
4.524997	317.022663	5.372595
4.276645	318.719572	5.377600
4.866115	311.904277	5.382605
4.400513	331.963184	5.387610
4.771055	328.194134	5.392614
4.434261	332.293580	5.397619
4.577022	321.160064	5.402624
4.714370	313.985329	5.407629
4.624426	319.931726	5.412634
4.327313	328.584006	5.417638
4.565151	317.660226	5.422643
4.580291	320.328270	5.427648
4.539318	316.538277	5.432653
4.518960	324.530249	5.437658
4.547507	320.985631	5.442662
4.757637	334.361104	5.447667
4.533482	348.614568	5.452672
4.788371	346.511984	5.457677
4.647825	344.423900	5.462682
5.022818	345.488460	5.467686
5.407413	348.383364	5.472691
5.047803	333.297852	5.477696
4.424076	327.080769	5.482701
4.880021	327.629598	5.487706
5.063481	328.673545	5.492710
4.582584	319.229145	5.497715
4.647297	332.418588	5.502720
4.635057	335.761653	5.507725
5.009775	350.038347	5.512730
5.163641	342.879995	5.517734
5.356356	336.357812	5.522739
5.124167	339.637262	5.527744
4.918234	320.237551	5.532749
4.318361	330.696348	5.537754
4.683809	329.816657	5.542758
4.742810	338.979468	5.547763
4.626459	344.085272	5.552768
4.772645	335.545539	5.557773
4.923262	343.039323	5.562778
4.995876	341.715122	5.567782
5.350505	347.452664	5.572787
4.848979	350.935670	5.577792
5.129636	339.578053	5.582797
4.992315	354.431696	5.587802
4.965714	343.789783	5.592806
5.042902	345.764725	5.597811
4.790659	350.951936	5.602816
5.014177	355.362237	5.607821
5.220474	362.024712	5.612826
5.643705	361.904774	5.617830
5.113102	350.784993	5.622835
5.085180	354.804412	5.627840
5.210038	341.275515	5.632845
4.969110	349.371662	5.637850
5.311322	355.263015	5.642854
5.582818	355.359844	5.647859
5.082622	360.044894	5.652864
5.374113	351.700690	5.657869
5.174863	347.049622	5.662874
5.132291	349.891231	5.667878
5.065546	365.024896	5.672883
5.136503	373.666985	5.677888
5.662978	373.091100	5.682893
5.170210	375.152183	5.687898
5.326202	372.755037	5.692902
5.796870	369.834014	5.697907
5.401373	372.866968	5.702912
5.839730	372.757315	5.707917
5.626750	361.869342	5.712922
5.678146	357.267585	5.717926
5.505389	347.059867	5.722931
5.117280	356.995108	5.727936
5.178297	344.311460	5.732941
5.211789	353.411834	5.737946
5.237368	356.448415	5.742950
5.736821	360.125771	5.747955
5.393992	381.870795	5.752960
5.540661	369.148399	5.757965
5.347815	369.501484	5.762970
5.779219	376.214117	5.767974
5.941767	374.012100	5.772979
5.445648	369.682792	5.777984
5.597419	361.993239	5.782989
5.430104	374.380657	5.787994
5.751615	381.113674	5.792998
5.840099	374.661594	5.798003
5.642533	374.151696	5.803008
5.684237	365.327756	5.808013
5.699363	368.451400	5.813018
5.952244	366.077039	5.818022
6.051562	349.761649	5.823027
5.405503	351.071613	5.828032
5.505761	343.178164	5.833037
5.413585	360.669688	5.838042
5.377278	366.863966	5.843046
5.538706	361.751413	5.848051
5.528151	370.738473	5.853056
5.507891	380.249088	5.858061
5.756950	381.440952	5.863066
5.799624	376.470390	5.868070
6.190572	374.387614	5.873075
6.088687	378.674896	5.878080
6.350155	368.139696	5.883085
5.804539	376.742349	5.888090
5.463145	378.877793	5.893094
5.910427	367.785122	5.898099
5.516977	374.022705	5.903104
5.910975	363.906514	5.908109
5.433300	367.759117	5.913114
5.500574	373.896039	5.918118
5.533363	368.091779	5.923123
5.587628	373.205661	5.928128
5.806455	379.704825	5.933133
5.955915	393.162616	5.938138
5.912242	400.566640	5.943142
6.257180	402.512292	5.948147
5.939612	400.132391	5.953152
6.047506	395.208554	5.958157
5.974738	397.276602	5.963162
5.944232	404.102749	5.968166
5.983920	403.172853	5.973171
5.643331	403.912928	5.978176
6.081230	399.139868	5.983181
6.081193	402.759450	5.988186
5.968976	399.809524	5.993190
6.292878	404.336990	5.998195
6.194957	406.921519	6.003200
6.374489	390.710586	6.008205
5.599146	388.541620	6.013210
6.085275	395.903762	6.018214
6.233980	401.214831	6.023219
5.969939	400.591958	6.028224
6.304450	398.926156	6.033229
5.803882	397.913227	6.038234
5.949119	390.199374	6.043238
5.728258	394.214229	6.048243
6.307352	395.281615	6.053248
6.520626	389.923644	6.058253
6.195823	399.652833	6.063258
5.873477	405.328780	6.068262
6.308216	407.304656	6.073267
6.319015	401.269708	6.078272
6.246821	397.468771	6.083277
6.429518	400.468086	6.088282
5.782591	400.079215	6.093286
6.164415	401.221803	6.098291
5.842119	400.142976	6.103296
6.260510	397.688894	6.108301
6.266166	401.725208	6.113306
5.592691	399.062543	6.118310
5.897240	397.869681	6.123315
6.197723	408.886659	6.128320
6.029418	408.444943	6.133325
5.836827	406.782631	6.138330
6.276331	414.253328	6.143334
6.378977	405.875411	6.148339
6.147126	408.047481	6.153344
5.889652	388.282440	6.158349
5.786842	404.937261	6.163354
5.915937	412.981788	6.168358
6.353948	410.989713	6.173363
6.294145	418.677853	6.178368
6.330637	416.843602	6.183373
6.149994	414.034112	6.188378
6.089311	411.034981	6.193382
6.077885	408.028132	6.198387
5.942986	418.679888	6.203392
6.253386	417.160234	6.208397
6.237024	422.095366	6.213402
6.336197	412.724548	6.218406
6.024738	404.778518	6.223411
5.792093	405.106202	6.228416
6.180170	415.419745	6.233421
6.722694	410.649273	6.238426
6.366415	402.634335	6.243430
6.396349	396.102834	6.248435
6.259911	391.375472	6.253440
6.166390	394.386426	6.258445
6.217131	392.597403	6.263450
5.943537	400.350670	6.268454
6.111621	396.091297	6.273459
6.043811	395.969201	6.278464
6.085566	395.842593	6.283469
5.990352	399.878893	6.288474
5.886649	399.218243	6.293478
6.066115	398.162040	6.298483
5.881141	399.295358	6.303488
5.978455	400.080718	6.308493
6.017745	405.525993	6.313498
6.367437	414.488269	6.318502
6.390641	422.704419	6.323507
6.098715	419.260616	6.328512
6.179477	406.792134	6.333517
6.243394	401.400612	6.338522
6.155277	399.184081	6.343526
6.135397	398.279339	6.348531
6.057621	403.496177	6.353536
6.446413	396.497152	6.358541
5.907434	404.700136	6.363546
5.592321	403.851142	6.368550
5.858767	413.620581	6.373555
6.422138	426.175129	6.378560
6.462797	418.366916	6.383565
6.376503	420.016297	6.388570
6.060080	411.697710	6.393574
6.155187	398.654333	6.398579
6.093269	409.712274	6.403584
5.783242	397.403107	6.408589
6.023837	410.156917	6.413594
6.355277	428.581905	6.418598
6.371405	423.906561	6.423603
6.059065	427.382087	6.428608
6.174213	407.950956	6.433613
6.015711	403.356764	6.438618
6.103943	396.765507	6.443622
6.196338	402.879520	6.448627
6.256884	407.878530	6.453632
6.122264	413.680094	6.458637
5.931007	413.001524	6.463642
6.022942	414.240155	6.468646
6.380847	418.581958	6.473651
6.073045	410.619534	6.478656
6.118917	406.550153	6.483661
6.152720	413.527583	6.488666
6.178076	419.800805	6.493670
5.977654	409.765068	6.498675
6.134790	417.099670	6.503680
6.298400	414.919628	6.508685
6.228546	414.165087	6.513690
6.149518	402.569550	6.518694
6.168050	389.224959	6.523699
5.916522	391.906321	6.528704
6.336802	402.626109	6.533709
6.130968	400.839320	6.538714
5.852870	397.855272	6.543718
6.246919	405.238173	6.548723
5.882996	406.288795	6.553728
6.351995	410.353756	6.558733
6.188541	406.219094	6.563738
6.082682	412.016152	6.568742
6.459693	393.597561	6.573747
6.108052	403.777057	6.578752
6.141106	391.221146	6.583757
6.161718	394.318623	6.588762
6.288183	400.756335	6.593766
6.011925	398.170641	6.598771
6.043012	400.921622	6.603776
6.417339	402.679167	6.608781
6.161190	402.368276	6.613786
5.931365	394.909345	6.618790
6.422128	394.506737	6.623795
6.382733	394.857926	6.628800
6.446552	395.243565	6.633805
6.148812	394.198857	6.638810
6.242476	395.415069	6.643814
6.040551	388.600352	6.648819
6.280757	387.752938	6.653824
6.228858	397.660834	6.658829
6.126331	399.796821	6.663834
6.046429	401.755252	6.668838
6.338858	393.252691	6.673843
6.322809	398.421891	6.678848
5.918690	400.883548	6.683853
6.184792	399.108239	6.688858
5.890684	400.888256	6.693862
6.100677	393.505950	6.698867
5.913040	396.746791	6.703872
6.371275	396.801706	6.708877
6.209644	399.750565	6.713882
6.108559	392.780839	6.718886
5.941265	399.115877	6.723891
6.024396	396.932628	6.728896
6.426786	390.852147	6.733901
6.263740	396.847990	6.738906
6.358180	401.019093	6.743910
6.454597	396.729819	6.748915
6.155165	404.863632	6.753920
6.328001	394.535297	6.758925
6.134028	395.638386	6.763930
6.119868	398.314196	6.768934
6.315055	391.143023	6.773939
5.946431	401.166986	6.778944
5.966878	399.657962	6.783949
5.976386	394.917223	6.788954
6.022478	397.061562	6.793958
6.230405	400.465057	6.798963
6.102036	393.765367	6.803968
6.307165	393.964346	6.808973
5.922114	397.995436	6.813978
6.178329	402.688534	6.818982
6.201247	396.667508	6.823987
5.982468	405.962464	6.828992
6.298632	397.636519	6.833997
6.285284	395.683527	6.839002
6.085308	397.847438	6.844006
6.263267	390.577721	6.849011
6.158728	408.757780	6.854016
6.467856	400.768302	6.859021
6.436428	407.721148	6.864026
6.053120	393.243589	6.869030
6.443524	392.249252	6.874035
5.853549	384.191842	6.879040
5.760612	380.027155	6.884045
5.942457	393.315353	6.889050
5.924230	395.754513	6.894054
5.975589	395.949111	6.899059
6.011718	410.079583	6.904064
6.462202	417.694097	6.909069
6.629669	412.093354	6.914074
6.172635	404.492843	6.919078
6.415514	404.739693	6.924083
5.949484	401.180800	6.929088
6.199674	393.456830	6.934093
6.231683	397.583929	6.939098
5.863499	386.982855	6.944102
5.836668	391.394425	6.949107
5.758710	404.701191	6.954112
5.933997	410.501654	6.959117
5.830527	394.781158	6.964122
6.183607	400.613874	6.969126
6.333997	403.627743	6.974131
5.981749	407.941604	6.979136
6.441215	398.451065	6.984141
6.119910	403.759846	6.989146
5.752509	416.488697	6.994150
5.960863	407.663936	6.999155
6.219954	409.822361	7.004160
6.092908	407.773284	7.009165
6.089335	409.235692	7.014170
6.101915	401.355954	7.019174
6.073249	407.935036	7.024179
6.269851	409.521107	7.029184
6.362826	404.605933	7.034189
5.920995	409.737442	7.039194
6.086964	406.702798	7.044198
6.417877	406.435970	7.049203
5.846047	406.516234	7.054208
6.276647	406.898190	7.059213
6.096361	405.952139	7.064218
6.139633	409.229571	7.069222
5.937656	404.664338	7.074227
6.090963	406.994364	7.079232
6.230592	397.620379	7.084237
5.971679	412.281145	7.089242
6.057297	405.123970	7.094246
6.161102	404.085950	7.099251
5.705830	406.697995	7.104256
5.942826	402.826465	7.109261
5.982897	412.935100	7.114266
5.999765	412.575105	7.119270
6.447473	416.728827	7.124275
6.047501	414.975618	7.129280
6.370250	410.220598	7.134285
6.187666	405.070182	7.139290
6.025572	405.298224	7.144294
6.037796	400.705758	7.149299
6.388933	403.558456	7.154304
6.186926	406.779404	7.159309
6.141029	402.107457	7.164314
6.140403	401.968506	7.169318
6.050343	405.570556	7.174323
5.997869	413.836525	7.179328
6.132182	403.935010	7.184333
5.978681	402.858210	7.189338
6.042923	413.127576	7.194342
6.258345	398.322080	7.199347
6.149633	408.536283	7.204352
6.381976	407.535072	7.209357
6.154587	404.432344	7.214362
6.141855	413.695020	7.219366
6.473451	406.268344	7.224371
6.059714	411.658050	7.229376
6.418768	409.621397	7.234381
6.526246	408.535344	7.239386
6.306911	404.776442	7.244390
6.352626	402.092843	7.249395
6.238882	416.148723	7.254400
6.142849	401.221177	7.259405
5.882548	406.425485	7.264410
5.884667	396.503557	7.269414
6.344582	399.206331	7.274419
6.118537	410.584224	7.279424
6.244386	402.158379	7.284429
6.220426	407.910965	7.289434
5.975232	405.649441	7.294438
6.529410	406.973838	7.299443
6.330318	407.153892	7.304448
6.488212	400.311268	7.309453
6.188750	413.655910	7.314458
6.181317	406.313993	7.319462
6.184188	396.819064	7.324467
5.772461	392.394268	7.329472
5.939012	398.926940	7.334477
6.555237	408.359991	7.339482
6.130304	400.298862	7.344486
6.192405	410.128791	7.349491
6.015530	409.014522	7.354496
6.075884	403.879828	7.359501
6.348931	405.384317	7.364506
5.959394	402.721457	7.369510
6.390892	406.887207	7.374515
6.084011	406.527317	7.379520
5.931977	397.581853	7.384525
6.176806	400.792901	7.389530
5.920971	404.148835	7.394534
6.152642	400.411020	7.399539
6.450122	406.274596	7.404544
6.682938	406.257261	7.409549
6.194260	391.979715	7.414554
5.899772	385.935657	7.419558
6.128365	385.564635	7.424563
6.049558	376.746916	7.429568
5.968867	375.560631	7.434573
6.260358	379.235773	7.439578
5.954919	386.509960	7.444582
5.975524	387.905301	7.449587
6.237789	405.822236	7.454592
6.379149	396.419506	7.459597
6.081473	384.089430	7.464602
5.975673	395.992651	7.469606
6.254275	387.887736	7.474611
5.957143	390.136472	7.479616
6.421240	391.342101	7.484621
6.324380	381.502130	7.489626
6.112297	376.761313	7.494630
5.861142	377.408278	7.499635
5.948947	380.685055	7.504640
6.236681	384.148811	7.509645
5.828368	386.845247	7.514650
6.010656	393.666523	7.519654
6.751100	394.604222	7.524659
6.306625	393.433804	7.529664
6.379931	379.995215	7.534669
6.494279	378.904923	7.539674
6.056930	375.502896	7.544678
6.245579	369.601448	7.549683
6.334882	379.110716	7.554688
6.328705	374.407242	7.559693
5.944808	376.773977	7.564698
6.105211	381.437788	7.569702
6.240663	366.252534	7.574707
6.068287	372.022035	7.579712
6.034443	375.222956	7.584717
6.039048	374.706692	7.589722
5.749452	378.839883	7.594726
6.216060	370.515690	7.599731
6.298636	383.392318	7.604736
6.102191	376.991208	7.609741
6.181299	371.907369	7.614746
5.792318	375.002580	7.619750
5.713376	375.897814	7.624755
5.588029	383.542424	7.629760
6.069164	393.594596	7.634765
6.196788	395.567968	7.639770
6.119094	396.972384	7.644774
6.185767	395.513066	7.649779
6.229230	394.114334	7.654784
6.249049	393.004050	7.659789
6.315779	389.928010	7.664794
5.774618	401.855155	7.669798
6.189814	390.764333	7.674803
6.120887	399.529594	7.679808
6.420085	405.820017	7.684813
6.773521	390.126015	7.689818
6.307791	382.102925	7.694822
6.117075	372.616193	7.699827
5.769160	377.277388	7.704832
5.749056	375.961384	7.709837
5.837619	373.214127	7.714842
5.849593	394.232845	7.719846
5.983629	388.532941	7.724851
6.128264	391.680590	7.729856
6.346575	390.412654	7.734861
5.969244	395.100609	7.739866
6.045928	393.791586	7.744870
6.281924	402.651445	7.749875
6.233671	400.545730	7.754880
6.441407	397.033134	7.759885
6.420601	399.697331	7.764890
6.012998	400.973100	7.769894
6.473285	390.912948	7.774899
6.034866	381.066380	7.779904
6.136334	374.615430	7.784909
6.173051	372.331887	7.789914
6.304585	381.508665	7.794918
5.958833	373.257968	7.799923
5.843497	384.488782	7.804928
6.105303	389.158853	7.809933
6.638448	390.483380	7.814938
6.040428	397.657878	7.819942
6.345850	375.188172	7.824947
6.055774	376.201911	7.829952
6.140398	380.260650	7.834957
5.791311	377.395299	7.839962
5.965820	381.101426	7.844966
6.467643	393.776329	7.849971
6.525776	389.651246	7.854976
6.084753	379.646896	7.859981
6.184813	377.084502	7.864986
6.503446	379.701839	7.869990
6.490138	377.027492	7.874995
6.304865	372.105302	7.880000
6.639919	376.861972	7.885005
6.623885	377.921360	7.890010
6.136776	373.384991	7.895014
6.209488	370.576942	7.900019
6.155043	369.908575	7.905024
6.200050	371.217832	7.910029
6.208352	369.748679	7.915034
5.952469	384.573467	7.920038
6.115416	372.775517	7.925043
6.185961	373.871961	7.930048
6.179485	373.414382	7.935053
6.287432	369.028393	7.940058
6.040255	365.368777	7.945062
5.945127	371.809559	7.950067
5.696442	369.235368	7.955072
6.307142	373.834951	7.960077
6.094703	369.160632	7.965082
5.958702	374.076531	7.970086
5.943335	372.085892	7.975091
5.934435	377.978480	7.980096
6.210065	379.466744	7.985101
6.215091	375.963766	7.990106
5.958285	373.748359	7.995110
6.063420	372.197594	8.000115
5.703090	378.476438	8.005133
5.865180	372.095522	8.010150
6.172266	374.562699	8.015168
6.181751	379.689467	8.020186
6.380895	377.979566	8.025203
5.902077	374.138463	8.030221
6.135206	375.313905	8.035238
6.105454	373.286424	8.040256
6.013637	369.731818	8.045274
6.223044	369.544537	8.050291
6.258137	379.754360	8.055309
6.092252	378.126898	8.060326
6.107006	375.284572	8.065344
6.088081	386.926107	8.070362
6.060284	383.771715	8.075379
5.730060	383.725788	8.080397
6.490417	392.654354	8.085414
6.380343	395.000707	8.090432
6.053787	387.831671	8.095450
6.365378	393.277176	8.100467
6.285480	397.780492	8.105485
6.484447	385.934340	8.110502
6.204152	384.712961	8.115520
5.967252	385.327742	8.120538
6.325811	387.603823	8.125555
6.243419	389.816452	8.130573
6.051509	401.062228	8.135590
6.043117	411.547122	8.140608
6.283491	404.440728	8.145626
6.235015	406.038984	8.150643
6.362863	403.065327	8.155661
5.878127	392.437120	8.160678
6.147909	398.012251	8.165696
6.282707	394.412667	8.170714
6.812633	390.684903	8.175731
6.663434	397.427038	8.180749
6.129843	401.020001	8.185766
6.308454	396.062889	8.190784
6.280211	404.505961	8.195802
6.463011	394.167632	8.200819
6.568951	394.122792	8.205837
6.275694	408.123646	8.210854
6.367951	400.122136	8.215872
6.380811	408.347334	8.220890
6.630204	405.679675	8.225907
6.517648	398.221489	8.230925
6.401502	402.222409	8.235942
6.558442	383.664243	8.240960
6.177478	383.200239	8.245978
6.367288	378.534862	8.250995
6.177453	389.272230	8.256013
6.173971	397.212810	8.261030
6.443028	399.102136	8.266048
6.181110	406.082838	8.271066
6.372208	402.909925	8.276083
6.566519	405.514696	8.281101
6.242812	405.919020	8.286118
6.269990	405.842340	8.291136
5.986150	412.996890	8.296154
6.429355	405.675682	8.301171
6.388221	400.510005	8.306189
6.156438	400.953574	8.311206
6.661526	407.725740	8.316224
6.207330	410.084988	8.321242
6.353873	403.116370	8.326259
6.371473	413.205879	8.331277
6.274091	402.797837	8.336294
6.353519	399.692914	8.341312
6.157496	409.746465	8.346330
6.592333	418.732360	8.351347
6.698069	418.883208	8.356365
6.498179	416.762462	8.361382
6.450285	407.135603	8.366400
6.562089	412.060159	8.371418
6.367353	406.694489	8.376435
6.481932	409.923969	8.381453
6.392817	422.371774	8.386470
6.580030	428.253338	8.391488
6.647025	431.389293	8.396506
6.482516	437.496379	8.401523
6.501509	424.892616	8.406541
6.391199	436.273949	8.411558
6.992818	437.511578	8.416576
6.646970	426.539702	8.421594
6.911042	421.487143	8.426611
6.571240	404.417410	8.431629
6.369919	416.504102	8.436646
6.485047	407.716377	8.441664
6.471179	417.378480	8.446682
6.653269	424.942864	8.451699
6.823303	415.947720	8.456717
6.545957	427.453048	8.461734
6.693015	408.965831	8.466752
6.869270	414.072791	8.471770
6.525640	407.868928	8.476787
6.729270	406.177256	8.481805
6.230354	410.206593	8.486822
6.637923	407.583577	8.491840
6.771019	429.006254	8.496858
6.642733	418.113903	8.501875
6.347214	408.595269	8.506893
6.578000	428.800296	8.511910
6.980509	420.027498	8.516928
6.773887	429.442102	8.521946
6.558302	427.885538	8.526963
6.799663	426.083812	8.531981
6.738299	434.835041	8.536998
6.647617	411.455775	8.542016
6.490976	424.090884	8.547034
6.811781	435.085937	8.552051
6.981092	429.035224	8.557069
6.679095	421.982245	8.562087
6.766317	415.275378	8.567104
6.670874	420.683682	8.572122
6.768587	423.180516	8.577139
6.851910	418.490788	8.582157
6.779115	420.348473	8.587175
6.681966	411.186914	8.592192
6.604376	421.991920	8.597210
6.505931	424.841376	8.602227
7.018902	422.915044	8.607245
6.780095	432.479858	8.612263
7.006483	429.370837	8.617280
7.016592	426.614436	8.622298
6.946618	422.614591	8.627315
6.755458	415.449576	8.632333
6.393723	417.841674	8.637351
6.965192	422.435440	8.642368
6.836997	421.849781	8.647386
6.741383	435.093864	8.652403
7.108525	425.342007	8.657421
6.869813	415.236965	8.662439
6.585092	409.380472	8.667456
7.054942	417.915918	8.672474
6.773785	410.070740	8.677491
6.933140	409.588348	8.682509
6.720280	406.219955	8.687527
6.963512	409.025341	8.692544
7.010013	413.546725	8.697562
6.945054	414.715226	8.702579
6.670169	399.677102	8.707597
6.579171	413.965001	8.712615
7.059973	419.219902	8.717632
7.267034	410.881668	8.722650
6.604302	418.868747	8.727667
6.790099	419.448857	8.732685
6.950503	423.504280	8.737703
6.956720	423.393015	8.742720
7.120838	424.304721	8.747738
7.249889	426.847138	8.752755
7.305596	414.026194	8.757773
6.782647	408.320634	8.762791
6.902229	396.834046	8.767808
6.942938	405.017011	8.772826
6.680919	406.847538	8.777843
7.036370	400.783448	8.782861
6.666874	417.626967	8.787879
6.967613	422.727047	8.792896
7.022389	426.540249	8.797914
7.134601	427.867181	8.802931
7.410937	421.408388	8.807949
6.885971	416.952822	8.812967
7.012592	405.304182	8.817984
6.861428	413.621353	8.823002
6.866944	436.105428	8.828019
7.226972	422.813924	8.833037
7.072477	432.441266	8.838055
7.268495	421.785274	8.843072
7.183909	406.335480	8.848090
6.934471	407.835838	8.853107
7.284153	398.967186	8.858125
6.850274	400.935092	8.863143
7.019619	404.020293	8.868160
7.032633	407.227817	8.873178
6.703024	411.085463	8.878195
7.195140	422.826828	8.883213
7.375492	430.445134	8.888231
7.134739	416.070668	8.893248
7.330701	422.010818	8.898266
7.142961	417.208929	8.903283
6.760793	406.305872	8.908301
6.886868	417.154702	8.913319
7.276048	416.203962	8.918336
7.157409	413.843270	8.923354
7.287157	429.977426	8.928371
7.126275	420.911054	8.933389
7.070059	427.285187	8.938407
7.154652	430.118588	8.943424
7.291558	427.440148	8.948442
7.155806	435.972662	8.953459
7.349612	425.673615	8.958477
6.972056	430.163618	8.963495
7.168381	432.379918	8.968512
6.953944	421.889221	8.973530
6.962859	431.582476	8.978547
7.368536	434.457086	8.983565
6.994336	438.015616	8.988583
7.070191	437.988112	8.993600
7.364878	432.716161	8.998618
7.170010	433.608376	9.003635
7.493853	422.689363	9.008653
7.081113	435.465590	9.013671
7.154083	425.153919	9.018688
7.444427	423.003696	9.023706
7.423272	431.398334	9.028723
7.308647	422.936930	9.033741
7.173915	433.283844	9.038759
7.054297	430.314243	9.043776
7.093001	423.883214	9.048794
7.046263	430.782875	9.053811
7.398888	425.448200	9.058829
7.274069	427.743219	9.063847
7.268145	428.580584	9.068864
7.518714	430.627442	9.073882
7.032088	427.841574	9.078899
7.302204	432.753955	9.083917
7.418517	429.946199	9.088935
7.317395	424.449093	9.093952
7.492016	425.759935	9.098970
7.601959	425.632418	9.103987
7.571333	427.278371	9.109005
7.436982	429.584352	9.114023
7.279565	430.499101	9.119040
7.408392	429.636489	9.124058
7.258967	432.976764	9.129075
7.222210	429.975245	9.134093
7.460875	418.583593	9.139111
7.233747	432.189102	9.144128
7.103230	421.047793	9.149146
6.870862	429.295645	9.154163
7.450913	428.930371	9.159181
7.311867	443.623448	9.164199
7.757360	441.363709	9.169216
7.881309	446.617726	9.174234
7.190556	446.208571	9.179251
7.262530	432.750756	9.184269
7.570875	426.709818	9.189287
7.464386	426.594121	9.194304
7.402351	421.059334	9.199322
7.418068	435.557745	9.204339
7.532166	444.029025	9.209357
7.251973	449.453662	9.214375
7.682869	454.552293	9.219392
7.978368	454.938493	9.224410
7.721673	444.833096	9.229427
7.303536	436.078418	9.234445
7.387827	436.734393	9.239463
7.056319	432.614580	9.244480
7.502058	441.207464	9.249498
7.571693	455.334530	9.254515
7.683865	450.318386	9.259533
7.882237	455.292506	9.264551
7.785641	451.019118	9.269568
7.718437	439.123118	9.274586
7.328184	438.821512	9.279603
6.865655	433.655580	9.284621
7.708439	457.984004	9.289639
7.728932	458.220791	9.294656
7.608368	454.787436	9.299674
7.394504	450.857466	9.304691
7.430260	449.895828	9.309709
7.566604	456.047299	9.314727
7.569311	453.752795	9.319744
7.643848	464.496123	9.324762
7.598474	459.889664	9.329779
7.914019	463.639925	9.334797
7.782330	454.840357	9.339815
7.632924	452.790590	9.344832
8.061532	446.626661	9.349850
7.821543	455.342772	9.354867
7.648642	454.685222	9.359885
7.926159	452.287701	9.364903
7.964003	448.649649	9.369920
7.835674	442.550894	9.374938
7.572616	446.454923	9.379955
7.824188	449.066507	9.384973
7.542311	441.587496	9.389991
7.566010	443.546827	9.395008
8.360538	442.589378	9.400026
7.756729	443.611938	9.405043
7.682811	430.587233	9.410061
7.409223	428.152989	9.415079
7.216813	438.471074	9.420096
7.788663	441.452191	9.425114
7.533207	445.995649	9.430131
7.622539	445.344349	9.435149
7.872419	447.700581	9.440167
7.947735	449.607645	9.445184
7.679539	440.242500	9.450202
7.620362	451.252919	9.455219
7.759837	446.219875	9.460237
7.447006	453.126523	9.465255
7.419546	456.577080	9.470272
7.687690	455.799934	9.475290
7.614031	448.894203	9.480307
7.651305	452.817448	9.485325
7.832270	456.213258	9.490343
8.039818	469.163717	9.495360
8.303328	469.949401	9.500378
7.785104	467.420939	9.505395
8.058226	447.910397	9.510413
8.287712	452.737632	9.515431
7.901241	453.432653	9.520448
7.994304	453.026918	9.525466
7.565163	452.794520	9.530483
7.307717	450.187332	9.535501
8.131970	459.989535	9.540519
7.834177	468.074089	9.545536
7.945449	474.706015	9.550554
8.126438	479.338887	9.555571
7.981578	464.128858	9.560589
8.010298	460.328133	9.565607
7.757963	462.053009	9.570624
8.170298	465.529332	9.575642
7.791123	460.839476	9.580659
7.935161	465.304566	9.585677
8.063179	472.053787	9.590695
8.073276	481.952009	9.595712
8.258430	477.612380	9.600730
7.725577	473.514637	9.605747
8.441382	475.655861	9.610765
8.227767	457.739495	9.615783
8.222510	462.168017	9.620800
8.312979	459.670415	9.625818
8.131299	464.369574	9.630835
7.978386	467.192857	9.635853
8.062808	461.590930	9.640871
7.851596	464.773637	9.645888
7.951668	457.200061	9.650906
8.097999	448.729316	9.655923
7.880930	460.629159	9.660941
8.054426	464.834016	9.665959
8.243898	473.265099	9.670976
8.311640	462.704920	9.675994
8.314776	462.975984	9.681011
8.157872	458.153474	9.686029
8.179091	462.076081	9.691047
8.088681	468.335667	9.696064
7.942989	463.994231	9.701082
8.009166	461.916997	9.706099
7.875581	460.764143	9.711117
8.268665	463.138965	9.716135
8.042465	490.086953	9.721152
8.148000	479.937403	9.726170
8.307152	482.219494	9.731187
8.205127	488.588203	9.736205
8.607175	482.456826	9.741223
8.259069	477.919885	9.746240
8.151906	469.734998	9.751258
8.032366	471.315992	9.756275
8.127910	483.289944	9.761293
8.527641	485.430201	9.766311
8.189605	486.657271	9.771328
8.056166	475.579502	9.776346
8.271593	481.336743	9.781363
8.528829	482.467389	9.786381
8.315486	483.059548	9.791399
8.095914	476.416506	9.796416
8.189089	483.493079	9.801434
8.294477	487.765417	9.806451
8.112928	485.351457	9.811469
8.251841	475.234550	9.816487
8.213163	478.857280	9.821504
8.171534	475.752376	9.826522
8.590322	484.305323	9.831539
8.379422	497.778953	9.836557
8.333942	490.174520	9.841575
8.381258	480.864060	9.846592
8.429491	479.565954	9.851610
8.457404	484.014530	9.856627
8.441733	488.504650	9.861645
8.812811	482.447552	9.866663
8.803029	486.933592	9.871680
8.178296	466.651690	9.876698
8.187118	460.045452	9.881715
8.451931	476.635008	9.886733
8.784846	480.114311	9.891751
8.189266	472.381485	9.896768
8.110597	468.004300	9.901786
8.397709	483.665730	9.906803
8.421771	481.260580	9.911821
8.555270	474.265577	9.916839
8.338307	486.165420	9.921856
8.486183	481.670686	9.926874
8.593645	473.875042	9.931891
8.345997	485.492518	9.936909
8.569390	480.241191	9.941927
8.766674	480.541796	9.946944
8.727740	486.389385	9.951962
8.621609	488.340661	9.956979
8.505682	490.189331	9.961997
8.646174	475.843445	9.967015
8.138938	478.952617	9.972032
8.136601	480.108155	9.977050
8.463634	477.794389	9.982067
8.302654	486.476045	9.987085
8.800932	475.838934	9.992103
8.209592	482.962798	9.997120
8.346698	482.026303	10.002138
8.755064	474.388637	10.007155
8.557940	482.788780	10.012173
8.604144	473.989732	10.017191
8.482155	477.685475	10.022208
8.639754	477.935494	10.027226
8.822912	485.509203	10.032243
8.441908	486.187591	10.037261
8.527952	469.423454	10.042279
8.667002	478.727120	10.047296
8.731722	488.982856	10.052314
8.664141	492.184089	10.057331
8.441712	493.607639	10.062349
8.639291	488.180475	10.067367
8.500567	487.457610	10.072384
8.288960	486.503169	10.077402
8.705761	488.328330	10.082419
8.625854	501.623650	10.087437
9.102499	507.709197	10.092455
8.542722	492.377964	10.097472
8.814157	503.645880	10.102490
8.979946	495.007963	10.107507
8.631476	495.267848	10.112525
8.641934	490.955587	10.117543
8.571967	495.290116	10.122560
8.768082	511.628539	10.127578
8.995025	502.062708	10.132595
8.855871	502.627464	10.137613
9.302692	500.929237	10.142631
8.819118	496.312533	10.147648
8.739388	486.135203	10.152666
8.632829	470.745601	10.157683
8.660143	496.303209	10.162701
8.713238	491.488812	10.167719
8.840346	503.912263	10.172736
8.708506	515.751452	10.177754
9.010739	506.312675	10.182771
8.523828	513.723144	10.187789
8.660699	502.767105	10.192807
8.629577	505.621804	10.197824
8.400492	518.858460	10.202842
8.830841	509.428010	10.207859
8.558377	513.305126	10.212877
8.925199	505.484610	10.217895
9.112194	518.015451	10.222912
8.835718	510.219987	10.227930
8.997595	505.126613	10.232947
9.102570	509.796648	10.237965
9.053342	503.906382	10.242983
9.315751	499.832351	10.248000
9.279279	496.259581	10.253018
9.156249	495.830899	10.258035
8.973348	510.676068	10.263053
9.443635	500.579808	10.268071
9.554506	502.664342	10.273088
8.750354	502.768408	10.278106
9.239610	497.118818	10.283123
9.417161	502.635850	10.288141
9.271021	495.763547	10.293159
9.011951	489.120377	10.298176
8.796135	483.098431	10.303194
8.894283	484.083592	10.308211
8.624766	476.072461	10.313229
9.113199	497.755122	10.318247
9.501851	498.082548	10.323264
9.302152	499.855984	10.328282
9.185890	490.599549	10.333299
9.246658	492.704555	10.338317
9.061574	493.292286	10.343335
8.840209	477.387340	10.348352
8.993017	491.501403	10.353370
9.166119	493.926476	10.358387
8.942514	512.473431	10.363405
9.032768	507.195620	10.368423
9.705403	505.562997	10.373440
9.140515	504.304150	10.378458
9.202782	487.568968	10.383475
8.965261	504.189920	10.388493
9.350977	493.690354	10.393511
9.318072	499.682168	10.398528
8.937643	500.063823	10.403546
9.193019	499.566384	10.408563
8.962416	508.987943	10.413581
9.005488	509.877594	10.418599
9.327542	508.748020	10.423616
9.008473	512.285303	10.428634
9.261063	495.952634	10.433651
9.024605	504.239030	10.438669
9.019420	502.529575	10.443687
9.310871	501.808735	10.448704
9.249719	508.849538	10.453722
9.207942	496.192130	10.458739
9.175224	510.158554	10.463757
9.146239	515.802624	10.468775
9.614869	511.159797	10.473792
9.470950	516.329575	10.478810
9.259260	488.781455	10.483827
9.458404	510.837659	10.488845
9.057941	511.042574	10.493863
9.186600	499.813272	10.498880
9.343978	502.433311	10.503898
9.538492	495.002710	10.508915
9.082302	498.769755	10.513933
9.156458	497.218281	10.518951
9.370747	508.678188	10.523968
9.163597	515.079157	10.528986
9.376379	520.133087	10.534003
9.298973	524.361492	10.539021
9.426825	537.008910	10.544039
9.539028	529.793161	10.549056
9.686535	536.529886	10.554074
9.323542	539.928890	10.559091
9.347499	539.231025	10.564109
9.591980	523.704325	10.569127
9.553448	526.392933	10.574144
9.507000	533.137954	10.579162
9.816670	527.450221	10.584179
9.366987	527.192638	10.589197
9.681495	532.593548	10.594215
9.682977	539.170118	10.599232
9.476077	531.796085	10.604250
9.778067	524.986099	10.609267
9.436247	517.292388	10.614285
9.247708	517.726028	10.619303
9.767779	524.517982	10.624320
9.944005	524.121305	10.629338
9.407900	507.467235	10.634355
9.608108	512.624118	10.639373
9.367705	522.807762	10.644391
9.729285	519.478730	10.649408
9.780897	523.841553	10.654426
9.790799	518.285997	10.659443
9.517959	518.846454	10.664461
9.499245	524.712977	10.669479
9.791497	523.676433	10.674496
10.020060	523.716521	10.679514
9.616687	515.394988	10.684531
9.536262	513.886666	10.689549
9.725942	524.258542	10.694567
10.098928	514.388957	10.699584
9.358092	506.025630	10.704602
9.676886	513.129979	10.709619
9.667180	519.818747	10.714637
9.470526	532.627458	10.719655
9.575174	533.027784	10.724672
9.666586	530.574206	10.729690
9.884971	532.774440	10.734707
9.984980	529.609465	10.739725
10.170665	529.135568	10.744743
9.729588	515.729675	10.749760
9.490115	525.764853	10.754778
9.862699	530.828462	10.759795
9.976708	530.703462	10.764813
9.720867	533.871084	10.769831
9.895039	532.660538	10.774848
9.619837	535.588199	10.779866
10.130540	531.147056	10.784883
10.173935	528.609484	10.789901
9.918253	527.175958	10.794919
9.805788	504.759338	10.799936
9.516372	517.920241	10.804954
9.631273	523.933085	10.809971
9.809561	523.264688	10.814989
10.063899	523.133481	10.820007
10.107319	529.321627	10.825024
9.812732	540.192262	10.830042
9.913681	529.797252	10.835059
9.914135	521.731178	10.840077
9.866517	538.309784	10.845095
9.779441	527.196316	10.850112
9.948774	529.454728	10.855130
9.956588	527.433966	10.860147
10.229573	537.960054	10.865165
10.161939	532.489225	10.870183
10.439449	523.477187	10.875200
10.391530	530.809413	10.880218
9.960225	519.267051	10.885235
10.083858	518.092827	10.890253
9.843024	510.298090	10.895271
10.128226	519.294858	10.900288
10.013272	525.403676	10.905306
10.145528	525.607175	10.910323
10.256457	529.073932	10.915341
9.931025	529.279715	10.920359
9.858851	526.252171	10.925376
9.982312	523.922959	10.930394
10.093824	531.148155	10.935411
10.063338	522.881801	10.940429
10.058932	533.527087	10.945447
10.371819	525.045988	10.950464
10.227045	527.429352	10.955482
10.185480	531.901450	10.960499
10.262019	523.870789	10.965517
9.905568	532.595718	10.970535
10.019758	525.688926	10.975552
10.111483	534.381503	10.980570
9.935562	533.339419	10.985587
9.968902	526.934440	10.990605
9.967589	530.538703	10.995623
10.101828	534.696080	11.000640
9.428709	531.330351	11.005658
9.795515	541.096977	11.010675
10.576715	554.607707	11.015693
10.075496	558.302926	11.020711
10.631209	555.896516	11.025728
10.543712	567.886581	11.030746
10.281063	558.766656	11.035763
10.438003	544.067846	11.040781
10.357134	543.231773	11.045799
10.020158	535.054460	11.050816
10.244674	551.536792	11.055834
9.990873	556.831095	11.060851
10.479746	551.954714	11.065869
10.435544	556.562929	11.070887
10.185686	549.902515	11.075904
10.458278	549.014216	11.080922
10.278517	554.151751	11.085939
10.421912	549.203270	11.090957
10.436702	550.356128	11.095975
10.614832	550.221083	11.100992
10.656901	552.262753	11.106010
10.363938	553.460676	11.111027
10.999035	557.552206	11.116045
10.543893	553.435957	11.121063
10.088881	540.499284	11.126080
9.699276	549.169455	11.131098
10.081526	554.809065	11.136115
10.232081	550.096145	11.141133
10.543071	550.334755	11.146151
10.687047	552.786489	11.151168
10.351261	562.565381	11.156186
10.421802	554.545114	11.161203
10.522638	552.295182	11.166221
10.771267	556.945878	11.171239
10.569882	549.031335	11.176256
10.734044	563.345646	11.181274
10.458820	556.468299	11.186291
10.339799	558.721401	11.191309
10.430777	557.564914	11.196327
10.668890	549.423720	11.201344
10.663518	547.016862	11.206362
10.402285	549.835040	11.211379
10.857803	550.871508	11.216397
10.784160	550.353035	11.221415
10.912584	556.508938	11.226432
11.027266	552.899851	11.231450
10.859986	556.195610	11.236467
10.929156	554.127363	11.241485
10.660028	560.531748	11.246503
10.785314	557.548998	11.251520
10.946497	559.840249	11.256538
10.791878	551.299844	11.261555
10.707299	555.314787	11.266573
10.664156	556.091718	11.271591
10.875291	557.166476	11.276608
10.567123	556.451222	11.281626
10.471077	563.062016	11.286643
10.941854	564.623110	11.291661
10.410393	559.868726	11.296679
10.829299	553.851447	11.301696
10.296856	550.634084	11.306714
10.315054	561.026538	11.311731
10.565168	560.993822	11.316749
10.587244	571.552930	11.321767
10.917189	574.127007	11.326784
10.843544	574.255471	11.331802
10.875325	581.029278	11.336819
10.751539	576.545528	11.341837
10.778605	569.844873	11.346855
10.864816	573.511170	11.351872
11.169794	573.144812	11.356890
10.680402	579.514287	11.361907
11.183835	576.346054	11.366925
10.921628	569.548712	11.371943
11.057317	572.093265	11.376960
10.900017	572.338977	11.381978
10.672065	580.523091	11.386995
10.983443	572.278889	11.392013
10.890266	573.366616	11.397031
10.613191	569.762102	11.402048
10.905212	570.477052	11.407066
11.063725	581.532338	11.412083
10.987388	570.988358	11.417101
10.627727	579.922094	11.422119
10.673907	587.441569	11.427136
11.098465	568.408938	11.432154
11.227518	575.019182	11.437171
11.388149	566.855407	11.442189
11.036276	579.906221	11.447207
11.062812	569.128374	11.452224
11.108949	575.234060	11.457242
10.984064	570.378100	11.462259
11.210887	573.044073	11.467277
11.149472	577.613966	11.472295
10.996957	574.498016	11.477312
11.474796	575.209098	11.482330
11.356952	571.469183	11.487347
11.484997	574.529327	11.492365
11.158434	574.852051	11.497383
11.317537	572.312123	11.502400
11.386512	575.129059	11.507418
11.399300	582.000517	11.512435
11.425197	578.708291	11.517453
11.451564	576.829784	11.522471
11.398172	572.202462	11.527488
11.488967	574.195475	11.532506
10.895484	573.815256	11.537523
11.360834	564.824259	11.542541
11.197053	566.901340	11.547559
11.288143	568.944799	11.552576
11.155016	559.593142	11.557594
11.022388	575.361444	11.562611
11.200136	567.213921	11.567629
11.282561	569.034678	11.572647
11.432464	563.914761	11.577664
11.216469	569.376711	11.582682
10.962921	573.948304	11.587699
11.387835	577.754037	11.592717
11.228242	564.818396	11.597735
11.172790	570.946310	11.602752
11.164919	577.391816	11.607770
11.567735	590.712553	11.612787
11.669936	590.658831	11.617805
11.715202	577.100952	11.622823
11.258818	578.248742	11.627840
11.612781	571.108706	11.632858
11.545803	576.739813	11.637875
11.718489	569.085386	11.642893
11.442947	564.767425	11.647911
11.333124	571.102672	11.652928
11.213552	560.757975	11.657946
11.067191	574.877953	11.662963
11.557212	587.402390	11.667981
11.606824	593.624302	11.672999
11.442006	603.127121	11.678016
11.681758	601.770597	11.683034
11.697849	597.754072	11.688051
11.785984	591.151137	11.693069
11.947679	595.203241	11.698087
11.803394	576.054603	11.703104
11.599144	570.015036	11.708122
11.378122	567.547290	11.713139
11.751413	573.772129	11.718157
11.889241	561.761872	11.723175
11.719809	566.149871	11.728192
