Thu Aug 25 09:46:55 2022

Number of Points = 9926

Depth (nm)	Load (N)	Time (s)
1.825406	97.633733	0.000000
1.647826	100.464775	0.005005
1.643456	97.244867	0.010010
1.877439	90.874469	0.015014
1.656831	99.549400	0.020019
1.396427	85.084460	0.025024
1.550082	75.512269	0.030029
0.931862	59.698703	0.035034
0.943262	55.394326	0.040038
0.267651	41.984734	0.045043
-0.122621	34.826314	0.050048
-0.230479	26.256907	0.055053
-0.679792	25.444741	0.060058
-0.599041	18.196708	0.065062
-1.334984	16.511966	0.070067
-1.810403	12.369298	0.075072
-1.801519	2.800847	0.080077
-2.186073	16.386255	0.085082
-2.270690	9.591243	0.090086
-3.056495	14.564518	0.095091
-3.200209	11.439225	0.100096
-3.227266	6.840329	0.105101
-3.708134	7.814300	0.110106
-3.722549	3.880976	0.115110
-3.573580	8.606545	0.120115
-4.302675	7.401620	0.125120
-4.698393	3.648263	0.130125
-5.259865	6.276849	0.135130
-5.027288	2.058053	0.140134
-4.744800	-1.611743	0.145139
-5.195593	2.274492	0.150144
-5.431390	5.741063	0.155149
-5.972695	0.422315	0.160154
-5.753851	3.295633	0.165158
-6.693371	4.752755	0.170163
-7.480928	4.901585	0.175168
-7.471926	-2.328870	0.180173
-7.762086	5.426771	0.185178
-7.950673	-0.377512	0.190182
-7.860448	-0.843943	0.195187
-8.271010	8.806668	0.200192
-7.877131	8.602706	0.205197
-7.851644	1.644913	0.210202
-8.517340	-1.294187	0.215206
-8.981915	-1.139016	0.220211
-9.005074	3.623012	0.225216
-9.335429	4.918249	0.230221
-10.499102	4.996297	0.235226
-10.432305	-2.445693	0.240230
-10.474624	-0.752663	0.245235
-10.780367	2.791306	0.250240
-10.261920	-2.503663	0.255245
-10.289651	-4.894153	0.260250
-11.128729	3.320816	0.265254
-11.748322	3.418019	0.270259
-11.943248	0.218495	0.275264
-11.880049	-1.743318	0.280269
-12.579477	1.261223	0.285274
-12.374943	0.998344	0.290278
-12.564180	3.793232	0.295283
-12.924389	6.690841	0.300288
-13.677672	-0.752369	0.305293
-13.600873	8.470703	0.310298
-14.034096	-4.084654	0.315302
-13.782723	1.263944	0.320307
-13.989540	4.694338	0.325312
-14.640430	-0.363630	0.330317
-15.024667	9.206926	0.335322
-14.857241	-1.338651	0.340326
-15.101124	2.882159	0.345331
-15.800123	6.123915	0.350336
-15.885132	-1.588518	0.355341
-16.812670	12.461614	0.360346
-16.666578	9.838242	0.365350
-16.563320	13.751563	0.370355
-16.754290	19.378283	0.375360
-16.577700	7.227243	0.380365
-16.691165	3.243000	0.385370
-17.425925	1.029729	0.390374
-17.612920	7.715678	0.395379
-18.121816	14.420430	0.400384
-18.010374	3.035737	0.405389
-18.768309	12.013115	0.410394
-19.301186	6.212156	0.415398
-19.341026	1.020481	0.420403
-19.890811	16.387658	0.425408
-19.609291	2.600339	0.430413
-19.921661	1.200408	0.435418
-19.963068	13.941110	0.440422
-19.700192	5.275660	0.445427
-20.697310	0.474422	0.450432
-20.751594	-2.206137	0.455437
-21.158253	15.562044	0.460442
-21.240533	14.189335	0.465446
-21.389878	12.703748	0.470451
-22.277397	8.530741	0.475456
-22.398135	7.518398	0.480461
-22.753435	1.705436	0.485466
-22.632932	4.360044	0.490470
-22.674991	10.684763	0.495475
-22.666845	7.953293	0.500480
-22.705755	7.336252	0.505485
-23.364124	9.790197	0.510490
-23.536759	13.715109	0.515494
-23.726707	3.371058	0.520499
-24.586444	18.495737	0.525504
-24.839217	13.286801	0.530509
-25.325665	14.593842	0.535514
-25.455848	7.600328	0.540518
-25.205644	11.825980	0.545523
-25.584389	17.744713	0.550528
-25.508552	8.725754	0.555533
-25.584472	18.225859	0.560538
-26.186772	5.918453	0.565542
-26.544088	12.729166	0.570547
-26.944748	3.512789	0.575552
-26.730178	8.237569	0.580557
-27.970436	9.871529	0.585562
-27.921807	10.449325	0.590566
-28.105723	9.067232	0.595571
-28.651021	7.358948	0.600576
-28.224695	0.290894	0.605581
-28.872754	8.324077	0.610586
-28.726177	3.856164	0.615590
-28.220802	5.308354	0.620595
-29.169959	4.172715	0.625600
-29.410928	3.891054	0.630605
-29.931333	0.438810	0.635610
-30.052685	1.093859	0.640614
-30.176218	6.108896	0.645619
-30.534585	6.889668	0.650624
-30.707180	6.458089	0.655629
-31.297944	8.420552	0.660634
-31.266948	9.953399	0.665638
-31.559335	8.509208	0.670643
-31.937895	21.160373	0.675648
-32.193477	1.433432	0.680653
-32.728424	2.849311	0.685658
-33.032133	0.894367	0.690662
-33.231391	10.049962	0.695667
-33.239657	16.983155	0.700672
-32.935167	5.251839	0.705677
-33.487484	7.103874	0.710682
-33.402445	5.619527	0.715686
-34.124776	6.982510	0.720691
-34.593838	11.301880	0.725696
-34.178405	5.194147	0.730701
-34.647100	12.427273	0.735706
-35.276242	2.610783	0.740710
-35.874897	8.377309	0.745715
-36.297259	5.077381	0.750720
-35.726319	9.167355	0.755725
-35.989548	13.321596	0.760730
-36.148521	13.960394	0.765734
-36.170121	2.103005	0.770739
-36.746073	8.998595	0.775744
-37.128582	5.122947	0.780749
-37.192129	5.110880	0.785754
-37.617157	11.438658	0.790758
-37.537351	10.553080	0.795763
-38.224237	8.601228	0.800768
-38.405610	6.655589	0.805773
-38.578998	8.897503	0.810778
-39.173201	9.424163	0.815782
-39.077143	9.700298	0.820787
-39.319885	21.779689	0.825792
-39.284535	8.597251	0.830797
-40.125454	9.165733	0.835802
-40.493127	12.725736	0.840806
-40.473203	3.161886	0.845811
-40.708623	5.318606	0.850816
-40.778404	2.551891	0.855821
-40.966685	9.067199	0.860826
-41.529583	14.328251	0.865830
-41.683692	3.747632	0.870835
-42.010083	13.736232	0.875840
-41.853957	8.589779	0.880845
-41.880758	15.070296	0.885850
-42.774459	13.584283	0.890854
-43.158414	14.125456	0.895859
-43.435565	9.907434	0.900864
-43.230046	15.756763	0.905869
-43.618682	10.866512	0.910874
-43.810345	9.998160	0.915878
-43.598771	12.958037	0.920883
-44.648034	8.484510	0.925888
-44.710579	3.258428	0.930893
-45.101175	16.873254	0.935898
-45.251640	8.016306	0.940902
-45.166002	4.896208	0.945907
-46.030872	12.678627	0.950912
-46.103325	13.117207	0.955917
-46.715565	19.531270	0.960922
-46.814894	8.109999	0.965926
-46.986726	2.322076	0.970931
-46.857197	13.697725	0.975936
-46.775902	19.047665	0.980941
-47.064388	19.497950	0.985946
-46.919708	22.227865	0.990950
-47.459306	13.087039	0.995955
-48.018934	20.423001	1.000960
-47.808728	2.736463	1.005965
-48.866703	5.227713	1.010970
-49.359797	10.942898	1.015974
-49.404372	9.444060	1.020979
-49.459424	15.179194	1.025984
-49.608919	12.965969	1.030989
-49.570209	14.285636	1.035994
-50.140497	6.503708	1.040998
-50.380084	5.010116	1.046003
-50.948112	11.366628	1.051008
-50.655945	3.430581	1.056013
-51.308957	6.294975	1.061018
-51.250250	18.222725	1.066022
-51.284087	22.695365	1.071027
-52.022770	27.091787	1.076032
-52.113254	13.853134	1.081037
-52.361296	13.408067	1.086042
-52.761743	16.308819	1.091046
-52.539569	9.199984	1.096051
-53.227120	16.188993	1.101056
-53.384504	13.249342	1.106061
-53.526210	8.972132	1.111066
-53.828138	10.383138	1.116070
-53.737104	15.117784	1.121075
-54.558435	18.018045	1.126080
-54.617822	16.559492	1.131085
-55.026887	11.833793	1.136090
-55.180464	12.648916	1.141094
-55.105543	8.227032	1.146099
-55.831562	7.050105	1.151104
-56.012568	0.330314	1.156109
-56.425134	10.974655	1.161114
-56.463540	5.077239	1.166118
-56.464837	6.649947	1.171123
-56.641569	23.328576	1.176128
-57.029721	11.307155	1.181133
-57.528175	12.128861	1.186138
-57.816577	22.092529	1.191142
-57.878114	10.355289	1.196147
-58.527234	6.129114	1.201152
-58.039595	7.951076	1.206157
-58.765847	13.051063	1.211162
-59.109481	11.058083	1.216166
-59.339053	4.779335	1.221171
-59.962578	19.053917	1.226176
-59.461727	8.380163	1.231181
-59.443244	6.412700	1.236186
-60.021661	7.443088	1.241190
-60.384942	13.229682	1.246195
-60.891698	16.523577	1.251200
-60.886593	2.504328	1.256205
-61.122949	12.586386	1.261210
-61.203118	13.459609	1.266214
-61.806820	11.899685	1.271219
-62.421463	18.715920	1.276224
-62.400351	9.775141	1.281229
-62.699002	10.021375	1.286234
-62.706429	3.486356	1.291238
-62.293247	5.190271	1.296243
-63.101701	16.070653	1.301248
-63.451179	1.553308	1.306253
-63.809027	12.565562	1.311258
-64.087158	9.081684	1.316262
-63.965475	8.679925	1.321267
-64.288768	8.474441	1.326272
-64.119392	8.308817	1.331277
-64.836106	8.743945	1.336282
-64.950160	5.139446	1.341286
-65.236671	13.486138	1.346291
-66.159121	14.187619	1.351296
-66.565337	9.173574	1.356301
-66.621358	8.923047	1.361306
-66.450009	6.308373	1.366310
-66.388115	10.351558	1.371315
-66.847711	14.122117	1.376320
-66.951103	5.915857	1.381325
-67.209180	4.997801	1.386330
-68.286809	11.848615	1.391334
-68.145318	8.273677	1.396339
-68.848985	12.661446	1.401344
-68.497598	3.504404	1.406349
-68.707854	5.568597	1.411354
-69.072915	20.735987	1.416358
-68.996662	4.636496	1.421363
-69.009829	10.010725	1.426368
-69.247554	7.412694	1.431373
-69.673592	0.250409	1.436378
-70.049748	6.095965	1.441382
-70.048505	8.592089	1.446387
-71.268694	11.380843	1.451392
-71.576515	9.625861	1.456397
-71.380045	12.932952	1.461402
-71.614852	7.290937	1.466406
-71.705040	9.988049	1.471411
-71.876446	6.180566	1.476416
-71.294600	9.256429	1.481421
-71.973681	7.157824	1.486426
-72.723621	6.569940	1.491430
-72.787822	4.245276	1.496435
-73.236138	12.497098	1.501440
-74.158748	11.237081	1.506445
-74.428056	9.431772	1.511450
-73.777644	9.352125	1.516454
-74.299566	15.179396	1.521459
-74.488242	22.760953	1.526464
-74.689356	8.270978	1.531469
-74.690828	11.694506	1.536474
-74.846898	7.020917	1.541478
-75.423195	11.192575	1.546483
-76.034728	18.308879	1.551488
-75.743830	-3.458874	1.556493
-76.286093	8.113781	1.561498
-76.191482	6.960129	1.566502
-76.830172	3.007568	1.571507
-77.197371	9.832484	1.576512
-77.072511	16.997915	1.581517
-77.217642	12.531417	1.586522
-77.336694	5.858866	1.591526
-78.008175	10.254246	1.596531
-78.753777	10.257303	1.601536
-78.717332	11.166038	1.606541
-78.744020	10.781200	1.611546
-78.919030	14.839360	1.616550
-78.886092	8.611227	1.621555
-79.169163	17.409797	1.626560
-80.107047	18.240249	1.631565
-80.018822	2.198997	1.636570
-80.588956	9.084185	1.641574
-80.479189	-0.091942	1.646579
-80.688668	16.737342	1.651584
-80.482972	1.573025	1.656589
-80.973471	8.047101	1.661594
-81.771301	24.202956	1.666598
-81.863115	14.511079	1.671603
-82.311786	18.156542	1.676608
-82.034050	8.115697	1.681613
-82.488108	21.034952	1.686618
-82.777974	10.418659	1.691622
-82.966458	1.127914	1.696627
-83.527647	8.789982	1.701632
-83.470129	10.426240	1.706637
-83.594618	16.564558	1.711642
-83.747747	0.877502	1.716646
-84.078471	0.378954	1.721651
-84.706671	9.585939	1.726656
-84.940131	1.283004	1.731661
-85.035914	7.037172	1.736666
-85.566481	9.632446	1.741670
-85.151138	3.917033	1.746675
-85.510581	16.055831	1.751680
-86.089296	10.980232	1.756685
-86.616306	10.325779	1.761690
-86.654569	8.012869	1.766694
-86.614436	7.975065	1.771699
-86.952051	15.908986	1.776704
-86.439720	3.145363	1.781709
-87.575048	9.204790	1.786714
-88.221937	11.220343	1.791718
-87.963245	10.313062	1.796723
-88.122770	11.926382	1.801728
-88.034988	7.483501	1.806733
-88.689316	-1.557076	1.811738
-89.037835	-6.535863	1.816742
-89.262278	-3.491850	1.821747
-89.802016	-1.179877	1.826752
-89.431714	6.206516	1.831757
-90.034492	6.620628	1.836762
-90.368627	4.176910	1.841766
-90.723014	1.935682	1.846771
-90.962627	10.670491	1.851776
-90.619064	7.864317	1.856781
-90.873564	7.787259	1.861786
-91.389778	7.861941	1.866790
-91.642325	0.666146	1.871795
-92.289595	13.761203	1.876800
-92.155503	6.087206	1.881805
-92.585870	12.615137	1.886810
-92.740508	8.536109	1.891814
-93.214327	3.576953	1.896819
-93.858220	6.284897	1.901824
-93.675712	9.600502	1.906829
-93.769991	10.640451	1.911834
-94.051729	2.452649	1.916838
-94.096048	-1.893600	1.921843
-93.938199	5.079995	1.926848
-94.448139	5.701022	1.931853
-95.133515	5.637697	1.936858
-95.338862	7.160120	1.941862
-95.485786	3.734780	1.946867
-95.318849	15.468394	1.951872
-95.994684	11.119857	1.956877
-96.650520	7.293371	1.961882
-96.665644	3.508857	1.966886
-96.787731	3.787536	1.971891
-96.993144	11.447640	1.976896
-96.829614	5.983655	1.981901
-97.918869	4.477672	1.986906
-98.611934	14.030181	1.991910
-98.406268	5.962156	1.996915
-98.055064	4.506410	2.006912
-98.128522	13.505208	2.016909
-97.401650	9.080179	2.026906
-97.163854	-1.084289	2.036902
-96.442558	7.584065	2.046899
-96.015520	9.579630	2.056896
-95.779746	3.891576	2.066893
-94.642849	10.948924	2.076890
-94.465839	11.393432	2.086886
-94.245823	7.389947	2.096883
-93.411071	6.169666	2.106880
-92.876025	9.380580	2.116877
-92.983028	4.544523	2.126874
-91.870427	5.064174	2.136870
-91.772613	5.714328	2.146867
-91.017849	12.308869	2.156864
-90.611756	3.844477	2.166861
-90.306704	5.358644	2.176858
-89.251045	10.322137	2.186854
-89.080717	8.686448	2.196851
-88.865003	-0.007869	2.206848
-87.926802	4.635072	2.216845
-87.583418	2.687166	2.226842
-86.750375	3.868344	2.236838
-85.917212	7.178264	2.246835
-85.738345	11.867332	2.256832
-86.067776	17.427998	2.266829
-85.413002	14.978302	2.276826
-84.455800	8.698865	2.286822
-83.502999	1.571150	2.296819
-83.171906	2.754954	2.306816
-83.367799	11.050679	2.316813
-82.933273	10.149703	2.326810
-81.979261	11.562183	2.336806
-81.683520	10.473879	2.346803
-80.588273	4.616305	2.356800
-80.555309	11.336619	2.366797
-80.442727	10.581124	2.376794
-79.210977	7.353608	2.386790
-78.834087	3.464927	2.396787
-78.723933	4.347564	2.406784
-77.596239	6.828887	2.416781
-77.392547	4.386518	2.426778
-77.378962	7.577774	2.436774
-76.449811	11.541060	2.446771
-76.152694	5.786373	2.456768
-75.487041	9.334785	2.466765
-74.899878	6.081560	2.476762
-74.947722	8.056503	2.486758
-73.798477	0.967699	2.496755
-73.641330	5.112140	2.506752
-72.550632	18.103686	2.516749
-72.229940	18.877307	2.526746
-71.838256	7.538808	2.536742
-71.767561	2.554530	2.546739
-71.229232	4.900122	2.556736
-70.517158	9.879441	2.566733
-69.914713	11.511736	2.576730
-68.813978	7.477955	2.586726
-68.931024	8.963229	2.596723
-68.774139	9.990599	2.606720
-68.147466	12.981251	2.616717
-67.517866	19.997721	2.626714
-67.223311	11.664843	2.636710
-66.434004	9.900488	2.646707
-65.865686	13.264582	2.656704
-65.554216	16.187417	2.666701
-64.666892	18.266084	2.676698
-64.536033	13.820404	2.686694
-64.200182	20.151141	2.696691
-63.465292	13.038561	2.706688
-62.944870	19.042603	2.716685
-61.882476	22.215241	2.726682
-61.994226	13.958697	2.736678
-61.636216	11.188038	2.746675
-61.115807	18.300812	2.756672
-60.272468	16.505816	2.766669
-59.860030	10.935796	2.776666
-59.672607	12.515914	2.786662
-58.876766	10.842401	2.796659
-58.515455	13.073182	2.806656
-57.415601	15.007675	2.816653
-57.295074	12.559329	2.826650
-57.078082	12.110589	2.836646
-56.670526	13.741745	2.846643
-55.760145	13.152680	2.856640
-55.814282	15.895217	2.866637
-55.166552	18.290194	2.876634
-54.530549	11.082237	2.886630
-53.925666	15.881952	2.896627
-53.442368	18.039766	2.906624
-52.993983	19.395262	2.916621
-52.267268	17.124363	2.926618
-51.908563	17.720967	2.936614
-51.459391	22.446881	2.946611
-50.746042	14.716787	2.956608
-50.259942	20.089481	2.966605
-49.980949	17.169644	2.976602
-49.802779	14.946684	2.986598
-48.967041	14.926848	2.996595
-48.397873	18.411187	3.006592
-47.581208	16.186383	3.016589
-47.419901	10.981996	3.026586
-47.269724	24.171608	3.036582
-46.383487	18.714246	3.046579
-45.740499	15.626503	3.056576
-45.555096	18.052741	3.066573
-44.264518	11.185711	3.076570
-44.131633	19.889256	3.086566
-44.123524	19.222990	3.096563
-43.723778	16.347589	3.106560
-42.674766	14.504529	3.116557
-42.715484	11.013900	3.126554
-41.849565	18.107384	3.136550
-41.403912	11.024287	3.146547
-41.023602	19.122027	3.156544
-39.951479	15.957540	3.166541
-40.085364	13.726454	3.176538
-39.556671	14.264746	3.186534
-38.556517	13.566582	3.196531
-38.343911	14.201918	3.206528
-38.076105	17.587759	3.216525
-37.349893	14.287405	3.226522
-36.885972	16.419746	3.236518
-36.807177	12.222978	3.246515
-36.031186	8.997187	3.256512
-35.019347	14.594780	3.266509
-34.822882	13.167239	3.276506
-34.258700	13.823515	3.286502
-34.007651	16.594261	3.296499
-33.376919	9.760930	3.306496
-32.504781	10.942325	3.316493
-32.679458	10.200162	3.326490
-32.186728	5.837166	3.336486
-31.002962	10.299090	3.346483
-31.061084	5.753143	3.356480
-30.187607	9.645965	3.366477
-29.632201	10.275105	3.376474
-29.377551	11.223801	3.386470
-29.109496	7.909705	3.396467
-28.136980	8.270751	3.406464
-27.953152	12.591580	3.416461
-27.426929	14.270668	3.426458
-26.586016	15.903616	3.436454
-26.663490	9.263615	3.446451
-26.035033	11.107249	3.456448
-25.522486	14.381884	3.466445
-24.620580	9.992788	3.476442
-23.747107	6.219534	3.486438
-23.755212	4.915913	3.496435
-23.631101	9.939848	3.506432
-23.043701	10.389746	3.516429
-22.330847	12.017417	3.526426
-22.065897	0.331313	3.536422
-20.952327	6.381800	3.546419
-20.679178	3.209458	3.556416
-20.499006	3.476075	3.566413
-19.979596	10.446457	3.576410
-19.049060	4.890294	3.586406
-19.162730	16.097021	3.596403
-18.278738	12.594549	3.606400
-17.937128	9.715587	3.616397
-17.437222	4.819277	3.626394
-16.411735	12.945807	3.636390
-16.293673	9.892798	3.646387
-16.084128	10.043940	3.656384
-15.361358	8.423062	3.666381
-14.910601	4.779399	3.676378
-14.402263	5.580640	3.686374
-13.037404	4.739805	3.696371
-13.270727	9.594831	3.706368
-12.886139	8.172660	3.716365
-12.738441	8.982892	3.726362
-11.725039	8.691302	3.736358
-11.319720	8.973327	3.746355
-10.911305	7.360522	3.756352
-9.989400	8.632323	3.766349
-9.790702	0.856161	3.776346
-9.563799	2.594820	3.786342
-8.727800	0.680603	3.796339
-8.408070	6.807959	3.806336
-7.721752	6.855888	3.816333
-7.244936	6.746575	3.826330
-7.184914	11.558806	3.836326
-6.451703	9.521310	3.846323
-5.933939	8.908237	3.856320
-5.076407	8.197578	3.866317
-4.848758	13.607602	3.876314
-4.780530	9.523362	3.886310
-3.987476	23.321837	3.896307
-3.598877	33.239776	3.906304
-2.724132	39.137631	3.916301
-2.847844	46.145440	3.926298
-2.346464	55.342468	3.936294
-1.710879	71.430637	3.946291
-1.361643	81.918643	3.956288
-0.765079	98.104817	3.966285
-0.391203	122.235947	3.976282
0.000000	135.032543	3.981286
-0.044659	144.189295	3.986291
0.316998	148.195037	3.991296
0.593219	146.563664	3.996301
0.882044	159.616564	4.001306
0.805491	166.933842	4.006310
1.002787	174.739731	4.011315
1.288726	168.902171	4.016320
1.290409	164.513869	4.021325
1.238074	175.294857	4.026330
1.215857	162.086520	4.031334
0.727280	160.014989	4.036339
0.983871	164.831306	4.041344
0.988070	167.421904	4.046349
1.299065	168.521749	4.051354
1.365411	167.565505	4.056358
0.819034	163.563634	4.061363
1.107977	166.087471	4.066368
1.205311	175.645937	4.071373
0.665737	169.833316	4.076378
1.242976	178.484517	4.081382
1.169404	166.755381	4.086387
1.478203	168.171948	4.091392
1.473229	173.453196	4.096397
0.868392	173.342440	4.101402
1.367410	169.217900	4.106406
1.210954	173.985041	4.111411
1.137306	174.632621	4.116416
1.185421	177.323908	4.121421
1.232825	171.144068	4.126426
1.280647	169.273231	4.131430
1.102340	170.772448	4.136435
1.207001	172.755679	4.141440
1.191406	163.675036	4.146445
1.202727	167.678727	4.151450
1.385880	164.309201	4.156454
1.416901	165.800929	4.161459
1.278015	164.810403	4.166464
1.287185	170.326718	4.171469
1.063641	166.859562	4.176474
1.120879	169.321626	4.181478
1.249738	182.744459	4.186483
1.373463	171.693093	4.191488
1.532732	171.266460	4.196493
0.861207	179.711522	4.201498
1.467809	164.594975	4.206502
1.456506	176.527478	4.211507
1.716607	182.260745	4.216512
1.655643	176.629398	4.221517
1.496590	173.291343	4.226522
1.469104	159.254924	4.231526
1.490743	173.719613	4.236531
1.382498	163.992256	4.241536
1.533912	177.345111	4.246541
1.514395	191.123395	4.251546
1.751027	194.250223	4.256550
1.748916	194.877104	4.261555
1.639317	174.130501	4.266560
1.508497	173.951801	4.271565
1.239635	178.549893	4.276570
1.717268	189.314291	4.281574
1.962053	196.726768	4.286579
1.946376	190.597934	4.291584
1.779672	186.049347	4.296589
1.464496	186.332971	4.301594
1.399517	179.079233	4.306598
1.308674	200.604144	4.311603
1.917525	196.006804	4.316608
2.281491	204.836968	4.321613
1.824794	194.120143	4.326618
2.101874	190.561888	4.331622
1.499802	179.769772	4.336627
1.931068	182.040355	4.341632
2.067809	179.272890	4.346637
1.298637	182.905325	4.351642
1.950386	185.163509	4.356646
1.583049	199.904302	4.361651
1.813745	199.248176	4.366656
1.781770	203.625658	4.371661
1.506512	206.430892	4.376666
1.652124	198.144393	4.381670
1.651521	201.760814	4.386675
1.796007	191.437018	4.391680
2.045940	199.921212	4.396685
1.903592	205.211338	4.401690
2.008060	192.995540	4.406694
1.637819	203.250548	4.411699
1.878866	190.257207	4.416704
2.204622	200.014016	4.421709
1.585733	199.908626	4.426714
1.657523	187.849813	4.431718
1.909044	206.669840	4.436723
1.742517	216.133628	4.441728
2.406909	214.770463	4.446733
2.216332	219.147488	4.451738
2.529686	216.605448	4.456742
2.000854	215.467207	4.461747
2.089312	198.811957	4.466752
2.262026	188.012336	4.471757
1.799567	191.821344	4.476762
2.039466	209.649768	4.481766
2.543182	214.794376	4.486771
2.257620	200.886946	4.491776
1.970773	201.131331	4.496781
2.130297	204.700517	4.501786
2.244271	214.436732	4.506790
2.273758	213.850097	4.511795
2.282011	214.124175	4.516800
2.338727	216.557853	4.521805
1.773163	221.110694	4.526810
2.662901	217.089440	4.531814
2.557317	215.122411	4.536819
2.224682	204.639244	4.541824
2.309681	206.483189	4.546829
1.860596	221.936006	4.551834
2.350379	211.191096	4.556838
2.362364	223.088344	4.561843
2.440332	228.916603	4.566848
2.485131	230.520074	4.571853
3.018026	232.856999	4.576858
2.736060	213.257339	4.581862
2.553047	210.653865	4.586867
2.363610	207.387004	4.591872
2.623104	203.613200	4.596877
2.506607	206.099327	4.601882
2.438598	208.979658	4.606886
2.398121	213.845698	4.611891
2.201653	208.128003	4.616896
2.503511	206.486280	4.621901
2.158176	205.104152	4.626906
2.402151	204.487074	4.631910
2.534933	216.071158	4.636915
2.723948	217.924117	4.641920
2.805243	222.673002	4.646925
2.328979	214.841441	4.651930
2.723630	195.331940	4.656934
2.396989	208.462326	4.661939
2.624135	214.052070	4.666944
3.202325	215.663716	4.671949
2.514149	226.942999	4.676954
2.589162	205.221460	4.681958
2.474534	218.125643	4.686963
2.553456	210.033088	4.691968
2.416555	216.224043	4.696973
2.833039	214.817463	4.701978
2.912798	214.061598	4.706982
2.526150	228.172683	4.711987
2.805508	224.133168	4.716992
2.814308	230.820161	4.721997
2.569820	223.341428	4.727002
2.783226	221.020693	4.732006
2.653164	220.395780	4.737011
2.650452	231.017166	4.742016
2.665795	225.259951	4.747021
2.622522	227.997202	4.752026
2.630124	220.994669	4.757030
2.698302	223.451863	4.762035
2.546254	218.758600	4.767040
2.872729	221.074081	4.772045
2.975128	230.584326	4.777050
2.857005	223.883068	4.782054
2.781873	227.925629	4.787059
2.728933	216.326106	4.792064
2.674661	225.832423	4.797069
2.489263	240.010062	4.802074
3.169642	246.784827	4.807078
3.036917	250.412468	4.812083
3.125376	247.696850	4.817088
3.187410	257.725969	4.822093
2.683939	254.334294	4.827098
3.120611	235.501545	4.832102
2.905040	257.479508	4.837107
3.015280	263.103402	4.842112
3.236902	257.006968	4.847117
2.986378	255.379024	4.852122
3.197764	252.596688	4.857126
2.988838	253.562864	4.862131
3.301065	257.351746	4.867136
3.299076	248.297402	4.872141
3.195136	250.547447	4.877146
3.024764	247.113074	4.882150
3.298023	256.988873	4.887155
3.188509	254.731386	4.892160
2.956727	253.151125	4.897165
2.874505	251.857483	4.902170
2.885911	251.615369	4.907174
2.805674	263.080998	4.912179
3.159596	258.545732	4.917184
3.135888	245.745696	4.922189
2.665636	253.770110	4.927194
2.757009	254.233648	4.932198
2.961645	268.381836	4.937203
3.454485	281.342747	4.942208
3.523469	282.831700	4.947213
3.513123	281.697639	4.952218
3.927370	280.696370	4.957222
3.269730	259.424924	4.962227
3.530743	265.053670	4.967232
2.894123	256.434120	4.972237
3.331757	266.350609	4.977242
3.844194	265.210568	4.982246
3.584262	261.163793	4.987251
3.674661	258.216913	4.992256
3.330020	249.434558	4.997261
3.180150	252.179024	5.002266
3.377196	251.268737	5.007270
3.503396	252.426016	5.012275
3.096490	248.500350	5.017280
3.575043	261.080666	5.022285
3.353894	267.832176	5.027290
3.881727	275.579992	5.032294
3.796683	273.495841	5.037299
3.763091	269.094057	5.042304
3.901249	255.344824	5.047309
3.603480	257.698007	5.052314
3.680443	250.092965	5.057318
3.328305	256.308167	5.062323
3.408461	256.042626	5.067328
3.508879	256.862255	5.072333
3.215067	253.232084	5.077338
3.664584	264.690641	5.082342
3.476233	278.552394	5.087347
3.855117	272.567358	5.092352
3.882925	275.552911	5.097357
3.614052	281.881627	5.102362
3.820041	277.454958	5.107366
3.698143	277.015428	5.112371
3.721372	281.438064	5.117376
4.206943	279.770714	5.122381
3.574572	265.651813	5.127386
3.739659	272.039084	5.132390
3.920866	270.634561	5.137395
3.675229	276.390152	5.142400
3.663812	278.470678	5.147405
4.115913	290.125002	5.152410
4.238283	284.145352	5.157414
3.651690	263.830890	5.162419
3.562568	268.400842	5.167424
4.017277	265.615180	5.172429
3.613838	277.058692	5.177434
3.879187	280.880235	5.182438
4.143387	283.142206	5.187443
4.328666	280.028594	5.192448
4.167610	270.828317	5.197453
3.473162	264.404008	5.202458
4.093860	261.219012	5.207462
3.887256	271.049781	5.212467
3.864313	279.668518	5.217472
4.123986	277.470242	5.222477
4.301767	282.919044	5.227482
4.167113	272.388997	5.232486
3.769223	269.300320	5.237491
4.004048	279.909827	5.242496
3.791190	275.868328	5.247501
3.745736	285.756114	5.252506
4.323322	283.435259	5.257510
4.015881	283.898009	5.262515
4.396131	275.182399	5.267520
4.258881	287.428944	5.272525
3.945048	282.444633	5.277530
4.350926	279.524250	5.282534
4.212726	272.652110	5.287539
4.145185	281.888449	5.292544
4.272284	283.608746	5.297549
3.905413	289.259947	5.302554
4.145776	284.502019	5.307558
4.173508	284.852141	5.312563
3.700054	287.909908	5.317568
4.189952	287.668753	5.322573
3.373668	289.638104	5.327578
4.207734	281.588552	5.332582
3.751920	285.823651	5.337587
4.141091	305.163225	5.342592
4.550565	305.130826	5.347597
4.218607	315.591875	5.352602
4.515675	304.019714	5.357606
4.465115	309.320800	5.362611
4.263053	308.564794	5.367616
4.252717	304.194159	5.372621
4.201625	311.630896	5.377626
4.533936	301.850256	5.382630
4.240892	308.692141	5.387635
4.680375	311.483481	5.392640
4.527212	309.444801	5.397645
4.303273	312.336925	5.402650
4.756438	304.707716	5.407654
4.320130	307.892546	5.412659
4.344590	309.423280	5.417664
4.508464	302.794868	5.422669
4.122584	308.072562	5.427674
4.521090	314.318869	5.432678
4.775373	301.025977	5.437683
4.427769	308.891991	5.442688
4.717635	299.927936	5.447693
4.577058	316.898578	5.452698
4.636350	299.384086	5.457702
4.638384	304.803482	5.462707
4.478967	310.767040	5.467712
4.563210	301.044251	5.472717
4.579928	311.624674	5.477722
4.725308	300.591983	5.482726
4.393338	307.430475	5.487731
4.522854	303.458714	5.492736
4.500830	303.588838	5.497741
4.384585	308.571181	5.502746
4.675962	298.730515	5.507750
4.189315	310.370586	5.512755
4.509241	327.076093	5.517760
4.814327	320.915938	5.522765
4.782794	332.130368	5.527770
5.115042	331.913913	5.532774
4.531706	335.536244	5.537779
4.392297	332.799368	5.542784
4.838266	331.840583	5.547789
4.662158	337.515696	5.552794
5.157661	331.860386	5.557798
4.741176	340.651548	5.562803
4.683289	335.940337	5.567808
4.985100	329.467476	5.572813
4.998433	340.598949	5.577818
5.001043	325.779386	5.582822
5.056224	335.787476	5.587827
4.809474	333.257247	5.592832
4.827316	328.935976	5.597837
4.689644	339.667158	5.602842
4.843381	332.508804	5.607846
4.825402	331.413901	5.612851
4.780736	336.720400	5.617856
4.800242	332.076159	5.622861
4.769567	333.207402	5.627866
5.102772	324.644675	5.632870
4.942876	338.859526	5.637875
4.902158	331.339328	5.642880
4.882972	338.233230	5.647885
4.906825	338.618763	5.652890
5.167666	354.463505	5.657894
5.122914	357.583830	5.662899
4.914074	366.737946	5.667904
5.281672	359.523926	5.672909
5.200623	363.602246	5.677914
5.482977	351.864677	5.682918
5.211296	355.441344	5.687923
5.414303	350.331741	5.692928
4.838935	339.304385	5.697933
5.173493	353.128558	5.702938
5.424831	353.019695	5.707942
5.103402	339.845453	5.712947
5.407141	348.821169	5.717952
5.442610	349.568720	5.722957
5.416492	339.657554	5.727962
5.750589	333.173306	5.732966
5.513801	339.025608	5.737971
4.862444	350.647218	5.742976
4.975118	342.827729	5.747981
4.834856	343.295925	5.752986
5.147409	352.659410	5.757990
5.401215	349.759680	5.762995
5.263952	357.741458	5.768000
5.490307	354.409421	5.773005
5.459887	361.466446	5.778010
5.559753	350.307975	5.783014
5.439023	361.900237	5.788019
5.236268	359.527629	5.793024
5.407433	363.841683	5.798029
5.230998	360.088693	5.803034
5.345578	362.826543	5.808038
5.400837	357.667319	5.813043
5.334579	361.332026	5.818048
5.130764	363.439543	5.823053
4.800887	372.954319	5.828058
5.328115	366.689739	5.833062
5.875150	375.507123	5.838067
5.881927	374.658281	5.843072
5.856883	369.676154	5.848077
5.314289	363.873434	5.853082
5.301318	360.053702	5.858086
5.206148	364.706885	5.863091
5.427757	375.157164	5.868096
5.699935	373.260644	5.873101
5.697352	389.200477	5.878106
6.057158	391.567708	5.883110
5.724873	387.234841	5.888115
5.634966	377.074216	5.893120
5.605252	373.709530	5.898125
5.416012	375.406633	5.903130
6.182124	372.879054	5.908134
5.843135	380.667819	5.913139
5.287436	374.908278	5.918144
5.856150	374.898387	5.923149
5.784839	385.881796	5.928154
6.197153	382.321297	5.933158
5.822181	374.568709	5.938163
5.729159	363.130399	5.943168
5.960808	370.443764	5.948173
5.731548	369.391455	5.953178
5.866239	373.087954	5.958182
5.881632	383.317444	5.963187
6.124311	384.228687	5.968192
5.928436	366.592755	5.973197
5.778265	366.717647	5.978202
5.735020	363.177910	5.983206
5.928250	365.400391	5.988211
5.777922	382.138501	5.993216
6.146444	378.869608	5.998221
5.826354	373.310437	6.003226
6.004009	366.575437	6.008230
5.753909	360.660448	6.013235
5.879164	372.720385	6.018240
5.911893	382.165696	6.023245
5.935890	386.553436	6.028250
5.990286	381.403832	6.033254
5.932119	374.250189	6.038259
5.949400	371.909543	6.043264
6.013728	375.851191	6.048269
5.805638	364.415089	6.053274
5.546649	363.838847	6.058278
5.634596	382.311359	6.063283
5.653720	387.652171	6.068288
6.131068	378.633390	6.073293
6.086346	384.911203	6.078298
6.073355	384.562176	6.083302
6.093510	383.337907	6.088307
5.852999	381.622958	6.093312
5.922204	375.809798	6.098317
5.934566	389.741431	6.103322
5.801395	384.820535	6.108326
5.880033	390.382982	6.113331
5.950425	392.061553	6.118336
5.921781	385.485422	6.123341
6.036550	381.841827	6.128346
6.055825	379.589455	6.133350
5.883268	373.440846	6.138355
5.799672	374.463322	6.143360
6.007179	375.797699	6.148365
5.967779	386.016793	6.153370
5.894294	374.967727	6.158374
5.756569	377.653360	6.163379
5.974495	383.244602	6.168384
6.277770	375.993196	6.173389
5.468727	372.472202	6.178394
5.704645	371.676044	6.183398
5.850658	383.612511	6.188403
5.752498	391.458461	6.193408
6.070529	395.015505	6.198413
6.442638	395.726131	6.203418
5.791889	373.096190	6.208422
5.890049	378.003828	6.213427
5.640257	377.695068	6.218432
6.071169	382.620175	6.223437
6.256761	391.968772	6.228442
5.905196	375.793598	6.233446
5.666655	374.644664	6.238451
5.747932	373.426638	6.243456
5.956234	379.819831	6.248461
5.922648	396.210626	6.253466
6.295116	383.978016	6.258470
5.886218	379.521112	6.263475
5.542072	367.169837	6.268480
5.689180	375.844236	6.273485
5.740938	386.264186	6.278490
6.223372	386.163408	6.283494
6.306403	388.729031	6.288499
5.780615	372.476752	6.293504
5.975586	371.430740	6.298509
5.677860	377.767175	6.303514
6.061776	377.381270	6.308518
6.134569	382.837060	6.313523
5.684697	382.474227	6.318528
5.516040	363.163538	6.323533
5.676704	388.050368	6.328538
5.936241	375.835458	6.333542
5.970200	390.111727	6.338547
5.872234	396.711105	6.343552
5.943933	388.698696	6.348557
6.229906	396.962197	6.353562
6.282649	389.541228	6.358566
5.763135	383.260312	6.363571
5.539111	380.530359	6.368576
6.026906	387.721339	6.373581
5.987828	391.074902	6.378586
5.777184	389.250867	6.383590
5.537539	392.882634	6.388595
5.881371	395.454853	6.393600
6.226264	393.331798	6.398605
5.867139	393.777338	6.403610
6.301647	394.085874	6.408614
5.938090	383.022140	6.413619
5.643956	371.877931	6.418624
5.852645	373.208959	6.423629
5.672195	385.206070	6.428634
6.035483	383.396515	6.433638
6.257945	390.853700	6.438643
5.748705	382.040121	6.443648
6.070296	384.482942	6.448653
5.948335	374.086891	6.453658
6.147735	368.686776	6.458662
5.757557	367.112341	6.463667
5.666316	360.476423	6.468672
5.849143	362.270254	6.473677
6.017627	384.172378	6.478682
5.935218	374.883793	6.483686
6.062484	391.929601	6.488691
5.890660	374.878362	6.493696
5.664701	370.655393	6.498701
5.675963	374.133946	6.503706
6.022105	385.811263	6.508710
5.984738	395.609256	6.513715
5.581611	381.970047	6.518720
6.053036	392.090124	6.523725
5.825809	393.834310	6.528730
6.161845	392.266311	6.533734
6.303939	399.388072	6.538739
6.163844	392.658554	6.543744
5.979653	375.033438	6.548749
5.422493	376.699601	6.553754
5.490649	374.914143	6.558758
6.083990	385.704826	6.563763
6.061924	390.422493	6.568768
5.960088	384.386188	6.573773
5.771431	391.566096	6.578778
6.060410	389.312595	6.583782
5.773631	385.978693	6.588787
5.985482	383.344963	6.593792
5.875303	388.418128	6.598797
5.629980	399.115592	6.603802
6.047408	401.840798	6.608806
6.112166	400.631686	6.613811
6.046029	383.465801	6.618816
5.865002	371.737547	6.623821
5.882447	369.713258	6.628826
5.801142	372.159092	6.633830
5.886739	381.605610	6.638835
5.839866	397.546063	6.643840
6.194440	385.711733	6.648845
5.818072	381.610406	6.653850
5.918008	375.460231	6.658854
5.780646	375.491366	6.663859
5.761005	385.226464	6.668864
5.885437	388.421527	6.673869
5.827681	393.957888	6.678874
5.946649	395.426364	6.683878
5.969719	390.946068	6.688883
5.624819	396.831147	6.693888
6.117588	392.786631	6.698893
6.413452	392.851130	6.703898
6.156199	378.935961	6.708902
5.720641	368.604867	6.713907
5.649629	365.050497	6.718912
5.819076	361.860256	6.723917
5.784467	386.518247	6.728922
5.918170	387.902155	6.733926
6.360451	382.100142	6.738931
5.770332	383.625934	6.743936
5.817405	369.099931	6.748941
5.826124	375.306091	6.753946
5.923653	387.481116	6.758950
6.152546	384.221444	6.763955
5.807930	390.824663	6.768960
5.827378	374.714747	6.773965
5.811850	377.080672	6.778970
5.843056	382.922636	6.783974
5.879565	392.528715	6.788979
5.904141	398.545733	6.793984
6.030801	398.788606	6.798989
6.020285	396.493443	6.803994
6.368920	391.174345	6.808998
5.867872	377.129694	6.814003
5.879575	375.008225	6.819008
5.888758	363.341925	6.824013
5.597543	365.020203	6.829018
5.666105	365.639181	6.834022
6.211687	381.439334	6.839027
5.966845	387.099920	6.844032
5.945481	382.477889	6.849037
5.597298	380.988623	6.854042
5.593994	387.003678	6.859046
5.878116	382.238867	6.864051
5.740555	396.393316	6.869056
5.984556	385.867150	6.874061
6.286477	395.048822	6.879066
6.333760	399.192466	6.884070
6.331058	374.834781	6.889075
5.718941	375.959051	6.894080
5.868142	363.505169	6.899085
5.664128	366.008195	6.904090
5.545140	370.684094	6.909094
5.750697	376.562014	6.914099
6.315219	397.592166	6.919104
6.068377	369.504632	6.924109
5.872261	383.449943	6.929114
5.815299	376.245489	6.934118
5.765290	368.002217	6.939123
5.608107	370.785813	6.944128
5.855734	378.099841	6.949133
5.961484	391.206906	6.954138
6.102861	390.324318	6.959142
6.169775	393.597998	6.964147
5.804691	380.224918	6.969152
5.840666	375.242721	6.974157
5.749886	388.918426	6.979162
6.020056	382.675134	6.984166
6.015977	394.100440	6.989171
6.417966	388.453438	6.994176
6.336355	368.993060	6.999181
6.080715	371.798410	7.004186
5.742489	369.696968	7.009190
5.965487	363.214297	7.014195
5.654416	368.787177	7.019200
5.980147	361.231696	7.024205
6.080672	373.422061	7.029210
5.681349	379.628880	7.034214
5.695894	375.254329	7.039219
5.615752	384.166822	7.044224
6.144611	361.991161	7.049229
5.732573	373.037440	7.054234
5.724801	375.335709	7.059238
6.114884	364.546217	7.064243
6.093327	375.110528	7.069248
5.983679	376.548383	7.074253
5.742483	378.348541	7.079258
5.738353	368.642725	7.084262
5.507803	377.034605	7.089267
6.010483	383.195011	7.094272
6.283719	379.827150	7.099277
5.693128	382.941252	7.104282
6.155358	376.917811	7.109286
5.969046	370.398028	7.114291
5.763280	371.259309	7.119296
6.205484	366.254594	7.124301
5.845712	371.642113	7.129306
5.875276	367.040580	7.134310
5.870550	366.892743	7.139315
5.792384	375.070917	7.144320
5.921329	359.589277	7.149325
5.751194	370.474264	7.154330
5.735732	368.847443	7.159334
5.932485	371.958405	7.164339
5.489882	371.214775	7.169344
6.270082	383.191083	7.174349
5.802739	380.878911	7.179354
5.740776	378.743674	7.184358
6.105628	394.610122	7.189363
6.222348	390.494811	7.194368
5.906525	368.252169	7.199373
5.893402	373.101310	7.204378
5.615297	370.221642	7.209382
5.964348	372.435528	7.214387
5.872028	372.032491	7.219392
5.992105	377.718157	7.224397
6.073820	382.274026	7.229402
6.225635	374.242743	7.234406
6.035801	370.476030	7.239411
5.808065	370.236582	7.244416
5.782934	359.638703	7.249421
5.507242	364.158816	7.254426
5.645781	370.025088	7.259430
5.698516	379.350202	7.264435
5.955545	383.945042	7.269440
6.217881	388.007531	7.274445
6.260987	383.562063	7.279450
6.142583	373.342628	7.284454
6.136558	366.139689	7.289459
6.005179	371.576845	7.294464
5.953551	365.501042	7.299469
5.802610	378.104140	7.304474
6.159297	374.697894	7.309478
6.092881	372.674089	7.314483
5.743199	368.391410	7.319488
6.050158	367.710674	7.324493
5.710326	374.398560	7.329498
6.015194	368.678194	7.334502
6.345732	365.880336	7.339507
6.019000	373.176785	7.344512
6.159027	368.561108	7.349517
5.752289	371.367986	7.354522
5.854487	366.055870	7.359526
5.863989	365.760268	7.364531
5.864726	369.484083	7.369536
5.910318	365.857658	7.374541
6.010051	378.130410	7.379546
5.747877	366.766057	7.384550
5.953437	370.922861	7.389555
5.777719	370.453796	7.394560
6.046942	370.823030	7.399565
6.060902	373.408965	7.404570
6.019660	372.295558	7.409574
5.793132	365.136659	7.414579
5.592416	364.690494	7.419584
6.078398	367.999751	7.424589
5.848368	369.130594	7.429594
5.847349	367.359139	7.434598
6.114299	378.707168	7.439603
5.797071	372.144620	7.444608
6.273722	367.950772	7.449613
5.990278	375.534675	7.454618
6.129725	365.645010	7.459622
6.268322	371.824491	7.464627
6.071971	367.581065	7.469632
6.243529	350.947454	7.474637
5.907519	350.206107	7.479642
5.561263	340.788034	7.484646
5.713946	349.249570	7.489651
5.951078	366.186389	7.494656
5.983752	362.229789	7.499661
5.415999	360.632556	7.504666
6.039412	361.680299	7.509670
6.040090	368.738782	7.514675
6.050097	367.433844	7.519680
5.735557	365.360330	7.524685
5.998747	366.641688	7.529690
6.019477	368.128718	7.534694
5.689790	373.400790	7.539699
5.984941	381.536294	7.544704
5.815865	369.499279	7.549709
5.780533	372.010677	7.554714
5.821243	366.135545	7.559718
5.786515	372.800937	7.564723
6.022056	372.115571	7.569728
6.033620	362.334532	7.574733
5.914577	364.333853	7.579738
5.894792	362.989290	7.584742
5.994846	372.044389	7.589747
5.509007	363.189187	7.594752
5.913332	364.236456	7.599757
5.752660	369.706676	7.604762
6.021202	360.714293	7.609766
6.094804	362.835292	7.614771
5.607777	370.296064	7.619776
5.806117	361.868347	7.624781
5.861593	373.217869	7.629786
5.758267	360.724460	7.634790
5.696060	366.584219	7.639795
5.472613	366.774378	7.644800
5.642982	368.820104	7.649805
5.494376	374.607979	7.654810
5.626203	367.304345	7.659814
5.784169	374.423609	7.664819
5.792974	395.040946	7.669824
5.921646	387.826384	7.674829
5.875608	387.083894	7.679834
6.021979	389.297901	7.684838
6.346132	405.275141	7.689843
5.945323	391.075565	7.694848
5.903459	381.771132	7.699853
5.727857	375.063004	7.704858
5.774189	382.180779	7.709862
6.330632	392.344483	7.714867
6.073835	387.597984	7.719872
5.993207	380.112493	7.724877
6.013904	385.952941	7.729882
5.433809	382.231555	7.734886
5.562286	382.698774	7.739891
6.247536	394.977874	7.744896
5.922565	373.015076	7.749901
6.187108	368.373562	7.754906
5.778877	375.024709	7.759910
5.721310	368.813790	7.764915
5.706882	375.415890	7.769920
6.030239	384.834648	7.774925
6.072479	395.202310	7.779930
6.314335	383.819087	7.784934
6.008581	371.249818	7.789939
5.764281	379.688147	7.794944
6.067907	366.371656	7.799949
5.969632	369.943302	7.804954
5.918097	367.325533	7.809958
5.674205	367.870078	7.814963
5.583222	362.006090	7.819968
5.585405	361.123166	7.824973
5.541742	377.721170	7.829978
6.558901	392.561576	7.834982
6.311107	382.033373	7.839987
5.760962	373.317958	7.844992
6.058185	363.583911	7.849997
5.685950	371.377881	7.855002
5.735535	360.407619	7.860006
5.786530	360.773080	7.865011
5.707693	373.083299	7.870016
5.979124	376.970350	7.875021
6.199667	382.475758	7.880026
5.859791	381.744506	7.885030
5.957231	373.936882	7.890035
5.562578	373.163592	7.895040
5.891849	374.830074	7.900045
6.007409	384.401615	7.905050
6.069374	384.274967	7.910054
5.930756	380.383167	7.915059
5.682385	383.665116	7.920064
6.088117	387.047062	7.925069
