Thu Aug 25 09:43:56 2022

Number of Points = 9924

Depth (nm)	Load (N)	Time (s)
1.844675	97.026858	0.000000
1.973049	102.527711	0.005005
2.259938	101.663535	0.010010
2.083681	101.321181	0.015014
1.810591	94.470309	0.020019
1.859548	95.108237	0.025024
2.025576	80.867611	0.030029
1.344335	71.397825	0.035034
1.146921	58.444865	0.040038
1.224686	50.811372	0.045043
0.608341	46.073908	0.050048
0.822156	35.593868	0.055053
0.077987	34.416680	0.060058
-0.187965	25.954364	0.065062
-0.402029	31.502521	0.070067
-0.905550	10.950760	0.075072
-0.774138	6.725733	0.080077
-1.237823	9.914872	0.085082
-1.722051	-4.378827	0.090086
-2.342095	-4.060024	0.095091
-2.141036	-2.120319	0.100096
-1.971590	-9.685894	0.105101
-2.852980	-8.867398	0.110106
-3.021526	-7.031135	0.115110
-3.272149	-5.593299	0.120115
-3.568006	-6.369327	0.125120
-3.725173	-4.332366	0.130125
-4.354621	-9.434756	0.135130
-4.756577	-3.967902	0.140134
-5.031157	-10.606528	0.145139
-5.419742	-9.779826	0.150144
-5.017402	-8.792310	0.155149
-5.488069	-5.994386	0.160154
-5.526731	-4.115198	0.165158
-5.626590	-6.418389	0.170163
-5.901362	-10.310851	0.175168
-6.122361	-6.754780	0.180173
-6.653704	-13.251935	0.185178
-6.432005	-12.055783	0.190182
-6.927254	-12.003305	0.195187
-7.985085	-5.807265	0.200192
-8.008211	-2.174629	0.205197
-8.125646	-13.732197	0.210202
-8.186451	-11.545821	0.215206
-7.912980	-7.915366	0.220211
-8.552476	-9.842940	0.225216
-8.394745	-11.151945	0.230221
-9.290931	-6.642200	0.235226
-9.246222	-14.678609	0.240230
-9.260108	-7.858364	0.245235
-9.977051	-0.551473	0.250240
-10.239050	-12.598918	0.255245
-11.047519	-7.375254	0.260250
-11.335615	-15.710694	0.265254
-11.112477	-8.604885	0.270259
-11.265444	-5.948487	0.275264
-11.446576	-14.965074	0.280269
-11.440726	-3.209309	0.285274
-11.784668	-4.971220	0.290278
-11.334303	-10.815437	0.295283
-12.456094	-2.793381	0.300288
-12.916216	-10.323587	0.305293
-13.446411	-1.916499	0.310298
-12.737813	-2.280434	0.315302
-12.775024	-4.371979	0.320307
-13.699558	-10.703124	0.325312
-14.067070	-16.374898	0.330317
-14.222311	-8.950376	0.335322
-14.357470	-2.215532	0.340326
-14.294069	-6.233746	0.345331
-14.485352	1.838669	0.350336
-14.989462	-7.377253	0.355341
-15.628352	-3.603845	0.360346
-15.730545	-13.458539	0.365350
-15.636166	-11.214220	0.370355
-16.463039	-2.602459	0.375360
-16.674878	-12.408337	0.380365
-16.974899	-4.170191	0.385370
-16.823500	-6.987313	0.390374
-16.988517	-1.459507	0.395379
-17.130802	3.014375	0.400384
-17.041318	-3.187751	0.405389
-18.166139	-6.845783	0.410394
-18.227232	-2.147343	0.415398
-18.353402	-8.878825	0.420403
-18.924670	-2.603995	0.425408
-18.337693	-2.822325	0.430413
-19.300795	3.036175	0.435418
-19.715506	-1.106444	0.440422
-19.549631	-8.209552	0.445427
-19.878891	1.023431	0.450432
-19.586925	-1.050089	0.455437
-20.558491	-0.989418	0.460442
-20.862159	-9.044010	0.465446
-21.106833	-9.375641	0.470451
-21.438576	4.185741	0.475456
-20.938637	-9.895158	0.480461
-21.602648	4.044151	0.485466
-21.152806	-7.235308	0.490470
-22.338679	-1.364051	0.495475
-22.814924	4.522570	0.500480
-22.881558	3.789719	0.505485
-23.008024	-1.701528	0.510490
-23.030739	-2.748143	0.515494
-23.094888	-8.451633	0.520499
-23.901953	-2.494197	0.525504
-24.048816	-2.800025	0.530509
-24.391223	-11.449658	0.535514
-24.259995	-6.328938	0.540518
-24.236132	-6.572931	0.545523
-25.229114	-5.464866	0.550528
-25.201128	-0.226727	0.555533
-25.692801	-8.302481	0.560538
-25.656387	-9.408981	0.565542
-25.840564	-7.804385	0.570547
-25.751393	-0.301098	0.575552
-26.365062	-7.857864	0.580557
-26.581510	2.515375	0.585562
-27.242420	-10.516767	0.590566
-27.040263	-11.684037	0.595571
-27.552920	-9.961536	0.600576
-27.434247	-8.907429	0.605581
-27.662007	-13.019225	0.610586
-28.202688	-12.304732	0.615590
-28.579399	-7.889035	0.620595
-28.713206	-6.627689	0.625600
-28.659098	-10.945002	0.630605
-29.361377	-9.869831	0.635610
-29.909803	-5.667672	0.640614
-29.998746	-6.397027	0.645619
-30.409784	-1.321053	0.650624
-30.456949	-8.166153	0.655629
-30.253208	-5.644741	0.660634
-30.220994	-9.721342	0.665638
-30.427584	-9.831151	0.670643
-31.112869	-1.545294	0.675648
-31.734815	-8.816025	0.680653
-31.510977	-4.662103	0.685658
-31.347157	-9.819182	0.690662
-31.732976	-1.333475	0.695667
-32.514699	-13.384904	0.700672
-32.748774	-14.290834	0.705677
-32.856872	-15.963147	0.710682
-33.414835	-6.824048	0.715686
-33.154768	-14.425965	0.720691
-34.046363	-9.214585	0.725696
-34.261664	-14.631798	0.730701
-34.413905	-12.532335	0.735706
-35.063056	-12.990414	0.740710
-34.409256	-15.247177	0.745715
-34.731895	-13.200109	0.750720
-34.954058	-7.467198	0.755725
-35.970012	-8.997263	0.760730
-36.253982	-1.698101	0.765734
-36.310967	-6.276418	0.770739
-36.501863	-5.800228	0.775744
-36.251359	-9.297266	0.780749
-36.405443	-13.161178	0.785754
-36.011834	-12.858830	0.790758
-36.587244	-8.921363	0.795763
-37.607852	-6.916791	0.800768
-37.542091	-10.736057	0.805773
-37.788728	-9.245062	0.810778
-38.405661	-0.757943	0.815782
-38.500132	-5.437954	0.820787
-39.079693	-7.770386	0.825792
-38.768418	-8.619396	0.830797
-38.998625	-6.308400	0.835802
-39.081845	-10.537757	0.840806
-39.859479	-2.607589	0.845811
-40.423245	-4.559682	0.850816
-40.251870	-7.253384	0.855821
-40.802716	-1.152596	0.860826
-41.086740	-14.753149	0.865830
-40.605612	-13.619794	0.870835
-40.734440	-2.779398	0.875840
-41.356449	-8.145541	0.880845
-41.912631	-5.093771	0.885850
-42.163098	-7.085462	0.890854
-41.996914	-12.698489	0.895859
-42.195791	-13.195483	0.900864
-42.543679	-18.753270	0.905869
-43.141596	-15.878460	0.910874
-43.686998	-21.079432	0.915878
-43.721722	-14.189488	0.920883
-43.753382	-8.495918	0.925888
-43.746785	-11.106854	0.930893
-43.620600	-6.007490	0.935898
-44.534633	-3.013544	0.940902
-44.638714	-10.988674	0.945907
-45.090381	-1.597309	0.950912
-45.164390	-7.511224	0.955917
-45.230267	-5.453766	0.960922
-46.232129	-7.818103	0.965926
-46.505400	-6.231186	0.970931
-46.491379	-7.172825	0.975936
-46.793850	-9.602456	0.980941
-46.850387	2.090319	0.985946
-47.056847	6.045909	0.990950
-46.785621	-5.461827	0.995955
-47.006383	-1.858337	1.000960
-47.515976	1.135514	1.005965
-48.166592	4.553259	1.010970
-48.291092	-2.475877	1.015974
-48.255137	-3.101415	1.020979
-48.515113	-2.573272	1.025984
-48.968352	-2.245801	1.030989
-49.612466	-2.600265	1.035994
-49.466256	-7.529958	1.040998
-49.803651	3.058383	1.046003
-50.255046	-1.366386	1.051008
-49.858150	-4.693374	1.056013
-50.467730	5.466218	1.061018
-51.059454	5.011796	1.066022
-50.749610	-0.952774	1.071027
-51.782544	10.839212	1.076032
-51.119305	-4.187929	1.081037
-51.125106	6.845166	1.086042
-51.993541	9.012558	1.091046
-52.286195	-3.381261	1.096051
-52.578065	9.683494	1.101056
-52.744574	-2.546593	1.106061
-52.822080	5.400426	1.111066
-53.442349	9.072844	1.116070
-53.576533	-2.817459	1.121075
-54.136602	4.430053	1.126080
-53.786549	-1.743297	1.131085
-53.868205	-0.078835	1.136090
-54.235520	6.448779	1.141094
-54.671759	0.901666	1.146099
-55.396819	5.261218	1.151104
-55.648274	-5.228149	1.156109
-55.260480	2.120779	1.161114
-55.754724	2.559080	1.166118
-55.566505	-2.105114	1.171123
-56.306995	6.094483	1.176128
-56.418253	-2.955200	1.181133
-56.657493	-1.838684	1.186138
-57.086334	6.783480	1.191142
-56.538384	-4.194977	1.196147
-57.278273	4.099439	1.201152
-58.168745	-4.938880	1.206157
-59.147567	-8.638764	1.211162
-58.994734	4.701155	1.216166
-58.300296	-7.356946	1.221171
-58.732951	-3.324786	1.226176
-58.715172	-1.489243	1.231181
-58.657172	-5.671125	1.236186
-59.402028	1.848949	1.241190
-59.674407	1.904474	1.246195
-59.812576	-0.291475	1.251200
-60.042583	-7.981118	1.256205
-61.093462	-2.023443	1.261210
-61.366386	-9.022992	1.266214
-60.983635	-4.264386	1.271219
-61.204329	0.307201	1.276224
-61.180875	-10.494156	1.281229
-61.665353	-6.181795	1.286234
-61.758160	-5.800068	1.291238
-62.324353	-7.489187	1.296243
-63.000052	3.297695	1.301248
-63.038133	-7.329508	1.306253
-63.202212	-10.030758	1.311258
-62.931447	-2.217407	1.316262
-63.265888	-4.138992	1.321267
-63.390618	2.610037	1.326272
-63.690702	-2.180125	1.331277
-64.377324	-8.143581	1.336282
-64.614961	-3.563012	1.341286
-64.527954	-6.139091	1.346291
-65.386868	2.629553	1.351296
-65.655848	1.909427	1.356301
-66.297343	4.579098	1.361306
-66.012652	0.187689	1.366310
-65.893027	-12.077734	1.371315
-66.658875	-2.409351	1.376320
-66.109220	-5.054759	1.381325
-66.382631	-2.917326	1.386330
-66.451894	-5.010175	1.391334
-67.000487	-2.408845	1.396339
-67.489577	6.010788	1.401344
-67.647365	-8.406811	1.406349
-67.992453	-8.105776	1.411354
-68.535096	-3.455270	1.416358
-68.612435	-7.410302	1.421363
-68.776470	-4.400994	1.426368
-68.865761	-1.609041	1.431373
-68.957149	-5.131602	1.436378
-69.409794	-6.537956	1.441382
-69.857696	-9.707261	1.446387
-69.952019	2.934229	1.451392
-70.309823	-3.280066	1.456397
-70.173884	-7.214733	1.461402
-70.841819	-14.259951	1.466406
-71.493828	-6.827195	1.471411
-71.599866	-1.207391	1.476416
-71.485794	1.486259	1.481421
-71.806315	2.637657	1.486426
-72.259904	0.987841	1.491430
-71.687317	-3.803018	1.496435
-72.629937	-1.703095	1.501440
-72.588770	0.321772	1.506445
-73.097245	3.790011	1.511450
-73.310067	7.658014	1.516454
-72.955262	-14.736617	1.521459
-73.921347	-3.869437	1.526464
-74.439428	-9.062036	1.531469
-74.673854	-8.306942	1.536474
-74.699822	-3.693102	1.541478
-74.968384	-3.293326	1.546483
-75.213113	3.056890	1.551488
-74.931825	-7.421037	1.556493
-75.338013	-7.350873	1.561498
-75.631294	0.240812	1.566502
-75.837979	-7.300625	1.571507
-76.490057	0.302987	1.576512
-76.563776	-2.523154	1.581517
-76.541222	-2.305035	1.586522
-77.761566	-2.945692	1.591526
-77.951786	-8.885688	1.596531
-77.754842	2.413026	1.601536
-77.642293	-8.797761	1.606541
-77.306739	-0.855357	1.611546
-77.756032	-5.280453	1.616550
-78.504903	-12.958393	1.621555
-79.183777	-5.360076	1.626560
-79.311416	-14.647629	1.631565
-79.299126	-4.626613	1.636570
-79.286110	-5.492165	1.641574
-79.237367	-6.613251	1.646579
-80.030341	5.941560	1.651584
-80.411799	-0.749919	1.656589
-80.404349	-6.353893	1.661594
-80.712433	5.982571	1.666598
-81.109151	3.865101	1.671603
-82.307260	8.779668	1.676608
-81.571999	-10.887317	1.681613
-81.990918	-6.987024	1.686618
-82.276165	-4.078945	1.691622
-82.156114	-9.279784	1.696627
-82.791561	-9.376177	1.701632
-82.607750	3.731095	1.706637
-82.432411	4.399836	1.711642
-83.188886	3.816208	1.716646
-83.264668	-6.241938	1.721651
-84.094748	2.927148	1.726656
-83.980885	4.095904	1.731661
-84.995812	-3.689048	1.736666
-84.810592	1.233387	1.741670
-85.042035	-4.810882	1.746675
-85.634864	0.160700	1.751680
-85.432156	-4.803155	1.756685
-85.701811	-7.120867	1.761690
-85.805103	0.099362	1.766694
-85.520720	-7.806921	1.771699
-86.017500	-7.931369	1.776704
-86.436229	-7.179033	1.781709
-86.827017	3.743539	1.786714
-86.910202	-3.516694	1.791718
-87.015285	-5.578620	1.796723
-87.555063	-5.266061	1.801728
-88.154579	-4.703696	1.806733
-88.369174	-6.049274	1.811738
-88.501202	-2.257208	1.816742
-88.438736	-6.382841	1.821747
-88.462216	-9.957169	1.826752
-89.063397	-2.415316	1.831757
-89.279980	1.503894	1.836762
-89.930064	-0.149932	1.841766
-89.632074	0.316093	1.846771
-90.162344	0.070343	1.851776
-90.077094	-8.235007	1.856781
-90.248770	-2.772598	1.861786
-90.728680	1.558033	1.866790
-91.041458	-6.064856	1.871795
-91.240573	-1.050562	1.876800
-91.482464	-0.335427	1.881805
-92.127513	-0.249980	1.886810
-92.348768	1.869790	1.891814
-92.387406	-1.195965	1.896819
-92.657540	8.401076	1.901824
-92.659484	13.650233	1.906829
-92.683964	1.783870	1.911834
-93.184826	8.357720	1.916838
-93.439733	3.373818	1.921843
-93.960121	6.758504	1.926848
-93.991523	7.019879	1.931853
-94.510474	7.107714	1.936858
-94.768885	-2.016985	1.941862
-95.268601	0.560869	1.946867
-95.921309	6.123965	1.951872
-95.757879	7.857592	1.956877
-95.537170	5.042264	1.961882
-95.862678	8.099021	1.966886
-95.975950	9.556467	1.971891
-96.095082	6.652020	1.976896
-96.036869	5.668654	1.981901
-96.691899	2.585589	1.986906
-97.290077	9.320220	1.991910
-97.457505	11.229076	1.996915
-97.387867	6.305226	2.006912
-97.532345	7.256411	2.016909
-96.756802	5.877652	2.026906
-96.211497	-0.514502	2.036902
-96.147645	-4.407848	2.046899
-95.611714	7.520852	2.056896
-94.682518	3.317682	2.066893
-94.466417	-2.110561	2.076890
-93.403214	5.671232	2.086886
-93.220262	2.557508	2.096883
-93.081858	1.794936	2.106880
-93.042456	2.787000	2.116877
-92.261142	1.926857	2.126874
-91.214712	-1.166945	2.136870
-90.999479	-3.563468	2.146867
-90.102657	0.981562	2.156864
-89.487640	7.439753	2.166861
-89.144970	-4.188700	2.176858
-89.076709	-2.938232	2.186854
-88.584121	2.313203	2.196851
-87.951100	-1.675664	2.206848
-87.422780	7.270163	2.216845
-86.765124	3.404147	2.226842
-86.443113	3.471279	2.236838
-85.863063	10.530497	2.246835
-85.311033	1.270429	2.256832
-85.044471	12.823192	2.266829
-84.163666	9.090103	2.276826
-83.429886	9.105386	2.286822
-83.252988	10.601760	2.296819
-83.208397	5.944822	2.306816
-82.255592	10.468412	2.316813
-81.900826	5.810389	2.326810
-81.347408	5.176025	2.336806
-80.763612	5.417548	2.346803
-80.683232	8.633323	2.356800
-79.826047	7.514204	2.366797
-79.741584	5.784402	2.376794
-78.411865	8.506643	2.386790
-77.928629	6.533792	2.396787
-78.251771	9.185571	2.406784
-77.369866	14.049724	2.416781
-76.493593	8.714438	2.426778
-76.419742	6.951453	2.436774
-75.978535	5.514210	2.446771
-74.844700	0.860827	2.456768
-75.250496	-0.614758	2.466765
-74.328560	6.888233	2.476762
-73.409718	9.636842	2.486758
-73.363280	3.221485	2.496755
-72.760942	2.072608	2.506752
-72.538929	6.770895	2.516749
-72.019846	6.357321	2.526746
-70.762857	6.474356	2.536742
-70.331161	7.119849	2.546739
-70.377771	7.064177	2.556736
-70.466292	4.503006	2.566733
-69.504189	0.006413	2.576730
-69.073581	5.410113	2.586726
-68.390027	8.496531	2.596723
-67.730146	8.469542	2.606720
-67.054453	6.241621	2.616717
-66.770742	2.874524	2.626714
-66.572843	5.349626	2.636710
-65.471907	0.891467	2.646707
-65.251089	4.344996	2.656704
-65.024964	6.419701	2.666701
-64.110917	12.618799	2.676698
-63.947669	9.454309	2.686694
-63.575783	4.337440	2.696691
-62.712774	0.097127	2.706688
-62.239375	4.344210	2.716685
-61.781105	5.568416	2.726682
-60.984500	2.938246	2.736678
-60.702878	3.981056	2.746675
-60.613189	7.493146	2.756672
-59.381001	10.971938	2.766669
-59.436496	8.278879	2.776666
-58.949907	5.060558	2.786662
-57.794465	-3.308871	2.796659
-57.844182	-0.164578	2.806656
-57.368685	9.147492	2.816653
-57.062140	0.299689	2.826650
-56.094127	8.596918	2.836646
-55.805956	5.146759	2.846643
-54.959055	5.271032	2.856640
-54.881023	6.976134	2.866637
-54.519766	10.049698	2.876634
-53.527851	9.438494	2.886630
-53.548984	-1.420204	2.896627
-52.588184	6.304783	2.906624
-51.974022	2.683169	2.916621
-51.391614	-0.138351	2.926618
-51.445335	3.063590	2.936614
-51.234197	-0.719788	2.946611
-50.441810	3.239730	2.956608
-49.620311	8.471312	2.966605
-48.808918	8.148153	2.976602
-48.683631	4.261018	2.986598
-48.668780	9.270534	2.996595
-47.835509	-0.435913	3.006592
-47.486272	8.233871	3.016589
-46.394772	11.050465	3.026586
-46.086871	1.458015	3.036582
-45.894401	4.738590	3.046579
-45.542279	8.504167	3.056576
-44.680800	3.617862	3.066573
-44.211387	4.757959	3.076570
-43.173902	4.605283	3.086566
-42.951084	1.960482	3.096563
-42.926894	10.415103	3.106560
-42.592628	4.803616	3.116557
-41.620793	2.808062	3.126554
-41.362356	1.953825	3.136550
-40.901926	3.678205	3.146547
-40.238168	4.889221	3.156544
-39.833359	6.394235	3.166541
-38.655726	7.562748	3.176538
-38.361869	6.965888	3.186534
-38.272081	5.358795	3.196531
-38.163787	6.903934	3.206528
-37.223213	9.915238	3.216525
-36.925955	4.024448	3.226522
-35.604674	10.460683	3.236518
-35.432835	6.699299	3.246515
-35.522383	4.011576	3.256512
-34.985956	2.613268	3.266509
-34.152496	9.826022	3.276506
-33.979363	0.042446	3.286502
-33.330352	1.797467	3.296499
-32.867756	-0.770862	3.306496
-31.819256	-0.066789	3.316493
-31.407147	2.767558	3.326490
-30.932222	-3.616735	3.336486
-30.927287	-3.471408	3.346483
-30.542092	-1.792260	3.356480
-29.784106	2.622479	3.366477
-29.209370	-0.403746	3.376474
-28.276380	-0.394329	3.386470
-27.973252	0.258640	3.396467
-27.966931	1.496641	3.406464
-27.513575	2.613913	3.416461
-27.083296	-4.241723	3.426458
-25.568039	-1.792466	3.436454
-25.241465	8.037119	3.446451
-25.082442	-2.723096	3.456448
-24.789079	-4.438112	3.466445
-24.756811	-3.543132	3.476442
-23.762087	-4.743984	3.486438
-23.028854	-5.330492	3.496435
-22.357979	-7.494298	3.506432
-22.307561	-2.731109	3.516429
-22.134282	-0.543586	3.526426
-21.184949	-6.736115	3.536422
-20.700752	-3.475907	3.546419
-20.073036	-0.067124	3.556416
-19.301272	-1.220370	3.566413
-19.204282	-2.822254	3.576410
-19.359082	-7.552487	3.586406
-18.225186	5.299396	3.596403
-17.182151	3.558783	3.606400
-17.006086	-2.395379	3.616397
-16.476530	-3.482164	3.626394
-16.749445	-1.177212	3.636390
-15.793353	-4.294866	3.646387
-14.826434	-5.212594	3.656384
-14.679202	-2.042139	3.666381
-14.075547	1.623839	3.676378
-13.563178	0.774164	3.686374
-13.431816	-1.260759	3.696371
-12.794279	-0.048800	3.706368
-11.822916	6.499285	3.716365
-11.550187	2.699920	3.726362
-11.381605	-0.307015	3.736358
-10.455251	-2.751603	3.746355
-10.268998	1.432771	3.756352
-9.235379	-1.798399	3.766349
-8.709549	2.031828	3.776346
-8.609240	0.245691	3.786342
-8.390753	-1.391069	3.796339
-7.823381	-2.236691	3.806336
-7.408207	-4.357264	3.816333
-6.762528	-5.642808	3.826330
-5.983394	-0.379242	3.836326
-5.639178	-0.204713	3.846323
-5.062043	0.706266	3.856320
-4.395955	0.076427	3.866317
-4.264742	3.509153	3.876314
-4.063607	4.365004	3.886310
-3.654420	19.389522	3.896307
-2.945006	35.228656	3.906304
-2.874475	46.390848	3.916301
-1.954331	64.823106	3.926298
-1.764577	68.680663	3.936294
-1.011822	87.861433	3.946291
-0.520376	103.360978	3.956288
0.000000	116.126665	3.961293
0.110267	111.281664	3.966298
-0.129836	110.553842	3.971302
0.128346	134.485486	3.976307
0.261352	143.377192	3.981312
0.418289	129.938387	3.986317
0.326653	148.726780	3.991322
-0.119643	139.878211	3.996326
0.008087	141.301071	4.001331
0.700505	160.944236	4.006336
1.170555	158.263824	4.011341
1.056801	141.048742	4.016346
1.047325	138.405500	4.021350
0.585464	136.867695	4.026355
0.784790	138.200242	4.031360
0.634467	136.626279	4.036365
0.941288	141.374680	4.041370
1.007003	142.392801	4.046374
0.518829	138.128780	4.051379
0.547175	138.364976	4.056384
1.033521	139.779103	4.061389
0.716708	144.862500	4.066394
0.746832	150.122496	4.071398
0.873957	147.391411	4.076403
1.042670	137.864348	4.081408
1.124621	143.097238	4.086413
1.079493	140.741159	4.091418
0.968924	133.678145	4.096422
0.922550	141.968365	4.101427
1.188094	139.161810	4.106432
1.017349	140.027154	4.111437
0.972446	147.307902	4.116442
0.906863	136.302100	4.121446
0.604908	144.281187	4.126451
1.131154	131.974096	4.131456
0.830243	135.289613	4.136461
0.716506	137.778533	4.141466
0.855652	133.533282	4.146470
0.974265	140.962415	4.151475
1.096119	129.035065	4.156480
0.997618	135.166265	4.161485
1.051742	144.560716	4.166490
1.518351	147.262430	4.171494
1.083257	143.252684	4.176499
1.326829	132.470530	4.181504
1.337266	138.274612	4.186509
1.153117	139.986784	4.191514
0.970785	138.281794	4.196518
0.741088	151.925378	4.201523
0.804656	140.715838	4.206528
1.421824	149.098251	4.211533
1.041985	157.725467	4.216538
1.307229	154.662690	4.221542
1.192526	164.662576	4.226547
1.229494	164.388053	4.231552
1.149478	167.874611	4.236557
1.463962	158.157017	4.241562
1.690568	162.000496	4.246566
1.276539	157.481241	4.251571
1.337431	149.049914	4.256576
1.111441	148.841902	4.261581
1.274991	147.924282	4.266586
1.605824	150.992122	4.271590
1.353452	156.777276	4.276595
0.900224	150.201381	4.281600
1.375233	146.615354	4.286605
1.402854	157.311113	4.291610
1.548461	150.442074	4.296614
1.410945	160.369601	4.301619
1.636427	152.301629	4.306624
1.400179	158.663228	4.311629
1.550897	163.455076	4.316634
1.422093	159.606146	4.321638
1.502054	172.252093	4.326643
1.595898	162.281163	4.331648
1.336925	159.167642	4.336653
1.246218	163.655629	4.341658
1.540633	162.110058	4.346662
1.625876	168.481401	4.351667
1.656874	161.911891	4.356672
1.343661	158.933420	4.361677
1.468383	162.941560	4.366682
1.614436	157.755579	4.371686
1.735229	168.547479	4.376691
1.623601	161.241009	4.381696
1.350896	165.425315	4.386701
1.446146	158.864722	4.391706
1.403292	155.179497	4.396710
1.384941	171.358969	4.401715
1.477604	156.025619	4.406720
1.597799	168.443795	4.411725
1.387427	162.959314	4.416730
1.556345	167.609105	4.421734
1.347812	162.953247	4.426739
1.521003	174.290602	4.431744
1.857810	188.582614	4.436749
1.929776	186.967490	4.441754
2.113678	183.964910	4.446758
1.642490	182.197605	4.451763
1.808598	175.306361	4.456768
1.479707	171.716571	4.461773
1.808386	196.257353	4.466778
2.290520	188.294685	4.471782
1.971675	184.994386	4.476787
1.952194	172.323516	4.481792
1.938441	173.727416	4.486797
2.139666	172.981064	4.491802
1.900490	169.965680	4.496806
1.572577	171.070788	4.501811
1.833931	168.922951	4.506816
1.966650	181.180985	4.511821
1.908701	191.380803	4.516826
2.322564	190.158204	4.521830
1.807470	183.304086	4.526835
1.883280	178.078484	4.531840
2.216442	192.152768	4.536845
2.295862	183.139549	4.541850
2.332082	170.630797	4.546854
2.135824	170.171352	4.551859
2.172200	163.142250	4.556864
2.103395	166.734620	4.561869
1.828359	173.219363	4.566874
2.064514	158.395043	4.571878
1.844262	166.446761	4.576883
1.888915	173.330670	4.581888
1.983427	177.042988	4.586893
2.214029	181.262335	4.591898
2.306421	185.136339	4.596902
1.825199	188.204868	4.601907
1.833007	191.326491	4.606912
2.160426	192.642136	4.611917
2.105852	198.453260	4.616922
2.059498	194.259206	4.621926
2.366394	192.854047	4.626931
2.574148	188.275328	4.631936
1.933802	187.556429	4.636941
2.347947	208.084814	4.641946
2.298188	197.184064	4.646950
1.958314	203.330959	4.651955
2.393932	191.639147	4.656960
2.014454	197.396772	4.661965
2.038677	189.357153	4.666970
2.487224	191.071439	4.671974
1.947093	194.598457	4.676979
2.265974	189.176577	4.681984
2.225412	195.067764	4.686989
2.396312	195.329082	4.691994
2.366876	202.781437	4.696998
2.269849	198.452951	4.702003
2.084249	205.641872	4.707008
2.543832	215.747961	4.712013
2.458716	221.067163	4.717018
3.102634	216.508683	4.722022
2.769652	215.305022	4.727027
2.457621	203.309561	4.732032
2.374952	196.011194	4.737037
2.252382	200.073908	4.742042
2.665657	194.665711	4.747046
2.363043	195.589684	4.752051
2.690605	198.338502	4.757056
2.729186	195.266940	4.762061
2.527873	190.328366	4.767066
2.731354	191.720378	4.772070
2.505958	192.037461	4.777075
2.089334	192.061800	4.782080
2.579309	200.600209	4.787085
2.725116	217.791725	4.792090
3.068432	216.709892	4.797094
2.605470	207.496901	4.802099
2.520458	189.435701	4.807104
2.843887	202.812323	4.812109
2.804573	199.983921	4.817114
2.518088	196.969617	4.822118
2.633163	200.106072	4.827123
3.038759	210.056100	4.832128
2.744848	202.370045	4.837133
2.778675	202.156125	4.842138
2.775728	206.836019	4.847142
2.378222	200.805038	4.852147
2.899855	204.599137	4.857152
2.683434	216.788511	4.862157
3.017947	218.508012	4.867162
2.985746	211.967368	4.872166
2.673535	229.081960	4.877171
3.010336	223.650935	4.882176
3.430792	223.192938	4.887181
2.625295	213.786837	4.892186
2.986769	214.363149	4.897190
2.617911	210.678371	4.902195
3.239260	213.283083	4.907200
2.774876	219.357742	4.912205
3.016651	221.186687	4.917210
2.977358	231.405752	4.922214
2.452907	222.022052	4.927219
3.164192	218.965308	4.932224
3.423920	212.780725	4.937229
2.898945	223.107521	4.942234
3.294085	218.572201	4.947238
3.048242	221.806338	4.952243
2.896036	212.623750	4.957248
3.261512	220.001582	4.962253
3.075407	215.326377	4.967258
3.218275	215.009950	4.972262
2.623669	219.782549	4.977267
2.929432	219.358341	4.982272
3.056744	217.971827	4.987277
2.781475	223.418901	4.992282
3.295388	216.909749	4.997286
2.849682	218.669238	5.002291
2.910498	223.693490	5.007296
3.249595	222.681921	5.012301
2.945108	225.419042	5.017306
3.175003	229.122813	5.022310
2.840849	230.478842	5.027315
2.920555	226.255537	5.032320
2.974629	241.974468	5.037325
3.049964	245.851158	5.042330
3.479855	243.044146	5.047334
3.388379	242.846696	5.052339
3.467753	243.150829	5.057344
3.587257	242.363494	5.062349
3.409665	235.893078	5.067354
3.459927	227.482362	5.072358
3.305921	228.765872	5.077363
2.966560	221.653248	5.082368
3.258743	234.231186	5.087373
3.500860	248.892427	5.092378
3.951151	246.050581	5.097382
3.531262	242.943275	5.102387
3.148816	235.967111	5.107392
3.170733	239.836351	5.112397
3.116460	242.467830	5.117402
3.504849	248.646170	5.122406
3.477725	255.981125	5.127411
3.656491	251.454388	5.132416
3.611667	255.356235	5.137421
3.379364	259.616491	5.142426
3.665822	247.169719	5.147430
3.599720	255.010661	5.152435
3.904232	244.861141	5.157440
3.922967	246.297923	5.162445
3.676170	233.846125	5.167450
3.543547	233.126768	5.172454
3.480468	228.913180	5.177459
3.279590	224.604123	5.182464
3.720534	239.167764	5.187469
3.593394	242.715505	5.192474
3.848838	249.389244	5.197478
3.708723	253.783754	5.202483
3.645165	246.665872	5.207488
3.669829	247.829639	5.212493
3.574698	257.301320	5.217498
3.696180	248.695935	5.222502
3.578408	252.172606	5.227507
3.746577	246.524384	5.232512
3.858511	248.648926	5.237517
3.671214	255.581864	5.242522
3.788052	251.330590	5.247526
3.575795	257.549258	5.252531
3.797094	254.632557	5.257536
3.816411	246.751870	5.262541
3.626709	247.980862	5.267546
4.106009	246.336713	5.272550
3.930159	244.320645	5.277555
3.529391	252.318426	5.282560
3.727515	255.201431	5.287565
3.711554	250.078773	5.292570
3.764709	249.184772	5.297574
3.631647	251.059795	5.302579
3.606203	258.252117	5.307584
3.589897	261.330074	5.312589
3.783040	269.025997	5.317594
3.915560	272.245154	5.322598
3.935417	274.225936	5.327603
4.026491	272.800802	5.332608
4.312010	275.322098	5.337613
3.915017	283.920424	5.342618
4.174589	277.618783	5.347622
4.120625	281.778335	5.352627
3.849224	267.258080	5.357632
4.445662	270.989852	5.362637
3.805088	271.144193	5.367642
3.747829	279.964538	5.372646
3.987919	282.375893	5.377651
4.432086	280.841650	5.382656
4.036550	279.230164	5.387661
4.066676	279.769808	5.392666
4.137640	278.657877	5.397670
4.142925	288.328980	5.402675
4.152182	279.541844	5.407680
4.106343	281.827153	5.412685
4.271298	287.970911	5.417690
4.363941	277.187008	5.422694
4.326653	280.391643	5.427699
3.680051	281.230310	5.432704
4.098537	286.217522	5.437709
3.804575	294.505476	5.442714
4.092108	278.625788	5.447718
4.332935	287.930950	5.452723
4.408747	283.344405	5.457728
4.312099	285.121976	5.462733
4.289441	285.027639	5.467738
4.184099	279.305200	5.472742
4.234552	288.105508	5.477747
4.229647	285.758926	5.482752
4.451816	281.105157	5.487757
4.182425	283.374873	5.492762
4.561148	283.356853	5.497766
4.341517	292.307050	5.502771
4.503698	285.979536	5.507776
4.342354	281.983815	5.512781
4.114304	299.404831	5.517786
4.672120	308.723614	5.522790
4.666909	316.858768	5.527795
4.709760	302.029814	5.532800
4.463233	286.461590	5.537805
4.318938	287.844824	5.542810
4.553004	295.869710	5.547814
4.505961	309.143104	5.552819
4.467009	309.453123	5.557824
4.580294	308.875570	5.562829
4.446570	313.145704	5.567834
4.884900	299.903131	5.572838
4.686725	309.495391	5.577843
4.461346	305.911501	5.582848
4.692292	308.590052	5.587853
4.486425	317.259689	5.592858
4.828419	310.676199	5.597862
5.050518	314.099631	5.602867
4.301112	302.992058	5.607872
4.723204	306.561326	5.612877
4.309867	301.719218	5.617882
4.394555	305.341351	5.622886
4.135374	309.504589	5.627891
4.425875	316.223481	5.632896
4.507815	310.538128	5.637901
4.594358	318.389983	5.642906
5.030867	310.934291	5.647910
4.650144	315.524705	5.652915
4.955192	315.034167	5.657920
4.753946	306.523613	5.662925
4.824017	317.712699	5.667930
4.597604	303.324573	5.672934
4.905532	326.897499	5.677939
4.969397	335.907704	5.682944
5.054736	319.347802	5.687949
5.115987	320.499514	5.692954
5.033272	312.862579	5.697958
4.795104	316.190445	5.702963
4.956222	315.421897	5.707968
4.985112	309.207009	5.712973
4.931895	315.732979	5.717978
4.848084	303.850391	5.722982
4.904538	309.875113	5.727987
4.954034	319.732298	5.732992
4.897187	312.066000	5.737997
4.831578	332.005297	5.743002
5.403102	331.504645	5.748006
4.772317	320.872029	5.753011
4.882784	336.442999	5.758016
5.079398	330.119565	5.763021
5.068930	337.398160	5.768026
5.121330	334.153562	5.773030
4.902700	333.162933	5.778035
4.841294	341.908027	5.783040
5.002162	344.426717	5.788045
5.398876	341.042747	5.793050
5.571869	327.895512	5.798054
5.323380	332.126684	5.803059
4.769798	339.585289	5.808064
5.212657	343.461365	5.813069
4.905029	342.820044	5.818074
5.112307	333.834173	5.823078
5.420086	341.186294	5.828083
5.048196	342.054689	5.833088
5.577344	340.057865	5.838093
5.215944	340.541795	5.843098
5.537160	336.897568	5.848102
5.368585	340.496114	5.853107
5.430950	330.194658	5.858112
5.424454	333.818428	5.863117
5.032404	347.544547	5.868122
5.175790	330.962885	5.873126
5.204796	341.680685	5.878131
5.359515	336.116800	5.883136
5.349159	336.305278	5.888141
5.066854	338.440980	5.893146
4.921503	332.493834	5.898150
5.102448	333.908371	5.903155
5.209731	334.179659	5.908160
5.353203	343.601346	5.913165
5.631510	355.615222	5.918170
5.625459	355.347437	5.923174
5.764288	358.821890	5.928179
5.253335	343.668377	5.933184
5.240493	340.247336	5.938189
5.490164	359.757608	5.943194
6.075531	363.114641	5.948198
5.473757	352.167406	5.953203
5.443027	342.899277	5.958208
5.811404	345.771440	5.963213
5.287542	349.140911	5.968218
5.796413	344.790224	5.973222
5.536096	334.485539	5.978227
5.782595	331.593351	5.983232
5.929894	336.578774	5.988237
5.443111	338.952162	5.993242
5.468945	330.051670	5.998246
5.612607	336.091211	6.003251
5.274654	334.951597	6.008256
5.297087	334.998893	6.013261
5.556508	354.963221	6.018266
5.754853	353.976863	6.023270
5.512079	362.225190	6.028275
5.618881	363.028075	6.033280
5.903483	350.224011	6.038285
5.371686	338.569782	6.043290
5.611886	334.542773	6.048294
5.366923	336.226526	6.053299
5.643886	350.714709	6.058304
5.452288	347.581107	6.063309
5.688135	360.411575	6.068314
5.474863	345.271532	6.073318
5.659112	351.665394	6.078323
5.726386	344.631380	6.083328
5.548984	342.283343	6.088333
5.203124	341.727108	6.093338
5.703426	344.641876	6.098342
5.774118	348.582593	6.103347
5.431658	348.946494	6.108352
5.837182	345.966111	6.113357
5.531981	342.185909	6.118362
5.412929	332.343155	6.123366
5.408360	334.473305	6.128371
5.405679	343.557218	6.133376
5.760428	347.937490	6.138381
5.841412	355.321988	6.143386
5.367679	340.605579	6.148390
5.249368	350.093597	6.153395
5.648704	358.200186	6.158400
5.934209	357.965814	6.163405
5.688172	358.365229	6.168410
5.661298	343.101068	6.173414
5.654500	331.453173	6.178419
5.657032	343.412172	6.183424
5.794482	330.548919	6.188429
5.256149	324.672840	6.193434
5.609737	326.224845	6.198438
5.637674	327.280534	6.203443
5.722960	329.921798	6.208448
5.761802	325.473915	6.213453
5.555007	337.927623	6.218458
5.892505	332.186403	6.223462
5.707268	329.415646	6.228467
5.288175	327.070678	6.233472
5.506841	322.986933	6.238477
5.473616	331.582070	6.243482
5.677371	330.930229	6.248486
5.600973	328.249988	6.253491
5.815196	338.416738	6.258496
5.537924	335.419950	6.263501
5.109644	339.005402	6.268506
5.536348	332.924332	6.273510
5.744080	329.683871	6.278515
5.422149	327.181309	6.283520
5.580986	322.822195	6.288525
5.288061	328.389128	6.293530
5.524507	328.007416	6.298534
5.716562	334.450670	6.303539
5.384909	335.730383	6.308544
5.476911	333.093360	6.313549
5.873718	337.033598	6.318554
5.629294	324.980005	6.323558
5.573790	341.016754	6.328563
5.665088	333.779659	6.333568
5.568238	323.515808	6.338573
5.753010	330.150030	6.343578
5.666656	327.430220	6.348582
5.863900	331.218224	6.353587
5.820464	342.213134	6.358592
5.777101	338.686142	6.363597
5.264777	335.931830	6.368602
6.017990	333.355725	6.373606
5.686141	332.452440	6.378611
5.694305	335.077314	6.383616
5.801328	326.856977	6.388621
5.520377	332.934572	6.393626
5.534937	325.342503	6.398630
5.531833	330.120532	6.403635
5.705460	339.091395	6.408640
6.233399	329.432013	6.413645
5.285746	324.759039	6.418650
5.645351	323.718942	6.423654
5.869865	331.969971	6.428659
5.132977	317.275831	6.433664
5.790709	323.506910	6.438669
5.670735	318.084149	6.443674
5.732686	307.751132	6.448678
4.989095	316.119037	6.453683
5.383450	335.258594	6.458688
5.782690	330.042385	6.463693
5.488129	323.432074	6.468698
5.565493	330.333065	6.473702
5.619849	331.542806	6.478707
5.583419	334.747317	6.483712
5.569779	327.343166	6.488717
5.261822	331.865234	6.493722
5.517885	336.447631	6.498726
5.767022	338.575997	6.503731
5.649288	344.118649	6.508736
5.718848	329.725258	6.513741
5.346005	331.856161	6.518746
5.493778	325.809306	6.523750
5.251183	328.122285	6.528755
5.135482	336.037473	6.533760
5.177547	329.219390	6.538765
5.643777	338.274123	6.543770
5.680789	338.341282	6.548774
5.332982	332.881446	6.553779
5.544044	333.063707	6.558784
5.451326	337.064826	6.563789
5.377348	342.417120	6.568794
5.384697	342.811636	6.573798
5.607733	344.361951	6.578803
5.267825	341.555313	6.583808
5.808020	335.915213	6.588813
5.648096	341.521423	6.593818
5.592484	333.313910	6.598822
5.633593	339.992792	6.603827
5.551936	341.394690	6.608832
6.103370	325.508413	6.613837
5.538884	335.034692	6.618842
5.285372	339.013548	6.623846
5.704129	339.387897	6.628851
5.337832	338.939270	6.633856
5.555577	341.202270	6.638861
5.803366	353.322169	6.643866
5.590216	346.303617	6.648870
5.852570	349.676455	6.653875
5.409561	344.313791	6.658880
5.891884	340.065343	6.663885
5.901805	344.325633	6.668890
5.579953	343.594791	6.673894
5.539089	349.875224	6.678899
5.506128	344.853281	6.683904
5.533756	346.525963	6.688909
5.239359	334.227089	6.693914
5.340038	337.191814	6.698918
5.404712	342.440126	6.703923
5.310569	346.501583	6.708928
5.740847	348.076375	6.713933
5.748371	344.044690	6.718938
5.429556	340.459614	6.723942
5.847978	324.553049	6.728947
5.621027	342.135289	6.733952
5.571128	334.945628	6.738957
5.373423	344.240435	6.743962
5.806939	344.704221	6.748966
5.557956	334.261717	6.753971
5.530439	337.660988	6.758976
5.606280	336.023097	6.763981
5.598147	338.201263	6.768986
5.946852	341.582717	6.773990
5.699630	338.774213	6.778995
5.387347	341.648616	6.784000
5.786311	339.343154	6.789005
5.823922	344.864630	6.794010
5.853482	339.456399	6.799014
5.484648	334.426972	6.804019
5.798713	344.223734	6.809024
5.832291	331.209074	6.814029
5.548902	333.363927	6.819034
5.530563	334.072521	6.824038
5.563864	336.842156	6.829043
5.674406	342.181359	6.834048
5.660254	324.001351	6.839053
5.488733	336.708964	6.844058
5.543412	341.993643	6.849062
5.490572	338.756043	6.854067
5.567239	341.686565	6.859072
5.841894	328.823963	6.864077
5.733221	338.987520	6.869082
5.422856	327.513743	6.874086
5.745847	330.402505	6.879091
5.329576	329.278326	6.884096
5.551878	324.143626	6.889101
5.343906	333.803873	6.894106
5.626259	336.439572	6.899110
5.609375	344.320298	6.904115
5.710297	338.862920	6.909120
6.050807	344.903260	6.914125
5.860700	323.552207	6.919130
5.331674	319.873519	6.924134
4.927035	305.785403	6.929139
5.273685	323.144872	6.934144
5.440927	323.644051	6.939149
5.539251	336.040461	6.944154
5.463389	340.013629	6.949158
5.678599	334.259930	6.954163
5.357762	347.161792	6.959168
5.775749	340.493616	6.964173
5.494014	338.269497	6.969178
5.573756	340.630051	6.974182
5.715373	346.467433	6.979187
5.521480	344.488982	6.984192
5.373978	341.342144	6.989197
5.343880	343.469968	6.994202
5.618028	334.837458	6.999206
5.479295	335.394069	7.004211
5.504489	340.003149	7.009216
5.810259	329.059268	7.014221
5.157573	345.493314	7.019226
5.408633	334.548511	7.024230
6.023642	340.194657	7.029235
5.653104	334.925047	7.034240
5.913139	337.355431	7.039245
5.849750	340.197164	7.044250
5.265125	341.728489	7.049254
5.817308	335.713181	7.054259
5.571909	339.127607	7.059264
5.807616	334.003459	7.064269
5.906652	341.328174	7.069274
5.485789	340.590698	7.074278
5.414327	321.818547	7.079283
5.320448	340.370208	7.084288
5.825885	332.372188	7.089293
5.720787	342.895861	7.094298
5.726672	337.206597	7.099302
5.577183	323.872606	7.104307
5.555041	334.974909	7.109312
5.353872	326.524445	7.114317
5.258923	332.626682	7.119322
5.313247	330.466970	7.124326
5.581014	332.238070	7.129331
5.262732	333.594783	7.134336
5.703092	332.598981	7.139341
5.487781	343.636641	7.144346
5.192124	340.079574	7.149350
5.746737	334.351793	7.154355
5.702672	340.597922	7.159360
5.678968	337.229204	7.164365
5.699186	332.053397	7.169370
5.948933	335.966056	7.174374
5.609986	333.811014	7.179379
5.507375	333.567849	7.184384
5.493920	336.306844	7.189389
5.863105	330.481564	7.194394
5.772685	328.812775	7.199398
5.826441	330.364301	7.204403
5.526542	320.056335	7.209408
5.572793	299.930637	7.214413
5.555566	314.290876	7.219418
5.547711	319.775175	7.224422
5.821785	313.866725	7.229427
5.013588	308.985240	7.234432
5.440644	314.214730	7.239437
5.928770	332.042431	7.244442
5.572511	337.049804	7.249446
5.587880	328.268014	7.254451
5.567694	336.316936	7.259456
5.731138	333.042285	7.264461
5.467379	333.700745	7.269466
5.661014	333.765511	7.274470
5.749036	313.127043	7.279475
5.583404	317.490765	7.284480
5.587895	313.301371	7.289485
5.364796	317.601329	7.294490
5.272267	318.220305	7.299494
5.534029	325.778949	7.304499
5.518187	337.797771	7.309504
5.781286	340.964843	7.314509
5.393217	342.440061	7.319514
5.623024	346.109069	7.324518
6.126465	339.101632	7.329523
5.907100	329.280924	7.334528
5.261520	315.841167	7.339533
5.342500	318.726716	7.344538
5.235159	327.944080	7.349542
5.647283	334.716691	7.354547
5.705395	333.350502	7.359552
5.647943	335.046005	7.364557
5.512841	325.120347	7.369562
5.354894	328.704570	7.374566
5.841634	336.860730	7.379571
5.298895	335.291286	7.384576
5.547500	333.332091	7.389581
5.878724	328.765629	7.394586
5.809789	336.477334	7.399590
5.559620	324.760005	7.404595
5.473707	318.797223	7.409600
5.463903	321.529316	7.414605
5.109728	320.866815	7.419610
5.472737	339.622140	7.424614
5.667913	335.959695	7.429619
5.540544	336.745484	7.434624
5.551960	348.098806	7.439629
5.628992	341.503034	7.444634
5.552109	341.081829	7.449638
5.881283	334.392769	7.454643
5.566921	343.357834	7.459648
5.699710	348.399318	7.464653
5.784437	336.496630	7.469658
5.350257	323.561591	7.474662
5.191138	330.347773	7.479667
5.598190	332.460887	7.484672
5.533948	332.933059	7.489677
5.221174	343.441815	7.494682
5.593473	338.467110	7.499686
5.889048	341.262092	7.504691
5.640299	345.369919	7.509696
5.852036	337.550794	7.514701
5.561492	342.861089	7.519706
5.561104	344.139521	7.524710
5.715466	335.427700	7.529715
5.512162	327.170563	7.534720
5.649896	335.625020	7.539725
5.369788	330.148250	7.544730
5.891560	331.316393	7.549734
5.447258	327.684541	7.554739
5.548846	326.684870	7.559744
5.600567	327.588134	7.564749
5.417158	332.748760	7.569754
5.631957	333.180376	7.574758
5.877250	328.621049	7.579763
5.213068	334.148075	7.584768
5.764126	332.527477	7.589773
5.536193	333.192979	7.594778
5.265588	326.303662	7.599782
5.928900	327.168049	7.604787
5.364109	335.375068	7.609792
5.775024	329.761553	7.614797
5.588141	335.220122	7.619802
5.402749	333.835137	7.624806
5.968041	325.201308	7.629811
5.179703	323.942433	7.634816
5.348325	331.335335	7.639821
5.718701	345.011598	7.644826
5.416345	338.975152	7.649830
5.723881	344.024058	7.654835
5.587393	341.590516	7.659840
5.727779	334.870923	7.664845
5.948648	340.755997	7.669850
5.128442	334.791200	7.674854
5.555300	335.268685	7.679859
5.708514	345.802508	7.684864
5.556083	344.361737	7.689869
5.355541	330.795290	7.694874
5.384355	343.825866	7.699878
5.905024	336.258900	7.704883
5.519301	346.342481	7.709888
5.319610	345.234987	7.714893
5.332797	343.391773	7.719898
5.253799	345.913244	7.724902
5.645053	338.214691	7.729907
5.410648	341.741293	7.734912
5.690934	331.560718	7.739917
5.637736	332.901208	7.744922
5.740053	352.757269	7.749926
5.998275	333.069730	7.754931
5.728338	339.645483	7.759936
5.749129	342.977074	7.764941
5.214012	336.891676	7.769946
5.589681	334.188060	7.774950
5.845769	340.864897	7.779955
5.349316	345.631642	7.784960
5.862415	338.186086	7.789965
5.756600	338.342063	7.794970
5.153627	331.302337	7.799974
5.299082	324.313029	7.804979
5.407801	343.810567	7.809984
5.653889	338.947387	7.814989
6.104819	342.774741	7.819994
5.725643	344.697827	7.824998
5.669049	330.302054	7.830003
5.477224	327.620916	7.835008
5.311779	315.735292	7.840013
5.382659	331.312460	7.845018
5.521539	341.120850	7.850022
5.845239	343.664648	7.855027
5.714492	354.423305	7.860032
5.556401	334.908563	7.865037
5.643804	325.593459	7.870042
5.460020	324.423362	7.875046
5.715161	328.275061	7.880051