12.019427	557.238494	11.733210
11.396891	568.078479	11.738227
11.954738	573.826280	11.743245
11.858710	571.622969	11.748263
11.716648	570.294713	11.753280
12.129725	572.300346	11.758298
11.829688	574.799562	11.763315
11.885585	560.103947	11.768333
11.820732	561.913065	11.773351
11.581356	560.618991	11.778368
11.742377	567.943741	11.783386
11.449358	561.545703	11.788403
11.727639	565.551131	11.793421
11.550364	572.565973	11.798439
11.180043	566.211603	11.803456
11.639763	570.406353	11.808474
11.595839	589.657378	11.813491
11.779900	589.650790	11.818509
11.943617	584.733829	11.823527
12.063345	598.862628	11.828544
12.350617	585.317317	11.833562
12.385902	592.791165	11.838579
11.684456	577.986980	11.843597
11.410120	571.472403	11.848615
11.261387	578.990857	11.853632
11.978602	583.688061	11.858650
11.693002	592.420852	11.863667
11.699343	592.704040	11.868685
11.602615	588.477977	11.873703
11.664919	596.073825	11.878720
11.975220	593.197780	11.883738
11.830288	596.751976	11.888755
11.942119	589.425809	11.893773
12.451271	587.455878	11.898791
12.123986	599.922189	11.903808
11.904120	585.295007	11.908826
12.084913	598.675784	11.913843
12.202107	593.895497	11.918861
12.210997	587.797282	11.923879
12.238722	600.116452	11.928896
12.028077	590.593889	11.933914
12.422439	592.570899	11.938931
12.209792	586.409567	11.943949
12.350955	594.491672	11.948967
11.599651	597.841076	11.953984
12.212367	585.049500	11.959002
11.737713	596.402816	11.964019
11.866839	589.809238	11.969037
12.184676	600.120053	11.974055
12.157341	612.952785	11.979072
12.383093	617.976309	11.984090
12.733673	612.897519	11.989107
12.229969	598.216968	11.994125
12.346920	581.722438	11.999143
12.079729	588.745062	12.004160
11.959910	581.890693	12.009178
12.000584	599.351765	12.014195
11.747680	608.843143	12.019213
12.427105	604.135707	12.024231
12.421936	612.026154	12.029248
12.655653	611.825594	12.034266
12.579778	613.200945	12.039283
12.433690	613.072517	12.044301
12.656791	609.913488	12.049319
12.480894	611.815748	12.054336
12.665196	598.911407	12.059354
12.314403	590.531108	12.064371
12.224880	590.516893	12.069389
12.304051	590.283743	12.074407
12.041691	610.979653	12.079424
12.067578	609.634546	12.084442
12.509976	611.657681	12.089459
12.395414	604.991826	12.094477
12.592911	610.010307	12.099495
12.445290	618.298616	12.104512
12.546308	616.329513	12.109530
12.555159	608.596598	12.114547
12.573433	612.844746	12.119565
12.926317	605.083174	12.124583
12.370527	622.218004	12.129600
12.722646	619.196548	12.134618
12.378071	617.218367	12.139635
12.477541	608.284675	12.144653
12.606067	606.317575	12.149671
12.521363	603.516042	12.154688
12.240433	606.974784	12.159706
12.489909	611.221420	12.164723
12.693948	618.997041	12.169741
13.138886	611.448261	12.174759
12.728164	607.110445	12.179776
13.025803	601.945279	12.184794
12.702855	603.596025	12.189811
12.706944	610.951693	12.194829
12.587618	603.109475	12.199847
12.631632	608.754760	12.204864
12.733046	605.778899	12.209882
12.975701	601.190391	12.214899
12.778634	601.331881	12.219917
12.592163	598.480022	12.224935
12.833343	608.828099	12.229952
12.463647	611.492868	12.234970
12.759866	606.599321	12.239987
12.630528	600.585876	12.245005
12.633063	604.628206	12.250023
12.402729	609.865198	12.255040
12.756415	607.777613	12.260058
12.899539	602.516737	12.265075
12.604340	609.253425	12.270093
12.669325	604.639105	12.275111
12.426259	607.296656	12.280128
12.929391	620.150420	12.285146
13.111738	623.789041	12.290163
13.058316	623.715521	12.295181
12.891096	607.192908	12.300199
12.873113	622.943289	12.305216
13.073885	634.471667	12.310234
13.180282	627.954219	12.315251
12.441729	621.209402	12.320269
12.917973	626.187369	12.325287
12.885167	634.334620	12.330304
13.298841	634.509806	12.335322
13.292150	637.310206	12.340339
13.036910	642.049338	12.345357
12.868385	633.703576	12.350375
13.275244	638.944882	12.355392
13.110615	634.366531	12.360410
13.211452	625.053921	12.365427
13.484204	628.776209	12.370445
13.470638	615.139156	12.375463
13.011446	612.049160	12.380480
12.612221	604.626336	12.385498
12.623229	614.414035	12.390515
12.853692	630.355868	12.395533
13.109139	626.513272	12.400551
12.975607	634.666838	12.405568
13.163439	630.973690	12.410586
13.655823	633.430807	12.415603
13.411405	635.151302	12.420621
13.500888	635.058547	12.425639
13.313281	624.629799	12.430656
13.462739	631.962698	12.435674
13.375970	625.156782	12.440691
13.567357	631.264976	12.445709
13.539476	625.708995	12.450727
13.507275	611.023986	12.455744
13.230165	606.627366	12.460762
13.098926	604.413790	12.465779
13.020016	611.217576	12.470797
13.330964	624.177193	12.475815
13.230745	636.992960	12.480832
13.569333	638.129805	12.485850
13.715697	637.094022	12.490867
13.571045	632.165404	12.495885
13.265283	617.210828	12.500903
13.089727	615.859413	12.505920
13.299565	631.949646	12.510938
13.870465	636.647698	12.515955
13.314495	641.721127	12.520973
13.579757	637.517231	12.525991
13.479860	629.350066	12.531008
13.504998	624.366444	12.536026
13.811940	627.998168	12.541043
13.399657	632.345340	12.546061
13.707894	628.036882	12.551079
13.372314	627.546825	12.556096
13.262023	639.313292	12.561114
13.544798	637.116894	12.566131
13.323038	634.409413	12.571149
13.027357	631.618842	12.576167
13.720632	636.042101	12.581184
13.386289	635.861118	12.586202
13.689391	627.905365	12.591219
13.551534	634.005186	12.596237
13.752873	624.919826	12.601255
13.426096	625.876899	12.606272
13.545680	625.312371	12.611290
13.499561	635.251043	12.616307
13.712853	628.164583	12.621325
13.672837	625.684247	12.626343
13.732875	644.448829	12.631360
13.751531	637.443353	12.636378
13.712834	635.107976	12.641395
13.542582	647.982061	12.646413
14.132866	641.530803	12.651431
13.828553	646.369144	12.656448
13.642969	637.028821	12.661466
14.236659	646.030968	12.666483
14.177687	642.714158	12.671501
14.080035	641.615622	12.676519
13.848115	621.549706	12.681536
13.606445	625.052793	12.686554
13.667843	618.621294	12.691571
13.301785	634.987953	12.696589
13.806952	651.912398	12.701607
14.265395	654.179176	12.706624
13.951941	656.317588	12.711642
14.316962	650.403393	12.716659
14.076866	652.255756	12.721677
13.723252	644.589084	12.726695
13.890390	643.108234	12.731712
14.187253	648.919042	12.736730
14.360538	643.281044	12.741747
13.632791	640.390910	12.746765
13.872132	643.288462	12.751783
14.034896	650.770763	12.756800
14.177275	648.287092	12.761818
14.348588	649.589002	12.766835
14.336872	656.445393	12.771853
14.103628	642.236826	12.776871
14.266441	645.553466	12.781888
13.964505	649.918065	12.786906
14.381475	648.858818	12.791923
14.264682	650.720264	12.796941
14.016511	636.182681	12.801959
14.302133	638.356615	12.806976
14.308314	646.453581	12.811994
14.332078	627.518398	12.817011
14.072210	622.244919	12.822029
14.152074	643.104995	12.827047
14.541270	646.856379	12.832064
14.143252	644.078684	12.837082
14.155247	636.051774	12.842099
14.152345	641.335193	12.847117
14.376998	639.356183	12.852135
13.982367	642.220522	12.857152
14.374383	654.889750	12.862170
14.843105	651.158900	12.867187
14.617416	648.385761	12.872205
14.223373	637.228803	12.877223
14.379715	628.655418	12.882240
14.584805	645.251333	12.887258
14.293552	642.592610	12.892275
14.124658	642.044877	12.897293
14.141445	653.763041	12.902311
14.241516	645.555070	12.907328
14.122134	644.459939	12.912346
14.406166	644.892122	12.917363
14.135369	650.772938	12.922381
14.231247	651.805801	12.927399
14.588247	647.379246	12.932416
14.538864	651.429721	12.937434
14.469472	645.618306	12.942451
14.371721	652.425060	12.947469
14.505099	643.110498	12.952487
14.649733	645.536895	12.957504
14.422839	652.666840	12.962522
14.719831	664.644065	12.967539
14.826216	661.575897	12.972557
14.699692	662.346962	12.977575
14.844754	646.150924	12.982592
14.347916	660.543633	12.987610
14.742914	660.185260	12.992627
14.744141	660.421913	12.997645
14.504463	669.999613	13.002663
14.892130	671.245535	13.007680
14.620378	669.186510	13.012698
14.853139	670.261043	13.017715
14.804391	670.900002	13.022733
14.585245	674.308051	13.027751
14.927573	675.248653	13.032768
14.773985	679.198697	13.037786
14.649914	672.067248	13.042803
14.526175	680.541192	13.047821
14.641007	667.003902	13.052839
14.688958	669.912510	13.057856
14.691525	677.315781	13.062874
15.344758	675.345357	13.067891
15.194171	667.940353	13.072909
15.100997	672.657257	13.077927
15.048541	670.866829	13.082944
14.802683	675.677084	13.087962
15.037375	667.536373	13.092979
15.037300	668.663166	13.097997
14.942508	669.981525	13.103015
15.310741	675.629680	13.108032
15.140551	674.034424	13.113050
15.298592	664.204747	13.118067
15.018844	665.078714	13.123085
14.804494	678.161701	13.128103
15.162055	674.539781	13.133120
14.863914	670.241114	13.138138
15.188383	665.797561	13.143155
15.080847	669.696206	13.148173
14.897777	674.809048	13.153191
14.792184	666.472345	13.158208
14.842952	674.237291	13.163226
15.090546	664.270506	13.168243
15.269531	678.273318	13.173261
14.977001	672.386404	13.178279
14.931275	665.911712	13.183296
14.852147	670.153044	13.188314
15.390044	673.433011	13.193331
15.255586	676.155606	13.198349
15.264336	673.976891	13.203367
15.143851	677.227472	13.208384
15.228532	683.958316	13.213402
15.761483	690.710447	13.218419
15.338796	675.610040	13.223437
15.129293	677.498637	13.228455
15.385111	681.911555	13.233472
15.410014	694.095532	13.238490
15.412642	695.812039	13.243507
15.617325	692.886256	13.248525
15.145309	689.530012	13.253543
15.782972	687.233822	13.258560
15.495229	683.331155	13.263578
15.532404	674.183128	13.268595
15.414076	664.983732	13.273613
15.339059	673.847670	13.278631
15.590537	666.174543	13.283648
15.065494	685.810323	13.288666
15.737643	688.826261	13.293683
15.634538	694.781802	13.298701
15.468958	698.307695	13.303719
15.648961	690.153452	13.308736
15.608923	700.776018	13.313754
15.590269	694.319165	13.318771
15.748535	696.885445	13.323789
15.598118	702.198306	13.328807
15.581357	699.875262	13.333824
15.632482	697.292274	13.338842
15.453607	690.589127	13.343859
15.674799	697.033500	13.348877
15.593737	701.716956	13.353895
15.572833	691.410372	13.358912
15.666688	696.492453	13.363930
15.560107	701.905743	13.368947
15.773109	702.039788	13.373965
15.801170	708.549139	13.378983
15.637092	696.440928	13.384000
15.778968	706.526910	13.389018
15.555553	698.347508	13.394035
15.890235	695.101554	13.399053
15.581392	702.998596	13.404071
15.924924	695.112219	13.409088
15.680313	695.501000	13.414106
15.572131	688.701570	13.419123
15.753989	699.103176	13.424141
16.031494	707.025114	13.429159
16.002197	719.927659	13.434176
16.285221	720.454676	13.439194
15.984601	711.047132	13.444211
15.918579	704.490399	13.449229
15.837945	714.096852	13.454247
16.318060	711.348817	13.459264
15.973618	705.025056	13.464282
15.766062	699.165844	13.469299
16.178880	714.766756	13.474317
16.054075	716.380155	13.479335
16.350758	714.421410	13.484352
15.843279	710.912928	13.489370
16.067414	712.329642	13.494387
16.133786	715.004998	13.499405
16.224605	726.373938	13.504423
16.305783	708.641505	13.509440
16.391701	718.679457	13.514458
16.109505	710.745945	13.519475
16.495650	704.550712	13.524493
16.182006	701.068666	13.529511
16.082734	694.646535	13.534528
15.955999	700.978166	13.539546
16.236121	710.089436	13.544563
16.638006	714.375333	13.549581
16.610341	724.014518	13.554599
16.346674	695.076198	13.559616
16.182092	693.824044	13.564634
16.123115	709.142266	13.569651
16.416704	699.455434	13.574669
16.088483	709.927498	13.579687
16.513167	708.649288	13.584704
16.534963	706.922962	13.589722
16.819423	716.566887	13.594739
17.014876	703.417726	13.599757
16.599493	689.332333	13.604775
16.477925	689.824911	13.609792
16.564428	683.064408	13.614810
16.357016	682.910873	13.619827
16.498026	681.456205	13.624845
16.517431	683.226887	13.629863
16.648029	684.828669	13.634880
16.308018	684.841077	13.639898
16.193541	683.568450	13.644915
16.390000	691.954361	13.649933
16.224904	702.647015	13.654951
16.299523	714.731698	13.659968
16.416140	716.035872	13.664986
16.562654	722.198465	13.670003
16.594388	713.013401	13.675021
15.864478	719.357493	13.680039
16.515388	720.328644	13.685056
16.502927	728.245532	13.690074
16.214820	735.558670	13.695091
16.736887	730.471913	13.700109
16.910276	747.751391	13.705127
16.716469	747.359038	13.710144
16.995773	738.842074	13.715162
16.777291	738.564041	13.720179
17.414206	732.206431	13.725197
16.948174	746.417657	13.730215
16.701991	735.388948	13.735232
17.238580	732.089262	13.740250
16.787568	739.595184	13.745267
17.209871	736.871982	13.750285
17.101606	733.020079	13.755303
16.594274	709.519510	13.760320
16.412643	725.238816	13.765338
16.505806	735.771105	13.770355
16.910464	731.728383	13.775373
16.794979	739.535185	13.780391
16.489109	745.765511	13.785408
16.650779	739.169934	13.790426
16.544589	750.437213	13.795443
16.804888	749.102705	13.800461
16.977887	759.026050	13.805479
17.054403	766.247357	13.810496
17.385018	758.937334	13.815514
16.989874	761.104337	13.820531
17.338695	755.489293	13.825549
17.057165	760.993128	13.830567
17.176940	753.198589	13.835584
17.210843	749.523223	13.840602
17.009060	761.657557	13.845619
17.769701	750.619412	13.850637
17.355659	765.317970	13.855655
17.562004	757.576137	13.860672
17.356696	744.647528	13.865690
17.756337	751.714060	13.870707
17.630781	734.916556	13.875725
17.485593	732.339075	13.880743
17.501693	728.947370	13.885760
17.424240	730.692207	13.890778
17.174063	723.369056	13.895795
17.333406	719.929663	13.900813
17.402064	731.093795	13.905831
17.315889	728.447108	13.910848
17.521479	730.990199	13.915866
17.102042	731.220179	13.920883
17.119227	723.517466	13.925901
17.663724	751.070930	13.930919
17.591938	747.263801	13.935936
17.820026	733.926467	13.940954
16.999407	736.289519	13.945971
17.443501	737.081636	13.950989
17.597047	756.582768	13.956007
17.522865	761.205201	13.961024
17.813089	757.183558	13.966042
17.321628	763.805888	13.971059
17.547276	746.571491	13.976077
17.315548	753.301445	13.981095
17.314679	757.943948	13.986112
17.990240	753.508480	13.991130
17.398300	764.350101	13.996147
17.641779	764.545643	14.001165
17.567646	757.295882	14.006183
17.358258	754.668496	14.011200
17.773111	757.642708	14.016218
17.363645	758.480200	14.021235
17.743853	771.870887	14.026253
17.842661	774.970361	14.031271
18.005660	775.352083	14.036288
18.330460	774.752241	14.041306
17.604538	768.399865	14.046323
17.651911	748.059671	14.051341
17.927434	764.234406	14.056359
17.737798	774.552250	14.061376
18.227773	767.078400	14.066394
18.142132	782.202046	14.071411
18.454331	781.544217	14.076429
18.278436	766.092639	14.081447
18.150470	765.033560	14.086464
18.471081	757.826091	14.091482
18.043877	760.528294	14.096499
17.970855	760.902815	14.101517
17.721966	761.065048	14.106535
17.886183	757.725870	14.111552
17.929234	756.308635	14.116570
17.611427	760.505334	14.121587
18.209108	762.832362	14.126605
18.356739	768.688681	14.131623
18.047783	781.300570	14.136640
18.420601	776.505430	14.141658
18.260198	773.955573	14.146675
18.082448	781.267218	14.151693
18.114157	771.277394	14.156711
18.131712	780.174217	14.161728
18.283103	768.878068	14.166746
18.523655	778.140740	14.171763
18.412836	770.404413	14.176781
18.428290	775.369413	14.181799
18.421735	777.040030	14.186816
18.430571	763.771740	14.191834
18.291249	765.087615	14.196851
18.377553	774.140923	14.201869
18.589857	774.177247	14.206887
18.027827	769.295051	14.211904
18.349279	774.963191	14.216922
18.255545	776.729519	14.221939
18.362126	781.194246	14.226957
18.603314	776.126238	14.231975
18.720209	789.507702	14.236992
19.051544	772.843705	14.242010
18.541654	779.068138	14.247027
18.678722	784.216058	14.252045
18.939940	779.122820	14.257063
18.281596	772.478986	14.262080
18.533959	775.888918	14.267098
18.247621	770.666878	14.272115
18.458822	778.261565	14.277133
18.850136	774.154652	14.282151
18.597657	787.275251	14.287168
18.857359	773.222874	14.292186
18.927674	785.141021	14.297203
18.928371	776.588796	14.302221
18.683116	771.407657	14.307239
18.607383	770.567612	14.312256
18.612081	772.425814	14.317274
18.827991	771.672619	14.322291
18.973200	769.529317	14.327309
18.773411	783.667299	14.332327
18.542796	785.385645	14.337344
18.887747	771.032734	14.342362
18.406856	783.056178	14.347379
18.444204	786.834318	14.352397
18.812344	784.119595	14.357415
18.798533	793.879724	14.362432
19.180737	800.286284	14.367450
19.456553	806.245609	14.372467
19.198418	791.927212	14.377485
19.331368	775.767669	14.382503
18.815531	783.608815	14.387520
19.095612	767.978495	14.392538
18.917690	767.069254	14.397555
19.033408	778.522689	14.402573
18.779303	781.406058	14.407591
19.014869	796.148028	14.412608
19.480576	797.823547	14.417626
19.154943	799.471576	14.422643
19.283732	811.115489	14.427661
19.214366	793.046796	14.432679
18.957048	797.003650	14.437696
19.233715	794.410556	14.442714
19.120305	798.063995	14.447731
18.931328	807.703253	14.452749
19.594482	796.194358	14.457767
19.175123	801.183310	14.462784
19.468806	805.448313	14.467802
19.281126	802.003316	14.472819
19.191159	803.728030	14.477837
19.497573	803.724362	14.482855
19.684547	810.322462	14.487872
19.518799	808.827484	14.492890
19.459428	799.025485	14.497907
19.254162	803.778921	14.502925
20.000837	794.570161	14.507943
19.404724	804.967489	14.512960
19.549676	801.198973	14.517978
19.248001	802.884274	14.522995
19.476180	797.291275	14.528013
19.495963	797.237843	14.533031
19.604214	794.510190	14.538048
19.617006	795.808545	14.543066
19.693030	789.671341	14.548083
19.419826	801.422414	14.553101
19.850768	799.843414	14.558119
19.715599	797.131809	14.563136
19.660240	795.149318	14.568154
19.957039	794.254059	14.573171
19.804050	788.433605	14.578189
19.805320	789.225678	14.583207
19.709976	796.780040	14.588224
19.537913	789.504583	14.593242
19.784490	809.199482	14.598259
19.559803	803.768956	14.603277
20.129591	793.600137	14.608295
19.622961	800.792905	14.613312
20.008089	795.146914	14.618330
19.720772	798.729771	14.623347
19.765196	803.769135	14.628365
19.979289	795.950331	14.633383
19.565395	793.645317	14.638400
19.999142	802.940849	14.643418
19.994188	816.395074	14.648435
20.180094	824.060016	14.653453
20.236117	814.681745	14.658471
19.999243	824.631475	14.663488
20.274884	822.808561	14.668506
20.245159	817.296990	14.673523
19.713469	813.382023	14.678541
20.100292	806.915248	14.683559
19.994653	817.503980	14.688576
20.110457	833.069481	14.693594
20.165652	823.205337	14.698611
19.874352	834.110349	14.703629
20.198904	819.028443	14.708647
19.785196	824.915927	14.713664
20.118275	821.465073	14.718682
19.964465	820.498402	14.723699
20.250764	829.469909	14.728717
20.313042	822.353384	14.733735
20.211311	832.405022	14.738752
20.568648	841.453768	14.743770
20.202978	829.402298	14.748787
20.331394	831.304239	14.753805
20.359468	845.924124	14.758823
20.694661	857.302197	14.763840
20.518046	846.925245	14.768858
20.693263	843.426536	14.773875
20.339283	848.458907	14.778893
20.224981	833.985395	14.783911
20.304678	841.269351	14.788928
20.122167	853.388104	14.793946
20.725850	856.998628	14.798963
20.325394	852.649676	14.803981
20.713374	848.795735	14.808999
20.753390	849.594364	14.814016
20.681996	852.493298	14.819034
21.035165	849.326471	14.824051
20.412299	851.996228	14.829069
21.038730	851.216578	14.834087
20.928606	848.725105	14.839104
21.254808	839.550644	14.844122
21.125566	847.249195	14.849139
20.535023	855.704842	14.854157
20.635863	852.814237	14.859175
20.697766	841.951788	14.864192
20.956448	840.437645	14.869210
20.852894	843.215383	14.874227
20.670812	847.198331	14.879245
21.180754	838.124471	14.884263
20.887912	847.615920	14.889280
20.868130	842.986418	14.894298
21.189673	844.198532	14.899315
20.899629	840.602306	14.904333
20.965303	839.108935	14.909351
21.085034	841.255237	14.914368
20.977690	837.485218	14.919386
21.103688	845.721294	14.924403
20.963879	843.726783	14.929421
21.098093	834.033290	14.934439
21.103878	851.913491	14.939456
20.925865	849.255928	14.944474
21.223786	841.622788	14.949491
21.063883	848.344679	14.954509
21.265732	848.745563	14.959527
21.400437	842.993625	14.964544
21.056916	844.445642	14.969562
21.184719	843.078238	14.974579
21.188897	852.611516	14.979597
20.963003	846.808777	14.984615
21.271324	848.991804	14.989632
21.539179	873.874786	14.994650
21.485909	850.801510	14.999667
21.665121	850.019347	15.004685
21.635203	840.184309	15.009703
21.155108	844.608428	15.014720
21.400020	853.722132	15.019738
21.647101	843.512329	15.024755
21.504687	845.870119	15.029773
21.549693	836.903821	15.034791
21.652122	842.183418	15.039808
21.778110	847.872740	15.044826
21.698080	844.492919	15.049843
21.396736	847.008156	15.054861
21.660449	840.570125	15.059879
21.458354	839.191293	15.064896
21.838731	852.689314	15.069914
22.130027	846.963333	15.074931
21.669946	840.686044	15.079949
21.731768	847.540454	15.084967
21.476653	840.022368	15.089984
21.030597	853.438434	15.095002
21.529760	858.646408	15.100019
21.406306	868.041900	15.105037
21.661344	854.977968	15.110055
21.805616	861.349245	15.115072
21.900207	857.042649	15.120090
21.677841	852.318652	15.125107
21.809675	861.942388	15.130125
21.639695	856.919844	15.135143
21.770815	863.476222	15.140160
21.932754	884.181708	15.145178
22.420984	885.784279	15.150195
22.075545	877.153694	15.155213
21.937262	860.115066	15.160231
22.240450	865.287475	15.165248
22.143106	865.706835	15.170266
22.257109	852.977428	15.175283
22.056569	856.407843	15.180301
22.272755	850.829331	15.185319
22.150035	852.546558	15.190336
21.800849	841.776921	15.195354
22.432925	853.906901	15.200371
22.560621	868.384963	15.205389
22.584072	864.420874	15.210407
22.458888	856.721475	15.215424
22.454296	861.102654	15.220442
22.404861	860.116472	15.225459
21.905398	857.458780	15.230477
21.990107	845.087422	15.235495
22.279172	861.806083	15.240512
22.327799	873.213286	15.245530
22.667826	876.000425	15.250547
22.764534	862.109218	15.255565
22.503796	856.198326	15.260583
22.436101	859.191357	15.265600
22.152056	857.935818	15.270618
22.367125	872.144570	15.275635
22.655288	884.246404	15.280653
22.583499	887.505171	15.285671
22.561223	887.221641	15.290688
22.556661	888.115618	15.295706
22.755871	876.884493	15.300723
22.581451	885.877720	15.305741
22.555416	884.976234	15.310759
22.789568	880.288000	15.315776
22.666287	888.051907	15.320794
22.648138	877.157797	15.325811
22.819508	871.081366	15.330829
22.763911	886.699016	15.335847
22.686267	878.761782	15.340864
22.540276	885.702416	15.345882
22.543439	878.213275	15.350899
22.433383	880.506038	15.355917
22.567512	887.469057	15.360935
23.010691	881.125970	15.365952
22.951063	891.319369	15.370970
23.091150	902.636521	15.375987
23.322236	890.595652	15.381005
22.949942	887.072264	15.386023
23.338006	880.277061	15.391040
23.077416	887.557547	15.396058
23.247059	885.792260	15.401075
23.195043	868.131031	15.406093
22.978017	877.127774	15.411111
22.956919	869.778138	15.416128
22.970603	886.846086	15.421146
23.263444	888.308855	15.426163
23.287252	883.416889	15.431181
23.083875	881.173555	15.436199
23.718262	891.902007	15.441216
23.190452	884.489744	15.446234
23.573428	868.174176	15.451251
23.472573	877.755482	15.456269
23.518893	881.361821	15.461287
23.601665	873.721351	15.466304
23.099150	882.728113	15.471322
23.131113	871.160274	15.476339
23.668136	880.512249	15.481357
23.093406	879.377993	15.486375
23.586435	873.314280	15.491392
23.613200	879.423106	15.496410
23.406713	879.329385	15.501427
23.666238	884.057357	15.506445
23.581074	892.228708	15.511463
23.640595	875.212723	15.516480
23.560675	885.955258	15.521498
23.665171	881.536650	15.526515
23.604704	880.561662	15.531533
23.606866	889.205329	15.536551
23.976156	887.418229	15.541568
23.635578	886.187324	15.546586
23.660741	889.074291	15.551603
23.588359	889.451870	15.556621
23.640540	898.034055	15.561639
24.382855	887.301660	15.566656
24.055037	894.800967	15.571674
23.741400	874.368868	15.576691
23.965379	877.612852	15.581709
23.611350	876.308315	15.586727
23.872758	887.331891	15.591744
23.878352	888.896471	15.596762
24.229659	890.750872	15.601779
24.306109	897.038114	15.606797
23.856723	884.990255	15.611815
24.157726	885.546020	15.616832
24.017203	890.327205	15.621850
23.972209	885.594343	15.626867
23.857668	899.854761	15.631885
23.661856	893.826385	15.636903
24.246214	892.220184	15.641920
24.357205	892.367058	15.646938
24.290380	895.116959	15.651955
24.436405	893.061878	15.656973
23.769698	896.473820	15.661991
24.178623	882.640978	15.667008
24.296842	896.164328	15.672026
24.391837	879.278482	15.677043
24.356426	880.429760	15.682061
24.433051	891.718978	15.687079
24.487028	893.285446	15.692096
24.275236	899.090825	15.697114
24.067356	893.862767	15.702131
24.334391	887.424199	15.707149
24.164808	897.660076	15.712167
24.717454	883.265066	15.717184
24.605869	896.963279	15.722202
24.029398	893.954725	15.727219
24.346281	905.354632	15.732237
24.446514	914.601491	15.737255
24.533687	907.793460	15.742272
24.621929	916.401562	15.747290
24.742294	915.142616	15.752307
25.166503	909.067583	15.757325
24.926189	909.616643	15.762343
24.649000	914.980988	15.767360
24.609546	914.154186	15.772378
24.757944	920.628982	15.777395
24.992480	912.608106	15.782413
24.789228	911.611307	15.787431
24.919463	909.236802	15.792448
24.768610	916.692613	15.797466
24.829328	919.977963	15.802483
25.046694	907.547907	15.807501
24.986292	913.080259	15.812519
25.039619	912.948986	15.817536
25.069480	910.937351	15.822554
25.310679	901.795111	15.827571
25.215735	910.898977	15.832589
24.961045	911.513406	15.837607
25.226611	902.020206	15.842624
24.843798	919.529009	15.847642
24.929582	911.004415	15.852659
24.974360	909.773092	15.857677
24.781958	913.621970	15.862695
24.783892	915.013555	15.867712
24.958287	912.524832	15.872730
25.149370	922.903032	15.877747
25.218674	929.996146	15.882765
25.441226	932.457713	15.887783
25.426774	936.647948	15.892800
25.531955	934.286833	15.897818
25.492529	929.979127	15.902835
25.263167	917.830499	15.907853
25.556767	924.418247	15.912871
25.854602	924.892458	15.917888
25.371728	920.726817	15.922906
24.983036	913.169667	15.927923
25.514268	924.479197	15.932941
25.277478	936.606511	15.937959
25.757127	932.264813	15.942976
25.399953	933.816807	15.947994
25.413307	930.138312	15.953011
25.492386	935.664597	15.958029
25.743476	939.497643	15.963047
25.838285	925.982230	15.968064
25.394246	934.276102	15.973082
25.797289	929.217406	15.978099
25.730937	930.591288	15.983117
25.595466	934.257679	15.988135
25.648606	932.573758	15.993152
25.617745	938.110957	15.998170
25.459484	939.616007	16.003187
25.810772	949.006587	16.008205
26.166538	955.221684	16.013223
26.107511	958.645725	16.018240
26.467383	956.222611	16.023258
26.334575	947.710157	16.028275
26.176168	934.518438	16.033293
26.104376	937.354331	16.038311
26.062714	930.667465	16.043328
26.145392	935.205404	16.048346
26.001439	924.577133	16.053363
25.742070	930.907535	16.058381
25.916516	942.875746	16.063399
26.478152	957.396345	16.068416
26.749287	953.683767	16.073434
26.310582	953.231949	16.078451
26.294251	938.058182	16.083469
26.195932	937.855994	16.088487
26.274836	932.813369	16.093504
26.623630	946.338500	16.098522
26.289697	946.794930	16.103539
26.573868	947.624738	16.108557
26.437372	947.557920	16.113575
26.256542	953.307972	16.118592
26.558699	950.063913	16.123610
26.465289	948.178886	16.128627
26.728505	943.176809	16.133645
26.328528	947.907141	16.138663
26.360392	939.536150	16.143680
26.461114	951.231890	16.148698
26.435367	949.967432	16.153715
26.662518	946.659385	16.158733
26.335703	952.788921	16.163751
26.727469	943.739835	16.168768
26.789545	949.448671	16.173786
26.970574	949.322637	16.178803
26.586360	933.445954	16.183821
26.663444	945.318966	16.188839
26.582058	947.215921	16.193856
26.769109	953.246009	16.198874
26.730272	952.469603	16.203891
26.922652	952.764674	16.208909
26.845285	955.828665	16.213927
27.133029	965.784641	16.218944
27.142273	951.698782	16.223962
26.789214	953.366900	16.228979
27.319906	963.840239	16.233997
27.370247	959.834046	16.239015
27.010968	951.890412	16.244032
27.202787	942.389810	16.249050
27.026870	950.730044	16.254067
26.991766	948.053231	16.259085
26.965622	959.784634	16.264103
27.374678	970.324373	16.269120
27.422527	965.949333	16.274138
27.292501	975.636250	16.279155
27.456465	964.041357	16.284173
27.011114	977.735121	16.289191
27.290848	975.024755	16.294208
27.281608	963.438064	16.299226
27.223283	972.094404	16.304243
27.172586	965.064952	16.309261
27.230829	968.375946	16.314279
27.207919	973.855104	16.319296
27.139339	970.905817	16.324314
27.148327	964.611796	16.329331
27.416118	973.583120	16.334349
27.639947	988.481725	16.339367
27.936535	983.748967	16.344384
27.874134	989.638268	16.349402
27.497770	987.387309	16.354419
28.209477	990.157258	16.359437
28.027615	978.698591	16.364455
27.956650	969.172875	16.369472
28.076174	959.753019	16.374490
27.872899	966.715284	16.379507
27.745062	966.028562	16.384525
27.730134	965.605021	16.389543
27.713644	958.027405	16.394560
27.996182	964.695798	16.399578
27.581517	961.548269	16.404595
28.087621	975.812492	16.409613
27.797641	990.693772	16.414631
27.911809	988.558463	16.419648
28.292271	977.504006	16.424666
28.283802	984.072832	16.429683
27.886080	979.578250	16.434701
28.530015	978.947335	16.439719
27.878317	985.282421	16.444736
28.344765	985.518772	16.449754
27.975569	985.201231	16.454771
28.357125	981.594426	16.459789
28.597281	983.324239	16.464807
28.097012	983.532171	16.469824
28.033254	983.785322	16.474842
27.867075	994.055435	16.479859
28.408394	990.559299	16.484877
28.353135	975.312703	16.489895
28.336106	989.153965	16.494912
28.527354	981.439648	16.499930
28.214586	974.239811	16.504947
28.367366	978.593206	16.509965
28.657008	972.125819	16.514983
28.509866	978.148315	16.520000
28.792002	975.346052	16.525018
28.471068	981.910184	16.530035
28.622234	983.066950	16.535053
28.053615	989.379554	16.540071
28.142459	999.786441	16.545088
28.921462	997.064119	16.550106
28.807074	1004.589993	16.555123
28.980031	1020.399172	16.560141
28.976374	1000.644209	16.565159
28.838646	1003.253755	16.570176
28.925500	1003.723153	16.575194
29.058429	1002.818846	16.580211
29.141462	1001.723536	16.585229
29.356924	994.182147	16.590247
29.101528	1007.972407	16.595264
29.315882	996.865067	16.600282
29.114085	1000.870073	16.605299
29.050901	997.405531	16.610317
29.084361	991.622071	16.615335
29.131558	999.684369	16.620352
29.254953	986.590472	16.625370
29.073965	993.722827	16.630387
29.000729	1005.650990	16.635405
29.418553	995.023022	16.640423
29.032559	1003.891665	16.645440
29.153797	997.681032	16.650458
29.057550	1002.751961	16.655475
29.049775	1000.866135	16.660493
29.241218	1000.899417	16.665511
29.066253	1002.621688	16.670528
29.287088	1004.458674	16.675546
29.034987	1011.444384	16.680563
29.504352	1026.831580	16.685581
29.361464	1027.128689	16.690599
29.470644	1031.545734	16.695616
29.604334	1029.120178	16.700634
29.628273	1036.599146	16.705651
29.940487	1025.883563	16.710669
29.925593	1027.318819	16.715687
29.790154	1027.703125	16.720704
29.517638	1027.133745	16.725722
29.535286	1023.214712	16.730739
29.685596	1023.516376	16.735757
29.869890	1014.512386	16.740775
29.755537	1024.963748	16.745792
30.037048	1025.342687	16.750810
30.047055	1024.504976	16.755827
30.066540	1022.908372	16.760845
30.068011	1022.441234	16.765863
29.636644	1023.357908	16.770880
29.924507	1011.244945	16.775898
30.020016	1020.953356	16.780915
30.236212	1024.577289	16.785933
30.510905	1023.606587	16.790951
30.233875	1027.566580	16.795968
30.340075	1009.470159	16.800986
30.436482	1018.026538	16.806003
30.275488	1018.137131	16.811021
30.312375	1013.637563	16.816039
30.446750	1017.763473	16.821056
30.456624	1018.475312	16.826074
30.114457	1018.257679	16.831091
30.254496	1024.544470	16.836109
30.615572	1012.448438	16.841127
30.230813	1017.343664	16.846144
30.666688	1012.368165	16.851162
30.761133	1018.851450	16.856179
30.646368	1013.428884	16.861197
30.649603	1015.214755	16.866215
30.432311	1027.512649	16.871232
30.333153	1016.779472	16.876250
30.262177	1019.476393	16.881267
30.147656	1011.210356	16.886285
30.502672	1010.163952	16.891303
30.158072	1014.598441	16.896320
30.510147	1024.143576	16.901338
30.551238	1041.636575	16.906355
30.929398	1049.325142	16.911373
31.089375	1043.998378	16.916391
30.452375	1040.617422	16.921408
30.643708	1040.445590	16.926426
30.578287	1045.091970	16.931443
31.050281	1044.525863	16.936461
31.049628	1040.385628	16.941479
30.860320	1045.313356	16.946496
30.828205	1045.864513	16.951514
31.071736	1036.781801	16.956531
30.830330	1049.777778	16.961549
31.103458	1036.095484	16.966567
30.785056	1045.723589	16.971584
30.794533	1054.508204	16.976602
31.552565	1059.281196	16.981619
31.395853	1072.450116	16.986637
31.651474	1065.524112	16.991655
31.243824	1070.167314	16.996672
31.173385	1063.226124	17.001690
31.420994	1066.756780	17.006707
31.416410	1071.977472	17.011725
31.756385	1066.975957	17.016743
31.527630	1064.944863	17.021760
31.769601	1064.335899	17.026778
31.957193	1056.019350	17.031795
31.406933	1044.435321	17.036813
31.668206	1035.409792	17.041831
31.046654	1043.734682	17.046848
31.259314	1049.508321	17.051866
31.308383	1061.108083	17.056883
31.509260	1062.616835	17.061901
31.716971	1055.808797	17.066919
31.412578	1058.611725	17.071936
31.613854	1059.107380	17.076954
31.576423	1059.372186	17.081971
31.554306	1081.460609	17.086989
32.078451	1081.716325	17.092007
32.137841	1089.802000	17.097024
32.269750	1091.157455	17.102042
32.539189	1073.937974	17.107059
31.996914	1064.792171	17.112077
32.082538	1060.660503	17.117095
31.947383	1055.121196	17.122112
32.237183	1053.914591	17.127130
32.441696	1061.854437	17.132147
32.167177	1058.003264	17.137165
32.416278	1055.127268	17.142183
32.369865	1051.944116	17.147200
32.227382	1053.995825	17.152218
32.409047	1051.111461	17.157235
31.888882	1057.479613	17.162253
32.434441	1056.658978	17.167271
32.561559	1072.090369	17.172288
32.356790	1073.896213	17.177306
32.592979	1076.503989	17.182323
32.547867	1069.650350	17.187341
32.665103	1071.232169	17.192359
32.594045	1073.878617	17.197376
32.682254	1071.214023	17.202394
32.383357	1064.734671	17.207411
32.510704	1071.787188	17.212429
32.992680	1071.819133	17.217447
32.856470	1074.169669	17.222464
32.744448	1076.102996	17.227482
33.324585	1064.793134	17.232499
32.838604	1050.532318	17.237517
32.785126	1044.352199	17.242535
32.682587	1048.086038	17.247552
32.723351	1041.398839	17.252570
32.967120	1057.108592	17.257587
33.042895	1071.604421	17.262605
32.878736	1068.193557	17.267623
33.032539	1073.717644	17.272640
32.955304	1075.228945	17.277658
33.125736	1067.192797	17.282675
33.214569	1081.478302	17.287693
33.338926	1071.173985	17.292711
32.999712	1070.394143	17.297728
33.006754	1078.910903	17.302746
33.356548	1069.691601	17.307763
33.108003	1078.333614	17.312781
33.314326	1072.807072	17.317799
33.197607	1076.640971	17.322816
33.029623	1076.383423	17.327834
33.231828	1068.601077	17.332851
33.284741	1068.873820	17.337869
32.927803	1077.207761	17.342887
32.916375	1084.771187	17.347904
32.764231	1093.726314	17.352922
33.364253	1088.677738	17.357939
33.222989	1093.427534	17.362957
33.743461	1100.610977	17.367975
33.572826	1102.872234	17.372992
33.679135	1104.686148	17.378010
34.064530	1097.701928	17.383027
33.831590	1100.610434	17.388045
33.758109	1094.827916	17.393063
33.752283	1107.884857	17.398080
33.651603	1110.684278	17.403098
34.276979	1113.808609	17.408115
34.134569	1118.710073	17.413133
34.105692	1113.425502	17.418151
34.221892	1108.304399	17.423168
33.809777	1094.890373	17.428186
34.087504	1106.059854	17.433203
34.427215	1111.444369	17.438221
33.951380	1097.011509	17.443239
34.238545	1100.867341	17.448256
33.926744	1111.412808	17.453274
34.200157	1102.521045	17.458291
34.130129	1118.308420	17.463309
34.524275	1110.738987	17.468327
34.622349	1109.754926	17.473344
34.364434	1115.510795	17.478362
34.392192	1105.717067	17.483379
34.383689	1111.496975	17.488397
34.677706	1107.215879	17.493415
34.501502	1116.973225	17.498432
34.581798	1102.090300	17.503450
35.016096	1109.277781	17.508467
34.596106	1109.255380	17.513485
34.716398	1104.515498	17.518503
34.667523	1110.109223	17.523520
34.731992	1106.539450	17.528538
34.887349	1105.104591	17.533555
34.911778	1104.113134	17.538573
34.802144	1102.123333	17.543591
34.953359	1104.905378	17.548608
34.826337	1111.357122	17.553626
35.102814	1111.326588	17.558643
34.917069	1114.473860	17.563661
35.056146	1104.706874	17.568679
35.094830	1100.894984	17.573696
34.893293	1102.226943	17.578714
34.932401	1104.846667	17.583731
35.040775	1102.532367	17.588749
35.279974	1097.414087	17.593767
35.465192	1098.562370	17.598784
35.018742	1109.280414	17.603802
35.141634	1102.766521	17.608819
35.097459	1095.748619	17.613837
35.227975	1094.967764	17.618855
35.560388	1093.543036	17.623872
35.229845	1099.177732	17.628890
35.200736	1090.289192	17.633907
34.870750	1106.158313	17.638925
35.061456	1095.045150	17.643943
35.473549	1103.397470	17.648960
35.107450	1116.129003	17.653978
35.396048	1109.841615	17.658995
35.561921	1124.629492	17.664013
35.351438	1129.506911	17.669031
35.468099	1125.392457	17.674048
35.395836	1126.164507	17.679066
35.335255	1129.478369	17.684083
35.322954	1144.139540	17.689101
35.476068	1151.686681	17.694119
35.765785	1152.155859	17.699136
36.081170	1153.100710	17.704154
35.834789	1146.060819	17.709171
35.970542	1147.437767	17.714189
35.875663	1139.275894	17.719207
36.270019	1144.352048	17.724224
35.938908	1158.829646	17.729242