6.016407	376.738051	7.930074
5.614071	379.534748	7.935078
5.923561	396.096420	7.940083
6.286356	382.833922	7.945088
5.916075	374.280154	7.950093
5.813311	369.455740	7.955098
5.795981	360.628374	7.960102
6.130552	359.414954	7.965107
5.719572	359.767376	7.970112
5.913313	360.752726	7.975117
5.950566	376.591392	7.980122
6.034970	363.913620	7.985139
5.995848	358.141709	7.990157
5.650825	376.723257	7.995174
6.356057	360.707935	8.000192
5.986994	372.388484	8.005210
5.848608	369.825734	8.010227
6.123787	360.552193	8.015245
6.003285	367.576944	8.020262
6.239874	365.100607	8.025280
5.968866	371.710293	8.030298
5.702067	368.833155	8.035315
5.855217	362.090705	8.040333
5.570090	377.043232	8.045350
5.581086	358.104018	8.050368
5.910751	382.976549	8.055386
5.472869	386.611273	8.060403
5.894162	394.450531	8.065421
6.026901	387.244219	8.070438
6.213181	382.699281	8.075456
6.309427	384.300065	8.080474
6.281930	399.988559	8.085491
6.273897	388.515641	8.090509
6.054804	390.557146	8.095526
5.783635	378.664724	8.100544
6.316527	378.092210	8.105562
5.793001	379.515552	8.110579
5.754930	373.352158	8.115597
5.912407	384.057139	8.120614
6.141212	390.945118	8.125632
6.127204	393.774985	8.130650
5.877603	392.441465	8.135667
6.228145	386.258202	8.140685
5.638289	394.552531	8.145702
5.858179	392.315488	8.150720
5.906837	395.176561	8.155738
5.786315	403.523587	8.160755
6.169951	398.111449	8.165773
5.761826	401.915080	8.170790
6.027620	390.020567	8.175808
5.932565	401.557218	8.180826
6.012077	398.758355	8.185843
6.049263	396.325880	8.190861
5.964234	404.282344	8.195878
6.080681	398.426085	8.200896
6.021404	394.670688	8.205914
6.252304	401.220678	8.210931
6.258774	388.123433	8.215949
6.355765	380.960593	8.220966
6.250687	397.355505	8.225984
6.494915	400.353190	8.231002
5.990714	399.280464	8.236019
6.116952	399.513266	8.241037
6.197456	408.207487	8.246054
6.460048	393.091453	8.251072
6.153853	396.481487	8.256090
6.243607	400.582642	8.261107
6.341084	403.357173	8.266125
6.329405	398.107959	8.271142
5.995684	390.018541	8.276160
5.965565	384.425087	8.281178
6.025295	393.166736	8.286195
6.493041	385.971049	8.291213
6.134884	398.088555	8.296230
6.412511	404.883685	8.301248
6.124926	401.646887	8.306266
6.062902	402.101688	8.311283
6.485462	395.430620	8.316301
6.389671	400.308759	8.321318
6.425651	410.770865	8.326336
6.483493	400.398442	8.331354
6.462966	404.927124	8.336371
6.736326	395.871597	8.341389
6.549231	400.877649	8.346406
6.296931	396.167900	8.351424
6.654596	390.715654	8.356442
6.348864	400.025799	8.361459
6.732294	393.957299	8.366477
6.158471	388.152394	8.371494
6.005691	370.952397	8.376512
6.143614	388.246482	8.381530
5.971502	398.371963	8.386547
6.241599	395.625289	8.391565
6.214576	411.222202	8.396582
6.235373	404.342686	8.401600
6.495837	403.535150	8.406618
6.247177	402.031072	8.411635
6.269831	397.641154	8.416653
6.375999	397.580460	8.421670
6.270750	395.492189	8.426688
6.334015	393.740425	8.431706
6.734305	398.449319	8.436723
6.419845	394.838044	8.441741
6.335251	397.003641	8.446758
6.169343	394.934341	8.451776
6.307187	401.906003	8.456794
6.069140	401.422725	8.461811
6.617359	409.775424	8.466829
6.124254	402.982740	8.471846
6.256285	402.539305	8.476864
6.771114	401.941218	8.481882
6.075896	409.381076	8.486899
6.629964	407.744911	8.491917
6.343605	403.340294	8.496934
6.164086	410.093446	8.501952
6.854127	402.856611	8.506970
6.300210	403.663034	8.511987
6.509221	396.870793	8.517005
6.463945	399.128057	8.522022
6.549678	384.317448	8.527040
6.562566	395.180787	8.532058
6.314396	402.749409	8.537075
6.764891	398.396594	8.542093
6.398365	399.012712	8.547110
6.892868	402.911597	8.552128
6.641988	401.780245	8.557146
6.561476	392.360450	8.562163
6.634304	399.080372	8.567181
6.729636	406.787675	8.572199
6.314814	401.522732	8.577216
6.764012	399.978737	8.582234
6.604833	408.836742	8.587251
6.579643	404.296531	8.592269
6.232055	411.319011	8.597287
6.193880	394.025297	8.602304
6.455489	398.415099	8.607322
6.267281	401.796115	8.612339
6.882002	396.732772	8.617357
6.509166	399.697756	8.622375
6.702833	395.356781	8.627392
6.664862	403.113371	8.632410
6.493742	395.850525	8.637427
6.490360	394.541541	8.642445
6.311770	409.707774	8.647463
6.374266	403.932548	8.652480
6.227512	406.982028	8.657498
6.333508	422.883152	8.662515
7.032916	428.359371	8.667533
6.800891	430.806843	8.672551
6.721462	422.857445	8.677568
7.119925	415.177148	8.682586
6.466090	419.858711	8.687603
6.315672	403.923770	8.692621
6.069043	421.031991	8.697639
6.584116	422.084324	8.702656
6.682243	417.998151	8.707674
6.280342	423.044177	8.712691
6.127732	420.477337	8.717709
6.403245	421.876470	8.722727
6.364247	425.483416	8.727744
6.628976	422.564012	8.732762
6.731240	447.639518	8.737779
6.883046	451.289156	8.742797
6.871394	446.626894	8.747815
6.788211	442.121006	8.752832
6.707733	423.861919	8.757850
6.591981	424.807969	8.762867
6.881705	426.236432	8.767885
6.858692	425.470156	8.772903
6.477899	427.663231	8.777920
6.542813	428.177037	8.782938
6.799397	450.318763	8.787955
7.010820	448.332345	8.792973
6.921068	443.272072	8.797991
7.017471	440.921830	8.803008
6.813311	434.061771	8.808026
6.693628	425.541175	8.813043
6.712110	424.575896	8.818061
6.795635	428.513934	8.823079
7.136143	436.410049	8.828096
6.825936	423.649570	8.833114
6.904185	431.507881	8.838131
6.701629	426.361148	8.843149
6.991940	421.695761	8.848167
6.793861	430.698725	8.853184
6.823969	430.227078	8.858202
6.890735	420.190911	8.863219
6.942601	422.625458	8.868237
6.657419	425.706098	8.873255
6.344876	439.438541	8.878272
7.274232	439.195220	8.883290
7.234809	446.431356	8.888307
6.967820	442.004760	8.893325
7.056584	432.470060	8.898343
6.967487	431.663646	8.903360
6.725820	425.797218	8.908378
6.607245	424.474723	8.913395
7.020915	437.080383	8.918413
7.165062	434.656390	8.923431
7.036487	434.291655	8.928448
7.214673	421.763918	8.933466
7.112302	417.554528	8.938483
6.786252	427.066682	8.943501
6.630985	418.261336	8.948519
6.574343	423.568841	8.953536
7.020788	432.451885	8.958554
7.015758	449.200392	8.963571
7.279355	445.981365	8.968589
7.225443	444.544597	8.973607
6.861266	439.388471	8.978624
7.016520	430.367210	8.983642
6.885960	438.466521	8.988659
7.131830	436.042368	8.993677
7.061099	442.144180	8.998695
6.747264	449.902989	9.003712
6.971686	455.718723	9.008730
6.963519	450.718248	9.013747
6.693646	460.616088	9.018765
7.296745	454.412165	9.023783
7.014979	464.349740	9.028800
7.079313	450.833134	9.033818
7.337333	458.767430	9.038835
7.293616	466.891015	9.043853
7.258188	456.940267	9.048871
6.960801	459.397984	9.053888
7.161641	447.343199	9.058906
7.169457	457.014494	9.063923
7.287748	450.037635	9.068941
7.105917	440.021474	9.073959
6.830539	446.167975	9.078976
7.228325	443.694773	9.083994
7.483152	455.018850	9.089011
7.346148	448.836218	9.094029
6.896723	434.260893	9.099047
6.822610	443.919773	9.104064
7.149824	446.314337	9.109082
7.057588	443.870576	9.114099
6.941876	453.078393	9.119117
7.194993	445.146307	9.124135
6.577034	460.438227	9.129152
6.871680	453.948123	9.134170
7.054548	454.304595	9.139187
7.249011	447.943798	9.144205
7.384299	450.829175	9.149223
7.230317	454.214306	9.154240
7.041280	453.048014	9.159258
7.121037	450.189146	9.164275
6.783758	455.417557	9.169293
7.379970	452.503014	9.174311
7.427001	450.062678	9.179328
7.151736	447.426692	9.184346
7.363687	456.576860	9.189363
6.990164	458.134492	9.194381
7.473078	462.966155	9.199399
7.287354	455.601433	9.204416
7.592005	451.353507	9.209434
7.774336	457.491412	9.214451
7.400002	458.957655	9.219469
7.302877	452.598362	9.224487
7.376276	460.744620	9.229504
7.386969	460.594745	9.234522
7.711777	461.815747	9.239539
7.373544	457.826336	9.244557
7.348542	458.256403	9.249575
7.402851	456.020050	9.254592
7.679308	452.751670	9.259610
7.529349	460.926613	9.264627
7.566144	452.643415	9.269645
7.424791	459.863970	9.274663
7.473924	458.994871	9.279680
7.664400	452.480065	9.284698
7.396960	459.436357	9.289715
6.953489	459.909901	9.294733
7.425839	456.345744	9.299751
7.502564	453.989115	9.304768
7.460102	447.409824	9.309786
7.546781	462.581874	9.314803
6.889493	456.196742	9.319821
7.396656	456.600230	9.324839
7.257353	456.085700	9.329856
7.636896	452.659159	9.334874
7.525236	450.982135	9.339891
7.161512	455.403659	9.344909
7.607217	449.296982	9.349927
7.406198	454.551379	9.354944
7.453744	457.283250	9.359962
7.377797	455.206159	9.364979
7.255956	463.193663	9.369997
7.407116	460.648649	9.375015
7.277627	461.256031	9.380032
7.047109	454.270708	9.385050
7.142747	462.864755	9.390067
7.251202	477.698896	9.395085
7.561764	470.827601	9.400103
7.795403	483.026005	9.405120
7.804408	475.343590	9.410138
7.858278	473.129394	9.415155
7.652064	465.455458	9.420173
7.480014	457.482687	9.425191
7.294500	460.607675	9.430208
7.414214	473.890571	9.435226
7.302996	476.249694	9.440243
7.052460	495.823249	9.445261
7.633066	482.405606	9.450279
7.541295	485.875668	9.455296
7.570484	485.104366	9.460314
7.802570	480.299765	9.465331
7.411468	489.629644	9.470349
7.662387	478.819830	9.475367
7.490790	485.559147	9.480384
7.592528	488.156301	9.485402
7.753491	485.474049	9.490419
7.688730	488.191963	9.495437
7.961332	483.863846	9.500455
7.534963	489.279793	9.505472
7.878314	485.076287	9.510490
7.794350	482.773235	9.515507
7.706967	487.735285	9.520525
7.936138	475.284728	9.525543
7.950185	491.531675	9.530560
7.714445	491.350985	9.535578
7.749752	485.403271	9.540595
7.655649	476.209621	9.545613
7.415778	477.446516	9.550631
7.846134	486.205878	9.555648
7.444846	478.685576	9.560666
7.859137	476.790443	9.565683
7.506563	490.784815	9.570701
7.897110	482.468266	9.575719
8.195791	484.813658	9.580736
7.846692	479.235441	9.585754
7.548730	477.922115	9.590771
7.415286	477.668594	9.595789
8.143835	471.508124	9.600807
7.920075	478.388153	9.605824
7.676205	481.632741	9.610842
7.890792	475.458126	9.615859
7.426291	478.412239	9.620877
7.687054	476.367594	9.625895
7.832689	478.026919	9.630912
7.839495	473.030403	9.635930
7.742205	475.986939	9.640947
7.822530	487.609774	9.645965
7.614165	483.167670	9.650983
7.768658	488.716664	9.656000
7.803958	504.818284	9.661018
8.016766	503.699478	9.666035
8.241962	502.834349	9.671053
8.015442	495.980925	9.676071
7.953652	492.330040	9.681088
8.059810	474.963142	9.686106
8.349361	476.101306	9.691123
7.977232	485.349316	9.696141
8.024916	479.888808	9.701159
7.732210	482.610879	9.706176
8.074673	482.323816	9.711194
7.976776	479.432819	9.716211
7.959352	479.681821	9.721229
7.838470	486.394257	9.726247
8.137570	487.259530	9.731264
7.644637	487.816563	9.736282
7.877966	489.512641	9.741299
7.454958	490.986512	9.746317
8.033504	499.448109	9.751335
8.178341	506.983600	9.756352
8.053498	512.203988	9.761370
8.352555	504.170004	9.766387
8.225835	498.168778	9.771405
8.249222	486.110214	9.776423
7.915091	493.597670	9.781440
7.743749	484.637021	9.786458
7.821928	500.122855	9.791475
8.050827	502.977795	9.796493
8.313784	501.466128	9.801511
8.367381	510.281378	9.806528
7.937565	495.848096	9.811546
8.201678	496.090855	9.816563
8.274364	515.288744	9.821581
8.276040	486.110386	9.826599
8.114455	475.819637	9.831616
8.044865	480.494879	9.836634
8.112116	482.324274	9.841651
8.158202	494.608877	9.846669
8.182055	495.523589	9.851687
8.355501	484.561810	9.856704
7.977224	485.567931	9.861722
8.467845	490.180646	9.866739
8.016428	486.859051	9.871757
8.278581	497.440403	9.876775
8.444411	498.074097	9.881792
8.065736	490.676477	9.886810
8.127731	488.685066	9.891827
8.053703	488.330718	9.896845
8.358036	502.048605	9.901863
8.385606	503.660160	9.906880
8.037495	502.951129	9.911898
8.471766	502.173160	9.916915
8.379782	518.048585	9.921933
8.261952	499.615394	9.926951
8.477830	499.846776	9.931968
8.022006	505.980546	9.936986
8.060455	498.454451	9.942003
8.413673	510.242824	9.947021
8.144693	503.591707	9.952039
8.659218	504.467409	9.957056
8.075623	509.425164	9.962074
7.833397	505.101968	9.967091
8.421183	504.713351	9.972109
8.707806	508.499666	9.977127
8.643736	505.556028	9.982144
8.268274	507.350651	9.987162
8.364207	511.289919	9.992179
8.295184	510.552938	9.997197
8.137142	503.871817	10.002215
8.156981	511.101849	10.007232
8.161519	514.493712	10.012250
8.322595	510.943602	10.017267
8.113591	518.474578	10.022285
8.115073	508.293958	10.027303
8.461632	511.367146	10.032320
8.200549	506.251651	10.037338
8.855119	509.854084	10.042355
8.600705	502.522195	10.047373
8.444949	502.606681	10.052391
8.289736	504.388884	10.057408
8.140271	506.653020	10.062426
8.322904	506.413090	10.067443
8.408290	506.630204	10.072461
8.117211	508.664067	10.077479
8.400842	517.149791	10.082496
8.804238	530.202089	10.087514
8.898764	526.902243	10.092531
8.707066	525.064184	10.097549
8.452653	508.959252	10.102567
8.667219	507.963246	10.107584
8.287501	515.915440	10.112602
8.772983	500.641317	10.117619
8.369016	496.548590	10.122637
8.345096	507.436699	10.127655
8.523402	522.054807	10.132672
8.797161	528.677024	10.137690
8.851248	532.449286	10.142707
8.394948	520.065074	10.147725
8.222468	527.927999	10.152743
8.583343	522.478365	10.157760
8.628833	535.526786	10.162778
9.049182	534.141933	10.167795
8.880406	529.034059	10.172813
8.386852	537.247093	10.177831
8.438449	528.882646	10.182848
8.392104	529.641103	10.187866
8.775268	523.897646	10.192883
8.719157	542.904308	10.197901
8.717804	539.890878	10.202919
8.394394	535.776052	10.207936
8.177155	536.886330	10.212954
8.534607	532.292445	10.217971
8.645447	532.518194	10.222989
8.737111	528.095341	10.228007
8.827501	530.927806	10.233024
8.365615	526.721072	10.238042
8.843059	520.464232	10.243059
8.565379	525.863204	10.248077
8.498536	527.398036	10.253095
9.003565	531.008126	10.258112
8.837622	539.699999	10.263130
8.930178	520.015695	10.268147
8.993254	518.857233	10.273165
8.743738	524.406425	10.278183
8.744552	517.703564	10.283200
8.876335	523.963020	10.288218
8.894026	528.858126	10.293235
8.522796	532.668626	10.298253
8.824629	537.269909	10.303271
8.953040	539.364279	10.308288
9.035210	543.873750	10.313306
9.149239	530.021097	10.318323
8.863111	524.076397	10.323341
8.773059	527.530419	10.328359
8.930214	532.463634	10.333376
8.706575	539.955887	10.338394
8.767100	535.771438	10.343411
9.142011	537.764070	10.348429
8.952118	535.524944	10.353447
9.336527	524.514308	10.358464
8.604522	540.903440	10.363482
8.551038	530.052928	10.368499
9.147414	545.861548	10.373517
8.868412	556.685514	10.378535
8.758805	551.113930	10.383552
8.833722	554.728300	10.388570
9.145205	558.854710	10.393587
9.072184	559.267057	10.398605
8.812131	559.361573	10.403623
9.243453	549.722645	10.408640
9.247183	557.296044	10.413658
9.360101	559.998754	10.418675
9.417549	549.560035	10.423693
9.021642	541.325658	10.428711
9.463160	531.833463	10.433728
9.030056	534.239873	10.438746
8.929086	528.509154	10.443763
9.113462	531.844440	10.448781
8.821494	529.236304	10.453799
8.880840	525.055198	10.458816
9.009178	537.563626	10.463834
9.106814	539.167361	10.468851
9.622958	545.581195	10.473869
8.848566	552.184613	10.478887
9.230964	532.571645	10.483904
9.048599	537.311908	10.488922
9.095101	544.058100	10.493939
9.403900	543.927788	10.498957
9.073714	545.658516	10.503975
9.345747	541.188464	10.508992
9.193487	540.057429	10.514010
9.143627	529.446189	10.519027
9.400955	539.624383	10.524045
9.044988	539.222692	10.529063
9.348838	523.958073	10.534080
9.184875	534.467358	10.539098
9.230409	540.582545	10.544115
9.264092	537.882359	10.549133
8.986107	552.019725	10.554151
9.215466	542.832163	10.559168
9.182486	558.789897	10.564186
9.227436	550.454883	10.569203
9.553863	553.149384	10.574221
9.215298	556.235254	10.579239
9.329626	551.411216	10.584256
9.438175	562.209175	10.589274
9.362248	557.522242	10.594291
9.840100	550.668886	10.599309
9.614773	549.981640	10.604327
9.169696	528.626953	10.609344
9.232669	540.725907	10.614362
9.097143	540.355948	10.619379
9.423912	541.295783	10.624397
9.000914	555.152918	10.629415
9.002302	552.221107	10.634432
9.120082	558.675271	10.639450
9.282682	561.064086	10.644467
9.358916	558.193129	10.649485
9.293873	562.331199	10.654503
9.454538	553.615138	10.659520
9.385011	555.809951	10.664538
9.446960	554.979864	10.669555
9.782012	545.131963	10.674573
9.312471	558.797579	10.679591
9.524841	551.285237	10.684608
9.431583	551.524031	10.689626
9.612203	556.380994	10.694643
9.139744	553.422441	10.699661
9.369947	553.241328	10.704679
9.713798	546.118638	10.709696
9.594216	547.661736	10.714714
9.592007	549.782885	10.719731
9.446553	553.652687	10.724749
9.158553	557.655277	10.729767
9.449119	554.198478	10.734784
9.504415	565.178351	10.739802
9.605443	581.818847	10.744819
9.828969	575.740627	10.749837
9.613635	570.043593	10.754855
9.508873	559.702866	10.759872
9.258178	564.614788	10.764890
9.350949	565.465057	10.769907
9.855090	573.849987	10.774925
9.458896	584.370442	10.779943
9.527128	579.105498	10.784960
9.780511	580.274583	10.789978
9.813083	569.527327	10.794995
9.799977	579.539636	10.800013
9.641050	584.680179	10.805031
9.570347	580.456321	10.810048
9.921358	574.844117	10.815066
9.797053	586.473832	10.820083
10.003421	590.967011	10.825101
9.622531	587.994105	10.830119
9.764265	574.566263	10.835136
9.781658	583.052709	10.840154
9.766019	573.957167	10.845171
9.882033	579.237665	10.850189
9.484606	577.463393	10.855207
9.550205	583.026345	10.860224
9.633201	570.696454	10.865242
9.616651	577.755492	10.870259
10.270588	578.782922	10.875277
9.744736	576.495446	10.880295
9.853371	574.714465	10.885312
10.187055	575.732114	10.890330
10.072045	583.317817	10.895347
9.898329	582.524654	10.900365
9.575360	583.941833	10.905383
9.835398	578.646837	10.910400
9.828470	581.434598	10.915418
9.392283	583.803627	10.920435
10.009569	577.692113	10.925453
10.032712	583.021878	10.930471
9.554399	578.076097	10.935488
10.290980	580.255061	10.940506
9.530321	583.990890	10.945523
9.876522	575.375136	10.950541
9.573709	579.481037	10.955559
9.939134	573.920222	10.960576
10.015058	568.461574	10.965594
10.001744	580.600910	10.970611
10.267073	571.997828	10.975629
9.818632	583.466891	10.980647
10.367392	583.055986	10.985664
9.974955	576.648246	10.990682
9.922880	580.522358	10.995699
10.119634	579.424998	11.000717
9.992225	583.358251	11.005735
9.919048	586.219509	11.010752
10.171357	577.129319	11.015770
10.120684	573.277862	11.020787
9.810776	572.105255	11.025805
9.926130	580.418561	11.030823
10.197657	579.741827	11.035840
10.053185	576.725569	11.040858
9.897786	575.667607	11.045875
10.239764	589.834096	11.050893
10.168277	600.868569	11.055911
10.144730	601.383617	11.060928
10.375819	590.236019	11.065946
10.166953	578.232717	11.070963
9.862408	572.537037	11.075981
10.236629	599.018647	11.080999
10.234118	599.820731	11.086016
10.359352	602.493115	11.091034
10.257706	600.252777	11.096051
10.674193	593.121844	11.101069
10.038364	582.520333	11.106087
10.333052	577.453435	11.111104
10.010924	573.764430	11.116122
10.050227	583.784308	11.121139
10.323837	596.699202	11.126157
10.138841	599.211911	11.131175
10.139491	609.521880	11.136192
10.448277	608.779347	11.141210
10.268116	612.960712	11.146227
10.409563	602.676057	11.151245
10.599459	611.659348	11.156263
10.481294	618.709077	11.161280
10.478436	601.807258	11.166298
10.419007	590.651530	11.171315
10.209325	582.634107	11.176333
10.482272	596.448502	11.181351
10.175775	594.227638	11.186368
10.728467	597.505228	11.191386
10.739947	589.579380	11.196403
10.421001	586.584146	11.201421
10.068446	583.846641	11.206439
10.314373	591.798669	11.211456
10.693532	597.710125	11.216474
10.311382	602.816222	11.221491
10.480435	599.574112	11.226509
10.828176	604.998191	11.231527
10.497553	589.416364	11.236544
10.867189	579.073879	11.241562
10.247284	586.470451	11.246579
10.567286	583.832693	11.251597
10.133557	584.276311	11.256615
10.567873	600.959278	11.261632
10.284094	608.710289	11.266650
10.363764	615.012656	11.271667
10.596617	609.750312	11.276685
10.709100	603.269762	11.281703
10.731834	615.621222	11.286720
10.698486	600.866961	11.291738
10.636953	607.396575	11.296755
10.428878	598.517363	11.301773
10.514846	608.697200	11.306791
10.351395	610.051518	11.311808
10.743987	597.439571	11.316826
10.741563	610.047433	11.321843
10.593032	608.944211	11.326861
10.576054	620.279423	11.331879
10.541966	618.129483	11.336896
10.216183	611.480915	11.341914
10.219746	618.319068	11.346931
10.151973	617.004378	11.351949
10.254624	624.196235	11.356967
10.514865	635.825690	11.361984
10.753882	629.360019	11.367002
10.745709	638.061934	11.372019
10.915403	641.667783	11.377037
11.201233	634.639355	11.382055
10.816097	646.786502	11.387072
11.144938	639.309522	11.392090
10.559226	623.029179	11.397107
10.889574	629.437441	11.402125
10.407397	630.504029	11.407143
10.584456	641.414378	11.412160
10.807981	640.047734	11.417178
10.491730	642.145515	11.422195
10.792790	637.386870	11.427213
10.555446	635.486524	11.432231
10.581349	642.785088	11.437248
10.610227	641.351111	11.442266
10.746642	640.490419	11.447283
10.522104	641.646028	11.452301
11.046186	643.741531	11.457319
10.869292	646.735814	11.462336
10.785972	626.242664	11.467354
10.798674	651.597576	11.472371
11.017607	659.415009	11.477389
11.115022	666.383642	11.482407
11.167348	658.915266	11.487424
10.828665	645.117678	11.492442
11.170932	649.510684	11.497459
11.126759	652.127567	11.502477
11.028886	648.971452	11.507495
10.737292	645.823600	11.512512
11.065716	652.658203	11.517530
11.271623	655.507302	11.522547
11.180500	657.036483	11.527565
11.242701	643.510598	11.532583
10.774776	646.238057	11.537600
11.185245	639.376290	11.542618
11.049096	644.743655	11.547635
11.158477	654.093031	11.552653
11.266290	642.832172	11.557671
10.969159	648.833829	11.562688
11.168315	641.437128	11.567706
11.206672	648.216193	11.572723
11.182118	648.605168	11.577741
11.075698	642.648050	11.582759
11.184645	647.945455	11.587776
11.469886	649.153734	11.592794
11.112936	646.432687	11.597811
11.356967	645.343695	11.602829
11.114462	640.073772	11.607847
11.146295	652.840397	11.612864
11.502451	654.271094	11.617882
11.343270	649.436235	11.622899
11.123703	640.435727	11.627917
11.318356	636.482702	11.632935
11.345657	651.468557	11.637952
11.188768	641.192755	11.642970
11.131998	651.675846	11.647987
11.152821	658.435572	11.653005
11.465141	659.399768	11.658023
11.486739	663.969253	11.663040
11.871301	665.281891	11.668058
11.441820	648.453184	11.673075
11.250452	643.168936	11.678093
11.485842	643.318368	11.683111
10.971950	641.492910	11.688128
11.307844	649.860056	11.693146
11.483311	659.464168	11.698163
11.466641	669.757951	11.703181
11.764216	657.851969	11.708199
11.322867	653.206487	11.713216
11.352584	647.527837	11.718234
11.542508	653.033461	11.723251
11.415016	659.270473	11.728269
11.687533	660.897311	11.733287
11.529328	665.662226	11.738304
11.451385	650.671914	11.743322
11.302166	649.660316	11.748339
11.219606	662.088267	11.753357
11.067887	657.946511	11.758375
11.075046	666.150578	11.763392
11.234662	659.747829	11.768410
11.912635	666.840093	11.773427
11.634391	668.651057	11.778445
11.596846	657.797970	11.783463
11.578391	659.467243	11.788480
11.454709	658.937635	11.793498
11.428691	661.400198	11.798515
11.724781	667.652895	11.803533
11.643818	656.992804	11.808551
11.740480	668.247125	11.813568
11.686341	654.212442	11.818586
11.918209	661.620753	11.823603
11.256205	665.281181	11.828621
11.714391	657.332649	11.833639
11.602951	660.559674	11.838656
11.338050	656.224215	11.843674
11.517446	670.378372	11.848691
11.718683	680.215141	11.853709
11.977337	681.973542	11.858727
11.897333	677.094712	11.863744
11.685619	679.769408	11.868762
11.961224	670.088543	11.873779
11.659681	669.078720	11.878797
11.807002	656.890169	11.883815
12.177638	671.509823	11.888832
12.050346	670.712538	11.893850
11.555630	657.488496	11.898867
11.781116	660.757404	11.903885
11.901334	656.778168	11.908903
11.602060	664.067730	11.913920
11.893989	678.857511	11.918938
12.143492	681.160143	11.923955
11.907666	677.293492	11.928973
12.008085	672.048724	11.933991
11.824206	667.833111	11.939008
12.017641	672.735435	11.944026
12.218575	679.328092	11.949043
11.813591	670.624864	11.954061
11.943036	666.801969	11.959079
12.135588	671.761235	11.964096
11.853652	662.344456	11.969114
12.338131	664.496659	11.974131
12.046757	671.601950	11.979149
11.993311	650.832693	11.984167
12.096928	666.150585	11.989184
11.766478	659.202929	11.994202
11.888226	668.635582	11.999219
11.971527	681.583511	12.004237
12.337058	679.885346	12.009255
12.083589	686.700682	12.014272
11.930423	678.390338	12.019290
11.968718	690.215550	12.024307
11.851841	697.255640	12.029325
12.011017	691.092790	12.034343
12.176122	703.879596	12.039360
12.144431	692.656342	12.044378
12.303542	688.762523	12.049395
12.084221	694.029325	12.054413
12.231194	684.248686	12.059431
12.364813	690.690949	12.064448
12.319943	684.219245	12.069466
12.267288	690.106872	12.074483
12.279470	689.975697	12.079501
12.578601	689.080040	12.084519
12.258565	688.259305	12.089536
12.074158	694.296964	12.094554
12.248103	677.850208	12.099571
12.108933	677.275690	12.104589
12.178687	671.963143	12.109607
12.608964	680.902494	12.114624
12.006673	686.860459	12.119642
12.553084	681.959218	12.124659
11.816841	686.265598	12.129677
12.672760	682.546624	12.134695
12.065148	689.733029	12.139712
12.239875	685.843076	12.144730
12.349887	688.798724	12.149747
12.043925	692.346567	12.154765
12.213937	684.408461	12.159783
12.268864	687.356961	12.164800
12.476810	689.981684	12.169818
12.640476	700.726911	12.174835
12.098355	707.003658	12.179853
12.484720	702.361018	12.184871
12.330478	713.531603	12.189888
12.297335	712.915225	12.194906
12.830424	712.838132	12.199923
12.570317	716.025345	12.204941
12.673378	711.275613	12.209959
12.517832	710.293405	12.214976
12.528647	711.184925	12.219994
12.845368	709.554364	12.225011
12.665559	712.170418	12.230029
12.676740	703.771196	12.235047
12.816221	697.636676	12.240064
12.578687	707.665285	12.245082
12.795435	698.034651	12.250099
12.399568	690.134714	12.255117
12.350846	696.927441	12.260135
12.507856	702.371966	12.265152
12.641165	707.081749	12.270170
12.828195	699.125191	12.275187
12.580486	708.966047	12.280205
12.942367	712.431345	12.285223
12.695394	705.824041	12.290240
12.508607	707.207269	12.295258
12.935507	703.861624	12.300275
12.878567	708.263545	12.305293
12.683245	701.900614	12.310311
13.077689	702.709935	12.315328
12.752795	712.244150	12.320346
12.883970	704.750777	12.325363
12.602511	702.721637	12.330381
12.924094	700.137263	12.335399
13.038055	709.315538	12.340416
12.667282	698.934359	12.345434
12.909607	698.265352	12.350451
12.854016	696.333367	12.355469
12.674964	698.078299	12.360487
12.450645	701.786921	12.365504
12.665328	691.793697	12.370522
13.024354	701.182878	12.375539
13.374650	699.793211	12.380557
12.990798	704.015978	12.385575
12.918171	708.985246	12.390592
12.832931	700.029933	12.395610
12.838790	700.136434	12.400627
12.928332	704.026253	12.405645
12.902113	701.540555	12.410663
12.837454	705.978399	12.415680
12.884083	709.477312	12.420698
12.759623	707.723373	12.425715
13.218702	717.892149	12.430733
13.119566	715.335823	12.435751
13.241804	708.386647	12.440768
12.768904	718.060820	12.445786
13.430102	715.495816	12.450803
12.916769	716.608316	12.455821
12.956967	726.337800	12.460839
13.092234	724.350660	12.465856
12.880498	724.929912	12.470874
13.034187	726.960383	12.475891
12.945447	736.773191	12.480909
13.132679	723.918777	12.485927
13.375694	731.498939	12.490944
13.272877	732.881636	12.495962
13.239631	731.400581	12.500979
13.182950	739.349597	12.505997
12.952268	735.245442	12.511015
13.183567	733.738717	12.516032
12.915471	733.436862	12.521050
13.136438	724.780698	12.526067
13.435942	727.208045	12.531085
13.388239	724.902435	12.536103
13.368944	726.966321	12.541120
13.136772	733.330214	12.546138
13.381432	726.923583	12.551155
13.505436	721.577275	12.556173
13.410201	722.557995	12.561191
13.435556	729.026703	12.566208
13.454315	737.563501	12.571226
13.668628	732.591204	12.576243
13.536251	727.414453	12.581261
13.364704	728.053680	12.586279
13.984021	723.466053	12.591296
13.629189	737.678722	12.596314
13.929307	728.609367	12.601331
13.809922	729.111032	12.606349
13.705372	741.873844	12.611367
13.553708	732.698548	12.616384
13.314612	734.083662	12.621402
13.729117	722.156161	12.626419
13.832921	723.837842	12.631437
13.735973	732.522154	12.636455
13.850972	725.075489	12.641472
13.554815	728.479791	12.646490
13.418818	721.558448	12.651507
13.425841	727.039105	12.656525
13.540756	735.592394	12.661543
13.946365	722.845776	12.666560
13.423037	735.387020	12.671578
13.758563	719.681770	12.676595
13.641713	728.378666	12.681613
13.587796	729.943049	12.686631
13.720908	727.990961	12.691648
13.472817	732.602718	12.696666
13.765164	727.308928	12.701683
13.299025	724.526081	12.706701
13.383201	737.436044	12.711719
13.750628	735.160063	12.716736
13.540624	738.478286	12.721754
13.384879	724.626725	12.726771
13.514784	741.281780	12.731789
13.566577	748.358579	12.736807
13.921162	744.812818	12.741824
13.730138	755.951323	12.746842
13.847175	753.200175	12.751859
13.959957	747.836683	12.756877
14.018225	750.948772	12.761895
13.992418	741.220419	12.766912
13.903732	751.351963	12.771930
14.138935	749.099854	12.776947
14.585214	755.565736	12.781965
13.975828	753.666865	12.786983
14.160291	753.628618	12.792000
13.734066	750.814266	12.797018
14.110629	748.880836	12.802035
13.874795	748.233098	12.807053
13.843252	748.907194	12.812071
13.950396	747.116963	12.817088
14.111131	758.162485	12.822106
13.934504	745.428182	12.827123
14.208215	743.605542	12.832141
13.974155	752.459671	12.837159
14.198409	755.416365	12.842176
14.268597	748.809844	12.847194
14.090320	757.560561	12.852211
14.243333	744.471652	12.857229
14.039864	740.707216	12.862247
14.412181	751.760608	12.867264
14.234080	752.883702	12.872282
14.354955	755.935489	12.877299
14.652798	744.357612	12.882317
14.393074	736.079717	12.887335
14.241409	727.119019	12.892352
13.823108	739.050517	12.897370
14.019504	743.810385	12.902387
14.328556	746.611780	12.907405
14.260682	749.989786	12.912423
14.136146	742.823642	12.917440
14.134473	747.724998	12.922458
14.255406	750.019381	12.927475
13.861516	750.781808	12.932493
13.880051	754.417676	12.937511
13.720248	753.817986	12.942528
13.765035	754.584264	12.947546
13.796737	766.543103	12.952563
14.371558	783.346238	12.957581
14.300202	775.291275	12.962599
14.870767	771.512852	12.967616
14.481082	778.624121	12.972634
14.551771	774.652619	12.977651
14.385430	775.360460	12.982669
14.434015	780.298132	12.987687
14.668745	779.633468	12.992704
14.275777	781.544470	12.997722
14.533508	779.591785	13.002739
14.818123	772.648701	13.007757
14.873044	776.039030	13.012775
14.976859	772.349518	13.017792
14.643840	769.889790	13.022810
14.805728	779.486626	13.027827
15.166093	773.797155	13.032845
14.805298	783.671549	13.037863
14.786054	772.155960	13.042880
14.663034	766.876745	13.047898
14.811601	771.240171	13.052915
15.055628	758.187485	13.057933
14.607043	751.526546	13.062951
14.667567	759.753853	13.067968
14.498225	755.125685	13.072986
14.750067	757.462674	13.078003
14.761460	768.323318	13.083021
14.701409	774.240534	13.088039
14.669945	772.617185	13.093056
14.724614	775.013472	13.098074
14.807563	777.755624	13.103091
14.993749	772.775100	13.108109
14.922533	777.059353	13.113127
15.135219	771.494008	13.118144
14.763182	774.329538	13.123162
14.737597	773.355366	13.128179
15.052332	773.135760	13.133197
14.966115	774.263394	13.138215
14.861219	781.087045	13.143232
15.090035	780.697864	13.148250
15.064837	774.030540	13.153267
15.063657	764.683326	13.158285
14.991380	768.308179	13.163303
15.030225	760.207554	13.168320
14.911937	748.672784	13.173338
14.920129	773.422660	13.178355
15.003551	765.378164	13.183373
14.827773	774.904828	13.188391
14.799214	774.104692	13.193408
15.065597	779.879243	13.198426
15.013993	781.951354	13.203443
15.216618	782.601385	13.208461
14.893836	781.487585	13.213479
14.902620	775.957341	13.218496
14.767800	776.521387	13.223514
15.096026	781.412089	13.228531
15.117728	772.724007	13.233549
14.631306	778.837417	13.238567
15.077658	775.532893	13.243584
15.415739	799.009815	13.248602
15.194372	796.381110	13.253619
15.391237	796.997330	13.258637
14.735158	799.268295	13.263655
15.185218	794.965948	13.268672
15.234419	805.517732	13.273690
15.328937	799.671090	13.278707
15.517370	790.196323	13.283725
15.062885	796.187969	13.288743
15.486329	804.472043	13.293760
15.450923	799.179091	13.298778
15.484487	811.267058	13.303795
15.621458	799.458730	13.308813
15.240430	800.591531	13.313831
15.339101	798.846803	13.318848
15.656075	800.356236	13.323866
15.503099	804.069479	13.328883
15.322335	795.113306	13.333901
15.537593	794.031970	13.338919
15.578102	802.284523	13.343936
15.674518	805.264411	13.348954
15.548361	798.556092	13.353971
15.506067	802.119449	13.358989
15.278601	800.350082	13.364007
15.363343	798.651719	13.369024
15.660069	798.296079	13.374042
15.546988	797.098928	13.379059
15.748621	799.519529	13.384077
15.498641	802.771443	13.389095
15.556676	792.016908	13.394112
15.381287	790.709599	13.399130
15.735441	802.365475	13.404147
15.789833	791.194943	13.409165
15.471565	803.729352	13.414183
15.435253	794.258238	13.419200
15.486075	795.575841	13.424218
15.801494	811.321421	13.429235
15.964797	802.472282	13.434253
15.577238	806.184411	13.439271
15.732976	813.320690	13.444288
15.881717	818.835974	13.449306
15.762467	825.482009	13.454323
16.192246	818.531942	13.459341
15.937350	809.792505	13.464359
15.902833	793.308878	13.469376
16.089123	792.399338	13.474394
15.921340	791.709378	13.479411
16.038316	792.293933	13.484429
15.780952	795.979349	13.489447
15.822243	797.746572	13.494464
15.998488	795.106061	13.499482
16.168037	794.732478	13.504499
16.182455	787.134287	13.509517
15.966938	792.700325	13.514535
15.890106	788.534182	13.519552
16.080560	777.159304	13.524570
16.123088	793.354726	13.529587
16.332399	784.056572	13.534605
15.979447	790.007062	13.539623
15.790056	796.380052	13.544640
16.306061	788.128913	13.549658
16.350741	789.750436	13.554675
16.204665	784.370686	13.559693
16.260188	788.269010	13.564711
16.443812	786.059692	13.569728
16.539542	790.412465	13.574746
16.444577	787.640880	13.579763
16.403752	791.901440	13.584781
16.132844	785.234741	13.589799
16.109910	786.661730	13.594816
16.253081	778.712008	13.599834
15.781216	786.943849	13.604851
16.124644	785.179709	13.609869
15.941407	789.083884	13.614887
15.981476	807.630788	13.619904
16.189899	801.605351	13.624922
16.233827	808.582420	13.629939
16.551610	802.700795	13.634957
16.562092	804.472846	13.639975
16.312722	798.585410	13.644992
16.703183	802.453349	13.650010
16.426509	818.228589	13.655027
16.472150	821.137540	13.660045
16.694108	812.433841	13.665063
16.405158	817.033087	13.670080
17.064679	816.349203	13.675098
16.222989	810.942735	13.680115
16.528793	816.180944	13.685133
16.533247	817.815085	13.690151
16.362006	819.334741	13.695168
16.327841	815.411217	13.700186
16.437409	811.127500	13.705203
16.569469	806.360576	13.710221
16.318745	811.954227	13.715239
16.570776	813.918807	13.720256
16.640628	806.274053	13.725274
16.394430	821.855172	13.730291
16.742478	815.987736	13.735309
16.222428	818.537193	13.740327
16.135660	828.466507	13.745344
16.627924	828.121255	13.750362
16.724466	840.691682	13.755379
16.827658	839.747823	13.760397
17.124047	834.080980	13.765415
17.260520	839.957957	13.770432
17.054653	827.505890	13.775450
16.747994	825.802578	13.780467
16.707110	811.355438	13.785485
17.336363	827.351663	13.790503
16.739441	823.184950	13.795520
16.719672	802.022074	13.800538
16.767044	821.580866	13.805555
17.242486	838.409092	13.810573
16.950055	818.090498	13.815591
16.708868	819.583243	13.820608
17.027999	827.694323	13.825626
17.147917	834.160876	13.830643
17.132881	828.990956	13.835661
17.150482	821.660498	13.840679
16.747564	813.509144	13.845696
17.281011	824.934969	13.850714
16.684276	827.670014	13.855731
16.927410	834.164598	13.860749
16.809531	835.928361	13.865767
16.692902	842.255253	13.870784
17.044779	831.726056	13.875802
17.250231	841.486515	13.880819
17.067964	837.030766	13.885837
17.301010	832.894956	13.890855
17.090178	835.506421	13.895872
17.555745	821.595306	13.900890
17.193079	829.642798	13.905907
17.138477	826.584014	13.910925
17.290178	830.887002	13.915943
17.142751	832.058943	13.920960
17.653073	839.887606	13.925978
17.231293	840.578667	13.930995
17.206371	842.343645	13.936013
17.345985	838.086773	13.941031
17.083206	833.343836	13.946048
17.183351	836.569299	13.951066
17.029185	840.948616	13.956083
17.376480	848.998488	13.961101
17.467138	853.014398	13.966119
17.717127	853.502374	13.971136
17.597137	852.429380	13.976154
17.414414	846.531486	13.981171
17.227859	840.596325	13.986189
17.611345	851.998326	13.991207
17.615972	853.285301	13.996224
18.135254	855.605647	14.001242
17.771554	846.889551	14.006259
17.689976	838.523734	14.011277
17.606779	829.757386	14.016295
17.424670	828.836137	14.021312
17.804070	830.869126	14.026330
17.450394	830.132550	14.031347
17.458379	829.197297	14.036365
17.632504	846.416726	14.041383
18.049098	859.426173	14.046400
18.058244	838.624800	14.051418
17.699597	830.501215	14.056435
17.478486	834.414490	14.061453
17.661819	839.637182	14.066471
17.654109	855.329287	14.071488
18.384684	847.969158	14.076506
17.804035	841.417241	14.081523
17.538497	832.136659	14.086541
17.602400	836.390288	14.091559
18.057420	839.938849	14.096576
18.255081	847.311571	14.101594
17.951690	834.148939	14.106611
17.701219	841.800158	14.111629
17.924437	838.066677	14.116647
18.141625	847.891573	14.121664
18.146116	843.460209	14.126682
18.024042	837.568595	14.131699
17.799277	838.948315	14.136717
17.983004	841.030898	14.141735
17.773801	855.145102	14.146752
18.073813	854.214586	14.151770
18.149346	862.594224	14.156787
17.888371	859.160667	14.161805
18.193430	856.910223	14.166823
18.100887	861.699615	14.171840
18.024084	851.698324	14.176858
18.320601	853.053174	14.181875
18.229934	851.953495	14.186893
18.128301	851.603465	14.191911
17.941331	855.268396	14.196928
18.299796	855.101899	14.201946
18.050627	868.919416	14.206963
17.519626	857.420838	14.211981
17.720356	850.314141	14.216999
18.061358	867.100342	14.222016
18.577660	870.033387	14.227034
18.774596	867.733610	14.232051
18.662518	863.885399	14.237069
18.078753	858.643634	14.242087
17.861226	865.443938	14.247104
18.409103	863.631978	14.252122
18.597981	865.253006	14.257139
18.671698	872.130758	14.262157
18.894516	876.258511	14.267175
18.517856	864.792551	14.272192
18.175813	845.709317	14.277210
18.731758	856.860237	14.282227
18.027898	853.047946	14.287245
18.568803	868.818208	14.292263
18.355569	872.379960	14.297280
18.605239	868.803275	14.302298
18.916660	873.939635	14.307315
18.829728	881.842961	14.312333
18.978817	870.619672	14.317351
18.428658	856.997066	14.322368
19.046056	873.181384	14.327386
18.922860	856.695813	14.332403
18.196015	858.845329	14.337421
18.746901	866.421493	14.342439
18.897047	878.970925	14.347456
18.810270	879.716796	14.352474
18.870355	873.635681	14.357491
18.461629	884.155119	14.362509
18.988420	872.317224	14.367527
19.214784	874.490961	14.372544
18.875769	876.945789	14.377562
18.818935	876.213195	14.382579
18.661748	876.364179	14.387597
19.051398	882.933655	14.392615
18.983914	883.603920	14.397632
18.980982	871.126338	14.402650
18.995785	879.231474	14.407667
18.836120	884.766699	14.412685
19.159629	875.355930	14.417703
18.859330	879.966438	14.422720
18.974729	883.066443	14.427738
19.073418	872.946124	14.432755
18.623935	880.685346	14.437773
18.741568	879.956974	14.442791
18.908720	874.755340	14.447808
18.772876	882.495915	14.452826
18.886301	880.344921	14.457843
18.845121	881.891542	14.462861
19.302068	884.158542	14.467879
19.137751	899.209342	14.472896
19.292565	900.712632	14.477914
19.323911	891.350788	14.482931
19.360439	906.710956	14.487949
19.593031	894.502571	14.492967
19.389780	887.083612	14.497984
19.262175	875.777440	14.503002
19.220889	873.899998	14.508019
18.761760	875.685675	14.513037
19.322402	886.857968	14.518055
19.349414	891.941064	14.523072
19.275091	897.945764	14.528090
19.767256	896.101504	14.533107
19.264136	906.919770	14.538125
19.662845	895.587927	14.543143
19.561306	903.607160	14.548160
19.403443	895.695087	14.553178
19.646734	890.544635	14.558195
19.679433	895.162933	14.563213
19.575065	890.013304	14.568231
19.534596	895.059637	14.573248
19.374596	902.759823	14.578266
19.261630	897.049800	14.583283
19.559028	907.771043	14.588301
19.865885	893.799532	14.593319
19.533643	899.181918	14.598336
19.736920	900.674459	14.603354
19.748510	897.236059	14.608371
19.494956	895.644340	14.613389
19.553737	893.028532	14.618407
19.578051	895.805136	14.623424
19.744048	893.768981	14.628442
19.732360	895.595008	14.633459
19.415625	900.129200	14.638477
19.321733	894.993708	14.643495
19.761239	908.611834	14.648512
19.923121	917.161007	14.653530