6.104127	315.068686	7.885056
5.682941	310.901695	7.890061
5.588409	311.021103	7.895066
5.377030	317.198525	7.900070
5.582903	315.100494	7.905075
5.290101	318.705844	7.910080
5.681732	310.896510	7.915085
5.524836	311.734382	7.920090
5.550506	300.372490	7.925094
5.427399	298.642385	7.930099
5.399282	314.184429	7.935104
5.552912	310.370309	7.940109
5.789372	319.185782	7.945114
5.491511	328.189383	7.950118
5.846841	312.526836	7.955123
5.545448	320.654613	7.960128
5.670965	310.742035	7.965146
5.869475	306.501373	7.970163
5.414424	318.523632	7.975181
5.526011	306.438807	7.980198
5.251988	321.493767	7.985216
5.531674	315.615180	7.990234
5.348686	314.662608	7.995251
5.713648	324.413646	8.000269
5.938959	324.779313	8.005286
5.342195	329.612925	8.010304
5.509089	325.901065	8.015322
5.357008	333.969062	8.020339
6.138654	334.474775	8.025357
5.947844	329.048590	8.030374
5.686026	335.956692	8.035392
5.312844	325.266908	8.040410
5.656201	327.510678	8.045427
5.415650	320.558601	8.050445
5.573655	335.053586	8.055462
5.525392	343.067452	8.060480
5.552934	340.712301	8.065498
6.101452	348.654755	8.070515
5.720427	350.440836	8.075533
5.971651	331.293657	8.080550
5.458715	317.416389	8.085568
5.700860	324.987122	8.090586
5.868506	330.685555	8.095603
5.146043	340.389235	8.100621
5.684766	335.817556	8.105638
6.019858	348.170461	8.110656
5.798284	338.788637	8.115674
5.951824	343.381620	8.120691
5.831800	334.630815	8.125709
5.648963	324.602315	8.130726
5.673600	325.917744	8.135744
5.644124	335.307720	8.140762
5.722790	344.125347	8.145779
5.854667	346.247624	8.150797
5.951168	336.301579	8.155814
5.448546	340.530320	8.160832
5.828298	339.962937	8.165850
5.892632	339.353457	8.170867
5.943142	342.851762	8.175885
5.820671	331.289577	8.180902
5.761160	335.906472	8.185920
5.970571	334.472704	8.190938
5.978631	323.574867	8.195955
5.617533	322.101103	8.200973
5.886676	326.609698	8.205990
5.589946	327.154988	8.211008
5.640734	331.382223	8.216026
5.938661	334.390489	8.221043
5.777655	346.183663	8.226061
5.860498	343.652592	8.231078
5.909350	350.038661	8.236096
5.793782	348.854622	8.241114
6.087446	348.619457	8.246131
5.892489	355.554959	8.251149
6.001913	334.530236	8.256166
5.794924	329.362201	8.261184
5.955342	343.525463	8.266202
5.862275	326.442440	8.271219
5.707886	334.419282	8.276237
5.974397	341.837885	8.281254
6.115098	349.424523	8.286272
5.947859	347.361817	8.291290
6.102386	338.422828	8.296307
5.698830	334.125017	8.301325
5.836095	333.175914	8.306342
5.912686	342.505095	8.311360
5.757568	347.446235	8.316378
6.099637	342.422538	8.321395
6.110838	353.917341	8.326413
5.911070	340.729431	8.331430
5.611471	334.386190	8.336448
6.167549	342.188604	8.341466
6.410587	340.269894	8.346483
5.944771	334.230402	8.351501
6.030199	328.669419	8.356518
5.851942	334.305288	8.361536
5.519832	332.208456	8.366554
5.915382	335.567493	8.371571
5.811948	341.573485	8.376589
6.088855	334.833809	8.381606
5.893050	346.462026	8.386624
6.016035	338.332694	8.391642
6.185512	342.295186	8.396659
6.154693	348.378164	8.401677
6.306843	349.758821	8.406694
6.383110	339.408855	8.411712
5.891924	324.401574	8.416730
6.065798	319.782925	8.421747
5.805977	327.403906	8.426765
5.929006	333.096708	8.431782
6.127277	344.742072	8.436800
6.039456	338.353025	8.441818
6.372633	341.485155	8.446835
6.247341	345.194038	8.451853
6.067474	337.572896	8.456870
5.845357	330.346533	8.461888
5.805277	344.894653	8.466906
6.347355	338.750889	8.471923
5.930241	349.583822	8.476941
6.131705	342.859120	8.481958
6.249122	352.715230	8.486976
5.952063	351.351348	8.491994
6.439983	347.380905	8.497011
5.953305	358.666548	8.502029
6.010512	341.922875	8.507046
6.052610	346.410245	8.512064
5.944466	351.561773	8.517082
6.251134	342.011977	8.522099
6.062989	353.941949	8.527117
6.233118	350.822856	8.532134
6.333558	348.194356	8.537152
6.495366	359.362614	8.542170
6.366128	336.724829	8.547187
6.315531	334.426102	8.552205
5.771764	347.326953	8.557223
5.940167	345.946946	8.562240
6.137294	345.114692	8.567258
6.336444	343.231260	8.572275
6.176609	352.256670	8.577293
5.998058	353.985782	8.582311
6.388350	343.681283	8.587328
6.242726	350.176717	8.592346
6.212139	342.314437	8.597363
6.465840	344.322954	8.602381
6.118514	342.054939	8.607399
6.256658	350.475094	8.612416
5.957005	352.586091	8.617434
6.394722	345.016501	8.622451
6.116528	353.000126	8.627469
6.209222	342.537133	8.632487
6.297416	345.354206	8.637504
5.908358	350.152123	8.642522
5.891840	349.460639	8.647539
5.920927	348.298116	8.652557
6.268311	355.969136	8.657575
6.527607	366.904378	8.662592
6.018543	366.252197	8.667610
6.348291	370.890160	8.672627
6.517532	367.622884	8.677645
6.329603	372.698557	8.682663
6.497560	367.503321	8.687680
6.021350	363.204263	8.692698
6.336088	366.190967	8.697715
6.289828	371.910305	8.702733
6.335046	373.367678	8.707751
7.066783	371.618543	8.712768
6.300520	359.343028	8.717786
6.301327	359.740716	8.722803
6.455918	352.385894	8.727821
6.287843	350.926065	8.732839
6.234697	349.659663	8.737856
6.143373	368.681207	8.742874
6.332932	369.289158	8.747891
6.435035	374.890580	8.752909
6.270347	366.014216	8.757927
6.462430	372.273712	8.762944
6.599109	375.919465	8.767962
6.704547	368.218894	8.772979
6.600098	366.622865	8.777997
6.101311	364.249193	8.783015
6.589132	369.679727	8.788032
6.577794	371.682437	8.793050
6.774129	373.504289	8.798067
6.577332	365.071605	8.803085
6.241983	358.109120	8.808103
6.729872	361.478940	8.813120
6.464404	364.127370	8.818138
6.886508	364.673640	8.823155
6.882914	345.623173	8.828173
6.224449	351.444738	8.833191
6.529987	338.591059	8.838208
6.557740	357.644426	8.843226
6.690872	345.486773	8.848243
6.230239	350.049757	8.853261
6.265672	345.395989	8.858279
6.257823	348.338561	8.863296
6.573619	366.116067	8.868314
6.875758	371.616719	8.873331
7.060933	370.079450	8.878349
6.634774	364.759555	8.883367
6.575717	353.487216	8.888384
6.437420	356.671130	8.893402
6.575439	341.372750	8.898419
6.404168	354.650735	8.903437
6.411336	348.530819	8.908455
6.857561	357.117296	8.913472
6.678190	362.412528	8.918490
6.676501	359.241461	8.923507
6.386285	348.469238	8.928525
6.532458	358.595395	8.933543
6.640567	364.382060	8.938560
6.740888	372.050773	8.943578
6.671711	367.321873	8.948595
6.205816	374.492333	8.953613
6.499088	375.043010	8.958631
6.521859	368.106460	8.963648
6.760944	373.667484	8.968666
6.891485	368.831553	8.973683
6.918099	370.900899	8.978701
6.862787	382.314625	8.983719
7.054809	365.155339	8.988736
6.698083	380.829210	8.993754
6.856553	368.500317	8.998771
6.863020	359.291032	9.003789
6.033998	355.261846	9.008807
6.375626	365.458367	9.013824
6.710285	380.178170	9.018842
6.636358	373.821647	9.023859
6.677589	377.902070	9.028877
6.487954	378.471606	9.033895
6.949644	372.179482	9.038912
6.862650	372.269042	9.043930
6.676448	367.255526	9.048947
6.575266	368.543336	9.053965
6.293615	375.953168	9.058983
6.633411	372.264699	9.064000
6.321932	369.565039	9.069018
6.830719	378.432053	9.074035
6.874886	381.136111	9.079053
6.770381	385.643305	9.084071
7.016924	384.636053	9.089088
7.066204	385.029303	9.094106
6.846161	383.498719	9.099123
6.771669	378.272041	9.104141
6.757758	381.998194	9.109159
6.999420	375.342919	9.114176
6.545271	385.771430	9.119194
6.964720	382.423923	9.124211
7.431559	396.438233	9.129229
7.005048	377.053216	9.134247
6.985741	377.233154	9.139264
6.669574	376.418208	9.144282
6.453362	374.287434	9.149299
6.923520	384.656327	9.154317
6.673386	390.663231	9.159335
6.923884	391.375242	9.164352
6.982831	403.894526	9.169370
6.979279	406.590286	9.174387
7.286941	397.620963	9.179405
6.584068	389.750391	9.184423
7.167486	386.746414	9.189440
7.280500	386.148241	9.194458
6.886360	384.414565	9.199475
6.953087	383.514381	9.204493
6.837008	375.002774	9.209511
7.113575	379.645917	9.214528
7.030495	379.397198	9.219546
6.867885	381.344717	9.224563
7.098933	380.510303	9.229581
6.942583	391.122527	9.234599
7.087965	389.563090	9.239616
7.052615	391.651614	9.244634
7.159104	392.121106	9.249651
7.306106	396.737217	9.254669
6.955666	385.927070	9.259687
6.737863	378.419150	9.264704
6.964671	381.997135	9.269722
7.068756	396.689964	9.274739
7.094504	389.364782	9.279757
6.943096	395.870605	9.284775
7.191416	391.309700	9.289792
7.270767	393.408655	9.294810
7.268396	404.441722	9.299827
7.042359	395.638070	9.304845
7.062328	387.243995	9.309863
7.352797	389.549708	9.314880
7.131908	386.501342	9.319898
7.137434	378.958430	9.324915
6.973230	370.182972	9.329933
7.184048	374.069568	9.334951
7.130289	387.083017	9.339968
7.028180	397.071375	9.344986
7.430202	399.690965	9.350003
7.139809	382.209624	9.355021
7.077267	387.322459	9.360039
7.192161	389.598878	9.365056
7.359312	394.363307	9.370074
7.084296	396.845983	9.375091
7.150912	387.608325	9.380109
7.211948	404.936645	9.385127
7.111891	396.697068	9.390144
7.447898	388.821510	9.395162
7.343810	388.642353	9.400179
7.166822	388.528266	9.405197
6.982829	391.296476	9.410215
7.485388	392.079445	9.415232
7.285668	398.693823	9.420250
6.974371	401.191651	9.425267
7.449989	401.713759	9.430285
7.392955	404.370561	9.435303
7.112254	404.099158	9.440320
7.409795	402.534814	9.445338
7.197160	402.877584	9.450355
7.389003	388.006225	9.455373
7.229536	399.073369	9.460391
7.312591	397.189187	9.465408
7.464602	393.713170	9.470426
7.197998	402.913122	9.475443
7.446788	398.266935	9.480461
7.313450	398.808717	9.485479
7.721322	395.507202	9.490496
7.695677	381.610338	9.495514
7.239390	382.186940	9.500531
7.193308	372.357888	9.505549
7.004219	382.321998	9.510567
7.405832	400.524741	9.515584
7.700097	397.379879	9.520602
7.305084	407.448848	9.525619
7.391357	393.777432	9.530637
7.577006	397.926748	9.535655
7.484426	402.125971	9.540672
7.457232	390.899107	9.545690
7.322384	398.954966	9.550707
7.495714	384.941718	9.555725
7.567534	398.465665	9.560743
7.005172	393.122922	9.565760
7.602870	388.311620	9.570778
7.613297	393.223679	9.575795
7.599837	396.047219	9.580813
7.628226	401.414050	9.585831
7.199831	391.575463	9.590848
7.160033	389.508562	9.595866
7.356985	393.735000	9.600883
7.654322	393.006962	9.605901
7.495154	405.188044	9.610919
7.651036	398.893334	9.615936
7.669707	391.383070	9.620954
7.453723	399.921848	9.625971
7.532357	391.045217	9.630989
7.286535	394.845577	9.636007
7.482917	397.860298	9.641024
7.418200	398.334524	9.646042
7.162861	397.844556	9.651059
7.301092	388.971211	9.656077
7.599474	389.148709	9.661095
7.037050	396.984387	9.666112
7.263614	397.842158	9.671130
7.218150	416.522057	9.676147
7.440472	413.666171	9.681165
7.701306	414.894107	9.686183
7.861002	416.592318	9.691200
7.753302	421.926830	9.696218
7.502376	428.445102	9.701235
7.890943	422.237000	9.706253
7.826613	420.653615	9.711271
7.760623	423.034117	9.716288
7.687666	414.092865	9.721306
7.658934	421.993254	9.726323
7.811893	404.852674	9.731341
7.818255	407.622618	9.736359
7.444543	407.829684	9.741376
7.819420	414.237276	9.746394
7.762006	421.504697	9.751411
7.549628	411.064217	9.756429
7.780742	413.950424	9.761447
7.789588	418.600810	9.766464
7.845365	420.981168	9.771482
7.799626	412.818279	9.776499
7.585453	387.991021	9.781517
7.578109	409.183228	9.786535
7.666496	422.101849	9.791552
8.306061	421.515846	9.796570
7.636614	424.255983	9.801587
7.962768	415.327934	9.806605
7.925533	409.846105	9.811623
7.676302	401.633055	9.816640
8.002702	396.491879	9.821658
7.796802	398.774381	9.826675
7.662287	394.393376	9.831693
7.873776	394.158463	9.836711
8.122952	410.141362	9.841728
7.879384	408.365158	9.846746
7.822568	397.745680	9.851763
7.983375	395.297060	9.856781
7.884469	387.322390	9.861799
7.503154	394.176654	9.866816
7.823076	401.135641	9.871834
8.280085	411.273085	9.876851
7.967722	416.541834	9.881869
7.884539	406.440870	9.886887
7.510063	402.611849	9.891904
7.935404	413.593685	9.896922
7.982372	426.960605	9.901939
7.980648	424.714168	9.906957
8.319638	426.283304	9.911975
7.829082	421.992791	9.916992
7.999931	408.446965	9.922010
7.911179	410.767917	9.927027
7.638159	418.031249	9.932045
8.024960	408.506732	9.937063
7.843944	423.938519	9.942080
8.464040	414.355355	9.947098
7.966536	422.247143	9.952115
7.979015	425.836628	9.957133
8.318379	423.874415	9.962151
8.264346	420.743096	9.967168
8.051411	400.500939	9.972186
7.709806	396.628899	9.977203
7.887077	415.823001	9.982221
8.228112	418.010343	9.987239
7.981526	420.769430	9.992256
8.247008	413.558152	9.997274
8.082559	411.905249	10.002291
8.280279	415.667676	10.007309
8.058324	403.193240	10.012327
7.986952	405.849134	10.017344
8.096227	414.655688	10.022362
7.947990	416.746124	10.027379
8.082724	429.420807	10.032397
8.076099	423.710118	10.037415
8.012009	424.641832	10.042432
7.964113	415.229600	10.047450
8.121598	422.848353	10.052467
8.342748	417.417554	10.057485
8.252157	420.631874	10.062503
8.092885	419.110700	10.067520
8.111692	419.461389	10.072538
8.043531	413.984404	10.077555
8.271985	426.685426	10.082573
8.246968	418.168998	10.087591
7.871771	414.283284	10.092608
8.164982	419.024813	10.097626
8.101151	425.431720	10.102643
7.811458	420.245059	10.107661
8.042659	416.324292	10.112679
7.610178	425.357743	10.117696
7.844349	429.833975	10.122714
8.099800	439.261412	10.127731
8.201663	450.050961	10.132749
8.572892	442.141459	10.137767
8.522020	447.883635	10.142784
8.507170	436.579071	10.147802
8.609134	445.456212	10.152819
8.158555	433.544588	10.157837
8.460296	435.993706	10.162855
8.364634	445.498250	10.167872
8.447893	437.857928	10.172890
8.446202	434.475412	10.177907
8.424587	432.636028	10.182925
8.492168	412.908474	10.187943
8.046926	428.413222	10.192960
8.414497	422.255746	10.197978
8.352010	434.106124	10.202995
8.240842	436.316984	10.208013
8.673516	439.269443	10.213031
8.525482	450.584133	10.218048
8.508965	438.762284	10.223066
8.397758	420.504916	10.228083
8.308654	425.669260	10.233101
8.621133	424.190934	10.238119
8.518762	430.209412	10.243136
8.375888	423.712198	10.248154
8.297856	426.848813	10.253171
8.617007	440.703264	10.258189
8.707542	439.480614	10.263207
8.278178	435.429815	10.268224
8.739896	445.137358	10.273242
8.337508	428.863239	10.278259
8.463164	432.087860	10.283277
8.874785	439.269176	10.288295
8.590535	434.321496	10.293312
8.451904	416.557570	10.298330
8.459079	417.272993	10.303347
8.225397	429.106010	10.308365
8.373990	442.311854	10.313383
8.157693	454.258926	10.318400
8.212505	450.223779	10.323418
8.446441	450.250432	10.328435
8.686921	454.523713	10.333453
8.798284	448.882891	10.338471
8.181091	446.196405	10.343488
8.335956	434.230944	10.348506
8.460204	441.340524	10.353523
8.380621	455.711890	10.358541
8.866762	460.659883	10.363559
8.614947	448.837025	10.368576
8.683307	441.675556	10.373594
8.463164	440.340640	10.378611
8.615218	445.981594	10.383629
8.638157	445.343883	10.388647
8.612596	451.183078	10.393664
8.730793	466.971959	10.398682
8.859675	471.448919	10.403699
8.766208	458.373652	10.408717
8.860320	445.076504	10.413735
8.349915	445.169289	10.418752
8.712308	463.491849	10.423770
9.001605	466.220627	10.428787
8.626537	466.569915	10.433805
9.027067	466.400054	10.438823
8.471708	465.663606	10.443840
8.666149	465.712226	10.448858
8.853800	476.346340	10.453875
8.775738	477.829348	10.458893
9.327306	473.694273	10.463911
9.177972	465.137342	10.468928
9.076216	455.156024	10.473946
8.836824	444.811274	10.478963
8.690649	442.347630	10.483981
8.678924	443.198557	10.488999
8.693910	453.544136	10.494016
8.621229	451.327748	10.499034
9.052950	449.767622	10.504051
8.562716	456.601106	10.509069
8.919796	457.728760	10.514087
8.717808	469.948152	10.519104
8.805364	472.329849	10.524122
9.260749	474.376208	10.529139
9.298538	474.427282	10.534157
9.058920	463.034843	10.539175
8.785273	454.431123	10.544192
8.866859	442.644393	10.549210
9.133025	451.615729	10.554227
8.939069	452.050247	10.559245
9.082082	451.592535	10.564263
9.166353	457.550222	10.569280
8.906373	450.929337	10.574298
9.066287	440.209605	10.579315
9.001706	450.469820	10.584333
8.370146	443.986051	10.589351
8.969397	454.694515	10.594368
8.896417	464.845603	10.599386
9.205204	458.769907	10.604403
9.226846	468.429651	10.609421
9.435757	474.210026	10.614439
9.260759	473.537057	10.619456
9.408769	457.735245	10.624474
8.818763	448.392156	10.629491
8.484754	457.148267	10.634509
8.834864	469.647223	10.639527
8.979574	472.215623	10.644544
9.100658	473.670584	10.649562
9.249113	477.093610	10.654579
9.070074	476.799965	10.659597
8.870495	468.790540	10.664615
9.065129	465.030124	10.669632
9.172508	465.218616	10.674650
9.259327	476.995136	10.679667
8.772909	465.922227	10.684685
8.765667	472.572746	10.689703
8.747097	473.844464	10.694720
8.796812	478.292805	10.699738
9.269011	487.370731	10.704755
9.386643	497.870663	10.709773
9.310048	496.847764	10.714791
9.474645	495.594572	10.719808
9.006054	492.310446	10.724826
9.538206	480.355266	10.729843
9.319125	485.669379	10.734861
9.440683	482.538939	10.739879
9.492265	472.123337	10.744896
8.996442	477.076870	10.749914
9.184713	465.712060	10.754931
8.944262	472.465389	10.759949
8.683221	478.025912	10.764967
9.228271	477.722956	10.769984
9.415654	489.963405	10.775002
9.429530	480.273220	10.780019
9.526608	490.792148	10.785037
9.353734	478.379396	10.790055
9.863100	483.749786	10.795072
9.543290	483.790618	10.800090
9.728444	485.724685	10.805107
9.611920	487.945858	10.810125
9.214046	474.410196	10.815143
9.476098	468.070425	10.820160
9.440682	476.284306	10.825178
9.269034	474.689328	10.830195
9.676161	490.218367	10.835213
9.603139	476.272048	10.840231
9.689492	465.011569	10.845248
9.491092	467.270814	10.850266
9.508216	461.142988	10.855283
9.542780	471.280384	10.860301
9.308894	462.761948	10.865319
9.631724	459.416942	10.870336
9.371706	465.498002	10.875354
9.815131	464.074894	10.880371
9.305641	473.461258	10.885389
9.309342	462.078033	10.890407
9.823191	462.120788	10.895424
9.314021	474.505076	10.900442
9.506823	472.912956	10.905459
9.513280	485.121790	10.910477
9.830244	488.802434	10.915495
9.903873	485.013637	10.920512
9.369338	484.782003	10.925530
9.454238	475.358400	10.930547
9.420046	482.193024	10.935565
9.634417	495.028843	10.940583
9.616087	486.833223	10.945600
9.389340	488.005017	10.950618
9.664849	493.058605	10.955635
9.432174	497.525950	10.960653
9.460842	492.705947	10.965671
10.064316	482.563625	10.970688
9.710713	492.837591	10.975706
10.036996	478.308005	10.980723
9.797728	489.968370	10.985741
9.807628	491.011569	10.990759
10.009784	477.132586	10.995776
9.692056	487.991056	11.000794
9.783657	477.575492	11.005811
9.701494	488.759966	11.010829
9.390720	489.348486	11.015847
9.680946	481.659939	11.020864
9.740021	484.295406	11.025882
10.074376	486.578476	11.030899
9.732372	487.992388	11.035917
9.889966	488.333956	11.040935
10.181832	475.655889	11.045952
9.561239	487.249768	11.050970
10.137906	486.635749	11.055987
9.906732	486.602734	11.061005
10.271052	485.453948	11.066023
10.355220	480.489555	11.071040
9.878009	469.187986	11.076058
9.971210	456.216016	11.081075
10.017808	464.543272	11.086093
9.698312	465.669638	11.091111
9.737630	459.667721	11.096128
9.681596	478.513441	11.101146
10.250100	477.320040	11.106163
9.804718	483.897202	11.111181
9.843057	475.143606	11.116199
9.807907	471.482307	11.121216
10.229378	488.501773	11.126234
10.324709	477.476562	11.131251
10.110548	474.660653	11.136269
10.046831	473.133970	11.141287
10.220578	457.220830	11.146304
9.477477	465.157429	11.151322
10.210695	473.304526	11.156339
9.782857	477.537360	11.161357
9.650694	478.293552	11.166375
10.302276	476.156184	11.171392
9.921271	493.938853	11.176410
10.006977	487.181742	11.181427
9.953896	484.927565	11.186445
10.056613	489.304489	11.191463
10.440834	488.373488	11.196480
9.860615	492.409298	11.201498
9.756390	490.576539	11.206515
10.057265	487.913458	11.211533
10.198402	483.290429	11.216551
10.073784	481.369350	11.221568
9.816339	492.789571	11.226586
10.361291	488.835408	11.231603
10.261692	487.809801	11.236621
9.982273	488.819437	11.241639
10.071250	484.722125	11.246656
9.999601	483.010494	11.251674
10.098533	484.257491	11.256691
10.049749	472.125099	11.261709
9.807512	485.871886	11.266727
10.282562	493.532430	11.271744
10.149694	504.686990	11.276762
10.260502	507.219682	11.281779
10.381151	509.974891	11.286797
10.171919	509.499786	11.291815
10.532004	516.607158	11.296832
10.670466	513.268939	11.301850
10.558356	496.816735	11.306867
10.405966	487.092638	11.311885
10.413356	489.947640	11.316903
10.421099	488.242504	11.321920
10.032841	490.783961	11.326938
10.394636	488.051375	11.331955
10.421031	483.711408	11.336973
10.094408	492.242319	11.341991
10.601742	496.543226	11.347008
10.751654	507.328437	11.352026
10.305178	503.037309	11.357043
10.465785	492.001861	11.362061
9.974588	491.337409	11.367079
10.346137	503.981352	11.372096
10.682401	513.790638	11.377114
10.235136	505.939924	11.382131
10.466808	508.573598	11.387149
10.558659	512.854401	11.392167
10.448988	509.286820	11.397184
10.780070	512.340415	11.402202
10.510066	507.144332	11.407219
10.400459	518.001769	11.412237
10.435462	519.343990	11.417255
10.710923	513.582764	11.422272
10.531366	508.542921	11.427290
10.429431	509.834014	11.432307
10.891002	513.425736	11.437325
10.253095	515.343599	11.442343
10.480455	506.484633	11.447360
10.640397	509.407253	11.452378
10.665305	519.170653	11.457395
10.810713	511.356462	11.462413
10.751280	511.318629	11.467431
11.116007	504.864928	11.472448
10.444787	520.335735	11.477466
10.664059	512.030293	11.482483
10.665221	508.079278	11.487501
10.754074	521.565936	11.492519
10.840823	521.284295	11.497536
10.729194	513.286316	11.502554
10.948432	518.102577	11.507571
11.043786	507.459192	11.512589
10.315648	507.078013	11.517607
10.486269	506.833723	11.522624
10.957704	514.239225	11.527642
10.946088	516.368226	11.532659
10.677771	520.639191	11.537677
10.731767	524.657688	11.542695
10.884084	515.652686	11.547712
10.850116	518.829750	11.552730
10.894073	521.738987	11.557747
11.112013	517.810809	11.562765
11.296932	505.449275	11.567783
10.790688	495.711188	11.572800
10.770148	494.502783	11.577818
10.513645	488.414664	11.582835
11.033745	502.281858	11.587853
10.880947	511.350426	11.592871
10.898264	520.458616	11.597888
11.033897	507.798693	11.602906
11.077197	516.943835	11.607923
10.782438	493.845795	11.612941
10.421423	504.818354	11.617959
10.855442	509.370589	11.622976
11.279909	510.342523	11.627994
11.046396	507.494927	11.633011
11.469706	507.999988	11.638029
10.946326	507.066025	11.643047
10.744409	508.653647	11.648064
10.827669	509.142560	11.653082
10.678866	522.420306	11.658099
10.746588	505.192000	11.663117
10.927941	516.227907	11.668135
10.763271	507.307289	11.673152
10.722265	499.307719	11.678170
10.842443	513.704636	11.683187
11.158895	511.136940	11.688205
11.052058	515.382604	11.693223
10.828263	504.656683	11.698240
11.177930	519.333225	11.703258
11.294158	528.362806	11.708275
11.279033	506.694683	11.713293
11.009036	515.608048	11.718311
10.942001	514.725659	11.723328
11.587133	524.212006	11.728346
10.863575	522.157549	11.733363
11.182253	526.263962	11.738381
11.115878	542.037647	11.743399
11.127041	537.772636	11.748416
11.567258	539.777198	11.753434
11.291895	537.377963	11.758451
11.611596	522.962980	11.763469
11.137571	519.622896	11.768487
11.144857	511.555794	11.773504
11.103282	514.323799	11.778522
10.982277	529.143522	11.783539
11.505731	529.244732	11.788557
11.321013	534.739666	11.793575
11.053365	532.105696	11.798592
11.289721	526.656703	11.803610
11.164970	539.766592	11.808627
11.290203	527.575339	11.813645
11.046524	533.716977	11.818663
11.295560	539.074524	11.823680
11.438552	532.882771	11.828698
11.312246	544.392930	11.833715
11.782312	538.916782	11.838733
11.468141	539.660469	11.843751
11.424127	543.454487	11.848768
11.575704	532.720228	11.853786
11.309091	534.437908	11.858803
11.347765	536.571655	11.863821
11.552693	528.277921	11.868839
11.503380	537.746850	11.873856
11.847587	531.889641	11.878874
11.566605	537.304985	11.883891
11.667934	534.187173	11.888909
11.715593	527.552771	11.893927
11.694248	537.585358	11.898944
11.852408	533.158462	11.903962
11.543777	536.946603	11.908979
11.515513	538.346075	11.913997
11.524921	539.304148	11.919015
11.508696	539.310037	11.924032
11.507018	533.977231	11.929050
11.160319	539.213526	11.934067
11.476422	540.767324	11.939085
11.490804	538.840238	11.944103
11.677526	529.507950	11.949120
11.697622	537.337625	11.954138
11.380951	539.015812	11.959155
11.385856	538.065346	11.964173
11.576292	531.790421	11.969191
11.439024	537.404153	11.974208
12.047456	549.029567	11.979226
11.623465	552.835786	11.984243
11.878744	543.568487	11.989261
11.893277	542.622824	11.994279
11.747993	535.378028	11.999296
11.554773	525.133293	12.004314
11.536814	551.720549	12.009331
11.903161	544.597556	12.014349
12.145179	556.930475	12.019367
12.034800	560.555016	12.024384
11.988813	552.458373	12.029402
11.705544	543.616279	12.034419
11.655787	537.066564	12.039437
11.993941	547.380497	12.044455
12.016622	555.178217	12.049472
11.708259	538.740944	12.054490
12.033036	553.336208	12.059507
12.103896	547.812154	12.064525
12.409480	537.448233	12.069543
11.860351	549.273950	12.074560
11.818532	532.842257	12.079578
11.712492	538.488965	12.084595
11.754864	533.228152	12.089613
11.963509	541.040910	12.094631
11.987253	557.627302	12.099648
12.610600	552.906611	12.104666
11.936937	544.576960	12.109683
11.782032	537.526172	12.114701
12.107194	539.583474	12.119719
12.149776	546.314576	12.124736
12.023217	543.563825	12.129754
11.640052	549.610559	12.134771
12.172030	553.210192	12.139789
12.141741	557.589037	12.144807
11.805756	561.725449	12.149824
11.931380	552.604692	12.154842
12.128423	562.865004	12.159859
12.154448	569.967935	12.164877
12.368831	560.956342	12.169895
12.385147	569.285236	12.174912
12.442758	561.794046	12.179930
12.186205	561.793409	12.184947
12.543458	577.140991	12.189965
12.524257	561.270613	12.194983
12.094587	552.678669	12.200000
12.131346	547.942590	12.205018
11.985440	547.290306	12.210035
12.283166	552.857977	12.215053
12.240887	557.033575	12.220071
12.357048	573.902146	12.225088
12.407207	565.692603	12.230106
12.433501	569.901642	12.235123
12.431365	563.773642	12.240141
12.798870	564.609338	12.245159
12.119151	550.199446	12.250176
12.266733	541.248821	12.255194
12.122738	546.620615	12.260211
12.266246	558.445111	12.265229
12.487488	557.971984	12.270247
12.047460	558.968919	12.275264
12.447427	557.584171	12.280282
12.230206	559.814819	12.285299
12.321161	565.673665	12.290317
12.315797	559.580886	12.295335
12.317897	566.166860	12.300352
12.204865	553.697343	12.305370
12.749484	557.055157	12.310387
12.305631	563.988711	12.315405
12.517346	560.528554	12.320423
12.612000	562.842880	12.325440
12.265600	565.551356	12.330458
12.326664	564.636271	12.335475
12.061252	559.884418	12.340493
12.517341	571.022479	12.345511
12.377304	588.593919	12.350528
12.626915	584.458793	12.355546
12.827921	591.288165	12.360563
12.701873	593.933719	12.365581
12.825324	587.877551	12.370599
12.587033	597.792685	12.375616
12.743524	580.869132	12.380634
12.698101	590.476334	12.385651
12.510430	581.972690	12.390669
13.052387	581.241031	12.395687
12.270101	591.983004	12.400704
12.683917	580.235647	12.405722
12.851946	589.244519	12.410739
12.489958	588.244239	12.415757
12.855246	580.247245	12.420775
12.808827	593.130308	12.425792
12.547135	583.290741	12.430810
13.062839	582.632623	12.435827
12.813632	582.491980	12.440845
12.963897	586.795207	12.445863
13.000431	593.852319	12.450880
13.030251	588.012792	12.455898
12.869669	585.895366	12.460915
12.983675	584.817352	12.465933
12.824457	569.057267	12.470951
12.766577	571.692136	12.475968
12.593300	590.256545	12.480986
12.878551	574.549891	12.486003
12.880319	586.936253	12.491021
13.418778	583.999249	12.496039
13.180996	589.470956	12.501056
13.129072	570.348928	12.506074
12.865511	569.595157	12.511091
12.783899	569.617603	12.516109
12.929516	574.013072	12.521127
12.641691	583.481527	12.526144
12.814820	586.998537	12.531162
13.129805	591.007714	12.536179
12.890232	589.789440	12.541197
13.156736	584.184227	12.546215
12.988683	586.735376	12.551232
13.090383	583.305075	12.556250
13.495065	590.042574	12.561267
13.057640	592.891548	12.566285
13.015825	582.443178	12.571303
12.970039	590.851240	12.576320
13.339000	574.437197	12.581338
12.945622	576.935287	12.586355
13.220165	580.505833	12.591373
13.142709	583.771773	12.596391
12.984903	585.945778	12.601408
13.223943	586.473401	12.606426
12.801143	588.322855	12.611443
12.498601	592.769612	12.616461
13.232182	601.711970	12.621479
13.107059	610.425960	12.626496
13.245713	606.065218	12.631514
13.586628	614.286471	12.636531
13.416711	610.078217	12.641549
13.657680	611.457601	12.646567
13.189768	610.221453	12.651584
13.569420	600.675864	12.656602
13.265468	594.244850	12.661619
13.382661	589.575052	12.666637
13.319836	578.987966	12.671655
13.433280	608.353898	12.676672
13.160695	611.524184	12.681690
13.861591	614.573502	12.686707
13.155123	605.289603	12.691725
13.768126	615.484772	12.696743
13.621281	608.363267	12.701760
13.462082	588.282889	12.706778
13.457725	584.455797	12.711795
13.285526	592.303001	12.716813
13.445296	593.647770	12.721831
13.032145	602.520493	12.726848
13.736980	610.533246	12.731866
14.029933	608.530949	12.736883
13.406501	611.869814	12.741901
13.689358	609.941681	12.746919
13.669858	598.735572	12.751936
13.828421	600.995709	12.756954
13.213248	590.173268	12.761971
13.419122	605.030200	12.766989
13.805229	602.479980	12.772007
13.707933	610.754111	12.777024
13.740330	603.399397	12.782042
13.819312	604.744201	12.787059
13.312744	605.486477	12.792077
13.376132	612.337420	12.797095
13.320404	604.889216	12.802112
13.542807	611.942460	12.807130
13.383768	610.162458	12.812147
13.120485	606.499006	12.817165
13.644832	617.235084	12.822183
13.972551	620.604804	12.827200
13.961988	622.768366	12.832218
14.170323	613.016084	12.837235
14.170316	607.979638	12.842253
14.065367	608.018363	12.847271
13.706563	620.549605	12.852288
13.638811	613.822802	12.857306
13.950800	599.857087	12.862323
13.949408	603.795918	12.867341
14.131624	601.981384	12.872359
13.969418	601.827110	12.877376
14.063395	610.203815	12.882394
13.822151	603.336942	12.887411
13.344581	615.208294	12.892429
13.738465	602.668786	12.897447
14.174114	610.821545	12.902464
14.016248	624.457391	12.907482
14.227538	620.350351	12.912499
13.989555	611.027760	12.917517
13.798221	611.559700	12.922535
14.346906	615.140948	12.927552
13.930783	611.763373	12.932570
14.141615	602.581902	12.937587
14.348775	613.156238	12.942605
14.179225	605.217785	12.947623
14.031967	603.843035	12.952640
13.875540	604.328481	12.957658
14.443704	602.980492	12.962675
14.294626	606.314462	12.967693
14.386518	605.381921	12.972711
14.401148	595.682088	12.977728
13.760645	594.425646	12.982746
14.254432	593.521655	12.987763
14.087696	605.849225	12.992781
14.040708	606.816137	12.997799
14.705884	612.187400	13.002816
14.448061	608.728218	13.007834
14.303622	600.003198	13.012851
14.314647	599.225338	13.017869
14.658340	606.603557	13.022887
14.370635	587.363820	13.027904
14.284970	595.916987	13.032922
14.477088	602.334347	13.037939
14.252191	609.855303	13.042957
13.751216	608.397119	13.047975
14.397163	619.694811	13.052992
14.549231	625.102291	13.058010
15.013297	626.077495	13.063027
14.251883	618.171810	13.068045
14.224249	603.116910	13.073063
14.305975	615.238301	13.078080
14.624662	621.692642	13.083098
14.724443	609.688356	13.088115
14.422830	612.913683	13.093133
14.549022	623.633254	13.098151
14.744528	624.988205	13.103168
14.488504	617.505107	13.108186
14.378794	601.383788	13.113203
14.948475	617.550185	13.118221
14.426946	615.678656	13.123239
14.750499	610.689343	13.128256
14.775402	612.758986	13.133274
14.765711	598.840517	13.138291
14.756160	611.607364	13.143309
14.760538	601.653516	13.148327
14.647272	606.342018	13.153344
14.491243	596.612120	13.158362
14.602830	610.862140	13.163379
14.409371	609.863855	13.168397
14.784773	634.505598	13.173415
15.114578	624.074717	13.178432
14.652462	627.075887	13.183450
15.068100	602.919662	13.188467
14.820702	615.206229	13.193485
14.307961	606.460017	13.198503
14.776044	609.242856	13.203520
14.921615	626.147894	13.208538
15.298378	622.172717	13.213555
14.935078	613.731289	13.218573
14.574162	620.639248	13.223591
15.356466	613.258551	13.228608
14.767691	616.402640	13.233626
14.726715	610.908712	13.238643
14.703009	620.525150	13.243661
14.855759	624.143191	13.248679
14.976378	623.537506	13.253696
15.158837	632.367415	13.258714
15.176350	626.103772	13.263731
15.385789	629.984329	13.268749
14.969706	616.249441	13.273767
15.021269	611.653036	13.278784
14.717647	623.389843	13.283802
14.915240	614.579669	13.288819
14.836679	620.266278	13.293837
14.802413	625.535696	13.298855
15.260166	631.646361	13.303872
14.812538	630.924583	13.308890
15.000377	628.137182	13.313907
14.864494	636.114415	13.318925
14.696081	629.109888	13.323943
14.997849	626.386687	13.328960
14.878704	635.983374	13.333978
15.147047	645.967477	13.338995
15.302732	660.835475	13.344013
14.873836	652.824027	13.349031
15.367917	656.473800	13.354048
15.224692	647.032202	13.359066
15.582825	650.785325	13.364083
15.692614	656.432967	13.369101
15.377107	653.629753	13.374119
15.750737	643.296135	13.379136
14.996122	635.058020	13.384154
15.434759	641.733414	13.389171
15.171974	646.700973	13.394189
15.224800	645.998613	13.399207
15.680703	648.319465	13.404224
15.380583	661.826149	13.409242
15.393393	645.922278	13.414259
15.300013	652.141393	13.419277
15.414216	655.595066	13.424295
15.532461	640.690846	13.429312
15.400405	651.498233	13.434330
15.348903	655.287137	13.439347
15.439871	651.921620	13.444365
15.421656	659.331319	13.449383
15.493596	646.510864	13.454400
15.387664	653.864876	13.459418
15.266798	654.493073	13.464435
15.626513	653.796277	13.469453
15.552821	664.727071	13.474471
15.541778	648.161062	13.479488
15.124405	659.906248	13.484506
15.461109	654.084888	13.489523
15.957674	655.550461	13.494541
15.602514	657.149484	13.499559
15.636449	645.221763	13.504576
15.605492	666.130798	13.509594
15.700312	660.839639	13.514611
16.198673	670.913948	13.519629
15.643628	671.865793	13.524647
15.694461	655.034464	13.529664
15.906721	663.758734	13.534682
15.864884	657.204578	13.539699
15.769002	652.804833	13.544717
15.562717	668.897196	13.549735
15.942199	676.822102	13.554752
15.517574	679.741667	13.559770
15.792817	663.298045	13.564787
15.970155	661.184469	13.569805
15.578410	672.606912	13.574823
15.973327	672.346412	13.579840
15.478043	669.558739	13.584858
15.777580	674.081596	13.589875
15.933934	665.997379	13.594893
15.800933	676.981654	13.599911
15.958824	664.753633	13.604928
16.058626	664.479412	13.609946
16.050556	676.425565	13.614963
16.379227	672.760870	13.619981
16.334353	668.643463	13.624999
16.417392	664.442899	13.630016
16.226329	666.783070	13.635034
16.069363	666.201942	13.640051
16.488680	653.525870	13.645069
15.982547	669.008808	13.650087
16.188264	662.355903	13.655104
16.266821	661.984025	13.660122
15.924210	659.885643	13.665139
16.313425	656.050519	13.670157
16.128579	664.360483	13.675175
16.176920	664.283672	13.680192
16.521630	667.492949	13.685210
16.247216	669.603183	13.690227
16.377964	663.081945	13.695245
16.173960	667.118807	13.700263
16.373993	664.130674	13.705280
16.538341	665.313785	13.710298
16.206220	671.980567	13.715315
16.059970	670.299541	13.720333
16.432559	671.680399	13.725351
16.516781	670.465035	13.730368
16.244119	666.077206	13.735386
16.298221	666.034207	13.740403
16.430159	660.128163	13.745421
16.606654	665.266741	13.750439
15.958641	667.246163	13.755456
16.526589	672.547472	13.760474
16.179826	687.525774	13.765491
16.632463	683.541852	13.770509
16.465712	688.835203	13.775527
16.842443	686.428451	13.780544
16.712012	690.987121	13.785562
16.577196	695.543324	13.790579
16.928685	685.408811	13.795597
16.885452	689.780250	13.800615
16.558416	665.730836	13.805632
16.802212	659.539024	13.810650
16.414920	663.976987	13.815667
16.491776	658.231053	13.820685
16.586659	676.570500	13.825703
16.778968	684.537359	13.830720
16.843035	687.891596	13.835738
16.562916	691.997194	13.840755
16.728611	681.068129	13.845773
16.548619	688.872416	13.850791
16.831264	687.591248	13.855808
16.802012	686.043368	13.860826
16.798481	690.408586	13.865843
16.741934	687.378600	13.870861
16.876372	695.733227	13.875879
16.688811	688.072114	13.880896
16.923252	690.102623	13.885914
16.649906	696.069084	13.890931
17.041577	686.897106	13.895949
17.214223	682.398477	13.900967
17.375704	686.321274	13.905984
17.231233	677.012398	13.911002
16.839457	685.922838	13.916019
17.196801	687.407072	13.921037
17.227517	688.125129	13.926055
17.159400	685.762829	13.931072
16.854952	685.236366	13.936090
17.056104	680.010592	13.941107
16.966365	686.222837	13.946125
17.054782	691.599284	13.951143
17.238580	685.770314	13.956160
17.181665	691.608189	13.961178
16.890290	697.893055	13.966195
17.412195	680.789077	13.971213
17.183031	682.712343	13.976231
17.047533	687.347545	13.981248
17.277349	686.857293	13.986266
17.120767	688.289505	13.991283
17.312773	689.373611	13.996301
16.921797	683.413791	14.001319
17.123285	684.578461	14.006336
17.155250	686.650162	14.011354
16.955046	702.561721	14.016371
17.460179	708.302072	14.021389
17.633544	716.918854	14.026407
17.741565	710.054020	14.031424
17.764881	690.686544	14.036442
17.171274	695.989973	14.041459
17.084506	683.633014	14.046477
17.455490	710.058581	14.051495
17.782445	711.755861	14.056512
17.802521	695.017675	14.061530
17.183356	700.287240	14.066547
17.523065	686.964054	14.071565
17.337862	689.779836	14.076583
17.392505	714.336246	14.081600
17.640185	712.148527	14.086618
17.442481	723.916141	14.091635
17.717399	714.977037	14.096653
17.472689	727.231701	14.101671
17.272250	717.076349	14.106688
18.174612	713.148189	14.111706
17.889294	717.374528	14.116723
17.767819	710.441510	14.121741
17.594162	715.631809	14.126759
17.610755	721.054233	14.131776
18.033193	716.052554	14.136794
17.567053	712.749067	14.141811
18.057183	718.965143	14.146829
17.993657	711.486558	14.151847
17.840921	719.778894	14.156864
17.846004	715.902957	14.161882
17.871461	717.079431	14.166899
18.002414	706.512401	14.171917
17.804181	706.067125	14.176935
17.612827	713.267288	14.181952
17.655746	707.125868	14.186970
17.882345	710.075947	14.191987
18.006278	708.412546	14.197005
17.782753	706.973998	14.202023
17.745236	706.333127	14.207040
18.001968	714.933690	14.212058
18.016120	723.095737	14.217075
18.024661	711.878851	14.222093
18.031032	715.914321	14.227111
17.875253	709.747228	14.232128
18.028939	713.636538	14.237146
17.738617	705.612822	14.242163
18.096210	707.030746	14.247181
17.888225	717.957368	14.252199
18.037370	705.673884	14.257216
18.141409	718.757525	14.262234
18.305256	729.291379	14.267251
18.311854	716.395905	14.272269
18.130053	723.320020	14.277287
18.030196	730.935044	14.282304
18.419823	728.636720	14.287322
18.457021	734.368344	14.292339
18.420937	729.148168	14.297357
18.564560	724.272223	14.302375
18.254536	726.331239	14.307392
18.459196	714.307295	14.312410
18.286042	718.705408	14.317427
18.301671	717.494476	14.322445
18.515200	728.396087	14.327463
18.182143	732.648843	14.332480
18.343584	732.371275	14.337498
18.368218	733.481607	14.342515
18.292383	728.791524	14.347533
18.305903	726.662582	14.352551
18.453689	728.012394	14.357568
18.456683	724.035798	14.362586
18.553870	728.353687	14.367603
18.641302	724.572143	14.372621
18.765333	734.055043	14.377639
18.571508	737.847328	14.382656
18.559932	732.620155	14.387674
18.369745	735.771241	14.392691
18.600726	736.593623	14.397709
18.657104	734.568418	14.402727
18.562171	738.755464	14.407744
18.793812	741.682668	14.412762
18.637999	734.512024	14.417779
18.849000	726.072079	14.422797
18.930187	726.005901	14.427815
18.643581	734.518034	14.432832
18.958173	722.208617	14.437850
18.780185	735.418510	14.442867
18.726425	727.240954	14.447885
18.592857	739.998921	14.452903
18.641901	751.999293	14.457920
18.839868	761.495869	14.462938
18.986867	756.717216	14.467955
19.138759	758.416683	14.472973
19.218171	746.705832	14.477991
18.964949	750.942929	14.483008
19.504401	741.129230	14.488026
19.023876	736.199594	14.493043
18.760111	728.563027	14.498061
18.769154	730.679349	14.503079
19.179287	729.747433	14.508096
19.158095	747.177331	14.513114
18.769653	739.140571	14.518131
19.087812	748.589906	14.523149
19.465326	748.051265	14.528167
19.132585	752.739479	14.533184
19.552584	739.567777	14.538202
19.506557	733.901032	14.543219
19.351771	723.176789	14.548237
19.198411	720.515416	14.553255
19.118776	729.203402	14.558272
19.101918	715.494249	14.563290
19.455138	731.227606	14.568307
19.450262	738.281796	14.573325
19.090015	733.134500	14.578343
19.315129	731.139662	14.583360
19.403597	736.629725	14.588378
19.536311	743.728632	14.593395
19.130119	741.226790	14.598413
19.548859	737.636332	14.603431