36.528379	1150.279670	17.734259
36.150665	1149.840380	17.739277
36.338149	1145.172013	17.744295
36.622694	1142.498739	17.749312
36.570137	1150.103351	17.754330
36.586957	1143.347280	17.759347
36.491808	1148.140360	17.764365
36.822985	1153.687175	17.769383
36.520749	1139.744646	17.774400
36.019348	1145.387192	17.779418
36.306339	1138.891757	17.784435
36.512737	1145.212376	17.789453
36.547029	1150.613197	17.794471
36.610451	1130.298456	17.799488
36.815650	1143.511713	17.804506
36.397743	1138.887706	17.809523
36.756084	1142.561978	17.814541
36.667117	1141.200111	17.819559
36.605647	1142.008342	17.824576
36.603396	1149.415719	17.829594
36.820730	1140.501165	17.834611
36.832695	1133.818444	17.839629
36.870216	1141.756087	17.844647
36.965738	1138.812620	17.849664
36.892150	1139.663775	17.854682
37.098358	1137.801214	17.859699
36.899512	1136.958349	17.864717
37.078644	1133.793495	17.869735
37.128448	1132.365704	17.874752
36.881126	1140.906567	17.879770
37.615892	1152.433669	17.884787
37.220515	1160.767359	17.889805
37.231126	1149.729718	17.894823
37.534587	1147.122909	17.899840
37.044391	1141.913764	17.904858
37.581638	1146.610916	17.909875
37.609544	1142.945876	17.914893
36.918251	1144.057919	17.919911
37.498569	1147.183004	17.924928
37.198943	1153.923746	17.929946
37.719367	1151.159862	17.934963
37.743363	1156.600169	17.939981
37.410180	1161.512600	17.944999
37.768308	1151.913244	17.950016
37.352516	1163.822599	17.955034
37.248761	1151.786679	17.960051
37.292672	1155.507062	17.965069
37.210497	1152.765008	17.970087
37.435592	1178.642910	17.975104
37.593994	1176.475402	17.980122
37.856682	1181.335504	17.985139
38.004864	1183.549975	17.990157
37.686789	1180.298908	17.995175
37.850062	1176.738888	18.000192
37.860047	1178.943453	18.005210
37.482806	1182.477356	18.010227
38.021562	1180.518505	18.015245
38.053688	1191.322565	18.020263
38.500359	1192.407799	18.025280
38.544769	1195.986098	18.030298
38.840168	1186.598529	18.035315
38.190723	1175.945163	18.040333
38.267948	1174.055468	18.045351
38.618606	1168.266435	18.050368
38.406399	1166.308477	18.055386
38.338874	1176.657915	18.060403
38.732945	1178.461465	18.065421
38.445634	1199.105158	18.070439
38.683262	1193.497933	18.075456
38.532677	1192.047884	18.080474
38.467446	1188.817162	18.085491
38.780365	1184.640386	18.090509
38.466513	1190.067363	18.095527
38.607874	1188.369596	18.100544
38.400076	1192.366116	18.105562
38.427879	1184.626825	18.110579
38.976101	1180.441587	18.115597
39.005382	1184.732329	18.120615
39.388030	1179.197063	18.125632
39.096699	1187.968913	18.130650
39.191269	1184.362849	18.135667
39.275138	1187.171238	18.140685
38.954111	1190.248198	18.145703
39.121404	1190.212680	18.150720
39.261217	1187.328539	18.155738
39.068780	1186.295314	18.160755
39.516792	1177.423497	18.165773
39.031951	1177.979317	18.170791
39.312139	1186.383902	18.175808
39.360137	1200.770577	18.180826
39.600394	1206.820818	18.185843
39.603737	1203.039691	18.190861
39.521694	1199.817912	18.195879
39.632168	1190.525589	18.200896
39.605048	1185.793002	18.205914
39.218359	1208.001820	18.210931
39.695063	1198.484850	18.215949
39.752663	1209.297554	18.220967
39.956404	1209.376249	18.225984
40.017654	1213.532598	18.231002
39.680945	1209.861554	18.236019
40.030141	1199.506157	18.241037
39.880688	1209.278297	18.246055
40.058547	1204.169597	18.251072
39.968828	1210.946902	18.256090
39.686780	1203.934668	18.261107
39.821046	1208.076419	18.266125
39.862611	1200.432798	18.271143
39.925069	1196.178493	18.276160
40.041766	1204.627638	18.281178
39.951444	1201.050540	18.286195
39.915039	1200.541993	18.291213
40.096754	1203.994636	18.296231
40.117649	1193.797981	18.301248
40.391781	1215.814907	18.306266
40.274033	1220.412725	18.311283
40.587146	1230.626814	18.316301
40.421544	1224.524163	18.321319
40.421861	1227.863216	18.326336
40.605456	1231.195645	18.331354
40.474293	1225.797675	18.336371
40.586113	1222.163654	18.341389
40.464244	1232.862476	18.346407
40.215654	1226.375182	18.351424
40.327303	1232.290943	18.356442
40.231464	1234.392170	18.361459
40.638462	1238.825723	18.366477
40.777369	1254.028200	18.371495
41.108404	1245.742739	18.376512
40.798891	1249.764677	18.381530
41.228713	1250.303427	18.386547
41.129199	1247.122248	18.391565
41.367249	1250.310445	18.396583
41.272694	1238.067892	18.401600
41.309105	1240.946842	18.406618
41.181488	1257.358764	18.411635
41.459318	1251.858835	18.416653
41.142853	1250.513669	18.421671
41.114614	1240.526663	18.426688
41.646017	1237.877815	18.431706
41.324304	1238.250283	18.436723
41.466133	1234.122393	18.441741
41.276330	1240.448317	18.446759
41.564331	1236.871899	18.451776
41.761103	1236.547730	18.456794
41.443442	1239.093980	18.461811
41.573933	1238.799132	18.466829
41.529858	1255.772337	18.471847
41.703178	1239.618673	18.476864
41.507028	1238.298839	18.481882
41.533945	1238.111740	18.486899
41.281113	1236.466262	18.491917
41.738430	1249.245609	18.496935
41.534541	1253.553965	18.501952
41.817073	1263.485677	18.506970
41.552054	1262.233439	18.511987
41.959184	1264.909138	18.517005
41.832365	1262.596953	18.522023
42.009444	1256.055579	18.527040
42.218396	1270.123592	18.532058
42.310347	1282.250128	18.537075
42.489432	1274.051580	18.542093
42.365870	1268.223202	18.547111
42.607666	1260.283087	18.552128
42.604585	1262.925224	18.557146
42.416458	1262.472006	18.562163
42.320484	1258.204639	18.567181
42.470333	1253.239173	18.572199
42.571595	1263.230846	18.577216
42.521019	1258.306249	18.582234
42.584043	1264.911315	18.587251
42.888676	1282.672538	18.592269
42.856475	1274.611239	18.597287
42.619456	1267.885424	18.602304
42.843252	1261.475588	18.607322
42.945370	1278.962415	18.612339
42.940897	1276.681554	18.617357
42.699322	1267.933515	18.622375
43.037552	1274.381853	18.627392
43.384438	1268.445051	18.632410
43.185785	1265.490847	18.637427
42.999833	1258.116386	18.642445
42.906003	1262.407500	18.647463
42.913616	1270.211027	18.652480
43.549632	1262.821391	18.657498
43.120525	1277.784669	18.662515
43.086029	1272.816522	18.667533
43.250604	1282.719388	18.672551
43.198589	1275.106176	18.677568
43.970026	1275.215851	18.682586
43.003913	1272.883680	18.687603
43.224142	1274.891208	18.692621
43.249837	1276.080276	18.697639
42.846361	1276.396125	18.702656
43.423937	1284.182943	18.707674
43.589818	1299.397012	18.712691
43.556418	1290.736270	18.717709
43.862695	1299.004272	18.722727
43.502300	1303.936785	18.727744
43.975963	1294.738988	18.732762
43.924996	1310.936971	18.737779
43.858494	1293.971891	18.742797
43.636864	1295.433249	18.747815
43.733228	1303.017750	18.752832
43.993314	1299.609801	18.757850
43.657741	1303.929333	18.762867
43.972544	1315.269868	18.767885
44.004670	1318.581863	18.772903
44.202291	1328.126114	18.777920
44.462619	1328.732450	18.782938
44.217157	1326.899609	18.787955
44.669430	1320.018439	18.792973
44.429609	1319.535448	18.797991
44.636040	1327.090090	18.803008
44.843209	1319.038606	18.808026
44.212731	1326.292013	18.813043
44.502268	1321.150002	18.818061
44.437285	1316.776776	18.823079
44.670435	1329.774346	18.828096
45.430080	1317.937565	18.833114
44.723341	1326.976546	18.838131
44.890634	1317.530082	18.843149
44.936072	1311.132394	18.848167
44.881747	1310.064899	18.853184
44.936260	1315.494160	18.858202
44.718793	1317.191561	18.863219
44.916469	1314.209969	18.868237
45.267009	1313.602922	18.873255
44.841743	1318.523511	18.878272
45.061300	1321.238075	18.883290
44.771486	1314.113401	18.888307
45.025442	1325.536062	18.893325
45.094573	1326.996049	18.898343
45.293152	1339.550902	18.903360
45.631240	1326.808140	18.908378
45.384090	1340.123976	18.913395
45.308720	1339.394304	18.918413
45.435953	1334.915215	18.923431
45.505635	1335.699749	18.928448
45.468674	1328.166210	18.933466
45.459324	1338.209971	18.938483
45.615831	1330.851253	18.943501
45.777436	1334.922476	18.948519
45.700823	1336.250659	18.953536
45.758359	1325.571643	18.958554
45.723105	1334.107775	18.963571
45.652059	1336.293496	18.968589
46.062605	1342.430716	18.973607
45.841962	1348.764665	18.978624
46.079392	1351.706816	18.983642
46.066782	1357.563189	18.988659
46.122204	1356.251270	18.993677
46.535442	1348.227448	18.998695
46.431402	1360.302691	19.003712
46.608984	1351.905520	19.008730
46.646625	1345.688928	19.013747
46.336543	1330.920627	19.018765
46.470738	1333.500239	19.023783
46.323173	1329.423981	19.028800
46.384050	1339.254760	19.033818
46.348406	1350.713343	19.038835
46.239880	1358.484610	19.043853
46.514041	1357.766448	19.048871
46.322391	1358.569837	19.053888
46.521128	1341.692547	19.058906
46.335960	1358.224036	19.063923
46.390781	1360.039731	19.068941
46.745517	1366.248822	19.073959
47.049659	1371.945115	19.078976
47.260239	1370.564702	19.083994
46.985245	1383.039143	19.089011
47.086607	1376.134033	19.094029
47.279009	1364.648038	19.099047
47.072919	1373.561263	19.104064
47.238002	1359.116137	19.109082
47.003763	1373.585042	19.114099
46.928428	1374.711048	19.119117
47.236996	1371.983482	19.124135
47.772947	1371.618793	19.129152
47.767580	1373.052584	19.134170
47.271319	1377.782334	19.139187
47.591625	1373.632761	19.144205
47.531206	1368.479293	19.149223
47.631918	1371.010506	19.154240
47.460566	1366.332029	19.159258
47.560104	1373.351152	19.164275
47.747485	1367.840111	19.169293
47.947158	1367.079968	19.174311
47.941195	1365.850252	19.179328
47.680401	1367.052654	19.184346
47.621453	1376.084842	19.189363
47.501072	1383.586567	19.194381
48.114437	1382.771075	19.199399
47.903177	1382.539238	19.204416
48.103446	1383.584192	19.209434
48.106199	1388.475610	19.214451
48.219368	1390.717685	19.219469
48.546715	1399.039239	19.224487
48.278994	1386.684854	19.229504
48.225654	1386.857480	19.234522
47.835140	1384.996865	19.239539
47.944528	1393.728122	19.244557
48.681242	1386.455208	19.249575
48.601506	1404.090575	19.254592
48.627571	1406.466224	19.259610
48.958642	1402.415948	19.264627
48.750355	1395.164854	19.269645
48.506481	1388.645203	19.274663
48.470532	1394.290641	19.279680
48.570058	1408.830363	19.284698
48.900195	1411.357195	19.289715
49.075992	1405.036883	19.294733
49.317888	1412.115772	19.299751
48.804502	1408.904730	19.304768
49.072848	1422.392335	19.309786
48.862218	1411.692165	19.314803
49.408448	1408.122593	19.319821
49.373305	1414.509556	19.324839
49.165656	1416.259079	19.329856
49.145063	1419.453115	19.334874
48.851482	1411.713584	19.339891
49.057267	1412.647218	19.344909
49.498842	1410.056604	19.349927
49.270738	1412.891815	19.354944
49.325605	1419.327796	19.359962
49.566848	1434.350284	19.364979
49.351777	1434.671332	19.369997
49.544196	1436.216157	19.375015
49.720761	1436.068728	19.380032
49.648211	1437.831801	19.385050
49.721382	1435.709175	19.390067
49.619098	1436.132477	19.395085
49.866614	1428.548012	19.400103
49.854889	1436.916398	19.405120
50.028108	1440.676544	19.410138
50.051221	1437.608668	19.415155
50.001638	1452.320116	19.420173
50.242266	1451.017043	19.425191
50.217602	1454.003432	19.430208
50.224590	1461.772424	19.435226
50.374782	1451.422814	19.440243
50.315766	1460.376157	19.445261
50.580148	1446.038485	19.450279
50.768967	1447.504977	19.455296
50.439620	1444.059958	19.460314
50.594163	1448.561522	19.465331
50.393415	1446.140971	19.470349
50.714998	1450.581648	19.475367
50.786710	1458.015436	19.480384
50.694358	1460.842010	19.485402
50.924176	1448.614765	19.490419
50.620853	1444.294629	19.495437
50.781838	1438.481576	19.500455
51.114770	1446.347823	19.505472
50.755212	1447.439466	19.510490
50.855119	1450.513639	19.515507
50.987071	1465.509093	19.520525
51.447946	1456.657215	19.525543
51.056973	1471.330645	19.530560
51.025718	1457.736746	19.535578
50.817364	1467.530880	19.540595
50.911297	1465.853141	19.545613
51.031773	1456.694819	19.550631
51.373661	1470.417100	19.555648
51.209162	1490.565340	19.560666
51.626532	1488.003754	19.565683
51.545532	1484.611340	19.570701
52.078800	1487.497694	19.575719
52.071350	1491.383993	19.580736
51.895612	1477.481342	19.585754
52.147324	1478.852772	19.590771
52.280399	1474.902932	19.595789
52.260488	1476.733504	19.600807
52.075031	1482.484449	19.605824
51.926129	1478.932254	19.610842
52.050059	1473.358535	19.615859
52.193602	1477.378970	19.620877
52.398868	1466.083407	19.625895
52.365329	1475.897494	19.630912
52.380063	1476.741140	19.635930
52.243127	1467.455877	19.640947
52.012397	1469.114342	19.645965
52.362387	1471.988383	19.650983
52.491053	1471.075252	19.656000
52.722095	1477.815025	19.661018
52.735224	1478.015109	19.666035
52.473902	1475.976445	19.671053
52.475183	1474.821330	19.676071
52.515109	1473.884231	19.681088
52.420904	1478.273290	19.686106
52.803497	1467.761021	19.691123
52.680456	1487.426214	19.696141
52.770559	1483.773452	19.701159
52.850159	1495.132017	19.706176
52.859929	1501.622432	19.711194
53.104946	1492.188947	19.716211
52.856182	1504.646739	19.721229
52.951174	1495.498702	19.726247
52.879291	1498.924860	19.731264
52.864595	1503.172074	19.736282
53.197057	1505.774299	19.741299
53.397004	1523.104019	19.746317
53.636816	1512.093363	19.751335
53.752259	1513.432495	19.756352
53.687106	1517.744425	19.761370
53.898374	1513.075392	19.766387
53.904025	1516.240086	19.771405
54.309735	1514.526118	19.776423
54.082333	1508.237382	19.781440
53.780778	1512.791487	19.786458
53.897802	1512.681790	19.791475
54.181485	1510.497769	19.796493
54.233671	1506.453293	19.801511
54.228922	1514.359853	19.806528
53.995510	1518.805448	19.811546
54.062328	1501.986548	19.816563
54.156489	1512.487580	19.821581
54.330187	1502.879062	19.826599
54.171497	1507.123590	19.831616
54.022355	1505.547051	19.836634
54.117496	1501.669423	19.841651
54.204608	1505.070672	19.846669
54.216816	1511.608049	19.851687
54.583041	1513.068842	19.856704
54.193060	1530.027073	19.861722
54.495774	1525.968588	19.866739
54.663432	1537.433310	19.871757
54.680318	1529.263214	19.876775
54.543246	1539.945666	19.881792
54.551201	1538.287703	19.886810
55.095298	1546.938302	19.891827
54.819711	1558.008558	19.896845
55.131267	1556.609154	19.901863
55.151357	1550.808672	19.906880
55.148533	1561.287057	19.911898
55.303854	1557.387365	19.916915
55.375141	1550.900330	19.921933
55.538630	1556.359930	19.926951
55.230596	1552.883147	19.931968
55.540677	1560.001907	19.936986
55.460285	1548.324994	19.942003
55.364959	1548.529447	19.947021
55.443629	1553.828759	19.952039
55.509555	1555.279799	19.957056
55.530848	1555.210348	19.962074
55.888663	1561.504236	19.967091
56.115404	1568.718112	19.972109
55.889588	1555.826842	19.977127
56.043925	1557.535443	19.982144
55.942281	1569.948139	19.987162
56.186908	1564.301830	19.992179
55.943134	1571.267517	19.997197
55.773415	1570.587334	20.002215
56.266369	1573.612570	20.007232
55.762670	1573.262437	20.012250
56.169685	1563.806689	20.017267
55.589623	1573.577063	20.022285
56.086817	1577.116057	20.027303
56.214254	1587.659259	20.032320
56.171040	1609.114135	20.037338
56.536031	1593.349865	20.042355
56.496843	1598.187948	20.047373
56.538607	1595.505306	20.052391
56.773331	1596.390233	20.057408
56.757109	1589.771720	20.062426
57.190708	1603.593351	20.067443
57.154334	1594.453220	20.072461
57.392899	1597.294244	20.077479
57.291693	1586.131834	20.082496
57.154796	1585.970397	20.087514
57.439034	1578.616813	20.092531
57.273438	1579.965267	20.097549
57.308466	1581.761994	20.102567
57.541386	1574.479572	20.107584
57.309388	1578.230648	20.112602
57.601325	1580.747710	20.117619
57.473176	1574.007878	20.122637
57.594313	1583.665240	20.127655
57.940447	1582.708564	20.132672
58.029252	1598.787074	20.137690
57.797098	1588.503602	20.142707
57.730518	1591.382965	20.147725
57.730224	1601.084610	20.152743
58.156244	1606.730323	20.157760
57.837869	1610.864188	20.162778
58.150612	1605.601690	20.167795
58.256793	1607.699713	20.172813
58.338481	1609.104104	20.177831
58.162905	1605.574998	20.182848
58.081975	1609.958853	20.187866
58.015581	1600.261661	20.192883
58.190964	1602.279409	20.197901
58.243976	1589.947218	20.202919
58.337067	1600.666232	20.207936
58.243721	1602.047551	20.212954
58.751791	1608.257951	20.217971
58.784736	1619.358804	20.222989
58.808774	1628.788394	20.228007
59.013632	1626.673517	20.233024
58.794039	1631.091726	20.238042
58.770065	1627.128587	20.243059
59.240713	1627.888184	20.248077
59.025807	1623.147032	20.253095
59.065511	1629.295115	20.258112
58.979305	1628.172632	20.263130
59.033531	1627.974938	20.268147
59.045929	1613.578777	20.273165
58.880682	1619.579078	20.278183
59.372281	1612.483341	20.283200
59.321311	1621.186182	20.288218
59.087008	1626.332569	20.293235
59.555852	1634.127109	20.298253
59.511237	1641.254135	20.303271
59.432347	1643.056092	20.308288
59.488274	1637.316243	20.313306
59.794007	1639.439812	20.318323
59.689980	1646.765506	20.323341
59.683034	1644.074709	20.328359
59.870430	1644.124408	20.333376
59.855710	1646.490699	20.338394
60.406987	1643.595671	20.343411
60.472122	1637.210560	20.348429
59.877136	1644.041944	20.353447
60.108434	1643.223184	20.358464
59.808429	1647.653996	20.363482
59.920214	1657.174000	20.368499
60.352828	1666.129319	20.373517
60.327137	1676.305224	20.378535
60.556415	1666.037779	20.383552
60.322160	1669.798696	20.388570
60.857019	1665.053677	20.393587
60.873292	1661.320922	20.398605
60.635531	1669.526005	20.403623
61.043623	1669.500099	20.408640
60.959316	1672.499024	20.413658
60.598735	1661.683334	20.418675
61.113541	1662.142509	20.423693
61.062925	1669.706011	20.428711
61.009761	1675.515190	20.433728
60.874289	1686.415241	20.438746
60.943410	1686.193121	20.443763
61.482616	1688.602026	20.448781
61.210107	1686.429383	20.453799
61.529765	1683.406526	20.458816
61.365683	1688.573488	20.463834
61.519878	1685.863749	20.468851
61.559105	1678.406493	20.473869
61.455872	1684.356071	20.478887
61.546506	1690.142726	20.483904
61.605279	1701.836064	20.488922
61.745285	1708.018954	20.493939
61.866520	1703.351354	20.498957
61.828575	1708.485935	20.503975
62.174118	1696.521273	20.508992
61.975037	1707.017868	20.514010
62.172546	1703.117846	20.519027
62.532213	1713.012477	20.524045
62.170513	1702.929126	20.529063
62.295115	1707.586934	20.534080
62.335392	1702.313445	20.539098
62.420206	1706.677668	20.544115
62.529930	1716.040228	20.549133
62.472569	1729.601187	20.554151
63.042597	1727.975071	20.559168
62.855059	1730.156999	20.564186
62.823270	1725.122026	20.569203
62.866041	1730.704741	20.574221
62.790843	1728.974577	20.579239
63.223824	1721.364088	20.584256
62.900268	1723.639913	20.589274
62.975370	1725.802783	20.594291
63.444498	1724.053612	20.599309
63.274411	1717.673767	20.604327
63.395248	1721.726218	20.609344
63.330752	1726.644045	20.614362
63.215377	1719.188903	20.619379
63.421074	1727.393964	20.624397
63.147928	1732.060444	20.629415
63.468112	1724.350854	20.634432
63.526287	1739.168739	20.639450
63.644199	1740.722109	20.644467
63.934553	1738.928359	20.649485
63.763902	1743.951190	20.654503
63.975950	1744.596666	20.659520
63.913881	1746.159299	20.664538
63.995089	1748.958725	20.669555
63.967710	1742.808991	20.674573
63.968677	1747.419904	20.679591
63.730660	1746.920837	20.684608
64.146726	1741.023538	20.689626
63.958492	1743.527487	20.694643
64.222690	1751.433042	20.699661
64.363753	1762.144637	20.704679
64.823865	1761.091194	20.709696
64.725342	1754.192008	20.714714
64.545498	1757.471019	20.719731
64.736119	1751.078831	20.724749
64.638512	1758.406721	20.729767
64.532996	1762.709254	20.734784
64.558030	1761.370507	20.739802
64.302376	1755.029302	20.744819
64.705978	1769.565860	20.749837
65.081170	1776.257914	20.754855
65.071691	1781.631067	20.759872
64.887372	1784.011325	20.764890
65.237171	1786.456231	20.769907
65.335906	1778.828654	20.774925
65.238419	1786.557349	20.779943
65.110169	1790.289058	20.784960
65.968989	1796.103723	20.789978
66.065744	1809.779461	20.794995
65.830987	1800.187439	20.800013
65.484486	1798.023219	20.805031
66.089595	1796.700889	20.810048
66.575675	1799.181253	20.815066
66.012056	1781.356264	20.820083
66.223915	1768.894915	20.825101
66.259759	1768.204608	20.830119
66.296714	1773.857680	20.835136
66.692244	1768.358088	20.840154
66.236961	1762.770881	20.845171
66.279496	1761.760771	20.850189
66.230043	1775.348930	20.855207
66.315274	1784.664867	20.860224
66.878600	1786.615543	20.865242
66.828336	1789.833230	20.870259
67.042499	1786.681709	20.875277
66.925676	1780.618563	20.880295
66.584206	1782.950855	20.885312
67.311801	1782.704467	20.890330
67.074055	1777.799583	20.895347
67.249166	1782.733537	20.900365
66.806432	1779.666001	20.905383
66.734569	1781.542615	20.910400
66.716541	1787.526218	20.915418
66.614935	1780.580164	20.920435
67.252699	1789.973647	20.925453
67.395281	1804.933006	20.930471
67.592936	1809.102838	20.935488
67.687660	1802.432148	20.940506
67.571247	1806.897355	20.945523
67.628388	1798.089630	20.950541
67.539540	1806.312471	20.955559
67.466544	1798.677076	20.960576
67.576617	1802.421944	20.965594
67.674910	1813.452715	20.970611
67.875837	1807.866829	20.975629
68.232002	1819.220141	20.980647
67.976849	1826.001506	20.985664
68.337714	1819.386948	20.990682
68.457653	1829.738952	20.995699
68.488139	1824.135581	21.000717
68.402249	1816.375958	21.005735
68.320594	1824.559809	21.010752
68.702085	1823.805878	21.015770
68.178234	1823.436804	21.020787
68.303735	1816.240546	21.025805
68.359414	1814.212140	21.030823
68.636920	1820.569199	21.035840
68.845192	1824.065143	21.040858
68.849218	1836.048030	21.045875
68.835154	1838.815058	21.050893
69.029456	1839.630586	21.055911
68.995720	1845.979610	21.060928
68.983807	1837.163748	21.065946
69.363096	1843.814158	21.070963
68.705165	1844.359241	21.075981
69.115191	1848.423221	21.080999
69.467539	1855.207253	21.086016
69.895996	1863.311199	21.091034
69.429670	1870.371835	21.096051
69.527650	1864.685288	21.101069
69.600654	1868.050945	21.106087
69.375980	1867.404607	21.111104
70.329208	1857.891531	21.116122
69.473654	1869.945996	21.121139
69.543583	1865.756638	21.126157
69.851646	1885.736603	21.131175
70.028443	1889.442632	21.136192
70.146502	1885.570799	21.141210
70.163158	1889.425002	21.146227
70.302940	1896.068772	21.151245
70.261282	1886.354925	21.156263
70.269859	1885.810907	21.161280
70.649854	1896.835465	21.166298
70.538248	1904.746316	21.171315
70.438273	1914.662577	21.176333
70.619314	1914.164126	21.181351
70.622583	1915.669196	21.186368
70.915618	1909.604913	21.191386
70.923205	1909.755373	21.196403
70.997165	1903.930557	21.201421
71.220528	1916.863812	21.206439
71.327782	1923.468504	21.211456
71.862801	1920.389774	21.216474
71.338031	1918.843645	21.221491
71.498870	1910.997984	21.226509
71.729183	1914.746130	21.231527
71.642825	1930.189618	21.236544
71.898518	1921.723134	21.241562
71.662104	1922.066469	21.246579
71.817372	1924.936376	21.251597
72.049263	1919.317200	21.256615
71.922303	1925.813411	21.261632
72.125056	1922.581598	21.266650
71.896956	1924.927705	21.271667
71.872813	1924.937960	21.276685
72.042469	1918.091374	21.281703
71.911619	1915.877572	21.286720
72.317493	1917.979173	21.291738
72.407193	1934.209334	21.296755
72.246717	1947.777146	21.301773
72.572314	1946.403918	21.306791
72.709466	1951.242873	21.311808
72.217783	1945.405672	21.316826
72.621868	1939.093590	21.321843
72.330150	1938.905909	21.326861
73.109220	1939.610888	21.331879
72.933805	1943.012323	21.336896
72.989400	1943.508738	21.341914
73.029000	1961.006027	21.346931
72.886199	1969.631900	21.351949
73.303438	1971.921089	21.356967
73.200746	1972.492801	21.361984
73.336996	1966.718169	21.367002
73.160591	1966.316747	21.372019
73.106146	1973.183494	21.377037
73.604245	1976.712960	21.382055
73.645953	1985.284684	21.387072
74.063538	1992.023831	21.392090
74.170104	1987.800300	21.397107
74.021745	1978.844789	21.402125
73.833514	1978.965965	21.407143
74.234835	1982.472722	21.412160
74.190632	1981.059593	21.417178
74.230490	1984.550394	21.422195
74.436275	1984.682427	21.427213
74.241808	1977.574108	21.432231
74.401179	1983.163882	21.437248
74.430445	1977.431257	21.442266
74.417357	1975.246337	21.447283
74.352672	1976.465393	21.452301
74.554557	1980.113857	21.457319
74.782106	1997.319784	21.462336
75.037060	1996.977020	21.467354
74.845548	2004.086176	21.472371
74.573268	2008.058263	21.477389
75.058924	1998.151278	21.482407
74.949686	2009.457699	21.487424
75.102049	2008.506112	21.492442
75.359384	2026.101905	21.497459
75.374400	2024.670026	21.502477
75.457600	2022.211220	21.507495
75.406654	2033.211855	21.512512
75.588143	2026.903057	21.517530
75.741727	2031.647934	21.522547
75.591178	2028.140071	21.527565
76.077866	2008.250361	21.532583
75.973028	2023.605299	21.537600
75.983738	2015.155062	21.542618
75.966302	2031.515714	21.547635
75.868272	2032.184534	21.552653
76.323814	2042.894366	21.557671
76.359853	2042.888880	21.562688
76.281048	2041.509572	21.567706
76.073515	2043.186547	21.572723
76.275264	2045.610501	21.577741
76.765690	2045.871521	21.582759
76.888347	2045.874556	21.587776
76.841352	2054.113046	21.592794
76.914572	2057.693316	21.597811
77.130851	2067.465431	21.602829
77.210574	2053.329789	21.607847
77.368730	2060.068579	21.612864
77.566991	2055.767545	21.617882
77.606562	2049.768175	21.622899
76.971158	2045.250593	21.627917
77.553864	2038.695879	21.632935
77.309601	2048.729502	21.637952
77.400819	2045.439397	21.642970
77.594036	2054.650186	21.647987
77.432484	2060.085122	21.653005
77.968818	2043.914887	21.658023
77.794511	2054.300497	21.663040
77.951752	2047.238040	21.668058
77.921752	2044.184694	21.673075
77.703025	2041.691131	21.678093
78.004161	2051.781328	21.683111
77.928462	2066.459500	21.688128
78.200143	2068.219198	21.693146
78.309298	2071.670755	21.698163
78.268462	2069.518576	21.703181
78.682383	2065.830741	21.708199
78.242304	2068.323696	21.713216
78.571924	2073.271396	21.718234
78.608147	2073.969680	21.723251
78.357159	2083.745580	21.728269
78.864272	2086.191130	21.733287
79.213834	2098.583996	21.738304
79.122225	2091.544730	21.743322
78.983432	2098.784530	21.748339
78.849741	2101.387289	21.753357
79.131678	2086.490890	21.758375
78.849509	2097.168002	21.763392
79.025928	2111.497416	21.768410
79.443677	2116.216708	21.773427
79.660086	2122.094259	21.778445
79.963154	2112.051703	21.783463
80.067560	2119.862527	21.788480
79.981539	2113.425184	21.793498
80.346396	2114.504361	21.798515
80.215103	2121.733527	21.803533
80.187943	2113.213432	21.808551
80.316876	2121.440170	21.813568
80.368586	2110.439682	21.818586
80.100698	2114.177555	21.823603
80.285964	2111.030505	21.828621
80.383378	2107.556366	21.833639
80.480734	2121.759310	21.838656
80.251480	2126.608378	21.843674
80.784120	2127.907441	21.848691
80.921126	2139.475190	21.853709
80.762378	2132.228658	21.858727
80.925579	2131.666719	21.863744
80.973215	2135.238388	21.868762
80.980238	2127.094814	21.873779
81.024606	2132.061973	21.878797
81.346422	2139.134942	21.883815
81.374597	2153.361374	21.888832
81.104592	2152.337088	21.893850
81.411381	2151.774744	21.898867
81.664662	2153.938154	21.903885
81.970507	2151.624343	21.908903
81.802522	2145.502812	21.913920
81.914993	2153.889947	21.918938
81.957449	2150.689519	21.923955
82.128555	2153.380242	21.928973
82.261614	2161.066665	21.933991
82.418610	2163.494491	21.939008
82.222887	2173.659446	21.944026
82.534671	2170.606182	21.949043
82.529077	2171.421484	21.954061
82.658776	2168.696575	21.959079
82.639142	2165.038775	21.964096
82.392530	2174.403750	21.969114
82.779715	2165.313742	21.974131
82.793702	2167.227443	21.979149
82.669550	2171.305756	21.984167
82.996410	2168.297472	21.989184
82.899736	2173.955826	21.994202
83.427146	2176.092071	21.999219
82.971332	2196.756999	22.004237
83.440510	2187.508954	22.009255
83.442270	2185.608885	22.014272
83.326530	2188.066821	22.019290
83.576110	2194.639846	22.024307
83.439318	2189.946269	22.029325
83.479857	2183.085095	22.034343
83.656834	2187.100452	22.039360
83.489058	2190.409212	22.044378
83.657491	2200.160491	22.049395
83.468678	2212.350583	22.054413
83.982099	2208.631351	22.059431
84.068462	2220.412231	22.064448
83.642649	2215.549316	22.069466
84.078324	2225.555410	22.074483
84.202993	2235.891128	22.079501
84.238709	2237.176529	22.084519
84.309363	2233.046938	22.089536
84.453299	2242.325511	22.094554
84.958599	2258.708621	22.099571
84.940745	2268.195609	22.104589
85.262659	2260.738006	22.109607
85.108222	2259.638798	22.114624
85.160586	2258.895387	22.119642
85.165154	2249.237222	22.124659
85.245259	2248.691455	22.129677
85.503927	2252.084905	22.134695
85.791256	2248.909216	22.139712
85.333686	2254.658855	22.144730
85.922117	2247.411989	22.149747
85.329801	2257.528663	22.154765
85.422350	2267.430736	22.159783
85.853112	2273.779727	22.164800
85.600136	2278.089705	22.169818
85.981984	2270.477529	22.174835
85.997080	2278.311883	22.179853
86.369222	2288.185943	22.184871
86.646353	2298.343162	22.189888
86.589831	2300.574065	22.194906
86.875318	2290.379516	22.199923
86.789754	2300.154864	22.204941
86.549507	2290.995822	22.209959
86.834539	2289.206009	22.214976
87.021899	2298.159043	22.219994
87.129225	2294.998924	22.225011
87.165119	2303.211917	22.230029
87.170733	2304.309517	22.235047
86.981228	2294.962627	22.240064
87.341921	2296.471696	22.245082
87.245737	2290.865932	22.250099
87.142026	2292.176338	22.255117
87.563165	2305.571238	22.260135
87.997557	2307.239191	22.265152
87.469770	2315.281704	22.270170
88.114324	2315.730040	22.275187
87.625272	2318.685178	22.280205
87.763129	2311.000748	22.285223
87.836125	2307.543021	22.290240
87.485501	2323.182898	22.295258
87.990706	2330.350298	22.300275
88.397549	2336.791430	22.305293
88.363064	2340.136143	22.310311
88.452369	2329.972308	22.315328
88.545182	2342.348760	22.320346
88.708432	2334.420478	22.325363
88.594963	2348.606135	22.330381
89.296059	2355.692357	22.335399
89.170526	2370.877249	22.340416
89.223277	2372.788055	22.345434
89.033809	2361.648457	22.350451
89.361756	2362.484101	22.355469
89.316914	2362.554409	22.360487
89.693982	2362.375561	22.365504
89.501838	2361.086576	22.370522
89.537920	2359.499877	22.375539
89.604552	2354.424058	22.380557
89.571885	2356.057884	22.385575
89.526251	2352.359933	22.390592
89.802134	2359.882041	22.395610
89.602762	2353.345594	22.400627
89.841774	2365.863274	22.405645
89.828336	2383.224104	22.410663
89.763042	2369.161431	22.415680
89.790095	2376.851931	22.420698
89.870224	2385.686096	22.425715
89.782333	2402.253802	22.430733
90.123676	2403.497644	22.435751
90.622076	2418.505919	22.440768
90.565798	2424.530444	22.445786
91.056307	2424.056085	22.450803
91.151479	2422.722080	22.455821
91.193208	2429.116297	22.460839
91.487005	2425.444055	22.465856
91.180592	2429.746661	22.470874
91.173719	2429.479629	22.475891
91.207651	2435.619424	22.480909
91.098230	2440.850628	22.485927
91.402381	2443.239657	22.490944
91.415059	2442.846472	22.495962
91.663338	2445.831292	22.500979
91.905741	2441.936703	22.505997
92.084017	2436.515133	22.511015
92.209564	2445.531579	22.516032
92.286415	2465.422172	22.521050
92.559649	2459.831068	22.526067
92.802753	2460.960904	22.531085
93.337690	2462.660461	22.536103
93.085759	2438.947163	22.541120
92.493027	2445.570190	22.546138
92.672453	2433.353327	22.551155
92.751979	2444.251713	22.556173
92.914559	2455.446394	22.561191
93.185813	2446.964602	22.566208
92.988685	2446.639005	22.571226
92.926948	2443.877769	22.576243
93.142450	2448.600432	22.581261
93.182747	2450.364860	22.586279
93.436927	2456.971979	22.591296
93.216572	2471.404875	22.596314
93.394960	2470.685896	22.601331
93.705793	2473.638828	22.606349
93.289321	2471.469705	22.611367
93.868568	2480.497145	22.616384
93.872932	2489.665156	22.621402
94.020115	2502.528711	22.626419
94.035581	2501.699544	22.631437
93.907653	2501.965925	22.636455
94.476920	2497.761310	22.641472
94.439948	2505.433490	22.646490
94.644832	2510.836400	22.651507
94.740338	2521.044294	22.656525
94.855180	2520.635102	22.661543
95.198575	2524.217322	22.666560
94.986448	2526.046554	22.671578
94.976369	2519.767598	22.676595
95.149528	2529.297388	22.681613
95.252461	2522.082291	22.686631
95.487601	2516.872717	22.691648
95.128023	2516.771407	22.696666
95.071597	2524.803286	22.701683
95.380540	2526.614004	22.706701
95.272946	2535.897419	22.711719
95.652383	2535.071192	22.716736
95.449702	2545.420502	22.721754
95.580124	2552.189071	22.726771
96.077651	2558.691823	22.731789
95.986328	2575.692617	22.736807
96.161119	2568.895478	22.741824
95.812106	2566.722087	22.746842
96.113366	2570.623375	22.751859
96.488960	2569.564195	22.756877
96.322451	2590.234745	22.761895
96.724498	2586.599166	22.766912
96.878145	2584.826753	22.771930
97.042322	2588.979920	22.776947
96.934116	2587.917633	22.781965
96.733120	2591.039146	22.786983
96.986238	2590.785032	22.792000
97.340145	2618.538521	22.797018
97.271660	2614.064529	22.802035
97.607794	2609.047412	22.807053
97.593803	2610.163883	22.812071
97.750673	2606.872857	22.817088
97.796654	2605.196214	22.822106
98.107318	2613.426267	22.827123
97.912326	2610.960467	22.832141
98.060004	2608.706097	22.837159
98.458163	2621.419951	22.842176
98.400572	2631.566678	22.847194
98.565409	2633.115931	22.852211
98.399155	2628.430010	22.857229
98.490946	2628.510474	22.862247
98.750220	2625.585295	22.867264
98.687103	2624.080394	22.872282
98.260438	2625.570823	22.877299
98.631364	2634.283803	22.882317
98.791918	2652.109992	22.887335
98.976091	2647.542753	22.892352
98.875843	2653.479559	22.897370
99.078490	2669.575911	22.902387
99.569886	2666.298744	22.907405
99.339919	2665.889916	22.912423
99.747567	2669.054955	22.917440
99.867842	2675.348581	22.922458
99.630163	2678.583165	22.927475
100.259521	2670.310281	22.932493
99.842016	2680.885850	22.937511
100.327285	2689.653534	22.942528
100.413731	2691.858930	22.947546
100.665586	2691.781758	22.952563
100.983855	2693.164951	22.957581
100.697001	2698.370373	22.962599
100.720878	2689.930380	22.967616
101.279987	2684.234452	22.972634
101.322036	2685.926038	22.977651
101.294373	2682.689159	22.982669
100.755551	2681.246158	22.987687
101.174479	2682.417897	22.992704
101.014121	2686.710305	22.997722
101.222898	2687.337393	23.002739
101.297546	2688.294799	23.007757
101.463116	2704.447490	23.012775
101.646662	2698.996612	23.017792
101.555352	2702.047303	23.022810
101.451442	2696.243785	23.027827
101.766378	2702.797290	23.032845
101.815425	2710.194120	23.037863
101.736902	2717.440506	23.042880
101.694601	2720.136345	23.047898
101.856911	2725.246154	23.052915
102.350833	2746.914915	23.057933
102.245183	2755.942489	23.062951
102.423503	2751.521324	23.067968
102.572652	2753.186668	23.072986
102.606832	2747.269969	23.078003
103.068971	2763.332064	23.083021
103.264638	2770.478702	23.088039
103.146837	2776.822289	23.093056
103.487754	2775.108890	23.098074
103.254547	2775.173993	23.103091
103.456911	2775.568532	23.108109
103.214799	2781.019462	23.113127
103.654680	2775.206470	23.118144
104.142135	2781.976001	23.123162
103.855050	2788.062057	23.128179
103.987683	2785.494405	23.133197
103.991466	2800.965547	23.138215
104.161631	2801.507160	23.143232
104.503293	2796.807899	23.148250
104.140165	2801.201538	23.153267
104.456507	2794.669350	23.158285
104.201253	2792.563301	23.163303
104.540982	2805.867177	23.168320
104.722994	2819.981662	23.173338
104.759969	2818.543123	23.178355
104.955332	2812.809459	23.183373
104.913178	2815.637848	23.188391
105.159848	2826.586028	23.193408
105.664765	2833.778927	23.198426
105.381579	2842.341995	23.203443
105.800985	2832.940455	23.208461
105.979665	2831.018912	23.213479
105.854044	2838.433691	23.218496
106.070401	2828.196014	23.223514
105.828003	2833.571256	23.228531
106.194252	2829.392061	23.233549
106.508400	2852.528334	23.238567
106.191119	2849.819697	23.243584
106.279371	2847.991224	23.248602
106.119506	2853.214669	23.253619
106.787025	2855.190176	23.258637
106.951494	2855.776869	23.263655
107.044123	2858.044440	23.268672
107.097247	2861.359743	23.273690
106.889344	2859.426171	23.278707
107.017462	2863.963795	23.283725
107.358393	2875.730471	23.288743
106.919608	2877.219662	23.293760
107.256396	2872.211838	23.298778
107.469306	2881.079100	23.303795
107.908916	2882.894632	23.308813
107.929769	2891.425870	23.313831
107.845407	2899.421262	23.318848
107.988948	2893.462133	23.323866
108.248789	2894.996524	23.328883
107.985334	2888.507796	23.333901
108.318703	2885.416314	23.338919
108.069615	2891.957257	23.343936
108.969340	2899.656442	23.348954
108.814313	2907.195792	23.353971
109.417517	2902.670149	23.358989
109.343256	2908.454626	23.364007
109.509218	2890.851937	23.369024
109.316864	2890.370930	23.374042
108.940304	2885.414897	23.379059
109.305235	2894.592904	23.384077
109.616879	2904.113821	23.389095
109.587792	2901.366336	23.394112
109.248441	2908.947189	23.399130
109.726063	2916.134930	23.404147
109.626333	2912.457964	23.409165
109.377455	2911.509227	23.414183
109.838134	2921.312955	23.419200
110.018310	2929.686689	23.424218
110.131986	2930.555932	23.429235
110.417298	2936.628109	23.434253
110.390079	2938.068606	23.439271
109.972198	2935.647149	23.444288
110.536690	2950.080557	23.449306
110.665728	2957.711140	23.454323
110.478066	2961.550241	23.459341
110.954750	2961.624061	23.464359
110.462305	2968.253657	23.469376
110.904360	2982.112906	23.474394
111.234144	2987.913011	23.479411
111.389909	2977.214468	23.484429
111.400780	2991.362213	23.489447
111.547394	3004.106280	23.494464
111.911961	3005.668461	23.499482
111.894566	3014.663400	23.504499
111.687253	3012.824405	23.509517
112.204690	3012.358440	23.514535
112.411111	3027.147850	23.519552
112.331379	3028.022149	23.524570
112.802808	3034.974191	23.529587
112.691284	3017.613694	23.534605
112.805362	3029.677978	23.539623
113.019182	3030.954470	23.544640
112.884971	3020.200333	23.549658
113.263839	3030.218936	23.554675
113.230080	3021.822536	23.559693