20.089998	922.566184	14.658547
20.340232	920.431620	14.663565
20.568467	915.441312	14.668583
19.962652	904.651866	14.673600
20.149585	889.629320	14.678618
20.326290	884.363070	14.683635
20.103292	891.404085	14.688653
20.101500	886.487696	14.693671
19.825329	892.476683	14.698688
19.731505	886.776287	14.703706
20.517321	891.327078	14.708723
19.862164	893.219210	14.713741
19.992134	894.133095	14.718759
20.183963	887.930347	14.723776
20.194374	893.053914	14.728794
20.085249	888.217459	14.733811
20.173777	893.928396	14.738829
19.987482	896.239376	14.743847
20.055093	903.989108	14.748864
19.751256	906.047104	14.753882
19.925357	909.197877	14.758899
20.087040	918.144718	14.763917
20.043328	917.482650	14.768935
20.150912	915.887996	14.773952
19.837419	912.655163	14.778970
20.131255	923.869284	14.783987
20.332929	933.917567	14.789005
20.644950	940.855839	14.794023
20.576655	946.143233	14.799040
20.486288	947.435632	14.804058
20.966623	930.959572	14.809075
20.700444	927.230168	14.814093
20.335715	916.286176	14.819111
20.366979	906.873843	14.824128
20.162283	912.182599	14.829146
20.447649	919.585791	14.834163
20.662944	933.844987	14.839181
20.188252	935.298588	14.844199
20.964107	931.535305	14.849216
20.784274	927.767125	14.854234
20.951638	937.334786	14.859251
20.661140	930.254530	14.864269
20.764645	931.898408	14.869287
20.711756	934.825971	14.874304
20.511037	942.879697	14.879322
20.878013	932.758335	14.884339
20.752989	944.959604	14.889357
20.847812	938.936141	14.894375
20.820274	939.940980	14.899392
20.785334	939.918173	14.904410
21.002406	927.090497	14.909427
20.734853	926.965280	14.914445
20.780182	929.643921	14.919463
21.263367	923.089393	14.924480
20.524320	925.663711	14.929498
21.185030	932.042411	14.934515
20.694450	932.324528	14.939533
20.974282	921.699267	14.944551
21.129736	930.697584	14.949568
21.103922	930.181036	14.954586
21.381827	931.327368	14.959603
21.154758	936.238845	14.964621
21.210818	930.079445	14.969639
21.115424	928.374580	14.974656
20.823478	933.605494	14.979674
21.437889	939.303477	14.984691
21.083292	927.559461	14.989709
21.192821	936.839534	14.994727
21.659869	938.811465	14.999744
21.065925	932.728662	15.004762
21.505429	927.746275	15.009779
21.506033	934.083234	15.014797
20.888680	932.245552	15.019815
21.331019	930.147160	15.024832
21.361312	927.598927	15.029850
21.322076	923.546784	15.034867
21.530808	925.259382	15.039885
20.930060	919.092442	15.044903
21.072088	932.050287	15.049920
21.317154	943.035373	15.054938
21.180777	940.071434	15.059955
21.483910	943.179905	15.064973
21.816055	954.801459	15.069991
21.904660	945.383277	15.075008
21.357445	937.838306	15.080026
21.524674	939.973979	15.085043
21.686557	948.523167	15.090061
21.552328	958.807133	15.095079
21.517552	944.336838	15.100096
21.582628	950.954039	15.105114
21.550700	952.609671	15.110131
21.747431	953.506787	15.115149
21.616370	964.942144	15.120167
21.990982	955.387626	15.125184
21.423832	961.182382	15.130202
21.462835	953.621294	15.135219
21.907069	955.653607	15.140237
21.844674	952.775905	15.145255
21.781529	948.187853	15.150272
21.727130	960.769391	15.155290
22.179545	952.430309	15.160307
22.183058	947.386838	15.165325
21.905202	953.745343	15.170343
22.141972	945.380090	15.175360
21.811245	960.135119	15.180378
21.851346	952.946250	15.185395
21.893760	958.247861	15.190413
22.125364	962.355323	15.195431
21.997901	941.348012	15.200448
22.052828	958.422122	15.205466
22.366910	952.471599	15.210483
22.245302	947.567655	15.215501
21.821878	953.879539	15.220519
21.881440	943.926259	15.225536
21.572481	956.008029	15.230554
21.657477	955.092262	15.235571
22.286267	976.324245	15.240589
22.157764	976.224578	15.245607
22.500998	976.795780	15.250624
22.521883	976.161459	15.255642
22.573010	972.167732	15.260659
22.740938	969.269719	15.265677
22.009791	966.944927	15.270695
22.634382	951.648626	15.275712
22.870128	970.581612	15.280730
22.484657	955.541396	15.285747
22.125479	956.380445	15.290765
22.338112	953.500677	15.295783
22.775964	956.319796	15.300800
22.648694	963.380554	15.305818
22.327202	960.732798	15.310835
22.337588	958.418056	15.315853
22.491196	972.178857	15.320871
22.529595	970.320479	15.325888
22.490905	973.305785	15.330906
22.728336	975.174839	15.335923
22.975087	974.022285	15.340941
22.512436	977.058239	15.345959
22.809709	968.569885	15.350976
22.647541	972.256201	15.355994
22.856679	974.230675	15.361011
22.853971	965.369597	15.366029
22.250991	976.282447	15.371047
22.840576	971.951885	15.376064
22.702928	972.169236	15.381082
22.434150	975.345230	15.386099
22.457988	971.586155	15.391117
22.552971	976.368287	15.396135
23.044321	978.096570	15.401152
22.796519	995.158185	15.406170
23.015733	996.449419	15.411187
23.216672	995.780575	15.416205
22.962976	991.683122	15.421223
23.337406	995.332706	15.426240
23.179296	996.894501	15.431258
23.143628	993.406681	15.436275
22.963252	984.516625	15.441293
22.781003	995.846412	15.446311
23.126800	995.145403	15.451328
23.120133	997.838513	15.456346
22.987861	996.505498	15.461363
23.248109	986.972037	15.466381
23.249458	990.108866	15.471399
23.484261	986.752241	15.476416
23.519910	996.384753	15.481434
23.302881	989.769496	15.486451
23.687274	986.544070	15.491469
23.499891	986.747124	15.496487
23.598878	980.527331	15.501504
23.544506	986.847676	15.506522
23.599896	985.453700	15.511539
23.694522	964.209591	15.516557
23.176507	964.148863	15.521575
23.316536	969.555105	15.526592
23.757451	985.934438	15.531610
23.683443	974.831247	15.536627
23.636474	966.560935	15.541645
23.277363	970.256017	15.546663
23.553815	967.896431	15.551680
23.464582	979.969037	15.556698
23.625174	982.973615	15.561715
23.420695	969.015889	15.566733
23.585801	984.813577	15.571751
23.649032	983.784452	15.576768
23.659525	992.808668	15.581786
23.440292	976.480047	15.586803
24.059192	979.848323	15.591821
23.565539	977.489474	15.596839
23.735958	980.094874	15.601856
23.848446	981.961415	15.606874
23.497066	985.598483	15.611891
23.692144	975.043276	15.616909
23.389341	983.580081	15.621927
24.175186	990.242158	15.626944
23.915387	1000.700459	15.631962
23.856403	1007.046781	15.636979
24.071368	1000.363834	15.641997
24.013949	1006.359610	15.647015
24.100088	995.669978	15.652032
24.464659	999.573576	15.657050
24.194499	1006.792442	15.662067
24.214229	999.269069	15.667085
24.063460	994.918800	15.672103
24.263146	993.975593	15.677120
24.630755	990.519263	15.682138
24.626413	990.062467	15.687155
24.438578	982.180297	15.692173
24.181999	980.421785	15.697191
24.116754	972.545659	15.702208
24.195499	985.630225	15.707226
24.183542	991.202300	15.712243
24.406020	988.750180	15.717261
24.509118	995.490830	15.722279
24.712560	999.874117	15.727296
24.756403	994.616028	15.732314
24.279791	995.397737	15.737331
24.683860	982.565969	15.742349
24.203596	987.015350	15.747367
24.425154	990.253377	15.752384
24.726018	996.625365	15.757402
24.570322	1005.337950	15.762419
24.777670	994.850238	15.767437
24.446064	1006.645252	15.772455
24.364250	1003.451844	15.777472
24.571195	1004.252687	15.782490
24.415822	1003.118954	15.787507
24.477039	1009.752561	15.792525
24.568899	1005.809249	15.797543
24.374650	1003.053186	15.802560
24.477537	1002.298717	15.807578
24.411998	1018.757432	15.812595
25.097739	1021.742852	15.817613
24.921702	1028.988006	15.822631
24.871922	1026.979333	15.827648
25.471514	1030.890296	15.832666
25.242211	1021.218922	15.837683
25.091259	1003.112297	15.842701
24.626893	1000.370154	15.847719
24.683568	1002.822963	15.852736
25.051031	1011.428335	15.857754
24.952647	1009.922749	15.862771
24.956119	1009.669858	15.867789
25.023742	1019.325776	15.872807
25.437989	1016.947749	15.877824
25.659247	1020.573999	15.882842
25.400751	1019.437487	15.887859
25.372012	990.752228	15.892877
25.011397	998.733201	15.897895
25.018172	994.440299	15.902912
25.231006	1004.218626	15.907930
25.226225	1017.903292	15.912947
25.385500	1014.558496	15.917965
25.354210	1022.639361	15.922983
25.652936	1022.592678	15.928000
25.731313	1011.809577	15.933018
25.247842	1008.975750	15.938035
25.237949	1012.988516	15.943053
25.087424	1018.632805	15.948071
25.398476	1018.536852	15.953088
25.487575	1020.328165	15.958106
25.463585	1028.357395	15.963123
25.362736	1019.587407	15.968141
25.146082	1025.696502	15.973159
25.138578	1019.152549	15.978176
25.236371	1026.234875	15.983194
25.164736	1039.696498	15.988211
25.638003	1036.308813	15.993229
25.466515	1040.233293	15.998247
25.774616	1046.468463	16.003264
25.845185	1045.526549	16.008282
25.645165	1046.179715	16.013299
26.210899	1042.929023	16.018317
25.835461	1053.380226	16.023335
25.901615	1042.226630	16.028352
26.014314	1042.388978	16.033370
25.675693	1048.100618	16.038387
25.933597	1037.699635	16.043405
26.228468	1044.937286	16.048423
26.255381	1050.648459	16.053440
26.358045	1042.427252	16.058458
26.195834	1038.277584	16.063475
26.096239	1037.911451	16.068493
25.991843	1039.228145	16.073511
25.936460	1040.723355	16.078528
26.451314	1030.976406	16.083546
25.992302	1033.563667	16.088563
26.253234	1029.518119	16.093581
26.066720	1039.529452	16.098599
26.084596	1032.290384	16.103616
26.199165	1041.979984	16.108634
26.586047	1047.694718	16.113651
26.282650	1041.364378	16.118669
26.634510	1037.749558	16.123687
26.259107	1040.642462	16.128704
26.858431	1028.622683	16.133722
26.528119	1047.237335	16.138739
26.162746	1030.070012	16.143757
26.507548	1027.519825	16.148775
26.382092	1042.501540	16.153792
26.897934	1030.352826	16.158810
26.741452	1043.628927	16.163827
26.734513	1026.541149	16.168845
26.873123	1027.942846	16.173863
26.855018	1036.397199	16.178880
26.650817	1027.652867	16.183898
26.367815	1038.941662	16.188915
26.563362	1036.440106	16.193933
26.733761	1037.164624	16.198951
26.186317	1046.096402	16.203968
26.639159	1029.864405	16.208986
26.778868	1040.193861	16.214003
26.660644	1034.292111	16.219021
27.022390	1043.213980	16.224039
27.012049	1044.055181	16.229056
26.957072	1042.170400	16.234074
26.764692	1038.240057	16.239091
26.492612	1046.724741	16.244109
26.986577	1049.232119	16.249127
27.041421	1056.633617	16.254144
27.119984	1057.675488	16.259162
27.271600	1061.520946	16.264179
27.139698	1059.013886	16.269197
27.459789	1055.609171	16.274215
27.484840	1056.485854	16.279232
27.487034	1048.946273	16.284250
27.086096	1044.496330	16.289267
27.223905	1041.296907	16.294285
26.937731	1041.168294	16.299303
26.967709	1049.735042	16.304320
27.367412	1044.361221	16.309338
27.179048	1053.792173	16.314355
27.276185	1052.347469	16.319373
27.585757	1046.659558	16.324391
27.111931	1047.847940	16.329408
27.397420	1040.904615	16.334426
27.341359	1050.172822	16.339443
27.390470	1042.938323	16.344461
27.696399	1045.822308	16.349479
27.276946	1051.657068	16.354496
27.300018	1048.147411	16.359514
27.506552	1048.919918	16.364531
27.354072	1059.326724	16.369549
28.062281	1060.613931	16.374567
27.679320	1077.759920	16.379584
27.615582	1066.440464	16.384602
27.815608	1075.734833	16.389619
28.179244	1071.894095	16.394637
28.210240	1060.881698	16.399655
27.983837	1052.891929	16.404672
27.948586	1041.293465	16.409690
28.132096	1046.181668	16.414707
27.777235	1035.583200	16.419725
27.773422	1041.128768	16.424743
27.727156	1037.011428	16.429760
27.790892	1038.611053	16.434778
27.823912	1054.786111	16.439795
27.829130	1066.872380	16.444813
27.875688	1073.303176	16.449831
27.817850	1082.060427	16.454848
27.794636	1071.634041	16.459866
27.938341	1070.551276	16.464883
27.871433	1070.063254	16.469901
28.119497	1065.227592	16.474919
28.139441	1074.177784	16.479936
28.133820	1080.771395	16.484954
28.055248	1089.061674	16.489971
28.321781	1086.015647	16.494989
28.849029	1090.215675	16.500007
28.571590	1091.228119	16.505024
28.588506	1087.621586	16.510042
28.244209	1081.139847	16.515059
28.290510	1083.376537	16.520077
28.782678	1083.069167	16.525095
28.562862	1085.439074	16.530112
28.700273	1070.626110	16.535130
28.313546	1076.689285	16.540147
28.183554	1083.838882	16.545165
28.908261	1082.945956	16.550183
28.774011	1088.341559	16.555200
28.700225	1079.785056	16.560218
28.767454	1092.798920	16.565235
28.633770	1088.502756	16.570253
28.582466	1089.968928	16.575271
28.641413	1078.895335	16.580288
29.058919	1078.359817	16.585306
29.021556	1089.600689	16.590323
28.961307	1093.977976	16.595341
29.294010	1087.822516	16.600359
28.929377	1089.489263	16.605376
28.846977	1089.388684	16.610394
29.191069	1093.188211	16.615411
28.855701	1089.172961	16.620429
28.843365	1076.674617	16.625447
28.686933	1089.849757	16.630464
28.789128	1084.064936	16.635482
28.906852	1079.530564	16.640499
28.858760	1084.628638	16.645517
29.076978	1078.084012	16.650535
29.130446	1092.302417	16.655552
29.021838	1087.065031	16.660570
28.834144	1094.725457	16.665587
29.261158	1114.326076	16.670605
29.900993	1102.820619	16.675623
29.445504	1110.541945	16.680640
29.256394	1110.335006	16.685658
29.639298	1107.545303	16.690675
29.412268	1115.568515	16.695693
29.399295	1109.265232	16.700711
29.681101	1106.914256	16.705728
29.591136	1105.681904	16.710746
29.458086	1103.755698	16.715763
29.562615	1097.156292	16.720781
29.848089	1098.165747	16.725799
29.471611	1101.055674	16.730816
29.736884	1095.611379	16.735834
29.687203	1103.887671	16.740851
29.787812	1102.773785	16.745869
29.726447	1090.983717	16.750887
29.898814	1101.472197	16.755904
29.914996	1098.478016	16.760922
30.042765	1102.526039	16.765939
29.867183	1108.423595	16.770957
29.706141	1093.802545	16.775975
29.569182	1103.758811	16.780992
30.116559	1100.015513	16.786010
30.066578	1093.913698	16.791027
29.532680	1101.196015	16.796045
29.827113	1095.841828	16.801063
29.882214	1102.088256	16.806080
30.024736	1106.582102	16.811098
29.747591	1106.789752	16.816115
29.981830	1115.274034	16.821133
30.191108	1114.199927	16.826151
29.936848	1121.268022	16.831168
30.239484	1125.610551	16.836186
30.183029	1121.545281	16.841203
30.221594	1126.847545	16.846221
30.006352	1117.925014	16.851239
30.302014	1129.369358	16.856256
30.470715	1117.451705	16.861274
30.883408	1119.488979	16.866291
30.503340	1120.997197	16.871309
30.812024	1116.025788	16.876327
30.506558	1115.960159	16.881344
30.584260	1118.084634	16.886362
31.058954	1110.373163	16.891379
31.040940	1116.719416	16.896397
30.914623	1120.794630	16.901415
30.831279	1114.877920	16.906432
30.827392	1114.793442	16.911450
31.023662	1086.464103	16.916467
30.392383	1093.162060	16.921485
30.828119	1097.038749	16.926503
30.471840	1101.891620	16.931520
30.664365	1112.929226	16.936538
31.075656	1106.644678	16.941555
30.681881	1111.604413	16.946573
30.926252	1107.315285	16.951591
30.949962	1108.949590	16.956608
30.989895	1116.220902	16.961626
31.454081	1110.698099	16.966643
31.052962	1112.585164	16.971661
31.454095	1109.287665	16.976679
30.923685	1108.304207	16.981696
31.039828	1113.565909	16.986714
31.432820	1111.787661	16.991731
31.183160	1112.862026	16.996749
31.645085	1111.006704	17.001767
30.782995	1116.323846	17.006784
30.844910	1119.640559	17.011802
31.294739	1111.166106	17.016819
30.931370	1113.722614	17.021837
30.920435	1107.620988	17.026855
30.864638	1118.072642	17.031872
30.929086	1134.511097	17.036890
31.511689	1137.989235	17.041907
31.259441	1146.379338	17.046925
31.367802	1137.466056	17.051943
31.532912	1145.140655	17.056960
31.707851	1152.842120	17.061978
31.671200	1148.107851	17.066995
31.512309	1143.301215	17.072013
31.570150	1135.724475	17.077031
31.526884	1145.505135	17.082048
31.930712	1143.879824	17.087066
31.692748	1150.872792	17.092083
31.705467	1158.015838	17.097101
31.974702	1167.760170	17.102119
32.164631	1166.234645	17.107136
31.910463	1154.714590	17.112154
32.244866	1155.009465	17.117171
31.813391	1143.788603	17.122189
31.981199	1152.914488	17.127207
32.229747	1164.666045	17.132224
32.003733	1157.600842	17.137242
32.118700	1158.797965	17.142259
32.332983	1165.265633	17.147277
32.296490	1160.641791	17.152295
31.951572	1151.111541	17.157312
32.105401	1155.887657	17.162330
32.262604	1152.205481	17.167347
32.278093	1163.434962	17.172365
32.577989	1154.008813	17.177383
32.452234	1164.660807	17.182400
32.250652	1166.712279	17.187418
33.028353	1157.425865	17.192435
32.335485	1162.337800	17.197453
32.780252	1156.076393	17.202471
32.904967	1149.975590	17.207488
32.237926	1132.546156	17.212506
32.491769	1136.489225	17.217523
32.269354	1153.035761	17.222541
32.345210	1147.299229	17.227559
32.392451	1161.136803	17.232576
32.381519	1162.946959	17.237594
32.335367	1160.953482	17.242611
32.578468	1155.143405	17.247629
32.751256	1144.683111	17.252647
32.650813	1154.349655	17.257664
32.469215	1157.085977	17.262682
32.834062	1161.750135	17.267699
32.641388	1179.150436	17.272717
33.064782	1170.705344	17.277735
32.880550	1177.424808	17.282752
32.719399	1184.412066	17.287770
32.950342	1182.592927	17.292787
32.543114	1187.917718	17.297805
32.790674	1177.041736	17.302823
33.016868	1184.078760	17.307840
33.604570	1194.489596	17.312858
33.394386	1185.499965	17.317875
32.700733	1185.561430	17.322893
33.361614	1188.897923	17.327911
33.534439	1203.826727	17.332928
33.415974	1213.376202	17.337946
33.791105	1193.413346	17.342963
33.126003	1186.221262	17.347981
33.347099	1185.053779	17.352999
33.728601	1197.280001	17.358016
33.497257	1196.805116	17.363034
33.742730	1193.743435	17.368051
33.778239	1199.166123	17.373069
33.639418	1194.867583	17.378087
33.654386	1182.320704	17.383104
33.697599	1178.539615	17.388122
33.825819	1191.960572	17.393139
33.876388	1196.361548	17.398157
33.890232	1191.411067	17.403175
33.715080	1174.620909	17.408192
33.946970	1187.811020	17.413210
33.852986	1191.833845	17.418227
33.926981	1194.956171	17.423245
33.713096	1192.941633	17.428263
34.096584	1190.925019	17.433280
33.596120	1188.658729	17.438298
34.234807	1187.179658	17.443315
33.912059	1184.008186	17.448333
33.970867	1187.123423	17.453351
33.977718	1192.307596	17.458368
33.951805	1189.847029	17.463386
34.011442	1190.232293	17.468403
34.125043	1192.452141	17.473421
33.897275	1198.304253	17.478439
34.362036	1204.697976	17.483456
34.581954	1212.095765	17.488474
34.647046	1209.702990	17.493491
34.445106	1198.130541	17.498509
34.420320	1191.702844	17.503527
34.497415	1198.040536	17.508544
34.417985	1198.416031	17.513562
34.639193	1204.301944	17.518579
34.545593	1208.839123	17.523597
34.647590	1207.949082	17.528615
34.362567	1211.916635	17.533632
34.237818	1210.926417	17.538650
34.527629	1205.415127	17.543667
34.682331	1209.092871	17.548685
34.908585	1208.738798	17.553703
34.748219	1204.951729	17.558720
34.710333	1213.598619	17.563738
35.053810	1211.373671	17.568755
34.978837	1208.182309	17.573773
34.780906	1210.201655	17.578791
35.204185	1207.560250	17.583808
34.750925	1202.881772	17.588826
34.866121	1201.484721	17.593843
35.096439	1204.557309	17.598861
34.755101	1207.113533	17.603879
34.880997	1206.996097	17.608896
35.141490	1231.880652	17.613914
35.033398	1224.961052	17.618931
35.420508	1231.540525	17.623949
35.176853	1237.070082	17.628967
35.503848	1231.010144	17.633984
35.567260	1224.275118	17.639002
35.717302	1217.160438	17.644019
35.835360	1230.794462	17.649037
35.774321	1210.432853	17.654055
35.397813	1203.946647	17.659072
35.417264	1207.039651	17.664090
35.829290	1210.430918	17.669107
35.495864	1206.573131	17.674125
35.745295	1210.576869	17.679143
35.878295	1196.253656	17.684160
35.628831	1203.128522	17.689178
35.675918	1204.225828	17.694195
36.036544	1216.060847	17.699213
35.891734	1214.537271	17.704231
35.968366	1197.625588	17.709248
35.986167	1208.296143	17.714266
35.792715	1213.338132	17.719283
36.077005	1210.099948	17.724301
36.026879	1216.053625	17.729319
36.098182	1221.139343	17.734336
35.727401	1231.867640	17.739354
36.167155	1223.025473	17.744371
36.126238	1219.333298	17.749389
35.880382	1224.553918	17.754407
36.027423	1223.656819	17.759424
36.235495	1219.445937	17.764442
36.182575	1219.861460	17.769459
36.047321	1225.115246	17.774477
35.868386	1231.291087	17.779495
36.284450	1225.753698	17.784512
35.930808	1234.083986	17.789530
36.512092	1238.518588	17.794547
36.319934	1251.882487	17.799565
36.404577	1246.548501	17.804583
36.493938	1240.765641	17.809600
36.360201	1253.041070	17.814618
36.700573	1237.776434	17.819635
36.456615	1244.978666	17.824653
36.497420	1246.443043	17.829671
36.458237	1244.631507	17.834688
36.246268	1254.183031	17.839706
36.187529	1261.529824	17.844723
36.783346	1266.640675	17.849741
36.726760	1268.824079	17.854759
36.743550	1269.964007	17.859776
36.752048	1267.147733	17.864794
36.913544	1269.650429	17.869811
37.331345	1264.920667	17.874829
36.809646	1262.742903	17.879847
36.966583	1264.520455	17.884864
37.135559	1264.045964	17.889882
36.926338	1264.249286	17.894899
37.508734	1269.248627	17.899917
37.017221	1279.443585	17.904935
37.208813	1264.760832	17.909952
37.172150	1286.580303	17.914970
37.401402	1282.804758	17.919987
37.837080	1284.046318	17.925005
37.635487	1283.970725	17.930023
37.994760	1262.574339	17.935040
37.702930	1260.887595	17.940058
37.730561	1255.537293	17.945075
37.764270	1247.232118	17.950093
37.537051	1260.749844	17.955111
37.843960	1254.431105	17.960128
37.911786	1255.130678	17.965146
38.191383	1254.010830	17.970163
38.183721	1248.423055	17.975181
37.746497	1249.959174	17.980199
37.881529	1246.551860	17.985216
38.190391	1244.243966	17.990234
37.904300	1254.188968	17.995251
38.275265	1252.843360	18.000269
37.913510	1246.582052	18.005287
38.176064	1244.672745	18.010304
38.185280	1248.335421	18.015322
38.294103	1246.636398	18.020339
38.319379	1238.935325	18.025357
38.123757	1253.019312	18.030375
38.147418	1238.706884	18.035392
38.566879	1240.932466	18.040410
37.939895	1252.044909	18.045427
37.876220	1247.008726	18.050445
38.006123	1247.654389	18.055463
38.090329	1240.628912	18.060480
38.285485	1250.485886	18.065498
38.106289	1243.271297	18.070515
38.366625	1245.370328	18.075533
38.325045	1266.111228	18.080551
38.630909	1265.735214	18.085568
38.434607	1276.044867	18.090586
38.207257	1279.981307	18.095603
38.728166	1265.246956	18.100621
38.559049	1281.523320	18.105639
38.595240	1275.527866	18.110656
38.519880	1277.385999	18.115674
38.561788	1275.148330	18.120691
39.069859	1291.227081	18.125709
38.918148	1296.868487	18.130727
39.175220	1293.943831	18.135744
39.279348	1294.359998	18.140762
38.678553	1289.250163	18.145779
39.377755	1287.449168	18.150797
39.399243	1294.811808	18.155815
39.285447	1271.482376	18.160832
39.116795	1270.350705	18.165850
38.995480	1272.329651	18.170867
39.616509	1276.672826	18.175885
39.472121	1288.422912	18.180903
39.583125	1273.162624	18.185920
39.452866	1271.204403	18.190938
39.149805	1270.794403	18.195955
39.200368	1283.126186	18.200973
39.491951	1288.635016	18.205991
39.619572	1289.994273	18.211008
39.822115	1291.714189	18.216026
39.239749	1291.893921	18.221043
39.846315	1287.292372	18.226061
39.540490	1298.401864	18.231079
39.673626	1298.573636	18.236096
40.041831	1285.851415	18.241114
39.485615	1290.644140	18.246131
39.833263	1285.657112	18.251149
39.563165	1285.434457	18.256167
39.926441	1286.636867	18.261184
40.127392	1292.181989	18.266202
39.697299	1296.778225	18.271219
40.009570	1293.649255	18.276237
39.850049	1299.932534	18.281255
39.691877	1294.743880	18.286272
39.890151	1301.150987	18.291290
40.095808	1311.192548	18.296307
40.073767	1307.617322	18.301325
39.983296	1316.162043	18.306343
40.302188	1314.341735	18.311360
40.488202	1314.243283	18.316378
40.508140	1314.435947	18.321395
40.236321	1310.593732	18.326413
40.167792	1312.911561	18.331431
40.191999	1308.846235	18.336448
40.488965	1315.360965	18.341466
40.094695	1318.061202	18.346483
40.623055	1323.526633	18.351501
40.355258	1331.537393	18.356519
40.760246	1327.630159	18.361536
40.599124	1321.921233	18.366554
40.443469	1331.596523	18.371571
40.690442	1331.542170	18.376589
40.720934	1331.597477	18.381607
40.669624	1328.575961	18.386624
41.107646	1338.410711	18.391642
40.728751	1340.313253	18.396659
41.119996	1340.785424	18.401677
41.115147	1342.837650	18.406695
41.474040	1339.972777	18.411712
41.255990	1342.206735	18.416730
41.363606	1344.635830	18.421747
41.492676	1331.117883	18.426765
41.535138	1318.358311	18.431783
41.418563	1316.202275	18.436800
41.694511	1311.264345	18.441818
41.571104	1316.996000	18.446835
41.788739	1305.865843	18.451853
41.590026	1316.497801	18.456871
41.362716	1317.565520	18.461888
41.340423	1313.210822	18.466906
41.312785	1314.411365	18.471923
41.363029	1316.470736	18.476941
42.000805	1336.975884	18.481959
41.704961	1347.159159	18.486976
41.918831	1333.290240	18.491994
41.867794	1339.562848	18.497011
41.957727	1339.059713	18.502029
41.932481	1339.114285	18.507047
41.836678	1342.058106	18.512064
42.263705	1337.942283	18.517082
42.139039	1333.351147	18.522099
42.358767	1336.867245	18.527117
42.196958	1338.521171	18.532135
42.205929	1333.688183	18.537152
42.203870	1331.018724	18.542170
42.278033	1333.383629	18.547187
42.124096	1330.633822	18.552205
42.320529	1338.158425	18.557223
42.369915	1330.595551	18.562240
42.464008	1337.820597	18.567258
42.129113	1335.809222	18.572275
42.601492	1330.856289	18.577293
42.387741	1331.120283	18.582311
42.119489	1335.116794	18.587328
42.328180	1328.611440	18.592346
42.176695	1326.306233	18.597363
42.266878	1331.079745	18.602381
42.433651	1340.796044	18.607399
42.881968	1353.586282	18.612416
43.365156	1354.836184	18.617434
43.162024	1348.196524	18.622451
42.850677	1329.041686	18.627469
43.110459	1331.405911	18.632487
42.836540	1333.894784	18.637504
43.127120	1348.268754	18.642522
43.033513	1347.033799	18.647539
42.969675	1345.958288	18.652557
42.832376	1358.073396	18.657575
42.883502	1357.301775	18.662592
42.972248	1352.752939	18.667610
43.055522	1358.079826	18.672627
42.558212	1352.240521	18.677645
43.302298	1354.418411	18.682663
43.216568	1372.947743	18.687680
43.459520	1374.951680	18.692698
43.470760	1376.922492	18.697715
43.676367	1381.081463	18.702733
43.688921	1371.009073	18.707751
43.795707	1378.951697	18.712768
43.792862	1373.574575	18.717786
43.598121	1376.256182	18.722803
43.680336	1372.576242	18.727821
43.587520	1371.255952	18.732839
43.426290	1376.457046	18.737856
44.008883	1371.685657	18.742874
43.722764	1378.673634	18.747891
43.866128	1375.940357	18.752909
44.054313	1369.154168	18.757927
43.801845	1375.171160	18.762944
43.638881	1373.997565	18.767962
44.022621	1386.494976	18.772979
43.891059	1392.057513	18.777997
44.554495	1398.918814	18.783015
44.032074	1398.145533	18.788032
44.137850	1394.843764	18.793050
44.222448	1396.026727	18.798067
44.073849	1397.148393	18.803085
44.477107	1399.711062	18.808103
44.116852	1391.495950	18.813120
44.411665	1393.769485	18.818138
44.582642	1400.215620	18.823155
44.526916	1412.015015	18.828173
45.178030	1414.639842	18.833191
44.990577	1408.521587	18.838208
45.019672	1388.903075	18.843226
44.733956	1400.003166	18.848243
44.862497	1381.770312	18.853261
44.656197	1382.749533	18.858279
45.082013	1394.546055	18.863296
45.334019	1398.988106	18.868314
44.809485	1401.367925	18.873331
45.009521	1399.553608	18.878349
45.351306	1405.455411	18.883367
45.166552	1408.274319	18.888384
45.451090	1404.354382	18.893402
44.963938	1400.867790	18.898419
45.399947	1405.120061	18.903437
45.241928	1398.760503	18.908455
45.621903	1407.241027	18.913472
45.714441	1407.949357	18.918490
45.544489	1391.861952	18.923507
45.229231	1385.656427	18.928525
45.250687	1386.025586	18.933543
45.066816	1398.419428	18.938560
45.459585	1401.207812	18.943578
45.421339	1402.012375	18.948595
45.235601	1398.027261	18.953613
45.549195	1397.618474	18.958631
45.600566	1400.207873	18.963648
45.698051	1404.718319	18.968666
45.962845	1424.666602	18.973683
45.845062	1430.485778	18.978701
46.345148	1422.558748	18.983719
46.260718	1426.504387	18.988736
46.392920	1416.571022	18.993754
46.106536	1422.583876	18.998771
46.003740	1420.681299	19.003789
46.384158	1428.918757	19.008807
46.078837	1433.220911	19.013824
46.009904	1425.644976	19.018842
46.237493	1425.429551	19.023859
46.005501	1415.950895	19.028877
46.264481	1413.079573	19.033895
46.227600	1428.912458	19.038912
46.347734	1421.076519	19.043930
46.233093	1436.871100	19.048947
46.600645	1450.302093	19.053965
46.817957	1446.462110	19.058983
46.513526	1451.764560	19.064000
46.896490	1449.350352	19.069018
47.018295	1451.010347	19.074035
46.452253	1453.803792	19.079053
47.153114	1444.674443	19.084071
46.889157	1452.905571	19.089088
47.438761	1442.237735	19.094106
47.650443	1450.088213	19.099123
47.036682	1451.386909	19.104141
47.176799	1448.733029	19.109159
47.296162	1446.719899	19.114176
46.977159	1445.002679	19.119194
47.461960	1438.981065	19.124211
47.237070	1442.898219	19.129229
47.206197	1435.802330	19.134247
47.084658	1436.291729	19.139264
46.927383	1441.280774	19.144282
47.417777	1436.268183	19.149299
47.409417	1451.762091	19.154317
47.831209	1464.559721	19.159335
47.573618	1466.048778	19.164352
47.640428	1466.647528	19.169370
47.868781	1471.112238	19.174387
47.765420	1476.114938	19.179405
47.680563	1471.713197	19.184423
47.655547	1473.658140	19.189440
47.561194	1467.064511	19.194458
48.131649	1464.340047	19.199475
47.498399	1467.380719	19.204493
47.935454	1460.135764	19.209511
48.007723	1465.009952	19.214528
48.155482	1481.524041	19.219546
48.414937	1487.123177	19.224563
48.560313	1487.220447	19.229581
48.652693	1470.274480	19.234599
48.169593	1470.224056	19.239616
48.355664	1474.307212	19.244634
48.414970	1481.569326	19.249651
48.325902	1487.728019	19.254669
48.443189	1481.735569	19.259687
48.452958	1483.012317	19.264704
48.361915	1483.276022	19.269722
48.319946	1484.036989	19.274739
48.236061	1485.820737	19.279757
48.048535	1493.534957	19.284775
48.649443	1501.589574	19.289792
48.562436	1514.965597	19.294810
49.421471	1504.476471	19.299827
49.429699	1502.843681	19.304845
49.343132	1506.565600	19.309863
49.167594	1512.557961	19.314880
49.095761	1504.786778	19.319898
49.377237	1503.149047	19.324915
49.135349	1508.747841	19.329933
49.117772	1503.518161	19.334951
49.531012	1509.033247	19.339968
49.295354	1501.956793	19.344986
49.643020	1505.314018	19.350003
49.375066	1500.776849	19.355021
49.636513	1503.036690	19.360039
49.736981	1499.659991	19.365056
49.310025	1509.280050	19.370074
49.759486	1502.481278	19.375091
49.763021	1507.880666	19.380109
49.993479	1503.432670	19.385127
49.717711	1508.317218	19.390144
49.718693	1512.615583	19.395162
49.892697	1503.177415	19.400179
49.792741	1505.004710	19.405197
50.040550	1502.444406	19.410215
49.874719	1501.002997	19.415232
49.861060	1492.645166	19.420250
50.220262	1496.041610	19.425267
49.735577	1496.799355	19.430285
50.064001	1519.382455	19.435303
50.101159	1528.361737	19.440320
50.189093	1527.584342	19.445338
50.430010	1534.745436	19.450355
50.132907	1524.737256	19.455373
50.452003	1521.045419	19.460391
50.432120	1519.571673	19.465408
50.225086	1520.936042	19.470426
50.495253	1528.654310	19.475443
50.510013	1541.559952	19.480461
50.891807	1552.198930	19.485479
50.819497	1546.450770	19.490496
50.925946	1549.085212	19.495514
51.240173	1546.145250	19.500531
51.306228	1549.540294	19.505549
51.055018	1544.249373	19.510567
51.166599	1538.759595	19.515584
51.040154	1547.344778	19.520602
51.451609	1545.525725	19.525619
51.228108	1549.650978	19.530637
51.509791	1531.772690	19.535655
51.257931	1540.620529	19.540672
51.241696	1539.553327	19.545690
51.314096	1534.110716	19.550707
51.404464	1542.589340	19.555725
51.267764	1530.599336	19.560743
51.486317	1531.136442	19.565760
51.490956	1540.531099	19.570778
51.687590	1537.404425	19.575795
51.479610	1542.369883	19.580813
51.581815	1535.518204	19.585831
51.216335	1538.797813	19.590848
51.441644	1550.430185	19.595866
51.679885	1554.599864	19.600883
51.520467	1559.160068	19.605901
51.885202	1567.759827	19.610919
52.325518	1566.422267	19.615936
51.953162	1561.197661	19.620954
52.354476	1556.126408	19.625971
51.724473	1560.350068	19.630989
52.068749	1574.346562	19.636007
52.118256	1578.741486	19.641024
52.279668	1581.651359	19.646042
52.473861	1584.477196	19.651059
52.543318	1591.554719	19.656077
52.747987	1584.339812	19.661095
52.626281	1580.877981	19.666112
52.522804	1584.608878	19.671130
52.794091	1578.753221	19.676147
52.874823	1582.111256	19.681165
52.748057	1586.843085	19.686183
52.810975	1576.185148	19.691200
52.627323	1580.853301	19.696218
52.434245	1577.838176	19.701235
52.783632	1583.113968	19.706253
52.379948	1582.126405	19.711271
52.973123	1585.344189	19.716288
53.366580	1594.065698	19.721306
53.382831	1599.068627	19.726323
53.249153	1601.788040	19.731341
52.994082	1595.225856	19.736359
53.614202	1600.194135	19.741376
53.329479	1605.645029	19.746394
53.503045	1593.237123	19.751411
53.603600	1598.889594	19.756429
53.404130	1601.168013	19.761447
53.338143	1592.827802	19.766464
53.525366	1603.604599	19.771482
53.537301	1596.053793	19.776499
53.540028	1617.192121	19.781517
53.601414	1617.943212	19.786535
53.658175	1615.535908	19.791552
53.759330	1628.762609	19.796570
54.144824	1614.894987	19.801587
53.819507	1619.364428	19.806605
54.202229	1627.304957	19.811623
54.195599	1608.739582	19.816640
54.343160	1617.528033	19.821658
54.438210	1615.575501	19.826675
54.228769	1623.457321	19.831693
54.044315	1614.962083	19.836711
54.325138	1627.911312	19.841728
54.415073	1637.257940	19.846746
54.702984	1635.391960	19.851763
55.037966	1642.096524	19.856781
54.864758	1640.208111	19.861799
54.787145	1632.223172	19.866816
54.813143	1629.501934	19.871834
55.182361	1626.363985	19.876851
54.907872	1619.047403	19.881869
55.108661	1623.664802	19.886887
55.277534	1611.443820	19.891904
54.836389	1611.115408	19.896922
55.563548	1611.291949	19.901939
54.979288	1602.752055	19.906957
54.832598	1617.371487	19.911975
55.446517	1615.495458	19.916992
55.356367	1628.518591	19.922010
55.390531	1618.237538	19.927027
55.597405	1622.027120	19.932045
55.206719	1619.424820	19.937063
55.441853	1624.683810	19.942080
55.293343	1626.894285	19.947098
55.589561	1630.029209	19.952115
55.313941	1629.466569	19.957133
55.403378	1628.897228	19.962151
55.800102	1627.456035	19.967168
55.410757	1626.665048	19.972186
55.660591	1635.049300	19.977203
55.314349	1641.563936	19.982221
55.355856	1639.919607	19.987239
55.619439	1644.558733	19.992256
55.988858	1649.152873	19.997274
56.054125	1665.897819	20.002291
56.117268	1676.832963	20.007309
56.328284	1684.964531	20.012327
56.450410	1668.449241	20.017344
56.388896	1672.558610	20.022362
56.670418	1665.502051	20.027379
56.520338	1669.779939	20.032397
56.714967	1668.745967	20.037415
56.891761	1672.142620	20.042432
56.696429	1667.635057	20.047450
56.974732	1673.651044	20.052467
57.005746	1675.233761	20.057485
56.927588	1664.913472	20.062503
57.042074	1666.031807	20.067520
56.744667	1673.946367	20.072538
56.625049	1667.587008	20.077555
57.188384	1674.874378	20.082573
57.075301	1668.498215	20.087591
57.161490	1666.294588	20.092608
57.030469	1662.411300	20.097626
56.992593	1671.030006	20.102643
57.037067	1669.445173	20.107661
57.376755	1692.424379	20.112679
57.346796	1685.422927	20.117696
57.255800	1691.364230	20.122714
57.659910	1689.281212	20.127731
57.765294	1689.772934	20.132749
57.413485	1696.073856	20.137767
57.683486	1687.024516	20.142784
57.516108	1693.586890	20.147802
57.491362	1688.355124	20.152819
57.832916	1696.690319	20.157837
57.817966	1705.248641	20.162855
58.121962	1713.163671	20.167872
58.139717	1710.238573	20.172890
58.416321	1706.815303	20.177907
58.507906	1710.941721	20.182925
57.933538	1713.629206	20.187943
58.511897	1711.206442	20.192960
58.207486	1708.729474	20.197978
58.592087	1706.081434	20.202995
58.449516	1715.025850	20.208013
58.033090	1718.528080	20.213031
58.326728	1715.275719	20.218048
58.507659	1716.389958	20.223066
58.823633	1735.017681	20.228083
58.715205	1739.869760	20.233101
58.411810	1741.138784	20.238119
58.952122	1733.069609	20.243136
59.145861	1737.886968	20.248154
59.207235	1729.892834	20.253171
59.267293	1733.090026	20.258189
58.727026	1738.401106	20.263207
59.299296	1723.980243	20.268224
59.238414	1729.822161	20.273242
59.554156	1736.289920	20.278259
59.603035	1731.460040	20.283277
59.522510	1734.859149	20.288295
59.340371	1724.504622	20.293312
59.490444	1724.853637	20.298330
59.171111	1719.904715	20.303347
59.220170	1718.565326	20.308365
59.274040	1724.938403	20.313383
60.016576	1739.974067	20.318400
59.388001	1752.204284	20.323418
59.700069	1756.390848	20.328435
60.101754	1754.033632	20.333453
60.049878	1755.342148	20.338471
60.318087	1751.598274	20.343488
60.138722	1746.179265	20.348506
60.133748	1755.755432	20.353523
60.374598	1745.956349	20.358541
60.105009	1756.214641	20.363559
60.569691	1751.549995	20.368576
60.466870	1741.334518	20.373594
60.450818	1739.901181	20.378611
60.475638	1743.602542	20.383629
60.105295	1748.227400	20.388647
60.307777	1755.460881	20.393664
60.362195	1765.232887	20.398682
60.694674	1765.834207	20.403699
60.461400	1767.231110	20.408717
60.827445	1777.307768	20.413735
60.970727	1767.489244	20.418752
60.782059	1774.468418	20.423770
60.904446	1778.406979	20.428787
61.163171	1781.434189	20.433805
61.446324	1800.231234	20.438823
61.725388	1790.400891	20.443840
61.760974	1789.047828	20.448858
61.323018	1776.748231	20.453875
61.493202	1765.767244	20.458893
61.422447	1778.512876	20.463911
61.598057	1777.652302	20.468928
61.515024	1786.921961	20.473946
61.400907	1800.154113	20.478963
61.579740	1785.996826	20.483981
61.738384	1786.969387	20.488999
61.729992	1778.774709	20.494016
61.626366	1787.716216	20.499034
61.686628	1785.156853	20.504051
62.031906	1804.461752	20.509069
62.030680	1821.523393	20.514087
62.248098	1814.082320	20.519104
62.010915	1818.585342	20.524122
62.178622	1815.125461	20.529139
62.561596	1810.183250	20.534157
62.646961	1816.267386	20.539175
62.357623	1812.093270	20.544192
62.525699	1801.904747	20.549210
62.678959	1802.732976	20.554227
63.057025	1802.686487	20.559245
62.891064	1797.631458	20.564263
62.993315	1799.259833	20.569280
63.194378	1798.638282	20.574298
63.222731	1797.627199	20.579315
63.324981	1797.118965	20.584333
63.237145	1808.289297	20.589351
63.385460	1800.177361	20.594368
63.353162	1798.279478	20.599386
63.265921	1798.416352	20.604403
63.315573	1793.753601	20.609421
63.149035	1794.344739	20.614439
63.600339	1791.840880	20.619456
63.572724	1797.481935	20.624474
63.378196	1787.075661	20.629491
63.287123	1790.596361	20.634509
63.371050	1792.281259	20.639527
63.177327	1796.098927	20.644544
63.682518	1803.729995	20.649562
63.448223	1824.921484	20.654579
63.538936	1810.680149	20.659597
63.816663	1821.506018	20.664615
63.846274	1823.543432	20.669632
63.862228	1827.429247	20.674650
63.989801	1838.546912	20.679667
64.146357	1845.623513	20.684685
64.252244	1850.467292	20.689703
64.358960	1842.525967	20.694720
64.073486	1830.830487	20.699738
64.180375	1850.147537	20.704755
64.548916	1840.483041	20.709773
64.592268	1841.786112	20.714791
64.570941	1835.922566	20.719808
64.769943	1849.055199	20.724826
64.455057	1870.505538	20.729843
64.647549	1872.691018	20.734861
64.572835	1872.380933	20.739879
64.874693	1871.967664	20.744896
65.080366	1864.698835	20.749914
65.043984	1870.754724	20.754931
65.218163	1862.916437	20.759949
64.843919	1869.334550	20.764967
64.721457	1875.927825	20.769984
64.976763	1880.669301	20.775002
65.583520	1887.615419	20.780019
65.995439	1881.933303	20.785037
65.973564	1882.299793	20.790055
65.756788	1881.074631	20.795072
66.219311	1883.321954	20.800090
65.890478	1883.228420	20.805107
65.836045	1874.453894	20.810125
65.729139	1875.187180	20.815143
65.727067	1876.178613	20.820160
65.588823	1876.029970	20.825178
65.741127	1883.482818	20.830195
66.591941	1899.214910	20.835213
66.248017	1907.689163	20.840231
66.766885	1903.817616	20.845248
66.911803	1902.933441	20.850266
66.542216	1899.387301	20.855283
66.510347	1894.491127	20.860301
66.756013	1903.109704	20.865319
66.449198	1903.060060	20.870336
66.841952	1895.266413	20.875354
66.624449	1902.982350	20.880371
66.998493	1902.863903	20.885389
66.698562	1899.960145	20.890407
66.845631	1899.694211	20.895424
67.121633	1901.352181	20.900442
66.829927	1902.969702	20.905459
66.777562	1905.682732	20.910477
66.929814	1904.680635	20.915495
67.290596	1922.313701	20.920512
67.180086	1925.758573	20.925530
67.347371	1928.288860	20.930547
67.216146	1919.235990	20.935565
67.564947	1918.247282	20.940583
67.342153	1920.065460	20.945600
67.467319	1910.322285	20.950618
67.623392	1931.638944	20.955635
67.907260	1935.116708	20.960653
68.251988	1940.134544	20.965671
68.239997	1946.413871	20.970688
68.421330	1937.968473	20.975706
68.178067	1928.295637	20.980723
68.154449	1910.105020	20.985741
67.986894	1917.216650	20.990759
68.222878	1931.078902	20.995776
68.675082	1929.152435	21.000794
68.307349	1941.793224	21.005811
68.478011	1939.071365	21.010829
68.788771	1933.704904	21.015847
68.459977	1935.022104	21.020864
68.251434	1925.457446	21.025882
68.333791	1927.931607	21.030899
68.396272	1923.721279	21.035917
68.775939	1931.409942	21.040935