19.455341	748.194742	14.608448
19.704018	741.020680	14.613466
19.941187	733.109964	14.618483
19.499741	719.360035	14.623501
19.539160	719.578112	14.628519
19.524035	722.092696	14.633536
19.506029	710.677999	14.638554
19.335905	720.784492	14.643571
19.667558	730.001329	14.648589
19.740255	739.211407	14.653607
19.525012	740.681217	14.658624
19.930602	741.561447	14.663642
19.438285	723.830540	14.668659
19.789326	741.568185	14.673677
19.876846	744.675762	14.678695
19.959198	743.135637	14.683712
19.914851	734.966070	14.688730
19.580944	736.848948	14.693747
19.169614	731.782239	14.698765
19.516601	732.586445	14.703783
19.565044	743.649630	14.708800
19.692862	735.500425	14.713818
19.475157	745.746931	14.718835
19.575054	749.994973	14.723853
19.490669	735.438004	14.728871
19.421185	747.365425	14.733888
19.700483	764.344316	14.738906
20.116939	767.463474	14.743923
20.072122	768.578378	14.748941
20.379411	759.965540	14.753959
20.142093	773.910595	14.758976
20.150862	771.438408	14.763994
20.014369	763.078138	14.769011
20.048127	761.779155	14.774029
20.439018	758.458145	14.779047
20.260494	764.390837	14.784064
20.396613	750.342107	14.789082
20.322022	742.521259	14.794099
20.103171	740.289867	14.799117
20.342540	733.757896	14.804135
20.318204	735.431324	14.809152
20.589505	735.445812	14.814170
20.304749	733.619223	14.819187
19.724211	739.734815	14.824205
20.485190	734.165691	14.829223
19.918563	740.067664	14.834240
20.417387	743.887127	14.839258
20.213838	739.731448	14.844275
20.287353	752.655795	14.849293
20.758088	759.793266	14.854311
20.412079	746.924614	14.859328
20.571444	735.179153	14.864346
20.456301	741.903482	14.869363
20.286036	730.247541	14.874381
20.412281	743.008984	14.879399
20.715460	750.535622	14.884416
20.893498	755.162743	14.889434
20.792719	734.656479	14.894451
20.323135	738.870668	14.899469
20.351226	737.989143	14.904487
20.062255	744.166351	14.909504
20.268002	754.154011	14.914522
20.407935	760.727929	14.919539
20.319149	764.175558	14.924557
20.863551	756.882571	14.929575
20.776596	759.878631	14.934592
20.632190	761.993753	14.939610
20.632236	751.071664	14.944627
20.594879	748.824458	14.949645
20.750137	750.857913	14.954663
20.647247	764.535745	14.959680
20.675471	754.186754	14.964698
21.019175	758.137821	14.969715
20.687349	768.481116	14.974733
20.962255	772.629159	14.979751
20.539432	775.135045	14.984768
21.284027	782.223305	14.989786
21.273196	791.342355	14.994803
21.270474	780.392280	14.999821
20.897027	754.128323	15.004839
20.787155	757.370970	15.009856
21.095590	767.869569	15.014874
21.377417	776.797591	15.019891
21.060414	778.680980	15.024909
21.402477	761.090705	15.029927
21.112472	760.129630	15.034944
20.698649	757.259751	15.039962
21.015444	775.649738	15.044979
20.899472	790.238514	15.049997
21.512135	781.899714	15.055015
21.237533	781.163442	15.060032
21.512870	791.301166	15.065050
21.623076	791.198883	15.070067
21.207610	788.401841	15.075085
21.593163	779.284424	15.080103
21.491290	762.035104	15.085120
21.299147	758.392032	15.090138
21.245916	753.651063	15.095155
21.261855	764.233359	15.100173
21.477210	778.978497	15.105191
21.578869	777.350138	15.110208
21.401550	784.936296	15.115226
21.655960	779.143569	15.120243
21.624324	780.221695	15.125261
21.675629	766.940481	15.130279
21.385638	761.883154	15.135296
21.385031	763.183637	15.140314
21.510996	778.646527	15.145331
21.305256	787.430039	15.150349
21.239385	785.711162	15.155367
21.591421	786.483020	15.160384
21.241948	784.606606	15.165402
21.475522	789.452253	15.170419
21.341605	785.140486	15.175437
21.080094	786.046345	15.180455
21.883431	783.304495	15.185472
22.039005	805.468886	15.190490
22.089204	780.703801	15.195507
21.769724	789.038073	15.200525
21.645695	773.938171	15.205543
21.917998	777.089385	15.210560
21.686168	790.541285	15.215578
22.164455	791.997111	15.220595
21.903852	797.289419	15.225613
22.004500	792.761016	15.230631
22.177154	790.610289	15.235648
21.805983	792.533725	15.240666
22.412490	792.659796	15.245683
22.073267	786.332069	15.250701
21.909401	776.215134	15.255719
22.142429	776.589071	15.260736
21.927147	778.560664	15.265754
22.256232	794.632375	15.270771
22.192202	789.659558	15.275789
22.362872	790.191589	15.280807
21.555933	786.177776	15.285824
21.849385	791.758816	15.290842
22.002565	791.959070	15.295859
22.047392	802.764081	15.300877
22.337859	808.752694	15.305895
22.158603	803.091023	15.310912
22.050683	815.270666	15.315930
22.408121	798.608914	15.320947
21.858617	809.418685	15.325965
22.136549	804.521674	15.330983
22.471698	802.260279	15.336000
22.395150	806.270890	15.341018
22.578447	811.297991	15.346035
22.501383	805.210051	15.351053
22.200630	801.984776	15.356071
22.808109	814.295328	15.361088
22.650335	820.243722	15.366106
22.632937	802.690792	15.371123
22.495361	808.478226	15.376141
22.570362	807.516763	15.381159
22.739849	814.483705	15.386176
22.589403	806.415936	15.391194
22.790604	812.661536	15.396211
22.958706	821.326529	15.401229
22.536438	806.235459	15.406247
22.778037	806.589118	15.411264
22.657982	815.217206	15.416282
23.034433	814.890170	15.421299
23.036502	810.837959	15.426317
22.711553	805.066569	15.431335
22.790556	797.600331	15.436352
22.592869	800.976666	15.441370
22.869408	811.496068	15.446387
22.855087	820.533628	15.451405
23.050291	818.013289	15.456423
23.633120	806.220368	15.461440
22.975408	806.579231	15.466458
22.784089	802.355349	15.471475
22.781729	802.024548	15.476493
22.945061	812.738414	15.481511
22.983020	809.886105	15.486528
22.750821	817.225254	15.491546
23.069224	811.646554	15.496563
23.215272	814.767063	15.501581
23.082695	814.194731	15.506599
23.469571	815.920503	15.511616
23.174380	807.774426	15.516634
23.378022	800.149802	15.521651
23.258720	814.546615	15.526669
23.235584	817.456945	15.531687
23.445090	812.229824	15.536704
23.482003	816.178479	15.541722
23.671644	813.655856	15.546739
23.501645	813.019960	15.551757
23.312758	805.857624	15.556775
23.474519	808.372908	15.561792
23.328671	809.942304	15.566810
23.545252	810.470298	15.571827
23.312376	818.090421	15.576845
23.085447	810.179802	15.581863
23.429017	805.846867	15.586880
23.206620	813.913474	15.591898
23.276080	806.057405	15.596915
23.028756	803.836777	15.601933
23.172274	815.443691	15.606951
23.860249	828.779908	15.611968
23.574846	829.522253	15.616986
23.897004	831.204518	15.622003
23.552868	824.637704	15.627021
23.595896	832.836303	15.632039
23.480965	826.504978	15.637056
23.685187	831.632948	15.642074
23.743401	833.214555	15.647091
23.997351	825.992295	15.652109
23.925614	839.214020	15.657127
24.071161	825.574011	15.662144
23.915827	826.425367	15.667162
23.648769	830.500547	15.672179
23.871394	829.853627	15.677197
23.483647	836.245160	15.682215
24.045862	823.306736	15.687232
24.021874	825.781697	15.692250
24.253001	839.378850	15.697267
23.890308	826.052003	15.702285
24.165497	834.138488	15.707303
24.236801	827.304609	15.712320
23.995052	825.275611	15.717338
23.778959	819.660732	15.722355
24.284469	820.613675	15.727373
23.727630	833.671558	15.732391
24.549977	846.008427	15.737408
24.645004	842.664329	15.742426
24.600731	832.418171	15.747443
24.439189	828.776601	15.752461
24.387452	826.825130	15.757479
24.347540	816.417351	15.762496
24.019930	820.028642	15.767514
23.939818	810.621249	15.772531
24.331431	836.475724	15.777549
24.359824	833.280925	15.782567
24.810219	829.751761	15.787584
24.770642	846.067475	15.792602
24.669660	836.877934	15.797619
24.606744	820.256776	15.802637
24.544818	815.567646	15.807655
24.680109	813.880365	15.812672
24.528522	817.511414	15.817690
24.748233	814.135163	15.822707
24.510875	817.233693	15.827725
24.360144	833.061878	15.832743
24.641203	833.690224	15.837760
24.800949	842.804665	15.842778
24.687785	847.278618	15.847795
24.917634	846.741020	15.852813
25.157870	849.613246	15.857831
25.068222	843.224304	15.862848
24.848661	831.061620	15.867866
25.013340	820.037955	15.872883
24.929927	821.509206	15.877901
24.818415	831.240503	15.882919
24.939207	824.307352	15.887936
24.786297	837.431339	15.892954
25.470445	842.597728	15.897971
25.271968	822.292864	15.902989
24.784993	820.390652	15.908007
24.893351	821.847636	15.913024
25.344935	826.643357	15.918042
25.130501	826.910677	15.923059
24.980326	825.577392	15.928077
25.014527	839.871279	15.933095
25.194036	838.568390	15.938112
25.308619	846.623239	15.943130
25.336547	845.214710	15.948147
25.521147	841.433697	15.953165
25.108880	839.930035	15.958183
25.470413	844.193911	15.963200
25.114465	846.692484	15.968218
25.003436	847.966092	15.973235
25.345418	836.542249	15.978253
25.247639	842.134109	15.983271
25.113192	834.597156	15.988288
25.027400	843.611212	15.993306
25.330311	844.838898	15.998323
25.234498	842.218984	16.003341
24.945215	849.645986	16.008359
25.427553	851.789153	16.013376
25.255972	862.233628	16.018394
25.368144	863.125124	16.023411
25.601159	862.463952	16.028429
25.686260	874.051654	16.033447
26.106016	863.745397	16.038464
25.712583	864.593033	16.043482
25.735589	860.401830	16.048499
26.069004	860.977792	16.053517
25.731849	868.478575	16.058535
25.799403	854.806582	16.063552
25.692353	860.106409	16.068570
25.956607	858.818643	16.073587
26.089696	856.188108	16.078605
25.920677	868.140673	16.083623
25.877143	863.691648	16.088640
25.784610	861.787591	16.093658
25.997848	860.444702	16.098675
26.066040	859.193966	16.103693
25.799317	862.379157	16.108711
25.923496	857.020223	16.113728
26.107561	857.521755	16.118746
26.142550	852.691198	16.123763
26.216874	856.084886	16.128781
26.178166	858.035134	16.133799
26.249918	852.018536	16.138816
26.339872	865.672542	16.143834
26.256156	866.679937	16.148851
26.353721	856.764995	16.153869
25.973963	856.799439	16.158887
26.328458	864.870357	16.163904
26.685001	875.481404	16.168922
26.419374	874.115711	16.173939
26.704107	862.265316	16.178957
26.405727	862.842438	16.183975
26.535381	858.091722	16.188992
26.562239	859.892841	16.194010
26.238976	851.167313	16.199027
26.714668	845.847983	16.204045
26.575014	851.077175	16.209063
26.500782	852.594328	16.214080
26.693994	856.632113	16.219098
26.488519	872.153327	16.224115
27.085439	874.786634	16.229133
26.727914	863.955215	16.234151
27.017318	855.603911	16.239168
26.886145	850.505897	16.244186
26.540684	860.491616	16.249203
26.734823	850.905532	16.254221
26.972861	866.098473	16.259239
26.880051	856.184956	16.264256
26.816498	861.168696	16.269274
26.481095	862.382784	16.274291
26.989440	862.814573	16.279309
26.845802	868.735522	16.284327
26.876508	868.405851	16.289344
27.416506	874.020872	16.294362
27.262696	877.813229	16.299379
27.492184	873.722216	16.304397
27.267359	862.450280	16.309415
27.059229	849.676716	16.314432
27.203409	848.836957	16.319450
27.325480	839.776571	16.324467
27.338081	846.550353	16.329485
27.104654	846.060094	16.334503
26.977850	838.859615	16.339520
27.150229	858.026558	16.344538
27.030876	861.819825	16.349555
27.412032	867.081031	16.354573
27.140914	879.907987	16.359591
27.559834	880.912371	16.364608
27.590425	874.390968	16.369626
27.310607	882.359305	16.374643
27.363424	869.481724	16.379661
27.143302	877.055693	16.384679
27.121360	874.152798	16.389696
27.550032	874.272019	16.394714
27.208248	880.754198	16.399731
27.346064	873.379700	16.404749
27.316314	886.093103	16.409767
27.289699	888.256056	16.414784
27.328463	894.710174	16.419802
27.190157	903.022425	16.424819
27.251336	896.108054	16.429837
27.345921	900.713574	16.434855
27.723286	910.134784	16.439872
28.302414	906.411865	16.444890
28.061413	902.877404	16.449907
27.855363	889.153578	16.454925
27.832047	888.355840	16.459943
27.629679	888.457166	16.464960
27.922351	899.469559	16.469978
28.269059	900.863959	16.474995
28.690516	894.871450	16.480013
28.716042	879.647039	16.485031
28.701684	879.554805	16.490048
28.922137	864.643852	16.495066
28.629939	876.606254	16.500083
28.547889	853.733198	16.505101
28.503507	850.338357	16.510119
28.201839	843.360935	16.515136
28.426382	843.597346	16.520154
28.252833	851.552175	16.525171
28.115578	838.496112	16.530189
28.033704	843.738340	16.535207
28.101701	848.657284	16.540224
28.068224	841.644155	16.545242
28.244432	846.946934	16.550259
28.749811	854.606039	16.555277
28.487107	853.811096	16.560295
28.350886	861.160471	16.565312
28.463395	860.953685	16.570330
28.604179	873.327932	16.575347
28.550690	867.384601	16.580365
28.636908	870.533429	16.585383
28.256408	866.481185	16.590400
28.644459	871.012315	16.595418
28.329574	869.278796	16.600435
28.606189	874.739422	16.605453
28.811293	877.257393	16.610471
28.934563	879.286407	16.615488
28.762863	870.057436	16.620506
28.822276	867.744559	16.625523
28.835497	865.145428	16.630541
28.670239	868.930110	16.635559
28.391109	865.458436	16.640576
28.929134	864.755786	16.645594
28.711202	877.148370	16.650611
28.897675	878.403770	16.655629
29.055698	885.621846	16.660647
29.240367	896.906782	16.665664
29.404065	896.199664	16.670682
28.975535	889.535594	16.675699
29.169116	869.298638	16.680717
29.536613	878.557275	16.685735
28.799287	876.732151	16.690752
29.385436	887.651217	16.695770
28.984458	899.081563	16.700787
29.570755	890.658479	16.705805
29.645478	889.618160	16.710823
29.269797	895.184150	16.715840
29.426445	885.891102	16.720858
28.944888	886.616846	16.725875
29.142342	895.444537	16.730893
29.356732	893.517634	16.735911
29.583764	899.266907	16.740928
29.472730	898.404015	16.745946
29.013461	912.125174	16.750963
29.239470	909.647333	16.755981
29.355224	901.452605	16.760999
29.386155	900.886210	16.766016
29.397202	915.048084	16.771034
29.630712	921.967167	16.776051
29.275388	922.348082	16.781069
29.531288	930.929945	16.786087
29.528761	923.227116	16.791104
29.882791	924.320565	16.796122
29.846377	921.896462	16.801139
29.792527	922.668804	16.806157
29.880661	914.923372	16.811175
29.974280	915.044596	16.816192
30.073333	915.426903	16.821210
29.969596	924.582669	16.826227
29.717955	920.705885	16.831245
30.708678	914.813529	16.836263
30.010506	920.067133	16.841280
30.277989	916.613949	16.846298
29.822907	916.180507	16.851315
30.135471	910.315509	16.856333
30.330562	914.883195	16.861351
30.114673	918.480157	16.866368
30.015957	916.738011	16.871386
30.027159	925.023691	16.876403
30.148576	923.054547	16.881421
30.384463	908.955346	16.886439
30.407979	917.870262	16.891456
30.332578	910.163078	16.896474
30.230705	930.357690	16.901491
30.613667	939.724390	16.906509
30.607949	937.977138	16.911527
30.464020	943.617287	16.916544
31.139569	938.408630	16.921562
30.819130	929.155594	16.926579
30.351215	914.361920	16.931597
30.628843	915.233807	16.936615
30.406672	917.266456	16.941632
30.722176	913.872021	16.946650
30.641981	928.164968	16.951667
30.767197	928.445345	16.956685
30.852555	931.603787	16.961703
30.900818	936.825652	16.966720
30.990807	931.793949	16.971738
30.808903	936.976137	16.976755
30.704712	945.327243	16.981773
31.063570	926.067887	16.986791
30.697167	942.393870	16.991808
30.895190	936.177576	16.996826
30.909261	942.578775	17.001843
31.028431	946.602935	17.006861
30.935219	937.705619	17.011879
30.841421	941.321327	17.016896
31.176879	932.265330	17.021914
31.269866	936.217850	17.026931
30.794831	938.230158	17.031949
31.171108	934.857756	17.036967
30.744572	940.466443	17.041984
31.299247	953.990899	17.047002
31.268222	961.547900	17.052019
31.290625	961.771802	17.057037
31.844819	953.789226	17.062055
31.486069	962.296992	17.067072
31.687427	953.050553	17.072090
31.391816	954.709699	17.077107
31.860673	954.311378	17.082125
31.910699	952.154598	17.087143
31.753721	951.573461	17.092160
31.729346	945.830672	17.097178
31.613612	935.317936	17.102195
31.416024	932.915928	17.107213
31.299765	937.150544	17.112231
31.604352	949.385570	17.117248
31.540923	949.622920	17.122266
31.396134	947.351495	17.127283
31.573020	953.017122	17.132301
31.929034	945.655745	17.137319
31.687955	963.028787	17.142336
31.686543	955.878043	17.147354
31.874644	963.728920	17.152371
31.809670	974.118887	17.157389
32.306917	973.873910	17.162407
31.896108	969.854794	17.167424
32.600033	968.687484	17.172442
32.449817	968.278859	17.177459
31.915877	954.328641	17.182477
32.324841	947.227214	17.187495
32.060553	950.232155	17.192512
32.027431	963.053440	17.197530
32.380879	962.537499	17.202547
32.425467	975.753723	17.207565
32.442254	964.951959	17.212583
32.150156	974.992498	17.217600
32.418288	973.028764	17.222618
32.659108	971.542688	17.227635
32.447635	972.936185	17.232653
32.973223	956.677135	17.237671
32.589853	953.423751	17.242688
32.245845	940.150695	17.247706
32.237437	946.564885	17.252723
32.101270	956.584139	17.257741
32.794085	967.792660	17.262759
32.728679	975.623301	17.267776
32.748036	970.810940	17.272794
32.783706	972.326663	17.277811
32.642617	978.919446	17.282829
32.549553	966.298185	17.287847
32.591931	962.529962	17.292864
32.575352	965.808524	17.297882
32.485036	964.816149	17.302899
32.438802	977.749954	17.307917
32.947125	989.385033	17.312935
33.024498	987.542705	17.317952
33.266474	997.442774	17.322970
33.266345	991.364806	17.327987
33.133565	998.461231	17.333005
33.329488	988.742247	17.338023
33.140113	991.956367	17.343040
33.084445	985.659882	17.348058
33.302946	983.009635	17.353075
32.915622	984.023579	17.358093
32.791094	984.677608	17.363111
33.264815	992.748839	17.368128
33.715895	987.247129	17.373146
33.367078	994.289036	17.378163
32.898217	983.301415	17.383181
33.420673	985.936939	17.388199
33.781115	997.121815	17.393216
33.773266	1004.129239	17.398234
33.965571	989.449813	17.403251
33.640284	987.102520	17.408269
33.760765	980.159890	17.413287
33.495854	983.979144	17.418304
33.739321	990.256055	17.423322
33.641397	976.868676	17.428339
33.728510	981.014633	17.433357
34.195544	988.553571	17.438375
33.871826	991.413193	17.443392
33.784809	981.893180	17.448410
33.883408	983.187602	17.453427
33.983284	1000.119090	17.458445
34.221226	999.255166	17.463463
34.114225	979.191415	17.468480
34.013521	982.063432	17.473498
34.140291	989.299071	17.478515
34.108941	999.645914	17.483533
34.482028	986.613927	17.488551
33.900449	982.959240	17.493568
34.110228	987.480461	17.498586
34.054597	993.952560	17.503603
34.362508	998.691943	17.508621
34.084064	999.398490	17.513639
34.396548	1005.692995	17.518656
34.694401	1001.439760	17.523674
34.516147	998.031152	17.528691
34.455889	998.776099	17.533709
34.531521	993.137548	17.538727
34.289284	996.341016	17.543744
34.512507	997.947278	17.548762
34.694377	989.155162	17.553779
34.438726	1001.635794	17.558797
34.257059	993.067895	17.563815
34.309919	992.308710	17.568832
34.025380	998.355921	17.573850
34.515934	999.093464	17.578867
34.347775	1012.522932	17.583885
34.670472	1021.078593	17.588903
34.548779	1019.270608	17.593920
34.701781	1016.419176	17.598938
34.924825	1010.252586	17.603955
34.979960	1019.282521	17.608973
34.607275	1005.780376	17.613991
34.955921	1015.307130	17.619008
34.763593	1010.723588	17.624026
34.989269	1017.912183	17.629043
35.037810	1034.353121	17.634061
35.512089	1034.256911	17.639079
35.795501	1034.275815	17.644096
35.577431	1022.743938	17.649114
35.702857	1019.827397	17.654131
35.514179	1014.791994	17.659149
35.563998	1016.690519	17.664167
34.993378	1013.797827	17.669184
35.173895	1012.422183	17.674202
35.280937	1005.393285	17.679219
35.646768	1014.368226	17.684237
35.558036	1013.413470	17.689255
35.533426	1010.495192	17.694272
35.444476	1010.405176	17.699290
35.495959	1022.029801	17.704307
35.773044	1036.629780	17.709325
35.973574	1026.051659	17.714343
35.928731	1019.507308	17.719360
35.491685	1012.724603	17.724378
35.917273	1017.123655	17.729395
35.931532	1026.788015	17.734413
35.967083	1029.398845	17.739431
35.941882	1016.959424	17.744448
35.934633	1033.469063	17.749466
36.104478	1029.680855	17.754483
36.260732	1032.742998	17.759501
35.921791	1009.752197	17.764519
36.426826	1023.701058	17.769536
35.812246	1021.399086	17.774554
36.217693	1029.051834	17.779571
36.275443	1036.920011	17.784589
36.256141	1039.009253	17.789607
36.395912	1037.368586	17.794624
35.939068	1039.359120	17.799642
36.364148	1035.142750	17.804659
36.147948	1041.059345	17.809677
35.647686	1034.857747	17.814695
36.318703	1031.470707	17.819712
36.010218	1032.753173	17.824730
36.198956	1036.125814	17.829747
36.188252	1045.847744	17.834765
36.174507	1054.374083	17.839783
36.496998	1059.067015	17.844800
36.430573	1060.800718	17.849818
36.633783	1053.636810	17.854835
36.739608	1062.740877	17.859853
36.711732	1055.010405	17.864871
37.060797	1050.007506	17.869888
36.665157	1054.367975	17.874906
37.181074	1048.483695	17.879923
36.964104	1053.157004	17.884941
36.813497	1050.526709	17.889959
36.961232	1045.586914	17.894976
36.986974	1048.552742	17.899994
37.176187	1040.917652	17.905011
37.278105	1045.850271	17.910029
37.134356	1044.058362	17.915047
37.239677	1049.034631	17.920064
37.392359	1054.319067	17.925082
37.232948	1045.753967	17.930099
37.113994	1046.167279	17.935117
37.084258	1044.512144	17.940135
37.098677	1043.367652	17.945152
36.737230	1053.185567	17.950170
37.366818	1063.744480	17.955187
37.383593	1055.322188	17.960205
37.588424	1070.817158	17.965223
37.723477	1062.988570	17.970240
37.665939	1069.634568	17.975258
38.021033	1057.927657	17.980275
37.618629	1061.901016	17.985293
37.691299	1063.688667	17.990311
37.895725	1057.521821	17.995328
37.742483	1063.797796	18.000346
37.752251	1059.971545	18.005363
38.053083	1058.119446	18.010381
37.553003	1055.824777	18.015399
38.001229	1051.983480	18.020416
37.647753	1062.977289	18.025434
37.771956	1053.948018	18.030451
37.739001	1056.803121	18.035469
37.753430	1055.639692	18.040487
38.370564	1047.236951	18.045504
37.876462	1062.734123	18.050522
38.181531	1064.608441	18.055539
38.128368	1071.064402	18.060557
37.648687	1084.691058	18.065575
38.268580	1090.886936	18.070592
38.424497	1086.280371	18.075610
38.634630	1086.036195	18.080627
38.239295	1085.287267	18.085645
38.151920	1083.972526	18.090663
38.230715	1085.708725	18.095680
38.191116	1084.727332	18.100698
38.355401	1092.279034	18.105715
38.663973	1085.007086	18.110733
38.504635	1079.717754	18.115751
38.671210	1090.822607	18.120768
38.813369	1095.752091	18.125786
38.933222	1087.502986	18.130803
39.189977	1087.336714	18.135821
39.199774	1082.383807	18.140839
38.979831	1073.948100	18.145856
38.452507	1081.403026	18.150874
38.589838	1076.082993	18.155891
38.916483	1083.606097	18.160909
38.768747	1098.989070	18.165927
39.232804	1095.811173	18.170944
39.445774	1105.949382	18.175962
39.229684	1101.151784	18.180979
39.154436	1109.397445	18.185997
39.135214	1104.262882	18.191015
39.182215	1096.173513	18.196032
39.220438	1090.446117	18.201050
39.265184	1090.720170	18.206067
39.307838	1102.882729	18.211085
39.207685	1101.222842	18.216103
39.403036	1099.939544	18.221120
39.351972	1102.623917	18.226138
39.716255	1101.440386	18.231155
39.833463	1092.491089	18.236173
39.709632	1103.297460	18.241191
39.687989	1089.093297	18.246208
39.523809	1101.405029	18.251226
39.514051	1093.608583	18.256243
39.445026	1098.826781	18.261261
39.599627	1103.915267	18.266279
39.716043	1096.550342	18.271296
40.017597	1098.822854	18.276314
39.450962	1097.141379	18.281331
39.614240	1107.135892	18.286349
39.849064	1116.800457	18.291367
39.853207	1115.663883	18.296384
39.674440	1116.695652	18.301402
40.014780	1115.241309	18.306419
40.082903	1117.348421	18.311437
39.733037	1122.828383	18.316455
39.748416	1121.049405	18.321472
40.244821	1129.375927	18.326490
40.221642	1144.783607	18.331507
40.864333	1145.213291	18.336525
40.548995	1142.634038	18.341543
40.373463	1131.631926	18.346560
40.575627	1135.557916	18.351578
40.498933	1128.504107	18.356595
40.826634	1130.283365	18.361613
40.731563	1141.145216	18.366631
41.176883	1127.719947	18.371648
40.761833	1118.232321	18.376666
40.794999	1112.130161	18.381683
40.691293	1104.089648	18.386701
40.550004	1106.576715	18.391719
40.736022	1109.192385	18.396736
41.098657	1128.645399	18.401754
41.123292	1127.619225	18.406771
40.841582	1116.217182	18.411789
40.984507	1129.036251	18.416807
41.103814	1130.444207	18.421824
41.191287	1133.662314	18.426842
41.037228	1128.940199	18.431859
41.184807	1127.314081	18.436877
40.824838	1130.094195	18.441895
41.518032	1135.256099	18.446912
41.664948	1138.168241	18.451930
41.546999	1137.208589	18.456947
41.388618	1135.138090	18.461965
41.375867	1147.239931	18.466983
41.482179	1137.396048	18.472000
41.641157	1132.662756	18.477018
41.205242	1135.581006	18.482035
41.660613	1128.595316	18.487053
41.399157	1138.968825	18.492071
41.657835	1128.327883	18.497088
41.753442	1131.333272	18.502106
41.324159	1130.188864	18.507123
41.719159	1120.659530	18.512141
41.207606	1132.303013	18.517159
41.247037	1139.568176	18.522176
41.679115	1145.780876	18.527194
41.904946	1162.093165	18.532211
42.516846	1146.631484	18.537229
42.103556	1155.236250	18.542247
42.613797	1151.956431	18.547264
42.443942	1151.427799	18.552282
42.008671	1133.147887	18.557299
41.842107	1124.325088	18.562317
41.689041	1140.090793	18.567335
41.955928	1145.780252	18.572352
42.255766	1145.929130	18.577370
42.583122	1148.402738	18.582387
42.311752	1138.362402	18.587405
42.228398	1152.545567	18.592423
42.690533	1146.164740	18.597440
42.467153	1153.370098	18.602458
42.448258	1145.653958	18.607475
42.593494	1147.218803	18.612493
42.362522	1155.053371	18.617511
42.722968	1142.506102	18.622528
42.686655	1141.158109	18.627546
42.605642	1143.594710	18.632563
42.791511	1142.660042	18.637581
43.099360	1154.184624	18.642599
42.700924	1146.991865	18.647616
42.932171	1141.559265	18.652634
43.088576	1161.666335	18.657651
43.290634	1160.031678	18.662669
43.057577	1172.679307	18.667687
43.316496	1160.488767	18.672704
43.151154	1146.865664	18.677722
43.030414	1165.614949	18.682739
43.588066	1161.481922	18.687757
43.507202	1154.845333	18.692775
43.503169	1152.507646	18.697792
43.406799	1136.213334	18.702810
42.980526	1133.752451	18.707827
43.645372	1147.894128	18.712845
43.553483	1158.168496	18.717863
43.704943	1169.332573	18.722880
43.836117	1162.205155	18.727898
43.516655	1161.658937	18.732915
43.810908	1155.216045	18.737933
43.803289	1161.977337	18.742951
43.996437	1162.966617	18.747968
43.611714	1163.446818	18.752986
43.520376	1167.055875	18.758003
43.734658	1163.020829	18.763021
43.470440	1152.584878	18.768039
43.843710	1157.200451	18.773056
43.732602	1151.761526	18.778074
43.404977	1160.264508	18.783091
43.649641	1171.877899	18.788109
44.091364	1182.781907	18.793127
44.013775	1182.008438	18.798144
44.262347	1173.606578	18.803162
43.937540	1173.260017	18.808179
44.448871	1178.510390	18.813197
44.541581	1184.744716	18.818215
44.316342	1186.888332	18.823232
44.241502	1186.609907	18.828250
44.396055	1186.664780	18.833267
44.723134	1173.434732	18.838285
44.611180	1187.022787	18.843303
44.027808	1186.252822	18.848320
44.537068	1192.437666	18.853338
44.719540	1208.359149	18.858355
44.637697	1203.679349	18.863373
44.577708	1200.024948	18.868391
44.834119	1205.911732	18.873408
44.853548	1202.241731	18.878426
44.710012	1199.585058	18.883443
44.820339	1197.980550	18.888461
44.716993	1193.925832	18.893479
44.554725	1202.835284	18.898496
45.011428	1215.889284	18.903514
45.158445	1222.241350	18.908531
44.960459	1229.382798	18.913549
45.514490	1229.293029	18.918567
45.136671	1226.445834	18.923584
45.610761	1218.213753	18.928602
45.163090	1225.362760	18.933619
45.335047	1211.159725	18.938637
45.462718	1215.750676	18.943655
45.716556	1219.722240	18.948672
45.684057	1210.105198	18.953690
45.684005	1223.350691	18.958707
45.611418	1213.642096	18.963725
45.710663	1218.149135	18.968743
45.447454	1217.890755	18.973760
45.981121	1210.372044	18.978778
45.625701	1212.384576	18.983795
45.517959	1212.411115	18.988813
45.627365	1213.934242	18.993831
45.597822	1231.580523	18.998848
46.151765	1224.819201	19.003866
46.092214	1238.055091	19.008883
46.304404	1236.068535	19.013901
46.444690	1245.397678	19.018919
46.152402	1235.871820	19.023936
46.668861	1232.161810	19.028954
46.314342	1230.229331	19.033971
46.876276	1225.899953	19.038989
46.537837	1217.492212	19.044007
46.416183	1209.381878	19.049024
46.503703	1204.164287	19.054042
46.630897	1213.350293	19.059059
46.905345	1219.556158	19.064077
46.786360	1202.470043	19.069095
46.583942	1204.985636	19.074112
46.999144	1210.939064	19.079130
46.557795	1210.146846	19.084147
47.180855	1211.564247	19.089165
46.823532	1207.744984	19.094183
46.820990	1212.914928	19.099200
47.111073	1207.542520	19.104218
46.734020	1223.920922	19.109235
47.178416	1218.148782	19.114253
47.435815	1215.003243	19.119271
47.123207	1226.637708	19.124288
47.448822	1216.772045	19.129306
47.220831	1219.705069	19.134323
46.940078	1224.135944	19.139341
47.074529	1222.660201	19.144359
47.015798	1218.844648	19.149376
47.135970	1216.175058	19.154394
47.004216	1222.270992	19.159411
47.190096	1228.386591	19.164429
47.200834	1232.465676	19.169447
47.417737	1244.171829	19.174464
47.738345	1242.395511	19.179482
47.354459	1244.396727	19.184499
47.493103	1252.302819	19.189517
47.714191	1240.228609	19.194535
47.417064	1257.714864	19.199552
47.623414	1253.927200	19.204570
47.996717	1254.638944	19.209587
47.829739	1261.403149	19.214605
47.961119	1259.650165	19.219623
47.918994	1270.352315	19.224640
48.243143	1268.130457	19.229658
48.122186	1270.825806	19.234675
48.408051	1268.543672	19.239693
48.529865	1266.230435	19.244711
48.396259	1271.105341	19.249728
48.534907	1271.298410	19.254746
48.735081	1265.308891	19.259763
48.315287	1269.130380	19.264781
48.738017	1266.028359	19.269799
48.423124	1266.816368	19.274816
48.792576	1257.896897	19.279834
48.635651	1258.253045	19.284851
48.758612	1258.568496	19.289869
48.780322	1258.685210	19.294887
48.649448	1277.575060	19.299904
49.069991	1264.507033	19.304922
48.508399	1256.538191	19.309939
48.599266	1260.680470	19.314957
48.494320	1265.815979	19.319975
48.456104	1263.991734	19.324992
48.955341	1274.833137	19.330010
48.693086	1282.931446	19.335027
48.951120	1282.373641	19.340045
49.280627	1286.775191	19.345063
49.163040	1279.304837	19.350080
49.350096	1283.072277	19.355098
49.365928	1282.101124	19.360115
48.941469	1283.048316	19.365133
49.420007	1281.777443	19.370151
49.512953	1292.253309	19.375168
49.440542	1281.332780	19.380186
49.574947	1292.367059	19.385203
49.540523	1302.866044	19.390221
49.826329	1302.202897	19.395239
49.615059	1299.086591	19.400256
49.769996	1311.225388	19.405274
49.805476	1309.916629	19.410291
49.606455	1312.482199	19.415309
50.239197	1307.826117	19.420327
50.095058	1316.641264	19.425344
50.405229	1300.857482	19.430362
49.998584	1303.203108	19.435379
50.195157	1305.059736	19.440397
50.214668	1305.722767	19.445415
50.247464	1306.140712	19.450432
50.405611	1308.435720	19.455450
50.389266	1305.036399	19.460467
50.248558	1303.565890	19.465485
50.473064	1289.370340	19.470503
50.362247	1299.395282	19.475520
50.614192	1301.814453	19.480538
50.711804	1316.442782	19.485555
50.397074	1325.675993	19.490573
50.804450	1321.610658	19.495591
50.824014	1330.513776	19.500608
51.114991	1321.439305	19.505626
51.425868	1320.728047	19.510643
50.996466	1309.721417	19.515661
50.801481	1305.283387	19.520679
51.377823	1311.546129	19.525696
51.148972	1307.413216	19.530714
51.205777	1310.973844	19.535731
50.955878	1308.911351	19.540749
51.155916	1315.185713	19.545767
50.830601	1315.833341	19.550784
50.976543	1318.351177	19.555802
51.191054	1319.867313	19.560819
51.089518	1319.034471	19.565837
51.174219	1315.392091	19.570855
51.499496	1322.053947	19.575872
51.883407	1328.106995	19.580890
51.983713	1317.869464	19.585907
51.478743	1317.150326	19.590925
51.585665	1313.375073	19.595943
51.755998	1315.059081	19.600960
51.904046	1325.352759	19.605978
51.846638	1327.021956	19.610995
51.659528	1335.515629	19.616013
52.366747	1324.046875	19.621031
52.288534	1326.012832	19.626048
52.507830	1322.456663	19.631066
51.955046	1306.912226	19.636083
51.971797	1319.943712	19.641101
52.254834	1321.830977	19.646119
52.274596	1326.271600	19.651136
52.534480	1328.872574	19.656154
52.714620	1334.705077	19.661171
52.350877	1333.004413	19.666189
52.788420	1325.122005	19.671207
52.785084	1328.026160	19.676224
52.306540	1324.323698	19.681242
52.838431	1315.470270	19.686259
52.302988	1326.461191	19.691277
52.683497	1310.852579	19.696295
52.605352	1318.890500	19.701312
52.374224	1321.663081	19.706330
52.485626	1322.412705	19.711347
52.236264	1339.607523	19.716365
52.451022	1346.838990	19.721383
52.778547	1346.869919	19.726400
52.749246	1339.843316	19.731418
53.344422	1358.752045	19.736435
53.074909	1371.295069	19.741453
53.436034	1369.199954	19.746471
53.575555	1374.931533	19.751488
53.357545	1373.514156	19.756506
53.471467	1366.657614	19.761523
53.293561	1367.228498	19.766541
53.657617	1369.759506	19.771559
53.646047	1374.148243	19.776576
53.550062	1375.482648	19.781594
53.654593	1370.710486	19.786611
53.427336	1370.875675	19.791629
53.753502	1360.785776	19.796647
53.725390	1371.501571	19.801664
53.653012	1366.290050	19.806682
53.836290	1369.486879	19.811699
53.558435	1391.435875	19.816717
54.201371	1385.468467	19.821735
54.348544	1388.311180	19.826752
54.270229	1388.124818	19.831770
54.795470	1384.018911	19.836787
54.562588	1382.376637	19.841805
54.540623	1387.647509	19.846823
54.583286	1381.818333	19.851840
54.602996	1391.930178	19.856858
54.684927	1378.631087	19.861875
54.993244	1381.338094	19.866893
54.627166	1381.944772	19.871911
54.386930	1390.516225	19.876928
54.720854	1395.519892	19.881946
55.041248	1381.564875	19.886963
54.614198	1384.888890	19.891981
54.905731	1384.773974	19.896999
54.759323	1379.283703	19.902016
54.975657	1386.152008	19.907034
55.110255	1380.541967	19.912051
55.024556	1383.563182	19.917069
54.815288	1372.793432	19.922087
54.855319	1379.720916	19.927104
54.900162	1395.433747	19.932122
55.246539	1400.580638	19.937139
55.016242	1409.819600	19.942157
55.354367	1409.208215	19.947175
55.498480	1405.329281	19.952192
55.309265	1404.541732	19.957210
55.823887	1399.844171	19.962227
55.421202	1403.880767	19.967245
55.429963	1402.497289	19.972263
55.676733	1403.506585	19.977280
55.647061	1415.415592	19.982298
55.852368	1419.937625	19.987315
55.851627	1432.848852	19.992333
56.208340	1419.680255	19.997351
56.368631	1424.332423	20.002368
56.041922	1423.468581	20.007386
56.449145	1425.298529	20.012403
56.350338	1427.993588	20.017421
55.895900	1427.222345	20.022439
55.946545	1429.190215	20.027456
56.163680	1428.679840	20.032474
56.077815	1422.829762	20.037491
56.177614	1424.527988	20.042509
56.179157	1438.221533	20.047527
56.451505	1440.520757	20.052544
56.715431	1456.240344	20.057562
56.835330	1448.991497	20.062579
56.335902	1457.284842	20.067597
56.996655	1452.302429	20.072615
57.231432	1445.193382	20.077632
57.265440	1449.612868	20.082650
57.229701	1444.973120	20.087667
57.140445	1443.762793	20.092685
57.325948	1451.933042	20.097703
57.297661	1445.660508	20.102720
56.914244	1437.909831	20.107738
57.208190	1441.111425	20.112755
57.284189	1451.880387	20.117773
57.059212	1452.187237	20.122791
57.445177	1445.805615	20.127808
57.467568	1453.338675	20.132826
57.740271	1458.569712	20.137843
57.526871	1463.977902	20.142861
57.610430	1468.616856	20.147879
57.611842	1467.161938	20.152896
57.792362	1457.902724	20.157914
57.835383	1457.138750	20.162931
58.215598	1454.340016	20.167949
57.719474	1458.801536	20.172967
58.257932	1453.109262	20.177984
58.074563	1451.541278	20.183002
57.754089	1457.468036	20.188019
58.281769	1454.709317	20.193037
58.313150	1452.609049	20.198055
57.885982	1454.869543	20.203072
57.985457	1470.703275	20.208090
58.483516	1476.028403	20.213107
58.471362	1471.738418	20.218125
58.285433	1479.783831	20.223143
58.989468	1473.017836	20.228160
59.194662	1481.412242	20.233178
58.766936	1475.151784	20.238195
58.866527	1479.409517	20.243213
59.067298	1467.322558	20.248231
59.099054	1464.045064	20.253248
59.199030	1462.824023	20.258266
59.185994	1463.078731	20.263283
59.238626	1463.430453	20.268301
59.118127	1473.330772	20.273319
59.578597	1447.881916	20.278336
59.175806	1461.746130	20.283354
59.144393	1451.876312	20.288371
59.332588	1452.314096	20.293389
59.266703	1461.300098	20.298407
59.596218	1454.804236	20.303424
59.212098	1461.722463	20.308442
59.334034	1455.540002	20.313459
59.241615	1457.441924	20.318477
59.392316	1478.282423	20.323495
59.953613	1478.724871	20.328512
59.751512	1490.427403	20.333530
59.791795	1499.851246	20.338547
59.830359	1494.518159	20.343565
60.221065	1491.080276	20.348583
60.220241	1487.675333	20.353600
60.227798	1492.553429	20.358618
60.123053	1496.631732	20.363635
60.220603	1481.853134	20.368653
59.922613	1490.326382	20.373671
60.211703	1490.404361	20.378688
60.311115	1498.660708	20.383706
60.520181	1504.450863	20.388723
60.494967	1508.939605	20.393741
60.809420	1514.804775	20.398759
60.634496	1513.465847	20.403776
60.620571	1524.918003	20.408794
60.350610	1519.715302	20.413811
60.699383	1516.448093	20.418829
60.544211	1509.213916	20.423847
60.678039	1516.066794	20.428864
60.470582	1527.347292	20.433882
60.841557	1531.480463	20.438899
61.260371	1534.337447	20.443917
61.233155	1548.609965	20.448935
61.432461	1544.381511	20.453952
61.063401	1543.865141	20.458970
61.449020	1539.474948	20.463987
61.167978	1541.662063	20.469005
61.024941	1551.682727	20.474023
61.366844	1556.593667	20.479040
61.769753	1565.361098	20.484058
62.181706	1565.460856	20.489075
62.149079	1547.956917	20.494093
62.054055	1553.996713	20.499111
62.171892	1550.879295	20.504128
62.645678	1556.179847	20.509146
62.644347	1541.587114	20.514163
62.277761	1538.899061	20.519181
62.082658	1533.176520	20.524199
61.945948	1530.114766	20.529216
62.048990	1546.310940	20.534234
62.265256	1545.623965	20.539251
62.697595	1546.695718	20.544269
62.218344	1546.073530	20.549287
62.777581	1543.587578	20.554304
62.439084	1547.869781	20.559322
62.725569	1556.374569	20.564339
62.910286	1541.298229	20.569357
62.614370	1549.253603	20.574375
62.934701	1541.657721	20.579392
62.676326	1552.236123	20.584410
62.643938	1543.458368	20.589427
62.532166	1541.680334	20.594445
62.979636	1561.726473	20.599463
63.235008	1561.819204	20.604480
62.903698	1570.562809	20.609498
62.816182	1568.436973	20.614515
63.258940	1565.584240	20.619533
63.141934	1572.987704	20.624551
63.149525	1567.309138	20.629568
63.276518	1574.778521	20.634586
63.261129	1587.231385	20.639603
63.579249	1589.839053	20.644621
63.592000	1596.745648	20.649639
63.964980	1592.811880	20.654656
63.709181	1600.590569	20.659674
63.895578	1599.065630	20.664691
64.181000	1593.220443	20.669709
63.953333	1588.402435	20.674727
64.196668	1575.753285	20.679744
64.161862	1590.648750	20.684762
64.079770	1593.514792	20.689779
64.220985	1587.095724	20.694797
63.905285	1598.011355	20.699815
64.591480	1599.993284	20.704832
64.340128	1605.726214	20.709850
64.548374	1620.015550	20.714867
64.889534	1614.221587	20.719885
64.665083	1606.824646	20.724903
64.804177	1604.221466	20.729920
64.898320	1609.534175	20.734938
64.459803	1594.646959	20.739955
64.819258	1607.492411	20.744973
64.787999	1603.306379	20.749991
65.086330	1602.685444	20.755008
64.824022	1603.998586	20.760026
65.087164	1611.033221	20.765043
65.233323	1610.997889	20.770061
65.025544	1609.856615	20.775079
65.307703	1629.376436	20.780096
65.641188	1618.600401	20.785114
65.618805	1625.989062	20.790131
65.477111	1627.538942	20.795149
65.410478	1627.312875	20.800167
65.510980	1622.048946	20.805184
65.565739	1627.781263	20.810202
65.650119	1633.783510	20.815219
66.309984	1643.271309	20.820237
66.080339	1644.544621	20.825255
66.206783	1644.338799	20.830272
66.137172	1647.070343	20.835290
66.171566	1650.508311	20.840307
66.482545	1648.569352	20.845325
66.636720	1651.556185	20.850343
66.454473	1650.937956	20.855360
66.327085	1640.997860	20.860378
66.169659	1642.114681	20.865395
66.617526	1639.119118	20.870413
66.275237	1647.548884	20.875431
66.617743	1650.414687	20.880448
66.739616	1648.647375	20.885466
66.355863	1653.520549	20.890483
66.964212	1662.864943	20.895501
66.570692	1672.928075	20.900519
66.695325	1669.923186	20.905536
67.033268	1665.862341	20.910554
66.466836	1666.828639	20.915571
67.032304	1670.742012	20.920589
67.520409	1682.749964	20.925607
67.364970	1697.228893	20.930624
67.425329	1690.693061	20.935642
67.005964	1694.647123	20.940659
67.788644	1682.642427	20.945677
67.635359	1684.036329	20.950695
67.581338	1690.480024	20.955712
67.853755	1688.607066	20.960730
67.663207	1690.672718	20.965747
67.933740	1675.440802	20.970765
67.672814	1682.544950	20.975783
67.861087	1687.552585	20.980800
67.773726	1691.104316	20.985818
68.094623	1701.017660	20.990835
68.239325	1707.111472	20.995853
68.115818	1705.676106	21.000871
68.147699	1709.859290	21.005888
68.574686	1709.672656	21.010906
68.654430	1714.031390	21.015923
68.309377	1704.860705	21.020941
68.651322	1707.786569	21.025959
68.492681	1706.833260	21.030976
68.969468	1697.385487	21.035994
68.382206	1713.456423	21.041011