113.344331	3015.978423	23.564711
113.752538	3033.718847	23.569728
113.649160	3039.261743	23.574746
113.414652	3043.616352	23.579763
113.899914	3040.898730	23.584781
113.774164	3043.636097	23.589799
113.653336	3043.598376	23.594816
113.713758	3042.604329	23.599834
113.752642	3052.130184	23.604851
114.231482	3053.904870	23.609869
114.237838	3057.805125	23.614887
114.156896	3070.521766	23.619904
114.580125	3079.640235	23.624922
114.343143	3089.799544	23.629939
114.931270	3092.971102	23.634957
114.762380	3083.462759	23.639975
114.513684	3095.202019	23.644992
115.383225	3104.212702	23.650010
115.258801	3119.716829	23.655027
115.248979	3113.778499	23.660045
115.599973	3109.945660	23.665063
115.164129	3114.726358	23.670080
115.701052	3116.002735	23.675098
115.783148	3133.990036	23.680115
115.896677	3142.443749	23.685133
116.268913	3137.038926	23.690151
115.941535	3135.644820	23.695168
116.374210	3143.657160	23.700186
116.377888	3153.769331	23.705203
116.690579	3157.792051	23.710221
116.815296	3147.940988	23.715239
116.585015	3157.329162	23.720256
116.780502	3149.657441	23.725274
116.828661	3153.270262	23.730291
116.916609	3154.629608	23.735309
117.444859	3161.695891	23.740327
117.516034	3175.395614	23.745344
117.558730	3166.160234	23.750362
117.677600	3172.072349	23.755379
117.789392	3175.649955	23.760397
117.821741	3166.119509	23.765415
117.383435	3170.673358	23.770432
118.228815	3170.629448	23.775450
117.876566	3188.340822	23.780467
118.318076	3189.616372	23.785485
118.253075	3192.722993	23.790503
118.275813	3195.345588	23.795520
118.649791	3191.606974	23.800538
118.619738	3203.211050	23.805555
118.572333	3225.530166	23.810573
118.694855	3220.499004	23.815591
118.683060	3220.863982	23.820608
118.834948	3230.567914	23.825626
118.929058	3244.450315	23.830643
119.335269	3250.999190	23.835661
119.616166	3238.939479	23.840679
119.836004	3254.112036	23.845696
120.121647	3257.836016	23.850714
120.530739	3265.482822	23.855731
120.001120	3261.162978	23.860749
120.146335	3256.156657	23.865767
120.332036	3262.067800	23.870784
120.869529	3259.449277	23.875802
121.151659	3244.927488	23.880819
120.666567	3254.576572	23.885837
121.184082	3248.221016	23.890855
120.942630	3246.740846	23.895872
121.160978	3258.040914	23.900890
121.613766	3270.831890	23.905907
121.807455	3264.195655	23.910925
121.802048	3264.420757	23.915943
121.723686	3272.614219	23.920960
121.704276	3268.072406	23.925978
122.075030	3274.863564	23.930995
121.651123	3275.447765	23.936013
122.127117	3264.531600	23.941031
122.290780	3268.685006	23.946048
122.177060	3263.416250	23.951066
122.307356	3267.903134	23.956083
122.569392	3281.364723	23.961101
122.453017	3289.330584	23.966119
122.629916	3286.288799	23.971136
122.900720	3284.570558	23.976154
123.094657	3291.793426	23.981171
123.060709	3311.828563	23.986189
123.171458	3313.642007	23.991207
122.838405	3317.576556	23.996224
123.212515	3313.377082	24.001242
123.562225	3329.703487	24.006259
123.683265	3333.854117	24.011277
123.795877	3332.157499	24.016295
123.536098	3335.408286	24.021312
124.106255	3341.805258	24.026330
123.924919	3351.817120	24.031347
124.005107	3356.491784	24.036365
124.336315	3361.202874	24.041383
124.417678	3363.529087	24.046400
124.601111	3365.842466	24.051418
124.799316	3374.598649	24.056435
124.646434	3387.247877	24.061453
125.036393	3382.843902	24.066471
124.955937	3376.373671	24.071488
124.939844	3377.619926	24.076506
125.474637	3392.421316	24.081523
125.410929	3401.935022	24.086541
125.795602	3396.966897	24.091559
125.828851	3405.130307	24.096576
125.556533	3401.110996	24.101594
126.273240	3410.013215	24.106611
126.198587	3418.067284	24.111629
126.720354	3419.516499	24.116647
126.558730	3431.652653	24.121664
126.772956	3432.146350	24.126682
126.687175	3416.618396	24.131699
126.738528	3423.488057	24.136717
126.799338	3409.944540	24.141735
126.785819	3421.467258	24.146752
127.042157	3435.412767	24.151770
127.654205	3436.017735	24.156787
126.925142	3449.271750	24.161805
127.480759	3437.001585	24.166823
127.510562	3455.912724	24.171840
127.507534	3458.233233	24.176858
127.885911	3468.220595	24.181875
127.651738	3465.874441	24.186893
128.334043	3479.765874	24.191911
128.541265	3483.562157	24.196928
128.681475	3485.793947	24.201946
128.722013	3489.660533	24.206963
128.803364	3489.442789	24.211981
129.223358	3493.316210	24.216999
129.188513	3486.655728	24.222016
129.213393	3489.495815	24.227034
129.695058	3496.405402	24.232051
129.455006	3503.671097	24.237069
129.798145	3509.387217	24.242087
129.718216	3510.854954	24.247104
129.923652	3509.658254	24.252122
129.962790	3499.618404	24.257139
129.811734	3506.466151	24.262157
129.829680	3502.395028	24.267175
130.391953	3519.884542	24.272192
130.336105	3527.597990	24.277210
130.658628	3528.923770	24.282227
130.515168	3541.353844	24.287245
130.727974	3536.128540	24.292263
130.706563	3552.724763	24.297280
130.656707	3566.446902	24.302298
131.201486	3554.882212	24.307315
130.934073	3559.030627	24.312333
131.191144	3578.376578	24.317351
131.761648	3579.196377	24.322368
130.981948	3581.881619	24.327386
131.666395	3598.364141	24.332403
131.736319	3602.797442	24.337421
132.036167	3602.993662	24.342439
132.204431	3605.457795	24.347456
132.277011	3610.360973	24.352474
132.695860	3621.036469	24.357491
132.800183	3630.145211	24.362509
132.781549	3628.118776	24.367527
132.983946	3630.006271	24.372544
132.905677	3623.011660	24.377562
133.082928	3622.283347	24.382579
133.391198	3631.988246	24.387597
133.721733	3632.507917	24.392615
133.803777	3644.833293	24.397632
133.702684	3642.570425	24.402650
134.045780	3637.248929	24.407667
133.817055	3643.483944	24.412685
134.058954	3648.199632	24.417703
133.713445	3649.803678	24.422720
134.152691	3663.603924	24.427738
134.192328	3667.991484	24.432755
133.951736	3661.546239	24.437773
134.235343	3665.100181	24.442791
134.623495	3685.552521	24.447808
134.505522	3694.131139	24.452826
135.060800	3687.722170	24.457843
135.485963	3718.126979	24.462861
135.560980	3713.017902	24.467879
135.672033	3712.524058	24.472896
135.477254	3716.626408	24.477914
135.949776	3713.364639	24.482931
136.090681	3722.142594	24.487949
136.095111	3713.402161	24.492967
136.222636	3726.449582	24.497984
136.140347	3742.698851	24.503002
136.569687	3728.125205	24.508019
136.256818	3735.989480	24.513037
136.786036	3739.511271	24.518055
136.777367	3743.259367	24.523072
136.882426	3759.466674	24.528090
137.494659	3746.268934	24.533107
137.247236	3754.760545	24.538125
137.264822	3762.550966	24.543143
137.455835	3763.654329	24.548160
137.448566	3777.669808	24.553178
137.840204	3774.455420	24.558195
137.883834	3786.496528	24.563213
137.751394	3794.228401	24.568231
138.278160	3803.305767	24.573248
138.206623	3797.193812	24.578266
138.474046	3807.422847	24.583283
138.626344	3823.408178	24.588301
138.831419	3824.878636	24.593319
139.151747	3822.483439	24.598336
139.322385	3818.924903	24.603354
139.354969	3817.070335	24.608371
139.852219	3825.637851	24.613389
139.906463	3836.585230	24.618407
139.673066	3838.228542	24.623424
139.834155	3846.915017	24.628442
140.080438	3836.021874	24.633459
139.896251	3838.209840	24.638477
140.041959	3831.817642	24.643495
140.671094	3851.455952	24.648512
141.021449	3862.057101	24.653530
141.037783	3852.216322	24.658547
141.306070	3857.941123	24.663565
140.832526	3858.103851	24.668583
141.106668	3852.332266	24.673600
141.120741	3854.082002	24.678618
141.181738	3856.237870	24.683635
141.141620	3867.187425	24.688653
141.447783	3877.063230	24.693671
141.568812	3869.904732	24.698688
141.563114	3892.773658	24.703706
141.860584	3893.901384	24.708723
141.893666	3900.477391	24.713741
142.039995	3909.125175	24.718759
142.035056	3927.906527	24.723776
142.459623	3934.900982	24.728794
142.348649	3930.969903	24.733811
142.597036	3938.152937	24.738829
142.783196	3954.114140	24.743847
143.347686	3952.463456	24.748864
143.128349	3954.682194	24.753882
143.261807	3948.803207	24.758899
143.463962	3966.406389	24.763917
143.742768	3968.452394	24.768935
143.874424	3975.173960	24.773952
143.857194	3978.693030	24.778970
144.234229	3982.860519	24.783987
144.203160	3992.419923	24.789005
144.083237	4008.741610	24.794023
144.386815	3998.732651	24.799040
144.552061	4004.470486	24.804058
144.774700	4025.880276	24.809075
144.958724	4020.409988	24.814093
145.012316	4029.454283	24.819111
145.456307	4019.890460	24.824128
145.508067	4031.955708	24.829146
145.660251	4044.967932	24.834163
145.965672	4047.129720	24.839181
145.822592	4055.778725	24.844199
146.031043	4048.158253	24.849216
146.371564	4042.887544	24.854234
146.335139	4064.016014	24.859251
146.398592	4064.476537	24.864269
146.727176	4068.086642	24.869287
146.940580	4061.270269	24.874304
146.774966	4064.645314	24.879322
147.046110	4069.599574	24.884339
147.514328	4080.785259	24.889357
147.510227	4084.823099	24.894375
147.616289	4084.042794	24.899392
147.922785	4084.916606	24.904410
147.718060	4078.894863	24.909427
147.596984	4090.450640	24.914445
147.886558	4106.316866	24.919463
148.309053	4092.416316	24.924480
148.202649	4111.257943	24.929498
147.964823	4121.310643	24.934515
148.497665	4127.716901	24.939533
148.596342	4138.708004	24.944551
148.938613	4146.441409	24.949568
149.089368	4153.103234	24.954586
149.434590	4148.295752	24.959603
149.123246	4153.925228	24.964621
149.529407	4164.129573	24.969639
149.900081	4169.472289	24.974656
149.712843	4181.600331	24.979674
149.904882	4173.392127	24.984691
150.091427	4173.173677	24.989709
150.351108	4196.563252	24.994727
150.591671	4183.852699	24.999744
150.598826	4196.654177	25.004762
151.021661	4207.364119	25.009779
151.264830	4208.724478	25.014797
151.628227	4212.133460	25.019815
151.627529	4215.577388	25.024832
151.675123	4225.266631	25.029850
151.423389	4220.066563	25.034867
151.729935	4219.352692	25.039885
151.470375	4221.022232	25.044903
152.005696	4238.343063	25.049920
151.783691	4246.521591	25.054938
152.211226	4246.764102	25.059955
152.286924	4244.375611	25.064973
152.438790	4266.604820	25.069991
153.011108	4265.634673	25.075008
152.883144	4274.464488	25.080026
153.072598	4277.645062	25.085043
152.961995	4271.245518	25.090061
152.586104	4284.918273	25.095079
153.004607	4293.160611	25.100096
153.072542	4296.230812	25.105114
153.470425	4307.796960	25.110131
153.733268	4309.233156	25.115149
153.844649	4329.312936	25.120167
154.261795	4325.706214	25.125184
154.568283	4343.113499	25.130202
154.919178	4336.834175	25.135219
155.036098	4335.982716	25.140237
154.823278	4339.709260	25.145255
155.238055	4331.633381	25.150272
155.280784	4336.913892	25.155290
155.566464	4346.666906	25.160307
155.886811	4348.144600	25.165325
155.842712	4366.193931	25.170343
156.181944	4358.180379	25.175360
156.144037	4358.704136	25.180378
156.076376	4364.964667	25.185395
156.221007	4356.893222	25.190413
156.398175	4363.229029	25.195431
156.540939	4369.175671	25.200448
156.837606	4369.385027	25.205466
156.688196	4380.825482	25.210483
156.905154	4379.134514	25.215501
157.006620	4397.625071	25.220519
157.414541	4406.484628	25.225536
157.606608	4405.731869	25.230554
157.391448	4402.135812	25.235571
157.693159	4415.181692	25.240589
157.515548	4424.966296	25.245607
158.062010	4430.107944	25.250624
158.246686	4446.281297	25.255642
158.237490	4458.580488	25.260659
158.343716	4447.200731	25.265677
158.327381	4468.635858	25.270695
158.638490	4467.387820	25.275712
158.946910	4477.945398	25.280730
159.167558	4480.878072	25.285747
159.408858	4491.995400	25.290765
159.350283	4497.863151	25.295783
159.590918	4510.524109	25.300800
160.001334	4520.402872	25.305818
159.712267	4529.860937	25.310835
160.390720	4522.974692	25.315853
160.211589	4522.510506	25.320871
160.761621	4534.024555	25.325888
160.977551	4542.541792	25.330906
160.751720	4539.070482	25.335923
160.917917	4546.146688	25.340941
161.204071	4561.609820	25.345959
161.314209	4560.832013	25.350976
161.637999	4568.937804	25.355994
161.572472	4575.639981	25.361011
161.704160	4573.324745	25.366029
161.886000	4587.465891	25.371047
161.871859	4587.588213	25.376064
162.405876	4589.578525	25.381082
162.287808	4601.099434	25.386099
162.601174	4603.705110	25.391117
162.517452	4620.659286	25.396135
162.845269	4615.358839	25.401152
163.414212	4623.129538	25.406170
163.409310	4632.410564	25.411187
163.564080	4627.424466	25.416205
163.724255	4632.838176	25.421223
163.758269	4637.987567	25.426240
163.729840	4637.547115	25.431258
163.684016	4652.402626	25.436275
164.240784	4651.965189	25.441293
164.059557	4658.900165	25.446311
164.001330	4662.997117	25.451328
164.726710	4678.618806	25.456346
164.657905	4683.519172	25.461363
164.862465	4686.504905	25.466381
165.291638	4701.311293	25.471399
165.392892	4708.880682	25.476416
165.659314	4709.618762	25.481434
165.423886	4703.904645	25.486451
165.974307	4715.314584	25.491469
166.245006	4728.709609	25.496487
166.196645	4726.785559	25.501504
166.518458	4725.150734	25.506522
166.590044	4735.281558	25.511539
166.735626	4727.680121	25.516557
166.968105	4745.961116	25.521575
166.980681	4751.994567	25.526592
167.077617	4749.776292	25.531610
167.162710	4766.101261	25.536627
167.426085	4764.582909	25.541645
167.662082	4772.614163	25.546663
167.558961	4784.656828	25.551680
167.901873	4794.603135	25.556698
167.808552	4793.472097	25.561715
168.257299	4795.068600	25.566733
168.781561	4811.463696	25.571751
168.633554	4813.437778	25.576768
168.752946	4819.227246	25.581786
168.604243	4822.808112	25.586803
168.878058	4830.407336	25.591821
169.004547	4845.141312	25.596839
169.223264	4866.956747	25.601856
169.678036	4865.935543	25.606874
169.397766	4874.054036	25.611891
170.126152	4879.634481	25.616909
170.146688	4900.171040	25.621927
169.848028	4906.931958	25.626944
170.468192	4912.999693	25.631962
170.608855	4922.955660	25.636979
170.946346	4917.830377	25.641997
171.082033	4931.098345	25.647015
171.495395	4943.274846	25.652032
171.841365	4937.479041	25.657050
171.618192	4941.734472	25.662067
171.813518	4925.709798	25.667085
172.424154	4947.631227	25.672103
172.633579	4955.041728	25.677120
172.597811	4958.352403	25.682138
172.654523	4969.527350	25.687156
172.928518	4952.568614	25.692173
173.012274	4955.503873	25.697191
172.738487	4960.932006	25.702208
173.429727	4968.626877	25.707226
173.435334	4983.884953	25.712244
173.729897	4976.354769	25.717261
173.512831	4980.176804	25.722279
173.509158	4995.568918	25.727296
173.767962	5010.708436	25.732314
173.912545	5007.043273	25.737332
174.089433	5023.612930	25.742349
174.363316	5024.665512	25.747367
174.519765	5034.549622	25.752384
175.001416	5040.216121	25.757402
175.183149	5060.809677	25.762420
175.288219	5051.329979	25.767437
175.699925	5058.266913	25.772455
175.272607	5059.868112	25.777472
175.631781	5054.243813	25.782490
175.575295	5072.422048	25.787508
175.698870	5075.638336	25.792525
176.280312	5089.338482	25.797543
176.305586	5107.472377	25.802560
176.986949	5100.023592	25.807578
176.883312	5108.802650	25.812596
176.969637	5100.818926	25.817613
177.186143	5105.864102	25.822631
177.199159	5121.945000	25.827648
177.625958	5115.631423	25.832666
177.481447	5120.240735	25.837684
177.509680	5138.670917	25.842701
178.323779	5147.290436	25.847719
178.220675	5149.645779	25.852736
178.598499	5144.870809	25.857754
178.496309	5155.682505	25.862772
178.989792	5166.628162	25.867789
178.973945	5167.161112	25.872807
178.851906	5174.175395	25.877824
179.007116	5179.047113	25.882842
179.503745	5188.202503	25.887860
179.478065	5194.901821	25.892877
179.763863	5197.849659	25.897895
179.842496	5212.752418	25.902912
180.136886	5213.943844	25.907930
180.025067	5224.514031	25.912948
179.838742	5241.188138	25.917965
180.373584	5242.698593	25.922983
180.465723	5259.515331	25.928000
180.662576	5270.662196	25.933018
181.072434	5273.606394	25.938036
181.206175	5292.493693	25.943053
181.686096	5281.083281	25.948071
181.715454	5303.048855	25.953088
182.017179	5316.142731	25.958106
181.715662	5312.941971	25.963124
182.238041	5330.818284	25.968141
182.658403	5339.114472	25.973159
182.545306	5333.169498	25.978176
183.273032	5344.239553	25.983194
183.398815	5361.691908	25.988212
183.832913	5368.016225	25.993229
183.737699	5361.443428	25.998247
184.287056	5361.799452	26.003264
183.924257	5350.454730	26.008282
184.158387	5355.620324	26.013300
183.950625	5368.020682	26.018317
184.433347	5369.877072	26.023335
184.177872	5381.502072	26.028352
184.349884	5388.344105	26.033370
184.863886	5400.492521	26.038388
184.833754	5399.383112	26.043405
185.236372	5419.607867	26.048423
185.062880	5428.603204	26.053440
185.500649	5433.809520	26.058458
185.901384	5443.661896	26.063476
185.973874	5446.002395	26.068493
186.512600	5457.348346	26.073511
186.407239	5468.066024	26.078528
186.306749	5477.826483	26.083546
186.506874	5470.872774	26.088564
186.882762	5483.500596	26.093581
187.115622	5492.498594	26.098599
187.112411	5499.039828	26.103616
187.134700	5501.934299	26.108634
187.498362	5514.160006	26.113652
187.678189	5522.522371	26.118669
188.243051	5532.172310	26.123687
187.888479	5534.570255	26.128704
188.367855	5545.066949	26.133722
188.550952	5543.889403	26.138740
188.590853	5553.555305	26.143757
188.871035	5562.192378	26.148775
189.053820	5578.136599	26.153792
189.478566	5579.408642	26.158810
189.544112	5579.354341	26.163828
189.468078	5597.624548	26.168845
190.060149	5598.078056	26.173863
189.885231	5602.846929	26.178880
190.580773	5606.775500	26.183898
190.647337	5621.825690	26.188916
191.072699	5621.443545	26.193933
191.286986	5617.887294	26.198951
191.133328	5619.773961	26.203968
191.310883	5626.684662	26.208986
191.298569	5644.790257	26.214004
191.350966	5656.035748	26.219021
191.442215	5653.429984	26.224039
191.689733	5665.263621	26.229056
192.059267	5669.192772	26.234074
192.184899	5682.245052	26.239092
192.239300	5696.126081	26.244109
192.696581	5708.836008	26.249127
192.548057	5715.450592	26.254144
193.006667	5723.791472	26.259162
193.685261	5734.209716	26.264180
193.986570	5741.533540	26.269197
193.960078	5740.638194	26.274215
193.862057	5744.596415	26.279232
193.851991	5750.491692	26.284250
194.530532	5757.166124	26.289268
194.411933	5769.281310	26.294285
194.953520	5768.953559	26.299303
194.928138	5782.982891	26.304320
195.303325	5777.759920	26.309338
195.605888	5784.509047	26.314356
195.556018	5796.300970	26.319373
195.901284	5804.426048	26.324391
195.697998	5803.350054	26.329408
196.493220	5819.451077	26.334426
196.944078	5826.385329	26.339444
196.848849	5823.685643	26.344461
197.393770	5825.702800	26.349479
197.480590	5822.318000	26.354496
197.593978	5819.367821	26.359514
197.736695	5823.970192	26.364532
197.687896	5832.548449	26.369549
197.815782	5840.884373	26.374567
197.871513	5839.038600	26.379584
198.338107	5850.291927	26.384602
198.537389	5844.405176	26.389620
198.316326	5858.522041	26.394637
198.264194	5872.694528	26.399655
198.705421	5883.472029	26.404672
198.799047	5903.332200	26.409690
199.000002	5901.170094	26.414708
199.211201	5921.378045	26.419725
199.281532	5918.617684	26.424743
199.548997	5932.575999	26.429760
199.449862	5946.897959	26.434778
200.051781	5949.575426	26.439796
200.051896	5963.392558	26.444813
200.442327	5965.200336	26.449831
200.491045	5984.666726	26.454848
200.324597	5994.118962	26.459866
200.830710	5992.130012	26.464884
201.550869	6016.330518	26.469901
201.546133	6024.422137	26.474919
201.706737	6023.898373	26.479936
202.160691	6031.094228	26.484954
202.535586	6031.840625	26.489972
202.447467	6038.272242	26.494989
202.679417	6040.126952	26.500007
202.802882	6047.027347	26.505024
203.011455	6056.638680	26.510042
203.449204	6061.750479	26.515060
203.457309	6072.873739	26.520077
203.614369	6068.300424	26.525095
203.719433	6085.860891	26.530112
203.825074	6088.982309	26.535130
204.258692	6098.716246	26.540148
204.164509	6115.989124	26.545165
204.547009	6120.819174	26.550183
204.523137	6129.040107	26.555200
204.917363	6134.846918	26.560218
205.131512	6148.097166	26.565236
205.534745	6163.107686	26.570253
205.684386	6162.017419	26.575271
205.718852	6167.561767	26.580288
205.947512	6187.363210	26.585306
206.210069	6183.941343	26.590324
206.144245	6208.779789	26.595341
206.881718	6219.605783	26.600359
206.664136	6214.314558	26.605376
206.868200	6234.666027	26.610394
207.377025	6232.645059	26.615412
207.874100	6255.412932	26.620429
207.705614	6252.213261	26.625447
207.682776	6259.865871	26.630464
208.116273	6277.573946	26.635482
208.940187	6277.751241	26.640500
209.207934	6288.600355	26.645517
209.277473	6283.358832	26.650535
209.481191	6282.550510	26.655552
209.595308	6291.226573	26.660570
209.723314	6293.126004	26.665588
209.975854	6310.606761	26.670605
210.316661	6298.128422	26.675623
210.432095	6296.885666	26.680640
210.663313	6306.010595	26.685658
210.835663	6317.796453	26.690676
210.874547	6322.007991	26.695693
211.009408	6320.269731	26.700711
211.119066	6321.578564	26.705728
210.818128	6341.128521	26.710746
211.213611	6347.235098	26.715764
211.304048	6362.771461	26.720781
212.007957	6369.618927	26.725799
212.499593	6385.288179	26.730816
212.526597	6399.117211	26.735834
212.666072	6398.438906	26.740852
212.397333	6406.944555	26.745869
212.973422	6412.287326	26.750887
213.028161	6422.933129	26.755904
213.262865	6433.235064	26.760922
213.697014	6448.165212	26.765940
213.783811	6465.198560	26.770957
214.192733	6472.726798	26.775975
214.154815	6481.392043	26.780992
214.133740	6488.946611	26.786010
214.700267	6495.635709	26.791028
214.568498	6511.781549	26.796045
215.077016	6507.415083	26.801063
215.438503	6510.382848	26.806080
215.609565	6534.183912	26.811098
215.651086	6524.978581	26.816116
215.775249	6541.857776	26.821133
215.857346	6557.149377	26.826151
216.043741	6555.857606	26.831168
216.613929	6576.666662	26.836186
216.485768	6578.091690	26.841204
216.571586	6592.157887	26.846221
216.453430	6605.934051	26.851239
217.271163	6618.114621	26.856256
217.432015	6634.050572	26.861274
217.791415	6636.914508	26.866292
218.208363	6659.266107	26.871309
218.241501	6667.042705	26.876327
218.815749	6669.674108	26.881344
218.913382	6688.827368	26.886362
219.281460	6683.343239	26.891380
218.789837	6691.637701	26.896397
219.290917	6709.884900	26.901415
219.763926	6712.699483	26.906432
219.669467	6728.366140	26.911450
220.093282	6726.276360	26.916468
220.480835	6726.421003	26.921485
220.514085	6749.618879	26.926503
220.893142	6748.754657	26.931520
221.202928	6758.710386	26.936538
221.344149	6764.626485	26.941556
221.497575	6772.276951	26.946573
221.467910	6768.720813	26.951591
221.757508	6784.551490	26.956608
222.169693	6791.157543	26.961626
222.730826	6806.112287	26.966644
222.821283	6810.262191	26.971661
222.977351	6817.988027	26.976679
223.460907	6809.584602	26.981696
223.333037	6827.134917	26.986714
224.048814	6828.765541	26.991732
224.080159	6834.130638	26.996749
224.150998	6837.870071	27.001767
224.390108	6829.530187	27.006784
224.393507	6859.498065	27.011802
224.601903	6855.364790	27.016820
224.862788	6875.054595	27.021837
224.955288	6885.192806	27.026855
225.599770	6887.554375	27.031872
225.528367	6895.464252	27.036890
225.986050	6914.173046	27.041908
225.912378	6919.977643	27.046925
225.923308	6921.169396	27.051943
226.669541	6932.414311	27.056960
226.553541	6942.080114	27.061978
226.764775	6945.563965	27.066996
226.933114	6975.474623	27.072013
227.112507	6968.918210	27.077031
227.390711	6986.550280	27.082048
227.547045	6991.823233	27.087066
227.877450	7004.711788	27.092084
228.096777	7029.516144	27.097101
228.156115	7026.258548	27.102119
228.728418	7046.982572	27.107136
228.616761	7054.390560	27.112154
228.974328	7052.819386	27.117172
229.078712	7063.410429	27.122189
229.545976	7081.833771	27.127207
229.739256	7081.585826	27.132224
230.040327	7094.425371	27.137242
229.789936	7098.549814	27.142260
230.276338	7113.418652	27.147277
230.344932	7114.153101	27.152295
230.690144	7131.083446	27.157312
230.634373	7140.730446	27.162330
231.109784	7153.798433	27.167348
231.573842	7171.142696	27.172365
231.573364	7175.862549	27.177383
232.131181	7191.073840	27.182400
231.928637	7194.010114	27.187418
232.475002	7202.767270	27.192436
232.693101	7218.893647	27.197453
232.812020	7229.138402	27.202471
233.229909	7237.243272	27.207488
233.113833	7254.984721	27.212506
233.374603	7262.924799	27.217524
233.473499	7281.926946	27.222541
233.650517	7295.777349	27.227559
234.250665	7294.493320	27.232576
234.308234	7318.136390	27.237594
234.652870	7335.161722	27.242612
235.002297	7344.963183	27.247629
235.020518	7351.504878	27.252647
235.608206	7359.074930	27.257664
235.782755	7380.010019	27.262682
235.686691	7380.656622	27.267700
236.552844	7392.817499	27.272717
236.677926	7405.959489	27.277735
236.899745	7400.725363	27.282752
236.868768	7419.934259	27.287770
237.454916	7425.023197	27.292788
238.019830	7433.790186	27.297805
237.725723	7434.452031	27.302823
237.762038	7443.813264	27.307840
238.164114	7462.133549	27.312858
238.463090	7470.187697	27.317876
238.698948	7474.387584	27.322893
238.629527	7501.043607	27.327911
239.279281	7502.166892	27.332928
239.213710	7505.905732	27.337946
239.498072	7514.258946	27.342964
240.002348	7526.220886	27.347981
240.085634	7544.944777	27.352999
240.594563	7544.817856	27.358016
240.694394	7556.600085	27.363034
240.742463	7567.313893	27.368052
240.694365	7570.825862	27.373069
240.939953	7588.147918	27.378087
241.314185	7597.873017	27.383104
241.666905	7623.831685	27.388122
241.876495	7629.993071	27.393140
242.183212	7639.510935	27.398157
242.218184	7660.130407	27.403175
243.012454	7670.162272	27.408192
242.978035	7679.534705	27.413210
242.846686	7690.945980	27.418228
243.057432	7697.798596	27.423245
243.323865	7717.589459	27.428263
243.658909	7732.826628	27.433280
244.013224	7750.030778	27.438298
244.517538	7764.085981	27.443316
244.636151	7765.526111	27.448333
244.928063	7783.658767	27.453351
245.201220	7778.432277	27.458368
245.441659	7800.920256	27.463386
245.862371	7806.862363	27.468404
246.352878	7813.175540	27.473421
246.191036	7817.197873	27.478439
246.502567	7816.887196	27.483456
246.905171	7824.328584	27.488474
247.222201	7832.310608	27.493492
247.447065	7828.941700	27.498509
247.462949	7845.302356	27.503527
247.662241	7845.924806	27.508544
247.569458	7857.143876	27.513562
247.985637	7863.159323	27.518580
248.231362	7877.012029	27.523597
248.264587	7890.841207	27.528615
248.720442	7910.315311	27.533632
249.137131	7918.745849	27.538650
248.909100	7936.612830	27.543668
249.712928	7930.798035	27.548685
249.632055	7953.772211	27.553703
250.221913	7957.948324	27.558720
250.525868	7973.016923	27.563738
250.418494	7998.625147	27.568756
250.867318	7998.734950	27.573773
250.873240	8000.940980	27.578791
251.109495	8015.095195	27.583808
251.084101	8028.706349	27.588826
251.301542	8044.265278	27.593844
251.524524	8061.600792	27.598861
251.859025	8082.025429	27.603879
252.142197	8095.155773	27.608896
252.619600	8109.490123	27.613914
252.976473	8123.969650	27.618932
253.494926	8131.655054	27.623949
253.841552	8149.056523	27.628967
254.131675	8151.934711	27.633984
254.703513	8174.172333	27.639002
254.641895	8178.782050	27.644020
254.723266	8177.557134	27.649037
255.067663	8193.206800	27.654055
255.200155	8193.265132	27.659072
255.792511	8211.126988	27.664090
255.682397	8226.563743	27.669108
256.004937	8228.057205	27.674125
256.313672	8239.371463	27.679143
256.885471	8243.481015	27.684160
256.847600	8250.110744	27.689178
257.011768	8276.630264	27.694196
257.696798	8267.983094	27.699213
257.694162	8284.520681	27.704231
257.894540	8293.922944	27.709248
258.500687	8302.437635	27.714266
258.320303	8302.368183	27.719284
258.760810	8310.788855	27.724301
258.552065	8333.789848	27.729319
259.052476	8337.935863	27.734336
259.510715	8342.404198	27.739354
259.371455	8350.110642	27.744372
259.452501	8359.184347	27.749389
259.800675	8376.727859	27.754407
260.311816	8389.428058	27.759424
260.348930	8401.485851	27.764442
260.680949	8427.335235	27.769460
260.966022	8430.258459	27.774477
261.134603	8451.388284	27.779495
261.476894	8460.127498	27.784512
262.193920	8464.899454	27.789530
262.447533	8473.943024	27.794548
262.669584	8476.879285	27.799565
263.170622	8498.440129	27.804583
263.134230	8498.035559	27.809600
263.604919	8497.772555	27.814618
263.000047	8507.275814	27.819636
263.637592	8516.473949	27.824653
264.164283	8534.535835	27.829671
263.724621	8540.499303	27.834688
264.003587	8551.572157	27.839706
264.506661	8565.426108	27.844724
264.807968	8568.258410	27.849741
264.911176	8584.672341	27.854759
265.577741	8598.649093	27.859776
265.998192	8612.061389	27.864794
265.944846	8627.129665	27.869812
266.415443	8620.419707	27.874829
266.647669	8639.023502	27.879847
266.635974	8643.240338	27.884864
267.146288	8659.562146	27.889882
267.350884	8681.125441	27.894900
267.875619	8682.969288	27.899917
267.940853	8692.380295	27.904935
268.046162	8701.595598	27.909952
268.706418	8712.564618	27.914970
268.688683	8715.355363	27.919988
268.932288	8718.281971	27.925005
269.262366	8751.687292	27.930023
269.504065	8760.786542	27.935040
269.701883	8763.543527	27.940058
269.944207	8777.823665	27.945076
270.716237	8795.477981	27.950093
270.423043	8811.363811	27.955111
270.639432	8823.283293	27.960128
271.276123	8835.954660	27.965146
271.304092	8848.945558	27.970164
271.836296	8851.520727	27.975181
271.783811	8873.651775	27.980199
272.055552	8880.763641	27.985216
272.771243	8896.216821	27.990234
272.750489	8919.621630	27.995252
273.536683	8932.980022	28.000269
273.483971	8946.132016	28.005287
273.657984	8954.708392	28.010304
274.290853	8957.681406	28.015322
273.939843	8970.431818	28.020340
274.704355	8989.650333	28.025357
274.550672	9004.100026	28.030375
275.218386	9003.199962	28.035392
275.322729	9014.139429	28.040410
275.470064	9027.629541	28.045428
275.580724	9034.081576	28.050445
276.053457	9054.870819	28.055463
276.452135	9074.576117	28.060480
276.570516	9082.308807	28.065498
277.113797	9100.273931	28.070516
277.240486	9113.255863	28.075533
277.772812	9130.196620	28.080551
278.029994	9137.288765	28.085568
278.684106	9139.393389	28.090586
278.657242	9148.222331	28.095604
279.141398	9139.536769	28.100621
279.041293	9147.149006	28.105639
279.337288	9166.223247	28.110656
279.792111	9157.684348	28.115674
279.925571	9181.137947	28.120692
279.993149	9182.867181	28.125709
280.527674	9200.571720	28.130727
280.475631	9205.950569	28.135744
280.837800	9215.946784	28.140762
281.157167	9227.727260	28.145780
281.407772	9239.622706	28.150797
281.891584	9237.640075	28.155815
281.980147	9252.494034	28.160832
282.288527	9254.955932	28.165850
282.289835	9269.179486	28.170868
282.730303	9283.362671	28.175885
283.132712	9292.203368	28.180903
282.801597	9315.723597	28.185920
283.357520	9324.518161	28.190938
283.428247	9349.320495	28.195956
283.769306	9359.957870	28.200973
284.181448	9374.846484	28.205991
283.893502	9387.700965	28.211008
284.666925	9408.898156	28.216026
284.666051	9427.056188	28.221044
284.873575	9444.303857	28.226061
285.395481	9461.334955	28.231079
285.560101	9481.213116	28.236096
286.387738	9501.827287	28.241114
286.503674	9519.392477	28.246132
286.824082	9539.830403	28.251149
287.163429	9561.193644	28.256167
287.555923	9569.088824	28.261184
288.207934	9580.173318	28.266202
288.363150	9595.500183	28.271220
288.607365	9601.757840	28.276237
288.910404	9613.635840	28.281255
288.993469	9625.772479	28.286272
289.120524	9640.396545	28.291290
289.587822	9653.688594	28.296308
289.933471	9667.388064	28.301325
290.778361	9676.257509	28.306343
290.696058	9695.846214	28.311360
291.087380	9687.664333	28.316378
291.160600	9704.914338	28.321396
291.350936	9725.038164	28.326413
291.770823	9737.977760	28.331431
292.181848	9752.349044	28.336448
292.230337	9756.676684	28.341466
292.195022	9775.759248	28.346484
292.728307	9788.292758	28.351501
293.236736	9802.948774	28.356519
293.229692	9821.013435	28.361536
293.526600	9832.519964	28.366554
293.866423	9861.530671	28.371572
294.264183	9874.571708	28.376589
294.721085	9891.957541	28.381607
295.127022	9903.011314	28.386624
295.256421	9910.812085	28.391642
295.618655	9925.235350	28.396660
295.776970	9939.949477	28.401677
296.406053	9939.705851	28.406695
296.283502	9967.109413	28.411712
296.538813	9973.491754	28.416730
296.642609	9990.266779	28.421748
296.677137	10012.442382	28.426765
296.786196	10024.051077	28.431783
297.477219	10049.578104	28.436800
297.812066	10066.686422	28.441818
298.071924	10082.202528	28.446836
298.327390	10099.212801	28.451853
298.747179	10115.379573	28.456871
299.194782	10131.017867	28.461888
299.908844	10153.576593	28.466906
300.438097	10160.067642	28.471924
300.653861	10181.880368	28.476941
301.264153	10166.509203	28.481959
301.176393	10183.497541	28.486976
301.486873	10175.602810	28.491994
301.773953	10195.857231	28.497012
301.892542	10202.775733	28.502029
302.192453	10203.158326	28.507047
302.490599	10216.717242	28.512064
302.925411	10223.437815	28.517082
302.875977	10233.666402	28.522100
302.939130	10245.762359	28.527117
303.565875	10253.671656	28.532135
303.704819	10279.269693	28.537152
304.186017	10287.343890	28.542170
304.223394	10303.182361	28.547188
304.578160	10321.212931	28.552205
304.928077	10327.501637	28.557223
304.734640	10350.449043	28.562240
305.398029	10356.691812	28.567258
305.659919	10387.673182	28.572276
305.579737	10407.726451	28.577293
306.410246	10427.056105	28.582311
306.470794	10448.224069	28.587328
306.722076	10466.337297	28.592346
307.095794	10488.495064	28.597364
307.569834	10498.894394	28.602381
308.051799	10514.887583	28.607399
308.172921	10540.975026	28.612416
308.363084	10558.264336	28.617434
308.830438	10573.467329	28.622452
309.289942	10581.431382	28.627469
309.761495	10612.039269	28.632487
309.856421	10622.769602	28.637504
310.014113	10628.892755	28.642522
310.509422	10647.583650	28.647540
310.831595	10671.647382	28.652557
311.452153	10673.972159	28.657575
311.636225	10694.230628	28.662592
311.524195	10711.081156	28.667610
311.994509	10730.240207	28.672628
312.373339	10753.130037	28.677645
313.184684	10761.105361	28.682663
313.551382	10779.961782	28.687680
313.009784	10785.247265	28.692698
313.608369	10803.015921	28.697716
313.811610	10821.604337	28.702733
314.371863	10834.781629	28.707751
314.760060	10851.809687	28.712768
315.388507	10863.896431	28.717786
315.991260	10870.556199	28.722804
316.032390	10880.824630	28.727821
316.233991	10890.906894	28.732839
316.424699	10897.473338	28.737856
316.816937	10911.573753	28.742874
317.044645	10926.261999	28.747892
317.135055	10940.457079	28.752909
317.502448	10948.719901	28.757927
317.926879	10976.055044	28.762944
318.167934	10984.634484	28.767962
318.673653	10995.625913	28.772980
318.600236	11010.929761	28.777997
318.956286	11028.591376	28.783015
319.719202	11052.861269	28.788032
319.532141	11066.029484	28.793050
320.232377	11070.293226	28.798068
320.497921	11090.150977	28.803085
320.912676	11104.045923	28.808103
321.326483	11121.985921	28.813120
321.480659	11125.937356	28.818138
321.903403	11139.512159	28.823156
322.132577	11144.847513	28.828173
322.659481	11161.304701	28.833191
322.694352	11172.515241	28.838208
323.007795	11188.996419	28.843226
323.188710	11189.002974	28.848244
323.616060	11210.527988	28.853261
323.876788	11216.439422	28.858279
324.120988	11238.899396	28.863296
324.249292	11254.077115	28.868314
324.642836	11260.450875	28.873332
324.758451	11272.703474	28.878349
325.272106	11292.086820	28.883367
325.649105	11312.473618	28.888384
325.814097	11328.466635	28.893402
326.378608	11344.776001	28.898420
326.539785	11371.401440	28.903437
326.825301	11386.497801	28.908455
327.313867	11402.250736	28.913472
327.640940	11416.143862	28.918490
327.848892	11433.702752	28.923508
328.086215	11448.484631	28.928525
328.669420	11465.372183	28.933543
328.962431	11496.148422	28.938560
329.348227	11510.534488	28.943578
329.903917	11528.424231	28.948596
329.872806	11545.521761	28.953613
330.022540	11565.878123	28.958631
330.569885	11586.311161	28.963648
331.084448	11603.051706	28.968666
331.314533	11613.019378	28.973684
331.435750	11632.088784	28.978701
331.933452	11648.462561	28.983719
332.239684	11669.744987	28.988736
332.607871	11697.276296	28.993754
333.187514	11706.734552	28.998772
333.508516	11729.789362	29.003789
333.839642	11735.598360	29.008807
334.248399	11754.900728	29.013824
334.248776	11766.271753	29.018842
334.890535	11781.240001	29.023860
335.020099	11800.987181	29.028877
335.457558	11822.716566	29.033895
336.407369	11840.004899	29.038912
336.402662	11858.115366	29.043930
336.696809	11867.128977	29.048948
336.692310	11874.957858	29.053965
337.496988	11895.401447	29.058983
337.992909	11907.433843	29.064000
338.197703	11934.334286	29.069018
338.704506	11935.758144	29.074036
338.355206	11942.715846	29.079053
338.794892	11958.934779	29.084071
339.140419	11979.917731	29.089088
339.358435	12002.035367	29.094106
339.830698	12011.216927	29.099124
340.008579	12040.483738	29.104141
340.341494	12049.598728	29.109159
340.929353	12061.326307	29.114176
341.260644	12086.988256	29.119194
341.724188	12105.897155	29.124212
341.800899	12121.355224	29.129229
342.006723	12133.338475	29.134247
342.520376	12148.529182	29.139264
343.284352	12166.150074	29.144282
343.747315	12175.295279	29.149300
343.826852	12202.471505	29.154317
344.122718	12205.068388	29.159335
344.481640	12219.440261	29.164352
344.617514	12229.154606	29.169370
345.197848	12237.732000	29.174388
345.288498	12254.050072	29.179405
346.058885	12253.939029	29.184423
346.082056	12266.901473	29.189440
346.278308	12285.814529	29.194458
347.041845	12301.553569	29.199476
347.207497	12308.544421	29.204493
347.333446	12318.812983	29.209511