68.891346	1943.754114	21.045952
69.253259	1948.860784	21.050970
68.916827	1956.892043	21.055987
69.249437	1947.630778	21.061005
69.507384	1946.031411	21.066023
69.296284	1947.784639	21.071040
69.742645	1948.775250	21.076058
69.362507	1952.410704	21.081075
69.601992	1947.932781	21.086093
69.441187	1953.310711	21.091111
69.517116	1956.230883	21.096128
69.560098	1942.656530	21.101146
69.430400	1952.801491	21.106163
69.721471	1967.772373	21.111181
69.801405	1977.234363	21.116199
69.600279	1977.013514	21.121216
69.857937	1982.411103	21.126234
69.911487	1983.438012	21.131251
70.028043	1972.301188	21.136269
70.025600	1983.663391	21.141287
69.781248	1989.003926	21.146304
70.456411	1991.419933	21.151322
70.386757	1994.041005	21.156339
70.373860	1990.574670	21.161357
70.548655	2000.772945	21.166375
70.212980	2014.134649	21.171392
70.546280	2014.199324	21.176410
70.673550	2024.433462	21.181427
70.813562	2015.817764	21.186445
71.113848	2023.275889	21.191463
70.944364	2018.189789	21.196480
71.226587	2014.481537	21.201498
71.010189	2017.409647	21.206515
71.071187	2022.800187	21.211533
71.298789	2034.173721	21.216551
71.323785	2038.380080	21.221568
71.785302	2039.456691	21.226586
71.958876	2032.413747	21.231603
72.061124	2036.197718	21.236621
72.234662	2033.292344	21.241639
72.151702	2026.570482	21.246656
72.184752	2012.530539	21.251674
72.093276	2007.006155	21.256691
71.881093	1998.505611	21.261709
72.290700	2002.396064	21.266727
72.050915	2006.085284	21.271744
72.206497	2009.346460	21.276762
72.252496	2022.481101	21.281779
72.450801	2032.315922	21.286797
72.490099	2031.460913	21.291815
72.474747	2032.261917	21.296832
72.657448	2029.007945	21.301850
72.341007	2037.490577	21.306867
72.223084	2032.001889	21.311885
72.529032	2034.131742	21.316903
72.650928	2035.858054	21.321920
72.974414	2022.388027	21.326938
72.495266	2036.352936	21.331955
72.549059	2049.306481	21.336973
73.212575	2056.417355	21.341991
73.080815	2062.765984	21.347008
72.977427	2055.169932	21.352026
73.440908	2051.897212	21.357043
73.050799	2057.058617	21.362061
73.284848	2051.688360	21.367079
73.202390	2072.212519	21.372096
73.595105	2075.436554	21.377114
73.762871	2085.790625	21.382131
73.803647	2089.256010	21.387149
73.653397	2080.578452	21.392167
73.419781	2083.054800	21.397184
73.286781	2080.967521	21.402202
73.725077	2087.835962	21.407219
73.662562	2098.431262	21.412237
73.740402	2100.742040	21.417255
73.650550	2102.668806	21.422272
74.197831	2119.266066	21.427290
74.538969	2125.711053	21.432307
74.665453	2120.401813	21.437325
74.555850	2125.020632	21.442343
74.521717	2128.286305	21.447360
74.535705	2121.126307	21.452378
75.191278	2115.674208	21.457395
75.014095	2119.558785	21.462413
75.216083	2119.038072	21.467431
75.014327	2119.637894	21.472448
75.135058	2118.561823	21.477466
75.113756	2131.047473	21.482483
75.544544	2139.028041	21.487501
75.866386	2140.199132	21.492519
75.568988	2129.632035	21.497536
75.443122	2118.624628	21.502554
75.348021	2126.551874	21.507571
75.483439	2136.762708	21.512589
75.933100	2137.601323	21.517607
75.874607	2146.144585	21.522624
75.743787	2143.760288	21.527642
75.793496	2139.845424	21.532659
75.962829	2142.788864	21.537677
76.110676	2134.774689	21.542695
75.821226	2137.417594	21.547712
75.902480	2143.174256	21.552730
76.252238	2156.782153	21.557747
76.284713	2159.728102	21.562765
76.766698	2156.487181	21.567783
76.316013	2159.518298	21.572800
76.156009	2163.927256	21.577818
76.244208	2163.285503	21.582835
76.618334	2176.949563	21.587853
77.180692	2178.177655	21.592871
77.247587	2186.758100	21.597888
77.248905	2180.329114	21.602906
77.507480	2175.567254	21.607923
77.212837	2177.248379	21.612941
77.960157	2169.799883	21.617959
77.692141	2171.940777	21.622976
77.173647	2148.156012	21.627994
77.226143	2149.154692	21.633011
77.372930	2164.022102	21.638029
77.598461	2162.860175	21.643047
77.455612	2179.180579	21.648064
77.407622	2179.342866	21.653082
77.893446	2178.272712	21.658099
77.646480	2175.553129	21.663117
77.509668	2184.080275	21.668135
77.743910	2180.903414	21.673152
77.919774	2188.336917	21.678170
78.247956	2190.318127	21.683187
77.738880	2202.264816	21.688205
78.424176	2202.447927	21.693223
78.046927	2195.563808	21.698240
78.288107	2196.062674	21.703258
78.529309	2205.291217	21.708275
78.531797	2220.061351	21.713293
78.805441	2231.178467	21.718311
78.769186	2223.278310	21.723328
78.865236	2217.850723	21.728346
78.700912	2213.133018	21.733363
79.263779	2220.202918	21.738381
78.883708	2221.528172	21.743399
79.174997	2219.825719	21.748416
79.247995	2230.327276	21.753434
79.806027	2232.304040	21.758451
79.737309	2228.978960	21.763469
79.839214	2233.242749	21.768487
80.014497	2239.275069	21.773504
79.963576	2233.526491	21.778522
79.973325	2225.644375	21.783539
80.078162	2228.967195	21.788557
80.024869	2223.897548	21.793575
80.180992	2225.874158	21.798592
80.175009	2222.703366	21.803610
80.569903	2215.821351	21.808627
80.272792	2227.564419	21.813645
80.367559	2225.346756	21.818663
80.293393	2229.707564	21.823680
80.442137	2228.680751	21.828698
80.744622	2227.490983	21.833715
80.439428	2234.428626	21.838733
80.415226	2222.966532	21.843751
80.543009	2224.483640	21.848768
80.531850	2241.509364	21.853786
81.069650	2252.070666	21.858803
80.921201	2253.261794	21.863821
80.831745	2255.459936	21.868839
80.612972	2264.400784	21.873856
80.692290	2266.329466	21.878874
80.853650	2269.390952	21.883891
81.219538	2282.428323	21.888909
81.495096	2272.604580	21.893927
81.203899	2277.867325	21.898944
81.450516	2295.963654	21.903962
81.712590	2303.263767	21.908979
81.422912	2315.760032	21.913997
81.912813	2302.920188	21.919015
82.177801	2307.174224	21.924032
82.143405	2297.695701	21.929050
82.560551	2300.461474	21.934067
82.287839	2301.924561	21.939085
82.403259	2311.905078	21.944103
82.821399	2306.906725	21.949120
82.533008	2304.629152	21.954138
83.032680	2313.340687	21.959155
82.888653	2312.321865	21.964173
82.946728	2305.375812	21.969191
83.172026	2317.317982	21.974208
83.292715	2310.983866	21.979226
83.236518	2285.826180	21.984243
82.976850	2293.299559	21.989261
83.166547	2296.833178	21.994279
83.406367	2308.624731	21.999296
83.264116	2309.830672	22.004314
83.283423	2303.802802	22.009331
83.208577	2309.309395	22.014349
83.259922	2311.542294	22.019367
83.292821	2309.577332	22.024384
82.938342	2308.285343	22.029402
83.352676	2313.254506	22.034419
83.338984	2335.346236	22.039437
83.547605	2330.992985	22.044455
83.840343	2346.951779	22.049472
83.878543	2364.134003	22.054490
84.137508	2359.252102	22.059507
84.111981	2369.059055	22.064525
84.356988	2358.065984	22.069543
84.522256	2362.947940	22.074560
84.481636	2360.994491	22.079578
84.562793	2362.458950	22.084595
84.422224	2377.633514	22.089613
84.916673	2375.615168	22.094631
85.203415	2379.600702	22.099648
84.821899	2382.936628	22.104666
84.844494	2387.670514	22.109683
84.930680	2381.859379	22.114701
85.323346	2385.657889	22.119719
85.575236	2392.363131	22.124736
85.384249	2405.645646	22.129754
85.529636	2397.429749	22.134771
85.331905	2401.513284	22.139789
85.687113	2396.764631	22.144807
85.843573	2398.719115	22.149824
85.784077	2399.845818	22.154842
85.911823	2400.160473	22.159859
85.845191	2399.293638	22.164877
85.554886	2412.178269	22.169895
85.955976	2416.253202	22.174912
85.856362	2428.915446	22.179930
86.172099	2413.865131	22.184947
86.450125	2431.435919	22.189965
86.656422	2439.227711	22.194983
86.834085	2435.160179	22.200000
86.915640	2445.676302	22.205018
87.217205	2441.851313	22.210035
87.554093	2445.286154	22.215053
87.272273	2432.633406	22.220071
87.554804	2415.085499	22.225088
87.233962	2408.782652	22.230106
87.675943	2400.637060	22.235123
87.336843	2413.728172	22.240141
87.429697	2414.057761	22.245159
87.716256	2421.414052	22.250176
87.627450	2427.014395	22.255194
87.660556	2431.484689	22.260211
87.726295	2441.529872	22.265229
88.017809	2428.061395	22.270247
87.986700	2425.061777	22.275264
87.690884	2425.846775	22.280282
88.111454	2429.066511	22.285299
87.673812	2432.070380	22.290317
87.903733	2438.630744	22.295335
87.714167	2449.495490	22.300352
87.996251	2458.525236	22.305370
88.243646	2456.034298	22.310387
88.439520	2463.275414	22.315405
88.344033	2477.953802	22.320423
88.848247	2470.123509	22.325440
88.447709	2476.602766	22.330458
89.138362	2473.638396	22.335475
89.032685	2473.812881	22.340493
89.204914	2473.770238	22.345511
89.607611	2472.504788	22.350528
89.133313	2476.688482	22.355546
88.897582	2479.720690	22.360563
89.447282	2484.289959	22.365581
89.791295	2488.676839	22.370599
89.874611	2492.034641	22.375616
89.708159	2495.191711	22.380634
90.217606	2489.099611	22.385651
89.994967	2480.925556	22.390669
89.785008	2491.051834	22.395687
89.906072	2492.964532	22.400704
90.058734	2495.030086	22.405722
90.135858	2502.425536	22.410739
90.103335	2511.883334	22.415757
90.498617	2518.818648	22.420775
90.551317	2519.201872	22.425792
90.381611	2521.589363	22.430810
90.448769	2521.092919	22.435827
90.744138	2528.602525	22.440845
90.819388	2529.686032	22.445863
91.217940	2532.224358	22.450880
91.182094	2537.627070	22.455898
90.924680	2533.296288	22.460915
91.084576	2536.092935	22.465933
90.863615	2537.828827	22.470951
91.443481	2544.145035	22.475968
91.537122	2553.393721	22.480986
91.781794	2550.578116	22.486003
91.749221	2549.434511	22.491021
91.644254	2564.237544	22.496039
92.025981	2544.998064	22.501056
91.683599	2549.656618	22.506074
92.012126	2557.628148	22.511091
92.254551	2571.508824	22.516109
92.293998	2580.848073	22.521127
92.594403	2573.368437	22.526144
92.241831	2576.788235	22.531162
92.255965	2576.186477	22.536179
92.424172	2569.425060	22.541197
92.549990	2591.154384	22.546215
92.982991	2587.510765	22.551232
93.402690	2590.569705	22.556250
93.300455	2597.980670	22.561267
93.486904	2592.832328	22.566285
93.466001	2592.747353	22.571303
93.570628	2585.803366	22.576320
93.592099	2600.491935	22.581338
93.499950	2600.358156	22.586355
93.562636	2596.182356	22.591373
93.469099	2602.891299	22.596391
93.555292	2595.789234	22.601408
93.382344	2601.014609	22.606426
93.760701	2603.717072	22.611443
94.175004	2610.507415	22.616461
94.035777	2615.923192	22.621479
94.384351	2615.483652	22.626496
94.224571	2612.138051	22.631514
94.170785	2612.326500	22.636531
94.629737	2627.202196	22.641549
94.469520	2634.574919	22.646567
94.503254	2638.862110	22.651584
94.682911	2637.243388	22.656602
94.541132	2643.480170	22.661619
94.519387	2640.157123	22.666637
94.641991	2644.559794	22.671655
95.374038	2647.670803	22.676672
95.443231	2656.806595	22.681690
95.357190	2657.296776	22.686707
95.611484	2656.865694	22.691725
95.638846	2651.212028	22.696743
95.770507	2647.132719	22.701760
95.645033	2652.650505	22.706778
95.655911	2643.792779	22.711795
95.685302	2646.493112	22.716813
95.636748	2670.462309	22.721831
96.388030	2673.636588	22.726848
96.469592	2677.083072	22.731866
96.368557	2682.092054	22.736883
96.729818	2683.468468	22.741901
96.453217	2678.329526	22.746919
96.658245	2680.762480	22.751936
96.720279	2680.244742	22.756954
96.357458	2679.534764	22.761971
96.620067	2677.458025	22.766989
96.702216	2709.694849	22.772007
97.206050	2693.677453	22.777024
97.028440	2702.656254	22.782042
97.076790	2701.897636	22.787059
96.993356	2701.882424	22.792077
97.282292	2727.840854	22.797095
97.622920	2729.179475	22.802112
97.354149	2730.209584	22.807130
97.223718	2723.378120	22.812147
97.658187	2727.735106	22.817165
97.968058	2739.651683	22.822183
98.053645	2747.677140	22.827200
98.082212	2748.174616	22.832218
97.947374	2752.939577	22.837235
98.237851	2745.855945	22.842253
98.236264	2750.798867	22.847271
98.627583	2768.689945	22.852288
98.719385	2780.981580	22.857306
98.929529	2778.537466	22.862323
98.879813	2767.372545	22.867341
98.895323	2780.714512	22.872359
99.066947	2770.127209	22.877376
99.659033	2773.241232	22.882394
99.113361	2779.721242	22.887411
99.485104	2765.065849	22.892429
99.241050	2771.877341	22.897447
99.452517	2788.404747	22.902464
99.685610	2794.002113	22.907482
99.892707	2794.443214	22.912499
99.886187	2793.841529	22.917517
99.849745	2795.725282	22.922535
100.100696	2798.567671	22.927552
99.755626	2789.096533	22.932570
100.177315	2813.244739	22.937587
100.433744	2827.177073	22.942605
100.744547	2818.830915	22.947623
100.596255	2816.253582	22.952640
100.550716	2815.355016	22.957658
100.612154	2816.462798	22.962675
100.817052	2821.089332	22.967693
100.831737	2824.524229	22.972711
100.988927	2819.263628	22.977728
100.931387	2835.732226	22.982746
101.035467	2838.452448	22.987763
101.439049	2838.035847	22.992781
101.428299	2843.968114	22.997799
101.274400	2840.192308	23.002816
101.596454	2836.742768	23.007834
101.362760	2844.871946	23.012851
101.880191	2853.694586	23.017869
101.955066	2862.173106	23.022887
102.055017	2869.726096	23.027904
101.962877	2870.637010	23.032922
101.849906	2864.623365	23.037939
101.976931	2864.688802	23.042957
102.041266	2881.192002	23.047975
102.125108	2892.282454	23.052992
102.392108	2886.790008	23.058010
102.444513	2893.763407	23.063027
102.707452	2885.263751	23.068045
102.797177	2902.356356	23.073063
102.818585	2903.688192	23.078080
102.991632	2909.525404	23.083098
102.687837	2915.734008	23.088115
103.151216	2922.652497	23.093133
103.019638	2935.017110	23.098151
103.306618	2932.589343	23.103168
103.668211	2941.461691	23.108186
103.220474	2935.689842	23.113203
104.085043	2944.578075	23.118221
103.936654	2950.752874	23.123239
104.188395	2952.237999	23.128256
104.385230	2939.825520	23.133274
104.011912	2946.808826	23.138291
104.235339	2943.494654	23.143309
104.721532	2944.176091	23.148327
104.732094	2951.149755	23.153344
104.888904	2945.371560	23.158362
104.679864	2958.979242	23.163379
104.893356	2968.900572	23.168397
105.103363	2965.033008	23.173415
105.451616	2960.566200	23.178432
105.594505	2959.944257	23.183450
105.435971	2960.294305	23.188467
106.010306	2958.711562	23.193485
105.841985	2959.798538	23.198503
105.791419	2957.392090	23.203520
105.917342	2962.021565	23.208538
105.714247	2953.676953	23.213555
105.900288	2956.220230	23.218573
106.256088	2962.988311	23.223591
106.271548	2971.936998	23.228608
106.584194	2972.765561	23.233626
106.537809	2978.264742	23.238643
106.500243	2980.467467	23.243661
106.656524	2977.034405	23.248679
106.566712	2976.067019	23.253696
106.930925	2974.788628	23.258714
106.864941	2973.041083	23.263731
107.059665	2967.850307	23.268749
107.332135	2985.463539	23.273767
107.051429	2994.067268	23.278784
107.268608	2993.626213	23.283802
107.384427	2999.415609	23.288819
107.453420	2997.400730	23.293837
107.373793	3001.961422	23.298855
107.557714	3022.659553	23.303872
107.853821	3022.752156	23.308890
107.748157	3028.443700	23.313907
107.882662	3028.539529	23.318925
107.652484	3033.262689	23.323943
108.007341	3041.710053	23.328960
108.121099	3045.202063	23.333978
108.182014	3054.421415	23.338995
108.361634	3048.191431	23.344013
108.489684	3061.841065	23.349031
108.591909	3073.844052	23.354048
108.877560	3065.956216	23.359066
108.860084	3071.854892	23.364083
109.140810	3072.104561	23.369101
109.036337	3069.207860	23.374119
109.012841	3085.220013	23.379136
109.592833	3086.685284	23.384154
109.714870	3099.733050	23.389171
109.417925	3089.439907	23.394189
109.282357	3095.006752	23.399207
109.271327	3098.073295	23.404224
109.730086	3105.702730	23.409242
110.031483	3119.195844	23.414259
110.199435	3118.753030	23.419277
110.308127	3118.038597	23.424295
110.590044	3130.464809	23.429312
110.682870	3137.081627	23.434330
110.559675	3138.878009	23.439347
110.729447	3135.225023	23.444365
111.038996	3138.623251	23.449383
111.046649	3128.938859	23.454400
110.926354	3129.002015	23.459418
111.383799	3142.477010	23.464435
111.379180	3153.698263	23.469453
111.539127	3161.134664	23.474471
111.205516	3157.172323	23.479488
111.786850	3149.329656	23.484506
111.806431	3159.028973	23.489523
112.119128	3158.487731	23.494541
112.574110	3149.711678	23.499559
111.903385	3154.721670	23.504576
112.163577	3159.446941	23.509594
112.226380	3174.097940	23.514611
112.299476	3175.440635	23.519629
112.732788	3179.182449	23.524647
112.385252	3187.010836	23.529664
112.372191	3189.645308	23.534682
112.744924	3205.595489	23.539699
113.060354	3203.018042	23.544717
113.138810	3199.635006	23.549735
113.066842	3210.705877	23.554752
113.130527	3216.743385	23.559770
113.684968	3224.597755	23.564787
113.966576	3217.534268	23.569805
114.096491	3225.748680	23.574823
114.037365	3222.264101	23.579840
114.182421	3220.530812	23.584858
114.204370	3219.713183	23.589875
114.208309	3212.535388	23.594893
114.165667	3217.822588	23.599911
113.898239	3225.752066	23.604928
114.411040	3232.770245	23.609946
114.766739	3238.061324	23.614963
114.495664	3241.083414	23.619981
115.159112	3237.488782	23.624999
114.651526	3241.984020	23.630016
115.154752	3242.255644	23.635034
115.162108	3257.139491	23.640051
115.236530	3255.190014	23.645069
115.358208	3252.481947	23.650087
115.223492	3260.617898	23.655104
115.162132	3257.534506	23.660122
115.591753	3279.374876	23.665139
115.985749	3288.772571	23.670157
116.094917	3281.546699	23.675175
116.072112	3282.478333	23.680192
115.860798	3277.493115	23.685210
115.930155	3286.957452	23.690227
116.096899	3299.644857	23.695245
116.796989	3309.468046	23.700263
116.318935	3315.893463	23.705280
116.683316	3306.610745	23.710298
116.684159	3312.901163	23.715315
116.783091	3330.642922	23.720333
117.176120	3326.355229	23.725351
116.903833	3332.862040	23.730368
117.209947	3332.662702	23.735386
117.504347	3337.054409	23.740403
117.244420	3352.447337	23.745421
117.380263	3363.580433	23.750439
117.433657	3357.666808	23.755456
117.648976	3365.249275	23.760474
118.147111	3377.004217	23.765491
117.989297	3383.171171	23.770509
118.420654	3378.647054	23.775527
118.284258	3385.643910	23.780544
118.070397	3380.182465	23.785562
118.244088	3402.097799	23.790579
118.254452	3407.111622	23.795597
118.549878	3403.675617	23.800615
118.862906	3422.403401	23.805632
119.168739	3424.482941	23.810650
119.500515	3428.619468	23.815667
119.547926	3430.392305	23.820685
119.660597	3421.944348	23.825703
119.688723	3425.898039	23.830720
119.966602	3426.094503	23.835738
120.070199	3421.880541	23.840755
119.661947	3425.467033	23.845773
119.935406	3438.355601	23.850791
120.226957	3449.309696	23.855808
120.679475	3438.434960	23.860826
120.605080	3445.365312	23.865843
120.503723	3447.994718	23.870861
120.919329	3431.103578	23.875879
120.643198	3448.929464	23.880896
120.677103	3458.449946	23.885914
121.184765	3462.726208	23.890931
121.113462	3455.550636	23.895949
121.262574	3455.347488	23.900967
121.243133	3466.460787	23.905984
121.942689	3479.743445	23.911002
121.746312	3482.116302	23.916019
121.882632	3489.733292	23.921037
122.272393	3479.158743	23.926055
122.224802	3483.850257	23.931072
122.077603	3478.413057	23.936090
122.248754	3474.592504	23.941107
122.226547	3482.673052	23.946125
122.861888	3482.687262	23.951143
122.684669	3500.043196	23.956160
122.886006	3507.132375	23.961178
122.995179	3494.124085	23.966195
122.834798	3501.134212	23.971213
123.015260	3496.030740	23.976231
122.990407	3503.625644	23.981248
123.230237	3519.350735	23.986266
123.270861	3521.856905	23.991283
123.369590	3529.735462	23.996301
123.940740	3532.275299	24.001319
123.837402	3547.640704	24.006336
124.077186	3549.973642	24.011354
124.465250	3544.941789	24.016371
124.260580	3549.983029	24.021389
124.511071	3541.819584	24.026407
124.367873	3555.347960	24.031424
124.334170	3548.961848	24.036442
124.344287	3545.052883	24.041459
124.452759	3570.267507	24.046477
124.730693	3565.656910	24.051495
124.887153	3577.307697	24.056512
125.170185	3569.568400	24.061530
125.677086	3577.316747	24.066547
125.663702	3588.943651	24.071565
125.709301	3583.211084	24.076583
125.283105	3602.326311	24.081600
125.333571	3596.921234	24.086618
125.824159	3593.842844	24.091635
125.799159	3605.155947	24.096653
125.909336	3617.969222	24.101671
125.828104	3623.584530	24.106688
126.112815	3621.908231	24.111706
126.511704	3630.554136	24.116723
126.360612	3637.818522	24.121741
126.546044	3629.845141	24.126759
127.131920	3648.546194	24.131776
127.040108	3651.344575	24.136794
127.532646	3662.355688	24.141811
127.384558	3653.121519	24.146829
127.575925	3659.824094	24.151847
127.587628	3648.248153	24.156864
127.488378	3654.364992	24.161882
127.961936	3657.100047	24.166899
127.689930	3674.360527	24.171917
128.070197	3672.950166	24.176935
128.164225	3678.891541	24.181952
128.102113	3680.514277	24.186970
128.347202	3694.297556	24.191987
128.435700	3708.089597	24.197005
128.762458	3702.814800	24.202023
128.931505	3704.496012	24.207040
129.019983	3704.842093	24.212058
129.349837	3721.632722	24.217075
129.521165	3723.891187	24.222093
129.489988	3716.731318	24.227111
129.835379	3723.857985	24.232128
129.625849	3722.552648	24.237146
129.557940	3711.150112	24.242163
129.549721	3729.571879	24.247181
130.159650	3729.511164	24.252199
130.203887	3743.632113	24.257216
130.371056	3736.229687	24.262234
130.827128	3739.485134	24.267251
130.746486	3732.358259	24.272269
130.476577	3735.784259	24.277287
130.908796	3756.778903	24.282304
130.668639	3760.853609	24.287322
131.044503	3762.694961	24.292339
130.806349	3771.967847	24.297357
131.330031	3782.361825	24.302375
131.232198	3790.990938	24.307392
131.299218	3796.365285	24.312410
131.935297	3799.030712	24.317427
132.085044	3807.422195	24.322445
132.232619	3809.239347	24.327463
132.093219	3816.874422	24.332480
132.398329	3816.160753	24.337498
132.769048	3810.317207	24.342515
132.386148	3813.236969	24.347533
132.687624	3807.375865	24.352551
132.692319	3819.022179	24.357568
132.623245	3830.285513	24.362586
132.905857	3833.681782	24.367603
132.922165	3834.304307	24.372621
133.014931	3833.355615	24.377639
133.459887	3839.377787	24.382656
133.682245	3857.107038	24.387674
133.642004	3854.159115	24.392691
133.508309	3859.157757	24.397709
133.520895	3855.235712	24.402727
134.118569	3874.572736	24.407744
133.947710	3871.481143	24.412762
134.160328	3876.154086	24.417779
134.173899	3883.105544	24.422797
134.848469	3890.584719	24.427815
134.772848	3900.596047	24.432832
135.284823	3905.099000	24.437850
135.431198	3899.688275	24.442867
135.044296	3909.530587	24.447885
135.414530	3894.606228	24.452903
135.597581	3898.475781	24.457920
135.097644	3903.620192	24.462938
135.502976	3916.542099	24.467955
135.697389	3924.661504	24.472973
135.633964	3921.199558	24.477991
136.000276	3931.460459	24.483008
135.990426	3934.091380	24.488026
136.366232	3943.132441	24.493043
136.276887	3953.834038	24.498061
136.443554	3956.863418	24.503079
136.868314	3963.261248	24.508096
136.330157	3968.844088	24.513114
136.914795	3962.465116	24.518131
137.416028	3993.170860	24.523149
137.455731	3991.744391	24.528167
137.593253	3997.622242	24.533184
137.727541	4002.045510	24.538202
137.869606	3992.844619	24.543219
137.808476	4002.771667	24.548237
138.017682	4010.210171	24.553255
138.395640	4012.815066	24.558272
138.076095	4017.019052	24.563290
138.107543	4003.416548	24.568307
138.201806	4024.739057	24.573325
138.572384	4035.684285	24.578343
139.029145	4032.892041	24.583360
139.090004	4032.611178	24.588378
139.429153	4039.196050	24.593395
139.279662	4054.158784	24.598413
139.346078	4056.465291	24.603431
139.882035	4045.779130	24.608448
139.792152	4056.910141	24.613466
139.562961	4055.301690	24.618483
140.140328	4068.193598	24.623501
140.299786	4072.376210	24.628519
140.595480	4073.608346	24.633536
140.476458	4081.578074	24.638554
140.630765	4067.590132	24.643571
140.515683	4075.171003	24.648589
141.006909	4079.241668	24.653607
141.212651	4084.408140	24.658624
141.282686	4097.461618	24.663642
141.823526	4096.502685	24.668659
141.603448	4093.573429	24.673677
141.676900	4099.578138	24.678695
141.983067	4088.861669	24.683712
141.437201	4091.636561	24.688730
141.898402	4098.173924	24.693747
141.649622	4120.752878	24.698765
141.906247	4121.132596	24.703783
142.273332	4114.670868	24.708800
142.226373	4140.570326	24.713818
142.447067	4139.598419	24.718835
142.630225	4142.839883	24.723853
142.063721	4156.274049	24.728871
142.687322	4166.198072	24.733888
142.910221	4175.802952	24.738906
143.391315	4166.539389	24.743923
143.501330	4189.333668	24.748941
143.446164	4196.106629	24.753959
143.498241	4200.549139	24.758976
143.788440	4208.713637	24.763994
144.076986	4204.344261	24.769011
144.302643	4212.503090	24.774029
144.379656	4221.663700	24.779047
144.564541	4219.100252	24.784064
144.676724	4218.505173	24.789082
144.628393	4229.377266	24.794099
144.781900	4230.483337	24.799117
145.116207	4236.497727	24.804135
145.425637	4231.894654	24.809152
145.557806	4246.134788	24.814170
145.642167	4239.316444	24.819187
145.572624	4246.369442	24.824205
145.860753	4267.885971	24.829223
146.039178	4267.113222	24.834240
145.990427	4268.762324	24.839258
145.868509	4256.398883	24.844275
146.014740	4284.689259	24.849293
146.254508	4289.465375	24.854311
146.459475	4289.345005	24.859328
146.615901	4300.885789	24.864346
146.982104	4300.058369	24.869363
147.014943	4302.730002	24.874381
147.274870	4312.149237	24.879399
147.219030	4318.556204	24.884416
147.593631	4330.267995	24.889434
147.645434	4335.900558	24.894451
147.579711	4341.093851	24.899469
147.675290	4349.519324	24.904487
148.216906	4351.539939	24.909504
148.191779	4355.180220	24.914522
148.085734	4353.457755	24.919539
148.586544	4371.153355	24.924557
148.572914	4382.414659	24.929575
148.687014	4386.553947	24.934592
149.245651	4394.786949	24.939610
149.079781	4395.179206	24.944627
149.509007	4405.118032	24.949645
149.374321	4406.509154	24.954663
149.436123	4405.634726	24.959680
149.788402	4419.821574	24.964698
149.973514	4420.881672	24.969715
150.135506	4427.077788	24.974733
149.954857	4432.191262	24.979751
150.298454	4435.271916	24.984768
150.316161	4454.078601	24.989786
150.903236	4450.189526	24.994803
150.988660	4456.233512	24.999821
150.838404	4465.644491	25.004839
151.116674	4476.279332	25.009856
151.585343	4481.202713	25.014874
151.481061	4481.301240	25.019891
151.792190	4479.529188	25.024909
151.630605	4490.829521	25.029927
152.021922	4492.460203	25.034944
151.998272	4499.354599	25.039962
152.257086	4502.663186	25.044979
152.155787	4506.643703	25.049997
152.137326	4521.785151	25.055015
152.410497	4528.920295	25.060032
152.599758	4533.035216	25.065050
152.509641	4538.841587	25.070067
152.983828	4547.507701	25.075085
153.064333	4554.186942	25.080103
153.489570	4546.645906	25.085120
153.428180	4561.153348	25.090138
153.330826	4576.938498	25.095155
153.785829	4583.726372	25.100173
153.809618	4580.951375	25.105191
154.159977	4582.509570	25.110208
154.376230	4603.507468	25.115226
154.291511	4606.437456	25.120243
154.844952	4603.901439	25.125261
154.637045	4596.510078	25.130279
154.750873	4603.985864	25.135296
155.138319	4622.362332	25.140314
155.149564	4634.184906	25.145331
155.130970	4626.684962	25.150349
155.327419	4639.548575	25.155367
156.152469	4643.806964	25.160384
156.069948	4644.694363	25.165402
156.428068	4653.220887	25.170419
156.436481	4653.150248	25.175437
156.713243	4645.837604	25.180455
156.321848	4642.316424	25.185472
156.817202	4659.407115	25.190490
156.934344	4672.245297	25.195507
157.351608	4682.593339	25.200525
157.044824	4680.053193	25.205543
156.974923	4681.393153	25.210560
157.175553	4683.116857	25.215578
157.529066	4684.160057	25.220595
157.745163	4697.983365	25.225613
157.637396	4706.330383	25.230631
157.947897	4715.896574	25.235648
158.205889	4727.929916	25.240666
158.159436	4719.411590	25.245683
158.214306	4731.334714	25.250701
158.556980	4742.499385	25.255719
158.658965	4739.194446	25.260736
158.723155	4754.102183	25.265754
159.167353	4770.108839	25.270771
159.291179	4770.010648	25.275789
159.258570	4770.628243	25.280807
159.349486	4783.682100	25.285824
159.574958	4789.679004	25.290842
159.653722	4797.491797	25.295859
160.390619	4811.094713	25.300877
160.152211	4818.449006	25.305895
160.115700	4822.160607	25.310912
160.640500	4830.907311	25.315930
160.389344	4845.772988	25.320947
160.621511	4834.957196	25.325965
160.829401	4854.069091	25.330983
161.547301	4864.354355	25.336000
161.443580	4859.250833	25.341018
161.489237	4864.982376	25.346035
161.679433	4874.094018	25.351053
162.088076	4889.714940	25.356071
162.074817	4885.888261	25.361088
162.169034	4878.638845	25.366106
162.365572	4893.696415	25.371123
162.545566	4896.452404	25.376141
162.965983	4902.017924	25.381159
163.087122	4901.945406	25.386176
162.913861	4904.033892	25.391194
163.209038	4905.300889	25.396211
163.538984	4920.956263	25.401229
163.366325	4929.335645	25.406247
163.572115	4922.892590	25.411264
163.738338	4927.500474	25.416282
163.897903	4932.150437	25.421299
164.078017	4941.734019	25.426317
164.032631	4942.426221	25.431335
164.423570	4945.291214	25.436352
164.453826	4956.132490	25.441370
164.527623	4977.951745	25.446387
165.024941	4971.674489	25.451405
165.044387	4979.727082	25.456423
165.371664	4982.529454	25.461440
165.459011	4991.379492	25.466458
165.728048	5000.185287	25.471475
165.776495	5001.194230	25.476493
165.899780	5006.253935	25.481511
166.143875	5013.987259	25.486528
166.658892	5020.279786	25.491546
166.640016	5022.975410	25.496563
166.661132	5018.483597	25.501581
166.439948	5020.705866	25.506599
166.842190	5037.587385	25.511616
167.441390	5042.307390	25.516634
167.367545	5046.387890	25.521651
167.548391	5045.093898	25.526669
167.774544	5055.958205	25.531687
167.899106	5067.460277	25.536704
168.093618	5068.594699	25.541722
168.001472	5074.379462	25.546739
168.380150	5074.377077	25.551757
168.306094	5087.444371	25.556775
168.078670	5092.723186	25.561792
168.589032	5108.123183	25.566810
168.666676	5118.609908	25.571827
168.920342	5117.272937	25.576845
168.890258	5135.746904	25.581863
169.297651	5144.692079	25.586880
169.584331	5143.700314	25.591898
169.717499	5163.685988	25.596915
169.763951	5167.400445	25.601933
169.644322	5174.622635	25.606951
170.270288	5189.632113	25.611968
170.410603	5189.540808	25.616986
170.607952	5199.781552	25.622003
170.609665	5205.406449	25.627021
171.015802	5209.377067	25.632039
170.960113	5221.892332	25.637056
171.634320	5234.851975	25.642074
171.670166	5245.648355	25.647091
172.213686	5244.853092	25.652109
172.293157	5248.906461	25.657127
172.115942	5237.690547	25.662144
172.631486	5238.036042	25.667162
172.524034	5266.077281	25.672180
172.810102	5254.971859	25.677197
172.761164	5254.414617	25.682215
173.042713	5262.625139	25.687232
173.161555	5260.093988	25.692250
173.205950	5276.918155	25.697268
173.509955	5273.619349	25.702285
173.545689	5276.719970	25.707303
173.387996	5279.771979	25.712320
173.656338	5300.266935	25.717338
174.020897	5296.194740	25.722356
174.170744	5296.101941	25.727373
174.633414	5324.268601	25.732391
174.660755	5331.309997	25.737408
174.996899	5324.546500	25.742426
174.953265	5325.582514	25.747444
175.004556	5331.613199	25.752461
175.020990	5345.266257	25.757479
175.306041	5350.332281	25.762496
175.350736	5343.649160	25.767514
175.509582	5367.955598	25.772532
175.952567	5372.763296	25.777549
176.271986	5387.464266	25.782567
176.167399	5386.647425	25.787584
176.727272	5401.774759	25.792602
176.408260	5413.993651	25.797620
177.210249	5404.814927	25.802637
177.057732	5402.004293	25.807655
177.079173	5426.625902	25.812672
177.291167	5425.576377	25.817690
177.279330	5429.394718	25.822708
177.879639	5441.810520	25.827725
178.520905	5440.191839	25.832743
178.336263	5450.454689	25.837760
178.464892	5442.915561	25.842778
178.446055	5445.958470	25.847796
178.720266	5454.088156	25.852813
178.936409	5457.378352	25.857831
178.953131	5465.529442	25.862848
179.299511	5462.934207	25.867866
179.501295	5474.171908	25.872884
179.490077	5484.887417	25.877901
179.647776	5486.444309	25.882919
179.760650	5497.569688	25.887936
180.251371	5504.563809	25.892954
180.327704	5524.751339	25.897972
180.507813	5524.098228	25.902989
180.461286	5525.778661	25.908007
180.707639	5538.455164	25.913024
180.663585	5536.262003	25.918042
180.835327	5561.336901	25.923060
181.270704	5557.831221	25.928077
181.555926	5564.074710	25.933095
181.559851	5587.329292	25.938112
181.859549	5592.030075	25.943130
182.074823	5596.207453	25.948148
182.489215	5612.194269	25.953165
182.281004	5614.559782	25.958183
182.254988	5617.613315	25.963200
182.710867	5627.712785	25.968218
183.232341	5634.455919	25.973236
182.894395	5641.482059	25.978253
183.424627	5642.914312	25.983271
183.411295	5664.069356	25.988288
183.673129	5653.927117	25.993306
183.727335	5673.190216	25.998324
183.895239	5683.464256	26.003341
184.445843	5687.197693	26.008359
184.436865	5699.857489	26.013376
184.521727	5701.277447	26.018394
184.772810	5713.284115	26.023412
184.978678	5723.646930	26.028429
185.092387	5733.964211	26.033447
185.563386	5738.461421	26.038464
185.613863	5741.629258	26.043482
186.133133	5749.370293	26.048500
186.145903	5751.937956	26.053517
186.780630	5749.104950	26.058535
186.943580	5754.518512	26.063552
186.715013	5747.051002	26.068570
186.734401	5757.367290	26.073588
187.194173	5759.700778	26.078605
187.252706	5767.315129	26.083623
187.270590	5770.147155	26.088640
187.218991	5776.828601	26.093658
187.482072	5772.769043	26.098676
187.868772	5795.986021	26.103693
188.243634	5796.413546	26.108711
187.916209	5806.790509	26.113728
188.584837	5812.825654	26.118746
188.443052	5808.662210	26.123764
188.519539	5807.135136	26.128781
189.121311	5818.408243	26.133799
188.905101	5820.696119	26.138816
188.915564	5836.443370	26.143834
189.027209	5841.258909	26.148852
189.225979	5864.543296	26.153869
189.918382	5868.860645	26.158887
189.819169	5881.692538	26.163904
190.000591	5890.850259	26.168922
190.153273	5901.388813	26.173940
190.430688	5907.854613	26.178957
190.559823	5922.658430	26.183975
190.615769	5928.382382	26.188992
191.076539	5929.809759	26.194010
191.347273	5944.929179	26.199028
191.238710	5936.416858	26.204045
191.871657	5946.599251	26.209063
191.618580	5975.292579	26.214080
192.332527	5972.087263	26.219098
192.417205	5990.796653	26.224116
192.320341	5998.283923	26.229133
192.937101	6002.947768	26.234151
193.225577	6025.842656	26.239168
193.121380	6024.656387	26.244186
193.096116	6023.205213	26.249204
193.364787	6037.532694	26.254221
193.920886	6043.822301	26.259239
193.737243	6053.558157	26.264256
194.312508	6054.494096	26.269274
194.437035	6069.526039	26.274292
194.763116	6075.034096	26.279309
194.403601	6075.478820	26.284327
194.437929	6088.892874	26.289344
194.872084	6090.677989	26.294362
195.314672	6107.503673	26.299380
195.343729	6122.894702	26.304397
195.955082	6114.193752	26.309415
195.746461	6133.410122	26.314432
196.095911	6147.646116	26.319450
196.273104	6141.077686	26.324468
196.155050	6156.037217	26.329485
196.900854	6174.163395	26.334503
196.819836	6171.584512	26.339520
196.853960	6166.563200	26.344538
197.031715	6194.848447	26.349556
197.356600	6200.186265	26.354573
197.758794	6198.024131	26.359591
198.072102	6213.670597	26.364608
198.308137	6217.049361	26.369626
198.524492	6216.961924	26.374644
198.421322	6215.213577	26.379661
198.566196	6222.107476	26.384679
199.218570	6240.166281	26.389696
198.916293	6236.400381	26.394714
199.226669	6243.782914	26.399732
199.425136	6263.412317	26.404749
199.726215	6263.478916	26.409767
199.735754	6272.509074	26.414784
199.734994	6282.652035	26.419802
200.135361	6279.442129	26.424820
200.224078	6284.299259	26.429837
200.404673	6296.844535	26.434855
200.834877	6317.264768	26.439872
200.747401	6314.320689	26.444890
201.224626	6325.073814	26.449908
201.227813	6340.598507	26.454925
201.249867	6336.807030	26.459943
201.874561	6345.144221	26.464960
201.733591	6359.675028	26.469978
202.177806	6352.720601	26.474996
202.222713	6374.962748	26.480013
202.831371	6371.265617	26.485031
203.023994	6386.100901	26.490048
202.809624	6385.105492	26.495066
202.968746	6396.489343	26.500084
203.448313	6413.489455	26.505101
203.593949	6409.444999	26.510119
203.654352	6411.402344	26.515136
204.303608	6432.091441	26.520154
204.624495	6420.610515	26.525172
204.564947	6426.693651	26.530189
205.132697	6440.153825	26.535207
205.251584	6450.205529	26.540224
205.185312	6454.531387	26.545242
205.568284	6440.947759	26.550260
205.237817	6449.642983	26.555277
206.099007	6465.352204	26.560295
205.981869	6474.184487	26.565312
206.232572	6479.085741	26.570330
206.262826	6477.739479	26.575348
206.493020	6501.171281	26.580365
206.675171	6507.191324	26.585383
206.909131	6517.524935	26.590400
207.004626	6527.678207	26.595418
207.302173	6529.907782	26.600436
207.611732	6554.798297	26.605453
207.174473	6548.998386	26.610471
207.788840	6565.393509	26.615488
207.945784	6578.785556	26.620506
208.291967	6587.823110	26.625524
208.424781	6601.506226	26.630541
208.859243	6594.600589	26.635559
209.030242	6607.725282	26.640576
208.956691	6627.034655	26.645594
209.389791	6626.496558	26.650612
209.647396	6641.157714	26.655629
209.766472	6654.050655	26.660647
209.901185	6650.231994	26.665664
209.916577	6660.622024	26.670682
210.579148	6678.281904	26.675700
210.562227	6687.123844	26.680717
210.769634	6704.744566	26.685735
210.743225	6706.863914	26.690752
211.268249	6720.580381	26.695770
211.852785	6717.426783	26.700788
211.730955	6732.425257	26.705805
211.912488	6732.624233	26.710823
212.233949	6748.074155	26.715840
212.329129	6751.582419	26.720858
212.953219	6752.207691	26.725876
213.157850	6768.531441	26.730893
213.212181	6771.288461	26.735911
213.605590	6775.409792	26.740928
213.350958	6783.815490	26.745946
213.507832	6785.577820	26.750964
213.873272	6803.666351	26.755981
214.136885	6803.325273	26.760999
214.330717	6810.410607	26.766016
213.994506	6817.070724	26.771034
214.508881	6817.624795	26.776052
214.645080	6829.470253	26.781069
214.912802	6842.115901	26.786087
215.109570	6850.615070	26.791104
215.266743	6868.486898	26.796122
215.536429	6869.066676	26.801140
215.863982	6888.408192	26.806157
216.004134	6896.420622	26.811175
216.447819	6895.303151	26.816192
216.288012	6906.797264	26.821210
216.949937	6922.367625	26.826228
216.900868	6934.040134	26.831245
217.432502	6942.707867	26.836263
217.414461	6948.008078	26.841280
217.427324	6953.177173	26.846298
217.657431	6959.249833	26.851316
217.794855	6967.581567	26.856333
218.112013	6984.377200	26.861351
218.499402	6994.990106	26.866368
218.474317	7000.884933	26.871386
219.167715	7007.064973	26.876404
219.341611	7032.403571	26.881421
219.522000	7021.626173	26.886439
219.458391	7037.749104	26.891456
219.753006	7045.238609	26.896474
219.870875	7053.062026	26.901492
220.046671	7065.179241	26.906509
220.119599	7075.077485	26.911527
220.520846	7096.746948	26.916544
220.663369	7108.591596	26.921562
221.125446	7115.259352	26.926580
221.207830	7131.946680	26.931597
221.460825	7147.294015	26.936615
221.740846	7149.924185	26.941632
221.761471	7166.554925	26.946650
222.428852	7185.815105	26.951668
222.944422	7190.018416	26.956685
222.775087	7196.999789	26.961703
223.251655	7207.248429	26.966720
223.525509	7202.299772	26.971738
223.509708	7217.038946	26.976756
223.779929	7229.637116	26.981773
223.716287	7229.760858	26.986791
223.778963	7241.962206	26.991808
224.022789	7254.665551	26.996826
224.344600	7265.175238	27.001844
224.964569	7280.329446	27.006861
225.207016	7285.086991	27.011879
225.688932	7291.076116	27.016896
225.711606	7308.536941	27.021914
226.035966	7300.461277	27.026932
225.902051	7308.128516	27.031949
226.207993	7319.111106	27.036967
226.597498	7326.169142	27.041984
226.543941	7336.320957	27.047002
227.238902	7342.002068	27.052020
227.163598	7351.955252	27.057037
227.362503	7351.706384	27.062055
227.533325	7363.505722	27.067072
227.980249	7374.810368	27.072090
227.885586	7374.007666	27.077108
228.102848	7395.087540	27.082125
228.122983	7396.423062	27.087143
228.455822	7403.736250	27.092160
228.852069	7420.021090	27.097178
228.737316	7428.127353	27.102196
229.335007	7439.250571	27.107213
229.162328	7447.981528	27.112231
229.514144	7451.825401	27.117248
229.470054	7466.386102	27.122266
229.525319	7484.631233	27.127284
230.206892	7492.909530	27.132301
230.372077	7504.207881	27.137319
231.145888	7516.064389	27.142336
231.190006	7536.900049	27.147354
231.163273	7525.741238	27.152372
231.412819	7542.873144	27.157389
231.502301	7551.370503	27.162407
232.097616	7568.119937	27.167424
232.224159	7581.956301	27.172442
232.511288	7578.754443	27.177460
232.802626	7595.194781	27.182477
232.434997	7612.366611	27.187495
232.964620	7619.573288	27.192512
233.182065	7634.516189	27.197530
233.641640	7652.032019	27.202548
233.966573	7662.326768	27.207565
233.741567	7668.613026	27.212583
234.306366	7680.653921	27.217600
234.287682	7693.446049	27.222618
234.718700	7701.255412	27.227636
235.155979	7702.756070	27.232653
235.359633	7726.010484	27.237671
235.765145	7732.791510	27.242688
235.926578	7741.321883	27.247706
236.177032	7753.866683	27.252724
236.546543	7764.328143	27.257741
236.366042	7774.339075	27.262759