68.966003	1717.543670	21.046029
68.980558	1732.188508	21.051047
69.482618	1724.642976	21.056064
69.711575	1737.338545	21.061082
69.605599	1724.816606	21.066099
69.577517	1718.556567	21.071117
69.406724	1708.938832	21.076135
69.216350	1710.228087	21.081152
69.992672	1711.170214	21.086170
69.502360	1719.146652	21.091187
69.589417	1718.726081	21.096205
69.537231	1724.711884	21.101223
69.740253	1717.134307	21.106240
69.645692	1727.807074	21.111258
69.482661	1731.351733	21.116275
69.906461	1717.850496	21.121293
69.787401	1728.713305	21.126311
69.477319	1721.951462	21.131328
70.049901	1732.847930	21.136346
69.943809	1740.893575	21.141363
70.111957	1746.765964	21.146381
70.376159	1737.995298	21.151399
70.336584	1739.522875	21.156416
70.223242	1750.722493	21.161434
70.283124	1767.190732	21.166451
70.510136	1759.801895	21.171469
70.580375	1772.468703	21.176487
70.726978	1769.627623	21.181504
71.106124	1765.591861	21.186522
71.148723	1772.099347	21.191539
71.105285	1760.801578	21.196557
71.322621	1768.913334	21.201575
71.159795	1768.405673	21.206592
71.401242	1762.119171	21.211610
71.267046	1761.935248	21.216627
71.471519	1756.383574	21.221645
71.205151	1754.882219	21.226663
71.580123	1754.915185	21.231680
71.998629	1762.714537	21.236698
71.605505	1760.835386	21.241715
71.805030	1759.399900	21.246733
71.680667	1762.670247	21.251751
71.870678	1768.917938	21.256768
72.142010	1775.433773	21.261786
72.272176	1780.207526	21.266803
72.011179	1781.662494	21.271821
72.761419	1787.266962	21.276839
72.265348	1776.349387	21.281856
72.432566	1775.950972	21.286874
72.312366	1788.448801	21.291891
72.283211	1778.338594	21.296909
72.300767	1779.276521	21.301927
72.005010	1779.607090	21.306944
72.447464	1772.266549	21.311962
72.285145	1780.160065	21.316979
72.224597	1782.959642	21.321997
72.728935	1788.214449	21.327015
72.606355	1800.977764	21.332032
72.747378	1798.165958	21.337050
73.043226	1795.683366	21.342067
72.880916	1790.072376	21.347085
73.157888	1796.442159	21.352103
73.333672	1815.092015	21.357120
73.863758	1801.826543	21.362138
73.456140	1802.594385	21.367155
73.810468	1817.593184	21.372173
73.873761	1820.392300	21.377191
74.032871	1804.101535	21.382208
73.988017	1788.568620	21.387226
73.675243	1785.679582	21.392243
73.776206	1789.135551	21.397261
73.938464	1799.301036	21.402279
74.037374	1807.077893	21.407296
74.208691	1802.765395	21.412314
74.251758	1808.767862	21.417331
74.301482	1807.450523	21.422349
74.428503	1805.458313	21.427367
74.224593	1804.695140	21.432384
74.258428	1803.686422	21.437402
74.125970	1804.518458	21.442419
74.573521	1805.830857	21.447437
74.392080	1820.926223	21.452455
74.327451	1832.528540	21.457472
74.848673	1830.143186	21.462490
74.517154	1823.640299	21.467507
74.762847	1833.915816	21.472525
75.109083	1829.351831	21.477543
74.799145	1849.687384	21.482560
75.420221	1851.184053	21.487578
75.142074	1860.171950	21.492595
75.259209	1850.764664	21.497613
75.204343	1853.544426	21.502631
75.274896	1852.741405	21.507648
75.122225	1852.039634	21.512666
75.172998	1855.260467	21.517683
75.468354	1864.688723	21.522701
76.165742	1865.558014	21.527719
75.899926	1879.637790	21.532736
75.996827	1867.885592	21.537754
75.743715	1871.542228	21.542771
75.988888	1872.586518	21.547789
76.027967	1874.149125	21.552807
76.131394	1881.028998	21.557824
76.514820	1882.581839	21.562842
76.643427	1897.972699	21.567859
76.297031	1891.888712	21.572877
76.984497	1899.977367	21.577895
76.891398	1889.094423	21.582912
76.847125	1885.030293	21.587930
76.998158	1881.686695	21.592947
77.151496	1876.515406	21.597965
77.283469	1878.325407	21.602983
76.956241	1884.853005	21.608000
77.387774	1878.609269	21.613018
77.332485	1881.376477	21.618035
77.199756	1875.896534	21.623053
77.406306	1872.626296	21.628071
77.655373	1871.665910	21.633088
77.514029	1865.003815	21.638106
77.483445	1880.444850	21.643123
77.471863	1882.498264	21.648141
77.847240	1872.968450	21.653159
77.480354	1874.676717	21.658176
77.635728	1871.001060	21.663194
78.151850	1888.897036	21.668211
78.225201	1892.347883	21.673229
78.113350	1893.492295	21.678247
78.300115	1893.185496	21.683264
78.266770	1888.886107	21.688282
78.319720	1887.328400	21.693299
78.094885	1894.367013	21.698317
78.636899	1888.311105	21.703335
78.447747	1891.418045	21.708352
78.337532	1882.011647	21.713370
78.819915	1883.255474	21.718387
78.645184	1903.547814	21.723405
79.309915	1911.311810	21.728423
79.047967	1910.368364	21.733440
79.092066	1901.250225	21.738458
79.125657	1902.229830	21.743475
78.948145	1905.391757	21.748493
79.210422	1899.849919	21.753511
78.971964	1903.734655	21.758528
79.244994	1895.527455	21.763546
79.188102	1909.634486	21.768563
78.907807	1920.765686	21.773581
79.597988	1927.512621	21.778599
79.322622	1930.711976	21.783616
79.797778	1932.285166	21.788634
79.895903	1937.998164	21.793651
79.817165	1942.918307	21.798669
79.885617	1942.469086	21.803687
79.860634	1949.274424	21.808704
79.997737	1948.533561	21.813722
80.237568	1948.070113	21.818739
80.322234	1957.578768	21.823757
80.478173	1961.127150	21.828775
80.741914	1976.212863	21.833792
80.946671	1972.466328	21.838810
81.224177	1967.515417	21.843827
81.079919	1975.027465	21.848845
81.228933	1969.733742	21.853863
81.168874	1968.550364	21.858880
81.168506	1972.369407	21.863898
81.472641	1971.106877	21.868915
81.443625	1970.136401	21.873933
81.789230	1964.287978	21.878951
81.124519	1954.709622	21.883968
81.141520	1958.898352	21.888986
81.488094	1970.164915	21.894003
81.003944	1972.396527	21.899021
81.474358	1967.405924	21.904039
81.235912	1962.696808	21.909056
81.584463	1991.419070	21.914074
81.943955	1985.843038	21.919091
81.810832	1994.202323	21.924109
82.389104	1992.079429	21.929127
82.281654	1993.194754	21.934144
82.062716	1982.435619	21.939162
82.097141	1988.815067	21.944179
82.202044	2000.668663	21.949197
82.239612	2000.760805	21.954215
82.500515	2017.030510	21.959232
82.577123	2012.685460	21.964250
82.666725	2005.475853	21.969267
82.823978	2020.101726	21.974285
82.890469	2016.724008	21.979303
82.509899	2012.813530	21.984320
82.712515	2018.920468	21.989338
82.892486	2030.497215	21.994355
83.330478	2032.985176	21.999373
83.407267	2020.358650	22.004391
83.466827	2028.488932	22.009408
83.527949	2020.223352	22.014426
83.543468	2025.236055	22.019443
83.377061	2027.588318	22.024461
83.588566	2015.275230	22.029479
83.998692	2034.320976	22.034496
83.814691	2048.952998	22.039514
84.140905	2047.642819	22.044531
84.063307	2050.921671	22.049549
84.138157	2052.235673	22.054567
84.117304	2054.849179	22.059584
84.241280	2053.608558	22.064602
84.358838	2050.431132	22.069619
83.615165	2054.464486	22.074637
84.421055	2062.537818	22.079655
84.515665	2081.064959	22.084672
84.680490	2078.621794	22.089690
84.955634	2077.764617	22.094707
84.591377	2073.974656	22.099725
84.920764	2069.744635	22.104743
84.968783	2092.823795	22.109760
85.389723	2096.882994	22.114778
85.273358	2096.772018	22.119795
85.380289	2094.511504	22.124813
85.532891	2097.890009	22.129831
85.812905	2097.783208	22.134848
85.410250	2097.997975	22.139866
85.705197	2094.357214	22.144883
85.661683	2102.257506	22.149901
85.922666	2093.329369	22.154919
85.972499	2107.000079	22.159936
86.056261	2114.040926	22.164954
86.662154	2109.792824	22.169971
86.590352	2124.814459	22.174989
86.403420	2112.977172	22.180007
86.683261	2118.999455	22.185024
86.507801	2117.401768	22.190042
86.728181	2116.676256	22.195059
86.638142	2125.139313	22.200077
87.028558	2112.753943	22.205095
87.116646	2109.003566	22.210112
87.011794	2108.770856	22.215130
87.326402	2097.928059	22.220147
87.032452	2115.152698	22.225165
87.076671	2112.005688	22.230183
87.044384	2107.298950	22.235200
87.214057	2109.936266	22.240218
87.316776	2107.111477	22.245235
86.933287	2116.299057	22.250253
87.437900	2130.286728	22.255271
87.752867	2127.933651	22.260288
87.342350	2136.797246	22.265306
87.610022	2127.340983	22.270323
87.724362	2139.594010	22.275341
88.186109	2151.328676	22.280359
87.852458	2156.749601	22.285376
88.000865	2163.811900	22.290394
88.408724	2159.579032	22.295411
88.208063	2158.067347	22.300429
88.436984	2166.597226	22.305447
88.393020	2165.120955	22.310464
88.316858	2164.239913	22.315482
88.597934	2167.156454	22.320499
88.783153	2183.021568	22.325517
88.727845	2179.183180	22.330535
88.966696	2192.903243	22.335552
88.718336	2182.741938	22.340570
89.241142	2177.051891	22.345587
88.861187	2174.883429	22.350605
89.407635	2177.146119	22.355623
89.822762	2194.777336	22.360640
89.613224	2195.817141	22.365658
89.837623	2196.908892	22.370675
89.798673	2206.812618	22.375693
90.081134	2193.045968	22.380711
90.200415	2192.853887	22.385728
90.245616	2194.166233	22.390746
90.287890	2199.193730	22.395763
89.922176	2209.644156	22.400781
89.933629	2197.741014	22.405799
90.366065	2183.969810	22.410816
90.244897	2194.956318	22.415834
90.282143	2190.983497	22.420851
90.247035	2198.128214	22.425869
90.281092	2205.457774	22.430887
90.528401	2208.259682	22.435904
90.597644	2212.443443	22.440922
90.862780	2206.140450	22.445939
90.924685	2214.295697	22.450957
91.177554	2223.749736	22.455975
91.317524	2224.570670	22.460992
91.042505	2225.971060	22.466010
91.347168	2227.750885	22.471027
91.228798	2238.493964	22.476045
91.390265	2233.144559	22.481063
91.753559	2235.413859	22.486080
91.700598	2245.935237	22.491098
91.847615	2242.510144	22.496115
92.318130	2245.289712	22.501133
91.938063	2245.475692	22.506151
92.112586	2245.057186	22.511168
91.667905	2240.235128	22.516186
92.319107	2250.097029	22.521203
92.475699	2259.635604	22.526221
91.989768	2259.595152	22.531239
92.496713	2265.948010	22.536256
92.389740	2267.596655	22.541274
92.698361	2268.100808	22.546291
92.849314	2274.575720	22.551309
93.287320	2284.145965	22.556327
93.276997	2288.818778	22.561344
93.502151	2293.334768	22.566362
93.544822	2291.788105	22.571379
93.377761	2288.794096	22.576397
93.411787	2288.265046	22.581415
93.451632	2278.882270	22.586432
93.475156	2282.445150	22.591450
93.552256	2283.121288	22.596467
93.397768	2280.671313	22.601485
93.500225	2301.498237	22.606503
93.746270	2303.839570	22.611520
94.119255	2308.360807	22.616538
94.597730	2305.508678	22.621555
94.324606	2300.328336	22.626573
94.175106	2302.674829	22.631591
94.543524	2298.561728	22.636608
94.311503	2309.016514	22.641626
94.769271	2318.249136	22.646643
94.945067	2324.070020	22.651661
94.845261	2333.219577	22.656679
94.999695	2330.380338	22.661696
94.905960	2328.457375	22.666714
95.069590	2330.991520	22.671731
95.157497	2332.963120	22.676749
95.320478	2332.940933	22.681767
95.577704	2324.057455	22.686784
95.295521	2323.290741	22.691802
95.089207	2334.997639	22.696819
95.382684	2339.465064	22.701837
95.576258	2350.408667	22.706855
95.839107	2343.768283	22.711872
95.873365	2347.061226	22.716890
96.147573	2333.759707	22.721907
96.534660	2359.970585	22.726925
96.163838	2364.557874	22.731943
96.623796	2357.643583	22.736960
96.233792	2367.621335	22.741978
96.699277	2366.567052	22.746995
96.731648	2361.856429	22.752013
96.688298	2372.635176	22.757031
96.986176	2364.452276	22.762048
96.544405	2366.418495	22.767066
96.667900	2371.720520	22.772083
96.871022	2379.629635	22.777101
96.670044	2385.585315	22.782119
97.727336	2384.034330	22.787136
96.880067	2385.985178	22.792154
97.373619	2394.956589	22.797171
97.430378	2411.908794	22.802189
97.298535	2416.190385	22.807207
97.906637	2397.960323	22.812224
97.582011	2412.273812	22.817242
97.990007	2422.151819	22.822259
98.278269	2421.642900	22.827277
98.620587	2434.204427	22.832295
98.526942	2435.951994	22.837312
98.672344	2444.330973	22.842330
98.352860	2433.587319	22.847347
98.495223	2440.549678	22.852365
98.508749	2437.776685	22.857383
98.727080	2430.470992	22.862400
98.671314	2442.315334	22.867418
98.776259	2451.322408	22.872435
99.024302	2447.325973	22.877453
99.050850	2459.185835	22.882471
99.690338	2452.915634	22.887488
99.762823	2460.043598	22.892506
99.860996	2452.191778	22.897523
99.943646	2454.833311	22.902541
99.653384	2452.224687	22.907559
100.000329	2448.256941	22.912576
99.573261	2452.704727	22.917594
99.990755	2467.574243	22.922611
100.582535	2473.225851	22.927629
100.016012	2484.455896	22.932647
100.174715	2471.803596	22.937664
100.050474	2474.578542	22.942682
100.743704	2482.227861	22.947699
100.440600	2471.046074	22.952717
100.336085	2479.117051	22.957735
100.863265	2481.228150	22.962752
100.610282	2496.123831	22.967770
100.755302	2500.775518	22.972787
100.724426	2499.237203	22.977805
101.080795	2499.976904	22.982823
101.197434	2505.936516	22.987840
101.466173	2517.076750	22.992858
101.369967	2524.373194	22.997875
101.603238	2522.522066	23.002893
101.616093	2519.376743	23.007911
101.942112	2513.591178	23.012928
101.777127	2515.207904	23.017946
101.600919	2508.655184	23.022963
102.230870	2523.403089	23.027981
101.964107	2542.946786	23.032999
102.439078	2534.723439	23.038016
102.432237	2538.212223	23.043034
102.370932	2542.719502	23.048051
102.847397	2537.077634	23.053069
102.529323	2534.845778	23.058087
102.661755	2543.908559	23.063104
102.918355	2545.929500	23.068122
102.705221	2555.204234	23.073139
103.058321	2546.217255	23.078157
103.385388	2559.964808	23.083175
103.226396	2560.084593	23.088192
103.618523	2555.904597	23.093210
103.207263	2550.130378	23.098227
103.710669	2546.706202	23.103245
103.304040	2568.282294	23.108263
103.795684	2563.117773	23.113280
104.268265	2566.534607	23.118298
104.074117	2580.868817	23.123315
104.171458	2565.691688	23.128333
104.104097	2568.179997	23.133351
104.184721	2564.171892	23.138368
104.261024	2585.075834	23.143386
104.383164	2590.744248	23.148403
104.900453	2591.032663	23.153421
104.689304	2583.699511	23.158439
105.164269	2592.415131	23.163456
104.871352	2591.249257	23.168474
104.940983	2593.810791	23.173491
105.319423	2598.384903	23.178509
105.159428	2618.492684	23.183527
105.680509	2616.981504	23.188544
105.487045	2614.531278	23.193562
105.566409	2617.110227	23.198579
105.870544	2615.923402	23.203597
105.619537	2621.931184	23.208615
105.652675	2634.102587	23.213632
106.175151	2636.656303	23.218650
106.041634	2641.490535	23.223667
106.040105	2637.138640	23.228685
105.983369	2644.924465	23.233703
106.395327	2641.347323	23.238720
106.460597	2659.055903	23.243738
106.766875	2661.293162	23.248755
106.716804	2660.673124	23.253773
106.776532	2665.057318	23.258791
106.808756	2662.997807	23.263808
107.452938	2659.810359	23.268826
107.311302	2674.884424	23.273843
107.591464	2679.256180	23.278861
107.804842	2672.670768	23.283879
107.667347	2665.332356	23.288896
107.820674	2677.573331	23.293914
107.826129	2681.091778	23.298931
107.835348	2679.225238	23.303949
107.835821	2669.797928	23.308967
107.719338	2664.542440	23.313984
107.767042	2683.554131	23.319002
107.837727	2697.285147	23.324019
107.990946	2693.256171	23.329037
108.474095	2696.753435	23.334055
108.342087	2694.927957	23.339072
108.674468	2707.484921	23.344090
108.835139	2714.248837	23.349107
109.066494	2714.105472	23.354125
109.157407	2715.429631	23.359143
109.168305	2708.490878	23.364160
109.127298	2715.863968	23.369178
109.553823	2715.923582	23.374195
109.490267	2713.582391	23.379213
109.273888	2714.342399	23.384231
109.476452	2727.247956	23.389248
110.018086	2726.835048	23.394266
109.882855	2739.588386	23.399283
110.032342	2744.312027	23.404301
109.975734	2741.133361	23.409319
109.888694	2740.582236	23.414336
110.418020	2746.373119	23.419354
110.187347	2757.093071	23.424371
110.822785	2760.067815	23.429389
110.396856	2769.041442	23.434407
110.561525	2777.231344	23.439424
111.243815	2771.077419	23.444442
111.023448	2784.737323	23.449459
111.198648	2791.565271	23.454477
111.414559	2789.555871	23.459495
111.510303	2795.780816	23.464512
111.689241	2789.137635	23.469530
111.385672	2784.845649	23.474547
111.546562	2787.534942	23.479565
111.740898	2789.278455	23.484583
111.663852	2796.786628	23.489600
112.370735	2813.612107	23.494618
111.987719	2818.330823	23.499635
111.984849	2808.310603	23.504653
112.098131	2803.227385	23.509671
112.150598	2810.573245	23.514688
112.625649	2818.083302	23.519706
112.340613	2833.249402	23.524723
112.934738	2827.008274	23.529741
113.215219	2821.763140	23.534759
113.280363	2829.451045	23.539776
113.509685	2819.467034	23.544794
113.315642	2821.583859	23.549811
113.730325	2810.658676	23.554829
113.788183	2811.719746	23.559847
113.802917	2824.945169	23.564864
113.930815	2829.173539	23.569882
113.983352	2832.097590	23.574899
114.246366	2825.176104	23.579917
113.955138	2829.170302	23.584935
114.406652	2834.515759	23.589952
114.538362	2829.192933	23.594970
114.501004	2824.553081	23.599987
114.536935	2825.361937	23.605005
114.557499	2825.428343	23.610023
114.695320	2822.657910	23.615040
115.106622	2842.909993	23.620058
114.903379	2856.999666	23.625075
115.127720	2853.770651	23.630093
115.262401	2854.283137	23.635111
115.244487	2855.507578	23.640128
115.576375	2845.308643	23.645146
115.116480	2848.322448	23.650163
115.242828	2859.718761	23.655181
116.128000	2871.150849	23.660199
115.731606	2863.426832	23.665216
116.009081	2863.560298	23.670234
115.304990	2876.620632	23.675251
115.773540	2880.019222	23.680269
115.876815	2894.310240	23.685287
115.813530	2891.208342	23.690304
116.369830	2905.179055	23.695322
116.802921	2924.900733	23.700339
116.746786	2913.919847	23.705357
117.003383	2924.121690	23.710375
116.726830	2914.387316	23.715392
116.886420	2912.405664	23.720410
116.732627	2922.873799	23.725427
117.362829	2932.723588	23.730445
117.560769	2939.904681	23.735463
117.431299	2940.269182	23.740480
117.752022	2941.058674	23.745498
118.311421	2962.761636	23.750515
118.101434	2960.354981	23.755533
118.581896	2962.211494	23.760551
118.209333	2963.987029	23.765568
118.120816	2966.166243	23.770586
118.660240	2968.294422	23.775603
118.723885	2964.850692	23.780621
119.000805	2962.677061	23.785639
118.597132	2963.933540	23.790656
118.955154	2956.078664	23.795674
118.724286	2968.452622	23.800691
118.898853	2975.062961	23.805709
119.216067	2970.026652	23.810727
119.246148	2973.759076	23.815744
119.644962	2975.110765	23.820762
119.657190	2987.995830	23.825779
119.407172	3010.406401	23.830797
119.737784	3004.698866	23.835815
119.432123	2996.430333	23.840832
119.928964	3007.074329	23.845850
119.993089	3017.448409	23.850867
120.277958	3028.286594	23.855885
120.393855	3026.974579	23.860903
120.403034	3036.751286	23.865920
120.692100	3042.194849	23.870938
120.353480	3042.453246	23.875955
120.777414	3056.952966	23.880973
120.803339	3046.511481	23.885991
121.006565	3063.469759	23.891008
121.443280	3068.255798	23.896026
121.621999	3071.062276	23.901043
121.642212	3073.972494	23.906061
121.993992	3075.830242	23.911079
121.750994	3076.913213	23.916096
122.353135	3076.108918	23.921114
122.190569	3100.260760	23.926131
122.468644	3093.860745	23.931149
123.048868	3080.150925	23.936167
122.827562	3091.377759	23.941184
123.025663	3081.546837	23.946202
122.886680	3085.940172	23.951219
122.723533	3091.770221	23.956237
122.977594	3084.790070	23.961255
122.885261	3085.177162	23.966272
122.972986	3082.824847	23.971290
122.801359	3097.477874	23.976307
123.087493	3101.940328	23.981325
123.446671	3090.291429	23.986343
123.530821	3095.732394	23.991360
123.849775	3102.436940	23.996378
123.915676	3126.603523	24.001395
123.622115	3126.454020	24.006413
124.136611	3129.861242	24.011431
124.133083	3124.366986	24.016448
124.084649	3119.179610	24.021466
124.369683	3127.559125	24.026483
124.800469	3137.364521	24.031501
125.038880	3139.849191	24.036519
124.923048	3145.905406	24.041536
125.056285	3146.105659	24.046554
125.049178	3143.916537	24.051571
125.047037	3152.779772	24.056589
125.539212	3148.801747	24.061607
125.550904	3160.190964	24.066624
125.692239	3169.038041	24.071642
125.678201	3172.572263	24.076659
125.822525	3177.795514	24.081677
126.029054	3172.741771	24.086695
126.091117	3176.535508	24.091712
126.000714	3172.844436	24.096730
126.194421	3192.364038	24.101747
126.293880	3198.667447	24.106765
126.739357	3199.869812	24.111783
126.695972	3201.499110	24.116800
126.764845	3191.031875	24.121818
127.054583	3215.706384	24.126835
126.999040	3214.670559	24.131853
127.247190	3216.099527	24.136871
127.311446	3221.931866	24.141888
127.327727	3212.580702	24.146906
127.491385	3234.813117	24.151923
127.628576	3238.674003	24.156941
128.019941	3235.472410	24.161959
127.826106	3242.282596	24.166976
128.359054	3244.355011	24.171994
128.679268	3258.404018	24.177011
128.553797	3258.679523	24.182029
128.833247	3258.967340	24.187047
128.495809	3267.542287	24.192064
128.525001	3267.058153	24.197082
128.794091	3266.438592	24.202099
128.882385	3274.732217	24.207117
129.324937	3272.374788	24.212135
129.048399	3280.776074	24.217152
129.116864	3277.763938	24.222170
129.764539	3297.714376	24.227187
129.437951	3298.933550	24.232205
129.891209	3296.580753	24.237223
130.135161	3301.485430	24.242240
129.971571	3293.626910	24.247258
129.811726	3299.049350	24.252275
130.239251	3325.896025	24.257293
130.586441	3314.693893	24.262311
130.592919	3317.880896	24.267328
130.827941	3326.088433	24.272346
130.683389	3333.686311	24.277363
131.306235	3341.848877	24.282381
131.410309	3345.137377	24.287399
131.087889	3351.718404	24.292416
131.268141	3346.551947	24.297434
131.771499	3347.221314	24.302451
131.489121	3356.160116	24.307469
132.028044	3364.932375	24.312487
131.900784	3367.281834	24.317504
132.099581	3369.352958	24.322522
132.232926	3371.061896	24.327539
132.345392	3381.766334	24.332557
132.735717	3384.732243	24.337575
132.878864	3393.604397	24.342592
132.778236	3389.586631	24.347610
132.950013	3394.733049	24.352627
132.752406	3393.018777	24.357645
132.909010	3381.616055	24.362663
133.375695	3379.620959	24.367680
133.127073	3382.715377	24.372698
133.363279	3394.341006	24.377715
133.386142	3406.303070	24.382733
133.395227	3399.351710	24.387751
133.337424	3406.472055	24.392768
133.621817	3430.721597	24.397786
134.154992	3432.585685	24.402803
134.090182	3442.800302	24.407821
134.618085	3438.936557	24.412839
134.560520	3452.003326	24.417856
134.833809	3451.783950	24.422874
135.170981	3453.353649	24.427891
135.128298	3444.365107	24.432909
135.492059	3446.722869	24.437927
135.356966	3449.528070	24.442944
135.595992	3452.094751	24.447962
135.706331	3448.855086	24.452979
135.912705	3455.908812	24.457997
136.136895	3458.809229	24.463015
136.082029	3464.338367	24.468032
136.036228	3468.224815	24.473050
136.620476	3463.036064	24.478067
136.092165	3470.015520	24.483085
136.285909	3455.431703	24.488103
136.535291	3473.692997	24.493120
136.620059	3480.907818	24.498138
136.863991	3488.227115	24.503155
136.533372	3490.630543	24.508173
136.938385	3499.357565	24.513191
137.199250	3519.065846	24.518208
137.317353	3515.288381	24.523226
137.757461	3512.505205	24.528243
137.713581	3511.050904	24.533261
138.177253	3512.749137	24.538279
138.397345	3539.483438	24.543296
138.300180	3527.675342	24.548314
138.569759	3524.606406	24.553331
138.174199	3530.113188	24.558349
138.700443	3525.305951	24.563367
138.503340	3538.416738	24.568384
138.529595	3545.094712	24.573402
139.033362	3551.407497	24.578419
138.888053	3557.938757	24.583437
139.022819	3550.390044	24.588455
139.127331	3570.372225	24.593472
139.235363	3570.251333	24.598490
139.469048	3568.516819	24.603507
139.847639	3578.276976	24.608525
140.109797	3583.200973	24.613543
140.195196	3599.865741	24.618560
140.307013	3587.892300	24.623578
140.552304	3580.723954	24.628595
140.299768	3599.979340	24.633613
140.748643	3601.304298	24.638631
140.726323	3619.472585	24.643648
140.904278	3619.987783	24.648666
141.151372	3620.564744	24.653683
141.231682	3615.072987	24.658701
141.162858	3620.033066	24.663719
141.713552	3630.372302	24.668736
141.572458	3634.677724	24.673754
142.012039	3636.606998	24.678771
142.513511	3629.969792	24.683789
142.415617	3620.257546	24.688807
142.248492	3616.448994	24.693824
142.424061	3628.377813	24.698842
142.520852	3628.470155	24.703859
142.332331	3634.474794	24.708877
142.871213	3641.249245	24.713895
142.858343	3648.012294	24.718912
142.590179	3655.045754	24.723930
142.741760	3642.355874	24.728947
143.208779	3669.076933	24.733965
143.378822	3664.221305	24.738983
143.589752	3672.887286	24.744000
143.508372	3692.248521	24.749018
143.895310	3680.405514	24.754035
143.845392	3703.016007	24.759053
143.730049	3691.153838	24.764071
143.657658	3703.459280	24.769088
144.129704	3718.204503	24.774106
144.582304	3710.811092	24.779123
144.505519	3715.201148	24.784141
144.863895	3720.867628	24.789159
144.821590	3731.249324	24.794176
144.685732	3744.783084	24.799194
145.457897	3734.937623	24.804211
145.109031	3749.820951	24.809229
145.695873	3754.059703	24.814247
145.811356	3763.242538	24.819264
145.538340	3766.694352	24.824282
145.908751	3770.566160	24.829299
146.230991	3795.185868	24.834317
146.107347	3789.000051	24.839335
146.384210	3793.227405	24.844352
146.436726	3805.207182	24.849370
146.720788	3801.675103	24.854387
146.991522	3813.024148	24.859405
147.212001	3809.880792	24.864423
147.630335	3808.928510	24.869440
147.598674	3826.290441	24.874458
148.682122	3821.809315	24.879475
147.971199	3821.744127	24.884493
148.321676	3825.016207	24.889511
148.773578	3827.177142	24.894528
148.231627	3825.390521	24.899546
148.507228	3823.153869	24.904563
148.796777	3823.004538	24.909581
148.467295	3828.447400	24.914599
148.963855	3823.742582	24.919616
148.552077	3829.731761	24.924634
149.054420	3837.660925	24.929651
148.916648	3841.094720	24.934669
149.046013	3850.786755	24.939687
149.389724	3844.896994	24.944704
149.634145	3861.335083	24.949722
149.842027	3867.972096	24.954739
150.014168	3873.279569	24.959757
149.636670	3869.813245	24.964775
150.426136	3880.658113	24.969792
150.502216	3888.770865	24.974810
150.868299	3880.115769	24.979827
150.766807	3875.021709	24.984845
150.726394	3891.040464	24.989863
150.987218	3894.165627	24.994880
151.146405	3905.251289	24.999898
151.596724	3909.306303	25.004915
151.560800	3904.353469	25.009933
151.512367	3919.707512	25.014951
151.763875	3912.983110	25.019968
151.859633	3924.574271	25.024986
152.048556	3927.802239	25.030003
152.506938	3933.509935	25.035021
152.277337	3940.275484	25.040039
152.161987	3932.270246	25.045056
152.209862	3939.828763	25.050074
152.507752	3945.921432	25.055091
152.311423	3953.174167	25.060109
152.768765	3969.317018	25.065127
152.907728	3976.949658	25.070144
153.183403	3984.857584	25.075162
153.418552	3973.590534	25.080179
153.585672	3976.739861	25.085197
153.820283	3995.032404	25.090215
153.804451	4007.291315	25.095232
153.945674	4003.125048	25.100250
154.376980	4008.382490	25.105267
154.775302	4026.068642	25.110285
154.928903	4024.775901	25.115303
154.840571	4028.050480	25.120320
154.754475	4037.776370	25.125338
154.875679	4028.247370	25.130355
155.038146	4036.848521	25.135373
155.235305	4042.029026	25.140391
155.464795	4047.867309	25.145408
155.686234	4049.250028	25.150426
155.740968	4067.078428	25.155443
156.101999	4068.761232	25.160461
156.151457	4080.009386	25.165479
156.491149	4073.185887	25.170496
156.011346	4077.058392	25.175514
156.215443	4087.423784	25.180531
156.489549	4085.203117	25.185549
156.650876	4103.368369	25.190567
157.199264	4113.910255	25.195584
157.384349	4122.255391	25.200602
157.530435	4122.289511	25.205619
157.941872	4112.901226	25.210637
158.025365	4141.747358	25.215655
158.032143	4141.553946	25.220672
158.133365	4150.145807	25.225690
158.267407	4143.215618	25.230707
158.457094	4143.214500	25.235725
158.561712	4158.080775	25.240743
158.720064	4163.996525	25.245760
158.633999	4169.802218	25.250778
158.682719	4162.181508	25.255795
159.077683	4172.251908	25.260813
158.911231	4188.271733	25.265831
159.348986	4193.288331	25.270848
159.193643	4207.863950	25.275866
159.830740	4215.336584	25.280883
160.051586	4215.557846	25.285901
159.636400	4219.537045	25.290919
160.364601	4227.061696	25.295936
160.292578	4233.051438	25.300954
160.380697	4230.159165	25.305971
160.904067	4247.283038	25.310989
160.618451	4259.401312	25.316007
160.786605	4259.637143	25.321024
160.854473	4266.621350	25.326042
161.029786	4277.812032	25.331059
161.768455	4280.903436	25.336077
161.587327	4279.581050	25.341095
161.867049	4294.410535	25.346112
162.227583	4299.253031	25.351130
162.216722	4307.136546	25.356147
162.633307	4300.966924	25.361165
162.713058	4319.309308	25.366183
162.274395	4320.757586	25.371200
162.484853	4327.624784	25.376218
162.766527	4327.845988	25.381235
163.156438	4333.476158	25.386253
162.887277	4351.658598	25.391271
163.182409	4350.236342	25.396288
163.646815	4348.875948	25.401306
163.558023	4366.342040	25.406323
164.095514	4366.377971	25.411341
163.933100	4380.951679	25.416359
164.069083	4372.288208	25.421376
164.903130	4388.754349	25.426394
165.091671	4403.052142	25.431411
165.017558	4395.226470	25.436429
165.063484	4402.406710	25.441447
165.206962	4390.105822	25.446464
165.006790	4393.454804	25.451482
165.186477	4398.903290	25.456499
165.655243	4417.958160	25.461517
165.566122	4421.087736	25.466535
165.739624	4430.555371	25.471552
166.045620	4445.324047	25.476570
165.879065	4438.835396	25.481587
166.311011	4447.362960	25.486605
166.548809	4466.596106	25.491623
166.561003	4466.278740	25.496640
166.634196	4473.113839	25.501658
167.185232	4496.407663	25.506675
167.409760	4488.210048	25.511693
167.008058	4502.884471	25.516711
167.641180	4508.719642	25.521728
168.190686	4511.307278	25.526746
168.029983	4519.024971	25.531763
168.432813	4517.686838	25.536781
168.505858	4518.177465	25.541799
168.535678	4536.581550	25.546816
168.758617	4540.776495	25.551834
168.854987	4541.951581	25.556851
168.925857	4539.510181	25.561869
169.210169	4551.179523	25.566887
169.001904	4553.144108	25.571904
169.275636	4557.059642	25.576922
169.655735	4578.057181	25.581939
169.789841	4589.431274	25.586957
169.978757	4590.781254	25.591975
170.275097	4574.542250	25.596992
170.237313	4606.072192	25.602010
170.418612	4612.590540	25.607027
171.371612	4617.381339	25.612045
171.415401	4613.845713	25.617063
171.485341	4611.552804	25.622080
171.745969	4609.129015	25.627098
171.509214	4611.735680	25.632115
171.949626	4614.495090	25.637133
171.944501	4625.685847	25.642151
172.022507	4626.109413	25.647168
171.940266	4631.965158	25.652186
172.181085	4633.606876	25.657203
172.661613	4647.805458	25.662221
172.552310	4649.527281	25.667239
173.030759	4642.186263	25.672256
172.801547	4655.621692	25.677274
173.054306	4665.938757	25.682292
173.270954	4667.517979	25.687309
173.334134	4685.601339	25.692327
173.246961	4681.186613	25.697344
173.678325	4690.484571	25.702362
173.533963	4707.063249	25.707380
174.256389	4701.612610	25.712397
174.679475	4718.260226	25.717415
174.666265	4711.349733	25.722432
174.540608	4714.292536	25.727450
174.536438	4719.075491	25.732468
174.706263	4713.850308	25.737485
175.106422	4736.943966	25.742503
175.545393	4735.319227	25.747520
175.642533	4736.459483	25.752538
175.381943	4743.249122	25.757556
175.904636	4745.957785	25.762573
176.013279	4758.791127	25.767591
176.180697	4763.095830	25.772608
176.068310	4769.483480	25.777626
176.158388	4791.817718	25.782644
176.683752	4795.400326	25.787661
176.818263	4803.406482	25.792679
177.083392	4811.913005	25.797696
176.959038	4818.457216	25.802714
177.134487	4834.332506	25.807732
177.325950	4836.171367	25.812749
177.551254	4846.792707	25.817767
177.587453	4844.517682	25.822784
178.004121	4859.023148	25.827802
177.885412	4869.698396	25.832820
178.561074	4877.913364	25.837837
178.480752	4891.707582	25.842855
178.936356	4887.460297	25.847872
178.841272	4897.579465	25.852890
179.040563	4911.181536	25.857908
179.431431	4913.891937	25.862925
179.606643	4915.894336	25.867943
179.572784	4932.932545	25.872960
180.256584	4931.095824	25.877978
180.468224	4934.140491	25.882996
180.574275	4932.028121	25.888013
180.469586	4950.431602	25.893031
180.818704	4945.617024	25.898048
181.364549	4950.029784	25.903066
180.909360	4946.534386	25.908084
181.281199	4956.681448	25.913101
181.572737	4969.786158	25.918119
181.674517	4972.361934	25.923136
181.887624	4981.684764	25.928154
181.823311	4995.587032	25.933172
182.288093	4988.850919	25.938189
182.224826	4996.376783	25.943207
182.397170	5003.477481	25.948224
182.678270	5005.974664	25.953242
182.627758	5020.332490	25.958260
182.833743	5024.624900	25.963277
183.273831	5045.219012	25.968295
183.270603	5047.688143	25.973312
183.690480	5052.158541	25.978330
183.840320	5064.859383	25.983348
183.946155	5071.964214	25.988365
184.300119	5077.177269	25.993383
184.258273	5074.415703	25.998400
184.555969	5085.066877	26.003418
184.765836	5107.089175	26.008436
184.190162	5106.788136	26.013453
184.890903	5119.083896	26.018471
184.857486	5126.238974	26.023488
185.646820	5137.851673	26.028506
185.655897	5149.125754	26.033524
185.635924	5155.953609	26.038541
185.997895	5156.724118	26.043559
185.866586	5169.885748	26.048576
186.410567	5172.272326	26.053594
186.575891	5182.496059	26.058612
186.567163	5173.476088	26.063629
187.112415	5197.743949	26.068647
186.833489	5199.618660	26.073664
187.408646	5199.206774	26.078682
187.477426	5215.525248	26.083700
187.731381	5212.351156	26.088717
187.708116	5225.334913	26.093735
187.675378	5222.565584	26.098752
188.159819	5231.372546	26.103770
188.184291	5256.410210	26.108788
188.296956	5247.506918	26.113805
188.866199	5251.647776	26.118823
189.037315	5269.998901	26.123840
189.483048	5260.696198	26.128858
189.359977	5255.876598	26.133876
189.389662	5269.846420	26.138893
190.071924	5287.006362	26.143911
189.771644	5291.097209	26.148928
190.432589	5288.774761	26.153946
190.358245	5299.171841	26.158964
190.771708	5308.147790	26.163981
190.991022	5313.858656	26.168999
190.835088	5303.220244	26.174016
191.228839	5315.636833	26.179034
191.291489	5333.506270	26.184052
191.812425	5331.676086	26.189069
191.604483	5340.443210	26.194087
191.952174	5336.165379	26.199104
192.316196	5346.566413	26.204122
192.206590	5362.796171	26.209140
192.611455	5363.484211	26.214157
192.481036	5367.359067	26.219175
192.671545	5378.633277	26.224192
193.151254	5380.865809	26.229210
192.833820	5388.194904	26.234228
193.080164	5400.899802	26.239245
193.627235	5404.646434	26.244263
193.651851	5426.183609	26.249280
193.701696	5430.039708	26.254298
193.715788	5445.849269	26.259316
194.066610	5463.594772	26.264333
194.283817	5464.959326	26.269351
194.381942	5484.284876	26.274368
194.817627	5489.317946	26.279386
194.928260	5501.406532	26.284404
195.189051	5516.069523	26.289421
195.517962	5523.016474	26.294439
195.844708	5533.868543	26.299456
196.150132	5533.811416	26.304474
195.981726	5535.684630	26.309492
196.265975	5540.062758	26.314509
196.732011	5551.237091	26.319527
196.714156	5569.892752	26.324544
197.095925	5570.739095	26.329562
196.982167	5585.413469	26.334580
197.346336	5585.899554	26.339597
197.450792	5580.141420	26.344615
197.573248	5591.937802	26.349632
198.194980	5595.477065	26.354650
198.109916	5599.673158	26.359668
198.288397	5606.953060	26.364685
198.925006	5615.231305	26.369703
198.812985	5628.999479	26.374720
199.075076	5625.650425	26.379738
199.035188	5629.249151	26.384756
199.213359	5643.363301	26.389773
199.669006	5650.694500	26.394791
199.835877	5662.133579	26.399808
199.900138	5654.080504	26.404826
199.907204	5666.166485	26.409844
199.937321	5675.205828	26.414861
200.368443	5675.466773	26.419879
200.445207	5685.253259	26.424896
200.723295	5702.609492	26.429914
200.892785	5702.384260	26.434932
200.932323	5715.933042	26.439949
201.732369	5724.031055	26.444967
201.239876	5741.706915	26.449984
201.610066	5739.164801	26.455002
201.942469	5761.001388	26.460020
201.969987	5755.103730	26.465037
202.458653	5762.174110	26.470055
202.225632	5772.662608	26.475072
202.358701	5782.301430	26.480090
203.136774	5792.802003	26.485108
203.280775	5792.574450	26.490125
203.212809	5804.773291	26.495143
203.683656	5814.927420	26.500160
204.263066	5812.535608	26.505178
203.792887	5827.556428	26.510196
204.241309	5842.076646	26.515213
204.509960	5845.115694	26.520231
204.308843	5859.055833	26.525248
204.983620	5868.155272	26.530266
205.424630	5884.008815	26.535284
205.304037	5882.995654	26.540301
205.809686	5888.680784	26.545319
205.981827	5899.014337	26.550336
206.027112	5900.427955	26.555354
206.132193	5908.208767	26.560372
206.304035	5918.712841	26.565389
206.738375	5916.422660	26.570407
207.231423	5924.395239	26.575424
206.998684	5934.950076	26.580442
207.323613	5947.974500	26.585460
207.561765	5941.112552	26.590477
207.893183	5954.442165	26.595495
207.844211	5960.997072	26.600512
208.047132	5969.112980	26.605530
208.237517	5973.597463	26.610548
208.336388	5983.519541	26.615565
208.587827	5990.358852	26.620583
208.858467	6001.213676	26.625600
208.914207	6015.994424	26.630618
209.376999	6024.505274	26.635636
209.457509	6037.732203	26.640653
209.404703	6030.959997	26.645671
209.760232	6055.628063	26.650688
209.824564	6070.148656	26.655706
210.442057	6067.463582	26.660724
210.449289	6091.643301	26.665741
210.820480	6090.347897	26.670759
210.707099	6108.965407	26.675776
211.125749	6111.510645	26.680794
210.871588	6117.772607	26.685812
211.310103	6133.500489	26.690829
211.847522	6135.016963	26.695847
212.133813	6139.429641	26.700864
212.700830	6154.376631	26.705882
212.986180	6158.530607	26.710900
212.936076	6154.491684	26.715917
213.494633	6157.229671	26.720935
213.471484	6157.978483	26.725952
213.678606	6168.631855	26.730970
213.999952	6167.637833	26.735988
214.294724	6176.945326	26.741005
214.167261	6170.165824	26.746023
214.448146	6172.328587	26.751040
214.342072	6166.903142	26.756058
214.385403	6170.943510	26.761076
214.654749	6192.755768	26.766093
215.127931	6195.084129	26.771111
214.915783	6198.286946	26.776128
215.407315	6211.045544	26.781146
215.970883	6212.987249	26.786164
215.955942	6214.886998	26.791181
216.201549	6220.770809	26.796199
216.519273	6241.167628	26.801216
216.237793	6242.067400	26.806234
216.722945	6251.310382	26.811252
216.883422	6271.924432	26.816269
216.909442	6272.883364	26.821287
217.301198	6282.968069	26.826304
217.706207	6288.615427	26.831322
217.882413	6290.412633	26.836340
218.036000	6297.387347	26.841357
218.539180	6307.861836	26.846375
218.875414	6318.239369	26.851392
218.531680	6320.455807	26.856410
218.733595	6322.037484	26.861428
219.093047	6335.896482	26.866445
219.227050	6347.978811	26.871463
219.648219	6348.307621	26.876480
219.808965	6363.245824	26.881498
220.491426	6362.015284	26.886516
220.189524	6372.682224	26.891533
220.428637	6374.854713	26.896551
220.410646	6383.497873	26.901568
220.783688	6404.890069	26.906586
221.390740	6406.016843	26.911604
221.215269	6419.404107	26.916621
221.604713	6425.132866	26.921639
221.791674	6431.136421	26.926656
221.878602	6440.536588	26.931674
222.542804	6444.558674	26.936692
222.137136	6452.157716	26.941709
222.794404	6479.904326	26.946727
222.824268	6476.389462	26.951744
223.232077	6486.313925	26.956762
223.487983	6492.186741	26.961780
223.401915	6511.223393	26.966797
223.906171	6519.143969	26.971815
224.017078	6522.151020	26.976832
224.270914	6520.596172	26.981850
224.704599	6530.835444	26.986868
224.873366	6548.165411	26.991885
225.193277	6546.006727	26.996903
225.518971	6550.066082	27.001920
225.499499	6563.810989	27.006938
225.927704	6563.807235	27.011956
225.862304	6564.430096	27.016973
226.246689	6571.299309	27.021991
226.592549	6587.944951	27.027008
226.429804	6596.440419	27.032026
227.034857	6592.816485	27.037044
227.029185	6610.669462	27.042061
227.123481	6613.050919	27.047079
227.494800	6621.633203	27.052096
227.431264	6637.380189	27.057114
227.666855	6639.758456	27.062132
227.571708	6657.455026	27.067149
227.746391	6672.814314	27.072167
228.188597	6682.525144	27.077184
228.265213	6695.415375	27.082202
228.822374	6703.817055	27.087220
228.912884	6723.198774	27.092237
229.219959	6718.873321	27.097255
229.147678	6737.756520	27.102272
229.220012	6748.497639	27.107290
229.531180	6756.126567	27.112308
229.892897	6773.423364	27.117325
230.144979	6790.816274	27.122343
230.721734	6800.105166	27.127360
231.044636	6820.479721	27.132378
231.340536	6831.012237	27.137396
231.541425	6831.886981	27.142413
231.452138	6845.573584	27.147431
232.068207	6851.658428	27.152448
232.115482	6860.029567	27.157466
232.410425	6869.908782	27.162484
232.715858	6873.163222	27.167501
232.971499	6892.872822	27.172519
233.172905	6903.003474	27.177536
233.007541	6911.366908	27.182554
233.189362	6913.532653	27.187572
233.444766	6926.862257	27.192589
233.666891	6946.545596	27.197607
233.818550	6962.328600	27.202624
234.026215	6980.082220	27.207642
234.681768	6979.632456	27.212660
234.724577	7004.650696	27.217677
235.002539	7013.790777	27.222695
235.338690	7022.463995	27.227712
235.327455	7040.087806	27.232730
235.742428	7058.449878	27.237748
236.155134	7054.565553	27.242765
236.374985	7077.090609	27.247783
236.593176	7077.223935	27.252800