347.775572	12330.194096	29.214528
348.082232	12357.319180	29.219546
348.353761	12362.285099	29.224564
348.189749	12386.559817	29.229581
348.915838	12399.153303	29.234599
349.107560	12421.556596	29.239616
349.395370	12442.211218	29.244634
349.965203	12459.168075	29.249652
350.266389	12485.668951	29.254669
350.819407	12494.228637	29.259687
350.814801	12514.067053	29.264704
351.183079	12548.136321	29.269722
351.849228	12565.046609	29.274740
352.198243	12582.319215	29.279757
352.681627	12592.910879	29.284775
353.013472	12606.996767	29.289792
353.126713	12632.826246	29.294810
353.916022	12647.472078	29.299828
354.008012	12666.695529	29.304845
354.382281	12682.789547	29.309863
354.817256	12696.281458	29.314880
355.147857	12713.506543	29.319898
355.352664	12715.543029	29.324916
356.178019	12743.897936	29.329933
356.431175	12766.115174	29.334951
356.737823	12781.714607	29.339968
357.023587	12799.837318	29.344986
357.409378	12810.914917	29.350004
357.503946	12825.413925	29.355021
357.529699	12854.873197	29.360039
358.347079	12866.600066	29.365056
358.558878	12894.334466	29.370074
359.059811	12899.454067	29.375092
359.520235	12929.836949	29.380109
359.709281	12944.962305	29.385127
360.304991	12961.694509	29.390144
360.534569	12988.832575	29.395162
360.753132	13004.758624	29.400180
361.054330	13026.981275	29.405197
361.384583	13043.208812	29.410215
361.835404	13065.787022	29.415232
362.300788	13084.333455	29.420250
362.281811	13102.459980	29.425268
362.817147	13123.506053	29.430285
363.455899	13149.396028	29.435303
363.479799	13164.121105	29.440320
363.869988	13180.370951	29.445338
364.591532	13208.607027	29.450356
364.790719	13224.691036	29.455373
365.327015	13251.980385	29.460391
365.393878	13259.274440	29.465408
366.202507	13275.916727	29.470426
366.410041	13302.117621	29.475444
366.355039	13308.868665	29.480461
366.940815	13336.504078	29.485479
367.705753	13351.321650	29.490496
367.775437	13374.850482	29.495514
368.464080	13385.492548	29.500532
368.722409	13393.107199	29.505549
368.796895	13413.253124	29.510567
369.717454	13423.963098	29.515584
369.794493	13442.434919	29.520602
370.159384	13453.541433	29.525620
370.150043	13468.480382	29.530637
370.558481	13475.067309	29.535655
370.979250	13477.366901	29.540672
370.978506	13504.494414	29.545690
371.569873	13525.266886	29.550708
372.118335	13551.638940	29.555725
372.355498	13568.996288	29.560743
372.711120	13587.070915	29.565760
373.182931	13604.183111	29.570778
373.661442	13625.484971	29.575796
374.209456	13639.468293	29.580813
374.336164	13663.269614	29.585831
374.803198	13669.569524	29.590848
375.366307	13696.050017	29.595866
375.322390	13706.146983	29.600884
376.104014	13719.616908	29.605901
376.306662	13751.323652	29.610919
376.878293	13759.697835	29.615936
376.998201	13781.444481	29.620954
377.717457	13800.416084	29.625972
377.691472	13814.754723	29.630989
377.837799	13828.921112	29.636007
378.368058	13847.767621	29.641024
379.132262	13881.303563	29.646042
379.475404	13893.692760	29.651060
379.989767	13907.236264	29.656077
380.172610	13932.450262	29.661095
380.598047	13940.468456	29.666112
380.770629	13968.188463	29.671130
381.115262	13982.105996	29.676148
381.674265	14001.608195	29.681165
381.792107	14026.421948	29.686183
382.437945	14049.633985	29.691200
382.884789	14069.112767	29.696218
382.962827	14080.450910	29.701236
383.852824	14105.017492	29.706253
384.104243	14134.430768	29.711271
384.665965	14142.291902	29.716288
384.793915	14166.412628	29.721306
384.872197	14185.627133	29.726324
385.605238	14203.899037	29.731341
385.394839	14226.086380	29.736359
386.006439	14247.447045	29.741376
386.693978	14270.292793	29.746394
386.594902	14292.469091	29.751412
387.339114	14318.653644	29.756429
387.608183	14342.161915	29.761447
387.993365	14356.723949	29.766464
388.405210	14385.098719	29.771482
388.429108	14401.767018	29.776500
389.317311	14430.616758	29.781517
389.383464	14451.788332	29.786535
390.118993	14467.476725	29.791552
390.640832	14497.012427	29.796570
390.694886	14523.507490	29.801588
391.124282	14539.957643	29.806605
391.695927	14557.614059	29.811623
392.184784	14577.620515	29.816640
392.156009	14605.903565	29.821658
392.569440	14625.546060	29.826676
393.020689	14635.834404	29.831693
393.229856	14679.852307	29.836711
394.008434	14695.268857	29.841728
394.719127	14707.256769	29.846746
395.148260	14729.612969	29.851764
395.731071	14740.190265	29.856781
395.884737	14759.867272	29.861799
396.363956	14768.070045	29.866816
396.619761	14766.653155	29.871834
396.628433	14786.532920	29.876852
397.006208	14804.794729	29.881869
397.311822	14833.101535	29.886887
397.799145	14837.974300	29.891904
398.231754	14863.687306	29.896922
398.558947	14886.808157	29.901940
399.202301	14900.730104	29.906957
399.187929	14931.307417	29.911975
399.736653	14947.878194	29.916992
400.589784	14968.898646	29.922010
400.723377	14995.912491	29.927028
401.085769	15014.925417	29.932045
401.574756	15034.505968	29.937063
402.072951	15040.605645	29.942080
402.230833	15059.154802	29.947098
402.786111	15086.017450	29.952116
403.416984	15095.327269	29.957133
403.822723	15126.758145	29.962151
404.021650	15131.647735	29.967168
404.377754	15156.599343	29.972186
405.276195	15175.847450	29.977204
405.833536	15177.149954	29.982221
405.940064	15201.455366	29.987239
406.468652	15219.296006	29.992256
406.947018	15233.547236	29.997274
407.025138	15247.744313	30.002292
407.475402	15263.288551	30.007309
407.519462	15282.541104	30.012327
408.063296	15307.008707	30.017344
408.762009	15319.463155	30.022362
408.690108	15344.971587	30.027380
409.336519	15362.500183	30.032397
409.882272	15396.868910	30.037415
410.284984	15410.569943	30.042432
410.860339	15425.854687	30.047450
410.962864	15442.085204	30.052468
411.567609	15465.308564	30.057485
411.229563	15486.178230	30.062503
411.978666	15508.778948	30.067520
412.472610	15539.309195	30.072538
412.787836	15569.895908	30.077556
413.671085	15578.632673	30.082573
414.244324	15612.542681	30.087591
414.467223	15626.357310	30.092608
415.329273	15646.615951	30.097626
415.511403	15666.674753	30.102644
415.919501	15667.482699	30.107661
416.138858	15702.329479	30.112679
416.346711	15714.706312	30.117696
416.980966	15727.209025	30.122714
417.050735	15757.689201	30.127732
417.735468	15776.715562	30.132749
417.979279	15796.338457	30.137767
418.244296	15813.450292	30.142784
419.164150	15830.759619	30.147802
419.400117	15860.282201	30.152820
419.514393	15882.196358	30.157837
420.158520	15902.220942	30.162855
420.470672	15916.884043	30.167872
421.075503	15957.801370	30.172890
421.148050	15967.495962	30.177908
421.887988	15996.061775	30.182925
422.114341	16019.291385	30.187943
422.316130	16030.507074	30.192960
422.845540	16049.798077	30.197978
423.135932	16080.746398	30.202996
423.994568	16096.543192	30.208013
424.181637	16125.404252	30.213031
424.353635	16143.004717	30.218048
424.881773	16154.554691	30.223066
425.228346	16187.920068	30.228084
425.500674	16202.444336	30.233101
426.180927	16224.914557	30.238119
426.265775	16258.065216	30.243136
426.837027	16278.648023	30.248154
427.196876	16300.701066	30.253172
427.827384	16322.272713	30.258189
428.145599	16361.091193	30.263207
428.231423	16387.144828	30.268224
429.216409	16403.651695	30.273242
429.066363	16435.478145	30.278260
429.867209	16461.786269	30.283277
430.295547	16492.969484	30.288295
430.656701	16525.726732	30.293312
431.625838	16528.474598	30.298330
431.783186	16575.818242	30.303348
432.121417	16594.571206	30.308365
432.515513	16615.298988	30.313383
433.293836	16645.704331	30.318400
433.977233	16663.872667	30.323418
434.341878	16687.517300	30.328436
434.582877	16707.015224	30.333453
435.091094	16727.137764	30.338471
435.396577	16753.258561	30.343488
435.757320	16777.418758	30.348506
436.168572	16799.249541	30.353524
436.761897	16815.650708	30.358541
437.182802	16849.075077	30.363559
437.392271	16875.858583	30.368576
438.174671	16896.434248	30.373594
438.353198	16929.321862	30.378612
438.955448	16955.349071	30.383629
439.333833	16975.132129	30.388647
440.063942	16995.605541	30.393664
440.317483	17020.070264	30.398682
440.592024	17053.167309	30.403700
441.297702	17071.022999	30.408717
441.911028	17100.232530	30.413735
442.279973	17129.897319	30.418752
442.771518	17134.918471	30.423770
443.272058	17160.999792	30.428788
443.709056	17175.568493	30.433805
443.944009	17196.454489	30.438823
443.960281	17229.465945	30.443840
444.606979	17250.306458	30.448858
445.032296	17281.377713	30.453876
445.727096	17307.289825	30.458893
446.045143	17328.055555	30.463911
446.316032	17351.311382	30.468928
447.225777	17379.881084	30.473946
447.193159	17406.829591	30.478964
447.858107	17437.535064	30.483981
448.360334	17455.119747	30.488999
448.855531	17475.181936	30.494016
449.475945	17494.984474	30.499034
449.761989	17527.417211	30.504052
450.691572	17548.959185	30.509069
450.992726	17575.634540	30.514087
451.498922	17587.444668	30.519104
451.457220	17598.228766	30.524122
451.882346	17621.561838	30.529140
452.419239	17641.497639	30.534157
452.834939	17657.510400	30.539175
452.687752	17684.445652	30.544192
453.591320	17695.820879	30.549210
453.695590	17719.336990	30.554228
454.473190	17742.349669	30.559245
454.841080	17772.028244	30.564263
454.895622	17796.304010	30.569280
455.644659	17814.658994	30.574298
456.555380	17847.373469	30.579316
456.804081	17869.117209	30.584333
457.194635	17888.235966	30.589351
457.674378	17911.358675	30.594368
458.577329	17929.165312	30.599386
458.840323	17954.943770	30.604404
459.176031	17989.353188	30.609421
459.797448	18000.349519	30.614439
459.768267	18016.558610	30.619456
460.674690	18039.027114	30.624474
460.894094	18070.883672	30.629492
461.140811	18097.037602	30.634509
461.808200	18120.383870	30.639527
462.113192	18144.999896	30.644544
462.953917	18174.864046	30.649562
463.757333	18203.394766	30.654580
463.776834	18220.942041	30.659597
464.334929	18242.315545	30.664615
464.594797	18267.494740	30.669632
465.327895	18289.908555	30.674650
465.774378	18323.802127	30.679668
465.957197	18339.150677	30.684685
466.745034	18365.820385	30.689703
466.944950	18395.898964	30.694720
467.569970	18414.330802	30.699738
468.211485	18450.417850	30.704756
468.402052	18468.298660	30.709773
468.995064	18494.108273	30.714791
469.252404	18519.635661	30.719808
470.014349	18546.189638	30.724826
470.129931	18578.859316	30.729844
470.720170	18613.659576	30.734861
471.763262	18638.413326	30.739879
471.769251	18655.091268	30.744896
472.430047	18677.965414	30.749914
472.889968	18707.334074	30.754932
473.305764	18725.817932	30.759949
473.853535	18764.030365	30.764967
474.124497	18783.787876	30.769984
474.859249	18800.819309	30.775002
475.258035	18840.028161	30.780020
475.692340	18862.704243	30.785037
476.128584	18884.508195	30.790055
476.207321	18905.900652	30.795072
477.035561	18939.400662	30.800090
477.350320	18962.127173	30.805108
477.637410	18999.420594	30.810125
478.159031	19020.434235	30.815143
478.335623	19045.684341	30.820160
479.155330	19071.377083	30.825178
479.825502	19100.871351	30.830196
480.448864	19142.876031	30.835213
481.407981	19167.018143	30.840231
481.529876	19193.085694	30.845248
482.010630	19202.291513	30.850266
482.233548	19235.754168	30.855284
482.623010	19258.450371	30.860301
483.776006	19284.129100	30.865319
484.223786	19296.631756	30.870336
485.001160	19304.894023	30.875354
485.644165	19323.526082	30.880372
485.708838	19328.418816	30.885389
485.820258	19346.255967	30.890407
486.084699	19367.929423	30.895424
486.592373	19389.842794	30.900442
487.178993	19402.797619	30.905460
487.604260	19433.303713	30.910477
488.515925	19459.285827	30.915495
488.272380	19481.885580	30.920512
488.885895	19494.709894	30.925530
489.270697	19515.164247	30.930548
489.486406	19555.767896	30.935565
490.452047	19579.397742	30.940583
490.933833	19607.614459	30.945600
491.382384	19628.482252	30.950618
491.749320	19661.070147	30.955636
492.288502	19695.968792	30.960653
492.608066	19720.723525	30.965671
493.215870	19753.583432	30.970688
493.463193	19780.327106	30.975706
494.000929	19817.696557	30.980724
494.326118	19849.665816	30.985741
495.353370	19893.479006	30.990759
495.555694	19922.668709	30.995776
496.035279	19947.158577	31.000794
496.588218	19981.606990	31.005812
497.183532	20020.585251	31.010829
497.539067	20039.945381	31.015847
498.178997	20068.245402	31.020864
498.824582	20101.978201	31.025882
499.409160	20132.826888	31.030900
499.341099	20160.258615	31.035917
500.128105	20189.293957	31.040935
500.686529	20230.824648	31.045952
501.362754	20259.953265	31.050970
501.853991	20285.206236	31.055988
502.378643	20320.032450	31.061005
503.091676	20345.952084	31.066023
503.248466	20379.521826	31.071040
504.023176	20414.296406	31.076058
504.931933	20430.366912	31.081076
504.888407	20465.383468	31.086093
505.882148	20489.199566	31.091111
506.112854	20514.443092	31.096128
506.867483	20539.610909	31.101146
507.706918	20560.860756	31.106164
507.754363	20588.205488	31.111181
508.386237	20603.068475	31.116199
509.473024	20630.983405	31.121216
509.757470	20649.628664	31.126234
510.116177	20665.267411	31.131252
510.787939	20695.661046	31.136269
511.662184	20697.116504	31.141287
511.756996	20725.881957	31.146304
512.345256	20749.445963	31.151322
512.902276	20764.668309	31.156340
512.816051	20791.503515	31.161357
513.741463	20805.682525	31.166375
514.164762	20843.248771	31.171392
514.441536	20860.511700	31.176410
515.174278	20879.295471	31.181428
515.462867	20912.422146	31.186445
515.885273	20925.599575	31.191463
516.207895	20955.479638	31.196480
516.926571	20982.662920	31.201498
517.453509	21004.846779	31.206516
517.503506	21042.547695	31.211533
518.170612	21061.702073	31.216551
518.330518	21086.489856	31.221568
519.179678	21119.724954	31.226586
519.885272	21146.910513	31.231604
519.974991	21172.992054	31.236621
520.441437	21194.692757	31.241639
521.035586	21237.439456	31.246656
521.428213	21268.130438	31.251674
521.854910	21291.208597	31.256692
522.182016	21328.026290	31.261709
522.725934	21352.766899	31.266727
523.543186	21393.621334	31.271744
523.925119	21431.972368	31.276762
524.524359	21459.838469	31.281780
524.996890	21499.868831	31.286797
525.838518	21535.348920	31.291815
526.304743	21568.682666	31.296832
526.797433	21599.743928	31.301850
527.478798	21626.933946	31.306868
528.241881	21661.548271	31.311885
528.442493	21692.516416	31.316903
528.958198	21723.492125	31.321920
529.527151	21753.151574	31.326938
530.252214	21790.413296	31.331956
530.476265	21826.022229	31.336973
531.152786	21850.477308	31.341991
531.779682	21874.162986	31.347008
531.979162	21909.118769	31.352026
532.838217	21939.428123	31.357044
533.219165	21978.500710	31.362061
533.865252	22014.473558	31.367079
534.529901	22048.099293	31.372096
534.756531	22082.855248	31.377114
535.569037	22113.127928	31.382132
536.013770	22151.287277	31.387149
537.108326	22187.588286	31.392167
537.617128	22216.960867	31.397184
537.815712	22245.566947	31.402202
538.743290	22264.239381	31.407220
539.117960	22297.860408	31.412237
539.799588	22314.738940	31.417255
540.501281	22352.024338	31.422272
540.608913	22379.652791	31.427290
541.277025	22403.825524	31.432308
541.560585	22440.222423	31.437325
542.284621	22462.459199	31.442343
542.667840	22498.745813	31.447360
543.459197	22526.305297	31.452378
544.235009	22553.620816	31.457396
544.498307	22595.777740	31.462413
545.144354	22613.875342	31.467431
545.680551	22653.329359	31.472448
545.948975	22680.515995	31.477466
547.000517	22711.940125	31.482484
547.307389	22746.811056	31.487501
547.699431	22765.473057	31.492519
549.095874	22787.604887	31.497536
549.209960	22816.932755	31.502554
549.814709	22842.525093	31.507572
550.104818	22870.144606	31.512589
550.751831	22903.521795	31.517607
551.187313	22933.633615	31.522624
551.839525	22955.762133	31.527642
552.100536	22980.618601	31.532660
552.590337	23018.020587	31.537677
552.973586	23047.420383	31.542695
553.845182	23079.024939	31.547712
554.499888	23100.047382	31.552730
555.257425	23123.214885	31.557748
555.107080	23147.308181	31.562765
555.488562	23175.526764	31.567783
556.167375	23199.439707	31.572800
556.349102	23236.466972	31.577818
557.176115	23261.096122	31.582836
557.978903	23297.255290	31.587853
558.556612	23324.173194	31.592871
559.076883	23364.642190	31.597888
559.429624	23394.116788	31.602906
560.448744	23419.259499	31.607924
560.391259	23452.552053	31.612941
561.088326	23483.786476	31.617959
561.852377	23521.026390	31.622976
562.258716	23561.816955	31.627994
562.777386	23582.753789	31.633012
563.397228	23625.476341	31.638029
564.369308	23646.418060	31.643047
565.139796	23679.398056	31.648064
565.717401	23711.289797	31.653082
566.216851	23735.048217	31.658100
566.529717	23773.022796	31.663117
566.994562	23799.440834	31.668135
568.121465	23825.932159	31.673152
568.337437	23862.765643	31.678170
569.066994	23883.176853	31.683188
570.075549	23918.388614	31.688205
569.981864	23953.229602	31.693223
570.770264	23981.777399	31.698240
571.036498	24013.415058	31.703258
571.632143	24039.320014	31.708276
572.054409	24081.360392	31.713293
572.849052	24105.597535	31.718311
573.812635	24140.620830	31.723328
574.018284	24173.209830	31.728346
574.604581	24210.099704	31.733364
575.756090	24246.294453	31.738381
576.203475	24272.039667	31.743399
576.668425	24307.311976	31.748416
577.031756	24339.288836	31.753434
577.860681	24356.405140	31.758452
578.232729	24403.155785	31.763469
578.586625	24441.984665	31.768487
579.194918	24473.986571	31.773504
580.101597	24504.368222	31.778522
580.245065	24539.811363	31.783540
581.087581	24574.860701	31.788557
581.577747	24613.832882	31.793575
581.954812	24646.269412	31.798592
582.777189	24683.824663	31.803610
583.249465	24713.497353	31.808628
583.970680	24739.111807	31.813645
584.008691	24778.072967	31.818663
585.179801	24814.682774	31.823680
585.930276	24849.209837	31.828698
586.629265	24874.638355	31.833716
587.472211	24900.726886	31.838733
587.682507	24931.780706	31.843751
588.449710	24963.360364	31.848768
588.482115	24997.646241	31.853786
589.237880	25031.066837	31.858804
589.982206	25053.018948	31.863821
590.331880	25090.459402	31.868839
591.417646	25117.047365	31.873856
591.371560	25148.571416	31.878874
592.358502	25174.422880	31.883892
593.056282	25210.905312	31.888909
593.433320	25234.855321	31.893927
594.413726	25254.476592	31.898944
594.719438	25292.682685	31.903962
595.078396	25320.591833	31.908980
595.675753	25338.927056	31.913997
595.903824	25371.811522	31.919015
596.537498	25393.528542	31.924032
597.462730	25429.482801	31.929050
597.786760	25466.277025	31.934068
598.581620	25504.893543	31.939085
598.780681	25540.405579	31.944103
599.836916	25554.005051	31.949120
600.146014	25596.192725	31.954138
600.626993	25630.877100	31.959156
601.435125	25668.310027	31.964173
602.043909	25703.341066	31.969191
602.946626	25736.708223	31.974208
603.176170	25770.958221	31.979226
604.105130	25802.096748	31.984244
604.796355	25829.872405	31.989261
605.380226	25875.240823	31.994279
605.576329	25911.961096	31.999296
606.145052	25943.396422	32.004314
607.057765	25985.155414	32.009332
607.751204	26015.395793	32.014349
607.988011	26059.182088	32.019367
608.928885	26086.723079	32.024384
609.380190	26132.270838	32.029402
610.213298	26169.214139	32.034420
611.015185	26190.444310	32.039437
611.561961	26235.313739	32.044455
612.221119	26263.284619	32.049472
612.729753	26304.993796	32.054490
613.021077	26335.961247	32.059508
613.876089	26365.203545	32.064525
614.409079	26418.335979	32.069543
615.177479	26455.037131	32.074560
615.730913	26486.184968	32.079578
616.120345	26532.248933	32.084596
616.562239	26570.455077	32.089613
617.122365	26614.425785	32.094631
618.068677	26644.065003	32.099648
618.888335	26686.939743	32.104666
619.727004	26715.420357	32.109684
620.186547	26746.260966	32.114701
620.382293	26783.728669	32.119719
621.383413	26824.900408	32.124736
621.902102	26865.446231	32.129754
622.469905	26911.704334	32.134772
623.503708	26942.935650	32.139789
624.014063	26981.264574	32.144807
624.614435	27004.056685	32.149824
625.041289	27044.465561	32.154842
625.592745	27086.068514	32.159860
626.607733	27114.591602	32.164877
627.437032	27156.296555	32.169895
627.927412	27180.047830	32.174912
628.486627	27216.030995	32.179930
629.262964	27257.586441	32.184948
630.026600	27286.755898	32.189965
630.282228	27310.999163	32.194983
631.073951	27344.563335	32.200000
631.601139	27386.632098	32.205018
631.965417	27427.664622	32.210036
632.914231	27456.742117	32.215053
633.216994	27488.518559	32.220071
634.189417	27526.226263	32.225088
634.631053	27551.287633	32.230106
635.193352	27593.597826	32.235124
636.138074	27616.286133	32.240141
636.487213	27645.950818	32.245159
636.835891	27664.510400	32.250176
637.265806	27698.422566	32.255194
637.874162	27736.257203	32.260212
638.898945	27765.936341	32.265229
639.296459	27817.842179	32.270247
639.869532	27839.489155	32.275264
640.645359	27873.138859	32.280282
641.315008	27911.254971	32.285300
642.135559	27940.517585	32.290317
642.307684	27991.340409	32.295335
643.259132	28028.565640	32.300352
644.067407	28057.052902	32.305370
644.526241	28107.041028	32.310388
645.637971	28132.567032	32.315405
646.116820	28169.164937	32.320423
646.799440	28205.004112	32.325440
647.408449	28240.304974	32.330458
647.860865	28270.927787	32.335476
649.020634	28303.506755	32.340493
649.430970	28346.992689	32.345511
650.021608	28379.104681	32.350528
650.533725	28409.756278	32.355546
651.046145	28444.958847	32.360564
651.975618	28485.411962	32.365581
652.628315	28524.865567	32.370599
653.658941	28555.044288	32.375616
654.414300	28590.221703	32.380634
654.456736	28621.231611	32.385652
655.308602	28657.993204	32.390669
655.893889	28686.667969	32.395687
657.017665	28732.476528	32.400704
657.650888	28756.358974	32.405722
657.822235	28806.621387	32.410740
658.522843	28835.347830	32.415757
658.894292	28880.187343	32.420775
659.792671	28913.313897	32.425792
660.614479	28949.669861	32.430810
661.465873	28998.170152	32.435828
662.072422	29036.336173	32.440845
662.751069	29067.348256	32.445863
663.431198	29100.553540	32.450880
663.914635	29144.390016	32.455898
664.163862	29186.253180	32.460916
665.027490	29214.613291	32.465933
665.905329	29272.553717	32.470951
666.608372	29306.349925	32.475968
667.144835	29349.401044	32.480986
667.571432	29390.946077	32.486004
668.687898	29431.321211	32.491021
669.047228	29470.797298	32.496039
669.666209	29511.212572	32.501056
670.573836	29550.862112	32.506074
671.031460	29590.942508	32.511092
671.813223	29627.577756	32.516109
672.362251	29671.303946	32.521127
672.954309	29711.028500	32.526144
674.194279	29754.918473	32.531162
674.466684	29791.696995	32.536180
675.461561	29827.016018	32.541197
675.791867	29870.435539	32.546215
676.816811	29904.492060	32.551232
677.512125	29938.789898	32.556250
678.028442	29986.535879	32.561268
678.839036	30013.685397	32.566285
679.632015	30058.025296	32.571303
680.072677	30086.535030	32.576320
680.933373	30107.583092	32.581338
681.416525	30141.769104	32.586356
681.908781	30168.058409	32.591373
682.453818	30205.218502	32.596391
682.849159	30237.597880	32.601408
683.751493	30276.358339	32.606426
684.433002	30319.414058	32.611444
684.933104	30356.663638	32.616461
685.859326	30394.927512	32.621479
685.977861	30440.454814	32.626496
687.043149	30478.570636	32.631514
687.142321	30524.158048	32.636532
688.118610	30574.873967	32.641549
688.897330	30622.030358	32.646567
689.704144	30658.979592	32.651584
690.607546	30707.267161	32.656602
690.850451	30751.536659	32.661620
691.743604	30787.252551	32.666637
692.731919	30845.755360	32.671655
693.270300	30888.986397	32.676672
694.319549	30927.465889	32.681690
694.538824	30977.327828	32.686708
695.706615	31009.031146	32.691725
696.270544	31071.646868	32.696743
697.217318	31111.451322	32.701760
698.193602	31141.655005	32.706778
698.633556	31186.703741	32.711796
698.953567	31217.712012	32.716813
700.014433	31254.072541	32.721831
700.719933	31308.126249	32.726848
701.522797	31352.214512	32.731866
702.373905	31384.897291	32.736884
703.158538	31419.057167	32.741901
703.500154	31454.563465	32.746919
704.226110	31506.401884	32.751936
705.094040	31542.843710	32.756954
706.469860	31597.747781	32.761972
706.833592	31624.697564	32.766989
707.566562	31653.081498	32.772007
708.108407	31690.756823	32.777024
708.926709	31718.640705	32.782042
709.936331	31756.622202	32.787060
710.585126	31792.245338	32.792077
711.224153	31831.941326	32.797095
711.630557	31871.964624	32.802112
712.346294	31894.459628	32.807130
713.395995	31940.836929	32.812148
714.077013	31974.343829	32.817165
714.747115	32017.227852	32.822183
715.238672	32045.087480	32.827200
716.205578	32082.197518	32.832218
717.002105	32122.760785	32.837236
717.776925	32147.016949	32.842253
718.418377	32188.786831	32.847271
719.100737	32221.364594	32.852288
720.037635	32252.353666	32.857306
720.473324	32293.574361	32.862324
720.951459	32328.972264	32.867341
721.705294	32363.429329	32.872359
722.010191	32412.282423	32.877376
722.872089	32450.206135	32.882394
723.761382	32498.664457	32.887412
724.367654	32545.087258	32.892429
725.084868	32575.896265	32.897447
725.836099	32629.345649	32.902464
726.669890	32653.473050	32.907482
727.251064	32705.419316	32.912500
728.039778	32743.652162	32.917517
728.731887	32769.692195	32.922535
729.350533	32805.151090	32.927552
730.303671	32828.684690	32.932570
730.920496	32875.530156	32.937588
731.626114	32907.232893	32.942605
732.402467	32947.876791	32.947623
732.496297	32990.454763	32.952640
733.819925	33015.194992	32.957658
733.974300	33068.182614	32.962676
734.531496	33101.521050	32.967693
735.543863	33146.313682	32.972711
736.440171	33190.745251	32.977728
737.026875	33234.270737	32.982746
737.628634	33283.357554	32.987764
738.153685	33322.132207	32.992781
739.360919	33372.597508	32.997799
739.500177	33428.325961	33.002816
740.435570	33469.831091	33.007834
741.245468	33516.514987	33.012852
741.920754	33577.584463	33.017869
742.974461	33621.859527	33.022887
743.295253	33671.225179	33.027904
744.423055	33721.179000	33.032922
745.226922	33765.348077	33.037940
746.213176	33817.353789	33.042957
747.173447	33862.029661	33.047975
747.788325	33908.150658	33.052992
748.426940	33954.508292	33.058010
749.233108	33996.255988	33.063028
749.727957	34043.066260	33.068045
750.917263	34089.135633	33.073063
751.156062	34149.516422	33.078080
752.046535	34190.290276	33.083098
753.199826	34242.662880	33.088116
754.057516	34285.844626	33.093133
754.905040	34326.157599	33.098151
755.134728	34374.255679	33.103168
755.888928	34420.716369	33.108186
756.970359	34456.971781	33.113204
757.916207	34508.252105	33.118221
759.077528	34546.354018	33.123239
759.894444	34593.772633	33.128256
760.836736	34613.939963	33.133274
761.565506	34666.607718	33.138292
762.026781	34692.951843	33.143309
763.049176	34728.293856	33.148327
763.487661	34767.558932	33.153344
764.858969	34806.102635	33.158362
765.690466	34839.881402	33.163380
766.151529	34874.407411	33.168397
766.921859	34918.780166	33.173415
767.292064	34949.779780	33.178432
768.327068	34987.466001	33.183450
769.359075	35027.289863	33.188468
769.564941	35065.472786	33.193485
770.554638	35100.959646	33.198503
771.138985	35149.838564	33.203520
771.905013	35185.234134	33.208538
772.454092	35227.720041	33.213556
773.044591	35273.335689	33.218573
774.262516	35306.295945	33.223591
774.561990	35357.142106	33.228608
775.469392	35402.961322	33.233626
776.389822	35453.248902	33.238644
776.853823	35496.564328	33.243661
777.830526	35538.768914	33.248679
778.334951	35580.333047	33.253696
779.174044	35615.800095	33.258714
780.137174	35657.665603	33.263732
780.854435	35703.407754	33.268749
781.465950	35731.114382	33.273767
781.994358	35781.470452	33.278784
782.893265	35806.950733	33.283802
783.915238	35849.376478	33.288820
784.472136	35891.767645	33.293837
785.327719	35937.292625	33.298855
785.835829	35987.001085	33.303872
786.812167	36025.299035	33.308890
787.255381	36069.402947	33.313908
788.163602	36123.589060	33.318925
789.110769	36166.950330	33.323943
790.069619	36221.343750	33.328960
791.038553	36255.577491	33.333978
791.745531	36304.774992	33.338996
792.498317	36359.080892	33.344013
793.667228	36395.743265	33.349031
794.527954	36435.362638	33.354048
795.400402	36474.758936	33.359066
796.092954	36519.311623	33.364084
796.494779	36558.541490	33.369101
797.688576	36595.345745	33.374119
798.253402	36652.483030	33.379136
799.124484	36683.899957	33.384154
800.223829	36719.201628	33.389172
800.514985	36777.311627	33.394189
801.761183	36818.983338	33.399207
801.946378	36865.911565	33.404224
802.676118	36919.963245	33.409242
803.589227	36961.080352	33.414260
804.405586	37020.740197	33.419277
805.215984	37073.843776	33.424295
806.448346	37120.893135	33.429312
807.224887	37166.496353	33.434330
808.351269	37200.694313	33.439348
808.710266	37262.007310	33.444365
810.000088	37307.245898	33.449383
810.770116	37351.718630	33.454400
811.540585	37397.032411	33.459418
812.500871	37442.759209	33.464436
812.999506	37481.469729	33.469453
814.090196	37531.229673	33.474471
814.642939	37575.231012	33.479488
815.381974	37615.086631	33.484506
816.436545	37671.764210	33.489524
817.010577	37712.752475	33.494541
818.167964	37760.289252	33.499559
818.691020	37807.798992	33.504576
819.392313	37851.802931	33.509594
820.377825	37900.897252	33.514612
821.148554	37946.629514	33.519629
821.973250	37990.197051	33.524647
822.761878	38043.995722	33.529664
823.698268	38088.184660	33.534682
824.693527	38132.446679	33.539700
825.263678	38181.246231	33.544717
826.271032	38226.271720	33.549735
827.262529	38271.204930	33.554752
827.775596	38320.684055	33.559770
829.044080	38354.248202	33.564788
829.545542	38404.589370	33.569805
830.203124	38453.116572	33.574823
831.216697	38492.633611	33.579840
831.792596	38548.035160	33.584858
832.849648	38581.013034	33.589876
833.591344	38636.755632	33.594893
833.963079	38672.693021	33.599911
835.154663	38715.243348	33.604928
836.089711	38761.375311	33.609946
836.529154	38791.756240	33.614964
837.368477	38839.307266	33.619981
838.238250	38878.423829	33.624999
838.826659	38927.336041	33.630016
839.693048	38971.942487	33.635034
840.622892	39016.058468	33.640052
841.071579	39070.969036	33.645069
841.898736	39120.103583	33.650087
842.811436	39176.598648	33.655104
843.289195	39238.303408	33.660122
844.906874	39278.416612	33.665140
845.804323	39344.805317	33.670157
846.398661	39394.805397	33.675175
847.375153	39445.877764	33.680192
848.232448	39490.689076	33.685210
849.050460	39542.697160	33.690228
850.190762	39598.556895	33.695245
850.829417	39650.251818	33.700263
851.683733	39704.493356	33.705280
852.642221	39747.335184	33.710298
853.647294	39792.908180	33.715316
854.459731	39847.510788	33.720333
855.285399	39903.610304	33.725351
856.632224	39950.274802	33.730368
856.893697	39998.273016	33.735386
858.167650	40051.810962	33.740404
858.697546	40102.202219	33.745421
859.451607	40148.896720	33.750439
860.283677	40199.544452	33.755456
861.331528	40254.244030	33.760474
862.720097	40304.798542	33.765492
863.925493	40360.068206	33.770509
864.365640	40399.488791	33.775527
865.367149	40449.731111	33.780544
866.320016	40495.351703	33.785562
867.202891	40543.785065	33.790580
868.204310	40595.096561	33.795597
869.087362	40633.303495	33.800615
870.013498	40676.088977	33.805632
870.778560	40720.221579	33.810650
871.850890	40763.920363	33.815668
872.281119	40815.473606	33.820685
873.140823	40858.699915	33.825703
873.973973	40906.016106	33.830720
874.936175	40959.282552	33.835738
876.127132	41001.008956	33.840756
876.821214	41050.826460	33.845773
877.502278	41100.450053	33.850791
878.324929	41138.268883	33.855808
879.181209	41202.158840	33.860826
879.811819	41242.183584	33.865844
880.648644	41300.700952	33.870861
881.960948	41350.529854	33.875879
883.169272	41391.583873	33.880896
884.073630	41444.082625	33.885914
884.966007	41478.406230	33.890932
885.660376	41535.453907	33.895949
886.743018	41564.713394	33.900967
887.207338	41614.384741	33.905984
888.028948	41668.990473	33.911002
889.133295	41716.367149	33.916020
890.004003	41756.658826	33.921037
890.584334	41801.834499	33.926055
891.996887	41853.868848	33.931072
892.483487	41889.970655	33.936090
893.678112	41936.618968	33.941108
894.243710	41971.715544	33.946125
895.244948	42019.368339	33.951143
895.835684	42048.496778	33.956160
896.242237	42098.911948	33.961178
897.273477	42136.472146	33.966196
898.226018	42189.939170	33.971213
898.873025	42233.422870	33.976231
899.816147	42288.112314	33.981248
900.538739	42344.733904	33.986266
901.748750	42400.279977	33.991284
902.642169	42449.886022	33.996301
903.455719	42504.830316	34.001319
904.496605	42553.711432	34.006336
905.642786	42607.503350	34.011354
906.383586	42656.570832	34.016372
907.369778	42707.345710	34.021389
908.296746	42755.283705	34.026407
909.406758	42812.206361	34.031424
910.541698	42873.053138	34.036442
911.174440	42912.460733	34.041460
912.203111	42952.736194	34.046477
913.182022	43010.388302	34.051495
914.237074	43059.432775	34.056512
914.782796	43111.175721	34.061530
915.852409	43164.664730	34.066548
916.934203	43222.623866	34.071565
917.614659	43276.762323	34.076583
918.449884	43323.754488	34.081600
919.393505	43387.529586	34.086618
920.278812	43442.338473	34.091636
921.183909	43495.430250	34.096653
922.249521	43550.109967	34.101671
923.470983	43596.789224	34.106688
924.267596	43662.555298	34.111706
925.010555	43710.460924	34.116724
926.060613	43764.460471	34.121741
926.687551	43823.751144	34.126759
927.851116	43870.996675	34.131776
928.390974	43935.835980	34.136794
930.065347	43990.870567	34.141812
930.932426	44038.789095	34.146829
931.959781	44095.240937	34.151847
933.329294	44144.478943	34.156864
934.038773	44201.341379	34.161882
934.949491	44243.320232	34.166900
935.777363	44292.693980	34.171917
937.115377	44348.199603	34.176935
937.934973	44389.623706	34.181952
938.856636	44446.314382	34.186970
939.586491	44490.428424	34.191988
940.679816	44532.474114	34.197005
941.662513	44581.122123	34.202023
942.406468	44623.728735	34.207040
943.279679	44687.025193	34.212058
944.300199	44732.757836	34.217076
945.348244	44787.120743	34.222093
946.145158	44842.573160	34.227111
947.062896	44891.276297	34.232128
948.038062	44947.738474	34.237146
948.893742	44983.768558	34.242164
949.837971	45040.172555	34.247181
950.362300	45089.734762	34.252199
951.431013	45147.137978	34.257216
952.531609	45210.912702	34.262234
953.395504	45266.260797	34.267252
954.346066	45308.754132	34.272269
955.177412	45367.264136	34.277287
956.523425	45410.910298	34.282304
957.322343	45462.018112	34.287322
958.383908	45496.795904	34.292340
959.034564	45546.725218	34.297357
960.053967	45593.996979	34.302375
961.302304	45629.131611	34.307392
962.027412	45682.908349	34.312410
962.700621	45722.175416	34.317428
964.103395	45780.616006	34.322445
964.432952	45823.118989	34.327463
965.604628	45877.825768	34.332480
966.477309	45933.357588	34.337498
967.384670	45983.646215	34.342516
968.371441	46042.918065	34.347533
969.164906	46098.576565	34.352551
970.544685	46150.176989	34.357568
970.951518	46220.148835	34.362586
972.047249	46268.061647	34.367604
972.957455	46331.641632	34.372621
974.061178	46389.839632	34.377639
975.528769	46443.584175	34.382656
976.029640	46518.261489	34.387674
977.566803	46567.136978	34.392692
978.432716	46621.684681	34.397709
979.331406	46677.378744	34.402727
980.617409	46735.099939	34.407744
981.829604	46800.614057	34.412762
982.335829	46850.847231	34.417780
983.364017	46900.157404	34.422797
984.101235	46964.303987	34.427815
985.500471	47011.196619	34.432832
986.352951	47084.074703	34.437850
986.895244	47137.067448	34.442868
988.285039	47188.681339	34.447885
989.864473	47261.642289	34.452903
991.162029	47303.711814	34.457920
991.701100	47373.071848	34.462938
992.489000	47416.815623	34.467956
993.648530	47480.233277	34.472973
994.631751	47538.699836	34.477991
995.580275	47583.519578	34.483008
996.919512	47634.819757	34.488026
997.608011	47702.702324	34.493044
999.074606	47745.024568	34.498061
999.770721	47804.574305	34.503079
1001.427447	47864.283791	34.508096
1001.979761	47912.810278	34.513114
1002.609399	47968.062503	34.518132
1003.866053	48023.684853	34.523149
1004.817880	48080.063640	34.528167
1006.273153	48127.493899	34.533184
1006.927214	48171.367636	34.538202
1007.616716	48236.455294	34.543220
1008.640244	48278.999745	34.548237
1009.815436	48346.573948	34.553255
1010.860696	48405.925081	34.558272
1011.994514	48462.890007	34.563290
1012.748978	48512.562879	34.568308
1014.272661	48560.571712	34.573325
1015.307048	48616.325214	34.578343
1016.597700	48667.375940	34.583360
1017.088724	48712.478322	34.588378
1018.071066	48760.028236	34.593396
1019.235068	48811.364838	34.598413
1020.553016	48861.671496	34.603431
1021.767586	48921.212573	34.608448
1022.886820	48954.537836	34.613466
1023.433587	49003.092820	34.618484
1024.750175	49041.543658	34.623501
1025.401020	49073.898506	34.628519
1025.976021	49125.391303	34.633536
1027.001029	49160.433540	34.638554
1027.718608	49206.526375	34.643572
1029.058541	49260.316572	34.648589
1029.627862	49307.698199	34.653607
1030.599027	49362.666234	34.658624
1031.599374	49420.394696	34.663642
1032.450762	49472.629538	34.668660
1033.435034	49528.956211	34.673677
1034.390683	49595.195535	34.678695
1035.845056	49653.043307	34.683712
1037.166670	49715.176409	34.688730
1037.701768	49767.353884	34.693748
1038.675985	49817.159687	34.698765
1040.168192	49879.026096	34.703783
1041.013172	49940.709290	34.708800