236.969475	7772.312561	27.267776
237.130939	7786.351973	27.272794
237.354649	7797.556096	27.277812
237.462777	7809.248731	27.282829
237.578920	7819.260572	27.287847
238.127759	7819.335723	27.292864
237.907408	7828.298477	27.297882
238.215387	7844.455454	27.302900
238.949398	7852.870925	27.307917
238.748311	7854.146424	27.312935
238.921539	7865.222744	27.317952
239.083380	7880.225067	27.322970
239.621695	7893.646726	27.327988
240.327640	7898.230795	27.333005
240.131766	7914.564635	27.338023
240.543461	7918.209804	27.343040
240.563043	7930.936117	27.348058
240.788031	7947.731284	27.353076
241.292343	7950.989417	27.358093
241.461382	7964.879396	27.363111
241.845911	7968.030014	27.368128
241.872685	7983.719722	27.373146
242.008132	7992.184827	27.378164
242.326911	7994.682765	27.383181
242.451849	8013.242683	27.388199
242.874057	8015.790720	27.393216
243.108275	8033.408515	27.398234
243.047393	8039.994367	27.403252
243.349472	8051.691500	27.408269
243.494389	8067.564824	27.413287
243.795083	8071.966171	27.418304
243.732059	8097.185494	27.423322
244.203754	8101.863139	27.428340
244.743516	8106.208100	27.433357
244.788406	8123.151609	27.438375
245.058486	8128.811131	27.443392
245.314532	8147.117019	27.448410
245.214531	8156.329430	27.453428
245.981656	8167.113996	27.458445
246.228869	8165.389499	27.463463
246.226574	8184.171574	27.468480
246.292530	8199.681687	27.473498
246.613470	8199.798858	27.478516
246.834132	8218.836494	27.483533
246.908127	8225.764350	27.488551
247.394563	8237.817888	27.493568
247.421205	8249.062629	27.498586
247.731174	8274.766786	27.503604
248.333940	8283.998610	27.508621
248.340461	8309.781924	27.513639
248.815156	8303.983817	27.518656
248.847089	8322.211331	27.523674
249.150821	8334.047298	27.528692
250.118429	8339.092472	27.533709
249.818386	8350.404237	27.538727
250.303707	8349.280163	27.543744
250.810739	8371.995354	27.548762
250.390395	8382.075758	27.553780
250.735565	8387.938282	27.558797
251.187678	8404.613042	27.563815
250.912462	8408.463789	27.568832
251.863619	8425.436089	27.573850
251.650602	8433.406642	27.578868
252.291045	8440.779399	27.583885
252.460076	8456.848181	27.588903
252.576197	8467.138206	27.593920
252.491593	8480.035918	27.598938
252.698164	8485.926500	27.603956
253.043094	8497.203616	27.608973
253.442535	8524.984142	27.613991
253.674080	8527.625264	27.619008
254.280501	8550.148303	27.624026
254.331574	8554.945629	27.629044
255.271890	8568.573165	27.634061
255.021949	8592.120730	27.639079
255.015627	8589.397203	27.644096
255.383701	8594.024907	27.649114
255.388769	8615.003658	27.654132
256.100788	8616.126694	27.659149
256.249886	8626.013838	27.664167
256.363650	8634.596293	27.669184
256.779949	8658.876225	27.674202
256.909565	8667.885589	27.679220
257.352681	8671.952207	27.684237
257.529691	8688.351444	27.689255
257.414132	8695.893250	27.694272
257.744688	8708.732399	27.699290
258.044622	8728.834745	27.704308
258.916457	8730.586293	27.709325
259.069611	8748.002779	27.714343
259.768736	8754.163578	27.719360
259.872110	8758.681245	27.724378
259.682851	8761.959774	27.729396
260.148370	8763.645532	27.734413
260.657997	8774.584454	27.739431
260.890704	8781.130891	27.744448
260.985971	8781.943277	27.749466
261.166794	8801.862300	27.754484
261.243994	8805.392716	27.759501
261.271169	8808.078522	27.764519
261.513753	8820.363233	27.769536
261.580639	8843.665737	27.774554
262.022367	8862.309482	27.779572
262.232024	8867.833465	27.784589
262.526479	8881.344563	27.789607
262.815846	8886.824493	27.794624
263.165166	8895.998455	27.799642
263.018187	8922.674904	27.804660
263.825364	8924.187180	27.809677
263.964072	8931.089376	27.814695
263.958540	8941.780748	27.819712
264.302382	8953.989697	27.824730
264.306735	8972.973593	27.829748
264.849402	8985.546071	27.834765
265.202176	8987.391587	27.839783
265.376955	9016.622490	27.844800
265.710275	9025.246505	27.849818
265.541992	9040.973979	27.854836
265.949109	9045.099994	27.859853
266.472359	9060.955947	27.864871
266.883917	9079.124735	27.869888
266.931672	9103.633477	27.874906
266.873631	9105.379183	27.879924
267.406588	9122.603920	27.884941
267.316163	9140.276783	27.889959
267.870752	9152.370760	27.894976
268.175085	9178.061269	27.899994
268.446110	9190.894292	27.905012
268.476431	9206.142461	27.910029
268.894667	9228.102238	27.915047
269.296967	9233.094144	27.920064
269.531806	9257.033886	27.925082
269.599228	9278.199369	27.930100
270.214446	9284.086178	27.935117
270.160243	9294.434918	27.940135
270.852634	9315.856157	27.945152
271.107968	9327.302523	27.950170
271.606610	9346.345132	27.955188
272.022975	9349.566778	27.960205
272.444153	9368.659433	27.965223
272.478511	9378.403930	27.970240
273.289370	9388.699297	27.975258
273.396541	9399.562715	27.980276
273.321219	9395.593270	27.985293
273.613764	9399.247930	27.990311
274.117351	9416.338619	27.995328
274.573816	9420.779034	28.000346
274.170864	9431.962339	28.005364
274.655674	9435.839472	28.010381
275.165233	9454.059580	28.015399
274.770122	9469.481958	28.020416
275.107299	9471.923544	28.025434
275.285237	9486.072171	28.030452
276.015540	9501.330906	28.035469
276.201740	9513.312333	28.040487
275.998328	9532.654552	28.045504
276.609100	9542.760336	28.050522
276.666043	9572.891469	28.055540
277.198057	9577.490583	28.060557
277.270713	9592.050451	28.065575
277.176199	9611.249398	28.070592
278.069218	9623.079126	28.075610
277.956931	9635.407338	28.080628
278.325452	9648.440105	28.085645
278.780701	9677.397623	28.090663
278.909951	9680.528540	28.095680
279.564273	9695.458343	28.100698
279.746499	9725.033344	28.105716
280.207020	9731.670725	28.110733
280.243035	9738.535634	28.115751
280.440602	9752.425642	28.120768
280.986111	9760.262149	28.125786
281.247062	9772.071008	28.130804
281.105681	9783.241963	28.135821
281.711102	9789.300968	28.140839
281.602280	9794.909849	28.145856
281.958696	9814.811924	28.150874
282.445266	9828.918778	28.155892
282.881200	9850.680763	28.160909
282.779859	9854.179357	28.165927
283.279522	9876.168191	28.170944
283.507035	9875.592759	28.175962
284.000891	9895.274475	28.180980
284.451575	9904.894038	28.185997
284.654893	9907.508207	28.191015
284.946497	9924.648360	28.196032
285.238139	9931.429092	28.201050
285.420093	9947.206658	28.206068
285.568839	9952.702619	28.211085
286.408467	9970.912574	28.216103
286.118996	9984.964301	28.221120
287.046472	9994.591314	28.226138
287.012963	9996.320631	28.231156
287.040215	9998.861357	28.236173
287.253037	10013.750070	28.241191
287.566163	10032.629842	28.246208
288.001259	10050.306495	28.251226
288.168531	10056.033233	28.256244
288.629939	10074.646699	28.261261
288.584360	10087.877255	28.266279
288.813068	10107.632306	28.271296
289.162965	10118.748604	28.276314
289.497462	10139.456447	28.281332
289.615357	10157.599673	28.286349
290.066367	10177.736756	28.291367
290.002289	10199.470122	28.296384
290.550575	10210.375423	28.301402
291.090756	10223.141737	28.306420
291.363821	10242.886824	28.311437
291.793029	10257.145076	28.316455
291.657256	10278.081457	28.321472
292.474268	10282.231949	28.326490
292.920508	10309.136356	28.331508
293.013571	10318.458521	28.336525
293.228340	10321.112002	28.341543
293.202466	10334.993242	28.346560
293.623436	10344.096706	28.351578
294.114714	10371.559335	28.356596
294.377396	10377.798524	28.361613
294.865316	10380.485004	28.366631
295.195778	10406.498336	28.371648
295.719119	10421.689211	28.376666
295.674753	10421.563669	28.381684
296.199279	10436.744899	28.386701
296.653612	10450.481535	28.391719
296.513507	10458.864633	28.396736
297.211865	10467.687894	28.401754
297.301207	10479.741951	28.406772
297.505543	10488.487893	28.411789
298.064187	10496.717343	28.416807
297.783409	10511.560634	28.421824
298.228681	10524.357810	28.426842
298.780769	10540.990415	28.431860
298.667300	10551.374395	28.436877
299.138330	10568.581758	28.441895
299.476278	10591.635591	28.446912
299.521365	10597.716332	28.451930
299.970108	10608.508003	28.456948
300.154104	10624.942586	28.461965
300.588405	10622.200258	28.466983
300.549778	10642.304032	28.472000
301.118585	10651.438167	28.477018
301.599926	10662.388953	28.482036
301.690045	10678.891967	28.487053
302.111013	10689.751187	28.492071
302.079788	10709.405504	28.497088
302.694105	10716.874838	28.502106
302.864660	10724.416849	28.507124
302.970382	10740.784857	28.512141
303.452814	10758.562123	28.517159
303.545276	10782.166168	28.522176
304.312025	10793.097583	28.527194
304.602535	10800.917643	28.532212
304.770806	10815.817132	28.537229
305.085654	10826.383615	28.542247
305.242319	10849.497740	28.547264
306.059259	10853.477867	28.552282
305.874821	10871.236561	28.557300
306.171864	10883.564626	28.562317
306.349116	10902.144492	28.567335
306.450197	10918.371293	28.572352
306.871254	10931.857734	28.577370
307.687665	10954.909689	28.582388
307.799348	10980.143437	28.587405
308.611940	10987.057664	28.592423
308.544926	11004.153944	28.597440
308.742287	11011.875011	28.602458
308.703558	11031.322440	28.607476
308.964743	11046.810657	28.612493
309.684793	11063.764753	28.617511
309.954694	11079.179007	28.622528
310.547939	11092.417560	28.627546
310.983052	11116.164121	28.632564
310.741096	11125.532853	28.637581
311.390855	11141.238147	28.642599
311.692633	11153.325670	28.647616
311.799675	11168.563423	28.652634
312.420944	11189.830612	28.657652
312.750611	11209.353137	28.662669
313.375165	11204.345333	28.667687
313.590547	11228.956910	28.672704
313.823087	11224.184178	28.677722
314.379021	11238.786456	28.682740
314.584409	11243.108762	28.687757
314.893378	11257.538181	28.692775
314.738199	11275.257940	28.697792
314.891628	11284.075382	28.702810
315.628464	11306.499239	28.707828
315.529749	11317.784414	28.712845
316.066071	11335.623256	28.717863
316.475765	11351.094777	28.722880
316.684388	11372.306824	28.727898
317.022301	11390.994629	28.732916
317.100690	11401.191142	28.737933
317.406364	11417.932598	28.742951
317.882673	11431.101296	28.747968
318.507362	11443.640490	28.752986
318.827924	11459.110274	28.758004
318.691301	11470.568835	28.763021
319.160061	11492.842291	28.768039
319.266094	11512.248596	28.773056
319.449698	11533.578421	28.778074
320.337037	11541.520021	28.783092
320.320521	11565.606300	28.788109
320.921178	11577.584125	28.793127
320.856174	11596.010010	28.798144
320.860383	11613.360932	28.803162
321.761717	11618.610027	28.808180
321.753332	11632.006361	28.813197
322.358424	11641.766838	28.818215
322.770883	11658.592827	28.823232
323.087505	11671.028863	28.828250
323.226254	11688.434563	28.833268
323.500219	11699.832104	28.838285
323.944358	11706.873788	28.843303
324.359956	11728.142231	28.848320
324.282634	11739.272737	28.853338
324.522791	11754.433274	28.858356
324.943164	11778.369288	28.863373
325.438227	11799.495898	28.868391
325.930122	11820.960904	28.873408
325.833427	11826.909525	28.878426
326.657024	11853.536002	28.883444
326.553992	11873.442771	28.888461
327.057301	11885.158163	28.893479
327.553632	11897.117801	28.898496
327.737159	11919.044886	28.903514
328.464981	11925.953799	28.908532
328.126286	11968.686974	28.913549
328.791174	11963.037949	28.918567
329.436723	11991.571369	28.923584
329.489499	11996.003015	28.928602
329.976397	12013.127122	28.933620
330.264150	12037.466328	28.938637
330.083926	12043.538624	28.943655
330.735769	12062.064242	28.948672
331.417151	12077.661165	28.953690
331.948796	12088.443864	28.958708
332.073884	12105.113173	28.963725
332.360217	12121.586720	28.968743
332.555043	12142.356552	28.973760
332.796633	12149.098566	28.978778
333.054494	12164.016670	28.983796
333.369946	12182.468791	28.988813
333.588715	12202.713906	28.993831
333.920936	12227.703211	28.998848
334.532322	12252.809867	29.003866
335.155890	12261.699382	29.008884
335.378544	12287.249069	29.013901
335.850921	12298.085383	29.018919
336.221398	12313.645944	29.023936
336.383472	12324.496144	29.028954
336.816832	12332.796559	29.033972
336.779987	12354.897616	29.038989
337.348624	12376.158608	29.044007
337.591268	12394.306561	29.049024
338.066938	12401.997237	29.054042
338.600957	12413.641835	29.059060
338.588499	12434.327620	29.064077
338.924804	12451.166250	29.069095
339.505256	12463.169913	29.074112
339.615329	12477.306170	29.079130
340.021608	12495.210697	29.084148
340.173963	12515.431815	29.089165
340.420429	12525.943655	29.094183
341.333048	12549.737229	29.099200
341.329267	12573.428071	29.104218
341.882265	12580.134091	29.109236
341.749471	12600.403125	29.114253
342.290680	12623.405511	29.119271
342.688054	12632.128532	29.124288
342.859054	12653.638439	29.129306
343.286596	12677.034481	29.134324
343.014918	12700.764289	29.139341
343.582651	12708.225934	29.144359
343.964006	12723.061979	29.149376
344.042044	12740.626581	29.154394
344.745548	12762.650036	29.159412
345.161353	12796.456423	29.164429
345.592171	12804.309026	29.169447
345.824960	12821.401043	29.174464
345.777933	12838.145329	29.179482
346.663052	12855.915192	29.184500
346.761530	12873.748294	29.189517
346.885291	12905.952204	29.194535
347.779444	12915.519645	29.199552
347.875985	12939.157335	29.204570
348.449817	12952.668669	29.209588
348.632881	12965.707538	29.214605
348.991040	12986.879033	29.219623
349.376766	13006.925172	29.224640
349.913663	13019.734967	29.229658
350.118358	13031.090481	29.234676
350.832647	13054.947341	29.239693
350.978149	13066.820573	29.244711
351.546955	13084.614938	29.249728
351.844731	13103.550735	29.254746
352.327871	13112.658444	29.259764
352.290015	13136.349012	29.264781
352.444546	13145.596634	29.269799
352.794008	13158.887469	29.274816
352.984140	13190.588828	29.279834
353.537131	13206.806812	29.284852
353.947975	13242.215853	29.289869
354.072207	13253.126201	29.294887
354.796093	13267.893229	29.299904
355.042001	13295.632262	29.304922
355.358095	13322.305579	29.309940
355.633980	13343.029297	29.314957
356.162267	13368.807315	29.319975
356.950896	13377.551502	29.324992
357.053326	13393.278104	29.330010
358.076003	13405.434157	29.335028
358.413926	13420.179656	29.340045
358.789233	13421.024172	29.345063
359.188419	13433.050534	29.350080
358.807300	13455.083641	29.355098
359.669683	13472.794489	29.360116
359.808944	13477.443469	29.365133
360.132168	13493.517686	29.370151
360.691180	13502.234740	29.375168
361.179168	13529.983566	29.380186
361.059877	13533.081427	29.385204
361.426627	13554.479588	29.390221
361.608179	13578.711096	29.395239
362.235991	13589.792238	29.400256
361.914139	13606.441299	29.405274
362.655461	13624.973390	29.410292
363.261979	13652.286969	29.415309
363.247517	13673.978673	29.420327
363.936694	13693.292716	29.425344
364.054107	13716.782836	29.430362
364.476202	13726.093045	29.435380
364.989476	13758.584773	29.440397
365.388094	13773.058922	29.445415
365.550503	13791.220784	29.450432
365.924069	13808.433753	29.455450
366.424828	13831.886074	29.460468
366.809871	13848.655155	29.465485
366.894578	13865.761836	29.470503
367.412285	13887.900978	29.475520
367.613175	13906.262196	29.480538
368.057512	13922.971525	29.485556
368.415903	13944.181951	29.490573
368.989309	13962.525927	29.495591
369.422017	13972.065135	29.500608
369.555436	13997.631109	29.505626
369.736705	14013.229026	29.510644
370.648237	14028.974687	29.515661
370.650022	14047.537767	29.520679
371.057359	14059.386398	29.525696
371.471075	14087.627704	29.530714
371.403959	14100.172824	29.535732
372.111574	14127.038593	29.540749
372.772037	14143.401610	29.545767
373.274459	14140.414417	29.550784
373.648289	14171.921260	29.555802
373.997380	14185.604481	29.560820
374.586846	14192.867512	29.565837
374.439921	14219.924115	29.570855
375.197395	14221.252003	29.575872
375.294050	14249.622168	29.580890
375.816113	14260.524466	29.585908
376.285790	14265.601918	29.590925
376.315318	14286.977934	29.595943
377.116520	14300.748325	29.600960
377.424712	14319.295255	29.605978
377.619546	14339.072685	29.610996
378.165922	14348.300571	29.616013
378.363924	14375.890779	29.621031
378.723855	14387.630190	29.626048
379.080163	14409.833120	29.631066
379.634378	14431.900857	29.636084
379.547261	14459.150553	29.641101
379.903688	14475.545691	29.646119
380.134350	14493.334344	29.651136
380.802866	14515.081090	29.656154
381.358223	14549.020335	29.661172
381.885507	14568.161665	29.666189
382.226895	14584.205537	29.671207
382.631182	14602.848227	29.676224
382.818345	14633.475518	29.681242
383.411540	14641.909826	29.686260
383.542539	14667.833955	29.691277
384.190372	14685.529018	29.696295
384.582832	14689.251182	29.701312
384.705677	14718.195891	29.706330
385.393404	14736.705885	29.711348
385.897379	14755.759468	29.716365
386.115839	14779.531943	29.721383
386.490614	14789.908089	29.726400
386.957933	14813.900599	29.731418
387.258709	14842.596551	29.736436
387.992976	14858.073798	29.741453
387.997389	14867.307875	29.746471
388.574430	14885.787979	29.751488
388.553001	14909.408699	29.756506
388.970373	14932.989138	29.761524
389.740917	14946.019459	29.766541
390.072382	14970.576663	29.771559
390.028724	14986.567491	29.776576
390.382334	15012.709878	29.781594
391.067326	15035.231568	29.786612
391.788171	15053.572454	29.791629
391.295065	15076.310311	29.796647
392.272919	15091.020036	29.801664
392.679270	15120.366261	29.806682
392.884110	15147.602788	29.811700
393.381294	15168.916012	29.816717
393.722105	15183.583471	29.821735
394.031875	15195.170166	29.826752
394.343024	15214.289153	29.831770
394.916465	15227.789543	29.836788
395.214855	15249.064513	29.841805
395.199376	15274.503925	29.846823
395.866482	15284.815601	29.851840
396.518627	15315.620657	29.856858
396.789267	15336.666357	29.861876
397.412385	15343.646630	29.866893
397.480434	15380.594593	29.871911
398.376808	15385.978191	29.876928
398.662282	15408.228121	29.881946
398.740610	15432.765563	29.886964
399.102194	15445.778171	29.891981
399.379255	15476.926488	29.896999
399.701975	15487.497510	29.902016
400.053423	15511.783822	29.907034
400.668014	15540.554841	29.912052
401.284541	15565.886168	29.917069
401.802214	15586.138605	29.922087
401.633197	15609.107419	29.927104
402.445303	15631.508836	29.932122
402.626105	15662.467240	29.937140
403.372419	15669.832606	29.942157
403.140566	15693.923106	29.947175
404.238389	15713.197305	29.952192
404.433573	15738.332715	29.957210
404.594384	15767.475199	29.962228
405.259235	15788.579666	29.967245
405.286414	15814.237356	29.972263
405.796984	15838.426516	29.977280
406.352539	15867.832635	29.982298
406.663280	15880.518713	29.987316
407.345253	15896.763012	29.992333
407.980609	15926.068286	29.997351
408.076214	15943.285665	30.002368
408.603873	15976.401126	30.007386
408.904852	15998.330314	30.012404
409.130651	16018.199383	30.017421
409.890963	16040.922076	30.022439
410.296969	16059.673306	30.027456
411.235366	16075.457522	30.032474
411.514868	16104.761958	30.037492
412.014619	16112.892557	30.042509
412.457523	16137.177971	30.047527
412.936528	16153.792234	30.052544
413.116757	16169.840573	30.057562
413.653906	16187.863897	30.062580
414.157510	16207.594895	30.067597
414.633812	16219.762548	30.072615
415.004717	16232.417327	30.077632
415.217269	16251.994977	30.082650
415.036084	16276.555196	30.087668
415.990013	16291.977094	30.092685
415.841803	16326.689819	30.097703
416.099130	16341.188053	30.102720
417.111962	16363.802090	30.107738
417.529290	16385.024949	30.112756
417.792862	16398.400989	30.117773
417.991676	16432.813187	30.122791
418.677974	16450.778654	30.127808
419.129397	16470.704446	30.132826
419.628498	16499.043332	30.137844
419.794704	16511.206048	30.142861
420.060417	16534.025750	30.147879
420.413925	16558.556270	30.152896
420.991414	16590.272086	30.157914
421.206222	16618.860982	30.162932
421.975120	16631.368404	30.167949
422.173846	16658.462742	30.172967
422.413825	16683.020679	30.177984
423.104927	16701.484674	30.183002
423.123646	16722.201807	30.188020
423.711312	16742.157077	30.193037
423.877710	16775.810600	30.198055
424.554401	16804.242143	30.203072
425.080868	16825.900065	30.208090
425.132473	16847.521843	30.213108
426.189891	16868.104862	30.218125
426.329982	16894.131649	30.223143
426.672298	16917.486237	30.228160
426.766287	16934.309936	30.233178
427.252356	16972.458905	30.238196
427.581088	16992.110708	30.243213
428.332492	17024.008464	30.248231
428.951408	17046.887158	30.253248
429.363409	17076.241808	30.258266
429.977212	17101.206036	30.263284
430.478317	17131.810250	30.268301
431.273368	17150.618476	30.273319
431.174402	17167.437856	30.278336
431.755134	17198.952016	30.283354
432.274302	17212.522325	30.288372
432.518510	17233.577403	30.293389
433.356685	17258.348760	30.298407
433.165588	17276.970444	30.303424
433.868199	17293.291662	30.308442
434.381574	17324.033238	30.313460
434.945985	17352.189426	30.318477
435.529319	17368.017692	30.323495
435.831231	17395.671774	30.328512
435.818359	17419.325820	30.333530
436.473330	17443.898689	30.338548
437.010046	17461.421052	30.343565
437.690040	17488.914970	30.348583
437.762012	17503.686329	30.353600
438.530145	17529.005977	30.358618
438.750236	17543.425665	30.363636
439.125474	17573.879728	30.368653
439.891702	17598.732283	30.373671
440.159006	17620.359043	30.378688
440.735549	17648.298973	30.383706
440.833973	17673.635267	30.388724
441.656055	17687.569093	30.393741
442.147292	17711.169805	30.398759
442.558895	17735.376853	30.403776
443.396338	17752.479651	30.408794
443.199419	17779.081601	30.413812
443.614759	17791.101865	30.418829
443.865396	17812.409263	30.423847
444.392642	17842.909431	30.428864
444.858965	17866.608996	30.433882
445.343851	17892.851611	30.438900
446.033995	17911.683332	30.443917
446.464374	17941.238576	30.448935
446.297247	17969.788215	30.453952
447.379983	17992.715415	30.458970
447.604149	18017.230144	30.463988
448.056326	18037.931331	30.469005
448.571583	18070.562730	30.474023
449.315479	18086.979235	30.479040
449.467868	18111.176815	30.484058
449.811358	18139.128687	30.489076
450.166790	18161.854133	30.494093
450.763449	18185.432593	30.499111
450.797985	18228.771971	30.504128
451.424454	18243.551805	30.509146
451.997054	18261.865286	30.514164
452.425546	18289.431325	30.519181
452.721152	18311.313444	30.524199
453.076339	18330.892972	30.529216
453.748295	18351.421083	30.534234
454.141135	18384.684991	30.539252
454.339262	18403.828009	30.544269
454.826595	18418.579229	30.549287
455.544541	18450.705699	30.554304
456.162503	18474.811856	30.559322
456.524118	18490.555737	30.564340
457.233050	18520.782127	30.569357
457.357014	18543.519004	30.574375
457.562960	18568.473201	30.579392
458.717438	18591.712078	30.584410
458.995776	18611.695622	30.589428
459.289927	18634.576526	30.594445
460.295958	18656.669961	30.599463
460.309518	18681.926098	30.604480
460.770241	18697.604083	30.609498
461.237437	18724.785616	30.614516
461.901555	18746.035593	30.619533
462.504145	18772.835876	30.624551
462.635411	18801.346314	30.629568
463.362429	18811.530475	30.634586
463.612277	18830.394149	30.639604
464.053890	18857.718866	30.644621
464.477342	18878.052702	30.649639
464.629466	18915.885059	30.654656
465.257507	18938.334956	30.659674
465.588855	18967.686153	30.664692
465.784086	18997.791578	30.669709
466.693955	19025.927679	30.674727
467.071287	19055.739323	30.679744
467.419068	19090.401417	30.684762
468.011346	19110.841728	30.689780
468.247093	19145.053946	30.694797
469.346228	19180.893675	30.699815
469.363659	19215.778316	30.704832
469.992229	19238.702318	30.709850
470.606393	19259.347847	30.714868
471.100464	19286.867122	30.719885
471.765492	19313.658371	30.724903
472.191255	19343.772447	30.729920
472.463396	19362.892180	30.734938
472.769040	19380.414566	30.739956
473.548427	19422.755424	30.744973
473.773210	19440.739104	30.749991
474.725969	19472.811532	30.755008
474.966382	19500.497198	30.760026
475.158224	19526.250893	30.765044
475.825566	19555.089135	30.770061
476.398109	19577.523191	30.775079
476.878207	19598.493343	30.780096
477.871459	19627.457549	30.785114
478.128847	19655.943162	30.790132
478.306967	19672.689716	30.795149
479.142602	19699.941263	30.800167
479.444248	19716.902273	30.805184
479.985385	19735.689609	30.810202
480.339442	19760.205142	30.815220
480.600444	19790.048765	30.820237
481.181310	19810.662187	30.825255
481.690699	19842.343450	30.830272
482.233286	19865.749195	30.835290
482.704379	19885.242635	30.840308
483.396735	19916.648955	30.845325
483.942943	19923.387071	30.850343
484.245435	19951.967141	30.855360
484.750590	19957.391214	30.860378
485.145265	19990.120536	30.865396
485.330699	20011.124648	30.870413
485.591939	20031.497732	30.875431
486.171852	20048.901943	30.880448
486.396826	20078.972785	30.885466
486.911087	20105.226421	30.890484
487.389493	20141.215687	30.895501
488.026808	20175.720630	30.900519
488.544549	20202.529852	30.905536
489.251849	20221.891858	30.910554
489.411022	20243.311015	30.915572
489.721797	20272.717940	30.920589
490.510090	20299.529147	30.925607
490.772135	20332.248223	30.930624
491.032162	20367.501285	30.935642
491.864045	20398.507431	30.940660
492.062243	20422.094149	30.945677
492.927250	20464.284852	30.950695
493.238832	20499.378437	30.955712
493.713370	20528.336771	30.960730
494.499951	20564.183770	30.965748
494.908877	20593.973857	30.970765
495.541659	20620.222257	30.975783
496.208457	20661.231311	30.980800
496.615979	20680.754456	30.985818
497.249232	20713.365479	30.990836
497.821782	20740.204763	30.995853
498.606471	20765.071117	31.000871
498.780239	20792.705863	31.005888
499.066080	20826.755214	31.010906
500.060738	20835.982356	31.015924
499.986431	20869.475305	31.020941
500.881738	20894.248677	31.025959
501.105064	20928.939837	31.030976
501.640457	20955.475632	31.035994
502.628881	20989.421540	31.041012
503.048455	21015.539585	31.046029
503.498752	21034.904739	31.051047
503.917609	21067.821625	31.056064
504.191015	21089.438640	31.061082
505.148205	21118.745586	31.066100
505.440340	21144.517290	31.071117
506.190868	21166.558821	31.076135
506.454888	21189.580122	31.081152
506.958713	21222.660877	31.086170
507.644162	21247.252735	31.091188
507.640693	21268.831172	31.096205
508.232363	21290.095269	31.101223
508.854620	21331.049512	31.106240
509.217762	21359.382026	31.111258
509.905108	21389.635196	31.116276
510.008117	21427.543276	31.121293
510.540995	21455.729290	31.126311
510.816245	21499.202483	31.131328
511.577987	21532.104352	31.136346
512.234832	21557.313984	31.141364
512.672954	21593.564964	31.146381
513.301891	21626.765812	31.151399
513.830469	21655.635200	31.156416
513.985511	21689.649660	31.161434
514.871192	21723.082160	31.166452
514.900861	21756.029558	31.171469
515.855027	21780.769556	31.176487
516.293702	21826.442054	31.181504
517.026834	21852.689021	31.186522
517.871530	21871.809984	31.191540
517.857600	21909.162298	31.196557
518.500801	21928.883562	31.201575
519.012446	21963.550340	31.206592
519.420100	21976.901330	31.211610
520.369794	21994.754853	31.216628
520.163215	22037.742327	31.221645
521.001270	22059.234054	31.226663
521.533855	22089.569407	31.231680
522.029766	22111.746659	31.236698
522.456666	22138.528518	31.241716
522.771871	22173.769849	31.246733
523.395181	22200.274595	31.251751
524.116683	22230.744865	31.256768
524.260327	22268.483902	31.261786
524.836573	22295.602756	31.266804
525.532680	22335.688152	31.271821
525.961297	22367.417729	31.276839
526.258183	22401.986215	31.281856
526.881944	22435.119725	31.286874
527.594481	22468.530056	31.291892
527.943328	22512.227747	31.296909
528.686326	22549.292103	31.301927
529.759114	22574.172492	31.306944
529.334654	22613.587219	31.311962
530.195725	22647.903475	31.316980
530.921416	22680.130456	31.321997
531.332830	22710.466781	31.327015
531.951254	22751.949046	31.332032
532.410890	22784.736025	31.337050
533.295278	22824.571755	31.342068
533.425127	22857.953944	31.347085
534.062397	22892.646905	31.352103
534.681405	22923.968410	31.357120
535.240330	22955.975515	31.362138
535.696677	23000.719048	31.367156
536.459981	23031.341980	31.372173
537.181083	23059.064783	31.377191
537.894065	23094.024279	31.382208
538.241717	23120.415453	31.387226
538.818064	23144.198959	31.392244
539.220564	23181.456847	31.397261
539.648991	23208.909741	31.402279
540.280707	23243.168164	31.407296
540.690233	23277.107572	31.412314
541.709451	23296.208902	31.417332
541.968702	23342.172078	31.422349
543.052953	23363.367578	31.427367
543.617482	23384.214796	31.432384
544.033901	23415.752063	31.437402
544.635130	23444.081866	31.442420
544.831628	23477.404101	31.447437
545.761434	23496.886145	31.452455
546.309777	23521.161069	31.457472
546.431255	23559.076646	31.462490
547.038388	23575.399121	31.467508
547.709531	23607.225398	31.472525
548.104964	23631.840371	31.477543
548.779247	23659.324893	31.482560
549.101180	23689.999012	31.487578
550.115074	23718.334086	31.492596
550.491637	23757.315966	31.497613
551.040081	23777.982856	31.502631
551.597153	23799.419374	31.507648
551.901228	23834.924486	31.512666
552.744003	23864.847449	31.517684
552.987710	23893.657284	31.522701
553.778591	23921.825357	31.527719
554.272495	23946.899249	31.532736
554.478210	23978.754781	31.537754
555.197837	24002.270416	31.542772
555.024054	24018.216331	31.547789
555.763817	24057.243022	31.552807
556.409765	24089.320474	31.557824
556.584451	24125.528865	31.562842
557.157714	24144.220583	31.567860
557.786267	24190.500718	31.572877
558.740505	24220.887037	31.577895
559.220109	24254.419007	31.582912
559.654900	24304.635192	31.587930
560.343625	24326.702567	31.592948
560.618226	24369.050946	31.597965
561.201226	24396.613977	31.602983
561.652846	24441.930240	31.608000
562.455352	24479.317489	31.613018
563.390560	24515.198927	31.618036
563.914563	24550.923647	31.623053
564.272770	24589.556129	31.628071
565.367939	24605.904127	31.633088
565.576032	24652.554524	31.638106
566.593495	24678.861813	31.643124
567.105882	24723.676267	31.648141
567.375095	24751.933535	31.653159
568.033015	24780.313234	31.658176
568.430035	24824.583533	31.663194
568.967405	24853.342436	31.668212
569.576028	24892.789437	31.673229
570.093582	24924.711387	31.678247
570.750754	24962.330850	31.683264
570.832561	25001.095889	31.688282
571.760986	25034.748462	31.693300
572.496957	25067.116729	31.698317
573.002476	25101.669855	31.703335
573.563205	25136.517742	31.708352
574.305114	25178.908397	31.713370
574.936946	25211.880946	31.718388
575.504636	25236.679468	31.723405
576.257863	25282.196864	31.728423
576.847629	25313.488781	31.733440
577.147822	25345.040974	31.738458
577.972323	25375.044899	31.743476
578.708161	25411.161403	31.748493
579.344664	25448.980930	31.753511
579.846831	25474.396715	31.758528
579.996013	25511.452141	31.763546
580.717429	25557.973684	31.768564
581.430830	25587.489735	31.773581
582.005345	25622.709180	31.778599
582.715474	25652.339598	31.783616
583.236363	25686.246690	31.788634
583.925802	25712.208558	31.793652
584.218965	25748.831075	31.798669
584.863837	25786.687847	31.803687
585.616927	25814.529546	31.808704
586.005754	25854.234057	31.813722
586.551150	25892.359406	31.818740
586.754976	25924.850319	31.823757
587.366032	25967.699210	31.828775
588.193380	25997.678339	31.833792
588.953557	26044.416135	31.838810
589.325346	26079.585969	31.843828
589.777943	26114.932810	31.848845
590.910753	26154.135866	31.853863
591.523267	26171.350752	31.858880
592.037071	26213.899393	31.863898
592.506811	26243.726333	31.868916
593.130134	26267.657880	31.873933
593.425558	26310.519012	31.878951
594.281888	26332.796191	31.883968
594.641498	26365.737424	31.888986
595.197995	26401.024252	31.894004
596.080279	26430.635173	31.899021
596.436449	26459.304668	31.904039
596.959655	26483.934730	31.909056
597.238426	26528.783468	31.914074
597.835811	26557.415324	31.919092
598.609752	26594.299046	31.924109
599.262001	26636.384480	31.929127
599.752449	26670.323273	31.934144
600.419574	26719.573699	31.939162
600.608080	26750.974934	31.944180
601.768275	26786.180526	31.949197
602.614215	26830.170030	31.954215
603.230569	26853.945356	31.959232
603.588447	26895.963667	31.964250
604.005981	26934.123647	31.969268
604.714442	26968.970525	31.974285
605.243603	27012.637138	31.979303
606.211592	27055.912781	31.984320
606.514046	27088.617647	31.989338
607.224252	27129.867060	31.994356
608.007261	27152.125027	31.999373
608.367136	27195.749023	32.004391
609.522057	27239.450850	32.009408
609.685341	27277.967317	32.014426
610.667816	27315.919448	32.019444
610.941455	27345.323652	32.024461
611.932337	27390.511519	32.029479
612.059447	27421.120707	32.034496
612.804592	27468.072721	32.039514
613.395139	27509.189954	32.044532
614.170268	27545.114506	32.049549
614.442236	27583.879992	32.054567
615.262242	27623.198094	32.059584
615.714938	27662.333617	32.064602
616.250572	27704.275195	32.069620
617.386837	27738.601314	32.074637
618.097027	27786.829973	32.079655
618.280184	27826.393581	32.084672
618.980321	27866.407230	32.089690
619.659261	27900.318559	32.094708
620.367712	27934.446546	32.099725
621.094466	27977.471185	32.104743
622.180660	28018.423333	32.109760
622.732741	28051.975544	32.114778
623.159179	28085.718145	32.119796
623.778105	28113.925340	32.124813
624.469942	28149.547971	32.129831
625.124000	28185.189222	32.134848
625.501754	28218.016844	32.139866
626.198630	28256.021782	32.144884
627.080376	28298.156885	32.149901
627.558592	28326.228392	32.154919
627.918336	28357.314531	32.159936
628.641253	28407.211345	32.164954
629.078215	28450.838597	32.169972
630.016475	28482.561215	32.174989
630.266236	28528.013056	32.180007
631.374668	28556.788923	32.185024
631.852971	28594.152394	32.190042
632.489455	28632.799575	32.195060
633.262668	28666.273918	32.200077
633.712799	28702.042822	32.205095
634.394279	28736.132129	32.210112
635.061178	28769.768672	32.215130
635.849355	28805.529061	32.220148
636.331739	28832.608230	32.225165
636.488038	28862.393288	32.230183
637.109790	28896.624956	32.235200
637.725599	28937.165907	32.240218
637.796989	28974.941452	32.245236
638.762728	29017.039600	32.250253
639.469796	29056.649955	32.255271
640.211665	29088.050298	32.260288
641.033215	29130.512594	32.265306
641.028359	29167.965422	32.270324
642.250751	29204.612978	32.275341
642.551844	29244.021794	32.280359
643.619261	29284.998389	32.285376
644.569775	29321.973181	32.290394
644.749331	29357.204067	32.295412
646.134423	29389.167847	32.300429
646.375359	29429.566207	32.305447
647.320076	29466.143940	32.310464
647.944882	29492.190300	32.315482
648.489484	29534.842193	32.320500
649.421491	29572.819075	32.325517
649.661141	29611.504966	32.330535
650.575546	29644.345646	32.335552
651.233661	29670.766286	32.340570
651.527922	29710.132817	32.345588
652.307806	29748.020066	32.350605
652.821280	29791.562333	32.355623
653.630031	29830.108938	32.360640
654.399270	29867.840045	32.365658
654.468477	29914.290377	32.370676
655.863245	29952.372483	32.375693
656.437254	29987.340392	32.380711
657.075729	30032.905360	32.385728
657.674198	30073.053029	32.390746
657.882538	30107.408352	32.395764
658.977323	30141.043347	32.400781
659.901391	30185.558838	32.405799
660.580987	30225.321141	32.410816
660.957259	30260.826188	32.415834
661.339478	30305.907220	32.420852
662.620688	30334.222359	32.425869
662.914916	30378.843228	32.430887
663.417428	30414.316126	32.435904
664.034071	30448.639680	32.440922
664.689175	30500.922729	32.445940
665.767594	30539.889895	32.450957
666.527310	30577.016936	32.455975
666.995260	30621.099085	32.460992
667.471916	30658.074635	32.466010
668.031335	30690.953617	32.471028
669.211630	30740.013249	32.476045
669.396816	30788.931729	32.481063
670.623958	30828.893913	32.486080
671.022570	30870.420916	32.491098
671.240182	30914.169923	32.496116
671.900228	30955.333755	32.501133
672.791939	30996.423459	32.506151
673.363599	31043.493011	32.511168
674.274670	31079.364542	32.516186
674.903584	31129.143608	32.521204
675.746704	31160.537579	32.526221
676.518055	31202.809720	32.531239
677.050307	31236.838040	32.536256
677.523805	31281.040836	32.541274
678.142058	31325.973335	32.546292
679.071783	31356.785091	32.551309
679.712459	31393.805807	32.556327
680.365676	31434.946375	32.561344
681.057560	31464.878894	32.566362
681.496330	31504.706659	32.571380
682.567112	31538.101145	32.576397
682.846531	31584.067136	32.581415
683.323818	31625.014371	32.586432
684.029579	31643.957759	32.591450
684.659708	31690.513881	32.596468
685.165754	31731.488431	32.601485
685.922774	31778.454761	32.606503
686.641160	31815.533599	32.611520
687.405163	31862.713967	32.616538
688.034029	31908.385718	32.621556
688.875171	31948.574884	32.626573
689.645339	31996.323556	32.631591
690.733946	32029.798228	32.636608
691.927725	32059.899559	32.641626
692.173311	32098.418474	32.646644
693.018208	32130.705027	32.651661
693.563557	32166.970777	32.656679
694.300882	32208.738219	32.661696
695.419985	32245.249315	32.666714
695.707843	32282.965386	32.671732
696.370847	32317.095116	32.676749
696.804361	32355.913818	32.681767
697.574964	32402.000673	32.686784
698.693046	32441.881898	32.691802
699.197133	32476.542537	32.696820
700.284101	32509.537766	32.701837
701.227400	32549.914400	32.706855
701.486765	32587.951586	32.711872
702.478124	32625.829953	32.716890
702.803127	32651.541601	32.721908
703.868103	32688.624616	32.726925
704.378081	32728.709099	32.731943
705.029471	32768.948531	32.736960
705.669862	32806.287911	32.741978
706.253692	32851.975105	32.746996
707.010107	32893.450112	32.752013
707.672213	32929.882246	32.757031
707.938771	32969.442638	32.762048
708.994301	33016.029934	32.767066
709.655317	33064.961429	32.772084
710.115276	33105.060788	32.777101
711.231578	33148.218547	32.782119
711.646315	33198.036099	32.787136
712.626105	33232.105071	32.792154
713.321749	33282.232877	32.797172
713.525350	33323.618286	32.802189
714.691455	33365.978412	32.807207
715.523152	33416.704818	32.812224
716.650989	33459.614844	32.817242
716.872783	33506.276897	32.822260
717.448755	33542.843711	32.827277
718.513168	33585.940954	32.832295
718.961407	33625.904052	32.837312
720.079409	33661.899368	32.842330
720.630167	33707.688443	32.847348
721.439054	33747.399300	32.852365
722.117343	33785.493179	32.857383
722.665031	33830.132322	32.862400
723.829117	33871.918448	32.867418
723.860542	33918.845158	32.872436
724.833479	33960.730942	32.877453
725.844024	33991.831098	32.882471
726.133907	34036.327700	32.887488
726.751282	34073.887908	32.892506
727.667682	34112.065218	32.897524
728.280965	34152.237404	32.902541
729.333935	34185.702150	32.907559
729.647785	34233.811904	32.912576
730.617547	34256.769080	32.917594
730.916141	34289.441681	32.922612
731.514739	34331.949535	32.927629
732.704881	34368.971670	32.932647
733.119766	34413.436847	32.937664
733.714306	34461.926780	32.942682
734.651438	34510.672982	32.947700
735.264824	34553.261161	32.952717
735.996854	34584.039097	32.957735
736.446661	34638.558620	32.962752
737.320420	34686.094878	32.967770
737.899460	34738.552194	32.972788
738.881606	34790.510247	32.977805
740.267160	34823.765859	32.982823
740.774540	34875.254715	32.987840
741.753347	34921.036299	32.992858
742.070239	34963.532635	32.997876
742.600928	35005.350653	33.002893
743.759676	35048.176888	33.007911
744.544989	35092.711940	33.012928
745.614665	35142.766635	33.017946
745.942689	35181.910574	33.022964
746.386329	35230.773656	33.027981
748.026704	35265.172433	33.032999
748.283207	35314.223086	33.038016
748.905342	35360.017214	33.043034
749.756630	35403.644741	33.048052
750.365504	35451.489762	33.053069
751.814305	35504.021428	33.058087
752.351033	35554.432442	33.063104
752.983300	35583.855381	33.068122
754.172105	35633.696571	33.073140
754.661261	35672.316667	33.078157
755.363514	35707.817845	33.083175
756.052304	35759.944355	33.088192
757.157211	35794.642832	33.093210
757.994047	35838.469531	33.098228
758.647736	35879.637710	33.103245
759.542276	35916.740469	33.108263
760.031759	35965.041635	33.113280
761.021965	35996.811859	33.118298
761.596357	36039.813811	33.123316
762.507936	36088.396927	33.128333
763.714580	36125.014883	33.133351
764.281879	36168.473469	33.138368
765.222121	36196.268249	33.143386
765.592323	36238.752467	33.148404
766.353976	36275.807109	33.153421
766.933160	36312.264398	33.158439
767.492238	36355.433788	33.163456
768.641216	36391.896832	33.168474
769.566130	36438.360392	33.173492
769.797688	36490.541324	33.178509
770.752380	36522.134523	33.183527
771.979366	36572.724403	33.188544
772.340788	36601.008719	33.193562
772.996828	36648.311572	33.198580
773.904631	36699.400688	33.203597
774.788314	36733.446107	33.208615
775.109891	36784.728401	33.213632
776.150856	36826.824201	33.218650
777.052025	36875.315894	33.223668
777.381394	36911.452897	33.228685
778.376098	36951.589629	33.233703
779.029761	36998.103209	33.238720
779.654803	37033.561780	33.243738
780.311508	37075.288255	33.248756
781.069943	37126.199434	33.253773
781.924568	37154.849889	33.258791
782.541850	37193.389443	33.263808
783.574159	37231.826135	33.268826