236.860909	7092.259620	27.257818
237.611657	7092.767272	27.262836
237.807427	7106.036897	27.267853
237.868909	7105.708607	27.272871
238.296645	7128.336908	27.277888
238.366127	7131.079052	27.282906
238.642725	7129.031266	27.287924
238.939492	7145.994484	27.292941
239.061127	7145.773577	27.297959
239.285372	7146.019606	27.302976
239.301447	7163.872869	27.307994
239.429908	7173.996157	27.313012
239.709179	7179.890790	27.318029
239.881012	7201.400674	27.323047
240.305082	7199.017241	27.328064
240.070247	7218.185266	27.333082
240.596089	7232.943861	27.338100
240.940648	7248.175997	27.343117
241.313062	7252.262917	27.348135
241.881986	7256.498999	27.353152
241.787544	7282.198919	27.358170
242.374946	7284.834697	27.363188
242.409695	7286.553140	27.368205
242.397692	7298.213837	27.373223
242.659123	7302.943231	27.378240
243.065371	7315.217164	27.383258
243.278925	7315.641659	27.388276
243.432759	7321.306588	27.393293
243.645253	7326.851836	27.398311
243.921078	7341.791749	27.403328
244.173465	7346.184776	27.408346
244.041447	7355.332428	27.413364
244.404208	7364.383632	27.418381
244.761588	7368.984362	27.423399
244.937077	7389.619414	27.428416
245.106701	7401.415887	27.433434
245.516777	7402.403109	27.438452
245.924113	7421.300269	27.443469
246.017930	7424.872087	27.448487
246.253262	7431.455591	27.453504
246.382468	7454.241553	27.458522
246.350194	7453.735369	27.463540
246.863875	7476.779985	27.468557
247.003537	7495.580247	27.473575
247.354960	7500.106175	27.478592
247.264099	7520.997775	27.483610
247.820679	7530.457521	27.488628
248.442384	7533.517312	27.493645
248.807173	7544.099430	27.498663
249.291996	7537.239289	27.503680
249.066670	7555.582199	27.508698
249.606155	7549.745829	27.513716
250.004806	7565.888441	27.518733
249.970294	7582.070511	27.523751
250.103190	7570.482630	27.528768
250.176074	7585.284055	27.533786
250.705242	7596.231921	27.538804
250.993109	7598.892570	27.543821
251.314989	7614.523188	27.548839
251.662661	7623.352737	27.553856
251.485235	7622.383108	27.558874
251.466265	7643.907614	27.563892
251.915160	7651.063888	27.568909
252.303216	7665.263527	27.573927
252.593791	7674.297780	27.578944
252.572093	7692.492117	27.583962
252.952602	7702.077402	27.588980
253.036999	7715.068153	27.593997
252.985274	7731.177281	27.599015
253.175546	7744.546096	27.604032
253.765451	7763.885406	27.609050
254.023646	7777.903425	27.614068
254.504893	7794.933054	27.619085
254.607756	7798.206766	27.624103
255.525121	7814.672439	27.629120
255.546683	7830.340816	27.634138
255.807255	7830.394899	27.639156
256.134321	7834.384871	27.644173
256.056081	7853.595322	27.649191
256.849314	7860.135781	27.654208
257.003782	7876.124338	27.659226
257.146797	7895.735845	27.664244
257.604282	7878.022750	27.669261
257.640257	7894.866504	27.674279
258.307598	7896.927895	27.679296
258.226324	7899.706399	27.684314
258.404862	7912.126900	27.689332
258.819137	7921.271336	27.694349
258.325848	7934.681072	27.699367
258.748410	7936.894467	27.704384
258.893321	7956.786721	27.709402
259.242554	7975.377846	27.714420
259.610019	7980.220245	27.719437
259.661652	7991.675674	27.724455
260.217282	8010.607037	27.729472
259.958160	8030.947827	27.734490
260.648301	8042.281163	27.739508
261.059470	8047.362986	27.744525
260.898712	8074.753965	27.749543
261.383562	8082.255212	27.754560
261.610350	8093.323357	27.759578
262.083465	8106.941735	27.764596
262.470220	8117.785939	27.769613
262.374514	8130.568414	27.774631
262.566841	8138.990025	27.779648
262.864212	8139.606622	27.784666
263.087754	8164.456054	27.789684
263.534408	8162.005821	27.794701
263.369842	8189.722748	27.799719
264.065870	8187.378674	27.804736
264.188083	8214.318265	27.809754
264.330318	8223.499153	27.814772
264.745204	8235.305095	27.819789
264.377820	8251.445183	27.824807
265.040548	8256.778111	27.829824
265.260984	8279.487659	27.834842
265.637270	8300.354316	27.839860
266.149379	8322.361543	27.844877
266.410850	8343.574576	27.849895
266.658345	8350.740574	27.854912
267.064975	8360.426296	27.859930
267.165528	8376.688931	27.864948
267.942547	8387.248001	27.869965
268.096266	8405.825988	27.874983
268.384908	8397.989136	27.880000
268.821187	8422.953975	27.885018
268.750942	8427.025260	27.890036
269.038140	8426.791032	27.895053
268.961027	8439.668680	27.900071
269.711967	8453.329036	27.905088
270.019900	8462.844002	27.910106
270.014786	8485.153448	27.915124
270.426743	8491.270818	27.920141
270.524683	8503.120268	27.925159
270.801086	8505.839675	27.930176
270.729694	8524.844534	27.935194
271.351272	8548.877567	27.940212
271.645404	8551.928863	27.945229
271.331135	8572.600916	27.950247
271.809647	8586.831296	27.955264
272.268195	8603.492683	27.960282
272.478553	8610.159451	27.965300
273.239462	8635.408384	27.970317
273.552954	8644.745771	27.975335
274.044216	8655.346603	27.980352
273.940899	8663.840024	27.985370
274.261623	8672.216506	27.990388
275.035698	8688.506509	27.995405
274.861970	8700.029251	28.000423
275.203592	8712.257411	28.005440
275.512338	8724.879065	28.010458
276.019982	8721.797239	28.015476
276.739573	8730.278596	28.020493
276.479226	8737.382225	28.025511
276.870299	8734.934311	28.030528
277.172959	8752.447439	28.035546
277.044751	8760.572253	28.040564
277.259905	8767.086781	28.045581
277.264689	8776.459965	28.050599
277.549668	8792.476228	28.055616
277.928532	8810.807819	28.060634
278.421787	8815.943299	28.065652
278.401593	8829.626861	28.070669
278.557361	8849.265797	28.075687
279.052628	8858.524301	28.080704
279.339388	8867.341889	28.085722
279.571174	8896.958418	28.090740
279.806589	8900.887208	28.095757
280.289932	8907.855458	28.100775
280.694099	8912.023023	28.105792
280.816976	8922.441767	28.110810
280.914868	8937.827602	28.115828
281.083794	8950.228206	28.120845
281.481676	8966.113272	28.125863
281.930968	8970.684222	28.130880
282.117916	8983.902907	28.135898
281.979885	9001.169581	28.140916
282.740067	9011.232804	28.145933
282.828254	9029.101830	28.150951
283.142230	9043.288878	28.155968
283.625135	9041.505349	28.160986
283.706335	9059.419700	28.166004
284.264821	9067.850678	28.171021
284.570064	9076.791761	28.176039
284.993021	9086.901538	28.181056
284.962576	9102.440218	28.186074
285.089976	9122.892146	28.191092
285.567851	9125.179112	28.196109
285.793772	9135.679710	28.201127
285.997647	9153.413914	28.206144
286.040853	9167.166725	28.211162
286.270104	9190.940011	28.216180
286.758734	9205.153496	28.221197
287.307189	9229.593530	28.226215
287.484307	9246.410088	28.231232
287.757037	9259.094580	28.236250
288.000631	9265.974231	28.241268
288.467704	9282.164459	28.246285
288.697413	9293.883268	28.251303
288.800273	9316.486213	28.256320
289.249974	9319.418549	28.261338
289.778162	9350.972154	28.266356
290.129980	9363.865340	28.271373
290.108088	9369.368988	28.276391
290.403092	9382.520513	28.281408
291.029775	9390.899911	28.286426
291.155005	9409.057130	28.291444
291.665056	9412.602018	28.296461
291.872470	9435.270819	28.301479
292.170743	9451.105602	28.306496
292.678515	9455.999031	28.311514
292.913394	9474.104407	28.316532
293.346807	9473.840950	28.321549
293.327707	9495.405514	28.326567
293.699391	9500.727569	28.331584
293.958608	9502.950959	28.336602
294.020885	9522.286361	28.341620
294.715163	9528.805037	28.346637
294.547383	9553.041961	28.351655
294.689499	9554.150217	28.356672
295.153147	9562.005856	28.361690
295.219924	9586.272385	28.366708
295.485943	9594.184254	28.371725
296.037443	9624.370700	28.376743
296.352362	9624.713071	28.381760
297.116660	9638.662692	28.386778
296.963930	9663.014224	28.391796
297.422602	9662.187957	28.396813
298.212431	9669.446323	28.401831
298.307401	9678.051225	28.406848
298.583146	9684.736554	28.411866
298.670848	9696.518909	28.416884
299.550105	9703.248629	28.421901
299.966104	9714.051302	28.426919
300.047594	9718.111730	28.431936
300.277314	9709.904674	28.436954
300.295854	9728.846158	28.441972
300.750028	9738.316771	28.446989
300.951010	9742.150099	28.452007
301.060157	9734.618653	28.457024
301.431972	9755.140340	28.462042
301.768084	9764.553684	28.467060
301.828497	9765.760001	28.472077
302.368840	9774.361486	28.477095
302.251131	9781.174789	28.482112
302.775804	9791.111149	28.487130
302.860961	9807.128017	28.492148
303.113524	9814.969469	28.497165
303.697184	9826.317430	28.502183
303.664673	9841.055075	28.507200
304.062619	9853.474082	28.512218
303.971733	9877.582560	28.517236
304.325705	9897.365212	28.522253
305.114420	9915.696843	28.527271
304.980158	9932.464919	28.532288
305.563072	9942.745867	28.537306
305.439341	9964.813605	28.542324
306.156667	9978.900296	28.547341
306.229668	9996.728426	28.552359
306.556361	10027.140187	28.557376
306.993731	10039.812052	28.562394
307.257075	10060.824681	28.567412
307.350402	10079.366442	28.572429
308.111464	10094.516738	28.577447
308.161754	10115.543858	28.582464
308.751268	10132.577629	28.587482
309.244772	10150.017976	28.592500
309.525074	10162.196709	28.597517
309.870219	10181.434808	28.602535
309.640363	10194.340753	28.607552
309.942281	10207.870674	28.612570
310.510218	10223.487055	28.617588
310.706712	10236.746184	28.622605
311.195280	10249.280716	28.627623
311.878446	10269.359516	28.632640
312.203231	10270.382366	28.637658
312.341752	10302.712214	28.642676
312.498485	10315.548212	28.647693
313.156879	10317.020843	28.652711
312.964108	10342.342560	28.657728
313.752540	10352.307370	28.662746
313.948043	10374.628701	28.667764
314.163370	10382.381502	28.672781
314.835257	10402.531677	28.677799
314.660507	10408.312174	28.682816
315.144156	10421.917980	28.687834
315.637847	10439.017562	28.692852
315.894598	10444.089507	28.697869
315.907101	10455.603104	28.702887
316.528483	10480.964821	28.707904
316.856273	10491.428125	28.712922
317.173211	10504.305465	28.717940
317.204205	10516.990793	28.722957
317.752745	10533.504046	28.727975
318.073156	10553.371590	28.732992
318.294629	10572.632623	28.738010
318.638807	10577.545664	28.743028
318.828069	10596.499175	28.748045
319.372564	10615.753858	28.753063
319.422597	10624.656728	28.758080
319.701305	10643.697315	28.763098
319.855106	10651.693522	28.768116
320.433250	10672.032338	28.773133
320.771959	10679.532278	28.778151
321.023598	10701.914672	28.783168
320.958146	10703.649129	28.788186
321.350651	10731.096278	28.793204
321.719083	10746.674885	28.798221
321.909502	10750.885824	28.803239
322.159765	10789.956147	28.808256
322.769687	10797.982009	28.813274
322.736391	10821.785872	28.818292
323.133461	10837.540049	28.823309
323.824285	10848.388744	28.828327
324.106764	10877.261613	28.833344
324.259000	10891.181754	28.838362
324.732573	10909.983689	28.843380
325.093762	10925.699355	28.848397
325.212929	10937.379679	28.853415
325.790746	10964.406603	28.858432
326.311191	10988.073414	28.863450
326.384900	10990.998609	28.868468
326.376376	11013.059007	28.873485
327.152214	11019.600171	28.878503
327.365835	11046.226413	28.883520
327.701933	11063.689116	28.888538
327.922414	11081.956188	28.893556
328.064180	11096.244402	28.898573
328.721634	11115.778721	28.903591
329.209767	11139.135026	28.908608
329.759577	11153.179382	28.913626
329.873339	11166.458445	28.918644
330.369688	11197.398117	28.923661
330.949810	11203.341638	28.928679
331.026315	11218.255904	28.933696
331.090210	11228.378888	28.938714
331.688646	11245.500693	28.943732
332.036127	11259.077919	28.948749
332.235635	11274.285567	28.953767
332.281564	11303.407707	28.958784
332.664374	11313.635505	28.963802
333.368314	11335.407851	28.968820
333.683232	11340.161481	28.973837
334.168266	11351.948949	28.978855
334.214615	11371.443483	28.983872
334.321611	11389.043422	28.988890
334.579556	11409.568978	28.993908
335.015495	11425.661747	28.998925
335.482331	11442.554892	29.003943
336.053773	11462.459862	29.008960
336.010727	11472.533419	29.013978
336.421987	11484.828280	29.018996
337.008441	11514.800747	29.024013
337.851361	11520.384281	29.029031
337.778406	11537.112611	29.034048
338.358337	11545.197175	29.039066
338.735641	11552.315658	29.044084
338.888559	11558.035707	29.049101
339.183925	11573.399096	29.054119
339.803443	11596.640660	29.059136
340.083964	11612.116926	29.064154
340.526001	11616.465476	29.069172
340.880270	11622.286628	29.074189
341.359653	11641.341003	29.079207
341.086067	11650.525564	29.084224
341.409768	11669.894863	29.089242
342.007450	11678.942960	29.094260
342.150181	11697.968027	29.099277
342.714322	11704.217353	29.104295
342.868858	11727.929787	29.109312
343.106876	11749.317732	29.114330
343.236020	11769.150215	29.119348
343.428502	11768.422401	29.124365
344.305529	11787.951448	29.129383
343.968633	11812.489346	29.134400
344.142328	11821.897595	29.139418
344.682650	11842.139405	29.144436
344.755349	11854.386496	29.149453
345.337689	11877.204781	29.154471
345.708524	11906.719044	29.159488
345.920953	11931.486823	29.164506
346.311968	11948.297569	29.169524
346.666535	11962.761520	29.174541
347.316723	11974.662452	29.179559
347.825666	11997.868154	29.184576
347.742294	12013.130184	29.189594
348.528533	12027.981284	29.194612
348.630208	12041.019711	29.199629
349.440910	12066.549705	29.204647
349.522732	12079.206022	29.209664
350.380463	12096.651132	29.214682
350.297852	12106.529129	29.219700
350.833893	12126.149835	29.224717
350.744289	12131.361754	29.229735
351.009191	12153.668017	29.234752
351.535492	12175.623898	29.239770
352.209640	12184.012917	29.244788
352.521777	12219.044036	29.249805
352.836458	12231.622928	29.254823
352.984835	12250.736088	29.259840
353.673106	12261.974417	29.264858
353.909098	12277.151899	29.269876
354.150308	12299.686250	29.274893
354.652485	12311.380062	29.279911
354.918654	12332.448479	29.284928
355.162560	12351.095211	29.289946
355.978372	12354.883294	29.294964
356.361410	12375.898718	29.299981
356.570851	12394.446683	29.304999
356.837585	12414.605653	29.310016
356.999726	12432.137931	29.315034
357.570393	12441.929561	29.320052
357.994923	12461.864921	29.325069
358.345216	12475.057332	29.330087
358.994561	12484.006151	29.335104
359.034067	12492.330514	29.340122
359.853358	12505.702109	29.345140
360.299901	12511.635397	29.350157
360.829399	12527.676563	29.355175
361.031566	12538.056483	29.360192
360.938584	12547.228978	29.365210
361.595179	12562.918692	29.370228
361.935121	12574.315981	29.375245
361.992202	12587.797554	29.380263
362.252742	12596.349442	29.385280
362.416037	12621.659501	29.390298
362.932333	12640.532269	29.395316
363.274757	12657.689153	29.400333
363.614623	12681.250600	29.405351
364.008343	12695.298460	29.410368
364.288129	12710.813639	29.415386
364.745054	12738.241001	29.420404
365.063915	12755.363770	29.425421
365.104582	12763.299652	29.430439
365.298689	12789.808261	29.435456
365.438836	12801.173826	29.440474
365.917511	12841.276839	29.445492
366.450265	12864.344090	29.450509
367.070168	12883.134556	29.455527
367.110064	12913.839079	29.460544
367.507580	12920.307547	29.465562
368.187743	12939.505473	29.470580
368.238515	12965.395726	29.475597
368.466487	12978.209753	29.480615
369.235506	12995.296964	29.485632
369.615269	13022.916826	29.490650
369.995552	13031.058572	29.495668
370.360698	13051.682812	29.500685
370.508087	13068.510616	29.505703
371.298454	13086.870369	29.510720
371.201220	13126.407348	29.515738
371.970592	13129.943917	29.520756
371.842339	13162.052042	29.525773
372.201555	13170.313992	29.530791
372.653108	13189.225872	29.535808
373.299347	13220.776983	29.540826
373.779441	13232.784308	29.545844
373.813983	13252.759487	29.550861
374.480400	13264.545011	29.555879
374.932281	13282.383226	29.560896
375.182562	13308.271118	29.565914
375.818154	13327.043780	29.570932
376.022801	13342.785990	29.575949
376.419540	13373.789055	29.580967
376.857786	13383.099800	29.585984
377.455357	13414.459905	29.591002
377.970740	13427.737654	29.596020
377.927260	13441.020844	29.601037
378.247396	13452.207023	29.606055
378.993841	13476.141577	29.611072
379.365519	13497.886369	29.616090
380.084237	13511.672345	29.621108
379.960620	13531.495743	29.626125
380.493926	13551.822599	29.631143
380.988890	13555.351706	29.636160
380.651226	13582.374210	29.641178
381.578600	13603.826809	29.646196
381.384575	13626.809879	29.651213
382.079592	13648.131549	29.656231
382.479195	13672.145946	29.661248
382.858996	13692.023293	29.666266
383.758156	13705.386392	29.671284
384.084984	13724.649938	29.676301
384.372248	13732.774978	29.681319
384.823043	13751.760175	29.686336
385.282677	13767.649123	29.691354
385.774368	13779.250750	29.696372
385.749983	13801.297940	29.701389
385.894203	13813.339298	29.706407
386.328158	13839.423366	29.711424
386.570467	13865.420641	29.716442
387.292794	13877.188318	29.721460
387.799800	13910.701439	29.726477
388.042844	13928.370860	29.731495
388.189090	13946.655493	29.736512
388.702760	13958.699076	29.741530
389.477238	13973.177748	29.746548
389.698990	13991.191635	29.751565
390.508387	14007.029155	29.756583
391.062563	14022.985618	29.761600
391.016214	14033.853735	29.766618
391.824050	14051.539019	29.771636
391.897537	14057.101733	29.776653
392.390060	14087.014051	29.781671
393.226772	14086.197874	29.786688
393.068447	14109.163301	29.791706
393.777437	14109.270347	29.796724
394.090498	14127.371120	29.801741
393.916004	14134.854930	29.806759
394.307489	14142.562742	29.811776
394.624504	14167.980270	29.816794
394.891210	14182.298622	29.821812
394.999100	14196.468166	29.826829
394.761585	14231.570157	29.831847
395.744863	14248.779692	29.836864
396.148266	14277.045095	29.841882
396.592872	14299.458381	29.846900
396.706337	14331.641153	29.851917
397.264446	14357.349616	29.856935
397.565893	14377.461025	29.861952
398.016016	14401.926362	29.866970
399.095409	14430.651418	29.871988
399.230958	14456.625167	29.877005
399.548392	14476.933142	29.882023
399.917694	14492.789474	29.887040
399.979287	14527.292477	29.892058
400.581364	14542.281791	29.897076
400.905930	14570.203105	29.902093
401.540244	14591.702730	29.907111
401.794746	14618.441297	29.912128
402.271592	14651.666738	29.917146
402.855389	14662.272282	29.922164
403.496624	14692.029614	29.927181
403.671679	14717.267987	29.932199
404.225728	14734.197795	29.937216
404.611953	14764.045714	29.942234
404.675756	14779.337445	29.947252
405.504703	14805.522038	29.952269
405.653127	14825.698946	29.957287
406.158615	14845.191460	29.962304
406.733555	14870.105266	29.967322
407.096886	14892.140360	29.972340
407.345245	14916.170544	29.977357
407.558632	14938.304976	29.982375
408.222808	14961.670020	29.987392
408.578221	14980.462942	29.992410
409.543462	15000.006772	29.997428
410.030139	15023.260732	30.002445
410.155035	15047.180931	30.007463
410.627787	15048.108239	30.012480
411.007288	15070.415776	30.017498
411.359692	15096.094292	30.022516
411.738745	15122.517179	30.027533
411.770374	15144.904558	30.032551
412.685703	15165.871283	30.037568
412.727306	15191.042754	30.042586
413.356170	15207.222227	30.047604
414.046825	15226.992481	30.052621
414.034720	15246.136952	30.057639
414.702863	15261.827101	30.062656
414.540409	15293.445161	30.067674
415.167003	15324.042722	30.072692
415.702470	15340.672783	30.077709
415.700269	15366.814629	30.082727
416.687979	15391.459171	30.087744
417.034556	15409.726462	30.092762
417.469963	15428.763119	30.097780
417.740100	15456.656355	30.102797
418.233615	15487.938272	30.107815
418.663562	15507.604370	30.112832
418.935839	15534.439343	30.117850
419.396240	15555.392480	30.122868
419.861862	15577.488144	30.127885
420.028405	15602.195257	30.132903
421.047595	15612.606802	30.137920
421.507808	15637.808041	30.142938
421.084870	15648.878188	30.147956
421.745980	15671.391826	30.152973
422.230971	15697.009323	30.157991
423.054534	15710.954190	30.163008
423.241304	15729.098374	30.168026
423.463255	15758.161876	30.173044
424.261427	15773.358324	30.178061
424.560311	15797.823874	30.183079
425.695698	15808.365771	30.188096
425.518595	15822.085294	30.193114
425.736070	15842.091381	30.198132
426.874046	15856.476657	30.203149
426.963188	15882.658590	30.208167
427.337355	15897.684672	30.213184
427.642622	15912.181471	30.218202
428.151870	15937.782857	30.223220
428.494447	15944.791581	30.228237
428.887065	15966.242180	30.233255
428.894639	15982.273271	30.238272
429.748907	16002.849365	30.243290
430.124061	16026.422064	30.248308
430.723986	16036.681583	30.253325
431.064421	16065.139526	30.258343
431.513970	16077.402954	30.263360
432.136774	16102.178217	30.268378
432.484336	16123.250721	30.273396
433.105527	16142.252672	30.278413
433.254916	16166.334671	30.283431
433.772760	16180.564652	30.288448
434.297920	16204.186717	30.293466
434.267776	16226.594509	30.298484
434.752584	16255.857635	30.303501
435.338695	16263.962216	30.308519
435.934144	16286.638470	30.313536
436.219482	16323.649065	30.318554
436.834981	16352.557071	30.323572
437.178425	16370.301462	30.328589
437.364404	16392.201824	30.333607
438.090820	16412.687839	30.338624
438.561714	16429.692189	30.343642
439.140998	16459.623061	30.348660
439.568635	16471.994404	30.353677
439.834838	16495.167823	30.358695
440.683799	16512.728935	30.363712
441.029429	16540.056026	30.368730
441.604266	16552.088515	30.373748
442.335673	16575.492381	30.378765
442.315362	16582.949834	30.383783
442.711341	16610.177542	30.388800
443.390053	16634.313033	30.393818
443.169929	16658.974681	30.398836
443.910556	16673.602851	30.403853
444.327100	16694.453557	30.408871
444.629745	16728.189984	30.413888
445.424578	16741.445230	30.418906
445.668336	16761.909304	30.423924
446.044049	16781.638901	30.428941
446.272219	16803.681573	30.433959
446.904306	16836.371648	30.438976
447.554952	16852.536470	30.443994
447.417785	16880.719829	30.449012
448.039057	16901.156506	30.454029
448.272674	16931.401257	30.459047
448.977299	16959.730833	30.464064
449.426371	16975.819941	30.469082
449.869789	17012.655488	30.474100
450.432724	17034.601770	30.479117
450.712129	17065.935588	30.484135
451.090701	17076.318779	30.489152
451.240767	17100.578720	30.494170
451.765144	17133.371451	30.499188
452.368824	17148.267806	30.504205
452.626489	17180.615968	30.509223
453.138961	17190.466553	30.514240
453.580256	17227.062787	30.519258
453.796653	17257.440249	30.524276
454.427893	17279.218180	30.529293
455.106257	17304.564321	30.534311
455.248911	17321.346072	30.539328
456.081873	17357.957015	30.544346
456.257216	17384.651820	30.549364
456.688633	17418.280843	30.554381
457.265088	17447.762008	30.559399
458.089941	17472.510550	30.564416
458.206824	17502.872398	30.569434
458.531233	17527.876281	30.574452
459.464751	17556.455164	30.579469
459.663835	17587.581302	30.584487
460.069380	17610.980612	30.589504
460.826414	17638.184806	30.594522
461.049579	17670.703443	30.599540
461.801317	17694.137074	30.604557
462.218411	17719.328843	30.609575
462.300456	17749.658630	30.614592
463.385325	17768.156823	30.619610
463.779796	17794.413558	30.624628
463.914357	17812.593152	30.629645
464.483219	17835.853441	30.634663
464.753133	17858.111888	30.639680
465.473843	17895.152065	30.644698
466.016634	17925.517357	30.649716
466.364595	17948.919779	30.654733
466.944842	17978.597002	30.659751
467.602676	18000.687456	30.664768
467.986769	18024.337009	30.669786
468.470229	18063.120390	30.674804
469.370651	18081.622505	30.679821
469.643197	18107.854539	30.684839
470.148085	18119.020832	30.689856
470.516904	18142.338093	30.694874
470.789053	18169.795874	30.699892
471.483639	18195.203818	30.704909
471.834307	18223.723360	30.709927
472.245542	18239.869990	30.714944
473.364689	18257.068185	30.719962
473.224474	18293.030997	30.724980
474.181898	18307.834937	30.729997
474.417648	18330.017149	30.735015
474.883771	18351.809518	30.740032
475.461763	18371.891271	30.745050
475.587942	18398.058177	30.750068
476.312962	18414.332698	30.755085
476.483282	18434.806886	30.760103
477.137998	18464.700625	30.765120
477.665470	18494.664880	30.770138
477.549421	18521.331080	30.775156
477.981700	18550.760696	30.780173
478.712173	18584.035337	30.785191
479.314723	18608.870696	30.790208
479.558578	18636.093496	30.795226
480.250301	18659.998890	30.800244
481.306268	18690.594571	30.805261
481.602010	18708.440190	30.810279
481.908862	18721.015111	30.815296
482.566586	18742.784227	30.820314
483.075666	18767.729196	30.825332
483.430944	18785.142273	30.830349
484.148644	18798.309938	30.835367
484.536582	18820.986929	30.840384
485.013303	18831.071393	30.845402
485.269943	18850.117322	30.850420
485.932213	18870.325384	30.855437
486.250165	18887.959203	30.860455
486.271877	18907.901202	30.865472
487.195889	18933.021470	30.870490
487.021252	18963.153278	30.875508
488.010891	18984.460022	30.880525
488.214762	19014.444175	30.885543
488.563554	19043.773894	30.890560
488.887344	19071.837690	30.895578
489.507850	19111.669412	30.900596
489.877512	19137.881308	30.905613
490.456381	19168.527199	30.910631
490.743222	19203.988869	30.915648
491.332866	19240.123416	30.920666
491.938091	19262.691073	30.925684
492.383211	19305.122043	30.930701
493.028952	19332.263916	30.935719
493.509775	19355.855715	30.940736
494.045273	19384.019477	30.945754
493.876157	19423.906016	30.950772
494.433991	19453.311014	30.955789
495.573235	19498.154548	30.960807
495.861652	19532.624648	30.965824
496.567561	19564.963436	30.970842
497.254987	19603.806394	30.975860
497.775436	19630.766131	30.980877
498.292913	19658.952067	30.985895
499.038631	19687.639327	30.990912
499.407180	19705.600817	30.995930
499.998352	19743.454562	31.000948
500.368717	19766.798800	31.005965
500.909109	19790.792468	31.010983
501.143592	19813.431467	31.016000
501.774069	19851.209766	31.021018
502.251725	19886.112069	31.026036
502.649109	19919.365346	31.031053
503.092831	19950.052586	31.036071
503.926815	19982.896410	31.041088
504.842501	19999.951120	31.046106
505.206938	20033.885792	31.051124
505.588976	20061.796569	31.056141
506.053212	20083.224720	31.061159
506.697436	20123.579199	31.066176
507.124690	20143.452621	31.071194
507.868338	20181.068513	31.076212
508.205889	20194.979033	31.081229
508.703176	20225.411906	31.086247
508.696964	20267.309106	31.091264
509.586077	20282.201078	31.096282
510.099532	20315.064073	31.101300
510.159652	20345.736196	31.106317
511.069302	20376.212127	31.111335
511.336484	20406.428591	31.116352
511.598297	20438.370830	31.121370
512.424781	20478.994454	31.126388
512.553974	20508.411310	31.131405
513.604519	20531.327695	31.136423
514.083797	20573.775020	31.141440
514.709147	20597.434137	31.146458
515.320543	20628.405776	31.151476
515.409719	20657.614300	31.156493
516.277975	20685.102303	31.161511
516.729350	20710.418939	31.166528
517.392671	20738.400355	31.171546
518.040844	20760.634463	31.176564
518.217711	20781.824060	31.181581
518.587286	20808.967011	31.186599
518.599420	20836.488221	31.191616
519.774559	20863.043833	31.196634
520.247397	20893.083511	31.201652
520.180037	20916.522951	31.206669
520.877155	20948.600030	31.211687
521.328060	20985.176546	31.216704
522.273182	21015.622643	31.221722
522.528277	21047.301549	31.226740
523.104654	21084.420940	31.231757
524.567279	21097.808373	31.236775
524.685002	21117.566981	31.241792
525.435316	21135.122473	31.246810
525.860321	21160.437502	31.251828
526.232230	21182.083507	31.256845
527.161909	21203.553717	31.261863
526.978904	21224.819111	31.266880
527.913698	21246.794049	31.271898
528.475674	21280.560929	31.276916
528.832743	21309.153475	31.281933
529.742668	21332.389795	31.286951
530.173431	21359.511286	31.291968
530.541388	21392.082943	31.296986
531.233291	21419.643827	31.302004
530.990986	21445.348074	31.307021
531.800781	21465.870604	31.312039
532.326463	21506.587697	31.317056
532.686853	21539.280836	31.322074
533.710305	21571.541610	31.327092
533.640798	21604.415923	31.332109
534.724488	21636.376711	31.337127
534.671680	21665.893307	31.342144
535.331191	21693.036297	31.347162
536.211829	21731.132879	31.352180
536.495644	21764.204867	31.357197
537.064616	21800.341052	31.362215
537.267447	21835.732171	31.367232
538.177871	21867.063325	31.372250
539.183409	21900.875533	31.377268
539.323136	21942.311122	31.382285
539.687581	21976.362881	31.387303
540.080166	22010.789417	31.392320
540.798820	22041.139879	31.397338
541.452395	22071.184641	31.402356
541.819871	22115.491566	31.407373
542.780521	22144.268815	31.412391
542.932952	22177.899172	31.417408
543.699830	22217.834333	31.422426
543.934904	22247.553141	31.427444
544.397975	22281.798500	31.432461
545.116290	22311.144732	31.437479
545.704866	22349.755847	31.442496
546.295416	22393.434481	31.447514
547.118906	22431.762527	31.452532
547.795575	22458.581619	31.457549
548.684068	22487.092637	31.462567
548.780470	22519.481201	31.467584
549.461319	22532.372811	31.472602
550.548468	22559.740687	31.477620
550.811727	22582.466828	31.482637
551.556178	22614.956257	31.487655
551.902157	22644.354980	31.492672
552.818398	22658.182927	31.497690
553.000001	22678.982041	31.502708
553.389256	22717.119572	31.507725
553.957441	22735.614955	31.512743
554.174428	22764.193630	31.517760
554.625987	22794.903033	31.522778
555.398217	22811.350761	31.527796
555.851593	22838.003131	31.532813
556.170031	22869.706630	31.537831
556.687134	22905.397985	31.542848
557.575406	22934.863862	31.547866
558.255543	22960.830018	31.552884
558.493270	22979.699658	31.557901
559.258714	23008.464506	31.562919
559.847648	23037.004277	31.567936
560.158872	23072.418542	31.572954
560.598031	23103.920253	31.577972
561.261349	23140.366383	31.582989
561.642819	23166.638669	31.588007
562.077884	23204.188599	31.593024
562.661290	23244.230394	31.598042
563.212759	23271.746346	31.603060
563.706088	23320.687164	31.608077
564.318692	23349.128888	31.613095
565.013722	23394.291012	31.618112
565.374655	23430.317410	31.623130
566.187543	23455.246026	31.628148
567.242258	23507.751896	31.633165
567.779425	23532.995520	31.638183
568.026508	23561.507435	31.643200
568.753078	23606.715655	31.648218
569.411900	23634.183699	31.653236
570.300985	23678.450332	31.658253
570.748226	23703.278544	31.663271
571.228209	23736.026086	31.668288
571.748205	23768.160758	31.673306
572.131524	23798.073523	31.678324
572.580486	23841.790155	31.683341
573.428720	23860.906259	31.688359
573.886642	23911.604535	31.693376
574.400917	23948.328262	31.698394
575.309825	23977.893565	31.703412
575.595943	24011.202750	31.708429
576.926439	24047.110009	31.713447
577.791370	24068.928410	31.718464
578.356133	24093.555439	31.723482
579.114024	24106.676149	31.728500
579.397868	24131.239791	31.733517
580.143722	24159.427985	31.738535
580.814828	24174.856295	31.743552
581.014214	24200.494919	31.748570
581.696425	24233.211604	31.753588
582.319835	24267.201450	31.758605
582.674504	24284.057052	31.763623
583.254033	24312.233595	31.768640
584.046363	24340.225181	31.773658
584.791917	24368.622262	31.778676
584.892238	24405.234714	31.783693
585.558199	24424.973945	31.788711
586.372951	24454.504147	31.793728
586.462524	24477.841051	31.798746
586.964033	24507.540462	31.803764
587.145917	24547.161151	31.808781
587.724487	24577.284647	31.813799
588.527581	24609.970378	31.818816
589.052386	24657.051580	31.823834
589.613168	24689.705875	31.828852
590.036814	24724.467181	31.833869
590.870384	24763.189959	31.838887
591.616767	24789.122846	31.843904
592.001679	24838.254991	31.848922
592.619162	24866.135665	31.853940
592.946685	24896.109368	31.858957
593.538274	24928.563318	31.863975
594.430253	24951.813022	31.868992
594.660876	24987.559289	31.874010
595.517531	25008.059195	31.879028
595.806082	25047.297621	31.884045
596.195446	25086.254907	31.889063
597.703577	25123.071607	31.894080
597.565001	25156.670401	31.899098
598.303535	25185.474207	31.904116
598.874842	25235.342823	31.909133
599.533374	25265.315795	31.914151
600.040596	25299.970210	31.919168
600.654119	25345.269583	31.924186
601.214651	25372.053910	31.929204
601.691783	25411.946056	31.934221
602.585933	25450.249884	31.939239
603.311037	25491.784435	31.944256
604.016161	25519.190940	31.949274
604.909764	25543.584976	31.954292
605.515701	25580.904049	31.959309
606.021497	25614.579646	31.964327
606.678542	25643.712867	31.969344
607.181894	25691.299126	31.974362
607.990426	25724.864295	31.979380
608.359495	25752.083591	31.984397
609.009103	25788.808454	31.989415
610.000098	25824.544562	31.994432
610.179542	25863.940707	31.999450
610.997377	25888.372309	32.004468
611.282885	25929.881811	32.009485
611.917561	25963.860128	32.014503
612.500258	26007.775415	32.019520
613.314184	26047.344311	32.024538
613.668867	26079.742421	32.029556
614.490573	26113.634819	32.034573
614.540188	26147.363789	32.039591
615.443742	26187.588852	32.044608
616.244365	26235.325759	32.049626
617.212252	26277.854086	32.054644
617.997751	26315.064235	32.059661
618.042953	26355.904392	32.064679
619.129928	26385.685531	32.069696
619.658422	26419.118750	32.074714
620.358456	26448.240083	32.079732
620.778549	26493.679772	32.084749
621.260211	26524.611387	32.089767
622.222542	26556.403161	32.094784
622.644377	26594.505046	32.099802
623.542728	26626.319591	32.104820
624.125879	26666.823316	32.109837
624.679984	26708.317631	32.114855
625.410144	26737.763316	32.119872
625.848934	26768.588253	32.124890
626.716430	26809.332144	32.129908
627.182160	26844.678303	32.134925
627.573181	26886.034195	32.139943
628.619899	26919.146909	32.144960
628.613937	26951.116232	32.149978
629.505238	26980.770886	32.154996
630.151367	27018.585629	32.160013
630.586499	27064.049523	32.165031
631.253089	27103.460272	32.170048
631.846533	27145.752009	32.175066
632.308851	27179.361178	32.180084
632.906201	27228.876695	32.185101
633.756911	27265.471620	32.190119
634.525657	27297.680424	32.195136
634.707765	27335.233444	32.200154
635.358807	27370.987608	32.205172
636.311130	27402.756999	32.210189
637.007958	27446.569045	32.215207
637.492754	27479.903411	32.220224
637.874884	27512.463846	32.225242
638.633248	27544.857963	32.230260
639.308120	27575.489140	32.235277
639.762504	27618.991899	32.240295
640.961456	27653.074297	32.245312
641.428102	27702.118434	32.250330
641.594238	27728.259749	32.255348
642.464627	27771.090907	32.260365
642.972680	27812.474600	32.265383
643.754937	27849.511099	32.270400
644.833021	27893.068461	32.275418
645.374671	27935.546930	32.280436
646.154962	27971.812842	32.285453
646.564271	27998.143964	32.290471
647.236479	28040.172400	32.295488
647.815798	28082.474618	32.300506
648.395686	28118.917553	32.305524
649.217248	28163.703958	32.310541
649.727475	28206.788380	32.315559
650.424879	28242.246061	32.320576
651.332282	28284.560525	32.325594
651.890645	28322.423041	32.330612
652.670592	28359.859038	32.335629
653.304493	28397.381184	32.340647
654.233573	28437.594072	32.345664
654.732063	28465.959766	32.350682
655.842682	28500.828559	32.355700
656.025697	28534.034928	32.360717
656.613890	28564.655885	32.365735
657.570213	28605.812963	32.370752
658.007415	28644.687424	32.375770
658.631100	28673.906078	32.380788
659.334105	28720.128145	32.385805
659.489113	28769.849417	32.390823
660.662384	28802.288012	32.395840
661.156897	28843.796013	32.400858
661.891121	28891.157662	32.405876
662.487322	28921.689407	32.410893
663.279375	28965.919629	32.415911
664.578206	28993.364276	32.420928
665.439916	29020.264283	32.425946
665.666904	29051.005746	32.430964
666.759883	29074.039093	32.435981
667.376812	29104.371914	32.440999
668.280726	29131.922842	32.446016
668.983281	29162.368760	32.451034
669.523010	29196.803505	32.456052
670.498880	29226.909628	32.461069
670.963850	29248.530796	32.466087
671.536347	29274.130049	32.471104
672.033439	29301.947191	32.476122
672.588538	29334.003042	32.481140
673.384435	29378.359975	32.486157
673.874547	29411.557598	32.491175
674.486768	29425.583229	32.496192
674.484760	29470.691107	32.501210
675.503528	29498.799764	32.506228
676.792618	29540.734677	32.511245
676.834412	29569.533728	32.516263
677.625285	29601.211731	32.521280
677.983833	29647.597293	32.526298
678.834455	29672.742613	32.531316
679.417670	29710.881936	32.536333
680.298223	29750.479210	32.541351
681.053025	29786.897723	32.546368
681.359284	29807.741543	32.551386
681.919528	29834.715118	32.556404
682.523325	29883.249946	32.561421
683.219254	29924.045895	32.566439
683.695526	29956.197238	32.571456
684.564035	29998.445482	32.576474
685.394115	30032.090247	32.581492
685.557562	30073.140556	32.586509
686.113101	30119.426796	32.591527
687.152550	30151.825278	32.596544
687.939433	30196.292851	32.601562
688.378935	30241.447055	32.606580
689.350894	30282.143594	32.611597
689.639085	30331.847784	32.616615
690.524422	30378.721417	32.621632
691.090516	30426.264649	32.626650
691.736172	30473.176031	32.631668
692.609044	30509.779619	32.636685
693.106508	30561.442836	32.641703
693.765484	30601.487340	32.646720
694.638229	30654.255167	32.651738
695.346260	30704.868010	32.656756
696.247344	30749.508535	32.661773
696.614654	30797.772795	32.666791
697.890698	30848.474039	32.671808
698.263463	30894.423991	32.676826
698.922142	30946.265211	32.681844
699.857790	30987.531447	32.686861
700.576135	31026.574991	32.691879
701.185725	31078.677093	32.696896
701.904263	31130.661120	32.701914
702.816392	31176.040465	32.706932
703.528438	31204.079377	32.711949
704.055573	31261.321700	32.716967
704.787372	31299.693556	32.721984
705.933104	31343.519486	32.727002
706.802644	31388.634134	32.732020
707.138981	31428.439967	32.737037
707.817448	31482.435131	32.742055
708.478103	31515.786439	32.747072
709.294356	31564.835611	32.752090
710.010431	31611.068439	32.757108
710.906542	31655.484113	32.762125
711.519296	31697.889676	32.767143
711.872567	31736.062424	32.772160
712.953919	31776.428685	32.777178
713.761959	31833.780318	32.782196
714.574857	31860.375592	32.787213
715.313799	31916.328504	32.792231
716.501471	31947.707740	32.797248
716.680438	31991.281837	32.802266
717.669587	32034.830300	32.807284
718.553963	32064.126733	32.812301
719.040916	32106.881569	32.817319
719.678090	32136.153596	32.822336
720.236214	32182.627375	32.827354
721.106498	32228.533974	32.832372
721.811722	32264.768635	32.837389
722.649134	32312.855321	32.842407
723.062286	32344.286907	32.847424
724.121590	32379.473767	32.852442
724.606180	32427.843562	32.857460
725.325528	32462.919429	32.862477
726.135552	32507.818235	32.867495
727.079303	32534.001915	32.872512
727.560973	32562.451740	32.877530
728.180056	32605.623129	32.882548
728.870714	32625.505531	32.887565
729.298300	32668.479444	32.892583
730.226662	32705.710428	32.897600
731.089606	32738.892933	32.902618
731.577958	32774.618742	32.907636
732.243186	32818.750628	32.912653
732.809945	32859.629482	32.917671
733.630589	32903.111316	32.922688
734.312864	32949.681160	32.927706
734.926920	32993.498998	32.932724
735.691990	33033.872973	32.937741
736.391875	33087.337877	32.942759
737.037172	33131.410322	32.947776
738.177105	33166.598530	32.952794
738.289426	33206.461802	32.957812
739.357588	33260.185587	32.962829
739.801075	33306.635562	32.967847
740.615648	33361.461461	32.972864
741.716440	33413.536734	32.977882
742.287196	33451.634304	32.982900
743.688473	33494.356275	32.987917
744.038360	33541.137543	32.992935
744.911835	33591.187772	32.997952
745.613893	33626.628674	33.002970
746.271739	33686.051038	33.007988
747.678986	33713.023460	33.013005
748.789564	33767.949483	33.018023
749.216127	33800.601381	33.023040
750.183233	33839.592273	33.028058
750.598656	33888.943605	33.033076
751.395561	33914.323773	33.038093
752.222339	33963.313707	33.043111
753.002662	33990.074862	33.048128
753.792987	34032.071683	33.053146
754.359843	34074.173130	33.058164
754.813856	34115.539953	33.063181
755.917218	34157.051749	33.068199
756.469827	34203.170491	33.073216
757.319946	34245.480824	33.078234
758.118901	34296.461173	33.083252
759.084544	34336.749344	33.088269
759.593305	34382.932249	33.093287
760.495615	34422.718373	33.098304
761.208759	34466.176023	33.103322
761.576378	34505.059705	33.108340
762.462230	34552.429488	33.113357
763.524262	34601.927816	33.118375
764.188066	34651.279974	33.123392
764.980452	34690.963686	33.128410
765.557087	34739.785950	33.133428
766.575289	34769.988334	33.138445
767.281128	34817.361611	33.143463
768.112728	34860.283061	33.148480
769.161121	34901.027236	33.153498
769.745082	34942.527076	33.158516
770.425818	34980.831488	33.163533
771.182338	35033.862521	33.168551
771.655119	35081.601671	33.173568
772.652928	35122.575493	33.178586
773.265923	35170.912524	33.183604
774.175572	35208.182494	33.188621
774.748268	35257.632531	33.193639
775.379120	35304.645593	33.198656
776.351806	35344.340237	33.203674
776.873135	35412.748368	33.208692
777.647455	35451.285570	33.213709
778.678840	35492.204267	33.218727
779.219661	35530.664365	33.223744
779.953020	35568.209170	33.228762
780.560056	35609.175576	33.233780
781.403546	35644.332159	33.238797
782.233492	35694.552271	33.243815
782.431992	35743.025066	33.248832
783.581289	35796.546602	33.253850
784.419741	35845.671858	33.258868
784.997717	35895.799119	33.263885