1042.460810	49995.768747	34.713818
1043.489644	50048.293471	34.718836
1044.962857	50114.649400	34.723853
1045.750519	50162.314961	34.728871
1046.443180	50217.062908	34.733888
1047.613100	50284.017273	34.738906
1048.872153	50332.406604	34.743924
1050.146101	50385.887088	34.748941
1051.445281	50439.711744	34.753959
1051.822792	50490.346384	34.758976
1052.734928	50559.860143	34.763994
1053.908126	50617.754368	34.769012
1055.345571	50673.588969	34.774029
1056.242708	50729.660154	34.779047
1057.427582	50793.943548	34.784064
1058.564356	50851.135405	34.789082
1059.424201	50905.631027	34.794100
1060.609760	50962.556102	34.799117
1061.399715	51031.590549	34.804135
1062.385188	51096.570376	34.809152
1063.574487	51161.119848	34.814170
1064.718668	51219.494680	34.819188
1066.189004	51272.123910	34.824205
1067.005750	51336.263970	34.829223
1067.750873	51387.399833	34.834240
1069.337290	51445.098560	34.839258
1070.830866	51509.430523	34.844276
1071.658217	51559.288393	34.849293
1072.576576	51625.583679	34.854311
1073.784627	51685.468292	34.859328
1074.977482	51732.282711	34.864346
1075.880155	51797.264811	34.869364
1077.087331	51846.026109	34.874381
1078.019183	51903.037511	34.879399
1079.160343	51959.446797	34.884416
1080.637618	52012.620799	34.889434
1081.165840	52070.613311	34.894452
1082.782458	52114.192005	34.899469
1083.585621	52172.920029	34.904487
1084.655386	52231.410302	34.909504
1085.991705	52272.976681	34.914522
1086.885932	52336.012677	34.919540
1088.266940	52389.398773	34.924557
1089.050081	52448.181247	34.929575
1089.998529	52499.667390	34.934592
1091.195462	52549.286016	34.939610
1092.255689	52611.005900	34.944628
1093.466218	52656.705724	34.949645
1094.397105	52708.055865	34.954663
1095.169860	52764.410879	34.959680
1096.678141	52808.336886	34.964698
1097.773774	52861.300482	34.969716
1098.776688	52892.200777	34.974733
1099.564781	52942.023460	34.979751
1100.432789	52990.460586	34.984768
1101.865587	53049.813620	34.989786
1102.178954	53091.168268	34.994804
1103.599152	53140.443129	34.999821
1104.280028	53199.800363	35.004839
1105.575829	53257.226363	35.009856
1106.815199	53311.712501	35.014874
1107.797952	53376.566231	35.019892
1108.978647	53440.794318	35.024909
1110.154387	53495.999583	35.029927
1111.470570	53557.947672	35.034944
1112.734615	53610.519572	35.039962
1113.622122	53682.938439	35.044980
1114.664839	53730.406858	35.049997
1115.877052	53801.864009	35.055015
1116.989223	53863.300627	35.060032
1117.810619	53914.265554	35.065050
1119.331064	53983.295620	35.070068
1120.555625	54041.740873	35.075085
1121.729209	54107.857694	35.080103
1122.532654	54162.901327	35.085120
1124.474920	54221.975066	35.090138
1125.253488	54285.888726	35.095156
1126.773998	54348.015741	35.100173
1127.759898	54408.068677	35.105191
1128.664568	54469.121696	35.110208
1129.974879	54519.808884	35.115226
1131.162936	54578.191573	35.120244
1132.035577	54629.270262	35.125261
1133.208514	54687.345500	35.130279
1134.334822	54762.907130	35.135296
1135.473684	54806.913707	35.140314
1136.584639	54879.617686	35.145332
1138.094673	54935.742239	35.150349
1139.281919	54996.277750	35.155367
1140.484802	55048.375148	35.160384
1142.081681	55105.701571	35.165402
1143.095274	55174.257571	35.170420
1144.140355	55215.159652	35.175437
1145.202567	55275.209172	35.180455
1146.116203	55339.161489	35.185472
1147.804366	55376.362241	35.190490
1148.763242	55436.415691	35.195508
1150.251971	55484.089943	35.200525
1151.328770	55534.841182	35.205543
1152.310621	55589.891850	35.210560
1153.474187	55636.376912	35.215578
1154.942793	55696.376533	35.220596
1156.134451	55743.983902	35.225613
1157.518524	55793.934484	35.230631
1157.837202	55839.925680	35.235648
1159.545890	55895.704978	35.240666
1160.442720	55952.491195	35.245684
1161.510135	56007.909157	35.250701
1163.036962	56063.128751	35.255719
1164.003473	56117.537514	35.260736
1165.264208	56161.470572	35.265754
1166.566085	56217.453546	35.270772
1167.100130	56265.139597	35.275789
1168.451624	56319.678414	35.280807
1169.413924	56375.670621	35.285824
1170.678444	56429.761304	35.290842
1172.098718	56491.067905	35.295860
1172.965755	56537.354327	35.300877
1174.369445	56587.069338	35.305895
1175.409256	56630.227754	35.310912
1176.302638	56665.630985	35.315930
1177.471768	56711.174275	35.320948
1178.696560	56765.575726	35.325965
1179.528100	56808.399994	35.330983
1180.254363	56866.246702	35.336000
1181.255502	56917.038049	35.341018
1182.512192	56987.371289	35.346036
1183.381595	57048.828852	35.351053
1184.575394	57112.311696	35.356071
1186.091726	57174.231582	35.361088
1187.534178	57237.922664	35.366106
1188.740941	57303.524209	35.371124
1189.819415	57368.146025	35.376141
1191.224957	57417.843488	35.381159
1191.989906	57495.318447	35.386176
1193.401154	57558.186153	35.391194
1194.735372	57622.224313	35.396212
1195.833281	57685.084443	35.401229
1197.312687	57752.543274	35.406247
1198.269565	57812.343515	35.411264
1199.593080	57869.421916	35.416282
1201.054154	57940.434822	35.421300
1202.132430	58009.033136	35.426317
1203.277512	58068.950121	35.431335
1204.640684	58140.687819	35.436352
1205.943970	58192.219391	35.441370
1206.891713	58252.281653	35.446388
1208.411480	58330.077849	35.451405
1209.844377	58389.513852	35.456423
1210.807730	58444.238526	35.461440
1212.240421	58522.213535	35.466458
1213.420350	58568.125762	35.471476
1214.730541	58637.841503	35.476493
1216.039998	58697.411518	35.481511
1217.252141	58761.218639	35.486528
1218.543467	58820.899397	35.491546
1219.934406	58880.393812	35.496564
1220.748071	58940.795247	35.501581
1222.035724	59004.850698	35.506599
1223.185295	59069.807736	35.511616
1224.903758	59123.105527	35.516634
1226.511397	59192.586415	35.521652
1227.327716	59248.595503	35.526669
1229.006163	59297.127461	35.531687
1229.808042	59356.189908	35.536704
1231.248031	59409.076194	35.541722
1232.529619	59460.841733	35.546740
1233.859409	59527.803588	35.551757
1234.855358	59575.734031	35.556775
1235.841482	59638.585091	35.561792
1237.172927	59695.388059	35.566810
1238.294049	59751.502501	35.571828
1239.588062	59819.008782	35.576845
1240.883585	59880.065033	35.581863
1242.142877	59937.772352	35.586880
1243.371942	59993.047589	35.591898
1244.639528	60049.279044	35.596916
1246.245099	60105.983090	35.601933
1247.595340	60153.340165	35.606951
1248.754081	60222.229643	35.611968
1250.026428	60266.851999	35.616986
1251.674173	60331.500217	35.622004
1252.508286	60383.154204	35.627021
1253.923904	60426.083345	35.632039
1254.901738	60491.919264	35.637056
1256.262882	60532.236552	35.642074
1257.451498	60576.809284	35.647092
1258.082662	60619.912208	35.652109
1259.511375	60667.321296	35.657127
1260.422403	60723.344266	35.662144
1261.106211	60766.312607	35.667162
1262.484229	60810.020562	35.672180
1263.435724	60873.899346	35.677197
1264.829046	60929.689037	35.682215
1266.060455	61000.810147	35.687232
1267.199870	61061.172168	35.692250
1268.518783	61128.811100	35.697268
1269.658544	61188.508727	35.702285
1271.284320	61264.240442	35.707303
1272.530134	61326.453831	35.712320
1273.893528	61398.277060	35.717338
1275.406236	61468.817430	35.722356
1276.255950	61533.422834	35.727373
1278.089090	61595.285426	35.732391
1279.532251	61660.197063	35.737408
1280.666913	61731.943129	35.742426
1282.075253	61794.999496	35.747444
1283.272829	61868.071783	35.752461
1284.827566	61924.939927	35.757479
1286.070302	61987.877117	35.762496
1287.289184	62055.876089	35.767514
1288.916658	62121.177886	35.772532
1289.866794	62186.737815	35.777549
1291.374926	62239.094140	35.782567
1292.713141	62303.789679	35.787584
1293.441230	62377.791563	35.792602
1294.938500	62439.430317	35.797620
1296.427891	62509.521527	35.802637
1297.626326	62565.535346	35.807655
1298.864796	62646.649477	35.812672
1300.150545	62719.843417	35.817690
1301.924486	62770.823535	35.822708
1303.153694	62848.103518	35.827725
1304.589473	62916.077231	35.832743
1305.623842	62977.093432	35.837760
1307.107346	63042.743055	35.842778
1308.835283	63108.278621	35.847796
1310.111847	63173.251963	35.852813
1311.233509	63243.769985	35.857831
1312.599660	63305.874559	35.862848
1314.068821	63371.438668	35.867866
1315.793099	63433.639436	35.872884
1316.979262	63490.727140	35.877901
1318.253138	63547.820237	35.882919
1318.938426	63602.454342	35.887936
1320.220643	63663.148547	35.892954
1321.485673	63739.267175	35.897972
1323.176821	63815.705505	35.902989
1324.204351	63876.370459	35.908007
1325.453681	63942.996063	35.913024
1326.782472	64015.794569	35.918042
1328.237315	64075.722054	35.923060
1329.643687	64149.426769	35.928077
1331.150749	64211.422910	35.933095
1332.343142	64276.494603	35.938112
1333.579102	64347.979131	35.943130
1335.020253	64409.530259	35.948148
1336.407215	64483.789782	35.953165
1337.713541	64539.594895	35.958183
1339.172621	64607.158062	35.963200
1340.744568	64671.430648	35.968218
1342.551997	64715.641742	35.973236
1343.802373	64787.302533	35.978253
1345.111131	64832.737799	35.983271
1346.474005	64876.429985	35.988288
1347.700343	64910.868709	35.993306
1348.911731	64964.442126	35.998324
1349.599355	65015.052423	36.003341
1350.802852	65058.567283	36.008359
1351.977059	65103.777192	36.013376
1353.235448	65175.482152	36.018394
1354.334352	65230.795794	36.023412
1355.860029	65302.490932	36.028429
1357.080993	65360.723380	36.033447
1358.780205	65427.244518	36.038464
1359.810240	65493.617334	36.043482
1361.325722	65553.456554	36.048500
1362.733094	65622.613334	36.053517
1363.971646	65684.984367	36.058535
1365.480626	65754.442162	36.063552
1366.781939	65824.534122	36.068570
1368.378014	65892.288226	36.073588
1369.323412	65964.645890	36.078605
1370.724654	66041.433945	36.083623
1372.578040	66111.965779	36.088640
1373.581861	66186.075030	36.093658
1375.226520	66239.975877	36.098676
1376.836550	66315.738063	36.103693
1378.095722	66376.708346	36.108711
1379.710204	66453.097050	36.113728
1380.682388	66524.591050	36.118746
1382.338040	66597.580114	36.123764
1383.548016	66670.784774	36.128781
1385.013165	66736.801492	36.133799
1386.392580	66803.142043	36.138816
1387.960937	66886.548207	36.143834
1389.552609	66954.394480	36.148852
1390.328493	67032.701677	36.153869
1392.170978	67113.761000	36.158887
1393.928891	67180.321876	36.163904
1394.686730	67253.795262	36.168922
1396.602925	67315.570367	36.173940
1398.039518	67392.325311	36.178957
1399.753403	67465.554682	36.183975
1401.309151	67532.135458	36.188992
1402.589208	67594.333727	36.194010
1404.209401	67656.250966	36.199028
1405.515856	67726.917215	36.204045
1406.886770	67794.160775	36.209063
1408.551191	67859.104474	36.214080
1409.928470	67917.539928	36.219098
1411.069850	67981.666701	36.224116
1412.990879	68049.609962	36.229133
1414.020621	68108.081255	36.234151
1415.732368	68179.825036	36.239168
1416.809891	68247.976838	36.244186
1418.688999	68308.886360	36.249204
1419.848934	68362.740938	36.254221
1421.447369	68430.938325	36.259239
1422.595713	68487.308732	36.264256
1423.883785	68556.606126	36.269274
1425.231234	68623.595925	36.274292
1426.600605	68690.316527	36.279309
1427.932120	68758.163982	36.284327
1429.540509	68822.966926	36.289344
1430.937277	68890.582897	36.294362
1432.317498	68963.710476	36.299380
1433.559771	69023.822231	36.304397
1434.968203	69097.490327	36.309415
1436.725941	69171.192605	36.314432
1437.637637	69232.692654	36.319450
1439.438842	69294.978102	36.324468
1441.018581	69357.754276	36.329485
1442.062669	69412.408030	36.334503
1443.258266	69469.387402	36.339520
1444.435512	69538.071566	36.344538
1445.589977	69585.052851	36.349556
1447.071652	69648.256670	36.354573
1448.414683	69718.359096	36.359591
1450.265624	69796.949682	36.364608
1451.282539	69859.897490	36.369626
1453.101662	69939.209028	36.374644
1454.508846	70006.161401	36.379661
1455.829417	70077.294138	36.384679
1457.538031	70145.238181	36.389696
1458.636451	70219.926833	36.394714
1460.648892	70285.379416	36.399732
1461.941607	70357.961051	36.404749
1463.102315	70431.044809	36.409767
1464.804952	70498.990713	36.414784
1466.471438	70571.983036	36.419802
1468.148480	70645.024570	36.424820
1469.600610	70710.717904	36.429837
1470.817778	70786.998030	36.434855
1472.766658	70860.339571	36.439872
1474.134699	70933.392284	36.444890
1475.705655	71003.931102	36.449908
1477.257289	71075.612987	36.454925
1478.602531	71142.565311	36.459943
1480.237534	71210.169032	36.464960
1481.746648	71296.651010	36.469978
1483.539589	71365.040979	36.474996
1484.882857	71433.868802	36.480013
1486.570360	71505.277294	36.485031
1488.302451	71576.830985	36.490048
1489.733837	71637.286473	36.495066
1491.172447	71697.550991	36.500084
1492.425870	71767.153670	36.505101
1493.754203	71846.991114	36.510119
1495.390083	71913.950579	36.515136
1496.924679	71997.150530	36.520154
1498.787458	72062.023052	36.525172
1500.286052	72134.020104	36.530189
1501.666249	72202.983483	36.535207
1503.361077	72269.947293	36.540224
1504.874068	72354.202999	36.545242
1506.225243	72413.976218	36.550260
1507.768252	72483.104832	36.555277
1509.272004	72549.668626	36.560295
1511.134193	72623.281983	36.565312
1512.181563	72694.971219	36.570330
1514.040504	72767.800207	36.575348
1515.277782	72828.998102	36.580365
1516.657872	72904.853564	36.585383
1518.282388	72969.461631	36.590400
1519.360850	73050.659082	36.595418
1520.974389	73119.145021	36.600436
1523.049082	73198.971062	36.605453
1524.533915	73275.989134	36.610471
1526.239436	73329.287260	36.615488
1527.672947	73405.883095	36.620506
1528.953807	73476.727266	36.625524
1530.572762	73555.245097	36.630541
1531.703110	73626.429880	36.635559
1533.600522	73687.830424	36.640576
1534.997837	73768.321515	36.645594
1536.750267	73839.295504	36.650612
1538.474922	73899.836933	36.655629
1539.765278	73966.931676	36.660647
1541.646307	74037.949400	36.665664
1543.015997	74097.432190	36.670682
1544.256356	74156.707358	36.675700
1545.603471	74201.399447	36.680717
1546.748723	74254.166461	36.685735
1548.735960	74320.443694	36.690752
1549.921636	74388.619874	36.695770
1551.315282	74449.062361	36.700788
1552.667639	74511.411447	36.705805
1554.132884	74588.347713	36.710823
1555.776033	74657.288978	36.715840
1557.051140	74735.256098	36.720858
1558.468085	74806.158500	36.725876
1559.921973	74882.160043	36.730893
1561.842909	74957.886032	36.735911
1563.339570	75032.107944	36.740928
1565.311594	75119.644624	36.745946
1566.717836	75199.986623	36.750964
1568.400700	75272.989359	36.755981
1569.513082	75361.117384	36.760999
1571.635561	75440.879320	36.766016
1572.839672	75524.243359	36.771034
1574.568752	75596.834392	36.776052
1576.673614	75675.687745	36.781069
1577.968329	75764.763926	36.786087
1579.775901	75831.503703	36.791104
1581.594764	75920.143678	36.796122
1582.843509	75996.357817	36.801140
1584.624866	76069.005276	36.806157
1586.657066	76150.974904	36.811175
1588.042683	76224.964131	36.816192
1589.737731	76307.620375	36.821210
1591.100816	76392.621653	36.826228
1592.980665	76457.464201	36.831245
1594.348574	76533.293841	36.836263
1596.146056	76614.034845	36.841280
1597.685101	76696.792698	36.846298
1598.922821	76775.835648	36.851316
1600.802582	76851.358047	36.856333
1602.595875	76938.865258	36.861351
1604.260240	77027.887734	36.866368
1605.940815	77102.213224	36.871386
1607.476012	77173.394692	36.876404
1609.475579	77249.444166	36.881421
1610.878520	77331.401834	36.886439
1612.560977	77405.094456	36.891456
1614.506929	77487.043614	36.896474
1615.798032	77561.824023	36.901492
1617.653523	77637.428409	36.906509
1619.063799	77716.485084	36.911527
1620.609729	77794.025909	36.916544
1622.503485	77868.294785	36.921562
1624.040985	77939.009165	36.926580
1625.965882	78009.333722	36.931597
1627.490400	78091.819377	36.936615
1628.860244	78161.230396	36.941632
1630.300807	78237.281431	36.946650
1631.694115	78324.982367	36.951668
1633.669197	78393.070409	36.956685
1635.246025	78483.720220	36.961703
1636.756847	78557.480813	36.966720
1638.679887	78630.898381	36.971738
1640.088830	78715.937714	36.976756
1641.819254	78790.019283	36.981773
1643.632955	78860.756154	36.986791
1645.165336	78934.691745	36.991808
1646.793982	79011.247570	36.996826
1648.476469	79100.159923	37.001844
1649.838131	79162.910963	37.006861
1651.156900	79237.210186	37.011879
1652.650591	79300.574318	37.016896
1654.359302	79364.766430	37.021914
1655.835142	79432.795821	37.026932
1657.410019	79509.133400	37.031949
1659.053891	79577.453573	37.036967
1660.310501	79648.837088	37.041984
1662.152559	79737.447797	37.047002
1663.605718	79811.233433	37.052020
1665.700914	79875.011508	37.057037
1667.192621	79975.371435	37.062055
1669.047806	80039.149443	37.067072
1670.671970	80115.987748	37.072090
1672.410165	80204.844251	37.077108
1674.049055	80280.781186	37.082125
1675.925297	80367.766882	37.087143
1677.588917	80438.341233	37.092160
1679.431976	80521.810509	37.097178
1680.978989	80598.117433	37.102196
1683.005394	80682.825445	37.107213
1684.246161	80758.559930	37.112231
1686.190571	80845.840518	37.117248
1688.034630	80924.445720	37.122266
1689.538584	81017.053670	37.127284
1691.203823	81090.226698	37.132301
1693.082282	81183.460751	37.137319
1694.634084	81275.441249	37.142336
1696.682904	81360.502560	37.147354
1698.214291	81451.916690	37.152372
1700.101101	81533.760397	37.157389
1701.501513	81614.704879	37.162407
1703.721407	81704.935136	37.167424
1705.547445	81785.357380	37.172442
1706.873792	81869.418340	37.177460
1708.714833	81943.643035	37.182477
1710.970259	82031.626176	37.187495
1712.442552	82124.420111	37.192512
1714.010322	82204.630568	37.197530
1715.832328	82292.872407	37.202548
1717.624543	82369.905990	37.207565
1719.345020	82458.303608	37.212583
1721.225214	82547.728146	37.217600
1722.809707	82624.427491	37.222618
1724.447146	82713.155660	37.227636
1726.662004	82802.300561	37.232653
1728.358852	82868.580534	37.237671
1729.871249	82951.817354	37.242688
1731.578884	83034.149596	37.247706
1732.995049	83119.441929	37.252724
1735.042116	83201.011980	37.257741
1736.901092	83288.250154	37.262759
1738.652456	83367.028726	37.267776
1740.807668	83453.118694	37.272794
1742.427924	83541.522701	37.277812
1743.842680	83612.511410	37.282829
1745.509378	83699.210748	37.287847
1747.500723	83775.431392	37.292864
1749.298071	83853.127086	37.297882
1750.909872	83938.277217	37.302900
1752.748879	84023.417387	37.307917
1754.005019	84107.711369	37.312935
1756.197820	84197.561003	37.317952
1757.817045	84273.156973	37.322970
1759.666870	84363.998467	37.327988
1761.221337	84446.928960	37.333005
1763.462834	84528.523067	37.338023
1764.643461	84611.069046	37.343040
1766.154782	84694.412486	37.348058
1767.598408	84758.962501	37.353076
1769.361699	84826.947259	37.358093
1771.260542	84896.418861	37.363111
1772.721100	84982.470087	37.368128
1774.541921	85045.631217	37.373146
1776.383471	85134.322296	37.378164
1778.006000	85208.817792	37.383181
1779.739309	85294.181018	37.388199
1780.973497	85385.134754	37.393216
1782.881620	85466.935756	37.398234
1784.583134	85561.111539	37.403252
1786.750898	85648.992848	37.408269
1788.528913	85739.267021	37.413287
1790.195443	85825.313870	37.418304
1791.615762	85921.270865	37.423322
1793.232421	86015.093920	37.428340
1795.160887	86110.008956	37.433357
1797.485998	86204.406040	37.438375
1799.058952	86301.924403	37.443392
1800.924485	86398.827064	37.448410
1802.835598	86500.943816	37.453428
1804.533857	86592.893168	37.458445
1806.366861	86696.632190	37.463463
1808.206144	86808.151343	37.468480
1810.474049	86894.994304	37.473498
1811.993700	87003.408829	37.478516
1814.121938	87107.419917	37.483533
1815.628708	87199.743300	37.488551
1817.674326	87306.619314	37.493568
1819.565065	87398.389011	37.498586
1821.732916	87501.102707	37.503604
1823.380884	87610.133022	37.508621
1825.364223	87706.920204	37.513639
1827.333662	87802.163818	37.518656
1829.543165	87894.328726	37.523674
1831.742267	87987.902225	37.528692
1833.198788	88079.881402	37.533709
1834.967864	88172.432923	37.538727
1836.924290	88266.235375	37.543744
1839.268529	88351.854115	37.548762
1840.876899	88454.810768	37.553780
1842.566482	88545.741092	37.558797
1843.985335	88635.434087	37.563815
1845.623670	88739.033363	37.568832
1847.621615	88842.044458	37.573850
1849.573025	88943.098855	37.578868
1851.387029	89035.531990	37.583885
1853.404593	89134.853137	37.588903
1855.172291	89233.972925	37.593920
1856.856580	89343.941774	37.598938
1858.946617	89446.218176	37.603956
1860.917265	89538.400242	37.608973
1862.997584	89638.156819	37.613991
1864.855217	89734.323963	37.619008
1866.890181	89832.390042	37.624026
1868.520724	89931.204102	37.629044
1870.231095	90029.423010	37.634061
1872.399105	90115.619386	37.639079
1874.039927	90225.078665	37.644096
1876.036862	90320.300718	37.649114
1878.057659	90416.672652	37.654132
1879.532822	90520.443066	37.659149
1881.248787	90612.414824	37.664167
1883.321139	90716.421985	37.669184
1885.144548	90810.532098	37.674202
1886.958620	90911.678021	37.679220
1888.615185	91008.476396	37.684237
1890.639330	91110.071726	37.689255
1892.138994	91201.331362	37.694272
1893.996315	91277.047523	37.699290
1895.794624	91368.818595	37.704308
1897.590367	91459.703154	37.709325
1899.269034	91545.752074	37.714343
1900.926105	91646.494104	37.719360
1902.730961	91743.879998	37.724378
1904.644091	91845.621917	37.729396
1906.391102	91944.221571	37.734413
1908.429885	92053.637890	37.739431
1910.130895	92167.366089	37.744448
1912.036093	92262.633981	37.749466
1913.630474	92377.013376	37.754484
1915.477158	92498.603610	37.759501
1917.900160	92605.731057	37.764519
1919.462851	92728.253873	37.769536
1921.876050	92837.791869	37.774554
1923.948741	92964.431179	37.779572
1925.674604	93073.241034	37.784589
1927.813725	93195.485400	37.789607
1929.631178	93309.224982	37.794624
1931.736788	93420.765142	37.799642
1933.633041	93533.897501	37.804660
1935.626155	93651.337332	37.809677
1937.411416	93767.783448	37.814695
1939.539513	93892.871551	37.819712
1941.766452	94007.943916	37.824730
1943.757942	94121.443790	37.829748
1945.492125	94242.919114	37.834765
1947.592894	94358.418141	37.839783
1949.475346	94480.428915	37.844800
1951.790960	94596.490959	37.849818
1954.022412	94714.911584	37.854836
1955.808681	94832.261518	37.859853
1958.016968	94949.976833	37.864871
1959.886254	95056.578359	37.869888
1961.935630	95177.450295	37.874906
1964.232939	95294.088222	37.879924
1965.542558	95407.674151	37.884941
1967.968114	95524.723852	37.889959
1969.731506	95653.488752	37.894976
1972.025974	95760.419111	37.899994
1974.150856	95880.128443	37.905012
1976.073710	96000.959988	37.910029
1978.283230	96101.085082	37.915047
1980.280035	96222.400277	37.920064
1982.253313	96320.332034	37.925082
1983.936831	96435.701236	37.930100
1986.057226	96559.013917	37.935117
1988.088293	96674.228201	37.940135
1989.913293	96792.555513	37.945152
1991.943232	96906.642626	37.950170
1993.688318	97019.684547	37.955188
1995.537428	97138.757297	37.960205
1997.763917	97255.096689	37.965223
1999.164128	97378.208347	37.970240
2001.400328	97497.690914	37.975258
2003.472378	97620.761774	37.980276
2005.415144	97758.114705	37.985293
2007.757528	97876.834156	37.990311
2009.658465	97995.001959	37.995328
2011.502007	98120.747299	38.000346
2013.483658	98238.434330	38.005364
2015.559774	98361.406005	38.010381
2017.944023	98483.987659	38.015399
2019.288415	98610.472238	38.020416
2021.516709	98739.291058	38.025434
2023.552670	98854.512493	38.030452
2025.170979	98962.599015	38.035469
2027.077134	99068.929428	38.040487
2028.932298	99181.264550	38.045504
2030.816376	99285.976437	38.050522
2032.821293	99393.839113	38.055540
2034.781538	99516.693901	38.060557
2037.148263	99631.093044	38.065575
2038.907337	99744.624177	38.070592
2040.591588	99862.503156	38.075610
2042.474779	99992.128974	38.080628
2044.418640	100132.369735	38.085645
2046.595788	100252.011279	38.090663
2048.235824	100392.706393	38.095680
2050.542585	100530.026908	38.100698
2052.319308	100666.885786	38.105716
2054.002814	100804.216232	38.110733
2056.174208	100947.683150	38.115751
2058.480705	101101.284703	38.120768
2060.265910	101243.380723	38.125786
2062.440594	101392.947268	38.130804
2064.490547	101542.001526	38.135821
2066.452650	101698.525056	38.140839
2068.774656	101857.249770	38.145856
2070.914624	102006.355445	38.150874
2073.050528	102164.933265	38.155892
2075.124487	102315.939766	38.160909
2077.065844	102472.203973	38.165927
2079.086007	102623.600657	38.170944
2081.455480	102782.423830	38.175962
2084.121912	102944.814757	38.180980
2086.057650	103098.217392	38.185997
2087.955665	103259.614351	38.191015
2090.206331	103421.781049	38.196032
2092.390978	103570.240155	38.201050
2094.520146	103728.471500	38.206068
2096.961952	103890.952911	38.211085
2098.823979	104037.575381	38.216103
2101.183912	104195.176908	38.221120
2103.547799	104342.330795	38.226138
2105.849079	104498.801788	38.231156
2107.594405	104663.094956	38.236173
2109.801457	104810.389548	38.241191
2111.735554	104962.811994	38.246208
2114.068660	105118.989262	38.251226
2116.483357	105270.830720	38.256244
2118.308835	105432.934193	38.261261
2120.631703	105569.068495	38.266279
2122.503561	105725.891324	38.271296
2124.611387	105890.235178	38.276314
2127.138763	106038.943194	38.281332
2129.221869	106206.525834	38.286349
2131.519881	106348.918402	38.291367
2133.622834	106508.485616	38.296384
2135.653637	106658.782967	38.301402
2138.004326	106804.149036	38.306420
2139.922282	106958.675200	38.311437
2142.106282	107099.123285	38.316455
2144.749737	107251.952216	38.321472
2146.883615	107404.037325	38.326490
2148.967694	107558.400710	38.331508
2151.461970	107700.349730	38.336525
2153.435125	107837.777803	38.341543
2155.678923	107983.989827	38.346560
2157.436208	108140.385129	38.351578
2159.738617	108269.001017	38.356596
2161.972130	108429.862835	38.361613
2163.831795	108568.135817	38.366631
2165.795377	108713.266160	38.371648
2167.449119	108851.014523	38.376666
2169.613015	108978.171033	38.381684
2171.558596	109113.972620	38.386701
2173.364075	109259.954244	38.391719
2175.274942	109397.740622	38.396736
2176.838624	109559.092883	38.401754
2178.845504	109709.204318	38.406772
2181.071298	109878.139323	38.411789
2183.183542	110032.281008	38.416807
2185.534375	110194.045649	38.421824
2187.592724	110361.715661	38.426842
2189.833205	110517.919177	38.431860
2191.608612	110688.881495	38.436877
2194.169016	110865.403229	38.441895
2196.228221	111035.435097	38.446912
2198.048326	111221.864757	38.451930
2200.675812	111395.106713	38.456948
2202.065648	111587.705599	38.461965
2204.659518	111762.489116	38.466983
2207.078759	111955.892766	38.472000
2208.899008	112150.025282	38.477018
2211.295628	112333.364864	38.482036
2213.624759	112525.339905	38.487053
2215.782493	112738.966230	38.492071
2218.149560	112927.031302	38.497088
2220.239664	113116.713316	38.502106
2222.967070	113308.008763	38.507124
2225.367724	113506.128873	38.512141
2227.411649	113693.944097	38.517159
2229.643797	113903.634002	38.522176
2231.891074	114097.836982	38.527194
2234.153486	114292.989845	38.532212
2236.375414	114490.369605	38.537229
2238.654012	114696.543601	38.542247
2240.805009	114887.823362	38.547264
2243.539234	115091.150684	38.552282
2245.808985	115290.074604	38.557300
2247.937168	115491.634509	38.562317
2250.234441	115698.825854	38.567335
2253.178869	115895.047376	38.572352
2255.160537	116088.452612	38.577370
2257.620260	116282.646546	38.582388
2259.610467	116476.382233	38.587405
2261.956806	116682.696206	38.592423
2264.073118	116871.974907	38.597440
2266.641832	117083.951327	38.602458
2269.041353	117279.326770	38.607476
2271.147569	117469.028629	38.612493
2273.042100	117669.064021	38.617511
2275.472106	117871.173002	38.622528
2277.476782	118076.165497	38.627546
2279.671097	118284.706396	38.632564
2282.364124	118488.350368	38.637581
2284.491004	118693.301705	38.642599
2286.865639	118902.502737	38.647616
2288.756269	119115.839690	38.652634
2291.383848	119321.578614	38.657652
2293.825803	119535.744943	38.662669
2295.817353	119748.308542	38.667687
2298.383078	119943.697028	38.672704
2300.806560	120149.941651	38.677722
2303.116054	120359.896529	38.682740
2305.198665	120575.012790	38.687757
2307.564303	120779.316319	38.692775
2310.284564	120973.417315	38.697792
2312.615642	121176.802319	38.702810
2314.840584	121378.568585	38.707828
2317.270811	121576.054183	38.712845
2319.529446	121746.052963	38.717863
2322.129432	121920.299449	38.722880
2324.030977	122096.888625	38.727898
2326.247747	122266.743980	38.732916
2328.006726	122453.949514	38.737933
2330.479699	122630.362883	38.742951
2332.660475	122819.508499	38.747968
2334.358722	123028.672605	38.752986
2336.362725	123211.948839	38.758004
2338.528795	123421.105249	38.763021
2340.497167	123638.476158	38.768039
2342.404080	123847.129841	38.773056
2344.740471	124078.755464	38.778074
2346.713297	124303.804403	38.783092
2349.494852	124541.845709	38.788109
2351.475428	124774.013072	38.793127
2353.884643	125019.613085	38.798144
2356.252024	125264.903965	38.803162
2358.293065	125498.436156	38.808180
2360.848012	125744.702824	38.813197
2363.171609	126004.087207	38.818215
2365.927158	126238.285739	38.823232
2368.021113	126477.955662	38.828250
2369.817117	126746.942441	38.833268
2372.419200	127005.807467	38.838285
2374.698357	127271.169695	38.843303
2377.544648	127519.152219	38.848320
2380.161671	127794.259462	38.853338
2382.843798	128058.802432	38.858356
2385.272591	128305.002581	38.863373
2387.371609	128571.352811	38.868391
2390.377728	128831.041390	38.873408
2393.051882	129097.076594	38.878426
2395.342085	129345.156903	38.883444
2397.587916	129602.317410	38.888461
2400.062393	129856.297099	38.893479
2402.347123	130117.222940	38.898496
2404.780588	130384.889848	38.903514
2407.348154	130643.516171	38.908532
2410.360542	130904.269528	38.913549
2412.711179	131157.540378	38.918567
2415.499514	131413.332669	38.923584
2417.280528	131675.920107	38.928602
2419.585649	131934.595206	38.933620
2421.952843	132200.037844	38.938637
2424.195118	132464.917954	38.943655
2426.981956	132736.160365	38.948672
2428.996710	132992.539712	38.953690
2431.277026	133270.767376	38.958708
2433.877742	133537.450442	38.963725
2436.099248	133817.276859	38.968743
2438.938653	134060.857005	38.973760
2441.579478	134349.795418	38.978778
2443.890736	134621.034919	38.983796
2446.510536	134898.420207	38.988813
2448.906820	135162.670517	38.993831
2451.294686	135435.146500	38.998848
2453.784075	135707.455965	39.003866
2456.079428	135983.058660	39.008884
2458.189970	136258.222409	39.013901
2460.738851	136540.006785	39.018919
2463.810630	136810.150587	39.023936
2465.730936	137090.628085	39.028954
2467.908528	137368.858967	39.033972
2470.871050	137654.900069	39.038989
2473.188449	137942.287489	39.044007
2475.650153	138221.113538	39.049024
2478.238072	138490.289518	39.054042
2480.244144	138756.423520	39.059060
2482.770106	139001.398772	39.064077
2485.152666	139255.839511	39.069095
2487.499803	139507.495218	39.074112
2489.868953	139783.667262	39.079130
2492.338176	140039.202732	39.084148
2494.279524	140299.835027	39.089165
2496.660142	140574.042762	39.094183
2499.109845	140843.647114	39.099200
2501.437801	141122.726858	39.104218
2503.752009	141407.686358	39.109236
2506.354709	141699.189141	39.114253
2508.083207	141986.121946	39.119271
2510.693430	142283.503106	39.124288
2513.298704	142584.783114	39.129306
2515.822040	142888.743000	39.134324
2518.077178	143207.215131	39.139341
2520.437557	143526.815093	39.144359
2523.006944	143827.295997	39.149376
2525.346629	144147.651981	39.154394
2527.879849	144472.041148	39.159412
2530.445451	144792.429354	39.164429
2532.779112	145133.683579	39.169447
2535.441255	145462.285385	39.174464
2537.935912	145803.366602	39.179482
2540.353854	146147.064016	39.184500
2543.080514	146489.915809	39.189517
2545.242748	146830.078503	39.194535
2547.780406	147172.126663	39.199552
2550.447340	147527.979163	39.204570
2552.560289	147886.230815	39.209588
2555.310125	148237.708842	39.214605
2557.719923	148594.662271	39.219623
2560.501664	148954.453925	39.224640
2563.073392	149318.088781	39.229658
2565.739673	149683.475663	39.234676
2568.522803	150038.984067	39.239693
2571.175376	150415.459265	39.244711
2574.197367	150782.536902	39.249728
2576.660733	151129.965945	39.254746
2579.379648	151497.133849	39.259764
2582.038588	151859.439194	39.264781
2584.685403	152233.058952	39.269799
2587.150262	152593.381117	39.274816
2590.346605	152941.836588	39.279834
2593.342757	153315.218499	39.284852
2596.276912	153645.287602	39.289869
2599.209348	154001.432716	39.294887
2602.348435	154324.276095	39.299904
2605.508755	154658.530159	39.304922
2608.371093	154975.593784	39.309940
2611.324217	155302.000759	39.314957
2613.985987	155628.290104	39.319975
2616.812757	155948.208158	39.324992
2619.225178	156275.428724	39.330010
2621.768217	156589.567784	39.335028
2624.357583	156912.613011	39.340045
2626.599745	157237.885118	39.345063
2628.940647	157567.853369	39.350080
2631.191642	157899.855995	39.355098
2633.663108	158233.400146	39.360116
2636.190653	158569.362127	39.365133
2638.662246	158921.863886	39.370151
2640.776752	159255.532917	39.375168
2643.673774	159596.216146	39.380186
2645.772789	159948.832816	39.385204
2648.258673	160292.085158	39.390221
2650.516867	160639.640702	39.395239
2652.982494	160976.679110	39.400256
2655.836719	161317.429153	39.405274
2657.825738	161649.975217	39.410292
2660.166687	161984.080331	39.415309
2662.560248	162333.617171	39.420327
2664.978682	162675.115449	39.425344
2667.475726	163032.117787	39.430362
2670.075037	163398.094923	39.435380
2672.624089	163763.142431	39.440397
2675.248862	164124.320441	39.445415
2677.919199	164489.022856	39.450432
2680.644136	164865.208948	39.455450
2683.005747	165247.916462	39.460468
2685.453265	165632.415600	39.465485
2687.808584	166024.358835	39.470503
2690.501989	166421.368180	39.475520
2693.008581	166831.093076	39.480538
2695.121140	167252.296456	39.485556
2698.138937	167650.696787	39.490573
2700.394279	168080.630940	39.495591
2702.529177	168511.995890	39.500608
2705.104733	168948.995515	39.505626
2707.739659	169400.971197	39.510644
2710.427621	169848.484627	39.515661
2713.188808	170311.911822	39.520679
2715.614225	170753.542113	39.525696
2718.817880	171207.865083	39.530714
2721.538239	171686.366420	39.535732
2724.075291	172147.084584	39.540749
2727.053379	172621.475496	39.545767
2729.388743	173095.157171	39.550784
2732.372438	173568.918078	39.555802
2734.707422	174046.097459	39.560820
2737.984092	174518.205560	39.565837
2740.679384	175003.130891	39.570855
2743.558634	175496.919090	39.575872
2746.403522	175970.982492	39.580890
2749.403889	176457.938518	39.585908
2752.685102	176928.408979	39.590925
2755.196667	177414.900959	39.595943
2758.337170	177887.481291	39.600960
2761.755907	178360.985792	39.605978
2764.549876	178824.583997	39.610996
2767.501171	179306.954227	39.616013
2770.537219	179774.430769	39.621031
2773.360504	180244.762177	39.626048
2775.852596	180720.405196	39.631066
2778.389120	181184.512999	39.636084
2781.202298	181714.361236	39.641101
2784.017952	182223.715593	39.646119
2786.255760	182696.868608	39.651136
2789.469965	183175.865316	39.656154
2791.973179	183664.423916	39.661172
2795.302773	184146.378985	39.666189
2798.088413	184624.154435	39.671207
2800.514525	185098.711897	39.676224
2803.699639	185584.277722	39.681242
2806.328889	186081.616469	39.686260
2809.121331	186560.873041	39.691277
2811.705151	187046.768304	39.696295
2814.352551	187538.421558	39.701312
2817.331685	188020.500230	39.706330
2820.121963	188513.964317	39.711348
2822.791514	188998.889661	39.716365
2825.371201	189494.295999	39.721383
2827.972161	189994.120798	39.726400
2831.097069	190491.605173	39.731418
2833.823269	190985.115333	39.736436
2836.559615	191461.886973	39.741453
2839.255402	191934.755132	39.746471
2841.348641	192402.258182	39.751488
2844.209876	192880.438238	39.756506
2846.744904	193365.021356	39.761524
2849.400818	193856.267872	39.766541
2852.473600	194351.896242	39.771559
2854.884418	194843.692802	39.776576
2857.656824	195324.512037	39.781594
2860.375794	195838.464766	39.786612
2863.205079	196328.143697	39.791629
2866.504945	196839.037265	39.796647
2869.330370	197350.514876	39.801664
2872.321199	197856.964252	39.806682
2875.207643	198374.252860	39.811700
2877.789780	198899.211400	39.816717
2880.585687	199420.556593	39.821735
2883.214438	199965.350393	39.826752
2886.152143	200495.974081	39.831770
2888.453696	201042.143546	39.836788
2891.076011	201589.610933	39.841805
2894.162617	202139.725501	39.846823
2896.713967	202712.889364	39.851840
2899.184549	203272.197843	39.856858
2901.746329	203845.490610	39.861876
2904.566755	204435.789891	39.866893
2907.539859	205019.640146	39.871911
2910.466062	205608.783221	39.876928
2913.687634	206204.943791	39.881946
2916.268876	206803.136783	39.886964
2919.257388	207406.932582	39.891981
2922.299893	208007.088868	39.896999
2925.282641	208620.872149	39.902016
2928.517081	209218.740529	39.907034
2931.363253	209824.393645	39.912052
2934.821436	210425.887881	39.917069
2938.782957	211017.346547	39.922087
2941.660899	211619.721570	39.927104
2944.702255	212215.086259	39.932122
2947.308015	212818.115872	39.937140
2950.031210	213422.677842	39.942157
2953.123591	214024.007663	39.947175
2956.363242	214636.747124	39.952192
2959.446366	215231.602362	39.957210
2962.310403	215842.446320	39.962228
2965.626901	216446.920215	39.967245
2968.697994	217057.453987	39.972263
2971.249603	217678.231303	39.977280
2974.101736	218277.623014	39.982298
2977.243281	218890.916849	39.987316
2979.786446	219520.131522	39.992333
2982.884800	220137.447055	39.997351
2986.083334	220756.982942	40.002368