784.252848	37273.859404	33.273844
784.637409	37318.202613	33.278861
785.566599	37370.447179	33.283879
786.212923	37416.652968	33.288896
787.184141	37461.321956	33.293914
788.101245	37505.544218	33.298932
788.520649	37561.410250	33.303949
789.713336	37612.950174	33.308967
790.580782	37658.135383	33.313984
791.104106	37705.075618	33.319002
792.280028	37742.491614	33.324020
793.028689	37806.173267	33.329037
793.791828	37848.637090	33.334055
794.671581	37901.466141	33.339072
795.173000	37943.262889	33.344090
796.290013	37988.997814	33.349108
796.772622	38043.078252	33.354125
797.674356	38090.636705	33.359143
798.669240	38143.511559	33.364160
799.213434	38202.888344	33.369178
800.363697	38238.020037	33.374196
800.842960	38293.657266	33.379213
802.321984	38344.932779	33.384231
803.049140	38382.533995	33.389248
803.591155	38432.976263	33.394266
804.684381	38483.850885	33.399284
805.027376	38534.077926	33.404301
806.161843	38566.069691	33.409319
806.673483	38626.154684	33.414336
807.769025	38672.001931	33.419354
809.256419	38711.369183	33.424372
809.652051	38767.615175	33.429389
810.556741	38804.658121	33.434407
811.427254	38861.943002	33.439424
811.750189	38899.899319	33.444442
812.820838	38938.876925	33.449460
813.773978	38985.170840	33.454477
814.440793	39039.996455	33.459495
815.161042	39084.202199	33.464512
816.046858	39127.680144	33.469530
816.781623	39173.369936	33.474548
817.347794	39221.982626	33.479565
818.245257	39271.403617	33.484583
819.182748	39328.426284	33.489600
819.849007	39370.225280	33.494618
820.626092	39423.251212	33.499636
821.654014	39483.333629	33.504653
822.530767	39525.662808	33.509671
823.298371	39580.056616	33.514688
824.043034	39634.795656	33.519706
824.838839	39678.345720	33.524724
825.511010	39740.154134	33.529741
826.899548	39788.449594	33.534759
827.445237	39835.979108	33.539776
827.988540	39888.283881	33.544794
829.118922	39930.004954	33.549812
830.044769	39986.790857	33.554829
830.799060	40028.343339	33.559847
831.291025	40078.069988	33.564864
831.920132	40128.515216	33.569882
833.182796	40179.430539	33.574900
833.847590	40227.694851	33.579917
835.020718	40273.798966	33.584935
835.702481	40310.911021	33.589952
836.147945	40350.969341	33.594970
837.080371	40398.964448	33.599988
837.538624	40441.379919	33.605005
838.607847	40482.637304	33.610023
839.314218	40537.163259	33.615040
840.332384	40596.763306	33.620058
840.796204	40644.389622	33.625076
841.821395	40697.259648	33.630093
842.678381	40744.932134	33.635111
843.865713	40788.517980	33.640128
844.431974	40850.864738	33.645146
845.825874	40883.552952	33.650164
846.683857	40939.580378	33.655181
847.607918	40985.497320	33.660199
848.294467	41036.764169	33.665216
849.151277	41088.282758	33.670234
849.948375	41126.877063	33.675252
850.771798	41185.022937	33.680269
851.548629	41231.077293	33.685287
852.738472	41287.799948	33.690304
853.707315	41336.607292	33.695322
854.410761	41375.608829	33.700340
855.604379	41423.527343	33.705357
856.207636	41468.679654	33.710375
857.037671	41511.076933	33.715392
857.783862	41556.580200	33.720410
858.491115	41612.493808	33.725428
859.693101	41666.932324	33.730445
860.581352	41717.985768	33.735463
861.549807	41768.078057	33.740480
862.387173	41813.909118	33.745498
863.301503	41869.126854	33.750516
864.051383	41914.604987	33.755533
864.944272	41964.589387	33.760551
865.924465	42010.158151	33.765568
866.443604	42068.897951	33.770586
867.449620	42114.405964	33.775604
868.004184	42163.330618	33.780621
869.361445	42218.492525	33.785639
869.988507	42272.851800	33.790656
870.885511	42327.124664	33.795674
871.782090	42369.791480	33.800692
872.247245	42433.385602	33.805709
873.703504	42474.984617	33.810727
874.550810	42526.400548	33.815744
875.393068	42582.763533	33.820762
876.422428	42633.253058	33.825780
877.245838	42688.645213	33.830797
878.066346	42739.964639	33.835815
879.105752	42791.452309	33.840832
879.757209	42838.775703	33.845850
880.894060	42884.068745	33.850868
881.703629	42936.668006	33.855885
882.386711	42979.641413	33.860903
883.658126	43030.479777	33.865920
884.321948	43075.025015	33.870938
885.655756	43124.455972	33.875956
886.119255	43175.958816	33.880973
886.474600	43220.274342	33.885991
887.439020	43273.109490	33.891008
888.423457	43338.358007	33.896026
889.568616	43388.198606	33.901044
890.551890	43438.602312	33.906061
891.687913	43483.959967	33.911079
892.448167	43526.966631	33.916096
893.175253	43576.569506	33.921114
894.016462	43616.280849	33.926132
894.610088	43652.571093	33.931149
895.465799	43693.380906	33.936167
896.702499	43727.856420	33.941184
897.266789	43781.571402	33.946202
898.464971	43822.612467	33.951220
898.792987	43871.772463	33.956237
899.763261	43918.611795	33.961255
900.542315	43971.363778	33.966272
901.345654	44021.543969	33.971290
902.344837	44071.200226	33.976308
903.291127	44122.199542	33.981325
903.997473	44184.565419	33.986343
905.137247	44231.606587	33.991360
905.725664	44291.707739	33.996378
906.699591	44353.235181	34.001396
907.761972	44402.926562	34.006413
908.683147	44469.390156	34.011431
909.683167	44518.307194	34.016448
910.589785	44579.516872	34.021466
911.673273	44641.628883	34.026484
912.451592	44692.940459	34.031501
912.946169	44751.197819	34.036519
914.039562	44812.012004	34.041536
915.123290	44865.945570	34.046554
915.798671	44926.281514	34.051572
917.030092	44987.909553	34.056589
918.141358	45050.423196	34.061607
919.274081	45103.565279	34.066624
919.925886	45168.523335	34.071642
920.822135	45221.335834	34.076660
922.189993	45279.691884	34.081677
922.678828	45345.188357	34.086695
923.988243	45390.630292	34.091712
924.748931	45450.220501	34.096730
925.758787	45506.286325	34.101748
927.161014	45563.467457	34.106765
927.421080	45625.679506	34.111783
928.859635	45664.396372	34.116800
929.530069	45737.304775	34.121818
930.502337	45780.035880	34.126836
931.915323	45834.255500	34.131853
932.201186	45892.605441	34.136871
933.272299	45941.881368	34.141888
934.332068	45993.651607	34.146906
935.202798	46050.778034	34.151924
936.413905	46106.851804	34.156941
937.424685	46160.331789	34.161959
938.414319	46223.013247	34.166976
939.319938	46275.744524	34.171994
940.510902	46318.417107	34.177012
941.580418	46361.519983	34.182029
942.211142	46416.774449	34.187047
943.089895	46464.803776	34.192064
944.208996	46515.819449	34.197082
945.146650	46567.306477	34.202100
946.294053	46615.914021	34.207117
947.054485	46674.046177	34.212135
948.373003	46712.789979	34.217152
948.881457	46762.402525	34.222170
949.983498	46806.760070	34.227188
950.806130	46856.608308	34.232205
951.315037	46912.205698	34.237223
951.922312	46964.548793	34.242240
953.060755	47019.117919	34.247258
954.034057	47078.078154	34.252276
955.274486	47132.928921	34.257293
956.142355	47183.498319	34.262311
956.930300	47221.940169	34.267328
957.619602	47271.500211	34.272346
958.572528	47315.363345	34.277364
959.660172	47370.567581	34.282381
960.187673	47422.133432	34.287399
961.371453	47468.250859	34.292416
962.393446	47533.107160	34.297434
963.144732	47585.580975	34.302452
963.728669	47635.227901	34.307469
964.751295	47707.012028	34.312487
965.956791	47748.451389	34.317504
967.025266	47810.688384	34.322522
968.062130	47876.821286	34.327540
968.992698	47933.253519	34.332557
969.844653	47999.864913	34.337575
970.607616	48055.703694	34.342592
971.759767	48114.898012	34.347610
973.096273	48178.201193	34.352628
973.748028	48236.752949	34.357645
974.839068	48299.525509	34.362663
976.035331	48352.247752	34.367680
976.990276	48419.774263	34.372698
977.730994	48485.328966	34.377716
979.274275	48545.393181	34.382733
979.808382	48610.518748	34.387751
981.052047	48661.380566	34.392768
982.236591	48724.285171	34.397786
983.036190	48786.503667	34.402804
984.381341	48830.523426	34.407821
985.234269	48896.188276	34.412839
986.007409	48947.706468	34.417856
987.339427	49009.861189	34.422874
987.809607	49077.750254	34.427892
989.371584	49135.415233	34.432909
990.345828	49200.600103	34.437927
991.301389	49249.407829	34.442944
992.451295	49303.879419	34.447962
993.562233	49366.632819	34.452980
994.633293	49420.566592	34.457997
995.453102	49473.862851	34.463015
996.799514	49520.262668	34.468032
997.640968	49577.592366	34.473050
998.596049	49642.484128	34.478068
999.663439	49684.461124	34.483085
1000.683965	49740.187772	34.488103
1001.791214	49794.502707	34.493120
1002.686512	49851.274208	34.498138
1003.448997	49906.611424	34.503156
1004.849912	49952.060854	34.508173
1005.614465	50007.151233	34.513191
1006.659361	50059.787231	34.518208
1007.895154	50127.167245	34.523226
1008.745241	50178.081407	34.528244
1009.666784	50237.905753	34.533261
1010.141660	50296.515777	34.538279
1011.384182	50350.481835	34.543296
1012.522628	50405.748733	34.548314
1013.344757	50478.211998	34.553332
1014.427224	50525.895309	34.558349
1015.477121	50590.559774	34.563367
1016.585110	50654.747110	34.568384
1017.591763	50703.562581	34.573402
1018.578982	50758.999531	34.578420
1019.732118	50818.517050	34.583437
1020.373503	50886.087260	34.588455
1021.697939	50944.527950	34.593472
1022.638836	50992.436866	34.598490
1023.389520	51044.007564	34.603508
1025.006373	51090.558033	34.608525
1025.804214	51128.264604	34.613543
1026.764350	51164.832205	34.618560
1027.927177	51216.250176	34.623578
1028.921132	51266.492493	34.628596
1030.248952	51303.224205	34.633613
1031.257745	51348.763100	34.638631
1032.558191	51398.552760	34.643648
1033.051165	51438.288063	34.648666
1033.780929	51489.628914	34.653684
1035.138473	51532.361115	34.658701
1035.886600	51596.455549	34.663719
1036.747339	51645.238909	34.668736
1037.957723	51700.162283	34.673754
1039.223048	51762.214662	34.678772
1040.090290	51807.485554	34.683789
1041.339347	51861.669259	34.688807
1042.239758	51936.972244	34.693824
1043.089784	51977.557413	34.698842
1044.257227	52034.133480	34.703860
1045.133188	52084.807340	34.708877
1046.411125	52141.948512	34.713895
1047.262508	52199.213559	34.718912
1048.442510	52262.122213	34.723930
1049.091569	52331.315316	34.728948
1050.477559	52388.345261	34.733965
1051.627046	52452.531079	34.738983
1052.877910	52505.399832	34.744000
1053.978577	52563.582235	34.749018
1054.883805	52633.672636	34.754036
1055.904153	52682.167414	34.759053
1056.863572	52745.415643	34.764071
1057.827017	52804.923663	34.769088
1059.172871	52867.067626	34.774106
1059.893118	52932.479965	34.779124
1061.526289	52990.016879	34.784141
1062.640091	53051.710418	34.789159
1063.135454	53110.482530	34.794176
1064.455873	53169.366074	34.799194
1065.546054	53237.897970	34.804212
1066.886242	53295.563771	34.809229
1067.618479	53357.703862	34.814247
1068.640374	53429.480609	34.819264
1069.948321	53488.860494	34.824282
1070.752205	53552.711105	34.829300
1072.439930	53606.292301	34.834317
1073.365342	53679.211310	34.839335
1074.606490	53740.177980	34.844352
1075.829764	53780.979955	34.849370
1076.519868	53853.025098	34.854388
1077.635351	53915.404083	34.859405
1078.978848	53975.652917	34.864423
1079.830534	54036.472503	34.869440
1081.193852	54093.681018	34.874458
1082.002788	54148.812226	34.879476
1083.097448	54191.375304	34.884493
1083.778973	54257.398575	34.889511
1085.102132	54319.689163	34.894528
1086.206257	54389.823280	34.899546
1087.274407	54447.161135	34.904564
1088.618945	54511.056264	34.909581
1089.729115	54561.825380	34.914599
1090.556829	54619.486071	34.919616
1092.071578	54674.299168	34.924634
1092.658629	54746.046755	34.929652
1093.886093	54790.311437	34.934669
1095.336906	54847.843489	34.939687
1096.244216	54902.543382	34.944704
1097.007949	54942.362477	34.949722
1098.259963	54999.539991	34.954740
1099.513477	55036.093038	34.959757
1100.526514	55079.455225	34.964775
1102.051668	55127.382401	34.969792
1103.173090	55170.000014	34.974810
1103.747644	55225.505839	34.979828
1104.698456	55269.011014	34.984845
1106.145624	55324.095670	34.989863
1106.588268	55377.521438	34.994880
1108.397541	55436.043008	34.999898
1109.006412	55491.360555	35.004916
1110.204927	55545.965715	35.009933
1111.447975	55611.347936	35.014951
1112.295238	55660.648042	35.019968
1113.507430	55715.048935	35.024986
1114.772323	55778.092937	35.030004
1115.578078	55835.563837	35.035021
1117.002986	55894.450492	35.040039
1117.996741	55958.486721	35.045056
1119.068365	56013.530515	35.050074
1120.336514	56089.498026	35.055092
1121.429321	56145.234967	35.060109
1122.736015	56204.818072	35.065127
1123.527541	56268.007098	35.070144
1124.374859	56319.884366	35.075162
1125.770152	56392.516660	35.080180
1126.991087	56455.417447	35.085197
1128.260817	56518.861369	35.090215
1128.958422	56585.325285	35.095232
1130.357098	56652.116318	35.100250
1131.396739	56726.077408	35.105268
1132.993681	56787.983530	35.110285
1133.983156	56849.124184	35.115303
1135.062962	56915.522851	35.120320
1136.555360	56977.426845	35.125338
1137.831202	57038.668716	35.130356
1139.007740	57100.141477	35.135373
1139.861296	57163.348473	35.140391
1141.318295	57234.150913	35.145408
1142.312566	57286.216128	35.150426
1143.579100	57353.669039	35.155444
1145.030921	57408.631209	35.160461
1146.169728	57468.186786	35.165479
1147.145684	57519.489556	35.170496
1148.307942	57581.661987	35.175514
1149.365161	57637.445952	35.180532
1150.383673	57698.780429	35.185549
1151.894951	57763.183506	35.190567
1153.133136	57819.458553	35.195584
1154.448736	57875.860854	35.200602
1155.622956	57933.994305	35.205620
1156.865706	57987.212028	35.210637
1158.282642	58034.237933	35.215655
1159.125582	58092.164132	35.220672
1160.219170	58158.393188	35.225690
1161.076493	58209.519796	35.230708
1162.226145	58258.765254	35.235725
1163.271956	58320.729970	35.240743
1164.289287	58379.838454	35.245760
1165.422541	58438.245366	35.250778
1166.794623	58500.640493	35.255796
1167.802997	58553.168284	35.260813
1169.128072	58607.171987	35.265831
1170.077736	58677.716315	35.270848
1170.898427	58738.489444	35.275866
1172.207236	58800.104074	35.280884
1173.290537	58848.747169	35.285901
1174.722709	58908.583180	35.290919
1175.868212	58962.413247	35.295936
1176.906356	59008.006600	35.300954
1178.305961	59057.701927	35.305972
1179.248281	59115.906176	35.310989
1180.658319	59166.720416	35.316007
1181.678732	59220.709890	35.321024
1182.541757	59272.242941	35.326042
1183.514029	59333.430569	35.331060
1185.400560	59388.221598	35.336077
1186.233053	59448.336382	35.341095
1187.304688	59503.248916	35.346112
1188.565577	59568.373275	35.351130
1189.741460	59629.187972	35.356148
1190.155947	59690.679030	35.361165
1192.134052	59744.969146	35.366183
1193.266580	59822.368524	35.371200
1194.518627	59875.981388	35.376218
1195.468929	59942.915030	35.381236
1196.953871	60012.474285	35.386253
1198.393711	60080.135543	35.391271
1199.674921	60145.226615	35.396288
1200.423158	60199.197573	35.401306
1201.871321	60264.041283	35.406324
1203.200370	60329.498815	35.411341
1204.515174	60393.331986	35.416359
1205.449763	60465.529615	35.421376
1206.901660	60533.740941	35.426394
1208.543286	60600.928961	35.431412
1209.850140	60652.319490	35.436429
1210.703273	60703.654559	35.441447
1211.660628	60776.014117	35.446464
1212.886079	60833.975586	35.451482
1214.102121	60901.300686	35.456500
1215.492009	60973.972914	35.461517
1216.809351	61031.173526	35.466535
1217.643856	61107.769076	35.471552
1219.544475	61169.050182	35.476570
1220.968193	61222.791047	35.481588
1221.765699	61288.606549	35.486605
1223.269976	61350.893337	35.491623
1224.091341	61415.509057	35.496640
1225.453843	61480.236465	35.501658
1226.991043	61546.911698	35.506676
1228.097316	61610.926277	35.511693
1229.634454	61671.309688	35.516711
1230.575859	61741.313432	35.521728
1231.834308	61801.114102	35.526746
1233.192611	61862.722386	35.531764
1234.139184	61925.439768	35.536781
1235.680241	61984.968753	35.541799
1237.123780	62052.691848	35.546816
1238.416780	62103.752080	35.551834
1239.582193	62169.746559	35.556852
1240.603464	62223.495640	35.561869
1241.873181	62276.389334	35.566887
1243.073029	62350.196850	35.571904
1244.369282	62399.566985	35.576922
1245.371267	62472.994370	35.581940
1246.595481	62532.992083	35.586957
1247.689791	62604.791156	35.591975
1249.032908	62670.727500	35.596992
1250.260251	62736.137725	35.602010
1251.938509	62787.626504	35.607028
1253.048404	62850.276349	35.612045
1254.116900	62920.814285	35.617063
1255.416319	62971.318222	35.622080
1256.411449	63028.858781	35.627098
1257.868119	63081.819886	35.632116
1258.957352	63144.093876	35.637133
1259.976849	63195.996826	35.642151
1261.224263	63260.588650	35.647168
1262.454289	63296.239935	35.652186
1263.520467	63343.527225	35.657204
1264.108450	63421.371340	35.662221
1266.028805	63483.693328	35.667239
1267.376321	63551.847043	35.672256
1268.529746	63609.433801	35.677274
1270.129599	63679.808409	35.682292
1271.134950	63743.755667	35.687309
1272.346177	63802.486009	35.692327
1273.779784	63872.956825	35.697344
1275.194097	63931.649349	35.702362
1276.739691	63988.346264	35.707380
1277.975339	64055.151423	35.712397
1279.375428	64112.637422	35.717415
1280.348084	64179.192865	35.722432
1281.453945	64248.513194	35.727450
1283.014743	64315.382103	35.732468
1284.640772	64381.873789	35.737485
1285.987823	64452.505398	35.742503
1287.583553	64514.184387	35.747520
1288.452609	64576.129224	35.752538
1290.172892	64623.892656	35.757556
1291.089120	64701.771668	35.762573
1292.481628	64760.393580	35.767591
1293.686660	64828.763008	35.772608
1294.979422	64894.396565	35.777626
1296.338601	64951.681973	35.782644
1297.436656	65025.595643	35.787661
1298.714938	65084.489433	35.792679
1300.135872	65159.156993	35.797696
1301.204941	65224.756789	35.802714
1302.748054	65293.713994	35.807732
1303.836331	65368.738142	35.812749
1305.345347	65428.831183	35.817767
1306.976352	65508.569775	35.822784
1307.999292	65573.468611	35.827802
1309.490520	65644.650803	35.832820
1310.562810	65716.405271	35.837837
1312.151596	65784.185399	35.842855
1313.507433	65850.545993	35.847872
1314.454403	65933.495304	35.852890
1316.493254	65986.801949	35.857908
1317.595529	66054.658960	35.862925
1318.713304	66119.955886	35.867943
1320.188881	66182.544153	35.872960
1321.414367	66250.838256	35.877978
1322.890708	66321.847407	35.882996
1324.131346	66391.747679	35.888013
1325.639815	66457.554137	35.893031
1326.989357	66521.612856	35.898048
1328.181138	66588.912786	35.903066
1329.847461	66649.655234	35.908084
1330.971495	66715.927752	35.913101
1332.384791	66775.754063	35.918119
1333.728510	66842.074830	35.923136
1334.832116	66906.173017	35.928154
1336.371519	66970.152494	35.933172
1337.713741	67031.769685	35.938189
1339.063316	67099.375504	35.943207
1340.244792	67160.290043	35.948224
1341.279787	67225.121568	35.953242
1342.541587	67293.425450	35.958260
1343.975464	67351.888604	35.963277
1345.615626	67413.523396	35.968295
1346.476236	67473.494847	35.973312
1347.826379	67527.159476	35.978330
1348.859514	67582.437760	35.983348
1349.927041	67647.347575	35.988365
1351.497072	67708.037975	35.993383
1352.589800	67767.378602	35.998400
1353.630318	67839.390967	36.003418
1355.177131	67903.061370	36.008436
1356.464871	67971.793561	36.013453
1357.996938	68050.352583	36.018471
1359.460996	68124.933465	36.023488
1360.425020	68195.768428	36.028506
1362.335603	68269.165436	36.033524
1363.492294	68339.862997	36.038541
1364.806217	68411.916484	36.043559
1366.840265	68492.665086	36.048576
1368.023791	68561.016260	36.053594
1369.682518	68625.987973	36.058612
1370.915750	68694.059448	36.063629
1372.557840	68760.902025	36.068647
1373.870451	68824.066827	36.073664
1375.232473	68892.694875	36.078682
1376.360622	68959.878028	36.083700
1378.135760	69027.852894	36.088717
1379.489024	69098.547095	36.093735
1380.915897	69163.797076	36.098752
1381.814112	69241.078567	36.103770
1383.768506	69301.807550	36.108788
1384.904867	69367.312478	36.113805
1386.722485	69440.106834	36.118823
1387.948805	69511.011997	36.123840
1389.291888	69584.102663	36.128858
1390.869235	69654.915280	36.133876
1392.069369	69723.520218	36.138893
1393.541798	69809.876183	36.143911
1395.070386	69877.011701	36.148928
1396.479439	69950.118401	36.153946
1398.036896	70012.133307	36.158964
1399.212101	70073.802931	36.163981
1400.662816	70151.120962	36.168999
1402.300006	70227.396866	36.174016
1403.532052	70303.850393	36.179034
1404.885902	70363.377747	36.184052
1406.292621	70428.798709	36.189069
1407.542758	70499.715508	36.194087
1409.143397	70575.947496	36.199104
1410.272652	70662.853936	36.204122
1411.736512	70725.683078	36.209140
1413.236962	70799.385770	36.214157
1414.692313	70878.845599	36.219175
1415.969213	70953.660235	36.224192
1417.724557	71017.976915	36.229210
1419.002578	71088.004398	36.234228
1420.311087	71159.129156	36.239245
1421.927601	71243.035628	36.244263
1423.812472	71315.172455	36.249280
1425.058154	71381.431580	36.254298
1426.594479	71440.907499	36.259316
1427.728875	71517.734487	36.264333
1429.462846	71576.736495	36.269351
1430.795893	71654.520679	36.274368
1431.975769	71721.892843	36.279386
1433.760468	71785.966176	36.284404
1435.106127	71850.652998	36.289421
1436.404658	71922.123352	36.294439
1437.878635	71984.928604	36.299456
1439.200419	72049.581656	36.304474
1440.996344	72112.020181	36.309492
1442.256318	72158.102884	36.314509
1443.290147	72216.000030	36.319527
1444.722101	72272.441772	36.324544
1445.772698	72333.034320	36.329562
1447.161028	72394.004775	36.334580
1448.474828	72455.354342	36.339597
1449.651605	72532.582960	36.344615
1451.292746	72593.577633	36.349632
1452.410688	72669.979924	36.354650
1453.702004	72741.453629	36.359668
1455.250392	72819.486193	36.364685
1456.642257	72896.365560	36.369703
1458.172724	72967.181814	36.374720
1459.774441	73055.871430	36.379738
1461.280590	73139.598564	36.384756
1462.263946	73220.621265	36.389773
1463.949900	73300.824938	36.394791
1465.491398	73373.831782	36.399808
1467.276112	73467.788566	36.404826
1469.022784	73546.906856	36.409844
1470.469742	73623.716376	36.414861
1471.675385	73707.277010	36.419879
1473.425359	73784.609547	36.424896
1474.799278	73877.808767	36.429914
1476.257240	73955.111508	36.434932
1477.761732	74040.247705	36.439949
1479.261429	74112.148473	36.444967
1481.417766	74202.857734	36.449984
1482.544515	74283.975221	36.455002
1484.407043	74355.389191	36.460020
1486.078822	74433.280511	36.465037
1487.311987	74516.307371	36.470055
1489.005574	74590.725075	36.475072
1490.965606	74660.819931	36.480090
1492.367622	74733.852332	36.485108
1494.033491	74804.297609	36.490125
1495.479650	74875.309468	36.495143
1496.860878	74941.264937	36.500160
1498.236274	75015.024281	36.505178
1499.528953	75088.682772	36.510196
1501.490643	75172.484317	36.515213
1502.539906	75250.146108	36.520231
1504.392116	75313.685380	36.525248
1505.924192	75395.388804	36.530266
1507.539382	75476.015429	36.535284
1508.928126	75544.352617	36.540301
1510.473065	75625.839385	36.545319
1512.156093	75688.139306	36.550336
1513.480077	75769.217739	36.555354
1514.920538	75842.424475	36.560372
1516.768909	75913.439456	36.565389
1517.893238	75990.318923	36.570407
1519.680951	76050.766533	36.575424
1521.062201	76129.518955	36.580442
1522.493008	76202.310153	36.585460
1524.358244	76279.403829	36.590477
1525.678804	76362.321360	36.595495
1527.333688	76423.385967	36.600512
1528.981927	76506.391994	36.605530
1529.759756	76579.172399	36.610548
1531.582388	76646.317044	36.615565
1533.371252	76732.303985	36.620583
1534.497013	76810.388983	36.625600
1536.064887	76885.643435	36.630618
1537.739587	76970.204872	36.635636
1539.251003	77029.494473	36.640653
1540.891583	77099.556998	36.645671
1542.521058	77157.358928	36.650688
1543.870838	77223.907614	36.655706
1545.167625	77277.011402	36.660724
1546.539477	77339.553847	36.665741
1547.896217	77408.192108	36.670759
1549.199637	77479.993228	36.675776
1550.618815	77547.988666	36.680794
1552.097025	77619.547438	36.685812
1553.852092	77696.738388	36.690829
1555.138615	77786.886420	36.695847
1556.863843	77856.101542	36.700864
1558.124654	77935.612797	36.705882
1559.553264	78026.271444	36.710900
1561.294018	78094.699305	36.715917
1562.685925	78181.614389	36.720935
1564.432896	78259.656973	36.725952
1566.057434	78353.592487	36.730970
1567.719115	78436.234896	36.735988
1569.073473	78522.434832	36.741005
1570.855432	78613.850899	36.746023
1572.723403	78704.062959	36.751040
1574.011556	78792.060373	36.756058
1575.545547	78881.793205	36.761076
1577.580419	78957.449004	36.766093
1579.237059	79052.091323	36.771111
1580.807107	79131.899692	36.776128
1582.698836	79210.150354	36.781146
1584.233611	79291.117566	36.786164
1586.137756	79382.124322	36.791181
1587.737534	79454.771039	36.796199
1589.456704	79532.783574	36.801216
1590.972008	79616.136553	36.806234
1592.882759	79700.099350	36.811252
1594.639878	79761.396118	36.816269
1596.357997	79848.962196	36.821287
1598.100804	79921.258354	36.826304
1599.728415	79990.190059	36.831322
1601.106618	80072.704363	36.836340
1603.092962	80137.234745	36.841357
1604.525023	80211.721399	36.846375
1606.062415	80293.831366	36.851392
1607.929119	80362.650559	36.856410
1609.276834	80448.882871	36.861428
1610.839289	80520.626024	36.866445
1612.472634	80594.689447	36.871463
1613.621979	80671.806148	36.876480
1615.401392	80747.975592	36.881498
1616.874854	80840.346822	36.886516
1618.656479	80916.896468	36.891533
1620.301409	80999.840546	36.896551
1621.805012	81074.280297	36.901568
1623.412894	81161.918432	36.906586
1625.241897	81243.047992	36.911604
1626.648846	81326.663771	36.916621
1628.350687	81406.356681	36.921639
1629.820917	81485.972036	36.926656
1631.503081	81561.500083	36.931674
1633.043175	81654.154974	36.936692
1634.933664	81725.520458	36.941709
1636.496399	81821.263828	36.946727
1637.658389	81908.746020	36.951744
1639.536854	81989.578585	36.956762
1641.015877	82075.934720	36.961780
1642.796777	82153.501463	36.966797
1644.704512	82238.878750	36.971815
1646.041476	82321.228747	36.976832
1647.863706	82411.573999	36.981850
1649.416238	82499.453028	36.986868
1651.056999	82560.609432	36.991885
1652.667373	82628.638065	36.996903
1654.361659	82697.565998	37.001920
1655.945116	82758.212312	37.006938
1657.005004	82835.260249	37.011956
1658.661284	82903.472415	37.016973
1660.148646	82989.830036	37.021991
1661.800761	83062.110476	37.027008
1663.247055	83144.357062	37.032026
1664.639677	83230.844278	37.037044
1666.670768	83309.832160	37.042061
1668.435482	83401.241235	37.047079
1670.079131	83491.453159	37.052096
1671.822064	83574.275429	37.057114
1673.441880	83665.175855	37.062132
1675.315539	83754.997832	37.067149
1676.850459	83837.967461	37.072167
1678.788085	83916.426805	37.077184
1680.729395	84007.835530	37.082202
1682.200076	84092.501192	37.087220
1684.444035	84179.783034	37.092237
1685.922661	84268.464699	37.097255
1687.761264	84350.526654	37.102272
1689.508327	84431.006603	37.107290
1691.296486	84526.419700	37.112308
1692.727577	84594.620473	37.117325
1694.366648	84694.821850	37.122343
1696.269122	84781.778830	37.127360
1698.176376	84862.665745	37.132378
1699.440492	84959.809572	37.137396
1701.649174	85037.329897	37.142413
1703.105762	85125.029284	37.147431
1705.075603	85211.204060	37.152448
1707.211136	85298.341545	37.157466
1708.509664	85401.437102	37.162484
1710.564840	85481.909788	37.167501
1711.992414	85566.916001	37.172519
1713.637344	85647.947548	37.177536
1715.373495	85733.007330	37.182554
1716.794808	85819.383813	37.187572
1718.898411	85916.247413	37.192589
1720.690363	86006.329979	37.197607
1722.120786	86095.709089	37.202624
1724.134731	86181.664435	37.207642
1725.533619	86278.487469	37.212660
1727.751058	86360.217073	37.217677
1729.397762	86457.382081	37.222695
1731.327442	86550.156598	37.227712
1733.112728	86629.622927	37.232730
1734.677000	86715.637553	37.237748
1736.341025	86803.740407	37.242765
1738.360144	86893.878877	37.247783
1739.933212	86974.469170	37.252800
1742.047795	87054.176584	37.257818
1743.311117	87153.469496	37.262836
1745.000701	87239.808209	37.267853
1746.547591	87328.399855	37.272871
1748.547606	87417.237669	37.277888
1750.738946	87494.691246	37.282906
1752.110882	87593.563130	37.287924
1753.698617	87669.641616	37.292941
1755.650243	87763.886572	37.297959
1756.849252	87857.730033	37.302976
1759.441445	87937.441145	37.307994
1760.692420	88036.612248	37.313012
1762.484449	88124.699043	37.318029
1764.207862	88205.864812	37.323047
1765.759988	88303.709731	37.328064
1767.874802	88376.590040	37.333082
1769.320204	88448.776896	37.338100
1770.743113	88524.528545	37.343117
1772.472658	88596.595258	37.348135
1773.897053	88682.371405	37.353152
1775.801178	88756.312139	37.358170
1777.126452	88854.739323	37.363188
1779.102968	88944.992139	37.368205
1780.916705	89035.321395	37.373223
1782.616841	89124.502771	37.378240
1784.843438	89206.872538	37.383258
1786.112142	89312.787304	37.388276
1787.718802	89399.043931	37.393293
1789.838978	89500.086295	37.398311
1791.213215	89601.372469	37.403328
1793.415662	89695.533638	37.408346
1794.907316	89794.318098	37.413364
1796.632590	89892.179178	37.418381
1798.917819	89995.326544	37.423399
1800.629904	90096.320729	37.428416
1802.484069	90194.264018	37.433434
1804.014030	90299.038789	37.438452
1806.254374	90404.906764	37.443469
1807.916179	90502.526299	37.448487
1810.049193	90618.043899	37.453504
1812.065846	90707.687427	37.458522
1813.981585	90809.640708	37.463540
1815.910567	90913.214528	37.468557
1817.578263	91004.396403	37.473575
1819.109231	91106.524968	37.478592
1821.368263	91202.988698	37.483610
1823.323382	91304.950168	37.488628
1824.956918	91410.599792	37.493645
1827.093923	91509.428319	37.498663
1828.766369	91615.047220	37.503680
1830.619234	91722.590097	37.508698
1832.468456	91828.815795	37.513716
1834.401344	91915.865111	37.518733
1836.277367	92018.652525	37.523751
1838.157784	92122.187392	37.528768
1840.090224	92227.514252	37.533786
1841.452301	92335.681108	37.538804
1843.323542	92449.459564	37.543821
1845.687577	92545.480206	37.548839
1847.406828	92656.266656	37.553856
1849.377817	92746.430362	37.558874
1850.856392	92860.119701	37.563892
1852.522154	92963.957191	37.568909
1854.839082	93068.897247	37.573927
1856.494746	93189.974890	37.578944
1858.609206	93284.034277	37.583962
1860.222864	93392.444353	37.588980
1862.266258	93502.169144	37.593997
1864.348465	93606.437971	37.599015
1865.876510	93712.973990	37.604032
1868.181793	93822.506842	37.609050
1869.881687	93920.131399	37.614068
1871.762616	94025.434485	37.619085
1873.596562	94130.580504	37.624103
1875.316972	94241.689380	37.629120
1877.089195	94342.498140	37.634138
1879.176115	94452.333585	37.639156
1880.827356	94551.995821	37.644173
1882.721403	94662.800179	37.649191
1884.605098	94777.928917	37.654208
1886.773553	94874.304340	37.659226
1888.372394	94972.632517	37.664244
1890.048381	95080.835959	37.669261
1892.176166	95165.797870	37.674279
1893.687348	95258.107028	37.679296
1895.479635	95342.006455	37.684314
1897.232644	95447.042849	37.689332
1898.939263	95534.302617	37.694349
1900.875116	95632.681551	37.699367
1902.485538	95743.496115	37.704384
1904.399347	95831.167951	37.709402
1905.644819	95943.181170	37.714420
1907.288560	96056.552187	37.719437
1910.007321	96173.824428	37.724455
1911.716629	96294.373407	37.729472
1913.202977	96409.430907	37.734490
1915.361973	96517.994737	37.739508
1917.072448	96646.670367	37.744525
1919.473023	96769.407409	37.749543
1921.032402	96897.068244	37.754560
1923.284858	97012.426388	37.759578
1924.813984	97133.260303	37.764596
1926.761753	97261.875957	37.769613
1928.726397	97389.183803	37.774631
1930.778956	97511.788041	37.779648
1932.271890	97644.203357	37.784666
1934.921574	97772.850695	37.789684
1936.920616	97910.157215	37.794701
1939.207314	98036.022813	37.799719
1940.608204	98162.116257	37.804736
1942.798666	98291.724938	37.809754
1944.892898	98422.439427	37.814772
1946.864165	98552.844089	37.819789
1948.829786	98679.459707	37.824807
1950.936361	98818.883069	37.829824
1952.946571	98932.447901	37.834842
1955.214745	99066.776168	37.839860
1957.173026	99194.840181	37.844877
1959.712192	99316.601898	37.849895
1961.523839	99445.488530	37.854912
1963.381395	99566.419719	37.859930
1965.485042	99692.561348	37.864948
1966.889694	99813.665754	37.869965
1969.308518	99930.047980	37.874983
1971.418505	100055.302601	37.880000
1973.186386	100188.534809	37.885018
1975.272277	100310.206395	37.890036
1976.842070	100449.898297	37.895053
1979.030787	100572.125279	37.900071
1981.456863	100694.607172	37.905088
1983.367970	100815.978379	37.910106
1985.815435	100934.679799	37.915124
1987.208005	101064.246992	37.920141
1989.541609	101184.311012	37.925159
1991.633760	101318.004232	37.930176
1993.785582	101436.119832	37.935194
1995.667561	101551.159234	37.940212
1997.188434	101682.268223	37.945229
1998.931749	101798.965692	37.950247
2001.259191	101930.329817	37.955264
2003.277739	102064.532057	37.960282
2005.096392	102196.623458	37.965300
2007.057638	102327.082902	37.970317
2009.041970	102452.036743	37.975335
2010.754164	102587.100477	37.980352
2012.750893	102724.503836	37.985370
2014.943256	102854.916525	37.990388
2016.334240	102988.498030	37.995405
2018.623153	103130.764050	38.000423
2020.632827	103254.968906	38.005440
2022.477895	103400.247034	38.010458
2024.119374	103515.318238	38.015476
2026.074998	103638.379196	38.020493
2028.060392	103757.695621	38.025511
2029.551640	103885.014249	38.030528
2031.755884	104012.348591	38.035546
2033.874528	104144.946015	38.040564
2035.365313	104278.897454	38.045581
2037.209519	104420.122784	38.050599
2039.238224	104574.937506	38.055616
2041.060110	104719.375474	38.060634
2042.970464	104863.280359	38.065652
2044.684101	105029.329793	38.070669
2046.947918	105172.293123	38.075687
2048.941764	105338.667944	38.080704
2051.046424	105499.599314	38.085722
2052.846902	105657.675370	38.090740
2054.780785	105825.646939	38.095757
2057.462168	105992.259748	38.100775
2059.236305	106159.040687	38.105792
2061.436394	106325.603635	38.110810
2063.689050	106492.564935	38.115828
2065.469985	106665.750743	38.120845
2067.591363	106832.074873	38.125863
2069.871118	107008.531950	38.130880
2071.948416	107179.670497	38.135898
2074.335121	107353.741386	38.140916
2076.651671	107524.210193	38.145933
2078.462358	107702.544854	38.150951
2080.364714	107870.518708	38.155968
2082.629784	108037.726507	38.160986
2084.705596	108219.889960	38.166004
2086.776319	108404.489883	38.171021
2089.378919	108574.310431	38.176039
2091.549393	108754.509023	38.181056
2093.767004	108916.580021	38.186074
2095.707013	109095.155223	38.191092
2097.648589	109276.685796	38.196109
2099.857873	109452.088450	38.201127
2101.929448	109633.144007	38.206144
2104.062114	109810.969883	38.211162
2106.563623	109984.516048	38.216180
2108.991019	110158.036621	38.221197
2110.845437	110320.424564	38.226215
2113.292656	110494.615811	38.231232
2115.180449	110663.848157	38.236250
2117.824657	110842.436184	38.241268
2119.822115	111010.372176	38.246285
2122.219092	111171.537775	38.251303
2124.388004	111337.850581	38.256320
2126.164290	111507.598986	38.261338
2128.541058	111672.143406	38.266356
2130.286718	111855.214343	38.271373
2132.629173	112004.154059	38.276391
2134.744902	112181.487180	38.281408
2136.783679	112357.945462	38.286426
2139.123605	112531.123507	38.291444
2140.934133	112701.417546	38.296461
2142.642791	112873.947748	38.301479
2145.098476	113049.722750	38.306496
2146.712182	113228.420498	38.311514
2149.423331	113411.500475	38.316532
2151.084953	113596.508473	38.321549
2153.238699	113770.863023	38.326567
2155.423998	113952.658265	38.331584
2158.016529	114136.191664	38.336602
2160.182783	114313.362443	38.341620
2162.123970	114493.486377	38.346637
2164.021594	114656.533968	38.351655
2166.074940	114819.164744	38.356672
2168.454797	114986.273036	38.361690
2170.585941	115122.296441	38.366708
2172.110311	115297.986999	38.371725
2174.241711	115464.286553	38.376743
2176.412608	115638.583880	38.381760
2178.666798	115794.275098	38.386778
2180.368825	115967.315568	38.391796
2182.438233	116153.528297	38.396813
2184.301683	116325.188038	38.401831
2186.600909	116514.271158	38.406848
2188.615768	116702.867009	38.411866
2190.464663	116896.398404	38.416884
2192.778551	117087.448115	38.421901
2194.989516	117281.077053	38.426919
2197.182007	117480.125942	38.431936
2199.245190	117691.689910	38.436954
2201.629134	117888.186870	38.441972
2203.739983	118094.063144	38.446989
2205.766681	118306.054833	38.452007
2208.114725	118524.326913	38.457024
2209.897546	118733.568585	38.462042
2212.568852	118940.947309	38.467060
2214.686981	119163.216573	38.472077
2216.880307	119372.283355	38.477095
2218.887876	119595.117858	38.482112
2221.690902	119815.761584	38.487130
2224.257652	120021.868664	38.492148
2226.444774	120233.173624	38.497165
2228.805813	120452.342580	38.502183
2231.321347	120666.744398	38.507200
2233.735476	120886.288051	38.512218
2236.211476	121095.078911	38.517236
2238.547285	121311.288323	38.522253
2240.684566	121515.719957	38.527271
2242.878043	121733.285928	38.532288
2244.956589	121941.915151	38.537306
2247.074893	122147.659646	38.542324
2249.495145	122364.863807	38.547341
2251.661773	122578.341200	38.552359
2254.087937	122796.384060	38.557376
2256.268979	123025.706088	38.562394
2258.832259	123237.919823	38.567412
2261.434637	123455.520097	38.572429
2263.014510	123670.490605	38.577447
2265.751569	123893.197339	38.582464
2267.795966	124121.709757	38.587482
2269.603111	124327.970904	38.592500
2272.211362	124544.497842	38.597517
2274.388670	124786.884721	38.602535
2276.406933	125003.798208	38.607552
2278.631454	125233.214844	38.612570
2281.177241	125452.864603	38.617588
2283.298215	125686.943281	38.622605
2285.297100	125917.261761	38.627623
2288.016966	126140.351457	38.632640
2289.900599	126377.084689	38.637658
2292.253079	126608.404738	38.642676
2294.547021	126843.896577	38.647693
2296.692333	127075.035973	38.652711
2299.217813	127312.828680	38.657728
2301.366067	127549.438417	38.662746
2303.760778	127781.405458	38.667764
2306.222153	128013.845480	38.672781
2308.322872	128260.413570	38.677799
2310.548218	128492.804364	38.682816
2312.595868	128733.065158	38.687834
2314.841334	128959.073531	38.692852
2317.199899	129182.286813	38.697869
2319.341591	129402.984958	38.702887
2321.621847	129614.108633	38.707904
2323.378622	129840.299660	38.712922
2325.607218	130058.741854	38.717940
2328.244666	130302.763720	38.722957
2330.005898	130524.491481	38.727975
2332.338808	130756.091165	38.732992
2334.643662	130998.836761	38.738010
2336.938772	131238.616180	38.743028
2338.908907	131491.174218	38.748045
2340.755729	131741.050374	38.753063
2343.078105	131993.974948	38.758080
2345.085512	132255.235922	38.763098
2347.695098	132526.935860	38.768116
2350.152000	132794.968935	38.773133
2351.993602	133062.427392	38.778151
2355.066437	133328.222940	38.783168
2357.307127	133605.456161	38.788186
2359.674690	133874.905550	38.793204
2362.223589	134140.216917	38.798221
2364.630697	134414.688284	38.803239
2367.208398	134695.263580	38.808256
2369.728254	134966.903661	38.813274
2371.922550	135237.682668	38.818292
2374.465698	135514.816937	38.823309
2376.217265	135812.139016	38.828327
2379.039156	136095.641480	38.833344
2381.207901	136378.765671	38.838362
2383.664092	136677.645514	38.843380
2386.203352	136957.669748	38.848397
2388.811776	137248.382545	38.853415
2391.389005	137539.203570	38.858432
2393.318417	137832.754625	38.863450
2395.897318	138121.218656	38.868468
2398.708910	138405.967871	38.873485
2401.156526	138696.461058	38.878503
2403.750474	138987.948386	38.883520
2406.529965	139283.431399	38.888538
2408.667135	139577.493860	38.893556
2410.750710	139865.335379	38.898573
2412.847162	140164.712556	38.903591
2415.419065	140462.494324	38.908608
2418.285613	140766.082377	38.913626
2420.904339	141051.778676	38.918644
2423.597958	141337.604550	38.923661
2425.802700	141635.489063	38.928679
2428.234484	141926.283538	38.933696
2430.565438	142221.309041	38.938714
2432.789468	142511.961815	38.943732
2435.594997	142805.571297	38.948749
2437.875540	143108.047213	38.953767
2440.203714	143395.008336	38.958784
2442.521061	143702.812604	38.963802
2444.998321	144004.425541	38.968820
2447.533591	144298.365330	38.973837
2449.813097	144603.198456	38.978855
2452.214020	144891.349807	38.983872
2454.937466	145194.619393	38.988890
2457.107487	145498.561199	38.993908
2459.887103	145797.916400	38.998925
2462.116595	146101.712870	39.003943
2464.752651	146387.716265	39.008960
2467.425992	146697.983397	39.013978
2469.461601	147008.529840	39.018996
2472.033111	147321.596291	39.024013
2474.184549	147614.574338	39.029031
2476.835795	147911.245585	39.034048
2479.122648	148207.277398	39.039066
2481.332923	148479.777524	39.044084
2483.576244	148765.944198	39.049101
2485.399293	149053.155515	39.054119
2487.906445	149347.204487	39.059136
2490.135889	149650.881854	39.064154
2492.464771	149955.015027	39.069172
2494.882225	150262.283996	39.074189
2497.008591	150588.589545	39.079207
2499.526052	150892.647692	39.084224