785.860690	35945.742762	33.268903
786.225688	35998.559303	33.273920
787.452726	36044.898923	33.278938
788.433806	36105.744428	33.283956
789.116727	36158.720244	33.288973
790.517634	36198.564417	33.293991
790.638972	36255.270540	33.299008
791.606140	36300.140178	33.304026
792.583386	36349.358680	33.309044
793.429774	36402.891238	33.314061
794.306573	36450.184481	33.319079
794.941162	36504.035004	33.324096
795.853375	36548.844216	33.329114
796.675129	36596.664910	33.334132
797.743436	36641.728097	33.339149
798.438440	36692.951804	33.344167
798.775976	36739.716776	33.349184
799.808768	36785.784910	33.354202
800.546459	36833.733119	33.359220
801.448736	36894.169552	33.364237
802.831966	36928.288915	33.369255
803.437748	36985.230959	33.374272
804.510613	37024.691738	33.379290
805.241088	37072.496175	33.384308
806.078966	37113.935199	33.389325
806.956096	37155.526242	33.394343
807.632015	37200.291620	33.399360
808.315642	37245.549113	33.404378
809.612256	37288.396327	33.409396
809.958091	37336.653640	33.414413
810.835531	37372.503345	33.419431
811.746335	37432.743938	33.424448
812.685508	37482.672925	33.429466
813.377692	37524.603499	33.434484
814.108852	37559.932600	33.439501
814.946145	37603.908404	33.444519
815.751786	37654.465762	33.449536
816.845940	37707.355728	33.454554
817.332557	37752.151902	33.459572
818.015922	37804.878784	33.464589
818.776595	37842.246256	33.469607
819.203567	37895.026155	33.474624
820.493761	37952.148158	33.479642
821.017479	37998.406123	33.484660
822.224753	38051.620702	33.489677
823.557848	38090.890931	33.494695
824.620624	38128.401306	33.499712
825.347402	38162.264986	33.504730
826.214428	38204.466725	33.509748
827.008760	38241.203572	33.514765
828.160972	38279.541263	33.519783
828.384026	38324.569614	33.524800
829.480633	38358.084799	33.529818
830.436549	38403.068116	33.534836
830.753345	38452.318991	33.539853
832.103927	38483.808929	33.544871
832.635764	38519.480689	33.549888
833.756718	38570.110980	33.554906
834.038726	38603.412618	33.559924
834.332355	38629.806840	33.564941
835.198145	38671.984395	33.569959
835.803077	38715.790172	33.574976
836.901860	38760.081533	33.579994
837.335839	38810.965412	33.585012
837.653125	38851.091727	33.590029
838.732674	38900.774367	33.595047
839.490479	38965.963232	33.600064
840.341605	39014.733310	33.605082
841.252504	39078.077239	33.610100
842.099519	39138.952348	33.615117
842.600071	39190.825887	33.620135
843.649065	39258.689365	33.625152
844.244426	39310.086689	33.630170
845.353324	39370.352277	33.635188
846.179689	39427.430666	33.640205
847.440301	39473.152689	33.645223
848.611570	39535.091179	33.650240
849.786893	39589.364362	33.655258
850.445649	39636.521691	33.660276
850.955101	39690.842478	33.665293
852.038894	39739.495542	33.670311
853.043192	39802.713129	33.675328
853.607664	39837.711588	33.680346
855.050103	39891.716031	33.685364
855.485029	39948.528226	33.690381
856.787855	40003.655226	33.695399
857.455414	40061.626574	33.700416
858.359066	40104.376501	33.705434
859.313403	40154.524325	33.710452
860.110910	40208.396545	33.715469
861.177094	40249.812176	33.720487
861.796280	40303.535473	33.725504
862.703227	40350.484730	33.730522
863.903198	40404.212198	33.735540
864.583568	40462.834018	33.740557
865.268073	40502.444202	33.745575
865.808642	40559.095986	33.750592
866.838485	40608.341292	33.755610
868.282865	40661.670632	33.760628
868.876597	40715.190223	33.765645
869.824194	40759.148852	33.770663
870.682075	40811.014576	33.775680
871.393689	40860.936406	33.780698
872.497797	40906.591090	33.785716
873.251230	40970.907546	33.790733
874.247228	41018.704436	33.795751
875.150981	41060.981885	33.800768
875.777113	41116.382103	33.805786
876.714751	41174.307793	33.810804
877.643695	41233.291208	33.815821
878.761800	41277.679555	33.820839
879.410024	41330.622903	33.825856
880.330959	41379.425304	33.830874
880.896602	41425.570166	33.835892
881.542539	41492.131267	33.840909
882.733908	41537.501645	33.845927
883.447968	41596.380542	33.850944
884.352769	41651.264124	33.855962
885.763936	41707.219659	33.860980
886.740949	41759.581282	33.865997
887.963880	41792.196535	33.871015
888.724557	41835.269506	33.876032
889.580647	41882.286943	33.881050
891.007279	41927.595993	33.886068
891.533691	41980.895200	33.891085
892.276646	42013.004055	33.896103
893.182995	42058.426467	33.901120
893.481296	42097.157611	33.906138
894.221202	42128.501804	33.911156
895.243181	42174.431315	33.916173
896.336806	42217.674273	33.921191
897.384550	42271.430169	33.926208
897.801479	42322.729703	33.931226
898.786650	42349.867685	33.936244
899.480610	42403.489552	33.941261
900.382940	42441.968599	33.946279
901.163220	42494.090806	33.951296
902.091926	42558.947394	33.956314
902.885889	42600.916106	33.961332
903.738797	42658.296055	33.966349
904.631088	42701.413366	33.971367
905.407860	42773.485935	33.976384
906.465179	42826.248653	33.981402
907.713164	42881.239697	33.986420
908.045280	42940.966307	33.991437
908.984540	42996.391809	33.996455
910.111251	43056.177739	34.001472
911.046011	43124.064778	34.006490
912.225371	43171.888247	34.011508
912.581834	43234.103949	34.016525
913.886979	43298.264922	34.021543
914.967550	43358.798944	34.026560
915.659870	43412.809356	34.031578
916.805431	43469.373909	34.036596
917.268892	43529.606535	34.041613
918.483671	43590.088548	34.046631
919.708454	43643.478501	34.051648
920.648772	43712.384845	34.056666
921.658059	43767.206733	34.061684
922.379913	43834.439824	34.066701
923.486914	43887.361754	34.071719
924.525596	43934.595338	34.076736
925.193278	43994.949058	34.081754
926.422467	44039.180099	34.086772
927.486103	44112.224171	34.091789
928.115873	44171.015597	34.096807
929.422522	44214.747800	34.101824
930.227910	44271.076691	34.106842
931.201586	44315.942887	34.111860
932.193879	44377.771261	34.116877
933.475746	44426.397379	34.121895
934.373915	44480.827268	34.126912
935.217252	44533.115189	34.131930
936.055883	44576.763248	34.136948
937.017930	44636.775315	34.141965
937.892703	44699.755263	34.146983
938.972343	44743.498749	34.152000
939.409629	44795.553560	34.157018
941.054888	44860.203472	34.162036
941.673720	44913.438330	34.167053
942.436851	44962.349262	34.172071
943.511964	45018.637809	34.177088
944.421656	45075.059936	34.182106
945.550679	45128.487427	34.187124
946.385968	45187.508707	34.192141
947.106240	45235.300967	34.197159
948.193163	45283.504026	34.202176
948.967401	45345.521042	34.207194
950.259058	45397.582646	34.212212
950.850720	45459.198410	34.217229
951.941484	45510.513657	34.222247
953.314080	45565.460208	34.227264
953.839454	45617.743520	34.232282
954.677418	45659.015276	34.237300
955.560320	45711.489535	34.242317
956.445579	45763.558690	34.247335
957.218152	45823.382202	34.252352
958.114956	45876.031795	34.257370
959.575736	45918.136423	34.262388
960.271121	45971.070813	34.267405
961.554684	46011.514334	34.272423
962.021243	46069.216609	34.277440
963.078059	46121.025670	34.282458
964.210211	46167.983656	34.287476
965.009784	46223.761686	34.292493
965.409567	46274.813637	34.297511
966.842045	46331.049527	34.302528
967.782316	46395.782630	34.307546
968.625823	46451.465780	34.312564
969.719033	46513.575252	34.317581
970.611435	46564.822751	34.322599
971.940121	46619.677542	34.327616
972.651285	46693.190095	34.332634
973.729010	46744.592445	34.337652
974.665709	46798.471554	34.342669
975.621057	46861.514541	34.347687
976.879483	46910.282579	34.352704
977.496166	46980.521227	34.357722
978.933898	47026.427286	34.362740
979.863593	47092.644388	34.367757
980.779430	47140.131720	34.372775
981.897263	47193.135688	34.377792
982.753581	47265.045799	34.382810
984.057044	47315.022314	34.387828
984.588350	47377.981303	34.392845
985.573819	47445.405363	34.397863
986.409391	47499.048920	34.402880
987.288207	47566.439428	34.407898
988.395648	47624.386953	34.412916
989.418311	47689.730851	34.417933
990.455758	47757.780345	34.422951
991.904128	47817.446391	34.427968
992.891440	47891.153675	34.432986
993.843577	47939.294955	34.438004
994.967197	48006.256195	34.443021
996.041469	48060.939216	34.448039
997.369002	48113.286177	34.453056
998.205359	48175.788388	34.458074
999.208521	48226.035362	34.463092
1000.214139	48295.470645	34.468109
1000.971499	48355.530996	34.473127
1002.035830	48402.630778	34.478144
1002.721054	48466.732783	34.483162
1003.700457	48526.259013	34.488180
1005.088590	48590.010895	34.493197
1006.210665	48651.590268	34.498215
1007.125024	48701.852195	34.503232
1008.095036	48774.609713	34.508250
1009.302275	48829.374989	34.513268
1010.049183	48880.296203	34.518285
1010.916799	48946.212086	34.523303
1011.933842	48992.491683	34.528320
1013.022042	49066.402082	34.533338
1014.193008	49127.949777	34.538356
1015.267250	49181.186647	34.543373
1016.114434	49250.156146	34.548391
1017.666252	49296.048939	34.553408
1018.295512	49361.623725	34.558426
1019.521935	49408.693879	34.563444
1020.796780	49465.632881	34.568461
1021.111531	49518.337775	34.573479
1022.306828	49574.777021	34.578496
1022.989969	49619.528427	34.583514
1024.496836	49668.092660	34.588532
1025.576086	49708.846839	34.593549
1026.590971	49747.548564	34.598567
1027.782624	49799.724534	34.603584
1028.944466	49853.455414	34.608602
1029.884760	49876.155317	34.613620
1030.931477	49929.543759	34.618637
1031.367836	49980.870357	34.623655
1032.199542	50025.434790	34.628672
1032.923723	50098.323580	34.633690
1034.115930	50147.747966	34.638708
1035.189785	50205.852829	34.643725
1036.371935	50265.952916	34.648743
1037.303834	50325.307774	34.653760
1038.173179	50391.885564	34.658778
1039.170471	50443.960558	34.663796
1040.408725	50505.925338	34.668813
1040.804233	50568.003249	34.673831
1042.066234	50639.291008	34.678848
1043.192862	50705.532041	34.683866
1044.209936	50769.727721	34.688884
1045.170014	50844.227027	34.693901
1046.334380	50914.202188	34.698919
1047.816493	50971.327599	34.703936
1048.397807	51052.100325	34.708954
1049.627873	51121.951936	34.713972
1050.639507	51186.339446	34.718989
1051.664588	51254.825196	34.724007
1053.251851	51316.883040	34.729024
1054.431721	51378.751736	34.734042
1055.420040	51444.636893	34.739060
1056.380977	51506.774325	34.744077
1057.458242	51579.821310	34.749095
1058.603482	51640.860898	34.754112
1059.637765	51701.354866	34.759130
1060.969858	51762.662914	34.764148
1062.368035	51826.080514	34.769165
1063.022212	51897.201553	34.774183
1064.535234	51952.578133	34.779200
1065.164269	52009.877635	34.784218
1066.282941	52063.468554	34.789236
1067.620550	52126.744595	34.794253
1068.459013	52201.140746	34.799271
1070.312432	52253.591986	34.804288
1071.049356	52321.942495	34.809306
1072.443952	52375.022682	34.814324
1073.674930	52411.081693	34.819341
1074.840954	52467.754064	34.824359
1075.901354	52516.640980	34.829376
1076.873640	52565.320322	34.834394
1078.141566	52627.381046	34.839412
1078.852632	52676.930460	34.844429
1080.000281	52731.682697	34.849447
1081.274831	52783.118394	34.854464
1081.932851	52829.898519	34.859482
1082.991860	52891.113083	34.864500
1084.346367	52946.643405	34.869517
1085.255073	53008.951221	34.874535
1086.211889	53060.260093	34.879552
1087.380073	53114.054499	34.884570
1088.160804	53170.668668	34.889588
1089.509914	53227.168677	34.894605
1090.346724	53282.249300	34.899623
1091.778547	53341.634844	34.904640
1092.577408	53400.758941	34.909658
1093.771630	53463.668721	34.914676
1094.649720	53513.699997	34.919693
1095.317816	53573.129762	34.924711
1096.695762	53620.260700	34.929728
1097.907168	53675.967031	34.934746
1098.371542	53715.476647	34.939764
1099.758281	53776.914324	34.944781
1100.595940	53842.867808	34.949799
1101.391706	53888.457777	34.954816
1102.158847	53952.998781	34.959834
1103.085213	54014.585093	34.964852
1104.662520	54085.340441	34.969869
1105.738332	54161.401610	34.974887
1107.110800	54222.646513	34.979904
1107.857356	54287.944715	34.984922
1108.889324	54342.402414	34.989940
1110.407033	54413.649026	34.994957
1111.948343	54482.911405	34.999975
1113.468387	54542.216563	35.004992
1114.593724	54595.084481	35.010010
1115.293679	54652.917245	35.015028
1116.881899	54698.169553	35.020045
1117.757341	54771.353019	35.025063
1119.059853	54823.744397	35.030080
1120.062396	54882.074590	35.035098
1121.228275	54942.606956	35.040116
1122.223862	55002.818074	35.045133
1123.460145	55067.630411	35.050151
1124.887915	55123.983438	35.055168
1126.121892	55187.847197	35.060186
1126.782536	55244.750947	35.065204
1128.511207	55295.114820	35.070221
1129.553835	55355.591596	35.075239
1131.022342	55423.969482	35.080256
1132.260339	55481.593465	35.085274
1133.100773	55536.254772	35.090292
1134.693506	55579.223450	35.095309
1135.364140	55645.480242	35.100327
1136.429260	55685.582588	35.105344
1137.395312	55753.362925	35.110362
1138.295531	55806.882671	35.115380
1139.735027	55869.703509	35.120397
1140.518902	55950.157590	35.125415
1141.749776	55998.468127	35.130432
1142.539652	56075.978852	35.135450
1143.741336	56146.963721	35.140468
1145.144159	56206.582522	35.145485
1145.905061	56277.060870	35.150503
1147.229859	56343.805764	35.155520
1148.427635	56404.153328	35.160538
1149.947040	56473.481913	35.165556
1151.062274	56543.962534	35.170573
1152.160043	56618.388975	35.175591
1153.274431	56670.782239	35.180608
1154.519365	56737.629342	35.185626
1155.736481	56808.037833	35.190644
1156.885182	56860.299562	35.195661
1158.029788	56935.403180	35.200679
1159.163517	56998.262203	35.205696
1160.770755	57066.888903	35.210714
1161.493278	57122.546966	35.215732
1163.024484	57184.407561	35.220749
1164.149926	57250.983670	35.225767
1165.280849	57306.179495	35.230784
1166.643470	57364.275853	35.235802
1167.753613	57424.032121	35.240820
1168.955593	57476.223563	35.245837
1170.027586	57538.682278	35.250855
1171.336807	57607.629334	35.255872
1172.697616	57662.543153	35.260890
1173.575928	57710.690830	35.265908
1174.635121	57748.424142	35.270925
1175.312722	57800.166734	35.275943
1176.232811	57851.327164	35.280960
1177.382023	57902.806268	35.285978
1178.647907	57961.216688	35.290996
1180.048500	58014.169358	35.296013
1180.938463	58072.664217	35.301031
1181.914241	58135.645883	35.306048
1183.130772	58196.798839	35.311066
1184.111739	58261.912986	35.316084
1185.711294	58325.215227	35.321101
1186.641224	58383.919779	35.326119
1188.231795	58450.590954	35.331136
1189.109332	58506.025409	35.336154
1190.394441	58576.086649	35.341172
1191.939446	58641.803421	35.346189
1193.107752	58708.674331	35.351207
1194.268038	58761.887793	35.356224
1195.510661	58820.101393	35.361242
1196.981997	58879.076839	35.366260
1198.049543	58936.526947	35.371277
1199.551443	58998.574019	35.376295
1200.613241	59073.577006	35.381312
1201.967781	59123.349252	35.386330
1203.049848	59184.108009	35.391348
1203.901580	59252.530079	35.396365
1205.467799	59319.523939	35.401383
1206.615931	59385.994784	35.406400
1208.159468	59431.218756	35.411418
1208.880400	59505.915653	35.416436
1210.837358	59561.500020	35.421453
1211.445759	59631.315789	35.426471
1212.971142	59697.848692	35.431488
1214.184340	59758.733940	35.436506
1215.474203	59825.215446	35.441524
1216.830973	59878.052465	35.446541
1218.235606	59940.262755	35.451559
1219.182188	59999.133182	35.456576
1220.421037	60057.027522	35.461594
1221.678935	60122.059000	35.466612
1223.297871	60183.388173	35.471629
1224.624990	60242.661689	35.476647
1225.230512	60294.636099	35.481664
1226.706928	60346.911040	35.486682
1227.602811	60412.943110	35.491700
1228.908412	60476.550178	35.496717
1230.514147	60544.155220	35.501735
1231.275084	60599.308866	35.506752
1232.868938	60660.567207	35.511770
1233.602819	60744.437905	35.516788
1235.127008	60799.921944	35.521805
1236.215833	60866.482066	35.526823
1237.238644	60938.888947	35.531840
1238.491723	61008.607723	35.536858
1239.802837	61072.101535	35.541876
1241.167858	61131.168711	35.546893
1242.084543	61199.231581	35.551911
1243.189463	61278.045277	35.556928
1244.744170	61348.015312	35.561946
1245.853699	61413.763425	35.566964
1247.464303	61487.415557	35.571981
1248.773636	61562.773569	35.576999
1249.617014	61629.785641	35.582016
1250.952418	61688.782831	35.587034
1252.158792	61769.386317	35.592052
1253.153833	61828.152265	35.597069
1254.832140	61893.154276	35.602087
1255.499131	61953.326545	35.607104
1257.453494	62009.853769	35.612122
1258.481110	62075.458214	35.617140
1259.571141	62132.114694	35.622157
1260.907134	62180.161573	35.627175
1262.086464	62251.655237	35.632192
1263.003878	62301.660644	35.637210
1264.429623	62361.506226	35.642228
1265.442067	62423.499342	35.647245
1266.624048	62488.454012	35.652263
1267.571932	62563.713401	35.657280
1269.455038	62625.146589	35.662298
1270.703580	62699.612336	35.667316
1271.942115	62767.831719	35.672333
1273.385175	62819.452446	35.677351
1274.683622	62894.531351	35.682368
1276.066667	62955.511880	35.687386
1277.674457	63033.992903	35.692404
1278.947446	63089.394813	35.697421
1279.787942	63160.709910	35.702439
1281.401280	63237.633393	35.707456
1282.555872	63303.708664	35.712474
1283.718704	63352.025487	35.717492
1284.954028	63425.970040	35.722509
1286.486331	63500.912879	35.727527
1288.072888	63570.763934	35.732544
1289.444561	63630.120920	35.737562
1290.592454	63692.887333	35.742580
1292.034650	63771.928383	35.747597
1293.534420	63829.759085	35.752615
1294.455808	63891.067404	35.757632
1296.413006	63952.599903	35.762650
1297.910281	64018.933633	35.767668
1299.423574	64077.813700	35.772685
1300.429995	64128.948390	35.777703
1301.418758	64201.623363	35.782720
1303.061101	64257.514502	35.787738
1304.414706	64329.518645	35.792756
1305.922925	64380.549974	35.797773
1307.268002	64446.383202	35.802791
1307.997645	64506.988664	35.807808
1309.636286	64567.376007	35.812826
1310.638522	64630.863975	35.817844
1311.972645	64700.143605	35.822861
1313.229482	64755.114908	35.827879
1314.678032	64824.794812	35.832896
1315.475493	64897.178867	35.837914
1316.977920	64969.440113	35.842932
1318.331678	65043.915373	35.847949
1319.542941	65112.126435	35.852967
1321.025140	65183.973615	35.857984
1321.940235	65243.906054	35.863002
1323.237584	65319.669837	35.868020
1324.761635	65391.029893	35.873037
1326.270651	65464.905963	35.878055
1327.314182	65545.078635	35.883072
1328.649734	65596.215439	35.888090
1330.056142	65678.876859	35.893108
1331.397104	65757.148608	35.898125
1332.937138	65824.677011	35.903143
1334.233169	65903.222157	35.908160
1335.389255	65972.102629	35.913178
1336.949762	66040.546436	35.918196
1338.065629	66120.519669	35.923213
1339.651886	66179.735130	35.928231
1340.775960	66260.562246	35.933248
1341.912325	66333.194933	35.938266
1343.558248	66401.556700	35.943284
1344.893123	66462.021461	35.948301
1346.137825	66516.688263	35.953319
1347.285018	66584.102906	35.958336
1348.263684	66633.493221	35.963354
1349.936315	66698.533945	35.968372
1350.958614	66767.557815	35.973389
1352.376737	66829.264047	35.978407
1353.386518	66903.095830	35.983424
1355.051890	66967.657186	35.988442
1356.508219	67042.217241	35.993460
1357.343618	67113.196087	35.998477
1358.891478	67182.284438	36.003495
1360.183114	67266.944439	36.008512
1361.694710	67336.203504	36.013530
1362.940854	67416.641618	36.018548
1363.878764	67487.795405	36.023565
1365.491298	67571.583072	36.028583
1367.159428	67657.553070	36.033600
1368.567430	67730.685410	36.038618
1369.645799	67804.990271	36.043636
1371.066453	67887.764276	36.048653
1372.534703	67963.287575	36.053671
1373.849284	68051.802616	36.058688
1375.367801	68128.546897	36.063706
1377.341478	68211.298698	36.068724
1378.258563	68300.104760	36.073741
1380.031802	68367.438774	36.078759
1381.573900	68449.701697	36.083776
1383.201499	68538.561992	36.088794
1384.795562	68602.283832	36.093812
1386.047969	68672.644509	36.098829
1387.753380	68738.711065	36.103847
1388.817707	68817.605375	36.108864
1390.557599	68892.341713	36.113882
1391.862636	68957.945948	36.118900
1393.088940	69024.569464	36.123917
1395.031258	69103.149918	36.128935
1396.373963	69172.788639	36.133952
1397.768470	69242.723377	36.138970
1399.004625	69311.701619	36.143988
1400.155278	69381.434284	36.149005
1401.883550	69443.832786	36.154023
1403.237843	69521.854350	36.159040
1404.570960	69582.763668	36.164058
1406.269997	69658.445777	36.169076
1407.458645	69734.176337	36.174093
1409.027214	69805.738051	36.179111
1410.440876	69875.475202	36.184128
1411.486963	69950.145898	36.189146
1413.186062	70008.580016	36.194164
1414.427541	70086.931219	36.199181
1416.004175	70162.304680	36.204199
1417.276670	70244.615514	36.209216
1418.614190	70314.581061	36.214234
1420.446093	70386.445102	36.219252
1421.822388	70461.242882	36.224269
1423.197750	70518.956276	36.229287
1424.888200	70591.868870	36.234304
1425.894310	70662.583790	36.239322
1427.865897	70730.690797	36.244340
1428.330416	70807.709324	36.249357
1429.949810	70871.933048	36.254375
1431.766084	70939.912934	36.259392
1433.225373	71029.086738	36.264410
1435.025135	71078.844652	36.269428
1436.388709	71152.126602	36.274445
1437.695384	71202.987803	36.279463
1439.302994	71272.824988	36.284480
1440.598755	71320.977794	36.289498
1442.175988	71376.166455	36.294516
1443.176514	71432.788011	36.299533
1444.807465	71483.624332	36.304551
1446.032062	71543.972624	36.309568
1447.053409	71596.069784	36.314586
1448.874958	71650.359544	36.319604
1449.989552	71714.322389	36.324621
1451.364681	71779.359162	36.329639
1452.669765	71846.965467	36.334656
1453.713413	71914.460882	36.339674
1455.165120	71983.336460	36.344692
1456.083171	72065.341201	36.349709
1457.698767	72136.749957	36.354727
1459.563141	72212.084288	36.359744
1460.981246	72295.214702	36.364762
1462.935730	72371.054673	36.369780
1464.240603	72448.288441	36.374797
1466.163021	72527.958917	36.379815
1467.072222	72593.703914	36.384832
1468.689651	72675.854397	36.389850
1470.310275	72736.118103	36.394868
1471.166456	72824.721108	36.399885
1472.862449	72900.299079	36.404903
1474.460827	72987.013231	36.409920
1475.724314	73075.591318	36.414938
1477.752147	73153.790594	36.419956
1478.896393	73247.175670	36.424973
1480.569470	73315.247442	36.429991
1482.211278	73394.571801	36.435008
1483.457070	73484.572628	36.440026
1485.345507	73564.010883	36.445044
1486.706647	73638.541410	36.450061
1488.470274	73735.656460	36.455079
1489.831516	73817.356591	36.460096
1491.617936	73899.991066	36.465114
1493.096381	73963.813733	36.470132
1494.637231	74052.060330	36.475149
1496.116466	74125.991080	36.480167
1497.736650	74202.243278	36.485184
1499.324350	74290.445331	36.490202
1500.988901	74366.855719	36.495220
1501.859002	74434.790038	36.500237
1503.752845	74524.034273	36.505255
1505.156019	74593.240891	36.510272
1506.718595	74677.901480	36.515290
1508.410059	74757.969459	36.520308
1509.936674	74847.753588	36.525325
1511.741198	74912.654830	36.530343
1513.262045	74980.387343	36.535360
1515.001669	75059.562004	36.540378
1516.506784	75126.892007	36.545396
1517.715490	75212.572358	36.550413
1519.271553	75286.304282	36.555431
1521.161136	75353.777350	36.560448
1522.151512	75432.361025	36.565466
1523.836136	75496.180409	36.570484
1525.101728	75571.693973	36.575501
1526.691085	75641.925526	36.580519
1528.159369	75727.452881	36.585536
1529.612349	75802.203062	36.590554
1531.059852	75875.852252	36.595572
1532.565986	75959.068969	36.600589
1534.593387	76031.956453	36.605607
1536.044406	76102.958233	36.610624
1537.106694	76183.660960	36.615642
1538.892758	76246.288171	36.620660
1540.519547	76328.575082	36.625677
1541.789092	76390.358743	36.630695
1543.168106	76448.895182	36.635712
1544.493639	76525.985475	36.640730
1546.282322	76593.426767	36.645748
1547.492446	76661.972193	36.650765
1548.923959	76722.135134	36.655783
1550.523845	76784.628051	36.660800
1552.096954	76857.132825	36.665818
1553.690079	76915.079378	36.670836
1555.374700	76987.199680	36.675853
1556.982542	77066.236167	36.680871
1558.870518	77133.321229	36.685888
1560.251407	77209.480041	36.690906
1562.209191	77269.447815	36.695924
1563.720551	77343.547042	36.700941
1565.217073	77412.834950	36.705959
1566.614732	77482.721237	36.710976
1568.042014	77564.131016	36.715994
1569.734841	77640.786937	36.721012
1571.321613	77719.486576	36.726029
1572.516600	77784.097400	36.731047
1574.099926	77852.042678	36.736064
1575.584728	77941.476224	36.741082
1577.148136	78032.050573	36.746100
1578.612469	78118.460178	36.751117
1580.505981	78206.804486	36.756135
1582.014298	78301.505569	36.761152
1583.521041	78381.258444	36.766170
1585.500821	78457.225648	36.771188
1586.848529	78547.480739	36.776205
1588.452785	78635.491641	36.781223
1590.306991	78715.482481	36.786240
1591.818599	78802.456924	36.791258
1593.540328	78888.587958	36.796276
1595.459578	78976.652000	36.801293
1596.759157	79056.730636	36.806311
1598.558266	79139.201738	36.811328
1600.066420	79232.347783	36.816346
1601.727913	79314.828279	36.821364
1603.474829	79405.986532	36.826381
1604.770333	79490.868585	36.831399
1606.857680	79566.568632	36.836416
1608.288237	79654.952032	36.841434
1610.057027	79730.955767	36.846452
1612.209745	79809.357430	36.851469
1613.515545	79905.692016	36.856487
1615.473149	79969.643833	36.861504
1616.714733	80051.191375	36.866522
1618.183882	80125.101989	36.871540
1620.050679	80204.626405	36.876557
1621.688048	80291.674526	36.881575
1623.426135	80365.455002	36.886592
1624.979037	80455.354791	36.891610
1626.751506	80528.180113	36.896628
1628.255863	80603.454786	36.901645
1629.821513	80676.566253	36.906663
1631.763306	80762.098537	36.911680
1633.013213	80839.288760	36.916698
1634.477198	80917.294556	36.921716
1636.666920	80999.456657	36.926733
1637.997380	81083.907327	36.931751
1639.671151	81153.252894	36.936768
1641.241100	81236.931699	36.941786
1642.778971	81320.489077	36.946804
1644.345254	81387.812211	36.951821
1645.789583	81474.222727	36.956839
1647.924579	81560.348037	36.961856
1648.728461	81642.906296	36.966874
1650.468191	81703.944096	36.971892
1652.082169	81776.987523	36.976909
1653.624883	81852.753680	36.981927
1655.082642	81922.363016	36.986944
1656.515552	82001.124221	36.991962
1658.060021	82085.100952	36.996980
1660.345027	82160.637734	37.001997
1661.281667	82235.878936	37.007015
1663.368962	82311.991886	37.012032
1664.566573	82392.311437	37.017050
1666.415972	82470.375256	37.022068
1667.972927	82554.997616	37.027085
1669.614940	82643.471384	37.032103
1671.335439	82732.541326	37.037120
1672.940357	82822.744636	37.042138
1674.816838	82914.565570	37.047156
1676.940099	83001.470020	37.052173
1678.154440	83092.520888	37.057191
1680.473069	83174.213024	37.062208
1681.981420	83262.595606	37.067226
1683.409159	83362.876195	37.072244
1685.634397	83439.388722	37.077261
1687.446888	83529.929244	37.082279
1689.102228	83608.039238	37.087296
1690.997582	83695.653032	37.092314
1692.682006	83783.426815	37.097332
1694.373416	83873.657935	37.102349
1695.682299	83953.254909	37.107367
1697.544723	84036.490750	37.112384
1699.316851	84136.314688	37.117402
1701.042758	84224.577505	37.122420
1702.920979	84310.421914	37.127437
1704.545509	84396.876486	37.132455
1706.302187	84489.734935	37.137472
1707.768856	84586.757226	37.142490
1709.767904	84671.532094	37.147508
1711.637773	84761.725412	37.152525
1712.717593	84857.174556	37.157543
1714.711973	84948.793509	37.162560
1716.470378	85048.305980	37.167578
1718.338570	85133.774278	37.172596
1720.228434	85227.742029	37.177613
1721.750917	85322.135056	37.182631
1723.789395	85407.767590	37.187648
1725.226433	85500.413219	37.192666
1726.895942	85595.278324	37.197684
1729.268439	85682.608092	37.202701
1730.669433	85783.522234	37.207719
1732.333058	85868.226398	37.212736
1733.925096	85958.834419	37.217754
1735.951921	86048.158181	37.222772
1737.662581	86134.731202	37.227789
1739.278857	86227.465152	37.232807
1741.346586	86323.600875	37.237824
1742.933843	86407.938406	37.242842
1744.607195	86497.572308	37.247860
1746.284522	86580.578348	37.252877
1748.106127	86680.327304	37.257895
1750.146391	86763.783954	37.262912
1751.904058	86852.011811	37.267930
1753.583245	86937.033459	37.272948
1755.601109	87020.925209	37.277965
1756.952450	87101.043770	37.282983
1758.818713	87189.825908	37.288000
1760.670832	87290.091740	37.293018
1762.542832	87372.220513	37.298036
1764.483808	87455.910112	37.303053
1765.997879	87537.575791	37.308071
1767.793160	87603.534407	37.313088
1769.405499	87674.831614	37.318106
1770.876583	87748.406826	37.323124
1772.373106	87821.217882	37.328141
1773.982663	87899.017139	37.333159
1776.025911	87965.368635	37.338176
1777.702142	88045.907825	37.343194
1779.375777	88132.099703	37.348212
1781.055426	88206.289734	37.353229
1782.231134	88292.534657	37.358247
1783.990230	88382.351001	37.363264
1785.828544	88478.732472	37.368282
1787.505195	88572.414867	37.373300
1789.929321	88655.512680	37.378317
1791.768967	88764.022943	37.383335
1793.884663	88843.038136	37.388352
1794.995564	88929.916040	37.393370
1796.785112	89030.311647	37.398388
1798.754287	89131.680667	37.403405
1800.296950	89224.486294	37.408423
1802.238061	89322.451254	37.413440
1803.921459	89420.190726	37.418458
1805.773001	89533.238991	37.423476
1807.484254	89633.636214	37.428493
1809.288979	89744.069208	37.433511
1811.466950	89844.457472	37.438528
1813.084127	89947.810729	37.443546
1814.638848	90046.092004	37.448564
1816.762934	90158.048077	37.453581
1818.374297	90273.113817	37.458599
1820.492163	90388.949877	37.463616
1822.417453	90492.598990	37.468634
1824.417243	90599.329217	37.473652
1825.992083	90704.199893	37.478669
1827.603360	90818.291848	37.483687
1829.486446	90921.391392	37.488704
1831.529024	91040.739761	37.493722
1833.349710	91159.426254	37.498740
1835.243073	91269.293331	37.503757
1837.110627	91382.865702	37.508775
1839.245166	91491.669241	37.513792
1841.448769	91601.488979	37.518810
1842.887083	91704.939634	37.523828
1844.859958	91810.182793	37.528845
1846.991437	91921.383806	37.533863
1848.861918	92028.025252	37.538880
1850.635322	92128.839333	37.543898
1852.305037	92241.799485	37.548916
1854.809658	92340.421223	37.553933
1856.650091	92448.551770	37.558951
1858.174011	92549.495009	37.563968
1860.179361	92654.026229	37.568986
1862.091923	92760.131320	37.574004
1864.282832	92860.413526	37.579021
1865.961545	92950.851834	37.584039
1867.692226	93064.832153	37.589056
1870.247224	93166.338551	37.594074
1871.613189	93266.282208	37.599092
1873.902362	93359.909008	37.604109
1875.892955	93455.382671	37.609127
1878.080412	93543.423592	37.614144
1879.918543	93624.611506	37.619162
1881.793239	93724.730551	37.624180
1884.100214	93801.130419	37.629197
1885.810957	93890.058143	37.634215
1887.903705	93978.913672	37.639232
1889.216817	94059.500430	37.644250
1890.744928	94140.459364	37.649268
1892.708844	94203.199244	37.654285
1894.545053	94278.989499	37.659303
1896.129574	94357.823393	37.664320
1898.094191	94440.438663	37.669338
1899.803853	94517.073209	37.674356
1901.127493	94600.955351	37.679373
1902.991960	94689.519088	37.684391
1904.612825	94770.984857	37.689408
1906.568246	94859.192607	37.694426
1908.257506	94967.697920	37.699444
1910.097719	95067.737988	37.704461
1911.644417	95177.090259	37.709479
1913.318126	95273.138838	37.714496
1915.570327	95372.076004	37.719514
1917.578970	95497.087788	37.724532
1919.217512	95606.528602	37.729549
1921.022033	95728.024001	37.734567
1922.699774	95839.500323	37.739584
1924.832346	95958.803043	37.744602
1926.809109	96081.210889	37.749620
1928.519691	96199.705909	37.754637
1930.411518	96327.401279	37.759655
1932.303472	96455.312644	37.764672
1934.716872	96571.531455	37.769690
1936.367484	96700.761888	37.774708
1938.660295	96817.963882	37.779725
1940.964978	96938.701178	37.784743
1942.709375	97071.924210	37.789760
1944.922341	97194.667047	37.794778
1946.821239	97323.658354	37.799796
1948.630462	97436.247977	37.804813
1950.872921	97566.695035	37.809831
1952.786063	97682.438443	37.814848
1954.757656	97809.252631	37.819866
1956.643695	97931.732560	37.824884
1958.582101	98064.485716	37.829901
1960.761468	98188.644792	37.834919
1962.794153	98320.509555	37.839936
1965.125249	98432.628061	37.844954
1967.060407	98562.100447	37.849972
1968.963888	98687.534311	37.854989
1970.824025	98804.595834	37.860007
1972.803172	98943.025642	37.865024
1974.952601	99057.342573	37.870042
1976.637393	99190.634504	37.875060
1978.520863	99320.827974	37.880077
1980.900899	99440.903748	37.885095
1982.672956	99576.566979	37.890112
1984.624900	99692.691918	37.895130
1987.046229	99829.319531	37.900148
1988.589232	99958.060217	37.905165
1991.057977	100079.924716	37.910183
1992.530115	100207.802725	37.915200
1994.893429	100341.335537	37.920218
1996.910491	100460.178766	37.925236
1998.746847	100587.278645	37.930253
2000.926130	100712.043336	37.935271
2002.776234	100854.951482	37.940288
2005.078714	100977.238387	37.945306
2006.808135	101099.602739	37.950324
2008.579350	101234.816627	37.955341
2010.742385	101355.542004	37.960359
2012.640082	101489.050956	37.965376
2014.684196	101619.862427	37.970394
2016.381794	101748.535289	37.975412
2018.320244	101881.494295	37.980429
2020.658295	102022.492829	37.985447
2022.418083	102157.027673	37.990464
2023.923204	102260.046064	37.995482
2025.776767	102385.223099	38.000500
2027.958329	102500.827650	38.005517
2030.217484	102623.431762	38.010535
2031.597893	102752.018710	38.015552
2033.349523	102878.418042	38.020570
2035.250790	103004.350685	38.025588
2037.044332	103134.332537	38.030605
2039.288249	103277.240307	38.035623
2041.214165	103425.333430	38.040640
2043.570545	103561.771235	38.045658
2045.172097	103702.283574	38.050676
2046.908076	103839.035131	38.055693
2049.633714	103998.137939	38.060711
2051.369316	104146.099210	38.065728
2053.577438	104287.837744	38.070746
2055.531212	104448.382111	38.075764
2057.578976	104591.364237	38.080781
2060.294801	104740.544134	38.085799
2061.934225	104896.828811	38.090816
2064.000221	105051.044095	38.095834
2065.793197	105197.378031	38.100852
2068.368987	105354.837002	38.105869
2070.669403	105505.239134	38.110887
2072.987695	105661.459168	38.115904
2075.120428	105815.629457	38.120922
2077.144562	105969.944238	38.125940
2079.480367	106125.453592	38.130957
2081.403681	106269.147004	38.135975
2083.596753	106429.105409	38.140992
2085.790071	106584.727914	38.146010
2087.487103	106733.911152	38.151028
2089.506034	106890.665512	38.156045
2092.007004	107040.941607	38.161063
2094.046890	107215.129613	38.166080
2095.931751	107370.271372	38.171098
2098.456336	107528.407778	38.176116
2100.503464	107683.487518	38.181133
2102.491107	107840.796369	38.186151
2104.338332	107996.973965	38.191168
2106.789319	108162.378136	38.196186
2109.121275	108327.142320	38.201204
2110.752089	108491.940902	38.206221
2112.973775	108644.195166	38.211239
2115.446001	108807.126311	38.216256
2117.413802	108968.082815	38.221274
2119.809722	109137.963965	38.226292
2121.357270	109309.855488	38.231309
2124.134774	109460.682152	38.236327
2125.659269	109621.647617	38.241344
2128.511747	109786.159715	38.246362
2130.888334	109951.279659	38.251380
2132.688434	110100.144207	38.256397
2135.012059	110260.112545	38.261415
2137.224193	110420.327320	38.266432
2139.651372	110572.722672	38.271450
2141.594670	110728.656481	38.276468
2143.613923	110893.215339	38.281485
2146.046708	111034.984529	38.286503
2148.221080	111195.259445	38.291520
2150.432376	111334.946622	38.296538
2152.422900	111487.490314	38.301556
2154.519945	111644.646915	38.306573
2156.719686	111792.872669	38.311591
2158.678218	111954.579792	38.316608
2160.812729	112115.676732	38.321626
2163.016465	112264.702790	38.326644
2165.079998	112415.552283	38.331661
2167.294318	112553.024350	38.336679
2169.400324	112692.137230	38.341696
2170.792216	112817.005899	38.346714
2172.563879	112952.075678	38.351732
2174.403466	113109.684808	38.356749
2176.960740	113256.769965	38.361767
2178.504528	113410.254124	38.366784
2180.572885	113580.765768	38.371802
2182.237180	113747.282958	38.376820
2184.407250	113915.649561	38.381837
2186.733257	114085.032536	38.386855
2188.607657	114268.907409	38.391872
2190.276412	114440.918761	38.396890
2192.751148	114640.111372	38.401908
2194.593169	114824.818496	38.406925
2196.712301	115016.141849	38.411943
2198.928873	115222.505941	38.416960
2201.317395	115413.459444	38.421978
2203.401402	115614.164348	38.426996
2205.628692	115819.578842	38.432013
2208.094310	116010.561413	38.437031
2210.088861	116220.682065	38.442048
2212.436939	116417.494189	38.447066
2214.920725	116625.105320	38.452084
2217.087422	116837.282637	38.457101
2219.771541	117038.598934	38.462119
2222.198928	117238.878344	38.467136
2224.047032	117450.487459	38.472154
2226.711341	117649.197224	38.477172
2228.522603	117854.941656	38.482189
2230.922303	118050.219479	38.487207
2232.910364	118263.396771	38.492224
2235.138172	118468.876418	38.497242
2237.890909	118683.192179	38.502260
2239.861288	118900.713871	38.507277
2242.306823	119115.397233	38.512295
2244.652038	119335.577246	38.517312
2246.516936	119532.202106	38.522330
2249.155884	119750.638798	38.527348
2251.493779	119965.280329	38.532365
2253.980317	120176.589042	38.537383
2256.065498	120395.103333	38.542400
2258.589031	120604.391685	38.547418
2260.630952	120812.564113	38.552436
2262.926300	121036.820854	38.557453
2265.592082	121236.221290	38.562471
2268.132708	121450.522183	38.567488
2270.305758	121655.494581	38.572506
2272.709471	121866.698569	38.577524
2275.101849	122081.584263	38.582541
2277.502926	122271.339650	38.587559
2279.564109	122481.205109	38.592576
2281.618655	122687.939351	38.597594
2283.876620	122894.807762	38.602612
2286.079516	123117.492418	38.607629
2288.670602	123324.907187	38.612647
2290.623337	123541.506057	38.617664
2293.048337	123750.458652	38.622682
2295.314837	123958.701340	38.627700
2297.124875	124176.822929	38.632717
2299.797333	124389.761657	38.637735
2302.104187	124607.503386	38.642752
2304.289623	124829.147315	38.647770
2306.672303	125038.214705	38.652788
2309.270300	125252.260660	38.657805
2311.530873	125469.265756	38.662823
2313.733743	125673.569019	38.667840
2316.206993	125885.303474	38.672858
2318.549777	126069.668705	38.677876
2320.147152	126259.784327	38.682893
2322.473302	126433.344624	38.687911
2325.132957	126636.198357	38.692928
2327.214433	126829.856657	38.697946
2329.835601	127018.014062	38.702964
2331.630889	127216.045228	38.707981
2333.732768	127420.994636	38.712999
2335.993780	127618.624998	38.718016
2337.844718	127822.384978	38.723034
2340.333528	128038.238721	38.728052
2342.139316	128259.630650	38.733069
2344.138516	128470.970367	38.738087
2346.778150	128703.183499	38.743104
2348.947376	128944.378223	38.748122
2351.263231	129166.050379	38.753140
2353.271278	129420.506311	38.758157
2356.130450	129650.406501	38.763175
2358.645069	129888.723175	38.768192
2360.840346	130126.583618	38.773210
2363.143790	130371.622594	38.778228
2365.695322	130619.440925	38.783245
2368.377968	130860.616930	38.788263
2371.022289	131097.092930	38.793280
2372.914938	131349.751262	38.798298
2375.164667	131592.496302	38.803316
2377.825733	131838.109392	38.808333
2380.244898	132095.511321	38.813351
2382.999556	132336.849221	38.818368
2385.105831	132593.871617	38.823386
2387.671683	132830.077462	38.828404
2390.171926	133092.751094	38.833421
2392.613903	133334.282962	38.838439
2395.180826	133577.205080	38.843456
2397.746280	133830.927152	38.848474
2400.923322	134057.895125	38.853492
2403.406326	134305.135961	38.858509
2405.861741	134544.375551	38.863527
2408.373258	134782.364086	38.868544
2410.316756	135024.148042	38.873562
2413.119984	135267.943325	38.878580
2415.484281	135522.455112	38.883597
2417.365390	135765.267952	38.888615
2420.111109	136005.586555	38.893632
2421.719689	136258.989782	38.898650
2424.615329	136515.822362	38.903668
2426.536620	136775.486367	38.908685
2428.988322	137036.591659	38.913703
2431.312745	137292.388525	38.918720
2433.168986	137564.452616	38.923738
2436.026022	137832.110535	38.928756
2438.383835	138118.337788	38.933773
2440.902293	138377.930039	38.938791
2443.221436	138651.501657	38.943808
2445.211584	138931.522331	38.948826
2447.980394	139207.882196	38.953844
2450.484379	139475.871219	38.958861
2452.842490	139747.120701	38.963879
2455.245249	140032.248444	38.968896
2457.735421	140315.917459	38.973914
2460.255332	140585.230070	38.978932
2462.787756	140868.578467	38.983949
2464.804513	141148.646060	38.988967
2467.577697	141425.474926	38.993984
2469.280209	141712.790806	38.999002
2472.126678	141993.964528	39.004020
2474.339165	142278.805310	39.009037
2477.050325	142550.827543	39.014055
2479.249903	142826.066104	39.019072
2481.360717	143096.890726	39.024090
2483.554031	143352.689716	39.029108
2485.870311	143636.468682	39.034125
2488.011718	143902.584281	39.039143
2490.532354	144184.227555	39.044160
2492.810491	144472.522829	39.049178
2495.133779	144761.574207	39.054196
2497.669069	145055.696283	39.059213
2500.009995	145352.921962	39.064231
2502.146531	145642.959478	39.069248