2989.090940	221359.604603	40.007386
2991.835497	221986.122147	40.012404
2994.704322	222610.994702	40.017421
2997.797097	223233.012624	40.022439
3001.057516	223843.140805	40.027456
3004.529233	224457.503949	40.032474
3007.748932	225080.645574	40.037492
3010.562293	225690.920069	40.042509
3014.184775	226310.035625	40.047527
3017.083005	226915.901786	40.052544
3019.908260	227527.876176	40.057562
3022.783053	228147.768669	40.062580
3025.666709	228770.885807	40.067597
3028.306255	229382.532748	40.072615
3030.328045	230009.416698	40.077632
3033.389424	230612.842147	40.082650
3036.316132	231210.165811	40.087668
3039.206684	231807.748638	40.092685
3042.315359	232411.622352	40.097703
3045.116116	233020.344904	40.102720
3047.849825	233629.382073	40.107738
3050.756798	234239.686973	40.112756
3053.565777	234860.040867	40.117773
3056.915377	235478.048371	40.122791
3059.352585	236106.689320	40.127808
3062.210222	236763.867995	40.132826
3065.499647	237406.040593	40.137844
3067.767370	238061.784807	40.142861
3070.829893	238711.103302	40.147879
3073.425471	239391.129987	40.152896
3076.329786	240071.894287	40.157914
3079.307540	240751.934115	40.162932
3082.280656	241449.170911	40.167949
3085.673857	242135.772349	40.172967
3088.837322	242840.291545	40.177984
3091.808644	243542.298333	40.183002
3094.918925	244236.888911	40.188020
3098.162484	244947.612620	40.193037
3101.498635	245651.511455	40.198055
3104.336748	246375.147363	40.203072
3107.233969	247100.651098	40.208090
3110.512349	247820.427646	40.213108
3113.811865	248544.135383	40.218125
3117.093614	249279.146911	40.223143
3120.156235	250014.265719	40.228160
3123.796418	250750.052985	40.233178
3127.347491	251470.279405	40.238196
3129.914931	252203.865235	40.243213
3133.574560	252932.450394	40.248231
3136.283154	253676.980423	40.253248
3139.538701	254407.805890	40.258266
3142.762728	255153.085793	40.263284
3145.847687	255900.923475	40.268301
3149.074513	256645.178622	40.273319
3152.317341	257394.938979	40.278336
3155.341230	258136.524705	40.283354
3158.694161	258888.087753	40.288372
3161.742138	259649.549170	40.293389
3165.597218	260390.330702	40.298407
3168.384782	261148.368662	40.303424
3171.403934	261899.964571	40.308442
3174.758925	262654.957244	40.313460
3177.791042	263416.497447	40.318477
3180.956732	264171.077306	40.323495
3183.949882	264930.733137	40.328512
3186.879498	265692.298203	40.333530
3190.542553	266456.308103	40.338548
3193.603211	267228.279851	40.343565
3196.832931	267990.186661	40.348583
3199.806408	268775.798545	40.353600
3203.003598	269542.091803	40.358618
3206.900986	270309.589874	40.363636
3209.635737	271091.028680	40.368653
3213.035645	271855.899157	40.373671
3216.370199	272641.116218	40.378688
3219.356503	273418.253570	40.383706
3222.783511	274176.267412	40.388724
3225.845382	274949.518481	40.393741
3229.500002	275727.596423	40.398759
3233.039539	276503.678581	40.403776
3236.384439	277266.323904	40.408794
3239.644368	278034.587468	40.413812
3242.619200	278786.711257	40.418829
3246.005250	279523.094665	40.423847
3249.107333	280265.432201	40.428864
3251.630951	280991.854278	40.433882
3254.727811	281730.038566	40.438900
3257.800912	282474.948390	40.443917
3261.023384	283224.042402	40.448935
3263.652027	283973.094311	40.453952
3266.322209	284739.221163	40.458970
3269.502766	285504.574039	40.463988
3272.189942	286300.415570	40.469005
3275.162956	287072.918307	40.474023
3278.477482	287863.920042	40.479040
3281.564384	288669.065450	40.484058
3285.270328	289470.295292	40.489076
3288.466034	290290.434838	40.494093
3291.695768	291100.072022	40.499111
3295.007766	291931.546732	40.504128
3297.845761	292752.902898	40.509146
3301.280067	293581.949236	40.514164
3304.510119	294426.224092	40.519181
3307.460722	295268.118601	40.524199
3310.930924	296117.130002	40.529216
3314.497224	296979.493337	40.534234
3317.925415	297824.880824	40.539252
3320.891422	298699.954791	40.544269
3324.386422	299566.909991	40.549287
3327.673280	300429.847574	40.554304
3330.811513	301308.990954	40.559322
3334.395352	302186.679406	40.564340
3337.775880	303077.661558	40.569357
3341.304939	303950.277511	40.574375
3344.734334	304845.638704	40.579392
3347.699039	305722.475872	40.584410
3351.582255	306618.445665	40.589428
3354.924654	307520.169763	40.594445
3358.541646	308411.732258	40.599463
3362.221388	309301.568109	40.604480
3365.779879	310185.924149	40.609498
3369.834390	311074.399589	40.614516
3373.207801	311965.274517	40.619533
3376.580314	312851.107410	40.624551
3380.140291	313733.924688	40.629568
3383.193952	314639.518563	40.634586
3387.639662	315500.413330	40.639604
3390.657939	316393.440619	40.644621
3394.642766	317287.415557	40.649639
3398.147256	318148.685584	40.654656
3401.481496	319016.207965	40.659674
3405.144801	319897.110933	40.664692
3408.606932	320771.226635	40.669709
3412.577855	321631.085536	40.674727
3415.976160	322508.601056	40.679744
3419.742705	323365.614471	40.684762
3423.092388	324231.784458	40.689780
3426.498966	325094.019857	40.694797
3429.798413	325951.179269	40.699815
3433.361191	326812.186609	40.704832
3436.573214	327684.190723	40.709850
3440.264453	328535.017612	40.714868
3443.770267	329395.394340	40.719885
3447.507538	330264.189420	40.724903
3450.682992	331119.252032	40.729920
3454.142769	331983.257016	40.734938
3457.375754	332841.950590	40.739956
3460.640320	333710.766697	40.744973
3463.940226	334572.606639	40.749991
3467.464142	335430.789589	40.755008
3471.557540	336278.059402	40.760013
3475.215883	337066.919442	40.765018
3478.060871	337840.759009	40.770023
3481.968373	338548.148098	40.775028
3484.692993	339202.232104	40.780032
3487.535384	339813.871745	40.785037
3490.305247	340354.925064	40.790042
3492.714192	340855.419143	40.795047
3495.508628	341300.313353	40.800052
3498.038292	341699.246454	40.805056
3500.494403	342041.841550	40.810061
3502.248925	342339.513148	40.815066
3503.874641	342598.732766	40.820071
3505.915749	342809.805203	40.825076
3507.777133	342988.181529	40.830080
3508.866243	343124.928784	40.835085
3511.301365	343211.910645	40.840090
3511.842110	343274.093455	40.845095
3513.186867	343309.250278	40.850100
3514.237180	343302.653580	40.855104
3515.372682	343275.931973	40.860109
3516.649195	343220.508266	40.865114
3517.502582	343143.971078	40.870119
3517.792480	343044.892948	40.875124
3518.906323	342921.760058	40.880128
3519.340055	342788.333871	40.885133
3520.237921	342627.221973	40.890138
3520.616948	342458.206638	40.895143
3520.935709	342266.468823	40.900148
3521.614753	342061.706152	40.905152
3521.661373	341848.218130	40.910157
3522.204488	341626.184078	40.915162
3522.072595	341401.101211	40.920167
3522.395744	341150.798381	40.925172
3522.571633	340903.262935	40.930176
3522.796390	340645.343710	40.935181
3523.025210	340385.413182	40.940186
3523.317070	340118.198529	40.945191
3523.357104	339837.518952	40.950196
3523.760302	339556.398957	40.955200
3523.455234	339267.987798	40.960205
3523.795615	338979.727688	40.965210
3523.393964	338690.564111	40.970215
3523.372112	338395.642718	40.975220
3523.834657	338090.166320	40.980224
3523.771452	337794.966754	40.985229
3523.942808	337483.122520	40.990234
3523.691616	337182.174808	40.995239
3523.579691	336875.226754	41.000244
3523.825954	336564.685302	41.005248
3523.433558	336266.625737	41.010253
3523.433206	335943.554883	41.015258
3523.203107	335643.226978	41.020263
3523.232250	335329.301274	41.025268
3523.121560	335020.760795	41.030272
3522.741881	334715.616774	41.035277
3522.767280	334404.811919	41.040282
3522.901345	334110.772628	41.045287
3522.331802	333801.022177	41.050292
3522.458149	333491.847051	41.055296
3522.483512	333190.721888	41.060301
3522.265788	332880.501932	41.065306
3522.084750	332592.120693	41.070311
3522.086718	332287.126172	41.075316
3521.920718	331989.632901	41.080320
3521.696620	331687.797239	41.085325
3521.782474	331381.866755	41.090330
3521.250770	331089.917374	41.095335
3521.115068	330797.344313	41.100340
3521.054652	330490.463107	41.105344
3520.825772	330201.689836	41.110349
3520.568125	329904.067592	41.115354
3520.780593	329634.907662	41.120359
3519.976388	329349.906087	41.125364
3520.493538	329066.221980	41.130368
3520.167893	328784.931348	41.135373
3520.066267	328496.710595	41.140378
3519.856426	328218.780768	41.145383
3519.429359	327949.047937	41.150388
3519.562170	327671.493114	41.155392
3519.318266	327406.662599	41.160397
3519.193758	327131.891379	41.165402
3518.983459	326876.718009	41.170407
3518.847326	326598.994281	41.175412
3518.990760	326333.383874	41.180416
3518.294720	326074.033346	41.185421
3518.278355	325814.447705	41.190426
3518.104768	325560.099691	41.195431
3517.877197	325299.297329	41.200436
3518.024568	325062.498959	41.205440
3517.650140	324811.535472	41.210445
3517.321672	324556.874715	41.215450
3517.143593	324312.389660	41.220455
3516.988748	324072.096877	41.225460
3517.142067	323834.756280	41.230464
3516.836244	323586.343893	41.235469
3516.806617	323339.311420	41.240474
3516.777533	323108.660194	41.245479
3516.544453	322864.124299	41.250484
3516.406784	322641.017486	41.255488
3516.166370	322414.643844	41.260493
3516.148103	322167.602658	41.265498
3516.042697	321953.340156	41.270503
3515.890749	321717.739709	41.275508
3515.401346	321485.370720	41.280512
3515.206937	321279.666590	41.285517
3515.581942	321052.273572	41.290522
3515.335459	320841.538268	41.295527
3514.891843	320625.032278	41.300532
3515.123041	320410.989208	41.305536
3514.723184	320197.806952	41.310541
3514.881521	319981.000069	41.315546
3514.524560	319778.977629	41.320551
3514.102597	319562.844510	41.325556
3514.548549	319366.495218	41.330560
3513.936056	319165.451188	41.335565
3514.045945	318973.045201	41.340570
3513.892232	318775.921973	41.345575
3514.008847	318574.430478	41.350580
3513.891211	318378.521021	41.355584
3513.601348	318175.946350	41.360589
3513.761089	317979.915420	41.365594
3513.251286	317796.226031	41.370599
3513.428930	317601.946135	41.375604
3513.446006	317410.870800	41.380608
3512.918317	317230.642033	41.385613
3512.651478	317044.036515	41.390618
3512.688116	316860.130592	41.395623
3512.320628	316669.570155	41.400628
3512.628724	316502.616192	41.405632
3512.413114	316323.607109	41.410637
3512.347130	316147.550775	41.415642
3512.283475	315974.699245	41.420647
3511.848650	315804.398534	41.425652
3511.947524	315625.286612	41.430656
3511.502307	315465.290869	41.435661
3511.455389	315310.499137	41.440666
3511.639980	315136.384284	41.445671
3511.778395	314976.015685	41.450676
3511.037123	314816.827252	41.455680
3510.997995	314668.291329	41.460685
3510.765663	314509.632912	41.465690
3511.051733	314364.887227	41.470695
3510.512780	314197.599179	41.475700
3511.122596	314048.196455	41.480704
3510.655111	313898.681781	41.485709
3510.877098	313732.748853	41.490714
3510.592676	313586.563229	41.495719
3510.439318	313446.387054	41.500724
3510.396626	313301.485862	41.505728
3509.975226	313161.121724	41.510733
3509.922922	313012.735180	41.515738
3510.066620	312879.355546	41.520743
3509.712636	312739.539385	41.525748
3509.621923	312582.378902	41.530752
3509.727836	312458.189691	41.535757
3509.536239	312320.255282	41.540762
3509.463336	312191.233255	41.545767
3509.035672	312061.655644	41.550772
3509.376025	311934.985626	41.555776
3508.925286	311807.013990	41.560781
3509.118955	311674.132022	41.565786
3508.977573	311563.287209	41.570791
3508.614930	311432.934328	41.575796
3508.390011	311312.737917	41.580800
3508.579798	311195.478991	41.585805
3508.377144	311078.790049	41.590810
3508.670693	310958.384454	41.595815
3508.451205	310840.425253	41.600820
3508.393166	310724.476218	41.605824
3508.104454	310613.957574	41.610829
3507.983237	310496.847333	41.615834
3507.895352	310382.072663	41.620839
3508.007090	310275.053125	41.625844
3508.103161	310168.799193	41.630848
3507.527011	310073.312231	41.635853
3507.641360	309953.212032	41.640858
3507.615031	309852.447561	41.645863
3507.473805	309743.914141	41.650868
3507.872426	309639.571139	41.655872
3507.438233	309537.037604	41.660877
3507.463257	309438.376328	41.665882
3507.641284	309346.383478	41.670887
3507.171971	309243.345873	41.675892
3507.591401	309141.924950	41.680896
3507.291018	309045.145935	41.685901
3507.197645	308929.121759	41.690906
3507.168306	308837.872886	41.695911
3507.192389	308738.472366	41.700916
3506.950742	308637.764481	41.705920
3506.529749	308555.126608	41.710925
3506.553522	308460.713254	41.715930
3506.625308	308376.827458	41.720935
3506.142180	308282.213087	41.725940
3506.578218	308202.596121	41.730944
3506.146199	308118.432383	41.735949
3506.589298	308027.311719	41.740954
3506.543731	307948.431275	41.745959
3506.578780	307867.273254	41.750964
3506.497405	307770.050316	41.755968
3506.437768	307698.347941	41.760973
3506.241740	307614.706300	41.765978
3506.365213	307527.884475	41.770983
3506.132063	307441.627211	41.775988
3506.116048	307353.427252	41.780992
3506.371258	307279.995482	41.785997
3505.857258	307180.752286	41.791002
3505.772682	307107.398831	41.796007
3506.106210	307034.539761	41.801012
3506.294674	306957.478865	41.806016
3505.778775	306880.375281	41.811021
3505.751710	306794.186468	41.816026
3505.768568	306728.451077	41.821031
3505.419872	306654.069419	41.826036
3505.657618	306576.262229	41.831040
3505.422998	306515.655550	41.836045
3505.471519	306438.997461	41.841050
3505.111303	306372.811585	41.846055
3505.138431	306305.750713	41.851060
3505.537640	306234.279879	41.856064
3505.283821	306177.136795	41.861069
3505.658694	306098.442175	41.866074
3505.882370	306027.812847	41.871079
3505.179838	305964.148471	41.876084
3505.165244	305896.686398	41.881088
3505.258272	305825.339199	41.886093
3505.565450	305759.760744	41.891098
3505.670600	305690.371016	41.896103
3505.492122	305617.920775	41.901108
3504.959568	305546.187457	41.906112
3504.777408	305485.469542	41.911117
3504.873653	305418.167646	41.916122
3505.029122	305355.564466	41.921127
3504.757538	305303.385726	41.926132
3505.041976	305239.617034	41.931136
3504.647864	305187.075595	41.936141
3504.683468	305124.898056	41.941146
3504.453709	305070.294873	41.946151
3504.236366	305009.200153	41.951156
3504.768788	304949.031559	41.956160
3504.551459	304899.261597	41.961165
3504.755090	304840.773029	41.966170
3504.544053	304776.674034	41.971175
3504.550382	304722.389860	41.976180
3504.540819	304667.573676	41.981184
3504.482027	304627.373062	41.986189
3504.821019	304572.400486	41.991194
3504.514069	304507.985308	41.996199
3504.183154	304449.579866	42.001204
3504.346397	304395.881601	42.006208
3504.323399	304338.242275	42.011213
3504.424017	304283.153961	42.016218
3504.138905	304232.706812	42.021223
3504.137463	304194.838252	42.026228
3504.341038	304135.585405	42.031232
3504.105718	304080.752992	42.036237
3503.963804	304031.250344	42.041242
3503.979627	303991.164817	42.046247
3503.925568	303949.359605	42.051252
3504.014041	303906.335939	42.056256
3504.235213	303858.176095	42.061261
3504.081835	303807.148042	42.066266
3503.889714	303761.114153	42.071271
3503.592556	303716.420034	42.076276
3504.009085	303671.436150	42.081280
3503.735124	303626.636528	42.086285
3503.884993	303577.851325	42.091290
3503.703785	303522.220916	42.096295
3503.555193	303492.187967	42.101300
3503.545815	303449.230121	42.106304
3503.485861	303413.100734	42.111309
3503.425426	303367.453107	42.116314
3503.631178	303320.440426	42.121319
3503.659267	303282.897434	42.126324
3503.686196	303241.562542	42.131328
3503.769684	303209.380794	42.136333
3503.511811	303162.974904	42.141338
3503.361618	303128.284632	42.146343
3503.125853	303096.178177	42.151348
3503.637806	303051.611492	42.156352
3503.422287	303020.061727	42.161357
3503.205955	302984.898148	42.166362
3503.638932	302947.189815	42.171367
3503.398622	302915.440261	42.176372
3503.691144	302866.937496	42.181376
3503.506779	302825.482607	42.186381
3503.787735	302778.279530	42.191386
3503.473310	302727.071997	42.196391
3503.448711	302703.203629	42.201396
3503.559566	302661.702457	42.206400
3503.373741	302626.661119	42.211405
3503.661618	302590.069580	42.216410
3503.688408	302560.364982	42.221415
3503.296153	302518.967804	42.226420
3503.687430	302465.969962	42.231424
3503.287464	302434.754087	42.236429
3503.187261	302399.648312	42.241434
3503.351478	302364.959282	42.246439
3503.079642	302329.014977	42.251444
3503.593475	302288.544880	42.256448
3503.323174	302265.249188	42.261453
3503.324986	302225.240850	42.266458
3503.438351	302184.833283	42.271463
3503.129187	302145.815174	42.276468
3503.422682	302104.972176	42.281472
3503.205422	302085.638403	42.286477
3503.211720	302043.644080	42.291482
3503.244575	302008.797200	42.296487
3503.108515	301974.663873	42.301492
3503.278835	301934.756224	42.306496
3503.105070	301913.150479	42.311501
3503.201831	301873.636045	42.316506
3503.341075	301838.237956	42.321511
3503.155792	301806.479133	42.326516
3503.231197	301765.135505	42.331520
3502.935846	301746.526438	42.336525
3503.160658	301707.679032	42.341530
3503.236514	301675.039428	42.346535
3502.712994	301642.900723	42.351540
3503.337955	301607.248388	42.356544
3503.101241	301577.915297	42.361549
3503.019668	301543.976782	42.366554
3503.125122	301517.644266	42.371559
3502.829173	301486.258865	42.376564
3503.061654	301450.413277	42.381568
3502.953484	301431.240367	42.386573
3502.995367	301379.212299	42.391578
3503.013123	301364.957159	42.396583
3502.420218	301330.105863	42.401588
3502.794354	301298.284729	42.406592
3502.783952	301266.981812	42.411597
3502.964990	301247.560014	42.416602
3502.827342	301220.094612	42.421607
3502.525769	301197.337812	42.426612
3502.742533	301159.738367	42.431616
3502.751479	301143.015794	42.436621
3502.990663	301120.836147	42.441626
3502.786530	301092.719347	42.446631
3502.793787	301063.653244	42.451636
3502.929574	301033.421733	42.456640
3502.891229	301014.339562	42.461645
3502.651442	300984.166740	42.466650
3502.680873	300958.787526	42.471655
3502.566556	300926.584416	42.476660
3502.790325	300901.174793	42.481664
3502.555195	300883.523154	42.486669
3502.734901	300848.423499	42.491674
3502.669355	300830.465368	42.496679
3502.927276	300807.493675	42.501684
3502.930794	300764.073516	42.506688
3502.714629	300747.793234	42.511693
3502.559680	300714.756459	42.516698
3502.741411	300684.339410	42.521703
3502.607576	300672.831071	42.526708
3502.586871	300646.416047	42.531712
3502.752218	300617.324988	42.536717
3502.771102	300588.587679	42.541722
3502.479995	300559.746110	42.546727
3502.503447	300541.086783	42.551732
3502.494102	300507.670799	42.556736
3502.638650	300488.738009	42.561741
3502.559494	300474.421430	42.566746
3502.783479	300448.578887	42.571751
3502.669678	300419.709524	42.576756
3502.575126	300389.895434	42.581760
3502.460947	300365.276484	42.586765
3502.467480	300349.012169	42.591770
3502.685207	300325.206659	42.596775
3502.626575	300299.535486	42.601780
3502.614416	300276.987565	42.606784
3502.598776	300257.036228	42.611789
3502.173991	300223.939534	42.616794
3502.545021	300209.679761	42.621799
3502.193200	300180.872934	42.626804
3502.608508	300167.140708	42.631808
3502.641690	300147.359859	42.636813
3502.447469	300123.873180	42.641818
3502.406114	300101.202492	42.646823
3502.387764	300084.051184	42.651828
3502.677441	300048.221175	42.656832
3502.435521	300039.783787	42.661837
3502.672601	300004.343745	42.666842
3502.670014	299987.978941	42.671847
3502.647188	299966.679687	42.676852
3502.561382	299928.108626	42.681856
3502.573621	299915.279257	42.686861
3502.252590	299889.521657	42.691866
3502.556866	299863.793542	42.696871
3502.549021	299849.211133	42.701876
3502.538272	299817.729271	42.706880
3502.140559	299802.978737	42.711885
3502.076794	299775.348341	42.716890
3502.614072	299772.693882	42.721895
3502.705409	299751.885729	42.726900
3502.555080	299714.851708	42.731904
3502.580646	299700.696715	42.736909
3502.735094	299681.176707	42.741914
3502.704407	299643.284025	42.746919
3502.586207	299626.708122	42.751924
3502.932371	299595.806626	42.756928
3502.485835	299578.263969	42.761933
3502.431593	299563.026992	42.766938
3502.453516	299536.070277	42.771943
3502.134553	299513.162777	42.776948
3502.506444	299484.955088	42.781952
3502.499773	299471.517728	42.786957
3502.465593	299447.598508	42.791962
3502.371478	299420.405359	42.796967
3502.566660	299412.866708	42.801972
3502.279759	299376.490105	42.806977
3502.435463	299353.584685	42.811981
3502.457811	299338.004797	42.816986
3502.346183	299306.538412	42.821991
3502.101838	299298.584874	42.826996
3502.415865	299276.061900	42.832001
3502.516513	299268.945239	42.837005
3502.255594	299248.726457	42.842010
3502.554509	299230.227232	42.847015
3501.861346	299201.142379	42.852020
3501.973206	299176.843882	42.857025
3501.994618	299172.742928	42.862029
3502.117521	299153.431280	42.867034
3502.296667	299130.802073	42.872039
3501.855421	299126.264408	42.877044
3502.186023	299094.168820	42.882049
3502.142572	299093.157693	42.887053
3501.950216	299078.171242	42.892058
3502.026235	299055.685388	42.897063
3502.376182	299046.035425	42.902068
3502.245482	299017.778812	42.907073
3502.146412	299002.243263	42.912077
3502.012793	298992.923412	42.917082
3501.967315	298964.526188	42.922087
3502.034134	298955.200446	42.927092
3502.026764	298943.162929	42.932097
3501.873982	298928.501128	42.937101
3501.889876	298917.096270	42.942106
3501.885663	298910.097765	42.947111
3501.956221	298887.180011	42.952116
3502.131942	298865.289342	42.957121
3501.653746	298858.670359	42.962125
3501.467323	298851.903950	42.967130
3501.580153	298829.157728	42.972135
3501.435280	298827.500696	42.977140
3501.886692	298814.042463	42.982145
3501.701917	298827.561138	42.987149
3502.115505	298803.291662	42.992154
3502.015312	298772.535845	42.997159
3501.719241	298766.728297	43.002164
3502.242932	298765.043098	43.007169
3502.024261	298756.398259	43.012173
3501.891061	298737.508287	43.017178
3501.989576	298718.938413	43.022183
3501.717946	298704.422394	43.027188
3501.955224	298684.303682	43.032193
3501.934024	298684.205348	43.037197
3502.105811	298672.801520	43.042202
3502.274052	298650.148370	43.047207
3501.557828	298647.104431	43.052212
3501.855088	298626.670895	43.057217
3502.050269	298605.158865	43.062221
3501.897508	298594.823850	43.067226
3502.191704	298586.633300	43.072231
3501.834417	298580.988017	43.077236
3502.063831	298557.383533	43.082241
3501.762173	298562.750374	43.087245
3501.779384	298530.372576	43.092250
3501.890720	298512.360578	43.097255
3501.770946	298513.779338	43.102260
3502.149242	298484.984736	43.107265
3501.871439	298482.813979	43.112269
3501.795287	298465.111253	43.117274
3502.015776	298455.863211	43.122279
3502.138842	298444.085169	43.127284
3502.042757	298432.188673	43.132289
3501.901267	298415.030644	43.137293
3502.071366	298391.282649	43.142298
3502.440695	298390.028808	43.147303
3502.288097	298373.254288	43.152308
3502.090849	298353.203391	43.157313
3501.647665	298340.317595	43.162317
3502.035810	298311.037769	43.167322
3502.136791	298309.367738	43.172327
3501.585624	298301.971072	43.177332
3501.896237	298288.891058	43.182337
3501.863671	298272.225003	43.187341
3501.837390	298262.201034	43.192346
3501.880855	298255.042278	43.197351
3501.841683	298234.992077	43.202356
3501.963854	298224.130415	43.207361
3501.841222	298215.546835	43.212365
3502.021590	298201.825400	43.217370
3502.078749	298183.872671	43.222375
3501.547402	298179.628990	43.227380
3501.367854	298170.468896	43.232385
3501.692877	298162.629799	43.237389
3501.667028	298140.388572	43.242394
3501.920010	298122.048874	43.247399
3501.762733	298129.480284	43.252404
3501.824357	298124.431226	43.257409
3502.046197	298104.620148	43.262413
3501.608067	298092.980675	43.267418
3501.722951	298075.731555	43.272423
3501.720968	298084.360411	43.277428
3501.821273	298047.362446	43.282433
3501.725318	298052.671723	43.287437
3501.633177	298035.505862	43.292442
3501.818124	298037.080614	43.297447
3501.662682	298019.008355	43.302452
3501.878919	297995.558409	43.307457
3501.904033	297989.293325	43.312461
3501.716788	297982.425129	43.317466
3501.852950	297958.427731	43.322471
3501.485232	297963.168643	43.327476
3501.770288	297945.307471	43.332481
3501.596883	297950.934296	43.337485
3501.650635	297940.668684	43.342490
3501.950450	297922.983365	43.347495
3501.784743	297907.101593	43.352500
3501.836192	297898.821631	43.357505
3501.861934	297903.526487	43.362509
3501.775599	297883.483535	43.367514
3501.972151	297869.708584	43.372519
3501.559575	297856.741532	43.377524
3501.565383	297855.900849	43.382529
3501.759038	297832.199839	43.387533
3501.626451	297823.439587	43.392538
3502.077217	297812.144684	43.397543
3502.043262	297817.469743	43.402548
3502.266984	297787.782656	43.407553
3502.139871	297774.185546	43.412557
3502.248882	297761.696885	43.417562
3502.364939	297739.484219	43.422567
3502.165327	297744.249774	43.427572
3502.261857	297713.055375	43.432577
3502.028792	297702.630939	43.437581
3502.013433	297682.118671	43.442586
3502.078894	297659.786620	43.447591
3502.025031	297656.893598	43.452596
3502.302016	297635.088427	43.457601
3502.040699	297620.036007	43.462605
3501.986082	297615.157791	43.467610
3501.944968	297597.245691	43.472615
3501.818213	297580.314177	43.477620
3501.949321	297569.043748	43.482625
3501.457753	297542.013629	43.487629
3501.410559	297525.782336	43.492634
3501.939791	297531.350258	43.497639
3501.883149	297521.789052	43.502644
3502.042991	297513.313919	43.507649
3501.932934	297490.932884	43.512653
3501.699645	297495.805535	43.517658
3502.175882	297492.956892	43.522663
3501.999661	297470.153496	43.527668
3502.032421	297447.724664	43.532673
3502.039779	297454.265030	43.537677
3502.173501	297422.046546	43.542682
3502.077053	297403.888508	43.547687
3501.995120	297391.633239	43.552692
3502.062717	297375.511220	43.557697
3502.451179	297362.189745	43.562701
3502.430500	297335.722229	43.567706
3502.314652	297313.571104	43.572711
3501.829684	297300.411619	43.577716
3502.199577	297282.307898	43.582721
3502.289518	297265.164241	43.587725
3502.196535	297254.921445	43.592730
3502.251376	297232.870867	43.597735
3502.099183	297225.768023	43.602740
3501.941774	297204.641467	43.607745
3502.149644	297199.671273	43.612749
3501.973606	297179.998434	43.617754
3502.274878	297155.033124	43.622759
3501.913686	297154.580695	43.627764
3502.353994	297125.775703	43.632769
3502.279079	297123.064115	43.637773
3502.236440	297102.963147	43.642778
3502.177716	297065.251266	43.647783
3502.081819	297060.837609	43.652788
3502.215132	297037.298418	43.657793
3502.185452	297039.314000	43.662797
3502.242318	297019.324710	43.667802
3502.250780	296992.216154	43.672807
3502.069323	296986.874108	43.677812
3502.118716	296964.366125	43.682817
3502.057058	296953.482052	43.687821
3502.023220	296936.739442	43.692826
3502.005836	296908.922203	43.697831
3501.860586	296906.272507	43.702836
3501.784607	296892.590832	43.707841
3501.602737	296878.467554	43.712845
3502.044744	296864.603078	43.717850
3501.977844	296858.963128	43.722855
3501.947815	296849.448553	43.727860
3501.870786	296819.527994	43.732865
3502.064861	296820.312309	43.737869
3501.652243	296809.177642	43.742874
3501.870095	296785.116068	43.747879
3501.795932	296780.902616	43.752884
3502.150874	296776.978420	43.757889
3501.951224	296756.494628	43.762893
3501.983929	296744.653999	43.767898
3501.805031	296731.573796	43.772903
3502.038079	296719.040060	43.777908
3502.039956	296695.495823	43.782913
3502.190090	296693.334451	43.787917
3501.744068	296677.394346	43.792922
3501.754801	296655.350440	43.797927
3501.818659	296650.199088	43.802932
3501.848431	296651.212718	43.807937
3502.166114	296630.978891	43.812941
3501.810271	296609.348622	43.817946
3501.937428	296596.373258	43.822951
3501.654612	296592.879647	43.827956
3501.807596	296562.312119	43.832961
3501.757972	296562.294583	43.837965
3501.358803	296553.957609	43.842970
3501.666123	296548.335482	43.847975
3501.651520	296561.242673	43.852980
3501.809570	296531.896087	43.857985
3501.570062	296522.134222	43.862989
3501.982527	296516.699279	43.867994
3501.979990	296505.474986	43.872999
3501.686543	296480.449641	43.878004
3501.715681	296474.870997	43.883009
3501.590981	296463.436717	43.888013
3501.539239	296469.401012	43.893018
3501.813382	296449.784805	43.898023
3501.552922	296436.513661	43.903028
3501.591503	296426.021067	43.908033
3501.968650	296418.733551	43.913037
3501.661369	296418.756298	43.918042
3501.910993	296385.297353	43.923047
3501.698789	296391.668542	43.928052
3501.777995	296389.009183	43.933057
3501.719364	296379.931707	43.938061
3501.693310	296365.962114	43.943066
3501.858894	296349.493593	43.948071
3501.735676	296356.054500	43.953076
3501.818169	296350.314783	43.958081
3501.750096	296338.286200	43.963085
3501.649173	296315.979634	43.968090
3501.787382	296307.100452	43.973095
3501.617694	296305.294505	43.978100
3502.056814	296289.343174	43.983105
3502.076087	296278.166334	43.988109
3501.405390	296264.424767	43.993114
3501.370654	296259.085168	43.998119
3501.202051	296258.602621	44.003124
3501.707908	296248.036941	44.008129
3501.974371	296234.174304	44.013133
3501.740427	296222.018909	44.018138
3501.854610	296208.790953	44.023143
3501.662729	296212.944547	44.028148
3501.654901	296187.848966	44.033153
3501.917509	296176.455890	44.038157
3501.916521	296175.234444	44.043162
3501.799134	296164.893454	44.048167
3501.821774	296151.348903	44.053172
3501.548190	296132.887260	44.058177
3501.625936	296131.398971	44.063181
3501.521367	296134.724413	44.068186
3501.472009	296125.441820	44.073191
3501.589961	296099.435669	44.078196
3501.554096	296083.253100	44.083201
3501.542680	296090.661972	44.088205
3501.706932	296089.083798	44.093210
3502.074154	296079.812429	44.098215
3501.598435	296069.120189	44.103220
3501.782389	296044.732711	44.108225
3501.607164	296053.999841	44.113229
3501.625228	296045.241215	44.118234
3502.122600	296027.193527	44.123239
3501.852865	296021.992459	44.128244
3501.973966	295999.294712	44.133249
3502.132998	295990.692212	44.138253
3501.844907	295974.167244	44.143258
3501.915978	295953.717201	44.148263
3501.978218	295954.420326	44.153268
3501.688004	295936.902996	44.158273
3501.947466	295914.336304	44.163277
3501.709130	295913.584669	44.168282
3501.730839	295907.141714	44.173287
3501.530016	295885.512389	44.178292
3501.791161	295874.424924	44.183297
3501.836678	295880.628610	44.188301
3501.795012	295868.188544	44.193306
3501.793902	295848.869700	44.198311
3501.363095	295842.675660	44.203316
3501.963700	295833.876834	44.208321
3501.808135	295830.897805	44.213325
3501.643107	295828.505685	44.218330
3501.959287	295799.923061	44.223335
3501.915768	295789.443187	44.228340
3501.945231	295784.958925	44.233345
3501.791151	295769.405634	44.238349
3501.656925	295753.441978	44.243354
3501.791720	295747.897652	44.248359
3501.810541	295747.233078	44.253364
3501.292793	295735.885556	44.258369
3501.745580	295723.164528	44.263373
3501.904022	295700.893535	44.268378
3502.054617	295701.302861	44.273383
3501.689772	295688.073316	44.278388
3501.908568	295679.588694	44.283393
3502.054430	295670.250054	44.288397
3502.078543	295666.861122	44.293402
3502.142656	295647.226571	44.298407
3501.804341	295629.843936	44.303412
3501.868666	295620.263499	44.308417
3501.522913	295608.150908	44.313421
3501.406668	295594.653393	44.318426
3502.055547	295589.741381	44.323431
3501.958676	295582.909672	44.328436
3501.727946	295557.339594	44.333441
3502.294905	295544.218874	44.338445
3501.734989	295538.604964	44.343450
3501.922608	295520.860082	44.348455
3501.906686	295509.332245	44.353460
3501.782074	295502.963028	44.358465
3501.988530	295489.465946	44.363469
3502.204104	295478.690972	44.368474
3502.014942	295453.827052	44.373479
3501.644446	295451.899751	44.378484
3501.851740	295427.991983	44.383489
3501.989374	295414.149291	44.388493
3501.875931	295415.134425	44.393498
3501.973665	295397.250836	44.398503
3501.867075	295382.784523	44.403508
3501.916615	295364.348478	44.408513
3501.899848	295358.878718	44.413517
3501.689065	295336.207144	44.418522
3501.951733	295323.821196	44.423527
3501.523313	295317.219467	44.428532
3501.707031	295328.237808	44.433537
3501.426834	295304.660741	44.438541
3501.453585	295285.515529	44.443546
3502.017233	295279.013232	44.448551
3501.535870	295275.245137	44.453556
3501.967478	295276.934125	44.458561
3501.857602	295262.926464	44.463565
3501.718721	295248.414258	44.468570
3501.654796	295235.952084	44.473575
3501.342134	295241.499131	44.478580
3501.642553	295226.969148	44.483585
3502.021449	295209.194266	44.488589
3501.701938	295205.731761	44.493594
3501.791538	295195.383690	44.498599
3501.652771	295208.590587	44.503604
3501.740985	295181.799608	44.508609
3501.723567	295157.545054	44.513613
3501.687032	295154.929187	44.518618
3501.766417	295146.669914	44.523623
3501.680263	295146.352644	44.528628
3501.720670	295127.841590	44.533633
3502.028154	295110.536011	44.538637
3501.622542	295114.214022	44.543642
3501.971888	295091.785681	44.548647
3501.718530	295080.905771	44.553652
3501.671356	295069.000925	44.558657
3501.645223	295063.048979	44.563661
3501.424066	295068.988998	44.568666
3501.632466	295045.488162	44.573671
3501.547737	295030.967436	44.578676
3501.537163	295014.856976	44.583681
3501.550060	295027.785664	44.588685
3501.273981	295016.934748	44.593690
3501.227625	295020.862044	44.598695
3501.548743	295019.081140	44.603700
3501.547483	295020.150558	44.608705
3501.453810	294999.064134	44.613709
3501.304939	294987.938786	44.618714
3501.835242	294975.638193	44.623719
3502.035775	294987.086685	44.628724
3501.822372	294978.389540	44.633729
3501.122402	294966.434008	44.638733
3501.544168	294953.743117	44.643738
3501.743924	294941.417832	44.648743
3501.713309	294938.317407	44.653748
3501.585151	294934.672246	44.658753
3501.679258	294935.395855	44.663757
3501.656751	294913.458297	44.668762
3501.351801	294897.470189	44.673767
3501.556352	294897.387462	44.678772
3501.538378	294897.823147	44.683777
3501.924520	294891.755821	44.688781
3501.816517	294882.736736	44.693786
3501.901918	294861.571359	44.698791
3501.712479	294854.728583	44.703796
3501.921552	294849.096198	44.708801
3502.050523	294825.505875	44.713805
3501.944670	294823.537178	44.718810
3502.018100	294810.595268	44.723815
3501.912896	294798.597624	44.728820
3501.782818	294779.578581	44.733825
3501.744916	294772.712104	44.738829
3501.892261	294767.394809	44.743834
3501.692014	294748.106733	44.748839
3501.715869	294741.739676	44.753844
3501.676064	294731.691748	44.758849
3501.697848	294741.691904	44.763853
3501.637786	294717.138388	44.768858
3501.859875	294698.573340	44.773863
3501.571407	294688.920636	44.778868
3501.840451	294686.486060	44.783873
3502.107485	294674.099293	44.788877
3501.813940	294666.738237	44.793882
3501.912989	294647.097887	44.798887
3501.927031	294649.004901	44.803892
3501.709978	294628.395805	44.808897
3501.836241	294613.714720	44.813901
3501.544527	294610.553282	44.818906
3501.706346	294605.106439	44.823911
3502.014291	294590.371489	44.828916
3501.911236	294565.341004	44.833921
3502.118083	294561.541629	44.838925
3501.754649	294553.351503	44.843930
3502.293243	294522.722613	44.848935
3502.014259	294525.540880	44.853940
3501.842700	294504.771904	44.858945
3501.809569	294479.628634	44.863949
3501.560984	294484.529383	44.868954
3501.802542	294479.426419	44.873959
3501.876928	294473.305974	44.878964
3501.944492	294438.907118	44.883969
3501.954064	294429.665949	44.888973
3501.649952	294431.215444	44.893978
3501.871050	294406.770566	44.898983
3501.413508	294404.271394	44.903988
3501.359998	294399.799999	44.908993
3501.346319	294401.253180	44.913997
3501.461037	294398.308184	44.919002
3501.419620	294389.736787	44.924007
3501.413833	294386.759721	44.929012
3501.784929	294376.723854	44.934017
3502.022816	294355.381730	44.939021
3501.921053	294360.081357	44.944026
3501.689544	294360.524977	44.949031
3501.886482	294330.254851	44.954036
3502.059661	294334.402413	44.959041
3501.915675	294321.367115	44.964045
3501.922122	294300.035701	44.969050
3502.057579	294279.193192	44.974055
3501.887736	294276.827215	44.979060
3501.812477	294266.072034	44.984065
3502.007678	294243.642015	44.989069
3501.742167	294240.476460	44.994074
3501.654996	294236.952118	44.999079
3501.839828	294210.807399	45.004084
3501.317968	294204.194697	45.009089
3501.605638	294188.088291	45.014093
3501.671421	294193.932630	45.019098
3501.653860	294177.823033	45.024103
3501.447864	294184.880755	45.029108
3501.497555	294171.382423	45.034113
3501.764750	294146.446600	45.039117
3501.315955	294155.273171	45.044122
3501.734991	294141.055280	45.049127
3501.768999	294150.188183	45.054132
3501.597164	294144.818916	45.059137
3501.783058	294123.535746	45.064141
3501.788323	294124.655068	45.069146
3501.808710	294106.884995	45.074151
3501.766127	294110.251769	45.079156
3501.560528	294085.949830	45.084161
3501.655949	294073.564313	45.089165
3501.716861	294064.696874	45.094170
3501.756311	294055.960061	45.099175
3502.060170	294049.396428	45.104180
3501.908606	294030.558682	45.109185
3501.528677	294016.058403	45.114189
3501.617330	294023.324622	45.119194
3501.800771	294007.819910	45.124199
3501.772139	293983.286628	45.129204
3501.478640	293982.823588	45.134209
3501.880244	293973.775600	45.139213
3501.715569	293972.426974	45.144218
3501.358558	293941.785077	45.149223
3501.439726	293941.314370	45.154228
3501.457249	293938.002731	45.159233
3501.793966	293920.743141	45.164237
3501.608289	293936.070365	45.169242
3501.521364	293921.575163	45.174247
3501.665745	293902.971106	45.179252
3501.560128	293896.166021	45.184257
3501.823422	293883.397859	45.189261
3501.302504	293888.875775	45.194266