2501.499311	151224.604188	39.089242
2503.503015	151546.834613	39.094260
2505.670694	151896.421552	39.099277
2508.357212	152237.792823	39.104295
2510.953745	152593.702020	39.109312
2513.241413	152932.245719	39.114330
2515.816222	153293.608438	39.119348
2518.532941	153641.584390	39.124365
2520.728774	154007.999711	39.129383
2523.666304	154371.178572	39.134400
2526.278382	154719.812163	39.139418
2528.580160	155098.099741	39.144436
2531.510668	155464.295143	39.149453
2533.816570	155828.394383	39.154471
2536.534697	156195.732006	39.159488
2539.109869	156570.863446	39.164506
2541.845651	156948.104860	39.169524
2544.395479	157310.804020	39.174541
2546.825562	157692.058743	39.179559
2549.994879	158063.069599	39.184576
2552.765202	158433.942014	39.189594
2555.370267	158808.663786	39.194612
2557.843616	159180.805918	39.199629
2560.546184	159551.340215	39.204647
2563.432426	159925.567753	39.209664
2566.057792	160297.248459	39.214682
2568.197480	160674.783821	39.219700
2570.672490	161048.269858	39.224717
2573.369134	161424.948136	39.229735
2575.985079	161806.211745	39.234752
2578.745072	162186.363237	39.239770
2580.619880	162572.990702	39.244788
2583.388688	162958.185629	39.249805
2585.944139	163354.956950	39.254823
2588.493211	163742.019082	39.259840
2591.170941	164138.826764	39.264858
2593.818590	164542.992683	39.269876
2596.215141	164925.832265	39.274893
2598.339480	165332.154281	39.279911
2600.767795	165740.005546	39.284928
2603.619781	166151.017909	39.289946
2605.713892	166571.153226	39.294964
2608.566131	166976.609292	39.299981
2611.274701	167390.330433	39.304999
2613.650307	167800.766791	39.310016
2616.040450	168209.933546	39.315034
2618.800300	168648.755963	39.320052
2621.496951	169059.733389	39.325069
2623.853608	169489.253473	39.330087
2626.463940	169906.546995	39.335104
2629.477840	170337.848437	39.340122
2631.320644	170763.507432	39.345140
2634.435477	171206.390870	39.350157
2636.963366	171630.195354	39.355175
2639.597781	172067.318075	39.360192
2641.946022	172488.984120	39.365210
2644.456097	172936.479867	39.370228
2647.137620	173352.435248	39.375245
2649.590110	173777.367999	39.380263
2651.895181	174182.441012	39.385280
2654.625172	174601.392092	39.390298
2656.919926	175023.753033	39.395316
2659.822395	175452.560688	39.400333
2661.750022	175886.957920	39.405351
2664.508058	176306.472085	39.410368
2666.842144	176738.867351	39.415386
2668.843193	177189.602713	39.420404
2671.444410	177632.449695	39.425421
2674.412802	178092.029077	39.430439
2677.018460	178548.696147	39.435456
2679.927017	179008.442112	39.440474
2681.902115	179486.216378	39.445492
2685.024702	179949.083039	39.450509
2687.352411	180431.175594	39.455527
2689.728192	180910.850369	39.460544
2692.563327	181392.944811	39.465562
2695.031459	181907.481934	39.470580
2697.493553	182446.303686	39.475597
2700.015961	182948.697527	39.480615
2702.731617	183462.772546	39.485632
2705.725135	183957.224326	39.490650
2708.096687	184485.734234	39.495668
2710.876828	184988.174375	39.500685
2713.735413	185520.296392	39.505703
2716.731836	186027.508264	39.510720
2719.544420	186543.387172	39.515738
2722.452941	187070.454805	39.520756
2725.432275	187587.836675	39.525773
2728.473746	188110.291256	39.530791
2731.051895	188618.292021	39.535808
2734.295239	189137.087680	39.540826
2737.098765	189662.939553	39.545844
2740.164730	190175.824044	39.550861
2742.557941	190702.684627	39.555879
2745.206749	191222.446239	39.560896
2748.195298	191730.802890	39.565914
2750.909878	192260.591913	39.570932
2754.056042	192780.104568	39.575949
2756.832867	193308.770665	39.580967
2759.315644	193839.999638	39.585984
2762.403227	194365.903551	39.591002
2765.015859	194891.782231	39.596020
2767.865675	195412.748812	39.601037
2770.632065	195937.540636	39.606055
2772.987133	196466.005782	39.611072
2776.553401	196992.886370	39.616090
2779.058824	197525.345359	39.621108
2782.266225	198047.408750	39.626125
2785.086404	198575.249941	39.631143
2787.817634	199100.592065	39.636160
2790.877028	199620.473990	39.641178
2793.854680	200150.353434	39.646196
2796.124557	200682.326669	39.651213
2798.886568	201209.779231	39.656231
2801.187462	201733.647602	39.661248
2804.057932	202274.295700	39.666266
2806.225951	202817.595555	39.671284
2808.717549	203374.182789	39.676301
2811.678789	203920.105309	39.681319
2814.755203	204462.277164	39.686336
2817.543353	205013.513598	39.691354
2820.410132	205560.319133	39.696372
2823.189179	206112.576060	39.701389
2825.654973	206671.767624	39.706407
2828.315474	207220.006827	39.711424
2831.663738	207760.595055	39.716442
2834.505263	208300.196850	39.721460
2836.783760	208822.029414	39.726477
2839.678927	209352.581574	39.731495
2841.909475	209877.573820	39.736512
2844.435353	210402.165263	39.741530
2847.283674	210958.080546	39.746548
2849.470782	211497.232388	39.751565
2852.563069	212060.122979	39.756583
2855.077811	212616.830225	39.761600
2857.867764	213162.216168	39.766618
2860.718138	213752.634264	39.771636
2863.653645	214323.047293	39.776653
2866.294596	214906.285346	39.781671
2868.681554	215493.247529	39.786688
2871.697003	216073.304012	39.791706
2874.044571	216686.236682	39.796724
2876.618913	217284.070158	39.801741
2879.362187	217896.561375	39.806759
2882.192447	218528.753124	39.811776
2884.650271	219150.638948	39.816794
2887.820780	219786.589318	39.821812
2890.060390	220418.798992	39.826829
2893.363614	221069.057488	39.831847
2896.318704	221713.350095	39.836864
2899.166201	222371.505098	39.841882
2901.711263	223027.751584	39.846900
2904.695452	223697.469998	39.851917
2907.653604	224362.924762	39.856935
2910.679352	225037.412901	39.861952
2913.192520	225710.025104	39.866970
2916.282026	226387.424701	39.871988
2919.073821	227060.374200	39.877005
2922.113378	227751.042189	39.882023
2925.163811	228434.823680	39.887040
2928.041821	229128.386916	39.892058
2930.890555	229831.099714	39.897076
2934.463002	230520.971369	39.902093
2937.779899	231207.147983	39.907111
2940.343196	231902.714198	39.912128
2943.397971	232589.717848	39.917146
2946.323214	233284.057221	39.922164
2949.338796	233986.256703	39.927181
2952.299635	234686.888649	39.932199
2955.651483	235390.659180	39.937216
2958.581827	236083.011910	39.942234
2961.286888	236793.536814	39.947252
2964.234181	237498.204975	39.952269
2967.752551	238186.371630	39.957287
2970.889616	238890.371986	39.962304
2974.236445	239584.024078	39.967322
2977.477079	240284.346768	39.972340
2980.620081	240985.495819	39.977357
2984.007423	241672.302733	39.982375
2986.958785	242362.630754	39.987392
2989.930097	243043.554507	39.992410
2992.744121	243735.144695	39.997428
2995.526614	244431.691215	40.002445
2998.653751	245110.475766	40.007463
3001.341872	245826.567179	40.012480
3004.566819	246519.277802	40.017498
3007.580562	247213.212869	40.022516
3010.293605	247911.002735	40.027533
3013.681802	248591.994946	40.032551
3016.442571	249298.764325	40.037568
3019.287749	249998.379545	40.042586
3022.389679	250694.522363	40.047604
3025.122153	251407.764640	40.052621
3028.289830	252094.238265	40.057639
3030.954173	252782.337002	40.062656
3033.744379	253455.095691	40.067674
3036.570149	254127.185248	40.072692
3039.325033	254806.471275	40.077709
3042.263426	255478.511309	40.082727
3045.092042	256166.898071	40.087744
3047.902369	256864.149038	40.092762
3050.626020	257566.286749	40.097780
3053.579303	258268.867255	40.102797
3056.821226	258979.882408	40.107815
3059.057473	259697.857944	40.112832
3062.106889	260418.724594	40.117850
3065.377751	261154.715974	40.122868
3067.955016	261893.833632	40.127885
3071.149665	262632.138646	40.132903
3073.719449	263382.042373	40.137920
3076.988425	264134.396843	40.142938
3080.087644	264887.483637	40.147956
3083.297166	265646.008454	40.152973
3086.684775	266407.369788	40.157991
3089.512958	267182.324810	40.163008
3093.097838	267949.129433	40.168026
3096.154759	268720.455141	40.173044
3099.115038	269497.453370	40.178061
3102.515253	270274.173072	40.183079
3105.673062	271052.625654	40.188096
3108.577972	271837.257127	40.193114
3112.265692	272610.330465	40.198132
3115.859360	273398.700480	40.203149
3119.108686	274173.631391	40.208167
3121.944641	274951.464130	40.213184
3125.610062	275729.693112	40.218202
3128.704100	276506.124644	40.223220
3131.867116	277284.645652	40.228237
3135.050654	278076.996207	40.233255
3138.328561	278858.911867	40.238272
3141.559642	279645.067754	40.243290
3144.886131	280423.937620	40.248308
3148.268310	281210.637418	40.253325
3151.256195	281994.139936	40.258343
3154.129115	282782.527494	40.263360
3157.637166	283568.191438	40.268378
3160.973247	284366.722405	40.273396
3163.412748	285169.447185	40.278413
3166.612638	285959.778970	40.283431
3169.794116	286761.835578	40.288448
3173.364434	287559.200335	40.293466
3176.519569	288355.934720	40.298484
3179.725614	289163.112561	40.303501
3182.873399	289958.253943	40.308519
3185.865486	290763.210454	40.313536
3189.383337	291564.418126	40.318554
3192.455312	292366.319825	40.323572
3195.679940	293169.075707	40.328589
3198.887599	293982.410877	40.333607
3201.502903	294791.968384	40.338624
3204.913088	295609.133967	40.343642
3208.138855	296421.366138	40.348660
3211.120287	297250.228713	40.353677
3214.318281	298060.842400	40.358695
3217.364249	298890.406975	40.363712
3220.532271	299716.842841	40.368730
3224.376707	300535.823784	40.373748
3227.388143	301365.229318	40.378765
3230.439626	302186.822349	40.383783
3233.840342	303008.373416	40.388800
3237.004102	303832.614065	40.393818
3240.094217	304640.759382	40.398836
3243.120208	305441.591393	40.403853
3246.168531	306240.478133	40.408871
3249.310683	307019.665488	40.413888
3252.645721	307812.390334	40.418906
3255.830167	308607.232734	40.423924
3259.027178	309416.198038	40.428941
3262.029341	310207.057820	40.433959
3264.718586	311027.192613	40.438976
3268.117812	311835.628618	40.443994
3271.579723	312656.248855	40.449012
3274.531898	313487.492361	40.454029
3277.602522	314321.138802	40.459047
3280.837031	315161.139910	40.464064
3283.697734	316007.756908	40.469082
3287.173518	316859.515004	40.474100
3290.074539	317712.691654	40.479117
3293.111169	318582.680887	40.484135
3296.078289	319458.703241	40.489152
3299.202228	320343.057385	40.494170
3302.218488	321226.268211	40.499188
3305.406747	322117.046225	40.504205
3308.884013	323029.328354	40.509223
3312.040564	323928.953761	40.514240
3314.938655	324863.640359	40.519258
3318.373295	325783.251855	40.524276
3321.740289	326703.436604	40.529293
3325.204635	327630.892010	40.534311
3328.822600	328561.853685	40.539328
3332.500708	329494.483768	40.544346
3336.129658	330420.300198	40.549364
3339.436455	331361.493114	40.554381
3343.104869	332299.156297	40.559399
3346.344881	333234.960751	40.564416
3349.284345	334173.325678	40.569434
3352.919634	335121.958515	40.574452
3356.734718	336080.101867	40.579469
3360.055811	337016.102914	40.584487
3363.674560	337972.147431	40.589504
3367.172286	338919.764749	40.594522
3370.475027	339860.666223	40.599540
3373.815618	340825.200053	40.604557
3377.576477	341773.460919	40.609575
3380.834486	342725.020867	40.614592
3383.987551	343679.462162	40.619610
3387.484667	344629.106240	40.624628
3391.072342	345604.905524	40.629645
3394.215913	346549.986501	40.634663
3397.573676	347524.599598	40.639680
3400.945679	348486.528873	40.644698
3404.435397	349448.158141	40.649716
3407.874621	350438.672089	40.654733
3411.479565	351400.783572	40.659751
3415.171477	352354.485989	40.664768
3418.940151	353334.996797	40.669786
3422.476709	354289.831802	40.674804
3425.972749	355253.593261	40.679821
3429.556580	356216.880323	40.684839
3433.537300	357180.430329	40.689856
3436.657103	358134.528183	40.694874
3440.078708	359089.284188	40.699892
3443.357102	360046.795435	40.704909
3446.406861	361008.139360	40.709927
3450.115226	361976.522319	40.714944
3453.761809	362948.482368	40.719962
3457.598266	363898.660727	40.724980
3461.502811	364866.056460	40.729997
3464.854172	365821.215376	40.735015
3468.348414	366768.052373	40.740020
3471.978788	367676.464788	40.745024
3475.024148	368533.850424	40.750029
3478.237988	369351.172181	40.755034
3481.629389	370108.541023	40.760039
3484.584008	370806.413369	40.765044
3487.266867	371469.128596	40.770048
3490.153474	372034.329739	40.775053
3492.973014	372569.632527	40.780058
3495.781050	373044.218778	40.785063
3498.125769	373478.228591	40.790068
3500.350833	373844.305061	40.795072
3502.738123	374169.711623	40.800077
3504.566089	374440.465789	40.805082
3506.816339	374664.645106	40.810087
3508.739037	374843.790304	40.815092
3510.102218	374979.970463	40.820096
3511.869004	375086.852681	40.825101
3513.269302	375153.204406	40.830106
3514.548695	375175.888884	40.835111
3515.996239	375170.481335	40.840116
3516.549071	375135.014401	40.845120
3518.069427	375053.855858	40.850125
3518.959247	374975.665741	40.855130
3519.550541	374865.036590	40.860135
3520.499078	374727.046939	40.865140
3521.175804	374572.157679	40.870144
3521.590757	374374.179980	40.875149
3522.176601	374191.515591	40.880154
3522.301823	373982.785444	40.885159
3522.943492	373760.942679	40.890164
3523.005004	373522.475365	40.895168
3523.659432	373275.988290	40.900173
3524.134224	373025.564555	40.905178
3524.380252	372762.067344	40.910183
3524.563502	372484.428880	40.915188
3524.419327	372199.827969	40.920192
3525.091070	371908.238064	40.925197
3525.426298	371605.165126	40.930202
3525.064203	371305.881251	40.935207
3525.588669	370991.036109	40.940212
3525.522828	370672.875698	40.945216
3525.412585	370357.081112	40.950221
3525.568510	370027.574224	40.955226
3525.452056	369709.359972	40.960231
3525.441175	369371.208744	40.965236
3525.295476	369048.622079	40.970240
3525.641571	368715.081605	40.975245
3525.424312	368387.188989	40.980250
3525.489619	368043.344651	40.985255
3525.145668	367701.668814	40.990260
3524.713882	367377.634361	40.995264
3525.210124	367025.809133	41.000269
3525.063182	366696.107648	41.005274
3524.575878	366364.372228	41.010279
3524.774581	366024.395448	41.015284
3524.646510	365687.514647	41.020288
3524.623844	365354.602464	41.025293
3524.165716	365018.654759	41.030298
3523.972646	364687.794217	41.035303
3524.092325	364357.440016	41.040308
3524.028918	364023.070687	41.045312
3523.815486	363686.662852	41.050317
3523.553737	363359.583999	41.055322
3523.098325	363024.324431	41.060327
3523.300212	362702.425624	41.065332
3522.805818	362385.765054	41.070336
3522.984178	362057.662798	41.075341
3522.879449	361739.587654	41.080346
3522.342799	361419.264224	41.085351
3522.457274	361099.318379	41.090356
3522.170739	360782.532033	41.095360
3521.615901	360471.527390	41.100365
3521.655025	360164.340151	41.105370
3521.625475	359860.921563	41.110375
3521.399164	359550.288062	41.115380
3521.309084	359250.938854	41.120384
3521.259562	358942.939854	41.125389
3521.230987	358645.430231	41.130394
3520.576765	358335.893165	41.135399
3520.789908	358040.372954	41.140404
3520.282221	357747.707323	41.145408
3520.144423	357450.381052	41.150413
3520.055746	357163.947143	41.155418
3519.961024	356885.237661	41.160423
3519.955294	356588.314484	41.165428
3519.334365	356307.369278	41.170432
3519.366166	356012.213795	41.175437
3519.137879	355746.578602	41.180442
3518.851487	355472.308756	41.185447
3519.182277	355195.550879	41.190452
3518.423014	354920.638465	41.195456
3518.528600	354657.763061	41.200461
3518.354822	354388.752809	41.205466
3517.977412	354121.042955	41.210471
3518.181086	353858.425136	41.215476
3517.510864	353605.371693	41.220480
3517.979356	353343.928251	41.225485
3517.649437	353086.877707	41.230490
3517.316702	352833.714516	41.235495
3517.235721	352583.407655	41.240500
3516.880680	352333.827983	41.245504
3516.825518	352085.139978	41.250509
3516.973362	351840.764959	41.255514
3516.491948	351602.104103	41.260519
3516.523268	351354.184916	41.265524
3516.041279	351128.026979	41.270528
3515.855988	350875.943756	41.275533
3515.849907	350647.826995	41.280538
3515.659472	350411.272549	41.285543
3516.119769	350195.891448	41.290548
3515.506002	349960.035411	41.295552
3515.176677	349729.751167	41.300557
3515.118912	349515.082082	41.305562
3514.733230	349291.006243	41.310567
3514.696345	349076.483547	41.315572
3514.261223	348863.114828	41.320576
3514.128869	348651.832798	41.325581
3514.378505	348453.556427	41.330586
3514.254531	348235.991275	41.335591
3514.450693	348027.679090	41.340596
3513.912571	347828.251031	41.345600
3513.666123	347623.412069	41.350605
3513.609182	347417.576166	41.355610
3513.473351	347215.869786	41.360615
3513.007125	347021.942357	41.365620
3512.979914	346829.978999	41.370624
3513.145990	346635.569133	41.375629
3512.942068	346455.681777	41.380634
3512.623901	346270.319882	41.385639
3512.840867	346085.000420	41.390644
3512.834284	345896.308125	41.395648
3512.587168	345710.271026	41.400653
3512.406849	345527.705530	41.405658
3512.323618	345334.293238	41.410663
3512.180394	345159.601406	41.415668
3511.794817	344998.192613	41.420672
3511.937499	344818.267774	41.425677
3512.209048	344640.762594	41.430682
3511.487328	344471.573096	41.435687
3511.732038	344297.985727	41.440692
3511.417331	344132.773461	41.445696
3511.501278	343958.573881	41.450701
3511.346773	343799.462398	41.455706
3511.261100	343632.762681	41.460711
3510.860836	343462.322952	41.465716
3510.720832	343303.893395	41.470720
3511.088307	343139.688425	41.475725
3510.881294	342996.548749	41.480730
3510.561533	342836.212791	41.485735
3510.627683	342671.417059	41.490740
3510.460337	342521.404196	41.495744
3510.522080	342368.913951	41.500749
3510.345563	342228.512367	41.505754
3510.085831	342079.071417	41.510759
3510.447768	341921.574126	41.515764
3510.175033	341780.677249	41.520768
3510.243394	341628.920105	41.525773
3509.859550	341477.156719	41.530778
3509.684752	341341.175572	41.535783
3510.014239	341195.325636	41.540788
3509.473894	341063.240049	41.545792
3509.531746	340920.279281	41.550797
3509.410025	340773.303054	41.555802
3509.320437	340641.501396	41.560807
3509.297820	340507.578287	41.565812
3509.045599	340378.038697	41.570816
3509.155997	340241.729013	41.575821
3508.936563	340111.217065	41.580826
3509.032360	339987.520900	41.585831
3508.899088	339851.425805	41.590836
3508.861004	339723.121746	41.595840
3508.658232	339586.349942	41.600845
3508.233464	339473.667511	41.605850
3508.378335	339355.708275	41.610855
3508.333310	339241.287467	41.615860
3508.289641	339118.042369	41.620864
3507.907248	338998.308099	41.625869
3507.872692	338879.536197	41.630874
3507.814576	338773.837995	41.635879
3507.665532	338657.066702	41.640884
3507.517557	338556.493116	41.645888
3507.805662	338444.509720	41.650893
3507.911836	338339.343994	41.655898
3507.749617	338229.718954	41.660903
3507.501298	338111.588234	41.665908
3507.744591	338011.536829	41.670912
3507.666723	337891.217245	41.675917
3507.324137	337790.519370	41.680922
3506.948796	337686.367913	41.685927
3507.418974	337567.283908	41.690932
3507.343941	337483.199774	41.695936
3507.216302	337379.491874	41.700941
3507.312461	337287.370135	41.705946
3507.117023	337178.713440	41.710951
3507.231264	337058.284768	41.715956
3506.836921	336961.585196	41.720960
3507.043584	336871.937279	41.725965
3506.619727	336781.014485	41.730970
3506.469721	336689.743488	41.735975
3506.857493	336582.697665	41.740980
3506.221477	336502.310079	41.745984
3506.615817	336407.443878	41.750989
3506.371627	336302.886502	41.755994
3506.295947	336225.335217	41.760999
3506.589138	336129.365165	41.766004
3506.403490	336048.270406	41.771008
3506.104031	335954.732178	41.776013
3506.248788	335876.281047	41.781018
3506.130553	335780.832162	41.786023
3506.065525	335688.960479	41.791028
3505.449042	335608.796760	41.796032
3505.435996	335543.034237	41.801037
3505.895552	335463.515770	41.806042
3505.658748	335391.328453	41.811047
3505.813906	335307.788253	41.816052
3505.691496	335225.054197	41.821056
3506.116199	335143.658576	41.826061
3505.618234	335058.668610	41.831066
3505.747963	334989.322386	41.836071
3505.572497	334910.563229	41.841076
3505.499301	334844.630849	41.846080
3505.769005	334758.096011	41.851085
3505.603630	334679.233059	41.856090
3505.185849	334603.232322	41.861095
3505.113774	334524.583341	41.866100
3505.212250	334467.982344	41.871104
3505.392039	334391.048500	41.876109
3505.329371	334325.011826	41.881114
3505.074754	334245.678703	41.886119
3505.408340	334169.305293	41.891124
3505.237137	334103.844701	41.896128
3505.017771	334036.941896	41.901133
3504.997691	333966.040399	41.906138
3504.546003	333905.480851	41.911143
3505.012334	333830.739089	41.916148
3505.221050	333770.152372	41.921152
3505.036363	333698.487704	41.926157
3504.907593	333630.222095	41.931162
3504.700363	333574.837430	41.936167
3505.031300	333500.268774	41.941172
3504.617083	333444.204168	41.946176
3504.776492	333371.366050	41.951181
3504.758828	333311.348070	41.956186
3504.298470	333252.416509	41.961191
3504.856352	333188.366295	41.966196
3504.360776	333129.160288	41.971200
3504.516946	333066.291710	41.976205
3504.582651	333005.395495	41.981210
3504.290196	332959.840309	41.986215
3504.485432	332891.293811	41.991220
3504.442628	332833.542527	41.996224
3504.441161	332780.413489	42.001229
3504.495585	332722.875732	42.006234
3504.173665	332666.414046	42.011239
3504.422578	332603.123271	42.016244
3504.528862	332549.239504	42.021248
3504.238354	332494.552969	42.026253
3504.715443	332427.970787	42.031258
3504.271780	332372.316125	42.036263
3504.209983	332308.030672	42.041268
3504.186868	332262.407106	42.046272
3504.258672	332201.534081	42.051277
3504.376970	332149.809703	42.056282
3504.107018	332089.803797	42.061287
3504.152346	332039.108014	42.066292
3503.971360	331991.474129	42.071296
3503.902443	331930.953307	42.076301
3504.472171	331879.870126	42.081306
3503.527189	331834.313871	42.086311
3504.036989	331775.635278	42.091316
3503.715743	331733.542094	42.096320
3503.729201	331689.845082	42.101325
3503.748569	331638.695020	42.106330
3503.418614	331598.307107	42.111335
3503.967512	331546.107654	42.116340
3503.994684	331502.916960	42.121344
3503.735962	331452.751176	42.126349
3503.819664	331407.364227	42.131354
3503.649064	331373.004422	42.136359
3503.845957	331304.632850	42.141364
3503.839034	331267.653100	42.146368
3503.389863	331224.765470	42.151373
3503.499409	331176.576470	42.156378
3503.720925	331132.286746	42.161383
3503.577912	331078.541618	42.166388
3503.721018	331035.688351	42.171392
3503.502572	330999.250095	42.176397
3503.458384	330944.268490	42.181402
3503.390673	330907.526805	42.186407
3503.403572	330862.328322	42.191412
3503.482976	330828.157852	42.196416
3503.578744	330784.828457	42.201421
3503.439772	330743.951970	42.206426
3503.274276	330702.876112	42.211431
3503.237211	330655.472411	42.216436
3503.436065	330618.968555	42.221440
3503.364494	330577.725274	42.226445
3503.404169	330536.591729	42.231450
3503.375666	330507.855381	42.236455
3503.344374	330454.142785	42.241460
3503.025127	330413.294133	42.246464
3503.364951	330375.063895	42.251469
3503.161423	330338.470075	42.256474
3502.643214	330304.468878	42.261479
3502.912298	330266.300461	42.266484
3503.085042	330233.132258	42.271488
3502.912971	330205.206605	42.276493
3503.067668	330159.247527	42.281498
3502.655575	330129.502612	42.286503
3503.007562	330089.642370	42.291508
3502.984898	330065.813685	42.296512
3503.315599	330023.133446	42.301517
3503.137918	329987.221993	42.306522
3502.996082	329953.822950	42.311527
3503.153311	329919.385164	42.316532
3502.941637	329892.101349	42.321536
3502.836204	329857.475659	42.326541
3502.942045	329815.822308	42.331546
3502.364700	329791.851259	42.336551
3502.788158	329754.828212	42.341556
3502.760079	329728.736457	42.346560
3502.763679	329693.406830	42.351565
3502.467681	329662.804053	42.356570
3502.137602	329630.527868	42.361575
3502.673858	329601.855166	42.366580
3502.696443	329576.569310	42.371584
3502.640542	329550.252868	42.376589
3502.409807	329520.936966	42.381594
3502.577828	329491.100868	42.386599
3502.868076	329456.870794	42.391604
3502.939685	329430.432596	42.396608
3502.784084	329399.248089	42.401613
3503.012864	329370.979382	42.406618
3502.704929	329335.443785	42.411623
3503.015412	329301.769987	42.416628
3502.824382	329274.228159	42.421632
3502.433782	329241.655891	42.426637
3502.833957	329200.566315	42.431642
3502.846205	329177.621865	42.436647
3503.132384	329146.291783	42.441652
3502.694398	329124.689458	42.446656
3502.283618	329089.703860	42.451661
3502.688156	329059.092830	42.456666
3502.619707	329034.304127	42.461671
3502.483860	328999.402642	42.466676
3502.628401	328983.355835	42.471680
3502.203014	328946.159508	42.476685
3502.688559	328917.646848	42.481690
3502.706430	328897.422952	42.486695
3502.729593	328861.377323	42.491700
3502.927208	328834.334007	42.496704
3502.593000	328808.569289	42.501709
3502.883858	328773.117616	42.506714
3502.505152	328755.168544	42.511719
3502.628012	328715.266419	42.516724
3502.279854	328687.723309	42.521728
3502.331303	328665.815292	42.526733
3502.590494	328634.336408	42.531738
3502.356089	328613.236123	42.536743
3502.235234	328588.506204	42.541748
3502.190155	328553.641004	42.546752
3501.977611	328540.320594	42.551757
3502.501083	328518.008036	42.556762
3502.136582	328501.328414	42.561767
3502.235912	328472.697763	42.566772
3502.498696	328465.458474	42.571776
3502.040550	328431.802356	42.576781
3502.627557	328406.376632	42.581786
3502.085286	328392.573570	42.586791
3502.251604	328377.489673	42.591796
3502.427972	328339.689977	42.596800
3502.372638	328319.222871	42.601805
3502.197268	328293.534727	42.606810
3502.388426	328275.038498	42.611815
3502.123734	328245.548900	42.616820
3502.350283	328223.486084	42.621824
3502.237217	328203.256867	42.626829
3502.581297	328172.222191	42.631834
3502.353064	328161.473139	42.636839
3502.298269	328118.978280	42.641844
3502.023734	328106.557675	42.646848
3502.198971	328084.986088	42.651853
3502.305035	328052.487803	42.656858
3502.259532	328039.420906	42.661863
3502.335680	328011.760116	42.666868
3502.134822	327990.781434	42.671872
3502.267765	327968.249824	42.676877
3502.470214	327945.503846	42.681882
3502.160789	327928.662755	42.686887
3502.449685	327891.023092	42.691892
3501.975061	327888.579236	42.696896
3502.010903	327859.474780	42.701901
3502.311660	327840.884906	42.706906
3502.141557	327818.629515	42.711911
3502.387409	327798.115052	42.716916
3502.305739	327770.962056	42.721920
3502.151662	327755.063181	42.726925
3502.401446	327721.448398	42.731930
3501.888674	327712.371630	42.736935
3502.238822	327683.167034	42.741940
3502.358096	327667.021898	42.746944
3502.230834	327642.012590	42.751949
3502.581913	327622.295548	42.756954
3502.267129	327598.714528	42.761959
3502.147278	327579.834180	42.766964
3502.064318	327559.625365	42.771968
3502.212573	327533.530024	42.776973
3502.229032	327502.164499	42.781978
3501.899784	327498.782180	42.786983
3502.340979	327466.434513	42.791988
3502.103807	327446.504114	42.796993
3502.174741	327426.652718	42.801997
3502.358507	327414.211119	42.807002
3502.043425	327376.385594	42.812007
3502.275991	327358.874488	42.817012
3502.071960	327334.640083	42.822017
3502.076629	327321.615979	42.827021
3501.924484	327293.125539	42.832026
3501.956115	327277.680735	42.837031
3502.321035	327252.975783	42.842036
3502.142204	327242.066139	42.847041
3501.911067	327222.287304	42.852045
3502.011081	327202.761926	42.857050
3501.893799	327181.362765	42.862055
3501.773377	327161.006985	42.867060
3501.989206	327147.288459	42.872065
3501.818632	327128.593884	42.877069
3501.777588	327110.972826	42.882074
3501.789518	327091.283108	42.887079
3501.748068	327093.680756	42.892084
3502.088229	327073.100303	42.897089
3501.564918	327052.807456	42.902093
3501.886447	327039.810032	42.907098
3501.602231	327021.438414	42.912103
3501.700262	327000.641412	42.917108
3501.794551	326995.183333	42.922113
3501.459112	326982.364911	42.927117
3501.899595	326960.166202	42.932122
3501.431101	326961.180727	42.937127
3501.567550	326947.347360	42.942132
3501.648552	326933.548093	42.947137
3501.300229	326919.434390	42.952141
3501.731374	326909.802878	42.957146
3501.752691	326907.128804	42.962151
3501.678623	326883.102739	42.967156
3501.837829	326876.133723	42.972161
3501.625866	326868.637689	42.977165
3501.536823	326837.898620	42.982170
3501.663379	326835.996630	42.987175
3501.835194	326821.267401	42.992180
3501.895341	326806.403004	42.997185
3501.575418	326784.373953	43.002189
3501.803190	326768.593045	43.007194
3501.677876	326772.860715	43.012199
3501.479744	326755.162312	43.017204
3501.530856	326740.909787	43.022209
3501.577816	326736.705480	43.027213
3501.644215	326718.940267	43.032218
3501.599790	326700.225770	43.037223
3501.669575	326684.418655	43.042228
3501.535630	326679.759323	43.047233
3501.572786	326668.103521	43.052237
3501.919538	326640.450349	43.057242
3501.611646	326640.625790	43.062247
3502.044823	326620.819110	43.067252
3501.986172	326615.715571	43.072257
3501.685772	326598.287456	43.077261
3501.927581	326575.381924	43.082266
3501.541438	326569.693654	43.087271
3501.775484	326564.061045	43.092276
3501.894732	326550.586348	43.097281
3501.429292	326521.050547	43.102285
3501.621323	326513.898278	43.107290
3501.449871	326504.818746	43.112295
3501.581115	326478.699940	43.117300
3501.702965	326467.005402	43.122305
3501.539902	326464.716244	43.127309
3502.086541	326450.182650	43.132314
3501.792544	326434.788429	43.137319
3502.042240	326429.280540	43.142324
3501.913974	326406.280146	43.147329
3501.648025	326401.132677	43.152333
3501.686263	326384.694449	43.157338
3501.725087	326364.465991	43.162343
3501.903434	326343.656092	43.167348
3501.833286	326337.104398	43.172353
3501.723925	326318.196378	43.177357
3502.123163	326291.196126	43.182362
3501.986481	326283.281218	43.187367
3501.800514	326256.092625	43.192372
3501.753921	326248.697806	43.197377
3501.644676	326240.905786	43.202381
3501.861244	326217.851373	43.207386
3501.966152	326218.216651	43.212391
3501.723894	326191.876244	43.217396
3501.804022	326178.076854	43.222401
3501.552894	326168.602707	43.227405
3501.942997	326148.522719	43.232410
3501.563971	326140.823732	43.237415
3501.715702	326125.232521	43.242420
3501.877611	326119.840064	43.247425
3501.528279	326095.525878	43.252429
3502.026416	326081.101484	43.257434
3501.876893	326077.919881	43.262439
3501.790927	326048.884028	43.267444
3501.740733	326037.343449	43.272449
3501.539119	326030.100013	43.277453
3501.881172	325997.003544	43.282458
3501.814051	325992.257373	43.287463
3501.470097	325981.627576	43.292468
3501.933529	325972.016230	43.297473
3501.820910	325948.275445	43.302477
3501.957327	325949.348047	43.307482
3501.593140	325930.301623	43.312487
3501.572053	325911.176112	43.317492
3501.961911	325904.679617	43.322497
3501.558562	325887.140103	43.327501
3501.763354	325874.542116	43.332506
3501.695174	325865.802419	43.337511
3501.633337	325843.503567	43.342516
3501.943965	325835.722138	43.347521
3501.604835	325821.555737	43.352525
3501.923978	325806.345230	43.357530
3501.823431	325789.012707	43.362535
3502.005201	325772.704415	43.367540
3501.672661	325759.325524	43.372545
3501.443437	325741.835037	43.377549
3501.931450	325723.214908	43.382554
3501.963416	325724.558220	43.387559
3501.706172	325702.874904	43.392564
3501.880127	325684.736295	43.397569
3501.642204	325676.786221	43.402573
3501.591854	325645.480567	43.407578
3501.285122	325638.100870	43.412583
3501.431736	325631.871299	43.417588
3501.863304	325633.610017	43.422593
3501.730413	325623.354129	43.427597
3501.421867	325596.031630	43.432602
3501.459661	325594.448711	43.437607
3501.581212	325590.334374	43.442612
3501.801963	325564.150109	43.447617
3501.890563	325566.578391	43.452621
3501.622072	325547.313324	43.457626
3501.337335	325532.604127	43.462631
3501.330014	325511.263200	43.467636
3501.562142	325507.716633	43.472641
3501.354534	325511.590299	43.477645
3501.646322	325496.969019	43.482650
3501.580283	325482.200176	43.487655
3501.413488	325475.154698	43.492660
3501.498530	325471.605685	43.497665
3501.524361	325465.140595	43.502669
3501.630203	325442.688120	43.507674
3501.801317	325431.977652	43.512679
3501.406027	325424.510009	43.517684
3501.785256	325415.700266	43.522689
3501.568961	325398.538300	43.527693
3501.565901	325385.260401	43.532698
3501.618076	325389.831158	43.537703
3501.484159	325365.915297	43.542708
3501.566739	325357.686113	43.547713
3501.041754	325354.715779	43.552717
3501.512937	325336.581422	43.557722
3501.196260	325343.855379	43.562727
3501.593830	325334.152430	43.567732
3501.639970	325308.020736	43.572737
3501.626761	325309.803568	43.577741
3501.639041	325296.396053	43.582746
3501.674984	325291.531936	43.587751
3501.446924	325262.110729	43.592756
3501.594593	325259.009788	43.597761
3501.268495	325247.588433	43.602765
3501.626530	325241.885381	43.607770
3501.589886	325223.321611	43.612775
3502.102194	325205.867588	43.617780
3501.529548	325204.812534	43.622785
3501.100923	325184.580254	43.627789
3500.942465	325173.081793	43.632794
3501.228715	325168.661848	43.637799
3501.296204	325161.808629	43.642804
3501.787431	325169.058061	43.647809
3501.452810	325177.301492	43.652813
3501.551762	325150.296553	43.657818
3501.774965	325132.302626	43.662823
3501.480467	325124.895484	43.667828
3501.911099	325110.176046	43.672833
3501.696978	325093.903937	43.677837
3501.862218	325084.466193	43.682842
3501.116428	325084.023276	43.687847
3501.453860	325073.261274	43.692852
3501.650696	325050.387349	43.697857
3501.826811	325041.024208	43.702861
3501.695560	325027.486417	43.707866
3501.651038	325009.839547	43.712871
3501.763686	325001.707343	43.717876
3501.832906	324991.394259	43.722881
3501.358009	324981.649561	43.727885
3501.533361	324951.986996	43.732890
3501.220092	324955.063217	43.737895
3501.954189	324942.712885	43.742900
3501.852774	324926.245024	43.747905
3501.718030	324917.947975	43.752909
3501.969264	324909.361639	43.757914
3501.777016	324886.879146	43.762919
3501.760302	324872.102370	43.767924
3501.786930	324868.409809	43.772929
3501.774583	324859.737480	43.777933
3501.954126	324833.915323	43.782938
3501.641889	324827.070537	43.787943
3502.098105	324806.572543	43.792948
3502.125496	324787.388050	43.797953
3501.902332	324769.997949	43.802957
3502.114560	324749.512633	43.807962
3501.895840	324735.454219	43.812967
3501.721184	324713.579397	43.817972
3501.885831	324700.961886	43.822977
3501.467877	324695.176571	43.827981
3502.099889	324686.225400	43.832986
3501.990339	324662.457946	43.837991
3501.601482	324655.218100	43.842996
3502.207557	324634.416771	43.848001
3501.709065	324616.866144	43.853005
3501.687143	324602.904108	43.858010
3501.614204	324594.953467	43.863015
3501.860865	324583.289751	43.868020
3502.178156	324570.037818	43.873025
3501.842079	324555.005598	43.878029
3501.898790	324538.283914	43.883034
3501.793836	324522.783097	43.888039
3501.802835	324496.733007	43.893044
3502.189403	324478.484308	43.898049
3501.617274	324466.795939	43.903053
3501.785312	324451.761182	43.908058
3501.482322	324445.627161	43.913063
3501.685809	324433.893837	43.918068
3501.907953	324414.526091	43.923073
3501.976620	324407.062041	43.928077
3502.073250	324380.336780	43.933082
3502.026378	324373.501308	43.938087
3501.681359	324359.767771	43.943092
3501.618361	324338.918266	43.948097
3501.475621	324328.282015	43.953101
3501.727639	324319.873502	43.958106
3501.614292	324310.682641	43.963111
3501.683875	324290.041329	43.968116
3501.531193	324280.958365	43.973121
3501.589761	324274.487968	43.978125
3501.785330	324255.022548	43.983130
3501.662215	324229.578028	43.988135
3501.598580	324231.826682	43.993140
3501.894547	324210.590291	43.998145
3501.741720	324206.162573	44.003149
3501.883236	324197.033595	44.008154
3501.841489	324182.565746	44.013159
3501.573062	324163.172823	44.018164
3501.750241	324150.807570	44.023169
3501.570322	324142.949882	44.028173
3501.537330	324114.464017	44.033178
3501.563842	324113.620522	44.038183
3501.314120	324116.178099	44.043188
3501.721937	324104.310983	44.048193
3501.620530	324089.572605	44.053197
3501.665110	324067.434216	44.058202
3501.568632	324066.406439	44.063207
3501.743456	324047.402059	44.068212
3501.627350	324027.145785	44.073217
3501.612315	324025.596504	44.078221
3501.954809	324004.708873	44.083226
3501.671832	324006.559375	44.088231
3501.397885	323981.621616	44.093236
3501.435535	323979.453569	44.098241
3501.483015	323968.100644	44.103245
3501.735011	323944.021865	44.108250
3501.703560	323937.768999	44.113255
3501.623968	323926.537683	44.118260
3501.619359	323905.882339	44.123265
3501.598867	323898.661084	44.128269
3501.758959	323883.805434	44.133274
3501.654640	323888.858721	44.138279
3501.775381	323868.031129	44.143284
3501.631022	323831.829120	44.148289
3501.571708	323852.494737	44.153293
3501.924758	323832.317653	44.158298
3502.035264	323816.248672	44.163303
3501.596640	323804.666435	44.168308
3501.824535	323785.144863	44.173313
3501.751191	323770.147595	44.178317
3501.663154	323756.602628	44.183322
3501.742415	323738.427086	44.188327
3501.475583	323730.684662	44.193332
3501.619584	323714.839354	44.198337
3501.753673	323715.327288	44.203341
3501.801790	323683.495965	44.208346
3501.734343	323677.655708	44.213351
3501.680296	323671.202823	44.218356
3501.814719	323643.962401	44.223361
3501.693024	323650.595640	44.228365
3501.737881	323638.378115	44.233370
3502.006569	323614.957945	44.238375
3501.756878	323610.468989	44.243380
3502.069610	323588.873515	44.248385
3501.577224	323569.591643	44.253389
3501.802588	323549.892284	44.258394
3501.845653	323549.987428	44.263399
3501.390399	323528.893572	44.268404
3501.855237	323512.972588	44.273409
3501.549393	323514.292470	44.278413
3501.441930	323502.938203	44.283418
3501.222866	323483.460927	44.288423
3501.171357	323481.535743	44.293428
3501.651229	323468.715940	44.298433
3501.150909	323468.794282	44.303437
3501.185637	323473.342541	44.308442
3501.566061	323459.520727	44.313447
3501.471587	323444.882790	44.318452
3501.510768	323437.906515	44.323457
3501.382642	323425.105437	44.328461
3501.319827	323418.730200	44.333466
3501.621118	323405.175129	44.338471
3501.563862	323387.682189	44.343476
3501.567271	323379.795694	44.348481
3501.509317	323372.427570	44.353485
3501.366176	323377.436111	44.358490
3501.390419	323352.324158	44.363495
3501.180495	323338.136696	44.368500
3501.641028	323332.569992	44.373505
3501.689393	323337.777549	44.378509
3501.519893	323323.049542	44.383514
3501.675656	323302.012679	44.388519
3501.473362	323297.007498	44.393524
3501.844031	323294.838229	44.398529
3501.530622	323270.262357	44.403533
3501.626867	323257.400710	44.408538
3501.708863	323247.721169	44.413543
3501.752115	323232.603722	44.418548
3501.912704	323211.515180	44.423553
3501.613071	323209.145433	44.428557
3502.025105	323195.827371	44.433562
3501.876557	323178.475811	44.438567
3501.493861	323167.647824	44.443572
3501.385948	323156.318971	44.448577
3501.448193	323142.495917	44.453581
3501.688450	323120.072039	44.458586
3501.448273	323115.759616	44.463591
3501.413034	323123.193476	44.468596
3501.563851	323104.192417	44.473601
3501.501463	323084.741337	44.478605
3501.683591	323073.825022	44.483610
3501.714454	323075.626499	44.488615
3501.307868	323056.712562	44.493620
3501.663966	323043.530392	44.498625
3501.527183	323043.679094	44.503629
3501.479568	323040.074295	44.508634
3501.293152	323037.356128	44.513639
3501.433056	323004.390611	44.518644
3501.831793	323000.207241	44.523649
3501.443033	322999.759357	44.528653
3501.700544	323002.186822	44.533658
3501.581796	322988.086743	44.538663
3501.489994	322968.105984	44.543668
3501.750039	322966.335582	44.548673
3501.514969	322964.032044	44.553677
3501.658046	322934.322198	44.558682
3501.571824	322932.860322	44.563687
3501.130215	322922.016043	44.568692
3501.824757	322924.171674	44.573697
3501.324513	322912.751456	44.578701
3501.443385	322890.422749	44.583706
3501.596711	322883.861004	44.588711
3501.367819	322884.914482	44.593716
3501.478204	322862.103740	44.598721
3501.023765	322855.967719	44.603725
3501.429344	322840.717166	44.608730
3501.418082	322833.367087	44.613735
3501.486655	322833.076655	44.618740
3501.730197	322821.540129	44.623745
3501.172874	322807.305040	44.628749
3501.271955	322805.356282	44.633754
3501.405496	322795.592260	44.638759
3500.916534	322797.398701	44.643764
3501.139860	322789.630348	44.648769
3500.612780	322788.237391	44.653773
3501.100378	322786.151573	44.658778
3501.797930	322784.032931	44.663783
3501.467535	322778.589807	44.668788
3501.090333	322762.011562	44.673793
3501.187432	322756.170890	44.678797
3501.329013	322739.053621	44.683802
3501.278472	322743.920564	44.688807
3501.664462	322737.296981	44.693812
3501.438037	322722.068875	44.698817
3501.209779	322710.504321	44.703821
3501.362801	322701.932883	44.708826
3501.206273	322702.288188	44.713831
3501.179060	322698.909124	44.718836