2504.299430	145965.323325	39.074266
2506.990252	146272.780366	39.079284
2509.529744	146590.010706	39.084301
2511.839966	146904.727655	39.089319
2513.931468	147229.622105	39.094336
2516.530105	147560.493654	39.099354
2518.831342	147891.616895	39.104372
2521.542765	148229.354486	39.109389
2524.212585	148556.756012	39.114407
2526.859292	148894.051015	39.119424
2529.705402	149242.626491	39.124442
2532.730023	149573.202796	39.129460
2535.135155	149896.300171	39.134477
2537.825578	150234.015624	39.139495
2540.938144	150561.461659	39.144512
2542.839227	150897.667250	39.149530
2545.755034	151233.018033	39.154548
2548.491623	151560.186119	39.159565
2551.362177	151911.656309	39.164583
2554.162098	152231.087986	39.169600
2556.531190	152580.851015	39.174618
2559.474114	152902.257089	39.179636
2561.994973	153239.052672	39.184653
2564.445056	153565.744153	39.189671
2567.220681	153901.196326	39.194688
2569.935711	154246.942267	39.199706
2571.856051	154587.698792	39.204724
2574.706719	154917.204232	39.209741
2576.968359	155268.219208	39.214759
2579.654267	155601.384910	39.219776
2582.506469	155954.063477	39.224794
2584.778117	156298.253369	39.229812
2587.239820	156643.037579	39.234829
2589.656554	156992.845274	39.239847
2592.730017	157348.988604	39.244864
2595.292921	157702.281369	39.249882
2597.960085	158051.764076	39.254900
2600.667007	158399.846113	39.259917
2603.149183	158752.649815	39.264935
2606.144415	159100.919259	39.269952
2608.743318	159460.614985	39.274970
2611.203435	159804.846113	39.279988
2614.051460	160158.133817	39.285005
2616.328641	160507.615269	39.290023
2619.086374	160854.319327	39.295040
2621.445320	161221.641974	39.300058
2623.667460	161570.376155	39.305076
2626.530221	161925.778906	39.310093
2628.773789	162296.820248	39.315111
2631.297322	162668.238889	39.320128
2633.739221	163030.404304	39.325146
2636.308912	163400.702634	39.330164
2639.545911	163768.626050	39.335181
2641.823847	164146.693469	39.340199
2644.574054	164503.105405	39.345216
2647.033352	164874.178282	39.350234
2649.586562	165238.763311	39.355252
2652.013371	165591.676563	39.360269
2654.640203	165941.855975	39.365287
2657.213270	166278.206226	39.370304
2659.846548	166630.381500	39.375322
2662.042590	166974.958088	39.380340
2664.669918	167321.817829	39.385357
2667.012810	167710.229961	39.390375
2669.145798	168071.784848	39.395392
2671.833661	168441.761796	39.400410
2674.187005	168832.870172	39.405428
2676.953126	169206.952670	39.410445
2679.024511	169611.263615	39.415463
2681.743135	170008.479332	39.420480
2683.891090	170400.288475	39.425498
2686.711552	170817.783015	39.430516
2689.262230	171240.540758	39.435533
2691.801544	171669.613347	39.440551
2694.607640	172074.432178	39.445568
2696.706579	172504.708419	39.450586
2699.154989	172943.147870	39.455604
2702.176537	173380.560497	39.460621
2704.726783	173828.893316	39.465639
2707.878220	174271.318942	39.470656
2710.511699	174731.199010	39.475674
2712.613720	175177.361915	39.480692
2715.753644	175629.193412	39.485709
2718.216383	176097.603001	39.490727
2721.181759	176558.596955	39.495744
2723.769831	177023.766750	39.500762
2726.656890	177490.593936	39.505780
2730.060962	177955.158651	39.510797
2733.176686	178403.034148	39.515815
2736.752259	178847.614551	39.520832
2740.026732	179296.663468	39.525850
2742.773422	179738.406476	39.530868
2746.323578	180171.695517	39.535885
2748.675936	180622.165177	39.540903
2751.303555	181067.133422	39.545920
2754.032836	181516.253206	39.550938
2756.312624	181964.531112	39.555956
2759.211966	182471.130600	39.560973
2761.788521	182941.285541	39.565991
2764.756831	183392.561085	39.571008
2767.032647	183849.915737	39.576026
2770.119034	184310.803174	39.581044
2772.852471	184769.512827	39.586061
2775.352484	185234.306065	39.591079
2778.274798	185686.869130	39.596096
2781.136233	186144.980759	39.601114
2783.627617	186617.706167	39.606132
2786.990713	187084.658644	39.611149
2789.683867	187551.514738	39.616167
2792.417302	188016.867953	39.621184
2795.053401	188480.815969	39.626202
2797.902512	188955.400611	39.631220
2800.998090	189409.323809	39.636237
2803.265083	189893.020459	39.641255
2806.067939	190363.147749	39.646272
2808.820462	190838.542685	39.651290
2811.503519	191316.668244	39.656308
2814.613965	191794.246244	39.661325
2817.220837	192287.754922	39.666343
2819.686534	192761.602001	39.671360
2822.281199	193242.339742	39.676378
2825.090132	193739.073823	39.681396
2827.996912	194209.478948	39.686413
2830.708784	194697.366861	39.691431
2833.760878	195172.477294	39.696448
2836.546748	195627.132111	39.701466
2838.992149	196081.308240	39.706484
2842.328635	196539.182112	39.711501
2844.734768	196992.173436	39.716519
2847.806699	197454.105056	39.721536
2850.660129	197915.564262	39.726554
2853.134406	198380.945271	39.731572
2856.045216	198845.014735	39.736589
2858.677056	199329.679445	39.741607
2860.899070	199797.085512	39.746624
2863.709195	200284.773495	39.751642
2866.308431	200771.479820	39.756660
2869.277111	201255.665758	39.761677
2871.766631	201763.120385	39.766695
2874.408485	202272.483251	39.771712
2877.072734	202795.307413	39.776730
2879.296279	203319.141892	39.781748
2882.296816	203845.091759	39.786765
2884.674155	204387.093459	39.791783
2887.481603	204921.662572	39.796800
2890.481282	205469.564956	39.801818
2893.913944	206008.687864	39.806836
2897.360329	206542.195924	39.811853
2900.360477	207106.843030	39.816871
2903.166101	207655.949845	39.821888
2905.642993	208211.282341	39.826906
2908.596527	208766.948027	39.831924
2911.231392	209329.549087	39.836941
2914.310526	209916.443724	39.841959
2916.828688	210487.677256	39.846976
2920.048222	211050.165096	39.851994
2922.615657	211641.995461	39.857012
2925.820167	212223.438910	39.862029
2928.833935	212814.744461	39.867047
2931.492699	213393.531776	39.872064
2934.538065	213982.624307	39.877082
2937.515169	214572.846229	39.882100
2940.536814	215167.888807	39.887117
2943.527315	215759.304378	39.892135
2946.927026	216356.702877	39.897152
2950.123667	216946.030066	39.902170
2953.584626	217539.305033	39.907188
2956.618460	218129.598981	39.912205
2959.463597	218718.652842	39.917223
2962.651588	219309.203277	39.922240
2965.996805	219896.401700	39.927258
2969.026378	220480.855489	39.932276
2972.576225	221053.415431	39.937293
2975.583656	221627.635580	39.942311
2979.201287	222203.869127	39.947328
2982.335289	222760.592008	39.952346
2985.393412	223340.597074	39.957364
2988.446282	223889.508513	39.962381
2991.649346	224463.927668	39.967399
2994.240517	225028.534973	39.972416
2997.704893	225593.132758	39.977434
3000.040989	226154.579015	39.982452
3003.176308	226719.787038	39.987469
3005.915458	227287.648109	39.992487
3008.628775	227856.859467	39.997504
3011.897160	228434.265533	40.002522
3014.204180	229005.572276	40.007540
3017.336351	229592.322344	40.012557
3019.965126	230162.384113	40.017575
3022.977074	230752.556335	40.022592
3025.976892	231338.411302	40.027610
3028.583352	231934.234802	40.032628
3031.112955	232526.563992	40.037645
3033.778536	233098.141710	40.042663
3036.701704	233674.276612	40.047680
3039.418578	234245.972008	40.052698
3041.666362	234827.825340	40.057716
3044.577884	235424.028819	40.062733
3046.988622	236033.799092	40.067751
3049.733264	236640.645546	40.072768
3052.751500	237258.320937	40.077786
3055.653710	237882.186414	40.082804
3058.335230	238510.378387	40.087821
3061.005750	239151.958425	40.092839
3063.749581	239794.744955	40.097856
3066.746696	240450.776356	40.102874
3069.564896	241106.656302	40.107892
3072.721015	241781.229311	40.112909
3075.532325	242464.110415	40.117927
3078.793946	243151.263055	40.122944
3082.037986	243826.756385	40.127962
3084.649560	244524.345464	40.132980
3088.114978	245220.579382	40.137997
3091.411637	245904.161337	40.143015
3094.776796	246617.756152	40.148032
3097.975953	247315.777077	40.153050
3101.333950	248014.380180	40.158068
3104.273739	248705.450641	40.163085
3107.648186	249429.625734	40.168103
3110.675022	250133.708164	40.173120
3114.070597	250846.290391	40.178138
3117.292297	251560.750953	40.183156
3120.471025	252276.942258	40.188173
3123.725828	252994.972586	40.193191
3126.636007	253732.079052	40.198208
3129.855416	254449.828283	40.203226
3132.638466	255180.571310	40.208244
3135.502913	255908.579762	40.213261
3138.739183	256645.086222	40.218279
3141.660639	257386.209883	40.223296
3145.059495	258129.896235	40.228314
3147.674740	258889.804605	40.233332
3151.071131	259629.951556	40.238349
3154.577987	260390.142795	40.243367
3157.669172	261140.996022	40.248384
3160.914230	261899.846589	40.253402
3163.875099	262657.644224	40.258420
3167.516535	263408.294497	40.263437
3171.673475	264153.296424	40.268455
3174.702845	264899.663124	40.273472
3178.410086	265636.520779	40.278490
3181.421217	266392.632600	40.283508
3184.798860	267141.087154	40.288525
3187.915183	267871.391543	40.293543
3191.111546	268614.783321	40.298560
3194.914600	269356.347288	40.303578
3197.768884	270103.184012	40.308596
3201.291098	270834.443017	40.313613
3204.614958	271565.955631	40.318631
3207.612824	272311.202217	40.323648
3210.526211	273054.169872	40.328666
3214.110412	273799.362662	40.333684
3216.911592	274536.468197	40.338701
3220.331390	275280.200447	40.343719
3223.151445	276022.368940	40.348736
3226.333036	276773.057825	40.353754
3229.214815	277532.878076	40.358772
3232.428328	278281.693669	40.363789
3235.946502	279028.448118	40.368807
3240.009701	279763.910872	40.373824
3243.414839	280492.587353	40.378842
3246.727027	281195.038832	40.383860
3249.937418	281895.036227	40.388877
3253.280222	282592.161997	40.393895
3256.426088	283279.636763	40.398912
3259.790299	283975.069560	40.403930
3262.819753	284679.841595	40.408948
3265.489314	285369.376182	40.413965
3268.812624	286086.911094	40.418983
3271.367055	286804.177655	40.424000
3274.465916	287529.730680	40.429018
3277.497515	288261.151661	40.434036
3280.161894	289001.508784	40.439053
3284.247324	289721.398414	40.444071
3287.286380	290482.601987	40.449088
3290.270882	291228.595896	40.454106
3293.259573	291984.583880	40.459124
3296.068554	292766.843745	40.464141
3299.472753	293530.796097	40.469159
3302.281993	294328.396245	40.474176
3305.386306	295118.932145	40.479194
3308.170596	295917.022369	40.484212
3311.333353	296723.141199	40.489229
3314.340865	297540.519700	40.494247
3317.395156	298369.734963	40.499264
3321.000224	299208.752718	40.504282
3324.110622	300050.424476	40.509300
3327.045153	300898.457289	40.514317
3330.663363	301750.736222	40.519335
3333.646204	302623.333049	40.524352
3336.675518	303484.891056	40.529370
3340.371728	304368.668975	40.534388
3342.930989	305262.839296	40.539405
3346.380056	306150.305803	40.544423
3349.573441	307047.086911	40.549440
3352.995835	307952.471592	40.554458
3357.183930	308835.789595	40.559476
3361.475722	309719.049987	40.564493
3365.912867	310600.773967	40.569511
3369.670416	311467.511636	40.574528
3373.333393	312336.405525	40.579546
3377.048551	313219.462519	40.584564
3380.545256	314097.384785	40.589581
3384.096098	314942.898149	40.594599
3387.158006	315828.900218	40.599616
3390.637456	316692.106210	40.604634
3393.774320	317565.094005	40.609652
3397.043373	318437.587069	40.614669
3400.614958	319307.553887	40.619687
3403.783569	320194.009878	40.624704
3407.372669	321070.130108	40.629722
3410.258095	321947.737911	40.634740
3413.797090	322832.913689	40.639757
3416.929411	323723.640398	40.644775
3420.381190	324611.126304	40.649792
3424.131168	325508.314879	40.654810
3428.005217	326379.533822	40.659828
3431.458123	327265.185483	40.664845
3434.954476	328142.438225	40.669863
3438.428804	329033.400414	40.674880
3442.092540	329915.737701	40.679898
3445.519224	330802.125756	40.684916
3448.894112	331679.038967	40.689933
3451.960873	332568.892658	40.694951
3455.383231	333463.438981	40.699968
3458.442076	334359.771176	40.704986
3461.936508	335254.973705	40.710004
3465.676209	336136.114311	40.715021
3468.984484	337003.557104	40.720026
3472.091609	337859.265836	40.725031
3475.539454	338656.160344	40.730036
3478.722498	339420.504848	40.735040
3481.746380	340126.094145	40.740045
3484.088205	340771.818309	40.745050
3487.302502	341370.049294	40.750055
3490.344438	341922.808952	40.755060
3492.868783	342405.413700	40.760064
3494.689449	342863.433254	40.765069
3497.562439	343246.124320	40.770074
3500.084959	343588.490544	40.775079
3501.845759	343877.350940	40.780084
3503.782679	344122.247130	40.785088
3505.554910	344341.157794	40.790093
3506.984591	344506.449245	40.795098
3508.646595	344636.744851	40.800103
3510.473762	344732.767399	40.805108
3512.025616	344775.161778	40.810112
3513.457261	344800.387998	40.815117
3514.600973	344787.598871	40.820122
3515.749399	344748.799797	40.825127
3516.565631	344689.763871	40.830132
3517.538054	344596.049758	40.835136
3517.655451	344483.324304	40.840141
3518.603610	344360.425827	40.845146
3519.096563	344218.783693	40.850151
3519.470011	344059.413035	40.855156
3519.917038	343869.901395	40.860160
3520.349514	343685.043804	40.865165
3521.096459	343485.160504	40.870170
3520.812298	343278.699477	40.875175
3521.194366	343063.666300	40.880180
3521.808535	342835.043514	40.885184
3522.104016	342587.094397	40.890189
3522.148962	342344.191643	40.895194
3522.296309	342091.227752	40.900199
3522.442565	341822.980806	40.905204
3522.601039	341547.762944	40.910208
3522.360968	341276.698975	40.915213
3522.714314	340993.360506	40.920218
3522.759935	340720.289684	40.925223
3522.464037	340449.100927	40.930228
3522.444420	340156.304115	40.935232
3522.655360	339872.216079	40.940237
3522.652213	339562.197017	40.945242
3522.386496	339279.551892	40.950247
3522.410674	338980.381443	40.955252
3522.333088	338689.997361	40.960256
3522.104022	338400.422913	40.965261
3522.312524	338102.869222	40.970266
3522.394191	337813.597489	40.975271
3522.112116	337504.290855	40.980276
3521.974443	337213.573698	40.985280
3521.628386	336911.722979	40.990285
3521.944946	336614.623360	40.995290
3521.757454	336323.118552	41.000295
3521.451606	336029.926072	41.005300
3521.361934	335723.549665	41.010304
3520.912699	335443.802462	41.015309
3521.222219	335158.161609	41.020314
3521.044965	334865.397535	41.025319
3520.605380	334582.946581	41.030324
3520.929605	334296.711877	41.035328
3520.501401	333995.867420	41.040333
3520.583128	333707.351794	41.045338
3520.403354	333415.263418	41.050343
3520.218038	333126.403596	41.055348
3519.815105	332849.249284	41.060352
3519.566879	332561.335995	41.065357
3519.698654	332281.881260	41.070362
3519.497904	332018.652135	41.075367
3519.377190	331739.436362	41.080372
3519.531255	331466.050805	41.085376
3519.261597	331193.060184	41.090381
3519.286036	330908.220187	41.095386
3518.538845	330642.828837	41.100391
3518.529206	330372.004539	41.105396
3518.694772	330101.812259	41.110400
3518.215282	329844.182041	41.115405
3518.203352	329577.066050	41.120410
3517.926570	329323.572050	41.125415
3517.572188	329071.589226	41.130420
3517.714959	328813.804061	41.135424
3517.694046	328557.670683	41.140429
3517.760519	328302.285056	41.145434
3517.085530	328046.199744	41.150439
3517.146099	327796.509450	41.155444
3516.915687	327553.323914	41.160448
3516.720585	327311.123397	41.165453
3516.878868	327065.101535	41.170458
3516.723893	326829.098371	41.175463
3516.313429	326585.375482	41.180468
3516.326997	326351.098309	41.185472
3515.857401	326126.968470	41.190477
3515.730723	325883.273279	41.195482
3515.632373	325651.909413	41.200487
3515.688976	325427.617123	41.205492
3515.219360	325200.912955	41.210496
3514.980628	324984.855384	41.215501
3515.105676	324761.642562	41.220506
3514.810806	324536.484549	41.225511
3514.602874	324326.065979	41.230516
3514.393668	324112.085137	41.235520
3514.398767	323904.353028	41.240525
3514.442458	323685.802358	41.245530
3514.486436	323489.382343	41.250535
3514.297017	323271.629100	41.255540
3514.225950	323052.940402	41.260544
3513.561341	322853.855293	41.265549
3513.621197	322655.368276	41.270554
3513.623650	322454.676052	41.275559
3513.306226	322258.917290	41.280564
3513.265991	322071.127808	41.285568
3513.252876	321866.644682	41.290573
3513.080833	321671.776296	41.295578
3512.669480	321485.746708	41.300583
3512.365574	321298.758216	41.305588
3512.906422	321110.161291	41.310592
3512.406247	320925.389708	41.315597
3512.411716	320752.724303	41.320602
3511.889853	320557.193155	41.325607
3511.816573	320381.358474	41.330612
3511.953760	320215.946371	41.335616
3511.638194	320052.283517	41.340621
3511.800210	319866.030019	41.345626
3511.603020	319696.139678	41.350631
3511.405953	319525.129231	41.355636
3511.491691	319366.565615	41.360640
3510.918870	319193.500968	41.365645
3510.643376	319030.031505	41.370650
3510.697648	318870.656865	41.375655
3510.709201	318718.132154	41.380660
3510.960507	318558.496592	41.385664
3510.464503	318405.566744	41.390669
3510.114192	318244.166828	41.395674
3510.238578	318097.372211	41.400679
3509.956489	317947.969219	41.405684
3510.537588	317798.481654	41.410688
3509.652433	317655.456198	41.415693
3510.001527	317494.961881	41.420698
3509.664848	317358.693739	41.425703
3509.715733	317213.078024	41.430708
3509.994072	317056.129704	41.435712
3509.551546	316932.470945	41.440717
3509.708277	316787.346142	41.445722
3509.588795	316637.557101	41.450727
3509.179526	316510.253625	41.455732
3509.298819	316364.039247	41.460736
3509.237732	316233.678260	41.465741
3509.419580	316090.709938	41.470746
3509.038897	315960.372678	41.475751
3509.436799	315831.490809	41.480756
3509.038975	315682.174627	41.485760
3509.138043	315560.691875	41.490765
3508.733133	315425.548018	41.495770
3508.870313	315292.456280	41.500775
3508.419028	315161.873312	41.505780
3508.505934	315023.674440	41.510784
3508.093786	314908.249170	41.515789
3508.396858	314791.770361	41.520794
3508.114537	314667.291559	41.525799
3508.047760	314555.297236	41.530804
3508.085163	314422.676545	41.535808
3507.623568	314310.972346	41.540813
3508.071340	314186.250869	41.545818
3507.735414	314085.162206	41.550823
3507.476814	313974.366893	41.555828
3507.604529	313860.203128	41.560832
3507.285230	313755.548906	41.565837
3507.567460	313647.568935	41.570842
3507.570734	313540.421108	41.575847
3507.328709	313434.023836	41.580852
3507.313658	313324.232118	41.585856
3506.984787	313226.499183	41.590861
3507.032852	313113.592823	41.595866
3506.967949	312997.854010	41.600871
3506.932443	312913.255057	41.605876
3506.880125	312819.498345	41.610880
3506.607772	312713.511282	41.615885
3506.815466	312610.527798	41.620890
3506.830841	312514.978726	41.625895
3506.554539	312418.635363	41.630900
3506.820907	312312.690393	41.635904
3506.419840	312233.618114	41.640909
3506.457454	312132.008773	41.645914
3506.686463	312039.656906	41.650919
3506.507998	311947.597571	41.655924
3506.519511	311836.195126	41.660928
3506.114194	311754.272793	41.665933
3505.995080	311658.768448	41.670938
3506.138889	311572.663187	41.675943
3506.080932	311489.312016	41.680948
3506.328808	311400.263902	41.685952
3505.738015	311311.219507	41.690957
3506.181125	311222.878469	41.695962
3506.049435	311140.301589	41.700967
3505.811662	311057.715704	41.705972
3506.258523	310955.759944	41.710976
3506.020226	310893.428949	41.715981
3505.749413	310786.114107	41.720986
3505.920416	310712.853360	41.725991
3505.582513	310623.590016	41.730996
3505.894239	310540.433847	41.736000
3505.469259	310482.126573	41.741005
3505.396661	310387.019539	41.746010
3505.520055	310301.576775	41.751015
3505.251471	310231.717501	41.756020
3505.067163	310144.363183	41.761024
3505.066676	310084.029676	41.766029
3505.079529	309995.270148	41.771034
3505.044555	309933.186027	41.776039
3505.321080	309852.324366	41.781044
3505.295104	309778.355033	41.786048
3504.481338	309705.679300	41.791053
3504.716908	309643.857871	41.796058
3504.771977	309570.206357	41.801063
3504.930198	309504.172666	41.806068
3504.836804	309441.053724	41.811072
3504.713735	309372.671821	41.816077
3504.943335	309291.358513	41.821082
3504.875747	309229.889315	41.826087
3504.470065	309161.805769	41.831092
3504.720149	309103.264051	41.836096
3504.313313	309043.603503	41.841101
3504.450286	308970.294533	41.846106
3504.483984	308904.457624	41.851111
3504.278614	308849.625754	41.856116
3504.500480	308787.270986	41.861120
3504.180855	308728.690649	41.866125
3504.259613	308665.289312	41.871130
3504.414952	308609.382887	41.876135
3504.401461	308549.736581	41.881140
3504.347614	308482.614975	41.886144
3504.278792	308426.234437	41.891149
3503.959218	308358.823388	41.896154
3504.108482	308302.841220	41.901159
3503.613386	308242.455514	41.906164
3504.293471	308199.673851	41.911168
3503.820481	308149.209119	41.916173
3503.953735	308096.435614	41.921178
3503.804843	308033.425317	41.926183
3503.497469	307991.383147	41.931188
3504.071033	307925.893132	41.936192
3503.699576	307882.792085	41.941197
3503.512711	307825.004240	41.946202
3503.713271	307779.065316	41.951207
3503.216262	307729.494581	41.956212
3503.530592	307676.921348	41.961216
3503.675792	307633.433936	41.966221
3503.774794	307585.423986	41.971226
3503.836402	307531.872195	41.976231
3503.296429	307477.421927	41.981236
3503.884181	307431.574835	41.986240
3503.521609	307390.787733	41.991245
3503.111149	307332.270830	41.996250
3503.283794	307281.042625	42.001255
3503.429262	307245.749094	42.006260
3503.173996	307199.906345	42.011264
3502.846484	307162.345479	42.016269
3502.935435	307115.227329	42.021274
3503.307182	307080.534508	42.026279
3502.979806	307041.828363	42.031284
3503.742082	306990.075057	42.036288
3503.129537	306948.054263	42.041293
3503.229247	306900.374368	42.046298
3503.272467	306846.926506	42.051303
3502.985884	306815.695593	42.056308
3503.229707	306778.401390	42.061312
3503.306635	306738.741112	42.066317
3503.042736	306700.559192	42.071322
3503.080269	306655.866238	42.076327
3502.974717	306620.560614	42.081332
3503.097369	306580.256852	42.086336
3502.878161	306540.006504	42.091341
3503.010663	306493.975241	42.096346
3502.795347	306451.179370	42.101351
3502.787684	306424.408982	42.106356
3503.052135	306382.530536	42.111360
3502.652728	306348.186806	42.116365
3503.006086	306313.598123	42.121370
3503.233939	306271.572615	42.126375
3502.808584	306229.750989	42.131380
3502.953596	306190.130530	42.136384
3502.999077	306159.229021	42.141389
3502.688126	306114.742760	42.146394
3502.879572	306083.538450	42.151399
3502.757069	306045.461169	42.156404
3502.656160	306006.108050	42.161408
3502.517108	305971.443424	42.166413
3502.346759	305930.396040	42.171418
3502.752709	305905.876544	42.176423
3502.815915	305878.814850	42.181428
3502.908834	305831.618529	42.186432
3503.061838	305801.336211	42.191437
3502.640935	305758.470097	42.196442
3502.912656	305725.624293	42.201447
3502.867020	305692.726288	42.206452
3502.675345	305652.420029	42.211456
3502.834680	305625.190477	42.216461
3502.494255	305585.518193	42.221466
3502.916123	305545.752150	42.226471
3502.790970	305512.102992	42.231476
3502.820863	305473.085294	42.236480
3502.656291	305445.804490	42.241485
3502.691692	305414.980450	42.246490
3502.651173	305377.958707	42.251495
3502.518291	305350.163918	42.256500
3502.713490	305325.422601	42.261504
3502.164396	305288.353058	42.266509
3502.374605	305249.306998	42.271514
3502.516791	305217.957163	42.276519
3502.152032	305192.030872	42.281524
3502.328113	305154.008038	42.286528
3502.119443	305134.597734	42.291533
3502.118353	305110.395983	42.296538
3502.144442	305078.987865	42.301543
3502.276923	305053.950833	42.306548
3502.453342	305019.617973	42.311552
3502.218979	304992.220591	42.316557
3502.268635	304961.699439	42.321562
3502.285668	304944.035219	42.326567
3501.978376	304915.809375	42.331572
3502.563138	304871.563726	42.336576
3502.251143	304859.727895	42.341581
3502.117045	304832.620144	42.346586
3502.352076	304807.668755	42.351591
3502.303002	304786.884556	42.356596
3502.203959	304748.166404	42.361600
3502.097280	304724.719008	42.366605
3501.858617	304703.302733	42.371610
3502.038700	304675.611343	42.376615
3501.707110	304652.326324	42.381620
3502.298799	304629.151442	42.386624
3501.981761	304615.178597	42.391629
3501.613901	304576.247848	42.396634
3501.761205	304560.853575	42.401639
3501.699708	304538.722399	42.406644
3501.861193	304518.541408	42.411648
3501.424185	304493.923978	42.416653
3501.773658	304481.068467	42.421658
3501.945529	304457.577400	42.426663
3501.786240	304442.434620	42.431668
3502.013101	304419.851120	42.436672
3501.993894	304401.327098	42.441677
3502.466552	304376.974587	42.446682
3502.171196	304352.818485	42.451687
3501.916573	304320.537607	42.456692
3502.263805	304294.703145	42.461696
3502.138647	304268.051789	42.466701
3501.830040	304232.852599	42.471706
3502.025785	304218.366835	42.476711
3501.747640	304203.446163	42.481716
3501.813992	304173.583621	42.486720
3501.722153	304154.510975	42.491725
3502.008290	304140.850894	42.496730
3501.905239	304110.149513	42.501735
3501.881126	304094.451055	42.506740
3502.221879	304064.112907	42.511744
3502.038660	304053.172944	42.516749
3501.830019	304023.226059	42.521754
3502.211566	304003.850301	42.526759
3501.822659	303993.044282	42.531764
3502.083677	303970.251648	42.536768
3502.008167	303944.712150	42.541773
3501.866557	303911.675307	42.546778
3502.041417	303887.445473	42.551783
3501.741031	303869.855960	42.556788
3501.727108	303832.905294	42.561792
3501.452494	303840.608794	42.566797
3501.442961	303806.227848	42.571802
3501.515732	303795.833154	42.576807
3501.447197	303790.397807	42.581812
3501.753273	303756.069284	42.586816
3501.744491	303754.238463	42.591821
3501.830876	303724.474329	42.596826
3501.637724	303694.982929	42.601831
3501.858698	303693.777881	42.606836
3502.141365	303653.879439	42.611840
3502.050681	303651.705120	42.616845
3501.929449	303632.916825	42.621850
3501.558659	303590.244662	42.626855
3501.531711	303583.708447	42.631860
3501.531452	303561.338230	42.636864
3501.504026	303542.662486	42.641869
3502.034257	303534.130413	42.646874
3501.947379	303510.373972	42.651879
3501.725378	303501.908598	42.656884
3502.004668	303470.510815	42.661888
3501.620919	303452.883294	42.666893
3501.673201	303438.063442	42.671898
3501.449300	303415.066428	42.676903
3501.752254	303406.188117	42.681908
3502.232505	303377.125707	42.686912
3502.093408	303366.127802	42.691917
3501.851050	303333.768042	42.696922
3501.749309	303314.416685	42.701927
3501.617522	303298.403970	42.706932
3501.923194	303265.754889	42.711936
3502.118337	303251.599801	42.716941
3501.765566	303232.262209	42.721946
3502.312787	303209.831698	42.726951
3501.737358	303183.530132	42.731956
3502.035772	303155.793981	42.736960
3501.785878	303143.744447	42.741965
3501.703909	303118.027402	42.746970
3501.759392	303092.441556	42.751975
3501.370997	303077.995899	42.756980
3502.019244	303056.949286	42.761984
3501.504775	303039.698363	42.766989
3501.519017	303018.012801	42.771994
3501.643885	303013.437891	42.776999
3501.589118	302994.435374	42.782004
3501.714510	302972.223411	42.787009
3501.806157	302961.621999	42.792013
3501.822408	302941.157699	42.797018
3501.988742	302922.629593	42.802023
3501.653044	302904.943474	42.807028
3501.816014	302880.918633	42.812033
3501.926782	302859.141563	42.817037
3501.859317	302837.595951	42.822042
3501.892970	302812.013381	42.827047
3501.736361	302795.877142	42.832052
3501.847066	302771.605920	42.837057
3501.669239	302762.980818	42.842061
3501.293232	302733.364762	42.847066
3501.680994	302717.270643	42.852071
3501.388989	302703.878725	42.857076
3501.617203	302676.840455	42.862081
3501.389882	302672.905935	42.867085
3501.392501	302653.512568	42.872090
3501.551052	302643.562340	42.877095
3501.599584	302639.737393	42.882100
3501.894373	302622.741568	42.887105
3501.811386	302599.060456	42.892109
3501.566430	302591.107530	42.897114
3501.671247	302556.784236	42.902119
3501.436470	302553.792537	42.907124
3501.623169	302526.837031	42.912129
3501.698308	302511.707940	42.917133
3501.629192	302494.336310	42.922138
3501.440562	302481.997091	42.927143
3501.224048	302473.912449	42.932148
3501.704399	302455.996796	42.937153
3501.371047	302437.113982	42.942157
3501.330958	302421.061213	42.947162
3501.553445	302405.476397	42.952167
3501.441486	302395.212109	42.957172
3501.290539	302384.343102	42.962177
3501.499580	302368.582224	42.967181
3501.287386	302350.113096	42.972186
3501.555740	302337.091587	42.977191
3501.248577	302333.933038	42.982196
3501.567767	302309.170900	42.987201
3501.400653	302298.329853	42.992205
3501.033526	302292.864681	42.997210
3501.181450	302261.384912	43.002215
3501.694092	302253.975206	43.007220
3501.751545	302241.037547	43.012225
3501.423457	302224.724338	43.017229
3501.298583	302223.700579	43.022234
3501.503241	302209.721877	43.027239
3501.600375	302191.636992	43.032244
3501.737461	302171.357106	43.037249
3501.169166	302154.368813	43.042253
3501.243797	302135.014898	43.047258
3501.623217	302128.618575	43.052263
3501.217247	302120.512597	43.057268
3501.107056	302097.980790	43.062273
3501.257358	302098.415592	43.067277
3500.947717	302083.626491	43.072282
3501.468339	302077.717099	43.077287
3501.262362	302071.259586	43.082292
3501.276752	302039.673310	43.087297
3501.320656	302032.005997	43.092301
3501.357767	302021.336571	43.097306
3501.461129	302000.400175	43.102311
3501.519913	302000.518429	43.107316
3501.779971	301978.768557	43.112321
3501.310582	301974.388267	43.117325
3501.649286	301954.254932	43.122330
3501.664084	301941.934685	43.127335
3501.255652	301920.416555	43.132340
3501.537884	301915.435188	43.137345
3501.779636	301891.881144	43.142349
3501.251150	301889.571593	43.147354
3501.261812	301874.172442	43.152359
3501.424576	301855.797224	43.157364
3501.311348	301837.592402	43.162369
3501.617869	301831.181990	43.167373
3501.463792	301803.872182	43.172378
3501.604766	301802.883205	43.177383
3501.291364	301788.629075	43.182388
3501.401997	301765.375433	43.187393
3501.587053	301755.675403	43.192397
3501.500033	301740.062428	43.197402
3501.532384	301707.480566	43.202407
3501.373720	301702.440855	43.207412
3501.518507	301692.950716	43.212417
3501.130181	301679.242737	43.217421
3501.244174	301660.620569	43.222426
3501.610048	301649.008891	43.227431
3501.548730	301629.141579	43.232436
3501.200625	301616.190821	43.237441
3501.460253	301618.873659	43.242445
3501.538824	301607.357791	43.247450
3501.621506	301584.999219	43.252455
3501.307088	301578.889461	43.257460
3501.354672	301558.623335	43.262465
3500.925188	301535.555838	43.267469
3501.023301	301538.213030	43.272474
3501.502814	301525.463721	43.277479
3501.455607	301514.043849	43.282484
3501.531309	301498.659872	43.287489
3501.143681	301477.443720	43.292493
3500.817337	301491.696528	43.297498
3501.127509	301460.521782	43.302503
3501.159929	301454.866803	43.307508
3501.040374	301445.825161	43.312513
3501.041417	301433.074281	43.317517
3501.060521	301444.448043	43.322522
3501.316611	301422.774918	43.327527
3501.614525	301412.624516	43.332532
3501.261421	301393.082695	43.337537
3501.246627	301396.292016	43.342541
3501.023317	301370.367160	43.347546
3501.628678	301359.125193	43.352551
3501.272778	301357.399458	43.357556
3500.986214	301331.382670	43.362561
3501.517702	301317.708951	43.367565
3501.475660	301312.549167	43.372570
3501.387168	301298.132488	43.377575
3501.444679	301289.444902	43.382580
3501.258650	301284.129470	43.387585
3501.788582	301272.695669	43.392589
3501.396801	301250.182076	43.397594
3501.635783	301239.150070	43.402599
3501.473724	301233.041903	43.407604
3501.535238	301200.633331	43.412609
3501.674328	301192.060230	43.417613
3501.588595	301179.984584	43.422618
3501.589418	301158.071299	43.427623
3501.247640	301149.929685	43.432628
3501.344280	301130.215651	43.437633
3501.738248	301129.645227	43.442637
3501.214121	301105.523396	43.447642
3501.546309	301084.449064	43.452647
3501.238944	301072.967967	43.457652
3501.179209	301076.998767	43.462657
3501.424126	301054.970926	43.467661
3501.066614	301037.262143	43.472666
3501.177205	301021.948928	43.477671
3501.489381	301025.183506	43.482676
3501.504261	301008.332733	43.487681
3501.490382	300992.249985	43.492685
3501.447235	300981.440192	43.497690
3501.340730	300955.904093	43.502695
3501.176114	300952.290506	43.507700
3501.355220	300938.773587	43.512705
3501.332233	300939.159138	43.517709
3501.052529	300919.503864	43.522714
3501.450691	300894.830530	43.527719
3501.230459	300899.420910	43.532724
3501.116517	300890.505553	43.537729
3501.482039	300866.499039	43.542733
3501.065072	300856.816614	43.547738
3500.755595	300858.290454	43.552743
3501.140927	300850.544142	43.557748
3501.175555	300836.108091	43.562753
3501.648937	300825.141159	43.567757
3501.167928	300817.810249	43.572762
3501.436464	300793.946122	43.577767
3501.209729	300780.110844	43.582772
3500.889711	300770.362344	43.587777
3501.379505	300768.478923	43.592781
3500.830818	300768.157675	43.597786
3500.915786	300763.054335	43.602791
3501.115027	300746.810938	43.607796
3500.753958	300734.472822	43.612801
3500.819625	300723.442355	43.617805
3501.264945	300734.546023	43.622810
3501.220763	300727.554027	43.627815
3501.110660	300707.464940	43.632820
3501.473067	300695.802696	43.637825
3501.422373	300680.005575	43.642829
3501.347250	300688.620039	43.647834
3501.438461	300655.315701	43.652839
3501.359376	300650.899732	43.657844
3501.443423	300649.385156	43.662849
3501.342784	300623.466214	43.667853
3501.326128	300618.175137	43.672858
3501.313378	300605.069899	43.677863
3501.192887	300596.155518	43.682868
3501.266724	300580.135287	43.687873
3501.371644	300565.688175	43.692877
3501.657145	300568.137960	43.697882
3501.327104	300542.636613	43.702887
3501.421663	300540.178691	43.707892
3501.160357	300525.636116	43.712897
3501.219956	300501.422754	43.717901
3500.933484	300490.065523	43.722906
3501.385136	300481.519798	43.727911
3501.466010	300474.126448	43.732916
3501.010744	300468.573062	43.737921
3501.188896	300454.343533	43.742925
3501.011958	300434.341148	43.747930
3501.354778	300439.148956	43.752935
3501.370671	300435.990690	43.757940
3501.431750	300418.419871	43.762945
3501.620965	300394.288004	43.767949
3501.313777	300376.342073	43.772954
3501.145727	300365.628038	43.777959
3501.183998	300367.480198	43.782964
3501.105093	300357.464865	43.787969
3501.333992	300343.023761	43.792973
3501.520898	300327.876579	43.797978
3501.024827	300320.115282	43.802983
3500.977958	300321.115406	43.807988
3500.995604	300310.957712	43.812993
3501.515991	300284.559744	43.817997
3501.116201	300279.812112	43.823002
3501.424983	300268.005452	43.828007
3501.334129	300256.566685	43.833012
3501.351584	300238.060924	43.838017
3501.513833	300233.810803	43.843021
3501.257904	300224.230344	43.848026
3501.495539	300210.653191	43.853031
3501.355642	300192.528336	43.858036
3500.853063	300188.178538	43.863041
3501.581380	300175.491819	43.868045
3501.107807	300159.404338	43.873050
3500.992831	300149.063735	43.878055
3500.948867	300147.747320	43.883060
3501.145387	300151.789029	43.888065
3501.207346	300127.218811	43.893069
3501.177669	300110.425628	43.898074
3501.252119	300108.021734	43.903079
3500.930745	300119.321747	43.908084
3500.975382	300103.204135	43.913089
3501.271488	300073.965105	43.918093
3501.227525	300070.027177	43.923098
3501.398041	300062.339789	43.928103
3501.154564	300057.542248	43.933108
3501.006789	300035.091806	43.938113
3501.153992	300026.008221	43.943117
3500.981485	300020.716001	43.948122
3501.175508	300014.908349	43.953127
3501.053790	300021.544980	43.958132
3501.105947	300001.735682	43.963137
3501.364134	299981.105168	43.968141
3501.042938	299980.697445	43.973146
3501.094935	299982.165699	43.978151
3501.098908	299967.047016	43.983156
3501.283119	299949.431344	43.988161
3501.308250	299941.766669	43.993165
3501.272811	299948.720691	43.998170
3501.173990	299924.404582	44.003175
3501.291798	299914.740187	44.008180
3501.215407	299904.062635	44.013185
3501.265116	299902.247987	44.018189
3501.123565	299884.810482	44.023194
3501.026052	299865.737181	44.028199
3501.380039	299866.547386	44.033204
3501.041375	299865.277036	44.038209
3500.831292	299850.446304	44.043213
3500.758489	299846.563772	44.048218
3501.061411	299828.140500	44.053223
3501.052806	299817.223268	44.058228
3500.715505	299813.229375	44.063233
3500.957450	299818.969270	44.068237
3500.836244	299816.723210	44.073242
3500.888310	299813.686511	44.078247
3500.841637	299815.170195	44.083252
3501.392811	299793.552093	44.088257
3501.015305	299778.289385	44.093261
3500.907061	299777.186623	44.098266
3500.787208	299773.107828	44.103271
3501.018359	299774.242658	44.108276
3500.751022	299760.413468	44.113281
3501.200699	299758.434478	44.118285
3500.813442	299750.452473	44.123290
3501.175099	299735.048741	44.128295
3500.950549	299738.672729	44.133300
3501.132610	299734.088599	44.138305
3501.061307	299721.094109	44.143309
3501.145148	299702.526884	44.148314
3501.026019	299690.888806	44.153319
3501.078320	299683.016233	44.158324
3501.214620	299685.260319	44.163329
3501.678534	299676.636196	44.168333
3501.253164	299662.806236	44.173338
3501.394286	299649.294936	44.178343
3501.255596	299645.346335	44.183348
3501.049488	299632.169286	44.188353
3500.909913	299614.273254	44.193357
3500.954300	299616.989844	44.198362
3500.978566	299608.434445	44.203367
3500.807304	299608.512314	44.208372
3501.123738	299611.084566	44.213377
3501.169413	299594.635768	44.218381
3501.316611	299578.578322	44.223386
3501.305207	299573.260872	44.228391
3501.145362	299565.345093	44.233396
3501.442081	299549.722395	44.238401
3501.798467	299521.288104	44.243405
3500.982888	299522.153904	44.248410
3501.158962	299511.207738	44.253415
3500.854945	299493.031954	44.258420
3501.044016	299479.665826	44.263425
3501.403808	299472.355994	44.268429
3501.275803	299480.215361	44.273434
3501.247519	299447.539811	44.278439
3500.872720	299437.341502	44.283444
3501.061936	299442.020703	44.288449
3501.208660	299432.148087	44.293453
3501.576669	299430.232758	44.298458
3501.592244	299407.629261	44.303463
3501.486952	299400.621197	44.308468
3501.372105	299384.782826	44.313473
3501.523522	299364.652358	44.318477
3501.429068	299357.795305	44.323482
3501.476060	299334.346954	44.328487
3501.314858	299330.020071	44.333492
3501.127387	299329.336918	44.338497
3501.651474	299312.126040	44.343501
3500.744834	299294.298922	44.348506
3501.049422	299283.892562	44.353511
3501.129479	299274.641187	44.358516
3501.139596	299275.174286	44.363521
3501.069776	299274.930873	44.368525
3501.202957	299254.599600	44.373530
3501.231479	299235.786346	44.378535
3500.979612	299226.815924	44.383540
3501.501300	299227.498112	44.388545
3501.028608	299215.762497	44.393549
3500.823153	299213.504132	44.398554
3501.110559	299188.567372	44.403559
3501.466171	299182.632561	44.408564
3501.199616	299176.845923	44.413569
3501.375709	299158.874939	44.418573
3501.137951	299154.865435	44.423578
3501.492036	299151.985098	44.428583
3501.149494	299133.153466	44.433588
3500.941506	299115.878815	44.438593
3501.141822	299113.200680	44.443597
3501.095244	299110.128460	44.448602
3501.120751	299103.456237	44.453607
3500.944251	299080.831731	44.458612
3501.176283	299072.345575	44.463617
3501.135423	299070.061471	44.468621
3500.769737	299073.071267	44.473626
3501.174341	299065.194431	44.478631
3501.511174	299052.288687	44.483636
3500.996830	299035.672756	44.488641
3501.329823	299033.941051	44.493645
3501.107201	299029.343775	44.498650
3501.187791	299012.914797	44.503655
3501.129928	298993.122337	44.508660
3501.427926	298990.657993	44.513665
3501.327229	298983.191020	44.518669
3501.172504	298968.529559	44.523674
3501.193260	298950.404628	44.528679
3501.453418	298948.531596	44.533684
3501.380502	298942.256522	44.538689
3501.368191	298926.529249	44.543693
3501.410111	298908.859134	44.548698
3501.040010	298897.998236	44.553703
3501.056680	298888.044047	44.558708
3501.041678	298870.713696	44.563713
3501.175911	298861.377426	44.568717
3501.145285	298862.196872	44.573722
3501.004383	298848.704015	44.578727
3500.886929	298864.273813	44.583732
3500.772215	298837.694470	44.588737
3500.937399	298826.698967	44.593741
3501.039227	298824.545258	44.598746
3501.158021	298817.273017	44.603751
3501.273764	298816.975138	44.608756
3500.661789	298814.016748	44.613761
3501.030897	298796.804487	44.618765
3500.968186	298792.818494	44.623770
3500.614528	298783.125802	44.628775
3500.906704	298782.698531	44.633780
3500.840010	298775.328023	44.638785
3501.369324	298772.980218	44.643789
3500.893634	298776.847149	44.648794
3501.153570	298757.081276	44.653799
3501.008598	298743.869003	44.658804
3500.946988	298733.316173	44.663809
3500.999310	298727.148757	44.668813
3500.621225	298722.652116	44.673818
3500.996594	298733.079919	44.678823
3500.652578	298725.930926	44.683828
3501.009222	298721.421227	44.688833
3501.342037	298697.342520	44.693837
3500.800613	298692.107848	44.698842