3501.336414	293876.372562	45.199271
3501.649422	293882.076462	45.204276
3501.467937	293875.919595	45.209281
3501.707353	293846.278939	45.214285
3501.445743	293844.920011	45.219290
3501.656324	293840.636374	45.224295
3501.590416	293838.254130	45.229300
3501.471765	293846.163684	45.234305
3502.102794	293828.908963	45.239309
3501.391015	293812.627804	45.244314
3501.560102	293803.997957	45.249319
3501.479382	293806.785261	45.254324
3501.290617	293803.836773	45.259329
3501.568086	293798.524502	45.264333
3501.333145	293792.732344	45.269338
3501.815117	293767.050062	45.274343
3501.781399	293762.295526	45.279348
3501.575488	293756.957005	45.284353
3501.770405	293745.574039	45.289357
3501.624591	293748.422431	45.294362
3501.504078	293733.856072	45.299367
3501.444531	293729.232843	45.304372
3501.226643	293722.521655	45.309377
3501.683695	293716.112216	45.314381
3501.322406	293715.863407	45.319386
3501.638829	293712.988659	45.324391
3501.692786	293711.045849	45.329396
3501.515941	293688.622878	45.334401
3501.935296	293682.499327	45.339405
3501.764431	293678.682584	45.344410
3501.688717	293674.952783	45.349415
3501.706210	293662.095730	45.354420
3501.800507	293639.732167	45.359425
3501.813289	293630.184918	45.364429
3501.813902	293633.621330	45.369434
3501.593548	293621.361450	45.374439
3501.618677	293598.474143	45.379444
3501.387038	293595.685074	45.384449
3501.594484	293585.445569	45.389453
3501.537290	293590.087379	45.394458
3501.556959	293586.851749	45.399463
3501.463145	293571.288452	45.404468
3501.390783	293559.107241	45.409473
3502.006889	293550.738379	45.414477
3501.865795	293552.007866	45.419482
3501.713812	293554.093598	45.424487
3501.790993	293532.776304	45.429492
3501.305200	293520.405175	45.434497
3501.593685	293514.022068	45.439501
3501.485006	293508.973778	45.444506
3501.769456	293496.685860	45.449511
3501.576426	293490.912575	45.454516
3501.468261	293485.711475	45.459521
3501.690496	293473.840552	45.464525
3501.746618	293473.679210	45.469530
3501.494517	293459.413356	45.474535
3501.700610	293473.712177	45.479540
3501.859301	293455.309379	45.484545
3502.209786	293432.345687	45.489549
3501.384840	293433.671181	45.494554
3501.829776	293420.925431	45.499559
3501.662876	293404.813517	45.504564
3501.579645	293386.423065	45.509569
3501.839988	293385.669796	45.514573
3501.764013	293386.827288	45.519578
3501.439089	293373.234615	45.524583
3501.895878	293354.250636	45.529588
3501.648372	293344.769490	45.534593
3501.561753	293341.015918	45.539597
3501.140484	293338.460120	45.544602
3501.401669	293339.513992	45.549607
3501.534030	293344.075277	45.554612
3501.361087	293318.215192	45.559617
3501.732145	293303.011874	45.564621
3501.471682	293305.470939	45.569626
3501.927678	293301.174350	45.574631
3501.796983	293304.351309	45.579636
3501.536098	293290.188605	45.584641
3501.511772	293257.916161	45.589645
3501.318717	293263.546511	45.594650
3501.522532	293257.074796	45.599655
3501.988156	293251.860333	45.604660
3501.503832	293260.132590	45.609665
3501.901584	293234.335973	45.614669
3501.745226	293223.338736	45.619674
3501.709606	293212.780804	45.624679
3501.574177	293200.100287	45.629684
3501.669733	293200.543691	45.634689
3501.554311	293189.769139	45.639693
3501.758058	293171.206482	45.644698
3501.615890	293165.017940	45.649703
3501.659804	293169.185793	45.654708
3501.457766	293159.595690	45.659713
3501.369746	293138.558629	45.664717
3501.486835	293143.096863	45.669722
3501.547625	293130.105653	45.674727
3501.619439	293129.127309	45.679732
3501.397860	293121.067534	45.684737
3501.720204	293123.817309	45.689741
3501.543791	293117.125023	45.694746
3501.399731	293098.998540	45.699751
3501.707208	293086.070572	45.704756
3501.739040	293085.582116	45.709761
3501.585621	293073.948026	45.714765
3501.431165	293082.728738	45.719770
3501.330177	293068.413710	45.724775
3501.391154	293054.175176	45.729780
3501.197067	293030.431010	45.734785
3501.415661	293037.193394	45.739789
3501.573224	293039.383478	45.744794
3501.826144	293036.009533	45.749799
3501.983603	293034.915979	45.754804
3501.655864	293018.218194	45.759809
3501.338029	293007.042526	45.764813
3501.360464	292987.795427	45.769818
3501.339699	292944.907646	45.774823
3501.423251	292839.232110	45.779828
3501.386484	292703.462154	45.784833
3501.063114	292505.983134	45.789837
3501.084116	292259.041481	45.794842
3501.132827	291973.275437	45.799847
3500.384202	291628.092862	45.804852
3500.184862	291249.806791	45.809857
3499.870248	290823.476266	45.814861
3499.523177	290333.686608	45.819866
3498.994182	289808.639536	45.824871
3498.682689	289231.979757	45.829876
3497.902104	288612.773943	45.834881
3497.640274	287947.277071	45.839885
3497.122729	287236.041638	45.844890
3496.314481	286472.198233	45.849895
3495.966613	285656.544191	45.854900
3494.876930	284800.619959	45.859905
3494.279923	283892.036642	45.864909
3493.209185	282951.972271	45.869914
3492.284976	281961.641914	45.874919
3491.515289	280916.408862	45.879924
3490.697204	279831.756805	45.884929
3489.819074	278702.161298	45.889933
3488.907258	277524.688599	45.894938
3487.886104	276297.821088	45.899943
3486.820343	275021.343104	45.904948
3485.368820	273712.161787	45.909953
3484.713688	272349.747099	45.914957
3483.490329	270943.196879	45.919962
3481.753949	269508.746394	45.924967
3480.665962	268005.293909	45.929972
3479.635854	266474.307823	45.934977
3478.183759	264896.662788	45.939981
3476.396974	263280.288852	45.944986
3475.268721	261615.633423	45.949991
3473.888596	259921.249169	45.954996
3471.860678	258185.687387	45.960001
3470.736637	256397.474470	45.965005
3468.743171	254573.923837	45.970010
3467.419409	252711.127692	45.975015
3465.932744	250809.216264	45.980020
3463.969829	248881.099755	45.985025
3462.381564	246912.715201	45.990029
3460.241971	244896.312887	45.995034
3458.244909	242858.602741	46.000039
3456.322204	240777.897909	46.005044
3453.960421	238663.957795	46.010049
3452.439096	236526.236523	46.015053
3449.922296	234351.473659	46.020058
3447.740328	232147.078320	46.025063
3445.662023	229901.322203	46.030068
3443.560805	227638.626805	46.035073
3441.236998	225335.823756	46.040077
3438.902081	223012.570458	46.045082
3436.179255	220649.903576	46.050087
3433.921160	218267.508065	46.055092
3431.247415	215856.687397	46.060097
3428.724578	213424.386165	46.065101
3425.896569	210967.954472	46.070106
3423.366033	208484.093285	46.075111
3420.886471	205987.438779	46.080116
3417.918115	203460.354114	46.085121
3415.014873	200903.572737	46.090125
3412.035076	198323.743536	46.095130
3409.333625	195739.865189	46.100135
3406.272293	193110.456123	46.105140
3402.608577	190492.909330	46.110145
3399.818125	187851.856369	46.115149
3396.545919	185202.233490	46.120154
3393.075507	182526.813749	46.125159
3390.154191	179851.255326	46.130164
3386.366622	177163.002328	46.135169
3383.221005	174455.561456	46.140173
3379.447480	171749.251552	46.145178
3375.868888	169026.789156	46.150183
3372.260274	166306.991652	46.155188
3368.581756	163571.897062	46.160193
3364.586202	160824.529273	46.165197
3360.583251	158097.441765	46.170202
3356.311294	155367.654675	46.175207
3352.589243	152630.705645	46.180212
3348.227187	149903.661097	46.185217
3344.082852	147172.456491	46.190221
3339.073932	144455.475330	46.195226
3334.548710	141751.173519	46.200231
3329.708970	139058.559033	46.205236
3324.123962	136386.009738	46.210241
3318.534644	133698.948429	46.215245
3312.762958	131096.161590	46.220250
3306.306730	128544.009099	46.225255
3300.355575	126017.599241	46.230260
3293.230935	123556.010547	46.235265
3286.312935	121140.527631	46.240269
3279.339260	118785.518558	46.245274
3271.864373	116488.133216	46.250279
3264.547087	114264.282552	46.255284
3256.612168	112102.532406	46.260289
3249.005667	110022.394728	46.265293
3240.545830	108044.256251	46.270298
3231.907334	106129.502765	46.275303
3223.239454	104309.207904	46.280308
3213.555767	102606.697383	46.285313
3204.363318	100989.815381	46.290317
3195.443973	99480.585383	46.295322
3186.499026	98064.360661	46.300327
3177.976925	96756.932908	46.305332
3169.221618	95540.091811	46.310337
3160.945973	94412.432375	46.315341
3152.724151	93375.676573	46.320346
3145.567265	92426.175708	46.325351
3138.063383	91556.734664	46.330356
3131.185244	90748.020698	46.335361
3125.033258	90006.506190	46.340365
3118.770768	89329.509133	46.345370
3112.871678	88713.025121	46.350375
3107.540525	88130.477114	46.355380
3102.444060	87603.424942	46.360385
3097.892576	87110.765205	46.365389
3093.005310	86658.998970	46.370394
3088.485453	86228.983112	46.375399
3084.080760	85817.173525	46.380404
3079.889350	85446.015005	46.385409
3076.370285	85082.607142	46.390413
3072.475453	84722.413146	46.395418
3068.865279	84386.392303	46.400423
3065.351803	84058.363473	46.405428
3061.654318	83744.747388	46.410433
3058.341691	83435.203103	46.415437
3054.886985	83131.134019	46.420442
3051.743862	82822.573406	46.425447
3048.528917	82501.807240	46.430452
3044.863965	82214.332613	46.435457
3041.830389	81907.390747	46.440461
3038.083047	81610.700367	46.445466
3034.740051	81313.873660	46.450471
3031.622334	81013.483646	46.455476
3028.470525	80723.009755	46.460481
3025.243834	80414.272551	46.465485
3021.727385	80118.946310	46.470490
3018.438257	79821.187034	46.475495
3015.404752	79524.470587	46.480500
3012.199546	79211.501024	46.485505
3008.492243	78908.977691	46.490509
3005.253470	78609.356440	46.495514
3001.457049	78298.051881	46.500519
2998.094613	77996.005343	46.505524
2994.472125	77696.809630	46.510529
2991.433477	77398.897525	46.515533
2987.763884	77093.987818	46.520538
2983.927176	76794.225837	46.525543
2980.368883	76502.132565	46.530548
2976.375317	76211.545592	46.535553
2973.077469	75910.032672	46.540557
2969.362635	75627.460045	46.545562
2965.767897	75332.121232	46.550567
2962.616105	75045.377375	46.555572
2958.862276	74773.245999	46.560577
2955.693448	74485.951987	46.565581
2951.624544	74205.049725	46.570586
2948.099833	73915.696734	46.575591
2944.558000	73631.975093	46.580596
2940.947943	73363.784846	46.585601
2937.791224	73085.913639	46.590605
2934.016098	72817.221373	46.595610
2929.881433	72537.210438	46.600615
2926.595876	72266.593240	46.605620
2922.735199	72007.458833	46.610625
2919.170824	71737.474760	46.615629
2915.827650	71486.657808	46.620634
2911.510509	71224.935958	46.625639
2908.165700	70962.836094	46.630644
2903.947253	70725.178211	46.635649
2900.327752	70472.065155	46.640653
2896.351542	70230.805958	46.645658
2893.144166	69992.933121	46.650663
2890.073185	69758.335966	46.655668
2886.719613	69520.547442	46.660673
2882.983406	69288.166230	46.665677
2879.080330	69057.120943	46.670682
2875.798014	68820.806837	46.675687
2872.124418	68588.942661	46.680692
2868.943688	68354.235713	46.685697
2865.035196	68122.361683	46.690701
2861.625185	67899.026001	46.695706
2857.813278	67662.265759	46.700711
2854.444741	67445.002509	46.705716
2850.654108	67224.271379	46.710721
2847.586931	66986.804207	46.715725
2843.696568	66771.691310	46.720730
2840.158438	66552.018304	46.725735
2837.090655	66323.907491	46.730740
2833.298060	66110.340052	46.735745
2830.042839	65884.814206	46.740749
2826.331206	65656.657741	46.745754
2822.875150	65433.560302	46.750759
2819.354004	65210.214770	46.755764
2815.956438	65000.035158	46.760769
2812.724181	64766.543518	46.765773
2808.735646	64553.267414	46.770778
2805.463746	64327.059892	46.775783
2802.209024	64107.497073	46.780788
2798.236261	63880.482871	46.785793
2795.014768	63655.600038	46.790797
2791.562254	63439.507698	46.795802
2788.225072	63225.195339	46.800807
2784.481393	63004.322376	46.805812
2780.775280	62783.280482	46.810817
2777.435543	62561.370877	46.815821
2774.011170	62333.085471	46.820826
2770.561148	62115.316042	46.825831
2766.988035	61892.395396	46.830836
2763.315521	61671.770673	46.835841
2760.087983	61452.233362	46.840845
2756.691604	61227.691787	46.845850
2753.251012	61005.558056	46.850855
2749.604877	60788.338706	46.855860
2745.842782	60570.885567	46.860865
2742.560131	60333.362859	46.865869
2738.841798	60126.073245	46.870874
2735.525504	59896.905058	46.875879
2732.088714	59676.565989	46.880884
2728.675204	59459.366466	46.885889
2725.169407	59232.867683	46.890893
2721.714228	59011.376223	46.895898
2718.596803	58791.242695	46.900903
2714.737797	58563.447420	46.905908
2711.288771	58334.346431	46.910913
2707.503855	58115.211823	46.915917
2704.014444	57897.536853	46.920922
2700.500692	57675.603552	46.925927
2697.216445	57446.193324	46.930932
2693.834735	57235.252574	46.935937
2690.420257	56996.025490	46.940941
2686.907297	56771.232372	46.945946
2683.029765	56551.225479	46.950951
2680.250817	56320.630231	46.955956
2676.257326	56097.105124	46.960961
2672.967336	55861.689573	46.965965
2669.569656	55640.867308	46.970970
2665.833625	55415.925141	46.975975
2662.036919	55184.630828	46.980980
2658.362842	54959.537362	46.985985
2655.227965	54725.783783	46.990989
2651.955509	54517.711384	46.995994
2648.321160	54288.303789	47.000999
2644.743827	54057.163818	47.006004
2640.989438	53832.442586	47.011009
2637.737224	53611.292927	47.016013
2634.166922	53388.196661	47.021018
2631.001157	53159.570547	47.026023
2627.604428	52926.053401	47.031028
2623.798274	52702.886349	47.036033
2620.281318	52472.697787	47.041037
2616.844526	52239.669555	47.046042
2613.293993	52016.012317	47.051047
2610.153022	51787.129294	47.056052
2606.362897	51560.367375	47.061057
2602.798113	51324.710284	47.066061
2599.580379	51098.402555	47.071066
2595.558738	50866.475512	47.076071
2592.474644	50642.612634	47.081076
2588.645672	50425.516367	47.086081
2585.267032	50175.473957	47.091085
2581.432647	49948.607885	47.096090
2577.941933	49726.492133	47.101095
2574.618791	49498.808365	47.106100
2570.826114	49287.146928	47.111105
2567.408454	49048.800577	47.116109
2564.203637	48828.190162	47.121114
2560.774736	48604.724543	47.126119
2557.173149	48370.372026	47.131124
2553.575353	48145.078862	47.136129
2550.193988	47909.466127	47.141133
2546.870691	47692.551333	47.146138
2543.079877	47463.407042	47.151143
2539.591875	47231.084472	47.156148
2535.947657	47003.647072	47.161153
2532.536002	46775.313007	47.166157
2529.076707	46553.724298	47.171162
2525.844226	46321.853113	47.176167
2522.366246	46083.109670	47.181172
2518.584387	45861.292823	47.186177
2515.174762	45630.344370	47.191181
2511.916395	45403.756986	47.196186
2508.083170	45170.349051	47.201191
2504.725970	44936.571015	47.206196
2501.163668	44709.036177	47.211201
2497.799346	44478.434970	47.216205
2494.560286	44244.201769	47.221210
2490.601884	44009.804522	47.226215
2487.397939	43783.770430	47.231220
2483.426861	43565.443105	47.236225
2480.382592	43315.703200	47.241229
2476.823046	43086.110864	47.246234
2473.148452	42856.488176	47.251239
2469.917332	42627.140927	47.256244
2465.908620	42400.479543	47.261249
2462.744471	42166.871657	47.266253
2459.052507	41941.218074	47.271258
2455.358312	41708.864720	47.276263
2451.992927	41481.027857	47.281268
2448.581828	41250.905117	47.286273
2445.132474	41020.086948	47.291277
2441.538498	40787.607202	47.296282
2438.176995	40557.674212	47.301287
2434.634161	40326.529252	47.306292
2430.964071	40102.444640	47.311297
2427.619514	39869.371352	47.316301
2424.150064	39622.123954	47.321306
2420.421352	39398.391808	47.326311
2417.265243	39170.964785	47.331316
2413.848115	38943.638043	47.336321
2410.408030	38705.881431	47.341325
2407.077651	38475.528138	47.346330
2403.452423	38233.931907	47.351335
2399.893996	37988.276728	47.356340
2396.281341	37763.478249	47.361345
2392.835504	37523.922372	47.366349
2389.609523	37282.502598	47.371354
2385.999923	37040.670080	47.376359
2382.400798	36809.279920	47.381364
2378.893357	36576.159916	47.386369
2375.363029	36326.405038	47.391373
2372.087443	36094.433154	47.396378
2368.279242	35863.104975	47.401383
2364.815851	35619.661839	47.406388
2361.223251	35389.864527	47.411393
2357.731007	35154.000183	47.416397
2354.569262	34920.692091	47.421402
2350.654890	34678.325532	47.426407
2347.694052	34436.782424	47.431412
2343.956788	34192.137099	47.436417
2340.327849	33954.133317	47.441421
2337.189480	33705.875613	47.446426
2333.418571	33467.259343	47.451431
2330.146465	33220.131206	47.456436
2326.220229	32982.463828	47.461441
2322.749278	32737.343739	47.466445
2319.595133	32503.820375	47.471450
2315.955473	32262.085198	47.476455
2312.537864	32022.631501	47.481460
2309.238884	31782.179593	47.486465
2305.453434	31544.164301	47.491469
2302.064897	31292.932123	47.496474
2298.504967	31053.841408	47.501479
2294.999167	30800.370927	47.506484
2291.722776	30556.982605	47.511489
2288.256012	30313.354410	47.516493
2284.900899	30059.222993	47.521498
2280.989953	29810.086858	47.526503
2277.816311	29568.253125	47.531508
2274.042753	29323.252373	47.536513
2270.478940	29075.553750	47.541517
2267.147024	28824.228666	47.546522
2263.694802	28581.005262	47.551527
2260.211476	28335.007666	47.556532
2256.479729	28085.161019	47.561537
2253.212282	27831.214550	47.566541
2249.748985	27594.994158	47.571546
2246.320574	27346.839035	47.576551
2242.978331	27096.138806	47.581556
2239.295341	26849.220869	47.586561
2235.672814	26588.261203	47.591565
2232.100081	26338.930708	47.596570
2228.676463	26095.675483	47.601575
2225.386798	25841.510243	47.606580
2221.750349	25593.706928	47.611585
2218.134158	25327.649262	47.616589
2214.760964	25085.120641	47.621594
2211.247807	24843.206081	47.626599
2208.166750	24578.943686	47.631604
2204.256166	24336.824967	47.636609
2200.911864	24070.386606	47.641613
2197.243790	23819.904785	47.646618
2193.580988	23574.633075	47.651623
2190.587239	23314.175022	47.656628
2186.793333	23053.262708	47.661633
2183.587393	22799.179937	47.666637
2180.274906	22545.288131	47.671642
2176.757783	22289.087597	47.676647
2173.395048	22026.163758	47.681652
2169.746091	21767.519931	47.686657
2166.564819	21503.256975	47.691661
2162.847353	21238.295933	47.696666
2159.376174	20975.840125	47.701671
2156.128901	20700.765922	47.706676
2152.292304	20445.861852	47.711681
2148.532355	20185.286110	47.716685
2145.200730	19919.649009	47.721690
2141.477978	19654.342742	47.726695
2138.207689	19384.681039	47.731700
2134.579905	19133.118487	47.736705
2131.173011	18870.155062	47.741709
2127.634928	18607.291716	47.746714
2123.583570	18341.921687	47.751719
2120.820548	18078.804864	47.756724
2116.739685	17835.424508	47.761729
2113.090120	17580.496921	47.766733
2108.636884	17334.090336	47.771738
2103.522168	17127.197041	47.776743
2099.197318	16924.957748	47.781748
2094.491065	16735.070050	47.786753
2090.558731	16543.900984	47.791757
2086.833323	16370.488214	47.796762
2082.707708	16200.198536	47.801767
2079.398833	16026.106222	47.806772
2075.574395	15857.773715	47.811777
2072.010520	15695.275750	47.816781
2068.641577	15531.535910	47.821786
2064.812416	15366.979714	47.826791
2061.731702	15198.470144	47.831796
2058.437205	15059.170530	47.836801
2054.979590	14900.231212	47.841805
2051.939720	14735.306820	47.846810
2048.399761	14575.661170	47.851815
2045.351310	14399.481661	47.856820
2041.595272	14243.023054	47.861825
2038.244853	14070.984627	47.866829
2034.815132	13905.928950	47.871834
2031.319574	13736.974800	47.876839
2027.959470	13565.135608	47.881844
2024.490383	13402.864004	47.886849
2021.530638	13234.660011	47.891853
2017.934710	13067.497376	47.896858
2014.305450	12891.267614	47.901863
2011.085240	12726.293917	47.906868
2007.689629	12556.353213	47.911873
2004.233180	12383.798998	47.916877
2000.687344	12212.855967	47.921882
1997.009449	12036.986884	47.926887
1993.718982	11850.972429	47.931892
1989.999065	11686.152517	47.936897
1986.551962	11508.511064	47.941901
1983.344639	11333.812754	47.946906
1979.745492	11160.136598	47.951911
1976.328035	10985.528232	47.956916
1972.668069	10814.121949	47.961921
1969.347737	10631.422893	47.966925
1966.115099	10455.030462	47.971930
1962.328277	10283.750195	47.976935
1959.300571	10094.676267	47.981940
1955.293765	9913.364209	47.986945
1951.834836	9744.956197	47.991949
1948.764605	9562.814086	47.996954
1945.042290	9391.000141	48.001959
1941.724729	9200.201679	48.006964
1938.248139	9022.946186	48.011969
1934.841928	8832.013442	48.016973
1930.829202	8650.508894	48.021978
1927.423995	8479.049442	48.026983
1924.207326	8297.623201	48.031988
1920.809359	8124.038862	48.036993
1917.501684	7934.628758	48.041997
1913.753107	7750.198742	48.047002
1910.243844	7571.664562	48.052007
1907.092382	7373.018946	48.057012
1903.354559	7193.030281	48.062017
1899.673040	7008.445281	48.067021
1896.204136	6819.866292	48.072026
1892.445553	6641.940358	48.077031
1889.367313	6466.799270	48.082036
1885.620277	6274.699366	48.087041
1881.651535	6096.416006	48.092045
1878.576591	5903.749587	48.097050
1875.237266	5724.880805	48.102055
1871.912858	5537.514024	48.107060
1868.055219	5370.610384	48.112065
1864.697272	5178.654166	48.117069
1861.233117	4991.311703	48.122074
1857.683862	4800.161593	48.127079
1854.733282	4611.590738	48.132084
1850.997269	4436.417001	48.137089
1847.107495	4249.256386	48.142093
1843.421482	4051.458361	48.147098
1839.811308	3876.662741	48.152103
1836.580192	3691.854122	48.157108
1833.126935	3509.670648	48.162113
1829.609606	3322.356907	48.167117
1826.562458	3133.297585	48.172122
1822.746027	2942.009538	48.177127
1819.495090	2764.045283	48.182132
1815.702328	2585.882793	48.187137
1811.881369	2397.132651	48.192141
1808.643201	2205.243007	48.197146
1804.828077	2020.248642	48.202151
1801.558906	1831.699699	48.207156
1797.403755	1657.140631	48.212161
1793.934385	1473.455197	48.217165
1790.419208	1303.131033	48.222170
1786.550502	1136.360041	48.227175
1783.581291	961.606348	48.232180
1779.457980	784.725299	48.237185
1775.882216	620.906370	48.242189
1772.195835	456.334270	48.247194
1768.456487	300.849083	48.252199
1764.295896	144.592765	48.257204
1759.793501	4.080611	48.262209
1750.417289	24.167136	48.267213
1742.856981	40.179255	48.272218
1737.315053	37.246996	48.277223
1734.017919	44.467273	48.282228
1731.274851	49.680409	48.287233
1729.076316	54.159744	48.292237
1726.746669	38.673809	48.297242
1723.355364	51.894758	48.302247
1720.504652	38.926507	48.307252
1716.904174	41.733292	48.312257
1713.197205	55.506693	48.317261
1710.821605	43.979552	48.322266
1706.993506	44.850911	48.327271
1703.626285	40.837989	48.332276
1700.034053	46.342219	48.337281
1696.250380	41.856628	48.342285
1693.380235	47.716094	48.347290
1689.796851	47.558888	48.352295
1686.656946	49.091354	48.357300
1682.698461	51.077806	48.362305
1679.310508	53.819706	48.367309
1676.495508	37.704221	48.372314
1672.375275	47.650822	48.377319
1669.151323	47.725276	48.382324
1665.822378	50.593988	48.387329
1662.034929	51.430527	48.392333
1659.084014	37.149185	48.397338
1655.423920	43.587880	48.402343
1652.011792	44.065120	48.407348
1648.277628	48.307074	48.412353
1644.919078	43.546156	48.417357
1641.450323	38.625317	48.422362
1637.744090	42.764823	48.427367
1634.575358	41.634727	48.432372
1631.084341	47.398388	48.437377
1627.371084	40.424543	48.442381
1624.310167	35.550613	48.447386
1620.814937	43.592875	48.452391
1617.558554	48.244123	48.457396
1613.720964	49.433382	48.462401
1610.447465	47.433824	48.467405
1606.811291	41.042720	48.472410
1602.940891	42.920500	48.477415
1600.105931	46.284565	48.482420
1596.528231	47.895070	48.487425
1592.564621	52.283688	48.492429
1588.930060	37.663278	48.497434
1585.896760	56.978664	48.502439
1582.380226	37.533960	48.507444
1579.086109	49.635559	48.512449
1575.738648	50.438066	48.517453
1572.308225	46.843213	48.522458
1568.601878	52.792459	48.527463
1565.157969	43.530180	48.532468
1561.664687	45.757081	48.537473
1558.032273	41.760409	48.542477
1554.803700	49.403445	48.547482
1550.812924	56.074270	48.552487
1547.427766	44.078765	48.557492
1543.462919	51.938287	48.562497
1540.791301	46.813621	48.567501
1537.330682	47.671818	48.572506
1533.500226	50.511497	48.577511
1529.808848	47.789586	48.582516
1526.738566	48.501267	48.587521
1523.644583	49.567842	48.592525
1519.989048	43.404433	48.597530
1515.737183	56.383634	48.602535
1512.674124	46.954193	48.607540
1508.758342	44.055440	48.612545
1505.711731	44.314163	48.617549
1502.540277	50.034171	48.622554
1498.742531	48.834892	48.627559
1495.267529	40.504505	48.632564
1492.011237	53.637932	48.637569
1488.217285	50.856160	48.642573
1484.551949	41.324850	48.647578
1480.853000	44.672318	48.652583
1478.043403	44.289664	48.657588
1474.531992	48.939741	48.662593
1470.393847	43.857983	48.667597
1467.352552	50.601682	48.672602
1463.278964	50.714278	48.677607
1460.184433	46.978305	48.682612
1457.159841	42.665065	48.687617
1453.281754	48.603262	48.692621
1449.681290	47.167475	48.697626
1446.526709	51.540241	48.702631
1442.536220	49.675117	48.707636
1439.139760	48.245366	48.712641
1435.816062	47.512919	48.717645
1432.769156	44.876831	48.722650
1428.636739	44.698089	48.727655
1425.299356	40.981160	48.732660
1422.021660	48.103564	48.737665
1418.336920	44.706768	48.742669
1415.101985	32.225899	48.747674
1411.062390	42.903452	48.752679
1407.768462	43.175607	48.757684
1404.064484	39.427484	48.762689
1400.692027	46.574217	48.767693
1397.573210	43.572905	48.772698
1393.857826	47.011562	48.777703
1390.385516	41.563021	48.782708
1386.615702	44.779242	48.787713
1382.900573	46.370204	48.792717
1379.922472	45.969661	48.797722
1376.127461	51.559519	48.802727
1372.987562	44.790264	48.807732
1369.209089	32.682405	48.812737
1365.695805	46.485678	48.817741
1362.470303	43.143569	48.822746
1358.711123	52.897712	48.827751
1355.608245	43.914336	48.832756
1352.038829	41.243007	48.837761
1348.689515	50.891863	48.842765
1344.902426	37.459728	48.847770
1341.142184	48.248602	48.852775
1338.160818	36.566478	48.857780
1334.481449	38.803600	48.862785
1330.506588	38.078209	48.867789
1327.487366	35.017039	48.872794
1323.724384	45.869622	48.877799
1320.344698	41.570886	48.882804
1316.740836	44.637766	48.887809
1313.033906	52.643654	48.892813
1309.768640	48.823726	48.897818
1306.386116	42.883429	48.902823
1302.921059	48.760184	48.907828
1298.968761	48.616576	48.912833
1295.429603	52.182707	48.917837
1292.705135	42.080246	48.922842
1288.980759	43.938448	48.927847
1285.717807	47.913765	48.932852
1282.199270	40.064854	48.937857
1278.194426	58.124484	48.942861
1274.929717	40.469192	48.947866
1271.230377	51.640865	48.952871
1267.829879	45.766671	48.957876
1264.510348	44.359742	48.962881
1260.779547	55.767302	48.967885
1257.499229	47.425518	48.972890
1253.776206	50.441471	48.977895
1250.257190	51.119080	48.982900
1246.853640	45.564916	48.987905
1243.033968	38.418070	48.992909
1239.609133	47.601042	48.997914
1236.266142	42.632197	49.002919
1232.631155	47.402937	49.007924
1229.467897	49.397947	49.012929
1225.908096	53.451393	49.017933
1222.727781	38.810671	49.022938
1218.951442	48.668781	49.027943
1215.386499	49.119472	49.032948
1211.869606	43.842498	49.037953
1207.999300	39.949649	49.042957
1204.652233	35.525629	49.047962
1200.603062	42.050686	49.052967
1197.852929	41.747390	49.057972
1194.324424	36.114735	49.062977
1190.962827	49.970236	49.067981
1187.400706	44.883852	49.072986
1183.962296	46.368288	49.077991
1180.663971	42.382740	49.082996
1176.606628	46.336922	49.088001
1173.289214	43.638865	49.093005
1169.756772	37.658819	49.098010
1166.201512	47.216574	49.103015
1162.786678	41.543988	49.108020
1159.123705	46.603875	49.113025
1155.468925	42.746909	49.118029
1152.585589	35.077023	49.123034
1149.065086	47.805790	49.128039
1145.508077	42.152305	49.133044
1142.056782	40.161764	49.138049
1137.825318	45.108178	49.143053
1134.324841	45.052089	49.148058
1131.094875	49.250082	49.153063
1127.482220	35.088388	49.158068
1124.283910	42.660355	49.163073
1120.578185	44.392311	49.168077
1117.558974	40.132131	49.173082
1113.667405	42.617694	49.178087
1110.269887	42.906167	49.183092
1106.979184	34.683137	49.188097
1103.071388	43.698146	49.193101
1099.975176	42.044338	49.198106
1096.073573	46.277892	49.203111
1092.563824	42.888633	49.208116
1089.102202	43.054271	49.213121
1085.799426	41.964325	49.218125
1082.253562	45.996653	49.223130
1078.854904	48.746746	49.228135
1075.062115	41.991241	49.233140
1071.886757	39.384877	49.238145
1067.882449	50.313286	49.243149
1064.906328	51.181212	49.248154
1061.158271	42.210382	49.253159
1057.693039	46.343990	49.258164
1054.083077	38.885984	49.263169
1050.795018	45.738024	49.268173
1047.665545	42.725847	49.273178
1043.193711	43.046506	49.278183
1040.029190	45.646056	49.283188
1036.681355	40.481893	49.288193
1033.295881	43.403945	49.293197
1030.242582	40.870235	49.298202
1026.404513	42.357188	49.303207
1022.748088	38.769458	49.308212
1019.235456	46.688065	49.313217
1015.284150	47.287909	49.318221
1012.361111	36.273837	49.323226
1008.553827	47.608018	49.328231
1005.063393	34.914230	49.333236
1001.421540	39.613353	49.338241
998.196499	40.317791	49.343245
994.904450	37.970174	49.348250
991.594918	40.070419	49.353255
987.754995	39.387318	49.358260
983.948019	42.400693	49.363265
980.321185	42.832687	49.368269
976.679622	33.604779	49.373274
973.662315	41.009239	49.378279
970.416462	41.087351	49.383284
967.075575	35.529819	49.388289
962.982087	41.321575	49.393293
959.535024	32.724454	49.398298
955.617182	38.147021	49.403303
952.565155	41.007397	49.408308
949.835897	40.558533	49.413313
946.050242	45.039746	49.418317
942.141651	45.848069	49.423322
938.325322	34.774581	49.428327
934.708611	35.995953	49.433332
931.355769	40.861821	49.438337
927.843269	37.007983	49.443341
924.877562	37.523140	49.448346
920.748976	38.457669	49.453351
917.849606	37.589358	49.458356
914.587741	44.741059	49.463361
910.760021	37.222301	49.468365
907.296225	30.235027	49.473370
903.378764	40.789213	49.478375
899.894280	42.663781	49.483380
896.470093	27.536217	49.488385
893.041424	35.716959	49.493389
889.450219	29.790529	49.498394
885.614833	30.362783	49.503399
882.213560	33.695486	49.508404
879.607745	39.156247	49.513409
875.782283	40.945009	49.518413
872.402619	36.307921	49.523418
868.639493	41.728441	49.528423
865.292509	38.788355	49.533428
861.697346	40.468293	49.538433
857.856586	43.354127	49.543437
854.592465	35.826237	49.548442
850.428182	45.068157	49.553447
847.220903	41.337401	49.558452
844.058727	40.174905	49.563457
840.457468	40.577636	49.568461
837.125040	36.179941	49.573466
833.559242	44.350541	49.578471
829.973487	48.167736	49.583476
826.558422	41.732851	49.588481
822.796023	46.972939	49.593485
819.216323	37.770218	49.598490
815.885066	43.797015	49.603495
812.548993	42.329564	49.608500
809.015221	40.753866	49.613505
805.577238	54.146853	49.618509
802.451968	40.374073	49.623514
798.591906	44.901793	49.628519
795.043698	40.367059	49.633524
791.612163	44.786547	49.638529
787.831004	48.773563	49.643533
784.388749	35.233934	49.648538
780.783608	40.357660	49.653543
777.638369	37.993461	49.658548
774.267185	45.535649	49.663553
770.030551	46.813033	49.668557
766.558160	39.004578	49.673562
763.419921	42.473303	49.678567
760.394930	39.707462	49.683572
757.005225	31.443137	49.688577
752.957788	40.217535	49.693581
749.606264	30.805110	49.698586
745.854382	38.558782	49.703591
742.079336	39.358929	49.708596
738.776289	39.332181	49.713601
735.344778	42.603231	49.718605
731.992781	27.401169	49.723610
728.433072	42.183146	49.728615
724.629188	37.128493	49.733620
721.618432	32.474825	49.738625
717.810013	41.487054	49.743629
714.362057	24.518823	49.748634
710.977834	33.546878	49.753639
707.143548	44.300079	49.758644
703.982236	32.880521	49.763649
700.345548	33.766585	49.768653
697.322001	27.858909	49.773658
693.097415	42.305255	49.778663
689.558450	32.909554	49.783668
686.108368	31.070861	49.788673
682.676370	34.098392	49.793677
679.727220	31.096075	49.798682
676.321838	37.096557	49.803687
672.519676	36.170391	49.808692
669.005255	29.662552	49.813697
665.221250	42.223899	49.818701
661.944677	34.410137	49.823706
658.382251	39.017847	49.828711
654.681230	38.882612	49.833716
651.277746	38.491972	49.838721
647.720880	44.845222	49.843725
644.455417	32.606764	49.848730
640.926171	42.524432	49.853735
637.438205	35.455636	49.858740
634.031255	30.525525	49.863745
630.079319	34.517198	49.868749
626.864309	37.343086	49.873754
623.076018	40.258759	49.878759
619.671016	34.505766	49.883764
616.422162	39.909109	49.888769
612.646176	33.679542	49.893773
609.153549	33.043449	49.898778
605.590613	40.546114	49.903783
602.477306	39.217860	49.908788
599.414660	25.777066	49.913793
595.407717	33.096168	49.918797
591.588053	34.944246	49.923802
587.980675	32.516454	49.928807
584.759748	35.181930	49.933812
581.725003	29.333000	49.938817
577.910899	33.929533	49.943821
574.467371	31.007846	49.948826
570.520388	34.764648	49.953831
566.824633	35.523973	49.958836
563.777083	26.991011	49.963841
560.179724	42.547726	49.968845
556.650511	33.846591	49.973850
553.025986	27.808469	49.978855
549.692610	39.147657	49.983860
546.877424	29.942387	49.988865
542.915961	42.661281	49.993869
539.143258	45.125290	49.998874
535.605390	46.302828	50.003879
532.014987	38.630022	50.008884
528.328870	33.591817	50.013889
525.207814	42.853961	50.018893
521.737703	28.644946	50.023898
517.851358	41.450159	50.028903
514.840113	32.376849	50.033908
511.189844	44.063079	50.038913
507.722548	46.229328	50.043917
504.295808	38.834623	50.048922
500.722650	42.982159	50.053927
496.958321	40.193006	50.058932
493.645816	43.072174	50.063937
490.034304	39.977513	50.068941
486.581621	30.005244	50.073946
483.085922	32.182276	50.078951
479.814324	41.910940	50.083956
476.813615	31.418625	50.088961
472.339194	35.976256	50.093965
468.767567	35.627840	50.098970
465.573056	33.195544	50.103975
462.296147	29.168959	50.108980
458.972282	32.692162	50.113985
455.259765	42.290577	50.118989
451.521084	31.224161	50.123994
447.835653	45.649418	50.128999
444.385579	36.872663	50.134004
441.745096	36.131636	50.139009
438.020803	36.373461	50.144013
434.029172	34.176764	50.149018
430.358084	38.627567	50.154023
427.064673	41.026038	50.159028
423.714292	32.948691	50.164033
420.045387	45.030176	50.169037
416.582296	34.439468	50.174042
413.080533	34.001037	50.179047
409.583144	30.100758	50.184052
406.124486	28.212899	50.189057
402.358817	34.269903	50.194061
399.228625	36.291638	50.199066
395.635781	31.121825	50.204071
391.692602	33.713836	50.209076
388.646522	28.904473	50.214081
384.906818	41.965170	50.219085
381.898811	37.763616	50.224090
378.191440	42.963609	50.229095
374.810704	35.327639	50.234100
370.871505	40.896144	50.239105
367.077056	45.435898	50.244109
364.149669	44.151374	50.249114
360.733532	39.646760	50.254119
357.497500	39.672930	50.259124
354.008794	29.614617	50.264129
349.504385	37.771044	50.269133
346.292551	32.551061	50.274138
343.078471	39.451833	50.279143
339.409035	35.584860	50.284148
336.178235	29.716116	50.289153
332.606049	33.885706	50.294157
329.069073	32.899165	50.299162
325.763548	31.294237	50.304167
321.954101	43.056079	50.309172
318.801620	39.108135	50.314177
314.867340	44.375334	50.319181
311.452122	38.231765	50.324186
307.891656	35.761941	50.329191
304.585300	40.396103	50.334196
301.178540	31.878388	50.339201
297.233797	39.001201	50.344205
293.900288	43.063814	50.349210
290.457609	41.847381	50.354215
287.115176	40.776597	50.359220
283.788266	39.504066	50.364225
279.981107	49.598262	50.369229
276.428573	43.574293	50.374234
272.961525	37.983029	50.379239
268.969570	47.394328	50.384244
265.932104	40.960646	50.389249
262.229750	43.913621	50.394253
258.860122	45.972913	50.399258
255.409979	45.653009	50.404263
252.132419	40.221894	50.409268
248.501629	34.431665	50.414273
245.300013	38.280643	50.419277
241.740331	34.269970	50.424282
237.808308	37.667059	50.429287
234.034897	38.976526	50.434292
231.256219	33.843758	50.439297
227.536072	42.747416	50.444301
224.011813	39.003284	50.449306
220.160705	37.040939	50.454311
216.893489	35.085200	50.459316
213.362650	38.868706	50.464321
209.689982	45.436401	50.469325
206.100083	40.421234	50.474330
202.831184	35.855657	50.479335
199.419447	43.610019	50.484340
196.285409	39.782620	50.489345
192.042478	35.913809	50.494349
188.615995	29.499978	50.499354
185.293522	40.299719	50.504359
181.973178	37.931536	50.509364
178.427034	36.633281	50.514369
174.846124	45.499326	50.519373
171.462769	42.780349	50.524378
168.033210	37.009251	50.529383
164.232099	29.388616	50.534388
160.861698	27.977415	50.539393
157.255782	32.513022	50.544397
154.211481	40.200341	50.549402
150.364046	38.999920	50.554407
146.768470	37.415192	50.559412
143.444204	30.023583	50.564417
139.590500	38.347078	50.569421
136.071449	41.733295	50.574426
133.069773	38.486300	50.579431
129.032968	42.130807	50.584436
126.143074	37.575486	50.589441
122.543459	34.437994	50.594445
118.980337	33.816305	50.599450
115.473857	45.442166	50.604455
111.905524	35.532485	50.609460
108.316919	33.658779	50.614465
104.480473	41.913146	50.619469
100.924309	29.536995	50.624474
97.582561	39.343196	50.629479
94.093259	35.628447	50.634484
91.196957	29.678926	50.639489
87.086173	40.880614	50.644493
84.071519	33.962543	50.649498
80.380864	34.974370	50.654503
76.709591	34.932793	50.659508
73.136398	36.802583	50.664513
69.965654	31.430744	50.669517
66.276915	26.782308	50.674522
63.069501	35.722747	50.679527
59.146352	36.479943	50.684532
55.779060	30.110683	50.689537
51.981281	32.426957	50.694541
48.515005	39.025647	50.699546
45.278225	28.076962	50.704551
41.637725	35.851396	50.709556
38.265320	31.083807	50.714561
34.638606	32.797481	50.719565
31.596933	28.310272	50.724570
27.706808	29.318573	50.729575
23.836144	34.269036	50.734580
20.773053	33.679775	50.739585
17.284076	27.127117	50.744589
13.688185	27.852042	50.749594
10.622090	33.590774	50.754599
6.964090	28.943878	50.759604
3.319928	33.453898	50.764609