3501.546254	322694.959610	44.723841
3501.295852	322689.275014	44.728845
3501.507605	322668.865063	44.733850
3501.383406	322658.683394	44.738855
3501.427328	322655.318645	44.743860
3501.496298	322641.138222	44.748865
3501.410893	322644.153548	44.753869
3501.183666	322619.182226	44.758874
3501.374292	322616.583161	44.763879
3501.054448	322616.226255	44.768884
3501.471999	322602.347474	44.773889
3501.186756	322605.241409	44.778893
3501.394349	322607.117035	44.783898
3501.518712	322589.519047	44.788903
3501.633571	322570.854080	44.793908
3501.405249	322562.036959	44.798913
3501.153293	322569.937269	44.803917
3501.355320	322561.994128	44.808922
3501.330453	322546.937962	44.813927
3501.031170	322536.885394	44.818932
3501.741087	322524.003898	44.823937
3501.407572	322521.308695	44.828941
3501.568828	322513.728071	44.833946
3501.437990	322511.586289	44.838951
3501.230908	322489.969756	44.843956
3501.538974	322481.195957	44.848961
3501.290237	322480.039307	44.853965
3501.379482	322477.685039	44.858970
3501.483379	322467.849257	44.863975
3501.326617	322459.071805	44.868980
3501.461155	322442.947659	44.873985
3500.824233	322436.026039	44.878989
3501.351786	322429.100441	44.883994
3501.254750	322426.571777	44.888999
3501.093389	322436.594873	44.894004
3501.338523	322427.983538	44.899009
3501.149031	322426.181636	44.904013
3501.128856	322406.978037	44.909018
3501.235817	322398.871650	44.914023
3501.117939	322395.252340	44.919028
3501.357880	322393.535937	44.924033
3501.344478	322400.941072	44.929037
3501.347907	322399.999392	44.934042
3501.453932	322386.779794	44.939047
3501.205106	322371.834897	44.944052
3501.325114	322353.347106	44.949057
3501.173918	322354.388449	44.954061
3501.200546	322345.455104	44.959066
3501.133265	322353.250265	44.964071
3501.275706	322352.744764	44.969076
3501.287939	322345.543564	44.974081
3501.132016	322351.673568	44.979085
3501.413952	322327.945330	44.984090
3501.286937	322311.175154	44.989095
3501.457099	322305.857228	44.994100
3501.255263	322302.556312	44.999105
3501.091099	322303.345288	45.004109
3500.820940	322305.753532	45.009114
3501.211025	322302.283756	45.014119
3501.019599	322306.969259	45.019124
3501.382110	322287.069784	45.024129
3500.821323	322272.784176	45.029133
3501.091204	322268.798957	45.034138
3500.875425	322268.069623	45.039143
3500.862986	322258.709894	45.044148
3501.546576	322260.943592	45.049153
3501.384067	322267.150957	45.054157
3501.319571	322258.028323	45.059162
3501.496267	322255.355095	45.064167
3501.239445	322252.037331	45.069172
3501.337148	322235.384631	45.074177
3501.239226	322218.915146	45.079181
3501.026107	322221.594314	45.084186
3501.601848	322216.060331	45.089191
3501.033698	322219.990670	45.094196
3501.004958	322205.698177	45.099201
3500.710051	322217.446663	45.104205
3500.863579	322213.098034	45.109210
3501.224327	322208.945965	45.114215
3500.660940	322218.192456	45.119220
3501.196339	322214.776273	45.124225
3501.228399	322214.186270	45.129229
3501.390661	322196.734830	45.134234
3501.288732	322174.313064	45.139239
3501.240410	322170.377584	45.144244
3501.656834	322165.733452	45.149249
3501.143686	322173.140437	45.154253
3501.026158	322164.458549	45.159258
3501.237115	322166.588066	45.164263
3500.984424	322168.103196	45.169268
3501.430943	322153.024072	45.174273
3501.454488	322140.656802	45.179277
3501.118412	322119.518160	45.184282
3501.362345	322117.673922	45.189287
3500.987530	322128.620854	45.194292
3501.365683	322123.702863	45.199297
3501.165624	322127.321266	45.204301
3501.463614	322110.764402	45.209306
3501.224490	322092.129124	45.214311
3500.877320	322084.449833	45.219316
3501.230812	322079.968169	45.224321
3501.009466	322088.626978	45.229325
3501.085508	322079.507773	45.234330
3501.500986	322078.501667	45.239335
3501.177575	322078.297952	45.244340
3501.271330	322071.287477	45.249345
3501.225878	322077.323932	45.254349
3501.436962	322051.266155	45.259354
3501.203451	322036.242424	45.264359
3501.043039	322048.733124	45.269364
3501.073791	322042.902725	45.274369
3500.847797	322046.016394	45.279373
3501.191268	322039.755507	45.284378
3501.486769	322043.016603	45.289383
3501.340524	322037.646351	45.294388
3501.100489	322019.087503	45.299393
3501.253463	322011.482644	45.304397
3501.506387	321999.511949	45.309402
3501.238038	321996.552124	45.314407
3501.178361	321999.614354	45.319412
3501.005695	321991.220888	45.324417
3501.105884	321993.164213	45.329421
3501.067914	321979.000285	45.334426
3501.250418	321980.421944	45.339431
3500.577361	321993.399845	45.344436
3501.322450	321977.383585	45.349441
3500.993546	321966.343358	45.354445
3501.193515	321963.386634	45.359450
3501.577521	321944.145074	45.364455
3501.011824	321951.026077	45.369460
3501.390221	321937.763755	45.374465
3500.956576	321941.545891	45.379469
3501.327383	321939.096694	45.384474
3501.245930	321935.955007	45.389479
3501.527118	321931.179353	45.394484
3501.393812	321908.660591	45.399489
3501.426976	321911.097756	45.404493
3501.265926	321904.788526	45.409498
3501.160653	321897.783699	45.414503
3501.171651	321895.670590	45.419508
3501.426891	321887.795322	45.424513
3501.156064	321870.589537	45.429517
3501.454015	321854.108898	45.434522
3501.592411	321861.693915	45.439527
3501.628282	321855.226692	45.444532
3501.654882	321831.512653	45.449537
3501.465288	321827.293948	45.454541
3501.437975	321816.257410	45.459546
3501.348701	321804.314719	45.464551
3501.190016	321809.860115	45.469556
3501.436270	321796.389449	45.474561
3501.211742	321786.096054	45.479565
3501.372124	321778.515436	45.484570
3501.601534	321776.037455	45.489575
3501.626298	321769.088596	45.494580
3501.759224	321759.680590	45.499585
3501.350011	321741.656867	45.504589
3501.382334	321737.047299	45.509594
3501.340695	321734.586252	45.514599
3501.405970	321732.159370	45.519604
3501.689979	321704.283739	45.524609
3501.288030	321699.665741	45.529613
3501.511750	321691.108484	45.534618
3501.223079	321682.529573	45.539623
3501.287300	321690.940297	45.544628
3501.372633	321675.459550	45.549633
3501.242722	321654.008602	45.554637
3501.396389	321652.000377	45.559642
3501.033363	321641.118039	45.564647
3501.306699	321645.934473	45.569652
3501.394805	321638.873930	45.574657
3501.278603	321644.997827	45.579661
3501.385711	321626.995095	45.584666
3501.285766	321617.190982	45.589671
3501.169931	321613.851126	45.594676
3501.487846	321600.216554	45.599681
3501.502216	321602.707554	45.604685
3501.195759	321607.004077	45.609690
3501.503274	321581.872217	45.614695
3501.002576	321580.093492	45.619700
3501.314999	321564.348240	45.624705
3501.360220	321567.114261	45.629709
3501.103095	321570.512671	45.634714
3501.533734	321561.007196	45.639719
3501.414152	321563.417381	45.644724
3501.378304	321536.278528	45.649729
3501.365920	321527.681830	45.654733
3501.274068	321521.768767	45.659738
3501.511591	321527.506658	45.664743
3501.311687	321522.958813	45.669748
3501.235723	321501.855515	45.674753
3501.357030	321489.498211	45.679757
3501.252670	321477.176183	45.684762
3501.455623	321472.616231	45.689767
3501.339052	321479.477973	45.694772
3501.397617	321472.142179	45.699777
3501.450222	321469.742703	45.704781
3501.695375	321451.489353	45.709786
3501.547484	321439.810124	45.714791
3501.489772	321448.545241	45.719796
3501.393611	321424.188722	45.724801
3501.210966	321414.804535	45.729805
3501.396970	321403.988942	45.734810
3501.401359	321396.763365	45.739815
3501.423285	321398.108388	45.744820
3501.660951	321376.498072	45.749825
3501.359643	321313.758848	45.754829
3501.204851	321211.131700	45.759834
3501.373949	321066.527938	45.764839
3500.934682	320877.294429	45.769844
3501.008097	320620.282415	45.774849
3500.756591	320336.606803	45.779853
3500.418679	319997.913935	45.784858
3500.390817	319605.641571	45.789863
3499.890934	319179.754908	45.794868
3499.525657	318682.809599	45.799873
3499.251691	318149.894678	45.804877
3498.605235	317578.969660	45.809882
3497.920598	316949.117757	45.814887
3497.833306	316276.800670	45.819892
3497.118248	315550.682150	45.824897
3496.238990	314786.360722	45.829901
3495.823615	313975.899474	45.834906
3495.323107	313104.394849	45.839911
3494.570741	312198.052988	45.844916
3493.622577	311232.918632	45.849921
3492.887514	310235.261592	45.854925
3491.978141	309182.976268	45.859930
3491.400718	308072.570242	45.864935
3490.501822	306926.918210	45.869940
3489.139469	305730.618313	45.874945
3488.229968	304491.006229	45.879949
3487.085036	303194.214798	45.884954
3486.153728	301862.973907	45.889959
3484.931584	300492.855510	45.894964
3483.403497	299060.850989	45.899969
3482.155988	297599.265804	45.904973
3481.005342	296087.128092	45.909978
3479.811578	294539.067193	45.914983
3478.084853	292948.539505	45.919988
3476.826051	291311.567815	45.924993
3475.509136	289632.890174	45.929997
3473.886705	287908.979115	45.935002
3472.382560	286150.152637	45.940007
3470.852867	284353.453171	45.945012
3469.040115	282518.130176	45.950017
3467.504060	280644.374670	45.955021
3465.758440	278733.381556	45.960026
3464.217761	276782.589735	45.965031
3462.395940	274783.264391	45.970036
3460.665499	272756.580936	45.975041
3458.820888	270693.888826	45.980045
3456.678619	268593.917735	45.985050
3454.754703	266456.994117	45.990055
3452.657865	264281.167404	45.995060
3450.225602	262082.556782	46.000065
3448.189748	259861.736595	46.005069
3446.228993	257591.153568	46.010074
3444.168893	255289.858328	46.015079
3441.747959	252971.263105	46.020084
3439.589894	250598.218041	46.025089
3437.389388	248220.280245	46.030093
3434.945090	245799.537368	46.035098
3432.641453	243348.868864	46.040103
3429.694158	240882.127320	46.045108
3427.482787	238378.037755	46.050113
3424.453923	235851.363050	46.055117
3421.903815	233298.236463	46.060122
3419.345674	230719.425367	46.065127
3416.599558	228133.706962	46.070132
3413.917433	225519.601071	46.075137
3411.081941	222884.353694	46.080141
3408.435840	220203.720214	46.085146
3405.334688	217531.316536	46.090151
3402.345168	214824.245686	46.095156
3399.188016	212106.293464	46.100161
3396.245159	209363.805252	46.105165
3392.818925	206601.683865	46.110170
3390.079403	203825.329612	46.115175
3386.204594	201032.664717	46.120180
3383.208687	198223.405816	46.125185
3379.516690	195416.192130	46.130189
3376.084372	192603.570847	46.135194
3372.642441	189766.771094	46.140199
3369.097336	186936.805119	46.145204
3365.322349	184093.250308	46.150209
3361.786944	181242.584023	46.155213
3357.939490	178400.532649	46.160218
3354.162745	175519.339197	46.165223
3350.144783	172671.713792	46.170228
3346.232480	169806.621540	46.175233
3342.243797	166934.091118	46.180237
3338.043394	164083.273730	46.185242
3334.164347	161214.351632	46.190247
3329.393799	158377.809358	46.195252
3324.994393	155529.122570	46.200257
3320.515935	152694.101770	46.205261
3315.414137	149884.568762	46.210266
3310.629151	147074.749875	46.215271
3305.030586	144318.778644	46.220276
3299.237823	141552.351117	46.225281
3293.129031	138805.583037	46.230285
3287.047600	136132.733507	46.235290
3280.981240	133510.427102	46.240295
3274.271768	130946.623798	46.245300
3267.127535	128429.200985	46.250305
3259.986684	125965.781042	46.255309
3252.600778	123573.859397	46.260314
3245.495803	121231.686290	46.265319
3238.042262	118985.033913	46.270324
3230.364223	116795.860209	46.275329
3222.011093	114704.409405	46.280333
3212.918404	112686.404789	46.285338
3204.899541	110777.635486	46.290343
3195.691942	108947.596620	46.295348
3186.347368	107227.742677	46.300353
3177.827377	105604.776455	46.305357
3169.029378	104079.467829	46.310362
3159.810406	102663.381298	46.315367
3151.243025	101330.113902	46.320372
3143.248574	100097.437317	46.325377
3135.189814	98953.099139	46.330381
3127.329472	97905.602665	46.335386
3120.094079	96913.618848	46.340391
3113.125404	96032.391979	46.345396
3106.389944	95201.706589	46.350401
3100.032475	94448.108412	46.355405
3093.652606	93751.906914	46.360410
3088.257650	93097.158248	46.365415
3083.005067	92511.527909	46.370420
3077.744875	91962.289771	46.375425
3072.822399	91446.744927	46.380429
3067.961813	90960.919585	46.385434
3063.582841	90508.279056	46.390439
3059.129939	90096.583235	46.395444
3055.261730	89697.304264	46.400449
3051.237538	89315.830387	46.405453
3047.591487	88944.466742	46.410458
3044.201364	88587.285120	46.415463
3040.320498	88267.004564	46.420468
3036.816321	87916.150701	46.425473
3033.260995	87589.359635	46.430477
3030.019076	87270.578086	46.435482
3026.886703	86946.116536	46.440487
3023.259088	86643.232250	46.445492
3020.040115	86327.633513	46.450497
3017.422940	86009.962192	46.455501
3013.727288	85701.584621	46.460506
3010.155933	85381.541236	46.465511
3006.833573	85083.351346	46.470516
3003.715908	84778.069192	46.475521
3000.772280	84460.834288	46.480525
2997.496440	84152.610826	46.485530
2993.886660	83822.936030	46.490535
2990.539495	83519.176709	46.495540
2987.130549	83193.720634	46.500545
2983.793739	82878.178012	46.505549
2980.330808	82575.615507	46.510554
2976.869499	82262.093532	46.515559
2973.428112	81949.753245	46.520564
2969.997376	81634.505884	46.525569
2966.237292	81322.666951	46.530573
2962.772864	81013.249449	46.535578
2959.298331	80700.661431	46.540583
2955.685928	80401.956192	46.545588
2952.305322	80094.098047	46.550593
2948.801859	79789.247383	46.555597
2944.952997	79483.425252	46.560602
2941.240762	79176.022857	46.565607
2937.711543	78878.679975	46.570612
2934.177396	78582.611161	46.575617
2930.751219	78294.377792	46.580621
2926.906216	78004.142711	46.585626
2923.335052	77714.604502	46.590631
2919.151522	77432.518709	46.595636
2915.902250	77142.529778	46.600641
2912.488600	76861.180393	46.605645
2908.548593	76590.216020	46.610650
2904.832608	76310.773813	46.615655
2901.159552	76041.322554	46.620660
2898.030887	75768.245603	46.625665
2894.186179	75506.484446	46.630669
2890.352434	75243.822445	46.635674
2886.642921	74978.197318	46.640679
2883.239481	74721.771989	46.645684
2879.968699	74465.506145	46.650689
2876.053279	74206.638678	46.655693
2872.511183	73952.083740	46.660698
2868.968291	73702.725142	46.665703
2865.007592	73458.272400	46.670708
2861.594850	73210.726649	46.675713
2858.233508	72966.629128	46.680717
2854.698190	72721.748368	46.685722
2851.193540	72474.807966	46.690727
2847.265806	72239.046842	46.695732
2843.821676	72001.802713	46.700737
2840.485551	71762.651845	46.705741
2836.707180	71533.019420	46.710746
2833.507017	71277.039910	46.715751
2829.657326	71056.349221	46.720756
2826.178104	70811.591692	46.725761
2823.017373	70583.191503	46.730765
2819.328216	70341.899463	46.735770
2816.123311	70105.511152	46.740775
2812.425402	69866.313540	46.745780
2808.801879	69633.289837	46.750785
2805.232680	69396.114257	46.755789
2802.019515	69175.816049	46.760794
2797.929968	68922.880849	46.765799
2794.793840	68703.539541	46.770804
2791.468540	68475.634325	46.775809
2788.192356	68244.397054	46.780813
2784.660929	68017.613645	46.785818
2780.943002	67770.008390	46.790823
2777.474571	67538.356830	46.795828
2774.198542	67307.254923	46.800833
2770.637631	67061.656909	46.805837
2766.836690	66833.624833	46.810842
2763.529962	66588.607338	46.815847
2759.926172	66369.136958	46.820852
2756.494184	66130.522800	46.825857
2753.367188	65895.049615	46.830861
2749.729200	65663.466991	46.835866
2746.329365	65420.880989	46.840871
2742.779522	65191.497779	46.845876
2739.071835	64945.790833	46.850881
2735.996442	64712.846780	46.855885
2732.201956	64474.920611	46.860890
2728.981219	64237.268736	46.865895
2725.542508	64003.569306	46.870900
2722.400386	63755.824300	46.875905
2718.690509	63508.278444	46.880909
2715.049625	63272.408747	46.885914
2711.660555	63032.915971	46.890919
2707.962007	62790.916183	46.895924
2704.584190	62545.669876	46.900929
2700.947352	62307.422351	46.905933
2697.044786	62072.233274	46.910938
2693.563500	61824.788996	46.915943
2690.443871	61610.406113	46.920948
2686.700032	61352.834351	46.925953
2683.535966	61124.094549	46.930957
2679.705965	60879.163957	46.935962
2676.490380	60638.943736	46.940967
2673.119520	60400.812630	46.945972
2669.671911	60155.493103	46.950977
2666.090420	59913.826864	46.955981
2662.515132	59675.525372	46.960986
2658.886538	59419.675617	46.965991
2655.286102	59188.464769	46.970996
2652.083205	58948.842980	46.976001
2648.408683	58701.784075	46.981005
2645.141492	58468.427545	46.986010
2641.616412	58215.607465	46.991015
2637.948711	57972.666826	46.996020
2634.627073	57734.693707	47.001025
2631.464166	57479.178652	47.006029
2627.654539	57239.763871	47.011034
2624.123307	56992.033787	47.016039
2620.833825	56754.503147	47.021044
2617.174703	56509.919852	47.026049
2613.778229	56258.933932	47.031053
2609.911088	56006.603001	47.036058
2606.805630	55758.609696	47.041063
2603.370993	55519.128088	47.046068
2599.242672	55269.954768	47.051073
2596.105322	55027.855640	47.056077
2592.730519	54775.936596	47.061082
2589.062733	54530.575561	47.066087
2585.980065	54288.900510	47.071092
2582.277346	54034.585337	47.076097
2578.911671	53783.113206	47.081101
2574.921155	53548.623625	47.086106
2571.501146	53289.647291	47.091111
2567.892537	53047.451855	47.096116
2564.474189	52814.929262	47.101121
2560.940833	52551.049459	47.106125
2557.041356	52317.611058	47.111130
2553.970774	52067.506826	47.116135
2550.469000	51823.353441	47.121140
2546.987078	51581.311979	47.126145
2543.720026	51331.817316	47.131149
2540.434217	51090.410033	47.136154
2536.761377	50830.980350	47.141159
2532.833269	50595.793872	47.146164
2529.034363	50342.954887	47.151169
2525.790582	50093.533361	47.156173
2522.113955	49847.417311	47.161178
2519.042272	49599.705923	47.166183
2515.317664	49355.994026	47.171188
2512.280481	49104.628930	47.176193
2508.604772	48845.006397	47.181197
2505.210526	48607.092690	47.186202
2501.589348	48356.778598	47.191207
2497.896792	48112.998811	47.196212
2493.751391	47857.958019	47.201217
2491.112896	47610.568281	47.206221
2487.353984	47375.699181	47.211226
2484.446749	47122.331337	47.216231
2480.449114	46875.377868	47.221236
2477.001316	46626.539847	47.226241
2473.957082	46366.986353	47.231245
2470.320443	46120.923322	47.236250
2466.890997	45860.909506	47.241255
2463.122997	45615.589213	47.246260
2459.789003	45372.442442	47.251265
2456.199404	45101.401971	47.256269
2452.422016	44860.492721	47.261274
2448.948172	44603.925035	47.266279
2445.536473	44350.819504	47.271284
2441.993949	44104.218498	47.276289
2438.658216	43842.672432	47.281293
2435.076884	43602.735388	47.286298
2431.867915	43343.141241	47.291303
2428.237330	43095.163744	47.296308
2424.829696	42844.180070	47.301313
2421.372358	42581.596211	47.306317
2417.877043	42331.710082	47.311322
2414.309149	42077.786180	47.316327
2410.542299	41821.702338	47.321332
2407.016939	41559.363233	47.326337
2403.902201	41308.389270	47.331341
2400.081795	41056.507704	47.336346
2396.849609	40801.062298	47.341351
2393.572716	40537.916638	47.346356
2390.177357	40290.466581	47.351361
2386.930398	40036.243478	47.356365
2383.005838	39765.897854	47.361370
2379.385673	39509.253846	47.366375
2375.693919	39257.911860	47.371380
2372.253873	38991.076002	47.376385
2369.043058	38726.768978	47.381389
2365.103540	38473.148039	47.386394
2361.458418	38213.251833	47.391399
2357.920937	37958.217299	47.396404
2354.712272	37702.652518	47.401409
2351.598313	37433.090484	47.406413
2347.672052	37180.541437	47.411418
2344.383038	36918.513079	47.416423
2340.762172	36660.755619	47.421428
2337.300351	36397.448396	47.426433
2333.842870	36135.994833	47.431437
2330.212226	35881.253169	47.436442
2326.825232	35624.853599	47.441447
2323.264127	35350.601681	47.446452
2319.889747	35096.108255	47.451457
2316.585576	34829.734006	47.456461
2312.721600	34560.705948	47.461466
2309.412633	34299.822260	47.466471
2306.260697	34055.569084	47.471476
2302.689006	33783.266111	47.476481
2299.694955	33506.306177	47.481485
2295.818823	33242.722659	47.486490
2292.145430	32964.234481	47.491495
2288.639313	32696.201087	47.496500
2285.508458	32429.963183	47.501505
2281.838075	32153.209325	47.506509
2278.364611	31881.828374	47.511514
2274.925442	31616.587113	47.516519
2271.186061	31345.489258	47.521524
2267.578515	31071.978612	47.526529
2264.218730	30800.587644	47.531533
2260.535685	30533.459016	47.536538
2257.148982	30252.382806	47.541543
2253.984174	29990.852247	47.546548
2250.326782	29714.433073	47.551553
2247.104498	29438.393147	47.556557
2243.473992	29169.607233	47.561562
2239.927565	28886.324914	47.566567
2236.178764	28624.535527	47.571572
2233.200798	28350.379459	47.576577
2229.691521	28062.552747	47.581581
2226.009507	27794.204833	47.586586
2222.486274	27513.295191	47.591591
2219.109059	27229.286961	47.596596
2215.708300	26956.489429	47.601601
2212.024635	26672.448211	47.606605
2208.733585	26386.017750	47.611610
2205.399299	26102.911988	47.616615
2201.730240	25820.394807	47.621620
2198.168889	25539.835260	47.626625
2194.942217	25240.884430	47.631629
2191.456330	24966.169220	47.636634
2187.985888	24671.959914	47.641639
2184.531526	24388.637241	47.646644
2180.778571	24106.024199	47.651649
2177.936685	23803.315515	47.656653
2174.054698	23524.519551	47.661658
2170.556089	23220.490622	47.666663
2167.226318	22937.016973	47.671668
2163.538335	22640.438833	47.676673
2160.510667	22345.630664	47.681677
2157.010367	22053.270118	47.686682
2153.538144	21752.566389	47.691687
2150.242547	21454.208820	47.696692
2146.540964	21149.052422	47.701697
2143.168854	20839.661999	47.706701
2139.391456	20555.057223	47.711706
2136.253862	20242.003468	47.716711
2132.976089	19940.657165	47.721716
2129.034959	19635.834097	47.726721
2125.622422	19318.176096	47.731725
2122.268603	19030.575458	47.736730
2118.779813	18715.688159	47.741735
2115.197661	18412.544511	47.746740
2111.556528	18107.432347	47.751745
2108.001336	17793.539418	47.756749
2104.265546	17494.677673	47.761754
2100.672596	17191.554773	47.766759
2097.362041	16896.290133	47.771764
2093.429502	16598.245692	47.776769
2090.266637	16292.143643	47.781773
2086.866121	15999.468568	47.786778
2083.097120	15704.126094	47.791783
2079.258268	15392.187981	47.796788
2075.704112	15097.331026	47.801793
2072.045703	14805.702421	47.806797
2067.986517	14525.362299	47.811802
2064.268613	14249.013023	47.816807
2060.592892	13963.833797	47.821812
2056.601201	13693.696836	47.826817
2053.270150	13422.713144	47.831821
2049.178361	13163.285003	47.836826
2045.541126	12904.384501	47.841831
2041.881124	12641.758417	47.846836
2037.744879	12390.687006	47.851841
2034.197031	12133.236242	47.856845
2030.180491	11895.661551	47.861850
2026.605249	11649.077394	47.866855
2022.786950	11430.801667	47.871860
2018.793243	11216.902480	47.876865
2014.992919	10993.731630	47.881869
2010.794599	10780.413944	47.886874
2007.024282	10578.975636	47.891879
2003.340569	10383.815987	47.896884
1999.562765	10185.934889	47.901889
1995.926939	9990.572428	47.906893
1992.258529	9815.026805	47.911898
1988.947771	9620.842405	47.916903
1985.664470	9436.829444	47.921908
1981.737549	9249.364268	47.926913
1978.326104	9063.285891	47.931917
1974.941378	8883.225680	47.936922
1971.325062	8699.110710	47.941927
1968.079431	8518.728405	47.946932
1964.320751	8346.724261	47.951937
1961.306053	8165.530612	47.956941
1957.597493	7981.893009	47.961946
1954.690263	7793.852548	47.966951
1951.214946	7616.037628	47.971956
1947.663470	7435.185190	47.976961
1944.345184	7248.436342	47.981965
1940.635561	7062.785591	47.986970
1937.445062	6885.293978	47.991975
1933.717159	6694.886482	47.996980
1929.939275	6513.205017	48.001985
1926.622266	6324.487280	48.006989
1923.099493	6147.722595	48.011994
1919.903892	5958.043339	48.016999
1916.571700	5774.046101	48.022004
1912.848356	5599.109391	48.027009
1909.118245	5408.832722	48.032013
1906.063956	5229.247122	48.037018
1902.767410	5030.273218	48.042023
1899.040631	4849.726932	48.047028
1895.432436	4668.122725	48.052033
1892.116971	4477.461785	48.057037
1888.670833	4294.978346	48.062042
1884.799071	4098.395792	48.067047
1881.807686	3915.401977	48.072052
1877.933762	3731.633590	48.077057
1874.427996	3543.777983	48.082061
1870.892767	3363.020338	48.087066
1867.630831	3166.985352	48.092071
1864.270363	2981.973429	48.097076
1860.572909	2792.260209	48.102081
1856.874072	2602.852972	48.107085
1853.715590	2419.406839	48.112090
1849.858567	2241.447856	48.117095
1846.539854	2050.572557	48.122100
1842.779625	1878.417755	48.127105
1839.200417	1691.507399	48.132109
1835.683612	1513.670094	48.137114
1832.131568	1326.790933	48.142119
1828.576864	1155.313337	48.147124
1824.788008	979.191351	48.152129
1821.475252	798.010226	48.157133
1817.992017	631.993762	48.162138
1814.229205	462.611933	48.167143
1810.575512	293.692380	48.172148
1806.484930	139.605198	48.177153
1801.593686	23.395110	48.182157
1790.657968	54.852729	48.187162
1783.718959	50.256587	48.192167
1778.741113	57.262103	48.197172
1775.249882	59.286094	48.202177
1773.215248	58.234703	48.207181
1770.544350	63.205537	48.212186
1767.855755	59.070535	48.217191
1765.206264	58.143845	48.222196
1762.047113	67.563476	48.227201
1759.051937	72.344614	48.232205
1755.395691	71.891863	48.237210
1751.664021	52.806595	48.242215
1748.383004	54.987524	48.247220
1744.680619	70.604653	48.252225
1741.585762	65.406922	48.257229
1738.001585	75.446746	48.262234
1734.776208	65.849602	48.267239
1731.677652	67.910230	48.272244
1727.745785	65.466296	48.277249
1724.522692	71.516998	48.282253
1721.095277	66.247931	48.287258
1717.456836	69.146045	48.292263
1714.055599	65.828118	48.297268
1710.791445	62.713370	48.302273
1707.201203	66.901104	48.307277
1704.074678	60.398527	48.312282
1700.384611	68.515516	48.317287
1697.011209	62.421745	48.322292
1693.772905	71.724065	48.327297
1690.263375	65.164373	48.332301
1686.596157	66.997633	48.337306
1683.117087	65.071319	48.342311
1679.682570	58.930172	48.347316
1675.898809	69.744740	48.352321
1673.100319	62.061355	48.357325
1669.384037	64.879916	48.362330
1665.756059	63.786848	48.367335
1662.769058	66.649463	48.372340
1658.778712	67.416481	48.377345
1655.188579	67.117937	48.382349
1651.681340	71.545803	48.387354
1648.665881	65.560545	48.392359
1645.233704	63.655380	48.397364
1641.672370	73.685326	48.402369
1638.207013	69.614984	48.407373
1634.349182	68.342763	48.412378
1630.456097	68.534576	48.417383
1627.352392	67.122181	48.422388
1624.067508	69.262624	48.427393
1620.570131	66.254013	48.432397
1617.098233	65.588958	48.437402
1613.789944	69.893947	48.442407
1610.544670	69.772401	48.447412
1606.810507	69.505908	48.452417
1603.475100	65.247560	48.457421
1599.403625	61.060126	48.462426
1596.068385	68.811557	48.467431
1592.825337	61.764100	48.472436
1588.812212	67.100080	48.477441
1585.793064	65.127127	48.482445
1582.557718	65.908884	48.487450
1579.216727	70.570184	48.492455
1575.525911	66.006799	48.497460
1571.681687	66.213133	48.502465
1568.641815	60.794883	48.507469
1564.774613	58.363042	48.512474
1560.906119	52.609412	48.517479
1557.555684	66.912301	48.522484
1554.193566	63.192834	48.527489
1551.124005	68.817747	48.532493
1547.747084	61.196466	48.537498
1543.637365	63.494511	48.542503
1540.577164	53.738718	48.547508
1536.865615	63.055031	48.552513
1533.563873	55.520070	48.557517
1529.878602	64.395669	48.562522
1526.167362	59.645674	48.567527
1523.113589	59.592261	48.572532
1519.420265	65.495150	48.577537
1515.934256	62.288643	48.582541
1512.418680	69.929115	48.587546
1508.828719	71.310576	48.592551
1505.594330	68.254515	48.597556
1501.753784	71.472240	48.602561
1498.316779	71.542095	48.607565
1495.119842	66.509127	48.612570
1491.192001	70.990222	48.617575
1488.232470	70.589868	48.622580
1484.374427	60.617285	48.627585
1481.402139	60.434069	48.632589
1477.874757	63.473068	48.637594
1474.199612	64.877365	48.642599
1470.743516	71.205054	48.647604
1467.066731	78.301291	48.652609
1463.249693	57.103459	48.657613
1459.799032	64.161136	48.662618
1456.342684	67.151057	48.667623
1453.206735	67.167476	48.672628
1449.438462	67.763771	48.677633
1446.199858	62.465257	48.682637
1442.347945	71.610581	48.687642
1438.987733	69.115249	48.692647
1435.836312	59.126996	48.697652
1432.226137	58.663988	48.702657
1428.632677	58.590676	48.707661
1425.104988	63.180001	48.712666
1421.312309	70.848056	48.717671
1418.256027	63.353810	48.722676
1414.452265	67.087835	48.727681
1411.125344	62.847212	48.732685
1407.208484	62.808712	48.737690
1403.888104	55.222935	48.742695
1400.835165	53.653969	48.747700
1396.808808	67.831740	48.752705
1393.582580	66.644247	48.757709
1390.106410	56.640409	48.762714
1386.547315	57.979114	48.767719
1383.334393	60.734797	48.772724
1379.753270	63.605068	48.777729
1376.250493	58.477649	48.782733
1372.590362	63.701500	48.787738
1368.883426	62.902480	48.792743
1365.513516	57.146819	48.797748
1361.618119	61.259042	48.802753
1358.103546	59.613655	48.807757
1354.570645	65.377588	48.812762
1351.702553	55.727838	48.817767
1348.608413	53.899580	48.822772
1344.941248	57.764107	48.827777
1341.712596	61.322706	48.832781
1337.669798	55.416123	48.837786
1334.161145	57.430330	48.842791
1330.523703	49.859417	48.847796
1326.903115	63.546572	48.852801
1323.330847	58.442708	48.857805
1319.950008	50.562707	48.862810
1316.459642	63.669488	48.867815
1313.550839	57.063370	48.872820
1309.405023	64.878490	48.877825
1306.161243	59.656770	48.882829
1302.717733	56.798037	48.887834
1298.838352	61.046983	48.892839
1295.193923	54.454789	48.897844
1291.917885	67.142044	48.902849
1288.575487	59.395241	48.907853
1285.052483	49.911319	48.912858
1281.344100	62.932014	48.917863
1278.593185	51.065113	48.922868
1274.674135	56.566811	48.927873
1271.496439	51.932719	48.932877
1267.609886	53.575832	48.937882
1263.607093	62.953637	48.942887
1260.615180	49.681782	48.947892
1256.706836	56.469474	48.952897
1253.194510	52.624938	48.957901
1250.145723	56.721725	48.962906
1246.910487	64.773971	48.967911
1243.374602	47.524972	48.972916
1239.350941	60.740567	48.977921
1236.106950	59.451503	48.982925
1232.378937	47.898942	48.987930
1228.775053	64.434083	48.992935
1225.873492	58.782328	48.997940
1222.348386	58.682571	49.002945
1218.476947	59.579846	49.007949
1214.792529	62.463179	49.012954
1211.171948	59.932761	49.017959
1208.094751	51.758494	49.022964
1204.529201	57.641479	49.027969
1200.945980	61.448621	49.032973
1197.128453	57.170990	49.037978
1193.729278	67.261088	49.042983
1190.835242	54.457996	49.047988
1186.712534	58.555248	49.052993
1183.648551	54.896816	49.057997
1180.424482	56.091393	49.063002
1176.692481	63.607653	49.068007
1173.011331	60.166069	49.073012
1169.227140	57.999809	49.078017
1166.024520	62.914816	49.083021
1162.246538	61.532206	49.088026
1158.727395	61.624530	49.093031
1155.485551	56.443695	49.098036
1151.845138	59.870660	49.103041
1148.632902	61.269042	49.108045
1144.941907	60.410665	49.113050
1141.467357	66.820433	49.118055
1138.114867	58.296980	49.123060
1134.574352	69.611464	49.128065
1130.788089	65.680146	49.133069
1127.549286	64.798436	49.138074
1123.816689	64.224994	49.143079
1120.589062	61.054116	49.148084
1116.781317	69.980652	49.153089
1113.292834	62.946498	49.158093
1110.303121	55.723527	49.163098
1106.584537	61.399546	49.168103
1103.363772	62.736002	49.173108
1099.610112	66.788165	49.178113
1095.739034	58.251009	49.183117
1092.215813	60.169503	49.188122
1088.880304	69.335326	49.193127
1085.921921	64.863117	49.198132
1081.928575	59.872736	49.203137
1078.597956	59.163609	49.208141
1074.631892	63.290165	49.213146
1070.972706	56.697215	49.218151
1067.919926	54.815118	49.223156
1064.329332	63.505186	49.228161
1060.766368	53.717568	49.233165
1057.726079	49.150628	49.238170
1054.111602	56.809878	49.243175
1050.679719	54.287946	49.248180
1046.849559	58.488147	49.253185
1043.661673	50.286982	49.258189
1039.569132	53.041287	49.263194
1036.222717	59.443678	49.268199
1033.138276	55.529071	49.273204
1029.391400	64.559998	49.278209
1026.057889	53.682928	49.283213
1022.333688	65.481785	49.288218
1018.533159	57.620163	49.293223
1015.605073	60.568645	49.298228
1011.728046	67.563496	49.303233
1008.157618	57.308828	49.308237
1004.976781	56.921128	49.313242
1001.242241	61.289874	49.318247
997.948056	55.456063	49.323252
994.519944	63.677782	49.328257
990.841585	53.490644	49.333261
987.349881	56.366031	49.338266
983.904893	58.177399	49.343271
981.035437	52.197999	49.348276
977.068481	59.766930	49.353281
973.303472	51.099332	49.358285
969.767255	58.262296	49.363290
966.160139	56.055738	49.368295
962.636945	50.352715	49.373300
959.631856	55.483626	49.378305
956.134357	53.785097	49.383309
951.933646	60.485796	49.388314
948.399807	58.036816	49.393319
945.597516	50.616881	49.398324
941.689830	58.258802	49.403329
938.483843	49.494197	49.408333
934.486559	53.881960	49.413338
930.963942	59.334363	49.418343
927.906702	55.077010	49.423348
924.631803	57.019955	49.428353
920.891832	57.545582	49.433357
917.279513	52.410195	49.438362
913.641332	65.514912	49.443367
910.277558	53.487851	49.448372
906.815552	56.197262	49.453377
903.407814	58.211636	49.458381
900.025085	52.549920	49.463386
896.239805	54.984084	49.468391
892.865827	51.880502	49.473396
889.283062	52.840273	49.478401
885.704868	53.830968	49.483405
882.322037	45.521191	49.488410
878.646770	56.078547	49.493415
875.772912	54.143188	49.498420
871.694436	57.961554	49.503425
868.212332	56.096132	49.508429
864.718516	56.232055	49.513434
861.008756	56.287899	49.518439
857.522018	60.611565	49.523444
854.067026	61.443774	49.528449
850.795107	51.639153	49.533453
847.737403	52.469263	49.538458
843.956026	48.632223	49.543463
839.982605	54.699417	49.548468
836.241102	55.832763	49.553473
833.100112	46.210133	49.558477
829.810311	53.470594	49.563482
826.234619	57.602554	49.568487
823.026710	43.440891	49.573492
819.497084	59.913875	49.578497
815.844728	48.906497	49.583501
812.347882	48.739192	49.588506
808.682328	54.913213	49.593511
805.549326	50.851268	49.598516
801.747062	60.659739	49.603521
798.082459	61.872807	49.608525
794.752493	55.864346	49.613530
791.170783	55.191478	49.618535
787.528516	50.877093	49.623540
784.202120	52.720581	49.628545
780.597702	56.932986	49.633549
777.244407	59.837392	49.638554
773.438557	54.207186	49.643559
770.480202	58.062155	49.648564
766.661185	53.617268	49.653569
762.967488	55.739748	49.658573
759.734474	52.047825	49.663578
756.040722	59.703766	49.668583
752.413090	54.520227	49.673588
749.176612	64.986766	49.678593
745.667874	57.775609	49.683597
742.452086	43.010937	49.688602
738.606128	53.478005	49.693607
735.264148	50.227103	49.698612
731.276632	54.774768	49.703617
727.869539	58.007157	49.708621
724.635466	43.362416	49.713626
721.144631	55.880952	49.718631
718.024782	51.497438	49.723636
714.034084	53.195045	49.728641
710.808964	52.516985	49.733645
707.065727	51.606854	49.738650
703.600783	61.166375	49.743655
700.575233	45.220313	49.748660
696.294315	48.244706	49.753665
692.910264	59.958749	49.758669
689.459740	55.373930	49.763674
685.965620	55.029074	49.768679
682.647894	54.099770	49.773684
678.800102	58.049767	49.778689
675.537492	59.029084	49.783693
672.351393	56.870606	49.788698
668.552712	53.808313	49.793703
665.261904	48.252524	49.798708
661.536100	55.499059	49.803713
658.512998	55.301912	49.808717
654.672707	49.053893	49.813722
650.928678	58.286975	49.818727
647.479221	52.161247	49.823732
644.148778	59.440785	49.828737
640.808425	57.388736	49.833741
637.159142	45.476126	49.838746
633.305249	63.382512	49.843751
629.818835	56.477961	49.848756
626.184207	54.813693	49.853761
622.696989	54.499419	49.858765
619.384305	54.195777	49.863770
616.179845	68.181783	49.868775
612.741898	56.590423	49.873780
608.973469	53.381049	49.878785
605.414580	54.599782	49.883789
601.915973	45.523645	49.888794
598.646587	53.537118	49.893799
595.141783	50.640805	49.898804
591.420232	57.595633	49.903809
587.920845	45.839907	49.908813
584.613287	51.499188	49.913818
581.069853	54.085424	49.918823
577.518302	53.670510	49.923828
573.888630	57.342775	49.928833
570.142837	57.224044	49.933837
566.987090	56.237776	49.938842
563.197722	60.722837	49.943847
560.134344	51.796850	49.948852
556.522718	57.003889	49.953857
552.887102	51.609718	49.958861
549.389729	51.594457	49.963866
546.089477	59.840575	49.968871
542.768127	62.218034	49.973876
538.891457	59.221797	49.978881
535.251181	45.944242	49.983885
531.900952	48.595148	49.988890
528.041376	55.059083	49.993895
525.036520	51.027794	49.998900
521.386723	60.958010	50.003905
518.457511	44.965308	50.008909
514.917015	47.475176	50.013914
510.669623	58.517728	50.018919
507.489097	48.132632	50.023924
503.858188	53.829930	50.028929
500.675335	53.262385	50.033933
496.926124	56.080201	50.038938
493.248974	58.968989	50.043943
490.291205	53.838836	50.048948
486.609937	52.311646	50.053953
482.860078	46.207734	50.058957
479.113728	48.705567	50.063962
475.363789	60.891432	50.068967
471.917660	54.211599	50.073972
468.426283	59.896547	50.078977
465.314531	56.495794	50.083981
462.075430	55.946565	50.088986
458.457856	60.284534	50.093991
454.975380	55.951592	50.098996
451.348325	54.362141	50.104001
447.858509	56.576195	50.109005
444.472756	55.420352	50.114010
440.634835	57.018214	50.119015
437.377800	48.869264	50.124020
433.775181	66.973631	50.129025
430.212765	54.237589	50.134029
426.996720	49.780669	50.139034
423.444318	54.658938	50.144039
420.263620	51.082340	50.149044
416.411769	59.560430	50.154049
412.388234	56.514489	50.159053
409.600077	52.212017	50.164058
405.720631	57.625576	50.169063
402.276986	60.231050	50.174068
398.733048	53.370417	50.179073
395.006431	59.778775	50.184077
392.122766	48.423409	50.189082
388.298525	59.080185	50.194087
384.912510	57.054370	50.199092
381.762130	53.178807	50.204097
378.064080	55.741881	50.209101
374.524454	56.169907	50.214106
370.304082	65.183472	50.219111
367.159621	52.299735	50.224116
363.511757	54.734731	50.229121
360.110843	59.298227	50.234125
356.957390	62.791572	50.239130
353.269284	54.776620	50.244135
349.991612	56.416474	50.249140
346.007314	54.740658	50.254145
342.555539	45.831314	50.259149
339.359747	50.780301	50.264154
335.744957	59.635738	50.269159
332.483109	56.635036	50.274164
329.134140	61.497292	50.279169
325.282595	57.671474	50.284173
321.903289	42.679519	50.289178
317.917867	47.613000	50.294183
314.593666	48.330008	50.299188
311.170857	46.392246	50.304193
307.749763	54.246073	50.309197
303.981158	44.971925	50.314202
300.443089	59.991027	50.319207
297.034998	51.233046	50.324212
293.831218	60.106371	50.329217
289.999590	56.707722	50.334221
286.752032	48.984462	50.339226
283.031054	61.675218	50.344231
279.899199	49.574164	50.349236
276.278381	59.572685	50.354241
272.702077	51.334615	50.359245
269.167857	51.834603	50.364250
265.777093	60.193060	50.369255
262.446539	52.833988	50.374260
258.656220	52.871061	50.379265
254.950081	57.991774	50.384269
251.799654	56.663100	50.389274
248.061336	52.961951	50.394279
244.578880	41.868136	50.399284
241.191965	46.173212	50.404289
237.391130	51.745365	50.409293
234.317803	55.245179	50.414298
230.651870	50.444365	50.419303
227.357664	51.672400	50.424308
223.657307	55.431799	50.429313
220.196247	53.088776	50.434317
216.831576	53.467311	50.439322
213.153640	52.287730	50.444327
209.761790	52.733800	50.449332
206.041509	52.566934	50.454337
201.976629	58.180467	50.459341
199.024373	45.424892	50.464346
195.365930	50.367311	50.469351
192.366803	49.976740	50.474356
188.872795	45.512845	50.479361
185.094389	50.980263	50.484365
181.952587	45.385513	50.489370
177.794957	57.189251	50.494375
174.433478	54.362409	50.499380
171.277666	57.169648	50.504385
167.533900	50.919397	50.509389
163.903621	46.862840	50.514394
160.173038	55.309368	50.519399
157.035450	54.111596	50.524404
153.638379	55.574074	50.529409
150.158873	49.465929	50.534413
147.002788	47.809151	50.539418
143.010217	50.339366	50.544423
139.551916	51.346369	50.549428
136.121367	55.563407	50.554433
132.278939	48.831921	50.559437
129.172848	39.403450	50.564442
125.554213	53.834103	50.569447
121.558469	54.574136	50.574452
118.438786	55.075677	50.579457
114.917476	64.520824	50.584461
111.729232	55.152680	50.589466
108.293161	63.666983	50.594471
105.021000	45.965990	50.599476
101.276076	53.377071	50.604481
97.118258	55.477616	50.609485
93.947627	54.379958	50.614490
90.428465	63.634950	50.619495
87.120770	47.872590	50.624500
83.523477	56.367865	50.629505
79.776850	49.346149	50.634509
76.245665	47.757657	50.639514
72.585527	62.631434	50.644519
69.082793	55.891047	50.649524
65.896881	58.595470	50.654529
62.643578	56.957118	50.659533
59.387066	50.687526	50.664538
55.789477	53.937344	50.669543
52.258860	55.303725	50.674548
48.613131	52.986544	50.679553
44.826829	61.666472	50.684557
41.377408	47.119081	50.689562
37.563170	52.323251	50.694567
33.959271	44.118098	50.699572
31.015249	57.107976	50.704577
27.480710	50.919924	50.709581
24.068054	48.828829	50.714586
20.429609	56.811717	50.719591
17.173955	51.105158	50.724596
13.487302	51.955000	50.729601
9.778349	55.079916	50.734605
6.685870	50.875890	50.739610
2.782082	53.819364	50.744615