3500.774333	298682.491216	44.703847
3501.100462	298679.640677	44.708852
3501.099659	298684.553268	44.713857
3501.032364	298666.162036	44.718861
3501.201298	298649.413712	44.723866
3500.881602	298642.515429	44.728871
3501.387148	298643.174696	44.733876
3500.949939	298643.421405	44.738881
3501.486049	298636.211158	44.743885
3501.266429	298613.389585	44.748890
3501.369210	298603.218265	44.753895
3501.357803	298594.413764	44.758900
3501.250018	298578.421344	44.763905
3501.194856	298568.071093	44.768909
3500.633266	298567.370062	44.773914
3501.210666	298558.778929	44.778919
3501.257589	298557.295552	44.783924
3501.469758	298540.514984	44.788929
3501.512903	298523.888097	44.793933
3501.558692	298518.561604	44.798938
3501.433956	298496.310550	44.803943
3500.962742	298490.352218	44.808948
3500.879771	298495.455838	44.813953
3501.233315	298475.318898	44.818957
3501.045213	298465.422100	44.823962
3501.034931	298461.351530	44.828967
3501.237852	298452.589855	44.833972
3500.909283	298451.216085	44.838977
3501.376396	298440.555087	44.843981
3501.097868	298422.044084	44.848986
3501.341553	298403.349624	44.853991
3501.153873	298404.829939	44.858996
3501.065773	298400.109769	44.864001
3501.100371	298378.750043	44.869005
3501.021352	298360.233281	44.874010
3500.985781	298369.198258	44.879015
3501.044863	298361.731674	44.884020
3500.852958	298362.932675	44.889025
3501.108364	298352.228401	44.894029
3501.077515	298340.398069	44.899034
3501.058575	298332.689156	44.904039
3501.302249	298328.858849	44.909044
3501.060371	298316.501553	44.914049
3501.013989	298311.291259	44.919053
3500.942005	298295.293160	44.924058
3500.902108	298281.478946	44.929063
3501.058251	298278.960391	44.934068
3501.188470	298276.776770	44.939073
3501.225789	298275.294887	44.944077
3500.946358	298267.321262	44.949082
3501.173143	298245.753270	44.954087
3500.988171	298240.946423	44.959092
3500.718699	298240.123361	44.964097
3500.883683	298239.130566	44.969101
3501.293209	298246.727904	44.974106
3501.017963	298218.162622	44.979111
3501.497567	298209.586725	44.984116
3501.097654	298211.202035	44.989121
3501.042113	298193.750549	44.994125
3501.389178	298189.191400	44.999130
3501.108895	298171.571424	45.004135
3501.110518	298153.296510	45.009140
3501.203159	298155.547484	45.014145
3501.293228	298145.479878	45.019149
3501.270857	298122.805432	45.024154
3501.242035	298119.144975	45.029159
3501.619196	298113.766636	45.034164
3501.006186	298103.274440	45.039169
3501.279241	298073.859789	45.044173
3501.011334	298069.905825	45.049178
3501.056012	298074.658644	45.054183
3501.255486	298056.200052	45.059188
3501.155298	298041.606177	45.064193
3501.461504	298040.184060	45.069197
3501.366309	298033.937819	45.074202
3501.399987	298022.275500	45.079207
3501.205036	297999.882511	45.084212
3501.321680	297994.290365	45.089217
3501.454317	297987.270377	45.094221
3501.405567	297969.334161	45.099226
3501.049026	297958.420054	45.104231
3501.110591	297954.720002	45.109236
3501.140578	297950.439478	45.114241
3501.139041	297926.259997	45.119245
3500.891341	297909.831114	45.124250
3501.214417	297910.468013	45.129255
3501.334860	297901.642789	45.134260
3501.041837	297892.042271	45.139265
3500.938294	297879.790514	45.144269
3501.103662	297875.412462	45.149274
3500.972663	297868.306413	45.154279
3500.946793	297870.092328	45.159284
3500.781393	297862.813489	45.164289
3501.255754	297850.751354	45.169293
3501.153520	297841.120999	45.174298
3501.074562	297827.720020	45.179303
3501.400694	297819.626204	45.184308
3501.092057	297824.663355	45.189313
3501.101243	297803.485549	45.194317
3501.066505	297797.687977	45.199322
3501.134976	297781.922300	45.204327
3501.018074	297785.911373	45.209332
3501.000508	297786.805151	45.214337
3501.193072	297762.086201	45.219341
3501.063405	297751.442014	45.224346
3501.053424	297739.786462	45.229351
3501.148875	297741.655224	45.234356
3500.902291	297742.203018	45.239361
3500.685919	297727.729036	45.244365
3500.775759	297709.389281	45.249370
3500.842072	297702.303268	45.254375
3501.289525	297703.022536	45.259380
3500.857182	297705.762846	45.264385
3500.704949	297693.976808	45.269389
3500.809725	297696.404072	45.274394
3500.327608	297698.286774	45.279399
3500.999276	297696.731155	45.284404
3500.841507	297696.017884	45.289409
3501.351771	297681.124856	45.294413
3501.184950	297666.210416	45.299418
3501.082109	297649.936978	45.304423
3501.373689	297654.193084	45.309428
3500.839859	297655.600271	45.314433
3501.268352	297626.135633	45.319437
3501.313901	297627.401336	45.324442
3500.743458	297616.469698	45.329447
3501.030578	297611.309009	45.334452
3500.836389	297612.714004	45.339457
3501.036608	297597.131299	45.344461
3500.936268	297588.951408	45.349466
3501.147683	297570.185357	45.354471
3501.232947	297565.361656	45.359476
3500.651916	297572.986685	45.364481
3500.948091	297568.053652	45.369485
3500.831954	297567.893830	45.374490
3500.682303	297544.831807	45.379495
3500.673074	297529.052753	45.384500
3500.691622	297522.330524	45.389505
3500.629360	297520.940548	45.394509
3500.794023	297517.097086	45.399514
3500.859218	297527.090005	45.404519
3501.277093	297517.989146	45.409524
3501.153282	297513.096316	45.414529
3501.250812	297509.059727	45.419533
3501.231547	297491.525993	45.424538
3501.092815	297486.788210	45.429543
3501.276258	297478.563936	45.434548
3500.943075	297484.673970	45.439553
3500.994005	297460.333369	45.444557
3500.952487	297451.507943	45.449562
3500.967882	297440.611945	45.454567
3501.312082	297435.671392	45.459572
3501.087681	297440.746312	45.464577
3501.248591	297433.060063	45.469581
3500.896306	297414.509353	45.474586
3501.240805	297401.983823	45.479591
3500.731019	297381.497862	45.484596
3501.206918	297397.789792	45.489601
3500.939249	297383.756439	45.494605
3500.694386	297386.976509	45.499610
3500.471265	297365.045822	45.504615
3500.746384	297363.806718	45.509620
3500.641451	297362.194335	45.514625
3500.847728	297351.955702	45.519629
3500.820979	297349.389341	45.524634
3500.949567	297353.085537	45.529639
3500.832975	297348.598809	45.534644
3500.814099	297340.762485	45.539649
3501.053497	297351.593596	45.544653
3500.940270	297347.360870	45.549658
3500.977108	297338.981327	45.554663
3500.922136	297319.518708	45.559668
3500.951193	297319.717979	45.564673
3501.114472	297310.784154	45.569677
3500.741317	297308.653741	45.574682
3500.629057	297305.108086	45.579687
3501.064663	297310.308908	45.584692
3500.954840	297314.984135	45.589697
3501.424577	297291.214305	45.594701
3501.048288	297283.128418	45.599706
3500.915537	297289.130778	45.604711
3501.383358	297276.178695	45.609716
3501.393065	297276.660971	45.614721
3501.150659	297252.264329	45.619725
3501.118812	297244.175492	45.624730
3501.068634	297234.333272	45.629735
3501.435293	297215.033776	45.634740
3500.919526	297212.620220	45.639745
3501.328634	297195.732103	45.644749
3501.053822	297201.222172	45.649754
3501.343640	297193.286661	45.654759
3501.203561	297168.543098	45.659764
3500.878890	297162.867147	45.664769
3501.177003	297154.930334	45.669773
3500.917761	297158.967159	45.674778
3500.809712	297158.347919	45.679783
3500.968319	297132.564981	45.684788
3501.177669	297125.787422	45.689793
3501.147514	297116.934714	45.694797
3501.096517	297127.938533	45.699802
3500.824100	297117.291092	45.704807
3501.322348	297108.966643	45.709812
3500.992818	297087.688806	45.714817
3500.897963	297071.159424	45.719821
3500.856502	297075.314924	45.724826
3500.709105	297056.477535	45.729831
3500.860000	296997.225119	45.734836
3500.948081	296909.933260	45.739841
3500.999742	296758.403448	45.744845
3500.587971	296573.322081	45.749850
3500.284993	296319.957490	45.754855
3500.453549	296030.679692	45.759860
3500.143849	295697.338790	45.764865
3499.650997	295310.342752	45.769869
3499.651465	294880.529936	45.774874
3499.022403	294397.511510	45.779879
3498.889250	293873.481043	45.784884
3498.186463	293302.189518	45.789889
3497.882265	292663.629473	45.794893
3497.304829	291993.566510	45.799898
3496.493222	291283.720541	45.804903
3496.245017	290511.360888	45.809908
3495.131867	289706.161320	45.814913
3494.825891	288852.916369	45.819917
3493.978083	287947.482060	45.824922
3492.821299	286990.380029	45.829927
3492.396024	285999.469478	45.834932
3491.626135	284960.940994	45.839937
3490.561377	283859.128024	45.844941
3489.388205	282729.717302	45.849946
3488.447899	281560.637782	45.854951
3487.702176	280323.684710	45.859956
3486.506809	279057.145834	45.864961
3485.147413	277738.061110	45.869965
3484.450507	276380.837327	45.874970
3482.863888	274977.619109	45.879975
3481.709412	273524.658884	45.884980
3480.371103	272039.569101	45.889985
3479.226203	270508.158150	45.894989
3477.762757	268922.483679	45.899994
3476.427636	267310.662095	45.904999
3475.066706	265643.128096	45.910004
3473.127280	263955.030838	45.915009
3471.925559	262223.195483	45.920013
3469.978575	260436.852098	45.925018
3468.494221	258629.654375	45.930023
3467.172374	256767.219787	45.935028
3465.208721	254883.466990	45.940033
3463.595058	252946.612079	45.945037
3461.792817	250981.085293	45.950042
3459.614985	248981.237413	45.955047
3457.738097	246937.336625	45.960052
3455.821768	244870.269425	45.965057
3453.625762	242767.366226	45.970061
3451.646892	240632.650991	45.975066
3449.729831	238476.515239	45.980071
3447.751500	236275.421653	45.985076
3445.256881	234045.692192	45.990081
3442.806191	231778.836763	45.995085
3440.872650	229491.058438	46.000090
3438.193837	227169.237013	46.005095
3436.028343	224818.425211	46.010100
3433.346594	222443.371560	46.015105
3430.939366	220038.658215	46.020109
3428.563938	217612.349424	46.025114
3425.798774	215161.025606	46.030119
3423.759560	212680.364942	46.035124
3420.466267	210173.813941	46.040129
3417.811667	207637.031747	46.045133
3415.237797	205095.119891	46.050138
3411.894966	202528.452655	46.055143
3409.377708	199936.429325	46.060148
3406.189945	197321.734017	46.065153
3403.092010	194700.322545	46.070157
3400.159585	192053.445128	46.075162
3396.862768	189393.006526	46.080167
3393.659223	186718.966168	46.085172
3390.060614	184028.197635	46.090177
3386.805537	181339.816174	46.095181
3383.157769	178623.895883	46.100186
3379.740249	175916.183856	46.105191
3376.288225	173181.717136	46.110196
3372.342728	170460.827096	46.115201
3369.205150	167716.398475	46.120205
3365.428032	164975.866966	46.125210
3361.207478	162230.933061	46.130215
3357.492744	159469.922560	46.135220
3353.154139	156733.950189	46.140225
3348.414046	153978.706796	46.145229
3344.428886	151251.665715	46.150234
3339.519696	148543.915322	46.155239
3334.401895	145830.723384	46.160244
3329.115680	143160.809853	46.165249
3323.178741	140499.360455	46.170253
3318.012507	137879.833158	46.175258
3311.450739	135217.492387	46.180263
3305.534683	132662.166732	46.185268
3299.021465	130174.971649	46.190273
3292.461687	127710.797941	46.195277
3285.455224	125303.451407	46.200282
3278.199248	122973.714592	46.205287
3271.410716	120697.568816	46.210292
3263.545943	118481.124270	46.215297
3255.583395	116343.243704	46.220301
3247.639739	114289.480057	46.225306
3239.257124	112314.947091	46.230311
3230.541309	110434.874174	46.235316
3221.167020	108648.739573	46.240321
3212.044322	106959.172241	46.245325
3203.069346	105363.772919	46.250330
3194.247071	103876.066562	46.255335
3185.750528	102477.632456	46.260340
3176.685029	101188.631874	46.265345
3168.644167	99980.154701	46.270349
3161.162448	98854.006448	46.275354
3153.185708	97816.583973	46.280359
3145.932416	96853.429040	46.285364
3138.857343	95968.293152	46.290369
3132.194262	95155.376550	46.295373
3125.862252	94396.082035	46.300378
3119.550569	93700.213840	46.305383
3113.692441	93059.465669	46.310388
3108.094713	92479.353830	46.315393
3102.897328	91919.521385	46.320397
3097.922392	91419.461977	46.325402
3093.319949	90946.493573	46.330407
3088.726206	90505.119020	46.335412
3084.749587	90080.617078	46.340417
3080.519007	89685.092262	46.345421
3076.869747	89296.088765	46.350426
3072.746237	88935.002506	46.355431
3069.549899	88568.972966	46.360436
3065.895960	88229.789597	46.365441
3061.969948	87893.981414	46.370445
3058.776053	87566.956084	46.375450
3055.523804	87245.254154	46.380455
3052.088956	86903.879220	46.385460
3049.280406	86585.990070	46.390465
3045.794152	86257.932431	46.395469
3042.740749	85940.457018	46.400474
3039.169230	85615.062445	46.405479
3035.796677	85289.869073	46.410484
3032.441758	84985.256929	46.415489
3029.062257	84661.989985	46.420493
3025.891876	84345.579328	46.425498
3022.058631	84019.100309	46.430503
3018.647689	83702.454869	46.435508
3015.631773	83387.453380	46.440513
3011.887692	83070.257276	46.445517
3008.683905	82747.174964	46.450522
3004.874302	82436.754116	46.455527
3001.793256	82116.581415	46.460532
2997.860430	81802.083828	46.465537
2994.391812	81477.952265	46.470541
2991.122138	81175.742749	46.475546
2987.453764	80866.498362	46.480551
2983.960870	80552.962084	46.485556
2980.321255	80250.883883	46.490561
2976.378724	79947.039979	46.495565
2973.069282	79643.100377	46.500570
2969.494922	79345.848350	46.505575
2965.955623	79042.154483	46.510580
2962.064658	78750.648509	46.515585
2958.625058	78457.627105	46.520589
2955.267010	78156.581819	46.525594
2951.453558	77880.212331	46.530599
2947.992132	77592.893459	46.535604
2944.617828	77308.167564	46.540609
2940.623442	77014.511672	46.545613
2936.752786	76722.516009	46.550618
2933.452415	76448.722366	46.555623
2929.761079	76171.792237	46.560628
2926.375569	75901.370199	46.565633
2922.764923	75630.439981	46.570637
2918.916454	75354.800036	46.575642
2915.125505	75096.564818	46.580647
2911.463806	74831.517732	46.585652
2907.814974	74570.458785	46.590657
2904.063131	74311.882102	46.595661
2900.556425	74056.660190	46.600666
2897.265447	73808.759588	46.605671
2893.412787	73552.021941	46.610676
2889.626776	73310.082887	46.615681
2886.519649	73052.522331	46.620685
2883.191369	72808.306718	46.625690
2879.066427	72561.437033	46.630695
2875.684429	72319.596190	46.635700
2872.203811	72074.077864	46.640705
2869.014602	71828.046422	46.645709
2865.727666	71581.765904	46.650714
2861.870233	71340.097274	46.655719
2858.892357	71103.334222	46.660724
2855.137756	70850.302428	46.665729
2851.368549	70606.607865	46.670733
2847.780930	70359.243086	46.675738
2844.643394	70111.556314	46.680743
2841.312260	69859.604262	46.685748
2837.675606	69623.649620	46.690753
2834.022461	69385.128618	46.695757
2830.380875	69142.760938	46.700762
2826.724076	68898.753713	46.705767
2823.803609	68651.726164	46.710772
2820.178676	68403.382831	46.715777
2816.582939	68164.635570	46.720781
2813.208428	67914.213712	46.725786
2809.404114	67676.138404	46.730791
2806.068154	67431.498184	46.735796
2802.388310	67178.763500	46.740801
2799.052641	66945.947487	46.745805
2796.031563	66689.534474	46.750810
2792.349819	66440.089145	46.755815
2788.808691	66194.001168	46.760820
2785.377487	65956.968959	46.765825
2781.773011	65705.595456	46.770829
2778.133123	65453.842795	46.775834
2774.739184	65208.744239	46.780839
2771.500564	64959.301288	46.785844
2768.124354	64722.456107	46.790849
2764.540266	64468.311651	46.795853
2761.078192	64222.503417	46.800858
2757.520538	63961.835164	46.805863
2754.209145	63718.451895	46.810868
2750.442073	63468.071842	46.815873
2747.132575	63221.126170	46.820877
2743.589404	62960.675526	46.825882
2739.338113	62718.965878	46.830887
2736.299243	62460.764473	46.835892
2732.950637	62224.655790	46.840897
2729.492693	61976.000389	46.845901
2726.155360	61722.784574	46.850906
2722.259414	61466.809205	46.855911
2718.979523	61215.474475	46.860916
2715.732332	60974.500600	46.865921
2711.826935	60722.170840	46.870925
2708.534654	60463.776085	46.875930
2704.886916	60208.574592	46.880935
2701.534319	59959.732686	46.885940
2698.083875	59704.962495	46.890945
2694.388482	59455.011697	46.895949
2691.138393	59204.092710	46.900954
2687.269813	58947.752275	46.905959
2684.227520	58696.209526	46.910964
2680.477985	58448.968091	46.915969
2677.221958	58190.369653	46.920973
2673.602440	57928.531200	46.925978
2669.801681	57687.619282	46.930983
2666.730286	57424.380722	46.935988
2662.997383	57174.941555	46.940993
2659.761046	56915.776281	46.945997
2656.042095	56661.289501	46.951002
2652.805628	56413.036933	46.956007
2649.035325	56147.624778	46.961012
2645.096874	55904.823416	46.966017
2641.755261	55642.928349	46.971021
2638.541031	55388.902794	46.976026
2634.538277	55139.501690	46.981031
2631.334257	54884.407671	46.986036
2627.855462	54648.723029	46.991041
2624.221071	54392.299472	46.996045
2621.125734	54122.693103	47.001050
2617.320788	53883.406364	47.006055
2614.178261	53625.816616	47.011060
2610.592710	53369.548797	47.016065
2606.967829	53113.841866	47.021069
2603.644154	52859.042223	47.026074
2600.398126	52602.894612	47.031079
2596.375378	52338.478239	47.036084
2593.362071	52076.006789	47.041089
2589.634139	51820.171519	47.046093
2586.332367	51570.800118	47.051098
2582.598381	51311.685321	47.056103
2579.191906	51052.078134	47.061108
2575.689680	50798.115550	47.066113
2572.163184	50532.849141	47.071117
2568.182289	50274.476005	47.076122
2564.760204	50025.717302	47.081127
2561.416884	49758.578885	47.086132
2558.197173	49505.024019	47.091137
2554.225095	49249.547156	47.096141
2550.954509	48987.614021	47.101146
2547.428650	48734.965521	47.106151
2544.325627	48463.098107	47.111156
2540.322153	48213.606386	47.116161
2537.235526	47963.035250	47.121165
2533.589398	47703.776108	47.126170
2529.915003	47436.887836	47.131175
2526.418913	47178.429414	47.136180
2522.757401	46925.999793	47.141185
2519.286709	46659.564491	47.146189
2515.899390	46405.474132	47.151194
2512.660190	46150.640447	47.156199
2508.951532	45878.321582	47.161204
2505.436723	45614.588262	47.166209
2501.960190	45364.772808	47.171213
2498.767628	45098.769083	47.176218
2495.343484	44831.276347	47.181223
2492.086390	44572.930931	47.186228
2488.254940	44305.457465	47.191233
2484.420584	44042.204865	47.196237
2481.309684	43786.293568	47.201242
2477.585454	43521.076696	47.206247
2474.376294	43253.429747	47.211252
2470.635353	42995.831488	47.216257
2467.181926	42732.268490	47.221261
2463.940658	42458.814865	47.226266
2460.201548	42194.465932	47.231271
2457.169786	41936.496417	47.236276
2453.447468	41663.134252	47.241281
2449.857012	41389.342700	47.246285
2446.473655	41119.231546	47.251290
2442.803653	40860.613607	47.256295
2439.204721	40591.994711	47.261300
2435.598450	40329.498936	47.266305
2432.155684	40057.102218	47.271309
2429.054696	39792.536601	47.276314
2425.281241	39525.219895	47.281319
2421.623524	39252.353309	47.286324
2418.229025	38983.766656	47.291329
2414.833655	38712.691800	47.296333
2411.295629	38440.488770	47.301338
2408.016555	38179.324579	47.306343
2404.302986	37905.038216	47.311348
2400.819348	37629.495795	47.316353
2397.642543	37370.791594	47.321357
2394.245648	37078.283902	47.326362
2390.658274	36820.411323	47.331367
2387.158271	36533.791294	47.336372
2383.494721	36261.819347	47.341377
2380.309372	35989.497126	47.346381
2377.278915	35708.761000	47.351386
2372.728363	35430.485084	47.356391
2369.470752	35146.755458	47.361396
2365.999004	34872.951944	47.366401
2362.358260	34607.361936	47.371405
2359.262566	34320.480283	47.376410
2355.486210	34044.218636	47.381415
2351.984216	33770.624294	47.386420
2348.921407	33492.084096	47.391425
2345.296250	33214.167994	47.396429
2341.875807	32927.134271	47.401434
2338.324500	32658.024365	47.406439
2334.885408	32365.993971	47.411444
2331.744882	32081.095729	47.416449
2327.927774	31804.914312	47.421453
2324.700495	31511.462021	47.426458
2321.274532	31228.363030	47.431463
2317.639173	30933.664451	47.436468
2314.085768	30644.439356	47.441473
2310.604412	30359.662377	47.446477
2307.363502	30074.072183	47.451482
2303.386081	29788.341327	47.456487
2300.561370	29498.992905	47.461492
2296.877766	29198.261759	47.466497
2292.862251	28911.028094	47.471501
2289.878722	28608.966635	47.476506
2286.427594	28325.328384	47.481511
2282.974010	28024.591129	47.486516
2279.655028	27733.336127	47.491521
2275.567841	27442.180118	47.496525
2272.611011	27137.576181	47.501530
2268.757572	26852.576590	47.506535
2265.393503	26544.370056	47.511540
2262.050104	26242.666068	47.516545
2258.548509	25949.424884	47.521549
2255.095031	25652.486438	47.526554
2251.406196	25349.151730	47.531559
2248.142039	25043.448849	47.536564
2245.088734	24746.942665	47.541569
2241.323990	24442.226933	47.546573
2238.171251	24127.891201	47.551578
2234.417895	23825.825038	47.556583
2230.694939	23514.287114	47.561588
2227.200874	23202.325444	47.566593
2223.591079	22902.886305	47.571597
2220.875155	22581.746790	47.576602
2217.147837	22281.613176	47.581607
2213.858901	21967.611536	47.586612
2210.350318	21652.318905	47.591617
2206.444533	21342.997478	47.596621
2203.174951	21011.466916	47.601626
2199.715599	20704.790559	47.606631
2196.648720	20392.698586	47.611636
2192.884049	20062.357325	47.616641
2189.296390	19751.129816	47.621645
2185.808232	19421.015798	47.626650
2182.647457	19104.157698	47.631655
2178.944527	18775.773041	47.636660
2175.646527	18449.091373	47.641665
2171.858300	18130.238081	47.646669
2169.208985	17795.289000	47.651674
2165.373169	17471.254034	47.656679
2161.775908	17146.408149	47.661684
2158.345743	16816.208902	47.666689
2154.634644	16479.928685	47.671693
2151.205845	16150.715923	47.676698
2147.461305	15828.255352	47.681703
2144.074533	15491.555335	47.686708
2140.728166	15170.861044	47.691713
2136.751375	14842.408719	47.696717
2133.802634	14512.819633	47.701722
2130.197790	14186.957893	47.706727
2126.933915	13847.870724	47.711732
2123.295362	13520.743347	47.716737
2119.918035	13187.672838	47.721741
2116.358683	12850.248556	47.726746
2112.343253	12514.652416	47.731751
2108.355692	12182.011658	47.736756
2104.836010	11872.316111	47.741761
2101.144480	11562.221990	47.746765
2097.335352	11246.427707	47.751770
2092.918431	10952.915853	47.756775
2086.744340	10710.726498	47.761780
2081.630618	10477.877552	47.766785
2077.028169	10239.671332	47.771789
2072.973401	10017.286117	47.776794
2068.744789	9818.092741	47.781799
2064.758229	9623.032550	47.786804
2061.260830	9435.456935	47.791809
2057.792138	9252.569857	47.796813
2053.925282	9059.085891	47.801818
2050.425850	8882.883045	47.806823
2047.161201	8701.422367	47.811828
2044.071187	8525.757099	47.816833
2040.438741	8349.383894	47.821837
2037.378705	8166.842410	47.826842
2033.846942	8000.401918	47.831847
2030.269118	7814.827215	47.836852
2027.173735	7635.683238	47.841857
2023.739726	7464.335830	47.846861
2020.627648	7274.579055	47.851866
2017.601672	7093.422836	47.856871
2014.111719	6909.919768	47.861876
2010.853482	6714.209779	47.866881
2007.324818	6538.597270	47.871885
2004.238465	6346.431200	47.876890
2000.445503	6159.299099	47.881895
1996.572170	5961.895736	47.886900
1993.385369	5772.504823	47.891905
1989.462454	5593.076691	47.896909
1986.263409	5394.602361	47.901914
1982.811229	5209.860353	47.906919
1979.450755	5026.833786	47.911924
1976.089921	4830.340360	47.916929
1972.645773	4651.115586	47.921933
1969.207838	4453.081308	47.926938
1965.800554	4261.449443	47.931943
1962.323453	4070.498240	47.936948
1958.728994	3872.209987	47.941953
1955.425402	3694.925152	47.946957
1951.831049	3495.372065	47.951962
1948.229491	3306.024281	47.956967
1944.662073	3116.970589	47.961972
1941.475829	2921.182521	47.966977
1937.784506	2745.825130	47.971981
1934.342471	2554.153512	47.976986
1930.705085	2363.447949	47.981991
1926.917990	2176.011127	47.986996
1923.056161	1979.215734	47.992001
1919.504352	1809.215218	47.997005
1915.918090	1623.350625	48.002010
1912.066774	1444.066380	48.007015
1908.477048	1269.292868	48.012020
1905.060617	1103.210760	48.017025
1901.308606	949.215287	48.022029
1897.690380	772.055975	48.027034
1893.933068	622.436720	48.032039
1889.822178	454.264081	48.037044
1885.807228	300.954465	48.042049
1881.434994	168.596023	48.047053
1876.847681	56.479490	48.052058
1869.024013	35.500365	48.057063
1861.990991	56.792584	48.062068
1856.862885	58.892430	48.067073
1852.566388	56.869409	48.072077
1850.089646	61.376469	48.077082
1847.161315	61.989941	48.082087
1844.571462	61.629777	48.087092
1841.457720	60.851713	48.092097
1838.663481	66.297493	48.097101
1836.034396	66.240868	48.102106
1832.410420	65.681863	48.107111
1828.845992	70.409763	48.112116
1825.688868	59.011246	48.117121
1821.397192	72.430055	48.122125
1817.964201	57.964683	48.127130
1815.032031	61.521110	48.132135
1811.344446	68.115955	48.137140
1808.789714	62.897014	48.142145
1805.182154	64.641868	48.147149
1801.870023	64.831352	48.152154
1798.050655	59.266149	48.157159
1794.224913	66.584985	48.162164
1791.083456	64.286317	48.167169
1787.518822	62.164609	48.172173
1784.448108	62.291007	48.177178
1780.715660	66.184660	48.182183
1777.545115	63.596314	48.187188
1773.981350	52.403831	48.192193
1770.118057	62.117226	48.197197
1766.887839	64.062473	48.202202
1763.291217	66.140993	48.207207
1759.750202	68.796118	48.212212
1756.634605	46.969544	48.217217
1753.118266	65.417708	48.222221
1749.960112	63.548781	48.227226
1746.409574	60.595964	48.232231
1742.557447	66.732517	48.237236
1739.520197	64.430212	48.242241
1735.337814	62.705763	48.247245
1731.964064	65.429633	48.252250
1729.003799	59.195324	48.257255
1725.469393	63.203535	48.262260
1721.845708	52.020453	48.267265
1718.295616	58.647589	48.272269
1714.695792	54.946348	48.277274
1711.663167	60.211160	48.282279
1707.543462	60.160060	48.287284
1704.606464	64.764491	48.292289
1700.744563	65.587388	48.297293
1697.616962	60.439153	48.302298
1694.043374	59.062376	48.307303
1690.452480	64.294341	48.312308
1687.345363	59.155560	48.317313
1683.748716	56.219475	48.322317
1680.317167	57.221803	48.327322
1676.306984	63.468536	48.332327
1672.996072	66.581229	48.337332
1669.690218	61.413445	48.342337
1666.075359	63.928294	48.347341
1662.627464	62.724848	48.352346
1659.582826	55.016779	48.357351
1655.275809	58.734635	48.362356
1652.304467	59.085970	48.367361
1648.406745	67.292491	48.372365
1644.959444	68.945878	48.377370
1642.079143	63.132523	48.382375
1638.427688	59.334985	48.387380
1634.949320	69.380490	48.392385
1631.188224	66.242366	48.397389
1627.708600	56.979355	48.402394
1624.091079	64.537741	48.407399
1620.628194	63.558123	48.412404
1617.370946	63.612524	48.417409
1613.644136	64.765491	48.422413
1610.223784	62.539007	48.427418
1606.627808	55.724019	48.432423
1603.119305	63.951894	48.437428
1599.516433	44.792824	48.442433
1596.011527	64.662938	48.447437
1593.122791	64.096512	48.452442
1589.520917	64.046670	48.457447
1585.843413	54.938037	48.462452
1582.531801	60.585074	48.467457
1579.046056	61.728798	48.472461
1575.157609	56.278906	48.477466
1572.083985	61.961465	48.482471
1568.068335	59.075184	48.487476
1564.901693	53.388935	48.492481
1561.416170	51.220127	48.497485
1558.064622	44.980685	48.502490
1554.314063	49.484693	48.507495
1550.540717	50.837958	48.512500
1547.216713	42.610505	48.517505
1543.608391	54.881536	48.522509
1540.316075	51.812450	48.527514
1536.686331	53.121097	48.532519
1533.008418	56.209015	48.537524
1530.394099	47.686985	48.542529
1526.692114	58.501515	48.547533
1522.986889	50.422324	48.552538
1519.147545	56.076047	48.557543
1515.643758	48.734134	48.562548
1512.654758	58.117764	48.567553
1508.780868	59.752542	48.572557
1505.517856	45.868170	48.577562
1501.947883	61.559609	48.582567
1498.196575	57.910636	48.587572
1495.136915	54.362216	48.592577
1490.972856	48.249976	48.597581
1487.723620	55.785555	48.602586
1484.766885	56.333971	48.607591
1480.929727	58.162329	48.612596
1477.544498	57.047217	48.617601
1473.533721	58.007398	48.622605
1470.282830	53.837176	48.627610
1466.593155	55.569687	48.632615
1463.169543	51.730229	48.637620
1460.075390	50.344933	48.642625
1456.610224	56.788006	48.647629
1453.120257	63.681061	48.652634
1449.628348	56.856176	48.657639
1445.887119	57.413502	48.662644
1442.694028	46.552298	48.667649
1438.822455	60.857759	48.672653
1435.043510	59.019668	48.677658
1431.753892	57.889607	48.682663
1428.083623	62.368437	48.687668
1425.490316	50.334497	48.692673
1421.716582	54.117668	48.697677
1418.153602	53.947903	48.702682
1414.553090	56.802280	48.707687
1410.834511	57.833807	48.712692
1407.281479	46.351907	48.717697
1403.570522	55.301233	48.722701
1400.095500	53.962919	48.727706
1396.760820	51.606042	48.732711
1392.841515	56.804082	48.737716
1390.099261	43.274851	48.742721
1386.425960	67.391870	48.747725
1382.747294	57.869050	48.752730
1379.188704	42.053631	48.757735
1375.897097	56.179733	48.762740
1372.582289	45.964044	48.767745
1369.204326	52.434621	48.772749
1365.462123	65.625180	48.777754
1362.053632	47.416582	48.782759
1358.367752	54.919304	48.787764
1354.834160	35.306596	48.792769
1351.532080	52.148876	48.797773
1347.667435	45.205213	48.802778
1344.362842	56.071481	48.807783
1340.722780	57.229950	48.812788
1337.447932	49.861765	48.817793
1333.476152	55.574247	48.822797
1330.180215	47.851857	48.827802
1327.500884	60.021815	48.832807
1323.738681	55.982307	48.837812
1320.242997	44.668644	48.842817
1316.461040	48.873923	48.847821
1312.490552	59.717889	48.852826
1309.369494	47.121195	48.857831
1305.609481	49.728489	48.862836
1302.130067	48.381408	48.867841
1298.499451	55.461040	48.872845
1295.551073	56.799152	48.877850
1292.219430	56.064865	48.882855
1288.326655	57.082577	48.887860
1285.136934	58.610336	48.892865
1281.139175	68.202559	48.897869
1277.465652	55.610099	48.902874
1274.270425	46.464077	48.907879
1270.963573	51.243574	48.912884
1267.508342	53.224196	48.917889
1263.965920	59.578180	48.922893
1260.174262	58.049037	48.927898
1257.092248	59.626382	48.932903
1253.100965	52.174230	48.937908
1249.800520	59.933028	48.942913
1246.062484	52.279880	48.947917
1242.622053	49.673855	48.952922
1239.051777	49.128806	48.957927
1235.605576	54.844466	48.962932
1232.633811	52.952860	48.967937
1228.967883	52.808771	48.972941
1225.576256	51.166397	48.977946
1222.098275	48.800379	48.982951
1218.082117	50.587254	48.987956
1214.805462	40.811757	48.992961
1211.168289	50.274776	48.997965
1207.597776	50.001862	49.002970
1204.474125	47.941052	49.007975
1200.981552	47.418655	49.012980
1197.019018	41.199076	49.017985
1193.324955	45.507697	49.022989
1190.435648	42.650895	49.027994
1187.337479	46.692221	49.032999
1183.450068	54.770719	49.038004
1179.901837	47.587768	49.043009
1175.988035	49.599083	49.048013
1172.496742	42.739421	49.053018
1169.464689	54.062941	49.058023
1165.916748	58.437284	49.063028
1162.321127	54.716619	49.068033
1158.608186	53.149884	49.073037
1155.361140	47.776936	49.078042
1151.798587	44.750299	49.083047
1148.104753	52.390373	49.088052
1144.734838	42.366911	49.093057
1140.916197	47.862493	49.098061
1137.664605	48.691295	49.103066
1134.459533	43.748388	49.108071
1130.457093	54.761928	49.113076
1127.114787	42.313851	49.118081
1123.654976	50.534232	49.123085
1120.238830	50.502941	49.128090
1116.648827	50.530509	49.133095
1112.812451	54.146424	49.138100
1109.884816	54.715705	49.143105
1106.449950	46.850640	49.148109
1103.202314	55.534526	49.153114
1099.525336	39.845354	49.158119
1095.389133	48.383615	49.163124
1091.949144	47.802404	49.168129
1088.672706	48.543362	49.173133
1085.131934	42.248311	49.178138
1081.621462	52.264177	49.183143
1078.098589	53.122817	49.188148
1074.942653	51.430942	49.193153
1071.416386	53.701165	49.198157
1067.567127	59.331285	49.203162
1064.408009	50.957987	49.208167
1060.244751	54.637755	49.213172
1056.985361	45.596783	49.218177
1053.616254	50.772074	49.223181
1049.969808	45.689494	49.228186
1046.805471	46.143993	49.233191
1043.139458	55.855191	49.238196
1039.525408	41.564083	49.243201
1036.365172	44.922299	49.248205
1032.503280	48.248006	49.253210
1029.331676	42.214720	49.258215
1026.023466	47.703191	49.263220
1022.670764	57.754486	49.268225
1018.556249	58.810187	49.273229
1014.888781	57.783724	49.278234
1011.281331	55.017273	49.283239
1007.881023	44.327906	49.288244
1004.732344	33.320735	49.293249
1001.153848	44.160363	49.298253
997.652483	51.362221	49.303258
994.315232	45.674426	49.308263
990.686680	52.209659	49.313268
987.040186	52.499223	49.318273
983.722108	52.797479	49.323277
980.176577	46.740500	49.328282
976.435760	43.317897	49.333287
972.741875	54.824182	49.338292
969.611706	48.417430	49.343297
966.318466	49.622973	49.348301
962.280912	42.181374	49.353306
959.197813	40.259834	49.358311
955.241038	49.171852	49.363316
951.886390	52.513079	49.368321
948.387503	60.768108	49.373325
945.198627	53.541644	49.378330
941.717867	47.329005	49.383335
938.157500	50.427199	49.388340
934.634463	45.809404	49.393345
930.819659	46.337317	49.398349
927.564557	46.242913	49.403354
923.935225	51.120466	49.408359
920.175537	42.686243	49.413364
917.245914	46.745548	49.418369
913.642228	42.513718	49.423373
910.129761	53.817606	49.428378
906.838319	39.567801	49.433383
902.923466	52.023038	49.438388
899.758772	53.898181	49.443393
896.228847	58.791818	49.448397
892.829355	52.923980	49.453402
889.436181	48.757272	49.458407
885.353926	48.884153	49.463412
881.826551	43.577355	49.468417
878.577057	50.220949	49.473421
874.708714	50.045417	49.478426
871.586438	42.523818	49.483431
868.161754	40.896244	49.488436
864.899916	40.777607	49.493441
861.198995	45.425943	49.498445
857.105644	45.617850	49.503450
853.926316	45.014892	49.508455
849.634795	45.835788	49.513460
846.979160	42.591328	49.518465
843.303209	49.665546	49.523469
840.234927	45.865603	49.528474
836.574944	38.915442	49.533479
833.114325	47.009482	49.538484
829.719728	53.299323	49.543489
825.773841	39.465252	49.548493
821.832732	53.285053	49.553498
818.824849	50.408974	49.558503
815.384472	44.908245	49.563508
812.459759	46.062459	49.568513
808.814009	40.521127	49.573517
804.973642	40.493105	49.578522
801.746807	35.310125	49.583527
797.526954	41.919030	49.588532
794.108848	44.298965	49.593537
790.910006	39.051492	49.598541
787.611683	42.463046	49.603546
784.108426	36.282476	49.608551
780.234501	43.574377	49.613556
776.813174	43.939495	49.618561
773.336325	35.287046	49.623565
769.750039	39.303688	49.628570
766.513608	49.276728	49.633575
762.924573	46.975736	49.638580
759.752371	41.986697	49.643585
756.348493	43.899341	49.648589
752.542826	53.138946	49.653594
748.848201	38.556884	49.658599
744.893987	45.848717	49.663604
741.757818	37.842126	49.668609
738.342696	41.319443	49.673613
734.643342	48.346741	49.678618
731.296985	38.133113	49.683623
727.803418	44.685257	49.688628
724.553386	47.035731	49.693633
721.025458	51.059073	49.698637
716.870337	52.595830	49.703642
713.821704	43.072743	49.708647
710.656678	51.123695	49.713652
707.501543	38.630684	49.718657
703.417708	57.047697	49.723661
699.626856	43.828497	49.728666
696.330313	38.068011	49.733671
693.043214	48.833622	49.738676
689.412597	41.477128	49.743681
685.621599	41.998249	49.748685
681.897482	46.248482	49.753690
678.939264	49.844093	49.758695
675.307126	53.361748	49.763700
671.636744	45.669800	49.768705
668.768006	50.997806	49.773709
664.861921	46.123735	49.778714
661.281631	43.318375	49.783719
657.718992	45.376141	49.788724
653.980650	38.216871	49.793729
650.632577	32.844129	49.798733
647.323048	34.868586	49.803738
643.901629	36.078494	49.808743
640.274158	31.534131	49.813748
636.651756	38.505114	49.818753
633.336406	43.165913	49.823757
629.517559	45.985156	49.828762
626.628298	38.901730	49.833767
622.692261	41.777294	49.838772
619.381703	33.443724	49.843777
615.961107	42.142169	49.848781
611.925825	39.060073	49.853786
608.766942	38.045873	49.858791
605.025278	47.541258	49.863796
601.658578	48.356632	49.868801
598.377875	35.668203	49.873805
594.616480	51.016501	49.878810
591.431849	40.075249	49.883815
587.714576	41.891502	49.888820
584.196546	39.981264	49.893825
580.393406	37.365866	49.898829
577.745345	45.902201	49.903834
573.835448	38.447132	49.908839
570.269895	32.241612	49.913844
566.786649	39.693864	49.918849
562.955462	32.735843	49.923853
559.544850	44.485783	49.928858
556.345748	34.350414	49.933863
552.775781	35.017307	49.938868
549.112104	39.080951	49.943873
545.980637	34.705716	49.948877
542.097795	47.102267	49.953882
538.962443	36.520319	49.958887
535.335992	49.243714	49.963892
531.642874	44.855209	49.968897
528.195995	42.446628	49.973901
524.193595	44.699872	49.978906
521.091972	47.672580	49.983911
517.437600	48.919022	49.988916
514.298123	47.797411	49.993921
510.121109	41.928131	49.998925
506.664126	56.172080	50.003930
504.040158	34.398880	50.008935
500.263564	44.130724	50.013940
496.627379	44.611856	50.018945
493.235586	45.728594	50.023949
489.499885	49.787724	50.028954
486.317703	35.600107	50.033959
482.344605	55.993014	50.038964
479.160338	37.385934	50.043969
475.572576	38.783311	50.048973
472.245209	40.582831	50.053978
468.837559	42.850511	50.058983
464.941128	49.307654	50.063988
461.539316	42.301408	50.068993
458.581825	43.672838	50.073997
454.536049	46.246119	50.079002
450.403391	37.184007	50.084007
447.141043	38.802509	50.089012
444.204942	38.247021	50.094017
440.731116	37.298030	50.099021
437.411320	45.980742	50.104026
433.717639	37.979345	50.109031
430.162399	35.964266	50.114036
426.352265	39.263118	50.119041
422.998309	37.412667	50.124045
419.301929	39.864796	50.129050
416.091173	31.768785	50.134055
412.526853	37.582298	50.139060
409.035544	34.013295	50.144065
405.452531	38.773042	50.149069
402.158099	31.016012	50.154074
398.848193	32.604014	50.159079
395.371263	36.015201	50.164084
391.652673	43.937812	50.169089
388.016724	39.980182	50.174093
384.001142	37.502554	50.179098
381.138173	33.993327	50.184103
377.624789	37.856322	50.189108
374.129741	39.561920	50.194113
370.319129	36.947786	50.199117
366.929085	43.838174	50.204122
363.102244	33.124177	50.209127
360.024990	31.948583	50.214132
356.515920	30.084492	50.219137
353.194066	42.269838	50.224141
349.266000	43.910397	50.229146
346.136077	39.114216	50.234151
342.192592	47.590933	50.239156
339.007724	51.690386	50.244161
335.333181	39.614268	50.249165
331.697845	45.964123	50.254170
328.649258	38.291998	50.259175
325.226222	36.955446	50.264180
321.913580	39.505690	50.269185
318.113771	34.925189	50.274189
314.609029	48.673625	50.279194
310.931303	42.587031	50.284199
307.247155	38.092821	50.289204
303.895302	22.979587	50.294209
300.267126	33.358962	50.299213
296.608557	33.755096	50.304218
293.535510	28.393207	50.309223
289.964015	39.877354	50.314228
286.526063	39.210708	50.319233
283.278644	33.575580	50.324237
279.485553	40.469021	50.329242
276.225648	39.198682	50.334247
272.397026	36.865826	50.339252
268.827630	36.754455	50.344257
265.121511	36.965061	50.349261
261.750855	39.847118	50.354266
258.287657	30.942833	50.359271
254.912519	36.578069	50.364276
251.550246	32.710508	50.369281
247.891774	33.650814	50.374285
244.356820	32.565946	50.379290
240.864127	37.298947	50.384295
237.339885	37.810104	50.389300
234.029058	36.468665	50.394305
231.014931	36.580372	50.399309
227.149062	28.460522	50.404314
223.103412	22.020326	50.409319
219.292002	36.949448	50.414324
216.052774	27.035659	50.419329
212.842989	25.994777	50.424333
209.048996	31.186279	50.429338
205.772578	30.491196	50.434343
202.485435	36.324636	50.439348
198.370517	34.147397	50.444353
195.214756	42.459631	50.449357
191.917054	39.913922	50.454362
188.676763	26.808076	50.459367
185.105806	39.307738	50.464372
181.665885	42.390501	50.469377
177.879589	45.635099	50.474381
174.013486	45.234890	50.479386
170.580654	42.473077	50.484391
167.383694	39.819846	50.489396
163.649421	51.649081	50.494401
160.275192	45.410605	50.499405
156.646752	48.310941	50.504410
153.357239	42.283825	50.509415
149.737633	44.948660	50.514420
146.397010	43.687853	50.519425
142.505102	37.103384	50.524429
138.823271	47.402639	50.529434
136.160825	40.075060	50.534439
132.509840	46.667883	50.539444
128.828151	52.980782	50.544449
125.391216	39.405890	50.549453
121.802137	53.107485	50.554458
118.283522	39.782676	50.559463
114.759086	47.244697	50.564468
110.935265	51.498114	50.569473
107.496285	37.708417	50.574477
103.873383	46.732947	50.579482
100.882336	43.332471	50.584487
97.488062	48.233605	50.589492
93.772582	36.736671	50.594497
90.400610	40.422592	50.599501
86.595048	36.371450	50.604506
83.516538	32.222220	50.609511
79.732592	36.501037	50.614516
76.341120	38.253797	50.619521
73.043721	39.118621	50.624525
68.979530	51.464650	50.629530
65.561992	34.261084	50.634535
62.092303	34.994718	50.639540
58.456994	43.265067	50.644545
55.685260	37.827588	50.649549
51.476739	46.861631	50.654554
48.525207	39.427518	50.659559
44.631478	45.118769	50.664564
40.965867	50.701516	50.669569
37.496749	43.016305	50.674573
33.991724	49.551496	50.679578
30.669408	44.611577	50.684583
26.894191	49.578750	50.689588
23.448713	38.242029	50.694593
20.669204	40.987260	50.699597
16.510435	39.136521	50.704602
13.053586	43.832352	50.709607
9.521138	40.443973	50.714612
6.254451	47.584071	50.719617
3.208956	38.731516	50.724621